Thu Jun 16 18:35:49 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
0.024291	96.970750	0.000000
-0.107003	85.318312	0.005005
-0.741391	70.980363	0.010010
-0.242374	69.741306	0.015014
-0.720624	65.207166	0.020019
-0.939797	64.632947	0.025024
-1.189340	61.945425	0.030029
-1.358529	43.329203	0.035034
-1.514692	35.572260	0.040038
-1.830607	39.745717	0.045043
-1.999969	16.929124	0.050048
-2.227608	8.149019	0.055053
-2.746760	2.808546	0.060058
-3.103149	1.695857	0.065062
-3.689979	-2.133090	0.070067
-3.453969	-3.614284	0.075072
-3.976154	-6.583088	0.080077
-4.640279	3.123137	0.085082
-4.983215	0.117903	0.090086
-5.066944	-0.729574	0.095091
-4.858276	-1.263704	0.100096
-5.013831	-10.253809	0.105101
-6.137898	-11.851785	0.110106
-6.045569	-6.630614	0.115110
-6.603854	-9.710653	0.120115
-6.479271	-20.531412	0.125120
-6.733238	-12.996686	0.130125
-7.052854	-10.850279	0.135130
-6.672369	-6.545479	0.140134
-7.796756	-3.815719	0.145139
-8.199012	-0.435197	0.150144
-8.528089	1.389090	0.155149
-8.486186	-5.272546	0.160154
-8.380899	-12.674007	0.165158
-8.500286	-5.706190	0.170163
-8.481338	-15.194626	0.175168
-8.340152	0.775872	0.180173
-9.464712	-2.590211	0.185178
-10.022103	-12.744428	0.190182
-10.150602	-5.671419	0.195187
-10.096227	-12.745023	0.200192
-9.954656	-8.833145	0.205197
-11.115226	-2.242771	0.210202
-11.572706	-5.689496	0.215206
-11.575894	-1.080573	0.220211
-11.109121	-9.608131	0.225216
-11.082582	-7.333851	0.230221
-12.061139	-1.144596	0.235226
-11.478457	-12.236696	0.240230
-12.622214	-17.717026	0.245235
-13.092181	-7.337710	0.250240
-12.921914	-10.893796	0.255245
-13.638074	-0.695270	0.260250
-13.279254	-6.930506	0.265254
-13.825557	-8.687297	0.270259
-13.509438	-15.557813	0.275264
-14.103499	-5.188275	0.280269
-14.518663	5.662836	0.285274
-14.572164	-4.963651	0.290278
-14.714076	-4.015568	0.295283
-15.268846	-4.409723	0.300288
-15.624323	-19.930275	0.305293
-16.444408	-8.731981	0.310298
-16.153592	-7.868629	0.315302
-16.422981	-4.671167	0.320307
-16.597330	-22.456768	0.325312
-16.297283	-12.953198	0.330317
-16.663249	0.171462	0.335322
-16.348775	-2.623757	0.340326
-17.273865	1.000916	0.345331
-17.821179	2.708650	0.350336
-17.561429	-9.596121	0.355341
-18.578260	3.967878	0.360346
-18.718064	-10.702207	0.365350
-19.191151	-0.349304	0.370355
-18.787568	-8.137263	0.375360
-18.828209	-1.277364	0.380365
-19.223826	4.195712	0.385370
-19.355819	-2.868406	0.390374
-20.519469	7.851179	0.395379
-20.508979	4.164831	0.400384
-20.452569	-1.854791	0.405389
-21.143931	5.875742	0.410394
-20.743108	-7.616272	0.415398
-21.171601	-1.402591	0.420403
-21.043218	-4.293434	0.425408
-21.864644	-8.550935	0.430413
-22.281693	11.241167	0.435418
-22.177015	-3.855856	0.440422
-22.408130	5.737970	0.445427
-22.459928	-2.046262	0.450432
-22.707491	-4.179363	0.455437
-23.811409	-0.431118	0.460442
-23.939238	-13.798767	0.465446
-24.218033	-3.661767	0.470451
-23.974693	-3.545673	0.475456
-24.118402	-8.147503	0.480461
-24.373115	-1.036766	0.485466
-24.315673	-7.346205	0.490470
-24.885640	-0.918346	0.495475
-25.576816	-1.409232	0.500480
-25.475164	-0.132924	0.505485
-26.058951	-3.034228	0.510490
-25.876584	0.230937	0.515494
-25.782252	5.587826	0.520499
-26.271262	0.579083	0.525504
-26.930948	2.736805	0.530509
-27.466850	13.332528	0.535514
-27.504110	8.379944	0.540518
-27.788190	8.050760	0.545523
-27.453171	4.051417	0.550528
-27.320753	0.775943	0.555533
-27.766354	-0.524736	0.560538
-28.236730	-0.614577	0.565542
-28.728947	1.478374	0.570547
-28.746591	1.221770	0.575552
-29.467857	3.325542	0.580557
-30.326410	17.143674	0.585562
-29.624672	2.114111	0.590566
-29.916740	13.255449	0.595571
-30.619041	6.707917	0.600576
-30.714349	1.118346	0.605581
-30.832113	-2.635200	0.610586
-30.536909	-5.589719	0.615590
-30.795636	3.793897	0.620595
-31.494698	4.455517	0.625600
-31.608595	5.679841	0.630605
-32.136726	9.303141	0.635610
-31.917709	4.829596	0.640614
-32.633364	5.781734	0.645619
-33.556536	-12.165335	0.650624
-33.282420	-6.120549	0.655629
-33.080869	-1.659606	0.660634
-33.594756	-5.907553	0.665638
-33.656897	5.170624	0.670643
-34.095060	-6.417609	0.675648
-34.182961	-6.020164	0.680653
-34.369420	0.945716	0.685658
-35.005766	-1.938515	0.690662
-34.914001	1.243757	0.695667
-35.450847	-0.712398	0.700672
-35.483681	2.926025	0.705677
-35.967132	6.109340	0.710682
-35.784258	-3.199411	0.715686
-36.145459	10.732944	0.720691
-36.793110	3.000912	0.725696
-37.026911	2.355617	0.730701
-37.547197	0.811174	0.735706
-37.180004	-10.221145	0.740710
-37.337942	1.653810	0.745715
-37.470860	-5.260197	0.750720
-37.288821	-12.990034	0.755725
-38.480944	-8.012578	0.760730
-38.539720	3.068395	0.765734
-38.643209	-1.910926	0.770739
-38.968154	-2.750997	0.775744
-39.231454	0.197343	0.780749
-39.911122	1.480440	0.785754
-40.415243	-5.104571	0.790758
-40.569114	6.986657	0.795763
-40.329198	-7.182862	0.800768
-39.966584	-8.737760	0.805773
-40.747373	-1.135501	0.810778
-40.384724	-1.150505	0.815782
-41.342562	0.034329	0.820787
-41.760172	-1.240391	0.825792
-41.897137	-6.159031	0.830797
-42.446782	-3.027325	0.835802
-42.047294	-9.156617	0.840806
-41.897104	-11.017064	0.845811
-42.588323	9.695408	0.850816
-42.645243	-2.745265	0.855821
-43.310051	4.721614	0.860826
-43.141531	-2.288873	0.865830
-43.910356	8.239187	0.870835
-44.561237	6.084147	0.875840
-44.445668	3.780936	0.880845
-45.038375	10.672585	0.885850
-45.101812	5.558392	0.890854
-44.776655	-1.076162	0.895859
-45.054438	0.569667	0.900864
-44.919957	-8.721218	0.905869
-45.888721	6.828058	0.910874
-46.029292	-5.049085	0.915878
-46.270723	-6.540956	0.920883
-46.555516	-8.291338	0.925888
-46.526295	-16.780518	0.930893
-47.000898	-4.012403	0.935898
-47.309812	-14.459737	0.940902
-47.898507	-8.853242	0.945907
-48.223435	-2.044426	0.950912
-48.373666	-7.566513	0.955917
-48.329439	0.399188	0.960922
-48.181737	-2.480149	0.965926
-48.538304	0.011937	0.970931
-48.756377	12.204640	0.975936
-49.269260	-10.059093	0.980941
-49.928734	4.978745	0.985946
-49.873297	-3.722739	0.990950
-50.127140	-6.792315	0.995955
-49.909488	-7.641652	1.000960
-50.278516	-16.216451	1.005965
-51.141405	2.420672	1.010970
-51.223330	-7.178458	1.015974
-51.713789	-1.272796	1.020979
-51.828793	-2.492852	1.025984
-51.624690	-4.483259	1.030989
-51.928984	5.166165	1.035994
-51.831838	-7.466593	1.040998
-52.486252	-2.629493	1.046003
-52.982029	1.143446	1.051008
-52.599497	-6.734560	1.056013
-53.330621	-4.832188	1.061018
-53.489929	1.494165	1.066022
-54.350625	-8.976126	1.071027
-54.497052	0.775160	1.076032
-54.489139	-0.602537	1.081037
-55.023911	2.041529	1.086042
-54.807158	-1.915774	1.091046
-54.731070	-1.124471	1.096051
-54.897526	-5.313223	1.101056
-54.884346	-0.333205	1.106061
-55.807942	1.668456	1.111066
-56.183233	-5.679924	1.116070
-56.214767	2.686208	1.121075
-56.301851	0.270381	1.126080
-56.903967	-2.415783	1.131085
-57.726553	2.682232	1.136090
-57.704095	4.755142	1.141094
-58.135686	-7.134378	1.146099
-58.143258	0.611201	1.151104
-57.904137	-11.116479	1.156109
-57.986407	4.027518	1.161114
-58.017367	-3.132118	1.166118
-58.014340	-3.479350	1.171123
-59.256926	2.669295	1.176128
-59.255484	1.537429	1.181133
-59.726615	-6.514501	1.186138
-59.725800	0.631647	1.191142
-60.038678	1.006193	1.196147
-60.762150	3.473086	1.201152
-61.050880	-0.877280	1.206157
-61.466215	-9.346070	1.211162
-61.584304	-6.200052	1.216166
-61.561142	-1.051900	1.221171
-61.621842	-7.117768	1.226176
-61.053096	-10.097861	1.231181
-61.478796	0.322681	1.236186
-61.805707	-0.656956	1.241190
-62.380710	-3.290971	1.246195
-62.782580	-2.207980	1.251200
-62.659389	6.543084	1.256205
-63.701446	1.712956	1.261210
-64.046438	-7.548311	1.266214
-64.213668	-5.772672	1.271219
-64.388464	-0.179231	1.276224
-64.170983	-9.080629	1.281229
-64.538864	-10.423350	1.286234
-64.684566	-5.899794	1.291238
-64.487614	-4.088054	1.296243
-65.611329	-5.610015	1.301248
-65.591556	-6.160579	1.306253
-66.018305	5.230703	1.311258
-65.933175	-3.225301	1.316262
-66.075204	7.842499	1.321267
-66.505744	1.721435	1.326272
-67.059169	-9.688019	1.331277
-67.514457	1.620471	1.336282
-67.370917	-8.039694	1.341286
-67.682311	-9.573176	1.346291
-67.752186	-5.238743	1.351296
-67.739228	1.986099	1.356301
-68.382883	8.139943	1.361306
-68.728231	2.619123	1.366310
-68.948974	1.372542	1.371315
-69.058768	10.118901	1.376320
-68.885836	-4.571394	1.381325
-69.349139	7.419338	1.386330
-69.673434	7.277833	1.391334
-70.287916	3.331033	1.396339
-70.288441	5.498306	1.401344
-70.354624	-1.176639	1.406349
-70.937999	3.821072	1.411354
-71.172837	9.598565	1.416358
-71.693496	7.189873	1.421363
-72.059605	0.320127	1.426368
-72.090160	-10.315568	1.431373
-72.454328	5.044307	1.436378
-71.880945	-11.708636	1.441382
-72.173198	-5.592943	1.446387
-72.439165	7.527919	1.451392
-72.985562	-3.666153	1.456397
-73.569221	6.554184	1.461402
-73.647462	-4.149105	1.466406
-73.921778	2.830209	1.471411
-74.173423	-4.789285	1.476416
-74.141025	-2.806019	1.481421
-74.849726	0.311527	1.486426
-75.064499	-3.278100	1.491430
-75.722819	-1.304888	1.496435
-75.883295	4.592511	1.501440
-75.589808	7.941516	1.506445
-75.893126	11.079871	1.511450
-75.443572	-4.123665	1.516454
-75.777198	1.925667	1.521459
-76.690645	-4.264356	1.526464
-76.973844	-1.340153	1.531469
-77.671410	2.445320	1.536474
-77.558216	7.847922	1.541478
-77.493951	2.961927	1.546483
-77.787235	6.194022	1.551488
-77.693807	-3.056043	1.556493
-78.524407	2.551566	1.561498
-79.018046	-1.894762	1.566502
-79.159218	4.067320	1.571507
-79.142926	8.150252	1.576512
-79.079607	0.555357	1.581517
-79.056514	-0.249396	1.586522
-79.857778	-9.452320	1.591526
-80.433511	-16.300732	1.596531
-80.744578	-18.931107	1.601536
-80.787822	-16.389881	1.606541
-81.180302	-17.996974	1.611546
-80.828591	-16.547521	1.616550
-80.692301	-8.232120	1.621555
-81.668136	-10.965430	1.626560
-81.727795	-6.808586	1.631565
-82.307705	-1.266875	1.636570
-81.920915	-4.228639	1.641574
-82.413651	-2.383025	1.646579
-83.118496	-0.914930	1.651584
-83.417590	-4.792898	1.656589
-83.730172	7.306403	1.661594
-83.848108	-7.595180	1.666598
-84.156384	-4.567685	1.671603
-83.992597	-1.602422	1.676608
-83.768794	-4.829267	1.681613
-85.022893	-0.697190	1.686618
-85.288250	-1.849088	1.691622
-85.151717	-6.648960	1.696627
-85.766037	0.395423	1.701632
-85.220590	-1.814671	1.706637
-85.517560	2.563807	1.711642
-85.746432	-7.675768	1.716646
-86.544322	-2.827484	1.721651
-86.875209	1.655155	1.726656
-86.755647	-2.280955	1.731661
-87.203941	-6.586695	1.736666
-87.143676	-9.878161	1.741670
-87.951962	-2.009724	1.746675
-88.147357	-2.759230	1.751680
-88.605516	-5.810130	1.756685
-88.697319	-2.960375	1.761690
-88.613224	-9.865945	1.766694
-88.606554	-0.761685	1.771699
-89.119372	-0.632597	1.776704
-88.588843	-6.058830	1.781709
-89.525627	-4.814823	1.786714
-90.006106	-10.357008	1.791718
-90.452405	-6.841843	1.796723
-90.747023	-7.924186	1.801728
-90.584985	-11.237503	1.806733
-90.741995	-2.607654	1.811738
-91.027401	-18.601869	1.816742
-91.407347	-5.396676	1.821747
-91.938885	3.675387	1.826752
-91.740025	-2.868938	1.831757
-92.423780	5.250419	1.836762
-92.093176	-2.767677	1.841766
-92.130395	-15.085608	1.846771
-93.137005	-13.773434	1.851776
-93.341318	-16.927943	1.856781
-93.801683	-8.970015	1.861786
-93.637131	-7.814500	1.866790
-93.638881	-14.940381	1.871795
-93.875620	3.639822	1.876800
-94.335987	4.914896	1.881805
-94.725470	1.682860	1.886810
-95.012755	0.012901	1.891814
-95.081662	-5.384704	1.896819
-95.142066	1.817731	1.901824
-95.622837	-7.398598	1.906829
-96.495587	-4.366405	1.911834
-96.405163	-14.177211	1.916838
-96.561699	-7.212830	1.921843
-96.716896	3.139033	1.926848
-96.708419	-1.962770	1.931853
-96.701386	12.324058	1.936858
-97.370980	-1.301119	1.941862
-97.678025	1.492363	1.946867
-97.995438	0.882987	1.951872
-97.659819	-9.654093	1.956877
-98.197731	-4.590103	1.961882
-98.737836	-11.173102	1.966886
-99.188104	-7.977316	1.971891
-99.748758	3.837519	1.976896
-99.728796	-2.420935	1.981901
-99.935723	-0.646627	1.986906
-99.893667	-9.483021	1.991910
-99.717910	-3.334084	1.996915
-100.068495	-3.839713	2.006912
-99.949671	3.540653	2.016909
-99.942174	-0.923971	2.026906
-99.704961	-0.689423	2.036902
-98.833895	-0.169102	2.046899
-98.027103	2.377566	2.056896
-97.519665	4.310789	2.066893
-97.280542	-0.575879	2.076890
-96.808588	-0.692225	2.086886
-96.048857	2.366546	2.096883
-95.737608	7.170763	2.106880
-95.360909	-4.582135	2.116877
-94.483594	-7.115866	2.126874
-94.436781	-7.997487	2.136870
-93.434167	-3.253995	2.146867
-93.033564	-0.503385	2.156864
-92.935879	-5.420661	2.166861
-92.314015	-3.321580	2.176858
-91.776126	-6.353819	2.186854
-90.905113	3.879490	2.196851
-90.042657	-0.347064	2.206848
-90.218653	5.916463	2.216845
-90.003035	-4.806841	2.226842
-89.531763	-5.452391	2.236838
-88.729357	-5.760852	2.246835
-87.898324	-7.014636	2.256832
-87.139197	-3.616798	2.266829
-86.854524	-0.624228	2.276826
-86.966037	-5.945814	2.286822
-86.374633	-3.911634	2.296819
-85.536469	-10.210742	2.306816
-85.377657	-5.347404	2.316813
-84.579879	-2.121955	2.326810
-83.935359	-4.638795	2.336806
-83.561933	0.410098	2.346803
-83.131831	-3.219140	2.356800
-82.187617	-6.219454	2.366797
-82.146525	-8.315233	2.376794
-82.148672	1.195036	2.386790
-80.930402	-4.589173	2.396787
-80.665017	6.271079	2.406784
-80.227199	-2.339476	2.416781
-79.474522	5.143232	2.426778
-79.345739	-9.241062	2.436774
-78.481279	-6.842464	2.446771
-77.823723	-7.063666	2.456768
-77.592246	-1.917277	2.466765
-77.472982	-1.557935	2.476762
-76.345877	1.966627	2.486758
-75.947577	-2.574487	2.496755
-75.917256	-10.358857	2.506752
-75.018264	-9.853866	2.516749
-74.524708	-9.427867	2.526746
-74.508685	-7.989469	2.536742
-73.345238	-0.165499	2.546739
-72.951455	-3.594136	2.556736
-72.903301	4.668123	2.566733
-72.057370	-2.131906	2.576730
-71.502143	-1.984783	2.586726
-71.082476	-0.284152	2.596723
-70.312417	-5.995026	2.606720
-69.860645	-1.893004	2.616717
-69.570011	-3.420200	2.626714
-69.518168	-7.126946	2.636710
-68.401531	-9.033998	2.646707
-68.131222	-4.006192	2.656704
-68.003463	-0.876164	2.666701
-66.840680	1.643977	2.676698
-66.553865	-3.979083	2.686694
-66.262671	1.629019	2.696691
-65.398860	-4.774838	2.706688
-65.237950	2.363181	2.716685
-64.433293	1.694491	2.726682
-63.650270	0.312623	2.736678
-63.741231	-6.823312	2.746675
-63.521098	-7.427256	2.756672
-62.375563	-7.438143	2.766669
-61.981380	-10.795822	2.776666
-61.804528	2.179340	2.786662
-60.684005	-2.983531	2.796659
-60.341300	-3.945711	2.806656
-60.436876	-3.135292	2.816653
-59.719369	-3.478961	2.826650
-58.863727	-9.896579	2.836646
-58.840245	-0.934778	2.846643
-57.626024	-0.323681	2.856640
-57.413713	4.873739	2.866637
-57.460822	6.579748	2.876634
-56.357431	10.510472	2.886630
-56.036852	7.992294	2.896627
-55.774835	3.919944	2.906624
-55.018543	2.585217	2.916621
-54.396253	0.428009	2.926618
-54.065608	5.634915	2.936614
-53.501845	9.209416	2.946611
-52.659212	5.643231	2.956608
-52.421511	4.283474	2.966605
-52.561714	3.474346	2.976602
-51.723374	-2.195607	2.986598
-51.298295	2.548165	2.996595
-50.022166	1.326375	3.006592
-49.731472	1.994231	3.016589
-49.533066	11.047151	3.026586
-49.385468	12.534780	3.036582
-48.618843	0.055800	3.046579
-47.978141	0.027391	3.056576
-47.866213	5.472994	3.066573
-46.790936	10.302927	3.076570
-46.251840	10.132075	3.086566
-46.216606	15.329228	3.096563
-45.563126	-1.491939	3.106560
-44.984645	3.435848	3.116557
-44.838302	-2.419890	3.126554
-43.663957	3.567335	3.136550
-43.239911	-1.577980	3.146547
-43.329948	5.183276	3.156544
-42.880335	1.184039	3.166541
-41.887738	4.031173	3.176538
-41.549597	-2.720053	3.186534
-40.519110	0.799395	3.196531
-40.151333	0.836686	3.206528
-40.293600	8.881244	3.216525
-39.802582	1.824017	3.226522
-39.033959	4.888935	3.236518
-38.782125	4.799339	3.246515
-37.639240	-4.655603	3.256512
-37.148411	-5.990958	3.266509
-37.082901	-0.399046	3.276506
-36.903298	-2.716316	3.286502
-35.829843	-4.590593	3.296499
-35.578787	0.335988	3.306496
-34.969698	-5.640575	3.316493
-34.127677	1.753734	3.326490
-33.699148	-7.913623	3.336486
-33.595098	0.230444	3.346483
-33.538058	-2.080845	3.356480
-32.442859	-9.107572	3.366477
-32.093085	-10.801157	3.376474
-30.965030	0.049345	3.386470
-30.547482	-2.859581	3.396467
-30.440616	-1.851223	3.406464
-30.461049	-3.559442	3.416461
-30.054427	-1.398754	3.426458
-29.012694	2.419972	3.436454
-27.920167	2.357347	3.446451
-27.707935	2.309315	3.456448
-27.836896	2.303196	3.466445
-27.180337	0.068019	3.476442
-26.205024	1.165934	3.486438
-25.649559	2.780363	3.496435
-25.592496	1.076524	3.506432
-25.315579	1.304958	3.516429
-24.362353	4.931859	3.526426
-24.222495	6.057995	3.536422
-23.498750	5.432959	3.546419
-22.753638	0.520555	3.556416
-22.537543	4.840474	3.566413
-21.941686	4.625128	3.576410
-21.289550	3.702889	3.586406
-20.923267	4.474519	3.596403
-20.598735	-0.419746	3.606400
-19.963857	-4.223092	3.616397
-19.720650	-3.003203	3.626394
-18.673648	-1.326326	3.636390
-18.228379	0.080551	3.646387
-18.058380	-0.737414	3.656384
-17.722601	-0.326331	3.666381
-16.808594	-3.583959	3.676378
-16.581232	1.546374	3.686374
-15.910203	5.855370	3.696371
-15.244267	7.036665	3.706368
-14.659756	7.776282	3.716365
-14.723220	3.293202	3.726362
-14.040688	-6.943326	3.736358
-13.501719	-4.525402	3.746355
-12.876723	0.940517	3.756352
-11.971461	7.782618	3.766349
-11.754874	2.124389	3.776346
-11.627330	-2.010788	3.786342
-11.527822	-0.365656	3.796339
-10.465910	2.733922	3.806336
-10.014877	0.546392	3.816333
-8.705736	4.995457	3.826330
-8.751737	3.089009	3.836326
-8.384949	0.265719	3.846323
-8.375985	-2.907491	3.856320
-7.266838	0.138200	3.866317
-6.716258	4.143693	3.876314
-6.969138	7.733431	3.886310
-5.893310	2.876072	3.896307
-5.249802	3.634785	3.906304
-5.018948	-0.650572	3.916301
-4.151931	-3.451523	3.926298
-3.822147	0.340936	3.936294
-3.788381	0.120143	3.946291
-3.269350	13.010822	3.956288
-2.746526	25.902170	3.966285
-2.379915	38.046578	3.976282
-1.998363	49.575194	3.986278
-1.548084	65.798308	3.996275
-0.916735	86.600170	4.006272
-0.250163	107.014943	4.016269
0.000000	110.392577	4.021274
-0.188307	126.157405	4.026278
0.154501	130.203482	4.031283
0.249078	147.322985	4.036288
0.415510	143.223017	4.041293
0.306544	151.285839	4.046298
0.423119	158.980206	4.051302
0.595040	159.951218	4.056307
0.602632	171.175646	4.061312
0.670961	161.450748	4.066317
0.333658	172.522826	4.071322
0.710811	170.112137	4.076326
1.014943	171.564643	4.081331
1.047477	188.026347	4.086336
0.857828	184.149376	4.091341
0.989654	191.366408	4.096346
1.083745	196.474989	4.101350
1.192559	192.662148	4.106355
0.716991	196.168577	4.111360
1.326403	192.138148	4.116365
0.948250	194.982480	4.121370
0.823071	188.086045	4.126374
1.239443	197.968997	4.131379
0.731890	199.578528	4.136384
1.485273	201.479179	4.141389
1.285960	202.363458	4.146394
1.154765	181.633596	4.151398
0.924304	177.120628	4.156403
0.739696	193.973877	4.161408
1.338391	192.156196	4.166413
1.190661	200.304769	4.171418
1.254392	206.152864	4.176422
1.433150	177.003589	4.181427
0.468217	190.165044	4.186432
1.037253	190.893641	4.191437
1.147434	205.407791	4.196442
1.382998	205.888820	4.201446
1.213225	214.925100	4.206451
1.203127	210.879937	4.211456
1.582264	207.377680	4.216461
1.181260	212.331999	4.221466
1.544174	209.185711	4.226470
1.491453	198.324446	4.231475
1.342209	209.723495	4.236480
1.401059	211.492184	4.241485
1.184773	205.901514	4.246490
1.345030	202.552928	4.251494
1.368703	196.741573	4.256499
1.369385	209.510841	4.261504
1.279898	203.039530	4.266509
1.330164	200.923083	4.271514
1.126445	212.626019	4.276518
1.362316	204.035378	4.281523
1.053701	193.314173	4.286528
1.210366	199.551299	4.291533
1.200741	207.538244	4.296538
1.404838	209.799197	4.301542
1.623225	210.807717	4.306547
1.604021	220.559334	4.311552
1.499598	204.845331	4.316557
1.055631	213.699519	4.321562
1.178969	216.565853	4.326566
1.549789	217.696971	4.331571
1.541241	225.326513	4.336576
1.612780	210.739379	4.341581
1.302847	227.192607	4.346586
1.509530	226.493253	4.351590
1.812867	234.889514	4.356595
1.968472	241.458712	4.361600
1.887046	223.729387	4.366605
1.658564	214.622750	4.371610
1.323577	211.664896	4.376614
1.727520	222.533322	4.381619
1.452782	226.457823	4.386624
1.727211	227.337808	4.391629
1.789564	233.681494	4.396634
1.923002	239.094848	4.401638
2.175171	217.287399	4.406643
1.966803	226.471536	4.411648
1.858345	224.519928	4.416653
1.642174	208.553182	4.421658
1.789865	206.395576	4.426662
1.544693	206.321986	4.431667
1.507896	215.319125	4.436672
1.941035	215.735836	4.441677
1.854392	233.322330	4.446682
1.638498	223.311299	4.451686
2.000181	225.220154	4.456691
1.957415	243.896663	4.461696
2.168088	225.358820	4.466701
1.830097	211.333234	4.471706
1.625799	210.845934	4.476710
2.003268	227.401919	4.481715
2.137167	231.161322	4.486720
1.932226	229.734032	4.491725
1.830694	220.476286	4.496730
1.804991	236.568728	4.501734
1.989209	232.614177	4.506739
1.847273	236.764559	4.511744
2.323382	258.453540	4.516749
2.258536	249.070734	4.521754
1.758526	239.565100	4.526758
1.972764	233.792384	4.531763
2.025450	242.352601	4.536768
2.441399	237.899917	4.541773
2.091373	245.933269	4.546778
2.108478	237.324205	4.551782
2.379616	232.675252	4.556787
1.953832	222.581111	4.561792
1.522780	220.788573	4.566797
1.776785	246.559042	4.571802
2.044441	242.403252	4.576806
1.986688	246.815174	4.581811
1.972835	242.720309	4.586816
2.054304	239.861936	4.591821
2.043256	239.487230	4.596826
2.120709	235.062861	4.601830
2.488535	236.907660	4.606835
2.495853	248.229564	4.611840
2.395107	241.922386	4.616845
2.567441	244.501037	4.621850
2.304847	255.205764	4.626854
2.492123	246.619677	4.631859
2.246621	248.956018	4.636864
2.375088	242.141259	4.641869
2.167942	250.109566	4.646874
1.875131	238.070926	4.651878
2.102936	240.110428	4.656883
1.912751	246.923922	4.661888
1.988932	239.326877	4.666893
2.341192	259.019694	4.671898
2.355029	276.399522	4.676902
2.514993	267.760025	4.681907
2.269019	284.836711	4.686912
2.280885	269.504364	4.691917
1.930634	269.592868	4.696922
2.255101	267.330963	4.701926
2.649682	272.624024	4.706931
2.278430	275.844098	4.711936
2.768228	273.288893	4.716941
2.314275	276.869214	4.721946
2.176397	279.649783	4.726950
2.622163	276.556678	4.731955
2.338560	274.787418	4.736960
2.619706	270.910660	4.741965
2.506048	275.881050	4.746970
2.270469	286.451798	4.751974
2.545359	284.722640	4.756979
2.538415	301.078422	4.761984
2.711992	299.542798	4.766989
2.966538	305.053859	4.771994
2.370642	293.251623	4.776998
3.004967	295.150948	4.782003
2.610060	295.324868	4.787008
2.739902	289.613927	4.792013
2.845709	286.215226	4.797018
2.421902	284.916738	4.802022
2.826419	284.082383	4.807027
2.815891	298.536953	4.812032
3.108568	301.414881	4.817037
2.884867	292.074085	4.822042
2.634338	279.714796	4.827046
2.859158	282.453581	4.832051
2.653029	288.562065	4.837056
2.970143	284.694356	4.842061
2.879162	282.397218	4.847066
2.766364	284.470321	4.852070
2.484036	284.912728	4.857075
2.790528	302.875330	4.862080
2.812400	293.418775	4.867085
3.009928	315.198564	4.872090
3.090301	314.000553	4.877094
3.011764	320.260811	4.882099
2.938411	321.853750	4.887104
3.050240	320.804544	4.892109
3.255241	320.425704	4.897114
3.063329	306.267763	4.902118
3.079348	287.512214	4.907123
2.445009	290.289292	4.912128
2.741475	302.406276	4.917133
2.702660	299.160317	4.922138
2.872186	308.544679	4.927142
2.986875	312.405538	4.932147
2.638784	313.680525	4.937152
3.046843	312.261140	4.942157
2.961227	313.628010	4.947162
2.481334	322.724086	4.952166
3.030281	307.684254	4.957171
2.682187	323.306690	4.962176
3.154090	322.368065	4.967181
3.130414	335.388598	4.972186
3.295574	341.826920	4.977190
3.222873	334.462203	4.982195
2.995714	332.273591	4.987200
3.305083	341.734210	4.992205
3.512484	339.950592	4.997210
3.333248	337.502780	5.002214
3.453602	338.200857	5.007219
3.029602	324.442831	5.012224
3.344981	331.172421	5.017229
3.114062	338.505110	5.022234
3.406892	342.107852	5.027238
3.614659	339.132004	5.032243
3.129884	326.616736	5.037248
3.267319	319.282316	5.042253
3.186660	340.231843	5.047258
3.474397	337.846461	5.052262
3.395299	345.593088	5.057267
3.251246	351.036749	5.062272
3.165119	352.859305	5.067277
3.369563	342.486610	5.072282
3.426458	340.207153	5.077286
3.372721	334.389893	5.082291
3.221329	342.664243	5.087296
3.628824	332.858820	5.092301
3.457341	338.425892	5.097306
3.348732	344.031312	5.102310
3.664260	341.931783	5.107315
3.483735	340.480322	5.112320
3.562914	332.805389	5.117325
3.402773	334.574863	5.122330
3.522853	348.117913	5.127334
3.616623	334.271453	5.132339
3.054125	345.172406	5.137344
3.519361	339.995102	5.142349
3.426833	348.009435	5.147354
3.441573	336.929054	5.152358
3.541833	336.198842	5.157363
3.239947	342.685933	5.162368
3.464042	350.668070	5.167373
3.754842	362.448236	5.172378
3.825165	364.683469	5.177382
3.846840	349.152108	5.182387
3.344156	345.921332	5.187392
3.701102	356.925972	5.192397
3.757039	362.791496	5.197402
3.499536	374.702336	5.202406
3.884510	368.102430	5.207411
3.754053	380.674296	5.212416
3.725926	379.083895	5.217421
3.819715	388.158015	5.222426
3.679004	378.974326	5.227430
3.868255	375.048306	5.232435
3.487955	389.423384	5.237440
3.837029	381.437155	5.242445
3.721923	381.906191	5.247450
3.657168	376.846153	5.252454
3.763619	385.541802	5.257459
3.804073	377.255160	5.262464
3.935877	373.354221	5.267469
3.877575	372.859166	5.272474
3.856402	376.032063	5.277478
4.021461	374.974057	5.282483
3.982646	376.509203	5.287488
3.862428	376.117413	5.292493
3.957058	382.960458	5.297498
4.021749	383.213123	5.302502
4.172307	374.484061	5.307507
4.091386	383.399305	5.312512
4.189855	384.107709	5.317517
4.064472	380.704770	5.322522
3.722801	383.723453	5.327526
4.079492	373.440020	5.332531
3.713200	385.077511	5.337536
3.959368	373.641579	5.342541
4.070948	376.159259	5.347546
3.920097	381.062920	5.352550
4.233570	381.440710	5.357555
3.902647	388.573298	5.362560
4.002245	371.315658	5.367565
3.905183	387.474411	5.372570
3.959216	386.344381	5.377574
4.276422	391.901748	5.382579
4.333872	396.113540	5.387584
4.504643	388.951259	5.392589
4.236775	382.780065	5.397594
4.051164	385.209824	5.402598
3.947955	376.257703	5.407603
4.085436	390.849601	5.412608
4.351445	399.712160	5.417613
4.208990	409.426550	5.422618
4.082664	417.014483	5.427622
4.418556	411.473273	5.432627
4.349545	417.003313	5.437632
4.285989	404.070310	5.442637
4.466691	414.054304	5.447642
4.032600	412.075980	5.452646
4.522510	408.721413	5.457651
4.140932	424.074723	5.462656
3.943470	424.378998	5.467661
4.087493	419.176415	5.472666
3.768794	425.319143	5.477670
4.130716	411.891399	5.482675
4.039658	433.616540	5.487680
4.273512	434.463484	5.492685
4.261967	443.447211	5.497690
4.050525	440.390660	5.502694
4.593996	441.625564	5.507699
4.220757	449.761318	5.512704
4.474000	443.543841	5.517709
4.690702	447.112228	5.522714
4.326759	452.956013	5.527718
4.407901	451.550684	5.532723
4.294111	448.750486	5.537728
4.592000	448.197849	5.542733
4.457671	451.655147	5.547738
4.632619	457.288630	5.552742
4.514788	444.356177	5.557747
4.649767	461.143981	5.562752
4.838488	458.979659	5.567757
4.891162	452.257935	5.572762
4.646833	440.381900	5.577766
4.513005	452.005394	5.582771
4.834494	453.307369	5.587776
5.054309	449.609210	5.592781
4.843555	440.409337	5.597786
4.414903	451.225500	5.602790
4.869511	444.943965	5.607795
4.647248	455.413675	5.612800
4.811675	457.226901	5.617805
4.832241	449.111915	5.622810
4.380440	463.127825	5.627814
4.801429	454.554895	5.632819
4.825879	469.242597	5.637824
4.780915	468.618461	5.642829
4.963269	472.913125	5.647834
4.583838	464.930233	5.652838
4.971214	470.313839	5.657843
4.965463	484.861126	5.662848
4.988899	480.367476	5.667853
4.531000	469.834715	5.672858
4.626091	483.312560	5.677862
4.892328	488.644072	5.682867
4.808353	491.986902	5.687872
5.099710	477.107863	5.692877
4.792781	476.250282	5.697882
4.822020	491.331647	5.702886
5.189101	473.599049	5.707891
4.817213	490.841106	5.712896
4.754986	493.105761	5.717901
4.658390	486.883135	5.722906
5.175215	494.388601	5.727910
5.071122	485.500592	5.732915
4.667563	490.169708	5.737920
4.851319	484.689918	5.742925
4.833473	478.678039	5.747930
4.850500	501.743044	5.752934
5.238963	510.898375	5.757939
5.206446	528.070777	5.762944
4.986090	526.087602	5.767949
5.038636	531.035540	5.772954
5.349582	525.683099	5.777958
5.292592	519.056817	5.782963
5.262403	538.438489	5.787968
5.038853	531.095055	5.792973
5.110106	524.273841	5.797978
5.042384	520.201813	5.802982
4.887832	521.150536	5.807987
5.098671	526.910217	5.812992
5.302761	523.772156	5.817997
5.459153	522.779996	5.823002
5.340038	526.770904	5.828006
5.330153	518.258882	5.833011
5.056637	521.916386	5.838016
5.557105	523.607889	5.843021
5.108583	521.177219	5.848026
5.186500	516.690242	5.853030
5.570155	516.875993	5.858035
5.335692	514.273408	5.863040
5.595182	515.167521	5.868045
5.470972	509.030448	5.873050
5.450825	527.222310	5.878054
5.547439	511.299751	5.883059
5.228783	520.240154	5.888064
5.256304	521.349988	5.893069
5.011470	524.262423	5.898074
4.947411	524.839149	5.903078
5.582810	528.953102	5.908083
5.254709	529.892522	5.913088
5.423227	539.214839	5.918093
5.628899	539.415697	5.923098
5.745945	545.447889	5.928102
5.857671	535.633895	5.933107
5.182896	529.857232	5.938112
5.461054	540.078557	5.943117
5.509434	548.151594	5.948122
5.467420	545.288314	5.953126
5.818313	554.633975	5.958131
5.931202	556.126607	5.963136
5.959572	542.883309	5.968141
5.864796	528.164814	5.973146
5.289364	518.170977	5.978150
5.716076	524.517022	5.983155
5.670191	546.006365	5.988160
5.778290	549.975911	5.993165
5.674506	550.499317	5.998170
5.759930	559.182261	6.003174
5.743844	555.920455	6.008179
5.667157	551.089147	6.013184
5.893713	554.709798	6.018189
5.815135	556.567732	6.023194
5.779687	553.637264	6.028198
6.005148	549.675224	6.033203
5.751705	532.161519	6.038208
5.627093	524.083211	6.043213
5.640579	533.069759	6.048218
5.494378	550.369990	6.053222
5.846852	547.758705	6.058227
5.553092	554.357505	6.063232
5.843786	542.080625	6.068237
5.666298	551.005018	6.073242
5.663473	558.568962	6.078246
5.872533	555.869497	6.083251
6.067795	562.602069	6.088256
5.853216	557.283384	6.093261
5.644973	564.039031	6.098266
5.354431	562.894108	6.103270
6.015643	556.905044	6.108275
5.784070	561.396293	6.113280
5.674604	554.911856	6.118285
5.546325	554.619755	6.123290
5.815772	549.034523	6.128294
5.828476	548.370072	6.133299
5.578864	567.445895	6.138304
5.422316	548.467460	6.143309
5.431466	557.013738	6.148314
5.432232	565.193508	6.153318
5.705768	555.325433	6.158323
5.536003	561.792656	6.163328
5.845877	563.483893	6.168333
5.890157	565.657260	6.173338
5.684282	560.856768	6.178342
5.974770	550.484513	6.183347
5.442449	567.603800	6.188352
6.024335	567.377847	6.193357
5.900006	568.112423	6.198362
5.900695	560.154076	6.203366
6.011875	550.849239	6.208371
5.764524	562.034986	6.213376
5.591076	553.682767	6.218381
5.699648	556.934992	6.223386
5.313330	559.064776	6.228390
6.106544	574.597815	6.233395
5.835433	564.092232	6.238400
5.944168	562.317100	6.243405
5.833626	558.099317	6.248410
5.758387	562.228800	6.253414
5.677918	551.013841	6.258419
5.665420	557.616183	6.263424
5.476565	560.815941	6.268429
5.557559	584.814758	6.273434
5.835323	591.172423	6.278438
6.102343	591.815493	6.283443
5.589803	592.669768	6.288448
6.345404	584.232670	6.293453
6.166345	571.951311	6.298458
5.788630	570.925962	6.303462
6.125485	555.324451	6.308467
5.972125	566.577838	6.313472
5.756157	563.362578	6.318477
6.273885	556.755749	6.323482
5.683892	564.359111	6.328486
5.781400	557.281373	6.333491
5.764926	563.852705	6.338496
5.901092	557.807253	6.343501
5.507700	550.254899	6.348506
5.760736	563.798959	6.353510
6.008002	554.528754	6.358515
5.817031	564.756784	6.363520
5.863957	561.646265	6.368525
6.183909	556.357144	6.373530
5.654874	573.277887	6.378534
5.748424	556.579050	6.383539
5.766649	566.993901	6.388544
5.562941	556.360078	6.393549
5.616075	562.329930	6.398554
5.790793	560.663961	6.403558
5.667966	554.980469	6.408563
5.868310	560.387221	6.413568
5.656409	555.792344	6.418573
5.626680	557.265430	6.423578
5.739955	561.997936	6.428582
6.222888	560.617656	6.433587
5.647621	571.726581	6.438592
5.696686	568.880408	6.443597
6.111551	563.854802	6.448602
5.781622	570.111717	6.453606
5.891339	573.223167	6.458611
5.956417	572.570877	6.463616
5.655732	562.249840	6.468621
5.647328	564.881104	6.473626
5.460554	558.869780	6.478630
5.850260	563.913058	6.483635
5.807538	565.948277	6.488640
5.779005	561.146695	6.493645
6.326910	556.628507	6.498650
5.806616	563.174178	6.503654
5.672371	559.810055	6.508659
5.760209	563.876875	6.513664
5.688840	566.606252	6.518669
5.815634	563.923241	6.523674
5.532985	574.087994	6.528678
5.743410	562.625962	6.533683
5.471150	565.654223	6.538688
5.371281	562.159715	6.543693
5.635777	569.175443	6.548698
5.539926	561.506629	6.553702
5.430202	571.986332	6.558707
5.544045	573.308721	6.563712
5.515859	589.336828	6.568717
5.853021	585.063600	6.573722
5.450719	596.750018	6.578726
5.808143	592.057299	6.583731
5.967747	592.891956	6.588736
5.941843	599.726307	6.593741
5.872281	597.166505	6.598746
5.615265	602.278981	6.603750
5.773690	588.326205	6.608755
5.838255	607.575199	6.613760
5.878968	601.766992	6.618765
6.073861	602.045600	6.623770
5.508037	588.010161	6.628774
5.944717	582.760837	6.633779
5.679805	596.330139	6.638784
5.775833	598.188920	6.643789
5.657434	596.633640	6.648794
5.475659	593.566433	6.653798
6.062779	591.466287	6.658803
6.000277	595.422305	6.663808
5.946094	595.378418	6.668813
5.778190	578.945238	6.673818
5.707631	567.377899	6.678822
5.787069	558.355138	6.683827
5.515064	561.315282	6.688832
5.872961	571.524438	6.693837
5.670669	597.313383	6.698842
5.742486	600.793178	6.703846
5.573583	599.260154	6.708851
5.791015	597.900561	6.713856
5.805079	592.625769	6.718861
5.850885	593.124259	6.723866
5.591177	595.940605	6.728870
5.902455	587.218012	6.733875
5.834028	597.281969	6.738880
5.790269	590.688691	6.743885
5.650510	596.953851	6.748890
5.795740	605.861153	6.753894
6.152142	587.100292	6.758899
5.549676	601.170428	6.763904
5.672233	599.489890	6.768909
5.880803	607.094891	6.773914
5.795566	618.084985	6.778918
5.993093	595.248636	6.783923
5.853822	605.236104	6.788928
5.854781	595.592607	6.793933
6.112870	583.630178	6.798938
5.588218	573.192534	6.803942
6.131217	572.919534	6.808947
5.548416	568.988946	6.813952
5.414584	568.185529	6.818957
5.717081	577.230105	6.823962
5.706636	601.120243	6.828966
5.656456	596.606857	6.833971
5.815750	598.230143	6.838976
5.946359	586.581105	6.843981
5.863742	593.919498	6.848986
5.487865	617.203907	6.853990
5.522402	598.120728	6.858995
5.704366	606.833522	6.864000
5.866060	595.577724	6.869005
5.955678	595.354883	6.874010
5.753910	593.256551	6.879014
6.153677	593.574803	6.884019
5.849642	600.442488	6.889024
6.133383	598.700487	6.894029
6.230534	581.963637	6.899034
5.553070	581.533008	6.904038
5.866051	566.405539	6.909043
5.537391	572.653661	6.914048
5.739425	565.937001	6.919053
5.631864	559.116316	6.924058
5.528000	585.579682	6.929062
5.603636	592.836773	6.934067
5.705746	596.317777	6.939072
5.696933	593.192588	6.944077
6.338508	593.690593	6.949082
5.879036	593.185858	6.954086
5.857524	580.295878	6.959091
5.805568	576.241356	6.964096
5.477993	574.789212	6.969101
5.543401	578.099679	6.974106
5.624179	592.226887	6.979110
6.026532	590.221107	6.984115
6.003737	594.256987	6.989120
5.632389	594.102726	6.994125
5.659463	595.252596	6.999130
5.805890	609.678956	7.004134
5.879118	605.603345	7.009139
5.723594	600.692409	7.014144
5.975882	594.013999	7.019149
6.042396	596.923634	7.024154
5.795491	588.628228	7.029158
6.118853	576.259202	7.034163
5.991249	566.017985	7.039168
5.765965	572.137146	7.044173
5.443781	562.518162	7.049178
5.382397	566.691332	7.054182
5.770545	576.008553	7.059187
5.880469	602.073851	7.064192
6.330714	595.717208	7.069197
6.004236	579.213745	7.074202
5.401792	576.996545	7.079206
6.118846	563.533660	7.084211
5.520766	565.859844	7.089216
5.657740	559.227044	7.094221
5.583279	568.553423	7.099226
5.549233	558.080887	7.104230
6.018730	577.056139	7.109235
5.716317	577.960732	7.114240
5.412600	586.577473	7.119245
5.644699	589.768052	7.124250
5.526913	603.857839	7.129254
5.731260	596.825075	7.134259
5.752197	605.360651	7.139264
5.891244	600.688626	7.144269
6.101005	592.464062	7.149274
5.684504	601.438736	7.154278
5.883165	596.327104	7.159283
5.758944	601.041647	7.164288
5.751376	611.967895	7.169293
5.730542	605.383154	7.174298
5.871440	612.886673	7.179302
5.514413	611.753916	7.184307
6.030005	608.700609	7.189312
5.965689	602.653838	7.194317
6.531276	602.265226	7.199322
5.735112	585.017055	7.204326
5.565721	581.035313	7.209331
5.835770	585.694661	7.214336
5.817918	553.554171	7.219341
5.488481	560.341091	7.224346
5.495701	569.898448	7.229350
5.599369	583.131375	7.234355
5.966695	592.122429	7.239360
5.471667	594.812410	7.244365
5.579597	605.093480	7.249370
5.435976	601.590802	7.254374
5.751824	602.198672	7.259379
5.764198	592.791550	7.264384
5.695868	593.784139	7.269389
5.755207	600.871176	7.274394
5.415858	609.289891	7.279398
5.953899	602.822346	7.284403
5.786321	590.993397	7.289408
5.794553	600.929257	7.294413
5.912366	594.325358	7.299418
5.757974	593.753929	7.304422
5.809455	603.823430	7.309427
5.778599	595.848179	7.314432
5.970121	589.440566	7.319437
6.121350	598.504036	7.324442
6.133847	597.516609	7.329446
6.308189	586.540594	7.334451
6.020170	589.219944	7.339456
5.717367	571.908313	7.344461
5.720226	553.968151	7.349466
5.294023	576.367860	7.354470
5.844531	594.677910	7.359475
5.714886	596.455396	7.364480
5.609230	598.540877	7.369485
5.769781	592.523052	7.374490
5.967145	604.676975	7.379494
6.057365	598.442967	7.384499
6.212898	598.435359	7.389504
5.600823	573.197111	7.394509
6.044770	572.237045	7.399514
5.870029	571.262113	7.404518
5.544786	562.770313	7.409523
5.862552	561.429758	7.414528
5.542833	564.647689	7.419533
5.914071	569.305505	7.424538
5.569358	568.320085	7.429542
5.508184	568.351051	7.434547
5.535424	593.474493	7.439552
5.628513	588.312038	7.444557
5.920032	589.765189	7.449562
5.822883	605.735254	7.454566
5.762650	596.372488	7.459571
5.594478	596.280843	7.464576
5.488862	598.944753	7.469581
5.689020	590.927382	7.474586
5.733028	603.711423	7.479590
6.017661	586.274977	7.484595
5.944458	594.330838	7.489600
5.546718	601.334963	7.494605
6.229669	604.802659	7.499610
5.785691	595.803232	7.504614
5.913540	595.984690	7.509619
5.810261	598.931165	7.514624
5.867437	608.340097	7.519629
5.645137	602.926184	7.524634
5.882819	596.702240	7.529638
5.783834	606.849291	7.534643
5.853604	600.363235	7.539648
5.823354	607.724946	7.544653
6.004431	592.281541	7.549658
5.962013	602.461763	7.554662
5.803628	574.473610	7.559667
5.497331	574.887921	7.564672
5.734871	583.860856	7.569677
5.736065	580.554457	7.574682
5.884497	597.680855	7.579686
5.910713	587.699130	7.584691
5.987942	601.466929	7.589696
5.610167	587.463852	7.594701
5.932204	580.609161	7.599706
5.866597	571.101186	7.604710
5.687246	556.711164	7.609715
5.659514	572.688665	7.614720
5.957865	562.834934	7.619725
5.977799	555.359400	7.624730
5.640199	561.765665	7.629734
5.563241	561.486789	7.634739
5.735089	564.489213	7.639744
5.729411	575.739511	7.644749
5.958040	576.538886	7.649754
5.663225	575.812387	7.654758
5.963126	570.939756	7.659763
5.874510	564.738965	7.664768
5.471646	562.931071	7.669773
5.728283	571.019035	7.674778
5.756955	588.234076	7.679782
6.409516	585.155573	7.684787
5.795078	578.478232	7.689792
5.382345	565.168996	7.694797
5.944477	556.623001	7.699802
5.919431	562.476136	7.704806
5.632985	552.892294	7.709811
5.585750	556.346864	7.714816
5.678536	559.612747	7.719821
6.004932	565.913726	7.724826
5.719320	573.235636	7.729830
5.662649	560.068728	7.734835
5.904177	567.143499	7.739840
5.825248	587.063083	7.744845
5.875394	569.510610	7.749850
5.332078	572.053673	7.754854
6.102362	584.399802	7.759859
5.752135	576.468557	7.764864
5.691149	565.696600	7.769869
5.886643	574.627247	7.774874
5.721604	587.320130	7.779878
6.085795	585.443289	7.784883
5.989150	566.225749	7.789888
5.495874	569.129821	7.794893
5.646860	565.490956	7.799898
5.515370	568.152625	7.804902
5.859711	581.051480	7.809907
6.013660	590.774126	7.814912
5.759342	586.060460	7.819917
5.920957	574.605794	7.824922
5.555873	568.467855	7.829926
5.984855	581.576283	7.834931
6.097401	568.606938	7.839936
5.865692	566.612512	7.844941
6.230963	566.286996	7.849946
5.873723	564.519313	7.854950
6.039451	565.319018	7.859955
6.032127	558.663399	7.864960
5.602064	565.556236	7.869965
5.866844	567.999400	7.874970
5.634170	572.246951	7.879974
5.806185	565.433831	7.884979
5.766225	558.502428	7.889984
5.981446	558.581641	7.894989
6.027696	563.825520	7.899994
5.665634	562.988982	7.904998
5.932694	558.472808	7.910003
5.823862	566.007411	7.915008
5.541078	563.943782	7.920013
5.767249	550.299794	7.925018
5.660410	565.971498	7.930022
5.954358	563.745277	7.935027
6.135145	570.416512	7.940032
5.936130	561.595941	7.945037
5.955236	560.475222	7.950042
5.924351	563.061760	7.955046
6.177638	549.451276	7.960051
5.804491	548.517123	7.965056
5.665564	528.977395	7.970061
5.895236	533.296321	7.975066
5.497325	536.735534	7.980070
5.929081	545.002121	7.985075
5.698853	545.545140	7.990080
5.811457	548.106582	7.995085
5.725712	534.685621	8.000090
5.758687	550.481995	8.005094
6.031185	549.200421	8.010099
5.675767	534.473000	8.015104
5.601991	529.373163	8.020109
5.869615	547.136639	8.025126
5.791853	557.274283	8.030144
5.938119	544.313529	8.035162
5.757557	541.070604	8.040179
5.833127	536.032832	8.045197
5.773999	526.838395	8.050214
5.613005	532.097209	8.055232
5.956056	551.625515	8.060250
5.951001	535.216418	8.065267
5.578016	542.154738	8.070285
5.899239	537.529041	8.075302
5.928519	559.069465	8.080320
6.046030	548.665634	8.085338
5.749555	543.325041	8.090355
5.336971	532.689000	8.095373
5.664925	544.569186	8.100390
5.735535	549.589180	8.105408
6.034573	570.629322	8.110426
6.016483	560.298079	8.115443
5.784810	556.602070	8.120461
5.929001	556.006539	8.125478
5.567354	558.484486	8.130496
5.776527	559.579372	8.135514
5.650481	554.489003	8.140531
5.505028	556.231749	8.145549
5.661175	558.503779	8.150566
5.722752	558.453000	8.155584
5.884424	558.077471	8.160602
5.779088	554.991273	8.165619
5.642320	564.558173	8.170637
6.061508	566.966130	8.175654
6.120712	571.783331	8.180672
5.898190	563.442293	8.185690
6.067387	555.797504	8.190707
5.817255	557.497324	8.195725
5.752133	558.339169	8.200742
5.933745	564.312590	8.205760
6.276029	572.286344	8.210778
6.015887	559.902779	8.215795
6.048557	565.180772	8.220813
6.053696	565.436312	8.225830
6.048109	562.232072	8.230848
6.046295	551.721604	8.235866
6.174983	553.950049	8.240883
5.963896	557.214774	8.245901
6.202943	552.787656	8.250918
5.957628	553.229143	8.255936
6.171840	562.585904	8.260954
5.968415	559.329237	8.265971
5.675074	569.270177	8.270989
5.969067	557.256863	8.276006
5.809270	562.292107	8.281024
5.896032	568.592661	8.286042
6.104524	574.534287	8.291059
6.332762	581.397282	8.296077
6.266968	565.135664	8.301094
5.940281	568.690408	8.306112
5.887978	555.513686	8.311130
5.997842	558.920907	8.316147
6.133945	579.164814	8.321165
6.292801	574.472648	8.326182
5.493440	566.777222	8.331200
6.152921	574.857683	8.336218
6.193665	583.799211	8.341235
6.340274	575.725845	8.346253
6.266810	576.806426	8.351270
6.244951	581.725592	8.356288
6.241498	571.789387	8.361306
6.409652	565.726654	8.366323
6.050889	571.463847	8.371341
5.940305	558.207204	8.376358
5.920217	568.707007	8.381376
6.065373	568.240229	8.386394
6.261059	580.550000	8.391411
6.158638	594.348932	8.396429
6.343794	589.231333	8.401446
6.382088	572.316011	8.406464
6.000184	557.478036	8.411482
6.065533	559.341232	8.416499
6.057800	560.025295	8.421517
6.209938	577.909909	8.426534
6.255130	590.285593	8.431552
6.107967	590.167951	8.436570
6.434803	585.940154	8.441587
6.404682	583.346150	8.446605
6.169215	561.553382	8.451622
6.000488	572.488500	8.456640
6.411757	595.799560	8.461658
6.493679	577.003654	8.466675
6.116065	570.290401	8.471693
6.161608	565.283659	8.476710
5.906385	566.429997	8.481728
5.967576	578.727747	8.486746
5.931231	583.337751	8.491763
6.189683	579.076482	8.496781
6.150261	578.176907	8.501798
6.373746	585.565394	8.506816
6.457863	587.925301	8.511834
6.674948	598.016118	8.516851
6.296278	602.440027	8.521869
6.415699	593.275187	8.526886
6.352975	594.297804	8.531904
6.083831	595.553413	8.536922
5.752137	601.608525	8.541939
5.811601	598.400023	8.546957
6.167216	590.308544	8.551974
6.203961	600.856840	8.556992
6.485480	597.254622	8.562010
6.571614	601.644725	8.567027
6.130947	593.814532	8.572045
6.425702	595.592096	8.577063
6.176478	589.874456	8.582080
5.842342	587.228741	8.587098
6.126380	601.110343	8.592115
6.245236	612.831669	8.597133
6.341092	618.387473	8.602151
6.756498	618.582103	8.607168
6.701516	635.852609	8.612186
6.838314	614.031314	8.617203
6.343964	606.782222	8.622221
6.435510	594.071172	8.627239
6.522121	598.693238	8.632256
6.315007	594.346825	8.637274
6.399343	594.150186	8.642291
6.279212	599.491034	8.647309
6.580895	613.345228	8.652327
6.452300	613.070116	8.657344
6.308329	610.658769	8.662362
6.718114	599.975545	8.667379
5.973569	601.104636	8.672397
6.851270	619.056075	8.677415
6.523674	623.351100	8.682432
6.513710	615.333109	8.687450
6.467432	612.738129	8.692467
6.332730	624.897158	8.697485
6.252115	632.997117	8.702503
6.595160	623.605084	8.707520
6.295302	625.613763	8.712538
6.608767	628.929096	8.717555
6.480681	639.328705	8.722573
6.520671	624.296461	8.727591
6.664571	630.818657	8.732608
6.502782	626.789193	8.737626
6.669104	629.225761	8.742643
6.667975	635.164164	8.747661
6.808827	617.054504	8.752679
6.641343	622.609052	8.757696
6.336194	629.455310	8.762714
6.723924	625.164595	8.767731
6.477640	628.344518	8.772749
6.628779	630.576153	8.777767
6.708972	622.349299	8.782784
6.646907	626.188415	8.787802
6.785686	626.480915	8.792819
6.402739	623.395213	8.797837
6.735498	617.188154	8.802855
6.708504	632.112732	8.807872
6.755854	640.263976	8.812890
6.653225	613.682146	8.817907
6.488268	617.314485	8.822925
6.312642	614.540130	8.827943
6.650059	616.854542	8.832960
6.664138	634.404426	8.837978
6.951030	622.979036	8.842995
6.571257	627.482648	8.848013
6.442189	627.606556	8.853031
6.614053	625.460770	8.858048
6.594486	636.125463	8.863066
6.703975	632.790402	8.868083
6.483721	631.820627	8.873101
6.594723	633.187993	8.878119
6.668190	632.290326	8.883136
6.660514	635.430721	8.888154
6.810941	631.745749	8.893171
6.713460	633.290750	8.898189
6.787606	627.867132	8.903207
6.731798	616.503005	8.908224
6.475253	626.645441	8.913242
6.723276	623.562438	8.918259
6.246836	619.381860	8.923277
6.264594	628.177733	8.928295
6.586050	632.420709	8.933312
6.642208	651.390069	8.938330
6.804123	657.641239	8.943347
6.717884	658.367703	8.948365
6.959366	654.703498	8.953383
6.915186	663.873044	8.958400
6.657661	670.096208	8.963418
7.306856	661.022292	8.968435
7.148545	634.553348	8.973453
6.898781	631.242523	8.978471
6.853232	638.671460	8.983488
6.716924	629.734749	8.988506
6.564814	615.173547	8.993523
6.765404	633.408323	8.998541
7.027636	655.850764	9.003559
6.744384	633.651201	9.008576
7.158513	654.857247	9.013594
6.606580	639.475150	9.018611
6.844850	642.585137	9.023629
6.725877	646.808003	9.028647
7.014379	654.563663	9.033664
7.108810	661.009220	9.038682
6.931156	644.454151	9.043699
7.000150	642.067930	9.048717
7.090969	649.217592	9.053735
6.871069	630.860205	9.058752
6.943348	636.214438	9.063770
6.987966	631.337233	9.068787
7.109375	633.150532	9.073805
7.169574	631.691678	9.078823
7.057270	621.675416	9.083840
6.862581	627.752771	9.088858
6.786048	625.217208	9.093875
6.549210	628.709882	9.098893
6.550861	641.244545	9.103911
7.189770	649.344683	9.108928
6.989580	658.670199	9.113946
6.668249	663.644981	9.118963
6.800018	661.841976	9.123981
6.800972	668.122406	9.128999
6.626890	665.231567	9.134016
6.619720	662.835984	9.139034
6.743592	660.281075	9.144051
7.355796	660.519352	9.149069
6.810929	674.488796	9.154087
7.057781	656.012522	9.159104
6.719476	666.675490	9.164122
6.697350	668.500803	9.169139
7.222733	673.747795	9.174157
7.081384	679.761544	9.179175
7.294319	684.061732	9.184192
7.089030	680.764114	9.189210
7.325344	676.348041	9.194227
7.016500	668.125227	9.199245
6.700736	662.439024	9.204263
6.972265	669.524291	9.209280
6.783161	680.174913	9.214298
7.175056	684.517464	9.219315
7.180866	689.479524	9.224333
7.049490	685.470703	9.229351
7.180876	686.792193	9.234368
7.235199	689.784780	9.239386
7.296959	686.912827	9.244403
7.323467	695.804813	9.249421
6.985909	690.710383	9.254439
7.105639	690.617618	9.259456
7.326860	692.536456	9.264474
7.191009	686.403462	9.269491
7.287139	684.234461	9.274509
7.391304	691.509769	9.279527
7.703831	686.393132	9.284544
7.402592	684.768451	9.289562
7.444602	663.813973	9.294579
7.288549	660.630150	9.299597
6.937369	664.094295	9.304615
7.228373	644.533966	9.309632
7.241704	673.708662	9.314650
7.250691	669.405438	9.319667
7.234687	664.816537	9.324685
6.974469	677.661385	9.329703
7.272867	678.055143	9.334720
7.293892	685.398410	9.339738
7.296367	693.187873	9.344755
7.559501	676.113848	9.349773
7.360046	694.497959	9.354791
7.353232	682.342855	9.359808
7.450673	689.632361	9.364826
7.312169	680.208178	9.369843
7.276825	674.399561	9.374861
7.292623	669.315827	9.379879
7.354129	664.285946	9.384896
7.338597	682.191207	9.389914
7.369915	678.071954	9.394931
7.588064	681.148863	9.399949
7.241349	684.523511	9.404967
7.248436	681.827985	9.409984
7.264735	683.614771	9.415002
7.176762	686.648881	9.420019
7.401527	692.418996	9.425037
7.429195	689.061033	9.430055
7.743563	693.236411	9.435072
7.604335	688.405708	9.440090
7.266487	688.200502	9.445107
7.414133	684.281178	9.450125
7.271146	688.643038	9.455143
7.363545	687.039611	9.460160
7.099804	693.775826	9.465178
7.395852	689.782378	9.470195
7.635550	687.233417	9.475213
7.383465	685.847223	9.480231
7.750481	677.018711	9.485248
7.507280	686.335607	9.490266
7.612521	690.390256	9.495283
7.397848	682.871132	9.500301
7.228078	687.753565	9.505319
7.263890	682.549807	9.510336
7.429184	684.317679	9.515354
7.291853	702.365115	9.520371
7.454407	690.482061	9.525389
7.047442	689.765439	9.530407
7.454470	687.078118	9.535424
7.594319	689.566109	9.540442
7.630844	696.315686	9.545459
7.565155	682.436372	9.550477
7.478744	688.508749	9.555495
7.514012	683.493138	9.560512
7.763532	687.046175	9.565530
7.692350	685.940758	9.570547
7.847927	684.310457	9.575565
7.518269	694.268696	9.580583
7.546779	697.903133	9.585600
7.438364	695.028597	9.590618
7.372339	694.058425	9.595635
7.684443	690.218005	9.600653
7.465131	691.953979	9.605671
7.696889	694.122999	9.610688
7.756106	685.248416	9.615706
7.566660	681.155902	9.620723
7.503433	688.662967	9.625741
7.925033	706.500938	9.630759
7.779881	697.292766	9.635776
7.996868	686.234231	9.640794
7.422323	697.477795	9.645811
8.187864	679.995012	9.650829
7.821492	698.525587	9.655847
7.709285	689.634555	9.660864
7.803574	693.115330	9.665882
7.853289	687.193851	9.670899
8.107412	697.126770	9.675917
7.998510	682.273081	9.680935
7.504943	684.642754	9.685952
7.664998	686.718424	9.690970
7.157893	684.484573	9.695987
7.529136	683.559247	9.701005
7.530427	694.731465	9.706023
7.680183	690.476122	9.711040
8.017436	714.027505	9.716058
7.813953	717.529743	9.721075
7.770412	694.574465	9.726093
7.384719	704.863862	9.731111
7.767912	709.042730	9.736128
8.072916	708.648728	9.741146
7.742565	717.748885	9.746163
7.954169	717.072535	9.751181
7.927121	730.169985	9.756199
7.793908	720.993874	9.761216
7.900287	723.008058	9.766234
7.665554	730.621129	9.771251
7.847850	737.468857	9.776269
7.956997	732.746183	9.781287
7.514987	734.892027	9.786304
7.713887	738.838610	9.791322
7.732438	732.444100	9.796339
7.718132	724.009817	9.801357
7.819122	729.419563	9.806375
7.717585	725.344689	9.811392
7.666988	721.663984	9.816410
7.556832	728.105294	9.821427
7.680533	722.948307	9.826445
7.641323	734.125672	9.831463
7.896242	747.940086	9.836480
8.287905	756.771765	9.841498
7.766131	758.320763	9.846515
8.235201	753.833140	9.851533
8.048969	755.679874	9.856551
8.115587	743.858885	9.861568
8.248660	727.046804	9.866586
7.755148	735.372503	9.871603
8.135137	734.231101	9.876621
7.785044	737.316901	9.881639
7.964991	742.002017	9.886656
8.150970	750.902815	9.891674
7.993899	746.080258	9.896691
8.242545	747.780730	9.901709
8.001445	753.912155	9.906727
7.933472	749.851311	9.911744
8.351938	749.549561	9.916762
8.194030	750.765347	9.921779
8.275220	730.218011	9.926797
8.287324	726.280825	9.931815
7.931757	728.439348	9.936832
7.992224	719.898042	9.941850
7.975208	731.147904	9.946867
8.564330	732.982726	9.951885
8.165300	732.002141	9.956903
7.986478	733.749437	9.961920
7.930117	717.817241	9.966938
8.150554	740.001602	9.971955
8.317210	744.160269	9.976973
8.081241	745.060863	9.981991
8.014507	760.742394	9.987008
8.229569	749.740225	9.992026
8.163591	751.241357	9.997043
8.247837	749.273193	10.002061
8.355261	757.016906	10.007079
8.233035	751.540672	10.012096
8.317690	742.277767	10.017114
8.393311	749.245079	10.022131
8.023521	746.564979	10.027149
7.903354	735.744573	10.032167
7.982645	754.638794	10.037184
8.137390	751.408118	10.042202
8.197547	753.827512	10.047219
8.148769	746.118668	10.052237
8.060612	755.153828	10.057255
7.898511	755.410929	10.062272
8.148659	754.198873	10.067290
8.050908	756.786365	10.072307
8.224894	751.110026	10.077325
8.168608	764.632637	10.082343
8.306813	762.618160	10.087360
8.534399	756.485107	10.092378
8.418431	766.962117	10.097395
8.337171	750.922112	10.102413
8.220990	767.126789	10.107431
8.438279	757.519572	10.112448
8.693621	753.526832	10.117466
8.334201	751.029533	10.122483
8.438865	745.469161	10.127501
8.310272	754.727205	10.132519
7.992426	756.960487	10.137536
8.309894	765.026223	10.142554
8.635698	791.300792	10.147571
8.512807	779.201402	10.152589
8.252798	776.147903	10.157607
8.126084	780.016832	10.162624
8.619296	789.504170	10.167642
8.475358	801.982723	10.172659
8.828213	782.185168	10.177677
8.743709	780.596990	10.182695
8.187768	774.139750	10.187712
8.282932	774.706540	10.192730
8.240821	785.509094	10.197747
8.166896	792.692640	10.202765
8.222864	781.748131	10.207783
8.381200	789.610295	10.212800
8.642969	793.682306	10.217818
8.413636	791.839763	10.222835
8.626348	791.075742	10.227853
8.503042	798.681750	10.232871
8.344076	806.269249	10.237888
8.596024	795.336037	10.242906
8.624700	796.174006	10.247923
8.395902	793.839925	10.252941
8.527565	802.374202	10.257959
8.285719	795.962669	10.262976
8.633981	798.702506	10.267994
8.571102	794.554111	10.273011
8.537242	799.215926	10.278029
8.760998	797.932453	10.283047
8.362140	798.280049	10.288064
8.594419	788.215985	10.293082
8.501298	794.917061	10.298099
8.869146	814.399584	10.303117
8.820961	814.376587	10.308135
8.595574	812.913934	10.313152
8.591422	795.135848	10.318170
8.503782	799.253004	10.323187
8.701488	812.640885	10.328205
8.893905	814.013609	10.333223
8.721221	825.533514	10.338240
8.773882	831.045262	10.343258
8.741178	824.417100	10.348275
9.200825	820.857922	10.353293
8.847734	807.499235	10.358311
8.873696	809.270956	10.363328
8.853339	796.015436	10.368346
8.640266	797.196550	10.373363
8.639462	793.421394	10.378381
8.857818	796.824319	10.383399
8.663350	807.967463	10.388416
8.785049	803.938735	10.393434
8.835622	792.265413	10.398451
8.791951	801.617012	10.403469
8.739067	809.349454	10.408487
8.754831	817.352298	10.413504
9.078056	811.610732	10.418522
8.832723	811.753854	10.423539
8.778214	806.368263	10.428557
9.041047	800.246590	10.433575
8.784714	802.749094	10.438592
8.831005	803.287551	10.443610
9.236656	821.133113	10.448627
8.602593	810.316489	10.453645
8.852612	814.707222	10.458663
8.837404	817.495515	10.463680
8.959807	814.625818	10.468698
8.816951	815.607174	10.473715
8.987059	825.028165	10.478733
9.255282	815.189995	10.483751
8.939726	835.254196	10.488768
8.927838	820.930705	10.493786
8.755657	824.693890	10.498803
8.866457	827.958717	10.503821
9.344816	824.346061	10.508839
8.938522	823.558369	10.513856
8.937005	824.044402	10.518874
9.055379	823.145700	10.523891
9.249762	821.221325	10.528909
9.478229	817.570550	10.533927
8.868581	802.507616	10.538944
8.822707	805.024546	10.543962
8.663613	809.307423	10.548979
8.816791	820.534343	10.553997
9.067141	834.596595	10.559015
8.920147	831.991947	10.564032
9.404716	826.283938	10.569050
9.450142	830.040589	10.574067
9.321299	813.605202	10.579085
8.853176	821.290345	10.584103
8.647085	833.830366	10.589120
8.938381	829.092028	10.594138
8.990086	832.873523	10.599155
8.796353	839.088280	10.604173
9.085708	824.892237	10.609191
9.048334	843.779375	10.614208
8.848203	843.154823	10.619226
9.165495	842.587457	10.624243
9.232866	832.488029	10.629261
9.396495	833.286379	10.634279
8.970031	831.901335	10.639296
9.194538	827.255910	10.644314
9.297274	836.062165	10.649331
9.144318	838.675720	10.654349
9.486728	835.024022	10.659367
9.365409	835.485274	10.664384
9.328379	832.548531	10.669402
9.234962	837.152691	10.674419
9.288336	834.271665	10.679437
9.462568	828.861256	10.684455
9.476118	834.495787	10.689472
9.178985	824.736078	10.694490
8.936376	827.746664	10.699507
8.840914	837.040122	10.704525
9.402403	848.318760	10.709543
9.294658	864.457196	10.714560
9.439984	860.558777	10.719578
9.783836	857.902139	10.724595
9.152183	856.784623	10.729613
9.553946	847.457541	10.734631
9.188744	854.035621	10.739648
9.369387	860.530981	10.744666
9.902241	853.200395	10.749683
9.429321	848.122277	10.754701
9.375805	831.694893	10.759719
9.179652	831.401320	10.764736
9.307857	844.858677	10.769754
9.422470	851.566091	10.774771
8.937351	857.660729	10.779789
9.221657	861.925752	10.784807
9.405369	865.359708	10.789824
9.354704	861.145115	10.794842
9.458347	866.033791	10.799859
9.476483	862.176466	10.804877
9.147806	860.151940	10.809895
9.084057	863.044014	10.814912
9.598668	862.687109	10.819930
9.188850	849.751075	10.824947
9.421318	861.976660	10.829965
9.360279	860.762683	10.834983
9.549206	880.459569	10.840000
9.498927	885.198717	10.845018
9.674969	887.218435	10.850035
9.433229	891.773316	10.855053
9.989075	885.216737	10.860071
9.851714	890.587890	10.865088
9.898669	873.270382	10.870106
10.088365	860.962704	10.875123
9.693015	871.250658	10.880141
9.845149	853.539280	10.885159
9.700710	858.826567	10.890176
9.759375	859.374002	10.895194
9.694496	864.295447	10.900211
9.503587	862.415842	10.905229
9.611976	849.304031	10.910247
9.596736	859.452995	10.915264
9.701762	846.986318	10.920282
9.543046	855.464396	10.925299
9.574489	863.238925	10.930317
9.689720	843.258058	10.935335
9.548939	851.904795	10.940352
9.662837	848.887605	10.945370
9.665193	860.990416	10.950387
9.842931	860.124513	10.955405
9.865064	874.691562	10.960423
9.736571	862.812581	10.965440
9.749783	854.334611	10.970458
9.672753	865.585534	10.975475
9.663435	874.392812	10.980493
10.137393	880.631280	10.985511
9.953783	867.373055	10.990528
9.930019	877.719863	10.995546
9.933484	857.303193	11.000563
9.676924	868.732383	11.005581
9.676550	850.317201	11.010599
9.802769	863.921334	11.015616
10.161667	883.617887	11.020634
9.969882	888.468791	11.025651
9.888490	875.169853	11.030669
9.702423	866.907257	11.035687
10.074089	884.106650	11.040704
9.836708	878.558372	11.045722
10.020860	890.229854	11.050739
9.868181	894.647400	11.055757
10.028975	884.481130	11.060775
10.034381	882.743068	11.065792
10.084172	884.337267	11.070810
10.170849	890.451581	11.075827
9.546865	867.219784	11.080845
9.844214	872.707841	11.085863
9.578646	885.068100	11.090880
9.229463	887.404889	11.095898
9.902303	881.947098	11.100915
9.858245	900.468739	11.105933
10.106537	888.720158	11.110951
9.859265	892.435543	11.115968
9.620761	895.900899	11.120986
10.016998	903.215428	11.126003
10.060852	915.395072	11.131021
10.377921	921.844688	11.136039
10.066392	903.690866	11.141056
9.968252	896.056136	11.146074
10.290436	896.664142	11.151091
10.351834	887.666662	11.156109
10.245421	887.480482	11.161127
10.335008	890.775890	11.166144
10.283959	896.045395	11.171162
10.458291	889.847283	11.176179
9.973923	886.532758	11.181197
10.166038	881.688373	11.186215
10.072207	883.104372	11.191232
10.251596	884.506318	11.196250
10.192862	889.973514	11.201267
10.146559	885.507447	11.206285
10.033808	891.426606	11.211303
10.025236	884.478735	11.216320
10.221804	909.131044	11.221338
10.453613	909.004898	11.226355
10.028790	911.805296	11.231373
10.208739	907.907443	11.236391
10.238881	919.243039	11.241408
10.386654	923.717619	11.246426
10.236009	916.152373	11.251443
10.805242	911.253926	11.256461
10.439451	909.181992	11.261479
10.716872	886.048606	11.266496
10.262276	894.215622	11.271514
10.496368	877.594622	11.276531
10.655641	892.307500	11.281549
10.522645	888.203142	11.286567
10.392439	884.642327	11.291584
10.241815	885.946275	11.296602
10.554183	881.397320	11.301619
10.320189	887.884452	11.306637
10.547936	875.471475	11.311655
10.333020	877.216289	11.316672
10.331657	885.098201	11.321690
10.573163	884.586068	11.326707
10.235839	880.398174	11.331725
10.593603	875.106607	11.336743
10.313084	871.964662	11.341760
10.266722	883.167821	11.346778
10.654164	866.928706	11.351795
10.089966	878.058800	11.356813
10.261645	891.779046	11.361831
10.727149	906.060098	11.366848
10.489925	916.486294	11.371866
10.695772	911.184589	11.376883
11.121820	916.256577	11.381901
10.532745	907.528756	11.386919
10.957042	883.777697	11.391936
10.238795	887.951358	11.396954
10.507157	879.813625	11.401971
10.505659	886.947458	11.406989
10.652531	900.419099	11.412007
10.499528	904.373393	11.417024
10.272435	917.889921	11.422042
11.062041	907.208374	11.427059
10.804108	909.269107	11.432077
10.719877	903.451458	11.437095
10.986748	908.384618	11.442112
10.818544	903.257702	11.447130
10.803869	886.797663	11.452147
10.453551	886.082987	11.457165
10.588536	871.145020	11.462183
10.766065	878.227812	11.467200
10.638124	904.618299	11.472218
10.872752	909.441059	11.477235
10.957436	906.493832	11.482253
10.515979	888.712621	11.487271
10.630976	896.112395	11.492288
10.863558	904.034581	11.497306
10.687369	905.284694	11.502323
10.812563	903.910235	11.507341
10.803598	910.274771	11.512359
10.864419	898.336924	11.517376
10.756825	916.153849	11.522394
11.142530	924.487086	11.527411
10.831953	917.924287	11.532429
10.690201	915.322892	11.537447
10.763376	915.189107	11.542464
10.397908	915.807814	11.547482
11.065591	913.084073	11.552499
10.614534	913.027275	11.557517
10.615801	914.380915	11.562535
10.669884	911.698150	11.567552
10.685552	920.164570	11.572570
10.865711	908.954311	11.577587
10.732789	911.415379	11.582605
10.737358	919.848205	11.587623
11.116622	919.499692	11.592640
11.208288	940.947087	11.597658
10.966977	932.129701	11.602675
10.962865	926.691061	11.607693
10.916298	935.979254	11.612711
11.371408	937.715107	11.617728
10.986585	932.047300	11.622746
11.051892	919.672153	11.627763
11.077661	911.880742	11.632781
10.898488	925.280320	11.637799
11.300982	934.247494	11.642816
10.902881	934.074876	11.647834
11.464427	927.473054	11.652851
11.095135	925.616424	11.657869
10.851981	918.639598	11.662887
11.368274	928.460259	11.667904
11.154598	929.277665	11.672922
11.190957	923.245821	11.677939
11.332108	921.541415	11.682957
11.209101	912.158518	11.687975
11.222626	899.391026	11.692992
10.760380	922.962663	11.698010
11.292052	920.927822	11.703027
11.241737	940.346066	11.708045
10.864209	945.246577	11.713063
11.122715	944.095516	11.718080
11.077630	942.234710	11.723098
11.029100	947.820496	11.728115
11.085580	946.274938	11.733133
11.237015	939.162631	11.738151
11.168760	938.706999	11.743168
11.054955	947.811067	11.748186
11.434753	939.024086	11.753203
11.351474	924.768684	11.758221
11.348117	930.584952	11.763239
11.571851	931.248001	11.768256
11.663703	937.790149	11.773274
11.203165	932.383632	11.778291
11.222119	928.240376	11.783309
11.352382	932.223642	11.788327
11.364967	942.499734	11.793344
11.255235	943.206672	11.798362
11.330867	931.720411	11.803379
11.189956	937.700137	11.808397
11.178432	942.219547	11.813415
11.314890	948.260708	11.818432
11.618722	965.552098	11.823450
11.396399	967.706150	11.828467
11.620946	971.908650	11.833485
11.136270	964.286196	11.838503
11.616508	964.831675	11.843520
11.553490	970.429902	11.848538
11.693567	958.589719	11.853555
11.820512	963.147661	11.858573
11.487882	955.976779	11.863591
11.414092	941.969555	11.868608
11.589953	961.755305	11.873626
11.930974	970.071546	11.878643
11.497383	946.727075	11.883661
11.330435	953.685951	11.888679
11.724100	960.452203	11.893696
11.448114	972.379088	11.898714
11.765042	981.590313	11.903731
11.789201	975.919659	11.908749
11.748724	970.257326	11.913767
11.698939	959.620375	11.918784
11.303656	956.130706	11.923802
11.581108	969.195458	11.928819
12.192470	961.837085	11.933837
11.672173	974.162947	11.938855
12.087072	955.434959	11.943872
11.757669	946.552213	11.948890
11.672501	940.245809	11.953907
11.749907	948.963023	11.958925
11.486323	957.676364	11.963943
11.961016	967.897759	11.968960
11.915793	976.102466	11.973978
11.681307	970.932158	11.978995
12.093496	963.305566	11.984013
11.638866	963.570566	11.989031
11.964169	959.138919	11.994048
12.183718	965.827862	11.999066
11.841009	949.127918	12.004083
11.735009	944.179851	12.009101
11.462382	940.841344	12.014119
11.608841	963.843436	12.019136
11.694554	974.599511	12.024154
11.559435	986.428140	12.029171
11.874007	980.133995	12.034189
11.712893	973.166614	12.039207
11.783230	974.471450	12.044224
11.868774	972.765403	12.049242
11.852007	966.153047	12.054259
12.296772	966.398532	12.059277
11.952097	958.717518	12.064295
12.313151	968.795317	12.069312
12.141744	967.883973	12.074330
12.030104	979.748080	12.079347
12.126102	975.238199	12.084365
12.152038	982.136674	12.089383
12.113632	969.203916	12.094400
12.141825	968.231639	12.099418
11.705156	972.123396	12.104435
11.982787	968.385143	12.109453
11.755695	962.822341	12.114471
11.936270	970.060748	12.119488
12.015493	973.481096	12.124506
11.989337	971.236708	12.129523
12.230208	973.598620	12.134541
12.228114	992.444683	12.139559
12.331421	980.358829	12.144576
12.348751	976.133951	12.149594
12.358382	971.173065	12.154611
12.607657	963.347054	12.159629
12.436417	962.499648	12.164647
12.413509	963.601031	12.169664
12.630379	957.180937	12.174682
12.543216	970.746620	12.179699
12.225477	964.856136	12.184717
12.136556	965.190405	12.189735
12.684351	964.486535	12.194752
12.341623	961.803204	12.199770
12.451496	965.841021	12.204787
12.737732	969.733572	12.209805
12.693042	966.002529	12.214823
12.564478	936.105184	12.219840
12.069432	935.287474	12.224858
12.022120	939.344764	12.229875
12.100561	942.997085	12.234893
11.973667	963.347744	12.239911
11.962572	966.580292	12.244928
12.142236	973.609634	12.249946
11.943896	974.717964	12.254963
12.365331	958.168854	12.259981
12.095471	967.170593	12.264999
12.554088	977.269868	12.270016
12.492529	989.877751	12.275034
12.593518	994.022144	12.280051
13.041085	984.619705	12.285069
12.617104	969.284133	12.290087
12.686033	974.947944	12.295104
12.607896	952.583139	12.300122
12.164340	965.000232	12.305139
12.568604	959.207922	12.310157
12.509695	961.441842	12.315175
12.407014	953.689742	12.320192
12.384465	954.882979	12.325210
12.478806	968.146860	12.330227
13.133094	980.007408	12.335245
12.605147	973.397449	12.340263
12.575285	956.738303	12.345280
12.867328	960.099466	12.350298
12.093967	962.557536	12.355315
12.620417	968.760599	12.360333
12.781477	986.809936	12.365351
12.671999	991.581336	12.370368
12.864146	996.867961	12.375386
12.549101	992.300234	12.380403
12.899906	995.334816	12.385421
12.543916	983.493731	12.390439
12.676585	988.283964	12.395456
12.854295	983.967631	12.400474
12.536866	983.012119	12.405491
12.974048	986.801396	12.410509
13.136669	990.084954	12.415527
12.658765	992.861073	12.420544
12.772754	989.073886	12.425562
12.850600	989.493373	12.430579
12.822095	992.716011	12.435597
12.529099	987.807885	12.440615
12.735409	998.341521	12.445632
12.995084	987.792759	12.450650
12.730763	995.076553	12.455667
12.846705	1004.226139	12.460685
13.130322	1003.822576	12.465703
12.940209	1002.000884	12.470720
13.234156	991.033924	12.475738
12.632545	998.426008	12.480755
12.795311	995.131663	12.485773
12.952669	994.626543	12.490791
12.844809	997.265541	12.495808
13.203253	990.953316	12.500826
12.923955	999.308707	12.505843
12.916024	991.707046	12.510861
12.969304	997.553737	12.515879
13.005033	995.020424	12.520896
13.122555	988.104613	12.525914
12.704603	1009.734531	12.530931
13.140544	987.107981	12.535949
13.006236	1000.568310	12.540967
13.223601	1015.019385	12.545984
13.199286	998.539366	12.551002
13.068056	1011.788010	12.556019
13.484452	1009.555116	12.561037
13.538009	998.132680	12.566055
13.084006	996.806296	12.571072
13.522747	986.788681	12.576090
13.169183	983.352141	12.581107
13.353741	978.516848	12.586125
13.366590	985.531445	12.591143
13.346249	989.738597	12.596160
13.285537	990.888151	12.601178
13.042586	985.187433	12.606195
13.624791	989.900625	12.611213
13.200928	989.962343	12.616231
13.014306	999.384921	12.621248
13.048156	991.749983	12.626266
12.814667	980.614916	12.631283
13.187588	1001.330399	12.636301
13.482702	1016.255556	12.641319
13.412295	1021.284641	12.646336
13.624380	1017.029930	12.651354
13.760173	1018.995303	12.656371
13.672875	998.426346	12.661389
13.635778	985.097948	12.666407
13.095739	985.043454	12.671424
13.518290	976.029147	12.676442
13.268597	981.814894	12.681459
13.513307	986.947183	12.686477
13.315655	988.281152	12.691495
13.557235	1012.781724	12.696512
13.699867	1008.199374	12.701530
13.788449	1003.482279	12.706547
13.661185	984.331333	12.711565
13.719623	975.368931	12.716583
13.357009	979.920784	12.721600
13.580000	974.401495	12.726618
13.927898	965.946883	12.731635
13.902926	974.308846	12.736653
13.942327	973.843098	12.741671
13.877246	984.791198	12.746688
13.949726	966.635840	12.751706
13.789780	965.843448	12.756723
13.796418	970.505314	12.761741
13.682766	967.611517	12.766759
13.549849	972.604466	12.771776
13.627601	965.220117	12.776794
13.570014	975.306679	12.781811
13.482739	971.554133	12.786829
13.555683	979.084696	12.791847
13.411483	976.373279	12.796864
13.693624	973.120619	12.801882
13.543139	979.296794	12.806899
13.817599	984.819181	12.811917
13.735726	983.056954	12.816935
13.762434	999.279397	12.821952
13.861265	995.885005	12.826970
13.866896	1008.431021	12.831987
13.585078	1005.977736	12.837005
13.965684	1008.692880	12.842023
13.550730	1010.198958	12.847040
13.767230	1014.196730	12.852058
13.831967	1013.177866	12.857075
13.824616	1013.918077	12.862093
13.963548	1014.307592	12.867111
13.740571	1012.679882	12.872128
13.914155	1021.928401	12.877146
13.774196	1018.514221	12.882163
13.920147	1014.310001	12.887181
13.989011	1010.217717	12.892199
13.729766	1010.444918	12.897216
13.890627	1006.858019	12.902234
13.942638	1009.542438	12.907251
13.794196	1015.484075	12.912269
14.173152	1026.740853	12.917287
14.101692	1034.636590	12.922304
14.299265	1043.149383	12.927322
13.996354	1035.772797	12.932339
14.172918	1041.779615	12.937357
14.456146	1030.839789	12.942375
13.899598	1023.363216	12.947392
14.228391	1020.329966	12.952410
14.067198	1024.923732	12.957427
14.498640	1040.595554	12.962445
14.366926	1014.831192	12.967463
14.226485	1016.598749	12.972480
14.136955	1006.088983	12.977498
14.165268	1008.114826	12.982515
14.357371	1021.100435	12.987533
14.365933	1011.401096	12.992551
14.140328	1011.529052	12.997568
14.272310	1022.766020	13.002586
14.398637	1026.676351	13.007603
14.396410	1033.322851	13.012621
14.491256	1041.054910	13.017639
13.792982	1045.463857	13.022656
14.144387	1034.559014	13.027674
14.196240	1032.395018	13.032691
14.026850	1039.869806	13.037709
14.262964	1027.505119	13.042727
14.251032	1039.954866	13.047744
14.628086	1023.891684	13.052762
14.389406	1015.849479	13.057779
14.685822	1021.492641	13.062797
14.766457	1031.679017	13.067815
14.486588	1037.080659	13.072832
14.367733	1039.207191	13.077850
14.490241	1036.502272	13.082867
14.295653	1038.597429	13.087885
14.464140	1040.945333	13.092903
14.190200	1044.995227	13.097920
14.581289	1034.055485	13.102938
14.345538	1035.882684	13.107955
14.589653	1056.226281	13.112973
14.924166	1051.204793	13.117991
14.903249	1055.011137	13.123008
14.916211	1036.420523	13.128026
14.729479	1031.062017	13.133043
14.680718	1035.723807	13.138061
14.855508	1021.528408	13.143079
14.661528	1027.153217	13.148096
14.656702	1037.102775	13.153114
14.643092	1034.925978	13.158131
14.430403	1029.154112	13.163149
14.792835	1018.712147	13.168167
14.724388	1026.175758	13.173184
14.822184	1019.261619	13.178202
14.735449	1024.865162	13.183219
15.020750	1044.488861	13.188237
14.702263	1033.684288	13.193255
14.991270	1049.918943	13.198272
15.082500	1035.149440	13.203290
14.840480	1034.710514	13.208307
14.793484	1031.928505	13.213325
14.922998	1032.598666	13.218343
14.813657	1036.208234	13.223360
15.131348	1041.094463	13.228378
14.986302	1024.401530	13.233395
14.725564	1029.113897	13.238413
15.118187	1033.975341	13.243431
15.235264	1033.458179	13.248448
14.961197	1041.196486	13.253466
14.930803	1027.884658	13.258483
14.670516	1030.006416	13.263501
14.903891	1040.552339	13.268519
14.930248	1045.860276	13.273536
15.690328	1043.701862	13.278554
15.323130	1048.197218	13.283571
15.088313	1041.612793	13.288589
15.491358	1013.196689	13.293607
14.891379	1015.561755	13.298624
15.291192	1026.379919	13.303642
15.555254	1015.549158	13.308659
15.137791	1021.486049	13.313677
15.110526	1012.336442	13.318695
15.053295	1009.483305	13.323712
15.409108	1018.927854	13.328730
15.371531	1014.593160	13.333747
15.410079	1002.702213	13.338765
15.414330	1008.437345	13.343783
15.317154	1020.639197	13.348800
15.686662	1009.334198	13.353818
15.684126	1019.312889	13.358835
15.452911	1017.125999	13.363853
15.174678	1020.364520	13.368871
15.488475	1012.711651	13.373888
15.479921	1012.731310	13.378906
15.713590	1013.612766	13.383923
15.433971	1019.267469	13.388941
15.666498	1003.438985	13.393959
15.428210	998.298622	13.398976
15.610280	1009.954794	13.403994
15.805893	999.820483	13.409011
15.530083	1014.011968	13.414029
15.720152	1004.646755	13.419047
15.623344	996.260104	13.424064
15.491117	996.708402	13.429082
15.175673	983.834008	13.434099
14.943173	993.770578	13.439117
15.674963	1008.722764	13.444135
15.745071	1007.834685	13.449152
15.665161	1010.091567	13.454170
15.584226	1012.946358	13.459187
15.470313	1007.902349	13.464205
15.992781	1002.668941	13.469223
15.653664	1004.358715	13.474240
15.689957	1015.596531	13.479258
15.556845	997.037189	13.484275
15.383251	1011.833729	13.489293
15.472793	998.669008	13.494311
15.526628	1006.221243	13.499328
15.279920	1014.473437	13.504346
15.606610	1001.275824	13.509363
15.436253	1016.255267	13.514381
15.550755	1003.425537	13.519399
15.346013	1018.996399	13.524416
15.758220	1037.746105	13.529434
16.080821	1038.375896	13.534451
15.761953	1056.760293	13.539469
16.109221	1052.128761	13.544487
16.041365	1052.654992	13.549504
16.034840	1038.471039	13.554522
15.466553	1023.654456	13.559539
15.486665	1036.835206	13.564557
15.564391	1028.218349	13.569575
15.523566	1033.891265	13.574592
15.901711	1047.974714	13.579610
15.871422	1041.180534	13.584627
15.416013	1055.645595	13.589645
15.708897	1053.289822	13.594663
15.793305	1051.718775	13.599680
15.914378	1071.857958	13.604698
16.652736	1061.284759	13.609715
16.518296	1059.998459	13.614733
16.358320	1040.487945	13.619751
16.372699	1030.877383	13.624768
16.262777	1039.499640	13.629786
16.518965	1026.611050	13.634803
15.999017	1047.291101	13.639821
16.563412	1039.261820	13.644839
16.450696	1040.987795	13.649856
16.410065	1028.879437	13.654874
16.524213	1035.028436	13.659891
16.137148	1037.508100	13.664909
16.265402	1018.151329	13.669927
16.400878	1035.544034	13.674944
16.179343	1042.217922	13.679962
16.535501	1029.842056	13.684979
16.336841	1031.426549	13.689997
16.276312	1029.436021	13.695015
16.318735	1038.063413	13.700032
16.412866	1037.976353	13.705050
16.639464	1033.676136	13.710067
16.275585	1041.088197	13.715085
16.199016	1035.102329	13.720103
16.369653	1042.780533	13.725120
15.967233	1047.860161	13.730138
16.240284	1039.945157	13.735155
16.236504	1037.816924	13.740173
16.219894	1036.370036	13.745191
16.018209	1041.584574	13.750208
16.056199	1041.031079	13.755226
16.409165	1045.890618	13.760243
16.448868	1060.228794	13.765261
16.772074	1063.759214	13.770279
16.703790	1067.477340	13.775296
16.231618	1064.096006	13.780314
16.879351	1070.650861	13.785331
16.756901	1072.818143	13.790349
16.713271	1073.837145	13.795367
16.975942	1068.297487	13.800384
16.508492	1059.986615	13.805402
16.750526	1055.191793	13.810419
16.596653	1057.592970	13.815437
16.848829	1053.011990	13.820455
16.885435	1057.098940	13.825472
16.710629	1046.068087	13.830490
16.748322	1029.431945	13.835507
16.549942	1036.314569	13.840525
16.837228	1049.120522	13.845543
17.238404	1052.476268	13.850560
16.873027	1049.119802	13.855578
17.047337	1036.607472	13.860595
16.821665	1033.651674	13.865613
16.626259	1034.120452	13.870631
16.765386	1017.683864	13.875648
16.352078	1044.982636	13.880666
16.898825	1051.294763	13.885683
16.869109	1052.535641	13.890701
16.575606	1061.736390	13.895719
16.680214	1056.269110	13.900736
16.607417	1059.829935	13.905754
16.893002	1047.233273	13.910771
17.052168	1061.482232	13.915789
16.838689	1066.441287	13.920807
17.219555	1064.006022	13.925824
16.628461	1067.523187	13.930842
16.769312	1062.146948	13.935859
17.014999	1084.883847	13.940877
17.371041	1086.358966	13.945895
17.549306	1092.337379	13.950912
16.909979	1092.307163	13.955930
17.042352	1081.653606	13.960947
17.054020	1094.591154	13.965965
17.667306	1096.430788	13.970983
17.426935	1086.174599	13.976000
17.105886	1075.746739	13.981018
17.060214	1069.685881	13.986035
17.334034	1082.865879	13.991053
17.468390	1088.920039	13.996071
17.682489	1064.451782	14.001088
17.409897	1061.046521	14.006106
17.724544	1057.834528	14.011123
17.140113	1062.382319	14.016141
17.064690	1060.700697	14.021159
17.205014	1049.128866	14.026176
17.025402	1073.359821	14.031194
17.539110	1091.262044	14.036211
17.222455	1101.838084	14.041229
17.352852	1103.081440	14.046247
17.719008	1100.360652	14.051264
17.167394	1093.975384	14.056282
17.511571	1085.765181	14.061299
17.609433	1088.611106	14.066317
17.771424	1094.448333	14.071335
17.685991	1085.358287	14.076352
17.576664	1092.757633	14.081370
17.451871	1098.156108	14.086387
17.402183	1096.271638	14.091405
17.419994	1096.405819	14.096423
17.740394	1087.020986	14.101440
17.578900	1093.337981	14.106458
17.932694	1088.999803	14.111475
17.424878	1096.376630	14.116493
17.119060	1089.262269	14.121511
17.629462	1090.552456	14.126528
17.501551	1091.771971	14.131546
17.704891	1083.604528	14.136563
17.449175	1085.470657	14.141581
17.416385	1088.824711	14.146599
17.893185	1104.782759	14.151616
17.800146	1105.946127	14.156634
17.818860	1112.341404	14.161651
17.651681	1120.277999	14.166669
17.805587	1114.199888	14.171687
17.984261	1110.657061	14.176704
18.023564	1105.570381	14.181722
17.984764	1114.533629	14.186739
18.203180	1112.459402	14.191757
17.786241	1115.365801	14.196775
18.236916	1113.041808	14.201792
17.824668	1114.245920	14.206810
18.045414	1116.271666	14.211827
18.096368	1104.342572	14.216845
18.030977	1106.855887	14.221863
18.398104	1106.482019	14.226880
18.068475	1112.866367	14.231898
18.365800	1101.562798	14.236915
18.214392	1101.817252	14.241933
17.987568	1085.978188	14.246951
18.252890	1084.691563	14.251968
18.156614	1092.348949	14.256986
17.882456	1091.313653	14.262003
17.960613	1104.621462	14.267021
18.179308	1110.389884	14.272039
18.439587	1111.340362	14.277056
17.754973	1109.335848	14.282074
17.819354	1115.853875	14.287091
18.325362	1111.405314	14.292109
18.120496	1109.988741	14.297127
18.347532	1107.890062	14.302144
17.904160	1117.142771	14.307162
17.983319	1103.495893	14.312179
18.288870	1111.842282	14.317197
18.417421	1127.013346	14.322215
18.562931	1120.621117	14.327232
18.451853	1118.272649	14.332250
18.318425	1114.496597	14.337267
18.736596	1107.688112	14.342285
18.069318	1101.988781	14.347303
18.221534	1114.369736	14.352320
18.552326	1129.940191	14.357338
18.430420	1130.008498	14.362355
18.817637	1132.899711	14.367373
18.776303	1139.661758	14.372391
18.788745	1119.632371	14.377408
18.977655	1132.059631	14.382426
18.832042	1113.039883	14.387443
18.775886	1099.335067	14.392461
18.482026	1100.488517	14.397479
18.731968	1089.438615	14.402496
18.685544	1104.865900	14.407514
18.624568	1091.786003	14.412531
18.800712	1110.520093	14.417549
19.143883	1109.562084	14.422567
19.193463	1087.951842	14.427584
18.596038	1092.465377	14.432602
18.495821	1098.144983	14.437619
18.925744	1085.612810	14.442637
18.737869	1092.790134	14.447655
18.967218	1082.737582	14.452672
18.738400	1087.405327	14.457690
18.911301	1098.334650	14.462707
18.606507	1108.740455	14.467725
18.806699	1117.109965	14.472743
19.081035	1122.835345	14.477760
19.122560	1129.327434	14.482778
18.787301	1130.884518	14.487795
18.866525	1124.770719	14.492813
18.702769	1122.749214	14.497831
19.263585	1123.018236	14.502848
19.204366	1123.810324	14.507866
19.232440	1117.932899	14.512883
18.991046	1123.531332	14.517901
18.913149	1130.366729	14.522919
19.262536	1123.806379	14.527936
19.218826	1129.080459	14.532954
19.106309	1119.372718	14.537971
19.232788	1126.237323	14.542989
19.010978	1127.917173	14.548007
19.090592	1131.705151	14.553024
18.892285	1123.528875	14.558042
18.977780	1116.498042	14.563059
19.159369	1116.807096	14.568077
18.940712	1123.884813	14.573095
19.334678	1125.136576	14.578112
19.396370	1117.924467	14.583130
19.140088	1129.863372	14.588147
19.353659	1128.773850	14.593165
19.184938	1151.761585	14.598183
19.535525	1147.835473	14.603200
19.524432	1154.562219	14.608218
19.514682	1148.762086	14.613235
19.710368	1145.519347	14.618253
19.571957	1141.658691	14.623271
19.677714	1124.914953	14.628288
19.510341	1128.689030	14.633306
19.430713	1123.838499	14.638323
19.486341	1116.911602	14.643341
19.453845	1143.984849	14.648359
19.822868	1149.645190	14.653376
19.848632	1155.853127	14.658394
19.388733	1136.087769	14.663411
19.906393	1135.931705	14.668429
19.582495	1139.669848	14.673447
19.638683	1139.207226	14.678464
19.893805	1140.979694	14.683482
19.999944	1150.364023	14.688499
19.918474	1134.631972	14.693517
19.684667	1127.779076	14.698535
19.641497	1117.927220	14.703552
19.650482	1130.479670	14.708570
19.524848	1145.097178	14.713587
19.671954	1148.371918	14.718605
19.700434	1146.012586	14.723623
19.864124	1151.503543	14.728640
19.947522	1142.882339	14.733658
19.898381	1154.158387	14.738675
20.087842	1154.943039	14.743693
19.897265	1151.267550	14.748711
20.249526	1146.398193	14.753728
19.965060	1146.668337	14.758746
19.813858	1145.018123	14.763763
20.165175	1143.485428	14.768781
19.743238	1150.778218	14.773799
19.818085	1155.429262	14.778816
19.869386	1164.280027	14.783834
19.863284	1155.178011	14.788851
19.923850	1150.625122	14.793869
19.967100	1152.596359	14.798887
20.285730	1156.711523	14.803904
20.543451	1163.450733	14.808922
20.120762	1166.475199	14.813939
19.869446	1147.996223	14.818957
19.774989	1167.203183	14.823975
20.166995	1179.376284	14.828992
20.295775	1181.483958	14.834010
20.330975	1187.384489	14.839027
20.549504	1180.692416	14.844045
20.497102	1187.688759	14.849063
20.299244	1181.055653	14.854080
20.658483	1182.783759	14.859098
20.080341	1185.417247	14.864115
20.717258	1171.819062	14.869133
20.309641	1181.258983	14.874151
20.575603	1180.598136	14.879168
20.723011	1183.099130	14.884186
20.515030	1198.161334	14.889203
20.915307	1182.544084	14.894221
20.692814	1192.886548	14.899239
20.711921	1173.251797	14.904256
20.459228	1159.082432	14.909274
20.316670	1165.003079	14.914291
20.545568	1172.488480	14.919309
20.493334	1171.599352	14.924327
20.332258	1178.232604	14.929344
20.880946	1176.218931	14.934362
20.785807	1177.063408	14.939379
20.871943	1174.786656	14.944397
20.688841	1189.036987	14.949415
20.449878	1182.363829	14.954432
20.854941	1181.114922	14.959450
20.346282	1182.443419	14.964467
20.766534	1181.074500	14.969485
20.928804	1184.267029	14.974503
20.865244	1187.185114	14.979520
21.048191	1178.126438	14.984538
20.777795	1179.333094	14.989555
20.879610	1175.238274	14.994573
20.965675	1172.751526	14.999591
21.003545	1171.427296	15.004608
20.827641	1167.141792	15.009626
20.743541	1184.327482	15.014643
20.770663	1170.354154	15.019661
20.538915	1181.047694	15.024679
20.582217	1204.242364	15.029696
21.266850	1195.296219	15.034714
21.271709	1211.558318	15.039731
21.554506	1195.567613	15.044749
21.776117	1200.104864	15.049767
21.442884	1190.955325	15.054784
21.152079	1166.804362	15.059802
20.926740	1171.601065	15.064819
21.196730	1178.828929	15.069837
21.099030	1190.548003	15.074855
21.192269	1208.034484	15.079872
21.575503	1189.943044	15.084890
21.558973	1198.231304	15.089907
21.418863	1189.629294	15.094925
21.234218	1184.278656	15.099943
21.303656	1189.177811	15.104960
21.465073	1193.981860	15.109978
21.602737	1199.482055	15.114995
21.451359	1186.332384	15.120013
21.725049	1191.772112	15.125031
21.545410	1185.512513	15.130048
21.556894	1178.380709	15.135066
21.173128	1179.977107	15.140083
21.509255	1181.115814	15.145101
21.750066	1193.765222	15.150119
21.157578	1197.461163	15.155136
21.591921	1189.054143	15.160154
21.567900	1186.753080	15.165171
21.415345	1186.515277	15.170189
21.514081	1191.220053	15.175207
21.523643	1187.636464	15.180224
21.652660	1183.981175	15.185242
21.451563	1197.832972	15.190259
21.579000	1192.438435	15.195277
21.505193	1193.710032	15.200295
21.458125	1195.168717	15.205312
21.988710	1210.096289	15.210330
21.922563	1227.425496	15.215347
22.364206	1204.464072	15.220365
22.057351	1187.139726	15.225383
21.893698	1195.131477	15.230400
21.601178	1193.292044	15.235418
21.298573	1186.383769	15.240435
21.893809	1198.743150	15.245453
22.009864	1215.045334	15.250471
21.805969	1217.238496	15.255488
22.036325	1204.712635	15.260506
21.775467	1216.902326	15.265523
22.058671	1217.147551	15.270541
22.341664	1212.944249	15.275559
22.071851	1227.254016	15.280576
22.392473	1218.183785	15.285594
22.364985	1216.682583	15.290611
22.013105	1217.977499	15.295629
22.503077	1224.809636	15.300647
22.100366	1226.809899	15.305664
22.327448	1215.745971	15.310682
21.905145	1228.036159	15.315699
22.276868	1206.086141	15.320717
22.381338	1212.279127	15.325735
22.113355	1216.184992	15.330752
22.398089	1208.071936	15.335770
22.037795	1218.934558	15.340787
21.965306	1208.671998	15.345805
22.471387	1208.584176	15.350823
22.396137	1212.359779	15.355840
22.496219	1206.760143	15.360858
22.178591	1204.487126	15.365875
22.574378	1210.305445	15.370893
22.627504	1211.303742	15.375911
22.274365	1220.228459	15.380928
22.657615	1228.826600	15.385946
22.726608	1233.128686	15.390963
22.544799	1256.863515	15.395981
22.834452	1237.484128	15.400999
22.806424	1234.257673	15.406016
22.739874	1216.585361	15.411034
22.451751	1214.440322	15.416051
22.836016	1225.951254	15.421069
23.108761	1225.195006	15.426087
22.899976	1216.353186	15.431104
23.015013	1203.038430	15.436122
22.809064	1200.391696	15.441139
22.713426	1203.262336	15.446157
23.057080	1195.862279	15.451175
22.859839	1200.689973	15.456192
23.029209	1189.313601	15.461210
22.789621	1198.843464	15.466227
22.775095	1197.417867	15.471245
22.766956	1196.487991	15.476263
22.730273	1228.315905	15.481280
22.858415	1225.033925	15.486298
23.275993	1235.993376	15.491315
23.135402	1233.842259	15.496333
23.222382	1230.287395	15.501351
22.765203	1235.640072	15.506368
23.120254	1225.915619	15.511386
22.909759	1230.793538	15.516403
22.769197	1229.869600	15.521421
23.044064	1220.492998	15.526439
23.042068	1226.790973	15.531456
22.868178	1221.993581	15.536474
23.015568	1220.071805	15.541491
22.691111	1234.822436	15.546509
23.258469	1246.185624	15.551527
23.073486	1265.508636	15.556544
23.494239	1253.853308	15.561562
23.160466	1262.366639	15.566579
23.597125	1261.269372	15.571597
23.597555	1262.301378	15.576615
23.577067	1263.867866	15.581632
23.741250	1260.032560	15.586650
23.533552	1245.409484	15.591667
23.535391	1255.116974	15.596685
23.758169	1256.302366	15.601703
23.534105	1262.340638	15.606720
23.580683	1269.128957	15.611738
23.518887	1268.098904	15.616755
23.842313	1263.051625	15.621773
23.679539	1254.763909	15.626791
23.547471	1263.228754	15.631808
24.061599	1253.817909	15.636826
23.829299	1249.123454	15.641843
23.643242	1229.055083	15.646861
23.804772	1244.502466	15.651879
23.713365	1250.500704	15.656896
24.116604	1236.447645	15.661914
23.648325	1232.857981	15.666931
23.626795	1243.316068	15.671949
23.875545	1248.711323	15.676967
23.708529	1259.252705	15.681984
23.491537	1264.432451	15.687002
23.901830	1255.590850	15.692019
24.118337	1268.503354	15.697037
24.050234	1262.403809	15.702055
23.748432	1260.948327	15.707072
23.889008	1257.269657	15.712090
23.931914	1252.769059	15.717107
23.837318	1255.967048	15.722125
24.107807	1253.544286	15.727143
23.921364	1251.865441	15.732160
24.094409	1260.041315	15.737178
24.000534	1260.240011	15.742195
23.701496	1272.722038	15.747213
24.320554	1271.259637	15.752231
24.224150	1284.190994	15.757248
24.149446	1288.410951	15.762266
24.465083	1275.135414	15.767283
24.088276	1279.849323	15.772301
24.382128	1281.457556	15.777319
24.275758	1290.410815	15.782336
24.394554	1286.347800	15.787354
24.556453	1282.159176	15.792371
24.388925	1286.478712	15.797389
24.874532	1276.088060	15.802407
24.509494	1272.509078	15.807424
24.457081	1282.699893	15.812442
24.453859	1279.090840	15.817459
24.596394	1284.528262	15.822477
24.623902	1291.274276	15.827495
24.588733	1274.703248	15.832512
24.892494	1281.965535	15.837530
24.774940	1285.606435	15.842547
24.631738	1286.455513	15.847565
25.064024	1284.994255	15.852583
24.591571	1284.227310	15.857600
24.610442	1284.982490	15.862618
24.736770	1286.677257	15.867635
24.778253	1282.423701	15.872653
24.817890	1274.927212	15.877671
24.493895	1281.339631	15.882688
24.443361	1286.140156	15.887706
24.624046	1283.695030	15.892723
24.348122	1288.816423	15.897741
24.797023	1290.478945	15.902759
24.719739	1305.285240	15.907776
24.992013	1312.242749	15.912794
25.379261	1294.759887	15.917811
25.093627	1318.407848	15.922829
25.306007	1301.964561	15.927847
25.022532	1309.303628	15.932864
25.249794	1309.103439	15.937882
25.495158	1296.420320	15.942899
25.112898	1281.413122	15.947917
25.138365	1279.168622	15.952935
25.343443	1281.419191	15.957952
25.003354	1275.649586	15.962970
25.285445	1292.535351	15.967987
25.017116	1294.097136	15.973005
25.315743	1296.102557	15.978023
24.978499	1310.187553	15.983040
25.234673	1304.974234	15.988058
25.506747	1295.700789	15.993075
25.309555	1298.542566	15.998093
25.501544	1293.278842	16.003111
25.294776	1302.361872	16.008128
25.088540	1303.961618	16.013146
25.696729	1294.810953	16.018163
25.752116	1305.422293	16.023181
25.665430	1301.720742	16.028199
25.560864	1303.172013	16.033216
25.438074	1311.885119	16.038234
25.691729	1298.722349	16.043251
25.582097	1308.485690	16.048269
25.642768	1300.278923	16.053287
25.487038	1297.851597	16.058304
25.552040	1300.571908	16.063322
25.576350	1300.081680	16.068339
25.299186	1310.259463	16.073357
25.686914	1327.026839	16.078375
25.954413	1333.273041	16.083392
26.228365	1337.690676	16.088410
26.443114	1320.520896	16.093427
25.951024	1323.109876	16.098445
26.033053	1305.437709	16.103463
25.833623	1301.810884	16.108480
25.918036	1299.286008	16.113498
26.069330	1288.593557	16.118515
26.077072	1303.984142	16.123533
26.110026	1303.115963	16.128551
26.126186	1301.618562	16.133568
26.123049	1299.152046	16.138586
26.473496	1297.050466	16.143603
25.885723	1295.168091	16.148621
25.983331	1309.536296	16.153639
26.213368	1321.031059	16.158656
26.131632	1321.277742	16.163674
26.082853	1311.970116	16.168691
26.105704	1320.686125	16.173709
26.350040	1314.650267	16.178727
26.511070	1322.592564	16.183744
26.420697	1326.066800	16.188762
26.495881	1315.904748	16.193779
26.477260	1318.774885	16.198797
26.593844	1320.608648	16.203815
26.526755	1312.335401	16.208832
26.579526	1319.914340	16.213850
26.499791	1318.082439	16.218867
26.259271	1322.022959	16.223885
26.283321	1322.560976	16.228903
26.190855	1319.987385	16.233920
26.195415	1323.347324	16.238938
26.667002	1315.764674	16.243955
26.356652	1322.166983	16.248973
26.578434	1330.271070	16.253991
26.910205	1328.169620	16.259008
26.681985	1340.499468	16.264026
27.036428	1332.663174	16.269043
26.806955	1336.080291	16.274061
26.791097	1327.132520	16.279079
26.906250	1316.508415	16.284096
26.847123	1325.423774	16.289114
26.926530	1316.176645	16.294131
26.782372	1322.922698	16.299149
26.891405	1329.837712	16.304167
26.728788	1346.745654	16.309184
26.695565	1352.026146	16.314202
27.146275	1351.593979	16.319219
27.255268	1353.799816	16.324237
27.361474	1349.419224	16.329255
27.388708	1345.133955	16.334272
27.363630	1352.064645	16.339290
27.669523	1342.749172	16.344307
27.188992	1329.090266	16.349325
27.435042	1318.870059	16.354343
27.252597	1309.220795	16.359360
26.904816	1315.417111	16.364378
27.318693	1319.918493	16.369395
27.048595	1329.241696	16.374413
27.024366	1337.747021	16.379431
27.257041	1337.298530	16.384448
26.981978	1341.745679	16.389466
26.844140	1342.731453	16.394483
26.883659	1344.635230	16.399501
27.580139	1357.525966	16.404519
27.833377	1364.715550	16.409536
27.537414	1355.991584	16.414554
27.700998	1341.941620	16.419571
27.382500	1345.423444	16.424589
27.610969	1346.260510	16.429607
27.631412	1360.214801	16.434624
27.367267	1372.919655	16.439642
27.676687	1373.206214	16.444659
27.750013	1375.398462	16.449677
28.208754	1362.485370	16.454695
28.078303	1364.996095	16.459712
27.904719	1377.214005	16.464730
27.770566	1370.708853	16.469747
28.000029	1373.856859	16.474765
28.025198	1368.248679	16.479783
27.908010	1366.244837	16.484800
27.837157	1353.815867	16.489818
28.058523	1353.651685	16.494835
27.892195	1357.103052	16.499853
28.290751	1358.428082	16.504871
28.375082	1351.579002	16.509888
27.969525	1345.785941	16.514906
28.131152	1348.373774	16.519923
28.373868	1357.516793	16.524941
28.407378	1357.077988	16.529959
28.626883	1340.655329	16.534976
28.004467	1332.424829	16.539994
28.100564	1333.185947	16.545011
27.679544	1333.651470	16.550029
28.296849	1352.673730	16.555047
28.206420	1356.869339	16.560064
28.154866	1358.761990	16.565082
28.037278	1347.188467	16.570099
28.322291	1346.300284	16.575117
28.179043	1351.665484	16.580135
28.322513	1353.783351	16.585152
28.484303	1349.130421	16.590170
28.657292	1348.813429	16.595187
28.731480	1350.653612	16.600205
28.607018	1365.077264	16.605223
28.690783	1353.679292	16.610240
28.477775	1363.307606	16.615258
28.474359	1356.176608	16.620275
28.626483	1356.947364	16.625293
28.803110	1358.114016	16.630311
29.041849	1357.385033	16.635328
28.531512	1362.805584	16.640346
28.546186	1357.201702	16.645363
28.668941	1363.359843	16.650381
28.608424	1373.426680	16.655399
28.970860	1374.791141	16.660416
28.883513	1387.670898	16.665434
28.671635	1382.231396	16.670451
28.944757	1379.010453	16.675469
28.786459	1390.324788	16.680487
28.673809	1379.855394	16.685504
28.639135	1385.743929	16.690522
29.200956	1376.593596	16.695539
28.865541	1375.177510	16.700557
28.908929	1377.896879	16.705575
29.117806	1373.125742	16.710592
29.224368	1394.917917	16.715610
29.527966	1397.987741	16.720627
29.634442	1404.011008	16.725645
29.337706	1389.776473	16.730663
29.529175	1377.996167	16.735680
29.592448	1376.025092	16.740698
29.323958	1368.916634	16.745715
29.656044	1363.801562	16.750733
29.179389	1363.339399	16.755751
29.111876	1374.466894	16.760768
28.964886	1387.091582	16.765786
29.254720	1391.619978	16.770803
29.911055	1392.217271	16.775821
29.834926	1398.592321	16.780839
29.726242	1401.826128	16.785856
29.602128	1390.282191	16.790874
29.760185	1390.650448	16.795891
29.975041	1396.538495	16.800909
29.629774	1399.871822	16.805927
29.957576	1401.884246	16.810944
29.748153	1402.262055	16.815962
29.821881	1398.759730	16.820979
29.820974	1397.683587	16.825997
29.567895	1405.382392	16.831015
29.857591	1395.494444	16.836032
29.897673	1394.001938	16.841050
29.872362	1393.016628	16.846067
29.949787	1388.364637	16.851085
29.632851	1399.648509	16.856103
30.024429	1388.658639	16.861120
29.819143	1397.077987	16.866138
30.011174	1411.474969	16.871155
30.184421	1394.870552	16.876173
30.220900	1399.472506	16.881191
30.380035	1394.076203	16.886208
30.126323	1395.736159	16.891226
30.120410	1394.932067	16.896243
30.151711	1387.983874	16.901261
29.929357	1388.874381	16.906279
30.322113	1401.858056	16.911296
30.469745	1419.931970	16.916314
30.503345	1409.499993	16.921331
30.732526	1413.717399	16.926349
30.586743	1421.648055	16.931367
30.833557	1399.149385	16.936384
30.304571	1391.797978	16.941402
30.680735	1386.995650	16.946419
30.343343	1386.979110	16.951437
30.341968	1391.382817	16.956455
30.337243	1409.765126	16.961472
30.821893	1423.110552	16.966490
30.630185	1427.172346	16.971507
30.891031	1424.113441	16.976525
30.539795	1419.315572	16.981543
30.799959	1414.111201	16.986560
30.803253	1419.706703	16.991578
30.780249	1418.406091	16.996595
30.720277	1415.881044	17.001613
30.607076	1424.686317	17.006631
31.034682	1428.432414	17.011648
30.805454	1411.437461	17.016666
30.911626	1414.742839	17.021683
30.903558	1421.655397	17.026701
30.783564	1418.812753	17.031719
30.830547	1408.773001	17.036736
30.867885	1420.022750	17.041754
30.953623	1432.348422	17.046771
31.570051	1434.276742	17.051789
31.217248	1442.344360	17.056807
31.077063	1443.702527	17.061824
31.409440	1442.921064	17.066842
31.333276	1439.809396	17.071859
31.466535	1448.499163	17.076877
31.371535	1443.081067	17.081895
31.556399	1439.084840	17.086912
31.538679	1437.727652	17.091930
31.306745	1430.236403	17.096947
31.628518	1430.896856	17.101965
31.247793	1439.934117	17.106983
31.447298	1430.925307	17.112000
31.864964	1439.242326	17.117018
31.390294	1435.126771	17.122035
31.627121	1427.125047	17.127053
31.484041	1442.407050	17.132071
31.438994	1435.075048	17.137088
31.574650	1429.320849	17.142106
31.576054	1438.098925	17.147123
31.963605	1434.173129	17.152141
31.788436	1430.344062	17.157159
31.510359	1437.119971	17.162176
31.643172	1442.987149	17.167194
31.661810	1451.728926	17.172211
32.075993	1449.742368	17.177229
32.019937	1467.675610	17.182247
32.234892	1464.831734	17.187264
32.445123	1461.514094	17.192282
32.388179	1464.576197	17.197299
32.733636	1443.663118	17.202317
32.344825	1429.652592	17.207335
32.528996	1424.163570	17.212352
32.516666	1408.597741	17.217370
32.250787	1410.881673	17.222387
32.437792	1417.316582	17.227405
32.187063	1407.138257	17.232423
32.163480	1413.392047	17.237440
32.211971	1427.777730	17.242458
32.062961	1422.790361	17.247475
32.183178	1419.125645	17.252493
32.228647	1423.463164	17.257511
32.508596	1444.250115	17.262528
32.417134	1453.184866	17.267546
32.607313	1453.857618	17.272563
32.806650	1447.968890	17.277581
32.794860	1450.026612	17.282599
32.779410	1443.640575	17.287616
32.450996	1425.562338	17.292634
32.378495	1443.610067	17.297651
32.770805	1442.015065	17.302669
32.517270	1456.756550	17.307687
32.586397	1456.093184	17.312704
32.768658	1451.592135	17.317722
32.603421	1450.839365	17.322739
32.982696	1445.464139	17.327757
32.793996	1451.960556	17.332775
32.762115	1443.757591	17.337792
32.847851	1443.368216	17.342810
32.779306	1451.605767	17.347827
33.105830	1451.748378	17.352845
32.890569	1475.592798	17.357863
33.152889	1469.671216	17.362880
33.674554	1475.595985	17.367898
33.005991	1470.796608	17.372915
33.375282	1463.698053	17.377933
33.002805	1476.130577	17.382951
32.982676	1477.786583	17.387968
33.404073	1469.962578	17.392986
33.443017	1479.099979	17.398003
33.298436	1475.666778	17.403021
33.319886	1487.461652	17.408039
33.337010	1478.462876	17.413056
33.553172	1488.420296	17.418074
33.333021	1485.331428	17.423091
33.590387	1478.330289	17.428109
33.579336	1470.365765	17.433127
33.845130	1476.034429	17.438144
33.853022	1468.940678	17.443162
33.278128	1481.526719	17.448179
33.486359	1473.928858	17.453197
33.257681	1471.358658	17.458215
33.433636	1479.593020	17.463232
33.798505	1493.503506	17.468250
33.910733	1505.125539	17.473267
34.307497	1494.243778	17.478285
33.864040	1501.334212	17.483303
33.772666	1511.088956	17.488320
34.295066	1502.550105	17.493338
33.906945	1499.252604	17.498355
34.071372	1497.925540	17.503373
34.020321	1498.416335	17.508391
34.315017	1506.085490	17.513408
34.394633	1502.251109	17.518426
34.220096	1509.861602	17.523443
34.569248	1499.573655	17.528461
34.287506	1505.218061	17.533479
34.254021	1505.169605	17.538496
34.786619	1508.208302	17.543514
34.441204	1500.620628	17.548531
34.481645	1482.369378	17.553549
34.380614	1467.324578	17.558567
34.200476	1479.925099	17.563584
34.662612	1489.241163	17.568602
34.199944	1503.178382	17.573619
34.323820	1499.059754	17.578637
34.520849	1508.754439	17.583655
34.262133	1503.359636	17.588672
34.912932	1506.014870	17.593690
34.406213	1504.018890	17.598707
34.432218	1499.690873	17.603725
34.551321	1499.305825	17.608743
34.731356	1500.723861	17.613760
34.771245	1489.985908	17.618778
34.607986	1495.773506	17.623795
34.756861	1510.060995	17.628813
34.925914	1515.718302	17.633831
34.828106	1526.316728	17.638848
34.780021	1518.180369	17.643866
34.760097	1521.115909	17.648883
34.838370	1524.721159	17.653901
34.933479	1532.709690	17.658919
34.990434	1523.460438	17.663936
35.238275	1517.222767	17.668954
34.913059	1521.956762	17.673971
35.128483	1516.818207	17.678989
35.225337	1508.807095	17.684007
34.893202	1517.982417	17.689024
35.337492	1524.133349	17.694042
35.442720	1544.453307	17.699059
35.449601	1546.206026	17.704077
35.575991	1547.818736	17.709095
35.919279	1549.282232	17.714112
36.008017	1522.086865	17.719130
35.781817	1530.702434	17.724147
35.570640	1516.236741	17.729165
35.479079	1514.509513	17.734183
35.556525	1515.552428	17.739200
35.777248	1517.014721	17.744218
35.596069	1521.649530	17.749235
35.842920	1531.858174	17.754253
35.713163	1528.537852	17.759271
35.645003	1537.462503	17.764288
36.243321	1535.375239	17.769306
36.047521	1542.448189	17.774323
35.875814	1539.726455	17.779341
35.991429	1540.495381	17.784359
35.746909	1541.252371	17.789376
35.891276	1553.150393	17.794394
35.856633	1551.358842	17.799411
35.979517	1536.661570	17.804429
35.983021	1546.391407	17.809447
35.813860	1545.855002	17.814464
36.404476	1546.854058	17.819482
35.595155	1538.120737	17.824499
36.164465	1561.224300	17.829517
36.457642	1559.435065	17.834535
36.373895	1569.397812	17.839552
37.337447	1551.337793	17.844570
37.045071	1530.474886	17.849587
37.305729	1516.904721	17.854605
37.099458	1511.538646	17.859623
36.913579	1521.385972	17.864640
37.210535	1503.378886	17.869658
36.850135	1497.181702	17.874675
36.784206	1495.412450	17.879693
37.203167	1479.528263	17.884711
37.157577	1482.237161	17.889728
37.093122	1477.916226	17.894746
37.131888	1482.235974	17.899763
36.770025	1481.753459	17.904781
37.068807	1469.566817	17.909799
36.720185	1469.055543	17.914816
37.058219	1462.266248	17.919834
36.906083	1473.136181	17.924851
36.679118	1475.276898	17.929869
37.092220	1478.445755	17.934887
36.944961	1478.110824	17.939904
36.880706	1474.440954	17.944922
36.726592	1476.543455	17.949939
36.725304	1486.220510	17.954957
37.133043	1497.515591	17.959975
37.107516	1516.889528	17.964992
37.236657	1512.427747	17.970010
37.315049	1519.989758	17.975027
37.476757	1518.653497	17.980045
37.152302	1519.366025	17.985063
36.911590	1528.660677	17.990080
37.020464	1520.883370	17.995098
37.176964	1513.127130	18.000115
37.037143	1509.790760	18.005133
37.571363	1521.516475	18.010151
37.480494	1536.228400	18.015168
37.784492	1544.440261	18.020186
37.433131	1545.851638	18.025203
37.638024	1547.134682	18.030221
37.607995	1535.488484	18.035239
37.799508	1542.099449	18.040256
37.717600	1540.371608	18.045274
37.959874	1530.171962	18.050291
37.521506	1534.624304	18.055309
37.781305	1541.118486	18.060327
37.765888	1538.814373	18.065344
37.612877	1558.325556	18.070362
37.752997	1571.255072	18.075379
37.886917	1571.637164	18.080397
38.278107	1560.312041	18.085415
37.917410	1573.959082	18.090432
38.346070	1576.773463	18.095450
38.172959	1564.729089	18.100467
38.170745	1564.361724	18.105485
38.251973	1569.216539	18.110503
38.356478	1572.510023	18.115520
38.473419	1570.954609	18.120538
38.584882	1568.476394	18.125555
38.491201	1570.276438	18.130573
38.655662	1572.403268	18.135591
38.331814	1558.200808	18.140608
38.334652	1574.346121	18.145626
38.860047	1586.412082	18.150643
38.849708	1589.451943	18.155661
39.220140	1588.593524	18.160679
38.788039	1592.767321	18.165696
38.914753	1591.349446	18.170714
38.926563	1578.319895	18.175731
38.904429	1581.740594	18.180749
39.023221	1572.291945	18.185767
38.609241	1581.764258	18.190784
38.863556	1587.667313	18.195802
39.013300	1588.878775	18.200819
39.172577	1597.588537	18.205837
39.182341	1590.520008	18.210855
39.020245	1600.898232	18.215872
39.218456	1590.684964	18.220890
39.386447	1601.138351	18.225907
39.328900	1586.984171	18.230925
39.429241	1600.086012	18.235943
39.131696	1584.505530	18.240960
39.106474	1584.338006	18.245978
39.087319	1586.743181	18.250995
38.952422	1593.115426	18.256013
39.189373	1592.891391	18.261031
39.489966	1608.494486	18.266048
39.370985	1619.688530	18.271066
39.180282	1617.760771	18.276083
39.190236	1635.526430	18.281101
39.339077	1624.115536	18.286119
39.596475	1614.854168	18.291136
39.420270	1620.850619	18.296154
39.513065	1623.445149	18.301171
39.655735	1644.279659	18.306189
40.088068	1646.305941	18.311207
39.981429	1652.792228	18.316224
40.087875	1656.962078	18.321242
39.948083	1644.357279	18.326259
39.792439	1644.321727	18.331277
40.268567	1640.411356	18.336295
40.352966	1641.100023	18.341312
40.295804	1644.806019	18.346330
40.403491	1635.012948	18.351347
40.450866	1640.600064	18.356365
40.626580	1633.311399	18.361383
40.402584	1620.451078	18.366400
39.910029	1602.692240	18.371418
40.429692	1611.684936	18.376435
40.196909	1631.537503	18.381453
40.576987	1631.331543	18.386471
40.612846	1628.291472	18.391488
40.566579	1632.026763	18.396506
40.451600	1635.565954	18.401523
40.511397	1638.232073	18.406541
40.737063	1639.528227	18.411559
40.824747	1635.239777	18.416576
40.650855	1641.227587	18.421594
40.788042	1645.249458	18.426611
40.805819	1649.573312	18.431629
41.074369	1638.363662	18.436647
40.907571	1636.147732	18.441664
40.860741	1640.734198	18.446682
40.683087	1636.203605	18.451699
40.466037	1639.214059	18.456717
41.056589	1647.012524	18.461735
41.321073	1661.044857	18.466752
41.203608	1665.807157	18.471770
41.612799	1648.524379	18.476787
41.256139	1648.093945	18.481805
41.490371	1622.740279	18.486823
41.232859	1629.495553	18.491840
41.361332	1647.676038	18.496858
41.625279	1641.216390	18.501875
41.424089	1642.136677	18.506893
41.613023	1643.121221	18.511911
41.383425	1648.286055	18.516928
41.490248	1664.608153	18.521946
41.860846	1659.691321	18.526963
41.710993	1664.871129	18.531981
41.669055	1662.680620	18.536999
41.566122	1665.458073	18.542016
41.482776	1652.867756	18.547034
41.850501	1654.848029	18.552051
41.708408	1664.805717	18.557069
41.541517	1661.139575	18.562087
41.447389	1662.659224	18.567104
41.993965	1672.858587	18.572122
41.858324	1657.457354	18.577139
41.694266	1669.532206	18.582157
41.936445	1674.114423	18.587175
42.252989	1678.276526	18.592192
41.982585	1680.713392	18.597210
42.463767	1672.017302	18.602227
41.973446	1677.258887	18.607245
42.267467	1678.976965	18.612263
42.317865	1679.348455	18.617280
42.241315	1683.809742	18.622298
42.639227	1677.578109	18.627315
42.147555	1681.366741	18.632333
42.129139	1674.384710	18.637351
42.699358	1672.932315	18.642368
42.558100	1667.313343	18.647386
42.760974	1665.305582	18.652403
42.813704	1677.409175	18.657421
42.530394	1670.142808	18.662439
42.558714	1674.074028	18.667456
42.363357	1685.552166	18.672474
42.782388	1696.931542	18.677491
42.601954	1702.335091	18.682509
42.788368	1703.641869	18.687527
43.081439	1706.800888	18.692544
42.985029	1708.279979	18.697562
42.942112	1705.029117	18.702579
42.910049	1700.914553	18.707597
43.109189	1700.112974	18.712615
43.067454	1697.614784	18.717632
43.181527	1697.547652	18.722650
43.309663	1687.302007	18.727667
43.012923	1701.974102	18.732685
43.478884	1716.980952	18.737703
43.948513	1717.847078	18.742720
43.445337	1705.351681	18.747738
43.698775	1694.467286	18.752755
43.340907	1693.634734	18.757773
43.563368	1693.751440	18.762791
43.548326	1711.866357	18.767808
43.701169	1720.474114	18.772826
43.733603	1706.087854	18.777843
43.707258	1717.796325	18.782861
43.954868	1723.058094	18.787879
43.879750	1715.490206	18.792896
44.254406	1724.148703	18.797914
44.520541	1717.243043	18.802931
44.189031	1691.417461	18.807949
44.250860	1677.969371	18.812967
44.104583	1674.865698	18.817984
43.973457	1681.242080	18.823002
44.221484	1673.470242	18.828019
44.029606	1683.172026	18.833037
44.168599	1689.867512	18.838055
44.535815	1685.315165	18.843072
44.092786	1714.292871	18.848090
44.175476	1714.393307	18.853107
44.330949	1712.020383	18.858125
44.596609	1712.513568	18.863143
44.694595	1714.560862	18.868160
44.560031	1719.786384	18.873178
45.011076	1707.154561	18.878195
44.904244	1715.519038	18.883213
44.817423	1717.412836	18.888231
45.031696	1706.723466	18.893248
44.638939	1692.603717	18.898266
44.584891	1695.404394	18.903283
44.943271	1709.964304	18.908301
44.846365	1714.736802	18.913319
44.933337	1712.166954	18.918336
44.731668	1715.077845	18.923354
44.803637	1707.889940	18.928371
44.682891	1716.665332	18.933389
44.586796	1708.441934	18.938407
44.866309	1708.616921	18.943424
45.122796	1723.644810	18.948442
45.519967	1735.721254	18.953459
45.205583	1739.593779	18.958477
45.411153	1739.867196	18.963495
45.544405	1737.455622	18.968512
45.516951	1725.721266	18.973530
45.136533	1717.707623	18.978547
45.479576	1721.797847	18.983565
45.759152	1725.377557	18.988583
45.815815	1731.840828	18.993600
45.387457	1729.363613	18.998618
45.938851	1726.558965	19.003635
45.521819	1730.770658	19.008653
45.651549	1735.603733	19.013671
45.771811	1722.981090	19.018688
45.636846	1740.261427	19.023706
45.673631	1732.321929	19.028723
45.804756	1736.631211	19.033741
45.611338	1736.578871	19.038759
45.965803	1730.679163	19.043776
45.598731	1741.559017	19.048794
45.943266	1735.757788	19.053811
45.974967	1745.379363	19.058829
46.150244	1747.031255	19.063847
46.280420	1741.648473	19.068864
46.442884	1745.858495	19.073882
46.356706	1741.052744	19.078899
46.371702	1755.951299	19.083917
46.175569	1751.426283	19.088935
46.463502	1751.567403	19.093952
46.017388	1761.679514	19.098970
46.498286	1763.290549	19.103987
46.656446	1774.658963	19.109005
46.374789	1776.644604	19.114023
46.530463	1769.199361	19.119040
46.686674	1774.298515	19.124058
46.746235	1766.514077	19.129075
46.709911	1768.219045	19.134093
46.906265	1777.368599	19.139111
47.004443	1776.901579	19.144128
46.904706	1774.512753	19.149146
46.908156	1777.649181	19.154163
47.026999	1776.081228	19.159181
46.909242	1784.141873	19.164199
47.342577	1788.495708	19.169216
47.249712	1795.092955	19.174234
47.309715	1796.497787	19.179251
47.770709	1802.195138	19.184269
47.749619	1787.177558	19.189287
47.800959	1784.216385	19.194304
47.432453	1765.142513	19.199322
47.202829	1768.746540	19.204339
47.717471	1765.664131	19.209357
47.445448	1791.848479	19.214375
47.403149	1801.016029	19.219392
47.733539	1797.889463	19.224410
47.994426	1795.764039	19.229427
48.264994	1797.098647	19.234445
47.955268	1793.271451	19.239463
48.239859	1799.435501	19.244480
47.969063	1792.275066	19.249498
47.782376	1803.326708	19.254515
48.290060	1792.345907	19.259533
47.976532	1800.957358	19.264551
48.183906	1795.956837	19.269568
48.081793	1803.845634	19.274586
48.247814	1803.305401	19.279603
47.934887	1797.968659	19.284621
47.803807	1789.642152	19.289639
48.144963	1786.742918	19.294656
48.477719	1790.846080	19.299674
48.114942	1789.803333	19.304691
48.335766	1798.451666	19.309709
48.262413	1817.464042	19.314727
48.528068	1826.559462	19.319744
48.418351	1832.295232	19.324762
48.453450	1818.006645	19.329779
48.587331	1817.189272	19.334797
48.507935	1825.321740	19.339815
48.613138	1819.617699	19.344832
48.725054	1822.189027	19.349850
48.856362	1834.811593	19.354867
49.280962	1844.775742	19.359885
49.085615	1854.317594	19.364903
49.333366	1846.339240	19.369920
49.373539	1842.808898	19.374938
49.091984	1842.406987	19.379955
49.198695	1839.824998	19.384973
49.476215	1853.844135	19.389991
49.673077	1847.601567	19.395008
49.257246	1833.123729	19.400026
49.568650	1835.237336	19.405043
49.507117	1834.113313	19.410061
49.222807	1837.248294	19.415079
49.682302	1838.228689	19.420096
49.623715	1845.361181	19.425114
49.691448	1840.778168	19.430131
49.697522	1838.030742	19.435149
49.704314	1844.370623	19.440167
49.611321	1831.124933	19.445184
49.512598	1831.332309	19.450202
49.494623	1834.491971	19.455219
49.658172	1837.380719	19.460237
49.785901	1852.248141	19.465255
49.981675	1866.416216	19.470272
50.069377	1865.923762	19.475290
49.991847	1865.503291	19.480307
50.146332	1862.411095	19.485325
50.063926	1862.062880	19.490343
50.475070	1854.576562	19.495360
50.560747	1853.018018	19.500378
50.365711	1862.086842	19.505395
50.638541	1860.636136	19.510413
50.158867	1851.934568	19.515431
50.603463	1855.457317	19.520448
50.563639	1857.057767	19.525466
50.784724	1884.715349	19.530483
50.890297	1882.269551	19.535501
50.940350	1885.076876	19.540519
51.254239	1874.843518	19.545536
50.770393	1866.417602	19.550554
50.656817	1864.005264	19.555571
51.056845	1870.181170	19.560589
50.948294	1881.779347	19.565607
51.246101	1883.192131	19.570624
51.480007	1886.338329	19.575642
50.869787	1892.886673	19.580659
51.267919	1874.586874	19.585677
50.916481	1890.382441	19.590695
51.074203	1894.151600	19.595712
51.214705	1883.625464	19.600730
50.873067	1884.889806	19.605747
51.190378	1891.097300	19.610765
51.091082	1904.573497	19.615783
51.524144	1904.905575	19.620800
51.608001	1895.293030	19.625818
51.628714	1896.124306	19.630835
51.971720	1898.065000	19.635853
52.044116	1897.867761	19.640871
51.910342	1889.483974	19.645888
51.971815	1898.840122	19.650906
52.098898	1901.649877	19.655923
52.241834	1897.930118	19.660941
51.793523	1899.898829	19.665959
52.367972	1902.901168	19.670976
52.204320	1903.532027	19.675994
51.918766	1906.319427	19.681011
51.977873	1892.546830	19.686029
52.095257	1900.192536	19.691047
52.226021	1897.743164	19.696064
52.310292	1899.906713	19.701082
52.345096	1903.557224	19.706099
52.284398	1899.575868	19.711117
52.243877	1920.040081	19.716135
52.301368	1931.931495	19.721152
52.300604	1926.823805	19.726170
52.331525	1937.947841	19.731187
52.512997	1928.950578	19.736205
52.570840	1929.496023	19.741223
52.506988	1942.377479	19.746240
53.179727	1944.340063	19.751258
53.418984	1956.238268	19.756275
53.593952	1941.514092	19.761293
53.808758	1928.444796	19.766311
53.493367	1916.327996	19.771328
53.469845	1908.174380	19.776346
53.565850	1905.281977	19.781363
53.573128	1902.935677	19.786381
53.237231	1902.172112	19.791399
53.075962	1908.096332	19.796416
53.426516	1906.874684	19.801434
52.972568	1913.882401	19.806451
53.281874	1911.233461	19.811469
53.647637	1932.129322	19.816487
53.270010	1941.800748	19.821504
53.612601	1952.009795	19.826522
53.547002	1948.456361	19.831539
54.018683	1941.805387	19.836557
53.765508	1939.097633	19.841575
53.689627	1941.264624	19.846592
54.025272	1935.285280	19.851610
54.032055	1934.960904	19.856627
54.314763	1941.767581	19.861645
54.108687	1934.800499	19.866663
54.019615	1947.730414	19.871680
54.448924	1933.406890	19.876698
53.839294	1945.405207	19.881715
54.211670	1949.603824	19.886733
54.388775	1958.040202	19.891751
54.442591	1958.962852	19.896768
54.532958	1966.203253	19.901786
54.486260	1967.403905	19.906803
54.578651	1967.762361	19.911821
54.733502	1968.571868	19.916839
54.747461	1970.732284	19.921856
55.080555	1959.398953	19.926874
54.864824	1964.196084	19.931891
55.102153	1955.802705	19.936909
55.254269	1959.486988	19.941927
54.858598	1961.192112	19.946944
54.985477	1961.768469	19.951962
54.681322	1968.561909	19.956979
55.089932	1959.525324	19.961997
54.845093	1969.627733	19.967015
54.791913	1988.282296	19.972032
55.014629	1980.722537	19.977050
54.853555	2000.658208	19.982067
55.086347	1998.185268	19.987085
55.400220	1990.213825	19.992103
55.435127	1992.755588	19.997120
55.365636	1985.875745	20.002138
55.512838	2011.951823	20.007155
55.795496	2017.885398	20.012173
55.811935	2011.199985	20.017191
55.672198	2016.616208	20.022208
56.040733	2013.919279	20.027226
56.159088	2019.144837	20.032243
56.140154	2018.668031	20.037261
56.306233	2019.007422	20.042279
55.961512	2016.658254	20.047296
56.456969	2012.791641	20.052314
55.969537	2012.956766	20.057331
56.769193	2017.277297	20.062349
56.376808	2016.860430	20.067367
56.250938	2012.078277	20.072384
56.264689	2023.776418	20.077402
56.343778	2017.892976	20.082419
56.291100	2017.341832	20.087437
56.248224	2013.069734	20.092455
56.365970	2015.400586	20.097472
56.546127	2018.579313	20.102490
56.222166	2046.154433	20.107507
56.617389	2040.869273	20.112525
56.815013	2046.843089	20.117543
56.666507	2038.193176	20.122560
56.881276	2047.130025	20.127578
56.802378	2043.053617	20.132595
57.298360	2037.123323	20.137613
56.719536	2053.950831	20.142631
56.748836	2072.303900	20.147648
57.329484	2073.255632	20.152666
57.222931	2065.599861	20.157683
57.578213	2058.819857	20.162701
57.978565	2056.263122	20.167719
57.557501	2071.307653	20.172736
57.664832	2048.395890	20.177754
57.983246	2067.580626	20.182771
57.825200	2068.615056	20.187789
57.909033	2057.135261	20.192807
58.073840	2061.947092	20.197824
58.049507	2045.480126	20.202842
57.943788	2055.007094	20.207859
58.007645	2056.939218	20.212877
58.082973	2052.939282	20.217895
57.993788	2058.723313	20.222912
58.147449	2056.889564	20.227930
58.108180	2058.600562	20.232947
57.870116	2060.974667	20.237965
57.885107	2058.709149	20.242983
58.251333	2074.465834	20.248000
58.373750	2075.448015	20.253018
58.210068	2082.157668	20.258035
58.517263	2074.136306	20.263053
58.826707	2075.431054	20.268071
58.664786	2074.066145	20.273088
58.926227	2069.854758	20.278106
59.158474	2084.753752	20.283123
58.792829	2075.934796	20.288141
59.175488	2071.885645	20.293159
59.157907	2081.125058	20.298176
58.872494	2070.005062	20.303194
58.736417	2079.730941	20.308211
58.803917	2081.232584	20.313229
59.232610	2076.766413	20.318247
58.820445	2084.683755	20.323264
59.027397	2068.258066	20.328282
58.946690	2081.868341	20.333299
59.096966	2085.482690	20.338317
59.481408	2091.453996	20.343335
59.043718	2099.562948	20.348352
59.470165	2103.906990	20.353370
59.317779	2096.679606	20.358387
59.513330	2099.756012	20.363405
59.606478	2111.373783	20.368423
59.773053	2127.504428	20.373440
59.998891	2121.585281	20.378458
60.078531	2120.594391	20.383475
59.822914	2131.748988	20.388493
60.210972	2115.070508	20.393511
59.947186	2122.383086	20.398528
59.997095	2118.098383	20.403546
59.838408	2119.145716	20.408563
60.262179	2109.102493	20.413581
60.387240	2119.436763	20.418599
60.335434	2119.787754	20.423616
60.581669	2120.493004	20.428634
60.310141	2102.961409	20.433651
60.644336	2131.638251	20.438669
60.745293	2132.698187	20.443687
60.760940	2138.979251	20.448704
60.982572	2139.752735	20.453722
61.203178	2144.942149	20.458739
61.022707	2137.331429	20.463757
61.209716	2141.267448	20.468775
60.829917	2143.709078	20.473792
60.929593	2143.212077	20.478810
61.038621	2146.672049	20.483827
60.904337	2156.223483	20.488845
61.125985	2143.615040	20.493863
61.355225	2152.261592	20.498880
60.839458	2141.586660	20.503898
61.204426	2154.171664	20.508915
61.205325	2166.896557	20.513933
60.881567	2169.344086	20.518951
61.363849	2175.286267	20.523968
61.521832	2181.538709	20.528986
61.561355	2183.767366	20.534003
61.744313	2188.436289	20.539021
62.099325	2194.481391	20.544039
61.897416	2200.268158	20.549056
62.463668	2196.981682	20.554074
62.353745	2186.794924	20.559091
62.541901	2190.902997	20.564109
62.151770	2167.331391	20.569127
62.303001	2159.008620	20.574144
62.314797	2177.486941	20.579162
62.646310	2183.518994	20.584179
62.367579	2187.708153	20.589197
62.635588	2183.732441	20.594215
62.588489	2193.806848	20.599232
62.830197	2182.294180	20.604250
62.737598	2183.386695	20.609267
62.379129	2187.535687	20.614285
63.094462	2176.864762	20.619303
62.742424	2176.358355	20.624320
62.961674	2183.923399	20.629338
62.804396	2180.924779	20.634355
62.919203	2182.628439	20.639373
63.083339	2178.605922	20.644391
62.891887	2187.946959	20.649408
62.975826	2186.169790	20.654426
63.296369	2194.194833	20.659443
63.071786	2205.392383	20.664461
63.254520	2207.541083	20.669479
63.515105	2206.546270	20.674496
63.619983	2210.891713	20.679514
63.599433	2211.271593	20.684531
63.623587	2201.166403	20.689549
63.692689	2202.151496	20.694567
63.311304	2210.485828	20.699584
63.466183	2206.495934	20.704602
63.664339	2206.586742	20.709619
63.738815	2229.326072	20.714637
63.891275	2229.955885	20.719655
63.977513	2237.418535	20.724672
63.853190	2237.598456	20.729690
64.401741	2244.601675	20.734707
63.862250	2245.050184	20.739725
64.231139	2242.163999	20.744743
64.199288	2251.397408	20.749760
64.153388	2277.782792	20.754778
64.633280	2268.913565	20.759795
64.411193	2270.602044	20.764813
65.014711	2264.931235	20.769831
64.945421	2271.099036	20.774848
64.952425	2267.260520	20.779866
64.976999	2259.380441	20.784883
65.097226	2262.416378	20.789901
65.135678	2251.638569	20.794919
65.128182	2269.769035	20.799936
65.008783	2265.986246	20.804954
65.117386	2267.232906	20.809971
65.406634	2279.427604	20.814989
64.944232	2263.253643	20.820007
65.093262	2264.630029	20.825024
65.085759	2267.822299	20.830042
65.704745	2283.246706	20.835059
65.326645	2286.596275	20.840077
65.442797	2284.356327	20.845095
65.298034	2282.111072	20.850112
65.442385	2290.258580	20.855130
65.621405	2296.765251	20.860147
65.727495	2312.316366	20.865165
66.134999	2312.948129	20.870183
66.086038	2313.437227	20.875200
65.918020	2322.254038	20.880218
66.033058	2310.253190	20.885235
66.573165	2321.155578	20.890253
66.735402	2311.430421	20.895271
66.684532	2321.490771	20.900288
66.688916	2320.350112	20.905306
66.812097	2320.820213	20.910323
66.158527	2326.172840	20.915341
66.386792	2316.589120	20.920359
66.248851	2319.588797	20.925376
66.218432	2327.606948	20.930394
66.712373	2344.849978	20.935411
66.879313	2346.762546	20.940429
67.068244	2336.666060	20.945447
67.233101	2342.053716	20.950464
67.281260	2341.694150	20.955482
67.436004	2334.099195	20.960499
67.436931	2338.513421	20.965517
67.614739	2342.408103	20.970535
67.737623	2329.970541	20.975552
67.977430	2333.115659	20.980570
67.879762	2331.708616	20.985587
67.473426	2336.804071	20.990605
67.899067	2331.271678	20.995623
67.541910	2335.960020	21.000640
67.549948	2342.003465	21.005658
67.590466	2325.233773	21.010675
67.456058	2324.470746	21.015693
67.495160	2327.338619	21.020711
67.557322	2333.435120	21.025728
67.441882	2356.091263	21.030746
68.029890	2351.991967	21.035763
68.165189	2361.455480	21.040781
68.079137	2364.392265	21.045799
68.135726	2368.119595	21.050816
68.311006	2370.119561	21.055834
68.622987	2372.687054	21.060851
68.738532	2389.499390	21.065869
69.087163	2389.652140	21.070887
68.968456	2371.458614	21.075904
69.015229	2365.567191	21.080922
68.871011	2351.040635	21.085939
68.865419	2360.879765	21.090957
69.043126	2370.971270	21.095975
69.296699	2369.801831	21.100992
69.407252	2378.593901	21.106010
69.624114	2382.159130	21.111027
69.415128	2366.849223	21.116045
69.100994	2358.507581	21.121063
69.253876	2362.005037	21.126080
69.621236	2376.401706	21.131098
69.687857	2371.925208	21.136115
69.560777	2376.594242	21.141133
69.753288	2368.710569	21.146151
69.716167	2368.117474	21.151168
69.517511	2380.729662	21.156186
69.915916	2363.992122	21.161203
69.716423	2382.960886	21.166221
69.842782	2374.802137	21.171239
69.641382	2381.393554	21.176256
69.860452	2399.424731	21.181274
69.938564	2405.209591	21.186291
69.764231	2408.321591	21.191309
69.925004	2411.630759	21.196327
70.209989	2422.027974	21.201344
70.166373	2431.911815	21.206362
70.945984	2420.272490	21.211379
70.841076	2418.699521	21.216397
70.846543	2419.416226	21.221415
70.958745	2429.528238	21.226432
71.026977	2434.061873	21.231450
71.206522	2428.969298	21.236467
71.006887	2430.975913	21.241485
70.875942	2424.324715	21.246503
71.204838	2424.170708	21.251520
71.069038	2426.464589	21.256538
71.320621	2423.544019	21.261555
71.446486	2425.041562	21.266573
71.014051	2428.956401	21.271591
71.589332	2428.576654	21.276608
71.177178	2439.929375	21.281626
71.591922	2450.285089	21.286643
71.533120	2447.872269	21.291661
71.651022	2454.755421	21.296679
71.800355	2449.002718	21.301696
71.603075	2452.529909	21.306714
71.840891	2457.428219	21.311731
71.843774	2469.057632	21.316749
71.840394	2465.367230	21.321767
71.809821	2462.167708	21.326784
71.971550	2468.484802	21.331802
72.013835	2468.758840	21.336819
72.112382	2481.114926	21.341837
72.130597	2478.418329	21.346855
72.576925	2485.770419	21.351872
72.689264	2496.632208	21.356890
72.735371	2476.483690	21.361907
72.802578	2490.842865	21.366925
72.653401	2494.001510	21.371943
73.364093	2483.432711	21.376960
73.301810	2490.746022	21.381978
72.957643	2487.185741	21.386995
73.041197	2481.864734	21.392013
73.189936	2490.690320	21.397031
73.364201	2493.600648	21.402048
72.762654	2496.108893	21.407066
73.220048	2506.735729	21.412083
73.397149	2515.209420	21.417101
73.614761	2520.508899	21.422119
73.636731	2509.897599	21.427136
73.452873	2522.027172	21.432154
73.858646	2512.588594	21.437171
73.930588	2514.047422	21.442189
73.546338	2524.461793	21.447207
73.938270	2538.220931	21.452224
73.882043	2538.583685	21.457242
74.334675	2538.936759	21.462259
74.645666	2536.342552	21.467277
74.769765	2535.747612	21.472295
74.977688	2525.831907	21.477312
74.622387	2525.775999	21.482330
74.793788	2528.576578	21.487347
74.701507	2530.768013	21.492365
74.873383	2530.303752	21.497383
74.982626	2531.544620	21.502400
74.938012	2532.759734	21.507418
74.926427	2531.641972	21.512435
75.095559	2519.431641	21.517453
75.173106	2517.488966	21.522471
75.534293	2520.585328	21.527488
75.167193	2522.819024	21.532506
75.656935	2516.250250	21.537523
75.592327	2509.591202	21.542541
75.287910	2514.816321	21.547559
75.559874	2506.152174	21.552576
75.163436	2523.257905	21.557594
75.156395	2519.390350	21.562611
75.540883	2514.853806	21.567629
75.305259	2538.302272	21.572647
75.699257	2536.214395	21.577664
75.394027	2548.396326	21.582682
75.659555	2544.395148	21.587699
75.689444	2560.271093	21.592717
75.788380	2579.357113	21.597735
76.169992	2574.409633	21.602752
75.768020	2585.902895	21.607770
76.271211	2565.957061	21.612787
76.531109	2576.213062	21.617805
76.613862	2579.423157	21.622823
77.004204	2584.152809	21.627840
76.841613	2595.543534	21.632858
77.149182	2583.509872	21.637875
77.107738	2581.511265	21.642893
76.831666	2582.272532	21.647911
77.479967	2578.793100	21.652928
77.051587	2598.169021	21.657946
77.474534	2581.169726	21.662963
77.327408	2587.576683	21.667981
77.248761	2591.692535	21.672999
77.567572	2580.438469	21.678016
77.556175	2592.075846	21.683034
77.502131	2586.266152	21.688051
77.752137	2575.253368	21.693069
77.587501	2577.974452	21.698087
77.918652	2576.331576	21.703104
77.560098	2578.015080	21.708122
77.584346	2581.446249	21.713139
77.456720	2586.934681	21.718157
77.286262	2606.745919	21.723175
77.715856	2617.208538	21.728192
77.668330	2627.924404	21.733210
77.629784	2630.122721	21.738227
78.365399	2638.123501	21.743245
77.871852	2649.999246	21.748263
77.954506	2644.772422	21.753280
78.254763	2666.085397	21.758298
78.501903	2680.091410	21.763315
78.738299	2678.888569	21.768333
78.707757	2674.048137	21.773351
78.973991	2672.802179	21.778368
79.035438	2677.125601	21.783386
78.827465	2671.394458	21.788403
79.181386	2681.378312	21.793421
79.273492	2686.005709	21.798439
79.419644	2677.130772	21.803456
80.274043	2680.427937	21.808474
80.087296	2677.840367	21.813491
80.425628	2655.465487	21.818509
80.055714	2657.812259	21.823527
80.012562	2645.995943	21.828544
80.260384	2655.474899	21.833562
80.224606	2651.569542	21.838579
80.128942	2643.614850	21.843597
80.068587	2644.187332	21.848615
80.347674	2640.963768	21.853632
80.223255	2643.179426	21.858650
80.259959	2650.959500	21.863667
80.263416	2644.542677	21.868685
80.229892	2646.447662	21.873703
80.514849	2648.645278	21.878720
80.402177	2671.231548	21.883738
80.312802	2662.971098	21.888755
80.833730	2664.519914	21.893773
80.592011	2671.109455	21.898791
80.586912	2678.930308	21.903808
80.679425	2680.715657	21.908826
80.681186	2700.724923	21.913843
80.907299	2702.383480	21.918861
80.856995	2713.172301	21.923879
81.436072	2708.681890	21.928896
81.323650	2710.213325	21.933914
81.238531	2730.175178	21.938931
81.671557	2722.731480	21.943949
81.576261	2732.030972	21.948967
81.897094	2736.491462	21.953984
81.867586	2735.492390	21.959002
81.757838	2732.971610	21.964019
82.036689	2727.247400	21.969037
81.678387	2735.214435	21.974055
82.150625	2750.743480	21.979072
82.429292	2758.658814	21.984090
82.281264	2764.199497	21.989107
82.561669	2756.440467	21.994125
82.323361	2761.994098	21.999143
82.337724	2765.454499	22.004160
82.401564	2760.746469	22.009178
82.369144	2769.884420	22.014195
82.517646	2764.769503	22.019213
82.683572	2778.103624	22.024231
82.810654	2776.815694	22.029248
83.214089	2784.949391	22.034266
83.345335	2784.669389	22.039283
83.283450	2778.333383	22.044301
83.369048	2776.285413	22.049319
83.307272	2776.462877	22.054336
83.612836	2774.801375	22.059354
83.629354	2781.676230	22.064371
83.695900	2784.320568	22.069389
83.597806	2784.497735	22.074407
83.554806	2780.401815	22.079424
83.854104	2788.552328	22.084442
83.579522	2797.534255	22.089459
84.004416	2806.873027	22.094477
84.037142	2806.685678	22.099495
83.670917	2809.792460	22.104512
84.166024	2812.309690	22.109530
84.259946	2812.918100	22.114547
84.504602	2804.936617	22.119565
84.484508	2819.890026	22.124583
84.445380	2831.875458	22.129600
84.911621	2835.190737	22.134618
84.656273	2828.705190	22.139635
84.730839	2827.150354	22.144653
84.905899	2828.875232	22.149671
84.953135	2828.651628	22.154688
84.949392	2827.736871	22.159706
84.929704	2850.664716	22.164723
85.200828	2844.887017	22.169741
85.329843	2856.896257	22.174759
85.443961	2853.623928	22.179776
85.589693	2850.801869	22.184794
85.809989	2853.649938	22.189811
86.008595	2840.695144	22.194829
86.003276	2848.848782	22.199847
85.686070	2854.335958	22.204864
85.839718	2851.290159	22.209882
86.233724	2863.542220	22.214899
86.719173	2859.392815	22.219917
86.427201	2869.268567	22.224935
86.863050	2880.788559	22.229952
86.758391	2850.513284	22.234970
86.640596	2844.910870	22.239987
86.697961	2831.567234	22.245005
86.917352	2853.601282	22.250023
86.828017	2854.819086	22.255040
87.070772	2864.993076	22.260058
87.098578	2867.807209	22.265075
87.161476	2861.667077	22.270093
86.950368	2865.122238	22.275111
87.404232	2862.391776	22.280128
87.423603	2863.990027	22.285146
86.836147	2856.839689	22.290163
87.114513	2850.273422	22.295181
86.794631	2868.718797	22.300199
87.086605	2894.972635	22.305216
87.561015	2897.055914	22.310234
87.435926	2899.642177	22.315251
87.756817	2904.987714	22.320269
87.712786	2910.722673	22.325287
87.860753	2907.379782	22.330304
88.018265	2912.159032	22.335322
88.008520	2913.658954	22.340339
88.207821	2904.107412	22.345357
88.504074	2920.701891	22.350375
88.438098	2937.738512	22.355392
88.741444	2931.499567	22.360410
88.424728	2952.458997	22.365427
88.999168	2934.360305	22.370445
88.819003	2936.098618	22.375463
88.822456	2931.278471	22.380480
89.462363	2939.000354	22.385498
89.049650	2946.998141	22.390515
89.351402	2935.858445	22.395533
89.545842	2937.811621	22.400551
89.340025	2937.698725	22.405568
89.555109	2936.364746	22.410586
89.282791	2935.221537	22.415603
89.602478	2929.037765	22.420621
89.616382	2933.829728	22.425639
89.372511	2945.252644	22.430656
89.936636	2950.421395	22.435674
90.140963	2965.068186	22.440691
90.185268	2959.743658	22.445709
90.070985	2956.451570	22.450727
90.172646	2960.290096	22.455744
90.378238	2947.254927	22.460762
90.345211	2954.129385	22.465779
90.663601	2970.906867	22.470797
90.798385	2974.817874	22.475815
90.657648	2983.931724	22.480832
90.780085	2976.332936	22.485850
90.838760	2979.773070	22.490867
91.072323	2968.574542	22.495885
90.737595	2972.285579	22.500903
90.729197	2980.332318	22.505920
91.259002	2982.159614	22.510938
91.181013	3002.444252	22.515955
91.378543	3009.578659	22.520973
91.475260	3001.186888	22.525991
91.373883	3003.150371	22.531008
91.663484	2993.887781	22.536026
91.108905	3005.608532	22.541043
91.550043	3015.178203	22.546061
91.981524	3025.704174	22.551079
92.037821	3033.384355	22.556096
92.047844	3025.926555	22.561114
92.248643	3040.197632	22.566131
92.258939	3049.503487	22.571149
92.862315	3052.474509	22.576167
92.621797	3048.948543	22.581184
92.830780	3050.819411	22.586202
92.639623	3051.074554	22.591219
92.917514	3050.333320	22.596237
92.899971	3042.971403	22.601255
92.853993	3052.608597	22.606272
92.976826	3049.181248	22.611290
93.070579	3054.506102	22.616307
93.287981	3073.842441	22.621325
93.639429	3076.169287	22.626343
93.583088	3085.284605	22.631360
93.633851	3087.990657	22.636378
93.655282	3085.834355	22.641395
93.276359	3089.696813	22.646413
93.539194	3075.187942	22.651431
93.535480	3096.178127	22.656448
94.034080	3094.085493	22.661466
93.825275	3103.262628	22.666483
94.004319	3117.099192	22.671501
94.285531	3113.237007	22.676519
94.297826	3115.061251	22.681536
94.205338	3128.684039	22.686554
94.095065	3136.170934	22.691571
94.460206	3142.883621	22.696589
94.503340	3140.926082	22.701607
94.683230	3144.255675	22.706624
95.262894	3135.452935	22.711642
95.704461	3142.481333	22.716659
96.138801	3120.378890	22.721677
95.987277	3112.111147	22.726695
96.109617	3110.390912	22.731712
96.357430	3105.923632	22.736730
95.938905	3090.890340	22.741747
96.190441	3081.100143	22.746765
96.278526	3072.748341	22.751783
95.932665	3085.040158	22.756800
96.079508	3071.959476	22.761818
96.203868	3083.719669	22.766835
96.221525	3077.101506	22.771853
96.176954	3077.606436	22.776871
95.866843	3078.676885	22.781888
95.985241	3085.154341	22.786906
95.868883	3105.358448	22.791923
96.036145	3112.873093	22.796941
96.597601	3117.030948	22.801959
96.461102	3134.668008	22.806976
96.467215	3132.499270	22.811994
96.569176	3138.433808	22.817011
96.552018	3129.851733	22.822029
97.020381	3160.860235	22.827047
97.150724	3163.874404	22.832064
96.999836	3166.412220	22.837082
97.015449	3164.799770	22.842099
97.446984	3173.675079	22.847117
97.783609	3174.933938	22.852135
97.625863	3184.362128	22.857152
97.863454	3168.664449	22.862170
98.290392	3172.739038	22.867187
98.171049	3175.513764	22.872205
98.557573	3174.653395	22.877223
98.016416	3180.636343	22.882240
98.287113	3173.311773	22.887258
98.391854	3176.627413	22.892275
98.773071	3196.216359	22.897293
99.025128	3199.321051	22.902311
99.005617	3209.572856	22.907328
98.855991	3203.515343	22.912346
98.866364	3202.843896	22.917363
99.095717	3206.631070	22.922381
99.115397	3202.037288	22.927399
98.915894	3212.699932	22.932416
99.288818	3203.819899	22.937434
98.898036	3214.179511	22.942451
98.937520	3239.068198	22.947469
99.403648	3232.437675	22.952487
99.267933	3242.521698	22.957504
99.444994	3252.372158	22.962522
100.107094	3258.661423	22.967539
99.910202	3260.912371	22.972557
99.959159	3252.361823	22.977575
99.883325	3269.694528	22.982592
100.316234	3254.866839	22.987610
100.078166	3273.061382	22.992627
100.499460	3288.239943	22.997645
100.668376	3283.393922	23.002663
100.817668	3292.376959	23.007680
100.704672	3287.759012	23.012698
101.207820	3273.080722	23.017715
100.971419	3287.475450	23.022733
101.142088	3281.246873	23.027751
101.171263	3297.897305	23.032768
101.004648	3306.442005	23.037786
101.233888	3317.085844	23.042803
101.259245	3319.478421	23.047821
101.422267	3316.247520	23.052839
101.465434	3313.288390	23.057856
101.428631	3316.973508	23.062874
101.832652	3343.060382	23.067891
101.711318	3350.120471	23.072909
101.914759	3352.135598	23.077927
102.020564	3348.434227	23.082944
102.103322	3342.113066	23.087962
102.353446	3368.198640	23.092979
102.192544	3373.493243	23.097997
102.495848	3365.448633	23.103015
102.708119	3375.719335	23.108032
102.823471	3372.185671	23.113050
102.686717	3363.797243	23.118067
102.721154	3380.111070	23.123085
103.186473	3388.084863	23.128103
103.268203	3404.318066	23.133120
103.534828	3402.541676	23.138138
103.564086	3391.072273	23.143155
103.482558	3401.442326	23.148173
103.673250	3393.510403	23.153191
103.460418	3396.366363	23.158208
103.966860	3407.250285	23.163226
104.106996	3407.523526	23.168243
104.131575	3417.459129	23.173261
104.654897	3413.268283	23.178279
104.253464	3425.112859	23.183296
104.262040	3418.894475	23.188314
104.334219	3417.469896	23.193331
104.518391	3416.555550	23.198349
104.499827	3410.102285	23.203367
104.510716	3435.054279	23.208384
104.679801	3446.182948	23.213402
105.041886	3453.744700	23.218419
104.820270	3447.638357	23.223437
105.633392	3439.873247	23.228455
105.324563	3440.565161	23.233472
105.181302	3443.941917	23.238490
105.436768	3449.849634	23.243507
105.721658	3467.168623	23.248525
106.198923	3465.326711	23.253543
105.618642	3467.242220	23.258560
105.628485	3463.875182	23.263578
105.990998	3458.385307	23.268595
105.804781	3481.672702	23.273613
106.216343	3498.575520	23.278631
106.323215	3501.533791	23.283648
106.359315	3501.012805	23.288666
106.492655	3479.135574	23.293683
106.694985	3486.980040	23.298701
106.821620	3499.123637	23.303719
106.971242	3514.294554	23.308736
107.222145	3515.032960	23.313754
107.068494	3517.607115	23.318771
106.881831	3525.343828	23.323789
107.004035	3527.340118	23.328807
106.904461	3527.192733	23.333824
107.192864	3532.511179	23.338842
107.708520	3551.403949	23.343859
107.528319	3547.439158	23.348877
107.503621	3556.641650	23.353895
107.591372	3579.026831	23.358912
107.875478	3582.268432	23.363930
108.430944	3578.385225	23.368947
108.159740	3582.824891	23.373965
108.521842	3578.919697	23.378983
108.393927	3578.764789	23.384000
108.889117	3588.588094	23.389018
108.965855	3590.757654	23.394035
108.968477	3596.423347	23.399053
109.203717	3602.446670	23.404071
108.817865	3598.620179	23.409088
109.192444	3592.673929	23.414106
109.422307	3591.574069	23.419123
109.134187	3597.461820	23.424141
109.521322	3603.034451	23.429159
109.492294	3588.891441	23.434176
109.322513	3597.767928	23.439194
109.481060	3608.964598	23.444211
109.578243	3620.878903	23.449229
109.484543	3623.601045	23.454247
109.875774	3623.921777	23.459264
110.287614	3635.648666	23.464282
110.432972	3639.471085	23.469299
109.850246	3646.977630	23.474317
110.200025	3652.204873	23.479335
110.448079	3668.720716	23.484352
110.549917	3689.489929	23.489370
110.953174	3681.456200	23.494387
110.893380	3685.614108	23.499405
110.805570	3679.728480	23.504423
111.378018	3685.125243	23.509440
110.985772	3701.478021	23.514458
111.407122	3702.937102	23.519475
111.334022	3705.304275	23.524493
111.616318	3709.388340	23.529511
111.929309	3696.236372	23.534528
111.909412	3711.842980	23.539546
111.956442	3721.169152	23.544563
111.754094	3730.710556	23.549581
111.972070	3724.403118	23.554599
112.055566	3726.197559	23.559616
112.454857	3748.039765	23.564634
112.924366	3751.934243	23.569651
113.162516	3744.648643	23.574669
113.304967	3752.561406	23.579687
113.704314	3742.507784	23.584704
113.199773	3734.611824	23.589722
113.675549	3730.287411	23.594739
113.360590	3717.973054	23.599757
113.776948	3727.323246	23.604775
114.011170	3732.671581	23.609792
113.584888	3734.411278	23.614810
113.845001	3737.117891	23.619827
114.169571	3734.105490	23.624845
113.787758	3735.595316	23.629863
113.903065	3732.141895	23.634880
113.766513	3746.976068	23.639898
114.263687	3739.183095	23.644915
114.311535	3770.177656	23.649933
114.266157	3774.761166	23.654951
114.298804	3771.839909	23.659968
113.722643	3776.058753	23.664986
114.423419	3794.783040	23.670003
114.651292	3803.072273	23.675021
114.742856	3803.779541	23.680039
115.151200	3806.506556	23.685056
114.912660	3838.426938	23.690074
115.412049	3830.147323	23.695091
115.582467	3833.548317	23.700109
115.719682	3834.125993	23.705127
115.897425	3833.110321	23.710144
115.562331	3841.116210	23.715162
116.076908	3847.050165	23.720179
115.993164	3857.587426	23.725197
116.111150	3855.804443	23.730215
116.313743	3848.315216	23.735232
116.253974	3861.024161	23.740250
116.405930	3865.673913	23.745267
116.485565	3885.093085	23.750285
116.775590	3892.753576	23.755303
116.659363	3886.014274	23.760320
116.805721	3884.512040	23.765338
117.028491	3886.222462	23.770355
116.978194	3897.622357	23.775373
117.200812	3904.334123	23.780391
117.190979	3915.827742	23.785408
116.997854	3911.704359	23.790426
117.470782	3925.391902	23.795443
117.861092	3943.045195	23.800461
117.759880	3946.642283	23.805479
118.283614	3931.394603	23.810496
118.105623	3952.378913	23.815514
118.212080	3939.752221	23.820531
118.482197	3952.445316	23.825549
118.487701	3971.561874	23.830567
118.908466	3956.118185	23.835584
118.770887	3965.503750	23.840602
118.573081	3960.833078	23.845619
118.770229	3962.871768	23.850637
119.122906	3991.735627	23.855655
119.342601	3987.291640	23.860672
119.533477	4000.425047	23.865690
119.549781	4000.314417	23.870707
119.668439	3999.743945	23.875725
119.514445	4007.274704	23.880743
119.763058	4004.831515	23.885760
119.408027	4020.126078	23.890778
119.522971	4022.320096	23.895795
119.962858	4018.949993	23.900813
120.256331	4044.937412	23.905831
119.982812	4049.354756	23.910848
120.233261	4053.993015	23.915866
120.698427	4058.775724	23.920883
120.679157	4072.158884	23.925901
120.962737	4084.505361	23.930919
121.472078	4075.491267	23.935936
121.729772	4073.610368	23.940954
121.610818	4066.861201	23.945971
121.696334	4064.011865	23.950989
121.601446	4062.160091	23.956007
122.122563	4055.669355	23.961024
121.638395	4057.590311	23.966042
121.817258	4062.203785	23.971059
122.159150	4075.921775	23.976077
121.787313	4077.857244	23.981095
122.272064	4081.924493	23.986112
121.955190	4085.848203	23.991130
122.740106	4096.134216	23.996147
122.876948	4105.239471	24.001165
122.712805	4113.825938	24.006183
122.802733	4109.383280	24.011200
122.850994	4113.031301	24.016218
122.886540	4109.220489	24.021235
123.195362	4114.824358	24.026253
123.382455	4133.060681	24.031271
123.646903	4130.813290	24.036288
123.830318	4139.987251	24.041306
123.934002	4133.793026	24.046323
124.370718	4141.927455	24.051341
123.595030	4138.836531	24.056359
124.070656	4135.420732	24.061376
124.183377	4144.487869	24.066394
124.389236	4155.609003	24.071411
124.296732	4157.142405	24.076429
124.378355	4159.877012	24.081447
124.379773	4158.777457	24.086464
124.642239	4168.125390	24.091482
124.783080	4189.628229	24.096499
124.804108	4196.996689	24.101517
124.552200	4201.110490	24.106535
124.875241	4204.265471	24.111552
124.664085	4219.811666	24.116570
124.840917	4242.460654	24.121587
125.635153	4236.419228	24.126605
125.764900	4259.143740	24.131623
125.976785	4264.001437	24.136640
125.734928	4257.655980	24.141658
126.143497	4259.128646	24.146675
126.570273	4270.560621	24.151693
126.417369	4274.839588	24.156711
126.896322	4282.940339	24.161728
126.622959	4280.103803	24.166746
127.020035	4278.313242	24.171763
127.212935	4278.213195	24.176781
127.273854	4270.638903	24.181799
127.416015	4275.192360	24.186816
127.365376	4289.651417	24.191834
127.504055	4299.480931	24.196851
127.823915	4305.236990	24.201869
127.513682	4305.764595	24.206887
127.856872	4302.898231	24.211904
127.633981	4314.265135	24.216922
127.949385	4318.819115	24.221939
128.325346	4321.662210	24.226957
128.482052	4330.905662	24.231975
128.632197	4326.546304	24.236992
128.388184	4333.642463	24.242010
128.705579	4334.863652	24.247027
128.731648	4349.867208	24.252045
128.539753	4352.448606	24.257063
128.947655	4349.216797	24.262080
128.879696	4366.690374	24.267098
128.993824	4368.222727	24.272115
129.703053	4371.375746	24.277133
129.330121	4382.263131	24.282151
130.020845	4395.639497	24.287168
130.104896	4392.789556	24.292186
130.206034	4412.731060	24.297203
130.587132	4405.254201	24.302221
130.313262	4401.586574	24.307239
130.643819	4405.779394	24.312256
130.509108	4411.758643	24.317274
130.618694	4416.037586	24.322291
130.997044	4410.180962	24.327309
130.702120	4435.229973	24.332327
131.037188	4431.951911	24.337344
131.294750	4432.521930	24.342362
131.348057	4423.118787	24.347379
131.588592	4447.260395	24.352397
131.774407	4457.903138	24.357415
131.782267	4455.952051	24.362432
131.887726	4458.529218	24.367450
131.427634	4472.926171	24.372467
131.685597	4474.797390	24.377485
131.801047	4492.782570	24.382503
132.168485	4493.918726	24.387520
132.475525	4505.748637	24.392538
132.622309	4522.395908	24.397555
132.878575	4523.658711	24.402573
132.529077	4520.665408	24.407591
132.977863	4516.592896	24.412608
133.095499	4536.676331	24.417626
133.177722	4550.598681	24.422643
133.755287	4543.271983	24.427661
133.636393	4538.965289	24.432679
133.765215	4550.691207	24.437696
134.059251	4550.412627	24.442714
133.841259	4543.526064	24.447731
133.986475	4552.367975	24.452749
134.106265	4566.325867	24.457767
134.384157	4564.735294	24.462784
134.312852	4572.004219	24.467802
134.211419	4581.012501	24.472819
134.315292	4584.406151	24.477837
134.852385	4593.542021	24.482855
134.836050	4596.432270	24.487872
135.231550	4603.423277	24.492890
135.730858	4613.813918	24.497907
136.450952	4604.687134	24.502925
136.492948	4594.288835	24.507943
136.442996	4571.112705	24.512960
136.240299	4573.183683	24.517978
136.278665	4572.102799	24.522995
136.505925	4572.778232	24.528013
136.639936	4574.419139	24.533031
136.336393	4573.693983	24.538048
136.792010	4585.696270	24.543066
136.387036	4599.288899	24.548083
136.957613	4604.475652	24.553101
137.094198	4611.126738	24.558119
137.087244	4602.349238	24.563136
137.571610	4611.204441	24.568154
137.449332	4618.702298	24.573171
137.611228	4618.823531	24.578189
137.737684	4620.457817	24.583207
137.891035	4629.070459	24.588224
137.894631	4618.945043	24.593242
138.110264	4623.238019	24.598259
138.048744	4639.543823	24.603277
138.313472	4655.363421	24.608295
138.148459	4657.289590	24.613312
138.595860	4644.837900	24.618330
138.566455	4675.485581	24.623347
139.022701	4673.181618	24.628365
138.967799	4688.367001	24.633383
138.784076	4688.413048	24.638400
139.247831	4698.278084	24.643418
139.198550	4718.630691	24.648435
139.712067	4718.329624	24.653453
139.416380	4731.466085	24.658471
139.714248	4733.987883	24.663488
139.903257	4748.396349	24.668506
139.963189	4751.870924	24.673523
139.910215	4739.635313	24.678541
139.940086	4771.791228	24.683559
140.322002	4785.700099	24.688576
140.572881	4772.553553	24.693594
140.518272	4793.658775	24.698611
140.690938	4800.376428	24.703629
140.524686	4804.493951	24.708647
140.976533	4826.363639	24.713664
141.270909	4830.044003	24.718682
141.386727	4838.892116	24.723699
141.627197	4844.700080	24.728717
141.546941	4856.934045	24.733735
141.658897	4866.861254	24.738752
141.753292	4850.256724	24.743770
141.982744	4867.350588	24.748787
142.586397	4883.228205	24.753805
142.615438	4881.323964	24.758823
142.190312	4881.198462	24.763840
142.968752	4882.670712	24.768858
142.962311	4880.434114	24.773875
142.960552	4890.511241	24.778893
143.071998	4906.622587	24.783911
143.179266	4901.060988	24.788928
143.221116	4905.841067	24.793946
143.273689	4923.967067	24.798963
143.656529	4929.807056	24.803981
144.011785	4938.621569	24.808999
144.105366	4934.707257	24.814016
144.611635	4930.457409	24.819034
144.401031	4947.356329	24.824051
144.944045	4954.892466	24.829069
145.247012	4957.021295	24.834087
145.119886	4957.219029	24.839104
145.570444	4967.696712	24.844122
145.169380	4972.787025	24.849139
145.137001	4959.253620	24.854157
145.399845	4959.172332	24.859175
145.272740	4966.656191	24.864192
145.677106	4983.164141	24.869210
145.665909	4989.722473	24.874227
145.871460	4994.353471	24.879245
145.833680	4999.503857	24.884263
145.999029	5013.180185	24.889280
146.368272	5014.811408	24.894298
146.200405	5026.459135	24.899315
146.390707	5031.284809	24.904333
146.578883	5044.104551	24.909351
146.748232	5057.766083	24.914368
147.067298	5052.054857	24.919386
147.017800	5081.962091	24.924403
147.094101	5074.002939	24.929421
147.232632	5081.536672	24.934439
147.270235	5104.845022	24.939456
147.632774	5100.727551	24.944474
147.733314	5121.594172	24.949491
148.175322	5135.174495	24.954509
148.012444	5145.624508	24.959527
147.904408	5147.759850	24.964544
148.550736	5156.927617	24.969562
149.068736	5168.652695	24.974579
149.127697	5157.375139	24.979597
149.007719	5172.512289	24.984615
149.211243	5178.946630	24.989632
149.724132	5188.556194	24.994650
150.055570	5193.701944	24.999667
149.646883	5187.414383	25.004685
150.121220	5189.885048	25.009703
149.763498	5193.568510	25.014720
150.168050	5199.310121	25.019738
150.077081	5213.770003	25.024755
150.357127	5207.365878	25.029773
150.172184	5213.059605	25.034791
150.471828	5234.876266	25.039808
150.929503	5240.640221	25.044826
150.948808	5247.442468	25.049843
151.250341	5247.307538	25.054861
151.870176	5264.495620	25.059879
151.595216	5279.927016	25.064896
151.911204	5278.575383	25.069914
151.806116	5274.012632	25.074931
152.101645	5264.201597	25.079949
152.237448	5261.874110	25.084967
152.310193	5273.627163	25.089984
152.904564	5268.623213	25.095002
152.937862	5263.771427	25.100019
152.828273	5271.119845	25.105037
153.173993	5265.773078	25.110055
153.048447	5274.386483	25.115072
153.173218	5284.957978	25.120090
153.295519	5282.724069	25.125107
153.217214	5281.811644	25.130125
153.625185	5283.341606	25.135143
153.540245	5295.982640	25.140160
153.524299	5296.689629	25.145178
153.624196	5312.489878	25.150195
153.855557	5312.716584	25.155213
154.206335	5325.804214	25.160231
154.221719	5348.095217	25.165248
154.607148	5349.415892	25.170266
154.225138	5369.516804	25.175283
154.862132	5388.408694	25.180301
154.837021	5379.136453	25.185319
155.450816	5399.769410	25.190336
155.592717	5399.663217	25.195354
155.587093	5398.413539	25.200371
155.630204	5390.469555	25.205389
155.702964	5397.744983	25.210407
155.473887	5426.384355	25.215424
156.242015	5426.711766	25.220442
156.295301	5429.763522	25.225459
156.265218	5450.617909	25.230477
156.647706	5466.902398	25.235495
156.431182	5474.609962	25.240512
156.189113	5481.882717	25.245530
156.723712	5503.501462	25.250547
156.822849	5511.546309	25.255565
157.234674	5527.616931	25.260583
157.397938	5524.420976	25.265600
157.753777	5537.172076	25.270618
157.735618	5541.550399	25.275635
157.808725	5560.394704	25.280653
158.270860	5557.524214	25.285671
158.522254	5566.866548	25.290688
158.477852	5577.275223	25.295706
158.686229	5581.785047	25.300723
158.835053	5579.149416	25.305741
159.308076	5595.745502	25.310759
159.412251	5607.297522	25.315776
159.732772	5604.829608	25.320794
159.863961	5606.003311	25.325811
159.746708	5599.496933	25.330829
159.838109	5593.171073	25.335847
160.223000	5612.511637	25.340864
160.296899	5625.703937	25.345882
160.313162	5628.207441	25.350899
160.678315	5624.628454	25.355917
160.860412	5619.953180	25.360935
161.131575	5648.040159	25.365952
161.054146	5660.115600	25.370970
160.820008	5665.544352	25.375987
160.957490	5667.684873	25.381005
161.450533	5675.596599	25.386023
161.347539	5690.129389	25.391040
161.715330	5701.332366	25.396058
162.029181	5696.247450	25.401075
162.235783	5705.045222	25.406093
162.642356	5704.591316	25.411111
162.742108	5708.527308	25.416128
162.803872	5718.467683	25.421146
162.643225	5704.831581	25.426163
162.629619	5715.675479	25.431181
162.656594	5718.496959	25.436199
162.874546	5732.058122	25.441216
162.695695	5737.411613	25.446234
163.129464	5747.624053	25.451251
163.509188	5768.122919	25.456269
163.750927	5757.737308	25.461287
163.867074	5793.163435	25.466304
164.079273	5792.529013	25.471322
164.580701	5801.117472	25.476339
163.815134	5796.721186	25.481357
164.226273	5812.904437	25.486375
164.229015	5832.076097	25.491392
164.715764	5832.354723	25.496410
165.222425	5848.292272	25.501427
165.325266	5861.871780	25.506445
165.743555	5849.405443	25.511463
165.905565	5871.991517	25.516480
165.869074	5862.136135	25.521498
166.504392	5871.864106	25.526515
166.499058	5864.127522	25.531533
166.986270	5857.350665	25.536551
166.482999	5869.553722	25.541568
166.967535	5865.558832	25.546586
166.853905	5867.239219	25.551603
166.956379	5879.468203	25.556621
167.091717	5891.231065	25.561639
167.235930	5894.319470	25.566656
167.112677	5899.761089	25.571674
167.796037	5915.949871	25.576691
167.851446	5928.837952	25.581709
168.781770	5920.280499	25.586727
168.634922	5915.642557	25.591744
168.882189	5913.122515	25.596762
168.790906	5912.450030	25.601779
168.659045	5930.932128	25.606797
169.015414	5933.052270	25.611815
168.835256	5939.739720	25.616832
168.904678	5937.443578	25.621850
169.737476	5965.910452	25.626867
169.682033	5972.037852	25.631885
169.962176	5978.585475	25.636903
169.926088	5970.662551	25.641920
169.704642	5987.394669	25.646938
170.353862	5984.673536	25.651955
170.300073	6010.254995	25.656973
170.734749	6006.713262	25.661991
170.736773	6023.791235	25.667008
170.681858	6028.801066	25.672026
171.288351	6029.400912	25.677044
171.168943	6037.604599	25.682061
171.192934	6043.996114	25.687079
171.494864	6058.909264	25.692096
171.094197	6067.758751	25.697114
171.589339	6080.174234	25.702132
171.767794	6097.903565	25.707149
172.025823	6107.729460	25.712167
172.234921	6124.541006	25.717184
172.325651	6130.062328	25.722202
172.693791	6148.732193	25.727220
172.766284	6152.606648	25.732237
173.330434	6157.224421	25.737255
173.511468	6163.410478	25.742272
173.483691	6176.312507	25.747290
173.892788	6180.668454	25.752308
174.033818	6190.181392	25.757325
174.214664	6176.921601	25.762343
174.294154	6175.606609	25.767360
174.221657	6199.614817	25.772378
174.182663	6207.232765	25.777396
174.677243	6208.103911	25.782413
174.681447	6201.829621	25.787431
174.726244	6223.162904	25.792448
175.128880	6231.583640	25.797466
175.246073	6225.656878	25.802484
175.349893	6247.311996	25.807501
175.813201	6259.924255	25.812519
175.925158	6265.113713	25.817536
175.777831	6276.150201	25.822554
175.867071	6269.292441	25.827572
176.031519	6285.337382	25.832589
176.285068	6290.185286	25.837607
176.510277	6310.283150	25.842624
176.559927	6322.355034	25.847642
177.165979	6320.793157	25.852660
177.230668	6350.816249	25.857677
177.406439	6353.526234	25.862695
177.826763	6345.661594	25.867712
177.431909	6351.726302	25.872730
177.785417	6366.166571	25.877748
177.998671	6385.286797	25.882765
178.123302	6388.780186	25.887783
178.830635	6401.816106	25.892800
178.777278	6401.914644	25.897818
179.210773	6404.335553	25.902836
179.143949	6416.244043	25.907853
179.424616	6426.160904	25.912871
179.618944	6423.036028	25.917888
179.940273	6429.270678	25.922906
179.882945	6415.015198	25.927924
179.972814	6429.806230	25.932941
180.215663	6458.195063	25.937959
180.140582	6453.970382	25.942976
180.345920	6467.584670	25.947994
180.893830	6479.342810	25.953012
180.915086	6481.923987	25.958029
180.949332	6497.286585	25.963047
180.808202	6503.381097	25.968064
180.748109	6520.686449	25.973082
181.004682	6529.240162	25.978100
181.222995	6541.655286	25.983117
181.495747	6558.796216	25.988135
182.287881	6575.134672	25.993152
182.284223	6582.364210	25.998170
182.538767	6600.995892	26.003188
182.734743	6620.843026	26.008205
182.826614	6619.234554	26.013223
183.238577	6622.786054	26.018240
183.112209	6624.653702	26.023258
183.654222	6623.400863	26.028276
183.605722	6633.643163	26.033293
183.939506	6637.569074	26.038311
184.033395	6653.274009	26.043328
184.347527	6650.692400	26.048346
184.842471	6645.011004	26.053364
184.816595	6654.711675	26.058381
185.215441	6664.457950	26.063399
185.725461	6670.631592	26.068416
185.584381	6672.507978	26.073434
185.740259	6671.633959	26.078452
185.839548	6667.382772	26.083469
185.901715	6672.271079	26.088487
186.412587	6657.741148	26.093504
186.093778	6668.865311	26.098522
186.268809	6679.077008	26.103540
186.150276	6692.941893	26.108557
186.373666	6697.358597	26.113575
186.502307	6705.606704	26.118592
186.446977	6732.244928	26.123610
186.253437	6735.306611	26.128628
186.998121	6762.464020	26.133645
186.783813	6760.072089	26.138663
187.625634	6776.281261	26.143680
187.671582	6808.291418	26.148698
187.840779	6796.471921	26.153716
187.817663	6805.172805	26.158733
188.179310	6822.277283	26.163751
188.417644	6824.743105	26.168768
188.318961	6843.859512	26.173786
188.597051	6854.841079	26.178804
188.663219	6869.583672	26.183821
189.000925	6888.272048	26.188839
189.233023	6893.504870	26.193856
189.370642	6923.484713	26.198874
189.731095	6924.579684	26.203892
190.040549	6937.696756	26.208909
190.223543	6952.399647	26.213927
190.247858	6953.212288	26.218944
190.127082	6965.060011	26.223962
190.576956	6980.586744	26.228980
190.969010	6992.052840	26.233997
191.151035	7004.088412	26.239015
191.475014	7013.026616	26.244032
191.585175	7034.005238	26.249050
192.237255	7030.266695	26.254068
192.704340	7029.272719	26.259085
192.652105	7028.301540	26.264103
193.020470	7025.694372	26.269120
193.107597	7028.417546	26.274138
193.669233	7017.854604	26.279156
193.549143	7012.744881	26.284173
193.483409	7024.904888	26.289191
193.727387	7043.659340	26.294208
193.622387	7051.016886	26.299226
194.017360	7037.381547	26.304244
194.450717	7042.618970	26.309261
194.569703	7060.096159	26.314279
194.866636	7050.819734	26.319296
195.104275	7059.446960	26.324314
195.239907	7063.798721	26.329332
195.405505	7062.853768	26.334349
195.444404	7077.219872	26.339367
195.592777	7067.360756	26.344384
195.303984	7086.137128	26.349402
195.538504	7100.445729	26.354420
195.603207	7100.860275	26.359437
195.375733	7124.128390	26.364455
196.267883	7133.859610	26.369472
195.945566	7162.048535	26.374490
196.519115	7172.282130	26.379508
196.827053	7187.715957	26.384525
196.642387	7205.325387	26.389543
197.035673	7208.899797	26.394560
197.275945	7226.274435	26.399578
197.232448	7231.796270	26.404596
197.772840	7241.664434	26.409613
197.839827	7256.764033	26.414631
198.274955	7269.519591	26.419648
198.497538	7281.550250	26.424666
198.577224	7270.406766	26.429684
199.049171	7302.181359	26.434701
199.297204	7312.576729	26.439719
199.506439	7308.546634	26.444736
199.333549	7305.443666	26.449754
199.466512	7327.215168	26.454772
199.764276	7331.652842	26.459789
200.131573	7336.737459	26.464807
200.439444	7350.691564	26.469824
200.562177	7355.814232	26.474842
200.677589	7366.300071	26.479860
201.091914	7370.479855	26.484877
200.849319	7372.400661	26.489895
201.326336	7383.452906	26.494912
201.285905	7390.693616	26.499930
201.379333	7403.295450	26.504948
201.442172	7410.039459	26.509965
201.564602	7423.579274	26.514983
201.765955	7437.226564	26.520000
201.914602	7462.611536	26.525018
202.244267	7479.520388	26.530036
202.551676	7479.220656	26.535053
202.641268	7509.093770	26.540071
203.001646	7533.902791	26.545088
203.358693	7537.020153	26.550106
203.473230	7543.423307	26.555124
203.685628	7549.889056	26.560141
203.652884	7576.676979	26.565159
204.165337	7581.161164	26.570176
203.969940	7593.691154	26.575194
204.589529	7607.743630	26.580212
205.014046	7610.182754	26.585229
204.835327	7625.452469	26.590247
205.563195	7623.152047	26.595264
205.510393	7635.129236	26.600282
205.626569	7639.688363	26.605300
205.899624	7645.929111	26.610317
206.290020	7659.964369	26.615335
206.722429	7660.321328	26.620352
206.550073	7683.774911	26.625370
206.278350	7696.393203	26.630388
206.696194	7704.494812	26.635405
206.885760	7715.956300	26.640423
207.341922	7729.030102	26.645440
207.579341	7754.890774	26.650458
207.680590	7764.879081	26.655476
207.933301	7779.984725	26.660493
208.072417	7790.216467	26.665511
208.287539	7802.114072	26.670528
208.310035	7806.641468	26.675546
208.529785	7823.304996	26.680564
209.016263	7842.021119	26.685581
209.064565	7854.244047	26.690599
209.747975	7875.403167	26.695616
209.729504	7886.293468	26.700634
209.979925	7894.370854	26.705652
210.252514	7891.461171	26.710669
210.299364	7919.889746	26.715687
210.422490	7918.063321	26.720704
210.812891	7932.107484	26.725722
210.773067	7963.255162	26.730740
211.030491	7941.941149	26.735757
210.953902	7981.044444	26.740775
211.215126	7992.810132	26.745792
211.774357	7999.355021	26.750810
211.765639	8010.748666	26.755828
211.853414	8013.143463	26.760845
211.889061	8041.676498	26.765863
212.094385	8046.780231	26.770880
213.176617	8061.518315	26.775898
213.181042	8070.824971	26.780916
213.317733	8082.508908	26.785933
213.497186	8090.842286	26.790951
213.436720	8095.645753	26.795968
214.089720	8110.064922	26.800986
214.124146	8122.622731	26.806004
214.161487	8130.126601	26.811021
214.256061	8137.183094	26.816039
214.698745	8154.474114	26.821056
214.988309	8157.054556	26.826074
215.111762	8169.381093	26.831092
215.146258	8176.738167	26.836109
215.369786	8195.969950	26.841127
215.306834	8214.407889	26.846144
215.659401	8227.538604	26.851162
215.780846	8233.993669	26.856180
216.149953	8253.581111	26.861197
217.010675	8254.121729	26.866215
217.500092	8248.051586	26.871232
217.905828	8264.035834	26.876250
218.622490	8260.975527	26.881268
219.022751	8251.196932	26.886285
219.061335	8224.984913	26.891303
218.948950	8218.676312	26.896320
219.105005	8215.354987	26.901338
218.775363	8206.188500	26.906356
219.126447	8215.529332	26.911373
219.037858	8237.473380	26.916391
218.976991	8243.836486	26.921408
219.170691	8241.416297	26.926426
219.148927	8279.262860	26.931444
219.215735	8277.139306	26.936461
219.459892	8304.279682	26.941479
219.833378	8311.833645	26.946496
220.192695	8334.170896	26.951514
219.983300	8351.962904	26.956532
220.554496	8366.212303	26.961549
220.706872	8380.563992	26.966567
220.769599	8402.452548	26.971584
221.177976	8419.543164	26.976602
221.553046	8436.163560	26.981620
221.694909	8447.344392	26.986637
222.291605	8461.804692	26.991655
222.718025	8464.297987	26.996672
222.834719	8479.552008	27.001690
222.904632	8498.830806	27.006708
223.077456	8498.123236	27.011725
223.153982	8504.837094	27.016743
223.283572	8533.342891	27.021760
223.740020	8534.911255	27.026778
223.531420	8565.182195	27.031796
223.746916	8569.540870	27.036813
223.828498	8597.564791	27.041831
224.344924	8606.633576	27.046848
224.508945	8632.001343	27.051866
224.757451	8650.017341	27.056884
225.235704	8653.257469	27.061901
225.289832	8668.121877	27.066919
225.634343	8685.532883	27.071936
226.244067	8699.696664	27.076954
226.266774	8719.189895	27.081972
226.736616	8710.347872	27.086989
226.702452	8728.776926	27.092007
226.937222	8743.734435	27.097024
227.067333	8749.808624	27.102042
227.197660	8766.377646	27.107060
227.453983	8776.059773	27.112077
227.495656	8780.507875	27.117095
227.946980	8803.548152	27.122112
228.276248	8803.631534	27.127130
228.600053	8818.041152	27.132148
228.824357	8831.032087	27.137165
228.956377	8839.945545	27.142183
228.744780	8837.817503	27.147200
229.508540	8857.387751	27.152218
229.050391	8869.385581	27.157236
229.860648	8879.952177	27.162253
229.875016	8907.625421	27.167271
229.790533	8910.287479	27.172288
230.347377	8913.224025	27.177306
230.483598	8938.696910	27.182324
230.966381	8948.469331	27.187341
230.907578	8959.022817	27.192359
231.550740	8963.940296	27.197376
231.676772	8972.697282	27.202394
231.537280	8985.479852	27.207412
231.920487	9004.772091	27.212429
231.786821	9017.003924	27.217447
232.322066	9035.803988	27.222464
233.097022	9043.211630	27.227482
233.025642	9059.765447	27.232500
233.123652	9076.597704	27.237517
233.503704	9091.125094	27.242535
233.619890	9097.609737	27.247552
234.095860	9108.487714	27.252570
234.160680	9118.299363	27.257588
234.465674	9134.804466	27.262605
234.558982	9142.843858	27.267623
234.981913	9159.903725	27.272640
234.979621	9158.377509	27.277658
235.528937	9198.218487	27.282676
235.717435	9197.661110	27.287693
235.949676	9206.599963	27.292711
236.001239	9229.815607	27.297728
236.208486	9234.281379	27.302746
236.444577	9261.904428	27.307764
236.873605	9270.053833	27.312781
237.065903	9282.525036	27.317799
237.503992	9287.455232	27.322816
237.607826	9289.416701	27.327834
237.838543	9322.639663	27.332852
237.873929	9329.611941	27.337869
238.210118	9338.343073	27.342887
238.376376	9360.343450	27.347904
238.929843	9361.755661	27.352922
238.857688	9385.848986	27.357940
239.269833	9385.201089	27.362957
239.561403	9398.819411	27.367975
239.584096	9420.884550	27.372992
239.971533	9434.753307	27.378010
240.277621	9462.354111	27.383028
239.988771	9462.633359	27.388045
240.409261	9479.912954	27.393063
240.435975	9503.846760	27.398080
240.574892	9505.508647	27.403098
240.951778	9516.900317	27.408116
242.149120	9526.272254	27.413133
242.537950	9526.259155	27.418151
242.364884	9552.009403	27.423168
242.890714	9556.790490	27.428186
243.178215	9563.847251	27.433204
243.088928	9559.767448	27.438221
243.637152	9569.785447	27.443239
243.306622	9585.766639	27.448256
243.683568	9588.161949	27.453274
243.852430	9610.364682	27.458292
244.114932	9629.193182	27.463309
244.354911	9631.841139	27.468327
244.056606	9653.121511	27.473344
244.784510	9655.490356	27.478362
244.834403	9667.867233	27.483380
244.849576	9688.275853	27.488397
245.254706	9696.369561	27.493415
245.024597	9721.621432	27.498432
245.174016	9736.033913	27.503450
245.895328	9753.173518	27.508468
246.408745	9772.322293	27.513485
246.689971	9781.891428	27.518503
246.805790	9795.316203	27.523520
246.968967	9812.764707	27.528538
247.454158	9819.601444	27.533556
247.851521	9828.011590	27.538573
248.346005	9830.961766	27.543591
248.301275	9841.197635	27.548608
248.915240	9852.250256	27.553626
249.116978	9861.904254	27.558644
249.149543	9870.291194	27.563661
249.171166	9882.836754	27.568679
249.277612	9896.137127	27.573696
249.603267	9897.621687	27.578714
249.815853	9929.686231	27.583732
250.007015	9939.126975	27.588749
250.263074	9948.946139	27.593767
250.590897	9963.706671	27.598784
250.829009	9981.614039	27.603802
250.915802	9995.718860	27.608820
251.363797	10021.676834	27.613837
251.726095	10030.056645	27.618855
251.594590	10048.225237	27.623872
252.248021	10049.808479	27.628890
252.520221	10072.750216	27.633908
252.896061	10076.536918	27.638925
253.289389	10092.672367	27.643943
252.903044	10112.952508	27.648960
253.448120	10115.372113	27.653978
253.416889	10134.129215	27.658996
253.957058	10149.718982	27.664013
254.334638	10170.296787	27.669031
254.672449	10190.313230	27.674048
255.053263	10198.988623	27.679066
255.693965	10204.915206	27.684084
255.837427	10210.218916	27.689101
255.878673	10213.414198	27.694119
255.875617	10233.423992	27.699136
256.070750	10235.267301	27.704154
256.315033	10253.709618	27.709172
256.648821	10267.411512	27.714189
256.885348	10281.366596	27.719207
256.902780	10305.042395	27.724224
257.119840	10304.870195	27.729242
257.541781	10321.930686	27.734260
257.770301	10344.199419	27.739277
258.288726	10355.182312	27.744295
258.543676	10370.523225	27.749312
258.697442	10385.375137	27.754330
259.077693	10400.967151	27.759348
258.971575	10423.650494	27.764365
259.261160	10433.006735	27.769383
259.186605	10452.127430	27.774400
259.552635	10455.833919	27.779418
259.751938	10481.298058	27.784436
259.948402	10507.243235	27.789453
260.327083	10523.309855	27.794471
260.502467	10541.709533	27.799488
260.971247	10557.870800	27.804506
261.090165	10586.995694	27.809524
260.956320	10593.096865	27.814541
261.809161	10614.854772	27.819559
261.771928	10648.754969	27.824576
262.284424	10659.824130	27.829594
262.660455	10673.544602	27.834612
262.700273	10695.784343	27.839629
262.973184	10715.766476	27.844647
262.922762	10724.432263	27.849664
263.469060	10749.889131	27.854682
263.614352	10753.067330	27.859700
264.383754	10776.762177	27.864717
264.776698	10782.378567	27.869735
264.754777	10801.995154	27.874752
264.902490	10816.473488	27.879770
265.170191	10825.249052	27.884788
265.287678	10862.279938	27.889805
265.571612	10857.288138	27.894823
266.105479	10879.940444	27.899840
266.349471	10893.116512	27.904858
266.957482	10916.798054	27.909876
266.962459	10927.184746	27.914893
267.290375	10939.946011	27.919911
267.692116	10958.356037	27.924928
268.061589	10972.480403	27.929946
268.100149	10976.884728	27.934964
268.295913	10985.755769	27.939981
268.463205	11002.101218	27.944999
268.534465	11025.425717	27.950016
268.592831	11047.906305	27.955034
269.121810	11075.750372	27.960052
269.370351	11101.785594	27.965069
269.722855	11110.099056	27.970087
269.997075	11140.536165	27.975104
269.754830	11148.459480	27.980122
270.519782	11170.981061	27.985140
270.367727	11197.335500	27.990157
271.031274	11212.368653	27.995175
271.243656	11236.192446	28.000192
271.670524	11251.895758	28.005210
272.180153	11263.854439	28.010228
272.190528	11279.755784	28.015245
273.107345	11313.903115	28.020263
273.323566	11314.080038	28.025280
273.017101	11325.992401	28.030298
273.364087	11342.042234	28.035316
273.300230	11370.422770	28.040333
273.826029	11386.231190	28.045351
274.097156	11416.908035	28.050368
274.732464	11433.351493	28.055386
274.809201	11454.433637	28.060404
274.770350	11479.317920	28.065421
275.523573	11481.113291	28.070439
275.463895	11489.786534	28.075456
275.979279	11508.647159	28.080474
276.833208	11521.236903	28.085492
276.702214	11519.495384	28.090509
277.216226	11525.793180	28.095527
277.363358	11541.806905	28.100544
277.499284	11551.235669	28.105562
278.320907	11557.690638	28.110580
278.317780	11585.770821	28.115597
278.462874	11581.945630	28.120615
278.702757	11599.785191	28.125632
278.851730	11601.547264	28.130650
278.686228	11623.108458	28.135668
279.031937	11659.581949	28.140685
279.786163	11675.174084	28.145703
280.376267	11680.206753	28.150720
280.463436	11686.443567	28.155738
280.972826	11688.615641	28.160756
280.868002	11714.095743	28.165773
281.409232	11713.249969	28.170791
281.408201	11705.034781	28.175808
281.293229	11732.196202	28.180826
281.449071	11749.032747	28.185844
281.692774	11760.453540	28.190861
282.132421	11777.220381	28.195879
282.439154	11808.429382	28.200896
282.353677	11813.193978	28.205914
283.010248	11829.318417	28.210932
283.129065	11854.483693	28.215949
283.399623	11858.021935	28.220967
283.399593	11879.500199	28.225984
283.657814	11904.916685	28.231002
284.349970	11918.724656	28.236020
284.655429	11952.827817	28.241037
285.335535	11968.021240	28.246055
285.661778	11988.787913	28.251072
285.651430	11997.236627	28.256090
286.083844	12010.009843	28.261108
286.246477	12031.852198	28.266125
286.652815	12042.415166	28.271143
287.067784	12053.280028	28.276160
287.073696	12094.738512	28.281178
287.738042	12100.067091	28.286196
287.633769	12125.662776	28.291213
287.786020	12127.884460	28.296231
288.264526	12142.490543	28.301248
287.978709	12169.892852	28.306266
288.865596	12186.466483	28.311284
289.034841	12218.677484	28.316301
289.657324	12220.246375	28.321319
289.911540	12241.873774	28.326336
289.888848	12262.337618	28.331354
290.803103	12262.620616	28.336372
291.139359	12288.935559	28.341389
291.099432	12307.167993	28.346407
291.809301	12299.283338	28.351424
291.653240	12326.266617	28.356442
292.469410	12333.449196	28.361460
292.555697	12342.625849	28.366477
292.850627	12353.212942	28.371495
292.996168	12373.571925	28.376512
292.905976	12394.708877	28.381530
293.036298	12406.914647	28.386548
292.952801	12441.793739	28.391565
293.461471	12467.092527	28.396583
293.740409	12492.994986	28.401600
294.114537	12502.069027	28.406618
294.587314	12514.235635	28.411636
294.688769	12553.619282	28.416653
294.904604	12576.719666	28.421671
295.546645	12600.286987	28.426688
295.793746	12616.784766	28.431706
296.248095	12639.043798	28.436724
296.226754	12660.007423	28.441741
296.708379	12676.296341	28.446759
297.056136	12688.070897	28.451776
297.192456	12724.001528	28.456794
297.678617	12741.701610	28.461812
297.999761	12757.493982	28.466829
298.254974	12790.690145	28.471847
298.357791	12792.979966	28.476864
298.458023	12821.482489	28.481882
299.026033	12843.850660	28.486900
298.643990	12860.956862	28.491917
298.953235	12892.232940	28.496935
299.465364	12919.008334	28.501952
299.571954	12949.664070	28.506970
300.293483	12968.441143	28.511988
300.594591	12983.386144	28.517005
300.737271	13008.728914	28.522023
301.516764	13025.050914	28.527040
301.811092	13053.137296	28.532058
302.348844	13057.350206	28.537076
302.574057	13060.524329	28.542093
303.178945	13073.224200	28.547111
303.848815	13088.757589	28.552128
303.877357	13095.933544	28.557146
304.148335	13106.214665	28.562164
304.396638	13125.371072	28.567181
304.526031	13122.436054	28.572199
305.107442	13139.184836	28.577216
305.278565	13165.394549	28.582234
305.066612	13160.787303	28.587252
305.474120	13194.496471	28.592269
305.419260	13211.460746	28.597287
305.699639	13222.791427	28.602304
305.871496	13264.451617	28.607322
305.968033	13285.183849	28.612340
306.400659	13319.060886	28.617357
306.453788	13354.598533	28.622375
306.897217	13381.346649	28.627392
307.173765	13407.403819	28.632410
307.565080	13420.426042	28.637428
307.950816	13461.332845	28.642445
308.605471	13488.482737	28.647463
309.375252	13511.615855	28.652480
309.457491	13539.998126	28.657498
310.116924	13544.629138	28.662516
310.385904	13561.458337	28.667533
310.829145	13569.396440	28.672551
310.774578	13591.647888	28.677568
311.036831	13611.026330	28.682586
311.230593	13628.427438	28.687604
311.562543	13658.785701	28.692621
311.951858	13680.588897	28.697639
311.863421	13701.601197	28.702656
312.194940	13732.296894	28.707674
312.771926	13753.245030	28.712692
313.102938	13778.023686	28.717709
313.252566	13819.933228	28.722727
313.632680	13828.925086	28.727744
313.656397	13861.889071	28.732762
314.220985	13878.059916	28.737780
314.584462	13906.848632	28.742797
314.616551	13927.127458	28.747815
315.347100	13947.632880	28.752832
315.477449	13973.842756	28.757850
315.717189	13990.711901	28.762868
316.245071	14019.505173	28.767885
316.788108	14041.584446	28.772903
317.343108	14053.185511	28.777920
317.995755	14083.756333	28.782938
317.917389	14097.149803	28.787956
318.392415	14109.202208	28.792973
318.278922	14128.993183	28.797991
318.759292	14144.736969	28.803008
318.802218	14164.524209	28.808026
319.422920	14189.991565	28.813044
319.627921	14200.890990	28.818061
319.574495	14231.285624	28.823079
319.914566	14261.155153	28.828096
320.461138	14280.764778	28.833114
320.616429	14298.179263	28.838132
321.076337	14321.044829	28.843149
321.246594	14353.372584	28.848167
321.957418	14359.213500	28.853184
321.925462	14377.464278	28.858202
322.387737	14405.350335	28.863220
322.482959	14414.392736	28.868237
323.015860	14436.571927	28.873255
323.148904	14450.108837	28.878272
323.859601	14470.488979	28.883290
324.257360	14487.825789	28.888308
324.358596	14503.686138	28.893325
324.608075	14534.489883	28.898343
324.957246	14544.216892	28.903360
325.201846	14569.353002	28.908378
325.749953	14592.398216	28.913396
326.083070	14603.517860	28.918413
326.217768	14624.108392	28.923431
326.843170	14643.453288	28.928448
327.325729	14658.785900	28.933466
327.739836	14672.073271	28.938484
328.042316	14685.019786	28.943501
328.046501	14702.029442	28.948519
328.608154	14709.343394	28.953536
328.726451	14725.161743	28.958554
329.718176	14728.817871	28.963572
330.441511	14724.039907	28.968589
330.838809	14732.862384	28.973607
331.192767	14751.922887	28.978624
331.328381	14764.443167	28.983642
331.255824	14774.123366	28.988660
331.769854	14775.242393	28.993677
331.516315	14805.239354	28.998695
331.521440	14812.222945	29.003712
332.008276	14838.299679	29.008730
332.476374	14853.586011	29.013748
332.753521	14883.265360	29.018765
332.720387	14902.024371	29.023783
332.840024	14917.410879	29.028800
333.320418	14959.626451	29.033818
333.572362	14978.434587	29.038836
334.093022	15003.924476	29.043853
333.969977	15042.315853	29.048871
334.649084	15068.261907	29.053888
334.884755	15107.588601	29.058906
334.927099	15141.647385	29.063924
335.801757	15152.933248	29.068941
336.320333	15179.681371	29.073959
337.061917	15188.715133	29.078976
337.086937	15211.431586	29.083994
337.572894	15229.946047	29.089012
337.760728	15243.316969	29.094029
338.201801	15276.318882	29.099047
338.719684	15287.881262	29.104064
338.890419	15317.924120	29.109082
338.892383	15341.804479	29.114100
339.150259	15367.568442	29.119117
339.423121	15382.733079	29.124135
339.975416	15417.029693	29.129152
340.236997	15431.129298	29.134170
340.703039	15463.903676	29.139188
340.847283	15482.794800	29.144205
341.147119	15514.439960	29.149223
341.546400	15537.821571	29.154240
341.824781	15570.434892	29.159258
342.262109	15585.235285	29.164276
343.344079	15589.595363	29.169293
343.688140	15612.223420	29.174311
344.052768	15625.355841	29.179328
343.737128	15651.290643	29.184346
344.244547	15669.496314	29.189364
344.507792	15669.616672	29.194381
344.215879	15694.644571	29.199399
344.445129	15711.863955	29.204416
344.984605	15737.574102	29.209434
345.039231	15763.544051	29.214452
345.705219	15807.211036	29.219469
346.494283	15820.832985	29.224487
347.339045	15840.872769	29.229504
347.331219	15856.011718	29.234522
347.817863	15874.807331	29.239540
348.301790	15890.712978	29.244557
348.643234	15905.535806	29.249575
348.731679	15920.091540	29.254592
349.040773	15947.609959	29.259610
349.165247	15968.112465	29.264628
350.150893	15984.354547	29.269645
350.001274	16010.424822	29.274663
350.144069	16023.559537	29.279680
350.624262	16048.638519	29.284698
350.812649	16083.499408	29.289716
351.332752	16098.450501	29.294733
351.516634	16119.747168	29.299751
351.908555	16139.026821	29.304768
352.729905	16170.049663	29.309786
352.855024	16200.093795	29.314804
353.337316	16220.093058	29.319821
353.460969	16234.835534	29.324839
354.037084	16258.924986	29.329856
354.122299	16286.027052	29.334874
354.439966	16314.591180	29.339892
354.638490	16339.516978	29.344909
354.703795	16367.791913	29.349927
355.279434	16398.345131	29.354944
355.988618	16420.598774	29.359962
355.800197	16460.845134	29.364980
356.507530	16483.676014	29.369997
357.049003	16517.256454	29.375015
357.140315	16543.407556	29.380032
357.510671	16578.177969	29.385050
357.750017	16606.894241	29.390068
358.547459	16623.844198	29.395085
358.532391	16663.020614	29.400103
358.816977	16692.016412	29.405120
359.320664	16716.268232	29.410138
359.387935	16746.348137	29.415156
359.834600	16778.617689	29.420173
360.115366	16805.440857	29.425191
360.611537	16843.954814	29.430208
361.573629	16874.643670	29.435226
361.375546	16900.207969	29.440244
362.155774	16929.248398	29.445261
362.049121	16966.355447	29.450279
362.463600	16987.181709	29.455296
363.253609	17004.598250	29.460314
363.571067	17038.287689	29.465332
364.143983	17059.633213	29.470349
364.263238	17088.062817	29.475367
364.453992	17112.991071	29.480384
364.758663	17149.808348	29.485402
364.839271	17183.264537	29.490420
365.764476	17202.651211	29.495437
365.820391	17235.922447	29.500455
366.387806	17270.077015	29.505472
366.686433	17289.609857	29.510490
366.996652	17329.498561	29.515508
367.247062	17345.935963	29.520525
367.417288	17370.428247	29.525543
367.881286	17392.085365	29.530560
368.195733	17424.934417	29.535578
368.559918	17454.438547	29.540596
369.471489	17486.229186	29.545613
369.319726	17526.038640	29.550631
369.535747	17540.735505	29.555648
370.141295	17575.125564	29.560666
370.147769	17607.792579	29.565684
370.880205	17632.198683	29.570701
370.850718	17671.873226	29.575719
371.181550	17715.594351	29.580736
371.582033	17743.326079	29.585754
371.439269	17784.792837	29.590772
372.206060	17810.050988	29.595789
372.577364	17865.109826	29.600807
372.812129	17902.395858	29.605824
373.737886	17930.895440	29.610842
373.806689	17970.456737	29.615860
374.358876	18000.643243	29.620877
374.975608	18035.962391	29.625895
375.362478	18066.489997	29.630912
376.084734	18098.071929	29.635930
376.483276	18119.523295	29.640948
376.960546	18140.231884	29.645965
377.213649	18177.149818	29.650983
377.696932	18200.860240	29.656000
377.930335	18224.927225	29.661018
378.086167	18259.457628	29.666036
378.742723	18293.093613	29.671053
379.049706	18319.442037	29.676071
379.298204	18346.134332	29.681088
380.251453	18369.045432	29.686106
380.406491	18404.463706	29.691124
381.000279	18428.376879	29.696141
381.335207	18452.542492	29.701159
381.406799	18478.324765	29.706176
381.924482	18497.733004	29.711194
382.028586	18529.384774	29.716212
382.512942	18558.503753	29.721229
382.862831	18586.774886	29.726247
383.453044	18608.469500	29.731264
383.913067	18633.353992	29.736282
384.064106	18679.935233	29.741300
384.505831	18695.899437	29.746317
384.818285	18723.217023	29.751335
385.508184	18752.902961	29.756352
385.684452	18788.350074	29.761370
385.843343	18813.158477	29.766388
386.116948	18832.103010	29.771405
386.476046	18864.916021	29.776423
387.077468	18894.824903	29.781440
387.283539	18928.457782	29.786458
387.513096	18974.628071	29.791476
388.021239	19005.335993	29.796493
388.298165	19034.549976	29.801511
388.540446	19076.102955	29.806528
389.064662	19116.244357	29.811546
389.518630	19150.646973	29.816564
390.108912	19184.065573	29.821581
390.429247	19214.757617	29.826599
390.797631	19241.485146	29.831616
391.524780	19271.816893	29.836634
391.869167	19301.764240	29.841652
392.635518	19312.861231	29.846669
393.580331	19329.873189	29.851687
393.780883	19344.156478	29.856704
394.499482	19361.011946	29.861722
394.513363	19378.956458	29.866740
394.834069	19389.977364	29.871757
395.439521	19406.498463	29.876775
395.508072	19425.745530	29.881792
395.692759	19436.025974	29.886810
395.863722	19467.417846	29.891828
396.371530	19487.520905	29.896845
396.735882	19514.642057	29.901863
396.770197	19536.681938	29.906880
397.475871	19564.218124	29.911898
397.418309	19593.526178	29.916916
397.808702	19618.800408	29.921933
398.152143	19647.971379	29.926951
398.307629	19680.190659	29.931968
398.983086	19719.737884	29.936986
399.212782	19761.583137	29.942004
399.370079	19787.555063	29.947021
400.008807	19827.942529	29.952039
400.244280	19867.091441	29.957056
400.940507	19902.272174	29.962074
401.276771	19935.953371	29.967092
401.718960	19979.971049	29.972109
402.302029	20012.597994	29.977127
402.590822	20055.424215	29.982144
403.167723	20085.288848	29.987162
403.421792	20121.767970	29.992180
403.929675	20128.407496	29.997197
404.745067	20162.495545	30.002215
405.056573	20196.413094	30.007232
405.370183	20232.242589	30.012250
405.880976	20260.934550	30.017268
406.121177	20289.430063	30.022285
406.522743	20319.801744	30.027303
406.899950	20353.298882	30.032320
407.483231	20379.258114	30.037338
407.675191	20424.754454	30.042356
408.132728	20453.833895	30.047373
408.533440	20486.463516	30.052391
408.560705	20524.609473	30.057408
409.081378	20560.659280	30.062426
409.805275	20594.772787	30.067444
410.032629	20637.005282	30.072461
410.799962	20662.045417	30.077479
410.756440	20703.224016	30.082496
411.260140	20728.667239	30.087514
411.585483	20770.642681	30.092532
411.680557	20814.737243	30.097549
412.378944	20840.665567	30.102567
412.936079	20890.017298	30.107584
414.150362	20889.053627	30.112602
415.330927	20905.083939	30.117620
415.752955	20926.483031	30.122637
416.161200	20938.166826	30.127655
416.440412	20966.545118	30.132672
416.629121	20973.318110	30.137690
416.799878	21001.236694	30.142708
417.015390	21027.323900	30.147725
417.402810	21038.054259	30.152743
417.580752	21079.630744	30.157760
417.772406	21101.068114	30.162778
418.177172	21135.561785	30.167796
418.213450	21162.607384	30.172813
418.970274	21203.311322	30.177831
419.004080	21253.546723	30.182848
419.356353	21289.488761	30.187866
419.680542	21325.590017	30.192884
419.978352	21370.105019	30.197901
420.409072	21404.489327	30.202919
420.813651	21442.784729	30.207936
420.969993	21485.538745	30.212954
421.362942	21521.056772	30.217972
422.026920	21565.716760	30.222989
422.550067	21598.725621	30.228007
422.669226	21649.370627	30.233024
422.802142	21683.952900	30.238042
423.690837	21736.539523	30.243060
424.554258	21756.663832	30.248077
425.453189	21789.292524	30.253095
425.518446	21822.478365	30.258112
426.007579	21851.895562	30.263130
426.564831	21887.757725	30.268148
427.091264	21914.217479	30.273165
427.795481	21924.085706	30.278183
428.028869	21960.086657	30.283200
428.309372	21992.918805	30.288218
428.784741	22012.921484	30.293236
429.542397	22050.212408	30.298253
429.944165	22070.170555	30.303271
430.380356	22101.726943	30.308288
430.560634	22121.937735	30.313306
430.970549	22164.301582	30.318324
431.528274	22194.054906	30.323341
431.889757	22221.824191	30.328359
431.817859	22269.970559	30.333376
432.145792	22306.497420	30.338394
432.470915	22341.544359	30.343412
432.745562	22396.968378	30.348429
432.943093	22435.352274	30.353447
433.455965	22490.041945	30.358464
433.869760	22530.682789	30.363482
434.300052	22574.381307	30.368500
434.347082	22622.441240	30.373517
434.885595	22674.309771	30.378535
435.579183	22725.198956	30.383552
435.936934	22777.127619	30.388570
436.634692	22831.269129	30.393588
437.231320	22878.299300	30.398605
437.667998	22923.493946	30.403623
438.079944	22968.867813	30.408640
438.490026	23022.166620	30.413658
439.179626	23046.608251	30.418676
439.389197	23096.410170	30.423693
440.302120	23137.296407	30.428711
440.760606	23185.485487	30.433728
441.130226	23220.725570	30.438746
441.990730	23247.007677	30.443764
442.274413	23291.000311	30.448781
442.670988	23320.151553	30.453799
443.165136	23365.643776	30.458816
443.612292	23404.234611	30.463834
444.446452	23433.473018	30.468852
444.433909	23461.498489	30.473869
445.236903	23492.695734	30.478887
445.622469	23522.281172	30.483904
445.976829	23566.313304	30.488922
446.339438	23591.790481	30.493940
446.743641	23643.193802	30.498957
447.524803	23656.479801	30.503975
447.881654	23692.918163	30.508992
448.171594	23726.173121	30.514010
448.679312	23754.956712	30.519028
448.897006	23791.836118	30.524045
449.650309	23825.669094	30.529063
449.849644	23861.036399	30.534080
449.917663	23899.621612	30.539098
450.261095	23935.998065	30.544116
450.357575	23973.224282	30.549133
451.197296	24015.132308	30.554151
451.406561	24067.337016	30.559168
452.040984	24104.053656	30.564186
452.211724	24148.958069	30.569204
452.464451	24194.612235	30.574221
453.316622	24243.816261	30.579239
453.777348	24291.541381	30.584256
453.990106	24319.013855	30.589274
454.660944	24355.726602	30.594292
455.078266	24411.196723	30.599309
455.433340	24445.255978	30.604327
456.146988	24492.354878	30.609344
456.531526	24529.277707	30.614362
456.371842	24582.260826	30.619380
457.070941	24629.092868	30.624397
457.779813	24676.426442	30.629415
458.102595	24717.018189	30.634432
458.738420	24775.883080	30.639450
459.076518	24817.183702	30.644468
459.641455	24862.307144	30.649485
460.576968	24894.333442	30.654503
460.946632	24937.869887	30.659520
461.592813	24973.408535	30.664538
462.433090	25004.682831	30.669556
462.451336	25058.434367	30.674573
462.570305	25086.787710	30.679591
463.126664	25121.335446	30.684608
463.403314	25183.698715	30.689626
464.099092	25219.030994	30.694644
463.878578	25273.305179	30.699661
464.541375	25318.759010	30.704679
464.986645	25368.593311	30.709696
465.846503	25406.256374	30.714714
466.774940	25457.987013	30.719732
467.249539	25497.827002	30.724749
467.412953	25542.701606	30.729767
468.931903	25566.341266	30.734784
469.631478	25595.320211	30.739802
470.823877	25605.843250	30.744820
471.215286	25635.283172	30.749837
471.581705	25649.339414	30.754855
471.961416	25672.271695	30.759872
472.315295	25693.533551	30.764890
472.751494	25714.100592	30.769908
472.152907	25746.545902	30.774925
472.396226	25769.841465	30.779943
472.943614	25805.916990	30.784960
473.531325	25861.250145	30.789978
474.047365	25904.973040	30.794996
473.986167	25945.183276	30.800013
474.192117	25987.478399	30.805031
474.890939	26033.577900	30.810048
474.763027	26088.140576	30.815066
475.537284	26131.547002	30.820084
475.828666	26172.264095	30.825101
476.393292	26232.938818	30.830119
477.150125	26290.323914	30.835136
477.436594	26328.604138	30.840154
478.073480	26369.084850	30.845172
478.747282	26424.102818	30.850189
479.395835	26464.452513	30.855207
480.135339	26514.952792	30.860224
480.347933	26569.832933	30.865242
481.026595	26595.183551	30.870260
481.590335	26644.795411	30.875277
481.798630	26676.219744	30.880295
482.181181	26718.484346	30.885312
482.046147	26763.424061	30.890330
482.739191	26804.940533	30.895348
482.948825	26848.369496	30.900365
483.490220	26896.134308	30.905383
484.085068	26948.050724	30.910400
484.195719	26995.732409	30.915418
484.851783	27051.840346	30.920436
485.069764	27111.963530	30.925453
485.471759	27172.293092	30.930471
485.954624	27223.295201	30.935488
486.477347	27289.162904	30.940506
487.221535	27322.095924	30.945524
487.942272	27384.827552	30.950541
488.563894	27431.918216	30.955559
489.091686	27467.798606	30.960576
489.650996	27522.574050	30.965594
490.676845	27555.757493	30.970612
490.998014	27601.135026	30.975629
491.704981	27654.142198	30.980647
492.119528	27677.623404	30.985664
492.128575	27732.253835	30.990682
493.124553	27778.195388	30.995700
493.308529	27834.374390	31.000717
493.596323	27878.348195	31.005735
494.343969	27930.967829	31.010752
494.962295	27976.076463	31.015770
495.298629	28026.871735	31.020788
495.440508	28074.768894	31.025805
496.208981	28121.039139	31.030823
496.883034	28157.622307	31.035840
497.057272	28221.548118	31.040858
497.152818	28272.043211	31.045876
497.802705	28329.941706	31.050893
498.387704	28377.094626	31.055911
498.795793	28435.900874	31.060928
499.384717	28490.188720	31.065946
499.718843	28540.837609	31.070964
500.432457	28599.142864	31.075981
500.761206	28665.596730	31.080999
501.712621	28713.447113	31.086016
501.894775	28764.112293	31.091034
502.574131	28818.531337	31.096052
503.441074	28876.389501	31.101069
503.660255	28937.610291	31.106087
504.416741	28971.487627	31.111104
504.073596	29030.672338	31.116122
505.185132	29085.017680	31.121140
505.824697	29141.706104	31.126157
505.933539	29204.277273	31.131175
506.728046	29236.694603	31.136192
507.051841	29309.719530	31.141210
508.410709	29343.034376	31.146228
508.892201	29403.563641	31.151245
509.430781	29451.269741	31.156263
510.254422	29473.058049	31.161280
510.811833	29518.392124	31.166298
511.592850	29552.149825	31.171316
512.086543	29572.841325	31.176333
513.077350	29592.046938	31.181351
513.782458	29611.350235	31.186368
514.126328	29657.171054	31.191386
514.498896	29674.661809	31.196404
515.003435	29720.872670	31.201421
514.974465	29739.029194	31.206439
515.702962	29765.164909	31.211456
515.751197	29801.413270	31.216474
516.350666	29839.504465	31.221492
516.517773	29879.190861	31.226509
516.968115	29932.260018	31.231527
517.325111	29956.769631	31.236544
516.998335	30009.614057	31.241562
517.661275	30050.095948	31.246580
518.095978	30108.367167	31.251597
518.159910	30169.311929	31.256615
518.424664	30228.655832	31.261632
518.734721	30301.327548	31.266650
519.296334	30358.840432	31.271668
520.072506	30423.924203	31.276685
520.367453	30493.980762	31.281703
521.214653	30557.504304	31.286720
521.499786	30627.443136	31.291738
522.077837	30685.900823	31.296756
522.596805	30760.682061	31.301773
523.023382	30821.559733	31.306791
523.957598	30885.470760	31.311808
524.581214	30950.496511	31.316826
525.564264	31009.005114	31.321844
526.212549	31067.443011	31.326861
526.408274	31134.117560	31.331879
527.216364	31182.793450	31.336896
527.637138	31236.855783	31.341914
528.087386	31297.933117	31.346932
529.380818	31348.374934	31.351949
530.140364	31385.461881	31.356967
531.560298	31428.942174	31.361984
531.388791	31465.621492	31.367002
532.141114	31510.477393	31.372020
532.787295	31550.933985	31.377037
532.645989	31603.891401	31.382055
533.125110	31638.308766	31.387072
533.341924	31694.258174	31.392090
533.852027	31748.881541	31.397108
534.170455	31801.426033	31.402125
535.112660	31851.419356	31.407143
536.110450	31886.739063	31.412160
536.744793	31947.390719	31.417178
537.207804	31988.055255	31.422196
537.855884	32042.732469	31.427213
537.899231	32086.242997	31.432231
538.490866	32123.097369	31.437248
538.983988	32183.060117	31.442266
539.212340	32237.012180	31.447284
539.645117	32282.667436	31.452301
540.372340	32351.101395	31.457319
540.892232	32402.093643	31.462336
541.082913	32472.456129	31.467354
541.634319	32515.735511	31.472372
542.348443	32574.684996	31.477389
542.758222	32641.004925	31.482407
543.642524	32687.738289	31.487424
544.227678	32748.003276	31.492442
544.591577	32816.060481	31.497460
545.114897	32862.200805	31.502477
545.820810	32920.376623	31.507495
546.182306	32978.363412	31.512512
546.333828	33051.129486	31.517530
546.833689	33103.474356	31.522548
547.883696	33163.944803	31.527565
548.041492	33234.546090	31.532583
548.447789	33299.307207	31.537600
548.775747	33372.073857	31.542618
549.597716	33434.829464	31.547636
550.162388	33507.024326	31.552653
550.620703	33572.093381	31.557671
551.307949	33631.476804	31.562688
551.498772	33700.850221	31.567706
552.165404	33758.615624	31.572724
553.330689	33804.781748	31.577741
553.674585	33875.108731	31.582759
554.057771	33935.354326	31.587776
554.978604	33993.510799	31.592794
555.184429	34051.009326	31.597812
555.843934	34106.678690	31.602829
556.320046	34168.894493	31.607847
556.842351	34218.228666	31.612864
557.373267	34275.415479	31.617882
557.682758	34339.505340	31.622900
558.251606	34400.794708	31.627917
558.826496	34460.748519	31.632935
559.495817	34525.972395	31.637952
559.847844	34590.384306	31.642970
560.686028	34659.130729	31.647988
561.643407	34718.921261	31.653005
561.896091	34800.188271	31.658023
562.457717	34848.675169	31.663040
562.997805	34910.977667	31.668058
563.729017	34976.091993	31.673076
564.726239	35031.055270	31.678093
564.809159	35099.486355	31.683111
565.130297	35156.164727	31.688128
565.784831	35226.928555	31.693146
566.389611	35299.543772	31.698164
567.346196	35358.677056	31.703181
567.968095	35432.321882	31.708199
568.453124	35481.088228	31.713216
569.271071	35552.334419	31.718234
569.575911	35615.056913	31.723252
570.676017	35667.335446	31.728269
570.706123	35724.868394	31.733287
571.770646	35772.047172	31.738304
572.550151	35825.152270	31.743322
573.291010	35874.603254	31.748340
574.211639	35926.703913	31.753357
574.162249	35967.335978	31.758375
575.080241	36026.310594	31.763392
575.823114	36082.300564	31.768410
576.296741	36136.735196	31.773428
576.622559	36181.894288	31.778445
576.690716	36251.013865	31.783463
577.210107	36295.936145	31.788480
577.817905	36353.678657	31.793498
578.107809	36435.710662	31.798516
578.964969	36501.702848	31.803533
579.006000	36570.446277	31.808551
579.968517	36622.785045	31.813568
581.555525	36671.615633	31.818586
581.768466	36732.113386	31.823604
582.833845	36761.198783	31.828621
583.226690	36819.849325	31.833639
584.209962	36870.613750	31.838656
584.790539	36923.218455	31.843674
584.588033	36971.692143	31.848692
585.364011	37032.792222	31.853709
585.636851	37102.733373	31.858727
586.212121	37155.888771	31.863744
586.620290	37216.542111	31.868762
587.139892	37278.745774	31.873780
587.606943	37328.681518	31.878797
587.946555	37408.658354	31.883815
588.346950	37468.972979	31.888832
588.747138	37530.559718	31.893850
589.197415	37616.925937	31.898868
589.936120	37684.441150	31.903885
590.641360	37758.473109	31.908903
591.232106	37833.998171	31.913920
592.048494	37888.009077	31.918938
592.291531	37948.881517	31.923956
593.166541	38018.581583	31.928973
593.385359	38077.861465	31.933991
593.899113	38148.963051	31.939008
594.513538	38219.423372	31.944026
594.747215	38298.632606	31.949044
595.322449	38372.477089	31.954061
596.171477	38449.502278	31.959079
597.304637	38533.992628	31.964096
597.420923	38602.008592	31.969114
597.857864	38682.457887	31.974132
598.401742	38751.499002	31.979149
599.073944	38827.942693	31.984167
600.055009	38901.353024	31.989184
601.224328	38950.886887	31.994202
601.764580	39024.960746	31.999220
602.632118	39092.504125	32.004237
603.236344	39155.176867	32.009255
604.085978	39208.056265	32.014272
604.806408	39275.927629	32.019290
604.853249	39331.420850	32.024308
605.853023	39383.720447	32.029325
606.199045	39456.287843	32.034343
606.933523	39529.536277	32.039360
607.869483	39570.360905	32.044378
608.859370	39621.393955	32.049396
609.857375	39686.304503	32.054413
610.324110	39734.432003	32.059431
610.684392	39789.878010	32.064448
611.122782	39833.247414	32.069466
611.688077	39899.271809	32.074484
612.266376	39956.604588	32.079501
612.630335	40014.465355	32.084519
612.974078	40081.095160	32.089536
613.637986	40145.633245	32.094554
614.156218	40219.472553	32.099572
614.713121	40287.377852	32.104589
615.107001	40360.228184	32.109607
615.446072	40437.298671	32.114624
616.466721	40510.570072	32.119642
616.910320	40583.094269	32.124660
617.386177	40646.636144	32.129677
618.550188	40708.079099	32.134695
619.356600	40782.851627	32.139712
619.547136	40838.133141	32.144730
619.986135	40916.524385	32.149748
620.514048	40994.718195	32.154765
621.134915	41075.690615	32.159783
621.374614	41165.795419	32.164800
622.408663	41239.569436	32.169818
622.703781	41325.495910	32.174836
623.196995	41400.906672	32.179853
623.810876	41480.515182	32.184871
624.197021	41566.080509	32.189888
625.203138	41643.588857	32.194906
626.270829	41729.143399	32.199924
627.357771	41789.371577	32.204941
627.713071	41862.483632	32.209959
628.308038	41949.553606	32.214976
629.305362	42011.221025	32.219994
629.771020	42083.097204	32.225012
629.982353	42153.487761	32.230029
630.955993	42233.823009	32.235047
631.227093	42303.187764	32.240064
632.051406	42379.027695	32.245082
632.643328	42458.928181	32.250100
633.169879	42517.234047	32.255117
633.861818	42581.886563	32.260135
634.270354	42656.391480	32.265152
635.356920	42712.967039	32.270170
636.600541	42766.186272	32.275188
637.152877	42822.787259	32.280205
637.707047	42882.039956	32.285223
638.106803	42944.806787	32.290240
638.825300	43006.599355	32.295258
639.320686	43062.364412	32.300276
640.066562	43131.357110	32.305293
640.868800	43190.285697	32.310311
641.401498	43250.174520	32.315328
642.189872	43318.150652	32.320346
642.854308	43381.446673	32.325364
643.280398	43436.892815	32.330381
643.923706	43503.321375	32.335399
644.363324	43574.983505	32.340416
644.867790	43644.788310	32.345434
645.491709	43713.313969	32.350452
645.914589	43788.477747	32.355469
646.643723	43864.693086	32.360487
647.018672	43953.273733	32.365504
647.588384	44033.083652	32.370522
647.713024	44105.276575	32.375540
648.969229	44190.173636	32.380557
649.569575	44263.478865	32.385575
650.349834	44350.040166	32.390592
651.051154	44441.458076	32.395610
651.272815	44519.076464	32.400628
651.944040	44610.771696	32.405645
652.932530	44680.790918	32.410663
653.749996	44761.440760	32.415680
654.803234	44836.160521	32.420698
655.243868	44915.272519	32.425716
655.830774	44990.145687	32.430733
656.821575	45066.278528	32.435751
657.522755	45141.035552	32.440768
658.286149	45218.737878	32.445786
659.134961	45285.934513	32.450804
659.737366	45372.463627	32.455821
660.280520	45430.977969	32.460839
660.797642	45506.111005	32.465856
661.840968	45586.187193	32.470874
662.238569	45664.930580	32.475892
662.559652	45732.879033	32.480909
663.191134	45806.816665	32.485927
663.785858	45892.241184	32.490944
664.308348	45973.784854	32.495962
665.045436	46057.080577	32.500980
665.675121	46135.992849	32.505997
666.427305	46220.846611	32.511015
666.977806	46303.700615	32.516032
667.373854	46392.481942	32.521050
668.104083	46482.042095	32.526068
668.750303	46574.868850	32.531085
669.373285	46655.502130	32.536103
669.758644	46745.325733	32.541120
670.751246	46823.656793	32.546138
671.434481	46922.990159	32.551156
672.768840	46990.491630	32.556173
673.475348	47080.118540	32.561191
673.600052	47150.820132	32.566208
674.648911	47237.492509	32.571226
674.976488	47331.720789	32.576244
675.510723	47412.293018	32.581261
676.296898	47504.305491	32.586279
676.932924	47589.487742	32.591296
677.712660	47659.340991	32.596314
678.279012	47739.634586	32.601332
678.752890	47824.677313	32.606349
679.679911	47885.611597	32.611367
680.035746	47984.774094	32.616384
680.565985	48062.649824	32.621402
681.252062	48150.245225	32.626420
681.963971	48251.545011	32.631437
682.881114	48321.889584	32.636455
683.315408	48413.134064	32.641472
683.862704	48511.159275	32.646490
684.677520	48592.091238	32.651508
685.220583	48688.715951	32.656525
685.997719	48779.337143	32.661543
686.632283	48868.873869	32.666560
687.343666	48953.929799	32.671578
687.840799	49052.313459	32.676596
688.571514	49150.870638	32.681613
689.889630	49224.373500	32.686631
690.750286	49313.486543	32.691648
691.612895	49398.690019	32.696666
691.986385	49492.861432	32.701684
692.625891	49589.957971	32.706701
693.594099	49669.716485	32.711719
693.824421	49752.682656	32.716736
694.858698	49846.977232	32.721754
695.433709	49939.636408	32.726772
696.214886	50025.175099	32.731789
696.642939	50118.753168	32.736807
697.493785	50211.295469	32.741824
699.453792	50276.327209	32.746842
700.175006	50340.992114	32.751860
700.988679	50426.186146	32.756877
701.606088	50503.975340	32.761895
702.257108	50575.228058	32.766912
702.605155	50649.398767	32.771930
703.238287	50736.904252	32.776948
703.612298	50818.041618	32.781965
704.520290	50907.239541	32.786983
704.813495	50994.903402	32.792000
705.119366	51081.100108	32.797018
705.866747	51176.250816	32.802036
706.404543	51281.458064	32.807053
707.356893	51382.665254	32.812071
708.169947	51468.855739	32.817088
709.971919	51543.942606	32.822106
711.675998	51606.121720	32.827124
712.334726	51666.720744	32.832141
713.206692	51727.237368	32.837159
713.995691	51792.761374	32.842176
714.605665	51861.460984	32.847194
715.088251	51915.450816	32.852212
715.304903	51989.329379	32.857229
716.376822	52050.761540	32.862247
717.170936	52122.612261	32.867264
717.432434	52194.172184	32.872282
718.255849	52252.291693	32.877300
718.423397	52342.458701	32.882317
719.186957	52408.086911	32.887335
719.558143	52492.131324	32.892352
720.307907	52567.654944	32.897370
720.597148	52667.923416	32.902388
720.992923	52766.292288	32.907405
721.559836	52847.747456	32.912423
722.347564	52956.141169	32.917440
722.930988	53043.406309	32.922458
723.575768	53141.180038	32.927476
724.118527	53240.405145	32.932493
724.788049	53334.871789	32.937511
725.719278	53429.295674	32.942528
726.444065	53509.337713	32.947546
727.333251	53596.422175	32.952564
727.910278	53703.149131	32.957581
728.805793	53772.354820	32.962599
729.612197	53867.521641	32.967616
730.016154	53961.517140	32.972634
731.192216	54047.513843	32.977652
731.550109	54154.462666	32.982669
731.900046	54240.413431	32.987687
732.684912	54353.547331	32.992704
733.249345	54455.757000	32.997722
733.721148	54557.635022	33.002740
734.497258	54664.890320	33.007757
735.416326	54785.497479	33.012775
735.709647	54890.496133	33.017792
736.845834	54997.055682	33.022810
737.792129	55099.268828	33.027828
738.255552	55219.296831	33.032845
739.319630	55327.190540	33.037863
740.102363	55436.432822	33.042880
741.054674	55550.323097	33.047898
741.722129	55643.089026	33.052916
742.286708	55759.824516	33.057933
743.300124	55862.757138	33.062951
743.702813	55966.719930	33.067968
744.332910	56090.396611	33.072986
745.731491	56182.766343	33.078004
746.558614	56290.439094	33.083021
747.620319	56389.720817	33.088039
748.280302	56498.963986	33.093056
749.113902	56590.297932	33.098074
750.467412	56678.835828	33.103092
751.209421	56768.903078	33.108109
752.387890	56851.821930	33.113127
753.020358	56942.577822	33.118144
753.826511	57029.861829	33.123162
754.460382	57106.843769	33.128180
755.576787	57203.504650	33.133197
755.868159	57274.951821	33.138215
756.833195	57366.362424	33.143232
757.487287	57454.090441	33.148250
758.558658	57534.211697	33.153268
759.203577	57631.217906	33.158285
759.952688	57710.748576	33.163303
760.899547	57807.219239	33.168320
761.284634	57891.455073	33.173338
762.298909	57976.990153	33.178356
762.484557	58066.820268	33.183373
763.270944	58155.540557	33.188391
764.097063	58249.391991	33.193408
764.758211	58345.805021	33.198426
765.877942	58423.805015	33.203444
766.472650	58531.294503	33.208461
767.095137	58610.432618	33.213479
767.818368	58714.382146	33.218496
768.404039	58813.375453	33.223514
768.752279	58915.776572	33.228532
769.455200	59015.693074	33.233549
770.390722	59128.633513	33.238567
770.998522	59242.191122	33.243584
771.384197	59348.898013	33.248602
772.088349	59439.141574	33.253620
772.548181	59570.059402	33.258637
773.420644	59677.148968	33.263655
773.807613	59796.920239	33.268672
775.246887	59904.713671	33.273690
777.780302	59972.640523	33.278708
778.794917	60056.712002	33.283725
779.471942	60135.398447	33.288743
780.601927	60201.541888	33.293760
781.496834	60275.813442	33.298778
782.257400	60339.117645	33.303796
783.191782	60403.271774	33.308813
783.390702	60487.896846	33.313831
783.921541	60562.242214	33.318848
784.477378	60648.711248	33.323866
785.189233	60708.529856	33.328884
786.091244	60794.443092	33.333901
786.353062	60899.105773	33.338919
787.444088	60983.301219	33.343936
788.104549	61074.045951	33.348954
788.914525	61166.687641	33.353972
789.269638	61257.957610	33.358989
789.803256	61353.363346	33.364007
790.129910	61448.778427	33.369024
790.997331	61569.416233	33.374042
792.509329	61665.666761	33.379060
792.789580	61775.330066	33.384077
793.418236	61878.837539	33.389095
794.026262	61989.326366	33.394112
795.110849	62101.892276	33.399130
795.979385	62210.980456	33.404148
796.774697	62327.343257	33.409165
796.900324	62443.975312	33.414183
797.668721	62556.558027	33.419200
798.289602	62686.736268	33.424218
799.430748	62797.204649	33.429236
800.292174	62940.269964	33.434253
801.187247	63045.780870	33.439271
801.877883	63178.447307	33.444288
802.444890	63299.859184	33.449306
803.556928	63432.274387	33.454324
804.086986	63540.186729	33.459341
804.974838	63677.602213	33.464359
805.867411	63790.619984	33.469376
806.887068	63908.237839	33.474394
808.088095	64037.993879	33.479412
808.819001	64154.750637	33.484429
809.807060	64269.948595	33.489447
810.712959	64381.033241	33.494464
811.433226	64500.189324	33.499482
812.263915	64607.337047	33.504500
813.029687	64738.079590	33.509517
813.741246	64852.713332	33.514535
814.718800	64956.399989	33.519552
815.696362	65074.941694	33.524570
816.787734	65189.451379	33.529588
817.443314	65300.417963	33.534605
818.091899	65408.725080	33.539623
818.788712	65516.980552	33.544640
819.821187	65640.238377	33.549658
820.627682	65753.439156	33.554676
821.793916	65868.016092	33.559693
822.578522	65967.744607	33.564711
823.704859	66070.735899	33.569728
824.374149	66192.931774	33.574746
825.344883	66310.413360	33.579764
825.987872	66406.962391	33.584781
827.004842	66520.233741	33.589799
827.477696	66630.428456	33.594816
828.134513	66738.475647	33.599834
828.958639	66839.573602	33.604852
829.898687	66948.788866	33.609869
830.426652	67066.094960	33.614887
831.437546	67163.693043	33.619904
832.281158	67281.472930	33.624922
832.852944	67377.456611	33.629940
833.861751	67498.535699	33.634957
833.878601	67602.849371	33.639975
834.853342	67723.303199	33.644992
835.691143	67842.566524	33.650010
836.338219	67954.086018	33.655028
836.950091	68079.001887	33.660045
838.182487	68189.243771	33.665063
839.242439	68303.194146	33.670080
839.896183	68421.732508	33.675098
840.492705	68548.676773	33.680116
841.650599	68657.751180	33.685133
842.291125	68796.973643	33.690151
843.259432	68905.208173	33.695168
843.876219	69033.909598	33.700186
844.792351	69164.484364	33.705204
845.680520	69271.760372	33.710221
846.469934	69407.864331	33.715239
847.683674	69524.280617	33.720256
848.420806	69653.003877	33.725274
849.294531	69787.629548	33.730292
850.320789	69900.177877	33.735309
850.681311	70043.583400	33.740327
851.982705	70165.154284	33.745344
852.451450	70296.568620	33.750362
853.595363	70424.571841	33.755380
854.730191	70551.970353	33.760397
855.711955	70670.783296	33.765415
857.312614	70780.864094	33.770432
858.159002	70895.464373	33.775450
859.371621	71014.361251	33.780468
859.979192	71117.020327	33.785485
860.604499	71228.288796	33.790503
861.364432	71342.703420	33.795520
862.055170	71473.266375	33.800538
862.717610	71590.455251	33.805556
863.776495	71717.316841	33.810573
864.556438	71830.364987	33.815591
865.824583	71943.522815	33.820608
866.315258	72067.034187	33.825626
867.359925	72189.746597	33.830644
867.988857	72323.701537	33.835661
868.535936	72441.995394	33.840679
869.763723	72576.396833	33.845696
870.754459	72698.229465	33.850714
871.718398	72809.051857	33.855732
872.361923	72927.477897	33.860749
872.835354	73056.695211	33.865767
874.021343	73190.550922	33.870784
874.965945	73310.725232	33.875802
876.182205	73440.935139	33.880820
877.192821	73563.559829	33.885837
877.530403	73696.768311	33.890855
878.345937	73826.490226	33.895872
879.119245	73958.022153	33.900890
879.477031	74093.392452	33.905908
880.784218	74218.235793	33.910925
881.408710	74358.369803	33.915943
882.221574	74486.736481	33.920960
882.962248	74641.214678	33.925978
884.060238	74776.340537	33.930996
884.815560	74911.036866	33.936013
885.616337	75050.393670	33.941031
886.484541	75196.127562	33.946048
886.982180	75336.054818	33.951066
888.116192	75483.783112	33.956084
888.887960	75615.812276	33.961101
889.566961	75740.869259	33.966119
890.546710	75869.324035	33.971136
891.769756	76006.713608	33.976154
892.264151	76150.308390	33.981172
893.571171	76262.628581	33.986189
894.212019	76408.281598	33.991207
895.326841	76547.286187	33.996224
896.402178	76683.148564	34.001242
897.244728	76807.748234	34.006260
898.442063	76938.779062	34.011277
899.140343	77068.583870	34.016295
900.097447	77211.305955	34.021312
900.774228	77349.078726	34.026330
901.580280	77482.979241	34.031348
902.091415	77618.529431	34.036365
903.274453	77773.842126	34.041383
904.275244	77927.465636	34.046400
905.598535	78050.620450	34.051418
906.700037	78188.037375	34.056436
907.980743	78318.037979	34.061453
908.302506	78464.630091	34.066471
909.276871	78598.237582	34.071488
910.347773	78723.069669	34.076506
911.071684	78864.487337	34.081524
912.398006	78987.937809	34.086541
913.721181	79117.771626	34.091559
915.197645	79238.864697	34.096576
916.413674	79358.578238	34.101594
917.182668	79479.694546	34.106612
918.188737	79599.886820	34.111629
918.757749	79714.187065	34.116647
919.428825	79834.201869	34.121664
920.625261	79970.545125	34.126682
921.105230	80091.073593	34.131700
922.041800	80229.156560	34.136717
922.485065	80357.023804	34.141735
923.436257	80494.068594	34.146752
924.556330	80637.285466	34.151770
925.432720	80774.812416	34.156788
926.014458	80915.602321	34.161805
927.169710	81056.070688	34.166823
928.048352	81190.209195	34.171840
928.796155	81332.018039	34.176858
929.462965	81495.981726	34.181876
930.654958	81631.507095	34.186893
931.085167	81790.071686	34.191911
932.067327	81926.810099	34.196928
933.034925	82075.868548	34.201946
933.535575	82242.357534	34.206964
935.060402	82384.645660	34.211981
935.497068	82540.804176	34.216999
936.722307	82699.901783	34.222016
938.027761	82839.008930	34.227034
938.740768	83002.279985	34.232052
939.802470	83150.172228	34.237069
940.455118	83299.221106	34.242087
941.713362	83447.228332	34.247104
942.623198	83600.279297	34.252122
943.146592	83757.785688	34.257140
944.281294	83910.409358	34.262157
945.124954	84068.611542	34.267175
946.407990	84215.094932	34.272192
947.562259	84373.127728	34.277210
948.747517	84517.642615	34.282228
949.957575	84652.898267	34.287245
951.111910	84800.159523	34.292263
952.054761	84927.584044	34.297280
953.474561	85055.310137	34.302298
954.412859	85167.109375	34.307316
955.330641	85290.971673	34.312333
956.152132	85416.179197	34.317351
956.897024	85543.595515	34.322368
957.774435	85674.438892	34.327386
958.316202	85807.078369	34.332404
959.210376	85922.931548	34.337421
960.138404	86063.778251	34.342439
960.467281	86197.562359	34.347456
962.014015	86336.340814	34.352474
962.329583	86489.977295	34.357492
963.597948	86626.772394	34.362509
964.196630	86783.875722	34.367527
964.825016	86933.559513	34.372544
965.935894	87089.751452	34.377562
966.721979	87257.982281	34.382580
967.569344	87419.250267	34.387597
968.111812	87577.753940	34.392615
969.702494	87746.981753	34.397632
970.859294	87907.379427	34.402650
971.858987	88069.139278	34.407668
973.058983	88219.129236	34.412685
973.616660	88379.572101	34.417703
974.651197	88556.218801	34.422720
976.408780	88715.927993	34.427738
977.291861	88866.670467	34.432756
978.246564	89005.663751	34.437773
979.028314	89179.129605	34.442791
979.886253	89342.402353	34.447808
980.947280	89494.815370	34.452826
981.584883	89662.157680	34.457844
982.750622	89823.870512	34.462861
983.814360	90009.313065	34.467879
984.518129	90154.796638	34.472896
986.052152	90326.330484	34.477914
987.149668	90501.576426	34.482932
988.105404	90651.419632	34.487949
989.179040	90812.970875	34.492967
990.258325	90981.648130	34.497984
991.434386	91132.305996	34.503002
992.246248	91304.567314	34.508020
993.504020	91459.403252	34.513037
994.228717	91615.638226	34.518055
994.943835	91788.311369	34.523072
996.042272	91951.391414	34.528090
996.931106	92121.595387	34.533108
997.886620	92290.909851	34.538125
998.736162	92459.882256	34.543143
999.802456	92629.320044	34.548160
1000.687300	92792.649904	34.553178
1001.585719	92967.092327	34.558196
1002.696235	93138.501030	34.563213
1004.058176	93314.958018	34.568231
1004.993398	93492.056361	34.573248
1006.815818	93649.730883	34.578266
1007.456798	93822.221948	34.583284
1008.200218	93983.152766	34.588301
1009.198712	94146.327413	34.593319
1009.836434	94319.613703	34.598336
1011.497867	94470.788252	34.603354
1012.063076	94640.221541	34.608372
1013.248000	94812.591838	34.613389
1014.936993	94976.778361	34.618407
1015.950000	95141.710541	34.623424
1017.842168	95260.938311	34.628442
1020.145776	95378.149218	34.633460
1021.688002	95488.701008	34.638477
1023.011220	95593.871257	34.643495
1023.305575	95702.623517	34.648512
1024.337768	95807.697144	34.653530
1024.848047	95933.093604	34.658548
1025.891398	96055.674560	34.663565
1026.274901	96166.787824	34.668583
1026.874030	96295.798446	34.673600
1027.782887	96436.760069	34.678618
1027.972062	96583.304030	34.683636
1028.640277	96725.560352	34.688653
1029.412663	96867.730663	34.693671
1030.068054	97044.786944	34.698688
1031.045604	97202.649132	34.703706
1031.925298	97377.277985	34.708724
1032.775778	97538.423300	34.713741
1033.750380	97715.659550	34.718759
1034.113173	97893.865310	34.723776
1035.481015	98072.545781	34.728794
1036.288370	98268.506960	34.733812
1037.128402	98457.203312	34.738829
1038.822825	98645.411863	34.743847
1039.879782	98835.208404	34.748864
1041.263977	99008.872786	34.753882
1042.255620	99201.018847	34.758900
1043.278792	99371.485086	34.763917
1044.687670	99550.840379	34.768935
1046.060462	99721.371555	34.773952
1047.537383	99891.595480	34.778970
1048.852350	100059.536548	34.783988
1049.585950	100228.321748	34.789005
1050.677687	100403.145595	34.794023
1051.851632	100580.628732	34.799040
1052.926213	100745.790445	34.804058
1053.636119	100929.867205	34.809076
1053.993975	101113.085411	34.814093
1055.114159	101293.342749	34.819111
1056.049048	101478.342333	34.824128
1057.126046	101666.612023	34.829146
1057.775894	101869.395201	34.834164
1058.851902	102062.865934	34.839181
1060.162021	102254.153155	34.844199
1061.184661	102452.504450	34.849216
1061.998005	102641.223714	34.854234
1063.468399	102844.626259	34.859252
1064.149866	103047.875734	34.864269
1065.431763	103239.111635	34.869287
1066.257411	103431.950198	34.874304
1067.811377	103636.174642	34.879322
1068.651549	103845.754883	34.884340
1069.682040	104039.507591	34.889357
1070.942271	104236.921612	34.894375
1071.896465	104435.400758	34.899392
1072.889763	104618.811305	34.904410
1074.689347	104832.990082	34.909428
1075.503291	105013.881233	34.914445
1076.952460	105214.925065	34.919463
1077.256618	105426.480823	34.924480
1078.411190	105618.128863	34.929498
1079.401577	105833.386590	34.934516
1080.368975	106034.034997	34.939533
1081.200846	106236.948950	34.944551
1082.405321	106449.060881	34.949568
1083.869801	106645.097917	34.954586
1085.171714	106847.407057	34.959604
1086.416422	107043.103383	34.964621
1089.212365	107198.396690	34.969639
1091.650248	107346.670192	34.974656
1092.931375	107494.628873	34.979674
1094.187814	107626.393529	34.984692
1095.118130	107769.902812	34.989709
1096.311173	107897.715021	34.994727
1096.892651	108041.929295	34.999744
1097.815543	108169.344114	35.004762
1099.083288	108315.891039	35.009780
1099.573346	108444.822509	35.014797
1100.782845	108586.491581	35.019815
1101.415645	108738.604587	35.024832
1102.371029	108881.976399	35.029850
1103.185097	109046.600476	35.034868
1104.089152	109210.298754	35.039885
1104.820107	109377.459127	35.044903
1105.493162	109564.326065	35.049920
1106.424274	109737.472093	35.054938
1107.245778	109924.000366	35.059956
1108.173509	110117.972950	35.064973
1109.195579	110305.395405	35.069991
1109.962843	110504.020549	35.075008
1111.207695	110694.220923	35.080026
1112.444793	110889.781987	35.085044
1113.041633	111097.103732	35.090061
1114.247107	111307.949361	35.095079
1114.753817	111530.350398	35.100096
1115.927861	111733.616896	35.105114
1117.223241	111944.984637	35.110132
1118.206380	112168.604296	35.115149
1120.070696	112385.277855	35.120167
1120.988061	112606.935815	35.125184
1122.328817	112806.610493	35.130202
1123.715325	113010.940828	35.135220
1124.464606	113226.855007	35.140237
1125.879182	113436.073683	35.145255
1126.725682	113651.341735	35.150272
1128.185925	113862.481657	35.155290
1129.510006	114073.594995	35.160308
1130.606128	114287.851330	35.165325
1131.884876	114495.326859	35.170343
1132.917724	114705.264231	35.175360
1134.792196	114912.758554	35.180378
1136.728300	115097.668480	35.185396
1137.337239	115286.029269	35.190413
1139.060722	115476.310393	35.195431
1140.211265	115681.066746	35.200448
1142.146554	115853.388784	35.205466
1143.456748	116026.499204	35.210484
1144.205572	116215.096530	35.215501
1145.492663	116393.141373	35.220519
1146.414848	116579.736104	35.225536
1147.506057	116761.768477	35.230554
1148.188179	116940.828846	35.235572
1149.459659	117138.898958	35.240589
1150.227260	117322.952164	35.245607
1150.942449	117526.222730	35.250624
1151.903527	117729.036053	35.255642
1153.175226	117941.555488	35.260660
1153.434458	118160.984156	35.265677
1154.505212	118360.324918	35.270695
1155.648187	118593.713010	35.275712
1156.499646	118807.676657	35.280730
1157.887291	119031.119647	35.285748
1158.852745	119248.514150	35.290765
1160.503937	119461.286325	35.295783
1161.632468	119691.657426	35.300800
1162.503827	119922.921769	35.305818
1163.674885	120133.877523	35.310836
1164.848946	120363.194768	35.315853
1165.905428	120589.416115	35.320871
1166.817233	120790.827334	35.325888
1167.796397	121012.845195	35.330906
1169.178930	121227.068552	35.335924
1170.463061	121441.487128	35.340941
1171.449468	121655.132764	35.345959
1172.924778	121877.442784	35.350976
1174.221755	122082.055981	35.355994
1175.735973	122305.186494	35.361012
1177.032677	122502.085440	35.366029
1178.234938	122714.309232	35.371047
1179.535282	122917.736508	35.376064
1180.527162	123126.069599	35.381082
1181.573818	123342.860284	35.386100
1182.688814	123566.775893	35.391117
1183.864990	123780.000094	35.396135
1185.777952	123989.099640	35.401152
1187.082782	124198.326384	35.406170
1188.820404	124401.222765	35.411188
1189.698990	124603.869462	35.416205
1190.984777	124808.211869	35.421223
1191.759679	125018.875173	35.426240
1192.810550	125221.560977	35.431258
1194.339529	125430.949442	35.436276
1195.193320	125655.202634	35.441293
1196.492955	125865.544463	35.446311
1197.919315	126084.573581	35.451328
1199.000554	126298.173558	35.456346
1199.962921	126508.030561	35.461364
1201.124642	126744.496519	35.466381
1202.246846	126963.975088	35.471399
1203.579788	127174.561311	35.476416
1204.491458	127384.242618	35.481434
1206.468306	127608.907890	35.486452
1207.207926	127837.289813	35.491469
1208.491497	128058.524016	35.496487
1209.670572	128289.625136	35.501504
1210.835427	128509.133102	35.506522
1212.459530	128731.013040	35.511540
1213.526968	128960.249095	35.516557
1214.879229	129180.326619	35.521575
1215.907693	129406.974074	35.526592
1217.078435	129628.212811	35.531610
1218.793219	129845.750916	35.536628
1219.626752	130078.189950	35.541645
1221.017530	130294.136890	35.546663
1222.642272	130499.044470	35.551680
1224.171283	130722.158500	35.556698
1225.447836	130937.279481	35.561716
1226.207484	131162.868617	35.566733
1227.043606	131385.848220	35.571751
1228.356523	131612.870349	35.576768
1229.151668	131847.978086	35.581786
1230.565544	132072.160122	35.586804
1231.585999	132318.490473	35.591821
1232.478786	132547.135140	35.596839
1233.703585	132783.116935	35.601856
1234.675479	133045.711963	35.606874
1235.543360	133290.338353	35.611892
1236.765730	133533.247469	35.616909
1238.285075	133780.051864	35.621927
1239.449580	134032.012798	35.626944
1240.660346	134285.185053	35.631962
1242.489540	134523.006799	35.636980
1243.587155	134765.349998	35.641997
1244.814387	135014.455911	35.647015
1246.335642	135255.452459	35.652032
1246.961679	135507.120776	35.657050
1248.689765	135746.058445	35.662068
1249.738860	135976.920232	35.667085
1251.194364	136189.131146	35.672103
1252.898493	136416.059274	35.677120
1253.957694	136650.562655	35.682138
1255.182938	136867.012324	35.687156
1256.666753	137103.540708	35.692173
1257.719013	137307.267763	35.697191
1258.862617	137539.075791	35.702208
1259.852282	137771.177094	35.707226
1261.272889	138003.411748	35.712244
1262.543836	138241.796409	35.717261
1263.729716	138480.589852	35.722279
1265.057549	138711.969948	35.727296
1266.296170	138956.285964	35.732314
1267.410258	139194.627249	35.737332
1268.855046	139433.600306	35.742349
1270.013622	139678.594098	35.747367
1271.263092	139915.992590	35.752384
1272.130147	140168.163689	35.757402
1273.756131	140409.877819	35.762420
1275.040472	140669.642046	35.767437
1276.422485	140914.595236	35.772455
1277.692333	141166.073301	35.777472
1278.526852	141420.655501	35.782490
1279.524316	141677.533091	35.787508
1280.636597	141948.582370	35.792525
1281.597782	142210.617947	35.797543
1283.112447	142474.859251	35.802560
1284.560920	142747.114655	35.807578
1286.711649	143004.027367	35.812596
1287.749825	143264.054762	35.817613
1289.101013	143519.366056	35.822631
1290.380647	143787.282761	35.827648
1291.390929	144069.904743	35.832666
1293.133697	144330.838257	35.837684
1294.376765	144583.702447	35.842701
1295.694710	144838.838657	35.847719
1297.645697	145102.482612	35.852736
1299.737647	145329.190724	35.857754
1302.793640	145537.645215	35.862772
1304.126409	145784.860122	35.867789
1305.702457	145990.594137	35.872807
1307.152888	146205.899141	35.877824
1308.061071	146426.722598	35.882842
1309.207638	146646.493556	35.887860
1310.223056	146864.651585	35.892877
1311.274426	147094.218515	35.897895
1312.240613	147309.419863	35.902912
1313.035805	147544.104649	35.907930
1314.111226	147783.424340	35.912948
1315.428729	148037.264605	35.917965
1316.195929	148289.548801	35.922983
1317.361348	148523.494005	35.928000
1318.413877	148782.646321	35.933018
1319.860731	149037.068292	35.938036
1320.425049	149300.667592	35.943053
1321.668058	149569.217109	35.948071
1323.170938	149828.644938	35.953088
1324.484956	150115.868249	35.958106
1325.497307	150376.915507	35.963124
1327.306257	150664.670178	35.968141
1328.019850	150942.423402	35.973159
1329.737948	151218.249965	35.978176
1331.231101	151473.391355	35.983194
1332.625195	151747.284043	35.988212
1334.001839	152018.061505	35.993229
1335.379873	152289.880736	35.998247
1336.711440	152549.330447	36.003264
1338.075293	152811.097721	36.008282
1339.388363	153057.895705	36.013300
1340.717975	153317.160752	36.018317
1341.908209	153574.979239	36.023335
1343.567770	153810.144530	36.028352
1344.741412	154068.933078	36.033370
1346.491128	154320.804231	36.038388
1348.047999	154575.296448	36.043405
1348.509620	154818.276174	36.048423
1350.070784	155092.507893	36.053440
1351.349637	155365.189905	36.058458
1352.332190	155616.866344	36.063476
1353.691858	155898.912669	36.068493
1354.931751	156162.943088	36.073511
1356.571365	156438.579373	36.078528
1357.962690	156717.214165	36.083546
1359.954709	156970.546676	36.088564
1361.456498	157230.481864	36.093581
1362.140376	157517.801518	36.098599
1363.666724	157771.824919	36.103616
1364.941035	158059.596527	36.108634
1366.335857	158318.389456	36.113652
1367.803464	158608.175484	36.118669
1368.757099	158891.743681	36.123687
1370.108655	159163.399758	36.128704
1371.388054	159462.153759	36.133722
1373.040704	159758.412681	36.138740
1373.894604	160038.669022	36.143757
1374.663679	160351.734803	36.148775
1376.157039	160649.536165	36.153792
1377.764885	160958.852625	36.158810
1379.085664	161267.254634	36.163828
1380.390685	161568.125803	36.168845
1381.911311	161888.767297	36.173863
1383.103916	162184.586892	36.178880
1384.226381	162508.927280	36.183898
1385.930216	162822.796416	36.188916
1387.418861	163125.843410	36.193933
1389.119472	163445.858234	36.198951
1390.154507	163747.043463	36.203968
1391.834326	164059.885482	36.208986
1393.507463	164374.545205	36.214004
1394.694652	164681.053337	36.219021
1396.298843	165005.777538	36.224039
1398.214503	165301.525105	36.229056
1399.665614	165618.184544	36.234074
1400.926081	165923.839419	36.239092
1402.339282	166230.067585	36.244109
1403.094757	166555.831717	36.249127
1404.614594	166875.166190	36.254144
1405.964877	167182.566074	36.259162
1407.409571	167507.792188	36.264180
1408.896771	167822.444327	36.269197
1410.295654	168134.055385	36.274215
1411.764919	168446.900501	36.279232
1413.039524	168780.944524	36.284250
1414.165381	169084.981483	36.289268
1415.915677	169407.519204	36.294285
1417.283772	169740.628704	36.299303
1418.956268	170054.162132	36.304320
1420.331901	170371.325042	36.309338
1422.036663	170680.213303	36.314356
1423.725954	170994.207285	36.319373
1425.187475	171301.122319	36.324391
1426.423639	171617.098761	36.329408
1428.061428	171932.300490	36.334426
1429.357805	172245.301976	36.339444
1430.779644	172554.769845	36.344461
1433.304432	172834.236899	36.349479
1435.385201	173089.021111	36.354496
1437.029375	173363.103914	36.359514
1438.408060	173615.925723	36.364532
1440.056120	173884.173563	36.369549
1441.135916	174142.288503	36.374567
1442.501153	174413.301703	36.379584
1443.767229	174679.383630	36.384602
1444.543970	174960.002047	36.389620
1445.767112	175239.913929	36.394637
1447.016098	175541.561925	36.399655
1448.363104	175814.299307	36.404672
1449.104094	176128.357316	36.409690
1450.260793	176431.041358	36.414708
1451.504379	176743.662511	36.419725
1452.317244	177071.166973	36.424743
1453.976764	177391.122403	36.429760
1454.930045	177723.671737	36.434778
1456.462301	178078.324522	36.439796
1457.940770	178389.127944	36.444813
1459.455522	178728.000424	36.449831
1461.955364	179049.630073	36.454848
1463.717837	179367.461815	36.459866
1465.019565	179696.540138	36.464884
1466.966635	180015.335445	36.469901
1468.540581	180340.476714	36.474919
1470.402785	180656.612107	36.479936
1472.097508	180961.900187	36.484954
1473.196558	181283.165969	36.489972
1474.884613	181594.919097	36.494989
1476.488494	181922.489626	36.500007
1477.309129	182237.829315	36.505024
1478.188972	182571.044490	36.510042
1479.498511	182904.787417	36.515060
1481.474645	183232.799733	36.520077
1482.461470	183582.706853	36.525095
1484.420613	183903.313723	36.530112
1486.333913	184242.956343	36.535130
1487.851474	184569.224840	36.540148
1490.110556	184889.902366	36.545165
1491.777371	185240.406220	36.550183
1492.862157	185552.726460	36.555200
1494.573851	185874.033241	36.560218
1496.261408	186199.851940	36.565236
1498.120706	186509.714312	36.570253
1499.476871	186828.305542	36.575271
1500.790321	187154.750118	36.580288
1502.306685	187456.195243	36.585306
1503.632504	187793.468970	36.590324
1504.955022	188111.451103	36.595341
1506.327887	188442.475742	36.600359
1507.434325	188777.214750	36.605376
1508.704965	189111.674757	36.610394
1510.224524	189454.790914	36.615412
1511.811791	189785.534090	36.620429
1513.128338	190134.514296	36.625447
1514.658714	190471.186171	36.630464
1516.040474	190810.550279	36.635482
1517.870703	191156.189449	36.640500
1519.072836	191500.715641	36.645517
1520.486658	191852.635100	36.650535
1522.002344	192201.099644	36.655552
1523.239883	192553.826689	36.660570
1524.613363	192916.143162	36.665588
1526.325567	193266.726841	36.670605
1527.740708	193626.476370	36.675623
1529.258756	193972.208682	36.680640
1530.966623	194322.951480	36.685658
1532.453913	194672.247362	36.690676
1534.072357	195000.043623	36.695693
1535.513161	195349.122468	36.700711
1537.683759	195664.732702	36.705728
1539.947353	195985.229523	36.710746
1540.846064	196312.999056	36.715764
1542.596773	196646.558412	36.720781
1544.072811	196958.036754	36.725799
1545.423637	197296.895979	36.730816
1546.909439	197624.448387	36.735834
1548.238058	197953.577244	36.740852
1549.780827	198306.743387	36.745869
1550.964613	198646.043455	36.750887
1552.647997	198987.256067	36.755904
1554.394254	199344.241007	36.760922
1555.395700	199700.068464	36.765940
1556.966101	200054.191534	36.770957
1558.541580	200409.077386	36.775975
1560.936088	200746.029985	36.780992
1562.680055	201084.246942	36.786010
1564.587345	201438.715202	36.791028
1566.723604	201779.410090	36.796045
1568.412102	202095.422609	36.801063
1570.041088	202428.992837	36.806080
1572.232151	202756.047482	36.811098
1573.137206	203089.321299	36.816116
1575.175195	203421.127383	36.821133
1576.518363	203757.531576	36.826151
1577.578025	204092.765234	36.831168
1579.233651	204440.560800	36.836186
1580.455671	204781.332036	36.841204
1581.839873	205127.652036	36.846221
1582.763683	205487.927407	36.851239
1584.450956	205832.664364	36.856256
1586.851681	206178.351748	36.861274
1588.260351	206547.427484	36.866292
1590.056673	206896.189015	36.871309
1591.639852	207254.192825	36.876327
1593.505868	207601.790625	36.881344
1595.428635	207948.136283	36.886362
1596.610348	208307.976154	36.891380
1598.103112	208655.525974	36.896397
1599.548939	209013.039948	36.901415
1601.059036	209379.737993	36.906432
1603.129303	209734.866607	36.911450
1604.248402	210086.674554	36.916468
1605.940152	210457.220339	36.921485
1607.387841	210807.224891	36.926503
1609.105792	211181.248833	36.931520
1610.600095	211557.266847	36.936538
1611.978426	211923.553624	36.941556
1613.574392	212277.184222	36.946573
1614.963943	212667.547885	36.951591
1616.294148	213050.456600	36.956608
1618.144284	213421.573469	36.961626
1619.287362	213814.090899	36.966644
1621.293178	214186.505959	36.971661
1622.881973	214564.578687	36.976679
1624.388101	214955.034943	36.981696
1626.526137	215332.791728	36.986714
1628.098449	215728.142032	36.991732
1629.298553	216109.231435	36.996749
1631.349004	216502.728384	37.001767
1632.817779	216875.725666	37.006784
1634.354518	217270.402701	37.011802
1636.222942	217646.943548	37.016820
1637.665541	218028.203922	37.021837
1639.781514	218437.851067	37.026855
1641.183747	218835.680670	37.031872
1643.268588	219185.930342	37.036890
1644.433834	219549.057435	37.041908
1645.966114	219899.375390	37.046925
1647.535192	220273.791476	37.051943
1648.816864	220644.725984	37.056960
1650.559942	221014.239585	37.061978
1651.763692	221405.381481	37.066996
1653.302754	221787.554582	37.072013
1654.742993	222186.889535	37.077031
1655.874400	222581.527349	37.082048
1657.128325	222971.498384	37.087066
1658.431064	223389.046122	37.092084
1660.065094	223803.340490	37.097101
1662.034230	224224.921488	37.102119
1663.465680	224650.732866	37.107136
1664.921959	225071.639646	37.112154
1666.632614	225505.535944	37.117172
1668.313258	225934.257283	37.122189
1670.641667	226340.343767	37.127207
1673.300986	226749.374207	37.132224
1676.103819	227147.384208	37.137242
1677.994164	227549.406842	37.142260
1680.469770	227935.687800	37.147277
1682.663455	228317.342839	37.152295
1683.778575	228710.124451	37.157312
1686.074985	229069.641230	37.162330
1687.877756	229448.874898	37.167348
1689.831936	229827.602069	37.172365
1691.661747	230196.546253	37.177383
1693.069531	230567.923323	37.182400
1694.865766	230943.301411	37.187418
1696.652793	231320.536286	37.192436
1697.697514	231689.461595	37.197453
1699.543468	232067.526969	37.202471
1700.473125	232452.323335	37.207488
1702.270160	232846.401364	37.212506
1703.866613	233231.267567	37.217524
1705.434477	233625.334662	37.222541
1706.992184	234025.983349	37.227559
1708.614798	234426.088939	37.232576
1710.215339	234834.683216	37.237594
1711.359694	235254.962214	37.242612
1712.937735	235660.056914	37.247629
1714.596785	236079.186256	37.252647
1716.169072	236501.937977	37.257664
1717.972946	236915.457161	37.262682
1719.740704	237341.150680	37.267700
1721.609537	237755.550188	37.272717
1723.401874	238185.051921	37.277735
1724.762713	238621.001708	37.282752
1726.585382	239054.107510	37.287770
1728.143373	239485.276609	37.292788
1729.940970	239913.130273	37.297805
1732.185883	240338.193040	37.302823
1733.910887	240771.496547	37.307840
1735.660682	241195.956915	37.312858
1737.541623	241629.668302	37.317876
1738.865947	242060.982963	37.322893
1741.152528	242488.100743	37.327911
1742.468731	242928.080593	37.332928
1744.233412	243348.960883	37.337946
1745.612810	243786.417068	37.342964
1747.263311	244223.778502	37.347981
1748.826148	244664.051047	37.352999
1750.227542	245112.937045	37.358016
1752.144538	245557.826735	37.363034
1754.189874	245995.913461	37.368052
1756.019965	246423.443449	37.373069
1758.209070	246829.754358	37.378087
1760.089575	247258.293345	37.383104
1762.330907	247651.107862	37.388122
1764.204281	248059.072848	37.393140
1766.025612	248457.038195	37.398157
1768.097584	248857.045696	37.403175
1769.594623	249263.804063	37.408192
1771.454093	249662.602774	37.413210
1773.252289	250071.293772	37.418228
1774.462635	250481.352320	37.423245
1776.004549	250903.296002	37.428263
1777.718065	251315.838064	37.433280
1779.628612	251745.444271	37.438298
1781.438429	252171.053799	37.443316
1783.220766	252598.065397	37.448333
1784.950874	253012.816246	37.453351
1786.219635	253454.062798	37.458368
1788.120429	253887.736884	37.463386
1790.132188	254332.976821	37.468404
1791.514131	254779.819744	37.473421
1793.206547	255228.770998	37.478439
1794.645979	255668.263432	37.483456
1796.317826	256127.100431	37.488474
1798.312549	256584.029949	37.493492
1801.002343	257029.819981	37.498509
1803.041219	257473.050212	37.503527
1804.723255	257935.620550	37.508544
1806.732954	258378.525621	37.513562
1808.469337	258828.563399	37.518580
1809.967853	259286.032857	37.523597
1812.081599	259743.934352	37.528615
1813.702253	260196.938177	37.533632
1815.368360	260654.786548	37.538650
1817.061379	261125.636960	37.543668
1818.176650	261583.703167	37.548685
1820.161354	262059.840056	37.553703
1822.180330	262547.529700	37.558720
1825.084281	262976.544057	37.563738
1827.667938	263439.880163	37.568756
1829.856664	263891.163899	37.573773
1831.773025	264329.993987	37.578791
1833.479988	264785.700789	37.583808
1835.107165	265220.412054	37.588826
1836.962351	265669.285887	37.593844
1838.413360	266124.856372	37.598861
1839.931485	266582.447751	37.603879
1841.369285	267058.443962	37.608896
1843.106167	267529.157420	37.613914
1844.590302	267999.454929	37.618932
1846.183059	268483.273966	37.623949
1848.131615	268963.782255	37.628967
1849.571160	269444.958297	37.633984
1851.677823	269925.261691	37.639002
1853.271994	270419.214290	37.644020
1855.060671	270921.822021	37.649037
1857.245678	271409.325189	37.654055
1859.100461	271904.376047	37.659072
1860.448378	272402.735991	37.664090
1862.558092	272900.791723	37.669108
1863.977527	273407.419692	37.674125
1865.905528	273908.653781	37.679143
1867.671975	274420.557421	37.684160
1869.526182	274935.646422	37.689178
1871.389246	275437.193429	37.694196
1873.543617	275948.598459	37.699213
1876.301976	276446.795169	37.704231
1878.830843	276931.057407	37.709248
1881.090012	277388.893872	37.714266
1883.357518	277825.948955	37.719284
1885.702031	278267.029491	37.724301
1888.305731	278689.395754	37.729319
1889.989150	279108.966365	37.734336
1892.229373	279536.496813	37.739354
1894.320739	279963.593723	37.744372
1895.383429	280399.470743	37.749389
1897.401800	280826.958941	37.754407
1898.799659	281275.403588	37.759424
1900.150451	281712.855950	37.764442
1902.024051	282157.714621	37.769460
1903.532181	282614.241137	37.774477
1905.343586	283070.208461	37.779495
1906.848277	283541.034386	37.784512
1908.346343	284018.464560	37.789530
1909.854003	284500.895933	37.794548
1910.987987	285013.259655	37.799565
1913.216639	285493.918154	37.804583
1914.990075	286006.935345	37.809600
1916.754038	286513.144932	37.814618
1918.923685	287007.423646	37.819636
1920.816576	287522.067243	37.824653
1922.811549	288029.732388	37.829671
1924.954349	288539.835289	37.834688
1926.548435	289055.919885	37.839706
1928.486650	289580.480476	37.844724
1930.226781	290106.240201	37.849741
1932.427339	290630.245542	37.854759
1934.966305	291153.075417	37.859776
1936.659453	291687.091866	37.864794
1938.595877	292208.899326	37.869812
1940.560279	292745.686090	37.874829
1942.274228	293269.862707	37.879847
1944.669281	293811.653863	37.884864
1946.451249	294347.955803	37.889882
1948.352322	294872.247088	37.894900
1949.891683	295425.043162	37.899917
1952.085449	295953.472267	37.904935
1954.244407	296500.395350	37.909952
1956.477559	297036.991501	37.914970
1958.802199	297584.618554	37.919988
1960.480630	298130.063564	37.925005
1961.985050	298671.064347	37.930023
1964.031276	299217.611520	37.935040
1965.984845	299776.641801	37.940058
1968.001080	300316.736955	37.945076
1970.103655	300869.971301	37.950093
1972.234025	301414.842060	37.955111
1974.413954	301972.578423	37.960128
1976.514222	302509.422370	37.965146
1979.208257	303041.187470	37.970164
1981.548344	303583.065415	37.975181
1983.614414	304102.737351	37.980199
1985.607787	304635.218595	37.985216
1987.197329	305170.277687	37.990234
1989.760607	305697.350782	37.995252
1991.250169	306234.731208	38.000269
1993.184148	306764.212931	38.005287
1995.173271	307298.583898	38.010304
1996.913568	307844.243198	38.015322
1999.174367	308355.680748	38.020340
2001.403905	308887.614964	38.025357
2003.812452	309411.491208	38.030375
2007.441891	309905.602204	38.035392
2010.136541	310385.541329	38.040410
2012.951521	310873.838269	38.045428
2014.715971	311357.632803	38.050445
2016.669849	311809.496934	38.055463
2018.317215	312256.152292	38.060480
2019.606676	312711.092066	38.065498
2021.484972	313167.836672	38.070516
2022.817666	313637.442007	38.075533
2024.348987	314106.732370	38.080551
2025.807390	314589.160661	38.085568
2027.530314	315075.325946	38.090586
2029.622931	315557.795771	38.095604
2031.472510	316071.638347	38.100621
2033.188298	316575.722890	38.105639
2034.814081	317086.903521	38.110656
2036.523066	317610.763375	38.115674
2038.245942	318138.095929	38.120692
2039.383642	318689.720363	38.125709
2040.935841	319228.651992	38.130727
2043.150335	319797.306224	38.135744
2044.692996	320383.942620	38.140762
2046.739401	320951.193022	38.145780
2048.483734	321532.073035	38.150797
2050.272242	322133.177715	38.155815
2052.430983	322723.551551	38.160832
2054.315153	323325.213568	38.165850
2056.918847	323921.520838	38.170868
2059.445651	324517.936818	38.175885
2062.344459	325098.239185	38.180903
2064.779181	325682.548215	38.185920
2066.944041	326283.171170	38.190938
2069.365341	326867.649015	38.195956
2071.112945	327445.910459	38.200973
2073.339241	328044.855746	38.205991
2075.285625	328630.842164	38.211008
2077.268967	329219.711047	38.216026
2079.304595	329811.104294	38.221044
2081.401922	330412.255830	38.226061
2083.288808	331012.598075	38.231079
2085.497371	331614.201186	38.236096
2087.412880	332223.716371	38.241114
2089.756953	332816.932037	38.246132
2091.556169	333448.996867	38.251149
2093.899049	334052.075107	38.256167
2096.558687	334642.680700	38.261184
2099.025961	335249.025545	38.266202
2102.034071	335838.951496	38.271220
2103.949562	336425.776493	38.276237
2106.547238	337008.522498	38.281255
2108.372157	337607.255062	38.286272
2110.054621	338209.685088	38.291290
2112.631519	338782.921149	38.296308
2114.377212	339371.797559	38.301325
2116.220102	339961.235051	38.306343
2119.003856	340545.103950	38.311360
2121.144442	341142.702919	38.316378
2123.174086	341731.911425	38.321396
2125.019761	342317.259832	38.326413
2127.170403	342912.297813	38.331431
2129.805644	343494.126297	38.336448
2131.691109	344095.437652	38.341466
2133.639405	344674.700317	38.346484
2135.917517	345278.622679	38.351501
2137.308371	345876.846234	38.356519
2139.586724	346464.510013	38.361536
2141.344794	347085.144738	38.366554
2143.353224	347685.908503	38.371572
2145.479527	348298.522616	38.376589
2147.484816	348902.672023	38.381607
2150.512695	349515.654285	38.386624
2152.266352	350118.814041	38.391642
2154.078832	350696.375108	38.396660
2156.494787	351274.438332	38.401677
2158.019947	351865.380419	38.406695
2160.806227	352448.366725	38.411712
2162.449962	353039.755802	38.416730
2164.361716	353638.908632	38.421748
2166.043309	354228.930493	38.426765
2167.983187	354834.786871	38.431783
2170.108502	355451.946894	38.436800
2171.678440	356064.825145	38.441818
2173.958013	356701.378830	38.446836
2175.907093	357317.551287	38.451853
2178.144570	357945.998793	38.456871
2180.696000	358590.141920	38.461888
2183.069041	359214.031479	38.466906
2185.907911	359836.236309	38.471924
2188.691242	360474.780534	38.476941
2190.665437	361092.922401	38.481959
2193.488574	361726.467498	38.486976
2195.026430	362360.595125	38.491994
2197.323338	362983.703539	38.497012
2199.737613	363602.825071	38.502029
2201.646422	364238.206175	38.507047
2203.967989	364878.227629	38.512064
2205.867121	365538.603399	38.517082
2208.278848	366171.231701	38.522100
2211.225096	366795.618303	38.527117
2213.681660	367445.772941	38.532135
2216.004852	368067.045155	38.537152
2218.026817	368708.472745	38.542170
2219.814932	369355.407101	38.547188
2222.274040	370002.371811	38.552205
2224.093391	370642.658159	38.557223
2226.098721	371304.285499	38.562240
2228.018682	371961.780566	38.567258
2230.546433	372625.327056	38.572276
2232.751499	373278.109689	38.577293
2234.864086	373946.722412	38.582311
2237.384253	374606.479949	38.587328
2239.240764	375295.273062	38.592346
2241.243139	375971.779001	38.597364
2243.263091	376656.891888	38.602381
2245.205899	377343.855430	38.607399
2247.280672	378033.598647	38.612416
2249.549204	378735.976052	38.617434
2252.130585	379440.595218	38.622452
2254.077999	380145.177607	38.627469
2256.344630	380847.917682	38.632487
2258.821877	381552.129873	38.637504
2261.237781	382254.942773	38.642522
2264.106159	382940.423781	38.647540
2266.476517	383644.178420	38.652557
2268.192771	384358.193481	38.657575
2270.819098	385063.523680	38.662592
2272.894064	385759.776600	38.667610
2275.186071	386472.103865	38.672628
2277.460771	387195.877956	38.677645
2279.784401	387888.114190	38.682663
2282.015709	388582.606976	38.687680
2284.289328	389309.172756	38.692698
2286.371136	390022.368083	38.697716
2288.758703	390733.494098	38.702733
2290.902325	391455.722031	38.707751
2293.124756	392168.515573	38.712768
2295.128094	392910.023508	38.717786
2296.914245	393643.311215	38.722804
2298.896932	394366.688732	38.727821
2300.934167	395105.856461	38.732839
2303.295822	395828.350806	38.737856
2305.440367	396545.490285	38.742874
2307.538157	397269.488755	38.747892
2309.961502	397982.619176	38.752909
2312.085161	398720.365281	38.757927
2314.741441	399428.074770	38.762944
2317.102927	400158.953479	38.767962
2319.479518	400891.129106	38.772980
2321.893651	401615.246830	38.777997
2323.868890	402363.137514	38.783015
2326.293582	403094.007467	38.788032
2328.479286	403837.339660	38.793050
2330.832419	404580.574064	38.798068
2333.206923	405324.849535	38.803085
2335.216682	406090.651391	38.808103
2338.113750	406819.547872	38.813120
2340.558096	407570.415414	38.818138
2343.140934	408338.239620	38.823156
2345.922005	409079.585774	38.828173
2348.281843	409833.192160	38.833191
2350.677557	410578.006474	38.838208
2353.544996	411325.357065	38.843226
2356.543395	412065.496421	38.848244
2359.543073	412788.871287	38.853261
2361.916777	413526.844001	38.858279
2364.575262	414248.740889	38.863296
2366.636996	414986.293713	38.868314
2368.837712	415720.434253	38.873332
2371.079931	416459.080950	38.878349
2373.102271	417210.051736	38.883367
2375.177925	417959.852273	38.888384
2377.609837	418704.557834	38.893402
2379.869356	419453.701981	38.898420
2382.983082	420210.913529	38.903437
2384.857986	420978.714511	38.908455
2387.225389	421725.494757	38.913472
2389.310176	422491.467818	38.918490
2391.409799	423268.910606	38.923508
2393.747008	424042.340044	38.928525
2395.906362	424831.599135	38.933543
2398.462958	425601.880000	38.938560
2400.691061	426396.850130	38.943578
2402.677916	427176.340343	38.948596
2405.513924	427961.488222	38.953613
2407.968577	428761.710640	38.958631
2410.402469	429549.556548	38.963648
2413.556671	430336.599649	38.968666
2416.890339	431118.575298	38.973684
2419.847090	431890.968866	38.978701
2422.283198	432660.132604	38.983719
2424.608339	433427.922744	38.988736
2427.068997	434192.071455	38.993754
2429.598922	434964.181159	38.998772
2431.555143	435734.284541	39.003789
2433.583963	436514.624818	39.008807
2435.882043	437299.196229	39.013824
2438.169632	438077.770511	39.018842
2440.568192	438866.421553	39.023860
2443.313426	439643.348541	39.028877
2445.373050	440438.984382	39.033895
2447.838584	441235.182997	39.038912
2450.554595	442017.953307	39.043930
2452.922357	442801.310134	39.048948
2455.879955	443578.571555	39.053965
2458.526996	444362.434283	39.058983
2461.321707	445133.748020	39.064000
2464.000292	445900.500441	39.069018
2466.443194	446643.284879	39.074036
2469.147923	447390.199623	39.079053
2471.405040	448128.006124	39.084071
2473.696041	448858.295154	39.089088
2475.629266	449580.575530	39.094106
2478.030185	450321.419121	39.099124
2480.465799	451063.293404	39.104141
2482.650736	451806.852151	39.109159
2484.823961	452565.711348	39.114176
2487.566275	453322.224077	39.119194
2490.226159	454082.111466	39.124212
2492.512891	454833.587349	39.129229
2494.846939	455611.223098	39.134247
2497.415352	456347.376409	39.139264
2500.233196	457117.189501	39.144282
2502.668115	457900.233952	39.149300
2505.505128	458649.811489	39.154317
2507.945117	459430.976191	39.159335
2510.667751	460200.183163	39.164352
2512.773364	460985.084348	39.169370
2515.284590	461758.665123	39.174388
2518.136476	462524.476013	39.179405
2520.784909	463303.535189	39.184423
2523.141886	464096.310421	39.189440
2525.707802	464877.141212	39.194458
2527.794657	465678.086048	39.199476
2530.167807	466479.507037	39.204493
2532.062072	467303.413840	39.209511
2534.404915	468112.353856	39.214528
2537.047122	468933.339370	39.219546
2539.013934	469776.888723	39.224564
2541.002805	470627.775065	39.229581
2543.444232	471493.252970	39.234599
2545.604464	472346.409584	39.239616
2548.039570	473222.976409	39.244634
2550.264804	474108.631227	39.249652
2552.651272	474994.167398	39.254669
2555.315906	475889.517334	39.259687
2557.638641	476777.253092	39.264704
2560.340467	477684.432292	39.269722
2562.793324	478596.507624	39.274740
2565.955859	479495.238570	39.279757
2568.846263	480396.243182	39.284775
2571.868478	481289.909429	39.289792
2575.139357	482181.218415	39.294810
2577.937520	483071.854634	39.299828
2581.433590	483950.213203	39.304845
2584.284208	484831.866863	39.309863
2586.593332	485698.621459	39.314880
2589.196905	486583.410499	39.319898
2592.000349	487471.757543	39.324916
2594.874639	488339.148686	39.329933
2597.035919	489220.042434	39.334951
2599.749875	490081.013832	39.339968
2602.637801	490957.258640	39.344986
2604.779241	491847.008167	39.350004
2607.495810	492714.612541	39.355021
2609.880102	493598.478691	39.360039
2612.056118	494488.238266	39.365056
2614.385165	495382.972761	39.370074
2616.438671	496280.531644	39.375092
2619.017836	497174.878784	39.380109
2621.274804	498090.775811	39.385127
2623.920967	499002.321202	39.390144
2626.701184	499915.308644	39.395162
2629.293364	500832.363527	39.400180
2632.395277	501732.688334	39.405197
2635.061886	502648.521386	39.410215
2638.167971	503545.720873	39.415232
2641.638143	504403.976792	39.420250
2644.249425	505269.591784	39.425268
2647.207967	506116.495333	39.430285
2649.737692	506977.091401	39.435303
2651.775779	507820.276215	39.440320
2654.286350	508661.372901	39.445338
2656.987683	509529.570292	39.450356
2659.725198	510387.329177	39.455373
2662.487047	511250.583730	39.460391
2665.431476	512103.326547	39.465408
2668.367486	512949.925737	39.470426
2670.840151	513810.871367	39.475444
2673.586357	514671.422677	39.480461
2676.054268	515543.766525	39.485479
2678.469121	516422.521557	39.490496
2681.141241	517296.699795	39.495514
2683.696819	518185.764177	39.500532
2686.859990	519058.200508	39.505549
2689.403717	519941.220459	39.510567
2691.932564	520823.335870	39.515584
2694.600354	521712.582163	39.520602
2697.014690	522611.742950	39.525620
2699.599234	523508.102579	39.530637
2702.552370	524408.428751	39.535655
2705.084015	525334.005368	39.540672
2707.678979	526233.828749	39.545690
2710.394338	527154.277311	39.550708
2713.159683	528085.035111	39.555725
2715.269403	529010.102505	39.560743
2717.202801	529961.324861	39.565760
2720.044829	530909.315575	39.570778
2722.541941	531875.225565	39.575796
2725.004702	532830.103221	39.580813
2728.231203	533794.105701	39.585831
2731.160478	534753.664073	39.590848
2734.405175	535729.062769	39.595866
2737.484302	536684.190840	39.600884
2740.422395	537637.417046	39.605901
2743.252598	538592.862539	39.610919
2745.672300	539579.711415	39.615936
2748.829295	540534.218916	39.620954
2751.072545	541505.013767	39.625972
2754.039831	542477.735962	39.630989
2757.281945	543461.715095	39.636007
2759.509382	544424.917483	39.641024
2762.450884	545404.082059	39.646042
2765.087901	546392.030012	39.651060
2767.636417	547378.665343	39.656077
2769.842078	548367.147849	39.661095
2773.198732	549370.556010	39.666112
2775.555898	550362.943959	39.671130
2777.886855	551379.095933	39.676148
2780.855264	552373.399773	39.681165
2783.532122	553397.288039	39.686183
2785.625874	554426.825138	39.691200
2788.689350	555449.690737	39.696218
2791.182369	556476.342259	39.701236
2794.077533	557509.935048	39.706253
2797.265667	558534.204081	39.711271
2800.021256	559558.767362	39.716288
2803.045878	560589.085848	39.721306
2805.661408	561630.896390	39.726324
2808.323090	562659.505962	39.731341
2811.631581	563695.664145	39.736359
2814.600841	564734.709570	39.741376
2817.415446	565756.371043	39.746394
2819.885275	566797.042187	39.751412
2822.330392	567820.209448	39.756429
2824.676980	568835.428927	39.761447
2827.621689	569850.971970	39.766464
2830.426315	570856.969455	39.771482
2833.481536	571849.644233	39.776500
2836.221036	572850.927394	39.781517
2839.434821	573867.713214	39.786535
2841.471279	574890.734315	39.791552
2844.399194	575903.990875	39.796570
2846.953386	576937.299063	39.801588
2849.728018	577960.751891	39.806605
2852.729784	579002.747007	39.811623
2855.283776	580048.441082	39.816640
2858.189735	581100.309522	39.821658
2861.276518	582146.541355	39.826676
2864.046238	583203.820617	39.831693
2867.020848	584254.455719	39.836711
2869.562694	585333.253470	39.841728
2873.659811	586383.520545	39.846746
2876.640170	587443.105982	39.851764
2879.646035	588499.285857	39.856781
2882.659440	589555.321984	39.861799
2885.460354	590619.971745	39.866816
2888.536195	591665.486740	39.871834
2891.696667	592729.739279	39.876852
2894.852792	593784.827589	39.881869
2898.521475	594830.117438	39.886887
2901.455352	595892.520409	39.891904
2904.477686	596941.637757	39.896922
2907.559015	597980.983999	39.901940
2910.572068	599030.617376	39.906957
2913.778316	600071.510289	39.911975
2916.688505	601126.781474	39.916992
2919.875738	602167.890314	39.922010
2922.693905	603224.337508	39.927028
2925.348022	604267.898310	39.932045
2928.618779	605313.315157	39.937063
2930.972018	606373.403975	39.942080
2933.785979	607418.953781	39.947098
2936.978710	608475.054985	39.952116
2939.549699	609537.815804	39.957133
2942.681490	610608.240066	39.962151
2945.608938	611678.546238	39.967168
2948.369118	612736.921448	39.972186
2951.414878	613809.255889	39.977204
2954.375343	614892.855326	39.982221
2957.316125	615962.648858	39.987239
2960.047300	617043.175400	39.992256
2963.167347	618117.581790	39.997274
2966.415882	619200.561854	40.002292
2969.324671	620283.940962	40.007309
2971.783293	621365.387398	40.012327
2974.472409	622450.187442	40.017344
2977.288847	623559.897378	40.022362
2980.591669	624660.968024	40.027380
2983.390451	625762.808925	40.032397
2987.115598	626854.941369	40.037415
2990.205636	627962.054620	40.042432
2993.495767	629045.592443	40.047450
2996.914576	630129.848010	40.052468
3000.067623	631207.793885	40.057485
3003.576340	632269.990919	40.062503
3006.760320	633366.937526	40.067520
3010.223894	634410.301503	40.072538
3013.385461	635476.475949	40.077556
3016.205481	636537.356689	40.082573
3019.777244	637594.611611	40.087591
3023.048854	638636.037793	40.092608
3025.619845	639659.060856	40.097626
3028.931135	640666.192903	40.102644
3031.816004	641670.502798	40.107661
3034.706387	642664.287102	40.112679
3037.540177	643665.317133	40.117696
3040.054372	644664.805422	40.122714
3042.858071	645666.392263	40.127732
3045.642205	646678.754844	40.132749
3049.144744	647677.434850	40.137767
3052.040145	648688.032268	40.142784
3055.397442	649692.918496	40.147802
3058.831897	650708.259291	40.152820
3061.263613	651721.519131	40.157837
3064.254298	652745.548464	40.162855
3066.831185	653775.022315	40.167872
3069.674071	654817.001862	40.172890
3072.790080	655863.958484	40.177908
3075.723108	656895.839314	40.182925
3078.785854	657957.577347	40.187943
3081.079201	659036.161867	40.192960
3083.642854	660110.051167	40.197978
3086.540008	661206.722985	40.202996
3089.140899	662324.878895	40.208013
3091.924635	663432.122537	40.213031
3094.921868	664568.921721	40.218048
3097.858554	665701.913737	40.223066
3100.661807	666854.302537	40.228084
3103.147004	668012.675912	40.233101
3106.395728	669192.824059	40.238119
3108.874002	670379.221114	40.243136
3112.276441	671560.990144	40.248154
3115.702559	672755.986461	40.253172
3118.508401	673964.260918	40.258189
3122.091192	675149.628371	40.263207
3126.159082	676344.758930	40.268224
3129.781980	677529.669084	40.273242
3133.503224	678711.181537	40.278260
3136.265655	679913.027747	40.283277
3139.240234	681106.682754	40.288295
3142.324871	682310.946692	40.293312
3145.461059	683513.603804	40.298330
3148.190234	684724.415636	40.303348
3151.334684	685954.516810	40.308365
3155.085803	687160.317557	40.313383
3158.227601	688364.370429	40.318400
3161.234090	689575.682515	40.323418
3164.438684	690785.062059	40.328436
3167.488707	692026.018843	40.333453
3170.503600	693248.299844	40.338471
3174.003881	694481.398477	40.343488
3177.314302	695700.764435	40.348506
3180.791546	696931.741253	40.353524
3183.910326	698152.835416	40.358541
3186.771660	699378.365393	40.363559
3190.364264	700597.009685	40.368576
3193.750897	701827.763967	40.373594
3197.585917	703031.602883	40.378612
3201.131982	704255.346425	40.383629
3204.648977	705439.079793	40.388647
3208.364187	706651.654422	40.393664
3212.584623	707832.070662	40.398682
3216.340933	708990.655616	40.403700
3220.211212	710155.355630	40.408717
3224.264059	711278.714420	40.413735
3228.100908	712404.189200	40.418752
3231.337355	713529.069542	40.423770
3235.313061	714631.551489	40.428788
3238.386038	715741.017567	40.433805
3241.246125	716823.945530	40.438823
3244.359455	717888.878547	40.443840
3247.027504	718942.963910	40.448858
3249.670184	719993.705264	40.453876
3252.431302	721066.801484	40.458893
3255.643361	722125.045628	40.463911
3258.245384	723183.947911	40.468928
3261.183604	724267.975815	40.473946
3263.880625	725357.586893	40.478964
3266.603538	726440.030383	40.483981
3269.370527	727573.776622	40.488999
3272.014259	728701.555102	40.494016
3274.501221	729838.098190	40.499034
3277.584511	730987.921804	40.504052
3279.880219	732171.599780	40.509069
3283.904252	733338.768416	40.514087
3287.228007	734529.588184	40.519104
3290.231468	735727.790172	40.524122
3293.516717	736928.828191	40.529140
3296.583707	738146.258445	40.534157
3299.659732	739362.613588	40.539175
3303.078792	740606.409979	40.544192
3305.712021	741839.681566	40.549210
3308.795276	743085.365259	40.554228
3311.792296	744362.630824	40.559245
3314.872775	745622.168963	40.564263
3318.182535	746927.322813	40.569280
3321.031375	748250.378410	40.574298
3323.899746	749549.793973	40.579316
3326.967628	750884.738436	40.584333
3329.905164	752222.135598	40.589351
3333.092551	753575.961207	40.594368
3336.365119	754952.833215	40.599386
3339.853054	756319.672359	40.604404
3343.186294	757687.868901	40.609421
3346.839374	759068.813557	40.614439
3350.512869	760450.488898	40.619456
3353.862783	761834.131420	40.624474
3357.647123	763212.676827	40.629492
3361.213777	764607.141603	40.634509
3364.801426	765984.080733	40.639527
3368.655755	767371.246520	40.644544
3372.034911	768748.842386	40.649562
3375.812581	770133.442260	40.654580
3379.933430	771512.616084	40.659597
3383.544668	772872.157996	40.664615
3387.714158	774227.378003	40.669632
3391.663874	775570.300882	40.674650
3396.027084	776904.953674	40.679668
3399.473867	778242.754592	40.684685
3402.830569	779578.950273	40.689703
3406.380710	780901.272023	40.694720
3409.182699	782228.137967	40.699738
3412.692962	783556.410059	40.704756
3416.087617	784877.882586	40.709773
3419.502772	786208.722200	40.714791
3422.930725	787516.901332	40.719808
3426.085777	788851.068141	40.724826
3429.088875	790183.588406	40.729844
3432.404613	791521.492510	40.734861
3435.586786	792862.056922	40.739879
3438.931885	794202.045929	40.744896
3441.778020	795554.989710	40.749914
3445.028657	796915.197068	40.754932
3447.692349	798298.788763	40.759949
3450.517169	799663.231736	40.764967
3454.333026	801055.436393	40.769984
3456.843092	802462.991219	40.775002
3460.531625	803852.635679	40.780007
3463.599007	805187.702371	40.785012
3466.716470	806482.687518	40.790016
3470.129569	807713.061072	40.795021
3473.507789	808880.088014	40.800026
3476.810441	809976.161922	40.805031
3479.664315	811005.102050	40.810036
3482.469059	811971.869968	40.815040
3485.670751	812868.972624	40.820045
3488.418491	813686.193847	40.825050
3491.205593	814428.868440	40.830055
3493.618440	815110.996440	40.835060
3495.447363	815716.668030	40.840064
3498.043828	816278.925959	40.845069
3499.699197	816784.256475	40.850074
3501.969782	817224.730277	40.855079
3503.266255	817620.447239	40.860084
3504.972946	817949.356079	40.865088
3506.394426	818245.011942	40.870093
3507.501756	818499.103368	40.875098
3508.803190	818703.231006	40.880103
3510.214109	818877.724406	40.885108
3510.887672	818998.695248	40.890112
3512.149690	819100.920649	40.895117
3513.054001	819175.405541	40.900122
3513.684606	819195.905318	40.905127
3514.667738	819211.599815	40.910132
3515.036374	819176.302345	40.915136
3515.928570	819129.662189	40.920141
3516.240383	819070.294839	40.925146
3517.095277	818976.529647	40.930151
3517.423611	818877.466235	40.935156
3517.642084	818760.702098	40.940160
3518.252082	818626.985772	40.945165
3518.337369	818469.516948	40.950170
3518.987783	818296.729011	40.955175
3518.993243	818114.840670	40.960180
3519.313552	817931.133355	40.965184
3519.624555	817726.324854	40.970189
3519.416313	817512.294707	40.975194
3519.358537	817287.365195	40.980199
3519.798645	817065.234492	40.985204
3519.946997	816831.443739	40.990208
3519.984809	816588.801483	40.995213
3519.913363	816349.057126	41.000218
3520.058047	816087.578221	41.005223
3520.137342	815827.715733	41.010228
3520.101293	815568.890485	41.015232
3520.515930	815296.367855	41.020237
3520.379209	815034.600522	41.025242
3520.114791	814747.280532	41.030247
3520.283297	814469.916719	41.035252
3519.976984	814193.599224	41.040256
3520.140035	813919.935878	41.045261
3519.641678	813645.488726	41.050266
3519.754097	813347.173338	41.055271
3519.726855	813065.228635	41.060276
3519.597510	812794.898796	41.065280
3519.763066	812518.092084	41.070285
3519.552467	812222.572615	41.075290
3519.364286	811926.007703	41.080295
3519.348008	811655.809708	41.085300
3519.244968	811365.183581	41.090304
3519.177139	811070.423288	41.095309
3518.925779	810784.843620	41.100314
3519.286536	810506.599584	41.105319
3518.860491	810211.910029	41.110324
3518.706008	809936.324790	41.115328
3518.388779	809640.710426	41.120333
3518.494970	809362.265472	41.125338
3518.353586	809089.976575	41.130343
3518.510802	808797.776432	41.135348
3518.267059	808538.471420	41.140352
3518.266172	808235.832578	41.145357
3518.254059	807978.232828	41.150362
3518.107889	807678.975707	41.155367
3518.024708	807392.490758	41.160372
3517.438526	807122.402792	41.165376
3517.636766	806832.906417	41.170381
3517.531192	806563.403645	41.175386
3517.123529	806289.772200	41.180391
3517.432672	806022.582489	41.185396
3517.152284	805751.017099	41.190400
3517.304950	805479.075401	41.195405
3516.814278	805209.975202	41.200410
3516.817244	804933.770009	41.205415
3516.586078	804667.156050	41.210420
3516.245356	804408.789663	41.215424
3516.289798	804153.832584	41.220429
3516.172050	803887.464039	41.225434
3515.915614	803625.571805	41.230439
3515.804868	803389.987673	41.235444
3515.384676	803137.963742	41.240448
3515.549801	802875.826445	41.245453
3515.324633	802640.873346	41.250458
3515.601125	802386.646756	41.255463
3515.563336	802138.301077	41.260468
3515.352724	801891.397824	41.265472
3515.136764	801634.673362	41.270477
3514.843055	801398.953376	41.275482
3515.011941	801160.450336	41.280487
3514.717900	800915.783262	41.285492
3514.268252	800679.721005	41.290496
3514.436849	800438.396018	41.295501
3514.060227	800224.340846	41.300506
3514.242087	799982.801544	41.305511
3514.653056	799756.872565	41.310516
3514.062950	799528.303506	41.315520
3513.824469	799306.687876	41.320525
3513.854999	799076.725600	41.325530
3513.686513	798849.439165	41.330535
3513.752017	798633.298767	41.335540
3513.611348	798405.256952	41.340544
3513.707953	798183.059500	41.345549
3513.091635	797969.121732	41.350554
3513.143312	797749.814335	41.355559
3513.297732	797543.984354	41.360564
3512.923446	797321.837064	41.365568
3512.937206	797111.746097	41.370573
3512.562164	796905.739046	41.375578
3512.440406	796683.922696	41.380583
3512.628974	796497.402201	41.385588
3512.448650	796289.037104	41.390592
3512.496892	796075.914028	41.395597
3512.330009	795875.538634	41.400602
3512.000898	795677.836089	41.405607
3512.023718	795477.810955	41.410612
3511.957100	795296.948192	41.415616
3511.896663	795093.684500	41.420621
3511.606736	794905.383337	41.425626
3511.385543	794713.971554	41.430631
3511.450391	794518.381661	41.435636
3510.974236	794340.115789	41.440640
3511.587402	794144.474308	41.445645
3511.027532	793975.398252	41.450650
3510.999833	793785.108219	41.455655
3510.728617	793599.421590	41.460660
3510.718861	793430.831325	41.465664
3510.906796	793254.393549	41.470669
3510.609787	793085.301963	41.475674
3510.590396	792908.496677	41.480679
3510.483026	792728.115042	41.485684
3510.259406	792558.310938	41.490688
3510.374321	792378.768112	41.495693
3510.431776	792226.646154	41.500698
3510.266035	792049.646954	41.505703
3510.098079	791892.297627	41.510708
3509.777004	791719.590478	41.515712
3510.324826	791555.482405	41.520717
3509.966049	791388.080185	41.525722
3509.686545	791214.960773	41.530727
3509.700297	791065.179749	41.535732
3509.565055	790913.994998	41.540736
3509.397234	790741.779322	41.545741
3509.453598	790610.213609	41.550746
3509.249650	790436.030715	41.555751
3509.426095	790289.056910	41.560756
3509.085650	790145.703781	41.565760
3508.819496	789990.490872	41.570765
3508.659793	789838.894066	41.575770
3508.466850	789707.352692	41.580775
3508.928262	789567.591214	41.585780
3508.417109	789419.729673	41.590784
3508.608121	789278.385041	41.595789
3508.339240	789146.698349	41.600794
3508.223828	789010.609172	41.605799
3508.477027	788880.306200	41.610804
3508.156222	788748.915637	41.615808
3508.491325	788607.927221	41.620813
3508.046683	788482.156088	41.625818
3508.486887	788351.714338	41.630823
3508.198298	788209.640957	41.635828
3507.797642	788089.902367	41.640832
3508.230272	787960.831230	41.645837
3507.957967	787829.120756	41.650842
3507.929402	787687.731597	41.655847
3507.497782	787569.611782	41.660852
3507.564526	787442.361473	41.665856
3508.018169	787315.831834	41.670861
3507.677937	787196.609138	41.675866
3507.542401	787070.319704	41.680871
3507.797761	786942.931104	41.685876
3507.542831	786819.607046	41.690880
3507.404808	786695.130680	41.695885
3507.334918	786583.277997	41.700890
3507.283039	786459.127538	41.705895
3506.979240	786341.900658	41.710900
3507.193760	786227.831960	41.715904
3507.254306	786116.491415	41.720909
3506.844878	786013.635541	41.725914
3507.250202	785894.809283	41.730919
3507.000007	785782.236151	41.735924
3506.693316	785683.243589	41.740928
3507.010459	785561.475680	41.745933
3506.854289	785455.373482	41.750938
3506.584072	785337.780395	41.755943
3506.751785	785234.178937	41.760948
3506.637231	785138.835767	41.765952
3506.695405	785023.593329	41.770957
3506.623323	784926.469788	41.775962
3506.604418	784818.515807	41.780967
3506.762826	784703.104171	41.785972
3506.328128	784613.610511	41.790976
3506.503313	784499.176538	41.795981
3506.381203	784393.938396	41.800986
3506.267790	784303.059916	41.805991
3506.543833	784193.375611	41.810996
3506.395335	784095.368052	41.816000
3506.517058	783986.493031	41.821005
3506.246950	783896.274685	41.826010
3506.352418	783791.334577	41.831015
3506.468730	783678.274592	41.836020
3506.191164	783595.284825	41.841024
3506.223005	783489.958921	41.846029
3505.918271	783391.918333	41.851034
3506.095340	783287.500224	41.856039
3505.677240	783203.987964	41.861044
3505.470477	783121.915780	41.866048
3505.789362	783021.455265	41.871053
3505.482938	782937.872332	41.876058
3505.568986	782856.978813	41.881063
3505.797633	782775.273741	41.886068
3505.378550	782688.853026	41.891072
3505.213736	782607.260060	41.896077
3505.613554	782517.947291	41.901082
3505.316809	782425.402565	41.906087
3505.182388	782347.294845	41.911092
3504.992402	782272.393493	41.916096
3505.268672	782184.031768	41.921101
3504.983659	782125.528628	41.926106
3505.012159	782030.317568	41.931111
3504.845092	781946.109772	41.936116
3504.937583	781884.295092	41.941120
3505.044240	781794.824872	41.946125
3504.882187	781723.062293	41.951130
3504.837730	781654.477966	41.956135
3504.701091	781563.273573	41.961140
3504.713281	781490.003812	41.966144
3504.666385	781416.152560	41.971149
3504.723361	781362.852038	41.976154
3504.866022	781287.590455	41.981159
3504.725390	781214.982782	41.986164
3504.505804	781154.787939	41.991168
3504.251552	781078.359348	41.996173
3504.250617	781023.835645	42.001178
3504.479472	780946.046639	42.006183
3504.536415	780878.619302	42.011188
3504.300733	780820.491169	42.016192
3504.452486	780747.584600	42.021197
3504.429007	780681.595805	42.026202
3504.260487	780610.020112	42.031207
3504.479581	780551.421215	42.036212
3504.307876	780480.435320	42.041216
3503.996029	780419.905079	42.046221
3504.073087	780369.251475	42.051226
3504.368411	780306.602512	42.056231
3503.996652	780247.557129	42.061236
3503.984960	780187.172366	42.066240
3504.046123	780129.481951	42.071245
3504.175317	780065.824752	42.076250
3503.764464	779997.580398	42.081255
3504.092630	779936.005592	42.086260
3503.824988	779892.738737	42.091264
3504.202661	779826.380792	42.096269
3503.900302	779768.747391	42.101274
3504.032229	779717.243500	42.106279
3504.177538	779643.834734	42.111284
3503.599692	779601.798490	42.116288
3504.065368	779548.909521	42.121293
3503.706836	779484.490840	42.126298
3503.804556	779434.467176	42.131303
3503.784164	779382.050819	42.136308
3503.626804	779327.786252	42.141312
3504.032702	779265.749984	42.146317
3503.520049	779216.022242	42.151322
3503.622121	779157.775942	42.156327
3503.500543	779101.436468	42.161332
3503.493406	779062.502554	42.166336
3503.589713	779013.805245	42.171341
3503.688515	778958.068260	42.176346
3503.829490	778901.979336	42.181351
3503.583145	778845.510761	42.186356
3503.643724	778797.014785	42.191360
3503.663937	778746.457693	42.196365
3503.523272	778687.755371	42.201370
3503.401088	778651.397920	42.206375
3503.776445	778600.928998	42.211380
3503.341481	778546.408978	42.216384
3503.417683	778492.001257	42.221389
3503.169234	778444.587595	42.226394
3503.076284	778401.086184	42.231399
3503.487860	778353.907806	42.236404
3503.279345	778313.280098	42.241408
3503.103455	778262.653497	42.246413
3503.189895	778231.674675	42.251418
3503.186275	778191.160222	42.256423
3503.572587	778137.289520	42.261428
3503.196556	778088.959209	42.266432
3503.097242	778066.182332	42.271437
3503.022799	778014.355792	42.276442
3502.901282	777967.213496	42.281447
3502.939430	777923.047648	42.286452
3502.723377	777882.763395	42.291456
3503.108688	777845.235258	42.296461
3503.200449	777806.032191	42.301466
3503.043998	777763.915912	42.306471
3503.245663	777716.078752	42.311476
3502.846348	777677.448200	42.316480
3502.956261	777625.243907	42.321485
3503.201459	777593.891603	42.326490
3503.093510	777552.750769	42.331495
3502.978238	777504.619800	42.336500
3502.816646	777476.484921	42.341504
3502.732898	777432.730054	42.346509
3502.802888	777403.375140	42.351514
3502.880943	777367.667583	42.356519
3503.038088	777325.694058	42.361524
3502.495619	777293.288582	42.366528
3502.675846	777264.407299	42.371533
3502.654819	777216.702022	42.376538
3502.518015	777182.456769	42.381543
3502.880231	777152.708068	42.386548
3502.725550	777112.310984	42.391552
3503.007425	777067.262810	42.396557
3502.910115	777032.813407	42.401562
3502.570833	776990.722785	42.406567
3503.110678	776956.611203	42.411572
3502.515293	776929.431933	42.416576
3502.584117	776890.276971	42.421581
3502.252842	776854.141957	42.426586
3502.406997	776830.383961	42.431591
3503.001907	776803.106636	42.436596
3502.822134	776767.487856	42.441600
3502.676686	776733.143447	42.446605
3502.656302	776704.342237	42.451610
3502.905283	776662.694454	42.456615
3502.723595	776636.332249	42.461620
3502.537250	776596.823836	42.466624
3502.912876	776558.650591	42.471629
3502.666022	776535.056170	42.476634
3502.577734	776496.712817	42.481639
3502.431714	776460.791544	42.486644
3502.137218	776423.515819	42.491648
3502.440903	776396.580396	42.496653
3502.271367	776357.511088	42.501658
3502.364532	776333.613806	42.506663
3502.448546	776309.570229	42.511668
3502.572472	776271.978605	42.516672
3502.756108	776243.634393	42.521677
3502.675808	776217.303220	42.526682
3502.865913	776181.275969	42.531687
3502.915217	776153.445956	42.536692
3502.648419	776115.425465	42.541696
3502.881896	776075.598875	42.546701
3502.428646	776029.729799	42.551706
3502.590331	776003.850431	42.556711
3502.628944	775967.453137	42.561716
3502.460962	775949.654570	42.566720
3502.822771	775913.351503	42.571725
3502.454785	775874.509282	42.576730
3502.358491	775844.387603	42.581735
3502.221339	775818.655294	42.586740
3502.214048	775785.170083	42.591744
3502.246032	775751.973720	42.596749
3502.367225	775736.933967	42.601754
3502.102733	775696.399421	42.606759
3502.421321	775679.307977	42.611764
3502.154704	775659.752115	42.616768
3502.467134	775626.410499	42.621773
3502.206153	775595.871713	42.626778
3502.094165	775568.509262	42.631783
3502.400677	775548.858701	42.636788
3502.247416	775520.813422	42.641792
3502.556134	775483.482800	42.646797
3502.293192	775449.397958	42.651802
3501.824677	775431.549140	42.656807
3502.550132	775397.104263	42.661812
3502.110720	775377.034387	42.666816
3501.951200	775355.539420	42.671821
3502.074883	775343.896538	42.676826
3502.018114	775314.012410	42.681831
3502.471392	775291.135871	42.686836
3501.980520	775275.063284	42.691840
3502.446859	775233.864073	42.696845
3502.183365	775213.814022	42.701850
3501.985140	775203.061166	42.706855
3502.065961	775174.729764	42.711860
3502.300968	775154.252697	42.716864
3502.557298	775119.391304	42.721869
3502.041426	775089.384886	42.726874
3502.026985	775066.732439	42.731879
3502.330977	775041.121737	42.736884
3501.695652	775024.284397	42.741888
3502.208233	774996.767688	42.746893
3502.143710	774977.816969	42.751898
3501.866652	774947.524382	42.756903
3501.992098	774929.625755	42.761908
3501.723468	774913.121762	42.766912
3501.610335	774883.097412	42.771917
3501.733975	774867.119711	42.776922
3501.912780	774861.081587	42.781927
3502.195720	774827.938213	42.786932
3501.979708	774819.207022	42.791937
3502.015402	774790.980077	42.796941
3501.962090	774773.455274	42.801946
3501.843939	774736.043416	42.806951
3502.165836	774723.874387	42.811956
3501.922264	774692.540943	42.816961
3501.887351	774682.006684	42.821965
3502.048862	774654.595777	42.826970
3501.893588	774631.718926	42.831975
3502.272641	774616.535903	42.836980
3502.064241	774588.939420	42.841985
3501.963792	774564.624998	42.846989
3502.021995	774538.954531	42.851994
3501.618568	774521.880822	42.856999
3501.683986	774490.003087	42.862004
3501.910483	774478.834437	42.867009
3502.153284	774463.328768	42.872013
3502.248797	774443.857775	42.877018
3502.122322	774434.372570	42.882023
3502.430843	774402.552922	42.887028
3501.965613	774384.454739	42.892033
3502.218873	774350.821566	42.897037
3502.395665	774330.401052	42.902042
3501.989444	774306.480924	42.907047
3502.382013	774279.129072	42.912052
3501.873558	774254.831576	42.917057
3502.254641	774216.694529	42.922061
3502.063261	774215.937910	42.927066
3501.999948	774198.413384	42.932071
3502.018216	774175.408017	42.937076
3501.940132	774143.601674	42.942081
3501.914869	774126.267733	42.947085
3502.545693	774111.042201	42.952090
3502.062753	774075.460284	42.957095
3502.262950	774052.326054	42.962100
3501.712031	774033.551530	42.967105
3502.092428	773992.704331	42.972109
3501.876127	773973.332712	42.977114
3501.974043	773954.943683	42.982119
3501.971898	773928.000343	42.987124
3501.913377	773913.479038	42.992129
3501.817135	773891.427534	42.997133
3502.387518	773865.128522	43.002138
3501.593298	773847.575780	43.007143
3502.065795	773835.331224	43.012148
3501.878682	773824.525260	43.017153
3501.927067	773777.722094	43.022157
3501.899350	773773.391878	43.027162
3501.735793	773762.089359	43.032167
3501.913240	773735.460542	43.037172
3501.502678	773722.031274	43.042177
3501.849986	773697.590976	43.047181
3501.723093	773686.134526	43.052186
3501.749003	773666.377391	43.057191
3501.903205	773655.416439	43.062196
3501.533146	773639.763693	43.067201
3501.916061	773601.130572	43.072205
3501.832494	773609.567627	43.077210
3501.759545	773587.905451	43.082215
3501.873515	773553.503434	43.087220
3501.515366	773562.330588	43.092225
3501.612611	773521.822980	43.097229
3501.538859	773514.249040	43.102234
3501.637249	773510.784577	43.107239
3501.688018	773485.949084	43.112244
3501.879525	773465.228191	43.117249
3501.624505	773446.354165	43.122253
3501.854226	773433.557811	43.127258
3501.915672	773421.872884	43.132263
3502.102500	773392.926039	43.137268
3501.997999	773377.031948	43.142273
3501.609245	773355.815196	43.147277
3501.455603	773332.096597	43.152282
3501.647110	773319.848213	43.157287
3501.463914	773323.474400	43.162292
3501.717014	773287.964481	43.167297
3501.779696	773278.643674	43.172301
3501.793085	773271.991100	43.177306
3501.986266	773243.683024	43.182311
3501.910819	773220.591589	43.187316
3501.925732	773210.490374	43.192321
3502.050099	773185.099865	43.197325
3502.326565	773169.585935	43.202330
3501.648805	773146.987579	43.207335
3502.071537	773124.601984	43.212340
3501.569693	773106.260368	43.217345
3501.839947	773093.801588	43.222349
3501.765707	773068.394128	43.227354
3501.500718	773055.826395	43.232359
3501.826803	773032.421918	43.237364
3501.520179	773016.461816	43.242369
3501.595477	772988.024388	43.247373
3501.720891	772987.116929	43.252378
3501.829599	772970.300100	43.257383
3502.165459	772934.528532	43.262388
3501.956770	772930.671004	43.267393
3501.869846	772910.142209	43.272397
3502.222834	772885.895349	43.277402
3501.976881	772866.969080	43.282407
3502.306559	772835.188456	43.287412
3501.944293	772816.527539	43.292417
3501.786490	772796.995395	43.297421
3502.102515	772776.449120	43.302426
3501.633757	772763.865188	43.307431
3501.947178	772743.516311	43.312436
3501.661393	772736.715473	43.317441
3501.521987	772718.313189	43.322445
3501.944833	772682.230482	43.327450
3501.766905	772661.420391	43.332455
3501.880409	772650.858780	43.337460
3501.716109	772638.076686	43.342465
3501.433662	772618.071942	43.347469
3501.772738	772617.671170	43.352474
3501.559457	772593.073231	43.357479
3501.863949	772579.573359	43.362484
3501.454280	772562.348325	43.367489
3501.916621	772536.160922	43.372493
3501.890706	772528.775155	43.377498
3501.530447	772513.266197	43.382503
3501.853815	772493.161326	43.387508
3501.883463	772483.056689	43.392513
3501.647537	772457.575225	43.397517
3501.699004	772433.475084	43.402522
3501.392760	772433.722537	43.407527
3501.638468	772397.027143	43.412532
3501.433585	772387.404413	43.417537
3501.519509	772384.089280	43.422541
3501.513522	772364.432450	43.427546
3501.638840	772350.961675	43.432551
3501.736868	772340.549974	43.437556
3501.744139	772325.571295	43.442561
3501.988376	772298.926300	43.447565
3501.542831	772294.023553	43.452570
3501.476443	772272.849118	43.457575
3501.791480	772254.124481	43.462580
3501.871541	772257.412215	43.467585
3501.697698	772237.092938	43.472589
3502.107956	772212.588099	43.477594
3501.745965	772205.405172	43.482599
3501.967055	772177.334760	43.487604
3501.531208	772181.200195	43.492609
3501.714399	772155.155964	43.497613
3501.770367	772134.010246	43.502618
3501.755694	772120.020149	43.507623
3501.625473	772095.357601	43.512628
3501.532976	772077.734304	43.517633
3501.925413	772073.875850	43.522637
3501.824478	772049.159054	43.527642
3501.875268	772037.325886	43.532647
3501.941984	772019.774766	43.537652
3501.580054	771994.903700	43.542657
3501.452013	771983.395521	43.547661
3501.922347	771973.119060	43.552666
3501.601557	771953.857883	43.557671
3501.569818	771947.802795	43.562676
3501.503337	771930.027050	43.567681
3501.463706	771915.400160	43.572685
3501.551813	771897.697416	43.577690
3501.528039	771898.637417	43.582695
3501.698883	771864.415252	43.587700
3501.545948	771854.290559	43.592705
3501.921055	771849.153797	43.597709
3501.915560	771824.026361	43.602714
3501.600456	771819.939420	43.607719
3501.905628	771793.676741	43.612724
3501.558323	771769.295221	43.617729
3501.693819	771765.331115	43.622733
3501.951200	771742.722227	43.627738
3501.827535	771723.280164	43.632743
3501.975920	771702.068718	43.637748
3501.642481	771679.162776	43.642753
3501.527420	771669.819948	43.647757
3501.992790	771660.874224	43.652762
3501.367868	771639.691431	43.657767
3501.445950	771618.442053	43.662772
3501.482891	771622.377716	43.667777
3501.497242	771588.524961	43.672781
3501.553904	771580.829009	43.677786
3501.685918	771570.410628	43.682791
3501.662361	771554.400735	43.687796
3501.564272	771543.133303	43.692801
3501.392211	771523.698687	43.697805
3501.544531	771523.082260	43.702810
3501.357329	771503.452992	43.707815
3501.522936	771473.418118	43.712820
3501.405506	771483.144286	43.717825
3501.443955	771478.604732	43.722829
3501.412584	771455.697616	43.727834
3501.422817	771454.316208	43.732839
3501.497364	771440.704320	43.737844
3501.771858	771437.948990	43.742849
3501.504207	771412.961887	43.747853
3501.479051	771392.369427	43.752858
3501.268248	771402.308179	43.757863
3501.648696	771375.391057	43.762868
3501.487308	771355.264402	43.767873
3501.741150	771342.903935	43.772877
3501.641405	771353.859220	43.777882
3501.597916	771332.530499	43.782887
3501.638383	771296.257656	43.787892
3501.478833	771302.837415	43.792897
3501.560029	771290.554573	43.797901
3501.451795	771267.610261	43.802906
3501.307448	771268.915127	43.807911
3501.323769	771265.315310	43.812916
3501.486866	771244.297231	43.817921
3501.292791	771218.952428	43.822925
3501.442210	771215.724866	43.827930
3501.136826	771212.227288	43.832935
3501.567697	771204.715684	43.837940
3501.135410	771190.644792	43.842945
3501.330233	771169.621276	43.847949
3501.120102	771170.394963	43.852954
3501.262740	771170.272858	43.857959
3501.715727	771147.827040	43.862964
3501.598531	771139.765062	43.867969
3501.295678	771125.426347	43.872973
3501.192392	771124.802715	43.877978
3501.492084	771121.993843	43.882983
3501.642252	771093.191870	43.887988
3501.147178	771091.647246	43.892993
3501.825690	771079.265667	43.897997
3501.876142	771064.523706	43.903002
3501.156492	771050.007116	43.908007
3501.376433	771021.883243	43.913012
3501.794344	771022.602772	43.918017
3501.683774	771012.322119	43.923021
3501.541939	770986.031658	43.928026
3501.197407	770986.778225	43.933031
3501.267092	770963.261619	43.938036
3501.311988	770941.621553	43.943041
3501.539527	770936.853412	43.948045
3501.845807	770924.877830	43.953050
3501.366359	770923.281319	43.958055
3501.174609	770885.615678	43.963060
3501.340271	770887.756540	43.968065
3501.575274	770891.068639	43.973069
3501.555098	770882.645458	43.978074
3501.605659	770861.546277	43.983079
3501.473736	770838.161038	43.988084
3501.157702	770845.259755	43.993089
3501.449574	770832.793621	43.998093
3501.496544	770817.460408	44.003098
3501.442701	770807.909295	44.008103
3501.510576	770791.044967	44.013108
3501.598947	770786.792435	44.018113
3501.378609	770771.749549	44.023117
3501.162221	770741.922469	44.028122
3501.368423	770747.161235	44.033127
3501.596697	770751.706465	44.038132
3501.432223	770735.767293	44.043137
3501.316098	770726.571284	44.048141
3501.354657	770713.555332	44.053146
3501.421473	770717.683670	44.058151
3501.395885	770693.836954	44.063156
3501.265277	770684.101211	44.068161
3500.860571	770671.256756	44.073165
3501.584577	770668.476381	44.078170
3501.391843	770669.937157	44.083175
3501.844498	770663.308442	44.088180
3501.494519	770644.935683	44.093185
3501.679726	770626.425446	44.098189
3501.809254	770614.232082	44.103194
3501.507406	770597.231096	44.108199
3501.579969	770578.640735	44.113204
3501.598323	770577.011429	44.118209
3501.247598	770547.550652	44.123213
3501.589862	770539.708018	44.128218
3501.298753	770541.628541	44.133223
3501.501903	770530.309948	44.138228
3501.569754	770504.032520	44.143233
3501.565089	770501.273549	44.148237
3501.632862	770491.406317	44.153242
3501.666386	770478.686463	44.158247
3501.567280	770450.711541	44.163252
3501.414916	770446.892710	44.168257
3501.893967	770423.405527	44.173261
3501.992012	770402.050816	44.178266
3501.569416	770401.972524	44.183271
3501.494577	770353.196761	44.188276
3501.371238	770349.718067	44.193281
3501.177042	770343.294178	44.198285
3501.695486	770339.956172	44.203290
3501.421990	770316.494046	44.208295
3501.447714	770294.411719	44.213300
3501.673401	770294.078798	44.218305
3501.608723	770287.584246	44.223309
3501.646791	770253.967901	44.228314
3501.582976	770273.050332	44.233319
3501.224945	770246.349326	44.238324
3501.242081	770231.414071	44.243329
3501.412534	770218.474091	44.248333
3501.645010	770205.573154	44.253338
3501.860598	770205.389738	44.258343
3501.806537	770184.601559	44.263348
3501.487404	770178.148824	44.268353
3501.492540	770166.566602	44.273357
3501.463114	770140.550322	44.278362
3501.055170	770130.169580	44.283367
3501.408402	770118.579229	44.288372
3501.203342	770126.498152	44.293377
3501.410866	770117.839467	44.298381
3501.367735	770094.338693	44.303386
3501.177031	770088.653249	44.308391
3501.521302	770083.471075	44.313396
3501.578143	770082.673129	44.318401
3501.809360	770052.128872	44.323405
3501.499934	770036.507771	44.328410
3501.462963	770025.671511	44.333415
3501.442211	770014.536865	44.338420
3501.457955	769994.377338	44.343425
3501.324828	769995.138458	44.348429
3501.526533	769984.706375	44.353434
3501.272906	769972.525789	44.358439
3501.576360	769952.121622	44.363444
3501.388818	769940.176515	44.368449
3501.282595	769935.856982	44.373453
3501.507820	769937.199771	44.378458
3501.419560	769918.535681	44.383463
3501.461910	769892.605279	44.388468
3501.679647	769894.540717	44.393473
3501.698917	769872.951042	44.398477
3501.613152	769862.073298	44.403482
3501.099989	769846.879629	44.408487
3501.315382	769842.753489	44.413492
3501.408973	769821.792121	44.418497
3501.201752	769813.595674	44.423501
3501.295550	769794.112731	44.428506
3501.018532	769809.880107	44.433511
3501.493526	769792.700032	44.438516
3501.472866	769792.506237	44.443521
3501.280290	769753.159304	44.448525
3501.626725	769747.631547	44.453530
3501.085727	769748.706299	44.458535
3501.417956	769748.897942	44.463540
3501.448424	769738.690861	44.468545
3501.610784	769721.069266	44.473549
3501.759464	769701.527756	44.478554
3501.307488	769697.412891	44.483559
3501.432169	769666.983173	44.488564
3501.565712	769668.094685	44.493569
3501.390859	769678.473384	44.498573
3501.825867	769655.730320	44.503578
3501.164230	769639.673540	44.508583
3501.368695	769629.782650	44.513588
3501.503898	769626.261029	44.518593
3501.483147	769609.260761	44.523597
3501.458974	769584.572390	44.528602
3501.587165	769577.010439	44.533607
3501.350886	769572.761404	44.538612
3501.410309	769548.009856	44.543617
3501.012598	769538.908042	44.548621
3501.448529	769524.050243	44.553626
3501.308293	769523.038267	44.558631
3501.340502	769518.991409	44.563636
3501.396813	769497.000249	44.568641
3501.699425	769481.129305	44.573645
3501.575525	769474.101642	44.578650
3501.292505	769477.943286	44.583655
3501.466640	769462.684906	44.588660
3501.362482	769452.302460	44.593665
3501.244068	769443.154523	44.598669
3501.225939	769444.340340	44.603674
3501.381072	769442.392534	44.608679
3501.553289	769406.088759	44.613684
3501.130047	769408.622779	44.618689
3501.215067	769387.612312	44.623693
3501.480598	769379.534666	44.628698
3501.252395	769369.566835	44.633703
3501.431913	769351.202227	44.638708
3501.366897	769341.798932	44.643713
3501.399516	769343.321419	44.648717
3501.413936	769323.702456	44.653722
3501.211824	769321.616312	44.658727
3501.219016	769300.076252	44.663732
3501.386582	769300.147168	44.668737
3501.391355	769294.330340	44.673741
3501.605148	769293.605033	44.678746
3501.158864	769287.221751	44.683751
3500.997069	769279.608688	44.688756
3501.074153	769268.506098	44.693761
3501.201251	769268.140087	44.698765
3501.260626	769252.259433	44.703770
3501.380435	769261.308681	44.708775
3501.112876	769218.915400	44.713780
3501.238958	769205.586662	44.718785
3501.074941	769218.773666	44.723789
3501.446441	769208.016798	44.728794
3501.260868	769206.125051	44.733799
3501.263686	769197.893327	44.738804
3501.423515	769186.875563	44.743809
3501.310710	769168.903677	44.748813
3501.291345	769163.977921	44.753818
3501.156874	769174.597114	44.758823
3501.288517	769161.316670	44.763828
3501.284402	769146.481315	44.768833
3501.285404	769132.039401	44.773837
3500.966115	769123.219892	44.778842
3500.940695	769127.955778	44.783847
3501.058084	769115.416936	44.788852
3501.274469	769118.585033	44.793857
3501.064544	769127.195865	44.798861
3501.333400	769114.730651	44.803866
3501.471726	769085.134225	44.808871
3501.334908	769078.453340	44.813876
3501.036297	769070.073967	44.818881
3501.220220	769074.036062	44.823885
3501.134991	769065.769405	44.828890
3501.113984	769050.295877	44.833895
3501.250844	769030.902424	44.838900
3501.399273	769027.871241	44.843905
3501.120306	769018.404198	44.848909
3501.465376	769026.184382	44.853914
3501.234468	769015.427885	44.858919
3501.304409	768985.004397	44.863924
3501.334298	768990.174870	44.868929
3501.217183	768979.547448	44.873933
3501.386214	768975.280597	44.878938
3501.319513	768971.200443	44.883943
3501.373476	768944.131150	44.888948
3501.325795	768940.885782	44.893953
3501.107454	768938.950073	44.898957
3501.483334	768931.494542	44.903962
3501.289633	768923.344174	44.908967
3501.204362	768895.262538	44.913972
3501.318847	768894.454971	44.918977
3501.303267	768887.704654	44.923981
3501.366870	768883.504408	44.928986
3501.391007	768886.309945	44.933991
3501.604330	768851.919038	44.938996
3501.334144	768847.231551	44.944001
3501.548316	768838.274542	44.949005
3501.449769	768822.813314	44.954010
3501.192509	768802.941984	44.959015
3501.300059	768807.754753	44.964020
3501.368496	768802.419966	44.969025
3501.143361	768807.681864	44.974029
3501.173661	768798.705803	44.979034
3501.349293	768781.178383	44.984039
3501.068096	768758.797015	44.989044
3501.294619	768752.795363	44.994049
3500.946192	768756.352399	44.999053
3501.279805	768753.142727	45.004058
3501.094968	768756.327775	45.009063
3500.850301	768736.602068	45.014068
3501.282226	768724.552969	45.019073
3501.212393	768717.072057	45.024077
3501.296112	768708.136381	45.029082
3501.121223	768724.924355	45.034087
3501.502387	768718.749328	45.039092
3501.626766	768698.716274	45.044097
3501.503889	768681.829294	45.049101
3501.764171	768662.315969	45.054106
3501.502826	768653.683526	45.059111
3501.273558	768637.996985	45.064116
3501.539514	768630.904308	45.069121
3501.148665	768625.743631	45.074125
3501.510616	768620.656123	45.079130
3501.259866	768600.043790	45.084135
3501.455852	768587.195360	45.089140
3501.503341	768591.278771	45.094145
3501.252902	768576.877198	45.099149
3501.382333	768566.947967	45.104154
3501.237738	768552.824670	45.109159
3501.140401	768540.418817	45.114164
3501.332089	768528.704732	45.119169
3501.255817	768540.103930	45.124173
3501.490662	768532.572648	45.129178
3501.354376	768503.906423	45.134183
3501.456770	768490.136670	45.139188
3501.408164	768492.855750	45.144193
3501.045223	768501.295334	45.149197
3501.485584	768477.118295	45.154202
3501.247380	768461.284973	45.159207
3501.415804	768447.997201	45.164212
3501.323271	768447.864503	45.169217
3501.367180	768453.624563	45.174221
3501.519216	768422.643029	45.179226
3500.895419	768410.520851	45.184231
3501.414886	768402.696087	45.189236
3501.655599	768409.409642	45.194241
3501.593294	768392.314853	45.199245
3501.543246	768356.486226	45.204250
3501.309083	768358.644389	45.209255
3501.250478	768355.006211	45.214260
3501.552204	768338.196396	45.219265
3501.170756	768325.146861	45.224269
3501.658938	768313.235719	45.229274
3501.672007	768308.698411	45.234279
3501.289872	768283.818219	45.239284
3501.448040	768264.074201	45.244289
3501.072679	768262.657125	45.249293
3501.211123	768264.162402	45.254298
3500.796398	768263.244759	45.259303
3501.273775	768258.581647	45.264308
3501.175621	768234.541821	45.269313
3501.328570	768219.284391	45.274317
3501.220065	768223.147223	45.279322
3501.398368	768220.307974	45.284327
3501.152670	768214.038607	45.289332
3501.190450	768213.933735	45.294337
3501.264694	768189.372416	45.299341
3501.375390	768173.776784	45.304346
3501.249351	768176.508734	45.309351
3501.399285	768179.343112	45.314356
3501.404169	768167.166278	45.319361
3501.363465	768147.158935	45.324365
3501.652374	768124.188798	45.329370
3501.547132	768129.135648	45.334375
3501.509770	768113.514983	45.339380
3501.453886	768090.601535	45.344385
3501.320376	768098.461523	45.349389
3501.444577	768075.764847	45.354394
3501.277095	768087.031871	45.359399
3501.710553	768058.812345	45.364404
3501.753213	768034.206422	45.369409
3501.032340	768055.768984	45.374413
3501.643139	768031.759618	45.379418
3501.267273	768014.814205	45.384423
3501.235405	768011.072862	45.389428
3501.451794	767990.283304	45.394433
3501.140139	767995.313539	45.399437
3501.593347	767973.991962	45.404442
3501.417162	767957.062823	45.409447
3501.573201	767939.240875	45.414452
3501.242367	767946.936337	45.419457
3501.176337	767932.552439	45.424461
3501.330161	767908.963029	45.429466
3500.910242	767902.229125	45.434471
3501.049257	767897.818714	45.439476
3501.182683	767910.022386	45.444481
3500.925711	767908.289956	45.449485
3501.069987	767901.611010	45.454490
3500.951107	767906.856037	45.459495
3501.134176	767905.593394	45.464500
3501.186169	767867.823021	45.469505
3501.210501	767866.586518	45.474509
3501.127636	767858.811107	45.479514
3501.201813	767859.932672	45.484519
3501.371949	767863.601901	45.489524
3501.303363	767864.007519	45.494529
3501.214522	767853.718915	45.499533
3501.279114	767828.467833	45.504538
3501.221958	767833.061875	45.509543
3501.347080	767828.357925	45.514548
3501.175093	767841.400779	45.519553
3501.456681	767827.403098	45.524557
3501.343134	767794.589392	45.529562
3501.456832	767795.950948	45.534567
3501.619720	767778.669766	45.539572
3501.810157	767773.412746	45.544577
3501.398277	767750.261103	45.549581
3501.501574	767732.841736	45.554586
3501.347380	767737.501118	45.559591
3501.242062	767711.932541	45.564596
3501.634957	767690.915884	45.569601
3501.042515	767697.274332	45.574605
3501.319393	767688.946502	45.579610
3501.377397	767691.599014	45.584615
3501.277898	767660.310661	45.589620
3501.356676	767648.268705	45.594625
3501.319255	767660.599525	45.599629
3501.355385	767643.930496	45.604634
3501.367964	767644.372056	45.609639
3501.306782	767611.401023	45.614644
3501.062144	767605.969054	45.619649
3501.123476	767598.366816	45.624653
3501.235580	767596.277724	45.629658
3501.041584	767597.049108	45.634663
3501.205082	767591.549901	45.639668
3501.498939	767562.710610	45.644673
3501.205156	767556.793705	45.649677
3501.601919	767540.015743	45.654682
3501.322039	767557.513827	45.659687
3501.450271	767540.927998	45.664692
3501.395786	767520.132451	45.669697
3501.556559	767494.322101	45.674701
3501.510829	767501.971057	45.679706
3501.306392	767481.249402	45.684711
3501.156417	767468.110936	45.689716
3501.524298	767462.183569	45.694721
3501.470906	767457.163690	45.699725
3501.640115	767455.558155	45.704730
3501.443738	767432.074226	45.709735
3501.322918	767415.331940	45.714740
3501.538053	767414.852741	45.719745
3501.258919	767402.869344	45.724749
3501.295163	767385.213710	45.729754
3501.280604	767378.708363	45.734759
3501.153092	767368.031053	45.739764
3501.576900	767351.987728	45.744769
3501.447118	767356.643325	45.749773
3501.437728	767326.176845	45.754778
3501.395312	767331.409679	45.759783
3501.397004	767322.929567	45.764788
3501.551628	767313.931244	45.769793
3501.178423	767285.299362	45.774797
3501.361740	767283.987275	45.779802
3500.971022	767284.495285	45.784807
3501.285046	767259.151894	45.789812
3501.211918	767188.070834	45.794817
3501.144597	767075.278195	45.799821
3501.281437	766883.860167	45.804826
3501.137274	766662.653829	45.809831
3500.681544	766370.638002	45.814836
3500.827591	766016.677633	45.819841
3500.349925	765619.901765	45.824845
3500.274069	765157.203115	45.829850
3499.569925	764644.126654	45.834855
3499.275558	764080.589750	45.839860
3499.108373	763451.928421	45.844865
3498.645323	762771.367508	45.849869
3498.375385	762036.740422	45.854874
3497.593291	761240.845267	45.859879
3496.977652	760403.092256	45.864884
3496.739376	759492.291791	45.869889
3495.757596	758547.694432	45.874893
3495.593387	757511.816827	45.879898
3494.677793	756453.606635	45.884903
3493.986197	755312.948142	45.889908
3493.448955	754133.770905	45.894913
3492.857656	752899.989442	45.899917
3491.940194	751588.255387	45.904922
3490.780079	750233.499573	45.909927
3490.130928	748818.624862	45.914932
3489.510115	747355.294969	45.919937
3488.367604	745832.054892	45.924941
3487.648319	744249.011846	45.929946
3486.778824	742623.486917	45.934951
3485.694236	740916.631894	45.939956
3484.646649	739169.225767	45.944961
3483.182944	737366.371534	45.949965
3482.240786	735517.136223	45.954970
3481.044964	733605.128957	45.959975
3479.526141	731644.037770	45.964980
3478.330206	729634.565142	45.969985
3477.052559	727574.167780	45.974989
3475.947531	725447.254286	45.979994
3474.274256	723280.620584	45.984999
3472.656992	721073.986928	45.990004
3471.560425	718803.140559	45.995009
3470.184008	716477.989095	46.000013
3468.914233	714097.683165	46.005018
3467.036692	711688.262983	46.010023
3465.168902	709215.787589	46.015028
3463.684337	706706.572526	46.020033
3461.924295	704141.866711	46.025037
3460.673390	701535.612795	46.030042
3458.905274	698887.550289	46.035047
3457.200818	696194.915292	46.040052
3455.500508	693428.181076	46.045057
3453.713855	690649.058938	46.050061
3452.174445	687793.271379	46.055066
3450.481473	684907.578150	46.060071
3448.372357	681979.647625	46.065076
3446.904302	678986.401135	46.070081
3444.556541	675963.374037	46.075085
3442.639288	672894.423764	46.080090
3440.856372	669775.273183	46.085095
3438.385688	666623.180701	46.090100
3436.532865	663424.581506	46.095105
3434.120106	660181.929618	46.100109
3432.406787	656887.491684	46.105114
3430.285273	653569.686444	46.110119
3428.104093	650198.506795	46.115124
3425.928243	646790.097355	46.120129
3423.637395	643361.205499	46.125133
3421.541754	639864.293949	46.130138
3419.269319	636333.748252	46.135143
3417.197431	632773.639679	46.140148
3414.955852	629165.081924	46.145153
3412.283381	625527.669659	46.150157
3409.872557	621827.546461	46.155162
3407.837904	618108.307524	46.160167
3405.216640	614351.551866	46.165172
3403.181109	610548.685447	46.170177
3400.324501	606707.486009	46.175181
3398.019046	602822.583923	46.180186
3395.575762	598900.291449	46.185191
3392.847265	594963.266603	46.190196
3390.663737	590978.662364	46.195201
3387.407553	586971.094059	46.200205
3385.147380	582902.201787	46.205210
3382.749285	578823.435189	46.210215
3379.456200	574706.197451	46.215220
3377.338290	570559.540698	46.220225
3374.419519	566371.949393	46.225229
3371.611917	562152.520368	46.230234
3368.850778	557895.963857	46.235239
3366.389371	553617.644738	46.240244
3363.477058	549298.076541	46.245249
3360.487475	544959.015805	46.250253
3357.922375	540582.425410	46.255258
3354.630405	536177.060761	46.260263
3351.725091	531747.226863	46.265268
3348.893103	527275.203765	46.270273
3345.413172	522797.611028	46.275277
3342.633755	518291.864956	46.280282
3339.848621	513747.216521	46.285287
3336.813408	509167.942934	46.290292
3333.967689	504575.254194	46.295297
3331.064215	499962.832330	46.300301
3328.167263	495299.005974	46.305306
3325.060540	490644.773345	46.310311
3321.715843	485932.800437	46.315316
3318.512086	481213.485156	46.320321
3314.987360	476459.931594	46.325325
3311.936970	471685.636674	46.330330
3308.731878	466898.063442	46.335335
3305.517761	462086.917707	46.340340
3302.424599	457248.590077	46.345345
3299.113131	452401.197253	46.350349
3295.936758	447530.401339	46.355354
3292.479948	442632.530244	46.360359
3289.125635	437716.107560	46.365364
3285.879007	432775.212562	46.370369
3282.531140	427830.351321	46.375373
3278.973268	422850.294547	46.380378
3275.901077	417869.621111	46.385383
3272.520972	412854.665583	46.390388
3269.036348	407836.369399	46.395393
3265.381337	402786.954864	46.400397
3261.835197	397729.158104	46.405402
3258.454305	392667.902603	46.410407
3254.573525	387581.393087	46.415412
3251.078245	382494.620733	46.420417
3247.661848	377399.685103	46.425421
3244.432441	372265.218003	46.430426
3240.453548	367150.012503	46.435431
3236.573455	362002.360263	46.440436
3233.430072	356845.403086	46.445441
3229.417337	351693.327501	46.450445
3225.980565	346520.358503	46.455450
3222.053031	341336.521815	46.460455
3218.493126	336138.220124	46.465460
3214.781306	330939.466469	46.470465
3211.189343	325730.730347	46.475469
3207.445566	320512.801447	46.480474
3203.632487	315293.234644	46.485479
3199.724278	310078.204708	46.490484
3196.171996	304846.666784	46.495489
3192.583675	299616.032708	46.500493
3188.446109	294367.756659	46.505498
3184.554956	289127.257010	46.510503
3180.428758	283883.596792	46.515508
3176.744004	278636.368397	46.520513
3172.861585	273385.533917	46.525517
3169.227542	268146.234004	46.530522
3165.183817	262899.511532	46.535527
3161.385799	257640.429211	46.540532
3157.745329	252398.936659	46.545537
3153.294812	247136.186112	46.550541
3149.421295	241891.790778	46.555546
3145.509873	236643.399171	46.560551
3141.168317	231409.497842	46.565556
3137.457662	226159.566193	46.570561
3133.355963	220926.606928	46.575565
3128.920414	215690.095391	46.580570
3124.945581	210477.000980	46.585575
3120.959503	205184.158009	46.590580
3117.191385	199950.869023	46.595585
3112.443689	194750.663838	46.600589
3108.466984	189549.644769	46.605594
3104.323295	184359.784657	46.610599
3099.805478	179189.406729	46.615604
3095.775172	174017.557619	46.620609
3091.352232	168866.488090	46.625613
3087.129254	163716.666149	46.630618
3083.036366	158597.019274	46.635623
3078.581180	153485.193335	46.640628
3074.147797	148382.998652	46.645633
3069.750122	143306.187671	46.650637
3065.376713	138238.831605	46.655642
3060.997691	133191.321306	46.660647
3056.662691	128157.711810	46.665652
3051.994535	123146.805888	46.670657
3047.012652	118160.932347	46.675661
3042.646907	113191.497559	46.680666
3038.178901	108236.127624	46.685671
3033.380001	103325.746425	46.690676
3028.713172	98414.992391	46.695681
3024.256716	93562.361872	46.700685
3019.251277	88711.524383	46.705690
3014.366876	83886.918582	46.710695
3009.055351	79110.804055	46.715700
3004.536229	74354.205307	46.720705
2999.343443	69651.861290	46.725709
2994.581475	64973.586317	46.730714
2988.886319	60335.670284	46.735719
2983.713525	55753.574487	46.740724
2978.568832	51186.009150	46.745729
2972.057299	46705.241985	46.750733
2965.324601	42301.446984	46.755738
2952.916485	38090.783720	46.760743
2937.840254	34066.879445	46.765748
2923.608424	30194.698316	46.770753
2909.305306	26560.299251	46.775757
2896.345186	23093.467081	46.780762
2883.338823	19876.113459	46.785767
2870.635399	16902.342221	46.790772
2858.414915	14134.612434	46.795777
2845.587997	11599.216775	46.800781
2832.182942	9338.059008	46.805786
2815.571261	7405.414798	46.810791
2797.889054	5796.275506	46.815796
2781.317955	4450.732678	46.820801
2766.411886	3365.284660	46.825805
2754.895859	2489.059254	46.830810
2745.803325	1826.321326	46.835815
2738.479601	1324.001182	46.840820
2732.776834	953.438853	46.845825
2728.432775	712.924728	46.850829
2725.659058	536.720689	46.855834
2723.217855	415.235583	46.860839
2721.327078	337.760354	46.865844
2719.881360	263.065367	46.870849
2718.777256	238.623682	46.875853
2717.492680	185.472365	46.880858
2716.133975	136.539362	46.885863
2713.895675	100.773428	46.890868
2706.873585	214.254101	46.895873
2702.437362	244.859897	46.900877
2701.168152	250.727986	46.905882
2700.534059	242.710159	46.910887
2698.677666	243.605457	46.915892
2696.550687	227.934533	46.920897
2693.548050	239.128408	46.925901
2690.557863	245.204763	46.930906
2687.677050	237.419537	46.935911
2683.882360	250.586666	46.940916
2681.269774	235.583419	46.945921
2678.040836	240.275687	46.950925
2674.712757	236.978513	46.955930
2671.556823	238.101495	46.960935
2668.410358	249.106784	46.965940
2665.012164	238.074659	46.970945
2661.686567	240.388513	46.975949
2658.392942	238.639546	46.980954
2655.416696	232.533364	46.985959
2651.398301	233.306936	46.990964
2648.601364	234.846767	46.995969
2645.392661	232.829363	47.000973
2642.087213	228.883147	47.005978
2638.856105	221.750916	47.010983
2634.790092	230.545034	47.015988
2631.806633	223.238685	47.020993
2629.020869	235.189147	47.025997
2625.156905	234.037591	47.031002
2621.736862	226.407411	47.036007
2618.402239	230.745080	47.041012
2615.310148	224.087674	47.046017
2611.627523	222.860843	47.051021
2608.250007	224.930218	47.056026
2605.397929	211.483598	47.061031
2601.812615	222.551085	47.066036
2598.135404	225.857040	47.071041
2594.334249	225.894344	47.076045
2590.461503	227.413472	47.081050
2587.790112	218.869614	47.086055
2584.462645	225.049556	47.091060
2581.549354	216.841564	47.096065
2578.059137	215.633440	47.101069
2574.049085	220.522611	47.106074
2570.567616	214.641848	47.111079
2567.272207	216.296455	47.116084
2563.433705	213.313968	47.121089
2559.928611	213.614925	47.126093
2556.755043	215.087743	47.131098
2553.310561	217.771875	47.136103
2549.686495	222.612507	47.141108
2546.562346	217.022090	47.146113
2543.162508	222.079896	47.151117
2539.927687	216.868526	47.156122
2536.896228	209.088393	47.161127
2533.052800	216.580250	47.166132
2529.338672	204.597849	47.171137
2525.377885	209.511079	47.176141
2521.905925	214.613637	47.181146
2519.073612	211.989532	47.186151
2515.700849	217.809166	47.191156
2512.288537	220.310819	47.196161
2508.718744	213.565308	47.201165
2505.222948	211.282265	47.206170
2501.774499	198.508441	47.211175
2497.876044	213.084591	47.216180
2494.681134	203.722705	47.221185
2491.045455	198.753176	47.226189
2487.270789	204.767937	47.231194
2484.287016	197.687454	47.236199
2480.731121	205.373825	47.241204
2477.340450	205.882372	47.246209
2473.752268	203.734154	47.251213
2470.150407	205.526548	47.256218
2467.170396	196.598563	47.261223
2463.430840	201.183900	47.266228
2460.183019	185.090710	47.271233
2456.738582	202.621603	47.276237
2453.543603	195.471089	47.281242
2450.124450	197.849682	47.286247
2445.603609	194.660424	47.291252
2442.524767	197.258258	47.296257
2438.696169	205.743465	47.301261
2435.494872	198.375768	47.306266
2432.190650	202.836153	47.311271
2428.215876	196.975652	47.316276
2425.217554	192.073512	47.321281
2421.606120	188.916230	47.326285
2418.478732	183.142916	47.331290
2414.955898	187.285664	47.336295
2411.100534	197.299171	47.341300
2407.545981	189.041934	47.346305
2403.931198	192.127632	47.351309
2400.415732	191.746569	47.356314
2397.598800	181.297847	47.361319
2393.993226	193.545525	47.366324
2390.678147	198.190925	47.371329
2386.932066	190.407175	47.376333
2383.228011	190.448599	47.381338
2379.878823	191.433282	47.386343
2376.099713	188.913384	47.391348
2372.712541	186.944778	47.396353
2369.561403	192.323508	47.401357
2365.566648	190.936951	47.406362
2362.323985	196.295262	47.411367
2358.950663	190.100316	47.416372
2355.459974	197.432154	47.421377
2351.774549	194.715187	47.426381
2348.315489	199.394116	47.431386
2344.848267	196.883768	47.436391
2341.062480	198.764465	47.441396
2337.918138	194.584749	47.446401
2334.785211	197.255770	47.451405
2331.071782	199.762365	47.456410
2327.956884	192.635508	47.461415
2323.818842	190.851925	47.466420
2319.973713	187.440516	47.471425
2316.622455	183.218182	47.476429
2313.667986	185.174398	47.481434
2310.429650	187.741166	47.486439
2306.147644	188.877748	47.491444
2303.330190	183.737371	47.496449
2299.692418	192.119136	47.501453
2296.241605	187.055296	47.506458
2292.878943	179.534932	47.511463
2288.962301	190.477493	47.516468
2285.375272	183.586577	47.521473
2282.007425	191.387821	47.526477
2278.680490	193.341747	47.531482
2275.334635	182.063978	47.536487
2271.607104	196.805868	47.541492
2268.207836	190.255835	47.546497
2264.849131	187.198526	47.551501
2261.074502	193.577425	47.556506
2257.555220	185.060806	47.561511
2253.630367	186.594117	47.566516
2250.750036	185.990180	47.571521
2247.480567	186.061416	47.576525
2243.502383	188.464716	47.581530
2240.095119	181.934568	47.586535
2236.541445	191.255231	47.591540
2233.373136	179.267659	47.596545
2229.804865	183.037059	47.601549
2226.251412	177.919647	47.606554
2222.958602	184.013980	47.611559
2218.806183	171.612472	47.616564
2215.426905	181.724913	47.621569
2212.005489	175.175116	47.626573
2208.534522	181.722674	47.631578
2205.460131	175.686579	47.636583
2201.990429	171.305269	47.641588
2198.535537	179.887173	47.646593
2194.513096	176.878601	47.651597
2190.831866	179.739064	47.656602
2187.603123	171.899513	47.661607
2184.218516	191.481171	47.666612
2180.357528	184.890629	47.671617
2177.039217	179.652276	47.676621
2173.979813	178.013680	47.681626
2170.692543	185.720181	47.686631
2166.874152	181.807506	47.691636
2163.319018	187.361864	47.696641
2159.309157	182.076573	47.701645
2156.292649	182.875658	47.706650
2152.841971	182.204035	47.711655
2149.233039	182.393460	47.716660
2145.710331	181.750591	47.721665
2142.101744	182.740475	47.726669
2138.608949	179.918053	47.731674
2134.660957	171.033098	47.736679
2131.615992	181.323356	47.741684
2128.620314	169.807474	47.746689
2125.056507	179.989944	47.751693
2121.588695	180.906006	47.756698
2117.968607	184.658548	47.761703
2114.435066	185.835258	47.766708
2110.843443	185.570584	47.771713
2107.196378	181.743732	47.776717
2103.408685	177.791894	47.781722
2099.764652	185.121988	47.786727
2096.218305	184.158062	47.791732
2093.510079	178.416100	47.796737
2090.125783	173.987313	47.801741
2086.365361	171.189432	47.806746
2082.965133	161.264084	47.811751
2079.376249	182.404606	47.816756
2075.715569	184.375785	47.821761
2072.050375	177.975487	47.826765
2068.549599	178.192691	47.831770
2065.309308	171.577777	47.836775
2061.599805	181.789928	47.841780
2058.567405	174.968466	47.846785
2054.981907	174.731421	47.851789
2051.175786	174.625679	47.856794
2047.488186	175.873609	47.861799
2044.338353	184.832145	47.866804
2041.261074	170.616179	47.871809
2037.361735	178.591408	47.876813
2033.667006	187.840504	47.881818
2029.749769	175.251552	47.886823
2026.570801	175.771649	47.891828
2022.939089	176.937956	47.896833
2019.697568	178.135796	47.901837
2016.404384	165.474502	47.906842
2013.047378	168.466546	47.911847
2009.427676	173.512181	47.916852
2005.883601	165.546766	47.921857
2002.368393	173.116495	47.926861
1998.240237	170.266163	47.931866
1995.139801	178.782172	47.936871
1991.828246	184.798193	47.941876
1988.650571	165.060166	47.946881
1984.800538	168.912753	47.951885
1980.905207	172.084973	47.956890
1977.668701	163.838372	47.961895
1974.158504	171.897023	47.966900
1970.762967	170.661933	47.971905
1967.036707	167.799582	47.976909
1963.803976	171.617631	47.981914
1960.295732	166.886551	47.986919
1957.055819	176.208826	47.991924
1953.762012	162.189155	47.996929
1950.118896	171.682325	48.001933
1946.368528	155.706519	48.006938
1943.007758	162.577647	48.011943
1939.065993	166.513956	48.016948
1935.645037	162.446863	48.021953
1932.399377	167.323582	48.026957
1928.729261	167.693591	48.031962
1924.772532	164.839687	48.036967
1921.337101	168.811357	48.041972
1917.766002	167.424811	48.046977
1914.854619	163.380015	48.051981
1910.976220	167.709494	48.056986
1908.516855	151.366139	48.061991
1904.363433	163.695271	48.066996
1900.965998	151.287936	48.072001
1897.252535	163.641469	48.077005
1893.457333	160.910403	48.082010
1890.190648	160.765968	48.087015
1886.410105	160.497648	48.092020
1883.291178	160.855474	48.097025
1879.770089	162.450027	48.102029
1876.400005	162.348702	48.107034
1872.822326	161.121314	48.112039
1869.009570	168.163924	48.117044
1865.793231	171.103029	48.122049
1862.189669	167.284822	48.127053
1858.572070	160.560012	48.132058
1855.010463	167.612297	48.137063
1851.752289	169.279212	48.142068
1848.554844	162.138011	48.147073
1844.953731	167.171474	48.152077
1841.095069	172.258679	48.157082
1837.815098	167.547224	48.162087
1833.764632	165.665818	48.167092
1830.517961	168.845438	48.172097
1827.090320	163.166054	48.177101
1823.618985	167.821369	48.182106
1820.542672	160.298913	48.187111
1816.612744	164.721686	48.192116
1813.161221	155.285817	48.197121
1809.945595	155.554559	48.202125
1806.334862	158.053531	48.207130
1803.232014	156.803184	48.212135
1799.499087	157.444373	48.217140
1795.749221	162.452281	48.222145
1792.195363	152.718987	48.227149
1788.706656	159.191001	48.232154
1784.988124	160.298446	48.237159
1781.030965	163.599749	48.242164
1778.030199	158.650471	48.247169
1774.977930	147.198788	48.252173
1771.189979	158.759215	48.257178
1767.904445	147.582407	48.262183
1764.120075	150.642206	48.267188
1760.438542	152.890748	48.272193
1757.270667	166.359419	48.277197
1753.185520	165.114796	48.282202
1750.255977	156.072216	48.287207
1746.391868	159.287249	48.292212
1743.612585	149.093017	48.297217
1740.092434	144.830579	48.302221
1736.111025	156.592728	48.307226
1732.730472	147.251652	48.312231
1728.966031	155.847998	48.317236
1725.595017	145.296010	48.322241
1722.093726	151.948892	48.327245
1718.772180	152.757443	48.332250
1715.145948	147.152231	48.337255
1711.519495	161.709593	48.342260
1707.802828	154.605897	48.347265
1704.627663	156.864047	48.352269
1701.344541	146.218743	48.357274
1697.895480	155.809029	48.362279
1694.110046	165.773982	48.367284
1690.784464	157.793912	48.372289
1686.851134	160.967812	48.377293
1683.278184	156.560601	48.382298
1680.021464	151.084352	48.387303
1676.594565	151.050605	48.392308
1673.059206	152.033959	48.397313
1669.978013	148.418832	48.402317
1666.123301	150.958918	48.407322
1662.755550	150.937616	48.412327
1658.761105	155.523833	48.417332
1655.311184	155.187070	48.422337
1652.054890	144.044772	48.427341
1648.291667	154.488014	48.432346
1645.182890	150.273074	48.437351
1641.648998	155.445196	48.442356
1638.483962	139.388129	48.447361
1634.845600	152.939492	48.452365
1631.058192	161.880731	48.457370
1627.867906	150.903259	48.462375
1624.118427	159.551740	48.467380
1620.735114	158.409120	48.472385
1616.970257	147.550837	48.477389
1613.255633	157.063629	48.482394
1610.062457	150.867090	48.487399
1606.242509	152.480010	48.492404
1603.054003	145.430799	48.497409
1599.618814	150.544425	48.502413
1595.969579	159.166806	48.507418
1592.739687	147.464348	48.512423
1588.886732	160.002221	48.517428
1585.626907	157.255788	48.522433
1582.396968	153.067384	48.527437
1578.875755	149.594859	48.532442
1575.591576	137.223996	48.537447
1571.350265	146.156790	48.542452
1567.833012	152.697633	48.547457
1564.152752	167.096509	48.552461
1560.728071	153.402350	48.557466
1557.489379	143.540438	48.562471
1554.153895	145.258420	48.567476
1550.384761	146.633309	48.572481
1546.986355	141.453597	48.577485
1543.369826	144.285335	48.582490
1540.088742	136.902489	48.587495
1536.357301	151.969923	48.592500
1533.391129	144.245154	48.597505
1529.633320	144.002771	48.602509
1525.892256	140.696885	48.607514
1522.737729	135.156799	48.612519
1518.888337	147.802428	48.617524
1515.575125	151.277390	48.622529
1511.815276	149.310034	48.627533
1508.253673	146.370748	48.632538
1505.225267	146.193480	48.637543
1501.685924	153.939347	48.642548
1497.812794	147.695156	48.647553
1494.438916	154.060240	48.652557
1490.688001	140.440892	48.657562
1487.210502	140.361918	48.662567
1483.577509	153.103364	48.667572
1480.506408	158.614726	48.672577
1477.021593	138.738729	48.677581
1473.005179	147.633965	48.682586
1470.157921	143.461192	48.687591
1466.488309	150.087600	48.692596
1463.116387	155.515230	48.697601
1459.521986	142.675804	48.702605
1455.838026	159.722394	48.707610
1452.554408	152.766796	48.712615
1448.761341	149.152647	48.717620
1445.472880	154.234429	48.722625
1442.044507	143.745647	48.727629
1438.566204	151.715282	48.732634
1435.247535	137.125475	48.737639
1431.417222	139.723610	48.742644
1427.680989	141.076756	48.747649
1424.193860	140.832179	48.752653
1420.751006	148.007699	48.757658
1417.669650	142.665727	48.762663
1413.808218	140.283864	48.767668
1410.196687	140.216592	48.772673
1406.927939	143.589352	48.777677
1403.091819	152.380184	48.782682
1400.064517	140.880493	48.787687
1396.333136	145.285699	48.792692
1392.961038	143.523650	48.797697
1389.660633	146.502279	48.802701
1385.802510	148.389371	48.807706
1382.683176	147.289526	48.812711
1378.849972	154.225530	48.817716
1375.255199	147.520324	48.822721
1371.574989	154.708997	48.827725
1368.303737	160.388203	48.832730
1365.182433	153.746033	48.837735
1361.372912	154.609046	48.842740
1358.040867	143.612511	48.847745
1354.089666	148.142910	48.852749
1350.852206	145.840512	48.857754
1347.194930	148.767271	48.862759
1343.858843	142.695585	48.867764
1340.652285	143.729014	48.872769
1337.031177	148.875018	48.877773
1333.123803	135.575703	48.882778
1329.902946	135.202280	48.887783
1326.326763	130.433640	48.892788
1322.752103	137.600071	48.897793
1319.531965	135.138657	48.902797
1315.779728	140.479258	48.907802
1312.198125	138.735256	48.912807
1308.649051	145.468711	48.917812
1305.069187	145.806778	48.922817
1301.471242	139.766203	48.927821
1298.165156	149.770190	48.932826
1294.960893	144.653673	48.937831
1291.416748	144.283315	48.942836
1288.073865	136.944942	48.947841
1284.504288	134.533727	48.952845
1280.490540	144.966971	48.957850
1277.373987	132.685530	48.962855
1273.419311	141.848880	48.967860
1270.451359	148.330948	48.972865
1267.006711	139.083501	48.977869
1263.246580	141.702795	48.982874
1260.147894	142.149303	48.987879
1256.215639	148.431536	48.992884
1252.365648	142.102388	48.997889
1249.129342	141.047466	49.002893
1245.701091	130.708849	49.007898
1242.591335	131.700791	49.012903
1239.099300	138.897228	49.017908
1235.391009	141.892544	49.022913
1231.723299	142.913254	49.027917
1228.065159	146.564553	49.032922
1225.066418	131.672275	49.037927
1220.907730	133.271957	49.042932
1217.573189	140.368907	49.047937
1214.132401	140.491880	49.052941
1210.757768	145.129819	49.057946
1207.350789	127.935304	49.062951
1203.584546	142.233549	49.067956
1200.216985	133.093191	49.072961
1196.860990	130.441462	49.077965
1193.159541	137.421108	49.082970
1189.824793	134.718520	49.087975
1186.059203	140.090787	49.092980
1182.259406	136.594126	49.097985
1179.066113	136.839735	49.102989
1175.721697	133.305692	49.107994
1172.506458	134.087772	49.112999
1168.648571	136.733414	49.118004
1165.329401	134.402866	49.123009
1161.811549	133.944673	49.128013
1158.012384	146.815878	49.133018
1154.978494	135.979009	49.138023
1151.281525	144.250935	49.143028
1147.941265	143.408365	49.148033
1143.996414	125.896517	49.153037
1140.310871	132.610740	49.158042
1137.469685	119.852705	49.163047
1133.489511	129.589376	49.168052
1129.845016	132.680170	49.173057
1126.508146	134.379930	49.178061
1122.887736	138.416521	49.183066
1119.714280	131.746300	49.188071
1116.301448	140.392498	49.193076
1112.444706	138.049007	49.198081
1109.154014	138.139065	49.203085
1105.551765	140.708403	49.208090
1102.416580	132.831812	49.213095
1098.410628	127.176196	49.218100
1095.176631	134.155965	49.223105
1091.799937	133.683285	49.228109
1087.874165	139.395477	49.233114
1084.539723	118.101635	49.238119
1080.923087	134.739726	49.243124
1077.544426	126.759901	49.248129
1074.197713	140.559680	49.253133
1070.644392	146.587362	49.258138
1067.533307	139.873424	49.263143
1063.797011	143.019463	49.268148
1059.924285	137.789183	49.273153
1056.407936	141.960361	49.278157
1052.698229	138.696630	49.283162
1049.478665	130.381659	49.288167
1045.942538	136.778742	49.293172
1042.544993	139.681121	49.298177
1039.273638	135.722011	49.303181
1035.800917	143.851107	49.308186
1032.358112	144.918945	49.313191
1028.404375	142.280057	49.318196
1024.929849	146.898167	49.323201
1021.621001	134.355711	49.328205
1018.426146	139.818124	49.333210
1014.482232	133.679358	49.338215
1011.011485	140.527377	49.343220
1007.241112	122.436525	49.348225
1003.955516	124.069669	49.353229
1000.060050	129.505200	49.358234
997.322200	118.669475	49.363239
993.872806	127.188863	49.368244
990.213415	136.754750	49.373249
986.399133	129.612868	49.378253
983.113729	145.499013	49.383258
979.788860	138.082763	49.388263
975.921837	141.476157	49.393268
972.350702	128.968853	49.398273
969.270365	126.260089	49.403277
965.277736	135.359804	49.408282
961.680987	129.940477	49.413287
958.677582	132.440808	49.418292
954.993893	129.939994	49.423297
951.540578	128.524547	49.428301
947.849716	144.975863	49.433306
944.537124	128.316940	49.438311
941.015507	136.154921	49.443316
937.352092	135.075961	49.448321
933.940768	133.867477	49.453325
930.393626	132.151437	49.458330
927.065740	123.951206	49.463335
923.388456	130.711816	49.468340
919.845024	132.515728	49.473345
916.294997	123.110590	49.478349
912.858334	126.315358	49.483354
909.496455	125.909778	49.488359
906.003722	124.387606	49.493364
902.126465	123.832128	49.498369
899.121215	128.288061	49.503373
895.529676	127.311994	49.508378
892.079859	124.958371	49.513383
888.457085	127.634301	49.518388
885.182291	132.332652	49.523393
881.491994	126.995611	49.528397
877.341018	125.968877	49.533402
874.384141	119.300621	49.538407
870.949493	123.276766	49.543412
867.211188	119.699013	49.548417
864.095890	119.615894	49.553421
860.463455	124.523661	49.558426
857.084973	116.860825	49.563431
853.056703	126.055759	49.568436
849.751468	123.275470	49.573441
846.491806	117.049090	49.578445
843.105032	126.528387	49.583450
839.888412	129.432358	49.588455
836.237735	126.075052	49.593460
832.365486	132.795585	49.598465
828.534500	130.618490	49.603469
824.730967	133.416644	49.608474
821.707894	136.169192	49.613479
818.574364	116.755316	49.618484
814.912676	135.728739	49.623489
811.614364	124.047039	49.628493
807.551260	136.227669	49.633498
804.017514	124.072430	49.638503
800.684615	122.360547	49.643508
797.781077	124.295431	49.648513
794.100064	120.858613	49.653517
790.342743	134.207949	49.658522
786.720724	120.242553	49.663527
783.268836	134.251880	49.668532
779.609716	137.340630	49.673537
776.387314	128.705551	49.678541
772.677603	125.578529	49.683546
769.631871	113.136640	49.688551
765.946592	125.242064	49.693556
762.082484	120.899547	49.698561
758.709091	118.220044	49.703565
755.088857	132.177564	49.708570
751.720280	125.608728	49.713575
748.376011	123.930024	49.718580
744.775642	131.489269	49.723585
741.968333	134.556350	49.728589
737.928648	129.266636	49.733594
734.375266	118.785238	49.738599
730.711228	122.898579	49.743604
727.055636	120.416244	49.748609
723.640554	118.242451	49.753613
720.111140	126.792828	49.758618
716.611048	127.354410	49.763623
713.492346	113.833960	49.768628
709.899929	129.976378	49.773633
706.256130	121.020850	49.778637
702.802273	132.455208	49.783642
699.261166	120.002427	49.788647
695.323200	133.506239	49.793652
692.083824	127.867442	49.798657
688.715307	124.205936	49.803661
685.112766	124.468556	49.808666
681.828619	113.670835	49.813671
678.385116	120.723942	49.818676
674.836080	126.492121	49.823681
671.441479	123.984473	49.828685
667.736077	124.007585	49.833690
664.053007	115.755085	49.838695
660.189252	128.757614	49.843700
657.360921	125.296467	49.848705
653.712732	130.927228	49.853709
649.828680	133.600953	49.858714
646.754427	124.651731	49.863719
643.446809	127.337103	49.868724
639.970106	130.669568	49.873729
636.342743	126.584787	49.878733
632.459862	132.240212	49.883738
629.165566	123.799116	49.888743
625.501175	127.855448	49.893748
622.043688	130.458047	49.898753
618.923197	124.985229	49.903757
615.139169	132.137722	49.908762
611.636449	132.415664	49.913767
608.032174	130.727489	49.918772
604.565796	115.349413	49.923777
601.384053	123.838375	49.928781
597.839973	125.636046	49.933786
594.249248	115.533829	49.938791
590.683448	130.314290	49.943796
586.780166	119.037008	49.948801
583.808100	122.021359	49.953805
579.965334	129.954567	49.958810
576.742102	121.401236	49.963815
573.068451	125.681594	49.968820
569.462924	127.446218	49.973825
566.343837	126.901267	49.978829
562.193021	129.662806	49.983834
558.991602	117.190618	49.988839
555.535589	120.721852	49.993844
552.060859	119.939188	49.998849
549.243780	118.773046	50.003853
545.126669	120.182668	50.008858
541.613828	114.473207	50.013863
537.831519	130.410478	50.018868
534.640920	122.704662	50.023873
531.139359	120.536772	50.028877
527.512598	128.160656	50.033882
523.950042	119.673269	50.038887
520.543678	121.473885	50.043892
517.181026	115.974235	50.048897
513.711685	122.281602	50.053901
509.890058	121.839599	50.058906
506.480436	119.091632	50.063911
503.307365	117.691797	50.068916
499.601382	116.295046	50.073921
496.459603	112.112091	50.078925
492.632917	120.563685	50.083930
489.054972	124.676248	50.088935
485.249229	128.498805	50.093940
481.754955	125.620894	50.098945
478.568677	124.793385	50.103949
474.872116	114.095583	50.108954
471.404854	118.879969	50.113959
467.744116	119.344306	50.118964
464.684854	116.640698	50.123969
461.056822	120.187074	50.128973
457.483651	131.497398	50.133978
454.079373	123.207267	50.138983
450.496383	121.810944	50.143988
447.152486	116.844728	50.148993
443.709659	111.670019	50.153997
439.639870	125.944810	50.159002
436.436122	117.953841	50.164007
433.034210	113.111362	50.169012
429.755643	130.793756	50.174017
426.223808	106.673771	50.179021
422.403596	118.578171	50.184026
418.839683	113.896731	50.189031
415.367946	120.166951	50.194036
411.599440	124.712364	50.199041
408.744051	107.641394	50.204045
404.965924	124.431888	50.209050
401.851300	116.589789	50.214055
397.981198	115.139211	50.219060
394.599666	117.970195	50.224065
390.952701	112.220532	50.229069
387.421993	115.420175	50.234074
383.768282	111.183730	50.239079
380.244380	123.785734	50.244084
376.539209	116.292382	50.249089
373.526167	109.945027	50.254093
369.892444	116.448217	50.259098
366.764150	112.410792	50.264103
362.989336	121.446506	50.269108
359.378038	111.882363	50.274113
355.786472	115.020550	50.279117
352.139151	128.649049	50.284122
349.173323	121.696147	50.289127
345.581790	122.557259	50.294132
341.992203	129.529881	50.299137
338.609424	115.506932	50.304141
334.839465	115.583418	50.309146
331.376513	110.515591	50.314151
327.811122	119.607982	50.319156
324.408786	110.739592	50.324161
320.622834	113.813128	50.329165
317.357192	115.205446	50.334170
313.809520	115.781317	50.339175
310.367429	117.761575	50.344180
306.580121	119.855199	50.349185
303.567333	121.405628	50.354189
299.913508	120.731810	50.359194
296.201051	113.863418	50.364199
292.873665	107.987820	50.369204
289.391737	104.881273	50.374209
286.050330	105.767194	50.379213
282.226342	110.306942	50.384218
278.563651	112.276306	50.389223
274.959671	117.994658	50.394228
271.412230	118.936428	50.399233
268.794036	110.349820	50.404237
264.829420	118.175850	50.409242
261.193373	112.590700	50.414247
257.761399	116.514015	50.419252
254.183863	114.124034	50.424257
251.466700	104.909073	50.429261
247.600975	110.675712	50.434266
243.844694	109.713614	50.439271
240.092259	113.265860	50.444276
236.648669	114.694720	50.449281
233.053493	106.199303	50.454285
229.681608	108.041230	50.459290
226.373859	119.091540	50.464295
222.999717	116.258551	50.469300
219.069826	115.552947	50.474305
216.263233	110.253426	50.479309
212.131687	130.331987	50.484314
208.504161	122.503507	50.489319
205.503737	121.385668	50.494324
201.718725	116.557488	50.499329
198.286741	106.379788	50.504333
194.476002	106.315210	50.509338
191.166863	118.926495	50.514343
187.725931	106.999240	50.519348
184.038830	120.993483	50.524353
180.910630	110.884478	50.529357
177.303209	111.268644	50.534362
173.804726	100.184158	50.539367
170.197756	105.861420	50.544372
166.444261	107.133556	50.549377
163.210206	107.318908	50.554381
159.631114	121.508510	50.559386
156.462247	112.454356	50.564391
153.094995	113.755812	50.569396
149.180460	104.391677	50.574401
145.548877	109.242438	50.579405
142.137279	121.286040	50.584410
138.769537	107.816280	50.589415
135.598513	102.629995	50.594420
131.900299	111.272844	50.599425
128.229454	105.685441	50.604429
124.532941	115.826198	50.609434
120.987028	106.832692	50.614439
117.524834	112.725596	50.619444
114.010540	108.997049	50.624449
110.532094	108.476382	50.629453
107.164720	104.985987	50.634458
103.797959	103.539832	50.639463
100.493128	106.273541	50.644468
96.602479	109.151505	50.649473
93.173788	103.635790	50.654477
89.386785	103.126068	50.659482
86.037027	105.800122	50.664487
82.868494	107.604674	50.669492
79.055065	118.470061	50.674497
75.695533	104.061270	50.679501
72.223056	110.055239	50.684506
68.827452	112.564232	50.689511
65.162963	118.262894	50.694516
61.296873	106.857426	50.699521
58.150760	111.753206	50.704525
54.314798	115.528704	50.709530
51.277663	98.342881	50.714535
47.784066	98.528463	50.719540
44.019100	116.247833	50.724545
40.485845	105.974898	50.729549
36.900080	112.252989	50.734554
33.927994	104.428989	50.739559
30.552546	97.983370	50.744564
26.374743	104.544572	50.749569
22.964373	95.774687	50.754573
19.303332	113.397572	50.759578
15.991601	115.416522	50.764583
12.405665	110.319585	50.769588
8.830313	109.387220	50.774593
5.753915	95.579073	50.779597
2.098954	113.805322	50.784602