Thu Jun 16 18:44:10 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.794559	77.776241	0.000000
0.366478	76.912389	0.005005
0.468818	83.711016	0.010010
0.918815	77.451441	0.015014
0.756988	79.156267	0.020019
0.501855	67.679052	0.025024
-0.123715	56.615162	0.030029
-0.477455	54.012765	0.035034
-0.692997	43.737744	0.040038
-1.187980	54.063124	0.045043
-0.934935	27.543239	0.050048
-1.548839	35.459284	0.055053
-1.870724	44.504322	0.060058
-2.065418	24.312948	0.065062
-2.775519	39.368643	0.070067
-3.006139	30.911368	0.075072
-3.231748	24.740182	0.080077
-3.835050	26.801394	0.085082
-3.516079	21.160356	0.090086
-3.848624	24.376364	0.095091
-3.709840	29.806129	0.100096
-3.878552	37.806649	0.105101
-4.536858	34.623987	0.110106
-5.079250	32.035901	0.115110
-5.389839	33.856463	0.120115
-5.762792	32.339782	0.125120
-5.771433	36.485556	0.130125
-5.630477	27.469559	0.135130
-5.487946	28.175617	0.140134
-5.955542	29.529839	0.145139
-6.845920	25.551998	0.150144
-6.752200	34.888930	0.155149
-6.729189	36.963250	0.160154
-6.681928	28.425329	0.165158
-7.775324	42.719222	0.170163
-8.090817	29.032973	0.175168
-8.208158	43.649072	0.180173
-8.609718	49.796966	0.185178
-8.566470	31.724235	0.190182
-8.557309	45.861279	0.195187
-8.409134	38.331500	0.200192
-9.035438	38.309575	0.205197
-9.780290	38.191520	0.210202
-10.378038	38.564526	0.215206
-10.505613	23.440115	0.220211
-10.251975	31.372215	0.225216
-10.193236	28.702545	0.230221
-10.351335	31.466103	0.235226
-10.724227	30.511645	0.240230
-11.905121	38.808774	0.245235
-11.417411	22.516324	0.250240
-11.620849	24.513824	0.255245
-11.779638	33.423184	0.260250
-12.150173	31.452293	0.265254
-13.049440	31.114698	0.270259
-13.403543	36.114198	0.275264
-13.526562	32.571776	0.280269
-13.880238	28.959249	0.285274
-13.227609	26.299263	0.290278
-13.774878	35.287425	0.295283
-13.375211	29.072098	0.300288
-13.877116	30.824241	0.305293
-14.584501	28.139315	0.310298
-14.745867	32.035968	0.315302
-15.258680	23.555684	0.320307
-14.764406	32.036589	0.325312
-15.671253	37.469768	0.330317
-16.582258	35.190222	0.335322
-16.471760	29.292800	0.340326
-17.051995	43.636454	0.345331
-16.591790	40.637521	0.350336
-16.691184	31.574328	0.355341
-16.781324	38.122788	0.360346
-16.505188	25.651271	0.365350
-17.567457	40.676673	0.370355
-18.121613	31.123048	0.375360
-18.388632	41.524494	0.380365
-18.576986	35.973211	0.385370
-18.244025	39.682415	0.390374
-18.741082	39.208800	0.395379
-18.595389	31.284324	0.400384
-19.499386	21.915291	0.405389
-19.819957	29.021934	0.410394
-19.690463	34.487468	0.415398
-20.070426	31.534155	0.420403
-19.872628	20.174602	0.425408
-20.083508	38.879304	0.430413
-20.630451	33.386000	0.435418
-20.883024	30.508217	0.440422
-20.967703	41.212094	0.445427
-21.542940	38.765382	0.450432
-22.522593	40.180157	0.455437
-22.839245	43.908028	0.460442
-22.509358	28.362821	0.465446
-22.981963	40.566822	0.470451
-22.945600	36.744419	0.475456
-23.277447	28.447617	0.480461
-23.148536	36.065102	0.485466
-22.900463	27.227333	0.490470
-23.068157	34.989332	0.495475
-24.027991	27.736689	0.500480
-24.338556	31.803711	0.505485
-24.526490	42.194751	0.510490
-24.431052	34.575036	0.515494
-25.413286	29.093196	0.520499
-25.492848	25.993854	0.525504
-25.990123	31.299856	0.530509
-26.371628	42.811046	0.535514
-26.184103	34.899288	0.540518
-26.335305	34.564346	0.545523
-26.410498	40.776785	0.550528
-26.259579	37.030948	0.555533
-26.767872	42.785384	0.560538
-27.002224	38.759899	0.565542
-27.663001	41.052685	0.570547
-27.588156	31.496232	0.575552
-28.590196	35.023253	0.580557
-29.069293	40.838765	0.585562
-29.120612	30.953037	0.590566
-29.062237	44.755396	0.595571
-29.229996	37.331796	0.600576
-29.537670	46.909884	0.605581
-29.519338	35.359092	0.610586
-29.315566	36.278678	0.615590
-29.412791	39.553172	0.620595
-30.334718	35.457624	0.625600
-30.594767	25.768879	0.630605
-30.839010	34.825545	0.635610
-30.939378	30.755426	0.640614
-31.066110	36.363538	0.645619
-31.991339	35.055529	0.650624
-32.142531	41.402957	0.655629
-32.668994	38.712402	0.660634
-32.258794	16.789134	0.665638
-32.681597	45.970855	0.670643
-32.743719	38.755518	0.675648
-32.472054	38.436620	0.680653
-33.133002	39.747328	0.685658
-33.374515	30.335894	0.690662
-33.622038	33.854930	0.695667
-33.852220	28.305631	0.700672
-34.905431	28.815668	0.705677
-35.404464	34.279513	0.710682
-34.727942	38.619855	0.715686
-35.303175	36.557997	0.720691
-35.473993	26.450614	0.725696
-35.713339	25.868707	0.730701
-35.710963	39.766342	0.735706
-35.444557	34.983008	0.740710
-36.431078	38.008273	0.745715
-36.796306	39.867562	0.750720
-37.004948	39.918579	0.755725
-37.282508	51.362382	0.760730
-37.138740	34.541445	0.765734
-37.387800	39.122950	0.770739
-37.512290	38.156052	0.775744
-38.285678	39.094670	0.780749
-38.712915	39.652692	0.785754
-38.636195	31.707849	0.790758
-39.121149	31.786773	0.795763
-38.906776	32.875674	0.800768
-38.931292	26.031285	0.805773
-39.705132	38.496582	0.810778
-40.339743	32.125143	0.815782
-40.674487	31.455809	0.820787
-40.518069	32.102351	0.825792
-40.481345	37.604229	0.830797
-40.739717	45.790044	0.835802
-40.423499	28.283081	0.840806
-41.241651	40.677470	0.845811
-41.819184	41.815461	0.850816
-42.171192	34.812492	0.855821
-42.398869	38.228805	0.860826
-42.339058	35.829566	0.865830
-42.832705	47.184772	0.870835
-42.606150	36.499300	0.875840
-43.204219	33.078106	0.880845
-43.853835	30.027593	0.885850
-43.767604	27.102699	0.890854
-43.841369	36.895961	0.895859
-43.871655	34.335218	0.900864
-43.825451	38.534079	0.905869
-44.507357	39.174243	0.910874
-45.418438	34.383758	0.915878
-45.487177	38.474251	0.920883
-45.536212	36.922884	0.925888
-45.583749	37.243931	0.930893
-45.883079	28.172450	0.935898
-45.750852	30.102145	0.940902
-46.506367	34.921051	0.945907
-46.636756	41.307660	0.950912
-46.701268	48.234075	0.955917
-46.864044	46.987307	0.960922
-46.811511	31.401318	0.965926
-47.906481	55.167017	0.970931
-48.322731	42.619908	0.975936
-48.231990	45.282757	0.980941
-48.456129	42.712812	0.985946
-48.326071	44.422374	0.990950
-48.467021	40.689848	0.995955
-49.062150	33.166012	1.000960
-49.742729	40.427851	1.005965
-50.013850	39.916505	1.010970
-50.074581	40.479365	1.015974
-50.109972	52.663109	1.020979
-50.265146	35.441910	1.025984
-50.452235	54.790755	1.030989
-51.001989	47.656893	1.035994
-51.260402	37.131973	1.040998
-51.703755	39.541052	1.046003
-51.812288	33.845172	1.051008
-51.716462	34.534481	1.056013
-51.824260	36.962490	1.061018
-51.818485	20.223865	1.066022
-52.445861	33.543669	1.071027
-52.830783	30.571348	1.076032
-53.026277	33.031706	1.081037
-53.350585	40.482980	1.086042
-53.877480	34.089498	1.091046
-54.675584	35.319386	1.096051
-54.754795	39.036229	1.101056
-54.154878	41.456685	1.106061
-54.718012	36.456670	1.111066
-54.690801	29.289419	1.116070
-54.922969	34.119601	1.121075
-55.063842	29.962061	1.126080
-55.859308	39.310194	1.131085
-56.357624	35.499206	1.136090
-56.534691	26.929799	1.141094
-56.691401	48.042885	1.146099
-56.382747	38.130418	1.151104
-56.294081	40.745465	1.156109
-56.914054	38.094142	1.161114
-57.624888	40.276423	1.166118
-58.016654	42.915228	1.171123
-58.078636	35.183612	1.176128
-58.249043	35.320652	1.181133
-58.276669	42.113012	1.186138
-57.967846	45.318724	1.191142
-58.838184	32.107650	1.196147
-59.260306	33.597903	1.201152
-59.466931	39.554742	1.206157
-59.971954	38.597264	1.211162
-59.645070	33.865397	1.216166
-59.968187	33.159021	1.221171
-60.729435	33.382363	1.226176
-61.090931	43.365538	1.231181
-61.480420	35.239368	1.236186
-61.236236	35.394705	1.241190
-61.405678	40.764719	1.246195
-61.593025	32.488434	1.251200
-61.879150	46.139365	1.256205
-61.861025	46.684359	1.261210
-61.887479	30.677051	1.266214
-62.515444	50.998778	1.271219
-62.932164	43.043041	1.276224
-62.940958	42.963955	1.281229
-63.852460	40.558221	1.286234
-64.182491	34.412581	1.291238
-64.507164	35.440515	1.296243
-64.080479	21.553293	1.301248
-64.547151	32.587743	1.306253
-64.939755	33.652948	1.311258
-64.584838	31.347100	1.316262
-64.883137	33.507964	1.321267
-64.989943	45.595082	1.326272
-65.781700	39.519830	1.331277
-66.141028	42.411947	1.336282
-66.287709	35.919719	1.341286
-66.424286	40.238562	1.346291
-66.594109	39.186225	1.351296
-66.640377	39.822757	1.356301
-67.528304	35.492718	1.361306
-67.697022	28.625597	1.366310
-67.980530	26.222921	1.371315
-67.612618	36.708153	1.376320
-67.843781	27.937947	1.381325
-68.316092	37.977809	1.386330
-68.746689	28.135928	1.391334
-69.137293	39.883712	1.396339
-69.103968	41.924855	1.401344
-68.986717	43.264111	1.406349
-69.362344	38.053163	1.411354
-70.107018	30.749284	1.416358
-70.892581	50.046285	1.421363
-71.105513	43.921935	1.426368
-71.298688	37.805471	1.431373
-71.198418	41.936696	1.436378
-70.825907	38.116058	1.441382
-71.083127	45.262847	1.446387
-71.183947	28.219036	1.451392
-71.443355	38.681963	1.456397
-72.127058	42.534424	1.461402
-72.306078	37.905897	1.466406
-72.579570	36.264165	1.471411
-72.864425	38.781713	1.476416
-73.352534	36.147075	1.481421
-74.235362	39.754732	1.486426
-74.084033	30.862907	1.491430
-74.212468	32.091924	1.496435
-74.317570	33.642842	1.501440
-74.107976	36.806546	1.506445
-74.715446	39.521548	1.511450
-74.155555	32.400529	1.516454
-75.217686	47.133700	1.521459
-75.445071	39.026317	1.526464
-75.606546	44.769607	1.531469
-76.029046	41.163624	1.536474
-75.927340	33.239316	1.541478
-76.828260	32.745538	1.546483
-77.072456	36.417432	1.551488
-77.240111	36.873955	1.556493
-77.322185	36.981598	1.561498
-77.487930	46.012568	1.566502
-77.543102	44.218143	1.571507
-77.584285	43.206303	1.576512
-77.786034	36.077482	1.581517
-78.640266	36.525933	1.586522
-78.759994	36.034060	1.591526
-79.188464	43.079026	1.596531
-79.310492	33.968871	1.601536
-79.218475	30.531300	1.606541
-79.882070	38.045946	1.611546
-79.947295	31.738258	1.616550
-80.386343	33.791569	1.621555
-80.651756	40.633881	1.626560
-80.549710	40.154091	1.631565
-80.734085	43.334764	1.636570
-80.755763	33.794662	1.641574
-81.974610	40.148361	1.646579
-81.939698	38.826205	1.651584
-82.056086	44.424913	1.656589
-82.327364	39.134962	1.661594
-82.215894	30.746649	1.666598
-82.331561	42.897972	1.671603
-83.286777	34.267752	1.676608
-83.586959	38.376271	1.681613
-84.341369	45.922011	1.686618
-83.921157	41.128646	1.691622
-83.959146	43.879754	1.696627
-83.681107	35.050251	1.701632
-83.887796	36.691357	1.706637
-84.490304	42.770944	1.711642
-84.868637	35.024825	1.716646
-85.432814	38.452160	1.721651
-85.659052	30.222064	1.726656
-85.484227	25.529142	1.731661
-85.936319	40.042704	1.736666
-86.791219	25.642475	1.741670
-86.982605	23.849158	1.746675
-86.760040	34.727571	1.751680
-86.909838	22.156280	1.756685
-87.399573	24.915158	1.761690
-87.153159	23.225287	1.766694
-86.994211	24.431766	1.771699
-87.829206	21.284930	1.776704
-88.311373	27.232255	1.781709
-88.481807	37.967560	1.786714
-88.503401	25.753417	1.791718
-88.866327	38.311905	1.796723
-89.490929	38.082729	1.801728
-89.682198	32.295460	1.806733
-90.101121	32.561080	1.811738
-90.190832	36.606204	1.816742
-90.401408	35.868010	1.821747
-90.554251	36.834497	1.826752
-90.445953	40.886753	1.831757
-90.817169	33.524705	1.836762
-91.245975	30.296234	1.841766
-91.637704	33.316925	1.846771
-91.837094	34.742547	1.851776
-91.910230	34.376651	1.856781
-92.264337	30.399378	1.861786
-92.208017	45.684155	1.866790
-92.937503	43.552101	1.871795
-93.487195	28.576882	1.876800
-93.609170	22.907698	1.881805
-93.846046	22.213511	1.886810
-93.730773	26.522295	1.891814
-93.807321	35.468372	1.896819
-93.822559	33.689843	1.901824
-93.985350	34.764224	1.906829
-95.075959	41.560210	1.911834
-95.305514	39.331523	1.916838
-95.549223	42.625096	1.921843
-95.175172	38.299683	1.926848
-95.418670	40.636075	1.931853
-95.922288	41.855378	1.936858
-96.272238	36.688530	1.941862
-96.836474	41.219426	1.946867
-96.971841	39.920875	1.951872
-96.857081	34.812282	1.956877
-97.351006	44.601290	1.961882
-97.093019	33.635580	1.966886
-97.603216	36.867734	1.971891
-98.296695	28.624890	1.976896
-98.161498	25.991716	1.981901
-98.194625	33.801317	1.986906
-98.302181	33.997719	1.991910
-99.200547	32.685479	1.996915
-99.632309	35.884100	2.006912
-98.965496	35.741370	2.016909
-98.321706	35.087845	2.026906
-98.348079	38.328240	2.036902
-97.532081	37.608569	2.046899
-97.080699	33.200278	2.056896
-96.823111	37.972901	2.066893
-95.909761	40.595790	2.076890
-95.801692	38.805281	2.086886
-94.705118	30.739827	2.096883
-94.574161	36.046298	2.106880
-94.275786	33.555344	2.116877
-93.001716	37.519328	2.126874
-92.707634	40.263482	2.136870
-92.685256	38.837214	2.146867
-92.233853	34.736127	2.156864
-91.196472	36.348288	2.166861
-91.145234	34.566876	2.176858
-90.727582	32.498746	2.186854
-89.841509	29.943211	2.196851
-89.468813	31.258298	2.206848
-89.233691	35.007857	2.216845
-88.568914	43.115990	2.226842
-88.082213	43.271811	2.236838
-87.263015	34.591946	2.246835
-86.684784	37.349493	2.256832
-86.275484	35.834336	2.266829
-86.484983	35.575408	2.276826
-85.346357	32.136322	2.286822
-84.924430	43.066903	2.296819
-84.753462	40.382600	2.306816
-83.960997	39.703073	2.316813
-83.573435	28.081435	2.326810
-82.536718	31.101779	2.336806
-82.260461	35.367585	2.346803
-82.131056	34.110572	2.356800
-81.810135	40.229140	2.366797
-80.668273	39.907785	2.376794
-80.330427	35.055914	2.386790
-80.027971	35.671240	2.396787
-79.798891	39.985147	2.406784
-79.200745	39.396016	2.416781
-78.428103	41.364674	2.426778
-77.702530	37.473772	2.436774
-77.392473	39.654557	2.446771
-77.174639	38.369840	2.456768
-76.576019	32.931626	2.466765
-76.129895	35.620474	2.476762
-75.019632	33.800305	2.486758
-74.493167	37.874416	2.496755
-74.426847	29.514470	2.506752
-74.121865	41.945155	2.516749
-73.841050	37.412633	2.526746
-73.227316	40.030862	2.536742
-72.360069	36.479763	2.546739
-71.744645	37.182598	2.556736
-71.468574	36.335932	2.566733
-71.103148	35.971811	2.576730
-70.205151	28.265699	2.586726
-70.129251	21.339707	2.596723
-69.641021	31.062694	2.606720
-68.906956	30.948759	2.616717
-68.504032	35.334691	2.626714
-67.887079	35.336423	2.636710
-67.069941	35.988387	2.646707
-66.831645	34.339690	2.656704
-66.786358	30.422236	2.666701
-65.793658	32.996453	2.676698
-65.245519	29.791524	2.686694
-65.093181	35.272467	2.696691
-64.033542	30.529689	2.706688
-63.833940	29.465601	2.716685
-63.834692	30.558365	2.726682
-62.968390	27.875808	2.736678
-62.052576	32.474158	2.746675
-61.877334	30.366080	2.756672
-61.771127	35.257221	2.766669
-60.904293	33.379738	2.776666
-60.177554	33.580447	2.786662
-60.189919	37.914749	2.796659
-59.519036	40.139228	2.806656
-58.823666	35.249655	2.816653
-58.357076	29.327850	2.826650
-57.544962	30.327663	2.836646
-57.139740	32.230507	2.846643
-56.967736	32.804915	2.856640
-56.880518	32.022552	2.866637
-56.001242	34.618135	2.876634
-55.425739	32.423953	2.886630
-54.308372	38.233142	2.896627
-54.132694	29.418016	2.906624
-53.923636	28.398447	2.916621
-53.873248	38.447867	2.926618
-52.811885	38.857069	2.936614
-52.179460	41.343599	2.946611
-52.168400	36.340219	2.956608
-51.342934	42.354911	2.966605
-50.912058	33.161357	2.976602
-50.695204	34.372157	2.986598
-49.329096	38.790200	2.996595
-48.985431	32.874337	3.006592
-49.116874	32.938362	3.016589
-48.861189	34.328651	3.026586
-47.776228	32.845164	3.036582
-47.433479	38.848852	3.046579
-46.617543	32.543729	3.056576
-46.038476	33.930459	3.066573
-46.108429	39.710998	3.076570
-45.683777	35.822366	3.086566
-44.666964	43.203236	3.096563
-44.423359	37.706785	3.106560
-43.989476	40.254379	3.116557
-43.211169	42.501064	3.126554
-43.080954	43.891000	3.136550
-42.286704	43.360934	3.146547
-41.626567	46.345978	3.156544
-41.461790	43.221542	3.166541
-41.286199	34.875487	3.176538
-40.364617	41.443916	3.186534
-39.879809	31.922930	3.196531
-38.739119	37.964305	3.206528
-38.671597	41.518866	3.216525
-38.266563	35.802769	3.226522
-38.063306	38.818076	3.236518
-37.743114	27.989272	3.246515
-36.643244	38.797794	3.256512
-36.278559	34.568795	3.266509
-35.782051	43.386830	3.276506
-35.293697	46.377890	3.286502
-35.074780	44.174431	3.296499
-34.360415	47.026741	3.306496
-33.550419	43.118283	3.316493
-33.508224	42.622467	3.326490
-32.875233	40.854953	3.336486
-31.800485	37.458534	3.346483
-31.929185	39.407389	3.356480
-31.750417	39.662458	3.366477
-30.835422	50.229746	3.376474
-30.472289	44.862451	3.386470
-29.730947	35.262864	3.396467
-29.120011	33.434442	3.406464
-28.820189	39.778415	3.416461
-28.753852	44.177849	3.426458
-27.462101	40.304461	3.436454
-27.151950	42.166666	3.446451
-27.055530	42.780040	3.456448
-26.201256	45.534452	3.466445
-25.724546	41.008228	3.476442
-25.568923	32.315147	3.486438
-24.830651	38.884980	3.496435
-23.981654	46.780531	3.506432
-23.893588	42.826318	3.516429
-23.529141	44.104793	3.526426
-22.812537	43.639965	3.536422
-22.612792	33.501785	3.546419
-21.616529	40.969427	3.556416
-21.354092	37.298151	3.566413
-21.115801	46.603921	3.576410
-20.338617	41.783804	3.586406
-19.716297	46.688341	3.596403
-19.218419	49.040000	3.606400
-18.434258	44.827665	3.616397
-18.152663	45.955362	3.626394
-18.037872	39.479250	3.636390
-17.633932	38.366824	3.646387
-16.565764	39.666653	3.656384
-16.328226	31.299545	3.666381
-15.704790	39.003890	3.676378
-14.896704	40.361814	3.686374
-14.958983	35.771357	3.696371
-14.667854	32.353554	3.706368
-13.228632	34.601703	3.716365
-13.059352	35.863041	3.726362
-13.127878	36.910256	3.736358
-12.527458	40.260437	3.746355
-11.555541	40.360575	3.756352
-11.398183	48.840331	3.766349
-10.883508	42.052119	3.776346
-9.854939	40.880325	3.786342
-9.686349	37.129976	3.796339
-9.529999	38.844732	3.806336
-8.984600	38.477395	3.816333
-8.179686	35.119349	3.826330
-8.003794	39.132670	3.836326
-6.951689	35.190725	3.846323
-6.420286	34.346367	3.856320
-6.433796	35.306206	3.866317
-5.881217	41.944366	3.876314
-5.245430	38.331756	3.886310
-4.863595	39.171487	3.896307
-4.368353	26.442447	3.906304
-3.548032	39.976017	3.916301
-3.215370	32.049062	3.926298
-3.229401	45.285390	3.936294
-2.505203	45.890738	3.946291
-2.102122	60.494523	3.956288
-1.633736	65.175628	3.966285
-0.886529	84.535087	3.976282
-0.551475	95.965144	3.986278
-0.417944	116.312028	3.996275
0.000000	109.102250	4.001280
0.106341	136.606977	4.006285
0.642505	127.577207	4.011290
0.665647	130.730017	4.016294
0.425399	134.940532	4.021299
0.570645	145.880353	4.026304
0.841688	156.467517	4.031309
0.843254	168.091597	4.036314
1.262959	165.029091	4.041318
0.753634	174.132508	4.046323
1.203311	166.128326	4.051328
1.278140	175.415192	4.056333
1.276469	174.736286	4.061338
1.410787	163.676572	4.066342
1.271358	173.190532	4.071347
1.236321	160.287509	4.076352
1.264892	157.763682	4.081357
1.094778	140.474778	4.086362
1.110984	140.752243	4.091366
0.962694	145.846216	4.096371
1.256183	156.521814	4.101376
1.218352	168.565870	4.106381
1.363875	179.406127	4.111386
1.119588	156.275144	4.116390
1.081710	157.874158	4.121395
1.417269	164.398591	4.126400
1.434849	170.879091	4.131405
1.603012	159.527784	4.136410
1.499822	150.143530	4.141414
1.392829	150.344081	4.146419
1.199761	147.757635	4.151424
0.974306	142.937757	4.156429
1.046946	138.650980	4.161434
1.219335	145.114863	4.166438
1.354375	176.300288	4.171443
1.570853	167.906577	4.176448
1.263038	163.909278	4.181453
1.479478	157.485235	4.186458
1.320530	165.661590	4.191462
1.631120	167.954872	4.196467
1.615039	156.923075	4.201472
1.263929	151.921814	4.206477
1.023446	153.300667	4.211482
1.177766	155.910904	4.216486
1.171986	171.017948	4.221491
1.413605	170.100243	4.226496
1.146168	176.308597	4.231501
1.675760	174.692175	4.236506
1.355671	173.039675	4.241510
1.461544	172.894087	4.246515
1.985212	165.596186	4.251520
1.511526	166.584723	4.256525
1.696402	171.337347	4.261530
1.892896	168.367172	4.266534
1.409068	178.987449	4.271539
1.580524	172.525058	4.276544
1.422884	173.301643	4.281549
1.426361	178.843303	4.286554
1.518045	173.427215	4.291558
1.340982	180.369431	4.296563
1.615739	177.363828	4.301568
1.529226	182.862844	4.306573
1.352666	171.516209	4.311578
1.620882	180.013741	4.316582
1.763813	198.925850	4.321587
1.802289	213.580981	4.326592
2.103557	205.142456	4.331597
1.919683	185.756480	4.336602
1.926619	173.630624	4.341606
2.071527	182.855106	4.346611
1.874938	172.537108	4.351616
1.869401	169.110791	4.356621
1.531881	169.330793	4.361626
1.896740	163.012051	4.366630
1.968961	175.932337	4.371635
1.835524	164.892995	4.376640
1.777792	169.169152	4.381645
1.603668	169.426770	4.386650
1.674397	166.762296	4.391654
1.777400	189.766021	4.396659
2.242063	196.346183	4.401664
1.878895	187.305670	4.406669
1.749474	184.840800	4.411674
2.399605	192.753140	4.416678
1.928394	178.836575	4.421683
1.893766	168.501088	4.426688
2.123595	175.889463	4.431693
2.008289	170.839954	4.436698
2.204983	169.795995	4.441702
2.011685	161.821713	4.446707
1.627512	172.499212	4.451712
1.613527	192.388875	4.456717
2.212665	194.069574	4.461722
2.796137	203.556331	4.466726
2.041243	199.450886	4.471731
1.962429	183.088021	4.476736
2.270486	195.593472	4.481741
1.939491	186.882085	4.486746
2.194881	191.870886	4.491750
1.732910	204.426448	4.496755
2.259029	202.019872	4.501760
2.174721	206.408952	4.506765
2.154848	206.540056	4.511770
2.416841	204.710363	4.516774
2.121737	199.935914	4.521779
2.275968	198.540850	4.526784
2.247256	196.768275	4.531789
2.008359	191.280040	4.536794
2.461088	197.778219	4.541798
2.080856	210.130661	4.546803
2.298164	201.436684	4.551808
2.058193	207.454348	4.556813
2.199206	210.152229	4.561818
2.256479	204.293427	4.566822
2.323130	213.861357	4.571827
2.292227	201.386670	4.576832
2.196440	198.948993	4.581837
2.262648	198.036203	4.586842
2.413004	201.236965	4.591846
2.253711	202.605167	4.596851
2.469830	196.986685	4.601856
2.539827	195.432204	4.606861
2.041987	200.192198	4.611866
2.567996	202.415257	4.616870
2.218213	211.016514	4.621875
2.286358	206.530683	4.626880
2.321560	224.872046	4.631885
2.620101	225.665884	4.636890
2.598475	228.771162	4.641894
2.832724	224.364818	4.646899
2.753749	215.256212	4.651904
2.549988	218.352124	4.656909
2.162528	201.503657	4.661914
2.785179	217.912245	4.666918
2.675124	221.476382	4.671923
2.975355	228.316362	4.676928
2.894606	220.300561	4.681933
2.604130	212.974202	4.686938
2.549969	202.276598	4.691942
2.337040	216.078273	4.696947
2.699980	218.405530	4.701952
2.818635	219.288487	4.706957
2.816825	210.534525	4.711962
2.741581	218.398445	4.716966
2.560691	214.566222	4.721971
2.679339	222.153138	4.726976
2.635333	217.102387	4.731981
2.541274	231.166094	4.736986
3.000624	235.284206	4.741990
2.711612	236.572627	4.746995
2.925499	227.327714	4.752000
2.945742	235.828274	4.757005
2.897904	236.265986	4.762010
2.902329	229.217435	4.767014
2.701816	228.031049	4.772019
2.835310	226.824882	4.777024
3.332093	228.721292	4.782029
2.590927	225.161308	4.787034
2.744393	219.509566	4.792038
2.513304	221.309119	4.797043
2.845084	237.706801	4.802048
2.872590	221.183077	4.807053
2.812861	222.108831	4.812058
2.949511	231.418663	4.817062
2.744847	240.025649	4.822067
2.962640	232.191361	4.827072
3.039495	238.091467	4.832077
2.792962	233.017058	4.837082
2.982416	237.528325	4.842086
2.695172	239.325913	4.847091
2.844357	224.544665	4.852096
2.892837	239.656029	4.857101
2.693615	236.832135	4.862106
3.409369	240.604706	4.867110
3.196116	238.005204	4.872115
2.965869	233.111011	4.877120
3.231045	243.989156	4.882125
2.894107	237.268220	4.887130
3.292925	238.136448	4.892134
3.404679	258.718799	4.897139
3.298140	240.383190	4.902144
3.096924	231.018637	4.907149
2.957421	237.773540	4.912154
3.000264	244.856235	4.917158
3.134042	261.067943	4.922163
3.046778	250.495150	4.927168
3.482363	267.358433	4.932173
2.985627	269.167362	4.937178
3.197513	258.493035	4.942182
2.950126	266.503124	4.947187
3.473824	264.264950	4.952192
3.581556	269.909084	4.957197
3.386561	262.909357	4.962202
3.448989	251.788947	4.967206
3.355749	259.513008	4.972211
3.298390	264.814856	4.977216
3.255702	265.098012	4.982221
3.125540	251.963301	4.987226
3.448894	250.856082	4.992230
3.301309	267.624346	4.997235
3.516381	253.397875	5.002240
3.188632	264.303085	5.007245
3.278044	257.550159	5.012250
3.421443	253.129816	5.017254
3.193019	263.637898	5.022259
3.089916	263.679168	5.027264
3.455580	264.113364	5.032269
3.074709	256.397926	5.037274
3.701666	278.077950	5.042278
3.891962	284.502232	5.047283
3.649109	275.761431	5.052288
3.644650	271.976989	5.057293
3.077717	264.147073	5.062298
3.396192	269.794165	5.067302
3.384271	292.931082	5.072307
3.409063	278.287247	5.077312
3.420504	300.443421	5.082317
3.422436	293.031212	5.087322
4.180513	290.044371	5.092326
3.885249	296.341920	5.097331
3.819185	281.692082	5.102336
3.745661	288.859536	5.107341
4.117883	284.139733	5.112346
4.128171	287.966549	5.117350
3.957131	266.977256	5.122355
3.776796	267.401152	5.127360
3.610344	263.043554	5.132365
3.579962	257.426521	5.137370
3.876158	255.085656	5.142374
3.676490	267.274823	5.147379
3.727596	265.662093	5.152384
3.795786	275.767285	5.157389
3.747539	287.022130	5.162394
4.293922	288.659468	5.167398
3.792757	286.976501	5.172403
3.773942	271.801709	5.177408
3.872265	278.634530	5.182413
3.679655	290.008635	5.187418
3.836586	286.118297	5.192422
3.904867	300.867440	5.197427
3.977851	297.336368	5.202432
4.198103	289.283416	5.207437
3.939619	287.018723	5.212442
4.097893	290.016443	5.217446
4.161679	297.234708	5.222451
3.971889	282.665595	5.227456
3.663803	283.533838	5.232461
3.766655	294.978986	5.237466
3.893164	289.379818	5.242470
3.563606	300.793334	5.247475
3.839202	291.104293	5.252480
4.123553	291.733653	5.257485
3.855217	297.065346	5.262490
4.015172	294.010027	5.267494
3.961137	294.594480	5.272499
3.833265	305.395557	5.277504
4.046625	292.489455	5.282509
3.500470	303.844353	5.287514
4.463243	306.522766	5.292518
4.058838	333.186557	5.297523
4.073091	327.500757	5.302528
3.914424	327.280300	5.307533
4.075520	320.902430	5.312538
4.540550	331.080296	5.317542
4.236042	330.669164	5.322547
4.363844	327.573672	5.327552
4.325210	311.515785	5.332557
4.406799	314.704948	5.337562
4.311217	321.833245	5.342566
4.244682	327.334241	5.347571
4.549888	318.354662	5.352576
4.323039	318.187894	5.357581
4.313521	315.057679	5.362586
4.512819	304.337849	5.367590
4.186558	308.203811	5.372595
4.427571	325.422018	5.377600
4.531153	312.496650	5.382605
4.227971	314.537997	5.387610
4.760827	309.266000	5.392614
4.318884	300.707352	5.397619
3.902453	307.988309	5.402624
4.284261	315.194575	5.407629
4.255102	322.065649	5.412634
4.520862	321.864139	5.417638
4.445136	322.808426	5.422643
4.484565	305.426994	5.427648
4.591485	320.905648	5.432653
4.416230	322.236740	5.437658
4.681338	318.560656	5.442662
4.337240	325.232992	5.447667
4.495359	323.368657	5.452672
4.639387	312.578536	5.457677
4.066234	336.474000	5.462682
4.506181	333.348627	5.467686
4.560360	332.497109	5.472691
4.208296	320.646522	5.477696
4.704077	322.473952	5.482701
4.438817	333.659624	5.487706
4.685392	323.329159	5.492710
4.430224	327.510128	5.497715
4.451327	321.323701	5.502720
4.667988	331.142166	5.507725
4.846211	355.541340	5.512730
5.051942	350.054056	5.517734
4.584501	336.148169	5.522739
4.611705	332.191552	5.527744
4.595254	351.993927	5.532749
4.424635	358.091544	5.537754
4.934819	346.700744	5.542758
4.710212	354.927513	5.547763
4.932939	358.422677	5.552768
4.939004	355.264130	5.557773
4.619945	352.997696	5.562778
4.637016	346.866384	5.567782
4.462792	357.150796	5.572787
5.275266	350.465292	5.577792
5.237555	341.931274	5.582797
4.846773	355.281021	5.587802
5.285219	347.421950	5.592806
4.872613	351.772884	5.597811
5.073554	353.541900	5.602816
5.170554	347.404778	5.607821
4.945661	350.966020	5.612826
5.127046	344.442624	5.617830
4.786006	342.975194	5.622835
4.778375	335.072347	5.627840
5.195460	348.743883	5.632845
4.861736	355.948646	5.637850
4.974354	341.124986	5.642854
4.863343	341.674363	5.647859
4.800455	354.396826	5.652864
5.437872	347.493315	5.657869
4.919747	347.601593	5.662874
5.042882	349.029486	5.667878
5.036639	346.990853	5.672883
5.098763	348.761499	5.677888
5.428476	344.398934	5.682893
5.124124	346.935834	5.687898
4.851172	340.776585	5.692902
5.070433	353.666999	5.697907
5.451649	331.180989	5.702912
5.418585	353.846758	5.707917
5.340759	347.775227	5.712922
5.453320	338.136284	5.717926
5.223158	342.350318	5.722931
5.132148	347.968130	5.727936
5.272887	346.306246	5.732941
4.969328	357.200815	5.737946
5.121974	345.146047	5.742950
5.183518	353.531028	5.747955
5.205434	351.531446	5.752960
4.895353	350.639099	5.757965
4.911848	350.797343	5.762970
5.371809	348.901079	5.767974
4.826222	354.926093	5.772979
5.211331	370.200580	5.777984
5.455726	380.064215	5.782989
5.357172	394.562806	5.787994
5.392761	376.945150	5.792998
5.345343	379.612442	5.798003
5.275857	383.211643	5.803008
5.571059	385.568274	5.808013
5.560333	375.663873	5.813018
5.696398	375.347451	5.818022
5.194305	383.668828	5.823027
5.504142	380.740556	5.828032
5.624843	385.219720	5.833037
5.441167	391.658494	5.838042
5.640285	393.959676	5.843046
5.491219	382.696047	5.848051
5.518855	385.413682	5.853056
5.250188	386.782611	5.858061
5.157564	384.011316	5.863066
5.163256	376.636527	5.868070
5.288388	382.049238	5.873075
5.414025	382.555266	5.878080
5.412289	386.116832	5.883085
5.586576	401.503635	5.888090
5.573196	399.763724	5.893094
5.573561	410.338771	5.898099
5.871071	413.342314	5.903104
5.870989	407.706505	5.908109
5.579994	422.189964	5.913114
5.805764	415.659399	5.918118
5.908851	414.639970	5.923123
5.555711	399.634743	5.928128
5.555408	408.037078	5.933133
5.397414	408.706690	5.938138
5.856495	404.957489	5.943142
5.258680	402.477843	5.948147
5.179939	403.847056	5.953152
5.524692	399.323547	5.958157
5.681950	410.873148	5.963162
6.074906	399.602115	5.968166
5.794720	412.685118	5.973171
5.816328	410.833860	5.978176
6.060520	407.622532	5.983181
6.046504	422.141905	5.988186
5.993347	419.801429	5.993190
5.869943	412.996095	5.998195
6.159665	408.678499	6.003200
5.603066	415.450711	6.008205
5.741702	407.415033	6.013210
6.040462	408.842717	6.018214
5.636169	417.166892	6.023219
5.627783	421.244061	6.028224
6.199940	426.224493	6.033229
5.982485	437.952454	6.038234
6.240055	414.471968	6.043238
5.928890	421.274064	6.048243
5.996983	423.880444	6.053248
5.765446	409.143190	6.058253
5.785814	413.632630	6.063258
6.040573	417.674205	6.068262
6.063241	413.579013	6.073267
5.860250	417.096202	6.078272
6.111099	413.039761	6.083277
6.052393	419.744789	6.088282
6.146292	408.107331	6.093286
5.858862	422.606183	6.098291
5.782285	416.234797	6.103296
6.054256	415.231164	6.108301
5.844032	417.915501	6.113306
6.138501	410.868165	6.118310
6.077530	414.949584	6.123315
6.143125	407.637294	6.128320
6.104446	412.041189	6.133325
5.846005	412.892651	6.138330
6.224752	407.534408	6.143334
6.009469	414.698611	6.148339
5.664687	417.303174	6.153344
6.057508	410.698439	6.158349
6.095903	419.422617	6.163354
6.303819	414.130981	6.168358
6.483297	417.511563	6.173363
6.202587	413.541289	6.178368
6.014209	400.016412	6.183373
5.646022	391.237950	6.188378
6.090199	405.292288	6.193382
5.997934	399.108385	6.198387
6.143546	397.393304	6.203392
6.140592	384.953608	6.208397
5.673752	380.012833	6.213402
5.871618	367.004159	6.218406
5.890760	394.063820	6.223411
5.727288	382.318462	6.228416
6.135582	397.204382	6.233421
5.712584	394.989550	6.238426
5.864753	393.217447	6.243430
5.927967	410.545537	6.248435
5.937760	410.980143	6.253440
6.124162	408.330055	6.258445
5.877756	411.023231	6.263450
6.080118	401.718063	6.268454
5.521330	405.433942	6.273459
5.860692	410.353986	6.278464
5.664516	418.205238	6.283469
5.382182	410.961987	6.288474
5.992234	408.875760	6.293478
5.967283	417.975239	6.298483
5.801926	422.151258	6.303488
5.701944	420.967184	6.308493
5.830002	419.398449	6.313498
5.976759	421.047482	6.318502
5.908708	420.878247	6.323507
5.877523	412.972050	6.328512
6.413961	421.402403	6.333517
6.046716	414.063477	6.338522
6.237955	410.140702	6.343526
6.178890	423.125018	6.348531
6.257165	419.226533	6.353536
6.307978	417.741300	6.358541
5.830753	410.687615	6.363546
6.200335	382.249895	6.368550
5.710519	393.956140	6.373555
5.850871	396.066168	6.378560
6.087136	381.284486	6.383565
5.864351	390.572521	6.388570
6.049052	395.916692	6.393574
5.766482	396.040600	6.398579
5.910661	390.123266	6.403584
5.896348	389.158558	6.408589
5.769832	403.001665	6.413594
6.205020	401.677456	6.418598
5.930569	396.192457	6.423603
6.137510	397.795138	6.428608
6.088848	383.545538	6.433613
5.576334	385.665390	6.438618
5.731402	387.149967	6.443622
6.053822	396.389046	6.448627
6.049956	396.486331	6.453632
5.860208	391.409588	6.458637
5.667773	401.240456	6.463642
6.046541	415.927744	6.468646
6.041962	413.281395	6.473651
5.863460	408.056282	6.478656
5.960579	410.661711	6.483661
5.765477	417.202323	6.488666
6.148618	420.165473	6.493670
6.128246	412.447010	6.498675
6.272223	401.099423	6.503680
6.022426	386.304831	6.508685
5.712195	389.460104	6.513690
6.010702	383.304860	6.518694
5.813062	384.450926	6.523699
5.899968	386.914689	6.528704
6.006396	381.471132	6.533709
6.045261	388.208364	6.538714
5.913448	377.890375	6.543718
6.016251	391.641412	6.548723
5.938899	380.070456	6.553728
5.967528	378.097483	6.558733
6.074708	393.502668	6.563738
6.083095	384.276822	6.568742
5.616321	384.653050	6.573747
5.774873	387.231452	6.578752
6.022279	383.294272	6.583757
5.977178	382.131913	6.588762
5.955567	379.797477	6.593766
5.724746	381.502786	6.598771
5.996012	366.908110	6.603776
6.366823	379.629956	6.608781
6.026755	377.322693	6.613786
5.711937	374.361997	6.618790
6.015712	389.225226	6.623795
6.190005	383.570870	6.628800
6.101498	381.889054	6.633805
5.860658	382.841689	6.638810
6.476387	386.178979	6.643814
6.341585	383.575465	6.648819
6.164331	382.514167	6.653824
6.430501	387.113825	6.658829
5.830800	367.729151	6.663834
5.864057	365.117105	6.668838
6.038848	360.620511	6.673843
5.897482	368.281053	6.678848
6.122221	362.358408	6.683853
5.645403	364.567660	6.688858
5.897711	361.807440	6.693862
5.737888	377.675433	6.698867
6.072365	368.964465	6.703872
5.947522	378.042051	6.708877
5.916171	381.222367	6.713882
6.306822	372.489387	6.718886
5.802894	369.246413	6.723891
5.916701	354.533829	6.728896
6.086428	360.577571	6.733901
5.662309	370.895989	6.738906
6.270070	359.536015	6.743910
5.836784	357.929923	6.748915
5.729306	340.059714	6.753920
6.165383	356.508755	6.758925
6.107768	359.010801	6.763930
6.026963	345.023254	6.768934
6.025825	346.085739	6.773939
5.948769	341.395869	6.778944
5.961024	340.012021	6.783949
6.034119	344.280221	6.788954
5.995941	339.639667	6.793958
5.853031	347.092387	6.798963
5.633708	349.861285	6.803968
5.793535	349.870450	6.808973
5.578174	353.328995	6.813978
5.856250	356.139312	6.818982
5.918447	368.635220	6.823987
6.019800	371.836717	6.828992
6.249855	369.012099	6.833997
6.077895	366.621711	6.839002
6.032269	350.002990	6.844006
6.003240	346.796870	6.849011
6.026002	343.515796	6.854016
6.085769	349.814876	6.859021
5.752373	352.695659	6.864026
6.033327	345.409766	6.869030
5.840084	342.442502	6.874035
5.713949	347.742229	6.879040
6.014565	349.544791	6.884045
5.947831	349.611326	6.889050
5.873845	341.862197	6.894054
5.710075	344.591725	6.899059
5.834561	349.709154	6.904064
5.873562	375.998741	6.909069
5.832968	381.711034	6.914074
6.115606	375.699890	6.919078
6.024701	378.607198	6.924083
6.035927	372.728811	6.929088
6.314864	352.884832	6.934093
5.809505	357.865529	6.939098
5.889447	346.660961	6.944102
5.763101	344.632113	6.949107
5.659469	345.154521	6.954112
5.684874	363.043158	6.959117
5.897816	373.399943	6.964122
6.262196	368.778094	6.969126
6.358035	374.916727	6.974131
5.993518	363.762709	6.979136
5.958609	349.071056	6.984141
6.114218	355.472885	6.989146
5.733840	348.593730	6.994150
5.989524	348.366360	6.999155
5.753007	353.285362	7.004160
6.050818	348.820927	7.009165
5.860388	348.284097	7.014170
5.900649	342.708041	7.019174
5.739302	350.689156	7.024179
5.803319	351.503704	7.029184
6.346648	351.404900	7.034189
5.890227	351.073035	7.039194
5.886063	348.434718	7.044198
5.883551	356.358214	7.049203
6.093852	351.914850	7.054208
5.917659	348.928686	7.059213
5.613040	339.119639	7.064218
5.740172	341.503742	7.069222
6.129312	359.277905	7.074227
5.990373	363.262587	7.079232
5.777146	354.243466	7.084237
5.697196	357.763197	7.089242
6.125439	366.004220	7.094246
6.250102	362.251002	7.099251
6.162140	362.293914	7.104256
6.033522	339.166821	7.109261
5.896674	351.137804	7.114266
5.896733	352.617114	7.119270
6.082127	355.637002	7.124275
5.948754	353.737667	7.129280
6.213513	349.320326	7.134285
6.030073	339.786139	7.139290
6.344925	339.777972	7.144294
5.756651	337.498020	7.149299
5.929840	334.789849	7.154304
5.880643	344.295219	7.159309
5.686899	351.329355	7.164314
5.862688	337.352784	7.169318
5.792053	342.374202	7.174323
5.958156	351.677760	7.179328
5.928556	337.226852	7.184333
5.582935	345.246309	7.189338
5.706462	336.839157	7.194342
5.450308	343.149303	7.199347
5.938434	372.833333	7.204352
6.357029	365.736895	7.209357
5.945360	363.246719	7.214362
6.006733	343.528680	7.219366
5.845214	349.220792	7.224371
6.086372	357.298769	7.229376
5.872381	349.119544	7.234381
5.742669	351.234338	7.239386
6.077605	358.399832	7.244390
5.849456	360.199112	7.249395
5.853756	369.593251	7.254400
6.184808	368.941730	7.259405
5.532371	362.537771	7.264410
6.029664	369.409671	7.269414
5.933157	371.883320	7.274419
6.098931	377.224497	7.279424
6.009215	368.452810	7.284429
5.963065	357.407094	7.289434
5.876768	348.873800	7.294438
5.728073	358.716749	7.299443
5.798037	373.784345	7.304448
5.796582	380.745380	7.309453
5.904704	381.657513	7.314458
6.134395	378.428264	7.319462
6.263422	383.040324	7.324467
5.999037	381.105710	7.329472
6.106400	347.794034	7.334477
5.728268	359.820682	7.339482
5.810230	345.555845	7.344486
5.829763	360.869031	7.349491
6.186422	369.539007	7.354496
6.086922	359.338617	7.359501
5.751888	359.603197	7.364506
5.913015	348.082534	7.369510
5.924608	356.305983	7.374515
5.861953	367.082612	7.379520
6.089207	367.228028	7.384525
5.890117	357.504232	7.389530
5.788767	354.249191	7.394534
5.959054	350.203416	7.399539
6.152856	362.471673	7.404544
5.969920	359.503294	7.409549
5.936737	352.712773	7.414554
5.639511	349.549297	7.419558
5.918875	358.694148	7.424563
5.937779	374.961759	7.429568
6.323749	371.726515	7.434573
6.044086	354.380987	7.439578
5.895606	349.875764	7.444582
5.723059	345.507805	7.449587
5.607198	340.975686	7.454592
5.920126	363.320977	7.459597
6.158854	377.631219	7.464602
6.213947	363.605312	7.469606
6.052509	347.821525	7.474611
5.832405	364.838063	7.479616
6.253816	342.003352	7.484621
6.207346	353.432278	7.489626
6.187796	352.117024	7.494630
6.152373	351.907473	7.499635
6.039293	345.391500	7.504640
5.960841	341.224543	7.509645
6.062896	351.328333	7.514650
5.836870	348.000370	7.519654
6.024967	341.506153	7.524659
5.752645	354.148390	7.529664
6.016399	348.065596	7.534669
5.605717	359.695597	7.539674
6.184183	351.293661	7.544678
5.857795	349.929371	7.549683
5.906853	354.288068	7.554688
6.112735	349.211368	7.559693
6.188450	351.423625	7.564698
5.640942	338.684066	7.569702
5.895561	351.542886	7.574707
5.516590	343.169345	7.579712
5.617987	351.403602	7.584717
5.595870	341.230786	7.589722
5.918590	332.805616	7.594726
5.885707	343.086887	7.599731
5.823403	349.188306	7.604736
5.725798	348.227204	7.609741
5.904709	367.443653	7.614746
6.185631	375.503032	7.619750
5.882921	354.516831	7.624755
5.664891	349.589604	7.629760
6.237975	361.132307	7.634765
5.929423	357.281978	7.639770
6.028656	352.541760	7.644774
5.990862	344.770863	7.649779
5.798800	348.936871	7.654784
6.167847	344.253979	7.659789
5.622916	354.062467	7.664794
5.786463	354.810252	7.669798
6.285965	360.566371	7.674803
6.027521	371.300182	7.679808
6.197060	351.496579	7.684813
5.925202	366.940699	7.689818
5.789189	355.337526	7.694822
6.144358	354.792812	7.699827
6.171992	346.359770	7.704832
6.147930	350.606933	7.709837
6.089429	351.263553	7.714842
5.806134	340.058443	7.719846
5.961469	345.601015	7.724851
5.846785	352.350484	7.729856
6.113476	345.643399	7.734861
5.756607	349.991731	7.739866
5.794391	344.664107	7.744870
5.901633	338.622966	7.749875
5.669286	358.255821	7.754880
6.114764	334.010892	7.759885
5.870504	352.891973	7.764890
5.856948	344.725700	7.769894
5.970169	353.208690	7.774899
5.852942	352.339326	7.779904
5.975101	348.874010	7.784909
5.802759	354.073839	7.789914
5.877107	346.883453	7.794918
6.028397	339.752867	7.799923
6.054895	344.195201	7.804928
6.479499	342.653728	7.809933
5.935816	348.976172	7.814938
6.149747	350.186814	7.819942
5.964896	355.855160	7.824947
6.065403	340.262304	7.829952
6.008526	341.964712	7.834957
5.800824	346.883489	7.839962
5.702976	346.289233	7.844966
5.615710	343.684381	7.849971
5.783826	353.125727	7.854976
5.830407	349.127230	7.859981
5.565144	362.227949	7.864986
5.638695	358.156920	7.869990
5.656524	365.855575	7.874995
5.817903	370.843396	7.880000
6.423197	374.376367	7.885005
5.959393	375.987781	7.890010
5.545261	362.888854	7.895014
6.080966	369.879799	7.900019
5.810530	374.564184	7.905024
5.968467	372.020325	7.910029
6.110039	385.348913	7.915034
5.886625	383.481423	7.920038
5.883935	377.653182	7.925043
6.135975	387.407529	7.930048
5.944987	367.640203	7.935053
5.699410	381.505827	7.940058
5.911799	371.666765	7.945062
5.989259	392.268282	7.950067
5.666851	378.818453	7.955072
6.092716	383.970933	7.960077
5.917317	383.604958	7.965082
5.979434	387.298532	7.970086
6.096465	386.185641	7.975091
5.998307	381.918241	7.980096
5.811777	369.098187	7.985101
5.769454	378.705242	7.990106
6.070039	371.951996	7.995110
6.096166	384.604132	8.000115
5.753956	384.535465	8.005133
5.847309	376.569058	8.010150
5.883925	391.630284	8.015168
6.007092	383.312362	8.020186
6.263316	376.191106	8.025203
5.863623	366.687418	8.030221
6.197447	365.959123	8.035238
5.979987	361.020252	8.040256
5.801827	350.257576	8.045274
5.875950	364.434510	8.050291
5.739118	373.698605	8.055309
6.240981	368.526905	8.060326
6.223939	383.196579	8.065344
6.128144	360.480687	8.070362
5.954636	357.290100	8.075379
5.599157	366.937694	8.080397
5.838751	358.629870	8.085414
5.894329	376.430399	8.090432
5.929911	381.297604	8.095450
6.034564	381.640927	8.100467
6.221881	391.193521	8.105485
6.276949	384.019695	8.110502
6.287719	388.972286	8.115520
6.147103	382.353330	8.120538
5.971382	379.973569	8.125555
5.970816	380.487398	8.130573
6.038854	383.223886	8.135590
6.177009	389.385687	8.140608
6.302567	377.444388	8.145626
6.205217	352.952453	8.150643
5.621435	362.672608	8.155661
6.194737	375.453744	8.160678
6.073333	373.737903	8.165696
5.985901	380.308952	8.170714
6.065727	382.032181	8.175731
5.983917	389.620504	8.180749
5.767567	391.584668	8.185766
5.632426	387.160522	8.190784
6.085532	386.567797	8.195802
6.380482	386.570877	8.200819
5.912105	384.817904	8.205837
6.351382	385.790140	8.210854
6.006224	375.983301	8.215872
6.231073	390.017361	8.220890
6.456697	389.845321	8.225907
6.177099	383.059706	8.230925
6.255065	379.654265	8.235942
6.065106	381.044989	8.240960
6.119615	388.385928	8.245978
6.128579	381.136274	8.250995
5.923539	393.935543	8.256013
6.111555	383.356180	8.261030
6.179108	385.555061	8.266048
6.009325	387.211000	8.271066
5.795398	375.012778	8.276083
5.874697	388.977307	8.281101
6.022428	393.981168	8.286118
6.032410	406.802383	8.291136
6.225022	419.139976	8.296154
6.492709	415.630945	8.301171
6.390702	416.630933	8.306189
6.301547	410.553744	8.311206
6.227451	404.229433	8.316224
6.133119	405.044823	8.321242
6.332630	417.736616	8.326259
6.309330	414.550913	8.331277
6.265704	412.283148	8.336294
6.296731	413.244226	8.341312
6.392563	402.158732	8.346330
6.332655	397.542265	8.351347
6.208870	394.349259	8.356365
6.285352	397.959767	8.361382
6.326443	392.572630	8.366400
6.449844	397.250068	8.371418
6.613977	397.746915	8.376435
6.049477	386.515490	8.381453
6.302019	383.065748	8.386470
6.121387	380.814529	8.391488
6.491748	402.924780	8.396506
6.418911	392.785387	8.401523
6.284488	395.855962	8.406541
6.111152	399.397934	8.411558
6.060703	405.878648	8.416576
6.214268	407.765348	8.421594
6.911901	406.996413	8.426611
6.040302	413.189195	8.431629
6.503088	407.149116	8.436646
6.467994	426.283810	8.441664
6.310285	412.505126	8.446682
6.746373	416.085536	8.451699
6.390049	422.878268	8.456717
6.694044	419.349557	8.461734
6.506480	405.986262	8.466752
5.920338	396.077235	8.471770
6.338265	400.152865	8.476787
6.184917	403.290336	8.481805
6.349210	406.722096	8.486822
6.463077	405.819561	8.491840
6.167998	416.450114	8.496858
6.221477	413.273470	8.501875
5.963540	417.851368	8.506893
6.210200	408.373785	8.511910
6.407203	415.965248	8.516928
5.922813	417.496542	8.521946
6.324219	423.400724	8.526963
6.507816	438.271204	8.531981
6.871696	451.130016	8.536998
6.596018	436.178129	8.542016
6.483168	424.362395	8.547034
6.287497	420.103724	8.552051
6.490429	440.010256	8.557069
6.697947	443.430649	8.562087
6.244131	432.648523	8.567104
6.376717	442.163057	8.572122
6.835706	443.785550	8.577139
6.638553	456.711004	8.582157
6.567795	447.554008	8.587175
6.684899	439.203896	8.592192
6.577599	423.112017	8.597210
6.346599	411.034477	8.602227
6.514526	433.754194	8.607245
6.365846	445.075194	8.612263
6.847897	441.317782	8.617280
6.406727	435.530403	8.622298
6.866793	442.197381	8.627315
6.760428	449.481388	8.632333
6.603605	435.631488	8.637351
6.452408	427.561303	8.642368
6.470100	442.688194	8.647386
6.781299	445.409012	8.652403
6.651061	456.759348	8.657421
6.646831	449.156500	8.662439
6.910979	447.832356	8.667456
6.508743	442.496126	8.672474
6.649615	429.602347	8.677491
6.711840	442.736351	8.682509
6.427424	438.481220	8.687527
6.497448	423.585874	8.692544
6.567878	440.498767	8.697562
6.883261	444.509088	8.702579
6.931726	454.015981	8.707597
6.806363	450.351467	8.712615
6.951908	439.278691	8.717632
6.240413	440.970919	8.722650
6.273682	431.225006	8.727667
6.819891	444.690365	8.732685
6.842813	450.303532	8.737703
6.935314	442.676239	8.742720
6.686515	447.075996	8.747738
6.545294	441.373468	8.752755
6.624534	452.565980	8.757773
6.615799	446.067793	8.762791
6.763447	455.648632	8.767808
6.498843	452.525332	8.772826
6.421495	443.499520	8.777843
6.751369	455.433432	8.782861
6.644176	456.025897	8.787879
6.632270	455.921352	8.792896
6.529735	450.726892	8.797914
6.726747	444.637431	8.802931
6.683083	452.280886	8.807949
6.821406	449.606941	8.812967
6.941143	441.400262	8.817984
6.505714	465.058837	8.823002
6.688555	448.653485	8.828019
6.648691	458.169860	8.833037
6.525543	466.089299	8.838055
7.008939	478.412244	8.843072
7.042810	481.104504	8.848090
7.092292	483.030456	8.853107
6.952751	474.463733	8.858125
7.055560	466.157889	8.863143
7.047080	454.822916	8.868160
6.639714	458.530323	8.873178
6.772226	439.549361	8.878195
6.885263	459.930919	8.883213
7.116988	467.362861	8.888231
7.126597	456.591320	8.893248
6.992927	451.208737	8.898266
7.036829	444.106891	8.903283
6.960294	444.973564	8.908301
7.245992	451.685894	8.913319
6.932250	444.500167	8.918336
6.896912	461.780296	8.923354
7.112112	447.205159	8.928371
6.837873	454.867137	8.933389
6.823212	445.903784	8.938407
7.063339	446.645011	8.943424
6.888650	450.645887	8.948442
7.049832	447.032525	8.953459
6.895438	452.387454	8.958477
6.791388	452.986583	8.963495
6.942901	444.313915	8.968512
6.726936	449.189057	8.973530
7.144086	451.902699	8.978547
6.862825	448.586818	8.983565
6.327961	457.296883	8.988583
6.944760	465.207601	8.993600
7.137115	481.114364	8.998618
7.199755	473.275792	9.003635
7.294435	473.154519	9.008653
7.228705	478.630703	9.013671
7.399707	457.913384	9.018688
6.858060	453.691901	9.023706
6.806529	457.044500	9.028723
6.739092	456.204889	9.033741
6.991419	469.613149	9.038759
7.330460	472.745331	9.043776
7.589528	469.900672	9.048794
7.524213	462.668765	9.053811
7.230926	454.051787	9.058829
7.167226	450.729670	9.063847
7.005344	444.862675	9.068864
6.713161	457.460496	9.073882
6.678946	449.197381	9.078899
6.916985	456.917095	9.083917
6.814068	470.421062	9.088935
7.055840	467.081033	9.093952
7.123486	480.264852	9.098970
7.151199	471.626306	9.103987
6.886144	472.683454	9.109005
7.040179	472.904566	9.114023
7.307431	468.467825	9.119040
7.032551	475.509569	9.124058
7.049274	476.846563	9.129075
7.022270	470.373033	9.134093
6.822621	481.677488	9.139111
7.239946	484.762392	9.144128
7.120829	479.580700	9.149146
7.050894	475.851520	9.154163
7.310213	477.712387	9.159181
6.943140	477.585351	9.164199
7.520804	496.797575	9.169216
7.073649	486.090082	9.174234
7.233961	488.880125	9.179251
7.196190	494.906311	9.184269
7.289596	507.523113	9.189287
7.257900	505.933054	9.194304
6.955405	515.083299	9.199322
7.408129	511.260259	9.204339
7.507044	522.205425	9.209357
7.084089	512.659042	9.214375
7.337159	511.908561	9.219392
7.377212	516.359699	9.224410
7.582769	508.767616	9.229427
7.784417	505.828030	9.234445
7.521978	494.336216	9.239463
7.379513	467.313764	9.244480
7.324156	472.647709	9.249498
7.285728	478.398067	9.254515
7.388415	474.728039	9.259533
7.009067	476.351210	9.264551
7.302095	479.585861	9.269568
7.340236	494.881241	9.274586
7.560030	504.817046	9.279603
7.531824	494.442301	9.284621
7.492672	489.209997	9.289639
7.602850	477.685451	9.294656
7.490554	477.426565	9.299674
7.141936	485.256921	9.304691
7.225491	479.740023	9.309709
7.288163	487.746655	9.314727
7.486382	491.908609	9.319744
7.947441	500.254057	9.324762
7.381949	483.207031	9.329779
7.342589	479.561166	9.334797
7.170003	478.468413	9.339815
7.597415	494.561399	9.344832
7.573710	498.347807	9.349850
7.532760	489.799027	9.354867
7.615786	469.827386	9.359885
7.559540	481.911725	9.364903
7.610150	473.546899	9.369920
7.550060	480.012606	9.374938
7.602618	477.596089	9.379955
7.350897	474.659989	9.384973
7.309214	474.851646	9.389991
7.468805	478.734996	9.395008
7.459153	485.068084	9.400026
7.391077	500.773859	9.405043
7.678420	506.583755	9.410061
7.498908	517.891502	9.415079
7.916016	502.871216	9.420096
7.358130	506.086286	9.425114
7.583439	502.898351	9.430131
7.893166	499.906365	9.435149
7.525533	487.591848	9.440167
7.400727	476.726387	9.445184
7.251328	489.770625	9.450202
7.259400	502.943643	9.455219
7.481732	501.404106	9.460237
7.736246	506.732515	9.465255
7.566360	498.687523	9.470272
7.566937	515.269983	9.475290
7.594804	507.669083	9.480307
8.138075	505.248816	9.485325
7.630465	515.569646	9.490343
7.920258	504.954781	9.495360
7.614688	505.410772	9.500378
7.622855	522.572876	9.505395
7.707414	509.178494	9.510413
7.073358	517.185342	9.515431
7.502797	505.731613	9.520448
7.491827	515.969682	9.525466
7.473729	516.345692	9.530483
7.774991	510.602686	9.535501
7.713253	511.618462	9.540519
7.682132	508.521613	9.545536
7.758323	510.032211	9.550554
7.636933	515.922647	9.555571
8.022858	504.918740	9.560589
7.682613	510.867678	9.565607
7.528142	506.168302	9.570624
7.697346	508.201515	9.575642
7.595655	509.991952	9.580659
8.066944	506.015874	9.585677
7.676747	511.042836	9.590695
7.654791	510.590118	9.595712
7.580176	514.586675	9.600730
7.880185	531.087096	9.605747
8.052730	542.362562	9.610765
7.754561	525.247400	9.615783
7.555854	528.447205	9.620800
7.867423	531.882799	9.625818
7.790125	539.944374	9.630835
7.873105	547.379976	9.635853
7.748984	549.142438	9.640871
7.836794	550.849212	9.645888
7.874603	551.707622	9.650906
7.805978	551.078005	9.655923
8.220818	542.992353	9.660941
7.844699	550.847362	9.665959
7.988849	557.146402	9.670976
8.061627	549.841742	9.675994
8.067444	542.273992	9.681011
8.061481	539.838500	9.686029
7.938784	536.266224	9.691047
7.798892	532.999290	9.696064
8.158192	537.860382	9.701082
7.835427	539.257125	9.706099
7.734439	533.308689	9.711117
7.719811	544.956459	9.716135
7.767430	543.346794	9.721152
7.961987	538.755149	9.726170
7.995010	550.043148	9.731187
8.427201	541.098692	9.736205
7.952934	540.632352	9.741223
7.963395	533.656243	9.746240
8.137370	543.084193	9.751258
8.411707	539.676279	9.756275
8.228566	548.216088	9.761293
7.956703	530.341896	9.766311
7.489231	524.349322	9.771328
8.062538	545.398389	9.776346
7.744390	545.521977	9.781363
8.135277	546.709169	9.786381
7.614162	553.016396	9.791399
7.776466	546.749988	9.796416
7.945809	550.479904	9.801434
7.922206	550.613466	9.806451
8.161022	546.669301	9.811469
7.950103	552.796156	9.816487
8.332567	548.627404	9.821504
8.120061	549.528853	9.826522
8.119634	550.150322	9.831539
8.043497	542.784956	9.836557
7.910042	548.518668	9.841575
7.936230	553.634185	9.846592
7.991302	556.308193	9.851610
7.973332	580.648601	9.856627
8.010571	575.376877	9.861645
7.881889	584.368937	9.866663
7.840640	584.221809	9.871680
8.732292	575.264778	9.876698
8.458778	581.822873	9.881715
8.460683	582.724318	9.886733
8.348896	582.646906	9.891751
8.294057	584.016696	9.896768
8.092048	573.782115	9.901786
8.116684	585.062964	9.906803
8.623825	591.615654	9.911821
8.348411	579.436681	9.916839
8.321966	580.380697	9.921856
8.396309	563.075021	9.926874
8.136846	560.424676	9.931891
8.298199	561.004059	9.936909
8.191172	575.647063	9.941927
8.099728	574.308655	9.946944
8.546949	578.829998	9.951962
8.375388	580.631695	9.956979
8.321971	582.708595	9.961997
8.442731	589.165029	9.967015
8.353347	571.354611	9.972032
8.555945	567.611861	9.977050
8.240246	558.302204	9.982067
8.282737	549.205748	9.987085
8.367387	562.057363	9.992103
8.021912	568.618095	9.997120
8.199802	573.384102	10.002138
8.159543	573.962263	10.007155
8.449721	569.757092	10.012173
8.591324	578.327684	10.017191
8.378648	574.083589	10.022208
8.745669	568.202651	10.027226
7.891315	582.897720	10.032243
8.391982	573.191875	10.037261
8.493008	579.985656	10.042279
8.725922	575.449658	10.047296
8.747996	576.943226	10.052314
8.581280	584.754692	10.057331
8.541626	575.196689	10.062349
8.694407	580.817179	10.067367
8.662628	579.671333	10.072384
8.706129	559.826950	10.077402
8.303904	554.466470	10.082419
8.392503	551.798954	10.087437
8.570739	567.804087	10.092455
8.626516	570.364026	10.097472
8.875678	574.268123	10.102490
8.272454	560.346830	10.107507
8.398860	556.977628	10.112525
8.511788	567.353394	10.117543
8.835785	568.171892	10.122560
8.762139	558.621682	10.127578
8.353468	557.941390	10.132595
8.546355	565.416208	10.137613
8.542195	569.150003	10.142631
8.513607	565.712139	10.147648
8.589912	567.367775	10.152666
8.611971	579.374400	10.157683
8.513022	573.832128	10.162701
8.604803	572.700404	10.167719
8.375884	577.490637	10.172736
8.669690	574.147497	10.177754
8.651992	572.644962	10.182771
8.475248	583.572156	10.187789
8.435102	585.567155	10.192807
8.117109	576.871430	10.197824
8.588953	572.057509	10.202842
8.734515	574.948314	10.207859
8.541031	578.496805	10.212877
8.642015	575.500627	10.217895
8.649854	588.073478	10.222912
8.733249	581.530781	10.227930
8.472642	586.968750	10.232947
8.576445	599.727287	10.237965
8.807585	596.607155	10.242983
8.507955	609.039433	10.248000
9.114849	598.595878	10.253018
9.087485	598.070443	10.258035
8.792989	588.101876	10.263053
8.712098	582.535262	10.268071
8.654175	576.181441	10.273088
8.852619	586.680760	10.278106
8.685490	588.442658	10.283123
8.743373	600.527221	10.288141
8.873675	593.797864	10.293159
8.895798	604.435564	10.298176
8.892004	603.801923	10.303194
8.859438	591.450353	10.308211
8.807392	591.131026	10.313229
8.594922	590.388689	10.318247
8.821502	601.170124	10.323264
9.058470	592.398622	10.328282
9.013709	586.444809	10.333299
8.966140	597.461471	10.338317
9.060992	594.538238	10.343335
8.898432	596.371514	10.348352
9.050278	589.422203	10.353370
9.048856	593.458446	10.358387
8.988525	604.103474	10.363405
9.025620	590.784667	10.368423
8.779606	593.185074	10.373440
9.067087	599.108544	10.378458
8.891563	604.688827	10.383475
8.875411	603.070308	10.388493
9.378002	596.175608	10.393511
8.676152	596.907286	10.398528
9.056238	596.978761	10.403546
8.998652	602.511311	10.408563
8.932086	595.583625	10.413581
8.964912	595.092625	10.418599
8.824189	594.671438	10.423616
9.189075	601.882167	10.428634
8.921098	601.003262	10.433651
8.849444	596.698854	10.438669
8.897829	595.201831	10.443687
8.913553	594.555026	10.448704
9.290915	582.544992	10.453722
9.184999	592.007319	10.458739
9.115580	592.899098	10.463757
8.965796	596.034740	10.468775
8.840949	600.487665	10.473792
8.976056	597.602653	10.478810
9.000786	602.066089	10.483827
8.876822	605.816936	10.488845
9.131255	586.793798	10.493863
8.903104	598.047646	10.498880
9.005190	604.508451	10.503898
8.948000	603.718606	10.508915
8.890650	616.840636	10.513933
9.342642	617.948850	10.518951
9.171013	626.210966	10.523968
9.295921	631.468925	10.528986
9.237807	618.729010	10.534003
9.176510	639.737929	10.539021
9.403751	629.811634	10.544039
8.967134	633.961433	10.549056
9.510401	629.012092	10.554074
9.075119	630.187325	10.559091
8.681432	643.676810	10.564109
9.241723	633.593525	10.569127
9.027757	636.068942	10.574144
9.281497	629.859719	10.579162
9.378149	631.202707	10.584179
9.396102	638.941663	10.589197
9.576981	629.962913	10.594215
9.368731	631.407262	10.599232
9.506949	633.346615	10.604250
9.268409	633.004180	10.609267
9.389950	634.145552	10.614285
9.551486	628.092978	10.619303
9.333722	637.275840	10.624320
9.318987	638.278051	10.629338
9.481772	647.496733	10.634355
9.652139	642.368310	10.639373
9.801323	644.539666	10.644391
9.303952	646.332626	10.649408
9.561165	638.356816	10.654426
9.319902	634.193300	10.659443
9.393126	633.206540	10.664461
9.550908	634.746868	10.669479
9.613045	643.565821	10.674496
9.506713	632.360351	10.679514
9.301103	627.898282	10.684531
9.238399	631.648754	10.689549
9.541890	631.116664	10.694567
9.302688	632.729780	10.699584
9.435276	639.067175	10.704602
9.528908	637.356705	10.709619
9.353706	639.589049	10.714637
9.721337	638.190515	10.719655
9.605959	643.234100	10.724672
9.619229	644.081908	10.729690
9.479748	646.865529	10.734707
9.461190	640.626414	10.739725
9.643514	631.049603	10.744743
9.504680	639.209080	10.749760
9.414426	634.795748	10.754778
9.429223	634.918636	10.759795
9.507963	629.070948	10.764813
9.503947	627.501986	10.769831
9.241700	636.376608	10.774848
9.377578	634.232268	10.779866
9.460055	638.616599	10.784883
9.520940	646.153323	10.789901
9.608129	648.800783	10.794919
9.478223	661.870483	10.799936
9.637099	657.621842	10.804954
9.790927	658.480373	10.809971
9.413016	672.221461	10.814989
9.598004	663.694587	10.820007
9.432984	661.624275	10.825024
9.676187	667.883178	10.830042
9.706051	661.707495	10.835059
9.406232	663.934161	10.840077
9.743562	650.912768	10.845095
9.853203	665.952453	10.850112
9.751610	661.871635	10.855130
9.886446	652.723053	10.860147
9.618724	656.543035	10.865165
9.748592	656.830238	10.870183
9.660307	667.550389	10.875200
9.677080	663.409466	10.880218
9.841294	661.244793	10.885235
9.766502	662.330834	10.890253
9.594054	668.653801	10.895271
9.966993	680.830529	10.900288
10.132350	674.391746	10.905306
10.099349	663.970149	10.910323
9.758426	669.351354	10.915341
9.915167	666.748626	10.920359
9.747819	672.336339	10.925376
9.772040	664.539348	10.930394
9.953775	670.477467	10.935411
9.814253	671.096833	10.940429
10.082166	671.704074	10.945447
9.938868	669.462191	10.950464
9.842690	656.541561	10.955482
10.086075	674.286403	10.960499
9.826306	673.684236	10.965517
9.958217	682.319271	10.970535
10.252180	696.861584	10.975552
9.928131	684.620892	10.980570
9.840528	679.051219	10.985587
10.154079	695.383960	10.990605
9.966453	694.822026	10.995623
10.045702	693.290173	11.000640
10.264943	690.717952	11.005658
10.221170	681.996532	11.010675
9.863750	672.318277	11.015693
10.189083	666.350410	11.020711
10.094879	671.416288	11.025728
10.147320	668.543448	11.030746
10.029906	671.585878	11.035763
9.723209	670.246524	11.040781
10.145083	687.429896	11.045799
10.186471	689.859679	11.050816
9.995236	699.535445	11.055834
10.617519	689.304896	11.060851
10.197456	696.661231	11.065869
10.261289	684.790710	11.070887
9.935360	674.127213	11.075904
10.320673	691.079076	11.080922
10.422742	681.991394	11.085939
10.102071	673.850187	11.090957
10.116614	666.412307	11.095975
9.972675	681.669962	11.100992
9.795971	700.163954	11.106010
10.467496	690.024953	11.111027
10.109149	704.319625	11.116045
10.404104	692.247449	11.121063
10.092798	704.248545	11.126080
10.242322	695.416153	11.131098
10.209409	694.398021	11.136115
10.215472	692.497133	11.141133
10.124531	701.520616	11.146151
10.523771	695.464750	11.151168
10.324487	703.665052	11.156186
10.300477	697.105121	11.161203
10.398379	702.912252	11.166221
10.242840	696.012509	11.171239
10.228080	696.733677	11.176256
9.847820	715.941615	11.181274
10.382179	704.149987	11.186291
10.133856	711.315772	11.191309
10.087493	694.121612	11.196327
10.156030	705.321587	11.201344
10.032195	719.364860	11.206362
10.504131	711.559691	11.211379
10.549045	729.625532	11.216397
11.055352	726.963254	11.221415
10.727295	709.031912	11.226432
10.361308	705.022723	11.231450
10.483591	700.590585	11.236467
10.306502	702.500080	11.241485
10.120594	698.382014	11.246503
10.612158	703.751323	11.251520
10.343965	716.546929	11.256538
10.651387	731.995252	11.261555
10.033240	740.038259	11.266573
10.545623	731.028286	11.271591
10.715661	739.432093	11.276608
10.732556	743.688636	11.281626
10.773446	734.793086	11.286643
10.654167	738.116890	11.291661
10.514842	739.073665	11.296679
10.739245	733.449460	11.301696
10.686293	725.919869	11.306714
10.732223	731.639061	11.311731
10.363789	708.132428	11.316749
10.575296	716.961280	11.321767
10.757621	720.416405	11.326784
10.406230	720.993832	11.331802
10.631667	730.014350	11.336819
10.530157	730.575281	11.341837
10.616891	726.602668	11.346855
10.715561	720.438619	11.351872
10.860160	731.784381	11.356890
10.707349	723.611669	11.361907
10.788282	730.970546	11.366925
10.789598	723.865276	11.371943
10.957094	738.664312	11.376960
10.812293	730.114454	11.381978
11.086442	720.642274	11.386995
10.962712	729.120701	11.392013
10.833049	719.249983	11.397031
10.632287	697.902761	11.402048
10.363500	711.280145	11.407066
10.688827	724.077263	11.412083
10.900601	732.183868	11.417101
10.653106	733.009727	11.422119
10.682394	731.520471	11.427136
10.683155	725.255200	11.432154
11.211884	727.084664	11.437171
10.707245	729.710279	11.442189
10.762192	728.443219	11.447207
10.583336	724.129527	11.452224
10.732607	724.900347	11.457242
10.368724	729.781718	11.462259
10.695048	727.716011	11.467277
10.685741	734.479972	11.472295
10.837945	748.925999	11.477312
11.080548	761.819382	11.482330
11.067736	758.954061	11.487347
10.893583	746.878770	11.492365
11.329695	747.898592	11.497383
11.079402	727.848652	11.502400
10.812610	730.573519	11.507418
10.918415	728.858173	11.512435
10.979218	737.473697	11.517453
10.981784	747.228274	11.522471
11.056172	752.425836	11.527488
10.825035	769.789543	11.532506
11.159662	771.357343	11.537523
10.993678	767.883981	11.542541
11.156075	768.794144	11.547559
11.242693	764.997494	11.552576
11.032430	769.488398	11.557594
11.197334	759.287333	11.562611
11.351337	757.021498	11.567629
11.236594	750.294287	11.572647
11.154412	746.362771	11.577664
11.019657	754.379829	11.582682
11.237573	754.771361	11.587699
10.907372	765.518568	11.592717
11.015201	761.371821	11.597735
11.338490	763.590197	11.602752
11.327771	758.189451	11.607770
11.093745	771.664078	11.612787
10.818722	766.833783	11.617805
10.955293	766.502668	11.622823
11.280241	770.974503	11.627840
11.058156	763.815303	11.632858
11.073944	762.119553	11.637875
11.300937	765.287042	11.642893
10.776575	777.451529	11.647911
11.455485	762.169163	11.652928
10.983218	769.148106	11.657946
10.910513	760.077353	11.662963
11.416655	774.196851	11.667981
11.386346	787.033897	11.672999
11.598011	774.962825	11.678016
11.500406	768.969750	11.683034
11.517058	767.237151	11.688051
11.124861	770.512673	11.693069
11.167920	772.319075	11.698087
11.507269	771.182540	11.703104
11.117032	792.786482	11.708122
11.834434	780.535981	11.713139
11.665839	794.687587	11.718157
11.377795	774.299496	11.723175
11.267994	777.884687	11.728192
11.235204	787.488270	11.733210
11.604107	794.342484	11.738227
11.450726	796.885067	11.743245
11.164216	783.710893	11.748263
11.552393	787.427633	11.753280
11.625353	799.238846	11.758298
11.681428	801.349641	11.763315
11.803823	803.425563	11.768333
11.492073	793.525647	11.773351
11.690600	787.692547	11.778368
11.418541	800.621909	11.783386
11.288902	795.801333	11.788403
11.534544	789.151336	11.793421
11.370515	788.754465	11.798439
11.530831	784.552098	11.803456
11.480055	795.659278	11.808474
11.388617	793.991184	11.813491
11.694640	801.072388	11.818509
11.018815	802.407245	11.823527
11.475938	784.308960	11.828544
11.640520	788.265468	11.833562
11.528893	798.750338	11.838579
11.932922	800.384512	11.843597
11.567222	800.385274	11.848615
11.765611	798.576189	11.853632
11.551239	810.880682	11.858650
11.983183	822.352224	11.863667
11.722261	802.193432	11.868685
11.577630	807.690940	11.873703
11.979489	806.255245	11.878720
12.049059	818.117418	11.883738
11.869026	807.638835	11.888755
11.794903	798.807523	11.893773
11.777240	791.848246	11.898791
11.737841	792.074365	11.903808
11.682156	794.725190	11.908826
11.886384	816.493282	11.913843
12.300026	802.609693	11.918861
11.845165	809.595814	11.923879
12.101671	800.472601	11.928896
12.062962	801.243196	11.933914
11.968646	781.364915	11.938931
12.123027	785.203150	11.943949
11.634185	797.902830	11.948967
11.975850	792.942273	11.953984
11.704559	791.355663	11.959002
11.353198	791.564353	11.964019
11.820349	815.809317	11.969037
11.784506	830.038803	11.974055
12.137548	831.364237	11.979072
11.963353	830.475725	11.984090
12.005621	837.930102	11.989107
12.260570	831.802179	11.994125
12.253717	834.848218	11.999143
12.167841	831.427831	12.004160
12.420623	841.298964	12.009178
11.949022	831.688583	12.014195
12.061468	828.812389	12.019213
12.125484	827.792106	12.024231
12.325319	831.740537	12.029248
12.363039	828.920385	12.034266
11.748668	806.437932	12.039283
11.977581	801.931165	12.044301
12.033125	822.647943	12.049319
12.173981	817.096165	12.054336
11.691481	826.225957	12.059354
12.015025	825.517251	12.064371
12.412201	826.092903	12.069389
12.106019	828.734253	12.074407
12.159091	825.541157	12.079424
12.293459	832.363687	12.084442
12.070195	833.663219	12.089459
12.044359	830.823163	12.094477
12.044809	825.982654	12.099495
12.105808	825.400195	12.104512
11.870066	836.706544	12.109530
12.110950	838.538225	12.114547
12.246639	847.173909	12.119565
12.447127	864.120195	12.124583
12.565553	855.999127	12.129600
12.312256	851.941163	12.134618
12.574227	852.975797	12.139635
12.527344	828.939053	12.144653
12.640067	826.915422	12.149671
12.593366	813.091759	12.154688
12.552191	820.458360	12.159706
12.573387	827.734554	12.164723
12.774428	811.418804	12.169741
12.545416	827.785648	12.174759
12.582694	813.873710	12.179776
12.562456	829.252383	12.184794
12.632340	833.329062	12.189811
12.385739	821.669060	12.194829
12.699234	828.557344	12.199847
12.638162	836.509325	12.204864
12.478397	822.339539	12.209882
12.401766	830.023564	12.214899
12.705149	818.856629	12.219917
12.520902	819.528463	12.224935
12.310182	824.709101	12.229952
12.291953	837.362139	12.234970
12.401197	834.886995	12.239987
12.508833	829.445900	12.245005
12.441254	829.773117	12.250023
12.255549	826.296604	12.255040
12.210267	819.859407	12.260058
12.324950	843.793829	12.265075
12.742541	852.220066	12.270093
12.582725	854.338302	12.275111
12.401714	848.201329	12.280128
12.575253	848.760405	12.285146
12.605501	849.314820	12.290163
12.863963	839.773025	12.295181
12.437768	856.410929	12.300199
12.882332	847.810353	12.305216
13.019857	839.359915	12.310234
12.413007	850.935440	12.315251
12.671078	854.383196	12.320269
12.591723	859.835984	12.325287
12.737119	848.044166	12.330304
12.873609	850.062755	12.335322
12.559117	857.029343	12.340339
12.893752	851.279810	12.345357
12.834893	860.644383	12.350375
12.782695	869.137734	12.355392
12.562074	851.808443	12.360410
12.796482	871.401725	12.365427
13.051323	867.981609	12.370445
12.983031	867.163866	12.375463
12.989257	866.922978	12.380480
13.139408	851.740993	12.385498
12.933521	852.457932	12.390515
13.585883	843.083285	12.395533
13.169338	851.453109	12.400551
13.086526	842.117586	12.405568
12.950080	840.933318	12.410586
12.728041	845.779279	12.415603
13.150830	842.517308	12.420621
13.060382	842.208454	12.425639
13.035134	837.523343	12.430656
13.228353	836.238542	12.435674
12.977677	846.646932	12.440691
13.133216	845.869943	12.445709
12.670589	845.229158	12.450727
12.752350	854.515479	12.455744
12.696750	853.222000	12.460762
12.872459	875.923272	12.465779
13.064336	880.169928	12.470797
13.372949	876.974743	12.475815
13.098996	881.959882	12.480832
13.682857	873.062501	12.485850
13.384499	872.748051	12.490867
13.391050	868.199089	12.495885
13.271134	852.459671	12.500903
13.184970	850.109812	12.505920
13.231524	846.620399	12.510938
13.352529	854.301102	12.515955
13.382775	849.455170	12.520973
12.978917	849.094387	12.525991
13.074505	860.317461	12.531008
13.331278	871.773410	12.536026
13.483273	886.221371	12.541043
13.498688	881.276716	12.546061
13.262787	877.244311	12.551079
12.975905	890.057812	12.556096
13.298035	888.315261	12.561114
13.055972	888.534132	12.566131
13.643475	883.018442	12.571149
13.211235	889.738898	12.576167
13.303132	884.940041	12.581184
13.533698	879.202677	12.586202
13.323005	892.923314	12.591219
13.346726	888.743689	12.596237
13.532354	882.114494	12.601255
13.253921	875.768648	12.606272
13.088124	892.671674	12.611290
13.236047	890.718583	12.616307
13.286108	882.870269	12.621325
13.509502	880.051900	12.626343
13.441846	895.435818	12.631360
13.562955	881.024320	12.636378
13.576035	890.426227	12.641395
13.451835	906.289499	12.646413
13.524646	901.162941	12.651431
13.721255	910.001549	12.656448
13.839905	902.177319	12.661466
13.545523	908.870278	12.666483
13.510962	906.534222	12.671501
13.963472	923.726967	12.676519
13.549178	912.790553	12.681536
14.018718	905.770197	12.686554
13.622079	904.323954	12.691571
13.387246	898.035843	12.696589
13.896122	908.342471	12.701607
13.476388	911.372124	12.706624
13.987266	902.751112	12.711642
13.660308	912.389707	12.716659
14.040668	914.609695	12.721677
13.806686	916.569064	12.726695
13.573138	915.645382	12.731712
14.058450	915.562192	12.736730
13.283836	922.244572	12.741747
13.729801	907.710479	12.746765
13.776927	909.395674	12.751783
13.695294	912.260221	12.756800
13.824265	910.096712	12.761818
13.851334	903.705486	12.766835
13.531332	907.574417	12.771853
14.074694	912.041494	12.776871
14.104770	908.088530	12.781888
14.168873	908.209177	12.786906
14.234018	914.698458	12.791923
14.154965	911.109729	12.796941
14.031561	910.191267	12.801959
13.959256	918.948161	12.806976
14.359112	909.112236	12.811994
14.263227	915.450993	12.817011
13.869722	925.148616	12.822029
13.985000	910.037778	12.827047
13.854297	923.037272	12.832064
13.922471	909.360553	12.837082
13.994891	914.999563	12.842099
13.998889	915.592072	12.847117
13.777021	911.276087	12.852135
13.613479	911.091497	12.857152
13.762419	904.738586	12.862170
13.651014	911.388318	12.867187
13.766245	926.545424	12.872205
14.204716	930.043194	12.877223
14.183330	935.717986	12.882240
14.213277	936.411505	12.887258
14.167406	951.527947	12.892275
14.068159	948.021077	12.897293
14.519085	938.371150	12.902311
14.416234	947.953050	12.907328
14.669643	947.979628	12.912346
14.378678	939.637340	12.917363
14.357441	935.550354	12.922381
14.408880	933.242003	12.927399
14.208640	935.256812	12.932416
14.428096	933.002965	12.937434
14.097136	932.810024	12.942451
14.352118	939.988493	12.947469
14.588701	936.580630	12.952487
14.393082	941.446955	12.957504
14.593095	934.003685	12.962522
14.467421	942.245484	12.967539
14.350257	929.644477	12.972557
14.421534	928.432665	12.977575
14.542793	934.776090	12.982592
14.405801	933.781145	12.987610
14.459766	937.501094	12.992627
14.512690	939.937768	12.997645
14.433616	940.513105	13.002663
14.646254	948.273873	13.007680
14.870070	941.322844	13.012698
14.398114	945.272004	13.017715
14.414048	939.859409	13.022733
14.760248	934.075952	13.027751
14.480595	940.383680	13.032768
14.388941	946.669201	13.037786
14.795575	944.048847	13.042803
14.416404	942.199780	13.047821
14.677840	924.341804	13.052839
14.686274	942.371410	13.057856
14.869316	931.079817	13.062874
14.408002	944.017251	13.067891
14.261096	938.017299	13.072909
14.301632	928.070494	13.077927
14.285192	939.602150	13.082944
14.417251	935.940149	13.087962
14.625918	939.225546	13.092979
14.160770	962.424321	13.097997
14.631310	970.740610	13.103015
14.658765	977.115496	13.108032
14.710559	958.694191	13.113050
14.665955	958.541709	13.118067
14.512566	970.945485	13.123085
15.083718	965.735961	13.128103
14.770041	967.329238	13.133120
14.960484	966.438816	13.138138
14.993114	960.524324	13.143155
14.624112	961.703979	13.148173
14.817096	966.182327	13.153191
14.883590	973.807246	13.158208
14.758680	956.731267	13.163226
14.932889	959.457496	13.168243
14.450847	972.966592	13.173261
14.979112	977.425752	13.178279
15.300307	1000.311005	13.183296
15.221695	989.061428	13.188314
15.719740	968.740287	13.193331
15.247928	960.388314	13.198349
15.467469	951.650289	13.203367
15.067167	958.292085	13.208384
15.216984	948.703916	13.213402
15.308108	954.295762	13.218419
15.101969	960.477787	13.223437
15.510217	951.918189	13.228455
15.273631	959.409555	13.233472
15.187751	954.720159	13.238490
15.549587	957.673016	13.243507
15.022669	953.661915	13.248525
15.482942	944.795742	13.253543
15.079165	962.423097	13.258560
15.437188	957.483010	13.263578
15.375158	944.315099	13.268595
15.492546	952.710011	13.273613
15.497602	944.705154	13.278631
15.180455	946.785732	13.283648
15.290525	947.512263	13.288666
15.444165	948.346338	13.293683
15.423648	955.882101	13.298701
15.416367	955.127093	13.303719
15.343681	952.063003	13.308736
15.320439	938.932971	13.313754
15.210503	955.435365	13.318771
15.100772	952.235295	13.323789
15.580418	955.021659	13.328807
15.271923	953.529944	13.333824
15.410277	947.642073	13.338842
15.499777	955.058491	13.343859
15.385117	957.737000	13.348877
15.731707	948.823480	13.353895
15.490167	951.421200	13.358912
15.298278	941.733232	13.363930
15.420125	942.100789	13.368947
15.304178	956.584633	13.373965
15.706425	946.628230	13.378983
15.438982	952.869390	13.384000
15.472538	953.181274	13.389018
15.597108	951.330049	13.394035
15.408610	949.537843	13.399053
15.742649	938.024474	13.404071
15.478237	953.661402	13.409088
15.320613	944.825894	13.414106
15.652858	956.375518	13.419123
15.490007	974.850525	13.424141
15.856964	972.588044	13.429159
15.845537	985.743441	13.434176
15.932027	992.635460	13.439194
15.945920	992.222367	13.444211
15.789877	975.268029	13.449229
15.838036	965.851939	13.454247
15.753987	962.202814	13.459264
15.656078	962.705686	13.464282
15.733460	969.729100	13.469299
15.906559	978.271093	13.474317
15.982378	974.946472	13.479335
15.810863	984.932001	13.484352
15.808215	987.329646	13.489370
15.923306	982.038816	13.494387
15.829171	987.315283	13.499405
16.031351	988.352722	13.504423
15.843199	993.664212	13.509440
15.806796	990.938944	13.514458
15.972299	985.559677	13.519475
15.908023	986.601982	13.524493
15.889341	986.907345	13.529511
15.829130	978.611928	13.534528
16.023536	984.435889	13.539546
16.139317	991.450802	13.544563
15.665692	989.659457	13.549581
15.910304	973.135680	13.554599
15.780870	982.939478	13.559616
15.843531	982.384490	13.564634
16.312579	983.431559	13.569651
15.907048	986.548234	13.574669
16.063399	992.811093	13.579687
16.318622	1005.350291	13.584704
16.153001	1013.716230	13.589722
16.059901	1003.755049	13.594739
16.262430	1011.893443	13.599757
16.552652	1001.923042	13.604775
16.289728	1011.488331	13.609792
16.382801	1008.723753	13.614810
17.070717	993.502456	13.619827
16.626959	996.678591	13.624845
16.517506	979.069214	13.629863
16.450996	974.594882	13.634880
16.323341	980.431519	13.639898
16.321054	976.240226	13.644915
16.207820	990.745106	13.649933
16.242418	976.126592	13.654951
16.342749	977.622914	13.659968
16.093187	981.884487	13.664986
16.401185	975.180315	13.670003
16.517281	1000.792524	13.675021
16.503978	1002.802625	13.680039
16.401024	993.783280	13.685056
16.656254	1004.407239	13.690074
16.801443	999.291124	13.695091
16.296196	990.094404	13.700109
16.426847	980.303315	13.705127
16.483708	997.119866	13.710144
16.677743	996.513053	13.715162
16.800811	998.528567	13.720179
16.566307	1006.040474	13.725197
16.654298	1010.022884	13.730215
16.394094	1002.752666	13.735232
16.522882	998.961290	13.740250
16.876617	990.351634	13.745267
16.367469	1013.769928	13.750285
16.689203	1012.637173	13.755303
16.980700	1003.914389	13.760320
16.873586	1016.774850	13.765338
16.943237	993.550149	13.770355
16.537714	1009.049651	13.775373
16.774027	1002.558461	13.780391
16.759255	1004.888242	13.785408
16.688258	999.264241	13.790426
16.633284	998.927478	13.795443
16.526339	1001.041623	13.800461
16.815216	1000.421302	13.805479
16.628391	1004.037972	13.810496
16.637458	1004.579458	13.815514
16.861935	1000.445551	13.820531
16.340721	1005.587910	13.825549
17.105602	1021.252415	13.830567
17.117137	1027.272925	13.835584
17.188914	1032.934915	13.840602
17.420488	1025.359634	13.845619
16.985096	1015.860063	13.850637
17.235593	997.416110	13.855655
17.056795	994.275665	13.860672
16.682706	999.975110	13.865690
17.151109	1003.273888	13.870707
17.210669	1033.486283	13.875725
17.413476	1027.537345	13.880743
17.126531	1010.554607	13.885760
17.013336	997.024103	13.890778
17.162062	992.271717	13.895795
17.262115	1003.091172	13.900813
17.409319	1004.777947	13.905831
17.353298	1007.934491	13.910848
16.826009	999.708770	13.915866
17.120020	1021.827611	13.920883
16.903140	1025.840921	13.925901
17.124838	1035.137783	13.930919
17.383093	1030.371222	13.935936
17.380788	1031.930369	13.940954
17.422611	1023.531663	13.945971
17.730315	1033.487037	13.950989
17.451358	1029.196198	13.956007
17.537645	1033.218260	13.961024
17.370884	1032.819668	13.966042
17.692457	1025.894564	13.971059
17.503180	1014.787449	13.976077
17.377688	1015.756027	13.981095
17.603829	1010.374407	13.986112
17.337393	1010.318219	13.991130
17.480232	1021.478985	13.996147
17.700289	1038.668155	14.001165
17.418056	1026.306321	14.006183
17.251598	1022.269093	14.011200
17.325760	1032.581907	14.016218
17.557169	1036.702408	14.021235
17.691722	1041.345331	14.026253
17.524792	1032.300912	14.031271
17.563471	1035.977552	14.036288
17.587119	1025.870902	14.041306
17.539823	1033.608734	14.046323
17.551688	1030.546992	14.051341
17.796559	1030.482870	14.056359
17.870341	1039.783317	14.061376
17.436826	1031.568849	14.066394
17.707079	1031.195267	14.071411
17.594162	1037.270200	14.076429
17.374820	1041.834029	14.081447
17.527824	1039.502187	14.086464
17.292614	1037.272880	14.091482
17.855330	1043.589059	14.096499
18.006634	1059.091656	14.101517
17.813881	1065.967070	14.106535
17.806447	1054.952100	14.111552
17.993258	1066.564614	14.116570
17.936524	1053.316022	14.121587
18.157485	1064.368453	14.126605
18.181040	1056.309308	14.131623
18.012003	1055.860115	14.136640
17.963962	1058.688040	14.141658
18.046115	1050.218885	14.146675
18.330683	1050.090929	14.151693
17.826899	1049.478586	14.156711
18.121843	1048.253027	14.161728
18.308453	1055.084048	14.166746
18.121710	1046.495184	14.171763
18.090889	1046.119396	14.176781
18.039856	1042.035927	14.181799
18.021286	1031.362524	14.186816
17.922314	1044.919385	14.191834
18.476420	1049.978530	14.196851
18.497273	1051.735395	14.201869
18.042501	1043.937557	14.206887
18.292335	1039.534924	14.211904
18.175450	1042.402171	14.216922
18.246474	1040.622373	14.221939
18.150222	1057.369032	14.226957
18.215945	1043.275147	14.231975
18.323001	1041.261281	14.236992
18.145227	1043.878593	14.242010
18.426095	1047.448884	14.247027
18.288643	1054.139197	14.252045
18.095136	1058.660580	14.257063
18.574086	1048.846726	14.262080
18.276313	1058.438076	14.267098
18.521839	1048.165632	14.272115
18.290836	1056.092076	14.277133
18.480033	1055.825181	14.282151
18.306906	1058.394097	14.287168
18.302658	1058.764387	14.292186
18.176814	1047.231084	14.297203
18.513424	1042.004398	14.302221
18.345338	1048.696622	14.307239
18.185739	1046.664036	14.312256
18.505712	1060.285908	14.317274
18.490885	1079.228627	14.322291
18.803608	1074.272173	14.327309
18.689712	1081.828744	14.332327
18.948455	1071.876884	14.337344
19.126146	1071.241869	14.342362
18.816816	1050.977480	14.347379
18.873367	1052.370235	14.352397
18.742529	1046.178442	14.357415
19.117923	1042.907237	14.362432
18.740049	1051.791266	14.367450
18.663377	1049.043907	14.372467
18.936069	1051.969787	14.377485
18.541869	1047.762348	14.382503
19.178468	1038.780578	14.387520
18.637835	1041.545635	14.392538
18.833793	1035.167579	14.397555
18.791802	1040.272088	14.402573
18.647130	1054.721998	14.407591
19.251892	1056.785061	14.412608
19.276094	1062.369112	14.417626
18.792475	1049.956103	14.422643
18.966549	1047.173015	14.427661
19.237432	1070.961427	14.432679
19.258356	1047.497886	14.437696
19.023221	1044.833792	14.442714
19.212143	1045.621694	14.447731
19.271561	1037.265931	14.452749
18.964496	1040.590719	14.457767
18.729362	1038.561760	14.462784
19.053822	1050.155451	14.467802
18.990574	1065.850376	14.472819
19.336345	1074.083617	14.477837
19.062949	1077.893519	14.482855
19.120869	1060.045596	14.487872
18.996864	1065.434883	14.492890
18.927452	1071.078494	14.497907
19.170440	1064.969382	14.502925
19.038683	1075.747484	14.507943
19.096667	1068.292980	14.512960
19.249184	1083.548788	14.517978
19.068757	1072.064637	14.522995
19.517771	1069.465208	14.528013
19.219959	1083.246467	14.533031
19.394890	1076.939575	14.538048
19.626878	1070.331767	14.543066
19.382779	1069.487759	14.548083
19.712328	1071.466208	14.553101
19.310293	1074.357358	14.558119
19.546690	1066.156950	14.563136
19.443989	1074.871325	14.568154
19.244172	1072.418875	14.573171
19.518100	1072.520987	14.578189
19.601550	1077.346551	14.583207
19.780063	1064.022663	14.588224
19.888184	1069.297816	14.593242
19.437468	1059.163843	14.598259
19.947899	1066.826058	14.603277
19.922450	1071.979410	14.608295
19.705974	1066.476260	14.613312
19.819452	1062.679330	14.618330
19.515457	1063.893517	14.623347
19.849382	1063.373607	14.628365
19.384955	1071.471684	14.633383
19.770427	1068.827252	14.638400
19.673004	1073.041271	14.643418
19.785755	1070.346056	14.648435
19.995543	1063.997982	14.653453
19.489214	1071.048426	14.658471
19.731963	1077.383642	14.663488
19.764392	1083.537314	14.668506
20.143946	1104.802113	14.673523
19.750629	1101.794915	14.678541
19.822151	1100.214799	14.683559
19.958533	1089.055979	14.688576
20.086770	1103.589161	14.693594
19.930422	1101.078547	14.698611
20.288164	1093.720337	14.703629
19.889025	1094.447770	14.708647
20.234533	1090.048601	14.713664
20.288387	1093.304308	14.718682
20.296982	1083.116263	14.723699
20.682906	1080.426093	14.728717
20.011210	1072.268677	14.733735
20.027451	1061.940429	14.738752
20.165252	1060.394042	14.743770
19.991062	1077.921985	14.748787
20.160097	1070.378077	14.753805
19.934184	1089.025625	14.758823
20.249569	1090.213037	14.763840
20.409294	1080.880393	14.768858
20.005477	1095.371197	14.773875
20.599162	1092.925387	14.778893
20.262680	1093.450566	14.783911
20.429010	1080.149737	14.788928
20.001032	1093.418938	14.793946
20.377348	1088.754483	14.798963
20.349180	1083.722492	14.803981
20.315789	1088.193411	14.808999
20.487828	1086.906873	14.814016
20.363261	1092.510599	14.819034
20.335996	1089.606862	14.824051
20.558603	1079.095900	14.829069
20.503412	1093.709181	14.834087
20.273294	1084.711781	14.839104
20.683985	1085.823414	14.844122
20.386218	1089.042360	14.849139
20.038325	1083.333399	14.854157
20.184678	1106.339815	14.859175
20.353482	1119.173463	14.864192
20.806259	1116.599974	14.869210
20.474922	1115.368277	14.874227
20.706724	1121.125293	14.879245
20.549890	1122.211048	14.884263
20.345808	1118.908246	14.889280
21.026844	1114.453426	14.894298
20.645009	1122.975017	14.899315
20.924450	1118.224413	14.904333
20.974687	1119.966195	14.909351
20.859805	1108.351716	14.914368
21.076128	1109.587779	14.919386
20.866676	1110.923136	14.924403
21.113437	1109.274697	14.929421
21.118246	1116.903583	14.934439
21.032831	1116.909985	14.939456
21.282920	1121.663740	14.944474
20.729143	1118.583072	14.949491
21.155555	1114.949735	14.954509
20.825551	1120.280972	14.959527
20.943518	1116.677941	14.964544
21.067502	1116.993977	14.969562
20.813437	1117.893665	14.974579
21.102559	1103.562641	14.979597
21.335155	1119.243962	14.984615
20.909901	1118.208663	14.989632
21.172710	1103.054360	14.994650
20.805263	1121.565322	14.999667
21.075714	1110.408736	15.004685
21.114564	1121.457056	15.009703
21.220185	1122.255973	15.014720
21.164375	1106.017292	15.019738
20.698492	1125.214499	15.024755
21.236804	1133.556090	15.029773
21.403191	1147.509082	15.034791
21.160940	1144.814261	15.039808
21.501749	1152.307336	15.044826
21.717742	1161.357028	15.049843
21.838155	1152.142237	15.054861
21.724737	1130.996677	15.059879
20.984423	1117.443146	15.064896
21.298159	1124.946783	15.069914
21.438076	1142.447888	15.074931
21.566900	1133.840483	15.079949
21.674844	1140.339516	15.084967
21.276625	1135.853822	15.089984
21.856321	1146.980867	15.095002
21.285713	1140.469644	15.100019
21.635315	1145.767309	15.105037
21.461450	1147.542586	15.110055
21.258202	1146.151748	15.115072
21.732805	1140.714065	15.120090
21.525046	1143.615636	15.125107
21.135258	1133.030669	15.130125
21.447180	1142.330597	15.135143
21.797918	1139.866276	15.140160
21.778150	1145.313747	15.145178
21.677858	1158.959102	15.150195
21.786541	1154.801579	15.155213
21.878470	1169.352042	15.160231
22.476410	1171.279460	15.165248
22.452764	1155.899257	15.170266
22.113940	1142.481095	15.175283
22.040999	1130.263501	15.180301
21.995572	1128.173656	15.185319
21.622063	1140.289586	15.190336
21.879228	1134.960267	15.195354
22.030835	1137.929399	15.200371
21.775258	1122.045121	15.205389
21.567739	1141.112855	15.210407
21.652960	1152.794183	15.215424
22.160313	1163.858208	15.220442
22.010081	1170.835089	15.225459
22.217818	1155.516830	15.230477
22.463525	1160.555137	15.235495
22.295261	1157.657172	15.240512
22.366666	1157.210755	15.245530
21.933134	1176.025374	15.250547
22.337266	1168.643324	15.255565
22.496576	1175.518668	15.260583
22.262244	1167.816995	15.265600
22.659103	1166.685789	15.270618
22.491075	1160.250134	15.275635
22.606943	1144.889006	15.280653
22.552924	1148.187941	15.285671
22.157926	1136.275296	15.290688
22.319273	1133.388997	15.295706
22.087783	1142.362846	15.300723
22.273277	1155.342168	15.305741
22.552583	1158.747808	15.310759
21.975817	1162.198674	15.315776
22.444265	1155.598401	15.320794
22.207287	1160.171084	15.325811
22.221005	1153.665443	15.330829
22.559059	1163.429104	15.335847
22.282712	1163.117702	15.340864
22.412045	1158.509196	15.345882
22.695862	1172.883093	15.350899
22.817082	1186.924872	15.355917
22.588468	1178.187759	15.360935
22.560929	1187.779603	15.365952
23.083083	1186.277940	15.370970
22.774737	1188.988890	15.375987
22.794924	1188.260035	15.381005
22.896592	1184.241242	15.386023
23.146745	1180.318956	15.391040
23.198657	1167.125922	15.396058
22.874250	1170.328819	15.401075
22.971035	1153.998936	15.406093
22.990149	1155.212482	15.411111
22.507281	1156.904002	15.416128
22.852637	1145.748987	15.421146
22.964872	1166.412083	15.426163
22.852153	1175.677300	15.431181
23.332965	1180.866300	15.436199
22.789861	1186.399088	15.441216
23.164398	1184.440593	15.446234
23.255332	1186.194749	15.451251
23.314918	1178.860185	15.456269
23.023718	1176.253947	15.461287
23.174900	1195.446301	15.466304
23.467478	1175.883733	15.471322
23.292620	1192.194384	15.476339
23.302719	1186.086512	15.481357
23.219472	1168.500338	15.486375
23.301321	1189.423566	15.491392
23.083192	1183.556135	15.496410
23.263559	1186.185929	15.501427
23.198189	1188.562676	15.506445
23.448296	1185.030692	15.511463
23.127943	1194.487689	15.516480
23.568589	1170.250375	15.521498
23.523454	1178.845471	15.526515
23.379943	1187.716828	15.531533
23.461183	1183.176686	15.536551
23.040600	1182.368135	15.541568
23.542008	1181.148599	15.546586
23.417633	1181.688721	15.551603
23.145965	1187.637607	15.556621
23.344583	1178.826940	15.561639
23.295731	1188.285123	15.566656
23.427400	1172.826291	15.571674
23.220641	1196.145094	15.576691
23.551870	1210.212417	15.581709
24.169147	1212.733406	15.586727
23.914657	1211.090833	15.591744
24.324671	1203.068323	15.596762
24.010198	1195.030522	15.601779
24.061176	1188.658451	15.606797
24.340847	1181.343019	15.611815
23.831882	1180.287892	15.616832
24.113073	1176.390985	15.621850
23.927557	1179.282983	15.626867
23.713312	1186.603273	15.631885
23.635114	1166.453662	15.636903
23.606771	1175.037910	15.641920
23.688674	1175.534497	15.646938
23.689023	1180.066392	15.651955
23.921184	1197.049243	15.656973
24.341672	1204.311099	15.661991
23.991016	1211.994050	15.667008
24.303896	1204.273376	15.672026
24.149710	1199.116721	15.677043
24.174907	1201.922334	15.682061
24.350648	1198.211523	15.687079
23.928555	1200.958593	15.692096
24.353109	1201.425126	15.697114
24.401146	1205.548028	15.702131
24.371153	1207.094645	15.707149
24.358511	1187.121941	15.712167
23.827637	1185.246346	15.717184
24.364536	1189.703946	15.722202
24.318722	1207.592260	15.727219
24.245923	1214.231020	15.732237
24.527103	1199.542611	15.737255
24.132634	1213.842246	15.742272
24.341627	1206.482191	15.747290
24.651607	1210.149270	15.752307
24.481580	1210.236967	15.757325
24.535043	1207.093524	15.762343
24.223874	1210.579828	15.767360
24.548153	1212.608962	15.772378
24.260667	1206.916542	15.777395
24.359587	1213.421821	15.782413
24.480828	1205.179748	15.787431
24.263543	1219.966173	15.792448
24.434592	1229.086709	15.797466
24.361080	1235.216615	15.802483
24.514288	1244.982730	15.807501
24.641892	1229.642803	15.812519
24.752578	1248.839948	15.817536
24.778476	1242.318872	15.822554
24.799457	1241.021857	15.827571
24.966912	1235.560893	15.832589
25.191078	1218.245664	15.837607
24.728534	1236.500472	15.842624
25.100810	1230.026477	15.847642
25.289820	1232.280496	15.852659
25.242723	1225.407765	15.857677
25.365133	1220.165833	15.862695
25.242661	1226.403222	15.867712
25.327256	1225.048065	15.872730
25.363609	1215.084052	15.877747
24.664039	1201.764620	15.882765
25.470138	1208.444919	15.887783
25.101403	1208.865605	15.892800
25.006315	1209.537483	15.897818
25.240400	1215.341591	15.902835
25.020654	1209.694266	15.907853
25.543518	1216.666613	15.912871
25.098254	1236.713574	15.917888
25.402106	1217.241794	15.922906
25.231866	1223.374296	15.927923
24.984747	1226.456771	15.932941
25.322642	1224.708233	15.937959
25.172388	1225.354980	15.942976
25.289024	1219.004325	15.947994
25.276853	1217.710232	15.953011
25.154329	1231.656328	15.958029
25.399578	1224.997255	15.963047
25.458599	1231.871484	15.968064
25.410440	1221.204216	15.973082
25.186123	1231.384232	15.978099
25.298297	1234.020382	15.983117
25.850611	1241.514765	15.988135
25.541266	1255.268954	15.993152
25.660820	1260.075619	15.998170
26.301563	1252.168673	16.003187
25.794739	1227.197225	16.008205
25.673965	1228.318360	16.013223
25.704319	1226.491136	16.018240
25.838051	1215.856402	16.023258
25.681292	1215.549839	16.028275
25.677164	1216.691849	16.033293
26.196188	1222.491386	16.038311
25.941908	1225.294574	16.043328
26.047350	1209.520795	16.048346
25.888783	1203.370130	16.053363
25.881896	1217.276044	16.058381
26.120314	1215.245959	16.063399
25.790103	1225.962488	16.068416
26.049390	1227.282589	16.073434
25.995716	1241.183463	16.078451
25.765294	1255.844160	16.083469
26.052471	1248.604215	16.088487
25.949227	1244.782433	16.093504
25.678777	1258.099749	16.098522
25.825623	1257.160224	16.103539
25.911048	1260.906937	16.108557
26.068526	1241.316226	16.113575
25.987054	1245.199161	16.118592
26.297303	1261.497033	16.123610
26.563360	1262.734731	16.128627
26.213543	1275.815411	16.133645
26.459718	1261.715124	16.138663
26.423587	1268.110480	16.143680
26.427736	1273.878800	16.148698
26.431917	1270.380352	16.153715
26.830466	1282.917349	16.158733
26.842807	1266.099406	16.163751
26.423707	1254.764977	16.168768
26.103919	1253.185151	16.173786
26.527151	1253.755827	16.178803
26.614063	1257.155297	16.183821
26.625956	1268.357171	16.188839
26.642176	1276.500317	16.193856
26.549937	1261.409059	16.198874
26.699529	1266.484542	16.203891
26.330907	1273.723116	16.208909
26.698624	1267.485061	16.213927
26.766617	1270.620770	16.218944
26.699375	1267.884607	16.223962
26.790156	1269.556527	16.228979
26.590676	1272.937786	16.233997
26.476436	1262.888211	16.239015
26.634707	1264.032714	16.244032
26.362129	1278.028252	16.249050
26.828878	1287.691013	16.254067
26.820999	1302.781446	16.259085
27.154915	1297.847794	16.264103
27.091731	1301.361632	16.269120
26.826430	1297.654794	16.274138
27.079664	1291.299053	16.279155
27.081639	1291.777163	16.284173
27.037689	1287.131319	16.289191
26.933106	1285.654686	16.294208
27.113750	1289.143973	16.299226
27.520029	1287.428413	16.304243
27.269954	1295.301643	16.309261
27.573539	1290.228342	16.314279
27.575370	1294.739754	16.319296
27.158940	1305.108629	16.324314
27.483644	1302.370476	16.329331
27.202684	1302.677263	16.334349
27.725966	1298.536215	16.339367
27.887533	1291.825990	16.344384
27.253661	1293.711548	16.349402
27.500365	1293.755376	16.354419
27.673781	1283.398446	16.359437
27.608354	1288.401806	16.364455
27.891325	1284.996830	16.369472
27.730576	1285.329022	16.374490
27.812432	1279.540702	16.379507
27.703897	1289.775825	16.384525
27.276531	1294.776016	16.389543
27.696842	1285.153173	16.394560
27.597508	1283.671539	16.399578
27.692379	1289.320754	16.404595
27.778959	1294.177952	16.409613
27.789113	1292.119249	16.414631
27.675468	1289.432082	16.419648
27.125052	1291.398323	16.424666
27.554422	1299.522609	16.429683
27.597591	1302.756705	16.434701
28.027440	1313.017227	16.439719
28.129304	1312.521488	16.444736
27.945346	1330.215285	16.449754
28.217386	1319.210626	16.454771
28.197215	1317.002229	16.459789
28.141523	1296.765669	16.464807
28.158585	1301.088962	16.469824
27.918311	1303.650317	16.474842
28.044783	1295.752360	16.479859
28.169057	1316.617774	16.484877
27.890734	1305.934159	16.489895
28.430687	1319.772237	16.494912
28.111584	1325.414493	16.499930
28.083512	1311.969827	16.504947
27.919385	1324.729942	16.509965
28.217190	1320.468101	16.514983
28.156053	1302.440977	16.520000
27.828736	1310.355913	16.525018
28.508130	1314.158990	16.530035
28.645831	1318.814074	16.535053
28.371399	1317.810521	16.540071
28.403055	1320.050798	16.545088
28.961501	1322.403798	16.550106
28.654883	1317.393929	16.555123
28.476599	1306.141893	16.560141
28.431029	1310.624730	16.565159
28.639095	1306.902057	16.570176
28.660420	1333.696851	16.575194
28.617721	1335.738031	16.580211
28.855145	1339.353361	16.585229
28.709485	1339.711009	16.590247
28.958403	1337.037137	16.595264
28.766485	1336.270896	16.600282
28.882332	1337.160051	16.605299
29.001471	1337.831763	16.610317
29.007176	1334.565692	16.615335
29.269699	1326.858789	16.620352
28.962695	1323.702853	16.625370
29.107654	1301.466085	16.630387
28.986385	1305.241455	16.635405
28.938696	1303.398776	16.640423
29.039080	1304.828006	16.645440
29.056234	1317.596145	16.650458
28.989089	1329.017788	16.655475
29.435979	1331.268178	16.660493
29.029865	1329.495552	16.665511
29.288926	1329.576308	16.670528
29.359545	1340.180425	16.675546
29.284394	1335.755440	16.680563
29.433658	1334.654707	16.685581
29.187950	1341.630516	16.690599
29.499554	1334.903548	16.695616
29.264924	1345.440411	16.700634
29.650868	1331.307122	16.705651
29.310899	1332.000577	16.710669
29.060534	1338.084367	16.715687
29.497319	1327.667942	16.720704
29.059183	1327.680474	16.725722
28.992953	1329.450384	16.730739
29.091224	1329.311486	16.735757
28.937915	1341.894460	16.740775
29.596098	1343.188608	16.745792
29.740523	1354.190322	16.750810
29.926527	1363.550361	16.755827
30.052509	1357.351036	16.760845
29.929151	1360.793937	16.765863
30.026135	1355.931306	16.770880
30.126588	1362.660970	16.775898
30.063741	1353.262790	16.780915
29.746531	1342.680248	16.785933
29.989294	1346.791085	16.790951
30.117006	1353.231241	16.795968
29.716796	1355.227581	16.800986
29.889080	1356.762634	16.806003
30.176680	1354.298085	16.811021
29.804419	1362.270074	16.816039
29.954586	1352.808744	16.821056
29.855516	1346.792263	16.826074
29.987612	1356.127156	16.831091
29.854526	1355.233491	16.836109
30.022601	1354.245577	16.841127
29.977592	1359.785669	16.846144
29.808271	1360.067317	16.851162
30.218842	1360.124807	16.856179
30.668741	1374.034698	16.861197
30.570265	1368.389318	16.866215
30.992937	1349.160888	16.871232
30.882588	1350.695212	16.876250
30.768548	1346.695293	16.881267
30.923747	1349.003139	16.886285
30.455547	1356.728220	16.891303
30.799549	1343.836718	16.896320
30.466528	1345.762316	16.901338
30.650733	1345.768250	16.906355
30.557401	1345.681879	16.911373
30.808364	1337.052995	16.916391
31.242157	1338.172443	16.921408
30.647771	1336.481315	16.926426
30.684910	1334.547459	16.931443
30.749863	1327.667778	16.936461
30.563446	1344.950640	16.941479
30.639200	1341.734203	16.946496
30.527065	1352.333494	16.951514
30.596332	1354.177262	16.956531
30.729497	1354.264062	16.961549
30.655994	1350.520004	16.966567
30.889167	1347.227363	16.971584
30.697217	1349.366624	16.976602
30.545037	1345.611360	16.981619
31.046585	1356.614091	16.986637
30.789200	1375.555532	16.991655
31.120485	1376.209115	16.996672
31.129584	1378.928851	17.001690
31.303059	1372.304406	17.006707
30.999942	1370.566125	17.011725
31.140425	1384.043956	17.016743
31.418210	1366.252048	17.021760
31.264878	1378.865366	17.026778
31.175402	1373.571205	17.031795
31.421071	1373.601229	17.036813
31.249137	1377.521191	17.041831
31.571005	1378.138934	17.046848
31.361328	1378.523104	17.051866
31.451783	1386.415885	17.056883
31.820673	1374.603165	17.061901
31.476914	1381.666839	17.066919
31.831247	1374.425777	17.071936
31.538051	1381.179759	17.076954
31.603953	1376.042375	17.081971
31.646924	1362.411736	17.086989
31.413577	1373.543402	17.092007
31.782346	1368.591174	17.097024
31.619938	1363.799354	17.102042
31.497850	1365.633806	17.107059
31.659405	1380.886251	17.112077
31.712042	1397.435472	17.117095
31.749745	1395.919372	17.122112
31.963058	1398.560292	17.127130
31.730541	1393.173635	17.132147
32.008406	1390.520558	17.137165
32.001154	1396.714175	17.142183
31.924875	1383.187268	17.147200
32.309036	1389.250855	17.152218
31.922518	1400.376754	17.157235
32.195309	1388.563174	17.162253
32.007622	1393.779463	17.167271
32.058894	1388.871233	17.172288
32.232661	1391.342530	17.177306
32.229792	1386.444035	17.182323
32.013764	1383.732241	17.187341
31.971995	1386.588122	17.192359
32.150651	1402.317617	17.197376
32.480953	1420.360531	17.202394
32.496890	1419.396179	17.207411
32.720431	1408.448481	17.212429
32.482722	1412.516113	17.217447
32.761515	1412.275149	17.222464
32.945243	1413.007835	17.227482
32.436767	1393.685030	17.232499
32.562930	1378.949046	17.237517
32.340881	1378.684367	17.242535
32.428281	1386.435743	17.247552
32.562671	1406.604428	17.252570
32.590326	1412.047306	17.257587
32.546443	1415.562507	17.262605
32.757611	1422.407939	17.267623
32.431082	1417.033661	17.272640
32.686321	1423.232330	17.277658
32.830526	1413.905198	17.282675
32.939380	1421.897698	17.287693
32.761589	1422.608838	17.292711
32.692801	1409.812854	17.297728
32.894560	1421.376324	17.302746
32.922513	1448.940001	17.307763
33.172333	1434.101257	17.312781
33.020077	1442.538832	17.317799
33.280528	1430.031094	17.322816
33.396835	1434.363415	17.327834
33.392500	1445.037265	17.332851
33.320928	1436.776347	17.337869
33.267943	1445.816136	17.342887
33.556440	1429.920753	17.347904
33.574389	1441.486270	17.352922
33.436130	1432.849222	17.357939
33.815610	1425.026499	17.362957
33.263656	1413.713709	17.367975
33.408671	1413.335228	17.372992
33.267874	1415.536705	17.378010
33.559780	1433.898732	17.383027
33.639787	1439.501056	17.388045
33.646431	1438.627400	17.393063
33.519816	1430.469467	17.398080
33.450069	1441.062404	17.403098
33.429586	1444.412547	17.408115
33.848821	1433.580897	17.413133
33.690603	1440.878271	17.418151
33.979654	1434.635238	17.423168
33.761929	1429.086697	17.428186
33.300743	1438.889907	17.433203
33.677315	1439.925327	17.438221
33.727444	1440.565344	17.443239
34.084388	1441.137732	17.448256
33.908226	1449.234228	17.453274
34.127000	1459.181941	17.458291
34.365807	1464.211648	17.463309
34.144296	1461.537553	17.468327
34.242025	1439.971096	17.473344
34.166519	1433.537160	17.478362
34.074934	1455.279855	17.483379
34.304237	1460.084784	17.488397
34.483139	1459.867215	17.493415
34.275877	1458.175871	17.498432
34.519754	1459.338915	17.503450
34.342813	1472.429179	17.508467
34.356217	1463.539522	17.513485
34.505961	1463.308467	17.518503
34.638366	1454.059826	17.523520
34.572655	1447.727204	17.528538
34.459273	1453.854535	17.533555
34.563983	1446.508056	17.538573
34.298569	1448.994465	17.543591
34.559325	1442.704536	17.548608
34.656270	1447.123710	17.553626
34.267146	1451.381116	17.558643
34.697796	1452.189520	17.563661
34.476088	1460.941691	17.568679
34.631504	1453.069575	17.573696
34.679149	1449.527097	17.578714
34.573335	1462.626266	17.583731
34.950053	1465.033135	17.588749
35.079720	1479.009031	17.593767
34.964039	1477.808586	17.598784
35.084247	1464.467809	17.603802
34.896513	1474.517940	17.608819
35.162556	1477.704417	17.613837
35.509123	1477.790988	17.618855
35.093587	1470.877470	17.623872
35.191662	1461.186131	17.628890
35.304607	1468.069859	17.633907
35.082570	1464.919338	17.638925
35.050094	1473.722912	17.643943
35.164600	1475.697586	17.648960
35.412001	1477.882355	17.653978
35.235329	1483.888285	17.658995
35.386732	1473.514002	17.664013
35.248717	1479.447409	17.669031
35.517421	1484.644207	17.674048
35.547303	1470.817432	17.679066
35.231422	1469.966368	17.684083
35.447350	1465.788874	17.689101
35.364058	1467.017794	17.694119
35.434758	1471.145485	17.699136
35.782368	1482.050928	17.704154
35.510270	1492.436230	17.709171
36.210496	1511.776801	17.714189
36.009393	1503.612439	17.719207
35.652328	1488.222049	17.724224
35.909751	1488.574302	17.729242
35.794706	1500.081537	17.734259
36.337194	1498.992179	17.739277
36.081948	1497.512080	17.744295
36.014339	1493.100958	17.749312
36.015749	1490.938569	17.754330
36.295031	1503.637369	17.759347
36.331750	1488.670817	17.764365
35.954902	1485.131362	17.769383
35.800308	1496.790583	17.774400
36.186471	1499.198062	17.779418
36.235873	1494.265308	17.784435
36.312286	1479.244968	17.789453
36.101253	1494.073137	17.794471
36.234936	1484.160967	17.799488
36.545986	1479.883903	17.804506
36.316561	1493.964619	17.809523
36.336450	1477.156613	17.814541
36.331784	1481.656754	17.819559
36.128872	1497.533643	17.824576
36.282174	1504.314274	17.829594
36.485173	1506.057624	17.834611
36.533123	1516.996078	17.839629
37.022280	1518.186302	17.844647
36.647136	1524.462022	17.849664
36.861699	1518.858742	17.854682
36.867270	1526.605604	17.859699
36.771373	1523.088207	17.864717
36.951906	1526.125855	17.869735
36.773252	1519.553042	17.874752
36.813907	1517.063930	17.879770
36.764476	1520.399190	17.884787
37.032504	1522.490411	17.889805
37.161250	1521.014168	17.894823
37.134659	1509.455652	17.899840
36.878096	1504.246332	17.904858
37.100080	1510.927833	17.909875
37.321762	1515.203989	17.914893
37.137679	1514.630906	17.919911
36.884717	1522.724977	17.924928
36.980893	1516.548228	17.929946
37.148801	1530.448962	17.934963
37.293094	1543.886348	17.939981
37.336081	1555.030741	17.944999
37.511049	1546.472166	17.950016
37.700955	1540.077975	17.955034
37.872832	1549.555606	17.960051
37.788026	1543.221376	17.965069
37.818460	1540.320616	17.970087
37.668737	1543.960607	17.975104
37.879931	1539.967513	17.980122
37.515396	1529.530243	17.985139
37.770260	1531.858060	17.990157
38.042297	1536.144008	17.995175
37.761496	1540.633309	18.000192
38.057678	1529.637108	18.005210
37.790038	1541.845882	18.010227
37.849315	1541.345954	18.015245
38.039453	1527.923102	18.020263
37.899967	1526.862396	18.025280
37.877547	1528.377680	18.030298
38.067586	1533.544980	18.035315
37.872569	1526.647548	18.040333
38.118020	1527.341107	18.045351
37.737076	1540.811357	18.050368
37.901779	1539.221900	18.055386
37.336230	1529.410094	18.060403
37.893094	1547.242709	18.065421
38.413190	1555.292304	18.070439
38.369357	1564.134022	18.075456
38.694448	1570.698916	18.080474
38.406724	1562.786209	18.085491
38.649163	1553.738194	18.090509
38.728456	1548.344045	18.095527
38.524009	1556.687170	18.100544
38.903146	1557.986315	18.105562
39.057030	1549.263723	18.110579
39.037030	1556.013969	18.115597
38.886704	1555.160734	18.120615
38.838580	1554.606713	18.125632
38.962186	1547.884739	18.130650
39.110062	1547.312303	18.135667
39.027218	1554.217993	18.140685
39.200362	1530.938572	18.145703
38.874013	1531.948246	18.150720
38.765350	1534.100538	18.155738
38.884847	1546.320527	18.160755
38.862824	1564.084080	18.165773
39.142050	1555.256335	18.170791
38.694129	1560.516667	18.175808
38.848497	1553.921677	18.180826
38.959536	1564.968228	18.185843
39.037031	1556.894790	18.190861
38.917774	1555.385914	18.195879
39.094602	1583.433827	18.200896
39.283679	1571.622132	18.205914
39.061928	1588.060031	18.210931
38.821994	1586.900974	18.215949
39.192425	1591.536577	18.220967
39.356101	1590.870005	18.225984
39.467778	1587.279320	18.231002
39.686668	1603.422399	18.236019
39.746873	1609.145759	18.241037
39.785174	1611.495795	18.246055
39.445666	1623.221885	18.251072
39.957664	1606.668792	18.256090
40.180709	1612.384336	18.261107
39.731065	1603.081808	18.266125
39.778928	1596.667766	18.271143
39.996701	1618.953788	18.276160
39.903533	1613.523162	18.281178
40.010047	1614.895903	18.286195
39.899665	1628.870073	18.291213
40.095860	1612.315822	18.296231
40.242069	1623.172176	18.301248
40.259239	1622.883116	18.306266
40.215044	1615.104526	18.311283
40.385556	1618.388897	18.316301
40.537202	1604.792243	18.321319
40.138965	1611.390870	18.326336
40.223310	1609.471814	18.331354
40.403211	1609.974266	18.336371
40.399841	1606.152619	18.341389
40.306119	1609.827066	18.346407
39.753951	1611.204141	18.351424
40.016290	1609.205874	18.356442
39.981297	1621.503808	18.361459
40.381481	1633.523958	18.366477
40.428302	1637.907972	18.371495
40.627230	1656.318304	18.376512
40.826490	1651.335935	18.381530
40.912860	1639.037481	18.386547
40.802576	1647.139531	18.391565
40.970148	1647.885134	18.396583
40.647071	1647.111420	18.401600
40.706597	1638.603560	18.406618
40.999567	1644.564026	18.411635
40.904050	1646.825761	18.416653
41.354955	1633.186519	18.421671
40.938935	1642.561381	18.426688
40.934139	1632.315547	18.431706
41.155414	1624.818438	18.436723
41.161419	1657.024721	18.441741
41.289441	1664.281197	18.446759
41.444468	1666.546606	18.451776
41.539581	1659.760206	18.456794
41.770336	1668.421977	18.461811
41.264151	1659.574571	18.466829
41.519942	1659.551356	18.471847
41.390185	1664.728245	18.476864
41.878853	1656.508865	18.481882
41.959698	1650.356640	18.486899
42.018534	1647.663936	18.491917
41.981849	1623.736258	18.496935
41.758835	1623.006436	18.501952
41.663968	1621.102035	18.506970
41.626781	1617.647740	18.511987
41.655987	1623.286279	18.517005
42.124855	1634.258002	18.522023
41.855969	1651.841218	18.527040
41.835325	1649.392919	18.532058
42.162450	1656.383841	18.537075
41.882735	1656.038341	18.542093
42.087059	1651.969592	18.547111
41.863727	1660.305855	18.552128
42.088536	1667.484339	18.557146
42.050650	1666.996330	18.562163
41.992787	1657.034412	18.567181
42.259967	1665.511838	18.572199
41.922358	1659.410062	18.577216
41.963640	1662.330410	18.582234
41.775074	1683.803662	18.587251
42.353678	1688.114181	18.592269
42.596214	1678.928495	18.597287
42.516710	1679.817082	18.602304
42.718054	1688.849430	18.607322
42.592241	1681.690718	18.612339
42.678364	1691.068644	18.617357
43.079268	1674.664925	18.622375
42.970538	1672.143394	18.627392
42.851216	1670.728797	18.632410
43.445791	1664.835529	18.637427
43.037138	1665.586011	18.642445
43.305918	1675.138049	18.647463
43.083194	1657.749933	18.652480
43.055778	1643.623257	18.657498
43.192624	1644.506598	18.662515
42.969484	1652.866445	18.667533
43.111117	1650.948940	18.672551
43.321217	1660.069184	18.677568
43.325886	1664.732776	18.682586
43.372085	1658.295757	18.687603
43.388972	1663.206513	18.692621
43.356208	1646.054900	18.697639
43.158872	1656.014031	18.702656
43.179693	1654.644969	18.707674
43.444819	1664.011997	18.712691
43.434048	1664.090305	18.717709
43.728719	1663.348939	18.722727
43.301520	1667.079098	18.727744
43.368157	1665.921926	18.732762
43.693086	1669.250073	18.737779
43.487827	1671.501800	18.742797
43.774498	1664.757356	18.747815
43.458926	1665.958542	18.752832
43.367958	1678.811573	18.757850
43.716749	1684.138888	18.762867
43.720629	1704.305518	18.767885
43.979190	1707.722978	18.772903
44.206748	1694.207981	18.777920
44.041433	1698.889242	18.782938
44.395100	1699.693455	18.787955
43.703220	1693.353589	18.792973
43.840866	1688.256799	18.797991
44.193090	1682.978111	18.803008
44.121633	1689.478681	18.808026
44.291558	1687.299439	18.813043
44.069682	1715.998254	18.818061
44.662648	1720.816980	18.823079
44.403224	1732.642700	18.828096
44.232371	1725.365638	18.833114
44.337787	1735.082686	18.838131
44.484212	1725.269425	18.843149
44.674685	1723.114930	18.848167
44.429281	1730.867742	18.853184
44.367913	1728.440332	18.858202
44.357459	1720.408504	18.863219
44.367657	1738.315342	18.868237
44.605712	1743.234451	18.873255
44.792674	1744.493528	18.878272
44.988687	1742.849079	18.883290
45.255960	1753.100154	18.888307
45.215921	1747.924844	18.893325
45.224789	1739.230440	18.898343
45.208548	1745.690220	18.903360
45.120037	1748.142719	18.908378
45.312665	1742.724655	18.913395
45.288443	1736.157525	18.918413
45.435765	1739.929950	18.923431
45.476391	1736.851308	18.928448
45.233973	1747.390716	18.933466
45.351010	1743.316291	18.938483
45.454146	1747.585727	18.943501
45.328973	1743.587937	18.948519
45.516851	1745.684562	18.953536
45.225756	1745.403531	18.958554
45.703662	1745.558351	18.963571
45.533358	1746.667829	18.968589
45.617493	1736.486748	18.973607
45.813419	1753.416760	18.978624
45.455061	1762.524913	18.983642
45.561986	1761.689976	18.988659
45.589223	1759.185131	18.993677
45.826140	1760.427490	18.998695
45.868267	1759.526104	19.003712
45.565475	1774.104774	19.008730
45.601592	1774.044050	19.013747
45.490972	1781.697261	19.018765
45.891910	1787.189204	19.023783
46.523060	1791.711321	19.028800
46.312827	1796.406923	19.033818
46.680471	1787.168809	19.038835
46.796923	1796.381569	19.043853
46.786146	1783.433183	19.048871
47.005593	1790.480736	19.053888
46.819672	1795.537830	19.058906
47.176400	1780.902716	19.063923
46.804143	1762.102543	19.068941
46.858960	1751.193899	19.073959
46.791486	1748.478552	19.078976
46.524554	1754.506194	19.083994
46.754284	1743.429298	19.089011
46.411751	1755.902752	19.094029
46.538843	1762.030424	19.099047
46.793188	1774.068486	19.104064
46.783199	1791.402211	19.109082
46.872396	1784.998974	19.114099
47.033392	1786.495390	19.119117
46.939289	1782.793209	19.124135
47.080770	1779.520944	19.129152
46.969105	1784.940328	19.134170
47.028168	1790.173645	19.139187
46.959521	1803.543506	19.144205
47.130741	1814.349411	19.149223
47.499497	1812.332156	19.154240
47.299678	1820.322531	19.159258
47.632618	1816.294290	19.164275
47.895963	1817.242555	19.169293
47.602775	1820.443573	19.174311
47.828228	1816.804313	19.179328
47.599562	1815.085956	19.184346
47.646378	1807.398320	19.189363
47.757290	1812.925012	19.194381
47.646184	1813.682230	19.199399
47.760875	1810.938737	19.204416
47.655773	1812.454524	19.209434
48.021818	1814.228638	19.214451
47.514366	1812.358342	19.219469
48.080972	1816.119367	19.224487
47.986514	1828.215505	19.229504
48.006203	1839.691476	19.234522
48.304771	1826.380355	19.239539
48.219587	1833.328087	19.244557
48.126003	1842.192751	19.249575
48.381694	1823.579647	19.254592
48.520192	1834.366567	19.259610
48.801491	1837.046914	19.264627
48.509695	1831.459488	19.269645
48.302259	1832.231247	19.274663
48.363050	1840.888136	19.279680
48.334368	1830.268009	19.284698
48.238685	1831.501957	19.289715
48.616997	1834.721527	19.294733
48.636623	1848.837387	19.299751
48.626408	1855.067501	19.304768
48.568315	1866.434902	19.309786
49.112134	1860.533022	19.314803
49.092750	1858.716894	19.319821
49.108766	1864.947598	19.324839
49.338319	1861.775907	19.329856
49.115907	1875.379484	19.334874
49.077231	1863.685116	19.339891
49.397121	1871.805951	19.344909
48.829331	1875.184628	19.349927
49.530329	1862.920635	19.354944
49.336120	1870.674702	19.359962
49.088882	1860.846101	19.364979
48.884751	1865.193902	19.369997
48.875286	1861.067524	19.375015
49.152193	1871.993982	19.380032
49.238154	1888.618334	19.385050
49.552227	1890.607913	19.390067
49.602516	1885.926042	19.395085
49.604943	1900.346924	19.400103
50.173689	1889.429627	19.405120
49.875828	1894.935915	19.410138
49.890968	1884.688390	19.415155
50.135357	1889.244924	19.420173
50.053749	1883.460361	19.425191
50.175798	1885.468681	19.430208
50.023819	1889.966122	19.435226
50.220390	1880.807988	19.440243
50.411691	1893.308680	19.445261
50.258520	1893.569953	19.450279
50.401627	1884.022466	19.455296
50.381982	1886.735231	19.460314
50.401010	1883.315087	19.465331
50.759844	1879.171538	19.470349
50.509278	1875.018469	19.475367
50.314423	1878.980530	19.480384
50.190191	1876.729609	19.485402
50.526812	1876.037595	19.490419
50.605768	1892.784356	19.495437
50.515563	1900.978290	19.500455
50.630121	1895.259131	19.505472
50.797479	1907.473073	19.510490
50.724028	1911.583960	19.515507
50.753217	1904.533965	19.520525
50.490676	1899.447336	19.525543
51.124541	1897.974979	19.530560
50.957958	1906.474813	19.535578
50.878498	1910.153667	19.540595
51.323516	1912.151923	19.545613
51.243470	1923.713132	19.550631
51.487491	1924.695697	19.555648
51.622938	1928.662827	19.560666
51.500981	1924.871917	19.565683
51.817045	1914.630348	19.570701
51.561671	1897.093042	19.575719
51.715723	1894.492620	19.580736
51.421007	1891.413266	19.585754
51.689410	1901.876436	19.590771
51.786970	1910.785726	19.595789
51.644407	1903.240350	19.600807
51.842008	1918.278929	19.605824
51.843573	1915.882030	19.610842
51.865357	1920.687739	19.615859
52.023739	1918.204302	19.620877
51.613596	1924.039359	19.625895
51.963787	1917.097911	19.630912
51.438003	1916.275601	19.635930
51.829671	1928.205077	19.640947
52.105564	1920.644670	19.645965
51.925301	1927.931155	19.650983
52.253459	1944.198844	19.656000
52.569908	1944.505926	19.661018
52.410358	1945.843931	19.666035
52.622142	1942.257289	19.671053
52.505120	1945.295574	19.676071
52.380483	1943.656065	19.681088
52.236083	1940.482183	19.686106
52.335090	1946.246103	19.691123
52.741900	1935.553938	19.696141
52.250549	1954.098378	19.701159
52.288052	1942.717705	19.706176
52.462919	1959.135138	19.711194
52.721005	1968.062812	19.716211
53.274773	1960.143310	19.721229
53.388248	1976.736244	19.726247
53.488135	1970.038871	19.731264
53.423263	1978.639248	19.736282
53.254772	1963.635878	19.741299
53.246380	1962.335193	19.746317
53.389221	1963.368728	19.751335
53.593406	1973.523103	19.756352
53.441410	1966.276863	19.761370
53.261044	1971.490757	19.766387
53.840971	1964.956555	19.771405
53.644448	1971.439332	19.776423
54.058561	1953.185681	19.781440
53.829267	1945.410546	19.786458
53.342554	1937.844472	19.791475
53.506412	1941.374869	19.796493
53.665614	1954.185017	19.801511
53.609860	1953.102374	19.806528
53.498082	1954.553930	19.811546
53.665259	1950.511712	19.816563
54.186865	1949.355116	19.821581
53.692374	1966.290410	19.826599
54.228857	1970.893966	19.831616
54.007216	1977.596425	19.836634
53.734470	1989.235192	19.841651
53.961831	1979.855201	19.846669
53.815734	1987.199841	19.851687
54.272080	1991.123998	19.856704
53.910570	2001.484262	19.861722
54.066185	2013.370340	19.866739
54.082991	2006.322738	19.871757
54.170370	2014.125414	19.876775
54.178135	2012.827369	19.881792
54.947230	2021.745032	19.886810
55.157142	2026.723800	19.891827
55.379537	2029.322191	19.896845
55.006441	2010.173658	19.901863
55.339464	2010.177244	19.906880
55.466144	2007.401817	19.911898
55.016287	2004.080387	19.916915
55.273616	2003.033200	19.921933
54.938672	2003.662077	19.926951
54.817051	2003.172935	19.931968
55.017174	2000.725891	19.936986
55.082716	2028.261364	19.942003
55.314365	2030.828308	19.947021
55.307360	2032.831599	19.952039
55.637010	2030.633985	19.957056
55.667606	2027.174499	19.962074
55.862166	2037.608630	19.967091
56.064829	2027.180234	19.972109
55.789465	2021.795908	19.977127
55.697953	2024.016883	19.982144
56.064101	2024.071683	19.987162
55.729744	2033.347861	19.992179
55.978213	2026.648939	19.997197
56.155255	2026.741485	20.002215
55.973139	2029.197489	20.007232
56.330410	2021.399592	20.012250
56.041658	2035.981897	20.017267
56.494226	2013.843058	20.022285
56.456084	2020.414829	20.027303
56.359279	2023.978871	20.032320
56.417593	2025.582427	20.037338
56.309908	2019.239381	20.042355
56.642887	2014.544415	20.047373
56.597895	2025.454105	20.052391
56.635777	2019.858976	20.057408
56.471558	2019.364473	20.062426
56.473223	2022.538263	20.067443
56.833348	2017.413654	20.072461
56.781397	2024.241424	20.077479
56.444601	2019.722680	20.082496
56.457309	2013.159958	20.087514
56.363382	2035.574660	20.092531
56.757436	2040.727118	20.097549
56.706251	2050.527915	20.102567
57.278325	2044.462650	20.107584
57.234395	2042.635007	20.112602
57.333862	2056.290662	20.117619
57.348501	2047.439633	20.122637
57.200867	2055.200858	20.127655
57.117199	2049.351618	20.132672
57.408921	2053.114431	20.137690
57.247163	2079.414252	20.142707
57.407223	2071.851262	20.147725
57.476864	2075.054180	20.152743
57.908762	2075.336873	20.157760
57.523994	2062.418758	20.162778
57.465518	2070.863814	20.167795
57.925221	2059.860489	20.172813
57.989305	2067.349945	20.177831
57.952987	2084.194893	20.182848
58.118008	2079.610135	20.187866
58.009669	2086.021699	20.192883
58.535508	2082.924810	20.197901
58.335486	2090.249278	20.202919
58.421450	2083.664776	20.207936
58.651745	2096.559349	20.212954
58.449636	2096.870046	20.217971
58.707728	2091.812466	20.222989
58.717335	2091.858474	20.228007
58.275064	2092.928083	20.233024
58.567405	2086.535833	20.238042
58.533756	2084.710030	20.243059
58.655464	2078.660518	20.248077
58.487780	2095.494315	20.253095
58.378061	2087.778474	20.258112
58.746151	2087.444211	20.263130
58.187551	2102.924241	20.268147
58.584449	2102.820038	20.273165
58.713310	2115.185769	20.278183
58.868476	2123.308173	20.283200
59.003276	2099.012474	20.288218
58.765242	2126.091838	20.293235
59.218208	2138.020599	20.298253
59.240532	2130.561436	20.303271
59.656520	2151.141019	20.308288
59.132598	2135.059702	20.313306
59.282428	2157.945870	20.318323
59.676257	2143.418249	20.323341
59.625486	2149.409143	20.328359
59.484436	2144.647404	20.333376
59.652444	2151.757161	20.338394
59.756548	2175.242394	20.343411
59.908563	2172.877478	20.348429
60.246032	2171.565878	20.353447
60.201221	2167.573003	20.358464
60.716339	2163.560824	20.363482
60.302615	2152.213227	20.368499
60.410334	2122.526772	20.373517
60.373430	2121.497100	20.378535
60.498679	2126.301521	20.383552
60.436193	2118.562704	20.388570
60.459383	2125.691066	20.393587
60.464823	2120.285892	20.398605
60.660633	2134.557529	20.403623
60.687277	2153.304772	20.408640
61.003701	2151.765569	20.413658
60.792038	2157.963746	20.418675
61.350154	2149.539340	20.423693
60.914696	2127.875204	20.428711
60.831629	2116.660770	20.433728
60.944098	2127.472865	20.438746
60.897727	2138.244685	20.443763
60.956686	2146.505431	20.448781
61.118728	2149.300808	20.453799
60.949070	2141.776719	20.458816
61.039036	2148.209668	20.463834
60.954893	2153.252029	20.468851
61.081470	2144.596601	20.473869
61.398005	2157.518703	20.478887
61.547634	2174.988871	20.483904
61.867671	2164.162082	20.488922
62.043320	2171.144022	20.493939
61.744231	2163.852513	20.498957
61.633299	2174.187625	20.503975
61.264383	2180.799164	20.508992
61.650603	2177.171833	20.514010
61.741981	2173.835724	20.519027
61.688998	2169.505055	20.524045
61.758545	2184.298936	20.529063
61.207630	2194.797312	20.534080
61.919011	2205.993719	20.539098
61.982549	2205.090147	20.544115
62.344168	2212.666125	20.549133
62.623833	2229.306273	20.554151
62.612978	2230.463445	20.559168
63.036816	2224.854854	20.564186
62.977772	2225.572191	20.569203
62.569050	2202.185368	20.574221
62.827485	2190.576682	20.579239
62.888941	2194.101423	20.584256
62.971523	2187.558377	20.589274
62.764750	2195.246774	20.594291
63.061890	2194.631345	20.599309
62.957761	2205.470626	20.604327
63.063234	2229.110426	20.609344
63.357348	2216.547084	20.614362
62.910868	2217.615625	20.619379
63.020189	2223.978878	20.624397
63.468091	2218.796789	20.629415
63.131539	2229.468605	20.634432
63.140972	2233.275158	20.639450
63.184028	2223.341469	20.644467
63.296894	2218.610576	20.649485
63.394375	2238.461675	20.654503
63.495687	2257.277999	20.659520
63.872624	2251.824380	20.664538
63.542179	2258.330391	20.669555
63.826277	2267.938531	20.674573
63.848830	2255.046047	20.679591
63.566824	2262.885285	20.684608
63.605820	2257.512703	20.689626
63.476388	2267.576548	20.694643
64.108306	2270.086444	20.699661
64.047788	2272.400552	20.704679
64.213821	2275.832249	20.709696
64.608622	2272.250719	20.714714
64.370334	2275.854339	20.719731
64.322253	2274.587939	20.724749
64.551228	2285.679490	20.729767
64.454783	2284.873408	20.734784
64.380468	2292.194126	20.739802
64.957092	2317.434813	20.744819
64.857486	2306.473545	20.749837
64.850789	2305.464457	20.754855
64.647687	2313.310365	20.759872
64.785547	2302.828127	20.764890
64.802429	2310.610518	20.769907
64.923051	2309.392610	20.774925
65.473575	2302.953474	20.779943
65.570062	2311.276014	20.784960
65.153877	2310.951473	20.789978
65.314907	2320.374881	20.794995
65.473517	2324.242034	20.800013
65.505033	2330.204834	20.805031
65.365359	2330.982741	20.810048
65.572902	2334.800278	20.815066
65.872669	2339.752686	20.820083
65.786976	2334.738452	20.825101
65.936361	2335.413085	20.830119
65.534548	2330.164892	20.835136
65.695121	2334.875556	20.840154
65.966827	2347.048787	20.845171
66.253651	2357.302743	20.850189
66.235296	2353.926071	20.855207
66.442982	2362.298368	20.860224
66.491625	2357.891605	20.865242
66.507261	2359.931745	20.870259
66.667748	2359.367826	20.875277
66.902927	2356.930089	20.880295
66.432768	2360.154556	20.885312
66.849652	2346.335088	20.890330
66.789921	2350.000944	20.895347
66.708928	2362.668461	20.900365
66.939353	2346.128829	20.905383
66.622752	2355.815816	20.910400
66.765703	2345.889359	20.915418
67.164842	2359.910298	20.920435
67.180721	2352.043856	20.925453
66.883184	2358.919442	20.930471
67.207453	2379.855801	20.935488
67.426852	2364.123424	20.940506
67.335830	2376.722339	20.945523
67.358689	2375.451098	20.950541
67.593846	2369.550233	20.955559
67.361755	2373.616006	20.960576
67.317504	2365.272718	20.965594
67.607230	2369.544366	20.970611
67.733272	2383.331539	20.975629
67.477946	2381.262234	20.980647
67.408265	2401.910991	20.985664
67.936095	2398.068687	20.990682
68.075763	2395.662277	20.995699
68.002212	2391.329434	21.000717
68.051045	2396.175699	21.005735
68.007582	2390.773000	21.010752
68.009244	2398.404418	21.015770
68.509664	2417.016215	21.020787
68.454119	2432.463441	21.025805
68.623360	2428.179633	21.030823
68.507933	2424.967007	21.035840
68.416981	2428.555173	21.040858
68.868918	2425.231471	21.045875
68.726839	2422.335432	21.050893
69.290267	2416.396248	21.055911
69.113247	2414.289197	21.060928
69.479249	2415.565001	21.065946
69.068814	2410.329621	21.070963
69.159644	2424.682649	21.075981
69.092536	2414.719998	21.080999
69.002670	2426.202699	21.086016
69.714284	2411.339855	21.091034
69.339985	2412.724607	21.096051
69.429186	2413.010201	21.101069
69.332601	2406.053197	21.106087
69.298108	2415.679236	21.111104
69.481465	2435.161698	21.116122
69.632777	2434.194990	21.121139
69.333436	2453.972972	21.126157
69.522684	2449.585663	21.131175
69.682577	2450.879979	21.136192
70.007175	2448.112710	21.141210
70.022544	2466.140002	21.146227
69.859136	2470.437347	21.151245
70.406793	2464.868836	21.156263
70.434641	2456.674007	21.161280
70.211591	2454.666086	21.166298
70.709306	2453.537811	21.171315
70.568004	2451.686843	21.176333
70.388590	2453.206114	21.181351
70.512695	2461.026174	21.186368
70.749397	2458.515341	21.191386
70.773371	2457.462201	21.196403
70.583533	2473.502093	21.201421
70.855903	2476.096633	21.206439
70.800564	2483.916438	21.211456
71.159927	2480.629280	21.216474
71.429249	2483.392228	21.221491
71.375772	2480.440792	21.226509
71.531833	2482.774257	21.231527
71.603331	2476.495108	21.236544
71.607328	2481.860192	21.241562
72.052982	2475.032043	21.246579
71.581021	2477.466333	21.251597
72.160499	2469.166564	21.256615
71.610708	2485.222054	21.261632
71.617825	2470.278929	21.266650
72.117882	2475.784269	21.271667
71.622656	2474.036464	21.276685
71.817885	2462.498842	21.281703
71.831337	2471.982159	21.286720
71.992735	2493.896901	21.291738
72.201050	2500.691518	21.296755
72.108271	2506.089925	21.301773
71.974303	2508.708116	21.306791
71.892290	2507.970695	21.311808
72.181346	2505.638789	21.316826
72.588115	2511.936278	21.321843
72.872717	2518.898995	21.326861
72.819558	2515.146567	21.331879
72.717365	2506.189393	21.336896
72.643020	2520.863486	21.341914
73.140342	2515.253278	21.346931
72.906777	2519.632501	21.351949
73.114472	2519.737504	21.356967
73.029459	2521.001040	21.361984
73.037752	2521.766119	21.367002
73.092371	2521.663755	21.372019
73.184485	2528.351216	21.377037
73.069964	2516.448033	21.382055
73.255935	2528.797573	21.387072
73.390036	2539.603036	21.392090
73.953737	2543.768636	21.397107
73.674042	2544.582092	21.402125
73.703477	2543.206016	21.407143
73.763438	2543.913348	21.412160
73.824839	2551.979825	21.417178
73.869932	2546.278597	21.422195
73.534321	2555.810986	21.427213
73.845752	2572.687186	21.432231
73.953201	2582.533361	21.437248
73.859290	2582.968502	21.442266
74.216038	2577.929893	21.447283
74.486488	2587.258616	21.452301
74.670322	2574.865167	21.457319
74.927992	2577.481051	21.462336
75.050416	2580.223215	21.467354
75.354423	2561.287086	21.472371
75.292046	2559.417157	21.477389
75.356068	2557.788924	21.482407
75.221369	2555.467589	21.487424
75.289819	2547.131563	21.492442
75.433205	2551.184348	21.497459
75.203686	2557.061245	21.502477
75.425326	2557.346610	21.507495
75.478876	2552.505346	21.512512
75.473220	2556.915812	21.517530
75.240746	2546.597748	21.522547
75.347927	2552.718987	21.527565
75.384996	2568.714592	21.532583
75.504667	2580.079914	21.537600
75.745566	2590.619355	21.542618
76.132337	2582.710600	21.547635
76.049208	2590.657288	21.552653
76.047352	2590.898881	21.557671
76.203494	2574.354746	21.562688
76.250932	2578.455676	21.567706
76.352503	2568.591422	21.572723
76.095223	2581.864985	21.577741
76.166252	2582.023672	21.582759
76.271961	2608.501048	21.587776
76.301164	2609.703201	21.592794
76.535446	2605.783968	21.597811
76.257587	2617.800800	21.602829
76.344537	2610.054562	21.607847
76.507448	2627.775788	21.612864
76.629680	2653.387962	21.617882
76.754666	2639.210979	21.622899
76.455494	2659.032893	21.627917
77.113513	2657.370270	21.632935
77.511350	2668.315697	21.637952
77.453382	2673.438345	21.642970
77.581438	2663.197234	21.647987
78.061679	2666.000357	21.653005
78.067822	2657.302934	21.658023
77.874998	2635.240725	21.663040
77.576274	2622.262844	21.668058
77.914190	2629.233729	21.673075
77.784851	2627.055190	21.678093
77.708582	2639.553658	21.683111
77.768673	2654.379079	21.688128
77.600918	2663.659399	21.693146
77.810457	2665.749423	21.698163
77.999525	2662.920659	21.703181
77.785998	2674.136790	21.708199
78.377198	2678.002231	21.713216
78.240462	2681.942687	21.718234
78.341385	2690.870768	21.723251
78.292995	2701.515566	21.728269
78.412468	2686.470205	21.733287
78.366764	2695.270559	21.738304
78.577176	2724.024804	21.743322
78.832590	2722.755458	21.748339
78.996250	2722.172106	21.753357
79.169824	2727.239188	21.758375
79.519081	2721.165604	21.763392
79.144313	2725.770176	21.768410
79.495295	2718.355037	21.773427
79.339940	2726.972751	21.778445
79.528351	2716.555891	21.783463
79.502761	2713.007904	21.788480
79.615035	2722.228208	21.793498
79.739367	2737.666683	21.798515
79.728563	2738.109747	21.803533
79.737513	2732.791963	21.808551
80.214858	2738.084823	21.813568
80.164085	2740.254091	21.818586
80.360823	2740.754981	21.823603
80.331639	2734.383315	21.828621
80.449282	2727.520484	21.833639
80.227661	2722.691175	21.838656
79.994265	2738.247815	21.843674
80.758592	2732.950478	21.848691
80.367060	2747.369144	21.853709
80.572640	2754.189915	21.858727
80.763326	2773.084613	21.863744
80.511779	2781.477713	21.868762
80.897410	2767.680357	21.873779
80.980890	2770.919912	21.878797
80.698790	2760.729190	21.883815
81.112064	2770.560775	21.888832
81.149830	2784.867988	21.893850
81.374684	2785.384312	21.898867
81.211633	2791.032213	21.903885
81.178134	2798.829081	21.908903
81.849863	2782.465262	21.913920
81.791303	2791.662657	21.918938
81.806665	2787.123680	21.923955
81.907014	2791.200963	21.928973
81.508177	2785.199793	21.933991
81.482470	2798.682507	21.939008
81.752172	2818.703522	21.944026
82.130309	2817.855602	21.949043
82.280210	2812.682602	21.954061
81.907093	2816.367284	21.959079
82.521809	2821.833528	21.964096
82.224001	2821.445713	21.969114
82.607385	2828.232411	21.974131
82.731883	2831.974233	21.979149
82.616214	2833.249159	21.984167
83.011142	2828.269513	21.989184
82.823624	2828.052835	21.994202
83.120748	2828.153692	21.999219
82.630726	2829.284188	22.004237
82.845142	2831.945451	22.009255
83.184566	2823.290888	22.014272
82.862028	2834.930643	22.019290
83.160353	2843.706120	22.024307
83.570868	2862.497676	22.029325
83.378842	2853.209687	22.034343
83.712150	2850.960965	22.039360
83.669572	2855.659889	22.044378
83.617189	2855.815745	22.049395
83.760503	2851.720546	22.054413
83.481829	2851.914977	22.059431
83.865346	2859.776818	22.064448
84.180647	2871.137979	22.069466
84.562426	2870.504800	22.074483
84.209379	2878.118694	22.079501
84.347464	2874.314892	22.084519
84.581169	2870.014209	22.089536
84.665121	2881.765167	22.094554
84.954225	2870.805996	22.099571
84.830180	2874.274345	22.104589
84.628399	2871.814053	22.109607
84.696413	2859.372590	22.114624
84.829307	2871.703223	22.119642
84.810132	2870.201299	22.124659
85.351984	2880.181386	22.129677
85.461542	2893.205234	22.134695
85.652144	2882.660348	22.139712
85.583226	2895.464094	22.144730
85.707938	2885.211185	22.149747
85.690465	2880.492574	22.154765
85.715172	2897.731851	22.159783
86.053634	2887.999896	22.164800
86.161799	2892.004657	22.169818
86.047353	2889.514183	22.174835
86.470824	2896.637187	22.179853
85.734837	2886.253285	22.184871
85.958388	2890.025208	22.189888
85.950550	2900.603601	22.194906
86.234878	2894.341474	22.199923
86.537279	2889.318045	22.204941
85.983083	2891.303996	22.209959
86.536922	2901.892328	22.214976
86.678761	2911.485404	22.219994
86.582957	2915.732529	22.225011
86.435436	2908.335504	22.230029
86.513762	2913.663654	22.235047
86.929738	2906.703022	22.240064
86.775701	2933.031363	22.245082
87.178303	2942.836477	22.250099
87.146380	2940.930762	22.255117
87.415834	2936.217869	22.260135
87.424975	2924.887221	22.265152
87.303597	2941.484964	22.270170
87.412911	2929.757065	22.275187
87.808639	2936.622871	22.280205
87.479132	2957.535178	22.285223
87.955261	2955.163633	22.290240
88.018573	2966.386589	22.295258
87.952459	2960.948065	22.300275
88.340397	2949.724090	22.305293
87.948521	2966.227192	22.310311
88.247304	2965.099868	22.315328
88.259165	2966.502939	22.320346
88.314399	2977.244578	22.325363
88.435538	2976.223770	22.330381
88.532515	2980.963055	22.335399
88.937352	2968.942207	22.340416
89.010821	2973.681437	22.345434
88.886908	2969.311479	22.350451
89.177127	2979.255655	22.355469
88.901503	2988.807923	22.360487
89.105784	2976.307236	22.365504
89.091137	2978.119398	22.370522
89.060027	2982.612929	22.375539
89.186266	2999.944593	22.380557
89.229147	3000.780749	22.385575
89.342851	3008.163646	22.390592
89.604955	3013.955934	22.395610
89.333633	3023.350824	22.400627
89.723066	3023.542333	22.405645
89.605959	3036.527775	22.410663
89.915833	3031.004656	22.415680
90.105451	3038.813200	22.420698
90.147270	3034.897711	22.425715
90.561924	3035.678341	22.430733
90.365361	3031.342810	22.435751
90.344231	3027.713701	22.440768
90.597225	3040.950973	22.445786
90.409151	3055.875265	22.450803
90.810042	3046.343125	22.455821
90.613992	3054.587441	22.460839
90.806208	3049.874286	22.465856
90.764084	3058.652207	22.470874
90.734935	3074.168741	22.475891
91.112508	3078.658545	22.480909
91.189809	3092.222915	22.485927
91.408864	3088.825749	22.490944
91.758840	3093.787428	22.495962
91.789811	3096.449917	22.500979
92.086278	3087.075949	22.505997
91.729820	3086.157675	22.511015
92.294438	3087.122183	22.516032
92.213259	3072.702895	22.521050
92.051964	3084.896490	22.526067
92.347016	3077.031775	22.531085
92.125916	3073.932535	22.536103
92.349970	3089.996598	22.541120
92.742795	3093.327225	22.546138
93.015903	3098.676794	22.551155
92.862612	3096.834027	22.556173
92.720603	3101.114034	22.561191
92.796425	3088.932113	22.566208
93.041729	3089.974188	22.571226
92.993393	3097.668936	22.576243
93.026121	3093.217155	22.581261
93.058635	3094.495962	22.586279
93.204800	3092.771818	22.591296
93.561344	3094.149833	22.596314
93.219460	3111.853063	22.601331
93.455298	3110.065675	22.606349
93.640756	3129.589610	22.611367
93.781079	3133.539121	22.616384
93.774006	3126.418776	22.621402
93.538415	3124.600235	22.626419
93.951877	3117.977712	22.631437
93.693430	3141.565070	22.636455
93.922424	3149.512435	22.641472
94.315535	3144.145990	22.646490
94.267643	3139.400438	22.651507
94.505566	3152.901313	22.656525
94.637438	3156.617193	22.661543
94.824776	3141.808203	22.666560
94.420431	3143.787139	22.671578
94.660032	3179.234886	22.676595
94.983705	3174.445641	22.681613
94.985816	3180.444729	22.686631
95.184972	3184.624684	22.691648
95.421656	3178.378190	22.696666
95.217167	3183.181131	22.701683
95.472962	3187.734791	22.706701
95.319631	3190.719476	22.711719
95.430544	3182.300502	22.716736
95.717823	3173.182720	22.721754
95.136448	3180.044744	22.726771
95.426783	3192.056316	22.731789
95.745713	3204.315136	22.736807
95.557149	3205.979295	22.741824
95.684841	3218.254373	22.746842
95.750118	3239.227805	22.751859
96.022617	3238.828021	22.756877
95.837231	3245.853769	22.761895
96.251280	3256.795361	22.766912
96.314007	3267.002113	22.771930
96.412072	3270.736205	22.776947
96.335991	3265.764174	22.781965
96.721849	3277.439954	22.786983
96.839803	3289.841105	22.792000
96.989713	3287.856876	22.797018
96.653951	3293.729165	22.802035
97.066179	3288.033533	22.807053
97.238472	3313.836162	22.812071
97.934075	3307.196859	22.817088
98.223949	3308.148121	22.822106
97.925032	3315.758795	22.827123
98.126837	3296.529215	22.832141
98.188608	3305.958603	22.837159
97.955599	3303.397891	22.842176
98.131215	3301.586575	22.847194
98.113052	3305.862315	22.852211
98.501967	3305.598015	22.857229
98.485348	3303.717679	22.862247
98.294924	3299.290508	22.867264
98.558310	3297.119812	22.872282
98.549973	3326.265256	22.877299
98.691249	3324.004893	22.882317
98.881481	3331.535928	22.887335
98.712316	3330.517399	22.892352
99.226584	3329.248539	22.897370
98.891093	3340.112867	22.902387
99.477321	3340.814376	22.907405
99.244178	3356.264901	22.912423
99.412942	3355.294467	22.917440
99.696136	3355.238579	22.922458
99.676358	3372.774708	22.927475
99.505301	3367.626607	22.932493
99.514994	3363.091941	22.937511
99.343041	3361.526239	22.942528
99.658818	3399.565813	22.947546
100.220403	3383.540824	22.952563
100.390819	3390.882643	22.957581
100.491731	3398.258392	22.962599
100.456488	3393.427602	22.967616
100.818275	3395.790598	22.972634
100.634687	3397.857495	22.977651
101.161938	3412.230466	22.982669
100.917593	3411.891279	22.987687
101.283093	3410.537941	22.992704
101.343707	3404.548403	22.997722
101.475367	3406.684468	23.002739
101.311016	3408.546221	23.007757
101.242377	3396.429662	23.012775
101.384158	3409.311220	23.017792
101.370945	3404.813791	23.022810
101.325603	3412.103478	23.027827
101.411893	3416.190730	23.032845
101.910221	3427.955126	23.037863
101.795619	3439.996009	23.042880
101.917842	3441.482067	23.047898
101.672827	3449.471298	23.052915
101.867601	3441.856827	23.057933
101.586860	3460.084205	23.062951
102.172528	3465.148002	23.067968
102.340823	3469.664236	23.072986
102.391641	3469.292416	23.078003
102.679295	3490.476292	23.083021
103.128186	3489.365073	23.088039
103.223974	3486.378346	23.093056
103.884057	3480.797988	23.098074
103.422422	3485.895874	23.103091
103.653373	3463.863639	23.108109
103.693904	3485.440704	23.113127
103.709033	3489.208238	23.118144
103.906055	3478.827635	23.123162
103.661490	3489.946333	23.128179
103.940612	3480.168303	23.133197
103.980321	3482.953036	23.138215
104.031967	3485.463751	23.143232
104.016936	3476.087872	23.148250
104.185508	3474.779668	23.153267
104.066030	3470.352142	23.158285
104.293349	3491.355044	23.163303
104.063395	3507.371727	23.168320
104.305852	3500.984780	23.173338
104.192343	3509.777508	23.178355
104.425649	3515.347579	23.183373
104.472576	3532.959480	23.188391
104.550894	3542.449270	23.193408
104.851127	3553.485077	23.198426
104.922167	3562.232379	23.203443
105.528877	3557.061996	23.208461
105.946161	3567.274532	23.213479
105.734432	3567.124440	23.218496
105.857994	3557.045689	23.223514
105.752187	3558.936762	23.228531
106.230329	3549.143519	23.233549
106.105604	3554.571584	23.238567
105.928664	3561.825213	23.243584
105.978155	3562.192982	23.248602
106.228979	3584.482682	23.253619
106.582871	3586.422208	23.258637
106.501488	3596.154562	23.263655
106.452084	3589.876830	23.268672
106.712490	3590.651484	23.273690
106.555813	3593.919084	23.278707
106.669842	3612.279046	23.283725
106.925266	3605.971410	23.288743
106.892996	3611.901937	23.293760
107.161529	3610.224053	23.298778
107.293104	3620.765333	23.303795
107.301384	3642.862909	23.308813
107.303946	3639.591950	23.313831
107.128508	3645.520556	23.318848
107.726682	3650.750855	23.323866
107.945658	3661.819063	23.328883
107.759106	3667.093602	23.333901
108.088859	3670.306825	23.338919
107.748248	3671.406781	23.343936
108.372358	3665.968918	23.348954
108.768492	3675.796828	23.353971
109.046470	3676.034325	23.358989
108.997322	3662.369440	23.364007
108.787842	3653.080310	23.369024
108.868680	3656.528363	23.374042
109.222687	3671.980213	23.379059
109.418796	3665.853222	23.384077
109.548921	3679.230636	23.389095
109.631217	3680.788670	23.394112
109.907436	3676.696098	23.399130
109.542943	3657.995477	23.404147
109.670630	3666.160244	23.409165
109.958003	3680.792397	23.414183
109.863455	3685.978510	23.419200
109.993028	3671.248641	23.424218
109.956976	3672.093152	23.429235
109.886972	3678.259075	23.434253
110.371034	3666.512005	23.439271
110.238100	3672.922973	23.444288
109.964336	3683.103317	23.449306
110.170901	3698.032306	23.454323
110.289664	3694.909852	23.459341
110.463339	3701.148906	23.464359
110.420742	3720.178586	23.469376
110.698922	3720.433767	23.474394
110.942338	3728.194005	23.479411
111.003513	3741.079709	23.484429
111.594705	3746.730098	23.489447
111.649253	3756.934588	23.494464
111.894281	3746.987219	23.499482
112.281133	3739.720397	23.504499
111.963825	3747.166600	23.509517
112.319104	3741.299110	23.514535
112.333268	3748.440144	23.519552
112.287467	3737.335702	23.524570
112.464162	3740.591160	23.529587
112.226689	3740.947690	23.534605
112.391855	3747.675184	23.539623
112.204219	3761.263051	23.544640
112.700386	3775.079677	23.549658
112.665726	3783.992210	23.554675
112.672001	3782.093072	23.559693
112.699543	3782.005018	23.564711
112.844988	3801.120655	23.569728
113.198624	3804.742172	23.574746
113.364543	3800.470939	23.579763
113.295541	3804.161899	23.584781
113.715074	3813.543896	23.589799
113.434047	3838.219919	23.594816
113.659497	3820.089352	23.599834
113.821278	3835.129812	23.604851
113.754052	3836.130273	23.609869
113.784011	3851.147254	23.614887
113.951789	3863.144166	23.619904
114.209804	3862.788101	23.624922
114.387523	3868.949388	23.629939
114.384656	3882.809986	23.634957
114.935416	3882.307515	23.639975
114.787375	3886.473376	23.644992
115.035663	3884.317300	23.650010
114.948190	3871.145584	23.655027
115.559458	3892.203699	23.660045
116.002378	3899.876726	23.665063
115.827773	3896.896017	23.670080
116.011334	3884.029907	23.675098
115.732646	3880.344729	23.680115
115.745487	3899.986742	23.685133
115.854355	3907.728751	23.690151
115.847992	3914.799630	23.695168
115.688587	3902.783502	23.700186
116.046028	3912.736464	23.705203
116.129696	3929.079326	23.710221
116.203209	3941.086362	23.715239
116.326046	3945.795291	23.720256
116.409714	3937.644591	23.725274
116.529094	3937.730736	23.730291
116.475033	3958.224057	23.735309
116.906977	3949.450039	23.740327
116.817645	3969.311784	23.745344
117.075764	3968.169063	23.750362
117.247701	3983.731627	23.755379
117.369921	3989.057618	23.760397
117.858745	3982.214793	23.765415
117.946082	3990.455691	23.770432
118.080278	4004.991410	23.775450
118.241744	3989.343737	23.780467
117.996063	3992.580850	23.785485
118.255445	3976.803621	23.790503
118.532614	3987.197860	23.795520
118.535554	3998.621308	23.800538
118.607962	3993.220164	23.805555
118.653994	4010.287068	23.810573
118.856772	4004.887607	23.815591
118.821523	4013.420042	23.820608
118.809638	4004.682321	23.825626
118.601808	4019.910416	23.830643
118.756486	4038.722448	23.835661
119.012650	4036.411109	23.840679
119.220364	4055.661657	23.845696
119.323007	4063.296894	23.850714
119.693452	4071.372153	23.855731
119.654322	4078.786328	23.860749
120.165480	4060.698825	23.865767
119.860557	4085.937869	23.870784
120.051980	4091.384749	23.875802
120.664587	4095.175755	23.880819
120.162192	4098.660041	23.885837
120.592501	4101.920127	23.890855
120.848082	4112.266047	23.895872
121.088085	4120.132168	23.900890
120.865374	4113.370637	23.905907
121.080210	4131.376354	23.910925
121.232802	4122.816122	23.915943
121.232464	4120.758186	23.920960
121.285926	4129.431938	23.925978
121.603090	4138.082987	23.930995
121.541193	4150.408241	23.936013
121.795785	4146.032888	23.941031
122.118980	4152.227732	23.946048
122.031476	4142.914216	23.951066
122.099273	4147.681516	23.956083
122.262640	4175.600523	23.961101
122.658232	4175.804422	23.966119
122.699342	4166.613347	23.971136
122.408795	4186.605078	23.976154
122.628796	4165.296133	23.981171
122.884996	4187.116105	23.986189
123.156850	4191.896553	23.991207
123.304284	4195.289625	23.996224
123.488613	4188.587974	24.001242
123.780020	4196.827940	24.006259
123.826338	4196.923797	24.011277
123.603048	4198.985153	24.016295
123.281721	4186.086074	24.021312
123.058589	4206.359223	24.026330
123.794597	4206.422223	24.031347
123.527758	4231.524494	24.036365
124.316112	4238.165763	24.041383
124.961418	4238.880788	24.046400
124.715387	4244.540957	24.051418
125.157067	4243.633253	24.056435
124.856726	4234.241460	24.061453
125.084116	4242.459350	24.066471
125.309217	4243.649340	24.071488
125.066364	4233.041300	24.076506
125.428365	4241.525148	24.081523
125.287485	4245.006425	24.086541
125.398699	4245.704186	24.091559
125.654489	4236.660676	24.096576
125.457490	4254.869238	24.101594
125.621043	4263.109106	24.106611
125.848926	4269.309115	24.111629
126.062698	4258.399610	24.116647
126.512424	4259.302473	24.121664
126.508940	4267.419543	24.126682
126.619860	4253.613116	24.131699
126.310493	4291.931017	24.136717
127.039178	4294.839465	24.141735
126.963551	4301.244765	24.146752
126.812789	4300.292030	24.151770
127.114142	4295.380931	24.156787
127.037237	4300.541103	24.161805
127.109904	4313.201355	24.166823
127.043644	4324.818770	24.171840
127.586705	4326.503894	24.176858
127.530430	4319.491138	24.181875
127.624328	4347.382560	24.186893
127.975467	4333.524559	24.191911
127.847710	4351.157196	24.196928
127.886822	4353.901631	24.201946
128.408112	4372.034557	24.206963
128.274571	4382.524093	24.211981
128.469037	4383.693564	24.216999
128.927262	4392.725014	24.222016
128.720170	4412.860733	24.227034
128.773691	4408.724843	24.232051
128.859374	4415.663410	24.237069
128.832816	4424.065491	24.242087
128.978363	4435.097170	24.247104
129.108868	4435.837425	24.252122
129.154367	4446.719098	24.257139
129.518879	4468.590863	24.262157
129.589895	4462.441316	24.267175
129.955252	4469.355349	24.272192
129.850105	4498.536307	24.277210
130.415621	4481.799266	24.282227
130.213178	4500.615350	24.287245
130.101830	4504.834371	24.292263
129.998329	4514.343773	24.297280
130.099727	4530.554800	24.302298
130.769756	4543.789805	24.307315
130.653086	4566.251880	24.312333
130.911896	4566.641784	24.317351
131.249947	4577.076756	24.322368
131.297528	4598.801846	24.327386
131.832535	4582.809160	24.332403
131.836348	4599.591146	24.337421
131.927451	4589.095802	24.342439
132.193207	4603.457968	24.347456
132.222237	4612.891197	24.352474
132.454109	4611.470859	24.357491
132.778797	4611.300627	24.362509
132.963261	4615.544820	24.367527
133.318483	4605.378291	24.372544
133.450300	4597.454741	24.377562
133.746708	4577.149216	24.382579
133.969657	4582.571373	24.387597
134.183737	4588.708039	24.392615
134.229908	4558.808580	24.397632
133.714378	4551.590877	24.402650
133.940587	4541.893768	24.407667
133.964454	4544.516338	24.412685
134.151754	4542.873828	24.417703
134.307284	4538.787982	24.422720
134.031684	4547.873449	24.427738
134.173561	4543.159108	24.432755
134.352707	4570.095049	24.437773
134.253121	4584.803018	24.442791
134.562657	4573.556582	24.447808
134.520585	4581.923515	24.452826
135.117977	4589.763501	24.457843
134.886792	4601.538697	24.462861
134.853622	4610.731791	24.467879
134.975343	4604.428523	24.472896
135.174517	4628.379552	24.477914
135.152559	4639.991062	24.482931
134.990526	4643.061325	24.487949
135.234103	4659.224975	24.492967
135.173495	4671.817770	24.497984
135.492220	4690.234164	24.503002
136.018508	4698.923419	24.508019
136.042620	4713.901249	24.513037
136.307599	4728.178219	24.518055
136.586913	4737.280381	24.523072
136.186026	4736.725276	24.528090
136.586142	4753.984900	24.533107
136.883312	4755.120106	24.538125
137.098588	4764.539188	24.543143
137.515402	4765.092375	24.548160
137.695731	4793.742029	24.553178
138.143335	4783.277026	24.558195
138.035922	4786.616661	24.563213
138.388430	4792.349401	24.568231
138.473755	4777.887238	24.573248
138.545310	4788.424660	24.578266
138.673422	4789.301165	24.583283
138.657815	4775.066330	24.588301
138.521697	4781.176678	24.593319
138.708389	4783.644814	24.598336
138.329966	4800.582309	24.603354
138.883066	4805.564920	24.608371
138.975778	4812.041440	24.613389
138.925288	4824.890975	24.618407
139.023670	4840.592150	24.623424
139.459850	4841.396099	24.628442
139.846585	4847.129897	24.633459
140.282293	4858.831709	24.638477
139.961768	4855.483160	24.643495
140.456755	4860.083626	24.648512
140.265232	4850.882946	24.653530
140.631419	4854.666432	24.658547
140.865078	4853.420989	24.663565
140.601678	4869.455618	24.668583
140.754811	4869.964182	24.673600
140.287423	4883.939043	24.678618
140.950169	4886.321447	24.683635
141.233194	4899.992391	24.688653
141.333758	4917.798982	24.693671
141.505932	4911.727040	24.698688
141.954302	4916.023386	24.703706
142.076927	4910.583704	24.708723
141.904838	4931.108436	24.713741
141.564467	4947.326350	24.718759
142.132142	4949.648089	24.723776
142.286311	4955.589269	24.728794
142.522893	4969.641998	24.733811
142.406020	4979.992552	24.738829
142.947057	4978.777421	24.743847
143.115175	4973.129000	24.748864
142.879151	4987.764214	24.753882
142.833659	4983.175591	24.758899
143.346165	4985.742300	24.763917
143.284118	5003.693192	24.768935
143.422671	5004.027775	24.773952
143.569758	5013.064143	24.778970
143.848621	5014.596132	24.783987
144.112023	5030.965574	24.789005
143.798296	5039.256760	24.794023
144.547538	5033.409135	24.799040
144.473697	5046.321772	24.804058
144.665572	5056.218172	24.809075
145.038994	5061.145115	24.814093
144.646028	5072.734776	24.819111
144.868786	5069.244438	24.824128
145.143069	5077.083331	24.829146
145.092969	5079.476456	24.834163
145.560447	5078.695561	24.839181
145.502078	5089.163306	24.844199
145.760983	5098.033594	24.849216
145.793825	5107.103068	24.854234
145.903054	5113.058427	24.859251
146.533444	5112.642779	24.864269
146.439340	5123.805892	24.869287
146.659312	5138.536784	24.874304
146.809670	5139.124171	24.879322
146.896444	5136.470938	24.884339
147.285929	5133.929122	24.889357
147.406886	5137.067694	24.894375
147.591336	5150.584261	24.899392
147.757863	5157.533031	24.904410
147.690957	5148.801399	24.909427
148.404954	5153.750057	24.914445
148.103396	5153.454142	24.919463
148.258071	5151.000733	24.924480
148.416726	5153.653502	24.929498
148.074813	5148.644862	24.934515
148.269596	5165.912885	24.939533
148.668185	5183.942218	24.944551
148.950672	5178.405548	24.949568
148.952894	5193.147666	24.954586
148.981183	5215.798555	24.959603
148.991236	5203.721924	24.964621
149.183825	5224.952614	24.969639
149.473708	5222.528827	24.974656
149.566935	5240.642544	24.979674
149.527187	5243.575382	24.984691
149.851695	5237.365927	24.989709
149.699656	5253.269542	24.994727
150.205908	5261.527730	24.999744
150.213105	5274.776022	25.004762
150.275284	5271.213736	25.009779
150.629968	5285.779579	25.014797
150.828030	5294.266287	25.019815
150.592987	5296.264365	25.024832
150.547496	5311.396805	25.029850
150.785605	5321.245966	25.034867
151.436203	5330.963977	25.039885
151.469043	5349.902853	25.044903
151.692107	5358.688650	25.049920
151.831503	5345.983773	25.054938
152.179824	5355.560778	25.059955
152.519656	5364.003231	25.064973
152.480168	5378.629960	25.069991
152.761508	5375.478341	25.075008
152.767718	5361.588621	25.080026
152.940655	5366.469645	25.085043
153.330329	5364.301034	25.090061
153.359592	5368.295848	25.095079
153.630528	5362.138508	25.100096
153.388383	5362.164306	25.105114
153.246230	5373.902532	25.110131
153.548831	5385.626342	25.115149
153.748645	5392.419304	25.120167
153.770566	5397.357578	25.125184
154.271476	5411.183149	25.130202
154.249016	5426.098876	25.135219
154.586224	5424.842186	25.140237
154.175239	5427.430051	25.145255
154.627871	5447.274604	25.150272
154.746861	5456.583621	25.155290
154.666482	5460.943469	25.160307
155.063601	5480.906306	25.165325
155.028401	5487.125466	25.170343
155.081452	5488.486914	25.175360
155.310844	5516.963625	25.180378
155.526857	5514.169668	25.185395
155.784208	5524.464261	25.190413
155.910519	5547.818029	25.195431
156.017047	5552.466746	25.200448
156.276206	5550.160600	25.205466
156.001894	5581.101281	25.210483
156.524445	5579.328457	25.215501
156.853879	5597.813061	25.220519
157.196424	5604.704201	25.225536
157.454909	5606.603840	25.230554
157.759128	5614.297487	25.235571
158.051809	5606.066102	25.240589
157.822279	5602.876394	25.245607
157.895055	5620.805715	25.250624
158.401928	5626.569959	25.255642
158.123493	5637.344153	25.260659
158.362496	5632.176370	25.265677
158.551083	5647.397639	25.270695
158.493126	5657.234900	25.275712
159.057248	5662.484904	25.280730
158.864863	5659.329603	25.285747
159.313452	5673.864936	25.290765
159.431262	5684.013769	25.295783
159.819880	5685.376096	25.300800
160.068388	5677.582347	25.305818
159.634830	5682.214422	25.310835
160.100609	5680.572639	25.315853
160.269271	5705.306451	25.320871
160.232049	5714.906037	25.325888
160.390899	5704.872048	25.330906
160.660937	5718.228881	25.335923
160.636049	5731.730928	25.340941
160.516147	5746.335848	25.345959
161.078039	5748.929966	25.350976
161.462196	5752.921364	25.355994
161.540172	5766.792326	25.361011
161.573453	5771.066147	25.366029
161.838603	5776.560500	25.371047
161.859436	5788.559549	25.376064
162.041939	5788.824675	25.381082
161.962628	5792.197680	25.386099
162.134036	5795.910023	25.391117
162.285197	5824.256497	25.396135
162.225788	5829.291428	25.401152
162.592487	5846.056922	25.406170
162.714515	5862.544704	25.411187
162.732555	5875.594832	25.416205
163.013600	5890.097804	25.421223
163.211618	5893.902639	25.426240
163.626213	5897.601600	25.431258
163.662323	5899.817982	25.436275
164.088534	5907.553438	25.441293
164.069649	5907.823491	25.446311
164.330309	5916.626623	25.451328
164.760870	5908.548703	25.456346
164.930991	5909.761692	25.461363
164.863227	5919.500328	25.466381
165.409199	5931.601722	25.471399
165.630793	5931.190209	25.476416
166.076241	5933.333448	25.481434
166.134904	5941.788021	25.486451
166.290247	5926.258343	25.491469
166.062767	5927.899289	25.496487
165.920853	5924.621403	25.501504
166.496471	5931.583251	25.506522
166.219506	5933.110308	25.511539
166.159830	5947.139628	25.516557
166.222206	5953.787014	25.521575
166.368973	5951.886843	25.526592
166.671409	5979.489199	25.531610
166.489500	6002.446471	25.536627
166.956654	5997.796865	25.541645
167.079673	6021.378691	25.546663
167.132313	6022.414217	25.551680
167.888923	6040.247172	25.556698
168.202105	6050.617546	25.561715
168.136589	6054.721912	25.566733
168.507040	6054.687440	25.571751
168.431458	6071.178166	25.576768
168.772391	6067.821257	25.581786
168.809970	6087.859240	25.586803
168.994594	6082.696357	25.591821
169.407704	6100.122282	25.596839
169.634603	6115.225846	25.601856
169.792561	6107.194443	25.606874
169.636608	6107.682455	25.611891
169.902066	6098.411045	25.616909
170.129181	6127.189291	25.621927
170.345968	6137.889088	25.626944
170.476541	6135.393833	25.631962
170.293949	6146.970786	25.636979
170.858275	6163.110953	25.641997
171.246756	6165.041553	25.647015
170.784788	6175.128994	25.652032
171.208775	6172.899479	25.657050
171.229915	6185.707579	25.662067
171.553336	6187.576479	25.667085
171.635394	6188.906419	25.672103
171.890751	6213.398323	25.677120
171.878200	6212.980602	25.682138
172.160193	6225.117967	25.687156
172.311918	6225.259030	25.692173
172.649292	6237.490421	25.697191
172.513646	6249.526702	25.702208
172.763468	6248.361568	25.707226
173.033929	6276.065022	25.712244
173.102344	6273.247673	25.717261
173.279485	6286.747529	25.722279
173.676228	6299.715749	25.727296
173.614388	6311.928105	25.732314
173.834862	6316.730300	25.737332
173.941616	6327.738223	25.742349
174.176961	6336.419767	25.747367
174.089842	6347.158109	25.752384
174.404153	6358.383773	25.757402
174.609687	6363.549934	25.762420
175.063638	6370.028840	25.767437
175.064982	6368.922080	25.772455
174.769346	6377.714219	25.777472
175.403018	6389.679409	25.782490
175.361795	6394.836736	25.787508
175.446156	6395.862321	25.792525
175.611747	6414.774641	25.797543
175.660071	6441.445601	25.802560
176.288416	6449.395218	25.807578
175.860598	6464.358432	25.812596
176.159640	6473.585537	25.817613
176.336268	6491.368354	25.822631
176.820214	6504.593251	25.827648
177.284943	6517.663825	25.832666
177.958720	6515.971842	25.837684
178.206254	6515.740317	25.842701
178.323671	6507.732735	25.847719
178.313539	6505.874961	25.852736
178.768417	6497.283179	25.857754
178.974819	6499.232881	25.862772
179.017758	6499.699067	25.867789
178.979450	6500.757529	25.872807
179.083599	6516.671676	25.877824
179.408363	6506.663316	25.882842
179.500592	6517.727327	25.887860
179.720626	6512.389130	25.892877
179.654471	6517.136364	25.897895
179.852317	6529.506020	25.902912
180.126034	6533.520594	25.907930
180.288322	6539.624846	25.912948
180.166830	6548.663951	25.917965
180.919277	6565.895717	25.922983
181.059350	6575.750054	25.928000
181.206472	6560.286476	25.933018
181.282957	6568.476186	25.938036
181.356364	6568.284457	25.943053
181.637709	6564.244242	25.948071
181.746893	6582.078470	25.953088
181.581477	6593.706467	25.958106
181.949733	6599.590060	25.963124
182.082186	6606.670326	25.968141
182.114178	6624.678019	25.973159
182.568143	6628.940843	25.978176
183.049188	6619.542937	25.983194
182.900868	6636.768465	25.988212
182.702856	6643.685196	25.993229
183.217519	6642.221106	25.998247
183.075579	6658.053198	26.003264
183.481557	6659.928204	26.008282
183.463921	6657.984233	26.013300
183.870493	6699.375789	26.018317
183.956916	6696.965709	26.023335
184.025891	6718.763446	26.028352
184.147252	6720.696512	26.033370
184.505462	6739.264735	26.038388
184.533387	6752.934558	26.043405
185.121024	6775.517722	26.048423
184.882144	6775.935974	26.053440
185.298367	6788.706851	26.058458
185.543011	6804.645330	26.063476
185.523007	6807.243631	26.068493
185.989978	6814.091516	26.073511
185.850059	6834.813459	26.078528
186.436475	6831.887583	26.083546
186.432627	6853.284853	26.088564
186.906574	6857.521600	26.093581
187.104180	6855.949214	26.098599
186.998395	6852.638386	26.103616
187.441800	6848.736712	26.108634
187.886774	6870.144904	26.113652
188.128662	6870.535701	26.118669
188.095350	6879.613980	26.123687
188.204317	6888.555346	26.128704
188.561407	6884.648235	26.133722
188.343217	6886.169607	26.138740
188.256588	6891.700819	26.143757
188.308855	6906.040915	26.148775
188.585258	6912.053213	26.153792
188.808283	6936.888668	26.158810
189.080178	6948.461209	26.163828
188.910067	6953.825882	26.168845
189.671328	6958.720063	26.173863
189.430385	6981.346707	26.178880
189.956189	6998.039892	26.183898
189.859855	7011.591069	26.188916
190.310967	7018.301476	26.193933
190.242673	7029.146644	26.198951
190.594002	7038.112631	26.203968
190.577405	7060.050992	26.208986
191.096934	7077.347009	26.214004
191.146087	7087.178097	26.219021
191.732776	7096.278498	26.224039
191.489329	7106.146917	26.229056
191.726842	7118.902699	26.234074
192.124509	7127.038845	26.239092
192.023638	7144.917080	26.244109
192.611783	7151.179607	26.249127
192.452923	7149.357358	26.254144
193.077250	7168.586218	26.259162
193.132654	7179.448856	26.264180
193.089092	7187.506719	26.269197
193.737999	7194.956355	26.274215
193.506930	7209.931868	26.279232
193.858516	7210.246268	26.284250
193.949395	7224.004546	26.289268
193.908222	7244.673694	26.294285
194.087796	7254.523505	26.299303
194.480656	7261.042806	26.304320
194.759754	7287.491983	26.309338
195.013946	7296.624598	26.314356
195.188065	7304.558344	26.319373
195.531065	7307.384220	26.324391
195.572563	7333.589987	26.329408
195.854602	7340.948304	26.334426
196.248730	7335.050228	26.339444
196.423730	7353.743959	26.344461
196.325394	7367.140615	26.349479
196.570475	7371.942219	26.354496
196.543334	7374.532342	26.359514
196.699827	7384.033205	26.364532
196.884486	7396.048940	26.369549
197.423674	7413.821726	26.374567
197.447903	7431.505557	26.379584
197.930689	7451.678065	26.384602
198.070621	7454.449309	26.389620
197.865340	7469.487753	26.394637
198.283610	7482.074558	26.399655
198.182627	7500.117822	26.404672
198.794326	7513.053892	26.409690
199.275256	7517.904784	26.414708
199.295120	7530.426713	26.419725
199.435403	7532.348877	26.424743
199.555117	7547.934638	26.429760
199.641526	7556.377618	26.434778
200.125023	7550.978215	26.439796
200.240824	7560.080291	26.444813
200.444550	7569.309614	26.449831
200.620993	7576.277509	26.454848
200.827666	7570.858466	26.459866
201.008860	7573.810364	26.464884
200.982168	7603.724866	26.469901
201.349994	7601.416225	26.474919
201.646754	7611.626523	26.479936
201.603359	7623.885678	26.484954
202.176210	7640.007057	26.489972
201.892941	7642.400897	26.494989
202.312685	7656.589595	26.500007
202.284048	7669.082630	26.505024
202.166569	7686.656266	26.510042
202.759945	7692.369970	26.515060
202.658947	7710.750574	26.520077
202.911537	7731.239502	26.525095
203.294553	7740.294381	26.530112
203.245741	7755.667970	26.535130
203.838547	7766.069677	26.540148
204.198890	7782.110534	26.545165
204.199592	7792.478557	26.550183
204.870093	7806.740951	26.555200
205.039841	7806.673486	26.560218
205.986272	7800.053104	26.565236
206.044225	7801.332819	26.570253
206.097605	7796.175313	26.575271
206.270829	7799.435741	26.580288
205.988906	7792.459896	26.585306
206.616704	7809.692361	26.590324
206.628187	7825.367165	26.595341
206.485317	7818.391175	26.600359
207.013240	7827.822272	26.605376
207.035642	7834.909459	26.610394
207.291175	7850.314768	26.615412
207.101795	7856.201970	26.620429
207.605032	7881.397450	26.625447
207.837644	7887.611901	26.630464
207.845063	7891.303793	26.635482
208.128500	7900.077496	26.640500
208.110760	7923.111249	26.645517
208.535300	7924.011419	26.650535
208.583585	7942.168358	26.655552
208.530896	7950.046176	26.660570
209.128756	7965.551773	26.665588
208.852036	7993.330539	26.670605
209.380755	8004.113177	26.675623
209.427408	8018.059821	26.680640
209.883486	8042.790774	26.685658
210.066559	8049.275754	26.690676
210.173058	8054.979458	26.695693
210.593755	8073.803574	26.700711
210.785937	8079.539600	26.705728
210.984524	8106.123171	26.710746
211.228737	8105.272311	26.715764
211.416580	8113.126221	26.720781
211.738194	8129.947285	26.725799
212.007409	8127.498124	26.730816
212.274082	8145.451447	26.735834
212.256700	8153.939463	26.740852
212.895164	8154.412847	26.745869
212.894552	8157.859598	26.750887
212.922033	8193.854678	26.755904
213.083209	8190.875951	26.760922
213.470909	8194.779967	26.765940
213.997396	8223.606306	26.770957
214.434046	8220.185876	26.775975
214.598103	8218.253438	26.780992
214.693055	8216.630932	26.786010
214.856422	8224.336927	26.791028
214.976511	8215.501810	26.796045
215.110292	8209.473936	26.801063
215.411677	8224.173399	26.806080
215.552567	8238.248016	26.811098
215.786376	8232.482431	26.816116
215.371759	8252.750677	26.821133
216.077121	8251.185629	26.826151
216.373882	8255.389024	26.831168
216.267914	8270.466952	26.836186
216.802934	8268.555918	26.841204
216.833585	8287.973240	26.846221
216.766015	8303.435525	26.851239
217.005450	8309.519055	26.856256
217.361971	8329.803341	26.861274
217.769237	8339.407484	26.866292
217.530787	8354.695628	26.871309
217.825463	8362.063363	26.876327
218.212912	8370.184514	26.881344
218.496503	8384.800426	26.886362
218.653803	8391.838007	26.891380
218.873041	8419.296129	26.896397
219.148019	8417.680878	26.901415
219.018563	8431.741261	26.906432
219.298576	8459.420193	26.911450
219.945362	8477.563138	26.916468
219.934570	8494.525366	26.921485
220.389887	8503.586068	26.926503
220.575153	8510.587575	26.931520
220.512380	8514.640926	26.936538
221.071042	8532.313301	26.941556
220.957538	8551.165598	26.946573
221.122788	8557.620651	26.951591
221.365827	8575.121528	26.956608
221.600428	8594.268443	26.961626
222.182195	8595.399453	26.966644
222.352592	8613.154972	26.971661
222.635821	8620.055275	26.976679
222.861709	8625.033719	26.981696
222.538671	8632.246075	26.986714
223.143138	8644.502949	26.991732
223.531336	8676.973042	26.996749
223.593222	8684.080079	27.001767
223.956187	8683.166247	27.006784
224.038962	8699.364957	27.011802
224.225479	8721.665891	27.016820
224.498256	8721.807460	27.021837
224.640994	8737.233057	27.026855
225.167395	8755.742784	27.031872
224.840962	8758.544053	27.036890
225.422962	8773.663173	27.041908
225.827269	8789.372484	27.046925
225.886491	8815.795958	27.051943
226.013603	8830.706729	27.056960
225.689485	8840.819551	27.061978
226.237695	8853.347388	27.066996
226.707038	8867.920453	27.072013
227.086306	8881.786120	27.077031
227.507740	8890.012986	27.082048
227.964001	8919.638292	27.087066
227.975994	8903.987597	27.092084
228.563665	8911.804989	27.097101
228.476556	8916.760409	27.102119
228.719909	8922.980583	27.107136
228.916644	8947.632136	27.112154
229.510588	8932.580779	27.117172
229.325881	8941.854602	27.122189
229.499956	8947.684518	27.127207
230.177381	8943.022167	27.132224
230.022618	8955.626060	27.137242
230.243405	8956.251977	27.142260
230.515344	8959.589282	27.147277
230.404763	8957.133431	27.152295
230.609220	8960.221953	27.157312
230.726079	8975.396063	27.162330
231.165388	8982.337689	27.167348
231.368892	8997.692848	27.172365
231.294946	9015.805046	27.177383
231.762436	9023.659679	27.182400
231.784778	9034.027301	27.187418
232.223741	9044.363116	27.192436
232.527905	9068.271655	27.197453
232.562711	9068.985018	27.202471
232.822747	9082.087607	27.207488
232.960540	9099.923888	27.212506
233.077887	9119.453931	27.217524
233.590248	9123.628239	27.222541
233.537826	9137.775766	27.227559
233.981753	9146.007714	27.232576
233.889677	9177.265594	27.237594
234.318224	9197.660394	27.242612
234.484700	9202.279412	27.247629
234.876056	9219.502860	27.252647
234.991831	9243.963450	27.257664
235.126469	9269.766334	27.262682
235.055937	9288.114584	27.267700
235.630651	9307.009244	27.272717
235.859330	9325.293135	27.277735
236.327353	9341.272098	27.282752
236.427895	9359.529150	27.287770
236.737609	9375.678451	27.292788
237.084637	9395.773472	27.297805
237.120048	9416.899899	27.302823
237.367151	9422.234279	27.307840
237.643663	9451.448376	27.312858
238.227173	9457.984354	27.317876
238.636039	9472.247375	27.322893
238.336040	9486.204531	27.327911
239.027039	9490.954377	27.332928
239.092614	9526.542090	27.337946
239.357668	9527.282812	27.342964
239.853483	9527.273325	27.347981
239.823421	9548.602155	27.352999
240.467623	9544.366543	27.358016
240.927231	9561.656280	27.363034
240.991657	9574.475725	27.368052
241.276353	9565.515776	27.373069
241.592474	9578.974216	27.378087
241.576167	9586.785392	27.383104
241.697150	9598.270592	27.388122
241.953498	9593.427135	27.393140
242.611738	9620.776205	27.398157
242.237067	9636.764723	27.403175
242.603214	9631.730606	27.408192
242.356009	9660.231305	27.413210
242.607171	9662.291378	27.418228
242.920080	9677.437704	27.423245
243.177900	9700.290655	27.428263
243.574100	9717.211361	27.433280
243.583816	9738.435409	27.438298
243.973750	9761.667566	27.443316
244.453871	9759.990720	27.448333
244.583376	9777.348623	27.453351
245.166367	9765.927296	27.458368
245.322043	9781.196588	27.463386
245.701021	9788.883476	27.468404
246.563180	9802.388165	27.473421
246.453015	9812.020403	27.478439
246.862854	9808.923884	27.483456
246.865523	9804.217590	27.488474
247.049817	9799.368646	27.493492
247.042884	9809.847164	27.498509
246.899602	9821.904744	27.503527
247.443073	9836.311273	27.508544
247.483723	9849.186069	27.513562
247.500943	9862.225441	27.518580
247.971237	9870.360460	27.523597
247.824409	9889.697991	27.528615
248.126766	9901.110906	27.533632
248.372056	9929.273131	27.538650
248.661501	9945.608324	27.543668
248.691347	9954.798447	27.548685
248.937886	9989.345857	27.553703
249.687639	10001.282809	27.558720
249.931562	10019.423189	27.563738
250.036910	10039.325786	27.568756
250.505971	10048.066076	27.573773
250.770780	10063.850112	27.578791
251.018295	10080.688640	27.583808
251.165768	10092.796852	27.588826
251.551130	10111.843490	27.593844
251.706016	10125.772525	27.598861
251.868651	10143.561756	27.603879
252.054818	10158.803528	27.608896
252.568744	10174.706425	27.613914
252.821597	10192.376037	27.618932
253.182028	10195.082188	27.623949
253.507968	10203.887171	27.628967
253.811729	10231.017787	27.633984
253.936431	10241.975840	27.639002
254.180556	10260.137729	27.644020
254.317664	10266.625698	27.649037
254.488197	10296.328346	27.654055
254.914585	10298.113778	27.659072
255.410228	10306.077045	27.664090
255.641914	10305.522759	27.669108
255.776325	10315.462285	27.674125
255.618283	10336.501367	27.679143
256.055032	10375.121535	27.684160
256.477188	10375.048599	27.689178
256.660501	10383.799260	27.694196
257.035154	10401.263860	27.699213
257.150972	10427.915402	27.704231
257.723405	10430.648013	27.709248
257.922345	10444.058011	27.714266
257.893215	10451.875667	27.719284
258.492162	10477.793641	27.724301
258.665472	10475.598660	27.729319
258.688295	10498.616045	27.734336
259.029656	10514.636808	27.739354
259.101667	10513.748107	27.744372
259.343787	10544.829770	27.749389
259.241407	10577.991363	27.754407
259.914799	10589.178042	27.759424
260.003107	10598.935512	27.764442
260.276218	10620.631618	27.769460
260.567947	10644.363393	27.774477
260.628455	10668.225572	27.779495
260.999164	10697.410634	27.784512
261.395218	10712.391383	27.789530
262.003403	10720.512723	27.794548
262.444973	10734.664338	27.799565
262.628350	10745.558687	27.804583
262.765079	10750.083811	27.809600
263.083919	10757.260394	27.814618
263.095947	10772.758398	27.819636
263.234809	10773.735878	27.824653
263.192466	10804.437287	27.829671
263.480903	10813.744309	27.834688
263.918374	10846.528943	27.839706
263.703942	10853.346222	27.844724
264.311062	10868.506518	27.849741
264.551072	10884.013442	27.854759
264.717715	10914.216537	27.859776
265.172618	10930.463956	27.864794
265.358242	10953.877342	27.869812
266.002433	10964.137963	27.874829
266.029268	10982.671376	27.879847
266.252671	11011.564663	27.884864
266.608925	11022.874944	27.889882
266.616624	11048.433830	27.894900
267.095079	11062.436266	27.899917
267.357927	11080.915832	27.904935
267.425393	11099.017266	27.909952
268.189152	11118.520160	27.914970
268.061437	11156.632032	27.919988
268.515933	11162.368377	27.925005
268.671641	11175.716018	27.930023
268.979747	11194.716053	27.935040
269.527055	11207.244326	27.940058
269.536904	11227.955902	27.945076
270.197967	11244.516994	27.950093
270.450715	11262.388690	27.955111
270.819155	11270.213537	27.960128
270.842564	11283.114392	27.965146
270.802686	11306.259099	27.970164
271.267002	11315.594864	27.975181
271.666590	11335.129829	27.980199
272.176069	11346.087303	27.985216
272.703540	11352.709743	27.990234
273.005945	11374.628915	27.995252
273.545532	11376.588780	28.000269
273.356534	11389.425551	28.005287
273.381732	11404.710860	28.010304
273.815058	11411.662421	28.015322
273.628058	11430.384512	28.020340
274.486950	11448.750271	28.025357
274.787449	11477.383504	28.030375
274.849787	11486.385580	28.035392
274.965215	11489.771338	28.040410
275.043614	11520.923696	28.045428
275.547828	11528.729390	28.050445
275.298553	11554.564725	28.055463
275.727850	11575.907807	28.060480
276.321415	11593.844100	28.065498
276.415645	11611.201154	28.070516
276.883167	11627.166738	28.075533
276.995170	11660.260481	28.080551
277.148969	11672.055296	28.085568
277.540997	11689.059140	28.090586
277.380040	11725.946507	28.095604
277.744717	11747.138205	28.100621
277.929182	11770.102344	28.105639
278.273594	11791.116251	28.110656
278.524404	11819.904048	28.115674
278.905071	11853.171238	28.120692
279.896123	11852.511141	28.125709
280.782746	11858.522985	28.130727
281.026162	11873.684452	28.135744
281.461060	11850.901376	28.140762
281.274547	11873.969497	28.145780
281.290683	11867.326281	28.150797
281.471622	11887.042213	28.155815
281.474822	11901.591079	28.160832
281.926265	11919.333779	28.165850
281.990205	11931.007337	28.170868
281.971974	11954.465315	28.175885
282.119480	11980.260989	28.180903
282.326423	11998.786300	28.185920
282.662207	12021.743131	28.190938
282.863672	12040.609736	28.195956
283.240046	12073.711073	28.200973
283.627044	12095.811846	28.205991
283.388581	12132.631803	28.211008
284.144166	12148.077616	28.216026
284.463750	12178.390963	28.221044
284.771044	12202.172104	28.226061
285.169661	12221.957264	28.231079
285.375637	12244.502550	28.236096
285.918674	12270.275885	28.241114
286.242817	12291.458453	28.246132
286.754779	12302.545378	28.251149
286.882578	12319.360344	28.256167
287.012387	12340.452966	28.261184
287.735623	12360.996143	28.266202
287.555810	12380.589500	28.271220
287.664441	12404.157166	28.276237
288.283824	12440.043526	28.281255
288.509688	12455.388070	28.286272
288.793226	12465.501253	28.291290
288.769206	12496.456547	28.296308
289.527770	12511.568172	28.301325
289.954508	12533.024823	28.306343
289.845772	12546.180937	28.311360
290.399148	12567.774283	28.316378
290.665337	12581.571247	28.321396
291.228767	12607.042368	28.326413
291.410940	12629.363648	28.331431
291.324772	12639.530141	28.336448
292.413904	12645.772761	28.341466
292.473094	12669.108687	28.346484
293.316476	12678.330625	28.351501
293.431120	12681.650585	28.356519
293.620361	12684.669865	28.361536
294.476890	12702.957884	28.366554
294.536033	12709.488873	28.371572
294.899320	12721.065489	28.376589
294.819911	12724.173280	28.381607
294.983247	12747.337693	28.386624
295.394652	12745.240159	28.391642
295.066878	12769.283054	28.396660
295.315636	12792.943954	28.401677
295.662354	12800.968529	28.406695
295.285231	12833.865798	28.411712
295.747302	12862.314863	28.416730
295.906093	12894.597423	28.421748
296.154346	12915.841409	28.426765
296.705090	12949.735907	28.431783
296.921503	12982.921476	28.436800
297.688139	13005.605258	28.441818
297.844789	13027.122946	28.446836
297.814940	13053.854116	28.451853
298.307952	13078.105379	28.456871
298.771887	13104.381601	28.461888
298.958837	13133.172839	28.466906
298.898250	13156.480407	28.471924
299.843935	13176.341026	28.476941
300.224198	13200.428312	28.481959
300.476783	13206.839302	28.486976
301.021408	13226.463695	28.491994
301.101556	13250.532880	28.497012
301.232720	13261.311499	28.502029
301.709104	13281.476692	28.507047
302.006406	13303.571880	28.512064
302.250574	13315.415999	28.517082
302.421769	13326.049379	28.522100
302.875772	13344.782816	28.527117
303.421108	13373.532607	28.532135
303.179161	13387.885368	28.537152
303.654341	13398.738034	28.542170
303.966918	13426.355565	28.547188
304.178481	13447.161939	28.552205
304.775839	13469.069112	28.557223
304.678980	13488.735195	28.562240
305.101397	13502.154159	28.567258
305.305145	13534.485720	28.572276
305.336723	13553.809201	28.577293
306.088562	13579.865294	28.582311
306.314059	13597.398196	28.587328
306.699298	13604.099437	28.592346
307.422403	13624.977533	28.597364
307.780696	13642.255325	28.602381
307.971002	13652.285380	28.607399
308.277887	13670.387965	28.612416
308.022755	13694.836241	28.617434
308.591537	13716.750047	28.622452
308.955073	13744.878145	28.627469
309.034186	13773.069039	28.632487
309.080695	13782.828254	28.637504
309.649560	13811.311773	28.642522
310.340066	13840.520612	28.647540
310.456077	13869.495067	28.652557
311.315806	13873.519489	28.657575
311.682043	13903.295734	28.662592
312.015737	13890.662276	28.667610
312.553992	13913.629321	28.672628
312.860407	13927.680803	28.677645
313.411082	13936.293129	28.682663
313.171004	13956.391581	28.687680
313.660908	13965.680542	28.692698
313.855201	13970.635936	28.697716
313.910405	13996.840884	28.702733
314.573489	14005.842819	28.707751
314.356703	14019.947725	28.712768
314.621983	14039.641319	28.717786
315.165798	14057.063824	28.722804
315.212601	14071.476642	28.727821
315.812100	14094.979069	28.732839
315.892886	14122.552560	28.737856
316.220746	14132.467213	28.742874
316.139441	14147.985451	28.747892
316.519656	14177.302892	28.752909
317.053147	14199.229485	28.757927
317.153643	14223.375545	28.762944
317.448393	14261.166495	28.767962
317.368861	14283.870525	28.772980
318.028534	14310.165220	28.777997
318.728759	14334.577968	28.783015
318.810756	14362.867113	28.788032
319.316566	14386.300344	28.793050
319.377307	14404.438109	28.798068
319.583376	14431.372104	28.803085
320.392419	14460.036133	28.808103
320.360872	14482.648992	28.813120
320.794712	14502.709272	28.818138
321.459821	14533.529390	28.823156
321.714317	14534.866215	28.828173
322.202461	14545.588289	28.833191
322.304659	14570.662784	28.838208
322.679362	14582.557181	28.843226
323.154082	14598.972078	28.848244
323.168516	14624.532349	28.853261
323.690441	14632.487919	28.858279
323.956525	14650.032588	28.863296
324.288797	14664.751773	28.868314
324.484264	14677.503201	28.873332
324.503422	14698.773189	28.878349
325.265011	14711.150604	28.883367
325.014931	14744.148938	28.888384
325.607810	14764.043011	28.893402
325.964230	14786.451940	28.898420
326.014831	14823.461901	28.903437
326.702547	14839.172087	28.908455
327.016756	14864.706849	28.913472
327.255269	14890.911319	28.918490
327.541468	14909.838187	28.923508
327.792974	14941.836864	28.928525
328.131279	14968.768814	28.933543
328.240799	14991.355920	28.938560
328.587379	15014.986565	28.943578
329.226578	15042.434690	28.948596
329.395662	15067.141160	28.953613
329.887592	15098.917617	28.958631
330.082646	15127.592854	28.963648
330.562621	15144.042105	28.968666
330.865479	15180.417067	28.973684
331.094532	15193.254756	28.978701
331.670910	15204.422869	28.983719
331.916545	15238.322128	28.988736
332.317700	15267.502541	28.993754
332.853028	15286.092407	28.998772
332.786558	15308.743698	29.003789
333.299066	15328.149006	29.008807
333.778722	15359.110069	29.013824
334.132826	15386.011731	29.018842
334.340044	15412.192265	29.023860
334.468493	15442.417213	29.028877
335.458151	15449.801057	29.033895
335.815513	15468.905935	29.038912
336.130943	15484.974535	29.043930
336.409113	15496.025060	29.048948
336.544095	15518.903400	29.053965
336.805504	15531.143437	29.058983
336.982353	15566.075982	29.064000
337.449968	15597.780204	29.069018
337.800591	15606.079753	29.074036
337.922766	15643.903995	29.079053
338.363897	15666.369483	29.084071
338.589194	15697.336961	29.089088
338.808229	15723.139375	29.094106
338.817928	15741.863878	29.099124
339.104171	15787.831386	29.104141
339.211140	15830.542641	29.109159
339.495538	15861.150788	29.114176
340.277891	15897.919364	29.119194
340.392289	15929.693614	29.124212
340.608553	15976.262646	29.129229
341.131476	16006.045219	29.134247
341.523136	16038.183645	29.139264
341.644507	16085.832490	29.144282
342.302272	16107.528361	29.149300
342.572077	16143.373494	29.154317
343.135287	16164.683168	29.159335
343.266330	16202.776739	29.164352
343.640683	16225.788311	29.169370
344.386176	16242.945010	29.174388
344.598241	16277.729832	29.179405
345.436875	16284.049952	29.184423
345.633050	16309.466203	29.189440
345.900979	16334.467167	29.194458
346.243642	16351.989983	29.199476
346.489674	16380.225574	29.204493
347.081725	16392.898641	29.209511
347.238523	16421.279860	29.214528
347.609569	16439.122751	29.219546
348.053929	16459.922884	29.224564
348.094689	16494.657662	29.229581
348.836858	16508.599982	29.234599
348.538634	16535.176300	29.239616
348.947296	16567.383879	29.244634
349.371218	16589.531957	29.249652
349.219482	16629.558239	29.254669
349.945612	16656.023842	29.259687
350.620118	16694.774267	29.264704
350.886692	16720.885619	29.269722
351.386543	16750.001937	29.274740
351.726185	16769.889859	29.279757
352.879535	16786.806381	29.284775
352.984322	16801.940190	29.289792
353.261157	16825.252414	29.294810
354.114322	16831.606601	29.299828
354.252053	16851.617817	29.304845
354.306379	16867.076821	29.309863
354.676795	16886.855778	29.314880
355.044383	16903.911688	29.319898
355.231446	16919.580503	29.324916
355.081028	16954.098807	29.329933
355.488206	16977.432270	29.334951
355.680520	17003.939339	29.339968
355.761337	17038.194232	29.344986
356.502552	17073.705033	29.350004
356.949100	17115.119957	29.355021
357.348265	17142.638059	29.360039
357.614924	17174.053844	29.365056
358.106142	17199.717471	29.370074
358.504994	17216.245258	29.375092
358.830276	17258.233805	29.380109
358.732694	17290.740791	29.385127
359.466027	17310.499708	29.390144
359.709848	17349.765730	29.395162
360.380249	17387.791858	29.400180
360.429044	17418.642005	29.405197
361.155028	17438.080751	29.410215
361.570711	17464.799120	29.415232
361.676847	17496.694401	29.420250
361.952342	17515.052321	29.425268
362.375639	17544.255198	29.430285
362.804150	17585.946965	29.435303
363.382490	17599.414479	29.440320
363.332415	17629.067688	29.445338
364.414672	17661.123575	29.450356
364.055630	17685.191456	29.455373
364.710170	17708.411011	29.460391
365.183781	17741.672519	29.465408
365.165106	17770.579980	29.470426
365.829330	17797.292506	29.475444
366.085691	17823.309570	29.480461
366.712644	17857.438114	29.485479
366.896026	17879.980740	29.490496
367.186904	17909.452029	29.495514
367.788200	17928.303535	29.500532
368.230328	17953.528801	29.505549
368.581443	17977.752476	29.510567
368.985664	17991.283754	29.515584
369.150206	18014.340374	29.520602
369.464624	18022.169535	29.525620
369.428711	18052.982845	29.530637
370.194290	18075.251446	29.535655
370.795285	18100.948783	29.540672
370.706478	18130.027657	29.545690
371.175941	18163.229227	29.550708
371.259749	18190.418150	29.555725
371.651638	18221.689143	29.560743
372.078870	18246.881065	29.565760
371.953909	18289.958568	29.570778
372.416783	18320.406251	29.575796
372.854893	18360.022457	29.580813
373.041763	18378.883043	29.585831
373.958948	18430.489722	29.590848
374.166182	18467.879231	29.595866
375.253574	18488.126466	29.600884
375.650475	18509.269626	29.605901
375.946457	18531.033198	29.610919
376.344215	18552.155780	29.615936
376.820232	18585.010333	29.620954
377.303164	18606.117337	29.625972
377.192325	18634.483526	29.630989
377.623673	18667.481184	29.636007
378.483552	18686.160008	29.641024
378.799856	18710.593851	29.646042
378.588159	18741.713331	29.651060
379.175944	18771.226957	29.656077
379.693232	18790.309281	29.661095
380.012919	18811.533364	29.666112
380.247963	18850.449733	29.671130
380.920805	18877.901876	29.676148
381.039894	18911.861135	29.681165
381.350627	18941.557972	29.686183
381.788214	18961.933629	29.691200
382.119314	19005.060602	29.696218
383.248059	19022.631376	29.701236
383.625856	19041.527382	29.706253
383.851553	19061.797873	29.711271
384.398394	19078.821694	29.716288
384.423436	19114.133630	29.721306
384.605293	19145.710619	29.726324
384.968861	19167.372436	29.731341
385.101068	19203.443993	29.736359
385.621115	19231.440579	29.741376
386.098753	19261.564405	29.746394
386.245987	19285.703874	29.751412
386.755566	19323.511965	29.756429
387.282387	19353.041429	29.761447
387.700005	19391.271566	29.766464
387.606633	19426.619490	29.771482
388.080503	19459.275934	29.776500
388.397214	19485.355000	29.781517
388.458817	19526.448617	29.786535
389.356941	19565.652794	29.791552
389.396551	19597.693948	29.796570
389.741081	19637.066987	29.801588
390.489499	19675.928858	29.806605
390.795338	19715.937453	29.811623
391.565132	19741.536941	29.816640
391.616408	19784.262890	29.821658
391.969570	19816.618392	29.826676
392.326238	19853.221781	29.831693
393.125226	19876.021693	29.836711
394.211173	19897.697548	29.841728
394.398715	19937.248566	29.846746
394.724462	19955.709664	29.851764
395.105303	19967.805584	29.856781
395.072469	19985.345422	29.861799
395.826274	19996.648294	29.866816
395.926890	20029.619745	29.871834
396.773644	20049.536619	29.876852
396.692920	20077.504610	29.881869
396.643338	20098.435068	29.886887
397.530335	20118.242908	29.891904
397.510268	20161.686272	29.896922
398.142252	20191.571893	29.901940
398.152268	20216.200426	29.906957
398.543749	20248.831044	29.911975
399.574574	20282.388680	29.916992
399.565177	20318.905379	29.922010
399.812161	20343.283711	29.927028
400.362587	20374.396997	29.932045
400.835975	20417.721677	29.937063
401.311147	20450.061407	29.942080
401.652300	20485.350829	29.947098
402.233242	20519.628034	29.952116
402.724709	20552.457128	29.957133
402.962336	20576.681277	29.962151
403.662495	20606.548498	29.967168
403.748178	20638.574581	29.972186
404.158564	20670.942783	29.977204
404.649658	20698.292384	29.982221
404.476042	20745.911932	29.987239
404.934843	20775.351109	29.992256
405.262843	20809.232430	29.997274
405.909097	20839.849925	30.002292
406.137219	20881.032876	30.007309
406.199537	20929.662344	30.012327
407.410648	20961.312375	30.017344
407.443843	21018.061192	30.022362
407.696907	21043.445356	30.027380
408.602936	21093.463567	30.032397
408.538881	21149.065421	30.037415
409.241388	21186.565249	30.042432
409.299612	21221.962870	30.047450
410.129902	21259.285676	30.052468
410.524180	21284.221213	30.057485
410.724358	21332.064454	30.062503
411.349916	21363.482481	30.067520
411.680959	21408.389291	30.072538
412.055855	21439.434235	30.077556
412.524810	21470.091632	30.082573
412.825643	21520.942616	30.087591
413.583715	21560.642863	30.092608
413.847317	21602.260010	30.097626
414.556791	21629.559295	30.102644
414.934292	21658.579900	30.107661
415.584917	21696.340115	30.112679
415.810970	21726.659730	30.117696
416.114085	21765.139668	30.122714
416.489156	21788.605025	30.127732
417.279773	21823.636984	30.132749
417.195957	21862.013944	30.137767
417.670070	21881.374969	30.142784
418.158225	21926.309239	30.147802
418.742708	21952.128777	30.152820
419.129314	21987.445387	30.157837
419.255334	22028.480902	30.162855
419.597238	22050.585186	30.167872
420.015881	22095.047371	30.172890
420.521168	22124.870665	30.177908
420.567666	22171.669585	30.182925
421.421349	22212.519127	30.187943
421.940246	22243.399876	30.192960
422.569954	22274.653380	30.197978
422.890459	22298.916779	30.202996
423.602989	22321.329128	30.208013
423.922221	22337.961885	30.213031
424.818677	22352.276249	30.218048
425.051445	22380.090657	30.223066
425.512535	22402.010168	30.228084
426.013279	22427.590432	30.233101
426.341443	22455.237847	30.238119
426.698931	22476.700000	30.243136
427.163141	22511.746322	30.248154
427.114725	22536.637025	30.253172
427.520811	22559.999007	30.258189
427.819550	22608.971100	30.263207
428.006198	22623.491242	30.268224
428.487191	22662.117283	30.273242
428.438719	22708.444614	30.278260
429.332048	22742.513946	30.283277
429.375415	22793.425497	30.288295
429.812589	22832.160073	30.293312
429.992571	22885.149474	30.298330
430.640309	22912.081063	30.303348
431.455118	22954.230140	30.308365
431.721023	23010.255065	30.313383
432.313493	23038.072630	30.318400
432.815498	23084.721579	30.323418
433.226179	23132.379070	30.328436
433.444656	23163.063589	30.333453
433.998735	23202.847139	30.338471
434.461705	23252.553947	30.343488
435.077155	23296.882729	30.348506
435.302567	23337.461950	30.353524
435.750458	23375.601576	30.358541
436.268614	23421.381584	30.363559
436.819903	23448.516018	30.368576
436.992842	23504.859096	30.373594
437.355846	23538.081054	30.378612
438.364735	23570.519959	30.383629
438.521346	23614.635247	30.388647
439.481674	23654.687027	30.393664
439.825940	23689.854946	30.398682
440.274902	23731.172372	30.403700
440.641249	23760.297778	30.408717
440.900072	23793.294625	30.413735
441.500040	23833.709096	30.418752
441.706901	23868.307215	30.423770
441.650252	23915.867510	30.428788
442.291714	23966.724788	30.433805
442.494256	24007.867575	30.438823
443.202698	24049.040423	30.443840
443.773260	24100.237786	30.448858
444.316032	24145.735016	30.453876
445.011146	24180.339843	30.458893
445.394632	24232.918257	30.463911
445.493204	24278.287386	30.468928
446.026208	24314.051419	30.473946
446.140202	24360.279163	30.478964
447.029306	24400.267209	30.483981
447.491851	24436.975045	30.488999
447.820101	24471.574841	30.494016
448.338312	24510.321948	30.499034
448.591052	24558.611892	30.504052
449.375799	24593.541778	30.509069
449.597642	24644.342677	30.514087
449.894951	24685.670134	30.519104
450.430054	24724.651468	30.524122
450.557928	24770.573701	30.529140
451.352235	24796.771342	30.534157
451.853539	24844.259413	30.539175
452.323173	24883.953633	30.544192
452.674640	24911.124997	30.549210
453.157676	24963.985679	30.554228
453.551142	24996.374445	30.559245
454.007281	25034.212101	30.564263
454.051326	25084.114895	30.569280
454.544508	25121.929281	30.574298
454.735802	25180.780567	30.579316
455.406245	25222.555452	30.584333
455.561232	25262.466528	30.589351
456.347239	25312.116545	30.594368
456.804907	25364.225741	30.599386
457.284713	25413.395212	30.604404
457.700439	25465.305069	30.609421
458.260665	25518.859607	30.614439
458.616539	25562.324142	30.619456
459.412882	25602.711960	30.624474
459.599297	25652.389472	30.629492
460.269587	25700.485945	30.634509
460.626711	25753.220062	30.639527
461.001634	25793.014046	30.644544
461.430240	25833.713891	30.649562
461.958036	25906.141764	30.654580
462.713645	25939.738805	30.659597
463.232346	25982.603496	30.664615
464.479942	26008.729708	30.669632
465.495323	26040.524134	30.674650
465.685632	26074.113892	30.679668
466.480225	26099.356267	30.684685
466.561248	26136.594420	30.689703
466.929763	26171.135819	30.694720
467.728087	26191.053791	30.699738
467.629572	26229.359463	30.704756
468.117471	26258.667769	30.709773
468.578476	26295.893965	30.714791
469.027086	26338.831053	30.719808
469.521603	26369.595610	30.724826
469.678677	26411.789379	30.729844
470.195489	26449.262166	30.734861
470.396163	26483.734145	30.739879
471.108062	26525.599994	30.744896
471.349366	26584.266489	30.749914
471.674774	26629.946610	30.754932
472.266859	26661.767958	30.759949
472.663462	26718.169867	30.764967
472.914970	26763.610224	30.769984
473.842616	26797.076450	30.775002
474.368100	26856.179510	30.780020
474.934472	26889.995772	30.785037
475.634666	26923.487200	30.790055
475.843400	26963.292429	30.795072
476.646718	27009.503365	30.800090
476.791548	27050.495846	30.805108
477.269649	27082.579672	30.810125
477.437567	27124.934263	30.815143
477.978810	27180.900605	30.820160
478.662880	27219.716357	30.825178
478.699949	27253.109789	30.830196
479.168365	27315.179322	30.835213
479.769849	27359.263916	30.840231
480.706191	27396.193190	30.845248
481.049965	27438.945323	30.850266
481.513919	27479.094403	30.855284
482.089665	27522.338336	30.860301
482.693111	27563.786194	30.865319
483.201841	27600.180926	30.870336
483.531301	27631.791960	30.875354
483.619193	27669.798782	30.880372
483.944593	27711.387551	30.885389
484.687221	27745.047057	30.890407
485.226646	27797.432452	30.895424
486.136727	27827.336101	30.900442
486.290256	27869.508796	30.905460
486.629202	27907.480981	30.910477
487.075802	27949.400432	30.915495
487.320709	27993.085020	30.920512
488.113090	28034.278847	30.925530
488.403405	28073.249887	30.930548
489.003468	28119.860129	30.935565
489.690140	28164.052578	30.940583
490.063686	28195.521727	30.945600
490.713863	28245.918719	30.950618
491.000484	28298.464105	30.955636
491.799667	28329.380572	30.960653
491.892263	28381.948798	30.965671
491.951875	28432.841337	30.970688
492.564376	28477.526308	30.975706
492.933368	28538.544168	30.980724
493.552877	28586.007302	30.985741
494.028249	28630.595452	30.990759
494.291338	28708.283660	30.995776
494.713141	28757.521177	31.000794
495.435252	28822.983120	31.005812
495.677632	28859.039656	31.010829
496.241395	28929.130534	31.015847
496.658963	28983.198911	31.020864
497.139790	29042.812095	31.025882
497.891081	29109.992663	31.030900
498.334327	29163.741910	31.035917
498.714847	29222.299739	31.040935
499.230325	29282.986877	31.045952
499.937561	29337.541630	31.050970
499.903057	29399.998248	31.055988
500.647560	29449.427328	31.061005
501.556264	29517.902089	31.066023
502.154568	29576.504003	31.071040
502.773052	29621.752457	31.076058
503.362023	29683.662309	31.081076
504.088840	29729.621868	31.086093
504.326988	29784.230270	31.091111
504.938560	29843.471286	31.096128
505.651625	29880.307107	31.101146
506.328205	29934.802552	31.106164
507.051861	29972.819822	31.111181
508.105180	30008.132788	31.116199
508.629176	30046.397716	31.121216
509.334732	30074.865802	31.126234
509.489220	30112.437937	31.131252
509.932900	30134.333968	31.136269
510.555276	30178.513784	31.141287
511.045359	30229.592857	31.146304
511.393197	30258.322232	31.151322
511.694308	30307.789135	31.156340
512.143403	30345.723226	31.161357
512.719509	30391.466513	31.166375
513.061728	30445.614979	31.171392
513.551964	30475.109881	31.176410
513.908844	30526.180277	31.181428
514.006149	30563.668185	31.186445
514.555065	30609.167306	31.191463
515.091161	30665.801954	31.196480
515.182386	30711.865936	31.201498
515.684955	30770.516074	31.206516
516.191973	30828.165593	31.211533
517.093214	30871.099112	31.216551
517.176649	30930.882199	31.221568
517.982059	30977.759597	31.226586
517.970147	31036.599717	31.231604
518.544616	31091.235528	31.236621
519.475085	31149.854119	31.241639
519.757125	31196.354781	31.246656
520.445966	31257.559645	31.251674
520.783539	31313.673918	31.256692
521.261874	31364.108335	31.261709
522.040370	31414.487008	31.266727
522.348416	31481.223056	31.271744
523.135766	31526.486420	31.276762
523.394285	31598.430463	31.281780
524.399490	31626.132256	31.286797
525.946394	31647.860584	31.291815
526.207440	31703.228394	31.296832
526.818655	31737.633536	31.301850
527.807341	31760.419637	31.306868
528.250644	31798.591307	31.311885
529.130460	31821.474345	31.316903
529.585902	31862.944291	31.321920
530.069250	31891.474131	31.326938
530.655335	31931.767923	31.331956
530.781725	31957.735002	31.336973
531.344839	31993.293870	31.341991
531.649264	32034.612483	31.347008
532.353561	32073.438908	31.352026
532.810641	32113.397904	31.357044
533.201322	32150.957486	31.362061
533.850205	32192.112302	31.367079
533.919936	32247.803695	31.372096
534.297411	32293.256632	31.377114
534.766815	32345.487439	31.382132
535.169865	32388.551141	31.387149
535.635236	32453.592689	31.392167
536.275155	32507.707816	31.397184
536.346076	32565.425611	31.402202
536.681970	32626.053051	31.407220
536.992707	32681.425197	31.412237
537.783030	32746.215377	31.417255
538.319632	32806.037266	31.422272
539.160821	32860.423131	31.427290
539.716993	32921.217135	31.432308
540.003660	32984.365481	31.437325
540.600001	33042.985635	31.442343
541.135042	33089.878627	31.447360
541.991208	33150.936240	31.452378
542.652028	33214.247632	31.457396
542.932632	33271.283115	31.462413
543.909218	33325.950958	31.467431
544.290523	33398.172354	31.472448
545.000453	33449.918652	31.477466
546.260010	33479.155859	31.482484
546.749237	33536.012594	31.487501
547.162152	33576.935108	31.492519
547.655904	33632.841654	31.497536
548.080289	33670.581915	31.502554
548.877709	33716.732748	31.507572
549.065538	33762.381715	31.512589
549.548119	33806.518026	31.517607
549.948819	33866.438526	31.522624
550.540516	33920.512308	31.527642
551.059770	33973.995540	31.532660
551.300668	34034.924330	31.537677
552.077667	34077.914608	31.542695
552.509453	34138.269494	31.547712
553.098280	34179.801740	31.552730
553.781256	34225.404825	31.557748
554.284999	34264.770916	31.562765
555.040103	34309.380960	31.567783
555.490232	34369.386503	31.572800
555.561773	34426.343481	31.577818
556.340498	34471.694724	31.582836
556.891103	34516.619904	31.587853
557.461407	34578.269246	31.592871
557.487248	34632.545946	31.597888
558.013957	34684.818372	31.602906
558.741289	34750.484595	31.607924
559.237068	34812.787631	31.612941
559.812151	34868.167127	31.617959
560.284726	34931.821832	31.622976
560.583295	34995.821063	31.627994
561.294632	35067.720204	31.633012
561.721198	35139.373199	31.638029
562.238522	35193.927013	31.643047
562.694692	35277.986692	31.648064
563.379399	35340.329791	31.653082
564.160244	35413.629415	31.658100
564.436553	35484.415564	31.663117
565.219421	35541.738276	31.668135
565.741717	35621.632632	31.673152
566.044988	35680.120558	31.678170
567.121748	35751.810625	31.683188
567.509699	35830.484755	31.688205
568.147428	35883.657517	31.693223
568.757459	35964.286821	31.698240
569.861515	36025.591080	31.703258
570.435501	36090.031571	31.708276
571.263682	36153.388902	31.713293
571.654751	36199.603828	31.718311
572.360284	36273.995542	31.723328
572.979472	36319.087504	31.728346
573.704403	36382.440609	31.733364
573.827614	36434.017936	31.738381
574.542104	36487.836227	31.743399
574.956305	36547.662518	31.748416
575.698280	36619.177825	31.753434
576.622552	36673.356508	31.758452
577.051624	36726.768213	31.763469
578.084710	36780.055067	31.768487
578.912145	36829.134521	31.773504
579.470785	36875.727467	31.778522
580.228603	36917.370724	31.783540
580.601116	36968.447647	31.788557
581.590223	37001.156356	31.793575
581.768429	37061.613496	31.798592
582.294804	37101.919419	31.803610
582.701698	37149.721619	31.808628
583.022486	37207.722460	31.813645
583.955645	37241.643271	31.818663
584.713282	37307.519016	31.823680
584.991840	37364.911922	31.828698
585.747359	37410.558500	31.833716
586.312036	37463.514469	31.838733
586.660073	37508.793069	31.843751
587.101232	37571.051601	31.848768
587.932765	37632.018175	31.853786
588.532094	37668.213624	31.858804
588.783261	37737.131804	31.863821
589.692225	37782.561463	31.868839
590.181277	37845.324315	31.873856
590.372500	37892.933714	31.878874
590.794047	37956.531839	31.883892
590.795393	38017.633676	31.888909
591.625609	38081.265738	31.893927
591.906642	38147.529412	31.898944
592.311641	38214.034814	31.903962
593.331243	38266.053219	31.908980
593.778381	38330.607902	31.913997
594.042602	38390.449302	31.919015
594.782606	38468.284618	31.924032
595.662811	38530.224603	31.929050
596.503072	38589.523341	31.934068
597.181777	38665.501156	31.939085
598.038931	38718.838589	31.944103
599.110690	38762.075499	31.949120
599.282995	38814.121800	31.954138
600.097430	38864.405161	31.959156
600.553189	38926.299823	31.964173
601.324825	38980.343373	31.969191
601.756311	39041.213490	31.974208
602.369402	39105.453147	31.979226
602.579881	39157.254247	31.984244
602.909248	39228.964828	31.989261
603.593753	39294.762049	31.994279
603.908951	39369.758106	31.999296
604.263116	39442.027259	32.004314
605.027270	39516.211183	32.009332
605.607406	39596.583898	32.014349
606.322473	39674.163369	32.019367
607.528259	39726.111030	32.024384
608.888768	39781.183385	32.029402
609.826662	39828.106387	32.034420
610.418453	39872.981335	32.039437
611.165021	39932.378848	32.044455
612.011155	39965.678397	32.049472
612.692860	40016.157319	32.054490
613.378952	40054.410687	32.059508
613.819286	40112.457897	32.064525
614.114479	40163.398778	32.069543
614.451078	40215.257814	32.074560
615.030907	40266.638072	32.079578
615.638093	40323.793517	32.084596
615.948503	40398.109634	32.089613
616.169745	40453.097568	32.094631
616.702385	40520.306857	32.099648
616.823277	40600.349495	32.104666
617.317530	40669.409099	32.109684
617.941157	40743.946355	32.114701
618.412625	40832.218123	32.119719
619.025110	40897.161803	32.124736
619.432205	40986.133084	32.129754
620.424414	41057.589857	32.134772
621.184511	41137.885971	32.139789
621.835761	41227.392609	32.144807
622.187652	41305.250485	32.149824
622.341316	41383.510763	32.154842
623.463998	41464.559692	32.159860
624.399191	41546.501728	32.164877
625.246643	41618.918985	32.169895
626.301820	41679.587560	32.174912
626.882095	41758.760723	32.179930
627.914627	41818.338104	32.184948
628.414418	41879.541013	32.189965
629.214649	41948.390745	32.194983
629.679127	42006.465221	32.200000
629.836145	42085.242488	32.205018
630.764993	42145.586217	32.210036
631.009729	42204.581519	32.215053
631.782815	42291.285735	32.220071
632.129342	42358.002141	32.225088
632.479749	42436.553243	32.230106
633.744774	42500.210992	32.235124
634.168409	42571.685481	32.240141
634.541548	42630.319993	32.245159
634.975982	42688.467874	32.250176
635.431834	42771.605763	32.255194
636.472343	42834.660892	32.260212
637.135928	42913.241221	32.265229
637.604672	42969.837416	32.270247
638.175875	43044.793588	32.275264
638.562346	43108.614321	32.280282
639.645223	43175.480410	32.285300
640.168924	43262.905971	32.290317
640.992376	43334.642549	32.295335
641.765894	43399.230658	32.300352
642.227956	43467.567328	32.305370
643.102674	43543.182569	32.310388
644.187974	43603.394730	32.315405
644.544023	43668.175849	32.320423
645.122627	43726.375794	32.325440
645.624621	43810.498894	32.330458
646.636924	43879.055603	32.335476
647.129925	43952.399290	32.340493
647.680151	44015.953002	32.345511
648.588227	44090.220024	32.350528
648.892799	44162.803216	32.355546
649.657065	44231.736851	32.360564
650.151384	44306.129897	32.365581
650.620158	44378.061688	32.370599
651.614478	44456.363457	32.375616
652.446091	44536.893014	32.380634
653.182644	44597.257558	32.385652
653.753906	44677.802307	32.390669
654.490551	44746.654007	32.395687
655.311777	44801.615785	32.400704
655.769805	44873.895407	32.405722
656.443552	44935.774286	32.410740
657.318568	45012.339485	32.415757
657.628784	45083.261428	32.420775
658.349897	45164.664422	32.425792
658.542605	45242.723004	32.430810
659.427504	45312.152202	32.435828
659.933455	45405.037197	32.440845
660.715996	45478.601132	32.445863
661.428409	45555.176465	32.450880
661.806305	45661.607019	32.455898
662.667056	45722.172550	32.460916
663.389649	45797.061126	32.465933
663.804407	45882.278345	32.470951
665.017454	45956.619257	32.475968
665.131747	46042.590941	32.480986
666.083903	46113.107648	32.486004
666.718377	46185.088490	32.491021
667.152047	46266.881598	32.496039
667.882849	46346.920924	32.501056
668.248404	46444.627385	32.506074
669.585175	46525.303103	32.511092
669.816976	46604.800741	32.516109
670.632217	46693.214113	32.521127
671.463800	46773.791190	32.526144
671.408116	46854.145703	32.531162
672.892408	46929.831867	32.536180
673.536267	47007.586451	32.541197
673.888227	47090.486018	32.546215
675.430950	47141.034780	32.551232
676.493996	47218.234726	32.556250
677.299399	47272.451681	32.561268
678.101004	47336.739310	32.566285
678.885662	47383.779412	32.571303
680.124238	47434.780223	32.576320
680.420765	47485.024170	32.581338
681.270310	47527.453116	32.586356
681.806529	47570.445456	32.591373
682.202058	47623.591169	32.596391
682.813706	47669.931118	32.601408
683.580333	47727.247225	32.606426
683.931285	47778.992375	32.611444
684.375785	47835.676772	32.616461
684.791677	47897.721675	32.621479
685.489041	47956.253032	32.626496
685.835571	48030.186311	32.631514
686.410004	48100.693896	32.636532
686.830737	48167.384041	32.641549
687.496972	48255.377767	32.646567
688.112445	48332.823549	32.651584
688.539880	48427.833232	32.656602
689.113469	48508.412946	32.661620
689.587609	48592.994703	32.666637
690.298567	48692.414689	32.671655
690.977494	48777.004497	32.676672
691.483872	48877.712939	32.681690
692.722953	48956.671990	32.686708
693.606123	49040.196584	32.691725
694.491554	49122.536924	32.696743
695.400425	49197.780867	32.701760
695.766649	49293.629220	32.706778
696.231496	49374.606365	32.711796
696.912030	49469.254168	32.716813
697.696950	49561.693504	32.721831
698.382603	49648.275652	32.726848
698.904316	49749.892536	32.731866
699.848519	49837.089725	32.736884
700.657187	49918.631386	32.741901
701.247667	50000.986330	32.746919
701.992438	50086.133219	32.751936
702.830545	50176.403411	32.756954
703.456445	50263.048741	32.761972
704.106318	50357.753379	32.766989
704.825484	50460.007803	32.772007
705.794556	50537.675750	32.777024
706.099311	50646.088666	32.782042
706.783490	50727.941732	32.787060
707.653071	50820.846906	32.792077
708.433735	50910.403638	32.797095
709.082505	51010.164938	32.802112
709.663830	51107.720753	32.807130
710.293758	51189.745819	32.812148
711.739497	51278.916501	32.817165
711.651832	51372.288783	32.822183
712.666511	51460.100753	32.827200
713.753891	51534.348461	32.832218
715.130089	51631.715654	32.837236
715.685377	51714.162716	32.842253
716.197771	51802.378195	32.847271
717.097945	51870.884501	32.852288
717.531790	51953.125230	32.857306
718.339397	52037.537625	32.862324
719.512601	52115.907842	32.867341
719.692094	52210.620315	32.872359
720.441102	52286.774523	32.877376
720.598579	52378.446645	32.882394
721.492971	52462.619150	32.887412
722.271409	52552.945086	32.892429
723.224128	52645.662128	32.897447
723.566758	52733.628776	32.902464
724.343079	52834.044897	32.907482
724.665674	52917.410445	32.912500
725.493865	53001.027671	32.917517
725.732147	53092.089680	32.922535
726.486352	53178.935390	32.927552
727.257049	53272.569911	32.932570
727.868829	53369.434037	32.937588
728.506474	53456.489757	32.942605
729.409839	53551.405098	32.947623
730.342653	53649.765376	32.952640
731.344694	53736.800078	32.957658
731.748320	53829.291254	32.962676
732.855619	53928.647565	32.967693
733.318507	54029.380637	32.972711
734.252764	54110.104292	32.977728
734.993145	54192.736639	32.982746
735.585556	54297.764657	32.987764
736.173125	54388.737134	32.992781
736.918854	54472.860761	32.997799
737.630268	54572.260454	33.002816
738.713909	54657.712665	33.007834
739.551301	54763.909429	33.012852
741.151685	54827.550047	33.017869
741.874434	54922.419750	33.022887
742.867817	54996.503530	33.027904
743.493708	55079.114303	33.032922
744.128417	55171.839019	33.037940
745.196437	55245.582882	33.042957
745.624032	55333.591442	33.047975
746.824878	55404.249732	33.052992
747.540263	55494.031079	33.058010
747.880744	55575.768637	33.063028
749.185340	55634.235667	33.068045
749.514042	55711.951101	33.073063
750.560225	55785.466828	33.078080
751.264972	55869.040897	33.083098
751.846815	55939.405288	33.088116
752.658928	56033.400004	33.093133
753.317425	56121.917327	33.098151
753.716078	56207.988550	33.103168
754.697845	56290.368730	33.108186
754.959828	56373.386222	33.113204
755.776691	56453.342797	33.118221
756.100443	56557.264679	33.123239
756.764137	56663.639389	33.128256
757.860651	56755.183252	33.133274
758.312776	56845.526024	33.138292
759.474731	56944.439961	33.143309
759.792381	57047.082761	33.148327
760.426772	57138.799491	33.153344
761.628449	57249.252458	33.158362
761.825625	57357.988959	33.163380
762.714937	57458.214217	33.168397
763.022611	57571.672659	33.173415
764.001595	57672.414963	33.178432
764.555837	57781.322290	33.183450
765.254528	57894.136671	33.188468
766.102257	58000.071113	33.193485
766.533187	58115.540656	33.198503
767.532447	58231.428850	33.203520
768.809345	58327.645150	33.208538
769.914656	58434.739972	33.213556
770.763908	58530.263271	33.218573
771.994566	58625.995765	33.223591
772.812742	58717.360831	33.228608
774.294254	58813.431945	33.233626
774.453572	58902.587541	33.238644
775.577218	58980.525736	33.243661
776.370014	59067.416301	33.248679
777.180607	59137.248716	33.253696
778.077108	59216.021560	33.258714
778.498041	59297.508383	33.263732
779.436375	59382.379392	33.268749
779.510573	59462.053628	33.273767
780.160985	59542.403989	33.278784
781.120655	59619.878843	33.283802
781.638819	59707.853913	33.288820
782.902967	59794.979449	33.293837
783.530517	59881.243609	33.298855
783.910290	59963.472989	33.303872
784.616922	60060.082491	33.308890
785.374058	60157.316072	33.313908
785.970597	60255.448743	33.318925
786.613384	60366.719037	33.323943
787.524409	60462.860667	33.328960
788.444872	60565.472540	33.333978
788.689016	60681.531194	33.338996
789.791448	60783.627510	33.344013
790.236563	60892.411768	33.349031
790.335240	61014.228387	33.354048
791.883585	61119.178838	33.359066
792.326907	61237.558774	33.364084
793.059644	61344.989755	33.369101
793.760417	61466.039755	33.374119
794.624591	61589.951732	33.379136
795.581715	61705.443480	33.384154
796.454094	61819.496265	33.389172
797.339423	61945.720063	33.394189
798.094657	62068.136124	33.399207
798.569035	62183.735588	33.404224
799.735205	62298.621053	33.409242
800.159223	62429.676830	33.414260
801.222280	62555.944589	33.419277
802.171918	62669.268868	33.424295
803.132258	62782.838504	33.429312
804.125956	62904.335362	33.434330
804.808585	63009.192046	33.439348
806.415563	63118.971964	33.444365
807.609585	63227.208937	33.449383
808.665375	63328.946523	33.454400
809.878531	63423.073957	33.459418
810.818573	63516.678072	33.464436
811.808363	63592.899033	33.469453
812.578882	63686.841628	33.474471
813.126896	63772.730942	33.479488
814.276091	63863.027998	33.484506
814.747164	63959.119758	33.489524
815.476761	64045.283623	33.494541
816.123551	64139.349854	33.499559
816.623647	64239.078900	33.504576
817.117363	64325.314493	33.509594
817.776262	64439.063188	33.514612
818.530580	64538.751708	33.519629
819.616394	64652.620715	33.524647
820.082086	64772.389082	33.529664
820.834117	64875.878515	33.534682
821.629970	64998.280102	33.539700
822.555357	65094.074582	33.544717
823.538806	65208.614633	33.549735
824.156087	65320.289095	33.554752
825.444986	65420.133804	33.559770
825.829087	65537.511713	33.564788
826.514205	65647.539547	33.569805
827.212396	65756.775647	33.574823
827.845482	65881.112039	33.579840
828.610800	65984.819752	33.584858
829.026154	66123.871714	33.589876
830.122431	66231.432626	33.594893
830.811800	66338.245819	33.599911
831.519394	66472.087230	33.604928
832.773261	66561.044973	33.609946
833.560864	66683.906704	33.614964
834.634204	66787.289411	33.619981
835.640084	66903.750560	33.624999
836.376891	67014.295468	33.630016
837.243770	67111.329003	33.635034
838.240664	67211.717318	33.640052
838.691621	67329.144869	33.645069
839.720848	67443.025898	33.650087
840.119316	67555.475499	33.655104
840.781251	67670.537378	33.660122
841.527115	67802.705711	33.665140
842.413479	67925.223375	33.670157
843.019329	68043.798914	33.675175
843.493718	68188.215901	33.680192
844.604671	68306.614690	33.685210
845.089777	68447.105697	33.690228
846.330627	68573.052079	33.695245
847.606669	68691.387844	33.700263
848.362372	68829.314179	33.705280
849.518341	68941.873722	33.710298
850.379955	69078.797933	33.715316
851.121963	69188.126916	33.720333
852.307149	69320.358692	33.725351
852.861354	69448.067496	33.730368
853.977805	69572.301736	33.735386
854.905156	69708.567966	33.740404
855.653091	69822.053109	33.745421
856.678870	69953.322533	33.750439
857.346223	70070.679063	33.755456
858.408274	70188.072232	33.760474
859.309549	70332.572494	33.765492
860.126160	70458.840433	33.770509
861.364255	70568.859676	33.775527
862.247934	70689.395849	33.780544
862.706781	70798.027486	33.785562
863.802141	70928.286125	33.790580
864.489114	71057.032276	33.795597
866.049894	71179.444801	33.800615
866.562528	71308.385652	33.805632
867.306166	71420.324594	33.810650
868.250582	71545.085646	33.815668
869.375585	71651.904423	33.820685
870.656551	71763.876580	33.825703
871.252435	71884.315270	33.830720
872.502178	71995.041818	33.835738
872.908321	72108.475440	33.840756
873.935486	72222.806188	33.845773
874.469409	72340.469137	33.850791
875.475384	72463.752061	33.855808
876.352304	72577.881871	33.860826
877.225394	72706.291044	33.865844
878.360784	72820.486962	33.870861
879.358953	72941.415292	33.875879
879.834511	73067.799210	33.880896
880.888544	73176.331983	33.885914
881.567496	73291.788259	33.890932
883.200501	73388.774606	33.895949
884.359326	73488.944564	33.900967
885.333218	73595.899140	33.905984
886.540106	73694.386359	33.911002
887.345382	73796.829397	33.916020
888.031035	73908.569544	33.921037
888.897853	74018.301025	33.926055
889.214851	74116.494439	33.931072
890.904662	74212.874353	33.936090
891.986468	74292.388281	33.941108
893.072263	74372.901010	33.946125
894.090403	74453.810965	33.951143
894.740930	74540.669459	33.956160
895.739723	74607.278550	33.961178
896.436206	74690.044810	33.966196
897.318143	74778.699988	33.971213
898.350461	74863.580576	33.976231
899.002141	74962.784985	33.981248
899.464168	75042.170007	33.986266
899.954127	75146.840626	33.991284
900.305143	75258.099101	33.996301
901.179985	75362.334083	34.001319
901.511562	75492.822317	34.006336
902.143757	75608.785599	34.011354
902.716286	75752.345664	34.016372
903.006470	75875.234954	34.021389
904.050679	76018.238237	34.026407
904.543962	76161.529474	34.031424
905.756988	76302.255265	34.036442
906.650427	76447.569351	34.041460
907.575656	76592.196105	34.046477
908.964279	76733.022156	34.051495
909.625718	76884.164372	34.056512
910.190464	77029.176073	34.061530
911.005724	77187.176144	34.066548
912.078938	77338.746812	34.071565
912.666212	77487.362881	34.076583
913.536993	77659.562532	34.081600
914.434864	77806.548267	34.086618
915.623561	77962.683324	34.091636
916.889813	78117.687167	34.096653
918.034697	78264.470709	34.101671
918.541725	78420.424270	34.106688
919.953036	78566.033641	34.111706
920.644605	78731.547687	34.116724
921.627225	78882.865575	34.121741
923.387609	79019.761175	34.126759
924.694110	79158.800904	34.131776
925.597935	79286.800845	34.136794
926.785751	79422.667565	34.141812
927.615591	79554.248718	34.146829
928.880102	79691.426405	34.151847
929.891493	79822.574340	34.156864
931.526750	79925.244136	34.161882
932.531138	80053.921341	34.166900
933.356122	80178.201053	34.171917
934.346820	80293.269416	34.176935
935.280474	80423.643014	34.181952
936.482292	80529.619516	34.186970
937.313391	80642.748760	34.191988
937.988996	80752.810997	34.197005
938.856829	80877.119132	34.202023
939.496660	80999.991703	34.207040
940.730915	81110.267087	34.212058
941.414758	81249.277106	34.217076
942.195271	81361.241714	34.222093
943.105199	81483.515651	34.227111
944.083983	81622.650071	34.232128
944.591255	81752.646295	34.237146
945.571553	81883.906274	34.242164
946.526827	82029.752620	34.247181
947.321201	82151.131972	34.252199
947.915880	82295.154398	34.257216
949.252584	82425.688104	34.262234
949.845526	82564.999560	34.267252
950.454674	82701.822994	34.272269
951.703282	82833.815966	34.277287
952.830166	82980.146182	34.282304
953.472431	83105.022547	34.287322
954.671008	83223.645876	34.292340
955.345651	83347.600902	34.297357
956.522092	83476.762641	34.302375
957.458017	83626.614393	34.307392
958.201798	83753.755072	34.312410
959.248156	83880.833847	34.317428
959.873032	84021.230758	34.322445
960.701593	84159.994266	34.327463
961.584677	84310.327384	34.332480
962.205682	84463.798510	34.337498
963.474268	84612.039086	34.342516
964.117250	84763.724446	34.347533
965.150932	84906.077510	34.352551
966.222468	85071.031072	34.357568
967.014158	85216.950072	34.362586
968.312728	85361.875228	34.367604
969.256635	85521.335988	34.372621
970.292788	85663.997015	34.377639
971.336173	85825.613618	34.382656
972.021921	85990.586821	34.387674
973.155920	86131.810976	34.392692
974.402911	86301.881996	34.397709
976.155074	86438.096050	34.402727
976.876523	86596.183632	34.407744
977.869207	86739.389941	34.412762
979.367458	86875.173931	34.417780
979.722750	87031.926577	34.422797
980.852052	87168.045265	34.427815
981.603529	87320.969619	34.432832
982.588725	87475.571143	34.437850
983.590666	87618.243480	34.442868
984.382692	87779.472217	34.447885
985.345847	87939.034951	34.452903
986.135259	88098.481919	34.457920
986.900949	88258.060440	34.462938
987.891606	88419.634117	34.467956
988.473490	88590.027762	34.472973
989.674072	88762.332752	34.477991
990.617297	88925.442746	34.483008
991.526930	89090.843804	34.488026
992.441849	89272.071469	34.493044
993.498467	89441.709460	34.498061
994.917174	89602.144798	34.503079
996.052813	89785.453536	34.508096
996.840995	89944.938496	34.513114
998.354142	90100.185165	34.518132
999.089714	90273.033563	34.523149
1000.036942	90436.090017	34.528167
1001.422005	90609.055118	34.533184
1002.087275	90779.058379	34.538202
1003.221029	90940.201625	34.543220
1004.266005	91106.809442	34.548237
1005.830760	91259.783226	34.553255
1006.453137	91427.956584	34.558272
1007.285009	91582.268512	34.563290
1008.836905	91745.658096	34.568308
1009.558804	91916.919495	34.573325
1010.806626	92076.292178	34.578343
1011.538970	92234.940936	34.583360
1012.227472	92409.964329	34.588378
1013.261571	92570.122370	34.593396
1014.092646	92740.896941	34.598413
1015.110086	92908.882524	34.603431
1016.160723	93087.357288	34.608448
1016.952095	93265.534403	34.613466
1017.964837	93425.315566	34.618484
1018.849726	93579.694820	34.623501
1020.125130	93753.219643	34.628519
1020.794198	93897.775687	34.633536
1022.004404	94072.383192	34.638554
1023.064401	94229.876984	34.643572
1023.963228	94395.816435	34.648589
1026.116584	94533.333488	34.653607
1027.135945	94685.102509	34.658624
1028.513896	94841.402135	34.663642
1029.738170	94977.676268	34.668660
1030.665190	95122.234962	34.673677
1031.796731	95271.235755	34.678695
1032.897277	95420.824895	34.683712
1033.901645	95561.790851	34.688730
1034.902158	95694.371421	34.693748
1035.498223	95851.749699	34.698765
1036.895244	96004.546928	34.703783
1037.655197	96145.727488	34.708800
1038.554710	96296.209667	34.713818
1039.420952	96446.881823	34.718836
1040.332409	96617.195502	34.723853
1041.421426	96764.034862	34.728871
1042.597293	96944.542689	34.733888
1044.131910	97092.601757	34.738906
1045.180967	97249.958470	34.743924
1046.011844	97409.643705	34.748941
1047.023576	97557.507017	34.753959
1048.069745	97713.512490	34.758976
1048.877595	97879.958872	34.763994
1050.313037	98030.084572	34.769012
1051.254229	98194.485352	34.774029
1052.067100	98360.389704	34.779047
1052.671112	98527.918569	34.784064
1053.760119	98710.270371	34.789082
1054.988534	98873.064573	34.794100
1055.677995	99065.366823	34.799117
1056.813068	99237.788568	34.804135
1057.804798	99407.753554	34.809152
1058.789047	99587.944960	34.814170
1060.118354	99750.563597	34.819188
1061.240562	99938.850715	34.824205
1062.206356	100104.804652	34.829223
1063.874211	100281.520173	34.834240
1064.890406	100455.609565	34.839258
1066.284590	100625.446674	34.844276
1066.903575	100792.146114	34.849293
1068.021288	100951.167096	34.854311
1069.597520	101140.888654	34.859328
1070.417435	101318.682056	34.864346
1071.531972	101460.796371	34.869364
1072.109463	101644.323763	34.874381
1073.248739	101824.334535	34.879399
1074.294669	101992.832735	34.884416
1074.903119	102164.671225	34.889434
1076.573319	102342.850557	34.894452
1077.478079	102527.837125	34.899469
1078.789501	102708.370197	34.904487
1079.941605	102876.065245	34.909504
1080.905069	103054.701763	34.914522
1081.642902	103237.599931	34.919540
1082.428651	103412.387007	34.924557
1083.655722	103594.548452	34.929575
1084.887771	103776.222818	34.934592
1085.393268	103970.675587	34.939610
1086.862229	104140.321049	34.944628
1088.001372	104331.752962	34.949645
1089.353831	104507.220031	34.954663
1090.738690	104689.141509	34.959680
1091.289945	104871.265193	34.964698
1092.341321	105028.353097	34.969716
1093.388382	105200.310329	34.974733
1094.626745	105370.945366	34.979751
1096.053746	105537.257185	34.984768
1096.814080	105710.670845	34.989786
1097.852492	105880.101104	34.994804
1098.654100	106071.645832	34.999821
1099.391578	106243.547042	35.004839
1100.680686	106428.428291	35.009856
1101.353252	106619.643701	35.014874
1102.515444	106817.618713	35.019892
1103.378376	107008.146938	35.024909
1104.799550	107199.901550	35.029927
1106.199379	107388.811413	35.034944
1106.847641	107586.167771	35.039962
1108.144020	107781.898762	35.044980
1109.023314	107985.299321	35.049997
1109.790370	108188.808622	35.055015
1110.760415	108397.795525	35.060032
1111.954647	108606.557071	35.065050
1113.094763	108818.267660	35.070068
1114.082611	109028.003841	35.075085
1115.280203	109242.279485	35.080103
1116.491839	109449.056161	35.085120
1117.533758	109661.245601	35.090138
1119.317892	109859.431878	35.095156
1120.863289	110064.068243	35.100173
1122.620102	110244.490861	35.105191
1123.798757	110448.354693	35.110208
1125.058940	110643.783241	35.115226
1126.559290	110819.932692	35.120244
1127.714423	111018.991326	35.125261
1128.686984	111204.350559	35.130279
1130.025800	111384.419102	35.135296
1130.703288	111590.971002	35.140314
1132.129402	111762.844661	35.145332
1133.164458	111966.401581	35.150349
1134.227247	112156.122623	35.155367
1135.506993	112349.900769	35.160384
1136.359630	112545.777607	35.165402
1137.173794	112737.051158	35.170420
1138.709138	112927.915634	35.175437
1139.504462	113138.310757	35.180455
1141.049085	113322.196445	35.185472
1141.421230	113523.758799	35.190490
1142.469161	113724.881697	35.195508
1143.742833	113926.374177	35.200525
1144.714919	114140.155506	35.205543
1146.468467	114334.920874	35.210560
1147.614360	114530.940752	35.215578
1148.959512	114725.206191	35.220596
1150.226416	114937.361415	35.225613
1151.142969	115146.028828	35.230631
1152.532166	115340.684019	35.235648
1152.721778	115556.657746	35.240666
1153.957077	115757.042274	35.245684
1155.326005	115962.119099	35.250701
1156.529723	116185.253033	35.255719
1157.949877	116379.188178	35.260736
1158.359191	116595.754421	35.265754
1159.812211	116802.673229	35.270772
1161.209529	117028.695875	35.275789
1161.720256	117233.302804	35.280807
1163.536086	117440.470463	35.285824
1164.499245	117654.862866	35.290842
1165.528672	117862.353466	35.295860
1166.773435	118064.577285	35.300877
1167.812724	118272.360656	35.305895
1169.077704	118463.193471	35.310912
1170.046143	118675.248679	35.315930
1170.952237	118878.193021	35.320948
1172.098041	119086.978363	35.325965
1172.939995	119298.590249	35.330983
1174.386431	119508.025910	35.336000
1175.240289	119733.323418	35.341018
1176.409992	119936.852588	35.346036
1178.034550	120164.167625	35.351053
1178.922156	120380.316135	35.356071
1180.351255	120585.530322	35.361088
1181.514892	120798.633311	35.366106
1184.303814	120980.956898	35.371124
1186.544264	121153.615149	35.376141
1187.830088	121331.209169	35.381159
1189.509380	121500.920945	35.386176
1190.690377	121682.868096	35.391194
1191.788441	121852.462438	35.396212
1192.735634	122027.455519	35.401229
1193.245607	122214.344703	35.406247
1194.572680	122396.779051	35.411264
1195.549768	122580.146676	35.416282
1196.348460	122783.389473	35.421300
1197.429881	122982.430507	35.426317
1198.368814	123180.406583	35.431335
1199.469707	123369.663980	35.436352
1200.398056	123585.778729	35.441370
1201.439971	123807.895786	35.446388
1202.425670	124005.033258	35.451405
1202.936152	124242.131674	35.456423
1204.378911	124468.001996	35.461440
1205.774480	124692.373735	35.466458
1206.857225	124906.495596	35.471476
1208.099215	125133.164467	35.476493
1208.859359	125378.113375	35.481511
1210.137831	125607.504553	35.486528
1211.431064	125852.660816	35.491546
1212.338935	126096.564631	35.496564
1213.757645	126318.663448	35.501581
1215.065222	126561.034887	35.506599
1216.410321	126800.702539	35.511616
1217.266690	127045.661746	35.516634
1218.833576	127280.024203	35.521652
1220.448082	127521.211968	35.526669
1221.718319	127758.275961	35.531687
1223.208282	127991.389149	35.536704
1224.096775	128228.101536	35.541722
1225.615252	128452.962463	35.546740
1227.027787	128692.785912	35.551757
1228.033297	128922.323156	35.556775
1229.720950	129155.501258	35.561792
1231.110325	129380.187459	35.566810
1232.309070	129598.391801	35.571828
1233.719240	129817.234560	35.576845
1234.892766	130050.618332	35.581863
1235.960972	130264.691436	35.586880
1237.456993	130490.293352	35.591898
1238.725229	130713.805019	35.596916
1240.219263	130928.205320	35.601933
1241.102293	131160.872124	35.606951
1241.984486	131382.322767	35.611968
1243.152339	131616.720531	35.616986
1244.527050	131839.157860	35.622004
1245.849240	132051.654766	35.627021
1247.035900	132289.641727	35.632039
1248.531699	132520.721634	35.637056
1250.032408	132727.565381	35.642074
1250.970735	132950.069860	35.647092
1252.618837	133151.314438	35.652109
1253.793784	133353.475035	35.657127
1254.852598	133548.519156	35.662144
1256.312317	133777.040778	35.667162
1257.283499	133973.217497	35.672180
1258.552223	134173.833903	35.677197
1259.763296	134397.900706	35.682215
1260.886185	134607.100809	35.687232
1261.802395	134817.895664	35.692250
1262.465676	135045.087197	35.697268
1264.503294	135263.965385	35.702285
1265.640552	135490.219750	35.707303
1266.872355	135702.514901	35.712320
1268.116245	135935.600580	35.717338
1268.979947	136170.918547	35.722356
1270.525233	136405.060781	35.727373
1271.478675	136638.199406	35.732391
1272.708769	136875.110070	35.737408
1274.360796	137108.910083	35.742426
1275.214734	137355.077823	35.747444
1276.755867	137585.362336	35.752461
1277.635000	137844.004873	35.757479
1278.766245	138098.918412	35.762496
1280.241081	138341.276241	35.767514
1281.455375	138588.306507	35.772532
1282.988160	138841.916964	35.777549
1284.348813	139089.281781	35.782567
1285.898794	139337.872381	35.787584
1287.346007	139582.703467	35.792602
1288.468150	139821.567457	35.797620
1289.890057	140066.888043	35.802637
1291.034114	140320.168091	35.807655
1292.292310	140568.435554	35.812672
1293.550974	140812.647354	35.817690
1294.734649	141068.753956	35.822708
1296.476716	141323.375567	35.827725
1297.703073	141585.831475	35.832743
1298.787393	141828.456330	35.837760
1300.219315	142074.943605	35.842778
1301.400415	142344.652988	35.847796
1302.996782	142583.813119	35.852813
1304.083964	142840.912571	35.857831
1305.090034	143104.912686	35.862848
1306.542857	143358.126202	35.867866
1307.693290	143626.633335	35.872884
1308.759371	143882.273058	35.877901
1310.003559	144153.292196	35.882919
1311.284814	144425.854363	35.887936
1313.175600	144674.503499	35.892954
1314.677212	144941.415709	35.897972
1316.581879	145193.616879	35.902989
1318.175088	145441.825996	35.908007
1319.451977	145695.795587	35.913024
1320.558781	145938.749697	35.918042
1321.759278	146199.367797	35.923060
1322.833730	146458.195161	35.928077
1324.385628	146707.244235	35.933095
1325.700134	146965.363534	35.938112
1327.293238	147219.494700	35.943130
1328.031048	147480.274589	35.948148
1329.635651	147730.323929	35.953165
1330.868751	147996.314153	35.958183
1331.877064	148248.887755	35.963200
1333.495251	148504.545682	35.968218
1334.225349	148781.391835	35.973236
1335.648944	149032.710213	35.978253
1337.002371	149289.076826	35.983271
1338.748255	149533.890103	35.988288
1340.599021	149768.072372	35.993306
1341.484911	150019.689189	35.998324
1342.855643	150248.157756	36.003341
1343.847605	150487.977979	36.008359
1345.155623	150754.445160	36.013376
1346.057216	151002.831928	36.018394
1347.498795	151255.291293	36.023412
1348.694863	151503.264991	36.028429
1350.603180	151760.876222	36.033447
1351.680550	152024.765117	36.038464
1352.758000	152287.184574	36.043482
1353.877917	152567.901208	36.048500
1355.424728	152820.125443	36.053517
1356.414586	153095.971585	36.058535
1357.724414	153369.014537	36.063552
1358.761683	153661.612289	36.068570
1359.863694	153929.302896	36.073588
1361.139349	154233.255924	36.078605
1362.578228	154527.633220	36.083623
1363.940251	154819.222226	36.088640
1365.463224	155108.135838	36.093658
1366.933332	155401.030580	36.098676
1368.657383	155685.970448	36.103693
1370.009276	155980.817135	36.108711
1371.289136	156261.229988	36.113728
1373.322979	156543.194820	36.118746
1374.461877	156846.150762	36.123764
1376.236975	157131.714317	36.128781
1377.507919	157423.642293	36.133799
1378.795986	157699.421296	36.138816
1380.149907	158000.003844	36.143834
1381.256807	158297.584933	36.148852
1382.620099	158588.174266	36.153869
1383.646496	158891.291265	36.158887
1385.464886	159174.363294	36.163904
1387.917291	159450.659960	36.168922
1389.304698	159736.394973	36.173940
1390.967772	160024.116267	36.178957
1392.370715	160311.768360	36.183975
1393.602798	160587.690630	36.188992
1395.426896	160864.709571	36.194010
1396.543883	161155.535623	36.199028
1397.340136	161427.539297	36.204045
1399.064051	161716.696046	36.209063
1400.812861	161996.703692	36.214080
1402.769140	162258.854237	36.219098
1404.626202	162543.503722	36.224116
1406.052677	162812.545296	36.229133
1407.355729	163080.695518	36.234151
1408.565352	163341.707418	36.239168
1409.861008	163608.593543	36.244186
1411.228677	163891.696343	36.249204
1412.558043	164161.980569	36.254221
1413.736699	164440.880709	36.259239
1414.913801	164717.981327	36.264256
1416.325312	164989.411824	36.269274
1417.803632	165273.406398	36.274292
1419.060387	165543.241946	36.279309
1421.025825	165834.544061	36.284327
1422.179644	166114.385429	36.289344
1423.477787	166386.998068	36.294362
1424.600255	166674.524411	36.299380
1426.370365	166949.194277	36.304397
1427.487517	167236.712525	36.309415
1428.929562	167533.593712	36.314432
1430.243085	167816.756678	36.319450
1431.325587	168101.659838	36.324468
1432.612614	168387.558852	36.329485
1434.210101	168646.978228	36.334503
1435.586743	168927.435240	36.339520
1437.237054	169202.608421	36.344538
1438.240879	169481.074872	36.349556
1439.540721	169761.207200	36.354573
1440.513155	170045.405012	36.359591
1441.765360	170345.305527	36.364608
1443.278421	170640.102028	36.369626
1444.696643	170944.623330	36.374644
1446.337602	171244.313364	36.379661
1447.634222	171536.981528	36.384679
1448.566159	171859.455802	36.389696
1450.229481	172164.706145	36.394714
1451.375870	172477.276897	36.399732
1452.854638	172793.639888	36.404749
1454.506171	173103.999632	36.409767
1455.702091	173438.775812	36.414784
1457.261203	173751.363146	36.419802
1459.003265	174079.416921	36.424820
1460.385591	174394.385359	36.429837
1461.829267	174713.140144	36.434855
1463.326566	175036.964342	36.439872
1465.001072	175357.297017	36.444890
1466.337841	175690.619171	36.449908
1468.088336	176024.192625	36.454925
1469.610939	176351.968290	36.459943
1470.861144	176668.623274	36.464960
1472.587103	177006.255886	36.469978
1473.989879	177349.401258	36.474996
1475.664905	177673.391456	36.480013
1477.558008	177991.344918	36.485031
1478.996460	178316.926697	36.490048
1480.224661	178648.205604	36.495066
1482.588853	178945.641848	36.500084
1484.521742	179265.614821	36.505101
1486.023750	179576.421537	36.510119
1487.506893	179898.833373	36.515136
1489.312973	180213.401303	36.520154
1491.595977	180495.300149	36.525172
1493.261192	180795.248689	36.530189
1495.175989	181072.261689	36.535207
1496.704902	181372.236099	36.540224
1498.353979	181637.606727	36.545242
1499.932968	181937.246167	36.550260
1500.793615	182223.679129	36.555277
1502.399677	182495.496157	36.560295
1504.064172	182795.684883	36.565312
1505.454150	183068.784389	36.570330
1506.658422	183377.721254	36.575348
1507.592057	183659.847277	36.580365
1509.537357	183961.849402	36.585383
1511.115967	184253.429640	36.590400
1512.197840	184542.605668	36.595418
1513.717793	184858.365773	36.600436
1515.139690	185159.623296	36.605453
1516.696222	185467.663680	36.610471
1517.433568	185792.989212	36.615488
1519.064600	186102.353654	36.620506
1520.218186	186406.924466	36.625524
1521.748103	186740.857708	36.630541
1522.831882	187058.568413	36.635559
1524.228432	187390.192010	36.640576
1525.789450	187718.870951	36.645594
1527.246697	188041.856866	36.650612
1528.534100	188375.332168	36.655629
1530.442113	188705.305128	36.660647
1531.915640	189036.113324	36.665664
1533.444772	189342.631031	36.670682
1535.021411	189659.995789	36.675700
1536.277588	189963.388383	36.680717
1538.130574	190264.081819	36.685735
1539.620794	190596.762245	36.690752
1540.901092	190900.422327	36.695770
1542.344641	191224.507403	36.700788
1543.492438	191550.191765	36.705805
1545.058447	191880.708927	36.710823
1546.243439	192212.420600	36.715840
1547.717161	192549.532405	36.720858
1548.931227	192901.503499	36.725876
1550.546998	193252.128201	36.730893
1552.599162	193582.891876	36.735911
1555.001481	193916.709786	36.740928
1556.736798	194245.358524	36.745946
1558.241001	194582.920894	36.750964
1559.932869	194921.126971	36.755981
1561.250389	195245.076646	36.760999
1562.250139	195600.640484	36.766016
1564.016247	195943.041920	36.771034
1565.638818	196289.569463	36.776052
1566.601455	196653.828901	36.781069
1568.664830	197001.341290	36.786087
1569.920589	197365.632577	36.791104
1571.821825	197719.967670	36.796122
1573.652777	198077.947237	36.801140
1574.859079	198423.907466	36.806157
1576.321706	198781.189907	36.811175
1577.923409	199156.669821	36.816192
1579.257924	199525.365555	36.821210
1580.807173	199889.762046	36.826228
1582.263428	200281.599265	36.831245
1584.240158	200645.408758	36.836263
1586.084618	201005.725182	36.841280
1588.105512	201364.503535	36.846298
1590.295030	201707.741063	36.851316
1591.732863	202080.610649	36.856333
1593.359521	202434.127110	36.861351
1594.993564	202798.956700	36.866368
1596.211323	203164.136184	36.871386
1597.716091	203531.123889	36.876404
1598.903113	203903.422328	36.881421
1600.646728	204265.283000	36.886439
1602.265729	204629.921245	36.891456
1604.177006	204990.665931	36.896474
1606.151167	205356.912482	36.901492
1607.747345	205721.229783	36.906509
1609.086111	206081.210853	36.911527
1610.933471	206452.727597	36.916544
1612.435108	206822.220875	36.921562
1614.239466	207182.536680	36.926580
1615.691697	207561.437648	36.931597
1617.164236	207922.598906	36.936615
1618.803752	208305.662746	36.941632
1620.359235	208664.591706	36.946650
1622.045418	209045.886508	36.951668
1623.846690	209414.441151	36.956685
1625.741188	209763.084875	36.961703
1627.365672	210144.674448	36.966720
1629.131062	210520.173030	36.971738
1630.710132	210879.831784	36.976756
1631.790458	211259.700560	36.981773
1633.818587	211614.780669	36.986791
1635.608551	211994.840462	36.991808
1636.851273	212347.742228	36.996826
1638.850731	212723.250223	37.001844
1640.252684	213086.084097	37.006861
1642.198345	213421.858775	37.011879
1643.669797	213784.303166	37.016896
1644.895420	214128.300866	37.021914
1646.484637	214481.535124	37.026932
1647.726883	214827.285175	37.031949
1649.692959	215186.885451	37.036967
1651.104448	215546.604062	37.041984
1652.302139	215905.648253	37.047002
1653.854696	216281.397478	37.052020
1655.148386	216642.612868	37.057037
1656.824595	217026.827424	37.062055
1658.203447	217427.601022	37.067072
1659.868309	217818.627217	37.072090
1661.418240	218236.392421	37.077108
1662.529999	218684.988560	37.082125
1664.106860	219085.609400	37.087143
1665.304190	219506.816147	37.092160
1666.744917	219925.520888	37.097178
1668.587277	220341.367290	37.102196
1670.106122	220778.044672	37.107213
1671.845299	221198.762681	37.112231
1673.335285	221646.700035	37.117248
1675.151947	222082.267012	37.122266
1677.253957	222497.266436	37.127284
1679.239668	222927.424413	37.132301
1681.308276	223355.462296	37.137319
1683.357419	223796.814200	37.142336
1684.771521	224224.760238	37.147354
1687.178467	224642.892351	37.152372
1688.635098	225073.044317	37.157389
1690.792551	225482.737252	37.162407
1692.714264	225902.935154	37.167424
1694.535774	226326.249846	37.172442
1696.591097	226721.511508	37.177460
1698.581771	227132.685439	37.182477
1700.447708	227530.571761	37.187495
1702.498516	227932.645263	37.192512
1704.951301	228327.643306	37.197530
1706.854794	228706.426288	37.202548
1708.442449	229104.414286	37.207565
1710.289070	229482.446917	37.212583
1712.040346	229869.386504	37.217600
1713.619146	230243.934837	37.222618
1715.950878	230631.695272	37.227636
1717.311829	231013.622424	37.232653
1718.689329	231392.830024	37.237671
1720.259162	231781.964012	37.242688
1722.186634	232169.719217	37.247706
1723.680500	232561.230130	37.252724
1724.849405	232953.735538	37.257741
1726.271896	233339.926095	37.262759
1728.079496	233741.294759	37.267776
1729.803639	234150.171589	37.272794
1730.995510	234545.725465	37.277812
1732.651489	234959.848309	37.282829
1734.724648	235367.502257	37.287847
1737.132561	235758.870495	37.292864
1738.818099	236156.277382	37.297882
1740.620217	236572.107490	37.302900
1741.967218	236967.082780	37.307917
1743.661357	237370.993881	37.312935
1745.651352	237771.732685	37.317952
1747.733589	238175.124350	37.322970
1749.873862	238562.859807	37.327988
1751.338504	238961.757349	37.333005
1753.343507	239354.063689	37.338023
1755.270746	239748.695235	37.343040
1756.788517	240136.968411	37.348058
1758.607548	240506.039473	37.353076
1759.826424	240877.750424	37.358093
1761.034787	241243.392656	37.363111
1762.828398	241626.034649	37.368128
1763.985581	242021.254819	37.373146
1765.586063	242433.777733	37.378164
1766.688499	242832.234458	37.383181
1768.320812	243246.963589	37.388199
1769.706720	243670.447130	37.393216
1770.608523	244106.890330	37.398234
1772.137804	244528.217884	37.403252
1774.295197	244970.907674	37.408269
1776.699943	245404.183840	37.413287
1778.991217	245826.226047	37.418304
1780.770955	246262.553383	37.423322
1783.074795	246687.033458	37.428340
1784.681108	247129.563561	37.433357
1786.364027	247569.490581	37.438375
1788.309647	247991.465880	37.443392
1789.880301	248432.428712	37.448410
1791.965036	248870.055738	37.453428
1793.622051	249314.892091	37.458445
1795.192902	249762.283494	37.463463
1797.093300	250221.382638	37.468480
1798.688000	250672.607001	37.473498
1800.710500	251125.285460	37.478516
1802.235961	251582.466519	37.483533
1804.082664	252046.758707	37.488551
1806.092994	252498.830852	37.493568
1807.777097	252957.307997	37.498586
1810.221506	253393.254520	37.503604
1812.434366	253842.144382	37.508621
1814.654469	254276.375736	37.513639
1816.676709	254734.264999	37.518656
1818.251211	255197.842531	37.523674
1819.556151	255635.655120	37.528692
1821.526546	256099.625117	37.533709
1823.290126	256555.500419	37.538727
1825.202764	257009.115842	37.543744
1826.814714	257466.312099	37.548762
1829.117064	257911.328054	37.553780
1830.907902	258368.901534	37.558797
1832.838190	258812.175461	37.563815
1834.723861	259262.036285	37.568832
1836.217801	259729.312249	37.573850
1837.809522	260199.315679	37.578868
1839.650182	260664.222799	37.583885
1841.301991	261133.047769	37.588903
1842.905918	261603.303186	37.593920
1844.746770	262072.731955	37.598938
1847.199561	262528.595944	37.603956
1848.930632	263006.425714	37.608973
1850.511344	263474.855528	37.613991
1852.720534	263965.104528	37.619008
1854.133748	264428.862012	37.624026
1856.214774	264894.820820	37.629044
1858.113477	265373.917537	37.634061
1859.820753	265855.738298	37.639079
1861.886122	266322.435582	37.644096
1863.589154	266819.244293	37.649114
1865.430788	267293.065295	37.654132
1867.314610	267783.492619	37.659149
1868.862394	268269.326173	37.664167
1870.859955	268758.082647	37.669184
1872.511203	269240.214756	37.674202
1874.661193	269726.506402	37.679220
1876.161051	270207.874961	37.684237
1877.766175	270703.908526	37.689255
1879.658942	271169.029440	37.694272
1881.159515	271652.098138	37.699290
1882.845875	272124.415532	37.704308
1885.266913	272595.442568	37.709325
1887.442212	273069.227583	37.714343
1889.319136	273540.546250	37.719360
1890.662474	274019.598447	37.724378
1892.763208	274500.379344	37.729396
1894.634760	274968.368910	37.734413
1897.045696	275440.256935	37.739431
1899.494410	275915.364038	37.744448
1901.231141	276381.722253	37.749466
1903.453670	276859.608416	37.754484
1905.507940	277318.876037	37.759501
1907.025637	277802.109531	37.764519
1909.155373	278269.085199	37.769536
1910.399994	278764.554852	37.774554
1912.231517	279248.165370	37.779572
1914.128130	279750.460061	37.784589
1915.761244	280251.247498	37.789607
1917.508604	280754.631284	37.794624
1919.039224	281260.488151	37.799642
1920.864281	281765.380680	37.804660
1922.864097	282282.664548	37.809677
1924.317123	282813.042879	37.814695
1926.090703	283332.901303	37.819712
1928.117533	283875.095256	37.824730
1929.953773	284412.264058	37.829748
1932.193677	284940.499480	37.834765
1933.956203	285487.304166	37.839783
1936.154086	286014.552428	37.844800
1938.256376	286555.328155	37.849818
1940.391642	287093.632667	37.854836
1942.544973	287617.910949	37.859853
1944.777845	288157.719651	37.864871
1946.789389	288692.152507	37.869888
1948.563386	289237.265480	37.874906
1950.475942	289777.120974	37.879924
1952.306244	290323.363479	37.884941
1954.050983	290864.309225	37.889959
1955.941118	291424.482262	37.894976
1957.736250	291972.019280	37.899994
1960.512391	292517.664965	37.905012
1962.799463	293057.470781	37.910029
1964.879615	293594.997012	37.915047
1967.327856	294131.469592	37.920064
1969.299230	294668.653448	37.925082
1971.203233	295196.702158	37.930100
1973.338259	295738.603886	37.935117
1975.250928	296270.710217	37.940135
1977.409736	296796.169673	37.945152
1979.265889	297329.728103	37.950170
1980.738563	297863.677401	37.955188
1983.045924	298400.864459	37.960205
1984.966410	298939.204793	37.965223
1986.839521	299481.715576	37.970240
1988.769287	300030.081244	37.975258
1990.725687	300567.848510	37.980276
1992.868033	301119.094094	37.985293
1994.733225	301661.061289	37.990311
1996.217199	302210.758562	37.995328
1998.143868	302778.996276	38.000346
2000.261027	303319.236471	38.005364
2002.491875	303865.245471	38.010381
2004.808217	304394.805144	38.015399
2006.973504	304950.266419	38.020416
2008.537052	305492.591743	38.025434
2010.578829	306025.565095	38.030452
2012.702373	306544.578998	38.035469
2014.758148	307073.708869	38.040487
2016.968354	307593.972123	38.045504
2018.641664	308121.228586	38.050522
2020.317514	308629.840653	38.055540
2022.440722	309165.473350	38.060557
2024.487707	309686.538022	38.065575
2026.881431	310221.001906	38.070592
2028.695772	310754.084933	38.075610
2030.833641	311274.667411	38.080628
2032.998240	311790.721775	38.085645
2035.016364	312328.128708	38.090663
2037.523201	312843.078569	38.095680
2039.446578	313386.436244	38.100698
2041.947952	313901.253003	38.105716
2044.605696	314412.917007	38.110733
2046.776058	314922.169314	38.115751
2048.972715	315449.519684	38.120768
2050.726703	315972.266871	38.125786
2053.058836	316482.091244	38.130804
2054.561059	317004.466287	38.135821
2056.857713	317516.219138	38.140839
2059.296412	318025.837280	38.145856
2061.230412	318553.817830	38.150874
2063.096770	319078.098245	38.155892
2065.487323	319595.660831	38.160909
2067.543739	320135.365896	38.165927
2069.276806	320658.386676	38.170944
2071.263022	321192.711826	38.175962
2073.036270	321730.851205	38.180980
2075.097272	322265.739459	38.185997
2076.790775	322825.948256	38.191015
2078.579138	323382.099445	38.196032
2080.014873	323942.391939	38.201050
2081.721611	324520.281291	38.206068
2083.379476	325101.144130	38.211085
2084.761037	325689.638830	38.216103
2086.619193	326281.273904	38.221120
2088.680219	326895.517391	38.226138
2090.768358	327510.029546	38.231156
2092.879618	328108.206506	38.236173
2095.100136	328737.587767	38.241191
2097.068042	329352.888027	38.246208
2099.063311	329981.201574	38.251226
2101.231691	330626.235929	38.256244
2103.940184	331222.734261	38.261261
2106.730283	331851.125012	38.266279
2108.949756	332466.833207	38.271296
2111.266391	333083.965740	38.276314
2112.946791	333708.126972	38.281332
2115.083864	334315.095497	38.286349
2116.804287	334951.167725	38.291367
2119.093500	335572.389631	38.296384
2120.991952	336206.564697	38.301402
2123.176907	336838.831928	38.306420
2125.282839	337468.464679	38.311437
2127.348585	338110.128858	38.316455
2129.302114	338756.195182	38.321472
2131.713863	339378.900852	38.326490
2133.940989	340013.965913	38.331508
2136.598004	340648.926827	38.336525
2139.501463	341270.310030	38.341543
2141.891796	341867.885083	38.346560
2144.590512	342484.438946	38.351578
2146.899022	343081.581458	38.356596
2149.599061	343689.794773	38.361613
2151.405077	344293.300116	38.366631
2153.564252	344875.876428	38.371648
2155.825734	345448.073456	38.376666
2157.603217	346019.302874	38.381684
2159.424604	346590.467444	38.386701
2161.383311	347150.054606	38.391719
2163.336840	347723.594763	38.396736
2165.392345	348307.618098	38.401754
2166.891371	348912.968067	38.406772
2168.855707	349498.438002	38.411789
2170.369587	350105.114883	38.416807
2172.250091	350723.625483	38.421824
2174.098588	351340.483346	38.426842
2175.496462	351967.938609	38.431860
2177.941367	352602.571672	38.436877
2179.993761	353263.372814	38.441895
2182.000130	353903.439289	38.446912
2184.121397	354559.895553	38.451930
2186.278396	355221.969311	38.456948
2188.635911	355883.644561	38.461965
2190.923948	356551.385545	38.466983
2192.821977	357215.120460	38.472000
2195.357988	357882.723393	38.477018
2197.389827	358573.463215	38.482036
2199.735345	359241.151922	38.487053
2201.866520	359933.324302	38.492071
2204.108754	360624.324926	38.497088
2206.400310	361303.025785	38.502106
2208.474029	362007.680581	38.507124
2211.107436	362684.931723	38.512141
2213.240697	363370.727537	38.517159
2215.762942	364068.650259	38.522176
2218.334153	364749.352011	38.527194
2220.328023	365446.424025	38.532212
2223.088476	366130.114706	38.537229
2225.093530	366829.011860	38.542247
2227.320743	367523.014402	38.547264
2229.875361	368204.900873	38.552282
2232.226061	368915.473077	38.557300
2234.525228	369612.875250	38.562317
2236.644785	370298.930135	38.567335
2238.628528	370998.971006	38.572352
2241.006834	371701.774371	38.577370
2243.170702	372407.846235	38.582388
2245.147829	373113.174272	38.587405
2247.447248	373827.414020	38.592423
2249.489844	374543.051505	38.597440
2251.823966	375247.593958	38.602458
2253.880948	375978.341501	38.607476
2256.095383	376695.352839	38.612493
2258.517683	377423.423232	38.617511
2261.020725	378139.621852	38.622528
2263.320782	378862.762310	38.627546
2265.697527	379575.376214	38.632564
2268.229920	380288.710347	38.637581
2270.431013	381021.356281	38.642599
2273.263142	381728.473993	38.647616
2275.786385	382433.117388	38.652634
2277.537639	383153.518145	38.657652
2280.522194	383853.922263	38.662669
2283.044562	384560.827981	38.667687
2285.213661	385275.662062	38.672704
2287.885942	385969.099890	38.677722
2290.631557	386654.828597	38.682740
2293.478223	387324.680284	38.687757
2295.444501	388005.336626	38.692775
2297.885569	388705.193134	38.697792
2300.250133	389359.287184	38.702810
2302.526301	390046.668205	38.707828
2304.966051	390707.034251	38.712845
2306.958102	391367.941798	38.717863
2309.077556	391999.915895	38.722880
2311.383246	392655.623668	38.727898
2313.358750	393317.683652	38.732916
2315.180574	393963.988298	38.737933
2317.372205	394627.606499	38.742951
2319.316202	395292.670415	38.747968
2321.251231	395968.949494	38.752986
2322.822775	396654.651131	38.758004
2325.151598	397353.949139	38.763021
2327.626342	398047.985669	38.768039
2329.232983	398765.921506	38.773056
2331.709242	399467.299389	38.778074
2333.423184	400200.210901	38.783092
2335.740603	400921.195114	38.788109
2337.886626	401654.657523	38.793127
2340.083935	402406.768811	38.798144
2342.594605	403149.078131	38.803162
2344.369664	403918.754440	38.808180
2346.616207	404657.621737	38.813197
2349.248805	405429.370622	38.818215
2351.416442	406193.472404	38.823232
2353.981871	406965.671341	38.828250
2356.351713	407746.976563	38.833268
2358.683878	408515.623659	38.838285
2361.196690	409314.164632	38.843303
2364.041940	410075.007002	38.848320
2367.587174	410834.876636	38.853338
2370.092624	411612.603521	38.858356
2372.505962	412382.141012	38.863373
2374.849379	413151.566546	38.868391
2376.684881	413933.845201	38.873408
2379.229338	414704.940283	38.878426
2381.623514	415492.602377	38.883444
2384.175350	416273.680225	38.888461
2386.634057	417051.406843	38.893479
2389.040079	417838.033628	38.898496
2392.117732	418611.204501	38.903514
2394.367931	419397.201475	38.908532
2396.824806	420166.502380	38.913549
2399.174771	420934.354194	38.918567
2401.422395	421725.496114	38.923584
2403.879647	422500.322157	38.928602
2406.357671	423287.882451	38.933620
2408.633370	424073.476245	38.938637
2411.290177	424859.716560	38.943655
2413.635069	425657.730943	38.948672
2416.323427	426437.839225	38.953690
2418.693603	427229.722001	38.958708
2421.361881	428006.036514	38.963725
2423.936580	428780.822641	38.968743
2425.855881	429573.968783	38.973760
2428.576854	430357.337415	38.978778
2430.885869	431153.505774	38.983796
2433.370827	431934.583265	38.988813
2435.786257	432725.770756	38.993831
2437.696487	433523.139952	38.998848
2440.353963	434318.637775	39.003866
2442.787033	435121.636689	39.008884
2445.075521	435926.909306	39.013901
2447.505684	436735.015420	39.018919
2449.541607	437547.308233	39.023936
2452.333195	438330.296558	39.028954
2455.109953	439133.503491	39.033972
2457.430673	439941.210462	39.038989
2460.239738	440746.885047	39.044007
2462.304670	441543.393187	39.049024
2465.198503	442331.134208	39.054042
2467.369656	443103.483275	39.059060
2469.988456	443857.364910	39.064077
2472.690596	444616.468960	39.069095
2475.088375	445382.578869	39.074112
2477.826049	446151.287283	39.079130
2480.328333	446901.036141	39.084148
2482.763200	447659.926680	39.089165
2484.824998	448430.588126	39.094183
2487.256952	449199.592832	39.099200
2490.369069	449954.193457	39.104218
2493.342021	450693.464280	39.109236
2496.376302	451450.351449	39.114253
2499.000573	452198.832713	39.119271
2501.296544	452962.817685	39.124288
2503.360038	453723.374176	39.129306
2505.184895	454509.278900	39.134324
2507.122188	455292.809228	39.139341
2509.259305	456078.097478	39.144359
2511.507432	456875.220629	39.149376
2513.996689	457684.610802	39.154394
2515.914284	458499.979016	39.159412
2518.492269	459328.806444	39.164429
2521.050860	460158.917766	39.169447
2523.375573	461005.211469	39.174464
2525.866984	461840.522526	39.179482
2528.206660	462680.272358	39.184500
2530.744935	463525.716791	39.189517
2533.155148	464380.750392	39.194535
2535.307716	465269.048231	39.199552
2538.164118	466129.593642	39.204570
2540.212233	466998.624320	39.209588
2541.929629	467910.173603	39.214605
2544.534848	468807.333247	39.219623
2546.834718	469724.816167	39.224640
2549.572393	470642.890705	39.229658
2552.700714	471547.921593	39.234676
2555.147054	472458.226260	39.239693
2557.795510	473378.407271	39.244711
2559.981905	474313.372007	39.249728
2562.725892	475216.826247	39.254746
2565.322889	476156.986718	39.259764
2568.244709	477082.599395	39.264781
2571.320635	478010.110578	39.269799
2573.849875	478938.019018	39.274816
2576.632474	479859.677259	39.279834
2579.775280	480767.745367	39.284852
2582.448595	481689.986147	39.289869
2585.563745	482603.573115	39.294887
2588.033701	483512.524274	39.299904
2591.050958	484416.542575	39.304922
2593.570935	485332.513311	39.309940
2596.094486	486249.042482	39.314957
2599.129481	487152.162453	39.319975
2601.449922	488050.457406	39.324992
2604.307018	488961.793776	39.330010
2606.663731	489873.872184	39.335028
2609.593426	490779.852620	39.340045
2612.401055	491675.762089	39.345063
2614.759015	492582.954452	39.350080
2617.264583	493473.572074	39.355098
2619.998331	494377.933585	39.360116
2622.322104	495297.958465	39.365133
2624.749095	496198.540400	39.370151
2627.639424	497106.617436	39.375168
2630.318800	498020.331603	39.380186
2632.509392	498933.723857	39.385204
2635.174725	499849.157678	39.390221
2637.572189	500745.163996	39.395239
2640.102234	501631.717988	39.400256
2643.493160	502507.288578	39.405274
2646.661187	503367.314763	39.410292
2649.422379	504231.700744	39.415309
2652.347668	505085.625153	39.420327
2654.769064	505944.328660	39.425344
2657.644287	506803.819992	39.430362
2660.068707	507670.298961	39.435380
2662.027187	508526.824902	39.440397
2664.829430	509393.199947	39.445415
2667.413201	510287.999555	39.450432
2669.889299	511164.567622	39.455450
2672.254882	512047.407319	39.460468
2674.591484	512946.585678	39.465485
2677.060300	513850.328684	39.470503
2679.106351	514780.147949	39.475520
2681.772699	515695.295077	39.480538
2684.184426	516618.746336	39.485556
2686.833054	517567.048948	39.490573
2689.991373	518492.282166	39.495591
2692.446124	519442.618882	39.500608
2695.251629	520393.746362	39.505626
2697.566707	521343.989147	39.510644
2699.620029	522315.878924	39.515661
2702.657680	523287.393616	39.520679
2705.287182	524274.327402	39.525696
2707.895969	525250.371250	39.530714
2710.536102	526246.593742	39.535732
2712.940946	527236.393205	39.540749
2715.691150	528241.127652	39.545767
2718.169940	529251.479078	39.550784
2721.120259	530265.762721	39.555802
2723.923266	531282.619393	39.560820
2726.860186	532295.255751	39.565837
2730.027894	533316.996832	39.570855
2732.602705	534322.757043	39.575872
2735.882482	535342.375045	39.580890
2739.353256	536359.625215	39.585908
2742.264732	537365.421565	39.590925
2745.671014	538355.868536	39.595943
2748.840886	539359.017269	39.600960
2751.778583	540352.825449	39.605978
2754.706947	541326.994139	39.610996
2757.447652	542332.872489	39.616013
2759.972523	543313.260100	39.621031
2762.491165	544312.142359	39.626048
2765.267338	545297.380796	39.631066
2768.012278	546303.427777	39.636084
2770.286023	547318.079855	39.641101
2773.511184	548310.776634	39.646119
2776.039852	549305.327361	39.651136
2778.926516	550298.239051	39.656154
2782.185592	551308.061751	39.661172
2784.794202	552304.946691	39.666189
2787.571391	553308.567838	39.671207
2790.206298	554332.596806	39.676224
2792.766167	555333.540655	39.681242
2795.503259	556350.866035	39.686260
2797.695438	557364.033229	39.691277
2800.402906	558393.973624	39.696295
2802.553575	559422.770775	39.701312
2805.318461	560460.531538	39.706330
2808.040480	561484.703859	39.711348
2810.761372	562538.988541	39.716365
2813.899908	563572.022878	39.721383
2816.593091	564627.551212	39.726400
2819.570592	565671.145051	39.731418
2822.957700	566693.093948	39.736436
2825.835189	567699.931563	39.741453
2828.948676	568681.345303	39.746471
2832.072617	569677.293134	39.751488
2834.640984	570666.528048	39.756506
2837.677858	571657.215785	39.761524
2840.155535	572664.282763	39.766541
2842.783933	573644.542990	39.771559
2844.981535	574657.621601	39.776576
2847.441888	575662.847374	39.781594
2850.349275	576691.754855	39.786612
2852.541449	577740.465220	39.791629
2855.050293	578770.371629	39.796647
2857.844997	579828.992225	39.801664
2860.923653	580881.205430	39.806682
2863.848844	581935.411027	39.811700
2866.741930	582988.027209	39.816717
2869.613571	584063.525681	39.821735
2872.262537	585136.760035	39.826752
2874.945797	586217.365494	39.831770
2878.019093	587303.426053	39.836788
2880.559348	588413.290079	39.841805
2883.066973	589514.886704	39.846823
2885.806301	590629.727242	39.851840
2888.121483	591748.042365	39.856858
2890.951613	592891.575666	39.861876
2893.853879	594024.664842	39.866893
2897.026550	595155.146150	39.871911
2900.360740	596303.127684	39.876928
2903.599834	597446.704885	39.881946
2906.875533	598588.211132	39.886964
2909.645716	599755.232375	39.891981
2913.596682	600879.775158	39.896999
2917.276293	601999.847127	39.902016
2920.641522	603111.801183	39.907034
2924.203467	604217.607746	39.912052
2927.692397	605323.920622	39.917069
2930.905887	606431.072982	39.922087
2934.072697	607516.453657	39.927104
2936.762814	608619.975966	39.932122
2939.551813	609728.578812	39.937140
2941.889373	610827.540328	39.942157
2944.685332	611934.524160	39.947175
2947.380409	613068.629642	39.952192
2949.968005	614188.832000	39.957210
2952.994043	615310.099909	39.962228
2955.865030	616430.279937	39.967245
2959.057360	617563.795234	39.972263
2962.059150	618684.725248	39.977280
2964.615788	619815.713442	39.982298
2967.372578	620961.299091	39.987316
2970.259010	622103.294212	39.992333
2972.835182	623259.864715	39.997351
2976.851777	624384.090778	40.002368
2980.200000	625523.400769	40.007386
2983.402548	626645.126800	40.012404
2986.254576	627789.924346	40.017421
2989.704293	628902.180968	40.022439
2993.234237	630027.794415	40.027456
2996.264379	631146.378978	40.032474
2999.620980	632251.408303	40.037492
3002.685336	633376.542917	40.042509
3005.930299	634481.356894	40.047527
3009.015469	635577.294580	40.052544
3011.849697	636675.105536	40.057562
3015.066166	637781.322705	40.062580
3017.745595	638890.305367	40.067597
3021.116376	639985.881574	40.072615
3024.379657	641055.064236	40.077632
3027.151197	642119.577067	40.082650
3030.325262	643162.462433	40.087668
3033.152066	644210.037380	40.092685
3035.822517	645244.263716	40.097703
3038.990787	646289.773047	40.102720
3041.560515	647346.841928	40.107738
3044.565692	648400.338122	40.112756
3047.080610	649483.917162	40.117773
3049.893689	650546.543219	40.122791
3052.435438	651621.562299	40.127808
3054.907289	652724.785466	40.132826
3057.754052	653825.781569	40.137844
3060.515312	654945.903029	40.142861
3063.385620	656071.061256	40.147879
3066.021978	657208.832812	40.152896
3068.324957	658376.463514	40.157914
3071.549972	659522.487235	40.162932
3074.042592	660705.547069	40.167949
3076.787844	661897.334444	40.172967
3079.870441	663068.059788	40.177984
3082.728380	664299.859840	40.183002
3085.723604	665513.561720	40.188020
3088.917070	666721.852279	40.193037
3091.999742	667957.924547	40.198055
3095.079873	669202.992115	40.203072
3097.777014	670448.308270	40.208090
3100.884507	671711.797627	40.213108
3104.085891	672978.236037	40.218125
3107.202135	674242.976818	40.223143
3111.295936	675494.309708	40.228160
3113.913029	676774.900938	40.233178
3117.415594	678037.673613	40.238196
3121.758583	679286.120794	40.243213
3125.933545	680526.227995	40.248231
3129.723131	681757.835074	40.253248
3133.284047	682994.780027	40.258266
3136.898745	684224.644773	40.263284
3139.938432	685436.856698	40.268301
3142.827916	686667.108189	40.273319
3146.396024	687897.280074	40.278336
3148.980509	689119.801382	40.283354
3151.997856	690342.483133	40.288372
3154.970980	691580.392721	40.293389
3157.683090	692825.023186	40.298407
3161.156555	694057.992168	40.303424
3164.241781	695308.020883	40.308442
3167.519628	696545.093388	40.313460
3170.615410	697780.832891	40.318477
3173.760459	699041.782746	40.323495
3177.012150	700292.270427	40.328512
3179.631446	701547.245417	40.333530
3182.999786	702784.715966	40.338548
3186.142808	704057.981983	40.343565
3189.114352	705306.856694	40.348583
3192.533605	706573.166948	40.353600
3195.875198	707849.906489	40.358618
3198.575848	709112.345946	40.363636
3201.834487	710383.472416	40.368653
3204.386678	711671.214827	40.373671
3207.463195	712946.001351	40.378688
3210.334206	714256.670435	40.383706
3213.231614	715565.251708	40.388724
3216.208422	716868.816824	40.393741
3219.488308	718189.102653	40.398759
3222.563580	719485.021725	40.403776
3225.423783	720811.494340	40.408794
3228.828364	722136.776159	40.413812
3232.081233	723445.948650	40.418829
3234.815637	724749.214991	40.423847
3238.165583	726031.609350	40.428864
3241.345619	727329.500612	40.433882
3244.525287	728628.076373	40.438900
3247.864918	729915.302126	40.443917
3250.778394	731214.400243	40.448935
3253.915305	732518.094947	40.453952
3256.662070	733829.694633	40.458970
3259.607632	735134.382493	40.463988
3262.586655	736484.226514	40.469005
3265.557455	737834.634916	40.474023
3269.493022	739176.611758	40.479040
3273.315288	740511.275650	40.484058
3276.876904	741836.285541	40.489076
3280.425388	743192.055742	40.494093
3283.406714	744542.113513	40.499111
3287.093725	745891.478587	40.504128
3290.595282	747222.547488	40.509146
3294.057689	748580.460429	40.514164
3297.754975	749936.964849	40.519181
3300.783989	751299.010004	40.524199
3304.453756	752645.732177	40.529216
3307.817102	754007.098159	40.534234
3311.271455	755364.957997	40.539252
3314.318058	756733.823578	40.544269
3317.350794	758097.523255	40.549287
3320.534291	759469.273916	40.554304
3323.521079	760863.548479	40.559322
3326.820471	762258.007431	40.564340
3330.367503	763638.933724	40.569357
3333.422964	765046.103463	40.574375
3337.270112	766443.092183	40.579392
3340.964216	767832.666386	40.584410
3344.473534	769245.856524	40.589428
3347.780265	770619.341176	40.594445
3350.956785	772037.953584	40.599463
3354.529838	773436.034012	40.604480
3357.983912	774839.665754	40.609498
3361.510275	776242.870143	40.614516
3365.242097	777643.611188	40.619533
3368.635229	779046.986987	40.624551
3372.817755	780434.204884	40.629568
3375.643225	781832.276604	40.634586
3379.015878	783239.998164	40.639604
3382.539878	784630.641581	40.644621
3385.536103	786057.154780	40.649639
3388.683704	787462.958344	40.654656
3391.845948	788891.527277	40.659674
3394.869889	790307.920391	40.664692
3398.258103	791740.634650	40.669709
3401.253655	793175.769583	40.674727
3404.528593	794615.367668	40.679744
3407.488176	796075.686780	40.684762
3410.098305	797545.014676	40.689780
3414.014355	799000.550301	40.694797
3417.028183	800496.167104	40.699815
3420.519897	801981.595156	40.704832
3423.935877	803463.830005	40.709850
3427.216148	804936.914469	40.714868
3431.132082	806428.212442	40.719885
3434.026329	807924.390534	40.724903
3437.546972	809409.138356	40.729920
3440.760261	810916.535663	40.734938
3444.250375	812423.308257	40.739956
3448.152817	813904.517602	40.744973
3451.750693	815413.731836	40.749991
3455.650630	816900.875996	40.755008
3459.460101	818341.023141	40.760013
3463.568116	819765.124082	40.765018
3467.090411	821114.600708	40.770023
3470.230076	822399.345357	40.775028
3473.381748	823618.449602	40.780032
3476.600815	824769.935120	40.785037
3479.505983	825852.188395	40.790042
3481.996181	826856.705192	40.795047
3484.244082	827802.212132	40.800052
3486.957084	828674.250198	40.805056
3489.383215	829483.771306	40.810061
3492.310119	830205.066992	40.815066
3495.163365	830861.271082	40.820071
3497.261344	831465.802392	40.825076
3499.128848	832004.912272	40.830080
3501.004388	832465.243970	40.835085
3502.556662	832889.114078	40.840090
3504.484011	833267.428990	40.845095
3505.720559	833597.637584	40.850100
3506.713515	833892.027759	40.855104
3507.927673	834126.650526	40.860109
3509.006522	834336.385129	40.865114
3510.582741	834487.342111	40.870119
3511.062127	834631.445397	40.875124
3512.229545	834718.258905	40.880128
3513.055584	834767.484184	40.885133
3513.670392	834813.960923	40.890138
3514.898994	834806.142007	40.895143
3515.286080	834797.778156	40.900148
3516.131174	834746.617756	40.905152
3517.010330	834675.140252	40.910157
3516.860261	834581.811213	40.915162
3517.704479	834477.233490	40.920167
3517.753968	834356.281399	40.925172
3518.338770	834215.219303	40.930176
3518.683688	834052.073907	40.935181
3519.256063	833897.578801	40.940186
3519.630225	833695.013099	40.945191
3519.997092	833511.975729	40.950196
3520.212991	833285.543608	40.955200
3520.396414	833062.039140	40.960205
3520.674497	832839.488143	40.965210
3521.183699	832575.718895	40.970215
3520.720773	832339.792763	40.975220
3521.210821	832078.643951	40.980224
3521.177660	831805.896525	40.985229
3520.985365	831544.496696	40.990234
3521.199739	831272.467675	40.995239
3521.418033	830994.173505	41.000244
3521.305226	830707.176983	41.005248
3521.127957	830424.966393	41.010253
3521.517344	830129.262873	41.015258
3521.713868	829821.704413	41.020263
3521.593326	829520.682537	41.025268
3521.880962	829210.979146	41.030272
3521.865868	828902.386033	41.035277
3521.955857	828585.795136	41.040282
3522.057904	828268.209465	41.045287
3521.742993	827954.684834	41.050292
3521.787138	827625.103032	41.055296
3521.870920	827312.703940	41.060301
3521.738667	826987.713868	41.065306
3522.133338	826651.084047	41.070311
3521.732756	826333.096309	41.075316
3521.574659	825995.448410	41.080320
3521.716103	825671.619259	41.085325
3521.416457	825345.402088	41.090330
3521.507599	825002.626016	41.095335
3521.369072	824653.904159	41.100340
3521.292031	824337.820485	41.105344
3521.162176	823993.561283	41.110349
3521.165504	823674.987387	41.115354
3520.855252	823337.472875	41.120359
3520.785913	823021.129270	41.125364
3521.071209	822686.613810	41.130368
3520.766980	822357.901831	41.135373
3520.562379	822035.320954	41.140378
3520.485863	821702.478655	41.145383
3520.420922	821388.111053	41.150388
3520.318897	821049.271462	41.155392
3520.485720	820733.269040	41.160397
3520.343223	820394.647384	41.165402
3520.238944	820069.165379	41.170407
3519.727834	819758.659967	41.175412
3520.122521	819430.960336	41.180416
3519.740197	819109.294422	41.185421
3519.799951	818797.622453	41.190426
3519.793198	818453.104486	41.195431
3519.380217	818150.192473	41.200436
3519.681360	817834.519987	41.205440
3519.521214	817511.565723	41.210445
3519.579561	817205.938830	41.215450
3519.373740	816879.192075	41.220455
3518.804917	816569.135382	41.225460
3518.825386	816258.330784	41.230464
3518.777365	815946.201050	41.235469
3518.918579	815647.980986	41.240474
3518.890881	815328.033579	41.245479
3518.459488	815028.264385	41.250484
3518.681451	814710.841942	41.255488
3518.613572	814405.989923	41.260493
3518.010211	814104.934588	41.265498
3518.108511	813815.848153	41.270503
3517.812384	813507.319638	41.275508
3517.739668	813204.912187	41.280512
3517.705319	812929.427138	41.285517
3517.754930	812633.783009	41.290522
3517.511568	812337.537344	41.295527
3517.072662	812049.492622	41.300532
3517.175410	811759.533637	41.305536
3516.928616	811475.009424	41.310541
3516.918861	811198.273967	41.315546
3516.973112	810918.086655	41.320551
3516.749658	810647.733996	41.325556
3516.800249	810359.242836	41.330560
3516.821267	810074.174758	41.335565
3516.794082	809805.275461	41.340570
3516.908156	809508.259297	41.345575
3516.465033	809252.198402	41.350580
3516.395804	808967.000801	41.355584
3516.264354	808681.899553	41.360589
3516.150861	808421.243629	41.365594
3516.049747	808141.506822	41.370599
3515.725755	807872.776268	41.375604
3515.957479	807615.513313	41.380608
3515.540000	807351.238846	41.385613
3515.242047	807082.816134	41.390618
3515.358702	806825.395342	41.395623
3515.405273	806568.417707	41.400628
3515.355561	806306.935216	41.405632
3515.204667	806048.205401	41.410637
3515.103703	805805.885044	41.415642
3515.236260	805530.073122	41.420647
3514.871931	805288.415391	41.425652
3514.668670	805038.483485	41.430656
3514.468837	804782.705651	41.435661
3514.704644	804546.465001	41.440666
3514.725329	804305.248809	41.445671
3514.614361	804063.261064	41.450676
3514.451216	803812.346085	41.455680
3514.101807	803570.085990	41.460685
3513.943439	803333.280044	41.465690
3514.113020	803100.925139	41.470695
3513.963091	802861.109169	41.475700
3513.939066	802619.694223	41.480704
3513.976132	802387.386212	41.485709
3513.652582	802149.291291	41.490714
3513.775617	801910.231450	41.495719
3513.433848	801702.838661	41.500724
3513.117396	801454.807289	41.505728
3513.499800	801238.399996	41.510733
3513.071221	801023.886092	41.515738
3513.239911	800789.785329	41.520743
3512.792549	800577.174540	41.525748
3512.871821	800352.446928	41.530752
3512.700153	800135.311298	41.535757
3512.645291	799919.769245	41.540762
3512.560450	799715.759332	41.545767
3512.399775	799487.509500	41.550772
3512.291521	799275.146593	41.555776
3512.350231	799076.198960	41.560781
3512.104796	798869.981893	41.565786
3512.358539	798661.467553	41.570791
3512.122664	798454.942106	41.575796
3512.092707	798241.258479	41.580800
3512.205507	798042.959727	41.585805
3511.937352	797835.488514	41.590810
3512.145911	797632.056594	41.595815
3511.655565	797436.687488	41.600820
3511.731353	797238.421096	41.605824
3511.632267	797036.937347	41.610829
3511.610668	796839.755881	41.615834
3511.261039	796644.292359	41.620839
3510.871614	796455.360666	41.625844
3511.323348	796267.660252	41.630848
3511.333872	796082.580994	41.635853
3511.064589	795895.234904	41.640858
3511.381412	795713.827608	41.645863
3510.990458	795517.602844	41.650868
3510.828809	795322.120601	41.655872
3510.734092	795158.986977	41.660877
3510.699270	794961.803999	41.665882
3510.493460	794774.417544	41.670887
3510.302054	794586.876373	41.675892
3510.542086	794419.986739	41.680896
3510.624951	794245.702121	41.685901
3510.512972	794065.550892	41.690906
3510.106872	793897.822033	41.695911
3509.948033	793730.834406	41.700916
3510.342812	793556.432237	41.705920
3510.410732	793375.791632	41.710925
3510.104951	793207.096440	41.715930
3510.172694	793042.364108	41.720935
3510.055268	792863.951649	41.725940
3509.825072	792706.187637	41.730944
3510.205975	792527.881124	41.735949
3509.979683	792358.661260	41.740954
3510.255847	792189.649379	41.745959
3509.464839	792021.693658	41.750964
3509.440659	791858.570302	41.755968
3509.565500	791689.276584	41.760973
3509.360875	791534.479540	41.765978
3509.814954	791362.765186	41.770983
3509.185574	791222.330642	41.775988
3509.606215	791065.110785	41.780992
3508.829470	790899.828833	41.785997
3508.678588	790756.308576	41.791002
3509.200413	790606.580758	41.796007
3508.822858	790455.081272	41.801012
3509.061664	790296.399989	41.806016
3508.974142	790161.801864	41.811021
3508.853413	789997.521213	41.816026
3508.977524	789844.648219	41.821031
3508.745554	789711.736436	41.826036
3508.776811	789561.231851	41.831040
3508.800842	789414.018473	41.836045
3508.463722	789264.797101	41.841050
3508.580982	789117.906315	41.846055
3508.427467	788980.494908	41.851060
3508.466977	788831.497347	41.856064
3508.152567	788702.611106	41.861069
3508.189805	788558.032342	41.866074
3508.644363	788424.196908	41.871079
3508.360984	788275.339227	41.876084
3508.020169	788138.237393	41.881088
3508.414567	788006.272151	41.886093
3508.097849	787879.092072	41.891098
3508.331397	787724.139881	41.896103
3507.698536	787612.297070	41.901108
3507.699815	787474.142839	41.906112
3508.112949	787348.652222	41.911117
3507.656845	787214.354124	41.916122
3507.926448	787084.113271	41.921127
3507.431375	786950.209975	41.926132
3507.539702	786818.319096	41.931136
3507.612015	786708.411126	41.936141
3507.079069	786586.603282	41.941146
3507.302378	786449.769504	41.946151
3507.444538	786351.006723	41.951156
3507.645929	786220.663056	41.956160
3507.597916	786080.621424	41.961165
3507.292629	785960.240681	41.966170
3507.327786	785834.294033	41.971175
3507.467391	785725.392618	41.976180
3507.281069	785604.297818	41.981184
3507.205045	785476.396064	41.986189
3507.001056	785363.660590	41.991194
3507.559237	785234.912370	41.996199
3507.230510	785121.701834	42.001204
3507.390099	785000.441508	42.006208
3507.092148	784882.795705	42.011213
3506.751061	784758.662766	42.016218
3507.123931	784647.739223	42.021223
3507.153903	784528.508872	42.026228
3507.012319	784410.337723	42.031232
3507.059158	784298.134457	42.036237
3506.979999	784195.837005	42.041242
3506.829740	784062.462443	42.046247
3506.735527	783970.592325	42.051252
3506.737993	783855.241332	42.056256
3506.692489	783729.812194	42.061261
3506.664521	783627.990156	42.066266
3506.874304	783513.927734	42.071271
3506.563319	783410.821044	42.076276
3506.408804	783299.373292	42.081280
3506.842439	783202.437823	42.086285
3506.443105	783094.716848	42.091290
3506.319222	782987.686836	42.096295
3506.201075	782897.381267	42.101300
3506.077386	782788.429588	42.106304
3506.250954	782673.031505	42.111309
3506.327741	782594.792853	42.116314
3506.508745	782478.554057	42.121319
3505.914907	782378.972396	42.126324
3505.883610	782279.099896	42.131328
3506.069866	782179.829805	42.136333
3505.808135	782082.255825	42.141338
3506.071906	781987.398547	42.146343
3505.964330	781884.334957	42.151348
3505.789075	781790.629900	42.156352
3505.926159	781698.741975	42.161357
3505.885763	781605.651975	42.166362
3505.800991	781502.087128	42.171367
3505.547531	781422.610830	42.176372
3505.402769	781318.708793	42.181376
3505.812598	781236.168732	42.186381
3505.228468	781147.787982	42.191386
3505.562920	781054.825995	42.196391
3505.149952	780979.012601	42.201396
3505.275606	780895.482064	42.206400
3505.372022	780814.219091	42.211405
3505.354023	780730.365837	42.216410
3505.261029	780632.744531	42.221415
3505.515820	780552.141509	42.226420
3505.390594	780472.239963	42.231424
3505.619691	780385.930572	42.236429
3505.412435	780302.103545	42.241434
3505.573481	780205.025217	42.246439
3505.518648	780137.067676	42.251444
3505.191694	780042.528342	42.256448
3505.317373	779957.166003	42.261453
3504.868871	779879.968902	42.266458
3505.189818	779814.308880	42.271463
3505.323850	779725.251102	42.276468
3505.199287	779631.312920	42.281472
3505.189286	779550.004116	42.286477
3504.931067	779473.017446	42.291482
3505.035059	779392.820172	42.296487
3504.980899	779317.816296	42.301492
3504.882263	779229.233763	42.306496
3505.155197	779156.979995	42.311501
3504.913751	779083.579669	42.316506
3504.883959	778997.394892	42.321511
3504.795948	778932.138843	42.326516
3504.998917	778845.175568	42.331520
3505.051231	778769.803938	42.336525
3504.721123	778690.310358	42.341530
3504.846229	778601.092624	42.346535
3504.724751	778548.095929	42.351540
3504.573002	778465.863067	42.356544
3505.075925	778399.963419	42.361549
3504.819567	778324.884171	42.366554
3504.693868	778253.031704	42.371559
3504.504718	778178.432161	42.376564
3504.655425	778104.022022	42.381568
3504.768910	778035.180235	42.386573
3504.607224	777967.515423	42.391578
3504.681999	777884.992548	42.396583
3504.612482	777816.966542	42.401588
3504.422285	777743.790438	42.406592
3504.432923	777682.691666	42.411597
3504.211797	777616.953453	42.416602
3504.508856	777556.692637	42.421607
3504.207591	777490.031053	42.426612
3504.415151	777420.872580	42.431616
3504.217919	777355.423482	42.436621
3503.911010	777291.124265	42.441626
3504.309531	777221.144691	42.446631
3504.048448	777164.468291	42.451636
3504.309694	777096.725747	42.456640
3504.040171	777033.452066	42.461645
3503.965331	776968.767132	42.466650
3504.149557	776911.178387	42.471655
3504.008168	776861.471638	42.476660
3503.959828	776809.582746	42.481664
3504.155632	776737.219269	42.486669
3503.997977	776671.757532	42.491674
3504.233681	776607.362925	42.496679
3504.294037	776544.079914	42.501684
3504.364483	776486.851255	42.506688
3504.195635	776432.320562	42.511693
3504.105351	776371.325943	42.516698
3504.133123	776302.186517	42.521703
3504.147650	776243.340196	42.526708
3503.867181	776172.379124	42.531712
3503.839870	776113.390924	42.536717
3504.006351	776072.097864	42.541722
3504.170630	776019.478950	42.546727
3504.121715	775956.405837	42.551732
3503.600087	775891.784984	42.556736
3504.056108	775839.756902	42.561741
3503.649884	775781.764096	42.566746
3503.927051	775714.006151	42.571751
3503.264545	775658.713841	42.576756
3503.766133	775614.211271	42.581760
3503.623357	775566.121084	42.586765
3503.525903	775507.681277	42.591770
3503.775706	775446.031979	42.596775
3503.530201	775407.462396	42.601780
3503.922067	775351.797107	42.606784
3503.861034	775282.810446	42.611789
3503.751217	775247.665060	42.616794
3503.605578	775181.104562	42.621799
3503.601064	775131.560531	42.626804
3503.375280	775074.024900	42.631808
3503.801575	775025.492687	42.636813
3503.527125	774978.159089	42.641818
3503.369505	774920.955784	42.646823
3503.430068	774880.165979	42.651828
3503.720982	774825.301352	42.656832
3503.692670	774761.475808	42.661837
3503.561085	774720.864525	42.666842
3503.768278	774657.147041	42.671847
3503.635791	774610.083203	42.676852
3503.491804	774549.328551	42.681856
3503.619702	774488.134584	42.686861
3503.636434	774464.883999	42.691866
3503.559052	774404.215685	42.696871
3503.456621	774359.509498	42.701876
3503.356503	774299.730650	42.706880
3503.397149	774249.532923	42.711885
3503.408821	774206.580203	42.716890
3503.717531	774158.307923	42.721895
3503.465896	774106.384151	42.726900
3503.286103	774060.457483	42.731904
3503.453849	774006.493663	42.736909
3503.082115	773960.597988	42.741914
3503.223693	773909.790233	42.746919
3503.072064	773874.300366	42.751924
3502.833406	773835.622888	42.756928
3503.216683	773788.567357	42.761933
3502.949380	773745.559384	42.766938
3503.156999	773708.236229	42.771943
3503.308784	773659.395425	42.776948
3503.041574	773615.105934	42.781952
3503.161061	773577.895156	42.786957
3502.904244	773534.637925	42.791962
3503.419788	773491.302479	42.796967
3503.289707	773450.043552	42.801972
3503.433079	773412.483181	42.806977
3503.303023	773372.652382	42.811981
3503.305993	773314.375655	42.816986
3503.209323	773250.351229	42.821991
3503.226049	773216.357583	42.826996
3503.269181	773181.127871	42.832001
3503.103475	773131.941772	42.837005
3503.003975	773101.365873	42.842010
3503.139742	773044.050396	42.847015
3503.142099	773012.767665	42.852020
3502.818918	772961.241715	42.857025
3503.067062	772926.863770	42.862029
3502.876143	772881.670551	42.867034
3502.914096	772845.651859	42.872039
3503.149671	772805.068065	42.877044
3503.175934	772769.494312	42.882049
3502.952387	772716.718613	42.887053
3502.756438	772705.863157	42.892058
3503.007647	772635.075964	42.897063
3502.963560	772602.321162	42.902068
3502.933379	772571.140452	42.907073
3503.313275	772521.712618	42.912077
3502.907177	772497.096738	42.917082
3502.996417	772433.872148	42.922087
3502.819365	772406.114387	42.927092
3502.855043	772355.461182	42.932097
3503.048817	772317.936213	42.937101
3502.729857	772294.389204	42.942106
3502.879209	772242.878942	42.947111
3503.050269	772198.065334	42.952116
3503.117281	772167.704486	42.957121
3503.102076	772125.236772	42.962125
3502.850865	772086.847808	42.967130
3503.073000	772028.179946	42.972135
3502.592693	772006.530860	42.977140
3502.665218	771964.885368	42.982145
3502.782728	771942.398564	42.987149
3502.514033	771912.091965	42.992154
3502.739253	771869.928079	42.997159
3502.797845	771825.771268	43.002164
3502.404937	771790.458937	43.007169
3502.551481	771765.848130	43.012173
3502.280474	771735.787549	43.017178
3502.771206	771705.601372	43.022183
3502.492059	771659.528310	43.027188
3502.442461	771634.308831	43.032193
3502.709835	771603.863395	43.037197
3502.700566	771579.770366	43.042202
3502.690640	771535.820205	43.047207
3502.638885	771501.977778	43.052212
3502.586265	771477.103177	43.057217
3502.566465	771437.687249	43.062221
3502.493718	771408.282516	43.067226
3502.690311	771376.911597	43.072231
3502.700113	771343.797425	43.077236
3502.411932	771328.027662	43.082241
3502.739976	771281.408758	43.087245
3502.338777	771258.660395	43.092250
3502.762031	771217.494958	43.097255
3502.492381	771193.197184	43.102260
3502.331770	771158.287051	43.107265
3502.557751	771142.826409	43.112269
3502.290453	771109.264072	43.117274
3502.690390	771063.026164	43.122279
3502.492732	771040.588539	43.127284
3502.390064	771014.488711	43.132289
3502.921016	770988.038037	43.137293
3502.574932	770946.455774	43.142298
3502.627809	770919.590831	43.147303
3502.667698	770888.785713	43.152308
3502.429404	770846.790914	43.157313
3502.824697	770810.358514	43.162317
3502.735167	770788.789324	43.167322
3502.548043	770751.368444	43.172327
3502.528513	770720.178185	43.177332
3502.611038	770705.085215	43.182337
3502.677275	770646.087144	43.187341
3502.277523	770624.568575	43.192346
3502.439335	770592.460878	43.197351
3502.534382	770560.511879	43.202356
3502.231565	770533.851969	43.207361
3502.219927	770496.893700	43.212365
3502.315445	770471.399960	43.217370
3502.473000	770449.000594	43.222375
3502.390549	770430.878841	43.227380
3502.536145	770393.204227	43.232385
3502.411112	770375.089351	43.237389
3502.522837	770355.013465	43.242394
3502.290171	770310.846328	43.247399
3502.350995	770293.932680	43.252404
3502.496042	770256.602435	43.257409
3502.574755	770224.802529	43.262413
3502.284121	770200.209261	43.267418
3502.241812	770171.928105	43.272423
3502.508412	770134.182964	43.277428
3502.357384	770124.991928	43.282433
3502.172361	770089.440110	43.287437
3502.118426	770063.624607	43.292442
3502.100736	770032.579006	43.297447
3502.006426	770012.388282	43.302452
3502.018652	769981.140404	43.307457
3502.354532	769963.047170	43.312461
3502.360617	769935.890673	43.317466
3502.437082	769921.832076	43.322471
3502.262649	769876.913504	43.327476
3502.054041	769863.739589	43.332481
3502.338769	769824.264932	43.337485
3502.261344	769809.442914	43.342490
3502.426257	769777.035476	43.347495
3502.081446	769755.357477	43.352500
3502.177190	769733.754703	43.357505
3502.070557	769704.053086	43.362509
3501.909412	769688.850334	43.367514
3502.041879	769661.129873	43.372519
3502.289440	769649.950445	43.377524
3502.320260	769616.430819	43.382529
3502.044984	769587.791525	43.387533
3501.907473	769569.036017	43.392538
3501.985952	769539.056817	43.397543
3502.058120	769522.385978	43.402548
3501.934836	769516.935414	43.407553
3502.280401	769484.004075	43.412557
3501.974964	769472.718323	43.417562
3502.273288	769455.812935	43.422567
3502.203328	769415.507365	43.427572
3502.180644	769393.331661	43.432577
3502.255747	769359.507858	43.437581
3502.123692	769338.187899	43.442586
3502.326517	769298.674659	43.447591
3502.306644	769291.136787	43.452596
3501.811681	769252.280411	43.457601
3502.304082	769239.433515	43.462605
3501.979894	769212.575224	43.467610
3502.174895	769191.595283	43.472615
3501.840319	769174.448486	43.477620
3502.337764	769145.975943	43.482625
3502.435604	769126.736949	43.487629
3502.382481	769098.552071	43.492634
3502.121734	769077.548301	43.497639
3502.430184	769042.205929	43.502644
3502.015507	769036.950879	43.507649
3502.366207	768989.722401	43.512653
3502.152662	768988.426700	43.517658
3502.112355	768956.788852	43.522663
3502.080967	768929.881310	43.527668
3502.165446	768879.245634	43.532673
3502.238646	768870.459729	43.537677
3502.360880	768861.665738	43.542682
3502.261448	768823.333462	43.547687
3502.228799	768798.988808	43.552692
3502.073107	768776.340260	43.557697
3502.229460	768738.655501	43.562701
3502.195054	768726.584589	43.567706
3502.204304	768707.014060	43.572711
3502.430523	768674.246683	43.577716
3502.372091	768657.201083	43.582721
3501.961247	768637.995325	43.587725
3501.770486	768616.190042	43.592730
3502.042711	768590.118532	43.597735
3502.052468	768575.969798	43.602740
3501.948806	768559.522941	43.607745
3502.041223	768531.558411	43.612749
3502.100501	768516.662008	43.617754
3502.294041	768486.166686	43.622759
3502.176068	768469.574107	43.627764
3501.974588	768441.854827	43.632769
3502.070469	768421.184811	43.637773
3501.999599	768382.746977	43.642778
3501.878134	768377.147393	43.647783
3502.002333	768355.437349	43.652788
3501.953759	768331.438853	43.657793
3501.920858	768315.620633	43.662797
3501.779703	768289.517576	43.667802
3502.153669	768269.590054	43.672807
3502.162331	768243.905816	43.677812
3501.889636	768231.232515	43.682817
3502.221626	768206.973751	43.687821
3502.098321	768177.120904	43.692826
3502.075668	768157.504892	43.697831
3501.867609	768125.743263	43.702836
3502.118371	768113.131425	43.707841
3502.104437	768088.288407	43.712845
3502.194491	768073.188864	43.717850
3502.185201	768050.267513	43.722855
3502.079510	768025.981663	43.727860
3501.945279	768009.587925	43.732865
3502.112880	767976.038393	43.737869
3501.666567	767960.238219	43.742874
3501.916150	767937.520366	43.747879
3502.067212	767919.255437	43.752884
3501.788683	767904.019075	43.757889
3501.564745	767898.436010	43.762893
3501.602864	767869.984972	43.767898
3501.734792	767843.243799	43.772903
3501.426376	767842.012819	43.777908
3501.656500	767848.777981	43.782913
3501.928024	767821.323567	43.787917
3501.615458	767820.191862	43.792922
3501.719686	767804.793654	43.797927
3501.621201	767782.132662	43.802932
3501.595676	767766.706450	43.807937
3501.862106	767748.274206	43.812941
3501.525072	767744.139310	43.817946
3501.329683	767710.451182	43.822951
3501.938803	767695.709065	43.827956
3501.331654	767698.471175	43.832961
3501.890083	767684.131776	43.837965
3501.817045	767658.754776	43.842970
3501.589291	767645.432187	43.847975
3501.710702	767631.854862	43.852980
3501.757501	767623.811330	43.857985
3501.914544	767595.832652	43.862989
3501.686322	767594.785618	43.867994
3501.484342	767574.014424	43.872999
3501.835678	767549.602444	43.878004
3501.848045	767541.761694	43.883009
3501.680875	767531.781312	43.888013
3501.521381	767506.911037	43.893018
3501.797012	767490.990949	43.898023
3501.781873	767492.571012	43.903028
3501.475313	767458.554958	43.908033
3501.649934	767436.686040	43.913037
3501.859125	767424.178491	43.918042
3501.780633	767410.485791	43.923047
3502.069225	767390.076985	43.928052
3501.617395	767389.806267	43.933057
3501.879487	767359.048551	43.938061
3501.596424	767354.756644	43.943066
3501.759236	767336.932069	43.948071
3501.583627	767326.706297	43.953076
3501.541379	767302.407643	43.958081
3502.096332	767275.742667	43.963085
3501.895607	767274.247342	43.968090
3501.660389	767257.572777	43.973095
3501.841404	767240.188689	43.978100
3501.910849	767217.054605	43.983105
3501.999518	767192.487520	43.988109
3501.776457	767198.933505	43.993114
3501.776414	767172.753998	43.998119
3502.261421	767140.479597	44.003124
3501.710052	767131.054989	44.008129
3501.667915	767106.262655	44.013133
3501.625061	767086.302039	44.018138
3501.952722	767065.343583	44.023143
3502.072866	767047.821166	44.028148
3502.044437	767030.766911	44.033153
3501.819523	767017.541338	44.038157
3501.863349	766991.847005	44.043162
3501.733028	766972.787957	44.048167
3502.187433	766982.968217	44.053172
3502.080830	766943.937223	44.058177
3502.153422	766934.606803	44.063181
3501.874439	766899.696192	44.068186
3501.794069	766876.141996	44.073191
3501.623307	766875.677044	44.078196
3501.429236	766852.535935	44.083201
3501.889355	766817.404588	44.088205
3501.522311	766818.993454	44.093210
3501.718646	766824.335279	44.098215
3501.736720	766789.276613	44.103220
3501.976048	766783.074048	44.108225
3501.882738	766771.305508	44.113229
3501.651355	766735.301580	44.118234
3501.513934	766727.977703	44.123239
3501.726289	766715.074010	44.128244
3501.728533	766704.325036	44.133249
3501.923574	766675.301247	44.138253
3501.844049	766676.694865	44.143258
3501.843286	766641.342776	44.148263
3501.599004	766623.090502	44.153268
3501.667032	766620.022291	44.158273
3501.777036	766597.175447	44.163277
3501.459797	766577.061446	44.168282
3501.565520	766572.754351	44.173287
3501.666573	766565.588258	44.178292
3501.501243	766557.381297	44.183297
3501.773101	766511.826575	44.188301
3501.694864	766515.340196	44.193306
3501.846270	766493.620270	44.198311
3502.006713	766473.032851	44.203316
3501.674020	766462.486622	44.208321
3501.846842	766450.673740	44.213325
3501.885599	766433.311214	44.218330
3501.703689	766397.445434	44.223335
3501.675808	766410.023368	44.228340
3501.514326	766391.263815	44.233345
3501.857619	766372.519685	44.238349
3501.310733	766363.635746	44.243354
3501.635658	766361.807113	44.248359
3501.588459	766327.743192	44.253364
3501.897662	766316.992408	44.258369
3501.815570	766303.051734	44.263373
3501.557504	766286.625305	44.268378
3501.870113	766272.668868	44.273383
3501.845591	766245.947762	44.278388
3501.471067	766252.518123	44.283393
3501.588665	766218.327942	44.288397
3501.820366	766214.394360	44.293402
3501.678627	766197.159636	44.298407
3502.176557	766207.531023	44.303412
3501.847267	766176.027619	44.308417
3502.042160	766166.774716	44.313421
3502.032753	766138.818016	44.318426
3502.227699	766120.689403	44.323431
3502.309004	766094.246181	44.328436
3501.983392	766075.414253	44.333441
3502.117213	766043.686081	44.338445
3502.117265	766018.340790	44.343450
3502.184173	766002.797097	44.348455
3501.837663	765981.256324	44.353460
3501.923686	765966.399749	44.358465
3501.883638	765934.206651	44.363469
3501.532730	765925.684391	44.368474
3501.633615	765903.132799	44.373479
3501.826352	765891.118515	44.378484
3501.538312	765886.875888	44.383489
3501.735025	765862.483891	44.388493
3501.524659	765849.697654	44.393498
3501.812645	765831.996818	44.398503
3501.931224	765810.329633	44.403508
3501.880785	765804.469861	44.408513
3501.729936	765791.427164	44.413517
3502.015824	765773.973094	44.418522
3501.854993	765763.348255	44.423527
3501.836056	765728.981090	44.428532
3501.636237	765716.340823	44.433537
3502.102131	765701.618400	44.438541
3501.863610	765691.252816	44.443546
3501.720524	765665.634038	44.448551
3501.677214	765659.723666	44.453556
3501.517965	765636.277189	44.458561
3501.554286	765609.247919	44.463565
3501.585711	765604.459383	44.468570
3501.801458	765585.438425	44.473575
3501.771848	765572.128813	44.478580
3501.288746	765565.649742	44.483585
3501.529451	765550.027171	44.488589
3501.380933	765552.024116	44.493594
3501.218993	765532.818673	44.498599
3501.597752	765522.400490	44.503604
3501.187987	765500.918068	44.508609
3501.350432	765509.225216	44.513613
3501.369125	765506.460557	44.518618
3501.226976	765497.015782	44.523623
3501.415212	765497.034052	44.528628
3501.275150	765480.191909	44.533633
3501.423550	765454.228515	44.538637
3501.096239	765452.309848	44.543642
3501.431011	765443.378210	44.548647
3501.688604	765446.639758	44.553652
3501.384373	765451.128061	44.558657
3501.780725	765426.110001	44.563661
3501.484409	765412.252270	44.568666
3501.829864	765395.280649	44.573671
3501.733783	765392.436226	44.578676
3501.449752	765379.513378	44.583681
3501.662193	765368.431982	44.588685
3501.810065	765359.235146	44.593690
3501.810033	765339.065567	44.598695
3501.725842	765305.989387	44.603700
3501.568362	765310.650859	44.608705
3501.924490	765296.241613	44.613709
3501.869622	765277.708285	44.618714
3501.826130	765257.249756	44.623719
3501.986846	765248.790394	44.628724
3501.690788	765220.532286	44.633729
3501.715699	765199.223974	44.638733
3501.672142	765204.113323	44.643738
3501.729272	765171.457110	44.648743
3501.632294	765162.152418	44.653748
3501.272363	765159.647261	44.658753
3501.757552	765144.032893	44.663757
3501.455004	765122.186514	44.668762
3501.556442	765100.914634	44.673767
3501.843190	765092.582284	44.678772
3501.433562	765091.416820	44.683777
3501.988845	765054.634133	44.688781
3501.712688	765059.265992	44.693786
3501.798187	765044.062467	44.698791
3501.730275	765020.204490	44.703796
3501.408846	765000.086941	44.708801
3501.799722	764991.835961	44.713805
3501.363363	764985.398001	44.718810
3501.493927	764977.337834	44.723815
3501.921904	764944.964770	44.728820
3501.654377	764952.159753	44.733825
3501.897574	764935.203941	44.738829
3501.522746	764924.317260	44.743834
3501.371682	764902.642558	44.748839
3501.506666	764903.360044	44.753844
3501.265220	764884.560576	44.758849
3501.864063	764872.675043	44.763853
3501.749954	764863.915296	44.768858
3501.736563	764851.933307	44.773863
3501.964478	764829.949382	44.778868
3501.714623	764818.351514	44.783873
3501.950127	764807.512084	44.788877
3501.842995	764784.596859	44.793882
3501.586977	764766.046084	44.798887
3501.562056	764761.759474	44.803892
3501.468360	764745.203953	44.808897
3501.579458	764716.137106	44.813901
3501.332685	764714.204979	44.818906
3501.396323	764715.180828	44.823911
3501.796029	764701.207135	44.828916
3501.673369	764685.691944	44.833921
3502.042885	764658.653692	44.838925
3501.528026	764660.218026	44.843930
3501.332249	764633.963263	44.848935
3501.524821	764613.562736	44.853940
3501.545283	764613.657966	44.858945
3501.870175	764602.754199	44.863949
3501.860401	764591.806903	44.868954
3501.621033	764577.839611	44.873959
3501.749943	764560.556546	44.878964
3501.325383	764559.048218	44.883969
3501.645073	764529.798334	44.888973
3501.599754	764518.462230	44.893978
3501.600270	764518.314148	44.898983
3502.032482	764504.285416	44.903988
3501.239385	764495.735721	44.908993
3501.635870	764468.396425	44.913997
3501.559182	764462.885170	44.919002
3501.309146	764463.616800	44.924007
3501.507275	764427.629685	44.929012
3501.415257	764410.974512	44.934017
3501.739537	764401.648810	44.939021
3501.679359	764400.770916	44.944026
3501.503386	764390.935755	44.949031
3501.557241	764372.037042	44.954036
3501.440942	764366.433599	44.959041
3501.956209	764351.996338	44.964045
3501.733384	764337.236740	44.969050
3501.815567	764305.065850	44.974055
3501.844466	764303.778703	44.979060
3501.871480	764297.855675	44.984065
3501.604169	764255.039435	44.989069
3501.226792	764267.727844	44.994074
3501.384913	764261.733871	44.999079
3501.954074	764247.090248	45.004084
3501.570896	764228.657734	45.009089
3501.727523	764215.315042	45.014093
3501.640593	764217.992697	45.019098
3501.498869	764184.773097	45.024103
3501.779125	764174.221318	45.029108
3501.347006	764162.011271	45.034113
3501.817644	764160.947269	45.039117
3501.532958	764119.859394	45.044122
3501.669517	764110.860189	45.049127
3501.822242	764099.194897	45.054132
3501.358127	764100.603015	45.059137
3501.442974	764065.372669	45.064141
3501.666077	764060.452932	45.069146
3501.373416	764056.210022	45.074151
3501.683752	764050.092163	45.079156
3501.369863	764030.118742	45.084161
3501.389845	764024.098012	45.089165
3501.504624	763996.458148	45.094170
3501.255229	763999.803842	45.099175
3501.489039	764000.653108	45.104180
3501.197353	763998.678868	45.109185
3501.570376	763980.170507	45.114189
3501.679311	763955.194911	45.119194
3501.190356	763962.476632	45.124199
3501.341555	763948.887746	45.129204
3501.213841	763954.876883	45.134209
3501.466776	763945.808989	45.139213
3501.325124	763916.879338	45.144218
3501.386876	763907.842890	45.149223
3501.450425	763898.855459	45.154228
3501.473963	763895.102934	45.159233
3501.704411	763890.132554	45.164237
3501.309800	763865.239603	45.169242
3501.627939	763857.887204	45.174247
3501.673722	763847.472240	45.179252
3501.411681	763852.546426	45.184257
3501.612189	763832.339775	45.189261
3501.673196	763811.564157	45.194266
3501.261768	763808.080534	45.199271
3501.640684	763798.399819	45.204276
3501.314691	763797.417666	45.209281
3501.688908	763779.056589	45.214285
3501.508952	763766.459090	45.219290
3501.523642	763759.008605	45.224295
3501.584343	763763.783065	45.229300
3501.300965	763734.234836	45.234305
3501.631677	763712.230722	45.239309
3501.413701	763708.369912	45.244314
3501.487654	763712.451671	45.249319
3501.764527	763701.159914	45.254324
3501.400779	763679.516721	45.259329
3501.507370	763665.096143	45.264333
3501.620756	763656.346841	45.269338
3501.548493	763649.995729	45.274343
3501.470205	763623.126181	45.279348
3501.482392	763615.232035	45.284353
3501.754743	763610.303895	45.289357
3501.760634	763599.895160	45.294362
3501.372539	763578.650293	45.299367
3501.559972	763570.924539	45.304372
3501.602150	763566.132935	45.309377
3501.608680	763542.701947	45.314381
3501.391710	763550.185891	45.319386
3501.484758	763517.516591	45.324391
3501.522745	763508.976842	45.329396
3501.559475	763502.015736	45.334401
3501.868818	763510.596859	45.339405
3501.767881	763477.318095	45.344410
3501.795781	763463.699320	45.349415
3501.806341	763447.518386	45.354420
3501.301092	763432.408918	45.359425
3501.528408	763406.770758	45.364429
3501.343519	763411.585895	45.369434
3501.684972	763412.565480	45.374439
3501.633948	763391.955142	45.379444
3501.634773	763378.143363	45.384449
3501.408602	763358.844292	45.389453
3501.704140	763361.952522	45.394458
3501.197060	763352.713143	45.399463
3501.887554	763316.639628	45.404468
3501.612683	763323.886694	45.409473
3501.319064	763290.145568	45.414477
3501.669963	763298.966726	45.419482
3501.700523	763293.535603	45.424487
3501.797918	763267.474422	45.429492
3501.348840	763264.835320	45.434497
3501.851088	763246.501190	45.439501
3501.802998	763231.217359	45.444506
3501.694864	763210.961230	45.449511
3501.604515	763197.805408	45.454516
3501.497942	763198.316209	45.459521
3501.474323	763160.781071	45.464525
3501.614260	763165.394873	45.469530
3501.328439	763166.428488	45.474535
3501.436882	763158.813981	45.479540
3501.552839	763125.152637	45.484545
3501.700874	763115.706397	45.489549
3501.455330	763097.741729	45.494554
3501.414868	763102.829245	45.499559
3501.366851	763095.092460	45.504564
3501.309244	763071.423928	45.509569
3501.563091	763055.596713	45.514573
3501.551676	763051.208246	45.519578
3501.701771	763049.555617	45.524583
3501.618483	763029.936191	45.529588
3501.640254	763016.317619	45.534593
3501.610846	763016.223766	45.539597
3501.466575	763004.457717	45.544602
3501.191922	762988.569427	45.549607
3501.856775	762971.145113	45.554612
3501.176281	762973.625000	45.559617
3501.059105	762970.980451	45.564621
3501.276954	762970.599221	45.569626
3501.367946	762964.664609	45.574631
3501.372668	762955.537756	45.579636
3501.170289	762938.798847	45.584641
3501.573782	762915.497845	45.589645
3501.201397	762912.155360	45.594650
3501.366148	762910.450957	45.599655
3501.622265	762908.287530	45.604660
3501.281608	762907.209009	45.609665
3501.664405	762883.664667	45.614669
3501.395479	762871.968274	45.619674
3501.310267	762862.757462	45.624679
3501.796071	762862.332089	45.629684
3501.413231	762861.309840	45.634689
3501.385481	762824.168355	45.639693
3501.389777	762816.176012	45.644698
3501.251426	762810.427049	45.649703
3501.455132	762791.401032	45.654708
3501.413749	762804.727179	45.659713
3501.661207	762789.295109	45.664717
3501.310602	762767.449804	45.669722
3501.465836	762760.616489	45.674727
3501.700096	762749.379665	45.679732
3501.209632	762755.528165	45.684737
3501.576880	762725.079510	45.689741
3501.189258	762711.429160	45.694746
3500.700803	762709.486987	45.699751
3500.972550	762700.907821	45.704756
3501.052493	762702.917212	45.709761
3501.293946	762703.913366	45.714765
3501.039922	762701.241933	45.719770
3500.872685	762708.471857	45.724775
3501.103576	762697.778158	45.729780
3501.269881	762696.813426	45.734785
3501.209305	762687.253019	45.739789
3501.474888	762684.594654	45.744794
3501.436632	762673.797261	45.749799
3501.512033	762659.231907	45.754804
3501.403426	762658.263121	45.759809
3501.482006	762649.469055	45.764813
3501.520733	762617.002137	45.769818
3501.174173	762548.141821	45.774823
3501.059365	762425.272125	45.779828
3500.982589	762257.647890	45.784833
3500.941160	762032.883264	45.789837
3500.883623	761738.696507	45.794842
3500.769284	761392.108613	45.799847
3500.858880	760980.388359	45.804852
3500.569748	760519.411826	45.809857
3500.343082	760002.237855	45.814861
3500.105616	759414.604084	45.819866
3499.650226	758791.621307	45.824871
3499.498761	758087.535633	45.829876
3498.993376	757341.580763	45.834881
3498.869131	756515.952943	45.839885
3498.039089	755649.270665	45.844890
3498.209564	754719.510513	45.849895
3497.707183	753723.715238	45.854900
3497.313150	752668.992110	45.859905
3496.830711	751556.831889	45.864909
3496.422123	750380.513057	45.869914
3495.304930	749130.301514	45.874919
3495.316992	747826.174084	45.879924
3494.199950	746476.089654	45.884929
3493.574550	745045.690880	45.889933
3492.861314	743554.564697	45.894938
3492.114242	742007.714103	45.899943
3491.517395	740394.687802	45.904948
3490.630141	738733.383158	45.909953
3489.730498	736995.761134	45.914957
3489.200162	735199.780461	45.919962
3488.177641	733355.548265	45.924967
3487.703420	731443.000993	45.929972
3486.557054	729466.603668	45.934977
3485.707210	727423.228975	45.939981
3485.127979	725328.992188	45.944986
3483.698162	723166.887853	45.949991
3482.904565	720933.199032	45.954996
3481.530826	718664.581631	45.960001
3480.844644	716324.579968	45.965005
3479.604199	713923.815704	45.970010
3478.365581	711473.767223	45.975015
3477.516890	708955.411271	45.980020
3476.011393	706384.165479	45.985025
3474.936624	703742.068384	45.990029
3473.366294	701056.204660	45.995034
3472.263138	698333.491492	46.000039
3471.188214	695522.145720	46.005044
3469.909770	692669.295157	46.010049
3468.226395	689754.783047	46.015053
3467.258719	686791.416319	46.020058
3465.485052	683768.996682	46.025063
3464.638724	680680.213228	46.030068
3463.097440	677546.705145	46.035073
3461.579645	674348.725191	46.040077
3459.895136	671096.372071	46.045082
3458.459514	667794.120926	46.050087
3457.203287	664424.325122	46.055092
3455.078467	661027.185971	46.060097
3453.775397	657559.258588	46.065101
3452.177494	654025.160220	46.070106
3450.435786	650461.940517	46.075111
3449.005800	646823.761169	46.080116
3447.215548	643157.227635	46.085121
3445.443757	639411.579736	46.090125
3443.707288	635617.273432	46.095130
3441.369797	631793.201275	46.100135
3439.864328	627899.542869	46.105140
3437.998151	623955.975794	46.110145
3436.373973	619971.435332	46.115149
3434.147624	615936.657118	46.120154
3431.962733	611840.714065	46.125159
3430.084303	607679.048586	46.130164
3428.272321	603494.665838	46.135169
3425.870452	599260.754576	46.140173
3424.036414	594978.798688	46.145178
3422.226839	590665.640776	46.150183
3420.151431	586267.378258	46.155188
3417.793138	581857.565033	46.160193
3415.790777	577360.246549	46.165197
3413.717518	572844.265691	46.170202
3411.321254	568268.540232	46.175207
3409.342737	563644.240959	46.180212
3407.002951	558970.363025	46.185217
3404.530469	554260.702282	46.190221
3402.796397	549507.291861	46.195226
3400.002640	544693.618319	46.200231
3398.037216	539838.860708	46.205236
3395.157254	534955.557335	46.210241
3392.937114	530008.568446	46.215245
3390.606407	525032.983790	46.220250
3387.856744	520018.300795	46.225255
3385.881495	514944.509582	46.230260
3383.249945	509829.968967	46.235265
3380.498726	504674.181752	46.240269
3377.971480	499488.215211	46.245274
3375.144556	494251.066029	46.250279
3372.798909	488980.157060	46.255284
3369.964718	483673.124234	46.260289
3367.548823	478318.430611	46.265293
3365.304967	472936.882634	46.270298
3362.073528	467513.994572	46.275303
3359.583371	462028.910421	46.280308
3356.616204	456528.918063	46.285313
3354.087976	450981.138647	46.290317
3351.282415	445397.919847	46.295322
3348.303868	439792.908928	46.300327
3345.373275	434137.374360	46.305332
3342.194273	428448.682555	46.310337
3339.503242	422742.220181	46.315341
3336.789885	416996.751429	46.320346
3333.836984	411205.044341	46.325351
3330.945746	405393.257667	46.330356
3327.427516	399550.285647	46.335361
3324.559840	393668.426285	46.340365
3321.426511	387768.268714	46.345370
3318.041007	381840.165611	46.350375
3315.044067	375881.073071	46.355380
3312.007824	369894.302317	46.360385
3308.763144	363889.255243	46.365389
3306.017798	357841.006692	46.370394
3302.544275	351779.637999	46.375399
3298.966317	345683.721537	46.380404
3295.814809	339549.700062	46.385409
3292.493770	333405.813076	46.390413
3289.232333	327240.774765	46.395418
3285.526973	321063.756127	46.400423
3281.951811	314848.188670	46.405428
3278.625269	308648.740936	46.410433
3274.956505	302415.716445	46.415437
3271.568817	296163.426692	46.420442
3267.792031	289902.504844	46.425447
3264.625807	283613.974187	46.430452
3260.943096	277325.811874	46.435457
3257.572116	271014.435363	46.440461
3253.823044	264696.037801	46.445466
3250.323689	258352.214516	46.450471
3246.732329	252003.713199	46.455476
3242.721197	245642.424467	46.460481
3238.923561	239268.358504	46.465485
3235.471592	232875.598869	46.470490
3231.528654	226495.340015	46.475495
3227.809950	220090.374932	46.480500
3223.642833	213703.021907	46.485505
3219.559538	207254.163358	46.490509
3216.005013	200798.755701	46.495514
3211.709764	194391.727238	46.500519
3207.743956	187964.371432	46.505524
3203.348807	181563.405939	46.510529
3199.577504	175167.083462	46.515533
3195.269489	168761.346593	46.520538
3190.326994	162363.616482	46.525543
3186.375468	155991.706662	46.530548
3182.088947	149624.284341	46.535553
3177.427328	143251.743325	46.540557
3173.150946	136907.771441	46.545562
3168.147890	130589.180820	46.550567
3163.255850	124273.430938	46.555572
3158.501123	117995.129543	46.560577
3153.756220	111737.939890	46.565581
3148.899807	105499.440505	46.570586
3143.322166	99284.241546	46.575591
3138.433720	93124.641967	46.580596
3132.819349	86985.177390	46.585601
3126.833915	80904.518342	46.590605
3120.583065	74871.898267	46.595610
3113.387729	68935.726097	46.600615
3103.512489	63127.254355	46.605620
3086.898240	57587.536148	46.610625
3070.317786	52243.345325	46.615629
3053.679119	47136.004695	46.620634
3037.519091	42274.136093	46.625639
3022.301089	37655.767666	46.630644
3007.770420	33321.245882	46.635649
2993.673100	29263.065254	46.640653
2980.589188	25479.312193	46.645658
2968.088603	21949.831247	46.650663
2956.610819	18666.174310	46.655668
2945.178773	15644.659381	46.660673
2933.950251	12834.889497	46.665677
2923.309358	10255.872878	46.670682
2913.014366	7894.105753	46.675687
2903.017804	5728.563493	46.680692
2892.575061	3783.270655	46.685697
2879.136358	2119.445266	46.690701
2860.735898	795.568028	46.695706
2823.445552	292.125901	46.700711
2784.185728	295.835033	46.705716
2767.105526	285.791868	46.710721
2767.120524	297.685690	46.715725
2777.211636	290.156884	46.720730
2789.008225	298.391386	46.725735
2798.659791	286.799965	46.730740
2803.049632	283.149289	46.735745
2803.987779	276.848612	46.740749
2801.670794	275.321698	46.745754
2798.120668	279.339096	46.750759
2794.365674	269.779054	46.755764
2791.299637	279.675857	46.760769
2788.161818	272.631200	46.765773
2785.396031	266.270682	46.770778
2782.338803	276.639301	46.775783
2780.055508	276.268649	46.780788
2777.349420	269.311861	46.785793
2774.296866	278.056672	46.790797
2771.528860	276.907304	46.795802
2767.997480	271.594882	46.800807
2764.841121	262.642961	46.805812
2761.898578	263.223947	46.810817
2758.488065	266.847185	46.815821
2755.491526	263.532346	46.820826
2752.190342	257.376435	46.825831
2749.067298	251.273439	46.830836
2746.033604	260.137575	46.835841
2742.709077	264.195048	46.840845
2739.403623	263.476057	46.845850
2736.105589	263.740855	46.850855
2732.816890	256.827463	46.855860
2729.325961	260.188119	46.860865
2725.992059	268.867150	46.865869
2722.923152	257.375164	46.870874
2719.429324	262.819092	46.875879
2716.039116	264.276000	46.880884
2712.584814	257.883018	46.885889
2708.822726	252.004581	46.890893
2705.886134	255.096463	46.895898
2702.194032	261.456677	46.900903
2699.222611	257.531956	46.905908
2696.271658	260.000514	46.910913
2692.434557	258.255635	46.915917
2689.030868	260.939035	46.920922
2685.581206	260.003115	46.925927
2682.469402	247.695809	46.930932
2678.947344	250.948850	46.935937
2675.305113	241.482085	46.940941
2671.604639	262.615392	46.945946
2668.626224	251.096483	46.950951
2665.493286	253.202492	46.955956
2662.203988	259.353845	46.960961
2657.717576	256.971660	46.965965
2654.819721	251.115322	46.970970
2651.701391	240.538703	46.975975
2648.114181	240.754139	46.980980
2643.942009	240.415469	46.985985
2640.763308	246.291089	46.990989
2637.687874	242.124076	46.995994
2633.803133	244.150621	47.000999
2630.492699	240.471947	47.006004
2627.426580	245.334332	47.011009
2623.892551	246.304135	47.016013
2620.964122	240.587231	47.021018
2616.744581	239.839750	47.026023
2613.681091	238.877781	47.031028
2609.977488	241.813405	47.036033
2606.732324	233.882939	47.041037
2602.778688	241.453442	47.046042
2599.626710	241.297706	47.051047
2596.694669	240.541280	47.056052
2592.842601	246.670806	47.061057
2589.493373	234.756499	47.066061
2585.682797	226.310750	47.071066
2582.067327	227.611779	47.076071
2578.889262	225.108037	47.081076
2575.387245	226.023747	47.086081
2571.854907	235.427326	47.091085
2568.479064	230.257785	47.096090
2565.135845	245.839666	47.101095
2561.771403	228.956475	47.106100
2558.156048	240.083800	47.111105
2554.067227	247.991340	47.116109
2551.413833	227.196299	47.121114
2547.411245	235.704062	47.126119
2544.084197	238.027208	47.131124
2540.564859	243.830776	47.136129
2537.211972	235.981543	47.141133
2533.872506	221.872585	47.146138
2529.989351	237.995554	47.151143
2526.526133	227.065954	47.156148
2523.485448	229.163314	47.161153
2519.648200	230.774227	47.166157
2516.598933	223.175066	47.171162
2512.728238	230.015665	47.176167
2509.572756	224.795513	47.181172
2505.937215	236.083741	47.186177
2502.078958	237.224566	47.191181
2498.938895	225.039638	47.196186
2495.056127	231.984052	47.201191
2491.907404	236.493882	47.206196
2488.492737	229.607809	47.211201
2484.848138	224.760847	47.216205
2481.802859	222.370512	47.221210
2478.091725	223.570158	47.226215
2474.505014	226.730745	47.231220
2471.267480	213.458222	47.236225
2467.289475	225.070787	47.241229
2464.191691	218.844396	47.246234
2460.561960	228.978458	47.251239
2456.959232	226.119974	47.256244
2453.717204	229.959428	47.261249
2450.060243	220.118261	47.266253
2446.648035	218.878330	47.271258
2443.254306	221.625199	47.276263
2439.574134	221.617999	47.281268
2436.244013	213.414445	47.286273
2432.194954	216.405240	47.291277
2429.294167	216.512809	47.296282
2425.646605	214.794335	47.301287
2422.220983	217.315414	47.306292
2418.684905	209.780604	47.311297
2415.070998	215.263284	47.316301
2411.983132	216.723536	47.321306
2408.307468	215.595243	47.326311
2404.819336	210.896953	47.331316
2401.114923	217.622763	47.336321
2397.295982	226.961194	47.341325
2394.309090	211.689012	47.346330
2390.792548	217.606811	47.351335
2387.092036	214.991207	47.356340
2383.752900	216.513923	47.361345
2380.332365	216.482284	47.366349
2377.070031	210.715593	47.371354
2373.129469	211.940496	47.376359
2370.138828	206.578393	47.381364
2366.105061	207.393256	47.386369
2362.459863	217.693671	47.391373
2359.282401	208.182031	47.396378
2355.859457	212.156327	47.401383
2352.385995	212.717388	47.406388
2348.895516	207.426875	47.411393
2345.360588	223.649328	47.416397
2341.979432	214.549149	47.421402
2338.317535	221.463811	47.426407
2334.983621	214.404583	47.431412
2331.370849	222.449170	47.436417
2328.179396	217.894865	47.441421
2324.742843	210.515062	47.446426
2320.744526	223.710553	47.451431
2317.052271	220.603488	47.456436
2313.544805	224.630023	47.461441
2310.237135	213.837689	47.466445
2306.966697	208.764754	47.471450
2303.492239	215.180283	47.476455
2299.986870	205.881596	47.481460
2296.709404	206.890231	47.486465
2292.906540	206.751206	47.491469
2289.524940	210.317468	47.496474
2285.811789	204.824664	47.501479
2282.160050	200.433613	47.506484
2278.909973	211.005904	47.511489
2275.066742	217.105687	47.516493
2272.442373	204.221699	47.521498
2268.462956	218.893369	47.526503
2264.833428	219.681177	47.531508
2261.518369	216.495159	47.536513
2258.137029	223.725955	47.541517
2254.561190	223.252939	47.546522
2250.661451	211.512907	47.551527
2247.181100	209.726496	47.556532
2244.127851	211.062320	47.561537
2240.243010	221.986660	47.566541
2236.846500	203.541705	47.571546
2233.217657	220.418687	47.576551
2229.956979	206.210307	47.581556
2226.507047	199.158538	47.586561
2222.772314	204.326674	47.591565
2219.503762	200.738969	47.596570
2216.287433	203.926087	47.601575
2212.901991	196.395656	47.606580
2209.370149	202.434830	47.611585
2205.339195	208.149563	47.616589
2201.868668	202.365210	47.621594
2198.285039	207.455160	47.626599
2194.839105	202.148108	47.631604
2191.255814	207.336958	47.636609
2187.684691	207.506251	47.641613
2184.659446	199.318259	47.646618
2180.822049	214.789539	47.651623
2177.370000	206.018235	47.656628
2174.478735	200.070674	47.661633
2170.600755	214.918128	47.666637
2167.219449	202.486194	47.671642
2163.288496	211.093584	47.676647
2159.724564	209.645388	47.681652
2156.221267	208.105406	47.686657
2152.964938	197.783885	47.691661
2149.778587	202.552209	47.696666
2146.030877	211.306669	47.701671
2142.314192	195.671597	47.706676
2138.789087	195.096546	47.711681
2135.373549	193.103664	47.716685
2132.266425	192.903829	47.721690
2128.540380	194.498661	47.726695
2125.098625	204.232747	47.731700
2121.406177	200.227344	47.736705
2117.752843	199.348572	47.741709
2114.325943	194.383926	47.746714
2111.059003	202.163377	47.751719
2107.638248	199.751677	47.756724
2104.041219	204.418069	47.761729
2100.561332	192.938708	47.766733
2097.056313	192.746313	47.771738
2093.624828	192.476972	47.776743
2089.869104	192.081264	47.781748
2086.382640	190.575045	47.786753
2082.875381	205.236864	47.791757
2079.787031	183.551790	47.796762
2075.669197	190.389627	47.801767
2072.181286	192.335890	47.806772
2068.983245	181.964559	47.811777
2065.228391	192.106757	47.816781
2061.995320	189.607887	47.821786
2058.307941	181.697699	47.826791
2055.100700	183.057518	47.831796
2051.455283	191.953874	47.836801
2047.948831	194.803360	47.841805
2044.842951	186.191691	47.846810
2041.200026	201.437854	47.851815
2037.416772	190.787875	47.856820
2033.782640	188.039867	47.861825
2030.233709	193.015538	47.866829
2027.096415	195.222253	47.871834
2023.501240	189.700275	47.876839
2019.896422	189.344034	47.881844
2016.438502	191.881760	47.886849
2012.936597	193.339437	47.891853
2009.567830	196.522679	47.896858
2005.722005	198.988352	47.901863
2002.288241	187.337970	47.906868
1999.214220	200.307198	47.911873
1995.695969	201.810693	47.916877
1992.441542	191.117307	47.921882
1988.884689	186.958397	47.926887
1984.936856	192.945330	47.931892
1981.445493	188.821495	47.936897
1977.789091	185.252511	47.941901
1974.556529	187.447634	47.946906
1970.952874	196.153730	47.951911
1967.367138	197.719871	47.956916
1963.849536	188.379601	47.961921
1960.201737	184.401652	47.966925
1956.812010	188.316269	47.971930
1953.210584	192.647914	47.976935
1950.003522	196.390531	47.981940
1946.539771	204.910776	47.986945
1942.827599	204.612436	47.991949
1939.755072	198.595044	47.996954
1936.080036	194.285669	48.001959
1932.568663	193.793101	48.006964
1929.212506	192.902099	48.011969
1924.739676	198.450915	48.016973
1921.806795	184.925041	48.021978
1918.282465	195.341719	48.026983
1914.858113	189.148173	48.031988
1911.764832	188.514619	48.036993
1907.638371	191.808403	48.041997
1904.285134	186.028445	48.047002
1900.900163	195.279879	48.052007
1897.367726	195.399521	48.057012
1893.867229	191.570251	48.062017
1890.381875	212.340960	48.067021
1887.346347	191.083749	48.072026
1883.891597	200.629260	48.077031
1880.073576	187.568399	48.082036
1876.276866	191.226796	48.087041
1872.508217	181.723091	48.092045
1869.442735	193.182860	48.097050
1865.795944	196.569391	48.102055
1862.242631	195.981370	48.107060
1858.696775	192.897955	48.112065
1855.234425	182.739349	48.117069
1852.325684	189.235154	48.122074
1848.509328	182.639769	48.127079
1844.757065	186.152134	48.132084
1841.317689	194.091936	48.137089
1837.769265	195.765734	48.142093
1834.736897	193.052030	48.147098
1830.842434	195.379704	48.152103
1827.477188	194.866037	48.157108
1824.472732	200.688425	48.162113
1820.021112	187.977601	48.167117
1816.859457	185.241138	48.172122
1813.326697	183.556823	48.177127
1809.947258	186.528611	48.182132
1806.377866	186.936358	48.187137
1802.447686	200.194985	48.192141
1799.610674	198.079190	48.197146
1795.870405	196.957134	48.202151
1792.344329	184.484606	48.207156
1789.097968	184.928644	48.212161
1785.265368	191.376924	48.217165
1781.984479	191.606262	48.222170
1778.292316	181.905308	48.227175
1774.484962	196.170899	48.232180
1771.558614	189.465312	48.237185
1767.999170	184.891500	48.242189
1764.734646	179.959148	48.247194
1760.878771	196.624800	48.252199
1757.108940	184.132924	48.257204
1753.789195	178.904147	48.262209
1750.383988	189.940726	48.267213
1746.812552	180.351680	48.272218
1743.009652	184.693279	48.277223
1739.533352	175.154742	48.282228
1736.676504	180.460203	48.287233
1733.048033	185.276178	48.292237
1729.515030	174.471758	48.297242
1725.567830	178.402883	48.302247
1721.915815	178.758698	48.307252
1718.719579	189.679218	48.312257
1715.199781	190.194946	48.317261
1712.128965	181.768273	48.322266
1708.450931	185.914564	48.327271
1704.541842	188.645560	48.332276
1701.332558	174.747217	48.337281
1697.833779	189.393343	48.342285
1694.445606	177.355010	48.347290
1690.643178	185.160417	48.352295
1687.279355	181.086234	48.357300
1683.924761	177.365106	48.362305
1680.399007	182.955092	48.367309
1676.812350	189.859876	48.372314
1673.165424	183.691055	48.377319
1669.776339	192.408726	48.382324
1666.109129	176.164715	48.387329
1662.541270	191.703460	48.392333
1659.320037	175.256622	48.397338
1655.766280	186.847239	48.402343
1652.251260	191.492896	48.407348
1648.809899	181.886588	48.412353
1645.073616	186.014994	48.417357
1641.936175	179.100722	48.422362
1637.953789	183.374812	48.427367
1634.659619	192.777598	48.432372
1631.412543	194.214811	48.437377
1627.611338	186.838059	48.442381
1624.452043	172.888105	48.447386
1620.904753	184.094679	48.452391
1617.447456	175.425406	48.457396
1614.092251	180.008103	48.462401
1610.045402	181.407020	48.467405
1606.601088	163.760173	48.472410
1603.411929	165.308794	48.477415
1599.693540	176.815899	48.482420
1596.065314	165.210102	48.487425
1592.217844	171.742706	48.492429
1589.413010	162.755055	48.497434
1585.553330	170.798835	48.502439
1582.417742	170.789312	48.507444
1579.041183	172.142747	48.512449
1575.213818	175.303688	48.517453
1571.433802	177.439464	48.522458
1568.038913	174.158743	48.527463
1564.542758	171.172160	48.532468
1561.066924	172.151402	48.537473
1557.499193	176.284096	48.542477
1554.217937	165.157861	48.547482
1550.933734	179.087586	48.552487
1547.152478	178.979917	48.557492
1543.795797	168.031482	48.562497
1540.363367	181.032941	48.567501
1536.677800	182.905717	48.572506
1533.146696	180.995840	48.577511
1529.494073	175.220110	48.582516
1526.290607	174.256255	48.587521
1522.316471	184.095381	48.592525
1519.207010	173.437745	48.597530
1515.629980	177.259645	48.602535
1511.792770	170.078928	48.607540
1508.680668	167.158432	48.612545
1504.850243	172.671012	48.617549
1501.768413	164.816614	48.622554
1498.487623	170.058833	48.627559
1494.610584	169.862522	48.632564
1491.210875	172.576649	48.637569
1487.455195	168.434254	48.642573
1484.270425	173.805165	48.647578
1480.633395	172.770326	48.652583
1477.277667	169.039530	48.657588
1473.958845	166.700122	48.662593
1469.529029	181.787361	48.667597
1466.604294	164.000598	48.672602
1463.131711	173.166604	48.677607
1459.587143	168.004095	48.682612
1456.212842	167.147197	48.687617
1452.369738	166.591525	48.692621
1449.008014	168.580192	48.697626
1445.550109	176.273795	48.702631
1442.091623	168.400593	48.707636
1438.858717	169.770143	48.712641
1435.114508	170.820080	48.717645
1431.574994	169.216299	48.722650
1428.225127	170.387618	48.727655
1424.375688	172.799624	48.732660
1421.107617	170.260965	48.737665
1417.268872	175.020629	48.742669
1413.772674	169.218362	48.747674
1410.476891	170.729022	48.752679
1407.074190	167.090761	48.757684
1403.754187	161.951896	48.762689
1399.631315	167.249083	48.767693
1396.531908	165.916797	48.772698
1392.722914	167.211661	48.777703
1389.640822	177.256607	48.782708
1386.218610	163.148644	48.787713
1382.622854	165.200731	48.792717
1379.372697	167.692417	48.797722
1375.934347	159.706721	48.802727
1371.878972	167.883332	48.807732
1368.323376	160.445596	48.812737
1364.885722	160.727046	48.817741
1361.534951	158.439634	48.822746
1358.046205	155.228187	48.827751
1354.404392	155.181269	48.832756
1351.118312	158.765996	48.837761
1347.272750	158.657507	48.842765
1344.111824	156.698077	48.847770
1340.423986	168.687407	48.852775
1336.862334	169.301093	48.857780
1333.623647	154.086434	48.862785
1330.092316	164.849180	48.867789
1326.295368	161.630018	48.872794
1322.688191	171.277839	48.877799
1319.383473	162.732042	48.882804
1316.079775	165.581839	48.887809
1312.296627	170.010460	48.892813
1309.171676	176.633884	48.897818
1305.567050	174.437431	48.902823
1302.043794	165.630067	48.907828
1298.326424	163.812525	48.912833
1294.656931	164.549004	48.917837
1291.291486	157.624711	48.922842
1287.858069	162.757640	48.927847
1284.511702	170.470583	48.932852
1281.373872	157.381443	48.937857
1277.408810	166.303835	48.942861
1274.042761	166.253862	48.947866
1270.471822	172.863210	48.952871
1266.786457	167.390098	48.957876
1263.178950	167.506267	48.962881
1259.929983	163.511715	48.967885
1256.948862	164.376591	48.972890
1252.907906	152.689984	48.977895
1249.255303	167.477062	48.982900
1246.034797	157.826364	48.987905
1242.415347	167.858143	48.992909
1238.683289	160.999131	48.997914
1235.392706	169.388845	49.002919
1232.059932	173.106432	49.007924
1228.549272	162.538674	49.012929
1225.059755	175.732671	49.017933
1221.434400	161.665255	49.022938
1217.676619	167.016911	49.027943
1214.145612	164.286463	49.032948
1211.058567	163.462476	49.037953
1207.349970	166.199309	49.042957
1203.914310	153.468869	49.047962
1200.411133	156.170117	49.052967
1196.582030	162.440705	49.057972
1193.257706	156.719211	49.062977
1189.491665	156.408361	49.067981
1186.559474	148.011391	49.072986
1183.348089	161.591101	49.077991
1179.757071	158.100662	49.082996
1176.015877	142.723808	49.088001
1171.968543	147.709712	49.093005
1168.688840	155.309185	49.098010
1165.181744	161.967921	49.103015
1161.642547	140.207104	49.108020
1158.649188	148.354798	49.113025
1154.847903	147.388886	49.118029
1151.368309	137.503505	49.123034
1147.930078	150.393369	49.128039
1144.335602	157.417756	49.133044
1140.952592	157.107136	49.138049
1137.122614	161.061932	49.143053
1133.461186	157.904073	49.148058
1130.138305	156.311059	49.153063
1126.487352	172.632223	49.158068
1123.645106	158.195860	49.163073
1119.726835	161.614342	49.168077
1116.463492	157.138427	49.173082
1112.839810	158.393870	49.178087
1109.262109	154.567419	49.183092
1105.895182	151.929418	49.188097
1101.768135	161.318446	49.193101
1098.399459	155.455652	49.198106
1095.159698	151.617914	49.203111
1091.984522	151.043532	49.208116
1088.840308	156.241566	49.213121
1084.823674	164.759391	49.218125
1081.407072	162.255586	49.223130
1077.585047	153.735256	49.228135
1074.028595	166.594857	49.233140
1070.995163	162.051607	49.238145
1066.933396	163.252823	49.243149
1063.744786	157.679178	49.248154
1060.146261	152.942732	49.253159
1056.536392	155.889167	49.258164
1053.446830	154.284900	49.263169
1049.513771	153.804784	49.268173
1046.058890	152.636322	49.273178
1042.848005	158.145890	49.278183
1039.252996	152.587364	49.283188
1035.769560	153.792266	49.288193
1032.243396	150.429028	49.293197
1028.965622	154.115621	49.298202
1025.167709	156.659917	49.303207
1021.388644	150.968315	49.308212
1018.370416	158.283366	49.313217
1014.370930	155.784971	49.318221
1011.458400	167.433922	49.323226
1007.550323	158.753713	49.328231
1004.294507	157.125322	49.333236
1000.683997	148.214959	49.338241
997.050125	163.436084	49.343245
993.702279	158.261687	49.348250
989.892909	153.367912	49.353255
986.860418	154.115400	49.358260
983.690322	152.689910	49.363265
979.786058	151.041822	49.368269
976.257561	151.175780	49.373274
972.662826	150.500842	49.378279
968.761422	157.234239	49.383284
965.829859	159.298315	49.388289
961.919133	158.276194	49.393293
958.706271	151.993620	49.398298
955.350339	160.675401	49.403303
951.530520	154.787437	49.408308
948.007679	147.545613	49.413313
944.743654	157.967910	49.418317
941.224291	146.787250	49.423322
937.135355	150.496434	49.428327
933.682711	165.834956	49.433332
930.765631	145.891932	49.438337
927.054820	149.173067	49.443341
924.099818	142.000678	49.448346
920.425979	156.445586	49.453351
916.639021	157.048941	49.458356
913.362848	144.639138	49.463361
909.548578	155.460406	49.468365
906.127781	146.765420	49.473370
902.207049	141.005243	49.478375
898.559176	144.202106	49.483380
895.475397	155.885970	49.488385
892.044609	155.064630	49.493389
888.730463	149.482607	49.498394
885.259157	155.315524	49.503399
881.864663	160.355291	49.508404
878.321360	158.721356	49.513409
874.184038	158.078350	49.518413
870.920029	146.401159	49.523418
867.418463	158.585939	49.528423
864.076231	162.486187	49.533428
860.765319	156.663513	49.538433
857.347001	164.738147	49.543437
853.556456	158.458775	49.548442
850.160108	152.358489	49.553447
846.336502	161.822538	49.558452
843.017395	139.149256	49.563457
839.472520	155.201319	49.568461
836.310999	153.527055	49.573466
832.736317	144.815597	49.578471
828.698566	145.477777	49.583476
825.309742	147.295800	49.588481
821.713712	153.822966	49.593485
818.535116	145.052819	49.598490
815.014600	143.690803	49.603495
811.170982	160.001265	49.608500
808.072824	133.555615	49.613505
804.695107	143.815005	49.618509
801.294079	138.744511	49.623514
797.417572	145.156008	49.628519
794.073974	144.858886	49.633524
790.849544	147.879330	49.638529
787.160756	152.766576	49.643533
783.379422	143.202356	49.648538
780.054256	150.607444	49.653543
776.456602	164.549908	49.658548
773.145382	138.542076	49.663553
769.332756	148.846864	49.668557
765.827373	146.091718	49.673562
762.678393	138.033552	49.678567
758.491125	151.177385	49.683572
755.662248	146.475718	49.688577
751.999267	148.778367	49.693581
748.481301	141.937984	49.698586
744.827999	144.531652	49.703591
741.204402	146.726384	49.708596
738.222781	148.397389	49.713601
734.681923	150.426037	49.718605
730.800007	144.265724	49.723610
727.188986	146.418331	49.728615
723.893597	147.960027	49.733620
720.699362	140.670884	49.738625
716.642140	148.262402	49.743629
713.343753	142.332383	49.748634
709.786924	155.257687	49.753639
706.225594	159.914775	49.758644
702.926991	145.816459	49.763649
699.491623	151.035113	49.768653
695.807303	150.049654	49.773658
692.367276	147.344725	49.778663
688.813835	151.635587	49.783668
685.613911	142.439886	49.788673
682.270395	148.200685	49.793677
678.264108	160.627339	49.798682
674.642215	147.495890	49.803687
670.945420	151.504801	49.808692
667.794314	153.474639	49.813697
664.195111	152.050524	49.818701
660.993600	153.638998	49.823706
657.451470	150.736571	49.828711
653.685433	152.249877	49.833716
650.329365	141.025177	49.838721
646.616117	146.608012	49.843725
642.928038	145.686837	49.848730
640.121299	143.609175	49.853735
636.596004	151.202267	49.858740
633.387490	143.392850	49.863745
629.269672	149.012028	49.868749
626.072080	145.174085	49.873754
622.095130	142.331656	49.878759
618.420635	145.461337	49.883764
615.551925	143.695809	49.888769
612.061066	151.534797	49.893773
608.159908	146.769581	49.898778
604.656162	141.902326	49.903783
600.951334	155.420969	49.908788
597.864102	140.122688	49.913793
594.299401	147.823033	49.918797
591.108098	153.199429	49.923802
587.567177	147.307466	49.928807
583.679195	150.450624	49.933812
580.365397	155.617587	49.938817
576.479836	149.426306	49.943821
573.397530	150.201247	49.948826
569.774661	146.726190	49.953831
566.227600	149.212036	49.958836
562.633799	130.223866	49.963841
559.093711	144.750996	49.968845
555.566657	145.076825	49.973850
552.194880	148.118657	49.978855
548.192029	150.847314	49.983860
545.295269	136.468160	49.988865
541.881586	143.846629	49.993869
538.774502	153.223842	49.998874
535.063520	139.711700	50.003879
531.173476	142.842007	50.008884
527.763507	141.506384	50.013889
524.242555	149.556769	50.018893
520.810653	145.222573	50.023898
517.033877	141.211716	50.028903
513.407779	135.021923	50.033908
510.191674	131.688373	50.038913
506.168603	141.302032	50.043917
503.061348	133.067041	50.048922
499.800152	132.508635	50.053927
496.604086	136.599678	50.058932
493.119899	147.132597	50.063937
489.303019	143.776649	50.068941
485.716970	138.846602	50.073946
482.476394	135.355905	50.078951
478.618806	141.311612	50.083956
475.121167	139.548619	50.088961
471.326911	136.082793	50.093965
468.169301	149.509220	50.098970
464.776906	145.195562	50.103975
461.333138	153.316000	50.108980
457.790325	142.252001	50.113985
453.750599	149.264719	50.118989
450.378619	138.421811	50.123994
447.301456	138.227852	50.128999
443.474409	137.782875	50.134004
440.274420	142.078612	50.139009
436.580809	147.374774	50.144013
433.488277	136.341876	50.149018
429.746219	136.992943	50.154023
426.096198	136.976200	50.159028
422.565238	131.116241	50.164033
418.986792	142.050108	50.169037
415.259293	138.059490	50.174042
412.067824	139.197242	50.179047
408.417352	150.664217	50.184052
405.269819	138.776097	50.189057
401.608010	136.337146	50.194061
398.212728	138.422619	50.199066
394.505795	142.297300	50.204071
391.167659	141.383279	50.209076
388.085068	133.798070	50.214081
384.227852	138.934034	50.219085
380.880453	138.628380	50.224090
377.144456	135.053939	50.229095
373.170521	144.948218	50.234100
369.929033	147.385955	50.239105
366.455823	146.190400	50.244109
362.965912	145.816449	50.249114
359.498394	138.448550	50.254119
355.702412	144.406280	50.259124
352.397066	132.975492	50.264129
348.950872	137.058398	50.269133
345.406890	137.411308	50.274138
342.636422	134.297529	50.279143
338.606556	132.772989	50.284148
335.355448	122.694314	50.289153
331.618675	134.917655	50.294157
328.019851	137.814591	50.299162
324.469025	125.895489	50.304167
320.627402	133.555381	50.309172
317.379551	139.183039	50.314177
314.128062	128.706655	50.319181
310.448124	131.514991	50.324186
306.968064	130.424191	50.329191
303.279436	149.829032	50.334196
300.137367	138.069708	50.339201
296.254214	143.731401	50.344205
292.933343	137.803465	50.349210
289.617365	133.179247	50.354215
286.220336	141.329623	50.359220
282.511889	132.395367	50.364225
279.105971	141.142799	50.369229
275.197661	140.331326	50.374234
272.055818	140.837444	50.379239
268.216607	146.016374	50.384244
265.148734	131.037524	50.389249
261.694771	139.703716	50.394253
257.801129	137.388194	50.399258
254.352808	137.096222	50.404263
250.515173	143.373036	50.409268
247.472111	140.122219	50.414273
243.960279	138.405899	50.419277
240.589144	156.589246	50.424282
237.232938	141.404892	50.429287
233.279729	150.742957	50.434292
229.927186	142.356166	50.439297
226.371060	157.890204	50.444301
222.871914	142.407759	50.449306
219.404174	149.014054	50.454311
215.764153	145.538293	50.459316
212.638529	134.005980	50.464321
208.690403	152.472408	50.469325
205.642650	139.294774	50.474330
202.104860	139.629967	50.479335
198.391490	158.843411	50.484340
195.095026	143.439174	50.489345
191.565664	152.718478	50.494349
187.792615	139.242098	50.499354
184.418453	148.085351	50.504359
180.731075	153.712001	50.509364
177.604453	135.753251	50.514369
173.698042	147.132489	50.519373
170.147563	140.601794	50.524378
166.902425	148.440733	50.529383
163.285321	143.872159	50.534388
159.870395	142.499868	50.539393
155.880967	136.752821	50.544397
152.894753	138.330133	50.549402
149.962145	134.679123	50.554407
146.182356	142.410185	50.559412
142.543744	122.628767	50.564417
138.939408	139.062828	50.569421
134.858561	127.792980	50.574426
131.350160	133.708239	50.579431
128.432639	140.301299	50.584436
125.062560	132.333605	50.589441
121.176240	130.438023	50.594445
117.616106	146.927246	50.599450
114.446702	136.272664	50.604455
110.764294	137.981509	50.609460
107.239979	137.524003	50.614465
103.661010	139.953013	50.619469
100.535076	129.203950	50.624474
97.182018	130.740488	50.629479
93.453501	141.350845	50.634484
89.670274	143.155682	50.639489
86.134362	151.380304	50.644493
82.573153	137.788397	50.649498
79.104624	139.472869	50.654503
75.662636	145.370477	50.659508
72.511346	131.435597	50.664513
69.223770	135.034867	50.669517
65.240279	145.257927	50.674522
61.589774	136.619483	50.679527
58.012291	139.556446	50.684532
54.803957	130.314374	50.689537
51.216227	132.104684	50.694541
47.957822	128.798993	50.699546
44.247394	136.938914	50.704551
40.480491	140.884468	50.709556
37.397238	135.161785	50.714561
33.766355	127.044279	50.719565
30.300015	140.977854	50.724570
27.071299	130.601375	50.729575
23.242446	137.529857	50.734580
19.867143	129.234176	50.739585
16.144115	135.741772	50.744589
12.641735	131.218266	50.749594
9.185842	134.770402	50.754599
5.472822	131.258003	50.759604
2.375299	127.108984	50.764609