Thu Jun 16 18:52:40 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.236359	86.367406	0.000000
-0.552134	99.064204	0.005005
-0.386005	89.067233	0.010010
-0.344729	99.660991	0.015014
-0.679038	91.043640	0.020019
-0.434618	98.818003	0.025024
-0.671564	85.449610	0.030029
-0.788388	77.142112	0.035034
-0.970575	61.111857	0.040038
-1.551059	58.693643	0.045043
-1.503430	55.517748	0.050048
-1.649762	46.986559	0.055053
-1.976100	33.307324	0.060058
-2.183036	26.097680	0.065062
-2.713405	18.499317	0.070067
-2.971793	12.448988	0.075072
-3.204884	6.629575	0.080077
-3.545790	10.246931	0.085082
-3.990242	7.276767	0.090086
-4.247696	0.769617	0.095091
-4.476030	-5.882334	0.100096
-4.664619	9.783591	0.105101
-5.173946	0.908030	0.110106
-5.957092	1.885762	0.115110
-6.505755	-2.512566	0.120115
-5.743709	-1.805773	0.125120
-6.152984	-5.167388	0.130125
-5.738167	2.219862	0.135130
-6.182474	-9.884254	0.140134
-6.529333	6.585516	0.145139
-7.040572	-0.339622	0.150144
-7.461601	5.190073	0.155149
-8.011548	-1.079126	0.160154
-8.059112	1.356507	0.165158
-7.990785	7.288150	0.170163
-7.982083	-0.004965	0.175168
-8.913423	7.246334	0.180173
-9.390759	-7.699397	0.185178
-9.405611	-9.576427	0.190182
-9.696758	7.255274	0.195187
-9.347090	-11.575896	0.200192
-9.607411	2.525376	0.205197
-9.560777	-0.101232	0.210202
-10.197390	-7.610499	0.215206
-10.840872	-4.389852	0.220211
-10.468527	2.642255	0.225216
-11.061854	0.295530	0.230221
-10.997716	-3.041719	0.235226
-11.970897	1.987098	0.240230
-12.314891	0.433885	0.245235
-12.212841	-7.450598	0.250240
-12.623882	-0.783095	0.255245
-12.619687	-2.840063	0.260250
-12.638285	2.232554	0.265254
-12.475353	1.205254	0.270259
-13.251107	-8.010038	0.275264
-13.877696	2.454981	0.280269
-14.096383	7.337706	0.285274
-14.296968	5.186525	0.290278
-14.286790	14.457076	0.295283
-14.260360	5.476798	0.300288
-14.700590	6.987126	0.305293
-15.191520	-0.081654	0.310298
-15.528446	-0.864063	0.315302
-16.043962	1.600659	0.320307
-15.817453	-0.484958	0.325312
-15.888099	-7.046849	0.330317
-16.282741	-1.951058	0.335322
-16.751012	-14.029405	0.340326
-17.432652	-13.815953	0.345331
-17.085212	-3.165823	0.350336
-17.510968	-2.545581	0.355341
-17.303371	-7.844505	0.360346
-17.393968	-3.294206	0.365350
-18.158963	-7.107571	0.370355
-18.351464	-4.611880	0.375360
-18.841630	1.518700	0.380365
-18.785335	-13.519451	0.385370
-18.888692	-3.656473	0.390374
-19.418011	-2.567969	0.395379
-19.097737	-3.658168	0.400384
-20.343732	5.982650	0.405389
-20.386997	2.546639	0.410394
-20.579003	-2.713281	0.415398
-20.618316	8.893101	0.420403
-20.555269	-5.860864	0.425408
-20.792071	3.219939	0.430413
-21.959292	-13.113297	0.435418
-22.133238	-2.719632	0.440422
-22.454915	-3.641690	0.445427
-22.240938	-5.872132	0.450432
-22.380636	-9.768409	0.455437
-22.485730	-5.554495	0.460442
-22.395229	-6.144821	0.465446
-22.792283	-3.425515	0.470451
-23.226979	-8.035839	0.475456
-23.860800	15.034881	0.480461
-23.954362	-2.682540	0.485466
-23.999007	-0.840206	0.490470
-23.939783	11.545345	0.495475
-24.921167	0.759316	0.500480
-25.538297	-0.493440	0.505485
-25.534338	0.673662	0.510490
-25.321593	8.908107	0.515494
-25.656640	0.531255	0.520499
-25.259494	-7.442343	0.525504
-25.692324	5.522427	0.530509
-26.606881	-1.353024	0.535514
-26.716497	-2.073652	0.540518
-27.307522	-1.765667	0.545523
-26.788284	1.541336	0.550528
-27.049658	1.666395	0.555533
-27.432697	1.965068	0.560538
-28.262683	-4.946950	0.565542
-28.889724	12.341294	0.570547
-28.818735	-1.067943	0.575552
-28.861292	-3.341919	0.580557
-28.811289	-1.522034	0.585562
-28.441103	-6.575442	0.590566
-28.811101	3.602707	0.595571
-29.622609	-5.488288	0.600576
-30.197587	5.250651	0.605581
-30.102817	6.788880	0.610586
-30.095168	-2.096146	0.615590
-30.445789	6.766698	0.620595
-31.132543	-7.170995	0.625600
-31.863451	7.243141	0.630605
-32.121608	8.240368	0.635610
-31.369483	3.410528	0.640614
-31.956205	9.649014	0.645619
-31.434229	-4.277117	0.650624
-31.845236	3.046138	0.655629
-32.589921	-5.310170	0.660634
-32.795054	-0.854888	0.665638
-33.181649	-2.156692	0.670643
-32.887728	-6.053500	0.675648
-33.502021	-4.869069	0.680653
-33.850891	1.351614	0.685658
-34.499103	-0.230740	0.690662
-34.837602	4.298574	0.695667
-34.518390	-4.468943	0.700672
-35.177858	6.549143	0.705677
-35.084226	-8.354796	0.710682
-35.264054	0.457819	0.715686
-36.192757	3.626556	0.720691
-36.110914	-2.974644	0.725696
-36.253931	-3.099107	0.730701
-36.625475	1.163677	0.735706
-36.616114	0.836059	0.740710
-36.726504	-3.480201	0.745715
-36.615767	-0.970201	0.750720
-37.548726	7.063599	0.755725
-37.693489	7.356536	0.760730
-38.175135	2.256060	0.765734
-38.156496	19.095374	0.770739
-38.255889	-4.748616	0.775744
-38.470651	5.066481	0.780749
-39.343379	-5.819872	0.785754
-39.602603	0.316839	0.790758
-39.666476	15.687105	0.795763
-39.681566	0.793134	0.800768
-40.103752	5.333221	0.805773
-40.231829	3.605618	0.810778
-39.981278	13.151841	0.815782
-40.775801	15.367797	0.820787
-40.848812	-2.250515	0.825792
-41.634082	13.989531	0.830797
-41.629677	-7.821366	0.835802
-41.157358	5.017100	0.840806
-41.435323	6.418039	0.845811
-41.930519	11.031457	0.850816
-42.441394	1.171981	0.855821
-42.610472	6.452569	0.860826
-42.487233	1.484067	0.865830
-43.353116	6.702627	0.870835
-43.875612	-1.153523	0.875840
-44.152134	-1.613940	0.880845
-43.924506	-2.586130	0.885850
-44.201403	0.071688	0.890854
-44.393420	15.898691	0.895859
-44.481686	2.600318	0.900864
-44.695301	16.425244	0.905869
-45.100663	13.653036	0.910874
-45.909585	15.739273	0.915878
-46.085537	-1.374574	0.920883
-45.983933	9.864903	0.925888
-46.094622	5.375158	0.930893
-46.182902	2.932047	0.935898
-46.118533	-1.412896	0.940902
-46.623453	3.619041	0.945907
-47.059235	3.298593	0.950912
-47.459480	17.950407	0.955917
-47.533203	0.461053	0.960922
-47.984576	7.518596	0.965926
-48.444495	7.775321	0.970931
-48.597881	6.491604	0.975936
-49.159026	12.936592	0.980941
-49.462782	-2.635569	0.985946
-48.845076	4.611796	0.990950
-49.257286	-0.511991	0.995955
-48.902656	0.732512	1.000960
-49.726374	3.602538	1.005965
-50.506374	-9.425337	1.010970
-50.533221	1.779820	1.015974
-50.626302	15.853461	1.020979
-50.793077	3.958007	1.025984
-51.939000	17.798794	1.030989
-51.826669	9.594741	1.035994
-51.658569	-4.100458	1.040998
-52.209174	2.320487	1.046003
-52.291921	-0.218936	1.051008
-52.189971	10.491400	1.056013
-52.393870	12.794134	1.061018
-52.514593	6.310265	1.066022
-53.253789	11.759854	1.071027
-53.965938	4.586857	1.076032
-53.777910	2.428083	1.081037
-54.151874	6.273663	1.086042
-54.280723	-1.275315	1.091046
-54.425101	8.650483	1.096051
-54.230678	-5.110330	1.101056
-54.838833	14.610079	1.106061
-55.579232	16.481568	1.111066
-55.315083	11.122781	1.116070
-55.729240	14.389392	1.121075
-55.735950	8.783648	1.126080
-56.212401	0.032690	1.131085
-57.169506	7.546232	1.136090
-57.137878	13.299948	1.141094
-57.301964	10.401446	1.146099
-57.494251	2.767156	1.151104
-57.397874	15.225784	1.156109
-57.383221	8.152278	1.161114
-57.125790	3.410899	1.166118
-58.087468	2.569158	1.171123
-58.440046	2.379293	1.176128
-58.889099	5.329168	1.181133
-59.074600	-9.399695	1.186138
-59.056347	1.009659	1.191142
-59.409368	-3.284259	1.196147
-59.933735	-3.767742	1.201152
-60.273734	-1.348598	1.206157
-60.502872	-3.795854	1.211162
-60.237692	6.474929	1.216166
-60.533926	5.977617	1.221171
-60.692957	0.204772	1.226176
-61.626479	11.526528	1.231181
-62.048420	-1.105431	1.236186
-61.856914	-7.909826	1.241190
-62.038111	11.620745	1.246195
-62.147929	-4.685686	1.251200
-61.963869	13.488500	1.256205
-62.386534	4.186249	1.261210
-62.840835	1.405164	1.266214
-63.694335	11.596631	1.271219
-64.079888	8.188381	1.276224
-64.055332	15.417560	1.281229
-64.512517	9.049474	1.286234
-63.875431	22.844011	1.291238
-64.275680	13.033136	1.296243
-64.161917	12.521932	1.301248
-64.909999	13.036119	1.306253
-65.388793	16.478364	1.311258
-65.300433	8.265153	1.316262
-65.573487	11.524526	1.321267
-65.795859	4.889942	1.326272
-66.449593	-1.514024	1.331277
-67.240478	4.619692	1.336282
-66.982161	-2.442975	1.341286
-67.507939	13.900391	1.346291
-67.369286	8.484803	1.351296
-67.278364	12.315215	1.356301
-67.383096	17.934804	1.361306
-67.147103	4.558378	1.366310
-67.911949	5.647137	1.371315
-68.200434	9.676099	1.376320
-68.368169	10.731684	1.381325
-68.942551	8.981849	1.386330
-69.418289	-0.152793	1.391334
-70.201530	6.524529	1.396339
-70.092303	0.457360	1.401344
-70.547521	8.973258	1.406349
-70.152569	3.207907	1.411354
-70.257973	6.343778	1.416358
-70.225862	16.457649	1.421363
-70.816606	10.204373	1.426368
-71.308772	17.686562	1.431373
-71.816351	12.526938	1.436378
-71.661823	7.899641	1.441382
-71.966870	4.222671	1.446387
-72.124285	8.759154	1.451392
-72.772233	9.872496	1.456397
-73.387751	10.270955	1.461402
-73.335730	9.966574	1.466406
-73.665330	7.502377	1.471411
-73.705662	2.511384	1.476416
-73.667065	14.266188	1.481421
-73.923326	14.080728	1.486426
-73.699149	0.119757	1.491430
-74.251484	14.367060	1.496435
-74.493986	13.722654	1.501440
-75.213100	14.375794	1.506445
-75.535947	16.974322	1.511450
-75.554396	5.584527	1.516454
-75.212735	8.557331	1.521459
-75.744828	10.298404	1.526464
-76.428046	1.166384	1.531469
-76.909881	12.450882	1.536474
-76.914647	-13.937336	1.541478
-77.204805	8.258725	1.546483
-76.960836	-7.029651	1.551488
-77.243790	7.437618	1.556493
-78.135110	-4.271589	1.561498
-78.441770	5.025564	1.566502
-78.688989	5.167721	1.571507
-78.736092	-4.850570	1.576512
-79.036057	11.185357	1.581517
-78.935386	17.435635	1.586522
-78.789102	19.555305	1.591526
-79.203678	11.440701	1.596531
-79.770189	4.830338	1.601536
-79.886709	7.936083	1.606541
-80.242585	18.228811	1.611546
-79.992818	4.979051	1.616550
-80.839188	22.973414	1.621555
-81.228161	9.199600	1.626560
-81.491758	13.460036	1.631565
-81.845850	15.639611	1.636570
-81.768222	6.792644	1.641574
-81.863575	11.910798	1.646579
-82.031006	11.888235	1.651584
-82.799034	6.117678	1.656589
-83.042400	6.802390	1.661594
-83.228113	8.043951	1.666598
-83.331516	8.479317	1.671603
-83.325309	11.333928	1.676608
-83.653551	8.115688	1.681613
-83.864032	2.294817	1.686618
-84.073846	6.610883	1.691622
-84.489839	12.766897	1.696627
-84.641330	1.656779	1.701632
-85.003879	2.646695	1.706637
-85.185737	4.420944	1.711642
-85.612581	-2.917876	1.716646
-86.362814	-4.411443	1.721651
-86.037328	-15.824618	1.726656
-86.485100	-6.421182	1.731661
-86.747632	1.969440	1.736666
-86.306838	-11.520234	1.741670
-86.640029	6.785199	1.746675
-87.287491	2.787369	1.751680
-87.325407	-1.716964	1.756685
-87.900628	12.875463	1.761690
-87.960605	8.671230	1.766694
-88.331448	2.808988	1.771699
-88.864988	2.983865	1.776704
-89.279423	-0.846090	1.781709
-89.830828	14.617270	1.786714
-88.767468	9.534238	1.791718
-89.639877	5.258679	1.796723
-89.746714	-0.882879	1.801728
-90.058862	0.518186	1.806733
-90.106280	-0.099662	1.811738
-90.380443	-7.839290	1.816742
-91.382202	-10.402530	1.821747
-91.403693	0.338652	1.826752
-91.568839	0.054278	1.831757
-91.497472	1.006320	1.836762
-91.286544	1.351262	1.841766
-91.505137	2.739529	1.846771
-92.088284	8.023043	1.851776
-92.683860	4.431678	1.856781
-93.206225	0.436951	1.861786
-93.270965	-8.332219	1.866790
-93.370956	0.318921	1.871795
-92.925800	-7.384997	1.876800
-93.714025	0.005037	1.881805
-93.956320	-3.138812	1.886810
-93.831198	0.130717	1.891814
-94.323150	5.480054	1.896819
-94.909009	-0.400713	1.901824
-95.722788	-1.096416	1.906829
-95.983394	5.353949	1.911834
-95.823966	-8.324319	1.916838
-96.000232	0.919908	1.921843
-95.926976	-8.636343	1.926848
-95.986042	-2.749952	1.931853
-96.021990	-2.272066	1.936858
-96.326935	-3.486731	1.941862
-97.144857	-2.353583	1.946867
-97.703986	6.379754	1.951872
-97.543981	5.838612	1.956877
-97.753479	12.251036	1.961882
-97.712454	-1.023609	1.966886
-98.718078	-0.531473	1.971891
-98.734468	3.757262	1.976896
-98.714656	-1.582448	1.981901
-99.313904	3.929249	1.986906
-99.075830	-8.207321	1.991910
-99.208357	0.062568	1.996915
-100.102927	5.719161	2.006912
-99.904275	0.978302	2.016909
-99.175279	8.099901	2.026906
-98.117043	-0.491203	2.036902
-98.097835	1.651748	2.046899
-97.774531	0.343715	2.056896
-97.086553	11.908390	2.066893
-96.575385	6.273477	2.076890
-96.099841	0.722541	2.086886
-95.055618	7.970441	2.096883
-94.874815	-4.796765	2.106880
-94.816196	3.328652	2.116877
-94.444295	-0.168295	2.126874
-93.687820	-3.709587	2.136870
-93.482090	-5.769616	2.146867
-92.273617	-5.307889	2.156864
-92.035840	-4.257966	2.166861
-91.782162	-4.018846	2.176858
-90.863550	-6.366397	2.186854
-90.799481	-7.773633	2.196851
-89.688950	1.430970	2.206848
-89.245767	3.483799	2.216845
-89.253005	12.210864	2.226842
-88.795056	3.055210	2.236838
-88.021344	-0.094499	2.246835
-87.850774	-0.535332	2.256832
-87.122370	-0.088352	2.266829
-86.528024	7.982857	2.276826
-86.219762	3.665976	2.286822
-85.075030	-6.690111	2.296819
-84.860731	-3.219735	2.306816
-84.812552	-6.060864	2.316813
-84.036864	-7.710467	2.326810
-83.443383	1.050025	2.336806
-83.092616	-3.234810	2.346803
-82.764161	-4.012500	2.356800
-82.032431	-1.873708	2.366797
-81.572240	0.592227	2.376794
-80.621941	-0.883338	2.386790
-80.261308	4.767002	2.396787
-80.367703	-1.792326	2.406784
-79.506142	0.112286	2.416781
-79.068390	-0.090634	2.426778
-78.607145	1.748314	2.436774
-77.917333	-9.756432	2.446771
-77.100691	-7.069611	2.456768
-76.948706	-7.401133	2.466765
-77.008244	-4.586004	2.476762
-75.847380	-6.438741	2.486758
-75.329128	-7.079870	2.496755
-75.373657	-12.336276	2.506752
-73.877173	-6.635546	2.516749
-74.143857	-3.486977	2.526746
-73.734745	-3.650985	2.536742
-73.201081	-4.669534	2.546739
-72.496104	-7.541567	2.556736
-71.950987	-4.854915	2.566733
-71.148571	-3.215188	2.576730
-70.916486	-9.123774	2.586726
-70.514513	-6.431048	2.596723
-70.328477	-6.358109	2.606720
-69.630503	-5.935980	2.616717
-69.052370	-7.330823	2.626714
-68.064257	-2.200793	2.636710
-67.792284	-2.195497	2.646707
-67.445530	-2.265186	2.656704
-67.471889	3.857717	2.666701
-66.337478	-1.830554	2.676698
-65.987258	4.017785	2.686694
-65.600979	0.843451	2.696691
-64.623226	-1.902821	2.706688
-64.038878	-5.351308	2.716685
-64.346850	-3.781050	2.726682
-63.855921	2.902835	2.736678
-62.836367	-1.920198	2.746675
-62.570557	-14.572787	2.756672
-61.543917	-7.793214	2.766669
-61.405467	-5.457837	2.776666
-61.212354	-2.374537	2.786662
-60.742523	-1.349282	2.796659
-59.653181	0.076435	2.806656
-59.684977	2.633954	2.816653
-58.991128	1.399570	2.826650
-58.066476	2.616221	2.836646
-58.026379	-2.322617	2.846643
-57.806765	-1.428333	2.856640
-57.211172	-0.826688	2.866637
-56.567723	-0.641955	2.876634
-55.388852	-4.360968	2.886630
-55.124788	-9.884951	2.896627
-54.998230	-1.325654	2.906624
-54.958105	2.308049	2.916621
-54.062482	9.901605	2.926618
-53.585053	7.738392	2.936614
-52.263900	2.193953	2.946611
-52.522189	0.863500	2.956608
-52.079258	6.320116	2.966605
-51.773950	3.067248	2.976602
-51.016557	-3.166019	2.986598
-50.519803	0.174359	2.996595
-49.688340	-0.886834	3.006592
-48.997726	-8.640906	3.016589
-48.734480	-2.702281	3.026586
-48.719771	-11.596549	3.036582
-48.147159	0.268818	3.046579
-47.324241	-6.011381	3.056576
-47.184667	2.295062	3.066573
-46.252257	-3.039428	3.076570
-45.785315	-2.037500	3.086566
-45.435494	-8.916359	3.096563
-45.248394	1.072319	3.106560
-45.016480	-4.522662	3.116557
-43.826812	-0.233419	3.126554
-43.124002	4.514763	3.136550
-43.036448	-4.693225	3.146547
-42.325389	-0.954318	3.156544
-41.637072	2.474621	3.166541
-41.593888	-2.030981	3.176538
-41.230575	3.198903	3.186534
-40.056349	-2.250178	3.196531
-39.629608	-3.474843	3.206528
-39.426609	-0.020326	3.216525
-39.069748	-8.932419	3.226522
-38.320326	-12.570282	3.236518
-38.270221	-3.635973	3.246515
-36.972697	-4.777890	3.256512
-36.640916	-7.902122	3.266509
-36.562317	-6.728937	3.276506
-36.122098	-15.601658	3.286502
-35.363132	-9.752464	3.296499
-34.390678	-8.027383	3.306496
-34.392931	-9.405334	3.316493
-34.348576	-3.559344	3.326490
-33.115171	-2.253840	3.336486
-32.877858	-9.941889	3.346483
-32.568283	-6.846670	3.356480
-31.826569	-8.650035	3.366477
-31.553603	3.977265	3.376474
-31.027696	-5.180678	3.386470
-29.763387	3.253920	3.396467
-29.731637	2.357338	3.406464
-29.780658	0.378970	3.416461
-29.036375	3.632710	3.426458
-28.454378	4.254582	3.436454
-27.967927	-3.808769	3.446451
-26.749901	-10.395137	3.456448
-26.974764	-6.281773	3.466445
-26.818938	-1.196639	3.476442
-25.860555	1.187910	3.486438
-25.042825	0.063003	3.496435
-25.183028	-2.864990	3.506432
-24.246673	-4.417317	3.516429
-23.608465	-7.584088	3.526426
-23.294835	-5.181053	3.536422
-23.365594	-2.621442	3.546419
-22.235918	-12.483202	3.556416
-21.778900	-7.828249	3.566413
-21.614259	-2.053304	3.576410
-20.630985	-5.112877	3.586406
-20.353702	-6.973932	3.596403
-20.075165	-6.267189	3.606400
-19.117473	-6.605617	3.616397
-18.833320	-1.961608	3.626394
-18.882559	-3.615247	3.636390
-17.560707	-5.016183	3.646387
-17.066047	-7.920775	3.656384
-17.157178	-4.808675	3.666381
-16.456571	-8.675347	3.676378
-15.937861	-4.624408	3.686374
-15.474606	-3.010810	3.696371
-14.631457	-7.793917	3.706368
-14.354973	-7.152030	3.716365
-14.162879	-4.355913	3.726362
-13.186440	-2.416341	3.736358
-12.632754	0.982793	3.746355
-12.406118	-1.651990	3.756352
-11.551665	-1.841434	3.766349
-11.088037	-0.775242	3.776346
-10.929746	9.211441	3.786342
-10.617820	0.513911	3.796339
-9.468288	4.729389	3.806336
-8.988890	2.012532	3.816333
-9.038891	4.698562	3.826330
-8.505423	-0.174085	3.836326
-7.531663	4.598326	3.846323
-7.337728	0.150390	3.856320
-7.313124	3.388969	3.866317
-6.390909	5.862919	3.876314
-6.010678	7.593565	3.886310
-5.253408	9.521104	3.896307
-4.616577	6.957616	3.906304
-4.685192	5.937894	3.916301
-3.847396	25.621690	3.926298
-3.465687	27.037130	3.936294
-3.011927	38.302178	3.946291
-2.617980	36.812914	3.956288
-2.138434	41.559584	3.966285
-1.804786	47.835593	3.976282
-1.142307	75.353821	3.986278
-0.798041	81.179128	3.996275
-0.375589	101.922142	4.006272
0.000000	124.099884	4.011277
0.343258	120.428508	4.016282
0.148910	144.492573	4.021286
0.261100	141.970337	4.026291
0.559516	159.077202	4.031296
0.396291	167.853332	4.036301
0.713745	160.576303	4.041306
0.832049	159.626117	4.046310
0.706540	149.817096	4.051315
0.550148	159.712129	4.056320
0.841273	173.207546	4.061325
1.254438	182.486485	4.066330
0.816316	197.947987	4.071334
1.003175	182.995994	4.076339
0.902560	186.775137	4.081344
0.839926	191.643477	4.086349
1.226313	189.869804	4.091354
1.024175	187.812675	4.096358
0.996346	189.024704	4.101363
1.382409	182.324216	4.106368
1.068093	195.990539	4.111373
1.156667	191.010834	4.116378
1.132448	184.520605	4.121382
1.257053	185.177859	4.126387
1.087299	183.768874	4.131392
0.757840	194.885968	4.136397
1.167437	191.087397	4.141402
1.261788	185.958261	4.146406
1.448795	185.122012	4.151411
1.583096	188.616386	4.156416
1.483878	197.289910	4.161421
1.746777	186.631576	4.166426
1.211113	182.893222	4.171430
1.146040	171.381465	4.176435
1.453188	184.183852	4.181440
1.272535	185.901589	4.186445
1.217525	179.220619	4.191450
1.222629	193.312733	4.196454
1.784951	192.983411	4.201459
1.233919	179.387446	4.206464
1.104223	180.701547	4.211469
1.482798	189.489474	4.216474
1.317178	190.419724	4.221478
1.682707	192.526078	4.226483
1.382169	183.722948	4.231488
1.305799	192.832304	4.236493
1.344970	191.320128	4.241498
1.165012	193.579865	4.246502
1.421026	203.550023	4.251507
1.392537	197.156684	4.256512
1.293084	199.494473	4.261517
1.530606	188.724312	4.266522
1.220083	200.786561	4.271526
1.579787	187.817297	4.276531
1.485262	196.390896	4.281536
1.582482	197.430232	4.286541
1.407177	189.453167	4.291546
1.442804	194.585058	4.296550
1.398698	194.325465	4.301555
1.225984	180.511105	4.306560
1.498343	191.847500	4.311565
1.258606	191.944616	4.316570
1.498293	203.071844	4.321574
1.797434	218.764325	4.326579
1.627780	214.653035	4.331584
1.614221	224.198843	4.336589
1.761320	225.830161	4.341594
1.751535	226.152886	4.346598
1.823406	223.216531	4.351603
1.753665	223.875222	4.356608
1.772168	217.985442	4.361613
1.856695	225.192286	4.366618
1.933617	230.854843	4.371622
2.099017	223.241535	4.376627
1.667753	212.374305	4.381632
1.651762	212.858568	4.386637
1.618134	206.922456	4.391642
1.658399	228.289698	4.396646
1.905918	233.605307	4.401651
1.859809	231.283836	4.406656
1.740748	224.768519	4.411661
1.970272	229.624206	4.416666
1.775362	237.327499	4.421670
2.129934	227.672908	4.426675
1.994683	224.974406	4.431680
1.754854	234.770216	4.436685
1.754599	238.179795	4.441690
1.795495	232.780083	4.446694
1.808014	225.758422	4.451699
2.044122	230.836478	4.456704
1.756088	230.812928	4.461709
1.993914	221.177633	4.466714
1.544372	224.938481	4.471718
1.629088	225.166566	4.476723
1.651929	233.417719	4.481728
1.714857	231.283336	4.486733
2.249079	250.906133	4.491738
2.419384	256.895408	4.496742
2.121272	248.875071	4.501747
1.891775	241.104247	4.506752
2.038084	244.570110	4.511757
2.096950	246.678610	4.516762
2.173528	259.237795	4.521766
2.429768	265.362928	4.526771
2.722511	251.872425	4.531776
2.377181	244.965731	4.536781
2.306935	225.039126	4.541786
2.084854	234.074718	4.546790
1.970483	218.541071	4.551795
2.183915	236.943904	4.556800
1.774339	221.259457	4.561805
1.914130	235.239280	4.566810
2.011346	266.878709	4.571814
2.173112	262.221724	4.576819
2.249758	266.391868	4.581824
2.176654	265.134324	4.586829
2.191877	257.204169	4.591834
2.233290	273.327312	4.596838
2.092356	269.996862	4.601843
2.410190	261.193411	4.606848
2.192855	272.917907	4.611853
2.318506	264.024472	4.616858
2.159493	266.096862	4.621862
2.309520	270.623264	4.626867
2.481303	255.888072	4.631872
2.083388	274.798145	4.636877
2.515663	263.414170	4.641882
2.456986	267.705235	4.646886
2.338738	273.343235	4.651891
2.708864	285.376730	4.656896
2.179265	260.971911	4.661901
2.599554	271.890874	4.666906
2.338455	293.834931	4.671910
2.676694	284.073298	4.676915
2.787416	307.679359	4.681920
2.549785	286.736056	4.686925
2.709498	263.838048	4.691930
2.432014	271.091813	4.696934
2.631885	279.767654	4.701939
2.679887	283.677249	4.706944
2.382837	280.421233	4.711949
2.464121	277.563618	4.716954
2.638264	286.979396	4.721958
2.741766	288.382137	4.726963
2.725625	295.147291	4.731968
2.575892	297.817786	4.736973
2.902074	292.939565	4.741978
3.040715	291.773208	4.746982
2.897656	289.429866	4.751987
2.567048	283.161593	4.756992
2.521184	270.907158	4.761997
2.922868	266.676182	4.767002
2.808169	294.342283	4.772006
2.688185	293.049272	4.777011
2.921134	295.265848	4.782016
2.842498	299.204366	4.787021
2.779234	282.399899	4.792026
2.729534	298.584494	4.797030
2.818615	301.759813	4.802035
2.720299	293.450126	4.807040
2.707408	299.433682	4.812045
3.172975	297.203944	4.817050
2.884007	293.493954	4.822054
2.759168	297.006511	4.827059
2.938070	298.573981	4.832064
2.829877	297.580021	4.837069
3.035055	299.171364	4.842074
2.866867	300.484733	4.847078
2.990627	288.084654	4.852083
2.920451	292.269400	4.857088
2.721893	302.630936	4.862093
3.132279	297.327006	4.867098
2.671953	302.443714	4.872102
2.865396	301.420528	4.877107
3.165878	296.601800	4.882112
3.020006	295.970809	4.887117
3.150187	282.127020	4.892122
2.671615	292.265096	4.897126
3.059485	294.942644	4.902131
3.088027	300.931488	4.907136
2.941748	303.148186	4.912141
2.828850	300.359258	4.917146
2.845605	308.910584	4.922150
2.856149	323.683438	4.927155
3.233774	320.533261	4.932160
3.168934	341.172579	4.937165
3.480173	323.563195	4.942170
3.073884	330.938804	4.947174
2.813101	341.249679	4.952179
3.162448	334.096834	4.957184
3.117597	335.285149	4.962189
3.145785	333.843045	4.967194
3.038833	346.585054	4.972198
3.196920	336.986148	4.977203
2.914604	339.449479	4.982208
3.051635	338.809719	4.987213
3.526348	333.877342	4.992218
3.260516	341.001946	4.997222
3.029395	351.304177	5.002227
3.037075	333.450061	5.007232
3.541847	350.216808	5.012237
3.393360	347.174680	5.017242
3.247117	339.138868	5.022246
3.348860	359.779391	5.027251
3.914727	357.276760	5.032256
3.624201	353.057154	5.037261
3.995637	328.692847	5.042266
3.643870	342.369238	5.047270
3.403601	341.037695	5.052275
3.670441	329.511813	5.057280
2.989452	331.476709	5.062285
3.163978	332.982554	5.067290
3.209980	338.649373	5.072294
3.271309	353.916422	5.077299
3.642695	355.440249	5.082304
3.506149	366.811495	5.087309
4.072912	354.029655	5.092314
3.558847	353.565859	5.097318
3.614188	341.575815	5.102323
3.713364	336.467930	5.107328
3.297981	345.509487	5.112333
3.743854	345.715380	5.117338
3.661697	353.394574	5.122342
3.614934	359.709811	5.127347
3.831314	363.133045	5.132352
3.642663	363.580041	5.137357
4.049126	350.838308	5.142362
3.494875	345.294212	5.147366
3.487986	339.953562	5.152371
3.559866	352.939106	5.157376
3.670593	367.296676	5.162381
4.032726	366.907892	5.167386
3.839409	371.556867	5.172390
3.804450	375.284657	5.177395
3.893451	368.383479	5.182400
3.823310	368.691812	5.187405
3.977113	358.893426	5.192410
3.731453	367.003250	5.197414
3.622068	358.572036	5.202419
4.105506	363.049583	5.207424
3.691344	369.285742	5.212429
3.625719	358.290010	5.217434
3.712912	360.820635	5.222438
3.899447	359.429313	5.227443
4.257243	355.095170	5.232448
3.897935	375.417770	5.237453
3.975507	357.151727	5.242458
3.995232	374.906004	5.247462
4.088194	361.366238	5.252467
4.187012	364.449592	5.257472
3.569890	373.216989	5.262477
3.592751	369.647632	5.267482
3.756362	359.011112	5.272486
3.558010	363.004059	5.277491
3.616156	363.016926	5.282496
3.427998	376.103768	5.287501
4.367363	394.079905	5.292506
4.339710	400.760091	5.297510
4.266386	392.187443	5.302515
3.807555	381.650512	5.307520
3.782366	387.146204	5.312525
4.293841	393.442901	5.317530
4.289777	409.316404	5.322534
4.213566	386.634488	5.327539
4.496843	396.097214	5.332544
4.114794	383.630488	5.337549
4.182087	363.730895	5.342554
3.867439	385.541373	5.347558
4.236256	392.553527	5.352563
4.369138	390.552884	5.357568
4.391963	409.346435	5.362573
4.117022	399.993968	5.367578
4.126961	403.893803	5.372582
4.290109	407.344293	5.377587
4.227831	397.331691	5.382592
4.281928	410.809957	5.387597
4.247516	410.202964	5.392602
4.608647	403.048831	5.397606
4.033574	414.708541	5.402611
4.383877	399.101967	5.407616
4.274759	410.024558	5.412621
4.303348	414.667359	5.417626
4.177414	406.133685	5.422630
4.187691	408.884209	5.427635
4.414826	394.418345	5.432640
4.379237	403.244353	5.437645
4.457958	401.084744	5.442650
4.280211	401.262480	5.447654
4.294992	404.200496	5.452659
4.466298	408.674389	5.457664
4.274954	403.960779	5.462669
4.427923	395.426108	5.467674
4.479301	404.420951	5.472678
4.395628	404.834914	5.477683
4.452199	391.938362	5.482688
4.365883	415.796761	5.487693
4.893298	420.252457	5.492698
4.767838	410.044884	5.497702
4.687020	409.318785	5.502707
4.634488	413.539816	5.507712
4.614083	400.315215	5.512717
4.331262	402.583595	5.517722
4.287404	414.377399	5.522726
4.331459	426.181053	5.527731
4.677931	415.423610	5.532736
4.385764	436.632385	5.537741
4.504149	433.333236	5.542746
4.289112	436.153456	5.547750
4.252226	434.513830	5.552755
4.377497	436.715664	5.557760
4.483083	448.666624	5.562765
4.848825	464.481736	5.567770
4.800151	470.187039	5.572774
5.030507	467.416139	5.577779
4.989837	466.730661	5.582784
4.725730	448.609468	5.587789
5.043098	439.565466	5.592794
4.799634	445.300187	5.597798
4.704221	450.436159	5.602803
4.948844	447.718351	5.607808
4.702173	443.335593	5.612813
4.794249	452.809232	5.617818
4.743320	455.239376	5.622822
4.918957	467.174631	5.627827
4.876500	461.867638	5.632832
4.930460	475.872913	5.637837
4.523736	472.428291	5.642842
4.952141	472.334886	5.647846
4.912134	466.501838	5.652851
4.905729	469.033150	5.657856
4.647387	466.716625	5.662861
4.833590	466.468198	5.667866
4.699168	469.519774	5.672870
4.690030	476.191408	5.677875
5.060013	459.450411	5.682880
4.656328	477.852515	5.687885
4.902651	491.041885	5.692890
5.289511	487.610651	5.697894
5.416508	500.902127	5.702899
5.134949	484.047583	5.707904
5.438355	479.585653	5.712909
5.058579	470.046049	5.717914
5.036785	480.597415	5.722918
4.752576	471.581970	5.727923
5.096116	489.169806	5.732928
4.907917	500.402982	5.737933
5.282847	492.101999	5.742938
5.585850	508.010790	5.747942
5.307949	503.140085	5.752947
5.550874	496.940915	5.757952
5.193303	493.912592	5.762957
5.395268	489.222061	5.767962
5.141799	486.215210	5.772966
5.302345	494.883859	5.777971
5.538722	489.044691	5.782976
5.131170	487.172117	5.787981
5.411329	483.833496	5.792986
5.426119	488.988069	5.797990
4.954201	482.977082	5.802995
5.493189	483.923210	5.808000
5.484518	506.140672	5.813005
5.485340	484.655130	5.818010
5.386586	491.665375	5.823014
5.352018	502.449726	5.828019
5.575918	493.844380	5.833024
5.060364	506.144477	5.838029
5.410416	501.756323	5.843034
5.274809	492.580951	5.848038
5.320162	511.022543	5.853043
5.307684	493.754838	5.858048
5.289875	506.553380	5.863053
5.077050	496.458746	5.868058
5.017496	491.242768	5.873062
5.136754	503.830123	5.878067
5.720705	516.324221	5.883072
5.367128	517.441330	5.888077
5.615058	521.823274	5.893082
5.729204	525.585655	5.898086
5.631264	531.043993	5.903091
5.529078	519.352828	5.908096
5.761912	531.629804	5.913101
5.858217	514.620637	5.918106
5.429685	513.939563	5.923110
5.377439	512.946309	5.928115
5.627429	533.649091	5.933120
5.372210	531.379002	5.938125
5.532043	546.228129	5.943130
6.197193	531.302521	5.948134
5.523047	549.972865	5.953139
5.947389	531.182559	5.958144
5.742493	541.580227	5.963149
5.915823	540.441565	5.968154
5.926935	529.498341	5.973158
5.899571	535.102179	5.978163
5.918376	529.392873	5.983168
5.895990	530.005077	5.988173
6.015866	513.612870	5.993178
5.790421	507.660590	5.998182
5.547792	513.723433	6.003187
5.690122	521.629227	6.008192
5.987519	520.219965	6.013197
5.976599	522.579380	6.018202
6.085947	528.831892	6.023206
6.038318	521.799417	6.028211
6.123393	504.277319	6.033216
5.986013	510.215625	6.038221
5.617156	497.515570	6.043226
5.801535	499.075447	6.048230
5.588681	513.882639	6.053235
6.015400	516.668151	6.058240
5.904563	528.281024	6.063245
5.972116	508.944044	6.068250
5.762437	515.754005	6.073254
5.682658	523.015073	6.078259
6.328745	529.005447	6.083264
5.906875	516.317294	6.088269
5.652892	507.076235	6.093274
5.711581	509.136360	6.098278
5.776702	523.759011	6.103283
6.012013	536.427155	6.108288
5.917503	537.644015	6.113293
5.881370	518.610956	6.118298
5.731987	525.527669	6.123302
5.749586	536.623469	6.128307
5.766181	527.569727	6.133312
5.897169	537.046065	6.138317
5.884349	530.175847	6.143322
6.013318	537.292916	6.148326
5.761000	542.099383	6.153331
6.274747	531.896200	6.158336
5.868482	532.531588	6.163341
5.662232	515.980269	6.168346
5.894967	526.496906	6.173350
5.711381	537.431498	6.178355
6.103001	533.802743	6.183360
5.816920	536.863411	6.188365
5.807276	533.147751	6.193370
6.105255	533.405417	6.198374
6.019900	532.861593	6.203379
5.954148	497.835577	6.208384
5.524141	515.960606	6.213389
5.856299	520.521111	6.218394
6.321724	524.256915	6.223398
6.121359	524.920827	6.228403
6.237739	509.363453	6.233408
5.803781	490.451419	6.238413
5.700124	497.878220	6.243418
5.942901	506.565055	6.248422
5.612247	493.344683	6.253427
5.820373	492.705796	6.258432
5.892984	505.222428	6.263437
5.636696	493.101148	6.268442
5.851907	499.573130	6.273446
5.789540	510.408745	6.278451
5.884862	518.154093	6.283456
5.865111	519.235177	6.288461
5.798858	522.255075	6.293466
5.857185	533.148898	6.298470
6.123565	522.326775	6.303475
6.310276	504.738454	6.308480
5.982579	502.334530	6.313485
6.098986	500.440383	6.318490
5.945253	495.144960	6.323494
5.861253	507.208293	6.328499
6.176148	493.626606	6.333504
5.612231	498.892403	6.338509
5.823501	493.807774	6.343514
5.938300	510.602934	6.348518
5.553441	514.818926	6.353523
6.080134	502.845772	6.358528
5.852934	516.444313	6.363533
5.960138	503.635393	6.368538
6.077753	499.911734	6.373542
5.870322	504.589324	6.378547
5.790330	504.523599	6.383552
5.892202	508.717659	6.388557
5.768041	503.233350	6.393562
5.934308	489.211846	6.398566
5.667186	507.845560	6.403571
5.992306	487.696315	6.408576
5.946122	500.463828	6.413581
5.609462	503.992691	6.418586
5.499581	502.684772	6.423590
5.636438	505.498649	6.428595
5.771237	509.519057	6.433600
5.597745	524.281870	6.438605
5.979762	534.246515	6.443610
6.112088	536.595875	6.448614
5.787070	532.683122	6.453619
5.681948	520.022140	6.458624
5.815520	528.450595	6.463629
5.730959	537.538718	6.468634
6.107372	533.367292	6.473638
5.935198	533.386157	6.478643
6.141204	533.091639	6.483648
5.745921	529.834537	6.488653
5.822269	530.952720	6.493658
6.064831	542.834058	6.498662
5.613067	537.515357	6.503667
6.326440	534.297223	6.508672
5.852330	524.273175	6.513677
5.453205	512.498588	6.518682
5.808391	526.147700	6.523686
5.727219	543.486624	6.528691
6.020458	536.266202	6.533696
5.964991	538.878245	6.538701
5.903952	536.228790	6.543706
5.873465	539.235974	6.548710
5.783476	541.888647	6.553715
6.155612	526.987983	6.558720
5.838145	534.579476	6.563725
5.738135	545.723032	6.568730
6.123936	541.987503	6.573734
5.815476	538.482330	6.578739
6.004228	530.549602	6.583744
5.771540	512.943660	6.588749
5.988448	519.395738	6.593754
5.967249	514.384443	6.598758
5.524641	514.315204	6.603763
5.760123	531.823274	6.608768
6.129200	528.887274	6.613773
5.817011	541.548720	6.618778
5.917262	542.780554	6.623782
5.904898	548.922861	6.628787
6.321008	526.352850	6.633792
5.818037	533.288732	6.638797
5.842580	515.698882	6.643802
5.480046	514.133188	6.648806
5.943147	521.707068	6.653811
5.797588	530.796486	6.658816
6.120655	518.219246	6.663821
5.628705	516.424446	6.668826
5.836100	515.937316	6.673830
5.895429	532.005678	6.678835
6.160598	527.480203	6.683840
5.949435	511.360738	6.688845
5.468075	499.894244	6.693850
5.821656	527.129789	6.698854
5.998521	528.283749	6.703859
6.128922	519.528094	6.708864
5.827998	518.626348	6.713869
5.815466	507.495158	6.718874
5.917784	500.177752	6.723878
5.612243	519.975678	6.728883
6.002455	523.578784	6.733888
6.075940	534.133088	6.738893
5.823973	524.387148	6.743898
6.025855	520.461812	6.748902
5.641116	510.152781	6.753907
5.907120	517.427739	6.758912
6.075989	536.114340	6.763917
6.088807	528.003406	6.768922
5.941085	514.875713	6.773926
5.439918	518.122078	6.778931
5.973791	499.733401	6.783936
5.653573	513.724183	6.788941
5.991834	515.412341	6.793946
5.979587	516.277110	6.798950
5.645681	509.577957	6.803955
5.923539	527.892256	6.808960
5.866324	529.330064	6.813965
5.955251	536.883503	6.818970
6.489494	520.804027	6.823974
6.003790	516.236204	6.828979
5.802012	511.074997	6.833984
6.227421	508.195792	6.838989
5.544140	508.200658	6.843994
5.798142	511.669602	6.848998
5.517096	512.202017	6.854003
5.856203	503.046651	6.859008
5.902706	520.701466	6.864013
5.707144	506.759471	6.869018
5.643209	508.179741	6.874022
5.752808	532.854107	6.879027
6.089462	533.470613	6.884032
6.528321	544.952704	6.889037
5.761956	526.790799	6.894042
6.170789	521.302264	6.899046
5.856881	507.566486	6.904051
5.907263	509.785441	6.909056
5.607160	509.233006	6.914061
5.604792	516.482858	6.919066
5.946742	505.251555	6.924070
5.680781	512.246130	6.929075
5.971469	522.913604	6.934080
5.764002	517.766654	6.939085
5.660128	524.248953	6.944090
5.885651	535.174540	6.949094
5.899292	546.849828	6.954099
5.866669	560.423850	6.959104
6.060217	549.684975	6.964109
5.947405	540.071317	6.969114
5.931772	531.088605	6.974118
5.890956	518.512598	6.979123
5.976780	506.548958	6.984128
5.692771	513.481895	6.989133
5.535377	512.777325	6.994138
6.222153	535.833828	6.999142
6.105424	542.353086	7.004147
5.776527	522.326968	7.009152
5.545603	526.589545	7.014157
5.568846	545.705509	7.019162
6.174237	545.795366	7.024166
6.139421	547.394134	7.029171
5.941032	541.558324	7.034176
5.885281	531.534000	7.039181
5.595347	514.938105	7.044186
5.877766	520.286721	7.049190
5.860859	545.103756	7.054195
6.244379	534.626118	7.059200
5.990563	520.350407	7.064205
5.573283	513.775428	7.069210
6.238931	510.205282	7.074214
5.626371	504.080788	7.079219
5.884550	505.365744	7.084224
5.692596	493.922660	7.089229
6.031554	512.720331	7.094234
6.065550	509.170609	7.099238
6.115083	505.026966	7.104243
5.998794	510.559954	7.109248
6.353843	510.713082	7.114253
5.979272	516.868073	7.119258
5.974040	508.379411	7.124262
5.892308	516.687066	7.129267
5.984788	506.746884	7.134272
6.156381	517.164700	7.139277
5.973366	522.453787	7.144282
5.665453	513.657802	7.149286
5.273565	521.831730	7.154291
6.065403	514.773003	7.159296
5.724967	508.725677	7.164301
5.916287	511.879902	7.169306
5.898523	515.686278	7.174310
5.786701	516.364366	7.179315
5.916736	516.767384	7.184320
5.557337	511.407679	7.189325
5.641389	513.918228	7.194330
5.637945	500.171898	7.199334
5.610554	516.970929	7.204339
5.794308	512.148930	7.209344
5.959939	529.049364	7.214349
5.903679	521.390455	7.219354
5.954025	519.200890	7.224358
5.676747	525.814844	7.229363
5.959004	530.771127	7.234368
6.069290	535.284147	7.239373
6.185265	527.351608	7.244378
5.846289	510.168324	7.249382
5.352255	513.763153	7.254387
5.824774	528.100648	7.259392
5.933538	538.743343	7.264397
5.923032	555.773445	7.269402
5.975988	541.980662	7.274406
6.013026	540.833346	7.279411
6.023000	532.889315	7.284416
5.841963	525.940051	7.289421
5.914344	507.254503	7.294426
5.960031	502.882314	7.299430
5.729270	514.225730	7.304435
5.881833	506.629202	7.309440
5.869362	509.745280	7.314445
5.605922	526.305904	7.319450
5.685824	527.775412	7.324454
5.948440	538.270840	7.329459
6.058622	540.709693	7.334464
6.007494	535.154009	7.339469
5.612602	523.657226	7.344474
6.074573	522.746812	7.349478
6.188214	533.967524	7.354483
6.110700	518.993285	7.359488
5.761000	516.783898	7.364493
5.778872	518.224095	7.369498
5.916908	506.504983	7.374502
5.762098	514.632527	7.379507
6.075374	508.922120	7.384512
6.205587	518.616312	7.389517
5.847837	511.075699	7.394522
5.820032	505.876273	7.399526
5.755657	517.204922	7.404531
6.093082	509.961129	7.409536
5.893236	503.784515	7.414541
5.782983	518.655557	7.419546
6.077466	514.331141	7.424550
5.760267	516.737815	7.429555
6.017189	510.364859	7.434560
5.485229	526.168458	7.439565
5.668691	517.644762	7.444570
6.130437	513.888698	7.449574
5.897612	511.150824	7.454579
6.236235	504.960206	7.459584
6.147760	505.000262	7.464589
5.875552	498.833832	7.469594
6.198219	512.674966	7.474598
6.020672	507.767844	7.479603
6.230118	507.679052	7.484608
6.112314	509.772289	7.489613
5.790523	513.079678	7.494618
6.002674	495.188723	7.499622
5.672613	513.576237	7.504627
5.757089	500.467604	7.509632
5.833493	507.237191	7.514637
5.754265	508.245427	7.519642
6.130279	514.239581	7.524646
5.593913	519.189764	7.529651
5.787477	513.207308	7.534656
5.764443	520.855603	7.539661
5.556911	511.346112	7.544666
5.871244	519.649485	7.549670
5.527911	519.266880	7.554675
5.870514	519.474255	7.559680
5.731134	521.113977	7.564685
5.599479	510.730664	7.569690
6.157220	508.124973	7.574694
5.802039	512.627002	7.579699
5.786079	510.194548	7.584704
6.154872	500.359853	7.589709
5.413680	510.029041	7.594714
5.782594	500.965139	7.599718
5.535345	511.158757	7.604723
5.556223	507.407081	7.609728
6.002287	528.684989	7.614733
5.884381	538.899970	7.619738
6.046601	531.967282	7.624742
5.943565	539.409983	7.629747
5.916463	528.364749	7.634752
5.861523	520.617620	7.639757
5.664017	521.731038	7.644762
6.152094	520.464693	7.649766
5.835694	517.515591	7.654771
5.712998	499.613668	7.659776
6.169923	509.534742	7.664781
5.657720	524.722608	7.669786
6.080789	509.135764	7.674790
5.727909	515.251061	7.679795
5.999345	506.009403	7.684800
5.515117	513.229075	7.689805
5.682683	537.077870	7.694810
5.979336	533.606975	7.699814
6.056739	546.512943	7.704819
6.264153	538.986655	7.709824
6.195861	524.699619	7.714829
5.964965	520.632010	7.719834
6.022747	507.494436	7.724838
5.823359	513.370378	7.729843
5.720173	506.380930	7.734848
5.664761	508.909691	7.739853
5.880336	516.744381	7.744858
5.878549	503.991357	7.749862
5.317971	511.848249	7.754867
5.494867	516.460062	7.759872
6.308281	531.845011	7.764877
5.919391	539.297756	7.769882
5.768352	519.721827	7.774886
5.738931	534.179863	7.779891
5.899639	539.736147	7.784896
6.281337	530.426727	7.789901
5.917679	525.463043	7.794906
6.250296	507.020203	7.799910
6.272581	513.885752	7.804915
6.001193	495.957991	7.809920
6.009172	505.696250	7.814925
6.063262	502.614695	7.819930
5.961526	493.746470	7.824934
5.798687	514.995148	7.829939
5.837212	502.033610	7.834944
6.009761	500.804413	7.839949
5.877618	505.501526	7.844954
6.072368	504.095220	7.849958
5.425739	499.875915	7.854963
5.625894	504.940272	7.859968
5.549581	498.663727	7.864973
5.529788	504.907283	7.869978
5.453334	496.613703	7.874982
5.543505	526.185089	7.879987
5.644315	531.031757	7.884992
5.958732	544.945415	7.889997
5.753667	544.445150	7.895002
6.243793	539.437155	7.900006
5.895352	545.518384	7.905011
5.853899	544.423995	7.910016
5.924275	538.338268	7.915021
5.846455	547.092115	7.920026
5.990662	542.595011	7.925030
5.701185	542.195515	7.930035
6.002214	550.261857	7.935040
5.981941	554.045966	7.940045
6.000860	559.636245	7.945050
6.402206	537.129234	7.950054
5.620700	534.898759	7.955059
5.698410	520.567967	7.960064
6.170883	532.746148	7.965069
5.983211	520.232885	7.970074
6.183273	509.186233	7.975078
6.163951	517.903364	7.980083
5.799762	516.612607	7.985088
5.746814	512.221889	7.990093
6.023158	515.620943	7.995098
5.991210	509.368139	8.000102
6.095698	515.335934	8.005107
5.913451	513.407082	8.010112
6.048525	511.345151	8.015130
5.562372	506.487353	8.020147
6.312769	507.044202	8.025165
6.075302	515.741398	8.030182
5.995598	490.117396	8.035200
6.370997	495.892494	8.040218
5.898485	503.741690	8.045235
5.974984	492.570863	8.050253
5.916701	503.790111	8.055270
5.881830	508.461881	8.060288
5.887724	508.586652	8.065306
5.701548	513.637394	8.070323
6.007505	503.514258	8.075341
5.985545	502.929203	8.080358
6.102230	506.844082	8.085376
6.220523	509.275715	8.090394
6.062638	509.606158	8.095411
6.064489	511.405683	8.100429
5.788722	505.340313	8.105446
6.012421	512.091090	8.110464
6.019059	512.360001	8.115482
5.890329	513.973469	8.120499
5.843278	500.543867	8.125517
5.971043	506.425529	8.130534
5.958014	509.155778	8.135552
6.180578	495.374107	8.140570
5.883381	506.520556	8.145587
5.994137	501.616077	8.150605
6.149702	509.879198	8.155622
5.937925	508.262528	8.160640
5.969022	508.345839	8.165658
5.880019	510.480690	8.170675
5.946610	509.871949	8.175693
6.076058	498.263612	8.180710
5.808182	505.672279	8.185728
5.638363	499.607510	8.190746
5.545043	497.475988	8.195763
6.357426	500.749721	8.200781
6.016995	502.064870	8.205798
6.027969	514.518109	8.210816
5.904940	497.002941	8.215834
5.773118	509.340232	8.220851
5.790226	502.647246	8.225869
6.058881	505.812152	8.230886
5.982567	524.005486	8.235904
6.306549	527.261922	8.240922
5.894810	523.771477	8.245939
6.150026	530.450530	8.250957
6.099967	549.235012	8.255974
6.037781	535.849802	8.260992
6.257835	538.905544	8.266010
6.066427	541.073755	8.271027
6.463222	536.683404	8.276045
6.187194	535.143872	8.281062
5.869774	521.937735	8.286080
6.296620	533.999394	8.291098
6.173285	542.060048	8.296115
6.172605	540.384774	8.301133
6.075694	537.017758	8.306150
6.235453	537.973829	8.311168
6.395072	542.319037	8.316186
6.111501	532.183580	8.321203
6.385639	533.398550	8.326221
5.902504	523.012372	8.331238
5.942255	527.466737	8.336256
6.531614	541.561190	8.341274
6.463468	546.108476	8.346291
6.364833	532.637085	8.351309
6.311140	520.371727	8.356326
6.284495	516.394006	8.361344
6.160623	509.056629	8.366362
5.988858	519.927488	8.371379
6.124338	545.271570	8.376397
6.130724	538.929486	8.381414
5.876115	555.480791	8.386432
6.265121	548.585410	8.391450
6.388844	556.777259	8.396467
6.485007	546.646350	8.401485
6.245427	547.420330	8.406502
6.131531	556.437025	8.411520
6.481744	547.604724	8.416538
6.059616	550.001283	8.421555
6.604715	545.647040	8.426573
6.559589	541.381084	8.431590
6.327662	550.267112	8.436608
6.541714	538.892747	8.441626
6.372145	528.635028	8.446643
6.201335	524.389551	8.451661
5.884272	531.621848	8.456678
6.014947	540.722502	8.461696
5.794264	544.970155	8.466714
6.096622	553.334609	8.471731
6.430038	546.429423	8.476749
6.379005	549.523174	8.481766
6.029649	552.280570	8.486784
5.911736	549.266267	8.491802
6.386180	549.924516	8.496819
6.243494	552.974567	8.501837
6.309633	550.189739	8.506854
6.093512	568.821702	8.511872
6.572503	576.262365	8.516890
6.389501	581.270093	8.521907
6.551746	575.916515	8.526925
6.328228	569.835400	8.531942
6.403521	579.246747	8.536960
6.687213	573.934111	8.541978
6.486992	574.515994	8.546995
6.204342	571.566599	8.552013
6.624354	560.925754	8.557030
6.407035	580.737036	8.562048
6.313222	576.491318	8.567066
6.545167	568.205615	8.572083
6.134715	579.293584	8.577101
6.420342	582.174159	8.582119
6.608619	574.888198	8.587136
6.487307	577.340543	8.592154
6.763157	579.459197	8.597171
6.582290	580.914783	8.602189
6.749568	575.563030	8.607207
6.466849	568.585275	8.612224
6.318912	557.975602	8.617242
6.245492	560.976224	8.622259
6.424022	567.503529	8.627277
6.380550	571.538967	8.632295
6.250193	579.112802	8.637312
6.612050	575.843160	8.642330
6.421198	579.394685	8.647347
6.529734	570.544446	8.652365
6.450276	578.879016	8.657383
6.148145	588.917298	8.662400
6.478480	579.687257	8.667418
6.354868	587.849437	8.672435
6.215799	577.789264	8.677453
6.400930	582.261543	8.682471
6.386002	587.233232	8.687488
6.712076	604.169051	8.692506
6.853580	606.717609	8.697523
6.531829	602.931716	8.702541
6.565550	584.418090	8.707559
6.508799	590.453972	8.712576
6.991331	601.749342	8.717594
6.349747	594.295940	8.722611
6.386007	606.902427	8.727629
6.740622	601.255583	8.732647
6.826966	615.539803	8.737664
6.931538	601.251060	8.742682
7.054903	585.826367	8.747699
6.480820	579.092979	8.752717
6.800195	572.482369	8.757735
6.315288	592.752276	8.762752
6.437578	583.088590	8.767770
6.433646	589.519309	8.772787
6.610221	612.041887	8.777805
6.851812	600.904515	8.782823
6.646765	618.650916	8.787840
6.780256	618.081893	8.792858
6.786587	603.876693	8.797875
6.702463	613.877193	8.802893
6.691416	616.782888	8.807911
6.726135	612.651624	8.812928
6.426841	614.257270	8.817946
6.816874	614.708352	8.822963
6.690276	615.633318	8.827981
6.916772	613.061010	8.832999
6.795362	621.700905	8.838016
6.520106	621.216748	8.843034
6.676272	614.266132	8.848051
6.644730	619.298145	8.853069
6.714528	619.552488	8.858087
7.080049	619.633773	8.863104
6.821827	629.261259	8.868122
6.985821	619.985467	8.873139
6.660107	623.793103	8.878157
6.796278	622.026124	8.883175
6.462204	622.924659	8.888192
6.562828	614.301055	8.893210
6.913962	617.107339	8.898227
6.841216	617.179764	8.903245
6.877792	605.147308	8.908263
6.477387	606.098430	8.913280
6.568452	614.183424	8.918298
7.042750	611.569379	8.923315
6.379212	616.399785	8.928333
6.858146	623.609520	8.933351
6.786870	634.487570	8.938368
6.963773	642.209246	8.943386
7.319891	644.141546	8.948403
6.889065	635.236530	8.953421
7.338345	625.391345	8.958439
6.762012	635.415335	8.963456
6.782006	620.217100	8.968474
7.016556	616.567676	8.973491
6.516168	623.737218	8.978509
7.122333	632.716248	8.983527
7.226699	637.177583	8.988544
7.019263	615.630029	8.993562
7.012045	610.826787	8.998579
6.912611	622.725040	9.003597
7.104752	609.902742	9.008615
6.758757	617.102269	9.013632
6.853352	623.653014	9.018650
6.993802	620.169800	9.023667
6.824871	620.068786	9.028685
7.116308	644.983202	9.033703
6.916274	641.783078	9.038720
7.266227	639.705524	9.043738
7.310497	626.505755	9.048755
6.980819	614.386402	9.053773
7.053866	611.624433	9.058791
7.010761	619.872619	9.063808
6.932129	620.278632	9.068826
6.922573	602.488932	9.073843
6.573036	623.320651	9.078861
6.979557	622.631719	9.083879
7.156134	647.377064	9.088896
7.173538	640.236218	9.093914
7.381883	653.405141	9.098931
7.063628	642.096426	9.103949
7.172677	641.369857	9.108967
7.100693	645.371844	9.113984
7.282516	643.414674	9.119002
7.119800	631.355005	9.124019
6.539586	638.358939	9.129037
7.057038	635.844530	9.134055
6.969782	652.814657	9.139072
7.116244	649.759696	9.144090
7.124510	646.290349	9.149107
6.976744	651.631978	9.154125
7.433570	645.295025	9.159143
7.309886	647.525373	9.164160
6.982069	648.478575	9.169178
7.193239	644.333593	9.174195
7.279069	653.357587	9.179213
7.407732	646.754351	9.184231
6.940441	646.687585	9.189248
6.801439	651.465566	9.194266
7.044417	644.265594	9.199283
6.948233	661.413061	9.204301
6.902818	649.000294	9.209319
6.972048	652.658927	9.214336
6.757753	658.669305	9.219354
7.220746	656.021202	9.224371
7.313186	672.830480	9.229389
7.498570	673.107350	9.234407
7.152729	673.395445	9.239424
7.261447	676.349654	9.244442
7.558327	674.262661	9.249459
7.057396	661.906659	9.254477
7.287735	661.142923	9.259495
7.643619	667.881765	9.264512
7.287100	652.243448	9.269530
7.236033	641.400427	9.274547
7.018328	658.300009	9.279565
7.244548	663.776555	9.284583
7.391369	676.707187	9.289600
7.338140	680.584256	9.294618
7.737269	675.840198	9.299635
7.217451	663.809303	9.304653
7.179033	653.829281	9.309671
7.575261	669.055466	9.314688
7.556865	657.666582	9.319706
7.208010	646.627635	9.324723
7.122188	663.651268	9.329741
7.414099	674.178240	9.334759
7.576906	674.331010	9.339776
7.261078	679.371249	9.344794
7.765169	673.897870	9.349811
7.347832	666.486986	9.354829
7.338845	670.722915	9.359847
7.493199	661.112926	9.364864
7.219583	674.673168	9.369882
7.457190	679.107674	9.374899
7.569383	678.703852	9.379917
7.321577	679.222749	9.384935
7.608218	681.842298	9.389952
7.471082	680.295937	9.394970
7.634314	670.904120	9.399987
7.204338	661.028260	9.405005
7.374862	679.687193	9.410023
7.848580	667.148965	9.415040
7.499111	673.251163	9.420058
7.585209	651.351466	9.425075
7.221699	666.650254	9.430093
7.332399	662.786487	9.435111
7.628068	668.255987	9.440128
7.202687	685.748280	9.445146
7.569624	675.421584	9.450163
7.282977	681.069291	9.455181
7.439141	679.525338	9.460199
7.191714	674.066327	9.465216
7.188242	685.204319	9.470234
7.399186	674.091444	9.475251
7.105037	684.429988	9.480269
7.438381	689.398577	9.485287
7.397827	675.343945	9.490304
7.416337	692.274595	9.495322
7.678985	691.511817	9.500339
7.698279	700.896376	9.505357
7.684456	694.657943	9.510375
7.794781	700.263478	9.515392
7.700025	698.397570	9.520410
7.664172	680.398777	9.525427
7.580730	683.006564	9.530445
7.522923	694.775378	9.535463
7.736004	688.690263	9.540480
7.652281	715.246423	9.545498
7.969177	703.813611	9.550515
7.652412	699.463783	9.555533
7.348006	690.693918	9.560551
7.800070	677.586923	9.565568
7.322000	693.850068	9.570586
7.555853	695.709880	9.575603
7.379316	709.675490	9.580621
7.492126	701.661129	9.585639
7.921779	704.391474	9.590656
7.706404	701.546860	9.595674
7.685594	704.304015	9.600691
7.705021	709.037923	9.605709
7.786085	715.746230	9.610727
7.928500	696.571513	9.615744
7.905036	721.152727	9.620762
7.798634	714.680515	9.625779
7.767674	714.699194	9.630797
7.792333	708.644126	9.635815
7.756983	712.452216	9.640832
7.669833	719.089719	9.645850
7.666678	711.309143	9.650867
7.794585	706.486690	9.655885
7.576831	715.512472	9.660903
7.846115	714.549222	9.665920
7.760762	709.880591	9.670938
7.702941	715.629841	9.675955
7.990744	720.621809	9.680973
8.063850	713.640394	9.685991
7.995614	709.420034	9.691008
7.914596	712.488956	9.696026
8.186239	709.540930	9.701043
8.261638	708.304658	9.706061
8.073778	714.629628	9.711079
8.041953	704.196497	9.716096
7.729521	715.850150	9.721114
8.137044	710.152110	9.726131
7.998379	709.649610	9.731149
7.996779	700.465886	9.736167
8.097247	713.060570	9.741184
8.299928	718.602039	9.746202
7.980728	700.774828	9.751219
7.698039	685.164919	9.756237
7.791231	697.974238	9.761255
7.816907	699.596848	9.766272
8.038923	700.954968	9.771290
8.060437	702.844457	9.776307
8.023770	703.879939	9.781325
7.956640	718.965264	9.786343
8.224583	714.948848	9.791360
8.045508	718.772229	9.796378
8.075421	720.333226	9.801395
8.150495	702.104993	9.806413
7.976592	713.667949	9.811431
8.122894	704.181093	9.816448
8.065392	707.221231	9.821466
8.014366	711.574432	9.826483
7.856236	702.419428	9.831501
8.070444	708.931254	9.836519
7.946358	705.731064	9.841536
7.654414	721.628108	9.846554
8.164300	710.872818	9.851571
7.955646	722.003413	9.856589
7.881671	714.082697	9.861607
8.297435	710.520508	9.866624
8.012721	723.090384	9.871642
8.074962	714.134151	9.876659
8.365704	712.765558	9.881677
7.944218	719.585649	9.886695
8.193861	704.197932	9.891712
8.115768	711.415916	9.896730
8.426369	715.244875	9.901747
8.357453	702.836834	9.906765
8.023467	707.412451	9.911783
8.137584	693.603848	9.916800
8.106110	712.838033	9.921818
7.553254	698.729679	9.926835
8.027679	704.193270	9.931853
8.200901	714.633898	9.936871
8.162331	695.982702	9.941888
7.996506	701.029158	9.946906
8.149405	701.572766	9.951923
8.034097	715.271026	9.956941
8.359139	737.271311	9.961959
8.641675	737.212105	9.966976
8.111550	715.363371	9.971994
7.798722	716.173082	9.977011
8.195670	726.814205	9.982029
8.433690	733.169377	9.987047
8.537434	737.940336	9.992064
8.332775	737.611999	9.997082
8.393373	755.939942	10.002099
8.212298	733.229706	10.007117
8.254412	752.543694	10.012135
8.469035	739.990950	10.017152
8.341487	746.166424	10.022170
8.408145	757.855477	10.027187
8.544266	733.595648	10.032205
8.320812	742.037355	10.037223
8.679117	726.355133	10.042240
7.909094	718.953598	10.047258
8.025164	726.662539	10.052275
8.258970	731.455302	10.057293
8.610752	737.737159	10.062311
8.476914	732.463453	10.067328
8.521977	749.532961	10.072346
8.221162	749.942039	10.077363
8.728277	737.032159	10.082381
8.247751	745.886067	10.087399
8.355242	744.342770	10.092416
8.771252	745.495343	10.097434
8.496513	745.812824	10.102451
8.577601	746.444862	10.107469
8.544657	749.786309	10.112487
8.756021	739.947204	10.117504
8.697219	719.844365	10.122522
8.383930	712.132162	10.127539
8.292941	702.969606	10.132557
8.030734	716.724322	10.137575
8.237818	737.209041	10.142592
8.529797	739.372091	10.147610
8.611668	740.408159	10.152627
8.621926	750.770151	10.157645
8.377763	746.402507	10.162663
8.706486	740.893922	10.167680
8.479463	748.384128	10.172698
8.638390	742.974653	10.177715
8.467846	736.731299	10.182733
8.383170	748.520930	10.187751
8.757405	737.312730	10.192768
8.846317	751.204596	10.197786
8.495522	747.868762	10.202803
8.524290	738.767482	10.207821
8.458978	759.362784	10.212839
8.336397	745.298420	10.217856
8.835574	745.368247	10.222874
8.686537	742.143634	10.227891
8.721776	737.541172	10.232909
8.695062	734.622076	10.237927
8.705527	742.126960	10.242944
8.401795	745.365149	10.247962
8.573858	748.979848	10.252979
8.632214	737.962012	10.257997
8.318092	748.361370	10.263015
8.488357	744.844466	10.268032
8.892255	755.448935	10.273050
8.737491	744.371153	10.278067
8.944891	740.855888	10.283085
8.638348	745.810476	10.288103
8.742440	735.747313	10.293120
8.944943	732.341501	10.298138
8.615887	746.293478	10.303155
8.420484	742.430776	10.308173
8.839486	771.793796	10.313191
9.040008	780.606721	10.318208
8.978581	771.155824	10.323226
8.567458	758.456909	10.328243
8.873649	763.882980	10.333261
8.736541	780.410680	10.338279
8.790517	782.706062	10.343296
8.944215	776.954094	10.348314
8.713781	780.075570	10.353331
9.210099	781.619429	10.358349
9.185868	773.666057	10.363367
9.098459	765.753734	10.368384
9.003955	745.386140	10.373402
8.711389	749.824731	10.378419
9.008386	733.260470	10.383437
9.205679	749.828529	10.388455
8.785414	739.217089	10.393472
8.773170	742.030010	10.398490
8.582488	742.777123	10.403507
8.603903	744.816707	10.408525
8.971383	763.870678	10.413543
8.872580	770.996853	10.418560
9.000732	766.758489	10.423578
8.916024	777.960359	10.428595
9.134152	767.092052	10.433613
9.163928	769.178575	10.438631
8.948877	770.607844	10.443648
8.905692	763.399900	10.448666
8.641187	764.422553	10.453683
8.917016	764.353631	10.458701
8.734921	774.976913	10.463719
8.788368	768.853787	10.468736
8.981513	762.461166	10.473754
9.306995	782.844505	10.478771
9.267011	773.010208	10.483789
9.089957	779.492348	10.488807
8.922123	773.276382	10.493824
9.088392	774.226077	10.498842
9.058457	778.412652	10.503859
9.245971	757.981412	10.508877
8.996913	778.194874	10.513895
8.766566	777.687939	10.518912
9.103438	769.370028	10.523930
8.918270	771.933332	10.528947
9.203748	755.973894	10.533965
9.036273	772.102444	10.538983
8.816743	769.827497	10.544000
9.127620	773.875580	10.549018
8.895800	781.004650	10.554035
9.147492	788.580600	10.559053
9.097005	806.104565	10.564071
9.195162	811.393210	10.569088
9.625688	811.536380	10.574106
9.361163	800.824862	10.579123
9.022567	786.633390	10.584141
9.083407	795.058553	10.589159
9.253943	797.172696	10.594176
9.585504	806.438898	10.599194
9.326794	797.090358	10.604211
9.348195	781.666672	10.609229
9.116083	781.608375	10.614247
9.279955	781.740205	10.619264
9.603520	797.401483	10.624282
9.199803	787.147547	10.629299
8.916484	798.238084	10.634317
9.293690	786.026678	10.639335
9.150100	807.925207	10.644352
9.405720	803.193115	10.649370
9.213229	814.308706	10.654387
9.388961	799.649617	10.659405
9.374394	804.074070	10.664423
9.298562	810.409105	10.669440
9.809663	798.458092	10.674458
9.563399	815.072459	10.679475
9.456823	804.412678	10.684493
9.682419	805.753191	10.689511
9.189470	807.041904	10.694528
9.528084	804.032409	10.699546
9.223418	802.962855	10.704563
9.431226	797.559552	10.709581
9.591966	808.794983	10.714599
9.415447	798.888663	10.719616
9.723155	797.885403	10.724634
9.424481	808.715441	10.729651
9.545549	802.497382	10.734669
9.463999	798.741026	10.739687
9.497481	813.649315	10.744704
9.537416	811.469256	10.749722
9.516965	812.093179	10.754739
9.374213	805.066896	10.759757
9.676972	810.926743	10.764775
9.556447	803.281147	10.769792
10.004677	807.118679	10.774810
9.642239	787.723786	10.779827
9.473512	773.322889	10.784845
9.578107	772.036519	10.789863
9.057606	767.706563	10.794880
9.199677	783.386206	10.799898
9.538396	803.742095	10.804915
9.866053	790.314776	10.809933
9.574137	804.256338	10.814951
9.567175	799.701769	10.819968
9.805649	796.153113	10.824986
9.358029	804.735817	10.830003
9.464274	803.174220	10.835021
9.621503	809.557142	10.840039
9.909929	807.889173	10.845056
9.631767	793.362075	10.850074
9.737004	808.903467	10.855091
9.613358	814.252286	10.860109
9.804378	805.994869	10.865127
9.834862	812.095149	10.870144
9.832036	808.584004	10.875162
9.769560	811.530611	10.880179
9.527118	812.499531	10.885197
9.888021	814.185633	10.890215
9.735438	816.012092	10.895232
9.943071	811.510822	10.900250
10.007044	819.321808	10.905267
9.891970	806.278509	10.910285
9.947332	797.572632	10.915303
9.151822	801.439150	10.920320
9.689472	804.890710	10.925338
9.690024	803.255748	10.930355
9.700748	810.367975	10.935373
9.638601	799.782732	10.940391
9.615422	809.309392	10.945408
9.897428	807.194530	10.950426
9.784582	805.716866	10.955443
9.348693	804.789644	10.960461
9.860082	820.058946	10.965479
9.871639	837.352653	10.970496
10.027575	832.662020	10.975514
10.005113	834.743408	10.980531
10.135117	829.925686	10.985549
9.937120	824.905620	10.990567
9.812982	818.601719	10.995584
9.863950	819.733239	11.000602
9.718065	829.531130	11.005619
9.659795	834.052660	11.010637
9.918632	835.572493	11.015655
9.889489	824.571514	11.020672
10.116814	841.095444	11.025690
10.062283	830.732799	11.030707
9.897288	838.332561	11.035725
9.785227	824.221020	11.040743
9.779495	830.518105	11.045760
10.026073	824.545294	11.050778
9.969109	833.445575	11.055795
9.871527	845.396441	11.060813
10.275354	829.412253	11.065831
10.070930	840.167988	11.070848
10.202345	821.132901	11.075866
10.473465	836.150636	11.080883
10.048548	830.995754	11.085901
10.470902	828.264983	11.090919
10.102379	833.029580	11.095936
10.091700	829.655925	11.100954
10.221564	833.632281	11.105971
10.095338	831.763684	11.110989
10.573319	830.898201	11.116007
10.287546	823.768301	11.121024
10.164950	832.294160	11.126042
10.065320	829.547697	11.131059
10.077476	837.350427	11.136077
10.298252	828.511507	11.141095
9.963759	840.843980	11.146112
10.107882	835.613364	11.151130
10.355679	833.835590	11.156147
10.149783	842.054015	11.161165
10.720656	838.724980	11.166183
10.272522	847.128295	11.171200
10.280380	830.926616	11.176218
10.071850	825.334865	11.181235
10.042249	841.094601	11.186253
10.326892	832.124869	11.191271
10.180652	833.877952	11.196288
10.325178	835.350545	11.201306
10.430394	826.765426	11.206323
10.197061	844.130214	11.211341
10.445229	844.969547	11.216359
10.267852	836.361350	11.221376
10.093007	826.778892	11.226394
10.245177	834.471096	11.231411
10.027119	839.818698	11.236429
10.151136	839.304866	11.241447
10.653309	863.454229	11.246464
10.668855	849.909075	11.251482
10.663800	838.967873	11.256499
10.300471	838.405071	11.261517
10.779103	827.334546	11.266535
10.498756	825.970175	11.271552
10.661985	829.621682	11.276570
10.654766	823.548612	11.281587
10.075522	838.283226	11.286605
10.506000	827.376636	11.291623
10.480206	823.061647	11.296640
10.241983	826.220536	11.301658
10.633863	842.960835	11.306675
10.330815	841.660341	11.311693
10.572535	862.759968	11.316711
10.589595	865.358656	11.321728
10.503945	851.918791	11.326746
11.123201	860.477164	11.331763
10.582837	840.459848	11.336781
10.657425	836.955585	11.341799
10.778577	821.708944	11.346816
10.527531	826.811643	11.351834
10.682963	819.071035	11.356851
10.288558	830.943305	11.361869
10.630847	831.269629	11.366887
10.778111	847.985014	11.371904
10.679646	855.869606	11.376922
10.917050	850.766656	11.381939
10.845160	833.962412	11.386957
10.690237	832.022587	11.391975
10.714502	836.419769	11.396992
10.746531	832.232207	11.402010
10.812788	821.005364	11.407027
10.748338	839.975913	11.412045
10.999254	828.068858	11.417063
10.945457	830.263278	11.422080
10.692563	837.211341	11.427098
10.905738	824.314241	11.432115
10.748796	831.792217	11.437133
10.454397	829.467243	11.442151
10.632810	823.145129	11.447168
10.481406	836.537508	11.452186
10.902054	841.479320	11.457203
10.857887	854.195052	11.462221
11.166939	862.286272	11.467239
10.981370	844.473025	11.472256
10.735508	842.355838	11.477274
10.624601	841.436317	11.482291
10.637502	841.753207	11.487309
10.727491	856.239966	11.492327
11.144124	866.312675	11.497344
10.655185	874.234839	11.502362
10.817917	853.525234	11.507379
10.640371	872.512348	11.512397
10.594509	864.908999	11.517415
10.905062	863.095757	11.522432
10.775694	871.071669	11.527450
10.929003	865.912938	11.532467
10.571765	872.967615	11.537485
10.712352	865.786134	11.542503
10.661360	868.180357	11.547520
10.610310	898.317929	11.552538
11.421961	883.349476	11.557555
11.246955	904.526193	11.562573
11.285414	900.451212	11.567591
11.122219	877.348209	11.572608
10.873886	876.113658	11.577626
11.057743	878.710764	11.582643
10.778581	888.266294	11.587661
11.243350	899.156128	11.592679
11.415631	881.146422	11.597696
11.087495	888.928654	11.602714
11.405327	883.716552	11.607731
10.895026	873.141843	11.612749
11.050099	878.662109	11.617767
11.235866	895.531096	11.622784
11.048012	894.214121	11.627802
11.496254	887.548622	11.632819
11.378156	882.900602	11.637837
11.348283	877.454673	11.642855
11.313381	856.741115	11.647872
11.206413	861.614441	11.652890
11.029448	850.155670	11.657907
10.931380	870.471347	11.662925
11.114453	878.389530	11.667943
10.944945	893.142790	11.672960
11.206114	892.086595	11.677978
11.661846	886.790298	11.682995
11.298817	905.477647	11.688013
11.167266	892.921366	11.693031
11.295645	890.567849	11.698048
11.087947	901.197023	11.703066
11.250137	901.337104	11.708083
11.395660	902.253235	11.713101
11.316744	902.134194	11.718119
11.654849	900.537814	11.723136
11.221451	893.603903	11.728154
11.347870	893.266118	11.733171
11.406487	895.524339	11.738189
11.421826	906.452036	11.743207
11.639280	895.020951	11.748224
11.542087	909.560540	11.753242
11.619301	897.309856	11.758259
11.352378	905.486243	11.763277
11.270617	903.000353	11.768295
11.700614	888.695847	11.773312
11.463364	893.872554	11.778330
11.571567	890.617997	11.783347
11.437934	902.831317	11.788365
11.360024	894.194842	11.793383
11.666995	891.135549	11.798400
11.494962	898.905963	11.803418
11.559076	892.833969	11.808435
11.277718	886.643310	11.813453
11.143593	894.833763	11.818471
11.445038	891.881468	11.823488
11.333909	889.388821	11.828506
11.149371	888.451745	11.833523
11.326565	894.468276	11.838541
11.516253	912.390394	11.843559
11.859862	911.676027	11.848576
11.736049	931.579572	11.853594
11.891994	916.070536	11.858611
11.777188	908.022927	11.863629
11.056859	898.417790	11.868647
11.952739	910.644421	11.873664
11.934678	920.045030	11.878682
11.801609	913.601547	11.883699
11.804856	902.798079	11.888717
11.895327	900.977705	11.893735
11.781813	891.291780	11.898752
11.427280	908.232748	11.903770
11.935032	904.543719	11.908787
11.819152	892.719567	11.913805
11.570228	896.194751	11.918823
11.745197	911.940534	11.923840
11.355627	924.431166	11.928858
11.662210	930.224591	11.933875
12.000938	928.003800	11.938893
11.778362	924.934584	11.943911
11.954951	915.656927	11.948928
11.897184	928.952234	11.953946
12.336200	921.964283	11.958963
12.152768	928.568287	11.963981
12.067607	931.869394	11.968999
11.800574	902.700075	11.974016
11.693012	906.564628	11.979034
11.903889	912.411061	11.984051
11.842934	920.363096	11.989069
11.767235	912.826061	11.994087
12.109747	929.667807	11.999104
11.836560	928.578280	12.004122
12.056022	925.549580	12.009139
12.277152	926.351463	12.014157
12.081996	924.332658	12.019175
12.069422	920.015557	12.024192
11.967555	927.331550	12.029210
12.177372	921.750146	12.034227
12.168889	919.181880	12.039245
12.055649	923.383933	12.044263
12.135890	903.686348	12.049280
12.205000	925.331526	12.054298
12.270184	911.281938	12.059315
12.364983	894.640896	12.064333
12.201573	888.391775	12.069351
12.046250	879.425835	12.074368
11.901957	896.346415	12.079386
11.933685	907.239324	12.084403
11.831206	916.435217	12.089421
11.874195	918.213033	12.094439
12.074488	910.848661	12.099456
12.051164	918.687409	12.104474
12.415855	916.866986	12.109491
12.315628	911.842641	12.114509
12.164716	927.982984	12.119527
12.366259	924.129234	12.124544
12.079109	926.710695	12.129562
12.095908	923.982961	12.134579
12.206729	932.656886	12.139597
12.216297	937.070303	12.144615
12.148949	921.013022	12.149632
12.213007	922.974531	12.154650
11.993055	922.604432	12.159667
12.196633	923.297817	12.164685
12.004592	916.559994	12.169703
12.446794	922.866153	12.174720
12.451399	947.831510	12.179738
12.591850	930.685920	12.184755
12.382144	921.467766	12.189773
12.284062	921.775246	12.194791
12.299363	908.601476	12.199808
12.179799	917.935406	12.204826
12.337824	930.428843	12.209843
12.737120	937.529566	12.214861
12.127280	939.482971	12.219879
12.409076	934.833015	12.224896
12.800899	943.085571	12.229914
12.604277	951.552677	12.234931
12.819312	944.106930	12.239949
12.510623	950.711173	12.244967
12.396770	950.121408	12.249984
12.588133	952.791094	12.255002
12.553069	962.204576	12.260019
12.331302	951.868895	12.265037
12.215785	953.481799	12.270055
12.654412	942.634303	12.275072
12.220093	945.038743	12.280090
12.271825	964.403760	12.285107
12.345485	943.234226	12.290125
12.359310	958.999994	12.295143
12.592416	940.066933	12.300160
12.199506	949.031162	12.305178
12.587747	955.716859	12.310195
13.285884	960.482757	12.315213
12.743691	963.569877	12.320231
12.744906	956.797936	12.325248
12.735713	947.040021	12.330266
12.767046	939.138296	12.335283
12.782139	945.354638	12.340301
12.903742	948.182677	12.345319
13.206587	945.657038	12.350336
12.896504	948.332435	12.355354
12.748861	959.201881	12.360371
12.912701	936.816469	12.365389
12.454380	943.480076	12.370407
12.505674	942.211357	12.375424
12.793669	943.429286	12.380442
12.844637	946.786038	12.385459
12.754691	947.800916	12.390477
12.546781	954.616816	12.395495
12.895016	986.313310	12.400512
13.171786	974.975300	12.405530
13.255485	980.240315	12.410547
13.335100	954.497495	12.415565
12.891348	964.833689	12.420583
12.942515	943.412992	12.425600
12.890225	948.089742	12.430618
13.020350	957.397787	12.435635
12.832963	937.249979	12.440653
12.709964	964.502610	12.445671
12.938039	965.591293	12.450688
13.129542	970.277361	12.455706
13.169607	972.669739	12.460723
13.100554	974.453678	12.465741
12.997364	972.010681	12.470759
13.212808	963.310338	12.475776
13.100806	964.363501	12.480794
13.053348	958.541771	12.485811
13.183878	959.605634	12.490829
13.276444	974.005873	12.495847
13.223139	957.332160	12.500864
13.070799	945.753914	12.505882
13.080043	964.646111	12.510899
13.064161	943.087109	12.515917
12.979356	961.108179	12.520935
12.961390	969.411738	12.525952
13.067048	974.463707	12.530970
13.010323	967.741290	12.535987
13.526824	981.639857	12.541005
13.437355	980.023984	12.546023
13.339357	983.383908	12.551040
13.404349	980.435046	12.556058
13.143700	988.953888	12.561075
13.078326	982.302961	12.566093
12.872727	975.443554	12.571111
13.142907	979.494677	12.576128
13.080129	961.280652	12.581146
13.199806	983.875666	12.586163
13.032900	970.524703	12.591181
13.330896	981.067413	12.596199
13.240555	973.780365	12.601216
13.242644	975.537589	12.606234
13.053308	987.587966	12.611251
13.193907	990.244988	12.616269
13.419998	998.474576	12.621287
13.589772	1005.247570	12.626304
13.707464	1005.737076	12.631322
13.549838	1000.894798	12.636339
13.529837	997.976116	12.641357
13.709206	1000.066391	12.646375
13.914672	1000.126498	12.651392
13.914765	974.072626	12.656410
13.542362	968.809626	12.661427
13.829628	982.896445	12.666445
13.507798	965.540641	12.671463
13.764462	970.044906	12.676480
13.825749	965.079272	12.681498
13.530193	971.492409	12.686515
13.799115	964.417015	12.691533
13.821734	977.030882	12.696551
13.726638	973.132060	12.701568
13.944230	962.768641	12.706586
13.753744	975.289003	12.711603
13.944289	968.710339	12.716621
13.869191	973.930148	12.721639
14.010362	970.000550	12.726656
13.673788	961.312112	12.731674
13.612914	977.724392	12.736691
13.962830	979.540654	12.741709
13.698310	961.816190	12.746727
13.720847	960.886026	12.751744
14.037323	955.193888	12.756762
13.832799	964.505673	12.761779
13.980187	954.652007	12.766797
13.912079	947.691952	12.771815
13.569624	940.922095	12.776832
13.896522	942.962592	12.781850
13.659497	963.688691	12.786867
13.803515	959.895021	12.791885
13.633459	975.157225	12.796903
13.827074	966.471312	12.801920
14.069067	969.363108	12.806938
13.831857	975.747316	12.811955
13.767104	957.662931	12.816973
13.926724	960.748623	12.821991
13.751648	961.364251	12.827008
13.730677	951.648628	12.832026
13.874675	962.508655	12.837043
13.962573	956.960178	12.842061
14.050756	961.153164	12.847079
13.433004	959.191594	12.852096
13.917363	953.127479	12.857114
13.844048	968.679546	12.862131
14.071700	976.770108	12.867149
14.045437	976.980696	12.872167
14.087725	984.906060	12.877184
14.353729	989.566045	12.882202
13.854041	972.751943	12.887219
14.002810	992.595564	12.892237
14.237191	992.714663	12.897255
14.044418	997.891534	12.902272
14.496983	988.186400	12.907290
14.086451	998.411436	12.912307
14.180362	987.249281	12.917325
14.336239	986.787158	12.922343
14.290903	1007.631812	12.927360
14.484258	988.850315	12.932378
13.924853	983.358214	12.937395
13.967594	993.459335	12.942413
14.108541	998.452142	12.947431
14.235240	1004.687067	12.952448
14.262186	1000.572236	12.957466
14.135021	994.082475	12.962483
14.185003	1003.383519	12.967501
14.082051	994.857604	12.972519
13.950398	997.710577	12.977536
14.533779	1000.562300	12.982554
14.594004	1004.199969	12.987571
14.245120	1001.128976	12.992589
14.364601	994.776183	12.997607
14.463437	1006.034389	13.002624
14.291518	1005.682134	13.007642
14.267196	1001.361833	13.012659
14.345075	1006.860852	13.017677
14.155103	1011.289944	13.022695
14.479842	1016.286632	13.027712
14.879646	1023.897662	13.032730
14.508513	1035.461862	13.037747
14.646649	1037.402287	13.042765
14.636573	1012.134159	13.047783
14.458368	1014.628351	13.052800
14.661217	1008.483984	13.057818
14.635880	1016.191639	13.062835
14.619109	1017.915967	13.067853
14.632946	1018.086075	13.072871
14.442122	1019.355385	13.077888
14.943144	1018.567568	13.082906
14.850707	1015.089489	13.087923
14.592663	993.909552	13.092941
14.644983	983.773989	13.097959
14.752746	1002.805635	13.102976
14.810034	1001.993524	13.107994
14.661695	1005.648143	13.113011
14.418851	1004.672671	13.118029
14.915260	1011.826857	13.123047
14.980375	1016.320867	13.128064
15.063175	1014.364762	13.133082
14.487389	1012.710371	13.138099
14.561311	1014.668097	13.143117
14.709027	1031.340602	13.148135
14.513176	1027.828633	13.153152
14.780002	1028.382064	13.158170
14.971012	1028.731129	13.163187
14.808459	1026.265655	13.168205
14.654473	1029.258720	13.173223
14.575918	1023.503315	13.178240
14.920274	1021.666165	13.183258
14.591617	1028.955324	13.188275
14.592927	1027.443324	13.193293
15.076975	1018.676715	13.198311
14.732614	1030.049706	13.203328
15.301461	1017.098492	13.208346
15.210929	1028.217365	13.213363
15.004599	1025.322187	13.218381
14.925815	1023.092831	13.223399
14.883136	1030.055644	13.228416
15.090406	1027.067515	13.233434
15.251043	1030.839755	13.238451
14.977564	1035.587723	13.243469
15.105340	1035.423306	13.248487
14.950953	1031.394329	13.253504
15.094230	1045.255630	13.258522
15.432484	1050.440420	13.263539
15.242484	1035.199816	13.268557
15.416267	1031.450611	13.273575
15.073368	1022.169380	13.278592
15.520571	1023.136043	13.283610
15.538796	1022.381559	13.288627
15.689536	1025.254002	13.293645
15.349582	1022.953256	13.298663
15.148377	1025.008408	13.303680
15.356275	1016.302000	13.308698
15.367652	1010.662228	13.313715
15.298535	1017.310952	13.318733
15.342074	1016.347790	13.323751
15.335345	1025.744623	13.328768
15.362036	1022.970165	13.333786
15.105023	1024.068946	13.338803
15.391058	1011.733868	13.343821
15.669443	1024.975873	13.348839
15.252733	1031.205741	13.353856
15.220727	1021.680055	13.358874
15.324705	1022.922299	13.363891
15.268043	1021.507070	13.368909
15.405802	1016.072556	13.373927
15.555680	1023.430052	13.378944
15.525504	1034.972942	13.383962
15.469264	1026.242668	13.388979
15.458487	1049.720814	13.393997
15.810603	1043.758230	13.399015
15.605095	1030.715120	13.404032
15.322454	1017.236611	13.409050
15.582773	1040.367827	13.414067
15.654022	1041.291713	13.419085
15.762080	1050.022254	13.424103
15.541879	1055.427461	13.429120
15.730935	1045.068899	13.434138
15.597628	1042.159880	13.439155
15.434076	1054.241672	13.444173
15.866533	1047.986917	13.449191
15.485773	1045.841706	13.454208
15.682108	1043.846169	13.459226
15.962817	1045.302084	13.464243
15.767818	1041.769305	13.469261
16.093327	1042.423848	13.474279
16.001684	1044.417598	13.479296
15.843723	1044.529890	13.484314
16.215157	1036.321165	13.489331
15.943236	1024.083004	13.494349
15.917720	1011.081416	13.499367
15.741384	1016.782855	13.504384
15.596159	1007.771477	13.509402
15.865107	1013.378468	13.514419
15.509587	1022.581797	13.519437
16.049287	1036.948356	13.524455
15.733280	1058.128509	13.529472
15.562446	1051.677824	13.534490
15.841264	1051.550445	13.539507
15.360688	1049.004078	13.544525
15.595629	1047.961654	13.549543
15.523527	1044.507369	13.554560
15.989317	1055.143446	13.559578
16.054786	1066.731372	13.564595
16.274011	1083.780835	13.569613
16.414512	1053.528491	13.574631
16.103383	1048.560997	13.579648
16.080056	1051.952290	13.584666
15.940324	1034.618473	13.589683
16.118018	1040.839868	13.594701
15.978641	1041.086863	13.599719
16.168715	1065.426581	13.604736
16.174695	1065.422820	13.609754
16.507865	1073.863064	13.614771
16.186306	1061.173503	13.619789
16.277196	1045.371788	13.624807
15.936643	1057.965434	13.629824
16.203888	1061.385471	13.634842
16.442256	1061.191362	13.639859
16.168676	1070.858466	13.644877
16.480623	1069.492341	13.649895
16.387493	1076.282438	13.654912
16.329838	1077.641933	13.659930
16.632543	1069.297918	13.664947
16.147184	1067.002102	13.669965
16.563881	1068.098395	13.674983
16.228313	1071.867421	13.680000
16.410849	1073.932186	13.685018
16.755080	1072.290099	13.690035
16.534323	1071.540464	13.695053
16.296938	1060.381633	13.700071
16.578325	1056.998241	13.705088
16.345550	1058.882067	13.710106
16.928892	1064.032659	13.715123
16.490752	1045.188152	13.720141
16.986796	1023.657612	13.725159
16.634268	1029.279724	13.730176
16.286687	1028.995467	13.735194
16.691775	1025.111598	13.740211
16.669211	1041.651649	13.745229
16.203221	1034.487073	13.750247
16.710031	1041.150459	13.755264
16.735162	1056.951855	13.760282
16.909272	1057.160626	13.765299
16.471686	1047.649200	13.770317
16.601766	1039.863761	13.775335
16.606831	1051.100297	13.780352
16.620616	1051.986444	13.785370
16.674882	1054.163924	13.790387
16.815257	1072.742110	13.795405
16.797846	1070.030829	13.800423
16.660859	1067.291481	13.805440
16.808626	1066.723232	13.810458
16.879006	1063.876006	13.815475
16.844583	1072.635419	13.820493
16.578161	1074.952891	13.825511
17.091476	1064.450392	13.830528
16.727922	1064.842486	13.835546
16.586321	1072.273169	13.840563
16.760556	1069.749474	13.845581
17.016473	1064.266880	13.850599
17.164854	1047.508568	13.855616
16.874867	1074.720890	13.860634
16.928478	1050.551842	13.865651
16.958224	1066.673498	13.870669
16.990413	1067.013973	13.875687
17.030175	1061.283679	13.880704
16.952254	1071.414632	13.885722
17.316851	1070.072085	13.890739
17.077218	1075.351199	13.895757
17.000397	1067.285223	13.900775
17.116676	1065.468044	13.905792
16.900081	1060.320383	13.910810
17.280266	1059.519467	13.915827
16.824891	1068.694646	13.920845
16.959432	1063.367718	13.925863
16.745858	1060.000970	13.930880
17.135484	1077.320252	13.935898
17.442385	1085.828024	13.940915
17.276294	1097.620944	13.945933
17.336355	1090.064734	13.950951
17.389240	1082.889575	13.955968
17.310146	1070.955286	13.960986
17.174440	1066.911600	13.966003
16.916461	1084.093064	13.971021
17.304949	1085.970474	13.976039
17.308881	1093.519811	13.981056
17.163039	1098.156957	13.986074
17.322637	1095.875404	13.991091
17.434855	1102.437907	13.996109
17.803057	1103.899643	14.001127
17.548699	1091.750834	14.006144
17.600808	1097.514142	14.011162
17.524587	1096.485937	14.016179
17.661941	1095.165588	14.021197
17.456634	1087.536124	14.026215
17.453464	1087.725773	14.031232
17.080973	1093.073692	14.036250
17.288226	1085.664787	14.041267
17.576547	1094.348441	14.046285
17.365444	1085.647267	14.051303
17.837310	1070.555087	14.056320
17.568296	1092.374665	14.061338
17.760273	1076.003347	14.066355
17.674301	1082.437004	14.071373
17.756772	1088.612157	14.076391
17.885630	1082.360911	14.081408
17.762934	1093.572929	14.086426
17.847665	1087.739343	14.091443
17.906804	1085.712937	14.096461
17.470162	1076.039158	14.101479
17.790143	1082.531893	14.106496
17.751859	1093.962011	14.111514
17.958502	1081.756515	14.116531
17.851669	1092.775192	14.121549
17.650781	1088.942437	14.126567
17.902997	1082.075428	14.131584
17.748978	1083.206594	14.136602
17.773741	1081.763733	14.141619
17.887922	1079.948474	14.146637
17.549562	1084.128529	14.151655
17.880091	1085.130025	14.156672
17.923080	1084.048071	14.161690
18.304230	1093.233037	14.166707
18.249088	1084.743652	14.171725
17.771266	1071.975196	14.176743
17.898292	1081.533986	14.181760
17.702371	1082.573274	14.186778
18.299647	1098.725568	14.191795
18.449306	1110.233286	14.196813
18.245647	1095.020073	14.201831
18.363696	1076.536302	14.206848
17.973546	1086.702328	14.211866
18.362097	1077.360811	14.216883
18.641946	1073.134494	14.221901
18.137056	1088.659984	14.226919
18.333837	1075.820394	14.231936
17.947391	1086.731163	14.236954
18.138211	1076.565369	14.241971
18.038740	1084.060738	14.246989
18.028864	1088.370145	14.252007
18.354972	1082.720654	14.257024
18.115511	1091.551159	14.262042
18.287601	1092.914810	14.267059
18.128838	1102.505685	14.272077
18.140431	1125.150259	14.277095
18.571238	1113.459775	14.282112
18.533950	1124.333735	14.287130
18.392948	1114.959841	14.292147
18.493506	1109.942993	14.297165
18.453591	1106.676652	14.302183
18.739151	1108.738765	14.307200
18.634052	1106.322633	14.312218
18.634652	1116.694143	14.317235
18.486152	1120.271465	14.322253
18.205748	1127.556240	14.327271
18.669584	1118.911007	14.332288
18.327756	1119.441813	14.337306
18.230188	1120.237916	14.342323
18.680227	1117.874708	14.347341
18.572196	1120.217579	14.352359
18.839411	1119.874237	14.357376
18.613653	1123.520223	14.362394
18.773116	1113.815619	14.367411
18.822163	1122.629366	14.372429
18.727931	1126.000705	14.377447
18.996074	1115.668981	14.382464
18.853011	1121.814694	14.387482
18.718029	1106.817644	14.392499
18.924434	1113.413006	14.397517
18.865081	1116.072781	14.402535
18.837699	1113.209030	14.407552
18.734882	1113.374602	14.412570
18.706899	1107.923948	14.417587
18.685088	1122.052720	14.422605
18.395645	1120.778492	14.427623
18.725667	1104.432160	14.432640
18.682882	1115.050369	14.437658
18.564393	1114.801666	14.442675
18.877893	1120.943573	14.447693
18.718866	1126.800436	14.452711
19.055626	1130.763247	14.457728
19.200165	1128.730793	14.462746
19.241410	1139.193619	14.467763
19.305199	1131.075244	14.472781
19.033540	1131.783796	14.477799
18.938735	1116.948968	14.482816
18.926710	1129.283296	14.487834
18.824465	1134.940846	14.492851
19.215874	1130.809644	14.497869
19.066363	1129.876999	14.502887
18.949295	1128.110577	14.507904
18.716386	1127.966989	14.512922
18.630335	1129.433134	14.517939
19.117662	1129.703712	14.522957
19.306103	1140.628951	14.527975
19.402626	1129.646352	14.532992
19.190599	1133.467997	14.538010
19.455367	1130.793723	14.543027
19.530714	1128.052931	14.548045
19.684530	1131.039436	14.553063
19.649062	1133.115435	14.558080
19.714790	1129.371465	14.563098
19.330482	1133.542594	14.568115
19.527640	1121.087491	14.573133
19.219180	1116.516519	14.578151
19.271976	1119.015068	14.583168
19.699882	1118.718783	14.588186
19.980477	1117.178729	14.593203
19.920919	1114.109697	14.598221
19.767297	1124.490952	14.603239
19.724124	1116.623099	14.608256
19.895283	1121.308442	14.613274
19.802915	1127.258013	14.618291
19.744473	1113.914981	14.623309
19.556565	1126.015616	14.628327
19.699967	1125.069995	14.633344
19.791485	1112.770523	14.638362
19.783626	1120.063792	14.643379
19.890362	1123.172624	14.648397
19.430139	1120.608513	14.653415
19.770700	1108.640667	14.658432
19.471778	1121.408755	14.663450
20.068129	1114.494901	14.668467
19.780005	1120.121755	14.673485
19.539340	1127.594618	14.678503
19.912627	1117.227017	14.683520
19.747815	1119.130717	14.688538
19.502439	1126.747644	14.693555
19.542200	1119.748231	14.698573
19.709910	1115.988594	14.703591
19.383902	1119.250813	14.708608
19.720908	1129.517733	14.713626
19.795775	1144.354454	14.718643
20.003333	1149.523087	14.723661
19.644297	1167.856407	14.728679
20.048206	1154.644188	14.733696
20.489955	1150.859529	14.738714
20.259317	1146.000534	14.743731
20.320014	1154.967273	14.748749
19.972568	1154.148032	14.753767
20.323218	1139.613333	14.758784
20.541898	1137.150383	14.763802
20.300105	1137.112184	14.768819
20.167006	1125.935481	14.773837
19.939718	1127.126389	14.778855
20.222317	1136.541020	14.783872
20.482517	1140.790459	14.788890
20.414695	1137.525180	14.793907
20.286167	1129.276406	14.798925
20.094669	1128.695529	14.803943
20.305059	1133.388761	14.808960
20.100486	1144.034709	14.813978
19.861179	1148.178731	14.818995
20.259319	1140.528445	14.824013
20.420759	1145.316764	14.829031
20.496770	1139.345447	14.834048
20.499963	1150.875234	14.839066
20.222037	1151.539751	14.844083
20.596685	1127.667477	14.849101
20.454058	1144.277471	14.854119
20.235353	1141.366209	14.859136
20.676765	1139.048314	14.864154
20.371859	1132.586291	14.869171
20.619348	1143.697217	14.874189
20.330133	1141.755532	14.879207
20.336855	1139.992073	14.884224
20.396636	1146.530195	14.889242
20.363412	1153.472410	14.894259
20.603152	1162.653230	14.899277
20.629745	1170.201813	14.904295
20.711732	1161.851905	14.909312
21.136596	1168.713507	14.914330
20.764378	1164.097554	14.919347
20.738925	1162.761197	14.924365
20.945086	1161.464703	14.929383
21.076404	1163.570420	14.934400
21.235235	1163.730151	14.939418
20.940427	1145.145650	14.944435
20.693949	1135.991898	14.949453
20.814623	1133.878755	14.954471
20.796699	1148.156689	14.959488
20.789262	1155.129480	14.964506
20.875474	1167.082699	14.969523
21.349696	1156.700360	14.974541
21.283111	1159.825441	14.979559
20.999907	1150.046546	14.984576
21.166228	1136.630728	14.989594
20.517844	1142.892823	14.994611
21.178705	1139.019014	14.999629
21.650415	1144.842903	15.004647
21.310604	1147.393738	15.009664
21.636447	1126.259825	15.014682
20.827778	1141.393510	15.019699
21.048921	1129.159402	15.024717
21.268965	1132.897247	15.029735
21.173749	1125.358216	15.034752
21.085395	1135.716491	15.039770
21.413027	1155.742348	15.044787
21.687413	1148.992296	15.049805
21.479072	1140.230408	15.054823
21.198950	1138.497424	15.059840
21.245900	1124.420934	15.064858
21.027334	1131.789376	15.069875
21.234698	1137.888799	15.074893
21.479553	1159.032699	15.079911
21.458145	1170.007005	15.084928
21.579361	1158.171810	15.089946
21.451102	1167.953521	15.094963
21.538665	1168.641487	15.099981
21.611680	1162.441754	15.104999
21.305275	1161.426979	15.110016
21.232011	1161.639235	15.115034
21.469633	1163.857680	15.120051
21.361518	1162.510577	15.125069
21.626368	1161.307716	15.130087
21.522585	1160.072675	15.135104
21.571265	1152.277800	15.140122
21.583325	1165.632234	15.145139
21.307567	1154.107487	15.150157
21.639721	1157.746510	15.155175
21.651668	1170.318211	15.160192
21.778638	1157.714071	15.165210
21.527179	1164.370355	15.170227
21.983932	1184.591219	15.175245
22.017170	1194.152981	15.180263
21.674728	1183.204503	15.185280
22.055378	1190.616646	15.190298
21.575756	1189.141788	15.195315
21.917708	1196.372562	15.200333
21.997439	1196.211752	15.205351
21.969529	1195.737088	15.210368
22.218639	1193.903061	15.215386
22.155653	1190.304344	15.220403
21.953116	1182.602141	15.225421
22.174685	1186.891830	15.230439
21.834563	1188.005930	15.235456
21.924527	1197.454596	15.240474
22.077161	1195.240508	15.245491
22.210662	1195.311525	15.250509
22.428430	1191.692197	15.255527
22.108087	1200.031481	15.260544
22.365996	1188.045544	15.265562
21.888061	1199.590907	15.270579
22.461329	1188.242715	15.275597
22.461845	1189.205854	15.280615
22.192975	1189.178624	15.285632
22.503499	1175.997565	15.290650
22.178070	1192.362073	15.295667
22.498915	1195.334373	15.300685
22.521740	1186.656680	15.305703
21.941323	1193.885567	15.310720
22.568910	1181.940105	15.315738
22.475629	1188.952881	15.320755
22.501945	1184.842238	15.325773
22.438247	1195.990652	15.330791
22.371247	1190.206506	15.335808
22.659866	1178.424329	15.340826
22.256805	1189.698296	15.345843
22.388607	1191.709462	15.350861
22.405752	1180.510056	15.355879
22.373413	1194.693580	15.360896
22.687180	1195.993282	15.365914
22.395889	1191.468460	15.370931
22.305669	1190.983228	15.375949
22.259552	1183.760022	15.380967
22.327260	1185.284019	15.385984
22.321143	1201.700479	15.391002
22.680767	1211.725957	15.396019
22.547725	1206.498701	15.401037
22.979214	1202.376209	15.406055
22.865929	1216.490857	15.411072
22.990130	1207.446846	15.416090
22.777838	1208.164879	15.421107
23.254593	1220.976497	15.426125
23.137313	1206.809569	15.431143
22.935776	1205.220852	15.436160
23.208966	1212.365767	15.441178
23.080995	1207.403775	15.446195
23.014452	1205.378047	15.451213
23.483084	1198.387835	15.456231
22.824744	1195.559250	15.461248
22.999920	1203.064597	15.466266
23.216064	1193.639116	15.471283
23.092508	1191.525582	15.476301
23.419085	1205.208728	15.481319
23.031213	1196.644954	15.486336
23.253636	1198.370910	15.491354
23.274098	1201.539284	15.496371
23.205737	1210.216602	15.501389
23.206421	1199.161811	15.506407
23.036200	1205.440963	15.511424
23.214313	1200.230981	15.516442
23.347408	1206.958559	15.521459
22.884848	1193.932201	15.526477
23.379775	1208.776133	15.531495
23.285555	1200.679896	15.536512
23.336448	1198.115745	15.541530
23.261137	1203.335273	15.546547
23.076399	1194.731240	15.551565
23.248696	1177.987335	15.556583
23.388848	1201.045948	15.561600
23.530577	1192.784365	15.566618
23.497019	1190.058214	15.571635
23.305944	1199.957003	15.576653
23.222413	1189.972868	15.581671
23.412547	1216.461315	15.586688
23.530375	1227.563615	15.591706
23.557052	1232.125054	15.596723
23.713225	1221.373245	15.601741
23.946841	1223.627198	15.606759
23.696237	1233.115238	15.611776
23.955431	1210.922301	15.616794
23.938159	1234.702546	15.621811
24.025034	1223.083378	15.626829
24.134490	1211.265044	15.631847
23.831406	1207.121047	15.636864
23.743739	1191.956866	15.641882
23.764620	1203.710507	15.646899
23.689657	1199.498701	15.651917
24.045481	1212.742243	15.656935
23.910746	1210.398305	15.661952
24.088396	1225.601134	15.666970
24.354118	1222.128576	15.671987
23.745397	1219.142005	15.677005
24.250533	1215.342133	15.682023
24.097134	1225.379376	15.687040
24.011386	1224.793419	15.692058
24.178095	1216.835327	15.697075
24.389034	1227.062328	15.702093
23.979592	1220.656709	15.707111
24.095926	1225.759549	15.712128
24.155636	1227.640134	15.717146
24.193567	1218.011051	15.722163
24.010087	1226.574744	15.727181
23.992147	1221.801424	15.732199
23.647240	1226.344751	15.737216
23.927198	1224.191693	15.742234
24.305901	1218.348646	15.747251
24.222048	1218.705938	15.752269
24.324756	1216.158809	15.757287
24.413551	1228.016190	15.762304
24.316920	1239.150198	15.767322
24.722898	1249.844123	15.772339
24.764064	1243.578371	15.777357
24.779134	1219.946254	15.782375
24.629525	1229.646112	15.787392
24.557326	1222.836389	15.792410
24.630289	1222.121662	15.797427
24.455389	1232.945418	15.802445
24.531780	1212.413551	15.807463
24.452835	1219.958342	15.812480
24.818325	1244.627376	15.817498
24.908003	1241.476579	15.822515
24.637270	1237.589590	15.827533
24.746214	1222.733784	15.832551
24.664780	1246.131203	15.837568
24.952659	1247.238366	15.842586
25.019790	1242.644852	15.847603
24.723118	1242.133901	15.852621
24.868342	1234.938295	15.857639
24.793633	1230.659322	15.862656
24.983537	1240.650670	15.867674
25.071372	1236.159626	15.872691
25.159607	1244.098197	15.877709
25.145116	1228.376495	15.882727
24.717027	1221.609641	15.887744
24.917340	1229.498979	15.892762
24.952563	1238.597911	15.897779
24.782477	1238.628755	15.902797
25.046972	1236.064729	15.907815
25.171079	1244.650820	15.912832
24.994069	1248.177773	15.917850
25.167375	1239.445463	15.922867
25.065976	1250.172453	15.927885
25.228216	1248.669068	15.932903
25.416416	1238.670898	15.937920
25.340251	1247.089328	15.942938
25.594132	1242.486407	15.947955
24.950816	1249.625728	15.952973
25.157168	1238.510154	15.957991
25.011307	1249.841254	15.963008
25.042399	1249.302908	15.968026
25.432301	1236.668441	15.973043
25.008782	1244.276483	15.978061
25.160898	1266.377648	15.983079
25.392757	1263.032116	15.988096
25.540527	1261.835014	15.993114
25.820424	1263.275930	15.998131
25.699702	1271.489562	16.003149
25.597999	1265.191513	16.008167
25.781631	1269.743757	16.013184
25.937183	1265.022451	16.018202
25.784450	1259.424469	16.023219
25.925787	1268.609805	16.028237
25.820181	1246.925657	16.033255
25.649761	1257.634928	16.038272
25.983503	1261.106414	16.043290
25.832017	1250.756949	16.048307
25.920160	1249.933821	16.053325
26.104670	1246.480780	16.058343
26.005713	1229.345486	16.063360
25.662690	1232.935100	16.068378
25.994078	1233.296007	16.073395
25.800456	1231.155469	16.078413
25.907144	1235.932198	16.083431
25.933776	1257.093991	16.088448
25.767491	1259.630143	16.093466
26.261382	1261.750554	16.098483
26.180984	1263.548603	16.103501
26.419919	1257.431437	16.108519
26.060225	1248.446108	16.113536
26.094234	1251.753375	16.118554
26.101157	1251.910064	16.123571
26.143336	1266.048274	16.128589
26.214090	1237.525939	16.133607
26.467016	1255.036492	16.138624
26.523463	1247.236742	16.143642
26.485622	1251.316795	16.148659
26.460844	1254.996520	16.153677
26.730857	1253.930377	16.158695
26.769574	1226.897393	16.163712
26.643987	1224.995576	16.168730
26.491980	1212.255826	16.173747
25.946611	1224.857669	16.178765
26.063464	1211.690476	16.183783
26.555234	1234.829008	16.188800
26.412068	1252.249719	16.193818
26.577473	1258.669072	16.198835
26.407862	1247.486701	16.203853
26.489080	1239.034728	16.208871
26.853869	1248.241779	16.213888
26.591366	1258.268337	16.218906
26.512122	1250.685666	16.223923
26.702255	1249.206211	16.228941
26.401744	1252.281791	16.233959
26.749128	1256.385969	16.238976
26.553660	1256.403490	16.243994
26.718823	1258.421356	16.249011
26.426927	1260.843837	16.254029
26.749959	1253.521215	16.259047
26.634189	1252.004331	16.264064
26.593138	1277.478680	16.269082
27.062294	1279.566572	16.274099
27.139846	1273.808107	16.279117
27.188574	1279.612785	16.284135
27.376336	1277.911113	16.289152
27.246274	1271.024329	16.294170
27.171735	1244.550109	16.299187
26.919510	1252.355997	16.304205
27.035324	1250.300326	16.309223
27.281933	1242.413454	16.314240
27.099695	1259.899480	16.319258
26.935475	1259.942149	16.324275
27.031831	1273.062306	16.329293
26.936278	1284.150899	16.334311
27.078054	1272.326981	16.339328
27.011129	1268.651152	16.344346
27.174686	1275.328653	16.349363
26.865210	1277.045088	16.354381
27.270667	1283.449779	16.359399
27.603016	1278.863600	16.364416
27.357533	1286.943746	16.369434
27.449267	1285.767317	16.374451
27.708452	1296.657753	16.379469
27.876261	1290.217139	16.384487
27.619786	1279.026661	16.389504
27.772766	1267.077291	16.394522
27.722288	1265.822608	16.399539
27.672541	1262.189407	16.404557
27.409938	1267.595987	16.409575
27.754726	1256.562233	16.414592
27.599458	1264.022034	16.419610
27.912569	1259.971640	16.424627
27.896202	1258.537724	16.429645
27.527486	1259.719340	16.434663
27.818701	1273.266089	16.439680
27.842473	1284.773681	16.444698
27.889696	1277.280712	16.449715
28.294071	1289.461724	16.454733
28.347731	1281.754137	16.459751
28.255059	1259.545270	16.464768
27.894814	1264.424165	16.469786
28.160739	1267.011713	16.474803
27.726892	1257.511740	16.479821
27.763203	1265.598450	16.484839
28.148973	1270.360957	16.489856
28.245354	1282.492087	16.494874
28.295118	1285.773729	16.499891
28.085394	1284.180255	16.504909
28.093306	1288.880029	16.509927
28.573005	1292.803517	16.514944
28.205774	1295.548250	16.519962
28.205159	1287.096980	16.524979
28.384942	1283.497882	16.529997
28.338269	1290.148329	16.535015
28.495991	1292.316423	16.540032
28.607240	1283.826790	16.545050
28.589972	1278.671113	16.550067
28.635727	1264.500611	16.555085
28.214925	1249.221960	16.560103
28.630704	1260.975930	16.565120
28.676874	1270.975304	16.570138
28.529523	1273.433932	16.575155
28.809996	1266.379914	16.580173
28.209790	1260.956255	16.585191
28.602060	1268.589516	16.590208
28.554961	1274.615904	16.595226
28.641344	1277.732658	16.600243
28.861374	1289.136572	16.605261
28.476270	1279.856254	16.610279
29.040853	1270.575873	16.615296
28.723333	1283.202898	16.620314
28.875313	1276.903271	16.625331
28.925296	1273.812759	16.630349
28.445125	1279.815255	16.635367
29.057705	1269.026371	16.640384
28.746632	1277.289963	16.645402
28.600424	1273.564054	16.650419
28.647827	1279.787986	16.655437
28.715205	1274.503378	16.660455
29.322561	1279.260369	16.665472
29.064107	1290.457961	16.670490
29.233269	1300.408884	16.675507
29.200821	1291.546986	16.680525
29.105246	1285.499848	16.685543
29.466026	1287.119106	16.690560
28.986831	1294.501170	16.695578
29.172013	1289.081359	16.700595
29.797440	1293.167156	16.705613
28.891492	1297.943746	16.710631
29.163850	1295.873419	16.715648
29.252260	1307.682901	16.720666
29.203585	1306.240935	16.725683
29.127466	1304.413402	16.730701
29.381410	1318.163369	16.735719
29.477990	1310.281966	16.740736
29.270260	1310.751647	16.745754
29.384772	1312.580083	16.750771
29.634662	1303.541619	16.755789
29.461515	1319.014291	16.760807
29.588951	1302.214681	16.765824
29.701265	1315.956165	16.770842
29.625161	1323.961890	16.775859
29.720580	1338.505286	16.780877
29.851531	1338.634985	16.785895
30.219940	1327.744107	16.790912
30.130992	1308.793349	16.795930
29.925173	1304.776932	16.800947
29.882558	1294.151412	16.805965
29.669221	1294.215187	16.810983
29.773919	1287.385847	16.816000
29.695635	1304.735669	16.821018
29.986380	1317.093333	16.826035
30.698293	1309.048642	16.831053
30.335213	1304.544112	16.836071
30.358617	1299.440359	16.841088
30.173218	1295.323734	16.846106
30.123905	1292.303556	16.851123
30.280570	1283.358451	16.856141
29.566677	1287.402417	16.861159
29.788857	1289.193769	16.866176
30.203882	1307.818181	16.871194
30.054119	1321.877350	16.876211
30.485335	1316.288937	16.881229
30.035482	1321.812096	16.886247
30.498767	1330.265623	16.891264
30.386164	1331.576748	16.896282
30.260535	1326.871578	16.901299
30.677512	1319.650904	16.906317
30.141413	1326.770575	16.911335
30.406020	1327.227155	16.916352
30.372266	1327.656868	16.921370
30.616117	1317.915358	16.926387
30.638444	1317.306618	16.931405
30.508672	1333.821006	16.936423
30.947788	1332.479311	16.941440
30.692111	1321.025912	16.946458
30.482781	1327.732974	16.951475
30.524001	1311.850229	16.956493
30.534535	1332.289298	16.961511
30.717426	1338.926826	16.966528
31.064312	1339.984488	16.971546
30.886315	1348.494790	16.976563
31.297445	1336.146458	16.981581
31.144551	1338.415290	16.986599
31.011610	1320.944022	16.991616
30.705187	1315.479866	16.996634
30.611098	1334.521465	17.001651
31.057888	1333.316081	17.006669
31.077184	1338.889064	17.011687
30.920125	1344.288661	17.016704
31.178455	1325.327339	17.021722
31.172477	1343.441918	17.026739
31.404847	1329.478478	17.031757
31.282176	1343.817598	17.036775
31.285553	1345.214269	17.041792
31.567546	1339.997703	17.046810
31.051482	1344.098546	17.051827
31.352826	1338.810879	17.056845
31.278469	1343.850204	17.061863
31.487635	1337.067547	17.066880
31.472186	1338.375215	17.071898
31.714103	1332.201825	17.076915
31.497090	1337.514097	17.081933
31.603681	1333.859178	17.086951
31.619187	1334.046532	17.091968
31.701012	1327.221938	17.096986
31.625256	1335.653536	17.102003
31.907124	1329.037584	17.107021
31.585682	1347.599322	17.112039
31.766664	1334.239168	17.117056
31.321545	1325.907781	17.122074
31.292405	1335.877521	17.127091
31.721446	1338.041529	17.132109
31.511462	1347.645745	17.137127
31.680892	1368.322543	17.142144
31.965508	1358.495936	17.147162
32.109501	1365.574097	17.152179
32.210116	1362.708829	17.157197
32.007517	1363.665589	17.162215
31.992377	1354.649043	17.167232
32.216760	1354.379498	17.172250
32.051344	1369.896017	17.177267
31.967022	1355.697130	17.182285
32.277806	1349.461770	17.187303
32.405171	1351.213294	17.192320
32.226038	1351.587909	17.197338
32.147120	1357.495982	17.202355
32.276003	1348.045855	17.207373
32.319937	1357.937402	17.212391
32.401918	1357.235547	17.217408
32.417922	1347.129954	17.222426
32.297177	1358.867163	17.227443
32.496516	1355.847807	17.232461
32.782007	1359.005877	17.237479
32.667324	1352.020465	17.242496
32.828179	1348.812025	17.247514
32.611807	1358.871767	17.252531
32.863347	1346.386828	17.257549
33.041569	1353.108982	17.262567
32.833052	1359.216006	17.267584
32.673970	1355.916162	17.272602
32.759954	1354.553893	17.277619
32.917598	1353.030395	17.282637
32.651803	1354.040504	17.287655
33.116699	1354.660810	17.292672
32.991001	1351.328485	17.297690
32.452043	1350.051380	17.302707
32.722183	1349.444005	17.307725
32.804725	1354.887662	17.312743
32.669367	1353.475368	17.317760
32.561645	1349.612980	17.322778
32.589108	1360.934416	17.327795
32.876991	1356.653553	17.332813
32.885067	1379.226456	17.337831
33.172799	1376.445210	17.342848
33.342209	1380.305248	17.347866
33.142201	1378.923711	17.352883
33.130813	1378.210712	17.357901
33.453780	1376.093434	17.362919
33.299676	1374.152026	17.367936
33.558164	1376.258605	17.372954
33.255652	1370.265902	17.377971
33.327864	1369.105290	17.382989
33.469831	1373.531595	17.388007
33.500272	1369.532214	17.393024
33.660054	1369.856925	17.398042
33.375127	1372.193244	17.403059
33.517058	1375.083939	17.408077
33.594182	1376.655802	17.413095
33.214673	1378.275764	17.418112
33.492077	1369.842671	17.423130
33.337847	1383.989236	17.428147
33.566137	1388.928964	17.433165
34.037064	1401.399029	17.438183
33.958299	1403.259414	17.443200
34.397645	1396.496560	17.448218
33.853149	1391.520476	17.453235
33.796975	1368.372673	17.458253
33.797886	1376.049403	17.463271
33.654069	1398.581302	17.468288
34.166327	1395.165197	17.473306
34.034068	1396.049713	17.478323
34.211279	1395.720846	17.483341
34.114416	1398.613609	17.488359
34.055133	1395.756061	17.493376
34.297891	1392.447277	17.498394
33.683721	1396.386811	17.503411
33.816852	1393.536438	17.508429
34.117513	1395.650616	17.513447
34.217657	1399.223720	17.518464
34.236371	1384.059877	17.523482
34.055313	1390.526499	17.528499
34.142604	1411.666869	17.533517
34.479489	1411.354917	17.538535
34.490327	1413.211716	17.543552
34.812867	1406.657701	17.548570
34.871749	1408.845097	17.553587
34.892820	1413.001076	17.558605
35.091193	1394.599699	17.563623
34.996985	1382.659594	17.568640
34.893113	1379.321295	17.573658
34.943498	1398.515256	17.578675
34.847510	1392.769678	17.583693
34.923900	1389.094543	17.588711
34.864409	1386.868244	17.593728
35.300285	1392.043909	17.598746
34.681480	1385.515751	17.603763
34.638532	1401.781841	17.608781
35.135641	1389.846365	17.613799
35.025040	1385.258756	17.618816
35.230163	1389.058965	17.623834
34.961997	1392.065259	17.628851
35.069697	1393.411432	17.633869
35.049737	1376.437109	17.638887
34.815300	1380.163318	17.643904
35.216806	1385.590887	17.648922
35.087592	1380.271416	17.653939
34.975808	1383.515610	17.658957
35.276107	1370.919656	17.663975
34.934373	1396.054377	17.668992
35.300683	1405.528952	17.674010
35.098121	1409.286314	17.679027
35.149707	1407.902564	17.684045
35.021712	1404.234432	17.689063
34.752945	1404.973025	17.694080
35.024427	1412.830032	17.699098
35.364760	1426.372343	17.704115
35.515407	1428.461321	17.709133
35.846384	1434.562088	17.714151
35.600446	1446.810734	17.719168
36.180653	1445.051870	17.724186
35.650324	1433.863428	17.729203
35.702052	1436.715702	17.734221
35.895403	1428.467309	17.739239
35.948225	1432.842229	17.744256
36.211057	1435.368515	17.749274
36.320943	1428.633716	17.754291
35.947597	1435.848375	17.759309
36.017197	1431.335488	17.764327
36.043735	1432.295720	17.769344
36.230018	1429.033658	17.774362
36.174190	1431.430932	17.779379
36.198925	1426.856768	17.784397
36.339035	1417.885388	17.789415
36.471706	1420.186166	17.794432
36.067021	1424.967744	17.799450
36.305847	1421.262020	17.804467
35.915711	1421.168815	17.809485
36.097819	1416.604274	17.814503
35.957140	1424.839197	17.819520
36.224649	1410.103837	17.824538
36.168710	1420.618540	17.829555
36.277736	1440.303190	17.834573
36.579208	1440.560401	17.839591
36.411189	1449.204722	17.844608
36.643046	1449.700374	17.849626
36.923091	1445.224745	17.854643
36.565881	1449.926251	17.859661
36.673425	1438.792810	17.864679
36.661875	1442.458387	17.869696
36.784578	1445.555199	17.874714
36.975739	1445.078573	17.879731
36.591107	1439.186606	17.884749
37.151699	1439.174256	17.889767
36.965224	1448.756738	17.894784
36.821828	1439.169880	17.899802
37.091114	1438.596300	17.904819
36.767174	1450.117583	17.909837
36.960985	1440.857234	17.914855
37.031310	1441.922224	17.919872
37.321326	1439.506880	17.924890
37.194476	1440.141718	17.929907
37.140382	1435.460516	17.934925
37.546589	1433.773707	17.939943
37.200382	1443.740605	17.944960
36.910496	1431.642075	17.949978
37.212739	1438.044402	17.954995
37.055089	1432.885299	17.960013
37.806644	1450.985637	17.965031
37.062271	1454.743579	17.970048
37.669818	1460.850025	17.975066
37.634888	1464.965081	17.980083
37.823567	1462.211014	17.985101
38.017533	1460.983629	17.990119
37.880794	1440.991333	17.995136
37.607368	1429.705921	18.000154
37.553457	1432.694926	18.005171
37.502764	1446.386505	18.010189
38.033171	1450.780923	18.015207
37.706227	1456.677664	18.020224
37.661389	1468.175081	18.025242
37.731104	1449.499465	18.030259
37.862937	1462.291524	18.035277
38.035360	1453.009115	18.040295
38.066717	1454.933975	18.045312
38.024408	1440.980593	18.050330
38.190336	1464.112892	18.055347
37.888466	1454.273114	18.060365
37.925699	1446.022365	18.065383
37.999440	1459.718588	18.070400
38.291783	1460.775233	18.075418
38.051151	1447.173670	18.080435
37.922524	1457.176660	18.085453
38.425872	1472.684725	18.090471
38.475224	1488.360139	18.095488
38.455190	1483.259567	18.100506
38.584447	1478.972407	18.105523
38.550408	1483.645319	18.110541
38.904495	1471.591898	18.115559
38.547299	1473.087726	18.120576
38.689385	1479.884401	18.125594
38.762087	1483.390219	18.130611
38.508817	1487.664180	18.135629
38.578874	1478.962772	18.140647
38.691895	1475.746660	18.145664
38.752090	1498.520351	18.150682
38.853750	1474.048246	18.155699
38.896175	1487.817967	18.160717
38.714439	1484.813926	18.165735
38.892671	1486.760970	18.170752
39.003135	1489.327403	18.175770
39.053540	1480.832954	18.180787
38.847739	1475.182449	18.185805
38.976884	1487.916516	18.190823
38.987188	1482.950480	18.195840
39.270956	1507.812751	18.200858
39.354494	1511.433699	18.205875
39.335964	1514.546974	18.210893
39.641247	1509.673506	18.215911
39.479300	1492.263718	18.220928
39.635677	1488.853849	18.225946
39.357779	1476.710001	18.230963
39.388325	1483.360958	18.235981
39.496707	1484.949514	18.240999
39.792147	1498.487498	18.246016
39.693773	1492.855451	18.251034
39.742492	1474.515712	18.256051
39.369734	1476.058397	18.261069
39.801355	1480.068412	18.266087
39.506774	1499.559041	18.271104
39.701534	1503.173613	18.276122
39.794212	1503.120097	18.281139
39.532885	1507.835693	18.286157
39.529821	1501.504910	18.291175
39.805921	1500.787306	18.296192
39.574262	1517.464181	18.301210
39.721471	1506.324924	18.306227
39.710702	1513.259261	18.311245
39.873635	1524.080932	18.316263
39.827895	1526.451951	18.321280
40.172465	1530.730467	18.326298
40.402379	1537.040273	18.331315
40.302035	1531.529782	18.336333
40.208756	1525.490436	18.341351
40.220723	1527.544282	18.346368
40.220206	1535.795270	18.351386
40.405590	1532.630960	18.356403
40.353127	1535.332381	18.361421
40.253593	1529.549547	18.366439
40.483040	1525.757564	18.371456
40.452520	1528.913763	18.376474
40.371110	1515.064400	18.381491
40.099349	1521.917081	18.386509
40.728265	1549.394288	18.391527
40.794364	1545.737547	18.396544
40.739951	1549.167546	18.401562
41.005598	1532.814668	18.406579
41.026607	1543.742276	18.411597
40.842962	1539.810704	18.416615
40.986879	1547.016110	18.421632
41.214016	1549.586892	18.426650
41.249800	1540.035707	18.431667
41.528663	1550.078887	18.436685
41.449246	1547.834994	18.441703
41.438173	1520.254869	18.446720
41.106950	1503.690850	18.451738
41.186589	1490.011327	18.456755
41.267439	1515.194310	18.461773
41.055714	1510.247634	18.466791
41.518498	1522.370566	18.471808
41.393788	1535.337936	18.476826
41.062196	1533.004433	18.481843
41.194583	1537.648483	18.486861
41.254823	1545.731386	18.491879
41.597920	1524.901320	18.496896
41.428257	1539.846147	18.501914
41.570732	1540.652008	18.506931
41.517051	1521.987838	18.511949
41.253467	1542.519919	18.516967
41.496775	1541.890989	18.521984
41.676187	1558.905835	18.527002
42.016633	1558.946988	18.532019
42.181205	1559.339802	18.537037
41.921452	1565.162497	18.542055
42.103855	1563.657325	18.547072
42.073286	1560.846175	18.552090
42.142402	1548.166837	18.557107
42.119309	1556.285364	18.562125
42.038503	1563.459221	18.567143
42.140829	1560.871552	18.572160
41.860679	1566.122887	18.577178
42.235694	1569.427409	18.582195
42.138733	1559.425372	18.587213
41.851248	1561.163200	18.592231
42.446821	1560.638835	18.597248
42.284601	1546.180631	18.602266
42.562133	1555.382211	18.607283
42.523170	1558.613819	18.612301
42.138440	1557.301368	18.617319
42.501845	1552.126585	18.622336
42.313575	1555.517100	18.627354
42.723448	1571.506008	18.632371
42.828345	1575.516699	18.637389
42.969869	1583.170888	18.642407
43.014757	1576.678428	18.647424
42.787425	1574.709926	18.652442
42.639616	1560.355613	18.657459
42.675555	1577.595344	18.662477
42.740495	1590.321210	18.667495
43.350527	1576.795864	18.672512
43.132405	1588.851861	18.677530
43.058389	1578.105365	18.682547
43.297549	1584.402838	18.687565
42.853040	1595.446379	18.692583
43.326031	1578.439974	18.697600
43.064128	1589.107710	18.702618
43.193622	1589.870252	18.707635
43.291227	1577.904598	18.712653
43.239075	1582.676978	18.717671
43.241078	1585.520373	18.722688
43.367330	1581.658432	18.727706
43.183993	1584.886936	18.732723
43.478052	1570.957369	18.737741
43.432184	1588.464733	18.742759
43.716873	1590.959090	18.747776
43.712504	1601.549243	18.752794
43.832847	1614.907235	18.757811
43.774367	1596.517946	18.762829
43.887594	1604.442734	18.767847
44.053138	1597.960048	18.772864
43.806107	1605.169265	18.777882
43.758393	1599.721107	18.782899
43.936448	1594.949728	18.787917
43.876074	1603.595046	18.792935
44.330270	1588.043330	18.797952
43.583656	1598.967526	18.802970
44.100605	1598.983056	18.807987
43.969903	1592.091115	18.813005
43.907825	1589.328665	18.818023
44.241660	1599.392318	18.823040
44.514730	1595.329362	18.828058
44.213230	1587.136283	18.833075
44.419680	1597.211143	18.838093
44.112879	1611.993684	18.843111
45.138795	1622.699982	18.848128
44.840167	1613.969078	18.853146
44.686969	1596.966337	18.858163
44.810127	1597.476218	18.863181
44.953725	1596.585254	18.868199
44.795036	1590.762769	18.873216
44.615023	1598.490764	18.878234
44.308234	1593.543434	18.883251
44.847029	1600.205522	18.888269
44.811718	1626.518573	18.893287
45.393026	1623.776753	18.898304
44.998268	1622.386632	18.903322
45.409856	1622.751028	18.908339
45.276420	1620.637099	18.913357
44.724180	1597.770111	18.918375
45.248045	1615.291417	18.923392
45.072382	1618.019312	18.928410
45.219559	1616.157401	18.933427
45.073411	1628.215510	18.938445
45.263280	1627.803651	18.943463
45.503265	1618.865841	18.948480
45.598368	1618.640881	18.953498
45.139226	1615.599397	18.958515
45.154713	1620.269678	18.963533
45.273014	1616.056329	18.968551
45.479087	1622.888552	18.973568
45.366478	1616.562242	18.978586
45.368862	1625.822913	18.983603
45.801714	1634.986672	18.988621
45.500744	1641.884583	18.993639
45.841596	1643.230041	18.998656
45.954486	1651.030317	19.003674
46.004001	1650.565478	19.008691
45.940517	1646.752195	19.013709
45.857815	1641.850880	19.018727
45.920816	1640.028267	19.023744
45.944802	1640.723808	19.028762
46.044610	1641.638288	19.033779
46.120196	1643.323018	19.038797
45.991863	1650.327624	19.043815
46.089515	1642.425601	19.048832
46.195571	1635.781294	19.053850
46.149281	1650.748356	19.058867
46.508688	1661.181401	19.063885
46.509739	1663.877937	19.068903
46.869492	1669.337504	19.073920
46.729506	1657.114037	19.078938
46.763585	1653.010253	19.083955
46.857472	1646.362835	19.088973
46.608650	1648.648154	19.093991
47.066273	1646.675301	19.099008
46.726677	1653.272746	19.104026
46.806922	1658.710199	19.109043
46.555279	1657.956386	19.114061
46.585305	1663.490907	19.119079
46.876146	1666.210612	19.124096
46.783224	1655.172141	19.129114
46.798913	1655.720843	19.134131
46.941456	1658.658140	19.139149
46.943957	1657.567090	19.144167
47.058994	1655.120005	19.149184
47.258902	1662.713214	19.154202
47.554497	1669.677891	19.159219
47.544078	1675.762146	19.164237
47.603341	1686.600670	19.169255
47.391506	1674.178063	19.174272
47.393320	1665.543134	19.179290
47.355996	1674.238614	19.184307
47.794952	1687.516266	19.189325
47.705140	1674.944179	19.194343
47.621382	1672.278396	19.199360
47.887647	1682.985282	19.204378
48.105845	1678.446389	19.209395
48.022416	1666.377329	19.214413
47.863294	1676.788209	19.219431
47.795244	1683.389017	19.224448
48.283631	1674.872080	19.229466
48.126053	1677.218695	19.234483
48.135920	1673.870393	19.239501
47.791032	1674.809940	19.244519
47.946359	1673.958565	19.249536
48.181856	1674.368792	19.254554
47.992732	1669.188239	19.259571
47.883001	1668.673149	19.264589
47.854308	1671.285242	19.269607
48.264105	1680.415638	19.274624
48.293831	1685.450669	19.279642
48.396312	1700.122361	19.284659
48.688604	1704.465660	19.289677
48.654646	1700.110735	19.294695
48.582491	1702.120047	19.299712
48.821100	1705.448124	19.304730
48.603612	1703.814750	19.309747
48.733435	1686.598232	19.314765
48.275729	1700.763940	19.319783
48.460733	1686.106708	19.324800
48.724543	1710.711219	19.329818
48.729475	1703.075639	19.334835
49.001558	1695.749025	19.339853
48.825493	1703.212278	19.344871
48.489680	1705.343890	19.349888
48.894228	1711.936489	19.354906
48.974072	1732.927171	19.359923
49.191383	1711.292340	19.364941
49.140293	1723.992024	19.369959
49.218307	1722.319068	19.374976
49.323708	1711.581802	19.379994
49.056884	1720.151864	19.385011
49.567358	1723.326174	19.390029
49.352346	1725.888366	19.395047
49.376009	1733.434167	19.400064
49.440654	1749.154165	19.405082
49.603265	1745.535556	19.410099
49.799132	1744.310196	19.415117
49.647438	1755.545792	19.420135
49.727632	1751.206041	19.425152
50.038833	1749.158958	19.430170
49.770724	1745.683366	19.435187
50.133823	1746.720271	19.440205
50.508541	1747.324596	19.445223
50.507429	1745.348213	19.450240
50.183682	1743.820179	19.455258
50.166964	1738.780188	19.460275
50.275033	1743.714901	19.465293
50.193041	1741.550332	19.470311
50.424655	1741.490390	19.475328
50.258648	1746.112954	19.480346
50.425200	1739.703459	19.485363
50.532429	1746.865225	19.490381
50.401759	1745.640877	19.495399
50.388375	1734.914760	19.500416
50.110634	1746.351276	19.505434
50.446605	1753.515595	19.510451
50.783037	1756.802915	19.515469
50.374042	1775.692789	19.520487
50.673536	1767.856353	19.525504
50.949204	1764.324951	19.530522
50.913399	1782.481390	19.535539
50.888561	1761.128602	19.540557
51.213396	1761.001883	19.545575
51.243290	1762.922104	19.550592
51.226666	1747.565733	19.555610
51.160579	1756.913576	19.560627
51.457303	1744.691095	19.565645
51.363513	1756.268265	19.570663
51.013284	1768.787718	19.575680
51.347513	1761.106354	19.580698
51.414648	1763.199338	19.585715
51.078624	1771.684221	19.590733
51.275599	1783.091723	19.595751
51.634235	1791.849186	19.600768
51.579563	1787.718501	19.605786
51.570315	1800.930961	19.610803
51.904439	1791.184669	19.615821
51.582836	1792.763217	19.620839
51.994013	1793.139694	19.625856
52.013902	1791.775909	19.630874
52.058384	1785.902061	19.635891
52.227825	1800.873183	19.640909
52.043939	1790.610390	19.645927
51.663387	1798.197036	19.650944
52.258342	1787.215650	19.655962
52.059082	1785.619605	19.660979
52.121035	1781.255107	19.665997
51.988384	1784.621324	19.671015
51.981097	1794.226964	19.676032
52.191469	1790.107593	19.681050
52.165578	1797.693698	19.686067
52.858182	1810.465618	19.691085
52.654383	1811.931208	19.696103
52.964413	1809.441051	19.701120
52.982731	1801.872690	19.706138
52.612904	1796.704436	19.711155
52.822842	1800.873597	19.716173
53.232142	1795.195536	19.721191
52.593263	1796.402347	19.726208
53.223738	1791.387268	19.731226
52.942026	1806.288868	19.736243
53.264473	1809.787542	19.741261
53.135514	1797.063967	19.746279
53.024654	1805.567560	19.751296
53.197237	1793.840305	19.756314
53.139135	1804.126715	19.761331
53.017861	1808.694273	19.766349
53.169946	1804.176701	19.771367
52.823564	1807.046016	19.776384
53.071469	1796.934283	19.781402
53.213512	1800.636370	19.786419
53.027667	1814.644279	19.791437
53.146242	1821.471170	19.796455
53.261567	1828.133264	19.801472
53.828331	1822.671666	19.806490
53.730965	1825.038271	19.811507
53.762516	1829.536491	19.816525
53.876116	1822.597188	19.821543
54.075623	1826.358281	19.826560
53.948671	1833.168078	19.831578
53.722298	1833.540078	19.836595
53.996373	1851.825688	19.841613
54.059009	1848.652663	19.846631
54.261702	1858.715719	19.851648
54.437971	1850.943890	19.856666
54.216460	1858.574160	19.861683
54.464011	1855.998267	19.866701
54.456366	1857.561158	19.871719
54.229752	1840.807656	19.876736
54.326269	1849.259094	19.881754
54.558349	1856.770122	19.886771
54.487747	1844.975741	19.891789
54.778462	1852.995527	19.896807
54.574638	1847.817343	19.901824
54.413605	1844.260852	19.906842
54.623984	1876.701185	19.911859
54.759506	1884.562005	19.916877
54.778589	1885.057798	19.921895
54.781948	1885.846317	19.926912
54.977436	1883.933876	19.931930
55.095085	1886.441320	19.936947
54.945739	1889.024377	19.941965
55.250174	1874.986533	19.946983
55.032538	1884.692336	19.952000
55.373013	1880.915578	19.957018
55.139887	1884.200792	19.962035
55.366072	1903.824948	19.967053
55.731615	1904.675062	19.972071
55.630585	1897.010837	19.977088
55.855736	1899.440880	19.982106
55.735357	1891.839888	19.987123
55.958684	1896.716238	19.992141
55.870472	1878.851156	19.997159
56.024391	1872.511404	20.002176
55.908973	1866.296270	20.007194
55.932242	1870.624236	20.012211
55.885970	1873.160143	20.017229
55.941871	1867.473924	20.022247
55.510659	1893.297595	20.027264
56.200504	1900.095862	20.032282
55.872167	1896.601647	20.037299
55.937459	1905.304313	20.042317
56.263427	1892.348808	20.047335
56.270170	1904.226963	20.052352
56.392619	1891.832987	20.057370
56.429591	1898.292727	20.062387
56.243358	1916.063003	20.067405
56.504712	1917.380289	20.072423
56.635015	1924.247803	20.077440
56.738937	1928.477820	20.082458
57.007493	1941.459672	20.087475
56.779956	1927.053630	20.092493
57.109805	1922.210813	20.097511
56.973019	1935.969017	20.102528
56.877064	1923.156231	20.107546
56.874081	1910.342264	20.112563
56.938016	1919.830515	20.117581
57.005199	1915.495624	20.122599
57.021251	1921.854904	20.127616
56.979718	1909.578357	20.132634
57.108905	1917.818746	20.137651
57.385640	1931.129125	20.142669
57.672517	1937.023230	20.147687
57.518909	1949.557774	20.152704
57.769305	1936.953859	20.157722
57.907916	1936.324108	20.162739
57.862105	1938.477114	20.167757
57.795000	1924.243560	20.172775
57.693571	1931.490280	20.177792
57.601877	1936.071096	20.182810
58.238455	1938.054653	20.187827
57.464601	1952.951505	20.192845
58.071954	1939.115688	20.197863
57.840049	1946.588483	20.202880
58.180873	1950.240043	20.207898
58.185299	1943.371870	20.212915
57.941549	1955.753616	20.217933
58.084170	1951.590876	20.222951
57.848994	1951.299634	20.227968
58.148433	1962.008713	20.232986
58.180951	1966.633966	20.238003
58.283214	1974.650117	20.243021
58.519940	1966.861745	20.248039
58.317825	1963.220291	20.253056
58.338111	1966.662644	20.258074
58.726780	1973.186729	20.263091
58.977091	1984.881601	20.268109
58.915882	1984.609245	20.273127
59.267417	1999.063312	20.278144
59.090424	1985.658018	20.283162
59.031032	1981.041888	20.288179
58.823971	1995.387686	20.293197
59.581965	1986.714031	20.298215
59.485206	1991.971619	20.303232
59.352019	1979.605250	20.308250
59.393116	1987.130186	20.313267
59.408938	1990.022941	20.318285
59.376522	1978.558139	20.323303
59.383757	1988.738609	20.328320
59.451379	1989.779284	20.333338
59.534764	1993.648575	20.338355
59.348041	1994.348441	20.343373
59.856644	1983.872674	20.348391
59.414663	1985.614032	20.353408
59.571744	1977.986044	20.358426
59.542157	1982.268647	20.363443
59.670876	2015.706922	20.368461
59.995132	2007.263772	20.373479
59.855045	2012.346064	20.378496
60.201760	2019.798666	20.383514
60.212556	2021.402814	20.388531
60.121204	2025.780272	20.393549
60.139424	2020.907234	20.398567
60.238565	2017.756487	20.403584
60.072883	2018.374342	20.408602
60.495029	2029.827488	20.413619
60.238831	2043.892698	20.418637
60.488842	2057.318025	20.423655
60.532121	2051.362787	20.428672
60.571912	2043.695296	20.433690
60.950138	2040.610227	20.438707
61.044537	2045.917734	20.443725
61.120362	2044.708054	20.448743
61.122702	2037.183553	20.453760
60.971029	2040.422863	20.458778
61.127287	2038.496022	20.463795
61.058938	2042.363039	20.468813
61.372766	2031.280902	20.473831
61.173599	2040.021243	20.478848
60.886685	2045.613195	20.483866
61.572597	2054.907027	20.488883
61.449444	2065.494098	20.493901
61.722836	2067.662676	20.498919
61.695162	2064.594877	20.503936
61.699896	2067.752840	20.508954
61.937878	2054.252145	20.513971
61.891057	2063.977468	20.518989
62.001443	2064.778425	20.524007
62.167382	2061.222573	20.529024
61.856123	2060.770492	20.534042
62.054342	2063.317796	20.539059
61.927324	2064.813434	20.544077
62.215388	2058.427819	20.549095
62.319928	2060.454432	20.554112
61.883251	2062.734242	20.559130
62.171370	2066.759073	20.564147
62.435886	2058.846782	20.569165
62.460188	2066.699502	20.574183
62.801102	2073.727341	20.579200
62.587716	2082.385418	20.584218
62.896946	2063.964924	20.589235
62.721583	2079.564698	20.594253
63.017314	2067.923175	20.599271
63.191858	2066.277732	20.604288
62.853841	2072.657790	20.609306
63.184881	2066.346362	20.614323
63.035541	2076.223070	20.619341
63.187606	2066.979480	20.624359
63.130587	2077.527680	20.629376
63.086612	2069.583690	20.634394
63.208283	2062.827180	20.639411
62.938496	2082.849437	20.644429
63.161988	2063.642003	20.649447
63.226143	2058.808799	20.654464
63.173160	2071.191591	20.659482
63.333993	2075.374847	20.664499
63.291464	2097.038549	20.669517
63.257219	2107.741653	20.674535
63.546010	2099.302936	20.679552
63.190870	2113.183198	20.684570
63.624080	2102.162576	20.689587
63.795485	2112.904924	20.694605
63.922406	2134.446001	20.699623
63.849586	2124.097709	20.704640
63.719262	2137.595796	20.709658
63.975948	2126.606884	20.714675
64.151059	2129.190692	20.719693
64.118795	2118.448138	20.724711
64.188742	2135.685039	20.729728
64.314959	2147.800112	20.734746
65.026176	2153.754878	20.739763
64.991488	2154.317237	20.744781
65.067376	2139.657135	20.749799
64.861413	2122.754059	20.754816
64.731623	2126.220853	20.759834
65.016800	2123.898716	20.764851
64.847979	2115.591705	20.769869
65.218832	2131.006004	20.774887
65.317648	2139.482023	20.779904
65.012504	2122.760873	20.784922
65.313936	2137.148947	20.789939
65.116866	2146.521032	20.794957
64.974272	2143.312182	20.799975
65.126206	2145.716373	20.804992
65.461854	2148.012459	20.810010
65.659018	2150.893978	20.815027
65.343385	2145.292868	20.820045
65.528128	2142.506854	20.825063
65.699171	2144.261882	20.830080
65.419903	2152.566349	20.835098
65.835084	2160.602930	20.840115
66.138035	2164.742256	20.845133
66.068235	2168.897118	20.850151
66.388569	2165.779862	20.855168
66.145028	2171.466455	20.860186
66.468827	2176.771924	20.865203
66.416325	2176.658545	20.870221
66.158696	2168.076638	20.875239
66.616229	2165.369155	20.880256
66.139181	2172.196798	20.885274
66.260064	2170.135247	20.890291
66.484024	2163.899540	20.895309
66.470077	2166.424051	20.900327
66.543661	2164.479363	20.905344
66.228944	2158.440929	20.910362
66.895180	2168.009516	20.915379
66.890895	2179.107685	20.920397
66.843174	2200.053160	20.925415
67.001980	2198.408925	20.930432
67.251909	2204.660784	20.935450
67.288622	2196.570532	20.940467
67.545306	2189.408225	20.945485
67.315454	2191.206670	20.950503
67.321355	2190.370512	20.955520
67.110272	2203.162376	20.960538
67.322439	2198.895960	20.965555
67.301148	2199.510433	20.970573
66.879522	2195.819377	20.975591
67.376990	2195.253535	20.980608
67.313612	2213.843939	20.985626
67.464562	2227.284209	20.990643
67.334303	2219.692758	20.995661
67.554897	2220.147783	21.000679
67.704485	2238.195980	21.005696
68.043003	2247.916794	21.010714
67.683019	2251.631479	21.015731
68.195218	2246.558249	21.020749
67.991944	2260.872960	21.025767
68.662919	2242.283039	21.030784
68.177027	2254.869590	21.035802
68.508652	2238.148793	21.040819
68.652718	2239.441791	21.045837
68.528217	2241.249997	21.050855
68.746242	2229.383418	21.055872
68.672615	2245.694638	21.060890
68.754734	2254.986209	21.065907
69.070216	2253.822731	21.070925
68.685422	2266.504978	21.075943
69.202242	2267.789529	21.080960
68.971256	2273.527821	21.085978
69.514603	2264.197214	21.090995
69.417432	2257.666924	21.096013
69.567458	2269.011488	21.101031
69.510512	2262.273580	21.106048
69.611426	2263.441832	21.111066
69.933009	2265.438513	21.116083
69.678750	2252.059532	21.121101
69.767421	2258.103433	21.126119
70.052797	2250.723184	21.131136
70.077749	2262.998378	21.136154
69.856504	2255.565632	21.141171
69.990748	2257.750736	21.146189
69.922846	2275.244411	21.151207
70.106412	2249.445637	21.156224
70.026946	2256.476692	21.161242
69.899584	2253.078702	21.166259
70.029662	2244.403555	21.171277
69.688523	2257.719474	21.176295
70.081219	2268.675737	21.181312
69.855657	2272.554027	21.186330
70.046652	2282.244914	21.191347
70.453030	2291.236488	21.196365
70.409525	2288.618469	21.201383
70.588805	2296.344524	21.206400
70.700583	2317.305333	21.211418
70.823619	2312.941221	21.216435
70.981904	2305.097142	21.221453
70.688016	2312.325059	21.226471
71.072350	2299.067269	21.231488
71.263715	2308.518956	21.236506
71.157717	2313.771290	21.241523
71.469033	2301.117646	21.246541
71.408696	2300.471350	21.251559
71.628014	2321.313024	21.256576
71.764018	2333.236287	21.261594
71.535000	2336.623271	21.266611
71.558062	2338.724404	21.271629
71.872239	2344.951334	21.276647
72.160934	2353.535454	21.281664
72.044572	2345.552499	21.286682
72.001079	2336.874291	21.291699
72.189657	2339.420282	21.296717
71.932838	2334.048146	21.301735
72.251983	2326.388483	21.306752
72.115651	2331.490532	21.311770
72.157762	2333.351133	21.316787
72.543133	2331.564730	21.321805
71.900592	2344.883681	21.326823
72.272650	2328.287001	21.331840
72.304267	2348.590874	21.336858
72.199122	2357.639258	21.341875
72.619677	2360.740381	21.346893
72.313699	2365.612028	21.351911
72.309136	2361.551447	21.356928
72.577208	2374.670742	21.361946
72.564510	2392.475090	21.366963
72.901383	2386.896572	21.371981
73.147809	2395.925071	21.376999
73.259018	2379.591109	21.382016
73.354218	2389.101450	21.387034
73.088989	2383.430707	21.392051
73.376187	2379.339822	21.397069
73.582511	2390.617105	21.402087
73.748420	2408.431719	21.407104
74.072090	2404.733985	21.412122
73.887774	2403.987904	21.417139
74.040481	2398.875806	21.422157
73.730094	2398.339718	21.427175
74.267115	2392.891892	21.432192
74.259155	2404.154205	21.437210
74.389500	2409.390547	21.442227
74.216185	2400.243042	21.447245
74.454611	2401.998381	21.452263
74.786023	2397.702758	21.457280
74.623547	2392.803756	21.462298
74.367085	2393.881870	21.467315
74.548102	2385.944630	21.472333
74.508624	2404.255546	21.477351
74.920734	2381.044391	21.482368
74.931230	2394.870785	21.487386
74.496033	2402.807872	21.492403
74.731477	2397.633682	21.497421
74.465410	2405.631990	21.502439
74.654236	2405.261424	21.507456
74.892712	2416.163558	21.512474
74.868548	2438.301639	21.517491
75.184940	2426.554078	21.522509
75.318808	2428.997912	21.527527
75.403756	2426.696220	21.532544
75.541959	2427.659517	21.537562
75.704682	2439.492232	21.542579
75.941041	2438.020775	21.547597
75.559333	2447.912299	21.552615
75.362357	2445.356816	21.557632
75.815674	2446.531807	21.562650
75.561358	2452.622814	21.567667
75.975928	2444.770368	21.572685
75.936153	2452.399637	21.577703
76.001497	2467.716539	21.582720
76.420500	2471.593481	21.587738
76.442233	2469.984859	21.592755
76.530585	2476.835932	21.597773
76.306011	2469.664640	21.602791
76.368384	2475.807256	21.607808
76.459148	2467.873078	21.612826
76.235115	2467.195954	21.617843
76.953516	2484.606389	21.622861
77.146161	2486.722233	21.627879
77.024280	2492.184522	21.632896
77.482246	2498.726120	21.637914
77.018178	2495.062081	21.642931
77.209737	2484.513375	21.647949
77.275909	2495.394630	21.652967
77.190484	2486.327033	21.657984
77.330974	2492.414428	21.663002
77.382318	2492.690159	21.668019
77.656373	2490.715060	21.673037
77.337980	2490.850326	21.678055
77.432351	2493.034571	21.683072
77.507877	2495.786856	21.688090
77.375715	2514.282301	21.693107
77.888452	2524.020956	21.698125
77.922677	2525.112064	21.703143
78.022027	2517.209117	21.708160
78.418635	2519.089110	21.713178
78.239513	2524.140816	21.718195
78.506402	2532.708366	21.723213
78.291737	2513.061588	21.728231
78.006990	2527.728964	21.733248
78.517620	2533.030848	21.738266
78.624656	2542.741677	21.743283
78.976581	2530.911793	21.748301
79.175290	2541.970775	21.753319
79.082473	2544.737106	21.758336
79.188393	2529.742164	21.763354
78.913498	2549.515096	21.768371
79.400445	2534.415458	21.773389
79.113051	2530.193116	21.778407
79.461809	2537.157081	21.783424
79.384951	2533.868787	21.788442
79.126832	2530.449431	21.793459
79.385450	2535.013086	21.798477
79.205298	2527.631486	21.803495
79.052543	2556.335657	21.808512
79.748813	2564.999979	21.813530
79.653525	2569.602047	21.818547
79.676705	2568.345911	21.823565
79.815444	2560.551780	21.828583
79.500746	2577.979892	21.833600
79.711440	2585.193452	21.838618
79.733236	2592.713015	21.843635
79.926116	2584.937483	21.848653
80.161758	2605.551267	21.853671
80.250877	2616.332758	21.858688
80.850783	2614.543550	21.863706
80.895407	2618.324133	21.868723
81.291592	2602.728826	21.873741
81.286643	2608.791089	21.878759
81.349812	2595.922318	21.883776
81.500733	2597.659464	21.888794
81.151705	2581.868439	21.893811
81.160895	2572.233220	21.898829
81.082029	2588.523228	21.903847
81.284203	2596.882228	21.908864
81.838077	2585.017751	21.913882
81.951439	2593.416227	21.918899
81.928322	2592.022866	21.923917
82.036462	2589.251596	21.928935
81.755054	2575.633527	21.933952
81.764630	2577.181048	21.938970
81.463006	2584.971360	21.943987
81.870822	2595.007302	21.949005
81.861496	2592.119230	21.954023
81.813001	2607.234622	21.959040
81.650971	2595.605750	21.964058
81.735626	2611.879391	21.969075
81.699584	2620.530115	21.974093
81.908920	2624.398436	21.979111
82.163702	2627.466774	21.984128
82.500613	2645.393554	21.989146
82.421070	2665.889825	21.994163
82.496692	2649.418356	21.999181
82.834812	2647.387378	22.004199
82.379929	2662.221963	22.009216
83.200167	2646.226638	22.014234
83.259651	2644.030690	22.019251
83.040856	2659.254584	22.024269
83.576200	2650.033922	22.029287
83.382382	2644.904796	22.034304
83.636634	2658.638395	22.039322
83.803790	2647.866457	22.044339
83.641119	2641.976714	22.049357
83.798211	2641.364156	22.054375
83.532449	2641.244282	22.059392
83.603121	2647.858208	22.064410
83.868268	2668.936467	22.069427
84.028742	2675.921766	22.074445
84.314812	2671.342828	22.079463
84.252396	2678.290946	22.084480
84.412036	2672.545954	22.089498
84.734620	2672.751673	22.094515
84.325225	2667.316447	22.099533
84.560009	2672.704117	22.104551
84.810662	2673.764985	22.109568
84.586283	2660.554718	22.114586
84.308960	2668.728437	22.119603
84.453710	2660.420298	22.124621
84.762502	2671.345441	22.129639
84.598222	2696.514956	22.134656
84.817498	2687.553970	22.139674
84.695689	2693.217489	22.144691
84.849997	2686.010062	22.149709
85.102930	2702.381970	22.154727
84.928529	2716.490373	22.159744
85.255514	2716.389476	22.164762
85.238497	2718.794118	22.169779
85.276188	2718.768976	22.174797
85.710544	2744.262857	22.179815
85.478345	2747.034540	22.184832
86.192717	2754.073617	22.189850
86.032507	2745.087906	22.194867
86.063703	2740.275092	22.199885
86.223459	2744.534296	22.204903
86.135176	2751.874498	22.209920
86.375124	2737.991799	22.214938
86.507740	2764.291048	22.219955
86.451386	2762.371299	22.224973
86.928959	2762.780139	22.229991
86.879260	2767.631807	22.235008
86.977071	2756.661813	22.240026
87.022559	2767.722654	22.245043
87.053050	2762.388321	22.250061
87.375192	2760.727668	22.255079
86.948098	2757.927887	22.260096
87.084542	2758.074213	22.265114
86.939957	2759.442511	22.270131
87.204726	2751.842409	22.275149
87.402701	2756.715349	22.280167
87.657412	2786.937582	22.285184
87.608185	2777.399680	22.290202
87.896352	2793.505638	22.295219
87.769982	2783.493100	22.300237
88.204235	2782.120205	22.305255
87.956004	2790.413584	22.310272
88.050942	2781.888425	22.315290
88.271844	2780.648417	22.320307
88.191299	2783.576929	22.325325
88.475120	2766.514660	22.330343
88.287937	2777.084451	22.335360
88.330914	2778.593798	22.340378
88.112977	2790.598536	22.345395
88.280331	2798.297288	22.350413
88.445247	2787.108319	22.355431
88.542868	2799.327051	22.360448
88.629007	2805.407409	22.365466
88.928518	2821.820958	22.370483
89.065659	2834.270185	22.375501
89.507075	2835.088528	22.380519
88.865768	2828.947109	22.385536
89.244091	2829.947130	22.390554
89.172688	2829.838050	22.395571
89.236557	2830.224312	22.400589
89.725386	2833.627229	22.405607
89.661144	2850.653254	22.410624
89.784077	2857.916480	22.415642
89.605620	2854.309486	22.420659
89.825356	2863.107837	22.425677
90.430353	2857.791921	22.430695
90.062517	2849.794749	22.435712
90.420100	2851.692256	22.440730
90.623455	2847.146619	22.445747
90.239585	2850.402025	22.450765
90.280490	2863.002998	22.455783
90.706997	2881.326255	22.460800
90.804270	2880.399176	22.465818
90.882184	2880.178418	22.470835
90.742937	2876.316524	22.475853
90.888205	2882.497769	22.480871
90.985370	2877.279933	22.485888
90.965064	2876.397479	22.490906
91.209951	2895.752693	22.495923
91.226616	2909.458847	22.500941
91.494494	2899.067715	22.505959
91.221273	2904.825225	22.510976
91.227982	2909.444002	22.515994
91.576176	2908.396722	22.521011
91.657424	2921.890256	22.526029
92.015675	2922.781793	22.531047
91.863752	2929.536554	22.536064
91.924481	2924.186145	22.541082
92.371712	2925.747994	22.546099
92.418128	2943.993192	22.551117
92.470175	2931.761391	22.556135
92.317182	2939.181662	22.561152
92.681482	2942.677621	22.566170
92.941284	2950.569826	22.571187
92.731761	2955.543234	22.576205
93.612157	2951.524647	22.581223
93.059618	2955.572486	22.586240
93.037558	2954.802518	22.591258
93.304114	2942.603370	22.596275
93.058263	2960.316980	22.601293
93.412140	2949.075806	22.606311
93.254062	2950.206595	22.611328
93.391095	2952.647627	22.616346
93.442582	2942.536308	22.621363
93.088264	2961.436305	22.626381
93.437881	2965.553965	22.631399
93.344504	2990.464218	22.636416
93.573304	2987.446963	22.641434
93.882466	2987.978911	22.646451
94.045989	3003.716721	22.651469
94.340719	3006.398625	22.656487
94.287908	3012.783119	22.661504
94.222990	3013.338693	22.666522
94.652955	3021.669733	22.671539
94.280922	3012.700758	22.676557
94.691745	3006.779496	22.681575
94.575255	3018.684579	22.686592
94.546531	3028.964980	22.691610
94.880772	3041.755022	22.696627
94.926541	3050.485378	22.701645
95.201546	3036.619848	22.706663
95.086526	3039.935983	22.711680
95.264334	3041.347487	22.716698
95.623782	3041.708929	22.721715
95.604108	3037.641415	22.726733
95.454417	3054.049911	22.731751
95.291557	3062.423420	22.736768
95.678676	3066.976236	22.741786
96.082448	3060.293542	22.746803
95.680934	3069.908818	22.751821
95.833004	3065.790478	22.756839
96.100410	3072.347275	22.761856
96.472118	3089.121215	22.766874
96.282126	3091.530482	22.771891
96.864831	3096.808056	22.776909
96.881791	3097.983946	22.781927
96.785285	3095.827883	22.786944
96.770570	3091.561509	22.791962
96.975862	3086.637539	22.796979
96.849963	3088.941730	22.801997
97.127960	3088.994986	22.807015
97.043441	3087.124338	22.812032
97.178737	3088.703497	22.817050
97.364180	3099.541848	22.822067
97.345348	3090.699500	22.827085
97.352227	3106.195195	22.832103
97.617574	3112.058272	22.837120
97.476464	3111.646542	22.842138
97.710399	3105.945018	22.847155
97.884959	3107.829494	22.852173
97.693922	3126.449174	22.857191
98.208750	3129.938412	22.862208
98.000986	3134.780093	22.867226
98.577998	3129.609653	22.872243
98.630997	3141.064392	22.877261
98.581112	3129.972874	22.882279
98.713259	3125.193258	22.887296
98.680253	3129.875749	22.892314
98.943909	3138.303623	22.897331
98.639298	3165.839947	22.902349
98.921360	3151.151119	22.907367
99.411860	3160.335991	22.912384
99.415178	3153.556439	22.917402
99.263744	3149.700427	22.922419
99.306700	3142.975745	22.927437
99.572733	3149.712719	22.932455
99.434419	3158.419618	22.937472
99.425006	3178.244362	22.942490
99.784114	3166.411234	22.947507
99.757111	3174.719835	22.952525
99.724770	3179.666006	22.957543
100.066171	3172.717591	22.962560
99.856533	3184.531501	22.967578
100.079803	3197.538431	22.972595
100.385759	3199.767342	22.977613
100.562293	3191.348551	22.982631
100.763510	3182.110349	22.987648
100.632398	3204.394557	22.992666
100.634306	3193.389315	22.997683
100.881705	3223.910060	23.002701
101.136533	3222.819135	23.007719
101.167598	3228.069011	23.012736
101.212443	3223.571897	23.017754
101.190445	3225.886498	23.022771
101.155495	3235.421621	23.027789
101.174054	3231.947335	23.032807
101.215124	3239.214425	23.037824
101.104551	3256.459570	23.042842
101.540501	3254.158811	23.047859
101.746083	3256.756279	23.052877
101.557216	3251.725737	23.057895
101.998264	3270.330514	23.062912
102.133339	3280.838343	23.067930
102.657245	3277.273458	23.072947
102.567074	3282.689447	23.077965
102.976195	3274.606977	23.082983
103.094958	3273.255071	23.088000
102.661836	3272.528601	23.093018
103.051134	3262.355742	23.098035
102.956763	3262.049276	23.103053
103.069732	3262.795147	23.108071
102.903524	3273.368109	23.113088
102.805086	3259.821170	23.118106
103.032074	3264.975300	23.123123
103.238678	3289.882134	23.128141
103.085886	3283.942482	23.133159
103.732962	3280.467873	23.138176
103.786214	3286.452281	23.143194
103.987181	3290.320973	23.148211
103.720970	3299.421127	23.153229
103.912811	3309.801881	23.158247
104.214826	3311.332649	23.163264
103.890762	3305.668137	23.168282
104.512715	3319.271095	23.173299
104.448755	3315.506098	23.178317
104.672444	3320.573391	23.183335
105.005191	3326.752969	23.188352
104.698432	3340.350349	23.193370
104.531359	3329.330807	23.198387
104.855454	3327.624499	23.203405
104.942790	3326.498251	23.208423
105.168090	3341.212428	23.213440
105.441924	3343.141553	23.218458
105.189380	3359.837442	23.223475
105.617050	3359.920693	23.228493
105.782561	3363.123614	23.233511
106.107498	3359.828594	23.238528
106.123073	3374.236909	23.243546
105.885812	3375.728053	23.248563
106.017967	3361.401983	23.253581
106.016992	3366.851293	23.258599
105.760878	3367.645951	23.263616
106.059727	3389.564499	23.268634
106.156115	3392.217041	23.273651
106.459903	3384.388926	23.278669
106.580032	3390.830038	23.283687
106.905508	3407.713538	23.288704
106.974468	3421.708353	23.293722
107.457479	3406.653798	23.298739
107.562547	3418.420609	23.303757
107.379015	3422.791842	23.308775
107.883733	3410.791557	23.313792
107.464909	3429.414199	23.318810
107.448688	3412.796861	23.323827
107.405723	3412.844887	23.328845
107.367903	3419.727856	23.333863
107.812542	3413.512272	23.338880
107.435069	3444.229616	23.343898
107.930897	3442.201219	23.348915
107.857207	3441.408656	23.353933
107.791579	3453.846611	23.358951
108.263491	3461.019780	23.363968
108.097378	3479.074347	23.368986
108.368609	3479.229906	23.374003
108.673079	3469.737464	23.379021
108.413770	3479.818864	23.384039
109.212189	3486.900299	23.389056
109.130470	3493.183074	23.394074
109.109556	3499.579820	23.399091
109.475929	3496.491704	23.404109
109.488950	3486.142293	23.409127
109.758331	3488.150519	23.414144
109.620458	3492.679187	23.419162
109.635496	3479.273148	23.424179
109.692454	3488.233791	23.429197
109.892835	3484.414445	23.434215
110.038320	3475.661655	23.439232
109.948553	3498.908744	23.444250
110.069176	3517.328969	23.449267
110.245558	3511.064759	23.454285
110.170989	3513.828247	23.459303
110.382393	3510.166522	23.464320
110.361776	3518.021496	23.469338
110.446361	3529.655556	23.474355
110.874041	3533.878974	23.479373
110.704237	3548.297609	23.484391
110.598791	3542.817753	23.489408
110.733885	3570.165995	23.494426
110.773963	3581.483824	23.499443
111.067236	3565.108098	23.504461
111.475561	3572.896160	23.509479
111.501918	3581.146949	23.514496
111.761725	3590.349332	23.519514
111.816782	3586.288618	23.524531
112.322044	3594.795717	23.529549
112.218098	3594.038067	23.534567
112.477420	3589.982576	23.539584
112.425835	3586.548935	23.544602
112.450507	3606.576862	23.549619
112.728096	3614.605447	23.554637
112.591360	3621.859183	23.559655
112.735297	3616.728254	23.564672
112.671824	3618.583621	23.569690
112.675075	3613.176330	23.574707
112.905445	3627.223007	23.579725
113.109498	3641.383889	23.584743
113.114123	3637.712207	23.589760
113.235237	3652.529328	23.594778
113.571215	3651.295043	23.599795
113.943940	3662.772929	23.604813
113.892356	3669.834269	23.609831
114.418441	3670.978046	23.614848
114.368504	3675.859957	23.619866
114.507129	3664.466433	23.624883
114.763366	3653.638134	23.629901
114.731644	3680.863346	23.634919
115.216436	3652.964410	23.639936
114.962122	3666.914043	23.644954
114.984318	3657.613800	23.649971
115.355897	3653.974788	23.654989
114.845462	3665.369469	23.660007
115.241492	3660.944910	23.665024
115.159669	3657.520187	23.670042
115.348969	3655.867220	23.675059
115.495716	3650.935030	23.680077
115.532880	3660.307709	23.685095
115.636076	3645.973957	23.690112
115.293058	3658.179561	23.695130
115.098519	3674.442577	23.700147
115.391358	3679.411554	23.705165
115.310949	3691.020240	23.710183
115.720959	3708.995233	23.715200
115.867011	3712.431761	23.720218
115.945048	3719.041778	23.725235
116.173521	3735.334174	23.730253
116.133208	3742.811014	23.735271
116.221778	3739.188430	23.740288
116.729568	3762.653716	23.745306
116.525034	3756.841725	23.750323
116.685884	3765.851111	23.755341
116.910983	3773.261669	23.760359
117.324086	3786.238120	23.765376
117.706216	3793.658568	23.770394
117.744715	3790.194642	23.775411
118.081547	3779.410815	23.780429
117.732682	3789.015076	23.785447
118.233112	3781.333409	23.790464
118.317672	3778.060697	23.795482
118.370707	3780.565742	23.800499
118.388846	3780.275320	23.805517
118.419661	3775.094132	23.810535
118.604222	3782.854312	23.815552
118.615709	3796.459742	23.820570
118.921588	3795.995001	23.825587
119.293134	3806.097571	23.830605
119.087743	3815.256874	23.835623
119.171813	3808.593223	23.840640
119.293355	3797.002813	23.845658
119.011635	3807.615697	23.850675
119.271997	3810.270744	23.855693
119.551894	3838.040029	23.860711
119.618828	3831.574086	23.865728
119.693375	3839.339874	23.870746
119.857453	3838.055237	23.875763
120.131416	3836.327236	23.880781
119.771686	3860.478940	23.885799
120.062900	3859.015810	23.890816
120.307581	3852.668129	23.895834
120.374371	3874.414285	23.900851
120.698444	3883.605043	23.905869
120.751316	3893.991828	23.910887
120.833063	3890.848695	23.915904
120.859861	3888.573719	23.920922
120.943611	3890.666610	23.925939
121.307885	3899.070399	23.930957
121.042734	3919.881283	23.935975
121.316368	3916.111147	23.940992
121.616809	3919.121412	23.946010
121.533494	3926.222758	23.951027
121.852273	3929.124480	23.956045
121.875396	3945.140783	23.961063
122.253110	3955.452280	23.966080
122.568549	3934.468432	23.971098
122.158252	3936.935884	23.976115
122.733293	3937.106605	23.981133
122.651148	3949.750446	23.986151
123.032052	3961.275630	23.991168
122.960141	3975.909594	23.996186
122.774233	3972.401602	24.001203
123.313146	3960.514148	24.006221
123.007215	3975.987592	24.011239
123.019794	3971.080226	24.016256
123.272893	3983.160024	24.021274
123.340490	3995.413007	24.026291
123.807969	3984.877144	24.031309
123.615991	3989.611753	24.036327
123.829674	4009.242027	24.041344
124.226579	4017.204648	24.046362
124.160672	4019.560088	24.051379
124.128887	4010.931568	24.056397
124.101795	4021.279681	24.061415
124.095854	4025.028016	24.066432
124.556179	4048.238182	24.071450
124.587361	4061.907128	24.076467
124.832402	4050.888665	24.081485
125.132724	4051.863076	24.086503
124.809653	4055.128367	24.091520
125.098901	4063.019427	24.096538
125.297339	4075.850088	24.101555
125.629708	4073.442308	24.106573
125.442109	4081.081447	24.111591
125.528371	4075.235067	24.116608
125.636577	4091.175649	24.121626
125.880063	4102.556314	24.126643
126.575763	4095.848173	24.131661
126.592420	4092.079116	24.136679
126.579617	4091.592219	24.141696
126.906265	4091.493344	24.146714
126.668801	4097.063485	24.151731
126.923792	4089.741526	24.156749
127.461490	4111.207834	24.161767
127.450968	4131.122956	24.166784
127.488899	4121.206819	24.171802
127.425587	4118.036820	24.176819
127.229277	4126.465641	24.181837
127.609543	4120.839573	24.186855
127.586374	4122.697396	24.191872
127.404482	4123.276667	24.196890
127.678428	4141.317560	24.201907
127.680615	4141.976657	24.206925
127.642043	4146.493831	24.211943
127.906130	4167.384534	24.216960
128.361781	4170.018793	24.221978
128.265625	4175.256545	24.226995
128.545407	4190.819257	24.232013
129.072675	4197.239496	24.237031
128.968802	4192.856050	24.242048
129.679269	4191.470078	24.247066
128.862670	4196.822154	24.252083
129.214020	4204.158118	24.257101
129.247588	4211.349734	24.262119
129.558979	4224.514627	24.267136
129.959475	4220.375802	24.272154
129.702324	4221.093503	24.277171
129.870044	4230.213053	24.282189
130.047155	4245.463241	24.287207
130.190334	4258.044509	24.292224
130.348788	4253.210201	24.297242
130.534478	4263.097704	24.302259
130.830313	4255.297636	24.307277
131.179337	4279.206887	24.312295
130.994968	4283.532826	24.317312
131.150633	4282.924380	24.322330
131.184965	4284.505778	24.327347
131.529936	4287.198900	24.332365
131.539761	4282.966335	24.337383
131.427193	4296.843893	24.342400
132.140895	4288.663724	24.347418
131.780354	4307.325028	24.352435
131.986614	4297.182530	24.357453
132.171483	4298.456364	24.362471
132.010564	4307.014875	24.367488
132.435286	4311.671698	24.372506
132.698479	4331.703669	24.377523
132.910462	4341.522702	24.382541
133.251162	4322.379141	24.387559
133.202992	4331.575763	24.392576
133.518403	4331.979559	24.397594
133.236894	4337.463358	24.402611
133.599724	4329.010416	24.407629
133.309540	4339.049437	24.412647
133.228631	4333.269955	24.417664
133.419487	4337.880385	24.422682
133.299292	4348.361428	24.427699
133.657103	4356.737399	24.432717
133.302462	4353.730455	24.437735
133.848244	4375.387536	24.442752
134.067224	4386.379916	24.447770
133.953948	4388.602285	24.452787
134.186247	4389.594258	24.457805
134.407411	4408.411549	24.462823
134.507774	4422.246949	24.467840
134.690485	4409.931762	24.472858
135.065681	4440.010134	24.477875
134.910554	4441.063370	24.482893
135.151032	4441.435454	24.487911
135.322254	4461.798950	24.492928
135.617116	4469.166422	24.497946
135.915553	4466.982707	24.502963
135.958799	4456.651280	24.507981
136.127277	4463.358094	24.512999
136.281319	4464.579945	24.518016
136.247634	4486.824297	24.523034
136.702327	4500.169302	24.528051
136.510240	4499.636814	24.533069
136.679915	4496.897955	24.538087
136.716488	4504.947534	24.543104
137.344506	4507.645110	24.548122
137.131638	4525.236536	24.553139
137.687747	4518.223702	24.558157
137.746255	4521.353594	24.563175
137.560932	4513.116331	24.568192
137.814546	4512.996844	24.573210
137.818418	4530.509153	24.578227
137.924115	4541.673915	24.583245
138.461368	4544.147504	24.588263
138.363610	4562.621587	24.593280
138.402856	4548.488138	24.598298
138.713939	4553.556358	24.603315
138.869782	4560.642886	24.608333
139.132040	4556.974091	24.613351
138.788086	4580.068321	24.618368
139.178565	4571.098835	24.623386
139.060118	4581.787240	24.628403
139.005460	4585.223658	24.633421
139.438323	4608.750246	24.638439
139.458482	4602.858288	24.643456
139.763310	4613.589383	24.648474
139.809590	4628.248921	24.653491
139.839551	4628.184106	24.658509
140.500790	4627.967342	24.663527
140.342789	4636.229860	24.668544
140.650240	4631.536576	24.673562
140.842663	4642.375246	24.678579
140.635398	4652.107831	24.683597
141.239720	4652.554064	24.688615
141.003326	4657.106828	24.693632
141.248457	4645.670184	24.698650
141.219359	4672.415163	24.703667
141.495966	4676.599290	24.708685
141.546504	4677.490202	24.713703
141.668902	4688.806259	24.718720
141.577478	4692.271219	24.723738
142.337915	4695.110742	24.728755
141.954824	4715.773262	24.733773
142.819333	4703.142419	24.738791
142.526292	4718.120726	24.743808
142.426161	4720.461846	24.748826
142.747154	4707.662910	24.753843
142.892713	4723.975162	24.758861
143.036366	4732.993069	24.763879
143.002237	4738.091616	24.768896
143.096878	4724.655210	24.773914
143.360367	4737.584339	24.778931
143.295839	4752.472162	24.783949
143.562431	4767.380885	24.788967
143.695146	4777.702307	24.793984
144.140849	4772.569568	24.799002
144.073271	4763.444536	24.804019
144.235755	4790.065534	24.809037
144.619703	4780.830450	24.814055
144.559929	4797.104652	24.819072
144.518049	4790.722439	24.824090
144.829527	4805.391478	24.829107
144.794333	4816.874624	24.834125
145.056203	4810.945012	24.839143
144.756048	4817.289216	24.844160
145.225245	4835.102966	24.849178
145.662649	4835.549618	24.854195
145.709831	4845.663545	24.859213
145.870738	4852.406033	24.864231
146.088356	4864.849103	24.869248
146.521329	4862.469468	24.874266
146.320181	4867.058993	24.879283
146.666184	4869.190974	24.884301
147.082353	4872.549267	24.889319
146.778147	4871.663604	24.894336
147.126730	4876.887166	24.899354
147.021000	4895.025528	24.904371
146.917839	4907.042851	24.909389
147.297781	4883.525585	24.914407
147.502197	4909.612646	24.919424
147.456451	4923.720686	24.924442
147.864202	4921.700754	24.929459
147.575006	4919.069141	24.934477
147.965231	4929.287086	24.939495
148.273046	4953.015187	24.944512
148.333343	4953.441074	24.949530
148.476609	4954.780898	24.954547
148.560078	4989.137276	24.959565
148.964995	4970.735142	24.964583
148.897737	4983.712431	24.969600
149.120157	4984.115469	24.974618
149.724131	4995.317528	24.979635
149.345803	4993.466058	24.984653
149.743506	4989.814550	24.989671
149.869541	4998.175616	24.994688
149.630499	5007.041146	24.999706
150.106956	5020.558217	25.004723
150.657574	5017.159023	25.009741
150.749867	5009.830838	25.014759
150.960060	5014.128402	25.019776
151.319411	5011.004143	25.024794
151.430523	5010.479812	25.029811
151.072017	5023.132386	25.034829
151.608517	5008.676572	25.039847
151.325764	5017.589098	25.044864
151.332517	5014.193932	25.049882
151.438923	5039.570956	25.054899
151.421634	5047.467887	25.059917
151.564858	5032.332469	25.064935
151.706138	5065.957740	25.069952
152.080509	5076.350072	25.074970
152.384705	5076.302548	25.079987
152.052792	5079.839222	25.085005
152.318984	5100.149274	25.090023
152.434388	5108.075890	25.095040
152.574918	5119.612908	25.100058
152.750239	5115.980398	25.105075
153.137602	5149.006861	25.110093
153.423056	5142.998022	25.115111
153.228573	5148.612226	25.120128
153.458925	5138.278177	25.125146
153.845220	5143.973208	25.130163
154.072838	5149.554286	25.135181
154.161093	5156.302217	25.140199
154.090167	5162.424413	25.145216
154.433606	5180.876727	25.150234
154.803577	5173.763243	25.155251
154.826435	5196.874160	25.160269
155.067172	5187.352624	25.165287
155.014095	5182.658110	25.170304
155.154319	5194.981147	25.175322
155.644054	5203.994906	25.180339
155.433371	5222.059640	25.185357
155.878117	5213.969503	25.190375
156.072422	5218.804453	25.195392
155.989812	5205.721760	25.200410
155.952838	5231.989417	25.205427
155.862954	5242.336508	25.210445
156.435948	5241.654348	25.215463
156.216645	5258.460957	25.220480
156.716712	5269.642190	25.225498
157.026040	5258.014158	25.230515
156.904469	5272.782359	25.235533
157.008393	5288.880796	25.240551
157.441420	5289.326218	25.245568
157.298923	5293.800651	25.250586
157.947097	5302.668590	25.255603
157.862284	5320.285424	25.260621
158.131132	5320.677257	25.265639
158.573929	5302.825627	25.270656
158.470909	5313.982509	25.275674
158.995260	5309.698514	25.280691
159.043154	5306.332318	25.285709
158.960928	5330.209701	25.290727
158.963543	5335.311427	25.295744
159.123072	5327.617219	25.300762
159.505407	5336.151104	25.305779
159.447456	5340.429276	25.310797
159.846125	5355.397457	25.315815
159.940823	5357.160352	25.320832
159.923340	5367.260101	25.325850
159.936564	5357.560280	25.330867
160.098332	5383.701248	25.335885
160.040082	5378.886255	25.340903
160.612134	5389.199279	25.345920
160.587584	5404.279565	25.350938
160.622622	5418.800740	25.355955
160.755744	5439.027301	25.360973
160.959775	5430.724826	25.365991
161.376211	5448.052659	25.371008
161.040712	5457.313167	25.376026
161.603542	5458.693961	25.381043
161.723739	5479.415685	25.386061
161.792494	5481.669162	25.391079
162.161982	5488.677107	25.396096
162.556554	5499.681030	25.401114
162.841614	5507.340023	25.406131
162.909874	5512.889681	25.411149
163.391356	5503.579784	25.416167
163.369231	5504.803264	25.421184
163.264404	5505.648232	25.426202
163.363042	5500.808855	25.431219
163.309873	5506.112398	25.436237
163.602417	5524.071494	25.441255
163.504508	5527.162070	25.446272
163.617773	5532.614917	25.451290
163.903008	5537.465262	25.456307
163.988772	5565.813867	25.461325
164.399141	5566.891079	25.466343
164.747193	5573.613196	25.471360
164.775128	5571.216905	25.476378
164.837731	5581.201972	25.481395
164.727400	5602.159218	25.486413
164.791169	5598.287513	25.491431
165.095505	5618.110768	25.496448
165.112117	5630.642787	25.501466
165.663361	5639.100105	25.506483
165.474588	5659.268309	25.511501
165.745949	5661.599769	25.516519
166.322589	5661.491087	25.521536
166.280065	5680.256616	25.526554
166.523090	5680.340477	25.531571
166.737267	5688.176648	25.536589
167.108215	5693.309378	25.541607
167.474489	5694.704952	25.546624
167.506890	5706.225225	25.551642
167.765246	5701.536981	25.556659
167.667173	5702.646235	25.561677
167.457249	5708.401004	25.566695
168.196796	5719.211843	25.571712
168.016522	5739.544518	25.576730
168.686641	5727.319443	25.581747
168.058351	5735.024718	25.586765
168.371335	5741.436908	25.591783
168.658014	5749.521011	25.596800
168.669507	5774.902309	25.601818
168.690847	5783.452772	25.606835
168.853461	5797.825642	25.611853
169.131497	5804.051477	25.616871
169.584578	5812.027398	25.621888
169.687845	5818.952294	25.626906
169.792271	5833.349773	25.631923
170.207238	5841.164264	25.636941
170.057976	5850.781692	25.641959
170.604142	5848.184755	25.646976
170.543736	5866.360459	25.651994
171.111047	5875.638999	25.657011
171.085071	5884.922643	25.662029
171.076835	5882.283425	25.667047
171.274187	5890.484344	25.672064
171.499670	5905.065855	25.677082
171.569647	5910.566150	25.682100
171.949222	5904.552104	25.687117
172.214269	5927.285840	25.692135
172.255153	5932.000276	25.697152
171.927677	5944.981585	25.702170
172.549575	5944.110976	25.707188
172.977297	5945.974449	25.712205
172.988401	5963.671448	25.717223
173.281321	5957.858342	25.722240
173.593229	5964.961462	25.727258
173.432429	5970.735380	25.732276
173.497668	5985.641915	25.737293
173.369578	5988.950200	25.742311
173.969369	5992.309114	25.747328
173.871229	6018.015267	25.752346
174.371602	6023.089314	25.757364
174.558277	6034.108276	25.762381
174.398014	6028.885854	25.767399
174.297883	6047.425869	25.772416
174.432072	6061.281544	25.777434
174.736516	6053.285039	25.782452
175.067152	6076.565726	25.787469
175.256040	6094.098041	25.792487
175.528549	6091.532894	25.797504
175.909923	6105.082368	25.802522
176.004322	6120.677243	25.807540
176.174801	6116.463315	25.812557
175.980867	6116.748926	25.817575
176.633550	6125.581154	25.822592
176.597172	6139.168967	25.827610
176.762420	6152.746316	25.832628
176.756523	6144.653772	25.837645
176.844506	6157.560312	25.842663
177.493886	6151.674063	25.847680
177.328129	6173.861909	25.852698
177.815839	6175.227227	25.857716
178.116359	6178.596252	25.862733
178.002007	6187.494609	25.867751
178.739599	6178.110499	25.872768
178.714552	6183.121779	25.877786
179.010916	6194.699209	25.882804
179.416357	6195.662301	25.887821
179.395891	6204.233290	25.892839
179.808840	6190.002750	25.897856
179.879604	6193.361701	25.902874
180.006224	6191.963360	25.907892
180.478590	6183.175132	25.912909
180.251769	6195.415483	25.917927
180.126784	6197.192325	25.922944
180.023670	6210.700660	25.927962
180.202050	6225.707648	25.932980
180.349658	6229.104312	25.937997
180.414648	6247.576329	25.943015
180.920072	6252.664580	25.948032
180.726289	6267.351142	25.953050
180.991501	6288.584321	25.958068
181.341473	6286.724583	25.963085
181.423591	6296.430059	25.968103
182.009653	6321.908680	25.973120
181.905815	6318.373209	25.978138
182.020502	6340.147957	25.983156
182.371863	6345.735009	25.988173
182.540262	6353.273904	25.993191
182.859268	6361.422680	25.998208
182.838208	6379.803538	26.003226
182.784175	6393.728408	26.008244
183.371486	6393.773111	26.013261
183.359544	6411.067258	26.018279
183.487718	6400.635463	26.023296
183.767024	6420.568614	26.028314
183.810115	6427.672257	26.033332
184.168416	6441.524317	26.038349
184.177942	6457.795091	26.043367
184.600070	6465.953660	26.048384
184.923312	6478.511298	26.053402
185.112329	6502.549228	26.058420
185.318616	6486.737297	26.063437
185.333624	6487.066359	26.068455
185.955559	6503.720341	26.073472
185.765900	6535.062439	26.078490
185.858253	6525.762683	26.083508
186.132654	6525.130600	26.088525
185.941815	6538.849023	26.093543
186.327328	6554.121373	26.098560
186.438209	6558.119569	26.103578
186.428529	6564.668104	26.108596
187.186739	6589.339824	26.113613
187.054410	6594.598927	26.118631
187.485992	6588.125547	26.123648
187.367936	6598.491179	26.128666
187.472308	6615.216617	26.133684
187.890984	6611.115124	26.138701
187.982279	6628.879165	26.143719
188.201291	6638.026694	26.148736
188.484684	6638.097199	26.153754
188.471122	6650.208947	26.158772
188.750453	6658.343957	26.163789
188.524881	6666.127659	26.168807
188.932698	6675.620469	26.173824
188.994051	6702.154316	26.178842
189.151239	6710.778921	26.183860
189.913912	6722.025312	26.188877
189.679641	6728.985903	26.193895
190.137986	6740.210921	26.198912
190.471794	6749.505724	26.203930
190.461812	6761.922541	26.208948
190.884453	6761.690455	26.213965
191.035196	6782.947941	26.218983
191.235626	6797.024865	26.224000
191.320211	6785.814813	26.229018
191.678519	6806.683631	26.234036
191.885812	6807.499150	26.239053
192.051254	6811.259214	26.244071
192.444290	6811.973163	26.249088
192.289624	6824.973896	26.254106
192.853288	6855.171474	26.259124
192.911484	6836.208964	26.264141
192.678525	6850.085830	26.269159
193.330691	6849.939469	26.274176
193.587406	6861.801955	26.279194
193.546447	6865.140130	26.284212
193.763415	6860.848230	26.289229
194.113291	6876.043299	26.294247
194.436394	6892.659649	26.299264
194.637118	6884.657022	26.304282
194.403953	6878.791889	26.309300
194.811993	6898.470467	26.314317
194.726636	6918.159710	26.319335
194.868928	6914.992188	26.324352
195.242281	6930.581155	26.329370
195.356260	6941.352079	26.334388
195.863141	6941.758184	26.339405
196.027553	6946.448577	26.344423
195.961779	6974.972826	26.349440
196.074058	6970.498937	26.354458
196.215545	6977.781890	26.359476
196.754818	6991.808518	26.364493
196.718863	7007.932222	26.369511
197.064599	7012.542271	26.374528
197.379345	7022.735863	26.379546
197.432742	7029.823111	26.384564
197.698683	7022.625572	26.389581
197.788551	7041.925306	26.394599
198.045891	7053.487766	26.399616
198.103054	7053.279045	26.404634
198.288150	7074.054763	26.409652
198.755902	7085.703769	26.414669
198.856394	7091.134854	26.419687
198.779008	7096.516573	26.424704
199.387311	7109.398569	26.429722
199.061797	7126.964259	26.434740
199.096158	7124.386314	26.439757
199.262705	7148.444695	26.444775
199.737178	7160.099734	26.449792
200.060289	7169.719464	26.454810
199.980301	7194.000579	26.459828
200.523812	7187.940849	26.464845
200.736842	7189.628087	26.469863
200.902332	7211.788654	26.474880
201.011552	7215.773903	26.479898
201.203533	7229.622635	26.484916
201.827579	7226.621970	26.489933
202.162521	7233.917972	26.494951
202.367863	7228.480376	26.499968
202.420635	7230.153143	26.504986
202.542555	7232.401239	26.510004
202.696287	7249.783134	26.515021
202.882437	7261.967892	26.520039
203.019006	7249.340709	26.525056
203.340860	7262.785243	26.530074
203.414756	7275.735982	26.535092
203.803529	7279.449808	26.540109
203.808715	7275.566106	26.545127
204.320534	7288.898942	26.550144
204.153053	7300.613683	26.555162
204.507236	7311.544434	26.560180
204.917332	7306.188758	26.565197
204.720550	7321.877826	26.570215
205.051001	7331.849285	26.575232
205.532751	7325.502784	26.580250
204.996897	7349.527880	26.585268
205.801620	7363.056540	26.590285
205.820520	7363.856747	26.595303
206.216833	7385.117003	26.600320
206.770362	7380.776445	26.605338
206.509457	7393.999974	26.610356
206.462021	7390.598284	26.615373
206.703117	7409.609637	26.620391
207.144659	7411.675785	26.625408
207.439150	7413.440163	26.630426
207.443763	7444.481034	26.635444
207.282953	7450.538241	26.640461
208.048818	7460.262207	26.645479
208.098856	7482.311487	26.650496
208.453106	7481.696893	26.655514
208.304170	7494.269562	26.660532
208.866345	7501.984167	26.665549
209.181548	7508.655839	26.670567
208.921258	7521.577721	26.675584
209.448723	7538.602047	26.680602
209.058061	7541.223140	26.685620
209.521945	7556.871806	26.690637
209.852818	7573.539574	26.695655
209.846416	7594.534279	26.700672
210.592948	7588.372333	26.705690
210.460679	7599.877487	26.710708
210.641166	7610.790676	26.715725
210.789486	7623.971987	26.720743
210.972792	7645.255185	26.725760
211.650309	7650.730535	26.730778
211.629980	7663.226956	26.735796
211.487822	7674.755851	26.740813
211.754958	7688.061718	26.745831
212.207842	7712.432014	26.750848
212.747924	7717.357499	26.755866
212.655501	7733.736221	26.760884
212.364485	7748.645790	26.765901
212.614447	7748.825793	26.770919
212.802535	7779.416421	26.775936
213.352157	7776.892647	26.780954
213.223265	7808.105149	26.785972
213.758442	7808.691698	26.790989
214.103957	7834.381066	26.796007
214.148986	7844.607940	26.801024
214.747576	7841.740539	26.806042
215.071782	7849.111063	26.811060
215.993521	7836.607300	26.816077
216.701913	7833.528793	26.821095
216.424042	7826.283693	26.826112
216.658072	7815.918538	26.831130
216.555243	7819.096224	26.836148
216.866106	7806.266524	26.841165
216.874796	7813.944349	26.846183
216.687244	7832.496966	26.851200
216.992277	7831.046951	26.856218
217.060204	7834.910010	26.861236
216.951087	7847.932412	26.866253
217.273764	7865.265807	26.871271
217.496746	7880.236286	26.876288
217.972008	7889.504456	26.881306
217.603460	7912.061412	26.886324
217.829103	7924.911212	26.891341
218.354216	7936.312724	26.896359
218.299907	7945.865328	26.901376
218.757336	7958.602824	26.906394
218.839549	7978.061704	26.911412
218.683498	7999.172248	26.916429
219.326647	8012.846310	26.921447
219.520707	8032.173359	26.926464
219.851815	8048.517087	26.931482
219.770065	8060.177267	26.936500
220.068408	8076.193269	26.941517
220.513168	8088.082320	26.946535
220.330383	8114.366664	26.951552
221.007023	8119.639903	26.956570
221.175714	8143.667940	26.961588
221.695583	8161.440873	26.966605
221.889205	8162.020071	26.971623
221.639524	8194.487515	26.976640
222.297094	8205.427048	26.981658
222.410258	8202.503525	26.986676
222.748233	8228.823316	26.991693
223.091061	8220.416897	26.996711
222.936374	8244.230717	27.001728
223.410971	8247.846318	27.006746
223.670147	8261.148471	27.011764
223.926912	8276.193295	27.016781
224.014399	8283.210099	27.021799
224.259041	8301.026299	27.026816
224.446972	8309.916075	27.031834
224.830230	8326.199490	27.036852
225.051348	8343.055547	27.041869
225.298434	8345.077548	27.046887
225.309901	8360.326023	27.051904
225.535286	8372.627241	27.056922
226.069334	8371.166122	27.061940
226.011580	8397.712254	27.066957
226.315285	8402.120932	27.071975
226.478426	8406.239351	27.076992
226.705397	8425.370832	27.082010
226.950676	8436.181731	27.087028
227.268787	8445.822760	27.092045
227.621065	8449.532657	27.097063
227.629476	8464.317810	27.102080
227.677014	8476.480723	27.107098
228.287471	8501.544540	27.112116
228.295664	8494.060471	27.117133
228.761396	8511.768704	27.122151
228.935734	8531.711628	27.127168
229.072810	8520.576742	27.132186
229.538888	8531.398486	27.137204
229.305233	8552.936106	27.142221
229.822176	8552.901090	27.147239
229.472814	8555.898322	27.152256
230.321477	8565.746351	27.157274
230.692299	8569.699749	27.162292
230.416657	8581.958671	27.167309
231.110691	8587.043309	27.172327
231.169694	8589.476067	27.177344
231.293686	8600.713549	27.182362
232.074738	8622.613709	27.187380
231.931903	8635.779380	27.192397
232.059929	8633.266056	27.197415
232.060203	8647.329654	27.202432
232.171363	8669.097957	27.207450
232.957535	8665.739429	27.212468
232.656999	8682.287415	27.217485
233.070884	8693.898467	27.222503
233.022700	8709.760482	27.227520
233.559892	8712.804247	27.232538
233.788574	8728.088077	27.237556
233.724551	8754.579130	27.242573
234.198701	8754.146326	27.247591
234.663447	8773.056204	27.252608
234.913285	8783.026148	27.257626
235.237084	8796.169204	27.262644
235.463558	8808.752566	27.267661
235.716312	8813.669947	27.272679
235.993438	8832.273772	27.277696
236.228512	8843.924716	27.282714
236.221874	8847.771199	27.287732
236.454552	8850.002803	27.292749
236.633728	8863.902343	27.297767
236.369361	8882.936752	27.302784
236.946253	8900.972056	27.307802
237.727012	8909.033264	27.312820
237.691406	8944.674275	27.317837
238.244107	8937.931032	27.322855
238.216313	8958.550630	27.327872
238.632205	8964.276828	27.332890
238.743734	8972.761344	27.337908
238.829275	8979.236857	27.342925
239.322270	8989.427479	27.347943
239.256906	9003.624326	27.352960
239.324546	9018.441956	27.357978
239.446883	9037.608792	27.362996
239.919662	9059.015415	27.368013
240.135224	9056.307972	27.373031
240.422444	9086.053742	27.378048
240.758716	9093.047130	27.383066
241.034438	9094.692712	27.388084
241.051907	9127.909544	27.393101
241.567907	9138.590339	27.398119
241.874077	9159.364545	27.403136
242.049000	9169.529064	27.408154
242.060814	9165.154652	27.413172
242.545138	9169.399010	27.418189
242.504669	9192.033542	27.423207
242.575065	9206.178995	27.428224
243.160070	9218.958659	27.433242
243.479870	9244.871178	27.438260
243.479515	9247.793547	27.443277
244.124435	9262.118246	27.448295
244.686666	9267.709314	27.453312
244.359158	9268.107626	27.458330
244.703480	9283.928996	27.463348
244.921823	9289.116087	27.468365
245.499957	9291.308797	27.473383
245.656861	9314.774204	27.478400
245.630268	9328.481291	27.483418
245.996416	9332.884641	27.488436
245.926769	9338.603760	27.493453
246.086343	9358.025557	27.498471
246.604498	9358.780403	27.503488
246.697374	9377.389313	27.508506
246.828920	9391.527192	27.513524
246.765731	9399.558731	27.518541
247.277273	9412.564942	27.523559
247.750530	9425.959523	27.528576
247.771426	9446.346426	27.533594
248.051219	9438.976156	27.538612
248.214862	9473.566148	27.543629
248.886159	9472.147639	27.548647
248.914021	9496.624774	27.553664
249.335510	9497.413715	27.558682
249.271955	9508.864785	27.563700
249.660958	9532.771090	27.568717
249.711122	9545.105318	27.573735
250.183686	9564.337020	27.578752
250.281511	9592.960252	27.583770
250.895068	9597.221974	27.588788
250.971848	9612.207216	27.593805
250.974834	9627.895485	27.598823
251.218187	9648.048966	27.603840
251.333326	9657.125608	27.608858
251.906445	9680.003688	27.613876
252.058860	9706.780376	27.618893
252.519715	9710.972044	27.623911
252.636896	9736.693555	27.628928
252.806654	9750.882942	27.633946
253.177472	9762.880785	27.638964
253.467997	9773.010049	27.643981
254.148687	9766.309121	27.648999
254.791175	9779.924960	27.654016
255.224962	9785.027782	27.659034
255.366543	9798.934351	27.664052
255.583135	9801.065558	27.669069
255.967542	9791.527375	27.674087
255.991854	9802.920026	27.679104
256.335773	9820.345002	27.684122
256.739386	9832.329602	27.689140
256.500186	9838.973336	27.694157
256.705704	9827.959356	27.699175
256.911467	9848.728995	27.704192
256.844088	9856.419586	27.709210
257.273368	9864.218755	27.714228
257.273869	9883.672988	27.719245
257.507153	9902.223867	27.724263
257.720499	9915.643685	27.729280
257.862235	9934.094718	27.734298
258.482237	9958.244717	27.739316
258.547164	9970.819454	27.744333
258.634809	9976.034665	27.749351
259.042117	9996.438779	27.754368
259.199673	10024.669295	27.759386
259.663748	10027.515865	27.764404
259.812375	10059.725157	27.769421
260.027046	10065.094287	27.774439
260.620838	10079.939411	27.779456
260.880412	10091.775491	27.784474
261.061155	10103.980659	27.789492
261.423911	10112.939453	27.794509
261.805602	10129.505413	27.799527
262.355214	10132.977510	27.804544
262.356594	10137.410627	27.809562
263.103075	10142.196438	27.814580
263.179050	10163.504684	27.819597
263.232985	10149.437059	27.824615
263.484305	10148.314749	27.829632
263.623692	10172.244349	27.834650
263.970246	10183.791996	27.839668
263.617535	10186.660104	27.844685
264.131210	10222.622845	27.849703
264.255806	10232.030678	27.854720
264.216378	10239.392287	27.859738
264.614407	10252.546343	27.864756
264.726181	10281.700230	27.869773
264.754656	10303.980705	27.874791
265.410166	10310.029379	27.879808
265.535795	10338.569005	27.884826
266.120393	10354.002773	27.889844
266.204426	10364.379221	27.894861
266.824910	10379.251725	27.899879
267.004269	10384.967104	27.904896
267.219781	10414.548382	27.909914
268.021168	10412.909794	27.914932
268.255461	10426.453409	27.919949
268.124171	10427.812678	27.924967
268.709415	10447.694843	27.929984
268.559893	10462.667855	27.935002
269.688466	10460.722340	27.940020
269.947558	10479.042755	27.945037
270.007341	10484.454159	27.950055
270.626562	10467.193853	27.955072
270.794064	10469.867356	27.960090
270.884217	10488.804930	27.965108
271.529621	10499.059574	27.970125
271.700975	10501.629251	27.975143
271.813901	10501.983183	27.980160
271.714498	10510.106340	27.985178
271.919751	10516.079021	27.990196
272.214385	10520.033683	27.995213
271.964617	10562.716021	28.000231
272.223671	10565.497305	28.005248
272.329055	10578.870922	28.010266
272.552394	10609.976364	28.015284
273.144550	10629.280976	28.020301
273.322439	10652.837053	28.025319
273.430603	10675.053674	28.030336
273.793496	10693.080682	28.035354
274.044664	10713.865215	28.040372
274.499987	10729.081226	28.045389
274.688401	10753.567635	28.050407
275.118590	10775.345977	28.055424
274.847474	10795.281826	28.060442
275.454350	10806.625425	28.065460
276.297995	10814.572453	28.070477
276.613397	10837.699595	28.075495
277.203980	10849.858893	28.080512
277.427220	10851.514121	28.085530
277.631014	10862.573009	28.090548
278.000596	10870.480219	28.095565
278.374153	10876.186536	28.100583
278.555415	10884.132744	28.105600
278.549921	10899.937100	28.110618
278.884202	10910.069314	28.115636
278.947189	10923.368295	28.120653
278.928458	10929.615255	28.125671
279.585042	10947.497921	28.130688
279.457486	10973.753426	28.135706
279.997911	10985.186121	28.140724
280.247943	11003.249455	28.145741
280.062539	11028.314823	28.150759
280.618062	11033.115126	28.155776
280.901121	11056.225082	28.160794
281.130196	11068.788531	28.165812
281.271410	11086.153058	28.170829
281.105877	11116.136543	28.175847
281.827557	11110.231042	28.180864
281.977906	11137.318490	28.185882
282.202166	11168.962133	28.190900
282.749671	11173.503047	28.195917
282.642365	11195.820586	28.200935
283.467451	11224.301379	28.205952
283.848710	11218.358333	28.210970
284.507364	11242.370757	28.215988
285.138163	11251.273307	28.221005
284.989563	11255.276170	28.226023
285.669220	11265.622550	28.231040
285.479353	11286.933669	28.236058
285.786464	11278.391328	28.241076
286.253283	11286.110155	28.246093
286.760142	11320.732524	28.251111
286.693441	11317.188223	28.256128
286.791688	11329.927111	28.261146
287.231231	11334.399250	28.266164
287.754667	11345.501775	28.271181
287.726549	11361.192942	28.276199
287.997014	11360.734649	28.281216
287.985858	11386.072725	28.286234
288.264362	11391.903647	28.291252
288.597783	11420.246222	28.296269
288.929483	11446.104417	28.301287
289.325099	11452.498983	28.306304
289.483151	11473.658335	28.311322
289.373658	11498.010753	28.316340
290.180951	11516.884634	28.321357
290.369584	11544.253204	28.326375
290.475048	11568.987751	28.331392
290.327549	11580.231219	28.336410
290.957768	11605.014631	28.341428
291.325175	11624.860986	28.346445
291.664136	11658.513671	28.351463
292.164037	11672.498175	28.356480
292.608562	11683.774685	28.361498
292.534643	11701.670164	28.366516
293.130729	11723.093872	28.371533
293.549718	11750.135609	28.376551
293.714256	11746.827169	28.381568
294.090219	11764.230065	28.386586
294.725152	11772.658748	28.391604
295.636306	11784.514488	28.396621
295.395435	11799.336031	28.401639
296.250576	11792.570791	28.406656
296.463686	11797.512980	28.411674
296.671312	11803.759124	28.416692
296.536030	11816.546432	28.421709
296.521103	11822.440957	28.426727
296.853533	11836.071181	28.431744
297.051318	11847.038779	28.436762
296.882817	11870.350559	28.441780
297.850825	11885.247416	28.446797
297.857414	11914.906946	28.451815
298.146816	11915.715478	28.456832
298.476334	11941.088745	28.461850
298.717504	11958.294318	28.466868
298.616870	11974.947390	28.471885
299.054837	11995.548311	28.476903
299.642270	12020.884610	28.481920
299.731044	12036.524823	28.486938
300.144045	12060.247383	28.491956
300.649958	12062.616294	28.496973
300.684290	12075.399420	28.501991
301.145280	12088.513864	28.507008
301.334845	12111.944100	28.512026
301.397570	12113.872571	28.517044
301.961101	12127.985619	28.522061
301.879934	12147.623109	28.527079
302.277172	12158.615481	28.532096
302.632829	12182.292546	28.537114
302.825869	12206.511755	28.542132
303.390176	12230.285990	28.547149
303.323365	12260.653941	28.552167
303.760285	12274.263335	28.557184
304.074232	12300.635570	28.562202
304.434756	12312.169055	28.567220
304.599448	12331.890630	28.572237
305.119464	12361.637122	28.577255
305.457385	12373.345347	28.582272
306.105457	12396.648253	28.587290
306.022458	12431.160108	28.592308
306.406705	12438.603209	28.597325
306.345538	12456.914977	28.602343
306.910737	12478.719025	28.607360
307.454758	12498.539646	28.612378
307.698703	12528.120910	28.617396
308.201816	12527.762028	28.622413
308.561811	12560.174623	28.627431
308.988489	12573.081623	28.632448
309.433241	12587.586566	28.637466
309.509316	12589.037813	28.642484
309.874964	12605.564868	28.647501
309.939974	12622.827040	28.652519
310.290134	12642.120488	28.657536
310.510856	12668.360609	28.662554
310.751547	12689.506330	28.667572
311.091779	12700.915026	28.672589
311.204243	12723.985444	28.677607
311.861445	12746.228464	28.682624
312.199591	12765.260898	28.687642
312.386451	12781.664825	28.692660
313.190318	12804.630590	28.697677
313.480323	12808.707920	28.702695
313.870502	12828.527576	28.707712
314.121768	12844.167727	28.712730
314.245520	12863.832899	28.717748
314.492454	12866.927798	28.722765
314.710790	12886.282709	28.727783
314.443361	12897.990476	28.732800
315.265610	12924.013457	28.737818
315.601967	12944.494504	28.742836
316.054725	12959.000036	28.747853
316.300420	12983.403953	28.752871
316.680293	12998.148469	28.757888
317.124424	13020.633491	28.762906
317.140224	13038.252478	28.767924
317.872614	13044.707077	28.772941
317.682384	13071.293075	28.777959
318.198083	13085.033537	28.782976
318.872056	13095.605803	28.787994
319.061434	13105.339466	28.793012
319.437096	13125.199704	28.798029
319.537610	13143.454023	28.803047
320.120235	13161.222170	28.808064
320.283117	13176.068877	28.813082
320.392720	13188.196750	28.818100
321.198235	13197.898015	28.823117
321.324250	13221.469575	28.828135
321.635986	13240.417114	28.833152
322.204067	13243.287273	28.838170
322.296541	13259.075394	28.843188
322.698690	13259.199608	28.848205
322.715188	13277.356079	28.853223
323.087784	13299.326999	28.858240
323.322847	13319.153974	28.863258
323.170191	13324.472216	28.868276
323.407384	13335.340559	28.873293
323.721641	13379.459374	28.878311
323.757655	13396.391520	28.883328
324.144693	13426.741835	28.888346
324.369176	13449.862542	28.893364
324.885513	13471.906073	28.898381
325.251333	13503.834256	28.903399
325.665877	13523.409643	28.908416
326.113574	13536.071271	28.913434
326.388770	13583.325056	28.918452
326.935898	13587.390048	28.923469
327.277287	13620.349920	28.928487
327.479685	13646.363012	28.933504
328.427505	13652.632568	28.938522
328.445715	13685.713723	28.943540
329.032214	13693.202785	28.948557
329.403931	13725.128854	28.953575
329.564956	13729.426279	28.958592
329.899618	13738.507571	28.963610
330.012945	13776.855345	28.968628
330.952665	13784.590232	28.973645
331.498079	13796.690687	28.978663
331.488744	13823.093601	28.983680
331.757879	13827.626901	28.988698
332.134927	13838.745096	28.993716
332.476574	13846.805735	28.998733
332.629125	13850.888704	29.003751
332.968032	13889.858176	29.008768
333.642059	13903.628334	29.013786
333.354647	13926.774405	29.018804
333.737489	13929.755660	29.023821
334.253583	13959.858734	29.028839
334.483587	13979.094837	29.033856
335.223621	14000.842122	29.038874
335.046713	14019.956394	29.043892
335.870176	14034.746764	29.048909
335.970226	14060.410255	29.053927
336.415864	14078.146888	29.058944
336.842102	14089.603818	29.063962
336.657391	14108.752577	29.068980
337.126053	14119.956686	29.073997
337.622563	14153.947841	29.079015
337.789159	14170.521989	29.084032
338.439099	14191.512242	29.089050
338.602386	14212.783053	29.094068
338.933515	14230.111710	29.099085
339.332226	14252.708381	29.104103
339.357532	14278.865205	29.109120
339.826599	14283.732783	29.114138
340.064862	14328.375740	29.119156
340.487417	14349.887556	29.124173
341.116182	14361.887993	29.129191
341.016590	14388.711737	29.134208
341.491088	14408.930707	29.139226
341.869749	14433.883737	29.144244
342.268360	14443.265312	29.149261
342.761040	14457.601704	29.154279
343.151883	14483.533002	29.159296
343.645452	14499.074841	29.164314
343.730733	14510.173935	29.169332
344.026801	14508.971453	29.174349
344.333062	14533.098221	29.179367
344.139019	14571.788612	29.184384
344.788803	14583.498928	29.189402
344.990205	14611.694778	29.194420
345.276999	14626.139399	29.199437
345.463544	14648.177554	29.204455
345.680797	14684.211051	29.209472
346.303241	14696.899879	29.214490
346.393883	14749.890771	29.219508
346.628697	14762.823341	29.224525
347.070161	14790.114662	29.229543
347.996247	14803.368021	29.234560
348.974345	14826.698713	29.239578
349.243515	14835.682702	29.244596
349.444709	14860.380463	29.249613
349.813958	14857.894094	29.254631
349.686584	14887.306192	29.259648
350.136331	14901.741474	29.264666
350.367571	14919.460864	29.269684
350.656112	14951.979877	29.274701
351.164958	14969.894581	29.279719
351.431121	15000.961221	29.284736
352.022697	15017.767032	29.289754
351.986674	15033.002885	29.294772
352.573956	15070.652913	29.299789
353.092964	15083.373315	29.304807
353.106546	15113.282598	29.309824
353.738149	15135.711220	29.314842
353.915027	15160.944550	29.319860
353.963113	15181.261715	29.324877
355.047519	15205.084425	29.329895
355.295624	15231.029463	29.334912
355.550038	15247.735189	29.339930
356.148696	15267.851192	29.344948
356.272070	15286.548564	29.349965
356.672961	15299.539228	29.354983
356.915373	15330.608844	29.360000
357.269846	15349.261808	29.365018
357.898095	15369.152411	29.370036
357.878836	15391.479302	29.375053
358.459977	15398.646970	29.380071
358.327954	15440.509500	29.385088
359.062024	15462.860183	29.390106
359.311123	15487.946553	29.395124
359.484962	15519.068831	29.400141
360.047103	15541.971254	29.405159
360.418510	15576.072727	29.410176
360.788737	15595.081121	29.415194
361.390610	15610.037197	29.420212
361.175423	15637.411623	29.425229
361.812296	15671.973762	29.430247
361.822721	15696.792559	29.435264
362.385395	15729.414404	29.440282
362.384058	15749.436270	29.445300
362.639612	15787.688054	29.450317
363.326681	15807.372474	29.455335
363.547907	15843.480370	29.460352
364.490934	15873.581075	29.465370
365.128218	15889.700970	29.470388
365.830052	15910.606072	29.475405
366.397839	15919.891210	29.480423
366.619682	15947.107275	29.485440
366.767335	15946.236536	29.490458
367.242353	15979.801645	29.495476
367.458219	15977.844780	29.500493
368.077075	16006.930732	29.505511
368.152635	16023.222355	29.510528
368.395836	16041.974871	29.515546
368.472931	16052.118132	29.520564
368.460159	16077.677350	29.525581
368.990216	16098.585854	29.530599
369.331018	16116.967722	29.535616
369.572399	16147.719123	29.540634
370.119534	16161.554720	29.545652
370.035476	16201.776903	29.550669
370.559812	16220.210522	29.555687
370.803627	16253.968841	29.560704
370.927674	16285.047214	29.565722
371.361679	16313.867948	29.570740
371.768114	16358.977255	29.575757
372.291407	16389.195532	29.580775
372.489376	16415.639314	29.585792
373.134218	16445.845497	29.590810
373.615056	16481.136480	29.595828
373.781088	16503.722699	29.600845
374.267517	16536.918260	29.605863
374.518801	16567.651475	29.610880
375.293256	16596.470053	29.615898
375.476545	16621.267996	29.620916
375.772059	16662.092139	29.625933
376.739504	16680.475144	29.630951
376.604438	16718.647052	29.635968
377.339064	16737.096951	29.640986
378.041441	16758.217401	29.646004
378.708115	16788.831975	29.651021
379.056512	16793.189098	29.656039
379.194920	16822.592284	29.661056
379.319110	16837.535407	29.666074
379.893282	16873.859935	29.671092
379.850986	16892.539225	29.676109
380.478550	16925.072351	29.681127
381.090306	16949.700715	29.686144
381.081369	16980.283825	29.691162
381.160665	16998.252802	29.696180
381.443636	17048.221551	29.701197
382.097446	17056.292111	29.706215
382.377821	17099.045881	29.711232
382.511126	17126.308474	29.716250
383.434431	17157.786051	29.721268
384.051918	17180.120518	29.726285
384.500522	17198.668625	29.731303
385.195092	17237.081383	29.736320
385.566236	17258.611832	29.741338
386.135800	17279.329332	29.746356
386.161770	17299.400588	29.751373
386.681418	17320.239869	29.756391
386.280158	17339.867919	29.761408
386.444375	17372.554130	29.766426
387.402544	17401.266543	29.771444
387.411664	17431.573254	29.776461
387.923431	17474.556149	29.781479
388.369050	17502.421887	29.786496
388.841488	17539.360488	29.791514
389.205213	17559.718298	29.796532
389.511666	17589.107702	29.801549
390.096510	17618.239960	29.806567
390.086108	17645.946420	29.811584
390.725138	17668.498660	29.816602
391.159351	17683.388185	29.821620
391.865432	17708.229078	29.826637
392.305295	17722.846599	29.831655
392.863297	17752.199469	29.836672
393.060852	17774.851578	29.841690
393.602038	17799.734035	29.846708
393.681162	17822.754116	29.851725
394.187067	17849.477187	29.856743
394.257915	17877.391282	29.861760
394.214443	17901.990605	29.866778
394.872663	17932.454238	29.871796
394.988660	17961.423391	29.876813
395.618611	17990.433792	29.881831
395.657865	18022.881856	29.886848
396.035122	18054.943139	29.891866
396.865307	18086.154156	29.896884
397.019227	18120.121876	29.901901
397.334647	18149.649506	29.906919
398.083241	18178.309629	29.911936
398.031132	18211.532905	29.916954
398.560953	18248.564496	29.921972
398.780330	18290.421932	29.926989
399.061119	18308.061139	29.932007
399.508073	18357.532310	29.937024
399.879858	18393.119677	29.942042
400.644838	18426.287222	29.947060
401.145029	18469.987096	29.952077
401.186801	18498.942655	29.957095
401.704252	18539.118458	29.962112
402.195345	18567.928981	29.967130
403.015659	18593.433294	29.972148
403.144079	18637.366837	29.977165
403.775088	18674.702654	29.982183
404.561478	18698.721560	29.987200
404.497885	18732.772180	29.992218
404.941670	18755.842086	29.997236
404.999356	18795.739793	30.002253
405.367220	18827.728463	30.007271
405.981042	18860.846188	30.012288
406.222171	18897.168714	30.017306
406.822204	18930.151716	30.022324
406.996350	18973.641956	30.027341
407.565267	19016.808581	30.032359
408.004228	19047.838559	30.037376
408.483145	19084.930873	30.042394
409.592338	19110.320482	30.047412
409.437794	19140.048889	30.052429
409.760255	19172.651038	30.057447
410.259395	19207.791930	30.062464
410.595695	19240.142863	30.067482
411.170412	19265.619424	30.072500
411.430736	19309.200346	30.077517
412.043634	19344.392095	30.082535
412.432586	19375.684742	30.087552
412.734527	19410.388882	30.092570
413.149410	19438.406410	30.097588
413.567018	19481.097954	30.102605
414.100975	19513.855000	30.107623
414.580941	19544.607998	30.112640
414.760034	19572.968944	30.117658
415.181459	19605.104750	30.122676
416.022063	19635.659622	30.127693
416.223568	19665.122069	30.132711
416.667234	19693.201481	30.137728
416.988899	19739.144287	30.142746
417.454209	19760.247848	30.147764
417.511510	19799.463871	30.152781
417.976547	19831.181469	30.157799
418.948456	19866.772178	30.162816
419.347350	19880.160899	30.167834
419.966304	19905.266986	30.172852
420.039647	19944.081867	30.177869
420.290485	19973.695928	30.182887
420.732573	19998.768315	30.187904
421.031011	20037.210454	30.192922
421.594627	20059.806793	30.197940
421.954694	20099.208395	30.202957
422.454067	20125.132240	30.207975
422.835317	20148.695224	30.212992
422.905903	20183.402935	30.218010
423.738698	20211.511953	30.223028
423.784027	20253.894934	30.228045
424.208445	20263.367018	30.233063
424.682470	20299.025133	30.238080
425.117978	20339.502589	30.243098
425.629750	20376.932872	30.248116
426.102110	20398.865294	30.253133
426.647402	20440.647508	30.258151
427.240623	20452.838010	30.263168
427.337176	20496.967748	30.268186
427.926804	20516.519410	30.273204
428.461399	20550.615237	30.278221
428.869135	20586.975412	30.283239
428.998039	20605.356292	30.288256
429.464018	20639.523542	30.293274
430.068114	20670.628589	30.298292
430.133557	20718.872363	30.303309
430.870977	20758.645147	30.308327
431.414586	20784.516993	30.313344
431.848521	20811.791158	30.318362
432.398592	20853.056525	30.323380
432.995970	20879.378398	30.328397
432.907533	20914.090246	30.333415
433.562137	20942.311912	30.338432
433.723605	20988.171110	30.343450
434.362632	21011.314370	30.348468
434.399719	21047.388362	30.353485
434.678759	21089.766386	30.358503
435.389521	21124.066033	30.363520
435.370454	21172.872128	30.368538
435.787226	21210.550145	30.373556
436.591090	21252.636938	30.378573
436.743604	21310.792334	30.383591
437.489809	21349.731083	30.388608
437.413752	21403.292665	30.393626
438.185838	21433.302482	30.398644
438.917576	21492.259888	30.403661
439.621274	21524.543527	30.408679
440.339116	21559.624873	30.413696
440.790019	21586.725654	30.418714
441.113134	21633.100676	30.423732
441.753249	21652.410421	30.428749
441.759863	21693.862225	30.433767
442.639705	21724.148008	30.438784
442.876424	21759.594608	30.443802
443.394632	21789.274926	30.448820
443.855678	21830.026096	30.453837
444.103976	21860.044370	30.458855
444.539561	21896.346031	30.463872
445.004089	21932.146361	30.468890
445.586544	21964.258530	30.473908
445.657691	22007.061055	30.478925
446.232927	22056.172005	30.483943
446.498938	22091.232925	30.488960
447.010069	22126.554563	30.493978
447.547495	22157.417975	30.498996
448.145070	22210.623326	30.504013
448.103596	22240.469417	30.509031
449.041596	22267.478225	30.514048
449.327247	22309.763637	30.519066
449.635745	22358.550598	30.524084
450.286795	22381.427316	30.529101
450.409982	22419.973243	30.534119
451.069606	22459.189017	30.539136
451.511339	22493.855967	30.544154
451.982974	22528.801847	30.549172
452.522920	22550.773227	30.554189
453.155948	22585.035099	30.559207
453.840166	22610.593282	30.564224
453.964386	22649.809646	30.569242
454.208104	22677.230210	30.574260
455.101837	22707.931718	30.579277
455.083016	22754.136118	30.584295
455.989949	22776.958494	30.589312
456.094484	22806.477169	30.594330
456.568600	22842.467054	30.599348
456.985281	22871.764001	30.604365
457.404094	22914.725832	30.609383
457.854656	22951.025718	30.614400
458.353005	22983.139536	30.619418
458.508726	23025.635834	30.624436
458.920999	23063.851674	30.629453
459.346092	23110.696394	30.634471
460.206011	23140.715255	30.639488
460.561853	23185.066223	30.644506
460.982775	23223.572689	30.649524
461.800441	23265.028406	30.654541
461.987911	23322.226323	30.659559
462.580514	23339.697932	30.664576
462.883544	23382.787297	30.669594
463.332818	23425.524652	30.674612
463.799753	23455.533305	30.679629
464.169503	23496.994201	30.684647
464.969386	23546.291555	30.689664
465.160905	23579.190379	30.694682
465.463242	23617.919155	30.699700
466.173381	23673.139815	30.704717
466.697165	23709.153301	30.709735
467.418796	23739.002129	30.714752
468.497797	23779.840423	30.719770
468.865855	23802.204486	30.724788
469.518684	23836.851941	30.729805
469.840044	23871.954721	30.734823
470.049850	23884.168490	30.739840
470.393413	23928.668499	30.744858
470.730484	23951.127755	30.749876
471.401252	23992.716744	30.754893
471.626208	24038.086523	30.759911
472.299966	24063.993958	30.764928
472.629401	24114.286796	30.769946
472.865650	24158.808289	30.774964
473.150044	24202.749563	30.779981
473.511302	24236.389532	30.784999
473.806775	24298.932500	30.790016
474.392424	24349.961087	30.795034
474.699724	24379.605117	30.800052
475.567414	24431.769984	30.805069
476.233932	24481.743323	30.810087
476.415034	24518.015391	30.815104
477.216748	24554.432589	30.820122
477.589271	24604.175748	30.825140
478.008481	24637.059513	30.830157
478.542819	24680.416723	30.835175
479.202755	24720.935449	30.840192
479.822220	24766.029131	30.845210
479.987911	24811.950052	30.850228
480.440615	24838.090716	30.855245
480.436190	24892.454138	30.860263
481.363941	24929.863678	30.865280
481.777447	24978.099972	30.870298
481.922922	25017.352991	30.875316
482.622869	25061.989482	30.880333
482.886238	25111.354776	30.885351
483.699444	25150.496232	30.890368
484.114145	25193.426671	30.895386
484.095322	25246.650344	30.900404
484.905079	25269.348648	30.905421
485.233123	25329.125696	30.910439
485.912420	25365.539623	30.915456
486.622966	25410.724045	30.920474
486.939488	25445.881335	30.925492
487.438096	25482.525628	30.930509
487.601040	25541.229992	30.935527
488.280629	25584.551319	30.940544
488.772531	25630.087825	30.945562
489.126333	25683.052614	30.950580
489.905301	25725.659297	30.955597
490.220779	25776.435587	30.960615
490.582262	25821.275053	30.965632
491.234798	25852.041033	30.970650
491.232552	25924.468361	30.975668
492.140965	25964.493258	30.980685
492.352932	26008.869050	30.985703
493.107524	26059.737656	30.990720
493.858080	26114.814485	30.995738
494.318221	26163.227777	31.000756
495.069762	26193.864478	31.005773
495.408143	26255.869776	31.010791
495.994477	26293.233046	31.015808
496.664096	26343.107248	31.020826
496.856238	26390.748559	31.025844
497.184362	26433.229617	31.030861
497.795724	26487.204645	31.035879
498.312218	26550.370663	31.040896
499.078544	26589.562591	31.045914
499.380448	26640.529774	31.050932
499.860672	26684.367815	31.055949
500.469571	26742.728229	31.060967
500.745916	26783.004532	31.065984
501.458225	26823.070140	31.071002
501.793351	26882.378323	31.076020
502.753107	26926.011611	31.081037
503.136887	26963.261556	31.086055
503.591465	27013.769359	31.091072
504.265945	27051.864102	31.096090
504.633213	27101.383564	31.101108
505.365902	27142.802840	31.106125
505.758590	27180.912873	31.111143
506.304314	27217.370156	31.116160
507.017828	27258.518465	31.121178
507.503068	27310.416226	31.126196
508.212733	27351.984903	31.131213
508.436417	27403.516100	31.136231
508.759627	27445.189839	31.141248
509.142781	27492.657560	31.146266
509.120955	27540.551887	31.151284
509.828016	27578.743353	31.156301
510.880109	27639.112255	31.161319
510.985843	27693.026337	31.166336
511.985073	27727.318516	31.171354
512.255593	27770.077351	31.176372
512.843886	27819.237480	31.181389
512.901075	27874.005496	31.186407
513.711353	27912.401455	31.191424
514.411698	27956.335707	31.196442
514.887479	28012.397686	31.201460
515.764994	28046.193296	31.206477
516.479782	28087.390693	31.211495
516.860300	28117.518025	31.216512
517.516477	28152.820328	31.221530
517.741353	28202.568352	31.226548
517.915314	28224.228991	31.231565
518.227694	28269.587653	31.236583
518.287717	28317.196183	31.241600
519.059155	28351.662870	31.246618
519.542010	28413.292475	31.251636
520.014351	28463.110779	31.256653
520.638602	28514.598056	31.261671
520.726784	28584.277288	31.266688
520.927569	28624.933134	31.271706
521.361880	28680.083032	31.276724
521.842430	28744.259835	31.281741
523.015231	28807.139609	31.286759
523.223011	28867.497697	31.291776
523.792158	28929.149584	31.296794
523.945705	28993.233058	31.301812
524.489554	29048.892840	31.306829
525.148377	29117.546224	31.311847
525.314923	29176.606223	31.316864
526.077416	29231.375597	31.321882
526.756052	29303.824520	31.326900
527.525611	29372.135702	31.331917
528.185860	29429.720696	31.336935
528.448079	29490.841676	31.341952
529.679944	29542.121235	31.346970
529.575454	29610.025663	31.351988
530.525746	29662.519293	31.357005
530.924522	29720.845611	31.362023
531.389439	29787.388518	31.367040
531.826707	29830.131203	31.372058
532.524964	29903.188232	31.377076
533.544740	29958.223407	31.382093
533.966914	30011.726487	31.387111
534.686249	30063.385627	31.392128
535.555137	30113.931845	31.397146
535.752700	30167.794283	31.402164
535.971591	30228.887153	31.407181
536.940126	30268.470462	31.412199
537.093916	30334.760838	31.417216
537.988095	30380.492666	31.422234
538.237901	30442.590699	31.427252
538.989361	30486.428280	31.432269
540.245940	30533.558158	31.437287
540.790331	30585.616852	31.442304
541.676878	30619.024801	31.447322
541.880108	30668.780303	31.452340
541.986032	30698.209779	31.457357
542.837804	30734.563978	31.462375
543.103704	30779.943177	31.467392
543.402134	30832.488062	31.472410
544.054387	30894.000680	31.477428
544.331723	30940.555165	31.482445
544.846884	30998.491103	31.487463
545.280563	31056.778264	31.492480
545.822104	31108.078659	31.497498
546.472030	31164.999102	31.502516
546.877951	31225.323161	31.507533
547.329393	31283.655466	31.512551
547.934706	31336.898893	31.517568
548.534008	31389.045557	31.522586
548.959783	31453.582118	31.527604
549.204000	31505.200955	31.532621
549.984150	31567.685472	31.537639
550.412074	31634.875673	31.542656
551.147048	31702.346691	31.547674
551.576715	31763.391172	31.552692
552.152284	31813.564831	31.557709
552.843147	31867.029208	31.562727
553.483954	31932.708838	31.567744
554.023422	31969.334885	31.572762
554.942714	32004.756148	31.577780
555.758980	32055.783623	31.582797
556.090017	32093.252049	31.587815
556.448370	32147.702944	31.592832
557.150681	32185.605592	31.597850
557.539769	32258.083039	31.602868
558.181870	32291.850070	31.607885
558.922264	32335.217691	31.612903
559.257740	32388.458394	31.617920
559.922100	32430.933292	31.622938
560.380349	32484.434813	31.627956
560.834039	32528.579101	31.632973
561.578853	32582.494241	31.637991
561.915878	32641.370551	31.643008
562.425892	32689.494063	31.648026
562.959025	32749.960103	31.653044
563.231273	32806.831504	31.658061
563.784892	32871.030321	31.663079
564.224262	32930.348196	31.668096
564.627585	32998.670921	31.673114
565.675307	33068.304181	31.678132
566.311511	33122.380896	31.683149
566.987382	33183.825060	31.688167
567.373951	33245.008004	31.693184
567.939752	33301.778875	31.698202
568.793728	33358.773687	31.703220
568.973808	33425.005112	31.708237
569.416207	33484.860749	31.713255
569.872366	33546.039550	31.718272
570.608243	33623.930345	31.723290
571.291875	33679.067433	31.728308
571.577753	33767.625681	31.733325
572.174422	33822.310585	31.738343
572.892045	33890.553289	31.743360
573.674870	33956.507292	31.748378
574.287688	34023.739160	31.753396
574.836650	34083.254211	31.758413
575.630314	34141.731930	31.763431
576.110267	34208.519440	31.768448
576.707388	34266.373701	31.773466
577.493213	34326.216478	31.778484
578.204934	34390.520911	31.783501
578.722705	34441.490987	31.788519
579.242474	34499.166298	31.793536
579.866668	34564.189490	31.798554
580.759683	34604.564994	31.803572
581.049786	34666.813248	31.808589
581.469741	34721.173534	31.813607
581.626101	34787.322446	31.818624
582.403115	34859.118516	31.823642
582.797397	34927.021006	31.828660
583.321792	34999.083408	31.833677
584.056340	35062.818498	31.838695
584.032189	35141.516770	31.843712
585.140120	35197.011345	31.848730
585.573877	35272.109744	31.853748
586.072517	35342.533705	31.858765
586.838122	35409.000843	31.863783
587.381799	35486.963101	31.868800
588.002052	35550.671476	31.873818
588.562836	35625.371698	31.878836
589.014708	35697.922253	31.883853
590.027806	35758.697953	31.888871
590.152446	35832.088870	31.893888
590.790797	35886.258848	31.898906
592.003051	35949.978167	31.903924
592.151784	36012.708889	31.908941
592.754581	36071.950295	31.913959
593.198605	36145.564298	31.918976
593.667606	36201.754500	31.923994
594.368179	36270.305780	31.929012
594.893995	36341.076322	31.934029
595.616897	36404.676110	31.939047
595.860727	36475.029846	31.944064
596.829631	36529.456449	31.949082
597.728222	36590.724110	31.954100
598.189006	36658.748424	31.959117
599.130007	36716.231932	31.964135
599.610196	36788.201541	31.969152
599.981696	36846.985077	31.974170
600.691904	36917.093099	31.979188
600.618746	36990.925378	31.984205
601.491082	37046.862255	31.989223
602.045131	37134.717529	31.994240
602.650584	37190.951409	31.999258
603.264323	37269.572598	32.004276
603.620984	37341.122982	32.009293
604.350720	37425.699988	32.014311
605.092472	37494.788817	32.019328
605.402106	37574.266345	32.024346
606.487641	37644.463545	32.029364
607.236474	37715.761283	32.034381
608.013424	37780.199678	32.039399
608.800843	37856.699114	32.044416
609.602757	37916.507057	32.049434
610.031196	37969.304056	32.054452
610.510622	38046.473759	32.059469
611.967961	38080.334905	32.064487
613.031063	38129.871436	32.069504
613.492760	38182.546789	32.074522
614.891997	38230.614132	32.079540
615.094411	38283.364163	32.084557
615.534576	38327.193635	32.089575
615.756150	38379.792443	32.094592
615.706149	38414.386059	32.099610
616.835378	38487.571383	32.104628
617.261693	38550.798492	32.109645
617.904754	38607.418788	32.114663
618.115983	38680.324103	32.119680
618.423424	38746.096506	32.124698
619.051195	38813.766804	32.129716
619.300269	38880.070113	32.134733
620.018289	38948.054258	32.139751
620.654924	39036.924614	32.144768
621.103403	39115.088742	32.149786
622.063660	39187.802949	32.154804
622.574478	39261.503853	32.159821
623.270196	39340.647612	32.164839
623.883689	39423.760206	32.169856
624.246583	39508.281275	32.174874
625.126907	39574.975257	32.179892
625.732330	39654.851793	32.184909
626.436740	39718.772478	32.189927
626.804460	39784.983736	32.194944
627.196793	39868.630443	32.199962
628.054959	39945.628881	32.204980
628.549945	40028.511290	32.209997
629.154565	40105.157718	32.215015
629.832574	40189.800353	32.220032
630.412671	40274.412203	32.225050
631.253337	40342.851622	32.230068
631.808956	40431.691659	32.235085
632.638139	40494.884238	32.240103
633.173219	40562.835182	32.245120
633.728103	40635.568457	32.250138
634.737692	40700.354427	32.255156
635.343620	40762.612579	32.260173
635.844185	40827.028516	32.265191
636.520412	40909.629304	32.270208
636.717584	40978.669809	32.275226
637.432498	41058.187170	32.280244
637.806896	41125.333387	32.285261
638.740447	41198.303084	32.290279
639.329121	41270.771299	32.295296
640.015790	41360.235000	32.300314
640.819604	41419.807929	32.305332
641.335953	41497.835304	32.310349
642.040783	41580.061896	32.315367
642.513645	41646.593979	32.320384
643.270490	41724.216416	32.325402
644.214736	41796.511182	32.330420
644.288100	41874.439693	32.335437
645.332209	41945.111752	32.340455
646.065012	42024.876574	32.345472
646.371878	42106.773487	32.350490
647.373481	42172.936038	32.355508
647.818293	42262.687148	32.360525
648.540066	42336.842277	32.365543
649.173702	42422.468539	32.370560
649.541599	42505.575695	32.375578
650.498975	42588.194416	32.380596
650.772511	42674.490599	32.385613
651.482132	42754.631765	32.390631
652.528141	42837.341143	32.395648
653.005361	42920.782531	32.400666
654.142984	42993.479404	32.405684
654.485914	43077.890769	32.410701
655.540665	43146.908263	32.415719
656.731120	43210.757686	32.420736
657.307634	43280.375565	32.425754
658.293119	43349.364213	32.430772
658.859034	43417.336389	32.435789
659.314692	43489.273338	32.440807
660.129220	43545.375455	32.445824
661.039012	43625.986154	32.450842
662.059445	43677.328525	32.455860
663.461471	43708.427894	32.460877
664.336856	43759.649223	32.465895
665.036287	43807.291179	32.470912
665.173447	43849.226498	32.475930
665.904933	43893.469485	32.480948
666.030066	43964.323141	32.485965
666.452514	44008.251212	32.490983
667.352082	44058.127587	32.496000
668.120366	44128.503110	32.501018
668.204531	44177.965123	32.506036
668.800365	44246.465800	32.511053
669.501714	44312.297261	32.516071
669.780490	44373.475568	32.521088
670.456212	44452.609899	32.526106
670.984894	44510.034497	32.531124
671.580473	44595.377147	32.536141
671.778226	44678.458990	32.541159
672.352456	44748.913108	32.546176
673.037079	44833.569644	32.551194
673.848209	44926.370436	32.556212
674.030645	45010.482407	32.561229
674.738439	45086.058998	32.566247
675.378676	45172.707200	32.571264
675.673355	45272.531672	32.576282
676.495744	45351.967644	32.581300
677.570471	45446.170403	32.586317
678.360789	45513.087021	32.591335
679.562519	45584.059509	32.596352
679.846133	45672.413929	32.601370
680.734837	45738.551009	32.606388
681.313616	45815.092767	32.611405
681.655304	45893.508474	32.616423
682.600698	45962.191367	32.621440
682.997242	46047.993457	32.626458
684.106223	46113.669224	32.631476
685.062817	46191.899378	32.636493
685.576196	46266.843450	32.641511
686.592296	46343.671943	32.646528
686.719688	46438.269793	32.651546
687.807373	46481.664391	32.656564
688.954767	46566.602826	32.661581
689.546972	46625.883235	32.666599
690.377282	46700.135706	32.671616
690.809037	46772.686029	32.676634
691.658874	46846.092771	32.681652
692.487662	46903.835118	32.686669
693.093357	46977.813172	32.691687
693.673238	47047.172977	32.696704
693.837228	47127.353567	32.701722
694.908975	47190.342601	32.706740
695.406665	47276.023067	32.711757
695.883505	47358.019165	32.716775
696.685809	47437.088348	32.721792
697.141259	47522.928479	32.726810
697.810498	47616.861732	32.731828
698.427951	47698.599255	32.736845
698.815622	47788.016893	32.741863
699.885934	47877.019073	32.746880
700.244325	47965.791880	32.751898
701.214937	48046.244197	32.756916
702.503648	48137.823052	32.761933
702.909615	48232.740715	32.766951
703.597264	48312.868266	32.771968
704.371474	48397.213416	32.776986
704.831610	48478.544495	32.782004
705.339882	48565.005883	32.787021
706.198808	48657.649807	32.792039
707.065495	48752.591878	32.797056
707.670931	48855.788242	32.802074
708.300225	48939.600773	32.807092
709.166156	49038.261322	32.812109
709.569243	49126.716373	32.817127
710.787723	49210.357005	32.822144
711.237339	49303.668532	32.827162
712.334249	49385.548883	32.832180
712.823060	49470.564898	32.837197
713.629307	49556.409971	32.842215
714.512928	49638.370844	32.847232
715.034269	49740.202642	32.852250
715.557724	49821.273189	32.857268
716.558024	49907.498350	32.862285
717.131211	49999.273809	32.867303
718.088041	50076.187234	32.872320
719.063220	50168.569807	32.877338
719.880899	50240.017973	32.882356
720.659992	50325.874144	32.887373
721.190978	50426.855290	32.892391
722.056346	50490.243074	32.897408
722.678207	50566.572667	32.902426
723.087062	50644.273678	32.907444
723.774084	50734.593699	32.912461
724.405886	50839.776649	32.917479
725.024530	50919.560178	32.922496
725.314843	51001.264817	32.927514
726.493578	51081.774528	32.932532
727.315367	51167.810597	32.937549
727.567576	51237.966192	32.942567
728.349375	51331.438028	32.947584
729.101274	51419.609183	32.952602
729.708061	51503.019746	32.957620
730.523092	51584.633892	32.962637
730.903655	51680.488788	32.967655
731.831319	51761.971382	32.972672
732.334126	51861.486563	32.977690
733.184275	51950.904144	32.982708
734.252759	52042.086415	32.987725
734.551655	52129.337543	32.992743
735.765975	52232.994787	32.997760
736.667054	52324.626118	33.002778
737.422469	52409.769034	33.007796
738.137319	52496.826787	33.012813
738.321297	52591.041469	33.017831
739.309876	52688.389713	33.022848
739.843991	52778.510817	33.027866
740.735567	52874.997927	33.032884
741.395147	52971.258503	33.037901
742.005754	53071.311699	33.042919
743.194369	53163.392263	33.047936
744.040447	53257.475572	33.052954
745.292225	53330.998770	33.057972
746.542276	53406.196643	33.062989
746.589271	53504.879507	33.068007
747.470176	53601.308813	33.073024
748.447109	53679.509416	33.078042
749.188839	53765.519716	33.083060
750.008091	53850.001383	33.088077
750.526744	53945.405596	33.093095
751.270123	54038.353522	33.098112
752.258444	54115.783249	33.103130
752.786673	54212.021110	33.108148
754.070485	54292.365725	33.113165
754.254076	54377.782263	33.118183
754.915399	54469.419072	33.123200
755.356589	54573.317553	33.128218
756.131271	54663.584548	33.133236
756.786789	54765.306918	33.138253
757.285926	54864.130467	33.143271
758.204706	54968.741912	33.148288
759.406898	55055.932798	33.153306
760.217120	55140.769021	33.158324
761.294236	55248.704331	33.163341
761.778274	55333.702658	33.168359
762.908934	55429.834383	33.173376
763.731859	55517.487987	33.178394
764.378008	55596.888137	33.183412
765.188688	55691.450229	33.188429
765.353973	55790.257749	33.193447
766.263986	55887.306372	33.198464
767.115616	55994.575375	33.203482
767.788261	56084.316063	33.208500
768.883176	56174.309663	33.213517
768.940709	56271.741045	33.218535
769.362335	56359.199292	33.223552
770.306562	56474.233501	33.228570
771.105032	56589.102896	33.233588
771.938297	56685.593143	33.238605
772.869304	56782.516333	33.243623
773.958559	56872.678332	33.248640
775.239292	56974.087722	33.253658
775.491093	57051.385263	33.258676
776.546233	57147.910631	33.263693
777.134844	57241.910231	33.268711
778.103463	57323.576693	33.273728
778.551594	57398.865429	33.278746
779.602287	57486.509118	33.283764
780.430578	57568.888502	33.288781
781.123469	57651.202123	33.293799
781.292739	57738.417466	33.298816
782.302895	57837.361075	33.303834
782.440389	57934.553623	33.308852
783.369254	58041.688265	33.313869
784.058700	58136.591684	33.318887
784.897548	58244.696438	33.323904
785.670187	58351.390941	33.328922
785.873414	58460.631819	33.333940
786.854190	58564.531682	33.338957
787.482034	58687.472896	33.343975
787.869291	58809.841639	33.348992
788.908753	58914.921629	33.354010
789.943673	59032.963591	33.359028
790.821007	59141.104757	33.364045
791.991130	59260.029383	33.369063
792.837780	59375.071202	33.374080
793.972822	59468.908916	33.379098
794.852498	59582.802674	33.384116
796.021360	59679.567979	33.389133
796.742739	59779.365136	33.394151
797.254802	59884.695286	33.399168
797.980692	59984.056671	33.404186
798.892356	60095.679356	33.409204
800.069236	60199.030792	33.414221
800.219461	60313.864367	33.419239
801.006232	60424.826982	33.424256
801.793985	60525.362595	33.429274
802.408551	60655.585668	33.434292
803.622341	60750.655025	33.439309
804.289896	60859.863872	33.444327
804.946240	60978.396875	33.449344
805.823834	61088.836239	33.454362
806.526790	61199.690555	33.459380
807.382603	61302.253795	33.464397
808.327651	61420.090762	33.469415
808.991093	61538.120275	33.474432
809.771074	61648.420809	33.479450
810.556424	61758.259692	33.484468
811.553238	61879.478328	33.489485
812.270789	61989.506620	33.494503
813.604904	62101.740556	33.499520
814.628086	62202.207699	33.504538
815.527672	62317.112173	33.509556
816.663882	62400.655040	33.514573
817.855367	62497.265779	33.519591
818.565423	62596.971260	33.524608
819.420551	62693.809121	33.529626
819.931727	62800.608259	33.534644
820.784477	62896.429894	33.539661
821.206207	63006.171223	33.544679
821.753116	63120.822440	33.549696
822.733325	63236.483558	33.554714
822.935873	63335.031303	33.559732
824.109895	63443.797486	33.564749
824.670617	63559.902613	33.569767
825.476345	63677.807248	33.574784
826.311521	63779.697421	33.579802
826.403820	63897.367163	33.584820
827.218125	64023.697881	33.589837
828.297265	64153.108115	33.594855
829.048485	64273.913776	33.599872
830.250902	64391.813896	33.604890
831.122707	64504.864266	33.609908
832.209516	64603.366898	33.614925
833.057987	64713.287085	33.619943
833.639265	64826.418797	33.624960
835.057679	64916.176801	33.629978
835.445879	65019.436409	33.634996
836.515734	65127.697739	33.640013
837.275954	65231.257280	33.645031
838.528856	65336.189853	33.650048
839.697817	65426.130333	33.655066
840.486180	65530.211383	33.660084
841.371988	65611.431904	33.665101
842.276883	65719.660361	33.670119
842.660680	65828.184030	33.675136
843.627483	65929.058005	33.680154
844.240785	66030.161518	33.685172
845.155334	66139.926667	33.690189
845.903928	66228.416585	33.695207
847.060203	66342.776497	33.700224
847.965067	66449.346222	33.705242
848.616895	66558.411025	33.710260
849.839761	66648.120333	33.715277
850.787821	66753.337992	33.720295
851.540818	66847.822683	33.725312
852.337904	66947.250367	33.730330
852.867774	67063.936570	33.735348
853.706194	67169.933037	33.740365
854.742181	67271.067610	33.745383
854.989093	67400.743023	33.750400
855.728920	67508.982755	33.755418
856.331397	67648.456700	33.760436
857.213951	67770.221956	33.765453
857.994258	67888.249577	33.770471
858.756817	68020.871888	33.775488
859.592302	68157.573335	33.780506
860.719857	68282.373607	33.785524
861.780074	68398.802660	33.790541
862.797482	68527.693997	33.795559
863.349125	68653.476663	33.800576
864.422165	68774.312221	33.805594
864.803449	68908.792269	33.810612
865.891326	69044.876162	33.815629
866.461231	69161.542126	33.820647
867.468079	69306.644057	33.825664
868.215303	69433.176727	33.830682
868.999190	69566.804189	33.835700
869.577677	69708.040729	33.840717
870.430370	69851.363624	33.845735
871.345668	69986.767632	33.850752
872.944655	70116.988898	33.855770
873.834989	70263.235723	33.860788
874.511921	70386.219724	33.865805
875.330164	70528.250409	33.870823
876.045938	70656.635484	33.875840
877.147178	70783.946040	33.880858
877.815894	70920.522172	33.885876
878.666536	71059.516091	33.890893
879.629547	71211.719906	33.895911
880.578024	71342.327972	33.900928
881.730569	71470.740677	33.905946
882.556188	71618.120337	33.910964
883.016735	71754.040636	33.915981
884.365466	71880.241946	33.920999
885.210290	72020.280066	33.926016
886.314336	72141.686103	33.931034
887.551432	72270.070676	33.936052
888.541947	72393.956624	33.941069
889.682801	72493.031126	33.946087
890.521930	72619.371517	33.951104
891.472831	72719.724125	33.956122
892.415860	72830.733422	33.961140
893.476473	72945.309261	33.966157
894.443447	73040.835938	33.971175
894.669985	73156.277812	33.976192
895.690883	73273.037233	33.981210
896.460530	73386.917286	33.986228
897.064619	73509.836396	33.991245
897.736019	73627.945455	33.996263
898.547669	73746.765548	34.001280
899.580660	73873.852766	34.006298
900.302875	74001.934280	34.011316
901.111483	74133.695372	34.016333
902.138435	74263.087726	34.021351
902.476927	74403.756126	34.026368
903.758683	74534.043955	34.031386
904.238308	74680.647953	34.036404
904.965992	74815.183777	34.041421
905.999898	74964.449098	34.046439
906.899752	75107.293357	34.051456
907.442518	75260.701846	34.056474
908.489641	75402.435977	34.061492
909.057097	75550.409983	34.066509
910.060934	75697.648896	34.071527
910.976349	75868.904030	34.076544
911.798174	76016.377516	34.081562
912.724558	76175.345079	34.086580
914.311574	76330.928673	34.091597
915.741314	76464.289905	34.096615
916.478607	76616.006114	34.101632
918.066823	76752.087762	34.106650
919.152410	76882.814107	34.111668
920.145344	77019.824217	34.116685
921.792894	77129.682908	34.121703
922.466757	77261.662190	34.126720
923.525025	77391.150102	34.131738
924.305678	77514.954383	34.136756
925.266131	77642.246254	34.141773
925.923784	77760.765722	34.146791
926.498610	77905.357927	34.151808
927.858558	78026.349734	34.156826
928.798853	78165.836030	34.161844
929.733691	78300.011123	34.166861
930.790587	78419.986195	34.171879
931.221659	78566.611474	34.176896
931.987391	78692.625917	34.181914
932.969618	78845.512426	34.186932
934.145227	78971.093916	34.191949
935.175820	79099.957538	34.196967
936.106370	79235.897393	34.201984
936.827387	79358.722416	34.207002
937.820435	79493.344188	34.212020
938.430164	79643.160311	34.217037
939.932480	79783.930231	34.222055
940.499976	79915.898563	34.227072
941.345227	80053.236418	34.232090
942.656397	80186.949577	34.237108
943.184537	80331.881506	34.242125
944.353781	80475.063868	34.247143
944.812421	80609.723653	34.252160
945.979855	80750.232326	34.257178
947.201044	80888.765706	34.262196
947.402245	81042.112453	34.267213
948.594875	81182.847393	34.272231
949.552002	81326.772358	34.277248
950.371377	81469.025650	34.282266
951.557650	81606.639304	34.287284
952.222271	81751.399680	34.292301
953.315326	81887.822179	34.297319
954.033928	82033.783713	34.302336
954.955250	82159.108717	34.307354
955.549968	82307.483717	34.312372
956.440485	82447.681753	34.317389
958.019207	82587.279915	34.322407
958.482216	82740.012921	34.327424
959.074972	82882.590850	34.332442
960.183695	83033.245420	34.337460
961.023846	83193.358935	34.342477
962.162387	83339.949091	34.347495
963.269089	83493.061672	34.352512
964.333770	83639.343296	34.357530
965.497409	83798.471327	34.362548
966.283553	83937.329225	34.367565
967.558031	84084.439469	34.372583
968.805503	84241.785292	34.377600
969.507653	84394.407620	34.382618
970.862027	84531.315255	34.387636
971.465181	84682.684171	34.392653
972.593276	84830.993816	34.397671
973.425911	84983.579530	34.402688
974.675595	85122.937478	34.407706
975.971454	85268.944568	34.412724
976.859632	85419.113435	34.417741
977.734863	85564.122579	34.422759
978.989277	85723.394460	34.427776
979.985226	85865.253673	34.432794
981.015298	86011.068902	34.437812
982.245062	86141.527690	34.442829
983.325367	86260.509047	34.447847
984.538045	86424.082473	34.452864
985.670887	86551.598421	34.457882
986.720252	86689.670146	34.462900
987.606504	86826.548442	34.467917
988.750557	86959.980848	34.472935
989.734306	87094.199774	34.477952
990.950559	87229.406135	34.482970
992.108131	87355.188677	34.487988
992.709005	87501.039808	34.493005
993.850768	87607.457757	34.498023
994.854762	87748.953796	34.503040
995.785529	87882.268493	34.508058
997.056559	88014.996249	34.513076
997.982386	88145.902420	34.518093
998.888651	88278.628611	34.523111
999.812109	88408.182498	34.528128
1000.612375	88545.762117	34.533146
1001.677143	88679.369280	34.538164
1002.462069	88819.895482	34.543181
1003.508120	88954.855137	34.548199
1003.818955	89113.856633	34.553216
1004.221550	89260.175384	34.558234
1005.656252	89405.717154	34.563252
1006.547007	89574.972359	34.568269
1007.583499	89726.220168	34.573287
1007.995358	89889.867698	34.578304
1009.016731	90053.643545	34.583322
1009.918301	90223.977390	34.588340
1010.808104	90392.637398	34.593357
1011.761172	90548.618804	34.598375
1013.005841	90714.140599	34.603392
1014.423172	90878.135200	34.608410
1015.445684	91044.892041	34.613428
1016.521015	91202.806711	34.618445
1017.928532	91352.453114	34.623463
1019.018198	91505.469112	34.628480
1020.221333	91644.924071	34.633498
1021.294180	91784.103904	34.638516
1022.181016	91932.574156	34.643533
1023.013245	92064.783128	34.648551
1024.148154	92203.531120	34.653568
1025.089658	92354.773291	34.658586
1026.136322	92483.132882	34.663604
1026.482056	92636.373833	34.668621
1027.606958	92793.524985	34.673639
1028.781964	92943.074115	34.678656
1029.325191	93111.411734	34.683674
1030.142110	93261.281438	34.688692
1031.409992	93435.058589	34.693709
1031.637703	93605.268179	34.698727
1032.819861	93788.340548	34.703744
1033.532574	93961.763750	34.708762
1034.535319	94132.285798	34.713780
1035.395460	94334.447611	34.718797
1036.455068	94499.456317	34.723815
1037.684879	94686.692307	34.728832
1038.557433	94877.115475	34.733850
1039.655596	95064.046957	34.738868
1040.851321	95261.059436	34.743885
1041.904399	95451.381312	34.748903
1043.226724	95630.652908	34.753920
1044.193782	95819.517023	34.758938
1045.885944	95997.888390	34.763956
1047.267841	96174.141146	34.768973
1048.515309	96341.644172	34.773991
1049.896421	96512.563408	34.779008
1051.277585	96683.743347	34.784026
1052.485685	96848.072346	34.789044
1053.188340	97013.213832	34.794061
1054.416098	97177.060687	34.799079
1055.463529	97341.052336	34.804096
1056.477019	97496.169468	34.809114
1057.813699	97658.210085	34.814132
1058.786926	97834.358552	34.819149
1059.775396	97995.901792	34.824167
1061.194454	98150.924400	34.829184
1062.043478	98323.146706	34.834202
1063.049692	98481.037539	34.839220
1063.935122	98651.394959	34.844237
1064.789189	98820.961073	34.849255
1066.159907	98982.422264	34.854272
1066.604045	99161.294593	34.859290
1067.781584	99326.524927	34.864308
1069.087544	99506.308321	34.869325
1069.811517	99676.876610	34.874343
1070.900010	99855.305642	34.879360
1071.523117	100043.036728	34.884378
1072.378036	100210.744482	34.889396
1073.453174	100411.198302	34.894413
1074.227503	100603.428835	34.899431
1075.360364	100797.247692	34.904448
1076.010133	100999.017253	34.909466
1077.738745	101178.078002	34.914484
1078.839365	101376.787864	34.919501
1079.997770	101567.961970	34.924519
1081.153461	101758.941689	34.929536
1082.321327	101939.170334	34.934554
1083.296319	102125.383523	34.939572
1084.477083	102323.220130	34.944589
1085.778842	102514.719545	34.949607
1087.094224	102683.196979	34.954624
1088.238272	102870.622305	34.959642
1089.439953	103045.787953	34.964660
1090.455457	103218.541536	34.969677
1091.494308	103396.256416	34.974695
1092.902928	103556.518392	34.979712
1093.694036	103740.937454	34.984730
1094.466642	103906.188339	34.989748
1095.604736	104077.122879	34.994765
1096.160067	104250.744468	34.999783
1097.316366	104431.562333	35.004800
1098.032984	104615.904936	35.009818
1099.526476	104808.497794	35.014836
1100.837626	104986.457232	35.019853
1101.901184	105174.862328	35.024871
1103.226421	105344.951140	35.029888
1103.953535	105532.641840	35.034906
1104.878785	105718.756122	35.039924
1106.289655	105907.172483	35.044941
1107.211039	106103.168421	35.049959
1108.447628	106271.935444	35.054976
1109.656868	106480.234710	35.059994
1110.711259	106647.742416	35.065012
1112.231414	106841.745290	35.070029
1113.340728	107027.851118	35.075047
1114.659958	107211.200610	35.080064
1115.691247	107401.602753	35.085082
1116.873060	107584.812869	35.090100
1118.247044	107772.476068	35.095117
1118.991718	107950.808715	35.100135
1120.528779	108132.292128	35.105152
1121.719330	108331.451866	35.110170
1122.984432	108508.739753	35.115188
1123.928869	108689.501518	35.120205
1124.612090	108872.321502	35.125223
1126.059058	109065.554751	35.130240
1127.285605	109263.385567	35.135258
1128.269122	109450.922371	35.140276
1129.453862	109646.660330	35.145293
1130.145383	109830.232780	35.150311
1131.399945	110022.643368	35.155328
1132.877877	110225.886334	35.160346
1133.661955	110406.901459	35.165364
1134.786481	110611.028990	35.170381
1135.857359	110815.622921	35.175399
1137.172601	111009.968543	35.180416
1138.258045	111219.731210	35.185434
1139.357349	111415.230072	35.190452
1140.204742	111628.265290	35.195469
1141.381240	111825.439089	35.200487
1142.177196	112035.433165	35.205504
1142.864086	112255.416153	35.210522
1144.233400	112465.420224	35.215540
1145.365504	112678.365956	35.220557
1146.158392	112901.528881	35.225575
1147.366158	113116.555701	35.230592
1148.413134	113353.830360	35.235610
1149.534798	113577.843919	35.240628
1150.722692	113790.687697	35.245645
1152.159223	114017.743881	35.250663
1154.276238	114215.590339	35.255680
1155.142171	114437.018044	35.260698
1156.783446	114649.122147	35.265716
1158.175888	114846.218574	35.270733
1158.897451	115054.296923	35.275751
1160.311286	115257.752442	35.280768
1161.360403	115467.439419	35.285786
1162.875231	115664.876154	35.290804
1164.096023	115867.747193	35.295821
1165.020667	116064.992777	35.300839
1166.374674	116263.929903	35.305856
1167.220607	116472.390997	35.310874
1168.011040	116654.966380	35.315892
1169.717001	116844.689484	35.320909
1170.784231	117035.684904	35.325927
1172.266495	117213.766003	35.330944
1173.242686	117400.876640	35.335962
1174.444654	117572.684030	35.340980
1175.876326	117759.430439	35.345997
1176.579315	117962.655395	35.351015
1177.913375	118153.234189	35.356032
1178.785947	118355.065574	35.361050
1180.219119	118554.335137	35.366068
1181.116777	118739.795050	35.371085
1182.093276	118949.747874	35.376103
1183.414016	119151.460216	35.381120
1184.501335	119347.079899	35.386138
1186.127650	119550.328434	35.391156
1187.441974	119745.165779	35.396173
1188.294575	119946.124688	35.401191
1189.809805	120136.813461	35.406208
1191.045913	120335.722426	35.411226
1192.609113	120539.596557	35.416244
1193.856171	120731.397893	35.421261
1194.615354	120931.289325	35.426279
1195.776416	121136.843290	35.431296
1197.037038	121327.670616	35.436314
1198.182126	121541.124434	35.441332
1199.475984	121739.273166	35.446349
1200.437770	121940.329207	35.451367
1201.689023	122159.827135	35.456384
1202.802756	122369.123110	35.461402
1203.844084	122589.013710	35.466420
1204.712462	122811.861771	35.471437
1205.883693	123024.713795	35.476455
1206.915028	123254.976922	35.481472
1207.727980	123483.047534	35.486490
1208.342562	123725.358584	35.491508
1209.782961	123957.042332	35.496525
1210.989903	124201.527894	35.501543
1212.100076	124439.074029	35.506560
1213.531011	124668.179603	35.511578
1214.925424	124911.486795	35.516596
1216.347839	125163.954045	35.521613
1217.415422	125408.282375	35.526631
1218.987048	125642.745644	35.531648
1220.387107	125875.338036	35.536666
1221.383837	126115.919778	35.541684
1222.894536	126347.952584	35.546701
1224.306539	126587.810502	35.551719
1225.507827	126813.028757	35.556736
1227.088576	127037.007368	35.561754
1228.136777	127283.280479	35.566772
1229.549734	127494.704810	35.571789
1230.778448	127731.129274	35.576807
1231.810741	127965.192534	35.581824
1233.445994	128193.023628	35.586842
1234.705767	128408.066416	35.591860
1236.335257	128624.177725	35.596877
1238.270048	128828.934324	35.601895
1240.073232	129036.603857	35.606912
1241.157361	129234.836620	35.611930
1242.078633	129445.341535	35.616948
1243.687969	129636.049982	35.621965
1244.858816	129847.733236	35.626983
1245.875577	130052.788882	35.632000
1247.453488	130248.246797	35.637018
1248.869575	130453.771533	35.642036
1249.832276	130642.108502	35.647053
1250.907824	130839.681105	35.652071
1251.995242	131043.628822	35.657088
1253.519633	131212.951846	35.662106
1254.172561	131423.932688	35.667124
1255.352206	131603.835596	35.672141
1256.278450	131813.037343	35.677159
1257.209801	132023.481879	35.682176
1258.080071	132217.395618	35.687194
1259.064405	132442.094776	35.692212
1260.235813	132653.923606	35.697229
1261.218840	132884.951558	35.702247
1262.061249	133110.223942	35.707264
1262.996018	133337.016531	35.712282
1264.390927	133576.626893	35.717300
1265.812487	133814.966978	35.722317
1266.918326	134061.347330	35.727335
1268.441876	134310.842527	35.732352
1269.683346	134539.190278	35.737370
1270.930495	134786.985355	35.742388
1271.873329	135038.179336	35.747405
1272.773354	135286.479230	35.752423
1274.250572	135546.032013	35.757440
1275.672643	135806.977815	35.762458
1276.915925	136066.002866	35.767476
1278.229108	136318.464068	35.772493
1279.619387	136594.799444	35.777511
1280.658286	136848.729913	35.782528
1282.266010	137113.826513	35.787546
1283.170823	137376.366182	35.792564
1284.961858	137644.783810	35.797581
1285.992989	137904.619047	35.802599
1287.061033	138175.670606	35.807616
1288.846087	138440.406246	35.812634
1289.843548	138699.391112	35.817652
1291.752778	138959.330547	35.822669
1293.378662	139230.108424	35.827687
1294.527792	139483.178682	35.832704
1295.977508	139733.957054	35.837722
1297.122490	140002.639741	35.842740
1298.370164	140272.448744	35.847757
1299.549056	140538.974635	35.852775
1300.566899	140815.748789	35.857792
1302.030428	141076.779785	35.862810
1302.964592	141359.392057	35.867828
1304.129835	141639.128276	35.872845
1305.687213	141905.120556	35.877863
1306.959193	142185.173291	35.882880
1308.553411	142451.480721	35.887898
1309.817076	142728.787690	35.892916
1311.411226	142989.317159	35.897933
1312.838719	143270.988785	35.902951
1313.777331	143543.613496	35.907968
1315.475455	143807.885349	35.912986
1317.187407	144073.348899	35.918004
1318.555608	144330.527310	35.923021
1319.774999	144605.827641	35.928039
1321.469339	144869.689675	35.933056
1322.821398	145117.733606	35.938074
1324.483677	145402.985044	35.943092
1325.754754	145640.596815	35.948109
1327.345157	145899.702909	35.953127
1328.860876	146145.545861	35.958144
1330.191037	146390.495392	35.963162
1331.314355	146647.566224	35.968180
1332.736731	146898.515060	35.973197
1333.656277	147145.591954	35.978215
1334.910971	147398.537625	35.983232
1336.613892	147661.531229	35.988250
1337.358251	147922.135879	35.993268
1338.591202	148177.145076	35.998285
1339.918266	148418.114091	36.003303
1341.236172	148664.323973	36.008320
1342.297006	148907.699065	36.013338
1343.146284	149158.605989	36.018356
1344.354173	149418.168313	36.023373
1345.490937	149687.902956	36.028391
1346.352637	149956.404026	36.033408
1348.011585	150216.430220	36.038426
1349.382681	150492.042244	36.043444
1351.043836	150768.813331	36.048461
1352.302534	151035.328909	36.053479
1353.160198	151308.089267	36.058496
1354.748627	151596.382116	36.063514
1356.291653	151875.032672	36.068532
1357.293906	152158.137643	36.073549
1358.465732	152448.167327	36.078567
1359.785772	152736.855686	36.083584
1361.178043	153023.441517	36.088602
1362.599536	153320.514202	36.093620
1363.817618	153607.856173	36.098637
1365.275500	153899.206931	36.103655
1366.630913	154206.216317	36.108672
1368.044919	154488.509673	36.113690
1369.604769	154797.519523	36.118708
1371.272395	155096.911977	36.123725
1373.230554	155392.250504	36.128743
1374.519221	155678.112225	36.133760
1376.150537	155969.526129	36.138778
1377.768911	156235.447958	36.143796
1379.755882	156523.737596	36.148813
1381.994073	156771.383381	36.153831
1383.138876	157054.183793	36.158848
1384.519981	157316.359289	36.163866
1385.748759	157583.382042	36.168884
1387.216537	157851.508830	36.173901
1388.770952	158114.967601	36.178919
1390.102774	158382.156320	36.183936
1391.291193	158647.556462	36.188954
1392.730199	158907.500250	36.193972
1394.155914	159190.650078	36.198989
1395.774519	159453.485476	36.204007
1396.913401	159727.717561	36.209024
1398.357794	159989.126322	36.214042
1399.543438	160263.328947	36.219060
1400.557891	160540.149645	36.224077
1402.097552	160824.421164	36.229095
1403.095773	161107.667618	36.234112
1404.843977	161368.629128	36.239130
1406.410797	161653.751906	36.244148
1407.858822	161948.449248	36.249165
1409.243251	162225.841899	36.254183
1410.507162	162506.592908	36.259200
1411.627311	162781.977636	36.264218
1413.627559	163065.934848	36.269236
1414.580441	163357.234988	36.274253
1416.257801	163627.052543	36.279271
1417.413121	163911.598967	36.284288
1418.865172	164196.923013	36.289306
1420.397118	164476.272750	36.294324
1421.953504	164765.922479	36.299341
1423.397467	165044.009039	36.304359
1424.339595	165346.020209	36.309376
1426.137046	165633.225397	36.314394
1427.636212	165912.729509	36.319412
1428.348907	166207.286129	36.324429
1430.234889	166480.386161	36.329447
1430.947969	166782.800459	36.334464
1432.193939	167064.498067	36.339482
1433.317151	167351.635605	36.344500
1434.461313	167639.038023	36.349517
1435.730530	167943.297190	36.354535
1436.675917	168244.998080	36.359552
1438.349529	168535.250003	36.364570
1439.334747	168852.568034	36.369588
1440.415214	169163.426748	36.374605
1442.149667	169475.753114	36.379623
1443.574713	169796.697711	36.384640
1445.426404	170113.564479	36.389658
1447.035216	170414.345766	36.394676
1448.593916	170731.899676	36.399693
1450.525052	171039.801288	36.404711
1451.874820	171360.820160	36.409728
1453.477133	171666.026679	36.414746
1454.810339	171986.519712	36.419764
1456.044069	172311.637708	36.424781
1457.579311	172617.813321	36.429799
1458.516380	172955.217626	36.434816
1460.276295	173275.179638	36.439834
1462.114731	173604.521433	36.444852
1463.483993	173927.699473	36.449869
1465.042069	174247.764878	36.454887
1466.627254	174574.261902	36.459904
1467.972110	174901.765294	36.464922
1470.046080	175228.731837	36.469940
1471.110812	175546.730036	36.474957
1472.946949	175869.907688	36.479975
1474.363009	176191.240545	36.484992
1475.967772	176524.410206	36.490010
1477.185936	176854.562087	36.495028
1478.397781	177193.182063	36.500045
1479.437853	177518.570665	36.505063
1481.016102	177860.002937	36.510080
1482.426245	178198.292528	36.515098
1484.274059	178540.421102	36.520116
1486.206384	178877.182349	36.525133
1488.095209	179196.553141	36.530151
1489.111679	179532.632297	36.535168
1490.860040	179866.435354	36.540186
1493.015319	180195.693316	36.545204
1494.049813	180529.148947	36.550221
1495.852365	180866.769848	36.555239
1497.245784	181196.299599	36.560256
1498.707665	181518.141521	36.565274
1500.718572	181827.190110	36.570292
1501.975636	182172.550193	36.575309
1503.932726	182471.356254	36.580327
1505.066361	182812.044822	36.585344
1506.678684	183137.032304	36.590362
1508.285169	183462.390834	36.595380
1509.709057	183776.434382	36.600397
1511.178481	184102.212920	36.605415
1512.868740	184433.973332	36.610432
1514.166163	184771.068113	36.615450
1515.519041	185103.662589	36.620468
1516.802259	185429.987613	36.625485
1518.250174	185773.067547	36.630503
1519.544835	186112.100451	36.635520
1521.093232	186443.223831	36.640538
1522.911240	186780.905187	36.645556
1524.430582	187119.843750	36.650573
1526.007742	187451.196894	36.655591
1527.468433	187786.061921	36.660608
1528.865035	188126.346963	36.665626
1530.883017	188443.860755	36.670644
1533.130296	188752.592556	36.675661
1535.174191	189047.459955	36.680679
1536.785787	189334.923565	36.685696
1538.511687	189629.364073	36.690714
1540.279863	189893.079819	36.695732
1541.739901	190185.028250	36.700749
1543.246773	190458.678304	36.705767
1544.690252	190750.327649	36.710784
1545.409958	191037.858023	36.715802
1547.400805	191330.232360	36.720820
1548.785986	191619.280627	36.725837
1550.678049	191905.720489	36.730855
1552.159267	192194.070213	36.735872
1552.889510	192482.392911	36.740890
1554.412360	192805.280389	36.745908
1555.449198	193109.766438	36.750925
1556.784750	193436.737775	36.755943
1558.447980	193762.222294	36.760960
1559.573471	194101.761570	36.765978
1561.009801	194410.440953	36.770996
1562.574963	194755.306604	36.776013
1564.185707	195087.712838	36.781031
1565.289101	195429.510054	36.786048
1566.603339	195777.368017	36.791066
1568.438754	196120.228849	36.796084
1570.093420	196468.453383	36.801101
1571.829522	196804.313794	36.806119
1573.264158	197162.303061	36.811136
1575.196003	197510.233611	36.816154
1576.971310	197868.170576	36.821172
1578.282986	198213.503065	36.826189
1579.958021	198572.780779	36.831207
1581.599660	198914.787015	36.836224
1582.651675	199272.774798	36.841242
1584.378123	199628.558394	36.846260
1585.345505	200012.958898	36.851277
1586.949370	200391.911531	36.856295
1588.469751	200770.968925	36.861312
1590.161664	201145.239046	36.866330
1591.949047	201510.138309	36.871348
1593.726690	201888.143710	36.876365
1595.642678	202235.568118	36.881383
1597.662894	202620.164972	36.886400
1599.217163	202992.690227	36.891418
1601.040923	203349.124479	36.896436
1602.693115	203723.046717	36.901453
1604.149347	204073.539695	36.906471
1605.645490	204453.573194	36.911488
1607.038394	204831.594214	36.916506
1608.750376	205205.907822	36.921524
1609.610515	205587.880489	36.926541
1611.406168	205975.071610	36.931559
1612.876805	206349.722826	36.936576
1614.319961	206752.149155	36.941594
1615.705554	207142.994531	36.946612
1617.237175	207539.556989	36.951629
1618.680435	207931.704682	36.956647
1620.420291	208343.651509	36.961664
1621.827848	208745.713186	36.966682
1623.746994	209144.099088	36.971700
1625.115217	209547.123637	36.976717
1627.001337	209942.230285	36.981735
1629.213558	210319.216158	36.986752
1631.282142	210732.276567	36.991770
1633.497170	211100.694559	36.996788
1635.285322	211489.450520	37.001805
1637.185406	211865.936267	37.006823
1638.931239	212228.557491	37.011840
1640.815023	212582.522803	37.016858
1642.494366	212943.583487	37.021876
1644.026535	213281.406867	37.026893
1645.643026	213632.652401	37.031911
1647.233813	213973.973520	37.036928
1648.930741	214307.303891	37.041946
1650.051505	214667.879754	37.046964
1651.371481	215026.544835	37.051981
1652.885524	215377.128480	37.056999
1654.903331	215738.297146	37.062016
1656.811605	216076.119894	37.067034
1658.947891	216433.233599	37.072052
1660.595010	216784.994348	37.077069
1662.466453	217146.776812	37.082087
1663.946518	217507.990299	37.087104
1664.849622	217922.787874	37.092122
1666.161872	218273.466503	37.097140
1667.704717	218644.502853	37.102157
1669.086647	219023.999291	37.107175
1670.497799	219403.492368	37.112192
1672.123598	219799.815867	37.117210
1673.618966	220194.867137	37.122228
1675.249336	220592.513704	37.127245
1677.112410	220969.931638	37.132263
1679.149548	221355.348177	37.137280
1680.484628	221750.355668	37.142298
1682.164294	222157.042009	37.147316
1684.028111	222558.213368	37.152333
1685.558305	222964.952834	37.157351
1687.155791	223366.221924	37.162368
1688.761710	223781.968589	37.167386
1690.535526	224190.170935	37.172404
1692.009144	224605.561497	37.177421
1693.772884	225024.918815	37.182439
1695.431615	225432.255620	37.187456
1696.857744	225861.450472	37.192474
1698.442781	226289.579279	37.197492
1700.182552	226712.451737	37.202509
1702.026341	227151.894623	37.207527
1703.738279	227568.170679	37.212544
1705.465955	228009.312171	37.217562
1707.601204	228415.716795	37.222580
1709.603768	228854.682270	37.227597
1711.342010	229294.708857	37.232615
1712.794042	229703.236870	37.237632
1714.217109	230150.455813	37.242650
1716.124994	230570.595479	37.247668
1717.934520	231013.765623	37.252685
1718.949017	231451.759600	37.257703
1721.006580	231888.465219	37.262720
1722.992987	232321.526189	37.267738
1725.161051	232762.813783	37.272756
1726.958314	233194.943308	37.277773
1728.924230	233613.228070	37.282791
1730.753711	234037.912178	37.287808
1732.200857	234476.986814	37.292826
1734.165483	234901.117551	37.297844
1735.657678	235335.945119	37.302861
1737.131187	235758.939871	37.307879
1739.497795	236202.795390	37.312896
1741.318201	236613.085138	37.317914
1743.060153	237047.596545	37.322932
1745.210199	237475.005444	37.327949
1746.359768	237899.913244	37.332967
1748.396615	238313.473471	37.337984
1750.045976	238755.116789	37.343002
1751.540892	239178.141622	37.348020
1753.383213	239604.005898	37.353037
1754.810936	240037.458494	37.358055
1756.436372	240453.402787	37.363072
1758.176812	240867.525404	37.368090
1759.953677	241262.489599	37.373108
1761.970807	241683.731585	37.378125
1763.257270	242104.155042	37.383143
1764.897873	242503.462353	37.388160
1766.363113	242944.509964	37.393178
1768.306318	243366.808790	37.398196
1769.943882	243793.959847	37.403213
1771.450878	244222.250896	37.408231
1773.118378	244645.689715	37.413248
1775.008543	245079.710770	37.418266
1777.367691	245504.510224	37.423284
1779.772515	245944.061746	37.428301
1781.671359	246381.665211	37.433319
1783.788383	246778.690583	37.438336
1785.638007	247213.559910	37.443354
1787.550097	247626.395316	37.448372
1789.210355	248054.997155	37.453389
1791.352553	248483.291421	37.458407
1793.175609	248889.614562	37.463424
1794.844875	249317.733846	37.468442
1796.498942	249735.720359	37.473460
1798.783717	250156.524627	37.478477
1800.650241	250578.033413	37.483495
1802.866176	250984.166960	37.488512
1804.418837	251424.170969	37.493530
1806.249392	251826.990258	37.498548
1807.837022	252257.996601	37.503565
1809.156066	252687.218598	37.508583
1811.280158	253103.784390	37.513600
1812.887431	253536.871597	37.518618
1814.633735	253970.215621	37.523636
1816.474614	254411.216107	37.528653
1817.871274	254863.442170	37.533671
1819.460689	255291.275020	37.538688
1821.393708	255745.902643	37.543706
1822.867449	256198.904251	37.548724
1824.467585	256662.554592	37.553741
1826.088898	257131.409310	37.558759
1828.265036	257579.367392	37.563776
1829.946301	258055.731919	37.568794
1831.542213	258515.344483	37.573812
1833.605882	258985.600178	37.578829
1835.026817	259469.222505	37.583847
1837.244627	259935.896443	37.588864
1838.760929	260418.868038	37.593882
1840.480486	260890.882683	37.598900
1842.350111	261382.814143	37.603917
1843.791633	261874.384312	37.608935
1846.070156	262357.382430	37.613952
1847.560084	262851.129100	37.618970
1849.492687	263328.874745	37.623988
1851.680766	263830.584179	37.629005
1853.551547	264319.517099	37.634023
1856.106622	264796.651416	37.639040
1858.470326	265263.300120	37.644058
1860.487562	265726.982736	37.649076
1862.901823	266206.552795	37.654093
1865.239331	266661.062244	37.659111
1867.431262	267101.750665	37.664128
1869.401024	267549.512091	37.669146
1871.723056	267993.760233	37.674164
1873.371473	268436.823568	37.679181
1875.040206	268879.171882	37.684199
1877.096085	269317.239021	37.689216
1878.528231	269771.818995	37.694234
1880.551696	270201.177376	37.699252
1882.590331	270619.660337	37.704269
1883.667195	271036.370885	37.709287
1885.166599	271477.575917	37.714304
1886.606205	271897.909103	37.719322
1887.685184	272359.682554	37.724340
1889.423421	272809.585125	37.729357
1890.795153	273283.172140	37.734375
1892.689689	273745.266374	37.739392
1894.221441	274221.619874	37.744410
1895.665274	274705.150667	37.749428
1897.174070	275199.212020	37.754445
1898.764578	275713.174639	37.759463
1900.486821	276203.540988	37.764480
1902.180475	276731.710024	37.769498
1903.776552	277239.140257	37.774516
1905.985599	277759.956985	37.779533
1908.318970	278280.625043	37.784551
1910.356101	278798.902166	37.789568
1912.698938	279314.308010	37.794586
1914.267526	279837.765807	37.799604
1916.829051	280358.746931	37.804621
1919.201009	280871.299130	37.809639
1921.172224	281391.485896	37.814656
1923.023724	281911.437003	37.819674
1925.722964	282415.929567	37.824692
1927.950732	282919.558665	37.829709
1930.030797	283426.868571	37.834727
1932.501445	283915.925061	37.839744
1934.585864	284419.014721	37.844762
1936.514768	284920.833073	37.849780
1938.805507	285416.036680	37.854797
1940.583290	285923.338208	37.859815
1942.313638	286415.887851	37.864832
1944.769492	286904.963333	37.869850
1946.817594	287400.353181	37.874868
1948.937713	287866.239005	37.879885
1950.891619	288368.702665	37.884903
1952.815556	288846.784776	37.889920
1954.432531	289341.756601	37.894938
1956.489746	289848.643172	37.899956
1958.972718	290313.826197	37.904973
1961.355046	290820.172959	37.909991
1963.121478	291300.939650	37.915008
1964.902818	291794.376863	37.920026
1966.784300	292284.747671	37.925044
1968.798761	292778.066477	37.930061
1970.586034	293275.383222	37.935079
1972.465094	293771.336647	37.940096
1974.389192	294250.085003	37.945114
1975.790128	294760.413318	37.950132
1977.770817	295260.611003	37.955149
1979.369804	295772.324656	37.960167
1981.514765	296269.112790	37.965184
1983.543252	296783.621215	37.970202
1985.194294	297304.285321	37.975220
1987.645742	297810.667738	37.980237
1989.205402	298342.923929	37.985255
1990.864569	298857.483570	37.990272
1992.926783	299378.323892	37.995290
1994.573682	299911.726174	38.000308
1997.060625	300428.884607	38.005325
1998.978979	300965.944803	38.010343
2001.004549	301496.203168	38.015360
2002.866863	302023.818850	38.020378
2004.583323	302540.585496	38.025396
2006.949743	303080.252468	38.030413
2008.623872	303620.589326	38.035431
2010.424990	304161.333908	38.040448
2012.801015	304668.354613	38.045466
2014.698523	305172.860954	38.050484
2016.685392	305678.797393	38.055501
2018.714013	306200.597111	38.060519
2020.499135	306706.992774	38.065536
2022.522712	307227.085712	38.070554
2024.223921	307736.968592	38.075572
2026.585706	308258.421764	38.080589
2028.254122	308798.652200	38.085607
2030.096815	309336.260057	38.090624
2032.278664	309854.203022	38.095642
2033.973924	310402.977010	38.100660
2036.054001	310939.138526	38.105677
2038.048155	311488.795515	38.110695
2040.170458	312035.938877	38.115712
2042.494640	312578.220136	38.120730
2044.180399	313128.119759	38.125748
2046.048334	313696.320260	38.130765
2047.674282	314259.350627	38.135783
2049.792677	314833.570583	38.140800
2051.869357	315406.955026	38.145818
2053.852369	315988.451087	38.150836
2056.276323	316534.979126	38.155853
2059.324127	317110.120026	38.160871
2061.552085	317668.048041	38.165888
2064.151332	318229.770182	38.170906
2066.106116	318799.262744	38.175924
2067.987471	319366.705987	38.180941
2070.039769	319936.274734	38.185959
2071.902658	320498.633244	38.190976
2074.317848	321069.732387	38.195994
2076.054719	321645.636013	38.201012
2078.021080	322213.777819	38.206029
2080.225689	322790.330724	38.211047
2081.822112	323379.953653	38.216064
2083.806402	323950.591134	38.221082
2085.144762	324559.085801	38.226100
2087.147198	325150.022004	38.231117
2089.277661	325763.985718	38.236135
2091.155704	326375.877675	38.241152
2093.572840	326977.798142	38.246170
2095.751768	327599.403297	38.251188
2097.891607	328216.133846	38.256205
2099.669829	328818.369950	38.261223
2101.692858	329445.745006	38.266240
2103.877245	330081.261804	38.271258
2106.165557	330711.245384	38.276276
2108.224240	331326.128938	38.281293
2110.141260	331969.387022	38.286311
2111.884400	332597.967387	38.291328
2114.119261	333228.414457	38.296346
2116.421474	333875.141490	38.301364
2118.407293	334513.764188	38.306381
2120.619329	335161.176485	38.311399
2122.718136	335801.796424	38.316416
2124.957938	336443.324787	38.321434
2127.793702	337076.903218	38.326452
2130.055292	337700.237202	38.331469
2132.523881	338339.699582	38.336487
2134.534627	338972.807470	38.341504
2136.955174	339592.970459	38.346522
2138.695119	340230.016729	38.351540
2140.729429	340839.744956	38.356557
2143.119396	341482.176519	38.361575
2145.687689	342098.375661	38.366592
2148.466013	342708.415435	38.371610
2150.748474	343335.383087	38.376628
2153.115496	343929.383450	38.381645
2154.939503	344521.994021	38.386663
2156.766518	345099.977388	38.391680
2159.580508	345674.745370	38.396698
2161.425317	346254.082463	38.401716
2163.825127	346822.940505	38.406733
2165.911185	347383.924932	38.411751
2168.474220	347955.864070	38.416768
2170.670885	348518.034857	38.421786
2172.727670	349097.530274	38.426804
2174.777909	349658.290096	38.431821
2177.025008	350229.847080	38.436839
2178.818607	350813.830698	38.441856
2181.211960	351378.877682	38.446874
2183.825775	351951.798893	38.451892
2186.040420	352533.457471	38.456909
2189.057557	353092.238627	38.461927
2190.933997	353670.791282	38.466944
2193.099584	354242.107206	38.471962
2194.966807	354813.642448	38.476980
2197.326639	355405.972738	38.481997
2199.429227	355983.797445	38.487015
2201.083546	356573.335174	38.492032
2203.258176	357157.450317	38.497050
2204.862908	357770.222303	38.502068
2206.608232	358366.672363	38.507085
2208.876487	358988.172396	38.512103
2210.973035	359603.678065	38.517120
2213.734089	360208.307059	38.522138
2215.672336	360825.114467	38.527156
2217.516425	361472.551515	38.532173
2219.971858	362093.668947	38.537191
2221.522925	362743.290400	38.542208
2223.742896	363391.091141	38.547226
2225.758626	364037.697200	38.552244
2227.308837	364709.180763	38.557261
2229.664200	365376.537075	38.562279
2231.119548	366051.996071	38.567296
2233.599568	366725.853655	38.572314
2235.626964	367417.227016	38.577332
2237.625859	368109.962353	38.582349
2239.604172	368802.739132	38.587367
2241.902933	369512.674025	38.592384
2244.424041	370208.861208	38.597402
2246.749993	370922.544228	38.602420
2249.256975	371635.701644	38.607437
2252.280402	372315.887793	38.612455
2254.416106	373029.738668	38.617472
2256.558772	373722.979238	38.622490
2259.216855	374422.107089	38.627508
2261.810635	375122.855049	38.632525
2264.394493	375819.203201	38.637543
2266.815237	376510.847283	38.642560
2269.210834	377192.007818	38.647578
2271.558470	377891.726764	38.652596
2273.697591	378583.274722	38.657613
2275.955051	379264.797688	38.662631
2277.688917	379964.854686	38.667648
2280.214792	380657.742436	38.672666
2282.465672	381367.346790	38.677684
2284.903119	382059.510320	38.682701
2287.232788	382766.891355	38.687719
2289.247949	383469.237962	38.692736
2291.494734	384157.915460	38.697754
2293.636964	384863.203397	38.702772
2295.817337	385580.538615	38.707789
2298.106259	386275.173601	38.712807
2300.316968	386997.543268	38.717824
2302.932437	387682.586523	38.722842
2305.076843	388375.273131	38.727860
2306.943387	389057.291989	38.732877
2309.677564	389732.054714	38.737895
2311.904707	390402.247377	38.742912
2314.747365	391072.907248	38.747930
2317.475322	391743.622277	38.752948
2319.870708	392416.633682	38.757965
2322.425050	393070.922284	38.762983
2325.067574	393745.384748	38.768000
2326.915354	394411.598675	38.773018
2329.554437	395082.458066	38.778036
2331.422986	395744.887883	38.783053
2333.868304	396414.608959	38.788071
2336.130397	397108.524551	38.793088
2338.129204	397797.753270	38.798106
2340.606533	398470.134645	38.803124
2342.593247	399168.558566	38.808141
2345.568890	399835.098910	38.813159
2348.425939	400524.020763	38.818176
2350.942195	401204.898458	38.823194
2353.369820	401890.031997	38.828212
2355.465487	402575.761415	38.833229
2357.829928	403246.732967	38.838247
2360.292387	403943.974643	38.843264
2362.642196	404620.870825	38.848282
2364.881787	405315.556181	38.853300
2366.853939	406009.229586	38.858317
2368.957767	406710.921112	38.863335
2371.353872	407425.645459	38.868352
2373.606014	408147.164939	38.873370
2375.672916	408867.986652	38.878388
2377.703612	409585.957929	38.883405
2380.685122	410314.317528	38.888423
2383.066460	411059.045414	38.893440
2385.166762	411772.134060	38.898458
2387.445922	412518.839591	38.903476
2389.838164	413253.650867	38.908493
2392.318407	413997.596729	38.913511
2394.464800	414745.325413	38.918528
2396.573525	415490.075623	38.923546
2398.848732	416255.545932	38.928564
2400.759287	417034.325195	38.933581
2403.311277	417799.147194	38.938599
2405.720074	418571.618401	38.943616
2408.068995	419340.353493	38.948634
2410.854627	420112.640082	38.953652
2413.257926	420902.008703	38.958669
2415.911317	421673.256605	38.963687
2418.826776	422455.300609	38.968704
2420.941131	423242.009995	38.973722
2423.440765	424000.576472	38.978740
2425.701290	424795.239029	38.983757
2428.579572	425562.886018	38.988775
2431.059288	426336.802845	38.993792
2433.466841	427116.428656	38.998810
2436.317804	427871.045438	39.003828
2438.929887	428650.993277	39.008845
2441.879166	429407.824194	39.013863
2444.340124	430181.975596	39.018880
2446.661722	430939.266575	39.023898
2449.460180	431692.911134	39.028916
2451.874622	432469.881245	39.033933
2454.130768	433233.487985	39.038951
2456.132381	433996.757489	39.043968
2458.317424	434766.754515	39.048986
2461.494411	435525.983827	39.054004
2463.506119	436281.887963	39.059021
2466.042751	437032.012175	39.064039
2468.645874	437789.793709	39.069056
2470.583185	438523.063888	39.074074
2473.033072	439250.810928	39.079092
2475.401427	439993.830958	39.084109
2477.734765	440744.119260	39.089127
2480.090106	441486.080076	39.094144
2482.443688	442238.440302	39.099162
2484.194024	442999.425779	39.104180
2486.362844	443773.269029	39.109197
2488.761533	444542.797246	39.114215
2491.184211	445327.472652	39.119232
2493.076250	446122.932860	39.124250
2495.481924	446907.098988	39.129268
2497.597064	447723.661030	39.134285
2500.139543	448536.833662	39.139303
2502.520065	449347.928293	39.144320
2505.335879	450170.099120	39.149338
2508.625506	450978.604597	39.154356
2511.195518	451813.043448	39.159373
2513.942780	452616.871994	39.164391
2516.495554	453435.924801	39.169408
2518.956186	454261.029469	39.174426
2521.521611	455098.372836	39.179444
2524.206042	455920.694577	39.184461
2526.613613	456757.137272	39.189479
2529.234336	457586.836356	39.194496
2531.477567	458430.974328	39.199514
2534.093885	459271.375555	39.204532
2536.195064	460118.247818	39.209549
2538.904718	460971.303819	39.214567
2541.367551	461823.858846	39.219584
2543.998944	462692.930767	39.224602
2546.326063	463561.155688	39.229620
2548.685476	464443.187287	39.234637
2550.988766	465303.555628	39.239655
2553.981949	466178.733319	39.244672
2556.308840	467053.324786	39.249690
2558.949181	467940.005123	39.254708
2561.324334	468840.232350	39.259725
2563.448597	469754.861112	39.264743
2566.275043	470639.264785	39.269760
2568.422240	471558.857113	39.274778
2571.297835	472459.186214	39.279796
2573.827007	473380.295110	39.284813
2576.237404	474279.907220	39.289831
2579.137255	475210.717481	39.294848
2581.312760	476140.034998	39.299866
2584.028558	477054.719774	39.304884
2586.679384	477988.766690	39.309901
2589.048907	478924.277655	39.314919
2591.904237	479848.347704	39.319936
2594.354997	480783.397268	39.324954
2597.477204	481707.632608	39.329972
2599.945136	482645.109017	39.334989
2602.197393	483591.207317	39.340007
2605.629772	484505.806155	39.345024
2608.282190	485440.481358	39.350042
2611.184049	486368.957583	39.355060
2613.398833	487318.096757	39.360077
2615.785411	488238.735082	39.365095
2618.527737	489176.732938	39.370112
2620.889274	490102.578514	39.375130
2624.170879	491033.371949	39.380148
2626.953780	491966.166354	39.385165
2629.470506	492891.939335	39.390183
2632.277737	493821.500853	39.395200
2634.530374	494754.282890	39.400218
2637.090124	495663.347792	39.405236
2640.180315	496579.240209	39.410253
2642.927036	497464.109633	39.415271
2645.427029	498347.762694	39.420288
2648.035554	499253.247221	39.425306
2650.784934	500141.457104	39.430324
2653.302100	501016.542457	39.435341
2656.017495	501914.147573	39.440359
2658.701560	502792.390980	39.445376
2661.322423	503693.093258	39.450394
2664.166021	504589.069742	39.455412
2667.018682	505472.942774	39.460429
2669.854352	506374.572355	39.465447
2672.738015	507266.462427	39.470464
2675.380395	508159.654379	39.475482
2678.210064	509045.354412	39.480500
2681.013112	509948.606069	39.485517
2683.408922	510854.243639	39.490535
2686.242051	511751.540787	39.495552
2688.427947	512669.259531	39.500570
2691.228354	513563.032260	39.505588
2693.855085	514473.567583	39.510605
2696.645010	515390.273175	39.515623
2699.533949	516310.487260	39.520640
2701.403284	517251.124400	39.525658
2704.276640	518173.448830	39.530676
2707.187105	519118.387307	39.535693
2709.914786	520062.744052	39.540711
2712.642075	520991.777235	39.545728
2715.192578	521948.794344	39.550746
2717.649963	522893.525632	39.555764
2720.171697	523863.323980	39.560781
2722.550900	524816.058999	39.565799
2725.326694	525789.419780	39.570816
2727.975377	526778.552806	39.575834
2730.727870	527747.862543	39.580852
2733.011236	528750.220853	39.585869
2735.280186	529765.757103	39.590887
2738.161990	530753.027772	39.595904
2740.606586	531775.094036	39.600922
2743.463519	532773.712743	39.605940
2745.985697	533809.720951	39.610957
2748.995505	534827.102184	39.615975
2752.039310	535836.101953	39.620992
2754.865415	536882.713440	39.626010
2757.418763	537901.212705	39.631028
2760.699447	538942.718353	39.636045
2763.344575	539982.391392	39.641063
2766.487556	540990.057810	39.646080
2769.646412	542022.151640	39.651098
2772.768596	543044.819307	39.656116
2775.906755	544053.828400	39.661133
2778.627363	545087.933610	39.666151
2782.084863	546091.663460	39.671168
2784.493356	547117.924559	39.676186
2787.720170	548123.759050	39.681204
2790.509332	549127.832748	39.686221
2793.450673	550132.612924	39.691239
2796.163941	551140.725989	39.696256
2798.735467	552156.279191	39.701274
2801.619469	553154.714057	39.706292
2804.532167	554156.690214	39.711309
2806.818871	555165.430813	39.716327
2810.012292	556157.914037	39.721344
2812.539996	557184.808660	39.726362
2815.028133	558188.565764	39.731380
2817.953098	559212.073743	39.736397
2820.530042	560234.354644	39.741415
2823.177912	561237.604647	39.746432
2825.509250	562230.883976	39.751450
2828.059486	563213.453354	39.756468
2830.909156	564227.393441	39.761485
2833.090712	565233.429621	39.766503
2836.419216	566210.774107	39.771520
2838.630007	567233.676027	39.776538
2841.174966	568248.608914	39.781556
2844.435105	569255.411131	39.786573
2846.976935	570306.985949	39.791591
2849.937394	571311.517641	39.796608
2852.499224	572358.051227	39.801626
2855.875512	573393.071178	39.806644
2858.868373	574433.791470	39.811661
2861.394869	575471.993760	39.816679
2864.808012	576497.168341	39.821696
2867.677540	577544.928332	39.826714
2870.841986	578595.110824	39.831732
2873.806344	579640.221065	39.836749
2876.425118	580703.208920	39.841767
2879.165141	581746.874463	39.846784
2881.540227	582827.025006	39.851802
2884.434777	583883.273746	39.856820
2887.254070	584969.632111	39.861837
2889.938701	586057.771319	39.866855
2892.964157	587131.768719	39.871872
2895.741247	588236.393401	39.876890
2898.538812	589343.119415	39.881908
2901.646707	590439.367084	39.886925
2904.386914	591552.415268	39.891943
2907.360202	592676.847785	39.896960
2910.037882	593784.937229	39.901978
2913.053656	594897.176590	39.906996
2916.460151	596013.355230	39.912013
2919.547779	597128.679198	39.917031
2922.993622	598237.476697	39.922048
2926.638671	599340.576768	39.927066
2929.414387	600473.213692	39.932084
2932.643489	601581.929304	39.937101
2934.834461	602716.446700	39.942119
2937.729462	603827.655835	39.947136
2940.346341	604963.784335	39.952154
2943.411805	606090.916305	39.957172
2946.118066	607226.705280	39.962189
2949.199372	608373.129253	39.967207
2952.115584	609522.517105	39.972224
2955.097914	610672.727875	39.977242
2957.704297	611829.387233	39.982260
2960.786470	612967.489296	39.987277
2963.350811	614120.017037	39.992295
2966.054023	615285.406905	39.997312
2968.834926	616458.863457	40.002330
2971.731708	617641.327485	40.007348
2974.838488	618817.030106	40.012365
2977.640609	619998.656496	40.017383
2981.146100	621156.844414	40.022400
2984.177205	622363.172099	40.027418
2986.625846	623534.327115	40.032436
2989.881268	624741.652908	40.037453
2992.824584	625943.148867	40.042471
2995.695795	627133.480970	40.047488
2998.973122	628321.266041	40.052506
3001.860416	629521.470968	40.057524
3005.435440	630698.452538	40.062541
3008.481196	631901.159490	40.067559
3011.880504	633094.833078	40.072576
3015.461125	634259.383179	40.077594
3018.673630	635432.101989	40.082612
3021.849383	636595.011500	40.087629
3025.368227	637715.210078	40.092647
3028.435648	638827.177657	40.097664
3031.263697	639953.087521	40.102682
3033.896610	641048.420600	40.107700
3036.861921	642166.182692	40.112717
3039.522060	643278.785082	40.117735
3042.490168	644397.051626	40.122752
3045.331337	645531.126225	40.127770
3047.569395	646668.066050	40.132788
3050.593865	647814.671413	40.137805
3052.914153	648978.213982	40.142823
3055.699846	650136.111650	40.147840
3058.600245	651331.639509	40.152858
3061.045651	652524.806841	40.157876
3063.712898	653714.655336	40.162893
3066.341962	654937.004445	40.167911
3069.270516	656161.096351	40.172928
3072.380881	657407.721966	40.177946
3075.258075	658655.722236	40.182964
3078.584221	659899.804287	40.187981
3081.491903	661161.972208	40.192999
3084.782125	662441.289814	40.198016
3087.801269	663698.031476	40.203034
3090.758768	664983.290867	40.208052
3094.063456	666264.738204	40.213069
3097.336350	667538.406042	40.218087
3100.249998	668830.970276	40.223104
3103.968743	670119.943183	40.228122
3107.105852	671421.421848	40.233140
3110.594096	672721.768516	40.238157
3113.725564	674015.679199	40.243175
3117.111325	675299.574722	40.248192
3120.688115	676596.536751	40.253210
3123.615055	677898.197675	40.258228
3126.508019	679200.377956	40.263245
3129.693024	680512.216409	40.268263
3132.694980	681815.352656	40.273280
3135.667230	683123.078710	40.278298
3138.628146	684462.361233	40.283316
3141.617643	685780.831797	40.288333
3144.418821	687108.279822	40.293351
3147.617517	688461.237232	40.298368
3150.936792	689782.597856	40.303386
3153.815928	691125.081776	40.308404
3156.859852	692493.839829	40.313421
3159.600922	693855.839060	40.318439
3162.854464	695219.084104	40.323456
3166.140346	696603.197395	40.328474
3168.870531	697969.380424	40.333492
3172.421903	699333.431641	40.338509
3175.793499	700720.257889	40.343527
3178.863874	702109.492405	40.348544
3181.931523	703480.761641	40.353562
3185.422961	704873.105181	40.358580
3188.791586	706222.978447	40.363597
3192.549139	707619.544192	40.368615
3195.811003	708997.488668	40.373632
3199.313600	710373.686656	40.378650
3202.201666	711759.767602	40.383668
3205.318413	713136.723190	40.388685
3208.617710	714513.475240	40.393703
3211.383841	715910.434013	40.398720
3214.732232	717310.232974	40.403738
3217.404770	718680.668468	40.408756
3220.532020	720084.346318	40.413773
3223.501248	721487.468260	40.418791
3226.585386	722892.956008	40.423808
3229.690216	724275.655194	40.428826
3232.992078	725646.473042	40.433844
3236.209396	727005.016178	40.438861
3238.936601	728385.556150	40.443879
3241.833686	729747.157474	40.448896
3245.276488	731118.964998	40.453914
3248.180590	732506.683736	40.458932
3251.054989	733897.330751	40.463949
3254.203133	735305.124237	40.468967
3257.285470	736716.039747	40.473984
3260.645201	738121.725472	40.479002
3263.941636	739544.102743	40.484020
3267.548700	740930.400642	40.489037
3270.723708	742363.396659	40.494055
3274.203338	743778.029796	40.499072
3277.894549	745211.756436	40.504090
3281.258166	746635.956468	40.509108
3285.150026	748051.479189	40.514125
3289.128091	749472.744802	40.519143
3292.356149	750890.178509	40.524160
3295.696483	752310.981154	40.529178
3298.741303	753740.931723	40.534196
3302.184088	755158.385785	40.539213
3305.483069	756599.732418	40.544231
3308.232765	758046.412838	40.549248
3311.579673	759474.654646	40.554266
3314.546418	760929.219272	40.559284
3317.803888	762381.882470	40.564301
3321.124318	763847.244570	40.569319
3324.909995	765303.637021	40.574336
3328.291642	766769.895319	40.579354
3330.810710	768240.040385	40.584372
3334.555728	769734.470346	40.589389
3337.874217	771206.896763	40.594407
3341.465121	772710.287927	40.599424
3345.655275	774170.973300	40.604442
3348.977802	775643.104074	40.609460
3352.423580	777115.361113	40.614477
3355.835816	778605.789011	40.619495
3358.542649	780091.659215	40.624512
3361.991237	781587.851877	40.629530
3364.693199	783082.631504	40.634548
3368.188127	784580.503151	40.639565
3371.501262	786088.295032	40.644583
3374.713010	787607.261563	40.649600
3378.165266	789123.463016	40.654618
3381.463415	790653.092012	40.659636
3384.675400	792175.691321	40.664653
3388.332111	793708.031885	40.669671
3391.507571	795239.971505	40.674688
3394.761211	796785.962923	40.679706
3398.113164	798327.042923	40.684724
3401.460818	799885.014933	40.689741
3404.870669	801433.034705	40.694759
3408.021092	803004.091840	40.699776
3411.747140	804549.747074	40.704794
3415.103496	806107.636900	40.709812
3418.406175	807665.132762	40.714829
3422.106850	809235.749969	40.719847
3425.515738	810796.375578	40.724864
3428.669545	812356.342370	40.729882
3432.436159	813916.727922	40.734900
3436.142707	815471.145382	40.739917
3439.608979	817043.896310	40.744935
3442.526649	818592.934918	40.749952
3446.608494	820142.496138	40.754970
3450.764035	821690.757148	40.759988
3454.217385	823241.162785	40.765005
3457.701825	824766.660263	40.770010
3461.113245	826228.014528	40.775015
3465.072165	827651.708916	40.780020
3467.946427	829005.978822	40.785024
3471.087068	830281.605387	40.790029
3474.193557	831480.881695	40.795034
3476.958563	832642.923299	40.800039
3480.046667	833703.279911	40.805044
3482.364264	834719.159458	40.810048
3484.858740	835655.131778	40.815053
3487.640644	836497.838999	40.820058
3490.000100	837313.809160	40.825063
3492.153812	838039.285220	40.830068
3494.094175	838708.259770	40.835072
3495.990996	839323.161923	40.840077
3497.934734	839873.698640	40.845082
3499.345192	840382.031241	40.850087
3501.308122	840837.893961	40.855092
3502.885782	841241.062270	40.860096
3504.263553	841577.225422	40.865101
3505.328015	841890.305597	40.870106
3506.586460	842164.665802	40.875111
3507.552154	842392.442384	40.880116
3508.823761	842579.100897	40.885120
3509.522619	842742.539503	40.890125
3510.732414	842867.416482	40.895130
3511.393475	842972.438003	40.900135
3512.267149	843026.809079	40.905140
3513.347827	843077.488549	40.910144
3513.653029	843084.215978	40.915149
3514.581178	843072.360549	40.920154
3515.138780	843040.184123	40.925159
3515.881346	842985.888250	40.930164
3516.413922	842897.444462	40.935168
3516.717529	842805.233669	40.940173
3517.310575	842681.228830	40.945178
3517.471307	842563.339582	40.950183
3517.952897	842399.945756	40.955188
3518.440831	842239.326406	40.960192
3518.442273	842081.514150	40.965197
3519.115148	841892.618720	40.970202
3519.281342	841699.314196	40.975207
3519.450013	841492.151948	40.980212
3519.865468	841271.870777	40.985216
3519.643718	841052.321031	40.990221
3520.059508	840811.976890	40.995226
3520.019092	840569.942758	41.000231
3520.197775	840321.863203	41.005236
3520.827742	840061.747680	41.010240
3520.910401	839797.174641	41.015245
3521.308784	839523.561692	41.020250
3520.885632	839238.265182	41.025255
3521.137726	838962.066425	41.030260
3521.249781	838680.657832	41.035264
3521.283974	838370.557363	41.040269
3521.187274	838082.130137	41.045274
3521.057131	837786.033678	41.050279
3521.266029	837476.202766	41.055284
3521.260375	837174.982042	41.060288
3521.235148	836868.869611	41.065293
3521.355623	836557.105405	41.070298
3520.979539	836252.973843	41.075303
3521.543372	835949.649383	41.080308
3521.268769	835639.077323	41.085312
3521.123783	835318.216792	41.090317
3521.198278	835004.090418	41.095322
3521.254367	834688.194095	41.100327
3521.105296	834357.228565	41.105332
3520.814469	834042.236664	41.110336
3520.416275	833717.187731	41.115341
3520.711126	833404.558716	41.120346
3520.537663	833074.703560	41.125351
3520.629288	832771.454097	41.130356
3520.468119	832438.292295	41.135360
3520.436800	832141.089941	41.140365
3520.444641	831799.222127	41.145370
3519.948727	831507.196134	41.150375
3520.409044	831165.806640	41.155380
3519.986426	830859.523784	41.160384
3520.184255	830538.760721	41.165389
3519.805884	830221.496837	41.170394
3519.716225	829911.987631	41.175399
3519.586408	829590.645530	41.180404
3519.449953	829300.220367	41.185408
3519.118190	828986.651327	41.190413
3519.635368	828669.262167	41.195418
3519.188322	828362.523931	41.200423
3519.146855	828043.876888	41.205428
3519.139854	827746.665561	41.210432
3519.053437	827429.315683	41.215437
3519.245312	827116.597216	41.220442
3518.697136	826802.421454	41.225447
3518.710954	826503.977149	41.230452
3518.817197	826201.397447	41.235456
3518.629024	825895.478865	41.240461
3518.708107	825580.603539	41.245466
3518.041129	825286.420863	41.250471
3518.280708	824983.225313	41.255476
3518.161270	824700.270417	41.260480
3517.802931	824409.714089	41.265485
3517.877037	824098.142924	41.270490
3517.794462	823825.169689	41.275495
3517.743515	823520.243043	41.280500
3517.675063	823229.782661	41.285504
3516.909468	822940.011296	41.290509
3517.291378	822654.831848	41.295514
3517.239559	822389.033595	41.300519
3516.914544	822090.689918	41.305524
3517.089791	821811.965494	41.310528
3516.717565	821535.618904	41.315533
3516.979607	821253.138578	41.320538
3516.569778	820970.218707	41.325543
3516.538920	820712.912048	41.330548
3516.614251	820436.152415	41.335552
3516.302120	820169.623123	41.340557
3516.317431	819889.131728	41.345562
3516.071950	819632.748409	41.350567
3515.994735	819352.151769	41.355572
3515.413897	819083.763601	41.360576
3515.732028	818820.747089	41.365581
3515.750589	818558.797398	41.370586
3515.377784	818307.621185	41.375591
3515.499006	818049.648231	41.380596
3515.491428	817802.210838	41.385600
3514.887003	817538.610518	41.390605
3515.053173	817289.118495	41.395610
3514.572778	817044.374472	41.400615
3514.592223	816785.488352	41.405620
3514.214270	816548.150882	41.410624
3514.284957	816297.658492	41.415629
3514.519929	816057.656732	41.420634
3514.309560	815823.693438	41.425639
3514.292519	815576.909923	41.430644
3514.133326	815352.421270	41.435648
3513.814752	815111.154744	41.440653
3513.543447	814885.444723	41.445658
3513.476957	814654.110458	41.450663
3513.258446	814432.490297	41.455668
3513.431118	814204.921245	41.460672
3513.180247	813980.352958	41.465677
3513.365947	813757.321613	41.470682
3513.117431	813540.917908	41.475687
3513.104674	813318.443544	41.480692
3513.116789	813102.276748	41.485696
3512.916791	812888.783218	41.490701
3512.724684	812650.297966	41.495706
3512.639175	812458.375524	41.500711
3512.553930	812236.563341	41.505716
3512.300496	812038.532814	41.510720
3512.238803	811817.045952	41.515725
3512.590289	811613.955007	41.520730
3512.205451	811416.074914	41.525735
3512.428748	811203.046458	41.530740
3512.090359	810985.301861	41.535744
3511.633842	810794.030385	41.540749
3512.056153	810580.900626	41.545754
3512.134040	810398.693484	41.550759
3511.749691	810194.211150	41.555764
3511.884256	809997.331274	41.560768
3511.720315	809801.720075	41.565773
3511.931525	809588.103897	41.570778
3511.504524	809405.071125	41.575783
3511.562080	809218.473736	41.580788
3511.506611	809009.882620	41.585792
3511.135082	808828.344646	41.590797
3511.430058	808639.829733	41.595802
3511.102258	808451.510228	41.600807
3511.142908	808262.340527	41.605812
3511.132147	808064.546407	41.610816
3511.019108	807885.342785	41.615821
3511.220809	807692.650217	41.620826
3510.950694	807521.698862	41.625831
3511.156845	807322.916085	41.630836
3511.063255	807153.838477	41.635840
3510.870565	806965.946047	41.640845
3510.656686	806781.484047	41.645850
3510.587429	806609.103971	41.650855
3510.248847	806422.789666	41.655860
3510.517428	806245.098307	41.660864
3510.398233	806073.105248	41.665869
3510.372188	805896.679270	41.670874
3509.902479	805719.390120	41.675879
3510.116377	805549.437685	41.680884
3510.207248	805382.100429	41.685888
3509.862402	805219.784020	41.690893
3509.577103	805054.413346	41.695898
3509.364908	804874.411683	41.700903
3509.390563	804726.539482	41.705908
3509.316847	804577.699556	41.710912
3509.513947	804425.378532	41.715917
3509.535681	804268.619669	41.720922
3509.185636	804107.013572	41.725927
3509.317481	803955.477691	41.730932
3509.360640	803791.837432	41.735936
3509.053518	803647.479516	41.740941
3509.027377	803489.288296	41.745946
3508.943237	803345.328808	41.750951
3509.136809	803195.581081	41.755956
3508.988056	803034.652526	41.760960
3508.834397	802898.102715	41.765965
3509.017345	802732.353889	41.770970
3508.598865	802597.215396	41.775975
3508.551357	802444.351270	41.780980
3508.601314	802298.925122	41.785984
3508.391237	802166.393220	41.790989
3508.316044	802017.351117	41.795994
3508.183599	801880.434263	41.800999
3508.239671	801739.754647	41.806004
3508.552432	801608.843255	41.811008
3508.249501	801475.577419	41.816013
3508.366724	801319.962604	41.821018
3508.416126	801199.980141	41.826023
3508.118957	801052.769423	41.831028
3508.180208	800918.255188	41.836032
3508.000760	800801.395038	41.841037
3508.000211	800649.563162	41.846042
3507.724633	800523.733702	41.851047
3507.700499	800393.787289	41.856052
3507.906048	800268.904546	41.861056
3507.560223	800128.454754	41.866061
3507.524583	799999.975189	41.871066
3507.512883	799883.611823	41.876071
3507.284737	799764.288293	41.881076
3507.323287	799651.299269	41.886080
3507.107588	799515.723722	41.891085
3507.505289	799413.175124	41.896090
3507.222298	799287.177249	41.901095
3507.344156	799170.485460	41.906100
3507.542508	799035.814047	41.911104
3507.098100	798932.317210	41.916109
3507.147894	798789.419105	41.921114
3507.185126	798678.427069	41.926119
3507.022175	798567.858945	41.931124
3506.886165	798457.039184	41.936128
3506.875458	798345.853395	41.941133
3506.951850	798227.827892	41.946138
3506.533919	798120.387382	41.951143
3506.565744	798018.565823	41.956148
3506.956704	797904.557686	41.961152
3506.707000	797795.906241	41.966157
3506.621578	797685.016796	41.971162
3506.609052	797576.912012	41.976167
3506.396094	797477.921318	41.981172
3506.802565	797353.444203	41.986176
3506.523218	797252.399186	41.991181
3506.744088	797144.052876	41.996186
3506.432082	797035.792661	42.001191
3506.415860	796929.053242	42.006196
3506.854942	796826.852648	42.011200
3506.261235	796727.668547	42.016205
3506.480401	796622.555124	42.021210
3506.395533	796517.833922	42.026215
3506.273323	796403.542138	42.031220
3505.933188	796307.600247	42.036224
3506.129963	796207.247380	42.041229
3506.056928	796116.856829	42.046234
3505.994005	796011.633393	42.051239
3505.920803	795930.619745	42.056244
3506.413578	795817.935854	42.061248
3506.187643	795730.462853	42.066253
3506.210077	795602.138341	42.071258
3505.862241	795529.759381	42.076263
3505.741309	795423.308936	42.081268
3506.134969	795333.715411	42.086272
3505.523781	795252.880775	42.091277
3505.897743	795148.652892	42.096282
3505.634416	795059.999000	42.101287
3505.750181	794969.808142	42.106292
3506.095666	794876.631443	42.111296
3505.731705	794773.943862	42.116301
3505.560429	794687.725854	42.121306
3505.735170	794598.601062	42.126311
3505.467895	794505.176561	42.131316
3505.707966	794423.455412	42.136320
3505.698971	794338.188735	42.141325
3505.367470	794239.761261	42.146330
3505.581307	794163.247982	42.151335
3505.218256	794064.725018	42.156340
3505.456768	793990.416188	42.161344
3505.399191	793901.369958	42.166349
3505.589185	793816.015061	42.171354
3505.504984	793726.578036	42.176359
3505.351429	793647.074093	42.181364
3505.292009	793557.237855	42.186368
3505.036136	793476.029518	42.191373
3505.132412	793393.534130	42.196378
3504.875903	793300.583118	42.201383
3504.997230	793229.822584	42.206388
3505.042547	793143.402615	42.211392
3504.963996	793070.659233	42.216397
3505.141095	792990.503904	42.221402
3504.999172	792914.232184	42.226407
3505.069347	792842.935792	42.231412
3505.067171	792761.186156	42.236416
3504.895606	792680.298675	42.241421
3504.944191	792595.443604	42.246426
3504.939614	792531.181970	42.251431
3504.607866	792451.055205	42.256436
3505.124780	792366.955478	42.261440
3504.646043	792306.700432	42.266445
3504.858424	792216.261908	42.271450
3504.927949	792150.510629	42.276455
3504.748916	792069.371719	42.281460
3504.790412	792008.291433	42.286464
3504.312187	791937.813254	42.291469
3504.466825	791868.065426	42.296474
3504.331485	791800.231826	42.301479
3504.451757	791735.794994	42.306484
3504.623828	791669.285313	42.311488
3504.171829	791591.330614	42.316493
3504.397406	791523.582327	42.321498
3504.311407	791459.029540	42.326503
3504.255447	791390.834977	42.331508
3504.379513	791330.423180	42.336512
3504.164038	791280.877419	42.341517
3504.319463	791214.661047	42.346522
3504.290920	791145.329394	42.351527
3504.047270	791080.799129	42.356532
3504.264687	791016.290613	42.361536
3504.106200	790945.405897	42.366541
3504.181186	790891.583401	42.371546
3504.003850	790814.066323	42.376551
3503.933875	790768.571830	42.381556
3504.184947	790714.817275	42.386560
3503.992626	790648.112320	42.391565
3503.907813	790581.438174	42.396570
3503.872197	790509.300260	42.401575
3503.813210	790468.175890	42.406580
3504.215856	790403.729588	42.411584
3503.951654	790349.811418	42.416589
3503.843748	790290.755910	42.421594
3503.871338	790235.756744	42.426599
3503.828635	790188.042450	42.431604
3503.963533	790126.045921	42.436608
3503.744019	790068.284772	42.441613
3504.237252	789996.595165	42.446618
3503.797316	789935.723769	42.451623
3503.560941	789880.863632	42.456628
3503.934136	789821.774130	42.461632
3503.359945	789765.395968	42.466637
3503.832484	789720.984995	42.471642
3503.913730	789671.526568	42.476647
3503.832891	789622.291098	42.481652
3503.968795	789562.353817	42.486656
3503.971140	789504.060027	42.491661
3503.531607	789448.443592	42.496666
3503.652280	789398.386951	42.501671
3503.876262	789340.546837	42.506676
3503.728542	789281.047124	42.511680
3503.236676	789242.002233	42.516685
3503.801851	789188.872553	42.521690
3503.421996	789129.999656	42.526695
3503.392675	789074.066954	42.531700
3503.759112	789022.934950	42.536704
3503.412266	788968.626674	42.541709
3503.563623	788900.914761	42.546714
3503.455199	788850.302136	42.551719
3503.438556	788812.307196	42.556724
3503.245211	788761.167206	42.561728
3502.973376	788732.504462	42.566733
3503.388805	788676.544539	42.571738
3503.503083	788631.940009	42.576743
3503.408348	788587.467943	42.581748
3503.623604	788537.635465	42.586752
3503.627389	788492.310890	42.591757
3503.446089	788441.658208	42.596762
3503.576487	788385.988750	42.601767
3503.352951	788348.172892	42.606772
3503.311512	788290.073017	42.611776
3503.245671	788252.328995	42.616781
3503.374769	788196.510793	42.621786
3503.524646	788145.703138	42.626791
3503.080077	788091.207623	42.631796
3503.507529	788046.842819	42.636800
3503.148305	788022.370338	42.641805
3503.372146	787966.534732	42.646810
3503.696399	787915.450906	42.651815
3503.331182	787872.198831	42.656820
3503.400779	787828.334079	42.661824
3503.179449	787785.057775	42.666829
3503.258204	787731.063269	42.671834
3503.525765	787682.297807	42.676839
3503.276498	787636.222853	42.681844
3502.973463	787581.847626	42.686848
3502.972529	787545.465787	42.691853
3502.872922	787502.511874	42.696858
3503.196628	787456.980534	42.701863
3502.927580	787415.135648	42.706868
3503.217470	787376.689246	42.711872
3503.163413	787329.400171	42.716877
3503.309142	787295.303724	42.721882
3503.012149	787252.626655	42.726887
3503.013696	787217.373577	42.731892
3503.228346	787166.990800	42.736896
3503.133444	787134.014905	42.741901
3502.944339	787087.533159	42.746906
3502.984977	787041.111605	42.751911
3502.800505	786995.267685	42.756916
3502.625918	786959.698168	42.761920
3502.370616	786926.354383	42.766925
3502.518242	786888.567993	42.771930
3502.655870	786866.419009	42.776935
3502.704393	786822.551558	42.781940
3502.875357	786786.875094	42.786945
3502.952430	786762.473934	42.791949
3503.028709	786713.044991	42.796954
3502.872540	786675.799225	42.801959
3502.828644	786645.861275	42.806964
3502.895247	786595.941406	42.811969
3502.633015	786577.496080	42.816973
3502.805844	786535.573260	42.821978
3502.829048	786476.956279	42.826983
3502.810819	786458.470455	42.831988
3503.120931	786416.425981	42.836993
3502.687256	786391.861824	42.841997
3502.832273	786340.107858	42.847002
3502.936159	786312.061928	42.852007
3502.575647	786285.960978	42.857012
3503.021410	786240.893541	42.862017
3502.704893	786198.311743	42.867021
3502.885980	786173.203005	42.872026
3502.894760	786118.519417	42.877031
3502.859788	786097.379982	42.882036
3502.886822	786052.183632	42.887041
3502.871741	786010.682097	42.892045
3502.938419	785982.641007	42.897050
3503.006985	785932.027730	42.902055
3502.759514	785896.268229	42.907060
3502.547308	785854.650732	42.912065
3502.734292	785812.623002	42.917069
3503.277837	785789.321940	42.922074
3503.307188	785753.811194	42.927079
3502.896498	785707.455339	42.932084
3503.323979	785665.485490	42.937089
3502.911277	785632.604205	42.942093
3502.983443	785577.512627	42.947098
3503.127513	785545.276910	42.952103
3502.787875	785514.596089	42.957108
3502.995728	785455.448554	42.962113
3503.104611	785431.234343	42.967117
3502.997902	785386.498444	42.972122
3502.997763	785341.744713	42.977127
3502.576951	785317.568187	42.982132
3502.911593	785273.545771	42.987137
3502.938187	785231.786965	42.992141
3502.915772	785196.183625	42.997146
3502.970477	785148.813060	43.002151
3503.205618	785106.969996	43.007156
3503.160101	785056.516884	43.012161
3502.630223	785020.012617	43.017165
3502.684156	784982.772628	43.022170
3502.234555	784956.927421	43.027175
3502.613558	784925.683064	43.032180
3502.226294	784882.121442	43.037185
3502.516790	784867.515324	43.042189
3502.152436	784822.965902	43.047194
3502.891728	784800.072053	43.052199
3502.540941	784784.981191	43.057204
3502.600150	784743.656831	43.062209
3502.211495	784735.113594	43.067213
3502.323513	784686.599305	43.072218
3502.555548	784665.264119	43.077223
3502.509349	784621.546367	43.082228
3502.467153	784592.780010	43.087233
3502.141808	784565.535739	43.092237
3502.394932	784538.638752	43.097242
3502.440614	784507.545856	43.102247
3502.132940	784479.757305	43.107252
3502.307903	784448.446115	43.112257
3502.076814	784436.581092	43.117261
3502.116045	784397.668162	43.122266
3502.561904	784374.280245	43.127271
3502.200821	784355.402798	43.132276
3502.555057	784322.094057	43.137281
3502.181179	784303.218580	43.142285
3502.207449	784259.831004	43.147290
3502.335549	784243.971498	43.152295
3502.092915	784205.448270	43.157300
3502.277817	784178.954680	43.162305
3502.318541	784161.240239	43.167309
3502.384213	784133.093723	43.172314
3502.343577	784107.178091	43.177319
3501.996405	784082.050687	43.182324
3502.413238	784048.877940	43.187329
3502.341576	784025.820082	43.192333
3502.222985	784013.099614	43.197338
3502.413695	783978.783250	43.202343
3502.396086	783957.241142	43.207348
3502.242775	783905.567972	43.212353
3502.338688	783900.190454	43.217357
3502.323255	783870.137862	43.222362
3502.514173	783832.574217	43.227367
3502.044722	783797.381920	43.232372
3502.303035	783779.729082	43.237377
3502.038320	783757.882744	43.242381
3502.263673	783730.052688	43.247386
3501.901718	783699.466167	43.252391
3502.011088	783685.428597	43.257396
3502.272633	783653.755354	43.262401
3502.318257	783636.924267	43.267405
3502.031053	783600.766345	43.272410
3502.126430	783579.745609	43.277415
3502.055963	783554.226438	43.282420
3502.289669	783544.693805	43.287425
3502.190546	783508.504441	43.292429
3502.222161	783486.018155	43.297434
3501.726736	783452.550196	43.302439
3501.580873	783435.209055	43.307444
3502.208548	783415.575956	43.312449
3502.026495	783389.041522	43.317453
3502.181849	783374.897387	43.322458
3502.377740	783334.034361	43.327463
3501.942013	783324.316540	43.332468
3501.913219	783295.936346	43.337473
3501.809990	783274.603076	43.342477
3502.123868	783256.497060	43.347482
3502.096846	783233.576897	43.352487
3502.003550	783223.261396	43.357492
3502.107754	783165.243595	43.362497
3501.983405	783161.574436	43.367501
3502.224755	783147.464886	43.372506
3501.830447	783139.019064	43.377511
3502.038374	783117.388101	43.382516
3502.116427	783084.168335	43.387521
3501.864320	783064.236439	43.392525
3501.934121	783044.497443	43.397530
3502.006060	783037.647360	43.402535
3501.916065	783004.897671	43.407540
3502.040233	782983.427692	43.412545
3501.982844	782967.743524	43.417549
3501.954123	782942.510490	43.422554
3501.996376	782927.203393	43.427559
3501.808583	782900.569713	43.432564
3501.998220	782878.793458	43.437569
3502.185977	782871.432171	43.442573
3501.992779	782849.079325	43.447578
3501.921724	782820.704223	43.452583
3501.892134	782807.376597	43.457588
3501.845171	782780.620883	43.462593
3502.052710	782759.579284	43.467597
3502.085924	782740.534253	43.472602
3501.804061	782711.111090	43.477607
3502.148432	782689.161184	43.482612
3502.179992	782677.348390	43.487617
3501.871527	782647.338969	43.492621
3502.005208	782624.488799	43.497626
3501.995705	782601.416148	43.502631
3501.872193	782588.497179	43.507636
3501.986013	782557.778244	43.512641
3501.794635	782537.392096	43.517645
3501.823926	782528.039393	43.522650
3501.944481	782504.059420	43.527655
3501.825007	782479.971306	43.532660
3501.828863	782468.753130	43.537665
3501.793064	782444.306717	43.542669
3501.672394	782447.770565	43.547674
3501.913977	782417.177587	43.552679
3501.733694	782404.907241	43.557684
3501.666654	782366.050055	43.562689
3501.765942	782365.984482	43.567693
3501.574749	782333.100814	43.572698
3501.656097	782331.217773	43.577703
3501.681569	782329.442337	43.582708
3502.011884	782300.605474	43.587713
3502.077220	782296.265019	43.592717
3502.113570	782268.558869	43.597722
3502.108376	782239.285015	43.602727
3501.829445	782216.009505	43.607732
3501.660879	782182.727814	43.612737
3501.841427	782169.019987	43.617741
3501.775138	782162.585457	43.622746
3501.973735	782138.148601	43.627751
3501.250003	782132.757173	43.632756
3501.817989	782131.384347	43.637761
3501.909261	782107.949107	43.642765
3501.508412	782071.457821	43.647770
3502.038047	782068.566027	43.652775
3501.724879	782054.644091	43.657780
3502.008232	782023.648950	43.662785
3501.814077	782013.987969	43.667789
3501.917988	781979.873218	43.672794
3502.143687	781979.048776	43.677799
3501.629643	781945.773696	43.682804
3501.703777	781929.081544	43.687809
3502.116257	781920.255378	43.692813
3501.733621	781879.627034	43.697818
3501.978824	781869.942694	43.702823
3501.792017	781861.854819	43.707828
3501.999193	781835.496580	43.712833
3501.717986	781836.034921	43.717837
3501.642300	781800.177562	43.722842
3501.841468	781785.137426	43.727847
3501.577106	781767.811796	43.732852
3501.567291	781762.154879	43.737857
3501.451684	781727.484643	43.742861
3501.626202	781725.192461	43.747866
3501.900333	781715.011102	43.752871
3501.708681	781703.676328	43.757876
3501.754573	781668.191928	43.762881
3501.732906	781680.004705	43.767885
3501.504256	781655.488980	43.772890
3501.663841	781616.196794	43.777895
3501.129724	781623.763986	43.782900
3501.510117	781621.683888	43.787905
3501.447181	781601.372352	43.792909
3501.537767	781560.565856	43.797914
3501.311336	781559.569812	43.802919
3501.562142	781554.263451	43.807924
3501.764322	781543.946086	43.812929
3501.593273	781542.448857	43.817933
3501.361774	781529.742605	43.822938
3501.487997	781532.526543	43.827943
3501.166569	781526.723945	43.832948
3501.491860	781522.438621	43.837953
3501.501415	781492.322811	43.842957
3501.334644	781474.242307	43.847962
3501.349589	781470.008070	43.852967
3501.598349	781467.801992	43.857972
3501.635511	781441.962391	43.862977
3501.877834	781436.312895	43.867981
3501.665291	781421.930302	43.872986
3501.620122	781391.478640	43.877991
3501.416143	781378.619968	43.882996
3501.981035	781357.170985	43.888001
3501.712886	781366.761338	43.893005
3501.863399	781336.326419	43.898010
3501.892394	781328.399229	43.903015
3501.626857	781316.436321	43.908020
3501.824085	781283.483901	43.913025
3501.826733	781282.892954	43.918029
3501.721156	781275.381534	43.923034
3502.010747	781234.934088	43.928039
3501.650051	781237.798343	43.933044
3501.878981	781199.821096	43.938049
3501.690668	781184.892750	43.943053
3501.622151	781188.840691	43.948058
3501.847448	781164.839032	43.953063
3501.548053	781149.436824	43.958068
3501.769071	781137.295058	43.963073
3501.639741	781119.994842	43.968077
3501.950210	781090.270676	43.973082
3502.053828	781083.807200	43.978087
3501.890062	781053.029186	43.983092
3501.864070	781038.811941	43.988097
3501.890299	781026.603656	43.993101
3501.565719	781006.678016	43.998106
3501.884425	780986.793991	44.003111
3501.521258	780972.386105	44.008116
3501.935282	780947.860544	44.013121
3501.709520	780934.118889	44.018125
3501.900416	780927.050376	44.023130
3502.001461	780890.273618	44.028135
3501.787787	780874.020126	44.033140
3501.636552	780868.730279	44.038145
3501.804707	780846.754614	44.043149
3501.780171	780848.579434	44.048154
3502.011205	780811.485602	44.053159
3501.910239	780800.085263	44.058164
3502.137406	780774.064351	44.063169
3502.132519	780751.329521	44.068173
3501.904987	780741.573912	44.073178
3501.625950	780707.220980	44.078183
3501.570879	780700.734090	44.083188
3501.985983	780675.223198	44.088193
3502.118542	780658.469285	44.093197
3501.853957	780643.109476	44.098202
3501.938671	780612.829997	44.103207
3501.478739	780607.049470	44.108212
3501.815686	780593.411331	44.113217
3501.779187	780584.362230	44.118221
3501.565494	780563.088366	44.123226
3501.856033	780553.296381	44.128231
3501.554223	780535.038924	44.133236
3501.440854	780498.443136	44.138241
3501.414161	780503.860953	44.143245
3501.499110	780495.382293	44.148250
3501.748208	780489.730949	44.153255
3501.484119	780464.823323	44.158260
3501.632057	780426.560093	44.163265
3502.021274	780437.175302	44.168269
3501.462217	780412.316082	44.173274
3501.603808	780402.892925	44.178279
3501.588855	780399.647264	44.183284
3501.701831	780380.632103	44.188289
3501.344693	780365.237735	44.193293
3501.337728	780355.100776	44.198298
3501.469282	780332.539016	44.203303
3501.579312	780346.497697	44.208308
3501.576221	780331.143368	44.213313
3501.599352	780307.664319	44.218317
3501.411919	780298.246008	44.223322
3501.743055	780280.867943	44.228327
3501.454765	780266.889247	44.233332
3501.665534	780238.506816	44.238337
3501.766566	780233.027307	44.243341
3501.440492	780215.855768	44.248346
3501.870985	780192.604540	44.253351
3501.431383	780187.952274	44.258356
3501.600885	780182.018512	44.263361
3501.674651	780170.932909	44.268365
3501.430489	780148.580110	44.273370
3501.638849	780129.548581	44.278375
3501.246774	780125.872759	44.283380
3501.474945	780125.047708	44.288385
3501.704475	780102.124585	44.293389
3501.522892	780097.528193	44.298394
3501.814002	780085.077832	44.303399
3501.674253	780061.083441	44.308404
3501.861569	780046.730685	44.313409
3501.554069	780033.837460	44.318413
3501.516365	780024.984725	44.323418
3501.775295	779992.705313	44.328423
3501.580494	780000.316721	44.333428
3501.712674	779979.574772	44.338433
3501.858259	779964.588912	44.343437
3501.511114	779958.001817	44.348442
3501.429093	779947.384484	44.353447
3501.683532	779930.707252	44.358452
3501.312483	779898.432756	44.363457
3501.769465	779904.608042	44.368461
3501.554369	779898.983484	44.373466
3501.981496	779866.331287	44.378471
3501.660539	779868.451266	44.383476
3501.557532	779849.716379	44.388481
3501.596981	779815.848158	44.393485
3501.601371	779810.827209	44.398490
3501.785593	779800.510331	44.403495
3501.756325	779792.886369	44.408500
3501.739727	779759.223988	44.413505
3501.715004	779764.100632	44.418509
3501.478005	779757.938174	44.423514
3501.779394	779720.138130	44.428519
3501.303649	779713.719649	44.433524
3501.771140	779714.725433	44.438529
3501.942546	779694.665268	44.443533
3501.708829	779669.356160	44.448538
3501.601984	779666.863588	44.453543
3501.455350	779634.403296	44.458548
3501.800805	779608.850922	44.463553
3501.885401	779606.769767	44.468557
3501.707485	779602.320114	44.473562
3501.927851	779568.519380	44.478567
3501.774435	779560.669526	44.483572
3501.709699	779546.997155	44.488577
3501.705934	779510.181457	44.493581
3501.741368	779498.362846	44.498586
3501.981454	779478.832193	44.503591
3501.595410	779473.186241	44.508596
3501.755339	779456.178951	44.513601
3501.796737	779442.981104	44.518605
3501.394851	779419.470754	44.523610
3502.024435	779400.515600	44.528615
3501.799345	779404.982503	44.533620
3501.661932	779366.859140	44.538625
3502.080751	779370.580133	44.543629
3501.602553	779348.164977	44.548634
3501.847041	779330.109826	44.553639
3501.754440	779314.669652	44.558644
3501.689222	779298.142068	44.563649
3501.637361	779281.415361	44.568653
3501.416532	779264.765669	44.573658
3501.631282	779268.471107	44.578663
3501.629011	779231.998305	44.583668
3501.236741	779219.659032	44.588673
3501.506165	779213.511137	44.593677
3501.531657	779198.346595	44.598682
3501.888183	779190.067792	44.603687
3501.370334	779175.435696	44.608692
3501.341511	779164.857679	44.613697
3501.595238	779162.453207	44.618701
3501.163177	779146.379480	44.623706
3501.316461	779115.491805	44.628711
3501.212419	779111.521905	44.633716
3501.530718	779111.961684	44.638721
3501.752618	779095.386346	44.643725
3501.446533	779083.770984	44.648730
3501.708058	779067.435170	44.653735
3501.392079	779060.546785	44.658740
3501.401192	779052.768057	44.663745
3501.683195	779047.110179	44.668749
3501.270504	779023.354211	44.673754
3501.544128	779020.454184	44.678759
3501.351676	779024.669828	44.683764
3501.273502	779007.897603	44.688769
3501.490320	778985.662187	44.693773
3501.370744	778983.073029	44.698778
3501.508134	778961.441301	44.703783
3501.688349	778966.481617	44.708788
3501.683540	778941.673728	44.713793
3501.766082	778928.369725	44.718797
3501.404251	778907.706094	44.723802
3501.366751	778906.038642	44.728807
3501.398355	778887.968238	44.733812
3501.464274	778876.389717	44.738817
3501.483779	778865.409512	44.743821
3501.344060	778879.166030	44.748826
3501.635701	778849.780385	44.753831
3501.310853	778835.804952	44.758836
3501.672302	778805.078571	44.763841
3501.793084	778800.628449	44.768845
3501.393801	778791.095401	44.773850
3501.618035	778765.117017	44.778855
3501.564581	778764.978129	44.783860
3501.751285	778764.258211	44.788865
3501.729361	778743.390451	44.793869
3501.502452	778725.362226	44.798874
3501.647436	778712.589019	44.803879
3501.299819	778706.394660	44.808884
3501.290619	778687.099849	44.813889
3501.459452	778656.601472	44.818893
3501.504228	778661.418181	44.823898
3501.301963	778653.132363	44.828903
3501.498086	778668.606079	44.833908
3501.769573	778640.108968	44.838913
3501.817200	778617.309590	44.843917
3501.646279	778625.558432	44.848922
3501.427359	778603.245945	44.853927
3501.685010	778580.559536	44.858932
3501.418219	778569.035329	44.863937
3501.681673	778561.017278	44.868941
3501.573072	778550.106925	44.873946
3501.382280	778514.990695	44.878951
3501.497869	778521.666439	44.883956
3501.369936	778521.638268	44.888961
3501.565352	778504.622914	44.893965
3501.522168	778488.434448	44.898970
3501.714082	778468.416759	44.903975
3501.518584	778480.017236	44.908980
3501.312189	778463.166423	44.913985
3501.596946	778425.313180	44.918989
3501.663398	778435.246086	44.923994
3501.742849	778429.719550	44.928999
3501.548120	778399.427664	44.934004
3501.444196	778372.960437	44.939009
3501.488245	778381.321828	44.944013
3501.132278	778371.978003	44.949018
3501.689822	778373.707565	44.954023
3501.867354	778359.353101	44.959028
3501.369260	778340.531722	44.964033
3501.336180	778325.325784	44.969037
3501.541093	778321.452245	44.974042
3501.835090	778292.408564	44.979047
3501.647880	778290.962543	44.984052
3501.381889	778285.394342	44.989057
3501.602034	778246.713938	44.994061
3501.254968	778240.174491	44.999066
3501.317035	778231.500053	45.004071
3501.251948	778228.458594	45.009076
3500.858126	778246.984086	45.014081
3501.753772	778227.292875	45.019085
3501.317821	778215.648286	45.024090
3501.237226	778208.572632	45.029095
3501.331600	778190.047103	45.034100
3501.129417	778176.099425	45.039105
3501.373894	778176.305282	45.044109
3501.320623	778178.332419	45.049114
3501.452391	778165.708120	45.054119
3501.297728	778142.645205	45.059124
3501.410743	778134.159176	45.064129
3501.217712	778122.474425	45.069133
3501.217718	778125.723529	45.074138
3501.310570	778133.289500	45.079143
3501.242075	778123.356483	45.084148
3501.121386	778108.607586	45.089153
3501.255073	778076.783386	45.094157
3500.933890	778092.934288	45.099162
3501.174671	778076.747364	45.104167
3501.213621	778078.660880	45.109172
3501.190974	778076.646185	45.114177
3501.493855	778062.812015	45.119181
3501.248303	778078.408967	45.124186
3501.230668	778037.846674	45.129191
3501.250231	778035.086569	45.134196
3500.961705	778017.559037	45.139201
3501.377895	778030.634827	45.144205
3500.957697	778026.076423	45.149210
3501.149796	778028.260104	45.154215
3501.335709	778028.574072	45.159220
3501.486349	778020.426323	45.164225
3501.553233	777996.144936	45.169229
3501.242624	777991.223849	45.174234
3501.498819	777971.883431	45.179239
3501.444934	777976.470693	45.184244
3501.224796	777955.190255	45.189249
3501.288195	777926.576946	45.194253
3501.032922	777931.000486	45.199258
3501.497692	777919.994747	45.204263
3501.290857	777925.641075	45.209268
3501.039504	777926.568608	45.214273
3501.330716	777921.942187	45.219277
3501.056808	777937.494879	45.224282
3501.213855	777904.976857	45.229287
3501.283233	777892.066978	45.234292
3501.271448	777887.441213	45.239297
3501.265107	777871.146848	45.244301
3500.915198	777888.139858	45.249306
3501.486289	777876.673464	45.254311
3501.262871	777875.676400	45.259316
3501.217382	777860.373074	45.264321
3501.311488	777828.406619	45.269325
3501.114434	777821.349772	45.274330
3501.283739	777827.278838	45.279335
3501.408144	777820.759815	45.284340
3501.368983	777824.704742	45.289345
3501.722249	777803.280181	45.294349
3501.574706	777788.978142	45.299354
3501.342630	777768.191439	45.304359
3501.756039	777764.627886	45.309364
3501.075709	777766.315339	45.314369
3501.161460	777736.417582	45.319373
3500.790947	777744.552597	45.324378
3501.201602	777741.087950	45.329383
3501.694191	777728.009608	45.334388
3501.315618	777721.474882	45.339393
3501.700363	777728.107020	45.344397
3501.408367	777712.253206	45.349402
3501.438792	777693.687720	45.354407
3501.260411	777692.387819	45.359412
3500.991353	777685.441165	45.364417
3501.404905	777667.649452	45.369421
3501.465358	777672.661161	45.374426
3501.319440	777655.896984	45.379431
3501.132350	777640.911916	45.384436
3501.145688	777633.574070	45.389441
3501.416124	777629.147818	45.394445
3501.355445	777635.558015	45.399450
3501.075684	777633.585548	45.404455
3501.051919	777620.395137	45.409460
3501.192718	777619.338044	45.414465
3501.257863	777590.033873	45.419469
3501.127016	777603.545167	45.424474
3501.191077	777589.404812	45.429479
3501.384315	777589.372965	45.434484
3500.979793	777592.344310	45.439489
3501.030424	777584.704876	45.444493
3501.283093	777594.165160	45.449498
3501.521465	777564.684656	45.454503
3501.312282	777562.158983	45.459508
3501.026219	777544.974538	45.464513
3501.377488	777553.778604	45.469517
3500.937489	777545.826080	45.474522
3501.201041	777535.049840	45.479527
3500.892560	777541.894801	45.484532
3500.901414	777538.742407	45.489537
3501.351107	777547.973366	45.494541
3501.066307	777552.008133	45.499546
3500.906140	777522.297706	45.504551
3501.149857	777499.216371	45.509556
3501.088281	777490.856821	45.514561
3501.172448	777472.971190	45.519565
3501.374269	777510.601483	45.524570
3501.400701	777488.146703	45.529575
3501.087996	777494.549302	45.534580
3501.094696	777494.498947	45.539585
3501.285873	777486.836261	45.544589
3500.914422	777464.299244	45.549594
3501.217473	777437.663123	45.554599
3501.336007	777437.594347	45.559604
3501.149095	777441.563817	45.564609
3501.241413	777425.990714	45.569613
3501.108169	777436.942549	45.574618
3501.065065	777433.503267	45.579623
3501.320277	777439.763135	45.584628
3501.272774	777438.589332	45.589633
3501.559387	777411.118847	45.594637
3501.251863	777406.738427	45.599642
3501.498241	777391.681449	45.604647
3501.468748	777413.398485	45.609652
3501.298475	777405.352145	45.614657
3501.356465	777368.318524	45.619661
3501.314050	777351.290427	45.624666
3501.379766	777353.052021	45.629671
3501.667698	777328.633539	45.634676
3501.372749	777329.962201	45.639681
3501.715391	777308.341004	45.644685
3501.027104	777305.795687	45.649690
3501.505538	777297.543906	45.654695
3501.241486	777287.248085	45.659700
3501.229105	777294.930729	45.664705
3501.605085	777254.890072	45.669709
3501.250356	777258.985752	45.674714
3501.198165	777237.872498	45.679719
3501.514866	777257.021984	45.684724
3501.238694	777253.522536	45.689729
3501.858182	777236.335911	45.694733
3501.288521	777216.637179	45.699738
3501.337606	777211.016255	45.704743
3501.119526	777191.505720	45.709748
3501.415194	777194.952716	45.714753
3501.566683	777191.382796	45.719757
3501.535437	777184.150313	45.724762
3501.366542	777162.612945	45.729767
3501.592456	777154.451834	45.734772
3501.468219	777146.545332	45.739777
3501.733034	777123.754753	45.744781
3501.419141	777111.103570	45.749786
3501.705401	777103.227878	45.754791
3501.538957	777090.847789	45.759796
3501.691086	777063.988987	45.764801
3501.586335	777071.194718	45.769805
3501.232802	777054.906484	45.774810
3501.450442	777032.074154	45.779815
3501.677050	776956.556868	45.784820
3500.984834	776840.224421	45.789825
3501.330274	776653.406182	45.794829
3501.243694	776435.632884	45.799834
3500.760335	776136.767245	45.804839
3501.072906	775782.751970	45.809844
3500.515554	775382.915060	45.814849
3500.468958	774920.473394	45.819853
3499.908409	774395.485474	45.824858
3499.837782	773815.998685	45.829863
3499.884630	773178.908801	45.834868
3499.306538	772498.709209	45.839873
3498.762342	771718.124177	45.844877
3498.717788	770925.646536	45.849882
3498.107261	770050.579365	45.854887
3497.838043	769140.259111	45.859892
3497.029475	768165.832393	45.864897
3496.530738	767108.547409	45.869901
3496.302750	766016.699563	45.874906
3495.739164	764834.842720	45.879911
3495.029578	763622.045136	45.884916
3494.351992	762344.814853	45.889921
3493.985816	760989.652641	45.894925
3492.991758	759569.207602	45.899930
3492.447289	758108.095294	45.904935
3491.720860	756588.278222	45.909940
3490.525173	755002.165106	45.914945
3489.784492	753336.870111	45.919949
3488.857076	751635.923763	45.924954
3488.213843	749885.094139	45.929959
3487.610190	748051.027329	45.934964
3486.486002	746176.275145	45.939969
3485.644356	744207.865927	45.944973
3484.608278	742222.823428	45.949978
3483.464938	740146.416119	45.954983
3482.325931	738018.048550	45.959988
3481.079388	735846.957446	45.964993
3480.349276	733612.360644	45.969997
3478.950388	731337.336254	45.975002
3477.900789	728977.939249	45.980007
3476.744693	726573.277082	45.985012
3475.325657	724128.644309	45.990017
3474.049329	721596.190036	45.995021
3472.678486	719041.056721	46.000026
3471.739376	716409.008258	46.005031
3470.204285	713732.707531	46.010036
3468.585207	711000.862704	46.015041
3467.509478	708190.874010	46.020045
3465.694179	705348.740182	46.025050
3464.116184	702452.159260	46.030055
3462.810891	699498.940650	46.035060
3461.666817	696519.241190	46.040065
3460.118548	693445.176957	46.045069
3458.346477	690364.617774	46.050074
3456.757613	687192.367461	46.055079
3455.299097	683985.221927	46.060084
3453.732292	680722.767456	46.065089
3452.094629	677395.031645	46.070093
3450.424660	674020.295647	46.075098
3448.609659	670595.645860	46.080103
3446.844096	667132.033823	46.085108
3444.853646	663604.719124	46.090113
3443.219671	660024.532989	46.095117
3441.311596	656414.359985	46.100122
3439.360205	652737.118420	46.105127
3437.767256	649018.323600	46.110132
3435.442554	645250.473371	46.115137
3433.385701	641424.509805	46.120141
3431.245307	637567.062897	46.125146
3429.151768	633669.882764	46.130151
3427.533845	629716.996803	46.135156
3425.487955	625721.083115	46.140161
3423.500896	621673.962869	46.145165
3421.265087	617586.426705	46.150170
3418.974583	613425.216037	46.155175
3417.135776	609246.927933	46.160180
3414.798391	605004.140986	46.165185
3412.573004	600721.406059	46.170189
3409.938005	596399.590078	46.175194
3407.812604	592029.074514	46.180199
3405.657092	587619.920006	46.185204
3402.987183	583171.030948	46.190209
3400.750218	578687.513377	46.195213
3398.244233	574152.462533	46.200218
3396.161871	569572.780975	46.205223
3393.576078	564969.546874	46.210228
3391.037651	560310.735032	46.215233
3388.620138	555610.511552	46.220237
3386.300955	550865.336046	46.225242
3383.485074	546078.717132	46.230247
3381.020187	541262.607499	46.235252
3378.610076	536403.280369	46.240257
3376.074278	531496.966460	46.245261
3373.091457	526585.005544	46.250266
3370.852838	521596.413728	46.255271
3368.194096	516582.421358	46.260276
3365.103450	511531.009975	46.265281
3362.502229	506438.082225	46.270285
3359.944916	501334.202399	46.275290
3357.173971	496172.238525	46.280295
3354.461485	490976.316786	46.285300
3351.214406	485751.349401	46.290305
3348.671278	480485.801518	46.295309
3345.529872	475195.540222	46.300314
3342.933598	469872.237448	46.305319
3339.943731	464500.349411	46.310324
3336.979720	459132.219552	46.315329
3333.986153	453682.211898	46.320333
3331.213023	448250.882095	46.325338
3327.947617	442768.093036	46.330343
3324.993030	437244.269596	46.335348
3321.989722	431709.580163	46.340353
3318.897920	426142.846709	46.345357
3315.702873	420532.135114	46.350362
3312.377582	414917.561138	46.355367
3309.507046	409253.504513	46.360372
3305.880995	403586.770178	46.365377
3302.987778	397885.954257	46.370381
3299.761395	392175.046131	46.375386
3296.137306	386409.029889	46.380391
3293.327211	380645.611781	46.385396
3289.801667	374851.198206	46.390401
3286.524419	369042.422342	46.395405
3283.132951	363203.157977	46.400410
3279.820938	357338.979716	46.405415
3276.450272	351465.927208	46.410420
3272.681402	345557.893838	46.415425
3269.453244	339639.880117	46.420429
3266.136941	333713.004320	46.425434
3262.341335	327748.183344	46.430439
3259.285565	321800.904593	46.435444
3255.049091	315812.247974	46.440449
3251.827250	309808.932928	46.445453
3248.067240	303811.329353	46.450458
3244.570122	297785.899724	46.455463
3241.141886	291767.968410	46.460468
3237.263133	285725.715336	46.465473
3233.571878	279660.537878	46.470477
3230.154069	273606.702771	46.475482
3226.318107	267529.615074	46.480487
3222.437558	261446.840129	46.485492
3218.241109	255366.576436	46.490497
3214.669654	249265.140583	46.495501
3210.983123	243167.210403	46.500506
3206.886040	237074.137663	46.505511
3203.087419	230951.838335	46.510516
3198.960610	224855.631106	46.515521
3195.036901	218753.702351	46.520525
3190.923592	212642.456037	46.525530
3187.328946	206446.524605	46.530535
3183.448431	200332.098666	46.535540
3179.349612	194217.467219	46.540545
3175.387470	188099.815490	46.545549
3170.969406	182003.933171	46.550554
3166.866982	175902.832203	46.555559
3163.142303	169812.067540	46.560564
3158.436570	163708.510581	46.565569
3154.208862	157631.827109	46.570573
3149.454815	151568.404062	46.575578
3145.028013	145511.004641	46.580583
3140.931985	139476.929711	46.585588
3136.096282	133460.284895	46.590593
3131.854212	127440.729596	46.595597
3127.109424	121455.113713	46.600602
3122.543820	115492.244255	46.605607
3117.927136	109540.019836	46.610612
3112.969102	103609.998580	46.615617
3108.150385	97714.127178	46.620621
3103.165018	91849.952183	46.625626
3097.221771	86023.163539	46.630631
3091.985326	80233.541060	46.635636
3085.684667	74509.928182	46.640641
3078.575962	68857.286662	46.645645
3065.786621	63425.255281	46.650650
3049.671462	58197.648288	46.655655
3034.038108	53165.306075	46.660660
3018.039037	48360.304521	46.665665
3003.281791	43775.403631	46.670669
2988.737940	39454.465373	46.675674
2974.929637	35392.341670	46.680679
2961.754778	31575.904732	46.685684
2949.309598	28018.729479	46.690689
2937.744325	24702.615685	46.695693
2926.102367	21630.090230	46.700698
2914.910259	18789.446063	46.705703
2904.019430	16171.285687	46.710708
2891.409351	13816.571136	46.715713
2876.537834	11765.294780	46.720717
2861.599721	9968.782273	46.725722
2846.538181	8439.342327	46.730727
2832.738431	7150.254106	46.735732
2820.817194	6098.788718	46.740737
2810.816881	5233.829769	46.745741
2802.373969	4545.815840	46.750746
2795.784119	4021.168022	46.755751
2790.467805	3601.044832	46.760756
2786.120394	3298.019044	46.765761
2782.592700	3057.159463	46.770765
2780.057854	2880.894453	46.775770
2777.862121	2729.751827	46.780775
2776.011478	2603.153214	46.785780
2774.072231	2495.500923	46.790785
2772.342253	2390.738751	46.795789
2770.769081	2301.009594	46.800794
2769.001866	2184.490475	46.805799
2767.656456	2070.444452	46.810804
2765.688138	1949.924820	46.815809
2764.190979	1820.460858	46.820813
2762.018878	1682.862558	46.825818
2759.621727	1537.004269	46.830823
2757.049298	1366.888756	46.835828
2754.616941	1208.442864	46.840833
2751.979001	1020.602963	46.845837
2748.970316	839.668546	46.850842
2745.765831	661.734112	46.855847
2742.823835	477.994318	46.860852
2739.070911	313.594081	46.865857
2734.936342	139.543045	46.870861
2723.246896	212.458853	46.875866
2715.424122	231.466223	46.880871
2711.371768	235.038242	46.885876
2709.158718	241.334073	46.890881
2707.524917	226.642185	46.895885
2705.729013	238.128551	46.900890
2702.823430	229.496622	46.905895
2700.268045	221.330249	46.910900
2697.037343	226.945195	46.915905
2693.621499	229.650830	46.920909
2690.345914	228.331343	46.925914
2686.950732	224.428658	46.930919
2683.481804	217.969650	46.935924
2680.320043	223.313466	46.940929
2676.643553	222.402233	46.945933
2673.385717	215.996530	46.950938
2670.023206	229.833938	46.955943
2667.196511	216.850700	46.960948
2663.460345	214.095613	46.965953
2660.183976	225.481551	46.970957
2656.428626	217.144849	46.975962
2653.007656	216.124706	46.980967
2650.058796	219.108436	46.985972
2646.564405	218.989120	46.990977
2643.575396	212.474094	46.995981
2639.965331	219.540524	47.000986
2636.381907	210.893129	47.005991
2633.424873	216.388978	47.010996
2630.073619	219.919234	47.016001
2626.997446	210.211882	47.021005
2623.102445	213.361092	47.026010
2618.949294	212.089152	47.031015
2615.759634	212.071540	47.036020
2612.074219	213.673168	47.041025
2608.661581	197.017629	47.046029
2605.764057	204.951588	47.051034
2602.564221	205.897384	47.056039
2598.964110	208.828191	47.061044
2595.227025	207.031070	47.066049
2591.403317	222.023666	47.071053
2588.378097	216.937194	47.076058
2584.741009	205.524199	47.081063
2581.953980	211.215691	47.086068
2578.588927	212.437358	47.091073
2574.923911	207.086124	47.096077
2571.544907	209.669808	47.101082
2567.577057	202.716868	47.106087
2564.328479	196.331702	47.111092
2561.233962	202.043413	47.116097
2557.662752	218.094722	47.121101
2554.136088	208.832053	47.126106
2550.135011	207.074242	47.131111
2546.406954	212.606091	47.136116
2543.017870	209.463034	47.141121
2540.361085	212.477567	47.146125
2536.831598	214.659578	47.151130
2533.127562	201.418265	47.156135
2530.005860	217.259312	47.161140
2526.457624	207.410336	47.166145
2522.813749	203.633985	47.171149
2519.373590	205.063011	47.176154
2515.969633	206.694930	47.181159
2512.749072	203.843359	47.186164
2509.147265	203.814825	47.191169
2505.270637	199.514017	47.196173
2501.938080	199.872128	47.201178
2498.174653	209.347784	47.206183
2495.066081	191.071242	47.211188
2491.523079	208.247252	47.216193
2487.843080	211.962988	47.221197
2484.439230	207.380498	47.226202
2481.021311	212.553025	47.231207
2477.663161	201.481730	47.236212
2474.064967	213.578442	47.241217
2470.660974	204.768267	47.246221
2467.633529	196.587010	47.251226
2463.888832	209.724557	47.256231
2460.425952	195.888868	47.261236
2456.456163	198.791706	47.266241
2452.973789	212.119031	47.271245
2449.706954	200.186500	47.276250
2446.156257	198.078333	47.281255
2442.914557	189.205212	47.286260
2439.392261	200.027372	47.291265
2435.819108	194.858582	47.296269
2432.426243	184.536145	47.301274
2428.687514	187.387671	47.306279
2425.274797	187.975786	47.311284
2422.095499	184.410174	47.316289
2418.313322	200.558845	47.321293
2414.799603	185.523505	47.326298
2411.172862	188.724666	47.331303
2408.099741	204.963697	47.336308
2404.253542	203.000570	47.341313
2400.900029	197.683501	47.346317
2397.690032	202.964429	47.351322
2394.021956	202.728547	47.356327
2390.527374	192.898534	47.361332
2387.116710	202.125941	47.366337
2383.239884	204.871120	47.371341
2380.265163	191.988033	47.376346
2376.521179	196.647872	47.381351
2373.018209	191.925021	47.386356
2369.407373	187.827697	47.391361
2365.743690	197.556582	47.396365
2362.541223	190.053416	47.401370
2359.363888	188.555484	47.406375
2355.557269	189.789589	47.411380
2352.359345	185.684163	47.416385
2348.795163	186.810610	47.421389
2345.411995	184.302234	47.426394
2341.800131	187.387219	47.431399
2338.316483	180.753547	47.436404
2334.667514	178.773720	47.441409
2331.006493	184.658252	47.446413
2327.408578	185.757714	47.451418
2324.110743	182.815485	47.456423
2320.759069	182.486022	47.461428
2317.310793	181.198144	47.466433
2313.547216	181.950625	47.471437
2310.405509	178.371664	47.476442
2306.114014	178.367193	47.481447
2303.207800	180.313324	47.486452
2299.871014	185.511305	47.491457
2296.210970	172.194739	47.496461
2292.888129	166.840021	47.501466
2288.780012	183.580554	47.506471
2285.934206	173.501448	47.511476
2282.208172	181.360905	47.516481
2278.979220	171.198684	47.521485
2275.617315	165.332167	47.526490
2271.704973	182.841718	47.531495
2267.981292	176.016221	47.536500
2264.638177	165.430359	47.541505
2261.115173	168.800445	47.546509
2257.955759	164.448782	47.551514
2254.176955	171.049095	47.556519
2250.684547	166.246338	47.561524
2247.183497	170.006652	47.566529
2243.766771	169.077556	47.571533
2240.306014	176.551723	47.576538
2236.792746	177.983260	47.581543
2233.295189	182.624023	47.586548
2229.940793	178.814985	47.591553
2226.142616	169.615361	47.596557
2223.265195	169.254882	47.601562
2219.480372	168.860364	47.606567
2215.971487	170.790792	47.611572
2212.339787	165.033624	47.616577
2208.453470	183.266111	47.621581
2205.478085	170.913927	47.626586
2201.426244	173.177994	47.631591
2198.414824	168.615781	47.636596
2194.892808	177.259794	47.641601
2191.480116	172.221838	47.646605
2187.828624	168.286608	47.651610
2184.141023	171.310159	47.656615
2180.783329	171.888124	47.661620
2177.312027	167.816235	47.666625
2174.115162	170.328898	47.671629
2170.493266	165.376270	47.676634
2166.517994	167.996607	47.681639
2163.266320	165.305426	47.686644
2159.694194	169.487029	47.691649
2156.104654	162.064105	47.696653
2152.922144	151.514275	47.701658
2149.333636	176.084663	47.706663
2145.696103	169.094873	47.711668
2142.355529	165.896464	47.716673
2138.969573	170.533851	47.721677
2135.487788	170.405097	47.726682
2131.735765	170.432007	47.731687
2128.380679	164.647807	47.736692
2124.983391	165.294679	47.741697
2121.340915	164.555304	47.746701
2117.676837	156.877336	47.751706
2114.249213	169.980926	47.756711
2110.912803	155.419420	47.761716
2107.500590	176.291655	47.766721
2103.640996	173.655096	47.771725
2100.719682	163.070588	47.776730
2096.971801	168.107666	47.781735
2093.204319	170.545286	47.786740
2089.743136	166.974435	47.791745
2086.281829	165.061453	47.796749
2083.104885	161.839240	47.801754
2079.193708	169.043446	47.806759
2075.854378	161.939297	47.811764
2072.407209	164.242204	47.816769
2068.616712	172.086629	47.821773
2065.465906	152.908526	47.826778
2061.670921	165.957199	47.831783
2058.653755	162.678057	47.836788
2055.088224	162.369983	47.841793
2051.356767	165.028692	47.846797
2047.935798	153.086827	47.851802
2043.992208	165.766671	47.856807
2040.889867	139.222807	47.861812
2037.658158	156.842211	47.866817
2033.705716	154.492122	47.871821
2030.654919	152.452948	47.876826
2026.400105	167.155321	47.881831
2023.466539	160.576607	47.886836
2019.956356	153.827725	47.891841
2016.207053	156.527672	47.896845
2012.817297	155.284650	47.901850
2009.411350	161.261507	47.906855
2005.771243	161.569150	47.911860
2002.262433	153.178781	47.916865
1999.044765	165.088246	47.921869
1995.699108	149.900187	47.926874
1991.717540	155.592469	47.931879
1988.327802	151.510877	47.936884
1984.987012	164.708802	47.941889
1981.247385	157.752428	47.946893
1977.954989	145.006651	47.951898
1974.354192	145.980571	47.956903
1970.832661	158.755177	47.961908
1967.181539	151.625573	47.966913
1963.559176	155.826497	47.971917
1960.328754	147.810316	47.976922
1957.027848	160.260254	47.981927
1953.708121	154.260964	47.986932
1950.055592	148.015082	47.991937
1946.414634	150.049699	47.996941
1943.066335	149.972219	48.001946
1938.985710	162.441581	48.006951
1935.556686	151.021829	48.011956
1932.138702	152.218964	48.016961
1928.818239	153.346243	48.021965
1925.629700	140.615628	48.026970
1921.645702	151.478985	48.031975
1918.353437	157.783707	48.036980
1914.852079	151.510340	48.041985
1911.198802	153.630174	48.046989
1907.704301	143.821670	48.051994
1904.421496	157.807201	48.056999
1900.558651	147.476301	48.062004
1897.489346	145.386175	48.067009
1893.992610	151.048636	48.072013
1890.504813	141.939604	48.077018
1886.981749	157.009658	48.082023
1883.398557	149.237192	48.087028
1879.777173	156.754169	48.092033
1876.056841	161.355963	48.097037
1872.925971	154.197407	48.102042
1869.415118	150.801006	48.107047
1866.063889	148.467452	48.112052
1862.266126	141.160549	48.117057
1858.409830	149.457896	48.122061
1855.249379	150.137146	48.127066
1852.028965	151.079151	48.132071
1848.597826	163.531867	48.137076
1845.012560	151.364372	48.142081
1841.258209	164.712557	48.147085
1837.891666	149.657679	48.152090
1834.382230	156.262664	48.157095
1830.633289	147.738378	48.162100
1827.207085	158.081381	48.167105
1823.706217	157.172879	48.172109
1820.455480	140.340443	48.177114
1816.344760	146.124162	48.182119
1812.888713	143.242918	48.187124
1809.651317	153.511068	48.192129
1806.105160	152.987117	48.197133
1803.072374	152.669209	48.202138
1799.288638	145.687965	48.207143
1795.568570	157.079751	48.212148
1792.413842	153.095829	48.217153
1788.741698	147.232120	48.222157
1785.203487	146.080098	48.227162
1782.109149	161.234445	48.232167
1778.364885	144.541469	48.237172
1774.759114	149.470594	48.242177
1771.096388	154.355548	48.247181
1767.775815	141.914762	48.252186
1763.954238	151.463318	48.257191
1761.136331	153.189476	48.262196
1757.400435	135.349831	48.267201
1753.596891	154.209263	48.272205
1750.570260	146.874835	48.277210
1746.431539	153.967561	48.282215
1743.257870	145.948150	48.287220
1739.896229	149.274079	48.292225
1735.899712	154.381250	48.297229
1733.088729	145.640010	48.302234
1729.379001	147.867114	48.307239
1725.687080	143.025542	48.312244
1722.020294	139.647945	48.317249
1718.573764	146.746931	48.322253
1715.201573	141.332093	48.327258
1711.812770	139.859286	48.332263
1708.207359	136.372617	48.337268
1704.913005	133.450445	48.342273
1700.778014	134.315129	48.347277
1697.814847	137.421124	48.352282
1694.155411	138.655939	48.357287
1690.733620	143.439412	48.362292
1687.209067	130.641263	48.367297
1684.184973	148.439984	48.372301
1680.575483	139.025686	48.377306
1676.770775	140.391326	48.382311
1673.096533	140.820887	48.387316
1669.841320	140.473145	48.392321
1665.942762	145.855816	48.397325
1662.549827	128.891473	48.402330
1659.143042	148.615995	48.407335
1655.431093	144.625035	48.412340
1652.348159	138.407280	48.417345
1648.591721	141.147650	48.422349
1645.281355	136.642726	48.427354
1641.865915	142.710972	48.432359
1638.219598	146.879788	48.437364
1634.791877	143.046456	48.442369
1631.308202	160.391052	48.447373
1628.087266	143.365086	48.452378
1623.818093	150.129264	48.457383
1620.162754	140.941191	48.462388
1617.138589	140.938631	48.467393
1613.691038	150.556450	48.472397
1610.140811	146.075830	48.477402
1606.948611	149.944885	48.482407
1603.011152	149.682526	48.487412
1599.779260	142.476068	48.492417
1595.866685	145.360224	48.497421
1592.442882	140.685413	48.502426
1588.980410	158.595576	48.507431
1585.896702	140.014946	48.512436
1582.533148	143.889398	48.517441
1578.751408	139.434571	48.522445
1575.406453	116.056477	48.527450
1571.605019	131.861766	48.532455
1567.798488	142.165901	48.537460
1564.548362	132.281566	48.542465
1560.675649	140.823362	48.547469
1557.536172	134.326908	48.552474
1553.792098	133.100158	48.557479
1550.666400	139.918564	48.562484
1547.405340	131.802105	48.567489
1543.559325	134.543004	48.572493
1540.290954	122.346712	48.577498
1536.555704	131.050713	48.582503
1532.801643	141.606461	48.587508
1529.734033	129.297324	48.592513
1525.906620	152.502960	48.597517
1522.380548	135.382301	48.602522
1518.932132	136.065909	48.607527
1515.456898	137.054652	48.612532
1512.357707	122.575650	48.617537
1508.725621	131.947022	48.622541
1505.013850	139.275340	48.627546
1501.377834	134.091211	48.632551
1497.946353	140.999366	48.637556
1494.747822	126.729344	48.642561
1490.759505	137.536076	48.647565
1487.408014	137.352392	48.652570
1484.149229	138.402704	48.657575
1480.560023	139.045834	48.662580
1477.368429	129.127325	48.667585
1473.467446	135.648396	48.672589
1470.390830	138.866631	48.677594
1466.573293	143.496000	48.682599
1462.912460	142.639534	48.687604
1459.411298	139.982272	48.692609
1455.815347	140.677237	48.697613
1452.890192	140.894295	48.702618
1448.881715	137.793049	48.707623
1445.243163	142.136678	48.712628
1441.890218	132.447260	48.717633
1438.389726	139.208682	48.722637
1435.518046	129.939441	48.727642
1431.921929	142.791352	48.732647
1428.028459	143.381035	48.737652
1424.284812	131.112004	48.742657
1420.549229	135.345375	48.747661
1417.475407	130.580639	48.752666
1413.818523	134.520445	48.757671
1410.122649	147.041658	48.762676
1406.977474	139.007368	48.767681
1403.378970	142.054960	48.772685
1400.293863	139.580834	48.777690
1396.724329	135.889226	48.782695
1392.851665	135.208444	48.787700
1389.449903	126.536970	48.792705
1385.809549	137.633493	48.797709
1382.276054	133.111766	48.802714
1378.931300	135.074487	48.807719
1375.606948	143.003080	48.812724
1372.371240	139.757170	48.817729
1368.245862	135.288743	48.822733
1364.934756	142.406069	48.827738
1361.333591	140.022563	48.832743
1357.864461	136.373993	48.837748
1354.600657	129.775240	48.842753
1350.831884	139.792458	48.847757
1347.428551	130.235820	48.852762
1343.854719	135.642396	48.857767
1340.291894	135.724817	48.862772
1337.115139	130.215183	48.867777
1333.119076	143.446281	48.872781
1329.811494	124.384146	48.877786
1326.510898	135.297247	48.882791
1322.913021	144.058784	48.887796
1319.810397	128.831849	48.892801
1315.857827	139.541997	48.897805
1312.261078	139.054961	48.902810
1308.910828	139.958357	48.907815
1305.368829	141.027972	48.912820
1301.741418	130.645296	48.917825
1298.205333	143.845770	48.922829
1294.738037	140.910120	48.927834
1291.509538	140.073839	48.932839
1287.886963	140.458667	48.937844
1284.466824	129.957735	48.942849
1280.861647	137.275070	48.947853
1277.503036	139.070732	48.952858
1274.046838	128.929147	48.957863
1270.510639	136.563431	48.962868
1267.074475	128.543710	48.967873
1262.921670	136.227784	48.972877
1259.625353	117.677355	48.977882
1256.066977	134.312598	48.982887
1252.616904	136.559924	48.987892
1249.528418	126.841472	48.992897
1245.995830	134.406603	48.997901
1242.621997	135.077245	49.002906
1238.908086	132.050333	49.007911
1235.083247	138.483283	49.012916
1231.619919	130.785938	49.017921
1228.254443	131.731940	49.022925
1224.940783	121.192065	49.027930
1221.604593	135.093273	49.032935
1217.681206	129.807182	49.037940
1214.591073	124.801756	49.042945
1210.748104	137.200915	49.047949
1207.298515	124.822327	49.052954
1204.052007	137.182026	49.057959
1200.213376	138.545723	49.062964
1196.690482	122.496783	49.067969
1192.962905	138.766342	49.072973
1189.710766	136.633618	49.077978
1186.448127	136.541666	49.082983
1182.647766	132.650518	49.087988
1179.549168	121.835828	49.092993
1176.144801	143.435440	49.097997
1172.419072	128.203624	49.103002
1169.016084	131.237601	49.108007
1165.185465	129.809392	49.113012
1161.625797	119.373997	49.118017
1158.085847	137.571125	49.123021
1154.552320	127.854765	49.128026
1151.235238	122.374019	49.133031
1147.670817	126.631161	49.138036
1144.317703	118.674267	49.143041
1140.637595	128.070884	49.148045
1137.102093	134.235323	49.153050
1133.710811	122.659990	49.158055
1130.179960	124.717082	49.163060
1127.015203	129.421567	49.168065
1123.279348	128.720129	49.173069
1119.817173	132.420952	49.178074
1116.156913	129.206192	49.183079
1112.244408	130.749552	49.188084
1109.226159	121.341601	49.193089
1105.686783	128.565671	49.198093
1102.143906	122.920573	49.203098
1098.923823	128.025770	49.208103
1095.219794	115.138073	49.213108
1091.774760	122.256103	49.218113
1088.342661	126.076775	49.223117
1084.458580	126.873363	49.228122
1081.241349	121.578022	49.233127
1078.025736	129.156401	49.238132
1074.361648	127.461707	49.243137
1070.714676	119.031968	49.248141
1067.405468	134.507276	49.253146
1063.518753	123.966998	49.258151
1059.999562	134.563587	49.263156
1056.728723	129.568439	49.268161
1052.744630	138.188348	49.273165
1049.851976	131.000870	49.278170
1046.307460	133.892823	49.283175
1042.658076	133.536855	49.288180
1039.450223	118.573131	49.293185
1035.433926	135.065329	49.298189
1031.920281	129.620550	49.303194
1028.408130	123.143187	49.308199
1024.974848	122.633558	49.313204
1022.130110	115.365186	49.318209
1017.882394	133.964915	49.323213
1014.334957	117.904768	49.328218
1011.098977	123.591738	49.333223
1007.702496	126.027054	49.338228
1004.328558	118.289638	49.343233
1000.362133	119.109932	49.348237
996.845777	119.010138	49.353242
993.684370	119.427010	49.358247
989.985087	124.230654	49.363252
986.735302	107.286859	49.368257
983.251830	123.491513	49.373261
979.914789	114.260382	49.378266
976.184725	115.343849	49.383271
972.398937	125.979453	49.388276
969.130724	113.260214	49.393281
965.489388	118.235237	49.398285
962.011568	111.780367	49.403290
958.879351	115.883168	49.408295
954.917975	122.327053	49.413300
951.998697	121.581749	49.418305
947.704364	122.236901	49.423309
944.336083	128.050321	49.428314
941.266211	129.826090	49.433319
937.494432	122.474342	49.438324
934.053048	126.715217	49.443329
930.391758	121.865210	49.448333
926.826693	119.534688	49.453338
923.446879	124.374407	49.458343
919.662303	121.940731	49.463348
917.091876	116.767467	49.468353
913.306750	127.073871	49.473357
909.599008	114.293562	49.478362
905.810338	109.872648	49.483367
902.395188	120.656035	49.488372
899.089907	105.878978	49.493377
895.594269	122.519758	49.498381
891.933044	112.078224	49.503386
888.496020	111.728910	49.508391
884.930595	115.740489	49.513396
881.639669	122.648283	49.518401
878.194701	118.467685	49.523405
874.542970	107.816828	49.528410
870.858520	112.582958	49.533415
867.435701	121.778175	49.538420
864.095430	113.466925	49.543425
860.350390	115.402852	49.548429
856.740857	109.934158	49.553434
853.686604	117.629225	49.558439
849.955793	108.758473	49.563444
846.683323	109.689795	49.568449
842.896704	115.948114	49.573453
839.660086	116.406185	49.578458
835.853912	116.817721	49.583463
832.411564	119.503783	49.588468
828.935722	109.952241	49.593473
825.498503	109.400845	49.598477
822.178963	119.909009	49.603482
818.406922	118.824322	49.608487
814.833048	119.100137	49.613492
811.199855	111.860946	49.618497
807.744576	122.076917	49.623501
804.542170	116.369954	49.628506
801.069740	110.668811	49.633511
797.386229	112.550216	49.638516
794.230894	111.859551	49.643521
790.302493	110.722862	49.648525
786.630296	109.737824	49.653530
783.512324	117.728950	49.658535
779.960898	109.903973	49.663540
776.293390	121.519516	49.668545
773.076051	114.995696	49.673549
769.410320	109.414889	49.678554
765.999796	115.676944	49.683559
762.228084	109.560182	49.688564
758.887621	100.158391	49.693569
755.433877	113.962936	49.698573
752.040535	120.220286	49.703578
748.453296	102.986000	49.708583
744.835094	114.694137	49.713588
740.988883	110.611450	49.718593
737.572739	110.559569	49.723597
734.195459	110.619658	49.728602
731.126008	110.548311	49.733607
727.404263	123.825125	49.738612
724.054799	109.247757	49.743617
720.476148	112.055827	49.748621
716.661076	107.227206	49.753626
713.449975	108.150331	49.758631
709.693928	111.094349	49.763636
706.520902	107.810812	49.768641
702.657630	108.480170	49.773645
699.487858	105.744330	49.778650
695.982687	109.196734	49.783655
692.239181	127.638152	49.788660
688.699942	115.416481	49.793665
685.188948	118.266769	49.798669
681.677922	121.274125	49.803674
678.246488	124.904966	49.808679
674.532422	127.003594	49.813684
671.516946	121.641709	49.818689
667.977273	132.964890	49.823693
664.063770	126.436921	49.828698
660.848433	123.436529	49.833703
657.154232	125.442602	49.838708
653.822424	123.474449	49.843713
649.925822	126.701674	49.848717
646.757092	126.267134	49.853722
643.409531	120.323382	49.858727
639.648348	120.902122	49.863732
636.490262	113.747059	49.868737
633.045669	126.054228	49.873741
629.534321	116.618475	49.878746
626.236898	123.663397	49.883751
621.886047	122.960718	49.888756
618.700112	113.878778	49.893761
615.215793	119.912073	49.898765
611.494380	120.186516	49.903770
608.006626	120.133209	49.908775
604.753275	111.405440	49.913780
601.462339	115.264684	49.918785
597.803116	115.632946	49.923789
593.942033	125.025660	49.928794
590.629290	122.265835	49.933799
587.081944	114.653497	49.938804
583.881956	113.620968	49.943809
580.508269	112.360527	49.948813
576.707116	108.929523	49.953818
573.062047	108.004351	49.958823
569.443738	121.970325	49.963828
566.114026	116.387021	49.968833
562.734654	118.835806	49.973837
559.089495	123.456600	49.978842
555.902204	109.579750	49.983847
551.970397	120.619780	49.988852
548.714238	119.050288	49.993857
545.014736	104.155277	49.998861
541.739264	117.983043	50.003866
538.761642	115.737238	50.008871
534.488453	111.685940	50.013876
531.205965	120.146711	50.018881
527.550988	104.862065	50.023885
524.279357	109.862661	50.028890
520.647175	108.218558	50.033895
516.766236	120.456466	50.038900
513.422427	112.703712	50.043905
510.373795	107.882600	50.048909
506.960898	103.671861	50.053914
503.294383	107.301855	50.058919
499.498843	105.815663	50.063924
496.010705	111.420686	50.068929
492.731744	120.137099	50.073933
488.905030	106.155481	50.078938
485.858891	98.225231	50.083943
482.325259	105.111024	50.088948
478.675230	103.104274	50.093953
475.037147	115.395511	50.098957
471.444080	104.020277	50.103962
468.176264	109.671100	50.108967
464.524445	119.787675	50.113972
461.121867	105.494706	50.118977
457.640144	104.494771	50.123981
453.825724	118.783723	50.128986
450.383717	103.527490	50.133991
446.846979	120.074189	50.138996
443.614996	110.494744	50.144001
440.201652	107.082734	50.149005
436.845766	103.944872	50.154010
433.568412	107.805895	50.159015
429.325077	103.436707	50.164020
426.083508	101.220945	50.169025
422.469692	103.692542	50.174029
418.893018	103.675928	50.179034
415.606715	105.649871	50.184039
411.895559	110.587076	50.189044
408.501045	105.811118	50.194049
405.141092	112.664018	50.199053
401.342486	117.879581	50.204058
398.399924	110.014344	50.209063
394.210144	111.766107	50.214068
391.105945	99.841657	50.219073
387.516643	107.827232	50.224077
383.695914	121.290820	50.229082
380.681115	107.077785	50.234087
377.324878	117.443411	50.239092
373.652020	110.022124	50.244097
370.064447	109.241868	50.249101
366.168197	113.809330	50.254106
363.040784	113.249125	50.259111
359.481626	116.385250	50.264116
356.144297	123.010392	50.269121
352.546830	108.086132	50.274125
349.088945	113.954867	50.279130
345.567149	107.551928	50.284135
342.146320	120.402228	50.289140
338.675338	98.538863	50.294145
335.018153	99.942226	50.299149
331.281957	107.824138	50.304154
328.034251	107.223841	50.309159
324.056066	101.066200	50.314164
321.023735	108.971434	50.319169
317.599335	111.701349	50.324173
314.068699	103.407875	50.329178
310.663955	109.136734	50.334183
306.744130	102.654555	50.339188
303.083894	105.262630	50.344193
299.717951	111.599611	50.349197
295.971855	112.680974	50.354202
293.087898	100.857033	50.359207
289.318590	107.961604	50.364212
286.263281	109.172231	50.369217
282.883162	105.894420	50.374221
278.845617	107.981296	50.379226
275.258754	105.674281	50.384231
271.760890	112.597380	50.389236
268.455724	100.892369	50.394241
264.774385	103.221698	50.399245
261.357958	102.948039	50.404250
257.968258	98.031285	50.409255
254.125181	109.583613	50.414260
250.657429	109.208043	50.419265
247.742637	104.114076	50.424269
243.779224	113.242399	50.429274
240.310453	100.694295	50.434279
236.988206	101.448766	50.439284
233.649354	105.762216	50.444289
229.952098	100.815195	50.449293
226.246748	107.297469	50.454298
222.829135	103.626726	50.459303
219.273330	116.068642	50.464308
215.610930	118.141129	50.469313
212.407814	102.827342	50.474317
208.730064	108.601652	50.479322
205.292455	101.947725	50.484327
201.836588	104.559282	50.489332
198.649774	110.891475	50.494337
194.760725	102.585672	50.499341
191.331630	99.738350	50.504346
188.308294	102.426728	50.509351
184.463760	114.453668	50.514356
181.047849	108.858984	50.519361
177.701238	100.457058	50.524365
173.408429	117.024795	50.529370
170.082751	104.253414	50.534375
166.376424	113.902031	50.539380
163.391259	110.158093	50.544385
159.902287	102.993062	50.549389
156.243430	117.613869	50.554394
152.981557	108.207155	50.559399
149.111892	117.435269	50.564404
145.631619	111.896029	50.569409
141.999731	102.712160	50.574413
139.074731	121.696398	50.579418
135.644310	98.029973	50.584423
131.934934	106.119069	50.589428
128.143234	94.591425	50.594433
124.982413	93.324371	50.599437
121.320066	105.461322	50.604442
117.895079	101.861608	50.609447
114.349705	115.584364	50.614452
110.641515	109.835576	50.619457
107.018836	103.799683	50.624461
103.447591	106.686958	50.629466
100.028405	98.044615	50.634471
96.797080	107.793240	50.639476
93.283931	106.210713	50.644481
90.006914	94.833343	50.649485
86.267651	107.015380	50.654490
82.847371	102.796931	50.659495
79.388067	103.928402	50.664500
75.763412	105.424500	50.669505
72.316091	101.694924	50.674509
68.473531	107.119084	50.679514
65.098934	100.548554	50.684519
61.715748	110.285688	50.689524
58.096546	92.624505	50.694529
54.480836	104.540091	50.699533
50.809020	103.718000	50.704538
47.587050	96.273333	50.709543
44.088584	94.738033	50.714548
41.055141	99.883873	50.719553
37.504868	96.725774	50.724557
33.830041	97.846811	50.729562
30.631096	97.771152	50.734567
26.676827	100.836202	50.739572
22.829935	94.976127	50.744577
19.686023	94.386758	50.749581
15.950901	97.264361	50.754586
12.460061	96.974919	50.759591
8.770543	94.743234	50.764596
5.673928	95.874100	50.769601
2.372408	85.999810	50.774605