Thu Jun 16 18:47:16 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
-0.136448	108.404068	0.000000
0.056228	105.007243	0.005005
-0.152384	107.700523	0.010010
0.003384	92.035122	0.015014
0.132306	95.377609	0.020019
-0.087346	89.307400	0.025024
-0.194991	89.103657	0.030029
-0.412010	80.318817	0.035034
-0.563338	76.518227	0.040038
-0.772822	67.470912	0.045043
-1.255426	62.785383	0.050048
-1.321042	54.026543	0.055053
-1.368600	48.497840	0.060058
-1.589453	40.745586	0.065062
-2.111193	26.852576	0.070067
-2.719382	14.576311	0.075072
-2.556565	15.312644	0.080077
-3.466302	5.869760	0.085082
-3.577021	-5.924296	0.090086
-3.723779	-6.448219	0.095091
-3.809897	1.520079	0.100096
-4.474783	-3.225278	0.105101
-5.314886	8.977475	0.110106
-5.368816	-4.737596	0.115110
-5.551267	5.805328	0.120115
-5.749984	3.077071	0.125120
-5.176076	4.828989	0.130125
-5.714802	11.592146	0.135130
-5.564026	8.580409	0.140134
-6.465361	2.683364	0.145139
-6.809956	17.058099	0.150144
-6.780832	5.276046	0.155149
-7.258879	18.246784	0.160154
-6.956383	2.980553	0.165158
-7.321867	10.453115	0.170163
-8.392081	6.181196	0.175168
-8.609963	6.049734	0.180173
-8.890952	4.989904	0.185178
-8.605205	3.307727	0.190182
-8.996753	6.943578	0.195187
-9.076387	12.418994	0.200192
-8.622880	10.820375	0.205197
-9.415469	10.009844	0.210202
-9.900171	11.408215	0.215206
-10.231646	5.915102	0.220211
-10.621442	7.539591	0.225216
-10.451330	10.592113	0.230221
-11.161804	14.420959	0.235226
-11.443668	6.090825	0.240230
-11.759071	-1.125772	0.245235
-12.204886	4.450702	0.250240
-12.073379	6.411282	0.255245
-12.281571	9.447991	0.260250
-12.028087	10.120209	0.265254
-12.146047	5.802698	0.270259
-12.574723	10.264998	0.275264
-13.478424	2.274698	0.280269
-13.809540	8.993876	0.285274
-13.682352	7.938018	0.290278
-13.802081	14.266713	0.295283
-13.843070	1.021858	0.300288
-14.070619	0.254291	0.305293
-14.941989	12.748806	0.310298
-14.953237	9.561998	0.315302
-15.226824	4.950960	0.320307
-15.279268	10.654804	0.325312
-14.995985	4.723587	0.330317
-16.052710	8.127429	0.335322
-16.306108	-4.449745	0.340326
-16.837318	10.096898	0.345331
-16.872076	10.989199	0.350336
-16.524032	1.557868	0.355341
-17.095935	2.887582	0.360346
-17.700827	7.366474	0.365350
-18.062385	8.926118	0.370355
-18.403515	11.714680	0.375360
-18.450960	11.438541	0.380365
-18.602804	9.402097	0.385370
-18.587280	18.540322	0.390374
-18.561151	9.062841	0.395379
-18.849348	13.853828	0.400384
-19.233836	7.465307	0.405389
-19.696105	8.372026	0.410394
-19.907491	6.384982	0.415398
-19.941551	7.177724	0.420403
-20.341915	6.368475	0.425408
-21.068646	3.669963	0.430413
-21.457627	3.778984	0.435418
-21.606423	-3.510625	0.440422
-21.620314	2.087993	0.445427
-21.896317	5.614974	0.450432
-21.562506	-1.700526	0.455437
-21.671107	9.122310	0.460442
-21.836543	-6.406838	0.465446
-22.988382	4.813531	0.470451
-23.111713	2.591443	0.475456
-23.125936	-6.918425	0.480461
-23.384998	2.804315	0.485466
-23.401754	7.644360	0.490470
-23.979049	7.621229	0.495475
-24.101018	-0.486419	0.500480
-24.171995	1.442511	0.505485
-24.312326	3.952731	0.510490
-24.882959	-5.842440	0.515494
-25.838083	-6.544026	0.520499
-25.861223	1.280088	0.525504
-26.115020	0.164367	0.530509
-26.598681	3.564266	0.535514
-26.118944	6.434210	0.540518
-26.100262	10.787360	0.545523
-26.113587	8.837827	0.550528
-26.125512	11.457446	0.555533
-27.344904	14.841905	0.560538
-27.499174	3.430226	0.565542
-27.691485	7.601500	0.570547
-27.752051	7.776803	0.575552
-28.201488	7.754344	0.580557
-29.012298	9.207201	0.585562
-29.081529	2.438853	0.590566
-29.327918	1.894104	0.595571
-29.521581	10.985899	0.600576
-29.158045	8.628597	0.605581
-29.655991	4.056612	0.610586
-29.298467	-7.352527	0.615590
-30.039038	4.606671	0.620595
-30.768801	15.487278	0.625600
-30.680669	6.682835	0.630605
-30.971930	15.191632	0.635610
-31.049986	10.327392	0.640614
-31.502204	14.215370	0.645619
-32.317428	8.998724	0.650624
-32.278441	6.478117	0.655629
-32.766611	12.915055	0.660634
-32.749662	3.962064	0.665638
-32.817922	-0.449784	0.670643
-33.095305	1.373267	0.675648
-33.011730	-1.165955	0.680653
-32.969895	7.929439	0.685658
-32.920889	5.201974	0.690662
-34.135873	8.036692	0.695667
-34.299255	6.937006	0.700672
-34.037286	3.304411	0.705677
-34.747860	11.896808	0.710682
-35.368209	2.618907	0.715686
-35.693664	10.383184	0.720691
-35.731920	14.351915	0.725696
-35.659123	7.116247	0.730701
-36.069820	17.878717	0.735706
-35.787575	9.643493	0.740710
-35.796339	1.421640	0.745715
-36.534479	0.183229	0.750720
-37.149534	-0.221077	0.755725
-37.529156	3.605969	0.760730
-37.388789	2.622811	0.765734
-37.579066	18.067401	0.770739
-37.831539	10.193326	0.775744
-38.551100	7.897720	0.780749
-39.068771	4.903127	0.785754
-38.867116	-6.751256	0.790758
-38.972981	-0.056877	0.795763
-39.622175	8.590190	0.800768
-38.996821	-1.838687	0.805773
-39.075632	2.730051	0.810778
-40.239812	6.387538	0.815782
-40.733730	3.409737	0.820787
-41.072222	5.138116	0.825792
-40.663185	5.160833	0.830797
-40.681784	9.292152	0.835802
-40.838100	0.043719	0.840806
-41.297429	-8.509926	0.845811
-41.737186	5.210362	0.850816
-42.094259	-3.131800	0.855821
-42.384673	3.484757	0.860826
-42.134539	-4.216463	0.865830
-42.535084	-0.845888	0.870835
-43.254316	-2.653404	0.875840
-43.413642	0.307649	0.880845
-44.009468	-1.796494	0.885850
-43.719212	-4.349747	0.890854
-44.127888	8.478503	0.895859
-44.270161	6.947761	0.900864
-43.989448	4.518021	0.905869
-44.773543	7.339933	0.910874
-45.088306	-1.387068	0.915878
-45.432536	4.908285	0.920883
-45.888862	2.335958	0.925888
-45.633301	7.748772	0.930893
-45.867284	7.875883	0.935898
-46.049980	6.111992	0.940902
-46.913310	1.899613	0.945907
-47.424120	11.802671	0.950912
-47.035811	-6.487480	0.955917
-47.184637	2.552504	0.960922
-47.356545	-2.175665	0.965926
-47.380299	1.484837	0.970931
-47.760534	6.274754	0.975936
-48.125624	5.958573	0.980941
-48.778039	-3.714263	0.985946
-48.939248	8.479090	0.990950
-48.938472	-1.135168	0.995955
-49.257706	5.526403	1.000960
-49.182364	-10.989413	1.005965
-49.676165	9.149880	1.010970
-50.177259	-7.441643	1.015974
-50.329915	2.626065	1.020979
-50.264682	10.027935	1.025984
-50.330247	6.320528	1.030989
-51.538568	0.845958	1.035994
-51.607679	3.468022	1.040998
-51.692167	1.994519	1.046003
-51.953681	0.844954	1.051008
-51.929613	11.047425	1.056013
-52.191484	10.440320	1.061018
-52.033778	11.200581	1.066022
-52.366922	8.046749	1.071027
-53.134047	14.522192	1.076032
-53.263971	-2.203781	1.081037
-53.416289	0.986077	1.086042
-53.459912	-1.880274	1.091046
-54.427549	-2.168398	1.096051
-54.837635	8.695282	1.101056
-55.035990	-8.507319	1.106061
-55.131316	-0.565916	1.111066
-54.985156	-0.154367	1.116070
-55.077056	2.596557	1.121075
-55.186418	9.827013	1.126080
-55.184482	1.959339	1.131085
-56.221434	2.547870	1.136090
-56.263113	5.656502	1.141094
-56.505664	0.313750	1.146099
-56.889379	6.265898	1.151104
-56.606055	-1.108737	1.156109
-56.900684	0.784446	1.161114
-57.944244	0.890466	1.166118
-57.824422	-4.665384	1.171123
-58.625439	1.917764	1.176128
-58.337715	-4.482595	1.181133
-58.540582	19.877901	1.186138
-58.751376	14.202066	1.191142
-58.718938	5.032042	1.196147
-59.042283	7.756993	1.201152
-59.242514	-6.595368	1.206157
-59.886620	4.337173	1.211162
-59.854642	6.056712	1.216166
-60.216733	-4.496944	1.221171
-61.116837	9.852384	1.226176
-61.449442	-1.098693	1.231181
-61.647509	13.766201	1.236186
-61.590302	-2.673127	1.241190
-61.668976	-0.208121	1.246195
-61.497913	4.189690	1.251200
-61.579384	-3.758412	1.256205
-61.750123	8.559439	1.261210
-62.241338	14.324254	1.266214
-62.469718	6.316768	1.271219
-62.971257	11.163729	1.276224
-63.233536	-1.221667	1.281229
-64.183527	6.878153	1.286234
-64.005972	2.071907	1.291238
-64.707246	2.182228	1.296243
-64.562520	-4.483949	1.301248
-64.360102	-8.420322	1.306253
-64.725609	3.735956	1.311258
-64.554670	-2.831263	1.316262
-64.731491	0.232125	1.321267
-65.586547	4.971375	1.326272
-65.829248	0.195123	1.331277
-66.278696	14.041519	1.336282
-66.621224	2.854717	1.341286
-66.490850	4.554146	1.346291
-66.828539	4.827042	1.351296
-66.754444	-3.758131	1.356301
-67.675776	8.408226	1.361306
-68.197104	4.722870	1.366310
-68.278402	4.479753	1.371315
-68.580542	12.051844	1.376320
-68.214277	2.881207	1.381325
-68.188649	4.664539	1.386330
-68.280765	-10.083334	1.391334
-68.396642	3.845449	1.396339
-69.397618	8.338405	1.401344
-69.633584	8.335127	1.406349
-69.966615	7.612322	1.411354
-69.558421	-2.343329	1.416358
-70.532408	3.947385	1.421363
-71.320889	9.145427	1.426368
-71.236290	-8.031325	1.431373
-71.261370	-0.126788	1.436378
-71.529065	5.587272	1.441382
-71.185104	0.897954	1.446387
-71.729520	-3.461241	1.451392
-71.495376	-6.748975	1.456397
-72.133009	5.911711	1.461402
-72.664214	-2.852913	1.466406
-73.047226	7.506311	1.471411
-73.230195	7.794282	1.476416
-73.125808	0.446753	1.481421
-73.143940	5.149992	1.486426
-74.175864	3.068697	1.491430
-74.635413	9.322240	1.496435
-74.630842	9.883369	1.501440
-74.556284	11.421153	1.506445
-74.510745	5.968044	1.511450
-74.785626	9.200060	1.516454
-74.702107	2.575960	1.521459
-75.475116	6.337798	1.526464
-75.746259	-0.230843	1.531469
-75.981534	3.193020	1.536474
-76.026212	8.941353	1.541478
-76.726790	-4.029035	1.546483
-77.334210	6.838844	1.551488
-77.204502	7.303623	1.556493
-77.345190	11.377281	1.561498
-77.755633	-2.614088	1.566502
-77.753606	-0.108455	1.571507
-77.911266	8.978175	1.576512
-78.228842	5.247011	1.581517
-78.889266	15.216429	1.586522
-78.917896	5.568357	1.591526
-78.951769	3.228196	1.596531
-79.314246	10.522582	1.601536
-79.024301	7.391361	1.606541
-79.631284	4.868699	1.611546
-80.499084	5.145646	1.616550
-80.909195	-1.056315	1.621555
-81.234782	1.627966	1.626560
-80.934669	3.151162	1.631565
-81.212356	17.020671	1.636570
-81.177844	19.353719	1.641574
-80.857484	10.263867	1.646579
-81.806240	10.913100	1.651584
-82.247966	10.258574	1.656589
-82.141739	13.491731	1.661594
-82.699392	6.629390	1.666598
-82.451568	5.841763	1.671603
-83.359329	14.138528	1.676608
-83.854355	4.435539	1.681613
-84.128552	4.744310	1.686618
-84.151362	13.988601	1.691622
-83.756158	-8.505266	1.696627
-84.146287	8.215087	1.701632
-84.257876	-3.447112	1.706637
-84.345911	5.892895	1.711642
-85.176489	8.094163	1.716646
-85.526118	5.176969	1.721651
-85.797867	-2.677235	1.726656
-85.503226	0.753954	1.731661
-85.918195	12.123355	1.736666
-86.363476	6.042926	1.741670
-86.574063	-4.031344	1.746675
-87.418543	-9.413711	1.751680
-86.765789	2.385253	1.756685
-86.990427	7.551176	1.761690
-87.646581	8.554660	1.766694
-88.166308	5.086180	1.771699
-88.610343	-7.331616	1.776704
-88.633958	4.406883	1.781709
-88.749821	6.869652	1.786714
-88.579377	-1.532952	1.791718
-89.054973	4.891349	1.796723
-88.946721	2.819914	1.801728
-89.327776	-3.106965	1.806733
-89.807670	7.603202	1.811738
-90.327030	2.951696	1.816742
-90.258997	0.352596	1.821747
-90.372765	8.240816	1.826752
-90.676759	3.393995	1.831757
-91.593162	-2.535069	1.836762
-91.983255	-1.764876	1.841766
-91.995023	4.444552	1.846771
-92.400922	4.006671	1.851776
-92.374938	4.289014	1.856781
-92.115722	4.689080	1.861786
-92.073455	-0.591827	1.866790
-91.819178	4.425984	1.871795
-92.810408	0.735819	1.876800
-93.144588	-0.724038	1.881805
-93.488889	8.376468	1.886810
-94.412839	3.077670	1.891814
-94.575034	-4.507060	1.896819
-95.079488	3.946990	1.901824
-94.439328	-0.567729	1.906829
-94.852005	9.272936	1.911834
-95.159964	13.313666	1.916838
-95.364384	-0.037349	1.921843
-95.565451	12.105666	1.926848
-95.411505	2.895538	1.931853
-96.019381	8.504422	1.936858
-96.428350	7.319839	1.941862
-96.769037	10.317082	1.946867
-97.037212	9.176512	1.951872
-96.740076	7.841686	1.956877
-97.550502	3.487094	1.961882
-98.083244	-3.143474	1.966886
-98.155531	8.779466	1.971891
-98.463308	3.316877	1.976896
-98.333165	4.054759	1.981901
-98.759510	3.091469	1.986906
-98.749790	1.265098	1.991910
-98.284586	4.181632	1.996915
-99.509243	10.241698	2.006912
-99.180042	4.420413	2.016909
-98.958075	7.066066	2.026906
-98.072987	1.114978	2.036902
-97.576521	4.294316	2.046899
-97.378481	15.454879	2.056896
-96.445241	16.913380	2.066893
-96.073287	15.519842	2.076890
-95.594028	10.021216	2.086886
-95.145490	0.372309	2.096883
-94.337801	3.945119	2.106880
-94.269775	-0.266731	2.116877
-94.181900	2.118867	2.126874
-93.039241	8.684198	2.136870
-92.696867	5.884219	2.146867
-91.725564	4.238861	2.156864
-91.452544	5.121533	2.166861
-91.576423	5.325043	2.176858
-90.421789	12.589296	2.186854
-89.668130	7.497787	2.196851
-89.435712	11.866723	2.206848
-89.647055	8.745501	2.216845
-88.904864	0.946480	2.226842
-88.482929	3.250641	2.236838
-87.776736	6.632985	2.246835
-87.122705	8.694954	2.256832
-86.307340	7.073987	2.266829
-85.499685	5.022770	2.276826
-85.512247	3.654900	2.286822
-85.301180	0.841901	2.296819
-85.001629	3.952732	2.306816
-84.315285	11.921492	2.316813
-83.456064	9.245903	2.326810
-82.418749	3.971790	2.336806
-82.457705	7.517194	2.346803
-82.254617	4.041509	2.356800
-82.049544	0.748093	2.366797
-80.945014	6.856298	2.376794
-80.582081	6.108550	2.386790
-80.199106	7.522765	2.396787
-79.293474	7.907788	2.406784
-79.112843	13.589932	2.416781
-78.875895	-1.319301	2.426778
-77.660063	2.649143	2.436774
-77.137232	-1.497752	2.446771
-77.221235	6.198159	2.456768
-77.004817	2.946826	2.466765
-76.382583	2.542901	2.476762
-75.677476	-0.961323	2.486758
-74.909013	-1.273496	2.496755
-74.795387	0.380079	2.506752
-73.833226	-3.836953	2.516749
-73.462569	-0.955933	2.526746
-73.136150	-1.526508	2.536742
-72.799779	8.020179	2.546739
-72.112587	-0.208782	2.556736
-71.893311	-2.040861	2.566733
-70.840610	0.417861	2.576730
-70.231859	-5.672372	2.586726
-70.044806	1.776735	2.596723
-69.779466	6.057156	2.606720
-68.862585	7.025399	2.616717
-68.490836	5.398231	2.626714
-68.307341	6.121845	2.636710
-67.310835	1.590544	2.646707
-66.954469	-4.152350	2.656704
-66.772881	-0.216713	2.666701
-65.881604	0.979550	2.676698
-65.324350	3.097620	2.686694
-65.265675	5.098749	2.696691
-64.601510	0.870413	2.706688
-63.808951	-4.617506	2.716685
-63.732947	-4.313084	2.726682
-63.056762	4.191264	2.736678
-62.244667	7.705121	2.746675
-62.689019	12.170843	2.756672
-61.290158	4.995064	2.766669
-61.101659	-1.211770	2.776666
-60.641162	-2.688097	2.786662
-59.389137	5.331099	2.796659
-59.528466	6.581373	2.806656
-59.150904	6.384283	2.816653
-58.786114	4.490371	2.826650
-57.883380	-1.399521	2.836646
-57.414725	6.465344	2.846643
-57.350357	9.095163	2.856640
-56.367029	7.406730	2.866637
-56.102217	7.737785	2.876634
-55.683241	5.404135	2.886630
-54.957355	4.359578	2.896627
-54.636160	4.423101	2.906624
-53.848258	4.787874	2.916621
-52.994127	1.771695	2.926618
-53.109205	8.372821	2.936614
-52.860199	7.143232	2.946611
-51.960318	-4.901615	2.956608
-51.484038	3.557193	2.966605
-51.450728	0.301844	2.976602
-50.410822	-0.620854	2.986598
-49.905178	-8.578486	2.996595
-49.633300	3.069802	3.006592
-48.656635	2.935207	3.016589
-48.364455	13.169508	3.026586
-48.323747	-0.655626	3.036582
-47.464102	12.258015	3.046579
-46.919700	6.830860	3.056576
-46.498438	1.707164	3.066573
-45.995280	8.697405	3.076570
-45.241224	3.630331	3.086566
-45.134489	9.057882	3.096563
-44.684375	-0.860613	3.106560
-43.944274	5.017215	3.116557
-43.445715	5.910376	3.126554
-42.980319	2.829039	3.136550
-42.105379	5.688413	3.146547
-41.858140	1.739729	3.156544
-41.835343	13.139071	3.166541
-41.224998	-3.498208	3.176538
-40.823869	2.126504	3.186534
-39.389157	6.301736	3.196531
-39.048961	-1.005645	3.206528
-38.829029	-2.169530	3.216525
-38.624139	-2.552833	3.226522
-38.266610	5.985761	3.236518
-37.307526	10.898763	3.246515
-37.138396	6.646691	3.256512
-36.622389	10.480244	3.266509
-35.762873	9.009738	3.276506
-35.339678	5.146758	3.286502
-35.227649	5.433769	3.296499
-34.162516	5.678790	3.306496
-34.080463	8.641888	3.316493
-34.005273	13.070745	3.326490
-32.236293	3.391149	3.336486
-32.256721	9.470383	3.346483
-32.175913	4.112831	3.356480
-31.898571	4.018935	3.366477
-30.918372	6.981478	3.376474
-30.594742	7.574856	3.386470
-29.373507	7.723847	3.396467
-29.017811	-0.387950	3.406464
-29.120949	6.599412	3.416461
-28.982835	5.011548	3.426458
-27.894438	4.521353	3.436454
-27.738808	5.425996	3.446451
-27.022555	5.763792	3.456448
-26.313762	11.028283	3.466445
-26.182437	5.695424	3.476442
-25.424596	3.004740	3.486438
-24.978262	-2.382003	3.496435
-24.417516	7.414619	3.506432
-23.392353	8.032527	3.516429
-23.380284	9.214022	3.526426
-22.991127	2.103024	3.536422
-22.877055	5.049272	3.546419
-21.879762	1.972296	3.556416
-21.443755	2.037937	3.566413
-20.927865	6.443253	3.576410
-20.232984	2.521349	3.586406
-19.805735	1.509108	3.596403
-19.732345	-0.576978	3.606400
-18.912697	4.578314	3.616397
-18.644249	6.828131	3.626394
-17.759055	11.893123	3.636390
-16.983236	11.689883	3.646387
-16.927596	8.107482	3.656384
-16.959841	18.690365	3.666381
-15.618992	15.136150	3.676378
-15.131940	4.243889	3.686374
-15.360464	2.764820	3.696371
-14.632983	-1.386851	3.706368
-13.893157	0.327710	3.716365
-13.108122	2.458324	3.726362
-12.560656	7.234433	3.736358
-12.055227	0.415232	3.746355
-11.819588	0.071646	3.756352
-11.946200	-0.140064	3.766349
-11.139035	-6.002007	3.776346
-10.619461	3.079331	3.786342
-9.266495	-0.889835	3.796339
-9.415270	-2.618762	3.806336
-9.204561	-3.148776	3.816333
-8.466949	2.276706	3.826330
-7.155011	3.069285	3.836326
-7.599312	3.406153	3.846323
-7.231263	4.085046	3.856320
-6.192021	-1.790506	3.866317
-5.527175	-0.948925	3.876314
-5.398447	4.376607	3.886310
-5.289263	5.495872	3.896307
-4.383670	-2.372081	3.906304
-3.905991	-6.989065	3.916301
-3.673661	-4.853842	3.926298
-3.066769	9.792114	3.936294
-2.721542	14.117325	3.946291
-2.253520	33.391322	3.956288
-1.939888	47.621853	3.966285
-1.349295	58.258899	3.976282
-1.196460	82.578881	3.986278
-0.552086	100.112679	3.996275
0.000000	122.745270	4.001280
0.108957	130.527890	4.006285
0.166904	138.166620	4.011290
0.431084	150.704737	4.016294
0.298820	160.396758	4.021299
0.492373	176.066846	4.026304
0.970547	168.042935	4.031309
0.434218	170.822545	4.036314
0.635293	168.403377	4.041318
0.792475	171.947401	4.046323
0.668695	176.432071	4.051328
1.066482	173.582417	4.056333
0.879442	174.816380	4.061338
0.945877	167.366123	4.066342
1.047130	164.835792	4.071347
1.000194	175.887796	4.076352
0.985571	184.186216	4.081357
0.817233	187.673938	4.086362
1.259821	190.870888	4.091366
1.247534	180.335350	4.096371
0.872140	178.578026	4.101376
1.138956	175.332701	4.106381
0.946323	179.624633	4.111386
1.428757	184.266813	4.116390
1.179524	183.819110	4.121395
1.167702	182.774176	4.126400
1.126487	178.149445	4.131405
1.167593	174.979700	4.136410
1.073020	176.954578	4.141414
1.046021	174.370362	4.146419
1.251927	184.707265	4.151424
1.197438	175.340080	4.156429
1.022390	185.170694	4.161434
1.348622	177.619292	4.166438
1.557976	176.677504	4.171443
1.321448	175.462134	4.176448
1.317339	172.608554	4.181453
1.423566	181.342791	4.186458
1.198933	181.222604	4.191462
1.129582	180.671380	4.196467
1.224884	169.631795	4.201472
1.092689	171.572245	4.206477
1.307990	176.277510	4.211482
1.405650	193.211752	4.216486
1.244933	182.285402	4.221491
1.495365	213.106754	4.226496
1.730853	192.324411	4.231501
1.244953	179.237374	4.236506
1.104179	176.013039	4.241510
1.599892	189.534012	4.246515
1.124855	192.489068	4.251520
1.482280	202.679596	4.256525
1.378608	206.331750	4.261530
1.493204	209.076999	4.266534
1.661255	210.173951	4.271539
1.598543	211.670908	4.276544
1.773036	210.336211	4.281549
1.361268	193.904513	4.286554
1.631457	195.429621	4.291558
1.363831	188.116444	4.296563
1.220025	200.957615	4.301568
1.503422	209.235607	4.306573
1.354844	208.912050	4.311578
1.496485	206.687776	4.316582
1.439840	206.321799	4.321587
1.153215	213.456749	4.326592
1.440965	203.348417	4.331597
1.292262	219.466773	4.336602
1.535313	210.805705	4.341606
1.410886	210.854629	4.346611
1.376707	221.059669	4.351616
1.782101	226.124509	4.356621
1.652031	248.743714	4.361626
1.922276	245.403888	4.366630
1.976913	235.434292	4.371635
1.688487	222.992055	4.376640
1.583897	220.386913	4.381645
1.299621	230.017479	4.386650
1.452290	232.751902	4.391654
1.792800	241.805578	4.396659
1.664776	237.105990	4.401664
1.735730	240.652835	4.406669
1.699119	239.566612	4.411674
2.072661	251.149506	4.416678
2.221684	235.830074	4.421683
1.869303	241.261953	4.426688
2.152245	235.254344	4.431693
2.148569	242.580113	4.436698
2.348854	234.350715	4.441702
2.140762	228.286039	4.446707
1.921267	223.884122	4.451712
1.819683	210.671887	4.456717
1.763882	207.115239	4.461722
2.012082	224.111652	4.466726
2.067480	222.868358	4.471731
1.866614	234.216061	4.476736
2.158012	231.965852	4.481741
1.867536	228.682584	4.486746
1.984633	237.517757	4.491750
1.955403	238.949694	4.496755
1.738518	250.032699	4.501760
2.037876	236.996285	4.506765
2.105357	245.486868	4.511770
2.183124	253.048979	4.516774
2.084655	247.225250	4.521779
2.112014	245.128674	4.526784
1.981084	240.052108	4.531789
2.023882	253.119187	4.536794
2.229284	247.015175	4.541798
2.137753	243.742929	4.546803
1.852253	247.259399	4.551808
2.182276	247.986461	4.556813
2.256459	243.136647	4.561818
2.273796	243.797587	4.566822
2.574706	240.201516	4.571827
1.946320	244.159309	4.576832
2.226925	229.903356	4.581837
2.195222	234.764984	4.586842
1.948694	236.908033	4.591846
2.328766	243.377881	4.596851
2.071205	248.217842	4.601856
2.449484	241.472017	4.606861
1.971399	256.371195	4.611866
2.347747	242.354927	4.616870
2.231881	242.813634	4.621875
1.959664	252.652655	4.626880
2.620889	265.224499	4.631885
2.328745	265.740455	4.636890
2.442404	263.533721	4.641894
2.479605	259.589659	4.646899
2.305776	267.890362	4.651904
2.612299	257.383083	4.656909
2.535347	263.250007	4.661914
2.441870	261.332037	4.666918
2.345989	251.585604	4.671923
2.306041	267.983487	4.676928
2.359262	269.400322	4.681933
2.444084	276.153975	4.686938
2.678501	265.920144	4.691942
2.327653	274.763314	4.696947
2.244258	272.547510	4.701952
2.437918	277.860357	4.706957
2.484331	274.298344	4.711962
2.295461	277.984622	4.716966
2.594247	272.508506	4.721971
2.437915	279.472491	4.726976
2.271996	268.776807	4.731981
2.590962	276.062197	4.736986
2.463999	283.137547	4.741990
2.479741	278.248840	4.746995
2.473742	293.555230	4.752000
2.802607	294.764225	4.757005
2.277920	310.167398	4.762010
2.155421	313.028404	4.767014
2.655940	311.626305	4.772019
2.369267	322.335146	4.777024
2.788949	304.799881	4.782029
2.752717	309.512718	4.787034
2.812609	308.470526	4.792038
2.973109	307.944551	4.797043
3.029094	312.186061	4.802048
2.937223	311.339624	4.807053
2.864178	316.702183	4.812058
2.718114	309.701134	4.817062
2.976895	304.932769	4.822067
2.676237	302.736192	4.827072
2.862565	300.041032	4.832077
2.978616	311.735781	4.837082
2.960036	309.458452	4.842086
2.647424	300.837663	4.847091
2.810822	311.535655	4.852096
3.051631	297.034445	4.857101
2.904218	300.997810	4.862106
2.882088	300.595839	4.867110
3.065435	297.318309	4.872115
2.906503	313.319672	4.877120
3.068389	315.155601	4.882125
3.059349	309.576339	4.887130
3.060544	307.291304	4.892134
3.230018	308.783147	4.897139
2.757037	309.254011	4.902144
3.197751	315.616888	4.907149
2.677839	318.048710	4.912154
2.927994	307.867498	4.917158
2.797665	318.131407	4.922163
2.999338	329.469780	4.927168
3.157107	334.356265	4.932173
2.827154	334.483055	4.937178
2.978799	338.770227	4.942182
3.234770	339.217212	4.947187
3.129521	344.620618	4.952192
3.191732	338.472259	4.957197
3.331142	340.584889	4.962202
3.146456	343.666515	4.967206
3.631621	337.808751	4.972211
3.606000	338.552661	4.977216
3.600599	341.162874	4.982221
3.319693	320.825101	4.987226
3.214979	325.418146	4.992230
2.992522	327.414079	4.997235
2.920859	326.221272	5.002240
3.797008	326.075642	5.007245
3.517541	334.785308	5.012250
3.596384	328.291964	5.017254
3.533341	324.873717	5.022259
3.040726	318.128036	5.027264
3.157786	316.185527	5.032269
3.349389	330.353654	5.037274
3.523743	339.428927	5.042278
3.765282	341.667732	5.047283
3.141334	338.893863	5.052288
3.545549	332.688001	5.057293
3.624250	336.607201	5.062298
3.287909	346.410608	5.067302
3.149803	334.998375	5.072307
3.385693	334.643147	5.077312
3.631777	335.731455	5.082317
3.436006	332.662976	5.087322
3.592127	330.489369	5.092326
3.607596	321.871077	5.097331
3.212524	344.503041	5.102336
3.627643	338.983209	5.107341
3.566788	349.137396	5.112346
3.556851	333.128480	5.117350
3.616775	345.103244	5.122355
3.340175	342.459520	5.127360
3.380901	351.019696	5.132365
3.556778	347.909528	5.137370
3.486769	339.112578	5.142374
3.570318	346.201510	5.147379
3.671102	343.428827	5.152384
3.760486	337.214712	5.157389
3.475007	340.057670	5.162394
3.642414	338.309972	5.167398
3.677059	338.557545	5.172403
3.569036	351.030660	5.177408
3.552346	348.121512	5.182413
3.760509	371.295391	5.187418
3.829046	380.099011	5.192422
3.922811	377.763348	5.197427
3.730805	371.540670	5.202432
4.001457	362.490589	5.207437
3.722215	369.266464	5.212442
3.750367	375.210378	5.217446
4.073222	377.244750	5.222451
3.780983	374.396524	5.227456
4.137219	366.641672	5.232461
3.794228	367.081288	5.237466
3.816691	365.392958	5.242470
3.856021	371.606132	5.247475
3.882052	377.258569	5.252480
4.344226	370.867899	5.257485
4.336412	366.937168	5.262490
3.870835	351.085416	5.267494
3.812753	347.798051	5.272499
3.501935	361.946929	5.277504
3.997892	363.957231	5.282509
4.040844	381.572379	5.287514
4.031056	378.401728	5.292518
4.144314	383.814914	5.297523
4.015427	382.651489	5.302528
4.232007	384.470101	5.307533
4.206643	374.945951	5.312538
3.752433	387.121535	5.317542
4.213089	374.745791	5.322547
4.068785	380.689201	5.327552
4.117009	367.691910	5.332557
3.977633	376.366412	5.337562
4.025519	382.681470	5.342566
4.360494	371.451189	5.347571
4.096680	378.430711	5.352576
4.332955	384.186626	5.357581
4.206625	385.202210	5.362586
4.060156	383.273250	5.367590
3.973866	372.058126	5.372595
3.758580	385.175269	5.377600
4.254152	387.451125	5.382605
4.063933	385.530382	5.387610
4.357629	391.275527	5.392614
4.686773	384.739710	5.397619
4.121282	385.161835	5.402624
4.285340	383.390218	5.407629
3.910307	379.480608	5.412634
3.709118	378.248923	5.417638
3.691280	381.540253	5.422643
3.800404	398.315174	5.427648
4.440283	398.310501	5.432653
4.576432	409.509606	5.437658
4.193383	409.460189	5.442662
4.697838	402.739613	5.447667
4.461136	416.756030	5.452672
4.579508	404.861941	5.457677
4.473621	410.910891	5.462682
4.538973	406.696653	5.467686
4.921270	402.157153	5.472691
4.487313	417.739201	5.477696
4.782565	404.241116	5.482701
4.394086	405.726123	5.487706
4.257249	397.805998	5.492710
4.416290	406.823068	5.497715
4.300838	403.146695	5.502720
4.480666	406.799303	5.507725
4.299619	407.869411	5.512730
4.458830	405.475277	5.517734
4.510035	401.026601	5.522739
4.214562	414.230322	5.527744
4.481440	406.756987	5.532749
4.549466	425.894859	5.537754
4.787356	448.960451	5.542758
4.743716	443.866531	5.547763
4.453834	447.960817	5.552768
4.822853	436.453061	5.557773
4.627321	442.262006	5.562778
4.746492	439.673321	5.567782
5.024856	431.049211	5.572787
4.662505	443.293616	5.577792
4.522652	440.262539	5.582797
4.533310	451.362544	5.587802
4.642317	443.778047	5.592806
4.634703	437.633098	5.597811
4.521280	442.990632	5.602816
4.656500	438.071377	5.607821
4.470056	446.681973	5.612826
4.495220	446.318354	5.617830
4.758835	434.549409	5.622835
4.501041	431.769769	5.627840
4.972482	450.853831	5.632845
5.140792	457.299965	5.637850
4.769267	461.456582	5.642854
5.263816	449.673141	5.647859
4.811502	454.509143	5.652864
4.906817	454.606204	5.657869
4.913892	448.191560	5.662874
4.855126	460.916290	5.667878
5.394109	461.154217	5.672883
4.842438	456.248430	5.677888
4.723302	443.495384	5.682893
4.934825	456.483452	5.687898
4.890212	469.114099	5.692902
5.220701	462.771395	5.697907
4.908416	480.095817	5.702912
5.055458	473.834530	5.707917
5.243951	473.599699	5.712922
5.079022	488.803701	5.717926
5.334844	474.186781	5.722931
5.245861	473.742084	5.727936
5.226259	476.201155	5.732941
5.324388	472.033672	5.737946
4.931604	467.294204	5.742950
5.212811	463.605245	5.747955
5.105940	479.111401	5.752960
5.194761	480.124979	5.757965
5.240703	473.772862	5.762970
5.116260	478.939454	5.767974
5.225651	462.807981	5.772979
5.412539	482.530460	5.777984
5.466570	473.801430	5.782989
5.137880	475.829242	5.787994
5.110759	489.361606	5.792998
5.444949	464.347831	5.798003
5.137149	483.797388	5.803008
5.395471	464.435916	5.808013
5.465375	471.806658	5.813018
5.351526	472.711069	5.818022
5.091451	468.924702	5.823027
5.231524	479.597069	5.828032
4.941963	473.325160	5.833037
5.167017	463.899172	5.838042
5.175670	484.728250	5.843046
5.217131	473.057354	5.848051
4.923246	469.193998	5.853056
5.228161	472.602096	5.858061
5.348768	494.923925	5.863066
5.384156	507.110741	5.868070
5.644643	505.182785	5.873075
5.378374	512.692369	5.878080
5.744217	513.011198	5.883085
5.537842	506.249406	5.888090
5.476191	521.433314	5.893094
5.558737	515.066745	5.898099
5.351176	528.583580	5.903104
5.726952	520.225977	5.908109
5.644551	508.216310	5.913114
5.436541	510.942610	5.918118
5.488882	511.783550	5.923123
5.593631	506.190739	5.928128
5.534681	512.182841	5.933133
5.527349	507.203755	5.938138
5.096839	512.461585	5.943142
5.393124	514.287562	5.948147
5.051550	519.267773	5.953152
5.397022	513.805166	5.958157
5.651893	525.802412	5.963162
5.611988	533.848985	5.968166
5.514147	535.036073	5.973171
5.444689	538.785650	5.978176
5.299937	528.837075	5.983181
5.202073	536.113533	5.988186
5.640722	530.957246	5.993190
5.765030	533.013302	5.998195
5.624975	533.791721	6.003200
6.080399	540.823333	6.008205
6.037461	536.257086	6.013210
5.815873	540.754376	6.018214
6.136884	535.073823	6.023219
5.568881	534.195561	6.028224
5.734495	531.662031	6.033229
5.585587	529.602340	6.038234
5.849346	537.056409	6.043238
6.080808	534.812805	6.048243
5.642396	526.547917	6.053248
5.579839	531.631983	6.058253
5.830825	545.055000	6.063258
5.563446	536.082977	6.068262
5.849502	540.662416	6.073267
5.661506	540.788440	6.078272
5.960145	540.323982	6.083277
5.835142	539.327423	6.088282
5.570547	529.641844	6.093286
6.056295	532.152376	6.098291
5.734723	542.196362	6.103296
6.139202	537.193016	6.108301
6.006035	536.138415	6.113306
5.761003	540.148854	6.118310
6.085921	533.326874	6.123315
5.704081	545.780381	6.128320
5.999399	531.546678	6.133325
5.999602	543.511833	6.138330
5.819174	538.861459	6.143334
6.234034	535.655624	6.148339
6.071222	544.146545	6.153344
5.997681	544.841162	6.158349
6.209311	533.451589	6.163354
6.179581	536.914511	6.168358
6.041476	517.530579	6.173363
5.798705	518.433213	6.178368
5.865316	516.136744	6.183373
5.834070	512.336623	6.188378
5.942784	508.703784	6.193382
5.997285	502.130037	6.198387
5.798681	511.316275	6.203392
5.933561	505.639460	6.208397
5.998521	503.293641	6.213402
5.995798	507.901259	6.218406
6.274398	511.988534	6.223411
5.672203	522.127915	6.228416
6.220115	521.906102	6.233421
6.075135	523.773037	6.238426
5.871357	518.812600	6.243430
6.078283	498.615954	6.248435
5.916186	508.891850	6.253440
5.739991	512.167350	6.258445
5.884516	512.589446	6.263450
5.460375	524.447325	6.268454
5.824163	512.266642	6.273459
5.704527	514.927924	6.278464
5.696019	509.499054	6.283469
5.709831	513.908796	6.288474
5.595435	523.607958	6.293478
5.840256	510.045206	6.298483
5.667753	515.375039	6.303488
5.515589	505.185006	6.308493
5.577420	512.041417	6.313498
5.538407	521.284851	6.318502
6.136960	513.163916	6.323507
5.841099	512.930102	6.328512
5.628296	515.908279	6.333517
5.684522	515.961781	6.338522
5.294720	526.457441	6.343526
5.742376	508.930640	6.348531
5.659315	521.500398	6.353536
5.670099	531.772503	6.358541
6.150766	529.236140	6.363546
5.777236	530.373089	6.368550
6.041835	514.247878	6.373555
5.937669	521.194078	6.378560
6.175772	515.261745	6.383565
6.223854	508.852927	6.388570
5.926911	514.399950	6.393574
5.863898	519.219289	6.398579
6.013213	523.856147	6.403584
5.842260	511.861012	6.408589
5.984932	513.496314	6.413594
5.939478	504.775716	6.418598
6.293771	512.081031	6.423603
5.868272	517.392198	6.428608
6.264718	508.627576	6.433613
5.788194	486.091554	6.438618
5.481911	486.353640	6.443622
5.766090	496.963826	6.448627
5.758845	512.565133	6.453632
5.719019	507.745619	6.458637
5.641539	514.726671	6.463642
6.028985	514.818767	6.468646
5.915658	504.098246	6.473651
5.738568	510.322675	6.478656
5.753535	502.785359	6.483661
5.785823	513.933432	6.488666
5.362248	516.011954	6.493670
5.855242	515.829504	6.498675
5.661612	526.402355	6.503680
5.956393	522.224361	6.508685
5.835256	519.512688	6.513690
5.949098	529.778219	6.518694
5.811564	508.254808	6.523699
5.881417	517.296251	6.528704
5.753030	516.965997	6.533709
6.196733	514.033516	6.538714
5.923444	522.299293	6.543718
5.875182	510.824134	6.548723
5.778805	506.923196	6.553728
5.789881	514.523194	6.558733
5.912196	500.797882	6.563738
5.620738	507.275621	6.568742
5.852231	504.029357	6.573747
5.735292	517.262265	6.578752
5.633609	519.809295	6.583757
5.822828	522.299965	6.588762
6.038569	515.195326	6.593766
5.650883	511.651228	6.598771
5.751926	511.992310	6.603776
5.797691	504.314546	6.608781
5.849469	516.525299	6.613786
5.430726	520.204042	6.618790
5.748761	514.889220	6.623795
5.417371	521.326504	6.628800
5.706505	526.340511	6.633805
5.741904	518.754922	6.638810
5.619483	519.900688	6.643814
5.972768	518.854393	6.648819
5.546213	526.721271	6.653824
5.681243	524.959270	6.658829
5.980251	518.201662	6.663834
5.603812	526.932197	6.668838
5.601310	519.094386	6.673843
5.560636	520.977036	6.678848
5.608649	519.134210	6.683853
5.477136	508.564086	6.688858
5.510300	527.307690	6.693862
5.806808	536.127987	6.698867
5.415685	543.526412	6.703872
5.344792	540.847573	6.708877
5.898460	537.958083	6.713882
5.723717	543.814144	6.718886
6.239011	541.710788	6.723891
5.935634	548.720307	6.728896
5.809256	548.851045	6.733901
6.205733	547.051460	6.738906
5.830344	549.727783	6.743910
5.831984	547.087864	6.748915
5.838700	547.589858	6.753920
5.986250	545.022808	6.758925
6.102176	549.261976	6.763930
5.702206	536.287800	6.768934
5.849925	528.683150	6.773939
5.956673	531.215667	6.778944
6.205366	544.290010	6.783949
6.117942	526.187942	6.788954
5.846055	525.956481	6.793958
6.015918	520.808704	6.798963
5.627506	533.341128	6.803968
5.724952	533.078032	6.808973
5.774048	522.265641	6.813978
5.874624	520.447574	6.818982
5.677129	512.976343	6.823987
5.734003	516.189945	6.828992
6.026310	527.233397	6.833997
5.834540	517.461008	6.839002
5.885875	524.926004	6.844006
5.904098	517.552901	6.849011
5.792391	515.211020	6.854016
5.507548	517.721822	6.859021
5.878334	512.464089	6.864026
5.638177	523.428109	6.869030
5.894744	509.913929	6.874035
5.799342	517.601374	6.879040
5.624865	522.098568	6.884045
5.990522	517.920208	6.889050
5.917019	524.293862	6.894054
5.974933	524.658252	6.899059
5.787774	524.469319	6.904064
6.024614	526.505002	6.909069
6.164566	528.758551	6.914074
6.099280	529.372779	6.919078
6.066107	516.703433	6.924083
5.727916	527.070794	6.929088
5.842380	521.098513	6.934093
5.933634	525.438831	6.939098
5.646716	525.356557	6.944102
6.008773	530.456779	6.949107
5.894542	523.018250	6.954112
5.990281	533.626059	6.959117
5.877638	530.154203	6.964122
5.486157	526.941429	6.969126
5.667029	525.190499	6.974131
5.949008	522.245970	6.979136
5.384881	528.559919	6.984141
5.699216	523.751723	6.989146
5.442391	516.633623	6.994150
5.652661	515.906442	6.999155
5.452546	522.285332	7.004160
5.566042	521.921222	7.009165
5.625315	515.765089	7.014170
5.588956	535.964543	7.019174
5.815948	532.525647	7.024179
5.611537	547.005964	7.029184
5.870187	550.729144	7.034189
5.950936	542.943468	7.039194
6.036761	544.037064	7.044198
5.691886	531.072335	7.049203
5.556155	536.452729	7.054208
5.841838	539.367771	7.059213
6.108460	540.890840	7.064218
5.641801	537.823381	7.069222
5.698376	541.490272	7.074227
5.680027	538.226391	7.079232
5.757604	559.464365	7.084237
6.228321	544.281578	7.089242
6.019017	551.515884	7.094246
5.831316	531.436008	7.099251
5.594013	524.373677	7.104256
5.325222	526.781296	7.109261
5.982771	533.474847	7.114266
5.812495	544.032603	7.119270
5.741372	538.196746	7.124275
5.887230	543.609435	7.129280
5.792505	546.447841	7.134285
5.831082	550.298747	7.139290
5.672599	550.000793	7.144294
6.066745	539.304119	7.149299
5.678737	547.080285	7.154304
5.921911	543.342048	7.159309
6.244658	532.800824	7.164314
5.948316	536.481936	7.169318
6.101846	514.337904	7.174323
6.330884	520.546918	7.179328
5.736059	514.420151	7.184333
6.110502	520.191562	7.189338
5.812263	522.286172	7.194342
6.002832	517.951072	7.199347
5.780598	525.976667	7.204352
5.672614	530.104056	7.209357
5.779678	521.003568	7.214362
5.827827	535.207430	7.219366
6.097418	529.683167	7.224371
5.528856	521.046836	7.229376
5.748563	530.241008	7.234381
6.036614	528.611473	7.239386
5.638941	528.089631	7.244390
5.831632	525.956421	7.249395
5.939097	520.072708	7.254400
5.749500	517.843540	7.259405
5.922338	526.671147	7.264410
5.663930	530.871836	7.269414
6.076911	512.987798	7.274419
5.813467	519.082362	7.279424
5.933789	524.947961	7.284429
5.845291	527.273398	7.289434
5.866310	526.817921	7.294438
6.047123	524.836930	7.299443
5.711629	539.403227	7.304448
5.744450	525.845405	7.309453
6.026183	528.372780	7.314458
5.707417	531.615215	7.319462
5.607565	532.980318	7.324467
5.888876	526.587311	7.329472
5.483392	524.515660	7.334477
5.929369	526.422663	7.339482
5.786934	522.520847	7.344486
5.441049	513.637482	7.349491
5.599499	509.849423	7.354496
5.457272	526.665330	7.359501
6.025366	519.127561	7.364506
5.729039	530.751813	7.369510
5.984741	522.054049	7.374515
5.750625	528.006438	7.379520
5.806637	527.746539	7.384525
6.008502	527.646830	7.389530
5.799514	525.480849	7.394534
5.608886	525.450046	7.399539
5.642214	536.298438	7.404544
5.607981	527.146909	7.409549
5.481944	516.882898	7.414554
5.758005	527.366389	7.419558
5.624551	524.834730	7.424563
5.776707	528.033773	7.429568
5.900539	542.601416	7.434573
5.737155	538.575494	7.439578
5.687183	543.074020	7.444582
5.936705	553.617460	7.449587
6.017270	547.066123	7.454592
5.936833	546.737612	7.459597
6.311333	523.107666	7.464602
6.075213	533.052185	7.469606
5.807648	525.316778	7.474611
5.719385	525.693190	7.479616
5.661824	523.844922	7.484621
5.910376	517.376531	7.489626
5.640890	522.430268	7.494630
5.854685	515.088383	7.499635
5.699974	516.084592	7.504640
5.477974	519.295149	7.509645
5.868197	524.737694	7.514650
5.630728	523.025905	7.519654
5.596456	525.403844	7.524659
5.782158	534.816740	7.529664
5.953139	541.358463	7.534669
6.025860	540.957187	7.539674
5.913102	529.692949	7.544678
6.138682	522.339839	7.549683
5.974430	530.782352	7.554688
5.691723	515.397347	7.559693
5.780570	517.647698	7.564698
5.586300	524.728560	7.569702
5.916007	510.332919	7.574707
5.463453	516.805121	7.579712
5.479205	525.604032	7.584717
6.095370	524.258374	7.589722
5.944982	534.319054	7.594726
5.837394	530.198180	7.599731
5.690536	528.219049	7.604736
5.744774	526.503746	7.609741
5.906959	516.419511	7.614746
5.714554	528.004882	7.619750
5.833204	526.842863	7.624755
5.881206	529.798168	7.629760
5.664591	540.462434	7.634765
5.829550	533.823557	7.639770
5.893744	536.461864	7.644774
5.931517	535.158217	7.649779
5.848646	527.683624	7.654784
5.810486	528.624169	7.659789
5.645733	525.079730	7.664794
5.561031	530.258418	7.669798
5.745776	544.626080	7.674803
5.965714	544.546075	7.679808
5.601173	549.270423	7.684813
5.942356	552.857925	7.689818
5.657914	548.387227	7.694822
5.746731	553.868838	7.699827
5.797633	550.837293	7.704832
6.086797	551.345591	7.709837
6.017565	542.007256	7.714842
6.049214	537.554571	7.719846
5.848428	516.269600	7.724851
5.554381	525.715008	7.729856
5.638468	532.946202	7.734861
5.891149	534.560367	7.739866
5.738877	552.255821	7.744870
6.154409	535.923325	7.749875
5.685340	535.869476	7.754880
5.787515	542.143367	7.759885
6.054921	530.370862	7.764890
5.908623	533.597029	7.769894
5.888538	525.633373	7.774899
5.793999	530.739101	7.779904
5.303602	533.685610	7.784909
5.816858	524.152961	7.789914
5.800931	536.018566	7.794918
5.802699	533.502838	7.799923
5.723769	539.494997	7.804928
5.663877	544.366512	7.809933
5.528548	545.630929	7.814938
5.674628	557.718001	7.819942
5.944318	553.955253	7.824947
5.837558	553.996621	7.829952
5.498163	559.178537	7.834957
5.906601	561.879335	7.839962
5.414344	557.764603	7.844966
5.956898	544.948099	7.849971
5.743474	552.371818	7.854976
5.737280	549.491777	7.859981
5.851818	555.197235	7.864986
5.860939	559.704055	7.869990
5.758454	544.983692	7.874995
6.075711	552.000752	7.880000
6.008048	552.074628	7.885005
6.037764	548.638832	7.890010
5.629282	553.977881	7.895014
5.696393	547.097769	7.900019
5.882759	546.581818	7.905024
5.770801	556.411418	7.910029
5.813034	547.075083	7.915034
5.940230	544.118342	7.920038
5.804752	542.104773	7.925043
6.005151	551.554713	7.930048
5.585558	559.069531	7.935053
6.105857	554.481234	7.940058
5.937375	556.268197	7.945062
5.885850	543.043951	7.950067
6.062676	554.432374	7.955072
5.502921	552.528676	7.960077
5.788636	553.163727	7.965082
5.631325	552.046225	7.970086
5.906909	551.462057	7.975091
5.862500	555.179282	7.980096
5.789143	547.630002	7.985101
5.991661	549.408338	7.990106
5.981274	554.793083	7.995110
5.665660	555.807203	8.000115
5.754332	547.491967	8.005133
5.519292	552.553910	8.010150
6.010673	545.915936	8.015168
5.814008	565.938664	8.020186
5.933026	553.907158	8.025203
5.759331	553.747559	8.030221
5.620589	562.608218	8.035238
6.108220	555.931103	8.040256
5.848766	554.757133	8.045274
5.833399	548.958366	8.050291
5.842078	540.418063	8.055309
5.634755	563.238863	8.060326
6.026690	550.261938	8.065344
5.583467	556.402870	8.070362
5.535303	546.263111	8.075379
5.726171	560.770768	8.080397
5.623324	559.744112	8.085414
5.316524	549.574763	8.090432
5.614772	550.136822	8.095450
5.373302	554.770777	8.100467
5.605935	575.923920	8.105485
5.940615	591.211427	8.110502
5.978965	587.617033	8.115520
6.019637	599.575034	8.120538
6.035266	590.040238	8.125555
6.019796	591.707290	8.130573
5.825888	591.341622	8.135590
6.347572	585.514611	8.140608
6.248754	587.600676	8.145626
5.750687	573.855627	8.150643
6.151362	581.328977	8.155661
5.962781	573.526632	8.160678
6.289441	568.230384	8.165696
6.283318	558.279104	8.170714
5.837959	560.027725	8.175731
6.194622	560.444035	8.180749
6.112324	557.523399	8.185766
6.274163	548.632350	8.190784
6.207732	554.091251	8.195802
6.221599	558.985414	8.200819
6.245771	563.205859	8.205837
6.045439	557.952420	8.210854
6.057070	564.010217	8.215872
6.131158	557.439820	8.220890
5.745962	557.030188	8.225907
6.018193	561.731783	8.230925
5.901985	562.830651	8.235942
6.000837	551.795203	8.240960
5.749577	559.501254	8.245978
5.743984	558.918675	8.250995
5.892256	555.644248	8.256013
5.910366	549.660456	8.261030
6.010477	553.881239	8.266048
5.968823	552.312584	8.271066
5.933282	559.598021	8.276083
6.119036	583.444236	8.281101
6.106930	588.597771	8.286118
6.580932	581.912072	8.291136
6.059825	571.291700	8.296154
5.598500	569.260707	8.301171
6.335978	579.428465	8.306189
6.129799	583.033955	8.311206
6.086253	584.649260	8.316224
6.055905	588.199814	8.321242
6.057244	583.787972	8.326259
6.407283	592.016797	8.331277
6.232660	588.177632	8.336294
6.267343	577.743111	8.341312
6.250146	579.802598	8.346330
5.981005	566.605835	8.351347
6.290600	569.682963	8.356365
5.839360	578.435265	8.361382
6.317966	588.612449	8.366400
6.381747	586.215988	8.371418
6.206612	584.423766	8.376435
6.306147	559.639131	8.381453
5.804975	569.034105	8.386470
6.161710	579.830818	8.391488
6.078521	583.029049	8.396506
6.165795	591.760856	8.401523
6.255354	589.719812	8.406541
6.058953	590.271016	8.411558
6.054281	573.353381	8.416576
6.172771	579.922952	8.421594
5.920232	595.287529	8.426611
6.024451	584.701480	8.431629
5.604541	592.708594	8.436646
5.887832	588.915780	8.441664
6.320861	588.369847	8.446682
6.220412	596.105905	8.451699
6.465151	589.700072	8.456717
6.297807	597.716524	8.461734
6.744592	579.189920	8.466752
6.526303	580.482692	8.471770
6.290343	592.340858	8.476787
6.312601	581.979733	8.481805
6.154860	594.197444	8.486822
6.154712	581.549804	8.491840
6.027781	585.546847	8.496858
5.956140	593.814754	8.501875
6.405308	598.693282	8.506893
6.072747	623.420537	8.511910
6.555326	613.911099	8.516928
6.340474	620.486374	8.521946
6.534396	626.555008	8.526963
6.744866	610.728438	8.531981
6.467750	606.753085	8.536998
6.505278	595.822112	8.542016
6.591299	593.739140	8.547034
6.419819	599.440276	8.552051
6.764616	591.455602	8.557069
6.290092	594.482921	8.562087
6.440773	591.373411	8.567104
6.574138	587.800809	8.572122
6.309388	591.153727	8.577139
6.645799	600.324887	8.582157
6.320519	580.328434	8.587175
6.285220	586.294112	8.592192
6.048870	592.386898	8.597210
5.937000	596.449552	8.602227
6.382809	594.020956	8.607245
6.277797	622.337088	8.612263
6.469273	613.676395	8.617280
6.307627	616.554983	8.622298
6.179082	623.313794	8.627315
6.146447	620.794508	8.632333
6.277238	629.703560	8.637351
6.256900	626.669639	8.642368
6.592943	620.506827	8.647386
6.594100	622.726445	8.652403
6.566746	615.702108	8.657421
6.640412	622.485660	8.662439
6.431819	622.119072	8.667456
7.060384	611.689516	8.672474
6.599044	627.159581	8.677491
6.611727	625.265561	8.682509
6.392070	634.035716	8.687527
6.419257	625.740883	8.692544
6.373710	625.302771	8.697562
6.268322	630.350892	8.702579
6.422250	631.220708	8.707597
6.338090	625.717382	8.712615
6.432600	626.029112	8.717632
6.798334	621.286717	8.722650
6.441291	624.305944	8.727667
6.609627	617.648503	8.732685
6.641314	624.149776	8.737703
6.509477	623.819608	8.742720
6.639521	617.332343	8.747738
6.277748	619.891020	8.752755
6.908367	621.286474	8.757773
6.803211	636.153497	8.762791
6.630726	630.025908	8.767808
6.628394	621.959240	8.772826
6.491702	626.123132	8.777843
6.692312	623.647174	8.782861
6.672869	613.536082	8.787879
6.308629	616.016243	8.792896
6.768192	616.271286	8.797914
6.684634	623.523554	8.802931
6.710929	621.666254	8.807949
6.521773	620.138894	8.812967
6.473113	638.402345	8.817984
6.796083	646.962286	8.823002
6.660273	661.868350	8.828019
6.566576	651.745198	8.833037
6.765796	650.421123	8.838055
6.582810	655.755352	8.843072
6.850128	652.646630	8.848090
6.786251	661.547032	8.853107
6.860496	649.336073	8.858125
6.968544	649.795834	8.863143
6.850853	654.094362	8.868160
6.558100	640.436562	8.873178
6.787923	650.276624	8.878195
6.765227	657.489623	8.883213
6.526126	660.437210	8.888231
6.556508	660.652471	8.893248
7.054545	660.145292	8.898266
6.693664	661.348959	8.903283
7.104986	659.050733	8.908301
7.058896	659.435296	8.913319
6.817388	646.641007	8.918336
7.088214	641.713638	8.923354
6.651535	634.757625	8.928371
6.873376	621.727366	8.933389
6.959754	627.685450	8.938407
6.615954	629.073757	8.943424
7.109268	629.684573	8.948442
6.875585	623.151823	8.953459
6.774234	621.128054	8.958477
6.757912	621.861665	8.963495
6.459838	649.958914	8.968512
7.164678	652.688806	8.973530
6.910365	664.064126	8.978547
6.721989	651.182918	8.983565
6.892883	658.452000	8.988583
6.869667	662.638283	8.993600
7.288516	650.206725	8.998618
7.088408	650.333228	9.003635
6.865112	643.318625	9.008653
6.694167	636.448889	9.013671
6.466607	658.781140	9.018688
6.852653	654.411491	9.023706
6.683098	651.155321	9.028723
6.606442	660.982664	9.033741
7.103608	659.569004	9.038759
6.627032	658.711366	9.043776
6.500439	656.791745	9.048794
6.781420	657.136919	9.053811
6.695226	654.715635	9.058829
7.006695	659.089772	9.063847
6.808742	660.718301	9.068864
7.022588	691.905346	9.073882
7.269741	688.836753	9.078899
6.989032	678.226079	9.083917
7.095798	670.775689	9.088935
6.819125	673.438498	9.093952
7.041407	665.143286	9.098970
7.110145	688.929293	9.103987
7.125602	682.515651	9.109005
6.981894	658.531841	9.114023
6.752790	675.893438	9.119040
7.155003	675.636893	9.124058
7.157415	688.033982	9.129075
7.324889	688.405295	9.134093
7.535693	674.936345	9.139111
6.795350	663.381155	9.144128
6.816852	659.567916	9.149146
6.748010	671.539839	9.154163
6.803978	685.750379	9.159181
7.296469	680.933781	9.164199
6.946432	682.869971	9.169216
7.387276	682.566401	9.174234
7.131931	684.380467	9.179251
7.033870	678.325780	9.184269
6.970509	681.992618	9.189287
7.016946	696.023378	9.194304
7.524826	684.100213	9.199322
7.170968	683.880342	9.204339
7.035592	684.779077	9.209357
7.171013	680.635646	9.214375
6.888713	693.094058	9.219392
7.159058	676.818236	9.224410
7.165412	681.336485	9.229427
7.081843	681.930354	9.234445
7.306845	684.454561	9.239463
7.087020	690.298439	9.244480
7.073345	691.153445	9.249498
6.952701	691.343575	9.254515
6.990553	693.271463	9.259533
7.200997	690.200966	9.264551
6.614473	690.647875	9.269568
7.195801	702.842239	9.274586
7.267560	717.919333	9.279603
7.169966	719.738529	9.284621
7.562590	721.614976	9.289639
7.273064	723.409208	9.294656
7.383990	726.501682	9.299674
7.260538	724.272141	9.304691
7.290795	726.900178	9.309709
7.432796	715.967010	9.314727
7.342640	710.964948	9.319744
7.515036	720.725585	9.324762
7.330363	698.100995	9.329779
7.224065	695.308587	9.334797
7.260564	692.930789	9.339815
7.203578	710.141071	9.344832
7.157467	714.054232	9.349850
7.654951	720.108460	9.354867
7.564448	736.610462	9.359885
7.407140	717.022706	9.364903
7.418263	704.461374	9.369920
7.236261	698.768520	9.374938
7.352405	702.854041	9.379955
7.037741	709.362695	9.384973
7.585705	723.797322	9.389991
7.644716	722.908937	9.395008
7.605562	716.915649	9.400026
7.220932	711.827136	9.405043
7.124899	716.366449	9.410061
7.738561	727.568955	9.415079
7.566878	727.535277	9.420096
7.456542	724.822356	9.425114
7.332672	727.357381	9.430131
7.070138	722.899654	9.435149
7.574305	712.471202	9.440167
7.644936	719.086825	9.445184
7.331439	720.329311	9.450202
7.505547	728.766779	9.455219
7.376244	737.626963	9.460237
7.478445	724.697279	9.465255
7.475024	733.855105	9.470272
7.629812	729.928796	9.475290
7.597244	730.802868	9.480307
7.219393	724.024656	9.485325
7.795291	725.696931	9.490343
7.570203	730.296445	9.495360
7.774535	715.190437	9.500378
7.983446	716.033263	9.505395
7.752637	728.983006	9.510413
7.867370	701.197449	9.515431
7.367513	697.150043	9.520448
7.486186	686.279697	9.525466
7.871492	687.802591	9.530483
7.424974	688.440301	9.535501
7.437732	691.836833	9.540519
7.968019	713.668107	9.545536
7.798231	707.266174	9.550554
7.580472	676.923679	9.555571
7.150422	691.704708	9.560589
7.732424	690.167696	9.565607
7.734418	712.415543	9.570624
7.602117	713.422019	9.575642
7.661452	706.639273	9.580659
7.504682	721.516777	9.585677
8.087723	719.995828	9.590695
7.448447	722.810676	9.595712
7.748775	710.055608	9.600730
7.803989	705.067805	9.605747
7.587197	717.439047	9.610765
7.733226	708.031223	9.615783
7.816691	721.264199	9.620800
7.709781	707.956661	9.625818
7.603507	709.259569	9.630835
7.452565	720.709663	9.635853
7.545418	716.857852	9.640871
7.500769	721.415835	9.645888
7.503844	722.319442	9.650906
7.635717	723.871232	9.655923
7.672846	729.119612	9.660941
7.800041	726.633136	9.665959
7.552868	727.506754	9.670976
7.685250	717.797494	9.675994
7.891888	722.400943	9.681011
7.721920	726.761172	9.686029
7.577913	724.208610	9.691047
7.806288	730.204871	9.696064
8.134015	735.058343	9.701082
7.817986	731.552494	9.706099
7.836172	733.082527	9.711117
7.791445	730.129670	9.716135
7.867314	726.902598	9.721152
7.685517	727.253792	9.726170
7.774423	721.436646	9.731187
7.573361	728.411683	9.736205
7.844705	726.516335	9.741223
7.945180	740.676369	9.746240
7.702959	745.171160	9.751258
8.018125	748.077553	9.756275
8.041114	756.950271	9.761293
8.231620	749.443787	9.766311
8.010018	744.311495	9.771328
7.688784	732.801638	9.776346
8.177595	724.346425	9.781363
7.954517	725.899009	9.786381
8.006666	720.468480	9.791399
8.059264	729.296533	9.796416
7.866102	728.114742	9.801434
8.093876	724.534674	9.806451
7.681942	714.407290	9.811469
7.825375	715.608215	9.816487
7.863071	730.168013	9.821504
8.222016	735.717677	9.826522
7.999112	743.362943	9.831539
8.068919	749.321254	9.836557
8.026002	737.903760	9.841575
7.958477	739.298773	9.846592
7.881103	750.212022	9.851610
8.197355	737.805812	9.856627
8.008363	750.964864	9.861645
8.231475	755.719904	9.866663
8.461140	756.266145	9.871680
8.055105	738.154644	9.876698
7.966954	724.075626	9.881715
7.907096	726.884470	9.886733
8.009070	735.277376	9.891751
8.210605	749.839738	9.896768
8.168248	751.559471	9.901786
8.205405	751.997491	9.906803
7.750953	748.762106	9.911821
7.798599	739.665351	9.916839
8.200415	749.230838	9.921856
8.148311	755.548411	9.926874
8.247337	759.508355	9.931891
7.887226	769.712472	9.936909
7.951842	757.788795	9.941927
8.144785	751.676739	9.946944
8.081825	749.649561	9.951962
8.212046	746.394413	9.956979
8.309829	756.052167	9.961997
8.086135	742.645022	9.967015
8.660427	758.198359	9.972032
8.441678	760.184307	9.977050
8.313702	747.008442	9.982067
8.254582	759.187844	9.987085
8.103635	756.341692	9.992103
8.217342	755.540115	9.997120
8.093873	761.599256	10.002138
8.435193	751.260769	10.007155
8.014665	766.232977	10.012173
8.206716	747.487094	10.017191
8.218743	756.441038	10.022208
7.934516	756.560286	10.027226
8.500322	757.953081	10.032243
8.364584	773.700726	10.037261
8.659800	759.159278	10.042279
8.571900	751.056495	10.047296
8.048470	767.783688	10.052314
7.949326	765.275369	10.057331
8.241809	760.594045	10.062349
8.119659	760.204999	10.067367
8.451078	755.969622	10.072384
8.531933	752.815330	10.077402
8.622240	757.271803	10.082419
8.416330	762.372793	10.087437
8.076000	754.048877	10.092455
8.714857	749.649330	10.097472
8.469939	763.949324	10.102490
8.341346	760.290467	10.107507
8.122581	761.983753	10.112525
8.206985	761.716058	10.117543
8.367659	757.136030	10.122560
8.228314	759.278806	10.127578
8.076610	771.248164	10.132595
8.478509	781.642153	10.137613
8.809980	787.182402	10.142631
8.562089	794.862919	10.147648
8.374265	792.266119	10.152666
8.808977	781.552300	10.157683
8.622090	780.715864	10.162701
8.362681	770.566583	10.167719
8.801305	763.778798	10.172736
8.333305	774.392509	10.177754
8.349091	759.214681	10.182771
8.396600	777.661386	10.187789
8.445193	789.697542	10.192807
8.765385	782.766160	10.197824
8.322570	792.409257	10.202842
8.331280	783.186158	10.207859
8.469312	790.027443	10.212877
8.583593	795.984327	10.217895
8.957751	783.252720	10.222912
9.002811	795.239079	10.227930
8.993971	788.449259	10.232947
8.628247	775.053846	10.237965
8.572201	766.682943	10.242983
8.729832	761.311727	10.248000
8.408899	763.963561	10.253018
8.248069	786.580882	10.258035
8.675932	785.926171	10.263053
8.699100	794.210401	10.268071
8.795410	790.525196	10.273088
8.710528	790.883205	10.278106
8.891292	787.013798	10.283123
8.969745	799.578103	10.288141
8.582983	796.442919	10.293159
9.009698	795.621497	10.298176
8.590462	791.469813	10.303194
8.781488	795.573098	10.308211
8.867414	781.241284	10.313229
8.440501	776.643018	10.318247
8.632486	782.789776	10.323264
8.216544	793.354353	10.328282
8.492955	793.955753	10.333299
8.758491	799.272396	10.338317
8.334818	791.038204	10.343335
8.718173	788.845450	10.348352
8.522069	791.167069	10.353370
8.689125	796.306319	10.358387
8.773399	800.686650	10.363405
8.567909	798.158308	10.368423
8.760449	806.324512	10.373440
9.004884	822.635551	10.378458
8.758221	813.833113	10.383475
8.653705	814.697135	10.388493
8.904897	820.133753	10.393511
9.015893	820.580239	10.398528
8.824483	835.177308	10.403546
8.870034	824.169762	10.408563
9.196943	820.729561	10.413581
8.817987	818.798878	10.418599
8.979946	813.544230	10.423616
8.803211	819.574999	10.428634
9.019847	823.971842	10.433651
9.130745	820.432618	10.438669
8.806162	817.489186	10.443687
9.228824	813.592492	10.448704
9.223334	808.719984	10.453722
9.321844	800.749825	10.458739
9.013048	795.182398	10.463757
8.671050	790.019011	10.468775
9.123595	789.792330	10.473792
8.727764	801.034374	10.478810
8.972065	784.492908	10.483827
9.167625	788.720026	10.488845
9.103711	792.905591	10.493863
9.226404	788.343443	10.498880
8.908189	789.417451	10.503898
8.933067	790.979450	10.508915
9.283482	783.074642	10.513933
8.978790	790.995507	10.518951
9.115012	794.859467	10.523968
9.079731	793.168003	10.528986
8.970061	794.528950	10.534003
8.932494	791.535140	10.539021
8.764733	805.582700	10.544039
9.181475	817.329634	10.549056
9.114503	824.559868	10.554074
9.204193	816.919941	10.559091
9.426727	828.590925	10.564109
9.102748	822.507189	10.569127
9.125659	821.963582	10.574144
8.794914	815.005430	10.579162
9.099406	806.117918	10.584179
9.365285	819.181586	10.589197
9.213356	821.954196	10.594215
9.252250	820.396706	10.599232
9.397163	819.674009	10.604250
9.175215	828.731119	10.609267
9.381773	823.604704	10.614285
9.253924	824.539106	10.619303
9.449428	815.501026	10.624320
9.339214	824.043199	10.629338
9.245545	804.021760	10.634355
9.689058	812.715390	10.639373
8.762101	802.910516	10.644391
9.207095	807.769825	10.649408
8.960992	808.924914	10.654426
9.184637	819.866307	10.659443
9.411318	818.897559	10.664461
9.101043	817.159132	10.669479
9.333347	815.298665	10.674496
9.701456	827.310981	10.679514
9.345678	821.410225	10.684531
9.242807	814.694485	10.689549
9.023994	821.861834	10.694567
9.242068	815.497710	10.699584
9.139543	817.157918	10.704602
9.135734	822.453540	10.709619
9.140906	818.908564	10.714637
8.964228	823.580604	10.719655
9.359520	835.406969	10.724672
9.443938	844.020515	10.729690
9.355334	854.465892	10.734707
9.260130	847.258699	10.739725
9.554924	854.653830	10.744743
9.382418	853.321889	10.749760
9.713996	860.928131	10.754778
9.450014	856.433701	10.759795
9.770908	857.341085	10.764813
9.769879	850.159561	10.769831
9.434205	837.954985	10.774848
9.101968	831.668904	10.779866
9.411007	849.902131	10.784883
9.759037	841.479961	10.789901
9.494088	854.025285	10.794919
9.551488	847.313650	10.799936
9.549037	854.048969	10.804954
9.460483	850.432579	10.809971
9.656689	856.224399	10.814989
9.672820	851.649631	10.820007
9.570112	857.719649	10.825024
9.952062	851.303039	10.830042
9.847359	867.387816	10.835059
9.604541	827.011020	10.840077
9.365753	832.975880	10.845095
9.537746	843.668883	10.850112
9.617738	853.584221	10.855130
9.422536	856.126037	10.860147
10.046447	855.945137	10.865165
9.696315	860.240804	10.870183
9.677481	861.602097	10.875200
9.939135	852.462331	10.880218
9.148809	851.460599	10.885235
9.671093	848.874469	10.890253
9.732637	851.459667	10.895271
9.801983	849.534705	10.900288
9.555012	853.911533	10.905306
9.643659	857.388163	10.910323
9.722474	851.287153	10.915341
9.664458	864.017936	10.920359
9.370825	854.228525	10.925376
9.279109	853.814570	10.930394
9.360668	849.595364	10.935411
9.755062	844.983673	10.940429
9.894119	863.942525	10.945447
9.744419	870.328725	10.950464
9.620903	863.425857	10.955482
9.956117	882.368749	10.960499
9.737125	878.364038	10.965517
9.766676	886.829910	10.970535
9.952255	892.514955	10.975552
10.118290	885.218223	10.980570
9.887035	891.210694	10.985587
9.880978	888.468997	10.990605
9.683379	887.967438	10.995623
9.943032	880.270262	11.000640
10.292309	889.666991	11.005658
10.123089	883.354639	11.010675
9.951573	856.682363	11.015693
10.052493	860.000102	11.020711
10.090759	865.115686	11.025728
10.009830	860.435321	11.030746
9.778216	862.840070	11.035763
9.854112	853.216326	11.040781
9.644848	861.487831	11.045799
9.926867	882.838121	11.050816
10.289752	880.835123	11.055834
9.924168	884.067782	11.060851
10.226601	895.148743	11.065869
10.058395	885.711356	11.070887
10.089322	877.791001	11.075904
10.128249	876.502451	11.080922
10.188321	890.217900	11.085939
9.992924	876.842372	11.090957
9.922388	886.929827	11.095975
9.581269	892.192549	11.100992
10.088231	890.256080	11.106010
9.867420	894.091876	11.111027
9.952748	883.207712	11.116045
9.906217	885.848171	11.121063
9.959105	883.748592	11.126080
9.887349	889.009312	11.131098
10.136821	891.970478	11.136115
10.143585	886.967793	11.141133
9.753400	891.558227	11.146151
9.647428	896.851175	11.151168
9.960685	901.066549	11.156186
9.946929	921.751719	11.161203
10.040285	916.503256	11.166221
10.009574	922.510425	11.171239
10.084357	919.657348	11.176256
10.189491	913.729297	11.181274
10.027519	918.367445	11.186291
10.289171	917.177495	11.191309
10.067458	930.008403	11.196327
10.267113	925.490278	11.201344
10.463733	924.618110	11.206362
10.385036	917.508631	11.211379
10.700600	914.099512	11.216397
10.257247	913.742681	11.221415
10.427235	923.660118	11.226432
10.441622	908.697201	11.231450
10.331332	926.252598	11.236467
10.473307	917.269361	11.241485
10.505209	917.088475	11.246503
10.060734	920.975214	11.251520
10.524139	925.915658	11.256538
10.394744	930.778702	11.261555
10.398375	921.940547	11.266573
10.437924	920.345642	11.271591
10.164102	918.043202	11.276608
10.268575	909.620798	11.281626
10.310067	920.337684	11.286643
10.609708	924.842865	11.291661
10.431337	911.099595	11.296679
10.335523	921.026512	11.301696
10.542489	909.880733	11.306714
10.326807	920.883582	11.311731
10.317860	915.845300	11.316749
10.660256	921.685317	11.321767
10.642585	935.587051	11.326784
10.727917	921.520121	11.331802
10.308404	930.493619	11.336819
10.028729	926.253688	11.341837
10.414560	936.526738	11.346855
10.460661	945.665189	11.351872
10.756933	955.275013	11.356890
10.513947	950.751696	11.361907
10.718758	943.824844	11.366925
11.025291	946.472311	11.371943
10.882052	950.379343	11.376960
11.074355	930.301034	11.381978
10.630244	920.601988	11.386995
10.855430	922.536834	11.392013
10.964527	911.558383	11.397031
10.519076	926.457615	11.402048
10.882259	913.517021	11.407066
10.966984	916.579027	11.412083
10.834478	922.978350	11.417101
11.039212	919.348609	11.422119
10.719440	918.644244	11.427136
10.740509	925.659617	11.432154
10.763836	932.115067	11.437171
10.635276	921.728547	11.442189
11.087071	916.607827	11.447207
10.793767	933.651835	11.452224
10.741863	916.143401	11.457242
10.664770	927.582330	11.462259
10.795398	927.209372	11.467277
10.577124	915.756365	11.472295
10.556532	922.006506	11.477312
10.740700	915.842990	11.482330
10.912361	914.963335	11.487347
10.903649	920.375825	11.492365
11.111867	905.110847	11.497383
10.721907	913.806466	11.502400
10.877275	909.006146	11.507418
10.858393	922.198935	11.512435
10.848437	919.007951	11.517453
10.827663	915.361353	11.522471
10.604455	917.106169	11.527488
10.841901	915.723205	11.532506
10.650087	917.896619	11.537523
10.573954	931.059513	11.542541
11.105324	938.871124	11.547559
10.981818	945.301246	11.552576
11.023157	951.482710	11.557594
11.258889	947.928928	11.562611
10.895147	933.111926	11.567629
10.813332	933.268875	11.572647
10.902355	946.348986	11.577664
11.256138	936.525553	11.582682
11.132708	940.615893	11.587699
10.920329	942.162695	11.592717
11.025429	939.147740	11.597735
10.829832	952.455964	11.602752
11.055457	948.004789	11.607770
11.096843	949.666323	11.612787
10.871660	953.130673	11.617805
11.297825	940.438268	11.622823
10.623616	954.840970	11.627840
10.949519	948.481606	11.632858
10.813924	946.845181	11.637875
10.679688	944.104777	11.642893
11.260782	939.512198	11.647911
10.884044	946.928107	11.652928
11.002644	953.971856	11.657946
11.324631	961.811978	11.662963
11.503017	974.264455	11.667981
11.597185	963.020564	11.672999
11.351678	961.679028	11.678016
11.031483	957.801238	11.683034
11.164195	951.409635	11.688051
11.225436	947.144655	11.693069
11.274244	943.916794	11.698087
11.161093	952.774137	11.703104
11.473478	968.169330	11.708122
11.266628	955.935203	11.713139
11.146869	967.176521	11.718157
11.496924	970.950473	11.723175
11.173392	985.795957	11.728192
11.221210	985.974587	11.733210
11.523612	978.672005	11.738227
11.471643	987.008120	11.743245
11.320707	980.008172	11.748263
11.147188	978.618719	11.753280
11.368337	970.143148	11.758298
11.641762	984.811451	11.763315
11.295781	986.946780	11.768333
11.451126	979.320721	11.773351
11.330368	970.461762	11.778368
11.357742	969.831305	11.783386
11.406568	982.786025	11.788403
11.073620	975.346353	11.793421
11.311721	980.917848	11.798439
11.106564	982.646895	11.803456
11.070750	981.126436	11.808474
11.249146	979.260785	11.813491
11.411439	976.682953	11.818509
11.449661	968.198839	11.823527
11.588627	990.157074	11.828544
11.765322	988.643418	11.833562
11.563529	981.143099	11.838579
11.620191	979.683526	11.843597
11.595737	969.534453	11.848615
11.172963	974.864822	11.853632
11.327195	1001.346189	11.858650
11.867319	997.805272	11.863667
11.796802	1006.907922	11.868685
12.070045	997.378817	11.873703
11.915348	997.348236	11.878720
11.739283	985.194812	11.883738
11.834713	974.580917	11.888755
11.725614	976.663714	11.893773
11.850953	975.405553	11.898791
11.904468	974.263772	11.903808
11.766382	974.495167	11.908826
11.801808	964.207482	11.913843
11.690437	972.910827	11.918861
12.023051	964.013952	11.923879
11.612373	968.498365	11.928896
11.472099	967.911555	11.933914
11.848436	965.875816	11.938931
11.293545	973.039532	11.943949
11.611653	978.809384	11.948967
11.684060	992.591182	11.953984
11.742615	994.938354	11.959002
12.088267	1003.476836	11.964019
12.056568	1005.894821	11.969037
11.909805	997.974639	11.974055
11.793587	984.461150	11.979072
11.603911	994.519749	11.984090
12.009773	1005.281384	11.989107
11.706417	1000.997913	11.994125
11.937378	1001.814476	11.999143
11.981286	1008.236247	12.004160
11.859408	1005.841962	12.009178
12.205373	1013.271128	12.014195
11.762615	1017.727003	12.019213
11.874380	1010.654106	12.024231
11.887919	1017.000204	12.029248
11.928252	1012.627260	12.034266
12.250034	1000.119548	12.039283
11.861388	1013.495155	12.044301
11.630719	998.570679	12.049319
12.256421	1004.906932	12.054336
12.137987	1004.922910	12.059354
11.945262	1002.117567	12.064371
11.580808	1004.903877	12.069389
11.590301	1003.395020	12.074407
11.928632	1015.397150	12.079424
12.033174	1013.862940	12.084442
12.294416	1024.742764	12.089459
11.989814	1020.758855	12.094477
12.015601	1020.626412	12.099495
12.316877	1027.426458	12.104512
12.363121	1031.898362	12.109530
12.181892	1019.621768	12.114547
11.998202	1019.655024	12.119565
12.645699	1024.121841	12.124583
12.047502	1019.338555	12.129600
11.823896	1014.373504	12.134618
12.257020	1024.515785	12.139635
12.213283	1030.867614	12.144653
12.634477	1018.402308	12.149671
12.394551	1027.672707	12.154688
12.339313	1016.486927	12.159706
12.355740	1011.145454	12.164723
12.012998	1013.137753	12.169741
12.256690	1023.591412	12.174759
12.494205	1032.596330	12.179776
12.243204	1036.714272	12.184794
12.582019	1038.768129	12.189811
12.317937	1039.185477	12.194829
12.317907	1041.297298	12.199847
11.920310	1037.721012	12.204864
12.206206	1045.575212	12.209882
12.324898	1039.448644	12.214899
12.186249	1058.649364	12.219917
12.368036	1039.251284	12.224935
12.417060	1053.179104	12.229952
12.063024	1040.179595	12.234970
12.495324	1042.352824	12.239987
12.253719	1050.354031	12.245005
12.393622	1049.279058	12.250023
12.150749	1055.387077	12.255040
12.203682	1052.268338	12.260058
12.796910	1055.681703	12.265075
12.788210	1058.851682	12.270093
12.875534	1054.800043	12.275111
12.774383	1035.620941	12.280128
12.831993	1040.671585	12.285146
12.874957	1030.088563	12.290163
12.671926	1042.579917	12.295181
12.479837	1038.174521	12.300199
12.582081	1042.983575	12.305216
12.432410	1033.747923	12.310234
12.694432	1029.779214	12.315251
12.422823	1044.461672	12.320269
12.772262	1040.589520	12.325287
12.915308	1035.072217	12.330304
12.465420	1041.110521	12.335322
12.974263	1035.067882	12.340339
12.769725	1045.073664	12.345357
12.957262	1041.755742	12.350375
13.048739	1034.591516	12.355392
12.779549	1039.567840	12.360410
12.988739	1037.771688	12.365427
12.883444	1041.401059	12.370445
12.886436	1040.205428	12.375463
13.068206	1039.587045	12.380480
12.845032	1028.242621	12.385498
13.199638	1026.080172	12.390515
12.967655	1037.617996	12.395533
12.857222	1031.548977	12.400551
13.158523	1034.818485	12.405568
13.064211	1038.970169	12.410586
13.038080	1009.110919	12.415603
12.894421	1008.883270	12.420621
12.771100	997.231667	12.425639
13.112297	991.544255	12.430656
12.813627	1000.502548	12.435674
12.861735	984.986041	12.440691
13.137669	1011.113509	12.445709
12.890994	1007.088146	12.450727
12.905807	1003.875338	12.455744
12.689915	1019.959951	12.460762
12.937537	1019.691456	12.465779
12.764873	1033.214428	12.470797
12.747297	1034.576316	12.475815
12.616760	1032.267500	12.480832
12.703336	1038.249427	12.485850
12.991712	1038.214316	12.490867
12.807484	1040.651805	12.495885
12.948949	1047.383994	12.500903
13.102669	1026.647277	12.505920
13.110481	1033.087816	12.510938
12.979092	1031.433761	12.515955
13.327807	1031.522712	12.520973
13.223815	1040.169176	12.525991
13.209170	1021.831958	12.531008
13.271832	1021.453697	12.536026
13.057493	1039.633800	12.541043
12.961067	1026.327994	12.546061
13.310724	1042.789568	12.551079
13.384826	1047.328318	12.556096
13.240088	1043.649230	12.561114
13.081074	1032.675242	12.566131
13.372661	1051.300015	12.571149
13.235895	1054.613184	12.576167
13.514243	1038.306726	12.581184
13.353045	1052.575143	12.586202
13.378462	1052.049123	12.591219
13.147763	1040.662633	12.596237
13.294067	1052.459557	12.601255
13.582826	1048.032560	12.606272
13.406731	1054.039203	12.611290
13.434670	1044.924169	12.616307
13.418586	1035.443444	12.621325
13.153311	1037.982895	12.626343
13.490799	1044.911392	12.631360
13.381058	1049.236075	12.636378
13.191498	1055.936567	12.641395
13.072529	1048.814197	12.646413
13.151781	1053.814623	12.651431
13.376698	1051.395300	12.656448
13.404777	1058.915203	12.661466
13.592705	1048.967754	12.666483
13.256017	1060.537265	12.671501
13.447477	1059.859219	12.676519
13.703567	1052.166483	12.681536
13.605632	1051.953321	12.686554
13.701769	1058.706192	12.691571
13.435691	1055.470118	12.696589
13.558301	1057.712045	12.701607
13.531774	1050.702724	12.706624
13.596025	1054.593601	12.711642
13.353743	1044.862501	12.716659
13.404529	1049.764693	12.721677
13.260948	1072.304299	12.726695
13.676258	1078.929249	12.731712
13.853886	1077.913187	12.736730
13.863917	1082.582202	12.741747
13.686559	1084.462744	12.746765
13.394398	1092.773462	12.751783
13.751956	1082.960728	12.756800
13.586766	1088.972865	12.761818
14.127237	1078.560311	12.766835
14.054031	1078.068498	12.771853
13.655124	1069.476477	12.776871
14.060082	1077.802869	12.781888
13.795139	1082.381716	12.786906
14.128323	1066.271253	12.791923
14.173194	1062.334485	12.796941
13.694193	1049.223553	12.801959
13.823583	1040.559399	12.806976
14.036292	1051.233320	12.811994
13.980877	1040.950754	12.817011
13.767179	1035.589437	12.822029
13.815740	1037.823325	12.827047
13.964853	1035.828867	12.832064
13.961631	1041.825045	12.837082
14.103116	1048.209254	12.842099
14.145591	1041.229277	12.847117
13.949097	1026.011771	12.852135
13.891626	1031.240066	12.857152
13.477862	1041.981884	12.862170
14.026675	1051.033779	12.867187
14.489743	1065.401572	12.872205
14.100344	1059.567589	12.877223
14.126538	1061.042895	12.882240
14.346020	1045.881214	12.887258
14.048179	1044.361144	12.892275
14.019516	1042.813910	12.897293
14.041195	1048.587113	12.902311
14.413057	1046.030730	12.907328
14.237678	1044.593555	12.912346
14.254393	1041.677425	12.917363
14.198831	1037.338626	12.922381
13.825234	1050.154976	12.927399
13.878497	1054.483426	12.932416
14.087944	1068.511107	12.937434
14.238475	1071.362498	12.942451
14.378695	1080.300269	12.947469
14.534893	1082.193592	12.952487
14.562010	1068.602413	12.957504
14.296324	1059.048766	12.962522
14.181280	1061.553947	12.967539
14.410010	1057.808612	12.972557
14.116856	1067.305316	12.977575
14.340109	1070.905003	12.982592
14.122421	1082.714667	12.987610
14.061689	1073.494603	12.992627
14.581540	1069.215799	12.997645
14.210794	1084.704908	13.002663
14.436439	1067.516520	13.007680
14.232643	1072.262987	13.012698
14.205359	1080.069566	13.017715
14.298105	1073.207034	13.022733
14.386601	1079.141817	13.027751
14.674804	1070.791899	13.032768
14.778303	1070.205542	13.037786
14.497263	1084.232613	13.042803
14.679694	1081.344790	13.047821
14.274628	1069.685566	13.052839
14.368374	1074.658607	13.057856
14.645263	1071.055681	13.062874
14.289058	1073.094300	13.067891
14.494137	1063.862397	13.072909
14.328895	1085.209924	13.077927
14.298676	1078.709192	13.082944
14.364351	1089.659170	13.087962
14.256112	1105.375349	13.092979
14.902890	1098.230334	13.097997
14.558662	1106.598672	13.103015
14.875139	1098.957933	13.108032
14.628059	1096.494968	13.113050
14.385642	1109.852790	13.118067
14.857352	1102.546379	13.123085
14.832998	1105.912232	13.128103
14.630328	1100.052493	13.133120
14.934172	1107.738824	13.138138
14.678455	1107.871370	13.143155
14.681565	1103.320133	13.148173
14.378350	1110.894022	13.153191
14.864033	1106.891875	13.158208
15.091984	1104.011484	13.163226
14.751251	1108.354083	13.168243
15.097700	1102.027672	13.173261
15.166861	1110.240310	13.178279
14.763485	1106.508294	13.183296
14.772972	1100.240324	13.188314
14.668480	1102.332611	13.193331
15.045313	1099.555747	13.198349
14.592600	1104.779511	13.203367
14.774978	1097.840158	13.208384
14.880438	1098.733167	13.213402
14.412580	1100.840036	13.218419
14.982881	1096.411177	13.223437
15.107334	1113.981728	13.228455
14.984900	1110.836650	13.233472
15.111122	1101.251081	13.238490
14.964289	1108.690088	13.243507
15.345385	1115.350231	13.248525
15.374362	1109.431345	13.253543
15.208674	1101.573479	13.258560
15.387893	1104.188872	13.263578
14.591258	1107.936836	13.268595
14.952573	1091.481987	13.273613
14.886553	1112.523633	13.278631
15.269328	1124.903485	13.283648
15.584418	1122.544632	13.288666
15.350875	1110.377184	13.293683
15.431463	1100.640126	13.298701
15.191971	1101.936149	13.303719
15.430643	1089.486974	13.308736
15.446938	1092.293634	13.313754
14.860212	1101.901265	13.318771
15.104557	1095.159515	13.323789
15.285338	1114.162461	13.328807
15.355187	1125.147399	13.333824
15.356238	1125.620526	13.338842
15.533575	1119.962704	13.343859
15.560271	1119.406948	13.348877
15.207372	1107.216714	13.353895
15.150670	1104.286331	13.358912
15.653783	1121.877373	13.363930
15.515500	1129.393902	13.368947
15.701628	1126.627488	13.373965
15.580276	1114.212596	13.378983
15.370244	1090.580850	13.384000
15.148715	1096.129146	13.389018
15.043332	1119.595434	13.394035
15.397520	1124.430585	13.399053
15.578174	1130.593625	13.404071
15.287366	1123.816696	13.409088
15.509480	1127.874191	13.414106
15.405824	1131.241148	13.419123
15.274107	1124.042516	13.424141
15.720121	1122.933287	13.429159
15.556341	1132.846183	13.434176
15.298730	1127.264566	13.439194
15.392501	1136.016374	13.444211
15.638775	1126.671540	13.449229
15.538655	1141.528278	13.454247
15.806594	1140.997408	13.459264
16.146341	1139.743363	13.464282
15.612560	1122.528271	13.469299
15.787517	1123.655034	13.474317
16.021355	1125.843162	13.479335
15.854116	1134.002963	13.484352
16.019902	1128.363974	13.489370
15.665597	1127.202188	13.494387
16.147956	1124.429531	13.499405
15.752959	1122.301588	13.504423
15.720871	1121.492791	13.509440
16.011416	1127.716791	13.514458
15.712785	1129.931308	13.519475
15.910879	1117.616749	13.524493
15.998358	1119.690108	13.529511
15.827163	1128.121975	13.534528
15.680414	1108.733421	13.539546
15.662456	1117.983332	13.544563
15.893064	1118.072907	13.549581
15.849339	1129.808787	13.554599
15.995031	1145.079366	13.559616
16.284110	1143.036965	13.564634
16.035924	1147.330821	13.569651
15.437623	1128.700814	13.574669
16.268579	1137.167832	13.579687
16.251759	1148.190137	13.584704
16.478427	1137.720952	13.589722
16.010149	1136.006237	13.594739
16.259126	1119.071377	13.599757
16.155544	1127.729828	13.604775
16.298580	1125.729278	13.609792
16.556242	1118.838685	13.614810
16.255155	1122.866516	13.619827
16.147097	1123.049453	13.624845
16.316080	1121.785446	13.629863
16.098030	1120.153575	13.634880
16.018743	1113.934517	13.639898
15.592007	1125.885043	13.644915
16.061915	1133.075708	13.649933
16.311150	1148.171526	13.654951
16.390271	1154.326752	13.659968
16.187195	1146.535859	13.664986
16.081785	1164.638669	13.670003
16.220119	1153.550506	13.675021
16.553025	1152.808930	13.680039
16.078528	1153.524792	13.685056
16.132698	1146.624908	13.690074
16.358744	1163.798470	13.695091
16.382400	1148.140193	13.700109
16.428486	1148.403546	13.705127
16.201779	1148.128015	13.710144
16.318351	1150.622095	13.715162
16.469101	1151.555056	13.720179
16.391028	1139.681924	13.725197
16.495233	1138.027304	13.730215
16.539862	1146.220396	13.735232
16.620489	1139.286226	13.740250
16.464159	1157.615913	13.745267
16.656210	1163.360611	13.750285
16.708377	1161.720689	13.755303
16.320836	1160.691342	13.760320
16.480513	1162.084372	13.765338
16.704532	1179.786356	13.770355
16.679333	1183.478891	13.775373
16.793403	1182.136959	13.780391
16.796509	1182.994729	13.785408
16.989658	1172.135648	13.790426
16.961127	1174.836361	13.795443
17.051362	1155.569781	13.800461
17.020735	1141.103373	13.805479
16.579902	1149.615435	13.810496
16.666095	1134.884686	13.815514
16.511976	1142.871287	13.820531
16.178614	1142.717301	13.825549
16.529008	1161.251005	13.830567
16.730533	1178.069044	13.835584
17.002913	1167.953254	13.840602
16.712050	1183.824673	13.845619
16.740992	1179.230370	13.850637
17.013792	1175.789488	13.855655
16.968306	1182.565817	13.860672
17.134143	1174.626164	13.865690
16.775822	1179.863681	13.870707
16.885129	1173.657520	13.875725
16.896738	1177.525637	13.880743
16.791608	1173.271948	13.885760
17.226984	1164.765198	13.890778
17.009563	1169.170494	13.895795
16.938017	1175.698606	13.900813
17.384148	1170.604129	13.905831
17.011588	1178.661487	13.910848
17.188224	1169.936114	13.915866
17.173404	1167.119843	13.920883
17.060034	1174.397470	13.925901
17.278534	1171.854798	13.930919
17.034557	1168.816395	13.935936
17.292885	1168.547703	13.940954
17.044907	1161.082286	13.945971
16.713179	1169.258660	13.950989
17.333423	1164.504450	13.956007
16.909759	1171.795958	13.961024
17.133928	1176.874823	13.966042
17.357656	1200.423244	13.971059
17.504734	1201.835287	13.976077
17.776798	1185.842657	13.981095
17.470340	1190.693515	13.986112
17.309131	1176.682642	13.991130
17.132220	1175.018774	13.996147
17.075455	1182.671244	14.001165
17.811631	1190.126944	14.006183
17.620767	1197.206593	14.011200
16.978799	1189.101651	14.016218
17.611882	1189.372711	14.021235
17.194729	1191.884340	14.026253
17.649898	1195.667351	14.031271
17.375536	1196.707569	14.036288
17.572679	1192.194112	14.041306
17.646209	1188.703295	14.046323
17.510116	1195.123792	14.051341
17.770754	1198.350653	14.056359
17.627800	1209.127153	14.061376
17.606241	1203.490754	14.066394
17.679450	1195.717162	14.071411
17.435727	1203.101371	14.076429
17.559468	1196.006728	14.081447
17.525104	1197.691238	14.086464
17.854339	1206.648429	14.091482
17.477878	1204.084208	14.096499
17.541027	1196.931477	14.101517
17.994904	1193.137487	14.106535
17.677818	1191.520793	14.111552
17.596941	1197.882174	14.116570
17.062477	1202.990563	14.121587
17.242673	1195.864743	14.126605
17.741100	1216.115917	14.131623
17.639971	1234.724720	14.136640
17.749208	1231.805467	14.141658
18.225726	1231.851256	14.146675
18.221475	1235.590728	14.151693
18.394409	1228.343474	14.156711
17.972319	1210.359345	14.161728
18.114281	1202.995585	14.166746
18.155166	1197.470110	14.171763
18.164619	1186.168808	14.176781
18.385518	1190.165899	14.181799
18.241220	1191.852240	14.186816
18.028773	1180.455348	14.191834
18.450374	1182.654181	14.196851
17.632492	1187.102224	14.201869
17.808486	1187.296677	14.206887
17.597822	1180.510611	14.211904
18.105678	1181.707937	14.216922
17.878784	1186.161057	14.221939
18.323257	1196.933570	14.226957
18.005436	1195.795272	14.231975
18.274313	1204.975791	14.236992
18.382548	1211.521839	14.242010
18.075560	1200.645205	14.247027
17.793696	1213.369573	14.252045
18.159757	1224.064722	14.257063
18.120792	1225.410086	14.262080
18.442988	1221.510703	14.267098
18.370084	1218.968351	14.272115
18.336375	1228.243960	14.277133
18.489334	1223.924972	14.282151
18.423795	1220.078052	14.287168
18.513540	1233.979034	14.292186
18.691665	1221.410644	14.297203
18.796021	1224.297249	14.302221
18.933082	1215.459904	14.307239
18.615545	1205.306557	14.312256
18.405323	1197.212534	14.317274
18.477606	1187.664560	14.322291
18.341648	1196.740938	14.327309
18.374958	1187.753456	14.332327
18.399833	1190.275687	14.337344
18.925070	1209.326340	14.342362
18.573109	1207.147382	14.347379
18.031532	1205.864394	14.352397
18.341950	1208.367193	14.357415
18.636850	1207.046155	14.362432
18.591009	1215.630951	14.367450
18.607559	1218.369884	14.372467
18.427975	1233.150683	14.377485
18.923892	1219.066017	14.382503
18.666996	1220.339338	14.387520
18.667978	1219.646903	14.392538
18.819456	1229.651837	14.397555
18.384467	1223.264384	14.402573
18.528679	1232.515907	14.407591
18.278485	1216.008262	14.412608
18.477259	1234.773577	14.417626
18.814180	1240.352061	14.422643
18.774424	1259.742958	14.427661
19.186675	1248.138467	14.432679
18.835854	1251.223704	14.437696
19.116011	1254.440659	14.442714
19.218542	1245.153755	14.447731
18.989172	1259.396232	14.452749
19.124909	1251.928375	14.457767
19.458154	1237.966623	14.462784
19.299191	1227.542013	14.467802
19.325273	1220.605995	14.472819
19.252271	1214.715533	14.477837
19.335152	1208.500735	14.482855
19.420009	1212.006217	14.487872
19.302831	1226.958560	14.492890
19.134290	1208.793970	14.497907
19.137170	1220.165972	14.502925
19.198954	1204.910724	14.507943
19.271690	1210.252385	14.512960
18.991599	1207.890119	14.517978
18.974759	1204.320152	14.522995
18.995269	1206.463242	14.528013
18.853960	1206.163755	14.533031
18.901867	1214.158143	14.538048
18.837748	1212.292784	14.543066
19.173082	1224.727203	14.548083
19.224878	1238.909027	14.553101
19.197191	1238.742512	14.558119
19.137224	1241.710402	14.563136
19.057466	1249.552702	14.568154
19.525127	1243.633503	14.573171
19.398059	1238.921481	14.578189
19.263849	1234.541104	14.583207
19.330006	1247.944495	14.588224
19.322558	1246.990695	14.593242
19.093848	1233.531792	14.598259
19.312529	1243.434107	14.603277
19.535311	1243.626143	14.608295
19.217373	1238.528991	14.613312
19.416192	1257.227997	14.618330
19.715115	1262.529148	14.623347
19.976870	1267.566601	14.628365
19.761211	1272.157632	14.633383
19.880570	1253.267952	14.638400
19.386554	1248.577005	14.643418
19.711845	1249.846036	14.648435
19.589109	1272.901313	14.653453
19.991684	1262.608653	14.658471
19.972184	1252.579816	14.663488
19.924925	1260.132934	14.668506
20.017611	1235.883305	14.673523
20.174722	1239.581547	14.678541
19.840652	1242.712236	14.683559
19.892316	1232.301431	14.688576
20.129582	1234.708070	14.693594
20.139639	1219.311772	14.698611
19.884020	1244.396544	14.703629
20.034991	1226.879817	14.708647
19.934270	1234.061105	14.713664
19.668929	1240.500618	14.718682
19.739990	1225.492599	14.723699
19.818460	1237.405387	14.728717
19.524717	1230.295479	14.733735
19.743461	1240.102913	14.738752
19.815553	1261.042620	14.743770
20.207534	1262.671050	14.748787
20.092741	1255.252465	14.753805
19.888349	1271.063432	14.758823
19.917898	1266.186366	14.763840
19.780430	1271.510824	14.768858
19.971020	1256.903828	14.773875
19.969344	1263.736330	14.778893
19.842494	1246.613473	14.783911
20.070294	1257.006147	14.788928
19.995738	1270.952028	14.793946
20.301711	1277.970276	14.798963
20.270770	1290.045259	14.803981
20.581018	1294.084100	14.808999
20.518758	1294.485816	14.814016
20.002665	1280.645684	14.819034
20.653775	1286.362394	14.824051
20.519239	1284.064042	14.829069
20.547250	1280.563406	14.834087
20.160124	1266.812588	14.839104
20.004092	1281.189402	14.844122
20.476323	1287.423792	14.849139
20.574349	1285.917597	14.854157
20.522282	1286.133206	14.859175
20.645800	1290.506601	14.864192
20.638493	1294.743962	14.869210
20.678559	1287.919170	14.874227
20.745221	1294.198737	14.879245
20.658999	1283.226122	14.884263
20.641618	1269.350035	14.889280
20.465623	1270.425570	14.894298
20.517476	1273.714504	14.899315
20.737535	1287.252710	14.904333
20.556100	1291.802467	14.909351
20.555139	1283.882645	14.914368
20.410166	1300.257165	14.919386
20.833901	1288.741284	14.924403
20.547221	1283.006955	14.929421
21.000272	1283.020802	14.934439
21.256731	1278.918126	14.939456
21.103716	1283.636780	14.944474
21.183124	1273.785257	14.949491
21.035703	1293.551222	14.954509
20.816738	1285.348771	14.959527
21.084851	1292.197913	14.964544
20.642641	1291.971965	14.969562
20.902387	1283.525272	14.974579
20.639323	1287.146722	14.979597
20.538023	1292.344165	14.984615
20.901190	1279.460544	14.989632
20.617235	1292.483705	14.994650
20.910278	1278.724988	14.999667
21.169852	1281.982551	15.004685
20.942353	1276.857057	15.009703
21.139317	1273.256663	15.014720
20.963314	1288.330187	15.019738
20.907780	1289.031143	15.024755
20.900973	1305.861705	15.029773
21.180174	1312.758033	15.034791
21.341392	1312.778380	15.039808
21.391402	1315.045529	15.044826
21.349355	1322.965874	15.049843
21.622432	1314.348678	15.054861
21.517452	1317.491713	15.059879
21.535099	1298.541829	15.064896
21.224363	1284.751406	15.069914
21.359237	1293.215645	15.074931
21.366112	1291.542059	15.079949
21.406113	1303.252032	15.084967
21.826534	1300.893854	15.089984
21.146681	1295.172139	15.095002
21.594063	1301.870025	15.100019
21.764474	1304.489861	15.105037
21.502331	1301.310753	15.110055
21.460302	1285.045956	15.115072
21.651141	1280.238281	15.120090
21.474931	1290.537923	15.125107
21.545621	1303.431238	15.130125
21.645571	1315.223427	15.135143
21.998640	1303.975081	15.140160
21.521823	1306.273785	15.145178
21.865335	1304.419190	15.150195
21.518734	1285.206529	15.155213
21.550116	1299.805306	15.160231
21.876984	1310.771128	15.165248
21.921145	1308.867788	15.170266
21.990892	1314.607167	15.175283
22.123192	1291.053167	15.180301
21.706001	1284.385621	15.185319
21.663268	1270.776480	15.190336
21.885580	1274.547015	15.195354
21.705793	1270.238914	15.200371
21.715391	1284.465936	15.205389
21.621457	1293.440951	15.210407
21.991360	1306.594227	15.215424
22.109233	1316.659685	15.220442
22.079087	1307.501936	15.225459
22.098387	1307.665010	15.230477
22.028042	1314.276435	15.235495
22.276498	1302.275408	15.240512
21.902862	1307.495816	15.245530
22.007731	1305.158882	15.250547
22.439443	1303.495982	15.255565
22.292691	1322.565122	15.260583
22.362013	1321.956258	15.265600
21.830408	1320.166564	15.270618
22.488945	1310.828087	15.275635
22.674859	1315.391740	15.280653
22.390257	1295.377791	15.285671
22.111794	1285.135465	15.290688
22.254510	1287.124532	15.295706
22.133340	1296.995261	15.300723
22.682078	1299.530532	15.305741
22.495617	1307.558384	15.310759
22.128724	1280.627542	15.315776
22.242901	1296.294171	15.320794
22.050207	1300.415931	15.325811
22.100769	1300.257151	15.330829
22.181126	1307.404809	15.335847
22.259425	1307.181218	15.340864
22.171500	1308.322308	15.345882
21.960878	1311.317862	15.350899
22.629850	1305.877899	15.355917
22.639060	1320.373681	15.360935
22.786208	1317.555022	15.365952
22.858769	1318.077943	15.370970
22.793579	1300.030990	15.375987
22.762512	1297.354761	15.381005
22.385324	1313.675951	15.386023
22.597278	1300.082956	15.391040
22.660273	1321.457060	15.396058
22.665528	1340.038569	15.401075
22.944514	1338.683345	15.406093
22.838047	1327.866384	15.411111
23.133535	1331.706915	15.416128
22.793311	1324.444825	15.421146
22.851303	1327.651272	15.426163
23.229501	1335.869646	15.431181
23.294404	1316.207894	15.436199
23.377351	1301.312585	15.441216
22.690225	1307.871820	15.446234
22.745995	1302.683958	15.451251
22.803737	1290.693790	15.456269
22.546056	1298.870198	15.461287
22.849314	1316.684622	15.466304
22.768171	1324.715745	15.471322
22.715075	1324.265871	15.476339
22.934392	1319.860704	15.481357
22.915465	1328.988478	15.486375
23.002116	1324.693017	15.491392
23.165377	1322.891629	15.496410
23.149138	1330.809289	15.501427
23.025249	1323.501017	15.506445
23.038766	1331.471231	15.511463
23.148072	1342.439176	15.516480
23.366358	1355.174501	15.521498
23.162042	1352.109628	15.526515
23.233872	1355.328753	15.531533
23.359022	1359.775510	15.536551
23.424255	1350.422078	15.541568
23.751475	1359.907572	15.546586
23.587995	1353.775941	15.551603
23.725790	1327.620158	15.556621
23.502077	1325.333583	15.561639
23.747496	1328.111083	15.566656
23.780199	1321.953343	15.571674
23.425473	1315.999965	15.576691
23.741946	1312.839983	15.581709
23.550105	1317.575890	15.586727
23.676778	1326.707945	15.591744
23.680594	1318.542075	15.596762
23.409959	1325.046662	15.601779
23.241693	1310.591424	15.606797
23.190697	1329.846295	15.611815
23.694767	1340.303002	15.616832
23.424268	1347.872978	15.621850
23.717892	1356.127579	15.626867
23.847315	1347.425064	15.631885
23.468071	1354.460729	15.636903
23.702519	1350.973397	15.641920
23.669307	1353.771753	15.646938
23.658330	1346.404068	15.651955
23.815142	1346.745571	15.656973
23.668183	1355.000746	15.661991
23.839456	1350.278752	15.667008
23.800206	1360.954571	15.672026
24.040822	1377.367210	15.677043
24.300131	1365.457635	15.682061
23.970321	1385.644749	15.687079
24.236749	1380.115398	15.692096
24.315116	1372.160377	15.697114
23.936295	1366.155063	15.702131
24.460230	1353.830164	15.707149
24.259014	1361.006664	15.712167
24.374277	1352.141745	15.717184
24.518815	1337.386006	15.722202
24.374618	1339.229016	15.727219
24.390138	1334.629209	15.732237
24.126058	1349.954717	15.737255
24.363506	1347.008548	15.742272
24.259366	1344.107215	15.747290
24.105326	1348.150562	15.752307
24.330809	1348.074474	15.757325
23.929927	1348.158777	15.762343
24.196077	1366.891075	15.767360
24.486346	1364.338283	15.772378
24.446073	1373.702651	15.777395
24.217908	1370.531494	15.782413
24.311683	1375.787463	15.787431
24.605557	1380.488195	15.792448
24.646562	1374.466643	15.797466
24.546847	1371.217967	15.802483
24.595829	1367.415660	15.807501
24.446886	1366.595259	15.812519
24.490720	1370.592529	15.817536
24.426908	1362.852911	15.822554
24.620924	1375.488932	15.827571
24.582824	1365.348937	15.832589
24.647679	1373.098711	15.837607
24.764545	1371.661038	15.842624
24.708606	1381.238797	15.847642
24.634184	1397.203784	15.852659
25.243780	1396.869168	15.857677
24.942176	1397.522419	15.862695
25.059420	1385.022215	15.867712
25.147065	1372.545612	15.872730
24.923324	1375.386676	15.877747
25.339473	1354.083585	15.882765
25.239751	1361.653689	15.887783
25.160756	1361.342130	15.892800
25.314784	1352.870158	15.897818
25.001368	1356.162394	15.902835
25.262711	1363.743492	15.907853
25.278666	1357.847722	15.912871
25.198859	1350.821088	15.917888
25.348824	1342.465526	15.922906
24.892712	1348.981485	15.927923
25.102635	1349.912553	15.932941
25.306503	1354.933423	15.937959
25.286180	1354.415149	15.942976
25.088654	1342.648201	15.947994
25.258807	1351.069837	15.953011
25.600294	1341.169057	15.958029
25.483406	1350.270519	15.963047
25.041045	1345.805225	15.968064
25.305542	1340.660601	15.973082
25.175797	1346.990952	15.978099
25.462675	1346.400655	15.983117
25.466406	1354.575620	15.988135
25.388970	1359.531380	15.993152
25.394109	1366.845215	15.998170
25.476936	1389.643696	16.003187
25.813784	1385.501333	16.008205
25.787853	1391.254583	16.013223
25.754480	1387.303107	16.018240
25.879020	1379.325494	16.023258
25.609710	1370.465660	16.028275
25.876615	1369.620430	16.033293
25.660001	1359.752229	16.038311
25.498013	1373.610303	16.043328
25.655623	1380.057528	16.048346
25.504069	1385.099353	16.053363
25.499231	1380.192112	16.058381
25.564584	1382.418749	16.063399
25.545732	1386.347849	16.068416
25.651626	1380.237039	16.073434
25.661160	1388.520890	16.078451
26.109224	1388.482026	16.083469
26.138297	1383.691604	16.088487
25.907164	1388.192916	16.093504
26.100658	1383.820144	16.098522
25.750297	1390.954582	16.103539
25.854123	1403.553568	16.108557
26.165575	1395.929456	16.113575
26.152157	1408.153977	16.118592
26.580499	1408.753915	16.123610
26.361455	1405.427918	16.128627
26.331842	1398.004832	16.133645
26.342135	1398.145579	16.138663
26.221912	1406.894524	16.143680
26.467234	1395.520236	16.148698
26.342541	1400.234246	16.153715
26.467233	1386.304461	16.158733
26.345464	1368.787572	16.163751
26.432586	1380.946054	16.168768
26.515569	1386.662607	16.173786
26.375690	1386.729562	16.178803
26.188166	1392.229240	16.183821
26.271757	1388.758956	16.188839
26.107968	1390.720746	16.193856
26.426404	1390.954253	16.198874
26.367815	1389.923474	16.203891
26.365281	1395.193594	16.208909
26.376439	1393.387811	16.213927
26.522535	1394.712054	16.218944
26.591583	1388.161721	16.223962
26.501920	1390.980827	16.228979
26.654143	1393.828259	16.233997
26.709311	1410.534931	16.239015
26.591776	1412.985863	16.244032
26.747032	1420.458159	16.249050
26.862234	1430.762880	16.254067
26.846402	1428.843655	16.259085
27.130251	1426.170473	16.264103
26.895455	1438.444789	16.269120
27.439152	1420.667890	16.274138
27.252538	1425.423239	16.279155
26.805493	1402.934754	16.284173
26.890179	1397.168734	16.289191
26.945582	1409.704281	16.294208
27.410888	1419.786200	16.299226
27.236724	1401.545550	16.304243
27.227285	1404.245511	16.309261
27.076385	1385.089151	16.314279
27.042910	1392.417056	16.319296
27.047672	1400.939466	16.324314
27.495251	1418.170785	16.329331
27.475757	1410.356507	16.334349
27.198354	1399.130203	16.339367
26.947431	1398.965543	16.344384
27.106717	1403.509217	16.349402
26.854707	1428.515159	16.354419
26.959559	1434.156077	16.359437
27.132260	1417.739922	16.364455
27.368690	1419.521027	16.369472
27.599662	1414.315786	16.374490
27.473569	1420.831168	16.379507
27.695984	1422.233145	16.384525
27.648866	1410.178924	16.389543
27.418770	1422.007234	16.394560
27.441235	1409.427805	16.399578
27.272257	1424.972482	16.404595
27.542396	1433.537068	16.409613
27.766946	1451.095203	16.414631
27.461196	1456.433559	16.419648
27.833780	1445.518258	16.424666
27.771727	1448.462519	16.429683
27.765057	1451.099637	16.434701
28.425115	1444.895846	16.439719
28.093908	1438.895034	16.444736
28.218096	1433.997159	16.449754
27.974196	1419.053990	16.454771
27.970878	1413.751659	16.459789
28.120314	1412.240695	16.464807
27.618869	1423.854041	16.469824
27.742784	1424.135637	16.474842
27.926727	1443.457717	16.479859
27.990917	1451.262948	16.484877
27.916574	1438.178893	16.489895
28.105549	1448.287404	16.494912
27.905236	1460.445817	16.499930
27.872461	1440.965578	16.504947
27.956361	1444.020740	16.509965
28.181122	1439.007831	16.514983
28.035847	1451.698212	16.520000
28.107256	1434.897650	16.525018
28.278809	1438.977755	16.530035
28.055900	1455.173218	16.535053
28.367047	1457.236626	16.540071
28.427895	1474.875573	16.545088
28.601027	1470.523856	16.550106
28.416294	1467.659043	16.555123
28.649227	1463.933779	16.560141
29.100418	1445.500574	16.565159
28.734449	1440.669328	16.570176
28.564099	1430.953453	16.575194
28.704980	1435.093933	16.580211
28.327618	1438.307001	16.585229
28.583974	1428.020878	16.590247
28.113356	1429.163611	16.595264
28.822023	1438.958511	16.600282
28.813107	1461.845478	16.605299
29.082378	1460.921321	16.610317
28.838013	1427.289557	16.615335
28.854891	1435.255137	16.620352
28.718465	1429.451441	16.625370
29.184289	1432.399005	16.630387
28.691244	1434.775596	16.635405
28.871734	1424.044790	16.640423
29.298138	1456.519147	16.645440
28.841075	1433.624059	16.650458
28.894243	1439.374491	16.655475
28.831412	1450.491612	16.660493
29.278715	1459.248954	16.665511
29.266627	1458.650191	16.670528
29.434543	1455.844215	16.675546
29.002442	1443.765607	16.680563
29.368961	1442.679336	16.685581
29.153034	1439.393165	16.690599
28.922272	1440.782248	16.695616
29.037004	1455.298707	16.700634
29.198758	1457.061058	16.705651
28.985976	1449.326923	16.710669
29.120012	1463.522329	16.715687
29.034209	1454.450058	16.720704
28.876484	1462.797018	16.725722
29.204590	1461.103198	16.730739
29.071190	1475.191648	16.735757
29.508567	1486.273176	16.740775
29.555509	1475.391000	16.745792
29.519044	1478.030685	16.750810
29.508445	1485.984298	16.755827
29.512306	1489.194410	16.760845
29.878255	1485.159993	16.765863
29.950062	1489.373705	16.770880
29.720459	1492.502729	16.775898
30.049146	1474.670760	16.780915
29.715197	1480.767032	16.785933
29.995196	1485.842679	16.790951
30.085745	1478.507754	16.795968
30.153111	1470.694836	16.800986
29.907445	1449.523025	16.806003
29.854205	1457.869249	16.811021
30.109093	1457.440316	16.816039
29.887495	1459.566569	16.821056
29.721860	1461.778246	16.826074
30.069858	1469.683220	16.831091
30.036143	1479.599055	16.836109
29.836176	1478.833924	16.841127
30.001847	1484.516575	16.846144
30.191216	1480.680412	16.851162
30.481812	1483.688041	16.856179
30.001395	1473.601780	16.861197
30.179625	1473.924985	16.866215
30.165366	1473.437984	16.871232
30.293140	1480.909733	16.876250
30.338026	1468.374379	16.881267
30.699202	1480.792140	16.886285
30.602439	1471.158358	16.891303
30.671744	1479.163126	16.896320
30.468611	1481.285739	16.901338
30.359816	1476.848146	16.906355
30.341395	1480.441023	16.911373
30.677426	1462.927694	16.916391
30.300772	1468.876118	16.921408
30.313804	1480.762117	16.926426
30.546686	1466.946451	16.931443
30.205303	1472.543424	16.936461
30.446370	1482.884066	16.941479
30.526001	1475.561181	16.946496
30.371004	1479.455528	16.951514
30.506360	1476.075280	16.956531
30.463376	1504.486510	16.961549
30.786710	1500.489442	16.966567
30.855503	1504.184826	16.971584
30.513779	1514.111036	16.976602
30.935374	1506.195672	16.981619
30.826446	1508.634765	16.986637
30.876546	1498.054572	16.991655
30.993555	1500.857062	16.996672
30.687348	1503.700164	17.001690
30.892278	1495.678108	17.006707
30.807311	1504.093175	17.011725
30.959140	1505.637122	17.016743
31.013037	1515.689072	17.021760
31.022894	1526.027996	17.026778
31.629471	1514.726779	17.031795
31.623053	1523.656367	17.036813
31.727656	1520.461680	17.041831
31.658974	1497.525935	17.046848
31.342667	1490.873709	17.051866
31.806225	1484.867511	17.056883
31.769201	1490.261852	17.061901
31.523487	1481.874369	17.066919
31.796993	1488.845331	17.071936
31.438038	1490.225488	17.076954
31.758185	1482.159993	17.081971
31.530087	1489.679337	17.086989
31.929200	1489.127567	17.092007
31.872821	1484.427406	17.097024
31.879366	1478.167641	17.102042
31.880601	1475.820842	17.107059
31.711668	1483.025130	17.112077
31.681111	1488.475284	17.117095
31.675873	1490.531736	17.122112
31.601269	1487.060017	17.127130
31.773538	1490.378503	17.132147
31.788591	1482.036302	17.137165
31.535407	1479.563261	17.142183
31.485721	1484.748696	17.147200
31.512006	1483.866856	17.152218
31.971355	1478.833669	17.157235
31.745638	1473.209258	17.162253
31.908355	1497.994239	17.167271
32.301973	1508.948780	17.172288
31.922653	1504.626151	17.177306
32.219427	1503.999375	17.182323
32.175109	1511.861933	17.187341
32.143383	1507.637748	17.192359
31.934485	1513.404943	17.197376
31.894467	1512.844845	17.202394
31.955539	1510.753275	17.207411
31.725936	1508.473354	17.212429
31.957175	1509.229672	17.217447
32.065850	1521.482133	17.222464
31.899489	1542.591926	17.227482
32.336298	1546.598702	17.232499
32.191227	1553.889620	17.237517
32.491282	1545.114707	17.242535
32.494758	1549.226947	17.247552
32.348382	1546.413647	17.252570
32.700950	1543.906430	17.257587
32.412017	1545.368709	17.262605
32.232185	1545.880204	17.267623
32.603966	1555.271065	17.272640
32.782112	1581.475893	17.277658
33.110124	1574.214462	17.282675
33.170201	1571.723886	17.287693
32.799860	1560.787001	17.292711
33.125721	1533.259997	17.297728
32.804086	1536.901616	17.302746
32.953061	1540.547937	17.307763
32.924203	1548.826606	17.312781
33.219170	1546.808571	17.317799
33.223450	1536.351460	17.322816
33.202054	1540.000544	17.327834
33.537831	1540.047747	17.332851
33.073175	1544.533568	17.337869
32.699932	1543.714991	17.342887
33.259523	1545.756054	17.347904
33.131752	1541.456798	17.352922
33.445109	1541.458303	17.357939
33.356816	1544.420696	17.362957
33.423215	1549.836545	17.367975
33.312664	1542.016580	17.372992
33.089199	1544.739927	17.378010
33.300149	1556.212028	17.383027
33.528300	1554.339662	17.388045
33.247238	1567.079345	17.393063
33.508792	1569.910908	17.398080
33.251641	1574.080789	17.403098
33.446234	1570.281530	17.408115
33.502260	1563.757090	17.413133
33.470643	1570.812365	17.418151
33.533687	1570.184059	17.423168
33.213594	1568.310569	17.428186
33.711198	1590.203115	17.433203
33.763017	1595.138181	17.438221
34.248229	1598.932469	17.443239
34.237679	1576.929207	17.448256
33.845149	1577.672677	17.453274
33.966554	1565.552104	17.458291
33.975056	1570.632689	17.463309
33.764308	1566.166057	17.468327
33.964487	1565.667630	17.473344
34.177748	1591.442119	17.478362
34.500596	1586.286000	17.483379
34.213892	1578.007982	17.488397
34.084615	1567.723098	17.493415
34.343756	1554.184278	17.498432
34.016767	1561.802666	17.503450
34.235513	1588.169279	17.508467
34.162317	1590.508988	17.513485
34.233037	1593.511247	17.518503
34.663113	1588.337015	17.523520
34.341398	1594.003804	17.528538
34.494330	1575.760461	17.533555
34.734040	1592.618309	17.538573
34.786167	1596.452082	17.543591
34.632584	1575.308772	17.548608
34.227979	1574.636304	17.553626
34.334729	1573.912400	17.558643
34.510405	1587.014954	17.563661
34.274214	1594.076688	17.568679
34.359710	1582.638133	17.573696
34.477920	1588.711099	17.578714
34.522937	1582.971838	17.583731
34.707936	1590.850472	17.588749
34.447443	1594.994338	17.593767
34.887170	1585.371030	17.598784
34.455953	1589.414186	17.603802
34.956124	1605.832795	17.608819
35.095478	1609.435649	17.613837
34.766035	1617.590427	17.618855
35.222079	1608.677706	17.623872
35.052796	1624.674352	17.628890
35.275242	1608.242098	17.633907
35.369621	1605.598228	17.638925
35.388741	1603.810393	17.643943
35.457340	1590.953933	17.648960
35.244998	1603.839948	17.653978
35.265410	1597.551272	17.658995
35.626079	1605.987426	17.664013
35.423016	1597.820953	17.669031
35.383281	1579.980068	17.674048
35.183700	1572.896757	17.679066
35.202775	1589.298012	17.684083
35.696566	1595.677768	17.689101
35.489116	1614.504181	17.694119
35.440992	1603.652387	17.699136
35.310637	1622.339511	17.704154
35.844737	1622.005755	17.709171
35.514747	1610.959422	17.714189
35.369916	1608.027760	17.719207
35.358574	1603.754122	17.724224
35.022085	1610.186454	17.729242
35.396219	1611.253178	17.734259
35.615799	1636.675954	17.739277
35.725788	1634.225539	17.744295
35.769842	1644.569914	17.749312
35.877338	1640.492153	17.754330
35.997221	1637.991683	17.759347
36.253706	1645.330249	17.764365
36.048480	1631.539005	17.769383
36.205651	1636.440928	17.774400
36.503815	1635.628311	17.779418
36.142059	1626.295671	17.784435
36.433003	1630.063811	17.789453
36.030533	1629.647058	17.794471
36.615968	1625.610188	17.799488
36.251305	1627.039523	17.804506
36.479355	1635.180915	17.809523
36.759690	1631.182652	17.814541
36.294043	1626.346561	17.819559
36.465321	1620.684047	17.824576
36.747962	1614.779734	17.829594
36.588035	1624.862761	17.834611
36.794490	1623.761005	17.839629
36.385487	1632.923700	17.844647
36.725584	1607.996849	17.849664
36.883664	1619.789114	17.854682
36.608010	1626.551515	17.859699
36.800421	1618.435806	17.864717
36.627049	1622.821748	17.869735
36.647902	1622.540331	17.874752
36.923467	1615.595975	17.879770
36.795609	1627.319173	17.884787
37.067365	1618.834687	17.889805
36.830271	1632.661513	17.894823
36.819986	1622.019372	17.899840
36.852927	1624.087246	17.904858
36.744182	1627.833059	17.909875
37.070976	1619.566812	17.914893
36.353297	1628.142599	17.919911
36.751995	1633.959021	17.924928
37.123090	1647.266903	17.929946
36.828889	1650.340893	17.934963
37.240221	1646.553825	17.939981
37.438529	1649.850328	17.944999
37.288164	1650.530952	17.950016
37.107528	1644.622879	17.955034
36.979947	1648.296622	17.960051
37.379317	1641.335535	17.965069
37.290167	1645.273759	17.970087
36.970490	1648.481274	17.975104
37.359199	1664.030873	17.980122
37.685159	1670.699190	17.985139
37.881337	1679.131468	17.990157
37.892955	1682.351952	17.995175
37.896100	1679.972526	18.000192
38.029502	1689.417034	18.005210
38.016094	1685.732032	18.010227
37.810796	1650.110093	18.015245
37.671124	1647.304720	18.020263
37.735376	1661.381148	18.025280
37.807406	1669.713675	18.030298
37.575101	1669.925023	18.035315
37.866294	1669.505438	18.040333
38.078594	1682.757122	18.045351
37.811366	1677.704979	18.050368
38.136234	1678.718833	18.055386
37.968491	1680.932070	18.060403
38.200171	1679.444888	18.065421
37.884215	1679.871217	18.070439
38.272303	1676.973508	18.075456
38.138124	1673.792661	18.080474
38.206572	1696.454424	18.085491
38.333864	1695.129552	18.090509
38.194200	1700.259858	18.095527
38.411936	1697.963065	18.100544
38.398252	1697.874536	18.105562
38.269981	1710.540275	18.110579
38.510458	1701.447008	18.115597
38.311843	1709.107238	18.120615
38.473919	1697.678972	18.125632
38.690989	1692.260804	18.130650
38.654547	1703.762874	18.135667
38.670426	1693.534422	18.140685
38.645274	1704.145755	18.145703
38.771607	1724.620884	18.150720
38.876647	1730.305969	18.155738
38.977223	1738.305311	18.160755
39.273444	1728.681812	18.165773
39.291635	1736.886870	18.170791
39.059694	1714.925113	18.175808
39.260660	1702.116757	18.180826
38.806827	1697.808944	18.185843
39.101640	1705.259498	18.190861
39.319098	1725.004692	18.195879
39.529958	1728.679409	18.200896
39.617890	1697.977035	18.205914
39.030914	1700.836454	18.210931
39.218318	1708.257718	18.215949
39.407345	1723.395151	18.220967
39.688170	1735.509898	18.225984
39.831067	1713.721409	18.231002
39.297811	1704.173586	18.236019
39.455566	1711.374580	18.241037
39.139241	1722.849106	18.246055
39.554711	1717.252490	18.251072
39.861541	1717.307431	18.256090
39.815748	1726.446573	18.261107
40.125346	1725.486803	18.266125
39.991231	1718.710089	18.271143
39.732660	1708.802735	18.276160
40.088796	1704.092796	18.281178
39.608216	1694.526630	18.286195
39.706407	1707.412394	18.291213
39.610055	1711.771265	18.296231
39.643982	1721.883141	18.301248
39.935631	1727.454524	18.306266
39.680892	1718.098829	18.311283
39.790349	1713.914044	18.316301
39.708880	1722.746518	18.321319
39.937414	1729.844299	18.326336
40.094981	1739.237605	18.331354
40.022792	1740.048998	18.336371
39.968609	1731.380544	18.341389
40.432784	1742.598365	18.346407
40.158863	1744.500848	18.351424
40.474130	1733.682404	18.356442
40.042797	1743.600146	18.361459
40.073175	1738.425781	18.366477
40.336307	1752.871350	18.371495
40.179243	1760.519622	18.376512
40.457289	1768.580783	18.381530
40.513165	1765.148456	18.386547
40.812400	1760.501047	18.391565
41.018083	1758.350315	18.396583
40.812302	1760.015384	18.401600
40.853749	1756.826755	18.406618
40.532341	1760.736862	18.411635
41.172212	1764.533979	18.416653
41.203617	1762.573248	18.421671
41.039503	1758.964504	18.426688
41.176967	1755.266167	18.431706
41.103950	1759.873726	18.436723
41.446180	1757.798844	18.441741
41.417479	1757.255171	18.446759
41.098532	1773.013150	18.451776
41.314036	1759.481755	18.456794
40.921728	1765.584830	18.461811
41.059017	1758.653419	18.466829
41.146554	1761.931641	18.471847
41.389128	1762.065697	18.476864
41.430212	1759.110368	18.481882
41.320899	1760.533537	18.486899
41.492692	1752.825844	18.491917
41.575159	1766.965493	18.496935
41.700348	1774.552958	18.501952
41.848910	1772.796462	18.506970
41.705134	1776.205422	18.511987
41.941340	1770.729149	18.517005
41.969901	1769.261745	18.522023
41.412658	1767.752186	18.527040
41.625974	1771.207438	18.532058
41.552085	1778.407967	18.537075
41.843489	1773.227262	18.542093
41.982814	1776.882910	18.547111
41.784441	1781.945394	18.552128
41.980374	1769.455496	18.557146
41.755524	1786.021664	18.562163
41.785845	1776.165335	18.567181
42.209285	1786.798451	18.572199
41.901671	1797.463414	18.577216
42.269266	1806.237473	18.582234
42.105954	1819.215357	18.587251
42.331014	1819.502094	18.592269
42.432123	1815.568831	18.597287
42.241066	1822.263013	18.602304
42.425713	1810.023542	18.607322
42.247644	1823.107006	18.612339
42.432903	1812.166110	18.617357
42.680755	1816.069749	18.622375
42.553311	1816.349981	18.627392
42.627270	1803.640670	18.632410
42.447751	1813.515663	18.637427
42.780639	1807.160502	18.642445
42.907774	1805.443761	18.647463
42.343561	1815.762403	18.652480
42.575345	1810.946617	18.657498
42.558807	1832.031261	18.662515
42.800441	1832.639241	18.667533
43.533197	1819.704134	18.672551
43.370845	1829.320029	18.677568
43.833681	1829.228141	18.682586
43.434722	1813.607924	18.687603
43.311037	1805.011931	18.692621
43.576025	1786.768914	18.697639
43.529025	1800.914439	18.702656
43.483620	1797.384484	18.707674
43.240236	1791.481016	18.712691
43.283161	1798.452432	18.717709
43.307033	1791.691306	18.722727
43.345818	1789.357150	18.727744
43.318389	1786.886117	18.732762
43.634710	1814.854926	18.737779
43.556318	1824.742346	18.742797
43.840974	1810.400354	18.747815
43.675703	1808.541992	18.752832
44.076248	1814.131038	18.757850
43.839932	1827.400293	18.762867
44.018483	1815.816281	18.767885
43.801696	1810.306005	18.772903
43.956612	1825.949318	18.777920
44.050119	1814.462226	18.782938
43.943038	1811.547118	18.787955
44.162623	1815.362525	18.792973
44.264982	1813.670741	18.797991
43.959523	1819.795111	18.803008
44.232729	1811.356141	18.808026
44.342424	1806.815032	18.813043
43.979142	1811.849862	18.818061
43.992076	1808.308296	18.823079
44.206212	1818.473320	18.828096
44.102675	1816.227632	18.833114
43.896315	1820.671831	18.838131
44.069200	1831.024369	18.843149
44.036297	1837.163739	18.848167
43.980766	1848.658444	18.853184
44.322583	1839.905791	18.858202
44.376813	1850.096473	18.863219
44.296937	1846.654872	18.868237
44.677296	1855.808305	18.873255
44.685173	1871.057306	18.878272
44.677841	1865.158104	18.883290
44.984510	1867.696866	18.888307
45.243326	1863.895977	18.893325
45.150562	1872.033625	18.898343
45.207412	1857.590469	18.903360
45.276298	1863.378222	18.908378
45.572546	1857.546167	18.913395
45.463999	1856.532469	18.918413
45.672856	1834.959263	18.923431
45.340935	1832.847365	18.928448
45.437918	1818.001397	18.933466
45.640526	1827.196981	18.938483
45.306223	1825.198261	18.943501
45.746440	1822.824532	18.948519
45.382065	1830.780689	18.953536
45.139562	1827.033718	18.958554
45.152614	1825.858014	18.963571
45.192242	1827.969688	18.968589
45.534335	1848.052280	18.973607
45.799131	1845.684703	18.978624
46.060872	1853.031555	18.983642
46.029049	1851.176330	18.988659
45.722627	1841.584835	18.993677
46.045904	1825.957252	18.998695
45.672028	1833.366812	19.003712
45.728553	1845.167174	19.008730
45.894554	1854.509163	19.013747
45.350602	1853.824475	19.018765
45.800533	1851.039338	19.023783
45.614597	1855.690386	19.028800
45.892812	1851.747136	19.033818
45.899976	1865.532232	19.038835
46.076940	1888.785730	19.043853
46.258439	1879.732809	19.048871
46.199374	1892.763993	19.053888
46.387510	1888.598834	19.058906
46.185474	1890.300105	19.063923
46.202582	1897.285673	19.068941
46.393143	1884.040349	19.073959
46.349783	1885.676622	19.078976
46.524898	1884.071419	19.083994
46.497450	1891.164534	19.089011
46.501358	1910.836999	19.094029
46.879909	1904.617349	19.099047
46.860130	1906.449707	19.104064
46.896723	1910.936060	19.109082
47.115427	1912.594771	19.114099
46.842200	1921.378149	19.119117
46.991489	1911.532779	19.124135
46.821135	1905.926419	19.129152
46.824835	1906.837866	19.134170
46.907747	1903.139257	19.139187
46.714219	1914.522576	19.144205
47.183003	1911.474300	19.149223
47.277017	1934.510102	19.154240
47.134754	1928.943378	19.159258
47.091803	1933.773359	19.164275
47.237696	1941.791300	19.169293
47.459119	1935.518279	19.174311
47.196815	1934.744727	19.179328
47.411357	1936.035072	19.184346
47.805380	1927.675473	19.189363
47.582909	1921.867898	19.194381
47.672240	1926.565202	19.199399
47.557725	1933.002517	19.204416
47.328151	1934.142849	19.209434
47.758327	1938.407493	19.214451
47.808811	1947.917235	19.219469
48.089143	1958.576678	19.224487
48.139475	1966.727340	19.229504
48.220153	1951.153695	19.234522
48.365990	1959.257866	19.239539
48.507400	1953.721807	19.244557
48.485245	1961.698440	19.249575
48.422837	1953.723277	19.254592
48.372846	1950.144837	19.259610
48.545321	1937.600811	19.264627
48.266186	1927.036741	19.269645
48.226770	1920.787738	19.274663
48.319966	1939.342644	19.279680
48.634794	1942.564646	19.284698
48.813463	1950.521472	19.289715
48.719961	1948.646707	19.294733
48.685876	1938.771392	19.299751
48.914442	1940.118075	19.304768
48.606151	1941.299169	19.309786
48.737094	1940.177000	19.314803
48.813037	1955.305398	19.319821
48.757708	1951.548331	19.324839
48.477175	1961.222613	19.329856
48.563412	1956.939247	19.334874
48.818494	1957.532807	19.339891
48.795408	1953.883194	19.344909
48.966943	1953.892194	19.349927
48.815591	1961.139267	19.354944
48.577046	1988.266908	19.359962
49.040068	1983.147135	19.364979
48.754468	1983.012800	19.369997
49.089209	1980.863544	19.375015
48.675346	1984.307929	19.380032
49.154443	2009.199508	19.385050
49.545050	2016.832200	19.390067
49.575687	2022.711955	19.395085
49.692650	2013.206082	19.400103
50.004668	2020.054595	19.405120
49.714263	2020.520406	19.410138
50.125203	1998.302416	19.415155
50.414443	2003.418240	19.420173
50.422665	2001.613264	19.425191
50.216267	1991.476457	19.430208
49.877211	1975.681232	19.435226
50.141472	1968.410470	19.440243
50.019434	1977.659398	19.445261
50.093086	1989.265327	19.450279
50.361732	1992.838639	19.455296
50.295659	2001.862410	19.460314
50.643489	2004.684915	19.465331
50.496237	1994.272611	19.470349
50.333251	1973.361977	19.475367
50.756284	1972.883005	19.480384
50.047837	1987.408450	19.485402
50.436903	1977.668283	19.490419
49.978302	1995.797366	19.495437
50.136290	1991.852297	19.500455
50.717091	1986.328846	19.505472
50.343742	1989.743705	19.510490
50.838068	1988.070783	19.515507
50.635931	1991.187888	19.520525
50.588501	1993.265945	19.525543
50.780294	2012.180790	19.530560
50.635701	2024.128293	19.535578
51.152496	2021.159062	19.540595
50.850795	2032.378668	19.545613
51.084022	2022.217023	19.550631
51.248816	2018.453483	19.555648
50.859285	2036.846371	19.560666
51.304147	2029.365437	19.565683
51.180049	2026.155098	19.570701
51.148683	2026.466696	19.575719
51.093703	2027.901971	19.580736
51.254812	2045.935990	19.585754
51.818907	2049.198312	19.590771
51.841885	2052.696300	19.595789
52.140944	2041.667939	19.600807
52.480161	2019.712928	19.605824
52.247201	2017.705702	19.610842
52.193660	1999.792603	19.615859
52.192123	1999.737692	19.620877
51.982252	2000.582873	19.625895
52.231733	1991.548374	19.630912
51.698933	2004.455398	19.635930
52.049677	2007.954720	19.640947
52.193743	2005.076806	19.645965
52.054218	2010.932712	19.650983
52.286729	1993.909071	19.656000
51.812673	2008.105871	19.661018
52.404278	2008.476122	19.666035
52.322611	2003.291248	19.671053
51.916614	2004.025939	19.676071
52.046918	2001.968725	19.681088
52.126082	2008.404180	19.686106
52.530123	2014.133654	19.691123
52.417601	2032.489028	19.696141
52.476099	2032.721019	19.701159
52.783802	2024.812993	19.706176
52.550972	2026.106414	19.711194
52.450068	2025.904750	19.716211
52.671248	2038.449435	19.721229
52.461071	2037.849923	19.726247
52.696813	2041.366091	19.731264
52.300321	2056.312447	19.736282
52.615985	2059.869344	19.741299
52.778283	2062.432192	19.746317
52.842444	2063.304723	19.751335
53.185785	2061.173325	19.756352
52.951276	2085.993204	19.761370
52.974392	2085.783643	19.766387
53.143585	2081.717222	19.771405
53.312107	2084.707156	19.776423
53.676550	2090.982916	19.781440
53.317694	2088.325483	19.786458
53.543753	2083.941425	19.791475
53.385726	2081.902322	19.796493
53.139356	2081.771542	19.801511
54.146349	2092.152941	19.806528
53.914187	2106.738362	19.811546
53.870477	2106.039691	19.816563
54.247082	2108.835022	19.821581
54.326192	2104.861624	19.826599
54.305806	2088.217632	19.831616
54.137285	2081.093524	19.836634
54.148943	2076.624830	19.841651
54.081586	2079.006950	19.846669
53.764809	2095.575454	19.851687
54.343313	2091.007377	19.856704
54.185092	2102.296622	19.861722
54.290028	2104.977018	19.866739
54.191455	2094.883934	19.871757
54.137190	2097.460332	19.876775
54.673002	2100.668290	19.881792
54.448924	2107.453870	19.886810
54.596849	2089.830575	19.891827
54.690312	2107.985873	19.896845
54.827458	2119.730018	19.901863
55.006578	2121.607873	19.906880
55.120699	2122.773110	19.911898
55.297039	2125.685192	19.916915
54.851606	2111.442112	19.921933
55.016535	2108.750872	19.926951
54.869836	2110.211744	19.931968
54.937923	2117.218316	19.936986
55.059860	2124.662409	19.942003
55.209918	2120.023011	19.947021
55.178541	2113.354331	19.952039
55.416350	2124.556695	19.957056
55.435251	2115.153964	19.962074
55.472081	2116.423696	19.967091
55.328652	2114.519172	19.972109
55.326993	2117.192777	19.977127
55.258087	2109.202860	19.982144
54.992597	2130.089112	19.987162
55.356082	2141.002633	19.992179
55.705509	2156.682835	19.997197
55.433746	2158.458053	20.002215
55.599907	2156.443904	20.007232
55.809586	2157.171342	20.012250
55.912195	2155.429878	20.017267
56.087013	2168.279942	20.022285
56.022301	2178.736144	20.027303
56.387053	2164.522309	20.032320
56.398885	2169.965502	20.037338
56.361665	2171.831677	20.042355
56.367706	2179.689796	20.047373
56.427787	2174.664103	20.052391
56.273981	2182.121116	20.057408
56.570870	2182.979013	20.062426
56.565884	2167.801164	20.067443
56.769758	2176.053325	20.072461
56.325062	2182.945074	20.077479
56.933338	2174.934157	20.082496
56.562006	2178.767192	20.087514
56.754013	2178.610225	20.092531
56.865439	2176.229758	20.097549
56.415929	2183.101044	20.102567
56.990826	2198.321625	20.107584
57.079001	2206.050840	20.112602
57.105603	2195.792529	20.117619
56.945201	2196.710247	20.122637
57.059373	2207.019399	20.127655
57.579251	2186.374343	20.132672
57.062726	2192.402646	20.137690
57.266515	2187.431738	20.142707
57.659947	2191.130921	20.147725
57.412364	2196.007593	20.152743
57.512894	2196.464315	20.157760
57.753420	2198.149765	20.162778
57.409776	2217.259632	20.167795
58.127260	2220.567506	20.172813
58.026334	2233.431106	20.177831
58.138164	2217.720363	20.182848
58.227528	2230.325960	20.187866
58.172567	2218.694217	20.192883
57.878741	2205.563108	20.197901
57.794095	2221.102131	20.202919
58.077570	2212.718131	20.207936
58.140458	2209.162707	20.212954
57.955886	2213.951420	20.217971
58.147533	2214.342892	20.222989
58.452536	2219.763049	20.228007
58.694157	2218.200361	20.233024
58.502936	2213.986394	20.238042
58.135264	2217.037992	20.243059
58.629022	2215.308650	20.248077
58.477992	2241.767210	20.253095
58.685433	2240.167259	20.258112
58.841869	2253.530429	20.263130
58.415861	2247.677237	20.268147
58.897975	2233.384106	20.273165
59.059045	2251.808104	20.278183
58.881121	2247.158895	20.283200
59.092050	2252.039142	20.288218
58.978172	2240.966090	20.293235
59.253155	2241.000512	20.298253
58.890523	2249.449861	20.303271
59.237588	2260.137263	20.308288
59.403787	2275.878176	20.313306
59.166591	2269.145614	20.318323
59.224305	2274.065554	20.323341
59.320026	2284.672075	20.328359
59.512898	2273.035359	20.333376
59.775316	2273.668267	20.338394
59.648144	2269.700571	20.343411
59.961943	2268.474348	20.348429
59.631715	2269.476428	20.353447
59.725215	2257.058767	20.358464
59.978644	2268.768062	20.363482
59.986333	2278.581513	20.368499
59.944597	2286.017695	20.373517
59.661191	2304.468357	20.378535
60.416666	2294.742832	20.383552
60.703218	2293.786640	20.388570
60.584534	2290.311395	20.393587
60.678100	2281.926656	20.398605
60.131638	2284.969429	20.403623
60.475923	2277.298912	20.408640
60.349892	2287.816301	20.413658
60.230900	2285.443974	20.418675
60.433660	2283.309400	20.423693
60.652171	2288.151401	20.428711
60.832267	2280.613320	20.433728
60.704889	2281.407484	20.438746
60.867487	2306.103833	20.443763
60.873935	2311.756021	20.448781
61.095647	2315.245242	20.453799
61.078644	2316.686079	20.458816
61.463701	2323.232326	20.463834
60.959078	2324.245316	20.468851
61.182446	2319.184326	20.473869
60.883661	2321.825379	20.478887
60.924647	2325.065355	20.483904
61.277614	2339.853100	20.488922
61.304555	2346.250873	20.493939
61.650867	2342.188775	20.498957
61.980080	2343.051970	20.503975
61.936853	2339.074123	20.508992
62.121412	2344.806725	20.514010
61.938348	2340.308916	20.519027
62.115417	2336.403911	20.524045
61.734654	2333.842567	20.529063
61.903259	2345.624201	20.534080
61.983813	2352.823491	20.539098
62.049572	2344.282892	20.544115
62.150818	2339.208614	20.549133
62.037633	2342.661260	20.554151
62.169699	2336.992564	20.559168
62.283724	2354.526101	20.564186
62.350891	2367.382703	20.569203
62.639395	2363.155165	20.574221
62.679187	2370.113185	20.579239
62.471202	2376.030342	20.584256
62.642874	2359.636387	20.589274
62.734862	2368.270696	20.594291
62.829758	2364.551100	20.599309
62.825639	2365.545947	20.604327
62.929390	2361.127696	20.609344
62.859063	2353.696902	20.614362
62.863828	2365.396775	20.619379
63.290690	2376.016153	20.624397
63.078757	2380.918290	20.629415
63.259271	2381.016942	20.634432
63.706911	2380.187265	20.639450
63.425147	2390.100386	20.644467
63.848408	2377.879299	20.649485
63.361671	2383.893896	20.654503
63.318116	2387.090772	20.659520
63.664426	2374.135017	20.664538
63.318260	2397.685555	20.669555
63.251892	2383.301636	20.674573
63.216956	2381.070118	20.679591
63.612711	2385.724800	20.684608
63.975159	2413.182977	20.689626
63.945306	2420.100760	20.694643
64.413867	2424.142678	20.699661
64.013375	2427.299536	20.704679
64.094814	2422.030487	20.709696
64.022290	2426.831063	20.714714
63.712316	2423.841893	20.719731
63.858902	2416.205945	20.724749
63.993138	2432.053080	20.729767
64.885718	2436.243422	20.734784
64.974382	2434.972506	20.739802
64.752010	2440.742468	20.744819
65.188683	2432.690294	20.749837
65.314022	2426.725060	20.754855
65.376284	2411.402796	20.759872
65.336155	2398.596502	20.764890
65.103474	2391.370064	20.769907
65.633410	2380.325160	20.774925
65.455413	2389.764867	20.779943
65.227973	2391.767022	20.784960
65.719560	2381.911637	20.789978
65.430530	2385.022117	20.794995
65.441493	2386.376258	20.800013
65.257239	2391.624587	20.805031
65.396426	2389.162142	20.810048
65.788341	2386.923665	20.815066
65.478650	2400.351392	20.820083
65.248031	2389.683126	20.825101
65.399723	2403.884159	20.830119
65.357333	2401.181462	20.835136
65.906166	2420.010842	20.840154
65.810182	2428.557752	20.845171
66.011155	2421.828695	20.850189
65.764955	2421.728982	20.855207
66.120383	2425.172315	20.860224
66.012449	2425.434767	20.865242
65.971815	2432.789347	20.870259
66.151213	2434.265452	20.875277
66.381274	2448.328190	20.880295
66.290956	2439.069680	20.885312
66.276089	2437.272208	20.890330
66.139525	2446.892099	20.895347
66.267298	2458.544159	20.900365
66.431385	2482.900607	20.905383
66.428168	2482.530048	20.910400
66.644241	2488.215569	20.915418
66.345759	2488.793153	20.920435
66.686127	2492.799780	20.925453
66.652467	2510.254558	20.930471
66.963794	2501.666208	20.935488
67.493314	2508.430182	20.940506
67.343011	2502.934062	20.945523
67.170800	2501.061409	20.950541
67.296424	2501.025639	20.955559
67.332854	2499.089377	20.960576
67.590297	2493.606978	20.965594
67.715463	2503.487571	20.970611
67.822703	2507.141610	20.975629
68.267478	2507.175927	20.980647
67.851264	2496.302839	20.985664
68.205903	2497.769283	20.990682
68.132956	2493.031593	20.995699
67.679657	2495.423619	21.000717
67.894257	2500.481870	21.005735
67.982990	2509.284305	21.010752
68.311032	2514.165951	21.015770
68.046194	2517.179553	21.020787
67.799809	2507.181486	21.025805
68.231746	2519.035282	21.030823
68.097060	2522.944642	21.035840
68.540753	2515.079245	21.040858
68.350489	2524.341545	21.045875
68.405336	2542.195094	21.050893
68.727202	2535.449751	21.055911
68.865105	2542.567413	21.060928
69.143105	2539.964494	21.065946
69.009649	2542.644598	21.070963
69.013598	2541.908506	21.075981
69.318467	2545.018904	21.080999
68.813775	2544.191283	21.086016
69.352078	2533.842680	21.091034
69.465903	2544.372770	21.096051
69.142525	2544.507253	21.101069
69.514095	2538.448534	21.106087
69.383980	2533.841531	21.111104
69.802235	2530.183218	21.116122
69.585865	2535.117827	21.121139
69.647483	2526.815593	21.126157
69.744971	2540.158833	21.131175
69.793820	2571.872003	21.136192
69.820923	2567.852360	21.141210
69.909932	2564.154357	21.146227
70.070964	2567.072400	21.151245
70.401277	2570.745100	21.156263
70.293205	2561.038296	21.161280
70.161059	2561.732875	21.166298
70.090009	2564.930591	21.171315
70.167288	2555.794307	21.176333
70.307151	2562.805362	21.181351
70.294651	2581.268867	21.186368
70.634814	2580.828769	21.191386
70.838767	2594.713486	21.196403
70.668763	2598.712161	21.201421
71.172648	2592.824459	21.206439
71.003880	2586.045609	21.211456
71.238637	2591.096229	21.216474
71.003714	2589.478795	21.221491
71.266831	2585.583129	21.226509
71.385504	2585.272933	21.231527
71.494743	2581.133814	21.236544
71.269066	2585.539299	21.241562
71.437454	2589.715505	21.246579
71.152058	2590.164952	21.251597
71.253956	2579.341221	21.256615
71.436175	2589.270705	21.261632
71.706516	2597.325112	21.266650
71.585556	2608.733759	21.271667
71.382208	2623.822356	21.276685
71.841273	2621.298552	21.281703
71.948943	2612.540656	21.286720
72.212992	2605.009607	21.291738
72.032146	2608.262481	21.296755
72.028953	2609.443991	21.301773
72.472252	2602.828544	21.306791
72.090479	2603.986791	21.311808
72.207841	2607.889166	21.316826
72.288623	2631.285851	21.321843
72.122335	2639.191578	21.326861
72.926191	2629.066338	21.331879
72.853818	2629.178633	21.336896
72.943640	2635.698806	21.341914
72.602808	2629.198749	21.346931
72.848941	2635.776945	21.351949
73.030661	2627.704796	21.356967
72.677444	2640.286427	21.361984
73.001060	2633.763969	21.367002
72.816016	2620.163767	21.372019
72.692129	2643.000623	21.377037
73.191289	2641.419745	21.382055
72.675890	2663.154857	21.387072
72.981737	2649.849081	21.392090
73.284146	2667.191420	21.397107
73.441336	2673.393012	21.402125
73.613263	2683.022699	21.407143
73.521955	2684.795910	21.412160
73.764082	2683.455523	21.417178
73.800233	2683.216438	21.422195
73.514082	2688.301989	21.427213
73.986200	2684.452467	21.432231
73.673555	2714.734799	21.437248
73.912897	2716.023475	21.442266
74.194507	2706.692323	21.447283
74.255649	2716.921410	21.452301
74.166379	2708.611729	21.457319
74.190108	2707.796381	21.462336
74.614984	2729.419907	21.467354
75.022891	2735.737567	21.472371
75.063601	2746.398769	21.477389
75.481950	2732.444442	21.482407
75.241664	2721.772033	21.487424
75.326258	2706.007620	21.492442
75.290504	2690.383971	21.497459
75.310339	2703.100060	21.502477
75.165560	2702.579079	21.507495
75.218744	2703.242645	21.512512
75.215960	2701.578178	21.517530
75.558161	2700.610996	21.522547
75.477417	2720.719325	21.527565
75.765645	2716.628148	21.532583
75.989174	2718.031638	21.537600
76.279969	2713.232199	21.542618
76.141348	2694.156429	21.547635
75.611679	2690.756289	21.552653
75.900807	2684.347377	21.557671
75.948648	2704.872210	21.562688
76.006182	2706.577130	21.567706
76.023391	2700.059609	21.572723
75.782875	2703.090485	21.577741
76.437950	2701.234244	21.582759
76.252439	2700.736134	21.587776
76.142686	2715.192062	21.592794
76.257111	2716.872623	21.597811
76.531810	2739.004813	21.602829
76.868648	2737.899939	21.607847
76.597606	2746.159628	21.612864
77.006250	2745.644434	21.617882
77.176079	2738.106843	21.622899
77.101905	2744.125053	21.627917
77.125470	2746.420995	21.632935
77.043901	2746.792279	21.637952
77.030474	2741.539190	21.642970
77.374252	2733.735468	21.647987
76.839965	2739.234461	21.653005
77.267958	2745.335825	21.658023
77.096915	2758.212235	21.663040
77.023813	2758.791165	21.668058
77.769244	2749.777417	21.673075
77.360450	2764.193047	21.678093
77.490024	2754.369297	21.683111
77.517927	2769.171015	21.688128
77.322838	2788.907795	21.693146
77.836648	2801.084091	21.698163
77.657266	2801.156987	21.703181
77.910002	2789.155873	21.708199
78.333954	2799.477418	21.713216
78.233196	2807.616091	21.718234
78.287837	2810.524597	21.723251
78.375145	2813.227713	21.728269
78.345043	2807.800594	21.733287
78.620433	2825.393627	21.738304
78.251632	2821.821212	21.743322
78.427234	2823.981417	21.748339
78.825710	2844.921309	21.753357
78.979581	2838.352015	21.758375
79.099166	2839.212085	21.763392
79.235838	2833.263325	21.768410
79.393550	2839.318842	21.773427
79.140638	2841.089642	21.778445
79.056036	2837.468686	21.783463
79.366875	2836.651161	21.788480
79.375534	2841.815993	21.793498
79.618708	2859.254552	21.798515
79.799110	2857.325163	21.803533
79.592810	2863.516820	21.808551
79.836896	2849.045932	21.813568
80.149371	2859.742616	21.818586
80.362350	2852.336811	21.823603
80.493478	2856.062179	21.828621
80.994052	2860.961093	21.833639
80.933371	2852.893845	21.838656
80.419973	2848.665818	21.843674
80.443151	2853.138126	21.848691
80.416991	2854.139599	21.853709
80.943385	2850.761757	21.858727
80.831452	2852.617919	21.863744
80.663924	2853.485279	21.868762
80.738246	2846.927158	21.873779
80.673115	2857.687419	21.878797
80.759405	2855.573589	21.883815
80.855831	2854.637956	21.888832
80.693798	2846.226451	21.893850
81.142477	2857.251793	21.898867
80.773691	2879.722790	21.903885
80.980939	2880.367205	21.908903
81.459299	2879.811354	21.913920
81.200961	2873.582196	21.918938
81.305135	2888.254894	21.923955
81.408917	2911.473013	21.928973
81.950317	2902.218495	21.933991
82.007186	2902.071256	21.939008
81.693585	2906.115390	21.944026
81.858181	2917.325508	21.949043
81.995664	2908.242845	21.954061
82.171413	2915.592999	21.959079
82.013865	2931.228636	21.964096
81.991278	2939.218640	21.969114
82.431616	2947.305374	21.974131
82.195299	2938.872236	21.979149
82.174242	2935.321068	21.984167
82.562651	2945.134430	21.989184
82.746138	2954.434041	21.994202
82.939405	2952.097016	21.999219
83.001556	2958.258524	22.004237
83.627197	2950.480950	22.009255
83.669305	2951.077462	22.014272
83.595436	2938.821946	22.019290
83.579497	2917.022183	22.024307
83.547259	2915.783804	22.029325
83.346236	2911.747439	22.034343
83.737922	2907.059612	22.039360
83.491477	2916.831016	22.044378
83.764018	2917.129616	22.049395
83.486270	2925.676324	22.054413
83.603210	2939.452900	22.059431
84.046556	2945.532910	22.064448
83.990905	2947.651821	22.069466
84.181465	2934.471936	22.074483
83.914176	2940.207184	22.079501
84.003759	2938.513256	22.084519
84.235733	2938.269761	22.089536
83.860906	2944.444419	22.094554
84.404449	2966.615578	22.099571
84.346886	2970.358768	22.104589
84.441452	2970.972990	22.109607
84.403650	2969.579232	22.114624
84.272291	2979.875735	22.119642
84.702104	2990.244076	22.124659
84.848227	2998.285756	22.129677
84.807072	2996.565002	22.134695
84.737987	2994.232742	22.139712
84.973781	3008.555075	22.144730
85.524958	3020.437191	22.149747
85.431278	3027.385871	22.154765
85.576771	3023.344577	22.159783
85.845301	3020.822670	22.164800
86.070260	3017.536727	22.169818
86.224372	3009.976800	22.174835
85.890202	3012.737394	22.179853
86.030818	3015.131353	22.184871
86.130288	3013.722782	22.189888
86.167338	3017.213349	22.194906
86.105446	3013.521278	22.199923
86.188351	3013.044549	22.204941
86.272853	3009.192466	22.209959
86.486068	3013.207841	22.214976
86.585355	3026.705137	22.219994
86.568799	3031.279729	22.225011
86.626161	3041.837599	22.230029
86.245757	3050.728100	22.235047
86.660085	3046.408526	22.240064
86.468084	3044.596948	22.245082
86.677382	3058.044598	22.250099
86.875200	3069.172567	22.255117
87.251120	3072.802421	22.260135
87.535424	3080.092984	22.265152
87.211034	3086.158578	22.270170
87.485069	3075.300151	22.275187
87.510364	3077.202560	22.280205
87.739977	3082.133329	22.285223
88.035944	3084.793353	22.290240
87.730128	3097.057685	22.295258
88.092271	3094.535257	22.300275
88.249511	3094.323795	22.305293
88.184412	3097.715120	22.310311
88.834831	3092.176237	22.315328
88.367628	3094.876547	22.320346
88.409604	3092.812920	22.325363
88.633874	3090.576654	22.330381
88.600656	3085.097591	22.335399
88.778146	3070.740648	22.340416
89.079620	3088.908790	22.345434
89.137154	3067.405721	22.350451
89.125149	3074.625957	22.355469
89.375858	3075.580907	22.360487
89.260248	3067.734428	22.365504
89.132667	3069.438482	22.370522
89.252459	3063.000705	22.375539
89.368307	3065.083813	22.380557
89.052197	3063.366754	22.385575
89.095025	3068.916556	22.390592
89.293653	3075.004380	22.395610
89.580124	3085.695676	22.400627
89.814873	3102.884729	22.405645
89.712749	3114.673302	22.410663
89.881610	3100.670898	22.415680
89.773416	3115.932433	22.420698
89.538331	3107.523014	22.425715
89.906819	3109.386040	22.430733
89.888662	3130.059740	22.435751
90.137716	3136.069178	22.440768
89.782643	3135.508129	22.445786
89.954866	3141.853092	22.450803
90.166518	3155.240990	22.455821
90.256878	3164.776190	22.460839
90.738628	3166.441377	22.465856
90.980440	3173.884279	22.470874
91.387157	3178.888174	22.475891
91.399928	3177.188803	22.480909
91.593881	3192.271748	22.485927
91.943556	3173.672169	22.490944
92.230808	3159.972188	22.495962
92.004560	3137.850969	22.500979
92.021510	3136.498148	22.505997
92.152081	3136.628091	22.511015
92.398236	3135.586994	22.516032
92.315857	3142.579920	22.521050
92.571566	3127.698593	22.526067
92.777614	3130.819536	22.531085
92.177393	3121.020873	22.536103
92.381282	3112.783002	22.541120
92.769742	3116.830863	22.546138
92.412468	3109.738057	22.551155
92.487585	3114.385713	22.556173
92.582628	3121.917408	22.561191
92.610268	3126.946131	22.566208
92.516382	3129.749321	22.571226
92.706374	3132.391827	22.576243
92.965791	3127.475796	22.581261
92.634601	3134.923209	22.586279
92.202297	3141.336963	22.591296
92.582654	3153.209615	22.596314
92.962829	3168.222397	22.601331
93.002257	3178.288452	22.606349
92.769281	3189.573519	22.611367
93.353863	3197.633401	22.616384
93.668031	3206.123003	22.621402
93.437206	3218.600232	22.626419
93.489055	3217.479428	22.631437
93.419473	3214.622816	22.636455
93.651910	3216.241806	22.641472
93.786417	3240.939961	22.646490
94.141570	3235.036046	22.651507
94.481768	3240.025363	22.656525
94.265426	3236.917412	22.661543
94.427982	3241.061688	22.666560
94.710400	3247.095577	22.671578
94.634657	3257.389767	22.676595
94.799376	3263.982079	22.681613
95.076191	3264.513049	22.686631
95.327712	3256.937299	22.691648
95.217059	3254.611474	22.696666
95.064017	3271.035673	22.701683
95.364038	3251.671776	22.706701
95.254896	3249.282317	22.711719
95.304979	3254.337688	22.716736
95.415209	3258.577622	22.721754
95.396996	3250.714956	22.726771
95.513808	3269.152403	22.731789
95.532436	3287.201770	22.736807
95.754118	3292.399661	22.741824
95.787961	3297.572689	22.746842
96.206357	3289.351641	22.751859
95.969243	3292.588758	22.756877
95.931008	3310.610148	22.761895
96.092526	3321.736030	22.766912
95.908621	3322.588011	22.771930
96.318623	3319.770635	22.776947
96.503292	3333.028501	22.781965
96.140663	3347.392554	22.786983
96.707765	3342.838208	22.792000
96.877887	3341.883282	22.797018
96.846715	3361.287407	22.802035
97.161844	3365.469891	22.807053
96.870328	3371.943546	22.812071
97.295144	3369.264657	22.817088
97.239878	3367.930048	22.822106
97.456143	3367.346627	22.827123
97.976681	3386.598989	22.832141
98.319643	3394.091425	22.837159
98.304529	3399.978083	22.842176
98.518675	3380.663255	22.847194
98.277336	3375.668476	22.852211
98.592890	3356.311724	22.857229
98.255167	3356.784797	22.862247
98.492486	3372.643817	22.867264
98.551849	3381.448059	22.872282
98.695349	3393.165154	22.877299
98.808572	3388.740125	22.882317
98.802053	3390.508854	22.887335
98.631521	3381.589015	22.892352
98.470336	3379.179003	22.897370
98.793568	3381.264893	22.902387
98.893120	3388.649123	22.907405
99.032076	3409.475974	22.912423
98.870982	3407.564757	22.917440
99.539806	3414.274621	22.922458
99.105175	3421.006589	22.927475
99.525362	3428.847302	22.932493
99.567133	3445.225320	22.937511
99.950128	3427.686464	22.942528
99.879060	3437.253625	22.947546
99.817803	3438.634162	22.952563
100.371389	3441.220184	22.957581
100.572026	3450.964109	22.962599
100.396227	3454.473017	22.967616
100.739103	3458.287557	22.972634
100.941399	3457.885574	22.977651
101.039116	3456.921347	22.982669
101.136343	3460.833171	22.987687
101.046269	3457.215729	22.992704
101.202494	3450.928070	22.997722
101.257634	3457.546446	23.002739
101.522341	3444.635372	23.007757
101.362570	3452.800277	23.012775
100.995693	3456.411231	23.017792
101.904780	3458.478671	23.022810
101.521227	3446.646759	23.027827
101.751025	3450.690611	23.032845
101.591967	3450.779047	23.037863
101.629190	3447.016164	23.042880
101.574548	3436.147229	23.047898
101.353728	3461.117834	23.052915
101.945578	3466.479814	23.057933
101.922137	3474.169054	23.062951
101.870626	3478.592074	23.067968
102.335994	3490.500545	23.072986
102.127473	3512.419202	23.078003
102.288668	3504.963377	23.083021
102.439733	3506.175371	23.088039
102.464662	3509.273563	23.093056
102.682298	3519.343857	23.098074
103.008069	3533.180549	23.103091
102.923258	3538.125231	23.108109
102.987585	3544.501181	23.113127
103.182937	3544.446801	23.118144
103.464675	3557.258898	23.123162
103.399692	3571.598383	23.128179
103.515732	3550.824745	23.133197
103.593396	3571.341073	23.138215
103.427508	3557.921133	23.143232
103.626819	3574.133097	23.148250
103.995493	3580.531606	23.153267
104.342908	3585.748585	23.158285
104.246723	3594.250696	23.163303
104.226687	3588.829513	23.168320
104.212242	3579.708177	23.173338
104.186327	3598.144008	23.178355
104.472663	3609.716010	23.183373
104.580276	3612.842687	23.188391
104.706087	3612.250582	23.193408
105.147704	3611.814956	23.198426
105.270169	3637.601567	23.203443
105.331766	3627.442038	23.208461
105.315022	3632.935744	23.213479
105.191064	3643.124768	23.218496
105.814576	3638.065343	23.223514
105.547036	3642.855999	23.228531
105.891177	3635.546655	23.233549
106.000551	3647.773916	23.238567
105.990646	3669.621393	23.243584
106.238547	3666.919719	23.248602
106.224496	3664.834959	23.253619
106.202972	3668.982602	23.258637
106.267341	3676.885781	23.263655
106.410436	3665.055262	23.268672
106.729651	3652.579896	23.273690
106.625293	3680.777310	23.278707
106.922470	3686.109712	23.283725
106.788721	3692.685777	23.288743
107.054254	3685.852002	23.293760
107.511349	3673.425097	23.298778
107.594909	3689.463393	23.303795
107.405656	3689.493826	23.308813
107.744485	3687.693670	23.313831
107.539542	3686.688888	23.318848
107.346797	3696.462537	23.323866
107.454268	3703.624346	23.328883
107.605319	3714.089239	23.333901
107.779615	3705.555548	23.338919
108.042116	3713.178758	23.343936
108.663872	3706.342806	23.348954
108.339263	3723.807263	23.353971
108.460952	3735.189239	23.358989
108.898676	3744.802440	23.364007
108.302476	3741.223682	23.369024
108.866898	3733.161346	23.374042
108.835735	3736.964532	23.379059
108.911829	3737.600735	23.384077
108.936323	3734.997384	23.389095
108.903151	3754.567687	23.394112
109.212891	3743.414702	23.399130
109.330277	3772.449671	23.404147
109.321913	3769.379688	23.409165
109.608198	3766.413776	23.414183
109.784506	3767.238149	23.419200
109.760371	3764.847163	23.424218
109.756406	3761.154790	23.429235
109.840182	3764.783083	23.434253
110.309583	3776.339921	23.439271
110.047683	3787.523111	23.444288
110.417168	3786.671833	23.449306
110.637169	3790.632747	23.454323
110.390001	3785.853369	23.459341
110.479456	3781.514047	23.464359
110.913788	3803.907610	23.469376
111.005885	3811.148782	23.474394
110.819895	3821.495814	23.479411
111.074242	3811.582667	23.484429
111.310398	3805.061181	23.489447
111.112590	3809.141139	23.494464
111.529629	3819.573963	23.499482
111.661867	3839.783984	23.504499
111.865010	3852.432143	23.509517
112.008327	3840.272313	23.514535
111.941155	3845.519696	23.519552
111.876014	3845.145360	23.524570
111.693096	3856.562010	23.529587
112.042772	3855.833297	23.534605
112.644553	3861.792608	23.539623
112.431230	3875.065914	23.544640
112.807962	3875.330391	23.549658
112.889656	3873.844363	23.554675
112.561902	3869.663722	23.559693
113.020972	3870.169718	23.564711
112.903854	3879.847519	23.569728
113.181782	3890.189988	23.574746
113.067933	3898.095562	23.579763
113.076965	3894.111633	23.584781
113.312607	3891.235958	23.589799
112.852456	3911.451830	23.594816
113.542739	3914.361813	23.599834
113.789102	3927.685586	23.604851
113.817253	3929.720309	23.609869
114.012755	3939.637049	23.614887
114.032031	3968.477960	23.619904
114.183150	3961.356662	23.624922
114.359125	3966.829271	23.629939
114.487479	3961.440134	23.634957
114.642791	3966.414567	23.639975
114.508610	3977.771283	23.644992
115.088570	3980.548322	23.650010
115.227704	3973.775467	23.655027
115.479866	3977.362205	23.660045
115.142724	3975.311499	23.665063
115.201903	3971.682660	23.670080
115.465584	3972.446149	23.675098
115.468629	3980.079686	23.680115
115.501779	4002.848891	23.685133
115.788963	3997.264593	23.690151
115.452040	4004.740137	23.695168
115.638597	4010.084631	23.700186
115.964971	4026.227645	23.705203
116.033278	4024.036311	23.710221
116.424574	4030.872623	23.715239
116.451561	4033.717422	23.720256
116.585797	4027.689473	23.725274
116.664928	4025.955815	23.730291
116.741364	4034.665871	23.735309
116.948469	4020.964992	23.740327
117.159573	4042.553237	23.745344
117.318124	4037.853596	23.750362
117.506468	4046.854233	23.755379
117.521998	4048.928460	23.760397
117.756458	4043.718225	23.765415
117.721880	4045.378669	23.770432
118.182157	4040.897683	23.775450
117.899071	4039.950673	23.780467
118.302247	4044.059737	23.785485
118.345647	4026.809007	23.790503
118.141288	4034.758741	23.795520
118.510243	4039.829397	23.800538
118.318978	4041.615734	23.805555
118.052801	4057.033830	23.810573
118.476795	4059.816970	23.815591
118.406559	4075.427911	23.820608
118.758299	4094.814170	23.825626
118.658931	4103.038333	23.830643
118.717587	4099.885554	23.835661
119.126605	4099.599404	23.840679
119.147172	4121.078292	23.845696
119.158005	4127.725929	23.850714
119.480431	4127.598582	23.855731
119.692384	4134.227950	23.860749
119.929664	4137.155741	23.865767
119.836308	4153.126106	23.870784
119.990984	4165.114390	23.875802
120.181625	4160.461775	23.880819
120.087774	4161.596963	23.885837
120.712199	4158.738498	23.890855
120.300780	4191.921643	23.895872
120.882485	4182.225442	23.900890
120.994752	4178.635423	23.905907
121.209149	4195.880235	23.910925
121.227721	4182.214305	23.915943
120.963974	4183.128738	23.920960
121.217788	4193.450197	23.925978
121.858866	4196.536877	23.930995
121.561882	4204.550429	23.936013
121.865394	4202.233588	23.941031
121.630171	4212.728390	23.946048
121.639207	4200.471172	23.951066
122.031474	4210.945363	23.956083
122.151629	4242.480078	23.961101
122.175602	4235.262337	23.966119
122.278898	4234.769210	23.971136
122.433860	4234.877417	23.976154
122.657597	4234.475024	23.981171
122.749788	4260.668871	23.986189
123.027512	4254.806110	23.991207
122.869131	4254.153455	23.996224
123.458316	4269.717444	24.001242
123.355634	4253.059135	24.006259
123.404905	4261.583640	24.011277
123.639659	4268.345131	24.016295
123.683375	4277.018208	24.021312
123.538104	4291.807864	24.026330
123.848189	4283.671914	24.031347
124.147540	4286.393798	24.036365
124.522637	4273.908309	24.041383
124.515121	4276.232449	24.046400
124.440165	4260.823156	24.051418
124.647853	4262.156569	24.056435
124.570586	4270.287401	24.061453
124.913725	4286.820455	24.066471
124.932779	4301.369965	24.071488
124.981049	4312.048711	24.076506
125.058774	4296.866529	24.081523
124.506782	4308.597263	24.086541
124.936452	4313.939881	24.091559
124.593950	4328.568845	24.096576
125.449778	4337.738113	24.101594
125.730930	4340.048031	24.106611
125.567808	4365.023936	24.111629
125.792247	4360.064872	24.116647
125.891799	4358.569155	24.121664
125.720102	4367.909801	24.126682
125.929959	4372.639119	24.131699
126.151796	4387.526482	24.136717
126.673047	4376.261321	24.141735
126.584231	4386.938753	24.146752
126.651503	4418.449097	24.151770
127.323146	4411.519554	24.156787
127.105842	4407.576043	24.161805
127.431924	4397.797925	24.166823
127.568114	4403.772172	24.171840
127.222524	4405.575783	24.176858
127.347567	4418.578666	24.181875
127.848291	4416.472135	24.186893
128.513660	4404.107487	24.191911
128.652085	4411.150722	24.196928
128.342618	4418.973522	24.201946
128.557884	4396.110586	24.206963
128.465906	4423.346219	24.211981
128.447706	4408.457748	24.216999
128.207054	4423.984198	24.222016
128.501878	4448.209724	24.227034
128.791510	4451.991969	24.232051
128.760323	4459.962520	24.237069
129.129276	4466.344815	24.242087
129.243388	4485.733423	24.247104
128.934797	4495.727513	24.252122
129.577588	4474.317540	24.257139
129.569645	4490.330046	24.262157
129.622083	4501.058236	24.267175
129.672285	4512.947508	24.272192
130.103347	4506.977422	24.277210
130.427039	4505.599389	24.282227
130.295255	4530.800711	24.287245
130.529807	4527.386876	24.292263
130.701345	4528.157352	24.297280
130.900426	4536.500944	24.302298
131.132623	4526.796530	24.307315
130.653235	4533.460378	24.312333
130.767420	4542.562145	24.317351
131.117465	4557.241072	24.322368
131.182485	4554.949413	24.327386
131.622909	4546.570122	24.332403
131.514835	4569.564291	24.337421
131.715982	4581.458991	24.342439
132.098075	4582.574232	24.347456
131.975650	4586.913214	24.352474
132.265513	4586.538865	24.357491
132.285261	4592.404858	24.362509
132.489398	4607.404026	24.367527
133.082775	4610.627030	24.372544
133.012189	4614.989739	24.377562
132.971699	4609.062884	24.382579
132.907986	4608.102818	24.387597
133.192352	4608.106569	24.392615
133.399787	4598.390060	24.397632
133.377497	4604.011805	24.402650
133.497295	4600.475174	24.407667
133.412496	4608.878705	24.412685
133.407242	4623.679007	24.417703
133.633707	4629.662442	24.422720
133.731830	4636.064754	24.427738
133.727776	4630.915785	24.432755
133.929287	4669.620335	24.437773
134.110286	4670.694395	24.442791
134.615986	4672.849534	24.447808
134.628873	4680.203814	24.452826
134.739425	4697.995121	24.457843
134.827902	4698.972652	24.462861
134.914046	4691.716866	24.467879
134.912042	4705.091796	24.472896
135.131389	4720.272432	24.477914
135.341882	4724.057190	24.482931
135.792341	4729.438647	24.487949
135.745405	4729.141209	24.492967
135.886943	4719.069736	24.497984
135.535124	4744.918045	24.503002
136.137245	4748.905442	24.508019
136.042613	4755.663301	24.513037
136.403748	4757.693903	24.518055
136.617561	4767.265992	24.523072
136.734727	4779.172751	24.528090
137.007457	4779.321745	24.533107
137.184471	4781.349306	24.538125
136.980274	4785.201026	24.543143
137.418200	4782.220893	24.548160
137.415481	4803.043096	24.553178
137.682391	4804.058872	24.558195
137.540400	4798.274317	24.563213
137.636170	4791.068080	24.568231
137.961538	4790.673293	24.573248
137.685687	4814.020768	24.578266
138.230850	4819.703564	24.583283
138.112740	4826.404304	24.588301
138.128525	4838.277068	24.593319
138.717780	4851.592619	24.598336
138.433995	4860.238631	24.603354
138.758017	4851.705562	24.608371
139.322974	4873.210897	24.613389
139.452575	4890.774847	24.618407
139.634587	4880.461917	24.623424
139.586496	4889.228857	24.628442
139.880901	4876.267597	24.633459
140.191897	4879.841281	24.638477
139.998868	4878.218647	24.643495
140.168287	4874.261121	24.648512
140.041630	4891.366583	24.653530
140.661435	4894.033657	24.658547
140.264619	4903.744526	24.663565
140.112817	4910.596158	24.668583
140.820777	4914.574379	24.673600
140.612040	4933.569211	24.678618
140.744537	4931.158857	24.683635
140.594037	4944.306930	24.688653
140.805870	4967.067311	24.693671
141.037057	4959.868545	24.698688
140.862460	4976.442994	24.703706
141.613817	4976.704655	24.708723
141.607084	4995.656341	24.713741
141.822834	5001.032577	24.718759
142.152722	5003.980667	24.723776
141.968266	5031.674022	24.728794
142.229868	5028.974579	24.733811
141.865935	5028.939376	24.738829
142.226195	5044.402586	24.743847
142.935717	5050.482762	24.748864
142.929018	5053.158886	24.753882
143.247320	5047.580494	24.758899
143.580786	5062.926090	24.763917
143.218886	5057.261248	24.768935
143.737214	5074.683607	24.773952
143.716150	5085.127070	24.778970
143.967299	5073.456783	24.783987
144.224228	5078.159245	24.789005
144.173124	5079.402408	24.794023
144.433623	5075.196687	24.799040
143.917297	5087.507205	24.804058
144.572017	5105.690213	24.809075
144.305131	5113.212590	24.814093
144.444773	5124.476857	24.819111
145.118696	5132.018611	24.824128
144.878570	5136.213789	24.829146
145.096836	5142.556295	24.834163
145.169777	5136.543560	24.839181
145.279097	5164.801665	24.844199
145.745235	5160.784014	24.849216
145.605032	5167.548792	24.854234
146.258246	5166.074126	24.859251
146.495754	5171.260192	24.864269
146.763829	5196.301229	24.869287
147.016287	5184.244775	24.874304
146.872502	5182.756507	24.879322
147.376173	5187.409964	24.884339
147.451497	5183.513582	24.889357
147.099361	5177.993948	24.894375
147.248590	5179.507593	24.899392
147.157000	5185.146904	24.904410
147.274830	5197.969720	24.909427
147.702566	5199.336550	24.914445
147.466385	5218.862697	24.919463
147.396285	5222.798282	24.924480
147.592585	5230.615876	24.929498
147.605554	5242.939069	24.934515
147.963682	5250.518099	24.939533
148.021034	5265.581529	24.944551
148.371046	5254.918903	24.949568
148.511889	5278.048200	24.954586
148.884341	5293.831727	24.959603
149.386013	5295.162331	24.964621
149.298649	5294.395916	24.969639
149.672371	5298.395604	24.974656
149.674217	5324.391572	24.979674
149.798005	5329.779573	24.984691
150.248066	5321.189593	24.989709
150.144553	5326.122574	24.994727
150.170854	5321.427470	24.999744
150.349654	5330.314272	25.004762
150.341783	5336.354813	25.009779
150.437989	5341.224873	25.014797
150.884314	5348.797253	25.019815
151.183944	5343.854200	25.024832
151.188094	5350.452669	25.029850
151.261017	5360.694543	25.034867
151.738590	5362.283102	25.039885
151.646076	5372.499951	25.044903
151.669270	5365.831095	25.049920
151.707923	5365.962074	25.054938
151.981703	5377.602832	25.059955
151.910489	5390.858666	25.064973
151.923092	5399.600900	25.069991
152.418085	5403.747133	25.075008
152.342241	5404.295112	25.080026
152.438215	5423.833962	25.085043
152.660802	5432.552937	25.090061
152.770416	5440.014441	25.095079
153.015534	5430.820785	25.100096
153.515408	5439.983772	25.105114
153.593585	5450.539836	25.110131
153.879029	5461.371935	25.115149
153.797709	5468.943752	25.120167
153.841049	5451.793441	25.125184
153.911010	5458.254687	25.130202
153.897477	5469.375593	25.135219
154.123989	5478.195533	25.140237
154.207515	5490.190293	25.145255
154.319181	5500.589657	25.150272
154.186368	5517.143205	25.155290
154.614459	5534.861735	25.160307
155.034674	5530.791335	25.165325
154.819275	5551.264979	25.170343
155.184289	5556.706519	25.175360
155.388666	5566.298378	25.180378
155.608519	5582.665360	25.185395
155.984337	5577.149334	25.190413
155.789052	5590.369136	25.195431
156.031377	5608.001893	25.200448
156.181703	5614.229422	25.205466
156.127954	5619.156634	25.210483
156.646423	5622.748580	25.215501
156.430643	5634.569252	25.220519
156.648430	5644.525135	25.225536
156.825981	5658.179127	25.230554
156.778435	5669.613711	25.235571
157.388459	5691.650993	25.240589
157.344526	5691.248301	25.245607
157.539159	5698.747856	25.250624
158.050017	5712.605126	25.255642
158.042845	5733.177297	25.260659
158.808219	5713.912624	25.265677
158.666208	5723.400373	25.270695
158.705068	5718.449497	25.275712
158.908323	5729.747789	25.280730
159.128925	5748.488387	25.285747
159.538976	5731.202365	25.290765
159.307136	5740.626216	25.295783
159.798234	5738.300997	25.300800
159.680199	5738.821701	25.305818
159.498134	5753.957054	25.310835
160.113272	5754.900394	25.315853
159.884732	5773.322659	25.320871
159.973371	5768.349760	25.325888
160.277573	5783.866673	25.330906
160.375731	5788.651105	25.335923
160.561437	5792.818622	25.340941
160.627921	5803.279203	25.345959
161.093709	5822.127825	25.350976
161.409548	5817.471753	25.355994
161.343406	5828.447253	25.361011
161.639397	5811.867492	25.366029
161.648615	5823.194369	25.371047
162.081170	5828.135403	25.376064
162.659989	5834.171336	25.381082
162.773102	5841.115053	25.386099
162.981950	5837.583907	25.391117
163.234485	5835.946614	25.396135
163.126101	5829.476100	25.401152
163.198734	5831.577748	25.406170
163.012330	5843.418137	25.411187
163.252817	5822.494128	25.416205
163.111744	5834.053751	25.421223
163.295650	5833.954010	25.426240
163.452442	5846.621291	25.431258
162.971657	5859.394718	25.436275
163.575967	5865.947002	25.441293
163.517259	5887.292967	25.446311
163.880782	5908.385702	25.451328
163.786750	5902.122268	25.456346
163.613526	5930.261484	25.461363
163.896015	5932.237118	25.466381
164.184119	5949.885927	25.471399
164.020932	5972.680204	25.476416
164.787025	5988.640375	25.481434
164.750879	6001.887779	25.486451
165.295692	6016.830042	25.491469
165.236950	6027.409118	25.496487
165.549346	6032.753598	25.501504
165.946056	6040.477450	25.506522
166.056021	6058.875619	25.511539
166.524665	6063.877705	25.516557
166.769768	6076.054124	25.521575
166.844522	6071.761488	25.526592
167.140609	6072.868609	25.531610
167.112641	6079.134840	25.536627
167.666227	6077.933687	25.541645
167.652760	6085.135475	25.546663
168.147979	6085.512728	25.551680
168.300269	6093.236829	25.556698
168.169295	6105.398232	25.561715
168.408164	6108.252107	25.566733
168.407604	6103.534826	25.571751
168.222754	6099.967080	25.576768
168.508793	6101.984677	25.581786
168.426090	6113.231660	25.586803
168.407782	6115.677561	25.591821
168.793178	6125.602119	25.596839
168.969708	6144.005926	25.601856
168.998600	6146.842526	25.606874
169.349080	6166.083119	25.611891
169.299662	6181.303283	25.616909
169.682762	6183.890780	25.621927
169.830907	6215.077937	25.626944
170.562849	6220.462628	25.631962
170.399333	6217.019699	25.636979
170.503487	6218.138068	25.641997
170.834403	6228.208725	25.647015
171.284325	6237.098891	25.652032
171.615322	6223.822155	25.657050
171.631152	6229.270044	25.662067
171.690074	6230.196640	25.667085
171.830597	6232.527324	25.672103
171.784205	6258.434761	25.677120
172.172801	6259.704595	25.682138
172.335049	6270.800174	25.687156
172.496480	6261.815959	25.692173
172.432794	6264.609599	25.697191
172.517995	6286.173315	25.702208
172.567735	6279.694601	25.707226
172.825609	6291.944682	25.712244
172.781968	6310.501620	25.717261
173.219858	6329.994161	25.722279
172.883808	6334.378765	25.727296
173.165189	6347.602348	25.732314
173.434850	6364.903427	25.737332
173.441680	6397.668912	25.742349
173.863475	6395.097129	25.747367
173.598551	6404.347281	25.752384
174.305228	6418.765454	25.757402
174.123750	6429.168980	25.762420
174.571369	6446.335213	25.767437
174.806971	6454.154408	25.772455
174.943688	6452.711026	25.777472
175.349473	6458.174105	25.782490
175.523617	6480.522754	25.787508
175.658387	6472.166566	25.792525
175.858496	6488.583828	25.797543
176.124042	6507.354529	25.802560
176.399882	6498.437906	25.807578
176.816232	6503.489728	25.812596
176.998727	6495.052400	25.817613
177.263444	6497.263371	25.822631
177.004936	6496.783098	25.827648
177.654568	6503.155691	25.832666
177.773559	6503.117864	25.837684
177.752694	6507.210234	25.842701
178.277109	6514.626553	25.847719
178.214207	6517.183054	25.852736
178.286277	6515.055726	25.857754
178.211223	6536.660439	25.862772
178.402665	6545.851021	25.867789
178.416516	6555.252088	25.872807
178.304443	6565.492238	25.877824
178.399534	6566.986219	25.882842
178.913372	6583.111539	25.887860
178.782033	6590.723661	25.892877
179.004577	6602.745130	25.897895
179.089752	6613.854474	25.902912
179.614515	6631.567331	25.907930
179.687050	6639.874284	25.912948
179.951890	6651.133532	25.917965
180.205618	6669.046363	25.922983
180.442101	6673.316772	25.928000
180.611217	6688.336717	25.933018
180.791439	6695.758801	25.938036
181.002252	6690.876471	25.943053
181.439410	6710.557834	25.948071
181.583076	6730.412937	25.953088
181.597609	6724.463589	25.958106
181.726405	6729.938665	25.963124
181.906929	6758.860455	25.968141
182.324299	6754.752806	25.973159
182.177130	6761.525719	25.978176
182.750743	6775.242435	25.983194
182.635654	6791.319885	25.988212
183.107327	6788.940629	25.993229
183.076080	6792.216506	25.998247
183.355592	6803.208816	26.003264
183.497737	6805.961455	26.008282
183.693387	6816.740024	26.013300
183.481260	6841.111691	26.018317
183.734184	6844.978558	26.023335
183.738818	6851.481493	26.028352
184.277410	6871.176225	26.033370
184.319268	6878.555101	26.038388
184.652350	6891.115340	26.043405
184.923961	6901.991677	26.048423
185.322475	6908.964318	26.053440
185.236572	6912.638312	26.058458
185.079611	6925.015709	26.063476
185.162684	6927.541070	26.068493
186.167160	6946.169726	26.073511
186.033440	6958.970964	26.078528
186.380510	6955.753026	26.083546
186.467024	6963.884574	26.088564
186.638855	6968.756428	26.093581
186.900574	6977.761596	26.098599
186.856005	6989.446308	26.103616
187.268428	6995.718897	26.108634
187.145892	6995.709951	26.113652
187.340775	7022.294685	26.118669
187.524387	7030.001471	26.123687
187.406600	7020.250965	26.128704
187.606897	7048.497428	26.133722
187.904618	7050.687274	26.138740
187.899219	7065.391454	26.143757
188.105189	7073.589954	26.148775
188.422018	7093.923319	26.153792
188.632109	7107.651560	26.158810
188.736697	7117.038758	26.163828
189.041114	7144.407360	26.168845
189.302951	7145.602129	26.173863
189.451976	7162.440442	26.178880
189.785158	7173.273715	26.183898
190.019657	7175.797723	26.188916
190.252171	7210.287075	26.193933
190.668732	7206.801640	26.198951
190.389264	7212.909829	26.203968
190.461092	7222.294626	26.208986
190.823514	7233.060102	26.214004
191.055617	7246.217762	26.219021
191.525042	7248.236713	26.224039
191.809471	7262.621471	26.229056
192.160710	7269.969889	26.234074
192.640290	7280.472674	26.239092
192.521709	7294.831113	26.244109
193.109073	7285.861002	26.249127
193.118545	7283.761240	26.254144
193.403818	7280.324259	26.259162
193.426635	7283.781115	26.264180
193.274837	7286.733623	26.269197
193.776808	7295.774887	26.274215
193.821589	7317.502636	26.279232
193.894489	7311.582802	26.284250
194.098373	7314.044158	26.289268
194.104423	7340.677957	26.294285
194.630289	7348.522097	26.299303
194.571129	7345.717744	26.304320
194.647947	7366.320307	26.309338
195.144457	7380.140866	26.314356
194.919060	7379.092748	26.319373
195.425313	7397.563258	26.324391
195.107984	7402.471963	26.329408
195.418579	7414.452726	26.334426
195.744190	7429.775950	26.339444
195.726997	7437.211312	26.344461
196.472068	7460.112852	26.349479
196.315299	7464.546115	26.354496
196.858118	7471.536120	26.359514
197.109077	7488.913986	26.364532
197.160977	7501.767691	26.369549
197.509222	7498.077677	26.374567
197.530753	7497.756664	26.379584
197.917381	7520.559208	26.384602
198.006622	7528.706348	26.389620
197.953826	7542.351600	26.394637
198.448221	7544.754754	26.399655
198.271411	7553.457021	26.404672
198.636263	7558.339697	26.409690
198.854900	7573.779186	26.414708
198.703932	7585.012505	26.419725
198.754347	7600.754691	26.424743
199.273876	7615.358473	26.429760
199.237997	7624.692784	26.434778
199.658791	7639.969769	26.439796
199.630280	7643.550175	26.444813
200.256310	7662.271356	26.449831
200.257643	7683.642911	26.454848
200.382075	7679.206162	26.459866
200.837683	7689.154766	26.464884
200.824271	7716.637521	26.469901
201.164732	7706.294990	26.474919
201.344897	7723.386306	26.479936
201.791252	7735.900938	26.484954
201.906091	7741.545647	26.489972
201.934112	7759.077999	26.494989
202.632003	7763.767093	26.500007
202.680514	7771.256341	26.505024
202.642575	7777.346104	26.510042
203.084031	7777.878002	26.515060
202.964933	7793.008055	26.520077
203.185816	7801.235188	26.525095
203.223367	7805.601784	26.530112
203.319545	7825.518883	26.535130
203.697491	7832.856852	26.540148
203.571342	7859.625208	26.545165
203.950049	7867.083573	26.550183
204.148471	7885.475560	26.555200
204.161037	7896.510378	26.560218
204.797946	7902.914004	26.565236
205.212692	7910.509783	26.570253
205.149632	7924.746201	26.575271
205.882934	7939.769424	26.580288
205.611318	7946.670521	26.585306
206.294483	7957.783613	26.590324
206.191295	7980.629157	26.595341
206.540504	7983.145371	26.600359
206.599808	7981.921788	26.605376
206.696429	7989.396889	26.610394
207.755263	7981.881212	26.615412
207.539984	7991.253256	26.620429
207.515856	7988.827362	26.625447
207.979439	7999.770405	26.630464
208.042259	8017.406775	26.635482
208.455860	8019.112125	26.640500
208.209993	8023.908397	26.645517
208.521369	8038.563505	26.650535
208.606605	8062.017590	26.655552
208.871939	8053.824876	26.660570
209.298760	8061.598312	26.665588
209.264233	8081.929569	26.670605
209.579751	8073.445006	26.675623
209.749358	8090.317139	26.680640
209.558091	8106.584152	26.685658
209.874205	8117.565033	26.690676
209.967841	8139.750543	26.695693
210.079356	8144.711491	26.700711
210.260148	8166.278522	26.705728
210.673076	8183.013671	26.710746
210.843847	8207.035114	26.715764
211.024101	8218.915940	26.720781
211.436979	8227.139141	26.725799
211.858148	8243.486263	26.730816
212.085730	8256.220976	26.735834
212.640989	8266.722157	26.740852
212.568958	8273.860580	26.745869
212.471386	8274.507550	26.750887
212.759111	8291.912518	26.755904
212.889891	8307.468059	26.760922
213.241547	8323.166704	26.765940
213.441843	8343.194061	26.770957
213.457507	8342.535313	26.775975
213.611437	8355.160190	26.780992
213.991289	8361.237859	26.786010
214.140699	8372.756067	26.791028
214.150452	8393.465565	26.796045
214.490615	8404.623043	26.801063
215.024622	8415.828842	26.806080
214.638429	8431.450229	26.811098
215.000520	8440.255341	26.816116
215.271857	8457.355227	26.821133
215.689890	8471.150329	26.826151
215.901834	8480.217354	26.831168
215.843739	8492.018831	26.836186
216.387410	8505.775089	26.841204
216.477411	8525.517654	26.846221
216.529522	8540.608315	26.851239
216.901750	8540.425464	26.856256
217.000371	8550.926668	26.861274
217.436281	8572.333952	26.866292
217.418806	8580.830081	26.871309
217.923909	8597.335411	26.876327
218.439359	8611.850212	26.881344
218.269079	8627.175402	26.886362
218.867166	8635.833722	26.891380
218.855797	8649.083189	26.896397
219.065535	8641.447571	26.901415
219.386847	8654.767315	26.906432
219.598848	8671.711828	26.911450
219.954933	8670.537616	26.916468
220.242854	8694.668042	26.921485
220.272665	8699.946701	26.926503
220.778937	8696.552458	26.931520
220.631742	8717.953885	26.936538
221.151742	8728.452537	26.941556
221.368331	8722.217001	26.946573
221.579932	8728.632951	26.951591
221.890679	8755.740218	26.956608
221.780326	8757.919752	26.961626
221.722196	8765.951674	26.966644
222.067757	8780.093778	26.971661
222.387902	8795.826454	26.976679
222.434684	8819.313217	26.981696
222.415224	8831.454348	26.986714
222.685676	8855.005818	26.991732
223.129066	8857.146648	26.996749
223.114815	8887.174955	27.001767
223.517644	8896.665166	27.006784
223.313167	8915.738513	27.011802
223.468992	8930.917170	27.016820
223.622165	8944.387814	27.021837
224.000127	8969.914507	27.026855
224.823248	8984.247275	27.031872
225.221865	9000.446096	27.036890
225.507957	9011.130878	27.041908
225.628944	9023.400185	27.046925
225.828416	9033.561310	27.051943
226.084924	9033.054935	27.056960
226.002241	9054.732870	27.061978
226.435304	9072.216293	27.066996
226.986006	9083.330801	27.072013
226.885273	9097.984088	27.077031
227.402177	9089.969830	27.082048
227.751094	9102.864768	27.087066
227.592722	9114.774645	27.092084
228.072649	9126.188381	27.097101
228.304629	9129.748926	27.102119
228.638907	9135.546133	27.107136
228.894031	9147.646078	27.112154
228.964097	9153.045053	27.117172
229.244246	9155.557115	27.122189
229.400237	9151.716534	27.127207
230.047373	9161.873094	27.132224
230.118129	9184.369465	27.137242
230.403238	9181.915927	27.142260
230.403169	9172.950447	27.147277
230.209950	9188.639939	27.152295
230.471444	9189.500947	27.157312
230.412995	9205.332815	27.162330
230.934938	9211.663028	27.167348
230.898463	9230.484503	27.172365
230.870906	9234.840983	27.177383
230.696854	9251.406430	27.182400
231.374601	9284.578250	27.187418
231.905112	9311.670637	27.192436
232.557990	9313.778495	27.197453
232.292317	9328.476575	27.202471
232.869567	9330.591417	27.207488
232.837048	9359.652408	27.212506
233.329076	9374.716864	27.217524
233.307760	9387.758275	27.222541
233.443331	9398.628878	27.227559
234.271105	9409.167717	27.232576
234.053298	9440.779312	27.237594
234.615180	9433.403365	27.242612
234.924811	9442.186984	27.247629
235.078788	9457.638206	27.252647
235.583175	9451.759714	27.257664
235.909674	9460.770565	27.262682
236.156066	9480.071783	27.267700
236.307646	9475.603268	27.272717
236.218681	9485.468112	27.277735
236.485441	9498.417119	27.282752
236.436634	9517.780546	27.287770
236.858770	9527.035575	27.292788
236.960757	9540.414356	27.297805
237.249931	9561.739304	27.302823
237.290094	9575.848292	27.307840
237.389022	9596.090903	27.312858
237.397393	9609.668745	27.317876
237.653233	9625.798846	27.322893
237.952633	9654.549528	27.327911
238.364776	9665.583361	27.332928
238.821755	9687.305329	27.337946
239.096715	9703.116477	27.342964
239.293275	9725.354938	27.347981
239.556267	9733.199593	27.352999
240.080428	9741.306734	27.358016
240.392890	9764.279942	27.363034
240.571612	9763.255478	27.368052
240.908340	9782.568132	27.373069
241.266106	9805.656011	27.378087
241.225610	9793.325435	27.383104
241.651940	9811.524456	27.388122
241.613146	9819.216571	27.393140
241.919103	9830.722576	27.398157
241.832152	9849.627166	27.403175
242.365440	9857.922700	27.408192
242.551784	9872.410322	27.413210
242.689411	9899.594617	27.418228
243.243366	9902.683073	27.423245
243.424817	9929.996456	27.428263
243.508933	9932.898657	27.433280
244.045283	9946.113062	27.438298
244.169195	9948.243811	27.443316
244.191032	9961.473129	27.448333
244.109271	9986.518124	27.453351
244.498697	9988.705052	27.458368
244.932884	10011.245737	27.463386
244.937364	10027.537508	27.468404
245.219878	10037.649319	27.473421
245.037582	10056.815678	27.478439
245.284334	10075.911961	27.483456
245.686482	10097.025180	27.488474
245.984595	10111.516609	27.493492
246.664210	10123.495173	27.498509
246.782017	10137.743073	27.503527
247.134968	10154.778526	27.508544
247.668873	10160.574637	27.513562
248.089405	10159.571641	27.518580
248.156003	10170.239114	27.523597
248.418446	10200.583385	27.528615
248.650602	10196.919028	27.533632
248.880810	10213.715657	27.538650
249.187930	10224.755415	27.543668
249.526842	10215.319782	27.548685
249.531300	10236.738364	27.553703
249.902618	10250.145713	27.558720
250.160825	10246.805528	27.563738
250.228838	10274.429705	27.568756
250.670733	10284.679191	27.573773
250.716073	10288.720634	27.578791
251.289008	10294.925486	27.583808
251.034069	10315.281041	27.588826
251.119532	10333.655925	27.593844
251.667861	10344.994644	27.598861
251.754346	10373.917293	27.603879
251.906002	10388.774266	27.608896
252.513737	10409.425398	27.613914
252.301955	10416.594958	27.618932
252.787680	10424.747400	27.623949
252.697216	10459.153801	27.628967
253.174686	10478.541726	27.633984
253.386342	10491.623534	27.639002
253.641085	10510.410219	27.644020
254.276040	10535.351839	27.649037
254.040050	10555.003467	27.654055
254.538414	10576.166019	27.659072
254.915067	10591.694199	27.664090
255.107921	10608.118504	27.669108
255.207660	10615.054712	27.674125
255.379897	10639.478975	27.679143
255.785277	10658.917630	27.684160
256.301733	10679.417977	27.689178
256.335834	10701.126903	27.694196
257.073065	10706.735222	27.699213
257.167317	10729.626132	27.704231
257.210483	10733.464016	27.709248
257.915022	10745.633511	27.714266
257.674032	10762.347863	27.719284
258.301310	10776.342790	27.724301
258.253986	10797.590278	27.729319
258.529994	10804.862969	27.734336
259.098913	10814.647510	27.739354
259.200061	10838.552868	27.744372
259.928746	10845.031556	27.749389
260.599714	10855.557883	27.754407
260.828257	10849.117092	27.759424
261.033159	10850.482264	27.764442
261.104672	10853.392229	27.769460
261.086990	10863.153188	27.774477
261.037537	10881.895247	27.779495
261.604495	10873.972671	27.784512
261.813701	10896.832224	27.789530
261.759526	10920.819298	27.794548
262.180245	10910.674141	27.799565
262.283429	10931.816588	27.804583
262.131222	10933.701613	27.809600
262.323436	10952.064297	27.814618
262.608694	10975.257229	27.819636
262.813462	10995.610170	27.824653
263.093481	10998.409300	27.829671
263.064978	11017.560850	27.834688
263.530369	11044.156464	27.839706
263.556887	11074.175841	27.844724
264.277810	11087.988563	27.849741
264.030059	11105.699354	27.854759
264.542162	11133.153168	27.859776
264.995480	11161.175280	27.864794
264.970851	11173.821651	27.869812
265.692129	11194.744946	27.874829
265.766126	11228.914699	27.879847
265.867083	11249.615196	27.884864
266.175055	11274.058966	27.889882
266.718205	11295.232403	27.894900
267.108600	11306.857084	27.899917
267.430252	11331.270321	27.904935
267.471303	11353.917242	27.909952
268.235633	11358.337265	27.914970
268.456625	11366.856137	27.919988
269.206744	11367.983171	27.925005
269.479014	11391.453003	27.930023
269.702290	11383.460914	27.935040
270.252279	11383.147051	27.940058
269.724227	11398.618295	27.945076
270.446725	11414.860600	27.950093
270.824033	11424.361269	27.955111
270.730594	11430.153566	27.960128
271.557485	11439.138012	27.965146
271.481270	11441.755797	27.970164
271.713178	11458.892994	27.975181
271.496800	11466.620752	27.980199
271.580185	11480.521813	27.985216
272.315503	11502.824205	27.990234
272.230647	11522.035298	27.995252
272.233377	11552.442371	28.000269
272.604446	11566.309369	28.005287
272.844651	11582.975797	28.010304
272.900405	11604.677641	28.015322
273.024965	11638.652414	28.020340
273.850517	11656.052559	28.025357
274.129622	11674.591576	28.030375
274.550199	11699.731933	28.035392
274.724130	11708.569947	28.040410
274.750915	11742.011200	28.045428
274.983947	11754.905373	28.050445
275.421677	11773.798811	28.055463
275.403099	11805.292338	28.060480
275.803700	11815.812762	28.065498
276.193235	11851.379711	28.070516
276.180035	11869.311782	28.075533
277.003058	11906.805143	28.080551
277.029563	11926.662452	28.085568
277.386872	11945.475628	28.090586
277.525226	11966.515936	28.095604
277.907656	11983.564223	28.100621
278.324754	12002.211599	28.105639
278.385649	12011.033790	28.110656
279.525359	12028.780290	28.115674
279.822467	12041.709013	28.120692
280.378469	12024.377893	28.125709
280.839964	12024.797926	28.130727
281.058406	12049.941502	28.135744
281.426598	12043.364505	28.140762
281.594892	12050.248253	28.145780
281.546617	12057.646783	28.150797
282.073035	12047.897062	28.155815
282.247327	12051.744323	28.160832
282.329558	12052.438942	28.165850
282.220171	12068.059097	28.170868
282.104854	12075.788569	28.175885
282.444506	12086.030109	28.180903
282.746844	12100.911043	28.185920
282.898215	12123.569184	28.190938
283.216607	12150.106620	28.195956
283.370575	12180.291357	28.200973
283.346980	12199.964262	28.205991
283.341940	12228.776167	28.211008
283.827271	12247.220323	28.216026
284.005730	12287.103424	28.221044
284.381039	12314.009101	28.226061
285.196895	12343.641239	28.231079
284.994447	12374.810939	28.236096
285.343641	12393.848940	28.241114
285.948634	12411.845717	28.246132
286.159372	12433.071636	28.251149
286.588211	12463.573901	28.256167
286.591666	12484.608810	28.261184
287.041350	12490.533142	28.266202
287.413725	12522.214013	28.271220
287.649963	12550.339017	28.276237
287.842223	12564.225390	28.281255
287.797272	12592.374862	28.286272
288.591203	12623.732599	28.291290
288.881510	12643.169824	28.296308
289.113322	12656.671571	28.301325
289.644822	12688.293390	28.306343
289.624349	12707.055631	28.311360
290.643298	12726.085797	28.316378
290.601133	12743.646239	28.321396
291.003281	12760.477794	28.326413
291.355488	12781.975461	28.331431
291.440635	12811.373856	28.336448
291.830356	12819.019458	28.341466
292.173365	12848.405257	28.346484
292.434084	12864.284909	28.351501
293.028081	12880.516054	28.356519
293.060681	12896.876207	28.361536
293.093436	12918.412650	28.366554
293.276402	12942.251675	28.371572
293.452014	12958.128146	28.376589
293.932512	12980.440026	28.381607
294.068041	13006.102240	28.386624
294.447681	13012.473244	28.391642
294.922390	13041.651699	28.396660
295.086774	13071.357353	28.401677
295.557643	13075.789316	28.406695
295.644829	13106.878695	28.411712
296.091498	13128.236732	28.416730
296.482409	13148.423764	28.421748
296.457239	13162.521482	28.426765
296.978403	13196.150373	28.431783
297.089357	13228.802370	28.436800
297.597786	13237.470143	28.441818
298.097218	13266.140672	28.446836
298.346382	13279.164190	28.451853
298.755147	13309.245911	28.456871
298.727701	13319.786038	28.461888
299.301630	13337.163399	28.466906
299.422966	13359.820356	28.471924
299.116886	13384.952604	28.476941
299.710099	13405.275144	28.481959
300.055590	13436.659699	28.486976
300.491877	13443.517890	28.491994
300.816387	13459.885537	28.497012
300.901113	13479.423916	28.502029
301.319051	13509.945717	28.507047
301.388150	13525.140688	28.512064
302.139101	13537.339313	28.517082
302.405768	13554.422570	28.522100
302.854355	13568.127212	28.527117
303.291703	13585.171273	28.532135
303.570889	13598.573009	28.537152
304.068838	13617.737581	28.542170
304.370963	13622.496977	28.547188
304.612410	13646.910427	28.552205
305.056507	13643.545142	28.557223
305.556202	13651.472375	28.562240
305.939465	13655.898488	28.567258
306.182517	13669.604080	28.572276
306.636371	13682.031542	28.577293
306.706656	13678.236352	28.582311
306.924385	13689.234172	28.587328
306.761551	13711.932265	28.592346
307.230180	13724.904127	28.597364
307.188252	13752.290844	28.602381
307.539266	13769.281603	28.607399
307.519828	13789.341827	28.612416
308.043440	13820.590544	28.617434
308.049081	13846.278699	28.622452
308.362054	13871.233786	28.627469
308.727937	13906.142593	28.632487
308.705274	13937.138251	28.637504
308.989995	13967.963422	28.642522
309.216577	13993.256017	28.647540
309.332837	14026.164028	28.652557
310.109576	14052.528800	28.657575
310.199389	14097.485541	28.662592
310.941794	14124.926106	28.667610
311.228210	14151.277492	28.672628
311.704132	14176.784468	28.677645
312.076104	14191.654251	28.682663
312.449354	14224.331104	28.687680
312.679653	14246.229064	28.692698
313.230275	14274.795220	28.697716
313.579296	14304.381228	28.702733
313.830572	14313.924126	28.707751
314.069991	14335.700934	28.712768
314.633042	14362.320559	28.717786
314.984452	14386.699621	28.722804
315.064198	14407.426577	28.727821
315.438570	14431.091188	28.732839
315.866779	14453.435801	28.737856
315.870313	14468.623576	28.742874
316.375647	14487.485387	28.747892
316.504880	14522.083190	28.752909
317.336605	14535.249435	28.757927
317.634016	14555.787759	28.762944
317.755673	14571.613264	28.767962
317.986225	14603.649425	28.772980
318.119079	14619.388028	28.777997
319.147645	14622.530600	28.783015
319.598018	14646.022227	28.788032
319.744349	14671.915372	28.793050
319.918972	14676.278530	28.798068
320.168461	14699.373197	28.803085
320.821837	14700.314761	28.808103
320.770490	14721.268643	28.813120
320.863385	14735.772140	28.818138
321.007531	14758.608510	28.823156
321.358964	14783.612226	28.828173
321.328313	14805.372819	28.833191
321.601476	14828.268344	28.838208
321.868916	14863.338879	28.843226
322.276285	14879.708455	28.848244
322.391119	14905.558321	28.853261
323.028418	14920.999552	28.858279
323.150888	14949.930752	28.863296
323.495938	14984.293738	28.868314
323.978246	15002.729721	28.873332
324.239353	15019.695667	28.878349
324.529669	15042.724191	28.883367
325.250439	15070.563917	28.888384
325.586852	15109.421620	28.893402
326.179241	15117.767649	28.898420
326.052643	15148.595243	28.903437
326.756045	15153.714308	28.908455
327.227493	15177.154365	28.913472
327.637884	15195.652879	28.918490
328.646910	15196.327693	28.923508
328.688933	15202.564651	28.928525
328.989671	15218.733126	28.933543
329.172676	15231.433462	28.938560
329.118930	15253.152765	28.943578
329.500893	15251.352898	28.948596
329.804594	15291.061155	28.953613
329.685888	15301.964354	28.958631
329.922224	15320.170267	28.963648
330.196617	15359.060873	28.968666
330.905066	15377.898044	28.973684
330.796095	15425.646095	28.978701
331.049323	15434.502201	28.983719
330.931219	15485.258909	28.988736
331.372773	15511.653058	28.993754
331.763425	15541.286443	28.998772
332.049972	15588.837245	29.003789
332.841129	15611.679815	29.008807
332.950169	15645.684455	29.013824
333.364018	15679.032049	29.018842
334.079301	15708.558523	29.023860
333.979803	15740.038373	29.028877
334.796353	15772.832642	29.033895
335.162788	15800.951221	29.038912
335.082625	15827.978949	29.043930
336.039305	15853.892970	29.048948
336.471240	15873.227138	29.053965
336.469495	15887.178347	29.058983
337.092651	15917.128610	29.064000
337.950083	15917.943557	29.069018
339.195459	15924.658109	29.074036
339.240100	15935.214810	29.079053
339.864326	15925.975389	29.084071
340.144795	15929.571208	29.089088
339.964846	15937.068115	29.094106
340.455131	15942.221065	29.099124
340.655923	15962.707778	29.104141
340.818645	15956.791210	29.109159
341.290617	15974.724096	29.114176
341.339636	15988.522011	29.119194
341.844415	15997.836471	29.124212
341.899407	16027.428476	29.129229
341.897442	16040.440534	29.134247
342.113471	16048.035984	29.139264
342.443148	16075.815956	29.144282
342.735389	16106.810991	29.149300
342.914854	16129.993325	29.154317
343.025808	16158.881285	29.159335
343.706765	16180.283435	29.164352
344.046628	16201.555989	29.169370
344.948179	16203.421198	29.174388
344.482760	16222.049802	29.179405
345.152187	16250.738491	29.184423
345.581739	16258.749518	29.189440
345.552389	16292.869776	29.194458
345.725124	16310.967518	29.199476
345.921245	16330.579171	29.204493
346.352035	16367.295004	29.209511
346.688122	16397.162757	29.214528
346.609525	16428.500205	29.219546
347.466508	16458.100767	29.224564
347.653904	16498.899751	29.229581
347.883139	16519.305233	29.234599
348.623324	16548.466614	29.239616
349.133096	16587.519841	29.244634
349.269861	16608.840660	29.249652
349.658490	16654.029309	29.254669
349.903647	16664.967868	29.259687
350.342086	16689.474689	29.264704
350.519603	16733.142818	29.269722
351.467531	16744.747081	29.274740
352.514371	16754.607598	29.279757
352.868289	16768.310092	29.284775
353.322847	16779.872949	29.289792
353.634324	16794.176670	29.294810
353.845194	16806.427586	29.299828
354.470915	16815.394703	29.304845
354.295155	16835.634220	29.309863
354.495319	16857.100924	29.314880
354.593836	16877.452793	29.319898
355.139753	16905.726449	29.324916
355.164108	16929.189293	29.329933
355.172167	16952.178871	29.334951
356.111263	16980.709234	29.339968
356.612980	17003.016825	29.344986
356.946519	17024.356113	29.350004
357.223205	17055.388608	29.355021
357.494062	17083.468438	29.360039
357.798012	17102.817322	29.365056
358.041303	17125.840785	29.370074
358.604479	17149.325259	29.375092
358.670131	17184.757213	29.380109
358.374652	17218.192020	29.385127
359.355368	17235.931914	29.390144
359.651262	17278.642546	29.395162
360.123072	17314.426939	29.400180
360.354396	17340.934423	29.405197
360.924418	17355.969820	29.410215
361.417983	17383.007775	29.415232
361.401540	17421.779516	29.420250
361.772347	17448.149070	29.425268
361.941850	17478.497095	29.430285
362.362472	17509.664286	29.435303
363.025342	17542.670328	29.440320
363.019197	17573.485724	29.445338
363.359935	17604.325835	29.450356
363.761035	17639.912983	29.455373
364.363380	17677.348941	29.460391
364.987881	17707.658475	29.465408
365.132032	17734.694835	29.470426
365.670247	17758.450682	29.475444
365.914436	17775.671319	29.480461
366.111118	17821.868979	29.485479
366.948537	17846.232805	29.490496
367.099965	17873.395863	29.495514
367.308684	17900.082940	29.500532
367.776933	17910.717518	29.505549
368.267354	17943.825359	29.510567
368.970221	17960.866387	29.515584
369.144089	18000.861147	29.520602
369.515306	18006.567190	29.525620
369.807933	18031.003950	29.530637
370.192668	18064.016003	29.535655
370.756244	18077.722784	29.540672
370.761609	18099.699310	29.545690
371.027481	18133.776184	29.550708
371.260455	18154.624424	29.555725
371.667883	18182.883748	29.560743
372.100286	18210.577849	29.565760
372.096059	18243.265183	29.570778
372.670051	18272.420827	29.575796
372.924008	18303.211953	29.580813
373.603444	18336.352407	29.585831
374.436960	18361.910871	29.590848
374.736331	18391.753631	29.595866
375.479486	18414.377912	29.600884
375.543342	18425.784220	29.605901
375.520331	18447.111743	29.610919
376.269401	18469.380461	29.615936
376.450310	18502.543706	29.620954
376.865408	18522.071354	29.625972
377.272513	18548.294805	29.630989
377.609539	18572.382978	29.636007
378.146270	18590.167736	29.641024
378.265524	18622.452382	29.646042
378.721151	18658.630131	29.651060
379.181551	18678.659622	29.656077
379.431255	18725.787364	29.661095
379.761516	18742.930164	29.666112
379.611476	18778.637608	29.671130
380.009737	18817.954141	29.676148
380.878038	18845.974528	29.681165
381.105377	18868.690948	29.686183
381.910644	18883.589574	29.691200
382.782268	18919.015051	29.696218
382.627984	18940.442134	29.701236
383.114685	18960.779733	29.706253
383.680501	18996.331557	29.711271
384.162929	19007.856702	29.716288
384.144587	19046.640444	29.721306
384.360700	19069.808247	29.726324
385.289008	19097.106647	29.731341
385.476837	19128.403623	29.736359
385.846150	19161.902773	29.741376
386.257021	19178.633894	29.746394
386.515130	19213.045303	29.751412
387.003571	19242.872550	29.756429
386.784358	19276.967279	29.761447
387.277540	19306.303612	29.766464
387.344903	19335.024626	29.771482
387.983737	19381.352213	29.776500
388.666481	19400.978557	29.781517
389.183953	19425.698657	29.786535
390.229229	19423.648483	29.791552
391.161462	19449.512326	29.796570
391.433938	19465.353884	29.801588
392.114135	19481.533230	29.806605
392.464921	19505.532210	29.811623
392.792624	19500.148314	29.816640
393.033189	19510.499960	29.821658
393.261725	19530.475779	29.826676
393.704236	19534.023557	29.831693
393.545068	19558.056411	29.836711
393.969054	19550.484348	29.841728
394.227698	19583.468240	29.846746
394.738025	19594.189962	29.851764
395.072783	19611.895687	29.856781
394.878616	19632.244122	29.861799
395.338244	19659.567277	29.866816
395.655119	19689.395295	29.871834
395.522400	19716.365548	29.876852
396.201753	19752.647449	29.881869
396.321256	19781.710581	29.886887
396.588039	19827.858110	29.891904
397.081748	19860.266167	29.896922
397.227358	19908.081278	29.901940
397.689508	19937.966139	29.906957
398.064449	19988.790802	29.911975
398.483473	20022.210960	29.916992
398.977613	20065.126185	29.922010
399.162533	20109.460942	29.927028
400.327440	20138.769756	29.932045
400.075173	20181.502755	29.937063
400.875549	20212.240262	29.942080
401.375218	20251.250218	29.947098
401.651959	20285.829446	29.952116
402.524208	20313.783880	29.957133
402.976466	20356.132947	29.962151
403.374814	20381.071204	29.967168
403.865665	20407.964788	29.972186
403.953885	20450.024256	29.977204
404.422262	20472.736156	29.982221
405.038213	20503.816808	29.987239
405.288383	20534.693096	29.992256
405.461398	20568.720940	29.997274
405.645129	20609.453407	30.002292
406.208980	20639.185573	30.007309
406.645862	20684.136048	30.012327
406.834247	20727.697820	30.017344
407.440845	20759.901376	30.022362
407.710803	20801.588032	30.027380
408.348220	20841.587145	30.032397
409.154987	20861.112752	30.037415
409.449665	20884.468741	30.042432
410.029991	20921.442712	30.047450
410.374906	20961.726908	30.052468
410.718836	20989.485979	30.057485
411.031076	21031.166222	30.062503
411.453717	21061.390691	30.067520
412.081269	21105.525696	30.072538
412.314694	21132.477162	30.077556
412.499467	21159.536028	30.082573
412.726169	21203.046988	30.087591
413.586892	21225.616275	30.092608
414.452855	21249.173214	30.097626
414.787646	21290.793623	30.102644
415.250766	21310.685527	30.107661
415.920857	21325.443149	30.112679
416.298975	21345.076394	30.117696
416.733110	21353.447025	30.122714
417.524491	21381.370890	30.127732
418.899375	21389.407987	30.132749
419.198003	21384.501259	30.137767
419.115588	21398.003773	30.142784
419.758683	21422.778610	30.147802
419.475238	21440.373987	30.152820
419.825203	21460.292644	30.157837
420.027721	21486.609704	30.162855
420.387586	21506.190974	30.167872
420.461371	21539.548227	30.172890
420.807442	21556.130059	30.177908
421.067520	21593.066977	30.182925
421.534904	21624.052861	30.187943
421.758766	21662.328117	30.192960
421.998919	21675.284100	30.197978
421.662110	21719.873271	30.202996
422.590309	21747.349471	30.208013
422.790301	21791.522229	30.213031
423.225012	21835.054072	30.218048
423.931898	21866.451746	30.223066
423.753455	21916.462407	30.228084
424.204458	21955.072885	30.233101
424.583042	22008.446140	30.238119
424.950370	22043.504359	30.243136
425.462301	22089.548258	30.248154
426.150242	22143.293371	30.253172
426.462713	22195.188234	30.258189
426.871815	22245.671978	30.263207
427.359511	22283.512483	30.268224
428.268534	22316.514153	30.273242
428.712386	22356.099517	30.278260
429.291866	22398.289258	30.283277
429.976494	22426.167858	30.288295
429.951727	22459.711916	30.293312
430.674091	22493.198842	30.298330
430.954473	22536.683892	30.303348
431.730354	22563.026173	30.308365
432.336562	22609.989305	30.313383
432.370651	22647.733705	30.318400
433.160421	22673.756955	30.323418
433.121235	22714.807270	30.328436
433.718649	22742.915231	30.333453
434.335529	22788.380833	30.338471
434.652166	22825.705284	30.343488
435.106318	22858.955017	30.348506
435.424133	22895.771735	30.353524
436.749379	22917.744690	30.358541
437.102009	22943.884717	30.363559
437.358634	22977.173620	30.368576
437.987820	22996.685336	30.373594
438.325309	23037.485009	30.378612
438.803773	23076.938637	30.383629
439.216376	23092.530285	30.388647
439.536323	23127.086157	30.393664
439.729919	23161.544717	30.398682
439.953348	23192.551716	30.403700
440.524334	23234.289282	30.408717
440.809279	23267.066374	30.413735
441.046670	23311.341000	30.418752
441.596444	23346.341835	30.423770
441.756757	23385.341030	30.428788
441.957260	23424.954911	30.433805
442.686215	23474.355156	30.438823
442.954062	23521.889161	30.443840
443.604829	23559.092238	30.448858
443.776675	23608.666894	30.453876
444.302544	23645.163908	30.458893
445.013981	23685.427192	30.463911
445.121430	23738.872782	30.468928
445.867446	23772.645317	30.473946
446.325903	23818.228160	30.478964
447.492492	23843.602838	30.483981
447.670186	23873.488089	30.488999
447.960140	23920.686861	30.494016
448.771491	23953.332600	30.499034
448.982527	23992.302738	30.504052
449.714817	24022.675324	30.509069
450.516236	24036.918531	30.514087
450.771914	24073.590398	30.519104
451.169966	24095.339624	30.524122
451.385969	24139.537954	30.529140
452.141983	24157.568366	30.534157
452.260124	24180.481896	30.539175
452.569584	24225.869695	30.544192
452.614851	24243.818925	30.549210
452.652807	24288.464909	30.554228
453.141880	24333.586804	30.559245
453.614655	24383.326885	30.564263
453.474423	24436.596405	30.569280
454.011283	24477.845972	30.574298
454.435186	24539.166990	30.579316
455.016953	24580.589149	30.584333
455.170959	24628.209708	30.589351
455.620587	24690.082072	30.594368
456.312944	24737.659740	30.599386
456.692202	24796.513389	30.604404
457.377751	24841.984203	30.609421
458.409699	24886.617366	30.614439
459.258880	24936.293735	30.619456
460.041193	24973.503419	30.624474
460.195467	25006.065769	30.629492
460.734728	25036.700706	30.634509
461.180971	25072.808684	30.639527
461.730026	25109.008562	30.644544
462.073337	25145.849608	30.649562
462.121148	25195.331112	30.654580
462.428517	25221.606704	30.659597
463.107432	25280.354181	30.664615
463.269886	25337.184488	30.669632
463.716141	25375.516557	30.674650
464.331086	25428.241817	30.679668
464.688485	25467.014540	30.684685
465.448279	25522.447404	30.689703
465.735013	25574.899329	30.694720
466.173329	25608.377842	30.699738
466.583969	25667.215120	30.704756
467.174833	25709.587845	30.709773
467.873887	25748.372580	30.714791
468.253497	25805.783586	30.719808
469.072739	25854.366861	30.724826
469.278554	25895.873242	30.729844
470.183264	25937.052966	30.734861
471.537631	25944.669901	30.739879
472.019514	25984.840935	30.744896
472.758846	25994.190079	30.749914
472.935461	26030.220041	30.754932
473.529180	26047.263699	30.759949
474.529740	26064.385254	30.764967
474.621481	26095.767812	30.769984
475.032218	26106.041792	30.775002
475.188332	26143.491513	30.780020
475.734821	26166.441038	30.785037
476.150347	26195.603508	30.790055
476.068090	26232.733243	30.795072
476.330725	26261.482675	30.800090
476.442686	26302.078269	30.805108
476.878142	26350.455104	30.810125
477.364403	26388.800187	30.815143
477.800529	26446.368017	30.820160
478.106350	26484.919746	30.825178
478.832186	26533.249133	30.830196
478.970568	26567.286870	30.835213
479.850902	26626.677520	30.840231
479.965219	26687.617398	30.845248
480.157209	26722.040846	30.850266
480.394804	26781.727446	30.855284
480.951522	26837.980336	30.860301
481.277894	26883.339286	30.865319
481.682215	26939.384276	30.870336
482.419914	26979.966428	30.875354
483.142387	27038.842070	30.880372
483.368717	27093.926562	30.885389
484.416130	27132.603274	30.890407
485.062310	27161.082684	30.895424
485.618015	27197.538220	30.900442
486.076030	27248.118627	30.905460
486.227305	27282.717095	30.910477
486.618344	27329.577399	30.915495
487.037453	27383.321983	30.920512
487.570257	27431.215806	30.925530
488.511391	27475.389722	30.930548
488.571746	27541.271589	30.935565
489.507272	27563.985243	30.940583
489.721826	27624.495520	30.945600
490.511053	27654.330528	30.950618
491.139820	27704.130203	30.955636
491.378632	27751.161895	30.960653
492.131920	27781.583447	30.965671
492.738783	27826.005890	30.970688
493.455228	27867.309673	30.975706
494.190748	27894.062759	30.980724
494.539927	27925.633242	30.985741
495.150835	27961.390485	30.990759
495.447867	28007.892799	30.995776
495.827421	28040.628729	31.000794
496.459868	28073.089528	31.005812
496.703344	28117.850328	31.010829
497.440568	28143.319703	31.015847
497.751314	28190.410105	31.020864
498.221669	28230.320175	31.025882
498.566751	28276.083461	31.030900
498.866097	28333.437309	31.035917
499.280527	28368.180595	31.040935
499.510440	28425.208696	31.045952
499.895424	28477.788890	31.050970
500.562550	28517.670276	31.055988
501.321795	28583.768736	31.061005
501.632051	28625.876410	31.066023
502.285078	28679.160543	31.071040
502.369504	28741.106260	31.076058
503.201075	28784.992495	31.081076
503.816810	28830.706233	31.086093
504.474412	28881.854656	31.091111
505.175808	28929.462968	31.096128
505.306793	28991.647939	31.101146
506.272511	29022.648567	31.106164
506.657615	29068.060340	31.111181
507.078124	29105.740957	31.116199
507.592116	29172.039899	31.121216
508.315773	29203.159698	31.126234
508.856852	29240.539939	31.131252
509.043832	29296.962862	31.136269
509.859177	29337.430485	31.141287
510.437569	29405.009896	31.146304
510.829040	29441.746512	31.151322
511.451401	29473.322015	31.156340
511.644234	29527.258903	31.161357
512.376502	29567.359079	31.166375
512.747688	29608.692505	31.171392
513.305018	29656.547433	31.176410
514.259335	29687.043242	31.181428
514.254251	29734.764148	31.186445
514.696803	29780.209305	31.191463
514.981201	29841.450819	31.196480
515.486550	29893.147890	31.201498
515.809326	29937.057991	31.206516
516.534614	29994.779163	31.211533
517.110495	30024.432680	31.216551
517.453228	30073.182275	31.221568
517.743127	30117.170817	31.226586
518.752877	30164.157427	31.231604
518.967712	30206.455048	31.236621
519.627496	30256.629198	31.241639
519.806272	30301.270660	31.246656
520.616884	30350.590471	31.251674
521.143844	30402.096198	31.256692
521.412159	30455.521885	31.261709
521.803354	30511.851917	31.266727
522.529739	30554.561187	31.271744
522.493317	30605.763068	31.276762
523.461687	30668.301549	31.281780
523.752874	30733.633701	31.286797
524.305570	30785.063746	31.291815
525.091862	30833.003970	31.296832
525.835154	30890.936510	31.301850
526.622622	30933.280120	31.306868
527.038946	30998.750336	31.311885
527.876047	31036.372632	31.316903
528.447164	31091.485427	31.321920
528.464588	31146.879144	31.326938
529.191537	31191.334534	31.331956
529.912542	31243.842344	31.336973
530.497487	31282.478531	31.341991
530.512529	31340.526537	31.347008
531.274799	31386.326897	31.352026
531.950683	31436.104254	31.357044
532.241053	31494.728818	31.362061
532.956139	31542.515536	31.367079
533.751593	31590.670862	31.372096
534.208461	31642.895380	31.377114
534.930399	31697.215355	31.382132
534.995893	31747.384674	31.387149
535.607620	31793.942925	31.392167
536.361695	31839.761600	31.397184
537.429847	31874.340807	31.402202
538.307657	31920.205511	31.407220
538.605586	31959.423798	31.412237
539.416476	32010.704372	31.417255
540.125927	32035.827528	31.422272
540.301169	32084.269645	31.427290
541.035251	32110.026161	31.432308
541.057362	32158.007894	31.437325
541.688894	32197.237867	31.442343
542.452091	32240.440522	31.447360
542.522753	32283.104564	31.452378
543.141293	32329.271879	31.457396
543.576319	32378.277675	31.462413
543.734373	32434.911113	31.467431
544.409535	32481.400763	31.472448
544.735347	32537.707085	31.477466
545.218733	32585.522293	31.482484
545.539485	32656.195229	31.487501
545.934087	32707.142732	31.492519
546.703416	32755.119412	31.497536
547.033793	32830.350691	31.502554
547.590336	32888.838125	31.507572
547.829000	32960.156877	31.512589
548.362007	33031.348419	31.517607
548.798698	33093.163006	31.522624
549.042032	33164.106335	31.527642
550.072111	33236.731126	31.532660
550.144683	33310.315806	31.537677
550.908406	33373.834848	31.542695
552.220660	33412.813107	31.547712
553.190931	33458.723345	31.552730
554.223158	33497.517707	31.557748
554.455519	33552.889795	31.562765
555.191013	33593.831668	31.567783
555.812724	33635.751652	31.572800
556.563613	33667.730000	31.577818
557.136452	33706.524970	31.582836
557.306362	33748.885865	31.587853
557.787481	33783.452198	31.592871
558.524705	33832.162843	31.597888
558.748375	33890.348858	31.602906
559.543465	33926.021637	31.607924
559.705033	33976.720992	31.612941
559.778291	34037.475583	31.617959
560.444149	34096.097258	31.622976
560.850052	34155.815976	31.627994
561.482196	34207.798257	31.633012
562.352017	34280.964986	31.638029
563.360768	34329.108345	31.643047
563.956610	34361.315505	31.648064
564.324693	34421.738723	31.653082
564.806988	34478.637536	31.658100
565.576307	34529.004581	31.663117
566.047777	34577.432996	31.668135
566.995295	34620.787740	31.673152
567.619050	34671.485316	31.678170
567.867248	34712.305152	31.683188
568.476948	34777.445052	31.688205
568.864504	34829.911327	31.693223
569.460483	34878.846975	31.698240
570.106477	34931.267708	31.703258
570.682744	34972.441022	31.708276
570.935811	35039.063946	31.713293
571.308429	35103.966507	31.718311
572.234958	35165.297181	31.723328
572.495015	35217.984460	31.728346
573.043724	35273.653621	31.733364
573.498916	35347.259272	31.738381
573.563989	35417.878144	31.743399
574.554389	35471.130320	31.748416
575.069151	35550.176796	31.753434
575.892717	35607.104895	31.758452
576.387311	35673.813367	31.763469
577.141121	35724.801717	31.768487
578.822444	35770.622591	31.773504
579.429080	35827.075995	31.778522
580.259520	35880.482043	31.783540
581.024971	35923.589173	31.788557
581.195846	35964.692882	31.793575
581.783009	36007.921180	31.798592
582.179073	36074.183523	31.803610
582.633708	36112.312151	31.808628
582.808705	36169.822530	31.813645
582.849709	36229.709447	31.818663
583.521853	36292.676531	31.823680
583.845680	36353.561721	31.828698
584.807680	36415.812331	31.833716
585.376104	36478.841381	31.838733
585.856272	36541.298241	31.843751
586.490572	36593.201912	31.848768
586.971536	36663.390923	31.853786
587.445534	36717.022443	31.858804
588.329666	36797.443031	31.863821
588.553559	36876.578115	31.868839
589.334210	36926.066398	31.873856
589.492490	37005.569505	31.878874
590.354700	37075.678222	31.883892
591.009842	37137.183562	31.888909
591.489651	37203.562479	31.893927
591.972590	37252.283436	31.898944
592.394491	37325.378814	31.903962
593.130871	37378.811172	31.908980
593.544052	37450.450427	31.913997
594.075127	37516.048806	31.919015
594.614343	37577.448556	31.924032
595.167606	37666.218571	31.929050
595.712104	37723.130046	31.934068
596.185897	37791.311073	31.939085
596.721806	37869.537375	31.944103
597.574051	37934.711813	31.949120
597.994000	38013.024167	31.954138
598.426310	38095.418839	31.959156
599.601916	38168.336336	31.964173
600.277782	38235.030685	31.969191
601.891127	38275.279668	31.974208
603.210257	38324.903792	31.979226
604.187900	38362.998153	31.984244
605.114950	38398.639134	31.989261
605.345316	38445.997376	31.994279
605.875950	38480.583547	31.999296
606.404674	38541.196104	32.004314
606.385444	38573.206278	32.009332
606.950867	38615.383948	32.014349
607.161418	38689.100493	32.019367
607.718482	38749.052569	32.024384
608.114535	38811.613246	32.029402
608.392007	38879.489924	32.034420
609.253740	38949.688063	32.039437
609.278077	39022.884370	32.044455
609.948001	39084.450713	32.049472
610.484279	39168.414396	32.054490
610.976105	39243.324008	32.059508
611.602454	39314.932278	32.064525
611.775639	39401.567295	32.069543
612.576863	39484.352393	32.074560
613.082148	39571.422604	32.079578
613.531850	39652.262222	32.084596
614.490503	39731.193739	32.089613
614.795266	39823.304332	32.094631
615.770088	39897.530831	32.099648
616.905482	39972.393967	32.104666
618.089953	40041.027922	32.109684
619.405563	40098.905321	32.114701
619.877958	40160.387984	32.119719
620.613524	40206.799341	32.124736
621.182322	40262.609999	32.129754
621.831130	40339.499411	32.134772
622.085556	40385.223654	32.139789
622.731812	40448.117943	32.144807
623.242380	40507.455342	32.149824
623.703496	40583.174136	32.154842
624.310697	40639.045890	32.159860
624.813317	40712.987534	32.164877
625.513770	40786.631651	32.169895
626.027554	40843.504313	32.174912
627.101400	40918.087932	32.179930
627.730972	40980.608015	32.184948
628.276847	41053.322278	32.189965
628.468136	41110.968746	32.194983
629.024535	41181.462657	32.200000
629.890501	41226.759710	32.205018
630.871052	41304.576953	32.210036
632.478044	41334.505142	32.215053
632.985168	41395.762096	32.220071
633.786734	41439.908649	32.225088
634.743816	41488.865703	32.230106
635.264505	41526.549721	32.235124
636.172634	41556.994600	32.240141
636.238995	41592.544084	32.245159
636.646971	41624.233354	32.250176
637.425515	41667.393044	32.255194
637.347656	41721.705013	32.260212
637.912698	41770.538162	32.265229
638.180497	41821.251456	32.270247
638.684705	41879.934585	32.275264
638.906855	41956.737095	32.280282
638.877987	42020.262837	32.285300
640.087998	42093.853300	32.290317
640.484881	42174.914813	32.295335
641.078465	42244.819494	32.300352
641.867693	42320.967949	32.305370
642.161458	42406.224024	32.310388
643.250482	42465.639533	32.315405
643.848433	42556.866232	32.320423
644.703384	42607.967724	32.325440
645.679171	42695.063460	32.330458
646.292835	42756.752472	32.335476
647.702352	42817.906165	32.340493
647.837379	42878.187714	32.345511
648.524481	42946.217009	32.350528
649.257616	43007.369386	32.355546
649.214247	43075.955459	32.360564
650.348961	43152.062913	32.365581
650.829713	43229.115291	32.370599
651.797348	43294.952773	32.375616
652.326545	43365.787865	32.380634
652.970238	43430.369162	32.385652
654.059518	43508.499779	32.390669
654.375996	43588.422129	32.395687
655.096869	43632.773534	32.400704
656.043666	43706.928505	32.405722
656.525881	43765.198205	32.410740
657.254225	43828.403043	32.415757
657.789303	43899.930611	32.420775
658.521013	43970.810339	32.425792
658.987061	44039.865183	32.430810
659.482850	44113.168061	32.435828
660.281187	44189.063813	32.440845
660.429542	44258.853886	32.445863
661.050716	44347.234627	32.450880
662.099301	44418.177388	32.455898
662.600430	44489.788604	32.460916
663.341656	44561.603549	32.465933
663.664556	44651.616768	32.470951
664.142048	44733.677004	32.475968
665.236276	44802.836154	32.480986
665.681203	44893.234517	32.486004
666.661482	44976.440970	32.491021
666.920283	45063.530469	32.496039
667.622249	45145.236552	32.501056
668.169529	45217.164985	32.506074
668.941348	45316.396175	32.511092
669.695847	45394.959415	32.516109
670.956028	45474.607706	32.521127
671.624713	45535.753785	32.526144
672.657076	45602.820134	32.531162
673.388345	45674.000049	32.536180
674.284376	45725.027560	32.541197
675.296407	45789.095221	32.546215
676.359930	45851.594816	32.551232
677.547739	45893.841097	32.556250
677.659175	45958.478011	32.561268
678.583166	46001.011228	32.566285
679.080190	46041.262730	32.571303
679.771876	46086.284712	32.576320
680.675803	46115.029591	32.581338
681.451269	46166.381338	32.586356
681.843673	46197.591578	32.591373
682.355660	46244.711786	32.596391
682.683529	46298.537527	32.601408
683.549328	46345.498517	32.606426
683.768594	46398.379432	32.611444
684.055127	46449.086463	32.616461
684.849581	46515.901722	32.621479
685.451809	46584.469841	32.626496
686.137504	46641.483455	32.631514
685.877039	46708.798846	32.636532
686.627928	46780.191277	32.641549
686.837272	46866.147941	32.646567
687.289588	46960.454709	32.651584
687.860367	47046.684057	32.656602
688.059989	47148.968676	32.661620
688.667534	47251.634872	32.666637
689.352390	47348.248175	32.671655
690.430399	47458.852050	32.676672
691.375697	47549.338446	32.681690
691.806714	47648.328770	32.686708
692.580582	47734.268781	32.691725
693.757472	47836.338885	32.696743
694.351054	47926.998853	32.701760
695.008559	48012.264628	32.706778
695.657136	48113.934016	32.711796
696.326962	48215.016239	32.716813
697.239887	48313.908350	32.721831
697.918752	48397.953397	32.726848
698.685201	48495.822230	32.731866
699.212002	48590.175340	32.736884
700.119298	48687.728217	32.741901
701.064530	48778.567865	32.746919
701.892603	48869.919937	32.751936
703.188930	48944.205250	32.756954
703.809981	49030.015312	32.761972
704.767335	49103.640366	32.766989
705.817127	49185.180193	32.772007
706.183391	49259.604543	32.777024
707.412022	49346.329416	32.782042
707.886186	49419.924958	32.787060
708.386016	49488.634189	32.792077
709.106015	49569.652201	32.797095
709.825388	49643.002834	32.802112
710.724643	49716.763018	32.807130
711.287891	49801.452340	32.812148
711.958697	49877.215215	32.817165
712.131422	49952.795360	32.822183
712.693043	50054.325246	32.827200
713.574444	50141.913247	32.832218
714.136693	50236.593937	32.837236
714.488582	50321.339413	32.842253
715.605206	50407.872847	32.847271
716.096814	50513.023399	32.852288
716.720022	50600.438218	32.857306
717.112357	50703.884968	32.862324
717.818267	50791.628091	32.867341
718.730365	50893.091904	32.872359
719.448576	50988.388521	32.877376
720.499200	51061.800424	32.882394
720.900281	51174.678996	32.887412
721.904541	51259.131374	32.892429
722.890111	51343.814612	32.897447
723.758002	51435.841932	32.902464
724.727878	51512.076687	32.907482
725.499549	51611.024975	32.912500
725.862530	51685.392952	32.917517
726.862280	51756.772414	32.922535
727.117357	51845.374924	32.927552
728.011001	51915.660723	32.932570
728.447811	52005.408901	32.937588
728.963884	52075.157524	32.942605
729.933304	52163.946742	32.947623
730.013142	52252.750615	32.952640
730.844165	52342.113086	32.957658
731.345947	52438.637057	32.962676
732.064395	52541.171205	32.967693
733.228292	52633.543852	32.972711
733.496274	52733.424401	32.977728
734.647634	52822.300302	32.982746
735.095380	52931.590093	32.987764
735.712862	53014.553661	32.992781
736.906906	53123.076925	32.997799
737.564291	53217.115323	33.002816
738.806295	53293.703839	33.007834
740.182850	53384.364527	33.012852
741.423124	53468.073716	33.017869
742.118544	53537.722174	33.022887
742.752987	53627.123027	33.027904
743.547273	53694.184510	33.032922
744.415180	53777.109977	33.037940
744.561827	53853.635202	33.042957
745.910379	53922.141102	33.047975
746.184581	54008.166439	33.052992
747.017097	54081.035124	33.058010
747.623278	54178.643439	33.063028
748.463015	54258.145123	33.068045
749.637399	54330.187528	33.073063
749.961944	54423.130573	33.078080
750.756060	54493.701171	33.083098
751.564305	54580.708536	33.088116
752.121287	54662.520323	33.093133
752.792634	54747.004960	33.098151
753.129423	54845.198103	33.103168
754.300733	54932.810453	33.108186
754.824880	55032.774194	33.113204
755.482253	55136.374538	33.118221
756.326069	55214.072498	33.123239
756.801677	55309.515672	33.128256
757.800951	55393.740448	33.133274
758.510364	55489.404926	33.138292
759.299475	55585.669565	33.143309
760.331856	55677.238040	33.148327
760.850276	55769.308814	33.153344
761.722141	55864.910383	33.158362
762.414998	55959.821700	33.163380
763.196167	56042.922722	33.168397
764.144314	56133.622677	33.173415
764.607426	56232.869674	33.178432
765.685506	56317.047481	33.183450
766.597890	56414.692165	33.188468
767.063936	56516.530633	33.193485
768.601534	56582.651542	33.198503
769.158476	56663.985140	33.203520
770.235992	56746.989644	33.208538
770.736061	56833.065865	33.213556
771.556320	56913.213358	33.218573
772.848503	56983.331533	33.223591
773.144163	57074.775413	33.228608
774.181674	57145.460660	33.233626
775.120416	57232.628800	33.238644
776.059447	57306.433329	33.243661
777.045469	57371.965552	33.248679
778.222463	57440.543659	33.253696
779.141316	57494.328298	33.258714
779.831724	57550.115931	33.263732
780.400461	57601.026786	33.268749
781.158711	57665.498132	33.273767
781.274177	57727.693650	33.278784
782.015352	57795.845771	33.283802
782.145819	57857.830698	33.288820
782.697306	57928.023981	33.293837
783.364352	58016.200893	33.298855
783.664707	58107.591881	33.303872
784.154774	58208.253429	33.308890
784.958407	58299.170414	33.313908
785.487770	58403.699985	33.318925
786.406259	58512.557573	33.323943
786.875835	58619.050725	33.328960
787.436673	58711.513618	33.333978
788.254794	58828.895006	33.338996
788.862859	58943.234335	33.344013
789.675616	59053.584695	33.349031
790.500070	59167.617848	33.354048
791.473032	59279.270037	33.359066
792.642593	59395.212792	33.364084
793.502045	59511.182148	33.369101
794.340206	59608.633590	33.374119
795.259989	59715.456348	33.379136
796.369287	59825.490255	33.384154
797.049338	59923.443291	33.389172
797.685782	60038.441401	33.394189
798.369185	60144.262752	33.399207
799.532455	60242.030114	33.404224
799.985492	60352.567086	33.409242
800.942202	60471.369746	33.414260
801.367448	60583.934862	33.419277
802.275538	60693.368451	33.424295
803.292879	60824.303357	33.429312
803.848975	60927.723054	33.434330
804.661766	61038.147495	33.439348
805.008533	61162.629026	33.444365
806.032107	61281.273731	33.449383
806.808542	61407.512267	33.454400
807.695454	61522.572267	33.459418
808.832763	61635.347970	33.464436
809.833666	61758.676022	33.469453
811.012592	61861.447795	33.474471
811.760963	61980.413800	33.479488
812.768694	62090.710663	33.484506
814.086651	62197.853688	33.489524
814.870975	62301.343826	33.494541
815.835731	62396.443008	33.499559
816.450661	62493.534404	33.504576
817.125771	62585.060777	33.509594
818.063941	62688.679167	33.514612
818.922057	62789.170079	33.519629
820.545806	62858.754737	33.524647
821.768242	62955.627932	33.529664
822.737505	63034.700771	33.534682
823.270482	63113.523614	33.539700
823.827289	63207.518335	33.544717
824.956101	63289.745027	33.549735
825.056419	63379.909835	33.554752
825.868613	63473.686633	33.559770
826.798771	63563.329666	33.564788
827.011234	63673.349247	33.569805
827.599433	63772.676001	33.574823
828.762330	63876.781602	33.579840
829.008874	63982.132530	33.584858
830.048232	64080.627789	33.589876
830.818146	64188.668172	33.594893
832.059654	64269.230458	33.599911
833.233455	64371.882980	33.604928
833.873943	64457.197398	33.609946
834.987462	64531.878145	33.614964
835.378893	64631.620796	33.619981
835.888384	64715.428248	33.624999
836.682350	64824.612093	33.630016
837.202459	64933.234917	33.635034
838.151196	65031.256651	33.640052
838.496406	65143.695776	33.645069
839.200973	65239.628609	33.650087
840.135264	65346.459549	33.655104
840.618385	65461.140601	33.660122
841.781892	65583.965461	33.665140
842.079154	65701.491479	33.670157
843.321689	65816.422057	33.675175
844.031606	65945.341834	33.680192
844.957912	66056.969332	33.685210
845.665540	66189.848185	33.690228
846.482341	66311.324928	33.695245
847.546453	66421.224838	33.700263
848.660471	66553.134938	33.705280
849.524734	66662.474899	33.710298
850.600055	66786.098987	33.715316
851.329962	66909.869346	33.720333
852.158472	67023.718108	33.725351
852.792232	67144.117320	33.730368
853.974483	67264.888147	33.735386
855.109121	67377.133141	33.740404
855.943241	67490.503068	33.745421
857.460357	67591.711409	33.750439
858.426957	67708.240525	33.755456
858.883552	67818.475699	33.760474
860.264032	67926.719218	33.765492
861.255398	68030.355611	33.770509
861.828727	68139.005347	33.775527
862.620993	68242.353241	33.780544
863.326802	68357.190467	33.785562
864.153652	68463.751672	33.790580
865.175928	68575.718182	33.795597
866.253706	68689.079645	33.800615
867.170551	68795.121896	33.805632
867.413053	68900.959917	33.810650
868.423001	69011.666336	33.815668
869.061780	69136.874752	33.820685
869.716318	69254.507149	33.825703
870.617926	69376.158368	33.830720
871.191563	69510.604097	33.835738
872.458996	69621.890798	33.840756
872.978834	69754.134102	33.845773
873.876856	69883.167170	33.850791
874.768269	70009.439156	33.855808
875.683110	70136.814481	33.860826
876.845203	70237.910820	33.865844
877.974941	70363.595495	33.870861
878.883672	70480.124197	33.875879
880.002116	70595.619919	33.880896
880.642203	70714.451480	33.885914
881.519349	70829.166353	33.890932
881.935009	70961.592446	33.895949
882.632071	71074.808248	33.900967
883.747404	71195.859227	33.905984
884.355582	71337.658040	33.911002
885.341530	71463.170615	33.916020
885.792653	71590.302407	33.921037
886.775402	71725.472318	33.926055
887.319679	71855.448332	33.931072
888.233235	71996.556133	33.936090
889.363745	72125.039570	33.941108
890.122622	72247.723511	33.946125
890.763527	72376.731922	33.951143
891.917985	72496.127104	33.956160
892.805655	72624.084529	33.961178
894.202601	72745.407616	33.966196
894.774097	72872.539776	33.971213
896.163777	72981.566371	33.976231
897.596303	73102.082519	33.981248
898.386531	73225.753325	33.986266
899.411992	73323.503739	33.991284
900.511650	73441.648508	33.996301
901.437770	73540.194107	34.001319
902.603527	73654.579232	34.006336
903.342628	73770.413969	34.011354
904.155720	73877.548342	34.016372
905.008142	74009.800955	34.021389
905.346597	74122.674657	34.026407
906.205313	74246.200868	34.031424
906.866619	74378.291246	34.036442
907.749867	74488.155279	34.041460
908.633605	74627.969849	34.046477
908.829112	74773.173137	34.051495
909.709384	74905.464549	34.056512
910.830236	75042.118574	34.061530
911.886898	75171.359588	34.066548
912.486432	75310.460252	34.071565
913.592574	75450.894766	34.076583
915.041759	75573.432987	34.081600
915.621207	75718.534903	34.086618
916.897326	75862.144060	34.091636
917.984057	76001.352083	34.096653
918.635671	76140.221751	34.101671
919.634367	76281.773454	34.106688
920.380396	76406.266514	34.111706
921.285464	76543.610644	34.116724
922.116114	76683.592593	34.121741
922.636568	76840.127416	34.126759
923.661488	76981.628701	34.131776
924.715539	77133.985495	34.136794
925.600391	77286.978448	34.141812
926.496849	77430.066020	34.146829
927.512466	77583.785758	34.151847
928.586288	77720.616029	34.156864
929.194420	77881.008216	34.161882
930.275649	78028.053810	34.166900
931.594232	78163.461255	34.171917
932.592521	78308.005078	34.176935
933.917533	78444.254399	34.181952
934.896995	78582.180824	34.186970
935.820062	78720.047841	34.191988
936.745340	78852.494709	34.197005
938.050085	78993.931032	34.202023
939.284129	79107.751414	34.207040
940.309606	79245.389720	34.212058
941.022939	79374.187066	34.217076
942.038562	79502.157231	34.222093
943.216088	79623.972132	34.227111
944.311069	79740.905478	34.232128
945.262972	79881.210187	34.237146
946.183357	79998.142078	34.242164
947.392462	80116.279358	34.247181
948.398079	80232.300180	34.252199
949.387493	80342.346628	34.257216
949.814305	80463.638514	34.262234
950.482863	80589.369682	34.267252
951.720655	80721.326904	34.272269
952.392920	80842.415840	34.277287
953.835823	80945.944491	34.282304
954.673782	81051.958307	34.287322
955.691585	81168.133767	34.292340
956.670653	81272.347777	34.297357
957.735072	81371.468524	34.302375
958.439181	81492.631607	34.307392
959.089539	81616.903911	34.312410
960.010346	81727.892043	34.317428
960.764239	81838.389549	34.322445
961.207521	81969.314946	34.327463
961.997034	82100.512889	34.332480
963.045704	82223.875071	34.337498
963.692201	82371.457445	34.342516
964.718374	82501.264843	34.347533
965.418232	82646.347686	34.352551
966.169779	82786.823745	34.357568
967.052084	82949.180661	34.362586
967.869175	83098.599513	34.367604
968.905632	83261.635426	34.372621
969.665293	83415.747350	34.377639
970.314546	83563.197807	34.382656
971.579613	83730.026823	34.387674
972.548494	83891.085536	34.392692
974.214370	84036.479560	34.397709
974.992227	84190.245733	34.402727
976.082800	84355.146857	34.407744
977.302958	84509.190108	34.412762
978.404326	84656.642546	34.417780
979.713510	84799.424080	34.422797
980.827075	84955.923738	34.427815
981.844241	85083.412673	34.432832
982.864450	85242.757803	34.437850
984.100222	85383.941716	34.442868
985.845702	85495.261210	34.447885
986.718185	85635.589228	34.452903
987.611262	85774.143120	34.457920
988.483980	85913.492090	34.462938
989.438901	86046.146872	34.467956
990.461594	86189.015933	34.472973
990.966398	86327.295567	34.477991
992.300745	86461.541483	34.483008
992.912682	86612.124276	34.488026
993.457998	86756.195567	34.493044
994.787298	86914.273655	34.498061
995.443650	87066.338983	34.503079
996.657472	87216.794675	34.508096
997.030397	87373.268409	34.513114
997.834939	87545.642637	34.518132
999.090639	87701.599498	34.523149
999.547225	87884.202092	34.528167
1000.514766	88039.905051	34.533184
1001.456851	88217.715969	34.538202
1002.288235	88383.681943	34.543220
1003.447636	88557.352831	34.548237
1004.831322	88727.039388	34.553255
1006.106042	88879.855987	34.558272
1007.339264	89041.514235	34.563290
1008.262283	89208.141650	34.568308
1009.795566	89361.051566	34.573325
1010.449634	89524.523631	34.578343
1012.884194	89647.747185	34.583360
1014.028295	89788.593145	34.588378
1014.832338	89936.602631	34.593396
1016.074521	90067.840535	34.598413
1017.231726	90204.383613	34.603431
1018.404570	90332.596867	34.608448
1019.076610	90465.861225	34.613466
1019.971071	90608.221431	34.618484
1021.272499	90734.523443	34.623501
1021.796837	90866.732272	34.628519
1022.724219	90982.908584	34.633536
1023.612983	91112.343699	34.638554
1024.027711	91256.464024	34.643572
1025.308801	91376.210103	34.648589
1025.499475	91529.861910	34.653607
1026.420270	91673.648052	34.658624
1027.597459	91817.620560	34.663642
1028.387085	91976.555724	34.668660
1029.736566	92125.488668	34.673677
1030.754915	92279.211146	34.678695
1031.803782	92429.568953	34.683712
1032.901162	92575.211003	34.688730
1033.744742	92736.256121	34.693748
1034.556915	92892.111419	34.698765
1035.523567	93057.676228	34.703783
1036.301409	93222.697398	34.708800
1037.432630	93393.414497	34.713818
1038.307051	93566.472672	34.718836
1039.447703	93745.317308	34.723853
1040.154505	93917.399316	34.728871
1041.257169	94088.562736	34.733888
1042.531786	94260.730652	34.738906
1043.652196	94429.026354	34.743924
1045.144974	94600.192260	34.748941
1046.237907	94764.083215	34.753959
1047.219353	94943.184460	34.758976
1048.624224	95099.152272	34.763994
1049.313906	95287.488362	34.769012
1050.063075	95444.243886	34.774029
1051.789064	95622.879054	34.779047
1053.094881	95782.146335	34.784064
1054.626346	95933.231005	34.789082
1055.806218	96103.237429	34.794100
1057.054505	96253.902414	34.799117
1057.917011	96416.405571	34.804135
1059.114515	96568.694981	34.809152
1060.333897	96730.723517	34.814170
1061.472187	96873.738539	34.819188
1063.507433	97004.256431	34.824205
1064.324088	97158.220171	34.829223
1065.298563	97285.040663	34.834240
1066.544747	97424.774726	34.839258
1067.207258	97584.824497	34.844276
1068.342602	97725.502755	34.849293
1069.344984	97869.273928	34.854311
1070.077050	98011.628261	34.859328
1071.494149	98158.035667	34.864346
1072.358302	98311.935402	34.869364
1073.524445	98453.524257	34.874381
1074.605416	98601.464735	34.879399
1075.522353	98758.131233	34.884416
1076.358028	98917.939397	34.889434
1076.884048	99070.481584	34.894452
1078.112330	99222.288365	34.899469
1079.177213	99393.697342	34.904487
1079.939300	99560.080273	34.909504
1080.788083	99730.628264	34.914522
1081.792654	99888.173639	34.919540
1083.052976	100053.097470	34.924557
1083.857616	100232.316668	34.929575
1084.594256	100412.656266	34.934592
1085.989532	100578.580519	34.939610
1086.971262	100763.908914	34.944628
1087.783058	100933.762054	34.949645
1088.968020	101119.825549	34.954663
1089.750272	101302.139229	34.959680
1091.287150	101463.835706	34.964698
1091.704208	101634.676704	34.969716
1093.176791	101796.056681	34.974733
1094.277259	101971.643168	34.979751
1095.362828	102154.615638	34.984768
1096.533178	102308.831044	34.989786
1097.225623	102480.391992	34.994804
1098.354514	102648.963243	34.999821
1099.587164	102830.111793	35.004839
1100.389356	103025.508979	35.009856
1101.751132	103204.815370	35.014874
1102.299365	103402.422737	35.019892
1103.704967	103579.039886	35.024909
1104.695742	103775.975547	35.029927
1105.126654	103961.899216	35.034944
1106.745570	104152.839180	35.039962
1107.347372	104361.164778	35.044980
1108.442323	104555.999653	35.049997
1109.772496	104762.182015	35.055015
1110.926031	104975.657983	35.060032
1112.612300	105166.423311	35.065050
1113.504029	105367.420901	35.070068
1115.655579	105527.939606	35.075085
1117.696511	105714.958758	35.080103
1118.464928	105906.001316	35.085120
1119.788741	106070.750618	35.090138
1120.501419	106263.046102	35.095156
1121.683299	106437.547580	35.100173
1122.859716	106619.700663	35.105191
1123.724594	106813.469489	35.110208
1125.154223	106999.927462	35.115226
1125.860054	107176.234854	35.120244
1127.189131	107368.639284	35.125261
1127.931632	107570.222938	35.130279
1128.921781	107750.603430	35.135296
1130.385104	107933.300804	35.140314
1131.371232	108145.246934	35.145332
1132.228823	108332.214004	35.150349
1133.323295	108533.987507	35.155367
1134.545262	108724.734893	35.160384
1135.712540	108927.778601	35.165402
1136.764761	109121.748650	35.170420
1138.528646	109307.078345	35.175437
1140.978098	109467.166466	35.180455
1142.636494	109640.660354	35.185472
1144.172255	109804.080543	35.190490
1145.065258	109975.764992	35.195508
1146.132624	110141.607836	35.200525
1147.212347	110301.065713	35.205543
1148.595397	110476.333090	35.210560
1149.775068	110617.713715	35.215578
1150.779576	110784.090214	35.220596
1152.093508	110942.322534	35.225613
1153.223984	111108.021552	35.230631
1154.165286	111261.035130	35.235648
1155.238385	111436.701893	35.240666
1156.094780	111600.891107	35.245684
1156.742177	111784.661369	35.250701
1157.697060	111953.789344	35.255719
1158.715589	112129.900270	35.260736
1159.984664	112299.700565	35.265754
1160.837148	112490.510176	35.270772
1161.704374	112674.997518	35.275789
1162.810827	112870.809581	35.280807
1163.437745	113062.927179	35.285824
1164.552852	113248.048844	35.290842
1165.688109	113443.632205	35.295860
1166.889860	113634.050057	35.300877
1168.795082	113819.805221	35.305895
1169.452306	113995.823049	35.310912
1171.086054	114174.809882	35.315930
1171.856549	114356.917450	35.320948
1172.856824	114548.033604	35.325965
1174.212320	114728.438139	35.330983
1174.562862	114929.723036	35.336000
1175.525899	115125.422697	35.341018
1176.396038	115336.696442	35.346036
1177.361142	115536.807412	35.351053
1178.482888	115745.496247	35.356071
1179.128935	115974.383786	35.361088
1180.604930	116189.554738	35.366106
1181.353667	116415.438970	35.371124
1182.633007	116638.032051	35.376141
1183.662429	116874.921405	35.381159
1184.686658	117116.488711	35.386176
1185.776308	117344.439932	35.391194
1187.068454	117600.524720	35.396212
1188.252405	117830.516800	35.401229
1189.760086	118078.676910	35.406247
1190.380806	118336.741657	35.411264
1192.202154	118567.749452	35.416282
1194.108397	118797.288001	35.421300
1195.668984	119017.737330	35.426317
1197.150083	119248.971502	35.431335
1198.211617	119479.161766	35.436352
1200.023191	119706.391800	35.441370
1201.027446	119922.048954	35.446388
1202.113146	120148.654703	35.451405
1203.547802	120369.819402	35.456423
1205.021100	120594.742761	35.461440
1206.799578	120794.426932	35.466458
1208.344429	121002.096002	35.471476
1209.629838	121202.092447	35.476493
1210.894482	121411.470653	35.481511
1211.979897	121615.405787	35.486528
1213.802107	121808.842568	35.491546
1215.334226	122018.459750	35.496564
1216.295631	122210.976842	35.501581
1217.717268	122392.990175	35.506599
1218.892865	122583.826995	35.511616
1219.766706	122777.261965	35.516634
1221.421378	122977.437673	35.521652
1222.753149	123170.939031	35.526669
1223.626351	123374.186398	35.531687
1224.215585	123583.488798	35.536704
1225.365786	123771.410131	35.541722
1226.346635	123990.459339	35.546740
1227.763952	124195.181253	35.551757
1229.641049	124390.628194	35.556775
1230.673908	124593.857545	35.561792
1232.550255	124794.819984	35.566810
1234.061161	124976.821772	35.571828
1235.156925	125174.151693	35.576845
1236.234445	125363.425729	35.581863
1237.500377	125559.196627	35.586880
1238.552355	125746.677676	35.591898
1239.789376	125940.478772	35.596916
1240.925766	126142.307427	35.601933
1242.299075	126336.887006	35.606951
1242.878237	126548.125490	35.611968
1244.208357	126743.145714	35.616986
1245.228731	126953.122848	35.622004
1245.654832	127166.621504	35.627021
1247.414844	127380.611232	35.632039
1248.034495	127603.573901	35.637056
1249.068896	127807.876565	35.642074
1250.184306	128023.029152	35.647092
1250.873325	128242.613639	35.652109
1252.016903	128461.719082	35.657127
1253.044615	128692.860768	35.662144
1254.315770	128917.144996	35.667162
1255.238282	129158.586745	35.672180
1255.795344	129408.367429	35.677197
1256.665621	129645.360015	35.682215
1258.757455	129891.139452	35.687232
1259.512824	130134.720453	35.692250
1260.865435	130388.966136	35.697268
1261.869468	130637.187213	35.702285
1263.696566	130894.476847	35.707303
1265.137936	131139.562240	35.712320
1266.939704	131392.043393	35.717338
1268.437880	131638.568334	35.722356
1269.703022	131890.596996	35.727373
1271.179974	132126.874419	35.732391
1272.238126	132383.238345	35.737408
1273.711897	132628.380654	35.742426
1275.127642	132869.034334	35.747444
1275.987913	133113.368943	35.752461
1277.510706	133361.830031	35.757479
1278.601749	133616.651918	35.762496
1280.133255	133866.852186	35.767514
1281.131884	134120.273533	35.772532
1282.523859	134381.035279	35.777549
1283.754975	134625.218778	35.782567
1285.349285	134879.511229	35.787584
1286.831068	135130.984553	35.792602
1288.358270	135384.315898	35.797620
1289.447326	135639.078019	35.802637
1290.371810	135875.017829	35.807655
1292.263754	136149.314246	35.812672
1293.327683	136399.738029	35.817690
1295.096456	136640.906689	35.822708
1296.449871	136887.407007	35.827725
1297.981676	137138.887538	35.832743
1299.193171	137393.541668	35.837760
1300.763288	137640.049882	35.842778
1301.904449	137876.576853	35.847796
1302.733569	138135.369528	35.852813
1304.267817	138375.562619	35.857831
1305.471690	138634.398750	35.862848
1306.829907	138884.830816	35.867866
1308.286636	139136.313513	35.872884
1309.431884	139388.052369	35.877901
1310.621009	139638.378507	35.882919
1312.110181	139892.359266	35.887936
1313.686219	140142.130805	35.892954
1315.406762	140383.207747	35.897972
1316.607053	140644.253452	35.902989
1317.491975	140880.970690	35.908007
1318.462082	141135.566299	35.913024
1319.994176	141402.674586	35.918042
1321.192490	141656.361524	35.923060
1322.363087	141917.929071	35.928077
1323.317507	142177.759106	35.933095
1324.640896	142444.529563	35.938112
1325.734348	142715.346944	35.943130
1327.288058	142990.046705	35.948148
1328.295285	143263.824417	35.953165
1330.038818	143527.224327	35.958183
1331.509617	143780.831189	35.963200
1333.480698	144035.244970	35.968218
1335.434762	144280.546014	35.973236
1337.620890	144519.622273	35.978253
1339.062805	144743.390415	35.983271
1340.417611	144957.815847	35.988288
1341.515898	145180.311987	35.993306
1342.704916	145392.434124	35.998324
1344.107758	145605.447968	36.003341
1345.264438	145833.746546	36.008359
1346.043467	146063.719448	36.013376
1347.283845	146282.863880	36.018394
1348.860121	146516.195505	36.023412
1349.795337	146755.404563	36.028429
1350.882127	146988.059162	36.033447
1351.985931	147228.765353	36.038464
1352.784369	147476.993136	36.043482
1354.254046	147729.930966	36.048500
1355.253820	147998.800605	36.053517
1356.489047	148269.307416	36.058535
1357.286728	148536.514998	36.063552
1358.343500	148820.194101	36.068570
1359.545282	149097.662480	36.073588
1360.812683	149380.068299	36.078605
1361.976584	149674.414990	36.083623
1363.540394	149970.803363	36.088640
1364.966056	150269.449089	36.093658
1366.320085	150554.994960	36.098676
1367.393372	150861.846030	36.103693
1369.201762	151151.925431	36.108711
1371.779877	151423.705075	36.113728
1373.908713	151691.426106	36.118746
1376.175509	151953.494880	36.123764
1377.369033	152226.561590	36.128781
1378.825359	152488.095632	36.133799
1380.044800	152763.444994	36.138816
1381.019679	153029.691767	36.143834
1382.484123	153285.877466	36.148852
1383.573319	153566.175470	36.153869
1384.847106	153848.537929	36.158887
1386.304632	154118.873018	36.163904
1387.549977	154396.195956	36.168922
1388.695122	154682.441783	36.173940
1390.091150	154965.781670	36.178957
1391.254734	155244.481439	36.183975
1392.705686	155541.071726	36.188992
1393.836599	155843.336392	36.194010
1395.078162	156134.752380	36.199028
1396.391567	156437.651143	36.204045
1397.508310	156734.419831	36.209063
1398.957652	157034.192963	36.214080
1400.347767	157346.371517	36.219098
1401.930616	157643.425317	36.224116
1402.976196	157958.710018	36.229133
1404.359162	158258.617554	36.234151
1406.134965	158571.452483	36.239168
1407.114829	158895.051764	36.244186
1408.961928	159202.526530	36.249204
1410.347168	159510.143298	36.254221
1411.834449	159820.219325	36.259239
1413.196142	160147.203531	36.264256
1414.564282	160448.969322	36.269274
1415.932197	160762.319887	36.274292
1417.580506	161078.151156	36.279309
1419.246618	161388.602890	36.284327
1420.851573	161683.437306	36.289344
1422.377461	161998.204812	36.294362
1424.027883	162282.087479	36.299380
1425.567769	162593.736280	36.304397
1426.740045	162881.381113	36.309415
1428.154588	163180.951734	36.314432
1429.313189	163485.260940	36.319450
1431.289747	163780.949676	36.324468
1432.782107	164064.832476	36.329485
1433.890401	164343.680274	36.334503
1435.828039	164620.261562	36.339520
1437.746631	164891.823560	36.344538
1439.267235	165153.861192	36.349556
1440.725025	165434.282465	36.354573
1442.263203	165698.287111	36.359591
1444.193804	165951.139506	36.364608
1445.301329	166228.083874	36.369626
1446.983097	166475.461191	36.374644
1448.496149	166737.623908	36.379661
1449.860118	167010.077465	36.384679
1451.353803	167265.065101	36.389696
1452.270919	167530.299959	36.394714
1453.702066	167800.856812	36.399732
1455.273968	168084.220065	36.404749
1456.461187	168361.558155	36.409767
1458.023433	168636.184187	36.414784
1458.892270	168920.912301	36.419802
1460.201189	169202.752717	36.424820
1461.683154	169509.106485	36.429837
1463.080174	169804.893837	36.434855
1464.120467	170092.202331	36.439872
1465.285251	170411.189353	36.444890
1466.579923	170707.735481	36.449908
1467.861430	171030.501649	36.454925
1469.922176	171339.221336	36.459943
1471.754457	171630.291795	36.464960
1473.506201	171943.419011	36.469978
1475.405439	172243.301495	36.474996
1476.857948	172539.033995	36.480013
1479.093091	172819.335430	36.485031
1481.005837	173112.736869	36.490048
1482.495869	173400.385257	36.495066
1483.950125	173682.673468	36.500084
1485.458051	173950.716309	36.505101
1486.859841	174253.434857	36.510119
1488.492678	174533.579450	36.515136
1489.424645	174818.409847	36.520154
1490.600127	175112.859107	36.525172
1492.152458	175421.448570	36.530189
1493.487881	175710.532451	36.535207
1494.756120	176024.350391	36.540224
1495.660807	176326.440743	36.545242
1496.940705	176636.821565	36.550260
1498.373205	176962.090898	36.555277
1499.269290	177294.900478	36.560295
1500.993373	177624.390243	36.565312
1502.298028	177963.114386	36.570330
1503.798739	178289.637671	36.575348
1505.386789	178617.570112	36.580365
1507.698351	178941.501775	36.585383
1509.706222	179253.314591	36.590400
1511.077925	179571.275471	36.595418
1512.975464	179887.247851	36.600436
1514.807455	180188.421872	36.605453
1516.541053	180496.403987	36.610471
1518.191388	180792.915628	36.615488
1519.785420	181110.506782	36.620506
1521.263226	181415.465205	36.625524
1522.674515	181706.272114	36.630541
1524.225986	182024.408984	36.635559
1525.959166	182321.004588	36.640576
1527.023162	182633.793373	36.645594
1528.682861	182940.291875	36.650612
1530.274197	183241.853412	36.655629
1531.383130	183538.596984	36.660647
1533.077216	183854.766777	36.665664
1534.519424	184146.724435	36.670682
1536.314817	184427.874715	36.675700
1537.974158	184711.333613	36.680717
1539.455839	185003.251344	36.685735
1541.457282	185272.123477	36.690752
1542.978193	185548.945857	36.695770
1544.166898	185830.406636	36.700788
1545.679355	186113.021284	36.705805
1546.847186	186413.147315	36.710823
1548.378224	186697.500862	36.715840
1549.355181	187006.039127	36.720858
1550.555423	187308.538310	36.725876
1551.917345	187629.824093	36.730893
1552.752884	187947.987125	36.735911
1553.897088	188277.347516	36.740928
1555.038879	188619.365778	36.745946
1556.354520	188979.953706	36.750964
1558.034233	189326.546050	36.755981
1559.140346	189687.693457	36.760999
1560.688961	190044.885761	36.766016
1562.262174	190402.469724	36.771034
1564.001230	190777.939906	36.776052
1565.898338	191138.496131	36.781069
1567.292311	191502.374625	36.786087
1569.145197	191853.206014	36.791104
1570.471881	192226.646201	36.796122
1571.716058	192619.271033	36.801140
1573.394807	192988.316350	36.806157
1574.675898	193370.314616	36.811175
1576.331297	193738.924040	36.816192
1578.057513	194136.772864	36.821210
1579.467506	194527.935446	36.826228
1581.462502	194914.408389	36.831245
1583.416077	195307.987105	36.836263
1585.207026	195689.509357	36.841280
1586.851560	196073.812941	36.846298
1588.478106	196450.568126	36.851316
1590.158737	196834.172111	36.856333
1591.590916	197233.409390	36.861351
1593.490709	197621.133316	36.866368
1595.166304	197999.057464	36.871386
1596.343146	198383.629755	36.876404
1598.296233	198770.564578	36.881421
1599.189418	199157.409939	36.886439
1600.982901	199551.383742	36.891456
1602.907286	199942.418191	36.896474
1604.592666	200344.222498	36.901492
1606.546216	200730.394106	36.906509
1609.091258	201099.406631	36.911527
1610.936707	201463.559642	36.916544
1612.626161	201832.691873	36.921562
1614.312488	202202.499486	36.926580
1616.250708	202570.121789	36.931597
1617.599658	202928.689052	36.936615
1619.215607	203306.487480	36.941632
1620.901263	203671.655938	36.946650
1622.385058	204046.255125	36.951668
1624.199535	204410.885507	36.956685
1625.582050	204785.187800	36.961703
1627.297854	205133.535328	36.966720
1629.010063	205507.913870	36.971738
1630.246531	205883.934528	36.976756
1631.761533	206249.702658	36.981773
1632.794125	206631.131568	36.986791
1634.476346	207005.052731	36.991808
1635.618550	207391.838290	36.996826
1637.049723	207780.990610	37.001844
1639.420634	208150.537403	37.006861
1640.564991	208535.893510	37.011879
1642.152842	208904.100155	37.016896
1643.524505	209275.543974	37.021914
1644.808102	209656.641567	37.026932
1646.496579	210022.678173	37.031949
1648.039072	210405.120635	37.036967
1649.743129	210781.252811	37.041984
1651.839582	211165.524798	37.047002
1653.027391	211561.008395	37.052020
1655.120586	211937.767308	37.057037
1656.596319	212330.781713	37.062055
1658.472309	212721.573221	37.067072
1659.850675	213107.445538	37.072090
1661.050145	213514.199594	37.077108
1663.113057	213913.981409	37.082125
1664.763988	214311.394939	37.087143
1666.394232	214710.312078	37.092160
1668.505053	215096.402455	37.097178
1670.642798	215483.582119	37.102196
1673.144778	215868.189024	37.107213
1674.609835	216261.781471	37.112231
1676.698126	216651.437768	37.117248
1678.294236	217028.732146	37.122266
1679.335855	217414.653102	37.127284
1681.669926	217825.353687	37.132301
1683.272572	218256.113965	37.137319
1685.020635	218635.700829	37.142336
1686.919428	219013.486441	37.147354
1688.683110	219406.179067	37.152372
1690.723594	219771.575334	37.157389
1691.848270	220160.465034	37.162407
1693.553698	220552.612994	37.167424
1695.442913	220938.103135	37.172442
1697.312338	221319.000842	37.177460
1699.096485	221705.704902	37.182477
1700.262156	222097.566769	37.187495
1701.530786	222476.967664	37.192512
1703.742016	222877.016099	37.197530
1705.076241	223279.725203	37.202548
1706.768144	223680.090852	37.207565
1708.623762	224074.995505	37.212583
1710.337033	224481.684903	37.217600
1711.970079	224891.487720	37.222618
1713.632484	225285.514083	37.227636
1715.575190	225688.207587	37.232653
1717.081238	226090.364921	37.237671
1718.888977	226499.230170	37.242688
1720.679462	226904.873879	37.247706
1722.236299	227321.174646	37.252724
1724.217196	227716.070870	37.257741
1725.483737	228127.748642	37.262759
1726.877698	228557.085236	37.267776
1728.805501	228966.980217	37.272794
1730.314356	229392.185801	37.277812
1731.921477	229811.839261	37.282829
1733.378578	230237.995913	37.287847
1735.076296	230664.393618	37.292864
1737.027403	231092.579690	37.297882
1738.247180	231540.039872	37.302900
1740.195541	231961.370858	37.307917
1742.231698	232397.776713	37.312935
1743.939060	232829.335738	37.317952
1747.149869	233232.833879	37.322970
1749.114940	233647.994514	37.327988
1752.685869	234018.998172	37.333005
1755.309169	234396.839577	37.338023
1757.128409	234753.248875	37.343040
1758.858954	235115.007882	37.348058
1760.522315	235468.320128	37.353076
1761.895947	235807.176722	37.358093
1763.259595	236152.182813	37.363111
1764.202330	236519.180573	37.368128
1765.541224	236872.523917	37.373146
1766.629049	237254.130621	37.378164
1768.163571	237630.050683	37.383181
1769.434569	238010.358708	37.388199
1770.500391	238414.147238	37.393216
1771.943159	238811.523996	37.398234
1773.366180	239230.166248	37.403252
1774.970321	239651.624549	37.408269
1776.334035	240067.611181	37.413287
1777.772249	240520.521002	37.418304
1779.912348	240949.742853	37.423322
1781.087935	241406.127222	37.428340
1782.803182	241849.188967	37.433357
1784.758637	242293.558300	37.438375
1787.100030	242742.564274	37.443392
1789.098511	243185.277096	37.448410
1790.596030	243646.667973	37.453428
1792.599958	244092.175839	37.458445
1794.585517	244544.063564	37.463463
1796.484722	244997.490485	37.468480
1798.765219	245457.129726	37.473498
1800.473586	245900.149182	37.478516
1802.544259	246354.007322	37.483533
1804.777217	246796.255755	37.488551
1806.471263	247241.159427	37.493568
1808.871554	247684.981923	37.498586
1810.692852	248133.422256	37.503604
1812.703435	248570.095842	37.508621
1814.407538	249005.296369	37.513639
1815.823642	249455.735891	37.518656
1818.006248	249912.070013	37.523674
1819.377130	250379.004614	37.528692
1820.913838	250823.100483	37.533709
1822.800664	251283.346202	37.538727
1823.848999	251750.614953	37.543744
1825.797592	252233.002919	37.548762
1827.417221	252705.182759	37.553780
1829.114595	253181.414700	37.558797
1830.709288	253675.725633	37.563815
1832.333936	254161.496560	37.568832
1833.934273	254648.364197	37.573850
1835.632387	255145.631362	37.578868
1837.781002	255651.664858	37.583885
1839.564986	256153.668882	37.588903
1840.795689	256674.715278	37.593920
1842.994827	257169.843246	37.598938
1845.710208	257650.431780	37.603956
1848.035521	258147.317523	37.608973
1850.561696	258631.265396	37.613991
1852.137296	259121.746410	37.619008
1854.184622	259600.921425	37.624026
1856.153091	260094.386154	37.629044
1858.157048	260575.168800	37.634061
1859.757159	261036.813156	37.639079
1861.593580	261541.985168	37.644096
1863.563169	262020.614098	37.649114
1865.442661	262504.948140	37.654132
1867.408604	262981.468994	37.659149
1869.089856	263467.156447	37.664167
1870.794221	263952.230234	37.669184
1873.236577	264433.676431	37.674202
1874.731348	264927.243644	37.679220
1876.169742	265417.492066	37.684237
1878.436118	265886.188701	37.689255
1879.858009	266362.950147	37.694272
1882.041398	266817.307058	37.699290
1883.392520	267289.506940	37.704308
1885.337341	267750.227907	37.709325
1887.505672	268211.470492	37.714343
1888.949248	268683.069675	37.719360
1890.964895	269144.031768	37.724378
1893.069504	269626.850757	37.729396
1894.544345	270109.595285	37.734413
1896.339853	270591.371859	37.739431
1897.676196	271078.075562	37.744448
1899.957286	271564.063944	37.749466
1902.326764	272050.164118	37.754484
1904.434016	272533.309339	37.759501
1906.533822	273017.852252	37.764519
1908.408672	273507.207273	37.769536
1910.465846	273989.164659	37.774554
1912.547905	274484.936237	37.779572
1913.786188	274979.169578	37.784589
1916.155236	275459.726743	37.789607
1917.848080	275964.069788	37.794624
1920.049953	276448.463137	37.799642
1922.294693	276949.995159	37.804660
1923.994981	277434.774173	37.809677
1925.880232	277931.384603	37.814695
1927.737778	278426.296592	37.819712
1930.144743	278919.262512	37.824730
1931.741265	279425.443143	37.829748
1933.403643	279922.162129	37.834765
1935.377700	280427.033395	37.839783
1937.066623	280956.920615	37.844800
1939.579452	281453.546401	37.849818
1941.251859	281975.762217	37.854836
1943.175058	282486.758437	37.859853
1945.155746	283004.627634	37.864871
1947.253939	283523.263418	37.869888
1949.639669	284021.351180	37.874906
1952.317192	284521.319894	37.879924
1954.294400	285009.870398	37.884941
1956.704988	285504.444309	37.889959
1958.764473	286008.549308	37.894976
1960.609596	286497.396553	37.899994
1963.122088	286985.039948	37.905012
1965.204979	287461.449194	37.910029
1967.647210	287945.875173	37.915047
1969.817461	288420.539696	37.920064
1971.768961	288885.611856	37.925082
1973.803601	289361.972112	37.930100
1975.362076	289836.301050	37.935117
1977.186770	290305.859958	37.940135
1979.171706	290797.209807	37.945152
1980.735180	291278.264035	37.950170
1982.576856	291771.665955	37.955188
1983.723577	292263.758226	37.960205
1985.415813	292773.767276	37.965223
1986.959973	293289.031083	37.970240
1988.730130	293795.924327	37.975258
1990.757389	294323.651655	37.980276
1992.243102	294852.075587	37.985293
1994.285710	295377.128775	37.990311
1996.252222	295902.700144	37.995328
1997.973505	296441.009203	38.000346
1999.988680	296981.629356	38.005364
2002.030948	297519.067547	38.010381
2004.300358	298050.979485	38.015399
2006.472843	298582.701614	38.020416
2008.942378	299109.114585	38.025434
2010.996968	299621.268597	38.030452
2012.897589	300141.445987	38.035469
2015.108752	300641.250900	38.040487
2016.762443	301172.258043	38.045504
2018.389903	301662.985437	38.050522
2020.640968	302178.040323	38.055540
2022.294469	302695.299071	38.060557
2024.252502	303205.571271	38.065575
2026.123975	303742.293803	38.070592
2027.946542	304270.081483	38.075610
2029.738340	304810.823817	38.080628
2031.516471	305344.885806	38.085645
2033.401465	305890.660396	38.090663
2035.093205	306444.946054	38.095680
2037.221530	307005.683162	38.100698
2039.048972	307568.015490	38.105716
2040.966171	308156.436695	38.110733
2043.018655	308705.797794	38.115751
2045.309382	309271.318616	38.120768
2047.200885	309845.891543	38.125786
2049.668619	310434.053634	38.130804
2051.448301	311014.782548	38.135821
2054.121012	311593.912473	38.140839
2056.607742	312160.930063	38.145856
2058.535484	312744.821740	38.150874
2060.456879	313313.930430	38.155892
2062.490186	313889.111130	38.160909
2064.821592	314471.247144	38.165927
2066.636409	315066.491012	38.170944
2068.736943	315654.115655	38.175962
2070.898557	316248.175536	38.180980
2072.361044	316846.738959	38.185997
2074.634440	317443.690885	38.191015
2076.857355	318051.412790	38.196032
2078.327801	318660.599402	38.201050
2080.316889	319283.330982	38.206068
2081.743977	319899.420697	38.211085
2083.741350	320536.232340	38.216103
2085.418758	321172.455988	38.221120
2087.565439	321822.129941	38.226138
2089.720632	322461.487256	38.231156
2092.029638	323108.760406	38.236173
2094.143415	323763.295712	38.241191
2096.234666	324403.558576	38.246208
2098.284226	325052.200701	38.251226
2100.814352	325693.977760	38.256244
2103.273151	326353.456691	38.261261
2105.714229	326992.746839	38.266279
2107.633078	327640.672632	38.271296
2109.819240	328282.098622	38.276314
2112.521993	328913.505580	38.281332
2114.588941	329567.707986	38.286349
2116.765504	330218.559214	38.291367
2119.186104	330848.951085	38.296384
2121.501153	331486.614363	38.301402
2123.869580	332114.132211	38.306420
2126.185435	332751.273505	38.311437
2128.368130	333381.245108	38.316455
2130.635331	333999.264032	38.321472
2132.801055	334615.134977	38.326490
2135.518313	335224.180798	38.331508
2137.297276	335847.692056	38.336525
2139.532581	336463.479883	38.341543
2141.953106	337081.083205	38.346560
2144.122064	337689.607721	38.351578
2146.682754	338292.450653	38.356596
2148.724939	338903.698166	38.361613
2151.207581	339505.575355	38.366631
2153.266717	340103.047855	38.371648
2155.392443	340671.463917	38.376666
2157.440523	341240.901749	38.381684
2159.539927	341807.304148	38.386701
2161.540803	342364.553333	38.391719
2163.614560	342943.562147	38.396736
2165.256917	343510.401269	38.401754
2167.003581	344093.384696	38.406772
2168.715989	344684.082700	38.411789
2170.949475	345283.367842	38.416807
2172.837315	345889.631417	38.421824
2174.532434	346511.781746	38.426842
2177.038263	347113.004036	38.431860
2178.453379	347741.935396	38.436877
2180.546795	348358.640517	38.441895
2182.889432	348980.346746	38.446912
2185.407403	349617.750388	38.451930
2187.718253	350239.647820	38.456948
2190.004359	350882.401430	38.461965
2192.350171	351511.330659	38.466983
2194.728130	352138.850005	38.472000
2197.410289	352764.660834	38.477018
2200.308729	353387.458080	38.482036
2202.570165	354007.103385	38.487053
2204.963994	354631.234921	38.492071
2207.379434	355249.035426	38.497088
2209.463240	355877.107859	38.502106
2211.811143	356491.983453	38.507124
2213.808131	357110.409649	38.512141
2216.259421	357728.345874	38.517159
2218.758563	358352.735331	38.522176
2220.889426	358972.076154	38.527194
2223.425974	359587.002063	38.532212
2225.148666	360216.616709	38.537229
2227.376927	360838.958013	38.542247
2229.579167	361459.923999	38.547264
2231.513336	362103.631829	38.552282
2233.794445	362747.931748	38.557300
2235.847719	363384.546226	38.562317
2238.543725	364027.539180	38.567335
2240.469772	364657.405692	38.572352
2242.340660	365300.894366	38.577370
2244.992290	365937.698513	38.582388
2247.059337	366600.540288	38.587405
2249.120381	367245.893171	38.592423
2251.302226	367903.112520	38.597440
2253.231495	368562.645148	38.602458
2255.682672	369217.438095	38.607476
2257.623925	369896.173129	38.612493
2259.454460	370559.720054	38.617511
2261.984267	371233.793120	38.622528
2264.021536	371924.802534	38.627546
2266.449837	372586.311949	38.632564
2268.831318	373282.108769	38.637581
2271.452327	373950.105309	38.642599
2274.072916	374624.176537	38.647616
2276.576167	375306.902899	38.652634
2278.837451	375975.580218	38.657652
2280.804382	376651.318463	38.662669
2283.157701	377323.835220	38.667687
2285.547684	378000.923159	38.672704
2287.144058	378679.345987	38.677722
2289.932150	379358.319720	38.682740
2292.978955	380010.559838	38.687757
2295.314852	380684.890353	38.692775
2297.834556	381351.037260	38.697792
2299.549346	382025.037686	38.702810
2302.149796	382690.307900	38.707828
2304.615350	383354.724943	38.712845
2306.488054	383983.956472	38.717863
2308.847941	384634.318057	38.722880
2310.515610	385272.103458	38.727898
2312.583752	385928.116165	38.732916
2314.339680	386577.270842	38.737933
2316.492719	387243.840744	38.742951
2318.616006	387905.026915	38.747968
2320.861098	388584.027266	38.752986
2323.044870	389257.014855	38.758004
2325.423397	389938.778179	38.763021
2327.505456	390631.729837	38.768039
2329.918525	391313.051938	38.773056
2331.873447	392035.044444	38.778074
2334.006533	392743.986752	38.783092
2335.698153	393459.829526	38.788109
2337.398709	394190.558482	38.793127
2339.813497	394929.440586	38.798144
2341.824418	395678.687204	38.803162
2344.298803	396425.506919	38.808180
2346.132893	397184.351104	38.813197
2348.398402	397956.309250	38.818215
2351.035841	398711.332280	38.823232
2353.600864	399486.673058	38.828250
2356.154155	400271.397254	38.833268
2358.680735	401051.543144	38.838285
2361.003562	401839.227869	38.843303
2363.248425	402627.588049	38.848320
2365.970320	403425.780979	38.853338
2367.885030	404210.097463	38.858356
2370.431473	405004.423326	38.863373
2372.880603	405791.800290	38.868391
2375.661755	406598.001596	38.873408
2377.940767	407392.252998	38.878426
2380.461743	408193.282228	38.883444
2383.329144	408983.438445	38.888461
2385.728900	409791.990655	38.893479
2388.662951	410577.656241	38.898496
2390.898898	411356.802342	38.903514
2393.803871	412156.891515	38.908532
2396.922797	412930.273369	38.913549
2399.923515	413700.739267	38.918567
2403.203064	414462.752724	38.923584
2406.446832	415202.612727	38.928602
2409.507295	415933.617260	38.933620
2412.384119	416655.209824	38.938637
2414.697157	417399.821205	38.943655
2417.123034	418107.467384	38.948672
2419.397767	418839.203288	38.953690
2422.041593	419542.291421	38.958708
2424.345705	420263.775917	38.963725
2426.688129	420982.144175	38.968743
2429.183193	421693.022073	38.973760
2430.728395	422425.180033	38.978778
2432.830730	423148.894169	38.983796
2435.102127	423873.521584	38.988813
2437.047613	424626.235443	38.993831
2439.245951	425371.010593	38.998848
2441.415887	426112.476545	39.003866
2443.705253	426877.698374	39.008884
2445.733190	427629.774815	39.013901
2447.860978	428399.279138	39.018919
2450.124590	429161.091511	39.023936
2452.765186	429934.461942	39.028954
2455.447170	430716.710713	39.033972
2458.312073	431469.338978	39.038989
2460.413385	432244.900092	39.044007
2463.033173	433006.125699	39.049024
2465.406068	433775.567679	39.054042
2467.965283	434526.781822	39.059060
2470.390952	435267.010015	39.064077
2472.591513	435997.027521	39.069095
2475.589251	436726.688051	39.074112
2477.966381	437470.851961	39.079130
2480.179012	438216.840732	39.084148
2482.403445	438954.047934	39.089165
2484.885513	439692.453863	39.094183
2487.476999	440447.820807	39.099200
2489.658892	441209.555283	39.104218
2492.209122	441969.938095	39.109236
2494.605106	442730.320406	39.114253
2496.687759	443497.457843	39.119271
2499.482367	444279.073546	39.124288
2501.621447	445058.037477	39.129306
2503.545555	445865.037353	39.134324
2505.502444	446655.762437	39.139341
2507.463138	447483.236059	39.144359
2510.095033	448301.512365	39.149376
2512.265547	449143.659041	39.154394
2514.528373	449976.956027	39.159412
2517.400139	450831.262828	39.164429
2519.455333	451684.354840	39.169447
2522.403002	452528.464978	39.174464
2525.070218	453386.546083	39.179482
2527.521905	454237.800293	39.184500
2530.371737	455096.792549	39.189517
2532.534712	455971.336406	39.194535
2535.259119	456838.772587	39.199552
2538.367679	457714.603627	39.204570
2540.519822	458600.363881	39.209588
2543.394818	459479.242071	39.214605
2545.710183	460363.482996	39.219623
2548.417229	461239.885713	39.224640
2551.051800	462125.968377	39.229658
2553.688650	463012.314766	39.234676
2556.344838	463892.704387	39.239693
2559.202839	464775.902828	39.244711
2562.348364	465649.006678	39.249728
2564.970932	466543.132817	39.254746
2567.550958	467422.568718	39.259764
2570.886369	468278.189023	39.264781
2573.723523	469148.711045	39.269799
2576.671043	470011.949506	39.274816
2579.583680	470873.538038	39.279834
2582.521464	471725.634936	39.284852
2585.278688	472581.866697	39.289869
2587.732656	473420.527656	39.294887
2591.246706	474248.165132	39.299904
2593.981788	475087.817237	39.304922
2596.685700	475926.072995	39.309940
2598.902518	476750.934581	39.314957
2601.667068	477594.813606	39.319975
2604.018716	478421.599387	39.324992
2606.702810	479254.253340	39.330010
2609.102651	480094.441849	39.335028
2611.268851	480943.417975	39.340045
2613.353937	481770.905135	39.345063
2615.795658	482621.676777	39.350080
2618.111647	483475.105534	39.355098
2620.329396	484332.751650	39.360116
2623.113042	485198.089774	39.365133
2625.401546	486071.394496	39.370151
2627.865295	486952.251063	39.375168
2630.480449	487823.951917	39.380186
2632.550150	488713.873097	39.385204
2635.354187	489584.597785	39.390221
2637.358028	490466.162694	39.395239
2640.146680	491330.544134	39.400256
2643.078675	492195.515206	39.405274
2645.295592	493059.551680	39.410292
2648.208771	493910.056638	39.415309
2650.609174	494769.435318	39.420327
2653.703032	495623.862844	39.425344
2656.003529	496485.190391	39.430362
2658.811823	497346.844802	39.435380
2661.556259	498221.382135	39.440397
2663.817547	499108.314375	39.445415
2666.890040	499968.429462	39.450432
2669.502336	500852.386731	39.455450
2672.556826	501731.734937	39.460468
2675.326119	502622.634576	39.465485
2678.184567	503504.947711	39.470503
2680.916976	504379.820573	39.475520
2683.747513	505261.691311	39.480538
2686.048611	506159.235090	39.485556
2688.990001	507045.076307	39.490573
2691.801009	507948.236700	39.495591
2694.326220	508834.855749	39.500608
2697.154787	509730.501909	39.505626
2700.058149	510636.673208	39.510644
2702.972295	511534.120539	39.515661
2705.326872	512437.104395	39.520679
2708.142882	513333.307256	39.525696
2710.988662	514254.908715	39.530714
2713.202890	515170.613185	39.535732
2715.929759	516083.710398	39.540749
2718.436642	517015.890569	39.545767
2720.998705	517949.265859	39.550784
2723.722475	518877.015724	39.555802
2726.387403	519814.696284	39.560820
2729.446222	520753.615375	39.565837
2731.446877	521707.866404	39.570855
2734.148691	522676.098421	39.575872
2736.825137	523629.413019	39.580890
2739.734171	524592.552578	39.585908
2742.544772	525541.040649	39.590925
2745.207580	526521.676233	39.595943
2747.985442	527494.725193	39.600960
2750.722574	528463.840178	39.605978
2753.337031	529451.291821	39.610996
2756.072159	530437.449623	39.616013
2758.798728	531417.501518	39.621031
2761.026050	532417.557305	39.626048
2764.032687	533411.325437	39.631066
2766.523449	534405.966934	39.636084
2769.824198	535412.436967	39.641101
2772.698782	536414.126189	39.646119
2775.731877	537419.091929	39.651136
2778.804546	538405.210531	39.656154
2781.210165	539417.537818	39.661172
2784.304648	540419.818029	39.666189
2787.211579	541422.008442	39.671207
2789.754446	542432.640175	39.676224
2792.467082	543428.935317	39.681242
2795.616398	544451.999783	39.686260
2798.184996	545442.190319	39.691277
2800.843533	546460.310305	39.696295
2803.803548	547465.482077	39.701312
2807.095721	548460.670067	39.706330
2809.699443	549476.063899	39.711348
2812.484313	550475.364066	39.716365
2815.455640	551487.833919	39.721383
2818.018392	552487.024261	39.726400
2820.857371	553494.742267	39.731418
2823.786360	554492.217169	39.736436
2827.110190	555457.687581	39.741453
2829.653611	556433.621071	39.746471
2832.228395	557390.432131	39.751488
2835.164783	558346.512352	39.756506
2837.689235	559326.359159	39.761524
2840.472334	560295.791327	39.766541
2842.899668	561260.488792	39.771559
2845.691522	562256.152203	39.776576
2847.976156	563227.662176	39.781594
2850.565575	564230.844992	39.786612
2853.765224	565235.658516	39.791629
2856.212011	566236.501078	39.796647
2859.096147	567250.100389	39.801664
2861.859119	568264.343401	39.806682
2864.529328	569305.132966	39.811700
2867.218975	570325.301277	39.816717
2869.964106	571380.771110	39.821735
2872.580725	572420.162151	39.826752
2876.110326	573456.758080	39.831770
2879.041066	574517.458617	39.836788
2882.353035	575562.450174	39.841805
2885.576886	576604.308592	39.846823
2888.732691	577656.478255	39.851840
2891.683886	578705.081137	39.856858
2894.077983	579776.062444	39.861876
2897.331425	580821.126206	39.866893
2900.408733	581884.539196	39.871911
2903.098441	582952.087268	39.876928
2906.332399	584016.494103	39.881946
2908.579342	585074.853318	39.886964
2911.207542	586154.117499	39.891981
2914.435838	587258.506322	39.896999
2917.037111	588348.810643	39.902016
2920.291901	589437.405047	39.907034
2922.592845	590530.920189	39.912052
2925.343234	591629.674456	39.917069
2928.189463	592747.806389	39.922087
2931.131942	593875.638968	39.927104
2933.816852	594996.342073	39.932122
2936.871993	596132.759654	39.937140
2939.449608	597254.468488	39.942157
2942.707314	598398.148096	39.947175
2945.722572	599532.339820	39.952192
2948.974046	600672.592257	39.957210
2952.470438	601804.930698	39.962228
2955.533936	602936.829133	39.967245
2958.421668	604076.055189	39.972263
2961.284567	605213.820788	39.977280
2964.575437	606352.804406	39.982298
2967.357068	607484.200602	39.987316
2970.196898	608625.333685	39.992333
2973.410859	609780.952143	39.997351
2976.017875	610935.101334	40.002368
2979.172290	612076.384269	40.007386
2982.185386	613222.326747	40.012404
2984.940771	614387.301881	40.017421
2987.436947	615540.844486	40.022439
2990.184664	616705.477925	40.027456
2993.432042	617876.856985	40.032474
2995.917621	619044.787117	40.037492
2998.583432	620239.709902	40.042509
3001.554755	621413.556799	40.047527
3004.558134	622620.910436	40.052544
3008.130647	623796.900322	40.057562
3011.008625	624978.073966	40.062580
3014.033278	626168.287923	40.067597
3017.623299	627348.934282	40.072615
3020.867250	628507.477234	40.077632
3024.336424	629649.723501	40.082650
3027.595417	630783.790734	40.087668
3030.278438	631908.343119	40.092685
3033.366930	633029.762955	40.097703
3036.196327	634158.096149	40.102720
3039.345425	635280.264634	40.107738
3041.880311	636420.484339	40.112756
3044.883194	637549.721233	40.117773
3047.947022	638688.158092	40.122791
3050.368583	639838.003206	40.127808
3053.368750	640972.157269	40.132826
3056.985368	642125.691812	40.137844
3059.996651	643290.719833	40.142861
3063.640876	644446.782046	40.147879
3066.206171	645596.806391	40.152896
3069.478482	646751.072235	40.157914
3072.852996	647919.799314	40.162932
3075.444400	649095.549883	40.167949
3078.662694	650261.687935	40.172967
3081.590107	651441.794538	40.177984
3084.722988	652638.722991	40.183002
3087.492156	653821.215804	40.188020
3090.651812	655020.594074	40.193037
3093.828167	656216.835045	40.198055
3096.619799	657418.772868	40.203072
3100.062846	658635.349194	40.208090
3103.148296	659831.265092	40.213108
3106.495530	661037.349066	40.218125
3110.049612	662253.705448	40.223143
3112.928807	663480.126646	40.228160
3116.184113	664680.645255	40.233178
3119.333938	665896.510589	40.238196
3122.275274	667118.924920	40.243213
3125.697157	668344.636909	40.248231
3128.758281	669580.002343	40.253248
3132.114734	670802.821819	40.258266
3135.330540	672019.687297	40.263284
3138.285501	673254.143948	40.268301
3142.079796	674472.040092	40.273319
3145.596481	675704.739924	40.278336
3148.978281	676922.584509	40.283354
3152.089770	678144.937377	40.288372
3154.804795	679383.098944	40.293389
3157.812786	680609.915530	40.298407
3160.954769	681835.702468	40.303424
3164.564960	683071.681965	40.308442
3167.410453	684304.590937	40.313460
3170.293836	685551.383263	40.318477
3173.686784	686800.056585	40.323495
3176.222511	688039.166219	40.328512
3179.145257	689298.645905	40.333530
3182.434107	690551.188344	40.338548
3185.325127	691814.044878	40.343565
3189.311895	693063.392426	40.348583
3192.786740	694332.298708	40.353600
3196.090492	695585.673037	40.358618
3199.563063	696836.412164	40.363636
3202.418919	698089.258586	40.368653
3206.065932	699337.581742	40.373671
3209.359711	700591.190631	40.378688
3212.426594	701841.435339	40.383706
3215.814438	703087.086377	40.388724
3218.941523	704344.497311	40.393741
3222.291375	705588.607144	40.398759
3225.118109	706849.569856	40.403776
3228.547342	708100.192505	40.408794
3231.744242	709348.839033	40.413812
3234.633054	710587.300859	40.418829
3237.918253	711804.769649	40.423847
3240.890089	713017.759244	40.428864
3244.222164	714231.457095	40.433882
3247.153377	715437.276081	40.438900
3250.454259	716654.195596	40.443917
3253.351364	717880.605762	40.448935
3255.736028	719122.110621	40.453952
3258.729037	720356.900348	40.458970
3262.154432	721597.866321	40.463988
3264.410863	722876.227274	40.469005
3267.673575	724135.782095	40.474023
3270.311043	725435.095958	40.479040
3273.552663	726729.607462	40.484058
3276.813857	728026.234865	40.489076
3279.927896	729342.299309	40.494093
3283.487128	730657.732622	40.499111
3286.942798	731975.736926	40.504128
3289.736674	733315.911748	40.509146
3293.276895	734654.408409	40.514164
3296.579020	735998.548449	40.519181
3300.399096	737330.579924	40.524199
3303.678813	738700.682302	40.529216
3306.841728	740037.060564	40.534234
3310.691443	741395.255787	40.539252
3313.516730	742762.217999	40.544269
3316.806706	744129.163525	40.549287
3319.656461	745518.038148	40.554304
3323.016872	746897.017799	40.559322
3326.284499	748278.580105	40.564340
3329.684601	749683.732365	40.569357
3333.100482	751076.160471	40.574375
3336.482336	752484.899639	40.579392
3340.134563	753868.706361	40.584410
3343.698137	755281.634611	40.589428
3347.335924	756693.158235	40.594445
3350.920799	758094.583336	40.599463
3354.178731	759504.961206	40.604480
3357.457333	760911.432219	40.609498
3361.183914	762316.486089	40.614516
3364.056221	763733.227372	40.619533
3367.592354	765149.494640	40.624551
3370.962088	766580.325643	40.629568
3373.817769	768007.525945	40.634586
3377.411728	769439.395398	40.639604
3380.752758	770888.479898	40.644621
3383.701519	772319.703679	40.649639
3387.231771	773770.109451	40.654656
3390.392719	775219.160646	40.659674
3393.732879	776685.871880	40.664692
3396.973726	778140.962602	40.669709
3400.198172	779611.132110	40.674727
3403.585882	781082.548125	40.679744
3407.183439	782545.386397	40.684762
3410.845162	784009.585982	40.689780
3414.344470	785495.735867	40.694797
3418.422191	786945.043215	40.699815
3422.346380	788395.553134	40.704832
3425.841950	789859.761251	40.709850
3429.461621	791310.217468	40.714868
3432.968241	792757.504058	40.719885
3436.939923	794191.972972	40.724903
3440.869661	795617.241350	40.729920
3444.441186	797052.122897	40.734938
3447.732849	798476.473770	40.739956
3451.205761	799899.916369	40.744973
3454.641953	801340.154831	40.749991
3457.881364	802770.828973	40.755008
3460.841718	804161.898884	40.760013
3464.308963	805534.555499	40.765018
3467.130237	806845.904457	40.770023
3470.365205	808097.080205	40.775028
3473.503888	809297.168265	40.780032
3476.134517	810430.189614	40.785037
3479.265581	811479.303485	40.790042
3482.089122	812477.259214	40.795047
3484.855709	813390.386998	40.800052
3487.408669	814238.092413	40.805056
3489.564166	815022.927707	40.810061
3492.228325	815741.386858	40.815066
3494.174348	816401.086107	40.820071
3496.175230	816994.816751	40.825076
3498.398697	817542.149504	40.830080
3500.046971	818020.661801	40.835085
3501.986101	818447.895099	40.840090
3503.240086	818838.947487	40.845095
3504.432875	819165.679845	40.850100
3506.126602	819459.427353	40.855104
3507.227123	819699.527732	40.860109
3508.755996	819924.085551	40.865114
3509.993084	820092.361693	40.870119
3510.689352	820225.344578	40.875124
3511.637090	820325.988525	40.880128
3512.254586	820388.519069	40.885133
3513.195015	820450.066146	40.890138
3513.718885	820468.230972	40.895143
3514.668064	820454.129322	40.900148
3515.283894	820435.776632	40.905152
3515.796379	820375.555811	40.910157
3516.261036	820289.555221	40.915162
3516.646276	820208.851322	40.920167
3516.927622	820102.424663	40.925172
3517.524495	819968.443291	40.930176
3517.672198	819841.286282	40.935181
3518.172588	819686.321868	40.940186
3518.628276	819512.079793	40.945191
3518.815749	819325.642593	40.950196
3519.224699	819144.008802	40.955200
3519.239654	818937.083105	40.960205
3519.676080	818715.447469	40.965210
3519.587060	818501.330689	40.970215
3519.429780	818266.318026	40.975220
3519.873120	818027.037540	40.980224
3519.996461	817789.661317	40.985229
3520.290592	817544.758874	40.990234
3520.108803	817298.653062	40.995239
3519.888843	817027.283301	41.000244
3519.994210	816753.107321	41.005248
3519.753127	816486.859734	41.010253
3520.333522	816211.163524	41.015258
3520.121792	815946.064729	41.020263
3520.157722	815662.552509	41.025268
3519.908443	815395.038826	41.030272
3520.000891	815096.607204	41.035277
3520.298258	814817.962280	41.040282
3520.134785	814522.926445	41.045287
3520.193558	814245.374565	41.050292
3520.319358	813939.588734	41.055296
3520.130719	813655.637164	41.060301
3520.187793	813356.546548	41.065306
3520.032990	813053.754743	41.070311
3519.753260	812764.931226	41.075316
3519.752042	812462.430543	41.080320
3519.511893	812168.872099	41.085325
3519.911745	811875.391481	41.090330
3519.717863	811579.350198	41.095335
3519.375403	811255.881741	41.100340
3519.162171	810972.703569	41.105344
3519.030543	810677.004647	41.110349
3519.230098	810390.304056	41.115354
3518.958154	810092.299608	41.120359
3518.838606	809797.687582	41.125364
3518.759779	809499.870414	41.130368
3518.559593	809227.399683	41.135373
3518.472199	808930.833370	41.140378
3518.145016	808636.205304	41.145383
3518.514941	808352.380871	41.150388
3518.591490	808063.543827	41.155392
3518.355432	807786.609585	41.160397
3518.360968	807478.934757	41.165402
3518.260213	807204.896164	41.170407
3518.327269	806908.608825	41.175412
3518.122030	806623.434560	41.180416
3517.985579	806336.030602	41.185421
3517.953697	806045.459118	41.190426
3517.716334	805752.261159	41.195431
3517.695975	805482.357660	41.200436
3517.699866	805196.403076	41.205440
3517.684569	804915.246003	41.210445
3517.187780	804627.192308	41.215450
3517.157189	804353.567780	41.220455
3516.896482	804081.245565	41.225460
3517.219962	803797.240270	41.230464
3516.620663	803528.630833	41.235469
3517.181578	803249.665415	41.240474
3516.910427	802981.765519	41.245479
3516.540824	802702.391638	41.250484
3517.023099	802425.270132	41.255488
3516.701838	802160.143115	41.260493
3516.522191	801875.307605	41.265498
3516.690718	801625.191396	41.270503
3516.348954	801346.003485	41.275508
3516.083769	801074.446727	41.280512
3515.731346	800818.253382	41.285517
3516.035696	800553.943295	41.290522
3515.658328	800309.316790	41.295527
3515.605807	800040.089255	41.300532
3515.612556	799787.774040	41.305536
3515.355835	799540.057644	41.310541
3515.575252	799270.510121	41.315546
3514.993533	799031.173305	41.320551
3515.054420	798779.107120	41.325556
3515.011459	798520.814677	41.330560
3514.578489	798292.178372	41.335565
3515.191595	798042.301844	41.340570
3514.945646	797803.358491	41.345575
3514.858647	797556.721905	41.350580
3514.937597	797296.351172	41.355584
3514.457480	797046.128130	41.360589
3514.394620	796807.071464	41.365594
3514.484060	796575.936120	41.370599
3514.470869	796334.449127	41.375604
3514.484981	796098.841993	41.380608
3514.371939	795844.096029	41.385613
3514.168842	795612.731576	41.390618
3513.891989	795381.518977	41.395623
3513.649194	795148.721561	41.400628
3514.022618	794916.600751	41.405632
3513.420107	794690.870699	41.410637
3513.659870	794472.116627	41.415642
3513.395389	794244.646596	41.420647
3513.260121	794019.996899	41.425652
3513.401549	793779.821106	41.430656
3512.948544	793573.581043	41.435661
3513.126589	793352.542703	41.440666
3513.036650	793142.791501	41.445671
3512.852918	792921.357109	41.450676
3513.176182	792706.906881	41.455680
3512.641630	792479.719169	41.460685
3512.665985	792267.859658	41.465690
3512.418118	792073.874188	41.470695
3512.022839	791841.434846	41.475700
3512.581291	791646.322135	41.480704
3512.293976	791444.660593	41.485709
3512.596177	791234.100239	41.490714
3512.524389	791021.777018	41.495719
3512.247390	790834.789558	41.500724
3512.231978	790620.135339	41.505728
3512.306281	790407.376516	41.510733
3512.166628	790211.208980	41.515738
3511.808427	790002.588435	41.520743
3511.345240	789810.001767	41.525748
3511.775664	789616.623728	41.530752
3511.287063	789432.730695	41.535757
3511.252660	789234.798557	41.540762
3511.533690	789042.953295	41.545767
3511.405222	788853.628118	41.550772
3511.397309	788654.495747	41.555776
3510.995626	788467.614024	41.560781
3510.847372	788281.226417	41.565786
3510.877826	788099.229009	41.570791
3510.640029	787911.666628	41.575796
3510.571792	787749.685659	41.580800
3510.445658	787569.372099	41.585805
3510.459292	787390.702611	41.590810
3510.718846	787204.514721	41.595815
3510.411835	787033.362549	41.600820
3510.511080	786858.894164	41.605824
3510.444939	786679.728360	41.610829
3510.262222	786490.496973	41.615834
3510.206719	786336.103582	41.620839
3509.927446	786175.547750	41.625844
3510.132335	785998.385585	41.630848
3509.599851	785842.879920	41.635853
3510.014113	785678.215401	41.640858
3509.858096	785506.854346	41.645863
3509.990918	785339.671114	41.650868
3509.893247	785167.062834	41.655872
3509.787857	785015.600117	41.660877
3510.345203	784848.532262	41.665882
3509.762652	784681.894211	41.670887
3510.069678	784527.549756	41.675892
3509.822170	784350.962519	41.680896
3509.558287	784182.243735	41.685901
3509.385001	784026.787144	41.690906
3509.478009	783883.925194	41.695911
3509.670769	783704.937657	41.700916
3509.446270	783544.805925	41.705920
3509.184163	783389.202629	41.710925
3509.038065	783240.611678	41.715930
3509.263842	783085.069041	41.720935
3509.089664	782948.234417	41.725940
3509.512111	782779.960115	41.730944
3508.778143	782617.776224	41.735949
3508.497884	782477.949037	41.740954
3508.436830	782340.444666	41.745959
3508.208396	782190.517249	41.750964
3508.918993	782041.465304	41.755968
3508.475675	781917.694179	41.760973
3508.232751	781748.669015	41.765978
3508.202218	781624.382037	41.770983
3508.213577	781486.308242	41.775988
3508.411262	781351.498017	41.780992
3508.333466	781207.430297	41.785997
3508.243347	781063.952255	41.791002
3508.224749	780934.287659	41.796007
3508.134853	780799.268484	41.801012
3508.177435	780659.500621	41.806016
3507.803635	780535.645211	41.811021
3508.097524	780387.513738	41.816026
3507.808541	780260.096255	41.821031
3507.577496	780123.414454	41.826036
3507.597824	780005.637034	41.831040
3507.845243	779876.598758	41.836045
3507.657550	779749.007973	41.841050
3507.723151	779629.100614	41.846055
3507.779695	779496.198728	41.851060
3507.599439	779375.097181	41.856064
3507.758752	779251.181279	41.861069
3507.696869	779125.035472	41.866074
3507.529670	778995.065412	41.871079
3507.372077	778876.117654	41.876084
3507.366183	778742.030907	41.881088
3507.262419	778621.347248	41.886093
3507.222964	778499.666466	41.891098
3507.222691	778380.684708	41.896103
3507.136076	778277.025199	41.901108
3507.015033	778155.155194	41.906112
3506.960575	778026.232323	41.911117
3507.032918	777912.400099	41.916122
3506.975976	777801.738202	41.921127
3506.540781	777698.423279	41.926132
3506.746494	777580.280721	41.931136
3506.479077	777474.768751	41.936141
3506.780181	777365.222871	41.941146
3506.842377	777258.619568	41.946151
3506.677684	777142.451113	41.951156
3506.711939	777030.777804	41.956160
3506.525324	776927.460269	41.961165
3506.679645	776831.470802	41.966170
3506.485240	776707.865415	41.971175
3506.822732	776608.346902	41.976180
3506.920920	776483.212347	41.981184
3506.829572	776372.879178	41.986189
3506.817753	776262.432763	41.991194
3506.204227	776153.364099	41.996199
3506.187710	776056.063067	42.001204
3506.624436	775940.909073	42.006208
3506.607765	775857.689165	42.011213
3506.255173	775743.745468	42.016218
3506.455079	775635.864736	42.021223
3506.053327	775530.593100	42.026228
3506.253811	775430.145484	42.031232
3506.325746	775336.316894	42.036237
3505.934951	775236.111763	42.041242
3506.229203	775145.740768	42.046247
3505.889585	775036.413374	42.051252
3506.208355	774946.035886	42.056256
3505.997654	774838.654335	42.061261
3505.885121	774749.182743	42.066266
3505.770132	774656.262793	42.071271
3505.844597	774567.398468	42.076276
3505.851257	774455.345726	42.081280
3505.412476	774368.878473	42.086285
3505.490367	774274.986103	42.091290
3505.742980	774188.895401	42.096295
3505.267687	774096.175492	42.101300
3505.529905	774015.893418	42.106304
3505.625498	773919.777049	42.111309
3505.571072	773848.313120	42.116314
3505.743077	773757.945224	42.121319
3505.844563	773662.021557	42.126324
3505.788861	773559.423203	42.131328
3505.399997	773482.198151	42.136333
3505.630949	773389.993404	42.141338
3505.722150	773301.997757	42.146343
3505.303779	773209.208044	42.151348
3505.493119	773127.598229	42.156352
3505.319075	773039.938723	42.161357
3505.387226	772939.626722	42.166362
3505.335475	772867.857268	42.171367
3505.323659	772773.862031	42.176372
3505.056682	772684.637131	42.181376
3504.579856	772610.373377	42.186381
3504.962007	772530.006120	42.191386
3504.882698	772444.442407	42.196391
3504.732013	772379.384847	42.201396
3504.796272	772304.191336	42.206400
3504.745706	772222.808118	42.211405
3504.451214	772150.677531	42.216410
3504.309103	772087.291141	42.221415
3504.148161	772016.763147	42.226420
3504.429757	771948.329491	42.231424
3504.386163	771894.828599	42.236429
3504.557296	771821.090703	42.241434
3504.642547	771744.065001	42.246439
3504.606901	771686.176090	42.251444
3504.693919	771588.552628	42.256448
3504.287887	771530.181504	42.261453
3504.470687	771452.939613	42.266458
3504.269267	771396.011943	42.271463
3504.525795	771323.043411	42.276468
3504.828424	771253.368006	42.281472
3504.474772	771190.402981	42.286477
3504.520030	771112.884550	42.291482
3504.186491	771053.167268	42.296487
3504.056477	770985.137455	42.301492
3504.146830	770931.656821	42.306496
3503.974174	770869.102748	42.311501
3503.791131	770799.158131	42.316506
3504.279615	770737.676725	42.321511
3504.126487	770669.155035	42.326516
3504.228900	770614.832387	42.331520
3503.865633	770555.362389	42.336525
3503.992050	770480.632932	42.341530
3503.970056	770430.567534	42.346535
3503.988256	770374.335053	42.351540
3504.172979	770312.259510	42.356544
3504.023352	770247.232329	42.361549
3503.987263	770181.545207	42.366554
3504.014943	770128.216956	42.371559
3503.938787	770071.110634	42.376564
3504.140792	769995.230335	42.381568
3503.892599	769951.507258	42.386573
3504.105261	769877.398219	42.391578
3504.070315	769815.354711	42.396583
3503.694816	769765.786625	42.401588
3504.046713	769695.250645	42.406592
3503.781235	769643.347200	42.411597
3503.698301	769589.343302	42.416602
3503.783829	769530.629037	42.421607
3503.540602	769474.334236	42.426612
3503.695335	769417.135573	42.431616
3503.509643	769372.708772	42.436621
3503.773230	769316.082854	42.441626
3503.347298	769265.878996	42.446631
3503.393208	769210.668206	42.451636
3503.270168	769164.652603	42.456640
3503.483505	769122.425875	42.461645
3503.322684	769064.586431	42.466650
3503.576393	769011.360814	42.471655
3503.311507	768967.683990	42.476660
3503.510123	768908.502579	42.481664
3503.361292	768862.144320	42.486669
3503.262783	768813.657954	42.491674
3502.971943	768766.139496	42.496679
3503.321247	768708.163966	42.501684
3503.561882	768672.140989	42.506688
3503.342532	768621.208661	42.511693
3503.428196	768573.528372	42.516698
3503.295783	768529.334227	42.521703
3502.953769	768480.836513	42.526708
3503.271147	768427.251186	42.531712
3502.982580	768394.370259	42.536717
3503.287674	768351.088875	42.541722
3503.213238	768293.820752	42.546727
3503.149028	768251.684108	42.551732
3503.279614	768210.057389	42.556736
3502.931459	768175.262792	42.561741
3503.018895	768120.825821	42.566746
3503.099501	768081.622119	42.571751
3502.619414	768036.102025	42.576756
3503.029029	767995.069001	42.581760
3502.710578	767963.324921	42.586765
3502.814100	767923.771536	42.591770
3502.998689	767885.190539	42.596775
3502.837473	767856.131465	42.601780
3503.075276	767802.406871	42.606784
3502.826173	767765.770020	42.611789
3503.383076	767713.175382	42.616794
3503.382696	767677.926791	42.621799
3503.049944	767633.316648	42.626804
3503.279147	767588.712274	42.631808
3502.662492	767542.422871	42.636813
3502.688398	767498.788142	42.641818
3502.869806	767461.930986	42.646823
3502.621652	767428.743344	42.651828
3502.517802	767390.305905	42.656832
3502.660608	767359.321391	42.661837
3502.683369	767335.110778	42.666842
3502.949818	767294.344000	42.671847
3502.566396	767262.163926	42.676852
3502.662326	767210.331909	42.681856
3502.483374	767179.153139	42.686861
3502.546058	767142.018151	42.691866
3502.770088	767112.744820	42.696871
3502.695280	767078.195897	42.701876
3503.090263	767035.385122	42.706880
3502.945115	767008.045711	42.711885
3502.977712	766952.968327	42.716890
3502.876324	766911.126068	42.721895
3502.675808	766894.050567	42.726900
3502.606372	766836.376018	42.731904
3502.723952	766807.612074	42.736909
3502.776896	766766.828289	42.741914
3502.762141	766743.262905	42.746919
3502.763121	766709.537982	42.751924
3503.087887	766658.601252	42.756928
3502.655478	766628.645269	42.761933
3502.911780	766587.777707	42.766938
3503.069422	766555.653385	42.771943
3502.469538	766514.581309	42.776948
3502.603190	766469.936703	42.781952
3502.458109	766451.618390	42.786957
3502.390529	766415.240859	42.791962
3502.741831	766373.616874	42.796967
3502.495327	766345.749355	42.801972
3502.526727	766301.120588	42.806977
3502.303298	766276.897798	42.811981
3502.465094	766238.805153	42.816986
3502.356673	766203.222254	42.821991
3502.314567	766181.188173	42.826996
3502.276537	766149.883284	42.832001
3502.505149	766120.506708	42.837005
3502.599389	766091.595934	42.842010
3502.756802	766056.560263	42.847015
3502.736433	766027.816051	42.852020
3502.811054	765982.044141	42.857025
3502.614616	765942.825561	42.862029
3502.692689	765918.699881	42.867034
3502.900856	765868.664583	42.872039
3502.161887	765838.460067	42.877044
3502.545590	765797.912395	42.882049
3502.720713	765779.046580	42.887053
3502.419003	765743.444026	42.892058
3502.442824	765725.934414	42.897063
3502.275391	765687.893204	42.902068
3502.435159	765651.080022	42.907073
3502.180756	765635.835077	42.912077
3502.175278	765605.706050	42.917082
3502.396581	765574.208104	42.922087
3502.011357	765548.185038	42.927092
3502.318907	765523.329908	42.932097
3502.110222	765491.754504	42.937101
3502.134993	765475.575609	42.942106
3502.379490	765445.749958	42.947111
3502.214555	765425.262609	42.952116
3502.373099	765393.724931	42.957121
3502.209584	765367.664718	42.962125
3502.302361	765331.847289	42.967130
3502.579957	765303.347108	42.972135
3502.280859	765275.188384	42.977140
3502.404040	765250.806555	42.982145
3502.367485	765217.919461	42.987149
3502.252115	765188.793163	42.992154
3502.353241	765154.009131	42.997159
3502.254704	765134.890885	43.002164
3502.370872	765092.953329	43.007169
3502.243728	765058.699615	43.012173
3502.146884	765038.643839	43.017178
3502.271741	764994.780971	43.022183
3502.116096	764979.765006	43.027188
3501.984598	764949.012987	43.032193
3501.947582	764933.928074	43.037197
3502.507618	764913.714447	43.042202
3502.479363	764882.747884	43.047207
3502.133582	764856.420016	43.052212
3502.337859	764818.954303	43.057217
3502.616203	764798.441544	43.062221
3502.438809	764765.230444	43.067226
3502.193916	764729.712357	43.072231
3502.063872	764698.712484	43.077236
3502.360800	764688.158685	43.082241
3502.207584	764653.660827	43.087245
3502.209062	764622.441700	43.092250
3502.516777	764600.591953	43.097255
3502.139466	764578.707023	43.102260
3502.361419	764545.083935	43.107265
3502.125688	764518.490158	43.112269
3502.027667	764488.815774	43.117274
3502.476226	764466.794481	43.122279
3502.362751	764442.942217	43.127284
3502.562144	764402.614670	43.132289
3502.292383	764390.279624	43.137293
3502.430387	764348.975492	43.142298
3502.255760	764320.694044	43.147303
3502.038174	764291.531787	43.152308
3502.276800	764258.545849	43.157313
3501.908907	764238.680550	43.162317
3502.299082	764216.668145	43.167322
3502.291252	764186.681785	43.172327
3502.171281	764173.976458	43.177332
3502.368061	764139.073336	43.182337
3502.237555	764118.872686	43.187341
3502.347875	764095.081100	43.192346
3502.228747	764056.826387	43.197351
3501.920926	764040.748513	43.202356
3502.215188	764017.616903	43.207361
3501.730167	763995.550723	43.212365
3502.001750	763969.315348	43.217370
3502.251567	763945.598959	43.222375
3501.884118	763930.763756	43.227380
3502.157968	763889.040139	43.232385
3501.960752	763871.365324	43.237389
3502.226895	763838.225044	43.242394
3502.293858	763822.134293	43.247399
3501.999234	763801.861177	43.252404
3502.530012	763767.986458	43.257409
3502.271246	763758.213439	43.262413
3501.725610	763717.709000	43.267418
3501.985625	763687.824510	43.272423
3501.968626	763671.895244	43.277428
3502.056204	763641.348421	43.282433
3502.179104	763622.929739	43.287437
3501.820631	763605.083558	43.292442
3502.003403	763587.493462	43.297447
3501.847478	763559.058096	43.302452
3502.144735	763529.758757	43.307457
3501.970067	763519.133031	43.312461
3501.794346	763491.045952	43.317466
3502.329322	763463.186989	43.322471
3501.962791	763451.359607	43.327476
3502.006727	763415.590436	43.332481
3502.236255	763397.202966	43.337485
3502.105859	763369.995856	43.342490
3502.146885	763347.594488	43.347495
3501.957227	763323.356608	43.352500
3502.181890	763304.032491	43.357505
3502.000086	763277.178807	43.362509
3502.224261	763260.222391	43.367514
3502.136617	763236.164739	43.372519
3502.215070	763196.639914	43.377524
3502.125690	763182.053400	43.382529
3502.292268	763159.680122	43.387533
3501.920199	763139.467307	43.392538
3502.347584	763104.077457	43.397543
3501.585574	763092.018678	43.402548
3501.629424	763049.539045	43.407553
3501.837308	763048.468836	43.412557
3501.412850	763024.071353	43.417562
3502.009492	762992.204817	43.422567
3502.099913	762992.535179	43.427572
3501.991831	762952.694496	43.432577
3502.072765	762948.340083	43.437581
3501.992713	762920.925741	43.442586
3502.062523	762884.557832	43.447591
3501.897584	762877.925353	43.452596
3501.942897	762842.350562	43.457601
3501.887331	762842.014349	43.462605
3501.738986	762812.193662	43.467610
3502.285730	762788.819381	43.472615
3501.805945	762775.924310	43.477620
3501.983358	762748.861582	43.482625
3501.848805	762735.120275	43.487629
3501.878856	762695.304813	43.492634
3502.082476	762679.682434	43.497639
3501.738974	762670.267279	43.502644
3501.848114	762648.099276	43.507649
3502.094738	762638.340217	43.512653
3501.965165	762601.905127	43.517658
3502.260357	762593.815305	43.522663
3501.914448	762571.919362	43.527668
3502.144149	762553.431149	43.532673
3502.284074	762524.203164	43.537677
3501.989100	762500.226651	43.542682
3501.980683	762463.474939	43.547687
3501.960596	762456.620897	43.552692
3502.211144	762421.207651	43.557697
3502.088845	762407.957063	43.562701
3502.047434	762384.382416	43.567706
3502.209234	762362.895574	43.572711
3501.755085	762337.711420	43.577716
3502.025035	762310.039875	43.582721
3501.710473	762284.141873	43.587725
3501.497015	762270.067377	43.592730
3501.692745	762257.602823	43.597735
3501.612321	762243.457030	43.602740
3501.893184	762222.542191	43.607745
3501.665489	762212.120695	43.612749
3501.533275	762195.812615	43.617754
3502.103305	762171.199227	43.622759
3501.824527	762169.271696	43.627764
3501.913566	762132.600994	43.632769
3501.720971	762112.651874	43.637773
3501.620026	762096.042416	43.642778
3501.867052	762080.460988	43.647783
3501.273642	762067.879431	43.652788
3502.063291	762051.764542	43.657793
3502.105518	762015.002311	43.662797
3502.044523	762012.792186	43.667802
3502.236079	761976.843884	43.672807
3501.959878	761965.147293	43.677812
3501.953445	761932.882282	43.682817
3502.118136	761913.367149	43.687821
3502.054428	761894.580303	43.692826
3501.865986	761858.891381	43.697831
3501.615845	761847.782360	43.702836
3501.933314	761825.972330	43.707841
3501.927388	761808.902556	43.712845
3501.787958	761791.312023	43.717850
3501.924716	761778.609709	43.722855
3501.902125	761754.536625	43.727860
3502.207245	761718.371040	43.732865
3502.084491	761702.553718	43.737869
3501.954531	761678.596754	43.742874
3502.066792	761659.681663	43.747879
3501.687264	761644.745267	43.752884
3501.655540	761628.320734	43.757889
3501.691488	761610.355522	43.762893
3501.801058	761591.934092	43.767898
3502.119333	761570.369890	43.772903
3501.782325	761544.275694	43.777908
3502.137421	761526.701765	43.782913
3501.791705	761514.127821	43.787917
3501.658105	761477.441282	43.792922
3501.643202	761465.503518	43.797927
3501.758875	761461.290548	43.802932
3501.700594	761434.607327	43.807937
3501.758891	761429.367655	43.812941
3502.023185	761410.426900	43.817946
3501.823208	761378.043386	43.822951
3501.753084	761374.354373	43.827956
3501.870527	761350.355619	43.832961
3502.034928	761337.796036	43.837965
3501.461782	761312.430702	43.842970
3501.853372	761279.307896	43.847975
3501.259398	761281.428655	43.852980
3501.520969	761266.287227	43.857985
3501.647781	761234.934772	43.862989
3501.857964	761220.443151	43.867994
3501.904255	761206.027840	43.872999
3501.684087	761193.975436	43.878004
3501.772134	761176.888760	43.883009
3501.593627	761170.454379	43.888013
3501.887747	761142.971962	43.893018
3501.906450	761123.281478	43.898023
3501.665635	761098.206077	43.903028
3501.974892	761069.289982	43.908033
3501.796631	761068.184424	43.913037
3501.694500	761045.553112	43.918042
3502.031126	761027.783704	43.923047
3501.709197	761021.520848	43.928052
3501.983583	760991.524668	43.933057
3501.694311	760988.068936	43.938061
3501.487554	760958.793335	43.943066
3501.936109	760937.255220	43.948071
3501.742046	760923.767138	43.953076
3501.587633	760903.956571	43.958081
3501.196544	760884.875744	43.963085
3501.523243	760887.683793	43.968090
3501.861871	760874.699999	43.973095
3501.670401	760848.974180	43.978100
3501.652124	760828.302151	43.983105
3501.715309	760825.429755	43.988109
3501.505833	760805.973408	43.993114
3501.560847	760794.467167	43.998119
3501.476187	760782.342442	44.003124
3501.719528	760763.058118	44.008129
3501.692624	760758.226770	44.013133
3501.675066	760732.718632	44.018138
3501.746566	760717.410043	44.023143
3501.488695	760703.191912	44.028148
3501.603163	760687.284050	44.033153
3501.519564	760668.990889	44.038157
3501.456337	760644.427526	44.043162
3501.576647	760629.604169	44.048167
3501.859247	760633.258443	44.053172
3501.566216	760609.275614	44.058177
3501.627933	760600.481957	44.063181
3501.402405	760584.333812	44.068186
3501.694620	760572.442746	44.073191
3501.262801	760563.927722	44.078196
3501.464475	760535.126009	44.083201
3501.770512	760529.006033	44.088205
3501.590547	760515.169482	44.093210
3501.705078	760486.135208	44.098215
3501.532929	760485.867437	44.103220
3501.742129	760472.213435	44.108225
3501.669232	760443.407255	44.113229
3501.892672	760439.126623	44.118234
3501.623187	760415.139301	44.123239
3501.619445	760393.131340	44.128244
3502.065198	760376.329368	44.133249
3501.844303	760360.328023	44.138253
3501.641649	760346.988370	44.143258
3501.650895	760328.432360	44.148263
3501.551613	760316.309299	44.153268
3501.591896	760298.290921	44.158273
3501.879094	760285.857415	44.163277
3501.615112	760254.022463	44.168282
3501.715198	760234.168226	44.173287
3501.441384	760229.771994	44.178292
3501.288666	760222.542997	44.183297
3501.654720	760208.073121	44.188301
3501.355459	760191.738895	44.193306
3501.805692	760183.620978	44.198311
3501.731381	760177.316632	44.203316
3501.746662	760143.263906	44.208321
3501.895975	760136.133121	44.213325
3501.419327	760123.381036	44.218330
3501.500147	760098.348046	44.223335
3501.648544	760088.207110	44.228340
3501.740729	760080.000015	44.233345
3501.824277	760057.187125	44.238349
3501.415256	760048.174277	44.243354
3501.479664	760038.886039	44.248359
3501.367805	760023.014069	44.253364
3501.747267	759988.555220	44.258369
3501.781846	759989.931249	44.263373
3501.537070	759969.392889	44.268378
3501.823300	759938.551669	44.273383
3501.457771	759946.063596	44.278388
3501.442445	759929.879434	44.283393
3501.742504	759903.822700	44.288397
3501.624212	759898.512362	44.293402
3501.695740	759893.911000	44.298407
3501.332292	759865.693337	44.303412
3501.611411	759843.834592	44.308417
3501.666624	759849.944857	44.313421
3501.357338	759837.559523	44.318426
3501.535808	759804.169301	44.323431
3501.339406	759800.253570	44.328436
3501.349430	759792.898656	44.333441
3501.675856	759786.182523	44.338445
3501.588163	759767.739814	44.343450
3501.738625	759750.886405	44.348455
3501.518480	759745.642087	44.353460
3502.062816	759718.902924	44.358465
3501.609194	759708.564542	44.363469
3501.786112	759692.348209	44.368474
3501.735810	759648.039035	44.373479
3501.603636	759647.962052	44.378484
3501.839336	759639.928249	44.383489
3501.709735	759609.400949	44.388493
3501.251319	759605.676331	44.393498
3502.031039	759594.986583	44.398503
3501.554502	759576.854220	44.403508
3501.560449	759561.504751	44.408513
3501.876037	759544.821095	44.413517
3501.547958	759522.469222	44.418522
3501.949327	759503.846611	44.423527
3501.741514	759492.134931	44.428532
3501.673444	759462.041075	44.433537
3501.703451	759462.036081	44.438541
3501.805693	759448.200452	44.443546
3502.028655	759424.770472	44.448551
3501.480251	759416.816238	44.453556
3501.505800	759409.557102	44.458561
3501.655701	759376.613888	44.463565
3501.315529	759362.160033	44.468570
3501.726731	759350.790351	44.473575
3501.301323	759340.545524	44.478580
3501.193916	759319.884074	44.483585
3501.480974	759318.899022	44.488589
3501.602280	759308.267977	44.493594
3501.898812	759297.163871	44.498599
3501.851433	759278.071737	44.503604
3501.679613	759267.044734	44.508609
3501.619126	759241.588018	44.513613
3501.353149	759226.134603	44.518618
3501.582201	759213.511513	44.523623
3501.456156	759211.804826	44.528628
3501.326218	759185.372278	44.533633
3501.315351	759171.554779	44.538637
3501.056409	759163.848725	44.543642
3501.361937	759164.686728	44.548647
3500.863051	759171.135582	44.553652
3501.411186	759155.251796	44.558657
3501.412431	759133.831625	44.563661
3500.891532	759127.698680	44.568666
3501.277685	759114.210518	44.573671
3501.499714	759118.418408	44.578676
3501.420967	759113.298426	44.583681
3501.527343	759083.914665	44.588685
3501.114577	759072.433517	44.593690
3501.689400	759064.491315	44.598695
3501.072207	759063.359048	44.603700
3501.030342	759059.368123	44.608705
3501.658543	759050.528720	44.613709
3501.541870	759029.571877	44.618714
3501.475367	759021.537848	44.623719
3501.200330	759017.042399	44.628724
3501.007301	759016.975432	44.633729
3501.547678	758995.416712	44.638733
3501.318211	758965.692969	44.643738
3501.580853	758964.563828	44.648743
3500.890772	758965.220360	44.653748
3501.213098	758949.077207	44.658753
3501.577358	758954.100811	44.663757
3501.116191	758919.035260	44.668762
3501.329709	758911.053701	44.673767
3501.466871	758925.591108	44.678772
3501.569309	758914.715842	44.683777
3501.395899	758892.089858	44.688781
3501.283941	758871.970861	44.693786
3501.367814	758865.441946	44.698791
3501.107420	758859.611367	44.703796
3501.250954	758864.819458	44.708801
3501.303891	758850.596016	44.713805
3501.281779	758831.498600	44.718810
3501.402215	758819.090177	44.723815
3501.231101	758821.981002	44.728820
3501.360109	758805.869390	44.733825
3501.413906	758801.418360	44.738829
3501.184545	758783.588884	44.743834
3501.358648	758758.930983	44.748839
3501.483500	758758.564866	44.753844
3501.573459	758750.307350	44.758849
3501.433430	758738.188485	44.763853
3501.289100	758729.327893	44.768858
3501.353170	758714.362003	44.773863
3501.235606	758706.484125	44.778868
3501.416908	758712.130317	44.783873
3501.606524	758687.913848	44.788877
3501.257432	758672.966575	44.793882
3501.726848	758656.304999	44.798887
3501.458966	758660.840631	44.803892
3501.129835	758653.441766	44.808897
3501.195166	758629.887237	44.813901
3501.147596	758620.368927	44.818906
3501.360687	758623.295257	44.823911
3500.928075	758616.801846	44.828916
3501.113661	758621.657671	44.833921
3501.155798	758618.096900	44.838925
3501.166910	758603.879887	44.843930
3501.529820	758575.439074	44.848935
3501.311054	758563.382258	44.853940
3501.228607	758579.832117	44.858945
3501.393302	758571.710173	44.863949
3501.401056	758567.957608	44.868954
3501.281321	758540.237824	44.873959
3501.269852	758524.889137	44.878964
3501.477225	758519.376115	44.883969
3501.421145	758520.471191	44.888973
3501.052245	758507.846714	44.893978
3501.640706	758482.823516	44.898983
3501.355491	758481.044165	44.903988
3501.191049	758474.802613	44.908993
3501.588681	758466.888983	44.913997
3501.267871	758454.700726	44.919002
3501.534428	758432.000905	44.924007
3501.299920	758435.001036	44.929012
3501.227908	758435.802594	44.934017
3501.541161	758432.591952	44.939021
3501.234322	758421.388526	44.944026
3501.805844	758387.335047	44.949031
3501.586232	758376.561423	44.954036
3501.127558	758369.973373	44.959041
3501.266585	758355.784188	44.964045
3501.474082	758324.998775	44.969050
3501.487273	758329.784464	44.974055
3501.066048	758329.656356	44.979060
3501.104464	758321.308147	44.984065
3501.106946	758316.421048	44.989069
3500.906287	758312.603968	44.994074
3501.005647	758292.547354	44.999079
3501.146554	758286.748952	45.004084
3501.179301	758280.474760	45.009089
3501.409487	758285.027292	45.014093
3501.276405	758282.581151	45.019098
3501.114146	758274.660828	45.024103
3501.043770	758278.522468	45.029108
3501.294854	758264.117214	45.034113
3501.017505	758246.837349	45.039117
3501.412289	758237.048255	45.044122
3501.505810	758231.701861	45.049127
3501.866837	758224.682502	45.054132
3501.691976	758212.074931	45.059137
3501.521825	758187.768056	45.064141
3501.130501	758179.638561	45.069146
3501.472082	758176.669952	45.074151
3501.291950	758162.927868	45.079156
3501.376915	758132.754196	45.084161
3501.497166	758132.191364	45.089165
3501.174766	758127.949993	45.094170
3501.452763	758115.119584	45.099175
3501.359117	758101.461866	45.104180
3501.687237	758087.290397	45.109185
3501.512070	758080.359227	45.114189
3501.081888	758078.653019	45.119194
3501.386113	758047.258217	45.124199
3501.353942	758039.168135	45.129204
3501.081044	758033.388341	45.134209
3500.958932	758036.962455	45.139213
3501.400717	758029.584082	45.144218
3501.625541	758020.760583	45.149223
3501.253342	757999.941724	45.154228
3501.345019	757979.145123	45.159233
3501.405825	757971.730725	45.164237
3501.529376	757990.764117	45.169242
3501.684668	757954.210443	45.174247
3501.550100	757953.689571	45.179252
3501.583887	757936.555203	45.184257
3501.368563	757929.383697	45.189261
3501.056207	757910.578599	45.194266
3501.561579	757886.998659	45.199271
3501.241623	757898.602191	45.204276
3501.631031	757893.700450	45.209281
3501.471813	757871.562727	45.214285
3501.420292	757864.610994	45.219290
3501.574828	757861.130082	45.224295
3501.507690	757859.758927	45.229300
3501.547798	757833.046867	45.234305
3501.603359	757804.258909	45.239309
3501.187888	757818.543913	45.244314
3501.460516	757799.839636	45.249319
3501.418193	757779.113927	45.254324
3501.675152	757762.485406	45.259329
3501.217968	757756.735757	45.264333
3501.318539	757759.927773	45.269338
3501.684489	757744.959623	45.274343
3501.514187	757725.933215	45.279348
3501.454194	757718.785289	45.284353
3501.752792	757707.481085	45.289357
3501.384439	757682.464790	45.294362
3501.193838	757668.131169	45.299367
3501.281260	757659.971622	45.304372
3501.446017	757663.646749	45.309377
3501.527697	757661.905495	45.314381
3501.063725	757637.447809	45.319386
3501.357393	757617.159960	45.324391
3501.442974	757609.346214	45.329396
3501.486333	757608.006177	45.334401
3501.299382	757593.030075	45.339405
3500.944042	757578.920881	45.344410
3501.332974	757563.010660	45.349415
3501.118976	757566.698857	45.354420
3501.326244	757568.836717	45.359425
3501.596396	757557.142058	45.364429
3501.283260	757543.914415	45.369434
3501.484711	757518.704996	45.374439
3500.981888	757514.344904	45.379444
3501.246311	757507.093977	45.384449
3501.503797	757508.236278	45.389453
3501.553685	757506.450861	45.394458
3501.678760	757470.887159	45.399463
3501.383107	757472.219309	45.404468
3501.288308	757468.779290	45.409473
3501.544805	757445.683278	45.414477
3501.392430	757427.837950	45.419482
3501.689020	757420.877838	45.424487
3501.289333	757415.809579	45.429492
3501.272596	757405.346725	45.434497
3501.396621	757382.124244	45.439501
3501.304697	757370.094013	45.444506
3501.317930	757378.237185	45.449511
3501.314287	757371.227750	45.454516
3501.183608	757351.947054	45.459521
3501.449408	757322.085961	45.464525
3501.149419	757315.816419	45.469530
3501.523243	757311.558641	45.474535
3501.589932	757319.989269	45.479540
3501.438518	757312.905389	45.484545
3501.703806	757279.094894	45.489549
3501.672909	757275.101228	45.494554
3501.580921	757255.024046	45.499559
3501.606853	757238.876746	45.504564
3501.709093	757228.788988	45.509569
3501.506620	757221.367863	45.514573
3501.328454	757204.809806	45.519578
3501.498576	757172.989205	45.524583
3501.451814	757184.400713	45.529588
3501.297295	757175.342523	45.534593
3501.556603	757159.551553	45.539597
3501.343735	757143.937062	45.544602
3501.463820	757132.710784	45.549607
3501.250198	757130.129434	45.554612
3501.345051	757129.768185	45.559617
3501.776920	757110.048643	45.564621
3501.377702	757099.055958	45.569626
3501.414751	757084.634375	45.574631
3501.440962	757092.825082	45.579636
3501.237428	757076.912709	45.584641
3501.235410	757047.242764	45.589645
3501.193459	757037.030400	45.594650
3501.195590	757034.956530	45.599655
3501.363204	757027.622362	45.604660
3501.212082	757029.868777	45.609665
3501.484304	756996.302733	45.614669
3501.519573	756998.913404	45.619674
3501.543433	756987.209078	45.624679
3501.269874	756980.638694	45.629684
3501.272723	756964.445248	45.634689
3501.253866	756951.168104	45.639693
3500.969642	756938.280230	45.644698
3501.295432	756930.080643	45.649703
3501.336929	756935.306863	45.654708
3501.133367	756942.893782	45.659713
3501.204613	756932.366419	45.664717
3501.169254	756915.586736	45.669722
3501.292738	756901.002464	45.674727
3501.419753	756892.144410	45.679732
3500.892090	756899.686019	45.684737
3501.522922	756900.371964	45.689741
3501.094087	756884.249455	45.694746
3501.455442	756852.297285	45.699751
3501.238241	756855.788871	45.704756
3501.121092	756829.691645	45.709761
3501.442403	756833.489495	45.714765
3501.389516	756837.892045	45.719770
3501.242466	756819.797572	45.724775
3501.408046	756800.071728	45.729780
3501.069736	756792.573822	45.734785
3501.436236	756783.774935	45.739789
3501.435004	756786.144841	45.744794
3501.533729	756769.490862	45.749799
3501.338195	756755.304451	45.754804
3501.168501	756738.941469	45.759809
3501.769049	756742.347778	45.764813
3501.276829	756715.571392	45.769818
3501.246969	756634.262896	45.774823
3500.964304	756511.671226	45.779828
3501.055090	756336.829241	45.784833
3501.089693	756106.051702	45.789837
3500.695051	755824.579503	45.794842
3500.724763	755467.972349	45.799847
3500.589230	755061.698779	45.804852
3500.428158	754610.073707	45.809857
3500.152131	754077.545149	45.814861
3499.758062	753504.301218	45.819866
3499.505057	752874.187471	45.824871
3499.241150	752178.175021	45.829876
3498.847024	751419.180699	45.834881
3498.512626	750600.317053	45.839885
3498.021091	749748.186290	45.844890
3497.569838	748818.414846	45.849895
3497.159391	747844.091227	45.854900
3496.414371	746799.950975	45.859905
3496.246486	745698.374211	45.864909
3495.372499	744540.685899	45.869914
3495.178153	743314.714720	45.874919
3494.208189	742019.729402	45.879924
3493.573014	740687.076860	45.884929
3493.065506	739275.506352	45.889933
3492.187991	737823.413295	45.894938
3491.736232	736280.503077	45.899943
3491.131798	734706.230470	45.904948
3489.946675	733061.974710	45.909953
3489.262372	731338.898185	45.914957
3488.487943	729581.883493	45.919962
3487.495122	727751.736711	45.924967
3486.553603	725877.608079	45.929972
3485.679449	723923.922409	45.934977
3484.761494	721919.056729	45.939981
3483.640282	719860.820387	45.944986
3482.690937	717718.107984	45.949991
3481.586411	715557.655738	45.954996
3480.361478	713309.360495	45.960001
3479.482453	711022.133456	45.965005
3478.236978	708677.887441	45.970010
3477.315681	706261.512848	45.975015
3476.005780	703814.215543	45.980020
3474.481647	701273.415041	45.985025
3473.419730	698696.400456	45.990029
3472.000990	696063.634615	45.995034
3470.932069	693388.588392	46.000039
3469.538545	690648.398709	46.005044
3467.952003	687839.107383	46.010049
3466.960975	684991.052013	46.015053
3465.051114	682090.056883	46.020058
3463.844006	679121.311702	46.025063
3462.604985	676110.799201	46.030068
3460.817098	673050.694111	46.035073
3459.403388	669921.950697	46.040077
3457.642474	666741.742382	46.045082
3456.323255	663519.030770	46.050087
3454.786981	660223.336047	46.055092
3453.068103	656902.435421	46.060097
3451.479939	653503.253324	46.065101
3449.619272	650060.122315	46.070106
3447.845747	646563.550215	46.075111
3446.561601	643033.882981	46.080116
3444.314273	639437.317345	46.085121
3442.811790	635798.388983	46.090125
3440.503268	632112.866937	46.095130
3439.028517	628359.911943	46.100135
3437.067397	624571.850161	46.105140
3435.173273	620740.048389	46.110145
3432.926047	616840.229199	46.115149
3431.145014	612901.843111	46.120154
3429.241461	608923.508354	46.125159
3427.208167	604884.774078	46.130164
3424.991887	600798.305713	46.135169
3422.892703	596663.168213	46.140173
3420.529078	592492.103902	46.145178
3418.607830	588270.804857	46.150183
3416.425596	584018.611358	46.155188
3414.172109	579718.682036	46.160193
3412.168805	575353.929895	46.165197
3409.820228	570948.868768	46.170202
3407.660080	566508.930304	46.175207
3405.091492	562013.147879	46.180212
3402.554738	557495.726492	46.185217
3400.413817	552909.989483	46.190221
3398.128615	548292.685591	46.195226
3395.648015	543629.696482	46.200231
3393.508693	538930.904202	46.205236
3391.084087	534185.654851	46.210241
3388.564066	529398.140394	46.215245
3385.671044	524564.405035	46.220250
3383.117900	519686.892781	46.225255
3380.799695	514790.369950	46.230260
3378.042473	509835.786908	46.235265
3375.576970	504846.916873	46.240269
3372.698204	499821.044603	46.245274
3370.424551	494763.212809	46.250279
3367.912833	489657.472407	46.255284
3364.783046	484533.036562	46.260289
3362.276322	479355.084015	46.265293
3359.299336	474142.373903	46.270298
3356.732387	468885.496807	46.275303
3353.697857	463593.112180	46.280308
3351.018338	458288.361109	46.285313
3348.198260	452926.480053	46.290317
3345.064324	447540.002425	46.295322
3342.339281	442130.047726	46.300327
3339.668545	436671.935039	46.305332
3336.416712	431187.904213	46.310337
3333.638630	425661.255152	46.315341
3330.493877	420119.406965	46.320346
3327.347242	414543.870781	46.325351
3324.300264	408944.328753	46.330356
3321.177336	403308.238204	46.335361
3318.118706	397639.943659	46.340365
3314.717111	391961.954161	46.345370
3311.688933	386243.384280	46.350375
3308.616667	380503.725265	46.355380
3305.264068	374747.298440	46.360385
3302.301236	368949.999658	46.365389
3298.797469	363149.248385	46.370394
3295.672233	357297.979598	46.375399
3292.125515	351442.556274	46.380404
3288.896293	345567.967932	46.385409
3285.650369	339651.001397	46.390413
3282.277591	333733.781924	46.395418
3278.556511	327779.641220	46.400423
3275.380056	321816.652945	46.405428
3271.823544	315841.327550	46.410433
3268.526288	309834.106019	46.415437
3264.929126	303827.183369	46.420442
3261.251107	297791.827940	46.425447
3257.748443	291743.172556	46.430452
3253.907376	285687.771500	46.435457
3250.530480	279615.613809	46.440461
3246.677486	273523.673106	46.445466
3243.041293	267431.142936	46.450471
3239.234060	261331.240560	46.455476
3235.368934	255220.640867	46.460481
3231.723518	249108.089460	46.465485
3227.735881	242979.320303	46.470490
3224.127423	236832.667436	46.475495
3220.037001	230701.181762	46.480500
3215.827501	224556.134307	46.485505
3212.366585	218412.565787	46.490509
3207.919859	212278.125844	46.495514
3204.317509	206045.091726	46.500519
3199.984511	199897.693436	46.505524
3196.090823	193752.867617	46.510529
3191.685465	187609.058275	46.515533
3187.578065	181465.259783	46.520538
3183.374469	175340.653046	46.525543
3179.255014	169210.171538	46.530548
3174.605722	163108.394390	46.535553
3170.500130	157007.489830	46.540557
3165.918078	150916.468090	46.545562
3161.365589	144838.844063	46.550567
3157.172590	138770.913318	46.555572
3151.915488	132730.740391	46.560577
3147.905931	126708.542986	46.565581
3142.928846	120697.196656	46.570586
3138.187905	114707.499123	46.575591
3133.287304	108744.876285	46.580596
3127.977701	102825.572387	46.585601
3123.121457	96912.336048	46.590605
3118.051223	91048.196398	46.595610
3112.481126	85227.113873	46.600615
3106.799566	79432.408474	46.605620
3100.902393	73698.977064	46.610625
3094.812887	68016.966256	46.615629
3088.039626	62410.275413	46.620634
3078.990582	56925.236621	46.625639
3063.671467	51696.095766	46.630644
3047.655357	46655.173065	46.635649
3031.979141	41822.934273	46.640653
3016.649500	37218.707972	46.645658
3001.648710	32859.406769	46.650663
2987.769197	28755.773805	46.655668
2974.113090	24920.095563	46.660673
2961.360779	21343.149668	46.665677
2948.805471	18009.134341	46.670682
2936.980187	14930.049083	46.675687
2925.326082	12073.445902	46.680692
2913.318214	9464.132892	46.685697
2902.385706	7086.800473	46.690701
2889.504950	4993.233395	46.695706
2874.855122	3172.559663	46.700711
2859.847134	1598.299755	46.705716
2840.680952	446.998977	46.710721
2797.280910	264.073141	46.715725
2765.923452	258.996145	46.720730
2756.430088	233.658974	46.725735
2761.246481	245.746077	46.730740
2771.895937	250.425042	46.735745
2783.577896	243.801405	46.740749
2791.366999	246.138699	46.745754
2794.597445	263.584627	46.750759
2794.355766	245.006057	46.755764
2791.488362	246.334501	46.760769
2787.699022	241.379012	46.765773
2784.049581	240.579166	46.770778
2780.367593	245.175319	46.775783
2777.594370	237.417528	46.780788
2774.863100	246.843765	46.785793
2772.631944	233.473479	46.790797
2769.802762	229.508789	46.795802
2766.876771	236.578690	46.800807
2763.830170	224.234831	46.805812
2760.416995	237.427124	46.810817
2757.688192	228.926520	46.815821
2754.530401	229.106709	46.820826
2751.346704	233.581552	46.825831
2748.316581	230.800758	46.830836
2744.536060	237.192385	46.835841
2742.083964	229.892131	46.840845
2738.850595	219.488032	46.845850
2735.459288	233.003976	46.850855
2732.178799	225.636573	46.855860
2728.693709	231.670991	46.860865
2725.662836	219.740706	46.865869
2722.373408	214.851717	46.870874
2718.920369	214.952638	46.875879
2715.761432	216.808160	46.880884
2712.118030	221.603580	46.885889
2708.629897	211.172051	46.890893
2705.439894	216.878320	46.895898
2702.309170	217.427195	46.900903
2698.897040	210.387068	46.905908
2695.362838	211.363955	46.910913
2691.790311	214.938139	46.915917
2688.301661	216.746809	46.920922
2685.447899	224.414630	46.925927
2682.294114	212.809297	46.930932
2678.354809	217.608725	46.935937
2675.167741	215.322371	46.940941
2671.437741	219.512903	46.945946
2668.400520	218.208165	46.950951
2665.275197	220.288631	46.955956
2661.786159	225.012745	46.960961
2658.003292	217.267084	46.965965
2654.760181	223.063720	46.970970
2651.165463	214.166378	46.975975
2647.817104	211.637983	46.980980
2644.082439	225.948230	46.985985
2640.982156	212.501510	46.990989
2637.458758	213.487593	46.995994
2633.635459	226.308308	47.000999
2630.128229	221.404364	47.006004
2626.495398	210.853290	47.011009
2623.590571	210.476529	47.016013
2619.740982	217.713846	47.021018
2616.514748	216.573385	47.026023
2613.443834	215.642518	47.031028
2609.566232	221.371332	47.036033
2606.487419	214.350187	47.041037
2603.198051	196.951532	47.046042
2599.780570	218.355232	47.051047
2596.364558	215.919211	47.056052
2592.678641	212.380690	47.061057
2589.264969	208.901071	47.066061
2585.402904	205.394363	47.071066
2582.072128	211.445709	47.076071
2579.004698	195.547380	47.081076
2574.817340	202.691923	47.086081
2571.929917	205.100207	47.091085
2568.293155	202.068495	47.096090
2564.607651	195.756535	47.101095
2561.458927	187.996653	47.106100
2557.443826	202.747587	47.111105
2554.894986	198.123309	47.116109
2550.983843	192.300123	47.121114
2547.464902	196.997635	47.126119
2544.211153	200.975906	47.131124
2540.382272	203.975018	47.136129
2537.078812	202.109854	47.141133
2533.298804	198.404562	47.146138
2529.817502	196.731317	47.151143
2526.726783	193.145893	47.156148
2523.317588	192.965303	47.161153
2519.637977	191.443943	47.166157
2515.987708	187.600754	47.171162
2512.651563	185.732706	47.176167
2509.226347	185.692393	47.181172
2505.680445	203.468488	47.186177
2502.295900	189.192651	47.191181
2499.142311	190.409547	47.196186
2495.253671	193.042150	47.201191
2491.848338	184.311793	47.206196
2488.246226	189.842893	47.211201
2484.657048	194.388732	47.216205
2481.140981	210.635451	47.221210
2477.715054	196.697347	47.226215
2474.493439	195.916192	47.231220
2471.099874	196.416652	47.236225
2467.465764	189.455782	47.241229
2463.888865	189.902716	47.246234
2460.177401	196.785921	47.251239
2456.913984	187.819964	47.256244
2453.169815	177.193058	47.261249
2449.882140	186.246908	47.266253
2446.519031	185.878800	47.271258
2442.987306	186.150477	47.276263
2440.131559	183.499413	47.281268
2436.067407	193.541618	47.286273
2432.635533	175.707832	47.291277
2428.939619	172.099134	47.296282
2425.620717	179.035407	47.301287
2421.952414	175.241120	47.306292
2418.361743	182.583698	47.311297
2415.123705	169.463923	47.316301
2411.513773	181.797050	47.321306
2408.233534	186.622280	47.326311
2404.823586	180.149542	47.331316
2400.787219	180.747849	47.336321
2397.771032	180.432260	47.341325
2393.861179	174.037531	47.346330
2390.427472	179.616862	47.351335
2386.889122	180.872689	47.356340
2383.696754	185.957016	47.361345
2380.208817	183.271027	47.366349
2376.855286	189.666664	47.371354
2373.174029	181.552910	47.376359
2369.730098	177.981809	47.381364
2365.928123	183.124253	47.386369
2362.489842	177.194884	47.391373
2359.343957	180.377809	47.396378
2355.639705	180.819258	47.401383
2352.285930	182.113819	47.406388
2348.852631	181.810113	47.411393
2345.151947	180.274065	47.416397
2341.836941	181.754029	47.421402
2338.029043	180.150722	47.426407
2334.812600	180.023768	47.431412
2331.164149	186.312179	47.436417
2327.737170	176.948942	47.441421
2324.375267	186.303354	47.446426
2320.535380	180.238878	47.451431
2317.150827	176.064188	47.456436
2313.673878	193.375223	47.461441
2310.420236	179.715155	47.466445
2306.770858	173.278801	47.471450
2303.337740	176.717583	47.476455
2300.095007	168.168888	47.481460
2296.568907	179.841228	47.486465
2292.988933	173.213088	47.491469
2289.118231	176.822210	47.496474
2285.165853	177.795735	47.501479
2282.468794	176.360868	47.506484
2278.865357	191.888711	47.511489
2275.637857	179.878553	47.516493
2271.713389	187.872436	47.521498
2268.311426	185.650320	47.526503
2264.531469	176.840105	47.531508
2260.783620	184.615930	47.536513
2257.943484	175.410285	47.541517
2254.567782	178.555089	47.546522
2250.648049	176.578008	47.551527
2247.590580	170.782816	47.556532
2243.434487	177.761043	47.561537
2240.297654	175.754981	47.566541
2237.080024	178.720405	47.571546
2233.233183	173.824353	47.576551
2230.100211	170.770601	47.581556
2226.634225	177.000347	47.586561
2222.728243	184.262709	47.591565
2219.280517	178.390615	47.596570
2215.717960	171.900431	47.601575
2212.505911	165.207413	47.606580
2209.015393	170.948512	47.611585
2205.475268	162.398704	47.616589
2201.844285	168.705690	47.621594
2197.911525	171.660037	47.626599
2194.906600	163.585296	47.631604
2191.451865	169.851378	47.636609
2187.713018	173.041010	47.641613
2184.264662	173.657975	47.646618
2180.822074	173.904417	47.651623
2177.702745	167.695627	47.656628
2173.779970	172.359856	47.661633
2170.320890	165.567116	47.666637
2167.174933	167.771438	47.671642
2163.225389	170.266752	47.676647
2159.916287	166.597257	47.681652
2156.072124	174.806232	47.686657
2153.020439	169.866580	47.691661
2149.358094	180.022183	47.696666
2145.553765	174.992589	47.701671
2142.531222	165.201073	47.706676
2138.676606	168.309488	47.711681
2135.536756	168.136246	47.716685
2131.893821	165.704638	47.721690
2128.483790	161.909543	47.726695
2125.243381	160.900390	47.731700
2121.016069	160.488318	47.736705
2117.634853	159.347107	47.741709
2114.472435	163.496244	47.746714
2111.029374	176.374359	47.751719
2107.542316	163.159298	47.756724
2103.998381	165.869799	47.761729
2100.249648	163.389461	47.766733
2096.601924	161.665052	47.771738
2092.949180	164.513770	47.776743
2090.040327	156.736377	47.781748
2086.029540	160.586241	47.786753
2083.124222	160.843156	47.791757
2079.325084	163.753913	47.796762
2076.177532	156.383698	47.801767
2072.605049	161.755084	47.806772
2069.052364	171.781732	47.811777
2065.246851	163.433140	47.816781
2061.822703	167.683582	47.821786
2058.336119	170.823572	47.826791
2054.901768	160.623616	47.831796
2050.914603	166.634153	47.836801
2047.732196	166.230006	47.841805
2044.108713	158.030959	47.846810
2040.847037	163.814485	47.851815
2037.831629	159.072634	47.856820
2033.777631	163.439713	47.861825
2030.271282	168.205502	47.866829
2026.979357	155.595045	47.871834
2022.983720	157.983097	47.876839
2019.952623	155.662339	47.881844
2016.184996	156.914819	47.886849
2013.057051	157.645146	47.891853
2009.517805	160.758228	47.896858
2005.853358	162.916832	47.901863
2002.450302	155.039972	47.906868
1998.822545	167.624297	47.911873
1995.193545	157.863648	47.916877
1991.968041	161.142126	47.921882
1988.058053	170.749356	47.926887
1985.092998	162.320571	47.931892
1981.133948	163.412363	47.936897
1977.768706	158.615585	47.941901
1974.443626	169.930382	47.946906
1970.502396	157.588575	47.951911
1967.731555	146.083885	47.956916
1963.941933	163.374646	47.961921
1960.266939	152.373392	47.966925
1957.241283	148.636720	47.971930
1953.550106	158.294974	47.976935
1950.186906	155.572150	47.981940
1946.378782	154.804426	47.986945
1942.772301	156.387992	47.991949
1939.243861	153.869624	47.996954
1935.469626	157.650743	48.001959
1932.431133	151.194926	48.006964
1928.721472	153.979313	48.011969
1925.491414	154.997634	48.016973
1921.860930	157.896033	48.021978
1918.093805	159.590367	48.026983
1914.711442	159.718375	48.031988
1910.981029	151.965718	48.036993
1907.874244	154.644143	48.041997
1904.435981	156.677774	48.047002
1900.762586	164.946290	48.052007
1897.288602	156.470201	48.057012
1893.766633	163.778266	48.062017
1890.313328	156.471315	48.067021
1886.749887	153.291922	48.072026
1882.864890	163.793248	48.077031
1879.837156	152.004916	48.082036
1876.204371	147.982004	48.087041
1872.821058	149.734485	48.092045
1869.855345	160.354865	48.097050
1865.741786	161.940340	48.102055
1862.215949	151.320121	48.107060
1858.916739	161.967706	48.112065
1855.217822	159.258387	48.117069
1851.914335	157.978590	48.122074
1848.373897	159.906867	48.127079
1844.996845	154.815937	48.132084
1841.405308	154.179562	48.137089
1837.627464	161.538053	48.142093
1834.253291	145.385968	48.147098
1830.419918	157.801924	48.152103
1827.401776	154.639440	48.157108
1823.729751	161.036524	48.162113
1820.064104	149.751657	48.167117
1816.816709	154.548407	48.172122
1813.228525	154.676384	48.177127
1809.912275	159.574671	48.182132
1805.791662	152.511747	48.187137
1802.617329	150.602245	48.192141
1799.597453	140.872636	48.197146
1795.914559	146.325396	48.202151
1792.531186	142.970924	48.207156
1788.884961	150.555643	48.212161
1785.400303	145.593491	48.217165
1781.694429	137.206153	48.222170
1778.013079	139.669250	48.227175
1774.873980	141.863421	48.232180
1770.986854	144.759838	48.237185
1767.530930	147.816759	48.242189
1763.960955	144.703920	48.247194
1760.636163	156.599331	48.252199
1757.457368	144.393025	48.257204
1753.724737	153.279692	48.262209
1750.179296	160.489676	48.267213
1746.965438	146.486689	48.272218
1743.321606	149.191735	48.277223
1739.698825	143.854218	48.282228
1736.259245	146.718441	48.287233
1732.828007	131.330679	48.292237
1729.333466	143.075530	48.297242
1725.411176	139.754668	48.302247
1722.468966	145.722573	48.307252
1718.490747	150.689475	48.312257
1715.136476	149.387046	48.317261
1711.930048	141.656380	48.322266
1708.003823	145.278098	48.327271
1704.816543	143.969333	48.332276
1700.636967	137.467708	48.337281
1697.718688	144.478918	48.342285
1694.147701	136.321052	48.347290
1690.697525	147.878156	48.352295
1687.246894	142.204353	48.357300
1683.762019	143.225757	48.362305
1680.097158	131.879103	48.367309
1676.594847	133.707147	48.372314
1673.141416	142.182938	48.377319
1669.633928	135.491211	48.382324
1666.129617	131.571133	48.387329
1662.714207	130.201671	48.392333
1659.441099	130.578145	48.397338
1655.805198	138.125892	48.402343
1652.163598	138.012076	48.407348
1648.846658	147.666507	48.412353
1645.361427	138.539614	48.417357
1641.622631	128.297619	48.422362
1637.670331	134.439923	48.427367
1634.694978	130.802441	48.432372
1630.981927	133.604597	48.437377
1627.814160	143.175025	48.442381
1624.161465	143.448903	48.447386
1620.450587	143.209598	48.452391
1617.045512	134.905222	48.457396
1613.660608	142.296536	48.462401
1610.147111	142.462999	48.467405
1606.706589	140.884115	48.472410
1603.410983	154.150831	48.477415
1600.177766	132.241495	48.482420
1596.060403	141.412999	48.487425
1592.534270	135.040688	48.492429
1588.940817	142.812910	48.497434
1585.481671	140.484257	48.502439
1582.260506	136.428805	48.507444
1578.634060	136.696400	48.512449
1574.938578	134.266661	48.517453
1571.442137	139.898892	48.522458
1567.796223	129.639642	48.527463
1564.613992	125.685115	48.532468
1560.866762	132.885847	48.537473
1557.354427	128.853400	48.542477
1554.133693	125.480304	48.547482
1550.679283	133.965179	48.552487
1547.693076	127.999941	48.557492
1543.602811	139.833104	48.562497
1540.071133	144.807006	48.567501
1536.808131	135.860649	48.572506
1532.926522	131.256863	48.577511
1529.282512	135.308511	48.582516
1525.692372	137.746616	48.587521
1522.284703	140.547362	48.592525
1518.816301	134.520929	48.597530
1515.264338	130.067563	48.602535
1512.129865	127.832763	48.607540
1508.659660	136.252288	48.612545
1505.150070	131.395235	48.617549
1501.545466	136.958527	48.622554
1497.742834	146.140097	48.627559
1494.467894	140.229732	48.632564
1490.886636	142.169650	48.637569
1487.327919	128.227894	48.642573
1484.082198	140.455340	48.647578
1480.602852	140.010873	48.652583
1477.200774	129.386363	48.657588
1473.437906	123.463312	48.662593
1470.295817	133.086180	48.667597
1466.539245	128.613533	48.672602
1463.065984	131.443875	48.677607
1459.416468	136.292331	48.682612
1455.867033	132.628428	48.687617
1452.207621	144.340312	48.692621
1449.188079	138.374503	48.697626
1445.378476	135.555920	48.702631
1442.156891	133.986072	48.707636
1438.352981	139.481855	48.712641
1435.155274	143.219662	48.717645
1431.626374	134.886697	48.722650
1427.876913	138.237182	48.727655
1424.615671	126.547545	48.732660
1420.991737	135.769006	48.737665
1417.149946	135.410731	48.742669
1414.050464	126.972279	48.747674
1410.243653	137.298893	48.752679
1406.963741	131.098756	48.757684
1403.422521	133.132146	48.762689
1399.721756	140.229686	48.767693
1396.573711	128.250865	48.772698
1392.675446	133.630140	48.777703
1389.294148	131.677745	48.782708
1386.130314	122.139944	48.787713
1382.763443	120.202833	48.792717
1379.052607	128.760582	48.797722
1375.224508	126.227549	48.802727
1371.718703	116.201025	48.807732
1368.502551	129.797910	48.812737
1364.914256	125.310276	48.817741
1361.337333	126.507345	48.822746
1357.871533	132.568995	48.827751
1354.554814	125.641648	48.832756
1350.897919	133.987276	48.837761
1347.540817	135.933280	48.842765
1343.918981	127.831276	48.847770
1340.326559	135.333900	48.852775
1336.836510	124.326609	48.857780
1333.244956	124.470677	48.862785
1329.717163	131.364580	48.867789
1326.613022	124.773505	48.872794
1322.266383	129.128771	48.877799
1319.209653	127.811859	48.882804
1315.943540	133.461923	48.887809
1312.169402	144.532884	48.892813
1309.189749	137.960727	48.897818
1305.802611	139.260770	48.902823
1302.165269	139.098979	48.907828
1298.172163	141.394161	48.912833
1294.435900	141.088681	48.917837
1291.467586	132.081885	48.922842
1287.366220	134.709855	48.927847
1284.376887	129.477788	48.932852
1280.745846	132.001786	48.937857
1277.484506	134.070726	48.942861
1273.806759	124.587331	48.947866
1270.202732	132.418355	48.952871
1267.300709	118.135230	48.957876
1262.964786	131.590828	48.962881
1259.722977	125.435489	48.967885
1256.909228	120.997449	48.972890
1252.606084	138.463171	48.977895
1249.497633	130.841980	48.982900
1245.529437	136.691232	48.987905
1241.610182	141.869338	48.992909
1238.809859	131.172473	48.997914
1235.087214	129.000561	49.002919
1231.978150	124.544094	49.007924
1228.678255	124.940383	49.012929
1224.960998	131.781452	49.017933
1221.553609	122.258593	49.022938
1217.688284	136.720277	49.027943
1214.011104	121.702088	49.032948
1210.636907	130.890795	49.037953
1207.288073	131.112164	49.042957
1203.804905	131.188191	49.047962
1200.125514	127.666145	49.052967
1196.803787	137.501971	49.057972
1193.067410	143.852637	49.062977
1189.673126	129.695794	49.067981
1186.456002	131.675887	49.072986
1182.607856	139.732036	49.077991
1179.563040	133.357953	49.082996
1175.787536	147.892049	49.088001
1172.152117	137.516179	49.093005
1168.909024	132.167616	49.098010
1165.263625	130.394093	49.103015
1161.663546	121.186717	49.108020
1158.448740	121.719542	49.113025
1154.346625	122.824551	49.118029
1150.928941	115.591678	49.123034
1147.792705	130.192590	49.128039
1144.402687	125.667613	49.133044
1140.604809	127.451083	49.138049
1137.249851	126.314404	49.143053
1134.011550	127.840743	49.148058
1129.969505	127.175619	49.153063
1126.726183	115.824070	49.158068
1123.165028	132.890618	49.163073
1119.722230	128.709602	49.168077
1116.277054	116.207799	49.173082
1112.488884	116.238923	49.178087
1109.020320	123.353701	49.183092
1105.681507	125.619009	49.188097
1101.979690	117.998094	49.193101
1098.686603	131.686595	49.198106
1095.078759	126.550418	49.203111
1091.513543	125.570808	49.208116
1088.238563	119.819021	49.213121
1084.832930	123.712645	49.218125
1081.254023	125.677041	49.223130
1077.494909	127.413696	49.228135
1074.207441	124.308266	49.233140
1070.401245	119.529137	49.238145
1067.027785	115.607815	49.243149
1063.765728	111.818949	49.248154
1059.996077	123.840409	49.253159
1057.003561	128.850906	49.258164
1053.459015	125.309938	49.263169
1049.674757	125.334729	49.268173
1046.013814	119.473445	49.273178
1042.351750	127.610710	49.278183
1039.038758	122.027021	49.283188
1035.767462	122.773942	49.288193
1031.878910	126.554349	49.293197
1028.806702	118.235126	49.298202
1025.021462	131.781548	49.303207
1021.547835	120.997275	49.308212
1018.065592	124.174311	49.313217
1014.300312	122.257290	49.318221
1011.196316	114.490673	49.323226
1007.511419	122.755141	49.328231
1004.444345	122.056289	49.333236
1000.663274	121.435960	49.338241
996.716944	131.255017	49.343245
993.367144	122.021420	49.348250
989.759842	130.921656	49.353255
986.718145	121.736244	49.358260
983.560230	116.928171	49.363265
979.498003	124.580044	49.368269
976.153933	116.145322	49.373274
972.686133	117.408923	49.378279
969.021632	119.724813	49.383284
965.452592	118.687202	49.388289
961.834526	125.387905	49.393293
958.586716	121.757450	49.398298
955.229011	131.550963	49.403303
951.872382	120.746824	49.408308
948.288176	116.947771	49.413313
944.499883	113.266179	49.418317
941.035617	118.307155	49.423322
937.065811	127.941878	49.428327
933.971861	114.584861	49.433332
930.740285	118.713229	49.438337
926.933158	115.954429	49.443341
923.458783	112.494887	49.448346
919.709742	115.045257	49.453351
916.550435	122.691522	49.458356
913.123063	109.364517	49.463361
909.789389	119.323465	49.468365
906.051257	123.733884	49.473370
902.083631	128.559659	49.478375
899.008053	116.508896	49.483380
895.268980	113.568105	49.488385
891.787901	112.743117	49.493389
888.267966	114.200151	49.498394
884.853658	118.768727	49.503399
881.645035	112.412878	49.508404
878.119685	115.981364	49.513409
874.794402	118.733486	49.518413
871.063669	112.600988	49.523418
867.326697	110.439152	49.528423
863.740968	122.819723	49.533428
860.255520	119.651400	49.538433
856.696403	123.158585	49.543437
853.578513	119.280414	49.548442
849.690153	125.771073	49.553447
846.509383	130.087515	49.558452
843.139783	125.332916	49.563457
839.164143	125.919409	49.568461
836.273051	130.344588	49.573466
832.201978	132.304650	49.578471
828.860949	115.906967	49.583476
825.543220	127.226649	49.588481
821.762344	117.834275	49.593485
818.614288	114.673600	49.598490
814.852172	118.554098	49.603495
811.424335	112.204890	49.608500
808.043065	115.607553	49.613505
804.505394	115.472289	49.618509
800.688288	120.215843	49.623514
797.144504	128.771525	49.628519
793.756076	118.794147	49.633524
790.453654	118.190987	49.638529
786.496142	118.607591	49.643533
783.452400	121.001905	49.648538
779.683629	122.526231	49.653543
776.439882	119.383746	49.658548
772.955211	124.442674	49.663553
769.464693	117.979927	49.668557
765.919179	116.047774	49.673562
762.459214	125.768075	49.678567
759.155573	120.561738	49.683572
755.334346	133.716239	49.688577
752.140204	121.728053	49.693581
748.655999	117.544614	49.698586
744.730824	123.238049	49.703591
741.072322	117.883443	49.708596
737.928019	111.278304	49.713601
734.272941	110.078435	49.718605
731.051583	102.318632	49.723610
727.087922	114.449616	49.728615
723.394669	108.236734	49.733620
720.284780	104.863716	49.738625
716.395873	107.790678	49.743629
713.346295	108.432769	49.748634
709.410207	120.843835	49.753639
706.378790	104.876951	49.758644
702.680401	121.203390	49.763649
699.057060	126.172885	49.768653
696.027343	117.028377	49.773658
692.149564	125.206952	49.778663
688.860554	117.965923	49.783668
685.654075	117.115623	49.788673
681.901542	113.292829	49.793677
678.441494	115.628576	49.798682
675.094749	128.281511	49.803687
671.367940	118.626170	49.808692
667.345289	118.573049	49.813697
664.226163	119.384300	49.818701
660.899414	122.634978	49.823706
657.179667	121.303076	49.828711
653.748716	120.298669	49.833716
650.136281	117.512419	49.838721
646.640426	109.500351	49.843725
643.367084	110.878210	49.848730
639.618549	128.636074	49.853735
636.396176	103.370382	49.858740
632.809670	117.349198	49.863745
628.800703	116.010524	49.868749
625.494966	105.740998	49.873754
621.871945	118.302640	49.878759
618.691134	108.611720	49.883764
615.656713	113.396676	49.888769
612.166778	121.634059	49.893773
608.530658	120.571713	49.898778
604.330370	120.239373	49.903783
600.844090	117.212905	49.908788
597.512083	114.472614	49.913793
593.957749	121.714449	49.918797
590.677034	107.336132	49.923802
587.209125	127.423101	49.928807
583.871259	121.653466	49.933812
580.165146	112.604169	49.938817
576.461846	121.797268	49.943821
573.190042	115.692843	49.948826
569.486970	123.971073	49.953831
566.310174	115.597954	49.958836
563.095617	116.251775	49.963841
559.363198	109.380721	49.968845
555.809486	112.251029	49.973850
551.905599	107.744473	49.978855
548.235181	115.361550	49.983860
544.862000	112.310416	49.988865
541.533562	108.702184	49.993869
538.423779	103.483194	49.998874
534.889335	113.624419	50.003879
530.945790	103.444715	50.008884
527.787383	117.531725	50.013889
523.881701	120.875232	50.018893
520.866238	106.207692	50.023898
517.046800	107.615338	50.028903
513.605026	108.429048	50.033908
509.668339	126.005335	50.038913
506.288216	121.530775	50.043917
503.008958	116.464395	50.048922
499.686778	111.330525	50.053927
495.919215	104.213156	50.058932
493.133433	103.437302	50.063937
489.134280	119.222455	50.068941
485.517440	109.074151	50.073946
481.861835	106.008834	50.078951
478.432280	104.410680	50.083956
474.898211	113.637823	50.088961
471.363783	102.110525	50.093965
468.375926	109.667177	50.098970
464.672187	122.574593	50.103975
461.308081	112.767044	50.108980
457.692313	113.718637	50.113985
453.974910	123.719155	50.118989
450.555696	116.894396	50.123994
446.941129	117.014129	50.128999
443.595094	114.227600	50.134004
440.281717	117.011011	50.139009
436.683572	116.543205	50.144013
433.062230	105.651917	50.149018
429.147861	113.006179	50.154023
426.179657	106.288563	50.159028
422.557005	101.877404	50.164033
418.874777	102.237803	50.169037
415.620488	93.214126	50.174042
412.123322	107.928342	50.179047
408.329764	116.003169	50.184052
404.733162	104.644921	50.189057
401.202723	106.867044	50.194061
398.063908	105.144940	50.199066
394.594279	111.584416	50.204071
391.189866	103.960215	50.209076
387.397607	105.347365	50.214081
383.749217	107.020627	50.219085
380.623701	98.736231	50.224090
376.997029	105.411003	50.229095
373.592249	111.016297	50.234100
370.331232	104.570539	50.239105
366.606973	102.956709	50.244109
363.079309	102.823189	50.249114
359.225277	116.375129	50.254119
355.922321	114.180471	50.259124
352.274004	113.262055	50.264129
348.480181	102.379688	50.269133
345.759468	108.875411	50.274138
341.925292	107.949724	50.279143
338.018062	100.024065	50.284148
334.686905	98.083481	50.289153
331.248387	109.805684	50.294157
328.129154	97.308477	50.299162
324.603126	98.471929	50.304167
321.241604	98.882101	50.309172
317.703976	105.068546	50.314177
313.847088	102.490893	50.319181
310.439722	97.666189	50.324186
306.947495	112.981432	50.329191
303.430886	108.206839	50.334196
299.934532	101.264501	50.339201
295.977694	122.100130	50.344205
292.606161	109.178569	50.349210
288.887497	111.270447	50.354215
285.732803	105.496675	50.359220
282.818267	106.840194	50.364225
278.923358	101.159814	50.369229
275.686618	102.846023	50.374234
271.701492	109.313897	50.379239
268.649828	104.953322	50.384244
265.189216	105.597134	50.389249
261.367834	118.388814	50.394253
257.833727	112.850683	50.399258
254.328080	113.770679	50.404263
250.903981	109.003228	50.409268
247.465400	103.625819	50.414273
243.738751	104.013288	50.419277
240.167417	100.555160	50.424282
236.662130	107.233427	50.429287
233.086205	102.663622	50.434292
229.665358	104.157014	50.439297
226.159859	110.212708	50.444301
223.398294	100.235619	50.449306
219.523934	114.332796	50.454311
215.788110	99.570096	50.459316
212.483943	102.845173	50.464321
208.347064	110.842455	50.469325
205.452261	111.442042	50.474330
201.741291	107.993786	50.479335
198.143175	105.635577	50.484340
194.804391	105.739679	50.489345
191.036853	104.137445	50.494349
187.653341	104.596208	50.499354
184.231859	114.518258	50.504359
180.944873	113.121249	50.509364
177.507236	98.603204	50.514369
173.740358	114.135639	50.519373
170.518813	98.746184	50.524378
166.835511	113.880549	50.529383
163.064347	107.244052	50.534388
159.774865	103.242078	50.539393
155.926816	106.811563	50.544397
152.673223	98.719924	50.549402
149.120352	109.144640	50.554407
146.188074	108.437244	50.559412
142.564861	98.717014	50.564417
138.464284	107.269092	50.569421
135.026141	103.776094	50.574426
131.600251	114.991872	50.579431
128.315339	116.166397	50.584436
124.893812	104.078959	50.589441
121.103966	109.648062	50.594445
118.012332	114.208176	50.599450
114.126930	111.419007	50.604455
110.742582	104.662592	50.609460
107.177768	106.792290	50.614465
103.464578	105.234009	50.619469
100.064055	106.415615	50.624474
96.619744	105.816825	50.629479
93.070268	91.860818	50.634484
89.489692	108.242305	50.639489
86.013650	102.172013	50.644493
82.796785	91.511386	50.649498
78.860772	113.410210	50.654503
75.569811	105.559885	50.659508
72.480658	104.133796	50.664513
68.632633	117.730260	50.669517
65.256452	94.582132	50.674522
61.710502	102.438633	50.679527
58.380379	97.062655	50.684532
54.667297	99.220729	50.689537
50.885968	109.923073	50.694541
47.800012	90.960995	50.699546
44.026499	103.762119	50.704551
40.370094	91.290232	50.709556
37.321584	91.745707	50.714561
33.638444	104.070294	50.719565
30.112483	93.496589	50.724570
26.561187	100.707206	50.729575
23.102305	98.677108	50.734580
20.063850	111.465892	50.739585
16.250347	98.490396	50.744589
12.853364	94.140558	50.749594
8.739360	96.960888	50.754599
5.289640	100.411160	50.759604
1.943926	100.935300	50.764609