Thu Jun 16 18:50:03 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.936787	111.472716	0.000000
0.334942	107.280041	0.005005
0.505324	107.519894	0.010010
0.488250	104.061063	0.015014
0.359581	95.074278	0.020019
0.591045	86.246604	0.025024
0.098086	75.437100	0.030029
-0.188356	71.627283	0.035034
-0.645741	66.185747	0.040038
-0.600642	48.500572	0.045043
-1.143226	32.591344	0.050048
-1.329598	35.521374	0.055053
-1.845241	35.192694	0.060058
-1.986941	29.703837	0.065062
-2.015682	21.936429	0.070067
-2.294697	9.429087	0.075072
-2.971254	12.672353	0.080077
-2.702185	-3.752959	0.085082
-3.699922	-1.364537	0.090086
-3.512983	-2.321635	0.095091
-3.295598	-9.898651	0.100096
-4.233674	-17.607217	0.105101
-4.727682	-26.805249	0.110106
-4.864566	-16.008809	0.115110
-4.992899	-24.541867	0.120115
-5.566807	-18.458045	0.125120
-5.799309	-14.765990	0.130125
-6.632263	-17.323022	0.135130
-6.265893	-9.766688	0.140134
-6.483052	-21.991123	0.145139
-6.771777	-15.314950	0.150144
-6.878296	-13.246159	0.155149
-6.953142	-15.515015	0.160154
-6.906088	-16.411112	0.165158
-7.475521	-19.327585	0.170163
-7.891826	-26.124778	0.175168
-8.361646	-19.703298	0.180173
-8.230791	-28.407930	0.185178
-8.333560	-18.637907	0.190182
-8.715530	-15.963041	0.195187
-9.325955	-27.493658	0.200192
-10.147815	-10.510849	0.205197
-10.096776	-19.356197	0.210202
-10.197306	-9.791247	0.215206
-10.169374	-17.398314	0.220211
-10.184246	-22.919161	0.225216
-10.313917	-14.124328	0.230221
-10.266843	-9.952448	0.235226
-10.899655	-9.856588	0.240230
-11.332735	-10.661008	0.245235
-11.214851	-18.513396	0.250240
-11.756300	-7.733949	0.255245
-12.410698	-23.988475	0.260250
-12.852617	-6.614641	0.265254
-12.929605	-9.775572	0.270259
-12.591699	-16.462513	0.275264
-13.141166	-17.103169	0.280269
-13.059444	-19.551799	0.285274
-13.328673	-14.041688	0.290278
-14.006644	-19.739247	0.295283
-14.103315	-29.716705	0.300288
-14.834934	-22.305569	0.305293
-14.738520	-31.404946	0.310298
-14.752680	-23.983733	0.315302
-14.809059	-27.148461	0.320307
-15.580145	-17.600162	0.325312
-16.190831	-14.996511	0.330317
-16.274926	-22.042856	0.335322
-16.376510	-22.026204	0.340326
-16.576948	-25.476011	0.345331
-16.238300	-18.961430	0.350336
-16.524698	-21.201045	0.355341
-16.311240	-24.764437	0.360346
-17.553340	-23.806175	0.365350
-17.806185	-23.993108	0.370355
-18.433376	-23.131237	0.375360
-18.372285	-14.714503	0.380365
-18.373677	-20.266484	0.385370
-18.289787	-11.666665	0.390374
-18.942375	-21.066482	0.395379
-19.509173	-22.178801	0.400384
-19.982178	-14.704445	0.405389
-20.114257	-31.560453	0.410394
-19.963801	-16.454134	0.415398
-19.780342	-26.821007	0.420403
-19.866567	-21.398460	0.425408
-20.686014	-9.269256	0.430413
-21.077220	-16.450517	0.435418
-21.618771	-15.662682	0.440422
-21.694544	-15.242753	0.445427
-21.434056	-5.011958	0.450432
-21.541845	-13.430523	0.455437
-21.673008	-23.070015	0.460442
-22.512640	-7.104058	0.465446
-22.634476	-13.989873	0.470451
-22.936160	-20.131804	0.475456
-23.576225	-12.158863	0.480461
-23.223205	-15.016067	0.485466
-23.073050	-14.114849	0.490470
-23.720926	-15.013106	0.495475
-24.186771	-24.741027	0.500480
-24.743117	-12.990138	0.505485
-24.488014	-31.562002	0.510490
-24.623002	-9.279047	0.515494
-25.320532	-15.856233	0.520499
-25.485358	-11.442261	0.525504
-25.721666	-17.552082	0.530509
-25.874542	-18.819128	0.535514
-26.043490	-11.025756	0.540518
-26.336770	-14.918275	0.545523
-25.926538	-10.489041	0.550528
-27.230145	-19.767556	0.555533
-27.084666	-14.333774	0.560538
-27.601952	-13.644361	0.565542
-27.695420	-10.303900	0.570547
-27.523534	-25.131003	0.575552
-28.510335	-8.502037	0.580557
-28.656846	-23.231340	0.585562
-29.082127	-15.711993	0.590566
-29.403561	-17.396608	0.595571
-29.136961	-16.126626	0.600576
-29.049690	-9.154868	0.605581
-28.964540	-20.631442	0.610586
-29.896900	-21.488011	0.615590
-30.616142	-18.070476	0.620595
-30.774379	-21.083017	0.625600
-30.828667	-11.478850	0.630605
-30.717592	-30.697367	0.635610
-30.752127	-16.934833	0.640614
-31.900099	-16.349943	0.645619
-32.155477	-20.311863	0.650624
-32.028819	-12.172234	0.655629
-32.153871	-17.040623	0.660634
-32.407853	-20.569089	0.665638
-32.479465	-14.659727	0.670643
-32.305466	-20.906808	0.675648
-33.371652	-13.293282	0.680653
-33.589093	-25.035638	0.685658
-33.964925	-17.238070	0.690662
-34.194105	-19.157142	0.695667
-33.962011	-27.418971	0.700672
-34.301060	-9.408854	0.705677
-34.488719	-21.673972	0.710682
-34.811161	-20.542329	0.715686
-35.282826	-11.529283	0.720691
-35.328030	-15.366414	0.725696
-35.839898	-28.263792	0.730701
-35.501228	-18.337255	0.735706
-36.415576	-2.468057	0.740710
-37.375195	-14.841289	0.745715
-36.398727	-5.091574	0.750720
-36.928737	-4.830683	0.755725
-36.966110	-10.976243	0.760730
-37.101290	-22.155856	0.765734
-37.371985	-16.276931	0.770739
-37.889270	-34.335798	0.775744
-38.292963	-19.669553	0.780749
-38.556618	-24.453868	0.785754
-39.019512	-14.379173	0.790758
-38.915389	-15.427948	0.795763
-39.023624	-20.284120	0.800768
-39.690758	-24.402626	0.805773
-40.174895	-30.875671	0.810778
-40.571480	-20.599339	0.815782
-40.157650	-21.994767	0.820787
-40.071995	-30.420823	0.825792
-40.512132	-18.186895	0.830797
-40.417366	-22.579791	0.835802
-41.023400	-18.603047	0.840806
-41.821721	-22.716052	0.845811
-41.898112	-17.524205	0.850816
-42.439667	-18.538291	0.855821
-41.999180	-15.732091	0.860826
-42.210314	-20.448728	0.865830
-42.482211	-18.789252	0.870835
-43.064062	-16.721323	0.875840
-43.532145	-18.514885	0.880845
-43.437578	-27.387348	0.885850
-43.938412	-15.551421	0.890854
-43.766621	-20.382839	0.895859
-43.837084	-27.676095	0.900864
-44.394721	-21.196497	0.905869
-44.853137	-30.304905	0.910874
-45.283279	-13.126588	0.915878
-45.505118	-23.278795	0.920883
-45.296150	-21.687443	0.925888
-45.419024	-14.870573	0.930893
-45.607950	-31.566930	0.935898
-46.668064	-27.290016	0.940902
-46.989842	-18.528453	0.945907
-46.712182	-17.813652	0.950912
-46.952537	-12.648868	0.955917
-47.184246	-33.961198	0.960922
-47.434159	-24.188864	0.965926
-47.595505	-14.183538	0.970931
-47.823451	-24.951917	0.975936
-48.793337	-17.525472	0.980941
-48.486906	-28.872671	0.985946
-49.028710	-12.912336	0.990950
-48.828313	-15.225296	0.995955
-48.723729	-29.722715	1.000960
-49.217075	-12.645925	1.005965
-49.895708	-25.080381	1.010970
-50.086543	-12.438279	1.015974
-50.342941	-17.998429	1.020979
-50.421775	-15.149911	1.025984
-50.687103	-15.459281	1.030989
-50.696065	-17.822681	1.035994
-51.408991	-5.683357	1.040998
-51.878536	-15.737410	1.046003
-51.626252	-8.120299	1.051008
-51.815070	-4.584034	1.056013
-51.776604	-15.739666	1.061018
-52.218422	-18.431081	1.066022
-52.735077	-15.074450	1.071027
-52.943337	-18.072015	1.076032
-53.494231	-12.844466	1.081037
-53.388085	-14.742003	1.086042
-53.376857	-15.525337	1.091046
-54.036694	-18.826118	1.096051
-54.380402	-18.223102	1.101056
-54.671310	-10.025711	1.106061
-54.857094	-23.503597	1.111066
-54.708658	-25.774328	1.116070
-54.790187	-17.885211	1.121075
-55.454651	-17.670466	1.126080
-56.147379	-20.813094	1.131085
-56.128490	-19.825959	1.136090
-56.684803	-9.556469	1.141094
-56.774269	-21.492916	1.146099
-56.296053	-13.480941	1.151104
-56.579296	-8.928618	1.156109
-57.500250	-15.046041	1.161114
-57.758631	-12.166962	1.166118
-58.057690	-21.870156	1.171123
-57.865790	-25.021062	1.176128
-58.163844	-18.408956	1.181133
-57.881778	-21.531554	1.186138
-58.454985	-27.701214	1.191142
-59.324045	-20.059990	1.196147
-59.168162	-21.516080	1.201152
-59.983060	-32.867669	1.206157
-59.741038	-33.609826	1.211162
-59.916687	-28.990152	1.216166
-60.302522	-17.413851	1.221171
-60.793073	-35.098592	1.226176
-61.362749	-12.520654	1.231181
-61.420668	-13.645645	1.236186
-61.367850	-24.570126	1.241190
-61.441392	-20.496506	1.246195
-61.467746	-17.529694	1.251200
-61.839931	-19.622438	1.256205
-61.823263	-22.596995	1.261210
-62.465406	-18.893770	1.266214
-62.768162	-24.892666	1.271219
-62.874775	-23.582612	1.276224
-62.725635	-18.330372	1.281229
-63.558880	-21.923119	1.286234
-63.783854	-23.464247	1.291238
-64.535496	-15.324195	1.296243
-64.381595	-25.568781	1.301248
-64.735353	-14.484442	1.306253
-64.542091	-16.844169	1.311258
-64.669269	-13.676407	1.316262
-65.093369	-17.362522	1.321267
-65.570835	-21.088651	1.326272
-66.108241	-22.219535	1.331277
-66.111451	-25.015005	1.336282
-65.985425	-15.003704	1.341286
-66.330993	-24.922759	1.346291
-66.896412	-30.107555	1.351296
-67.236399	-22.362578	1.356301
-67.561537	-15.137592	1.361306
-67.731970	-9.172437	1.366310
-67.612847	-11.955374	1.371315
-67.210178	-20.111029	1.376320
-68.166362	-17.667808	1.381325
-68.714742	-11.713492	1.386330
-68.978875	-26.528806	1.391334
-69.383951	-13.158451	1.396339
-69.489347	-27.062781	1.401344
-69.730846	-18.205079	1.406349
-69.713244	-18.773610	1.411354
-69.465874	-22.863009	1.416358
-70.252997	-17.936087	1.421363
-70.724839	-18.695423	1.426368
-71.170414	-14.661240	1.431373
-71.044400	-18.970412	1.436378
-71.122584	-10.405866	1.441382
-71.275068	-17.616609	1.446387
-72.041479	-23.675514	1.451392
-72.854130	-15.403638	1.456397
-72.203614	-16.914839	1.461402
-72.556481	-9.066508	1.466406
-72.876855	-12.229732	1.471411
-72.612058	-16.932782	1.476416
-72.718085	-20.324002	1.481421
-73.237221	-17.570923	1.486426
-73.754527	-26.505631	1.491430
-74.287212	-15.641417	1.496435
-74.173325	-13.044058	1.501440
-74.199086	-13.838840	1.506445
-74.746328	-24.229082	1.511450
-75.155449	-11.716350	1.516454
-75.806831	-18.460677	1.521459
-75.643686	-20.751005	1.526464
-76.184350	-15.622716	1.531469
-76.220296	-7.353516	1.536474
-75.830125	-18.579304	1.541478
-76.163726	-10.291397	1.546483
-76.666345	-8.343698	1.551488
-77.300964	-5.125218	1.556493
-77.355211	-2.887289	1.561498
-77.006771	-15.540521	1.566502
-77.801473	-14.999703	1.571507
-78.231108	-14.069750	1.576512
-78.878262	-9.365239	1.581517
-79.113245	-19.277218	1.586522
-79.260448	-17.917540	1.591526
-79.402473	-16.760762	1.596531
-79.001731	-25.859922	1.601536
-79.125553	-18.525654	1.606541
-79.187728	-16.056849	1.611546
-79.755422	-18.046742	1.616550
-80.508516	-22.248408	1.621555
-80.500489	-15.954339	1.626560
-80.834053	-18.536280	1.631565
-80.826739	-26.766976	1.636570
-81.681677	-23.466311	1.641574
-82.446053	-13.427226	1.646579
-81.663905	-31.634644	1.651584
-81.965640	-14.605411	1.656589
-82.339959	-18.488971	1.661594
-82.347030	-11.931365	1.666598
-82.751176	-14.571784	1.671603
-82.455142	-20.767803	1.676608
-83.446475	-15.571937	1.681613
-83.990517	-18.343333	1.686618
-84.207674	-26.908660	1.691622
-84.115349	-12.354578	1.696627
-84.024922	-21.674938	1.701632
-84.139057	-10.538944	1.706637
-84.851667	-14.905051	1.711642
-84.984029	-13.412669	1.716646
-85.672665	-3.779135	1.721651
-85.871847	-14.098162	1.726656
-85.752003	-7.801260	1.731661
-85.916771	-18.671629	1.736666
-85.795061	-20.298663	1.741670
-86.823171	-18.901424	1.746675
-86.804926	-15.351833	1.751680
-87.115454	-12.691534	1.756685
-87.244404	-24.965159	1.761690
-87.213135	-16.945028	1.766694
-88.060925	-9.459240	1.771699
-88.329170	-11.626776	1.776704
-88.558099	-13.811267	1.781709
-88.835158	-17.590837	1.786714
-89.063532	-22.207446	1.791718
-89.168444	-5.933870	1.796723
-88.856312	-18.704613	1.801728
-88.931641	-12.861133	1.806733
-89.962124	-12.617066	1.811738
-90.122290	-21.537401	1.816742
-90.524208	-8.735124	1.821747
-90.323893	-10.999830	1.826752
-90.530269	-7.863076	1.831757
-91.305426	-15.501373	1.836762
-91.600183	-15.068732	1.841766
-91.980034	-7.989589	1.846771
-91.867686	-14.544936	1.851776
-92.223979	-10.358880	1.856781
-92.444553	-19.463088	1.861786
-92.160488	-25.702705	1.866790
-92.691369	-16.207420	1.871795
-93.048279	-25.733530	1.876800
-93.638751	-10.971301	1.881805
-93.786750	-20.805411	1.886810
-93.745972	-24.966620	1.891814
-94.288451	-12.858628	1.896819
-94.018424	-15.666010	1.901824
-94.685388	-16.520360	1.906829
-95.119059	-18.644770	1.911834
-95.099338	-19.880258	1.916838
-95.603213	-16.579406	1.921843
-95.319217	-17.945191	1.926848
-95.568803	-15.247511	1.931853
-96.071015	-11.598189	1.936858
-96.657430	-13.156728	1.941862
-97.116588	-3.405049	1.946867
-97.342818	-12.207627	1.951872
-96.752262	-2.627955	1.956877
-97.262881	-8.525513	1.961882
-97.009068	-14.160316	1.966886
-97.596846	-13.329614	1.971891
-97.750578	-11.288734	1.976896
-98.637998	-14.686362	1.981901
-98.674990	-16.292298	1.986906
-98.608594	-25.832923	1.991910
-99.062934	-14.774877	1.996915
-99.619256	-16.493869	2.006912
-99.248798	-12.829011	2.016909
-98.653118	-12.429778	2.026906
-97.571352	-19.631056	2.036902
-97.676338	-26.074131	2.046899
-97.199887	-25.804598	2.056896
-96.991702	-31.660813	2.066893
-96.360888	-20.394601	2.076890
-95.210542	-22.116586	2.086886
-94.714699	-28.577565	2.096883
-94.897014	-25.950020	2.106880
-94.399374	-18.553161	2.116877
-93.152880	-21.810184	2.126874
-93.052565	-19.822428	2.136870
-92.989611	-20.216816	2.146867
-91.884194	-24.616332	2.156864
-91.480471	-21.583095	2.166861
-91.290816	-15.934573	2.176858
-90.221767	-22.609963	2.186854
-90.006552	-21.249241	2.196851
-89.834384	-26.090411	2.206848
-89.233939	-15.959054	2.216845
-88.559684	-21.998589	2.226842
-88.357295	-13.316985	2.236838
-87.188582	-15.998894	2.246835
-86.721239	-23.884818	2.256832
-86.720236	-18.417991	2.266829
-86.176778	-14.718011	2.276826
-85.267510	-14.897153	2.286822
-85.161757	-20.186087	2.296819
-84.882473	-14.806540	2.306816
-83.914296	-19.091459	2.316813
-83.624491	-17.213402	2.326810
-83.021383	-13.632333	2.336806
-82.447193	-13.109133	2.346803
-82.242446	-16.599728	2.356800
-81.329196	-16.721543	2.366797
-80.792260	-16.504185	2.376794
-80.700584	-19.273859	2.386790
-80.434860	-18.211109	2.396787
-79.431744	-11.935920	2.406784
-79.139753	-13.995129	2.416781
-78.196997	-18.298122	2.426778
-77.885306	-18.633258	2.436774
-77.825959	-20.569461	2.446771
-77.329506	-18.309887	2.456768
-76.486405	-11.597718	2.466765
-76.444559	-14.121788	2.476762
-75.308307	-11.499682	2.486758
-74.948854	-21.690310	2.496755
-74.560900	-26.271196	2.506752
-74.151585	-16.340136	2.516749
-73.297497	-10.622825	2.526746
-72.975923	-18.903195	2.536742
-72.908918	-15.537918	2.546739
-71.605912	-13.604608	2.556736
-71.766038	-14.339274	2.566733
-71.017047	-15.513368	2.576730
-70.373756	-12.155416	2.586726
-70.299671	-16.008921	2.596723
-69.297015	-17.871655	2.606720
-68.808465	-13.804963	2.616717
-68.704664	-21.222842	2.626714
-68.217135	-19.753075	2.636710
-67.232718	-20.431624	2.646707
-66.826148	-22.257433	2.656704
-66.633231	-22.784626	2.666701
-66.158508	-22.630230	2.676698
-65.318914	-18.809139	2.686694
-65.237495	-21.970463	2.696691
-64.287353	-14.063450	2.706688
-63.722081	-16.831136	2.716685
-63.787611	-16.435924	2.726682
-63.157021	-19.941579	2.736678
-62.583801	-15.293577	2.746675
-62.232090	-19.452807	2.756672
-60.987619	-18.637897	2.766669
-60.577614	-18.948335	2.776666
-60.774002	-17.059566	2.786662
-60.361480	-6.512783	2.796659
-59.284304	-13.717549	2.806656
-59.246410	-13.117420	2.816653
-58.312948	-9.225603	2.826650
-57.536794	-15.424273	2.836646
-57.263219	-14.080109	2.846643
-57.480221	-15.089962	2.856640
-56.812785	-16.022393	2.866637
-56.292353	-13.642611	2.876634
-54.911876	-4.507645	2.886630
-54.818243	-10.220227	2.896627
-54.367236	-11.396784	2.906624
-54.163410	-13.440386	2.916621
-53.613439	-11.151721	2.926618
-53.025639	-13.871121	2.936614
-52.648754	-15.637745	2.946611
-51.359645	-17.284220	2.956608
-51.221101	-16.090952	2.966605
-51.628757	-18.157367	2.976602
-50.727866	-21.302048	2.986598
-49.926130	-22.513997	2.996595
-49.538586	-22.878114	3.006592
-48.510816	-21.139153	3.016589
-48.114765	-17.483362	3.026586
-48.013466	-10.247148	3.036582
-48.043670	-7.890357	3.046579
-47.208029	-14.204356	3.056576
-46.537173	-15.473304	3.066573
-45.457056	-11.050278	3.076570
-45.521086	-14.533102	3.086566
-45.238623	-16.418215	3.096563
-44.172414	-15.469183	3.106560
-43.739361	-13.957911	3.116557
-43.625682	-6.657954	3.126554
-43.057982	-5.023775	3.136550
-42.119566	-20.300691	3.146547
-41.758553	-22.540912	3.156544
-41.568670	-29.588463	3.166541
-41.187643	-19.411452	3.176538
-40.723276	-20.997835	3.186534
-39.823545	-17.830580	3.196531
-38.988323	-14.517877	3.206528
-38.807030	-16.200414	3.216525
-38.946432	-9.150579	3.226522
-37.840475	-11.269381	3.236518
-37.462019	-15.044625	3.246515
-37.220219	-10.799103	3.256512
-36.169328	-18.139938	3.266509
-35.496677	-16.318826	3.276506
-35.541391	-12.711641	3.286502
-35.203200	-10.016163	3.296499
-33.967027	-14.819516	3.306496
-33.898526	-17.523821	3.316493
-33.775465	-17.410038	3.326490
-32.844120	-13.601880	3.336486
-32.564113	-15.879932	3.346483
-32.006745	-16.396627	3.356480
-30.829920	-13.858859	3.366477
-30.662097	-22.870677	3.376474
-30.587807	-21.903765	3.386470
-30.311539	-13.408465	3.396467
-29.319947	-22.384493	3.406464
-28.952782	-29.118820	3.416461
-28.483162	-23.619838	3.426458
-27.889166	-21.238679	3.436454
-27.797258	-20.488538	3.446451
-26.704272	-19.428207	3.456448
-26.470629	-21.938386	3.466445
-25.867019	-14.973955	3.476442
-25.075067	-17.128480	3.486438
-24.507692	-11.714844	3.496435
-24.407123	-16.428317	3.506432
-24.400238	-12.854403	3.516429
-23.411804	-13.801404	3.526426
-22.732942	-16.844986	3.536422
-22.677860	-23.774050	3.546419
-21.579232	-23.874090	3.556416
-21.219090	-22.811827	3.566413
-21.412917	-22.640389	3.576410
-20.397439	-14.773205	3.586406
-19.889880	-16.957286	3.596403
-19.503961	-23.683997	3.606400
-18.388265	-21.222607	3.616397
-18.274474	-25.228968	3.626394
-18.364592	-17.911286	3.636390
-17.199740	-26.114734	3.646387
-16.541375	-18.162407	3.656384
-16.437761	-19.506476	3.666381
-16.085624	-15.550687	3.676378
-15.321845	-20.566185	3.686374
-14.787916	-24.080804	3.696371
-14.441730	-28.010193	3.706368
-13.632398	-27.385182	3.716365
-13.400812	-21.327125	3.726362
-13.099316	-18.152917	3.736358
-12.266146	-16.311803	3.746355
-11.660046	-21.653841	3.756352
-11.697097	-21.052735	3.766349
-10.675827	-22.188695	3.776346
-10.015776	-13.560933	3.786342
-10.037040	-18.377402	3.796339
-9.522279	-17.708451	3.806336
-8.700606	-16.283921	3.816333
-8.643398	-17.813240	3.826330
-8.063960	-16.555575	3.836326
-6.886831	-21.238332	3.846323
-6.864106	-21.563346	3.856320
-6.691079	-18.326666	3.866317
-5.760166	-14.907679	3.876314
-5.437326	-14.380716	3.886310
-4.868146	-6.815039	3.896307
-4.411362	2.922049	3.906304
-4.121533	5.933473	3.916301
-3.721064	13.266952	3.926298
-3.419897	27.495612	3.936294
-2.916491	38.382090	3.946291
-2.183313	53.343657	3.956288
-1.885709	57.661622	3.966285
-1.410209	82.124704	3.976282
-0.678823	94.707952	3.986278
-0.375401	112.546882	3.996275
0.000000	123.521994	4.001280
-0.017491	135.987988	4.006285
0.451171	141.204948	4.011290
0.504860	150.970335	4.016294
0.457692	150.092463	4.021299
0.622568	147.523418	4.026304
0.380290	161.871735	4.031309
0.620629	175.602340	4.036314
0.942756	175.340117	4.041318
0.998371	184.737716	4.046323
1.391971	182.290196	4.051328
1.158925	185.197089	4.056333
1.070813	189.002758	4.061338
1.283998	185.248859	4.066342
0.823767	185.386242	4.071347
1.036094	178.153489	4.076352
1.045334	181.344426	4.081357
0.864566	177.691838	4.086362
1.141953	179.579417	4.091366
0.871517	193.256033	4.096371
1.179939	190.501069	4.101376
1.049228	195.760271	4.106381
0.888258	186.645290	4.111386
1.358366	180.114688	4.116390
1.310210	182.327368	4.121395
1.338819	185.803476	4.126400
1.237895	181.618665	4.131405
1.393003	180.148281	4.136410
1.190098	170.206992	4.141414
0.840381	163.489275	4.146419
1.203466	169.676902	4.151424
1.213736	185.326604	4.156429
0.824249	188.523255	4.161434
1.225617	187.686782	4.166438
1.165601	185.883765	4.171443
1.319278	178.297454	4.176448
1.297833	199.304091	4.181453
1.387778	194.922683	4.186458
1.493628	188.746564	4.191462
1.297818	185.897743	4.196467
1.342811	198.644200	4.201472
1.205050	195.786376	4.206477
1.363291	194.029568	4.211482
1.401389	188.864720	4.216486
1.203455	197.201551	4.221491
1.523983	196.495937	4.226496
1.449435	183.572075	4.231501
1.276133	197.920669	4.236506
1.248629	192.421069	4.241510
1.188833	193.788320	4.246515
1.341325	193.733487	4.251520
1.569837	194.479409	4.256525
1.624014	184.389078	4.261530
1.647401	191.635885	4.266534
1.313572	202.902860	4.271539
1.623027	193.166342	4.276544
1.670651	200.970401	4.281549
1.449959	201.727812	4.286554
1.837844	189.459848	4.291558
1.759128	208.341840	4.296563
1.748443	197.113471	4.301568
1.720590	201.701194	4.306573
1.396173	206.356279	4.311578
1.587086	200.979516	4.316582
1.210231	205.428196	4.321587
1.600593	195.779132	4.326592
1.190820	196.572526	4.331597
1.321745	205.934310	4.336602
1.560662	210.032519	4.341606
1.955161	214.508324	4.346611
1.866067	210.560199	4.351616
1.733942	210.313752	4.356621
1.773962	211.477852	4.361626
1.719512	206.337664	4.366630
1.533617	215.549665	4.371635
2.023892	216.066562	4.376640
2.074801	228.134004	4.381645
2.055653	219.850814	4.386650
2.339940	208.739037	4.391654
1.768449	207.296976	4.396659
1.472889	206.782063	4.401664
1.718081	214.119196	4.406669
1.573487	206.956067	4.411674
1.797325	199.170902	4.416678
1.619234	207.074616	4.421683
1.987237	215.371501	4.426688
2.335935	229.660300	4.431693
1.911294	224.938122	4.436698
1.971561	214.543300	4.441702
1.775827	212.534516	4.446707
1.999005	223.274680	4.451712
2.192933	231.494583	4.456717
2.144091	227.416185	4.461722
1.847710	213.806696	4.466726
2.141548	210.528006	4.471731
1.744996	214.547436	4.476736
1.985578	221.859289	4.481741
1.537494	225.256234	4.486746
1.835258	227.180703	4.491750
2.029084	234.598649	4.496755
2.041118	240.248041	4.501760
2.078512	238.061525	4.506765
2.053005	235.907305	4.511770
2.053663	234.257926	4.516774
1.961271	230.526594	4.521779
2.014832	221.051067	4.526784
2.232572	229.834898	4.531789
1.925137	224.369807	4.536794
2.227657	215.902348	4.541798
2.342214	236.682739	4.546803
2.167766	230.462260	4.551808
2.093454	230.244142	4.556813
1.831223	232.761933	4.561818
2.272407	234.372652	4.566822
2.046198	231.062203	4.571827
2.205165	242.865060	4.576832
2.396165	263.487435	4.581837
2.405765	260.397772	4.586842
2.439238	252.999497	4.591846
2.428926	254.270377	4.596851
2.254297	246.092483	4.601856
2.508015	245.611499	4.606861
2.142611	249.911794	4.611866
2.484988	257.209703	4.616870
2.163629	271.247500	4.621875
2.182883	262.133668	4.626880
2.745509	264.552837	4.631885
2.609285	271.791036	4.636890
2.868511	258.503059	4.641894
2.308524	248.868653	4.646899
2.329495	242.569605	4.651904
2.294215	246.938961	4.656909
2.327926	257.662907	4.661914
2.603330	249.176135	4.666918
2.075991	268.142303	4.671923
2.419636	264.596201	4.676928
2.541749	262.458524	4.681933
2.428193	265.620640	4.686938
2.584713	254.366176	4.691942
2.303772	256.872362	4.696947
2.586233	265.414761	4.701952
2.484788	262.973665	4.706957
2.230963	264.861039	4.711962
2.481518	263.117677	4.716966
2.330887	262.551089	4.721971
2.813858	257.888261	4.726976
2.345550	258.466888	4.731981
2.561151	284.830967	4.736986
2.972074	279.721286	4.741990
2.472376	279.426862	4.746995
2.553098	288.064272	4.752000
2.944086	296.590430	4.757005
2.758059	285.608214	4.762010
2.896026	296.728329	4.767014
2.965046	296.013071	4.772019
2.764442	282.262794	4.777024
2.819830	269.064532	4.782029
2.770016	265.502355	4.787034
2.937314	263.727173	4.792038
2.757486	264.063774	4.797043
2.693005	271.574049	4.802048
2.924859	269.489072	4.807053
2.775164	282.799136	4.812058
3.016640	289.713880	4.817062
2.948864	288.515516	4.822067
2.939658	291.932389	4.827072
3.161223	282.815892	4.832077
2.761269	277.965311	4.837082
3.019696	273.855656	4.842086
2.972057	294.082632	4.847091
2.866595	287.211829	4.852096
2.568369	287.229309	4.857101
2.755295	297.138120	4.862106
3.050164	292.936903	4.867110
3.101730	285.209859	4.872115
3.077779	293.124943	4.877120
3.234851	289.638081	4.882125
3.020933	298.928064	4.887130
3.038111	294.552733	4.892134
2.884446	293.802749	4.897139
3.009393	292.788693	4.902144
3.312257	297.821980	4.907149
2.924850	288.619064	4.912154
2.982455	273.653494	4.917158
2.927486	298.615416	4.922163
3.120997	292.491757	4.927168
3.322940	289.526575	4.932173
3.290006	283.012270	4.937178
3.323735	286.060175	4.942182
3.192098	289.214728	4.947187
3.284594	283.200404	4.952192
3.284270	284.313265	4.957197
3.115235	299.203760	4.962202
3.160740	291.420000	4.967206
3.030661	293.169922	4.972211
3.259696	295.676090	4.977216
3.353967	298.442292	4.982221
2.956114	306.340938	4.987226
2.984870	304.178629	4.992230
3.244459	297.671719	4.997235
3.188163	291.504498	5.002240
3.363530	291.842483	5.007245
3.320322	316.827649	5.012250
3.798660	319.506115	5.017254
3.347438	309.805749	5.022259
3.385240	299.354598	5.027264
3.307052	298.635649	5.032269
3.423121	289.087498	5.037274
3.484522	290.038130	5.042278
3.313782	304.006177	5.047283
3.799301	306.001836	5.052288
3.695415	300.565431	5.057293
3.644558	306.549919	5.062298
3.897126	303.990035	5.067302
3.382134	303.923962	5.072307
3.218803	309.852158	5.077312
3.485726	298.287393	5.082317
3.518674	305.069086	5.087322
3.818468	301.054599	5.092326
3.547092	299.899154	5.097331
3.549196	295.101499	5.102336
3.703791	294.094283	5.107341
3.580657	298.703405	5.112346
3.497488	287.050787	5.117350
3.676852	298.221480	5.122355
3.471828	292.124515	5.127360
4.064338	284.639464	5.132365
3.342327	293.301308	5.137370
3.614399	295.602953	5.142374
4.020992	327.965529	5.147379
3.518206	300.481359	5.152384
3.821776	311.775574	5.157389
3.714563	322.534102	5.162394
3.885140	311.649898	5.167398
3.575739	304.698349	5.172403
3.836996	323.385786	5.177408
3.778006	319.707120	5.182413
3.895428	324.358776	5.187418
3.882714	327.356649	5.192422
3.780559	331.088413	5.197427
3.960452	316.923120	5.202432
3.896318	306.380879	5.207437
3.646447	320.755263	5.212442
4.074870	319.723117	5.217446
4.011159	333.712966	5.222451
3.820419	319.354090	5.227456
4.087082	324.117131	5.232461
3.638107	329.492015	5.237466
3.975353	333.097299	5.242470
4.191974	327.330595	5.247475
3.943580	323.215102	5.252480
4.055956	323.405647	5.257485
3.561388	332.539784	5.262490
3.778531	333.310284	5.267494
3.864882	333.738650	5.272499
3.863427	332.104507	5.277504
4.282774	330.804921	5.282509
4.180750	322.227958	5.287514
4.197948	325.788164	5.292518
4.120421	338.087944	5.297523
3.654504	330.896269	5.302528
4.112821	321.851021	5.307533
3.932139	333.994801	5.312538
4.165424	318.910180	5.317542
3.946360	339.183006	5.322547
3.764337	336.788955	5.327552
3.938294	338.946602	5.332557
3.495074	334.327300	5.337562
4.214063	343.916371	5.342566
4.178843	364.127673	5.347571
4.405017	353.445970	5.352576
4.568458	351.781319	5.357581
4.289830	353.007461	5.362586
3.954654	341.136191	5.367590
3.879158	351.314624	5.372595
4.198067	360.081318	5.377600
4.260455	366.228643	5.382605
4.372872	365.717829	5.387610
4.646607	356.899589	5.392614
4.291303	368.512968	5.397619
4.234198	375.680228	5.402624
4.059320	369.788785	5.407629
4.193972	368.408483	5.412634
4.422330	361.747376	5.417638
4.084834	367.091815	5.422643
4.246011	367.264035	5.427648
4.278089	362.298720	5.432653
4.037680	381.135823	5.437658
4.497758	371.336318	5.442662
4.411268	365.988273	5.447667
4.299746	364.474327	5.452672
4.761779	371.151203	5.457677
4.315613	366.532082	5.462682
4.377609	353.516551	5.467686
4.422611	377.722352	5.472691
4.601753	387.319173	5.477696
5.019185	374.267183	5.482701
4.450290	368.878003	5.487706
4.627229	357.596115	5.492710
4.509347	364.124350	5.497715
4.580159	365.474472	5.502720
4.548131	364.277889	5.507725
4.420565	365.723737	5.512730
4.459239	381.991669	5.517734
4.526651	390.405609	5.522739
4.569966	409.200594	5.527744
4.899859	397.503803	5.532749
4.892663	397.556849	5.537754
4.893246	397.614924	5.542758
4.926736	387.006378	5.547763
4.213062	383.348576	5.552768
4.935885	390.638531	5.557773
4.610161	396.944027	5.562778
4.679430	389.161125	5.567782
4.910270	397.220618	5.572787
4.689789	402.112134	5.577792
4.793206	398.671012	5.582797
4.600390	406.892273	5.587802
4.917864	399.354849	5.592806
4.946269	400.592409	5.597811
4.720608	408.871980	5.602816
4.660469	402.154842	5.607821
4.963122	404.008282	5.612826
4.800667	404.465139	5.617830
4.945067	416.995372	5.622835
4.895218	405.201209	5.627840
5.361096	392.034352	5.632845
4.831662	410.655149	5.637850
5.017434	406.384718	5.642854
4.807837	404.025106	5.647859
4.878522	403.018825	5.652864
4.975232	393.169649	5.657869
4.967779	402.215929	5.662874
5.131697	388.997260	5.667878
4.977038	406.000591	5.672883
4.663046	403.771490	5.677888
4.627774	394.107598	5.682893
4.502474	404.548142	5.687898
4.788357	395.166513	5.692902
5.096259	410.416434	5.697907
4.929290	417.075533	5.702912
5.019532	416.708871	5.707917
4.775589	426.558840	5.712922
5.133423	429.246092	5.717926
5.007248	426.034399	5.722931
5.198057	425.920649	5.727936
5.325670	423.100122	5.732941
5.256714	431.015907	5.737946
5.062932	436.240232	5.742950
5.042192	427.180661	5.747955
5.164584	429.722037	5.752960
5.285041	424.679055	5.757965
4.805642	424.844370	5.762970
5.098054	428.513517	5.767974
5.362812	432.661581	5.772979
5.063846	433.792531	5.777984
4.926265	428.106817	5.782989
4.809975	443.375076	5.787994
5.368711	444.055588	5.792998
5.615307	461.382565	5.798003
5.309532	457.852679	5.803008
5.372663	439.614255	5.808013
5.269254	456.715525	5.813018
5.678801	461.029190	5.818022
5.497263	447.063106	5.823027
5.109390	441.106499	5.828032
5.494291	450.580960	5.833037
5.632498	460.067583	5.838042
5.417264	441.075342	5.843046
5.716989	440.675836	5.848051
5.298733	439.012397	5.853056
5.412164	426.452783	5.858061
5.435896	437.956319	5.863066
5.248277	451.687453	5.868070
5.696555	469.967093	5.873075
5.226441	467.215739	5.878080
5.621658	461.696304	5.883085
5.525939	471.605765	5.888090
5.587254	458.031659	5.893094
5.317184	470.823798	5.898099
5.363717	472.316556	5.903104
5.754442	469.143150	5.908109
5.165756	475.891598	5.913114
5.559154	467.710383	5.918118
5.264870	470.669575	5.923123
5.163543	474.100528	5.928128
5.514622	472.046038	5.933133
5.731815	474.656107	5.938138
5.769314	476.135756	5.943142
5.965014	471.481663	5.948147
5.361150	480.832251	5.953152
5.817832	479.051743	5.958157
5.742099	488.950907	5.963162
5.868212	479.162326	5.968166
6.265025	489.071402	5.973171
5.669494	486.431831	5.978176
6.016138	468.475742	5.983181
5.672316	472.884509	5.988186
5.977556	476.239691	5.993190
6.041902	474.641620	5.998195
5.729815	476.213274	6.003200
6.053489	463.109025	6.008205
5.805303	483.210157	6.013210
6.007997	459.673518	6.018214
5.836235	468.815064	6.023219
5.829513	478.027999	6.028224
5.947028	453.864467	6.033229
5.795394	473.612321	6.038234
5.865499	488.461407	6.043238
6.017023	472.035083	6.048243
5.639414	472.193147	6.053248
6.047323	469.112303	6.058253
5.959327	475.923036	6.063258
5.989780	467.049338	6.068262
5.750378	463.006414	6.073267
5.718304	472.715047	6.078272
6.119526	456.187098	6.083277
6.048004	465.758107	6.088282
6.112666	474.835231	6.093286
5.841270	474.021723	6.098291
5.895172	470.722547	6.103296
5.799780	475.675398	6.108301
5.775648	462.834327	6.113306
6.037714	458.634145	6.118310
5.960033	460.650286	6.123315
6.064915	464.230860	6.128320
6.341937	467.324526	6.133325
5.702230	453.550469	6.138330
5.824458	464.944023	6.143334
5.863509	463.433400	6.148339
5.854816	461.932048	6.153344
5.810357	452.805447	6.158349
6.192847	467.846180	6.163354
6.058593	448.833937	6.168358
5.794261	427.120468	6.173363
5.613923	440.652383	6.178368
5.979278	439.274893	6.183373
5.745733	441.972467	6.188378
5.860595	452.417454	6.193382
6.156691	447.321465	6.198387
5.727537	441.774103	6.203392
5.731929	437.972959	6.208397
5.847562	442.469758	6.213402
5.870031	440.273741	6.218406
5.639644	450.614674	6.223411
6.044283	461.410554	6.228416
5.907349	457.929127	6.233421
5.750113	440.280785	6.238426
5.666751	447.718892	6.243430
5.936601	457.535966	6.248435
5.743226	464.371607	6.253440
6.029281	468.435458	6.258445
5.847546	469.106630	6.263450
5.777741	462.376857	6.268454
5.792390	466.613025	6.273459
5.576008	474.852226	6.278464
6.149552	462.658632	6.283469
5.930716	471.427634	6.288474
6.023446	465.698222	6.293478
5.921173	454.630616	6.298483
5.488352	446.355781	6.303488
6.061055	448.818402	6.308493
5.814672	461.726982	6.313498
5.679718	463.212733	6.318502
5.626836	470.353196	6.323507
6.014349	462.168812	6.328512
6.320263	468.963874	6.333517
5.794160	453.536484	6.338522
5.612704	439.127521	6.343526
5.860974	449.457820	6.348531
5.871437	459.399153	6.353536
6.099728	455.710075	6.358541
5.627866	439.355333	6.363546
5.719790	447.591518	6.368550
5.782648	457.806944	6.373555
5.458072	453.449568	6.378560
5.724604	455.228380	6.383565
5.631977	466.507087	6.388570
5.627537	465.253354	6.393574
5.878225	459.174047	6.398579
5.541447	462.788243	6.403584
5.841324	456.742343	6.408589
5.652167	466.747845	6.413594
5.536584	468.837042	6.418598
5.834734	470.823830	6.423603
5.744866	480.471577	6.428608
5.653777	469.027213	6.433613
5.480926	470.258476	6.438618
5.878587	487.484650	6.443622
6.066496	481.889168	6.448627
5.798203	476.693069	6.453632
5.797377	477.610291	6.458637
5.869988	472.730783	6.463642
5.710518	478.542483	6.468646
6.197498	478.652971	6.473651
6.006795	481.759313	6.478656
5.838615	473.045902	6.483661
5.789383	471.786942	6.488666
5.845153	465.020926	6.493670
5.923624	474.204094	6.498675
5.836601	472.212827	6.503680
5.807313	463.359363	6.508685
5.770509	466.532415	6.513690
5.855085	474.113361	6.518694
5.980083	469.837071	6.523699
6.097277	463.685408	6.528704
5.920171	472.000990	6.533709
6.008023	453.587392	6.538714
5.896458	463.607002	6.543718
5.795289	466.798387	6.548723
5.928274	459.344302	6.553728
6.242568	451.210895	6.558733
6.196338	456.555968	6.563738
5.835233	447.002618	6.568742
5.932251	457.717525	6.573747
5.592292	463.283397	6.578752
6.166662	452.706967	6.583757
5.867480	470.732963	6.588762
5.820507	465.096094	6.593766
6.110613	456.967371	6.598771
5.501869	469.569524	6.603776
5.874766	458.676250	6.608781
5.603158	461.689013	6.613786
5.837304	467.610483	6.618790
6.011462	450.985001	6.623795
5.744656	469.027152	6.628800
5.761527	460.657375	6.633805
5.782635	465.303680	6.638810
5.701133	468.966358	6.643814
5.767095	475.435747	6.648819
5.701664	472.910628	6.653824
5.914238	460.215227	6.658829
5.620977	472.137884	6.663834
5.792234	472.972800	6.668838
6.072355	464.040678	6.673843
5.566816	467.165009	6.678848
5.558377	463.685234	6.683853
5.671810	465.143159	6.688858
6.032973	470.754869	6.693862
5.899593	467.625159	6.698867
5.640448	478.840530	6.703872
5.750774	477.994819	6.708877
5.764071	474.402335	6.713882
5.785096	489.371114	6.718886
6.235115	482.711899	6.723891
5.880332	484.608486	6.728896
5.968889	472.136706	6.733901
5.684070	468.400909	6.738906
5.475649	463.622305	6.743910
5.929417	471.992272	6.748915
5.552279	488.324691	6.753920
5.719859	489.314319	6.758925
5.990758	493.717401	6.763930
6.187972	479.758842	6.768934
6.185134	482.132782	6.773939
6.010533	492.387077	6.778944
6.080715	471.113034	6.783949
5.997301	466.520262	6.788954
5.752969	479.826403	6.793958
5.840420	458.198008	6.798963
5.825718	469.623764	6.803968
5.943652	466.173420	6.808973
6.142265	461.566895	6.813978
5.937594	465.125618	6.818982
5.975563	465.893769	6.823987
5.697249	470.463177	6.828992
5.794733	460.397868	6.833997
5.856861	466.302776	6.839002
5.870728	462.803531	6.844006
6.349087	465.142441	6.849011
5.603399	470.469921	6.854016
5.989380	455.685403	6.859021
5.720385	468.121801	6.864026
5.720526	461.520168	6.869030
6.035369	452.555578	6.874035
5.733424	451.826145	6.879040
5.525413	458.533086	6.884045
5.882319	459.124222	6.889050
5.612986	469.524089	6.894054
5.656228	459.114945	6.899059
5.502143	471.105958	6.904064
5.655379	472.480254	6.909069
5.745732	485.009313	6.914074
6.033374	486.349658	6.919078
6.319890	490.671331	6.924083
5.775286	477.784747	6.929088
5.820030	466.373877	6.934093
5.701246	467.257908	6.939098
5.901582	464.819591	6.944102
6.236693	459.241819	6.949107
5.874862	465.444688	6.954112
6.224193	461.261260	6.959117
5.796589	461.331691	6.964122
5.975107	467.097200	6.969126
6.005176	463.584128	6.974131
5.999914	474.727647	6.979136
6.162478	475.032631	6.984141
6.038855	463.491931	6.989146
6.213007	456.436626	6.994150
6.222469	460.566113	6.999155
5.913494	460.290777	7.004160
5.897245	455.898035	7.009165
6.014881	441.747849	7.014170
5.577674	439.479515	7.019174
6.011105	436.603515	7.024179
5.758049	452.613498	7.029184
5.961762	450.156276	7.034189
5.780151	442.673585	7.039194
5.877966	446.127758	7.044198
5.785200	444.233734	7.049203
5.701458	457.663870	7.054208
5.961299	455.561023	7.059213
5.849203	456.190102	7.064218
5.949549	459.631528	7.069222
6.240811	448.160004	7.074227
5.777808	451.519506	7.079232
5.781558	436.581620	7.084237
5.797528	431.487632	7.089242
5.387499	431.377081	7.094246
6.240229	454.700120	7.099251
5.830606	451.425162	7.104256
5.944828	441.489991	7.109261
5.691797	441.211527	7.114266
5.656203	454.339211	7.119270
5.752185	456.109902	7.124275
6.403128	465.893009	7.129280
5.766458	443.694583	7.134285
5.589351	440.221673	7.139290
5.557073	448.963877	7.144294
6.111676	456.227599	7.149299
5.807825	459.659460	7.154304
5.812891	463.759584	7.159309
5.808733	464.307587	7.164314
5.910893	460.223214	7.169318
6.145416	462.067991	7.174323
5.643595	452.547264	7.179328
6.002351	454.477271	7.184333
5.854936	444.573299	7.189338
5.819865	446.393369	7.194342
6.000452	452.847752	7.199347
5.450454	456.102552	7.204352
5.572757	458.777727	7.209357
5.902653	466.197372	7.214362
5.753403	473.411081	7.219366
5.834118	472.822335	7.224371
5.710837	469.048398	7.229376
5.711096	470.552255	7.234381
5.840844	471.188527	7.239386
5.841134	475.832060	7.244390
6.033537	459.285440	7.249395
5.949078	467.747902	7.254400
5.683759	466.648072	7.259405
5.842893	460.361028	7.264410
5.752779	464.008454	7.269414
5.897724	463.604436	7.274419
5.632584	473.706259	7.279424
5.978313	456.180088	7.284429
5.961391	463.005313	7.289434
5.770946	475.918078	7.294438
5.960611	467.023890	7.299443
5.642341	462.988572	7.304448
5.840067	462.911465	7.309453
5.946763	461.512590	7.314458
5.726492	471.181980	7.319462
5.901508	466.003292	7.324467
5.848079	456.446347	7.329472
5.669031	468.342530	7.334477
5.668284	467.865509	7.339482
5.507078	468.340807	7.344486
6.114790	469.381417	7.349491
5.877470	480.346143	7.354496
6.241386	478.283612	7.359501
5.999931	463.011618	7.364506
5.730381	472.465989	7.369510
6.082876	468.906243	7.374515
5.850431	476.310497	7.379520
5.582504	465.462246	7.384525
5.741667	476.336192	7.389530
5.591665	471.624786	7.394534
5.808637	448.760918	7.399539
5.455244	464.802886	7.404544
5.875601	463.891637	7.409549
5.626007	469.876277	7.414554
5.761569	468.713948	7.419558
5.657277	461.341003	7.424563
5.692871	469.849629	7.429568
5.777438	467.246743	7.434573
5.943766	474.593778	7.439578
5.759638	492.274327	7.444582
6.300980	484.263898	7.449587
5.911604	478.669500	7.454592
5.751334	473.583312	7.459597
5.583047	470.448616	7.464602
5.553245	465.243200	7.469606
5.659432	477.041641	7.474611
5.682673	485.466879	7.479616
6.046463	495.382698	7.484621
6.240549	488.077342	7.489626
5.925075	493.186931	7.494630
6.196645	478.412420	7.499635
5.654805	477.269297	7.504640
5.674137	476.959635	7.509645
5.827021	464.527547	7.514650
5.917345	480.924576	7.519654
6.004663	459.178107	7.524659
5.511757	474.388174	7.529664
5.604353	479.376851	7.534669
5.893046	480.717318	7.539674
5.837219	488.495900	7.544678
5.766421	490.917575	7.549683
5.691592	498.171483	7.554688
5.993426	500.950875	7.559693
6.003893	491.768904	7.564698
5.886084	499.459669	7.569702
5.774302	492.282895	7.574707
6.106711	485.381573	7.579712
5.673198	496.315789	7.584717
5.870741	489.187938	7.589722
5.813613	488.104017	7.594726
6.082786	488.431142	7.599731
6.064737	488.041134	7.604736
5.892956	477.135747	7.609741
6.174924	476.239968	7.614746
5.690090	460.737282	7.619750
5.848222	462.340739	7.624755
6.243256	467.934518	7.629760
5.739065	459.456891	7.634765
5.507359	461.916793	7.639770
5.622407	461.564084	7.644774
5.691788	466.677350	7.649779
6.149008	483.201002	7.654784
6.159026	474.698768	7.659789
5.975793	471.584695	7.664794
5.568110	462.183861	7.669798
5.709410	471.127956	7.674803
5.663941	472.453006	7.679808
5.754485	475.770070	7.684813
6.139520	489.503485	7.689818
5.657008	481.636406	7.694822
6.000876	470.118485	7.699827
5.538700	483.377264	7.704832
5.877864	494.917507	7.709837
6.354874	487.512910	7.714842
5.768306	492.641352	7.719846
5.947766	480.409278	7.724851
5.784780	471.154760	7.729856
5.549672	471.760168	7.734861
6.157760	463.627038	7.739866
5.771143	462.455996	7.744870
5.940903	466.196822	7.749875
5.713093	460.204186	7.754880
5.887168	469.834651	7.759885
5.739439	458.492787	7.764890
5.999341	463.944631	7.769894
6.205555	463.434889	7.774899
6.033420	468.360858	7.779904
5.650139	472.013325	7.784909
5.907411	466.155302	7.789914
5.777478	469.275277	7.794918
6.094867	463.780739	7.799923
5.856900	465.530652	7.804928
5.854114	468.143627	7.809933
5.895562	468.418606	7.814938
5.864079	475.637618	7.819942
6.070030	469.790738	7.824947
5.859322	469.431878	7.829952
5.852604	475.134376	7.834957
6.067819	468.953391	7.839962
5.430170	466.720742	7.844966
5.900530	464.927123	7.849971
5.728195	470.156499	7.854976
5.621881	469.352707	7.859981
6.012732	469.176399	7.864986
5.635779	469.614246	7.869990
5.781356	453.595493	7.874995
5.729953	465.504715	7.880000
5.653172	460.421901	7.885005
5.874016	468.653367	7.890010
5.884137	475.607612	7.895014
6.007142	464.155792	7.900019
5.715350	475.446306	7.905024
5.761447	453.701330	7.910029
6.284808	463.693757	7.915034
5.847815	463.331547	7.920038
5.693455	459.807617	7.925043
5.784562	465.457935	7.930048
5.978202	462.968634	7.935053
6.009358	465.137764	7.940058
5.706875	477.331579	7.945062
5.778737	462.751884	7.950067
5.417659	475.462481	7.955072
5.705214	474.384840	7.960077
6.053182	484.375584	7.965082
5.786397	492.508089	7.970086
5.722180	489.419332	7.975091
6.159459	487.086981	7.980096
5.721216	490.530403	7.985101
5.839264	487.545602	7.990106
5.997123	493.066214	7.995110
6.060219	488.264930	8.000115
5.995410	468.140861	8.005133
5.648276	471.892349	8.010150
5.966541	461.948939	8.015168
5.816025	464.963741	8.020186
6.033585	463.628892	8.025203
6.110161	465.819509	8.030221
5.617924	460.903668	8.035238
5.839736	462.342670	8.040256
5.850787	471.960970	8.045274
5.913971	460.118559	8.050291
6.018811	471.609276	8.055309
6.164725	467.906319	8.060326
6.111385	474.017446	8.065344
6.065436	477.511034	8.070362
6.153489	467.717060	8.075379
6.214678	469.701600	8.080397
5.765095	466.902800	8.085414
6.007406	471.291086	8.090432
6.075115	474.203205	8.095450
6.042845	475.724249	8.100467
6.289138	470.901178	8.105485
6.149489	462.852278	8.110502
6.163627	463.344788	8.115520
5.885697	470.619088	8.120538
5.732258	459.311492	8.125555
6.090289	465.078213	8.130573
5.733612	472.163892	8.135590
6.075053	461.113818	8.140608
5.755597	480.455318	8.145626
6.161012	466.870061	8.150643
6.030644	465.419810	8.155661
5.800631	473.194852	8.160678
6.145687	465.248196	8.165696
5.978056	470.993246	8.170714
5.905014	454.197063	8.175731
5.776973	456.847393	8.180749
5.740232	469.909725	8.185766
6.131072	459.021140	8.190784
6.093788	465.596251	8.195802
5.874073	463.170703	8.200819
5.573893	460.298209	8.205837
5.636466	462.411332	8.210854
5.841380	472.290549	8.215872
6.100980	494.025061	8.220890
6.142876	494.095841	8.225907
6.125219	494.769655	8.230925
5.928184	497.708309	8.235942
6.222435	488.236772	8.240960
5.946666	483.974387	8.245978
5.989042	493.170773	8.250995
6.203914	493.682661	8.256013
6.017668	485.043140	8.261030
6.303623	486.233402	8.266048
6.068317	493.764102	8.271066
6.125876	485.675612	8.276083
6.247475	489.573124	8.281101
6.103488	499.540522	8.286118
6.261000	491.930987	8.291136
6.043546	493.707296	8.296154
6.177172	494.319995	8.301171
6.334289	497.479399	8.306189
6.178172	491.499930	8.311206
6.255619	491.417620	8.316224
6.162341	480.808689	8.321242
6.316770	490.583488	8.326259
6.481822	484.900091	8.331277
6.212862	488.753012	8.336294
6.340377	477.967072	8.341312
6.187647	472.575716	8.346330
6.085469	469.730428	8.351347
6.199753	464.052575	8.356365
5.970608	483.541918	8.361382
6.194213	489.256368	8.366400
6.307834	486.172502	8.371418
6.277104	493.306079	8.376435
6.518234	489.631074	8.381453
6.008389	487.872344	8.386470
6.123176	486.517771	8.391488
6.344683	487.147240	8.396506
6.162981	495.459184	8.401523
6.504064	480.186550	8.406541
5.955856	491.104133	8.411558
6.359024	479.336108	8.416576
6.165379	484.449070	8.421594
6.145465	499.030790	8.426611
6.210278	477.091239	8.431629
6.151217	490.281072	8.436646
6.493634	482.521618	8.441664
6.346461	488.733674	8.446682
6.344657	497.807271	8.451699
6.447352	488.393369	8.456717
6.352759	494.397171	8.461734
6.330281	495.064991	8.466752
6.608020	488.682296	8.471770
6.633851	489.892223	8.476787
6.387176	480.956845	8.481805
6.093166	495.433198	8.486822
6.304897	487.991442	8.491840
6.643192	496.331310	8.496858
6.366271	480.145746	8.501875
6.506971	481.164873	8.506893
6.174403	484.773334	8.511910
6.204664	482.767211	8.516928
6.350801	488.897042	8.521946
6.371000	485.291318	8.526963
6.747600	474.684745	8.531981
6.768647	488.865079	8.536998
6.468323	473.494944	8.542016
6.183583	464.072163	8.547034
6.027932	478.043939	8.552051
6.528837	476.151734	8.557069
6.401978	492.267459	8.562087
6.458825	497.018619	8.567104
6.529303	487.154914	8.572122
6.721351	493.963838	8.577139
6.761603	484.764547	8.582157
6.441856	477.211256	8.587175
6.386388	474.787298	8.592192
6.563328	467.618178	8.597210
6.331999	462.764908	8.602227
6.652731	464.660404	8.607245
6.289936	485.463708	8.612263
6.450859	489.848719	8.617280
6.552562	486.388648	8.622298
6.420331	483.309198	8.627315
6.914439	484.089052	8.632333
6.561158	486.979129	8.637351
6.540587	474.906009	8.642368
6.474303	470.116979	8.647386
6.227659	472.578685	8.652403
6.816139	485.152843	8.657421
6.665755	477.477388	8.662439
6.739339	482.613892	8.667456
6.651714	478.377393	8.672474
6.593145	473.976480	8.677491
6.461974	468.019763	8.682509
6.345712	467.126027	8.687527
6.591631	475.265739	8.692544
6.602082	478.165475	8.697562
6.464543	486.625893	8.702579
6.744874	485.533376	8.707597
6.661659	490.824411	8.712615
6.522272	485.556804	8.717632
6.390620	487.639934	8.722650
6.511231	492.717104	8.727667
6.624505	487.616561	8.732685
6.479260	495.039187	8.737703
6.543822	489.371904	8.742720
6.864963	492.872732	8.747738
6.378942	505.232621	8.752755
6.284059	486.885096	8.757773
6.507046	493.218329	8.762791
6.572748	484.552327	8.767808
6.681544	485.283870	8.772826
6.011916	495.829079	8.777843
6.573904	491.649956	8.782861
6.213460	493.316850	8.787879
6.435599	506.974694	8.792896
6.303695	512.936450	8.797914
6.497795	528.394662	8.802931
6.561559	523.936616	8.807949
6.772305	524.981073	8.812967
6.969306	530.959433	8.817984
6.905528	532.544733	8.823002
6.685415	525.635455	8.828019
6.747010	536.541650	8.833037
6.698058	530.918007	8.838055
6.694338	519.374740	8.843072
6.910664	518.321926	8.848090
6.685073	530.517955	8.853107
7.091029	519.931396	8.858125
6.922129	531.411697	8.863143
6.645565	526.761809	8.868160
6.841225	523.966780	8.873178
6.599163	537.282743	8.878195
6.758895	534.891014	8.883213
6.858326	537.416875	8.888231
7.196079	537.043760	8.893248
7.150235	528.936713	8.898266
6.627460	531.827353	8.903283
6.604905	523.078296	8.908301
6.933832	521.456192	8.913319
6.570439	530.451598	8.918336
6.755598	524.495624	8.923354
6.500525	530.191379	8.928371
6.811750	522.655718	8.933389
6.884103	530.292748	8.938407
6.698835	531.293221	8.943424
6.780758	526.654352	8.948442
6.508464	528.249410	8.953459
6.985285	509.453708	8.958477
6.809894	525.683177	8.963495
6.603680	524.730400	8.968512
6.988965	522.580185	8.973530
7.019156	547.695643	8.978547
6.653375	539.966301	8.983565
6.794132	552.977525	8.988583
7.181456	552.504405	8.993600
7.060905	559.062220	8.998618
7.023820	563.110360	9.003635
6.639538	536.692359	9.008653
6.729253	545.674497	9.013671
6.792229	561.479252	9.018688
7.198130	545.891568	9.023706
7.030763	557.590589	9.028723
7.253240	553.892672	9.033741
7.243094	567.659120	9.038759
6.827027	546.174262	9.043776
7.278454	557.593695	9.048794
6.871114	559.753687	9.053811
7.031987	555.953176	9.058829
7.250540	550.255010	9.063847
6.766650	545.399758	9.068864
7.280107	540.383331	9.073882
7.064267	541.937866	9.078899
6.864565	524.761039	9.083917
6.791789	538.389513	9.088935
7.139751	550.835984	9.093952
7.592597	548.663185	9.098970
7.222977	536.896470	9.103987
7.116096	526.873010	9.109005
7.160861	529.589265	9.114023
6.738383	526.717189	9.119040
7.095941	521.763631	9.124058
6.941934	537.376310	9.129075
6.859556	549.343509	9.134093
7.234109	551.693813	9.139111
6.977269	562.926613	9.144128
7.260942	556.453852	9.149146
7.127614	554.720179	9.154163
7.191848	570.844458	9.159181
7.238536	563.018108	9.164199
7.157377	565.194460	9.169216
7.233300	558.523199	9.174234
6.907929	559.807309	9.179251
7.148592	562.243803	9.184269
7.384142	558.126382	9.189287
6.909765	561.106649	9.194304
7.017886	549.193075	9.199322
6.916695	559.153833	9.204339
7.163262	559.319605	9.209357
7.180087	552.562659	9.214375
6.979481	557.732001	9.219392
7.127109	552.386927	9.224410
6.948853	557.065365	9.229427
6.965298	566.458761	9.234445
7.062140	566.866361	9.239463
6.936680	563.063668	9.244480
7.384970	572.243308	9.249498
7.440291	587.887968	9.254515
7.333420	582.300054	9.259533
7.472714	559.070267	9.264551
7.344150	551.070562	9.269568
7.214279	562.530364	9.274586
6.938737	564.277704	9.279603
6.903137	577.518350	9.284621
7.506743	582.752302	9.289639
7.151382	586.566977	9.294656
7.479514	593.144933	9.299674
7.416627	585.115462	9.304691
7.492086	593.132843	9.309709
7.660984	579.716273	9.314727
7.470425	577.608072	9.319744
7.549058	575.412776	9.324762
7.115784	567.602269	9.329779
7.008390	568.844846	9.334797
7.694148	570.064991	9.339815
7.369694	594.113361	9.344832
7.925392	581.992161	9.349850
7.776880	565.440174	9.354867
7.507851	562.401814	9.359885
7.370248	553.477596	9.364903
7.363866	555.503032	9.369920
7.423320	555.985498	9.374938
7.057431	566.853029	9.379955
7.324010	558.311732	9.384973
7.335809	562.983858	9.389991
7.209722	561.083271	9.395008
7.519208	569.532841	9.400026
7.497080	575.073406	9.405043
7.410850	583.661297	9.410061
7.703542	584.183749	9.415079
7.346230	566.480565	9.420096
7.316698	578.473102	9.425114
7.529998	585.819299	9.430131
7.405892	603.165457	9.435149
7.826849	589.240580	9.440167
7.463375	581.510246	9.445184
7.536576	580.552818	9.450202
7.394137	564.651871	9.455219
7.242303	581.739350	9.460237
7.543760	584.872656	9.465255
7.250045	589.999238	9.470272
7.265574	582.980928	9.475290
7.387783	582.458920	9.480307
7.271633	582.984085	9.485325
7.449018	574.823493	9.490343
7.665037	587.903888	9.495360
7.456772	589.421159	9.500378
7.869362	592.305337	9.505395
7.848971	599.029851	9.510413
7.972295	580.610039	9.515431
7.591337	592.058708	9.520448
7.587614	589.100886	9.525466
7.513772	597.670599	9.530483
7.467547	601.264932	9.535501
7.772519	586.041951	9.540519
7.446276	599.768950	9.545536
7.621682	590.158752	9.550554
7.542045	583.353277	9.555571
7.491686	594.482208	9.560589
7.876678	583.560551	9.565607
7.796817	595.846504	9.570624
7.595656	593.273801	9.575642
7.970511	586.907295	9.580659
7.755051	595.829187	9.585677
7.780290	587.129172	9.590695
7.569576	591.086054	9.595712
7.360267	585.921093	9.600730
7.693823	589.048997	9.605747
7.723249	594.029480	9.610765
7.950577	586.479312	9.615783
8.025344	582.513235	9.620800
8.275393	592.980530	9.625818
8.345828	584.455494	9.630835
8.165085	589.403003	9.635853
8.268348	581.673968	9.640871
7.880613	572.878459	9.645888
7.663766	547.669642	9.650906
7.663631	562.795392	9.655923
7.610008	578.234368	9.660941
8.182112	574.946395	9.665959
8.117232	574.068173	9.670976
7.515663	567.934182	9.675994
7.768834	566.678954	9.681011
7.514665	582.444229	9.686029
8.101001	568.715620	9.691047
8.086128	594.730756	9.696064
7.834080	582.490528	9.701082
7.979704	572.237354	9.706099
7.921470	569.870619	9.711117
8.005970	563.235530	9.716135
7.803433	561.795129	9.721152
7.735977	559.100061	9.726170
8.154232	565.161927	9.731187
7.714437	575.491782	9.736205
7.952730	569.763088	9.741223
8.029722	576.411569	9.746240
8.351279	569.751768	9.751258
7.879521	556.044118	9.756275
7.586213	550.699386	9.761293
7.887282	558.235850	9.766311
7.961569	568.346026	9.771328
7.758687	580.777174	9.776346
7.915276	587.282314	9.781363
7.935385	588.898532	9.786381
8.158367	585.390842	9.791399
8.226565	585.339681	9.796416
8.165105	598.349918	9.801434
8.133712	568.346353	9.806451
7.647365	572.613396	9.811469
7.540147	580.581446	9.816487
7.889896	586.508705	9.821504
7.596865	590.914148	9.826522
7.805677	579.954102	9.831539
7.705621	590.736290	9.836557
7.740572	581.624121	9.841575
7.783068	588.731569	9.846592
7.664854	602.554482	9.851610
8.053970	601.912789	9.856627
8.192488	620.541992	9.861645
8.350030	624.968932	9.866663
8.326617	625.463421	9.871680
8.216603	617.962491	9.876698
8.096718	608.570438	9.881715
8.196903	604.551641	9.886733
7.695161	588.917684	9.891751
8.082164	605.145323	9.896768
8.001456	611.720882	9.901786
8.235733	612.077431	9.906803
8.205100	606.032405	9.911821
8.343725	614.011805	9.916839
8.402927	609.791845	9.921856
8.310787	610.805569	9.926874
8.311793	608.945477	9.931891
8.324659	613.272330	9.936909
8.190515	594.656412	9.941927
8.240703	592.651311	9.946944
8.111451	596.500558	9.951962
8.390341	600.137601	9.956979
8.367062	595.345165	9.961997
8.036077	597.185219	9.967015
8.381415	593.905686	9.972032
8.158476	599.220439	9.977050
8.344929	602.431207	9.982067
8.071060	609.904372	9.987085
8.236242	609.747535	9.992103
8.443089	621.787838	9.997120
8.595835	621.722015	10.002138
8.696827	607.580363	10.007155
8.451366	596.483506	10.012173
8.300700	589.550226	10.017191
8.307719	582.077404	10.022208
8.578936	597.341579	10.027226
8.329066	583.389500	10.032243
7.997936	584.497038	10.037261
7.918716	578.013089	10.042279
8.685295	592.816238	10.047296
8.521783	598.990298	10.052314
8.733769	582.586455	10.057331
8.127635	587.180228	10.062349
8.491541	585.643855	10.067367
8.721513	581.717275	10.072384
8.189132	582.627503	10.077402
8.065173	574.642081	10.082419
8.361543	586.121208	10.087437
8.483451	591.460058	10.092455
8.438450	591.927804	10.097472
8.407243	597.876298	10.102490
8.476773	593.582012	10.107507
8.524268	602.649787	10.112525
8.493905	608.908816	10.117543
8.840439	603.182592	10.122560
8.647409	588.925009	10.127578
8.404501	584.448248	10.132595
8.304998	588.036128	10.137613
8.244882	586.931669	10.142631
8.560829	599.578906	10.147648
8.383442	614.380424	10.152666
8.623172	607.428576	10.157683
8.463171	618.136945	10.162701
8.063517	623.903075	10.167719
8.580331	606.815583	10.172736
8.266836	615.845797	10.177754
8.698349	610.085747	10.182771
8.269123	617.749026	10.187789
8.169335	616.047788	10.192807
8.658865	612.012572	10.197824
8.188656	613.119871	10.202842
8.219140	601.877132	10.207859
8.304678	616.554804	10.212877
8.696323	622.254032	10.217895
8.976313	626.133473	10.222912
8.876091	634.306952	10.227930
8.538971	609.843857	10.232947
8.531863	614.875356	10.237965
8.611657	622.364083	10.242983
8.918214	625.401297	10.248000
8.584692	630.130608	10.253018
8.451383	637.582722	10.258035
8.823116	643.576830	10.263053
8.680116	646.640809	10.268071
9.074491	646.617128	10.273088
8.707169	634.540664	10.278106
8.478265	618.380084	10.283123
8.800437	643.210089	10.288141
8.797961	629.781154	10.293159
9.126054	628.477032	10.298176
8.884360	623.431070	10.303194
8.911972	608.911260	10.308211
8.597912	604.813112	10.313229
8.722492	599.429318	10.318247
8.596046	612.373353	10.323264
8.826529	635.006114	10.328282
8.643200	642.283066	10.333299
8.903328	637.481276	10.338317
8.882474	661.115965	10.343335
8.955598	647.562730	10.348352
8.843806	648.474015	10.353370
8.756214	647.681221	10.358387
9.176974	648.680746	10.363405
8.948709	641.087752	10.368423
8.769762	619.158562	10.373440
8.747580	632.409043	10.378458
8.918885	634.734395	10.383475
9.144423	638.799479	10.388493
8.813730	639.558488	10.393511
8.963646	619.943215	10.398528
8.768453	623.582343	10.403546
8.709400	636.759703	10.408563
9.213056	638.339513	10.413581
8.750875	643.490902	10.418599
9.135464	641.448541	10.423616
8.857732	645.554873	10.428634
9.061376	646.240539	10.433651
9.194905	654.314584	10.438669
9.027342	644.695392	10.443687
9.161625	635.417000	10.448704
8.924042	626.684425	10.453722
8.892700	613.131362	10.458739
8.856500	619.333594	10.463757
8.953625	636.479088	10.468775
8.943355	642.169264	10.473792
8.980511	638.298742	10.478810
9.007082	642.836881	10.483827
8.979786	644.448244	10.488845
9.003261	651.453667	10.493863
9.128439	636.900586	10.498880
9.133789	649.118769	10.503898
9.110934	645.273120	10.508915
8.947938	642.083093	10.513933
8.983967	644.686857	10.518951
9.061933	637.146389	10.523968
9.107080	643.415587	10.528986
9.178180	648.821995	10.534003
9.110006	651.343885	10.539021
8.940660	640.930156	10.544039
9.091084	639.615243	10.549056
9.013687	648.484434	10.554074
9.103735	652.832592	10.559091
9.257434	646.873110	10.564109
8.772398	651.373872	10.569127
9.088840	646.427560	10.574144
9.034218	662.425738	10.579162
9.104506	645.540809	10.584179
9.102644	654.384729	10.589197
9.164947	671.846293	10.594215
9.423431	667.948242	10.599232
9.216106	670.262267	10.604250
9.691087	680.648265	10.609267
9.318513	657.774326	10.614285
9.184611	650.549915	10.619303
9.233631	642.688008	10.624320
9.159346	639.213785	10.629338
9.170954	661.339451	10.634355
9.776625	665.364356	10.639373
9.556687	673.439255	10.644391
9.057744	654.512259	10.649408
9.093298	644.169372	10.654426
9.250388	665.491323	10.659443
9.306631	670.841051	10.664461
9.215926	676.353426	10.669479
9.310558	675.663662	10.674496
9.638987	671.944566	10.679514
9.500321	683.061978	10.684531
9.518070	668.548958	10.689549
9.202310	686.093386	10.694567
9.639186	686.831932	10.699584
9.509668	682.181215	10.704602
9.367497	685.577977	10.709619
9.456375	677.714091	10.714637
9.608747	685.526326	10.719655
9.580213	680.114175	10.724672
9.354092	667.999689	10.729690
9.553728	670.627002	10.734707
9.576894	664.115075	10.739725
9.468445	669.178297	10.744743
9.285495	665.390787	10.749760
9.438537	672.823643	10.754778
9.324925	684.756058	10.759795
9.494726	676.647936	10.764813
9.302617	675.614585	10.769831
9.538496	684.988618	10.774848
9.524603	679.323700	10.779866
9.626293	685.737283	10.784883
9.471317	679.931339	10.789901
9.673858	691.188102	10.794919
9.319144	686.069770	10.799936
9.646680	677.982225	10.804954
9.074354	686.015580	10.809971
9.653422	679.493361	10.814989
9.606621	688.408691	10.820007
9.331536	685.643699	10.825024
9.714297	672.388226	10.830042
9.193805	688.652852	10.835059
9.388621	690.319722	10.840077
9.320290	695.622735	10.845095
9.429753	716.005160	10.850112
9.905817	704.091773	10.855130
9.632121	719.243793	10.860147
9.721393	709.830203	10.865165
9.807085	711.243701	10.870183
9.887474	713.381272	10.875200
9.755807	704.676909	10.880218
9.803437	715.130306	10.885235
9.862812	702.385745	10.890253
9.754593	705.829351	10.895271
9.670594	707.220408	10.900288
9.906051	702.296319	10.905306
9.740905	702.679809	10.910323
10.002000	711.354246	10.915341
9.825876	704.215316	10.920359
9.877629	710.012274	10.925376
10.251961	704.126526	10.930394
9.902400	695.648201	10.935411
9.786503	679.577228	10.940429
9.774918	679.314784	10.945447
9.513542	678.979172	10.950464
9.838346	696.646356	10.955482
9.751905	712.225511	10.960499
9.915737	714.434120	10.965517
9.824145	714.298164	10.970535
9.857394	707.447409	10.975552
10.069266	707.110937	10.980570
9.703727	712.670317	10.985587
9.879261	711.452019	10.990605
10.116209	709.672194	10.995623
9.968848	707.582520	11.000640
9.988745	713.016307	11.005658
10.057674	715.036994	11.010675
10.342709	705.873780	11.015693
10.145726	717.943203	11.020711
9.760935	709.447666	11.025728
10.129629	715.283671	11.030746
9.722474	720.329748	11.035763
9.673215	712.628510	11.040781
9.651275	706.760617	11.045799
9.578071	709.911384	11.050816
9.325117	699.995301	11.055834
9.341787	714.449647	11.060851
10.198493	735.417146	11.065869
10.229195	745.140716	11.070887
9.839883	740.633191	11.075904
10.505779	748.764854	11.080922
10.006378	755.000290	11.085939
10.545910	739.415619	11.090957
10.075490	734.159923	11.095975
9.945795	732.320530	11.100992
10.200133	727.711464	11.106010
10.223704	739.021751	11.111027
10.577023	734.144699	11.116045
10.133836	714.325699	11.121063
9.917160	702.202047	11.126080
10.371549	712.960302	11.131098
10.039925	723.072611	11.136115
10.176314	720.139928	11.141133
10.285355	728.447939	11.146151
10.184653	742.751462	11.151168
10.187903	735.902404	11.156186
10.025705	741.354878	11.161203
10.140046	740.679567	11.166221
10.269704	741.588646	11.171239
9.773310	743.269865	11.176256
10.334157	739.249892	11.181274
10.278052	745.734844	11.186291
9.948302	739.341531	11.191309
10.443054	740.116275	11.196327
10.261143	745.241751	11.201344
10.455577	726.828809	11.206362
10.337390	729.801416	11.211379
10.258979	732.259767	11.216397
10.123159	734.932686	11.221415
10.099184	727.379793	11.226432
10.477951	720.495650	11.231450
9.981310	738.442010	11.236467
10.043575	735.939707	11.241485
10.578943	746.053318	11.246503
10.157794	756.727787	11.251520
10.721908	757.296320	11.256538
10.606871	755.812017	11.261555
10.586205	745.471071	11.266573
10.273770	742.081841	11.271591
10.275651	738.897415	11.276608
10.763445	745.766023	11.281626
10.740657	746.267499	11.286643
10.621649	740.312503	11.291661
10.494595	739.873309	11.296679
10.514041	743.765625	11.301696
10.463086	732.594014	11.306714
10.462773	738.137332	11.311731
10.747881	736.810979	11.316749
10.648721	738.287501	11.321767
10.780441	737.661868	11.326784
10.511777	731.202273	11.331802
10.398349	735.864148	11.336819
10.234646	728.339167	11.341837
10.537802	731.768725	11.346855
10.555148	762.998165	11.351872
10.642626	763.931241	11.356890
10.460258	764.027767	11.361907
10.655445	756.552106	11.366925
10.715978	767.798344	11.371943
10.541487	771.216605	11.376960
10.570177	757.288795	11.381978
10.680339	767.078071	11.386995
10.591722	776.736748	11.392013
10.910871	766.423475	11.397031
10.895446	766.575568	11.402048
10.567107	766.622607	11.407066
10.303849	780.897822	11.412083
10.338290	769.698296	11.417101
10.562546	758.862615	11.422119
10.572410	762.334251	11.427136
10.792822	763.680716	11.432154
10.790635	761.256863	11.437171
10.635705	756.966657	11.442189
10.611123	764.318301	11.447207
10.631817	771.405523	11.452224
10.987666	763.650204	11.457242
10.905609	763.369488	11.462259
10.943680	775.275430	11.467277
11.130018	772.628525	11.472295
10.751704	770.842120	11.477312
10.771268	768.834381	11.482330
10.855984	767.278688	11.487347
10.815656	767.339342	11.492365
10.911971	768.867703	11.497383
10.977881	766.882615	11.502400
11.158024	765.357108	11.507418
11.077911	765.625088	11.512435
10.654004	769.989229	11.517453
11.058313	754.920503	11.522471
10.862480	771.603823	11.527488
11.137161	761.283731	11.532506
10.983034	754.824782	11.537523
10.781292	761.707265	11.542541
10.583724	767.988479	11.547559
10.657777	785.448428	11.552576
10.670254	785.916031	11.557594
11.378359	790.806072	11.562611
11.050481	793.651365	11.567629
11.290847	784.787757	11.572647
11.017140	794.551527	11.577664
11.318086	797.199023	11.582682
11.244869	795.283076	11.587699
10.793376	788.680669	11.592717
11.139891	790.619870	11.597735
11.080402	793.967565	11.602752
11.261810	781.625631	11.607770
11.044670	800.714445	11.612787
10.591301	791.233518	11.617805
11.000922	787.187254	11.622823
11.049135	804.705226	11.627840
10.995212	793.263046	11.632858
11.152890	797.486899	11.637875
11.096254	794.604699	11.642893
11.388300	801.838595	11.647911
10.895289	806.651393	11.652928
11.109609	791.482357	11.657946
11.061950	799.473055	11.662963
10.917749	803.082641	11.667981
11.510770	799.586476	11.672999
10.903381	799.072944	11.678016
10.938871	821.246754	11.683034
11.352973	821.219813	11.688051
11.384388	833.676215	11.693069
11.391965	839.976992	11.698087
11.362823	834.213865	11.703104
11.388719	821.659549	11.708122
11.477963	833.902000	11.713139
10.929432	830.344519	11.718157
11.365093	818.312250	11.723175
11.146183	830.546972	11.728192
11.394509	845.858181	11.733210
11.628616	832.177017	11.738227
11.203403	826.756169	11.743245
11.511208	818.693757	11.748263
11.384887	826.996432	11.753280
11.524180	831.425069	11.758298
11.503569	827.356799	11.763315
11.373176	838.967555	11.768333
11.637190	833.370513	11.773351
11.406106	836.716461	11.778368
11.433092	831.727489	11.783386
11.534878	826.238642	11.788403
11.589808	828.812153	11.793421
11.891000	825.684626	11.798439
11.935320	832.890392	11.803456
11.723235	820.799740	11.808474
11.621032	806.544758	11.813491
11.435796	791.913223	11.818509
11.712071	797.934188	11.823527
11.570793	790.757575	11.828544
11.293516	791.943613	11.833562
11.127521	814.907370	11.838579
11.515606	827.917907	11.843597
11.791399	810.513094	11.848615
11.861340	832.932562	11.853632
11.811736	834.016719	11.858650
12.170669	821.910134	11.863667
11.601388	816.415082	11.868685
11.913178	813.441390	11.873703
11.633689	808.760310	11.878720
11.739921	811.156865	11.883738
11.687135	804.029588	11.888755
11.538824	820.222318	11.893773
11.955546	814.637442	11.898791
11.741455	822.114016	11.903808
11.532191	820.051582	11.908826
12.029045	819.554746	11.913843
11.480968	830.245420	11.918861
11.764266	825.306596	11.923879
11.761464	832.077606	11.928896
11.862226	838.312796	11.933914
12.056831	827.907484	11.938931
11.720284	831.488834	11.943949
11.907865	824.416297	11.948967
12.025755	835.211056	11.953984
11.761930	827.456552	11.959002
11.633711	826.557095	11.964019
11.694311	830.074192	11.969037
11.816037	825.204187	11.974055
11.583285	822.812916	11.979072
11.488654	835.543943	11.984090
11.739642	823.936904	11.989107
11.504421	837.683121	11.994125
11.430213	834.408905	11.999143
11.808753	849.169655	12.004160
11.778825	854.768293	12.009178
12.294578	846.934548	12.014195
11.617585	858.750096	12.019213
11.754133	853.988736	12.024231
12.109093	850.763653	12.029248
11.856804	862.399787	12.034266
12.256568	854.539150	12.039283
11.915470	860.565526	12.044301
12.085071	859.758264	12.049319
12.414132	860.812321	12.054336
12.028472	862.206499	12.059354
12.327749	852.129189	12.064371
11.798491	864.816041	12.069389
12.008306	858.700281	12.074407
12.223666	858.804198	12.079424
12.028643	858.683267	12.084442
11.777844	862.022736	12.089459
11.786094	868.893986	12.094477
11.949303	865.694486	12.099495
12.241543	868.185291	12.104512
12.138755	881.197086	12.109530
12.260292	875.342716	12.114547
12.430754	890.394639	12.119565
12.212003	870.284356	12.124583
12.170592	864.992850	12.129600
12.132031	873.501483	12.134618
12.290717	876.199761	12.139635
12.560813	895.716356	12.144653
12.158901	872.150114	12.149671
12.124459	873.146743	12.154688
12.075418	887.043406	12.159706
12.468278	878.838484	12.164723
12.167849	894.440983	12.169741
12.429924	892.737681	12.174759
12.519847	883.928991	12.179776
12.557794	882.356216	12.184794
12.673290	883.747485	12.189811
12.670335	889.480237	12.194829
12.597249	875.923114	12.199847
12.504176	855.143570	12.204864
12.331756	855.102353	12.209882
12.483350	853.291350	12.214899
12.213205	858.607104	12.219917
12.234129	847.865090	12.224935
12.835682	871.179173	12.229952
12.564776	858.894506	12.234970
12.620694	863.784788	12.239987
12.382348	850.798212	12.245005
12.278116	862.501004	12.250023
12.383878	867.198633	12.255040
12.672475	871.715484	12.260058
12.748628	881.544109	12.265075
12.526825	881.951333	12.270093
12.568811	888.879999	12.275111
12.961200	887.430116	12.280128
12.482758	882.874887	12.285146
12.689964	879.441970	12.290163
12.537787	881.149474	12.295181
12.586543	879.409784	12.300199
12.855258	889.894862	12.305216
12.410441	888.744918	12.310234
12.709790	876.971016	12.315251
12.499720	878.986855	12.320269
12.663562	885.634993	12.325287
12.745209	875.063407	12.330304
12.526280	884.145657	12.335322
12.399385	878.378002	12.340339
12.447664	881.811531	12.345357
12.081774	879.631787	12.350375
12.628498	890.667477	12.355392
12.508642	895.212076	12.360410
12.823217	905.819683	12.365427
13.326790	912.312297	12.370445
12.820839	906.209308	12.375463
13.032608	893.321905	12.380480
12.597583	884.644446	12.385498
12.800051	881.397911	12.390515
13.074814	892.890877	12.395533
12.665741	893.204069	12.400551
13.148416	896.715987	12.405568
12.827688	893.806852	12.410586
12.979041	891.090721	12.415603
12.851548	885.591621	12.420621
13.119823	902.783328	12.425639
12.852060	886.689507	12.430656
12.533253	894.856733	12.435674
12.801923	911.448288	12.440691
13.119499	910.517571	12.445709
12.884256	922.385933	12.450727
13.079918	914.832768	12.455744
13.010839	920.631569	12.460762
13.109860	916.155085	12.465779
12.765258	919.540968	12.470797
13.345580	920.993789	12.475815
13.123799	907.061868	12.480832
13.228263	914.999538	12.485850
13.263411	914.171192	12.490867
12.863020	910.230315	12.495885
12.944420	913.380668	12.500903
12.921108	919.126046	12.505920
13.265509	920.461187	12.510938
13.104387	913.788696	12.515955
13.242183	925.256100	12.520973
13.309163	926.100365	12.525991
13.179669	910.284210	12.531008
13.394674	904.253189	12.536026
13.243346	903.720577	12.541043
13.234738	907.528018	12.546061
13.271371	911.126443	12.551079
13.540400	911.919407	12.556096
13.313948	900.296737	12.561114
13.363508	906.239088	12.566131
13.576133	910.808459	12.571149
12.901109	912.002666	12.576167
13.375746	914.345049	12.581184
12.938096	917.590233	12.586202
12.939112	923.027115	12.591219
13.300383	916.282663	12.596237
13.094509	911.305477	12.601255
13.229050	913.082513	12.606272
13.258629	917.832897	12.611290
13.294207	936.378035	12.616307
13.770360	934.200053	12.621325
13.408464	937.088487	12.626343
13.422322	917.982246	12.631360
13.095872	920.881352	12.636378
13.392426	940.360172	12.641395
13.637821	942.954975	12.646413
13.419789	942.730973	12.651431
13.762920	947.897583	12.656448
13.434814	952.670086	12.661466
13.580233	948.137311	12.666483
13.692027	932.572944	12.671501
13.625073	939.282863	12.676519
13.755639	930.875040	12.681536
13.767173	928.638822	12.686554
13.971639	931.267547	12.691571
13.524795	909.345016	12.696589
13.443122	915.153768	12.701607
13.636691	908.865111	12.706624
13.697378	931.004901	12.711642
13.649225	933.385263	12.716659
13.976840	933.456854	12.721677
13.627622	925.716608	12.726695
13.867008	912.305027	12.731712
13.691977	914.628414	12.736730
13.807891	911.574296	12.741747
13.952448	894.363487	12.746765
13.314759	915.590098	12.751783
13.665472	916.261510	12.756800
13.719207	920.010629	12.761818
13.772277	932.712309	12.766835
14.239455	933.964377	12.771853
13.434715	930.499105	12.776871
13.800247	933.193127	12.781888
13.823343	933.780318	12.786906
13.817592	934.848377	12.791923
14.035311	929.793312	12.796941
13.997127	935.503168	12.801959
14.351956	931.530969	12.806976
14.007855	933.201112	12.811994
14.084148	924.066557	12.817011
13.520992	905.784107	12.822029
13.682808	921.224433	12.827047
13.630756	933.327249	12.832064
13.843585	930.911728	12.837082
13.680308	930.364556	12.842099
14.098762	923.118804	12.847117
13.932544	939.741713	12.852135
14.108797	935.532533	12.857152
13.903108	929.002614	12.862170
13.689907	934.807523	12.867187
14.120698	933.024178	12.872205
13.921268	934.809564	12.877223
14.240011	931.796715	12.882240
14.376661	942.459140	12.887258
14.091274	945.753760	12.892275
14.228660	938.137786	12.897293
13.715306	937.526242	12.902311
14.319912	935.881468	12.907328
14.308056	939.843366	12.912346
13.871169	948.919751	12.917363
14.247420	940.776980	12.922381
14.064555	947.024050	12.927399
14.260030	948.337355	12.932416
14.342771	962.171568	12.937434
14.233200	954.309632	12.942451
14.512073	944.004372	12.947469
14.332398	947.006766	12.952487
14.121890	943.009702	12.957504
14.390956	934.850007	12.962522
14.116916	950.193913	12.967539
14.818693	955.478788	12.972557
14.195436	952.607236	12.977575
14.496054	944.954639	12.982592
14.684371	938.996311	12.987610
14.333961	941.960001	12.992627
14.511594	937.568142	12.997645
14.480725	934.421169	13.002663
14.609105	932.186504	13.007680
14.470075	929.227851	13.012698
14.491889	923.494256	13.017715
14.743868	928.510203	13.022733
14.375517	937.043453	13.027751
14.368761	935.821901	13.032768
14.324301	928.156074	13.037786
14.332469	933.563239	13.042803
14.708722	945.443343	13.047821
14.799207	949.769568	13.052839
14.394298	948.217813	13.057856
14.781623	955.718274	13.062874
14.490062	957.560219	13.067891
14.623668	945.182065	13.072909
14.632018	961.120745	13.077927
14.520171	973.234459	13.082944
14.924235	962.047419	13.087962
14.536638	966.684899	13.092979
14.589180	956.349525	13.097997
14.938316	955.283690	13.103015
14.598921	959.991732	13.108032
14.615469	958.740741	13.113050
14.671460	961.932698	13.118067
14.611688	960.622677	13.123085
14.690950	954.936851	13.128103
14.371920	957.712907	13.133120
14.981077	961.891425	13.138138
14.762879	954.923477	13.143155
14.972505	951.961327	13.148173
14.541428	955.728771	13.153191
14.739119	954.956226	13.158208
14.746679	951.430323	13.163226
14.626830	961.683255	13.168243
14.935520	964.368569	13.173261
14.909573	962.027928	13.178279
14.705342	956.464528	13.183296
14.908531	954.672738	13.188314
14.978316	969.385529	13.193331
14.865761	962.547734	13.198349
14.884063	954.824679	13.203367
14.604163	959.657513	13.208384
15.168101	975.774430	13.213402
14.990660	983.336152	13.218419
15.344795	968.022402	13.223437
15.448024	967.025545	13.228455
15.087737	955.709155	13.233472
15.156112	946.812863	13.238490
14.905749	939.630786	13.243507
15.192890	940.003504	13.248525
15.161340	943.291604	13.253543
15.225801	938.417742	13.258560
15.417358	933.272526	13.263578
15.343197	941.049406	13.268595
15.614728	949.182086	13.273613
15.388624	939.251570	13.278631
15.200358	946.687526	13.283648
15.594999	936.748903	13.288666
15.341939	952.724082	13.293683
15.278827	932.315995	13.298701
15.460900	938.681071	13.303719
15.334720	947.718312	13.308736
15.754449	928.693386	13.313754
15.263473	943.751732	13.318771
15.771059	947.037141	13.323789
15.395618	945.649583	13.328807
15.323607	932.051886	13.333824
15.468126	932.063984	13.338842
15.592444	935.984483	13.343859
15.542510	946.148699	13.348877
15.310578	931.065080	13.353895
15.003253	939.308569	13.358912
15.537667	937.861781	13.363930
14.941231	949.334810	13.368947
15.078263	946.070930	13.373965
15.298710	944.830134	13.378983
15.371508	945.442571	13.384000
15.495212	943.935723	13.389018
15.560045	945.809504	13.394035
15.512268	946.348968	13.399053
15.506552	950.224238	13.404071
15.308178	951.678797	13.409088
15.509292	942.542301	13.414106
15.339623	947.545467	13.419123
15.694525	956.180431	13.424141
15.794024	965.285291	13.429159
15.687734	964.211266	13.434176
15.785872	942.004368	13.439194
15.537120	956.854812	13.444211
15.781671	965.818202	13.449229
16.069371	956.446363	13.454247
15.376053	950.062165	13.459264
15.484031	962.848482	13.464282
15.423991	965.438653	13.469299
15.546502	977.183775	13.474317
15.792335	976.893941	13.479335
15.674877	974.622940	13.484352
15.926335	979.160525	13.489370
15.645596	975.091803	13.494387
15.737233	984.347753	13.499405
15.931767	970.878977	13.504423
15.818576	977.718581	13.509440
16.100863	985.446813	13.514458
15.889789	997.243927	13.519475
15.722823	984.482411	13.524493
16.078161	982.604657	13.529511
15.717561	990.514513	13.534528
15.922835	973.805901	13.539546
16.013813	987.556506	13.544563
15.928086	984.885835	13.549581
16.015267	976.738068	13.554599
15.494581	984.684414	13.559616
15.669201	972.781468	13.564634
16.017832	985.832710	13.569651
16.137611	1000.446930	13.574669
16.391686	996.887364	13.579687
16.055663	994.575129	13.584704
16.050725	982.969521	13.589722
16.311245	997.615589	13.594739
16.332766	991.690513	13.599757
16.148918	983.531241	13.604775
16.046911	968.655999	13.609792
16.166486	974.042209	13.614810
16.447300	991.632863	13.619827
16.153888	994.368675	13.624845
16.266392	992.987275	13.629863
15.893251	1000.191645	13.634880
16.263467	1004.377382	13.639898
16.220306	1010.318563	13.644915
16.579273	1001.672005	13.649933
16.621682	1000.015620	13.654951
16.465955	1006.779209	13.659968
16.485692	999.424142	13.664986
16.129458	988.639847	13.670003
16.246401	991.975453	13.675021
16.650473	995.722002	13.680039
16.637257	998.883482	13.685056
16.475948	992.172018	13.690074
16.629330	983.842468	13.695091
16.216708	988.249286	13.700109
16.792184	981.806164	13.705127
16.260000	981.423677	13.710144
16.159982	983.560100	13.715162
16.418380	993.474607	13.720179
16.495767	1004.616871	13.725197
16.628319	999.878368	13.730215
16.598405	1010.540024	13.735232
16.565904	1000.010636	13.740250
16.635645	1008.116075	13.745267
16.630255	998.465925	13.750285
16.632170	1002.221855	13.755303
16.281612	1006.994149	13.760320
16.587248	1000.325379	13.765338
16.538092	993.734532	13.770355
16.499952	1002.239820	13.775373
16.468866	1003.234131	13.780391
16.302883	993.751248	13.785408
16.464736	1002.146530	13.790426
16.438160	1008.069224	13.795443
16.448420	1031.602899	13.800461
16.994323	1024.198265	13.805479
17.184807	1027.674458	13.810496
17.211232	1023.854522	13.815514
16.830685	1011.762429	13.820531
16.771944	1008.252193	13.825549
17.220001	1007.974996	13.830567
16.760680	1020.517959	13.835584
16.795341	1006.762826	13.840602
17.021609	1009.736921	13.845619
16.744388	1020.359347	13.850637
17.076784	1027.500279	13.855655
16.953076	1030.883142	13.860672
16.913386	1021.393936	13.865690
17.004335	1028.514934	13.870707
16.828975	1022.432451	13.875725
17.462609	1020.051296	13.880743
17.218800	1028.679745	13.885760
17.394710	1012.917723	13.890778
17.002658	996.961038	13.895795
16.684553	995.787586	13.900813
17.201359	993.374569	13.905831
17.000083	1017.341147	13.910848
17.021863	1009.433858	13.915866
17.369322	1019.498204	13.920883
17.036721	1022.487505	13.925901
17.155692	1015.122527	13.930919
17.412211	1019.941526	13.935936
17.462518	1021.893689	13.940954
17.270095	1020.049570	13.945971
17.052748	1037.850729	13.950989
17.388668	1016.449767	13.956007
17.493406	1030.015094	13.961024
17.248572	1031.932384	13.966042
17.288121	1022.848323	13.971059
17.544982	1034.459886	13.976077
17.584826	1018.256047	13.981095
17.289789	1025.673667	13.986112
17.323670	1019.457607	13.991130
17.484267	1020.222834	13.996147
17.242479	1030.874642	14.001165
17.680083	1024.504475	14.006183
17.628308	1033.324976	14.011200
17.533743	1026.878801	14.016218
17.590939	1024.432891	14.021235
17.503388	1030.563473	14.026253
17.523040	1037.959602	14.031271
17.496083	1031.108418	14.036288
17.520178	1026.370312	14.041306
17.654491	1022.141468	14.046323
17.250532	1022.000543	14.051341
17.882457	1016.490448	14.056359
17.734231	1035.407166	14.061376
17.650160	1024.187183	14.066394
17.612051	1015.478697	14.071411
17.796829	1019.656506	14.076429
17.672094	1016.331359	14.081447
17.365140	1016.377718	14.086464
17.400508	1013.946044	14.091482
17.809181	1004.369568	14.096499
17.338557	1009.243186	14.101517
17.300661	1015.152205	14.106535
17.438332	1015.054036	14.111552
17.251422	1035.371412	14.116570
18.250429	1032.463611	14.121587
17.870773	1033.320873	14.126605
18.273964	1039.044823	14.131623
18.197567	1035.267265	14.136640
17.872668	1019.910189	14.141658
17.973754	997.688158	14.146675
17.830282	1016.076790	14.151693
18.054564	1005.217413	14.156711
18.041713	1005.600541	14.161728
17.705617	1016.743832	14.166746
17.896122	1008.746663	14.171763
17.711475	1025.951161	14.176781
18.016697	1035.171059	14.181799
18.097604	1032.716702	14.186816
18.201094	1047.219503	14.191834
18.356052	1045.405756	14.196851
18.142278	1042.852283	14.201869
18.243253	1041.776870	14.206887
18.198329	1044.349205	14.211904
17.709443	1054.958610	14.216922
18.196142	1036.504282	14.221939
17.966228	1047.916223	14.226957
18.202157	1046.744897	14.231975
18.562571	1038.774744	14.236992
18.233458	1039.018238	14.242010
18.512375	1040.099686	14.247027
18.287752	1047.308468	14.252045
18.173782	1044.518458	14.257063
18.416440	1040.780285	14.262080
18.256341	1042.087212	14.267098
18.492612	1038.809274	14.272115
18.111027	1043.223574	14.277133
18.314905	1036.898522	14.282151
18.342095	1032.555706	14.287168
18.129669	1050.210223	14.292186
18.446637	1051.487123	14.297203
18.282815	1047.627569	14.302221
18.523364	1041.363964	14.307239
18.441165	1045.742567	14.312256
18.217954	1050.494419	14.317274
18.485651	1046.007737	14.322291
18.562653	1049.471198	14.327309
18.352305	1033.462207	14.332327
18.478838	1039.434402	14.337344
18.076090	1047.626012	14.342362
18.564783	1066.518801	14.347379
18.074758	1078.216625	14.352397
18.402981	1071.659231	14.357415
18.917239	1065.486781	14.362432
18.691682	1073.474740	14.367450
18.804273	1065.607919	14.372467
18.640422	1066.558830	14.377485
18.904145	1066.186721	14.382503
18.947105	1061.472254	14.387520
19.149367	1066.814720	14.392538
19.228539	1051.732122	14.397555
18.996771	1068.175874	14.402573
19.039955	1075.200080	14.407591
19.406549	1061.365246	14.412608
18.620394	1044.958561	14.417626
18.885140	1034.772486	14.422643
18.968183	1045.928608	14.427661
18.807848	1043.142521	14.432679
19.107871	1053.566641	14.437696
18.794340	1053.402900	14.442714
19.001690	1050.718623	14.447731
18.974910	1061.398101	14.452749
19.095324	1067.425247	14.457767
19.247807	1063.322502	14.462784
19.142723	1064.548697	14.467802
19.415469	1039.064889	14.472819
18.884521	1038.067726	14.477837
19.084143	1024.206195	14.482855
19.134396	1032.916543	14.487872
18.906941	1044.414676	14.492890
18.917442	1045.969351	14.497907
19.049161	1057.752376	14.502925
19.003929	1063.969861	14.507943
19.239532	1064.248359	14.512960
19.058904	1066.778370	14.517978
19.209814	1064.105583	14.522995
19.197525	1059.505151	14.528013
19.077947	1070.614472	14.533031
19.106814	1065.638201	14.538048
18.930598	1067.841944	14.543066
19.397297	1060.940856	14.548083
19.078422	1055.205056	14.553101
19.060934	1063.885284	14.558119
19.344379	1062.241414	14.563136
19.167244	1089.675026	14.568154
19.515940	1086.747143	14.573171
19.585933	1087.799351	14.578189
19.702949	1082.126724	14.583207
19.941422	1067.569471	14.588224
19.647110	1065.937823	14.593242
19.651299	1046.541332	14.598259
19.766262	1056.058980	14.603277
19.384984	1056.508898	14.608295
19.830034	1055.394535	14.613312
19.296870	1049.170807	14.618330
19.394781	1051.785080	14.623347
19.843935	1066.702750	14.628365
19.712132	1068.044366	14.633383
19.648274	1061.161281	14.638400
19.612860	1071.256064	14.643418
19.871338	1074.384470	14.648435
20.028232	1077.583986	14.653453
19.599145	1068.782034	14.658471
20.047844	1049.425255	14.663488
19.753364	1064.258166	14.668506
19.625152	1055.072302	14.673523
19.799782	1059.054783	14.678541
19.897120	1069.213243	14.683559
19.998481	1078.679224	14.688576
20.015950	1077.305256	14.693594
19.317653	1068.586565	14.698611
19.650236	1071.955047	14.703629
19.813888	1083.033908	14.708647
20.112166	1075.762676	14.713664
19.878734	1077.562357	14.718682
20.118033	1082.732986	14.723699
20.184248	1077.429526	14.728717
19.832669	1084.053691	14.733735
20.174176	1071.042747	14.738752
20.003616	1078.023155	14.743770
20.062559	1069.753647	14.748787
19.929976	1064.012449	14.753805
19.554217	1063.409455	14.758823
20.426512	1070.060462	14.763840
20.510924	1075.964447	14.768858
20.212500	1078.017547	14.773875
20.386528	1072.105813	14.778893
20.162546	1068.486277	14.783911
20.050521	1074.824629	14.788928
20.024118	1077.623992	14.793946
20.113884	1073.826838	14.798963
20.062198	1085.689004	14.803981
20.279117	1099.022699	14.808999
20.438645	1106.497699	14.814016
20.630528	1118.668011	14.819034
21.019224	1110.446728	14.824051
20.618618	1095.357165	14.829069
20.200612	1095.508870	14.834087
20.567585	1074.111160	14.839104
20.423690	1088.051235	14.844122
20.550565	1077.296866	14.849139
20.807697	1070.069635	14.854157
20.732340	1064.714981	14.859175
20.770335	1073.244532	14.864192
20.630375	1076.454921	14.869210
20.146138	1073.971134	14.874227
20.691332	1071.792353	14.879245
20.531294	1073.636982	14.884263
20.483707	1074.522428	14.889280
20.575350	1075.509650	14.894298
20.674322	1083.828964	14.899315
20.709305	1078.168911	14.904333
20.575615	1101.757186	14.909351
20.736381	1105.131828	14.914368
20.760740	1113.026154	14.919386
20.808271	1112.828529	14.924403
20.902829	1105.267179	14.929421
20.900659	1109.810501	14.934439
21.390530	1107.541857	14.939456
20.900314	1092.181520	14.944474
20.844992	1078.403403	14.949491
21.066763	1075.167808	14.954509
20.561368	1081.217287	14.959527
21.018890	1090.771837	14.964544
20.789013	1098.943960	14.969562
20.595812	1114.801557	14.974579
21.155334	1104.264605	14.979597
20.937602	1116.602984	14.984615
21.086379	1108.582940	14.989632
21.068724	1117.833216	14.994650
21.061140	1111.189392	14.999667
21.312052	1108.303251	15.004685
21.002982	1117.266303	15.009703
21.339618	1111.637872	15.014720
21.028999	1109.598544	15.019738
21.288824	1107.828868	15.024755
21.235150	1104.903705	15.029773
20.900154	1109.920074	15.034791
21.085546	1112.218175	15.039808
21.034457	1105.376457	15.044826
21.166102	1108.373885	15.049843
21.532744	1102.101817	15.054861
21.295498	1112.537807	15.059879
21.177311	1106.597984	15.064896
21.486226	1105.146327	15.069914
21.092161	1110.660570	15.074931
21.200010	1106.483707	15.079949
21.400944	1127.826905	15.084967
21.680342	1132.638222	15.089984
21.747599	1124.804055	15.095002
21.497111	1119.384439	15.100019
21.498159	1106.655874	15.105037
21.104259	1117.321857	15.110055
21.313267	1114.989800	15.115072
21.764606	1125.651522	15.120090
21.645422	1125.988849	15.125107
21.559863	1123.695825	15.130125
21.471517	1125.623087	15.135143
21.462162	1123.253109	15.140160
21.674550	1130.420810	15.145178
21.830547	1139.433773	15.150195
21.673027	1128.881263	15.155213
21.465068	1137.218262	15.160231
21.557910	1133.211760	15.165248
21.637661	1130.921923	15.170266
21.474485	1139.745148	15.175283
21.826148	1134.555300	15.180301
21.567002	1141.299823	15.185319
21.789149	1161.019729	15.190336
21.944430	1166.031068	15.195354
21.934090	1179.137860	15.200371
22.249763	1166.178933	15.205389
22.133790	1168.642773	15.210407
22.276911	1149.804602	15.215424
22.110851	1139.474919	15.220442
21.869329	1136.999627	15.225459
22.448307	1129.412339	15.230477
22.006640	1134.256608	15.235495
21.823236	1130.181404	15.240512
22.220508	1125.499101	15.245530
22.170394	1134.343791	15.250547
22.206937	1128.545883	15.255565
22.175778	1120.749042	15.260583
22.187696	1132.235828	15.265600
22.207891	1129.592700	15.270618
22.274994	1138.520565	15.275635
22.038757	1129.307830	15.280653
22.157290	1149.313306	15.285671
22.188245	1155.795361	15.290688
22.949182	1162.406159	15.295706
22.198817	1150.232769	15.300723
22.546693	1157.139742	15.305741
22.435364	1159.878165	15.310759
22.325107	1150.504068	15.315776
22.391953	1148.695816	15.320794
22.393381	1166.858351	15.325811
22.661068	1160.173150	15.330829
22.422028	1161.246712	15.335847
22.198020	1154.801208	15.340864
22.644279	1151.232089	15.345882
22.193667	1156.912952	15.350899
22.638973	1150.654830	15.355917
22.587860	1159.105074	15.360935
22.681802	1157.566121	15.365952
22.768319	1153.607305	15.370970
22.731467	1149.986546	15.375987
22.737215	1150.160139	15.381005
22.885588	1162.461870	15.386023
22.763639	1154.591445	15.391040
22.773783	1143.019439	15.396058
22.428205	1152.938597	15.401075
22.893147	1136.319752	15.406093
22.763283	1146.163698	15.411111
22.704480	1149.736618	15.416128
22.763138	1146.984390	15.421146
22.607431	1149.576428	15.426163
22.614290	1143.299636	15.431181
22.769468	1158.640329	15.436199
22.844265	1170.850894	15.441216
23.040005	1171.141888	15.446234
23.170141	1191.367712	15.451251
23.466751	1166.609169	15.456269
23.055929	1169.850561	15.461287
23.053893	1165.924876	15.466304
23.058028	1159.961079	15.471322
22.902822	1174.189869	15.476339
23.024298	1171.300897	15.481357
23.178555	1172.779868	15.486375
23.180990	1177.656060	15.491392
23.283685	1176.203835	15.496410
23.150913	1191.725590	15.501427
23.358009	1178.624973	15.506445
23.693493	1181.743235	15.511463
23.426922	1182.251354	15.516480
23.240238	1186.005234	15.521498
23.517672	1187.121382	15.526515
23.680392	1184.679855	15.531533
23.417545	1170.645245	15.536551
23.230845	1157.893537	15.541568
23.156832	1155.903672	15.546586
23.385962	1179.986160	15.551603
23.468574	1180.991413	15.556621
23.571337	1175.940109	15.561639
23.516903	1188.468850	15.566656
23.515668	1182.377801	15.571674
23.427481	1188.512684	15.576691
23.725299	1181.313122	15.581709
23.727659	1185.031431	15.586727
23.459129	1189.143667	15.591744
23.433418	1174.046397	15.596762
23.123918	1175.709272	15.601779
23.287582	1180.417701	15.606797
23.236766	1188.100704	15.611815
23.321088	1196.687422	15.616832
23.996085	1201.285968	15.621850
24.119278	1199.610897	15.626867
24.186301	1206.435780	15.631885
24.081697	1188.494869	15.636903
23.551786	1172.235044	15.641920
23.865779	1187.572353	15.646938
24.043414	1198.133512	15.651955
23.959375	1201.481121	15.656973
23.977721	1201.638855	15.661991
24.035768	1200.131417	15.667008
24.310249	1191.737852	15.672026
24.011970	1183.389934	15.677043
24.010387	1171.466945	15.682061
23.921484	1177.416537	15.687079
24.390103	1194.647697	15.692096
24.424946	1184.750857	15.697114
24.180624	1174.115430	15.702131
23.897051	1174.000271	15.707149
24.382588	1177.676325	15.712167
24.063917	1192.914282	15.717184
24.392605	1187.577251	15.722202
24.163952	1192.615830	15.727219
24.119157	1202.300106	15.732237
24.452365	1200.604698	15.737255
24.061596	1202.385715	15.742272
24.243302	1195.335827	15.747290
24.460047	1206.716194	15.752307
24.392421	1205.537548	15.757325
24.410093	1193.049435	15.762343
24.271003	1203.200998	15.767360
24.536015	1201.526307	15.772378
24.108125	1197.249397	15.777395
24.288093	1200.142612	15.782413
24.404682	1199.255721	15.787431
24.444800	1202.981572	15.792448
24.632051	1197.383898	15.797466
24.455961	1199.387077	15.802483
24.356450	1209.330362	15.807501
24.690334	1220.279632	15.812519
24.469757	1231.199096	15.817536
24.901958	1222.873532	15.822554
24.544434	1233.085814	15.827571
24.673089	1227.585594	15.832589
24.956566	1229.404975	15.837607
24.456490	1240.091934	15.842624
24.820623	1225.234871	15.847642
24.868566	1229.182237	15.852659
24.786038	1220.068438	15.857677
25.088860	1215.462139	15.862695
25.084197	1224.418841	15.867712
24.974027	1222.538076	15.872730
25.145244	1229.791749	15.877747
25.002228	1220.462978	15.882765
25.040741	1221.852041	15.887783
24.814163	1219.931074	15.892800
25.136330	1225.429542	15.897818
24.880537	1226.133490	15.902835
24.718545	1219.490336	15.907853
24.917137	1221.821308	15.912871
24.432309	1226.253114	15.917888
24.832941	1233.336613	15.922906
25.444687	1239.690841	15.927923
25.355063	1246.414285	15.932941
25.938827	1252.256091	15.937959
25.392078	1237.341107	15.942976
25.620120	1223.343421	15.947994
25.216701	1215.995786	15.953011
25.443206	1207.185794	15.958029
25.322144	1198.604085	15.963047
25.271736	1216.793156	15.968064
25.663315	1235.052889	15.973082
25.687865	1228.355089	15.978099
25.527685	1220.237246	15.983117
25.397475	1212.800572	15.988135
25.467482	1224.960012	15.993152
25.649905	1234.625458	15.998170
25.895529	1232.451482	16.003187
25.627989	1221.388820	16.008205
25.747091	1212.563507	16.013223
25.635654	1211.331283	16.018240
25.502652	1215.118812	16.023258
25.900785	1229.488856	16.028275
25.865589	1239.569148	16.033293
25.967766	1232.547147	16.038311
25.957674	1224.299199	16.043328
25.637629	1215.230950	16.048346
25.757016	1228.859968	16.053363
25.781340	1239.033165	16.058381
25.970941	1241.320553	16.063399
26.100434	1252.352827	16.068416
26.187417	1238.155832	16.073434
26.254509	1221.038354	16.078451
25.703720	1215.420728	16.083469
26.018059	1224.519173	16.088487
26.019660	1239.241522	16.093504
25.850214	1241.030451	16.098522
26.206619	1241.383465	16.103539
26.060096	1239.273111	16.108557
26.276896	1229.593971	16.113575
25.973936	1236.597510	16.118592
26.075380	1236.726949	16.123610
26.351752	1232.783975	16.128627
25.920653	1245.122289	16.133645
26.045285	1239.679020	16.138663
26.091323	1242.382595	16.143680
26.038144	1245.061825	16.148698
26.118709	1241.541307	16.153715
25.913446	1236.884930	16.158733
26.459663	1260.839566	16.163751
26.778491	1266.953473	16.168768
26.708067	1259.523824	16.173786
26.313900	1256.590342	16.178803
26.124270	1248.907799	16.183821
26.287101	1261.242058	16.188839
26.195817	1264.757783	16.193856
26.422151	1270.513802	16.198874
26.535221	1258.431070	16.203891
26.413019	1271.600515	16.208909
26.851872	1267.190785	16.213927
26.364738	1263.981171	16.218944
26.317563	1265.827839	16.223962
26.721267	1257.139302	16.228979
26.259167	1260.820029	16.233997
26.602621	1282.704573	16.239015
26.875787	1296.654055	16.244032
26.893282	1294.924010	16.249050
27.365851	1295.375727	16.254067
27.299353	1279.137028	16.259085
27.072232	1271.993663	16.264103
26.943469	1270.310229	16.269120
26.724332	1273.640814	16.274138
26.871531	1259.435423	16.279155
27.091889	1276.155813	16.284173
27.414798	1278.630399	16.289191
26.914616	1265.943790	16.294208
26.969134	1260.566030	16.299226
27.379742	1273.842282	16.304243
26.921446	1275.570893	16.309261
27.084999	1276.640128	16.314279
27.164289	1283.635238	16.319296
27.436628	1288.348770	16.324314
27.702684	1293.047595	16.329331
27.466288	1280.884230	16.334349
27.563661	1260.482646	16.339367
27.178075	1262.026430	16.344384
27.418459	1257.623323	16.349402
27.561760	1256.000034	16.354419
27.222775	1249.875808	16.359437
27.498198	1254.050315	16.364455
27.625186	1268.562630	16.369472
27.569344	1260.971341	16.374490
27.638434	1256.402475	16.379507
27.393517	1259.694213	16.384525
27.457590	1265.905329	16.389543
27.833325	1281.160098	16.394560
27.853422	1281.209489	16.399578
27.585288	1267.229003	16.404595
27.711862	1279.189794	16.409613
27.278592	1284.957196	16.414631
27.503956	1290.913551	16.419648
27.527452	1295.984698	16.424666
27.915683	1284.360537	16.429683
27.502757	1298.719223	16.434701
27.402130	1287.145929	16.439719
27.367765	1279.436925	16.444736
27.554352	1287.883978	16.449754
27.969362	1294.174100	16.454771
27.733740	1304.678643	16.459789
27.921110	1306.852646	16.464807
28.383289	1302.072962	16.469824
28.002745	1301.378832	16.474842
28.343648	1302.658491	16.479859
28.372303	1293.873666	16.484877
28.749380	1302.330974	16.489895
28.383228	1287.458134	16.494912
27.976153	1285.957087	16.499930
28.389395	1280.623569	16.504947
28.138308	1276.731533	16.509965
28.328928	1280.341207	16.514983
28.446309	1276.350885	16.520000
28.324995	1280.544905	16.525018
28.413769	1282.072300	16.530035
28.354433	1273.735036	16.535053
28.327090	1282.087142	16.540071
28.242828	1284.498522	16.545088
28.227733	1288.597639	16.550106
28.518554	1297.098919	16.555123
28.163911	1305.795634	16.560141
28.622832	1309.449351	16.565159
28.533324	1304.232758	16.570176
28.362262	1307.194434	16.575194
28.814853	1309.630865	16.580211
28.432697	1301.841745	16.585229
28.468886	1304.846325	16.590247
28.645932	1295.009367	16.595264
28.546893	1296.922868	16.600282
28.700857	1289.953888	16.605299
28.160364	1298.604551	16.610317
28.274111	1304.253024	16.615335
28.851667	1311.569884	16.620352
28.625008	1328.837167	16.625370
28.957929	1319.325173	16.630387
29.001907	1313.707044	16.635405
29.182256	1309.992488	16.640423
29.116002	1320.719411	16.645440
28.992320	1327.864405	16.650458
29.386382	1320.125718	16.655475
29.135602	1315.766365	16.660493
29.165971	1325.682751	16.665511
29.229587	1323.051113	16.670528
29.201783	1323.837057	16.675546
29.632491	1317.156537	16.680563
29.432678	1308.050060	16.685581
28.912487	1298.333241	16.690599
29.200070	1305.703527	16.695616
28.951847	1313.364498	16.700634
29.328914	1312.938028	16.705651
29.423169	1312.200470	16.710669
29.253676	1323.591806	16.715687
29.349544	1309.602696	16.720704
29.465381	1315.900146	16.725722
29.461846	1313.929121	16.730739
29.251147	1317.819463	16.735757
29.282898	1317.693921	16.740775
29.523808	1314.405712	16.745792
29.266640	1320.043055	16.750810
29.427178	1313.285940	16.755827
29.594226	1312.242694	16.760845
29.677606	1326.392833	16.765863
29.905120	1310.343474	16.770880
29.987378	1317.293430	16.775898
30.132643	1306.023336	16.780915
30.196291	1310.020680	16.785933
30.040855	1302.971149	16.790951
30.165305	1301.942422	16.795968
29.765006	1302.247675	16.800986
30.177833	1297.548184	16.806003
29.891805	1282.065343	16.811021
29.933814	1302.952833	16.816039
30.135587	1291.892672	16.821056
29.943599	1310.026915	16.826074
30.148331	1293.529630	16.831091
30.182595	1305.172279	16.836109
29.660941	1303.708666	16.841127
29.721645	1299.768250	16.846144
29.493733	1307.488253	16.851162
30.183167	1318.542398	16.856179
30.158518	1327.263322	16.861197
30.080221	1327.310668	16.866215
30.623546	1323.563288	16.871232
30.376200	1323.852910	16.876250
30.293143	1327.296827	16.881267
30.156582	1328.205650	16.886285
30.428529	1324.938094	16.891303
30.174200	1322.139736	16.896320
30.338106	1323.950348	16.901338
30.313634	1325.728320	16.906355
30.615271	1330.244530	16.911373
30.453047	1334.751384	16.916391
30.535183	1323.133296	16.921408
30.601882	1325.049132	16.926426
30.614628	1314.939551	16.931443
30.800298	1319.694576	16.936461
30.484682	1330.285377	16.941479
30.724719	1321.327238	16.946496
30.712727	1320.407856	16.951514
30.594581	1322.342429	16.956531
30.763532	1329.223544	16.961549
30.849306	1344.834912	16.966567
30.794531	1336.579525	16.971584
31.013840	1354.897590	16.976602
31.128265	1347.441682	16.981619
31.578564	1351.138167	16.986637
31.300815	1339.318353	16.991655
31.180978	1327.284291	16.996672
30.833887	1328.026358	17.001690
31.208850	1326.345097	17.006707
31.258848	1317.327236	17.011725
31.116254	1316.250328	17.016743
31.069266	1310.819255	17.021760
30.755890	1323.418846	17.026778
30.970982	1342.720526	17.031795
31.007312	1351.869909	17.036813
31.195507	1345.489850	17.041831
31.160833	1343.015376	17.046848
31.007692	1350.290231	17.051866
30.935336	1345.784864	17.056883
31.200671	1354.127221	17.061901
31.393994	1349.831260	17.066919
31.765709	1361.973230	17.071936
31.248593	1355.851039	17.076954
31.559220	1357.874975	17.081971
31.499155	1372.574380	17.086989
31.682191	1377.508180	17.092007
31.991927	1363.081766	17.097024
31.958976	1369.759486	17.102042
32.122126	1356.505963	17.107059
32.157232	1346.847327	17.112077
32.020075	1341.982249	17.117095
31.756730	1336.945926	17.122112
31.615337	1341.042507	17.127130
32.027430	1342.867219	17.132147
32.129153	1338.764720	17.137165
31.934162	1326.797400	17.142183
32.043389	1331.986263	17.147200
31.591436	1337.117687	17.152218
31.801500	1341.154221	17.157235
32.378239	1327.476520	17.162253
31.802955	1339.869047	17.167271
32.103354	1349.443426	17.172288
31.890639	1356.385066	17.177306
32.009487	1359.076827	17.182323
32.125195	1370.340172	17.187341
32.101697	1365.556684	17.192359
32.226489	1358.288992	17.197376
32.882201	1377.223062	17.202394
32.086310	1361.799005	17.207411
32.521212	1362.125864	17.212429
32.228428	1365.455452	17.217447
32.611820	1372.622563	17.222464
32.347049	1364.978556	17.227482
32.209968	1373.029598	17.232499
32.566536	1356.945480	17.237517
32.233268	1373.295716	17.242535
32.734854	1357.780465	17.247552
32.222315	1364.428002	17.252570
32.471800	1361.185013	17.257587
32.718672	1365.081434	17.262605
32.513178	1363.624025	17.267623
32.925422	1362.362919	17.272640
33.074427	1365.138858	17.277658
32.710339	1365.878225	17.282675
32.960131	1355.178930	17.287693
32.875278	1362.614136	17.292711
32.665833	1356.652096	17.297728
32.704378	1371.028160	17.302746
32.947933	1393.621008	17.307763
33.300417	1391.674200	17.312781
32.923628	1398.306798	17.317799
33.119930	1388.228441	17.322816
33.094409	1392.230504	17.327834
32.990958	1386.519798	17.332851
33.519694	1387.088991	17.337869
33.202229	1397.930109	17.342887
33.061244	1391.552270	17.347904
33.096016	1394.161880	17.352922
33.000371	1388.385129	17.357939
33.360042	1384.767676	17.362957
33.184745	1386.507989	17.367975
33.169106	1383.802441	17.372992
33.222326	1381.348864	17.378010
33.351908	1391.301647	17.383027
33.345420	1394.122772	17.388045
33.341488	1384.804967	17.393063
33.572097	1406.351101	17.398080
33.656655	1417.449770	17.403098
33.627752	1426.257465	17.408115
33.812729	1414.902000	17.413133
33.951142	1409.568387	17.418151
34.029887	1405.952083	17.423168
33.798856	1380.559227	17.428186
33.471156	1384.020162	17.433203
33.840195	1387.190198	17.438221
33.810401	1407.202611	17.443239
33.952941	1401.973620	17.448256
33.925085	1413.963382	17.453274
34.127097	1410.495386	17.458291
34.136062	1402.934847	17.463309
33.976193	1404.186064	17.468327
33.916870	1404.727649	17.473344
34.550686	1406.622604	17.478362
34.154392	1408.153802	17.483379
34.072155	1399.226437	17.488397
34.177978	1405.126421	17.493415
34.220820	1407.270589	17.498432
34.276483	1409.698821	17.503450
34.035721	1402.230135	17.508467
34.466570	1406.798825	17.513485
34.155625	1420.790622	17.518503
34.111735	1409.073625	17.523520
34.214503	1406.886820	17.528538
34.077680	1408.506029	17.533555
34.114988	1397.100580	17.538573
34.064835	1411.086275	17.543591
34.299899	1433.831550	17.548608
34.245004	1441.331716	17.553626
34.231017	1435.805394	17.558643
34.866684	1436.168951	17.563661
34.578682	1443.689925	17.568679
34.859760	1436.771123	17.573696
35.010070	1432.486972	17.578714
34.646871	1430.920203	17.583731
34.525159	1423.311770	17.588749
34.585707	1439.001408	17.593767
34.490874	1435.171491	17.598784
34.683024	1440.924956	17.603802
34.544331	1456.819561	17.608819
34.730856	1443.439873	17.613837
35.017475	1461.186386	17.618855
34.842929	1467.190394	17.623872
35.459798	1453.126277	17.628890
35.193991	1464.209659	17.633907
35.213103	1466.070000	17.638925
35.202847	1460.293085	17.643943
35.362601	1462.998968	17.648960
35.681938	1462.009669	17.653978
35.695883	1459.937324	17.658995
35.969613	1460.341207	17.664013
35.620559	1447.510983	17.669031
35.501988	1438.004834	17.674048
35.674335	1420.358391	17.679066
35.316440	1425.376283	17.684083
35.626994	1418.303622	17.689101
35.553932	1425.991010	17.694119
35.119437	1407.198770	17.699136
35.310510	1424.438856	17.704154
35.553297	1445.339221	17.709171
36.077224	1436.678545	17.714189
35.934834	1444.504744	17.719207
35.772733	1441.507092	17.724224
35.808013	1434.129567	17.729242
35.739633	1443.304574	17.734259
36.037162	1444.841972	17.739277
35.931195	1451.841398	17.744295
35.725602	1442.580108	17.749312
35.751186	1449.574328	17.754330
35.933197	1454.161518	17.759347
36.200448	1445.626904	17.764365
36.039701	1453.927535	17.769383
36.111155	1457.543756	17.774400
36.013552	1451.869653	17.779418
35.647573	1450.062625	17.784435
35.910779	1447.019884	17.789453
36.301764	1459.226257	17.794471
36.092586	1475.104383	17.799488
36.490792	1466.515837	17.804506
36.362721	1491.747267	17.809523
36.491091	1471.115703	17.814541
36.777062	1479.995002	17.819559
36.421835	1473.019938	17.824576
36.595472	1468.678779	17.829594
36.420096	1476.892089	17.834611
36.618644	1465.642006	17.839629
36.653769	1472.487828	17.844647
36.497783	1472.621232	17.849664
36.471824	1461.391129	17.854682
36.426975	1476.557151	17.859699
36.317100	1471.039577	17.864717
36.606297	1471.214752	17.869735
36.324219	1464.669672	17.874752
36.818426	1477.201477	17.879770
36.390768	1496.999476	17.884787
36.937626	1502.555194	17.889805
37.021476	1502.966050	17.894823
37.046324	1510.124374	17.899840
37.207249	1500.249600	17.904858
36.936949	1491.750254	17.909875
37.212531	1500.795827	17.914893
37.314335	1497.528993	17.919911
37.264947	1490.008365	17.924928
37.067714	1484.607374	17.929946
37.171600	1484.225257	17.934963
37.418872	1483.075841	17.939981
37.308814	1477.516961	17.944999
36.776623	1485.943943	17.950016
37.182370	1488.502107	17.955034
37.089178	1492.038669	17.960051
37.362145	1499.324665	17.965069
37.487948	1504.836002	17.970087
37.852909	1515.153263	17.975104
37.895472	1516.132681	17.980122
37.824640	1500.094439	17.985139
37.916266	1494.130028	17.990157
38.021074	1476.457088	17.995175
37.504301	1495.216602	18.000192
37.765603	1479.167585	18.005210
37.558793	1488.912865	18.010227
37.745891	1492.153141	18.015245
38.104916	1499.702636	18.020263
38.155313	1505.343151	18.025280
38.367542	1489.898022	18.030298
37.973364	1475.177249	18.035315
38.002313	1486.928578	18.040333
38.424768	1483.886478	18.045351
37.986739	1472.980924	18.050368
38.117826	1468.261217	18.055386
37.921468	1473.295732	18.060403
38.067078	1492.667146	18.065421
38.056184	1511.381070	18.070439
38.022284	1514.090029	18.075456
38.345238	1514.623164	18.080474
38.198433	1513.558353	18.085491
38.048521	1520.063758	18.090509
38.481531	1509.612194	18.095527
38.046315	1519.238958	18.100544
38.370386	1512.357501	18.105562
38.302991	1512.409737	18.110579
38.747661	1531.977813	18.115597
38.861321	1541.584746	18.120615
38.756127	1536.601149	18.125632
39.084360	1537.720346	18.130650
38.953922	1522.346572	18.135667
38.859434	1523.712766	18.140685
39.095535	1507.703903	18.145703
38.706156	1510.504081	18.150720
38.837710	1505.078668	18.155738
39.147367	1511.772265	18.160755
38.957219	1517.250592	18.165773
39.065527	1506.037240	18.170791
38.981538	1531.232517	18.175808
38.923636	1541.697420	18.180826
39.057067	1529.614654	18.185843
38.920520	1530.490223	18.190861
39.325614	1528.325480	18.195879
39.308532	1534.162369	18.200896
39.314779	1522.773179	18.205914
39.409195	1522.118841	18.210931
39.186072	1538.457153	18.215949
39.557893	1535.207296	18.220967
39.233438	1531.507217	18.225984
39.609676	1527.604549	18.231002
39.422803	1523.351292	18.236019
39.149850	1526.815415	18.241037
39.244996	1528.868684	18.246055
39.389753	1543.495237	18.251072
39.507387	1550.578215	18.256090
39.945317	1559.063597	18.261107
39.605854	1567.928599	18.266125
39.624677	1568.956032	18.271143
39.918938	1570.688447	18.276160
40.519729	1561.620758	18.281178
40.577231	1537.740790	18.286195
40.160414	1532.834277	18.291213
40.288106	1517.684354	18.296231
40.259334	1523.749717	18.301248
40.072138	1519.030826	18.306266
40.259252	1510.171666	18.311283
40.269078	1521.969287	18.316301
39.800814	1512.042790	18.321319
39.874594	1505.779590	18.326336
40.078398	1518.362174	18.331354
40.236198	1526.896980	18.336371
40.181436	1536.100891	18.341389
40.416435	1538.931343	18.346407
40.210770	1539.624068	18.351424
40.687758	1546.790163	18.356442
40.632268	1550.739943	18.361459
40.218970	1544.315713	18.366477
40.341962	1545.824490	18.371495
40.592352	1546.634741	18.376512
40.623658	1553.862088	18.381530
40.607452	1545.020958	18.386547
40.516306	1547.362069	18.391565
40.530082	1547.452854	18.396583
40.375897	1540.720093	18.401600
40.718024	1561.482955	18.406618
40.943158	1570.677637	18.411635
40.893800	1564.381620	18.416653
40.986929	1573.626461	18.421671
40.952633	1571.212707	18.426688
41.168066	1566.496155	18.431706
40.841297	1567.251015	18.436723
41.261851	1571.550820	18.441741
41.215183	1569.444979	18.446759
41.004759	1576.710314	18.451776
41.268481	1582.436654	18.456794
41.213867	1583.149886	18.461811
41.205183	1574.037254	18.466829
41.498319	1574.934132	18.471847
41.377325	1569.728360	18.476864
40.990873	1568.720861	18.481882
41.311681	1569.016390	18.486899
41.441138	1588.070555	18.491917
41.920102	1593.521202	18.496935
41.765693	1593.481926	18.501952
41.630711	1592.938516	18.506970
41.732658	1604.717237	18.511987
41.875418	1596.305068	18.517005
41.725135	1599.869787	18.522023
41.742252	1606.025422	18.527040
41.673074	1611.321410	18.532058
41.840632	1602.847863	18.537075
41.816097	1593.274116	18.542093
41.539648	1599.485543	18.547111
41.992289	1594.908897	18.552128
41.783150	1599.908954	18.557146
42.195316	1601.662041	18.562163
41.851229	1616.255285	18.567181
42.492162	1619.494205	18.572199
42.187625	1621.529686	18.577216
42.231879	1625.353567	18.582234
42.399837	1617.863882	18.587251
42.000364	1622.911540	18.592269
42.366839	1619.507056	18.597287
42.524557	1617.677238	18.602304
42.476611	1615.917425	18.607322
42.680930	1611.194234	18.612339
42.380986	1613.581865	18.617357
42.216556	1602.974862	18.622375
42.833801	1607.774787	18.627392
42.502320	1616.616846	18.632410
42.698396	1610.077324	18.637427
42.670598	1611.806475	18.642445
42.697255	1607.323247	18.647463
42.643136	1620.636838	18.652480
42.886370	1643.422408	18.657498
43.190395	1647.216751	18.662515
42.911594	1648.722652	18.667533
43.523086	1620.596583	18.672551
44.012286	1614.362121	18.677568
43.836522	1603.758958	18.682586
43.871968	1588.821428	18.687603
43.914127	1592.322459	18.692621
43.815439	1576.521979	18.697639
43.551450	1577.520566	18.702656
43.124485	1569.221454	18.707674
43.541303	1564.567676	18.712691
43.172889	1570.873019	18.717709
43.520954	1560.713966	18.722727
43.739694	1564.661144	18.727744
43.428198	1575.965516	18.732762
43.647004	1566.778882	18.737779
43.549424	1583.951114	18.742797
43.821390	1575.921689	18.747815
43.848752	1584.357033	18.752832
43.611169	1585.401448	18.757850
43.863730	1583.247338	18.762867
43.665676	1589.251539	18.767885
43.926448	1599.134555	18.772903
43.621622	1579.032447	18.777920
43.958105	1583.243996	18.782938
43.986409	1587.392511	18.787955
43.835330	1597.882692	18.792973
43.986426	1595.281427	18.797991
43.785010	1594.933816	18.803008
43.760200	1607.075963	18.808026
44.164258	1601.092752	18.813043
43.951054	1622.421424	18.818061
44.116559	1623.101236	18.823079
44.331114	1615.271411	18.828096
44.145195	1628.319029	18.833114
44.198847	1618.858708	18.838131
44.132722	1626.521234	18.843149
44.562343	1633.308827	18.848167
44.753388	1640.117542	18.853184
44.589356	1646.708985	18.858202
44.755635	1646.852907	18.863219
44.723890	1646.613264	18.868237
44.667406	1652.382702	18.873255
45.029100	1644.467729	18.878272
44.989513	1648.798129	18.883290
45.328803	1639.859620	18.888307
44.897178	1644.018019	18.893325
44.854814	1641.428247	18.898343
44.836493	1651.050366	18.903360
44.595044	1648.412004	18.908378
45.001291	1644.839742	18.913395
45.289932	1646.199517	18.918413
44.558524	1641.704361	18.923431
45.214349	1635.112277	18.928448
44.959542	1657.480229	18.933466
45.664303	1665.760573	18.938483
45.295588	1664.249801	18.943501
44.850434	1668.561212	18.948519
45.330202	1674.716397	18.953536
45.491301	1671.583018	18.958554
45.788116	1676.137132	18.963571
45.475564	1680.133755	18.968589
45.646492	1684.681316	18.973607
45.799760	1666.709238	18.978624
45.895073	1673.920947	18.983642
45.792352	1667.090856	18.988659
45.775137	1664.863416	18.993677
46.101101	1658.633473	18.998695
45.765536	1658.076756	19.003712
45.716333	1674.433906	19.008730
46.139309	1659.823758	19.013747
46.207068	1663.958688	19.018765
45.919044	1673.071911	19.023783
46.116337	1665.013249	19.028800
45.672734	1681.912494	19.033818
46.009442	1695.644777	19.038835
46.257960	1703.120126	19.043853
46.267067	1697.252334	19.048871
46.542953	1698.866161	19.053888
46.558694	1697.889817	19.058906
46.487299	1686.194279	19.063923
46.283723	1692.930449	19.068941
46.604044	1696.522923	19.073959
46.652750	1696.146770	19.078976
46.430730	1692.042958	19.083994
46.465540	1680.293460	19.089011
46.709436	1689.367214	19.094029
46.278080	1694.385324	19.099047
46.924097	1710.611488	19.104064
46.806052	1715.872483	19.109082
46.622786	1721.718600	19.114099
46.988720	1708.974116	19.119117
46.971678	1721.744525	19.124135
47.235060	1722.278261	19.129152
46.955668	1719.900655	19.134170
47.236923	1716.243138	19.139187
47.106226	1721.279872	19.144205
47.088045	1726.555663	19.149223
47.399976	1719.656634	19.154240
47.081980	1726.492623	19.159258
47.057547	1731.068348	19.164275
47.450477	1744.820909	19.169293
47.436597	1749.302976	19.174311
47.641944	1758.925993	19.179328
47.623731	1753.441786	19.184346
47.861947	1748.235052	19.189363
48.084308	1753.699030	19.194381
47.837300	1746.124921	19.199399
47.599030	1751.698084	19.204416
47.644288	1752.095641	19.209434
47.878501	1758.040285	19.214451
47.961229	1747.443318	19.219469
47.883376	1749.666724	19.224487
48.102951	1745.364151	19.229504
47.908473	1742.762691	19.234522
47.882835	1752.342584	19.239539
47.930350	1754.089617	19.244557
47.786558	1762.116776	19.249575
48.081523	1755.810036	19.254592
48.515792	1780.050490	19.259610
48.369449	1775.730236	19.264627
48.571436	1776.458548	19.269645
48.374093	1776.289964	19.274663
48.602820	1782.918716	19.279680
48.689010	1771.210850	19.284698
48.535240	1780.684979	19.289715
48.650829	1774.345872	19.294733
48.584619	1768.782396	19.299751
48.931647	1766.568364	19.304768
48.906519	1765.839097	19.309786
49.260674	1772.539627	19.314803
49.032911	1759.011024	19.319821
49.037837	1762.020861	19.324839
49.085735	1756.829828	19.329856
48.729746	1751.603188	19.334874
48.828345	1763.694754	19.339891
48.983702	1752.735032	19.344909
48.871819	1764.871420	19.349927
48.893295	1764.423395	19.354944
49.056326	1758.688001	19.359962
48.670621	1759.381356	19.364979
48.986585	1769.265400	19.369997
49.005679	1785.779867	19.375015
49.163304	1792.686092	19.380032
49.210352	1795.457897	19.385050
48.996887	1801.911725	19.390067
49.538260	1799.946841	19.395085
49.377021	1819.146169	19.400103
49.725046	1815.107753	19.405120
49.798748	1812.148810	19.410138
49.936449	1818.723336	19.415155
49.885039	1814.895989	19.420173
49.956836	1807.193585	19.425191
50.020288	1805.775735	19.430208
50.232203	1804.817159	19.435226
50.147303	1811.357804	19.440243
50.229497	1813.334914	19.445261
50.374065	1811.731435	19.450279
50.374578	1801.398580	19.455296
50.479046	1810.003570	19.460314
50.242624	1816.267517	19.465331
50.274039	1804.895807	19.470349
50.696204	1805.519437	19.475367
50.817020	1805.887189	19.480384
50.639918	1801.750927	19.485402
51.086807	1805.927564	19.490419
50.760239	1777.736365	19.495437
50.481427	1770.972921	19.500455
50.792800	1769.378295	19.505472
50.900936	1790.229735	19.510490
51.071812	1796.136637	19.515507
51.068088	1784.275330	19.520525
50.895902	1788.586544	19.525543
51.054909	1775.915564	19.530560
50.859646	1785.625466	19.535578
51.078047	1799.004205	19.540595
51.040620	1795.607773	19.545613
50.703710	1797.391371	19.550631
51.036851	1802.873867	19.555648
51.172761	1801.036609	19.560666
50.825464	1794.714936	19.565683
51.132314	1791.708218	19.570701
50.995612	1808.383283	19.575719
51.037048	1818.706185	19.580736
51.052558	1823.482794	19.585754
51.167089	1820.339759	19.590771
51.389030	1824.538418	19.595789
51.340334	1826.136021	19.600807
51.668112	1819.717151	19.605824
51.906242	1833.724679	19.610842
51.949539	1837.095473	19.615859
52.352101	1820.693659	19.620877
51.682926	1817.870268	19.625895
51.870412	1811.962721	19.630912
52.040263	1817.198220	19.635930
52.118395	1834.551120	19.640947
52.267697	1842.944805	19.645965
52.300843	1840.712363	19.650983
52.216800	1840.865766	19.656000
52.471973	1834.138647	19.661018
52.079479	1838.430183	19.666035
52.604569	1839.850302	19.671053
52.511089	1846.989758	19.676071
52.535518	1848.745340	19.681088
52.513161	1845.087379	19.686106
52.607942	1848.661457	19.691123
52.627031	1838.161548	19.696141
52.631405	1852.181345	19.701159
53.061491	1853.213861	19.706176
52.540389	1841.900556	19.711194
52.465582	1844.271882	19.716211
52.821831	1841.135154	19.721229
52.650843	1856.028528	19.726247
52.333962	1846.536001	19.731264
52.695647	1852.329119	19.736282
52.474365	1871.892728	19.741299
52.899206	1869.425691	19.746317
52.958353	1868.492552	19.751335
52.852571	1860.569491	19.756352
53.106548	1887.448689	19.761370
53.236798	1893.554251	19.766387
53.612042	1901.379190	19.771405
53.727225	1902.972552	19.776423
53.672097	1899.691019	19.781440
53.690991	1891.711910	19.786458
53.686285	1898.506439	19.791475
53.894790	1890.959927	19.796493
53.796882	1890.817425	19.801511
53.957709	1902.416386	19.806528
54.067386	1899.317243	19.811546
54.097491	1901.692892	19.816563
53.885436	1871.347582	19.821581
53.944415	1891.334539	19.826599
54.020084	1889.212767	19.831616
54.059274	1890.541550	19.836634
53.974252	1897.263139	19.841651
54.345051	1894.975483	19.846669
54.218784	1882.800723	19.851687
54.283864	1883.688461	19.856704
54.332327	1883.366276	19.861722
54.126575	1893.066562	19.866739
54.416030	1878.274946	19.871757
54.551030	1878.455336	19.876775
54.176830	1888.404298	19.881792
54.443279	1893.527807	19.886810
54.375734	1910.967065	19.891827
54.818851	1906.567475	19.896845
54.465090	1918.610502	19.901863
54.302264	1923.995490	19.906880
54.743579	1913.106303	19.911898
54.399758	1926.303874	19.916915
55.017594	1917.878569	19.921933
55.029999	1931.495184	19.926951
55.330432	1938.223757	19.931968
55.451475	1941.431939	19.936986
55.206631	1943.913456	19.942003
55.375748	1939.138901	19.947021
55.745141	1935.489601	19.952039
55.753546	1931.640728	19.957056
55.744116	1929.696383	19.962074
55.699320	1907.579814	19.967091
55.895704	1892.649053	19.972109
55.587854	1897.122267	19.977127
55.816858	1899.531774	19.982144
55.819738	1896.423314	19.987162
55.486646	1899.719916	19.992179
55.743193	1895.052174	19.997197
56.099510	1914.077522	20.002215
55.600084	1928.724286	20.007232
55.827624	1927.310804	20.012250
55.943064	1933.286756	20.017267
56.136348	1919.874439	20.022285
55.973703	1920.847837	20.027303
56.037465	1922.144415	20.032320
56.135023	1916.108002	20.037338
55.852378	1926.584520	20.042355
56.196552	1924.904152	20.047373
55.997176	1934.795319	20.052391
56.079653	1952.881223	20.057408
56.411645	1945.178662	20.062426
56.309780	1948.805138	20.067443
56.143180	1947.823480	20.072461
56.209690	1951.314270	20.077479
56.282465	1975.833843	20.082496
56.660060	1974.068427	20.087514
57.125840	1985.256070	20.092531
56.927674	1974.236512	20.097549
57.009631	1974.989589	20.102567
57.027250	1992.151899	20.107584
57.346635	1965.084204	20.112602
56.867011	1978.652455	20.117619
57.016841	1967.177601	20.122637
57.169855	1973.767771	20.127655
57.686751	1989.218403	20.132672
57.849204	2000.584712	20.137690
57.760526	1983.593495	20.142707
57.591244	1967.915292	20.147725
57.657019	1971.249333	20.152743
57.695420	1967.414587	20.157760
57.771237	1956.487155	20.162778
57.964846	1975.015108	20.167795
57.724929	1964.303411	20.172813
58.063185	1980.497460	20.177831
57.925230	1992.703485	20.182848
57.981758	1989.382421	20.187866
57.871314	1991.062285	20.192883
58.080002	1994.691188	20.197901
58.073420	1996.380265	20.202919
58.104479	1994.132793	20.207936
58.549857	1995.544055	20.212954
58.241567	1990.503920	20.217971
58.416231	1994.178599	20.222989
58.502636	1985.331873	20.228007
58.142793	1985.913296	20.233024
58.819311	1992.561047	20.238042
58.587800	1997.089188	20.243059
58.515978	2004.473736	20.248077
58.664733	1995.899941	20.253095
58.528651	1998.591819	20.258112
58.830038	1999.115152	20.263130
58.724414	2013.520560	20.268147
58.948517	2028.132888	20.273165
59.228895	2015.343241	20.278183
59.173013	2027.506403	20.283200
59.174271	2015.092377	20.288218
59.402812	2022.344826	20.293235
59.061863	2027.997058	20.298253
59.214317	2023.674991	20.303271
59.029989	2025.069655	20.308288
59.146370	2019.130279	20.313306
58.979748	2024.854480	20.318323
59.169244	2026.087774	20.323341
59.721516	2027.053659	20.328359
59.395875	2045.756077	20.333376
60.000042	2040.900939	20.338394
59.846638	2043.129392	20.343411
60.152018	2034.426948	20.348429
60.155426	2031.791163	20.353447
59.958390	2036.858646	20.358464
60.217503	2036.261316	20.363482
60.366632	2029.031803	20.368499
60.117514	2030.665105	20.373517
60.408952	2020.833583	20.378535
60.004829	2028.410246	20.383552
60.334661	2021.130405	20.388570
59.985495	2027.465425	20.393587
60.094085	2028.881168	20.398605
60.212105	2028.726012	20.403623
59.931729	2026.851819	20.408640
59.951462	2029.047132	20.413658
60.173894	2055.732053	20.418675
60.625353	2049.526684	20.423693
60.373713	2062.611904	20.428711
60.209639	2059.704803	20.433728
60.797009	2079.668659	20.438746
60.999771	2089.737349	20.443763
60.821489	2084.193066	20.448781
61.329388	2074.822939	20.453799
61.317180	2082.492331	20.458816
61.369102	2078.203002	20.463834
61.507076	2078.657091	20.468851
61.593162	2072.839422	20.473869
61.626758	2062.296613	20.478887
61.300165	2072.579526	20.483904
61.326829	2063.321603	20.488922
61.516536	2075.685537	20.493939
61.636930	2076.068719	20.498957
61.557421	2073.476744	20.503975
61.882957	2073.347330	20.508992
61.474664	2076.744970	20.514010
61.928528	2085.659864	20.519027
61.815649	2113.281119	20.524045
62.235104	2101.205558	20.529063
62.120663	2115.614880	20.534080
62.498626	2099.958897	20.539098
62.561502	2100.692301	20.544115
62.373852	2102.980945	20.549133
62.940739	2094.536211	20.554151
62.198143	2084.299193	20.559168
62.470049	2084.353232	20.564186
62.405792	2076.458038	20.569203
62.478342	2099.416373	20.574221
62.660115	2088.829771	20.579239
62.514591	2107.411759	20.584256
62.663513	2097.001824	20.589274
62.855985	2098.184440	20.594291
62.690141	2108.764603	20.599309
63.112712	2093.561647	20.604327
62.883688	2108.619171	20.609344
62.869431	2107.630831	20.614362
62.848104	2103.363638	20.619379
62.580074	2121.882823	20.624397
62.759886	2126.350315	20.629415
62.838736	2131.178555	20.634432
63.009048	2119.200051	20.639450
63.557590	2118.842464	20.644467
63.398650	2113.239270	20.649485
63.743953	2123.543657	20.654503
63.519855	2124.459118	20.659520
63.651999	2139.789835	20.664538
63.986798	2146.298470	20.669555
63.855985	2152.127815	20.674573
64.154754	2147.413457	20.679591
63.800735	2157.909799	20.684608
64.190516	2146.926808	20.689626
64.039811	2157.142133	20.694643
63.946793	2156.893513	20.699661
64.416127	2147.467319	20.704679
64.207831	2143.198927	20.709696
64.279778	2148.313525	20.714714
64.364181	2139.642223	20.719731
64.288005	2147.578495	20.724749
64.555259	2147.374467	20.729767
64.535609	2147.879799	20.734784
64.224351	2143.184759	20.739802
64.615806	2140.159467	20.744819
64.593879	2129.807661	20.749837
64.658714	2158.733372	20.754855
64.694927	2163.940290	20.759872
64.883425	2164.788754	20.764890
65.162607	2157.324126	20.769907
65.013154	2165.958283	20.774925
65.152805	2169.279963	20.779943
65.091238	2171.613918	20.784960
65.097605	2171.806120	20.789978
65.442681	2172.923567	20.794995
65.121587	2177.723825	20.800013
65.400712	2170.981973	20.805031
65.416006	2193.576517	20.810048
65.575611	2196.869907	20.815066
65.718409	2188.112754	20.820083
65.841150	2207.517979	20.825101
66.045742	2187.799163	20.830119
65.986898	2198.406782	20.835136
66.066637	2192.670228	20.840154
66.088653	2183.460831	20.845171
65.945916	2188.594188	20.850189
65.973761	2186.132276	20.855207
66.003073	2196.071444	20.860224
65.749103	2188.511650	20.865242
65.832379	2192.040862	20.870259
66.312481	2216.225617	20.875277
66.898713	2210.603967	20.880295
66.537499	2210.373683	20.885312
66.485730	2207.398786	20.890330
66.488528	2213.317483	20.895347
66.641895	2209.531390	20.900365
66.530299	2206.590000	20.905383
66.699202	2219.643061	20.910400
66.776423	2220.902798	20.915418
66.842256	2225.743651	20.920435
66.875939	2243.686987	20.925453
67.061835	2250.072646	20.930471
67.084389	2238.456825	20.935488
67.343201	2238.015037	20.940506
67.989932	2231.349804	20.945523
67.690587	2235.939219	20.950541
68.052589	2223.499662	20.955559
68.030762	2222.534217	20.960576
67.821148	2216.122103	20.965594
67.817048	2194.655234	20.970611
67.956959	2195.043066	20.975629
67.941304	2192.992049	20.980647
68.077165	2193.158325	20.985664
68.096912	2190.247789	20.990682
68.005874	2187.314225	20.995699
67.829025	2190.715176	21.000717
68.157002	2189.132331	21.005735
68.049040	2182.272367	21.010752
67.898259	2198.319524	21.015770
68.321183	2209.309116	21.020787
68.352753	2214.875254	21.025805
68.261040	2232.042316	21.030823
68.237492	2223.508481	21.035840
67.968989	2220.157816	21.040858
68.296630	2224.806796	21.045875
68.458381	2244.885095	21.050893
68.322431	2244.183172	21.055911
68.541947	2251.140001	21.060928
68.781906	2254.783483	21.065946
68.534724	2254.736504	21.070963
68.847108	2261.520721	21.075981
68.959235	2273.800988	21.080999
69.197220	2280.436694	21.086016
69.059661	2282.173034	21.091034
69.555487	2278.096495	21.096051
69.216762	2287.660351	21.101069
69.319169	2298.453384	21.106087
69.618878	2287.560368	21.111104
69.364553	2287.523624	21.116122
69.410818	2281.635298	21.121139
69.523007	2291.279357	21.126157
69.855989	2293.564667	21.131175
70.206002	2295.800317	21.136192
69.981532	2302.989776	21.141210
70.303450	2299.465353	21.146227
70.167442	2300.756592	21.151245
70.019278	2306.477256	21.156263
70.151077	2300.400983	21.161280
69.927900	2305.314223	21.166298
70.204035	2287.852576	21.171315
70.128371	2306.137651	21.176333
70.143006	2319.239908	21.181351
70.394050	2322.307011	21.186368
70.315043	2329.759629	21.191386
70.523394	2314.845970	21.196403
70.846170	2328.463809	21.201421
71.024787	2308.366680	21.206439
71.105018	2325.416464	21.211456
71.192770	2317.399775	21.216474
71.326654	2314.841783	21.221491
71.265561	2315.500808	21.226509
71.150886	2316.900128	21.231527
71.351899	2310.244150	21.236544
71.361687	2327.511072	21.241562
71.059458	2334.235872	21.246579
71.268987	2343.292662	21.251597
71.311329	2342.076663	21.256615
71.550214	2338.769678	21.261632
71.304670	2344.502708	21.266650
71.664198	2340.592759	21.271667
71.985199	2362.309732	21.276685
72.148916	2364.151994	21.281703
72.425321	2352.964184	21.286720
72.315464	2362.643209	21.291738
72.481975	2353.894641	21.296755
72.442578	2334.399013	21.301773
72.331212	2326.649457	21.306791
72.310317	2321.726472	21.311808
72.526616	2330.386497	21.316826
72.277937	2350.086330	21.321843
72.415321	2352.719499	21.326861
72.410922	2366.045792	21.331879
72.741907	2358.011328	21.336896
72.341569	2357.898521	21.341914
72.689343	2368.622319	21.346931
72.719656	2360.513138	21.351949
72.468693	2359.509372	21.356967
73.048287	2366.840580	21.361984
73.354633	2385.328942	21.367002
73.482452	2382.423345	21.372019
73.491077	2378.560152	21.377037
73.414892	2390.636804	21.382055
73.586147	2371.204346	21.387072
73.896667	2370.016072	21.392090
73.786344	2369.906716	21.397107
73.724497	2375.521613	21.402125
73.748097	2380.764544	21.407143
73.979696	2358.295182	21.412160
73.854099	2371.472031	21.417178
73.858394	2367.491258	21.422195
73.984811	2358.126326	21.427213
73.730774	2365.592728	21.432231
73.763509	2379.887825	21.437248
73.997113	2375.048941	21.442266
74.241680	2387.304265	21.447283
74.304888	2397.399367	21.452301
74.612349	2404.026598	21.457319
74.430329	2391.722666	21.462336
74.373254	2401.235721	21.467354
74.562455	2391.816106	21.472371
74.960326	2401.999600	21.477389
74.676273	2396.753764	21.482407
74.522784	2400.044412	21.487424
74.402787	2412.366297	21.492442
74.690923	2412.980609	21.497459
74.808381	2418.463538	21.502477
74.850436	2428.175568	21.507495
75.106000	2428.541344	21.512512
75.202116	2464.452336	21.517530
75.533203	2455.317484	21.522547
75.964720	2471.441722	21.527565
75.689799	2450.450913	21.532583
75.801608	2440.963748	21.537600
75.981272	2450.765053	21.542618
76.050504	2457.775351	21.547635
76.525521	2444.241424	21.552653
76.187095	2449.833552	21.557671
76.286534	2453.047182	21.562688
76.178969	2449.075621	21.567706
76.075405	2442.856307	21.572723
76.293785	2437.876818	21.577741
75.947511	2453.133764	21.582759
76.060031	2444.477526	21.587776
76.112750	2449.480645	21.592794
76.105812	2437.718967	21.597811
76.466373	2455.471339	21.602829
76.075590	2473.618933	21.607847
76.564580	2475.162987	21.612864
76.433962	2475.911455	21.617882
76.500184	2493.842816	21.622899
76.882553	2499.223341	21.627917
76.838201	2506.628587	21.632935
76.877161	2510.221097	21.637952
76.731160	2512.337968	21.642970
77.080664	2522.998009	21.647987
77.218923	2526.856381	21.653005
77.327459	2534.730440	21.658023
77.950194	2513.925247	21.663040
77.679522	2530.370094	21.668058
77.767895	2524.279061	21.673075
77.789689	2527.489790	21.678093
77.382574	2531.584336	21.683111
77.964516	2525.528270	21.688128
77.879764	2527.371259	21.693146
77.748110	2525.555296	21.698163
78.066348	2528.900100	21.703181
78.156681	2554.498136	21.708199
78.459235	2552.673408	21.713216
78.353138	2560.465238	21.718234
78.628783	2562.210491	21.723251
78.786427	2552.596792	21.728269
78.626266	2557.723701	21.733287
78.752878	2551.884196	21.738304
78.598229	2563.603499	21.743322
78.739480	2555.615639	21.748339
79.072208	2552.908813	21.753357
78.557786	2561.235412	21.758375
78.896371	2572.864951	21.763392
79.421476	2579.481685	21.768410
79.208138	2577.099327	21.773427
79.397623	2583.155024	21.778445
79.434232	2587.767960	21.783463
79.501263	2585.079444	21.788480
79.440405	2592.053625	21.793498
79.620304	2584.335726	21.798515
79.427653	2591.945036	21.803533
79.280527	2586.223582	21.808551
79.806133	2604.483665	21.813568
79.777138	2614.375260	21.818586
79.997970	2604.416461	21.823603
80.055601	2599.117834	21.828621
79.850488	2603.351057	21.833639
80.059962	2607.103198	21.838656
80.378135	2621.047826	21.843674
79.811695	2636.003556	21.848691
80.462626	2628.773517	21.853709
80.635811	2639.178538	21.858727
80.683400	2634.786627	21.863744
80.777854	2623.299572	21.868762
80.845090	2621.890472	21.873779
81.207341	2624.061947	21.878797
80.758176	2639.391587	21.883815
80.727993	2653.944172	21.888832
81.313530	2665.988855	21.893850
81.132682	2657.938819	21.898867
81.708333	2656.029190	21.903885
81.767743	2665.205853	21.908903
82.041976	2651.928140	21.913920
82.152174	2655.062480	21.918938
82.167221	2647.191879	21.923955
82.187645	2642.304481	21.928973
82.006813	2641.860337	21.933991
82.063443	2645.392481	21.939008
82.119935	2632.279892	21.944026
81.870648	2640.162349	21.949043
81.994327	2645.765190	21.954061
82.034554	2634.403617	21.959079
82.001915	2640.912947	21.964096
82.005479	2641.855971	21.969114
82.121061	2647.327087	21.974131
82.218222	2660.357536	21.979149
82.199889	2677.625756	21.984167
82.458963	2661.559348	21.989184
82.436437	2665.147094	21.994202
82.437436	2690.644769	21.999219
82.523763	2695.289284	22.004237
82.811383	2711.016510	22.009255
82.812441	2700.493602	22.014272
82.936585	2699.351062	22.019290
82.819577	2715.403802	22.024307
83.048907	2718.967659	22.029325
83.048758	2739.209961	22.034343
83.450995	2714.193111	22.039360
83.743495	2725.707552	22.044378
83.598572	2738.900505	22.049395
83.774203	2733.204793	22.054413
83.884887	2724.475477	22.059431
83.909871	2745.430921	22.064448
84.060613	2750.734067	22.069466
83.722382	2756.960494	22.074483
84.420136	2750.993074	22.079501
84.460620	2760.864620	22.084519
84.423902	2741.755027	22.089536
84.306045	2748.916248	22.094554
84.493359	2746.506633	22.099571
84.609612	2745.875605	22.104589
84.566013	2742.596710	22.109607
84.376975	2745.678158	22.114624
84.773243	2754.194515	22.119642
84.891672	2772.207921	22.124659
85.067899	2769.425349	22.129677
84.678493	2769.556585	22.134695
84.974741	2779.531936	22.139712
85.476539	2776.973504	22.144730
85.326184	2785.038496	22.149747
85.511394	2781.683991	22.154765
85.605924	2794.253197	22.159783
85.934802	2791.041084	22.164800
85.967935	2786.930640	22.169818
85.839747	2790.345726	22.174835
86.297303	2785.822645	22.179853
86.169358	2788.233013	22.184871
86.356382	2785.310864	22.189888
86.312721	2779.582871	22.194906
85.995395	2791.968962	22.199923
86.368232	2789.883393	22.204941
86.418004	2787.273674	22.209959
86.483282	2787.563231	22.214976
86.415636	2787.647992	22.219994
86.281001	2789.066990	22.225011
86.891648	2811.112307	22.230029
86.527350	2819.939016	22.235047
86.685151	2817.412225	22.240064
87.115730	2811.155087	22.245082
86.898373	2813.575115	22.250099
86.936820	2817.950031	22.255117
87.312048	2829.417417	22.260135
87.189913	2840.512685	22.265152
87.458650	2840.026921	22.270170
87.506801	2849.731123	22.275187
87.316766	2843.824939	22.280205
87.355343	2833.691788	22.285223
87.550872	2847.140767	22.290240
87.786512	2844.652681	22.295258
87.902519	2859.662385	22.300275
88.270290	2858.899637	22.305293
88.290328	2862.547716	22.310311
88.258672	2861.841916	22.315328
88.478210	2852.588655	22.320346
88.624516	2868.753943	22.325363
88.557858	2864.479661	22.330381
88.514974	2867.748390	22.335399
88.569100	2873.806491	22.340416
89.113194	2857.739630	22.345434
88.667270	2879.573431	22.350451
88.841730	2858.487142	22.355469
88.755135	2873.609075	22.360487
89.228442	2879.892387	22.365504
89.281718	2882.786189	22.370522
89.219132	2895.554662	22.375539
89.408915	2884.641796	22.380557
89.187781	2892.462644	22.385575
89.066234	2892.171287	22.390592
89.289741	2890.898539	22.395610
89.263305	2891.504816	22.400627
89.463325	2908.964763	22.405645
89.961750	2920.759484	22.410663
89.715703	2925.940862	22.415680
89.856593	2922.965684	22.420698
89.558252	2932.334293	22.425715
89.979756	2936.022345	22.430733
90.188824	2955.356373	22.435751
90.016004	2951.663369	22.440768
90.208223	2941.193747	22.445786
90.534949	2952.704277	22.450803
91.018547	2962.166128	22.455821
91.544307	2957.038048	22.460839
91.447807	2942.325730	22.465856
91.587308	2931.601055	22.470874
91.481648	2930.450410	22.475891
91.465803	2924.231170	22.480909
91.405701	2929.101518	22.485927
91.666501	2927.930868	22.490944
91.743212	2924.257265	22.495962
91.816988	2921.214440	22.500979
91.601404	2921.892523	22.505997
91.623896	2916.098038	22.511015
91.588467	2922.061905	22.516032
91.991610	2930.682338	22.521050
91.913668	2943.502205	22.526067
92.204481	2956.643812	22.531085
92.440757	2949.704184	22.536103
91.911670	2947.750701	22.541120
92.397014	2952.029369	22.546138
92.190780	2958.256111	22.551155
92.401089	2958.860277	22.556173
92.505481	2956.174578	22.561191
92.099325	2979.749920	22.566208
92.175890	2977.569587	22.571226
92.448891	2995.757705	22.576243
92.857332	3013.207345	22.581261
93.075743	3011.077976	22.586279
92.680924	3015.564697	22.591296
92.921359	3003.596954	22.596314
92.907689	3009.982836	22.601331
93.107460	3042.772823	22.606349
93.317042	3033.986442	22.611367
93.148788	3051.671179	22.616384
93.290226	3043.736185	22.621402
93.864967	3050.902781	22.626419
93.935278	3065.513161	22.631437
94.136635	3072.051720	22.636455
94.127869	3064.647428	22.641472
94.186938	3056.221722	22.646490
94.214294	3055.778988	22.651507
94.063759	3058.700596	22.656525
94.133225	3071.410780	22.661543
94.417130	3083.258396	22.666560
94.813366	3083.593661	22.671578
94.765695	3089.342691	22.676595
94.844048	3082.864128	22.681613
95.122545	3078.740621	22.686631
95.338208	3094.134074	22.691648
95.639561	3077.641756	22.696666
95.588686	3079.659128	22.701683
95.417812	3074.279991	22.706701
95.793626	3064.855510	22.711719
95.440338	3071.916416	22.716736
95.528897	3063.648821	22.721754
95.639078	3067.778103	22.726771
95.388372	3061.560610	22.731789
95.790456	3064.486570	22.736807
95.674537	3085.870864	22.741824
96.033485	3091.827108	22.746842
95.992607	3092.370426	22.751859
95.917889	3084.720336	22.756877
96.354308	3080.146728	22.761895
95.966319	3107.664040	22.766912
96.671285	3113.426504	22.771930
96.725848	3123.596342	22.776947
96.787016	3127.575080	22.781965
97.099901	3121.280182	22.786983
96.828977	3122.477642	22.792000
96.868667	3123.699758	22.797018
96.993005	3124.507503	22.802035
97.287540	3128.526025	22.807053
97.458121	3140.042418	22.812071
97.216053	3152.215577	22.817088
97.242850	3144.351443	22.822106
97.267030	3153.174382	22.827123
97.442272	3149.678929	22.832141
97.891652	3152.185682	22.837159
97.644795	3173.522051	22.842176
98.022734	3166.609704	22.847194
98.164401	3169.464545	22.852211
98.238026	3173.014475	22.857229
98.365914	3175.440106	22.862247
98.231096	3180.937434	22.867264
98.388761	3177.361416	22.872282
98.394637	3188.795222	22.877299
98.603227	3198.376282	22.882317
99.054628	3199.098097	22.887335
99.155668	3198.635310	22.892352
99.355372	3193.061041	22.897370
99.303136	3191.732260	22.902387
99.290645	3193.787004	22.907405
99.671906	3183.436766	22.912423
99.228653	3200.862396	22.917440
99.442937	3193.868420	22.922458
99.710806	3194.092226	22.927475
99.712111	3196.232878	22.932493
99.957009	3201.685579	22.937511
99.981146	3215.662009	22.942528
100.030311	3220.657304	22.947546
99.783500	3236.830850	22.952563
99.939130	3231.252827	22.957581
100.118049	3217.419918	22.962599
100.232558	3228.352740	22.967616
100.279813	3233.061746	22.972634
100.900305	3230.095053	22.977651
100.460611	3243.078091	22.982669
101.428245	3225.829861	22.987687
101.588446	3227.639936	22.992704
101.506133	3231.811305	22.997722
101.876081	3217.619670	23.002739
101.794197	3217.325296	23.007757
101.722452	3194.035572	23.012775
101.785393	3192.469260	23.017792
101.546993	3187.945319	23.022810
101.728417	3180.496158	23.027827
101.445349	3187.678976	23.032845
101.460510	3180.275005	23.037863
101.509061	3203.373196	23.042880
101.565489	3214.535680	23.047898
101.833186	3222.657802	23.052915
101.885460	3220.080274	23.057933
101.689733	3224.680218	23.062951
102.389044	3244.772563	23.067968
102.392640	3251.391120	23.072986
102.474780	3253.491652	23.078003
102.010417	3256.460429	23.083021
102.682286	3258.981617	23.088039
102.546230	3279.388024	23.093056
102.685709	3282.066479	23.098074
103.087140	3272.332919	23.103091
102.824224	3282.689965	23.108109
103.123045	3297.403747	23.113127
103.084725	3318.875146	23.118144
103.106627	3308.571214	23.123162
103.273248	3306.062571	23.128179
103.029004	3330.741992	23.133197
103.355252	3339.200559	23.138215
103.512779	3337.749310	23.143232
103.736846	3342.335826	23.148250
103.909881	3368.590040	23.153267
104.228875	3369.279413	23.158285
104.223198	3376.909391	23.163303
104.264073	3376.976222	23.168320
104.440985	3375.095391	23.173338
104.675048	3385.528258	23.178355
104.753865	3392.982078	23.183373
105.232921	3383.949791	23.188391
105.386160	3389.951952	23.193408
105.490887	3393.132228	23.198426
105.826706	3387.414927	23.203443
105.516920	3378.778737	23.208461
105.649287	3377.608018	23.213479
105.768628	3381.543745	23.218496
105.677842	3387.102373	23.223514
105.676083	3375.120428	23.228531
105.720699	3389.554651	23.233549
105.826878	3374.951738	23.238567
106.026850	3377.570213	23.243584
106.000731	3383.734685	23.248602
106.180181	3387.553002	23.253619
106.120479	3405.802092	23.258637
106.352837	3410.553399	23.263655
106.059218	3409.858183	23.268672
106.349701	3412.091238	23.273690
106.668466	3422.355803	23.278707
106.489829	3427.767546	23.283725
106.518085	3432.960458	23.288743
106.520271	3439.172637	23.293760
106.742669	3464.103506	23.298778
106.835542	3465.210562	23.303795
106.990237	3472.507395	23.308813
107.400906	3479.325714	23.313831
107.937823	3495.534986	23.318848
107.847553	3496.492386	23.323866
108.220389	3485.898458	23.328883
108.057925	3476.661493	23.333901
108.137542	3481.317195	23.338919
108.665619	3485.482259	23.343936
108.322600	3483.302683	23.348954
108.845696	3480.705582	23.353971
108.881303	3480.167772	23.358989
108.903089	3473.220441	23.364007
108.606971	3477.578386	23.369024
108.329650	3482.715509	23.374042
108.775442	3469.396153	23.379059
108.883870	3491.460470	23.384077
108.984220	3496.504876	23.389095
109.087636	3496.586964	23.394112
108.757588	3516.416289	23.399130
109.117662	3503.853588	23.404147
109.149764	3519.758506	23.409165
109.308939	3532.357000	23.414183
109.466131	3537.464862	23.419200
109.448628	3533.436210	23.424218
109.834422	3551.874456	23.429235
109.821231	3562.301841	23.434253
110.206275	3563.113775	23.439271
110.355278	3560.593830	23.444288
110.369024	3563.921459	23.449306
110.330953	3554.482789	23.454323
110.538753	3572.917007	23.459341
110.395386	3576.085953	23.464359
110.598809	3589.067735	23.469376
110.836134	3605.067570	23.474394
111.085193	3592.792829	23.479411
110.830501	3604.345588	23.484429
111.472631	3623.675428	23.489447
111.439935	3625.174508	23.494464
111.813562	3624.207608	23.499482
111.868775	3621.316927	23.504499
112.056788	3620.121247	23.509517
112.308457	3611.846487	23.514535
112.452426	3612.504557	23.519552
111.972576	3620.768129	23.524570
112.292132	3613.632554	23.529587
112.049142	3602.045809	23.534605
112.272995	3617.787645	23.539623
112.669920	3632.409944	23.544640
112.337834	3644.184185	23.549658
112.710988	3631.533392	23.554675
112.740894	3646.313595	23.559693
112.809190	3644.909346	23.564711
113.014193	3663.770123	23.569728
112.644533	3679.043157	23.574746
113.314616	3661.757001	23.579763
113.505432	3661.723860	23.584781
113.540074	3662.014165	23.589799
113.852494	3679.052861	23.594816
113.718641	3685.611637	23.599834
113.812883	3674.154550	23.604851
113.910539	3693.145700	23.609869
113.951145	3698.075240	23.614887
114.138195	3689.755998	23.619904
114.240848	3701.494272	23.624922
114.522242	3709.568324	23.629939
114.624057	3716.534241	23.634957
114.881100	3714.435402	23.639975
114.927866	3701.444385	23.644992
115.027370	3697.282575	23.650010
115.882505	3692.865197	23.655027
115.734849	3699.027829	23.660045
115.428385	3699.322924	23.665063
115.848754	3685.115447	23.670080
115.534232	3693.802138	23.675098
115.817126	3700.879467	23.680115
115.643802	3701.088782	23.685133
115.744046	3699.622555	23.690151
116.217601	3708.513291	23.695168
115.994610	3726.725958	23.700186
116.275136	3724.669694	23.705203
116.530270	3724.831046	23.710221
116.226776	3737.798288	23.715239
116.659096	3725.204181	23.720256
116.541202	3719.984176	23.725274
116.431958	3733.781141	23.730291
116.779473	3730.412213	23.735309
116.832756	3745.396525	23.740327
116.831297	3754.905944	23.745344
116.977185	3748.846266	23.750362
116.720842	3754.298915	23.755379
117.236906	3765.894910	23.760397
117.397781	3774.340885	23.765415
117.577166	3770.960752	23.770432
117.752484	3785.830055	23.775450
117.563520	3787.786082	23.780467
117.367793	3789.495978	23.785485
117.305891	3819.341419	23.790503
117.762118	3826.506703	23.795520
117.828642	3828.743361	23.800538
117.916950	3832.642598	23.805555
118.420691	3834.607794	23.810573
118.551047	3860.671464	23.815591
118.869818	3865.875967	23.820608
118.817048	3868.209116	23.825626
119.115666	3861.330438	23.830643
119.411751	3861.153128	23.835661
119.019029	3863.640089	23.840679
119.443133	3887.041422	23.845696
119.723604	3893.983410	23.850714
119.877691	3886.319133	23.855731
120.077542	3884.376577	23.860749
119.670356	3884.921394	23.865767
119.849306	3891.429357	23.870784
119.944151	3896.874420	23.875802
120.283860	3907.570505	23.880819
120.631787	3911.224889	23.885837
120.237897	3913.567952	23.890855
120.664599	3913.318664	23.895872
120.637254	3933.743006	23.900890
120.622216	3926.294850	23.905907
120.801177	3937.557689	23.910925
121.044957	3948.888962	23.915943
120.790083	3939.703212	23.920960
120.834954	3960.119987	23.925978
121.402767	3971.887119	23.930995
121.572448	3965.724211	23.936013
121.790135	3976.517673	23.941031
122.071938	3993.533820	23.946048
122.200622	3998.281179	23.951066
122.033275	4000.873839	23.956083
122.606591	3996.358846	23.961101
122.451333	4006.714331	23.966119
122.732149	3999.466475	23.971136
122.825528	3999.184071	23.976154
122.464672	3993.450559	23.981171
122.869228	4003.865120	23.986189
122.719268	4019.870320	23.991207
122.986900	4021.465880	23.996224
123.107483	4033.399875	24.001242
123.210537	4033.089099	24.006259
123.451112	4035.605306	24.011277
123.629583	4055.248922	24.016295
123.908205	4053.871303	24.021312
123.724009	4050.502761	24.026330
123.756906	4055.984495	24.031347
123.485911	4056.585950	24.036365
124.079422	4073.960930	24.041383
123.984840	4083.982413	24.046400
124.271305	4081.537313	24.051418
124.009467	4075.897256	24.056435
124.421522	4092.449058	24.061453
124.456881	4112.966428	24.066471
124.609046	4112.991250	24.071488
124.781091	4108.340948	24.076506
124.771646	4115.954981	24.081523
125.217393	4128.852684	24.086541
125.432825	4137.981208	24.091559
125.750127	4133.663604	24.096576
125.620663	4132.604207	24.101594
125.903051	4137.295501	24.106611
126.189830	4134.379061	24.111629
126.030015	4128.414634	24.116647
126.196937	4142.978566	24.121664
126.185070	4152.037172	24.126682
126.238820	4155.185476	24.131699
126.562891	4149.202898	24.136717
126.689361	4155.083790	24.141735
126.715900	4155.569547	24.146752
126.845151	4165.506063	24.151770
126.788747	4191.789737	24.156787
127.026029	4183.083176	24.161805
127.097464	4189.972038	24.166823
127.296935	4198.159492	24.171840
127.486634	4203.024791	24.176858
127.630999	4215.190439	24.181875
127.637118	4208.764291	24.186893
127.877261	4203.039667	24.191911
127.858314	4216.463460	24.196928
128.009671	4235.211742	24.201946
127.979174	4256.910712	24.206963
128.339746	4250.018477	24.211981
128.250083	4255.127994	24.216999
128.555693	4267.898961	24.222016
128.831507	4256.793353	24.227034
128.540995	4275.821793	24.232051
129.374534	4268.610049	24.237069
129.242250	4285.496502	24.242087
129.517038	4291.851389	24.247104
129.636901	4279.120268	24.252122
129.419746	4286.238363	24.257139
129.792096	4268.820411	24.262157
129.748972	4287.068188	24.267175
129.878178	4297.713887	24.272192
130.314981	4297.466469	24.277210
130.208754	4307.632152	24.282227
130.432237	4296.620600	24.287245
130.404647	4313.915792	24.292263
130.190953	4320.558109	24.297280
130.687543	4325.148709	24.302298
130.816664	4343.875992	24.307315
131.044238	4332.709399	24.312333
130.993029	4352.074396	24.317351
130.960411	4351.541136	24.322368
131.585776	4373.177568	24.327386
131.588203	4372.346768	24.332403
131.337403	4376.046255	24.337421
131.875612	4385.968096	24.342439
131.961147	4386.446868	24.347456
132.390225	4381.689049	24.352474
132.394449	4386.723643	24.357491
132.688242	4371.925794	24.362509
132.567346	4384.594487	24.367527
132.440479	4385.954073	24.372544
132.985474	4398.959231	24.377562
132.953170	4419.579135	24.382579
133.068750	4412.705262	24.387597
133.219583	4414.124876	24.392615
133.271422	4410.629847	24.397632
133.422184	4415.656774	24.402650
133.259079	4414.667092	24.407667
133.388719	4409.709515	24.412685
133.595656	4437.769884	24.417703
133.680760	4441.128432	24.422720
133.778710	4444.745110	24.427738
133.672372	4449.987768	24.432755
134.080827	4465.669251	24.437773
134.166273	4479.644167	24.442791
134.380240	4479.559560	24.447808
134.472952	4493.338787	24.452826
134.782253	4502.125617	24.457843
135.290939	4490.636066	24.462861
135.224183	4493.158245	24.467879
135.160391	4503.913933	24.472896
135.870014	4490.473340	24.477914
135.640553	4488.233513	24.482931
135.970789	4493.293806	24.487949
135.821921	4506.990908	24.492967
136.195367	4517.197949	24.497984
136.454461	4516.813740	24.503002
136.421256	4502.536365	24.508019
136.813087	4500.156867	24.513037
137.022391	4503.008654	24.518055
136.926586	4500.558934	24.523072
137.425314	4501.940365	24.528090
137.058776	4510.811310	24.533107
137.402961	4501.739247	24.538125
137.126218	4511.015856	24.543143
137.196468	4506.665739	24.548160
137.416615	4519.171882	24.553178
137.097733	4546.173979	24.558195
137.405435	4547.847232	24.563213
137.436696	4551.996250	24.568231
137.604762	4573.114781	24.573248
137.776981	4568.539122	24.578266
137.784547	4579.643332	24.583283
138.184826	4587.053665	24.588301
138.207692	4591.515913	24.593319
138.108212	4615.627738	24.598336
138.656624	4619.350353	24.603354
138.599838	4622.033515	24.608371
138.580669	4634.200921	24.613389
138.805021	4652.109236	24.618407
139.280014	4665.921914	24.623424
139.818903	4658.313371	24.628442
139.470570	4684.761869	24.633459
139.802449	4669.214082	24.638477
140.129596	4682.150348	24.643495
139.879613	4676.639619	24.648512
140.167282	4676.229817	24.653530
140.210993	4708.274244	24.658547
140.312988	4707.359646	24.663565
140.417402	4712.638835	24.668583
140.748193	4721.328530	24.673600
140.994643	4717.209497	24.678618
141.161249	4728.141459	24.683635
141.476927	4720.922946	24.688653
141.389911	4736.007383	24.693671
141.434865	4737.860304	24.698688
141.711272	4738.294555	24.703706
141.548180	4758.266778	24.708723
141.824686	4764.595589	24.713741
141.815008	4770.653948	24.718759
141.873735	4772.950697	24.723776
142.460212	4772.775795	24.728794
142.429226	4791.397382	24.733811
142.552691	4781.175309	24.738829
142.742662	4788.516937	24.743847
142.341823	4794.629307	24.748864
143.049155	4804.111233	24.753882
142.712806	4818.117168	24.758899
142.937506	4812.602766	24.763917
143.434325	4818.495555	24.768935
143.800647	4820.119386	24.773952
144.139194	4828.199933	24.778970
144.175128	4825.270086	24.783987
144.346489	4827.412394	24.789005
144.643184	4820.019004	24.794023
144.617678	4822.702151	24.799040
144.815421	4817.318590	24.804058
144.845499	4816.899769	24.809075
145.088084	4815.783967	24.814093
145.179148	4816.483118	24.819111
145.316007	4824.143013	24.824128
145.532550	4808.088510	24.829146
145.541806	4814.406378	24.834163
145.652543	4820.609834	24.839181
145.913239	4829.590330	24.844199
145.908001	4841.963881	24.849216
146.239394	4851.346917	24.854234
146.068926	4854.814324	24.859251
146.066673	4849.941006	24.864269
146.462110	4845.632740	24.869287
146.043345	4860.758333	24.874304
146.500252	4865.743089	24.879322
146.206706	4877.553622	24.884339
146.333963	4880.993891	24.889357
146.856378	4903.787545	24.894375
146.528886	4918.996941	24.899392
146.788690	4921.060862	24.904410
147.083017	4941.437310	24.909427
146.962113	4959.828263	24.914445
147.637258	4971.348480	24.919463
147.412505	4992.804165	24.924480
147.946976	4990.657744	24.929498
147.946023	4993.039590	24.934515
148.052411	4998.518175	24.939533
148.304177	5016.900379	24.944551
148.639269	5025.777348	24.949568
148.574883	5024.701229	24.954586
148.977682	5050.920316	24.959603
148.973983	5055.872175	24.964621
149.121494	5053.439255	24.969639
149.492629	5056.061235	24.974656
149.732878	5064.221146	24.979674
150.017620	5077.497853	24.984691
149.942535	5079.588781	24.989709
150.112880	5082.643983	24.994727
150.011105	5089.863863	24.999744
150.433763	5087.589433	25.004762
150.495829	5104.873048	25.009779
150.627415	5109.075723	25.014797
151.032466	5109.622208	25.019815
151.099537	5109.779217	25.024832
150.984953	5109.366966	25.029850
151.111179	5129.326901	25.034867
151.399904	5127.982171	25.039885
151.689269	5121.534045	25.044903
151.604223	5126.628908	25.049920
151.926732	5141.538183	25.054938
151.854050	5153.348654	25.059955
151.939657	5154.051872	25.064973
152.461576	5148.358701	25.069991
151.952027	5165.814401	25.075008
152.570817	5177.496067	25.080026
152.590889	5191.922235	25.085043
152.601813	5195.395970	25.090061
153.067130	5185.121480	25.095079
152.917152	5211.293970	25.100096
153.514494	5206.806561	25.105114
153.376201	5211.773620	25.110131
153.509982	5212.973661	25.115149
153.760865	5211.074485	25.120167
153.903214	5234.603151	25.125184
153.781676	5245.996519	25.130202
154.071494	5253.818775	25.135219
154.408109	5263.270889	25.140237
154.646657	5269.565229	25.145255
154.578479	5280.274926	25.150272
154.569158	5274.975822	25.155290
154.777001	5288.027985	25.160307
154.878217	5309.303457	25.165325
155.274751	5310.045868	25.170343
154.951820	5316.090835	25.175360
155.213241	5320.497338	25.180378
155.879314	5325.773704	25.185395
155.947386	5322.507707	25.190413
155.906679	5347.265354	25.195431
156.227228	5356.569769	25.200448
156.125591	5355.940385	25.205466
156.406513	5357.842984	25.210483
156.740856	5376.152904	25.215501
157.073195	5376.502728	25.220519
157.475352	5377.323358	25.225536
157.609855	5372.660773	25.230554
157.990980	5377.991721	25.235571
158.100946	5376.468215	25.240589
158.160306	5361.589256	25.245607
158.081657	5374.801836	25.250624
158.372802	5391.124577	25.255642
158.705812	5400.961670	25.260659
158.743851	5409.480410	25.265677
158.690900	5394.253397	25.270695
158.922035	5399.700486	25.275712
158.894858	5396.641574	25.280730
158.961017	5395.322572	25.285747
159.076685	5424.290454	25.290765
159.146989	5425.280106	25.295783
159.434877	5428.726243	25.300800
159.355988	5422.894815	25.305818
160.004207	5445.066826	25.310835
159.958726	5450.652957	25.315853
160.293120	5439.308852	25.320871
160.717152	5452.809351	25.325888
160.569881	5438.922062	25.330906
160.850630	5445.870607	25.335923
160.963588	5467.175853	25.340941
161.384941	5457.695952	25.345959
161.235713	5466.814635	25.350976
161.426566	5467.765865	25.355994
161.849175	5466.246605	25.361011
161.749374	5475.237426	25.366029
161.746774	5461.981020	25.371047
161.794050	5485.774623	25.376064
162.037805	5490.240005	25.381082
161.924000	5493.407208	25.386099
161.811831	5509.366343	25.391117
162.149588	5516.475206	25.396135
162.438749	5519.272249	25.401152
162.350086	5525.066355	25.406170
162.905886	5541.898353	25.411187
162.940532	5557.787209	25.416205
163.059713	5555.349837	25.421223
163.402051	5563.157271	25.426240
163.326491	5578.048474	25.431258
163.724077	5567.047821	25.436275
163.839831	5576.166885	25.441293
164.095964	5589.561762	25.446311
164.131625	5596.914305	25.451328
164.299632	5593.671902	25.456346
165.099973	5595.677708	25.461363
164.984267	5599.813487	25.466381
165.083124	5589.995795	25.471399
165.209169	5611.202211	25.476416
165.105967	5619.616827	25.481434
165.329844	5616.667197	25.486451
165.503429	5626.609526	25.491469
165.698896	5629.165736	25.496487
165.892609	5650.288968	25.501504
165.954392	5648.922236	25.506522
166.255677	5645.767658	25.511539
166.000402	5667.302547	25.516557
166.226294	5666.393411	25.521575
166.451013	5675.215356	25.526592
166.810419	5689.624502	25.531610
167.363021	5692.554057	25.536627
167.172820	5700.752350	25.541645
167.312802	5696.390382	25.546663
167.586199	5706.542679	25.551680
167.893157	5717.067838	25.556698
168.291586	5720.395367	25.561715
168.050788	5724.445534	25.566733
168.388784	5719.759067	25.571751
168.518795	5749.594597	25.576768
168.822306	5752.618872	25.581786
168.836369	5757.383345	25.586803
168.732962	5772.149787	25.591821
169.084848	5774.098201	25.596839
169.308158	5784.425779	25.601856
169.255026	5786.965602	25.606874
169.606277	5782.560433	25.611891
169.486204	5806.669618	25.616909
169.648590	5806.862468	25.621927
170.031240	5814.379860	25.626944
170.181005	5835.604712	25.631962
170.338164	5844.353257	25.636979
170.424982	5849.280566	25.641997
170.292547	5870.167782	25.647015
170.877226	5885.599497	25.652032
170.537615	5895.872893	25.657050
170.997879	5909.557200	25.662067
170.956796	5914.521413	25.667085
171.355158	5935.460404	25.672103
171.719502	5946.221550	25.677120
171.442663	5952.693464	25.682138
171.998314	5961.527436	25.687156
172.122975	5956.205177	25.692173
172.187622	5982.000916	25.697191
172.560295	6001.144740	25.702208
172.478704	5987.307933	25.707226
172.561223	6014.022966	25.712244
172.958420	6027.825689	25.717261
172.947677	6035.813766	25.722279
173.736097	6058.810866	25.727296
173.783311	6071.251536	25.732314
173.924036	6062.591391	25.737332
173.992525	6057.431947	25.742349
174.648795	6080.859644	25.747367
174.974789	6070.517427	25.752384
174.838305	6084.170545	25.757402
174.360927	6079.504504	25.762420
174.469379	6089.199971	25.767437
175.237803	6103.052465	25.772455
175.241021	6112.477098	25.777472
175.208142	6123.461505	25.782490
175.727293	6106.804403	25.787508
175.430480	6126.666974	25.792525
175.830879	6134.357209	25.797543
176.137665	6135.302714	25.802560
176.059871	6155.798539	25.807578
176.482655	6155.026164	25.812596
176.609249	6164.598188	25.817613
176.806421	6171.591974	25.822631
176.725259	6174.282185	25.827648
176.912759	6198.476607	25.832666
177.033844	6199.851293	25.837684
177.505921	6204.574089	25.842701
177.833567	6226.417435	25.847719
177.911955	6218.989764	25.852736
178.060217	6241.230550	25.857754
178.509025	6246.853425	25.862772
178.811101	6250.171000	25.867789
178.685052	6257.236343	25.872807
179.192922	6244.006764	25.877824
178.925031	6246.764854	25.882842
179.047090	6267.347509	25.887860
179.303962	6278.705485	25.892877
179.110291	6291.823252	25.897895
179.674298	6303.625863	25.902912
179.810815	6312.484398	25.907930
179.768637	6302.559620	25.912948
180.273679	6328.936823	25.917965
180.703223	6341.483858	25.922983
181.195288	6335.346297	25.928000
180.987100	6343.729425	25.933018
180.878322	6330.033054	25.938036
181.181407	6349.646365	25.943053
181.255001	6350.439041	25.948071
181.747993	6352.445332	25.953088
181.644845	6370.627091	25.958106
181.808374	6378.014789	25.963124
182.126668	6400.676608	25.968141
182.046228	6406.724058	25.973159
182.348463	6412.992586	25.978176
182.223802	6412.542193	25.983194
182.485960	6422.580255	25.988212
182.937693	6447.652835	25.993229
182.928878	6455.264357	25.998247
183.540982	6455.622327	26.003264
183.202965	6487.304640	26.008282
183.451655	6487.843152	26.013300
183.727384	6483.687322	26.018317
184.320708	6515.048060	26.023335
184.371828	6513.622767	26.028352
184.552611	6505.690548	26.033370
184.740655	6505.846879	26.038388
185.038542	6522.212608	26.043405
185.011940	6531.002137	26.048423
185.378701	6533.694005	26.053440
185.355096	6536.669313	26.058458
185.540618	6559.103644	26.063476
185.652133	6570.215716	26.068493
185.486700	6574.902200	26.073511
186.237034	6581.880377	26.078528
186.280204	6592.182335	26.083546
186.360793	6598.288308	26.088564
186.777806	6590.074446	26.093581
187.564197	6600.658415	26.098599
187.809585	6593.799944	26.103616
187.628326	6595.096249	26.108634
187.307138	6596.814967	26.113652
187.707310	6602.347561	26.118669
187.748966	6606.670638	26.123687
188.209424	6608.045204	26.128704
187.959968	6622.623147	26.133722
187.901896	6621.502558	26.138740
187.898462	6636.552564	26.143757
187.890264	6664.230338	26.148775
188.552701	6673.310906	26.153792
188.443219	6687.718506	26.158810
188.219650	6704.118604	26.163828
188.937510	6734.546418	26.168845
189.038219	6737.216913	26.173863
189.213101	6756.688102	26.178880
189.418282	6779.254173	26.183898
189.799411	6798.373946	26.188916
190.187376	6803.638494	26.193933
190.373832	6814.166582	26.198951
190.901852	6823.916827	26.203968
191.378424	6830.483560	26.208986
191.552790	6835.467595	26.214004
191.561608	6834.817932	26.219021
191.427401	6854.865621	26.224039
191.862037	6854.970187	26.229056
192.138930	6857.026427	26.234074
192.055336	6853.526062	26.239092
192.755339	6857.897158	26.244109
192.775878	6879.581873	26.249127
193.086058	6874.798067	26.254144
193.107405	6873.302055	26.259162
193.187012	6871.037985	26.264180
193.699531	6888.379875	26.269197
193.916660	6897.942112	26.274215
193.803544	6903.849450	26.279232
193.796640	6910.475622	26.284250
194.057564	6926.868357	26.289268
194.531446	6922.886017	26.294285
194.484082	6930.038682	26.299303
194.645695	6939.077717	26.304320
194.662751	6955.220947	26.309338
194.990054	6968.092532	26.314356
195.098997	6977.384440	26.319373
195.048944	6982.564692	26.324391
195.534109	7003.812099	26.329408
195.941972	7011.723631	26.334426
195.837846	7024.373566	26.339444
196.156803	7024.757149	26.344461
196.295811	7037.818206	26.349479
196.385242	7057.900872	26.354496
196.560221	7060.692252	26.359514
196.792688	7079.477794	26.364532
197.100090	7085.278703	26.369549
197.006733	7095.294027	26.374567
197.453347	7100.183547	26.379584
197.645136	7115.691632	26.384602
197.580369	7133.936448	26.389620
198.036762	7139.923046	26.394637
198.262156	7144.608917	26.399655
198.796838	7161.170100	26.404672
198.815091	7167.545709	26.409690
198.810336	7184.279529	26.414708
199.526552	7185.450436	26.419725
199.588385	7199.619912	26.424743
199.533948	7190.758268	26.429760
199.910902	7200.331299	26.434778
200.258959	7207.866894	26.439796
200.379421	7207.029437	26.444813
200.103567	7234.848521	26.449831
200.181019	7236.490414	26.454848
200.448386	7244.727712	26.459866
200.297228	7269.764963	26.464884
200.624715	7277.284300	26.469901
200.661941	7297.234917	26.474919
201.246588	7297.292651	26.479936
201.256545	7316.238103	26.484954
201.509878	7327.603724	26.489972
202.116383	7337.505143	26.494989
202.319753	7346.930522	26.500007
202.970443	7333.485053	26.505024
202.835600	7351.301434	26.510042
202.976576	7372.847213	26.515060
202.979931	7368.382525	26.520077
203.260608	7383.828144	26.525095
203.501833	7386.813413	26.530112
204.209935	7399.673628	26.535130
204.717158	7398.044519	26.540148
204.828996	7385.458308	26.545165
204.778748	7391.247539	26.550183
204.749449	7388.527256	26.555200
204.987222	7413.930503	26.560218
205.125439	7420.565991	26.565236
205.365905	7406.248634	26.570253
205.233183	7431.668232	26.575271
205.641517	7445.586929	26.580288
205.782037	7457.007512	26.585306
205.949063	7475.999664	26.590324
206.037788	7492.070169	26.595341
205.799027	7501.223722	26.600359
206.256294	7525.650485	26.605376
206.438655	7526.182667	26.610394
206.452442	7561.602110	26.615412
206.953901	7563.944260	26.620429
207.101204	7575.272445	26.625447
206.991823	7586.646200	26.630464
207.319562	7606.531880	26.635482
207.857656	7634.199067	26.640500
207.928876	7631.288072	26.645517
208.064587	7661.772911	26.650535
208.666298	7660.836227	26.655552
209.353097	7657.318661	26.660570
209.546149	7664.888750	26.665588
210.062923	7680.318492	26.670605
210.177283	7687.784239	26.675623
210.409835	7690.559919	26.680640
210.656928	7675.442585	26.685658
210.363883	7679.639318	26.690676
210.526008	7672.651582	26.695693
210.646369	7693.937355	26.700711
210.745125	7710.726303	26.705728
211.405725	7710.639173	26.710746
210.850090	7735.273784	26.715764
211.455753	7737.276610	26.720781
211.757993	7761.443449	26.725799
211.837616	7778.261620	26.730816
212.137523	7780.505573	26.735834
211.844774	7786.795771	26.740852
212.013794	7789.730825	26.745869
212.393303	7808.206248	26.750887
212.732800	7824.934275	26.755904
213.093276	7833.107665	26.760922
213.280440	7848.332117	26.765940
213.570863	7865.268350	26.770957
213.596569	7862.582216	26.775975
213.692654	7875.146981	26.780992
214.199036	7887.565991	26.786010
213.949448	7916.287696	26.791028
214.363204	7912.477298	26.796045
214.558876	7925.953470	26.801063
214.810788	7947.777850	26.806080
215.050136	7949.815236	26.811098
214.972454	7969.480876	26.816116
215.428342	7978.852310	26.821133
216.048049	7984.106535	26.826151
215.971352	7979.048428	26.831168
216.685905	8003.538965	26.836186
216.694093	8017.848784	26.841204
216.984308	8007.741206	26.846221
217.218111	8015.637897	26.851239
217.172350	8034.673754	26.856256
217.404348	8040.533158	26.861274
217.775410	8055.915669	26.866292
217.874248	8070.358633	26.871309
217.875807	8077.528149	26.876327
218.172875	8092.046286	26.881344
218.493062	8091.905133	26.886362
218.459064	8109.983739	26.891380
218.582791	8123.634218	26.896397
219.226374	8130.603166	26.901415
219.305661	8140.299202	26.906432
219.627483	8153.278205	26.911450
219.709245	8167.499603	26.916468
219.888691	8168.334743	26.921485
219.948443	8186.943779	26.926503
220.283760	8204.300645	26.931520
220.442716	8222.816144	26.936538
220.516698	8225.276283	26.941556
220.887924	8259.833263	26.946573
220.971223	8268.226744	26.951591
221.068352	8289.081591	26.956608
221.454278	8294.050038	26.961626
221.309157	8323.916994	26.966644
221.484602	8337.818247	26.971661
222.121424	8350.592565	26.976679
222.283516	8380.271818	26.981696
222.691222	8387.887128	26.986714
222.801832	8405.823244	26.991732
222.931472	8413.383690	26.996749
223.340783	8438.620827	27.001767
223.436070	8458.450681	27.006784
224.236221	8477.419770	27.011802
224.498743	8477.783575	27.016820
224.609153	8481.383769	27.021837
224.963241	8497.366554	27.026855
224.941097	8513.079915	27.031872
225.406750	8506.107826	27.036890
225.596898	8528.928567	27.041908
225.665436	8532.319873	27.046925
225.976660	8527.321947	27.051943
225.681679	8551.278330	27.056960
226.122329	8558.322744	27.061978
226.406732	8574.869267	27.066996
226.996554	8577.092216	27.072013
227.112107	8596.454177	27.077031
227.018031	8623.446188	27.082048
227.506314	8615.931555	27.087066
227.831700	8623.536163	27.092084
228.069829	8646.864275	27.097101
228.121347	8660.132529	27.102119
228.059036	8663.502160	27.107136
228.518042	8682.527861	27.112154
228.728401	8684.916704	27.117172
228.908541	8698.082610	27.122189
229.443089	8718.185997	27.127207
229.243133	8727.690654	27.132224
229.635380	8718.972536	27.137242
230.045702	8747.797808	27.142260
229.864303	8751.463604	27.147277
230.301275	8753.913475	27.152295
230.282397	8776.134249	27.157312
230.667697	8769.990557	27.162330
230.833360	8795.545778	27.167348
230.992822	8810.129056	27.172365
231.438771	8823.489025	27.177383
231.341222	8847.147788	27.182400
231.993536	8856.561333	27.187418
232.077596	8876.541646	27.192436
232.164911	8873.129957	27.197453
232.682782	8893.374165	27.202471
232.473964	8905.160703	27.207488
232.720192	8922.593727	27.212506
232.970276	8935.458410	27.217524
233.274011	8951.694940	27.222541
233.940612	8960.479198	27.227559
234.394800	8969.961778	27.232576
234.834564	8986.979300	27.237594
234.776499	8989.640965	27.242612
234.853321	8991.309139	27.247629
235.259330	9000.909185	27.252647
235.677337	9008.882276	27.257664
235.883743	9014.727366	27.262682
236.011868	9024.600978	27.267700
235.986212	9038.312371	27.272717
236.622524	9042.716669	27.277735
236.449533	9052.092610	27.282752
236.516146	9059.998542	27.287770
236.847629	9076.217225	27.292788
236.826595	9087.701123	27.297805
237.465842	9106.441557	27.302823
237.526368	9125.164203	27.307840
237.682056	9134.653666	27.312858
237.570609	9159.630622	27.317876
237.494992	9168.833794	27.322893
238.330681	9199.313852	27.327911
238.414987	9211.606718	27.332928
238.633332	9242.654379	27.337946
238.878532	9255.612288	27.342964
238.739369	9272.294899	27.347981
239.167167	9284.225446	27.352999
239.410451	9312.501175	27.358016
239.902192	9327.812997	27.363034
240.337003	9357.450592	27.368052
240.497232	9367.384491	27.373069
240.822080	9378.709051	27.378087
240.741644	9405.397658	27.383104
241.262493	9417.990353	27.388122
241.663821	9419.428513	27.393140
242.059815	9435.635329	27.398157
242.843039	9453.338618	27.403175
242.647303	9453.878199	27.408192
242.970482	9473.467653	27.413210
243.237034	9484.958673	27.418228
243.217858	9491.079883	27.423245
243.681551	9497.341874	27.428263
243.782287	9515.620373	27.433280
244.110370	9520.780725	27.438298
244.291285	9529.615613	27.443316
244.447680	9549.503686	27.448333
244.752875	9542.235490	27.453351
244.763967	9559.152730	27.458368
245.094791	9566.528460	27.463386
245.401693	9585.322795	27.468404
245.160020	9595.620203	27.473421
245.457369	9609.155051	27.478439
245.958972	9620.056727	27.483456
246.126963	9634.789805	27.488474
246.472952	9655.798317	27.493492
246.435581	9668.478712	27.498509
246.829856	9691.446207	27.503527
246.882751	9711.550873	27.508544
247.071247	9719.408637	27.513562
247.548241	9733.545657	27.518580
247.736085	9740.164466	27.523597
248.576633	9751.269391	27.528615
248.819541	9762.948844	27.533632
249.093963	9755.846329	27.538650
249.432837	9770.455987	27.543668
249.487262	9783.468689	27.548685
249.730587	9791.336336	27.553703
249.988770	9801.838021	27.558720
250.439863	9806.530721	27.563738
250.859605	9810.661446	27.568756
250.525052	9803.791860	27.573773
251.025562	9832.289899	27.578791
250.704716	9842.847891	27.583808
251.165418	9859.723463	27.588826
251.551021	9874.839090	27.593844
251.257242	9899.771707	27.598861
251.708789	9918.105351	27.603879
251.807114	9938.454081	27.608896
251.986820	9956.456151	27.613914
252.227583	9973.622617	27.618932
252.710274	9990.927944	27.623949
252.989685	10008.745814	27.628967
252.832218	10036.273741	27.633984
253.060602	10048.641915	27.639002
253.587816	10068.522935	27.644020
253.846237	10107.639897	27.649037
254.540481	10121.145055	27.654055
254.719324	10146.189814	27.659072
255.011196	10160.091544	27.664090
255.494909	10168.541185	27.669108
255.460082	10188.506548	27.674125
255.937377	10199.360649	27.679143
255.666932	10215.665763	27.684160
256.136031	10236.074925	27.689178
256.783617	10247.711507	27.694196
256.738532	10269.211606	27.699213
256.936838	10274.957669	27.704231
257.297411	10293.959026	27.709248
257.781169	10305.532915	27.714266
258.255469	10324.119284	27.719284
258.074056	10329.350687	27.724301
258.678680	10344.336832	27.729319
259.134969	10353.927029	27.734336
259.644328	10350.596545	27.739354
259.890941	10352.232084	27.744372
260.200704	10376.285073	27.749389
260.355426	10372.630331	27.754407
260.284933	10373.736119	27.759424
260.150219	10390.337235	27.764442
260.521000	10402.477344	27.769460
260.917385	10419.117571	27.774477
260.832921	10435.025091	27.779495
261.193782	10459.970948	27.784512
261.213074	10480.383842	27.789530
261.802748	10484.615072	27.794548
261.892787	10512.752820	27.799565
262.048827	10519.518215	27.804583
262.005439	10542.585241	27.809600
261.952313	10562.579302	27.814618
262.508015	10582.316037	27.819636
262.709992	10604.157829	27.824653
263.054617	10626.968658	27.829671
263.290703	10647.745340	27.834688
263.445007	10670.194582	27.839706
264.211283	10684.131829	27.844724
263.897001	10711.764811	27.849741
264.248789	10724.046161	27.854759
264.881507	10736.292923	27.859776
265.314031	10753.586886	27.864794
265.789327	10771.333856	27.869812
265.683465	10776.047176	27.874829
266.327854	10792.903631	27.879847
266.714664	10795.106091	27.884864
266.710064	10801.422335	27.889882
267.342660	10813.233542	27.894900
267.583627	10820.894118	27.899917
267.938682	10847.656555	27.904935
268.024074	10849.417253	27.909952
268.236390	10871.520817	27.914970
268.805737	10875.074091	27.919988
268.911240	10883.290397	27.925005
268.804609	10909.220915	27.930023
269.223859	10910.987120	27.935040
269.462180	10949.084570	27.940058
269.785945	10949.406811	27.945076
269.719151	10970.369449	27.950093
270.141123	10990.617992	27.955111
270.801791	11006.395094	27.960128
270.754761	11022.244230	27.965146
271.097901	11028.867854	27.970164
271.012851	11060.619090	27.975181
271.436120	11076.996383	27.980199
271.651439	11092.012101	27.985216
271.830838	11119.110459	27.990234
272.428126	11124.916957	27.995252
272.567053	11154.761968	28.000269
273.303449	11167.875040	28.005287
273.028852	11180.879427	28.010304
273.228009	11211.153389	28.015322
273.570594	11222.765449	28.020340
273.751853	11252.142793	28.025357
274.272948	11263.890038	28.030375
274.292428	11286.887087	28.035392
274.358724	11314.400719	28.040410
274.990304	11325.887905	28.045428
275.201660	11356.783270	28.050445
275.422964	11372.608114	28.055463
275.720848	11394.333512	28.060480
276.052275	11421.586093	28.065498
276.595078	11427.515147	28.070516
276.911746	11444.341352	28.075533
277.452320	11450.149462	28.080551
278.269512	11451.987849	28.085568
278.779696	11447.498157	28.090586
279.313104	11445.071023	28.095604
279.318546	11454.000567	28.100621
279.655826	11452.975815	28.105639
279.866705	11448.630108	28.110656
279.795626	11458.887919	28.115674
280.101935	11466.587641	28.120692
280.380460	11487.731818	28.125709
280.052088	11492.415934	28.130727
280.411044	11496.755670	28.135744
280.193866	11518.252787	28.140762
280.256051	11522.711675	28.145780
280.614550	11548.437967	28.150797
280.795812	11560.314842	28.155815
281.017898	11592.476463	28.160832
281.328832	11608.453747	28.165850
281.519259	11630.639966	28.170868
281.750654	11658.568871	28.175885
282.113461	11683.503708	28.180903
282.533674	11695.644512	28.185920
282.868238	11731.219530	28.190938
283.095972	11748.779232	28.195956
283.537110	11769.333629	28.200973
283.465156	11790.147715	28.205991
284.002739	11809.435966	28.211008
283.972002	11834.977286	28.216026
284.292787	11854.822157	28.221044
284.530541	11882.991473	28.226061
285.059332	11896.821696	28.231079
285.620829	11918.727206	28.236096
285.717810	11947.196417	28.241114
286.320401	11959.373467	28.246132
286.549754	11982.764625	28.251149
286.940196	12010.739557	28.256167
287.388967	12017.834593	28.261184
287.702027	12032.200843	28.266202
288.405355	12041.080803	28.271220
288.714206	12050.684564	28.276237
288.715276	12056.369315	28.281255
288.942330	12080.065884	28.286272
289.201067	12082.503187	28.291290
289.614966	12094.686304	28.296308
289.781521	12116.762902	28.301325
289.873045	12131.218626	28.306343
290.665701	12138.171028	28.311360
290.737573	12156.612512	28.316378
290.922387	12178.407285	28.321396
291.136386	12176.041482	28.326413
291.269610	12200.228005	28.331431
291.822798	12206.099698	28.336448
291.844797	12241.843296	28.341466
291.888743	12244.014368	28.346484
292.454644	12279.660313	28.351501
292.550427	12293.712893	28.356519
292.846701	12308.695103	28.361536
292.883173	12330.787183	28.366554
293.691917	12344.907163	28.371572
293.941684	12364.768335	28.376589
294.451464	12382.615391	28.381607
294.791300	12398.462631	28.386624
295.075966	12411.616692	28.391642
295.371997	12425.061965	28.396660
295.381952	12449.762419	28.401677
295.568943	12457.124647	28.406695
295.937025	12480.803233	28.411712
296.082129	12509.283607	28.416730
296.484984	12526.127434	28.421748
297.142718	12522.635703	28.426765
296.993493	12561.179954	28.431783
297.660243	12561.860768	28.436800
298.212308	12588.572287	28.441818
298.375386	12599.375150	28.446836
298.664387	12612.337998	28.451853
298.869987	12628.763868	28.456871
299.225953	12644.384934	28.461888
299.064632	12664.637413	28.466906
299.400760	12681.977747	28.471924
300.514818	12688.236765	28.476941
300.684270	12710.719445	28.481959
301.201438	12704.986590	28.486976
301.009109	12715.860853	28.491994
301.279610	12717.059371	28.497012
301.579504	12736.452610	28.502029
301.236148	12756.450072	28.507047
301.751010	12769.816936	28.512064
302.008592	12793.777384	28.517082
302.574385	12809.264674	28.522100
302.782887	12807.608767	28.527117
302.676308	12841.074368	28.532135
303.316723	12859.084732	28.537152
303.295122	12874.921246	28.542170
303.508547	12904.654770	28.547188
304.047575	12925.995736	28.552205
304.276885	12948.856491	28.557223
304.347248	12970.868999	28.562240
304.641161	13002.198240	28.567258
304.650922	13010.954600	28.572276
305.455260	13046.807091	28.577293
305.775500	13085.694181	28.582311
306.015599	13105.267924	28.587328
306.779708	13124.389543	28.592346
307.094129	13146.305242	28.597364
307.679466	13162.139463	28.602381
307.736791	13183.848717	28.607399
308.225141	13205.575034	28.612416
308.254830	13228.081523	28.617434
307.999458	13250.715502	28.622452
308.534518	13279.684330	28.627469
308.518697	13307.779844	28.632487
308.895825	13330.536353	28.637504
309.575795	13364.120488	28.642522
309.788003	13396.666314	28.647540
310.168927	13413.995306	28.652557
310.226974	13449.259728	28.657575
310.761572	13472.253578	28.662592
311.348246	13482.580496	28.667610
311.525876	13507.020068	28.672628
311.980480	13532.129332	28.677645
312.216158	13555.232565	28.682663
312.580880	13578.966894	28.687680
313.244289	13594.361599	28.692698
312.789078	13618.217261	28.697716
313.105323	13631.975363	28.702733
313.709744	13672.424238	28.707751
314.270029	13695.683627	28.712768
314.691248	13711.841754	28.717786
314.603776	13746.279921	28.722804
315.628225	13745.174602	28.727821
315.779577	13784.917002	28.732839
316.336035	13791.695628	28.737856
316.399593	13808.743400	28.742874
316.635137	13829.511671	28.747892
317.167849	13849.345259	28.752909
317.115722	13867.486920	28.757927
317.329941	13882.672460	28.762944
318.065070	13898.974318	28.767962
318.122728	13931.969075	28.772980
318.258648	13936.185589	28.777997
318.437465	13967.436434	28.783015
318.822332	13976.594642	28.788032
319.281732	14003.705166	28.793050
319.484225	14039.528493	28.798068
319.998399	14047.976734	28.803085
319.623538	14064.383343	28.808103
320.309498	14095.649931	28.813120
321.001080	14115.537967	28.818138
320.932415	14140.903239	28.823156
321.293964	14158.012457	28.828173
321.398493	14188.141381	28.833191
321.629272	14210.407996	28.838208
321.825274	14227.092364	28.843226
322.077585	14259.727847	28.848244
322.724406	14280.572155	28.853261
322.939248	14316.799052	28.858279
323.313475	14338.909772	28.863296
323.906916	14362.936821	28.868314
324.011328	14376.368099	28.873332
324.345079	14402.488331	28.878349
324.871650	14423.704110	28.883367
325.426907	14444.133539	28.888384
325.980816	14464.378837	28.893402
325.926992	14485.725251	28.898420
326.320901	14514.967022	28.903437
326.272560	14531.509265	28.908455
326.717589	14561.001121	28.913472
327.249750	14587.772812	28.918490
327.205526	14607.948482	28.923508
328.117754	14625.406896	28.928525
328.335940	14647.663584	28.933543
328.776943	14673.709800	28.938560
328.982681	14685.848107	28.943578
329.252066	14708.555010	28.948596
329.850148	14730.998046	28.953613
329.949204	14758.601161	28.958631
329.999175	14787.964855	28.963648
330.751034	14802.257139	28.968666
330.586525	14842.582237	28.973684
331.396821	14871.837810	28.978701
331.397072	14895.645308	28.983719
331.819783	14905.790627	28.988736
332.333435	14938.976849	28.993754
332.389323	14966.382575	28.998772
332.761980	14973.072294	29.003789
333.074846	15011.120510	29.008807
333.500919	15034.013158	29.013824
333.720446	15059.663196	29.018842
334.206069	15075.134386	29.023860
334.924488	15093.306134	29.028877
335.351008	15114.574016	29.033895
335.498766	15140.368418	29.038912
336.220687	15153.561214	29.043930
335.587210	15182.129198	29.048948
336.126488	15198.163715	29.053965
336.467499	15231.158418	29.058983
336.700354	15256.365294	29.064000
337.219173	15279.517183	29.069018
337.577058	15312.747234	29.074036
338.005238	15328.007519	29.079053
338.685279	15350.210930	29.084071
338.840001	15384.250070	29.089088
339.574415	15395.097520	29.094106
339.569444	15426.818073	29.099124
340.054125	15435.145835	29.104141
340.603804	15452.004699	29.109159
340.379608	15482.746643	29.114176
340.970074	15486.220249	29.119194
340.981561	15522.305332	29.124212
341.336507	15540.890650	29.129229
341.468175	15554.127700	29.134247
342.029909	15593.177892	29.139264
342.351820	15620.416263	29.144282
342.448499	15645.264844	29.149300
343.217714	15664.878763	29.154317
343.432411	15683.217915	29.159335
343.470522	15714.635620	29.164352
344.152188	15722.628393	29.169370
344.326559	15759.709922	29.174388
344.367942	15772.475075	29.179405
344.943634	15799.947624	29.184423
345.340283	15822.882489	29.189440
345.671396	15841.604472	29.194458
345.780361	15881.601692	29.199476
346.070391	15901.419564	29.204493
346.896243	15920.923571	29.209511
347.080826	15957.505835	29.214528
347.911936	15957.266056	29.219546
347.927495	15989.731347	29.224564
348.413222	16010.845623	29.229581
348.794934	16031.581522	29.234599
348.759195	16055.139758	29.239616
348.920340	16079.781343	29.244634
349.377152	16099.482068	29.249652
349.736671	16116.264288	29.254669
349.933915	16165.837877	29.259687
349.955467	16188.587780	29.264704
350.413414	16228.868623	29.269722
350.454318	16262.428780	29.274740
350.881292	16307.599152	29.279757
351.289985	16330.145026	29.284775
351.938550	16369.868317	29.289792
352.327370	16401.826732	29.294810
352.781671	16434.266129	29.299828
353.380803	16452.069810	29.304845
354.274454	16459.999559	29.309863
355.200705	16481.929002	29.314880
356.237495	16479.078346	29.319898
357.114379	16471.984497	29.324916
357.715956	16465.085860	29.329933
358.372216	16459.108080	29.334951
358.454717	16448.758474	29.339968
358.985954	16452.566749	29.344986
358.583213	16433.682457	29.350004
358.821873	16424.982440	29.355021
359.023473	16417.968649	29.360039
358.829276	16437.941243	29.365056
359.208751	16440.127583	29.370074
359.434241	16460.301957	29.375092
359.847626	16485.009656	29.380109
359.482864	16491.074760	29.385127
359.706940	16514.348017	29.390144
360.267412	16535.343449	29.395162
359.939979	16567.346437	29.400180
360.105451	16589.590837	29.405197
360.838918	16612.532636	29.410215
360.770609	16665.688366	29.415232
360.992674	16685.959726	29.420250
361.282880	16736.451159	29.425268
361.383390	16777.175393	29.430285
361.889868	16813.098009	29.435303
362.203485	16861.885331	29.440320
362.718511	16895.371610	29.445338
363.317803	16929.553293	29.450356
363.908429	16966.357584	29.455373
364.504589	16999.238046	29.460391
364.449500	17031.088189	29.465408
365.252939	17059.212425	29.470426
365.718493	17088.355550	29.475444
365.845455	17113.533917	29.480461
366.148527	17146.776745	29.485479
366.489028	17169.179000	29.490496
366.803383	17209.854792	29.495514
367.044413	17238.037568	29.500532
367.675455	17267.779407	29.505549
368.078107	17289.031995	29.510567
368.317851	17335.093555	29.515584
368.607015	17346.731445	29.520602
369.139446	17384.458886	29.525620
369.461165	17411.120234	29.530637
369.761650	17429.180794	29.535655
369.980145	17473.039606	29.540672
370.409415	17501.752856	29.545690
370.921486	17529.883475	29.550708
370.927643	17558.764445	29.555725
372.010719	17582.775246	29.560743
372.428416	17614.698150	29.565760
373.600759	17624.202760	29.570778
374.346459	17636.350204	29.575796
374.997783	17637.317536	29.580813
375.233670	17627.439929	29.585831
375.267472	17641.512875	29.590848
375.546683	17651.366796	29.595866
375.620288	17677.125422	29.600884
375.316106	17693.605934	29.605901
376.312948	17714.524485	29.610919
376.560874	17738.334595	29.615936
376.991328	17764.962792	29.620954
376.995530	17774.827541	29.625972
376.846329	17808.463236	29.630989
377.037904	17830.687663	29.636007
377.322080	17877.622926	29.641024
377.666216	17923.544364	29.646042
377.661414	17958.518365	29.651060
378.154232	17999.609543	29.656077
378.653091	18038.239325	29.661095
378.943604	18081.312349	29.666112
379.365256	18118.101419	29.671130
379.880414	18166.129507	29.676148
380.566748	18210.609693	29.681165
381.192151	18235.598670	29.686183
381.233673	18274.930328	29.691200
381.683711	18301.214107	29.696218
382.258401	18333.917936	29.701236
382.751476	18372.093916	29.706253
383.500217	18391.804338	29.711271
383.763222	18428.147425	29.716288
384.021096	18458.884637	29.721306
384.175857	18498.037338	29.726324
384.323520	18534.563645	29.731341
384.890736	18571.916054	29.736359
385.188205	18604.149193	29.741376
385.421013	18646.427738	29.746394
386.107214	18685.094288	29.751412
386.536135	18716.954417	29.756429
387.375435	18749.533389	29.761447
387.777282	18782.597682	29.766464
388.124147	18794.474543	29.771482
388.681821	18824.959565	29.776500
388.347997	18856.369036	29.781517
389.037165	18881.640075	29.786535
389.387326	18920.066339	29.791552
389.884883	18945.752174	29.796570
390.592505	18982.896311	29.801588
390.698127	19011.131277	29.806605
391.129919	19037.067719	29.811623
391.669017	19075.962830	29.816640
391.720227	19098.711844	29.821658
392.085847	19127.742668	29.826676
392.268294	19169.562693	29.831693
392.767486	19194.376928	29.836711
393.032769	19222.833365	29.841728
393.109219	19262.774792	29.846746
393.740947	19297.372180	29.851764
393.603565	19333.151274	29.856781
394.068923	19375.784197	29.861799
394.614581	19411.129047	29.866816
395.988054	19425.814523	29.871834
396.517173	19452.137509	29.876852
396.855922	19490.040472	29.881869
397.317871	19511.409082	29.886887
397.491228	19530.374132	29.891904
397.450253	19553.570923	29.896922
397.981919	19577.954745	29.901940
398.183236	19618.276799	29.906957
398.780668	19644.970291	29.911975
398.982916	19676.874439	29.916992
399.367938	19700.748270	29.922010
400.139246	19746.285760	29.927028
400.094242	19788.012496	29.932045
400.788033	19816.235217	29.937063
401.044643	19851.162138	29.942080
401.517638	19888.949248	29.947098
402.038425	19921.553191	29.952116
401.918705	19963.699423	29.957133
402.488007	19995.121066	29.962151
402.709113	20038.604739	29.967168
403.124840	20074.278290	29.972186
403.954854	20118.194416	29.977204
404.090965	20150.591206	29.982221
404.791162	20171.363252	29.987239
405.702775	20214.326597	29.992256
406.064945	20237.802983	29.997274
406.158293	20276.050950	30.002292
406.382598	20313.102917	30.007309
406.901007	20338.820568	30.012327
407.505917	20366.661641	30.017344
407.352488	20418.774624	30.022362
407.734378	20438.505524	30.027380
408.200795	20489.795893	30.032397
408.492055	20524.177771	30.037415
408.870851	20565.169594	30.042432
409.514634	20596.573762	30.047450
410.276950	20621.081814	30.052468
410.504470	20665.699548	30.057485
411.188550	20697.552853	30.062503
411.193001	20735.081913	30.067520
412.076313	20780.196993	30.072538
412.704241	20804.100070	30.077556
412.979347	20825.055085	30.082573
413.238535	20855.790202	30.087591
413.938410	20884.122508	30.092608
414.217145	20927.304170	30.097626
415.072926	20948.838163	30.102644
414.966119	20978.418476	30.107661
415.708589	21014.235549	30.112679
415.421547	21052.429889	30.117696
415.608265	21085.275744	30.122714
416.223733	21115.652945	30.127732
416.383060	21163.873017	30.132749
417.090046	21192.923570	30.137767
417.439602	21234.279736	30.142784
417.798936	21265.599722	30.147802
418.389385	21304.901455	30.152820
418.794251	21343.073598	30.157837
418.953378	21389.372543	30.162855
419.444252	21429.469832	30.167872
419.604686	21467.416198	30.172890
420.344441	21497.822436	30.177908
420.520593	21547.961082	30.182925
421.044620	21576.709870	30.187943
421.678055	21614.628885	30.192960
421.922427	21644.893349	30.197978
422.613035	21679.041362	30.202996
422.779409	21709.585269	30.208013
423.284243	21740.341340	30.213031
423.813133	21772.250708	30.218048
423.949325	21821.122889	30.223066
424.539558	21838.481367	30.228084
425.017130	21887.607938	30.233101
424.875091	21932.004724	30.238119
425.577883	21956.951830	30.243136
426.095858	22010.510223	30.248154
426.684072	22038.907076	30.253172
427.188176	22084.490350	30.258189
427.345931	22111.213120	30.263207
427.837104	22165.875338	30.268224
428.275879	22191.586922	30.273242
428.794317	22231.711530	30.278260
429.263773	22274.354324	30.283277
429.651531	22304.396058	30.288295
430.197961	22345.135930	30.293312
430.334791	22405.161273	30.298330
431.103735	22427.428892	30.303348
431.036445	22478.379928	30.308365
431.204385	22509.117379	30.313383
431.966559	22556.625390	30.318400
432.285715	22607.129850	30.323418
432.818565	22664.634257	30.328436
433.156228	22702.714953	30.333453
433.812542	22746.516887	30.338471
434.523624	22787.645297	30.343488
435.226215	22826.667184	30.348506
435.937071	22846.479021	30.353524
436.659978	22885.002609	30.358541
436.978181	22918.164583	30.363559
437.423134	22945.389923	30.368576
437.678900	22982.330638	30.373594
437.995071	23011.562422	30.378612
438.586832	23041.981716	30.383629
438.813595	23078.255756	30.388647
439.511008	23113.998036	30.393664
439.414805	23152.665425	30.398682
439.900170	23176.354200	30.403700
440.075686	23236.418678	30.408717
440.771639	23259.404253	30.413735
441.460461	23294.154998	30.418752
441.669320	23336.209680	30.423770
442.034381	23371.368829	30.428788
442.473875	23412.942542	30.433805
442.655088	23453.545176	30.438823
443.245822	23503.395679	30.443840
443.406359	23551.425290	30.448858
443.857420	23590.777463	30.453876
444.649994	23635.344420	30.458893
444.815726	23685.065414	30.463911
445.824657	23713.830784	30.468928
446.278856	23761.823519	30.473946
446.832817	23792.516884	30.478964
446.888566	23828.500696	30.483981
447.445548	23875.655275	30.488999
448.115080	23912.906525	30.494016
448.065223	23961.024084	30.499034
448.502709	24000.567090	30.504052
448.908726	24036.482446	30.509069
449.190853	24085.780151	30.514087
449.525833	24137.861792	30.519104
449.786179	24182.876042	30.524122
450.545726	24223.350297	30.529140
451.350331	24265.994791	30.534157
451.785854	24300.559230	30.539175
452.474291	24334.055450	30.544192
452.986677	24361.484803	30.549210
453.234733	24389.432490	30.554228
453.796691	24436.412779	30.559245
454.200197	24465.317280	30.564263
454.583449	24488.897037	30.569280
454.724314	24545.718857	30.574298
455.340726	24571.395262	30.579316
456.034663	24621.760251	30.584333
456.171213	24666.636969	30.589351
456.550442	24705.562075	30.594368
457.047098	24746.008468	30.599386
457.294990	24792.062387	30.604404
457.509700	24850.467238	30.609421
457.867906	24888.741833	30.614439
458.618184	24932.801974	30.619456
459.166230	24998.342843	30.624474
459.419040	25034.720837	30.629492
460.005617	25084.275486	30.634509
460.877289	25137.250785	30.639527
461.041952	25177.467624	30.644544
461.355199	25225.547699	30.649562
461.971865	25273.508406	30.654580
462.708405	25321.523563	30.659597
463.012797	25354.976426	30.664615
463.468990	25402.577659	30.669632
463.922066	25455.541093	30.674650
464.543197	25501.852238	30.679668
465.157410	25541.120479	30.684685
465.632524	25584.923411	30.689703
466.309456	25625.108725	30.694720
466.701497	25670.160345	30.699738
467.464793	25705.080347	30.704756
467.770021	25751.307157	30.709773
467.900641	25799.767523	30.714791
468.334436	25842.440952	30.719808
468.896418	25885.008158	30.724826
469.120044	25929.930585	30.729844
469.749513	25981.172844	30.734861
470.119813	26021.567440	30.739879
470.534998	26061.210380	30.744896
471.149247	26113.209348	30.749914
471.395057	26152.255989	30.754932
472.085537	26207.970662	30.759949
472.524740	26258.724772	30.764967
473.117495	26292.302155	30.769984
473.796845	26350.548647	30.775002
474.408679	26399.852197	30.780020
474.704721	26433.560872	30.785037
474.979087	26471.427069	30.790055
475.613612	26508.987842	30.795072
475.883783	26565.325063	30.800090
476.571400	26613.932280	30.805108
477.189550	26662.926445	30.810125
477.400687	26706.711194	30.815143
477.806305	26747.811337	30.820160
478.297954	26791.805449	30.825178
478.741469	26839.561016	30.830196
479.285053	26887.748071	30.835213
479.620811	26935.250449	30.840231
480.335484	26980.823120	30.845248
480.579077	27038.872673	30.850266
480.799163	27090.144866	30.855284
481.939475	27120.066075	30.860301
483.150299	27146.764748	30.865319
484.260728	27156.639932	30.870336
484.433704	27190.042388	30.875354
485.200942	27211.152691	30.880372
485.491227	27242.460423	30.885389
485.693240	27254.182667	30.890407
486.309835	27271.797856	30.895424
486.194373	27306.143971	30.900442
486.502893	27332.140343	30.905460
486.962786	27370.738040	30.910477
486.956813	27406.548747	30.915495
487.429223	27442.759952	30.920512
487.893929	27493.832078	30.925530
488.286922	27540.077597	30.930548
489.046879	27572.885470	30.935565
489.295529	27623.296579	30.940583
489.895109	27677.233113	30.945600
490.240086	27716.541350	30.950618
490.493930	27768.330442	30.955636
491.161142	27807.150369	30.960653
491.568376	27857.971260	30.965671
491.943576	27909.832206	30.970688
492.493527	27963.746290	30.975706
492.819546	28019.038121	30.980724
493.367709	28065.464450	30.985741
493.901930	28121.860934	30.990759
494.995095	28174.266494	30.995776
495.497284	28220.546271	31.000794
495.525666	28262.327442	31.005812
496.219344	28316.550097	31.010829
496.292610	28372.257023	31.015847
497.021849	28420.105415	31.020864
499.196529	28442.240207	31.025882
500.243590	28450.104642	31.030900
501.186134	28471.600768	31.035917
501.343555	28503.096764	31.040935
501.755623	28522.087646	31.045952
502.178991	28543.407800	31.050970
502.219897	28582.156276	31.055988
502.891261	28604.239922	31.061005
503.074878	28631.116889	31.066023
503.108413	28668.920446	31.071040
503.535363	28704.583472	31.076058
503.851339	28745.479222	31.081076
504.091058	28783.636970	31.086093
504.408876	28838.002207	31.091111
504.912233	28879.372038	31.096128
505.721256	28940.299802	31.101146
505.713529	28996.306018	31.106164
505.726690	29032.142165	31.111181
505.857051	29094.762981	31.116199
506.540662	29161.759457	31.121216
507.183400	29224.056362	31.126234
507.364075	29291.426630	31.131252
508.233237	29349.569888	31.136269
508.205947	29429.479755	31.141287
509.142602	29475.593331	31.146304
510.056336	29542.736234	31.151322
510.766546	29606.124321	31.156340
511.374832	29653.696413	31.161357
511.799018	29711.756652	31.166375
513.088752	29753.787336	31.171392
513.963177	29783.917987	31.176410
514.493444	29821.228743	31.181428
515.064377	29846.983655	31.186445
515.410099	29905.019644	31.191463
515.707383	29938.245982	31.196480
516.207498	29980.120565	31.201498
516.676500	30029.603193	31.206516
517.184420	30061.570955	31.211533
517.184102	30102.847077	31.216551
517.505765	30148.881050	31.221568
517.854436	30185.878719	31.226586
518.139091	30237.928782	31.231604
518.922389	30277.041083	31.236621
519.224953	30330.337739	31.241639
519.627072	30382.649604	31.246656
520.400192	30428.587664	31.251674
520.949897	30499.611652	31.256692
521.261154	30548.989308	31.261709
521.829391	30596.403388	31.266727
522.189644	30664.651574	31.271744
522.699264	30723.085955	31.276762
523.462772	30773.727189	31.281780
523.940362	30824.898485	31.286797
524.421304	30886.619180	31.291815
524.666465	30942.091407	31.296832
525.648319	31004.370215	31.301850
526.068134	31066.565406	31.306868
526.510105	31118.469067	31.311885
526.804875	31187.424182	31.316903
527.682250	31242.856036	31.321920
528.557969	31296.979047	31.326938
528.843604	31359.055468	31.331956
529.222872	31398.839610	31.336973
530.061277	31470.927240	31.341991
530.592301	31523.120265	31.347008
531.235675	31571.855972	31.352026
531.732626	31624.660682	31.357044
532.378731	31678.832264	31.362061
532.686247	31734.552254	31.367079
533.296983	31794.806564	31.372096
534.140942	31839.064476	31.377114
534.235729	31902.060899	31.382132
534.728686	31947.541265	31.387149
535.549430	32014.229467	31.392167
535.825081	32061.799959	31.397184
537.021595	32108.574845	31.402202
537.828585	32158.493548	31.407220
538.420294	32208.384849	31.412237
538.997317	32250.876872	31.417255
539.638210	32292.263629	31.422272
539.991112	32337.279097	31.427290
540.403879	32394.589743	31.432308
540.806608	32441.600747	31.437325
541.336747	32494.235367	31.442343
542.028454	32544.107948	31.447360
543.338540	32576.727133	31.452378
543.135429	32622.327370	31.457396
543.810984	32667.347182	31.462413
544.006234	32701.870302	31.467431
544.284846	32761.242540	31.472448
544.977526	32809.342500	31.477466
545.088018	32874.387523	31.482484
545.470561	32941.798435	31.487501
546.062911	32984.387509	31.492519
546.786099	33054.519183	31.497536
548.154508	33102.473626	31.502554
549.327664	33131.207113	31.507572
550.939969	33151.200636	31.512589
551.375626	33169.732018	31.517607
551.929360	33202.616125	31.522624
552.105983	33231.255642	31.527642
552.339807	33266.985119	31.532660
553.003743	33265.887821	31.537677
553.503967	33305.870857	31.542695
553.926519	33348.731814	31.547712
554.297344	33377.484635	31.552730
554.656274	33420.435156	31.557748
554.899187	33441.762702	31.562765
555.270175	33480.158274	31.567783
555.304589	33541.214229	31.572800
555.679250	33578.511355	31.577818
555.956118	33628.442900	31.582836
556.519013	33685.105028	31.587853
556.674458	33739.780497	31.592871
556.727880	33803.610929	31.597888
557.519642	33880.266167	31.602906
557.405937	33941.865446	31.607924
558.007625	34016.618412	31.612941
558.518630	34088.767672	31.617959
559.659344	34155.609913	31.622976
560.426319	34225.196262	31.627994
560.891556	34301.960895	31.633012
561.643803	34362.298418	31.638029
562.471686	34431.465304	31.643047
562.908214	34504.537333	31.648064
563.922273	34573.566736	31.653082
563.863820	34635.963947	31.658100
564.385303	34697.211643	31.663117
565.161386	34777.114069	31.668135
565.381930	34836.345070	31.673152
566.426382	34909.422485	31.678170
566.876600	34983.459821	31.683188
567.658127	35041.737377	31.688205
568.502872	35105.340799	31.693223
569.191853	35163.517282	31.698240
570.356639	35211.230229	31.703258
571.082395	35267.760058	31.708276
571.370408	35310.897266	31.713293
571.980057	35366.020236	31.718311
572.460360	35428.785648	31.723328
573.029096	35480.520244	31.728346
573.343464	35539.069081	31.733364
574.250893	35600.559082	31.738381
574.927521	35655.324758	31.743399
574.789836	35724.220657	31.748416
575.758887	35781.027499	31.753434
576.618543	35837.574886	31.758452
576.950191	35886.699006	31.763469
577.501439	35937.844536	31.768487
578.180313	36000.392969	31.773504
578.892443	36051.471228	31.778522
579.233919	36110.430862	31.783540
579.712345	36166.508930	31.788557
580.957076	36209.474512	31.793575
581.578081	36259.571185	31.798592
582.429223	36314.714000	31.803610
583.128205	36355.122345	31.808628
583.728908	36405.052364	31.813645
584.020883	36450.356564	31.818663
584.505597	36508.732112	31.823680
584.850487	36536.702204	31.828698
585.326986	36591.260798	31.833716
586.021405	36653.594347	31.838733
586.739515	36695.347858	31.843751
587.114826	36755.863030	31.848768
587.748268	36812.192076	31.853786
588.039783	36869.849605	31.858804
588.469850	36927.310858	31.863821
589.492739	36985.927288	31.868839
589.786461	37049.019538	31.873856
590.878462	37072.474000	31.878874
591.783570	37127.588312	31.883892
592.126736	37175.262318	31.888909
592.948076	37218.549575	31.893927
593.144593	37256.518163	31.898944
593.842698	37295.297132	31.903962
594.321391	37358.217896	31.908980
594.482364	37400.598428	31.913997
595.042288	37454.325303	31.919015
595.106273	37518.934157	31.924032
595.431209	37568.082920	31.929050
595.999661	37623.408999	31.934068
596.720304	37694.730234	31.939085
597.493091	37756.751681	31.944103
598.173091	37814.221827	31.949120
599.452553	37868.746359	31.954138
600.000192	37935.372462	31.959156
600.153795	37988.931331	31.964173
600.878450	38052.290465	31.969191
601.277178	38099.550599	31.974208
602.244962	38172.404654	31.979226
602.776109	38228.145890	31.984244
602.956228	38294.489996	31.989261
603.644480	38361.504746	31.994279
604.164214	38420.350974	31.999296
604.903024	38497.063133	32.004314
605.142852	38560.352624	32.009332
605.462417	38641.600667	32.014349
606.318097	38705.382320	32.019367
606.578809	38788.714385	32.024384
607.246490	38862.996908	32.029402
607.955803	38929.076027	32.034420
608.913078	39020.629821	32.039437
609.738883	39069.570532	32.044455
610.119794	39146.256171	32.049472
610.797360	39214.358453	32.054490
611.734392	39289.554600	32.059508
612.178284	39360.309464	32.064525
613.095157	39423.471204	32.069543
613.350105	39495.936982	32.074560
613.927219	39555.468659	32.079578
614.698995	39632.236986	32.084596
615.619300	39694.688915	32.089613
616.009823	39761.300328	32.094631
616.645923	39835.800366	32.099648
617.232473	39898.443842	32.104666
618.245392	39953.952987	32.109684
618.908359	40017.591159	32.114701
619.598714	40083.923811	32.119719
620.294448	40158.860382	32.124736
620.704329	40220.729241	32.129754
621.581556	40279.749715	32.134772
621.708793	40341.072240	32.139789
622.326787	40401.407996	32.144807
622.625372	40482.759259	32.149824
623.219681	40551.388492	32.154842
623.762528	40621.102869	32.159860
624.410718	40691.374610	32.164877
625.671632	40760.772062	32.169895
626.512823	40828.332513	32.174912
627.208338	40887.378648	32.179930
628.571329	40954.818666	32.184948
628.682170	41010.205384	32.189965
630.033664	41046.267622	32.194983
630.602697	41103.144639	32.200000
631.510351	41152.364685	32.205018
632.089573	41179.454103	32.210036
632.669993	41226.269356	32.215053
633.405470	41280.167952	32.220071
633.672411	41326.861619	32.225088
634.244906	41366.389760	32.230106
634.935509	41399.269418	32.235124
635.293364	41451.482075	32.240141
635.935887	41474.416722	32.245159
636.282965	41541.209099	32.250176
636.454621	41591.729337	32.255194
637.118919	41634.484855	32.260212
637.738363	41691.920428	32.265229
638.440034	41743.950863	32.270247
638.637621	41799.218305	32.275264
639.313785	41871.554475	32.280282
640.070347	41933.599150	32.285300
640.280061	42004.797517	32.290317
640.901083	42065.605459	32.295335
641.280698	42151.401837	32.300352
641.606407	42226.180682	32.305370
642.332016	42298.605068	32.310388
642.743957	42378.825327	32.315405
643.544811	42454.836725	32.320423
644.045156	42536.409995	32.325440
644.399224	42622.316959	32.330458
645.548247	42712.316991	32.335476
646.070834	42787.005610	32.340493
647.078718	42870.374909	32.345511
647.526679	42951.403041	32.350528
648.268773	43038.144430	32.355546
648.685474	43109.742219	32.360564
649.344887	43202.262693	32.365581
650.251842	43296.586446	32.370599
650.687285	43379.844218	32.375616
651.659862	43453.413074	32.380634
652.533299	43531.528976	32.385652
653.314143	43611.292707	32.390669
653.839207	43687.057952	32.395687
655.031006	43752.882190	32.400704
655.633969	43830.614656	32.405722
656.363503	43889.857380	32.410740
656.832695	43976.417761	32.415757
657.662345	44043.218409	32.420775
658.646969	44116.472192	32.425792
659.277671	44188.897550	32.430810
660.468311	44246.966566	32.435828
660.646813	44314.923913	32.440845
661.330650	44366.532142	32.445863
662.201829	44443.048395	32.450880
662.408062	44498.672914	32.455898
662.943834	44583.315001	32.460916
663.445648	44661.329695	32.465933
664.005281	44732.322883	32.470951
664.870739	44804.127770	32.475968
665.576905	44877.462110	32.480986
666.618303	44948.386028	32.486004
667.681733	45010.352445	32.491021
668.115166	45080.938407	32.496039
668.877592	45135.434210	32.501056
669.352376	45218.690553	32.506074
669.933890	45280.181761	32.511092
670.537453	45356.777533	32.516109
671.171351	45420.767504	32.521127
671.801526	45496.465914	32.526144
671.892615	45572.424161	32.531162
672.878044	45641.885449	32.536180
672.786200	45737.144297	32.541197
673.553870	45811.018378	32.546215
674.407577	45902.146684	32.551232
674.584784	45987.097465	32.556250
675.568105	46073.822626	32.561268
676.236616	46165.986880	32.566285
676.476292	46251.560041	32.571303
677.268816	46338.870501	32.576320
677.912985	46423.727192	32.581338
678.940400	46491.230170	32.586356
679.246010	46580.958762	32.591373
679.913289	46664.963337	32.596391
680.665604	46743.327397	32.601408
681.640175	46832.997233	32.606426
682.800682	46902.036413	32.611444
683.374163	46967.320471	32.616461
684.223040	47040.159741	32.621479
684.994008	47115.667753	32.626496
685.461961	47190.844031	32.631514
686.432932	47260.481051	32.636532
687.003187	47349.187551	32.641549
687.708467	47413.330403	32.646567
688.360139	47489.121702	32.651584
688.797564	47573.383009	32.656602
689.700214	47642.994830	32.661620
690.158835	47731.216319	32.666637
690.829629	47815.395955	32.671655
691.457103	47900.899920	32.676672
691.842006	47986.235915	32.681690
692.662074	48074.070896	32.686708
693.475424	48167.143091	32.691725
694.349330	48238.214455	32.696743
695.510463	48325.283760	32.701760
695.688289	48409.822181	32.706778
696.856248	48488.159572	32.711796
697.290035	48566.482741	32.716813
697.844358	48649.229518	32.721831
698.674968	48737.580572	32.726848
699.174333	48828.592047	32.731866
700.295497	48914.350632	32.736884
701.010747	48999.712415	32.741901
701.909481	49066.588987	32.746919
702.828574	49139.175254	32.751936
703.563748	49215.755477	32.756954
704.541245	49300.099474	32.761972
704.845168	49368.212224	32.766989
705.589191	49450.391132	32.772007
706.345364	49526.457531	32.777024
706.523340	49613.028744	32.782042
707.186120	49687.756393	32.787060
708.157507	49769.902287	32.792077
708.634752	49857.928444	32.797095
709.222555	49939.971035	32.802112
709.636228	50035.420646	32.807130
710.488871	50122.410157	32.812148
710.805499	50221.890749	32.817165
711.621355	50309.720945	32.822183
712.814597	50404.206732	32.827200
712.993517	50507.078196	32.832218
714.297801	50599.973814	32.837236
714.691627	50682.421131	32.842253
715.315303	50790.753929	32.847271
715.682983	50880.577824	32.852288
717.156504	50966.893826	32.857306
718.132533	51036.837555	32.862324
719.532618	51117.291900	32.867341
719.924919	51203.667505	32.872359
720.791471	51279.409961	32.877376
721.149972	51361.613356	32.882394
722.057414	51434.952471	32.887412
722.690294	51523.961771	32.892429
723.069183	51606.728196	32.897447
724.319905	51688.485594	32.902464
724.803828	51766.794623	32.907482
725.261113	51849.233298	32.912500
725.859246	51926.421816	32.917517
726.458448	52003.430433	32.922535
726.849995	52091.297776	32.927552
727.509752	52183.833708	32.932570
727.944013	52262.699367	32.937588
728.774659	52361.468103	32.942605
729.397848	52441.421411	32.947623
730.543235	52544.453674	32.952640
730.615617	52640.215761	32.957658
731.412292	52729.339380	32.962676
732.059108	52831.937496	32.967693
732.439158	52935.174030	32.972711
733.518473	53032.673258	32.977728
734.081765	53135.564733	32.982746
734.903613	53241.490600	32.987764
735.690651	53335.672471	32.992781
736.292166	53449.627340	32.997799
737.249413	53546.460707	33.002816
738.060866	53651.720876	33.007834
738.972604	53750.792844	33.012852
739.604027	53851.541533	33.017869
740.375967	53954.270209	33.022887
741.002545	54053.270771	33.027904
741.742476	54163.479565	33.032922
742.092447	54264.118920	33.037940
743.324182	54377.438133	33.042957
743.856747	54490.386996	33.047975
744.987231	54578.971172	33.052992
745.811050	54708.665858	33.058010
746.476540	54799.033630	33.063028
747.161830	54901.554149	33.068045
748.238511	55015.818757	33.073063
749.197540	55102.405564	33.078080
750.102735	55210.059463	33.083098
750.553052	55311.161471	33.088116
751.624392	55406.096123	33.093133
752.472074	55510.229379	33.098151
753.477934	55597.745713	33.103168
753.802741	55709.737641	33.108186
754.402836	55804.088630	33.113204
755.543337	55887.515117	33.118221
756.320796	56007.394920	33.123239
756.931864	56097.430146	33.128256
757.538188	56191.624005	33.133274
758.164077	56285.075838	33.138292
759.168410	56389.971347	33.143309
759.826005	56489.680408	33.148327
760.921354	56580.749904	33.153344
762.006039	56666.273984	33.158362
763.185790	56745.401076	33.163380
763.956226	56822.176094	33.168397
764.672994	56915.767547	33.173415
765.704541	57000.252972	33.178432
766.695915	57074.085948	33.183450
767.333133	57166.718663	33.188468
768.652679	57239.114289	33.193485
768.905295	57321.309676	33.198503
770.008664	57383.081956	33.203520
770.772855	57468.731935	33.208538
770.851698	57539.747546	33.213556
771.860969	57616.852690	33.218573
772.534112	57707.940224	33.223591
773.280407	57790.706865	33.228608
773.446135	57863.251071	33.233626
774.191867	57954.542587	33.238644
775.247840	58040.759778	33.243661
776.062396	58127.105672	33.248679
776.712683	58217.245156	33.253696
777.355424	58301.414868	33.258714
777.692320	58381.768217	33.263732
778.627451	58463.969359	33.268749
779.221193	58562.991646	33.273767
780.204172	58640.894982	33.278784
780.744081	58722.808586	33.283802
781.705341	58803.932566	33.288820
783.017124	58891.311828	33.293837
783.984186	58956.321636	33.298855
784.853485	59027.982954	33.303872
785.790695	59110.293841	33.308890
787.000798	59185.229677	33.313908
788.192421	59246.658251	33.318925
788.383496	59322.508548	33.323943
790.137443	59390.612668	33.328960
790.780499	59447.405601	33.333978
790.964419	59507.592169	33.338996
791.582164	59573.995050	33.344013
792.206267	59653.446646	33.349031
792.941298	59729.474071	33.354048
793.379813	59814.012483	33.359066
793.877599	59895.944160	33.364084
794.823098	59980.153092	33.369101
795.029846	60087.525360	33.374119
796.094853	60178.319298	33.379136
796.583067	60272.690984	33.384154
796.979703	60378.061733	33.389172
797.523592	60475.597625	33.394189
797.989749	60591.101048	33.399207
798.664249	60706.823518	33.404224
799.435267	60826.752313	33.409242
800.099281	60958.214165	33.414260
800.809091	61068.523125	33.419277
801.858922	61198.823180	33.424295
802.893882	61305.831326	33.429312
803.674307	61421.761592	33.434330
804.444192	61551.591908	33.439348
805.820771	61665.984172	33.444365
806.505219	61776.591897	33.449383
807.627288	61866.657194	33.454400
808.516429	61994.865353	33.459418
809.107496	62099.245971	33.464436
810.148338	62213.709403	33.469453
810.878662	62326.391887	33.474471
811.135275	62442.104781	33.479488
811.905388	62553.922398	33.484506
812.875373	62677.709940	33.489524
813.863964	62786.092413	33.494541
814.181709	62917.478751	33.499559
815.079094	63037.090029	33.504576
815.964876	63154.965790	33.509594
816.560153	63286.397157	33.514612
817.560966	63404.091025	33.519629
818.235773	63541.054028	33.524647
819.021085	63661.686118	33.529664
820.356068	63785.318965	33.534682
820.784068	63905.088669	33.539700
822.070467	64022.814782	33.544717
822.795865	64151.360585	33.549735
823.333814	64266.354684	33.554752
824.340416	64384.931818	33.559770
825.152247	64500.893341	33.564788
826.034450	64624.764029	33.569805
827.063840	64747.018272	33.574823
827.469803	64865.387625	33.579840
828.755904	64983.814598	33.584858
829.727510	65108.191753	33.589876
830.923823	65203.114070	33.594893
831.675484	65302.478157	33.599911
833.314012	65393.820098	33.604928
834.700195	65458.440170	33.609946
835.293981	65531.231871	33.614964
836.672902	65610.076353	33.619981
837.143541	65691.037027	33.624999
838.407026	65788.422558	33.630016
838.685593	65853.226758	33.635034
839.308337	65955.649499	33.640052
839.849391	66035.683297	33.645069
840.367522	66136.076079	33.650087
840.805536	66237.892254	33.655104
841.569035	66337.607029	33.660122
841.913455	66456.798463	33.665140
842.813789	66561.498342	33.670157
843.253585	66684.588356	33.675175
844.147675	66807.547189	33.680192
845.148182	66927.587543	33.685210
845.556504	67070.901641	33.690228
846.363082	67180.784926	33.695245
846.988812	67302.697332	33.700263
847.953245	67442.438867	33.705280
849.071467	67567.078370	33.710298
849.957666	67697.415000	33.715316
851.155751	67817.054850	33.720333
852.207586	67949.180086	33.725351
852.950482	68068.700554	33.730368
854.056588	68179.962073	33.735386
854.575983	68305.678439	33.740404
855.577700	68433.579224	33.745421
856.240725	68556.080714	33.750439
857.189024	68686.811530	33.755456
858.533675	68798.390977	33.760474
859.125231	68932.861747	33.765492
860.048485	69042.615397	33.770509
860.822513	69172.062966	33.775527
861.403144	69299.937384	33.780544
862.843089	69420.564323	33.785562
863.801471	69546.468499	33.790580
864.600904	69656.467071	33.795597
865.094598	69789.391481	33.800615
865.880941	69914.441103	33.805632
866.990760	70037.319990	33.810650
867.733364	70173.057186	33.815668
868.873698	70289.186269	33.820685
870.212182	70397.006881	33.825703
871.898956	70505.826426	33.830720
873.491474	70600.107144	33.835738
874.369247	70699.817422	33.840756
874.870103	70792.704877	33.845773
875.521430	70907.501778	33.850791
876.307981	71011.230929	33.855808
877.156616	71112.452792	33.860826
877.539564	71220.707241	33.865844
878.623980	71322.289513	33.870861
879.811011	71419.878169	33.875879
880.624783	71530.813553	33.880896
881.266364	71634.531732	33.885914
882.123314	71760.908385	33.890932
883.027600	71866.063912	33.895949
884.066290	71967.479755	33.900967
884.445817	72095.328303	33.905984
885.267916	72195.762956	33.911002
885.939305	72314.908148	33.916020
886.960522	72435.159722	33.921037
888.175805	72541.335846	33.926055
889.141036	72654.237557	33.931072
889.399642	72767.977401	33.936090
890.033092	72880.081423	33.941108
890.525513	72996.218378	33.946125
891.453898	73113.997639	33.951143
891.977119	73237.807516	33.956160
893.014474	73357.479816	33.961178
893.685541	73488.355421	33.966196
894.860244	73604.326082	33.971213
895.870842	73727.337399	33.976231
896.579672	73866.056719	33.981248
897.179099	73985.653035	33.986266
898.073984	74111.107630	33.991284
899.361147	74229.643174	33.996301
900.446674	74369.732700	34.001319
901.534366	74491.692194	34.006336
902.529260	74606.445782	34.011354
903.049567	74734.255084	34.016372
904.284226	74863.370087	34.021389
904.878593	74989.404265	34.026407
905.421519	75130.739257	34.031424
906.840830	75253.704388	34.036442
907.408069	75391.293185	34.041460
908.386712	75520.663049	34.046477
909.265269	75670.161228	34.051495
910.102295	75798.373490	34.056512
911.263039	75925.622354	34.061530
911.695270	76068.986491	34.066548
912.605906	76205.391650	34.071565
913.386146	76348.074037	34.076583
913.900442	76497.201617	34.081600
915.228162	76639.359114	34.086618
916.723667	76771.838577	34.091636
918.241777	76903.973579	34.096653
919.655999	77031.636051	34.101671
920.428924	77160.847169	34.106688
922.171419	77271.272755	34.111706
923.042705	77393.878679	34.116724
923.668145	77511.472396	34.121741
924.775618	77624.977237	34.126759
925.438445	77756.101129	34.131776
926.632199	77872.034375	34.136794
927.169796	77984.015987	34.141812
927.972443	78118.762077	34.146829
928.763043	78240.759850	34.151847
929.390411	78372.253765	34.156864
930.454713	78499.767445	34.161882
930.952350	78641.309555	34.166900
931.623274	78785.303400	34.171917
932.380346	78915.457163	34.176935
933.328713	79068.736636	34.181952
934.265198	79205.023210	34.186970
935.302153	79359.321067	34.191988
936.473434	79504.951099	34.197005
937.933376	79628.338739	34.202023
938.917115	79764.684183	34.207040
940.325106	79885.298647	34.212058
941.241094	80006.355546	34.217076
942.346424	80130.658445	34.222093
943.094641	80257.690371	34.227111
943.956472	80396.729165	34.232128
945.271277	80523.694352	34.237146
945.932209	80643.291306	34.242164
946.402128	80775.445272	34.247181
947.566354	80902.804351	34.252199
947.921192	81044.366257	34.257216
948.748456	81178.437223	34.262234
949.538871	81324.546798	34.267252
950.338518	81470.744358	34.272269
951.349688	81605.938808	34.277287
951.445957	81756.113148	34.282304
952.257238	81897.807469	34.287322
953.080688	82041.215022	34.292340
953.845283	82191.794313	34.297357
955.142384	82354.192439	34.302375
956.158846	82501.562817	34.307392
957.279868	82634.714569	34.312410
958.367274	82798.668782	34.317428
959.153978	82952.083618	34.322445
960.134120	83103.689851	34.327463
960.975402	83256.117141	34.332480
962.189239	83404.726051	34.337498
962.827712	83561.990613	34.342516
963.621238	83713.739257	34.347533
965.104732	83874.586433	34.352551
965.771169	84031.387766	34.357568
967.348467	84183.952784	34.362586
968.165561	84336.802496	34.367604
968.992594	84504.177715	34.372621
970.355388	84648.461609	34.377639
971.129805	84796.614320	34.382656
971.853795	84960.745246	34.387674
973.371313	85108.536856	34.392692
974.934360	85246.363327	34.397709
976.680192	85380.022616	34.402727
977.746938	85522.102138	34.407744
978.990788	85646.070642	34.412762
980.166691	85768.760310	34.417780
981.101890	85901.860478	34.422797
982.279646	86034.877075	34.427815
982.915719	86174.494525	34.432832
983.540548	86299.334314	34.437850
984.307188	86429.320717	34.442868
984.923923	86562.116596	34.447885
986.408434	86709.113987	34.452903
987.151601	86850.704593	34.457920
988.022454	87001.740760	34.462938
988.740653	87146.798372	34.467956
989.351873	87287.021373	34.472973
990.428718	87453.433855	34.477991
991.096607	87605.823561	34.483008
991.789761	87769.023957	34.488026
993.007098	87924.710292	34.493044
993.920847	88098.272884	34.498061
995.148450	88245.145177	34.503079
996.111584	88416.019006	34.508096
996.773337	88579.185922	34.513114
998.231386	88748.550368	34.518132
998.724492	88905.976377	34.523149
1000.116487	89082.226236	34.528167
1000.707968	89256.432740	34.533184
1001.785543	89427.307658	34.538202
1003.257200	89578.526977	34.543220
1004.694689	89740.282914	34.548237
1005.859985	89882.233416	34.553255
1006.665876	90040.722762	34.558272
1007.807564	90208.232446	34.563290
1009.286179	90349.640412	34.568308
1009.946900	90498.316281	34.573325
1010.911231	90654.574972	34.578343
1011.691970	90813.478633	34.583360
1012.571973	90965.753726	34.588378
1013.554866	91126.860044	34.593396
1014.235390	91298.016467	34.598413
1015.323626	91458.329215	34.603431
1015.956213	91622.971101	34.608448
1017.371642	91791.313723	34.613466
1018.248710	91949.209090	34.618484
1019.034716	92114.107478	34.623501
1020.154271	92267.325921	34.628519
1021.227473	92424.578136	34.633536
1022.028082	92589.926720	34.638554
1022.529629	92738.218723	34.643572
1023.806999	92906.971679	34.648589
1024.567312	93064.627813	34.653607
1025.511245	93250.026551	34.658624
1026.329599	93429.789219	34.663642
1027.511609	93599.777937	34.668660
1028.092941	93783.791243	34.673677
1029.416115	93968.942989	34.678695
1030.740753	94150.456560	34.683712
1031.715225	94318.914907	34.688730
1032.996541	94489.330174	34.693748
1033.675022	94675.726685	34.698765
1035.292374	94848.671392	34.703783
1036.145619	95032.117553	34.708800
1037.213004	95193.888951	34.713818
1038.719587	95367.741754	34.718836
1039.599159	95546.357927	34.723853
1040.487888	95723.264869	34.728871
1041.365950	95901.307869	34.733888
1042.396374	96078.991524	34.738906
1043.172262	96263.269862	34.743924
1044.284081	96450.886936	34.748941
1045.292006	96639.180900	34.753959
1046.117530	96834.171881	34.758976
1047.089376	97027.405813	34.763994
1048.346153	97216.334067	34.769012
1049.087453	97416.280995	34.774029
1050.088612	97602.564081	34.779047
1051.055745	97812.579880	34.784064
1052.348864	98002.482964	34.789082
1054.009314	98199.859947	34.794100
1054.827300	98404.594206	34.799117
1056.322380	98595.354714	34.804135
1057.364913	98791.331737	34.809152
1058.436630	98982.772814	34.814170
1060.015193	99156.197161	34.819188
1061.342547	99338.501720	34.824205
1062.189997	99511.618736	34.829223
1063.702900	99692.445507	34.834240
1064.559431	99865.582449	34.839258
1065.893254	100036.869163	34.844276
1066.864200	100215.839272	34.849293
1067.986853	100387.644369	34.854311
1069.516582	100568.664566	34.859328
1070.569257	100730.543990	34.864346
1072.368207	100886.362764	34.869364
1073.556343	101039.485010	34.874381
1074.822067	101191.208865	34.879399
1076.299469	101339.150658	34.884416
1077.659180	101496.330904	34.889434
1079.119552	101617.002513	34.894452
1080.438135	101742.623789	34.899469
1082.176097	101867.511670	34.904487
1083.127130	101994.904303	34.909504
1084.198756	102125.177404	34.914522
1084.841626	102247.690076	34.919540
1085.527599	102377.857181	34.924557
1086.100068	102518.572818	34.929575
1086.921953	102653.530758	34.934592
1087.681550	102800.155941	34.939610
1088.198948	102956.648457	34.944628
1088.605897	103126.576728	34.949645
1089.715750	103294.990799	34.954663
1090.237652	103458.912589	34.959680
1091.097267	103634.980822	34.964698
1092.058896	103800.649382	34.969716
1092.769372	103984.304693	34.974733
1093.458966	104164.564568	34.979751
1094.138911	104349.690155	34.984768
1095.024584	104538.955824	34.989786
1096.288402	104730.332305	34.994804
1097.328124	104919.815928	34.999821
1098.545805	105109.923752	35.004839
1100.210702	105288.555043	35.009856
1101.967401	105478.367611	35.014874
1103.288532	105648.281778	35.019892
1104.441053	105824.544434	35.024909
1105.592066	106005.988312	35.029927
1106.842686	106175.575596	35.034944
1107.849482	106359.059393	35.039962
1109.131688	106535.064782	35.044980
1110.346242	106711.500455	35.049997
1111.079296	106889.574583	35.055015
1112.441133	107072.346159	35.060032
1113.412821	107262.997786	35.065050
1114.473099	107445.530425	35.070068
1116.059221	107621.530880	35.075085
1116.948632	107793.341287	35.080103
1118.441896	107975.654114	35.085120
1119.347738	108157.317894	35.090138
1120.440211	108335.304402	35.095156
1121.217585	108522.324111	35.100173
1122.072027	108721.402929	35.105191
1123.414889	108908.116670	35.110208
1124.398363	109104.871847	35.115226
1125.453111	109281.984267	35.120244
1126.371017	109491.368525	35.125261
1127.512130	109697.842322	35.130279
1128.380028	109895.319014	35.135296
1129.584602	110090.803607	35.140314
1130.583543	110301.320768	35.145332
1131.405570	110518.556770	35.150349
1132.541323	110738.174745	35.155367
1133.545011	110946.973465	35.160384
1134.437690	111170.979806	35.165402
1135.727668	111381.343310	35.170420
1137.862359	111595.571825	35.175437
1139.212922	111776.603913	35.180455
1140.906901	111988.691502	35.185472
1142.192556	112190.967537	35.190490
1143.114265	112381.156982	35.195508
1144.334857	112577.049509	35.200525
1145.327596	112786.560835	35.205543
1146.428971	112966.248479	35.210560
1147.396839	113173.131954	35.215578
1148.822014	113375.216335	35.220596
1150.370797	113578.105217	35.225613
1151.574102	113767.472342	35.230631
1152.752826	113962.887580	35.235648
1153.546065	114155.441441	35.240666
1155.148035	114348.407883	35.245684
1155.919671	114541.221355	35.250701
1157.348926	114736.131947	35.255719
1158.277130	114929.276984	35.260736
1159.021538	115137.922287	35.265754
1160.527209	115327.224793	35.270772
1161.360084	115546.551077	35.275789
1161.959933	115749.194369	35.280807
1163.594005	115939.442670	35.285824
1165.054551	116139.881637	35.290842
1166.357020	116329.338478	35.295860
1167.366913	116533.908827	35.300877
1168.519614	116718.527952	35.305895
1170.036738	116889.024892	35.310912
1170.826685	117078.875440	35.315930
1172.087800	117258.551697	35.320948
1173.129589	117445.753166	35.325965
1173.975525	117631.961936	35.330983
1175.076188	117835.475105	35.336000
1175.694763	118036.256547	35.341018
1176.706781	118239.951950	35.346036
1177.805201	118446.257290	35.351053
1178.481405	118662.998174	35.356071
1179.721578	118888.757669	35.361088
1180.584479	119124.565627	35.366106
1181.305690	119355.102566	35.371124
1182.415710	119595.118266	35.376141
1183.806041	119818.668232	35.381159
1185.371561	120046.879274	35.386176
1186.799986	120282.235894	35.391194
1188.245411	120506.745091	35.396212
1189.176672	120740.084079	35.401229
1190.693007	120962.215564	35.406247
1192.736841	121163.860608	35.411264
1194.123290	121382.075913	35.416282
1195.285414	121601.419639	35.421300
1196.820047	121808.411929	35.426317
1198.128771	122027.734654	35.431335
1199.082308	122229.985198	35.436352
1199.949424	122466.643264	35.441370
1201.223577	122675.788225	35.446388
1202.059506	122898.236793	35.451405
1202.701857	123141.805717	35.456423
1204.288706	123366.833066	35.461440
1205.538527	123608.582111	35.466458
1206.239775	123839.474533	35.471476
1208.007968	124076.085447	35.476493
1208.977378	124303.388844	35.481511
1210.311896	124538.883773	35.486528
1211.217567	124777.442175	35.491546
1212.425669	125023.252272	35.496564
1213.994480	125259.601315	35.501581
1215.023413	125497.181932	35.506599
1216.470268	125739.815500	35.511616
1217.920664	125979.028588	35.516634
1219.367192	126206.191599	35.521652
1220.730711	126432.964459	35.526669
1221.945550	126669.813886	35.531687
1223.529872	126906.198608	35.536704
1224.859366	127119.091612	35.541722
1226.190387	127339.615652	35.546740
1227.474453	127563.406300	35.551757
1228.228919	127800.479923	35.556775
1229.462627	128020.530641	35.561792
1230.598928	128253.184757	35.566810
1232.134525	128477.865801	35.571828
1233.566569	128698.687137	35.576845
1235.017704	128929.038308	35.581863
1236.699206	129137.387689	35.586880
1238.010479	129352.289141	35.591898
1239.211591	129571.088818	35.596916
1240.862377	129792.578985	35.601933
1241.670221	129985.728737	35.606951
1243.478025	130197.892298	35.611968
1243.948843	130416.767761	35.616986
1245.077854	130643.990634	35.622004
1246.388307	130852.083186	35.627021
1247.187887	131081.188881	35.632039
1248.303102	131285.792714	35.637056
1249.594375	131516.265451	35.642074
1250.836071	131719.849840	35.647092
1251.734865	131935.128671	35.652109
1252.591929	132148.298955	35.657127
1254.385948	132351.606108	35.662144
1255.334297	132575.602289	35.667162
1256.502985	132788.497268	35.672180
1258.070841	132991.148649	35.677197
1259.387407	133218.511201	35.682215
1260.939747	133423.576422	35.687232
1262.035142	133648.924940	35.692250
1262.888670	133870.752803	35.697268
1264.289075	134083.757607	35.702285
1265.298915	134313.358966	35.707303
1266.945550	134527.175416	35.712320
1268.199463	134761.493552	35.717338
1269.295760	134985.723019	35.722356
1270.825310	135211.061513	35.727373
1271.395786	135458.986099	35.732391
1272.989824	135678.916644	35.737408
1274.162263	135930.079628	35.742426
1274.925729	136165.781949	35.747444
1276.096110	136408.556362	35.752461
1276.761924	136689.715554	35.757479
1278.132239	136939.547803	35.762496
1278.890615	137195.974097	35.767514
1279.732391	137484.312147	35.772532
1281.328248	137750.328647	35.777549
1282.684727	138022.637215	35.782567
1284.111698	138289.243761	35.787584
1285.703932	138567.552820	35.792602
1286.526413	138848.349479	35.797620
1288.403217	139114.774270	35.802637
1289.714876	139387.012622	35.807655
1290.856171	139659.953285	35.812672
1292.441813	139941.799598	35.817690
1293.358671	140223.048615	35.822708
1295.251179	140478.793073	35.827725
1296.586407	140760.598788	35.832743
1297.877621	141032.371959	35.837760
1299.628396	141296.121355	35.842778
1300.552719	141569.341435	35.847796
1302.038351	141846.997733	35.852813
1303.040134	142131.050718	35.857831
1303.982670	142401.865245	35.862848
1305.197822	142679.484149	35.867866
1306.553187	142967.137530	35.872884
1308.003706	143244.100791	35.877901
1309.381872	143534.899833	35.882919
1310.540936	143826.675825	35.887936
1312.231937	144099.358238	35.892954
1314.064047	144368.164556	35.897972
1316.302372	144630.070946	35.902989
1317.401269	144904.302961	35.908007
1319.117351	145145.515413	35.913024
1321.238528	145400.446977	35.918042
1322.675753	145649.710656	35.923060
1324.038062	145886.560832	35.928077
1325.315474	146125.316119	35.933095
1326.561929	146375.580160	35.938112
1327.728960	146625.060132	35.943130
1328.485889	146867.140072	35.948148
1329.983485	147114.780795	35.953165
1330.816268	147374.631359	35.958183
1332.244249	147638.532534	35.963200
1333.356638	147895.563379	35.968218
1334.479898	148152.962037	35.973236
1335.609768	148419.429159	35.978253
1336.998073	148682.786483	35.983271
1338.090695	148939.219237	35.988288
1339.325203	149188.693100	35.993306
1340.413796	149457.990121	35.998324
1341.514129	149703.101489	36.003341
1343.033568	149973.789683	36.008359
1344.249837	150223.882362	36.013376
1345.561845	150493.035941	36.018394
1346.756591	150765.356201	36.023412
1348.359761	151032.664668	36.028429
1349.383161	151294.756512	36.033447
1350.894959	151563.529747	36.038464
1352.513499	151843.841795	36.043482
1353.436465	152111.511233	36.048500
1354.779382	152394.067111	36.053517
1356.118035	152665.312047	36.058535
1357.769058	152942.176985	36.063552
1358.775505	153227.661144	36.068570
1359.866484	153510.571354	36.073588
1361.527998	153795.330154	36.078605
1362.839098	154087.746665	36.083623
1364.058169	154385.469894	36.088640
1365.296964	154679.450320	36.093658
1366.540213	154985.292131	36.098676
1368.140225	155275.843452	36.103693
1370.508259	155547.091167	36.108711
1372.359537	155820.848830	36.113728
1374.200501	156086.707541	36.118746
1375.339442	156395.393691	36.123764
1376.625640	156664.912330	36.128781
1377.636976	156942.165290	36.133799
1379.062525	157224.666895	36.138816
1380.297662	157509.891207	36.143834
1381.425660	157802.137527	36.148852
1383.339559	158073.401562	36.153869
1385.200182	158355.052937	36.158887
1386.371784	158652.309061	36.163904
1388.197071	158920.954896	36.168922
1389.540842	159193.513084	36.173940
1390.981492	159477.284067	36.178957
1392.061714	159756.854069	36.183975
1393.112923	160038.955302	36.188992
1394.784761	160316.921902	36.194010
1395.991901	160621.937865	36.199028
1397.081605	160897.302346	36.204045
1398.576407	161194.371578	36.209063
1399.882355	161480.145147	36.214080
1401.338653	161780.371204	36.219098
1402.484647	162088.427549	36.224116
1403.821115	162382.283701	36.229133
1405.206498	162682.045905	36.234151
1406.688528	162986.818324	36.239168
1408.073272	163282.943815	36.244186
1409.255753	163586.387155	36.249204
1411.002986	163882.038377	36.254221
1412.111673	164189.190201	36.259239
1413.270792	164501.309369	36.264256
1414.750451	164794.816218	36.269274
1415.730919	165135.237126	36.274292
1417.474256	165443.409774	36.279309
1418.821111	165757.346853	36.284327
1420.258977	166063.201758	36.289344
1421.793059	166374.092736	36.294362
1423.168327	166696.596289	36.299380
1424.431233	167014.515004	36.304397
1425.885477	167337.974570	36.309415
1426.561202	167653.863226	36.314432
1428.799106	167967.072871	36.319450
1430.367866	168290.507869	36.324468
1431.748485	168582.026538	36.329485
1433.535706	168877.007459	36.334503
1434.806574	169187.822233	36.339520
1436.338829	169478.078256	36.344538
1438.236083	169757.883740	36.349556
1439.848171	170039.083057	36.354573
1441.444742	170321.530215	36.359591
1442.357292	170610.423885	36.364608
1445.722181	170868.321069	36.369626
1447.644021	171131.343222	36.374644
1449.024947	171396.194596	36.379661
1450.546666	171650.124075	36.384679
1451.657438	171930.161572	36.389696
1453.295103	172189.112618	36.394714
1454.530526	172466.747170	36.399732
1455.554938	172733.670034	36.404749
1456.599629	173015.184322	36.409767
1457.861722	173297.362374	36.414784
1458.927587	173584.752002	36.419802
1459.717617	173884.257104	36.424820
1460.853069	174188.681623	36.429837
1462.527282	174484.478711	36.434855
1463.565932	174805.864552	36.439872
1464.940974	175113.313820	36.444890
1466.380866	175430.462536	36.449908
1467.794280	175751.907111	36.454925
1469.294487	176075.471530	36.459943
1470.801064	176405.928101	36.464960
1472.829052	176717.620081	36.469978
1474.292056	177049.598423	36.474996
1475.255021	177385.316524	36.480013
1476.759235	177712.076582	36.485031
1478.058194	178037.565496	36.490048
1479.740801	178358.652858	36.495066
1481.459753	178698.646285	36.500084
1483.046920	179027.660375	36.505101
1484.620496	179366.628956	36.510119
1486.153088	179695.301070	36.515136
1487.502455	180026.759638	36.520154
1488.696645	180361.571202	36.525172
1490.473931	180705.744115	36.530189
1492.025770	181032.061033	36.535207
1493.163392	181393.452744	36.540224
1494.508280	181724.669218	36.545242
1495.789566	182071.103450	36.550260
1497.403463	182420.188539	36.555277
1498.902558	182785.236407	36.560295
1500.438370	183130.049122	36.565312
1502.499553	183477.036652	36.570330
1504.126504	183823.628489	36.575348
1505.044178	184175.695908	36.580365
1506.604714	184523.661362	36.585383
1508.045912	184900.626385	36.590400
1509.387910	185265.247552	36.595418
1510.666933	185604.102174	36.600436
1512.133044	185986.223969	36.605453
1513.815948	186349.768000	36.610471
1514.660263	186713.630517	36.615488
1516.575260	187083.576540	36.620506
1517.932570	187453.528199	36.625524
1519.409310	187824.401915	36.630541
1521.172252	188185.621843	36.635559
1522.724175	188557.351143	36.640576
1524.000559	188920.458544	36.645594
1526.070297	189295.128322	36.650612
1527.809484	189660.461632	36.655629
1529.719645	190019.079335	36.660647
1531.002389	190376.101791	36.665664
1532.723315	190711.436079	36.670682
1534.779421	191054.727004	36.675700
1536.349159	191369.055763	36.680717
1538.026156	191694.349073	36.685735
1539.560708	192028.909182	36.690752
1540.918789	192361.786537	36.695770
1542.400668	192687.790272	36.700788
1543.499269	193041.190474	36.705805
1544.788789	193379.645002	36.710823
1546.172631	193729.574585	36.715840
1547.320820	194074.403658	36.720858
1549.177059	194432.891778	36.725876
1550.337982	194788.475311	36.730893
1552.109702	195139.326407	36.735911
1553.719474	195507.154156	36.740928
1555.438792	195860.518874	36.745946
1557.191235	196211.950427	36.750964
1558.878288	196574.388857	36.755981
1560.465332	196932.402462	36.760999
1562.247161	197297.419204	36.766016
1563.582192	197655.300673	36.771034
1564.713624	198014.119096	36.776052
1565.985844	198379.581483	36.781069
1568.383568	198737.547442	36.786087
1570.002995	199110.218551	36.791104
1571.934369	199466.627639	36.796122
1573.432638	199834.917319	36.801140
1574.914607	200206.423797	36.806157
1576.117824	200574.271050	36.811175
1577.592909	200954.568445	36.816192
1579.160629	201329.113969	36.821210
1581.103055	201692.566620	36.826228
1582.841626	202062.542649	36.831245
1584.933893	202412.833605	36.836263
1586.253162	202802.968472	36.841280
1587.687974	203172.708443	36.846298
1589.289600	203534.741352	36.851316
1590.698261	203931.876185	36.856333
1592.313435	204287.321061	36.861351
1593.761534	204679.565235	36.866368
1595.493378	205046.739125	36.871386
1596.997631	205430.280678	36.876404
1598.463119	205821.778943	36.881421
1600.236612	206193.357502	36.886439
1601.796739	206580.933415	36.891456
1603.282882	206975.087977	36.896474
1605.084706	207364.354824	36.901492
1606.074052	207751.434087	36.906509
1607.896792	208141.653704	36.911527
1608.946143	208543.481394	36.916544
1610.687399	208942.200354	36.921562
1612.576592	209347.093338	36.926580
1614.113283	209742.866129	36.931597
1616.004557	210133.439781	36.936615
1617.831684	210530.781120	36.941632
1619.476967	210926.427487	36.946650
1621.437628	211308.144906	36.951668
1623.064070	211701.258506	36.956685
1624.871866	212093.836108	36.961703
1626.216328	212494.263211	36.966720
1627.872287	212883.441040	36.971738
1629.276831	213280.382621	36.976756
1630.751385	213678.279539	36.981773
1632.328480	214068.466172	36.986791
1633.812578	214483.101546	36.991808
1635.283560	214883.518777	36.996826
1636.916246	215301.308045	37.001844
1638.277410	215700.223209	37.006861
1639.979943	216089.229680	37.011879
1641.126045	216482.240788	37.016896
1642.767277	216863.590646	37.021914
1644.386760	217294.140638	37.026932
1645.921800	217746.929459	37.031949
1647.211428	218139.009480	37.036967
1649.151632	218545.587518	37.041984
1650.930315	218948.206424	37.047002
1652.549815	219346.687959	37.052020
1654.333950	219768.815021	37.057037
1655.993512	220158.607013	37.062055
1657.888135	220569.721749	37.067072
1659.624380	220976.114753	37.072090
1661.516887	221374.051247	37.077108
1663.402779	221781.489449	37.082125
1664.795917	222193.404510	37.087143
1666.521275	222597.799081	37.092160
1667.922353	223020.459723	37.097178
1670.074088	223430.095431	37.102196
1671.424019	223852.259736	37.107213
1672.738958	224255.839164	37.112231
1674.422270	224684.910988	37.117248
1675.930026	225122.166607	37.122266
1678.070212	225544.435412	37.127284
1679.884286	225969.655104	37.132301
1681.594241	226379.374280	37.137319
1683.842500	226800.080353	37.142336
1685.663123	227207.142504	37.147354
1687.474444	227637.651706	37.152372
1688.762158	228070.280790	37.157389
1690.417209	228483.292644	37.162407
1691.639090	228912.760442	37.167424
1693.416284	229359.765858	37.172442
1695.252442	229783.242304	37.177460
1696.553380	230228.322600	37.182477
1698.132574	230652.657000	37.187495
1699.940840	231100.983919	37.192512
1701.509564	231541.807791	37.197530
1703.450841	231992.350878	37.202548
1704.790263	232440.530791	37.207565
1706.791339	232885.275394	37.212583
1708.829147	233327.017951	37.217600
1710.410165	233769.294387	37.222618
1713.201060	234205.225408	37.227636
1714.632618	234649.942137	37.232653
1716.660674	235093.063026	37.237671
1718.305711	235523.141211	37.242688
1719.822259	235972.267409	37.247706
1721.445052	236408.879741	37.252724
1722.910126	236848.821420	37.257741
1724.662685	237284.068287	37.262759
1726.403371	237728.183382	37.267776
1728.405692	238182.290109	37.272794
1729.965215	238613.634767	37.277812
1731.902652	239058.330268	37.282829
1733.605625	239504.462594	37.287847
1735.568710	239939.376145	37.292864
1737.098798	240385.564389	37.297882
1738.833967	240825.191434	37.302900
1740.442021	241269.311159	37.307917
1742.125538	241715.527745	37.312935
1743.774881	242175.315695	37.317952
1745.268763	242628.068392	37.322970
1747.732611	243054.776944	37.327988
1749.887449	243499.852394	37.333005
1751.809896	243934.272568	37.338023
1753.977877	244363.064447	37.343040
1755.465924	244769.919811	37.348058
1757.633481	245166.299452	37.353076
1759.018858	245588.821009	37.358093
1760.527921	245988.866857	37.363111
1761.706519	246414.167265	37.368128
1763.331882	246841.604627	37.373146
1765.050584	247251.423079	37.378164
1766.353634	247688.567853	37.383181
1768.007062	248120.574853	37.388199
1769.852028	248553.947975	37.393216
1771.604913	248981.443362	37.398234
1773.425030	249411.239837	37.403252
1775.016366	249853.090154	37.408269
1776.995698	250288.805654	37.413287
1778.423919	250747.653081	37.418304
1779.821235	251200.358569	37.423322
1781.422819	251649.017137	37.428340
1782.961524	252120.015830	37.433357
1784.712389	252595.273103	37.438375
1786.751615	253070.076788	37.443392
1788.107274	253551.725486	37.448410
1790.090462	254025.650097	37.453428
1791.521580	254500.021781	37.458445
1793.452536	254974.692383	37.463463
1795.207122	255471.366177	37.468480
1796.981499	255952.032961	37.473498
1799.167687	256446.629260	37.478516
1800.597813	256946.609001	37.483533
1802.298268	257437.729422	37.488551
1804.301136	257942.111456	37.493568
1806.379694	258450.240847	37.498586
1808.266681	258957.741481	37.503604
1810.085957	259448.004534	37.508621
1811.957383	259932.187652	37.513639
1814.158927	260442.989816	37.518656
1815.947468	260938.592723	37.523674
1817.937929	261436.245362	37.528692
1820.347165	261930.501024	37.533709
1822.049929	262428.759845	37.538727
1823.763104	262909.793398	37.543744
1825.732402	263406.331368	37.548762
1827.388704	263908.865159	37.553780
1829.066826	264419.524178	37.558797
1830.549536	264917.234121	37.563815
1832.664631	265430.310040	37.568832
1833.784450	265955.514736	37.573850
1835.462496	266463.606831	37.578868
1837.036531	267001.234194	37.583885
1838.887926	267529.416173	37.588903
1840.719901	268050.767429	37.593920
1842.450234	268584.480855	37.598938
1844.214097	269111.761204	37.603956
1846.471882	269653.921878	37.608973
1848.331232	270171.100244	37.613991
1850.838647	270695.614142	37.619008
1852.641805	271222.174149	37.624026
1854.669667	271752.074944	37.629044
1856.751310	272273.532335	37.634061
1858.593803	272795.892086	37.639079
1860.673798	273315.519138	37.644096
1862.475228	273834.454611	37.649114
1864.866568	274341.835269	37.654132
1866.681762	274850.173782	37.659149
1868.918839	275353.894722	37.664167
1870.996131	275863.509087	37.669184
1872.518476	276367.523850	37.674202
1874.625352	276859.857674	37.679220
1876.529892	277375.263895	37.684237
1878.160646	277869.782629	37.689255
1879.976424	278357.817612	37.694272
1881.444496	278849.287408	37.699290
1883.946821	279314.091014	37.704308
1885.900563	279798.213538	37.709325
1887.670269	280271.544020	37.714343
1889.766305	280738.164254	37.719360
1891.442294	281220.525709	37.724378
1893.280917	281701.563656	37.729396
1895.270981	282170.865170	37.734413
1896.935301	282661.404325	37.739431
1898.908296	283136.828043	37.744448
1900.011550	283627.050717	37.749466
1901.675896	284141.971400	37.754484
1903.452131	284642.926673	37.759501
1904.934110	285161.608379	37.764519
1906.964660	285672.933188	37.769536
1908.500946	286202.321996	37.774554
1910.044936	286733.739859	37.779572
1911.611922	287270.918154	37.784589
1913.471190	287815.285621	37.789607
1915.675520	288348.900411	37.794624
1917.369413	288899.107968	37.799642
1920.406888	289440.785765	37.804660
1922.321856	289969.997137	37.809677
1924.325987	290530.002582	37.814695
1926.722775	291073.735499	37.819712
1928.549386	291605.977716	37.824730
1930.510042	292146.095119	37.829748
1932.627565	292684.050777	37.834765
1933.991265	293230.002481	37.839783
1936.221604	293780.584016	37.844800
1937.943381	294341.000461	37.849818
1940.254180	294897.227804	37.854836
1942.752906	295436.276876	37.859853
1944.764026	295974.743502	37.864871
1946.976174	296502.481356	37.869888
1948.557039	297054.678658	37.874906
1950.776839	297589.420309	37.879924
1952.699400	298131.370875	37.884941
1954.398595	298695.528693	37.889959
1956.241488	299239.874297	37.894976
1957.706049	299800.737715	37.899994
1960.074267	300350.070585	37.905012
1962.171339	300916.030267	37.910029
1964.187982	301477.555377	37.915047
1966.388271	302020.252557	37.920064
1968.378523	302581.394781	37.925082
1970.401921	303126.756353	37.930100
1972.384713	303680.731265	37.935117
1974.449670	304233.013149	37.940135
1976.763991	304784.158553	37.945152
1978.520693	305332.979913	37.950170
1980.716997	305879.820687	37.955188
1982.894889	306425.264348	37.960205
1984.789109	306980.198975	37.965223
1986.833671	307518.216677	37.970240
1988.981773	308065.458203	37.975258
1991.145744	308598.827348	37.980276
1993.534893	309134.213068	37.985293
1995.448844	309672.340303	37.990311
1997.728491	310208.473664	37.995328
1999.471967	310755.535808	38.000346
2001.260153	311286.232335	38.005364
2003.216318	311815.754870	38.010381
2004.827641	312368.744880	38.015399
2006.982838	312915.394187	38.020416
2008.713328	313465.385602	38.025434
2009.986315	314011.131502	38.030452
2011.714999	314547.808785	38.035469
2013.474634	315097.682038	38.040487
2015.633180	315628.973341	38.045504
2016.840507	316185.227316	38.050522
2018.834313	316721.997534	38.055540
2020.614655	317277.285288	38.060557
2022.823210	317844.204326	38.065575
2024.676098	318412.955005	38.070592
2026.787809	318965.991132	38.075610
2029.252236	319531.889459	38.080628
2031.267915	320108.521905	38.085645
2032.944624	320678.730429	38.090663
2035.048023	321250.133372	38.095680
2037.356845	321831.247941	38.100698
2038.658026	322413.717017	38.105716
2041.278968	322993.652678	38.110733
2042.812124	323591.688579	38.115751
2044.861821	324171.352464	38.120768
2047.015875	324789.130338	38.125786
2048.976906	325381.086813	38.130804
2050.993882	325978.055696	38.135821
2052.854936	326587.536309	38.140839
2054.892564	327202.491290	38.145856
2056.976998	327823.373437	38.150874
2058.645806	328443.099098	38.155892
2060.834583	329077.204142	38.160909
2062.330279	329715.529650	38.165927
2064.391857	330347.763317	38.170944
2066.455693	330999.639949	38.175962
2068.065400	331662.094573	38.180980
2070.059294	332317.775942	38.185997
2071.960165	332977.044641	38.191015
2073.783458	333644.772162	38.196032
2075.928138	334314.291883	38.201050
2077.913384	334990.785554	38.206068
2080.886442	335669.824220	38.211085
2082.503308	336363.623879	38.216103
2084.966267	337023.741366	38.221120
2087.256542	337693.296897	38.226138
2089.466728	338370.548628	38.231156
2091.737954	339043.846993	38.236173
2093.902807	339738.882667	38.241191
2095.895222	340411.066928	38.246208
2098.219324	341094.863847	38.251226
2100.118587	341763.238112	38.256244
2102.458782	342446.024103	38.261261
2104.527505	343142.729470	38.266279
2107.160658	343801.259369	38.271296
2110.005228	344475.913459	38.276314
2111.828775	345150.345838	38.281332
2114.316521	345808.973991	38.286349
2116.792913	346475.538966	38.291367
2119.322859	347123.203058	38.296384
2121.674825	347772.359598	38.301402
2123.782041	348433.272683	38.306420
2126.224879	349071.457653	38.311437
2128.043209	349719.076058	38.316455
2129.784631	350376.087883	38.321472
2131.696100	351030.042185	38.326490
2133.558317	351690.872389	38.331508
2135.912820	352359.072481	38.336525
2137.327170	353025.793445	38.341543
2139.515186	353680.754393	38.346560
2141.659461	354356.698601	38.351578
2143.871200	355034.676569	38.356596
2146.189543	355703.009131	38.361613
2148.467998	356354.768154	38.366631
2151.429380	356995.417476	38.371648
2153.782906	357624.256938	38.376666
2156.041415	358248.256288	38.381684
2157.932934	358869.439644	38.386701
2160.021658	359493.067692	38.391719
2161.850200	360112.644235	38.396736
2163.942982	360732.446903	38.401754
2165.396007	361374.190595	38.406772
2167.484491	362005.087265	38.411789
2169.222635	362663.102451	38.416807
2171.145085	363307.731553	38.421824
2173.638366	363960.983302	38.426842
2175.136949	364631.360470	38.431860
2177.388037	365301.906481	38.436877
2179.356236	365985.222638	38.441895
2181.513507	366656.014356	38.446912
2183.512495	367337.474906	38.451930
2185.754242	368035.169048	38.456948
2188.154128	368722.956552	38.461965
2190.023314	369424.922696	38.466983
2192.412614	370117.531334	38.472000
2194.922726	370798.997073	38.477018
2197.404655	371496.485521	38.482036
2199.965588	372192.222888	38.487053
2201.938508	372888.525850	38.492071
2204.657371	373586.417130	38.497088
2207.294628	374261.988887	38.502106
2209.522111	374944.615512	38.507124
2211.846160	375641.365120	38.512141
2214.270009	376337.349047	38.517159
2216.395747	377012.065076	38.522176
2219.135761	377696.126254	38.527194
2221.227064	378392.073339	38.532212
2223.897076	379076.879565	38.537229
2225.851476	379760.851840	38.542247
2228.272740	380453.051004	38.547264
2230.840677	381125.305827	38.552282
2232.928631	381818.901323	38.557300
2235.226959	382497.030749	38.562317
2237.451868	383183.424686	38.567335
2239.704549	383858.161465	38.572352
2241.955831	384550.633439	38.577370
2244.247916	385244.630702	38.582388
2246.626863	385922.296041	38.587405
2248.711973	386608.768075	38.592423
2250.979195	387294.536280	38.597440
2253.105996	387992.406208	38.602458
2255.049439	388690.367154	38.607476
2257.098792	389394.835982	38.612493
2258.807773	390106.494182	38.617511
2261.068546	390822.582974	38.622528
2263.245583	391521.076344	38.627546
2265.020160	392263.905500	38.632564
2267.513178	392975.140643	38.637581
2269.622513	393716.890918	38.642599
2271.731185	394459.459733	38.647616
2274.056753	395190.061610	38.652634
2275.743612	395931.295126	38.657652
2278.037770	396675.299587	38.662669
2280.121507	397432.651618	38.667687
2282.421459	398204.318857	38.672704
2284.703883	398948.471003	38.677722
2286.526691	399715.818179	38.682740
2288.464901	400483.506284	38.687757
2290.916011	401240.395352	38.692775
2293.578910	402016.007278	38.697792
2295.922443	402778.296592	38.702810
2298.639139	403555.074268	38.707828
2301.226029	404303.421866	38.712845
2303.273802	405044.059690	38.717863
2305.392639	405776.938314	38.722880
2307.716633	406524.332606	38.727898
2309.680502	407264.824066	38.732916
2312.144877	408010.457632	38.737933
2314.113847	408759.294201	38.742951
2315.796506	409526.752752	38.747968
2317.995006	410279.081913	38.752986
2320.049464	411059.330578	38.758004
2322.416049	411824.660665	38.763021
2324.782845	412604.736988	38.768039
2326.916015	413386.779471	38.773056
2329.194583	414184.378053	38.778074
2331.236014	414985.056444	38.783092
2333.937636	415780.333311	38.788109
2336.455315	416587.900087	38.793127
2338.795594	417382.630425	38.798144
2341.330087	418172.087188	38.803162
2343.468373	419006.334411	38.808180
2345.916184	419799.680761	38.813197
2348.307043	420617.043719	38.818215
2350.376338	421440.434776	38.823232
2353.257063	422245.154917	38.828250
2355.429777	423079.743406	38.833268
2357.930151	423899.665564	38.838285
2360.582189	424730.878648	38.843303
2362.916015	425550.874832	38.848320
2365.800574	426367.309643	38.853338
2368.289021	427202.871286	38.858356
2370.984837	428021.560300	38.863373
2373.556393	428833.153893	38.868391
2375.937040	429651.586417	38.873408
2378.738771	430461.821302	38.878426
2381.709378	431270.785804	38.883444
2383.746026	432086.862691	38.888461
2386.536715	432887.904369	38.893479
2388.613692	433693.339079	38.898496
2391.052062	434505.823587	38.903514
2393.298430	435321.803901	38.908532
2395.908084	436134.608102	38.913549
2398.710671	436938.393418	38.918567
2400.745968	437758.320691	38.923584
2403.326349	438570.689152	38.928602
2405.528795	439385.216395	38.933620
2408.294998	440201.645583	38.938637
2410.648871	441019.327640	38.943655
2412.702539	441846.542471	38.948672
2415.711986	442645.486212	38.953690
2418.049937	443458.173365	38.958708
2420.481935	444266.615677	38.963725
2423.074244	445085.323086	38.968743
2425.110207	445915.677264	38.973760
2427.241504	446735.309566	38.978778
2429.323951	447563.974323	38.983796
2431.910015	448392.423120	38.988813
2434.617887	449214.294544	38.993831
2437.097903	450036.374339	38.998848
2439.824786	450852.767303	39.003866
2442.970520	451681.046978	39.008884
2445.514222	452483.346448	39.013901
2448.344979	453285.062272	39.018919
2450.802932	454110.426421	39.023936
2453.312685	454902.979478	39.028954
2455.615226	455715.460646	39.033972
2457.740867	456527.433420	39.038989
2460.014245	457339.754376	39.044007
2462.119534	458147.570795	39.049024
2464.433758	458961.489281	39.054042
2466.445035	459753.583707	39.059060
2468.699028	460542.169296	39.064077
2471.076715	461351.330128	39.069095
2472.939709	462147.096169	39.074112
2475.086851	462954.562115	39.079130
2477.284607	463775.483572	39.084148
2479.977052	464589.010813	39.089165
2482.282957	465416.367009	39.094183
2484.513139	466242.437379	39.099200
2487.681055	467059.979206	39.104218
2490.289919	467912.399830	39.109236
2492.397447	468745.308322	39.114253
2495.035771	469580.771803	39.119271
2497.468523	470446.602503	39.124288
2499.846224	471287.896542	39.129306
2502.460540	472140.028447	39.134324
2504.731257	472997.837677	39.139341
2507.432071	473859.629560	39.144359
2509.968360	474729.543023	39.149376
2512.703344	475573.720431	39.154394
2514.959216	476451.885294	39.159412
2517.333627	477331.858297	39.164429
2519.968834	478203.109308	39.169447
2522.329037	479099.669357	39.174464
2524.805176	479985.358430	39.179482
2527.501566	480867.988762	39.184500
2529.958253	481765.059294	39.189517
2532.595480	482646.249824	39.194535
2535.962045	483543.941004	39.199552
2538.928090	484426.000568	39.204570
2541.479628	485308.337655	39.209588
2543.854285	486206.715811	39.214605
2546.751869	487082.546713	39.219623
2549.265318	487969.857536	39.224640
2551.656607	488863.050288	39.229658
2554.128888	489767.743989	39.234676
2556.557483	490660.687876	39.239693
2559.018908	491552.419862	39.244711
2561.378585	492464.967338	39.249728
2563.877202	493363.413802	39.254746
2565.849114	494295.106549	39.259764
2568.467813	495214.884453	39.264781
2570.574228	496143.780205	39.269799
2572.975676	497082.314980	39.274816
2575.899195	498024.142757	39.279834
2578.490736	498973.439658	39.284852
2580.488330	499923.386390	39.289869
2583.236821	500879.864873	39.294887
2585.526822	501847.814724	39.299904
2588.086755	502807.593436	39.304922
2590.541538	503780.800579	39.309940
2593.751150	504737.636644	39.314957
2596.483121	505692.528955	39.319975
2599.133010	506663.869098	39.324992
2601.929444	507625.647337	39.330010
2604.396320	508598.162859	39.335028
2606.546555	509566.991541	39.340045
2609.496871	510537.596325	39.345063
2611.720354	511508.615113	39.350080
2614.276582	512486.879913	39.355098
2617.612058	513468.837475	39.360116
2620.424813	514437.866661	39.365133
2623.882607	515401.337209	39.370151
2626.589140	516370.970669	39.375168
2628.972944	517335.658690	39.380186
2632.028754	518281.430789	39.385204
2634.304558	519228.432863	39.390221
2637.493702	520182.230029	39.395239
2639.651709	521096.235638	39.400256
2642.619754	521998.969995	39.405274
2645.331744	522922.649828	39.410292
2647.380278	523824.873826	39.415309
2650.112547	524750.958140	39.420327
2652.462883	525675.336340	39.425344
2654.832705	526592.402346	39.430362
2657.657901	527514.272759	39.435380
2659.895090	528451.341066	39.440397
2662.545686	529385.613663	39.445415
2664.633352	530337.946169	39.450432
2666.955776	531290.984399	39.455450
2669.446858	532257.929200	39.460468
2672.079947	533232.136924	39.465485
2674.632766	534195.822844	39.470503
2677.142387	535188.344449	39.475520
2679.954351	536185.026700	39.480538
2682.684637	537164.995415	39.485556
2684.997971	538165.398069	39.490573
2687.958288	539163.662045	39.495591
2690.587946	540177.056523	39.500608
2693.493682	541194.358701	39.505626
2696.248247	542193.451126	39.510644
2698.967502	543213.557407	39.515661
2702.643988	544209.337143	39.520679
2705.768559	545212.229580	39.525696
2708.826514	546221.096741	39.530714
2712.170598	547210.632276	39.535732
2715.338294	548196.958337	39.540749
2717.757391	549189.975249	39.545767
2720.372243	550194.503535	39.550784
2722.632134	551196.452879	39.555802
2725.804169	552190.185143	39.560820
2728.345534	553209.134533	39.565837
2731.010000	554207.076524	39.570855
2733.333348	555210.781586	39.575872
2735.896369	556230.556082	39.580890
2738.678026	557241.774476	39.585908
2740.955223	558283.452219	39.590925
2744.153649	559298.466823	39.595943
2746.897597	560326.994580	39.600960
2749.960837	561343.684179	39.605978
2753.176161	562378.154580	39.610996
2755.497702	563406.763751	39.616013
2758.647077	564425.160574	39.621031
2761.290135	565470.933753	39.626048
2764.154088	566495.243162	39.631066
2766.854911	567523.064081	39.636084
2769.170022	568578.483658	39.641101
2772.140364	569607.349758	39.646119
2774.546031	570647.120871	39.651136
2777.006379	571698.746180	39.656154
2780.250618	572740.116550	39.661172
2783.158495	573799.726850	39.666189
2785.942328	574847.926693	39.671207
2788.811180	575897.631419	39.676224
2791.526598	576948.979994	39.681242
2794.474121	577979.580347	39.686260
2797.045554	579037.751601	39.691277
2799.900084	580093.127507	39.696295
2802.732169	581155.189275	39.701312
2805.710633	582202.489660	39.706330
2808.706558	583255.315390	39.711348
2811.641748	584296.075229	39.716365
2814.594910	585343.362773	39.721383
2817.735919	586401.911393	39.726400
2820.329968	587444.364247	39.731418
2823.147399	588465.585022	39.736436
2825.954711	589485.568178	39.741453
2828.281974	590492.862749	39.746471
2831.075782	591500.797793	39.751488
2833.546934	592504.641738	39.756506
2836.622904	593518.273572	39.761524
2839.131783	594553.157613	39.766541
2841.672159	595568.556474	39.771559
2844.122762	596606.777561	39.776576
2846.864525	597648.315517	39.781594
2849.822600	598684.415896	39.786612
2852.317287	599726.010111	39.791629
2855.262094	600788.721047	39.796647
2857.754659	601850.858433	39.801664
2860.424069	602929.492704	39.806682
2863.183505	603995.144311	39.811700
2865.378540	605104.193344	39.816717
2868.560392	606196.353684	39.821735
2871.255062	607295.997595	39.826752
2873.759982	608414.384108	39.831770
2876.779436	609518.063427	39.836788
2879.331771	610649.282277	39.841805
2882.165515	611779.440582	39.846823
2885.297856	612922.342788	39.851840
2887.926869	614079.467303	39.856858
2891.181814	615217.162275	39.861876
2893.955006	616389.627898	39.866893
2896.411912	617552.520353	39.871911
2899.049684	618717.960449	39.876928
2901.956748	619892.181755	39.881946
2904.933005	621084.712017	39.886964
2907.830754	622280.223944	39.891981
2910.736867	623474.503543	39.896999
2913.714926	624662.043201	39.902016
2916.683931	625877.985331	39.907034
2919.987404	627085.141469	39.912052
2922.886786	628298.972393	39.917069
2925.890633	629503.107607	39.922087
2929.074948	630708.375460	39.927104
2931.764706	631931.366284	39.932122
2934.930846	633145.298885	39.937140
2938.235747	634378.240979	39.942157
2941.020299	635585.364278	39.947175
2944.242867	636794.322654	39.952192
2947.516666	638017.606359	39.957210
2950.694279	639230.481512	39.962228
2953.793515	640426.361696	39.967245
2957.007701	641636.702904	39.972263
2960.789293	642840.472445	39.977280
2963.440747	644024.932844	39.982298
2966.996827	645223.271384	39.987316
2970.279529	646407.899448	39.992333
2973.505434	647587.362245	39.997351
2976.811307	648782.977747	40.002368
2979.716065	649963.362441	40.007386
2982.780505	651132.566058	40.012404
2985.280280	652310.448177	40.017421
2988.696925	653480.116464	40.022439
2991.385298	654647.973308	40.027456
2994.037452	655843.748651	40.032474
2997.400681	657011.613863	40.037492
3000.667489	658171.486320	40.042509
3002.940100	659362.364112	40.047527
3006.020993	660530.853133	40.052544
3009.264022	661724.021987	40.057562
3012.572880	662882.382001	40.062580
3015.338263	664069.814774	40.067597
3017.992362	665251.794018	40.072615
3020.844006	666415.330571	40.077632
3024.031324	667560.805993	40.082650
3026.570608	668699.285104	40.087668
3029.628703	669853.313787	40.092685
3032.191558	670999.523840	40.097703
3035.334434	672140.028476	40.102720
3037.680926	673308.327153	40.107738
3040.306929	674464.450862	40.112756
3043.411590	675644.865411	40.117773
3046.378127	676821.425340	40.122791
3049.438896	677997.920824	40.127808
3052.594803	679172.015295	40.132826
3055.579958	680373.371147	40.137844
3058.477179	681570.809067	40.142861
3061.107132	682775.935510	40.147879
3064.207611	683997.517257	40.152896
3067.202804	685227.049385	40.157914
3070.435155	686448.083294	40.162932
3073.535619	687672.153017	40.167949
3076.796684	688894.988470	40.172967
3080.128331	690134.028690	40.177984
3083.117944	691379.903804	40.183002
3086.487763	692613.880926	40.188020
3089.404965	693861.755745	40.193037
3092.413407	695105.223896	40.198055
3095.788579	696364.381773	40.203072
3098.816135	697623.219765	40.208090
3102.172140	698885.097551	40.213108
3104.982949	700144.157253	40.218125
3107.955858	701423.733726	40.223143
3111.323458	702691.607183	40.228160
3113.742891	703973.181985	40.233178
3116.823244	705257.283888	40.238196
3119.852771	706566.474260	40.243213
3122.421259	707864.544007	40.248231
3125.641602	709179.102979	40.253248
3128.383426	710509.982438	40.258266
3131.446114	711839.265097	40.263284
3134.505274	713171.906023	40.268301
3137.462125	714516.186264	40.273319
3140.673585	715867.685149	40.278336
3143.919809	717221.287963	40.283354
3147.183632	718560.519041	40.288372
3150.503371	719922.185174	40.293389
3153.445347	721275.184078	40.298407
3156.968747	722624.158390	40.303424
3160.241518	724001.288321	40.308442
3163.853408	725346.541634	40.313460
3167.170906	726705.810889	40.318477
3170.408477	728077.174992	40.323495
3174.373366	729414.143082	40.328512
3177.732515	730774.312135	40.333530
3181.086674	732101.800054	40.338548
3184.642741	733438.965108	40.343565
3187.907446	734782.574411	40.348583
3191.422747	736111.896397	40.353600
3194.243890	737436.867490	40.358618
3197.529616	738774.326676	40.363636
3200.436556	740117.299552	40.368653
3203.259067	741456.754044	40.373671
3206.460053	742804.405430	40.378688
3209.264306	744142.225122	40.383706
3212.568088	745493.346844	40.388724
3215.595627	746840.238716	40.393741
3218.643932	748194.882163	40.398759
3221.914514	749547.381117	40.403776
3225.025247	750907.458064	40.408794
3228.478877	752266.304090	40.413812
3231.744335	753607.502917	40.418829
3234.611866	754924.842011	40.423847
3238.152892	756223.721395	40.428864
3241.221380	757548.013817	40.433882
3244.185143	758835.909449	40.438900
3247.931268	760166.971254	40.443917
3250.717019	761484.522742	40.448935
3254.360668	762802.392650	40.453952
3257.292927	764113.360648	40.458970
3260.326526	765434.462413	40.463988
3263.788762	766763.769122	40.469005
3266.781607	768113.765345	40.474023
3269.867946	769428.351369	40.479040
3272.657458	770784.976355	40.484058
3276.147994	772135.389616	40.489076
3279.534630	773488.226619	40.494093
3281.989823	774872.654836	40.499111
3285.752844	776242.657776	40.504128
3289.240968	777616.280118	40.509146
3292.510687	779000.579791	40.514164
3296.087405	780380.982208	40.519181
3299.251961	781786.122140	40.524199
3303.200593	783155.677111	40.529216
3306.648782	784543.157689	40.534234
3310.396961	785919.235620	40.539252
3314.381325	787291.822759	40.544269
3317.607901	788660.691725	40.549287
3321.050412	790037.252808	40.554304
3324.289586	791429.999959	40.559322
3327.850667	792810.316335	40.564340
3330.669881	794183.282935	40.569357
3333.717938	795570.198448	40.574375
3337.259857	796978.992872	40.579392
3340.409320	798366.758290	40.584410
3343.569040	799785.381084	40.589428
3346.788271	801206.837074	40.594445
3349.811022	802635.814502	40.599463
3353.007567	804055.857087	40.604480
3356.025920	805510.903417	40.609498
3359.027905	806947.843154	40.614516
3362.115946	808415.269953	40.619533
3365.218367	809875.486333	40.624551
3368.638276	811334.799351	40.629568
3372.118664	812810.938795	40.634586
3375.724064	814278.723674	40.639604
3379.250990	815742.147944	40.644621
3382.469948	817232.404548	40.649639
3385.908110	818699.397316	40.654656
3389.244379	820193.270483	40.659674
3392.312094	821693.196045	40.664692
3395.799471	823177.979892	40.669709
3398.955716	824678.190317	40.674727
3402.529715	826180.477348	40.679744
3405.905457	827682.502188	40.684762
3409.275594	829187.644027	40.689780
3413.282389	830693.308501	40.694797
3416.156221	832210.844647	40.699815
3419.748540	833716.363743	40.704832
3423.142854	835223.317894	40.709850
3426.338993	836750.302451	40.714868
3429.612926	838280.415685	40.719885
3432.988319	839795.840167	40.724903
3436.330712	841323.559229	40.729920
3439.954516	842856.701685	40.734938
3443.059846	844384.696304	40.739956
3446.703526	845934.012209	40.744973
3449.986349	847470.856057	40.749991
3453.423257	849005.257752	40.755008
3457.527619	850523.868885	40.760013
3460.538742	852006.006926	40.765018
3464.081328	853416.728947	40.770023
3467.177804	854770.455089	40.775028
3470.146287	856063.276687	40.780032
3473.463257	857276.860354	40.785037
3476.289010	858428.901230	40.790042
3479.382773	859506.663952	40.795047
3481.742798	860521.438513	40.800052
3484.673025	861478.486191	40.805056
3487.407202	862355.502363	40.810061
3489.695777	863155.186998	40.815066
3492.152205	863891.076633	40.820071
3493.675670	864581.548965	40.825076
3496.262890	865198.401743	40.830080
3498.292295	865742.021561	40.835085
3499.914818	866256.609729	40.840090
3501.842848	866711.940043	40.845095
3502.837974	867128.824125	40.850100
3504.512511	867467.081099	40.855104
3505.923462	867790.695571	40.860109
3507.245857	868055.253839	40.865114
3508.099679	868278.114401	40.870119
3508.965544	868473.285293	40.875124
3509.817959	868631.158686	40.880128
3510.612041	868755.046870	40.885133
3511.336199	868860.395122	40.890138
3512.243721	868935.606196	40.895143
3513.055640	868974.803289	40.900148
3513.637759	868996.849077	40.905152
3514.232651	868993.352116	40.910157
3515.057729	868952.331632	40.915162
3515.763401	868902.881619	40.920167
3516.385114	868838.877782	40.925172
3516.352988	868741.864267	40.930176
3517.075714	868646.375866	40.935181
3517.585137	868514.598191	40.940186
3517.835467	868368.000555	40.945191
3517.854504	868227.362074	40.950196
3518.517910	868063.692105	40.955200
3518.626350	867886.996507	40.960205
3518.429563	867702.478200	40.965210
3518.721629	867503.400386	40.970215
3518.933411	867308.311959	40.975220
3519.178503	867094.365987	40.980224
3519.588796	866865.424621	40.985229
3519.666580	866647.507354	40.990234
3520.030417	866408.452678	40.995239
3519.767878	866162.884971	41.000244
3519.928011	865930.354545	41.005248
3519.979298	865656.440401	41.010253
3519.981539	865401.761715	41.015258
3520.248828	865138.866003	41.020263
3520.138280	864864.748368	41.025268
3520.004550	864601.312324	41.030272
3520.225096	864322.548037	41.035277
3519.956443	864055.611769	41.040282
3520.124006	863756.419874	41.045287
3520.296368	863493.954535	41.050292
3520.322488	863195.924769	41.055296
3520.107365	862910.460279	41.060301
3520.008770	862633.226462	41.065306
3520.353126	862329.171751	41.070311
3520.110760	862039.684935	41.075316
3519.962051	861739.959917	41.080320
3519.934772	861435.824657	41.085325
3519.847942	861157.063288	41.090330
3520.031096	860854.128502	41.095335
3519.717880	860572.265968	41.100340
3519.284129	860268.042292	41.105344
3519.450674	859980.821857	41.110349
3519.392947	859681.758982	41.115354
3519.725623	859387.577795	41.120359
3519.497398	859096.879370	41.125364
3519.118275	858799.188179	41.130368
3519.274983	858509.273997	41.135373
3518.634774	858218.699117	41.140378
3518.663021	857918.757883	41.145383
3518.460107	857636.644938	41.150388
3518.395944	857338.539225	41.155392
3518.564711	857051.862514	41.160397
3518.464693	856776.796361	41.165402
3518.576051	856464.996388	41.170407
3518.464394	856183.775005	41.175412
3518.237929	855899.056146	41.180416
3518.309772	855599.384131	41.185421
3518.261684	855324.342015	41.190426
3518.313205	855027.760215	41.195431
3518.138088	854745.413134	41.200436
3517.938602	854460.720928	41.205440
3517.689450	854166.386297	41.210445
3517.934563	853899.117806	41.215450
3518.007056	853616.386428	41.220455
3517.506771	853316.211358	41.225460
3517.436172	853035.034859	41.230464
3517.377907	852745.761811	41.235469
3517.279342	852481.702159	41.240474
3517.183885	852194.357086	41.245479
3516.871410	851930.796180	41.250484
3516.478944	851642.111157	41.255488
3516.646214	851374.162587	41.260493
3516.414155	851112.599055	41.265498
3516.502447	850834.121450	41.270503
3516.151862	850582.684909	41.275508
3516.023311	850318.928150	41.280512
3516.095978	850044.898731	41.285517
3515.905254	849799.249112	41.290522
3515.830292	849536.911781	41.295527
3515.732014	849281.387054	41.300532
3515.247251	849021.920962	41.305536
3515.394994	848780.462483	41.310541
3515.046219	848522.707105	41.315546
3515.458509	848279.626775	41.320551
3515.181001	848036.260871	41.325556
3514.805983	847787.639383	41.330560
3514.995258	847539.304910	41.335565
3514.704412	847305.560639	41.340570
3514.523497	847042.941509	41.345575
3514.665434	846809.302424	41.350580
3514.412553	846565.290708	41.355584
3514.755066	846321.366406	41.360589
3514.025955	846097.299055	41.365594
3514.023990	845852.925986	41.370599
3513.858629	845625.727181	41.375604
3513.797624	845400.257738	41.380608
3513.917876	845177.967514	41.385613
3513.623969	844952.617934	41.390618
3513.767554	844722.020978	41.395623
3513.664054	844501.303732	41.400628
3513.521937	844274.247471	41.405632
3513.478287	844039.756369	41.410637
3513.469535	843832.553540	41.415642
3513.217092	843607.441716	41.420647
3513.095902	843391.369289	41.425652
3513.090999	843180.292598	41.430656
3513.248981	842960.307474	41.435661
3512.920124	842755.657755	41.440666
3512.467707	842536.343626	41.445671
3512.655290	842329.839581	41.450676
3512.249913	842129.034795	41.455680
3512.499507	841908.900617	41.460685
3512.079063	841716.424855	41.465690
3512.269994	841515.112284	41.470695
3512.216491	841305.493235	41.475700
3511.871463	841113.620872	41.480704
3511.769051	840907.557393	41.485709
3511.404321	840716.700635	41.490714
3511.849428	840513.656068	41.495719
3511.596620	840329.842417	41.500724
3511.847374	840134.671636	41.505728
3511.984205	839939.074591	41.510733
3511.571218	839740.683736	41.515738
3511.646373	839540.449956	41.520743
3511.563179	839349.749865	41.525748
3511.256427	839156.592588	41.530752
3511.136732	838977.206799	41.535757
3510.934507	838787.631760	41.540762
3511.028934	838596.977550	41.545767
3511.035672	838417.799225	41.550772
3510.999975	838239.208448	41.555776
3511.046293	838056.109681	41.560781
3510.650966	837876.592052	41.565786
3510.807882	837694.391941	41.570791
3510.528329	837527.973129	41.575796
3510.581375	837348.854900	41.580800
3510.769513	837168.879726	41.585805
3510.330827	836996.079777	41.590810
3510.311603	836818.276441	41.595815
3510.289216	836647.058016	41.600820
3510.058996	836495.832922	41.605824
3510.182591	836317.357664	41.610829
3510.426648	836146.667775	41.615834
3510.379784	835986.955778	41.620839
3509.744396	835810.934592	41.625844
3510.036220	835649.010518	41.630848
3509.972336	835485.432319	41.635853
3509.790467	835320.258349	41.640858
3509.400940	835139.784539	41.645863
3509.675700	834997.521788	41.650868
3509.366604	834834.162739	41.655872
3509.495827	834691.966046	41.660877
3509.173329	834532.458699	41.665882
3509.461754	834373.237397	41.670887
3509.300244	834227.074546	41.675892
3509.432067	834068.066831	41.680896
3509.083649	833905.960328	41.685901
3509.123756	833768.934021	41.690906
3509.146344	833612.179333	41.695911
3508.902101	833463.961880	41.700916
3508.725906	833319.685447	41.705920
3508.968132	833169.525397	41.710925
3508.861851	833036.463406	41.715930
3508.462967	832884.351188	41.720935
3508.285651	832737.375864	41.725940
3508.684271	832598.556358	41.730944
3509.024666	832454.273240	41.735949
3508.714069	832313.073530	41.740954
3508.629231	832172.126621	41.745959
3508.656785	832023.489534	41.750964
3508.508800	831878.834462	41.755968
3508.539624	831746.260712	41.760973
3508.288074	831616.612780	41.765978
3508.130482	831473.806478	41.770983
3507.904166	831345.028245	41.775988
3508.319583	831212.038298	41.780992
3508.104785	831073.140672	41.785997
3507.644441	830944.588460	41.791002
3508.084675	830818.963151	41.796007
3507.713969	830684.284315	41.801012
3507.528141	830543.856118	41.806016
3507.716722	830428.866423	41.811021
3507.539667	830306.264295	41.816026
3507.613381	830177.950971	41.821031
3507.263285	830062.066359	41.826036
3507.362404	829936.968823	41.831040
3507.491412	829821.978233	41.836045
3506.968641	829705.089628	41.841050
3507.529419	829570.332052	41.846055
3507.182828	829461.521323	41.851060
3507.050731	829349.985890	41.856064
3507.035554	829232.858619	41.861069
3506.929186	829141.154773	41.866074
3507.084893	829006.892088	41.871079
3506.816321	828899.134209	41.876084
3506.786223	828785.715349	41.881088
3506.761041	828674.297371	41.886093
3506.708094	828577.738708	41.891098
3506.722619	828465.626446	41.896103
3506.459625	828367.828626	41.901108
3506.295429	828245.136779	41.906112
3506.549259	828132.783904	41.911117
3506.303164	828044.899844	41.916122
3506.618175	827931.898077	41.921127
3506.235796	827838.706286	41.926132
3506.384390	827730.860439	41.931136
3506.645343	827631.499007	41.936141
3506.112421	827529.676282	41.941146
3506.479326	827428.632461	41.946151
3506.473732	827323.053736	41.951156
3505.979012	827218.091563	41.956160
3506.038192	827116.360407	41.961165
3505.723121	827027.740837	41.966170
3505.840642	826940.417530	41.971175
3506.015409	826844.235741	41.976180
3505.693115	826743.588190	41.981184
3506.116862	826643.745024	41.986189
3505.816120	826554.921165	41.991194
3505.798404	826456.956641	41.996199
3505.925341	826363.024451	42.001204
3505.606071	826286.470635	42.006208
3505.698458	826187.701758	42.011213
3505.348143	826109.635456	42.016218
3505.595842	826003.798231	42.021223
3505.681483	825936.267111	42.026228
3505.445862	825857.445568	42.031232
3505.666799	825743.443801	42.036237
3505.517983	825678.588799	42.041242
3505.653219	825578.923663	42.046247
3505.446671	825494.176942	42.051252
3505.330712	825422.713385	42.056256
3505.493653	825323.919916	42.061261
3505.378611	825243.897685	42.066266
3505.685375	825156.421717	42.071271
3505.383006	825057.847588	42.076276
3505.067027	824987.390184	42.081280
3505.109979	824891.837214	42.086285
3505.164390	824815.253614	42.091290
3504.908000	824746.397467	42.096295
3505.059512	824660.847555	42.101300
3505.319213	824595.474497	42.106304
3505.342389	824509.356958	42.111309
3505.030753	824425.640709	42.116314
3505.439567	824336.523310	42.121319
3505.251393	824266.623972	42.126324
3504.584425	824194.406504	42.131328
3504.813070	824102.283626	42.136333
3504.672805	824038.486948	42.141338
3504.435091	823969.521800	42.146343
3504.691391	823893.334387	42.151348
3504.755021	823827.545872	42.156352
3504.903937	823743.647296	42.161357
3504.394802	823691.009770	42.166362
3504.866234	823616.006395	42.171367
3504.539345	823538.297003	42.176372
3504.365464	823458.311701	42.181376
3504.895349	823397.381867	42.186381
3504.825227	823328.969333	42.191386
3504.707923	823248.629808	42.196391
3504.572385	823184.677373	42.201396
3504.108893	823109.479876	42.206400
3504.591187	823040.826636	42.211405
3504.254013	822984.242217	42.216410
3504.405789	822913.930180	42.221415
3504.437819	822849.751255	42.226420
3504.331282	822773.953102	42.231424
3504.294079	822712.523411	42.236429
3504.195608	822657.902357	42.241434
3504.507578	822582.081988	42.246439
3504.138526	822518.895304	42.251444
3504.314228	822456.645523	42.256448
3504.149286	822369.797347	42.261453
3503.911498	822342.492043	42.266458
3504.099796	822276.961073	42.271463
3503.839412	822215.465698	42.276468
3503.900915	822164.140626	42.281472
3503.966946	822094.714543	42.286477
3504.162125	822034.561091	42.291482
3503.929051	821983.821253	42.296487
3504.029233	821937.918116	42.301492
3503.832681	821868.337235	42.306496
3504.000640	821812.442316	42.311501
3503.575938	821757.818654	42.316506
3503.857696	821699.751513	42.321511
3504.065118	821649.719307	42.326516
3503.779463	821595.560623	42.331520
3504.079121	821546.539816	42.336525
3503.745124	821482.701477	42.341530
3503.649402	821413.001363	42.346535
3504.008448	821370.769861	42.351540
3503.766353	821307.795333	42.356544
3503.871138	821250.682980	42.361549
3503.629663	821211.533796	42.366554
3503.521266	821140.022674	42.371559
3503.793460	821090.415917	42.376564
3503.555368	821042.556339	42.381568
3503.865398	820988.245654	42.386573
3503.510770	820938.887793	42.391578
3504.082588	820884.630996	42.396583
3503.626098	820824.573922	42.401588
3503.724186	820782.332739	42.406592
3503.880409	820724.179895	42.411597
3503.456392	820671.944684	42.416602
3503.757553	820629.766942	42.421607
3503.788551	820570.899442	42.426612
3503.356436	820505.355320	42.431616
3503.636980	820452.219443	42.436621
3503.578683	820404.178859	42.441626
3503.519516	820354.523333	42.446631
3503.522499	820299.327902	42.451636
3503.304086	820244.951397	42.456640
3503.602388	820202.869287	42.461645
3503.340167	820158.334727	42.466650
3503.274030	820100.017322	42.471655
3503.455130	820069.501928	42.476660
3503.446773	820010.146614	42.481664
3503.452979	819961.798607	42.486669
3503.435416	819917.368938	42.491674
3503.308031	819867.623147	42.496679
3503.122889	819817.739690	42.501684
3503.135069	819789.012509	42.506688
3503.294940	819747.977976	42.511693
3503.095644	819687.281029	42.516698
3503.080677	819640.059710	42.521703
3503.462341	819599.721783	42.526708
3503.129349	819561.899253	42.531712
3503.170619	819508.159076	42.536717
3502.921767	819466.994385	42.541722
3502.967376	819419.712589	42.546727
3503.085772	819389.057593	42.551732
3502.936102	819360.208407	42.556736
3503.155346	819304.969115	42.561741
3503.067305	819274.788050	42.566746
3502.872040	819220.693001	42.571751
3502.834209	819190.356464	42.576756
3502.829733	819163.244350	42.581760
3502.828754	819120.568484	42.586765
3502.840586	819087.482630	42.591770
3502.880687	819044.799512	42.596775
3503.149765	819012.943385	42.601780
3502.913263	818969.522286	42.606784
3503.133562	818927.347094	42.611789
3503.094072	818888.934037	42.616794
3503.209699	818843.251715	42.621799
3503.343891	818803.977538	42.626804
3503.215915	818772.234606	42.631808
3503.212469	818713.747916	42.636813
3502.939405	818670.820329	42.641818
3502.905023	818633.628556	42.646823
3503.075009	818578.244533	42.651828
3502.797450	818547.504060	42.656832
3503.067062	818510.114693	42.661837
3502.797981	818476.142124	42.666842
3502.861038	818438.590599	42.671847
3503.002569	818396.180302	42.676852
3502.869253	818361.450599	42.681856
3502.943688	818324.092341	42.686861
3502.639436	818286.551515	42.691866
3503.081043	818235.867736	42.696871
3503.093594	818206.742106	42.701876
3502.874004	818170.606153	42.706880
3502.961871	818110.777561	42.711885
3502.531023	818091.220349	42.716890
3502.597820	818057.288221	42.721895
3502.760094	818016.193701	42.726900
3502.470933	817988.046837	42.731904
3502.646510	817946.509159	42.736909
3502.485219	817918.487787	42.741914
3502.687822	817875.917283	42.746919
3502.357451	817828.588251	42.751924
3502.223380	817819.603496	42.756928
3502.959197	817787.615704	42.761933
3502.721851	817755.249599	42.766938
3502.544221	817721.845535	42.771943
3502.586257	817685.027502	42.776948
3502.641368	817660.004365	42.781952
3502.763676	817636.781268	42.786957
3502.637654	817601.263191	42.791962
3502.680654	817578.787231	42.796967
3502.853915	817533.429129	42.801972
3502.416054	817496.150629	42.806977
3502.672823	817463.554867	42.811981
3502.466970	817437.399019	42.816986
3502.312283	817409.961862	42.821991
3502.841073	817367.774978	42.826996
3502.774467	817351.386520	42.832001
3502.532461	817304.577712	42.837005
3502.232673	817270.701977	42.842010
3502.410948	817243.160338	42.847015
3502.831666	817200.500661	42.852020
3502.615758	817174.590215	42.857025
3502.572761	817144.098375	42.862029
3502.516116	817125.651614	42.867034
3502.260229	817078.207092	42.872039
3502.357190	817046.467867	42.877044
3502.508291	817028.818868	42.882049
3502.623282	816991.103798	42.887053
3502.495269	816960.233475	42.892058
3502.329232	816928.977621	42.897063
3502.379374	816906.106575	42.902068
3502.343650	816873.556123	42.907073
3502.301102	816846.783583	42.912077
3502.280158	816828.819696	42.917082
3502.216826	816799.161909	42.922087
3502.540916	816764.593361	42.927092
3502.219559	816741.244408	42.932097
3502.233493	816700.900623	42.937101
3502.050797	816691.139028	42.942106
3501.703021	816656.827465	42.947111
3502.287033	816630.832113	42.952116
3502.032641	816624.460382	42.957121
3502.209810	816595.986051	42.962125
3502.309490	816567.132690	42.967130
3502.126650	816542.438330	42.972135
3502.351849	816510.430649	42.977140
3502.055471	816497.456161	42.982145
3502.204993	816460.368895	42.987149
3502.115918	816440.554711	42.992154
3501.990328	816417.906786	42.997159
3502.306562	816397.682992	43.002164
3501.959626	816381.974823	43.007169
3502.187579	816348.399178	43.012173
3501.621490	816321.319089	43.017178
3502.190858	816303.501367	43.022183
3502.231196	816279.356809	43.027188
3501.870688	816264.336057	43.032193
3502.050993	816248.540730	43.037197
3502.151429	816218.216899	43.042202
3501.882222	816200.243258	43.047207
3502.041267	816158.011755	43.052212
3502.169791	816145.407256	43.057217
3502.440394	816120.195991	43.062221
3502.063440	816100.281331	43.067226
3502.432741	816063.841152	43.072231
3502.202414	816048.700547	43.077236
3502.303250	816026.405708	43.082241
3502.324211	815992.519638	43.087245
3501.925155	815975.790869	43.092250
3501.840036	815958.618638	43.097255
3502.096759	815922.343126	43.102260
3501.852438	815910.974734	43.107265
3501.862321	815879.538117	43.112269
3501.756364	815852.233447	43.117274
3501.766522	815859.478466	43.122279
3501.814169	815830.287760	43.127284
3501.752192	815821.386374	43.132289
3502.246321	815801.082521	43.137293
3502.101679	815777.162486	43.142298
3501.796375	815757.675690	43.147303
3502.113964	815729.370419	43.152308
3501.933736	815717.011834	43.157313
3502.075411	815687.902952	43.162317
3501.764989	815659.553933	43.167322
3501.873922	815645.678613	43.172327
3502.080068	815613.376004	43.177332
3502.005789	815622.300036	43.182337
3502.225289	815573.836209	43.187341
3502.125690	815561.170258	43.192346
3501.988521	815538.472305	43.197351
3502.009396	815515.307542	43.202356
3502.025036	815490.135912	43.207361
3502.158172	815470.380195	43.212365
3502.235655	815437.363426	43.217370
3502.067624	815431.612907	43.222375
3502.047399	815399.689331	43.227380
3502.181570	815369.405081	43.232385
3502.190178	815361.079074	43.237389
3502.334230	815324.133344	43.242394
3501.959476	815317.829158	43.247399
3502.020022	815276.098023	43.252404
3502.127919	815274.709093	43.257409
3501.942728	815250.157268	43.262413
3501.997343	815222.138025	43.267418
3502.055377	815202.785645	43.272423
3501.910598	815178.422779	43.277428
3502.005325	815157.399268	43.282433
3502.099220	815130.793288	43.287437
3501.957782	815117.496786	43.292442
3501.958345	815101.973224	43.297447
3501.862904	815076.818344	43.302452
3501.924695	815054.379805	43.307457
3502.059444	815035.112248	43.312461
3501.993952	815017.199822	43.317466
3501.989146	814979.835986	43.322471
3502.031912	814975.960214	43.327476
3501.952697	814943.652424	43.332481
3501.699979	814924.644257	43.337485
3501.818902	814911.598289	43.342490
3501.577172	814870.404139	43.347495
3502.185898	814884.015860	43.352500
3501.972901	814850.603315	43.357505
3502.023381	814836.344183	43.362509
3502.157827	814810.366892	43.367514
3502.137982	814785.688192	43.372519
3501.996958	814768.669044	43.377524
3501.785884	814745.539836	43.382529
3501.964051	814737.381018	43.387533
3502.010909	814705.149262	43.392538
3501.971833	814700.160438	43.397543
3502.108590	814659.441356	43.402548
3501.892807	814651.102457	43.407553
3501.924218	814630.871303	43.412557
3501.840195	814608.455296	43.417562
3501.782127	814596.074525	43.422567
3502.154485	814568.196118	43.427572
3502.002608	814553.284085	43.432577
3502.209882	814531.162656	43.437581
3501.666837	814503.385788	43.442586
3501.562943	814495.762880	43.447591
3501.708729	814465.962398	43.452596
3501.558413	814458.298120	43.457601
3501.671588	814449.561964	43.462605
3501.815653	814436.217088	43.467610
3501.584785	814411.473825	43.472615
3502.090490	814403.113729	43.477620
3501.677644	814385.452736	43.482625
3501.726798	814365.217861	43.487629
3501.607262	814362.886702	43.492634
3501.876184	814326.208782	43.497639
3501.893597	814296.232793	43.502644
3501.836939	814298.984730	43.507649
3501.759699	814270.689393	43.512653
3501.755538	814250.756812	43.517658
3501.774988	814241.154256	43.522663
3501.840686	814210.190408	43.527668
3501.711121	814204.971241	43.532673
3501.840072	814195.791371	43.537677
3501.832398	814165.378144	43.542682
3501.798003	814158.184197	43.547687
3501.985738	814129.012014	43.552692
3501.703254	814120.242650	43.557697
3501.767543	814097.604606	43.562701
3501.740582	814064.647288	43.567706
3501.585920	814073.341724	43.572711
3501.913887	814054.235448	43.577716
3501.843530	814033.431534	43.582721
3502.025160	814010.088180	43.587725
3501.947540	813992.958672	43.592730
3501.845880	813972.012790	43.597735
3501.770814	813951.013484	43.602740
3501.709462	813934.811735	43.607745
3501.875536	813916.466412	43.612749
3501.869603	813910.785845	43.617754
3501.826783	813884.099507	43.622759
3502.287791	813864.774867	43.627764
3501.850337	813843.345128	43.632769
3502.081721	813814.507251	43.637773
3502.136931	813809.208361	43.642778
3502.034702	813772.833465	43.647783
3502.074190	813760.239171	43.652788
3501.791081	813738.244899	43.657793
3501.834058	813707.331466	43.662797
3501.753577	813690.789421	43.667802
3501.672818	813680.369910	43.672807
3502.187500	813680.236118	43.677812
3502.148692	813653.989031	43.682817
3502.120450	813615.641884	43.687821
3502.041587	813595.180883	43.692826
3501.731104	813577.843772	43.697831
3502.053500	813559.520713	43.702836
3501.970918	813530.684358	43.707841
3502.021461	813525.777865	43.712845
3501.886786	813507.285043	43.717850
3501.807906	813492.064747	43.722855
3502.165632	813462.567797	43.727860
3501.418673	813451.816830	43.732865
3501.651594	813437.916546	43.737869
3501.609569	813405.791184	43.742874
3501.327781	813385.705848	43.747879
3501.982824	813378.985296	43.752884
3501.456746	813370.793883	43.757889
3501.326944	813358.765532	43.762893
3501.699943	813341.315232	43.767898
3501.279587	813336.829045	43.772903
3501.760374	813328.422752	43.777908
3501.710004	813304.380433	43.782913
3501.637678	813293.077242	43.787917
3501.530705	813288.490421	43.792922
3501.603078	813268.101483	43.797927
3501.578990	813250.177540	43.802932
3501.349685	813247.668140	43.807937
3501.778092	813233.098452	43.812941
3501.572047	813223.041755	43.817946
3501.694265	813200.440144	43.822951
3502.015532	813188.876014	43.827956
3501.914896	813175.666922	43.832961
3501.925081	813148.821994	43.837965
3501.740366	813119.804771	43.842970
3501.683372	813095.860769	43.847975
3501.906603	813090.288719	43.852980
3501.553449	813075.700474	43.857985
3501.819735	813042.200016	43.862989
3501.566221	813041.506964	43.867994
3501.303086	813039.101028	43.872999
3501.730310	813010.031522	43.878004
3501.389857	812994.608263	43.883009
3501.503795	812986.506900	43.888013
3501.596249	812985.218019	43.893018
3501.349847	812967.721826	43.898023
3501.514899	812943.593755	43.903028
3501.763934	812940.466608	43.908033
3501.574195	812927.369678	43.913037
3501.917283	812914.674815	43.918042
3501.472671	812900.836043	43.923047
3501.729707	812911.325621	43.928052
3501.687766	812874.837984	43.933057
3501.487319	812867.376095	43.938061
3501.519793	812864.921404	43.943066
3501.632198	812839.430021	43.948071
3501.759645	812822.753628	43.953076
3501.461912	812816.238448	43.958081
3501.359518	812799.501883	43.963085
3501.506853	812779.246084	43.968090
3501.333974	812760.806496	43.973095
3501.561863	812753.714809	43.978100
3501.321641	812760.416560	43.983105
3501.282007	812747.637464	43.988109
3501.215857	812727.465661	43.993114
3501.321597	812715.005468	43.998119
3501.522200	812704.293170	44.003124
3501.254643	812718.200592	44.008129
3501.311809	812699.673958	44.013133
3501.322402	812674.492648	44.018138
3501.455322	812658.157860	44.023143
3501.317571	812662.246485	44.028148
3501.244416	812659.368230	44.033153
3501.262147	812656.768929	44.038157
3501.207616	812660.696884	44.043162
3501.204456	812642.180029	44.048167
3501.164830	812625.481682	44.053172
3501.132000	812615.101619	44.058177
3501.446553	812612.894302	44.063181
3501.393230	812614.666615	44.068186
3501.717542	812609.077521	44.073191
3501.654990	812585.083637	44.078196
3501.306821	812574.020631	44.083201
3501.324549	812572.890945	44.088205
3501.487057	812566.789597	44.093210
3501.487963	812547.488001	44.098215
3501.755004	812527.505662	44.103220
3501.197737	812509.716566	44.108225
3501.196601	812503.936048	44.113229
3501.569014	812497.310176	44.118234
3501.597831	812474.329615	44.123239
3501.689334	812468.778753	44.128244
3501.360078	812466.040577	44.133249
3501.648752	812454.333597	44.138253
3501.651236	812416.513464	44.143258
3501.397172	812411.117454	44.148263
3501.639264	812405.639715	44.153268
3501.226472	812385.132072	44.158273
3501.739497	812363.394096	44.163277
3501.859844	812369.204015	44.168282
3501.826445	812358.872643	44.173287
3501.732854	812323.909225	44.178292
3501.346745	812321.621264	44.183297
3501.803294	812306.604044	44.188301
3501.754164	812281.823032	44.193306
3501.547353	812274.067591	44.198311
3501.741322	812249.295408	44.203316
3501.494751	812237.921171	44.208321
3501.483533	812222.980814	44.213325
3501.673996	812218.834180	44.218330
3501.533877	812237.914617	44.223335
3501.709698	812190.952404	44.228340
3501.288343	812187.004508	44.233345
3501.528799	812182.212733	44.238349
3501.859727	812181.913233	44.243354
3501.536222	812146.349883	44.248359
3501.982011	812135.743276	44.253364
3501.778539	812138.079350	44.258369
3501.739867	812103.154737	44.263373
3501.706461	812083.710496	44.268378
3501.572800	812072.317381	44.273383
3501.697047	812045.988200	44.278388
3501.698227	812051.524069	44.283393
3501.627607	812023.463185	44.288397
3501.552638	812011.766348	44.293402
3501.216353	812000.455480	44.298407
3501.562400	811993.049584	44.303412
3501.383102	811994.597845	44.308417
3501.368181	811968.977182	44.313421
3501.928938	811955.068851	44.318426
3501.462569	811951.226215	44.323431
3501.593550	811944.345618	44.328436
3501.246155	811927.549263	44.333441
3501.486221	811897.770924	44.338445
3501.223785	811903.105370	44.343450
3501.514414	811899.187008	44.348455
3501.588209	811892.609737	44.353460
3501.613080	811870.068713	44.358465
3501.328527	811859.875935	44.363469
3501.723496	811855.891368	44.368474
3501.616659	811834.645750	44.373479
3502.133198	811821.430340	44.378484
3501.639534	811813.329669	44.383489
3501.914559	811783.692053	44.388493
3501.714311	811767.458991	44.393498
3501.540204	811751.858508	44.398503
3501.464267	811720.612623	44.403508
3501.328203	811706.181634	44.408513
3501.329745	811706.769277	44.413517
3501.598048	811691.389751	44.418522
3501.484860	811681.070487	44.423527
3501.530516	811652.939920	44.428532
3501.462400	811665.885743	44.433537
3501.631235	811663.555141	44.438541
3501.691771	811637.479842	44.443546
3501.268361	811614.815828	44.448551
3501.350474	811617.301019	44.453556
3501.616502	811612.210662	44.458561
3501.404868	811588.629764	44.463565
3501.803402	811574.355414	44.468570
3501.365377	811572.369718	44.473575
3501.513069	811558.577612	44.478580
3501.091033	811564.134593	44.483585
3501.367338	811527.832253	44.488589
3501.529296	811516.046538	44.493594
3501.243165	811531.380330	44.498599
3501.537470	811521.728639	44.503604
3501.416100	811517.289972	44.508609
3501.460622	811485.827179	44.513613
3501.640613	811481.093868	44.518618
3501.414092	811473.389749	44.523623
3501.709227	811450.263855	44.528628
3501.820599	811446.864725	44.533633
3501.756477	811424.434871	44.538637
3501.976085	811424.839631	44.543642
3501.525968	811412.664589	44.548647
3501.551947	811390.562759	44.553652
3501.660530	811396.277459	44.558657
3501.604977	811348.808559	44.563661
3501.667480	811342.722586	44.568666
3501.430544	811351.287072	44.573671
3501.996568	811319.786608	44.578676
3501.636946	811297.894981	44.583681
3501.520904	811290.270451	44.588685
3501.507398	811267.880739	44.593690
3501.210240	811247.301597	44.598695
3501.695655	811248.985527	44.603700
3501.456340	811246.330030	44.608705
3501.644610	811229.051724	44.613709
3501.760032	811209.090480	44.618714
3501.613877	811203.920717	44.623719
3501.951194	811195.731424	44.628724
3501.476367	811164.303686	44.633729
3501.408362	811162.256918	44.638733
3501.560062	811150.374262	44.643738
3501.340225	811139.385759	44.648743
3501.564795	811117.446323	44.653748
3501.474581	811117.608142	44.658753
3501.549906	811096.330204	44.663757
3501.772491	811103.300345	44.668762
3501.826081	811077.322035	44.673767
3501.620309	811060.500199	44.678772
3501.787309	811050.035824	44.683777
3501.641922	811023.502091	44.688781
3501.758392	811025.736844	44.693786
3501.314470	811001.408172	44.698791
3501.891502	810977.989241	44.703796
3501.386643	810971.212392	44.708801
3501.477854	810967.081346	44.713805
3501.693695	810956.412783	44.718810
3501.396447	810932.549703	44.723815
3501.841090	810912.435359	44.728820
3501.518312	810914.056497	44.733825
3501.574270	810887.097064	44.738829
3501.835693	810858.682663	44.743834
3501.529690	810860.301050	44.748839
3501.512924	810845.946580	44.753844
3501.302309	810831.575008	44.758849
3501.730749	810822.978252	44.763853
3501.775113	810821.892889	44.768858
3501.445824	810796.074571	44.773863
3501.579655	810776.403029	44.778868
3501.537414	810768.226741	44.783873
3501.570296	810765.967229	44.788877
3502.103085	810745.886876	44.793882
3501.495753	810742.213765	44.798887
3501.579656	810717.062108	44.803892
3501.757836	810702.038202	44.808897
3501.278501	810680.213298	44.813901
3501.645615	810683.729931	44.818906
3501.464150	810670.970280	44.823911
3501.735290	810644.611467	44.828916
3501.634048	810635.415692	44.833921
3501.601085	810635.176074	44.838925
3501.809762	810601.477043	44.843930
3501.563159	810585.101774	44.848935
3501.535781	810582.264096	44.853940
3501.454211	810583.502561	44.858945
3501.796918	810554.926495	44.863949
3501.973628	810525.838618	44.868954
3501.500983	810527.925557	44.873959
3501.805764	810492.789070	44.878964
3501.765512	810478.829719	44.883969
3501.728492	810473.984445	44.888973
3501.693557	810439.099651	44.893978
3501.446533	810430.368643	44.898983
3501.597876	810426.521387	44.903988
3501.551118	810406.780515	44.908993
3501.740946	810402.779895	44.913997
3501.738147	810383.227729	44.919002
3501.628698	810375.552079	44.924007
3501.792796	810346.514517	44.929012
3501.444410	810344.905718	44.934017
3501.485146	810334.657059	44.939021
3501.754334	810311.580572	44.944026
3501.651443	810298.856283	44.949031
3501.537580	810288.584014	44.954036
3501.537843	810288.338910	44.959041
3501.803416	810248.748189	44.964045
3501.875559	810234.083751	44.969050
3501.393138	810230.781822	44.974055
3501.523355	810200.132045	44.979060
3501.867805	810195.468766	44.984065
3501.878353	810181.108392	44.989069
3501.642941	810155.272171	44.994074
3501.720328	810148.300575	44.999079
3501.615236	810145.916566	45.004084
3501.902147	810122.542486	45.009089
3501.586803	810110.783951	45.014093
3501.678375	810103.172894	45.019098
3501.345834	810081.468900	45.024103
3501.358490	810072.547639	45.029108
3501.541185	810064.529479	45.034113
3501.892501	810045.065032	45.039117
3501.822132	810029.982569	45.044122
3501.675122	810016.823959	45.049127
3501.696790	810001.579253	45.054132
3501.557397	809980.627232	45.059137
3501.615285	809969.640093	45.064141
3501.840685	809953.773638	45.069146
3501.706468	809942.573062	45.074151
3501.694188	809921.256869	45.079156
3501.513621	809912.024173	45.084161
3501.432406	809901.157851	45.089165
3501.486154	809878.360421	45.094170
3501.289546	809879.912008	45.099175
3501.777481	809877.773278	45.104180
3501.448397	809859.302511	45.109185
3501.463177	809829.895277	45.114189
3501.563142	809830.907944	45.119194
3501.488635	809815.580648	45.124199
3501.889668	809805.173828	45.129204
3501.799812	809785.242217	45.134209
3501.806033	809773.528147	45.139213
3501.777188	809749.616696	45.144218
3501.583821	809730.780165	45.149223
3502.027341	809726.051241	45.154228
3501.749233	809710.169137	45.159233
3501.751536	809682.723679	45.164237
3501.779256	809674.926625	45.169242
3501.488711	809656.546976	45.174247
3501.742054	809631.902502	45.179252
3501.712108	809633.769757	45.184257
3501.538599	809616.448931	45.189261
3501.525279	809594.592781	45.194266
3501.433098	809599.851968	45.199271
3501.586293	809576.743090	45.204276
3501.536002	809555.677062	45.209281
3501.366217	809536.787099	45.214285
3501.448038	809545.742438	45.219290
3501.348082	809545.513815	45.224295
3501.535953	809530.142658	45.229300
3501.704816	809512.618143	45.234305
3501.436087	809507.614305	45.239309
3501.977195	809495.125506	45.244314
3501.567718	809466.178667	45.249319
3501.474639	809451.784812	45.254324
3501.523291	809434.917038	45.259329
3501.538061	809416.927549	45.264333
3501.389872	809396.759353	45.269338
3501.587739	809400.941684	45.274343
3501.754158	809390.866946	45.279348
3501.421338	809375.287138	45.284353
3501.312361	809357.611944	45.289357
3501.670466	809341.869242	45.294362
3501.516684	809345.325344	45.299367
3501.339210	809327.171238	45.304372
3501.437073	809319.313212	45.309377
3501.299085	809306.494822	45.314381
3501.670933	809302.022472	45.319386
3501.710608	809301.525782	45.324391
3501.562601	809275.867869	45.329396
3501.622467	809265.467413	45.334401
3501.551449	809270.919416	45.339405
3501.805932	809240.146827	45.344410
3501.455243	809223.785419	45.349415
3501.960938	809212.331199	45.354420
3501.863688	809197.251318	45.359425
3501.490393	809176.531397	45.364429
3501.665302	809151.800081	45.369434
3501.588892	809159.556669	45.374439
3501.580748	809129.856111	45.379444
3501.705811	809113.857192	45.384449
3501.969678	809119.695273	45.389453
3501.594192	809080.301382	45.394458
3501.300898	809072.605528	45.399463
3501.897450	809059.518643	45.404468
3501.722453	809045.431503	45.409473
3501.193006	809021.992064	45.414477
3501.738769	809021.019883	45.419482
3501.511976	809022.527618	45.424487
3501.593122	808995.850628	45.429492
3501.580273	808986.638061	45.434497
3501.574280	808980.071118	45.439501
3501.716417	808954.168145	45.444506
3501.620547	808942.861577	45.449511
3501.518819	808924.791950	45.454516
3501.592920	808932.573018	45.459521
3501.212909	808904.599223	45.464525
3502.030720	808879.319893	45.469530
3501.381102	808880.750261	45.474535
3501.430308	808872.654660	45.479540
3501.421672	808848.099522	45.484545
3501.357810	808827.719690	45.489549
3501.635236	808827.673957	45.494554
3501.579814	808830.672980	45.499559
3501.863066	808804.207026	45.504564
3501.586182	808790.871373	45.509569
3501.340096	808793.264616	45.514573
3501.622616	808783.709030	45.519578
3501.383694	808751.790122	45.524583
3501.515033	808754.954478	45.529588
3501.558232	808739.017180	45.534593
3501.147450	808731.438323	45.539597
3501.951251	808704.739194	45.544602
3501.280761	808695.928655	45.549607
3501.446188	808703.645925	45.554612
3501.667877	808683.463708	45.559617
3501.231085	808669.026781	45.564621
3500.993973	808646.910354	45.569626
3501.027608	808639.111142	45.574631
3501.148187	808628.601682	45.579636
3501.185251	808632.222774	45.584641
3501.278605	808637.550175	45.589645
3501.800103	808622.514154	45.594650
3501.109823	808605.079806	45.599655
3501.340695	808590.042568	45.604660
3501.100245	808581.455147	45.609665
3501.293677	808587.305290	45.614669
3501.646488	808584.306121	45.619674
3501.180139	808557.472512	45.624679
3500.990945	808556.425260	45.629684
3501.306753	808548.726518	45.634689
3501.314917	808550.195654	45.639693
3501.592097	808538.630899	45.644698
3501.294300	808540.689625	45.649703
3501.155451	808518.262491	45.654708
3501.473729	808495.907041	45.659713
3501.219295	808500.850676	45.664717
3501.129323	808481.748568	45.669722
3501.475282	808479.681819	45.674727
3501.579237	808480.350909	45.679732
3501.501693	808457.080175	45.684737
3501.580834	808438.979468	45.689741
3501.568178	808430.942552	45.694746
3501.160401	808442.921071	45.699751
3501.090083	808408.865010	45.704756
3501.302333	808409.173140	45.709761
3501.050778	808388.087636	45.714765
3501.028950	808390.689171	45.719770
3501.219115	808401.000684	45.724775
3501.323237	808387.405410	45.729780
3501.669951	808384.358140	45.734785
3501.447389	808383.855560	45.739789
3501.539366	808361.782040	45.744794
3501.171633	808357.725011	45.749799
3501.291257	808346.872145	45.754804
3501.637601	808356.765851	45.759809
3501.663497	808325.830720	45.764813
3501.698951	808295.237007	45.769818
3501.090951	808230.680648	45.774823
3501.226218	808101.637678	45.779828
3501.268493	807914.418946	45.784833
3500.816628	807682.371121	45.789837
3501.096547	807393.619635	45.794842
3500.673873	807051.041105	45.799847
3500.252067	806636.124985	45.804852
3500.394154	806192.111732	45.809857
3499.963624	805674.754802	45.814861
3499.685822	805097.698959	45.819866
3499.367774	804460.911973	45.824871
3499.099913	803764.215291	45.829876
3498.637244	803017.982196	45.834881
3497.994995	802202.078616	45.839885
3498.015110	801352.357798	45.844890
3497.513577	800439.410382	45.849895
3497.137392	799445.533709	45.854900
3496.445647	798413.719315	45.859905
3495.636210	797325.015791	45.864909
3495.562839	796145.864842	45.869914
3494.466335	794931.125832	45.874919
3494.015281	793665.818319	45.879924
3493.061348	792324.212450	45.884929
3492.233676	790936.138238	45.889933
3491.988071	789480.457317	45.894938
3491.112744	787963.621550	45.899943
3490.282559	786391.284206	45.904948
3489.478408	784769.266003	45.909953
3488.741903	783065.304740	45.914957
3487.737874	781318.617590	45.919962
3486.822745	779506.820061	45.924967
3485.976920	777645.918348	45.929972
3484.910550	775700.123351	45.934977
3483.823353	773718.497202	45.939981
3482.901664	771678.662441	45.944986
3481.501513	769585.608315	45.949991
3480.411475	767430.732426	45.954996
3479.269133	765216.066066	45.960001
3478.156882	762951.461451	45.965005
3476.820841	760635.438751	45.970010
3475.719331	758272.913987	45.975015
3474.169604	755837.643251	45.980020
3473.056121	753353.321670	45.985025
3471.781300	750817.930008	45.990029
3470.491846	748222.700383	45.995034
3469.115638	745582.620529	46.000039
3467.694636	742886.070842	46.005044
3465.968695	740139.325776	46.010049
3464.516703	737332.593293	46.015053
3463.027228	734480.473944	46.020058
3461.144669	731574.317912	46.025063
3459.689884	728620.974901	46.030068
3458.169991	725615.427419	46.035073
3456.406850	722561.374585	46.040077
3455.315116	719450.635095	46.045082
3453.209692	716291.470821	46.050087
3451.667557	713097.773352	46.055092
3450.129656	709821.239974	46.060097
3448.290604	706503.067687	46.065101
3446.511023	703137.892281	46.070106
3444.454509	699735.122167	46.075111
3442.823428	696285.209919	46.080116
3440.889439	692771.465727	46.085121
3438.665399	689227.023821	46.090125
3437.030484	685615.467000	46.095130
3435.124302	681977.966795	46.100135
3432.944503	678287.995946	46.105140
3430.856225	674535.376087	46.110145
3428.537064	670753.964127	46.115149
3426.990633	666924.716531	46.120154
3424.415431	663052.880334	46.125159
3422.683489	659132.270402	46.130164
3420.741014	655171.261385	46.135169
3418.353721	651153.120093	46.140173
3416.583473	647084.320186	46.145178
3413.975993	642999.318611	46.150183
3411.499478	638844.670123	46.155188
3409.696617	634652.155935	46.160193
3407.118927	630422.390736	46.165197
3404.785718	626148.370421	46.170202
3402.189989	621819.774012	46.175207
3399.934050	617455.460374	46.180212
3397.343517	613051.910347	46.185217
3394.976389	608622.505884	46.190221
3393.110748	604145.662184	46.195226
3390.432024	599625.833164	46.200231
3387.860796	595076.304514	46.205236
3385.430425	590477.916480	46.210241
3382.652682	585834.389532	46.215245
3380.275882	581145.223820	46.220250
3377.331908	576448.236346	46.225255
3374.941542	571683.321458	46.230260
3372.185861	566896.298242	46.235265
3369.541100	562087.395479	46.240269
3366.917716	557206.351212	46.245274
3363.969294	552319.352165	46.250279
3361.242930	547398.400581	46.255284
3358.585568	542427.175522	46.260289
3355.747375	537432.741578	46.265293
3352.862248	532395.704042	46.270298
3350.024615	527341.483986	46.275303
3347.259547	522236.809980	46.280308
3344.318582	517116.467324	46.285313
3341.713834	511947.540370	46.290317
3338.550658	506753.572702	46.295322
3335.394708	501526.391938	46.300327
3332.598704	496273.027985	46.305332
3329.363454	490997.724719	46.310337
3325.926499	485682.238150	46.315341
3323.354520	480333.635737	46.320346
3319.980332	474971.550136	46.325351
3317.238517	469580.624733	46.330356
3314.174962	464157.282482	46.335361
3310.624262	458724.932819	46.340365
3307.762524	453239.049670	46.345370
3304.367808	447757.397801	46.350375
3301.103111	442233.546114	46.355380
3297.812435	436699.854010	46.360385
3294.353818	431136.890934	46.365389
3291.409837	425551.775759	46.370394
3287.981543	419950.134880	46.375399
3284.401138	414310.564690	46.380404
3281.128178	408663.692418	46.385409
3277.750199	402998.219875	46.390413
3274.341762	397312.669778	46.395418
3271.064477	391608.193275	46.400423
3267.792573	385888.151183	46.405428
3264.397675	380143.145288	46.410433
3261.087822	374397.713158	46.415437
3257.497824	368607.939622	46.420442
3254.163560	362812.247346	46.425447
3250.571401	357009.698057	46.430452
3247.024754	351160.876662	46.435457
3243.316689	345326.230711	46.440461
3240.081081	339443.793335	46.445466
3236.208702	333580.412620	46.450471
3232.589599	327703.747392	46.455476
3229.135770	321805.788306	46.460481
3225.440678	315902.049263	46.465485
3221.814616	309990.313071	46.470490
3218.082799	304047.792219	46.475495
3214.309615	298118.879196	46.480500
3210.545994	292165.548739	46.485505
3206.396475	286222.726202	46.490509
3203.209094	280266.914316	46.495514
3199.071733	274304.361581	46.500519
3195.362659	268334.713912	46.505524
3191.424099	262367.911181	46.510529
3187.689888	256401.081439	46.515533
3183.613813	250405.613265	46.520538
3179.828897	244438.477624	46.525543
3175.808245	238448.012199	46.530548
3171.909916	232458.888914	46.535553
3167.945181	226477.863022	46.540557
3163.768977	220487.287178	46.545562
3159.924003	214524.784085	46.550567
3155.828313	208452.999752	46.555572
3152.225000	202487.862181	46.560577
3147.613892	196506.554185	46.565581
3143.457890	190547.822160	46.570586
3139.291639	184580.636758	46.575591
3135.106145	178632.092407	46.580596
3131.126732	172679.450041	46.585601
3126.621363	166760.854564	46.590605
3122.467630	160819.943998	46.595610
3117.889427	154921.954160	46.600615
3113.771007	149017.170226	46.605620
3109.209348	143134.475185	46.610625
3104.594000	137272.217469	46.615629
3100.257563	131421.498600	46.620634
3095.464991	125597.031496	46.625639
3090.842564	119787.263476	46.630644
3086.211139	114000.456347	46.635649
3081.261348	108238.130383	46.640653
3076.553432	102509.264777	46.645658
3071.410887	96819.333470	46.650663
3066.158263	91147.155901	46.655668
3060.871712	85516.324707	46.660673
3055.149581	79937.543962	46.665677
3049.623635	74389.951462	46.670682
3042.753950	68926.468518	46.675687
3032.307827	63623.267907	46.680692
3016.806594	58561.037924	46.685697
3002.019030	53639.108278	46.690701
2987.285266	48933.208743	46.695706
2973.543800	44436.488804	46.700711
2960.116343	40165.630940	46.705716
2947.298697	36119.029670	46.710721
2935.086659	32339.788144	46.715725
2923.142385	28762.425542	46.720730
2912.070882	25417.057163	46.725735
2900.878147	22290.236806	46.730740
2890.714144	19376.823276	46.735745
2881.064115	16661.489733	46.740749
2871.009188	14145.158359	46.745754
2859.696498	11870.289740	46.750759
2847.415399	9813.313124	46.755764
2835.473282	7974.493329	46.760769
2823.033026	6364.621932	46.765773
2811.716676	4947.990034	46.770778
2800.691732	3732.702716	46.775783
2791.044113	2701.884201	46.780788
2782.426752	1832.167605	46.785793
2774.887778	1121.105147	46.790797
2767.971510	517.983356	46.795802
2757.998432	152.874657	46.800807
2735.969778	263.238048	46.805812
2727.781891	251.207099	46.810817
2726.169060	241.702367	46.815821
2729.010293	248.123654	46.820826
2732.338111	246.598532	46.825831
2734.755116	251.632571	46.830836
2735.785192	249.564506	46.835841
2734.000912	230.551461	46.840845
2731.733498	242.017880	46.845850
2728.680789	239.800422	46.850855
2725.719975	236.323528	46.855860
2722.604671	229.910759	46.860865
2719.794689	240.704985	46.865869
2717.019176	219.479876	46.870874
2713.807654	234.127620	46.875879
2710.810830	237.352655	46.880884
2707.914150	227.248139	46.885889
2704.409071	237.633879	46.890893
2701.807038	228.779138	46.895898
2698.770704	220.774426	46.900903
2695.341460	227.216203	46.905908
2692.405216	224.438910	46.910913
2689.171808	231.796218	46.915917
2686.097499	217.214364	46.920922
2682.550628	220.566106	46.925927
2679.289194	229.638092	46.930932
2676.201056	214.137447	46.935937
2672.992890	228.844233	46.940941
2669.713232	225.018196	46.945946
2666.074604	217.113794	46.950951
2662.348077	224.419913	46.955956
2659.517860	211.763119	46.960961
2656.035398	223.707795	46.965965
2652.930483	212.416942	46.970970
2649.639187	225.910123	46.975975
2645.890017	222.531481	46.980980
2643.116407	206.728212	46.985985
2639.170669	212.045213	46.990989
2636.190713	208.267059	46.995994
2632.552745	206.298770	47.000999
2628.981093	208.634488	47.006004
2625.551486	202.445857	47.011009
2622.329513	216.143768	47.016013
2619.395164	197.240233	47.021018
2615.884253	200.949233	47.026023
2611.926228	204.291446	47.031028
2608.540452	200.893559	47.036033
2604.953241	205.388135	47.041037
2602.109490	203.689166	47.046042
2598.587588	195.762507	47.051047
2595.226667	208.190901	47.056052
2591.609166	210.178037	47.061057
2588.199083	209.083801	47.066061
2584.951824	203.542120	47.071066
2581.657152	206.223270	47.076071
2578.117177	202.259758	47.081076
2573.960653	200.436495	47.086081
2570.794471	205.159118	47.091085
2566.877688	204.575141	47.096090
2564.358571	211.433091	47.101095
2560.441570	213.001687	47.106100
2557.123698	209.217722	47.111105
2553.766532	214.503912	47.116109
2550.531645	207.537745	47.121114
2546.741392	201.301283	47.126119
2543.197258	219.519898	47.131124
2540.104624	200.281414	47.136129
2536.537029	207.080015	47.141133
2532.668758	202.947100	47.146138
2529.499096	202.816013	47.151143
2526.397139	200.395441	47.156148
2522.810799	193.486064	47.161153
2519.219608	200.820724	47.166157
2515.532652	198.929337	47.171162
2512.215349	194.572689	47.176167
2508.455571	189.673872	47.181172
2505.288934	193.284217	47.186177
2501.923992	196.056996	47.191181
2498.331051	186.030918	47.196186
2494.662996	180.736165	47.201191
2490.957873	206.667115	47.206196
2488.075465	189.993663	47.211201
2484.563182	193.402034	47.216205
2481.182573	194.061083	47.221210
2477.544385	193.373792	47.226215
2474.082320	198.699800	47.231220
2470.412151	191.217257	47.236225
2466.791341	204.672761	47.241229
2463.386744	196.788098	47.246234
2460.267662	196.506335	47.251239
2456.416861	201.722520	47.256244
2452.958660	194.582893	47.261249
2449.406228	197.064295	47.266253
2446.304283	199.872458	47.271258
2443.218364	191.906843	47.276263
2439.165831	196.987595	47.281268
2435.759994	185.997883	47.286273
2432.002842	198.116758	47.291277
2428.370687	197.954445	47.296282
2425.139810	191.004952	47.301287
2421.589647	195.200675	47.306292
2418.246174	187.781100	47.311297
2414.754629	190.713704	47.316301
2411.443295	192.453507	47.321306
2408.074351	193.377633	47.326311
2404.292381	181.864334	47.331316
2401.063322	190.526945	47.336321
2397.465546	200.062031	47.341325
2393.821783	187.506899	47.346330
2390.770724	194.618751	47.351335
2386.793165	198.492510	47.356340
2383.666556	188.975623	47.361345
2379.596205	195.881462	47.366349
2376.230023	179.139287	47.371354
2372.766566	180.588683	47.376359
2369.468382	190.526616	47.381364
2365.998096	186.124435	47.386369
2362.605834	187.040587	47.391373
2358.829386	190.157236	47.396378
2355.817089	183.915026	47.401383
2351.938661	179.552045	47.406388
2348.543748	175.926613	47.411393
2344.855952	165.346135	47.416397
2341.249804	170.592062	47.421402
2337.816569	172.418592	47.426407
2334.158457	167.847034	47.431412
2331.118017	164.232214	47.436417
2327.531860	170.632898	47.441421
2324.519701	177.073886	47.446426
2320.960500	169.340009	47.451431
2316.883629	166.813449	47.456436
2313.858901	175.207971	47.461441
2309.987885	177.071986	47.466445
2306.613690	176.229166	47.471450
2303.263537	180.930524	47.476455
2299.501447	175.492745	47.481460
2295.928357	173.954240	47.486465
2292.545915	177.569768	47.491469
2289.053905	165.660074	47.496474
2285.878318	163.404775	47.501479
2282.120453	166.390531	47.506484
2278.717013	165.181396	47.511489
2275.334922	167.091270	47.516493
2271.720685	175.002527	47.521498
2268.523825	176.331046	47.526503
2264.628342	177.950304	47.531508
2261.183654	167.846551	47.536513
2257.756465	168.935044	47.541517
2254.096956	170.323595	47.546522
2250.788091	172.807432	47.551527
2247.175973	174.923963	47.556532
2243.746086	165.588399	47.561537
2239.951551	163.706022	47.566541
2236.514073	174.629668	47.571546
2233.238288	161.907020	47.576551
2229.317574	161.989319	47.581556
2226.616716	168.065160	47.586561
2222.656498	162.111963	47.591565
2219.184247	156.970748	47.596570
2215.418958	163.121029	47.601575
2212.162162	166.009473	47.606580
2208.900681	166.202170	47.611585
2205.407683	168.103631	47.616589
2201.913234	172.567778	47.621594
2198.573214	170.382061	47.626599
2194.633933	169.102802	47.631604
2191.483801	167.477520	47.636609
2187.558342	172.812979	47.641613
2183.889545	170.982010	47.646618
2180.625489	165.071272	47.651623
2176.783778	167.384247	47.656628
2174.061024	156.812225	47.661633
2170.460164	174.335238	47.666637
2167.123864	159.479956	47.671642
2163.452085	147.546924	47.676647
2159.466411	164.779417	47.681652
2156.318183	159.839128	47.686657
2152.526273	167.638655	47.691661
2149.019533	167.196321	47.696666
2146.097021	162.403986	47.701671
2142.233169	166.139528	47.706676
2139.241138	171.178582	47.711681
2135.735581	169.048614	47.716685
2131.823282	157.793682	47.721690
2128.116746	163.193489	47.726695
2124.641894	157.080576	47.731700
2121.052866	159.319440	47.736705
2117.614914	169.186576	47.741709
2114.642356	154.888832	47.746714
2111.070560	155.547417	47.751719
2107.151965	171.005066	47.756724
2103.601109	156.285651	47.761729
2100.110762	174.521805	47.766733
2096.718948	161.280295	47.771738
2093.388728	152.851031	47.776743
2089.578769	164.645453	47.781748
2086.508354	153.789862	47.786753
2082.629424	164.004411	47.791757
2079.420571	159.356420	47.796762
2075.952037	164.631059	47.801767
2072.054465	162.198781	47.806772
2068.857542	154.591461	47.811777
2065.349449	153.241049	47.816781
2061.455991	163.882725	47.821786
2058.076726	162.590978	47.826791
2054.930258	156.575965	47.831796
2051.536235	159.247865	47.836801
2048.001506	163.860688	47.841805
2044.100534	158.460965	47.846810
2040.590811	151.640655	47.851815
2037.067693	159.013687	47.856820
2034.386842	150.895449	47.861825
2030.294556	148.802043	47.866829
2026.820250	156.547056	47.871834
2023.228462	162.548833	47.876839
2019.276307	166.440378	47.881844
2016.332396	157.160433	47.886849
2013.036316	156.421676	47.891853
2009.199479	158.986690	47.896858
2005.741048	156.305015	47.901863
2002.150819	150.747508	47.906868
1998.813246	146.262269	47.911873
1994.912860	157.172967	47.916877
1991.724050	152.189731	47.921882
1988.537409	145.294352	47.926887
1984.801404	146.146423	47.931892
1981.461076	152.283822	47.936897
1977.605157	155.486467	47.941901
1974.488604	154.044969	47.946906
1971.244934	159.128156	47.951911
1967.061712	161.300652	47.956916
1963.677570	148.473416	47.961921
1960.244254	167.468045	47.966925
1956.860992	155.354549	47.971930
1953.574226	151.249464	47.976935
1949.741819	154.610732	47.981940
1946.482192	145.309612	47.986945
1942.553314	152.721600	47.991949
1939.309073	146.446044	47.996954
1935.796152	150.374182	48.001959
1932.294516	144.960248	48.006964
1929.083378	142.575819	48.011969
1925.220460	147.887265	48.016973
1921.616582	150.532673	48.021978
1918.116692	152.676222	48.026983
1914.742169	152.120438	48.031988
1911.643088	152.107410	48.036993
1907.692124	160.544463	48.041997
1904.501487	160.785590	48.047002
1900.731483	153.245082	48.052007
1896.930617	156.020968	48.057012
1894.028248	161.120293	48.062017
1890.162820	151.114591	48.067021
1886.693726	161.399135	48.072026
1883.043682	157.970429	48.077031
1879.609031	155.493950	48.082036
1876.131652	156.089715	48.087041
1872.517238	143.692594	48.092045
1869.140208	155.678395	48.097050
1866.191772	137.442857	48.102055
1862.670895	146.684650	48.107060
1859.256295	144.451617	48.112065
1855.493419	149.771453	48.117069
1851.637677	143.577890	48.122074
1847.754768	147.431158	48.127079
1844.564147	150.222606	48.132084
1841.124289	138.150496	48.137089
1837.654968	145.135585	48.142093
1833.924449	144.705366	48.147098
1830.875074	144.387015	48.152103
1827.107092	156.652013	48.157108
1824.231707	154.692105	48.162113
1820.261589	146.752052	48.167117
1816.730058	142.099817	48.172122
1813.344035	145.386022	48.177127
1809.656290	148.448533	48.182132
1806.299070	148.062299	48.187137
1802.986497	141.138170	48.192141
1799.253064	144.120714	48.197146
1795.652400	132.877548	48.202151
1791.952229	153.144518	48.207156
1788.578619	132.617126	48.212161
1785.358478	143.415568	48.217165
1781.651297	146.614387	48.222170
1778.362255	142.477111	48.227175
1774.466427	153.172468	48.232180
1771.508101	142.467265	48.237185
1767.813043	145.840489	48.242189
1764.148014	153.807383	48.247194
1760.593849	153.819882	48.252199
1757.486699	152.634919	48.257204
1754.161744	139.686174	48.262209
1750.345751	155.752202	48.267213
1746.370640	163.168164	48.272218
1743.093453	151.868288	48.277223
1739.491538	155.177028	48.282228
1736.222186	146.920930	48.287233
1732.963303	141.238955	48.292237
1728.999865	157.462805	48.297242
1725.605416	143.196723	48.302247
1722.027160	147.799897	48.307252
1718.718243	138.988487	48.312257
1714.976382	141.067281	48.317261
1711.392490	135.706605	48.322266
1708.524810	139.930797	48.327271
1704.957334	137.810873	48.332276
1701.176750	138.176072	48.337281
1697.582791	138.271037	48.342285
1694.140585	143.048792	48.347290
1690.711357	143.065967	48.352295
1686.809751	133.385535	48.357300
1683.660788	136.280373	48.362305
1680.181719	136.104024	48.367309
1676.597775	147.727228	48.372314
1673.213905	132.941098	48.377319
1669.466613	144.851810	48.382324
1666.156375	137.831377	48.387329
1662.447589	143.341762	48.392333
1658.880721	143.787146	48.397338
1656.150892	143.507795	48.402343
1652.355366	146.120925	48.407348
1649.015860	143.875803	48.412353
1645.375868	153.864050	48.417357
1641.500557	150.241101	48.422362
1638.113976	149.098157	48.427367
1634.188361	147.062524	48.432372
1631.102646	142.786701	48.437377
1627.421407	143.529878	48.442381
1623.741785	140.973396	48.447386
1620.640518	136.413842	48.452391
1617.086848	133.406929	48.457396
1613.880138	145.010228	48.462401
1610.251397	135.821315	48.467405
1606.794319	135.292127	48.472410
1603.533753	137.593740	48.477415
1599.455080	141.156827	48.482420
1595.945915	133.994243	48.487425
1592.168530	147.566309	48.492429
1588.913675	144.919525	48.497434
1585.674684	143.810362	48.502439
1581.994587	133.956803	48.507444
1578.639134	133.675063	48.512449
1575.167064	131.064923	48.517453
1571.297506	133.424132	48.522458
1568.293921	127.672889	48.527463
1564.281640	132.591339	48.532468
1560.838547	118.013664	48.537473
1557.534588	131.472777	48.542477
1554.138070	127.231416	48.547482
1550.976766	122.474924	48.552487
1547.030397	131.168174	48.557492
1543.739018	124.186927	48.562497
1539.866342	138.656429	48.567501
1536.308094	126.630295	48.572506
1533.049573	123.211269	48.577511
1529.516802	141.831814	48.582516
1526.174590	136.653040	48.587521
1522.581299	134.899643	48.592525
1519.223836	136.712258	48.597530
1515.570861	127.877344	48.602535
1511.568484	133.499387	48.607540
1508.321483	134.129822	48.612545
1505.057291	129.155330	48.617549
1501.519858	142.823580	48.622554
1498.362614	136.711877	48.627559
1494.605202	129.911945	48.632564
1491.001156	132.165914	48.637569
1487.598111	136.050564	48.642573
1483.945919	134.091145	48.647578
1480.413185	120.304548	48.652583
1476.935431	130.749493	48.657588
1473.463121	129.191820	48.662593
1470.158897	123.819757	48.667597
1466.114431	125.188662	48.672602
1463.034035	124.194562	48.677607
1459.229636	129.067313	48.682612
1455.791581	121.125726	48.687617
1452.348383	137.465357	48.692621
1449.178256	124.009121	48.697626
1445.465237	132.589420	48.702631
1441.902183	132.893796	48.707636
1438.512894	137.688874	48.712641
1434.916468	128.041608	48.717645
1431.494237	139.414456	48.722650
1427.822748	140.415100	48.727655
1424.395687	138.751820	48.732660
1420.999950	135.031010	48.737665
1417.820821	132.694423	48.742669
1414.018643	140.496451	48.747674
1410.298210	132.031844	48.752679
1406.632886	133.836720	48.757684
1403.475888	129.361650	48.762689
1399.910200	123.698824	48.767693
1396.528987	133.058821	48.772698
1393.206396	128.948987	48.777703
1389.454675	143.499713	48.782708
1385.973098	133.534193	48.787713
1382.397477	131.732670	48.792717
1378.730245	145.015922	48.797722
1375.683409	129.210578	48.802727
1371.858213	130.383718	48.807732
1368.252938	125.445272	48.812737
1364.657630	135.067629	48.817741
1361.172951	141.304965	48.822746
1357.915679	126.516991	48.827751
1354.379676	138.297945	48.832756
1350.962488	127.532468	48.837761
1347.518812	132.271644	48.842765
1343.835373	128.015104	48.847770
1340.742907	121.569500	48.852775
1336.991625	141.801128	48.857780
1333.371490	120.962061	48.862785
1329.890131	119.576831	48.867789
1326.355688	137.551112	48.872794
1322.882297	119.806872	48.877799
1318.902146	126.462028	48.882804
1315.482641	121.057380	48.887809
1312.451247	126.387941	48.892813
1308.558534	136.257515	48.897818
1305.677237	121.285975	48.902823
1301.942550	126.654588	48.907828
1298.581663	121.390232	48.912833
1294.949333	122.319368	48.917837
1291.464848	127.626858	48.922842
1288.046438	121.854745	48.927847
1284.240613	127.065519	48.932852
1280.683484	123.815481	48.937857
1277.547123	126.172503	48.942861
1273.620338	120.460932	48.947866
1270.590284	122.606155	48.952871
1266.494159	124.762298	48.957876
1263.408434	118.353704	48.962881
1259.605833	115.957228	48.967885
1255.990301	123.312970	48.972890
1252.793945	124.475604	48.977895
1249.514864	129.737467	48.982900
1245.727700	127.036954	48.987905
1242.774617	129.000780	48.992909
1238.915087	120.781621	48.997914
1235.365285	120.503122	49.002919
1231.454389	126.010464	49.007924
1228.440365	110.751008	49.012929
1224.902062	120.972322	49.017933
1220.970789	123.527771	49.022938
1217.677767	112.143834	49.027943
1213.767733	126.731696	49.032948
1210.373428	120.753303	49.037953
1207.204638	129.225814	49.042957
1203.952750	120.089690	49.047962
1200.510903	128.352743	49.052967
1196.918321	129.416744	49.057972
1193.228870	129.759080	49.062977
1189.882845	123.751516	49.067981
1186.508114	131.173006	49.072986
1182.958429	126.714431	49.077991
1179.283974	124.837090	49.082996
1175.838481	128.771012	49.088001
1172.072862	121.352776	49.093005
1168.229027	129.899446	49.098010
1165.073768	118.385455	49.103015
1161.689095	122.668254	49.108020
1157.921669	116.524873	49.113025
1154.536642	124.441158	49.118029
1151.129986	124.968676	49.123034
1147.945201	116.315384	49.128039
1144.294209	132.454116	49.133044
1140.989285	114.192762	49.138049
1137.358059	121.131166	49.143053
1133.476200	123.333898	49.148058
1130.184969	121.845463	49.153063
1126.388719	129.455248	49.158068
1123.263107	120.518624	49.163073
1119.727337	124.512757	49.168077
1116.281336	126.828526	49.173082
1112.717588	125.799841	49.178087
1109.121782	129.675835	49.183092
1105.665731	125.888793	49.188097
1102.477372	118.942183	49.193101
1098.821717	118.089687	49.198106
1095.183910	125.907636	49.203111
1091.523494	128.170714	49.208116
1088.017657	117.932069	49.213121
1084.728400	128.224205	49.218125
1081.086147	120.939169	49.223130
1077.522288	119.887239	49.228135
1073.952504	126.001910	49.233140
1070.755285	112.037767	49.238145
1067.307570	124.512007	49.243149
1063.674860	128.329989	49.248154
1060.378286	118.983493	49.253159
1056.485138	132.074287	49.258164
1052.742791	123.928046	49.263169
1049.625389	126.844182	49.268173
1045.946433	135.727832	49.273178
1042.727590	121.808801	49.278183
1038.825735	134.422954	49.283188
1035.517793	135.802606	49.288193
1032.313200	128.957169	49.293197
1028.482938	128.981886	49.298202
1025.479879	131.614854	49.303207
1021.760834	132.133041	49.308212
1018.022832	126.233499	49.313217
1014.753021	126.696168	49.318221
1010.829790	129.697122	49.323226
1008.028964	117.426119	49.328231
1003.888401	130.063318	49.333236
1000.325801	129.987427	49.338241
997.055547	121.530941	49.343245
993.396136	118.995846	49.348250
990.058941	113.608771	49.353255
986.629278	117.982342	49.358260
983.191871	126.180625	49.363265
979.627961	115.274460	49.368269
976.050978	108.904510	49.373274
972.702172	116.811828	49.378279
969.009989	121.287847	49.383284
965.428678	113.797090	49.388289
962.307700	126.111368	49.393293
958.421321	122.822148	49.398298
954.688471	123.047571	49.403303
951.547995	118.894782	49.408308
948.132675	123.037911	49.413313
944.532713	121.233148	49.418317
940.770040	133.775823	49.423322
937.398876	128.529835	49.428327
933.830554	126.863004	49.433332
930.533780	128.457215	49.438337
927.133723	131.090267	49.443341
923.583921	126.834006	49.448346
919.923311	131.513695	49.453351
916.530589	131.358201	49.458356
912.865204	131.006317	49.463361
909.488409	123.266454	49.468365
906.013747	126.482166	49.473370
902.820580	119.578388	49.478375
898.833476	128.223228	49.483380
895.557170	123.522365	49.488385
892.250855	113.452258	49.493389
888.178226	124.406560	49.498394
884.817991	120.976937	49.503399
881.383329	130.962564	49.508404
877.695113	124.536548	49.513409
874.739711	120.421706	49.518413
870.816326	118.859908	49.523418
867.934263	112.699261	49.528423
864.093726	125.643525	49.533428
860.269181	119.929740	49.538433
856.836973	114.927007	49.543437
853.220164	124.722419	49.548442
850.083463	110.924818	49.553447
846.593816	127.931923	49.558452
842.855341	115.046128	49.563457
839.500662	110.143368	49.568461
835.729860	130.301518	49.573466
832.504550	120.599570	49.578471
828.733163	123.465153	49.583476
825.321398	126.385302	49.588481
821.998920	116.597003	49.593485
818.155266	119.164054	49.598490
815.243649	118.457688	49.603495
811.306329	119.574770	49.608500
807.713678	108.941911	49.613505
804.526711	113.017798	49.618509
800.890220	104.194042	49.623514
797.619774	111.530787	49.628519
793.671540	118.592632	49.633524
790.323894	114.412676	49.638529
786.893151	111.709911	49.643533
783.271812	123.390531	49.648538
779.787891	124.326605	49.653543
776.111621	120.871292	49.658548
772.701411	110.055706	49.663553
769.681701	117.768867	49.668557
765.911260	113.928470	49.673562
762.239051	108.931390	49.678567
758.804480	119.921956	49.683572
755.586310	114.878607	49.688577
751.911471	123.323670	49.693581
748.130754	114.682004	49.698586
744.945277	102.653544	49.703591
740.998477	124.258372	49.708596
737.932928	111.541215	49.713601
734.717562	113.085868	49.718605
730.703174	120.166267	49.723610
727.241530	112.168436	49.728615
723.512101	125.684968	49.733620
720.336944	121.276291	49.738625
716.794809	113.635574	49.743629
713.099072	118.525185	49.748634
709.959351	131.595590	49.753639
706.392796	131.522678	49.758644
702.768050	122.300930	49.763649
699.587311	127.414391	49.768653
695.782254	118.368735	49.773658
692.326680	129.443306	49.778663
688.622721	122.955684	49.783668
685.293604	129.967334	49.788673
681.794952	120.890913	49.793677
678.164883	124.045978	49.798682
674.942409	114.546496	49.803687
671.313397	125.438789	49.808692
667.627664	116.339213	49.813697
664.093249	115.614228	49.818701
660.356569	127.004172	49.823706
657.232056	120.254243	49.828711
654.008310	127.517439	49.833716
650.475618	123.329150	49.838721
646.977894	113.928812	49.843725
643.135584	114.489271	49.848730
639.755481	126.370537	49.853735
636.049095	115.056309	49.858740
632.411892	124.575891	49.863745
629.486874	110.580191	49.868749
625.758066	112.310028	49.873754
622.457219	103.929757	49.878759
618.740482	109.189585	49.883764
615.103218	112.486060	49.888769
611.534911	110.236153	49.893773
607.885817	107.226129	49.898778
604.714150	109.423929	49.903783
601.109910	116.540638	49.908788
597.801060	118.931479	49.913793
594.216932	110.825214	49.918797
590.555114	111.028354	49.923802
587.459047	101.650118	49.928807
583.815822	117.868363	49.933812
579.914947	116.279939	49.938817
576.650018	114.616274	49.943821
573.350927	121.326745	49.948826
569.726572	113.245882	49.953831
566.128037	117.953968	49.958836
562.783815	110.869833	49.963841
559.286618	114.755263	49.968845
555.583405	127.507492	49.973850
552.022510	108.247714	49.978855
548.686561	112.385120	49.983860
544.953840	124.803145	49.988865
541.451112	115.247429	49.993869
537.992189	120.624047	49.998874
534.625497	111.665330	50.003879
531.272408	109.367785	50.008884
527.659485	115.693065	50.013889
524.312654	112.113740	50.018893
520.551783	123.885394	50.023898
516.904215	114.331717	50.028903
513.178188	121.498676	50.033908
509.982694	111.817355	50.038913
506.631989	117.831680	50.043917
503.022143	115.177596	50.048922
499.676065	123.977205	50.053927
496.073694	113.097343	50.058932
492.841372	110.811244	50.063937
489.297221	107.489369	50.068941
485.506897	115.849645	50.073946
481.975936	116.743625	50.078951
478.417901	109.877668	50.083956
475.074969	111.131763	50.088961
471.619293	103.412007	50.093965
467.730111	115.812693	50.098970
464.736190	106.840391	50.103975
461.443321	109.653765	50.108980
457.291170	113.475477	50.113985
453.997885	112.025908	50.118989
450.632631	118.117640	50.123994
447.373073	107.934522	50.128999
443.543834	110.226419	50.134004
440.239591	123.867975	50.139009
436.474698	109.734400	50.144013
432.879174	116.718142	50.149018
429.469661	113.836459	50.154023
426.092219	117.731080	50.159028
422.458515	110.704318	50.164033
419.119271	108.684730	50.169037
415.227901	116.962387	50.174042
411.896619	113.955817	50.179047
408.737232	113.798247	50.184052
405.187736	119.011520	50.189057
401.643123	121.409833	50.194061
397.704792	111.382183	50.199066
394.548965	120.286846	50.204071
390.752019	115.385379	50.209076
387.014268	122.483306	50.214081
384.054034	106.797287	50.219085
380.489954	117.010484	50.224090
376.962598	111.294386	50.229095
373.187041	104.284482	50.234100
370.078321	105.418350	50.239105
366.892806	98.133991	50.244109
362.794465	110.166858	50.249114
359.700554	115.655907	50.254119
356.047662	117.199521	50.259124
352.352829	119.187900	50.264129
349.086008	118.740302	50.269133
345.529220	112.636927	50.274138
341.947019	115.139544	50.279143
338.421090	117.106144	50.284148
334.772307	119.828322	50.289153
331.227937	122.505334	50.294157
327.973911	118.616988	50.299162
324.542340	120.127706	50.304167
320.763840	111.698073	50.309172
317.263763	107.730419	50.314177
314.179360	112.211430	50.319181
310.315364	114.922414	50.324186
306.855428	98.028493	50.329191
303.127497	107.111953	50.334196
299.905964	99.825098	50.339201
296.604848	109.152562	50.344205
292.735846	121.975996	50.349210
289.560148	103.954447	50.354215
285.990001	102.447613	50.359220
282.287623	98.410704	50.364225
278.770563	100.005417	50.369229
275.152194	112.865184	50.374234
272.040294	103.369386	50.379239
268.307163	108.734705	50.384244
264.685901	114.829454	50.389249
261.747159	100.809122	50.394253
257.757812	103.797841	50.399258
254.351355	109.000182	50.404263
251.149751	107.721439	50.409268
247.232787	99.066819	50.414273
244.119965	101.646726	50.419277
240.250199	102.461063	50.424282
236.715524	118.997233	50.429287
233.283638	110.728421	50.434292
229.636082	105.159737	50.439297
226.570748	105.520938	50.444301
222.924381	102.521645	50.449306
219.220712	95.213574	50.454311
215.433760	107.016992	50.459316
212.422583	108.347124	50.464321
209.118161	97.852226	50.469325
205.090175	116.936693	50.474330
201.948950	112.374806	50.479335
198.431991	102.333623	50.484340
194.506000	102.208704	50.489345
191.263153	103.587582	50.494349
187.909824	112.002574	50.499354
184.192068	101.058633	50.504359
180.604040	95.914331	50.509364
177.098448	105.694914	50.514369
173.907134	104.142025	50.519373
170.361970	107.750065	50.524378
166.859715	106.739072	50.529383
163.359984	105.522460	50.534388
159.704295	113.633054	50.539393
156.353664	111.264966	50.544397
152.725952	110.386980	50.549402
149.578715	112.281636	50.554407
145.966136	98.902004	50.559412
142.285090	111.566289	50.564417
138.980275	101.219678	50.569421
135.253047	104.686849	50.574426
131.785576	99.602862	50.579431
128.099486	91.684035	50.584436
124.470612	104.658457	50.589441
121.093799	95.521336	50.594445
117.585471	102.728577	50.599450
114.045719	87.192275	50.604455
110.757329	93.621779	50.609460
106.978960	100.602639	50.614465
103.973374	95.466914	50.619469
100.285230	104.666328	50.624474
97.077892	99.967739	50.629479
93.119871	103.845691	50.634484
89.686494	106.776185	50.639489
86.054415	105.467046	50.644493
82.552228	111.180538	50.649498
79.070661	107.759280	50.654503
75.855954	87.431962	50.659508
71.927402	98.746030	50.664513
68.381078	85.717286	50.669517
64.887706	91.707828	50.674522
61.580404	97.341767	50.679527
58.100041	96.268124	50.684532
54.906531	109.144691	50.689537
51.672041	102.928460	50.694541
47.927051	102.480617	50.699546
44.533541	89.764134	50.704551
40.733413	95.338050	50.709556
36.879460	97.819340	50.714561
33.646454	89.887166	50.719565
29.922387	91.816231	50.724570
26.394326	86.577374	50.729575
23.049835	101.279550	50.734580
19.752437	93.486769	50.739585
16.251381	100.239634	50.744589
12.045437	102.193884	50.749594
8.747651	94.684511	50.754599
5.739291	100.905796	50.759604
2.205323	105.078354	50.764609