Thu Jun 16 18:41:14 2022

Number of Points = 9932

Depth (nm)	Load (N)	Time (s)
-0.970096	96.600111	0.000000
-0.682115	102.726637	0.005005
-0.736097	88.024556	0.010010
-1.449535	93.073117	0.015014
-1.097561	76.500840	0.020019
-1.246956	64.215026	0.025024
-2.164018	58.751301	0.030029
-2.009887	48.399983	0.035034
-2.624914	44.584104	0.040038
-2.813116	25.444274	0.045043
-3.300874	36.602110	0.050048
-3.088556	23.185360	0.055053
-3.494158	9.943247	0.060058
-3.946599	15.402068	0.065062
-4.285425	17.636331	0.070067
-4.964343	14.706381	0.075072
-5.297394	10.744075	0.080077
-5.207295	12.310002	0.085082
-5.428495	24.048166	0.090086
-5.299956	8.806349	0.095091
-5.586693	19.448433	0.100096
-6.149185	26.249589	0.105101
-6.413932	18.556018	0.110106
-7.123268	18.062836	0.115110
-6.825131	16.754115	0.120115
-7.286378	23.138790	0.125120
-7.209585	19.049955	0.130125
-7.315214	11.850200	0.135130
-7.955430	17.546636	0.140134
-8.146210	-1.184699	0.145139
-8.278660	3.891240	0.150144
-8.466307	7.502597	0.155149
-9.247683	3.036068	0.160154
-9.783004	6.294082	0.165158
-9.697522	7.204028	0.170163
-10.198722	6.570693	0.175168
-10.304791	5.140438	0.180173
-10.013930	5.286202	0.185178
-10.138343	14.439989	0.190182
-10.126688	8.013841	0.195187
-10.460081	16.696262	0.200192
-11.335415	14.056755	0.205197
-11.405811	9.887968	0.210202
-11.387885	8.621608	0.215206
-11.441148	-2.065061	0.220211
-12.524013	12.079511	0.225216
-12.983492	10.392655	0.230221
-12.852824	8.487125	0.235226
-13.319840	2.605437	0.240230
-13.194794	3.481615	0.245235
-13.067804	12.248662	0.250240
-13.334339	12.699139	0.255245
-13.956629	10.071385	0.260250
-14.387436	14.344453	0.265254
-14.678614	1.144606	0.270259
-14.621633	4.442658	0.275264
-14.852675	1.790501	0.280269
-14.757537	1.771004	0.285274
-15.499028	27.424068	0.290278
-16.328648	5.594978	0.295283
-16.341778	12.820913	0.300288
-17.113646	19.817178	0.305293
-16.487643	11.220912	0.310298
-17.073963	24.860310	0.315302
-16.802163	8.614586	0.320307
-16.663088	16.912804	0.325312
-16.997145	13.873678	0.330317
-17.133802	4.937602	0.335322
-17.996958	18.955604	0.340326
-17.899999	4.062231	0.345331
-18.362624	4.932728	0.350336
-19.218874	6.266542	0.355341
-19.452530	8.860087	0.360346
-19.463420	18.427222	0.365350
-19.414378	9.849649	0.370355
-19.531060	13.036411	0.375360
-20.087621	18.888512	0.380365
-19.864783	14.357741	0.385370
-20.178612	25.613598	0.390374
-20.798768	14.692574	0.395379
-21.283350	12.196360	0.400384
-21.608544	14.542907	0.405389
-21.676337	19.504380	0.410394
-21.998618	16.164384	0.415398
-21.348410	12.295796	0.420403
-21.644214	6.123885	0.425408
-22.675847	14.128904	0.430413
-22.738972	-4.554756	0.435418
-23.053457	3.560426	0.440422
-22.815445	-0.702929	0.445427
-23.329911	6.713878	0.450432
-23.986617	8.807012	0.455437
-24.108582	8.531276	0.460442
-24.008456	15.284881	0.465446
-24.106262	5.491686	0.470451
-24.591853	17.922485	0.475456
-25.058289	10.892260	0.480461
-25.528411	6.262223	0.485466
-26.354032	9.044160	0.490470
-26.482147	13.627393	0.495475
-25.929480	11.568861	0.500480
-25.916440	2.725547	0.505485
-25.872291	16.535303	0.510490
-26.128374	17.113784	0.515494
-26.692783	4.616426	0.520499
-26.858381	3.852852	0.525504
-27.317815	9.804720	0.530509
-27.829103	-6.373037	0.535514
-28.786534	10.036730	0.540518
-28.648038	8.043189	0.545523
-29.103979	3.930918	0.550528
-29.009313	10.029862	0.555533
-28.717664	6.700878	0.560538
-29.085119	6.183362	0.565542
-29.166494	5.915223	0.570547
-29.102055	5.233105	0.575552
-29.941630	12.933013	0.580557
-30.158942	16.916074	0.585562
-30.408326	16.277233	0.590566
-30.619291	9.688889	0.595571
-30.860068	13.854687	0.600576
-31.796509	13.783792	0.605581
-31.843276	14.615656	0.610586
-32.648624	8.078481	0.615590
-31.680045	-3.748800	0.620595
-32.135703	8.930094	0.625600
-32.417787	10.679464	0.630605
-32.119659	3.579224	0.635610
-33.221655	12.817611	0.640614
-33.663593	13.319273	0.645619
-33.652224	9.236913	0.650624
-33.977086	4.744271	0.655629
-33.960392	12.031670	0.660634
-34.168511	9.424164	0.665638
-33.823536	8.772635	0.670643
-34.574787	9.507826	0.675648
-35.113360	20.047590	0.680653
-35.270400	9.834245	0.685658
-35.499520	13.236108	0.690662
-35.574908	2.626692	0.695667
-35.567461	10.860236	0.700672
-36.885882	14.740941	0.705677
-36.849437	-1.206611	0.710682
-36.936864	13.755762	0.715686
-37.238123	6.968656	0.720691
-37.038853	12.620475	0.725696
-37.277671	17.338417	0.730701
-37.115583	6.355807	0.735706
-38.348323	23.826242	0.740710
-38.822067	14.864085	0.745715
-38.667511	17.202382	0.750720
-38.848428	18.635419	0.755725
-38.694020	17.376298	0.760730
-38.827809	9.857317	0.765734
-39.113455	16.702494	0.770739
-39.873697	10.385264	0.775744
-40.211214	25.724010	0.780749
-40.482087	20.703419	0.785754
-40.245446	18.797936	0.790758
-40.539405	16.255028	0.795763
-41.178769	22.446079	0.800768
-41.429158	25.586178	0.805773
-41.758557	10.784374	0.810778
-41.938667	14.505179	0.815782
-41.667842	15.290674	0.820787
-41.903556	2.887476	0.825792
-42.775354	13.622098	0.830797
-42.865771	18.461326	0.835802
-43.266118	11.746630	0.840806
-43.638933	12.706170	0.845811
-43.662084	14.724103	0.850816
-43.593277	5.822245	0.855821
-43.635803	17.122442	0.860826
-44.445997	21.201116	0.865830
-45.088519	21.365282	0.870835
-45.353130	12.924287	0.875840
-45.471809	8.011537	0.880845
-45.715783	11.318285	0.885850
-45.309507	15.571501	0.890854
-45.374685	10.210796	0.895859
-45.153771	10.138549	0.900864
-45.883362	24.016787	0.905869
-46.352003	5.443148	0.910874
-47.047967	19.360417	0.915878
-46.896236	12.904609	0.920883
-47.071642	8.869394	0.925888
-47.847633	-0.295853	0.930893
-48.016739	7.153952	0.935898
-48.271287	18.204569	0.940902
-48.346217	4.998979	0.945907
-48.187237	6.038741	0.950912
-48.476100	4.398670	0.955917
-48.676249	17.462420	0.960922
-49.278209	6.537711	0.965926
-49.296208	3.936967	0.970931
-49.677817	5.178534	0.975936
-49.884156	18.701460	0.980941
-50.424050	13.473071	0.985946
-50.911356	18.421298	0.990950
-50.966449	9.572964	0.995955
-51.165502	21.617829	1.000960
-51.546817	15.729475	1.005965
-51.229651	9.682777	1.010970
-51.424638	18.117589	1.015974
-51.770563	18.190911	1.020979
-52.347313	10.824947	1.025984
-52.754030	16.345765	1.030989
-52.798526	10.878844	1.035994
-52.921962	13.182184	1.040998
-53.357630	8.085739	1.046003
-53.801768	1.805657	1.051008
-54.644125	21.236656	1.056013
-54.286890	-3.471363	1.061018
-54.731182	10.876072	1.066022
-54.592761	7.371352	1.071027
-54.507795	8.390889	1.076032
-54.828892	15.461134	1.081037
-54.611546	-0.571558	1.086042
-55.381958	7.672048	1.091046
-55.865885	-0.123797	1.096051
-56.032650	16.854278	1.101056
-56.331062	17.596617	1.106061
-56.301884	12.974829	1.111066
-57.084208	16.657336	1.116070
-57.494554	18.453160	1.121075
-57.800888	15.590980	1.126080
-58.172271	21.440005	1.131085
-57.966518	7.354198	1.136090
-58.128766	16.536038	1.141094
-58.120982	12.466601	1.146099
-57.974302	14.286881	1.151104
-58.428185	19.284634	1.156109
-58.804323	11.950234	1.161114
-59.358480	12.447260	1.166118
-59.825940	15.720602	1.171123
-59.837237	1.054475	1.176128
-60.189815	18.563536	1.181133
-60.017339	15.385850	1.186138
-60.926221	16.818736	1.191142
-61.219583	7.374248	1.196147
-61.149074	7.354183	1.201152
-61.354748	11.925767	1.206157
-61.369879	3.705774	1.211162
-61.416174	13.712439	1.216166
-61.624201	4.645607	1.221171
-62.266890	8.031763	1.226176
-62.749465	5.225743	1.231181
-62.352802	5.182262	1.236186
-62.851309	8.674912	1.241190
-63.710804	-2.886956	1.246195
-64.025312	5.059036	1.251200
-64.242391	9.393957	1.256205
-64.262848	6.377395	1.261210
-64.393393	6.083840	1.266214
-64.716173	1.715460	1.271219
-64.443668	7.225737	1.276224
-64.517791	16.067648	1.281229
-65.432797	8.976602	1.286234
-65.728622	15.064017	1.291238
-65.894812	3.148427	1.296243
-66.025821	13.436445	1.301248
-66.021636	18.323966	1.306253
-66.178155	7.048919	1.311258
-67.186782	3.233291	1.316262
-67.899123	-3.144822	1.321267
-67.671055	1.190028	1.326272
-67.706401	6.716158	1.331277
-67.211945	7.266990	1.336282
-67.612824	18.651762	1.341286
-68.187707	16.505901	1.346291
-68.758896	10.041514	1.351296
-69.306472	13.998159	1.356301
-68.848880	13.367084	1.361306
-69.072756	11.761950	1.366310
-69.294969	10.504398	1.371315
-70.305304	7.393939	1.376320
-70.991660	7.221738	1.381325
-70.516765	0.439157	1.386330
-70.900735	8.836729	1.391334
-71.359406	7.444228	1.396339
-71.363066	10.519673	1.401344
-71.541178	13.490372	1.406349
-71.369099	8.349033	1.411354
-71.363521	16.861387	1.416358
-71.269807	9.071987	1.421363
-72.132537	-0.389779	1.426368
-72.534671	20.242391	1.431373
-72.314886	13.223265	1.436378
-72.659964	10.804333	1.441382
-73.678503	5.501449	1.446387
-74.040449	9.529620	1.451392
-74.160821	17.090648	1.456397
-74.084025	7.854018	1.461402
-74.156801	9.881927	1.466406
-74.435901	11.677567	1.471411
-74.742925	7.041300	1.476416
-75.761355	14.972420	1.481421
-75.463450	10.642537	1.486426
-75.802430	15.879380	1.491430
-75.959104	8.995773	1.496435
-75.560704	6.908867	1.501440
-75.979131	12.099448	1.506445
-76.469178	7.931849	1.511450
-77.047297	8.506926	1.516454
-77.292902	9.257310	1.521459
-77.340181	7.699745	1.526464
-77.487370	12.569662	1.531469
-77.551525	3.767719	1.536474
-78.376392	1.975516	1.541478
-78.524727	8.583224	1.546483
-78.728719	5.540466	1.551488
-78.851267	-4.304466	1.556493
-78.707897	5.051494	1.561498
-78.913208	8.149905	1.566502
-79.803489	8.635101	1.571507
-80.369791	12.347514	1.576512
-80.643922	16.824457	1.581517
-80.521282	0.881113	1.586522
-80.934404	17.166501	1.591526
-80.651237	10.622480	1.596531
-80.581850	13.883360	1.601536
-80.821454	18.928867	1.606541
-81.853600	18.708450	1.611546
-81.953837	21.572756	1.616550
-81.896432	7.626401	1.621555
-81.814177	18.147023	1.626560
-83.052650	16.450994	1.631565
-83.484158	4.853119	1.636570
-83.870717	14.031577	1.641574
-83.314043	8.799449	1.646579
-83.790705	12.101245	1.651584
-83.925199	13.990978	1.656589
-83.791920	13.462137	1.661594
-84.011338	24.564663	1.666598
-84.290451	13.025058	1.671603
-84.875953	13.360145	1.676608
-85.702929	24.374847	1.681613
-85.075910	18.948184	1.686618
-85.456799	14.444679	1.691622
-85.573230	15.727858	1.696627
-86.530682	9.733077	1.701632
-86.914420	20.062471	1.706637
-87.166883	4.786264	1.711642
-87.053701	15.271880	1.716646
-87.253156	9.195235	1.721651
-87.029836	4.117941	1.726656
-87.424085	20.818804	1.731661
-87.399444	20.832857	1.736666
-87.882208	16.833345	1.741670
-88.540757	13.503746	1.746675
-88.292338	21.682174	1.751680
-88.991304	19.067890	1.756685
-88.716108	9.609844	1.761690
-89.555313	16.884396	1.766694
-90.261816	16.140765	1.771699
-90.226876	16.478085	1.776704
-90.721664	9.366035	1.781709
-90.066968	10.395001	1.786714
-90.216728	14.716923	1.791718
-90.169663	18.025690	1.796723
-91.014558	14.819228	1.801728
-91.645386	19.518593	1.806733
-91.676730	14.209616	1.811738
-92.006231	12.779195	1.816742
-92.110281	16.334120	1.821747
-91.991093	4.653916	1.826752
-92.964221	27.245030	1.831757
-92.965593	-1.178840	1.836762
-93.590326	13.410030	1.841766
-93.785874	7.796812	1.846771
-93.267437	7.888683	1.851776
-93.515095	18.157505	1.856781
-94.088185	15.661817	1.861786
-94.511913	18.760024	1.866790
-94.824639	19.633474	1.871795
-94.661033	18.374509	1.876800
-95.108348	23.448425	1.881805
-95.131829	8.456678	1.886810
-95.863325	10.579443	1.891814
-96.382294	8.913870	1.896819
-96.735183	-0.387192	1.901824
-96.972310	15.593564	1.906829
-96.917988	-3.564093	1.911834
-96.600467	7.878236	1.916838
-97.105493	7.387505	1.921843
-96.529362	8.602790	1.926848
-97.505416	12.732949	1.931853
-97.889735	5.506063	1.936858
-98.357915	10.034016	1.941862
-98.549710	4.476511	1.946867
-98.337351	5.473020	1.951872
-98.610399	4.531377	1.956877
-99.058656	9.772762	1.961882
-99.558683	13.506680	1.966886
-99.568126	13.876887	1.971891
-99.686531	14.661397	1.976896
-100.250067	14.604354	1.981901
-100.845171	14.921002	1.986906
-100.851175	17.406388	1.991910
-101.180180	18.755874	1.996915
-101.324948	18.252735	2.006912
-100.676212	11.739573	2.016909
-100.395319	11.763973	2.026906
-100.122619	13.358220	2.036902
-99.653705	18.737330	2.046899
-98.962731	12.343577	2.056896
-98.560453	14.717029	2.066893
-97.940684	13.836599	2.076890
-97.560470	14.878327	2.086886
-96.560495	8.843300	2.096883
-96.070351	17.154324	2.106880
-95.694164	15.056027	2.116877
-95.724808	17.311418	2.126874
-95.350557	21.016871	2.136870
-94.600659	18.505695	2.146867
-93.452493	14.420165	2.156864
-92.723526	14.290698	2.166861
-93.112583	16.101737	2.176858
-92.878896	15.906200	2.186854
-92.016697	26.336083	2.196851
-91.172821	19.244853	2.206848
-90.947903	18.624180	2.216845
-90.094807	24.042631	2.226842
-89.765325	12.353013	2.236838
-89.798616	19.892584	2.246835
-89.120567	15.602236	2.256832
-88.526860	8.971433	2.266829
-87.605177	14.151498	2.276826
-86.801441	13.688243	2.286822
-86.843326	24.042814	2.296819
-86.917511	24.327856	2.306816
-86.104949	24.210998	2.316813
-85.479493	18.931257	2.326810
-84.751262	19.013749	2.336806
-84.106692	12.212588	2.346803
-83.809601	13.573288	2.356800
-83.716820	7.759264	2.366797
-82.578221	11.266582	2.376794
-82.179017	17.081429	2.386790
-82.271865	16.615016	2.396787
-81.205464	15.014994	2.406784
-80.652599	12.892685	2.416781
-80.516371	12.065005	2.426778
-79.916069	9.523385	2.436774
-79.225111	15.717984	2.446771
-79.015777	16.405622	2.456768
-77.985003	15.230616	2.466765
-77.447466	23.270365	2.476762
-77.326940	17.849000	2.486758
-77.375395	15.506562	2.496755
-76.745318	13.482226	2.506752
-76.022940	17.068261	2.516749
-75.040143	14.927945	2.526746
-74.335352	17.419678	2.536742
-74.341389	19.707205	2.546739
-74.270575	8.906446	2.556736
-73.414458	0.629807	2.566733
-73.061788	11.911222	2.576730
-72.017674	3.976460	2.586726
-71.521454	10.850207	2.596723
-71.502051	9.043603	2.606720
-71.087103	16.883871	2.616717
-70.059583	8.910114	2.626714
-69.839349	15.430201	2.636710
-69.843204	16.006679	2.646707
-68.556326	10.954278	2.656704
-68.218731	16.064677	2.666701
-68.098696	13.628803	2.676698
-67.243671	8.330241	2.686694
-66.978528	12.207826	2.696691
-66.275114	11.414677	2.706688
-65.266616	7.425728	2.716685
-64.950132	4.975565	2.726682
-64.999531	10.757471	2.736678
-64.915112	18.585737	2.746675
-63.933847	14.399181	2.756672
-63.506095	14.671948	2.766669
-62.663147	19.095133	2.776666
-62.392464	19.693460	2.786662
-61.847752	13.749034	2.796659
-60.924263	12.273587	2.806656
-60.659480	16.392209	2.816653
-60.465644	16.352121	2.826650
-59.711632	21.244843	2.836646
-58.942139	16.083594	2.846643
-58.601465	6.987450	2.856640
-58.426640	5.769184	2.866637
-58.121819	14.628649	2.876634
-57.616872	13.447148	2.886630
-56.632702	4.605656	2.896627
-55.836390	7.005709	2.906624
-55.534526	9.186639	2.916621
-55.305794	13.389008	2.926618
-55.371944	15.834542	2.936614
-54.412296	23.751146	2.946611
-53.882993	18.861973	2.956608
-52.767780	16.640508	2.966605
-52.204020	14.105669	2.976602
-52.648324	13.661974	2.986598
-52.242949	14.703943	2.996595
-51.345090	17.368496	3.006592
-51.115175	12.130518	3.016589
-49.954356	14.213899	3.026586
-49.333461	11.265456	3.036582
-49.456524	19.860771	3.046579
-49.390050	15.969911	3.056576
-48.347810	18.438627	3.066573
-47.781821	13.187732	3.076570
-46.971947	11.692539	3.086566
-46.584312	14.430151	3.096563
-46.674010	20.326492	3.106560
-45.487333	16.778393	3.116557
-45.202072	12.559973	3.126554
-44.803820	4.640872	3.136550
-44.453247	11.537260	3.146547
-43.437310	16.259072	3.156544
-43.319153	19.247967	3.166541
-42.860435	13.521538	3.176538
-41.885381	16.072183	3.186534
-41.636199	22.181156	3.196531
-41.554984	16.377484	3.206528
-40.674074	14.180616	3.216525
-39.968469	13.748055	3.226522
-39.827496	10.886827	3.236518
-39.541274	11.288482	3.246515
-38.384944	13.916397	3.256512
-38.080989	12.977727	3.266509
-38.005774	10.844812	3.276506
-37.615534	9.347945	3.286502
-36.938780	20.105470	3.296499
-35.938794	11.733731	3.306496
-35.392839	22.862361	3.316493
-35.240747	10.817401	3.326490
-35.212947	10.333223	3.336486
-33.954120	13.411187	3.346483
-33.537665	6.031038	3.356480
-33.607383	5.893743	3.366477
-32.535983	1.980541	3.376474
-31.948865	6.276399	3.386470
-32.021855	14.924682	3.396467
-31.457124	12.301769	3.406464
-30.635430	18.862339	3.416461
-30.482333	15.831179	3.426458
-29.489920	19.949971	3.436454
-29.133269	12.581530	3.446451
-29.040317	19.635183	3.456448
-27.699686	18.174274	3.466445
-27.366658	10.229400	3.476442
-27.232444	15.390601	3.486438
-26.885035	23.627929	3.496435
-26.313205	20.167413	3.506432
-25.747525	17.730990	3.516429
-25.345408	10.088821	3.526426
-24.524684	12.103601	3.536422
-23.998478	24.176387	3.546419
-23.980667	12.984710	3.556416
-23.117304	11.988414	3.566413
-22.199486	9.858696	3.576410
-22.301992	10.892139	3.586406
-22.295545	12.769885	3.596403
-21.269532	14.556043	3.606400
-20.664053	12.470976	3.616397
-20.244813	14.003919	3.626394
-19.717307	9.449569	3.636390
-18.858154	12.631764	3.646387
-19.150680	10.557892	3.656384
-18.141655	10.351827	3.666381
-17.651684	4.603246	3.676378
-17.115684	5.699247	3.686374
-16.245033	17.966160	3.696371
-15.909909	18.367243	3.706368
-15.753102	11.967086	3.716365
-15.674298	11.112595	3.726362
-14.672496	12.310019	3.736358
-14.242530	14.845990	3.746355
-13.617749	14.506652	3.756352
-13.141290	13.934254	3.766349
-12.980807	18.243477	3.776346
-11.869189	22.522850	3.786342
-11.419989	17.308345	3.796339
-11.247819	21.462971	3.806336
-11.077752	19.868937	3.816333
-9.967259	15.023449	3.826330
-9.597568	18.913298	3.836326
-9.253060	16.924404	3.846323
-8.336048	15.494239	3.856320
-8.249743	13.489981	3.866317
-7.902035	17.187185	3.876314
-7.110382	12.959464	3.886310
-6.753274	19.649662	3.896307
-6.374754	21.981214	3.906304
-5.290051	17.644808	3.916301
-4.918025	12.270142	3.926298
-4.633554	13.502343	3.936294
-4.591525	16.676589	3.946291
-3.588813	26.489452	3.956288
-3.125725	16.859755	3.966285
-3.026615	21.308130	3.976282
-2.575235	36.122270	3.986278
-2.022157	46.838175	3.996275
-1.797029	54.379912	4.006272
-1.222312	69.333334	4.016269
-0.739455	91.671644	4.026266
-0.161479	106.161476	4.036262
0.000000	126.683955	4.041267
0.381904	136.481136	4.046272
0.642203	148.222005	4.051277
0.522987	151.082665	4.056282
1.232523	157.218474	4.061286
1.002140	162.777191	4.066291
0.980549	144.891906	4.071296
0.700425	160.797355	4.076301
0.833902	157.522694	4.081306
1.388381	184.729866	4.086310
1.159579	190.124365	4.091315
1.045182	171.021977	4.096320
0.880612	176.626156	4.101325
0.976209	184.210970	4.106330
1.438811	192.221021	4.111334
1.295880	194.359894	4.116339
1.193633	199.239514	4.121344
1.415736	202.876829	4.126349
1.357011	203.965310	4.131354
1.505795	199.808494	4.136358
0.990688	197.565607	4.141363
0.998350	188.904106	4.146368
1.260918	195.931158	4.151373
1.157230	191.202031	4.156378
1.356543	194.947390	4.161382
1.117401	201.985828	4.166387
1.224507	209.661885	4.171392
1.310252	193.290341	4.176397
1.307455	197.287622	4.181402
1.562960	200.676626	4.186406
0.995498	199.671249	4.191411
0.898126	198.120461	4.196416
1.117494	199.526828	4.201421
1.317568	204.351458	4.206426
1.351384	200.365176	4.211430
1.244390	215.624585	4.216435
1.485425	214.800510	4.221440
1.818957	223.632302	4.226445
1.627206	226.114185	4.231450
2.046768	200.853412	4.236454
1.242985	200.935603	4.241459
1.424659	196.348046	4.246464
1.632889	201.882439	4.251469
1.338813	202.910466	4.256474
1.573379	211.251415	4.261478
1.533037	222.731948	4.266483
1.908292	234.004606	4.271488
1.790661	210.240413	4.276493
1.715815	199.100096	4.281498
1.838085	186.671325	4.286502
1.378175	203.741959	4.291507
1.707098	199.157988	4.296512
1.508687	206.950631	4.301517
1.684255	204.603374	4.306522
1.501592	195.547127	4.311526
1.481699	223.218060	4.316531
1.696314	223.540689	4.321536
1.970949	224.718220	4.326541
1.849291	234.783166	4.331546
2.108317	225.826559	4.336550
1.824439	214.906444	4.341555
1.715289	203.471089	4.346560
1.927320	205.797946	4.351565
1.422083	199.434741	4.356570
1.857702	210.718815	4.361574
1.688351	230.577724	4.366579
2.057307	231.314361	4.371584
2.208849	237.003850	4.376589
1.935198	223.018471	4.381594
1.876942	211.603014	4.386598
1.710730	205.669168	4.391603
1.557538	218.256225	4.396608
2.061233	233.169771	4.401613
2.042888	240.326037	4.406618
2.016922	231.300996	4.411622
1.900941	232.127636	4.416627
1.783494	235.814560	4.421632
2.225577	231.570594	4.426637
1.839902	236.561089	4.431642
2.223345	235.109606	4.436646
2.149419	233.412678	4.441651
1.901558	225.610649	4.446656
1.849052	230.023801	4.451661
1.733327	227.595734	4.456666
2.332965	219.213453	4.461670
1.900730	234.829897	4.466675
1.992135	235.062096	4.471680
2.145563	218.131799	4.476685
1.786419	238.702513	4.481690
1.919952	220.043889	4.486694
2.034560	233.885116	4.491699
2.141804	223.186366	4.496704
1.918228	232.454734	4.501709
1.600250	234.317397	4.506714
2.317281	241.534260	4.511718
2.092709	262.191684	4.516723
2.487036	256.998340	4.521728
2.021204	253.716344	4.526733
1.880471	257.306393	4.531738
2.453557	262.064565	4.536742
2.071042	272.783819	4.541747
2.314410	261.097393	4.546752
2.195852	264.872706	4.551757
2.107840	266.030453	4.556762
2.638287	268.461959	4.561766
2.070987	275.491717	4.566771
2.539009	260.952611	4.571776
2.605768	265.379114	4.576781
2.334236	263.800569	4.581786
2.323787	251.344152	4.586790
2.656098	270.315966	4.591795
2.565970	269.580355	4.596800
2.553317	276.080718	4.601805
2.405467	274.516362	4.606810
2.618755	271.752747	4.611814
2.480849	267.869014	4.616819
2.509166	267.434068	4.621824
2.469056	259.759191	4.626829
2.289318	268.900962	4.631834
2.721983	278.928792	4.636838
2.566047	274.316500	4.641843
2.583755	273.700596	4.646848
2.825056	269.608778	4.651853
2.514524	267.198987	4.656858
2.571743	251.976606	4.661862
2.806083	263.212294	4.666867
2.338113	257.431983	4.671872
2.655056	258.253182	4.676877
2.350604	268.623214	4.681882
2.598589	267.471732	4.686886
2.358662	260.716499	4.691891
2.439789	266.003870	4.696896
2.598253	268.854378	4.701901
2.703803	263.910702	4.706906
2.742128	259.148813	4.711910
2.664574	268.684700	4.716915
2.872297	265.110854	4.721920
2.934153	261.348805	4.726925
2.802100	259.753525	4.731930
2.859219	265.082747	4.736934
2.597786	265.411928	4.741939
2.903855	266.772800	4.746944
2.826164	261.536307	4.751949
2.907876	271.355657	4.756954
3.001020	276.922710	4.761958
2.690885	279.329356	4.766963
2.488993	264.983626	4.771968
2.585323	269.228648	4.776973
2.706414	273.885416	4.781978
2.589597	270.878410	4.786982
2.623356	276.222250	4.791987
2.855105	268.117091	4.796992
3.142712	260.797580	4.801997
2.724023	268.316677	4.807002
2.940447	262.714597	4.812006
2.772931	273.734938	4.817011
2.995282	291.979897	4.822016
3.302752	297.914157	4.827021
2.855928	292.601521	4.832026
2.804272	284.890655	4.837030
2.904726	296.591756	4.842035
2.725330	306.807073	4.847040
2.891359	290.230074	4.852045
2.655371	307.145135	4.857050
3.133406	306.441419	4.862054
3.094601	299.976822	4.867059
3.003620	308.182596	4.872064
3.177408	304.390694	4.877069
2.840824	310.855317	4.882074
3.070704	306.219511	4.887078
3.169232	312.552742	4.892083
3.197102	304.827047	4.897088
3.161316	304.943726	4.902093
3.076536	311.085666	4.907098
2.939379	303.198907	4.912102
2.731768	307.399358	4.917107
3.196425	310.390175	4.922112
3.506181	314.773379	4.927117
3.447640	320.998693	4.932122
3.316837	298.066440	4.937126
3.363147	308.935550	4.942131
3.210385	299.832469	4.947136
3.258862	298.813005	4.952141
2.683745	298.878520	4.957146
3.403236	309.705445	4.962150
3.412863	328.027035	4.967155
3.248595	328.707756	4.972160
3.490903	328.509936	4.977165
3.429748	332.960260	4.982170
3.406868	334.239153	4.987174
2.906412	331.459993	4.992179
3.052594	334.117794	4.997184
3.275947	333.635324	5.002189
3.173707	335.632827	5.007194
3.361870	337.153084	5.012198
3.072117	337.043583	5.017203
2.959939	338.162808	5.022208
3.614218	348.036462	5.027213
3.442219	354.056193	5.032218
3.961975	354.525418	5.037222
3.516256	353.271916	5.042227
3.494016	357.406231	5.047232
3.681564	343.604291	5.052237
3.545782	339.689803	5.057242
3.518066	335.545641	5.062246
3.352521	335.292491	5.067251
3.441399	365.171500	5.072256
3.711440	364.071219	5.077261
3.681236	373.259177	5.082266
3.645880	355.830433	5.087270
3.572237	352.747809	5.092275
3.382545	360.394161	5.097280
3.472604	363.942149	5.102285
3.484697	360.678328	5.107290
3.677120	353.513313	5.112294
3.646304	373.191661	5.117299
3.447469	365.686507	5.122304
3.777243	356.950667	5.127309
3.684655	364.405168	5.132314
3.749760	353.808297	5.137318
3.721145	357.084167	5.142323
3.290331	366.715192	5.147328
3.667153	362.233951	5.152333
3.392734	368.213490	5.157338
4.185357	374.058333	5.162342
3.965595	394.116881	5.167347
3.753550	391.964569	5.172352
3.872886	386.213534	5.177357
3.957666	396.167222	5.182362
4.160019	388.937705	5.187366
3.976492	382.143501	5.192371
3.676360	374.490620	5.197376
3.862455	370.857775	5.202381
3.540616	397.369778	5.207386
4.264062	404.124437	5.212390
3.961425	397.716618	5.217395
3.888997	394.067690	5.222400
3.737276	398.046915	5.227405
3.590258	394.263905	5.232410
3.760986	382.041153	5.237414
3.971009	397.613287	5.242419
3.746209	399.487702	5.247424
4.465130	396.526658	5.252429
3.870381	394.775883	5.257434
4.126863	399.240428	5.262438
4.198112	399.734246	5.267443
4.227881	402.518043	5.272448
3.929203	398.398121	5.277453
4.070412	405.086015	5.282458
4.158357	394.307266	5.287462
4.200160	408.181005	5.292467
4.279640	399.391397	5.297472
4.286432	395.234315	5.302477
3.994136	408.219214	5.307482
4.154540	388.691215	5.312486
3.875221	402.092862	5.317491
3.860935	403.737741	5.322496
4.138544	398.821429	5.327501
4.013055	410.227578	5.332506
4.786126	418.290032	5.337510
4.471204	414.558343	5.342515
3.855465	406.044725	5.347520
4.593663	403.199574	5.352525
4.279006	416.913996	5.357530
4.465264	400.287464	5.362534
4.333178	409.577026	5.367539
4.451583	406.511489	5.372544
4.296475	393.311704	5.377549
4.164877	396.123844	5.382554
4.542094	415.907666	5.387558
4.388626	420.939267	5.392563
4.319155	414.721696	5.397568
4.620425	411.566252	5.402573
4.580910	413.825989	5.407578
4.379447	387.352632	5.412582
4.020238	407.375936	5.417587
4.366314	411.552892	5.422592
4.367850	420.141025	5.427597
4.431917	428.967150	5.432602
4.681102	418.989573	5.437606
4.393869	427.808735	5.442611
4.440842	424.923506	5.447616
4.802000	428.242418	5.452621
4.403992	428.004792	5.457626
4.664595	426.545277	5.462630
4.577710	428.862863	5.467635
4.681241	427.936206	5.472640
4.807708	422.538653	5.477645
4.520580	427.371450	5.482650
4.533699	434.028136	5.487654
4.640968	427.119264	5.492659
4.187342	428.281306	5.497664
4.931300	421.172708	5.502669
4.532045	436.849315	5.507674
4.662604	433.219121	5.512678
4.621291	427.366167	5.517683
4.863582	435.164727	5.522688
4.672779	418.038434	5.527693
4.305617	427.799960	5.532698
4.909053	424.833527	5.537702
4.347396	427.125980	5.542707
4.572878	432.982386	5.547712
4.843356	442.060319	5.552717
4.784761	445.497928	5.557722
4.531497	468.188076	5.562726
4.926029	457.913468	5.567731
4.975797	465.775331	5.572736
5.010034	459.558757	5.577741
4.946022	459.730910	5.582746
5.267894	447.991215	5.587750
4.846390	431.398883	5.592755
4.479017	443.392084	5.597760
5.041724	454.647445	5.602765
4.995796	455.785920	5.607770
5.036735	456.626597	5.612774
5.203986	470.074672	5.617779
5.333937	461.628699	5.622784
5.016836	435.378787	5.627789
4.561199	435.125329	5.632794
4.759437	445.605482	5.637798
4.964657	446.783747	5.642803
4.896159	457.896873	5.647808
5.108721	459.425344	5.652813
4.678177	462.585534	5.657818
4.958765	466.543948	5.662822
4.953213	468.660651	5.667827
5.088202	460.230420	5.672832
5.179302	459.653189	5.677837
5.040611	463.969068	5.682842
5.123152	457.872570	5.687846
5.202085	453.736798	5.692851
4.868245	476.117268	5.697856
5.038635	458.671674	5.702861
5.143729	467.488772	5.707866
5.458668	461.794079	5.712870
5.340354	464.558752	5.717875
5.384331	464.301460	5.722880
5.301766	461.667206	5.727885
5.278660	476.355398	5.732890
5.215355	466.851388	5.737894
5.268717	473.729735	5.742899
5.112048	470.860884	5.747904
5.113014	464.058256	5.752909
5.115204	468.467468	5.757914
5.212589	464.105185	5.762918
4.836382	467.807301	5.767923
5.441379	483.516499	5.772928
5.435886	494.467011	5.777933
5.052902	505.886777	5.782938
5.335683	503.973809	5.787942
5.682264	499.421855	5.792947
5.402377	499.018497	5.797952
5.463232	495.501327	5.802957
5.416279	506.161541	5.807962
5.337489	500.355991	5.812966
5.339099	493.853261	5.817971
5.354960	506.872856	5.822976
5.413489	508.472366	5.827981
5.483905	510.867167	5.832986
5.608894	495.278080	5.837990
5.715670	500.909950	5.842995
5.283433	511.095954	5.848000
5.561062	509.021741	5.853005
5.144191	508.037727	5.858010
5.394127	508.718377	5.863014
5.018931	515.030824	5.868019
5.374863	509.377978	5.873024
5.741200	519.194946	5.878029
5.505541	541.981543	5.883034
5.813117	538.199638	5.888038
5.701789	533.566676	5.893043
5.432660	545.549640	5.898048
6.064545	542.516528	5.903053
5.814337	523.280758	5.908058
5.688418	512.068050	5.913062
5.733089	514.266831	5.918067
5.374787	511.873971	5.923072
5.771144	529.435467	5.928077
5.586986	538.574181	5.933082
5.866113	536.143858	5.938086
5.817423	549.117033	5.943091
5.673069	543.206279	5.948096
6.037168	535.698583	5.953101
5.952781	536.142947	5.958106
6.005153	535.279691	5.963110
5.839174	539.185539	5.968115
5.754441	542.065138	5.973120
5.804395	525.422123	5.978125
5.753964	540.077500	5.983130
5.854113	534.395385	5.988134
5.797089	542.784307	5.993139
5.813024	532.743780	5.998144
5.920696	537.336449	6.003149
5.419220	540.553956	6.008154
5.825287	534.480326	6.013158
5.714346	531.490253	6.018163
5.523345	543.666599	6.023168
5.585263	543.637892	6.028173
5.476368	552.211198	6.033178
5.847129	545.765636	6.038182
6.143009	557.792474	6.043187
6.262981	550.125134	6.048192
6.143595	552.599649	6.053197
5.852085	556.739446	6.058202
6.137982	555.525936	6.063206
6.125085	564.945067	6.068211
5.700433	573.198821	6.073216
6.246718	558.027619	6.078221
5.848352	567.251374	6.083226
5.955299	572.306191	6.088230
6.118520	567.637122	6.093235
5.834416	565.654250	6.098240
6.095079	561.557479	6.103245
5.885882	571.978469	6.108250
6.036550	572.941508	6.113254
5.863681	551.270764	6.118259
6.044337	566.400408	6.123264
6.084544	563.570336	6.128269
5.980608	566.223140	6.133274
6.127110	571.586337	6.138278
6.081925	576.061321	6.143283
5.795260	569.033585	6.148288
6.042132	566.708725	6.153293
5.663563	574.623570	6.158298
5.802275	569.479368	6.163302
5.864254	564.258069	6.168307
6.191307	569.214652	6.173312
6.196203	559.325992	6.178317
5.532502	571.199851	6.183322
6.033129	557.951941	6.188326
6.176444	560.813491	6.193331
5.979477	562.267482	6.198336
6.210174	563.730911	6.203341
6.119524	572.389908	6.208346
6.283806	569.300972	6.213350
6.273504	560.128122	6.218355
6.270162	580.250794	6.223360
6.348148	568.307625	6.228365
6.242147	573.133030	6.233370
6.476805	569.551999	6.238374
6.226333	566.332905	6.243379
5.972697	580.021406	6.248384
6.378386	564.003562	6.253389
6.217790	559.752254	6.258394
6.290296	541.449419	6.263398
5.734175	540.765051	6.268403
5.870289	545.932244	6.273408
6.102613	543.654977	6.278413
5.860863	542.522349	6.283418
6.128350	559.640595	6.288422
6.095216	561.156205	6.293427
5.883260	562.371158	6.298432
6.389765	558.385991	6.303437
5.740928	556.024561	6.308442
6.100813	549.166036	6.313446
6.044951	553.563260	6.318451
6.277916	564.340142	6.323456
6.513419	552.149369	6.328461
6.225013	542.339969	6.333466
6.072404	541.287618	6.338470
5.964835	535.739474	6.343475
5.888956	537.634580	6.348480
6.112828	525.216173	6.353485
6.159116	546.639199	6.358490
6.140248	536.420523	6.363494
6.537733	555.144646	6.368499
5.966694	538.176456	6.373504
6.373220	536.507537	6.378509
6.090114	538.111316	6.383514
6.011498	543.836289	6.388518
5.996430	546.983481	6.393523
5.852512	545.511876	6.398528
5.940961	549.270808	6.403533
5.651541	551.836464	6.408538
5.792127	539.071312	6.413542
6.035263	542.724472	6.418547
5.869556	543.031623	6.423552
6.049550	530.478198	6.428557
5.614668	544.033240	6.433562
5.959678	538.036885	6.438566
5.829076	536.150986	6.443571
6.049042	564.392700	6.448576
5.964691	567.651878	6.453581
5.718755	564.892177	6.458586
5.848981	555.711301	6.463590
5.699541	567.706370	6.468595
5.792831	574.966976	6.473600
6.198502	560.887873	6.478605
6.157812	567.477740	6.483610
6.058835	548.592144	6.488614
5.967207	563.193774	6.493619
5.926554	562.396994	6.498624
6.420782	554.703124	6.503629
6.374615	567.359500	6.508634
6.364986	562.584329	6.513638
6.189272	570.084631	6.518643
5.973759	551.826913	6.523648
6.095501	543.708810	6.528653
6.174011	554.557874	6.533658
6.121003	563.554963	6.538662
5.997681	548.727061	6.543667
5.862603	545.653859	6.548672
6.041460	541.518323	6.553677
5.779281	551.257447	6.558682
6.042925	563.999463	6.563686
6.243611	573.962033	6.568691
6.046582	574.232925	6.573696
6.143597	570.431545	6.578701
5.879057	558.886739	6.583706
6.132964	563.113991	6.588710
6.031891	565.570881	6.593715
6.368130	575.416044	6.598720
6.080523	552.603641	6.603725
5.719427	551.257013	6.608730
6.022352	559.302918	6.613734
6.048043	546.592263	6.618739
5.985518	560.129591	6.623744
6.127976	558.232800	6.628749
5.804945	557.538819	6.633754
6.134026	568.985200	6.638758
6.264911	567.412242	6.643763
6.110485	569.432310	6.648768
6.143086	554.538580	6.653773
5.739090	548.388470	6.658778
5.949197	550.449912	6.663782
6.362506	564.641544	6.668787
6.059525	558.747921	6.673792
6.169114	542.270250	6.678797
6.102523	545.073352	6.683802
5.925835	545.125215	6.688806
6.002946	543.750865	6.693811
5.744334	554.141236	6.698816
6.087697	535.022734	6.703821
5.815565	548.368270	6.708826
5.880720	556.503089	6.713830
6.102072	561.288503	6.718835
5.824285	569.495589	6.723840
6.003579	550.354358	6.728845
6.045973	562.695978	6.733850
5.999951	571.946455	6.738854
6.289553	574.681130	6.743859
5.921355	585.050267	6.748864
6.231829	560.622442	6.753869
5.983179	571.217867	6.758874
6.101514	575.592625	6.763878
6.143615	569.573504	6.768883
5.796685	574.172641	6.773888
6.296901	570.793583	6.778893
6.182649	569.951841	6.783898
6.218759	562.809303	6.788902
6.010271	555.901448	6.793907
5.577758	558.855096	6.798912
6.333286	563.230907	6.803917
5.935529	561.969361	6.808922
6.060822	566.000426	6.813926
5.942629	573.999512	6.818931
5.925559	580.180685	6.823936
6.088769	576.804041	6.828941
5.646832	574.592415	6.833946
5.735077	576.747993	6.838950
5.801716	579.127446	6.843955
5.632176	587.472534	6.848960
5.623818	569.935101	6.853965
5.885208	572.385862	6.858970
5.662594	582.419376	6.863974
5.740083	582.066272	6.868979
5.925501	590.618884	6.873984
6.412995	595.040477	6.878989
6.060571	590.114565	6.883994
5.872331	585.357754	6.888998
6.146728	584.674458	6.894003
6.077319	579.956023	6.899008
5.795003	562.514876	6.904013
6.000870	586.937535	6.909018
6.019602	603.894885	6.914022
6.120477	595.200584	6.919027
6.052913	600.434899	6.924032
6.494179	587.885114	6.929037
6.061981	591.315730	6.934042
5.928511	578.476555	6.939046
6.091340	560.695571	6.944051
5.868559	571.618114	6.949056
5.889478	580.163177	6.954061
5.805608	580.780208	6.959066
6.200259	595.190519	6.964070
6.642127	590.655153	6.969075
6.231573	588.064029	6.974080
6.197162	574.621668	6.979085
6.033055	573.140768	6.984090
6.247819	564.959433	6.989094
6.405815	575.538866	6.994099
5.843442	581.777003	6.999104
6.061227	571.249760	7.004109
5.864749	570.687885	7.009114
6.089518	570.297025	7.014118
6.031086	573.805867	7.019123
6.127856	574.200367	7.024128
5.879055	572.912923	7.029133
6.018587	575.450614	7.034138
5.691719	569.096945	7.039142
6.267199	575.029939	7.044147
5.598378	573.623664	7.049152
6.164220	567.705248	7.054157
5.733718	570.479995	7.059162
5.882753	578.060317	7.064166
6.106232	574.524246	7.069171
6.082504	584.418738	7.074176
6.051843	570.074912	7.079181
6.006677	571.335112	7.084186
6.180712	574.505322	7.089190
6.064440	578.636885	7.094195
6.114769	574.811549	7.099200
6.382810	578.342113	7.104205
5.957884	575.854097	7.109210
6.206848	567.171745	7.114214
5.920337	574.573449	7.119219
5.867832	571.015898	7.124224
6.017237	571.661170	7.129229
6.196512	572.949199	7.134234
6.451443	579.130708	7.139238
6.279331	577.984596	7.144243
5.701048	581.874137	7.149248
6.182490	576.340620	7.154253
6.008964	576.063823	7.159258
5.754634	573.591321	7.164262
6.018223	576.535012	7.169267
5.492436	581.844845	7.174272
5.767779	569.209826	7.179277
5.681684	585.947897	7.184282
5.978099	596.528247	7.189286
6.487450	605.762244	7.194291
6.253439	598.001837	7.199296
6.180382	576.179401	7.204301
6.059856	584.526155	7.209306
5.892188	584.297324	7.214310
6.039135	582.293336	7.219315
5.695985	585.308978	7.224320
6.133614	592.611545	7.229325
6.033744	595.159401	7.234330
6.005303	608.369217	7.239334
6.207876	597.942832	7.244339
6.347963	597.089643	7.249344
6.195836	577.776132	7.254349
6.182696	580.552156	7.259354
6.419706	570.221322	7.264358
6.483155	572.335615	7.269363
5.921997	578.643992	7.274368
6.188040	568.945103	7.279373
6.152620	570.418373	7.284378
5.825789	570.700652	7.289382
6.059025	569.594008	7.294387
6.035837	572.613107	7.299392
6.248034	566.410590	7.304397
6.052265	579.753893	7.309402
6.146353	572.099501	7.314406
5.965748	562.467618	7.319411
5.908233	576.062538	7.324416
5.861074	567.909981	7.329421
5.910823	577.714486	7.334426
6.046618	564.877393	7.339430
5.891894	566.710848	7.344435
5.958985	576.692537	7.349440
6.016903	566.151562	7.354445
5.809141	578.223957	7.359450
5.705503	577.237800	7.364454
6.093057	566.384262	7.369459
6.019609	590.096078	7.374464
6.026379	576.092351	7.379469
6.007251	573.597655	7.384474
5.772058	580.697570	7.389478
6.066020	575.869759	7.394483
5.826693	573.615180	7.399488
6.098845	571.552717	7.404493
6.037986	565.035418	7.409498
6.052454	554.667377	7.414502
6.230319	567.332509	7.419507
6.016953	570.683844	7.424512
5.986806	564.167982	7.429517
6.074740	573.168620	7.434522
5.983110	578.531115	7.439526
6.146152	571.264599	7.444531
5.955385	580.217276	7.449536
6.372374	567.477162	7.454541
6.010027	577.904818	7.459546
5.927338	573.864586	7.464550
6.431965	581.651045	7.469555
5.889433	575.993727	7.474560
5.872069	571.464208	7.479565
6.066573	566.888135	7.484570
6.323783	569.298052	7.489574
6.327660	568.921793	7.494579
6.048441	562.405359	7.499584
6.078082	566.340154	7.504589
6.058501	569.312287	7.509594
5.683735	575.927865	7.514598
5.948500	575.496950	7.519603
5.979114	577.000449	7.524608
6.152414	573.953926	7.529613
6.179537	575.010290	7.534618
6.116718	581.022821	7.539622
6.327100	575.020285	7.544627
6.215126	563.715357	7.549632
6.473350	574.151352	7.554637
6.488919	574.226989	7.559642
6.230334	577.244440	7.564646
6.264274	561.915892	7.569651
6.028431	570.318692	7.574656
5.858591	561.269581	7.579661
6.009611	556.280314	7.584666
6.177636	563.456643	7.589670
6.278974	549.281138	7.594675
5.966511	553.611255	7.599680
6.021063	536.375224	7.604685
5.939268	549.466932	7.609690
5.907951	547.592150	7.614694
6.273787	557.215461	7.619699
6.124437	567.479261	7.624704
6.132836	551.645966	7.629709
5.830132	553.301821	7.634714
5.759890	558.768609	7.639718
5.952283	567.590675	7.644723
5.873880	570.761953	7.649728
6.213515	565.897888	7.654733
6.172781	574.785022	7.659738
5.952024	576.265834	7.664742
6.314367	576.519960	7.669747
6.004952	558.702771	7.674752
5.999678	559.759456	7.679757
6.067166	557.984466	7.684762
5.932474	559.428264	7.689766
6.157113	556.046208	7.694771
6.069765	567.351557	7.699776
5.852863	560.761586	7.704781
5.757632	560.743950	7.709786
5.993943	564.220165	7.714790
6.047167	567.801912	7.719795
5.950939	578.855185	7.724800
6.020528	574.216485	7.729805
6.317552	574.949439	7.734810
6.337771	574.035850	7.739814
5.926914	557.562380	7.744819
5.637774	563.210962	7.749824
5.891538	566.379045	7.754829
6.269880	566.297061	7.759834
5.915457	573.006454	7.764838
6.300241	565.712867	7.769843
6.300543	577.127457	7.774848
6.173649	570.580223	7.779853
5.869117	567.037289	7.784858
5.957294	566.108425	7.789862
6.133045	560.303015	7.794867
6.089918	571.221619	7.799872
5.890420	571.091577	7.804877
6.053234	573.732662	7.809882
6.180717	577.633632	7.814886
6.036131	577.493430	7.819891
5.973267	576.880666	7.824896
6.126436	570.549386	7.829901
5.760305	564.081153	7.834906
6.156769	570.964704	7.839910
6.347300	557.746630	7.844915
6.047620	558.963943	7.849920
5.887895	547.337499	7.854925
6.101085	550.785468	7.859930
5.967711	550.231614	7.864934
5.911906	555.498402	7.869939
6.075173	570.202057	7.874944
6.017526	573.159861	7.879949
6.419491	566.928451	7.884954
5.967155	570.591474	7.889958
6.232963	557.743656	7.894963
5.875873	550.007263	7.899968
5.799989	552.547497	7.904973
5.868728	549.196730	7.909978
5.856541	571.246659	7.914982
6.456932	572.267880	7.919987
6.052638	572.941116	7.924992
6.299712	561.066794	7.929997
6.404430	545.913918	7.935002
5.378893	547.281567	7.940006
6.002267	548.219567	7.945011
6.139091	566.333465	7.950016
6.549233	559.824759	7.955021
6.008256	560.418274	7.960026
6.179788	551.125010	7.965030
5.968370	547.380426	7.970035
5.642169	559.459059	7.975040
6.063611	546.345101	7.980045
6.037157	550.489833	7.985050
5.920019	547.008971	7.990054
6.094333	540.513297	7.995059
5.838835	548.734349	8.000064
5.778127	541.032052	8.005069
5.712708	565.008978	8.010074
5.854641	566.776342	8.015078
6.152638	575.915611	8.020083
6.114411	586.422900	8.025088
6.205025	576.701989	8.030093
6.096759	584.959504	8.035098
6.048184	578.315465	8.040102
6.305660	567.159755	8.045120
5.864668	579.852466	8.050138
6.279897	568.198706	8.055155
6.295249	571.085656	8.060173
5.748269	566.012723	8.065190
6.225336	562.081539	8.070208
6.035955	573.461253	8.075226
6.059803	572.694142	8.080243
5.862649	555.793879	8.085261
5.776081	577.989395	8.090278
6.313623	585.752801	8.095296
6.081876	583.115000	8.100314
5.988081	575.247116	8.105331
5.988934	582.297983	8.110349
6.032741	584.354404	8.115366
6.279575	578.912242	8.120384
6.093263	575.786513	8.125402
6.276931	569.402905	8.130419
6.081595	580.903862	8.135437
5.603512	573.494290	8.140454
5.890594	576.058240	8.145472
5.819710	576.396244	8.150490
6.287761	581.992606	8.155507
6.259921	581.014885	8.160525
6.016478	583.063962	8.165542
6.298968	576.689311	8.170560
6.257313	582.973038	8.175578
6.216484	572.426826	8.180595
6.378118	571.131924	8.185613
6.005334	588.890365	8.190630
6.507683	572.722853	8.195648
6.075798	577.021647	8.200666
6.073236	564.767273	8.205683
6.321487	578.795711	8.210701
6.195186	579.485820	8.215718
6.422401	590.099393	8.220736
6.325752	579.560433	8.225754
6.265438	581.051296	8.230771
6.373005	580.924164	8.235789
6.189963	585.879148	8.240806
6.354414	589.217259	8.245824
6.102569	591.915143	8.250842
6.241060	578.316535	8.255859
6.237267	585.093420	8.260877
6.104516	581.885328	8.265894
5.966938	578.996184	8.270912
6.101313	574.493694	8.275930
6.262689	591.075883	8.280947
6.202894	575.566807	8.285965
5.982207	590.188399	8.290982
6.476303	582.075260	8.296000
6.132921	580.400808	8.301018
6.213394	563.145168	8.306035
6.294429	569.201469	8.311053
6.258710	581.432401	8.316070
6.352456	568.229509	8.321088
6.205972	579.470175	8.326106
6.001861	579.787093	8.331123
6.083322	583.288200	8.336141
6.560739	612.527316	8.341158
6.398145	600.806547	8.346176
6.297213	616.469496	8.351194
6.154899	618.530404	8.356211
6.599722	612.588375	8.361229
6.294494	616.051637	8.366246
6.463053	606.808543	8.371264
6.585632	617.954981	8.376282
6.665915	600.352152	8.381299
6.083142	597.687135	8.386317
6.188177	590.270056	8.391334
6.554356	593.801462	8.396352
6.664906	602.508011	8.401370
6.157723	590.226790	8.406387
6.443346	592.459157	8.411405
6.303261	605.767885	8.416422
6.909985	595.507193	8.421440
6.420791	592.848363	8.426458
5.943992	602.567548	8.431475
6.136058	594.586286	8.436493
6.565023	604.087598	8.441510
6.774812	612.490405	8.446528
6.625714	610.523459	8.451546
6.560773	587.868031	8.456563
6.164691	589.104104	8.461581
6.101850	593.470732	8.466598
6.178060	599.206543	8.471616
6.550362	595.685700	8.476634
6.477980	601.153799	8.481651
6.327203	609.997319	8.486669
6.505526	603.445911	8.491686
6.559981	602.085564	8.496704
6.563121	609.804346	8.501722
6.774089	597.347466	8.506739
6.778273	601.894520	8.511757
6.261085	609.541048	8.516774
6.596385	607.084781	8.521792
6.696063	603.651205	8.526810
6.888670	610.746563	8.531827
6.959721	603.634939	8.536845
6.259715	589.749176	8.541862
6.260593	598.034165	8.546880
6.478490	609.731274	8.551898
6.415463	617.875287	8.556915
6.563841	605.190894	8.561933
6.578041	610.776849	8.566951
6.573565	604.283203	8.571968
6.461650	616.556573	8.576986
6.417700	609.785052	8.582003
6.770425	620.032201	8.587021
6.723447	610.853163	8.592039
6.873891	620.474513	8.597056
6.871041	607.383300	8.602074
6.590438	613.913180	8.607091
6.874234	613.191676	8.612109
6.936912	615.905884	8.617127
6.416531	610.585181	8.622144
6.829929	613.789459	8.627162
6.396789	626.664833	8.632179
6.822375	616.170133	8.637197
6.358330	616.737350	8.642215
6.618930	609.195360	8.647232
6.409826	600.861962	8.652250
6.286887	605.359270	8.657267
6.697193	600.212369	8.662285
6.501703	609.720044	8.667303
6.626813	604.314718	8.672320
6.822001	613.539569	8.677338
6.182482	613.241166	8.682355
6.506456	611.730885	8.687373
6.187848	616.710841	8.692391
6.410942	628.797879	8.697408
6.361157	622.602211	8.702426
6.089109	633.019826	8.707443
6.686158	632.647565	8.712461
6.779457	642.694535	8.717479
6.985868	642.545951	8.722496
7.121159	641.107884	8.727514
6.511179	648.508397	8.732531
6.851101	635.552213	8.737549
6.799622	646.227231	8.742567
6.336894	639.712760	8.747584
6.745935	638.072496	8.752602
6.694404	652.006965	8.757619
6.748233	642.375503	8.762637
6.663194	646.355531	8.767655
6.608746	634.825784	8.772672
6.560426	630.541426	8.777690
6.485120	642.983537	8.782707
6.949291	654.143814	8.787725
6.881359	671.945854	8.792743
6.746440	676.154369	8.797760
7.278061	674.773813	8.802778
6.893745	662.312023	8.807795
6.966116	640.801723	8.812813
6.914027	646.043395	8.817831
6.846608	638.270315	8.822848
6.997485	635.789215	8.827866
6.841836	650.740704	8.832883
7.100234	633.502228	8.837901
6.588495	631.938057	8.842919
6.751427	636.943936	8.847936
6.742434	648.420939	8.852954
6.545531	674.058607	8.857971
6.981826	671.183056	8.862989
7.138213	682.608842	8.868007
6.922717	674.740353	8.873024
7.109257	683.081305	8.878042
6.908197	687.992753	8.883059
7.270998	680.113622	8.888077
7.181153	672.617900	8.893095
6.919823	658.211043	8.898112
6.795870	645.804747	8.903130
7.021082	662.950276	8.908147
7.044106	667.566172	8.913165
7.144558	666.773998	8.918183
7.082027	655.091859	8.923200
7.177862	640.630917	8.928218
6.680543	647.738157	8.933235
6.765133	649.680092	8.938253
7.131645	652.708597	8.943271
7.389986	671.799780	8.948288
7.267948	659.034265	8.953306
6.705811	647.672346	8.958323
7.204946	644.645891	8.963341
7.356667	644.383434	8.968359
7.044668	646.341604	8.973376
6.989448	637.887203	8.978394
6.868504	649.217285	8.983411
7.200489	643.201683	8.988429
6.983399	635.522124	8.993447
6.919653	637.124858	8.998464
7.093493	653.581751	9.003482
7.176448	663.404304	9.008499
7.160958	646.575378	9.013517
7.130057	647.055076	9.018535
7.058044	645.924148	9.023552
7.222664	656.638646	9.028570
6.882710	656.761518	9.033587
7.044980	666.903878	9.038605
7.445998	669.473125	9.043623
7.290115	661.253712	9.048640
7.136196	643.381522	9.053658
6.846942	655.387826	9.058675
7.269785	663.675940	9.063693
7.471715	670.000734	9.068711
6.816056	661.086985	9.073728
7.359563	665.223535	9.078746
7.138004	677.349649	9.083763
7.274516	684.872150	9.088781
7.548631	676.566418	9.093799
7.067499	657.875214	9.098816
6.977920	646.478700	9.103834
6.764140	673.207341	9.108851
7.132390	676.782905	9.113869
7.127549	672.113860	9.118887
6.871193	681.008621	9.123904
7.316886	680.745115	9.128922
7.298938	680.992597	9.133939
7.209022	677.102530	9.138957
7.396236	682.833019	9.143975
7.561287	689.398616	9.148992
7.571285	675.598460	9.154010
7.235794	680.403305	9.159027
7.528418	682.841872	9.164045
7.328155	673.192548	9.169063
7.397145	682.555202	9.174080
7.483684	688.538507	9.179098
7.425024	672.580310	9.184115
7.265984	658.969687	9.189133
7.378770	654.432954	9.194151
7.040788	657.609172	9.199168
7.391527	655.924318	9.204186
7.311175	675.693803	9.209203
7.613251	668.579300	9.214221
7.731822	681.983809	9.219239
7.165430	661.805388	9.224256
7.417388	649.237676	9.229274
7.151636	648.207157	9.234291
7.061423	668.293459	9.239309
7.305965	668.869543	9.244327
7.121203	688.190831	9.249344
7.217318	672.670949	9.254362
7.546509	680.109057	9.259379
7.111169	684.869490	9.264397
7.291427	678.565717	9.269415
7.528805	688.726187	9.274432
7.267996	678.933152	9.279450
7.090770	678.571539	9.284467
7.334113	688.594433	9.289485
7.405839	683.003054	9.294503
7.207172	683.016964	9.299520
7.374273	671.215876	9.304538
7.021216	678.474653	9.309555
7.316796	696.461291	9.314573
7.512413	698.362251	9.319591
7.742230	712.348196	9.324608
7.696984	713.579148	9.329626
7.421538	700.211307	9.334643
7.291123	715.399491	9.339661
7.771018	708.461552	9.344679
7.473226	710.193406	9.349696
7.730860	710.327742	9.354714
7.565459	694.273894	9.359731
7.399007	698.253022	9.364749
7.665058	687.223716	9.369767
7.324961	694.237981	9.374784
7.381023	702.206383	9.379802
7.617422	712.578705	9.384819
7.328156	717.605704	9.389837
7.328377	715.441266	9.394855
7.551425	713.295508	9.399872
7.790509	714.829410	9.404890
7.807671	716.246175	9.409907
7.571153	711.295579	9.414925
7.676627	707.346448	9.419943
7.586331	711.979312	9.424960
7.396898	712.627015	9.429978
7.343139	710.861782	9.434995
7.426874	711.555763	9.440013
7.355309	698.616649	9.445031
7.106780	714.727928	9.450048
6.922913	710.757234	9.455066
7.365915	721.248935	9.460083
7.413122	743.587809	9.465101
7.713651	738.500040	9.470119
7.253312	738.851627	9.475136
7.744791	738.207688	9.480154
7.425205	737.034314	9.485171
7.523861	733.243264	9.490189
7.584852	725.159995	9.495207
7.627878	748.746884	9.500224
7.637342	743.069431	9.505242
7.801222	739.009084	9.510259
7.526020	745.618625	9.515277
7.882543	736.762231	9.520295
7.624729	748.500171	9.525312
7.929302	736.649845	9.530330
7.941283	747.186614	9.535347
7.538064	749.057625	9.540365
7.510573	751.683823	9.545383
7.707973	758.196179	9.550400
7.987480	767.473417	9.555418
8.191792	780.046270	9.560435
7.532949	762.917797	9.565453
7.704416	748.634083	9.570471
7.634521	763.050736	9.575488
7.993770	769.775679	9.580506
8.125607	771.347386	9.585523
7.640387	771.245587	9.590541
7.819156	768.788886	9.595559
8.039989	773.496907	9.600576
8.209862	762.265664	9.605594
7.843520	756.903413	9.610611
7.674300	744.728789	9.615629
7.811558	744.126164	9.620647
7.991333	756.678255	9.625664
7.740990	754.553151	9.630682
8.181878	761.892245	9.635699
7.776567	759.300808	9.640717
7.866805	754.275141	9.645735
8.141167	769.124194	9.650752
8.065782	757.204085	9.655770
8.253054	759.669718	9.660787
7.613465	748.657766	9.665805
8.053499	741.394077	9.670823
7.745567	744.816581	9.675840
7.994247	744.211879	9.680858
8.101500	744.881015	9.685875
8.190999	747.969585	9.690893
8.108912	751.290510	9.695911
7.791955	742.319463	9.700928
7.911206	747.064435	9.705946
7.764328	755.401873	9.710963
7.621884	764.651807	9.715981
8.321816	778.496850	9.720999
8.150710	778.715420	9.726016
8.225480	779.640078	9.731034
8.178333	776.122281	9.736051
7.820876	760.478086	9.741069
8.184359	761.424017	9.746087
8.122683	783.416144	9.751104
7.923338	777.462807	9.756122
7.899329	764.637804	9.761139
7.659743	776.099179	9.766157
8.181530	781.676106	9.771175
7.817729	781.047441	9.776192
7.828884	782.981650	9.781210
8.152753	776.231050	9.786227
7.821229	784.561326	9.791245
8.193136	766.385110	9.796263
7.993770	777.630821	9.801280
7.995098	785.551136	9.806298
8.248823	779.210088	9.811315
8.351048	777.959330	9.816333
8.180838	766.329934	9.821351
8.394452	783.566968	9.826368
7.944553	776.045966	9.831386
8.174503	779.339836	9.836403
7.720920	780.899052	9.841421
8.050992	780.963358	9.846439
8.183089	787.864405	9.851456
8.125228	779.595173	9.856474
8.401378	780.608087	9.861491
7.857004	780.795049	9.866509
8.069409	788.100370	9.871527
8.636088	799.100040	9.876544
8.221310	795.591522	9.881562
8.156621	783.681237	9.886579
8.534577	791.312978	9.891597
8.593440	781.685911	9.896615
8.130892	780.294075	9.901632
8.147029	781.037806	9.906650
8.516952	777.313808	9.911667
8.157426	787.693433	9.916685
8.231907	786.194843	9.921703
8.331992	785.962371	9.926720
8.076387	787.674764	9.931738
8.626862	793.342706	9.936755
8.394148	798.841208	9.941773
8.306676	793.471339	9.946791
8.416870	774.424446	9.951808
8.299089	782.548564	9.956826
8.560034	777.033738	9.961843
8.294179	773.611324	9.966861
8.359500	773.274380	9.971879
8.219991	776.169049	9.976896
8.218363	807.009085	9.981914
8.842684	806.976545	9.986931
8.591259	801.720366	9.991949
8.364621	784.024371	9.996967
8.210736	774.364465	10.001984
8.198094	790.418244	10.007002
8.344206	798.337273	10.012019
8.348779	814.376915	10.017037
8.256976	818.113561	10.022055
8.466663	815.865881	10.027072
8.570841	818.332855	10.032090
8.800536	811.523012	10.037107
8.576427	815.110881	10.042125
8.603427	807.343664	10.047143
8.613645	805.927332	10.052160
8.438410	804.135813	10.057178
8.617252	806.657463	10.062195
8.228657	809.258909	10.067213
8.338676	802.876453	10.072231
8.355503	799.395117	10.077248
8.050927	816.172835	10.082266
8.294853	793.840702	10.087283
8.187113	806.780739	10.092301
8.278951	811.729735	10.097319
8.430949	811.369019	10.102336
8.502488	818.777737	10.107354
8.571389	816.514844	10.112371
8.399506	832.217290	10.117389
8.270996	845.789129	10.122407
8.564794	841.046080	10.127424
8.733150	853.732398	10.132442
8.706175	849.536365	10.137459
8.628461	847.185806	10.142477
8.718175	856.306993	10.147495
8.623379	849.635978	10.152512
8.408874	858.064652	10.157530
8.700313	839.410590	10.162547
8.556466	858.416327	10.167565
8.951510	854.465854	10.172583
9.092225	851.488945	10.177600
8.687197	856.413092	10.182618
9.284288	844.230633	10.187635
9.101155	829.924255	10.192653
8.742858	822.542890	10.197671
8.915539	818.186729	10.202688
8.549521	813.602027	10.207706
8.832379	818.758787	10.212723
8.640047	812.987808	10.217741
8.432706	820.100249	10.222759
8.854548	819.420382	10.227776
8.663044	812.393676	10.232794
8.735325	819.951656	10.237811
8.807434	816.005846	10.242829
8.561579	821.704132	10.247847
8.954517	826.667143	10.252864
8.784103	849.362846	10.257882
8.962783	843.229218	10.262899
8.640678	844.597156	10.267917
8.964607	845.388140	10.272935
9.130981	835.645062	10.277952
8.606489	823.507927	10.282970
8.798044	836.652325	10.287987
8.834241	841.974143	10.293005
8.951434	849.519598	10.298023
9.071794	847.499237	10.303040
8.757235	845.700524	10.308058
9.323809	845.418714	10.313075
8.910691	840.346498	10.318093
8.727779	835.243032	10.323111
9.097729	830.527651	10.328128
8.741692	830.849899	10.333146
8.960152	843.288501	10.338163
8.828611	847.463833	10.343181
9.112986	849.367857	10.348199
8.889371	840.761381	10.353216
8.576017	846.358054	10.358234
9.002311	843.383945	10.363251
8.852320	858.980456	10.368269
8.630455	847.404901	10.373287
8.872592	843.680846	10.378304
8.894871	854.511507	10.383322
9.077999	844.498672	10.388339
9.146758	845.949041	10.393357
8.466969	853.873599	10.398375
8.609339	843.936583	10.403392
8.232180	858.143121	10.408410
8.721350	867.359104	10.413427
9.117015	877.729722	10.418445
8.987684	877.918952	10.423463
8.915062	884.385546	10.428480
8.818809	882.782801	10.433498
8.998702	887.844906	10.438515
9.182557	894.535415	10.443533
8.989545	893.290530	10.448551
9.287648	876.939461	10.453568
9.086261	895.695348	10.458586
9.136978	882.196298	10.463603
9.279085	884.104943	10.468621
8.863891	882.178195	10.473639
9.265441	875.683764	10.478656
9.279560	876.623962	10.483674
9.444619	885.087549	10.488691
9.467501	880.698457	10.493709
9.253077	890.592637	10.498727
9.170911	884.813463	10.503744
9.234199	888.830056	10.508762
9.149666	880.914824	10.513779
9.014820	883.102661	10.518797
8.971914	886.510529	10.523815
9.102421	890.415441	10.528832
8.867901	890.383119	10.533850
8.589364	885.193585	10.538867
9.019280	910.113796	10.543885
9.248365	908.043772	10.548903
9.337240	900.315782	10.553920
9.091915	920.468885	10.558938
9.127077	914.642166	10.563955
9.149738	911.541274	10.568973
8.917335	923.879968	10.573991
9.153403	910.277047	10.579008
9.012995	914.533179	10.584026
9.424170	907.443346	10.589043
9.317087	908.260881	10.594061
9.408167	920.083005	10.599079
9.511211	915.048675	10.604096
9.160294	924.779636	10.609114
9.287865	910.880130	10.614131
9.462826	909.744289	10.619149
9.393432	926.580687	10.624167
9.273461	912.269798	10.629184
9.404149	928.301806	10.634202
9.607214	934.818320	10.639219
9.782325	937.907542	10.644237
9.471724	920.889230	10.649255
9.416372	924.079712	10.654272
9.275158	922.245259	10.659290
9.687366	917.725493	10.664307
9.833316	925.574252	10.669325
9.373721	913.981249	10.674343
9.524767	915.699673	10.679360
9.571998	923.060695	10.684378
9.390200	919.447615	10.689395
9.489743	911.451957	10.694413
9.517171	917.025405	10.699431
9.292854	912.025689	10.704448
9.344484	934.022925	10.709466
9.478999	938.533189	10.714483
9.632084	952.739381	10.719501
9.579367	971.013386	10.724519
9.631944	958.193182	10.729536
9.734448	967.330626	10.734554
9.681751	969.676918	10.739571
10.075011	951.583359	10.744589
9.539007	942.895202	10.749607
9.674061	918.292873	10.754624
9.471625	923.059962	10.759642
9.333724	922.563519	10.764659
9.258229	943.555765	10.769677
9.619873	951.109292	10.774695
9.950750	948.370580	10.779712
9.630203	953.097756	10.784730
9.629414	952.145458	10.789747
9.998953	950.598388	10.794765
9.776917	960.262806	10.799783
9.480244	957.432749	10.804800
9.507466	956.959601	10.809818
9.623772	960.127431	10.814835
9.861614	956.554034	10.819853
9.791793	958.140288	10.824871
9.874007	957.006977	10.829888
9.853348	958.501459	10.834906
9.637781	957.410272	10.839923
9.593846	956.336581	10.844941
9.530446	957.731844	10.849959
9.553364	951.698704	10.854976
9.480253	959.859227	10.859994
9.529301	967.010949	10.865011
9.670027	952.572507	10.870029
9.663554	958.961283	10.875047
9.639870	956.135123	10.880064
9.814074	962.824894	10.885082
9.790725	977.614505	10.890099
10.076293	979.304211	10.895117
9.564484	982.281993	10.900135
9.731459	983.074517	10.905152
10.220783	983.163680	10.910170
9.789356	987.706074	10.915187
10.091369	988.642003	10.920205
9.876788	996.548803	10.925223
9.896513	989.630886	10.930240
9.863484	988.882306	10.935258
9.738399	999.806899	10.940275
9.999639	986.534736	10.945293
10.089774	997.880775	10.950311
10.570530	993.785809	10.955328
10.204819	990.320409	10.960346
9.795201	980.259596	10.965363
10.299426	965.718757	10.970381
10.186005	975.502418	10.975399
10.092848	964.439080	10.980416
10.075477	966.354407	10.985434
9.995623	965.337627	10.990451
9.980062	952.749124	10.995469
10.114237	956.185609	11.000487
9.921073	956.757770	11.005504
9.737861	954.015049	11.010522
10.067450	979.616409	11.015539
10.376238	980.463044	11.020557
10.033291	982.566603	11.025575
9.835665	991.806995	11.030592
10.216655	985.311586	11.035610
10.048842	991.665236	11.040627
10.464657	986.135569	11.045645
10.436997	996.327640	11.050663
10.209317	980.525085	11.055680
10.029676	975.550439	11.060698
9.923891	985.528089	11.065715
10.139440	987.119344	11.070733
10.443082	990.356404	11.075751
10.103498	991.815614	11.080768
10.296928	1000.533393	11.085786
9.980309	1001.533567	11.090803
10.271759	1006.711507	11.095821
9.795757	999.310242	11.100839
10.123178	1005.623391	11.105856
9.991097	998.533344	11.110874
9.832486	1000.165175	11.115891
10.365955	994.729036	11.120909
10.340594	993.807956	11.125927
10.482865	993.562802	11.130944
10.245213	993.821107	11.135962
10.089835	998.821152	11.140979
10.342427	988.797335	11.145997
10.432518	993.852861	11.151015
10.050648	990.708780	11.156032
10.435186	984.242111	11.161050
10.263881	998.111857	11.166067
10.279709	996.462433	11.171085
10.036008	991.898698	11.176103
9.964394	1014.323436	11.181120
10.647589	1020.159559	11.186138
10.393447	1031.097037	11.191155
10.588492	1024.968703	11.196173
10.295866	1022.997671	11.201191
10.252094	1013.092290	11.206208
10.720471	1018.215606	11.211226
10.604412	1030.405849	11.216243
10.811487	1016.860964	11.221261
10.440515	1000.064514	11.226279
10.387096	1000.642712	11.231296
10.567334	994.058052	11.236314
10.420433	1010.058668	11.241331
10.579859	1016.566879	11.246349
10.518308	1018.339931	11.251367
10.526398	1015.061533	11.256384
10.309595	1030.466141	11.261402
10.356624	1041.632160	11.266419
10.745966	1037.743598	11.271437
10.635095	1029.355158	11.276455
10.637088	1036.268664	11.281472
10.962767	1031.235295	11.286490
10.499385	1034.275742	11.291507
10.664350	1025.398683	11.296525
10.585598	1030.024321	11.301543
10.664549	1031.928660	11.306560
10.689843	1018.798200	11.311578
10.192832	1016.518478	11.316595
10.487337	1022.473156	11.321613
10.757906	1016.369544	11.326631
10.836134	1028.908130	11.331648
10.806915	1029.700603	11.336666
10.425456	1020.527290	11.341683
10.398432	1011.952394	11.346701
10.514354	1024.924048	11.351719
10.328430	1015.797154	11.356736
10.312349	1024.026226	11.361754
10.180659	1033.829869	11.366771
10.484785	1042.693330	11.371789
10.721895	1049.768350	11.376807
10.514326	1058.494366	11.381824
11.049872	1052.140685	11.386842
10.471942	1062.460735	11.391859
10.904896	1048.767882	11.396877
10.669368	1046.761628	11.401895
10.737199	1063.289520	11.406912
11.053724	1069.582846	11.411930
10.829241	1059.425255	11.416947
10.859588	1061.530316	11.421965
10.978605	1068.857304	11.426983
10.519837	1065.225994	11.432000
10.954800	1054.530169	11.437018
10.973408	1070.606433	11.442035
10.962887	1052.287007	11.447053
10.929137	1058.037323	11.452071
10.814454	1059.875056	11.457088
11.185878	1062.789759	11.462106
11.082862	1059.032350	11.467123
11.111201	1058.139001	11.472141
10.951700	1053.486738	11.477159
10.870721	1062.441010	11.482176
10.713390	1055.772366	11.487194
10.911093	1063.421926	11.492211
11.116376	1049.094361	11.497229
11.118100	1054.508156	11.502247
10.787177	1061.918745	11.507264
11.042986	1052.745599	11.512282
10.694836	1058.914545	11.517299
10.899337	1055.627890	11.522317
11.016301	1055.575076	11.527335
11.246310	1055.289245	11.532352
11.431860	1053.692464	11.537370
11.232592	1067.962894	11.542387
11.232876	1059.026034	11.547405
11.024130	1055.545702	11.552423
11.214787	1056.384702	11.557440
11.762527	1061.443352	11.562458
11.551539	1055.953863	11.567475
11.651824	1057.327991	11.572493
11.664580	1048.252287	11.577511
11.241387	1029.820599	11.582528
11.300283	1025.867964	11.587546
11.173821	1029.974012	11.592563
11.352849	1022.362933	11.597581
11.313923	1027.052844	11.602599
11.186344	1030.944347	11.607616
10.917352	1019.233757	11.612634
10.911290	1027.541872	11.617651
10.971261	1029.272800	11.622669
11.216632	1042.272675	11.627687
11.421626	1051.910867	11.632704
11.413470	1041.136136	11.637722
11.264279	1054.564552	11.642739
11.531831	1056.212959	11.647757
11.586998	1053.458776	11.652775
11.070142	1044.682765	11.657792
11.258900	1035.363648	11.662810
11.387204	1045.153266	11.667827
11.259326	1054.267031	11.672845
11.383794	1061.921214	11.677863
11.327104	1057.917604	11.682880
11.479915	1048.379455	11.687898
11.514839	1058.810201	11.692915
11.214296	1039.900825	11.697933
11.408323	1052.166989	11.702951
11.276165	1055.047603	11.707968
11.430852	1045.528237	11.712986
11.253772	1055.111871	11.718003
11.142364	1054.849788	11.723021
11.554837	1055.341354	11.728039
11.071756	1062.473198	11.733056
11.300582	1058.893592	11.738074
11.267548	1064.828999	11.743091
11.232983	1057.825550	11.748109
11.230628	1055.747106	11.753127
11.382940	1073.037107	11.758144
11.622612	1086.725059	11.763162
11.704913	1083.872110	11.768179
11.846223	1076.817348	11.773197
11.723028	1073.430338	11.778215
11.466533	1060.587315	11.783232
11.434566	1059.820055	11.788250
11.596053	1084.191496	11.793267
11.814167	1085.397162	11.798285
11.894282	1083.312959	11.803303
11.631519	1071.382436	11.808320
11.686562	1060.549027	11.813338
11.322500	1054.265082	11.818355
11.645097	1074.886849	11.823373
11.966781	1086.083092	11.828391
11.600534	1087.876193	11.833408
11.623688	1075.126885	11.838426
11.724132	1083.891175	11.843443
11.306585	1090.604982	11.848461
11.831316	1097.463230	11.853479
11.460204	1094.546645	11.858496
11.666166	1090.000291	11.863514
11.539822	1090.431119	11.868531
11.842032	1098.703485	11.873549
11.523225	1092.842097	11.878567
11.468702	1094.774011	11.883584
11.970139	1093.369477	11.888602
11.783647	1092.731868	11.893619
11.697045	1096.850635	11.898637
11.886114	1095.964773	11.903655
11.629238	1100.230755	11.908672
11.835496	1094.919311	11.913690
11.727419	1100.737232	11.918707
11.707425	1090.411794	11.923725
11.986559	1092.317897	11.928743
11.781232	1107.183563	11.933760
12.103182	1103.353358	11.938778
11.742688	1107.556359	11.943795
11.610184	1123.678906	11.948813
12.215886	1101.326304	11.953831
11.942109	1120.706930	11.958848
12.301266	1119.638849	11.963866
12.136274	1108.998239	11.968883
12.026602	1101.016979	11.973901
12.083863	1100.495365	11.978919
11.549400	1098.364514	11.983936
11.799146	1108.551560	11.988954
12.054030	1115.726217	11.993971
11.884604	1114.028666	11.998989
12.426302	1109.806689	12.004007
12.266192	1119.428300	12.009024
12.009087	1117.363997	12.014042
12.207010	1111.647689	12.019059
11.632430	1112.751906	12.024077
11.827080	1111.675977	12.029095
11.959806	1112.222630	12.034112
12.277278	1112.633456	12.039130
12.287956	1107.341732	12.044147
12.213183	1107.527067	12.049165
12.510093	1097.126622	12.054183
12.191872	1113.582360	12.059200
12.224261	1107.189776	12.064218
12.357930	1109.486988	12.069235
12.055205	1113.276176	12.074253
12.210250	1119.747760	12.079271
12.113067	1118.279966	12.084288
12.244631	1112.321708	12.089306
12.276042	1108.045495	12.094323
12.056047	1121.606321	12.099341
12.445777	1121.269886	12.104359
12.491985	1122.233925	12.109376
12.562977	1117.759072	12.114394
12.530452	1117.518789	12.119411
12.278448	1119.171183	12.124429
12.542066	1116.927734	12.129447
12.250450	1120.097860	12.134464
12.190256	1115.679917	12.139482
12.326290	1115.984920	12.144499
11.983717	1118.468297	12.149517
12.387921	1110.826458	12.154535
12.221569	1115.917907	12.159552
12.021303	1123.748992	12.164570
12.155779	1114.332318	12.169587
12.165687	1117.202261	12.174605
12.577562	1130.366989	12.179623
12.755669	1126.061412	12.184640
12.930903	1128.969578	12.189658
13.118379	1112.058284	12.194675
12.685005	1103.643189	12.199693
13.088250	1098.409608	12.204711
12.855791	1100.969062	12.209728
13.002357	1097.079862	12.214746
12.967905	1090.221239	12.219763
12.982313	1081.822303	12.224781
12.734847	1076.597259	12.229799
12.849153	1082.163103	12.234816
12.797402	1080.213469	12.239834
12.753185	1078.611749	12.244851
12.555608	1071.559455	12.249869
12.635870	1081.335385	12.254887
12.677813	1084.310444	12.259904
12.402278	1086.960467	12.264922
12.992634	1081.822723	12.269939
12.764284	1084.197863	12.274957
12.987729	1074.149481	12.279975
12.941976	1080.916197	12.284992
12.470301	1082.205738	12.290010
12.540729	1078.903445	12.295027
12.344066	1067.286557	12.300045
12.626028	1066.817365	12.305063
12.568976	1078.621182	12.310080
12.504510	1079.722781	12.315098
12.366380	1069.395426	12.320115
12.473832	1084.074759	12.325133
12.880003	1083.627356	12.330151
12.811317	1093.347409	12.335168
12.816340	1096.623210	12.340186
13.076840	1093.065130	12.345203
12.866088	1099.297002	12.350221
13.155392	1100.739686	12.355239
12.899925	1111.135398	12.360256
12.986873	1096.155006	12.365274
12.812497	1095.915727	12.370291
12.908189	1102.024334	12.375309
12.881154	1104.912976	12.380327
13.072655	1110.834520	12.385344
12.724958	1101.368223	12.390362
12.943515	1086.644789	12.395379
12.925120	1092.654941	12.400397
12.773961	1097.617121	12.405415
12.862072	1100.588097	12.410432
12.746960	1097.032448	12.415450
13.039723	1093.870746	12.420467
12.745579	1106.592959	12.425485
12.817334	1104.776629	12.430503
12.860157	1106.737136	12.435520
12.627655	1107.772621	12.440538
12.944359	1106.169317	12.445555
12.900311	1128.157449	12.450573
12.838904	1131.299179	12.455591
13.168800	1145.000812	12.460608
13.083090	1137.593439	12.465626
13.285095	1134.912993	12.470643
13.190855	1136.932566	12.475661
13.412099	1132.446460	12.480679
13.412355	1139.447491	12.485696
13.083694	1138.655645	12.490714
13.283019	1126.999649	12.495731
13.765763	1122.450454	12.500749
13.720796	1109.903683	12.505767
13.385653	1104.941702	12.510784
12.998821	1100.403555	12.515802
13.205611	1097.467640	12.520819
13.053157	1099.939673	12.525837
12.794467	1089.147853	12.530855
13.254334	1116.396552	12.535872
13.396227	1127.218858	12.540890
13.586763	1129.517895	12.545907
12.979741	1131.126020	12.550925
13.044920	1125.919363	12.555943
13.360207	1129.644217	12.560960
13.519836	1129.809122	12.565978
13.624985	1119.683423	12.570995
13.616238	1129.197363	12.576013
13.440238	1133.008325	12.581031
13.315813	1128.939326	12.586048
13.480338	1133.767474	12.591066
13.346939	1133.757213	12.596083
13.345144	1136.553711	12.601101
13.337155	1136.335944	12.606119
13.401604	1134.462559	12.611136
13.141865	1137.657928	12.616154
13.709506	1131.014309	12.621171
13.669255	1130.716847	12.626189
13.530936	1137.524077	12.631207
13.793713	1134.650940	12.636224
13.159180	1133.430382	12.641242
13.403753	1133.655451	12.646259
13.723249	1141.496111	12.651277
13.393116	1125.128537	12.656295
13.104732	1124.670141	12.661312
13.584228	1134.897966	12.666330
13.441693	1127.745620	12.671347
13.469407	1129.388990	12.676365
13.603221	1152.452911	12.681383
13.849879	1151.427824	12.686400
13.928041	1156.120273	12.691418
13.931221	1136.753759	12.696435
13.515464	1125.805417	12.701453
13.615047	1124.111829	12.706471
14.038793	1134.875557	12.711488
13.846083	1138.886495	12.716506
13.852511	1130.814195	12.721523
13.762057	1127.096025	12.726541
13.645456	1132.792157	12.731559
13.971523	1129.405882	12.736576
13.899007	1121.400758	12.741594
13.745481	1112.142291	12.746611
13.810222	1128.585147	12.751629
13.856271	1139.965737	12.756647
13.967774	1131.020691	12.761664
13.831274	1140.795674	12.766682
13.659767	1138.751273	12.771699
13.846382	1155.893397	12.776717
13.907318	1152.667055	12.781735
14.219761	1165.472120	12.786752
13.969833	1173.513376	12.791770
14.155337	1156.411836	12.796787
14.215435	1168.125704	12.801805
13.752100	1163.450006	12.806823
13.911330	1147.687066	12.811840
13.850584	1168.268976	12.816858
13.971100	1158.068873	12.821875
14.223073	1162.026803	12.826893
13.875141	1159.271901	12.831911
14.164703	1159.690489	12.836928
14.115463	1159.976511	12.841946
14.296977	1154.961611	12.846963
13.701337	1160.940624	12.851981
14.005863	1155.537342	12.856999
14.199395	1154.250012	12.862016
13.941031	1163.627297	12.867034
14.002123	1165.569244	12.872051
13.738060	1163.233094	12.877069
13.645292	1170.970663	12.882087
14.082171	1149.435534	12.887104
13.887572	1172.204595	12.892122
14.267719	1176.538138	12.897139
14.224997	1180.938807	12.902157
14.237247	1187.890641	12.907175
14.397884	1182.396380	12.912192
14.329647	1187.300995	12.917210
14.304093	1163.146013	12.922227
14.388178	1178.575838	12.927245
14.195998	1178.920712	12.932263
14.288542	1174.540298	12.937280
14.541071	1183.697757	12.942298
14.322865	1185.960229	12.947315
14.273401	1180.543989	12.952333
14.502472	1180.096918	12.957351
14.497516	1175.284257	12.962368
14.589085	1187.640874	12.967386
14.393817	1164.051651	12.972403
14.456180	1158.980270	12.977421
14.237721	1159.082673	12.982439
14.440640	1169.644765	12.987456
14.300943	1191.893245	12.992474
14.446812	1181.113826	12.997491
14.477713	1181.744032	13.002509
14.332377	1196.321565	13.007527
14.821854	1181.575709	13.012544
14.437451	1193.380961	13.017562
14.723079	1189.270362	13.022579
14.804164	1189.534258	13.027597
14.580804	1184.025905	13.032615
14.664565	1188.819589	13.037632
14.597843	1186.660833	13.042650
14.481753	1180.770438	13.047667
14.560266	1179.526913	13.052685
14.486898	1187.119573	13.057703
14.729434	1187.255819	13.062720
14.602440	1187.711950	13.067738
14.438919	1185.331431	13.072755
14.461449	1183.701546	13.077773
14.466929	1179.927358	13.082791
14.749485	1182.061416	13.087808
14.596565	1187.144568	13.092826
14.658609	1190.506031	13.097843
14.593866	1181.850278	13.102861
14.606010	1189.599059	13.107879
14.870606	1191.283791	13.112896
14.957239	1196.813704	13.117914
14.826913	1200.411456	13.122931
14.628681	1196.890187	13.127949
14.847890	1203.755670	13.132967
14.956627	1211.720946	13.137984
14.882952	1224.230668	13.143002
15.292404	1221.365555	13.148019
15.345862	1198.628943	13.153037
14.709196	1197.769112	13.158055
14.960482	1188.463582	13.163072
14.700919	1194.568343	13.168090
14.893581	1191.739060	13.173107
15.145372	1204.559889	13.178125
15.221554	1210.345237	13.183143
15.218936	1186.729457	13.188160
14.981202	1186.148337	13.193178
14.790262	1196.695426	13.198195
14.901898	1194.226922	13.203213
14.957439	1205.533365	13.208231
15.103683	1209.130487	13.213248
15.219579	1217.694888	13.218266
15.212009	1204.124688	13.223283
15.170905	1198.442729	13.228301
14.838564	1200.357583	13.233319
15.374905	1205.219966	13.238336
15.371051	1200.327599	13.243354
15.406394	1202.811718	13.248371
14.972182	1193.748185	13.253389
15.219328	1193.577613	13.258407
15.462966	1196.814595	13.263424
15.263784	1201.090753	13.268442
15.197536	1192.171502	13.273459
15.397568	1182.311341	13.278477
15.010496	1184.487955	13.283495
15.267608	1205.462598	13.288512
15.425904	1203.516815	13.293530
15.326699	1210.830924	13.298547
15.546482	1206.336968	13.303565
15.137932	1212.440573	13.308583
15.390529	1213.866699	13.313600
15.462477	1203.175453	13.318618
15.369026	1201.772379	13.323635
15.526578	1214.942205	13.328653
15.329755	1207.061106	13.333671
15.362199	1211.394646	13.338688
15.401789	1210.306150	13.343706
15.264431	1209.931833	13.348723
15.614896	1212.506379	13.353741
15.431417	1213.020656	13.358759
15.657432	1217.842212	13.363776
15.506572	1219.167712	13.368794
15.247825	1201.142832	13.373811
15.623362	1205.471043	13.378829
15.421398	1214.280067	13.383847
15.631528	1207.878735	13.388864
15.485263	1200.970045	13.393882
15.335505	1216.522988	13.398899
15.806377	1193.407215	13.403917
15.388207	1210.271051	13.408935
15.342390	1192.652070	13.413952
15.316442	1201.840010	13.418970
15.130430	1215.730882	13.423987
15.489044	1225.668750	13.429005
15.558888	1233.426716	13.434023
15.722168	1239.190793	13.439040
15.528844	1231.729121	13.444058
15.337059	1249.279302	13.449075
15.894006	1240.410758	13.454093
15.510662	1244.566989	13.459111
15.880172	1237.361861	13.464128
15.713809	1241.192710	13.469146
15.799108	1243.338707	13.474163
15.956475	1234.217543	13.479181
15.706547	1241.936637	13.484199
16.181061	1233.970172	13.489216
16.070744	1225.055036	13.494234
15.797996	1247.000433	13.499251
15.839693	1239.222795	13.504269
15.941256	1237.073815	13.509287
15.738589	1236.455603	13.514304
16.067263	1238.981399	13.519322
15.691186	1239.121658	13.524339
16.311057	1253.189583	13.529357
16.010466	1256.594650	13.534375
16.010882	1241.734110	13.539392
16.178909	1243.804438	13.544410
15.878128	1249.723146	13.549427
16.072290	1243.353174	13.554445
15.979219	1258.224251	13.559463
16.208363	1264.347282	13.564480
16.220004	1271.903892	13.569498
16.216950	1266.433896	13.574515
16.554135	1249.071790	13.579533
16.178139	1248.452106	13.584551
15.908916	1254.564982	13.589568
16.125740	1232.297906	13.594586
16.156801	1242.225749	13.599603
16.088879	1260.323698	13.604621
16.032183	1260.460976	13.609639
16.194305	1261.938666	13.614656
16.100883	1267.167895	13.619674
16.367998	1260.271564	13.624691
16.504814	1269.888291	13.629709
16.207024	1256.013495	13.634727
16.251590	1263.283204	13.639744
16.626851	1263.263680	13.644762
16.672999	1266.546105	13.649779
17.091524	1262.340899	13.654797
16.817564	1247.331824	13.659815
16.819876	1237.229734	13.664832
16.682101	1229.220183	13.669850
16.468788	1234.556207	13.674867
16.647110	1223.890276	13.679885
16.586830	1230.409692	13.684903
16.615874	1233.854756	13.689920
16.620838	1228.635577	13.694938
16.477733	1234.425089	13.699955
16.664710	1220.502103	13.704973
16.764021	1241.479056	13.709991
16.558393	1227.221984	13.715008
16.355232	1229.258780	13.720026
16.616315	1227.686897	13.725043
16.652570	1239.282336	13.730061
16.641233	1221.246071	13.735079
16.517897	1233.008802	13.740096
16.941435	1229.156071	13.745114
16.748950	1228.051208	13.750131
16.946471	1220.726696	13.755149
16.926714	1229.118667	13.760167
16.820967	1224.723966	13.765184
16.893909	1207.758079	13.770202
16.692273	1222.427803	13.775219
16.568905	1209.757510	13.780237
16.826225	1220.564350	13.785255
16.561388	1230.203927	13.790272
16.456965	1219.989190	13.795290
16.369568	1226.262532	13.800307
16.806504	1226.272376	13.805325
16.547232	1225.890454	13.810343
16.507278	1222.915380	13.815360
17.090202	1233.512934	13.820378
16.560012	1251.271576	13.825395
17.140782	1254.005286	13.830413
17.145977	1250.661381	13.835431
16.747060	1257.425914	13.840448
16.783092	1249.328781	13.845466
16.721185	1252.591270	13.850483
17.112047	1256.596734	13.855501
16.801732	1246.753947	13.860519
16.618970	1255.716884	13.865536
17.010562	1258.616877	13.870554
16.898908	1259.038393	13.875571
17.064790	1254.186652	13.880589
17.063583	1261.497974	13.885607
17.159077	1267.275035	13.890624
17.261086	1267.949981	13.895642
17.025060	1267.001699	13.900659
17.025171	1259.279341	13.905677
16.991701	1262.377707	13.910695
17.011972	1262.900043	13.915712
17.589647	1252.838080	13.920730
17.330587	1247.045488	13.925747
17.235499	1258.613245	13.930765
17.263748	1255.951060	13.935783
17.013937	1254.586809	13.940800
17.182726	1243.739789	13.945818
17.041029	1252.800254	13.950835
17.262798	1280.590880	13.955853
17.433035	1268.504213	13.960871
17.558848	1282.394987	13.965888
17.952282	1277.419230	13.970906
17.404224	1259.611750	13.975923
17.259363	1243.577553	13.980941
17.621634	1248.619678	13.985959
17.828020	1251.709306	13.990976
17.924725	1245.796122	13.995994
17.491655	1253.432116	14.001011
17.497186	1253.396142	14.006029
17.494501	1247.049644	14.011047
17.278011	1240.982736	14.016064
17.578237	1245.919380	14.021082
17.690225	1248.644939	14.026099
17.654628	1238.750658	14.031117
17.276818	1246.279893	14.036135
17.488621	1252.289463	14.041152
17.918396	1242.805608	14.046170
17.691666	1247.483517	14.051187
17.664756	1240.325198	14.056205
17.759749	1238.912237	14.061223
17.543919	1247.741678	14.066240
17.650122	1236.657206	14.071258
17.629083	1245.721150	14.076275
17.685368	1278.793082	14.081293
18.098716	1278.938499	14.086311
17.528444	1267.124968	14.091328
17.835333	1262.285547	14.096346
17.704764	1280.237006	14.101363
17.808211	1271.739800	14.106381
18.046914	1269.742341	14.111399
17.817416	1276.070086	14.116416
18.343526	1274.510299	14.121434
18.137766	1262.041149	14.126451
17.686391	1264.980458	14.131469
17.693255	1262.924278	14.136487
17.736113	1267.696010	14.141504
18.098346	1268.662749	14.146522
17.784008	1292.573661	14.151539
17.642980	1286.629875	14.156557
18.059602	1279.906242	14.161575
17.812668	1294.212116	14.166592
17.976100	1281.308767	14.171610
18.047360	1278.974265	14.176627
17.659080	1284.561039	14.181645
17.977480	1270.547796	14.186663
17.833094	1280.818981	14.191680
18.010901	1287.150082	14.196698
17.709877	1290.253500	14.201715
18.090345	1296.657596	14.206733
18.306339	1297.590834	14.211751
18.321660	1317.378200	14.216768
18.736688	1306.077904	14.221786
18.283638	1296.290951	14.226803
18.165073	1286.516437	14.231821
18.470887	1284.578743	14.236839
18.098478	1286.466769	14.241856
18.210952	1293.542226	14.246874
18.146530	1300.613655	14.251891
18.307987	1313.596333	14.256909
18.897787	1310.605942	14.261927
18.584408	1302.219720	14.266944
18.600051	1288.133871	14.271962
18.675555	1273.011911	14.276979
18.387787	1280.190505	14.281997
18.386656	1272.443152	14.287015
18.654845	1271.237557	14.292032
18.681990	1271.518831	14.297050
18.387654	1272.753691	14.302067
18.463292	1272.369959	14.307085
18.584211	1264.426286	14.312103
18.441996	1273.632694	14.317120
18.521808	1269.469483	14.322138
18.564883	1274.230159	14.327155
18.266455	1290.249216	14.332173
18.771559	1287.771377	14.337191
18.632152	1303.850772	14.342208
18.498499	1300.404031	14.347226
18.743831	1309.984152	14.352243
18.381390	1306.941110	14.357261
18.744107	1297.003605	14.362279
18.625077	1302.240227	14.367296
18.677118	1297.867061	14.372314
18.852351	1296.654190	14.377331
18.323331	1301.820393	14.382349
18.439299	1302.648130	14.387367
18.588227	1304.408871	14.392384
18.670316	1301.564774	14.397402
18.615314	1308.672047	14.402419
18.667645	1317.530629	14.407437
18.820145	1324.689435	14.412455
19.213912	1339.245724	14.417472
18.857665	1338.262389	14.422490
19.123092	1336.473469	14.427507
19.028595	1333.789828	14.432525
19.076419	1324.678446	14.437543
19.195289	1335.101216	14.442560
19.114046	1317.105323	14.447578
18.942851	1301.861724	14.452595
19.070485	1309.496612	14.457613
19.222865	1307.618910	14.462631
18.920742	1301.890492	14.467648
18.884972	1325.006117	14.472666
19.189779	1326.822193	14.477683
18.900531	1332.426472	14.482701
19.152821	1328.604968	14.487719
19.255558	1329.768114	14.492736
19.063311	1329.570952	14.497754
19.209187	1331.505798	14.502771
18.988626	1335.735729	14.507789
19.002047	1327.878282	14.512807
18.952317	1337.807334	14.517824
19.243630	1320.007515	14.522842
19.275678	1326.215102	14.527859
19.114453	1335.926193	14.532877
19.396802	1340.611922	14.537895
19.083841	1330.319974	14.542912
19.102457	1333.667979	14.547930
18.991025	1337.885388	14.552947
19.223000	1365.796118	14.557965
19.471496	1355.004933	14.562983
19.525058	1360.410466	14.568000
19.680946	1361.482560	14.573018
19.502111	1348.913038	14.578035
19.403481	1355.034372	14.583053
19.357402	1354.980158	14.588071
19.854391	1355.900818	14.593088
19.750789	1362.878568	14.598106
19.749013	1353.245911	14.603123
19.450761	1351.508016	14.608141
19.469654	1352.528545	14.613159
19.532004	1351.295550	14.618176
19.480224	1357.653204	14.623194
19.707178	1349.614416	14.628211
19.592947	1346.307743	14.633229
19.820984	1357.931020	14.638247
19.734542	1349.083904	14.643264
19.740674	1360.536402	14.648282
19.741658	1345.133026	14.653299
19.561601	1354.444541	14.658317
19.577405	1351.243920	14.663335
19.469696	1354.906071	14.668352
19.864714	1348.810105	14.673370
20.143334	1347.065060	14.678387
19.740557	1349.809962	14.683405
19.856057	1342.128132	14.688423
19.751103	1339.708583	14.693440
19.441384	1362.338702	14.698458
19.872758	1367.927638	14.703475
20.367957	1363.931357	14.708493
20.888131	1362.158990	14.713511
20.386126	1345.459591	14.718528
20.345626	1331.864409	14.723546
20.561866	1327.343252	14.728563
20.546941	1330.957983	14.733581
20.661378	1328.384087	14.738599
20.536138	1319.819148	14.743616
20.618795	1306.259141	14.748634
20.584511	1289.922213	14.753651
20.424963	1292.321837	14.758669
20.151514	1289.566018	14.763687
20.295921	1287.687078	14.768704
20.044445	1294.560905	14.773722
20.384097	1286.826315	14.778739
20.092760	1296.229796	14.783757
20.422267	1292.738208	14.788775
20.298231	1297.291500	14.793792
20.083180	1290.309897	14.798810
20.163840	1293.765733	14.803827
19.904581	1308.300200	14.808845
20.417442	1311.563180	14.813863
20.467036	1320.756028	14.818880
20.447514	1325.612091	14.823898
20.719825	1329.294104	14.828915
20.479860	1333.034003	14.833933
20.295659	1324.778172	14.838951
20.168303	1331.499436	14.843968
20.083123	1334.412097	14.848986
20.660900	1320.396689	14.854003
20.029429	1339.294845	14.859021
20.292548	1331.467974	14.864039
20.315946	1325.662923	14.869056
20.317955	1326.512446	14.874074
20.500449	1334.965921	14.879091
20.316608	1354.144210	14.884109
20.804608	1352.471636	14.889127
20.802469	1361.513433	14.894144
20.522356	1366.310224	14.899162
20.689954	1361.087547	14.904179
20.698391	1371.910231	14.909197
20.921993	1362.276146	14.914215
20.813126	1362.286828	14.919232
20.818497	1369.487484	14.924250
20.982959	1361.069898	14.929267
21.140911	1370.782394	14.934285
20.917511	1365.002169	14.939303
21.041298	1364.160933	14.944320
21.049053	1366.160532	14.949338
21.303240	1357.243541	14.954355
20.901093	1343.766567	14.959373
20.390457	1340.781664	14.964391
20.363228	1341.417742	14.969408
20.303891	1359.542930	14.974426
20.715648	1357.975264	14.979443
20.824656	1365.536694	14.984461
20.959226	1359.166681	14.989479
21.018314	1365.421580	14.994496
21.114559	1377.059171	14.999514
21.439214	1381.238777	15.004531
21.434859	1387.597857	15.009549
21.130663	1363.382911	15.014567
21.159535	1357.551554	15.019584
20.966656	1369.754562	15.024602
21.291468	1371.789551	15.029619
21.459861	1398.749366	15.034637
21.482623	1386.277583	15.039655
21.226838	1372.651611	15.044672
20.948282	1377.950245	15.049690
21.877677	1380.606292	15.054707
21.373227	1389.228425	15.059725
21.357985	1367.250847	15.064743
21.480108	1370.839200	15.069760
21.275405	1385.694994	15.074778
21.260698	1392.794269	15.079795
21.447488	1389.972022	15.084813
21.653217	1395.972811	15.089831
21.768422	1390.966628	15.094848
21.602797	1392.080832	15.099866
21.583245	1391.576034	15.104883
21.492176	1384.332201	15.109901
21.640780	1384.680205	15.114919
21.938682	1385.202133	15.119936
21.544683	1393.081901	15.124954
21.838918	1383.580206	15.129971
21.813909	1370.994300	15.134989
21.745352	1373.837695	15.140007
21.702229	1361.672252	15.145024
21.657906	1362.772313	15.150042
21.638863	1372.307394	15.155059
21.802414	1384.347198	15.160077
21.528856	1377.618497	15.165095
21.532916	1382.673016	15.170112
21.377103	1383.546457	15.175130
21.746131	1381.543785	15.180147
21.389388	1386.071787	15.185165
21.647034	1394.170599	15.190183
21.923199	1385.340106	15.195200
21.656139	1405.012656	15.200218
21.998210	1397.433496	15.205235
22.050728	1420.954501	15.210253
21.912650	1419.755999	15.215271
22.237391	1418.722519	15.220288
22.245207	1413.952155	15.225306
22.445982	1395.029765	15.230323
22.336142	1386.339032	15.235341
22.354381	1389.622356	15.240359
22.508366	1377.049774	15.245376
21.918029	1383.532059	15.250394
21.856062	1375.753769	15.255411
21.922338	1394.645928	15.260429
21.775182	1390.986860	15.265447
22.235297	1382.607204	15.270464
22.295665	1410.449536	15.275482
22.421134	1422.641903	15.280499
22.235788	1412.618143	15.285517
21.995850	1415.361144	15.290535
22.411852	1415.634454	15.295552
22.332115	1426.513671	15.300570
22.579474	1409.821652	15.305587
22.738647	1421.819498	15.310605
22.143126	1429.160222	15.315623
22.549567	1413.715166	15.320640
22.431861	1413.444669	15.325658
22.586581	1404.845622	15.330675
22.639028	1419.253694	15.335693
22.475777	1410.409393	15.340711
22.553705	1413.554727	15.345728
22.321699	1412.863807	15.350746
22.235024	1412.634435	15.355763
22.326125	1405.357930	15.360781
22.322587	1413.975834	15.365799
22.450744	1405.879731	15.370816
22.558966	1421.628406	15.375834
22.412375	1418.701818	15.380851
22.625417	1427.296733	15.385869
22.528580	1434.196635	15.390887
22.822645	1438.308683	15.395904
23.046522	1451.155391	15.400922
23.145567	1445.197656	15.405939
23.218429	1438.531942	15.410957
22.852983	1422.857589	15.415975
22.765310	1403.154619	15.420992
22.937158	1413.436028	15.426010
23.356405	1416.109661	15.431027
22.968243	1417.364366	15.436045
23.124286	1408.670033	15.441063
23.151086	1400.890248	15.446080
22.678853	1395.986451	15.451098
22.950783	1402.795090	15.456115
22.973711	1410.420366	15.461133
23.185802	1424.273392	15.466151
23.347419	1426.528047	15.471168
23.054738	1411.251272	15.476186
23.334735	1409.017475	15.481203
23.163761	1415.690086	15.486221
23.391990	1405.091363	15.491239
23.192967	1398.301523	15.496256
22.885025	1411.872020	15.501274
23.203038	1414.356503	15.506291
23.347354	1411.030316	15.511309
23.182139	1432.505315	15.516327
23.196284	1428.319650	15.521344
23.230665	1424.316641	15.526362
23.112227	1430.559373	15.531379
23.339086	1423.308253	15.536397
23.240748	1439.159378	15.541415
23.360504	1426.940987	15.546432
23.383753	1441.393466	15.551450
23.408758	1434.425467	15.556467
23.408676	1435.581994	15.561485
23.444203	1440.015666	15.566503
23.520827	1434.645224	15.571520
23.508639	1441.106591	15.576538
23.476887	1421.251265	15.581555
23.522357	1441.143243	15.586573
23.435570	1434.087826	15.591591
23.511701	1441.863951	15.596608
23.850071	1459.929440	15.601626
23.638862	1471.920232	15.606643
24.067596	1468.171295	15.611661
23.724273	1470.801289	15.616679
24.022897	1455.926298	15.621696
24.044938	1446.137895	15.626714
23.859636	1440.814079	15.631731
24.246177	1433.906007	15.636749
24.129539	1439.964414	15.641767
24.106190	1436.310464	15.646784
24.094531	1424.482443	15.651802
24.084870	1434.427767	15.656819
23.886067	1429.212276	15.661837
23.674434	1429.444439	15.666855
23.970308	1418.737101	15.671872
23.488452	1426.182842	15.676890
23.627997	1429.131998	15.681907
24.148959	1440.805739	15.686925
24.145400	1452.317379	15.691943
23.952117	1448.911360	15.696960
23.835185	1464.637058	15.701978
24.155469	1463.047495	15.706995
24.472355	1459.614248	15.712013
24.527641	1470.358993	15.717031
24.644004	1455.968786	15.722048
24.458221	1459.322646	15.727066
24.092273	1458.393655	15.732083
24.178105	1457.195545	15.737101
24.324373	1445.189856	15.742119
24.601930	1462.554271	15.747136
24.356431	1463.860790	15.752154
24.292447	1448.643613	15.757171
24.465168	1455.060850	15.762189
24.372134	1470.823347	15.767207
24.661424	1459.918669	15.772224
24.559452	1460.607846	15.777242
24.558335	1458.880278	15.782259
24.565283	1451.609587	15.787277
24.334486	1457.666397	15.792295
24.485199	1444.648492	15.797312
24.693742	1445.438305	15.802330
24.566885	1435.502489	15.807347
24.718999	1447.069493	15.812365
24.661347	1446.424159	15.817383
24.603643	1448.719390	15.822400
24.355928	1451.474704	15.827418
24.424707	1450.678376	15.832435
24.688041	1450.166786	15.837453
24.725821	1453.413041	15.842471
24.833751	1449.575604	15.847488
24.862974	1452.116476	15.852506
24.930817	1459.415105	15.857523
24.949565	1453.344077	15.862541
24.516115	1460.892058	15.867559
24.718580	1462.305235	15.872576
24.751280	1473.885693	15.877594
24.775520	1483.022403	15.882611
24.863053	1476.067671	15.887629
24.792212	1485.548595	15.892647
24.659287	1479.082203	15.897664
24.790030	1484.239427	15.902682
24.833601	1481.891362	15.907699
25.314633	1496.522740	15.912717
24.847628	1508.805011	15.917735
25.224844	1504.900623	15.922752
25.039381	1507.132143	15.927770
25.129322	1502.570987	15.932787
25.363273	1503.656369	15.937805
25.123139	1504.780925	15.942823
25.132464	1505.674125	15.947840
25.117235	1508.793735	15.952858
25.202463	1502.787677	15.957875
25.404781	1495.840934	15.962893
25.239633	1500.041086	15.967911
25.332661	1496.208659	15.972928
25.497853	1503.542199	15.977946
25.339141	1500.853001	15.982963
25.535702	1506.445165	15.987981
25.482285	1508.921169	15.992999
25.707644	1501.722026	15.998016
25.778029	1503.262335	16.003034
25.877585	1505.118451	16.008051
25.920915	1506.951186	16.013069
25.962897	1501.289437	16.018087
25.563654	1497.385620	16.023104
25.702804	1494.893035	16.028122
25.591141	1500.407407	16.033139
25.674150	1496.491607	16.038157
25.599424	1500.730551	16.043175
25.571781	1489.274365	16.048192
25.993706	1485.993024	16.053210
25.645102	1502.341220	16.058227
26.060934	1507.018916	16.063245
25.855551	1503.183640	16.068263
25.743103	1511.158854	16.073280
25.637895	1515.159169	16.078298
25.612505	1530.813908	16.083315
26.257572	1521.708034	16.088333
26.326264	1532.809420	16.093351
26.326097	1535.048115	16.098368
26.308253	1529.092933	16.103386
26.545051	1522.687064	16.108403
26.272456	1510.990077	16.113421
26.316158	1509.081301	16.118439
26.315244	1494.963554	16.123456
26.251346	1482.476884	16.128474
26.351299	1491.045450	16.133491
26.439035	1490.143245	16.138509
26.218885	1495.645231	16.143527
25.976619	1489.823397	16.148544
26.537872	1483.706011	16.153562
25.850798	1494.608876	16.158579
26.312527	1510.828095	16.163597
26.611669	1521.248560	16.168615
26.494274	1519.548467	16.173632
26.706818	1514.279930	16.178650
26.371645	1532.532782	16.183667
26.514391	1526.183984	16.188685
26.637160	1534.840328	16.193703
26.505962	1531.478748	16.198720
26.949800	1522.026450	16.203738
26.863071	1531.732046	16.208755
26.641374	1514.775145	16.213773
26.473194	1504.171987	16.218791
26.704512	1506.387384	16.223808
26.796785	1523.412455	16.228826
26.563968	1531.889792	16.233843
26.893945	1524.207858	16.238861
26.727161	1525.798777	16.243879
26.707005	1519.531028	16.248896
26.754166	1520.012319	16.253914
26.387798	1524.163653	16.258931
26.619689	1531.234642	16.263949
26.440015	1530.098313	16.268967
26.489338	1520.943266	16.273984
26.827841	1523.236413	16.279002
26.793297	1544.176064	16.284019
26.966647	1549.326662	16.289037
27.208973	1547.900742	16.294055
27.187956	1561.698134	16.299072
27.283939	1551.799229	16.304090
27.060393	1546.864129	16.309107
26.946599	1547.338952	16.314125
26.829393	1550.121333	16.319143
27.043861	1550.841677	16.324160
27.357893	1549.832988	16.329178
27.155028	1546.630473	16.334195
27.579208	1551.384747	16.339213
27.266451	1554.432485	16.344231
27.024983	1556.301463	16.349248
27.679522	1557.019550	16.354266
27.280452	1547.441008	16.359283
27.443895	1553.931070	16.364301
27.708734	1552.418172	16.369319
27.299787	1552.718175	16.374336
27.698334	1539.395096	16.379354
27.169013	1548.790818	16.384371
27.252782	1537.683462	16.389389
27.563123	1532.410568	16.394407
27.061891	1550.121662	16.399424
27.578790	1547.619593	16.404442
28.049545	1564.796706	16.409459
27.540505	1555.225899	16.414477
27.802155	1566.811895	16.419495
27.785709	1550.471744	16.424512
27.677751	1566.587155	16.429530
27.742642	1561.189281	16.434547
28.030012	1557.019250	16.439565
28.002317	1565.035597	16.444583
27.913055	1570.629353	16.449600
28.224620	1570.180056	16.454618
27.998929	1555.775028	16.459635
28.178589	1547.550867	16.464653
27.811986	1539.017817	16.469671
27.678012	1541.768917	16.474688
27.752199	1555.354729	16.479706
27.726485	1568.001865	16.484723
27.716761	1559.601735	16.489741
27.971855	1567.449124	16.494759
27.972475	1574.219022	16.499776
28.023052	1555.533237	16.504794
28.122226	1555.108605	16.509811
27.991671	1554.904591	16.514829
28.099875	1572.276449	16.519847
28.153315	1587.728283	16.524864
28.408718	1591.610767	16.529882
28.373623	1602.891539	16.534899
28.730944	1597.028844	16.539917
28.755889	1584.112107	16.544935
28.541471	1574.881334	16.549952
28.537641	1563.909876	16.554970
28.521985	1558.137566	16.559987
28.285476	1561.712206	16.565005
28.595681	1569.367835	16.570023
28.379490	1572.045332	16.575040
28.499332	1584.820969	16.580058
28.790126	1594.542360	16.585075
28.904286	1592.715816	16.590093
28.967738	1578.052776	16.595111
28.858565	1570.571129	16.600128
28.711754	1562.562699	16.605146
28.666723	1552.013952	16.610163
28.397181	1560.804619	16.615181
28.802546	1561.956746	16.620199
28.694082	1580.427080	16.625216
28.621841	1583.442756	16.630234
28.868401	1581.328422	16.635251
29.045750	1575.654511	16.640269
29.039416	1580.559059	16.645287
28.696602	1580.493060	16.650304
29.051611	1575.272802	16.655322
29.376851	1586.223185	16.660339
29.107245	1583.026181	16.665357
29.025492	1578.195183	16.670375
29.006958	1584.097098	16.675392
29.034463	1585.106969	16.680410
29.021566	1584.376093	16.685427
29.187061	1581.081996	16.690445
29.422669	1579.666040	16.695463
29.242539	1583.349070	16.700480
29.592758	1576.801420	16.705498
29.563390	1569.864783	16.710515
29.350615	1570.546097	16.715533
29.607007	1583.744587	16.720551
29.534599	1576.518639	16.725568
29.395004	1571.249619	16.730586
29.265995	1578.557805	16.735603
29.341018	1583.566022	16.740621
29.656204	1572.547747	16.745639
29.553053	1569.930053	16.750656
29.680399	1579.605421	16.755674
29.493766	1575.335193	16.760691
29.591691	1583.480379	16.765709
30.142596	1576.525990	16.770727
29.623016	1570.513562	16.775744
29.637095	1568.973408	16.780762
29.821632	1573.395092	16.785779
29.272321	1572.368654	16.790797
29.555270	1558.365141	16.795815
29.524714	1577.076109	16.800832
29.665842	1565.233558	16.805850
29.957382	1588.771417	16.810867
29.740809	1599.020889	16.815885
30.112019	1596.602132	16.820903
29.911344	1598.661200	16.825920
29.663922	1596.192524	16.830938
29.740159	1599.360613	16.835955
29.720168	1596.976584	16.840973
30.190570	1595.621422	16.845991
29.757469	1599.758019	16.851008
30.344386	1602.787987	16.856026
30.384917	1598.053887	16.861043
30.130437	1597.691238	16.866061
30.262721	1598.295850	16.871079
30.197063	1604.372076	16.876096
30.497104	1588.003992	16.881114
30.416972	1612.512446	16.886131
30.158162	1609.172724	16.891149
30.730327	1597.672255	16.896167
30.331553	1599.080678	16.901184
30.287171	1603.763793	16.906202
30.267102	1603.723979	16.911219
30.128121	1601.338157	16.916237
30.621505	1615.083660	16.921255
30.768608	1636.161115	16.926272
30.461886	1616.700343	16.931290
30.680324	1616.818138	16.936307
30.534407	1636.389479	16.941325
30.630447	1638.489077	16.946343
30.821960	1632.661247	16.951360
30.720534	1632.516977	16.956378
30.877057	1640.911141	16.961395
30.695822	1638.953309	16.966413
30.795998	1633.832418	16.971431
31.060480	1635.412902	16.976448
30.731982	1640.360275	16.981466
30.940128	1636.358217	16.986483
30.827424	1636.449247	16.991501
31.012673	1640.430137	16.996519
30.902706	1640.189062	17.001536
30.661177	1635.783613	17.006554
30.444166	1637.792046	17.011571
30.817812	1638.362484	17.016589
30.890790	1627.073207	17.021607
30.629588	1628.629154	17.026624
31.185547	1653.131761	17.031642
31.442257	1652.180366	17.036659
31.290779	1668.093651	17.041677
31.484655	1645.330617	17.046695
31.316923	1658.842928	17.051712
31.740300	1647.660872	17.056730
31.699854	1644.152594	17.061747
31.196454	1639.692398	17.066765
31.362770	1633.249121	17.071783
31.306716	1652.119297	17.076800
31.178944	1653.417201	17.081818
31.402742	1651.775659	17.086835
31.487029	1641.793796	17.091853
31.635980	1654.667622	17.096871
31.593463	1647.939004	17.101888
31.636496	1654.358269	17.106906
31.716037	1650.297351	17.111923
31.301011	1658.521043	17.116941
31.550459	1643.770716	17.121959
31.514787	1654.651866	17.126976
31.450965	1659.853307	17.131994
31.534467	1671.094455	17.137011
31.806444	1680.081498	17.142029
31.793284	1690.558607	17.147047
31.655224	1686.140376	17.152064
31.493009	1683.660951	17.157082
31.992711	1682.435571	17.162099
31.491738	1678.747510	17.167117
32.404116	1681.523145	17.172135
32.097975	1676.121983	17.177152
32.070212	1679.154143	17.182170
32.345583	1678.229581	17.187187
32.264050	1683.873473	17.192205
32.165601	1689.074151	17.197223
32.178513	1676.583094	17.202240
32.146210	1682.678048	17.207258
32.263299	1682.141608	17.212275
32.121378	1689.295502	17.217293
32.244795	1702.383208	17.222311
32.412341	1717.289802	17.227328
32.483723	1720.504776	17.232346
32.594976	1710.367840	17.237363
32.475018	1717.631294	17.242381
32.787725	1701.157860	17.247399
32.441298	1703.057584	17.252416
32.557785	1691.985454	17.257434
32.822120	1702.059867	17.262451
32.579240	1707.328113	17.267469
32.532904	1701.298645	17.272487
32.730519	1709.121751	17.277504
32.823230	1708.318700	17.282522
33.004048	1692.624856	17.287539
32.718607	1708.325110	17.292557
32.837798	1701.104840	17.297575
33.055487	1691.868923	17.302592
32.805524	1705.007506	17.307610
33.123104	1696.732328	17.312627
32.880413	1706.165219	17.317645
33.206836	1715.652282	17.322663
33.257917	1706.381099	17.327680
33.116753	1711.116456	17.332698
33.289483	1705.132667	17.337715
33.162358	1706.086021	17.342733
32.854173	1703.142778	17.347751
33.093260	1698.689383	17.352768
32.890634	1704.335184	17.357786
33.358119	1696.918795	17.362803
33.092395	1702.775196	17.367821
33.502620	1697.218645	17.372839
33.449577	1701.667422	17.377856
33.164618	1704.551559	17.382874
33.305393	1697.064368	17.387891
33.303383	1710.044870	17.392909
33.193772	1704.492535	17.397927
32.944897	1700.400844	17.402944
32.897532	1722.957827	17.407962
33.720781	1723.424251	17.412979
33.277533	1733.699853	17.417997
33.631463	1733.943669	17.423015
33.693384	1730.825889	17.428032
33.905939	1731.278479	17.433050
34.059519	1719.970501	17.438067
33.697871	1725.531183	17.443085
33.639485	1727.582698	17.448103
33.823679	1730.940629	17.453120
33.692748	1729.391354	17.458138
33.942390	1724.528183	17.463155
33.811346	1724.103799	17.468173
33.976921	1721.966810	17.473191
33.993071	1712.201453	17.478208
34.314329	1732.379889	17.483226
34.347276	1715.607433	17.488243
34.243965	1718.634567	17.493261
34.152956	1722.099776	17.498279
34.400684	1720.136395	17.503296
33.911699	1724.029926	17.508314
33.791377	1721.668952	17.513331
33.958737	1720.007599	17.518349
34.277399	1750.479015	17.523367
34.469018	1751.810557	17.528384
34.207245	1746.907493	17.533402
34.684402	1744.238752	17.538419
34.428963	1758.676171	17.543437
34.566688	1754.855780	17.548455
34.600887	1740.638906	17.553472
34.648001	1745.327611	17.558490
34.583825	1742.160202	17.563507
34.576258	1747.026232	17.568525
34.690555	1742.772757	17.573543
34.914316	1741.828967	17.578560
34.558582	1744.149478	17.583578
34.462394	1744.015166	17.588595
34.577724	1747.734834	17.593613
34.877193	1755.776539	17.598631
34.696065	1752.694194	17.603648
34.520879	1755.237009	17.608666
34.675665	1758.320112	17.613683
34.614547	1753.381723	17.618701
34.884206	1742.357466	17.623719
34.667141	1753.979802	17.628736
34.574012	1769.559176	17.633754
34.979675	1769.331109	17.638771
35.126377	1767.491688	17.643789
35.130728	1781.963356	17.648807
35.022190	1762.063593	17.653824
35.041350	1771.269022	17.658842
35.122514	1768.248043	17.663859
35.289957	1773.776817	17.668877
35.236702	1773.777128	17.673895
35.234670	1768.984465	17.678912
35.427889	1765.030899	17.683930
35.522342	1766.996147	17.688947
35.416230	1772.993897	17.693965
35.438870	1760.073259	17.698983
35.580915	1760.202499	17.704000
35.581202	1785.601972	17.709018
35.765604	1766.390329	17.714035
35.534749	1760.426954	17.719053
35.569306	1767.608212	17.724071
35.938289	1767.947955	17.729088
36.065955	1762.517789	17.734106
36.074842	1757.397968	17.739123
35.849605	1759.140680	17.744141
35.667081	1766.440477	17.749159
35.846232	1756.456643	17.754176
35.973730	1751.599672	17.759194
35.966277	1748.977550	17.764211
36.073075	1755.770136	17.769229
36.010982	1756.441517	17.774247
36.260300	1757.480485	17.779264
35.990349	1758.286400	17.784282
36.191841	1763.422186	17.789299
36.167491	1756.829873	17.794317
36.287282	1759.199548	17.799335
36.714353	1754.839665	17.804352
36.368956	1751.032385	17.809370
36.386946	1748.336578	17.814387
36.684584	1746.120289	17.819405
36.387896	1753.093905	17.824423
36.616493	1729.245997	17.829440
36.552420	1741.502219	17.834458
36.287007	1742.427644	17.839475
36.501059	1736.483466	17.844493
36.371034	1740.554271	17.849511
36.506209	1733.923206	17.854528
36.367331	1752.361179	17.859546
36.854686	1764.776466	17.864563
36.797628	1765.768830	17.869581
36.342131	1785.370259	17.874599
36.988767	1777.130416	17.879616
36.779883	1775.080886	17.884634
36.858882	1772.162419	17.889651
36.790243	1777.026938	17.894669
36.768531	1781.701637	17.899687
37.306073	1771.180867	17.904704
36.951219	1767.392072	17.909722
37.026660	1767.956090	17.914739
37.180169	1765.346339	17.919757
36.940361	1772.945336	17.924775
37.473992	1768.988661	17.929792
37.029020	1776.138152	17.934810
37.078649	1768.431566	17.939827
37.087726	1769.701946	17.944845
36.813866	1778.337167	17.949863
37.411767	1773.984283	17.954880
37.075743	1776.642842	17.959898
37.341725	1770.241693	17.964915
37.103903	1767.518872	17.969933
37.057838	1777.928651	17.974951
37.540424	1779.448308	17.979968
37.472186	1798.651546	17.984986
37.681580	1798.176414	17.990003
38.079451	1789.413562	17.995021
37.834390	1794.159421	18.000039
38.255273	1762.296704	18.005056
37.809743	1759.794604	18.010074
37.544365	1764.480236	18.015091
37.599978	1761.381010	18.020109
37.671111	1754.481219	18.025127
37.649455	1754.301918	18.030144
37.695337	1787.569949	18.035162
37.524513	1794.627695	18.040179
37.732214	1790.677043	18.045197
37.370620	1804.092987	18.050215
37.691188	1787.805543	18.055232
37.722604	1796.565900	18.060250
38.030993	1796.825116	18.065267
38.224915	1811.526087	18.070285
37.972967	1820.665137	18.075303
37.852765	1816.209078	18.080320
37.797574	1819.778024	18.085338
37.952318	1828.969940	18.090355
38.350297	1824.496551	18.095373
38.241329	1817.328889	18.100391
38.246544	1809.823104	18.105408
38.213138	1824.266212	18.110426
38.258378	1831.160726	18.115443
38.662187	1833.117967	18.120461
38.512241	1848.925685	18.125479
38.750579	1842.120260	18.130496
38.641861	1843.159350	18.135514
38.780044	1844.694592	18.140531
39.242193	1840.618819	18.145549
39.065472	1847.704923	18.150567
38.748491	1818.961537	18.155584
38.859155	1824.032440	18.160602
38.877568	1835.322649	18.165619
39.057628	1843.047160	18.170637
38.987989	1844.338033	18.175655
38.884277	1839.699341	18.180672
39.189831	1837.896844	18.185690
38.963372	1846.572494	18.190707
39.273677	1842.341320	18.195725
38.852203	1847.268299	18.200743
39.199356	1844.126195	18.205760
39.661609	1840.213183	18.210778
39.099671	1851.588480	18.215795
39.295986	1842.634321	18.220813
38.749814	1849.839541	18.225831
38.920373	1844.927990	18.230848
39.221301	1832.963955	18.235866
39.246638	1839.488573	18.240883
39.391851	1828.145878	18.245901
39.195400	1850.816455	18.250919
39.514144	1858.921558	18.255936
39.482570	1861.683545	18.260954
39.599216	1881.541302	18.265971
39.803756	1868.074624	18.270989
39.848072	1874.143805	18.276007
39.706390	1858.984924	18.281024
39.994239	1861.433920	18.286042
39.638818	1860.720659	18.291059
39.913448	1853.941709	18.296077
39.908452	1876.534431	18.301095
40.159026	1862.324007	18.306112
40.058346	1869.307408	18.311130
40.069230	1867.203834	18.316147
39.886042	1851.652648	18.321165
39.987566	1856.581780	18.326183
40.098577	1847.455514	18.331200
40.404532	1855.860138	18.336218
40.001169	1854.646586	18.341235
40.122412	1852.276773	18.346253
40.295134	1869.530247	18.351271
40.123737	1852.649297	18.356288
40.391049	1841.061441	18.361306
40.332136	1866.485395	18.366323
40.532591	1846.489979	18.371341
40.300981	1854.380938	18.376359
40.029804	1853.218960	18.381376
40.509352	1862.853037	18.386394
40.702405	1874.105559	18.391411
40.717138	1883.023824	18.396429
40.682685	1889.830756	18.401447
40.614273	1879.403549	18.406464
40.882707	1882.016763	18.411482
40.590649	1885.460906	18.416499
40.828681	1878.170723	18.421517
40.753906	1892.012920	18.426535
40.650561	1881.411976	18.431552
40.433707	1881.890258	18.436570
40.606353	1890.673979	18.441587
40.980578	1889.130574	18.446605
41.346306	1910.000838	18.451623
41.010368	1905.838842	18.456640
41.628367	1917.166828	18.461658
41.158411	1912.229419	18.466675
41.398160	1907.743969	18.471693
41.180980	1916.347659	18.476711
41.372848	1904.911578	18.481728
41.230979	1902.436235	18.486746
41.391644	1906.161638	18.491763
41.178964	1918.121329	18.496781
41.542033	1902.956154	18.501799
41.436958	1909.919238	18.506816
41.957741	1912.731481	18.511834
41.510069	1915.685256	18.516851
41.729144	1902.458642	18.521869
41.651860	1914.059574	18.526887
41.620307	1903.752034	18.531904
41.779563	1906.749989	18.536922
41.742352	1909.148780	18.541939
41.480410	1907.983501	18.546957
41.629456	1906.735939	18.551975
41.941545	1909.030165	18.556992
42.375562	1917.382758	18.562010
41.894524	1907.927366	18.567027
41.996170	1916.489000	18.572045
42.252278	1936.827078	18.577063
41.914344	1937.275571	18.582080
42.041819	1941.364108	18.587098
41.991972	1938.105716	18.592115
42.766826	1933.741066	18.597133
42.569814	1942.947480	18.602151
42.543932	1939.310362	18.607168
42.578843	1939.915529	18.612186
42.655452	1933.307835	18.617203
42.823009	1923.094730	18.622221
42.514462	1911.769088	18.627239
42.376794	1901.018896	18.632256
42.315938	1910.942480	18.637274
42.462862	1929.447007	18.642291
42.381157	1935.662221	18.647309
42.539343	1938.057072	18.652327
42.702973	1927.432450	18.657344
42.498388	1917.904402	18.662362
42.656998	1930.150745	18.667379
42.632183	1935.390711	18.672397
42.738484	1923.863451	18.677415
42.762480	1944.186159	18.682432
42.772666	1945.683315	18.687450
42.697510	1959.466193	18.692467
42.984522	1957.147704	18.697485
42.713594	1964.188410	18.702503
42.934530	1964.679579	18.707520
43.083316	1954.288865	18.712538
43.126717	1964.925104	18.717555
43.232245	1954.887959	18.722573
43.441087	1981.654138	18.727591
43.521927	1990.260783	18.732608
43.680902	1983.193831	18.737626
43.729929	1985.942522	18.742643
43.677588	1966.110563	18.747661
43.893014	1953.009890	18.752679
43.558114	1951.400606	18.757696
43.722371	1948.415069	18.762714
43.586059	1966.772764	18.767731
43.528974	1958.897317	18.772749
43.748327	1969.421225	18.777767
43.469994	1988.314567	18.782784
43.851807	1982.279980	18.787802
43.747495	1984.905796	18.792819
43.797792	1980.007186	18.797837
44.043696	1986.235994	18.802855
44.000422	1989.552247	18.807872
44.369726	1972.263541	18.812890
43.970983	1975.482444	18.817907
44.249485	1968.572305	18.822925
44.298311	1968.764978	18.827943
44.241220	1967.576275	18.832960
44.329203	1962.499806	18.837978
44.139737	1966.310638	18.842995
44.414875	1972.766280	18.848013
44.423149	1971.755143	18.853031
44.157206	1979.189089	18.858048
44.580332	1985.607882	18.863066
44.327586	1991.171133	18.868083
44.433179	1999.797313	18.873101
44.626820	2001.263373	18.878119
44.668293	2000.512076	18.883136
45.072495	1986.317685	18.888154
45.139043	1987.960241	18.893171
45.123487	1999.522300	18.898189
45.030688	1982.795723	18.903207
45.034644	1982.921606	18.908224
45.257206	1977.774276	18.913242
45.146963	2002.740053	18.918259
45.312260	1976.556976	18.923277
45.592245	1976.943319	18.928295
45.184137	1968.273003	18.933312
45.334706	1955.183045	18.938330
44.708977	1960.786859	18.943347
45.204280	1965.015388	18.948365
45.694641	1974.506818	18.953383
45.431068	1982.797771	18.958400
45.771462	1982.921990	18.963418
45.194542	1974.355543	18.968435
45.192003	1975.736510	18.973453
45.507391	1986.716955	18.978471
45.275100	1997.219854	18.983488
45.109429	1971.654808	18.988506
45.339872	1989.546059	18.993523
45.767544	1986.221149	18.998541
46.048061	1975.309094	19.003559
45.578310	1992.935775	19.008576
45.534541	1974.424702	19.013594
45.656666	1978.991252	19.018611
45.641427	2002.795183	19.023629
46.027263	2004.028125	19.028647
46.056152	2008.352832	19.033664
46.116842	2007.105494	19.038682
46.247954	2008.231723	19.043699
46.217142	2007.293965	19.048717
46.226960	1994.722658	19.053735
46.068838	2010.823597	19.058752
46.223805	1999.020744	19.063770
46.055123	2000.913964	19.068787
46.020915	2005.120566	19.073805
46.250880	1992.575080	19.078823
46.189196	2005.022240	19.083840
46.598688	2016.207410	19.088858
46.539054	2026.185979	19.093875
46.537880	2034.719202	19.098893
46.743362	2030.650167	19.103911
46.542399	2036.295223	19.108928
46.218905	2028.525963	19.113946
46.264854	2035.939496	19.118963
46.614977	2048.991610	19.123981
47.001110	2029.744927	19.128999
46.801405	2028.395944	19.134016
46.815353	2024.511893	19.139034
46.910233	2043.648721	19.144051
46.950030	2047.346301	19.149069
47.532602	2060.551334	19.154087
47.315477	2047.116584	19.159104
47.466946	2050.792169	19.164122
47.476946	2057.660326	19.169139
47.532643	2048.078952	19.174157
47.198568	2042.664364	19.179175
47.574859	2058.683736	19.184192
47.402617	2048.477293	19.189210
47.292350	2052.808080	19.194227
47.483388	2054.725124	19.199245
47.554216	2050.520475	19.204263
47.633738	2059.854278	19.209280
47.992384	2055.227102	19.214298
47.836540	2063.105253	19.219315
47.336098	2056.629866	19.224333
47.854150	2052.796156	19.229351
47.790343	2063.690314	19.234368
47.779131	2055.633829	19.239386
47.661581	2064.639407	19.244403
47.604810	2067.733518	19.249421
47.828200	2077.238028	19.254439
47.959439	2085.489186	19.259456
47.810136	2081.548246	19.264474
48.274166	2085.155459	19.269491
48.321446	2078.151798	19.274509
48.481943	2070.375368	19.279527
48.337943	2092.107598	19.284544
48.253241	2075.510869	19.289562
48.500899	2079.728193	19.294579
48.291926	2077.155849	19.299597
48.176846	2070.651813	19.304615
48.201122	2075.287705	19.309632
48.696207	2086.222781	19.314650
48.740801	2097.598218	19.319667
48.648303	2098.220509	19.324685
49.049001	2100.160979	19.329703
48.822953	2098.970857	19.334720
49.013407	2100.821080	19.339738
49.054374	2099.248283	19.344755
49.163080	2112.066352	19.349773
49.342833	2097.695187	19.354791
49.178362	2093.518583	19.359808
49.019675	2085.351031	19.364826
48.774011	2084.942821	19.369843
48.935806	2091.101327	19.374861
49.567015	2087.866767	19.379879
49.318496	2105.776084	19.384896
49.461334	2097.409501	19.389914
49.208071	2091.342820	19.394931
49.290489	2095.337475	19.399949
49.688474	2088.670310	19.404967
49.744618	2096.220167	19.409984
49.344805	2086.731558	19.415002
49.320685	2085.512400	19.420019
49.455935	2083.871864	19.425037
49.821121	2089.375162	19.430055
49.914235	2092.428370	19.435072
49.422122	2089.860493	19.440090
49.717728	2098.389981	19.445107
49.747843	2119.620095	19.450125
49.739645	2112.402378	19.455143
49.867246	2117.263708	19.460160
50.035998	2116.063459	19.465178
50.139520	2110.979650	19.470195
50.128640	2119.590501	19.475213
50.387586	2113.706470	19.480231
50.097801	2123.221996	19.485248
50.324208	2110.351442	19.490266
50.281256	2098.550316	19.495283
50.178291	2109.623600	19.500301
50.522214	2113.318771	19.505319
50.672148	2132.044678	19.510336
50.761798	2136.531806	19.515354
51.318324	2128.163376	19.520371
50.946978	2116.243092	19.525389
51.007730	2102.819260	19.530407
50.916514	2099.907010	19.535424
50.715622	2095.896448	19.540442
50.736655	2102.904129	19.545459
50.737112	2112.147495	19.550477
51.030864	2108.224272	19.555495
51.092689	2117.663388	19.560512
50.782487	2135.216232	19.565530
51.021392	2127.896460	19.570547
51.081183	2134.693438	19.575565
51.067262	2131.693415	19.580583
51.106855	2132.840486	19.585600
50.892585	2131.608458	19.590618
51.256822	2124.881112	19.595635
51.104913	2141.103590	19.600653
51.717776	2145.007258	19.605671
51.694161	2157.014035	19.610688
51.554257	2165.223237	19.615706
51.721622	2158.175093	19.620723
51.406890	2156.512852	19.625741
51.577352	2159.719419	19.630759
51.763017	2161.834395	19.635776
51.460393	2157.090496	19.640794
51.580624	2155.629584	19.645811
51.239228	2156.842762	19.650829
51.602808	2155.564060	19.655847
51.881727	2171.892332	19.660864
51.742778	2192.964476	19.665882
52.057811	2181.288172	19.670899
51.979550	2186.094769	19.675917
52.034465	2196.462752	19.680935
52.378740	2187.864818	19.685952
52.006456	2186.901199	19.690970
52.340624	2178.352968	19.695987
52.417286	2185.028293	19.701005
52.529909	2182.375626	19.706023
52.722243	2187.109165	19.711040
52.288913	2184.506560	19.716058
52.763842	2192.926160	19.721075
52.721279	2204.385167	19.726093
53.014516	2205.382858	19.731111
53.057658	2203.059753	19.736128
52.863369	2194.129586	19.741146
53.175446	2190.434201	19.746163
53.155504	2205.461219	19.751181
53.294233	2190.603873	19.756199
52.900976	2186.115669	19.761216
52.789475	2184.996959	19.766234
53.360467	2194.473234	19.771251
53.012327	2199.219125	19.776269
53.004605	2194.778028	19.781287
53.186009	2198.900436	19.786304
53.132581	2214.100108	19.791322
53.518525	2209.471525	19.796339
53.114937	2208.550279	19.801357
53.013036	2210.694868	19.806375
53.181108	2233.108542	19.811392
53.146119	2239.451581	19.816410
53.738076	2240.060767	19.821427
53.508523	2239.719176	19.826445
53.581278	2250.090940	19.831463
53.864480	2243.716276	19.836480
53.855954	2252.259889	19.841498
54.019991	2259.162914	19.846515
53.761734	2267.011048	19.851533
54.029817	2270.507192	19.856551
54.352527	2264.379122	19.861568
54.404322	2258.168665	19.866586
54.638202	2248.613034	19.871603
54.589146	2253.371915	19.876621
54.942806	2246.781294	19.881639
54.801489	2230.094943	19.886656
54.418838	2220.979368	19.891674
54.671936	2214.742554	19.896691
54.558962	2213.309347	19.901709
54.296703	2210.365699	19.906727
54.572421	2223.918997	19.911744
54.621616	2244.546573	19.916762
54.731249	2240.702163	19.921779
54.873098	2246.878396	19.926797
54.821171	2240.722288	19.931815
54.984083	2245.516017	19.936832
54.718557	2258.651934	19.941850
55.074830	2250.011238	19.946867
55.000242	2254.974127	19.951885
55.075024	2242.875505	19.956903
55.099954	2244.933005	19.961920
54.849119	2247.575400	19.966938
55.192656	2272.225703	19.971955
55.479678	2275.650811	19.976973
55.871715	2273.248391	19.981991
56.037291	2271.144002	19.987008
55.492128	2263.697253	19.992026
55.858301	2239.423690	19.997043
55.614920	2232.678602	20.002061
55.472487	2238.036130	20.007079
55.719113	2230.158779	20.012096
55.680319	2253.079856	20.017114
55.848719	2264.505622	20.022131
55.738780	2267.695756	20.027149
55.618840	2273.952658	20.032167
55.913139	2266.672482	20.037184
56.030253	2275.345531	20.042202
55.699858	2260.193621	20.047219
55.928374	2264.809796	20.052237
55.715520	2263.331480	20.057255
56.280180	2279.555567	20.062272
56.244069	2290.142576	20.067290
56.292483	2295.415441	20.072307
56.301686	2307.308456	20.077325
56.095499	2301.770485	20.082343
56.455007	2291.731505	20.087360
56.396220	2301.692790	20.092378
56.318413	2300.084485	20.097395
56.563152	2306.835821	20.102413
56.401630	2323.622044	20.107431
56.887704	2322.488626	20.112448
56.985499	2335.310456	20.117466
57.114239	2337.500409	20.122483
57.108943	2333.200003	20.127501
56.952283	2337.213560	20.132519
57.153967	2333.511385	20.137536
57.095653	2343.709609	20.142554
57.156716	2332.046027	20.147571
57.218364	2329.988722	20.152589
57.247202	2326.761928	20.157607
57.300584	2321.646377	20.162624
57.313796	2348.772859	20.167642
57.273662	2351.142873	20.172659
57.327832	2345.788816	20.177677
57.564941	2361.557901	20.182695
57.902533	2337.344219	20.187712
57.670294	2344.243872	20.192730
57.710270	2356.260570	20.197747
57.822124	2349.054595	20.202765
57.678592	2357.027704	20.207783
58.226504	2349.980168	20.212800
57.791299	2355.920918	20.217818
57.849913	2369.592693	20.222835
58.300305	2377.687143	20.227853
58.436036	2378.509510	20.232871
58.729442	2371.633931	20.237888
58.772702	2381.220163	20.242906
59.108932	2359.710218	20.247923
59.061845	2337.313911	20.252941
58.715976	2337.011419	20.257959
59.020646	2335.331248	20.262976
59.025644	2340.875850	20.267994
59.064792	2335.066439	20.273011
59.106119	2347.581492	20.278029
58.860868	2332.214078	20.283047
58.923312	2329.905873	20.288064
58.976257	2335.949403	20.293082
59.108119	2340.726248	20.298099
58.872505	2335.245683	20.303117
58.660500	2333.747732	20.308135
58.996954	2327.479975	20.313152
58.830790	2331.578361	20.318170
58.945789	2336.463692	20.323187
59.059401	2335.181993	20.328205
58.688320	2345.411234	20.333223
59.151767	2352.493549	20.338240
59.226647	2354.241060	20.343258
59.351835	2344.006137	20.348275
59.505406	2350.238541	20.353293
59.649317	2358.703484	20.358311
59.518884	2344.600849	20.363328
59.568828	2368.548302	20.368346
59.825061	2381.425873	20.373363
59.743836	2384.357565	20.378381
59.722454	2392.025489	20.383399
60.125964	2380.842252	20.388416
60.070343	2387.276550	20.393434
60.006653	2380.814084	20.398451
60.447050	2389.114705	20.403469
59.781130	2396.373622	20.408487
60.386446	2386.002644	20.413504
60.035877	2383.594975	20.418522
59.918827	2391.830636	20.423539
60.323164	2405.789976	20.428557
60.439492	2416.931763	20.433575
60.544114	2413.688884	20.438592
60.751229	2418.938717	20.443610
60.926361	2417.947220	20.448627
60.812680	2408.991010	20.453645
60.742418	2412.484832	20.458663
60.587936	2412.557574	20.463680
60.477899	2417.798598	20.468698
60.724596	2431.134644	20.473715
61.117022	2432.932244	20.478733
60.711916	2444.459013	20.483751
61.258765	2427.588266	20.488768
61.272543	2439.865443	20.493786
60.983501	2441.547714	20.498803
61.687768	2439.636946	20.503821
61.170422	2440.581208	20.508839
61.559826	2447.277404	20.513856
61.605252	2446.586256	20.518874
61.799529	2461.430890	20.523891
61.787009	2464.576032	20.528909
61.899810	2473.748888	20.533927
62.161046	2469.193195	20.538944
62.229005	2462.984316	20.543962
62.380910	2451.390666	20.548979
62.308072	2432.388605	20.553997
62.139889	2434.772115	20.559015
62.446482	2422.556509	20.564032
62.131104	2430.110052	20.569050
61.995286	2416.530647	20.574067
62.218216	2424.853837	20.579085
62.196361	2451.366257	20.584103
62.418018	2453.349548	20.589120
62.416395	2465.744440	20.594138
62.304616	2468.853429	20.599155
62.826854	2460.975495	20.604173
62.411106	2473.672470	20.609191
62.263520	2457.568761	20.614208
62.553849	2465.225762	20.619226
62.677785	2477.563501	20.624243
62.952705	2493.939622	20.629261
62.696072	2490.400737	20.634279
62.784346	2491.893901	20.639296
63.022446	2499.178865	20.644314
63.035298	2489.643074	20.649331
63.336882	2496.786452	20.654349
62.951861	2495.682800	20.659367
63.059397	2499.794662	20.664384
63.497265	2519.571422	20.669402
63.217200	2525.775952	20.674419
63.772082	2525.051598	20.679437
63.537724	2527.198041	20.684455
63.747084	2511.242367	20.689472
63.712047	2519.245267	20.694490
63.518386	2521.429076	20.699507
63.880444	2517.727717	20.704525
63.639828	2521.722716	20.709543
63.694921	2526.740045	20.714560
63.554274	2519.838100	20.719578
63.687107	2533.963278	20.724595
64.099245	2539.299149	20.729613
64.339310	2544.881551	20.734631
64.243444	2546.139810	20.739648
64.124693	2534.049911	20.744666
64.310143	2535.558122	20.749683
64.511089	2531.398374	20.754701
64.434685	2537.516503	20.759719
64.639182	2527.658881	20.764736
64.623906	2539.114217	20.769754
64.551777	2544.480113	20.774771
64.659685	2557.252034	20.779789
64.683474	2560.087277	20.784807
64.714096	2564.335086	20.789824
65.190170	2561.216810	20.794842
64.829140	2563.828651	20.799859
65.135029	2559.683442	20.804877
64.960438	2571.770997	20.809895
65.419184	2571.373138	20.814912
65.274543	2570.521868	20.819930
65.232687	2591.400765	20.824947
65.536393	2588.338524	20.829965
65.594606	2592.445175	20.834983
65.743698	2584.800089	20.840000
66.107873	2596.026240	20.845018
65.977950	2592.909674	20.850035
66.105141	2586.009108	20.855053
66.095932	2590.815837	20.860071
65.922720	2573.144285	20.865088
66.196063	2566.473499	20.870106
65.619151	2582.272996	20.875123
66.013137	2580.452458	20.880141
66.274714	2570.301535	20.885159
66.140418	2581.442731	20.890176
66.505993	2572.103708	20.895194
66.248561	2577.401029	20.900211
66.358224	2581.473981	20.905229
66.123937	2587.006443	20.910247
66.218424	2583.222519	20.915264
66.370755	2605.655082	20.920282
66.407083	2626.383714	20.925299
66.367918	2611.063460	20.930317
66.629201	2614.397627	20.935335
66.988281	2608.857866	20.940352
66.778956	2617.276996	20.945370
66.653422	2617.368181	20.950387
66.872167	2632.678399	20.955405
67.500370	2632.513547	20.960423
67.283401	2645.835261	20.965440
67.385437	2637.292855	20.970458
67.323014	2631.450316	20.975475
67.515147	2625.700748	20.980493
67.532105	2631.888521	20.985511
67.770172	2623.012245	20.990528
67.622866	2628.739786	20.995546
67.557939	2638.140129	21.000563
67.841443	2640.567136	21.005581
67.822520	2641.010370	21.010599
67.768240	2634.596831	21.015616
67.928617	2640.070002	21.020634
67.555323	2643.126772	21.025651
67.821965	2647.886361	21.030669
67.961461	2670.367987	21.035687
67.785786	2662.784401	21.040704
68.304249	2660.652749	21.045722
67.995664	2669.346168	21.050739
68.248674	2669.000020	21.055757
68.021679	2673.020364	21.060775
68.474737	2684.752731	21.065792
68.669130	2682.259687	21.070810
68.630535	2691.517923	21.075827
68.884184	2678.754201	21.080845
69.211641	2696.009801	21.085863
68.972567	2690.341698	21.090880
69.216995	2682.963866	21.095898
69.409514	2681.403761	21.100915
69.449779	2672.315273	21.105933
69.601876	2677.296938	21.110951
69.773648	2679.501876	21.115968
69.755185	2656.666737	21.120986
69.476497	2642.638325	21.126003
69.254537	2635.848184	21.131021
69.410972	2635.845929	21.136039
69.614723	2662.749361	21.141056
69.941761	2656.470037	21.146074
69.623347	2667.011437	21.151091
69.615938	2664.957626	21.156109
69.645282	2671.143762	21.161127
69.523861	2673.906175	21.166144
70.206459	2666.716563	21.171162
70.009751	2673.823078	21.176179
69.919884	2658.673350	21.181197
70.015741	2683.349885	21.186215
70.046421	2703.096139	21.191232
69.903454	2708.924957	21.196250
70.000715	2703.167416	21.201267
70.140205	2703.398658	21.206285
70.180474	2701.301532	21.211303
70.431982	2715.639145	21.216320
70.717372	2723.803365	21.221338
70.540607	2724.546292	21.226355
70.762285	2710.931569	21.231373
70.820214	2721.833239	21.236391
70.784732	2720.011607	21.241408
71.423810	2713.251585	21.246426
70.958994	2713.117353	21.251443
71.090338	2739.367955	21.256461
71.507932	2746.324966	21.261479
71.253481	2738.188638	21.266496
71.434834	2746.553124	21.271514
71.764048	2749.067472	21.276531
71.690080	2744.175966	21.281549
71.854368	2746.591983	21.286567
71.659813	2739.301228	21.291584
71.974039	2729.859184	21.296602
71.751007	2739.635696	21.301619
71.758480	2745.565253	21.306637
71.863225	2748.825321	21.311655
72.048625	2751.059906	21.316672
71.714523	2739.565640	21.321690
71.707249	2750.347008	21.326707
71.801434	2763.882748	21.331725
72.330512	2773.992068	21.336743
72.260462	2775.249623	21.341760
72.718948	2755.557820	21.346778
72.723952	2768.408334	21.351795
72.765668	2763.801235	21.356813
72.927386	2759.616807	21.361831
72.599544	2766.624960	21.366848
72.781504	2755.624907	21.371866
72.781611	2763.809125	21.376883
72.483258	2762.075411	21.381901
72.733349	2783.973994	21.386919
73.091328	2796.342209	21.391936
73.161631	2793.267316	21.396954
72.971728	2805.324908	21.401971
73.292147	2810.039443	21.406989
73.292901	2808.973591	21.412007
73.059680	2808.423939	21.417024
73.134902	2803.938845	21.422042
73.067881	2810.147653	21.427059
73.477559	2820.517667	21.432077
73.622323	2810.218575	21.437095
73.585023	2821.329349	21.442112
73.772246	2817.941050	21.447130
74.012294	2821.343730	21.452147
74.135953	2820.121353	21.457165
74.107336	2821.574812	21.462183
74.193954	2845.623632	21.467200
74.651227	2847.815668	21.472218
74.572288	2852.360389	21.477235
74.617217	2833.345068	21.482253
74.865778	2841.027267	21.487271
74.666970	2846.536243	21.492288
75.712684	2832.765171	21.497306
75.045836	2818.436975	21.502323
74.827148	2815.899968	21.507341
74.789888	2803.414518	21.512359
74.646820	2799.212729	21.517376
74.986979	2822.684996	21.522394
75.144961	2828.618059	21.527411
74.951155	2835.452526	21.532429
75.471936	2843.838139	21.537447
74.724625	2841.059358	21.542464
75.185702	2827.629374	21.547482
75.115617	2841.660024	21.552499
75.496243	2851.847467	21.557517
75.454042	2863.704326	21.562535
75.237560	2870.228395	21.567552
75.222857	2857.596660	21.572570
75.355592	2862.661503	21.577587
75.364616	2869.103822	21.582605
76.095665	2874.735130	21.587623
76.100069	2890.404238	21.592640
76.041010	2873.097324	21.597658
76.349014	2878.502487	21.602675
76.370882	2880.751121	21.607693
76.422041	2880.921768	21.612711
76.428612	2876.449966	21.617728
76.185048	2881.703761	21.622746
76.547255	2875.592546	21.627763
76.715340	2897.706801	21.632781
77.413556	2895.843436	21.637799
77.188673	2892.192128	21.642816
76.866304	2883.897662	21.647834
76.914740	2890.738580	21.652851
76.860618	2906.980345	21.657869
77.094903	2902.583108	21.662887
76.931343	2904.618300	21.667904
77.308080	2911.479779	21.672922
77.084012	2915.500489	21.677939
77.232852	2910.796907	21.682957
77.571633	2901.697539	21.687975
77.301256	2917.040045	21.692992
77.377848	2928.930079	21.698010
77.557271	2925.916261	21.703027
77.466132	2930.816158	21.708045
77.690551	2932.144747	21.713063
77.703095	2933.572912	21.718080
77.710759	2931.579959	21.723098
78.308034	2941.761976	21.728115
78.112407	2957.393340	21.733133
78.310563	2947.626654	21.738151
78.221762	2962.976996	21.743168
78.398511	2960.199432	21.748186
78.571303	2953.876187	21.753203
78.549340	2951.289721	21.758221
78.808586	2960.602836	21.763239
78.380364	2958.426008	21.768256
78.572372	2955.746707	21.773274
78.730844	2963.486766	21.778291
78.618565	2986.102184	21.783309
78.760154	2984.117801	21.788327
78.945492	2989.638151	21.793344
79.214765	2988.214147	21.798362
79.100191	2980.272288	21.803379
78.971784	2992.655285	21.808397
79.287893	2997.239098	21.813415
79.622641	2999.345501	21.818432
79.459885	3014.151832	21.823450
79.794124	3003.035500	21.828467
79.708748	3007.470704	21.833485
80.131019	3004.512802	21.838503
79.999049	2997.482835	21.843520
79.816290	3007.610330	21.848538
80.090331	3002.144718	21.853555
79.802115	3001.252582	21.858573
80.004270	3013.102248	21.863591
80.516087	3023.960232	21.868608
80.409168	3034.636613	21.873626
80.714029	3028.911969	21.878643
80.661799	3031.153185	21.883661
80.708449	3026.708180	21.888679
80.814580	3026.923680	21.893696
80.668932	3024.078121	21.898714
81.002155	3030.407490	21.903731
80.982746	3032.219672	21.908749
81.279804	3019.554794	21.913767
81.051565	3018.435036	21.918784
80.831488	3023.716887	21.923802
81.310415	3029.387552	21.928819
81.246083	3046.466166	21.933837
81.506902	3054.357070	21.938855
81.594540	3057.147209	21.943872
81.209668	3065.294809	21.948890
81.498608	3052.843050	21.953907
81.155386	3061.816420	21.958925
81.447297	3059.493811	21.963943
81.579407	3077.282498	21.968960
81.982228	3085.353492	21.973978
82.015848	3085.382555	21.978995
82.094697	3087.176540	21.984013
82.390738	3075.419241	21.989031
82.248456	3072.877833	21.994048
82.270870	3081.934100	21.999066
82.750085	3097.353310	22.004083
82.554780	3102.948409	22.009101
82.715780	3108.772422	22.014119
82.845052	3107.007771	22.019136
82.845549	3094.563091	22.024154
83.106084	3102.887914	22.029171
82.922118	3107.841394	22.034189
83.215857	3104.027569	22.039207
83.193318	3093.088234	22.044224
83.296098	3096.475075	22.049242
83.517556	3097.212845	22.054259
83.569866	3095.007380	22.059277
83.701932	3086.782591	22.064295
83.415134	3093.594349	22.069312
83.401844	3087.725016	22.074330
83.485769	3086.282812	22.079347
83.463879	3102.350957	22.084365
83.904431	3114.649092	22.089383
83.790966	3127.606879	22.094400
83.412678	3136.267589	22.099418
83.902525	3135.582304	22.104435
83.583763	3146.928792	22.109453
83.962176	3143.641111	22.114471
83.941720	3161.353532	22.119488
84.155798	3168.186886	22.124506
84.236599	3161.617739	22.129523
83.932241	3169.587526	22.134541
84.358242	3179.123606	22.139559
84.627163	3187.151820	22.144576
84.803341	3191.929676	22.149594
84.883557	3179.250500	22.154611
85.050628	3192.419067	22.159629
85.212601	3209.178187	22.164647
85.303753	3200.286489	22.169664
85.206871	3216.425410	22.174682
85.680288	3210.107109	22.179699
85.794589	3209.716943	22.184717
85.921508	3221.063462	22.189735
85.822424	3200.459703	22.194752
85.799895	3198.411863	22.199770
86.069538	3203.122705	22.204787
85.837013	3216.756921	22.209805
86.131767	3197.097914	22.214823
86.331228	3197.136975	22.219840
86.352380	3195.064989	22.224858
86.314586	3194.834204	22.229875
86.341673	3197.129265	22.234893
86.249816	3197.701887	22.239911
86.249748	3198.519180	22.244928
86.351527	3220.919651	22.249946
86.896578	3225.985379	22.254963
86.641474	3237.250549	22.259981
86.858652	3227.622275	22.264999
86.975648	3222.832524	22.270016
86.616847	3226.767311	22.275034
87.054504	3229.468936	22.280051
86.917073	3242.791403	22.285069
87.097072	3253.235488	22.290087
87.194406	3272.828938	22.295104
87.213302	3262.088540	22.300122
87.883574	3257.464833	22.305139
87.379514	3262.646053	22.310157
87.308182	3246.113968	22.315175
87.595027	3270.568938	22.320192
87.080091	3285.550648	22.325210
87.587516	3271.289014	22.330227
88.451278	3265.819958	22.335245
88.178529	3265.009501	22.340263
88.480373	3273.103185	22.345280
88.722924	3271.474913	22.350298
89.262789	3260.235445	22.355315
88.837049	3269.206034	22.360333
89.182884	3268.857921	22.365351
89.023590	3264.092553	22.370368
88.992014	3271.615748	22.375386
89.520801	3269.529555	22.380403
89.245365	3272.150596	22.385421
89.242645	3269.352239	22.390439
88.884431	3260.938297	22.395456
88.991110	3264.467048	22.400474
89.105474	3263.349322	22.405491
88.923010	3265.061311	22.410509
88.979742	3268.562884	22.415527
89.296864	3277.366240	22.420544
89.623442	3286.157409	22.425562
89.865385	3292.133863	22.430579
89.671778	3288.780044	22.435597
90.014005	3288.812838	22.440615
90.002960	3297.353900	22.445632
89.608680	3300.641820	22.450650
89.944839	3296.188663	22.455667
89.957316	3311.397025	22.460685
90.023344	3322.445022	22.465703
89.923208	3316.155311	22.470720
89.957152	3314.105211	22.475738
90.349436	3336.581861	22.480755
90.516056	3350.443544	22.485773
90.459364	3340.038808	22.490791
90.361686	3337.657700	22.495808
90.675305	3352.091546	22.500826
90.778213	3375.647949	22.505843
91.000170	3364.195586	22.510861
90.724846	3368.234723	22.515879
91.412248	3369.168348	22.520896
91.343487	3379.592994	22.525914
91.649439	3387.833302	22.530931
91.505260	3400.560567	22.535949
91.539230	3402.606491	22.540967
91.773820	3390.781156	22.545984
91.593375	3406.925815	22.551002
91.927768	3398.476092	22.556019
92.001549	3394.914288	22.561037
91.977950	3405.619283	22.566055
92.438671	3411.568294	22.571072
92.281788	3414.596932	22.576090
92.456784	3421.178590	22.581107
92.735707	3418.843509	22.586125
92.766626	3425.194646	22.591143
92.803847	3421.044392	22.596160
92.762652	3418.965749	22.601178
92.865500	3423.530992	22.606195
92.923671	3426.445752	22.611213
92.985224	3440.456765	22.616231
93.035001	3441.776069	22.621248
93.360155	3443.192783	22.626266
93.481214	3442.115276	22.631283
93.572918	3441.935531	22.636301
93.470853	3443.017721	22.641319
93.743489	3449.893492	22.646336
93.681373	3442.613986	22.651354
93.915522	3431.462313	22.656371
94.145076	3462.898684	22.661389
93.988442	3470.318230	22.666407
94.155031	3464.192260	22.671424
94.114766	3470.883524	22.676442
94.340590	3468.209572	22.681459
94.617905	3471.497971	22.686477
94.283487	3463.591402	22.691495
94.494576	3468.294285	22.696512
94.291678	3476.147463	22.701530
94.619743	3466.796781	22.706547
94.795798	3490.225917	22.711565
94.748979	3499.532057	22.716583
94.919193	3498.093274	22.721600
95.039438	3498.568655	22.726618
94.821262	3492.988535	22.731635
95.141042	3501.600241	22.736653
95.145580	3507.207739	22.741671
95.249823	3517.614127	22.746688
95.138898	3538.163585	22.751706
95.147709	3523.617574	22.756723
95.368163	3531.946496	22.761741
95.424322	3550.952217	22.766759
96.005362	3551.794768	22.771776
95.838715	3552.116767	22.776794
95.884720	3555.016238	22.781811
96.309437	3555.413358	22.786829
96.412613	3586.523615	22.791847
96.940505	3570.879577	22.796864
97.055593	3572.808576	22.801882
96.730460	3561.642138	22.806899
97.085729	3547.979018	22.811917
96.868920	3567.044037	22.816935
97.092087	3560.768522	22.821952
97.212745	3567.617096	22.826970
97.577563	3574.479266	22.831987
97.416278	3563.175122	22.837005
97.350557	3575.670273	22.842023
97.647057	3571.846036	22.847040
97.557361	3570.089956	22.852058
97.591742	3567.698803	22.857075
97.843046	3571.278925	22.862093
97.657414	3575.232428	22.867111
97.739578	3562.472695	22.872128
97.653104	3568.239349	22.877146
97.740264	3584.491155	22.882163
98.080591	3595.062524	22.887181
97.986068	3593.619444	22.892199
98.219475	3592.825334	22.897216
98.299928	3609.379064	22.902234
97.913657	3618.314590	22.907251
98.381725	3625.563662	22.912269
98.509182	3639.609636	22.917287
98.679232	3639.062215	22.922304
98.999623	3655.666900	22.927322
99.084802	3651.700001	22.932339
98.979175	3654.039106	22.937357
99.321799	3654.770269	22.942375
99.519428	3655.065150	22.947392
99.455237	3648.063452	22.952410
99.468032	3646.567989	22.957427
99.720219	3661.220544	22.962445
99.894272	3688.329486	22.967463
100.082120	3674.179347	22.972480
100.081468	3680.652736	22.977498
100.157314	3682.238622	22.982515
100.797310	3676.805220	22.987533
100.464134	3680.041782	22.992551
100.579980	3679.552923	22.997568
100.335878	3677.298321	23.002586
100.320207	3675.988664	23.007603
100.671606	3669.155296	23.012621
100.496807	3682.139822	23.017639
100.774008	3690.705913	23.022656
100.939937	3694.497023	23.027674
100.910499	3697.824347	23.032691
101.499294	3699.671151	23.037709
101.173655	3699.119806	23.042727
101.331997	3694.684501	23.047744
101.516434	3702.881670	23.052762
101.363027	3705.083400	23.057779
101.894845	3708.963665	23.062797
101.511180	3725.708383	23.067815
101.418423	3724.132321	23.072832
101.436642	3718.872906	23.077850
101.342095	3724.780717	23.082867
101.699712	3743.202995	23.087885
102.097858	3750.480610	23.092903
102.252369	3741.991526	23.097920
102.233722	3749.008477	23.102938
102.212578	3747.720190	23.107955
102.595744	3771.971450	23.112973
102.677953	3781.732825	23.117991
102.570869	3782.140264	23.123008
103.000726	3784.955879	23.128026
102.905632	3779.920683	23.133043
103.222513	3792.948469	23.138061
103.184344	3817.774154	23.143079
103.416038	3802.408361	23.148096
103.730035	3806.128968	23.153114
103.636389	3810.987035	23.158131
103.932318	3802.320218	23.163149
103.673904	3803.927490	23.168167
104.092191	3796.600721	23.173184
104.151624	3791.883695	23.178202
103.773433	3801.599107	23.183219
103.846141	3801.897309	23.188237
104.047871	3826.844003	23.193255
104.317945	3818.541298	23.198272
103.971319	3828.783413	23.203290
104.303995	3836.651427	23.208307
104.877718	3845.448536	23.213325
105.035849	3857.881334	23.218343
105.349598	3850.847016	23.223360
105.264570	3835.331157	23.228378
105.358481	3844.541807	23.233395
105.782281	3831.732490	23.238413
105.833615	3830.697975	23.243431
106.012440	3825.455294	23.248448
106.175625	3835.003711	23.253466
105.809838	3832.280600	23.258483
106.320987	3825.507384	23.263501
106.192239	3833.922517	23.268519
106.553415	3835.518360	23.273536
106.599512	3828.101891	23.278554
106.302180	3833.000315	23.283571
106.561789	3830.696712	23.288589
106.550022	3831.743535	23.293607
106.890742	3818.524719	23.298624
106.759287	3825.314276	23.303642
107.071144	3828.150578	23.308659
107.180812	3824.622905	23.313677
106.634806	3822.965029	23.318695
106.812022	3822.707763	23.323712
106.930352	3826.097314	23.328730
107.007659	3829.927905	23.333747
106.779217	3837.970135	23.338765
106.932503	3858.700774	23.343783
107.171156	3858.883760	23.348800
107.194753	3879.833105	23.353818
107.337673	3887.004135	23.358835
107.670557	3881.523769	23.363853
107.735207	3913.759187	23.368871
107.663840	3902.991134	23.373888
107.940327	3918.065912	23.378906
107.887539	3918.594701	23.383923
108.454755	3937.588106	23.388941
108.611254	3946.136487	23.393959
108.218705	3952.777503	23.398976
108.545735	3950.443451	23.403994
108.429435	3960.991305	23.409011
108.875420	3969.296977	23.414029
109.214427	3979.041636	23.419047
109.059280	3987.685630	23.424064
109.301930	3976.410507	23.429082
109.059754	3981.078595	23.434099
109.588567	3974.596894	23.439117
109.741238	3978.449716	23.444135
109.513181	3970.950129	23.449152
109.733014	3994.563744	23.454170
109.803101	4001.065737	23.459187
110.085976	4000.422100	23.464205
109.919999	4005.115401	23.469223
110.024608	3997.803361	23.474240
110.256171	4001.737644	23.479258
110.180362	4021.239777	23.484275
110.640337	4021.717309	23.489293
110.890125	4021.581518	23.494311
110.896878	4012.380850	23.499328
111.183474	4010.238515	23.504346
111.270682	4022.294962	23.509363
111.178661	4009.415214	23.514381
111.108873	4017.249031	23.519399
111.206971	4038.255967	23.524416
111.391319	4037.697903	23.529434
111.556653	4040.816732	23.534451
111.556499	4045.581468	23.539469
111.772419	4042.362974	23.544487
111.822497	4048.322603	23.549504
112.398450	4058.871104	23.554522
112.092701	4071.096853	23.559539
112.326534	4080.186882	23.564557
112.148668	4073.940023	23.569575
112.415709	4082.024133	23.574592
112.643097	4069.383696	23.579610
112.744776	4075.739156	23.584627
112.494156	4086.513628	23.589645
112.914560	4101.145890	23.594663
112.638398	4091.765142	23.599680
112.863475	4089.944785	23.604698
112.874966	4110.150349	23.609715
113.072490	4122.399284	23.614733
113.218904	4132.237675	23.619751
113.176024	4130.158427	23.624768
113.405555	4148.949610	23.629786
113.412959	4162.624145	23.634803
113.670081	4159.971284	23.639821
113.917255	4185.116958	23.644839
113.984399	4181.128494	23.649856
114.636994	4187.228394	23.654874
114.885616	4182.823706	23.659891
115.021625	4179.796348	23.664909
115.219907	4175.312967	23.669927
115.442752	4170.516855	23.674944
115.560056	4164.334972	23.679962
115.257366	4167.145710	23.684979
115.581782	4156.068373	23.689997
115.653628	4166.908521	23.695015
115.437879	4171.924283	23.700032
115.682181	4167.385661	23.705050
115.331283	4164.022994	23.710067
115.423053	4173.306637	23.715085
115.525717	4157.811807	23.720103
115.679771	4180.892063	23.725120
115.870295	4172.892485	23.730138
115.760833	4195.342259	23.735155
115.971619	4190.684754	23.740173
116.180265	4183.542452	23.745191
115.986332	4214.040824	23.750208
116.444632	4220.898860	23.755226
116.237530	4226.174247	23.760243
116.616189	4221.356310	23.765261
116.639972	4227.710136	23.770279
116.766634	4245.528622	23.775296
116.995981	4242.655917	23.780314
116.663157	4261.213762	23.785331
117.139372	4272.745866	23.790349
117.195672	4269.600159	23.795367
117.188871	4295.889608	23.800384
117.629858	4286.352841	23.805402
117.515641	4287.691440	23.810419
117.769275	4306.876095	23.815437
117.690001	4310.945288	23.820455
118.040093	4317.919678	23.825472
118.276176	4306.750919	23.830490
118.359200	4339.470034	23.835507
118.482355	4327.925803	23.840525
119.284136	4338.669477	23.845543
118.946981	4337.059321	23.850560
119.333405	4324.621546	23.855578
119.427635	4333.681244	23.860595
119.285327	4332.721214	23.865613
119.477469	4330.865718	23.870631
119.712080	4325.430571	23.875648
119.627999	4324.374302	23.880666
119.730979	4322.720164	23.885683
119.703590	4323.574315	23.890701
119.820966	4332.242372	23.895719
119.707821	4340.861510	23.900736
120.026633	4354.514681	23.905754
119.814822	4352.282598	23.910771
120.193261	4349.401774	23.915789
120.248071	4364.104143	23.920807
120.252777	4379.958177	23.925824
120.506037	4372.037508	23.930842
120.742936	4388.907576	23.935859
120.509628	4402.065763	23.940877
121.205233	4412.713640	23.945895
120.881101	4408.864184	23.950912
121.157455	4416.222084	23.955930
121.236583	4424.940215	23.960947
121.465327	4446.850974	23.965965
121.672760	4437.739738	23.970983
121.637195	4449.708528	23.976000
121.785551	4438.480938	23.981018
121.921655	4447.091236	23.986035
122.161641	4454.196486	23.991053
122.340843	4450.954446	23.996071
122.565718	4465.367376	24.001088
122.394357	4459.429149	24.006106
122.575597	4456.600183	24.011123
122.643585	4479.015531	24.016141
123.342143	4492.202901	24.021159
123.304218	4488.976650	24.026176
123.535596	4485.584634	24.031194
123.512202	4488.974517	24.036211
123.476593	4492.417604	24.041229
123.919399	4480.151503	24.046247
123.708159	4494.227440	24.051264
123.726671	4495.526408	24.056282
124.006625	4488.847019	24.061299
123.863903	4483.735993	24.066317
123.943355	4487.193534	24.071335
124.013980	4513.888300	24.076352
124.356877	4499.332636	24.081370
124.408876	4505.253144	24.086387
124.088384	4518.466782	24.091405
124.745762	4526.609471	24.096423
124.726630	4546.129275	24.101440
124.817683	4538.054603	24.106458
124.626456	4537.395576	24.111475
124.873320	4556.358021	24.116493
125.360314	4555.410932	24.121511
125.065208	4564.202789	24.126528
125.227566	4570.898056	24.131546
125.577588	4570.684672	24.136563
125.804647	4590.386702	24.141581
126.201589	4585.261282	24.146599
126.471617	4594.264129	24.151616
126.337029	4583.188706	24.156634
127.013786	4582.026390	24.161651
126.894436	4587.314172	24.166669
126.750010	4587.643937	24.171687
126.861540	4579.725713	24.176704
126.850997	4581.459834	24.181722
126.713572	4586.454125	24.186739
126.725983	4596.361018	24.191757
127.344039	4614.783821	24.196775
127.020704	4616.389301	24.201792
127.100267	4618.408166	24.206810
127.531681	4629.779423	24.211827
127.678330	4641.508788	24.216845
127.625982	4643.589613	24.221863
127.342547	4658.233572	24.226880
127.854131	4663.311216	24.231898
127.891334	4674.471243	24.236915
127.768833	4673.077571	24.241933
128.353467	4689.649545	24.246951
128.366915	4698.939749	24.251968
128.699723	4700.321851	24.256986
129.273180	4695.971229	24.262003
129.097337	4692.358243	24.267021
129.214004	4698.293339	24.272039
129.067504	4726.897326	24.277056
129.130855	4716.255675	24.282074
129.272781	4723.371345	24.287091
129.235446	4735.474515	24.292109
129.584456	4741.900019	24.297127
129.503084	4766.636708	24.302144
129.777494	4755.646351	24.307162
130.357773	4766.100125	24.312179
130.332982	4785.286490	24.317197
130.706160	4784.050689	24.322215
130.622258	4783.986173	24.327232
130.621833	4785.661947	24.332250
130.899164	4792.519036	24.337267
131.203162	4792.698720	24.342285
131.386423	4805.911654	24.347303
131.630951	4812.203257	24.352320
131.525349	4820.835982	24.357338
131.663749	4810.389758	24.362355
131.805941	4814.242157	24.367373
131.942260	4807.267048	24.372391
132.066439	4806.277130	24.377408
132.005868	4807.451777	24.382426
132.115973	4796.286555	24.387443
131.996450	4831.102940	24.392461
132.427686	4828.764929	24.397479
132.328866	4835.394007	24.402496
132.325235	4841.609292	24.407514
132.598439	4854.406978	24.412531
132.800581	4863.195587	24.417549
133.181034	4875.126281	24.422567
133.055534	4875.725389	24.427584
132.912504	4868.205807	24.432602
133.635138	4874.253855	24.437619
133.651781	4879.659435	24.442637
133.882957	4880.731941	24.447655
133.959316	4876.790994	24.452672
134.381620	4878.449690	24.457690
134.004879	4870.910450	24.462707
134.195125	4881.818546	24.467725
134.805788	4869.169258	24.472743
134.446660	4869.940445	24.477760
134.160535	4888.961044	24.482778
134.890130	4900.060376	24.487795
134.519314	4904.540919	24.492813
134.721728	4906.559603	24.497831
134.880769	4924.340835	24.502848
134.983246	4936.827790	24.507866
135.275932	4929.977198	24.512883
135.286310	4942.965641	24.517901
135.329637	4958.848924	24.522919
135.275082	4965.223868	24.527936
135.620806	4965.192310	24.532954
136.121522	4980.094836	24.537971
135.623820	4998.963108	24.542989
135.985200	4992.711827	24.548007
136.292870	5005.794915	24.553024
136.361399	5019.130540	24.558042
136.673303	5020.709453	24.563059
136.902214	5033.492948	24.568077
137.125473	5036.386245	24.573095
137.590156	5037.800926	24.578112
138.209006	5037.265138	24.583130
138.279903	5022.195215	24.588147
138.120527	5027.025540	24.593165
138.315319	5021.189606	24.598183
138.336765	5014.227873	24.603200
138.458226	5026.909814	24.608218
138.758944	5019.988557	24.613235
138.499630	5014.285144	24.618253
138.719234	5005.538139	24.623271
138.787379	5015.956613	24.628288
138.546015	5017.102088	24.633306
139.121535	5007.769450	24.638323
138.681081	5022.292829	24.643341
139.050440	5039.917383	24.648359
139.265055	5037.774206	24.653376
139.438134	5044.158032	24.658394
139.510382	5050.267940	24.663411
139.483797	5067.399230	24.668429
139.724846	5078.661706	24.673447
139.865102	5071.776389	24.678464
139.786710	5075.129025	24.683482
140.277266	5087.944144	24.688499
140.333942	5103.649761	24.693517
140.717657	5106.210227	24.698535
140.924755	5095.734350	24.703552
140.936905	5101.901852	24.708570
140.929002	5101.862970	24.713587
141.027775	5120.604483	24.718605
141.460787	5121.021937	24.723623
141.407549	5131.444401	24.728640
141.474358	5134.024948	24.733658
141.665894	5128.991959	24.738675
141.725550	5140.501403	24.743693
141.886053	5139.214881	24.748711
142.110133	5137.374096	24.753728
142.178030	5143.397742	24.758746
142.132812	5154.713873	24.763763
142.390657	5168.216398	24.768781
142.700093	5175.460914	24.773799
142.593944	5177.912155	24.778816
142.283851	5177.227065	24.783834
142.736597	5192.932690	24.788851
142.630326	5218.477445	24.793869
143.119376	5210.997368	24.798887
143.584328	5227.301864	24.803904
143.586896	5240.353269	24.808922
143.495247	5235.789525	24.813939
143.297555	5244.574722	24.818957
143.135970	5247.334774	24.823975
143.799348	5274.186077	24.828992
144.202590	5277.401295	24.834010
144.765385	5276.877520	24.839027
144.734445	5296.151758	24.844045
144.689493	5298.472026	24.849063
144.790164	5286.342153	24.854080
145.170666	5299.194925	24.859098
145.344885	5308.950717	24.864115
145.451000	5328.982755	24.869133
145.507734	5320.739314	24.874151
145.518272	5332.851967	24.879168
145.373314	5336.190852	24.884186
145.743122	5342.021367	24.889203
146.054964	5348.495001	24.894221
146.111744	5348.454093	24.899239
146.277431	5335.501926	24.904256
146.470473	5368.924002	24.909274
146.474057	5379.482141	24.914291
146.582581	5377.091455	24.919309
147.192221	5395.335057	24.924327
147.419058	5398.555430	24.929344
147.283801	5419.650820	24.934362
147.480796	5405.401923	24.939379
147.384611	5410.251849	24.944397
147.789309	5406.818792	24.949415
147.735010	5414.073513	24.954432
148.230880	5430.010470	24.959450
147.950091	5430.094638	24.964467
147.844519	5436.121073	24.969485
148.284137	5450.102926	24.974503
148.706948	5451.368246	24.979520
148.415578	5457.935689	24.984538
148.693949	5461.672035	24.989555
148.461530	5469.606688	24.994573
148.580862	5482.981565	24.999591
149.459458	5501.026895	25.004608
149.346370	5530.531276	25.009626
149.677234	5521.241123	25.014643
149.974139	5528.719400	25.019661
149.844731	5529.494004	25.024679
150.393774	5533.607748	25.029696
150.330586	5549.237934	25.034714
150.847387	5550.339288	25.039731
150.660781	5554.087909	25.044749
150.779661	5554.784477	25.049767
151.007677	5552.090913	25.054784
151.183531	5546.651667	25.059802
151.257937	5553.955274	25.064819
151.550241	5561.091369	25.069837
151.719215	5572.760257	25.074855
151.621184	5560.675210	25.079872
151.704078	5579.303738	25.084890
152.082865	5581.733980	25.089907
152.279157	5584.787762	25.094925
152.227159	5600.325980	25.099943
152.310846	5600.888977	25.104960
152.126731	5610.407273	25.109978
152.266234	5606.268677	25.114995
152.465730	5618.151877	25.120013
152.329044	5635.676834	25.125031
152.855018	5634.026695	25.130048
152.580668	5642.480244	25.135066
152.788165	5657.196008	25.140083
153.204168	5662.747320	25.145101
153.365021	5693.722704	25.150119
153.742995	5685.935908	25.155136
153.657605	5694.153904	25.160154
154.023722	5690.651166	25.165171
154.534590	5717.305565	25.170189
154.283161	5728.575068	25.175207
154.683001	5714.708577	25.180224
154.535685	5709.197851	25.185242
154.885903	5724.694936	25.190259
154.822323	5746.644400	25.195277
154.981771	5751.748299	25.200295
155.053315	5755.437383	25.205312
155.190506	5772.944410	25.210330
155.416276	5772.071525	25.215347
155.581939	5789.716800	25.220365
155.561993	5805.379079	25.225383
156.046385	5801.512629	25.230400
156.238974	5804.774971	25.235418
156.281561	5820.198552	25.240435
156.772287	5824.559841	25.245453
156.828290	5831.431120	25.250471
157.122811	5824.085274	25.255488
157.283386	5838.306524	25.260506
157.166334	5847.080701	25.265523
157.380484	5852.043685	25.270541
157.166625	5852.522369	25.275559
157.876761	5860.805495	25.280576
157.864713	5885.182836	25.285594
157.944320	5885.567355	25.290611
158.114391	5896.856718	25.295629
157.863790	5893.178627	25.300647
158.520745	5910.126233	25.305664
158.759215	5919.930855	25.310682
158.855058	5918.945550	25.315699
158.815509	5928.985119	25.320717
158.947076	5951.837025	25.325735
159.195748	5949.367182	25.330752
159.329962	5949.752131	25.335770
159.405884	5970.675944	25.340787
159.756132	5967.050552	25.345805
160.009448	5962.319738	25.350823
160.259766	5979.952029	25.355840
160.501910	5983.556670	25.360858
160.899610	5989.503706	25.365875
160.978527	5981.389345	25.370893
161.000027	5990.259626	25.375911
161.183197	5984.889111	25.380928
161.255956	5988.650895	25.385946
161.221989	5985.459119	25.390963
161.432344	5996.816713	25.395981
161.501166	6024.045935	25.400999
161.699953	6010.606956	25.406016
161.626837	6023.135210	25.411034
161.897189	6035.238947	25.416051
161.933378	6041.902534	25.421069
161.425865	6056.424163	25.426087
162.550824	6065.669738	25.431104
162.738055	6082.790434	25.436122
162.910291	6075.214241	25.441139
162.995713	6089.703297	25.446157
163.159959	6095.188863	25.451175
163.663139	6086.757850	25.456192
164.054012	6085.239456	25.461210
163.971831	6089.860862	25.466227
164.446913	6080.408340	25.471245
164.335160	6073.190934	25.476263
164.294970	6074.971857	25.481280
164.574191	6077.462337	25.486298
164.341379	6084.049896	25.491315
164.397957	6095.145521	25.496333
164.553297	6103.306236	25.501351
164.838181	6108.991596	25.506368
164.920995	6115.978275	25.511386
165.086375	6133.433402	25.516403
165.391219	6149.929912	25.521421
165.213968	6151.572045	25.526439
165.333005	6165.730365	25.531456
165.533593	6180.758052	25.536474
165.664313	6195.991032	25.541491
166.153089	6196.030740	25.546509
166.133232	6205.827821	25.551527
166.808927	6202.706180	25.556544
167.214897	6206.966601	25.561562
167.061764	6226.800060	25.566579
167.304308	6216.766085	25.571597
167.067760	6228.052779	25.576615
167.645753	6221.171814	25.581632
167.424250	6234.803682	25.586650
167.639705	6246.402390	25.591667
167.983129	6234.048180	25.596685
167.839814	6256.826241	25.601703
168.295848	6264.796388	25.606720
168.484377	6279.959258	25.611738
168.826847	6282.101465	25.616755
168.635416	6274.035559	25.621773
168.509779	6303.124492	25.626791
168.565266	6323.514260	25.631808
168.852227	6331.474574	25.636826
168.926243	6343.201466	25.641843
169.583469	6355.988123	25.646861
169.504326	6377.960335	25.651879
169.794927	6374.361245	25.656896
169.924788	6391.856391	25.661914
170.156692	6420.865203	25.666931
170.528162	6406.442845	25.671949
170.414316	6416.391832	25.676967
170.615359	6429.465773	25.681984
170.979430	6446.941185	25.687002
170.867446	6455.659735	25.692020
171.081229	6456.750585	25.697037
171.198629	6473.398113	25.702055
171.513463	6466.184073	25.707072
171.829150	6492.684998	25.712090
171.739489	6504.179161	25.717108
172.287215	6504.355617	25.722125
172.286309	6511.215333	25.727143
172.530474	6516.878430	25.732160
173.001393	6536.366602	25.737178
172.943606	6535.209755	25.742196
172.968317	6539.218239	25.747213
173.101898	6552.354620	25.752231
173.282344	6556.542142	25.757248
173.797561	6556.336493	25.762266
173.792764	6559.863148	25.767284
174.316197	6576.488590	25.772301
174.183458	6585.781620	25.777319
174.136452	6589.610590	25.782336
174.128108	6579.735972	25.787354
174.167103	6604.430467	25.792372
175.223405	6603.901512	25.797389
175.015308	6613.436189	25.802407
175.273188	6618.374866	25.807424
175.210621	6619.683862	25.812442
175.140819	6633.547755	25.817460
175.626617	6648.645325	25.822477
175.684900	6651.753622	25.827495
175.864466	6646.777258	25.832512
176.389705	6679.772754	25.837530
176.030816	6687.361910	25.842548
176.172879	6684.469321	25.847565
176.314752	6691.092095	25.852583
176.473629	6693.275719	25.857600
176.951115	6697.740252	25.862618
176.953099	6721.546375	25.867636
177.403129	6719.874024	25.872653
177.079631	6731.441641	25.877671
177.172347	6740.303729	25.882688
177.777228	6748.749635	25.887706
177.750763	6774.923236	25.892724
178.139940	6775.388153	25.897741
178.366633	6785.577232	25.902759
179.038043	6785.523765	25.907776
179.365851	6791.456667	25.912794
179.192739	6799.853941	25.917812
179.669600	6798.592986	25.922829
179.450952	6804.374396	25.927847
179.649308	6805.625334	25.932864
180.102311	6794.048814	25.937882
180.122796	6798.098228	25.942900
180.337243	6806.795328	25.947917
180.145651	6814.545919	25.952935
180.632343	6816.536787	25.957952
180.698539	6823.254027	25.962970
180.634109	6837.566913	25.967988
180.636722	6850.236101	25.973005
181.135215	6855.670646	25.978023
181.284090	6882.882615	25.983040
181.518931	6879.777768	25.988058
181.319269	6896.890032	25.993076
181.796010	6900.913705	25.998093
181.738953	6920.605363	26.003111
182.042493	6912.393554	26.008128
182.382782	6933.478164	26.013146
182.237155	6943.510704	26.018164
182.843994	6953.793811	26.023181
183.070344	6969.285816	26.028199
183.069417	6972.360643	26.033216
183.511196	6974.622003	26.038234
183.356883	6991.448074	26.043252
183.659152	7001.397984	26.048269
183.636979	7013.746916	26.053287
183.585472	7018.345411	26.058304
184.014250	7026.940276	26.063322
184.158114	7045.516758	26.068340
184.619367	7043.738560	26.073357
184.995505	7066.850171	26.078375
184.931540	7061.361032	26.083392
185.622432	7060.158417	26.088410
185.418116	7092.271940	26.093428
185.603945	7089.915479	26.098445
186.154975	7087.383691	26.103463
186.232760	7089.913130	26.108480
186.347744	7091.141636	26.113498
186.311089	7114.293167	26.118516
186.741429	7111.622224	26.123533
186.821067	7130.440967	26.128551
186.786185	7126.398519	26.133568
187.128455	7114.898343	26.138586
187.225517	7131.187639	26.143604
187.300307	7134.436645	26.148621
187.748670	7135.015447	26.153639
187.424404	7134.667328	26.158656
187.723786	7151.867533	26.163674
187.943737	7170.382761	26.168692
187.806333	7176.224129	26.173709
188.165179	7194.673906	26.178727
188.147107	7208.766033	26.183744
188.423642	7209.340937	26.188762
188.546390	7238.275567	26.193780
188.538317	7245.810963	26.198797
189.041827	7266.279146	26.203815
189.001685	7275.299739	26.208832
189.564052	7300.167969	26.213850
189.714444	7299.631947	26.218868
189.764842	7318.832215	26.223885
190.186353	7325.732756	26.228903
189.946599	7354.240758	26.233920
190.600075	7362.018963	26.238938
190.321368	7372.204503	26.243956
190.570807	7391.560997	26.248973
190.943194	7406.690637	26.253991
191.307151	7430.457712	26.259008
191.451992	7427.830738	26.264026
191.881547	7460.107275	26.269044
192.039489	7462.775537	26.274061
192.739453	7450.099988	26.279079
192.825028	7459.610281	26.284096
193.632985	7463.466750	26.289114
193.558097	7485.343713	26.294132
193.740853	7482.245780	26.299149
193.910273	7479.302846	26.304167
193.594290	7491.213957	26.309184
193.923527	7477.837239	26.314202
194.050128	7485.026794	26.319220
194.056127	7477.606564	26.324237
194.617022	7502.505286	26.329255
194.653143	7497.507463	26.334272
194.785698	7493.766475	26.339290
194.592694	7502.358007	26.344308
195.115535	7529.534507	26.349325
195.191606	7525.435820	26.354343
194.861892	7538.095096	26.359360
195.417139	7546.727635	26.364378
195.079552	7576.406831	26.369396
195.606253	7597.737193	26.374413
195.756721	7588.499658	26.379431
195.932386	7618.432016	26.384448
196.512609	7609.916586	26.389466
196.165277	7640.671810	26.394484
196.797347	7648.136288	26.399501
197.041490	7664.391594	26.404519
197.167050	7680.801979	26.409536
197.659396	7685.760538	26.414554
197.671607	7695.346891	26.419572
197.874442	7717.535865	26.424589
198.326821	7710.484413	26.429607
198.177659	7735.718989	26.434624
198.689973	7739.074620	26.439642
198.792923	7737.861985	26.444660
198.881076	7745.061949	26.449677
199.233674	7769.196865	26.454695
199.293748	7775.971444	26.459712
199.416573	7773.292130	26.464730
199.717871	7786.350634	26.469748
200.093369	7810.805542	26.474765
200.308273	7801.025594	26.479783
200.455552	7796.945789	26.484800
200.692946	7818.024955	26.489818
200.646351	7835.862756	26.494836
200.824292	7828.614008	26.499853
201.353411	7824.029253	26.504871
201.052226	7846.281205	26.509888
201.700592	7844.998138	26.514906
202.013335	7861.413227	26.519924
202.076604	7854.435452	26.524941
202.372205	7870.085452	26.529959
202.240856	7882.014396	26.534976
202.802093	7881.610531	26.539994
202.704363	7888.435646	26.545012
202.812459	7892.796942	26.550029
202.897442	7909.260739	26.555047
203.054927	7934.919117	26.560064
203.168180	7942.290664	26.565082
203.023618	7958.321437	26.570100
203.260300	7982.078080	26.575117
203.392250	7987.221512	26.580135
203.274914	8014.839360	26.585152
203.428712	8044.494166	26.590170
203.809491	8059.051227	26.595188
204.079188	8089.445456	26.600205
204.470684	8110.047449	26.605223
204.537711	8129.846131	26.610240
205.087855	8138.304984	26.615258
205.623124	8162.936461	26.620276
205.833528	8180.041431	26.625293
206.291398	8170.112420	26.630311
206.874403	8195.318124	26.635328
206.825345	8200.970416	26.640346
206.774117	8204.817014	26.645364
207.077461	8206.839933	26.650381
207.191863	8216.930346	26.655399
207.268666	8236.243148	26.660416
207.640782	8238.473673	26.665434
208.264701	8258.675932	26.670452
208.092531	8268.146593	26.675469
208.460542	8270.232875	26.680487
208.679166	8284.438079	26.685504
208.620217	8306.348985	26.690522
208.851189	8290.384660	26.695540
208.886395	8306.832676	26.700557
209.313022	8318.153064	26.705575
209.284083	8337.248742	26.710592
209.565145	8347.254992	26.715610
209.960858	8351.621667	26.720628
210.390332	8372.638330	26.725645
210.440262	8378.556308	26.730663
210.555665	8391.590891	26.735680
211.160119	8392.916639	26.740698
211.095447	8403.124974	26.745716
211.045820	8415.684324	26.750733
211.500344	8422.308943	26.755751
211.717834	8433.780539	26.760768
211.770967	8437.073561	26.765786
212.309926	8445.008279	26.770804
212.316531	8460.226932	26.775821
212.964661	8470.193093	26.780839
212.903307	8477.919038	26.785856
213.183246	8467.354463	26.790874
212.952354	8482.706107	26.795892
213.488239	8484.481915	26.800909
214.559425	8474.203274	26.805927
215.531609	8452.226266	26.810944
215.785958	8444.787392	26.815962
215.953886	8426.949286	26.820980
215.820196	8409.301234	26.825997
216.294558	8406.579487	26.831015
215.644551	8397.682461	26.836032
215.817044	8375.156367	26.841050
215.859738	8379.942906	26.846068
215.698190	8372.670448	26.851085
216.301699	8389.145166	26.856103
215.917787	8397.908925	26.861120
216.096960	8411.420543	26.866138
216.039959	8419.234745	26.871156
216.186624	8438.069964	26.876173
216.637773	8446.327949	26.881191
216.487605	8466.061329	26.886208
216.523681	8470.370097	26.891226
216.849779	8493.651171	26.896244
216.941663	8524.820735	26.901261
217.066282	8527.081954	26.906279
217.189619	8547.202669	26.911296
217.239820	8567.674185	26.916314
217.586359	8593.094453	26.921332
217.823522	8625.387041	26.926349
218.073216	8638.057796	26.931367
218.530777	8666.532500	26.936384
218.682853	8691.817283	26.941402
219.183953	8710.670668	26.946420
218.927676	8731.047313	26.951437
219.238546	8741.756211	26.956455
219.606512	8762.732357	26.961472
219.859105	8786.932609	26.966490
220.255288	8808.451582	26.971508
220.177746	8831.152377	26.976525
220.729037	8841.137136	26.981543
220.973067	8865.579950	26.986560
221.205950	8877.943332	26.991578
221.842788	8892.339917	26.996596
221.970070	8916.041206	27.001613
222.655530	8900.385565	27.006631
222.845596	8912.047929	27.011648
223.179568	8926.604071	27.016666
223.938958	8919.593524	27.021684
223.968711	8925.845075	27.026701
224.122064	8916.095880	27.031719
224.709065	8921.020291	27.036736
224.514523	8917.247155	27.041754
224.933416	8913.925616	27.046772
224.742832	8910.203815	27.051789
224.925293	8900.603416	27.056807
224.753035	8914.638253	27.061824
224.735791	8944.981497	27.066842
224.976009	8940.827757	27.071860
225.080053	8967.588353	27.076877
225.199709	8977.697287	27.081895
225.118178	9012.170042	27.086912
225.257503	9030.361279	27.091930
225.689934	9040.913240	27.096948
225.806492	9060.491438	27.101965
226.116585	9065.712915	27.106983
226.850313	9092.832056	27.112000
227.067589	9099.248826	27.117018
227.535073	9108.907323	27.122036
227.638886	9115.327093	27.127053
227.715226	9121.986133	27.132071
228.352821	9154.694126	27.137088
228.434337	9150.965909	27.142106
228.835041	9150.068672	27.147124
228.424917	9175.900029	27.152141
228.960034	9179.234090	27.157159
229.117505	9191.585758	27.162176
229.140766	9201.625690	27.167194
229.372867	9218.057874	27.172212
229.560491	9232.160349	27.177229
230.054982	9231.472892	27.182247
230.324123	9248.454308	27.187264
230.154055	9264.893120	27.192282
230.262334	9277.282914	27.197300
230.406082	9311.702555	27.202317
231.049708	9313.959271	27.207335
231.136257	9340.173574	27.212352
230.835921	9349.280082	27.217370
231.452202	9364.636756	27.222388
231.727190	9379.130591	27.227405
232.588827	9382.811687	27.232423
232.747323	9386.930335	27.237440
232.901528	9401.689907	27.242458
233.849097	9408.257903	27.247476
233.952410	9414.168235	27.252493
233.991179	9425.864639	27.257511
234.049723	9421.287864	27.262528
234.273032	9431.313007	27.267546
234.689418	9444.245164	27.272564
234.475233	9455.251609	27.277581
234.919413	9453.133327	27.282599
234.940707	9470.613583	27.287616
234.957721	9484.072560	27.292634
235.231514	9493.380471	27.297652
235.504935	9512.805702	27.302669
235.614476	9538.888926	27.307687
235.546470	9546.495969	27.312704
235.848151	9581.683320	27.317722
236.243908	9591.492599	27.322740
236.543472	9616.517385	27.327757
236.534692	9627.987844	27.332775
236.936273	9639.801697	27.337792
237.004245	9665.513895	27.342810
237.431421	9676.117562	27.347828
237.591658	9694.797635	27.352845
238.347760	9706.244183	27.357863
238.794151	9736.450105	27.362880
238.999097	9741.834116	27.367898
239.333813	9742.260871	27.372916
239.221970	9760.568485	27.377933
239.706753	9777.181635	27.382951
239.980150	9779.780015	27.387968
239.600013	9805.026886	27.392986
239.901971	9818.156277	27.398004
240.124704	9834.161339	27.403021
240.344795	9847.484667	27.408039
240.986958	9859.021833	27.413056
240.890319	9879.124647	27.418074
241.585259	9895.391263	27.423092
241.648105	9907.861523	27.428109
242.043868	9921.504064	27.433127
242.272271	9927.649930	27.438144
242.430573	9938.762952	27.443162
242.536953	9950.542309	27.448180
242.806915	9963.127274	27.453197
242.861321	9975.650973	27.458215
243.277040	9983.897500	27.463232
242.931297	10007.007420	27.468250
243.644911	10018.552590	27.473268
243.728562	10050.442544	27.478285
244.011978	10060.795302	27.483303
244.704045	10075.385500	27.488320
244.549762	10094.950636	27.493338
244.980086	10096.037480	27.498356
245.041775	10126.500694	27.503373
245.394301	10120.020825	27.508391
245.884492	10138.657146	27.513408
245.968390	10160.942444	27.518426
245.919239	10155.256791	27.523444
246.428634	10169.634633	27.528461
246.254168	10172.972708	27.533479
247.031924	10194.973268	27.538496
247.102734	10214.165786	27.543514
247.509609	10217.361348	27.548532
247.420287	10241.337503	27.553549
247.712776	10252.598725	27.558567
248.006241	10269.386579	27.563584
247.952515	10290.054719	27.568602
248.401371	10304.151220	27.573620
248.945439	10312.809184	27.578637
249.024825	10338.749025	27.583655
249.627458	10340.503785	27.588672
249.592843	10358.323525	27.593690
250.541450	10360.284235	27.598708
250.753799	10368.165963	27.603725
251.011147	10373.457243	27.608743
251.686572	10372.553156	27.613760
251.900525	10373.549728	27.618778
252.030696	10355.659777	27.623796
252.472145	10366.985485	27.628813
252.373128	10366.164445	27.633831
252.745447	10366.653540	27.638848
252.689760	10373.733516	27.643866
252.947103	10389.227685	27.648884
252.781028	10398.308666	27.653901
252.777965	10413.535508	27.658919
253.070036	10420.987372	27.663936
253.422242	10450.680055	27.668954
253.227689	10464.701028	27.673972
253.451967	10477.757933	27.678989
254.057097	10499.316360	27.684007
253.954190	10524.448452	27.689024
254.210751	10544.950646	27.694042
254.303206	10564.466926	27.699060
254.573477	10585.849981	27.704077
254.863068	10609.164603	27.709095
255.273510	10622.268857	27.714112
255.463429	10660.005751	27.719130
256.128708	10670.999287	27.724148
256.877460	10678.748434	27.729165
256.792362	10700.457404	27.734183
257.219156	10707.897386	27.739200
257.187729	10728.846002	27.744218
257.584753	10739.682238	27.749236
258.008975	10751.341927	27.754253
258.401044	10767.141125	27.759271
258.816149	10777.014113	27.764288
258.990257	10793.499254	27.769306
258.815754	10796.236398	27.774324
259.371299	10806.345377	27.779341
259.533313	10821.095519	27.784359
260.020029	10828.187706	27.789376
260.487471	10841.876701	27.794394
260.394673	10838.313174	27.799412
260.470294	10860.734735	27.804429
260.665611	10876.609875	27.809447
261.118651	10885.695195	27.814464
261.248433	10911.073047	27.819482
261.293301	10927.869579	27.824500
261.776102	10936.124425	27.829517
261.534520	10950.697943	27.834535
262.392850	10966.954419	27.839552
262.287900	10978.934881	27.844570
262.621385	10989.578537	27.849588
262.572125	11007.932380	27.854605
262.700053	11020.837063	27.859623
263.009043	11038.663814	27.864640
263.130348	11056.509777	27.869658
263.420799	11071.539862	27.874676
263.701107	11102.894455	27.879693
263.981381	11126.660407	27.884711
264.216069	11142.436347	27.889728
264.399858	11180.880546	27.894746
264.503873	11201.043251	27.899764
265.240893	11212.297883	27.904781
264.861305	11248.090670	27.909799
265.380259	11272.914007	27.914816
266.007035	11298.045714	27.919834
266.191772	11316.271442	27.924852
266.857899	11342.286922	27.929869
266.412955	11351.954939	27.934887
267.186942	11371.536070	27.939904
267.641212	11395.981114	27.944922
267.728393	11406.943044	27.949940
268.548545	11421.230499	27.954957
268.853242	11442.077247	27.959975
268.981427	11449.187191	27.964992
269.393895	11478.700871	27.970010
269.461361	11477.502485	27.975028
269.742927	11504.421557	27.980045
270.059634	11517.900481	27.985063
270.533789	11531.972618	27.990080
270.436947	11536.438099	27.995098
270.523218	11552.921989	28.000116
270.956185	11567.305841	28.005133
271.204550	11582.437107	28.010151
271.626105	11600.103294	28.015168
271.810445	11610.659348	28.020186
271.675017	11643.655355	28.025204
272.235461	11655.006437	28.030221
272.455034	11674.277753	28.035239
272.900056	11691.422573	28.040256
273.438767	11715.328683	28.045274
274.168852	11698.303983	28.050292
274.675858	11709.749805	28.055309
274.852500	11715.417258	28.060327
275.057355	11700.946753	28.065344
275.554130	11720.892388	28.070362
275.230436	11726.417978	28.075380
275.943453	11732.397820	28.080397
275.885548	11746.331157	28.085415
276.167371	11747.082626	28.090432
276.344190	11773.820926	28.095450
276.564433	11779.348058	28.100468
276.462265	11794.424777	28.105485
276.741752	11822.602867	28.110503
276.954437	11830.027539	28.115520
277.095769	11850.347972	28.120538
277.176697	11866.016098	28.125556
277.970103	11876.953062	28.130573
277.529779	11898.682156	28.135591
278.126468	11929.029681	28.140608
279.004324	11933.670643	28.145626
279.646191	11941.113487	28.150644
280.358228	11952.112003	28.155661
280.695218	11952.407672	28.160679
280.992764	11942.088433	28.165696
281.229761	11946.442939	28.170714
281.317163	11936.701231	28.175732
281.677549	11943.587107	28.180749
281.940377	11945.111427	28.185767
282.119184	11934.134282	28.190784
281.850682	11944.229650	28.195802
281.911416	11947.506386	28.200820
282.046164	11963.795974	28.205837
282.169308	11980.152098	28.210855
282.361217	11984.037429	28.215872
282.340686	12008.854132	28.220890
282.673469	12038.140932	28.225908
283.188738	12059.717886	28.230925
283.071890	12079.836248	28.235943
283.434733	12100.840477	28.240960
283.740400	12120.260398	28.245978
283.650375	12153.239706	28.250996
284.146015	12171.760111	28.256013
284.609422	12205.684097	28.261031
284.437861	12227.808056	28.266048
284.615053	12255.267964	28.271066
285.033646	12277.795558	28.276084
285.756959	12301.681500	28.281101
285.994646	12327.612582	28.286119
286.332730	12356.523284	28.291136
286.887713	12383.552287	28.296154
286.662489	12398.763350	28.301172
287.131220	12429.726995	28.306189
287.606014	12458.830378	28.311207
287.576988	12482.505257	28.316224
288.061991	12503.150266	28.321242
288.181522	12539.319623	28.326260
288.705739	12554.692222	28.331277
288.896206	12578.290011	28.336295
290.243267	12581.989376	28.341312
290.619159	12588.661824	28.346330
290.756837	12610.398017	28.351348
291.231918	12626.662776	28.356365
291.018998	12629.910801	28.361383
291.372048	12645.718300	28.366400
291.615551	12660.302248	28.371418
291.739276	12688.211350	28.376436
292.243674	12692.228012	28.381453
292.587550	12717.798672	28.386471
292.964234	12727.100924	28.391488
293.077518	12749.811979	28.396506
293.103040	12758.674335	28.401524
293.827006	12769.523326	28.406541
294.517786	12776.198982	28.411559
294.740931	12763.353018	28.416576
295.234794	12795.449312	28.421594
295.106823	12816.482774	28.426612
295.684251	12820.061956	28.431629
295.810299	12840.634340	28.436647
296.009198	12840.959146	28.441664
295.837488	12863.291995	28.446682
295.956595	12881.960514	28.451700
296.685756	12891.647413	28.456717
296.651936	12914.940814	28.461735
296.587277	12935.911971	28.466752
296.943577	12957.640877	28.471770
297.395684	12996.641502	28.476788
297.663366	13001.040862	28.481805
298.044063	13035.811465	28.486823
298.221788	13045.610042	28.491840
298.609583	13077.273754	28.496858
298.883759	13108.463086	28.501876
299.173011	13120.952013	28.506893
299.292579	13148.481263	28.511911
299.748690	13162.315145	28.516928
300.308784	13184.856874	28.521946
300.461087	13201.008507	28.526964
301.094159	13207.257390	28.531981
301.356075	13227.090845	28.536999
301.521686	13240.917634	28.542016
302.085249	13257.574963	28.547034
302.168250	13299.108107	28.552052
302.377339	13283.686083	28.557069
302.338813	13314.109645	28.562087
302.786943	13326.990065	28.567104
303.264622	13343.833431	28.572122
303.153159	13372.652400	28.577140
303.533893	13390.507726	28.582157
303.805827	13400.584051	28.587175
304.061615	13437.033880	28.592192
304.638256	13456.505191	28.597210
304.865029	13479.589318	28.602228
305.065193	13503.177401	28.607245
305.360545	13524.595675	28.612263
305.626343	13553.527554	28.617280
305.933244	13573.694374	28.622298
305.967082	13608.499874	28.627316
306.745510	13608.583982	28.632333
307.060196	13644.668415	28.637351
306.931829	13663.424418	28.642368
307.755930	13685.727831	28.647386
307.892929	13715.204446	28.652404
308.487736	13732.972783	28.657421
308.932531	13743.288654	28.662439
309.263426	13767.879808	28.667456
309.841894	13784.929174	28.672474
310.028216	13802.426269	28.677492
310.492394	13811.727301	28.682509
310.705779	13828.036506	28.687527
310.856326	13843.998396	28.692544
311.420716	13852.764448	28.697562
311.533466	13872.166345	28.702580
312.012553	13888.825675	28.707597
312.346729	13911.322221	28.712615
312.571436	13926.725125	28.717632
313.078457	13920.813890	28.722650
313.501721	13945.615399	28.727668
313.897324	13942.573257	28.732685
314.186798	13966.552251	28.737703
314.195681	13978.653227	28.742720
314.381391	13977.018313	28.747738
314.436622	14008.081660	28.752756
315.289030	14022.911356	28.757773
315.437954	14038.791761	28.762791
315.921383	14054.943122	28.767808
316.400955	14055.279894	28.772826
316.191146	14074.150679	28.777844
316.635378	14093.951925	28.782861
316.755540	14102.766289	28.787879
317.233614	14134.363576	28.792896
317.715687	14135.059232	28.797914
317.809898	14166.948497	28.802932
317.761042	14180.211116	28.807949
318.201807	14201.131928	28.812967
318.290776	14230.133623	28.817984
319.184588	14230.677743	28.823002
319.188336	14271.265188	28.828020
319.472783	14282.172056	28.833037
319.961844	14303.187453	28.838055
320.150925	14326.397203	28.843072
320.507026	14346.916158	28.848090
320.769879	14366.018069	28.853108
321.051122	14387.517033	28.858125
321.401933	14407.453862	28.863143
321.618959	14429.417345	28.868160
321.874703	14439.542693	28.873178
322.146423	14464.324330	28.878196
322.574531	14479.276546	28.883213
322.688470	14498.482008	28.888231
322.980976	14518.529463	28.893248
323.244635	14551.705785	28.898266
323.394478	14577.035654	28.903284
323.810700	14596.303183	28.908301
324.051207	14621.875016	28.913319
324.284729	14645.608959	28.918336
324.520331	14671.605600	28.923354
324.771535	14708.366342	28.928372
324.764010	14741.507479	28.933389
325.288714	14769.703773	28.938407
325.679340	14812.472763	28.943424
326.193678	14839.496828	28.948442
326.754628	14884.138435	28.953460
326.985305	14911.551458	28.958477
327.337418	14924.439558	28.963495
327.543336	14958.786135	28.968512
328.614332	14984.654724	28.973530
328.833712	15017.402773	28.978548
328.982395	15036.215447	28.983565
329.515595	15049.968868	28.988583
329.692252	15074.182462	28.993600
330.670831	15103.117544	28.998618
330.762411	15121.169108	29.003636
331.009179	15128.034145	29.008653
331.437843	15145.683341	29.013671
331.784379	15174.045302	29.018688
332.104293	15181.262324	29.023706
332.407467	15203.650736	29.028724
332.587321	15229.395867	29.033741
333.015004	15247.264393	29.038759
333.209892	15276.672811	29.043776
333.419147	15290.366482	29.048794
334.214381	15308.831537	29.053812
334.547095	15336.802072	29.058829
335.216683	15349.729470	29.063847
335.026361	15366.436289	29.068864
335.384384	15394.607619	29.073882
335.296840	15406.591626	29.078900
335.625685	15428.958771	29.083917
336.197322	15447.265499	29.088935
336.610215	15464.303012	29.093952
337.354588	15489.449402	29.098970
337.385739	15514.962662	29.103988
337.698439	15531.852894	29.109005
337.864333	15554.229794	29.114023
337.993609	15584.940346	29.119040
338.317120	15603.292968	29.124058
338.560206	15652.071028	29.129076
338.833954	15671.595039	29.134093
339.565928	15692.288422	29.139111
339.578874	15725.316275	29.144128
340.051402	15742.486068	29.149146
340.776759	15773.213550	29.154164
340.538784	15805.086819	29.159181
341.325507	15811.653335	29.164199
341.670813	15842.230968	29.169216
342.174758	15857.047417	29.174234
342.970800	15876.264748	29.179252
343.136729	15894.774540	29.184269
343.906309	15900.571671	29.189287
343.915456	15927.250741	29.194304
344.187836	15936.438111	29.199322
344.348795	15948.461839	29.204340
344.475694	15960.800105	29.209357
345.132248	15973.150173	29.214375
345.142049	16002.343035	29.219392
345.401533	15999.212684	29.224410
345.698041	16028.873593	29.229428
345.928395	16045.987574	29.234445
346.436219	16065.460779	29.239463
346.703727	16080.442574	29.244480
347.234782	16095.623558	29.249498
347.313766	16123.218126	29.254516
347.768886	16142.586654	29.259533
348.444243	16153.865190	29.264551
348.429801	16194.621174	29.269568
348.904242	16205.746963	29.274586
348.802180	16227.929488	29.279604
348.835761	16259.325363	29.284621
349.341630	16293.243785	29.289639
349.576071	16329.342691	29.294656
349.850719	16356.134629	29.299674
350.226859	16384.309400	29.304692
350.666573	16427.350320	29.309709
351.038935	16457.748113	29.314727
351.281091	16497.772135	29.319744
351.618309	16522.798250	29.324762
351.936809	16564.078573	29.329780
352.387694	16597.847523	29.334797
352.907161	16631.890487	29.339815
353.219436	16664.765184	29.344832
353.587921	16688.620071	29.349850
354.105446	16731.664696	29.354868
354.425162	16765.695229	29.359885
354.968597	16782.230261	29.364903
355.344352	16801.130388	29.369920
355.928672	16826.455011	29.374938
356.396334	16844.700102	29.379956
356.460031	16869.338498	29.384973
357.161831	16892.222892	29.389991
357.595353	16910.267224	29.395008
358.188033	16941.099202	29.400026
358.636057	16948.644170	29.405044
358.934815	16986.086213	29.410061
359.102074	16996.872406	29.415079
359.535621	17022.852692	29.420096
359.600200	17039.147134	29.425114
359.857699	17057.222282	29.430132
359.838716	17089.247846	29.435149
360.006363	17110.598935	29.440167
360.121514	17162.424088	29.445184
360.599427	17188.096262	29.450202
361.131414	17220.417221	29.455220
361.393565	17261.714909	29.460237
361.869837	17283.507000	29.465255
362.009365	17325.800749	29.470272
362.575131	17359.520764	29.475290
363.237241	17391.923015	29.480308
363.348527	17433.994738	29.485325
364.234674	17450.674005	29.490343
364.533234	17478.237726	29.495360
364.589821	17510.787525	29.500378
365.456374	17534.224059	29.505396
365.675550	17555.891907	29.510413
366.614302	17572.543695	29.515431
367.092862	17596.947569	29.520448
367.363723	17609.452435	29.525466
367.891222	17625.029474	29.530484
367.869329	17649.675294	29.535501
367.943588	17668.197499	29.540519
368.384675	17685.019880	29.545536
368.500433	17702.799184	29.550554
369.072613	17721.737275	29.555572
368.927857	17750.281001	29.560589
369.648718	17769.861322	29.565607
369.887092	17799.413662	29.570624
370.113948	17827.937115	29.575642
370.346905	17851.677372	29.580660
370.669932	17884.885311	29.585677
371.037775	17899.579506	29.590695
371.475630	17925.136503	29.595712
372.195303	17948.126602	29.600730
372.834647	17979.395737	29.605748
372.920941	18005.178013	29.610765
373.211121	18028.258088	29.615783
373.414313	18061.096848	29.620800
373.351715	18091.654629	29.625818
374.450225	18122.826118	29.630836
374.167381	18158.885234	29.635853
374.777128	18184.664861	29.640871
375.230258	18221.827280	29.645888
375.570845	18259.035171	29.650906
376.812366	18260.592306	29.655924
377.168480	18290.849577	29.660941
377.688441	18304.193373	29.665959
378.433351	18321.809514	29.670976
378.278103	18348.713541	29.675994
378.830661	18356.650144	29.681012
378.846926	18391.672039	29.686029
379.207481	18403.417118	29.691047
379.511725	18447.267525	29.696064
379.814872	18470.475330	29.701082
380.131100	18480.236951	29.706100
379.905547	18530.172823	29.711117
380.251706	18545.252637	29.716135
381.120605	18575.460398	29.721152
381.245898	18608.123958	29.726170
382.049687	18640.755891	29.731188
382.131890	18662.867112	29.736205
382.551080	18701.774868	29.741223
383.035027	18741.671392	29.746240
383.513030	18768.589714	29.751258
384.049769	18797.014783	29.756276
384.254193	18829.604232	29.761293
384.404333	18865.095243	29.766311
384.914317	18890.406948	29.771328
384.960775	18918.561698	29.776346
385.534996	18963.497515	29.781364
385.813562	19006.122536	29.786381
386.590347	19038.597354	29.791399
386.898405	19055.979060	29.796416
387.156318	19101.219715	29.801434
387.623914	19126.078493	29.806452
387.863096	19151.900351	29.811469
388.246940	19189.576088	29.816487
389.022936	19217.528862	29.821504
388.695624	19252.095439	29.826522
389.500626	19274.981864	29.831540
389.713664	19322.892992	29.836557
390.370801	19362.685159	29.841575
390.881279	19396.200928	29.846592
390.846703	19423.491886	29.851610
391.402262	19438.099692	29.856628
391.623358	19488.147517	29.861645
392.243715	19539.382757	29.866663
393.012718	19555.654742	29.871680
393.468276	19590.174669	29.876698
394.194659	19599.008494	29.881716
394.766343	19621.390090	29.886733
395.284482	19630.572032	29.891751
395.265239	19648.333162	29.896768
395.027919	19671.455373	29.901786
395.532339	19691.865078	29.906804
395.817536	19726.065048	29.911821
396.608886	19752.800790	29.916839
396.886854	19768.318609	29.921856
397.293655	19807.256225	29.926874
397.389721	19827.817103	29.931892
397.751580	19863.146006	29.936909
398.082344	19891.093067	29.941927
398.405671	19929.354291	29.946944
398.196962	19966.483343	29.951962
398.550782	20007.302960	29.956980
398.825462	20058.403001	29.961997
399.419855	20088.469699	29.967015
400.265712	20125.705507	29.972032
400.972788	20160.970133	29.977050
401.719581	20171.118794	29.982068
402.574456	20188.974147	29.987085
403.219354	20213.609787	29.992103
403.431813	20245.857020	29.997120
403.357645	20274.174291	30.002138
403.808518	20284.606795	30.007156
403.858097	20325.892055	30.012173
404.348782	20365.242760	30.017191
404.717699	20392.134442	30.022208
404.729224	20430.842436	30.027226
405.615228	20463.383977	30.032244
405.560086	20501.754750	30.037261
405.738662	20544.870014	30.042279
406.473144	20583.905080	30.047296
406.782445	20619.222196	30.052314
406.903709	20657.389197	30.057332
407.488282	20701.744702	30.062349
407.253670	20730.617371	30.067367
408.010758	20776.525795	30.072384
408.165007	20824.633821	30.077402
409.089702	20872.206403	30.082420
409.739168	20918.010027	30.087437
409.776884	20965.161849	30.092455
410.486565	20999.732578	30.097472
410.658564	21054.415547	30.102490
410.965215	21085.157452	30.107508
411.521964	21127.073497	30.112525
411.749283	21185.908207	30.117543
412.628906	21223.399440	30.122560
413.061250	21253.660543	30.127578
413.579856	21289.955061	30.132596
413.995246	21335.708632	30.137613
414.164498	21366.833203	30.142631
415.219013	21387.005923	30.147648
415.836304	21414.028488	30.152666
416.330017	21445.662438	30.157684
416.992265	21465.770773	30.162701
416.921819	21499.914879	30.167719
417.312981	21521.196878	30.172736
417.684332	21564.527290	30.177754
418.403596	21579.532459	30.182772
418.815431	21609.975747	30.187789
419.077243	21644.932377	30.192807
419.640694	21673.870334	30.197824
420.329842	21697.545452	30.202842
420.279471	21729.320263	30.207860
420.731242	21748.665957	30.212877
421.035022	21791.118922	30.217895
421.546772	21814.255937	30.222912
421.509783	21844.559374	30.227930
422.174236	21861.997074	30.232948
422.983615	21877.555201	30.237965
423.272938	21906.220368	30.242983
423.650806	21938.423041	30.248000
424.233308	21954.777062	30.253018
424.414383	21982.348735	30.258036
424.976594	21995.981773	30.263053
425.229673	22029.844906	30.268071
425.958596	22058.953271	30.273088
425.950062	22084.393320	30.278106
426.157748	22120.097736	30.283124
426.436948	22146.579793	30.288141
426.799336	22191.731147	30.293159
427.135695	22227.871759	30.298176
427.259213	22276.356375	30.303194
427.681583	22316.054042	30.308212
428.515022	22359.906144	30.313229
428.500232	22406.299705	30.318247
428.833675	22450.051743	30.323264
429.215241	22491.654849	30.328282
429.690026	22534.183925	30.333300
430.405240	22582.502310	30.338317
430.610792	22638.982285	30.343335
431.302440	22668.824707	30.348352
431.999888	22723.035292	30.353370
432.232874	22758.990727	30.358388
432.759550	22801.962837	30.363405
433.191287	22843.747727	30.368423
433.766932	22869.907610	30.373440
434.144893	22917.946832	30.378458
434.753950	22967.441149	30.383476
435.353590	22999.648636	30.388493
435.674562	23041.280452	30.393511
436.485866	23067.414329	30.398528
436.718505	23100.079960	30.403546
437.384045	23138.601013	30.408564
437.785789	23178.354572	30.413581
437.741163	23219.269896	30.418599
438.628416	23252.434729	30.423616
438.723752	23293.908924	30.428634
439.098273	23336.980060	30.433652
439.272660	23381.727322	30.438669
439.442089	23426.972195	30.443687
440.131221	23464.194013	30.448704
440.223135	23519.142606	30.453722
440.944046	23568.785767	30.458740
441.168350	23617.279657	30.463757
441.583445	23664.553292	30.468775
442.170938	23708.829529	30.473792
443.126855	23753.713576	30.478810
443.543531	23799.875704	30.483828
444.193419	23832.190007	30.488845
444.259953	23866.942252	30.493863
445.065912	23896.460494	30.498880
445.836635	23946.536459	30.503898
446.167804	23976.260986	30.508916
446.457223	24020.787529	30.513933
446.534327	24060.566826	30.518951
447.020994	24088.999696	30.523968
447.354993	24156.520055	30.528986
447.801286	24185.240428	30.534004
448.113612	24233.000935	30.539021
448.357298	24290.719497	30.544039
449.400709	24321.686200	30.549056
449.617772	24364.913680	30.554074
449.781734	24410.493212	30.559092
450.851953	24446.443235	30.564109
451.194925	24482.847752	30.569127
451.987443	24512.063382	30.574144
452.615137	24550.961306	30.579162
452.648531	24581.098754	30.584180
453.228010	24607.615485	30.589197
453.593116	24635.676716	30.594215
454.081951	24665.959844	30.599232
454.661578	24701.824299	30.604250
454.844699	24739.105696	30.609268
455.801830	24766.009700	30.614285
456.136160	24800.859961	30.619303
456.755409	24837.594897	30.624320
457.326350	24852.203317	30.629338
457.535792	24880.214974	30.634356
458.235518	24909.795107	30.639373
458.257420	24941.089365	30.644391
458.786746	24976.994248	30.649408
458.967988	25001.189973	30.654426
459.274048	25047.321726	30.659444
459.603396	25081.763393	30.664461
459.764475	25132.366165	30.669479
460.208465	25180.571194	30.674496
460.510571	25240.987717	30.679514
461.006663	25287.725801	30.684532
461.664405	25337.583263	30.689549
461.984642	25388.067465	30.694567
462.605724	25427.162447	30.699584
462.926565	25477.053888	30.704602
463.174745	25533.741453	30.709620
464.254779	25583.015798	30.714637
464.624028	25635.766584	30.719655
464.902983	25676.437247	30.724672
465.567087	25722.100099	30.729690
466.077654	25774.988822	30.734708
466.786662	25817.664062	30.739725
466.755627	25858.708062	30.744743
467.397129	25908.339637	30.749760
468.025425	25956.942196	30.754778
468.375159	26008.987719	30.759796
469.036218	26053.229524	30.764813
469.026297	26103.410820	30.769831
469.638848	26157.069219	30.774848
470.596243	26195.187867	30.779866
471.090992	26233.808810	30.784884
471.716069	26276.152119	30.789901
472.637188	26309.949718	30.794919
473.242696	26338.589075	30.799936
474.070784	26362.224127	30.804954
474.326851	26394.876445	30.809972
475.634365	26412.067546	30.814989
475.919456	26433.269161	30.820007
476.214816	26450.072375	30.825024
476.805168	26481.928443	30.830042
477.245697	26508.671369	30.835060
477.688087	26538.016125	30.840077
478.272473	26554.367982	30.845095
478.767137	26567.328288	30.850112
479.043104	26594.391857	30.855130
479.247406	26624.179808	30.860148
479.851706	26643.209422	30.865165
479.796400	26679.575595	30.870183
479.745143	26702.154661	30.875200
480.284924	26743.056028	30.880218
480.704718	26787.519367	30.885236
481.089703	26825.418561	30.890253
481.374587	26877.878007	30.895271
481.590652	26925.879581	30.900288
482.146584	26964.321742	30.905306
482.002797	27025.699793	30.910324
482.597862	27080.420610	30.915341
482.807060	27129.903186	30.920359
483.234710	27182.242199	30.925376
483.881866	27245.095862	30.930394
483.875064	27311.599935	30.935412
484.130269	27348.771020	30.940429
484.838314	27412.164066	30.945447
486.012558	27462.412381	30.950464
486.661652	27516.926947	30.955482
487.161325	27569.848238	30.960500
487.617457	27622.739032	30.965517
487.985065	27686.993658	30.970535
488.612025	27728.182623	30.975552
489.185905	27783.473790	30.980570
489.427527	27843.154016	30.985588
490.010951	27886.221047	30.990605
490.606311	27942.777206	30.995623
490.761756	27989.217752	31.000640
491.375263	28048.256865	31.005658
491.581779	28107.880717	31.010676
492.353812	28156.645558	31.015693
492.741286	28236.418365	31.020711
493.463094	28281.889235	31.025728
494.036867	28328.122801	31.030746
494.242437	28401.942553	31.035764
494.895588	28450.361950	31.040781
495.515054	28514.111199	31.045799
495.947010	28567.636609	31.050816
496.879267	28619.852472	31.055834
497.090191	28671.534669	31.060852
497.937334	28718.787175	31.065869
498.433311	28771.308987	31.070887
499.428087	28811.095982	31.075904
500.421294	28852.630910	31.080922
501.118291	28893.653364	31.085940
501.729577	28935.712130	31.090957
502.030104	28966.765802	31.095975
502.223572	29017.802087	31.100992
502.751097	29042.954171	31.106010
502.677145	29083.647011	31.111028
503.084031	29121.295269	31.116045
503.643315	29184.754092	31.121063
504.389257	29224.031094	31.126080
504.983706	29268.658095	31.131098
505.575869	29313.563190	31.136116
506.310024	29342.331408	31.141133
506.651537	29391.025731	31.146151
507.212202	29425.942624	31.151168
507.873724	29469.098490	31.156186
507.806719	29524.138297	31.161204
508.389162	29556.042366	31.166221
509.244566	29608.731325	31.171239
509.475256	29652.179631	31.176256
510.337404	29702.312514	31.181274
510.002424	29746.236198	31.186292
510.709771	29793.328602	31.191309
511.511331	29842.787340	31.196327
511.823404	29887.629769	31.201344
512.299093	29928.542956	31.206362
512.590383	29988.932163	31.211380
513.000736	30040.503470	31.216397
513.189934	30101.540868	31.221415
513.451502	30152.430426	31.226432
514.272739	30215.789805	31.231450
514.540266	30284.761663	31.236468
515.491596	30332.168557	31.241485
516.392260	30378.533416	31.246503
517.141444	30420.964191	31.251520
518.523431	30433.651505	31.256538
519.113718	30462.663023	31.261556
519.854743	30490.684331	31.266573
520.571750	30514.119447	31.271591
521.017560	30527.788012	31.276608
521.435148	30546.584621	31.281626
521.586660	30587.237421	31.286644
521.962491	30605.198661	31.291661
522.605624	30639.634305	31.296679
522.613283	30670.685761	31.301696
523.216005	30704.957850	31.306714
523.484252	30739.695378	31.311732
523.997265	30782.159732	31.316749
524.176204	30834.844251	31.321767
524.517977	30874.595560	31.326784
525.024989	30928.551209	31.331802
525.307721	30965.586682	31.336820
525.895908	31012.329790	31.341837
526.764853	31073.034315	31.346855
527.033360	31123.654237	31.351872
527.802291	31168.774691	31.356890
528.012102	31233.538573	31.361908
528.591585	31298.109129	31.366925
529.097229	31345.545069	31.371943
529.878626	31393.484551	31.376960
530.585725	31446.194097	31.381978
530.890084	31499.755905	31.386996
531.438469	31543.046017	31.392013
532.039449	31600.105321	31.397031
532.663546	31646.541314	31.402048
533.607433	31701.723885	31.407066
533.914280	31751.367550	31.412084
534.149283	31807.159718	31.417101
535.255190	31828.822351	31.422119
535.646583	31895.499019	31.427136
535.943710	31942.971015	31.432154
536.194969	31991.681184	31.437172
536.794623	32044.558561	31.442189
537.097108	32104.808087	31.447207
537.575106	32165.786047	31.452224
538.097794	32235.449106	31.457242
539.027521	32274.658455	31.462260
539.220134	32332.809838	31.467277
540.144735	32384.899429	31.472295
540.482476	32443.733955	31.477312
541.100074	32505.333680	31.482330
541.375077	32568.003009	31.487348
542.043863	32623.341190	31.492365
542.631871	32684.807603	31.497383
542.668129	32746.377982	31.502400
543.816776	32799.226900	31.507418
544.034942	32863.490571	31.512436
544.204847	32924.799703	31.517453
544.972201	32978.024500	31.522471
545.436004	33051.458379	31.527488
546.298815	33117.320327	31.532506
546.881294	33182.405300	31.537524
547.574677	33246.128050	31.542541
548.167738	33307.308666	31.547559
548.515062	33360.903745	31.552576
548.904020	33425.582990	31.557594
549.724840	33490.181677	31.562612
549.852547	33543.665282	31.567629
550.873926	33602.018424	31.572647
550.981221	33675.106735	31.577664
551.515169	33731.448816	31.582682
551.776469	33803.269009	31.587700
552.314528	33865.031759	31.592717
553.486940	33910.534360	31.597735
554.098648	33966.305840	31.602752
554.943587	34015.617722	31.607770
555.401559	34066.034941	31.612788
555.996243	34110.926664	31.617805
556.955426	34156.869011	31.622823
557.104659	34206.936883	31.627840
557.856342	34254.494631	31.632858
558.824926	34291.313374	31.637876
559.105479	34342.435949	31.642893
559.548291	34391.597567	31.647911
560.173166	34449.788642	31.652928
560.237260	34506.040390	31.657946
560.574242	34556.207611	31.662964
561.024401	34632.367180	31.667981
561.748120	34677.182224	31.672999
562.236370	34741.092539	31.678016
563.529035	34788.581301	31.683034
563.616170	34843.104225	31.688052
563.861315	34921.570890	31.693069
564.756440	34959.526535	31.698087
565.872138	35023.148053	31.703104
567.242393	35058.718705	31.708122
568.045727	35106.891856	31.713140
568.222326	35140.081693	31.718157
568.830578	35186.024709	31.723175
569.015717	35229.885592	31.728192
569.490978	35277.302395	31.733210
569.863848	35331.508235	31.738228
570.058825	35385.667886	31.743245
571.175488	35426.191350	31.748263
571.793473	35485.800684	31.753280
572.137222	35535.007065	31.758298
572.716037	35580.750841	31.763316
573.329054	35640.399380	31.768333
573.683781	35694.672433	31.773351
573.858755	35765.429236	31.778368
574.362691	35819.832655	31.783386
574.684437	35885.636449	31.788404
575.089224	35966.000022	31.793421
575.616847	36031.738792	31.798439
575.911229	36096.733693	31.803456
576.361049	36175.553907	31.808474
576.989950	36263.960621	31.813492
577.298963	36333.274258	31.818509
578.154098	36419.176525	31.823527
578.909557	36496.423402	31.828544
579.638699	36562.982915	31.833562
580.474161	36637.234902	31.838580
581.202421	36712.637863	31.843597
582.294760	36769.080360	31.848615
583.197235	36811.374930	31.853632
584.400671	36863.983895	31.858650
585.067345	36933.180815	31.863668
585.162703	36972.238544	31.868685
585.926394	37014.891043	31.873703
586.012820	37076.897296	31.878720
586.589117	37139.936908	31.883738
586.972849	37187.165590	31.888756
587.464319	37258.608187	31.893773
588.213879	37314.872315	31.898791
588.109401	37394.919268	31.903808
588.682484	37453.589447	31.908826
589.374294	37523.178985	31.913844
589.632575	37583.728918	31.918861
590.679872	37649.637105	31.923879
591.265866	37717.796245	31.928896
592.266060	37777.552055	31.933914
592.860676	37834.891213	31.938932
593.116447	37888.085763	31.943949
594.477763	37935.647300	31.948967
595.264652	37969.865144	31.953984
595.409417	38035.545071	31.959002
596.145712	38081.174527	31.964020
596.347968	38126.437815	31.969037
596.870356	38185.863595	31.974055
597.388484	38248.395926	31.979072
597.734114	38303.618887	31.984090
598.540466	38370.276482	31.989108
599.146233	38430.061721	31.994125
599.862776	38480.757966	31.999143
600.312448	38546.512480	32.004160
600.785027	38611.386022	32.009178
601.772536	38668.757623	32.014196
602.207045	38719.841990	32.019213
602.905052	38790.666318	32.024231
603.326048	38852.976904	32.029248
603.434154	38917.574017	32.034266
603.965813	38992.188876	32.039284
604.631810	39072.276963	32.044301
605.169792	39143.220628	32.049319
605.704888	39221.093168	32.054336
606.179759	39289.541710	32.059354
607.262080	39372.598754	32.064372
607.567870	39441.950102	32.069389
608.089411	39516.761323	32.074407
608.597435	39605.033912	32.079424
609.231400	39685.341467	32.084442
610.394503	39750.862570	32.089460
610.586814	39830.053737	32.094477
611.670316	39907.857582	32.099495
612.113663	39971.285686	32.104512
612.867958	40046.887633	32.109530
613.070347	40117.196097	32.114548
613.691621	40208.782986	32.119565
614.145532	40286.531446	32.124583
614.672139	40373.646247	32.129600
616.136462	40432.646035	32.134618
617.059621	40495.598995	32.139636
617.624566	40562.140358	32.144653
618.747467	40625.322771	32.149671
619.825933	40677.815116	32.154688
620.228727	40744.162962	32.159706
621.132354	40796.217349	32.164724
621.417158	40866.136289	32.169741
622.507422	40913.387401	32.174759
623.248211	40964.692635	32.179776
623.939851	41003.982529	32.184794
624.936544	41053.408591	32.189812
624.559298	41100.561634	32.194829
625.108147	41161.214379	32.199847
625.576872	41214.017305	32.204864
625.632597	41282.375237	32.209882
626.102100	41338.628641	32.214900
626.569400	41422.958249	32.219917
627.148081	41489.008266	32.224935
627.260399	41574.385246	32.229952
627.904093	41660.179942	32.234970
628.586220	41735.459856	32.239988
629.086519	41825.654267	32.245005
629.676345	41916.162640	32.250023
630.105835	41984.710838	32.255040
631.075561	42070.270508	32.260058
631.750053	42145.651221	32.265076
632.246275	42231.188820	32.270093
632.820998	42313.803233	32.275111
633.282979	42398.883207	32.280128
634.039197	42470.776042	32.285146
635.154713	42543.256982	32.290164
635.747794	42616.743147	32.295181
636.091340	42682.125972	32.300199
636.811765	42755.929450	32.305216
637.362436	42849.798371	32.310234
638.105070	42914.216378	32.315252
638.744479	42985.830599	32.320269
639.584435	43060.155393	32.325287
640.380444	43134.045765	32.330304
641.360968	43202.706372	32.335322
642.230709	43265.437713	32.340340
642.367261	43349.230917	32.345357
643.247635	43414.530829	32.350375
644.022906	43477.900429	32.355392
644.275257	43560.197961	32.360410
644.825840	43624.400749	32.365428
645.222326	43707.274973	32.370445
646.058561	43785.694883	32.375463
646.724250	43854.248888	32.380480
647.105474	43938.711537	32.385498
648.183475	44016.467382	32.390516
648.930850	44103.149766	32.395533
649.848033	44176.257090	32.400551
650.452880	44234.719607	32.405568
651.193937	44308.169098	32.410586
652.341479	44378.277728	32.415604
652.865446	44448.697982	32.420621
653.470428	44509.049354	32.425639
654.386545	44578.704432	32.430656
654.596264	44644.709832	32.435674
655.595201	44703.645472	32.440692
656.036384	44776.937957	32.445709
656.776215	44846.859946	32.450727
657.392133	44918.277118	32.455744
657.871895	44994.093078	32.460762
658.694807	45071.898619	32.465780
659.047066	45150.817818	32.470797
659.572975	45222.481503	32.475815
660.158284	45288.900754	32.480832
661.343142	45352.051228	32.485850
662.354898	45420.519115	32.490868
662.876775	45487.615754	32.495885
663.258603	45555.108336	32.500903
663.994248	45634.938742	32.505920
664.657855	45711.396620	32.510938
665.558868	45771.317977	32.515956
665.844952	45860.667490	32.520973
666.141377	45940.094954	32.525991
666.739271	46005.201161	32.531008
667.079481	46080.381495	32.536026
668.087794	46155.881216	32.541044
668.578187	46250.759208	32.546061
669.191344	46329.785529	32.551079
670.055834	46405.821527	32.556096
670.844611	46503.044935	32.561114
671.352792	46585.512464	32.566132
672.031143	46652.451651	32.571149
672.775888	46738.830926	32.576167
673.235092	46813.631415	32.581184
673.729012	46913.728545	32.586202
674.346234	46995.248359	32.591220
674.870088	47093.415335	32.596237
675.177995	47186.443053	32.601255
676.040133	47266.894191	32.606272
676.762078	47360.394354	32.611290
677.346220	47443.689882	32.616308
678.016327	47539.122541	32.621325
678.718851	47618.486856	32.626343
679.482901	47710.627124	32.631360
679.928123	47801.377389	32.636378
680.630774	47876.732387	32.641396
681.267855	47974.181050	32.646413
682.078496	48068.380571	32.651431
683.137814	48144.650344	32.656448
683.713538	48234.193783	32.661466
684.732294	48312.078275	32.666484
685.253887	48390.582029	32.671501
685.990295	48479.957987	32.676519
687.002131	48554.301463	32.681536
687.565569	48636.462492	32.686554
688.728449	48710.086893	32.691572
689.248393	48792.069460	32.696589
689.746337	48877.693980	32.701607
690.591592	48950.168582	32.706624
691.464008	49023.801113	32.711642
692.352537	49092.662698	32.716660
693.687384	49167.277346	32.721677
694.280655	49238.278817	32.726695
695.321888	49297.379760	32.731712
695.896683	49367.967906	32.736730
696.472981	49419.361444	32.741748
697.015103	49493.325087	32.746765
697.742825	49571.363860	32.751783
698.204901	49642.252704	32.756800
698.754839	49711.567202	32.761818
699.091850	49794.427501	32.766836
699.547989	49869.527928	32.771853
699.948663	49965.768896	32.776871
700.752571	50045.739280	32.781888
701.136839	50134.593734	32.786906
701.798070	50231.986798	32.791924
702.718661	50323.725410	32.796941
703.123890	50427.607624	32.801959
703.565261	50521.911836	32.806976
704.372868	50622.169331	32.811994
705.200697	50733.465296	32.817012
705.747740	50826.524990	32.822029
706.305487	50933.224044	32.827047
707.408177	51011.888955	32.832064
708.266333	51109.351858	32.837082
709.367216	51199.397286	32.842100
710.119037	51300.248665	32.847117
711.059387	51387.352629	32.852135
711.664479	51460.988150	32.857152
712.194594	51575.900810	32.862170
713.068375	51655.957955	32.867188
713.670442	51737.061524	32.872205
714.015694	51837.986014	32.877223
714.836851	51926.902937	32.882240
715.635595	52032.541780	32.887258
716.153893	52121.474869	32.892276
717.067092	52216.565410	32.897293
717.412313	52324.895988	32.902311
717.936617	52405.857278	32.907328
718.869972	52527.427213	32.912346
719.691854	52623.109689	32.917364
720.242165	52718.805898	32.922381
720.859476	52816.456167	32.927399
721.645862	52913.087199	32.932416
722.474297	53016.269098	32.937434
722.904381	53130.642107	32.942452
723.798242	53222.683200	32.947469
724.284376	53325.588448	32.952487
725.658561	53410.481971	32.957504
726.387936	53501.559715	32.962522
727.315884	53578.390813	32.967540
728.668319	53649.175782	32.972557
729.323500	53723.512871	32.977575
730.213720	53800.370029	32.982592
730.730950	53875.513853	32.987610
731.279134	53962.201386	32.992628
732.136071	54036.651657	32.997645
732.673479	54130.733317	33.002663
733.350297	54213.831263	33.007680
733.934113	54291.897089	33.012698
734.169443	54383.161618	33.017716
734.629018	54466.321783	33.022733
735.097218	54572.982993	33.027751
736.000752	54674.430196	33.032768
736.515525	54787.181569	33.037786
737.387631	54888.995192	33.042804
738.194069	54997.055967	33.047821
738.964794	55101.269287	33.052839
739.868080	55196.262292	33.057856
740.432941	55304.206702	33.062874
741.168764	55409.899520	33.067892
742.467294	55509.845304	33.072909
743.036185	55617.607545	33.077927
744.030641	55714.710888	33.082944
744.652044	55810.947542	33.087962
745.517725	55917.777872	33.092980
746.459629	56005.900520	33.097997
747.432111	56100.880151	33.103015
748.259686	56190.892714	33.108032
748.781807	56293.858153	33.113050
749.271130	56397.492973	33.118068
750.972901	56466.916227	33.123085
751.588480	56565.154133	33.128103
752.173910	56657.015875	33.133120
752.994930	56758.436905	33.138138
753.386155	56838.888800	33.143156
754.614222	56932.686578	33.148173
755.038841	57036.651358	33.153191
755.817257	57121.520328	33.158208
756.574024	57211.087972	33.163226
757.024968	57297.054342	33.168244
758.198851	57398.729995	33.173261
758.923608	57497.529495	33.178279
759.945764	57583.807180	33.183296
760.385438	57673.928455	33.188314
761.685610	57769.241110	33.193332
762.850498	57839.402361	33.198349
763.344568	57932.883760	33.203367
764.101202	58021.115483	33.208384
764.768002	58108.111287	33.213402
765.655308	58202.318879	33.218420
766.152035	58284.124096	33.223437
766.383159	58376.741066	33.228455
767.137455	58474.447353	33.233472
767.950300	58574.008571	33.238490
768.228694	58676.464213	33.243508
769.186990	58766.321533	33.248525
769.860227	58879.057407	33.253543
770.378436	58971.939366	33.258560
770.843473	59087.409083	33.263578
771.676838	59199.513674	33.268596
772.845392	59302.090935	33.273613
773.323869	59414.779833	33.278631
774.270681	59512.503634	33.283648
774.823911	59629.333207	33.288666
775.771548	59738.439191	33.293684
776.757218	59829.061409	33.298701
777.371257	59941.939421	33.303719
778.487211	60028.446000	33.308736
779.110713	60119.331555	33.313754
779.676243	60214.998369	33.318772
780.819329	60307.220879	33.323789
781.242948	60420.170934	33.328807
782.338952	60513.147878	33.333824
782.947536	60612.285284	33.338842
783.709966	60714.570275	33.343860
785.246410	60783.163761	33.348877
786.141083	60859.207030	33.353895
786.909774	60953.308095	33.358912
787.767960	61050.466257	33.363930
788.916740	61120.256156	33.368948
790.444622	61187.202952	33.373965
791.177461	61278.631825	33.378983
791.786701	61351.911725	33.384000
792.384606	61441.410758	33.389018
792.649630	61533.215066	33.394036
793.040276	61611.038146	33.399053
793.343890	61712.424345	33.404071
794.045460	61822.978960	33.409088
794.840129	61925.542831	33.414106
795.425874	62040.036218	33.419124
796.291721	62147.386441	33.424141
796.710844	62260.353819	33.429159
796.730753	62367.168625	33.434176
798.350017	62486.354128	33.439194
798.819352	62617.820979	33.444212
799.474456	62734.601093	33.449229
800.011510	62872.258669	33.454247
801.115010	62985.875505	33.459264
801.792135	63117.071081	33.464282
802.516636	63252.690356	33.469300
803.240327	63376.604996	33.474317
803.999304	63515.273145	33.479335
804.718174	63654.650446	33.484352
806.030949	63766.113324	33.489370
806.711520	63887.490941	33.494388
807.643527	64020.110295	33.499405
808.333637	64157.561610	33.504423
809.429381	64281.426600	33.509440
810.228043	64409.064385	33.514458
810.931013	64536.794612	33.519476
812.915190	64637.715538	33.524493
814.076246	64746.389650	33.529511
815.210173	64853.684513	33.534528
816.333008	64948.560928	33.539546
816.996592	65053.892803	33.544564
817.649443	65149.290220	33.549581
818.431471	65246.120607	33.554599
819.208282	65346.707076	33.559616
819.410057	65456.301863	33.564634
820.195597	65576.584850	33.569652
820.933264	65676.901253	33.574669
821.881558	65804.314354	33.579687
822.289663	65913.005146	33.584704
823.004600	66022.214766	33.589722
823.899856	66146.288402	33.594740
824.855565	66271.124013	33.599757
825.763074	66387.194124	33.604775
826.544032	66499.132548	33.609792
827.571643	66610.278583	33.614810
828.478954	66717.886029	33.619828
829.735228	66834.103336	33.624845
830.339099	66927.905006	33.629863
831.790033	67018.754090	33.634880
833.199475	67093.079200	33.639898
833.729464	67189.233270	33.644916
834.555026	67270.565062	33.649933
835.353478	67364.216452	33.654951
836.239367	67450.665940	33.659968
837.015766	67543.392471	33.664986
837.386052	67642.824416	33.670004
838.094528	67720.870964	33.675021
838.350401	67834.831426	33.680039
839.049171	67935.740425	33.685056
839.865374	68025.864201	33.690074
840.316571	68147.962099	33.695092
841.049883	68260.625892	33.700109
841.426722	68388.654897	33.705127
842.344661	68520.236876	33.710144
843.242594	68644.268004	33.715162
843.692107	68777.085888	33.720180
844.492153	68908.348360	33.725197
845.162929	69047.403071	33.730215
845.771775	69184.900988	33.735232
846.703332	69315.866098	33.740250
847.406617	69465.925423	33.745268
848.272642	69594.886236	33.750285
849.541753	69736.969974	33.755303
850.650033	69868.193838	33.760320
851.386328	70005.821464	33.765338
852.165965	70156.726622	33.770356
853.388252	70299.972582	33.775373
853.896643	70439.196021	33.780391
854.677569	70584.653846	33.785408
855.495693	70726.173756	33.790426
856.489301	70868.689928	33.795444
857.664519	71009.956755	33.800461
858.661298	71146.733107	33.805479
859.350954	71281.417569	33.810496
860.731488	71402.647320	33.815514
861.294091	71550.386116	33.820532
862.179455	71692.843466	33.825549
863.418120	71829.141634	33.830567
864.133984	71963.946206	33.835584
865.320423	72093.419364	33.840602
865.988223	72230.585772	33.845620
866.758829	72365.731609	33.850637
867.685803	72502.888579	33.855655
868.582389	72643.586191	33.860672
869.983131	72756.701101	33.865690
871.108810	72889.287545	33.870708
872.259765	73011.557082	33.875725
873.330871	73125.367026	33.880743
874.185673	73243.121221	33.885760
875.309826	73353.774502	33.890778
876.167930	73463.985362	33.895796
877.318971	73575.634467	33.900813
878.152588	73684.927250	33.905831
879.482106	73791.014809	33.910848
880.655821	73886.568021	33.915866
881.214936	73983.456262	33.920884
881.944972	74093.887515	33.925901
882.646035	74197.077041	33.930919
883.272059	74316.468452	33.935936
884.166185	74428.752495	33.940954
884.725297	74547.403683	33.945972
885.319695	74652.073804	33.950989
886.068000	74769.860210	33.956007
886.945604	74908.640559	33.961024
887.611334	75021.287897	33.966042
888.083357	75160.187407	33.971060
888.612073	75280.163013	33.976077
889.352135	75416.060211	33.981095
889.657880	75544.131052	33.986112
890.457200	75665.056990	33.991130
891.271292	75817.153447	33.996148
892.321065	75944.635790	34.001165
893.134903	76096.493905	34.006183
893.377936	76248.788835	34.011200
894.541506	76390.250862	34.016218
895.828360	76533.072182	34.021236
896.745384	76684.948953	34.026253
897.721207	76825.590974	34.031271
898.142388	76981.156656	34.036288
899.275301	77122.451368	34.041306
900.206727	77271.243380	34.046324
901.869553	77410.036413	34.051341
903.310075	77525.693101	34.056359
904.276948	77659.821098	34.061376
905.590136	77797.238568	34.066394
906.599161	77921.393254	34.071412
907.467349	78052.573562	34.076429
908.308566	78181.943841	34.081447
909.186193	78307.311475	34.086464
910.148544	78431.084575	34.091482
910.873828	78571.159218	34.096500
911.435053	78694.127155	34.101517
912.245006	78841.969387	34.106535
913.067634	78987.558747	34.111552
914.049821	79124.159885	34.116570
914.843296	79257.984607	34.121588
916.237078	79388.055001	34.126605
917.754801	79517.080987	34.131623
918.425619	79670.037243	34.136640
919.605665	79791.473200	34.141658
920.483191	79947.471369	34.146676
921.240739	80059.686461	34.151693
922.048456	80191.977332	34.156711
922.656222	80340.419507	34.161728
923.410625	80471.006598	34.166746
925.229801	80589.444236	34.171764
925.947331	80725.238559	34.176781
927.158734	80854.411386	34.181799
927.899750	80995.245045	34.186816
928.750449	81120.822676	34.191834
929.566743	81265.921822	34.196852
930.198087	81400.115033	34.201869
931.117646	81547.046085	34.206887
931.599770	81702.533396	34.211904
932.507851	81834.254332	34.216922
933.469497	81981.712641	34.221940
934.141333	82135.482554	34.226957
935.054327	82287.765017	34.231975
935.635096	82451.458784	34.236992
936.417163	82607.548042	34.242010
937.199992	82770.964026	34.247028
938.012665	82944.169340	34.252045
939.118686	83102.055778	34.257063
939.782933	83276.641957	34.262080
941.132378	83437.312089	34.267098
942.391776	83581.897372	34.272116
943.166183	83758.765551	34.277133
944.518237	83908.493707	34.282151
946.199620	84048.058579	34.287168
947.998515	84175.097161	34.292186
949.341654	84307.696909	34.297204
950.514615	84436.244801	34.302221
951.500720	84559.459195	34.307239
952.167206	84688.528662	34.312256
953.078439	84794.402366	34.317274
954.040338	84913.383701	34.322292
954.597267	85026.017077	34.327309
955.607952	85140.973978	34.332327
956.217134	85266.709220	34.337344
957.198338	85398.527203	34.342362
957.841141	85533.299572	34.347380
958.404826	85655.387436	34.352397
959.395989	85788.768775	34.357415
960.120203	85937.088961	34.362432
961.502032	86070.401097	34.367450
962.080113	86191.647899	34.372468
963.070958	86338.503016	34.377485
964.067320	86479.726894	34.382503
964.703136	86631.849810	34.387520
965.501305	86772.583021	34.392538
966.689247	86919.725633	34.397556
968.704803	87055.805097	34.402573
969.912081	87184.723255	34.407591
970.756690	87316.865743	34.412608
971.692916	87449.493725	34.417626
972.937815	87568.144559	34.422644
973.890960	87710.661191	34.427661
975.092351	87846.803754	34.432679
975.540152	87983.375250	34.437696
976.454239	88126.084359	34.442714
977.294660	88259.352858	34.447732
978.019829	88404.126049	34.452749
979.026025	88550.916602	34.457767
979.898706	88694.502907	34.462784
980.481344	88847.984174	34.467802
981.248720	89001.442267	34.472820
981.829317	89161.703129	34.477837
982.590841	89318.923069	34.482855
983.857761	89494.551219	34.487872
985.003391	89655.968774	34.492890
985.978406	89822.889449	34.497908
986.543139	89990.904203	34.502925
987.470822	90148.627455	34.507943
988.395267	90338.936639	34.512960
989.224894	90520.656456	34.517978
990.379939	90696.343607	34.522996
990.750743	90881.363070	34.528013
992.158468	91071.357834	34.533031
993.090704	91247.351621	34.538048
994.941821	91411.113747	34.543066
996.201198	91573.544420	34.548084
997.449443	91753.337557	34.553101
998.720540	91915.958475	34.558119
999.397805	92083.899753	34.563136
999.856219	92246.903900	34.568154
1000.826012	92421.893823	34.573172
1001.963933	92607.034113	34.578189
1003.609272	92754.681726	34.583207
1005.643906	92891.715588	34.588224
1007.191221	93025.267455	34.593242
1008.862226	93160.343926	34.598260
1009.719637	93310.068032	34.603277
1010.615474	93436.451291	34.608295
1011.650837	93572.666648	34.613312
1012.552893	93703.081934	34.618330
1013.305241	93847.902607	34.623348
1014.096340	93989.205010	34.628365
1015.095880	94113.669570	34.633383
1015.886662	94264.106780	34.638400
1016.361801	94408.736040	34.643418
1017.174763	94552.772387	34.648436
1018.170583	94730.736836	34.653453
1018.705626	94873.877870	34.658471
1019.318147	95032.887715	34.663488
1020.170314	95184.896512	34.668506
1021.078073	95345.625593	34.673524
1021.644760	95518.906754	34.678541
1022.386313	95670.082315	34.683559
1023.306507	95848.947193	34.688576
1024.462076	96019.938250	34.693594
1025.639051	96194.984375	34.698612
1026.209725	96378.734125	34.703629
1027.417936	96556.227315	34.708647
1029.326856	96721.363965	34.713664
1030.455623	96889.042243	34.718682
1031.409141	97054.452784	34.723700
1032.652959	97222.696691	34.728717
1033.543934	97381.941580	34.733735
1034.656952	97552.893291	34.738752
1035.378332	97732.019834	34.743770
1036.840957	97894.845159	34.748788
1037.454933	98065.534613	34.753805
1038.981171	98248.640360	34.758823
1039.836811	98413.487372	34.763840
1040.851536	98597.768949	34.768858
1041.737243	98776.913842	34.773876
1042.733449	98966.556773	34.778893
1043.649405	99133.006516	34.783911
1044.690220	99323.720978	34.788928
1045.571884	99503.428816	34.793946
1047.324101	99673.548811	34.798964
1048.389323	99867.802229	34.803981
1049.404797	100047.042371	34.808999
1050.348057	100220.509317	34.814016
1050.874007	100416.185453	34.819034
1052.388414	100608.471143	34.824052
1052.964280	100786.611541	34.829069
1053.969548	100988.088112	34.834087
1055.290117	101165.304185	34.839104
1056.247244	101359.263997	34.844122
1057.382769	101552.227166	34.849140
1058.407265	101744.779602	34.854157
1059.860568	101923.200960	34.859175
1060.651009	102100.941578	34.864192
1061.985502	102291.876795	34.869210
1063.628146	102478.697806	34.874228
1064.276545	102674.067148	34.879245
1065.336642	102859.480214	34.884263
1066.495020	103041.130121	34.889280
1067.239433	103235.063276	34.894298
1068.421203	103416.180112	34.899316
1069.216603	103618.326189	34.904333
1070.166389	103816.832941	34.909351
1071.315292	104011.300331	34.914368
1072.382495	104212.912302	34.919386
1073.758422	104402.045408	34.924404
1074.537756	104606.019086	34.929421
1075.641388	104807.522015	34.934439
1076.597042	105006.328164	34.939456
1077.524665	105202.645620	34.944474
1078.579356	105402.324924	34.949492
1079.352717	105606.269416	34.954509
1080.463061	105805.663995	34.959527
1081.748855	106014.174913	34.964544
1082.632233	106223.653107	34.969562
1084.340064	106422.168530	34.974580
1086.444686	106599.330403	34.979597
1087.601026	106779.689584	34.984615
1088.989104	106963.595934	34.989632
1089.812250	107146.773593	34.994650
1091.228133	107330.513260	34.999668
1091.900780	107492.871319	35.004685
1092.934937	107665.568918	35.009703
1094.224260	107825.370141	35.014720
1095.059788	107994.797003	35.019738
1096.636780	108146.573425	35.024756
1097.806923	108298.620525	35.029773
1098.971999	108459.319997	35.034791
1100.253502	108621.445116	35.039808
1100.886001	108796.686184	35.044826
1101.923862	108955.066457	35.049844
1103.151789	109119.660633	35.054861
1103.724071	109298.448741	35.059879
1104.805060	109475.064145	35.064896
1105.528767	109669.320460	35.069914
1106.652861	109850.592402	35.074932
1107.586931	110054.253201	35.079949
1108.181037	110235.057893	35.084967
1109.862648	110415.646275	35.089984
1110.451292	110622.509701	35.095002
1111.867352	110812.049267	35.100020
1112.706152	111006.131528	35.105037
1113.791259	111209.586087	35.110055
1115.226579	111400.887298	35.115072
1116.340364	111606.379491	35.120090
1117.619769	111796.087820	35.125108
1118.348029	112012.844574	35.130125
1119.367692	112216.279449	35.135143
1120.942027	112398.887508	35.140160
1122.741537	112596.673432	35.145178
1124.094606	112780.828011	35.150196
1124.864942	112984.791119	35.155213
1126.006897	113177.331290	35.160231
1126.733244	113384.889637	35.165248
1127.819543	113587.183544	35.170266
1128.947355	113785.342255	35.175284
1130.123488	113992.742244	35.180301
1131.176350	114199.315354	35.185319
1132.371450	114406.981347	35.190336
1133.043746	114616.926852	35.195354
1134.188867	114816.458274	35.200372
1135.280833	115043.073000	35.205389
1136.048999	115257.466903	35.210407
1137.163208	115476.657533	35.215424
1138.391769	115708.626740	35.220442
1139.769946	115918.680880	35.225460
1140.781566	116147.509571	35.230477
1141.355939	116379.414935	35.235495
1142.496825	116617.487405	35.240512
1143.367011	116852.996636	35.245530
1144.306113	117088.319078	35.250548
1145.394336	117336.098590	35.255565
1146.235217	117572.492856	35.260583
1147.583346	117820.347720	35.265600
1148.500368	118078.285290	35.270618
1149.638481	118322.251454	35.275636
1151.049172	118582.316708	35.280653
1152.109062	118829.721105	35.285671
1153.367870	119074.345291	35.290688
1154.189592	119331.841079	35.295706
1155.488075	119575.461999	35.300724
1157.143643	119831.886979	35.305741
1158.233543	120083.529278	35.310759
1159.838130	120324.381728	35.315776
1160.741718	120576.223788	35.320794
1162.276241	120798.705826	35.325812
1163.247522	121039.757450	35.330829
1164.235376	121299.739583	35.335847
1165.651896	121531.826374	35.340864
1166.465343	121782.122455	35.345882
1167.763865	122013.370865	35.350900
1168.856223	122245.567509	35.355917
1169.924391	122491.050274	35.360935
1171.413690	122712.870049	35.365952
1172.400294	122950.982256	35.370970
1173.657712	123172.374890	35.375988
1175.206645	123412.146773	35.381005
1176.115105	123637.554285	35.386023
1177.649970	123860.731110	35.391040
1179.095774	124095.570544	35.396058
1180.481237	124316.329613	35.401076
1182.403147	124514.583396	35.406093
1184.216384	124723.476399	35.411111
1186.137163	124913.267461	35.416128
1187.297106	125122.549894	35.421146
1188.098701	125321.665627	35.426164
1189.516873	125517.816733	35.431181
1190.138104	125740.727506	35.436199
1191.093292	125941.925776	35.441216
1191.703347	126164.005068	35.446234
1192.975457	126386.458308	35.451252
1194.088182	126590.499142	35.456269
1195.273617	126823.717261	35.461287
1196.447560	127048.739009	35.466304
1197.714510	127274.431468	35.471322
1198.610340	127500.465685	35.476340
1199.660190	127732.255609	35.481357
1201.020520	127975.060744	35.486375
1202.156476	128186.763730	35.491392
1202.974232	128432.158904	35.496410
1203.788291	128660.902172	35.501428
1206.233899	128885.841585	35.506445
1208.337327	129094.349188	35.511463
1209.852841	129298.835899	35.516480
1211.113302	129523.810805	35.521498
1212.235135	129732.687530	35.526516
1213.621738	129962.296543	35.531533
1214.198151	130168.401633	35.536551
1215.841791	130373.938993	35.541568
1216.946563	130617.694323	35.546586
1217.601978	130819.607775	35.551604
1219.014919	131045.430426	35.556621
1219.548644	131272.363175	35.561639
1220.611428	131502.898889	35.566656
1222.409547	131727.889641	35.571674
1224.171615	131948.590795	35.576692
1225.680131	132159.448021	35.581709
1227.187713	132385.518172	35.586727
1228.247614	132596.642496	35.591744
1228.764151	132829.014675	35.596762
1229.832002	133048.456349	35.601780
1230.983481	133288.092064	35.606797
1231.669591	133518.413033	35.611815
1233.023714	133756.675091	35.616832
1233.924626	134005.801665	35.621850
1234.909237	134239.133641	35.626868
1236.376214	134487.790208	35.631885
1237.154482	134751.369188	35.636903
1238.351496	134987.308346	35.641920
1239.461078	135250.164812	35.646938
1239.990392	135517.239327	35.651956
1240.995440	135773.981432	35.656973
1242.158734	136038.153852	35.661991
1243.765388	136296.854540	35.667008
1244.811207	136570.685687	35.672026
1246.351134	136840.659554	35.677044
1248.280700	137080.372365	35.682061
1249.351101	137336.875042	35.687079
1250.905326	137577.731057	35.692096
1252.488801	137818.190973	35.697114
1253.149709	138059.476858	35.702132
1254.712575	138301.401688	35.707149
1255.878305	138552.928088	35.712167
1257.034663	138792.235726	35.717184
1258.628174	139038.420867	35.722202
1259.442711	139280.818635	35.727220
1260.498652	139518.030671	35.732237
1261.856904	139788.755805	35.737255
1264.108475	140026.522148	35.742272
1265.738775	140261.628647	35.747290
1266.250955	140500.687070	35.752308
1268.233706	140737.285572	35.757325
1269.712105	140966.120386	35.762343
1271.821683	141182.870407	35.767360
1273.752199	141404.025827	35.772378
1275.038269	141612.862948	35.777396
1276.346717	141833.477157	35.782413
1277.279269	142052.734683	35.787431
1277.941234	142272.583505	35.792448
1279.077253	142511.096555	35.797466
1279.801262	142745.114418	35.802484
1281.142777	142970.016330	35.807501
1282.019726	143225.340283	35.812519
1283.151582	143485.277741	35.817536
1283.836164	143743.173323	35.822554
1284.547263	144009.613138	35.827572
1286.078450	144284.035257	35.832589
1287.119817	144561.266735	35.837607
1288.111137	144831.813164	35.842624
1289.900600	145113.021444	35.847642
1291.064339	145382.922281	35.852660
1292.023915	145664.753804	35.857677
1292.963128	145961.745043	35.862695
1294.259780	146249.688675	35.867712
1295.509270	146538.276491	35.872730
1296.561583	146834.774443	35.877748
1298.588518	147122.046588	35.882765
1299.621710	147416.142983	35.887783
1300.961699	147713.361617	35.892800
1302.828394	148000.882818	35.897818
1303.495313	148296.124803	35.902836
1305.209096	148601.430944	35.907853
1306.005074	148904.684404	35.912871
1307.576942	149195.079189	35.917888
1309.079358	149484.955079	35.922906
1311.023750	149781.367953	35.927924
1312.444352	150074.737037	35.932941
1314.130012	150345.248341	35.937959
1315.930313	150613.903685	35.942976
1318.197656	150873.276050	35.947994
1319.157780	151154.579400	35.953012
1321.223683	151394.672327	35.958029
1322.488496	151659.136698	35.963047
1323.950613	151909.174786	35.968064
1325.122544	152167.747645	35.973082
1326.154194	152428.590415	35.978100
1327.623703	152683.033611	35.983117
1328.460877	152940.271824	35.988135
1329.942305	153202.098450	35.993152
1331.182752	153469.141669	35.998170
1332.022833	153726.980873	36.003188
1333.638948	153973.937688	36.008205
1334.848143	154243.020928	36.013223
1336.445831	154500.714947	36.018240
1337.912683	154768.884142	36.023258
1338.657401	155030.857564	36.028276
1340.246376	155283.624040	36.033293
1341.098061	155535.270763	36.038311
1342.176389	155779.118725	36.043328
1343.730497	156046.140754	36.048346
1344.766298	156306.844333	36.053364
1345.825873	156559.110285	36.058381
1346.879693	156838.144073	36.063399
1347.509449	157124.416884	36.068416
1349.271138	157398.352594	36.073434
1350.889247	157672.326585	36.078452
1352.140119	157947.669668	36.083469
1353.860105	158223.558823	36.088487
1354.954490	158500.783631	36.093504
1356.840673	158791.757717	36.098522
1358.158295	159055.743835	36.103540
1360.208253	159319.877229	36.108557
1361.391655	159599.619408	36.113575
1363.063716	159861.636755	36.118592
1363.832024	160136.909595	36.123610
1365.249949	160415.438908	36.128628
1366.572756	160690.928454	36.133645
1368.015975	160977.031082	36.138663
1369.028450	161263.980664	36.143680
1370.728622	161541.583025	36.148698
1372.547381	161827.287069	36.153716
1374.186473	162095.845060	36.158733
1375.319281	162387.654265	36.163751
1376.152915	162659.380955	36.168768
1377.851525	162943.006511	36.173786
1378.363527	163247.040154	36.178804
1379.684249	163528.448388	36.183821
1381.068600	163855.369475	36.188839
1381.943711	164156.266788	36.193856
1383.345329	164464.438003	36.198874
1384.561348	164797.610944	36.203892
1385.909331	165091.763261	36.208909
1386.944110	165427.470471	36.213927
1388.654317	165739.748825	36.218944
1390.511553	166055.380138	36.223962
1392.264392	166361.578509	36.228980
1394.175452	166670.214403	36.233997
1395.352983	166983.439747	36.239015
1396.680912	167291.059730	36.244032
1398.325735	167598.591514	36.249050
1399.390005	167922.398902	36.254068
1400.608686	168231.477289	36.259085
1401.975614	168554.896784	36.264103
1403.529270	168871.803938	36.269120
1405.163322	169178.460296	36.274138
1406.620052	169498.991499	36.279156
1407.976761	169797.653177	36.284173
1409.475648	170124.919690	36.289191
1410.573683	170448.625657	36.294208
1412.191735	170749.661432	36.299226
1413.459136	171075.069644	36.304244
1414.774270	171394.089568	36.309261
1415.911148	171717.709324	36.314279
1417.147956	172047.266247	36.319296
1418.540108	172374.744174	36.324314
1419.598716	172717.088330	36.329332
1420.903719	173044.014331	36.334349
1422.089390	173393.867535	36.339367
1423.717732	173731.404481	36.344384
1425.436175	174064.373254	36.349402
1426.560814	174415.982675	36.354420
1428.543166	174748.595462	36.359437
1430.238110	175064.811345	36.364455
1431.709129	175379.581498	36.369472
1433.358887	175676.341803	36.374490
1435.798161	175962.871965	36.379508
1437.696792	176255.711462	36.384525
1439.163403	176547.926035	36.389543
1440.496567	176826.293357	36.394560
1442.764657	177093.987265	36.399578
1444.102975	177372.458378	36.404596
1445.966605	177646.389844	36.409613
1447.860771	177893.742705	36.414631
1449.126571	178171.316551	36.419648
1450.761239	178421.544999	36.424666
1451.684160	178705.270190	36.429684
1452.752919	178966.953455	36.434701
1454.287774	179263.805210	36.439719
1455.267518	179544.327545	36.444736
1456.497152	179825.711304	36.449754
1457.831967	180120.037421	36.454772
1459.430147	180414.232944	36.459789
1460.678973	180690.338584	36.464807
1462.264139	181000.531265	36.469824
1463.586523	181293.723938	36.474842
1464.813755	181592.658070	36.479860
1466.030941	181898.246230	36.484877
1467.259608	182214.292619	36.489895
1468.274481	182520.108199	36.494912
1469.566982	182840.780504	36.499930
1471.027330	183166.580173	36.504948
1472.888977	183485.525171	36.509965
1474.440958	183821.264635	36.514983
1475.634506	184144.512375	36.520000
1476.743778	184483.882995	36.525018
1477.882714	184829.102230	36.530036
1479.073782	185175.089336	36.535053
1480.272827	185528.020368	36.540071
1481.777152	185879.380151	36.545088
1483.469928	186243.023397	36.550106
1485.382848	186602.786688	36.555124
1486.882482	186946.258909	36.560141
1488.913322	187286.916532	36.565159
1489.805013	187654.877355	36.570176
1492.066058	188000.769114	36.575194
1493.968064	188324.216539	36.580212
1496.352438	188649.337942	36.585229
1498.185403	188982.244591	36.590247
1499.358058	189311.238211	36.595264
1500.521768	189649.628654	36.600282
1501.858165	189984.577918	36.605300
1502.997083	190316.438980	36.610317
1504.255941	190663.641988	36.615335
1505.396312	191009.381392	36.620352
1506.973321	191358.313200	36.625370
1508.243087	191716.729643	36.630388
1509.725394	192076.166814	36.635405
1511.238408	192422.563866	36.640423
1512.692453	192791.733960	36.645440
1514.229500	193145.176681	36.650458
1515.443711	193517.424795	36.655476
1516.758702	193885.037655	36.660493
1518.615313	194235.412613	36.665511
1519.754900	194613.265427	36.670528
1521.428158	194978.312097	36.675546
1522.870371	195356.513038	36.680564
1523.949179	195742.901121	36.685581
1525.557834	196112.586092	36.690599
1527.120343	196499.736869	36.695616
1528.438519	196880.519146	36.700634
1529.559591	197261.044211	36.705652
1530.928148	197632.618421	36.710669
1532.217367	198009.666955	36.715687
1533.589478	198397.888872	36.720704
1535.231043	198765.717340	36.725722
1536.451295	199157.206199	36.730740
1537.610467	199558.280141	36.735757
1539.416250	199935.140145	36.740775
1541.133452	200332.051221	36.745792
1542.636359	200713.244102	36.750810
1544.501170	201122.196733	36.755828
1546.669960	201506.242362	36.760845
1548.284058	201891.130733	36.765863
1549.762714	202269.060560	36.770880
1551.379689	202659.919995	36.775898
1552.926418	203050.577343	36.780916
1554.731416	203431.341657	36.785933
1556.854647	203809.452669	36.790951
1558.553582	204202.109960	36.795968
1560.267939	204583.872970	36.800986
1561.766288	204969.571557	36.806004
1562.904657	205353.795235	36.811021
1565.201251	205719.533413	36.816039
1567.500467	206080.549646	36.821056
1569.485564	206446.545931	36.826074
1570.888721	206819.623464	36.831092
1571.954542	207193.406045	36.836109
1573.129958	207563.375869	36.841127
1574.711781	207955.183377	36.846144
1576.095427	208357.107325	36.851162
1577.221649	208732.398356	36.856180
1578.345170	209127.449023	36.861197
1580.304807	209530.096547	36.866215
1580.933763	209948.291770	36.871232
1582.410954	210348.343777	36.876250
1584.015022	210766.826744	36.881268
1585.318039	211189.361350	36.886285
1587.338049	211600.796080	36.891303
1588.728677	212030.723406	36.896320
1590.202897	212459.978830	36.901338
1591.798880	212895.032078	36.906356
1593.067812	213321.887660	36.911373
1594.737000	213755.180816	36.916391
1596.179342	214193.262724	36.921408
1598.225456	214632.593215	36.926426
1600.299282	215073.013368	36.931444
1601.880149	215498.481968	36.936461
1604.096457	215928.317616	36.941479
1605.287197	216363.276961	36.946496
1606.935557	216800.905761	36.951514
1608.571458	217230.386064	36.956532
1610.444857	217644.895333	36.961549
1612.732857	218075.592544	36.966567
1614.236538	218488.566406	36.971584
1616.223064	218960.461803	36.976602
1618.244513	219377.239875	36.981620
1619.910504	219776.274224	36.986637
1622.247806	220172.735765	36.991655
1624.021163	220564.542409	36.996672
1625.706428	220942.751512	37.001690
1627.933919	221331.971704	37.006708
1629.446075	221719.355677	37.011725
1631.241190	222089.016864	37.016743
1632.336455	222481.602953	37.021760
1633.986665	222860.485091	37.026778
1636.861724	223208.205074	37.031796
1639.046814	223570.466679	37.036813
1640.637376	223916.013314	37.041831
1642.278326	224289.237882	37.046848
1643.647676	224614.173576	37.051866
1645.729018	224940.084899	37.056884
1646.926608	225271.781638	37.061901
1648.577756	225605.334857	37.066919
1650.130753	225945.483720	37.071936
1651.247578	226258.908859	37.076954
1652.970811	226599.691898	37.081972
1654.047147	226943.579809	37.086989
1655.435681	227293.919554	37.092007
1656.613775	227655.852002	37.097024
1658.301011	228013.612093	37.102042
1659.642842	228386.111454	37.107060
1660.712554	228759.317206	37.112077
1662.363453	229133.901365	37.117095
1663.400434	229539.144497	37.122112
1664.580098	229913.910230	37.127130
1666.140202	230327.426192	37.132148
1666.977038	230745.457042	37.137165
1668.553228	231168.218703	37.142183
1669.755689	231595.183623	37.147200
1671.305609	232033.141853	37.152218
1672.755891	232487.476023	37.157236
1674.100318	232940.051003	37.162253
1675.941920	233398.489178	37.167271
1677.353943	233863.400700	37.172288
1678.736964	234342.720889	37.177306
1680.497014	234813.089897	37.182324
1682.142740	235299.913825	37.187341
1683.819341	235783.609744	37.192359
1685.569129	236260.233385	37.197376
1687.350868	236734.592360	37.202394
1689.509604	237222.505720	37.207412
1691.164623	237716.955571	37.212429
1693.480421	238188.385366	37.217447
1694.973952	238664.498961	37.222464
1697.522204	239130.228191	37.227482
1699.597080	239602.209329	37.232500
1701.036473	240078.030544	37.237517
1703.443926	240535.606895	37.242535
1705.835984	240988.131783	37.247552
1707.771706	241432.934462	37.252570
1709.946122	241880.950169	37.257588
1711.741398	242335.735543	37.262605
1713.657106	242784.557819	37.267623
1714.846692	243237.031692	37.272640
1716.368461	243681.983307	37.277658
1717.916067	244132.164383	37.282676
1719.031015	244588.641268	37.287693
1720.727473	245058.359375	37.292711
1722.637211	245516.586547	37.297728
1724.067206	245981.091881	37.302746
1725.731631	246430.825738	37.307764
1727.607101	246911.516813	37.312781
1729.465497	247383.726942	37.317799
1731.782482	247834.015705	37.322816
1733.606796	248292.464481	37.327834
1735.297598	248749.945195	37.332852
1737.257004	249224.478360	37.337869
1738.432570	249678.615873	37.342887
1740.006331	250140.156713	37.347904
1741.631007	250604.458618	37.352922
1743.520455	251070.139933	37.357940
1745.587323	251534.319098	37.362957
1747.152924	251998.632235	37.367975
1749.078143	252459.253845	37.372992
1750.004340	252926.670900	37.378010
1752.047840	253394.386692	37.383028
1754.027055	253856.321543	37.388045
1755.920419	254311.513652	37.393063
1757.370101	254740.893397	37.398080
1759.505445	255199.170767	37.403098
1760.962963	255637.593283	37.408116
1762.486096	256084.921741	37.413133
1763.712008	256537.888163	37.418151
1765.395986	257001.601008	37.423168
1766.542951	257475.894181	37.428186
1768.204962	257936.740419	37.433204
1769.998678	258430.944991	37.438221
1771.329571	258907.773968	37.443239
1773.004950	259418.586629	37.448256
1774.255273	259917.072663	37.453274
1776.081069	260400.780681	37.458292
1777.512483	260926.469221	37.463309
1779.588988	261437.698441	37.468327
1782.071059	261937.607029	37.473344
1784.068065	262430.177784	37.478362
1786.809205	262926.563173	37.483380
1788.722338	263415.133779	37.488397
1790.690075	263914.821837	37.493415
1793.000331	264394.892669	37.498432
1795.044230	264880.443513	37.503450
1796.856463	265361.739172	37.508468
1798.425270	265858.316639	37.513485
1799.885498	266353.235080	37.518503
1802.017274	266845.476663	37.523520
1803.449727	267351.068277	37.528538
1804.844372	267848.612901	37.533556
1806.348297	268357.468838	37.538573
1808.023434	268862.307745	37.543591
1809.994476	269377.283941	37.548608
1811.449123	269886.654464	37.553626
1813.350096	270405.934139	37.558644
1815.138304	270926.755937	37.563661
1817.264178	271449.782198	37.568679
1819.081163	271969.454688	37.573696
1820.806942	272498.718339	37.578714
1822.850327	273019.952287	37.583732
1824.788985	273552.456104	37.588749
1826.691772	274072.619201	37.593767
1828.786877	274599.328966	37.598784
1830.446591	275118.412593	37.603802
1832.489624	275636.187292	37.608820
1834.435400	276169.701211	37.613837
1835.870797	276698.598765	37.618855
1837.920017	277212.152491	37.623872
1839.333141	277750.475774	37.628890
1841.313722	278288.424797	37.633908
1842.868580	278829.973696	37.638925
1844.894085	279363.060914	37.643943
1847.057267	279910.298494	37.648960
1848.917350	280446.890377	37.653978
1851.219752	280972.103997	37.658996
1853.310345	281501.136058	37.664013
1855.134770	282024.418958	37.669031
1857.339399	282538.543853	37.674048
1858.818404	283072.803569	37.679066
1861.164533	283592.134911	37.684084
1862.486428	284133.860047	37.689101
1864.177879	284658.122504	37.694119
1866.170519	285186.575685	37.699136
1867.415308	285730.569138	37.704154
1869.371964	286259.253395	37.709172
1871.126829	286797.316795	37.714189
1872.916917	287335.651929	37.719207
1874.682534	287870.407655	37.724224
1877.380319	288392.688271	37.729242
1879.970212	288882.268597	37.734260
1881.918499	289383.256403	37.739277
1884.125185	289872.896533	37.744295
1886.256598	290370.548517	37.749312
1887.741784	290853.293627	37.754330
1890.411092	291318.798049	37.759348
1891.996751	291800.964345	37.764365
1893.727380	292297.583033	37.769383
1895.476704	292778.016877	37.774400
1896.951275	293285.773770	37.779418
1898.795286	293781.275722	37.784436
1900.642968	294280.686626	37.789453
1902.310343	294782.944566	37.794471
1904.057598	295277.668946	37.799488
1905.963485	295789.357289	37.804506
1907.377266	296309.506310	37.809524
1908.669800	296840.391414	37.814541
1910.570722	297376.380465	37.819559
1912.712726	297904.504277	37.824576
1914.030662	298454.147263	37.829594
1915.974067	298994.108965	37.834612
1917.926848	299546.537059	37.839629
1919.560265	300100.792798	37.844647
1921.664752	300664.923980	37.849664
1923.167678	301229.430632	37.854682
1925.144143	301797.310121	37.859700
1927.126191	302371.661874	37.864717
1928.580324	302957.018324	37.869735
1930.923193	303535.722846	37.874752
1932.430056	304123.120645	37.879770
1934.364723	304709.250522	37.884788
1936.430319	305297.513828	37.889805
1938.612556	305889.614422	37.894823
1941.190640	306460.845904	37.899840
1942.935707	307060.147322	37.904858
1944.935238	307638.882391	37.909876
1946.971287	308238.534044	37.914893
1948.683062	308835.111262	37.919911
1950.798186	309435.604882	37.924928
1952.756978	310039.497584	37.929946
1954.604991	310636.623536	37.934964
1956.895156	311234.687987	37.939981
1958.626566	311837.030341	37.944999
1960.661802	312439.775124	37.950016
1962.626399	313042.044432	37.955034
1964.984341	313642.187233	37.960052
1967.022951	314240.575015	37.965069
1968.702714	314837.950712	37.970087
1971.040085	315443.212272	37.975104
1973.035548	316051.851864	37.980122
1974.832879	316650.869564	37.985140
1976.807486	317263.489273	37.990157
1978.854449	317868.321549	37.995175
1980.693817	318461.984675	38.000192
1982.830629	319073.495534	38.005210
1984.829428	319683.398672	38.010228
1987.015983	320285.241517	38.015245
1988.647797	320908.372823	38.020263
1990.684069	321516.933001	38.025280
1993.295708	322122.523504	38.030298
1995.321405	322722.949115	38.035316
1997.080980	323326.231521	38.040333
1998.652366	323947.973062	38.045351
2000.941993	324546.459354	38.050368
2002.596813	325159.847260	38.055386
2004.185101	325770.117200	38.060404
2006.087113	326400.438148	38.065421
2007.923428	327010.985068	38.070439
2009.567771	327623.309430	38.075456
2011.249971	328237.246274	38.080474
2013.335723	328849.206142	38.085492
2015.646151	329455.283320	38.090509
2018.790307	330033.188153	38.095527
2020.916516	330616.713596	38.100544
2022.845706	331216.742321	38.105562
2024.495766	331808.356810	38.110580
2026.916291	332413.166389	38.115597
2029.107880	332998.992456	38.120615
2032.264750	333571.579077	38.125632
2034.429043	334164.784974	38.130650
2036.181857	334742.973006	38.135668
2038.513754	335320.044009	38.140685
2040.114147	335916.776457	38.145703
2042.159456	336496.649243	38.150720
2043.836742	337110.922418	38.155738
2045.405852	337707.665485	38.160756
2047.734361	338314.557269	38.165773
2049.364270	338925.441014	38.170791
2051.060388	339537.753539	38.175808
2053.217179	340163.918390	38.180826
2055.143845	340782.016277	38.185844
2057.787004	341388.337704	38.190861
2059.653555	342010.644056	38.195879
2061.824607	342641.725485	38.200896
2063.750897	343260.503611	38.205914
2066.166065	343880.690852	38.210932
2068.660838	344497.329088	38.215949
2070.576352	345135.197400	38.220967
2073.448610	345736.199012	38.225984
2075.618730	346360.481134	38.231002
2077.581933	346972.911316	38.236020
2079.599288	347592.380164	38.241037
2081.439650	348230.295408	38.246055
2083.308404	348840.457957	38.251072
2085.270302	349479.681025	38.256090
2087.261729	350110.896133	38.261108
2089.751951	350741.867950	38.266125
2091.240991	351383.502384	38.271143
2093.118430	352023.566326	38.276160
2095.553420	352659.773339	38.281178
2097.210202	353324.013673	38.286196
2099.246427	353962.779898	38.291213
2100.780291	354635.623086	38.296231
2103.090082	355294.549048	38.301248
2105.255671	355962.014666	38.306266
2107.389203	356624.983836	38.311284
2110.981477	357256.517229	38.316301
2113.112283	357921.268060	38.321319
2115.382539	358553.938764	38.326336
2118.140349	359198.393981	38.331354
2119.826268	359856.057405	38.336372
2121.965197	360492.119967	38.341389
2123.784494	361137.815840	38.346407
2125.759559	361789.843934	38.351424
2127.519085	362437.228743	38.356442
2129.090713	363103.433617	38.361460
2130.987862	363760.415017	38.366477
2132.399739	364455.367793	38.371495
2134.456377	365138.937982	38.376512
2136.243980	365829.136409	38.381530
2137.792472	366526.084547	38.386548
2139.432235	367231.148064	38.391565
2141.168607	367952.798243	38.396583
2142.858658	368683.117788	38.401600
2145.031205	369415.246070	38.406618
2146.699008	370153.277398	38.411636
2149.096116	370867.152777	38.416653
2151.223875	371579.181751	38.421671
2153.769922	372290.189427	38.426688
2156.068280	372993.640253	38.431706
2158.082983	373720.382418	38.436724
2160.079668	374431.184968	38.441741
2162.084223	375159.827191	38.446759
2163.963508	375874.373921	38.451776
2166.320362	376617.079949	38.456794
2168.118152	377365.213554	38.461812
2170.503973	378107.122296	38.466829
2172.531670	378866.699168	38.471847
2174.707796	379618.474885	38.476864
2176.833140	380380.766232	38.481882
2178.978739	381141.921363	38.486900
2181.471659	381891.996917	38.491917
2183.933316	382664.349501	38.496935
2186.177135	383431.750264	38.501952
2189.065108	384189.518630	38.506970
2190.928645	384959.811737	38.511988
2193.828439	385721.548829	38.517005
2195.817433	386498.503798	38.522023
2198.093661	387244.588474	38.527040
2200.686698	388010.581471	38.532058
2203.176516	388759.713957	38.537076
2206.184353	389502.861770	38.542093
2208.260289	390248.985024	38.547111
2210.912744	390983.435713	38.552128
2213.822735	391724.062638	38.557146
2216.931020	392437.236790	38.562164
2219.682813	393144.445612	38.567181
2222.057333	393854.412547	38.572199
2224.217695	394582.521592	38.577216
2226.959655	395288.009357	38.582234
2228.960768	395989.851544	38.587252
2230.774575	396685.245080	38.592269
2233.146267	397391.707540	38.597287
2235.842854	398084.920548	38.602304
2238.614014	398766.041352	38.607322
2240.579175	399464.994142	38.612340
2243.197438	400151.860839	38.617357
2245.074789	400824.616640	38.622375
2247.472659	401532.647531	38.627392
2250.437103	402204.152933	38.632410
2252.458177	402887.885409	38.637428
2254.321778	403568.662734	38.642445
2256.398528	404266.340335	38.647463
2258.598544	404952.552801	38.652480
2260.939890	405630.617148	38.657498
2262.958150	406324.756703	38.662516
2265.103961	407013.562605	38.667533
2267.144054	407712.503138	38.672551
2269.376552	408417.474669	38.677568
2271.276139	409124.712420	38.682586
2273.357461	409833.548591	38.687604
2275.739510	410533.450078	38.692621
2278.042009	411258.831082	38.697639
2279.504313	411963.533647	38.702656
2281.715157	412697.858368	38.707674
2283.496781	413440.415371	38.712692
2285.218641	414182.961450	38.717709
2287.056100	414930.356088	38.722727
2289.135353	415704.106989	38.727744
2291.042094	416465.174348	38.732762
2293.183165	417243.554969	38.737780
2295.597554	418010.318455	38.742797
2297.590849	418794.602963	38.747815
2299.599391	419586.002452	38.752832
2301.537300	420351.153689	38.757850
2303.429529	421131.407168	38.762868
2305.592352	421898.297798	38.767885
2307.936024	422684.860538	38.772903
2309.942165	423471.049054	38.777920
2311.920921	424250.710067	38.782938
2314.227757	425070.321672	38.787956
2316.643943	425875.355399	38.792973
2319.153087	426678.473880	38.797991
2321.680430	427487.892018	38.803008
2323.949876	428295.300436	38.808026
2326.271496	429107.533687	38.813044
2328.571197	429928.197929	38.818061
2330.999293	430738.839525	38.823079
2334.558712	431545.470155	38.828096
2337.107865	432353.404194	38.833114
2339.253583	433185.826886	38.838132
2342.128761	433999.623847	38.843149
2344.854352	434810.278831	38.848167
2347.335435	435612.948598	38.853184
2349.560430	436420.845939	38.858202
2351.962603	437230.710189	38.863220
2354.653557	438026.631021	38.868237
2357.547883	438834.079856	38.873255
2359.935922	439641.583440	38.878272
2362.606253	440443.343893	38.883290
2364.597408	441231.170725	38.888308
2367.000324	442033.323291	38.893325
2369.161296	442848.389711	38.898343
2371.883030	443661.360441	38.903360
2374.443455	444459.199762	38.908378
2376.405504	445275.524923	38.913396
2378.957678	446095.972072	38.918413
2381.005487	446907.466483	38.923431
2382.962678	447737.612476	38.928448
2385.148095	448564.046747	38.933466
2387.487324	449406.003806	38.938484
2390.358501	450223.661793	38.943501
2393.041624	451048.046577	38.948519
2395.609664	451875.554153	38.953536
2398.688875	452686.204295	38.958554
2401.360859	453507.713228	38.963572
2404.379086	454319.119529	38.968589
2406.799662	455130.289363	38.973607
2409.214213	455945.170560	38.978624
2411.511948	456738.244782	38.983642
2413.345077	457556.141635	38.988660
2415.499063	458367.936043	38.993677
2418.245198	459188.853102	38.998695
2420.115700	460024.138817	39.003712
2422.499979	460853.238625	39.008730
2424.577090	461690.949176	39.013748
2426.538393	462546.539265	39.018765
2428.837368	463387.225968	39.023783
2430.664222	464237.003031	39.028800
2433.092679	465096.349211	39.033818
2435.165911	465969.363204	39.038836
2437.276675	466845.465761	39.043853
2439.856855	467735.147677	39.048871
2442.049061	468618.434790	39.053888
2444.434160	469507.410752	39.058906
2446.983240	470408.597949	39.063924
2449.556573	471303.069022	39.068941
2452.366045	472191.345592	39.073959
2455.001892	473087.743833	39.078976
2457.937192	473952.271854	39.083994
2461.432746	474808.180585	39.089012
2464.407934	475658.831794	39.094029
2467.307557	476496.423856	39.099047
2469.099995	477321.178961	39.104064
2471.707902	478130.761283	39.109082
2473.997757	478951.018000	39.114100
2476.606232	479758.761112	39.119117
2478.886946	480588.239606	39.124135
2481.211465	481405.350809	39.129152
2483.746404	482232.036166	39.134170
2486.470945	483053.501910	39.139188
2488.713259	483872.232631	39.144205
2491.679385	484687.575310	39.149223
2494.716047	485510.897343	39.154240
2497.276374	486308.157587	39.159258
2499.441284	487137.455483	39.164276
2502.102107	487966.885332	39.169293
2504.354172	488772.314615	39.174311
2506.853484	489613.859734	39.179328
2508.858832	490450.398324	39.184346
2511.345960	491288.331730	39.189364
2513.775356	492133.048047	39.194381
2516.294142	492970.895213	39.199399
2518.339038	493842.087927	39.204416
2520.648142	494693.764393	39.209434
2523.089292	495560.363947	39.214452
2525.567225	496443.110873	39.219469
2528.169783	497326.598834	39.224487
2530.215863	498211.494802	39.229504
2532.860313	499091.755690	39.234522
2535.155941	499998.513490	39.239540
2537.660370	500893.181818	39.244557
2540.260735	501796.613964	39.249575
2542.062174	502727.517796	39.254592
2545.040418	503643.245963	39.259610
2547.269770	504587.037954	39.264628
2549.273913	505524.912457	39.269645
2551.896776	506459.908163	39.274663
2554.293076	507414.150306	39.279680
2556.903763	508360.082204	39.284698
2559.762633	509314.539734	39.289716
2562.047667	510283.051253	39.294733
2566.125196	511209.466297	39.299751
2568.760843	512168.529989	39.304768
2571.386574	513111.759975	39.309786
2574.027222	514064.710018	39.314804
2576.233038	515013.390184	39.319821
2578.729705	515964.636433	39.324839
2581.367147	516926.888882	39.329856
2583.780559	517877.579147	39.334874
2586.931164	518832.776094	39.339892
2589.730230	519782.883153	39.344909
2592.646406	520723.641976	39.349927
2595.044256	521692.188249	39.354944
2597.879192	522647.049918	39.359962
2600.093881	523607.847901	39.364980
2602.576434	524564.813673	39.369997
2605.600379	525514.628743	39.375015
2608.043906	526469.717665	39.380032
2610.646550	527425.273738	39.385050
2613.573517	528377.895426	39.390068
2615.746396	529338.234587	39.395085
2618.940814	530278.353891	39.400103
2622.314084	531218.031677	39.405120
2625.222839	532158.481444	39.410138
2627.926191	533094.625940	39.415156
2630.874112	534031.777843	39.420173
2633.551336	534963.075377	39.425191
2635.415797	535898.121598	39.430208
2638.146710	536822.345369	39.435226
2640.477074	537728.962078	39.440244
2642.596786	538648.137162	39.445261
2645.011907	539553.215951	39.450279
2647.137445	540466.033968	39.455296
2649.694241	541372.181819	39.460314
2652.863919	542281.139190	39.465332
2655.541692	543202.545059	39.470349
2658.491758	544108.805253	39.475367
2661.027196	545022.519850	39.480384
2663.748530	545956.765963	39.485402
2666.033357	546876.687992	39.490420
2668.107523	547814.789011	39.495437
2670.858193	548769.259446	39.500455
2673.100604	549708.461768	39.505472
2675.703286	550671.373311	39.510490
2677.962558	551645.887767	39.515508
2680.442037	552623.815668	39.520525
2683.330762	553615.329432	39.525543
2685.409893	554603.134463	39.530560
2688.031813	555596.809413	39.535578
2690.705747	556596.986434	39.540596
2693.172108	557622.602063	39.545613
2695.920338	558627.791761	39.550631
2698.727065	559662.340491	39.555648
2701.236449	560686.256697	39.560666
2703.948860	561720.761186	39.565684
2706.536149	562768.969556	39.570701
2709.572918	563809.787221	39.575719
2712.056848	564870.754220	39.580736
2714.844155	565914.911301	39.585754
2718.225164	566961.347515	39.590772
2720.539709	568009.030040	39.595789
2723.563298	569074.134587	39.600807
2725.781996	570155.751284	39.605824
2728.437441	571224.102236	39.610842
2731.450676	572299.935001	39.615860
2733.891179	573385.257850	39.620877
2736.831309	574465.537264	39.625895
2739.726413	575545.230000	39.630912
2742.667715	576624.672095	39.635930
2745.644508	577717.663425	39.640948
2748.714362	578799.104825	39.645965
2751.603387	579864.729696	39.650983
2754.600338	580950.962682	39.656000
2757.036734	582034.333706	39.661018
2759.889235	583114.581919	39.666036
2762.678947	584206.580869	39.671053
2765.273130	585287.683319	39.676071
2768.202068	586373.598772	39.681088
2771.115558	587469.597464	39.686106
2773.828635	588561.118468	39.691124
2776.341209	589661.546615	39.696141
2778.953872	590736.946701	39.701159
2781.838492	591857.662599	39.706176
2784.303302	592953.536472	39.711194
2786.986014	594061.099229	39.716212
2789.715351	595176.918271	39.721229
2792.449554	596292.581094	39.726247
2794.854585	597420.465648	39.731264
2797.614660	598548.734307	39.736282
2800.352146	599660.670373	39.741300
2803.075427	600811.865557	39.746317
2805.672143	601949.547401	39.751335
2808.652735	603093.663379	39.756352
2811.569703	604216.949365	39.761370
2815.334023	605324.567323	39.766388
2818.651859	606444.265106	39.771405
2821.919308	607540.087304	39.776423
2825.297378	608610.862849	39.781440
2828.238612	609663.494310	39.786458
2831.422607	610712.284976	39.791476
2834.285684	611752.275259	39.796493
2836.890047	612789.710462	39.801511
2839.648351	613839.229642	39.806528
2841.990004	614880.065641	39.811546
2844.882212	615937.968046	39.816564
2847.306523	616992.295992	39.821581
2849.774723	618071.667901	39.826599
2852.264990	619151.680374	39.831616
2854.975062	620224.301290	39.836634
2857.848030	621318.785268	39.841652
2860.415194	622416.758649	39.846669
2863.454147	623494.701863	39.851687
2866.594066	624586.213991	39.856704
2869.700211	625688.214708	39.861722
2872.647248	626774.939941	39.866740
2875.483544	627890.799020	39.871757
2878.546835	628991.518345	39.876775
2881.357249	630104.702638	39.881792
2884.064382	631219.834997	39.886810
2886.866884	632331.438504	39.891828
2889.617518	633465.053460	39.896845
2892.709574	634593.647152	39.901863
2895.309458	635722.849491	39.906880
2898.137547	636869.113255	39.911898
2901.330438	638007.354889	39.916916
2904.518694	639166.183058	39.921933
2907.368613	640292.652408	39.926951
2910.120790	641453.142279	39.931968
2912.767447	642617.808978	39.936986
2916.127795	643755.388971	39.942004
2918.655023	644925.000566	39.947021
2921.609722	646101.339485	39.952039
2925.068002	647234.076200	39.957056
2928.067212	648406.699433	39.962074
2931.130678	649572.943983	39.967092
2934.040622	650742.717426	39.972109
2936.580226	651920.240555	39.977127
2939.529947	653097.009064	39.982144
2941.848167	654279.373351	39.987162
2945.004881	655464.099271	39.992180
2947.967278	656672.030296	39.997197
2950.597543	657862.334061	40.002215
2953.915782	659070.609335	40.007232
2956.621953	660267.282712	40.012250
2960.015432	661468.725286	40.017268
2963.034299	662670.877773	40.022285
2965.961187	663867.022104	40.027303
2969.369149	665074.287909	40.032320
2972.318546	666276.252164	40.037338
2975.442152	667461.615417	40.042356
2978.371891	668672.040741	40.047373
2980.656088	669880.578068	40.052391
2984.075760	671099.718395	40.057408
2986.607650	672312.780150	40.062426
2989.471911	673527.720079	40.067444
2992.444130	674755.165277	40.072461
2995.375616	675966.497050	40.077479
2998.608562	677199.048106	40.082496
3001.306207	678428.989450	40.087514
3004.188572	679671.162247	40.092532
3007.133608	680908.586486	40.097549
3010.027988	682150.921125	40.102567
3013.134012	683388.383399	40.107584
3015.750901	684627.100466	40.112602
3019.004125	685849.850684	40.117620
3021.752803	687074.009738	40.122637
3024.849745	688265.076897	40.127655
3028.364762	689469.819245	40.132672
3031.536094	690658.473749	40.137690
3035.211551	691845.051808	40.142708
3038.682062	693025.104979	40.147725
3041.672540	694205.974713	40.152743
3045.121264	695367.759773	40.157760
3048.102841	696543.062099	40.162778
3051.131910	697724.648735	40.167796
3053.816484	698920.119369	40.172813
3056.623686	700104.796202	40.177831
3059.487816	701298.476114	40.182848
3061.789841	702505.173147	40.187866
3064.729626	703726.914175	40.192884
3067.179014	704973.938553	40.197901
3069.729612	706213.929000	40.202919
3073.202450	707463.250926	40.207936
3076.747107	708706.039273	40.212954
3080.431796	709938.174052	40.217972
3082.843670	711188.714363	40.222989
3085.561984	712449.766050	40.228007
3088.707073	713721.601041	40.233024
3091.450542	714994.202708	40.238042
3094.624678	716280.796120	40.243060
3098.021356	717564.682395	40.248077
3100.862295	718858.409307	40.253095
3104.067209	720162.957966	40.258112
3106.530196	721472.223087	40.263130
3109.423811	722768.996202	40.268148
3112.442002	724108.861776	40.273165
3115.661815	725433.151219	40.278183
3118.249324	726769.986574	40.283200
3121.473562	728127.059585	40.288218
3124.736236	729466.408844	40.293236
3128.522695	730838.109840	40.298253
3131.829077	732178.340498	40.303271
3135.920585	733514.565642	40.308288
3138.938660	734849.462988	40.313306
3142.612187	736183.685787	40.318324
3145.933773	737523.027211	40.323341
3148.783208	738859.162427	40.328359
3151.916556	740201.245354	40.333376
3154.826439	741553.401721	40.338394
3157.906703	742904.461039	40.343412
3160.648963	744272.361969	40.348429
3163.864013	745628.210801	40.353447
3166.409213	746995.769696	40.358464
3169.364138	748366.867682	40.363482
3172.633523	749747.826746	40.368500
3175.728574	751129.111665	40.373517
3179.119241	752514.930641	40.378535
3182.881771	753886.646510	40.383552
3186.042930	755270.383119	40.388570
3189.506590	756639.982909	40.393588
3192.872537	758010.781800	40.398605
3196.545474	759391.178769	40.403623
3200.558729	760737.849953	40.408640
3204.039668	762103.463247	40.413658
3207.422736	763452.167024	40.418676
3210.593045	764788.612559	40.423693
3213.687645	766132.308909	40.428711
3217.401570	767474.088771	40.433728
3220.538847	768815.378518	40.438746
3223.762058	770145.057359	40.443764
3227.336532	771491.986177	40.448781
3230.445445	772814.324465	40.453799
3233.729568	774119.299599	40.458816
3236.801148	775401.236660	40.463834
3239.875287	776674.059847	40.468852
3242.734459	777949.888895	40.473869
3245.608306	779238.159328	40.478887
3248.580567	780541.844388	40.483904
3251.072017	781850.233185	40.488922
3254.057033	783156.881034	40.493940
3256.980226	784458.298156	40.498957
3259.134207	785800.417637	40.503975
3262.470176	787133.214544	40.508992
3264.676866	788493.848969	40.514010
3267.835327	789870.685988	40.519028
3271.154341	791256.003328	40.524045
3274.396384	792657.919998	40.529063
3277.691894	794037.403918	40.534080
3280.839258	795450.245776	40.539098
3283.738133	796859.660801	40.544116
3287.213464	798289.507225	40.549133
3290.499745	799723.448689	40.554151
3294.462741	801140.928999	40.559168
3297.388869	802603.408212	40.564186
3300.410018	804054.847823	40.569204
3303.740463	805529.751810	40.574221
3306.509146	806999.932401	40.579239
3310.047549	808476.808804	40.584256
3312.931081	809975.861436	40.589274
3316.330918	811459.837179	40.594292
3319.732351	812961.028778	40.599309
3322.730551	814461.611325	40.604327
3326.268960	815974.126802	40.609344
3329.584218	817489.072605	40.614362
3333.061494	819009.262657	40.619380
3336.703377	820513.412512	40.624397
3340.000196	822027.184172	40.629415
3344.548973	823539.525715	40.634432
3349.014342	825018.174419	40.639450
3353.075659	826510.893409	40.644468
3356.778328	827984.416847	40.649485
3360.598360	829464.315135	40.654503
3363.886357	830918.041790	40.659520
3366.866404	832414.706525	40.664538
3370.237754	833895.911128	40.669556
3373.208760	835368.028393	40.674573
3376.476474	836862.933891	40.679591
3379.652963	838350.643656	40.684608
3382.814005	839837.523668	40.689626
3385.821754	841334.882780	40.694644
3389.384063	842836.418805	40.699661
3392.365562	844330.109267	40.704679
3395.910979	845836.091168	40.709696
3399.370675	847358.544127	40.714714
3402.650751	848876.284544	40.719732
3405.948554	850392.002576	40.724749
3408.779937	851920.445710	40.729767
3412.018041	853450.680149	40.734784
3415.333735	854974.796248	40.739802
3420.131605	856495.866059	40.744820
3424.721479	857986.221184	40.749837
3428.276871	859503.549968	40.754855
3432.084112	860972.741069	40.759872
3435.422168	862486.553015	40.764890
3439.231280	863960.066582	40.769908
3443.152172	865453.073153	40.774925
3446.336625	866935.174008	40.779943
3449.760180	868411.543475	40.784960
3453.437020	869884.603490	40.789978
3456.645301	871356.701203	40.794996
3460.464733	872802.939150	40.800000
3463.589391	874207.362448	40.805005
3466.886136	875551.282281	40.810010
3470.696475	876819.843799	40.815015
3473.847350	878022.305611	40.820020
3477.366987	879150.491518	40.825024
3480.309968	880210.899727	40.830029
3483.452937	881196.557728	40.835034
3486.121411	882101.703090	40.840039
3488.387012	882962.498950	40.845044
3491.069910	883738.046950	40.850048
3493.203955	884457.016677	40.855053
3495.106060	885105.333739	40.860058
3497.151359	885705.910620	40.865063
3498.729912	886248.985889	40.870068
3500.591092	886726.028746	40.875072
3502.147184	887183.235788	40.880077
3504.480411	887534.178187	40.885082
3505.452491	887873.900816	40.890087
3506.632745	888158.685277	40.895092
3508.577597	888400.547220	40.900096
3509.151005	888614.459123	40.905101
3510.236321	888773.207127	40.910106
3511.277888	888917.730620	40.915111
3512.082027	889015.156392	40.920116
3513.135175	889071.407210	40.925120
3513.661012	889123.679514	40.930125
3514.787565	889123.493938	40.935130
3515.262861	889120.318625	40.940135
3515.800397	889084.130495	40.945140
3516.667693	889014.497735	40.950144
3517.082822	888942.422221	40.955149
3517.699678	888846.696857	40.960154
3518.181086	888715.277499	40.965159
3518.502172	888595.302812	40.970164
3518.982172	888424.289763	40.975168
3519.061285	888264.082022	40.980173
3519.471235	888081.842079	40.985178
3519.826225	887895.830181	40.990183
3520.056762	887685.825124	40.995188
3520.318468	887463.803006	41.000192
3520.344785	887251.879675	41.005197
3520.651162	887011.728896	41.010202
3520.889188	886760.057765	41.015207
3520.877020	886521.681944	41.020212
3521.258895	886260.379794	41.025216
3521.424674	885991.354798	41.030221
3521.447917	885731.927793	41.035226
3521.235259	885446.864802	41.040231
3521.479134	885174.593344	41.045236
3521.609406	884870.366688	41.050240
3521.482924	884589.702725	41.055245
3521.733001	884283.585415	41.060250
3521.831040	883975.055400	41.065255
3521.611873	883685.838874	41.070260
3521.632357	883383.974548	41.075264
3521.537863	883073.103527	41.080269
3521.388996	882764.743996	41.085274
3521.543592	882462.131760	41.090279
3521.344177	882150.163143	41.095284
3521.625429	881839.842980	41.100288
3521.482334	881532.192787	41.105293
3521.221746	881201.092869	41.110298
3521.298847	880888.430064	41.115303
3521.283143	880582.065914	41.120308
3521.431366	880255.206858	41.125312
3521.161258	879943.423301	41.130317
3520.955132	879626.959599	41.135322
3521.094900	879290.742179	41.140327
3521.113960	878961.699757	41.145332
3520.909666	878650.612482	41.150336
3520.940885	878332.488860	41.155341
3520.868843	877998.365746	41.160346
3520.942660	877689.703115	41.165351
3520.771300	877364.578797	41.170356
3520.767230	877030.486728	41.175360
3520.307099	876709.641158	41.180365
3520.404105	876395.184906	41.185370
3520.369864	876085.292452	41.190375
3520.198345	875759.109997	41.195380
3520.342450	875437.513994	41.200384
3520.089523	875138.181916	41.205389
3519.678536	874814.606329	41.210394
3520.129018	874482.915311	41.215399
3519.722699	874179.000073	41.220404
3519.765083	873853.745064	41.225408
3519.654018	873546.158630	41.230413
3519.450601	873228.867148	41.235418
3519.545728	872922.476133	41.240423
3519.118925	872594.512306	41.245428
3519.355967	872284.668273	41.250432
3518.930497	871985.982605	41.255437
3519.265488	871671.819843	41.260442
3519.111514	871361.118718	41.265447
3519.258162	871065.010892	41.270452
3518.902290	870750.525242	41.275456
3518.709957	870452.307108	41.280461
3518.582989	870150.567994	41.285466
3518.374704	869846.205429	41.290471
3518.158441	869549.694134	41.295476
3518.462255	869245.605192	41.300480
3518.211977	868959.558078	41.305485
3518.145218	868661.133166	41.310490
3518.176694	868357.626890	41.315495
3517.862062	868051.734129	41.320500
3517.584667	867765.051933	41.325504
3517.724953	867477.607346	41.330509
3517.482701	867187.880670	41.335514
3517.408523	866901.026787	41.340519
3517.235702	866620.198874	41.345524
3517.058545	866329.643085	41.350528
3516.913246	866054.710839	41.355533
3517.196605	865780.958629	41.360538
3516.984628	865497.850260	41.365543
3516.553402	865214.764765	41.370548
3517.126410	864941.898658	41.375552
3516.664362	864668.024575	41.380557
3516.637308	864392.900235	41.385562
3516.637429	864110.178053	41.390567
3516.590980	863844.556774	41.395572
3516.680468	863569.861931	41.400576
3516.172628	863305.070664	41.405581
3515.834428	863021.867557	41.410586
3516.003203	862750.913799	41.415591
3515.679231	862497.333763	41.420596
3515.466249	862215.433555	41.425600
3515.580129	861981.690278	41.430605
3515.445465	861705.976016	41.435610
3515.509275	861451.608008	41.440615
3515.112105	861210.821333	41.445620
3515.212234	860940.868082	41.450624
3515.107709	860700.985528	41.455629
3514.952898	860441.457469	41.460634
3514.945715	860192.300218	41.465639
3514.390625	859962.285504	41.470644
3514.638134	859703.729729	41.475648
3514.502978	859456.800643	41.480653
3514.643381	859225.573798	41.485658
3514.463273	858967.543756	41.490663
3514.295710	858726.037870	41.495668
3514.326679	858482.641452	41.500672
3514.113646	858241.902261	41.505677
3513.854272	858019.548721	41.510682
3514.289731	857778.392703	41.515687
3513.931962	857545.725302	41.520692
3513.910459	857314.355905	41.525696
3514.062419	857100.171807	41.530701
3514.076443	856846.593983	41.535706
3513.705809	856619.732100	41.540711
3513.065635	856388.916402	41.545716
3513.641976	856167.039515	41.550720
3513.326338	855948.123877	41.555725
3513.407899	855724.560817	41.560730
3513.174453	855509.217075	41.565735
3512.857304	855283.465192	41.570740
3513.104154	855055.568140	41.575744
3512.772506	854840.703960	41.580749
3512.469093	854632.933590	41.585754
3512.782872	854419.019220	41.590759
3512.299705	854204.255249	41.595764
3512.354183	853997.280740	41.600768
3512.266005	853793.924938	41.605773
3512.132741	853600.208303	41.610778
3512.361106	853386.953901	41.615783
3511.939548	853181.198905	41.620788
3512.245146	852984.567212	41.625792
3512.018661	852779.545716	41.630797
3512.311959	852582.319103	41.635802
3512.237477	852371.903581	41.640807
3511.554878	852167.910807	41.645812
3511.835119	851975.146578	41.650816
3511.905752	851772.380136	41.655821
3511.590206	851561.489989	41.660826
3512.015638	851373.650100	41.665831
3511.653048	851179.603646	41.670836
3511.512187	850987.949592	41.675840
3511.322497	850790.745806	41.680845
3511.374552	850598.853223	41.685850
3511.194642	850402.804424	41.690855
3510.778485	850227.341995	41.695860
3511.063923	850032.568673	41.700864
3510.952852	849861.624151	41.705869
3510.844062	849681.030120	41.710874
3510.751267	849493.803566	41.715879
3510.722270	849315.523964	41.720884
3510.992878	849137.677074	41.725888
3510.802442	848952.691246	41.730893
3510.587125	848771.503939	41.735898
3510.747232	848589.957250	41.740903
3510.272248	848414.648542	41.745908
3510.145079	848246.585732	41.750912
3510.249736	848086.470619	41.755917
3510.110806	847909.825680	41.760922
3510.229770	847728.358285	41.765927
3510.297257	847567.846274	41.770932
3510.147262	847393.624930	41.775936
3510.039214	847223.972329	41.780941
3510.132650	847050.870875	41.785946
3509.929302	846893.602426	41.790951
3509.619021	846733.423719	41.795956
3509.597397	846567.442828	41.800960
3509.561659	846399.705430	41.805965
3509.575333	846236.634099	41.810970
3509.611353	846078.818505	41.815975
3508.936930	845920.823545	41.820980
3509.118756	845770.579433	41.825984
3509.088677	845616.759817	41.830989
3509.070073	845465.761604	41.835994
3509.012579	845317.300833	41.840999
3508.989578	845181.114466	41.846004
3509.157587	845033.877241	41.851008
3508.897752	844874.520397	41.856013
3508.701863	844726.166016	41.861018
3508.957444	844578.903766	41.866023
3508.807458	844434.337392	41.871028
3508.866402	844277.642995	41.876032
3508.922635	844142.006202	41.881037
3508.501356	843987.041282	41.886042
3508.678429	843844.650224	41.891047
3508.334441	843715.018260	41.896052
3508.474917	843570.384305	41.901056
3508.142378	843440.354778	41.906061
3508.275681	843306.588947	41.911066
3508.264043	843167.529349	41.916071
3507.992926	843038.310371	41.921076
3508.301379	842894.706072	41.926080
3508.153917	842769.459726	41.931085
3508.050148	842629.184428	41.936090
3508.125060	842494.582107	41.941095
3507.948957	842369.381347	41.946100
3508.150244	842232.021752	41.951104
3508.104965	842101.234718	41.956109
3507.970169	841978.311543	41.961114
3507.952349	841835.907503	41.966119
3508.113428	841715.466554	41.971124
3508.236303	841564.254478	41.976128
3507.983402	841443.291297	41.981133
3507.708488	841318.525070	41.986138
3507.839877	841194.177223	41.991143
3507.443909	841057.914921	41.996148
3507.853714	840922.736409	42.001152
3507.594027	840811.078739	42.006157
3507.568656	840678.161723	42.011162
3507.582270	840559.186560	42.016167
3507.238253	840433.194871	42.021172
3507.232939	840315.193888	42.026176
3507.300211	840194.446940	42.031181
3507.040117	840076.239589	42.036186
3507.250620	839967.611844	42.041191
3507.033861	839858.711129	42.046196
3507.293337	839730.313250	42.051200
3506.959335	839633.478176	42.056205
3507.020140	839512.426673	42.061210
3507.056742	839406.208628	42.066215
3506.703843	839285.855225	42.071220
3506.698453	839180.030654	42.076224
3506.877370	839070.368261	42.081229
3506.559225	838960.590691	42.086234
3507.043207	838852.191697	42.091239
3506.443696	838745.335554	42.096244
3506.481366	838634.566702	42.101248
3506.669358	838542.118207	42.106253
3506.398317	838425.833932	42.111258
3506.540429	838322.069108	42.116263
3506.403647	838220.739628	42.121268
3506.492604	838120.591324	42.126272
3506.413842	838032.717670	42.131277
3506.479054	837918.027960	42.136282
3506.372735	837821.713549	42.141287
3506.432696	837722.149405	42.146292
3506.824178	837612.768657	42.151296
3506.097204	837515.868647	42.156301
3506.525476	837406.478324	42.161306
3506.576350	837295.586549	42.166311
3506.094992	837215.381538	42.171316
3506.425033	837104.245255	42.176320
3506.147730	837017.659356	42.181325
3506.140875	836907.209643	42.186330
3506.378666	836804.819943	42.191335
3505.927292	836713.084911	42.196340
3505.977514	836619.801653	42.201344
3505.951161	836528.140403	42.206349
3505.693107	836429.340753	42.211354
3505.695963	836340.356635	42.216359
3505.599319	836251.875802	42.221364
3505.633872	836147.458980	42.226368
3505.709943	836069.442071	42.231373
3505.920489	835971.827373	42.236378
3505.889921	835886.552408	42.241383
3505.818209	835802.015331	42.246388
3505.638055	835704.802650	42.251392
3505.589840	835611.716258	42.256397
3505.287997	835526.139478	42.261402
3505.632600	835439.869258	42.266407
3505.459595	835366.376187	42.271412
3505.663961	835268.019553	42.276416
3505.589378	835190.114449	42.281421
3505.368902	835103.151668	42.286426
3505.347072	835012.786275	42.291431
3505.012652	834926.376919	42.296436
3505.358466	834853.915471	42.301440
3505.397885	834772.764214	42.306445
3505.314063	834679.523755	42.311450
3505.254396	834603.464441	42.316455
3504.778417	834525.226818	42.321460
3505.146460	834444.505563	42.326464
3504.848952	834370.289251	42.331469
3504.605175	834294.842548	42.336474
3504.576637	834213.011862	42.341479
3504.596677	834144.600019	42.346484
3505.041240	834081.244584	42.351488
3504.729533	834017.134163	42.356493
3504.374819	833934.425912	42.361498
3505.064507	833870.246754	42.366503
3504.721769	833804.918571	42.371508
3504.719446	833719.219652	42.376512
3504.697989	833664.140633	42.381517
3504.321547	833591.539837	42.386522
3504.714860	833520.764770	42.391527
3504.513669	833449.891517	42.396532
3504.358795	833375.982125	42.401536
3504.556504	833326.821930	42.406541
3504.368274	833267.274200	42.411546
3504.372963	833202.566398	42.416551
3504.231604	833132.949546	42.421556
3504.403993	833053.708253	42.426560
3504.545788	833003.871102	42.431565
3504.437994	832936.200095	42.436570
3504.720579	832861.431370	42.441575
3504.534772	832802.123154	42.446580
3504.559410	832725.441798	42.451584
3504.301479	832663.946426	42.456589
3504.427391	832600.042915	42.461594
3504.581590	832531.738447	42.466599
3504.205526	832481.054599	42.471604
3504.425600	832412.347294	42.476608
3504.371210	832351.108477	42.481613
3504.476382	832282.125667	42.486618
3504.534324	832218.864551	42.491623
3504.371576	832164.382168	42.496628
3504.395209	832089.549512	42.501632
3504.322492	832026.747641	42.506637
3504.317873	831960.172876	42.511642
3504.235967	831892.389018	42.516647
3504.166672	831850.148834	42.521652
3504.141118	831776.834898	42.526656
3504.242821	831711.803160	42.531661
3504.317991	831654.053405	42.536666
3504.225474	831591.592518	42.541671
3504.081608	831535.880551	42.546676
3504.252835	831475.670975	42.551680
3504.174237	831411.349810	42.556685
3504.275731	831355.107388	42.561690
3504.226282	831285.406714	42.566695
3503.931909	831226.981279	42.571700
3504.015175	831176.846638	42.576704
3503.946381	831118.529626	42.581709
3503.759520	831054.955536	42.586714
3503.986909	830990.482103	42.591719
3504.125994	830944.098106	42.596724
3503.817421	830875.901303	42.601728
3503.904368	830828.010616	42.606733
3503.807757	830786.745090	42.611738
3504.056496	830714.693051	42.616743
3503.675583	830663.214129	42.621748
3503.855621	830620.289770	42.626752
3503.759983	830561.581346	42.631757
3503.573838	830502.789586	42.636762
3503.689991	830454.647062	42.641767
3503.462029	830404.460021	42.646772
3503.629793	830355.037984	42.651776
3503.467026	830301.565982	42.656781
3503.384290	830250.034677	42.661786
3503.594385	830209.154692	42.666791
3503.409743	830163.404755	42.671796
3503.617810	830107.671445	42.676800
3503.184875	830062.987737	42.681805
3503.090008	830015.169879	42.686810
3503.267511	829973.805191	42.691815
3503.234521	829940.439136	42.696820
3503.443594	829894.915625	42.701824
3503.503226	829852.885537	42.706829
3503.221866	829813.207819	42.711834
3503.730076	829759.327683	42.716839
3503.137290	829715.987186	42.721844
3503.430304	829660.284923	42.726848
3503.631582	829623.311707	42.731853
3503.542168	829569.186399	42.736858
3503.750167	829524.637743	42.741863
3503.560571	829483.134957	42.746868
3503.695235	829415.094165	42.751872
3503.574812	829361.021102	42.756877
3503.392381	829321.372960	42.761882
3503.887563	829286.255157	42.766887
3503.252741	829235.881803	42.771892
3503.378323	829190.073936	42.776896
3503.420568	829155.811891	42.781901
3503.367528	829111.107946	42.786906
3503.556530	829059.815675	42.791911
3503.303664	829006.299023	42.796916
3503.320275	828967.202351	42.801921
3503.092420	828919.789308	42.806925
3503.315426	828876.944141	42.811930
3503.110280	828835.537532	42.816935
3503.080844	828797.766881	42.821940
3503.230178	828749.215359	42.826945
3503.282834	828705.370873	42.831949
3503.234551	828663.888470	42.836954
3503.597579	828629.864049	42.841959
3503.559953	828574.842306	42.846964
3503.363349	828531.575286	42.851969
3503.383755	828477.276226	42.856973
3503.320789	828429.685853	42.861978
3503.472818	828395.303995	42.866983
3503.286227	828345.338651	42.871988
3503.341281	828289.712778	42.876993
3503.171509	828264.131424	42.881997
3503.347422	828203.988616	42.887002
3503.343461	828172.270435	42.892007
3502.764305	828133.706769	42.897012
3503.168292	828089.116052	42.902017
3503.398916	828041.572246	42.907021
3503.403346	828012.784375	42.912026
3503.309382	827966.857479	42.917031
3503.013672	827932.302562	42.922036
3503.355131	827877.505767	42.927041
3503.340928	827829.365363	42.932045
3503.330631	827794.860461	42.937050
3503.465931	827736.284089	42.942055
3503.236118	827710.417198	42.947060
3503.414877	827665.518560	42.952065
3503.225837	827612.419877	42.957069
3503.201762	827572.392895	42.962074
3503.457054	827533.101706	42.967079
3503.531433	827491.542789	42.972084
3503.425866	827443.316839	42.977089
3503.245198	827403.607893	42.982093
3503.230760	827349.305216	42.987098
3503.365451	827308.272879	42.992103
3503.255799	827274.710321	42.997108
3503.312334	827231.832932	43.002113
3503.206704	827183.702843	43.007117
3503.443443	827151.988956	43.012122
3503.196494	827103.197217	43.017127
3502.946890	827057.778397	43.022132
3503.154424	827009.693212	43.027137
3503.387378	826984.040520	43.032141
3503.301197	826940.989207	43.037146
3503.121704	826885.487810	43.042151
3502.718080	826860.281667	43.047156
3503.067084	826817.842232	43.052161
3503.215159	826784.234713	43.057165
3502.860682	826759.851114	43.062170
3503.239955	826713.593066	43.067175
3502.537131	826672.401394	43.072180
3502.770213	826624.064754	43.077185
3502.822125	826597.316017	43.082189
3502.492303	826556.111061	43.087194
3502.929640	826528.125305	43.092199
3503.060602	826510.015961	43.097204
3503.061422	826462.254132	43.102209
3502.871465	826410.221358	43.107213
3502.757159	826380.125937	43.112218
3502.674488	826342.838766	43.117223
3502.432407	826317.310603	43.122228
3502.701632	826287.542684	43.127233
3502.755041	826267.001068	43.132237
3502.761928	826232.534004	43.137242
3502.640589	826185.719155	43.142247
3502.500361	826162.960247	43.147252
3502.687482	826135.698475	43.152257
3503.002939	826097.806561	43.157261
3502.765302	826059.027746	43.162266
3502.888617	826022.193719	43.167271
3502.996658	826009.806842	43.172276
3502.892261	825952.965171	43.177281
3502.610802	825924.850796	43.182285
3502.306658	825905.686980	43.187290
3502.635679	825862.560206	43.192295
3502.517890	825852.410311	43.197300
3502.764442	825815.603719	43.202305
3502.733608	825775.713565	43.207309
3502.615173	825754.807523	43.212314
3503.038347	825711.126444	43.217319
3502.674334	825674.468522	43.222324
3502.648867	825652.520108	43.227329
3502.458291	825610.552897	43.232333
3502.265080	825580.075667	43.237338
3502.749445	825546.015286	43.242343
3502.726646	825525.239440	43.247348
3502.339401	825490.540046	43.252353
3502.485628	825467.878227	43.257357
3502.367453	825437.779127	43.262362
3502.602045	825403.123528	43.267367
3502.625713	825384.295348	43.272372
3502.686612	825349.472500	43.277377
3502.617938	825317.702284	43.282381
3502.515716	825282.661476	43.287386
3502.793699	825260.808459	43.292391
3502.402247	825236.718657	43.297396
3502.643898	825187.783310	43.302401
3502.403326	825171.051662	43.307405
3502.555384	825145.747401	43.312410
3502.500048	825120.819476	43.317415
3502.196725	825091.287144	43.322420
3502.304834	825061.197947	43.327425
3502.691875	825032.822955	43.332429
3502.223281	825009.918552	43.337434
3502.380385	824976.642591	43.342439
3502.077922	824957.866909	43.347444
3502.258174	824917.545606	43.352449
3502.246047	824900.482256	43.357453
3502.127301	824888.521808	43.362458
3502.426088	824856.982232	43.367463
3501.940435	824833.199855	43.372468
3502.217578	824812.616849	43.377473
3502.347145	824788.146193	43.382477
3502.198909	824758.293431	43.387482
3502.216351	824737.166178	43.392487
3502.165363	824707.932857	43.397492
3502.144072	824689.110095	43.402497
3502.287288	824668.402000	43.407501
3502.389758	824658.262880	43.412506
3502.644445	824617.927486	43.417511
3502.279091	824599.601239	43.422516
3502.302108	824564.487082	43.427521
3502.370869	824543.497457	43.432525
3502.289367	824508.351316	43.437530
3502.815146	824477.701653	43.442535
3502.274397	824465.369837	43.447540
3502.417971	824435.320843	43.452545
3502.116255	824398.792252	43.457549
3502.478707	824379.318580	43.462554
3502.593196	824349.665201	43.467559
3502.222055	824332.610612	43.472564
3502.304350	824301.544160	43.477569
3502.230581	824273.584124	43.482573
3502.327362	824259.679837	43.487578
3502.554588	824230.643088	43.492583
3502.421121	824204.159674	43.497588
3502.536997	824176.314699	43.502593
3502.613204	824149.258594	43.507597
3502.553654	824127.457423	43.512602
3502.624064	824097.125519	43.517607
3502.253839	824073.468093	43.522612
3502.400653	824036.227863	43.527617
3502.464790	824015.726364	43.532621
3502.612515	823991.445382	43.537626
3502.433905	823965.897635	43.542631
3502.408853	823936.803338	43.547636
3502.307334	823908.846327	43.552641
3502.460699	823871.457373	43.557645
3502.287550	823858.819340	43.562650
3502.514672	823818.532510	43.567655
3502.478948	823795.503671	43.572660
3502.308556	823769.562561	43.577665
3502.681166	823737.956577	43.582669
3502.092850	823709.051865	43.587674
3502.399858	823671.245219	43.592679
3502.191264	823671.572992	43.597684
3502.230624	823634.837268	43.602689
3502.297843	823632.478624	43.607693
3501.766205	823598.526644	43.612698
3502.115526	823570.591757	43.617703
3502.321308	823568.503713	43.622708
3502.150563	823540.165281	43.627713
3502.380801	823513.081200	43.632717
3502.250571	823500.924493	43.637722
3502.289421	823477.344271	43.642727
3502.284635	823450.787731	43.647732
3502.026233	823434.348056	43.652737
3502.388280	823407.339649	43.657741
3502.182800	823386.978427	43.662746
3502.551852	823350.333545	43.667751
3502.162311	823332.154480	43.672756
3502.272131	823311.203086	43.677761
3502.495732	823287.983035	43.682765
3502.308293	823263.754587	43.687770
3502.209796	823242.299278	43.692775
3501.949892	823219.990100	43.697780
3502.110582	823187.144724	43.702785
3502.498776	823163.212379	43.707789
3501.933542	823148.876780	43.712794
3502.154874	823124.531582	43.717799
3502.110510	823114.267547	43.722804
3502.329354	823069.575522	43.727809
3502.485726	823052.724198	43.732813
3502.178676	823032.427523	43.737818
3502.511693	823003.123403	43.742823
3502.406367	822980.934691	43.747828
3502.320126	822950.036382	43.752833
3502.029973	822935.752834	43.757837
3502.126315	822919.253446	43.762842
3502.134227	822878.018745	43.767847
3502.304376	822868.648340	43.772852
3502.231224	822842.687572	43.777857
3502.347889	822813.320422	43.782861
3502.139162	822796.577496	43.787866
3502.372983	822772.864822	43.792871
3502.348211	822751.493604	43.797876
3502.251579	822723.628600	43.802881
3502.530790	822702.843037	43.807885
3501.804313	822679.581686	43.812890
3502.478741	822658.681973	43.817895
3502.027320	822643.005836	43.822900
3502.075582	822627.981077	43.827905
3502.038862	822601.573131	43.832909
3502.075206	822584.397982	43.837914
3502.437319	822554.353361	43.842919
3502.171101	822537.374672	43.847924
3502.067001	822518.216956	43.852929
3502.198989	822475.736426	43.857933
3501.994909	822459.774533	43.862938
3502.120038	822435.833978	43.867943
3502.113130	822422.921233	43.872948
3502.009814	822410.073258	43.877953
3502.492900	822361.321796	43.882957
3502.100084	822361.141888	43.887962
3501.899477	822324.927583	43.892967
3502.087433	822327.684861	43.897972
3502.027980	822291.398205	43.902977
3501.837370	822268.389560	43.907981
3501.875958	822262.806601	43.912986
3502.140434	822240.554496	43.917991
3501.960342	822221.163850	43.922996
3502.313382	822207.800056	43.928001
3501.676199	822176.352950	43.933005
3501.840013	822164.194268	43.938010
3502.029560	822144.008740	43.943015
3501.774939	822125.755209	43.948020
3501.711547	822096.414539	43.953025
3501.848163	822098.740102	43.958029
3501.847448	822094.044010	43.963034
3502.209807	822066.883338	43.968039
3502.186529	822052.700679	43.973044
3501.852910	822020.517966	43.978049
3502.354042	822004.389899	43.983053
3502.007594	821987.080576	43.988058
3502.272409	821953.233547	43.993063
3502.194366	821950.653634	43.998068
3502.004643	821918.153204	44.003073
3502.078216	821901.606113	44.008077
3501.511158	821886.778865	44.013082
3501.923382	821862.935715	44.018087
3501.924918	821851.243472	44.023092
3502.080814	821843.586182	44.028097
3502.154362	821809.476401	44.033101
3501.863432	821807.127180	44.038106
3502.187773	821793.571599	44.043111
3501.959942	821761.125597	44.048116
3502.341691	821746.630965	44.053121
3502.197057	821718.818561	44.058125
3502.042787	821711.799264	44.063130
3502.125796	821686.493143	44.068135
3501.736535	821657.791265	44.073140
3502.015147	821631.718889	44.078145
3501.991787	821631.673788	44.083149
3501.923557	821600.864062	44.088154
3502.259458	821595.867561	44.093159
3502.015437	821567.092445	44.098164
3501.898652	821562.268327	44.103169
3502.096969	821534.985734	44.108173
3501.773757	821517.671354	44.113178
3501.895404	821512.367621	44.118183
3502.064771	821498.641275	44.123188
3501.841498	821473.629405	44.128193
3502.203427	821449.401672	44.133197
3501.798927	821436.943880	44.138202
3502.088219	821414.244610	44.143207
3501.944172	821398.906277	44.148212
3501.880987	821389.131906	44.153217
3501.882495	821348.475829	44.158221
3501.804742	821347.412280	44.163226
3502.047429	821320.366118	44.168231
3501.950510	821295.870933	44.173236
3502.092910	821283.567394	44.178241
3502.023960	821272.423912	44.183245
3502.315981	821257.649448	44.188250
3502.211501	821231.247204	44.193255
3502.224882	821214.316915	44.198260
3502.046991	821189.638974	44.203265
3502.221669	821157.759750	44.208269
3501.943183	821138.186437	44.213274
3501.929806	821116.172036	44.218279
3502.151082	821102.338471	44.223284
3501.987419	821081.522930	44.228289
3502.128721	821052.633189	44.233293
3501.887662	821040.881624	44.238298
3502.128814	821029.197392	44.243303
3502.051296	821011.156249	44.248308
3501.936992	821014.306351	44.253313
3501.793257	820979.592051	44.258317
3501.536300	820970.093612	44.263322
3502.169432	820952.767016	44.268327
3502.062634	820939.329638	44.273332
3501.747445	820905.621734	44.278337
3501.805406	820898.713399	44.283341
3501.725674	820898.041522	44.288346
3502.087268	820859.329165	44.293351
3501.955982	820856.268317	44.298356
3501.743100	820855.275873	44.303361
3502.102338	820815.242599	44.308365
3501.782657	820796.164343	44.313370
3501.558243	820797.326628	44.318375
3502.050245	820775.472497	44.323380
3501.622059	820751.323436	44.328385
3501.798069	820743.172283	44.333389
3501.815141	820746.398729	44.338394
3501.932680	820701.364940	44.343399
3501.930801	820701.365224	44.348404
3501.720586	820682.317538	44.353409
3502.174890	820658.267427	44.358413
3501.754403	820636.465280	44.363418
3502.207794	820629.442605	44.368423
3502.021768	820611.222530	44.373428
3502.109943	820587.868555	44.378433
3502.431644	820565.601420	44.383437
3501.808736	820545.447000	44.388442
3502.041945	820525.591878	44.393447
3501.891256	820502.717318	44.398452
3501.971097	820493.945607	44.403457
3501.967064	820479.609626	44.408461
3501.907870	820453.686136	44.413466
3501.963147	820438.459544	44.418471
3501.914937	820426.528333	44.423476
3501.932202	820393.937413	44.428481
3501.961634	820393.100710	44.433485
3501.831105	820367.384358	44.438490
3502.006569	820338.877340	44.443495
3501.881436	820337.576774	44.448500
3501.700075	820309.030539	44.453505
3501.920676	820292.308429	44.458509
3501.614915	820290.597218	44.463514
3501.766047	820264.736212	44.468519
3501.695217	820252.857347	44.473524
3501.764970	820241.444628	44.478529
3501.747480	820229.899462	44.483533
3501.546303	820225.186134	44.488538
3501.688588	820190.567398	44.493543
3501.970749	820187.144545	44.498548
3501.641087	820186.122300	44.503553
3501.838630	820180.217815	44.508557
3501.836241	820152.962614	44.513562
3502.127228	820138.773036	44.518567
3502.059400	820127.235983	44.523572
3502.050526	820097.094569	44.528577
3502.095168	820079.079708	44.533581
3501.767128	820064.845134	44.538586
3501.851046	820038.162449	44.543591
3501.885812	820039.673642	44.548596
3501.572646	820029.302306	44.553601
3502.033305	819992.036606	44.558605
3501.977291	819989.648036	44.563610
3502.251006	819973.601456	44.568615
3501.648915	819951.239758	44.573620
3501.763350	819938.938342	44.578625
3502.187705	819922.132810	44.583629
3502.010101	819891.479976	44.588634
3502.022662	819882.963217	44.593639
3502.093268	819866.020070	44.598644
3501.896615	819836.202014	44.603649
3502.053246	819823.844500	44.608653
3501.796855	819807.297612	44.613658
3502.129422	819783.558014	44.618663
3501.802262	819788.847983	44.623668
3501.758396	819748.825762	44.628673
3501.995516	819736.405894	44.633677
3501.548451	819735.647593	44.638682
3501.793414	819720.143436	44.643687
3501.997647	819699.214032	44.648692
3501.867144	819701.486567	44.653697
3501.623520	819671.137209	44.658701
3501.307309	819647.455052	44.663706
3501.872224	819647.117295	44.668711
3501.600495	819630.670366	44.673716
3501.239760	819630.778694	44.678721
3501.663526	819623.661975	44.683725
3501.218950	819602.839134	44.688730
3501.504453	819586.202439	44.693735
3501.286071	819576.597775	44.698740
3501.735435	819572.413012	44.703745
3501.653834	819567.728458	44.708749
3501.567494	819573.810863	44.713754
3501.696865	819535.618438	44.718759
3501.590836	819533.727316	44.723764
3501.781510	819522.587074	44.728769
3502.005799	819523.088418	44.733773
3501.635369	819495.842210	44.738778
3501.878170	819480.680418	44.743783
3502.122925	819470.705689	44.748788
3501.634049	819458.992140	44.753793
3501.534042	819426.464739	44.758797
3501.274747	819427.681939	44.763802
3501.556857	819419.120190	44.768807
3501.474113	819418.448656	44.773812
3501.699224	819412.490015	44.778817
3501.654959	819391.649516	44.783821
3501.433547	819376.857579	44.788826
3501.645378	819366.251916	44.793831
3501.679544	819378.774552	44.798836
3501.871426	819348.205174	44.803841
3501.905916	819328.623914	44.808845
3501.820120	819339.747153	44.813850
3502.213491	819317.415110	44.818855
3501.876901	819289.085824	44.823860
3501.731095	819287.494818	44.828865
3501.891800	819249.736050	44.833869
3501.985961	819236.213190	44.838874
3502.048138	819216.724920	44.843879
3501.845592	819202.027368	44.848884
3501.602846	819194.139059	44.853889
3501.841712	819176.138707	44.858893
3501.560252	819172.808174	44.863898
3501.890029	819140.257527	44.868903
3501.515954	819127.986139	44.873908
3501.476258	819124.664701	44.878913
3501.764627	819117.373987	44.883917
3501.648272	819100.166046	44.888922
3502.091956	819083.404165	44.893927
3501.587254	819078.397429	44.898932
3501.670412	819063.946157	44.903937
3502.176142	819040.517983	44.908941
3501.858267	819028.481861	44.913946
3501.497640	819028.100764	44.918951
3501.686740	818993.272336	44.923956
3501.671521	818980.892627	44.928961
3501.913838	818979.824917	44.933965
3501.740833	818974.469818	44.938970
3501.885901	818935.635135	44.943975
3501.797766	818938.243542	44.948980
3501.605251	818930.836065	44.953985
3501.942996	818916.195715	44.958989
3501.753798	818889.749189	44.963994
3501.665154	818869.012250	44.968999
3501.651456	818865.735343	44.974004
3501.466817	818841.832878	44.979009
3501.961659	818821.538052	44.984013
3501.447403	818820.252335	44.989018
3501.752411	818813.496919	44.994023
3501.922586	818799.520170	44.999028
3501.423507	818784.038509	45.004033
3501.843988	818769.188438	45.009037
3501.797177	818774.041483	45.014042
3501.895745	818751.560337	45.019047
3501.781496	818737.679250	45.024052
3501.486108	818732.637773	45.029057
3501.675701	818714.986899	45.034061
3501.452579	818688.447275	45.039066
3501.871584	818690.825416	45.044071
3501.825211	818684.910846	45.049076
3501.575546	818681.966378	45.054081
3501.735850	818663.390261	45.059085
3501.627653	818641.970623	45.064090
3501.525037	818636.212106	45.069095
3501.974556	818625.272455	45.074100
3501.692836	818610.929247	45.079105
3502.018401	818588.018608	45.084109
3502.094353	818587.418739	45.089114
3501.667718	818557.339173	45.094119
3501.610998	818537.770617	45.099124
3501.910058	818530.575394	45.104129
3502.178029	818516.386166	45.109133
3501.909091	818509.724981	45.114138
3502.182415	818485.794753	45.119143
3501.906218	818465.038506	45.124148
3501.682417	818440.504764	45.129153
3501.791712	818427.516174	45.134157
3501.745849	818429.628361	45.139162
3501.392808	818400.808551	45.144167
3501.665541	818401.889355	45.149172
3501.543719	818403.720387	45.154177
3501.885675	818382.372608	45.159181
3502.010899	818370.017579	45.164186
3501.849357	818329.369927	45.169191
3502.214925	818320.156727	45.174196
3501.765912	818309.315614	45.179201
3501.720789	818288.471810	45.184205
3501.715986	818285.731566	45.189210
3501.937838	818267.437891	45.194215
3501.880922	818251.099011	45.199220
3501.505323	818238.532551	45.204225
3501.724350	818226.798118	45.209229
3501.564801	818209.203417	45.214234
3501.511348	818181.752782	45.219239
3501.503355	818186.453017	45.224244
3501.479838	818182.736867	45.229249
3502.057663	818175.544296	45.234253
3501.958429	818164.009017	45.239258
3501.750562	818136.192049	45.244263
3501.967730	818136.400991	45.249268
3502.125009	818109.698514	45.254273
3502.204293	818086.777778	45.259277
3501.889782	818067.690838	45.264282
3502.100237	818044.503611	45.269287
3502.251395	818044.674481	45.274292
3501.653576	818017.802319	45.279297
3501.917531	817994.704005	45.284301
3501.690500	817989.405960	45.289306
3502.032139	817961.693550	45.294311
3502.011181	817958.662139	45.299316
3501.794836	817933.586866	45.304321
3501.798093	817914.398198	45.309325
3501.791110	817895.406960	45.314330
3502.015140	817882.936860	45.319335
3501.996861	817866.394877	45.324340
3501.597824	817855.446892	45.329345
3502.077247	817841.564056	45.334349
3501.935338	817837.328765	45.339354
3502.071873	817819.243719	45.344359
3501.800514	817816.253488	45.349364
3501.674520	817778.778381	45.354369
3501.983321	817763.993432	45.359373
3501.774863	817748.804144	45.364378
3502.024355	817734.910010	45.369383
3501.400835	817716.019813	45.374388
3501.793331	817697.941230	45.379393
3502.295698	817695.900422	45.384397
3501.783576	817678.998759	45.389402
3501.893695	817660.526027	45.394407
3501.931143	817644.610682	45.399412
3501.542019	817625.485815	45.404417
3502.109503	817599.741718	45.409421
3502.050844	817585.065852	45.414426
3502.073875	817561.663066	45.419431
3501.964247	817555.121539	45.424436
3501.804308	817554.413578	45.429441
3501.783064	817523.136681	45.434445
3501.720163	817513.258667	45.439450
3501.557048	817492.921340	45.444455
3501.853196	817494.047392	45.449460
3501.622242	817473.182702	45.454465
3501.581540	817454.440529	45.459469
3501.451337	817446.482657	45.464474
3501.563377	817444.652925	45.469479
3501.641650	817434.017250	45.474484
3501.957471	817423.587196	45.479489
3501.686102	817408.554355	45.484493
3502.133169	817408.823363	45.489498
3501.722294	817381.917846	45.494503
3502.358168	817352.930626	45.499508
3502.067787	817343.236691	45.504513
3502.320035	817314.410399	45.509517
3502.144982	817304.012059	45.514522
3502.200599	817275.560664	45.519527
3501.896737	817257.938274	45.524532
3501.896374	817247.168393	45.529537
3502.234956	817223.761405	45.534541
3502.066734	817212.137937	45.539546
3501.808757	817184.961671	45.544551
3502.024067	817158.001068	45.549556
3501.750118	817153.395452	45.554561
3502.245208	817145.432138	45.559565
3502.082519	817117.603489	45.564570
3502.043758	817093.964471	45.569575
3501.935739	817081.400709	45.574580
3501.887720	817065.595976	45.579585
3501.776203	817055.725295	45.584589
3501.502008	817038.782818	45.589594
3501.837855	817018.214996	45.594599
3501.832902	817015.376344	45.599604
3501.673085	817011.877817	45.604609
3501.834282	816973.371778	45.609613
3501.839811	816976.161344	45.614618
3501.775415	816955.512385	45.619623
3501.723760	816940.980822	45.624628
3501.792985	816922.219053	45.629633
3501.842335	816912.713316	45.634637
3501.984424	816892.079109	45.639642
3501.673580	816867.113315	45.644647
3501.851843	816866.300615	45.649652
3501.444714	816861.422991	45.654657
3501.648975	816849.247970	45.659661
3501.640898	816828.981001	45.664666
3501.321944	816815.325466	45.669671
3501.447468	816817.507845	45.674676
3501.519043	816816.370011	45.679681
3501.815586	816808.096301	45.684685
3501.691345	816787.848343	45.689690
3501.406168	816759.842552	45.694695
3501.689408	816772.378005	45.699700
3501.482199	816768.985071	45.704705
3501.615533	816748.253948	45.709709
3501.288493	816721.429879	45.714714
3501.644451	816714.712926	45.719719
3501.557550	816709.586612	45.724724
3501.792708	816702.742670	45.729729
3502.063872	816679.149056	45.734733
3501.921851	816669.870330	45.739738
3501.906502	816661.598855	45.744743
3501.767739	816642.821604	45.749748
3501.435765	816624.125083	45.754753
3501.595226	816602.263154	45.759757
3501.612428	816624.193850	45.764762
3501.346098	816605.437506	45.769767
3501.541517	816572.113167	45.774772
3501.593437	816562.949225	45.779777
3501.477489	816542.846038	45.784781
3501.411745	816549.662186	45.789786
3501.752707	816534.379642	45.794791
3501.728096	816527.431430	45.799796
3501.484511	816513.322228	45.804801
3501.507890	816477.332979	45.809805
3501.344017	816411.214901	45.814810
3501.368881	816290.522546	45.819815
3501.502411	816120.554105	45.824820
3501.318255	815890.603970	45.829825
3501.433838	815583.572983	45.834829
3501.219870	815236.819655	45.839834
3501.094595	814827.056341	45.844839
3500.658253	814339.791729	45.849844
3500.225181	813821.830459	45.854849
3500.033148	813251.524745	45.859853
3500.079141	812612.255006	45.864858
3499.891897	811903.687455	45.869863
3499.451751	811146.334090	45.874868
3498.710122	810334.453186	45.879873
3498.770468	809453.630500	45.884877
3498.413835	808512.079191	45.889882
3497.887954	807515.910652	45.894887
3497.617075	806446.889506	45.899892
3496.778247	805315.661298	45.904897
3496.187995	804139.081154	45.909901
3495.498502	802891.281284	45.914906
3495.064151	801583.450706	45.919911
3494.422150	800214.356382	45.924916
3493.594859	798790.536807	45.929921
3493.127093	797293.212699	45.934925
3492.298303	795751.626797	45.939930
3491.694815	794126.457369	45.944935
3491.302302	792453.908995	45.949940
3489.984813	790710.302313	45.954945
3489.425800	788913.545888	45.959949
3488.334505	787050.833614	45.964954
3487.754041	785127.944242	45.969959
3487.054258	783150.445386	45.974964
3485.621563	781108.307816	45.979969
3484.879116	778987.314862	45.984973
3483.724399	776834.456804	45.989978
3482.726166	774615.285923	45.994983
3481.632371	772331.610045	45.999988
3480.285352	769990.988717	46.004993
3479.602962	767596.425371	46.009997
3478.265202	765138.769353	46.015002
3477.125447	762626.505117	46.020007
3476.172044	760056.426782	46.025012
3474.827142	757421.961194	46.030017
3473.976830	754727.889129	46.035021
3472.275679	751989.739324	46.040026
3470.843123	749187.766642	46.045031
3469.788462	746320.704587	46.050036
3468.154571	743411.841072	46.055041
3467.130870	740432.049153	46.060045
3465.623026	737397.374043	46.065050
3464.137200	734333.176658	46.070055
3462.602550	731188.972867	46.075060
3460.876504	727994.135188	46.080065
3459.672200	724747.009753	46.085069
3458.146066	721452.742391	46.090074
3456.307078	718095.808560	46.095079
3455.166983	714678.558422	46.100084
3453.174555	711220.648953	46.105089
3451.973578	707699.768808	46.110093
3449.990330	704131.964191	46.115098
3448.116980	700504.616171	46.120103
3446.386085	696839.392151	46.125108
3444.855560	693110.080795	46.130113
3443.068332	689316.991100	46.135117
3441.507286	685499.515381	46.140122
3439.538406	681625.663275	46.145127
3437.801008	677669.410312	46.150132
3435.714031	673680.423012	46.155137
3433.812159	669633.551068	46.160141
3431.728468	665542.722267	46.165146
3429.945299	661414.011007	46.170151
3427.997953	657228.787425	46.175156
3425.891062	652980.704048	46.180161
3423.638991	648694.092658	46.185165
3421.373668	644370.454971	46.190170
3419.297821	639985.069655	46.195175
3417.630234	635551.208931	46.200180
3415.218281	631082.594773	46.205185
3412.770448	626553.644795	46.210189
3410.540191	621976.043311	46.215194
3408.460197	617384.208941	46.220199
3406.522505	612719.220255	46.225204
3404.278132	608000.706488	46.230209
3402.002296	603257.497863	46.235213
3399.497947	598458.591354	46.240218
3397.028717	593611.440841	46.245223
3394.914790	588731.998132	46.250228
3392.191213	583799.096452	46.255233
3390.044716	578817.638647	46.260237
3387.767052	573822.789321	46.265242
3385.215717	568746.531291	46.270247
3382.842125	563632.944144	46.275252
3379.955491	558496.894885	46.280257
3377.499083	553304.471797	46.285261
3374.871288	548074.249776	46.290266
3372.807560	542802.824482	46.295271
3369.916685	537500.761116	46.300276
3367.047080	532164.997889	46.305281
3364.464275	526761.362015	46.310285
3361.693929	521338.944543	46.315290
3358.934175	515875.250038	46.320295
3356.111947	510376.557454	46.325300
3353.646298	504837.445387	46.330305
3350.607775	499260.953129	46.335309
3347.967280	493648.243726	46.340314
3344.893819	488003.057785	46.345319
3341.873418	482320.773765	46.350324
3338.970300	476626.867124	46.355329
3336.081416	470873.518653	46.360333
3333.058606	465101.945741	46.365338
3330.095872	459305.407824	46.370343
3327.250304	453468.459092	46.375348
3323.804950	447614.919090	46.380353
3320.961086	441702.621942	46.385357
3317.841634	435786.470275	46.390362
3314.630233	429834.100246	46.395367
3311.612490	423856.964448	46.400372
3308.184725	417848.063148	46.405377
3305.471630	411812.474606	46.410381
3302.008497	405750.680245	46.415386
3298.602465	399656.284270	46.420391
3295.724977	393554.250974	46.425396
3292.100422	387421.991962	46.430401
3288.855294	381269.555661	46.435405
3285.515537	375091.879630	46.440410
3282.580871	368890.503255	46.445415
3279.032807	362653.534062	46.450420
3275.445895	356413.965996	46.455425
3272.180766	350137.781078	46.460429
3268.852971	343850.534465	46.465434
3265.229072	337547.307859	46.470439
3261.863892	331226.767439	46.475444
3258.352148	324896.061782	46.480449
3254.808254	318537.843558	46.485453
3251.088539	312160.058737	46.490458
3247.386271	305785.573289	46.495463
3243.624213	299380.164840	46.500468
3239.844028	292976.403460	46.505473
3236.535540	286566.862353	46.510477
3232.754275	280142.159703	46.515482
3229.007799	273698.225698	46.520487
3225.216727	267265.189712	46.525492
3221.298788	260804.648334	46.530497
3217.835079	254345.503062	46.535501
3214.009913	247892.716634	46.540506
3209.873681	241412.067314	46.545511
3206.129993	234933.659850	46.550516
3201.874336	228461.783964	46.555521
3198.138581	221981.005879	46.560525
3194.016496	215500.098263	46.565530
3189.782032	208937.712126	46.570535
3185.865248	202454.198370	46.575540
3182.020125	195979.361389	46.580545
3178.006827	189501.087487	46.585549
3173.608261	183028.705855	46.590554
3169.207139	176559.329856	46.595559
3165.356682	170105.935184	46.600564
3160.858745	163663.474809	46.605569
3156.952370	157226.578778	46.610573
3152.095023	150798.005891	46.615578
3147.780258	144382.313680	46.620583
3143.530444	137980.923198	46.625588
3138.849427	131593.757245	46.630593
3134.464877	125223.890654	46.635597
3129.583868	118868.865519	46.640602
3125.080166	112548.010866	46.645607
3120.584928	106235.207869	46.650612
3115.137645	99955.013126	46.655617
3110.391663	93694.216253	46.660621
3105.179844	87482.219068	46.665626
3099.935660	81288.638353	46.670631
3094.235459	75144.194030	46.675636
3088.391440	69064.002001	46.680641
3082.617522	63021.009915	46.685645
3075.995453	57048.650927	46.690650
3066.436770	51207.006310	46.695655
3048.882349	45686.290273	46.700660
3030.520918	40359.607938	46.705665
3013.335568	35253.070890	46.710669
2996.558859	30434.188296	46.715674
2980.501251	25895.342182	46.720679
2965.113083	21639.086250	46.725684
2950.064879	17693.505064	46.730689
2935.885131	14058.882873	46.735693
2919.453786	10757.662860	46.740698
2900.854402	7848.672105	46.745703
2881.231060	5324.182200	46.750708
2861.737343	3168.298997	46.755713
2842.804643	1385.042455	46.760717
2812.283368	315.737351	46.765722
2760.588170	301.159917	46.770727
2734.827974	300.594122	46.775732
2732.661813	298.830735	46.780737
2744.722535	288.057479	46.785741
2761.173566	279.597576	46.790746
2774.643064	278.212194	46.795751
2783.178258	272.097126	46.800756
2785.209413	288.023876	46.805761
2783.374797	284.912293	46.810765
2780.414883	274.965924	46.815770
2776.381860	269.845697	46.820775
2772.596599	273.535453	46.825780
2768.907932	279.271760	46.830785
2766.220023	268.151896	46.835789
2763.600209	275.487168	46.840794
2761.094450	269.191119	46.845799
2758.435001	262.953659	46.850804
2755.838517	273.711028	46.855809
2753.270146	261.999342	46.860813
2750.403815	266.776571	46.865818
2746.994850	267.233390	46.870823
2744.131545	249.848698	46.875828
2740.685392	261.826954	46.880833
2737.351447	260.889589	46.885837
2733.967121	255.935434	46.890842
2730.753326	270.347396	46.895847
2727.844123	254.419283	46.900852
2724.580243	258.047072	46.905857
2721.629332	251.809539	46.910861
2717.906741	254.304482	46.915866
2714.554657	247.235000	46.920871
2711.668011	238.619360	46.925876
2708.385301	249.519063	46.930881
2704.864874	246.860174	46.935885
2701.850139	249.682780	46.940890
2698.309841	255.228406	46.945895
2695.221924	243.925132	46.950900
2691.750179	246.767642	46.955905
2687.915107	249.309457	46.960909
2684.826244	243.259153	46.965914
2681.212736	250.674802	46.970919
2677.914901	249.337367	46.975924
2674.706531	247.112445	46.980929
2671.458841	245.167688	46.985933
2668.366268	245.435735	46.990938
2664.805125	244.531915	46.995943
2661.351349	238.718981	47.000948
2657.580509	242.279824	47.005953
2653.661067	229.122250	47.010957
2650.738134	244.193538	47.015962
2647.332729	241.035836	47.020967
2644.110201	228.340815	47.025972
2640.460178	236.542392	47.030977
2637.855522	227.899043	47.035981
2634.084832	228.270623	47.040986
2629.995483	238.135022	47.045991
2627.015877	237.319534	47.050996
2623.527606	239.216288	47.056001
2619.882802	246.752057	47.061005
2616.246357	237.846312	47.066010
2612.868342	243.234488	47.071015
2610.107639	232.591804	47.076020
2605.979173	227.268207	47.081025
2602.842096	223.665535	47.086029
2599.436927	233.404507	47.091034
2596.175857	233.702041	47.096039
2592.557717	223.157043	47.101044
2588.517089	223.248171	47.106049
2585.267978	232.280768	47.111053
2582.200235	231.254986	47.116058
2578.836836	228.287711	47.121063
2575.451384	225.107519	47.126068
2571.789777	230.173975	47.131073
2568.077164	232.626197	47.136077
2564.655156	221.580444	47.141082
2561.276103	228.663172	47.146087
2557.762376	224.586809	47.151092
2553.865887	225.841546	47.156097
2550.715040	228.467821	47.161101
2547.697977	226.339078	47.166106
2543.842647	218.141049	47.171111
2540.918231	217.890493	47.176116
2536.971613	215.115304	47.181121
2533.389990	211.415782	47.186125
2529.630551	211.567521	47.191130
2526.316248	217.379511	47.196135
2523.378289	205.408078	47.201140
2519.801392	220.569942	47.206145
2515.952034	206.384637	47.211149
2513.048952	215.617195	47.216154
2508.747460	222.767099	47.221159
2506.044235	211.969578	47.226164
2501.906805	225.913003	47.231169
2498.865329	216.473159	47.236173
2495.223451	224.442582	47.241178
2491.678060	219.358645	47.246183
2488.453334	216.027288	47.251188
2484.932488	219.734630	47.256193
2481.610498	216.339006	47.261197
2478.286330	206.352856	47.266202
2474.323847	223.615224	47.271207
2471.255351	208.687427	47.276212
2467.651258	210.936121	47.281217
2463.694443	204.154749	47.286221
2460.538907	205.859272	47.291226
2456.525609	209.437193	47.296231
2453.375346	207.297408	47.301236
2450.204366	222.284918	47.306241
2446.419246	212.671755	47.311245
2443.263435	213.319697	47.316250
2439.141284	212.515307	47.321255
2435.775430	216.511042	47.326260
2432.675206	221.459230	47.331265
2429.143507	212.596023	47.336269
2425.667479	208.335534	47.341274
2421.910763	214.658562	47.346279
2418.702941	206.260604	47.351284
2415.244929	209.537424	47.356289
2411.655065	225.850540	47.361293
2408.248016	211.690033	47.366298
2404.161792	213.615637	47.371303
2401.068963	209.878986	47.376308
2397.166001	203.878633	47.381313
2394.370946	206.839643	47.386317
2391.624979	203.321646	47.391322
2387.682436	212.280311	47.396327
2383.806810	209.412402	47.401332
2379.673288	213.469049	47.406337
2376.143845	207.893693	47.411341
2373.554292	216.849349	47.416346
2369.584996	214.608577	47.421351
2366.168003	214.654889	47.426356
2362.964243	206.618958	47.431361
2359.641174	202.225150	47.436365
2355.953055	205.215850	47.441370
2352.093112	210.407150	47.446375
2348.839113	209.340755	47.451380
2345.306318	202.733904	47.456385
2341.790524	209.920055	47.461389
2338.351569	209.409326	47.466394
2334.300977	211.606518	47.471399
2331.241493	209.291099	47.476404
2327.915259	202.342081	47.481409
2324.629233	198.516572	47.486413
2321.305628	197.183551	47.491418
2317.448130	203.019984	47.496423
2314.152776	192.031645	47.501428
2309.982229	200.637746	47.506433
2306.615622	193.141632	47.511437
2303.451041	196.439856	47.516442
2299.563489	201.693249	47.521447
2296.743265	203.664064	47.526452
2292.652523	197.171460	47.531457
2289.528105	195.170540	47.536461
2286.217943	199.776523	47.541466
2282.106776	195.149767	47.546471
2279.408878	191.799305	47.551476
2275.400947	196.814372	47.556481
2271.800243	200.306281	47.561485
2268.568769	194.542341	47.566490
2264.547237	193.662654	47.571495
2261.466556	195.552423	47.576500
2258.081761	191.976366	47.581505
2254.557243	189.710254	47.586509
2250.915255	198.643867	47.591514
2247.260685	204.520364	47.596519
2243.896403	191.513735	47.601524
2240.484913	195.133191	47.606529
2237.097757	203.938260	47.611533
2233.929243	199.483309	47.616538
2229.742886	192.105962	47.621543
2226.337808	198.343645	47.626548
2222.615854	199.208473	47.631553
2219.177236	197.361023	47.636557
2215.684073	195.779083	47.641562
2212.354041	202.742753	47.646567
2209.323094	192.386870	47.651572
2205.839273	196.503274	47.656577
2202.299696	205.474084	47.661581
2198.868563	189.696148	47.666586
2194.931625	196.676655	47.671591
2191.533453	199.975369	47.676596
2187.981377	196.571568	47.681601
2184.369401	190.432980	47.686605
2180.803532	191.300498	47.691610
2177.124013	200.094514	47.696615
2174.047599	188.754833	47.701620
2170.683068	196.392517	47.706625
2166.764977	192.576032	47.711629
2163.346221	191.812349	47.716634
2159.959232	200.819172	47.721639
2156.524232	196.262396	47.726644
2152.986018	185.916025	47.731649
2149.359206	192.132297	47.736653
2145.789998	197.839072	47.741658
2142.407953	206.360480	47.746663
2139.121210	191.196393	47.751668
2135.473625	194.214839	47.756673
2132.297488	199.199229	47.761677
2128.496503	194.536399	47.766682
2124.669374	203.148293	47.771687
2121.269640	190.668895	47.776692
2118.010242	200.549023	47.781697
2114.582351	195.431014	47.786701
2111.255026	190.536455	47.791706
2107.433856	204.681207	47.796711
2104.244960	188.320362	47.801716
2100.490937	196.357854	47.806721
2097.263558	196.069737	47.811725
2093.639552	195.921039	47.816730
2089.737577	190.233948	47.821735
2086.428701	191.783171	47.826740
2083.039024	196.699113	47.831745
2079.533937	185.902273	47.836749
2076.330952	183.769283	47.841754
2072.387423	184.878014	47.846759
2068.941670	186.454262	47.851764
2065.327515	185.579804	47.856769
2062.081400	189.909720	47.861773
2058.741587	188.819924	47.866778
2054.974710	183.323969	47.871783
2051.678092	190.236800	47.876788
2047.810054	183.555190	47.881793
2044.254806	185.047795	47.886797
2040.862908	177.386113	47.891802
2037.746943	193.104563	47.896807
2034.063354	178.650548	47.901812
2030.487449	186.132540	47.906817
2026.792991	189.336845	47.911821
2023.116242	176.868880	47.916826
2019.684325	184.652891	47.921831
2016.545406	178.101620	47.926836
2013.366832	184.012949	47.931841
2009.531088	184.574337	47.936845
2006.217282	180.729298	47.941850
2002.271952	186.547011	47.946855
1999.069193	174.207364	47.951860
1995.329253	178.660499	47.956865
1991.747502	181.765130	47.961869
1988.592473	187.137761	47.966874
1984.920421	189.925309	47.971879
1981.771498	177.318798	47.976884
1978.203052	184.808755	47.981889
1974.309279	179.560891	47.986893
1970.996441	193.317664	47.991898
1967.556868	181.151665	47.996903
1964.188955	178.571389	48.001908
1960.673225	186.615304	48.006913
1956.712660	175.758226	48.011917
1953.669752	185.912570	48.016922
1950.148979	183.775827	48.021927
1946.498430	185.622102	48.026932
1942.949290	178.450007	48.031937
1939.478493	181.365483	48.036941
1935.959704	177.970533	48.041946
1932.273010	172.611088	48.046951
1928.698495	184.044531	48.051956
1925.355431	179.354816	48.056961
1922.195923	177.632540	48.061965
1918.634202	178.564119	48.066970
1914.849982	177.090230	48.071975
1911.511614	169.904202	48.076980
1908.217327	179.365323	48.081985
1904.549331	176.866055	48.086989
1900.994960	187.085458	48.091994
1897.492211	187.872650	48.096999
1893.797513	185.156501	48.102004
1890.242710	182.374064	48.107009
1886.697842	180.192000	48.112013
1883.403066	183.829346	48.117018
1879.715403	187.403453	48.122023
1876.810361	172.873492	48.127028
1873.115667	178.405539	48.132033
1869.519612	177.085417	48.137037
1866.138288	166.140637	48.142042
1862.210441	167.208711	48.147047
1859.147637	165.011654	48.152052
1855.424307	175.859373	48.157057
1851.850684	177.128285	48.162061
1848.752777	170.637915	48.167066
1844.897878	173.939313	48.172071
1841.286140	178.833185	48.177076
1837.997001	183.881806	48.182081
1834.445006	174.968936	48.187085
1831.137542	167.869408	48.192090
1826.995002	172.469645	48.197095
1823.903656	161.518783	48.202100
1820.710003	178.430530	48.207105
1816.925772	169.779942	48.212109
1813.444056	177.165973	48.217114
1809.864442	176.373948	48.222119
1806.655727	171.392795	48.227124
1803.294299	173.639934	48.232129
1799.234520	170.642126	48.237133
1796.023914	160.763536	48.242138
1792.305913	164.383333	48.247143
1788.951696	170.524784	48.252148
1785.227786	168.988529	48.257153
1781.342929	162.902007	48.262157
1778.567329	157.696988	48.267162
1774.977063	174.739689	48.272167
1771.731283	168.577227	48.277172
1767.895443	175.527232	48.282177
1764.498135	173.748368	48.287181
1761.052780	167.425669	48.292186
1757.273166	174.613736	48.297191
1754.002164	179.301073	48.302196
1750.493162	167.411667	48.307201
1746.628726	173.943651	48.312205
1743.388026	165.370261	48.317210
1739.829779	166.513663	48.322215
1736.504093	170.427377	48.327220
1732.761893	169.036531	48.332225
1729.224422	166.626910	48.337229
1725.863770	175.206390	48.342234
1722.308342	164.396184	48.347239
1719.078065	165.968410	48.352244
1715.258912	163.984612	48.357249
1711.938166	163.840724	48.362253
1708.679157	152.896089	48.367258
1704.629482	164.228544	48.372263
1701.515801	162.072906	48.377268
1697.580661	168.939188	48.382273
1694.280251	167.608160	48.387277
1690.986780	152.477068	48.392282
1687.356851	169.501474	48.397287
1683.938553	170.136022	48.402292
1679.954614	168.165622	48.407297
1676.684587	170.695878	48.412301
1673.449503	170.497719	48.417306
1669.742603	174.100058	48.422311
1666.177023	168.779186	48.427316
1662.569355	167.556884	48.432321
1659.451837	166.612918	48.437325
1656.434673	159.877973	48.442330
1652.455970	161.281008	48.447335
1649.201594	153.652209	48.452340
1645.260260	157.646138	48.457345
1641.648288	174.526323	48.462349
1638.622445	157.265873	48.467354
1634.598896	169.541360	48.472359
1631.116145	159.881701	48.477364
1627.798400	166.406697	48.482369
1623.908109	173.973383	48.487373
1621.021879	169.969686	48.492378
1616.918534	162.989767	48.497383
1613.788653	159.544036	48.502388
1610.315620	164.410778	48.507393
1606.895478	161.868405	48.512397
1603.566568	154.946378	48.517402
1599.606328	173.187507	48.522407
1596.222059	154.483185	48.527412
1592.604886	159.190315	48.532417
1588.947118	157.802091	48.537421
1586.071964	156.050215	48.542426
1582.506769	163.697049	48.547431
1578.902381	161.597778	48.552436
1575.067114	158.013735	48.557441
1571.711692	166.271078	48.562445
1568.125805	154.000051	48.567450
1564.521006	168.162839	48.572455
1561.342641	152.731560	48.577460
1557.980542	153.406123	48.582465
1554.453994	153.682415	48.587469
1550.861264	164.449305	48.592474
1546.969939	160.526070	48.597479
1543.880723	160.445768	48.602484
1540.136004	154.353733	48.607489
1536.146258	166.290714	48.612493
1533.338756	162.134565	48.617498
1529.776623	161.194674	48.622503
1526.318700	154.008663	48.627508
1522.453678	155.423394	48.632513
1518.836768	161.921342	48.637517
1515.635660	151.403033	48.642522
1512.154376	158.084893	48.647527
1508.827739	147.755122	48.652532
1505.464925	153.428492	48.657537
1501.748535	151.058978	48.662541
1498.282959	156.214983	48.667546
1494.558536	165.038968	48.672551
1491.249615	154.570824	48.677556
1487.833287	154.542458	48.682561
1484.209386	158.875950	48.687565
1480.720904	156.259878	48.692570
1477.027647	165.436163	48.697575
1473.237289	158.703816	48.702580
1470.176977	155.589408	48.707585
1466.448940	158.324582	48.712589
1463.279460	148.011818	48.717594
1459.722900	163.341586	48.722599
1456.051691	153.836558	48.727604
1452.531863	152.463921	48.732609
1449.227554	155.483254	48.737613
1445.849384	161.947851	48.742618
1442.152684	166.833526	48.747623
1439.046510	162.989238	48.752628
1435.323382	148.993928	48.757633
1431.635648	160.153806	48.762637
1428.022854	161.933428	48.767642
1424.561425	155.518072	48.772647
1421.138577	155.025154	48.777652
1417.344676	159.331880	48.782657
1413.897586	158.743027	48.787661
1410.564208	156.928633	48.792666
1407.049769	154.143346	48.797671
1403.789408	148.419951	48.802676
1400.244655	154.172228	48.807681
1396.640483	154.786288	48.812685
1393.228679	143.118056	48.817690
1389.442953	154.584468	48.822695
1386.075245	152.626682	48.827700
1382.480051	142.486636	48.832705
1379.015628	148.626505	48.837709
1375.983686	149.740244	48.842714
1371.912098	153.115230	48.847719
1368.595574	151.221913	48.852724
1365.128817	156.973961	48.857729
1361.548834	147.725148	48.862733
1358.118712	146.691046	48.867738
1354.460977	162.782606	48.872743
1351.048369	159.192370	48.877748
1347.885663	144.647843	48.882753
1343.772387	154.346044	48.887757
1340.577725	149.309145	48.892762
1337.024607	156.809555	48.897767
1333.425742	160.974918	48.902772
1330.000979	159.556760	48.907777
1326.386293	159.163132	48.912781
1323.176458	162.175905	48.917786
1319.324804	164.350566	48.922791
1316.156971	157.556606	48.927796
1312.414029	159.694089	48.932801
1309.028956	165.884828	48.937805
1305.561257	150.910301	48.942810
1302.240162	160.565279	48.947815
1298.622465	147.291899	48.952820
1295.135251	144.214300	48.957825
1291.070052	153.904985	48.962829
1288.145481	157.603807	48.967834
1284.406164	163.339517	48.972839
1281.088848	162.574811	48.977844
1277.441571	156.246746	48.982849
1273.802078	162.482157	48.987853
1270.787198	162.001983	48.992858
1266.780340	162.174987	48.997863
1263.258443	151.757819	49.002868
1259.938656	146.191210	49.007873
1256.302720	154.971486	49.012877
1253.329567	156.740619	49.017882
1249.729151	142.731699	49.022887
1246.204335	142.233304	49.027892
1242.803463	144.753874	49.032897
1239.033729	146.350045	49.037901
1235.436757	144.103528	49.042906
1231.706510	151.118230	49.047911
1228.431081	149.072286	49.052916
1224.949181	148.883507	49.057921
1221.364849	150.072116	49.062925
1218.121557	162.063205	49.067930
1213.920176	150.307974	49.072935
1210.575407	165.070714	49.077940
1207.565336	155.738865	49.082945
1203.941880	154.795652	49.087949
1200.474791	156.655616	49.092954
1196.844414	153.262122	49.097959
1193.512398	156.897716	49.102964
1190.134805	149.926142	49.107969
1186.168258	150.549123	49.112973
1182.986434	144.368137	49.117978
1179.562848	159.251428	49.122983
1175.962717	150.964407	49.127988
1172.503244	159.935498	49.132993
1168.569861	160.015038	49.137997
1165.503441	143.129980	49.143002
1161.511722	143.106489	49.148007
1158.096191	135.992330	49.153012
1154.732858	130.755580	49.158017
1151.647643	146.087443	49.163021
1148.157305	143.990495	49.168026
1144.468025	151.110647	49.173031
1141.068261	139.060757	49.178036
1137.327143	139.280536	49.183041
1133.484564	147.843103	49.188045
1130.261021	138.469497	49.193050
1126.956054	142.667040	49.198055
1123.252738	145.743111	49.203060
1120.138152	141.768765	49.208065
1116.364845	147.487372	49.213069
1112.604731	135.905924	49.218074
1109.047994	148.657831	49.223079
1105.917377	144.493757	49.228084
1102.443514	132.133819	49.233089
1098.777496	140.277854	49.238093
1095.776815	137.124187	49.243098
1091.983340	146.130515	49.248103
1088.513415	139.932523	49.253108
1084.874521	140.300407	49.258113
1081.062379	143.627295	49.263117
1077.727518	141.445425	49.268122
1074.043101	143.130301	49.273127
1070.798163	155.652678	49.278132
1067.711789	137.454900	49.283137
1063.680687	145.167126	49.288141
1060.284418	133.421269	49.293146
1056.741653	143.294256	49.298151
1053.187455	139.331452	49.303156
1050.000693	135.810350	49.308161
1046.314464	145.620408	49.313165
1043.060148	137.215118	49.318170
1039.373985	143.298709	49.323175
1035.838681	148.123202	49.328180
1032.505281	144.080350	49.333185
1028.839684	144.674256	49.338189
1025.027008	144.896142	49.343194
1021.566714	146.012383	49.348199
1018.053679	145.700103	49.353204
1015.037800	150.691214	49.358209
1011.002763	154.990008	49.363213
1007.695098	141.531963	49.368218
1004.252175	139.935346	49.373223
1000.716390	150.256786	49.378228
997.256684	135.826436	49.383233
993.704313	150.817173	49.388237
990.384620	141.817742	49.393242
986.633865	142.948807	49.398247
983.305089	138.620003	49.403252
979.754550	135.879486	49.408257
976.177052	142.198713	49.413261
972.884534	132.122809	49.418266
969.241327	124.580796	49.423271
965.525728	142.056116	49.428276
962.102932	136.073973	49.433281
958.568677	127.427570	49.438285
955.663551	134.130355	49.443290
951.925327	137.286564	49.448295
948.254902	147.613384	49.453300
944.771017	135.511707	49.458305
941.018304	148.797409	49.463309
937.917543	150.137572	49.468314
934.251452	141.207306	49.473319
930.559235	140.571960	49.478324
927.243051	140.910914	49.483329
923.703435	147.555991	49.488333
919.956979	142.116548	49.493338
916.338586	140.486006	49.498343
913.080178	133.329375	49.503348
909.647000	135.678543	49.508353
906.064526	143.077137	49.513357
902.948117	132.546493	49.518362
899.135071	142.491501	49.523367
895.672230	141.981084	49.528372
891.917163	130.004331	49.533377
888.586140	142.575011	49.538381
885.019158	145.104630	49.543386
881.378329	137.245387	49.548391
878.472073	139.131586	49.553396
875.132522	135.702000	49.558401
871.015789	129.516032	49.563405
867.686716	128.370097	49.568410
864.054808	135.260304	49.573415
860.189694	133.613214	49.578420
857.373684	130.965268	49.583425
853.506880	126.341507	49.588429
850.436857	124.488849	49.593434
846.987450	133.773408	49.598439
842.970711	134.377547	49.603444
839.288420	119.256679	49.608449
835.804868	135.771582	49.613453
832.749091	123.061717	49.618458
829.012245	131.038110	49.623463
825.812105	137.387435	49.628468
822.549744	129.043884	49.633473
818.425317	133.858517	49.638477
814.993820	120.178762	49.643482
811.402090	127.921159	49.648487
807.847922	142.754600	49.653492
804.391030	135.847848	49.658497
800.956528	136.272700	49.663501
797.798401	130.509770	49.668506
794.035891	141.533673	49.673511
790.268314	140.824821	49.678516
787.254080	133.804041	49.683521
783.423572	143.814436	49.688525
779.864269	131.279890	49.693530
776.718713	134.595813	49.698535
772.791585	127.421045	49.703540
769.667810	132.509582	49.708545
765.989123	130.159914	49.713549
762.651574	128.762181	49.718554
759.048530	137.532303	49.723559
755.218572	120.129098	49.728564
752.176137	125.715543	49.733569
748.279494	136.270700	49.738573
745.008278	129.330661	49.743578
741.522594	138.992797	49.748583
738.012539	136.869829	49.753588
734.642841	139.072257	49.758593
731.352806	142.472735	49.763597
727.569746	130.174857	49.768602
724.225444	139.821347	49.773607
720.186653	132.247637	49.778612
716.573282	130.166112	49.783617
713.420636	138.137343	49.788621
710.286217	124.180599	49.793626
706.326349	136.110139	49.798631
702.663104	122.503652	49.803636
699.516184	120.905572	49.808641
695.824028	138.843365	49.813645
692.719918	121.217042	49.818650
689.151305	127.085650	49.823655
685.514782	121.871886	49.828660
681.810876	126.706529	49.833665
678.360119	141.875044	49.838669
674.670878	134.163132	49.843674
671.171933	127.362657	49.848679
667.647219	132.514294	49.853684
664.384223	124.894586	49.858689
661.126766	136.335223	49.863693
657.707007	126.605204	49.868698
653.872962	128.272887	49.873703
650.701709	115.950196	49.878708
646.944891	133.784831	49.883713
643.273227	137.744024	49.888717
639.782244	130.891147	49.893722
636.353001	127.220887	49.898727
632.748578	131.220872	49.903732
629.420255	128.096288	49.908737
625.653447	128.183263	49.913741
622.520996	131.923284	49.918746
618.856240	133.887113	49.923751
615.441815	138.632548	49.928756
612.057080	132.563524	49.933761
607.946251	145.229261	49.938765
604.820772	134.578447	49.943770
601.488071	139.233341	49.948775
598.011998	127.078220	49.953780
594.649149	123.557236	49.958785
591.080819	138.652658	49.963789
587.535471	134.871076	49.968794
583.907337	127.583616	49.973799
580.400556	124.282047	49.978804
576.958570	125.256876	49.983809
573.074507	135.897941	49.988813
569.534148	118.729501	49.993818
565.828957	128.838074	49.998823
562.173911	132.006696	50.003828
559.370447	125.121707	50.008833
555.975535	134.403603	50.013837
552.507477	120.148286	50.018842
549.292002	127.487111	50.023847
545.751913	134.482368	50.028852
542.188897	124.847708	50.033857
538.102473	132.662273	50.038861
534.624638	137.771901	50.043866
531.158792	136.653563	50.048871
527.645610	135.904324	50.053876
524.442082	128.729873	50.058881
520.340705	126.754125	50.063885
516.871943	124.901192	50.068890
513.891190	128.330101	50.073895
510.233721	135.421023	50.078900
507.126874	134.428973	50.083905
503.157308	138.928752	50.088909
499.935694	126.290674	50.093914
496.540794	135.909800	50.098919
492.731296	134.805726	50.103924
489.570133	129.650199	50.108929
485.343955	134.885925	50.113933
482.095641	138.923060	50.118938
478.467228	124.760870	50.123943
475.173182	129.249019	50.128948
472.166773	125.995086	50.133953
468.249364	131.651493	50.138957
464.808211	133.046419	50.143962
461.510929	142.837970	50.148967
457.310020	136.093885	50.153972
454.092681	127.889025	50.158977
450.779293	139.389889	50.163981
447.508265	119.722881	50.168986
443.791741	132.812200	50.173991
439.982045	130.926539	50.178996
436.804495	124.929254	50.184001
432.791527	137.925780	50.189005
429.671998	124.746036	50.194010
426.228157	126.925838	50.199015
422.808368	126.640401	50.204020
419.216734	117.792402	50.209025
415.581944	123.325888	50.214029
412.379551	123.393744	50.219034
408.472056	121.872810	50.224039
405.102018	123.429850	50.229044
401.558115	124.942410	50.234049
397.941934	125.537672	50.239053
394.507418	125.749542	50.244058
391.324637	119.068773	50.249063
387.948627	131.149736	50.254068
384.565575	126.529627	50.259073
380.901936	129.302772	50.264077
377.407433	125.734696	50.269082
373.434679	123.694388	50.274087
369.708823	122.397807	50.279092
366.767705	124.953341	50.284097
362.848044	122.062833	50.289101
359.498061	122.081302	50.294106
355.931451	120.160667	50.299111
352.204464	118.288923	50.304116
349.459348	110.826644	50.309121
345.938758	120.943292	50.314125
342.411323	117.588349	50.319130
338.698246	118.088269	50.324135
335.086592	122.167043	50.329140
331.632640	108.735604	50.334145
328.075305	121.437980	50.339149
324.691015	123.386711	50.344154
320.803921	119.258739	50.349159
316.998754	123.337429	50.354164
314.018786	128.350211	50.359169
310.507001	128.160239	50.364173
307.282352	123.458562	50.369178
303.591277	121.488375	50.374183
300.200311	106.201494	50.379188
297.095982	114.582703	50.384193
293.171413	123.499476	50.389197
289.527886	120.516930	50.394202
286.259824	118.985439	50.399207
282.621494	123.042997	50.404212
279.053493	122.183481	50.409217
275.118414	119.886919	50.414221
271.774002	137.730915	50.419226
268.536924	134.149967	50.424231
264.769032	128.551701	50.429236
261.541687	120.005191	50.434241
258.105945	132.030962	50.439245
254.521685	128.504028	50.444250
251.175060	133.401708	50.449255
247.744974	129.515454	50.454260
244.198876	125.000400	50.459265
240.622371	133.473069	50.464269
236.658594	126.550866	50.469274
233.553537	129.509914	50.474279
229.930053	122.375423	50.479284
226.456063	115.773938	50.484289
222.927017	136.210243	50.489293
219.705166	121.199323	50.494298
216.091928	114.631013	50.499303
212.352444	133.196159	50.504308
208.858005	119.197209	50.509313
205.109568	126.361513	50.514317
201.994011	111.650822	50.519322
198.814966	121.742773	50.524327
195.014032	122.311354	50.529332
191.686186	113.315644	50.534337
187.866759	124.600789	50.539341
184.335827	118.168954	50.544346
180.728928	111.450355	50.549351
177.241364	120.580688	50.554356
174.004475	107.674548	50.559361
170.352115	126.143818	50.564365
167.274547	123.770557	50.569370
163.538747	114.152271	50.574375
159.718525	115.168799	50.579380
156.502401	110.555084	50.584385
153.189449	119.075891	50.589389
149.605982	104.668276	50.594394
146.204068	113.246697	50.599399
142.241684	118.128273	50.604404
138.946497	117.383976	50.609409
135.097612	122.808251	50.614413
131.834825	112.421440	50.619418
128.292840	117.514136	50.624423
124.819942	124.896166	50.629428
121.495836	115.542648	50.634433
117.806587	115.727105	50.639437
114.314970	116.397737	50.644442
110.975527	113.058335	50.649447
107.053006	114.938064	50.654452
103.885646	111.327540	50.659457
100.340458	117.706654	50.664461
96.979130	118.291247	50.669466
93.467196	116.283200	50.674471
89.895609	124.726315	50.679476
86.707521	111.242824	50.684481
82.874394	117.572646	50.689485
79.431855	101.751545	50.694490
75.741367	115.425286	50.699495
71.823508	111.494152	50.704500
68.791614	113.455518	50.709505
65.558725	118.405716	50.714509
61.937653	120.788428	50.719514
58.290880	113.129797	50.724519
54.444675	113.802822	50.729524
51.577170	112.024826	50.734529
48.030727	125.494838	50.739533
44.569329	112.879618	50.744538
40.898900	117.094043	50.749543
37.321852	121.170313	50.754548
33.799278	112.960902	50.759553
30.460966	123.741217	50.764557
26.924984	118.216762	50.769562
23.224994	117.762084	50.774567
19.581291	123.633956	50.779572
16.068323	120.565282	50.784577
12.694439	121.393009	50.789581
8.907860	129.579278	50.794586
5.949044	121.042018	50.799591
1.908337	131.390786	50.804596