Thu Jun 16 18:38:27 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.002426	85.638690	0.000000
-0.172758	82.157751	0.005005
-0.188787	96.555537	0.010010
-0.057337	78.980457	0.015014
-0.256760	85.780923	0.020019
-0.482046	93.217849	0.025024
-0.263052	73.626889	0.030029
-1.128908	67.465197	0.035034
-0.898753	66.964729	0.040038
-1.325229	55.856674	0.045043
-1.283443	54.978806	0.050048
-1.533722	40.389016	0.055053
-2.106262	34.899932	0.060058
-2.144574	25.712783	0.065062
-2.879501	13.304164	0.070067
-3.640840	13.198702	0.075072
-3.178603	16.607155	0.080077
-3.728365	16.122620	0.085082
-3.775404	11.237775	0.090086
-4.420364	-0.161370	0.095091
-4.711298	2.251919	0.100096
-4.564524	-8.917086	0.105101
-4.565704	-1.086812	0.110106
-5.050661	-3.539659	0.115110
-5.659186	-4.186239	0.120115
-5.946276	-0.586081	0.125120
-6.062708	-13.427878	0.130125
-5.956097	-3.887486	0.135130
-6.390828	-11.708041	0.140134
-6.998043	-15.606293	0.145139
-7.515907	1.545704	0.150144
-7.383654	-3.872990	0.155149
-7.691005	4.625463	0.160154
-7.471162	-5.752472	0.165158
-7.613876	-3.940709	0.170163
-8.540449	-3.428317	0.175168
-8.863456	-11.667084	0.180173
-8.958391	-10.881630	0.185178
-8.978409	-13.696424	0.190182
-9.015810	-4.508007	0.195187
-8.934391	-6.182151	0.200192
-9.605373	-8.705967	0.205197
-10.456065	4.283260	0.210202
-10.662338	-7.190054	0.215206
-10.899390	0.890125	0.220211
-10.846377	-0.117353	0.225216
-10.549652	-4.015435	0.230221
-11.665585	-3.611048	0.235226
-12.133243	-8.349718	0.240230
-12.560273	2.453351	0.245235
-12.473519	0.338227	0.250240
-12.154848	-5.276915	0.255245
-12.665924	-4.120015	0.260250
-12.401812	-1.936473	0.265254
-12.155053	-6.911597	0.270259
-13.344594	-2.960942	0.275264
-13.629629	-8.824563	0.280269
-14.104645	-1.450591	0.285274
-14.017757	-7.909892	0.290278
-14.076601	0.636377	0.295283
-14.769105	-8.112635	0.300288
-15.090654	-6.116628	0.305293
-15.621173	-4.160076	0.310298
-15.666791	-11.828488	0.315302
-15.718202	-4.668758	0.320307
-15.741130	-14.221176	0.325312
-15.289134	-9.365651	0.330317
-16.151254	-5.777404	0.335322
-16.722821	-20.944733	0.340326
-17.272741	-1.689161	0.345331
-17.281417	-4.164782	0.350336
-16.874957	-15.380447	0.355341
-17.248475	-15.553946	0.360346
-17.919212	-16.168342	0.365350
-18.450262	-12.118354	0.370355
-18.608953	-8.384431	0.375360
-18.533169	-17.137189	0.380365
-18.880989	0.146031	0.385370
-18.811559	-15.227176	0.390374
-19.083022	-5.006134	0.395379
-19.859231	-9.544941	0.400384
-19.947725	-7.360149	0.405389
-20.121015	-10.493917	0.410394
-20.463491	-22.328574	0.415398
-20.137501	-8.154829	0.420403
-20.853245	-2.360093	0.425408
-21.241841	-10.894638	0.430413
-21.525493	-4.498292	0.435418
-21.698964	-16.910783	0.440422
-22.023169	-6.410121	0.445427
-22.158786	-10.872579	0.450432
-21.863598	-7.057891	0.455437
-22.717912	-6.324318	0.460442
-22.947953	-7.884145	0.465446
-23.255286	-6.698073	0.470451
-23.323705	-2.751570	0.475456
-23.249542	-6.504350	0.480461
-23.789826	1.369441	0.485466
-24.603859	-3.804370	0.490470
-24.392251	-6.834629	0.495475
-24.953773	-7.552410	0.500480
-25.061226	-4.034326	0.505485
-25.105680	-1.356534	0.510490
-25.090404	-0.940405	0.515494
-24.992373	-5.816662	0.520499
-25.917988	3.584352	0.525504
-26.344264	-1.993112	0.530509
-26.420801	-1.036769	0.535514
-26.855544	-6.526706	0.540518
-26.838448	0.370826	0.545523
-26.713372	-0.568454	0.550528
-27.212507	-11.066206	0.555533
-28.145496	4.111658	0.560538
-28.241105	-5.852672	0.565542
-28.273298	-7.417474	0.570547
-28.534645	-3.581347	0.575552
-28.385244	-17.486369	0.580557
-28.397103	-7.811174	0.585562
-28.791320	-9.075133	0.590566
-29.566122	-14.084258	0.595571
-29.941285	-8.854572	0.600576
-30.045498	-14.063410	0.605581
-30.415929	0.243883	0.610586
-30.005267	-12.925739	0.615590
-29.952862	0.358573	0.620595
-31.019318	4.675024	0.625600
-31.017648	-12.519691	0.630605
-31.209527	2.974605	0.635610
-31.545352	-1.383145	0.640614
-32.152271	-1.448025	0.645619
-32.971708	7.680225	0.650624
-32.892446	-7.944109	0.655629
-33.052595	0.568982	0.660634
-32.744769	-9.061087	0.665638
-32.754515	-4.817861	0.670643
-33.059984	-9.613324	0.675648
-32.863763	-13.554579	0.680653
-33.783442	-4.480603	0.685658
-33.960064	-4.134768	0.690662
-34.232883	2.444275	0.695667
-34.555413	4.709674	0.700672
-35.486504	1.781942	0.705677
-35.626308	-4.919777	0.710682
-35.467104	5.493503	0.715686
-35.658544	-2.287252	0.720691
-36.335200	-2.738776	0.725696
-36.064918	-5.820758	0.730701
-36.505143	8.501628	0.735706
-36.325018	-1.636425	0.740710
-36.532467	-5.227040	0.745715
-37.298232	11.164662	0.750720
-37.434545	-2.735575	0.755725
-38.007543	10.498104	0.760730
-37.743343	-7.581330	0.765734
-37.824523	8.062486	0.770739
-38.362780	-4.583518	0.775744
-38.938112	-6.920403	0.780749
-39.250932	-3.746620	0.785754
-39.634692	-8.392112	0.790758
-39.510361	-9.171152	0.795763
-39.718610	-6.446956	0.800768
-39.438864	-2.853859	0.805773
-39.517264	-3.524910	0.810778
-40.326616	-4.207059	0.815782
-40.874193	-3.037909	0.820787
-41.064899	-0.771309	0.825792
-41.049371	-3.287432	0.830797
-41.348164	-0.975051	0.835802
-41.420397	-0.477472	0.840806
-42.095162	2.292552	0.845811
-42.590021	5.773741	0.850816
-42.618329	-10.911105	0.855821
-42.725281	2.696099	0.860826
-42.869759	-9.337223	0.865830
-42.926165	-7.018139	0.870835
-43.138685	-3.549973	0.875840
-43.601961	-6.829079	0.880845
-44.207075	1.586582	0.885850
-44.613791	8.806518	0.890854
-44.448640	-8.598420	0.895859
-44.538176	-4.177944	0.900864
-44.054634	-16.343564	0.905869
-45.222351	-7.846569	0.910874
-45.584942	-14.604100	0.915878
-46.118139	-9.079363	0.920883
-46.330376	-10.810534	0.925888
-45.819061	-11.553396	0.930893
-45.968072	0.804194	0.935898
-46.614969	-1.673876	0.940902
-46.760695	-9.580764	0.945907
-47.596459	1.144931	0.950912
-47.441750	-5.220906	0.955917
-47.373906	-1.324349	0.960922
-47.662187	-8.552316	0.965926
-48.193462	-2.424819	0.970931
-48.946355	-3.862718	0.975936
-48.738285	-0.304538	0.980941
-49.074728	-1.759766	0.985946
-49.219324	-1.501600	0.990950
-49.305155	-9.698565	0.995955
-49.256688	-0.014100	1.000960
-49.887776	-4.767586	1.005965
-50.351478	-3.231787	1.010970
-50.459165	-3.474868	1.015974
-50.523701	-8.262893	1.020979
-50.860071	-9.823298	1.025984
-51.408136	-10.410412	1.030989
-51.798972	-2.063512	1.035994
-52.087975	-7.865801	1.040998
-52.117197	-10.421486	1.046003
-52.374112	-1.139573	1.051008
-52.285000	-9.406590	1.056013
-52.389730	-4.571820	1.061018
-52.443839	-15.283894	1.066022
-53.250677	-6.619931	1.071027
-53.955337	-2.752859	1.076032
-53.721669	-5.820504	1.081037
-53.819952	0.075415	1.086042
-53.989651	-1.437657	1.091046
-54.122937	-12.258092	1.096051
-54.835902	-0.260516	1.101056
-55.134696	-5.551834	1.106061
-55.938833	8.911691	1.111066
-55.701776	-7.894950	1.116070
-55.504709	-13.157230	1.121075
-55.480286	-2.718625	1.126080
-55.601695	-16.243561	1.131085
-56.531786	-18.912778	1.136090
-57.158345	-14.561498	1.141094
-57.213792	-8.274591	1.146099
-57.478209	-6.405818	1.151104
-57.418233	-9.068290	1.156109
-57.581085	-7.254384	1.161114
-57.606506	-6.331647	1.166118
-57.797685	-13.829988	1.171123
-58.776668	-10.559624	1.176128
-58.338065	-13.935692	1.181133
-58.641339	-14.341192	1.186138
-59.378873	-12.861060	1.191142
-59.832176	-5.065873	1.196147
-60.050103	-1.653736	1.201152
-60.221181	-2.977361	1.206157
-60.612054	-1.548602	1.211162
-60.512096	-9.056094	1.216166
-60.493179	-5.563336	1.221171
-60.544092	1.818384	1.226176
-60.799437	-14.509982	1.231181
-61.753181	-2.317924	1.236186
-62.118920	-7.753952	1.241190
-61.870118	-6.061847	1.246195
-62.069063	-4.971328	1.251200
-61.943311	-5.063375	1.256205
-62.626015	-3.832133	1.261210
-63.333412	1.376304	1.266214
-63.364793	-1.408101	1.271219
-63.660779	-0.421212	1.276224
-63.555705	-10.587400	1.281229
-63.513760	3.558017	1.286234
-63.875422	-2.636945	1.291238
-64.670360	-7.459437	1.296243
-65.227894	-7.961820	1.301248
-64.921610	-10.885196	1.306253
-65.323116	-4.794834	1.311258
-65.384212	-1.409801	1.316262
-65.080194	-14.277373	1.321267
-65.934989	-8.336831	1.326272
-66.584882	-7.113281	1.331277
-66.679126	-7.007176	1.336282
-66.909277	-10.536718	1.341286
-66.651061	-5.284939	1.346291
-67.010144	-3.591910	1.351296
-67.856316	-24.715584	1.356301
-68.294957	-6.297641	1.361306
-68.535833	-12.363493	1.366310
-68.270759	-2.857288	1.371315
-68.819155	-16.867571	1.376320
-68.364290	-11.165776	1.381325
-68.273741	-4.106363	1.386330
-68.794345	-9.270355	1.391334
-69.380866	-12.009771	1.396339
-70.060606	-5.350358	1.401344
-70.014255	-0.114172	1.406349
-70.172571	-6.109717	1.411354
-70.237472	-11.288943	1.416358
-70.736110	-5.459451	1.421363
-71.674905	-7.549903	1.426368
-71.409052	-7.511501	1.431373
-71.774072	-4.131879	1.436378
-71.725540	0.028217	1.441382
-71.834140	-1.358415	1.446387
-71.978339	-11.543780	1.451392
-71.801747	-17.022180	1.456397
-72.481077	-1.096516	1.461402
-72.892468	0.253455	1.466406
-72.907504	-9.141036	1.471411
-73.901119	3.697095	1.476416
-74.435625	-12.859491	1.481421
-74.187852	-1.038163	1.486426
-74.406189	-8.440071	1.491430
-74.858088	-8.124900	1.496435
-75.173444	-3.234603	1.501440
-75.089795	-8.972002	1.506445
-75.150903	3.034055	1.511450
-75.178778	-2.510790	1.516454
-75.044744	-10.070872	1.521459
-76.097956	-6.274543	1.526464
-76.319417	-13.396937	1.531469
-76.815527	-5.001367	1.536474
-76.593863	6.566793	1.541478
-76.343199	0.628648	1.546483
-77.067459	-2.280973	1.551488
-77.538349	-3.432911	1.556493
-78.169497	5.762677	1.561498
-78.191067	-4.877336	1.566502
-78.060167	-7.693000	1.571507
-78.508019	-2.347217	1.576512
-78.616869	-5.577660	1.581517
-79.136632	7.140723	1.586522
-79.309083	1.557521	1.591526
-79.744196	-3.796305	1.596531
-80.051325	12.207847	1.601536
-79.631076	-8.982891	1.606541
-80.031200	-8.117300	1.611546
-80.815524	-12.981892	1.616550
-80.930713	-10.744448	1.621555
-81.471032	-10.178780	1.626560
-81.451688	-22.303583	1.631565
-81.652233	-7.925923	1.636570
-81.533943	-18.070513	1.641574
-81.554062	-8.298264	1.646579
-82.391484	0.744265	1.651584
-82.573248	-8.236733	1.656589
-83.163646	-0.888678	1.661594
-83.205053	-9.812173	1.666598
-83.253549	-10.542228	1.671603
-83.187663	-9.433820	1.676608
-83.218449	-12.795252	1.681613
-83.995948	-11.737857	1.686618
-84.553501	-9.564825	1.691622
-84.517393	-10.469176	1.696627
-84.762877	-6.970998	1.701632
-84.641759	-9.302723	1.706637
-84.934825	3.877381	1.711642
-85.872985	-1.600872	1.716646
-85.728189	-11.787040	1.721651
-86.507713	-1.593214	1.726656
-86.161953	-10.890275	1.731661
-86.449456	-1.040583	1.736666
-86.664923	-5.760155	1.741670
-87.171206	-11.518240	1.746675
-88.009654	-9.158002	1.751680
-87.750478	-9.869850	1.756685
-88.125292	-3.059577	1.761690
-87.917288	-8.076339	1.766694
-88.065368	-14.906214	1.771699
-88.376047	-6.237732	1.776704
-88.325164	-8.195097	1.781709
-88.823412	-0.962801	1.786714
-89.346445	4.974414	1.791718
-89.299578	-10.003498	1.796723
-89.486840	-0.453709	1.801728
-89.832453	-12.726854	1.806733
-90.908986	-4.976051	1.811738
-91.277963	-13.687360	1.816742
-91.096344	-22.037037	1.821747
-91.339706	-18.553813	1.826752
-90.998402	-19.522220	1.831757
-90.945655	-10.930676	1.836762
-91.051443	-20.378823	1.841766
-91.475552	-14.655176	1.846771
-92.502076	-2.735905	1.851776
-92.576293	-22.761474	1.856781
-92.736071	-12.497538	1.861786
-93.075686	-18.564430	1.866790
-93.465097	-11.591139	1.871795
-93.925482	-1.840633	1.876800
-94.266814	-5.301682	1.881805
-94.331533	-5.964239	1.886810
-94.429986	-2.961140	1.891814
-94.425883	-11.098874	1.896819
-94.619558	-13.476831	1.901824
-94.489028	-25.621387	1.906829
-95.280551	-18.519290	1.911834
-95.747576	-11.756526	1.916838
-95.545018	-14.903080	1.921843
-96.030302	-19.003292	1.926848
-96.190490	-27.536104	1.931853
-97.080535	-20.165762	1.936858
-97.151667	-25.439054	1.941862
-97.186523	-20.400773	1.946867
-97.615792	-18.296889	1.951872
-97.604026	-28.494403	1.956877
-97.514990	-14.072370	1.961882
-97.860842	-8.763179	1.966886
-97.622019	-16.868574	1.971891
-98.419968	-22.615443	1.976896
-98.627501	-24.366230	1.981901
-98.670947	-22.234071	1.986906
-99.329093	-12.768552	1.991910
-99.886925	-21.875124	1.996915
-100.017380	-24.292658	2.006912
-99.172630	-12.704658	2.016909
-98.996455	-12.806847	2.026906
-98.834516	-13.655342	2.036902
-98.167734	-23.494431	2.046899
-97.948212	-13.710155	2.056896
-97.091433	-11.723553	2.066893
-96.618334	-9.933379	2.076890
-96.167682	-6.013832	2.086886
-95.434990	-8.893108	2.096883
-95.099008	-10.087208	2.106880
-94.346443	-15.012455	2.116877
-93.835461	-5.566613	2.126874
-93.384885	-12.040272	2.136870
-93.355918	-10.358598	2.146867
-92.571674	-4.924311	2.156864
-92.149565	-3.333544	2.166861
-91.791666	-1.378133	2.176858
-90.857690	0.384717	2.186854
-90.474301	-5.668443	2.196851
-90.142569	-7.421038	2.206848
-89.165582	-13.102205	2.216845
-88.956672	-15.917236	2.226842
-88.738995	-7.144461	2.236838
-88.212465	-9.115206	2.246835
-87.735132	6.066875	2.256832
-86.874821	-0.404818	2.266829
-86.080409	-6.823240	2.276826
-85.962845	-6.737639	2.286822
-85.810585	-5.337469	2.296819
-85.197404	-7.217235	2.306816
-84.417771	-4.303071	2.316813
-84.230436	-3.115544	2.326810
-83.356409	-10.574493	2.336806
-83.237274	-8.083791	2.346803
-82.580413	-1.520325	2.356800
-81.412785	-9.014463	2.366797
-81.468205	-7.968474	2.376794
-81.326760	-8.668028	2.386790
-80.311952	-8.761144	2.396787
-79.848884	-9.234897	2.406784
-79.777039	-0.455598	2.416781
-79.049908	1.056260	2.426778
-78.082966	2.404317	2.436774
-78.070016	-1.295312	2.446771
-77.883398	-6.662367	2.456768
-76.698056	-5.234389	2.466765
-76.309655	-5.439465	2.476762
-76.378358	-11.055132	2.486758
-75.371935	-7.006266	2.496755
-74.843739	-1.549710	2.506752
-74.788463	-8.477032	2.516749
-73.973613	-7.828050	2.526746
-73.510503	-12.484188	2.536742
-73.130148	-2.400803	2.546739
-72.226221	0.091327	2.556736
-72.158194	-4.152056	2.566733
-71.707121	-15.434642	2.576730
-70.882713	-16.808443	2.586726
-70.771054	-24.979490	2.596723
-69.822133	-18.575477	2.606720
-69.356513	-10.435425	2.616717
-69.118997	-8.722776	2.626714
-68.380862	-12.333334	2.636710
-67.477017	-6.808769	2.646707
-67.538071	-9.349172	2.656704
-67.449049	-10.641489	2.666701
-66.265267	-17.577809	2.676698
-65.969868	-11.084353	2.686694
-65.365072	-7.164348	2.696691
-64.552501	-5.862048	2.706688
-64.678055	-4.112309	2.716685
-64.276346	3.624718	2.726682
-63.260234	-6.574879	2.736678
-62.914097	-5.518207	2.746675
-62.731662	-15.046006	2.756672
-61.862734	-14.606683	2.766669
-61.255672	-10.588470	2.776666
-61.245545	-7.140345	2.786662
-60.310461	-12.851330	2.796659
-59.743560	-13.349010	2.806656
-59.614418	-10.686946	2.816653
-59.240136	-5.702214	2.826650
-58.516114	-2.851062	2.836646
-57.934293	-15.420642	2.846643
-56.758158	-4.927357	2.856640
-56.968748	-4.137149	2.866637
-56.571020	-7.242341	2.876634
-56.171696	-14.678346	2.886630
-55.420242	-16.057127	2.896627
-54.964388	-9.004714	2.906624
-54.364294	-8.422969	2.916621
-53.455002	-10.713653	2.926618
-53.340298	-19.335599	2.936614
-53.176446	-15.360846	2.946611
-52.648762	-13.804861	2.956608
-52.059545	-16.183655	2.966605
-51.763285	-12.549500	2.976602
-50.527368	-12.201598	2.986598
-50.406681	-15.535069	2.996595
-49.983192	-9.491143	3.006592
-49.273882	-17.454403	3.016589
-48.823204	-18.479081	3.026586
-48.827027	-18.128639	3.036582
-48.009613	-17.343366	3.046579
-47.176037	-14.251911	3.056576
-47.155088	-6.467565	3.066573
-46.357783	-7.412966	3.076570
-45.893297	-12.124501	3.086566
-45.547180	-14.169393	3.096563
-44.819875	-12.693022	3.106560
-44.272690	-15.128879	3.116557
-43.998184	-11.681380	3.126554
-43.516145	-19.059684	3.136550
-42.664171	-17.974988	3.146547
-42.657608	-8.803755	3.156544
-41.868179	-5.756169	3.166541
-41.131971	-9.133236	3.176538
-40.542951	-15.935747	3.186534
-40.755798	-10.160835	3.196531
-40.006867	-8.568661	3.206528
-39.704026	-10.089037	3.216525
-38.591139	-17.427381	3.226522
-37.794049	-13.199644	3.236518
-37.576118	-10.767546	3.246515
-37.428248	-3.285305	3.256512
-37.592202	-7.171534	3.266509
-36.428484	-3.158632	3.276506
-35.868003	-11.983461	3.286502
-35.198288	-10.575213	3.296499
-34.508128	-11.753363	3.306496
-34.359667	-8.351956	3.316493
-34.232212	-9.162499	3.326490
-33.298337	-11.218292	3.336486
-32.719654	-15.073500	3.346483
-32.782721	-16.498434	3.356480
-31.588144	-9.753022	3.366477
-31.251038	-9.264228	3.376474
-31.334913	-5.955405	3.386470
-29.897617	-9.723640	3.396467
-29.641784	-8.246644	3.406464
-29.439377	-18.637977	3.416461
-29.202219	-11.830005	3.426458
-28.135915	-17.057507	3.436454
-28.167363	-11.212757	3.446451
-27.336758	-6.974948	3.456448
-26.425952	-9.102595	3.466445
-26.563569	-4.748630	3.476442
-26.168647	-13.379947	3.486438
-25.057551	-15.314930	3.496435
-25.068768	-8.547798	3.506432
-24.645647	-7.589192	3.516429
-24.029908	-9.811504	3.526426
-23.338595	-17.770307	3.536422
-22.557017	-8.427552	3.546419
-22.140322	-16.223768	3.556416
-22.165838	-13.309293	3.566413
-21.486194	-12.186976	3.576410
-20.889311	-14.529794	3.586406
-20.489950	-14.874972	3.596403
-19.338479	-19.874040	3.606400
-18.847394	-16.607887	3.616397
-18.852735	-18.106223	3.626394
-18.579919	-15.542235	3.636390
-18.109335	-21.401224	3.646387
-17.341612	-23.245279	3.656384
-16.937307	-7.463528	3.666381
-15.875757	-15.575533	3.676378
-15.596444	-12.959129	3.686374
-15.539591	-14.591763	3.696371
-15.571040	-10.025877	3.706368
-14.407571	-12.417436	3.716365
-13.594758	-7.593878	3.726362
-12.733372	-10.647032	3.736358
-12.689025	-12.148443	3.746355
-12.373249	-12.138420	3.756352
-12.331631	-8.868068	3.766349
-11.501820	-2.667892	3.776346
-10.822726	-7.026981	3.786342
-9.946311	-15.285109	3.796339
-9.472007	-21.320888	3.806336
-9.361896	-18.472144	3.816333
-9.451098	-16.040357	3.826330
-7.979578	-10.128188	3.836326
-7.640118	-12.175881	3.846323
-7.754304	-10.487834	3.856320
-6.757371	-6.099012	3.866317
-6.171461	0.609350	3.876314
-5.917104	-7.744182	3.886310
-5.296792	0.754480	3.896307
-4.444649	-4.498233	3.906304
-4.502178	-1.251451	3.916301
-4.208817	4.672192	3.926298
-3.790432	21.181887	3.936294
-2.978858	31.472259	3.946291
-2.677406	31.201593	3.956288
-2.246736	48.882116	3.966285
-1.895258	63.414646	3.976282
-1.442531	72.242920	3.986278
-0.477066	97.891830	3.996275
-0.280948	110.161805	4.006272
0.000000	116.339382	4.011277
0.327204	128.418603	4.016282
0.545048	143.706919	4.021286
0.231497	142.459210	4.026291
0.728051	153.468168	4.031296
0.461629	161.101936	4.036301
0.654331	149.171497	4.041306
0.823476	162.418804	4.046310
0.890153	173.211730	4.051315
1.239485	173.431186	4.056320
1.038512	180.027930	4.061325
1.718056	173.765688	4.066330
1.177923	170.453069	4.071334
0.865940	161.731241	4.076339
1.157681	149.167837	4.081344
0.843502	152.374925	4.086349
1.145775	143.608026	4.091354
0.846651	150.449168	4.096358
0.840277	152.448059	4.101363
1.110555	170.174889	4.106368
0.856115	187.371067	4.111373
1.275533	183.034262	4.116378
1.125227	180.725758	4.121382
0.851208	182.983461	4.126387
1.317455	183.203227	4.131392
0.730544	188.003699	4.136397
1.271932	181.742089	4.141402
1.366619	194.063413	4.146406
1.092096	186.251795	4.151411
1.382532	175.028430	4.156416
0.751481	182.348759	4.161421
1.346068	173.860381	4.166426
1.525535	174.338270	4.171430
1.440542	178.209916	4.176435
1.616109	173.125647	4.181440
1.618322	187.603276	4.186445
1.799383	171.965186	4.191450
1.886514	174.709066	4.196454
1.374236	167.742076	4.201459
1.172928	157.641991	4.206464
0.915686	161.878417	4.211469
1.371658	165.559834	4.216474
1.426594	180.123945	4.221478
1.555934	186.138689	4.226483
1.844210	181.057693	4.231488
1.670624	187.577402	4.236493
1.315196	177.453644	4.241498
1.309103	166.920355	4.246502
1.528519	176.642982	4.251507
1.563444	170.868380	4.256512
1.505555	181.784500	4.261517
1.670115	182.226180	4.266522
1.554138	178.561898	4.271526
1.017691	177.949370	4.276531
1.718941	181.811837	4.281536
1.300856	181.237067	4.286541
1.444813	181.353825	4.291546
1.563136	176.023989	4.296550
1.576002	176.589986	4.301555
1.805868	186.092666	4.306560
1.756587	184.283041	4.311565
1.757269	179.414821	4.316570
1.659985	170.686906	4.321574
1.458254	187.034122	4.326579
1.810734	177.707026	4.331584
1.773352	185.269115	4.336589
1.865895	177.263358	4.341594
1.947227	176.684090	4.346598
1.778060	173.003147	4.351603
1.932348	174.991571	4.356608
1.475679	183.492404	4.361613
1.741269	173.276279	4.366618
1.660801	171.247466	4.371622
1.405868	184.091822	4.376627
1.969624	182.813763	4.381632
1.754822	187.741961	4.386637
1.613955	178.459103	4.391642
1.932614	177.046140	4.396646
1.850086	188.015960	4.401651
2.030144	180.588956	4.406656
1.668371	182.945315	4.411661
1.772198	187.790372	4.416666
1.964154	176.991913	4.421670
1.640201	180.988487	4.426675
2.016728	179.830949	4.431680
1.939644	187.649298	4.436685
1.734027	175.794235	4.441690
1.567272	186.619435	4.446694
1.425117	184.705588	4.451699
1.787265	197.368162	4.456704
2.018893	212.485370	4.461709
2.264238	220.199840	4.466714
2.465022	218.646826	4.471718
2.129761	213.330377	4.476723
2.225813	200.326117	4.481728
1.899552	195.711504	4.486733
2.060493	180.928525	4.491738
2.168933	191.848538	4.496742
1.818976	197.965483	4.501747
2.250083	195.038509	4.506752
1.896439	213.752357	4.511757
1.985307	213.225512	4.516762
2.281229	204.844287	4.521766
2.157792	218.217242	4.526771
2.370893	214.252323	4.531776
2.324229	231.736226	4.536781
2.175083	216.835855	4.541786
2.412745	223.767183	4.546790
2.392498	218.430044	4.551795
2.373171	219.664824	4.556800
1.727127	215.286455	4.561805
1.688720	208.790943	4.566810
1.972475	210.878534	4.571814
2.180274	216.857140	4.576819
2.503402	201.664848	4.581824
2.453913	226.295848	4.586829
2.228206	208.875340	4.591834
1.987472	220.915011	4.596838
2.140857	212.800426	4.601843
2.497603	201.154392	4.606848
2.291377	218.893630	4.611853
2.510832	214.860378	4.616858
2.241205	216.512500	4.621862
2.270493	219.279068	4.626867
2.200036	200.808173	4.631872
1.994038	218.521130	4.636877
2.629244	230.059408	4.641882
2.793109	233.468582	4.646886
2.913179	225.811637	4.651891
2.592112	208.227532	4.656896
2.510104	212.355594	4.661901
2.286878	204.557292	4.666906
2.410561	209.905574	4.671910
2.201627	217.729154	4.676915
2.541333	215.970964	4.681920
2.670879	240.472953	4.686925
2.564348	244.160236	4.691930
3.118092	240.216362	4.696934
2.676916	231.929411	4.701939
2.564208	211.203400	4.706944
2.542914	214.144463	4.711949
2.548666	212.745916	4.716954
2.598909	222.313030	4.721958
2.762863	235.783432	4.726963
3.048896	224.227005	4.731968
2.859370	217.617753	4.736973
2.568609	216.243840	4.741978
2.511107	218.288284	4.746982
2.417559	229.387123	4.751987
2.633790	221.954220	4.756992
2.650452	233.974153	4.761997
2.842798	230.870474	4.767002
2.968603	238.737993	4.772006
2.807417	243.992089	4.777011
3.010559	244.602707	4.782016
2.805598	239.715869	4.787021
3.174388	242.638841	4.792026
2.764250	237.663775	4.797030
2.612109	240.046074	4.802035
2.984162	229.102585	4.807040
2.832216	241.065445	4.812045
2.929955	235.383237	4.817050
3.088091	233.773538	4.822054
2.936047	240.785851	4.827059
3.011130	228.967623	4.832064
2.997867	240.131042	4.837069
3.140262	232.739241	4.842074
2.708871	218.865760	4.847078
2.524200	228.798153	4.852083
3.044081	228.050415	4.857088
2.908660	233.135494	4.862093
3.121940	239.414894	4.867098
3.141870	238.837287	4.872102
3.235580	241.808185	4.877107
3.192206	224.995930	4.882112
3.164906	241.495608	4.887117
3.043331	240.257995	4.892122
3.049359	232.388939	4.897126
3.128665	224.684668	4.902131
3.302685	236.923068	4.907136
3.228570	246.614239	4.912141
3.190693	233.261038	4.917146
3.402138	242.639828	4.922150
2.930576	245.024699	4.927155
3.220177	234.116043	4.932160
3.063881	239.606005	4.937165
2.994595	241.344100	4.942170
3.417867	242.009990	4.947174
3.414956	247.046142	4.952179
3.437587	243.331414	4.957184
3.150298	234.464385	4.962189
3.235441	243.087525	4.967194
3.503302	247.277348	4.972198
2.837611	234.745426	4.977203
3.212777	232.787811	4.982208
3.409011	237.812557	4.987213
3.042081	250.526604	4.992218
3.285783	241.617004	4.997222
3.082571	245.868300	5.002227
3.271396	235.992555	5.007232
3.079293	242.846733	5.012237
3.226506	245.998604	5.017242
3.203631	245.917899	5.022246
3.361207	241.332131	5.027251
3.465230	240.147505	5.032256
3.079077	238.974729	5.037261
3.417925	249.989102	5.042266
3.870442	264.013841	5.047270
3.747010	252.843919	5.052275
3.682492	240.985514	5.057280
3.527378	237.993418	5.062285
3.260712	238.980900	5.067290
3.342370	245.555825	5.072294
3.493532	251.327354	5.077299
3.575033	247.625981	5.082304
3.425124	256.183397	5.087309
3.688828	265.397391	5.092314
3.622062	277.336140	5.097318
3.486818	275.143520	5.102323
3.853976	279.585780	5.107328
3.940521	266.968979	5.112333
3.616862	256.811900	5.117338
3.570874	246.190834	5.122342
3.475285	266.115427	5.127347
3.728478	266.721918	5.132352
3.678844	282.014916	5.137357
3.726013	270.434198	5.142362
4.036006	278.651915	5.147366
3.693147	274.328394	5.152371
3.642403	258.167170	5.157376
3.683641	270.866758	5.162381
3.612896	275.770783	5.167386
3.873607	277.093461	5.172390
3.901733	279.072658	5.177395
3.985687	274.204853	5.182400
3.771858	276.699165	5.187405
3.875168	268.947595	5.192410
4.306150	264.307066	5.197414
3.779448	258.792271	5.202419
3.782790	248.619040	5.207424
3.478931	250.838769	5.212429
3.632748	271.703289	5.217434
3.967912	270.459548	5.222438
4.062261	271.824714	5.227443
4.098161	272.539528	5.232448
4.141185	266.282799	5.237453
4.133826	270.094580	5.242458
4.005595	270.975822	5.247462
3.928426	271.911863	5.252467
3.883157	276.448721	5.257472
3.952724	281.273227	5.262477
3.832080	277.986856	5.267482
4.104277	270.191392	5.272486
4.031844	276.059569	5.277491
4.259025	267.650602	5.282496
4.144768	268.387370	5.287501
4.341812	277.922465	5.292506
4.119906	269.075983	5.297510
3.737796	277.704737	5.302515
4.272597	267.422059	5.307520
3.627019	267.741908	5.312525
3.904202	273.738371	5.317530
3.832713	277.858103	5.322534
3.838371	275.008132	5.327539
4.096322	269.681630	5.332544
3.943809	273.580639	5.337549
4.355698	293.726743	5.342554
4.189096	272.774358	5.347558
4.165920	285.257003	5.352563
4.085947	273.874974	5.357568
4.077676	281.934066	5.362573
3.991856	286.420211	5.367578
4.473413	286.716177	5.372582
4.466621	300.818335	5.377587
4.568148	296.408247	5.382592
4.407417	290.455006	5.387597
4.359554	282.992022	5.392602
4.453949	279.510191	5.397606
4.071240	280.443256	5.402611
4.230436	303.354544	5.407616
4.459274	296.258308	5.412621
4.515111	302.769649	5.417626
4.660838	296.703409	5.422630
4.340218	294.048633	5.427635
4.439158	301.521953	5.432640
4.509186	290.035309	5.437645
4.446101	296.714385	5.442650
4.548470	291.028037	5.447654
4.602860	282.843154	5.452659
4.485899	273.657411	5.457664
4.640637	277.835354	5.462669
4.523066	278.812701	5.467674
4.481183	270.572703	5.472678
4.313306	277.679104	5.477683
4.502268	285.120965	5.482688
4.701040	307.968696	5.487693
4.682327	300.306927	5.492698
4.831361	304.843549	5.497702
4.588813	289.993269	5.502707
4.642286	281.606589	5.507712
4.415900	278.272383	5.512717
4.425266	292.745673	5.517722
4.822210	296.029821	5.522726
4.754121	307.742197	5.527731
5.050239	306.079795	5.532736
4.507156	301.485000	5.537741
4.626090	304.791218	5.542746
4.679787	298.932666	5.547750
4.683815	307.474339	5.552755
4.996549	305.169205	5.557760
4.930428	305.616159	5.562765
4.485997	311.810620	5.567770
4.554957	309.270421	5.572774
4.383950	314.745478	5.577779
4.694941	301.699889	5.582784
4.626826	308.990485	5.587789
4.631193	297.264296	5.592794
4.541629	299.776355	5.597798
4.606903	310.148445	5.602803
4.941394	300.687509	5.607808
4.834049	304.650784	5.612813
4.629277	303.614757	5.617818
4.811592	306.155385	5.622822
4.798129	317.301430	5.627827
5.031710	330.421720	5.632832
5.014738	334.142171	5.637837
5.042199	334.897451	5.642842
5.342009	332.103928	5.647846
4.954666	320.302068	5.652851
4.984262	310.176746	5.657856
5.042181	301.425673	5.662861
4.746836	294.245783	5.667866
5.138788	309.874567	5.672870
5.039086	320.099404	5.677875
5.162626	323.755689	5.682880
5.176855	321.621034	5.687885
5.018117	312.328125	5.692890
5.133866	310.902215	5.697894
5.340198	323.570617	5.702899
5.312618	305.766927	5.707904
4.966116	313.648806	5.712909
4.706844	301.835957	5.717914
5.077602	314.847634	5.722918
5.188181	332.725845	5.727923
5.358873	331.529800	5.732928
5.312886	337.791611	5.737933
5.292313	327.531318	5.742938
5.298259	328.069360	5.747942
5.304366	345.886814	5.752947
5.263355	338.874025	5.757952
5.456876	330.171558	5.762957
5.185781	330.853448	5.767962
5.440529	323.373386	5.772966
4.941371	326.459937	5.777971
5.343468	327.037679	5.782976
5.228054	321.878226	5.787981
5.415108	339.541560	5.792986
5.349016	336.757796	5.797990
5.274213	331.560157	5.802995
5.289526	336.384866	5.808000
5.358194	336.517521	5.813005
5.220946	330.350244	5.818010
5.277883	340.610672	5.823014
5.217545	331.975216	5.828019
5.306904	328.477337	5.833024
5.469391	333.340665	5.838029
5.282690	325.316261	5.843034
5.376924	331.317922	5.848038
5.275321	341.555519	5.853043
5.453175	330.464101	5.858048
5.520859	330.176049	5.863053
4.915323	339.276935	5.868058
5.586737	338.349457	5.873062
5.495030	357.170347	5.878067
5.590100	354.259513	5.883072
5.761603	361.393824	5.888077
5.745929	353.587881	5.893082
5.725876	339.991116	5.898086
5.163995	344.438254	5.903091
5.614182	338.105723	5.908096
6.011310	354.497991	5.913101
5.439304	343.697414	5.918106
5.662736	357.539895	5.923110
5.839231	372.404340	5.928115
6.001805	358.975974	5.933120
5.660040	343.748793	5.938125
5.541876	345.624513	5.943130
5.741119	356.289604	5.948134
5.918785	361.096270	5.953139
6.081349	350.232501	5.958144
5.670306	361.272324	5.963149
5.484826	339.607507	5.968154
5.835241	354.769845	5.973158
5.830333	363.787567	5.978163
5.900424	360.171319	5.983168
6.040153	353.957076	5.988173
5.666297	344.019754	5.993178
5.681451	344.624940	5.998182
5.846021	357.804211	6.003187
5.968812	353.993090	6.008192
6.150173	361.803544	6.013197
5.915607	342.185187	6.018202
5.751847	325.208328	6.023206
5.798001	349.576386	6.028211
6.137861	349.506570	6.033216
5.807928	338.336182	6.038221
5.665715	340.008894	6.043226
5.962055	346.933738	6.048230
5.598579	357.593070	6.053235
6.083445	356.068765	6.058240
5.870405	359.274572	6.063245
5.795472	355.228667	6.068250
6.002657	350.994667	6.073254
5.672638	369.266073	6.078259
5.671612	358.064203	6.083264
5.671965	363.572717	6.088269
5.725473	365.964655	6.093274
5.690847	358.517106	6.098278
5.543385	367.186945	6.103283
5.838319	365.411375	6.108288
5.872003	362.474280	6.113293
5.741440	366.567689	6.118298
5.648478	361.800621	6.123302
5.827168	365.054850	6.128307
5.757755	358.062235	6.133312
5.884340	373.037434	6.138317
5.876767	370.799135	6.143322
5.865114	364.229879	6.148326
5.989961	366.542941	6.153331
6.148938	361.114572	6.158336
5.907186	367.676699	6.163341
5.659506	366.655060	6.168346
5.906924	357.855767	6.173350
5.716548	367.824216	6.178355
5.770312	360.269913	6.183360
5.888937	372.648493	6.188365
5.884734	371.040944	6.193370
5.920023	375.230071	6.198374
5.330777	380.993387	6.203379
5.828390	386.917752	6.208384
5.952264	401.538556	6.213389
6.058889	390.679465	6.218394
6.225908	397.917235	6.223398
5.926052	388.966361	6.228403
6.065723	376.467070	6.233408
5.674111	376.865707	6.238413
5.832245	384.820400	6.243418
6.077953	385.941248	6.248422
5.623466	393.666391	6.253427
6.227256	384.961995	6.258432
5.809727	387.987417	6.263437
5.590294	389.409284	6.268442
6.340580	384.639788	6.273446
6.248151	374.286664	6.278451
5.853451	362.157164	6.283456
5.702818	366.391221	6.288461
5.416412	366.057799	6.293466
5.878477	367.854503	6.298470
5.866007	394.384128	6.303475
5.913049	384.590026	6.308480
6.062162	401.433843	6.313485
5.865088	401.477524	6.318490
6.246697	398.690301	6.323494
5.458454	384.162055	6.328499
6.312131	388.419171	6.333504
5.820781	371.068129	6.338509
5.774025	365.112302	6.343514
6.130407	368.048003	6.348518
5.650636	365.015910	6.353523
5.834030	374.207133	6.358528
5.915135	392.455611	6.363533
6.000310	385.420072	6.368538
6.111739	376.204120	6.373542
5.868204	372.404699	6.378547
5.760233	379.546530	6.383552
5.586091	365.554337	6.388557
5.844216	381.953228	6.393562
6.172869	395.996782	6.398566
5.755343	390.733427	6.403571
5.998221	392.636799	6.408576
6.078470	386.056291	6.413581
6.075626	378.565201	6.418586
5.975651	371.042416	6.423590
5.696041	363.277423	6.428595
5.606376	352.560405	6.433600
5.761013	366.768443	6.438605
5.925984	388.898429	6.443610
6.042596	383.936500	6.448614
6.206628	390.282703	6.453619
6.016516	371.813223	6.458624
5.903113	370.615388	6.463629
5.628165	373.312099	6.468634
5.856326	374.255402	6.473638
5.560330	383.033852	6.478643
5.744283	392.652475	6.483648
5.892172	396.057124	6.488653
6.103176	397.825078	6.493658
6.128969	391.233541	6.498662
6.001002	393.304353	6.503667
6.072939	375.102925	6.508672
5.883934	373.115798	6.513677
5.589897	377.971419	6.518682
5.939003	372.176981	6.523686
5.754839	383.564877	6.528691
6.106109	390.104877	6.533696
6.199329	386.174623	6.538701
5.625711	374.629726	6.543706
5.975472	357.647188	6.548710
5.890289	375.822891	6.553715
5.798034	368.072414	6.558720
5.842504	376.513127	6.563725
6.078709	372.277482	6.568730
5.825417	375.296577	6.573734
5.620278	374.815452	6.578739
5.718995	388.682519	6.583744
6.253815	393.674348	6.588749
5.829340	390.655112	6.593754
6.090513	399.249249	6.598758
5.685247	391.341138	6.603763
5.962881	385.189430	6.608768
5.735721	385.893068	6.613773
5.765122	394.542967	6.618778
6.261656	387.447931	6.623782
5.778761	390.742243	6.628787
6.241292	384.825268	6.633792
5.833268	368.670191	6.638797
6.036926	365.000299	6.643802
6.131206	353.728124	6.648806
5.729776	371.231846	6.653811
5.903563	355.789718	6.658816
6.002355	361.257989	6.663821
5.164006	362.114031	6.668826
5.894930	362.144838	6.673830
5.945117	382.314134	6.678835
6.469659	381.849654	6.683840
6.156144	372.883979	6.688845
5.551509	363.411179	6.693850
5.870881	358.379642	6.698854
5.721371	366.648384	6.703859
5.800975	361.363261	6.708864
5.895690	377.470195	6.713869
6.128423	378.495122	6.718874
6.213477	376.742101	6.723878
5.794723	382.260393	6.728883
5.850606	370.859688	6.733888
6.001297	370.337419	6.738893
5.770988	371.351359	6.743898
6.121275	358.033348	6.748902
5.866959	358.143413	6.753907
6.130826	367.435282	6.758912
6.153416	366.013714	6.763917
5.952610	363.746775	6.768922
5.934765	362.415550	6.773926
5.934309	366.600321	6.778931
5.875921	372.215920	6.783936
5.756253	377.644137	6.788941
5.503486	371.903882	6.793946
5.794626	367.591284	6.798950
6.035098	371.865481	6.803955
5.954158	367.363784	6.808960
5.816262	365.043928	6.813965
5.870534	365.960424	6.818970
6.267759	362.452699	6.823974
6.260894	366.152348	6.828979
6.101260	359.808514	6.833984
6.222480	365.068959	6.838989
6.109793	371.708612	6.843994
6.248196	371.326099	6.848998
6.039760	366.918577	6.854003
6.023364	362.755165	6.859008
6.084305	350.381868	6.864013
5.653654	336.648447	6.869018
5.600830	332.559728	6.874022
5.686781	356.528370	6.879027
5.768741	350.860665	6.884032
6.009755	348.896003	6.889037
5.754500	365.086707	6.894042
6.007328	360.197676	6.899046
6.043527	370.336849	6.904051
5.912605	365.734890	6.909056
6.350409	361.599118	6.914061
5.970224	349.779675	6.919066
5.955808	336.563982	6.924070
5.646065	341.638442	6.929075
5.814154	342.155903	6.934080
5.861872	347.905495	6.939085
5.954888	355.116407	6.944090
6.264549	343.453778	6.949094
5.302807	338.823484	6.954099
5.783660	354.529964	6.959104
6.048680	356.339006	6.964109
5.976967	350.919760	6.969114
6.340272	351.012700	6.974118
5.440032	341.454001	6.979123
5.848259	341.984262	6.984128
6.262333	342.259812	6.989133
5.804492	340.091787	6.994138
5.669695	334.987525	6.999142
6.027023	347.960803	7.004147
5.927019	348.447098	7.009152
6.068986	351.585553	7.014157
5.696330	338.237173	7.019162
6.063518	340.729890	7.024166
5.695603	344.412545	7.029171
5.884393	357.534933	7.034176
6.093380	357.261216	7.039181
5.807448	353.341341	7.044186
6.050513	364.837681	7.049190
5.672470	344.995896	7.054195
5.954150	352.148990	7.059200
6.073485	344.334947	7.064205
5.799057	348.155663	7.069210
5.592687	334.564635	7.074214
5.868691	356.053602	7.079219
6.122261	347.810118	7.084224
6.191892	346.166593	7.089229
5.923793	355.689026	7.094234
5.862643	325.662441	7.099238
5.759906	341.760138	7.104243
5.631117	334.245488	7.109248
5.999153	343.099948	7.114253
6.100297	354.882753	7.119258
5.900447	338.421801	7.124262
5.432195	353.941114	7.129267
5.842044	359.024124	7.134272
6.122437	360.162521	7.139277
5.521360	372.061784	7.144282
5.896308	367.576400	7.149286
5.814969	366.546607	7.154291
5.835958	370.100673	7.159296
5.838047	357.364666	7.164301
5.781466	367.890022	7.169306
6.065188	359.841723	7.174310
5.692891	365.066720	7.179315
5.966700	364.710961	7.184320
5.859091	363.657195	7.189325
5.791857	370.249282	7.194330
5.966775	358.827730	7.199334
6.120708	371.237372	7.204339
5.913021	361.872215	7.209344
5.899035	362.660391	7.214349
5.681970	354.758884	7.219354
6.166943	359.446099	7.224358
6.026454	354.362799	7.229363
5.706439	366.080646	7.234368
5.965299	355.556716	7.239373
5.639787	361.583361	7.244378
5.583320	356.005618	7.249382
5.603896	370.698909	7.254387
5.623951	368.337755	7.259392
5.707278	373.024560	7.264397
5.711217	369.275005	7.269402
5.683097	364.077731	7.274406
5.879073	361.852164	7.279411
5.879547	350.607531	7.284416
5.926702	355.298137	7.289421
5.745066	365.724585	7.294426
5.943114	353.029796	7.299430
5.769214	356.514055	7.304435
5.621733	363.301127	7.309440
6.120499	383.092033	7.314445
6.189767	375.624839	7.319450
5.916184	368.924245	7.324454
5.683252	371.046142	7.329459
5.877125	357.349783	7.334464
5.905598	355.298009	7.339469
5.814467	374.202387	7.344474
6.016126	366.233648	7.349478
5.698811	374.496682	7.354483
5.910705	381.606568	7.359488
6.129889	382.133247	7.364493
5.702860	381.391045	7.369498
6.166137	377.211399	7.374502
5.868360	373.076530	7.379507
5.829730	369.147352	7.384512
5.791449	365.007189	7.389517
5.577544	380.674902	7.394522
6.283251	393.108311	7.399526
5.856333	378.497667	7.404531
5.904970	375.844400	7.409536
5.576080	371.059690	7.414541
6.016862	379.934410	7.419546
6.029744	386.849289	7.424550
5.801517	384.389565	7.429555
6.145122	389.480178	7.434560
6.258924	369.339046	7.439565
5.783615	366.555226	7.444570
5.857097	356.526901	7.449574
5.546639	367.145612	7.454579
5.404657	367.831225	7.459584
5.956847	389.198235	7.464589
6.064224	401.413842	7.469594
5.879646	395.904610	7.474598
5.613220	404.168227	7.479603
6.154010	400.751606	7.484608
6.186778	398.246379	7.489613
5.912699	392.616582	7.494618
6.290635	381.373773	7.499622
6.061945	366.553784	7.504627
5.844808	372.142442	7.509632
6.100295	363.226483	7.514637
5.949079	370.573264	7.519642
6.030886	358.765467	7.524646
6.153568	366.907538	7.529651
5.787209	375.243001	7.534656
5.932505	369.513619	7.539661
5.623552	373.709715	7.544666
6.055363	367.820613	7.549670
5.981470	372.395280	7.554675
6.034966	369.390091	7.559680
6.054943	358.864201	7.564685
5.754528	362.869165	7.569690
6.125513	364.706572	7.574694
5.826183	359.738311	7.579699
5.882443	363.059636	7.584704
5.858523	360.738406	7.589709
5.547821	358.027126	7.594714
5.978163	355.318675	7.599718
6.017715	354.323166	7.604723
5.846712	369.030555	7.609728
5.813902	355.007320	7.614733
5.553111	367.159238	7.619738
6.199568	362.311507	7.624742
6.065316	366.896147	7.629747
6.105628	360.288707	7.634752
6.096802	377.791780	7.639757
5.842984	363.448119	7.644762
6.175835	367.944121	7.649766
5.869923	367.851588	7.654771
5.769393	362.125246	7.659776
6.011723	360.716692	7.664781
6.020232	363.425356	7.669786
5.739878	360.929953	7.674790
5.824851	362.804464	7.679795
5.983293	344.484890	7.684800
5.971301	353.085076	7.689805
5.718335	365.806726	7.694810
5.968215	353.277204	7.699814
5.966549	355.471573	7.704819
6.101398	353.463880	7.709824
6.020976	350.087383	7.714829
5.711398	363.514905	7.719834
6.027875	357.455446	7.724838
5.980689	357.566995	7.729843
5.693646	356.604741	7.734848
5.959116	362.192664	7.739853
5.887993	358.746851	7.744858
5.672804	362.341623	7.749862
5.732374	371.161146	7.754867
5.473843	363.640299	7.759872
5.867991	354.277994	7.764877
5.750901	357.393556	7.769882
5.868423	351.371518	7.774886
5.829887	363.866631	7.779891
5.657116	355.763153	7.784896
5.908175	360.564300	7.789901
5.763938	368.489635	7.794906
6.137166	355.141592	7.799910
5.781706	360.980904	7.804915
5.780722	359.911096	7.809920
6.103938	368.493088	7.814925
5.832222	368.521283	7.819930
6.010478	358.414573	7.824934
5.728540	358.638812	7.829939
5.697458	372.904480	7.834944
6.169707	364.051453	7.839949
5.902257	368.768306	7.844954
5.716517	358.648942	7.849958
5.492744	371.426643	7.854963
5.738892	370.286890	7.859968
6.205384	372.068656	7.864973
6.225690	376.657551	7.869978
6.193799	364.746402	7.874982
5.852140	363.695306	7.879987
6.022139	356.860045	7.884992
6.200983	361.474333	7.889997
6.107983	358.995323	7.895002
6.134106	342.025245	7.900006
5.755039	354.640656	7.905011
5.723830	362.725187	7.910016
5.957211	353.529149	7.915021
5.724318	350.492466	7.920026
5.838291	360.680736	7.925030
5.884568	363.833034	7.930035
5.730104	360.809532	7.935040
5.721461	362.741641	7.940045
5.690123	371.021735	7.945050
5.581724	362.244049	7.950054
5.899137	358.589297	7.955059
5.439999	376.867251	7.960064
5.846086	365.664690	7.965069
5.973212	382.049714	7.970074
6.021882	392.728961	7.975078
6.071649	374.027158	7.980083
5.893257	364.562447	7.985088
5.641200	371.127660	7.990093
5.635001	376.684913	7.995098
6.184944	387.118630	8.000102
6.222381	387.735821	8.005107
5.942800	378.015630	8.010112
6.056163	366.744535	8.015130
5.992265	363.757044	8.020147
6.075242	356.243142	8.025165
6.170342	353.561888	8.030182
6.088291	359.010726	8.035200
6.170995	339.198293	8.040218
6.222849	348.650654	8.045235
6.224947	345.457810	8.050253
6.106783	359.223525	8.055270
5.972101	354.796157	8.060288
5.917561	365.596451	8.065306
5.928780	365.110111	8.070323
5.933844	354.247169	8.075341
6.177880	355.992464	8.080358
5.906750	354.593729	8.085376
6.401585	347.216647	8.090394
6.050864	342.466496	8.095411
5.673550	326.525590	8.100429
5.957534	337.977747	8.105446
5.963850	351.912313	8.110464
5.942761	348.259025	8.115482
5.488381	354.697649	8.120499
5.517671	349.077378	8.125517
5.584859	357.859629	8.130534
5.591741	356.000270	8.135552
6.018584	355.982537	8.140570
5.793276	356.978301	8.145587
6.137323	352.428914	8.150605
6.330781	361.209784	8.155622
5.892855	360.196218	8.160640
5.968073	352.998300	8.165658
5.622148	351.151586	8.170675
5.997917	363.051393	8.175693
6.090396	376.099772	8.180710
6.235546	386.887253	8.185728
6.318905	387.693355	8.190746
6.192968	375.100234	8.195763
6.073005	364.260997	8.200781
6.052022	368.708904	8.205798
5.806806	357.283407	8.210816
6.310007	370.600648	8.215834
5.868650	386.226322	8.220851
6.275946	390.083680	8.225869
6.095058	380.981811	8.230886
6.097577	394.631470	8.235904
6.400929	371.654813	8.240922
5.958442	374.373530	8.245939
5.925051	362.981710	8.250957
5.957832	385.759356	8.255974
5.905354	386.760312	8.260992
6.386626	391.036165	8.266010
6.211655	400.934721	8.271027
6.140909	401.331338	8.276045
6.356427	392.897073	8.281062
6.249076	389.642600	8.286080
6.175144	389.146911	8.291098
5.960513	401.295960	8.296115
6.137216	388.111584	8.301133
6.248521	385.347249	8.306150
6.168466	395.398880	8.311168
6.363090	395.104036	8.316186
6.186420	383.741390	8.321203
6.331571	383.087178	8.326221
6.503119	383.751467	8.331238
6.168145	390.734826	8.336256
6.328612	385.623564	8.341274
6.329041	377.651538	8.346291
5.736840	362.184996	8.351309
6.145969	378.837098	8.356326
5.797664	401.571173	8.361344
6.261195	393.954311	8.366362
6.309064	394.506390	8.371379
6.423174	398.298445	8.376397
6.480784	391.401292	8.381414
6.365057	395.754453	8.386432
6.445897	397.835225	8.391450
6.459750	391.133652	8.396467
6.286851	400.752984	8.401485
6.472084	394.348022	8.406502
6.199931	403.396081	8.411520
6.221137	390.956547	8.416538
6.122560	391.570713	8.421555
5.976579	393.457519	8.426573
6.378886	382.628494	8.431590
6.064403	392.570569	8.436608
6.077168	384.657315	8.441626
6.001792	391.750892	8.446643
6.026532	398.428597	8.451661
6.185312	399.051699	8.456678
5.835094	402.437910	8.461696
6.280195	413.847555	8.466714
6.580641	422.923316	8.471731
6.470562	404.735355	8.476749
6.581874	402.914626	8.481766
6.006088	395.307841	8.486784
6.326318	395.700857	8.491802
6.281738	408.888624	8.496819
6.388095	417.752410	8.501837
6.803127	422.921524	8.506854
6.419649	415.046283	8.511872
6.557652	399.161942	8.516890
6.683826	398.021889	8.521907
6.489477	397.873495	8.526925
6.378026	387.802760	8.531942
6.450778	393.558047	8.536960
6.479461	392.035760	8.541978
6.388593	387.325902	8.546995
6.289911	394.454527	8.552013
6.465881	395.410055	8.557030
6.124986	386.577490	8.562048
6.571212	412.172588	8.567066
6.731400	419.880464	8.572083
6.560440	415.756259	8.577101
6.484551	386.443332	8.582119
6.693720	400.658331	8.587136
6.698979	395.220720	8.592154
6.592825	393.648388	8.597171
6.471718	402.339563	8.602189
6.476739	395.354465	8.607207
6.248584	408.926042	8.612224
6.471402	402.778986	8.617242
6.515814	395.222334	8.622259
6.307042	409.935754	8.627277
6.877241	410.409582	8.632295
6.620458	420.957076	8.637312
6.799217	388.768077	8.642330
6.540962	396.144190	8.647347
6.329656	396.581553	8.652365
6.848733	386.164539	8.657383
6.342129	394.183049	8.662400
6.337328	394.452355	8.667418
6.802688	405.995431	8.672435
6.453422	417.152181	8.677453
6.738059	417.131183	8.682471
6.510423	422.924709	8.687488
6.620565	413.660180	8.692506
6.831707	412.492897	8.697523
6.478296	420.396161	8.702541
6.818839	412.577120	8.707559
6.417169	416.056367	8.712576
6.567036	412.705553	8.717594
6.712043	422.758092	8.722611
6.666749	425.269178	8.727629
6.918705	409.614173	8.732647
6.401565	417.706272	8.737664
6.220799	415.409112	8.742682
6.466502	413.359521	8.747699
6.769826	426.656900	8.752717
7.184075	416.487066	8.757735
6.983908	421.020986	8.762752
6.871392	422.097012	8.767770
6.826913	410.661131	8.772787
6.367246	409.535036	8.777805
6.652101	411.725569	8.782823
6.637885	418.632807	8.787840
6.683280	416.260385	8.792858
7.147350	415.139868	8.797875
6.867356	422.400712	8.802893
6.777859	412.117811	8.807911
6.632743	405.701507	8.812928
6.603199	418.352552	8.817946
6.789435	410.428724	8.822963
6.517690	417.904696	8.827981
6.562986	414.411057	8.832999
6.778787	414.446209	8.838016
6.790167	414.035417	8.843034
6.970293	412.509061	8.848051
6.614136	424.255224	8.853069
6.583981	404.780784	8.858087
6.617021	414.454557	8.863104
6.734983	423.851658	8.868122
6.878798	417.912003	8.873139
6.852875	414.907992	8.878157
6.980072	423.342931	8.883175
6.820975	422.219120	8.888192
6.652810	427.207997	8.893210
6.943267	426.631127	8.898227
6.714852	423.434442	8.903245
6.543107	425.266269	8.908263
6.537158	427.592837	8.913280
6.508333	423.901349	8.918298
7.048237	419.112727	8.923315
6.712901	423.465680	8.928333
6.912542	441.311985	8.933351
6.972291	449.924587	8.938368
7.084142	446.970424	8.943386
6.803733	439.288332	8.948403
6.685448	448.786584	8.953421
6.881546	446.578881	8.958439
7.025460	459.238885	8.963456
6.862040	460.851273	8.968474
7.246644	453.649119	8.973491
7.024274	455.912560	8.978509
7.332022	450.112992	8.983527
7.023451	426.942556	8.988544
7.302165	422.548110	8.993562
6.949803	425.046864	8.998579
6.821099	423.002464	9.003597
6.698962	420.223563	9.008615
6.427404	435.359899	9.013632
7.114549	437.886433	9.018650
7.172461	445.786682	9.023667
7.128502	453.903535	9.028685
7.329773	450.848193	9.033703
6.988070	442.918012	9.038720
6.884518	423.738102	9.043738
7.005792	430.024548	9.048755
6.533639	432.242668	9.053773
6.934591	444.126469	9.058791
6.939906	450.360251	9.063808
7.048794	450.624350	9.068826
7.086960	449.988602	9.073843
7.071605	465.296268	9.078861
7.255246	460.033346	9.083879
7.099122	455.675621	9.088896
7.010985	456.996981	9.093914
6.940033	458.975902	9.098931
7.028373	455.413932	9.103949
7.079107	453.215292	9.108967
7.022472	451.934515	9.113984
7.010879	455.185067	9.119002
6.926442	458.527564	9.124019
7.021722	457.798536	9.129037
7.076794	448.391050	9.134055
7.340355	456.787530	9.139072
7.407752	459.533885	9.144090
7.020067	451.355640	9.149107
7.292789	456.358656	9.154125
7.273311	451.534638	9.159143
7.330718	463.378299	9.164160
7.005672	460.401472	9.169178
7.495250	453.051582	9.174195
7.058139	454.928152	9.179213
7.071856	453.200303	9.184231
7.139373	456.400092	9.189248
7.385349	463.154726	9.194266
7.340509	452.901516	9.199283
7.279850	465.345482	9.204301
6.989962	458.675378	9.209319
7.052808	460.372003	9.214336
7.009395	472.744929	9.219354
6.992452	464.399031	9.224371
6.852240	462.627932	9.229389
7.183503	460.606804	9.234407
7.575278	475.910079	9.239424
7.178216	468.910015	9.244442
7.382077	467.969675	9.249459
7.275304	476.869406	9.254477
7.349736	474.040493	9.259495
7.108671	475.391949	9.264512
7.075614	490.824392	9.269530
7.687738	498.015974	9.274547
7.160070	500.126371	9.279565
7.550573	489.707411	9.284583
7.471292	483.966674	9.289600
7.376244	478.913845	9.294618
7.458357	461.588664	9.299635
7.218838	468.540538	9.304653
7.022968	458.936965	9.309671
7.289479	478.753468	9.314688
7.533952	468.717836	9.319706
7.512959	474.769398	9.324723
7.546517	491.921696	9.329741
7.385769	492.028131	9.334759
7.355632	492.548035	9.339776
7.401005	499.107534	9.344794
7.806681	486.358370	9.349811
7.379785	477.523728	9.354829
7.375033	472.317521	9.359847
7.433367	466.547751	9.364864
7.279875	479.495852	9.369882
7.474083	490.002910	9.374899
7.624749	492.752337	9.379917
7.604237	479.961329	9.384935
7.564497	468.971484	9.389952
6.886230	476.800339	9.394970
7.608074	474.744872	9.399987
7.455955	490.378058	9.405005
7.427139	504.787571	9.410023
7.772753	504.861299	9.415040
7.663648	494.093390	9.420058
7.610216	493.679727	9.425075
7.397619	480.498891	9.430093
7.585574	495.714042	9.435111
7.678272	496.354859	9.440128
7.329268	489.633598	9.445146
7.882532	487.806443	9.450163
7.883425	480.402779	9.455181
7.344523	483.959729	9.460199
7.627939	474.031515	9.465216
7.291295	462.884875	9.470234
7.523303	482.859615	9.475251
7.499115	498.519197	9.480269
7.648232	495.035345	9.485287
7.756305	489.859789	9.490304
7.291760	502.159253	9.495322
7.714612	489.761608	9.500339
7.670646	491.849634	9.505357
7.551881	501.757761	9.510375
7.618570	493.182320	9.515392
7.478813	495.170649	9.520410
7.635296	490.695518	9.525427
7.666617	501.702540	9.530445
7.698476	498.864323	9.535463
7.876314	490.954143	9.540480
7.575694	506.900806	9.545498
7.765271	487.878239	9.550515
7.602656	493.989328	9.555533
7.637588	483.635432	9.560551
7.824611	489.140518	9.565568
7.623961	493.769403	9.570586
7.794554	485.713207	9.575603
7.613907	496.582455	9.580621
7.669220	493.801768	9.585639
7.773790	488.213682	9.590656
7.698000	494.344865	9.595674
7.644256	480.737755	9.600691
7.478964	489.634274	9.605709
7.553457	495.930250	9.610727
7.677654	487.935942	9.615744
7.675455	501.424992	9.620762
7.855581	492.272546	9.625779
7.974126	489.981215	9.630797
7.427711	491.257864	9.635815
7.736431	480.491570	9.640832
7.157878	490.735860	9.645850
7.781357	504.558534	9.650867
8.176691	519.238550	9.655885
7.706283	509.592438	9.660903
7.982761	506.363566	9.665920
7.814687	509.623261	9.670938
7.850783	512.760059	9.675955
7.855138	509.325713	9.680973
8.017051	526.816217	9.685991
8.199096	512.214490	9.691008
7.687073	500.469565	9.696026
7.771728	491.368324	9.701043
7.859372	499.349793	9.706061
8.091756	505.725762	9.711079
7.982755	493.846732	9.716096
7.772339	484.988020	9.721114
7.751376	499.893674	9.726131
7.902552	514.901282	9.731149
8.018610	522.416640	9.736167
8.341894	512.149888	9.741184
7.896264	508.181167	9.746202
7.703092	494.805019	9.751219
7.967752	494.545933	9.756237
7.920903	506.086839	9.761255
8.335445	504.694634	9.766272
7.976346	498.965201	9.771290
7.671988	499.281554	9.776307
8.064415	506.607066	9.781325
7.863794	516.276909	9.786343
8.233313	510.322552	9.791360
8.191443	523.854489	9.796378
8.045731	519.609866	9.801395
7.955981	509.708757	9.806413
7.915194	527.001112	9.811431
8.217067	521.208000	9.816448
7.874961	526.914694	9.821466
8.044794	515.243555	9.826483
7.912079	524.358978	9.831501
7.852291	530.714160	9.836519
8.226959	519.184231	9.841536
8.029412	519.428907	9.846554
8.051746	526.255265	9.851571
8.259160	519.298660	9.856589
7.988651	532.206902	9.861607
7.743909	517.834036	9.866624
8.045942	528.958810	9.871642
7.933565	516.792875	9.876659
8.011267	521.723240	9.881677
7.844505	524.902323	9.886695
7.976576	513.559017	9.891712
8.094281	520.802795	9.896730
8.000908	517.662105	9.901747
8.477491	527.463398	9.906765
8.423693	527.285379	9.911783
8.443526	520.741195	9.916800
8.056976	525.776330	9.921818
7.905800	522.500730	9.926835
8.070078	521.152638	9.931853
8.306591	544.790478	9.936871
8.139991	525.795334	9.941888
8.234491	532.922209	9.946906
8.375876	541.155300	9.951923
8.305555	532.643613	9.956941
8.204804	543.223070	9.961959
8.467738	529.054232	9.966976
8.676480	525.170241	9.971994
8.576362	530.341766	9.977011
8.584646	507.606742	9.982029
8.322332	516.043516	9.987047
8.504880	513.709622	9.992064
8.431974	516.106510	9.997082
8.433153	516.849640	10.002099
8.490092	516.055404	10.007117
8.514856	527.145107	10.012135
8.667887	523.771704	10.017152
8.439056	521.201422	10.022170
7.816133	517.311398	10.027187
8.295315	520.631026	10.032205
8.317681	517.556625	10.037223
8.304150	510.714868	10.042240
8.305469	523.958226	10.047258
8.251275	515.164214	10.052275
8.413444	524.004274	10.057293
7.897734	521.658042	10.062311
8.063605	509.950560	10.067328
8.092009	521.882015	10.072346
8.583476	536.146434	10.077363
8.677638	538.700621	10.082381
8.188148	534.763152	10.087399
8.396279	530.215805	10.092416
8.374766	534.513974	10.097434
8.327420	542.992880	10.102451
8.443491	544.451726	10.107469
8.372555	547.358530	10.112487
8.459278	532.582907	10.117504
8.463700	546.208375	10.122522
8.271595	540.432140	10.127539
8.205183	551.421203	10.132557
8.217336	554.605560	10.137575
8.438745	542.016108	10.142592
8.517061	545.698389	10.147610
8.366457	547.277966	10.152627
8.622667	536.304998	10.157645
8.504896	534.535593	10.162663
8.784813	532.454353	10.167680
8.723568	538.793543	10.172698
8.356434	544.918966	10.177715
8.843378	538.387327	10.182733
8.744302	548.971727	10.187751
8.707458	545.034633	10.192768
8.823230	545.675674	10.197786
8.475392	537.184458	10.202803
8.776668	533.250829	10.207821
8.412225	540.383389	10.212839
8.478887	543.607447	10.217856
8.622498	543.383618	10.222874
8.614079	535.467883	10.227891
8.851108	545.613049	10.232909
8.427032	552.524116	10.237927
8.559205	550.561071	10.242944
8.649657	566.047377	10.247962
8.642706	573.069602	10.252979
8.944872	572.556135	10.257997
8.970343	571.134146	10.263015
8.905223	554.423631	10.268032
8.903721	549.058526	10.273050
8.790773	532.354365	10.278067
8.555696	532.573261	10.283085
8.448892	549.781491	10.288103
8.737279	558.703350	10.293120
8.656610	567.776543	10.298138
8.543219	583.524561	10.303155
9.077765	584.320960	10.308173
8.596669	581.647011	10.313191
8.681681	585.989980	10.318208
9.121627	582.975568	10.323226
8.769133	578.994290	10.328243
8.875962	581.743597	10.333261
8.399125	577.384913	10.338279
8.780682	584.020853	10.343296
9.010135	569.733322	10.348314
8.839726	578.754632	10.353331
8.938434	562.980730	10.358349
9.055324	579.406891	10.363367
8.840083	574.677674	10.368384
9.052843	584.093157	10.373402
8.553648	578.332231	10.378419
9.025893	575.639880	10.383437
8.782322	571.884652	10.388455
8.807270	587.781040	10.393472
8.742630	580.831776	10.398490
9.058422	579.375190	10.403507
8.965592	585.262913	10.408525
9.026710	580.044505	10.413543
9.011425	572.680964	10.418560
9.357866	570.552708	10.423578
9.047569	577.639533	10.428595
8.920461	568.406345	10.433613
8.918032	571.119485	10.438631
8.661852	570.260872	10.443648
9.114443	575.737945	10.448666
8.842015	574.071443	10.453683
8.991522	577.307993	10.458701
9.008029	582.794155	10.463719
8.965364	581.321134	10.468736
9.114579	573.559217	10.473754
8.850698	583.731786	10.478771
9.025138	581.290285	10.483789
9.105049	581.285014	10.488807
8.735503	583.436699	10.493824
8.909886	575.996150	10.498842
8.908959	603.766151	10.503859
9.159917	603.612261	10.508877
9.084601	615.698404	10.513895
9.455449	607.735798	10.518912
9.183556	608.436577	10.523930
9.106460	616.544033	10.528947
9.292407	610.334005	10.533965
9.141764	618.009015	10.538983
9.318812	614.158679	10.544000
9.229277	603.612516	10.549018
9.069688	612.763824	10.554035
9.416698	605.007385	10.559053
9.027462	596.311699	10.564071
8.806910	602.172021	10.569088
9.298688	602.937701	10.574106
9.023804	619.294619	10.579123
9.245875	609.199618	10.584141
9.518878	615.053760	10.589159
9.565620	613.184043	10.594176
9.600266	603.263792	10.599194
9.359448	606.776527	10.604211
9.317936	594.023042	10.609229
9.231662	601.735822	10.614247
9.188910	613.742383	10.619264
9.354362	618.880579	10.624282
9.445155	618.595903	10.629299
9.190430	609.175552	10.634317
9.432709	613.591438	10.639335
9.110252	616.219605	10.644352
9.191252	605.984466	10.649370
8.966677	606.179880	10.654387
9.189529	618.419960	10.659405
9.229811	612.036501	10.664423
9.151598	611.667671	10.669440
9.247638	606.929120	10.674458
8.987526	611.074356	10.679475
9.413648	611.526636	10.684493
9.119881	607.869639	10.689511
8.985566	622.903474	10.694528
9.374999	638.901461	10.699546
9.330876	641.226399	10.704563
9.464051	631.072565	10.709581
9.538974	647.206380	10.714599
9.555586	644.269099	10.719616
9.840427	647.125589	10.724634
9.392689	651.110244	10.729651
9.589566	640.417431	10.734669
9.649071	647.177475	10.739687
9.390540	643.523010	10.744704
9.851465	639.234291	10.749722
9.709952	648.966285	10.754739
9.913486	618.333252	10.759757
9.674420	621.734403	10.764775
9.469858	607.497995	10.769792
9.783891	612.840627	10.774810
9.025347	608.171566	10.779827
9.667761	603.486298	10.784845
9.326060	610.799842	10.789863
9.574561	637.570397	10.794880
9.935492	642.092840	10.799898
9.637146	632.976971	10.804915
9.430100	622.821406	10.809933
9.119011	633.332555	10.814951
9.418964	652.699251	10.819968
9.811102	648.710033	10.824986
9.324392	646.275933	10.830003
9.652788	660.047630	10.835021
9.500086	652.090830	10.840039
9.419159	648.524412	10.845056
9.811569	642.534732	10.850074
9.429510	650.611911	10.855091
9.472623	646.295700	10.860109
9.567685	651.619720	10.865127
9.614830	650.093372	10.870144
9.729263	640.051370	10.875162
9.763628	641.044289	10.880179
9.739987	635.534906	10.885197
10.050554	645.814416	10.890215
9.803033	653.760918	10.895232
9.747808	643.985883	10.900250
9.565000	652.723412	10.905267
9.910863	661.643608	10.910285
9.544113	660.827274	10.915303
9.920577	666.920295	10.920320
10.073592	668.975202	10.925338
9.811797	662.955661	10.930355
9.811437	646.961376	10.935373
9.883890	657.939867	10.940391
9.777659	668.876845	10.945408
9.873026	667.700926	10.950426
9.777246	678.374518	10.955443
9.848761	688.866562	10.960461
9.951383	677.650913	10.965479
9.687411	689.868175	10.970496
9.951331	692.006411	10.975514
9.790840	681.547891	10.980531
9.954092	683.346529	10.985549
10.296984	680.242939	10.990567
9.666761	675.960648	10.995584
9.821193	684.449388	11.000602
10.363067	678.281576	11.005619
10.284235	673.448010	11.010637
10.390647	676.193959	11.015655
9.978822	679.156238	11.020672
10.278803	679.095408	11.025690
10.165003	667.494940	11.030707
9.723842	656.428117	11.035725
10.155209	655.930297	11.040743
9.729370	680.125853	11.045760
9.744249	672.823212	11.050778
9.848759	680.358564	11.055795
9.992891	669.811823	11.060813
10.322617	665.045854	11.065831
9.785980	672.468203	11.070848
10.303004	675.985511	11.075866
10.606562	677.816266	11.080883
9.956173	678.343715	11.085901
10.243207	678.513626	11.090919
9.904674	681.661394	11.095936
10.008782	679.953122	11.100954
10.006473	676.130345	11.105971
9.957851	682.092477	11.110989
10.305108	677.143030	11.116007
10.107498	683.833889	11.121024
10.284020	675.061783	11.126042
9.972014	674.247719	11.131059
9.906802	681.827948	11.136077
10.215039	672.119873	11.141095
10.026239	673.725948	11.146112
10.172648	670.853417	11.151130
10.174501	680.745760	11.156147
9.992743	673.588980	11.161165
10.131381	679.630184	11.166183
10.514909	698.541967	11.171200
10.286640	704.967477	11.176218
10.626188	710.745513	11.181235
10.484473	690.271713	11.186253
10.256533	688.572948	11.191271
9.924409	682.962095	11.196288
10.382962	689.262877	11.201306
10.695552	699.337893	11.206323
10.324738	698.320002	11.211341
10.621335	675.739015	11.216359
10.283139	688.544619	11.221376
10.275384	671.042257	11.226394
10.295483	681.256034	11.231411
10.219387	693.568704	11.236429
10.637169	698.082950	11.241447
10.508217	712.934622	11.246464
10.390668	703.517030	11.251482
10.430618	710.986211	11.256499
10.421862	717.882249	11.261517
10.894398	706.177964	11.266535
10.573875	701.421824	11.271552
10.406520	682.612700	11.276570
10.458854	683.710605	11.281587
10.269765	682.260395	11.286605
10.705425	694.008953	11.291623
10.491581	698.601701	11.296640
10.922695	706.117042	11.301658
10.606023	686.308462	11.306675
10.247822	681.754091	11.311693
10.610803	686.986020	11.316711
10.447996	703.872340	11.321728
10.863944	703.220795	11.326746
10.629671	693.000207	11.331763
10.388266	693.587309	11.336781
10.902974	701.886917	11.341799
10.295375	696.692876	11.346816
10.581513	710.933625	11.351834
10.427114	711.902537	11.356851
10.403883	721.662266	11.361869
10.453122	715.057245	11.366887
10.351297	721.859630	11.371904
10.359182	717.209124	11.376922
10.432935	710.963374	11.381939
10.556209	713.268630	11.386957
10.560304	702.283971	11.391975
10.489251	716.490956	11.396992
10.406355	718.131395	11.402010
10.436969	726.079008	11.407027
10.178450	739.884002	11.412045
10.549391	734.644355	11.417063
10.310681	738.775165	11.422080
10.929952	735.156780	11.427098
10.824605	737.443238	11.432115
10.714337	753.224568	11.437133
11.147649	740.566576	11.442151
10.922548	742.509897	11.447168
11.151969	751.475761	11.452186
11.205191	749.640580	11.457203
11.056128	740.934938	11.462221
11.299615	732.083143	11.467239
10.882244	735.817176	11.472256
11.013107	730.439186	11.477274
11.052713	735.251331	11.482291
10.789210	734.041128	11.487309
11.342799	736.825373	11.492327
11.056315	726.257943	11.497344
10.787356	713.610635	11.502362
10.565645	717.410146	11.507379
10.671978	735.849176	11.512397
11.138263	737.113280	11.517415
10.771928	740.112631	11.522432
10.657329	736.077137	11.527450
10.892149	737.815045	11.532467
10.803468	748.537701	11.537485
10.839378	725.896985	11.542503
10.788987	740.261376	11.547520
10.952165	740.265962	11.552538
11.099725	729.612825	11.557555
10.753786	740.481121	11.562573
11.175123	727.852377	11.567591
11.003105	750.430296	11.572608
10.831549	749.109441	11.577626
11.070280	738.883181	11.582643
10.677339	746.599969	11.587661
10.724954	772.647203	11.592679
11.073314	780.647827	11.597696
11.271568	782.171841	11.602714
11.446899	778.066871	11.607731
11.203002	786.876176	11.612749
11.238400	770.731784	11.617767
11.227230	779.062937	11.622784
11.109863	771.275401	11.627802
11.379333	774.541766	11.632819
11.429991	781.677281	11.637837
11.132809	770.158409	11.642855
11.315640	758.184105	11.647872
11.602457	760.593420	11.652890
11.362544	742.073133	11.657907
10.902753	745.245087	11.662925
11.546760	745.468387	11.667943
11.131584	737.294040	11.672960
11.049485	742.175996	11.677978
11.582347	749.351569	11.682995
11.341337	757.917805	11.688013
11.530525	740.126564	11.693031
11.491344	735.281210	11.698048
11.279228	735.346046	11.703066
11.527541	738.253365	11.708083
11.145941	734.823314	11.713101
11.399291	722.470815	11.718119
11.700488	729.788681	11.723136
11.519212	741.603115	11.728154
11.379313	731.725306	11.733171
11.374846	745.789744	11.738189
11.294022	740.158891	11.743207
11.343486	730.988043	11.748224
11.042943	735.048179	11.753242
11.504771	750.056934	11.758259
11.403376	769.555447	11.763277
11.532375	770.498588	11.768295
11.707002	773.817037	11.773312
11.361351	788.696721	11.778330
11.744224	777.460369	11.783347
11.241283	773.547793	11.788365
11.417175	771.452222	11.793383
11.781381	774.834010	11.798400
11.514212	775.362392	11.803418
11.943390	762.614824	11.808435
11.583889	770.511695	11.813453
11.571939	760.637128	11.818471
11.584736	751.404425	11.823488
11.702926	759.190365	11.828506
11.589227	736.629761	11.833523
11.396394	758.010066	11.838541
11.519111	764.656780	11.843559
11.767763	771.817926	11.848576
11.598183	780.848960	11.853594
11.828323	773.790175	11.858611
11.824670	778.357361	11.863629
11.588731	777.016441	11.868647
11.754641	769.386977	11.873664
11.222110	772.806053	11.878682
11.523479	770.964599	11.883699
11.400949	772.588762	11.888717
11.541643	773.610862	11.893735
11.659977	770.689222	11.898752
11.780828	774.125495	11.903770
11.923006	768.767370	11.908787
11.158752	771.462179	11.913805
11.710582	772.781132	11.918823
11.902488	774.072574	11.923840
11.318381	786.671697	11.928858
11.724995	781.731893	11.933875
11.411821	794.124170	11.938893
11.826949	795.353531	11.943911
11.955990	799.094014	11.948928
11.612655	801.884592	11.953946
11.548743	797.007682	11.958963
11.669290	799.950889	11.963981
12.037306	798.829589	11.968999
12.195210	805.239346	11.974016
11.886872	801.086174	11.979034
12.231560	802.895091	11.984051
11.863952	805.912772	11.989069
11.837594	800.706285	11.994087
12.011461	801.998841	11.999104
12.094857	800.528485	12.004122
11.982405	799.595427	12.009139
11.550861	808.592124	12.014157
11.530069	812.114501	12.019175
11.942752	813.236314	12.024192
12.089053	810.210455	12.029210
12.229782	811.815620	12.034227
12.062717	801.144166	12.039245
12.246746	797.845094	12.044263
12.230499	797.659783	12.049280
12.139295	804.258319	12.054298
11.919359	797.419744	12.059315
12.190589	806.920959	12.064333
12.101884	806.874865	12.069351
12.158842	796.836256	12.074368
12.140425	805.977633	12.079386
12.460958	799.574353	12.084403
12.391447	803.497525	12.089421
12.160047	811.802700	12.094439
12.336164	802.058219	12.099456
11.632121	798.059304	12.104474
11.972222	804.593747	12.109491
12.172877	824.092994	12.114509
11.994753	838.124217	12.119527
12.429158	825.721541	12.124544
12.012377	834.595460	12.129562
12.624358	834.088354	12.134579
12.071119	839.956904	12.139597
12.306006	839.690333	12.144615
12.516466	841.155653	12.149632
12.115609	837.660662	12.154650
12.488623	837.869507	12.159667
12.584612	843.698373	12.164685
12.165913	840.222272	12.169703
12.555456	836.679521	12.174720
12.087858	843.094058	12.179738
12.481355	835.784763	12.184755
12.416185	834.402823	12.189773
12.115173	838.217043	12.194791
12.329368	839.109009	12.199808
12.485605	840.417964	12.204826
12.210272	836.152555	12.209843
12.703402	842.831085	12.214861
12.476473	840.548870	12.219879
12.608257	842.040772	12.224896
12.359499	846.452751	12.229914
12.277207	847.494682	12.234931
12.225206	845.864150	12.239949
12.179126	841.617339	12.244967
12.776400	844.644440	12.249984
12.375707	841.852648	12.255002
12.735944	833.451893	12.260019
12.685743	839.582428	12.265037
12.357713	834.435429	12.270055
12.716586	835.730183	12.275072
12.329790	852.880611	12.280090
12.505068	853.306452	12.285107
12.566136	871.366873	12.290125
12.697736	868.050962	12.295143
12.820626	870.941737	12.300160
12.599384	876.887106	12.305178
12.863031	873.725130	12.310195
12.752813	877.670400	12.315213
12.745810	868.563418	12.320231
12.882589	870.432386	12.325248
12.834872	854.046371	12.330266
12.685611	845.955853	12.335283
12.464672	850.487820	12.340301
12.632134	860.850463	12.345319
12.991296	864.567989	12.350336
12.839028	877.877479	12.355354
12.787884	870.815242	12.360371
12.686820	869.789565	12.365389
12.893700	876.998601	12.370407
13.090804	866.602984	12.375424
12.812205	869.827190	12.380442
12.684677	869.170785	12.385459
12.831182	869.333513	12.390477
12.883174	876.355584	12.395495
13.005031	865.556529	12.400512
12.901505	875.568954	12.405530
12.886245	867.848536	12.410547
12.317127	872.986382	12.415565
12.459713	884.490361	12.420583
12.942512	875.359508	12.425600
12.646833	873.316367	12.430618
12.638339	867.739546	12.435635
12.987523	884.033959	12.440653
12.738972	889.085571	12.445671
13.242945	907.624518	12.450688
12.931314	912.269703	12.455706
13.242275	901.302583	12.460723
13.058111	898.105177	12.465741
12.970136	904.896300	12.470759
13.049512	899.348246	12.475776
12.833172	907.718197	12.480794
12.758576	910.128710	12.485811
13.000892	898.924749	12.490829
12.601193	917.826399	12.495847
13.053938	909.422223	12.500864
12.693872	926.433987	12.505882
12.957861	904.957282	12.510899
13.153711	910.762880	12.515917
13.043714	929.944961	12.520935
13.067979	938.933522	12.525952
13.190699	931.911213	12.530970
13.340463	940.803654	12.535987
13.724442	942.518215	12.541005
13.347998	932.856602	12.546023
13.771849	911.662079	12.551040
13.342459	906.263642	12.556058
13.172612	903.936950	12.561075
13.309842	912.433678	12.566093
13.007276	907.158943	12.571111
13.106926	897.907568	12.576128
13.127980	920.023388	12.581146
13.371004	934.444571	12.586163
13.701802	930.606635	12.591181
13.517647	947.099669	12.596199
13.443616	930.855102	12.601216
13.324295	925.391442	12.606234
13.419922	928.274335	12.611251
13.595158	943.701839	12.616269
13.366754	942.380718	12.621287
13.582987	936.374279	12.626304
13.820881	921.066397	12.631322
13.520188	917.400924	12.636339
13.473240	914.152299	12.641357
13.052000	916.111720	12.646375
13.539425	924.764915	12.651392
13.456518	927.054974	12.656410
13.785704	932.016044	12.661427
13.932685	929.553933	12.666445
13.453798	922.873136	12.671463
13.713530	914.522701	12.676480
13.397929	909.291254	12.681498
13.646374	917.088813	12.686515
13.489373	926.763119	12.691533
13.413643	921.357010	12.696551
13.402928	929.633946	12.701568
13.592201	930.786293	12.706586
13.519204	937.765671	12.711603
13.512222	938.162196	12.716621
13.472682	941.167806	12.721639
13.523775	937.475485	12.726656
13.771234	935.006412	12.731674
13.304521	940.075987	12.736691
13.619522	926.166148	12.741709
13.439125	948.405247	12.746727
13.760225	954.813486	12.751744
13.655711	961.555801	12.756762
13.571403	979.634862	12.761779
13.838770	965.437239	12.766797
13.729584	971.947297	12.771815
13.819275	960.624640	12.776832
13.783406	969.192125	12.781850
13.889870	972.181878	12.786867
13.989115	965.769634	12.791885
13.652191	971.234828	12.796903
14.015504	962.945583	12.801920
14.091605	964.266611	12.806938
13.905929	964.629095	12.811955
14.089507	967.420504	12.816973
13.902697	970.453606	12.821991
13.819115	972.177734	12.827008
13.891221	968.428989	12.832026
13.849948	974.379293	12.837043
13.909666	962.067853	12.842061
13.889603	969.569710	12.847079
14.235650	960.428538	12.852096
13.954135	962.664037	12.857114
13.861016	972.800179	12.862131
14.063991	962.727490	12.867149
13.800099	970.679221	12.872167
14.264955	962.681216	12.877184
13.963163	976.571316	12.882202
13.670070	981.730697	12.887219
13.693618	984.813276	12.892237
13.685501	996.462107	12.897255
13.748662	995.142789	12.902272
14.393399	999.680140	12.907290
14.272819	1006.610533	12.912307
14.389563	1003.242530	12.917325
14.129623	1001.392842	12.922343
14.433560	998.210799	12.927360
14.399401	999.738407	12.932378
14.153996	1010.190244	12.937395
14.469435	1001.659520	12.942413
14.272157	1009.428637	12.947431
14.255651	997.558634	12.952448
14.550523	994.764051	12.957466
14.193999	1014.986029	12.962483
14.243373	997.370428	12.967501
14.269346	1000.274095	12.972519
14.420323	994.617340	12.977536
14.242033	998.725637	12.982554
14.139244	1007.940123	12.987571
14.546307	999.153157	12.992589
14.287452	1000.108744	12.997607
14.341612	999.396524	13.002624
14.392097	995.990465	13.007642
14.309529	999.672380	13.012659
14.634764	1000.453894	13.017677
14.341772	997.195330	13.022695
14.296501	998.397268	13.027712
14.665057	1021.257645	13.032730
14.588904	1027.615638	13.037747
14.855090	1004.086397	13.042765
14.593192	1001.070095	13.047783
14.553248	999.604259	13.052800
14.678925	990.646511	13.057818
14.310125	993.872462	13.062835
14.662809	999.465002	13.067853
14.824913	1022.716725	13.072871
14.856005	1008.965327	13.077888
14.743650	994.850898	13.082906
14.631373	992.060028	13.087923
14.727469	985.335552	13.092941
14.267712	1002.742750	13.097959
14.420495	1010.875406	13.102976
14.849065	1026.393587	13.107994
14.578882	1025.125418	13.113011
14.823050	1029.235354	13.118029
14.692415	1022.477476	13.123047
14.510748	1028.206749	13.128064
15.057399	1031.987805	13.133082
14.603183	1031.781775	13.138099
15.134915	1022.891331	13.143117
14.808196	1041.493716	13.148135
14.741849	1032.358065	13.153152
15.110641	1040.243852	13.158170
14.484910	1038.341439	13.163187
14.401728	1045.497522	13.168205
14.777616	1040.088773	13.173223
14.482048	1042.321291	13.178240
15.205874	1030.323404	13.183258
14.786703	1031.047654	13.188275
14.761569	1018.900561	13.193293
14.641021	1032.139204	13.198311
14.632271	1044.112139	13.203328
15.110020	1045.503784	13.208346
15.092775	1047.146496	13.213363
15.198667	1049.416001	13.218381
14.824877	1051.937191	13.223399
15.009630	1053.266448	13.228416
15.452237	1058.325529	13.233434
15.017931	1060.050943	13.238451
15.426481	1053.463354	13.243469
15.218329	1060.862896	13.248487
15.278424	1054.973342	13.253504
15.572315	1049.218354	13.258522
15.210019	1050.215051	13.263539
15.352424	1026.081921	13.268557
15.229786	1032.633199	13.273575
15.110209	1032.956812	13.278592
15.184895	1028.159959	13.283610
15.044961	1037.080846	13.288627
15.117773	1039.890770	13.293645
15.515012	1047.583111	13.298663
15.503695	1050.731692	13.303680
15.651465	1038.812464	13.308698
15.217965	1033.912810	13.313715
15.481449	1018.609656	13.318733
15.381333	1020.593764	13.323751
14.972006	1028.332196	13.328768
15.183112	1025.964770	13.333786
14.995890	1042.968961	13.338803
15.460568	1049.547576	13.343821
15.540837	1052.501327	13.348839
15.360331	1059.646929	13.353856
15.582270	1048.812508	13.358874
15.569563	1056.610586	13.363891
15.777600	1047.453003	13.368909
15.966480	1048.252134	13.373927
15.196042	1040.262988	13.378944
15.599142	1025.726589	13.383962
15.449317	1031.517127	13.388979
15.292960	1037.986788	13.393997
15.314417	1042.966471	13.399015
15.483830	1061.183591	13.404032
15.926332	1049.558114	13.409050
15.536605	1055.247581	13.414067
16.083045	1059.354217	13.419085
15.775867	1048.345862	13.424103
15.514041	1055.706444	13.429120
15.792866	1054.982484	13.434138
15.531331	1059.994769	13.439155
15.664869	1067.731485	13.444173
15.746815	1064.965976	13.449191
15.382717	1070.598465	13.454208
15.392090	1055.431546	13.459226
15.346769	1059.568074	13.464243
15.375353	1058.198962	13.469261
15.816332	1051.105700	13.474279
15.589524	1055.941798	13.479296
15.651883	1048.529869	13.484314
15.468696	1063.551249	13.489331
15.709039	1082.676213	13.494349
16.112201	1082.665644	13.499367
15.910576	1091.299362	13.504384
15.956551	1084.555768	13.509402
15.789593	1099.460935	13.514419
15.783349	1080.621747	13.519437
15.989277	1084.194204	13.524455
15.846438	1094.654735	13.529472
15.889378	1084.881797	13.534490
15.881318	1096.764319	13.539507
15.815303	1100.473636	13.544525
15.561402	1089.787300	13.549543
15.856450	1098.806784	13.554560
15.758686	1089.917986	13.559578
15.793181	1101.839535	13.564595
15.797843	1098.258377	13.569613
16.009752	1086.731206	13.574631
15.891892	1094.940518	13.579648
16.234842	1103.846199	13.584666
15.885924	1109.042599	13.589683
16.248973	1118.322468	13.594701
16.255038	1113.569994	13.599719
16.407974	1113.529332	13.604736
16.481319	1103.137279	13.609754
16.375287	1100.735454	13.614771
16.231771	1091.880786	13.619789
16.292800	1087.118647	13.624807
16.048674	1090.225407	13.629824
16.373937	1090.651662	13.634842
16.419967	1090.816827	13.639859
16.065556	1079.863689	13.644877
16.250912	1093.630284	13.649895
16.408416	1104.466318	13.654912
16.538816	1102.338561	13.659930
16.385973	1087.593436	13.664947
16.443233	1070.425393	13.669965
16.743082	1075.987525	13.674983
16.225655	1082.239359	13.680000
16.547619	1082.260907	13.685018
16.808948	1081.668360	13.690035
16.504526	1087.141017	13.695053
16.638892	1080.594792	13.700071
16.424670	1077.801859	13.705088
16.281736	1078.235616	13.710106
16.454744	1079.882318	13.715123
16.235972	1076.991727	13.720141
16.568461	1088.398935	13.725159
16.538903	1107.110140	13.730176
16.774163	1093.891964	13.735194
16.830294	1109.264526	13.740211
16.271210	1098.541428	13.745229
16.790267	1102.824622	13.750247
16.642497	1111.538414	13.755264
16.658274	1111.457437	13.760282
16.585509	1113.952902	13.765299
16.928797	1104.868194	13.770317
16.741615	1102.739386	13.775335
16.533250	1110.141545	13.780352
16.996997	1100.656283	13.785370
16.807593	1112.700853	13.790387
16.949559	1113.390828	13.795405
17.077311	1092.074741	13.800423
16.750655	1086.422291	13.805440
16.826817	1086.382508	13.810458
16.728283	1081.199958	13.815475
16.654705	1077.617170	13.820493
16.832978	1101.798479	13.825511
16.512977	1119.752310	13.830528
16.901685	1114.312681	13.835546
16.849043	1114.922433	13.840563
16.920348	1109.210506	13.845581
17.068625	1105.105886	13.850599
17.145960	1116.637355	13.855616
16.946979	1114.906301	13.860634
17.228672	1113.017673	13.865651
17.101451	1123.649828	13.870669
17.148851	1114.112318	13.875687
16.799464	1116.837722	13.880704
17.001538	1110.042536	13.885722
17.229471	1099.981772	13.890739
16.793660	1105.887502	13.895757
17.089463	1094.379724	13.900775
16.834188	1106.748512	13.905792
17.084783	1105.258468	13.910810
16.932576	1100.353047	13.915827
16.890458	1107.264811	13.920845
17.032851	1102.540000	13.925863
16.889677	1113.825078	13.930880
17.021279	1115.598687	13.935898
16.828928	1121.619874	13.940915
17.050534	1141.803555	13.945933
17.174949	1130.629342	13.950951
17.125130	1146.349125	13.955968
17.420869	1145.108860	13.960986
17.446053	1138.402334	13.966003
17.232999	1134.156466	13.971021
17.385780	1137.847348	13.976039
17.304879	1147.583811	13.981056
17.546451	1143.238994	13.986074
17.606891	1134.602133	13.991091
17.367529	1143.836908	13.996109
17.330109	1145.219422	14.001127
17.199633	1149.340524	14.006144
17.636947	1136.048572	14.011162
17.470193	1136.657304	14.016179
17.045938	1150.160380	14.021197
17.355214	1134.766091	14.026215
17.413091	1139.549068	14.031232
17.289720	1139.580245	14.036250
17.260589	1143.659207	14.041267
17.414396	1166.453730	14.046285
17.395536	1157.831732	14.051303
17.318752	1162.282693	14.056320
17.767756	1158.612737	14.061338
17.682000	1168.711772	14.066355
17.693937	1175.720916	14.071373
18.246885	1174.428303	14.076391
17.511753	1169.502282	14.081408
18.000916	1168.549885	14.086426
17.934348	1166.104723	14.091443
17.935454	1166.322385	14.096461
18.121547	1164.991003	14.101479
17.808480	1149.233870	14.106496
17.825448	1140.038134	14.111514
17.799678	1138.389458	14.116531
17.487987	1152.964910	14.121549
17.786073	1156.116113	14.126567
17.542856	1167.694690	14.131584
17.979328	1171.254064	14.136602
17.923978	1168.654905	14.141619
17.995310	1183.245422	14.146637
18.366023	1177.425337	14.151655
18.237904	1170.347144	14.156672
17.872723	1182.379878	14.161690
18.005825	1167.579351	14.166707
17.670848	1174.530291	14.171725
17.583089	1167.959329	14.176743
18.136706	1160.885192	14.181760
17.940052	1175.966378	14.186778
17.840421	1173.717596	14.191795
17.844165	1170.891380	14.196813
17.876806	1173.546181	14.201831
17.945839	1175.727124	14.206848
17.826428	1174.525548	14.211866
17.789639	1182.578617	14.216883
17.926010	1198.739266	14.221901
18.176470	1201.270883	14.226919
18.308297	1208.742245	14.231936
18.094775	1206.474489	14.236954
18.055797	1209.899287	14.241971
17.860374	1201.186580	14.246989
18.399533	1196.313703	14.252007
18.103561	1214.404597	14.257024
18.209462	1208.081493	14.262042
18.245929	1198.583922	14.267059
17.896837	1212.300187	14.272077
18.346281	1203.833808	14.277095
18.315523	1205.291396	14.282112
18.269555	1213.587301	14.287130
18.520513	1222.991254	14.292147
18.491292	1234.197557	14.297165
18.649294	1227.438339	14.302183
18.481975	1221.591224	14.307200
18.546777	1227.005078	14.312218
18.751095	1233.976748	14.317235
18.427585	1216.240656	14.322253
18.164082	1197.849685	14.327271
18.737367	1210.559707	14.332288
18.531942	1233.207820	14.337306
19.037911	1212.518333	14.342323
18.811190	1221.984299	14.347341
18.892087	1205.555398	14.352359
18.734976	1207.124799	14.357376
18.683614	1195.304491	14.362394
18.721745	1193.455907	14.367411
18.401502	1205.413526	14.372429
18.557572	1204.758657	14.377447
18.833803	1222.592818	14.382464
18.555730	1232.632745	14.387482
18.947084	1223.192045	14.392499
18.951360	1228.460018	14.397517
18.796784	1226.822778	14.402535
18.679648	1230.436653	14.407552
18.655614	1233.150035	14.412570
18.836605	1225.247422	14.417587
18.426654	1232.964605	14.422605
18.791871	1230.070966	14.427623
18.530949	1228.744959	14.432640
18.839145	1232.153327	14.437658
19.207800	1235.176170	14.442675
18.471060	1231.726164	14.447693
18.747258	1244.522903	14.452711
19.293821	1244.010951	14.457728
18.927977	1246.556446	14.462746
19.428920	1243.018024	14.467763
19.210116	1236.037649	14.472781
19.425696	1225.947748	14.477799
19.146140	1231.557663	14.482816
18.842519	1234.539659	14.487834
19.352149	1230.234365	14.492851
19.110978	1234.894966	14.497869
19.247618	1228.402428	14.502887
19.152984	1219.216625	14.507904
19.562296	1226.746257	14.512922
19.638113	1226.913586	14.517939
19.313305	1235.614783	14.522957
19.405353	1228.035680	14.527975
19.373777	1227.235861	14.532992
19.311643	1231.737562	14.538010
19.387986	1219.666637	14.543027
19.087917	1232.520811	14.548045
19.066859	1219.917046	14.553063
19.024765	1226.791266	14.558080
19.047958	1228.506043	14.563098
19.201843	1242.605288	14.568115
18.930884	1260.933996	14.573133
19.119016	1260.330511	14.578151
19.572171	1263.090809	14.583168
19.564345	1273.346694	14.588186
19.649495	1266.046428	14.593203
19.574875	1264.039723	14.598221
19.875183	1262.558769	14.603239
19.837069	1255.456608	14.608256
19.524357	1268.396353	14.613274
19.773770	1262.982054	14.618291
19.757893	1260.644428	14.623309
19.670849	1251.400076	14.628327
19.499730	1260.208152	14.633344
19.232311	1263.638632	14.638362
19.568522	1249.711022	14.643379
19.647094	1254.603591	14.648397
19.557342	1260.903700	14.653415
19.750219	1258.195994	14.658432
19.362668	1267.884208	14.663450
19.604580	1257.626178	14.668467
19.693150	1268.663653	14.673485
19.769845	1281.167455	14.678503
20.232660	1282.008914	14.683520
20.075670	1276.718653	14.688538
19.880923	1261.573651	14.693555
19.950017	1263.345010	14.698573
20.021855	1246.340481	14.703591
20.057633	1255.366295	14.708608
20.003976	1252.426340	14.713626
20.190371	1244.603323	14.718643
20.130059	1250.476183	14.723661
19.626233	1259.940926	14.728679
19.985913	1261.944932	14.733696
19.713296	1281.195853	14.738714
20.429557	1279.742797	14.743731
20.319560	1291.607674	14.748749
20.103531	1285.188156	14.753767
20.231720	1279.105400	14.758784
20.186162	1291.544978	14.763802
19.972981	1283.353588	14.768819
20.347580	1282.141614	14.773837
20.205807	1290.346911	14.778855
20.290190	1277.217873	14.783872
20.472428	1290.630683	14.788890
20.577538	1283.601087	14.793907
20.366723	1265.150745	14.798925
20.099918	1263.517089	14.803943
20.324200	1268.528672	14.808960
20.724223	1279.968360	14.813978
20.462508	1258.543989	14.818995
20.749655	1255.710878	14.824013
20.254012	1262.945656	14.829031
20.615998	1248.108998	14.834048
20.147364	1248.429286	14.839066
20.356737	1245.519279	14.844083
20.122035	1262.625245	14.849101
20.390234	1268.159809	14.854119
20.589172	1265.169645	14.859136
20.214604	1272.347022	14.864154
20.598908	1267.237548	14.869171
20.388516	1273.889047	14.874189
20.440170	1272.527913	14.879207
20.626331	1274.594252	14.884224
20.245948	1280.093898	14.889242
20.497436	1272.171343	14.894259
20.957280	1271.478867	14.899277
20.742852	1285.834266	14.904295
20.541306	1274.632332	14.909312
20.713781	1266.606910	14.914330
20.866668	1264.421486	14.919347
21.092575	1265.701643	14.924365
20.441733	1278.292412	14.929383
20.777345	1266.865513	14.934400
20.586960	1273.715055	14.939418
20.708163	1296.017789	14.944435
21.166186	1311.750652	14.949453
20.522861	1312.950280	14.954471
20.788152	1298.101212	14.959488
20.984068	1308.272277	14.964506
20.893220	1305.426241	14.969523
21.029963	1299.414297	14.974541
20.668103	1306.087889	14.979559
20.900201	1301.165936	14.984576
20.683147	1307.104872	14.989594
20.896934	1299.733929	14.994611
20.936433	1305.029568	14.999629
21.315822	1308.322069	15.004647
21.158585	1290.692449	15.009664
21.165148	1311.883013	15.014682
21.071197	1310.559321	15.019699
21.119028	1297.191263	15.024717
21.256588	1299.477418	15.029735
21.142498	1298.156269	15.034752
21.229849	1313.584694	15.039770
21.310217	1314.167946	15.044787
21.245583	1329.131808	15.049805
21.467902	1327.584810	15.054823
21.710364	1318.086189	15.059840
21.606364	1302.747631	15.064858
21.413314	1301.874311	15.069875
21.506063	1294.186807	15.074893
21.212821	1302.730484	15.079911
21.256917	1291.843208	15.084928
21.020322	1298.466376	15.089946
21.353119	1317.051821	15.094963
21.662067	1328.228288	15.099981
21.437173	1333.331245	15.104999
21.591986	1334.269073	15.110016
21.567735	1331.587790	15.115034
21.621137	1333.935686	15.120051
21.987661	1331.933224	15.125069
21.493581	1325.668482	15.130087
21.953704	1320.742693	15.135104
21.934342	1340.214003	15.140122
21.368015	1326.134338	15.145139
21.929108	1325.869160	15.150157
21.661669	1334.409180	15.155175
21.839121	1325.836327	15.160192
21.578245	1330.789740	15.165210
21.824100	1333.631546	15.170227
22.054572	1331.493322	15.175245
21.646833	1338.070587	15.180263
22.121317	1328.867428	15.185280
22.064994	1332.191197	15.190298
21.785076	1340.568345	15.195315
22.071023	1330.975928	15.200333
21.826690	1333.429122	15.205351
22.057562	1322.423175	15.210368
22.041619	1334.170785	15.215386
21.982861	1335.779842	15.220403
22.179514	1328.308385	15.225421
21.967309	1343.108290	15.230439
21.856053	1325.731624	15.235456
22.088275	1332.384205	15.240474
21.985040	1330.505825	15.245491
22.209235	1335.019285	15.250509
21.739544	1337.252277	15.255527
22.058414	1327.039743	15.260544
22.005836	1327.868360	15.265562
21.961875	1333.438591	15.270579
22.094369	1325.919676	15.275597
21.855496	1336.629279	15.280615
22.164325	1331.778088	15.285632
22.166510	1353.563641	15.290650
22.280847	1351.307815	15.295667
22.515350	1354.188306	15.300685
22.287924	1365.986439	15.305703
22.397606	1364.745020	15.310720
22.803339	1364.680098	15.315738
22.361107	1367.894642	15.320755
22.755320	1355.726007	15.325773
22.769828	1355.344098	15.330791
22.632961	1335.133858	15.335808
22.711535	1323.816511	15.340826
22.499465	1330.782441	15.345843
22.828857	1315.119332	15.350861
22.480003	1320.832254	15.355879
22.233490	1308.788830	15.360896
22.548364	1332.285816	15.365914
22.637395	1349.938099	15.370931
22.693964	1355.434056	15.375949
22.637430	1362.889580	15.380967
22.260525	1358.027312	15.385984
22.522550	1363.068313	15.391002
22.529836	1351.697578	15.396019
22.723451	1354.870024	15.401037
22.588460	1362.648117	15.406055
22.939049	1352.692099	15.411072
23.010013	1352.903533	15.416090
22.666680	1366.460934	15.421107
22.954142	1353.303979	15.426125
22.681068	1348.449551	15.431143
22.805467	1352.879326	15.436160
22.625518	1358.852499	15.441178
22.601280	1375.857283	15.446195
23.365283	1386.313601	15.451213
22.955206	1389.436430	15.456231
22.913593	1386.046095	15.461248
22.951668	1392.864626	15.466266
23.151234	1389.245483	15.471283
23.476821	1384.117332	15.476301
23.144222	1381.091381	15.481319
23.324032	1381.343087	15.486336
23.304315	1382.281222	15.491354
23.170536	1389.811327	15.496371
23.272030	1377.774305	15.501389
23.250660	1386.302426	15.506407
22.966454	1385.917920	15.511424
23.069117	1379.737781	15.516442
23.206730	1384.172270	15.521459
23.513677	1388.532916	15.526477
23.449254	1392.686074	15.531495
23.240592	1396.394039	15.536512
23.649362	1386.327414	15.541530
23.249554	1391.370332	15.546547
23.456035	1382.678493	15.551565
23.330668	1392.401201	15.556583
23.262157	1383.360962	15.561600
23.258195	1388.079836	15.566618
23.231141	1387.419991	15.571635
23.218848	1377.110597	15.576653
23.187909	1402.679524	15.581671
23.563034	1407.673507	15.586688
23.830230	1413.147667	15.591706
23.553753	1409.950449	15.596723
23.827572	1414.924567	15.601741
23.702901	1415.646614	15.606759
23.608244	1411.575368	15.611776
23.799545	1406.177708	15.616794
23.903255	1412.715163	15.621811
24.065710	1408.751998	15.626829
23.864138	1412.204302	15.631847
23.996186	1409.814258	15.636864
24.281768	1412.539883	15.641882
23.819315	1418.417264	15.646899
24.364175	1401.123792	15.651917
24.004041	1397.860492	15.656935
23.918617	1379.482978	15.661952
24.122351	1368.597412	15.666970
24.097669	1380.235690	15.671987
23.973806	1360.981206	15.677005
23.526352	1375.918233	15.682023
23.880292	1387.902355	15.687040
23.853713	1396.695282	15.692058
24.117660	1398.828891	15.697075
24.515454	1399.674411	15.702093
24.255126	1405.062540	15.707111
24.238789	1412.956268	15.712128
24.508445	1414.068994	15.717146
24.220676	1407.954350	15.722163
24.080420	1410.677326	15.727181
24.050282	1413.420289	15.732199
24.228128	1404.252328	15.737216
24.374936	1406.198632	15.742234
24.223907	1401.405307	15.747251
24.302176	1400.720576	15.752269
24.233676	1410.097330	15.757287
24.354937	1395.129076	15.762304
24.491107	1399.207556	15.767322
24.126446	1398.670226	15.772339
24.584396	1394.187824	15.777357
24.687833	1403.046265	15.782375
24.380047	1411.050549	15.787392
24.570970	1406.545154	15.792410
24.326703	1417.156702	15.797427
24.433472	1418.742744	15.802445
24.433674	1421.600953	15.807463
24.556767	1428.012786	15.812480
24.831835	1426.328929	15.817498
24.823671	1440.911374	15.822515
24.772828	1431.162178	15.827533
24.801822	1431.398853	15.832551
24.671157	1430.713418	15.837568
24.872552	1436.403945	15.842586
24.736600	1442.139201	15.847603
24.810964	1432.751349	15.852621
24.867541	1436.646168	15.857639
24.695105	1446.806554	15.862656
24.801151	1443.449277	15.867674
24.281533	1441.857185	15.872691
24.621314	1432.707323	15.877709
24.684330	1442.737666	15.882727
24.854345	1457.515847	15.887744
25.460015	1461.560451	15.892762
25.151787	1470.867424	15.897779
25.512169	1460.384590	15.902797
25.468503	1438.490330	15.907815
25.045684	1435.801086	15.912832
25.040110	1431.520454	15.917850
24.888205	1431.867132	15.922867
25.193426	1428.041765	15.927885
25.270105	1443.435868	15.932903
25.332978	1442.240362	15.937920
25.156033	1440.797125	15.942938
25.352750	1465.973071	15.947955
25.320923	1453.475015	15.952973
25.394935	1466.552171	15.957991
25.522177	1463.498827	15.963008
25.780034	1468.189220	15.968026
25.190933	1450.772302	15.973043
25.504677	1451.835231	15.978061
25.581497	1457.160576	15.983079
25.494812	1472.476995	15.988096
25.726849	1453.990047	15.993114
25.367332	1460.911711	15.998131
25.519142	1452.419984	16.003149
25.927984	1451.787301	16.008167
25.623613	1453.343075	16.013184
26.018848	1448.853897	16.018202
25.575571	1450.460771	16.023219
25.806106	1450.779677	16.028237
25.916059	1441.820133	16.033255
25.794127	1433.304175	16.038272
25.854257	1431.817627	16.043290
25.403250	1436.874138	16.048307
25.594947	1434.374837	16.053325
25.495107	1442.605565	16.058343
25.916708	1444.573381	16.063360
26.073512	1440.274376	16.068378
26.060993	1453.826981	16.073395
26.129744	1457.394246	16.078413
26.254012	1455.670354	16.083431
26.137652	1444.751030	16.088448
26.183124	1448.626431	16.093466
25.913813	1445.690586	16.098483
26.123168	1445.679374	16.103501
26.240170	1446.383332	16.108519
25.966779	1445.814187	16.113536
26.255518	1440.901724	16.118554
25.897780	1445.444072	16.123571
26.069867	1444.051998	16.128589
26.067008	1441.379166	16.133607
26.193792	1442.834557	16.138624
26.525281	1438.944422	16.143642
26.180660	1449.039182	16.148659
26.366240	1447.227610	16.153677
26.679133	1443.861541	16.158695
26.205054	1443.187981	16.163712
26.344874	1440.467361	16.168730
26.395805	1435.436346	16.173747
26.823355	1434.750775	16.178765
26.616081	1428.083916	16.183783
26.601050	1434.952773	16.188800
26.668165	1432.418163	16.193818
26.739944	1432.351744	16.198835
26.748403	1428.421700	16.203853
26.897423	1424.794368	16.208871
26.406611	1441.208309	16.213888
26.479228	1435.104561	16.218906
26.427232	1434.094158	16.223923
26.674395	1428.926203	16.228941
26.654988	1430.348280	16.233959
26.583388	1437.109572	16.238976
27.014623	1424.802499	16.243994
26.957778	1438.449806	16.249011
26.781429	1438.960738	16.254029
26.939961	1439.355314	16.259047
26.917363	1439.254302	16.264064
26.677174	1431.922497	16.269082
26.824789	1434.237126	16.274099
27.097949	1452.614313	16.279117
27.225345	1459.184089	16.284135
26.996667	1447.441112	16.289152
27.309843	1442.376598	16.294170
26.893471	1436.268631	16.299187
27.023718	1442.333271	16.304205
26.983676	1445.141844	16.309223
27.221141	1452.761593	16.314240
27.729635	1440.682456	16.319258
27.791588	1438.024108	16.324275
27.428358	1423.864141	16.329293
27.417736	1414.200619	16.334311
27.041977	1428.562145	16.339328
27.424999	1417.154069	16.344346
27.078298	1412.598954	16.349363
27.264011	1423.936783	16.354381
27.553885	1423.030690	16.359399
27.547949	1437.413775	16.364416
27.623561	1414.696006	16.369434
27.556844	1416.918903	16.374451
27.397246	1408.258811	16.379469
27.804384	1415.619037	16.384487
27.608197	1419.169258	16.389504
27.526903	1418.368986	16.394522
27.604633	1419.775599	16.399539
27.792326	1428.433345	16.404557
27.569852	1423.499281	16.409575
27.360654	1428.964785	16.414592
27.399894	1434.337666	16.419610
27.517435	1437.086539	16.424627
27.725891	1431.448074	16.429645
27.608251	1439.630962	16.434663
27.398248	1435.825391	16.439680
27.875791	1426.462635	16.444698
27.960901	1433.850500	16.449715
27.875484	1424.359154	16.454733
27.953080	1434.232182	16.459751
27.850607	1437.869662	16.464768
27.820628	1436.555464	16.469786
27.828917	1450.365223	16.474803
27.935920	1473.212221	16.479821
28.393149	1463.798869	16.484839
27.930517	1481.372019	16.489856
28.366646	1471.508862	16.494874
28.003822	1473.896828	16.499891
28.108588	1481.699327	16.504909
28.349803	1478.872586	16.509927
28.039130	1477.891348	16.514944
28.077093	1468.670492	16.519962
28.401735	1475.795988	16.524979
28.144404	1478.857966	16.529997
28.217042	1463.824265	16.535015
28.091963	1475.966544	16.540032
28.098875	1464.844180	16.545050
28.140891	1473.640184	16.550067
28.223434	1479.197042	16.555085
28.378483	1489.957780	16.560103
28.050910	1506.317454	16.565120
28.595283	1503.768717	16.570138
28.556477	1507.246892	16.575155
28.438408	1519.573653	16.580173
28.482780	1505.093135	16.585191
28.573578	1499.731734	16.590208
29.110756	1504.907603	16.595226
29.017316	1495.811189	16.600243
28.513839	1504.069879	16.605261
29.063353	1504.858249	16.610279
28.746398	1498.454533	16.615296
28.868132	1499.936942	16.620314
29.129176	1501.078063	16.625331
28.475671	1508.119778	16.630349
28.930885	1488.093935	16.635367
28.733379	1498.090015	16.640384
28.713008	1499.382353	16.645402
28.858757	1493.721556	16.650419
28.636500	1505.619715	16.655437
29.047435	1505.007351	16.660455
28.851688	1532.998108	16.665472
29.100198	1531.516635	16.670490
29.316901	1531.504603	16.675507
28.929932	1533.918809	16.680525
29.132229	1528.715918	16.685543
29.122552	1525.883786	16.690560
28.762079	1530.428184	16.695578
29.193296	1524.195464	16.700595
29.055609	1531.919173	16.705613
29.175801	1532.877891	16.710631
29.028329	1529.363697	16.715648
29.345090	1530.315321	16.720666
29.584481	1538.518973	16.725683
29.472488	1543.863151	16.730701
29.537748	1541.279426	16.735719
29.710075	1550.338155	16.740736
29.630890	1540.302075	16.745754
29.681323	1525.855374	16.750771
29.646024	1534.509485	16.755789
29.584187	1519.484568	16.760807
29.681001	1532.660952	16.765824
29.842748	1538.678698	16.770842
29.873676	1529.628828	16.775859
29.844831	1531.046569	16.780877
29.739732	1526.264510	16.785895
29.436539	1525.705798	16.790912
29.704500	1544.656519	16.795930
30.169009	1548.694163	16.800947
29.902010	1558.773215	16.805965
30.291856	1546.254212	16.810983
30.366712	1548.839707	16.816000
29.747495	1516.635263	16.821018
30.009124	1517.845768	16.826035
29.846984	1526.383845	16.831053
30.083657	1529.488787	16.836071
30.051307	1543.209096	16.841088
30.257083	1546.404569	16.846106
30.257798	1555.480443	16.851123
30.156674	1547.216660	16.856141
30.458403	1543.929963	16.861159
30.439935	1553.463279	16.866176
30.211818	1547.856570	16.871194
30.076446	1540.945722	16.876211
30.140040	1551.694848	16.881229
30.276875	1543.330924	16.886247
30.432132	1547.422036	16.891264
30.428894	1544.686658	16.896282
30.390418	1550.207248	16.901299
30.249203	1548.017441	16.906317
30.530409	1546.582919	16.911335
30.548558	1548.632185	16.916352
30.560223	1542.388092	16.921370
30.513615	1537.026948	16.926387
30.176393	1547.340600	16.931405
30.339779	1535.936256	16.936423
30.164181	1546.111008	16.941440
30.324125	1567.891657	16.946458
30.554071	1569.430787	16.951475
30.620213	1569.007470	16.956493
30.705098	1567.839218	16.961511
30.647329	1577.482181	16.966528
30.729176	1584.413037	16.971546
31.053672	1578.100700	16.976563
30.989164	1580.471269	16.981581
30.795524	1570.621385	16.986599
31.023196	1571.792039	16.991616
30.930282	1581.283351	16.996634
31.064805	1571.656564	17.001651
30.905959	1581.875611	17.006669
31.091043	1564.614841	17.011687
31.244829	1566.486005	17.016704
30.989796	1567.648842	17.021722
31.002006	1575.517859	17.026739
30.963714	1587.434492	17.031757
31.070620	1594.222253	17.036775
31.010268	1600.467451	17.041792
30.972075	1607.465000	17.046810
31.382641	1595.660753	17.051827
31.507352	1609.163654	17.056845
31.187063	1599.857452	17.061863
31.581912	1589.617427	17.066880
31.692151	1599.302709	17.071898
31.632705	1599.089295	17.076915
31.596596	1604.200509	17.081933
31.298854	1594.741980	17.086951
31.276286	1600.953182	17.091968
31.373383	1594.631178	17.096986
31.480178	1593.959834	17.102003
31.397735	1600.300600	17.107021
31.952280	1616.048334	17.112039
31.818922	1631.831623	17.117056
32.094788	1624.507741	17.122074
32.013304	1612.865691	17.127091
31.874781	1599.285676	17.132109
32.231769	1594.284730	17.137127
31.953257	1590.651447	17.142144
31.855614	1579.019966	17.147162
32.134439	1578.337907	17.152179
32.100034	1577.689110	17.157197
31.810077	1572.009157	17.162215
32.124741	1579.642784	17.167232
31.834684	1603.037816	17.172250
32.302828	1606.664295	17.177267
32.102075	1614.580926	17.182285
32.219817	1620.527442	17.187303
32.473065	1621.091584	17.192320
32.237161	1635.861831	17.197338
32.028358	1622.282781	17.202355
32.039935	1628.569444	17.207373
32.005102	1622.530617	17.212391
32.229479	1622.020330	17.217408
32.205612	1617.483842	17.222426
32.627942	1621.551702	17.227443
32.323018	1619.158454	17.232461
32.215736	1614.183839	17.237479
32.533636	1616.597898	17.242496
32.339625	1613.346069	17.247514
32.639523	1616.336853	17.252531
32.530087	1621.618438	17.257549
32.433075	1617.930354	17.262567
32.899308	1630.493281	17.267584
32.759003	1630.735893	17.272602
32.918630	1638.380211	17.277619
32.532452	1631.320438	17.282637
32.647807	1636.115131	17.287655
32.800573	1643.349021	17.292672
32.620106	1648.181779	17.297690
33.092898	1644.451290	17.302707
32.858443	1642.720132	17.307725
32.910322	1649.606370	17.312743
33.014589	1638.461887	17.317760
32.817416	1646.358063	17.322778
33.070086	1640.807874	17.327795
33.080210	1651.519455	17.332813
33.358262	1645.654476	17.337831
33.205181	1633.150331	17.342848
33.284228	1641.782850	17.347866
33.328298	1633.483021	17.352883
33.269755	1630.945918	17.357901
33.007614	1630.478437	17.362919
33.386409	1630.264639	17.367936
33.043314	1639.614479	17.372954
33.336030	1635.052240	17.377971
33.245953	1633.887900	17.382989
33.287958	1662.409219	17.388007
33.587663	1659.019695	17.393024
33.677449	1675.221218	17.398042
33.650506	1668.034747	17.403059
33.735782	1661.825877	17.408077
33.903182	1670.092278	17.413095
34.151312	1647.901693	17.418112
33.848039	1649.675782	17.423130
33.624718	1643.788357	17.428147
33.734794	1637.830486	17.433165
33.387003	1634.904424	17.438183
33.905271	1647.458962	17.443200
33.570715	1655.948251	17.448218
34.005767	1662.360592	17.453235
33.908201	1661.098877	17.458253
33.847112	1659.876405	17.463271
34.294290	1652.049452	17.468288
33.710741	1663.045347	17.473306
34.185358	1664.181301	17.478323
33.896908	1664.476542	17.483341
33.950727	1667.151744	17.488359
34.195223	1661.592270	17.493376
33.994005	1668.939388	17.498394
34.222684	1665.412602	17.503411
34.170707	1661.509806	17.508429
34.048282	1669.942395	17.513447
34.194490	1667.088609	17.518464
34.101675	1664.349315	17.523482
34.570236	1686.107671	17.528499
34.461112	1694.729785	17.533517
34.447066	1692.157960	17.538535
34.585711	1693.136470	17.543552
34.739610	1692.934250	17.548570
34.940624	1676.971949	17.553587
34.782499	1670.835184	17.558605
34.722140	1661.196654	17.563623
34.686204	1647.928147	17.568640
34.770497	1659.421280	17.573658
34.522971	1659.689878	17.578675
34.580017	1660.019745	17.583693
34.545643	1675.853250	17.588711
34.875743	1672.820272	17.593728
34.772873	1675.462715	17.598746
34.515389	1686.688961	17.603763
34.923358	1688.685439	17.608781
35.087353	1681.768751	17.613799
35.085298	1684.869283	17.618816
35.033240	1686.174942	17.623834
34.974181	1691.094331	17.628851
34.889466	1685.617989	17.633869
34.976572	1682.676931	17.638887
35.134302	1683.027950	17.643904
34.611923	1683.345119	17.648922
35.006997	1687.397228	17.653939
35.089994	1700.854747	17.658957
35.096700	1713.884975	17.663975
35.461904	1718.695288	17.668992
35.182019	1725.081331	17.674010
35.588409	1726.294109	17.679027
35.609435	1718.899120	17.684045
35.346792	1705.517652	17.689063
35.637486	1713.879633	17.694080
35.525994	1716.552835	17.699098
35.830412	1707.617686	17.704115
35.651304	1700.532322	17.709133
35.484917	1700.557814	17.714151
35.540613	1700.707020	17.719168
35.503063	1699.737318	17.724186
35.786045	1699.123457	17.729203
36.022427	1713.172891	17.734221
35.802907	1701.839378	17.739239
35.850634	1714.382175	17.744256
35.589100	1698.048113	17.749274
35.579304	1686.176666	17.754291
35.912197	1705.935068	17.759309
36.034028	1719.356859	17.764327
36.081582	1712.454282	17.769344
36.313575	1733.471771	17.774362
36.390959	1723.967114	17.779379
36.662688	1713.704051	17.784397
36.421362	1705.211610	17.789415
36.574909	1696.645454	17.794432
36.504937	1694.894391	17.799450
36.333318	1688.223101	17.804467
36.417935	1690.008281	17.809485
36.249233	1690.678372	17.814503
36.638103	1679.662201	17.819520
36.318958	1695.624863	17.824538
36.408392	1693.290632	17.829555
36.673696	1688.949614	17.834573
36.671636	1689.196347	17.839591
36.943586	1688.135739	17.844608
36.683252	1689.053230	17.849626
36.592799	1688.772310	17.854643
36.877079	1685.876414	17.859661
36.673357	1701.146071	17.864679
36.535450	1685.035855	17.869696
36.533281	1696.890902	17.874714
36.739158	1699.310102	17.879731
37.143251	1706.234016	17.884749
36.807458	1714.998509	17.889767
36.994282	1711.321561	17.894784
37.152933	1714.730346	17.899802
36.742098	1724.669908	17.904819
37.255823	1710.748765	17.909837
37.205499	1712.604077	17.914855
37.118269	1712.208267	17.919872
36.948975	1710.914116	17.924890
37.156242	1719.173561	17.929907
37.248302	1722.080419	17.934925
37.008719	1715.394761	17.939943
37.504817	1720.236194	17.944960
37.304251	1723.092995	17.949978
37.246639	1720.415582	17.954995
37.495849	1713.124012	17.960013
37.226903	1717.235081	17.965031
37.422375	1707.765243	17.970048
37.293619	1711.165624	17.975066
37.607854	1712.789450	17.980083
37.734908	1707.176147	17.985101
37.243537	1715.170970	17.990119
37.328960	1717.961221	17.995136
37.309856	1718.284384	18.000154
37.251973	1733.818915	18.005171
37.741988	1739.612826	18.010189
37.754431	1757.937018	18.015207
37.930933	1742.247370	18.020224
37.880284	1744.595007	18.025242
38.035537	1741.709007	18.030259
38.130289	1738.948545	18.035277
37.935250	1743.600296	18.040295
37.925683	1739.965638	18.045312
37.676070	1746.251029	18.050330
37.863537	1747.322251	18.055347
37.830039	1751.655610	18.060365
38.165698	1758.011590	18.065383
38.350250	1764.136668	18.070400
38.779484	1767.622192	18.075418
38.010641	1759.910912	18.080435
38.357461	1756.668683	18.085453
38.711889	1780.043492	18.090471
38.554889	1761.707858	18.095488
38.218755	1746.190707	18.100506
38.640005	1760.183062	18.105523
38.915993	1758.731669	18.110541
38.536105	1742.754088	18.115559
38.501896	1736.084673	18.120576
38.886633	1743.099193	18.125594
38.937163	1753.303437	18.130611
38.788868	1741.805189	18.135629
38.735410	1750.314998	18.140647
38.762149	1742.527955	18.145664
38.967525	1743.486387	18.150682
38.880187	1764.550392	18.155699
39.122925	1761.664890	18.160717
38.862786	1758.148989	18.165735
38.975650	1759.731894	18.170752
38.864770	1766.241977	18.175770
38.769912	1769.772580	18.180787
38.852829	1761.739656	18.185805
38.685896	1777.526281	18.190823
38.996047	1767.224160	18.195840
38.717718	1767.429748	18.200858
39.188437	1770.044930	18.205875
39.285216	1774.702004	18.210893
39.217014	1801.737039	18.215911
39.410096	1794.939693	18.220928
39.543413	1799.227784	18.225946
39.350969	1803.125861	18.230963
39.500224	1790.258273	18.235981
39.603600	1796.364498	18.240999
39.677234	1794.131277	18.246016
39.719990	1792.274968	18.251034
39.698504	1794.619959	18.256051
39.842497	1788.772160	18.261069
39.796601	1786.460278	18.266087
39.871144	1788.254418	18.271104
39.944744	1788.616193	18.276122
39.904046	1793.685122	18.281139
40.293961	1777.919624	18.286157
40.084547	1769.066007	18.291175
39.660475	1765.992700	18.296192
39.788283	1767.184794	18.301210
39.637358	1782.873711	18.306227
40.135757	1785.512666	18.311245
39.652658	1780.645372	18.316263
39.689203	1787.563730	18.321280
39.936696	1790.191005	18.326298
39.777501	1792.661891	18.331315
40.108061	1800.709491	18.336333
40.250516	1811.497729	18.341351
40.297163	1817.096070	18.346368
40.308892	1807.259729	18.351386
40.279307	1819.967143	18.356403
40.584568	1813.582503	18.361421
40.332080	1805.463464	18.366439
40.547950	1805.781653	18.371456
40.643795	1802.319303	18.376474
40.368511	1801.721128	18.381491
40.809083	1791.850342	18.386509
40.689366	1799.669629	18.391527
40.952088	1799.249643	18.396544
40.776085	1797.942225	18.401562
40.874964	1810.226477	18.406579
40.931404	1795.267169	18.411597
40.866279	1796.659437	18.416615
40.834938	1792.637265	18.421632
41.161715	1792.434425	18.426650
41.121844	1792.118572	18.431667
41.126086	1784.724947	18.436685
40.696292	1796.991842	18.441703
40.997598	1785.156693	18.446720
41.238083	1813.662813	18.451738
41.018164	1821.360103	18.456755
41.290721	1822.887100	18.461773
41.396245	1825.104228	18.466791
41.423958	1811.392234	18.471808
41.662080	1814.235212	18.476826
41.234430	1820.709092	18.481843
41.455312	1820.746562	18.486861
41.335084	1814.081290	18.491879
41.295884	1819.106284	18.496896
41.770553	1810.979858	18.501914
41.398488	1814.291349	18.506931
41.373471	1823.891852	18.511949
41.439071	1817.939884	18.516967
41.602721	1815.051696	18.521984
41.721253	1830.302081	18.527002
41.939799	1845.640666	18.532019
41.862770	1847.904695	18.537037
41.709116	1848.970885	18.542055
41.881632	1853.629639	18.547072
41.913954	1848.193341	18.552090
42.049103	1857.655991	18.557107
41.937857	1844.054521	18.562125
42.411182	1840.829554	18.567143
42.145508	1857.770056	18.572160
42.328868	1846.635382	18.577178
42.205056	1846.353476	18.582195
42.244561	1852.919247	18.587213
42.395492	1856.589350	18.592231
41.943281	1864.672847	18.597248
42.229477	1845.855845	18.602266
42.293607	1857.389264	18.607283
42.023252	1857.900589	18.612301
42.429736	1872.665878	18.617319
42.576516	1870.864606	18.622336
42.847092	1869.357213	18.627354
42.821386	1878.412055	18.632371
43.046799	1869.044640	18.637389
43.074812	1867.593670	18.642407
42.723050	1861.435881	18.647424
43.055497	1845.337721	18.652442
42.884885	1833.950167	18.657459
43.038529	1839.551305	18.662477
42.933001	1835.086313	18.667495
42.793484	1837.937180	18.672512
43.142795	1846.829254	18.677530
42.919940	1869.459924	18.682547
43.135018	1859.857436	18.687565
43.344751	1863.439683	18.692583
43.300461	1865.368024	18.697600
43.631935	1860.917609	18.702618
43.224321	1870.721313	18.707635
43.367844	1860.822808	18.712653
43.935181	1863.609619	18.717671
43.381067	1856.019679	18.722688
43.617628	1853.602454	18.727706
43.433862	1862.463352	18.732723
43.436253	1854.696416	18.737741
43.814444	1859.249143	18.742759
43.645631	1857.215411	18.747776
43.718457	1861.294641	18.752794
43.544393	1874.846363	18.757811
43.530389	1855.363087	18.762829
43.902233	1849.825607	18.767847
43.741328	1869.185952	18.772864
43.490974	1856.872681	18.777882
43.562822	1858.301564	18.782899
43.591820	1869.345772	18.787917
43.900013	1871.561301	18.792935
44.225410	1883.947928	18.797952
43.953713	1881.719799	18.802970
44.235416	1888.788221	18.807987
44.070584	1881.992115	18.813005
44.247797	1879.856517	18.818023
43.866400	1888.716431	18.823040
44.373727	1880.390104	18.828058
44.020743	1883.074112	18.833075
44.187130	1880.494089	18.838093
44.286461	1879.064399	18.843111
44.294371	1910.933001	18.848128
44.797597	1912.320914	18.853146
44.745049	1920.721229	18.858163
44.684537	1932.287112	18.863181
44.710911	1917.743242	18.868199
44.529235	1923.118357	18.873216
44.562749	1919.372610	18.878234
44.737287	1917.157732	18.883251
44.732900	1905.990662	18.888269
44.901926	1915.943172	18.893287
44.723211	1911.108007	18.898304
45.064727	1907.976060	18.903322
44.912508	1909.724822	18.908339
44.877351	1902.582508	18.913357
45.196929	1905.035506	18.918375
45.064095	1916.194081	18.923392
45.285198	1924.486583	18.928410
45.107689	1923.864372	18.933427
45.129394	1933.879030	18.938445
45.602928	1937.661377	18.943463
45.538050	1945.988160	18.948480
45.617127	1942.187245	18.953498
45.561092	1943.156413	18.958515
45.266526	1939.654032	18.963533
45.539656	1928.243860	18.968551
45.443832	1948.491490	18.973568
45.587699	1935.850043	18.978586
45.553655	1942.279005	18.983603
45.555909	1938.851381	18.988621
45.586354	1932.762869	18.993639
45.599474	1944.341788	18.998656
45.859966	1937.459034	19.003674
45.549173	1936.609071	19.008691
45.564633	1936.694660	19.013709
45.989310	1950.610252	19.018727
46.001496	1966.782980	19.023744
46.315624	1960.647578	19.028762
46.168993	1951.703567	19.033779
46.615580	1950.543618	19.038797
46.405114	1942.634272	19.043815
46.244094	1960.894467	19.048832
46.568834	1957.755638	19.053850
46.825084	1960.799171	19.058867
46.733848	1942.305618	19.063885
46.642739	1927.753400	19.068903
46.365827	1915.619059	19.073920
46.560387	1914.542292	19.078938
46.784972	1933.773667	19.083955
46.641804	1930.071287	19.088973
46.702713	1930.912478	19.093991
46.565727	1949.949121	19.099008
47.091599	1942.464495	19.104026
46.971713	1951.168838	19.109043
46.657929	1948.170566	19.114061
47.063699	1940.194618	19.119079
46.850292	1951.045699	19.124096
46.767951	1948.638448	19.129114
47.038028	1955.845423	19.134131
47.002448	1952.523447	19.139149
47.249631	1952.456974	19.144167
46.951065	1949.926022	19.149184
47.208776	1949.166934	19.154202
46.978618	1956.471141	19.159219
46.971325	1957.335807	19.164237
47.362006	1968.725788	19.169255
47.361927	1980.912368	19.174272
47.354243	1979.190935	19.179290
47.350076	1980.087367	19.184307
47.168919	1986.577859	19.189325
47.244140	1971.138355	19.194343
47.342165	1983.133742	19.199360
47.426373	2005.892000	19.204378
47.601244	2006.992288	19.209395
47.620239	2012.213811	19.214413
48.076247	2009.501268	19.219431
47.611508	2012.383079	19.224448
48.279359	2004.676160	19.229466
48.201514	2009.442470	19.234483
47.968941	2006.097530	19.239501
48.395369	1992.575367	19.244519
47.978004	2002.830722	19.249536
48.016638	2003.090024	19.254554
48.324797	1994.879416	19.259571
47.957717	1998.243660	19.264589
48.235153	1989.217345	19.269607
48.162914	1999.477863	19.274624
48.405544	2015.213780	19.279642
48.473629	2022.348664	19.284659
48.792288	2028.111757	19.289677
49.232015	2006.521612	19.294695
48.825198	2001.745371	19.299712
49.142850	1991.869576	19.304730
49.218846	1989.878827	19.309747
48.820379	1987.074838	19.314765
49.159231	1987.991152	19.319783
49.078949	1985.323738	19.324800
49.102174	1987.313567	19.329818
49.052620	1992.447011	19.334835
49.114353	1984.411371	19.339853
49.119586	1975.833944	19.344871
48.946467	1980.315625	19.349888
49.086022	1983.429426	19.354906
49.292980	1982.009891	19.359923
49.216373	1978.542932	19.364941
49.326155	1973.363448	19.369959
49.376969	1965.023549	19.374976
49.148778	1967.434217	19.379994
49.162348	1957.986807	19.385011
48.938160	1975.633111	19.390029
49.564698	1976.169238	19.395047
49.502186	1996.485239	19.400064
49.682914	2005.562925	19.405082
49.907320	2008.543627	19.410099
49.603204	2008.374183	19.415117
49.867176	2003.221368	19.420135
49.852098	2005.073844	19.425152
49.668563	2008.169198	19.430170
50.037141	2000.924296	19.435187
49.481581	2010.435442	19.440205
50.167897	1997.650567	19.445223
49.969899	2009.308316	19.450240
49.693608	2013.071890	19.455258
49.915283	2014.787023	19.460275
49.928044	2041.850435	19.465293
50.310113	2033.875403	19.470311
50.238048	2036.558482	19.475328
50.151446	2039.651012	19.480346
50.647110	2038.536485	19.485363
50.401078	2034.916624	19.490381
50.817325	2022.205687	19.495399
50.351640	2026.826862	19.500416
50.155721	2034.063248	19.505434
50.805173	2030.723908	19.510451
50.799826	2053.435625	19.515469
51.055539	2043.951690	19.520487
50.931150	2049.937205	19.525504
50.710151	2038.906219	19.530522
51.226030	2045.311270	19.535539
50.713138	2052.156583	19.540557
51.047639	2049.817230	19.545575
51.112877	2056.816393	19.550592
51.053797	2052.858771	19.555610
51.069825	2064.165277	19.560627
51.060770	2065.156016	19.565645
51.215618	2059.089216	19.570663
51.096021	2058.131081	19.575680
51.024874	2066.098959	19.580698
51.198398	2057.802309	19.585715
51.285983	2074.175465	19.590733
51.736887	2077.941313	19.595751
51.753243	2084.300594	19.600768
51.456323	2098.334583	19.605786
51.653598	2082.981283	19.610803
51.552038	2089.026224	19.615821
51.607393	2077.303734	19.620839
51.854595	2081.988795	19.625856
51.481801	2089.549094	19.630874
51.804318	2072.944313	19.635891
51.578443	2085.193287	19.640909
51.961232	2076.769337	19.645927
51.990203	2085.631423	19.650944
51.731716	2103.740192	19.655962
52.126904	2106.730089	19.660979
52.229897	2124.555544	19.665997
52.348838	2120.441726	19.671015
52.326750	2110.980432	19.676032
52.242490	2117.833673	19.681050
52.440169	2117.763375	19.686067
52.394133	2113.432749	19.691085
52.636445	2115.992636	19.696103
52.442061	2106.592688	19.701120
52.359676	2104.248603	19.706138
52.553319	2109.022437	19.711155
52.807745	2134.870983	19.716173
53.162447	2129.270297	19.721191
53.070841	2138.034830	19.726208
53.163399	2128.120169	19.731226
53.206931	2106.654013	19.736243
53.026960	2103.391886	19.741261
52.956260	2104.322743	19.746279
52.994524	2115.952945	19.751296
52.988147	2132.596197	19.756314
53.290965	2119.457507	19.761331
53.415222	2129.860822	19.766349
53.376165	2125.446172	19.771367
53.717824	2122.442495	19.776384
53.455691	2124.137403	19.781402
53.446037	2128.262025	19.786419
53.373492	2117.364703	19.791437
53.517220	2121.790916	19.796455
53.611235	2116.027821	19.801472
53.687423	2131.551423	19.806490
53.837679	2123.543990	19.811507
53.578917	2123.947117	19.816525
53.633178	2124.373312	19.821543
53.825107	2135.878342	19.826560
54.023417	2133.584118	19.831578
54.259581	2134.016470	19.836595
54.067343	2139.483161	19.841613
53.809770	2140.627168	19.846631
54.191170	2134.313863	19.851648
54.210190	2142.359194	19.856666
54.585109	2128.384441	19.861683
54.404872	2141.416203	19.866701
54.388115	2148.354948	19.871719
54.631376	2144.076300	19.876736
54.320044	2143.699403	19.881754
54.449813	2136.216565	19.886771
54.653590	2146.938611	19.891789
54.542210	2143.382094	19.896807
54.567430	2137.582135	19.901824
54.746888	2139.055855	19.906842
55.212288	2161.562982	19.911859
54.939943	2156.473943	19.916877
54.922588	2157.642423	19.921895
54.956047	2161.931174	19.926912
54.768714	2167.276405	19.931930
54.740436	2172.278844	19.936947
55.092803	2170.222323	19.941965
55.301889	2170.994359	19.946983
55.391378	2168.274057	19.952000
55.158474	2175.271169	19.957018
55.089930	2166.257638	19.962035
55.065117	2171.732102	19.967053
55.291962	2173.572569	19.972071
55.519562	2179.036423	19.977088
55.510184	2186.874481	19.982106
55.521473	2189.467834	19.987123
55.362755	2188.331919	19.992141
55.465811	2191.441756	19.997159
55.538207	2179.333727	20.002176
55.667908	2196.114192	20.007194
55.863254	2191.001984	20.012211
55.738425	2193.199166	20.017229
55.988312	2213.535474	20.022247
56.315763	2212.357796	20.027264
56.004938	2216.293254	20.032282
56.370938	2215.202112	20.037299
56.698243	2224.420062	20.042317
56.354512	2215.903909	20.047335
56.954023	2203.390080	20.052352
56.968277	2191.635519	20.057370
56.838036	2169.921833	20.062387
56.875747	2168.721572	20.067405
57.028697	2175.077018	20.072423
56.943247	2158.933230	20.077440
56.829962	2156.036417	20.082458
57.319144	2149.513184	20.087475
56.924164	2156.972270	20.092493
56.997825	2166.154155	20.097511
56.927402	2160.623318	20.102528
56.596770	2172.633001	20.107546
56.802114	2161.593869	20.112563
57.093756	2166.035018	20.117581
56.887569	2169.105409	20.122599
56.914203	2166.886594	20.127616
56.945734	2180.455391	20.132634
57.421797	2183.637827	20.137651
57.427499	2200.098856	20.142669
57.401626	2199.549204	20.147687
57.245371	2192.455112	20.152704
57.416802	2199.736766	20.157722
57.283460	2187.489515	20.162739
57.416027	2194.208936	20.167757
57.505768	2206.686732	20.172775
57.699540	2205.551616	20.177792
57.441116	2224.188622	20.182810
57.623488	2218.391007	20.187827
57.796280	2229.334158	20.192845
57.419769	2227.882095	20.197863
57.668665	2240.823341	20.202880
57.910847	2258.213778	20.207898
57.829537	2256.144470	20.212915
58.262019	2252.242759	20.217933
57.996012	2256.617832	20.222951
58.485531	2267.391947	20.227968
58.040040	2258.550094	20.232986
58.223536	2271.078978	20.238003
58.530233	2278.146205	20.243021
58.701948	2283.093389	20.248039
59.348337	2275.544991	20.253056
59.448364	2273.710851	20.258074
59.230243	2247.809547	20.263091
58.970989	2251.487101	20.268109
58.922264	2237.240357	20.273127
59.138786	2241.693548	20.278144
58.891157	2241.427568	20.283162
59.105956	2241.499311	20.288179
59.212588	2243.963344	20.293197
59.129197	2245.997989	20.298215
59.076837	2240.755059	20.303232
58.977121	2249.086582	20.308250
59.318824	2261.293472	20.313267
59.726394	2271.300879	20.318285
59.447499	2278.986096	20.323303
59.374115	2263.951338	20.328320
59.425905	2277.025966	20.333338
59.220656	2269.452571	20.338355
59.276639	2266.320302	20.343373
59.268647	2275.872607	20.348391
59.742843	2272.674966	20.353408
59.443872	2274.854483	20.358426
59.772014	2288.534977	20.363443
59.943553	2303.924304	20.368461
59.939696	2301.489265	20.373479
60.011092	2299.481718	20.378496
59.867534	2289.358943	20.383514
60.060434	2300.676352	20.388531
60.302635	2304.056305	20.393549
59.978287	2296.044149	20.398567
60.469724	2310.916285	20.403584
60.408016	2318.564253	20.408602
60.839818	2319.201469	20.413619
60.742503	2321.985809	20.418637
60.577784	2319.125810	20.423655
60.829896	2329.426444	20.428672
60.617360	2325.262436	20.433690
60.515899	2315.254726	20.438707
60.968187	2315.053973	20.443725
60.955207	2335.024857	20.448743
60.825843	2325.330193	20.453760
60.744870	2330.375838	20.458778
60.921898	2325.368968	20.463795
61.237269	2315.804542	20.468813
61.439213	2345.212830	20.473831
61.651064	2343.080499	20.478848
61.301384	2329.891399	20.483866
61.258568	2336.255641	20.488883
61.232466	2338.277682	20.493901
61.317541	2344.793222	20.498919
61.894471	2348.400330	20.503936
61.711057	2349.067367	20.508954
61.490444	2346.647473	20.513971
61.881958	2340.933550	20.518989
61.743588	2354.102261	20.524007
61.969736	2357.329576	20.529024
61.728642	2353.196458	20.534042
61.884908	2348.811470	20.539059
61.884465	2363.775373	20.544077
62.124870	2376.239825	20.549095
62.313889	2372.140736	20.554112
62.366618	2375.211489	20.559130
62.142019	2376.922267	20.564147
62.406947	2376.391478	20.569165
62.044228	2369.604237	20.574183
62.331232	2377.908928	20.579200
62.368043	2379.345619	20.584218
62.701789	2385.817720	20.589235
62.711473	2400.697118	20.594253
63.031114	2414.871221	20.599271
63.046862	2416.112393	20.604288
62.925157	2399.579294	20.609306
63.100195	2411.260734	20.614323
63.415932	2402.420159	20.619341
62.912188	2403.930039	20.624359
63.213268	2400.446632	20.629376
62.815087	2416.230788	20.634394
62.679170	2409.149768	20.639411
63.219579	2408.330362	20.644429
62.699874	2406.366745	20.649447
62.797855	2408.589534	20.654464
63.052675	2425.601523	20.659482
63.433252	2428.199241	20.664499
63.577156	2436.505368	20.669517
63.632915	2430.853785	20.674535
63.757923	2434.727117	20.679552
63.867511	2438.121141	20.684570
63.871378	2445.601654	20.689587
64.183124	2449.168952	20.694605
64.666542	2426.615555	20.699623
64.742811	2414.366948	20.704640
65.006119	2404.216821	20.709658
64.685192	2397.683273	20.714675
65.053201	2394.213215	20.719693
64.959029	2400.179109	20.724711
64.942125	2383.495646	20.729728
65.043708	2369.453845	20.734746
64.702738	2367.536676	20.739763
64.914993	2365.115123	20.744781
64.715427	2370.856708	20.749799
64.779672	2366.970744	20.754816
64.776978	2375.808705	20.759834
64.860049	2372.964436	20.764851
64.884055	2361.377610	20.769869
64.771428	2378.138087	20.774887
64.908530	2377.678221	20.779904
65.104316	2376.365805	20.784922
64.931592	2402.797163	20.789939
65.493950	2402.432562	20.794957
65.130718	2403.405873	20.799975
65.028695	2400.284727	20.804992
65.028680	2396.479056	20.810010
65.115824	2397.002180	20.815027
65.104039	2397.678256	20.820045
64.953641	2419.529898	20.825063
65.166101	2421.249750	20.830080
65.377330	2418.794503	20.835098
65.528468	2441.258899	20.840115
65.666697	2450.219668	20.845133
65.945408	2453.293838	20.850151
65.879980	2458.309792	20.855168
66.222082	2458.172323	20.860186
65.807721	2473.345865	20.865203
66.189976	2448.930339	20.870221
66.095454	2467.506893	20.875239
66.411294	2495.079837	20.880256
66.987350	2481.598857	20.885274
66.932329	2473.707444	20.890291
66.576081	2445.019172	20.895309
66.775049	2450.970304	20.900327
66.665778	2445.477277	20.905344
66.660761	2450.204918	20.910362
66.590944	2472.042728	20.915379
67.158565	2467.209833	20.920397
67.194046	2475.751601	20.925415
67.164133	2473.372412	20.930432
67.312681	2477.827063	20.935450
67.077437	2477.852910	20.940467
67.210191	2477.307742	20.945485
67.092340	2468.281317	20.950503
67.216222	2471.640115	20.955520
67.402316	2475.479743	20.960538
67.352954	2480.951287	20.965555
67.478238	2470.104681	20.970573
67.082683	2472.993053	20.975591
67.566410	2482.094962	20.980608
67.510862	2492.804989	20.985626
67.482833	2505.374924	20.990643
67.684914	2504.386436	20.995661
67.595654	2499.092433	21.000679
67.635036	2500.133460	21.005696
67.712419	2498.280990	21.010714
67.691253	2530.336373	21.015731
68.264119	2517.563720	21.020749
68.222979	2523.927959	21.025767
68.301417	2529.379189	21.030784
68.136873	2513.843142	21.035802
68.225288	2525.159676	21.040819
68.316578	2528.941563	21.045837
68.685824	2537.916565	21.050855
68.575288	2552.459502	21.055872
69.161605	2550.149324	21.060890
68.914764	2549.620428	21.065907
69.165517	2541.653060	21.070925
68.795040	2545.006564	21.075943
68.638975	2544.919332	21.080960
68.790137	2529.519276	21.085978
69.154880	2552.313080	21.090995
69.363384	2531.103111	21.096013
69.122629	2541.382782	21.101031
68.959526	2548.778148	21.106048
69.186903	2561.286238	21.111066
69.150245	2585.340839	21.116083
69.430750	2575.852483	21.121101
69.656113	2579.014230	21.126119
69.692267	2590.350471	21.131136
69.555161	2577.750207	21.136154
69.555173	2591.390318	21.141171
69.940353	2586.082841	21.146189
70.193787	2594.086127	21.151207
70.219383	2601.708982	21.156224
70.396907	2592.149843	21.161242
70.305538	2607.854557	21.166259
70.424284	2596.744194	21.171277
70.290230	2595.732512	21.176295
70.537650	2599.494914	21.181312
70.634363	2605.235654	21.186330
70.576815	2611.343600	21.191347
70.898880	2602.156216	21.196365
70.747609	2587.807204	21.201383
70.567436	2595.949070	21.206400
70.937696	2586.544689	21.211418
70.452035	2592.095851	21.216435
70.648688	2588.845394	21.221453
70.979296	2600.733343	21.226471
70.733161	2624.881280	21.231488
71.100348	2619.816121	21.236506
71.166285	2630.539237	21.241523
71.277412	2625.567962	21.246541
71.300154	2629.885975	21.251559
71.199261	2620.277951	21.256576
71.371445	2624.217350	21.261594
71.712600	2629.664569	21.266611
71.997186	2647.063398	21.271629
71.819328	2639.931727	21.276647
71.767262	2651.403844	21.281664
72.804619	2627.655330	21.286682
72.886698	2606.608661	21.291699
73.136294	2591.502495	21.296717
73.062672	2597.482785	21.301735
72.762816	2574.895429	21.306752
72.810063	2558.298414	21.311770
72.801581	2547.609873	21.316787
72.682079	2544.894712	21.321805
72.642872	2534.977353	21.326823
72.877364	2546.888230	21.331840
73.015703	2536.615172	21.336858
72.689521	2544.059530	21.341875
72.773097	2539.820744	21.346893
72.730906	2546.824104	21.351911
72.594996	2546.714646	21.356928
73.003757	2537.163783	21.361946
72.806414	2539.204502	21.366963
72.612602	2547.024601	21.371981
73.030104	2549.028675	21.376999
72.845708	2562.610658	21.382016
73.182351	2565.043426	21.387034
72.859112	2577.885025	21.392051
72.694035	2571.733104	21.397069
72.928012	2589.192591	21.402087
73.100847	2597.234788	21.407104
73.137109	2597.918877	21.412122
73.254683	2619.743448	21.417139
73.172536	2638.959465	21.422157
73.507221	2644.995522	21.427175
73.537250	2652.897970	21.432192
73.849279	2663.058028	21.437210
73.932823	2670.314273	21.442227
74.024324	2667.740197	21.447245
74.398296	2667.031546	21.452263
74.164176	2662.795229	21.457280
74.533312	2670.367646	21.462298
74.284257	2660.463232	21.467315
74.350666	2666.021216	21.472333
74.808750	2673.629722	21.477351
74.583501	2683.293570	21.482368
74.969023	2697.515705	21.487386
74.959858	2692.949307	21.492403
74.906241	2699.776681	21.497421
75.178160	2694.409541	21.502439
74.975389	2696.403936	21.507456
75.391792	2685.139209	21.512474
75.017255	2694.307289	21.517491
74.925208	2689.097535	21.522509
75.305308	2688.007575	21.527527
75.177174	2710.450406	21.532544
75.372931	2706.975675	21.537562
75.416100	2725.173503	21.542579
75.671983	2721.847880	21.547597
75.731323	2720.949893	21.552615
75.588018	2724.726896	21.557632
75.748198	2722.380426	21.562650
75.935744	2738.660018	21.567667
76.206261	2744.003602	21.572685
76.241960	2750.946153	21.577703
76.281512	2749.188483	21.582720
76.272283	2739.950258	21.587738
76.305465	2746.572373	21.592755
76.497430	2743.121881	21.597773
76.644908	2743.488007	21.602791
76.892865	2742.637193	21.607808
76.987353	2746.031221	21.612826
76.795592	2742.787440	21.617843
76.810808	2741.021589	21.622861
76.956912	2736.475974	21.627879
76.442372	2737.110939	21.632896
76.639808	2744.767276	21.637914
76.860000	2762.137114	21.642931
76.823507	2772.586717	21.647949
77.181412	2760.622580	21.652967
77.299814	2764.982695	21.657984
77.459741	2764.929067	21.663002
77.422927	2765.690591	21.668019
77.243247	2780.386105	21.673037
77.751762	2794.263217	21.678055
77.233043	2797.092870	21.683072
77.837721	2797.849960	21.688090
77.683613	2804.958541	21.693107
77.936954	2794.680481	21.698125
78.196880	2795.090622	21.703143
78.071075	2799.376145	21.708160
77.961598	2785.917246	21.713178
78.236371	2789.904299	21.718195
78.043367	2816.201137	21.723213
78.508345	2814.971558	21.728231
78.307866	2819.209193	21.733248
78.476493	2820.919406	21.738266
78.885306	2819.261331	21.743283
78.888832	2816.767513	21.748301
79.020409	2811.660916	21.753319
78.729247	2818.487833	21.758336
78.976867	2819.105511	21.763354
78.989226	2825.484261	21.768371
78.968132	2812.919749	21.773389
79.418692	2829.722091	21.778407
79.372002	2846.718428	21.783424
79.159614	2847.061350	21.788442
79.356931	2848.860915	21.793459
79.357197	2845.584199	21.798477
79.709343	2839.808887	21.803495
79.742080	2852.831248	21.808512
79.657817	2837.094215	21.813530
79.616144	2840.131253	21.818547
79.634244	2843.216680	21.823565
80.318102	2856.601506	21.828583
80.486540	2854.150507	21.833600
80.378264	2846.180503	21.838618
80.751096	2860.575351	21.843635
80.428097	2848.230379	21.848653
80.726843	2834.024086	21.853671
80.586558	2840.850883	21.858688
80.819741	2846.814033	21.863706
80.704787	2846.100739	21.868723
80.705492	2853.285724	21.873741
81.060351	2840.544108	21.878759
80.862279	2844.311293	21.883776
80.836691	2843.959989	21.888794
81.172732	2845.103191	21.893811
80.598588	2848.591986	21.898829
81.037272	2836.975056	21.903847
80.767825	2851.276040	21.908864
81.303940	2872.314905	21.913882
80.962715	2879.952846	21.918899
81.119964	2887.776912	21.923917
81.175417	2875.602047	21.928935
81.624057	2893.415760	21.933952
81.604533	2891.190295	21.938970
81.641494	2895.586739	21.943987
81.584487	2902.459248	21.949005
81.833278	2900.355973	21.954023
81.866845	2910.212617	21.959040
82.217592	2919.919614	21.964058
82.510243	2915.270993	21.969075
83.051846	2919.101392	21.974093
83.138583	2901.814045	21.979111
83.225259	2896.066833	21.984128
83.315392	2881.582383	21.989146
83.269628	2866.015723	21.994163
83.325449	2878.719737	21.999181
83.542373	2868.625198	22.004199
83.417305	2868.289938	22.009216
83.303175	2853.290472	22.014234
83.046861	2853.090675	22.019251
82.992224	2840.792696	22.024269
83.293080	2847.561165	22.029287
83.477657	2862.312702	22.034304
83.206239	2876.096339	22.039322
83.298556	2875.155493	22.044339
83.581743	2870.222634	22.049357
83.650877	2862.437864	22.054375
83.555605	2876.414825	22.059392
83.693735	2876.646678	22.064410
83.634653	2877.441807	22.069427
83.441168	2879.023683	22.074445
83.983979	2901.694488	22.079463
83.836108	2905.385678	22.084480
83.771748	2900.506699	22.089498
84.075024	2900.112465	22.094515
83.760893	2906.435362	22.099533
84.015497	2929.231389	22.104551
84.188539	2936.978858	22.109568
84.317345	2934.486365	22.114586
84.508470	2946.949974	22.119603
84.406133	2963.363136	22.124621
85.047442	2964.621252	22.129639
85.095666	2970.077236	22.134656
85.130382	2964.203944	22.139674
85.098553	2966.312246	22.144691
85.340165	2964.601081	22.149709
85.315801	2947.132049	22.154727
85.506249	2946.633235	22.159744
85.673835	2940.710437	22.164762
85.932139	2949.320957	22.169779
85.545129	2945.871610	22.174797
85.670802	2962.119144	22.179815
85.646675	2973.543184	22.184832
85.928926	2982.435583	22.189850
86.349412	2975.838324	22.194867
85.878597	2983.627253	22.199885
85.842968	2983.227213	22.204903
86.052554	2989.978937	22.209920
86.096485	3005.755001	22.214938
86.653001	2997.182559	22.219955
86.398352	3019.254237	22.224973
86.448366	3008.963179	22.229991
86.551979	3008.079513	22.235008
87.034110	3010.465871	22.240026
86.996562	3015.834474	22.245043
86.680430	3020.410557	22.250061
86.718013	3013.691916	22.255079
87.120539	3031.447662	22.260096
86.874838	3028.513513	22.265114
87.243367	3035.142932	22.270131
87.117216	3040.894678	22.275149
87.511219	3031.502247	22.280167
87.510892	3038.026877	22.285184
87.873541	3061.516249	22.290202
87.922044	3060.826720	22.295219
87.957119	3056.637146	22.300237
88.036581	3056.416504	22.305255
88.040263	3059.728760	22.310272
87.878284	3055.536316	22.315290
88.135902	3055.970861	22.320307
88.052335	3065.563504	22.325325
88.387428	3052.587193	22.330343
88.121763	3052.554681	22.335360
87.938302	3078.367330	22.340378
88.572746	3076.055425	22.345395
88.162073	3086.828876	22.350413
88.456377	3086.368801	22.355431
88.776696	3088.465383	22.360448
88.533785	3108.327430	22.365466
88.874225	3108.235311	22.370483
89.168174	3116.583348	22.375501
89.166456	3109.633764	22.380519
89.539131	3110.624087	22.385536
89.286861	3113.823142	22.390554
89.270233	3102.755258	22.395571
89.403037	3116.470343	22.400589
89.672365	3119.833988	22.405607
89.918189	3134.962662	22.410624
89.926201	3139.980480	22.415642
90.128040	3133.040948	22.420659
90.207286	3135.375794	22.425677
90.486203	3128.347151	22.430695
90.149545	3133.169172	22.435712
90.183978	3127.726958	22.440730
90.699277	3126.299281	22.445747
90.457271	3131.430850	22.450765
90.740288	3131.226176	22.455783
90.817603	3128.539016	22.460800
90.948889	3132.473100	22.465818
90.469243	3122.142724	22.470835
90.747891	3127.287071	22.475853
91.033470	3136.873875	22.480871
90.979531	3142.909782	22.485888
90.771660	3157.371734	22.490906
91.039014	3158.643239	22.495923
91.108729	3156.341180	22.500941
91.252143	3155.571398	22.505959
91.287828	3172.398578	22.510976
91.166938	3185.437944	22.515994
91.675040	3183.473274	22.521011
91.227704	3191.595821	22.526029
91.870498	3212.265560	22.531047
91.948826	3215.038751	22.536064
91.654974	3220.820244	22.541082
92.172934	3227.768355	22.546099
91.847621	3222.073749	22.551117
91.853928	3231.901245	22.556135
92.506913	3226.323711	22.561152
92.627717	3234.057914	22.566170
93.468359	3224.290386	22.571187
93.384131	3236.471389	22.576205
93.431511	3228.900655	22.581223
93.517942	3225.439545	22.586240
93.218456	3213.997858	22.591258
93.926624	3209.080491	22.596275
93.482696	3205.034596	22.601293
93.367382	3193.407376	22.606311
93.522024	3191.208992	22.611328
93.490162	3202.269525	22.616346
93.430829	3219.975041	22.621363
93.761212	3219.873167	22.626381
93.307349	3225.475988	22.631399
93.434767	3226.687553	22.636416
93.314411	3227.786915	22.641434
93.895629	3234.608436	22.646451
93.914478	3244.512607	22.651469
93.526784	3253.198944	22.656487
93.931457	3262.959844	22.661504
93.833766	3284.408725	22.666522
94.305606	3291.292046	22.671539
94.395403	3281.142264	22.676557
94.585373	3286.788320	22.681575
94.759974	3300.776185	22.686592
95.026052	3298.584569	22.691610
95.221705	3293.713679	22.696627
95.416112	3305.675467	22.701645
95.463248	3304.199155	22.706663
95.596806	3308.194325	22.711680
95.405005	3306.248053	22.716698
95.891929	3289.329966	22.721715
95.961782	3292.864012	22.726733
95.905834	3292.084648	22.731751
96.149124	3279.904803	22.736768
96.102276	3282.826250	22.741786
96.039822	3264.557652	22.746803
95.895096	3266.329932	22.751821
95.872746	3278.875541	22.756839
95.942150	3282.771464	22.761856
96.032475	3281.998245	22.766874
95.939990	3295.877093	22.771891
96.111958	3293.504968	22.776909
96.204201	3308.585964	22.781927
96.491577	3315.466708	22.786944
96.594701	3326.780611	22.791962
96.427784	3315.748434	22.796979
96.814999	3334.798778	22.801997
96.770147	3353.775269	22.807015
96.985262	3344.857088	22.812032
96.927821	3350.472792	22.817050
97.124233	3346.045851	22.822067
97.296115	3367.655024	22.827085
97.007148	3368.564937	22.832103
97.653173	3380.558059	22.837120
97.348094	3382.347794	22.842138
97.827536	3388.221642	22.847155
97.943403	3406.940539	22.852173
97.943418	3408.494823	22.857191
98.275331	3396.867562	22.862208
97.967933	3404.712767	22.867226
98.200563	3388.656668	22.872243
98.354790	3401.404691	22.877261
98.313144	3422.518126	22.882279
98.545337	3429.701345	22.887296
98.762164	3433.775307	22.892314
98.638712	3439.559431	22.897331
98.497623	3431.365021	22.902349
98.813093	3450.059254	22.907367
99.235293	3448.546541	22.912384
98.832517	3457.171704	22.917402
98.905347	3456.833255	22.922419
99.166210	3461.917268	22.927437
99.373744	3468.306550	22.932455
99.720825	3487.760171	22.937472
99.815099	3485.776053	22.942490
100.183409	3481.651770	22.947507
100.341031	3480.036712	22.952525
100.260242	3500.040186	22.957543
100.550274	3482.236708	22.962560
100.279846	3490.980177	22.967578
100.350998	3487.462084	22.972595
100.489692	3489.086374	22.977613
100.300759	3488.828188	22.982631
100.560118	3474.571521	22.987648
100.629458	3505.278927	22.992666
100.771964	3495.723051	22.997683
100.785365	3515.471610	23.002701
100.790765	3516.180131	23.007719
100.933633	3507.666711	23.012736
100.799885	3516.327765	23.017754
101.136243	3533.590298	23.022771
101.467504	3543.313113	23.027789
101.549273	3546.603514	23.032807
101.585570	3537.068707	23.037824
101.708000	3541.395304	23.042842
101.854630	3544.354120	23.047859
101.960861	3541.426283	23.052877
101.829971	3543.849853	23.057895
101.980826	3551.536335	23.062912
102.144150	3558.455010	23.067930
102.102151	3558.796955	23.072947
102.184963	3564.642711	23.077965
102.102856	3569.786583	23.082983
102.562853	3572.391651	23.088000
102.556076	3592.186161	23.093018
102.329205	3593.757089	23.098035
102.790099	3588.962751	23.103053
102.864544	3596.673300	23.108071
103.210841	3591.251043	23.113088
103.105053	3595.387807	23.118106
103.521172	3603.741904	23.123123
103.812352	3615.371402	23.128141
104.162775	3614.194553	23.133159
104.365998	3605.184488	23.138176
103.888101	3592.462150	23.143194
104.101129	3584.176859	23.148211
104.427681	3576.239351	23.153229
104.021281	3583.659269	23.158247
104.023400	3589.975065	23.163264
104.104642	3604.561312	23.168282
103.945774	3610.258832	23.173299
104.422781	3609.994144	23.178317
104.495324	3602.780491	23.183335
104.563382	3623.667408	23.188352
104.843719	3632.649475	23.193370
104.742068	3624.792937	23.198387
105.206186	3627.841433	23.203405
104.987085	3636.714298	23.208423
104.839637	3630.833060	23.213440
104.565661	3648.757605	23.218458
104.708327	3665.356615	23.223475
105.193838	3663.976336	23.228493
104.999429	3681.546427	23.233511
105.560514	3681.095009	23.238528
105.810654	3687.814354	23.243546
106.159273	3687.788207	23.248563
106.327999	3676.353061	23.253581
106.132194	3691.584784	23.258599
106.305023	3697.466504	23.263616
106.668998	3715.832565	23.268634
106.663960	3718.364108	23.273651
107.002917	3699.589685	23.278669
107.172051	3697.078202	23.283687
107.179323	3686.683915	23.288704
107.120241	3702.093846	23.293722
107.322098	3699.293488	23.298739
107.504601	3692.743915	23.303757
107.101031	3691.411336	23.308775
107.118967	3694.433967	23.313792
107.525159	3694.629018	23.318810
107.458395	3685.109576	23.323827
107.488849	3691.423880	23.328845
107.691330	3714.708029	23.333863
108.021116	3717.464563	23.338880
107.876985	3713.229226	23.343898
107.773719	3718.629798	23.348915
108.293857	3711.543710	23.353933
107.558769	3733.278854	23.358951
107.978193	3746.818392	23.363968
108.039177	3757.439167	23.368986
108.025500	3759.068191	23.374003
108.486132	3780.451875	23.379021
108.390198	3785.236680	23.384039
108.568991	3778.905012	23.389056
108.961300	3783.286689	23.394074
108.792147	3777.530638	23.399091
109.380456	3797.542435	23.404109
109.496093	3807.401443	23.409127
109.671371	3795.902921	23.414144
109.931081	3790.677190	23.419162
109.689018	3806.664716	23.424179
110.164090	3795.364691	23.429197
109.956515	3806.481068	23.434215
110.032527	3798.784458	23.439232
110.015619	3795.451323	23.444250
109.750033	3801.922861	23.449267
110.114909	3818.617602	23.454285
110.112700	3834.990335	23.459303
110.223683	3825.826089	23.464320
110.357382	3825.491748	23.469338
109.990444	3848.782789	23.474355
110.683987	3848.326408	23.479373
110.838177	3860.195661	23.484391
111.070902	3866.601025	23.489408
111.450573	3874.558526	23.494426
111.185520	3885.625401	23.499443
111.773719	3879.104384	23.504461
111.656002	3873.959498	23.509479
111.737064	3877.057167	23.514496
112.239333	3872.578750	23.519514
111.896569	3884.360057	23.524531
111.970159	3878.427238	23.529549
112.041270	3896.920651	23.534567
112.114683	3905.883525	23.539584
112.448795	3895.102798	23.544602
112.230208	3911.768854	23.549619
112.381111	3902.542847	23.554637
112.406071	3914.957526	23.559655
112.733301	3940.363191	23.564672
113.033769	3934.130649	23.569690
112.925694	3944.266875	23.574707
113.097597	3939.477270	23.579725
113.125556	3944.168420	23.584743
113.344764	3930.353417	23.589760
113.589488	3947.841403	23.594778
113.615921	3970.744779	23.599795
114.013455	3959.598005	23.604813
113.913011	3980.432927	23.609831
113.532320	3978.119345	23.614848
113.858591	3967.774523	23.619866
113.634340	3979.345367	23.624883
114.065054	3986.615730	23.629901
114.040494	3997.101194	23.634919
114.137898	3993.567625	23.639936
114.357419	4000.270511	23.644954
114.484869	4021.812344	23.649971
114.835834	4029.707343	23.654989
115.160881	4020.902506	23.660007
115.172427	4030.745784	23.665024
114.974873	4024.760074	23.670042
115.240158	4036.541416	23.675059
115.175374	4046.912690	23.680077
115.363469	4057.981581	23.685095
115.609315	4054.693558	23.690112
115.485160	4049.121315	23.695130
115.478094	4060.133083	23.700147
116.073720	4063.055208	23.705165
115.863869	4077.925836	23.710183
115.926611	4066.170110	23.715200
116.270186	4071.910367	23.720218
116.573389	4093.981153	23.725235
116.477851	4100.066432	23.730253
116.642589	4100.731721	23.735271
116.447786	4110.929632	23.740288
116.815240	4106.568706	23.745306
116.892711	4117.337796	23.750323
116.915551	4104.026367	23.755341
117.133814	4120.909447	23.760359
116.954409	4130.672526	23.765376
117.413952	4130.531196	23.770394
117.305905	4139.666716	23.775411
117.217913	4143.541224	23.780429
117.604720	4153.429661	23.785447
117.918901	4151.874495	23.790464
118.407175	4153.363921	23.795482
118.089153	4160.711631	23.800499
118.432122	4148.613462	23.805517
118.720417	4151.299762	23.810535
118.338146	4161.540889	23.815552
118.616534	4165.880081	23.820570
118.798944	4180.480468	23.825587
119.165911	4185.769638	23.830605
119.044636	4183.780497	23.835623
118.853824	4186.655031	23.840640
119.366644	4171.630223	23.845658
119.383520	4202.655562	23.850675
119.599930	4207.403844	23.855693
119.603656	4201.108809	23.860711
119.358396	4210.471777	23.865728
119.849644	4209.369652	23.870746
119.892316	4226.435806	23.875763
119.923490	4231.345419	23.880781
120.121299	4235.655424	23.885799
120.167775	4245.048950	23.890816
120.309593	4230.199569	23.895834
120.127171	4239.760055	23.900851
120.749721	4252.797944	23.905869
120.688770	4252.270158	23.910887
120.480021	4269.597600	23.915904
121.051483	4269.405885	23.920922
120.900664	4288.645132	23.925939
121.186941	4290.895941	23.930957
121.284432	4294.869765	23.935975
121.342900	4299.133124	23.940992
121.705738	4311.642689	23.946010
121.453193	4330.447985	23.951027
121.781200	4322.902007	23.956045
122.057340	4319.207327	23.961063
122.010536	4327.775326	23.966080
122.440702	4331.776476	23.971098
122.274722	4348.858736	23.976115
122.496741	4347.022308	23.981133
122.756563	4348.971968	23.986151
122.588989	4355.747634	23.991168
122.678810	4350.353717	23.996186
122.699498	4369.562755	24.001203
123.147198	4373.077526	24.006221
123.299403	4380.022028	24.011239
123.181835	4389.584882	24.016256
124.032135	4374.646641	24.021274
124.050009	4381.898790	24.026291
124.329617	4365.958340	24.031309
124.620373	4357.935403	24.036327
124.701164	4357.636567	24.041344
124.679974	4348.385976	24.046362
124.725881	4358.326151	24.051379
124.990511	4343.772527	24.056397
125.072799	4347.249637	24.061415
124.943902	4354.893370	24.066432
125.034262	4345.185740	24.071450
124.949316	4350.800050	24.076467
124.848798	4339.933741	24.081485
125.192499	4343.286547	24.086503
125.215016	4350.819033	24.091520
125.619518	4339.333417	24.096538
125.352245	4350.231686	24.101555
125.289296	4335.555025	24.106573
125.711763	4345.826691	24.111591
125.050041	4373.638731	24.116608
125.398133	4375.745472	24.121626
125.315971	4390.179920	24.126643
125.680528	4394.691562	24.131661
125.927480	4402.155095	24.136679
125.819301	4425.157765	24.141696
126.319851	4439.570384	24.146714
126.313051	4434.277055	24.151731
126.711777	4438.860628	24.156749
127.175315	4461.967318	24.161767
127.298747	4457.492278	24.166784
127.556300	4453.030905	24.171802
127.642640	4445.281873	24.176819
128.021164	4441.361572	24.181837
128.033519	4442.983609	24.186855
128.097482	4443.696277	24.191872
128.293106	4430.341057	24.196890
128.255795	4444.877993	24.201907
128.392465	4439.111321	24.206925
128.589564	4440.377614	24.211943
128.272003	4434.276134	24.216960
128.740280	4433.034869	24.221978
128.761614	4432.502142	24.226995
128.419413	4453.237872	24.232013
128.915677	4466.840938	24.237031
128.518293	4469.730760	24.242048
128.927250	4468.363459	24.247066
129.123173	4477.137905	24.252083
128.856048	4504.022712	24.257101
128.932973	4499.726615	24.262119
129.142116	4517.731391	24.267136
129.220550	4525.461034	24.272154
129.503162	4541.238983	24.277171
129.910247	4557.341678	24.282189
130.159536	4558.411549	24.287207
130.171323	4558.985196	24.292224
130.379932	4554.266509	24.297242
130.466458	4562.140513	24.302259
130.314030	4574.580304	24.307277
130.798067	4583.182389	24.312295
130.870948	4588.831733	24.317312
130.838964	4580.031244	24.322330
131.234859	4602.597707	24.327347
131.366394	4614.791382	24.332365
131.618325	4604.546226	24.337383
131.823025	4598.755655	24.342400
131.794972	4605.944626	24.347418
131.701164	4614.484327	24.352435
131.982990	4634.321849	24.357453
132.124708	4647.944680	24.362471
132.159292	4648.329116	24.367488
132.533077	4642.061737	24.372506
132.506954	4649.506728	24.377523
132.315324	4654.868282	24.382541
133.501955	4645.335250	24.387559
133.479633	4647.975319	24.392576
133.766618	4650.778074	24.397594
134.114693	4637.035648	24.402611
133.555018	4627.542350	24.407629
133.998181	4607.761751	24.412647
133.535573	4612.451087	24.417664
134.060437	4602.147053	24.422682
133.903222	4616.745697	24.427699
133.781244	4639.977358	24.432717
134.047836	4635.512472	24.437735
134.014354	4644.565488	24.442752
134.203173	4646.938761	24.447770
134.397869	4647.085306	24.452787
134.493440	4661.932796	24.457805
134.776897	4666.583913	24.462823
134.695342	4677.548186	24.467840
134.991263	4666.179100	24.472858
135.083450	4675.975206	24.477875
134.728846	4688.131148	24.482893
134.962918	4695.092975	24.487911
135.149504	4706.893737	24.492928
135.482157	4728.926303	24.497946
135.868743	4730.630245	24.502963
135.559656	4750.787623	24.507981
135.547942	4733.218424	24.512999
135.966725	4760.882531	24.518016
135.920969	4748.774110	24.523034
136.314217	4777.279147	24.528051
136.304011	4787.322182	24.533069
136.527626	4783.096265	24.538087
136.427786	4791.548863	24.543104
136.931096	4802.146478	24.548122
137.223010	4821.344722	24.553139
137.164275	4832.400616	24.558157
137.012021	4835.026356	24.563175
137.411907	4844.572494	24.568192
137.672935	4853.953770	24.573210
137.819125	4856.992839	24.578227
137.970783	4874.010193	24.583245
138.165445	4870.717859	24.588263
138.413539	4869.165671	24.593280
138.280964	4855.967478	24.598298
138.980376	4864.612879	24.603315
138.956717	4881.999793	24.608333
139.160773	4897.554842	24.613351
139.148941	4887.161336	24.618368
139.296146	4890.890069	24.623386
139.398472	4892.007873	24.628403
139.357204	4888.364721	24.633421
139.267971	4902.371244	24.638439
139.315370	4916.736733	24.643456
139.397152	4920.038055	24.648474
139.843505	4919.939064	24.653491
139.727342	4930.854503	24.658509
140.164513	4948.168493	24.663527
140.339757	4954.898796	24.668544
140.533865	4963.264328	24.673562
140.726327	4982.712691	24.678579
140.785493	4987.838411	24.683597
141.218361	4981.141015	24.688615
141.395527	4983.370582	24.693632
141.349301	4983.422283	24.698650
141.848985	4975.364901	24.703667
141.266336	4983.464269	24.708685
141.666630	4994.953138	24.713703
141.875877	5007.419346	24.718720
142.100979	5004.768868	24.723738
142.248392	5006.278087	24.728755
141.964996	5005.304701	24.733773
142.349256	5008.011519	24.738791
142.963215	5025.926760	24.743808
143.127285	5020.648309	24.748826
143.072964	5021.513632	24.753843
142.864241	5018.085146	24.758861
142.971253	5015.287628	24.763879
143.336332	5019.068588	24.768896
143.197173	5019.338815	24.773914
143.281802	5024.372929	24.778931
143.596032	5035.858331	24.783949
143.674193	5041.786128	24.788967
144.078935	5044.637221	24.793984
144.037111	5047.241599	24.799002
144.312904	5043.173936	24.804019
144.167269	5053.256058	24.809037
144.466309	5059.452119	24.814055
144.561714	5071.059541	24.819072
144.040990	5073.107165	24.824090
144.717455	5076.164177	24.829107
144.834032	5087.819299	24.834125
145.223063	5096.030241	24.839143
145.241311	5089.999010	24.844160
145.451628	5111.347535	24.849178
145.861132	5124.482788	24.854195
145.664720	5135.476596	24.859213
145.687120	5124.743383	24.864231
145.885904	5145.437098	24.869248
146.222986	5160.475888	24.874266
146.579648	5156.028652	24.879283
146.320884	5161.299099	24.884301
146.515171	5164.633856	24.889319
146.596083	5182.935422	24.894336
146.544063	5186.038412	24.899354
146.654684	5191.135222	24.904371
146.679737	5211.371064	24.909389
147.460232	5218.726747	24.914407
147.569192	5220.932970	24.919424
147.619338	5234.321810	24.924442
148.157743	5237.285514	24.929459
147.992832	5240.305976	24.934477
148.173577	5233.308364	24.939495
148.534965	5236.337935	24.944512
148.643459	5256.427356	24.949530
149.013608	5257.954527	24.954547
149.231092	5265.588323	24.959565
149.243519	5266.468224	24.964583
149.688718	5269.749732	24.969600
149.291357	5265.212468	24.974618
149.549081	5266.588118	24.979635
149.428415	5265.868172	24.984653
149.347137	5262.087827	24.989671
149.666542	5282.291660	24.994688
149.783312	5290.479575	24.999706
150.009079	5291.928626	25.004723
149.912829	5305.107045	25.009741
150.250333	5310.613700	25.014759
150.264550	5319.278471	25.019776
150.207779	5334.031285	25.024794
150.589607	5340.132667	25.029811
150.609531	5343.331293	25.034829
150.850227	5354.924763	25.039847
151.466253	5367.213793	25.044864
151.186432	5379.884354	25.049882
151.397967	5379.679265	25.054899
151.626590	5395.252407	25.059917
151.739668	5402.039244	25.064935
152.098712	5405.768928	25.069952
152.350062	5402.178105	25.074970
152.465845	5395.005305	25.079987
152.623327	5408.630134	25.085005
152.936508	5414.098320	25.090023
153.412037	5416.292037	25.095040
153.248694	5427.426667	25.100058
153.532998	5415.259254	25.105075
153.830850	5407.058210	25.110093
153.698924	5408.125377	25.115111
153.753098	5421.777131	25.120128
153.556809	5410.939288	25.125146
153.747576	5407.214362	25.130163
153.796554	5411.244526	25.135181
153.880278	5424.337788	25.140199
154.015689	5430.051523	25.145216
154.135764	5447.551946	25.150234
154.212109	5452.741130	25.155251
154.517000	5467.595354	25.160269
154.390569	5491.827172	25.165287
154.603875	5491.806065	25.170304
154.620745	5509.175560	25.175322
154.908209	5514.173166	25.180339
155.328726	5535.787970	25.185357
155.366744	5544.018956	25.190375
155.408811	5540.069717	25.195392
155.806272	5555.268225	25.200410
156.190601	5554.420328	25.205427
155.792498	5559.572574	25.210445
156.014993	5577.442490	25.215463
156.575681	5586.129725	25.220480
156.372924	5610.535384	25.225498
156.880698	5603.013427	25.230515
156.879024	5623.032534	25.235533
156.807241	5633.171731	25.240551
157.133113	5654.096729	25.245568
157.217011	5660.250222	25.250586
157.820351	5665.712684	25.255603
158.138731	5678.271646	25.260621
158.999505	5664.278624	25.265639
159.158544	5658.694055	25.270656
159.108583	5665.668598	25.275674
159.516848	5667.375366	25.280691
159.350850	5634.808479	25.285709
159.179126	5634.137509	25.290727
159.626248	5642.182034	25.295744
159.417271	5662.327977	25.300762
159.530000	5656.609309	25.305779
159.817358	5669.413975	25.310797
159.754598	5655.064041	25.315815
160.117883	5660.348815	25.320832
159.627989	5656.962709	25.325850
160.032699	5674.871930	25.330867
160.286147	5687.524318	25.335885
159.629675	5696.042209	25.340903
159.975392	5702.177263	25.345920
160.481975	5716.518014	25.350938
160.659030	5724.674144	25.355955
160.800024	5749.295305	25.360973
160.843306	5749.870485	25.365991
161.040097	5758.980991	25.371008
160.913714	5777.088336	25.376026
161.258175	5786.404412	25.381043
161.410981	5806.808918	25.386061
161.791406	5806.169559	25.391079
161.975395	5823.544863	25.396096
162.065671	5827.037522	25.401114
162.886879	5822.125488	25.406131
162.885260	5828.064403	25.411149
162.848670	5853.908163	25.416167
163.091478	5858.511230	25.421184
163.445916	5852.081584	25.426202
163.511355	5860.439720	25.431219
163.729980	5861.604529	25.436237
163.546600	5859.820345	25.441255
163.542982	5864.970509	25.446272
163.849440	5884.158994	25.451290
164.023879	5890.876840	25.456307
163.978982	5891.130717	25.461325
164.215714	5918.304435	25.466343
164.803442	5911.514908	25.471360
164.861179	5928.363073	25.476378
164.696284	5921.156085	25.481395
165.019865	5935.398515	25.486413
164.969984	5938.432392	25.491431
165.553692	5952.689345	25.496448
165.475477	5956.661913	25.501466
165.456208	5964.530873	25.506483
165.553985	5972.566352	25.511501
165.507100	5979.968942	25.516519
166.078779	6001.320398	25.521536
166.177395	5998.540631	25.526554
166.419700	6012.187014	25.531571
166.828082	6024.240359	25.536589
166.483607	6047.350607	25.541607
167.138612	6042.981801	25.546624
167.067562	6063.137756	25.551642
167.304811	6054.860942	25.556659
167.468245	6059.170835	25.561677
167.439511	6075.337269	25.566695
168.041018	6081.089993	25.571712
168.031461	6089.514196	25.576730
168.398090	6091.668122	25.581747
168.516590	6103.937959	25.586765
168.738654	6120.261457	25.591783
169.081813	6100.399034	25.596800
168.816092	6115.839186	25.601818
169.171406	6140.231026	25.606835
169.508190	6141.162910	25.611853
169.254293	6148.231218	25.616871
169.633790	6151.253253	25.621888
169.778975	6164.448020	25.626906
169.906795	6174.686104	25.631923
170.021232	6180.070451	25.636941
170.070489	6195.455485	25.641959
170.435561	6207.292466	25.646976
170.736484	6209.119412	25.651994
171.088291	6216.563340	25.657011
171.454796	6238.639695	25.662029
171.146318	6240.598839	25.667047
171.515720	6227.428377	25.672064
171.330947	6244.600467	25.677082
171.657827	6252.593509	25.682100
171.842327	6255.851758	25.687117
171.912695	6261.201674	25.692135
172.262425	6264.797255	25.697152
172.429572	6279.713206	25.702170
172.427659	6286.735214	25.707188
172.512037	6288.355387	25.712205
172.707792	6305.738732	25.717223
172.780788	6302.972595	25.722240
173.020449	6321.910402	25.727258
173.040152	6336.901173	25.732276
173.731261	6344.996314	25.737293
173.581004	6365.859571	25.742311
173.813289	6365.117875	25.747328
174.001482	6388.869876	25.752346
174.309034	6391.479358	25.757364
174.444680	6386.366988	25.762381
174.184678	6398.218405	25.767399
174.459612	6409.527813	25.772416
174.489459	6429.509268	25.777434
174.499261	6439.459880	25.782452
174.657329	6450.639781	25.787469
174.696003	6461.383426	25.792487
175.433551	6461.480461	25.797504
175.519484	6475.382263	25.802522
175.889074	6491.846369	25.807540
176.356461	6496.933877	25.812557
176.396398	6503.219792	25.817575
176.141661	6501.362269	25.822592
176.884377	6517.817516	25.827610
176.787864	6532.646539	25.832628
177.049065	6518.640003	25.837645
176.945533	6545.694617	25.842663
177.710462	6552.359282	25.847680
177.549613	6560.952070	25.852698
177.414422	6564.074194	25.857716
178.253333	6580.815247	25.862733
178.234636	6591.314866	25.867751
178.283859	6596.575459	25.872768
178.794017	6584.590343	25.877786
178.646336	6595.817717	25.882804
178.920168	6605.308977	25.887821
179.098933	6606.134692	25.892839
179.106909	6611.217029	25.897856
179.483528	6621.497776	25.902874
179.356624	6635.285250	25.907892
179.871798	6634.794497	25.912909
180.105892	6640.551436	25.917927
180.002576	6651.367500	25.922944
180.170170	6669.119754	25.927962
180.495813	6664.379920	25.932980
180.379643	6673.356017	25.937997
180.467887	6684.396410	25.943015
180.991928	6685.109948	25.948032
180.859661	6711.475753	25.953050
181.173270	6724.334436	25.958068
181.475343	6721.268117	25.963085
181.758410	6736.499275	25.968103
182.159501	6749.797949	25.973120
182.973197	6733.516014	25.978138
182.949109	6733.412849	25.983156
183.320911	6736.689867	25.988173
183.032354	6733.563623	25.993191
183.115878	6739.032814	25.998208
183.111541	6742.727175	26.003226
183.310632	6748.712818	26.008244
183.435077	6771.081939	26.013261
183.599776	6760.138230	26.018279
183.900680	6763.939674	26.023296
184.307640	6772.171772	26.028314
184.026117	6782.565309	26.033332
184.282846	6789.670028	26.038349
184.228433	6789.380495	26.043367
184.816269	6804.488905	26.048384
184.675789	6813.706945	26.053402
184.793393	6821.626173	26.058420
185.322666	6833.523131	26.063437
185.295439	6850.265037	26.068455
185.817452	6844.849258	26.073472
185.412542	6843.659951	26.078490
185.430316	6869.849228	26.083508
185.672851	6879.054424	26.088525
185.571423	6903.232303	26.093543
185.991282	6911.016576	26.098560
186.802623	6926.010204	26.103578
186.938148	6933.186995	26.108596
187.148975	6933.805811	26.113613
187.413019	6938.423803	26.118631
187.497609	6939.417098	26.123648
187.852302	6954.315303	26.128666
188.081311	6961.112800	26.133684
188.289290	6956.505732	26.138701
188.158248	6963.190243	26.143719
188.147566	6970.772396	26.148736
188.579860	6981.678967	26.153754
188.465845	6988.972623	26.158772
188.813028	6976.436846	26.163789
188.780265	7002.203888	26.168807
189.251902	7024.133238	26.173824
189.334252	7026.294890	26.178842
189.461269	7051.455953	26.183860
190.050006	7057.593130	26.188877
189.857375	7067.551597	26.193895
189.946835	7069.759335	26.198912
190.464267	7083.396632	26.203930
190.599312	7082.395317	26.208948
190.905855	7103.444762	26.213965
191.061618	7121.958711	26.218983
190.878128	7110.748595	26.224000
191.214492	7124.477277	26.229018
191.244545	7139.698652	26.234036
191.803245	7144.585415	26.239053
191.826034	7166.996310	26.244071
191.680257	7173.413989	26.249088
191.850419	7181.567291	26.254106
191.663764	7206.332293	26.259124
192.365149	7220.613490	26.264141
192.553761	7239.947544	26.269159
193.008581	7252.377719	26.274176
193.279117	7263.719185	26.279194
193.176624	7282.185422	26.284212
193.650526	7285.432297	26.289229
194.215552	7289.656484	26.294247
194.441180	7313.362740	26.299264
195.063555	7287.015689	26.304282
195.174173	7302.668112	26.309300
194.926922	7300.878562	26.314317
195.121703	7301.325987	26.319335
195.346084	7315.152098	26.324352
195.648970	7307.074861	26.329370
195.479492	7324.896937	26.334388
195.794767	7315.231434	26.339405
195.901238	7341.940040	26.344423
196.126461	7348.764321	26.349440
196.324034	7351.666222	26.354458
196.407832	7364.684691	26.359476
196.362058	7375.164103	26.364493
196.903978	7375.911741	26.369511
197.211608	7392.149963	26.374528
197.443979	7407.873734	26.379546
197.448827	7390.015686	26.384564
197.683202	7403.340099	26.389581
198.024630	7423.735226	26.394599
198.296940	7439.720214	26.399616
198.452401	7428.160091	26.404634
198.400474	7436.188763	26.409652
198.449441	7450.436989	26.414669
198.625659	7459.290399	26.419687
198.891295	7465.025890	26.424704
199.418761	7475.913142	26.429722
199.376301	7482.005923	26.434740
199.586471	7478.554542	26.439757
199.863341	7498.770622	26.444775
199.667431	7507.635139	26.449792
199.906087	7507.797297	26.454810
200.163979	7521.132100	26.459828
200.637680	7532.668598	26.464845
200.634508	7533.963120	26.469863
200.795472	7550.339942	26.474880
200.599868	7565.740782	26.479898
200.816731	7585.241502	26.484916
200.898251	7608.715252	26.489933
201.134791	7609.222733	26.494951
201.076605	7651.868769	26.499968
201.655869	7658.106200	26.504986
201.692619	7679.093876	26.510004
201.846057	7696.694467	26.515021
202.276849	7706.433760	26.520039
203.138452	7716.991881	26.525056
203.299114	7726.830954	26.530074
203.301375	7729.755745	26.535092
203.806114	7734.689416	26.540109
204.379068	7742.228276	26.545127
204.228696	7757.818732	26.550144
204.532309	7751.846447	26.555162
204.666440	7745.883265	26.560180
204.780570	7754.635258	26.565197
204.743142	7761.692932	26.570215
205.072439	7790.946498	26.575232
205.131192	7785.280873	26.580250
205.342648	7812.666031	26.585268
205.555182	7813.918635	26.590285
205.669820	7814.900721	26.595303
205.792085	7844.418577	26.600320
206.519869	7847.751218	26.605338
206.253279	7849.145212	26.610356
206.700328	7869.271426	26.615373
206.592745	7872.211242	26.620391
206.864248	7889.440472	26.625408
206.981441	7889.416347	26.630426
207.243823	7910.603336	26.635444
207.611806	7932.161204	26.640461
207.885267	7935.928088	26.645479
208.290238	7952.357949	26.650496
208.373432	7955.482856	26.655514
208.702461	7955.561564	26.660532
208.896199	7982.116634	26.665549
209.325964	7985.803358	26.670567
209.370953	7997.493733	26.675584
209.425697	7989.632004	26.680602
209.709147	8002.768448	26.685620
209.993684	8007.894541	26.690637
210.398653	8006.516979	26.695655
210.123460	8028.890116	26.700672
210.506140	8039.328317	26.705690
210.685225	8042.266481	26.710708
210.692270	8059.581338	26.715725
210.794829	8068.689063	26.720743
211.185122	8081.276268	26.725760
211.188216	8098.849376	26.730778
211.665851	8106.703462	26.735796
211.745536	8119.602725	26.740813
212.311813	8129.345100	26.745831
212.117098	8147.833884	26.750848
212.585500	8157.906714	26.755866
212.586312	8160.801106	26.760884
213.024115	8176.189247	26.765901
213.112103	8192.420476	26.770919
213.413756	8203.125005	26.775936
213.431297	8195.627697	26.780954
213.823509	8221.228052	26.785972
213.586769	8223.834835	26.790989
213.702331	8238.701303	26.796007
213.764705	8260.965431	26.801024
214.090382	8274.412543	26.806042
214.520147	8289.576857	26.811060
214.666245	8296.361852	26.816077
214.859498	8319.844187	26.821095
214.964132	8334.403007	26.826112
215.575591	8348.577218	26.831130
215.535395	8359.825888	26.836148
215.676865	8377.761601	26.841165
216.050494	8388.566996	26.846183
216.175076	8409.180385	26.851200
216.764897	8423.687476	26.856218
216.779541	8436.490623	26.861236
217.337600	8452.667292	26.866253
217.547648	8445.616162	26.871271
217.520785	8458.938158	26.876288
217.986513	8470.860247	26.881306
218.647157	8471.627711	26.886324
218.299782	8479.242588	26.891341
218.702808	8482.429751	26.896359
219.355888	8493.071686	26.901376
219.580459	8487.250026	26.906394
219.816291	8495.872837	26.911412
219.511788	8489.440734	26.916429
219.906856	8498.008093	26.921447
219.841870	8529.315418	26.926464
220.195739	8527.751706	26.931482
220.195959	8526.768642	26.936500
220.472039	8539.009611	26.941517
220.990116	8543.546722	26.946535
220.887022	8574.674546	26.951552
221.201273	8583.816904	26.956570
221.595476	8588.291791	26.961588
221.448977	8611.992165	26.966605
221.566050	8605.802271	26.971623
222.059900	8632.094602	26.976640
221.916026	8648.317349	26.981658
222.344196	8664.975691	26.986676
222.298854	8687.202290	26.991693
222.632767	8697.107073	26.996711
223.003703	8719.337403	27.001728
223.295753	8736.666558	27.006746
223.152946	8744.587244	27.011764
223.422287	8760.363751	27.016781
224.066908	8779.396708	27.021799
224.247600	8788.514780	27.026816
224.502560	8807.944548	27.031834
224.637222	8815.204255	27.036852
224.743413	8837.917225	27.041869
225.177699	8849.138256	27.046887
225.003564	8859.334240	27.051904
225.362478	8874.648665	27.056922
225.643328	8888.904768	27.061940
225.832538	8902.942086	27.066957
226.045318	8908.953859	27.071975
226.695760	8926.500479	27.076992
226.862436	8922.809433	27.082010
227.868504	8937.766512	27.087028
228.109267	8947.846741	27.092045
228.555073	8936.854300	27.097063
228.553403	8950.190661	27.102080
228.775110	8942.682109	27.107098
228.519947	8935.936841	27.112116
228.393692	8936.275098	27.117133
228.723241	8945.174110	27.122151
228.683573	8954.984032	27.127168
229.017645	8961.803631	27.132186
229.080877	8977.688451	27.137204
229.170868	9002.355407	27.142221
229.511939	9008.757189	27.147239
229.584643	9018.882559	27.152256
230.137507	9031.222323	27.157274
229.900004	9042.905006	27.162292
230.100442	9072.716276	27.167309
230.284333	9084.955571	27.172327
230.732350	9098.309129	27.177344
230.910307	9107.127729	27.182362
231.464194	9125.563277	27.187380
230.975634	9150.060604	27.192397
231.446234	9161.660247	27.197415
231.692938	9181.205263	27.202432
231.921367	9197.252840	27.207450
232.316527	9231.824526	27.212468
232.242941	9257.378273	27.217485
232.934581	9254.233717	27.222503
233.067372	9278.979101	27.227520
233.945646	9293.489745	27.232538
234.197558	9292.419361	27.237556
233.893966	9310.981834	27.242573
234.501116	9324.156477	27.247591
234.902912	9318.448594	27.252608
234.856439	9346.205121	27.257626
235.314230	9340.950355	27.262644
235.292232	9368.539037	27.267661
235.943850	9366.858309	27.272679
235.837171	9392.585520	27.277696
236.036283	9395.775055	27.282714
236.499406	9390.403601	27.287732
236.143934	9411.820712	27.292749
236.937029	9418.245649	27.297767
237.451526	9445.474066	27.302784
237.463543	9450.486541	27.307802
237.735149	9443.135715	27.312820
237.727423	9454.830359	27.317837
237.921212	9468.635049	27.322855
238.133099	9468.703981	27.327872
238.043260	9492.466408	27.332890
238.607401	9497.629498	27.337908
238.691293	9517.226247	27.342925
238.989049	9534.227646	27.347943
239.281944	9559.232949	27.352960
239.289586	9574.375290	27.357978
239.594381	9590.263346	27.362996
239.177501	9598.731507	27.368013
240.028979	9622.384287	27.373031
240.290201	9640.639566	27.378048
240.303349	9665.262742	27.383066
240.771253	9682.582780	27.388084
241.122788	9693.217847	27.393101
241.434585	9709.003249	27.398119
242.146358	9709.467731	27.403136
242.159093	9716.577062	27.408154
242.531103	9728.338350	27.413172
242.739147	9752.381211	27.418189
242.904133	9749.366114	27.423207
242.958542	9756.984530	27.428224
243.411208	9784.355292	27.433242
243.585272	9786.046082	27.438260
243.647233	9809.912298	27.443277
243.783232	9813.581037	27.448295
244.101481	9836.466777	27.453312
244.244163	9851.334211	27.458330
244.222018	9851.455992	27.463348
244.441587	9871.725528	27.468365
244.785363	9881.716860	27.473383
245.496528	9908.269219	27.478400
245.338584	9914.907423	27.483418
245.910148	9927.960050	27.488436
245.944608	9952.439933	27.493453
246.113734	9949.839245	27.498471
246.243228	9972.915488	27.503488
246.379867	9981.664203	27.508506
246.855133	10003.133903	27.513524
246.783664	10021.653334	27.518541
247.062602	10027.089012	27.523559
247.277322	10043.571382	27.528576
247.601573	10068.833830	27.533594
248.036823	10091.420173	27.538612
247.973567	10104.498270	27.543629
247.952138	10122.948895	27.548647
248.439843	10150.403510	27.553664
248.719931	10178.926773	27.558682
249.111275	10192.929469	27.563700
249.058085	10222.900593	27.568717
249.961285	10241.472719	27.573735
250.547389	10239.523084	27.578752
250.691272	10257.354172	27.583770
251.419804	10261.133866	27.588788
251.600735	10255.933213	27.593805
251.713790	10278.142948	27.598823
251.914312	10277.635561	27.603840
251.858691	10287.100756	27.608858
252.308397	10304.034546	27.613876
252.222591	10319.130013	27.618893
252.487333	10333.037953	27.623911
253.343912	10339.522890	27.628928
253.268583	10340.651533	27.633946
253.771988	10345.617762	27.638964
253.832711	10375.186719	27.643981
254.041356	10368.741539	27.648999
254.352841	10389.495977	27.654016
254.346621	10408.774703	27.659034
254.939451	10408.434093	27.664052
254.666301	10427.604122	27.669069
254.882610	10441.694250	27.674087
255.132851	10455.619660	27.679104
255.245275	10482.290808	27.684122
255.713860	10494.826033	27.689140
255.841891	10520.449320	27.694157
255.803558	10522.497473	27.699175
256.210681	10545.083591	27.704192
256.640896	10559.421285	27.709210
257.222402	10582.298473	27.714228
257.561623	10597.961274	27.719245
257.748379	10609.727038	27.724263
258.146385	10614.942367	27.729280
258.271387	10642.293901	27.734298
258.307341	10651.147848	27.739316
258.869569	10663.136784	27.744333
259.287407	10675.868024	27.749351
259.305828	10682.957151	27.754368
259.507134	10704.512448	27.759386
259.969869	10703.329941	27.764404
260.159532	10725.020321	27.769421
260.000901	10743.501420	27.774439
260.682396	10755.907142	27.779456
260.386051	10776.786141	27.784474
261.049522	10783.081806	27.789492
261.289335	10813.776848	27.794509
261.251330	10822.328790	27.799527
261.925117	10834.643678	27.804544
262.233113	10833.651372	27.809562
262.779744	10855.925770	27.814580
262.638427	10860.266058	27.819597
263.072251	10869.161525	27.824615
263.284760	10893.166765	27.829632
263.065741	10897.143346	27.834650
263.242797	10907.065972	27.839668
263.816914	10927.806076	27.844685
264.058982	10939.811881	27.849703
264.481118	10950.826072	27.854720
264.314305	10972.466183	27.859738
265.138936	10986.707586	27.864756
265.376680	10986.806131	27.869773
265.243091	11004.898170	27.874791
265.770556	11020.258501	27.879808
265.635148	11047.791614	27.884826
265.973405	11050.935648	27.889844
266.133025	11075.184656	27.894861
266.385694	11091.506645	27.899879
266.607616	11116.534778	27.904896
266.796727	11143.212475	27.909914
267.226359	11158.795503	27.914932
267.349799	11184.388311	27.919949
267.828721	11200.413848	27.924967
268.298905	11207.081154	27.929984
268.595915	11241.533183	27.935002
269.186236	11246.346686	27.940020
269.385932	11257.628663	27.945037
269.482726	11280.941440	27.950055
270.048388	11283.331848	27.955072
270.262885	11295.108501	27.960090
270.427089	11307.326757	27.965108
270.752712	11328.355016	27.970125
270.822076	11334.340196	27.975143
271.384594	11357.417004	27.980160
271.665781	11370.651141	27.985178
272.059719	11371.895334	27.990196
272.404073	11391.607328	27.995213
272.186947	11395.563236	28.000231
272.587272	11410.050800	28.005248
272.848617	11433.615492	28.010266
272.834919	11444.809173	28.015284
273.258662	11469.338924	28.020301
273.544115	11490.756903	28.025319
273.895535	11503.268951	28.030336
274.139983	11532.702546	28.035354
274.287325	11540.869736	28.040372
274.533751	11548.526608	28.045389
274.741301	11580.705578	28.050407
275.130185	11595.349610	28.055424
275.097883	11612.128082	28.060442
275.340525	11628.702009	28.065460
275.652624	11645.726133	28.070477
276.355284	11676.781226	28.075495
276.504958	11689.058895	28.080512
276.479220	11704.485285	28.085530
276.823556	11729.651712	28.090548
277.639752	11754.224201	28.095565
277.712150	11757.527322	28.100583
278.425748	11775.525163	28.105600
278.496168	11792.329393	28.110618
278.874226	11805.882707	28.115636
279.138666	11818.089518	28.120653
279.267845	11833.091014	28.125671
280.001709	11832.809017	28.130688
279.612571	11858.935853	28.135706
279.694343	11874.141386	28.140724
280.138624	11879.997074	28.145741
280.427564	11904.429226	28.150759
280.988903	11914.381948	28.155776
280.862101	11913.896293	28.160794
281.438334	11947.764048	28.165812
281.695185	11952.375245	28.170829
281.655835	11968.689649	28.175847
281.993331	11969.535911	28.180864
281.882257	12003.158090	28.185882
282.120573	12013.569185	28.190900
282.386041	12040.461863	28.195917
282.387188	12077.231144	28.200935
283.268297	12092.950052	28.205952
283.467894	12112.686848	28.210970
284.284361	12137.856269	28.215988
284.613507	12139.583141	28.221005
284.773990	12161.600142	28.226023
285.066074	12178.417787	28.231040
285.708372	12172.060173	28.236058
286.200874	12172.051248	28.241076
286.554922	12173.938667	28.246093
286.906884	12187.900774	28.251111
287.267787	12183.224403	28.256128
287.446315	12197.962040	28.261146
287.428793	12200.621478	28.266164
287.593557	12213.928331	28.271181
287.465612	12241.908954	28.276199
287.639967	12252.144055	28.281216
288.086615	12282.144371	28.286234
288.395482	12291.368535	28.291252
289.080525	12311.635161	28.296269
289.063012	12324.468003	28.301287
289.297589	12347.247465	28.306304
289.531556	12364.264775	28.311322
289.595164	12381.849923	28.316340
289.943821	12390.006345	28.321357
290.154933	12418.094339	28.326375
290.607931	12435.301649	28.331392
290.995452	12459.073110	28.336410
291.136593	12475.068279	28.341428
291.604911	12489.123299	28.346445
291.499231	12517.747545	28.351463
291.646362	12526.578641	28.356480
292.251142	12558.322071	28.361498
292.461656	12580.637066	28.366516
292.779603	12605.726499	28.371533
292.617842	12641.320138	28.376551
293.277363	12654.440830	28.381568
293.670684	12678.985332	28.386586
294.119754	12710.754789	28.391604
294.448537	12722.931172	28.396621
294.701797	12750.525884	28.401639
295.062548	12760.432700	28.406656
295.616180	12785.325902	28.411674
296.155008	12803.360864	28.416692
296.642791	12813.098607	28.421709
296.519725	12828.583120	28.426727
297.077936	12838.266698	28.431744
297.335172	12844.880056	28.436762
297.242375	12876.903240	28.441780
297.599114	12892.579571	28.446797
297.652921	12903.689051	28.451815
298.221346	12912.866750	28.456832
298.602505	12934.526897	28.461850
298.754026	12953.908670	28.466868
299.584016	12967.942173	28.471885
299.698748	12978.116677	28.476903
300.238271	12971.877371	28.481920
300.586541	12977.471994	28.486938
300.815480	12988.443872	28.491956
300.956859	13013.961776	28.496973
300.963618	13026.632802	28.501991
301.507452	13005.590179	28.507008
301.994052	13007.274588	28.512026
302.127044	13022.260015	28.517044
302.518051	13035.699562	28.522061
302.473681	13043.694342	28.527079
302.568827	13065.400342	28.532096
302.912957	13073.773738	28.537114
303.043800	13102.842124	28.542132
303.182356	13117.358720	28.547149
303.005266	13139.551009	28.552167
303.302215	13177.703140	28.557184
303.666194	13197.075316	28.562202
303.944963	13226.478758	28.567220
304.764283	13242.391007	28.572237
304.627134	13279.204781	28.577255
305.209014	13297.326154	28.582272
305.495997	13321.928598	28.587290
305.681051	13352.600497	28.592308
306.526629	13368.858357	28.597325
306.588846	13396.205244	28.602343
307.015526	13412.921575	28.607360
307.493921	13436.614856	28.612378
307.504817	13449.704690	28.617396
308.094095	13464.911392	28.622413
308.159120	13493.734498	28.627431
308.685988	13505.757411	28.632448
309.268646	13523.997096	28.637466
309.127195	13537.394239	28.642484
310.064144	13544.828462	28.647501
310.302024	13577.616239	28.652519
310.644585	13593.486266	28.657536
310.901787	13600.503347	28.662554
311.060756	13628.041071	28.667572
311.518893	13633.731231	28.672589
311.577918	13652.862811	28.677607
311.746443	13661.783967	28.682624
312.237153	13686.261909	28.687642
312.243236	13712.056971	28.692660
313.060752	13730.130447	28.697677
313.585861	13766.177220	28.702695
313.743646	13760.489188	28.707712
314.104538	13772.795005	28.712730
314.136122	13798.480412	28.717748
314.530636	13804.103928	28.722765
314.873179	13826.383071	28.727783
315.025308	13852.192047	28.732800
315.449850	13854.669990	28.737818
315.567843	13889.852983	28.742836
315.681645	13901.454351	28.747853
316.020939	13926.750318	28.752871
316.482319	13941.239532	28.757888
316.689729	13975.631049	28.762906
316.909347	14002.354133	28.767924
317.157643	14013.963303	28.772941
317.624835	14042.577539	28.777959
317.834975	14072.836935	28.782976
317.930368	14100.233106	28.787994
318.339805	14121.470994	28.793012
318.659212	14149.205292	28.798029
319.113053	14181.496883	28.803047
319.391731	14195.160816	28.808064
319.355201	14226.296457	28.813082
319.314163	14262.671095	28.818100
320.205164	14284.089655	28.823117
320.697269	14311.909163	28.828135
321.584391	14312.786884	28.833152
322.187470	14313.531882	28.838170
322.331551	14340.401952	28.843188
323.028087	14339.656490	28.848205
323.845412	14341.863178	28.853223
323.819320	14346.038802	28.858240
323.997927	14358.810124	28.863258
323.855882	14371.815657	28.868276
324.224715	14378.174826	28.873293
324.171376	14387.969829	28.878311
324.184529	14408.149959	28.883328
324.988426	14430.711438	28.888346
324.869808	14454.073048	28.893364
325.141173	14472.464514	28.898381
325.472138	14507.862649	28.903399
325.718437	14530.480142	28.908416
326.260501	14536.443571	28.913434
326.010513	14577.344739	28.918452
326.817708	14599.062801	28.923469
326.871757	14633.704824	28.928487
326.772222	14649.804939	28.933504
327.157804	14702.445945	28.938522
327.469416	14734.376034	28.943540
328.123967	14751.741625	28.948557
328.773313	14779.543835	28.953575
328.730287	14815.745109	28.958592
329.239557	14835.429337	28.963610
329.359734	14872.415375	28.968628
329.665169	14899.700970	28.973645
330.708051	14919.725796	28.978663
330.801194	14958.825096	28.983680
330.913244	14987.428751	28.988698
331.048093	15014.607190	28.993716
331.633633	15039.114058	28.998733
332.023257	15072.593683	29.003751
332.688241	15107.934787	29.008768
333.134998	15114.721063	29.013786
333.443627	15141.316268	29.018804
333.617805	15162.726765	29.023821
334.007170	15182.275202	29.028839
334.144482	15205.408065	29.033856
334.757002	15230.769663	29.038874
334.920150	15264.755160	29.043892
335.696151	15285.082988	29.048909
335.954414	15306.793400	29.053927
336.296829	15335.071204	29.058944
336.597102	15343.766642	29.063962
336.523767	15363.472113	29.068980
337.032227	15396.841365	29.073997
337.275814	15411.495529	29.079015
337.569509	15433.345246	29.084032
338.025608	15463.256121	29.089050
338.321036	15496.493716	29.094068
338.323150	15517.799146	29.099085
339.123831	15530.693982	29.104103
339.323128	15565.644944	29.109120
339.849847	15585.694404	29.114138
340.234555	15609.456767	29.119156
340.550880	15623.777600	29.124173
340.927631	15646.860499	29.129191
340.896759	15677.063402	29.134208
341.561529	15687.627838	29.139226
341.691208	15719.151781	29.144244
342.092302	15733.698260	29.149261
342.790306	15760.476004	29.154279
343.011500	15785.505961	29.159296
343.568633	15801.847022	29.164314
343.961097	15827.565836	29.169332
344.132817	15832.018060	29.174349
344.826037	15849.498216	29.179367
344.804451	15859.262061	29.184384
345.185679	15862.519728	29.189402
345.633425	15877.731591	29.194420
345.987832	15897.745286	29.199437
345.926548	15911.287157	29.204455
346.027825	15933.621652	29.209472
346.497036	15949.436809	29.214490
346.745090	15983.776989	29.219508
346.812610	16001.844520	29.224525
347.357556	16026.799295	29.229543
347.386970	16050.691918	29.234560
347.975607	16082.381872	29.239578
348.602864	16110.656514	29.244596
348.662078	16129.526191	29.249613
349.240399	16157.745958	29.254631
349.305460	16187.822053	29.259648
349.980371	16214.922721	29.264666
350.492471	16236.155864	29.269684
350.705170	16260.697796	29.274701
351.277816	16276.825579	29.279719
350.645814	16309.839787	29.284736
351.809572	16330.692736	29.289754
352.070506	16366.552498	29.294772
352.454634	16387.417689	29.299789
352.793495	16415.403223	29.304807
352.887391	16464.214635	29.309824
353.151075	16475.528291	29.314842
353.691872	16506.803004	29.319860
353.795785	16544.260452	29.324877
354.328906	16574.428571	29.329895
354.274625	16606.339231	29.334912
354.806803	16632.844766	29.339930
355.083649	16672.948578	29.344948
355.445364	16695.934570	29.349965
356.200993	16731.357202	29.354983
356.144423	16764.187417	29.360000
356.555720	16786.263810	29.365018
356.629573	16832.006204	29.370036
356.857413	16869.927788	29.375053
357.736757	16898.182634	29.380071
357.912652	16947.610807	29.385088
358.648158	16984.876653	29.390106
358.666986	17020.672238	29.395124
359.234394	17057.839929	29.400141
359.894328	17082.217786	29.405159
360.063440	17113.580278	29.410176
360.788304	17145.646971	29.415194
361.214983	17170.870482	29.420212
361.319388	17196.761973	29.425229
362.215619	17211.889953	29.430247
362.404173	17243.419705	29.435264
362.851971	17261.495149	29.440282
363.360350	17272.187327	29.445300
363.313347	17298.800654	29.450317
364.119037	17316.399350	29.455335
364.203964	17350.785098	29.460352
364.795849	17360.133254	29.465370
365.618145	17373.922824	29.470388
366.035565	17391.536883	29.475405
366.291342	17412.315826	29.480423
366.491977	17413.125897	29.485440
366.912388	17438.632991	29.490458
367.127550	17449.923812	29.495476
367.354763	17477.354294	29.500493
367.582795	17482.841096	29.505511
367.896809	17517.310712	29.510528
367.714590	17536.664796	29.515546
368.135237	17567.871537	29.520564
368.496348	17590.863610	29.525581
368.957950	17606.205615	29.530599
369.175318	17640.593731	29.535616
369.577892	17665.109543	29.540634
369.791967	17684.740366	29.545652
369.938788	17718.043263	29.550669
370.400136	17750.657480	29.555687
370.600715	17791.693967	29.560704
371.152970	17812.071364	29.565722
371.563202	17841.872788	29.570740
371.815690	17884.849132	29.575757
372.166104	17921.513979	29.580775
372.526918	17954.208256	29.585792
373.082350	17974.878507	29.590810
373.466714	18018.399278	29.595828
373.562132	18046.137777	29.600845
374.062886	18073.530365	29.605863
374.192465	18130.097474	29.610880
374.489635	18161.440802	29.615898
375.099209	18198.195854	29.620916
374.884369	18250.082070	29.625933
376.018137	18278.103381	29.630951
377.198449	18292.632167	29.635968
377.986026	18322.810320	29.640986
378.828654	18341.892006	29.646004
378.617399	18372.731781	29.651021
379.276254	18370.838570	29.656039
379.426417	18402.914385	29.661056
379.821144	18407.503858	29.666074
380.017433	18424.164082	29.671092
380.036071	18448.470214	29.676109
380.580536	18484.524185	29.681127
380.760801	18507.624649	29.686144
380.937734	18527.811155	29.691162
381.269512	18561.209721	29.696180
381.543758	18591.632373	29.701197
381.903475	18629.526757	29.706215
382.292656	18660.048769	29.711232
383.027584	18704.736636	29.716250
383.381417	18722.882801	29.721268
383.434819	18757.908779	29.726285
384.264642	18776.685705	29.731303
384.833195	18806.527343	29.736320
385.430542	18844.029868	29.741338
386.208377	18847.301434	29.746356
386.601807	18876.499044	29.751373
387.093565	18887.961111	29.756391
387.112112	18907.630417	29.761408
387.822270	18928.719249	29.766426
388.242688	18926.907929	29.771444
388.273723	18948.681181	29.776461
388.665749	18960.582227	29.781479
388.818039	18977.664849	29.786496
388.899875	19006.884214	29.791514
389.327888	19027.337234	29.796532
389.344735	19063.917849	29.801549
389.735590	19093.524536	29.806567
389.979695	19124.083982	29.811584
390.495810	19169.059887	29.816602
391.051096	19202.151691	29.821620
391.034277	19244.826105	29.826637
391.510124	19276.911285	29.831655
392.059084	19303.347409	29.836672
392.416227	19339.446798	29.841690
393.144248	19360.266826	29.846708
393.027478	19397.328968	29.851725
393.598845	19421.042354	29.856743
394.278832	19465.590018	29.861760
394.548984	19482.819208	29.866778
394.864460	19497.000106	29.871796
395.496715	19535.190457	29.876813
395.851749	19564.939471	29.881831
395.989394	19597.531985	29.886848
396.252567	19616.100812	29.891866
396.508598	19648.995452	29.896884
396.558735	19695.348703	29.901901
397.246852	19718.679081	29.906919
397.865068	19754.580181	29.911936
398.191162	19792.506420	29.916954
398.826886	19820.363558	29.921972
398.947893	19864.471811	29.926989
399.674255	19891.037205	29.932007
399.557396	19922.493245	29.937024
400.331869	19957.087346	29.942042
400.968388	19975.151926	29.947060
400.999857	20026.219514	29.952077
401.658266	20046.484393	29.957095
402.357217	20078.282036	29.962112
402.303659	20117.684212	29.967130
402.854758	20136.795641	29.972148
403.265137	20176.696712	29.977165
403.786618	20207.876006	29.982183
403.974805	20252.467611	29.987200
404.527126	20285.029224	29.992218
404.793154	20314.587767	29.997236
405.306767	20349.093355	30.002253
405.716996	20376.807385	30.007271
405.968980	20414.901776	30.012288
405.750647	20464.063466	30.017306
406.557392	20496.640215	30.022324
406.870774	20550.350708	30.027341
407.220018	20580.947482	30.032359
407.454121	20631.166830	30.037376
408.023139	20677.317277	30.042394
408.837398	20704.898895	30.047412
409.463912	20732.122181	30.052429
410.317588	20753.515961	30.057447
410.911165	20790.189537	30.062464
410.957908	20823.537261	30.067482
411.389548	20846.870604	30.072500
411.780811	20880.405885	30.077517
412.149955	20900.940302	30.082535
414.082473	20901.801824	30.087552
414.210899	20921.627193	30.092570
414.983769	20942.191134	30.097588
415.114584	20947.884330	30.102605
415.797582	20963.479802	30.107623
416.100134	20964.490777	30.112640
416.262668	20993.813801	30.117658
416.254033	20993.821498	30.122676
416.614073	21011.598658	30.127693
416.716495	21032.593499	30.132711
417.070389	21056.498066	30.137728
417.106794	21089.263138	30.142746
417.495873	21121.668899	30.147764
417.834546	21152.069823	30.152781
417.932784	21177.812462	30.157799
418.302052	21220.166439	30.162816
418.054388	21254.484351	30.167834
418.855294	21302.695013	30.172852
419.179392	21345.944363	30.177869
419.595553	21379.381939	30.182887
420.253134	21420.774398	30.187904
420.637320	21472.713569	30.192922
421.074045	21492.206480	30.197940
421.624017	21529.694504	30.202957
421.902139	21574.746168	30.207975
422.096653	21608.197166	30.212992
422.186792	21649.083253	30.218010
423.007685	21684.567188	30.223028
423.371589	21736.021785	30.228045
423.936794	21773.383288	30.233063
424.674255	21821.542861	30.238080
424.571402	21855.652039	30.243098
425.113337	21887.493258	30.248116
425.691075	21918.939202	30.253133
426.314678	21954.498868	30.258151
426.949852	22004.074309	30.263168
426.965804	22038.520545	30.268186
427.402752	22075.864493	30.273204
427.901093	22123.745958	30.278221
428.233666	22150.681139	30.283239
428.924158	22198.980413	30.288256
429.024563	22235.153695	30.293274
429.524461	22271.443951	30.298292
429.909247	22316.457909	30.303309
430.586047	22355.243318	30.308327
431.264071	22377.204255	30.313344
431.601646	22423.017772	30.318362
432.229398	22455.194329	30.323380
432.830633	22491.865637	30.328397
433.279905	22529.361491	30.333415
433.666988	22559.756968	30.338432
434.131278	22591.390038	30.343450
434.946544	22613.826840	30.348468
435.172217	22641.198281	30.353485
435.210644	22679.514409	30.358503
436.043371	22715.652889	30.363520
436.359536	22748.037570	30.368538
437.512360	22751.038291	30.373556
439.373998	22755.235296	30.378573
439.513501	22760.541387	30.383591
439.921186	22757.833069	30.388608
440.386530	22770.371167	30.393626
440.562024	22765.760313	30.398644
440.768297	22794.177393	30.403661
441.046963	22804.684055	30.408679
441.551420	22825.840189	30.413696
441.299169	22851.763115	30.418714
441.637131	22869.301507	30.423732
442.183809	22889.903635	30.428749
442.050445	22920.518179	30.433767
442.474470	22954.563041	30.438784
442.502749	22992.643476	30.443802
442.931749	23026.801185	30.448820
443.070255	23074.412111	30.453837
443.265050	23117.676339	30.458855
443.997371	23161.972928	30.463872
444.039669	23205.262571	30.468890
444.601430	23251.780788	30.473908
444.881588	23309.111555	30.478925
445.417179	23356.408557	30.483943
446.154684	23406.248727	30.488960
446.423056	23469.332350	30.493978
446.845834	23493.495474	30.498996
447.440122	23535.360851	30.504013
448.134478	23589.089071	30.509031
448.547727	23621.960799	30.514048
449.164320	23685.489113	30.519066
449.590193	23713.898269	30.524084
450.032943	23756.251217	30.529101
450.337503	23799.571587	30.534119
450.843945	23834.656316	30.539136
450.767169	23887.872696	30.544154
451.439875	23919.934249	30.549172
452.021962	23957.367186	30.554189
452.646578	24001.112968	30.559207
453.145864	24044.184199	30.564224
453.151659	24081.600655	30.569242
455.391104	24091.101465	30.574260
455.887864	24107.099605	30.579277
456.785789	24118.875034	30.584295
458.032198	24102.041709	30.589312
458.730363	24117.565085	30.594330
459.088243	24101.476144	30.599348
459.989668	24098.731786	30.604365
459.932207	24099.096022	30.609383
460.524071	24096.904223	30.614400
460.505209	24112.722641	30.619418
460.553362	24111.457938	30.624436
460.813774	24127.047327	30.629453
460.643068	24145.063695	30.634471
460.857988	24165.840447	30.639488
461.019369	24191.886310	30.644506
461.026492	24234.304531	30.649524
461.871967	24270.775372	30.654541
461.891881	24312.297619	30.659559
461.826154	24353.231766	30.664576
462.282447	24411.131631	30.669594
462.321668	24471.844284	30.674612
463.584116	24502.483405	30.679629
464.280212	24537.114092	30.684647
464.864093	24583.055190	30.689664
465.217630	24623.603784	30.694682
465.601259	24660.309439	30.699700
465.920141	24701.418996	30.704717
466.065443	24749.604325	30.709735
466.801943	24803.668461	30.714752
467.033199	24853.568133	30.719770
467.417750	24896.534331	30.724788
467.894805	24954.875719	30.729805
468.280632	25002.922689	30.734823
469.119560	25045.549289	30.739840
469.553833	25098.921572	30.744858
470.237445	25155.695208	30.749876
470.567919	25194.235269	30.754893
471.289182	25244.007834	30.759911
471.830765	25282.046456	30.764928
472.202513	25318.932108	30.769946
472.676365	25369.720443	30.774964
473.269256	25408.115140	30.779981
473.199249	25467.002801	30.784999
473.888849	25505.485820	30.790016
474.540812	25554.464926	30.795034
474.873026	25605.045549	30.800052
475.367980	25642.996485	30.805069
475.669336	25699.855576	30.810087
476.512662	25741.934414	30.815104
477.019854	25788.124819	30.820122
477.397235	25831.794727	30.825140
478.039372	25880.385305	30.830157
478.332672	25928.740327	30.835175
479.206052	25963.554371	30.840192
480.035326	25996.354085	30.845210
480.593110	26042.085804	30.850228
481.587800	26066.509787	30.855245
481.498326	26100.067026	30.860263
482.129704	26121.636828	30.865280
482.702148	26155.687248	30.870298
482.764344	26189.891408	30.875316
483.286183	26218.702070	30.880333
483.385427	26257.653320	30.885351
483.775939	26297.389205	30.890368
484.072145	26333.709187	30.895386
484.371358	26385.237465	30.900404
484.940495	26412.517246	30.905421
485.558222	26459.571181	30.910439
485.882501	26492.887370	30.915456
486.239911	26535.931564	30.920474
486.649441	26587.981572	30.925492
487.226154	26625.470152	30.930509
487.290517	26694.007066	30.935527
488.063624	26744.079807	30.940544
488.877370	26794.742107	30.945562
489.141262	26829.674363	30.950580
490.217208	26878.650310	30.955597
490.010653	26926.712220	30.960615
490.506497	26976.140684	30.965632
491.187238	27028.162998	30.970650
491.580594	27074.776252	30.975668
492.660505	27121.594796	30.980685
492.645399	27170.928433	30.985703
493.627170	27215.041394	30.990720
493.760246	27262.354220	30.995738
494.202728	27304.354867	31.000756
494.757290	27348.352639	31.005773
495.169148	27409.025192	31.010791
495.352855	27461.550429	31.015808
495.927825	27509.699358	31.020826
496.264314	27570.132588	31.025844
497.057723	27625.216641	31.030861
497.465806	27683.966689	31.035879
498.039721	27729.264950	31.040896
498.898703	27781.279025	31.045914
499.048794	27835.653055	31.050932
499.873098	27886.982387	31.055949
500.518192	27938.887170	31.060967
500.849128	27980.655547	31.065984
501.977270	28019.525995	31.071002
502.342027	28055.002393	31.076020
502.972906	28095.308361	31.081037
503.742026	28144.209269	31.086055
504.217120	28177.008575	31.091072
504.363498	28216.297140	31.096090
504.786262	28265.268221	31.101108
505.407115	28307.708697	31.106125
505.942247	28354.749916	31.111143
506.096683	28395.539046	31.116160
506.723414	28437.051476	31.121178
506.912306	28490.033218	31.126196
507.785871	28534.691068	31.131213
507.686216	28583.339268	31.136231
508.494099	28622.002160	31.141248
509.182925	28675.923929	31.146266
509.698115	28725.783218	31.151284
510.089718	28783.416741	31.156301
510.605062	28824.440632	31.161319
511.460113	28854.781063	31.166336
512.397735	28889.773393	31.171354
513.106694	28934.257579	31.176372
513.731270	28962.819282	31.181389
514.214927	29001.820485	31.186407
514.645319	29038.000977	31.191424
515.046324	29065.785915	31.196442
515.831286	29101.295995	31.201460
516.098872	29126.879130	31.206477
516.402209	29184.055386	31.211495
516.573520	29212.686063	31.216512
517.150004	29249.735601	31.221530
517.550164	29303.678616	31.226548
518.131749	29313.238628	31.231565
518.663049	29345.750111	31.236583
519.562692	29382.238668	31.241600
521.053944	29401.339328	31.246618
521.281053	29433.109422	31.251636
521.707360	29451.278785	31.256653
522.235521	29473.261016	31.261671
522.262574	29500.805580	31.266688
522.750338	29535.535983	31.271706
522.937255	29567.950192	31.276724
523.181544	29597.607316	31.281741
523.436761	29649.285097	31.286759
524.074374	29695.139510	31.291776
524.572232	29742.641768	31.296794
524.647194	29797.072216	31.301812
524.996245	29842.719155	31.306829
525.527310	29897.620335	31.311847
526.036967	29951.802804	31.316864
526.549669	30008.070187	31.321882
526.848332	30079.695483	31.326900
527.557315	30131.258730	31.331917
528.108664	30188.599223	31.336935
528.573456	30249.556906	31.341952
529.083363	30306.882550	31.346970
529.386155	30380.868147	31.351988
530.075707	30443.716938	31.357005
530.482904	30503.949962	31.362023
531.177052	30564.306154	31.367040
532.100721	30624.763455	31.372058
532.300524	30695.700931	31.377076
532.648932	30756.379899	31.382093
533.684383	30812.964195	31.387111
533.796674	30869.193228	31.392128
534.792839	30936.211173	31.397146
534.914479	31005.698963	31.402164
535.290745	31064.352127	31.407181
536.260914	31126.772129	31.412199
536.370802	31182.182292	31.417216
537.324411	31254.079651	31.422234
537.618803	31316.268065	31.427252
538.587812	31370.902779	31.432269
538.884295	31433.116502	31.437287
539.373077	31506.243228	31.442304
539.880614	31556.695552	31.447322
540.341239	31636.140562	31.452340
540.928526	31700.641885	31.457357
541.778597	31758.550252	31.462375
542.403316	31818.956944	31.467392
543.250972	31879.579422	31.472410
544.197951	31925.237150	31.477428
545.156913	31955.616312	31.482445
545.716250	32011.475436	31.487463
546.012798	32047.147918	31.492480
546.623655	32083.623577	31.497498
546.779620	32139.385671	31.502516
547.733750	32197.199422	31.507533
547.954627	32227.953376	31.512551
548.781678	32281.576353	31.517568
549.529689	32313.063713	31.522586
550.268096	32370.270025	31.527604
550.940026	32407.985696	31.532621
551.163332	32436.023055	31.537639
551.606778	32495.950886	31.542656
552.638510	32524.242937	31.547674
552.493596	32576.702198	31.552692
552.719824	32617.536656	31.557709
553.586663	32662.890869	31.562727
553.650349	32704.143616	31.567744
554.307866	32747.775191	31.572762
554.711340	32805.779707	31.577780
555.063318	32858.899203	31.582797
555.566853	32891.898305	31.587815
555.996805	32970.379445	31.592832
556.751851	33018.684239	31.597850
556.825965	33080.811150	31.602868
557.129540	33140.628598	31.607885
558.157787	33181.271939	31.612903
559.061544	33230.051281	31.617920
559.750110	33276.742801	31.622938
560.287974	33337.793794	31.627956
560.746636	33395.756424	31.632973
561.317517	33446.011228	31.637991
561.436716	33519.557596	31.643008
562.201891	33569.458816	31.648026
562.466801	33641.956143	31.653044
563.330023	33709.139145	31.658061
563.947059	33762.826559	31.663079
564.196011	33832.080432	31.668096
564.701180	33876.042875	31.673114
565.437917	33947.053062	31.678132
565.601224	34020.108289	31.683149
566.314419	34094.265739	31.688167
566.873303	34166.558882	31.693184
567.363898	34232.297117	31.698202
567.822953	34298.627720	31.703220
568.384663	34362.821140	31.708237
569.421829	34433.117846	31.713255
569.851244	34501.312679	31.718272
570.581635	34561.566146	31.723290
571.183603	34629.518396	31.728308
571.796926	34698.128535	31.733325
572.561386	34760.355564	31.738343
573.130225	34828.124712	31.743360
575.053576	34857.301951	31.748378
576.614230	34899.293928	31.753396
576.863273	34948.672100	31.758413
577.552398	34969.760542	31.763431
577.764152	35011.215086	31.768448
578.342342	35037.418199	31.773466
578.801426	35081.750975	31.778484
579.142816	35118.469899	31.783501
579.771974	35155.163457	31.788519
579.751931	35207.366881	31.793536
579.864414	35257.948666	31.798554
580.467901	35322.059756	31.803572
580.783151	35397.115144	31.808589
581.385068	35456.755421	31.813607
581.674246	35523.954896	31.818624
582.350642	35576.959515	31.823642
582.662078	35652.218568	31.828660
583.279990	35727.503054	31.833677
583.689550	35781.192960	31.838695
584.333966	35854.599106	31.843712
585.161784	35917.564463	31.848730
585.536865	35990.491800	31.853748
586.157967	36057.133533	31.858765
586.795282	36131.747492	31.863783
587.429814	36202.767774	31.868800
588.296366	36260.176900	31.873818
588.855087	36330.449660	31.878836
589.295211	36395.585662	31.883853
590.288854	36467.929933	31.888871
590.896746	36517.458295	31.893888
591.064601	36575.062729	31.898906
591.639532	36641.682703	31.903924
592.564983	36703.662690	31.908941
592.842529	36746.896616	31.913959
593.001949	36826.534520	31.918976
593.966655	36873.385532	31.923994
595.216385	36937.496658	31.929012
596.384518	36975.976395	31.934029
597.200645	37010.184412	31.939047
597.686280	37047.868121	31.944064
598.333855	37088.030984	31.949082
598.980428	37128.282470	31.954100
599.099693	37182.649397	31.959117
599.959490	37228.543472	31.964135
599.911607	37284.175455	31.969152
600.271106	37331.648360	31.974170
600.577002	37398.457595	31.979188
600.627076	37462.926538	31.984205
601.764059	37528.727929	31.989223
601.828974	37621.747573	31.994240
602.488937	37681.925344	31.999258
603.323147	37739.502345	32.004276
604.192847	37820.668481	32.009293
605.223941	37876.767919	32.014311
605.622725	37945.122942	32.019328
606.374208	38018.018422	32.024346
606.835764	38085.530395	32.029364
607.256565	38149.243053	32.034381
608.096662	38210.699474	32.039399
608.216409	38291.464515	32.044416
608.977147	38358.173769	32.049434
609.703336	38421.092089	32.054452
610.049664	38496.373052	32.059469
611.741103	38536.281517	32.064487
612.542238	38598.272777	32.069504
614.063869	38632.168513	32.074522
614.967575	38675.300486	32.079540
615.784014	38700.251302	32.084557
617.181665	38713.885749	32.089575
617.749705	38753.137527	32.094592
618.120900	38796.193616	32.099610
618.774157	38810.809582	32.104628
619.102062	38849.915013	32.109645
619.332018	38877.762539	32.114663
619.682079	38923.337960	32.119680
620.306381	38956.473508	32.124698
620.558959	38992.157660	32.129716
620.637358	39055.677558	32.134733
621.323310	39084.895670	32.139751
621.679761	39162.267196	32.144768
621.779034	39223.830478	32.149786
622.562533	39287.897558	32.154804
622.810437	39355.553709	32.159821
623.565929	39426.970718	32.164839
623.951867	39502.104119	32.169856
624.084048	39577.614317	32.174874
624.418341	39648.852409	32.179892
624.825801	39735.725009	32.184909
625.696353	39820.731845	32.189927
626.260960	39907.026933	32.194944
626.614415	39997.732148	32.199962
627.472383	40082.041548	32.204980
628.037806	40168.546064	32.209997
628.627822	40245.069238	32.215015
629.811963	40327.627706	32.220032
630.523862	40405.488722	32.225050
631.127924	40478.292166	32.230068
631.292353	40576.259945	32.235085
632.551336	40640.048072	32.240103
632.958488	40722.319987	32.245120
634.524758	40762.579167	32.250138
635.363826	40818.643661	32.255156
636.362242	40876.235060	32.260173
637.155065	40919.908358	32.265191
637.567871	40984.699201	32.270208
637.635317	41031.652350	32.275226
638.501297	41076.639726	32.280244
638.991494	41152.596048	32.285261
639.864885	41199.605917	32.290279
640.622755	41249.204517	32.295296
641.478794	41312.310255	32.300314
641.861057	41353.681729	32.305332
642.232804	41430.293258	32.310349
642.591236	41485.122831	32.315367
643.607445	41532.416169	32.320384
644.867444	41584.445494	32.325402
645.568295	41632.889716	32.330420
646.196351	41692.243175	32.335437
646.826173	41746.533098	32.340455
647.451219	41803.276776	32.345472
647.452713	41860.347745	32.350490
648.421768	41909.417638	32.355508
648.978220	41973.900979	32.360525
649.376160	42030.635515	32.365543
650.233063	42081.337518	32.370560
650.916943	42152.979036	32.375578
651.773701	42210.294968	32.380596
651.995105	42285.318588	32.385613
652.344295	42344.297190	32.390631
653.058434	42409.832503	32.395648
653.379580	42492.319117	32.400666
654.099634	42547.145796	32.405684
654.855228	42630.132670	32.410701
655.313913	42704.620014	32.415719
656.531872	42778.369814	32.420736
656.755302	42844.113991	32.425754
657.724293	42911.237977	32.430772
658.245919	42982.271807	32.435789
659.109822	43062.171007	32.440807
659.604119	43139.997465	32.445824
660.025813	43216.469258	32.450842
660.702542	43285.451837	32.455860
661.292110	43371.626479	32.460877
661.860140	43439.702574	32.465895
662.530556	43529.432058	32.470912
663.218821	43604.409177	32.475930
663.451539	43678.912503	32.480948
663.829057	43768.246365	32.485965
664.298079	43861.897108	32.490983
665.275628	43943.571422	32.496000
665.811552	44040.691175	32.501018
666.192770	44125.704010	32.506036
666.890976	44228.884950	32.511053
667.547808	44316.735643	32.516071
668.368754	44424.784734	32.521088
668.937887	44522.823423	32.526106
669.849465	44612.755097	32.531124
670.393720	44718.818325	32.536141
670.991632	44806.453733	32.541159
671.912335	44891.033660	32.546176
672.357074	44995.829879	32.551194
673.291328	45072.657200	32.556212
673.836445	45164.830609	32.561229
674.527715	45268.842512	32.566247
675.553379	45350.638186	32.571264
676.211020	45458.385549	32.576282
676.920555	45525.486051	32.581300
677.629579	45611.875500	32.586317
678.211310	45682.265593	32.591335
679.128642	45769.309684	32.596352
679.408589	45853.996632	32.601370
680.289892	45922.718380	32.606388
681.167710	46007.897729	32.611405
682.290072	46087.501993	32.616423
682.579250	46159.170456	32.621440
682.992403	46231.930164	32.626458
683.586255	46317.817738	32.631476
684.089941	46404.367892	32.636493
684.595046	46492.121240	32.641511
685.470185	46580.600121	32.646528
686.427732	46682.738177	32.651546
687.189738	46761.050202	32.656564
687.937296	46855.513006	32.661581
688.625418	46925.141829	32.666599
689.510220	47010.665592	32.671616
689.744857	47093.663630	32.676634
690.793267	47189.824609	32.681652
691.174329	47271.987725	32.686669
691.649976	47356.699633	32.691687
693.174458	47448.558299	32.696704
693.644211	47528.484848	32.701722
694.322314	47604.717498	32.706740
695.291496	47692.503993	32.711757
695.997587	47778.843875	32.716775
696.989325	47853.377372	32.721792
697.568873	47942.192499	32.726810
698.431325	48006.920874	32.731828
699.122616	48094.164615	32.736845
699.873330	48165.745527	32.741863
700.875927	48242.375568	32.746880
701.425032	48338.081697	32.751898
701.897655	48407.476836	32.756916
702.707268	48487.348144	32.761933
703.157093	48562.406559	32.766951
703.608277	48642.110343	32.771968
703.946342	48743.351303	32.776986
704.719635	48829.754344	32.782004
705.335387	48928.717760	32.787021
705.594819	49014.568595	32.792039
706.457901	49107.937208	32.797056
707.089319	49225.468602	32.802074
708.011235	49316.529487	32.807092
708.556288	49416.820853	32.812109
709.485898	49508.367723	32.817127
710.630006	49593.645564	32.822144
711.202549	49691.562119	32.827162
712.165789	49786.761841	32.832180
712.861146	49881.349389	32.837197
713.135022	49978.056643	32.842215
714.046601	50059.300966	32.847232
714.690588	50155.126872	32.852250
715.460845	50247.013097	32.857268
716.296403	50340.515452	32.862285
716.901379	50437.208241	32.867303
718.142616	50515.699786	32.872320
718.222871	50621.689556	32.877338
719.027553	50708.689662	32.882356
719.773975	50799.057029	32.887373
720.041320	50904.085768	32.892391
721.415082	50977.504051	32.897408
723.049590	51061.444124	32.902426
724.159050	51139.678896	32.907444
725.390438	51200.939871	32.912461
725.471372	51288.352694	32.917479
726.267129	51344.721136	32.922496
726.869223	51419.026553	32.927514
727.666593	51470.727019	32.932532
728.106977	51536.904649	32.937549
728.775890	51607.507595	32.942567
729.611367	51665.332760	32.947584
729.812948	51750.801120	32.952602
730.114961	51807.325099	32.957620
731.162909	51893.759773	32.962637
731.836976	51969.344074	32.967655
732.679168	52049.262766	32.972672
733.054074	52139.811484	32.977690
733.836534	52219.737586	32.982708
735.212096	52288.378597	32.987725
735.528483	52371.029133	32.992743
736.369350	52449.954763	32.997760
736.784677	52539.930139	33.002778
737.742212	52617.845399	33.007796
738.755885	52698.505988	33.012813
738.986351	52776.946258	33.017831
739.656398	52877.670909	33.022848
740.486444	52964.566449	33.027866
741.192609	53050.484706	33.032884
741.565965	53138.467209	33.037901
742.664052	53220.411077	33.042919
743.954002	53309.057921	33.047936
744.530829	53389.351309	33.052954
745.567550	53481.136281	33.057972
746.179624	53553.849936	33.062989
746.758834	53652.256147	33.068007
747.435860	53730.967661	33.073024
748.083533	53821.750829	33.078042
748.597175	53918.943612	33.083060
749.211987	54010.674402	33.088077
749.870479	54101.362321	33.093095
751.337070	54192.416304	33.098112
752.041694	54275.958467	33.103130
753.349355	54360.241656	33.108148
754.197733	54440.071240	33.113165
755.486727	54503.174777	33.118183
756.704552	54552.157413	33.123200
757.188363	54634.088635	33.128218
757.694796	54705.535197	33.133236
758.381020	54783.156452	33.138253
759.040765	54862.747245	33.143271
759.668371	54933.403848	33.148288
760.173777	55015.358369	33.153306
760.673339	55105.053683	33.158324
761.044378	55185.451617	33.163341
761.518807	55289.443187	33.168359
762.556749	55383.865190	33.173376
762.639936	55485.155104	33.178394
762.870435	55591.867417	33.183412
763.686043	55691.255734	33.188429
764.350453	55809.156493	33.193447
765.220519	55909.863737	33.198464
765.901341	56043.141707	33.203482
766.471612	56151.222544	33.208500
767.254951	56269.359145	33.213517
767.868621	56395.352921	33.218535
768.375890	56502.631017	33.223552
769.191283	56630.810738	33.228570
769.796734	56763.044512	33.233588
770.684205	56870.798889	33.238605
771.379246	57000.776383	33.243623
772.389125	57138.461975	33.248640
773.032675	57251.629513	33.253658
774.344188	57361.167891	33.258676
775.733999	57453.955703	33.263693
776.269710	57565.285141	33.268711
777.683795	57656.926203	33.273728
778.784555	57743.039937	33.278746
779.618542	57831.321221	33.283764
780.401159	57921.601819	33.288781
781.027529	58008.161534	33.293799
781.669275	58090.908788	33.298816
782.676291	58189.450263	33.303834
783.223389	58276.220120	33.308852
783.788698	58364.781941	33.313869
784.346282	58470.160339	33.318887
785.316606	58565.562860	33.323904
785.727482	58677.993368	33.328922
786.226266	58775.711718	33.333940
787.100157	58871.618196	33.338957
787.857280	58987.013817	33.343975
789.304734	59077.120344	33.348992
790.356859	59178.610325	33.354010
790.922496	59280.768850	33.359028
792.202413	59380.768805	33.364045
792.536626	59477.809995	33.369063
793.759154	59570.572094	33.374080
794.591816	59665.301142	33.379098
795.075022	59775.330810	33.384116
795.866835	59870.484654	33.389133
796.499432	59974.379823	33.394151
797.432254	60064.285076	33.399168
797.909182	60171.707986	33.404186
798.588692	60288.210868	33.409204
799.758869	60385.314297	33.414221
800.329022	60498.253225	33.419239
800.678913	60609.895701	33.424256
801.581369	60718.224486	33.429274
802.996645	60827.101145	33.434292
804.816057	60886.592025	33.439309
806.259077	60982.540996	33.444327
807.181530	61073.716428	33.449344
807.761501	61166.554073	33.454362
808.400978	61241.737171	33.459380
809.324633	61330.632083	33.464397
809.561129	61426.795038	33.469415
810.038843	61510.891699	33.474432
810.642365	61610.224424	33.479450
810.842425	61717.840310	33.484468
812.090516	61818.407464	33.489485
812.235752	61944.892707	33.494503
812.802780	62060.887160	33.499520
813.861040	62176.169138	33.504538
814.506417	62310.328928	33.509556
815.335457	62404.654279	33.514573
815.584793	62534.083869	33.519591
816.532857	62664.479675	33.524608
817.348393	62788.388215	33.529626
818.448478	62917.648150	33.534644
819.268275	63029.365378	33.539661
819.807290	63157.183610	33.544679
820.524401	63276.446845	33.549696
821.477973	63407.971540	33.554714
821.968756	63548.030470	33.559732
823.218262	63658.416053	33.564749
824.080941	63788.093609	33.569767
824.923594	63915.221720	33.574784
825.900398	64034.269501	33.579802
826.126064	64169.888715	33.584820
827.617051	64292.177824	33.589837
828.275870	64426.033217	33.594855
829.050021	64555.407868	33.599872
830.003306	64664.931244	33.604890
831.601339	64761.649885	33.609908
833.061437	64863.416960	33.614925
833.924978	64951.149204	33.619943
834.320696	65052.751637	33.624960
835.284773	65138.148242	33.629978
835.983664	65245.523290	33.634996
836.993535	65347.645231	33.640013
837.907031	65448.209614	33.645031
838.322743	65550.203104	33.650048
838.930628	65656.685058	33.655066
839.344969	65768.907639	33.660084
840.120630	65894.807399	33.665101
840.981478	66013.196720	33.670119
841.752447	66120.343153	33.675136
842.731350	66244.207590	33.680154
843.299694	66357.596351	33.685172
844.009549	66474.616191	33.690189
844.840975	66605.353318	33.695207
845.136063	66738.076304	33.700224
846.692424	66858.719863	33.705242
847.185222	66988.838900	33.710260
848.197381	67108.056567	33.715277
848.797467	67251.340257	33.720295
849.733006	67375.326048	33.725312
850.858385	67492.510569	33.730330
851.720883	67637.251841	33.735348
853.009250	67768.047234	33.740365
853.904979	67894.565111	33.745383
854.950293	68017.133110	33.750400
856.334556	68113.377944	33.755418
857.578821	68225.748544	33.760436
858.665853	68325.880907	33.765453
859.588656	68429.802512	33.770471
860.525572	68543.818732	33.775488
861.171374	68650.025197	33.780506
861.833966	68765.624201	33.785524
862.551547	68872.034887	33.790541
863.326377	68992.035835	33.795559
863.488704	69107.915311	33.800576
864.690819	69231.362262	33.805594
864.956993	69364.353201	33.810612
865.747559	69503.985433	33.815629
866.515537	69623.852009	33.820647
867.159976	69764.117041	33.825664
868.168587	69894.990813	33.830682
868.708393	70029.571958	33.835700
869.781135	70170.331665	33.840717
870.536301	70309.323820	33.845735
871.343318	70451.558188	33.850752
872.208965	70584.527340	33.855770
873.177158	70734.355882	33.860788
873.811195	70877.329810	33.865805
874.686392	71020.935100	33.870823
875.691227	71171.190619	33.875840
876.794101	71311.270024	33.880858
877.397226	71455.093881	33.885876
878.255974	71597.453812	33.890893
879.474453	71751.731204	33.895911
879.942181	71884.869009	33.900928
881.161856	72040.552017	33.905946
882.044574	72172.352129	33.910964
883.031923	72332.084527	33.915981
883.980674	72464.349773	33.920999
884.832075	72601.285878	33.926016
885.902366	72741.468542	33.931034
886.778352	72883.353584	33.936052
887.019835	73032.262190	33.941069
888.295291	73163.276329	33.946087
889.564839	73305.016957	33.951104
890.454660	73426.452980	33.956122
891.226992	73545.676852	33.961140
892.429344	73657.286274	33.966157
893.755585	73779.651357	33.971175
894.723588	73897.712924	33.976192
895.947713	74012.008160	33.981210
896.701249	74132.749747	33.986228
897.270637	74245.212922	33.991245
898.358790	74365.021540	33.996263
899.457392	74463.258347	34.001280
900.823551	74583.079182	34.006298
901.792346	74692.980784	34.011316
902.605793	74799.696013	34.016333
903.784259	74891.066385	34.021351
904.276065	75012.779383	34.026368
905.377748	75122.711806	34.031386
906.124864	75237.275652	34.036404
906.719111	75354.477208	34.041421
907.588075	75470.438765	34.046439
908.033376	75599.833931	34.051456
908.824698	75718.712436	34.056474
909.439481	75843.647769	34.061492
910.213455	75983.229936	34.066509
911.530255	76118.220422	34.071527
912.177423	76274.325626	34.076544
913.072182	76394.721224	34.081562
913.575372	76531.518244	34.086580
914.351564	76678.320691	34.091597
915.104334	76816.672052	34.096615
916.118753	76979.843077	34.101632
916.921712	77123.026397	34.106650
917.763909	77284.912590	34.111668
918.919804	77429.361484	34.116685
920.066896	77582.047631	34.121703
920.907857	77735.607606	34.126720
921.986569	77865.512370	34.131738
922.885307	78013.214241	34.136756
923.888502	78155.118857	34.141773
925.036318	78306.127447	34.146791
925.680242	78454.462554	34.151808
927.119723	78591.889386	34.156826
928.172070	78727.129255	34.161844
929.166032	78880.361962	34.166861
929.842410	79019.827632	34.171879
930.752279	79168.958516	34.176896
931.992118	79313.114857	34.181914
933.182700	79440.499229	34.186932
934.485944	79570.927191	34.191949
935.686951	79693.415474	34.196967
936.676689	79831.708561	34.201984
937.837368	79941.484459	34.207002
938.997938	80065.664027	34.212020
939.909966	80192.750778	34.217037
941.023977	80302.466572	34.222055
941.508709	80439.259079	34.227072
942.161257	80558.180135	34.232090
942.658387	80697.609949	34.237108
943.402601	80835.728366	34.242125
944.329615	80955.656272	34.247143
944.865975	81112.541197	34.252160
946.120495	81243.904170	34.257178
946.470292	81399.759159	34.262196
947.259426	81542.574598	34.267213
948.419071	81682.014975	34.272231
948.824059	81841.052162	34.277248
950.039368	81987.601957	34.282266
950.993906	82143.893606	34.287284
952.157064	82293.401934	34.292301
952.987515	82419.059692	34.297319
954.339824	82564.287411	34.302336
955.604574	82693.379683	34.307354
956.305840	82813.234508	34.312372
956.879837	82968.474914	34.317389
957.878592	83094.766551	34.322407
958.706058	83246.417932	34.327424
959.456926	83382.096135	34.332442
960.174087	83532.565610	34.337460
960.364819	83706.176728	34.342477
961.399201	83863.567803	34.347495
962.316105	84026.964302	34.352512
963.454094	84184.852930	34.357530
964.776226	84358.845257	34.362548
965.804712	84520.581913	34.367565
967.359396	84668.048229	34.372583
968.406152	84832.023732	34.377600
969.593944	84973.674983	34.382618
971.040888	85110.191177	34.387636
972.049500	85250.310973	34.392653
973.208816	85402.858193	34.397671
974.081003	85552.271345	34.402688
974.863822	85679.789678	34.407706
976.137590	85817.547112	34.412724
976.811157	85967.375361	34.417741
977.937394	86113.346201	34.422759
978.740167	86259.263803	34.427776
979.890026	86405.276869	34.432794
980.962345	86557.358857	34.437812
981.477613	86709.495847	34.442829
982.610870	86865.030828	34.447847
983.455559	87017.824106	34.452864
984.508719	87173.235164	34.457882
986.000918	87313.509033	34.462900
987.075710	87463.350268	34.467917
988.828810	87572.565130	34.472935
989.729372	87722.778482	34.477952
990.907132	87862.462147	34.482970
992.221742	87992.746450	34.487988
992.701816	88129.844986	34.493005
993.921201	88252.382366	34.498023
994.580719	88396.925888	34.503040
995.492560	88539.378429	34.508058
996.696722	88668.387515	34.513076
996.921521	88817.510818	34.518093
998.012912	88968.706762	34.523111
998.791177	89113.076873	34.528128
999.213498	89265.125551	34.533146
1000.021015	89438.734553	34.538164
1000.713890	89595.619613	34.543181
1002.039614	89766.601569	34.548199
1002.855182	89927.879285	34.553216
1004.026021	90091.162443	34.558234
1005.157267	90271.596548	34.563252
1005.620135	90438.194754	34.568269
1006.733857	90607.623029	34.573287
1007.499718	90787.172111	34.578304
1008.524322	90967.249386	34.583322
1009.551297	91131.753180	34.588340
1010.044383	91308.395803	34.593357
1011.137160	91479.232328	34.598375
1012.151337	91667.632370	34.603392
1013.158441	91856.047717	34.608410
1014.806001	92033.846764	34.613428
1015.442680	92210.269799	34.618445
1016.849196	92378.497768	34.623463
1017.494327	92571.554225	34.628480
1018.353570	92729.001980	34.633498
1019.701059	92902.274842	34.638516
1020.667434	93073.485321	34.643533
1021.663435	93233.401086	34.648551
1022.691823	93400.065705	34.653568
1024.187615	93552.590957	34.658586
1026.039313	93705.292589	34.663604
1026.857467	93855.349318	34.668621
1028.075036	94022.809781	34.673639
1029.273109	94163.691557	34.678656
1030.186412	94325.856085	34.683674
1031.361121	94466.661189	34.688692
1032.338326	94612.626539	34.693709
1033.594926	94758.920071	34.698727
1034.429498	94907.037424	34.703744
1035.484578	95069.860742	34.708762
1036.463664	95217.816867	34.713780
1036.838065	95384.286551	34.718797
1037.354431	95543.568757	34.723815
1038.746541	95724.348648	34.728832
1039.353443	95908.797832	34.733850
1040.372716	96071.393173	34.738868
1041.446422	96260.122815	34.743885
1042.263209	96436.856876	34.748903
1044.822512	96580.072426	34.753920
1046.781325	96730.642076	34.758938
1048.718023	96868.214488	34.763956
1049.483987	97018.533396	34.768973
1050.432506	97152.808005	34.773991
1051.356207	97300.703488	34.779008
1052.088098	97444.770132	34.784026
1054.617020	97553.807281	34.789044
1055.718817	97691.015686	34.794061
1056.780967	97811.690489	34.799079
1058.068629	97950.901649	34.804096
1058.420932	98081.373931	34.809114
1059.263551	98211.759618	34.814132
1059.758583	98361.909812	34.819149
1060.468007	98493.217869	34.824167
1061.118720	98656.543030	34.829184
1061.773846	98812.227627	34.834202
1062.756980	98978.152478	34.839220
1063.676065	99149.318051	34.844237
1064.365660	99317.097814	34.849255
1065.302718	99492.719511	34.854272
1066.198976	99688.259233	34.859290
1067.194101	99861.658168	34.864308
1068.328090	100039.175709	34.869325
1069.456355	100207.623352	34.874343
1070.198314	100391.608566	34.879360
1071.278611	100577.090338	34.884378
1072.503500	100761.378366	34.889396
1073.528546	100952.057070	34.894413
1074.490218	101140.867341	34.899431
1075.529398	101322.790625	34.904448
1076.342013	101531.906972	34.909466
1077.411835	101713.815326	34.914484
1078.404233	101903.784787	34.919501
1079.226041	102114.835423	34.924519
1080.096914	102305.144492	34.929536
1081.136460	102506.095547	34.934554
1082.528369	102714.530772	34.939572
1083.183370	102923.836460	34.944589
1084.425129	103125.436448	34.949607
1085.756802	103329.840735	34.954624
1086.697045	103542.130864	34.959642
1087.784765	103744.077699	34.964660
1088.782479	103942.583828	34.969677
1089.999396	104142.062048	34.974695
1091.624634	104316.913132	34.979712
1092.971446	104512.079760	34.984730
1093.976967	104680.735362	34.989748
1094.928004	104877.717686	34.994765
1095.569168	105071.124398	34.999783
1096.825364	105255.015207	35.004800
1097.362476	105466.900044	35.009818
1098.476105	105647.955030	35.014836
1099.401433	105864.578784	35.019853
1100.493673	106080.467557	35.024871
1101.891070	106281.996664	35.029888
1102.584640	106496.852847	35.034906
1103.496406	106698.389324	35.039924
1105.084618	106916.609401	35.044941
1105.996309	107129.484323	35.049959
1107.448240	107334.710672	35.054976
1108.387603	107546.482510	35.059994
1109.640801	107762.928410	35.065012
1110.657640	107977.021321	35.070029
1111.547070	108194.721343	35.075047
1112.823916	108412.181868	35.080064
1114.643580	108622.613713	35.085082
1116.269633	108827.848176	35.090100
1117.314728	109026.403829	35.095117
1118.628154	109218.760956	35.100135
1120.277813	109406.377484	35.105152
1121.212795	109613.239319	35.110170
1122.607275	109813.415063	35.115188
1123.683584	110004.752990	35.120205
1124.581741	110200.238302	35.125223
1125.576827	110400.889671	35.130240
1127.036540	110601.985162	35.135258
1128.641113	110790.847445	35.140276
1129.469752	110992.176681	35.145293
1130.622385	111202.852825	35.150311
1131.566870	111385.342720	35.155328
1132.428555	111596.639961	35.160346
1133.419965	111786.623762	35.165364
1135.038784	111974.972564	35.170381
1136.352324	112179.245355	35.175399
1137.549044	112371.378130	35.180416
1138.266348	112584.328286	35.185434
1139.503759	112778.686699	35.190452
1140.704708	112980.615186	35.195469
1142.405023	113165.956454	35.200487
1144.206348	113345.835067	35.205504
1145.144853	113523.120988	35.210522
1146.361973	113715.183777	35.215540
1147.498041	113894.352356	35.220557
1148.586375	114078.799991	35.225575
1149.526482	114270.506976	35.230592
1150.170054	114469.155893	35.235610
1151.235672	114669.168108	35.240628
1152.403672	114873.636899	35.245645
1152.763814	115086.741291	35.250663
1153.883112	115283.556523	35.255680
1154.447191	115495.768885	35.260698
1155.677272	115708.810423	35.265716
1157.131570	115934.739099	35.270733
1157.961897	116153.943869	35.275751
1158.829544	116378.072563	35.280768
1160.224880	116597.035481	35.285786
1161.087429	116825.868942	35.290804
1162.720609	117048.787011	35.295821
1163.564356	117267.719484	35.300839
1165.148808	117493.284405	35.305856
1166.385570	117705.148951	35.310874
1167.824260	117907.035765	35.315892
1169.034380	118099.598521	35.320909
1169.937518	118306.555929	35.325927
1171.763417	118486.691537	35.330944
1173.108698	118694.769779	35.335962
1174.210981	118894.400429	35.340980
1175.412685	119082.827955	35.345997
1176.040003	119300.215261	35.351015
1177.402508	119483.537941	35.356032
1178.399750	119694.785212	35.361050
1179.607757	119899.169616	35.366068
1181.192548	120117.444047	35.371085
1182.329370	120298.135575	35.376103
1183.282905	120500.741599	35.381120
1184.273862	120708.930890	35.386138
1185.318266	120921.471797	35.391156
1186.680226	121134.088552	35.396173
1187.051453	121348.973876	35.401191
1189.116136	121549.439695	35.406208
1190.740780	121753.755702	35.411226
1191.554555	121980.585410	35.416244
1193.005083	122187.328157	35.421261
1193.945440	122408.412574	35.426279
1195.195468	122618.169370	35.431296
1196.155283	122851.419114	35.436314
1197.367303	123069.485683	35.441332
1198.751017	123290.300771	35.446349
1199.914388	123504.944365	35.451367
1202.078997	123702.050159	35.456384
1202.867343	123909.877390	35.461402
1204.057918	124127.701831	35.466420
1205.835647	124327.828387	35.471437
1206.859539	124554.883935	35.476455
1208.078289	124766.093124	35.481472
1208.841005	124979.026582	35.486490
1209.908245	125210.084644	35.491508
1211.424682	125416.192668	35.496525
1212.297775	125646.842570	35.501543
1213.449722	125868.399345	35.506560
1214.403143	126093.120888	35.511578
1215.385510	126330.994587	35.516596
1216.624017	126568.903916	35.521613
1217.982724	126803.715521	35.526631
1219.437862	127023.253575	35.531648
1220.927895	127244.384383	35.536666
1222.209261	127475.551138	35.541684
1223.645570	127703.348067	35.546701
1224.323379	127930.739573	35.551719
1225.383766	128152.188681	35.556736
1226.654050	128397.166671	35.561754
1227.219511	128632.921756	35.566772
1228.729087	128881.729862	35.571789
1229.712526	129123.744390	35.576807
1230.913392	129365.877021	35.581824
1231.815497	129620.659830	35.586842
1233.044718	129873.502140	35.591860
1234.581325	130131.251782	35.596877
1235.519795	130378.214172	35.601895
1236.812946	130641.052993	35.606912
1237.880576	130885.146092	35.611930
1239.082189	131138.586272	35.616948
1240.537269	131385.927653	35.621965
1241.790372	131650.746278	35.626983
1243.340734	131895.008373	35.632000
1244.980586	132138.382938	35.637018
1246.885682	132378.660644	35.642036
1248.137623	132606.891475	35.647053
1249.672371	132848.488815	35.652071
1250.693435	133062.233955	35.657088
1252.361401	133276.431516	35.662106
1253.278920	133497.511001	35.667124
1254.594475	133702.312854	35.672141
1255.392240	133933.657861	35.677159
1256.620074	134152.725744	35.682176
1257.784235	134374.112830	35.687194
1258.973025	134598.717333	35.692212
1260.263952	134833.067912	35.697229
1261.367069	135059.705420	35.702247
1262.705814	135286.660583	35.707264
1264.127260	135517.102639	35.712282
1265.401381	135741.751688	35.717300
1266.634646	135986.997378	35.722317
1267.787488	136203.239048	35.727335
1269.175198	136434.098835	35.732352
1270.503730	136674.719262	35.737370
1271.741905	136905.708472	35.742388
1273.120377	137146.780517	35.747405
1274.067843	137384.045967	35.752423
1275.633603	137614.478950	35.757440
1277.070318	137862.025156	35.762458
1278.054579	138097.882360	35.767476
1279.804738	138330.901632	35.772493
1281.065566	138567.096869	35.777511
1282.795745	138808.338480	35.782528
1283.499074	139042.068010	35.787546
1284.492466	139307.410314	35.792564
1285.677118	139548.721943	35.797581
1286.856764	139796.832080	35.802599
1288.008680	140053.976145	35.807616
1288.972685	140312.636650	35.812634
1290.454305	140564.278119	35.817652
1291.978015	140814.963553	35.822669
1293.362275	141072.558816	35.827687
1294.621887	141322.797082	35.832704
1296.504292	141569.130487	35.837722
1297.421904	141827.049380	35.842740
1298.783107	142071.760658	35.847757
1299.815402	142347.860139	35.852775
1301.139969	142595.890664	35.857792
1302.349997	142861.770163	35.862810
1303.282648	143128.204698	35.867828
1305.019263	143385.898631	35.872845
1306.155109	143676.434534	35.877863
1307.268412	143930.811662	35.882880
1308.776851	144198.985359	35.887898
1309.429608	144492.575056	35.892916
1311.030660	144753.116583	35.897933
1312.235601	145030.362806	35.902951
1313.913080	145298.998880	35.907968
1314.890119	145583.857644	35.912986
1315.958238	145860.663762	35.918004
1317.721565	146153.183601	35.923021
1318.931448	146426.077553	35.928039
1320.670086	146685.963841	35.933056
1322.237316	146952.601569	35.938074
1323.799153	147223.592001	35.943092
1325.415305	147489.058924	35.948109
1327.063513	147757.096941	35.953127
1327.887337	148023.332666	35.958144
1329.404555	148292.803977	35.963162
1330.822177	148562.103496	35.968180
1331.790040	148827.890156	35.973197
1333.155055	149095.857984	35.978215
1334.107406	149360.496986	35.983232
1335.395183	149629.838496	35.988250
1336.684481	149909.873207	35.993268
1337.804520	150159.233058	35.998285
1338.943874	150419.562052	36.003303
1339.823520	150687.063542	36.008320
1341.510560	150949.563428	36.013338
1342.836428	151211.934532	36.018356
1344.342038	151483.536548	36.023373
1345.532476	151752.922250	36.028391
1346.333279	152022.970315	36.033408
1347.869856	152297.388833	36.038426
1349.081176	152596.557933	36.043444
1349.876878	152867.158289	36.048461
1351.304519	153162.465701	36.053479
1352.159440	153458.263136	36.058496
1353.879754	153762.240716	36.063514
1354.987317	154061.971217	36.068532
1356.864817	154364.380192	36.073549
1358.043935	154657.977099	36.078567
1359.775077	154955.594868	36.083584
1361.644527	155249.462878	36.088602
1362.847438	155546.817218	36.093620
1364.167970	155843.228445	36.098637
1365.782108	156139.060713	36.103655
1367.352158	156419.503115	36.108672
1369.045205	156708.020208	36.113690
1370.729112	156995.031415	36.118708
1372.896496	157260.983761	36.123725
1374.683803	157540.611837	36.128743
1376.201726	157795.841825	36.133760
1377.677356	158053.630192	36.138778
1378.473660	158337.372588	36.143796
1380.077123	158593.367390	36.148813
1381.476602	158874.515006	36.153831
1382.661806	159151.602477	36.158848
1383.884138	159425.184452	36.163866
1384.734366	159705.502466	36.168884
1386.197617	159996.770726	36.173901
1387.743712	160267.450626	36.178919
1388.924752	160558.465027	36.183936
1390.723420	160834.891898	36.188954
1391.826643	161126.354522	36.193972
1393.178506	161414.670013	36.198989
1394.290067	161703.230168	36.204007
1395.472401	162005.114264	36.209024
1396.581266	162290.253585	36.214042
1398.053342	162598.640512	36.219060
1399.107352	162887.497520	36.224077
1400.669250	163207.469916	36.229095
1401.823626	163520.863999	36.234112
1403.506345	163821.092779	36.239130
1404.937436	164142.717840	36.244148
1406.501824	164449.961290	36.249165
1407.746359	164744.255148	36.254183
1408.975906	165072.898601	36.259200
1410.783906	165368.841969	36.264218
1412.165114	165686.566459	36.269236
1413.372866	165990.581051	36.274253
1415.325957	166288.333848	36.279271
1416.549520	166605.228348	36.284288
1418.430809	166908.110506	36.289306
1419.523233	167219.334189	36.294324
1420.823905	167506.671846	36.299341
1422.533506	167823.913698	36.304359
1424.248984	168113.927551	36.309376
1425.925037	168414.405130	36.314394
1426.867227	168715.500715	36.319412
1428.514915	169012.827577	36.324429
1429.832445	169317.481560	36.329447
1431.038012	169602.602612	36.334464
1432.788094	169908.965671	36.339482
1434.159309	170178.278034	36.344500
1435.702958	170458.603035	36.349517
1437.519843	170726.931506	36.354535
1438.606587	171013.007386	36.359552
1440.145870	171290.559305	36.364570
1441.548471	171566.143235	36.369588
1442.677857	171837.446807	36.374605
1444.913063	172122.540656	36.379623
1446.631454	172394.118302	36.384640
1447.747381	172667.598902	36.389658
1449.039548	172943.133147	36.394676
1450.397024	173232.540918	36.399693
1451.755333	173517.661156	36.404711
1452.799229	173803.329924	36.409728
1454.030441	174110.758358	36.414746
1455.036221	174414.837726	36.419764
1456.133928	174721.162736	36.424781
1457.715047	175034.884539	36.429799
1458.358656	175371.707366	36.434816
1459.593399	175684.449978	36.439834
1461.193865	176028.416536	36.444852
1462.388371	176357.502933	36.449869
1464.275288	176686.464607	36.454887
1465.721912	177032.836851	36.459904
1467.100565	177373.727595	36.464922
1468.447820	177712.899910	36.469940
1469.983688	178054.746639	36.474957
1471.717546	178405.599185	36.479975
1473.674884	178755.554323	36.484992
1475.239182	179079.914830	36.490010
1477.324422	179398.378787	36.495028
1479.103168	179725.703261	36.500045
1480.788823	180053.451351	36.505063
1482.091549	180383.714249	36.510080
1484.029031	180707.033673	36.515098
1485.022100	181032.249777	36.520116
1486.209681	181361.890711	36.525133
1487.843172	181697.031961	36.530151
1488.452036	182042.244306	36.535168
1490.174972	182370.140646	36.540186
1491.713115	182729.444819	36.545204
1493.017946	183078.255300	36.550221
1494.726643	183418.751361	36.555239
1495.976728	183772.601666	36.560256
1497.640922	184125.002494	36.565274
1499.301930	184470.552123	36.570292
1500.506561	184821.637178	36.575309
1502.160681	185169.895995	36.580327
1503.425031	185527.664913	36.585344
1505.291494	185882.366655	36.590362
1506.357198	186261.243571	36.595380
1507.694099	186629.619157	36.600397
1509.171796	186987.133911	36.605415
1510.680451	187368.991711	36.610432
1512.351288	187724.918050	36.615450
1514.080446	188086.917219	36.620468
1515.394688	188446.511930	36.625485
1516.916376	188808.169149	36.630503
1518.596052	189176.568369	36.635520
1520.153411	189529.554434	36.640538
1521.998058	189883.244199	36.645556
1523.459274	190255.862682	36.650573
1525.037189	190605.462628	36.655591
1526.543858	190973.356004	36.660608
1528.123408	191330.639973	36.665626
1529.495686	191697.734928	36.670644
1530.712622	192055.070414	36.675661
1532.874507	192391.420500	36.680679
1534.155933	192735.001312	36.685696
1535.590227	193086.924601	36.690714
1536.959157	193415.248624	36.695732
1538.089779	193767.010156	36.700749
1540.070561	194106.776462	36.705767
1541.785970	194452.275746	36.710784
1543.206613	194788.824877	36.715802
1545.044585	195138.738304	36.720820
1546.340039	195493.415011	36.725837
1548.172648	195827.768984	36.730855
1549.849365	196185.192307	36.735872
1551.611491	196530.212927	36.740890
1553.599617	196860.103320	36.745908
1554.963220	197207.846689	36.750925
1556.947554	197534.326093	36.755943
1558.806319	197856.777976	36.760960
1561.122618	198187.839770	36.765978
1563.012104	198496.641939	36.770996
1564.352432	198819.856985	36.776013
1565.951333	199142.066059	36.781031
1567.402972	199467.817751	36.786048
1568.434943	199783.458135	36.791066
1570.200119	200125.094686	36.796084
1571.580033	200466.352172	36.801101
1572.694028	200806.449116	36.806119
1573.857958	201150.741951	36.811136
1575.098230	201506.082349	36.816154
1576.389703	201867.637322	36.821172
1577.979827	202220.612917	36.826189
1579.569067	202576.561405	36.831207
1580.788263	202942.412552	36.836224
1582.209444	203328.521397	36.841242
1583.907524	203707.654265	36.846260
1584.971554	204083.897328	36.851277
1586.476396	204465.935524	36.856295
1587.716947	204851.853781	36.861312
1588.988008	205254.719421	36.866330
1590.839837	205651.650810	36.871348
1592.171635	206050.092192	36.876365
1593.764242	206470.293623	36.881383
1595.213183	206872.821200	36.886400
1596.522084	207284.998537	36.891418
1598.566679	207703.329176	36.896436
1599.944876	208125.809809	36.901453
1601.726167	208533.941563	36.906471
1603.536370	208949.587607	36.911488
1605.392608	209360.047613	36.916506
1607.349880	209779.825842	36.921524
1608.730282	210206.812175	36.926541
1610.715355	210600.432749	36.931559
1612.348884	211014.594865	36.936576
1613.891291	211432.812033	36.941594
1615.588128	211822.867086	36.946612
1617.999587	212214.634555	36.951629
1620.354412	212597.397534	36.956647
1622.113666	212985.949275	36.961664
1624.016253	213374.885465	36.966682
1625.796363	213747.640617	36.971700
1627.009780	214138.243119	36.976717
1628.763068	214512.123396	36.981735
1630.311436	214903.537498	36.986752
1631.710544	215293.403324	36.991770
1633.624179	215666.525447	36.996788
1634.721702	216059.771342	37.001805
1636.191670	216450.874886	37.006823
1637.277960	216854.030960	37.011840
1638.849092	217246.187839	37.016858
1640.622816	217630.922212	37.021876
1642.006717	218003.379167	37.026893
1643.373068	218463.056585	37.031911
1645.143963	218841.091232	37.036928
1647.070243	219224.003517	37.041946
1649.164860	219592.336382	37.046964
1651.011500	219963.937094	37.051981
1652.769854	220325.394418	37.056999
1654.267822	220699.747581	37.062016
1655.714376	221082.822274	37.067034
1657.548194	221461.618320	37.072052
1659.013873	221856.553843	37.077069
1660.104800	222240.783590	37.082087
1661.848790	222626.913477	37.087104
1663.123336	223041.594435	37.092122
1664.854369	223426.941937	37.097140
1666.353847	223818.805773	37.102157
1668.559079	224218.860089	37.107175
1670.272657	224628.191501	37.112192
1671.471899	225035.374096	37.117210
1673.314306	225438.413490	37.122228
1674.838901	225865.915722	37.127245
1676.271146	226277.839331	37.132263
1677.961234	226699.627729	37.137280
1679.743615	227120.843573	37.142298
1681.271667	227551.170608	37.147316
1682.679543	227970.977947	37.152333
1684.435307	228405.639160	37.157351
1686.291904	228838.761206	37.162368
1687.338771	229283.524635	37.167386
1689.401046	229718.088889	37.172404
1691.097996	230165.872279	37.177421
1692.925600	230610.943141	37.182439
1694.353372	231043.279503	37.187456
1695.761358	231509.073204	37.192474
1697.938878	231962.193487	37.197492
1699.357657	232417.396253	37.202509
1701.823154	232841.032174	37.207527
1704.118825	233283.367076	37.212544
1705.748340	233728.886720	37.217562
1708.026902	234162.387432	37.222580
1710.035207	234589.329621	37.227597
1711.919022	235006.564806	37.232615
1713.691623	235437.180543	37.237632
1715.518258	235868.525142	37.242650
1717.322598	236283.490572	37.247668
1718.781341	236722.315303	37.252685
1720.335189	237146.138501	37.257703
1722.196108	237579.488498	37.262720
1723.405625	238005.986938	37.267738
1725.177585	238437.245328	37.272756
1727.282534	238866.493838	37.277773
1728.963008	239295.559335	37.282791
1730.830723	239715.500985	37.287808
1732.233153	240142.048617	37.292826
1734.429886	240575.934319	37.297844
1736.204798	241009.204672	37.302861
1738.147124	241432.643054	37.307879
1739.688418	241857.520155	37.312896
1741.124576	242293.033577	37.317914
1742.858387	242716.178604	37.322932
1745.015395	243151.066694	37.327949
1746.551439	243570.283126	37.332967
1748.314786	243990.072442	37.337984
1749.933615	244433.815478	37.343002
1751.391171	244863.512876	37.348020
1753.014699	245290.795752	37.353037
1754.751400	245725.300385	37.358055
1756.292621	246152.191744	37.363072
1757.556509	246580.679059	37.368090
1759.490563	246995.669185	37.373108
1760.518603	247426.940119	37.378125
1762.454622	247858.138056	37.383143
1764.140073	248296.490703	37.388160
1765.754710	248737.726129	37.393178
1767.144935	249183.546259	37.398196
1768.755003	249633.852391	37.403213
1770.492706	250087.923046	37.408231
1772.612494	250532.913122	37.413248
1774.283691	250995.912226	37.418266
1776.696099	251442.785617	37.423284
1778.683795	251902.939118	37.428301
1780.207229	252345.438286	37.433319
1782.123740	252785.891550	37.438336
1783.903191	253256.800761	37.443354
1785.657975	253721.007995	37.448372
1786.948959	254184.860245	37.453389
1788.853269	254654.352765	37.458407
1790.808906	255120.687130	37.463424
1792.636361	255592.123573	37.468442
1795.264918	256037.465997	37.473460
1797.794096	256488.007297	37.478477
1799.554212	256944.010354	37.483495
1801.525305	257389.207794	37.488512
1803.268533	257857.534562	37.493530
1805.058610	258298.951651	37.498548
1806.605554	258744.346464	37.503565
1807.830828	259212.454173	37.508583
1809.941451	259678.637659	37.513600
1811.089537	260154.048957	37.518618
1813.134927	260628.296110	37.523636
1814.961124	261100.216906	37.528653
1816.554512	261578.857141	37.533671
1818.528405	262064.395045	37.538688
1820.243266	262547.917921	37.543706
1821.960372	263024.860854	37.548724
1823.787300	263509.965383	37.553741
1825.365560	264007.914004	37.558759
1827.119171	264492.420562	37.563776
1828.718850	265004.718027	37.568794
1830.736510	265495.150275	37.573812
1832.146820	265990.178787	37.578829
1834.198404	266501.791076	37.583847
1836.045887	267001.344735	37.588864
1837.814145	267527.940018	37.593882
1840.195416	268017.370528	37.598900
1842.971789	268509.148710	37.603917
1844.794790	269003.700206	37.608935
1847.287173	269488.538410	37.613952
1848.796095	269965.942825	37.618970
1850.562095	270452.932036	37.623988
1852.568171	270943.970940	37.629005
1854.552644	271435.470040	37.634023
1856.310370	271911.840364	37.639040
1857.965812	272408.854050	37.644058
1859.660535	272890.034571	37.649076
1861.214303	273376.927864	37.654093
1863.203793	273881.403438	37.659111
1865.004878	274382.657709	37.664128
1866.582647	274880.315380	37.669146
1868.362678	275392.316689	37.674164
1870.463421	275890.267321	37.679181
1871.997838	276392.933695	37.684199
1874.179815	276886.957030	37.689216
1876.186054	277389.467378	37.694234
1878.468821	277867.036746	37.699252
1880.346323	278348.380730	37.704269
1881.595077	278828.176271	37.709287
1883.557758	279291.163759	37.714304
1885.410882	279782.821953	37.719322
1887.137457	280255.321302	37.724340
1889.298836	280734.733401	37.729357
1891.082110	281220.099985	37.734375
1892.908760	281701.774941	37.739392
1894.706864	282179.643121	37.744410
1896.880142	282651.097755	37.749428
1898.775459	283129.125271	37.754445
1900.751535	283604.039196	37.759463
1902.704798	284106.084481	37.764480
1904.234718	284604.210105	37.769498
1906.272454	285101.818669	37.774516
1908.348113	285593.119950	37.779533
1909.792283	286102.939827	37.784551
1912.072555	286598.090678	37.789568
1913.792761	287101.155882	37.794586
1915.685040	287606.146928	37.799604
1917.720364	288107.835962	37.804621
1919.134048	288627.863637	37.809639
1921.120090	289141.978262	37.814656
1923.299111	289659.539087	37.819674
1924.819637	290176.495401	37.824692
1926.829031	290698.627024	37.829709
1928.325131	291234.963899	37.834727
1930.534104	291760.766908	37.839744
1932.912230	292279.656453	37.844762
1934.672727	292809.440800	37.849780
1936.987375	293324.805946	37.854797
1938.668144	293874.131494	37.859815
1940.934122	294407.965812	37.864832
1942.261622	294954.855561	37.869850
1944.058559	295491.073763	37.874868
1946.401485	296037.638578	37.879885
1947.676806	296595.831950	37.884903
1949.727069	297142.236542	37.889920
1951.706295	297705.667494	37.894938
1953.636212	298255.413697	37.899956
1955.642907	298798.210582	37.904973
1957.608824	299360.466754	37.909991
1960.007892	299911.600135	37.915008
1962.035996	300468.582588	37.920026
1963.732730	301046.874940	37.925044
1966.131882	301596.399117	37.930061
1967.971765	302162.597327	37.935079
1970.342433	302714.786743	37.940096
1972.482245	303260.636282	37.945114
1974.389504	303820.159490	37.950132
1976.552572	304358.989166	37.955149
1978.147324	304929.020980	37.960167
1980.348364	305488.409496	37.965184
1982.181529	306050.191748	37.970202
1984.148526	306607.961121	37.975220
1986.344114	307153.676716	37.980237
1988.301761	307720.557924	37.985255
1990.365321	308276.700748	37.990272
1992.299513	308834.639007	37.995290
1993.813486	309407.524861	38.000308
1996.292838	309956.578772	38.005325
1998.379313	310529.870355	38.010343
2000.370434	311075.899045	38.015360
2001.986680	311636.156371	38.020378
2004.666227	312178.102360	38.025396
2006.840725	312738.462981	38.030413
2008.874374	313289.954692	38.035431
2010.847307	313834.189669	38.040448
2012.714207	314374.806880	38.045466
2014.382676	314906.793577	38.050484
2016.277296	315434.117505	38.055501
2017.714973	315986.627446	38.060519
2019.830650	316516.878247	38.065536
2021.763614	317065.895610	38.070554
2022.940319	317612.468819	38.075572
2025.017771	318165.313694	38.080589
2026.867168	318742.543505	38.085607
2028.590661	319292.644702	38.090624
2030.758590	319868.492236	38.095642
2032.386579	320460.624165	38.100660
2034.586255	321041.941269	38.105677
2036.417120	321646.496777	38.110695
2038.214835	322246.431032	38.115712
2040.017534	322837.827570	38.120730
2041.928947	323450.706983	38.125748
2044.191553	324061.618367	38.130765
2046.068161	324663.904052	38.135783
2048.150540	325274.478090	38.140800
2050.123472	325902.431009	38.145818
2052.216119	326533.023779	38.150836
2054.438565	327151.147861	38.155853
2056.595386	327787.683697	38.160871
2058.570148	328423.024204	38.165888
2060.730617	329056.473985	38.170906
2062.528854	329693.658079	38.175924
2064.780290	330336.066654	38.180941
2066.520121	330993.734464	38.185959
2068.755271	331631.866242	38.190976
2070.778527	332283.125690	38.195994
2072.857960	332945.335574	38.201012
2075.239956	333606.319977	38.206029
2076.972270	334256.716035	38.211047
2078.843171	334919.139965	38.216064
2081.156871	335591.916398	38.221082
2083.488897	336272.754036	38.226100
2085.640323	336928.506967	38.231117
2087.614339	337592.581925	38.236135
2089.872832	338257.515466	38.241152
2092.550140	338921.279978	38.246170
2094.651426	339590.283931	38.251188
2096.661569	340252.466068	38.256205
2098.738799	340927.396295	38.261223
2100.963463	341582.393077	38.266240
2103.654039	342235.959209	38.271258
2105.834586	342907.749138	38.276276
2107.801077	343564.386915	38.281293
2109.878599	344215.388284	38.286311
2111.653997	344891.685007	38.291328
2114.132724	345546.206457	38.296346
2116.138673	346221.481989	38.301364
2118.292933	346887.205944	38.306381
2120.138953	347560.483731	38.311399
2122.539718	348239.852904	38.316416
2124.672505	348899.105428	38.321434
2126.683634	349578.925258	38.326452
2128.589686	350244.413615	38.331469
2130.812688	350919.432774	38.336487
2132.515289	351603.562023	38.341504
2134.679218	352287.427085	38.346522
2136.739023	352978.480383	38.351540
2139.241482	353650.849020	38.356557
2141.698677	354328.898983	38.361575
2143.944296	355014.687398	38.366592
2146.811664	355654.205050	38.371610
2149.046771	356320.816126	38.376628
2151.803641	356956.551637	38.381645
2154.456931	357583.591386	38.386663
2156.314825	358201.263215	38.391680
2158.367268	358808.363923	38.396698
2160.257519	359441.616502	38.401716
2162.208121	360058.230436	38.406733
2163.823285	360681.360269	38.411751
2165.668537	361324.080272	38.416768
2167.833047	361963.845075	38.421786
2169.581315	362606.662081	38.426804
2171.546669	363244.916988	38.431821
2173.825956	363901.985140	38.436839
2175.570703	364561.464481	38.441856
2177.553074	365217.367205	38.446874
2179.724437	365887.002918	38.451892
2181.651800	366569.478242	38.456909
2184.244658	367251.172119	38.461927
2186.331475	367926.747621	38.466944
2188.792050	368598.520503	38.471962
2190.754814	369283.782352	38.476980
2193.471357	369954.118968	38.481997
2195.662319	370637.973906	38.487015
2197.721364	371326.708036	38.492032
2199.858415	372015.898311	38.497050
2201.783652	372715.763424	38.502068
2203.990311	373410.115445	38.507085
2206.240421	374120.552502	38.512103
2208.421447	374826.142599	38.517120
2211.168957	375515.216005	38.522138
2213.098961	376232.156399	38.527156
2215.193869	376943.576987	38.532173
2217.619362	377655.917635	38.537191
2219.406530	378378.619750	38.542208
2221.707096	379088.567675	38.547226
2223.735702	379817.184604	38.552244
2226.424224	380535.584482	38.557261
2228.617867	381260.060556	38.562279
2230.595945	381992.518800	38.567296
2233.367405	382717.147081	38.572314
2235.425759	383442.080023	38.577332
2237.908579	384171.034702	38.582349
2240.401899	384899.667226	38.587367
2242.906432	385628.991586	38.592384
2245.177181	386354.256136	38.597402
2246.853202	387088.298694	38.602420
2249.463663	387822.880267	38.607437
2251.750323	388552.706761	38.612455
2253.672232	389291.424352	38.617472
2256.298779	390026.687472	38.622490
2258.414577	390761.535928	38.627508
2260.578146	391493.798864	38.632525
2263.608497	392211.503201	38.637543
2265.871241	392939.887818	38.642560
2269.003339	393657.541641	38.647578
2271.637923	394380.406160	38.652596
2273.941166	395086.553808	38.657613
2276.875075	395784.115279	38.662631
2279.190089	396492.357105	38.667648
2281.862870	397164.102210	38.672666
2284.656378	397847.242619	38.677684
2286.587180	398551.570329	38.682701
2288.605600	399223.275185	38.687719
2290.816572	399913.128994	38.692736
2293.218432	400597.587794	38.697754
2295.380418	401284.832219	38.702772
2297.670554	401968.390041	38.707789
2300.409698	402637.818983	38.712807
2302.473180	403327.159349	38.717824
2304.614071	403995.286703	38.722842
2306.750479	404657.039040	38.727860
2308.583712	405309.729486	38.732877
2310.937390	405959.810519	38.737895
2312.987319	406616.007327	38.742912
2315.254081	407278.005545	38.747930
2316.957439	407945.806659	38.752948
2318.959064	408634.621078	38.757965
2320.964933	409303.428707	38.762983
2322.767082	410006.479342	38.768000
2324.447985	410697.701244	38.773018
2326.647448	411422.790657	38.778036
2328.384451	412154.041703	38.783053
2330.759646	412876.175045	38.788071
2332.793407	413624.131315	38.793088
2335.080247	414357.004324	38.798106
2337.110400	415126.220834	38.803124
2339.051975	415890.794363	38.808141
2341.420416	416658.466363	38.813159
2344.029713	417439.853616	38.818176
2346.666949	418188.947550	38.823194
2349.695950	418962.976245	38.828212
2352.339351	419739.071048	38.833229
2354.821613	420498.455236	38.838247
2357.362753	421278.267759	38.843264
2359.742371	422042.864289	38.848282
2362.020834	422826.748965	38.853300
2363.710099	423620.176017	38.858317
2366.255528	424410.094393	38.863335
2368.636837	425201.584361	38.868352
2370.729689	425999.324653	38.873370
2373.083659	426813.654570	38.878388
2375.226817	427606.675735	38.883405
2377.870269	428418.018123	38.888423
2379.908168	429233.280890	38.893440
2382.192609	430047.310903	38.898458
2384.831028	430871.784967	38.903476
2387.289333	431714.940360	38.908493
2390.068250	432523.488564	38.913511
2392.193910	433354.845261	38.918528
2394.765782	434180.834564	38.923546
2396.742830	435018.382686	38.928564
2399.106101	435860.797166	38.933581
2401.836082	436698.464050	38.938599
2404.089880	437556.271553	38.943616
2406.392168	438387.064128	38.948634
2408.849998	439235.260304	38.953652
2410.816910	440096.511277	38.958669
2413.149357	440946.991720	38.963687
2415.756626	441822.594226	38.968704
2418.295197	442671.861883	38.973722
2421.236713	443518.601942	38.978740
2423.962054	444380.119181	38.983757
2426.307963	445234.986862	38.988775
2429.059085	446086.212936	38.993792
2431.502215	446931.739889	38.998810
2434.192189	447779.115532	39.003828
2436.792928	448631.784157	39.008845
2439.204818	449469.881930	39.013863
2441.339245	450316.540970	39.018880
2443.962750	451166.171101	39.023898
2446.617708	452011.361728	39.028916
2449.014928	452864.349684	39.033933
2451.793665	453709.906917	39.038951
2453.925208	454557.559543	39.043968
2456.566769	455402.261684	39.048986
2458.714109	456258.388603	39.054004
2460.719899	457108.637759	39.059021
2463.192751	457942.442751	39.064039
2465.238377	458776.840376	39.069056
2467.642965	459603.965230	39.074074
2470.334988	460424.790429	39.079092
2472.892435	461240.801714	39.084109
2475.486152	462074.012544	39.089127
2478.537259	462882.848802	39.094144
2481.842350	463680.843438	39.099162
2484.665203	464486.063197	39.104180
2486.761208	465295.363071	39.109197
2489.981310	466084.884296	39.114215
2492.426362	466892.089757	39.119232
2495.647002	467668.002137	39.124250
2498.605508	468459.289999	39.129268
2500.937617	469246.707146	39.134285
2503.443434	470035.377425	39.139303
2505.730230	470833.702842	39.144320
2507.591040	471634.187452	39.149338
2509.754357	472453.333911	39.154356
2511.758845	473261.305467	39.159373
2514.716330	474071.409485	39.164391
2517.084949	474893.094325	39.169408
2519.470459	475721.711900	39.174426
2522.268554	476544.365029	39.179444
2524.608713	477360.541190	39.184461
2527.199439	478180.731584	39.189479
2529.766168	479020.486931	39.194496
2531.782813	479860.193712	39.199514
2534.259978	480706.200194	39.204532
2536.231330	481570.077999	39.209549
2538.727640	482413.376152	39.214567
2541.058257	483295.595474	39.219584
2543.472534	484158.923581	39.224602
2545.709491	485035.417913	39.229620
2547.903059	485928.538058	39.234637
2550.701751	486808.488189	39.239655
2553.147885	487718.642530	39.244672
2555.480602	488614.331051	39.249690
2557.864446	489530.662118	39.254708
2560.082941	490456.209853	39.259725
2562.931237	491379.484921	39.264743
2565.170321	492306.849189	39.269760
2567.449703	493242.030332	39.274778
2569.926290	494192.570842	39.279796
2572.106346	495146.741062	39.284813
2574.578143	496100.002719	39.289831
2577.417547	497058.902649	39.294848
2579.712958	498035.497138	39.299866
2582.613139	498997.153350	39.304884
2584.827998	499983.032455	39.309901
2587.343692	500970.821879	39.314919
2590.047176	501953.074180	39.319936
2592.703547	502937.495607	39.324954
2595.922683	503899.472860	39.329972
2598.340411	504892.744489	39.334989
2600.945816	505875.738207	39.340007
2603.581135	506858.567099	39.345024
2606.378053	507845.041491	39.350042
2609.189659	508824.949158	39.355060
2612.143152	509827.966411	39.360077
2614.868775	510796.323564	39.365095
2617.573319	511783.378992	39.370112
2620.248558	512774.612584	39.375130
2622.833226	513749.014200	39.380148
2625.720812	514713.174996	39.385165
2628.340231	515685.838611	39.390183
2631.456747	516651.556553	39.395200
2634.274193	517633.087725	39.400218
2637.295816	518568.517154	39.405236
2639.297923	519518.015569	39.410253
2641.828646	520433.359262	39.415271
2644.609772	521355.862231	39.420288
2647.107749	522289.389288	39.425306
2649.801739	523208.016806	39.430324
2652.412636	524131.337651	39.435341
2655.526076	525058.649797	39.440359
2658.225170	525992.118065	39.445376
2660.661912	526920.736972	39.450394
2663.370963	527844.217639	39.455412
2666.516959	528766.159336	39.460429
2669.555950	529679.904423	39.465447
2672.423897	530590.902610	39.470464
2675.134044	531522.311770	39.475482
2678.049645	532446.076680	39.480500
2680.188717	533366.991793	39.485517
2682.664351	534296.904705	39.490535
2685.293056	535235.340379	39.495552
2687.359066	536186.491755	39.500570
2689.943320	537134.073031	39.505588
2692.286631	538096.980872	39.510605
2694.396239	539065.599449	39.515623
2696.917523	540052.400419	39.520640
2699.367767	541033.107260	39.525658
2702.269180	542030.073489	39.530676
2705.066796	543016.271333	39.535693
2707.653072	544018.834191	39.540711
2710.415051	545025.018917	39.545728
2713.359864	546038.344028	39.550746
2716.077070	547048.615627	39.555764
2718.869190	548059.053037	39.560781
2721.217052	549081.407728	39.565799
2723.911348	550098.199299	39.570816
2726.612564	551139.198895	39.575834
2729.707146	552175.680836	39.580852
2732.655200	553204.919687	39.585869
2735.466628	554228.473428	39.590887
2738.705122	555260.926853	39.595904
2741.120638	556285.345400	39.600922
2744.281245	557322.428518	39.605940
2746.662649	558370.564905	39.610957
2749.161254	559413.022398	39.615975
2751.851621	560451.497997	39.620992
2754.543286	561507.827545	39.626010
2757.617408	562554.766410	39.631028
2760.514093	563615.213753	39.636045
2763.053760	564655.493200	39.641063
2766.174121	565708.300669	39.646080
2768.721894	566772.466965	39.651098
2771.697943	567814.230255	39.656116
2774.200124	568883.603754	39.661133
2777.014344	569938.578430	39.666151
2779.933357	571002.686464	39.671168
2782.595085	572063.184348	39.676186
2785.226303	573132.634032	39.681204
2788.359596	574192.977151	39.686221
2791.123406	575273.868507	39.691239
2794.172638	576336.755633	39.696256
2796.417575	577415.892670	39.701274
2799.608943	578473.356956	39.706292
2802.795802	579542.220995	39.711309
2805.201762	580606.306100	39.716327
2808.490335	581665.339025	39.721344
2810.962242	582745.029695	39.726362
2813.428215	583809.280349	39.731380
2816.212118	584889.232665	39.736397
2818.513028	585973.681960	39.741415
2821.001779	587042.009727	39.746432
2823.895957	588089.922651	39.751450
2827.103423	589148.170149	39.756468
2829.945330	590181.974139	39.761485
2832.509062	591227.663697	39.766503
2835.852670	592262.809447	39.771520
2838.459043	593303.950189	39.776538
2841.550083	594354.690853	39.781556
2844.328039	595393.816161	39.786573
2847.073661	596459.858507	39.791591
2849.866645	597507.311834	39.796608
2852.652242	598557.477886	39.801626
2855.286839	599618.543141	39.806644
2858.316392	600696.724450	39.811661
2860.984732	601776.117104	39.816679
2863.709394	602842.281229	39.821696
2866.319196	603931.896979	39.826714
2869.036643	605016.135282	39.831732
2872.146890	606118.226739	39.836749
2874.917396	607217.114566	39.841767
2877.880579	608319.868328	39.846784
2880.405360	609447.808407	39.851802
2883.412600	610558.143513	39.856820
2886.542898	611669.249493	39.861837
2888.953349	612792.971027	39.866855
2892.296480	613927.080752	39.871872
2895.054653	615051.668279	39.876890
2898.016434	616189.011563	39.881908
2901.119497	617323.164350	39.886925
2903.964182	618479.343918	39.891943
2907.044488	619609.514978	39.896960
2909.656360	620758.293460	39.901978
2912.297339	621913.894406	39.906996
2915.173024	623077.580823	39.912013
2917.671405	624257.746395	39.917031
2920.934342	625421.766789	39.922048
2923.522222	626607.207352	39.927066
2926.293115	627788.739981	39.932084
2928.989424	628983.641796	39.937101
2931.650687	630195.797221	39.942119
2934.624618	631398.673430	39.947136
2937.514905	632612.462637	39.952154
2940.385036	633829.211201	39.957172
2943.187560	635045.031291	39.962189
2946.439245	636284.946655	39.967207
2949.487174	637506.130861	39.972224
2952.194432	638738.856139	39.977242
2954.804221	639989.165685	39.982260
2958.081082	641217.160448	39.987277
2961.806310	642459.701898	39.992295
2964.885846	643692.372269	39.997312
2967.990778	644939.802926	40.002330
2970.688297	646173.034522	40.007348
2974.090925	647404.005484	40.012365
2976.887535	648645.546329	40.017383
2980.196892	649870.548003	40.022400
2983.483826	651110.706760	40.027418
2986.533904	652337.343879	40.032436
2990.242143	653550.216662	40.037453
2992.844061	654779.566965	40.042471
2996.263476	656014.857733	40.047488
2999.206116	657226.260685	40.052506
3001.938113	658442.679586	40.057524
3004.874287	659662.798625	40.062541
3007.578758	660890.024101	40.067559
3011.055881	662115.125411	40.072576
3013.732739	663340.502696	40.077594
3016.650619	664562.051307	40.082612
3019.788620	665775.495219	40.087629
3022.815800	666963.374002	40.092647
3026.145299	668141.750678	40.097664
3029.199932	669327.639517	40.102682
3031.536772	670492.853845	40.107700
3034.887678	671678.848258	40.112717
3037.594637	672854.256319	40.117735
3040.758959	674037.548300	40.122752
3043.200597	675235.528223	40.127770
3046.220107	676433.160379	40.132788
3049.466006	677620.063278	40.137805
3051.890934	678844.128096	40.142823
3055.024188	680056.584017	40.147840
3057.999801	681272.236265	40.152858
3061.098292	682503.407990	40.157876
3064.336569	683730.815089	40.162893
3067.087138	684958.982542	40.167911
3070.240826	686208.323331	40.172928
3073.736986	687430.423144	40.177946
3076.712944	688683.524854	40.182964
3079.967312	689925.584989	40.187981
3082.665398	691177.095813	40.192999
3085.968655	692428.630464	40.198016
3089.134778	693706.064445	40.203034
3091.877776	694969.592481	40.208052
3095.113383	696246.204522	40.213069
3097.896149	697525.385927	40.218087
3101.031874	698796.190835	40.223104
3104.246228	700092.733200	40.228122
3107.343213	701382.608742	40.233140
3110.784381	702683.292047	40.238157
3113.514727	703984.592543	40.243175
3116.570048	705273.602583	40.248192
3119.828554	706590.283816	40.253210
3122.856677	707906.158386	40.258228
3125.929218	709222.617196	40.263245
3128.959494	710560.920405	40.268263
3132.299710	711863.904012	40.273280
3135.422995	713204.204258	40.278298
3138.210291	714522.567127	40.283316
3141.744195	715850.253538	40.288333
3145.224191	717191.349244	40.293351
3148.507761	718527.167235	40.298368
3151.806664	719860.642737	40.303386
3154.738204	721200.050228	40.308404
3157.943618	722541.175637	40.313421
3161.073088	723887.882507	40.318439
3164.332796	725229.701562	40.323456
3167.393970	726574.251687	40.328474
3170.525945	727928.405768	40.333492
3174.139553	729264.368405	40.338509
3176.611387	730628.463109	40.343527
3179.480697	731993.696550	40.348544
3182.674464	733365.808702	40.353562
3185.415703	734750.651616	40.358580
3188.613413	736128.713632	40.363597
3191.875850	737510.527397	40.368615
3194.948152	738881.966693	40.373632
3198.047776	740276.359788	40.378650
3201.042405	741689.176352	40.383668
3204.201672	743060.276279	40.388685
3207.373927	744471.679350	40.393703
3210.603912	745869.061755	40.398720
3213.934940	747271.799711	40.403738
3217.147175	748673.960891	40.408756
3220.670657	750075.424605	40.413773
3224.050156	751485.283211	40.418791
3227.235738	752872.598504	40.423808
3230.873263	754255.994314	40.428826
3234.087967	755621.037522	40.433844
3237.438268	756963.114764	40.438861
3240.346771	758300.943054	40.443879
3243.733091	759655.391759	40.448896
3247.173646	760993.840977	40.453914
3250.149464	762349.943919	40.458932
3253.598972	763682.405100	40.463949
3257.143657	765026.568388	40.468967
3259.952905	766365.104013	40.473984
3263.517426	767706.914881	40.479002
3266.579027	769064.939189	40.484020
3270.418478	770412.707473	40.489037
3274.278467	771750.300063	40.494055
3277.763142	773080.636879	40.499072
3281.537707	774423.361221	40.504090
3284.638519	775768.751234	40.509108
3287.741395	777101.076222	40.514125
3290.501802	778461.644654	40.519143
3293.327943	779819.935534	40.524160
3296.651795	781187.510840	40.529178
3299.536856	782579.780632	40.534196
3302.575669	783965.133054	40.539213
3305.693193	785365.412908	40.544231
3308.358738	786771.526580	40.549248
3311.567352	788179.137831	40.554266
3314.894255	789622.240454	40.559284
3317.868483	791052.168174	40.564301
3321.172306	792498.856069	40.569319
3324.017760	793942.824462	40.574336
3327.382363	795395.571559	40.579354
3330.731017	796879.609588	40.584372
3334.086616	798342.717588	40.589389
3337.595126	799824.291961	40.594407
3340.648882	801325.692462	40.599424
3344.133848	802815.148408	40.604442
3346.815248	804310.971152	40.609460
3350.508852	805820.339909	40.614477
3353.480481	807329.153263	40.619495
3356.613548	808847.580813	40.624512
3360.190668	810378.843299	40.629530
3363.522539	811910.192022	40.634548
3366.801122	813452.928951	40.639565
3370.442020	814991.297075	40.644583
3373.779778	816531.707400	40.649600
3377.167548	818055.595022	40.654618
3380.783366	819612.143545	40.659636
3384.715472	821145.632627	40.664653
3388.278424	822684.536676	40.669671
3391.759624	824227.291241	40.674688
3395.051919	825768.643206	40.679706
3398.449941	827319.659994	40.684724
3401.486573	828865.056128	40.689741
3404.907375	830416.602198	40.694759
3408.227339	831966.138600	40.699776
3412.130241	833509.169044	40.704794
3415.500212	835076.316425	40.709812
3419.085140	836617.925772	40.714829
3422.796439	838154.374403	40.719847
3426.318747	839694.378542	40.724864
3429.781800	841252.848620	40.729882
3432.944946	842803.398854	40.734900
3436.005530	844349.307851	40.739917
3439.688179	845904.459341	40.744935
3442.897024	847453.278403	40.749952
3446.370684	849018.192771	40.754970
3449.734556	850584.871573	40.759988
3452.986753	852128.543726	40.765005
3456.925293	853670.670271	40.770010
3460.485845	855161.602804	40.775015
3463.968073	856590.883273	40.780020
3467.045452	857964.055407	40.785024
3470.178471	859277.481073	40.790029
3473.453396	860508.621931	40.795034
3475.279767	861684.138244	40.800039
3478.112539	862791.894615	40.805044
3481.245426	863827.378346	40.810048
3483.664282	864812.755666	40.815053
3486.263212	865698.543442	40.820058
3488.439691	866545.118930	40.825063
3490.779771	867315.100346	40.830068
3492.602330	868026.306374	40.835072
3494.642041	868684.852232	40.840077
3496.771523	869275.044585	40.845082
3498.554848	869817.560372	40.850087
3500.441867	870304.668162	40.855092
3501.863351	870736.280997	40.860096
3503.405211	871125.322829	40.865101
3504.964625	871470.848143	40.870106
3506.029532	871765.474597	40.875111
3507.471678	872014.987017	40.880116
3508.199554	872245.777060	40.885120
3509.234656	872428.852814	40.890125
3510.560354	872563.347910	40.895130
3511.101998	872686.905110	40.900135
3512.258695	872761.541733	40.905140
3512.814524	872823.368686	40.910144
3513.864198	872845.420278	40.915149
3514.276285	872856.027872	40.920154
3514.992790	872839.314252	40.925159
3515.483911	872788.184680	40.930164
3516.012224	872732.195949	40.935168
3516.575253	872657.663846	40.940173
3516.919755	872547.935959	40.945178
3517.242906	872439.762483	40.950183
3517.963494	872303.956913	40.955188
3517.944486	872158.563960	40.960192
3518.182657	872006.427712	40.965197
3518.557708	871823.203773	40.970202
3518.862857	871659.205508	40.975207
3519.446368	871445.941163	40.980212
3519.564186	871241.191562	40.985216
3519.498444	871030.057944	40.990221
3519.711890	870793.338005	40.995226
3519.678415	870575.193028	41.000231
3519.879084	870331.272506	41.005236
3520.350406	870090.501615	41.010240
3520.310737	869845.241594	41.015245
3520.342419	869583.937824	41.020250
3520.231695	869329.832072	41.025255
3520.546832	869041.365070	41.030260
3520.331606	868788.516101	41.035264
3520.031369	868504.786282	41.040269
3519.998137	868235.762090	41.045274
3519.872875	867963.438647	41.050279
3520.858566	867687.811633	41.055284
3520.416279	867398.030792	41.060288
3520.467387	867114.954757	41.065293
3520.479686	866813.608104	41.070298
3520.419139	866533.340476	41.075303
3520.412725	866222.543655	41.080308
3520.676922	865930.924367	41.085312
3520.275688	865628.809469	41.090317
3520.208745	865326.624429	41.095322
3520.321685	865035.084080	41.100327
3520.384916	864731.195911	41.105332
3519.965551	864429.510099	41.110336
3519.898777	864132.610745	41.115341
3519.786164	863833.468928	41.120346
3519.706254	863538.875408	41.125351
3520.328162	863227.335544	41.130356
3519.866124	862929.859313	41.135360
3520.070028	862628.078616	41.140365
3520.110677	862314.740725	41.145370
3519.736206	862013.802631	41.150375
3520.000907	861711.966569	41.155380
3519.685672	861397.862356	41.160384
3519.497388	861091.500214	41.165389
3519.594958	860788.868145	41.170394
3519.089003	860480.874569	41.175399
3519.404474	860166.311424	41.180404
3519.174058	859868.064258	41.185408
3519.248337	859579.867765	41.190413
3519.125054	859266.595117	41.195418
3518.881473	858965.485417	41.200423
3519.000772	858661.869224	41.205428
3518.890237	858362.361748	41.210432
3518.495530	858059.675997	41.215437
3518.721207	857770.202161	41.220442
3518.542221	857472.900341	41.225447
3518.418901	857172.072143	41.230452
3518.056273	856871.949812	41.235456
3517.947077	856582.475302	41.240461
3517.742960	856283.660568	41.245466
3517.669644	856002.716690	41.250471
3517.500884	855717.298832	41.255476
3517.266577	855440.930156	41.260480
3517.396619	855159.817121	41.265485
3517.391773	854875.501391	41.270490
3517.458740	854608.000921	41.275495
3517.127521	854308.040843	41.280500
3517.006695	854037.334225	41.285504
3517.100277	853763.562464	41.290509
3516.997037	853475.986002	41.295514
3516.800341	853217.912846	41.300519
3516.520428	852926.250744	41.305524
3516.594020	852669.570806	41.310528
3516.610161	852386.208599	41.315533
3516.474176	852111.914974	41.320538
3516.358431	851859.420173	41.325543
3516.466384	851594.996841	41.330548
3516.233544	851320.489529	41.335552
3516.157312	851050.327222	41.340557
3516.064496	850785.415635	41.345562
3515.820836	850535.615526	41.350567
3515.983607	850260.801612	41.355572
3515.717197	850007.672200	41.360576
3515.830638	849731.674182	41.365581
3515.725663	849475.086984	41.370586
3515.122472	849216.233103	41.375591
3515.081271	848962.244879	41.380596
3515.093054	848718.565625	41.385600
3514.959384	848467.495594	41.390605
3515.068725	848204.390149	41.395610
3514.625294	847982.584207	41.400615
3514.809427	847725.585421	41.405620
3514.286856	847493.835411	41.410624
3514.239192	847242.799676	41.415629
3513.950917	847004.073577	41.420634
3513.957015	846784.490334	41.425639
3513.968164	846538.679854	41.430644
3514.079890	846312.532415	41.435648
3513.726018	846085.381328	41.440653
3514.001310	845860.360416	41.445658
3513.639182	845628.612752	41.450663
3513.898121	845394.804566	41.455668
3513.482439	845169.580374	41.460672
3513.641016	844951.955441	41.465677
3513.867800	844709.352874	41.470682
3513.471842	844486.830970	41.475687
3513.452212	844255.561492	41.480692
3513.622921	844026.397349	41.485696
3513.085747	843798.706651	41.490701
3513.090680	843563.458682	41.495706
3512.701852	843361.910178	41.500711
3512.887028	843134.612962	41.505716
3512.556728	842914.609255	41.510720
3512.702802	842708.758365	41.515725
3512.452694	842501.503109	41.520730
3512.329695	842294.561515	41.525735
3512.412720	842073.777848	41.530740
3512.447102	841878.306065	41.535744
3512.432074	841675.910894	41.540749
3512.351579	841466.643092	41.545754
3512.280980	841262.585646	41.550759
3511.994797	841057.532872	41.555764
3511.846278	840849.670494	41.560768
3511.953038	840653.856517	41.565773
3511.352246	840455.128671	41.570778
3511.574303	840263.186153	41.575783
3511.615724	840067.803982	41.580788
3511.571458	839878.430507	41.585792
3511.243792	839687.683286	41.590797
3510.890545	839494.641544	41.595802
3510.901836	839306.461655	41.600807
3510.813569	839125.757620	41.605812
3510.862973	838950.539314	41.610816
3510.825071	838777.428709	41.615821
3510.960310	838593.208480	41.620826
3511.031542	838416.849686	41.625831
3510.946207	838227.141285	41.630836
3511.054015	838045.056904	41.635840
3510.615013	837856.664563	41.640845
3511.162211	837673.716454	41.645850
3510.739967	837491.703667	41.650855
3510.462175	837321.033386	41.655860
3510.332948	837135.106656	41.660864
3510.235829	836976.940583	41.665869
3510.249983	836794.689722	41.670874
3510.138622	836638.225953	41.675879
3509.839774	836459.873119	41.680884
3509.770369	836302.564480	41.685888
3509.961057	836129.149502	41.690893
3510.134892	835963.835896	41.695898
3509.845945	835805.184444	41.700903
3509.789445	835634.188834	41.705908
3509.672155	835474.329338	41.710912
3509.361161	835315.034799	41.715917
3509.712981	835159.288716	41.720922
3509.274593	835000.934994	41.725927
3509.249081	834846.854650	41.730932
3509.559711	834692.910556	41.735936
3509.422972	834531.566156	41.740941
3509.416910	834378.154979	41.745946
3509.221498	834222.622915	41.750951
3509.202301	834087.810456	41.755956
3509.336289	833912.489705	41.760960
3509.161914	833766.953424	41.765965
3509.330414	833605.975114	41.770970
3508.859392	833459.601790	41.775975
3509.035913	833305.695583	41.780980
3508.991999	833158.317226	41.785984
3508.713451	833004.283467	41.790989
3508.758162	832854.588250	41.795994
3508.735793	832724.094511	41.800999
3508.511640	832585.719244	41.806004
3508.824610	832441.586943	41.811008
3508.537420	832294.619744	41.816013
3508.477283	832142.825131	41.821018
3508.359992	832015.068005	41.826023
3508.427379	831871.256557	41.831028
3508.224132	831726.460718	41.836032
3508.398650	831584.872235	41.841037
3508.530213	831449.393863	41.846042
3508.196472	831318.874303	41.851047
3507.855395	831175.358979	41.856052
3507.920303	831044.426285	41.861056
3507.730291	830917.050358	41.866061
3507.885756	830778.427480	41.871066
3508.223028	830663.612905	41.876071
3508.033994	830516.833586	41.881076
3507.543054	830393.161164	41.886080
3507.371291	830273.489012	41.891085
3507.742965	830146.787215	41.896090
3507.434376	830015.309041	41.901095
3507.381239	829897.222808	41.906100
3507.136551	829764.556393	41.911104
3507.185522	829646.204487	41.916109
3507.660697	829529.832491	41.921114
3507.277629	829413.453197	41.926119
3507.289119	829309.369687	41.931124
3507.373947	829187.192081	41.936128
3507.100118	829069.518144	41.941133
3507.288385	828936.910187	41.946138
3506.994665	828817.280270	41.951143
3506.836129	828709.012491	41.956148
3507.080964	828591.537727	41.961152
3507.043202	828478.017100	41.966157
3507.435297	828369.897364	41.971162
3507.052869	828255.647696	41.976167
3507.121881	828132.671019	41.981172
3507.213649	828013.989255	41.986176
3507.046777	827900.430997	41.991181
3506.834420	827785.900733	41.996186
3506.817314	827673.340270	42.001191
3506.736581	827563.183378	42.006196
3506.762587	827452.420505	42.011200
3506.480556	827332.517112	42.016205
3506.723566	827232.468314	42.021210
3506.382197	827141.703916	42.026215
3506.299321	827027.139058	42.031220
3506.472049	826928.661429	42.036224
3506.223153	826834.797934	42.041229
3506.325398	826719.463959	42.046234
3506.134990	826627.885432	42.051239
3506.495338	826515.731775	42.056244
3506.233951	826414.726992	42.061248
3506.199919	826328.300505	42.066253
3506.334966	826221.752082	42.071258
3506.038161	826125.050823	42.076263
3506.279463	826018.628272	42.081268
3506.138582	825922.387241	42.086272
3505.819003	825835.756859	42.091277
3506.013403	825721.710244	42.096282
3505.927901	825641.590237	42.101287
3505.488775	825538.645568	42.106292
3505.914291	825449.442709	42.111296
3505.597685	825361.729928	42.116301
3505.884649	825265.946656	42.121306
3505.614220	825175.387866	42.126311
3505.942650	825078.030367	42.131316
3505.830038	824984.900342	42.136320
3505.477297	824893.128797	42.141325
3505.808189	824803.932788	42.146330
3505.560761	824727.886911	42.151335
3505.773804	824627.950117	42.156340
3505.415581	824541.064554	42.161344
3505.472416	824465.210031	42.166349
3505.539006	824357.958105	42.171354
3505.446923	824279.827591	42.176359
3505.517359	824185.482461	42.181364
3505.701766	824099.284146	42.186368
3505.443101	824012.570835	42.191373
3505.564717	823934.841176	42.196378
3505.292429	823849.546212	42.201383
3505.347981	823769.771455	42.206388
3505.188756	823677.217515	42.211392
3505.125061	823610.812054	42.216397
3505.232743	823514.445998	42.221402
3505.221492	823425.923535	42.226407
3505.046839	823358.213275	42.231412
3505.198090	823270.444511	42.236416
3505.066966	823203.899338	42.241421
3505.306001	823126.483204	42.246426
3504.957670	823052.146519	42.251431
3504.911518	822965.677928	42.256436
3504.692131	822885.595403	42.261440
3504.717517	822805.911810	42.266445
3504.901356	822735.396973	42.271450
3504.529906	822666.440283	42.276455
3504.690178	822590.253712	42.281460
3504.752285	822516.674955	42.286464
3504.760401	822462.181501	42.291469
3504.887656	822379.002962	42.296474
3504.408206	822309.473343	42.301479
3504.344093	822239.629992	42.306484
3504.751888	822170.588698	42.311488
3504.403683	822097.366378	42.316493
3504.564453	822023.032110	42.321498
3504.279304	821968.142626	42.326503
3504.272709	821885.762657	42.331508
3504.751663	821809.905985	42.336512
3504.369190	821756.351637	42.341517
3504.286397	821679.950035	42.346522
3504.549122	821616.161485	42.351527
3504.280505	821558.379477	42.356532
3504.401419	821496.863578	42.361536
3504.004009	821433.524471	42.366541
3504.185378	821369.844802	42.371546
3504.341405	821302.695064	42.376551
3504.298689	821246.047312	42.381556
3504.318928	821179.212241	42.386560
3504.191199	821123.164548	42.391565
3504.330244	821048.186906	42.396570
3503.752075	820992.212303	42.401575
3503.866834	820925.359108	42.406580
3504.234663	820861.643857	42.411584
3503.838077	820808.622384	42.416589
3503.751280	820733.727322	42.421594
3503.851346	820703.472836	42.426599
3504.090716	820632.877581	42.431604
3504.093964	820572.889320	42.436608
3503.933993	820527.900046	42.441613
3504.080510	820460.009409	42.446618
3503.910556	820393.491349	42.451623
3503.927271	820344.214718	42.456628
3504.045246	820281.611563	42.461632
3503.921567	820223.989796	42.466637
3503.781048	820167.936154	42.471642
3503.428016	820116.859297	42.476647
3503.476286	820061.801260	42.481652
3503.690588	819998.885977	42.486656
3503.494051	819964.664396	42.491661
3503.792136	819906.432131	42.496666
3503.671031	819860.061766	42.501671
3503.953919	819805.794863	42.506676
3503.676428	819754.947461	42.511680
3503.449001	819706.440362	42.516685
3503.906690	819637.707107	42.521690
3503.690324	819594.433594	42.526695
3503.503148	819530.552343	42.531700
3503.341832	819480.760335	42.536704
3503.615255	819431.385728	42.541709
3503.663411	819375.685844	42.546714
3503.567731	819337.871908	42.551719
3503.541432	819273.619122	42.556724
3503.403766	819232.141049	42.561728
3503.353173	819183.845714	42.566733
3503.155541	819140.370405	42.571738
3503.304593	819095.516310	42.576743
3503.445265	819043.811549	42.581748
3503.442770	818994.968573	42.586752
3503.250978	818951.442128	42.591757
3502.940364	818899.467992	42.596762
3503.194831	818861.544737	42.601767
3503.104038	818821.377832	42.606772
3503.190854	818776.336072	42.611776
3503.018527	818731.336695	42.616781
3503.187303	818685.595616	42.621786
3503.173187	818635.626219	42.626791
3503.150188	818599.117612	42.631796
3502.736586	818558.855466	42.636800
3502.731429	818518.770523	42.641805
3503.214922	818480.660548	42.646810
3502.975112	818446.193569	42.651815
3502.797174	818400.899215	42.656820
3503.399835	818358.168010	42.661824
3503.206629	818322.322225	42.666829
3503.148503	818273.874708	42.671834
3503.154836	818240.002428	42.676839
3503.107527	818191.454637	42.681844
3503.225212	818151.445151	42.686848
3503.019505	818112.712392	42.691853
3503.071668	818068.209994	42.696858
3502.876709	818023.943799	42.701863
3502.773996	817992.388807	42.706868
3502.914156	817951.884937	42.711872
3502.800046	817909.415781	42.716877
3502.970520	817867.291077	42.721882
3502.886440	817837.641322	42.726887
3502.690624	817792.394737	42.731892
3502.895126	817754.424485	42.736896
3502.618616	817723.924813	42.741901
3502.809379	817682.823571	42.746906
3502.673155	817658.223563	42.751911
3502.661450	817621.707757	42.756916
3502.843758	817574.684113	42.761920
3502.830905	817545.119232	42.766925
3503.231883	817506.919406	42.771930
3502.965687	817465.843150	42.776935
3502.760124	817435.526286	42.781940
3502.724178	817384.425218	42.786945
3502.479732	817366.107969	42.791949
3502.938866	817323.197994	42.796954
3502.833468	817291.150599	42.801959
3502.792662	817249.693212	42.806964
3502.785067	817203.040920	42.811969
3502.699648	817180.633740	42.816973
3502.802841	817140.914330	42.821978
3502.876462	817103.157766	42.826983
3502.483521	817065.967396	42.831988
3502.803735	817038.058857	42.836993
3502.876772	817004.120378	42.841997
3502.528989	816960.410834	42.847002
3502.851814	816925.451686	42.852007
3502.652839	816899.978008	42.857012
3502.832994	816857.845362	42.862017
3503.014478	816828.685922	42.867021
3502.958802	816797.215460	42.872026
3502.601514	816754.387370	42.877031
3502.678448	816725.783240	42.882036
3502.977901	816687.301723	42.887041
3502.921343	816647.556746	42.892045
3502.836906	816614.376612	42.897050
3502.885897	816565.066781	42.902055
3502.542278	816539.811395	42.907060
3502.744930	816496.497750	42.912065
3502.600796	816489.422296	42.917069
3502.742468	816437.990995	42.922074
3502.876860	816396.450512	42.927079
3502.595596	816362.567147	42.932084
3502.787790	816325.325240	42.937089
3502.613136	816303.566318	42.942093
3502.513524	816265.197078	42.947098
3502.761397	816235.142819	42.952103
3502.595809	816203.883523	42.957108
3502.553869	816152.578204	42.962113
3502.146231	816135.214746	42.967117
3502.573435	816090.343661	42.972122
3502.851459	816069.341780	42.977127
3502.593907	816035.208040	42.982132
3502.644270	816000.435847	42.987137
3502.824594	815971.566656	42.992141
3503.006944	815939.465401	42.997146
3502.631825	815903.293877	43.002151
3502.545273	815861.100980	43.007156
3502.783724	815825.121754	43.012161
3502.583717	815803.169527	43.017165
3502.259883	815763.414373	43.022170
3502.386131	815744.150254	43.027175
3502.309187	815714.440962	43.032180
3502.517609	815677.045894	43.037185
3502.416013	815644.451378	43.042189
3502.735190	815622.510972	43.047194
3502.447994	815596.802043	43.052199
3502.410148	815550.534972	43.057204
3502.795296	815525.400554	43.062209
3502.525504	815503.948510	43.067213
3502.515629	815454.885058	43.072218
3502.435459	815435.115415	43.077223
3502.142221	815410.092309	43.082228
3502.488678	815378.744827	43.087233
3502.410957	815344.675889	43.092237
3502.437820	815315.535352	43.097242
3502.255009	815292.452350	43.102247
3502.061866	815252.770582	43.107252
3502.282352	815224.136412	43.112257
3502.147566	815207.460139	43.117261
3502.212648	815191.926164	43.122266
3502.006365	815152.441844	43.127271
3502.090509	815131.322066	43.132276
3502.274343	815116.355991	43.137281
3502.573933	815098.187775	43.142285
3502.451937	815069.952152	43.147290
3502.411893	815044.445247	43.152295
3502.400148	815012.714332	43.157300
3502.534261	814982.183511	43.162305
3502.425949	814956.834431	43.167309
3502.367898	814913.651474	43.172314
3502.387288	814901.209541	43.177319
3502.105960	814872.313734	43.182324
3502.402822	814844.595830	43.187329
3502.473452	814814.466479	43.192333
3502.451618	814793.461041	43.197338
3502.415450	814756.541897	43.202343
3502.102512	814726.671224	43.207348
3502.426712	814695.324231	43.212353
3502.463816	814687.972157	43.217357
3502.459698	814647.129303	43.222362
3502.475096	814614.020790	43.227367
3502.098110	814595.179090	43.232372
3502.170945	814557.310401	43.237377
3501.913910	814542.758490	43.242381
3502.216364	814515.038310	43.247386
3502.380803	814483.031008	43.252391
3502.150490	814459.267329	43.257396
3502.305974	814434.313600	43.262401
3501.918265	814395.393443	43.267405
3502.117430	814382.284264	43.272410
3502.497349	814360.182822	43.277415
3502.079492	814334.196731	43.282420
3502.545768	814310.758565	43.287425
3502.558282	814302.381634	43.292429
3502.099879	814253.285352	43.297434
3502.213350	814244.255030	43.302439
3502.005763	814210.495599	43.307444
3502.391423	814181.486959	43.312449
3502.238656	814167.455802	43.317453
3501.969546	814138.456877	43.322458
3501.879417	814092.727143	43.327463
3502.260529	814093.252057	43.332468
3502.432030	814056.245892	43.337473
3502.328369	814043.234914	43.342477
3502.209218	814005.149860	43.347482
3502.360773	813990.872297	43.352487
3502.371940	813962.708051	43.357492
3502.085914	813935.719142	43.362497
3502.133330	813906.226274	43.367501
3502.004506	813887.684562	43.372506
3502.262247	813855.707895	43.377511
3502.378045	813829.631951	43.382516
3502.333900	813794.863933	43.387521
3502.067163	813783.446655	43.392525
3502.588176	813748.585306	43.397530
3502.266453	813728.115742	43.402535
3502.031167	813709.933936	43.407540
3502.575815	813674.284632	43.412545
3502.285377	813643.229918	43.417549
3502.084626	813619.801270	43.422554
3502.044378	813589.880634	43.427559
3501.863707	813584.571444	43.432564
3502.006035	813549.575522	43.437569
3501.762869	813545.452142	43.442573
3501.887382	813530.443343	43.447578
3502.177103	813497.578050	43.452583
3502.126299	813487.398220	43.457588
3502.367699	813468.451502	43.462593
3502.281105	813447.011699	43.467597
3502.437966	813415.735313	43.472602
3502.342034	813397.529711	43.477607
3501.873612	813357.588224	43.482612
3502.011746	813351.589564	43.487617
3502.130785	813309.199861	43.492621
3501.773788	813287.118331	43.497626
3502.037152	813256.068578	43.502631
3502.036139	813255.970742	43.507636
3502.230717	813226.352698	43.512641
3501.770564	813194.246234	43.517645
3501.683117	813196.905722	43.522650
3501.956100	813162.033224	43.527655
3501.585217	813150.240154	43.532660
3502.205341	813125.988800	43.537665
3502.162960	813106.793908	43.542669
3502.218774	813085.427469	43.547674
3502.340726	813058.171907	43.552679
3502.071154	813031.666515	43.557684
3502.070035	813003.059425	43.562689
3502.011772	812997.827579	43.567693
3501.978940	812970.842086	43.572698
3502.286234	812951.099300	43.577703
3502.314288	812941.983339	43.582708
3501.899442	812899.385094	43.587713
3502.009090	812888.002270	43.592717
3501.584817	812858.386578	43.597722
3502.075010	812832.098158	43.602727
3501.970965	812811.687926	43.607732
3501.936863	812793.470510	43.612737
3502.265288	812772.009190	43.617741
3501.972862	812755.695720	43.622746
3501.823066	812735.047858	43.627751
3502.031427	812714.193977	43.632756
3502.003091	812700.923066	43.637761
3502.171919	812684.092560	43.642765
3501.782167	812657.556507	43.647770
3501.541031	812642.214066	43.652775
3501.814740	812624.974235	43.657780
3502.010415	812589.621644	43.662785
3501.831260	812591.953558	43.667789
3501.814328	812567.756157	43.672794
3501.970957	812541.227624	43.677799
3501.902795	812533.890545	43.682804
3502.017926	812502.959732	43.687809
3501.963027	812486.116598	43.692813
3501.793865	812472.819447	43.697818
3501.823353	812434.652061	43.702823
3502.028189	812432.658716	43.707828
3502.089888	812396.837294	43.712833
3502.094496	812391.643611	43.717837
3501.722538	812360.302483	43.722842
3502.119660	812333.145645	43.727847
3501.975578	812336.745608	43.732852
3502.106993	812303.459684	43.737857
3502.146815	812291.989380	43.742861
3502.460679	812252.353408	43.747866
3502.591856	812233.274419	43.752871
3502.387013	812209.694579	43.757876
3502.722155	812170.887470	43.762881
3502.152743	812149.572071	43.767885
3501.967746	812127.850345	43.772890
3502.384047	812096.231177	43.777895
3501.949861	812080.331358	43.782900
3502.199334	812050.454169	43.787905
3502.139819	812035.717329	43.792909
3502.162604	812001.516966	43.797914
3502.291856	811982.584566	43.802919
3501.874766	811960.655569	43.807924
3502.075407	811940.584462	43.812929
3501.974178	811928.940806	43.817933
3501.964848	811912.284709	43.822938
3501.988976	811872.302295	43.827943
3501.642672	811875.396885	43.832948
3502.119181	811854.202230	43.837953
3502.121357	811824.511760	43.842957
3502.244644	811810.871174	43.847962
3502.176742	811770.560363	43.852967
3502.076492	811758.083354	43.857972
3501.861950	811729.163075	43.862977
3502.243334	811713.471012	43.867981
3501.676021	811685.392565	43.872986
3501.814099	811662.048298	43.877991
3502.070021	811652.697088	43.882996
3501.824107	811641.174759	43.888001
3501.752834	811616.884921	43.893005
3501.527053	811608.739883	43.898010
3501.539378	811574.098128	43.903015
3501.461889	811570.142224	43.908020
3501.700675	811552.709442	43.913025
3501.482813	811554.068173	43.918029
3502.031597	811534.624458	43.923034
3501.807762	811508.056560	43.928039
3501.740432	811505.323843	43.933044
3502.222117	811468.791388	43.938049
3501.794202	811453.330024	43.943053
3501.604648	811444.051905	43.948058
3501.788319	811406.686270	43.953063
3501.722613	811397.583674	43.958068
3501.861166	811391.926191	43.963073
3502.103345	811358.764375	43.968077
3501.577627	811348.463563	43.973082
3501.987718	811339.772488	43.978087
3501.755625	811319.035865	43.983092
3501.840717	811288.496436	43.988097
3501.663388	811279.755051	43.993101
3501.705739	811273.574343	43.998106
3501.837409	811256.354434	44.003111
3501.639956	811238.845710	44.008116
3501.745535	811224.667886	44.013121
3501.733246	811204.188694	44.018125
3502.125095	811198.538326	44.023130
3501.898056	811165.746845	44.028135
3501.820959	811152.725924	44.033140
3501.888137	811128.803520	44.038145
3501.899518	811112.044048	44.043149
3501.945572	811096.993784	44.048154
3502.164038	811079.073146	44.053159
3501.837226	811071.532090	44.058164
3501.947783	811033.196462	44.063169
3502.112212	811030.523376	44.068173
3501.790820	810997.991622	44.073178
3501.768222	810982.217418	44.078183
3501.697904	810966.745037	44.083188
3501.993622	810944.989333	44.088193
3501.909794	810926.040085	44.093197
3501.817536	810913.021200	44.098202
3501.760884	810891.666369	44.103207
3501.807520	810870.196455	44.108212
3501.757566	810861.335547	44.113217
3501.717990	810845.710824	44.118221
3501.797112	810822.422383	44.123226
3501.798145	810808.309912	44.128231
3501.866024	810783.651162	44.133236
3502.000457	810772.995725	44.138241
3501.869850	810763.020945	44.143245
3501.510851	810740.882419	44.148250
3501.797601	810719.519482	44.153255
3501.792869	810724.567390	44.158260
3501.799573	810689.971050	44.163265
3501.906595	810668.882568	44.168269
3501.393990	810662.498703	44.173274
3501.994329	810627.167235	44.178279
3501.844871	810630.768982	44.183284
3501.683103	810597.473980	44.188289
3502.235230	810579.154047	44.193293
3501.930974	810561.220141	44.198298
3501.901313	810550.934405	44.203303
3501.509899	810527.085420	44.208308
3502.163947	810515.608945	44.213313
3501.992742	810492.213596	44.218317
3501.875349	810471.504491	44.223322
3501.989753	810459.430763	44.228327
3501.599666	810427.054596	44.233332
3502.030713	810412.674457	44.238337
3502.024206	810399.885483	44.243341
3501.741503	810380.085398	44.248346
3501.917544	810377.900186	44.253351
3501.473868	810350.971933	44.258356
3502.134913	810329.056076	44.263361
3501.861442	810329.150090	44.268365
3501.680788	810304.922577	44.273370
3501.964522	810275.423976	44.278375
3501.771867	810263.351474	44.283380
3501.933024	810244.948030	44.288385
3501.788273	810232.622558	44.293389
3501.720756	810214.697745	44.298394
3502.034943	810195.582887	44.303399
3501.523771	810188.169222	44.308404
3501.652315	810175.357580	44.313409
3501.766970	810155.736416	44.318413
3501.600707	810141.307076	44.323418
3502.128565	810128.968636	44.328423
3501.778798	810098.544495	44.333428
3501.784772	810081.832378	44.338433
3502.060006	810055.274596	44.343437
3501.811138	810043.014935	44.348442
3501.938580	810027.801879	44.353447
3501.675121	810004.420046	44.358452
3501.592787	809981.253332	44.363457
3501.907589	809978.310032	44.368461
3501.358685	809954.926039	44.373466
3501.974560	809943.454895	44.378471
3501.720327	809925.805112	44.383476
3501.527870	809912.457762	44.388481
3501.574899	809894.464230	44.393485
3501.409099	809886.013191	44.398490
3501.675909	809879.059129	44.403495
3501.407102	809870.134961	44.408500
3501.346118	809837.750781	44.413505
3501.532029	809823.703829	44.418509
3501.367852	809821.427456	44.423514
3501.373641	809823.729847	44.428519
3501.482009	809807.931344	44.433524
3501.549514	809770.967919	44.438529
3501.884075	809770.177648	44.443533
3501.813921	809766.023448	44.448538
3501.573541	809740.578548	44.453543
3501.485358	809723.341965	44.458548
3501.254703	809730.241150	44.463553
3501.660584	809723.852127	44.468557
3501.665922	809702.238303	44.473562
3501.701954	809689.342968	44.478567
3501.378962	809658.912446	44.483572
3501.589028	809659.907003	44.488577
3501.739451	809637.239879	44.493581
3501.258947	809618.548361	44.498586
3501.309394	809618.834073	44.503591
3501.499314	809611.745376	44.508596
3501.935223	809601.724583	44.513601
3501.589444	809578.942960	44.518605
3501.453933	809582.101874	44.523610
3501.639964	809561.683085	44.528615
3501.569197	809545.913482	44.533620
3501.647541	809526.737578	44.538625
3501.870975	809531.748787	44.543629
3501.539933	809511.071947	44.548634
3501.743386	809472.565190	44.553639
3501.706755	809481.148036	44.558644
3501.896073	809468.129012	44.563649
3502.113827	809441.186221	44.568653
3501.798435	809428.887398	44.573658
3501.961305	809392.249286	44.578663
3501.869517	809387.804351	44.583668
3501.702283	809387.390761	44.588673
3502.019858	809356.461283	44.593677
3501.574291	809336.635970	44.598682
3502.102695	809330.961574	44.603687
3501.569954	809308.013793	44.608692
3501.856859	809290.812354	44.613697
3501.715270	809278.582654	44.618701
3501.462995	809255.686522	44.623706
3501.836936	809246.704673	44.628711
3501.667589	809232.224899	44.633716
3501.876480	809211.703272	44.638721
3501.983173	809195.511527	44.643725
3501.324336	809190.620728	44.648730
3501.886142	809170.825048	44.653735
3501.458046	809158.250222	44.658740
3502.062499	809136.879009	44.663745
3502.284302	809112.433915	44.668749
3501.927809	809103.278115	44.673754
3501.920167	809078.037466	44.678759
3501.361485	809059.210244	44.683764
3502.036031	809044.198957	44.688769
3501.664245	809031.663634	44.693773
3501.449783	808994.154275	44.698778
3501.902079	808989.276360	44.703783
3501.514079	808998.701917	44.708788
3501.691670	808978.527843	44.713793
3501.919064	808943.004014	44.718797
3501.615467	808943.299059	44.723802
3501.879614	808923.600709	44.728807
3501.609696	808916.685065	44.733812
3501.654799	808889.719520	44.738817
3501.630562	808877.567798	44.743821
3501.426353	808854.172249	44.748826
3501.581984	808841.206594	44.753831
3501.546036	808841.261495	44.758836
3501.689119	808828.739019	44.763841
3501.748080	808791.526613	44.768845
3501.756025	808795.936662	44.773850
3501.844672	808787.050220	44.778855
3501.692326	808767.174946	44.783860
3501.593960	808766.995050	44.788865
3501.591335	808755.329707	44.793869
3501.645970	808741.939358	44.798874
3501.964499	808702.723078	44.803879
3501.723217	808689.724483	44.808884
3501.664999	808679.538654	44.813889
3501.616620	808652.979702	44.818893
3501.469369	808650.308014	44.823898
3501.716820	808634.728967	44.828903
3501.763847	808624.721788	44.833908
3501.791148	808595.895379	44.838913
3501.746170	808611.097974	44.843917
3501.714721	808587.231900	44.848922
3501.710910	808555.861565	44.853927
3501.536313	808559.762645	44.858932
3501.725466	808532.820979	44.863937
3501.945908	808511.413033	44.868941
3501.700256	808511.551496	44.873946
3501.692713	808496.749400	44.878951
3501.861943	808469.369607	44.883956
3501.913903	808455.145834	44.888961
3501.922308	808439.311610	44.893965
3501.777769	808419.336000	44.898970
3502.013673	808393.072337	44.903975
3501.810154	808379.380671	44.908980
3501.562640	808369.960837	44.913985
3501.775524	808343.063533	44.918989
3501.844521	808337.071846	44.923994
3501.842322	808311.729428	44.928999
3501.840407	808299.965152	44.934004
3501.685044	808283.520295	44.939009
3501.705908	808263.958157	44.944013
3501.737732	808264.443072	44.949018
3501.588520	808231.673638	44.954023
3501.560966	808217.707565	44.959028
3501.750962	808199.587972	44.964033
3501.463598	808196.301926	44.969037
3501.327914	808173.333930	44.974042
3501.422686	808166.406470	44.979047
3501.260377	808161.139009	44.984052
3501.640630	808151.223307	44.989057
3501.833409	808155.603324	44.994061
3501.383201	808135.971353	44.999066
3501.742200	808108.901999	45.004071
3501.538951	808111.092339	45.009076
3501.393894	808097.439497	45.014081
3501.631005	808075.047030	45.019085
3501.617402	808069.264797	45.024090
3501.713101	808061.258622	45.029095
3501.403898	808037.632461	45.034100
3501.756313	808012.230520	45.039105
3501.462631	808011.837669	45.044109
3501.353353	808006.365269	45.049114
3501.700262	807986.209397	45.054119
3501.385377	807980.966929	45.059124
3501.259205	807970.791235	45.064129
3501.532879	807967.118537	45.069133
3501.379370	807959.104270	45.074138
3501.820003	807936.383697	45.079143
3501.430367	807915.221441	45.084148
3501.576333	807902.402664	45.089153
3501.513658	807906.138614	45.094157
3501.346494	807898.126525	45.099162
3501.772380	807867.613665	45.104167
3501.418728	807869.142546	45.109172
3501.562579	807859.853629	45.114177
3501.478758	807830.306960	45.119181
3501.243680	807818.335149	45.124186
3501.672806	807801.645787	45.129191
3501.528872	807822.455010	45.134196
3501.528054	807805.934523	45.139201
3501.652043	807781.941986	45.144205
3501.508778	807775.837703	45.149210
3501.673067	807752.034514	45.154215
3501.480871	807744.320505	45.159220
3501.558527	807715.923296	45.164225
3501.498111	807708.579725	45.169229
3501.541213	807719.504769	45.174234
3501.808803	807704.851731	45.179239
3501.923066	807678.654385	45.184244
3501.586247	807667.385396	45.189249
3501.216483	807662.053673	45.194253
3501.367881	807648.007935	45.199258
3501.554893	807617.141117	45.204263
3501.607365	807620.711183	45.209268
3501.743115	807603.334305	45.214273
3501.622046	807600.903010	45.219277
3501.283275	807587.869346	45.224282
3501.306978	807568.402797	45.229287
3501.232315	807571.895782	45.234292
3501.309048	807568.353360	45.239297
3501.546172	807555.715016	45.244301
3501.500358	807543.025204	45.249306
3501.514966	807497.920116	45.254311
3501.368299	807514.073372	45.259316
3501.566460	807499.872553	45.264321
3501.438591	807478.910949	45.269325
3501.351500	807470.934193	45.274330
3501.726437	807468.421149	45.279335
3501.499287	807455.025669	45.284340
3501.203214	807447.181359	45.289345
3501.422927	807420.034175	45.294349
3501.072802	807417.689570	45.299354
3501.641583	807414.360171	45.304359
3501.666009	807419.699875	45.309364
3501.515503	807410.556886	45.314369
3501.832754	807377.510417	45.319373
3501.506719	807377.269932	45.324378
3501.791341	807367.270801	45.329383
3501.669242	807333.168895	45.334388
3501.537376	807326.572073	45.339393
3502.207778	807308.223911	45.344397
3501.500622	807294.613025	45.349402
3501.425090	807266.190156	45.354407
3501.328953	807275.177788	45.359412
3501.381219	807274.335695	45.364417
3501.401641	807261.634451	45.369421
3501.419169	807244.031002	45.374426
3501.324776	807227.083291	45.379431
3501.613153	807236.154718	45.384436
3501.460981	807221.716870	45.389441
3501.197178	807223.133036	45.394445
3501.253433	807207.288077	45.399450
3501.846075	807203.317298	45.404455
3501.594587	807187.375903	45.409460
3501.583320	807190.760586	45.414465
3501.328014	807160.405810	45.419469
3501.045226	807149.862472	45.424474
3501.522207	807144.881139	45.429479
3501.328610	807144.177583	45.434484
3501.237583	807141.839229	45.439489
3501.367033	807144.269237	45.444493
3501.377536	807133.726591	45.449498
3501.479399	807094.389699	45.454503
3501.348203	807086.125593	45.459508
3501.298937	807084.368674	45.464513
3501.315579	807079.512149	45.469517
3501.438157	807087.630528	45.474522
3501.512695	807064.771260	45.479527
3501.235187	807043.783942	45.484532
3501.271693	807031.471846	45.489537
3501.424587	807032.427188	45.494541
3501.384050	807031.453267	45.499546
3501.316832	807017.638359	45.504551
3501.374678	806996.938856	45.509556
3501.306514	806993.027778	45.514561
3501.508562	806981.080550	45.519565
3501.039275	806975.862737	45.524570
3501.046946	806977.430350	45.529575
3501.798762	806975.002136	45.534580
3501.002017	806957.532076	45.539585
3501.421688	806932.360199	45.544589
3501.311415	806935.074912	45.549594
3501.334776	806925.412346	45.554599
3501.366912	806925.259930	45.559604
3501.252001	806914.639547	45.564609
3501.590044	806897.815906	45.569613
3501.092589	806891.131794	45.574618
3501.478558	806877.928364	45.579623
3501.444961	806889.896981	45.584628
3501.284063	806878.744797	45.589633
3501.651526	806871.427906	45.594637
3501.637435	806847.650956	45.599642
3501.460516	806836.501342	45.604647
3501.378448	806828.572038	45.609652
3501.450149	806829.883990	45.614657
3501.488545	806799.234085	45.619661
3501.500546	806787.562975	45.624666
3501.389694	806774.048942	45.629671
3501.436813	806781.493695	45.634676
3501.270846	806772.646578	45.639681
3501.656596	806737.134240	45.644685
3501.273597	806736.216687	45.649690
3501.395354	806726.194421	45.654695
3501.275093	806723.027223	45.659700
3500.946659	806724.307045	45.664705
3501.374058	806720.167091	45.669709
3501.123685	806697.163994	45.674714
3501.392615	806674.124312	45.679719
3501.340720	806679.771349	45.684724
3501.352972	806676.190058	45.689729
3501.795928	806668.517302	45.694733
3501.367794	806656.330098	45.699738
3501.442157	806640.088598	45.704743
3501.462872	806631.504733	45.709748
3501.468990	806629.885667	45.714753
3501.378956	806630.930112	45.719757
3501.413667	806608.958442	45.724762
3501.360987	806585.334032	45.729767
3501.540643	806581.087709	45.734772
3501.271704	806590.447921	45.739777
3501.310687	806586.764117	45.744781
3501.288977	806575.833668	45.749786
3501.295315	806542.932454	45.754791
3501.007576	806545.431394	45.759796
3501.200124	806535.985569	45.764801
3501.390669	806518.498851	45.769805
3501.327226	806534.150389	45.774810
3501.649580	806493.695033	45.779815
3501.414926	806431.560833	45.784820
3501.128741	806314.419471	45.789825
3501.233072	806128.808888	45.794829
3500.740336	805903.376291	45.799834
3501.115311	805594.232439	45.804839
3501.100089	805259.735870	45.809844
3500.719768	804851.276621	45.814849
3500.516858	804378.610627	45.819853
3500.403761	803866.951239	45.824858
3500.096171	803287.541524	45.829863
3499.774793	802647.742670	45.834868
3498.992186	801958.454895	45.839873
3498.684375	801193.698706	45.844877
3498.272590	800393.295755	45.849882
3498.125772	799530.571020	45.854887
3497.800064	798602.040310	45.859892
3497.329107	797618.472907	45.864897
3496.955543	796573.029782	45.869901
3496.233934	795453.233899	45.874906
3495.839743	794276.179356	45.879911
3495.289194	793045.454781	45.884916
3494.047103	791753.308229	45.889921
3493.734978	790410.742960	45.894925
3492.940044	789014.473940	45.899930
3492.255284	787531.432222	45.904935
3491.674139	786005.922282	45.909940
3490.751579	784415.611681	45.914945
3490.240839	782756.595556	45.919949
3489.041186	781053.909264	45.924954
3488.347381	779282.076229	45.929959
3487.682994	777442.406280	45.934964
3486.718390	775544.605971	45.939969
3485.922010	773606.288551	45.944973
3484.691359	771576.329179	45.949978
3483.998878	769501.021619	45.954983
3483.028170	767374.844992	45.959988
3481.659665	765183.230578	45.964993
3480.958101	762942.819754	45.969997
3479.634763	760629.951404	45.975002
3478.411872	758259.893831	45.980007
3477.200399	755853.054182	45.985012
3475.779563	753371.357647	45.990017
3474.780031	750832.419655	45.995021
3473.635483	748258.572826	46.000026
3472.053604	745610.728396	46.005031
3470.700780	742909.182976	46.010036
3469.285748	740161.604243	46.015041
3468.082970	737345.386669	46.020045
3466.444993	734476.909712	46.025050
3465.117432	731566.105635	46.030055
3463.673310	728597.201765	46.035060
3462.146368	725575.093633	46.040065
3460.765057	722505.990417	46.045069
3459.192058	719378.992145	46.050074
3457.413666	716190.621572	46.055079
3456.040296	712954.617097	46.060084
3454.047523	709674.182132	46.065089
3452.499531	706333.402873	46.070093
3450.800281	702943.202251	46.075098
3449.101963	699500.426709	46.080103
3447.353060	696015.579043	46.085108
3445.626054	692471.146149	46.090113
3443.823436	688863.154164	46.095117
3441.920122	685230.434978	46.100122
3440.301138	681540.629543	46.105127
3438.176935	677791.820598	46.110132
3436.171044	674000.152082	46.115137
3434.399768	670145.817982	46.120141
3432.345071	666252.295132	46.125146
3430.064402	662329.576608	46.130151
3428.383311	658356.634813	46.135156
3426.440612	654327.923462	46.140161
3424.460671	650235.859515	46.145165
3422.462322	646114.080520	46.150170
3420.139725	641944.764005	46.155175
3418.090586	637714.613743	46.160180
3415.796488	633447.340281	46.165185
3413.790039	629125.054200	46.170189
3411.658243	624773.681010	46.175194
3409.335475	620364.450285	46.180199
3407.327165	615903.500075	46.185204
3404.980211	611400.179933	46.190209
3402.504201	606859.949499	46.195213
3399.986829	602280.767962	46.200218
3397.762977	597643.827754	46.205223
3395.266333	592962.444525	46.210228
3392.612438	588264.469468	46.215233
3390.703816	583507.024689	46.220237
3387.985238	578717.689569	46.225242
3385.569641	573894.462136	46.230247
3382.921523	569014.669351	46.235252
3380.322214	564096.813498	46.240257
3377.822397	559140.875246	46.245261
3375.095814	554145.890503	46.250266
3372.670241	549119.626832	46.255271
3370.146237	544027.250929	46.260276
3367.500565	538939.611809	46.265281
3364.815521	533770.739057	46.270285
3362.137109	528588.528616	46.275290
3359.033361	523356.813326	46.280295
3356.543379	518105.821483	46.285300
3353.666376	512804.706591	46.290305
3350.774243	507477.560621	46.295309
3347.980197	502125.693454	46.300314
3344.910637	496722.978600	46.305319
3342.137155	491283.685087	46.310324
3339.149441	485838.275207	46.315329
3336.530974	480331.396941	46.320333
3333.428392	474798.125683	46.325338
3330.353476	469241.335557	46.330343
3327.321976	463647.567110	46.335348
3324.268307	458036.208746	46.340353
3321.570758	452387.757504	46.345357
3318.291880	446712.273827	46.350362
3315.087102	441006.174070	46.355367
3312.369621	435263.628569	46.360372
3308.584189	429501.867112	46.365377
3305.604269	423711.705000	46.370381
3302.444182	417895.364691	46.375386
3299.133263	412063.031308	46.380391
3296.336800	406203.051118	46.385396
3292.678765	400315.835949	46.390401
3289.669774	394409.582329	46.395405
3286.348256	388484.234640	46.400410
3282.634931	382529.500193	46.405415
3279.798574	376550.189775	46.410420
3276.213021	370563.243031	46.415425
3272.976380	364550.749732	46.420429
3269.507766	358513.559572	46.425434
3265.893956	352442.237181	46.430439
3262.697064	346362.328510	46.435444
3258.891470	340276.599420	46.440449
3255.891842	334152.699738	46.445453
3252.258876	328031.610861	46.450458
3248.476745	321893.199660	46.455463
3245.059350	315727.071506	46.460468
3241.016923	309564.654507	46.465473
3237.572516	303374.435583	46.470477
3233.978011	297184.244245	46.475482
3230.365869	290978.531960	46.480487
3226.672535	284766.074807	46.485492
3222.948768	278548.246519	46.490497
3219.041070	272311.963785	46.495501
3215.428774	266067.469298	46.500506
3211.510723	259820.753543	46.505511
3208.116301	253565.958122	46.510516
3204.003345	247301.896008	46.515521
3200.196796	241031.412984	46.520525
3196.409922	234762.944516	46.525530
3192.439969	228497.067876	46.530535
3188.481843	222217.361175	46.535540
3184.701905	215953.039481	46.540545
3180.750029	209573.186206	46.545549
3176.668949	203287.378831	46.550554
3172.301400	197008.201774	46.555559
3168.346426	190731.042620	46.560564
3164.014805	184469.134875	46.565569
3160.232359	178206.832909	46.570573
3155.905917	171958.944125	46.575578
3151.709645	165711.852121	46.580583
3147.391534	159468.685177	46.585588
3142.873271	153239.751177	46.590593
3138.750046	147017.007814	46.595597
3134.110565	140812.776267	46.600602
3129.833978	134626.414582	46.605607
3125.229852	128447.335160	46.610612
3120.412166	122295.278370	46.615617
3115.512190	116155.885687	46.620621
3110.720090	110050.573289	46.625626
3106.035762	103973.148125	46.630631
3101.198486	97906.294423	46.635636
3096.281207	91880.847240	46.640641
3091.078830	85901.337087	46.645645
3085.402019	79946.937419	46.650650
3079.712166	74035.814602	46.655655
3073.656671	68183.389454	46.660660
3066.258659	62420.494718	46.665665
3054.506660	56854.671562	46.670669
3036.718300	51545.131586	46.675674
3019.536993	46436.996796	46.680679
3003.099679	41534.469161	46.685684
2987.101731	36917.090638	46.690689
2971.732270	32566.586291	46.695693
2957.851852	28495.208820	46.700698
2944.130580	24699.802352	46.705703
2930.966067	21166.672970	46.710708
2918.129278	17911.102850	46.715713
2906.422981	14905.274950	46.720717
2894.323675	12147.998180	46.725722
2882.743479	9636.533616	46.730727
2871.475469	7360.424088	46.735732
2858.647491	5365.585036	46.740737
2842.103610	3698.783916	46.745741
2823.926964	2362.832778	46.750746
2807.501484	1281.567050	46.755751
2792.679719	474.642581	46.760756
2767.613626	246.701133	46.765761
2747.712998	260.560057	46.770765
2742.165551	260.356830	46.775770
2746.441107	259.110730	46.780775
2753.851618	263.191058	46.785780
2760.393130	262.693920	46.790785
2765.094540	245.863660	46.795789
2766.621846	252.927198	46.800794
2765.291980	259.834918	46.805799
2762.836540	247.681874	46.810804
2759.270373	246.795528	46.815809
2755.956299	242.142943	46.820813
2752.793428	241.255520	46.825818
2749.516675	248.514115	46.830823
2747.224223	238.833743	46.835828
2744.388527	243.004501	46.840833
2741.774052	248.777317	46.845837
2738.751459	225.383953	46.850842
2735.831730	239.321700	46.855847
2733.167950	240.617704	46.860852
2729.690472	249.238634	46.865857
2726.418190	246.129205	46.870861
2723.164880	239.074925	46.875866
2719.962292	236.957965	46.880871
2717.181275	237.292533	46.885876
2713.717333	237.099502	46.890881
2710.549132	230.608060	46.895885
2707.452316	231.466783	46.900890
2704.072696	242.021579	46.905895
2701.002567	228.492014	46.910900
2697.620150	233.674302	46.915905
2694.058477	232.192431	46.920909
2690.735965	233.019411	46.925914
2687.187384	244.696693	46.930919
2684.257261	228.649657	46.935924
2680.902438	244.648321	46.940929
2677.560863	232.132650	46.945933
2674.435641	230.357140	46.950938
2670.307607	220.918689	46.955943
2667.362874	228.463722	46.960948
2663.873450	227.118238	46.965953
2660.450282	224.708648	46.970957
2657.468520	220.666385	46.975962
2653.566113	218.952435	46.980967
2650.107308	220.811184	46.985972
2646.730433	228.575761	46.990977
2643.546555	222.942607	46.995981
2640.632890	219.834176	47.000986
2637.409626	221.881995	47.005991
2633.586342	228.149632	47.010996
2629.760782	226.219490	47.016001
2626.429097	224.731597	47.021005
2622.863404	217.495952	47.026010
2619.307190	229.959039	47.031015
2616.004008	211.683305	47.036020
2612.487693	228.933645	47.041025
2609.736434	213.693801	47.046029
2605.916497	215.468270	47.051034
2602.266587	229.919988	47.056039
2599.021984	217.367173	47.061044
2595.351543	223.641390	47.066049
2592.255346	215.105175	47.071053
2588.927323	215.030773	47.076058
2585.532501	200.337584	47.081063
2582.062378	215.482325	47.086068
2578.192994	217.742272	47.091073
2574.859304	217.864845	47.096077
2571.480658	216.639952	47.101082
2567.444873	213.759599	47.106087
2564.410951	207.191931	47.111092
2560.934685	227.874724	47.116097
2557.804879	214.477132	47.121101
2554.178857	215.742931	47.126106
2550.687289	214.722640	47.131111
2547.275105	210.022708	47.136116
2543.985636	219.833687	47.141121
2540.333675	220.080877	47.146125
2536.865825	206.549917	47.151130
2533.623878	216.842506	47.156135
2530.256905	213.655852	47.161140
2526.267739	217.018651	47.166145
2522.508285	214.298064	47.171149
2519.495230	213.432011	47.176154
2515.371893	217.612820	47.181159
2512.490229	212.177234	47.186164
2508.721773	207.462868	47.191169
2505.675154	217.511239	47.196173
2502.119206	219.613084	47.201178
2498.548250	223.511810	47.206183
2495.023941	207.514443	47.211188
2491.545107	217.613078	47.216193
2488.302002	206.662994	47.221197
2484.729428	212.324822	47.226202
2480.600336	205.616856	47.231207
2477.742763	204.068016	47.236212
2474.013093	206.591083	47.241217
2470.571389	200.999156	47.246221
2467.391399	196.907389	47.251226
2463.729297	208.508038	47.256231
2460.228694	199.245668	47.261236
2456.808686	202.367835	47.266241
2453.442954	193.543177	47.271245
2449.849780	199.128203	47.276250
2446.551053	203.755931	47.281255
2443.290556	194.851868	47.286260
2439.288795	202.005269	47.291265
2435.954711	203.082291	47.296269
2432.259652	206.337437	47.301274
2428.686243	199.742289	47.306279
2425.457558	203.410366	47.311284
2422.043261	206.788711	47.316289
2418.297526	203.820653	47.321293
2415.265130	196.876032	47.326298
2411.431276	198.112634	47.331303
2408.104668	185.516156	47.336308
2404.432367	191.081689	47.341313
2400.758251	189.877783	47.346317
2397.643744	187.903610	47.351322
2393.969155	193.476925	47.356327
2390.139724	181.174021	47.361332
2387.017246	188.873927	47.366337
2383.475094	187.312630	47.371341
2380.140923	191.858519	47.376346
2376.395226	204.930956	47.381351
2373.517431	196.369004	47.386356
2369.692344	199.969912	47.391361
2365.883581	196.288322	47.396365
2362.255224	188.905216	47.401370
2359.129864	201.858480	47.406375
2356.001352	194.379521	47.411380
2352.466759	193.063342	47.416385
2348.867641	199.428692	47.421389
2345.483214	192.446860	47.426394
2341.366666	197.231012	47.431399
2337.943401	187.513776	47.436404
2334.682296	191.753335	47.441409
2331.076165	186.305809	47.446413
2327.844287	187.631807	47.451418
2323.922090	205.398431	47.456423
2320.553849	186.067738	47.461428
2316.869462	197.093970	47.466433
2313.788886	197.249794	47.471437
2310.397773	182.320976	47.476442
2306.593081	191.516220	47.481447
2303.662796	184.824252	47.486452
2299.657279	182.923871	47.491457
2295.850348	191.782966	47.496461
2292.873908	185.179317	47.501466
2289.316671	191.571227	47.506471
2285.919733	192.903155	47.511476
2282.379181	189.543695	47.516481
2278.500579	187.787152	47.521485
2275.130272	182.534287	47.526490
2271.945969	193.347824	47.531495
2268.333570	178.230987	47.536500
2265.089858	191.380584	47.541505
2261.147183	186.916780	47.546509
2257.496448	185.708695	47.551514
2253.943902	193.566499	47.556519
2250.632134	188.859731	47.561524
2247.109363	194.308721	47.566529
2243.849561	181.415706	47.571533
2240.515257	181.843185	47.576538
2236.792439	191.114338	47.581543
2233.427963	187.551138	47.586548
2229.895222	181.559205	47.591553
2226.485131	195.566862	47.596557
2223.042037	190.798204	47.601562
2219.307774	192.273112	47.606567
2215.613455	181.665871	47.611572
2212.349261	181.479785	47.616577
2208.891942	187.535692	47.621581
2205.588163	181.662182	47.626586
2201.777006	183.943486	47.631591
2198.263459	173.130339	47.636596
2194.742789	184.184753	47.641601
2191.253184	188.583504	47.646605
2188.198414	178.541470	47.651610
2184.216303	182.706739	47.656615
2180.792115	184.357040	47.661620
2177.292227	175.784347	47.666625
2174.140433	180.205027	47.671629
2170.609266	170.444329	47.676634
2166.369173	179.388830	47.681639
2163.315813	173.530768	47.686644
2159.627641	177.570216	47.691649
2156.458593	168.473158	47.696653
2153.036441	165.811978	47.701658
2149.233995	172.848467	47.706663
2145.891597	166.364751	47.711668
2142.139629	177.220355	47.716673
2138.674877	173.186178	47.721677
2135.294642	178.764717	47.726682
2131.690024	184.007343	47.731687
2128.460482	191.106411	47.736692
2124.977170	178.174962	47.741697
2121.708207	180.800372	47.746701
2118.541563	178.577227	47.751706
2114.514297	180.596472	47.756711
2110.627585	177.041145	47.761716
2107.342910	179.311616	47.766721
2103.614433	180.891091	47.771725
2100.467520	176.259122	47.776730
2096.851490	181.656368	47.781735
2093.434011	173.292900	47.786740
2089.968769	170.643494	47.791745
2086.137690	173.477862	47.796749
2082.565786	165.777110	47.801754
2079.248922	166.397520	47.806759
2076.096817	162.512771	47.811764
2072.509556	169.190592	47.816769
2068.741843	165.525391	47.821773
2065.548432	167.937294	47.826778
2061.888119	165.473298	47.831783
2058.378468	162.792167	47.836788
2054.314457	168.139412	47.841793
2051.066808	179.285280	47.846797
2048.087635	171.175007	47.851802
2044.520766	178.460369	47.856807
2041.000332	175.057466	47.861812
2037.665274	164.944453	47.866817
2033.581296	173.443866	47.871821
2030.232846	171.700634	47.876826
2026.949475	166.704180	47.881831
2023.378411	166.429004	47.886836
2019.732222	164.526233	47.891841
2016.043642	175.629616	47.896845
2012.944385	167.535621	47.901850
2009.354615	170.357250	47.906855
2006.028389	163.863246	47.911860
2002.443170	162.736039	47.916865
1998.835310	167.376059	47.921869
1995.501949	158.851678	47.926874
1991.367603	180.164121	47.931879
1988.083931	170.124639	47.936884
1985.006289	165.379388	47.941889
1981.414069	154.180588	47.946893
1978.139291	150.639033	47.951898
1974.074331	163.656123	47.956903
1970.883694	157.182491	47.961908
1967.162606	158.705465	47.966913
1963.758733	164.372517	47.971917
1960.343522	157.429430	47.976922
1957.144247	175.889426	47.981927
1953.452597	165.904250	47.986932
1949.821419	168.929856	47.991937
1946.134402	169.712122	47.996941
1943.291157	162.956842	48.001946
1939.110365	165.785834	48.006951
1935.417850	159.684183	48.011956
1932.227976	170.287701	48.016961
1928.771148	159.645615	48.021965
1925.635135	158.167307	48.026970
1921.858662	163.590994	48.031975
1918.401022	165.113840	48.036980
1914.773148	165.650177	48.041985
1911.282734	172.176731	48.046989
1908.050185	159.775091	48.051994
1904.468995	165.355695	48.056999
1901.007380	161.245457	48.062004
1897.733575	162.428296	48.067009
1893.421468	154.549070	48.072013
1890.281463	160.091224	48.077018
1886.628377	166.267850	48.082023
1883.447574	166.083840	48.087028
1880.002547	164.266343	48.092033
1876.428867	158.345988	48.097037
1873.090220	155.707871	48.102042
1868.990075	176.135273	48.107047
1865.431773	168.504222	48.112052
1862.467014	159.504441	48.117057
1858.555278	175.261486	48.122061
1855.510235	167.468609	48.127066
1851.952741	165.459738	48.132071
1848.457870	169.068561	48.137076
1844.888309	174.763791	48.142081
1841.293749	162.573552	48.147085
1838.053583	161.449284	48.152090
1834.191638	161.738075	48.157095
1830.644841	164.366825	48.162100
1827.358324	156.563001	48.167105
1823.778911	165.424303	48.172109
1820.336641	168.810670	48.177114
1816.543573	166.259394	48.182119
1813.357712	153.722151	48.187124
1809.714137	161.537718	48.192129
1806.110200	160.518769	48.197133
1803.169623	157.659128	48.202138
1799.360451	159.372626	48.207143
1795.901785	152.332914	48.212148
1792.473662	151.432655	48.217153
1788.840538	157.013194	48.222157
1785.365160	157.655155	48.227162
1781.567400	163.736026	48.232167
1777.899951	162.427652	48.237172
1774.588123	157.098812	48.242177
1771.408773	162.305852	48.247181
1768.222201	162.364261	48.252186
1764.069429	164.994568	48.257191
1760.540241	166.055835	48.262196
1757.279604	153.902014	48.267201
1753.377208	160.500947	48.272205
1750.278067	158.688203	48.277210
1746.934300	154.811954	48.282215
1743.445256	151.483156	48.287220
1740.154787	146.702308	48.292225
1736.133131	158.679210	48.297229
1732.768874	146.342824	48.302234
1729.057685	160.927220	48.307239
1725.463093	146.599165	48.312244
1722.271740	156.430401	48.317249
1718.696036	167.111069	48.322253
1715.012279	153.284405	48.327258
1711.847614	155.461641	48.332263
1708.388483	153.381565	48.337268
1704.682408	149.719916	48.342273
1700.806707	149.627074	48.347277
1697.558873	139.677561	48.352282
1694.411662	158.432283	48.357287
1690.923188	150.244245	48.362292
1687.494043	153.779151	48.367297
1683.747926	159.081819	48.372301
1680.207877	150.206861	48.377306
1676.424657	168.603549	48.382311
1673.190932	151.784957	48.387316
1669.570216	146.174770	48.392321
1666.040395	152.873863	48.397325
1662.870032	152.050902	48.402330
1659.166210	152.279954	48.407335
1655.689332	140.356044	48.412340
1652.080521	145.635177	48.417345
1648.579404	154.079820	48.422349
1645.343066	139.414986	48.427354
1641.775805	152.663514	48.432359
1638.009926	148.351064	48.437364
1634.901432	143.239437	48.442369
1631.172743	144.716773	48.447373
1627.641711	136.950853	48.452378
1623.841750	152.728389	48.457383
1620.255007	147.016630	48.462388
1616.942983	152.208131	48.467393
1613.287553	152.685829	48.472397
1610.099448	145.917181	48.477402
1606.338566	159.250460	48.482407
1603.214143	150.892096	48.487412
1600.176477	152.186354	48.492417
1596.542536	152.223166	48.497421
1593.026851	147.814501	48.502426
1589.297860	133.311315	48.507431
1585.660765	141.037008	48.512436
1582.013266	144.218593	48.517441
1578.410885	147.002546	48.522445
1574.798787	147.575419	48.527450
1571.485335	159.669436	48.532455
1567.929890	158.138074	48.537460
1564.865168	148.126940	48.542465
1561.003861	159.128077	48.547469
1557.397041	146.936405	48.552474
1553.892677	144.312971	48.557479
1550.377716	149.250996	48.562484
1547.178124	153.562300	48.567489
1543.782301	143.514268	48.572493
1540.677493	137.327112	48.577498
1536.947647	137.202792	48.582503
1533.150019	138.473227	48.587508
1529.859402	134.342372	48.592513
1525.840345	145.141651	48.597517
1522.420542	141.993334	48.602522
1518.977072	144.748227	48.607527
1515.536989	139.420176	48.612532
1511.946428	131.642347	48.617537
1508.250561	148.208968	48.622541
1504.837382	145.663348	48.627546
1501.517893	142.684257	48.632551
1497.943810	143.235012	48.637556
1494.659163	144.631242	48.642561
1491.010122	153.947432	48.647565
1487.629951	131.864139	48.652570
1484.078192	143.044081	48.657575
1480.798566	133.284628	48.662580
1477.049776	140.716158	48.667585
1473.142279	140.963630	48.672589
1470.085091	140.665977	48.677594
1466.911057	132.227981	48.682599
1463.258307	137.105713	48.687604
1459.676265	135.544172	48.692609
1455.827421	142.458096	48.697613
1452.284004	129.031707	48.702618
1448.743581	145.237947	48.707623
1445.418993	142.343486	48.712628
1442.301862	142.184092	48.717633
1438.506368	133.900672	48.722637
1435.295237	136.908196	48.727642
1431.376144	150.984195	48.732647
1428.129389	142.462421	48.737652
1424.531819	139.644893	48.742657
1420.463779	135.275500	48.747661
1417.390236	128.853281	48.752666
1414.073094	127.459367	48.757671
1410.471441	138.169380	48.762676
1406.959876	114.729026	48.767681
1403.309506	127.678003	48.772685
1400.031673	127.035589	48.777690
1396.276485	126.198686	48.782695
1393.107255	124.543198	48.787700
1389.872998	127.867398	48.792705
1386.029349	134.354001	48.797709
1382.732419	133.424498	48.802714
1379.131402	131.451871	48.807719
1375.455644	138.291290	48.812724
1371.906940	143.036563	48.817729
1368.405648	142.376488	48.822733
1365.037702	129.271229	48.827738
1361.296812	138.410737	48.832743
1357.994274	138.169219	48.837748
1354.449008	134.706365	48.842753
1350.706448	142.220487	48.847757
1347.475059	126.643739	48.852762
1343.867492	141.471314	48.857767
1340.041516	135.384355	48.862772
1336.987772	134.330580	48.867777
1333.319567	140.049015	48.872781
1330.156703	129.663244	48.877786
1326.590790	130.240262	48.882791
1323.062120	139.839029	48.887796
1319.388497	128.681723	48.892801
1315.868595	131.956718	48.897805
1312.610107	124.379424	48.902810
1308.950572	126.562845	48.907815
1305.109053	130.250733	48.912820
1301.977012	120.168002	48.917825
1298.057424	132.738915	48.922829
1294.551441	122.636224	48.927834
1291.142620	127.705120	48.932839
1287.158683	132.684168	48.937844
1284.823435	129.433018	48.942849
1281.267336	131.783078	48.947853
1277.860455	132.056151	48.952858
1274.027057	120.459200	48.957863
1270.343312	123.308228	48.962868
1266.777366	123.208300	48.967873
1263.330115	122.323795	48.972877
1259.925500	122.742614	48.977882
1256.301874	120.968536	48.982887
1252.620484	129.158363	48.987892
1249.370747	130.647993	48.992897
1245.717987	137.081746	48.997901
1242.376114	120.942516	49.002906
1238.733887	135.548244	49.007911
1235.515327	126.774698	49.012916
1232.073069	130.008995	49.017921
1228.369519	129.061155	49.022925
1224.738267	131.970701	49.027930
1221.227494	129.588340	49.032935
1217.713571	136.097252	49.037940
1214.508938	124.779232	49.042945
1210.636212	127.226188	49.047949
1207.249952	126.254198	49.052954
1203.394037	126.897108	49.057959
1200.076881	121.384089	49.062964
1196.870593	125.098875	49.067969
1193.259631	130.663490	49.072973
1189.930142	115.412140	49.077978
1186.499819	130.798298	49.082983
1182.955532	138.651602	49.087988
1179.664807	130.415544	49.092993
1175.185921	137.645427	49.097997
1171.904492	127.576080	49.103002
1168.564366	127.457865	49.108007
1164.988561	123.467513	49.113012
1162.131834	119.485918	49.118017
1158.535146	130.655146	49.123021
1155.026471	117.008156	49.128026
1150.866151	130.734483	49.133031
1147.653636	125.524456	49.138036
1144.094941	115.986791	49.143041
1140.510593	135.485049	49.148045
1137.259945	117.777284	49.153050
1134.031885	125.757459	49.158055
1130.101528	127.300215	49.163060
1126.973743	122.744808	49.168065
1123.168984	136.605523	49.173069
1119.645767	120.896563	49.178074
1116.199967	118.205394	49.183079
1112.758060	116.133444	49.188084
1109.108311	113.512158	49.193089
1105.306155	126.263049	49.198093
1102.293947	128.131934	49.203098
1098.798407	118.751388	49.208103
1095.003827	126.937971	49.213108
1091.652472	110.474457	49.218113
1088.022467	123.021421	49.223117
1084.832014	118.368453	49.228122
1081.870407	123.947161	49.233127
1077.836395	128.819650	49.238132
1074.452683	128.059320	49.243137
1070.505845	128.719190	49.248141
1067.175365	128.634652	49.253146
1063.829453	118.526891	49.258151
1060.268915	129.773258	49.263156
1056.848486	114.471108	49.268161
1053.087083	131.643000	49.273165
1049.468045	120.295042	49.278170
1045.737069	125.588995	49.283175
1042.337276	132.508888	49.288180
1039.195247	126.925605	49.293185
1035.971173	130.177641	49.298189
1032.454992	120.920705	49.303194
1028.862513	123.837166	49.308199
1025.085801	124.894479	49.313204
1021.761442	117.498508	49.318209
1017.953600	131.660674	49.323213
1014.522684	122.296342	49.328218
1011.060470	118.950887	49.333223
1007.669256	125.440812	49.338228
1004.097171	124.836913	49.343233
1000.409127	128.095621	49.348237
997.179549	128.922225	49.353242
994.013204	119.119697	49.358247
989.950617	118.784733	49.363252
986.488705	115.566609	49.368257
983.315799	124.495097	49.373261
979.626805	112.719226	49.378266
976.120721	121.623506	49.383271
972.213853	114.782794	49.388276
968.915664	108.369989	49.393281
965.397331	129.114079	49.398285
962.138453	123.895528	49.403290
958.709333	110.927910	49.408295
954.936154	129.455543	49.413300
951.464427	115.257315	49.418305
947.569929	129.287706	49.423309
944.772948	114.858894	49.428314
941.132455	122.315206	49.433319
937.621714	127.762763	49.438324
934.174114	116.142796	49.443329
930.735281	130.587883	49.448333
927.217534	120.860878	49.453338
923.800019	126.761665	49.458343
919.632747	114.875880	49.463348
916.567517	110.992365	49.468353
913.113502	124.785573	49.473357
909.659427	114.589712	49.478362
906.089111	127.027648	49.483367
902.779944	125.711401	49.488372
899.038905	119.650953	49.493377
895.100830	135.513512	49.498381
891.861257	118.112286	49.503386
888.393861	122.820480	49.508391
884.823094	133.726273	49.513396
881.917431	110.482939	49.518401
878.370248	126.852169	49.523405
874.476120	117.515777	49.528410
870.658112	117.078248	49.533415
867.178908	113.904382	49.538420
864.150121	114.502058	49.543425
860.389497	117.932448	49.548429
857.326102	115.910105	49.553434
853.804875	119.335299	49.558439
849.821135	123.335283	49.563444
846.676708	111.326428	49.568449
842.647700	127.649351	49.573453
839.263995	111.436608	49.578458
836.207178	118.268771	49.583463
832.595167	123.341433	49.588468
829.448654	111.290215	49.593473
825.277675	118.730986	49.598477
821.746341	120.374752	49.603482
818.548166	112.463500	49.608487
814.593943	121.482302	49.613492
811.102384	104.650767	49.618497
807.643535	123.043766	49.623501
804.321161	110.032872	49.628506
801.016098	110.266777	49.633511
797.506233	125.114217	49.638516
794.151360	121.307400	49.643521
790.458726	118.474261	49.648525
786.727627	110.981434	49.653530
783.583882	118.737682	49.658535
779.818725	112.822768	49.663540
776.364625	111.688173	49.668545
772.883376	123.469792	49.673549
769.493952	107.450820	49.678554
766.182524	108.583465	49.683559
762.250063	123.579828	49.688564
758.823779	104.680667	49.693569
754.957047	111.875199	49.698573
751.882043	111.250514	49.703578
748.493057	115.040356	49.708583
744.973328	116.375917	49.713588
741.246758	107.524273	49.718593
737.277477	120.773902	49.723597
734.398511	118.482610	49.728602
731.450600	114.168712	49.733607
727.386854	124.016600	49.738612
724.054264	113.168506	49.743617
720.001826	123.426912	49.748621
716.918790	116.244612	49.753626
713.534831	113.627209	49.758631
709.895387	116.025552	49.763636
706.410983	109.832476	49.768641
702.732896	118.060381	49.773645
699.258433	125.662528	49.778650
695.941442	104.967873	49.783655
692.329149	115.104071	49.788660
688.707213	98.536462	49.793665
685.265476	116.648161	49.798669
681.878382	109.653331	49.803674
678.625671	115.400135	49.808679
674.639393	120.932468	49.813684
671.316969	109.358792	49.818689
667.705678	108.528132	49.823693
664.333199	117.023055	49.828698
660.873873	110.388522	49.833703
657.195487	112.875603	49.838708
653.881798	104.415762	49.843713
650.297085	123.525816	49.848717
646.626110	121.206339	49.853722
643.327999	116.159989	49.858727
639.678280	109.367890	49.863732
636.353084	107.026335	49.868737
632.955490	115.015959	49.873741
629.373003	103.274736	49.878746
625.864728	110.161219	49.883751
621.834939	117.290213	49.888756
618.628608	114.137517	49.893761
615.106535	113.804964	49.898765
611.912919	113.481203	49.903770
608.388862	114.128438	49.908775
604.719429	115.317630	49.913780
601.369532	113.387129	49.918785
597.846285	120.650502	49.923789
594.187738	114.643413	49.928794
590.566544	124.260721	49.933799
587.335349	114.431852	49.938804
583.651310	116.538602	49.943809
580.184948	117.297570	49.948813
576.756800	115.251260	49.953818
573.152572	109.632798	49.958823
569.460724	114.767411	49.963828
565.974833	114.224691	49.968833
562.560932	113.723355	49.973837
559.563517	109.801690	49.978842
555.763690	110.204948	49.983847
552.110916	114.567151	49.988852
548.762206	108.093377	49.993857
544.939684	118.956734	49.998861
541.515599	117.266907	50.003866
538.216121	115.145597	50.008871
534.404745	113.635765	50.013876
531.398713	115.533078	50.018881
527.788741	119.439538	50.023885
524.130898	124.404200	50.028890
520.886320	106.728322	50.033895
517.093802	111.751338	50.038900
513.952818	100.310186	50.043905
510.059815	103.462417	50.048909
506.580681	111.786787	50.053914
503.130816	105.272529	50.058919
499.421973	116.414575	50.063924
495.941145	111.979378	50.068929
492.706453	111.461401	50.073933
489.022678	114.045060	50.078938
485.894812	118.985730	50.083943
482.442367	122.132291	50.088948
478.884979	114.086020	50.093953
474.872902	117.710773	50.098957
471.463484	114.474893	50.103962
467.864278	112.949389	50.108967
464.643263	111.692998	50.113972
461.031651	104.264407	50.118977
457.644537	104.078742	50.123981
453.988170	112.613841	50.128986
450.528385	105.505866	50.133991
446.926897	123.127973	50.138996
443.778476	106.402895	50.144001
439.882153	108.085942	50.149005
436.651575	114.778756	50.154010
433.466204	97.470824	50.159015
429.659659	110.422796	50.164020
426.174531	100.943788	50.169025
422.343273	102.079507	50.174029
418.677214	102.181058	50.179034
415.529075	112.659100	50.184039
412.029107	106.625833	50.189044
408.617066	106.092703	50.194049
404.742485	103.209844	50.199053
401.454391	105.766462	50.204058
397.886533	108.188266	50.209063
394.064498	106.541274	50.214068
391.399846	101.468856	50.219073
388.082719	107.533145	50.224077
384.053074	106.233690	50.229082
380.445404	92.254952	50.234087
377.012822	102.738261	50.239092
373.588585	100.683132	50.244097
370.081044	106.167320	50.249101
366.621280	107.704198	50.254106
363.451084	101.027015	50.259111
359.589366	107.367450	50.264116
355.951220	96.298579	50.269121
352.259746	101.017504	50.274125
348.494682	110.400500	50.279130
345.065362	100.005581	50.284135
342.041930	105.591232	50.289140
338.636777	96.769929	50.294145
335.471404	98.909313	50.299149
331.624515	96.522999	50.304154
328.059501	89.214463	50.309159
324.159007	96.799644	50.314164
320.643735	96.402792	50.319169
317.304329	95.560462	50.324173
313.988530	103.098874	50.329178
311.038398	99.018878	50.334183
306.686039	106.855813	50.339188
303.419366	103.477468	50.344193
299.513443	98.129716	50.349197
296.126174	96.394284	50.354202
293.090703	96.021272	50.359207
289.232079	87.034010	50.364212
285.844974	91.429207	50.369217
282.678019	101.939307	50.374221
278.905355	107.963876	50.379226
275.597903	96.024739	50.384231
271.851418	104.749529	50.389236
268.679199	102.572416	50.394241
265.116720	98.555632	50.399245
261.247704	95.761724	50.404250
258.276861	103.725591	50.409255
254.342635	106.159365	50.414260
250.579496	107.013811	50.419265
247.247466	97.107210	50.424269
243.738048	106.555551	50.429274
240.526297	100.310609	50.434279
236.962681	105.306311	50.439284
233.498360	94.609840	50.444289
229.770409	99.967237	50.449293
226.328259	102.483492	50.454298
222.655488	93.707172	50.459303
219.287073	101.171447	50.464308
215.672010	100.578637	50.469313
212.463273	101.113313	50.474317
208.751861	98.708933	50.479322
205.612862	84.058491	50.484327
201.857402	105.879431	50.489332
198.377982	94.920291	50.494337
194.591825	97.468344	50.499341
190.844334	102.804623	50.504346
188.060465	92.832251	50.509351
184.305180	106.051011	50.514356
181.225568	93.657471	50.519361
177.492425	105.136930	50.524365
173.770950	110.227019	50.529370
170.588346	100.768925	50.534375
166.800265	100.807418	50.539380
163.649590	91.969238	50.544385
159.824718	94.731377	50.549389
155.936376	89.829998	50.554394
152.857541	99.057666	50.559399
149.202397	100.784395	50.564404
145.810426	85.270924	50.569409
142.342060	95.370651	50.574413
138.628671	108.209987	50.579418
135.597621	96.856959	50.584423
131.821593	105.983591	50.589428
128.416526	113.082629	50.594433
124.786330	107.471698	50.599437
121.140540	108.709737	50.604442
118.054690	94.785838	50.609447
114.017290	99.767352	50.614452
110.643357	102.009773	50.619457
107.180251	104.608674	50.624461
103.505537	102.753625	50.629466
100.192767	95.215907	50.634471
96.573866	113.593850	50.639476
93.175676	112.320363	50.644481
89.797853	101.013514	50.649485
86.647798	113.208206	50.654490
83.093913	107.475775	50.659495
79.102090	108.118118	50.664500
75.840422	102.622914	50.669505
72.010576	102.586580	50.674509
68.558580	107.419788	50.679514
65.419238	91.879615	50.684519
61.578129	100.030678	50.689524
58.093335	103.252645	50.694529
54.721498	95.750859	50.699533
51.081246	98.254954	50.704538
47.713375	97.387875	50.709543
44.117266	104.309765	50.714548
40.913097	106.110999	50.719553
36.929815	102.677295	50.724557
33.110159	109.276240	50.729562
29.777396	95.600476	50.734567
26.529220	106.821987	50.739572
23.533554	107.415663	50.744577
19.955248	114.283030	50.749581
16.319818	112.228274	50.754586
12.555037	106.180810	50.759591
9.341886	115.504633	50.764596
5.738009	103.910915	50.769601
2.155717	97.007361	50.774605