Thu Jun 16 18:55:26 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
0.280958	110.841395	0.000000
-0.176590	98.651877	0.005005
0.049355	88.760548	0.010010
-0.279909	100.806361	0.015014
-0.149172	97.506323	0.020019
-0.618164	72.704188	0.025024
-0.912594	76.905698	0.030029
-0.978898	54.762391	0.035034
-1.395734	48.770490	0.040038
-1.674154	51.659113	0.045043
-1.617329	29.693988	0.050048
-2.171939	32.014124	0.055053
-2.162152	17.266870	0.060058
-2.933247	26.706970	0.065062
-3.173853	12.138821	0.070067
-3.234177	10.253512	0.075072
-3.873959	8.112455	0.080077
-4.268336	-2.581163	0.085082
-4.561615	4.665206	0.090086
-5.128879	8.646700	0.095091
-4.988724	13.696527	0.100096
-5.431270	11.940085	0.105101
-4.877020	7.762689	0.110106
-5.081746	11.170579	0.115110
-6.069342	9.295654	0.120115
-6.219317	7.501322	0.125120
-6.586348	12.102327	0.130125
-6.474191	5.398641	0.135130
-6.798554	13.225898	0.140134
-6.738895	2.577702	0.145139
-7.393209	6.225233	0.150144
-7.868660	25.655857	0.155149
-7.890584	-3.818816	0.160154
-8.482918	4.707194	0.165158
-8.843287	22.483796	0.170163
-8.387931	2.432159	0.175168
-8.781962	19.270789	0.180173
-8.890444	10.056301	0.185178
-9.429153	12.856425	0.190182
-9.674891	11.177657	0.195187
-9.972182	14.638925	0.200192
-9.956885	25.320170	0.205197
-10.252501	2.346576	0.210202
-10.865924	10.017485	0.215206
-11.439724	13.737936	0.220211
-11.176485	2.125095	0.225216
-11.598639	22.709748	0.230221
-11.289382	8.924421	0.235226
-11.623856	18.701384	0.240230
-11.900288	18.603991	0.245235
-12.525529	14.556202	0.250240
-13.010459	21.606457	0.255245
-12.816883	12.299630	0.260250
-13.020171	12.267790	0.265254
-13.049969	7.471075	0.270259
-12.973797	3.027986	0.275264
-14.033234	17.351676	0.280269
-14.374531	13.577592	0.285274
-14.667309	12.763413	0.290278
-14.644254	14.556076	0.295283
-14.901641	7.915135	0.300288
-15.087211	16.092470	0.305293
-15.562631	5.557954	0.310298
-15.749593	7.241880	0.315302
-15.949509	4.017517	0.320307
-16.067656	9.136763	0.325312
-16.105745	14.354260	0.330317
-16.340764	0.272654	0.335322
-16.963620	9.205234	0.340326
-17.913988	15.396665	0.345331
-17.733147	-1.068987	0.350336
-18.003264	19.232357	0.355341
-17.572336	6.522780	0.360346
-17.574181	0.796956	0.365350
-17.950115	11.914673	0.370355
-18.513139	13.045734	0.375360
-18.952713	12.258380	0.380365
-19.120689	-0.799221	0.385370
-19.413704	5.131350	0.390374
-19.697892	-0.718092	0.395379
-19.910191	1.764287	0.400384
-20.741638	7.182737	0.405389
-20.766691	6.669705	0.410394
-21.082853	15.813928	0.415398
-21.147340	12.917308	0.420403
-20.884662	7.866071	0.425408
-21.315372	13.731696	0.430413
-20.937358	11.083465	0.435418
-21.890697	16.074466	0.440422
-22.306207	10.384247	0.445427
-22.240589	18.101974	0.450432
-22.008466	7.089061	0.455437
-22.835527	14.163395	0.460442
-23.698945	5.594961	0.465446
-23.934524	11.177855	0.470451
-23.730410	5.959113	0.475456
-24.001090	13.107437	0.480461
-24.054362	4.372565	0.485466
-23.608793	8.646806	0.490470
-24.464260	1.420735	0.495475
-24.867554	1.445429	0.500480
-25.450472	10.131975	0.505485
-25.412281	0.142002	0.510490
-25.404844	11.895823	0.515494
-26.454606	14.865642	0.520499
-26.748668	2.965278	0.525504
-27.051524	3.754520	0.530509
-26.599636	3.858183	0.535514
-26.774827	4.293861	0.540518
-27.231591	9.830141	0.545523
-27.115283	-9.236023	0.550528
-27.614281	16.961436	0.555533
-27.524769	11.731344	0.560538
-28.530231	8.136671	0.565542
-29.078561	6.813247	0.570547
-29.078963	11.964532	0.575552
-29.122564	0.048430	0.580557
-29.013774	8.938629	0.585562
-28.797004	13.846259	0.590566
-29.311071	6.489579	0.595571
-29.944982	7.077128	0.600576
-30.511965	9.489675	0.605581
-30.249865	6.247068	0.610586
-30.348918	3.160038	0.615590
-30.742666	13.274917	0.620595
-31.600288	11.599898	0.625600
-32.176959	14.363086	0.630605
-32.316044	-1.029013	0.635610
-32.059391	17.041314	0.640614
-32.281202	0.824715	0.645619
-32.103291	8.209565	0.650624
-32.386693	12.353595	0.655629
-32.081551	-2.582733	0.660634
-33.229814	11.423264	0.665638
-33.588298	8.899312	0.670643
-33.654661	-1.024251	0.675648
-34.068143	10.328942	0.680653
-33.849897	12.352558	0.685658
-34.809455	4.578103	0.690662
-35.225906	-4.416976	0.695667
-35.291494	6.151638	0.700672
-35.603643	2.883376	0.705677
-35.463874	-1.399646	0.710682
-35.100468	-2.671402	0.715686
-35.619331	0.773601	0.720691
-35.512113	-6.439405	0.725696
-36.453802	-1.450925	0.730701
-36.706328	-10.943672	0.735706
-36.828867	7.221863	0.740710
-37.132749	-0.283296	0.745715
-37.877913	6.112077	0.750720
-38.538758	11.556694	0.755725
-38.059363	5.936712	0.760730
-38.327283	7.026996	0.765734
-39.021504	15.255734	0.770739
-38.692925	9.393320	0.775744
-38.544757	6.717666	0.780749
-38.884447	6.320559	0.785754
-38.906398	7.164006	0.790758
-39.807272	12.147817	0.795763
-40.198084	12.114018	0.800768
-40.599101	-0.812232	0.805773
-40.389122	0.344391	0.810778
-40.528485	1.632837	0.815782
-40.817766	6.422247	0.820787
-41.220039	1.774696	0.825792
-41.708178	15.722313	0.830797
-41.525513	3.784009	0.835802
-41.730259	12.386258	0.840806
-41.867655	5.918262	0.845811
-42.294933	2.523019	0.850816
-43.068717	12.812477	0.855821
-42.567024	2.378911	0.860826
-42.832387	15.536288	0.865830
-43.446769	15.602576	0.870835
-44.388937	12.464673	0.875840
-44.616362	16.249722	0.880845
-44.039420	6.802693	0.885850
-44.700417	17.931218	0.890854
-44.865138	16.230480	0.895859
-44.690378	12.440172	0.900864
-44.848700	13.469824	0.905869
-45.132692	14.080542	0.910874
-45.721121	10.197545	0.915878
-46.363383	14.613086	0.920883
-45.995675	0.096157	0.925888
-46.750700	8.751065	0.930893
-46.626484	4.444270	0.935898
-46.533576	8.071509	0.940902
-47.404374	5.775668	0.945907
-47.577932	6.957102	0.950912
-47.932172	12.385480	0.955917
-48.071342	4.471011	0.960922
-48.060585	16.925422	0.965926
-48.404273	1.908283	0.970931
-48.830126	0.839768	0.975936
-49.284251	15.530550	0.980941
-49.800811	1.535728	0.985946
-49.625493	4.220121	0.990950
-49.805591	17.861514	0.995955
-49.664523	7.131893	1.000960
-49.926135	7.613719	1.005965
-50.198665	5.843293	1.010970
-50.834628	-1.171917	1.015974
-51.532356	12.130703	1.020979
-51.090881	7.839351	1.025984
-51.212029	10.533968	1.030989
-51.514248	12.335399	1.035994
-52.101049	11.756566	1.040998
-52.778697	0.693841	1.046003
-52.695251	-2.373526	1.051008
-52.922737	15.537172	1.056013
-52.940867	7.729371	1.061018
-52.501231	3.988914	1.066022
-53.100419	4.024674	1.071027
-53.697861	-0.492361	1.076032
-53.984329	10.581267	1.081037
-54.298055	17.721612	1.086042
-54.165706	11.914416	1.091046
-54.650920	17.346091	1.096051
-55.561617	6.441940	1.101056
-55.879859	8.960672	1.106061
-55.925842	10.542179	1.111066
-55.922235	10.256051	1.116070
-55.888995	8.075990	1.121075
-55.850480	5.867631	1.126080
-55.974384	8.919043	1.131085
-56.711275	9.279542	1.136090
-57.310245	12.193610	1.141094
-57.717023	5.193697	1.146099
-57.457757	12.870536	1.151104
-57.979346	16.409913	1.156109
-57.925854	15.399901	1.161114
-57.683031	4.348722	1.166118
-58.325635	14.130235	1.171123
-58.795105	0.504198	1.176128
-59.127661	14.206595	1.181133
-59.740720	-2.293587	1.186138
-59.357851	1.268860	1.191142
-59.439647	0.411332	1.196147
-59.940163	9.620151	1.201152
-60.902924	11.705858	1.206157
-60.815544	9.998481	1.211162
-61.231489	-2.529397	1.216166
-61.503893	16.561134	1.221171
-61.113528	-2.707777	1.226176
-61.206165	12.861662	1.231181
-61.088490	-0.343768	1.236186
-61.727567	6.023025	1.241190
-62.408488	4.122191	1.246195
-62.341645	0.720168	1.251200
-62.644751	-6.614638	1.256205
-62.580266	2.792228	1.261210
-63.367901	-5.924068	1.266214
-64.162486	12.776747	1.271219
-64.140481	8.823059	1.276224
-64.165075	2.529294	1.281229
-64.388370	9.653013	1.286234
-64.072530	4.861134	1.291238
-64.404210	1.962308	1.296243
-64.917875	1.491255	1.301248
-65.747358	4.911631	1.306253
-66.110425	-8.080270	1.311258
-65.588894	9.616464	1.316262
-66.406633	7.671156	1.321267
-65.862865	-1.955066	1.326272
-66.205828	5.558579	1.331277
-66.557076	2.372055	1.336282
-66.979832	9.424460	1.341286
-67.475278	14.487970	1.346291
-67.230158	6.625516	1.351296
-67.348050	9.499245	1.356301
-68.221264	6.571825	1.361306
-68.872422	4.847992	1.366310
-69.386726	11.419197	1.371315
-69.100912	1.140188	1.376320
-69.565979	4.780715	1.381325
-69.403703	11.585790	1.386330
-69.314420	11.447494	1.391334
-69.112644	9.368817	1.396339
-69.396173	1.376101	1.401344
-70.415588	10.390104	1.406349
-70.582526	19.094724	1.411354
-70.746439	1.558827	1.416358
-71.115011	3.294174	1.421363
-71.058441	16.088471	1.426368
-71.565546	12.717174	1.431373
-71.891306	5.013194	1.436378
-72.087608	14.254905	1.441382
-72.272598	3.172718	1.446387
-72.358559	4.495056	1.451392
-72.338321	13.092776	1.456397
-72.956620	19.259127	1.461402
-73.357428	4.229135	1.466406
-73.739349	14.413681	1.471411
-73.941250	8.571163	1.476416
-73.962903	12.475612	1.481421
-74.440943	12.539397	1.486426
-74.910118	6.819481	1.491430
-75.333200	18.218362	1.496435
-75.248427	10.257116	1.501440
-75.555853	15.555822	1.506445
-75.661459	10.652758	1.511450
-75.861622	8.552312	1.516454
-75.738235	5.788215	1.521459
-75.586443	9.674456	1.526464
-76.149313	13.416781	1.531469
-77.036679	13.846742	1.536474
-77.267686	10.703781	1.541478
-77.379294	0.883394	1.546483
-77.197890	-0.284787	1.551488
-77.582292	13.672417	1.556493
-78.497802	2.609052	1.561498
-78.589956	1.215767	1.566502
-79.122543	10.370989	1.571507
-79.162668	6.590547	1.576512
-79.164509	9.142818	1.581517
-78.999017	10.104157	1.586522
-78.864534	1.353751	1.591526
-79.435069	8.446758	1.596531
-79.949184	-11.974896	1.601536
-80.367332	6.301341	1.606541
-80.459935	-1.098936	1.611546
-80.745023	2.856248	1.616550
-81.384768	2.388276	1.621555
-81.922766	10.836844	1.626560
-81.955554	12.503381	1.631565
-82.318612	11.335503	1.636570
-82.119958	3.134256	1.641574
-82.457004	0.140131	1.646579
-82.140535	11.542174	1.651584
-82.418394	-0.864684	1.656589
-82.444930	-1.983405	1.661594
-82.845737	8.182948	1.666598
-83.582492	14.887008	1.671603
-83.623605	-0.771659	1.676608
-84.434932	9.361519	1.681613
-84.957032	-10.085097	1.686618
-84.721602	-4.577685	1.691622
-85.467114	3.941479	1.696627
-85.375851	-9.401242	1.701632
-85.808534	1.933510	1.706637
-85.600927	5.003827	1.711642
-85.466029	-0.241750	1.716646
-85.766386	9.661071	1.721651
-85.626382	1.456004	1.726656
-86.475526	12.210642	1.731661
-86.834196	4.410390	1.736666
-86.688016	-2.962658	1.741670
-87.234376	10.220235	1.746675
-87.559692	6.667364	1.751680
-88.447058	9.738307	1.756685
-88.819087	8.489733	1.761690
-88.643966	1.217263	1.766694
-88.772299	3.690698	1.771699
-88.578434	13.563834	1.776704
-89.012141	3.212547	1.781709
-89.041804	1.738002	1.786714
-89.035156	0.982862	1.791718
-89.895258	14.988989	1.796723
-90.063224	9.357509	1.801728
-90.394652	2.652358	1.806733
-90.441535	17.077342	1.811738
-90.528037	-0.513172	1.816742
-91.778111	1.791285	1.821747
-91.746200	1.614524	1.826752
-91.988236	-1.667391	1.831757
-92.155454	1.125501	1.836762
-92.232985	5.933090	1.841766
-92.376338	-0.999168	1.846771
-91.977719	6.292374	1.851776
-91.971892	11.241470	1.856781
-93.064165	9.829582	1.861786
-92.945064	2.710700	1.866790
-93.463233	18.435112	1.871795
-93.443457	0.019251	1.876800
-94.462322	7.148074	1.881805
-94.896306	2.335886	1.886810
-95.098212	2.593372	1.891814
-95.084629	-1.982219	1.896819
-94.805435	-7.390251	1.901824
-95.202602	4.310954	1.906829
-95.340098	12.076742	1.911834
-95.433709	-6.839688	1.916838
-96.367789	2.740197	1.921843
-96.312402	-14.854413	1.926848
-96.466614	8.685015	1.931853
-96.701311	1.939512	1.936858
-97.222488	-2.602552	1.941862
-97.927065	8.948405	1.946867
-97.840722	-0.453054	1.951872
-97.905607	-6.839893	1.956877
-98.086285	0.431171	1.961882
-98.083515	-4.321888	1.966886
-98.318137	-0.349789	1.971891
-98.714123	9.575939	1.976896
-99.180613	-3.929923	1.981901
-99.859953	-12.451505	1.986906
-99.782163	-18.449742	1.991910
-99.969756	-4.838705	1.996915
-99.994848	-8.632515	2.006912
-99.851998	-3.284533	2.016909
-99.456498	-6.373823	2.026906
-98.693878	2.227014	2.036902
-98.526884	1.925445	2.046899
-97.917784	-2.402444	2.056896
-97.193418	6.132558	2.066893
-97.121407	0.189120	2.076890
-96.438284	4.571729	2.086886
-95.589039	1.208306	2.096883
-95.682918	2.026313	2.106880
-94.535802	5.594742	2.116877
-94.175250	-0.328817	2.126874
-94.214826	4.312413	2.136870
-93.323570	-11.665031	2.146867
-92.810264	-3.163112	2.156864
-92.711502	-2.118631	2.166861
-91.748714	-6.879499	2.176858
-91.597324	-2.660459	2.186854
-90.722126	-3.534303	2.196851
-90.175536	2.065326	2.206848
-90.066488	1.240016	2.216845
-89.383281	-9.131370	2.226842
-88.419308	2.838494	2.236838
-88.217284	0.184056	2.246835
-88.107217	7.382734	2.256832
-87.374876	3.898857	2.266829
-87.090250	11.626700	2.276826
-86.123973	4.179996	2.286822
-85.200801	2.417841	2.296819
-85.468646	2.437163	2.306816
-85.310436	7.811751	2.316813
-84.340128	8.625910	2.326810
-83.949651	-0.190301	2.336806
-83.176255	2.716373	2.346803
-82.206389	1.028144	2.356800
-82.208599	6.136656	2.366797
-82.326942	3.190024	2.376794
-81.583062	-4.343149	2.386790
-80.842837	8.335804	2.396787
-80.310800	-1.915626	2.406784
-79.377135	1.202919	2.416781
-79.354170	1.334303	2.426778
-79.041439	5.407453	2.436774
-78.116919	8.359140	2.446771
-78.104069	7.871112	2.456768
-77.249068	7.410300	2.466765
-76.185463	4.075018	2.476762
-76.245149	-0.367958	2.486758
-75.797154	6.709232	2.496755
-75.550298	-5.166336	2.506752
-74.778022	5.556401	2.516749
-74.472268	6.499750	2.526746
-74.177398	6.075600	2.536742
-73.106747	-1.846840	2.546739
-72.952232	3.084290	2.556736
-71.789242	2.615351	2.566733
-71.451599	9.151435	2.576730
-71.584934	11.684871	2.586726
-71.414013	3.562229	2.596723
-70.147824	-3.033944	2.606720
-69.844597	-2.074866	2.616717
-69.028756	-8.840698	2.626714
-68.528352	0.189119	2.636710
-68.215339	-0.598430	2.646707
-68.283778	-1.352031	2.656704
-67.216790	-2.389687	2.666701
-66.686417	-5.269278	2.676698
-66.370637	-2.271021	2.686694
-65.400470	-0.756185	2.696691
-65.392307	0.753710	2.706688
-65.074955	-2.772116	2.716685
-64.239383	2.385475	2.726682
-63.847273	-2.773599	2.736678
-63.013632	-11.585452	2.746675
-62.331115	-5.752098	2.756672
-62.117596	1.973567	2.766669
-62.139320	4.433190	2.776666
-61.306019	5.081274	2.786662
-60.541134	6.053207	2.796659
-60.578482	0.608853	2.806656
-59.789243	-3.099123	2.816653
-58.993274	-7.748553	2.826650
-59.074412	-2.661868	2.836646
-58.096880	-5.862804	2.846643
-57.533396	-8.470985	2.856640
-57.104443	2.018027	2.866637
-57.097338	-4.436049	2.876634
-56.443647	2.050815	2.886630
-56.003891	-4.142761	2.896627
-54.851962	-0.430357	2.906624
-54.377800	1.855843	2.916621
-54.408306	-5.664035	2.926618
-54.132109	-2.941057	2.936614
-53.094261	-4.025409	2.946611
-52.925673	-5.715308	2.956608
-51.964507	-6.392259	2.966605
-51.448283	2.670460	2.976602
-51.424539	-4.752541	2.986598
-51.058850	-2.688748	2.996595
-50.143728	-4.398103	3.006592
-49.573864	-0.045125	3.016589
-49.316239	0.527652	3.026586
-48.438942	-8.609540	3.036582
-48.110468	-2.463609	3.046579
-47.992425	-7.945000	3.056576
-47.261714	-2.947241	3.066573
-46.751651	-0.796623	3.076570
-46.456975	0.104551	3.086566
-44.972754	2.529753	3.096563
-45.011516	4.963743	3.106560
-44.559634	2.773080	3.116557
-44.645420	1.812733	3.126554
-43.924645	3.065531	3.136550
-43.510752	-5.678536	3.146547
-42.559649	-3.146760	3.156544
-42.229175	-2.883006	3.166541
-42.180718	6.161697	3.176538
-40.937001	3.647601	3.186534
-40.380272	2.112703	3.196531
-40.271865	5.815461	3.206528
-39.940605	-2.121891	3.216525
-39.070778	-4.651640	3.226522
-38.898533	-0.376132	3.236518
-37.938407	-7.009042	3.246515
-37.471762	-3.149059	3.256512
-37.586082	-3.627085	3.266509
-36.642327	-4.585300	3.276506
-35.792355	-2.524835	3.286502
-35.513441	-0.041798	3.296499
-35.461068	-2.988145	3.306496
-34.722085	-5.655307	3.316493
-33.942530	-0.884071	3.326490
-33.759649	-2.508272	3.336486
-33.411694	9.257245	3.346483
-32.209616	-3.757279	3.356480
-32.164446	-4.082820	3.366477
-32.113501	-3.906719	3.376474
-31.009303	1.876219	3.386470
-30.785133	-5.837377	3.396467
-30.248093	-8.433431	3.406464
-29.269293	-7.874880	3.416461
-29.329800	-7.589630	3.426458
-28.892065	-2.319367	3.436454
-27.941795	-3.821260	3.446451
-27.473952	-2.689551	3.456448
-27.487806	-6.416582	3.466445
-26.706664	-2.085378	3.476442
-26.346937	-1.751484	3.486438
-25.685656	-7.855524	3.496435
-24.545175	-5.939328	3.506432
-24.367546	-7.246364	3.516429
-24.303005	-2.781821	3.526426
-24.192064	-10.877259	3.536422
-23.346523	-12.853623	3.546419
-22.597515	-6.062409	3.556416
-21.680225	-5.714417	3.566413
-21.338045	-6.215135	3.576410
-20.877697	-7.416918	3.586406
-20.843237	-3.314176	3.596403
-20.574080	5.374599	3.606400
-19.467413	-0.761954	3.616397
-19.247551	-1.285279	3.626394
-18.847027	-4.676876	3.636390
-17.913230	-2.826439	3.646387
-18.006876	-12.318166	3.656384
-17.151735	-11.244138	3.666381
-16.529817	-6.785371	3.676378
-16.328150	-10.681964	3.686374
-15.502699	-6.724362	3.696371
-14.733980	-7.730351	3.706368
-14.541716	-9.180814	3.716365
-14.572607	-6.559850	3.726362
-13.353191	-6.396077	3.736358
-13.040420	-2.192440	3.746355
-12.848974	-6.868059	3.756352
-12.325895	-11.833036	3.766349
-11.879964	-2.002185	3.776346
-10.636993	-6.868861	3.786342
-10.483330	-8.852190	3.796339
-9.860359	-12.011911	3.806336
-9.786771	-14.227526	3.816333
-9.577372	-2.387602	3.826330
-8.679449	-4.491999	3.836326
-8.115410	-3.858679	3.846323
-6.962548	-7.753426	3.856320
-7.254398	-8.565777	3.866317
-6.676658	-8.902427	3.876314
-6.239823	-3.132675	3.886310
-5.307211	-8.952514	3.896307
-5.254962	-4.358364	3.906304
-4.968977	-7.086783	3.916301
-3.865993	-5.252351	3.926298
-3.632130	-11.324527	3.936294
-3.559080	-5.062493	3.946291
-2.958695	2.108652	3.956288
-2.430607	22.782600	3.966285
-2.013793	36.889233	3.976282
-1.304237	48.402603	3.986278
-1.226022	58.326514	3.996275
-0.642103	83.757708	4.006272
-0.367143	110.509344	4.016269
0.000000	139.704002	4.021274
0.077001	138.474140	4.026278
0.179083	160.427414	4.031283
0.626405	169.156499	4.036288
0.863092	176.450824	4.041293
0.253319	177.253402	4.046298
0.602845	172.912976	4.051302
0.846299	198.316013	4.056307
1.226387	198.339303	4.061312
1.308424	205.731809	4.066317
1.356725	209.430201	4.071322
1.630682	199.772179	4.076326
1.514899	198.740603	4.081331
1.079988	187.619267	4.086336
1.355375	173.881514	4.091341
1.031362	172.550205	4.096346
1.140408	175.985992	4.101350
1.241304	205.473364	4.106355
1.306180	201.901834	4.111360
1.330107	208.113366	4.116365
0.979542	209.091139	4.121370
1.403099	213.359706	4.126374
1.407159	210.157430	4.131379
1.499890	205.810202	4.136384
1.405142	208.597273	4.141389
1.280317	207.881705	4.146394
1.323313	200.815062	4.151398
1.435681	203.361122	4.156403
1.266250	210.639212	4.161408
1.348259	210.746092	4.166413
1.321459	212.238127	4.171418
1.853955	213.332790	4.176422
1.375925	214.324524	4.181427
1.337427	214.101091	4.186432
1.562767	209.272508	4.191437
1.305000	210.496680	4.196442
1.435816	211.540026	4.201446
1.499172	212.503954	4.206451
1.171818	218.783998	4.211456
1.640454	218.166486	4.216461
1.674167	211.782098	4.221466
1.466073	224.740182	4.226470
1.341415	216.123434	4.231475
1.121318	217.315928	4.236480
1.458074	220.215587	4.241485
1.825143	244.746972	4.246490
1.835884	238.115585	4.251494
1.509385	226.846375	4.256499
1.709588	234.929000	4.261504
1.903454	234.450420	4.266509
1.741556	223.940694	4.271514
1.876813	210.926621	4.276518
1.720029	215.930974	4.281523
1.530464	219.937021	4.286528
1.711410	210.989788	4.291533
1.697856	233.838537	4.296538
1.871269	239.492834	4.301542
1.828146	239.267600	4.306547
1.911989	241.374724	4.311552
1.926150	230.517339	4.316557
1.625317	223.060889	4.321562
1.776619	225.570034	4.326566
1.556927	249.090880	4.331571
1.891409	240.461876	4.336576
1.551185	249.668816	4.341581
1.723699	255.091031	4.346586
1.923072	253.916409	4.351590
1.909083	248.426215	4.356595
1.614889	243.976583	4.361600
1.940973	251.895067	4.366605
1.550824	257.398327	4.371610
1.966640	259.377194	4.376614
1.751849	258.582176	4.381619
1.814240	259.733220	4.386624
1.886398	246.403979	4.391629
1.664156	254.031180	4.396634
1.876450	260.365607	4.401638
2.043029	269.681976	4.406643
1.970145	283.319113	4.411648
2.563103	280.760907	4.416653
2.143972	272.813338	4.421658
1.715865	267.951544	4.426662
1.914845	272.470633	4.431667
2.327552	274.381351	4.436672
1.994952	281.276916	4.441677
2.015734	283.650184	4.446682
2.336851	278.382615	4.451686
2.097325	287.021942	4.456691
2.230058	291.215369	4.461696
2.515517	279.747025	4.466701
2.162109	286.622157	4.471706
2.099016	282.874245	4.476710
2.284697	283.643835	4.481715
2.088240	291.079543	4.486720
2.349885	280.002558	4.491725
1.949525	286.952633	4.496730
2.262611	283.337502	4.501734
2.261382	288.787256	4.506739
2.172388	283.173595	4.511744
2.092584	287.219728	4.516749
1.941856	283.684696	4.521754
2.110218	289.663044	4.526758
2.138727	278.098157	4.531763
1.902670	282.118316	4.536768
2.441915	294.023123	4.541773
2.092082	310.458760	4.546778
2.483036	302.946454	4.551782
2.281459	321.007139	4.556787
2.452864	314.089209	4.561792
2.539975	322.080961	4.566797
2.612947	321.222995	4.571802
2.762875	324.220437	4.576806
2.697711	306.402570	4.581811
2.167444	299.858094	4.586816
2.778096	296.624717	4.591821
2.398739	300.112731	4.596826
2.514991	287.851128	4.601830
2.418045	297.792445	4.606835
2.461812	301.987554	4.611840
2.548588	310.167296	4.616845
2.381484	320.929402	4.621850
2.662009	321.080430	4.626854
2.749766	322.357415	4.631859
2.429101	322.641236	4.636864
2.699065	320.628400	4.641869
2.194898	321.383343	4.646874
2.864600	321.412936	4.651878
2.347794	321.241512	4.656883
2.798192	334.560574	4.661888
3.042701	325.546437	4.666893
2.487981	320.998560	4.671898
2.816100	321.693903	4.676902
2.804187	318.155359	4.681907
2.686040	322.298405	4.686912
2.824722	309.193412	4.691917
2.728752	327.215737	4.696922
2.606981	315.816636	4.701926
2.781404	317.711687	4.706931
2.564400	331.740869	4.711936
2.960494	318.035526	4.716941
2.790961	333.112982	4.721946
2.728570	332.444016	4.726950
3.006453	317.159874	4.731955
2.845746	324.920288	4.736960
2.842690	324.533343	4.741965
2.575596	332.557786	4.746970
3.107727	326.882408	4.751974
2.918709	328.462822	4.756979
2.770406	324.759664	4.761984
3.017809	324.745687	4.766989
2.816402	322.789930	4.771994
3.012674	331.732850	4.776998
2.986556	323.267769	4.782003
2.468089	347.281698	4.787008
3.058133	317.912947	4.792013
2.927880	332.749110	4.797018
2.825922	334.031895	4.802022
2.924977	340.815606	4.807027
3.039935	365.570375	4.812032
3.194090	353.242078	4.817037
3.211117	366.084943	4.822042
3.194278	351.209272	4.827046
3.121148	350.877216	4.832051
2.892639	357.161404	4.837056
3.080456	355.015239	4.842061
3.345169	367.335137	4.847066
3.455774	355.344733	4.852070
3.207915	349.202455	4.857075
2.888075	337.399514	4.862080
3.119631	349.605503	4.867085
3.057552	357.705588	4.872090
2.956882	361.496609	4.877094
3.353188	349.702186	4.882099
3.253582	363.672830	4.887104
3.184562	364.443472	4.892109
3.301048	367.126013	4.897114
3.296714	363.258369	4.902118
3.708387	370.564121	4.907123
3.395446	368.701473	4.912128
3.852752	350.207642	4.917133
3.172978	343.288787	4.922138
3.029860	348.937323	4.927142
3.245068	356.915225	4.932147
3.212473	351.570332	4.937152
3.566722	352.193286	4.942157
3.349524	363.328631	4.947162
3.049338	355.843301	4.952166
3.494355	356.605357	4.957171
3.200845	356.851543	4.962176
3.307573	351.692087	4.967181
3.397576	353.391250	4.972186
3.350439	353.828862	4.977190
3.569165	350.421491	4.982195
3.228837	358.505603	4.987200
3.674374	349.875648	4.992205
3.313929	364.858700	4.997210
3.426894	351.842963	5.002214
3.553722	361.800123	5.007219
3.397843	365.749932	5.012224
3.618614	342.991985	5.017229
3.401877	364.262455	5.022234
3.444894	355.572537	5.027238
3.313770	355.475496	5.032243
3.191285	361.409790	5.037248
3.312045	378.965525	5.042253
3.408899	386.855268	5.047258
3.365327	385.396697	5.052262
3.569954	378.495249	5.057267
3.589210	394.653135	5.062272
3.619040	381.086300	5.067277
3.533512	392.209576	5.072282
3.886595	389.819838	5.077286
3.738636	386.549910	5.082291
3.872275	394.472646	5.087296
3.929176	387.690317	5.092301
3.797520	397.958760	5.097306
3.466392	391.784744	5.102310
3.516984	395.517135	5.107315
3.329620	395.546592	5.112320
3.876105	406.050347	5.117325
3.998357	423.258318	5.122330
3.307501	405.723980	5.127334
4.091766	418.922830	5.132339
3.647194	423.703303	5.137344
4.183809	422.075647	5.142349
3.909746	435.874221	5.147354
4.049183	430.869652	5.152358
4.090554	425.949167	5.157363
3.857999	424.340687	5.162368
4.163784	416.495719	5.167373
3.677993	412.664315	5.172378
3.763759	416.322135	5.177382
4.105556	424.023039	5.182387
3.869328	427.979038	5.187392
3.918033	428.197677	5.192397
3.697273	424.970552	5.197402
3.607324	436.418482	5.202406
4.210177	427.482794	5.207411
4.109486	426.525168	5.212416
4.057784	428.462336	5.217421
4.165584	441.755728	5.222426
3.667966	430.669143	5.227430
3.966784	434.336846	5.232435
3.635777	438.813339	5.237440
4.105365	425.612227	5.242445
4.226907	434.974813	5.247450
4.058039	430.559368	5.252454
4.253533	423.794076	5.257459
4.009955	431.240006	5.262464
4.204482	432.950022	5.267469
4.131997	440.244263	5.272474
4.195887	448.366988	5.277478
4.302495	449.445823	5.282483
4.382066	456.116290	5.287488
4.402842	442.883669	5.292493
4.142235	434.701257	5.297498
4.334133	433.065451	5.302502
4.173751	434.277986	5.307507
4.136350	459.160490	5.312512
4.218781	466.596170	5.317517
4.728493	475.139608	5.322522
4.272198	457.207040	5.327526
4.438932	455.458679	5.332531
3.966542	469.243787	5.337536
4.158843	457.438302	5.342541
4.203715	459.320939	5.347546
4.382610	465.277193	5.352550
4.599566	459.775101	5.357555
4.507434	474.529528	5.362560
4.601003	475.925533	5.367565
4.365463	463.860440	5.372570
4.432710	461.797720	5.377574
4.418484	473.874141	5.382579
4.415019	465.821475	5.387584
4.516121	477.473457	5.392589
4.236597	473.096905	5.397594
4.457047	471.221770	5.402598
4.272982	470.075671	5.407603
4.134986	457.444053	5.412608
4.623640	469.213120	5.417613
4.382309	475.483788	5.422618
4.293269	458.784421	5.427622
4.343633	465.412956	5.432627
4.238407	500.007231	5.437632
4.355529	503.319718	5.442637
4.491492	499.118873	5.447642
4.657120	506.693940	5.452646
4.643788	503.075380	5.457651
4.454170	499.825926	5.462656
4.938593	500.480058	5.467661
4.449121	507.957781	5.472666
4.496567	499.886719	5.477670
4.574107	495.613151	5.482675
4.509708	510.094977	5.487680
4.735478	501.435056	5.492685
4.801550	504.020782	5.497690
4.596126	497.313424	5.502694
4.799556	493.503264	5.507699
4.618202	509.280356	5.512704
4.770890	510.012000	5.517709
4.791914	531.458089	5.522714
5.000207	526.653633	5.527718
5.261786	521.737473	5.532723
4.798223	515.452203	5.537728
4.747972	512.002921	5.542733
4.707664	512.928060	5.547738
4.865653	524.431175	5.552742
4.972117	529.870815	5.557747
4.734471	532.467470	5.562752
5.009222	530.538958	5.567757
5.039954	531.857645	5.572762
4.931216	543.730423	5.577766
5.243587	536.745294	5.582771
4.948239	529.574193	5.587776
4.860312	542.737034	5.592781
5.007254	530.187709	5.597786
5.036178	534.882866	5.602790
5.411869	540.309491	5.607795
5.184340	542.236957	5.612800
5.096597	524.210257	5.617805
4.963833	531.057420	5.622810
5.075772	539.354573	5.627814
5.166390	526.101953	5.632819
4.963101	542.290949	5.637824
5.242800	527.446313	5.642829
5.089143	543.323834	5.647834
4.681599	528.645055	5.652838
5.255700	526.630275	5.657843
4.957982	526.236277	5.662848
5.087136	520.878604	5.667853
4.925744	532.542041	5.672858
4.732430	523.739249	5.677862
5.141787	524.999411	5.682867
4.953511	531.506598	5.687872
4.982089	531.947487	5.692877
5.303686	551.456411	5.697882
5.471367	568.350999	5.702886
5.411828	552.523825	5.707891
5.001626	555.891599	5.712896
5.140283	559.718593	5.717901
5.551275	568.383074	5.722906
5.404222	558.320546	5.727910
5.565770	569.529303	5.732915
5.405784	569.182689	5.737920
5.512791	554.680988	5.742925
5.062668	537.909497	5.747930
5.503037	561.655897	5.752934
5.764569	557.131406	5.757939
5.016840	547.361025	5.762944
5.614313	552.320855	5.767949
5.567475	566.007509	5.772954
5.368800	573.610057	5.777958
5.749891	569.581392	5.782963
5.303083	573.918912	5.787968
5.413799	568.136686	5.792973
5.411857	569.247772	5.797978
5.402709	574.586762	5.802982
5.637391	580.150259	5.807987
5.267190	583.139783	5.812992
5.382098	571.006235	5.817997
5.497060	575.681169	5.823002
5.319423	580.408699	5.828006
5.722002	576.325969	5.833011
5.408308	574.643174	5.838016
5.730875	584.716613	5.843021
5.405587	572.554979	5.848026
5.527170	578.033080	5.853030
5.764869	581.575066	5.858035
5.512786	579.595882	5.863040
5.643588	573.335986	5.868045
5.442816	575.512093	5.873050
5.552658	572.010000	5.878054
5.762655	571.317715	5.883059
5.639385	602.019784	5.888064
5.644734	601.326589	5.893069
5.890013	594.658658	5.898074
5.987778	607.544617	5.903078
5.995232	594.101854	5.908083
5.608374	593.965678	5.913088
5.818898	592.793431	5.918093
5.690684	593.701334	5.923098
5.736697	596.405426	5.928102
6.106426	601.626665	5.933107
5.901951	604.949895	5.938112
6.134392	611.680212	5.943117
5.853927	594.384667	5.948122
5.564665	597.428103	5.953126
5.936873	601.441551	5.958131
5.631600	607.712579	5.963136
6.034097	592.603408	5.968141
5.927209	595.616508	5.973146
5.542631	600.311451	5.978150
6.226454	597.130542	5.983155
5.789834	597.501604	5.988160
6.178836	593.916772	5.993165
5.881607	601.382699	5.998170
6.137549	590.669793	6.003174
6.039484	592.743590	6.008179
5.501438	608.802892	6.013184
5.724069	602.033137	6.018189
5.783563	600.883973	6.023194
5.854879	605.085070	6.028198
6.128693	602.985236	6.033203
6.135651	633.316103	6.038208
5.932317	611.009753	6.043213
6.019680	627.545638	6.048218
6.148463	631.676473	6.053222
6.227206	622.393877	6.058227
6.261656	616.806853	6.063232
5.862644	600.986102	6.068237
5.871634	603.380508	6.073242
5.692450	611.407242	6.078246
6.022969	618.674334	6.083251
5.942765	631.288519	6.088256
5.942352	628.491395	6.093261
6.033080	625.906914	6.098266
6.169023	634.485670	6.103270
6.363973	624.404763	6.108275
5.991952	622.183159	6.113280
6.242918	635.262058	6.118285
6.001023	628.360589	6.123290
5.987048	632.088613	6.128294
6.132605	631.198410	6.133299
6.228319	637.631185	6.138304
6.133262	638.333926	6.143309
6.326176	636.119496	6.148314
5.985077	645.363616	6.153318
5.939704	642.488974	6.158323
6.045587	633.196362	6.163328
5.734980	642.767328	6.168333
6.261670	632.286882	6.173338
5.855129	640.941082	6.178342
5.755657	644.826983	6.183347
5.751599	644.046942	6.188352
5.878089	645.913747	6.193357
5.786868	637.936266	6.198362
5.760455	648.400981	6.203366
6.122260	647.144733	6.208371
5.877021	660.287203	6.213376
6.156305	669.657014	6.218381
6.163769	680.099973	6.223386
6.562877	667.896988	6.228390
6.181721	659.756476	6.233395
6.025050	650.243133	6.238400
5.818588	648.929746	6.243405
6.348505	644.395901	6.248410
5.963272	654.861018	6.253414
6.391835	633.082319	6.258419
6.290183	650.469613	6.263424
6.298754	637.565500	6.268429
6.330861	627.560238	6.273434
6.222811	643.167993	6.278438
6.639322	644.112361	6.283443
6.304793	651.050438	6.288448
6.447387	647.319355	6.293453
6.361192	639.056117	6.298458
6.084455	626.308771	6.303462
6.188639	597.282409	6.308467
6.024644	607.469417	6.313472
5.941604	611.953622	6.318477
6.369881	611.004071	6.323482
6.221446	613.549297	6.328486
6.236608	612.966161	6.333491
5.778946	604.428297	6.338496
5.567766	601.659891	6.343501
5.946544	627.267499	6.348506
5.865389	631.444372	6.353510
6.214835	625.012175	6.358515
6.170847	642.348001	6.363520
6.321745	629.861082	6.368525
6.227077	629.653930	6.373530
5.788708	642.555016	6.378534
6.203448	628.653242	6.383539
6.133939	641.316378	6.388544
6.293982	639.191930	6.393549
6.156203	637.064804	6.398554
5.994322	637.994453	6.403558
6.124406	627.724874	6.408563
5.740639	634.696238	6.413568
6.156097	633.728777	6.418573
6.349694	641.631768	6.423578
6.175873	638.982774	6.428582
6.296579	631.131286	6.433587
5.832483	628.835512	6.438592
6.145991	630.965412	6.443597
6.106255	637.078522	6.448602
5.913018	641.221828	6.453606
6.262581	651.821238	6.458611
5.903059	645.002441	6.463616
6.062754	642.130513	6.468621
6.404202	639.531828	6.473626
5.792306	629.814915	6.478630
6.010003	627.654007	6.483635
6.179400	636.533274	6.488640
6.337646	636.811755	6.493645
6.244626	629.967374	6.498650
6.121061	621.600612	6.503654
5.874140	610.842339	6.508659
5.773822	606.130885	6.513664
6.019943	635.474029	6.518669
6.319685	638.703387	6.523674
5.759576	641.664715	6.528678
6.117246	638.068081	6.533683
6.143993	631.723541	6.538688
6.062405	637.193309	6.543693
6.231274	642.729424	6.548698
6.206902	634.167889	6.553702
6.215961	630.083877	6.558707
6.113001	645.310266	6.563712
6.087360	643.770372	6.568717
6.070853	644.960726	6.573722
5.822611	636.841179	6.578726
5.929953	654.019018	6.583731
5.794924	643.901567	6.588736
6.007667	640.641334	6.593741
5.914263	640.113430	6.598746
5.861713	654.806438	6.603750
6.207611	644.509965	6.608755
6.107537	644.528252	6.613760
6.283556	646.878982	6.618765
6.414279	658.267326	6.623770
6.066390	643.700520	6.628774
6.330060	644.860458	6.633779
5.951681	656.732302	6.638784
5.989316	649.823897	6.643789
6.052097	637.958975	6.648794
5.740210	650.425490	6.653798
6.236624	639.927844	6.658803
5.932525	654.297778	6.663808
6.282713	651.204452	6.668813
5.932891	647.214962	6.673818
5.776994	650.870251	6.678822
6.059417	647.834691	6.683827
6.015717	649.119220	6.688832
5.988026	645.267599	6.693837
6.124841	644.237857	6.698842
6.050406	647.156318	6.703846
6.142088	643.764255	6.708851
6.087833	645.743703	6.713856
6.064449	639.827533	6.718861
6.073351	629.289698	6.723866
5.975186	649.679383	6.728870
6.297661	638.542563	6.733875
6.183759	650.589126	6.738880
6.104520	640.390831	6.743885
6.081277	636.809887	6.748890
6.004481	650.316385	6.753894
5.818310	635.786891	6.758899
5.883678	645.176253	6.763904
5.776630	639.827679	6.768909
6.350618	634.804213	6.773914
5.716557	639.232087	6.778918
6.097187	634.947265	6.783923
6.215619	637.869863	6.788928
6.067341	641.771228	6.793933
6.350460	638.639855	6.798938
6.105323	639.198889	6.803942
6.095028	631.934954	6.808947
5.865856	645.590839	6.813952
5.643636	648.076637	6.818957
6.223765	645.220176	6.823962
6.118325	657.193622	6.828966
6.190175	643.059231	6.833971
6.209717	652.092120	6.838976
5.965937	629.244181	6.843981
6.280456	636.854494	6.848986
6.127847	646.042998	6.853990
6.151263	643.469539	6.858995
6.164510	646.424715	6.864000
6.083103	640.149643	6.869005
6.414389	639.563496	6.874010
6.139524	652.341576	6.879014
6.190976	642.026379	6.884019
6.089637	649.696541	6.889024
6.027182	641.155305	6.894029
6.083532	632.660937	6.899034
6.215011	632.068740	6.904038
6.052440	642.966076	6.909043
5.868858	646.184146	6.914048
5.936296	638.097178	6.919053
6.149328	651.926146	6.924058
5.978127	654.868197	6.929062
6.090191	631.429088	6.934067
6.329247	641.840458	6.939072
6.103205	649.159285	6.944077
6.289964	643.523897	6.949082
5.784871	653.312882	6.954086
5.904382	652.051487	6.959091
6.164328	645.150546	6.964096
6.014289	642.159716	6.969101
6.532698	649.326810	6.974106
5.997129	651.433253	6.979110
6.083538	645.832797	6.984115
6.016536	645.456115	6.989120
5.952585	643.324286	6.994125
6.203489	646.937112	6.999130
5.886315	650.205081	7.004134
6.097798	645.349153	7.009139
5.877967	648.677398	7.014144
5.766023	643.736401	7.019149
6.125746	643.721425	7.024154
6.251576	652.326033	7.029158
6.256785	649.613711	7.034163
5.893328	654.493124	7.039168
5.949482	651.392941	7.044173
6.357085	645.118943	7.049178
5.873887	652.964583	7.054182
6.464028	647.686173	7.059187
6.155216	651.987098	7.064192
6.358473	650.035954	7.069197
6.322714	649.803873	7.074202
6.038809	651.104320	7.079206
6.154846	647.138674	7.084211
6.093162	640.297495	7.089216
6.163972	644.630101	7.094221
6.348391	655.922552	7.099226
5.861513	651.179168	7.104230
6.387256	649.145727	7.109235
6.076880	642.112612	7.114240
6.075617	650.801561	7.119245
6.376730	652.591069	7.124250
6.126930	655.118423	7.129254
6.243364	648.959233	7.134259
6.012578	659.005083	7.139264
6.071836	652.795455	7.144269
6.464186	653.698927	7.149274
6.205741	653.709052	7.154278
6.356095	641.408186	7.159283
5.838853	649.208345	7.164288
6.042806	647.157539	7.169293
6.051880	639.546181	7.174298
6.017190	646.935694	7.179302
5.934381	645.970067	7.184307
5.991258	651.972702	7.189312
5.816019	643.823723	7.194317
6.242880	652.030320	7.199322
6.056135	652.710427	7.204326
6.478723	647.633345	7.209331
6.450936	655.399189	7.214336
6.292310	653.627224	7.219341
6.659340	644.137543	7.224346
6.009030	625.699643	7.229350
6.020571	621.680337	7.234355
5.797748	620.298819	7.239360
5.920408	611.397884	7.244365
5.887227	627.656729	7.249370
5.810673	640.158340	7.254374
6.066133	639.097942	7.259379
6.220140	645.801673	7.264384
5.863335	654.623471	7.269389
6.475249	661.926758	7.274394
5.979340	653.656139	7.279398
6.520236	659.576720	7.284403
6.466913	638.792508	7.289408
6.230903	625.523139	7.294413
6.113110	621.157999	7.299418
5.486521	624.462295	7.304422
6.090574	632.203036	7.309427
6.341219	649.593477	7.314432
6.091676	647.586437	7.319437
5.846660	615.458895	7.324442
5.813140	632.229443	7.329446
6.387994	638.323567	7.334451
6.001785	643.893893	7.339456
6.189363	644.346494	7.344461
6.413101	640.361671	7.349466
5.856958	622.335011	7.354470
6.128340	615.633851	7.359475
5.835550	617.330496	7.364480
5.963259	642.846628	7.369485
6.381224	644.772903	7.374490
6.335481	637.361508	7.379494
6.121936	628.933546	7.384499
5.945821	612.550494	7.389504
5.822803	612.278078	7.394509
6.304795	626.819781	7.399514
6.376307	626.581713	7.404518
6.262759	612.278994	7.409523
6.016405	615.321756	7.414528
6.286131	615.909262	7.419533
6.005314	609.981185	7.424538
6.058638	604.159495	7.429542
5.705613	615.221473	7.434547
6.087702	614.779852	7.439552
6.118554	620.061340	7.444557
5.741865	616.626615	7.449562
6.214019	641.612264	7.454566
6.278219	639.068274	7.459571
6.029264	630.116860	7.464576
5.812608	634.369500	7.469581
6.315587	633.366167	7.474586
5.964579	634.040466	7.479590
6.179356	642.359848	7.484595
5.987675	633.946029	7.489600
6.220047	644.923721	7.494605
6.164015	640.035838	7.499610
6.080040	635.418952	7.504614
6.084341	623.567356	7.509619
5.903277	623.288154	7.514624
6.115851	644.184592	7.519629
6.312033	642.117412	7.524634
6.283687	627.148565	7.529638
6.271249	626.317127	7.534643
5.932132	614.713291	7.539648
5.641242	626.278822	7.544653
6.188017	633.486309	7.549658
6.097071	646.443739	7.554662
6.190666	638.559039	7.559667
6.199831	622.842973	7.564672
5.750627	613.918544	7.569677
6.029356	620.622864	7.574682
6.024628	635.197650	7.579686
6.259415	643.471993	7.584691
6.602556	639.584646	7.589696
6.064480	632.104849	7.594701
6.101353	621.570882	7.599706
6.132540	621.245655	7.604710
6.125088	623.057736	7.609715
6.035077	612.609168	7.614720
5.777983	621.726328	7.619725
6.201718	618.097472	7.624730
6.190299	616.997614	7.629734
6.221909	612.843877	7.634739
6.233146	618.206743	7.639744
5.864675	615.067819	7.644749
6.109468	620.609830	7.649754
5.880295	615.464950	7.654758
5.758973	608.480720	7.659763
6.096553	629.268970	7.664768
5.712883	641.191992	7.669773
6.376193	646.150445	7.674778
5.976248	648.313204	7.679782
5.791275	645.989751	7.684787
6.311924	653.905494	7.689792
6.158047	657.685155	7.694797
6.228472	649.533954	7.699802
6.136411	656.213238	7.704806
6.107450	654.922610	7.709811
6.147853	646.370194	7.714816
6.000563	667.576923	7.719821
6.294262	649.051168	7.724826
6.082112	661.773114	7.729830
6.147124	644.934531	7.734835
6.634799	647.997870	7.739840
6.119561	640.013998	7.744845
6.119187	624.728769	7.749850
5.983635	619.226665	7.754854
5.733033	617.233912	7.759859
5.926518	614.471541	7.764864
5.977467	633.598695	7.769869
6.460420	647.321491	7.774874
6.207781	629.930246	7.779878
6.103374	610.699703	7.784883
6.360124	617.247137	7.789888
5.578496	627.285238	7.794893
5.677818	615.184716	7.799898
5.466795	637.354483	7.804902
5.846914	654.237737	7.809907
6.189245	644.883254	7.814912
6.211125	652.286409	7.819917
6.319993	654.085685	7.824922
6.455985	648.567406	7.829926
6.137179	667.055822	7.834931
6.250042	664.713436	7.839936
6.208390	660.982509	7.844941
6.384547	644.959817	7.849946
6.144921	639.399331	7.854950
6.168921	626.062922	7.859955
6.040449	627.999482	7.864960
5.665697	620.992900	7.869965
6.014693	623.209378	7.874970
6.125474	638.999494	7.879974
6.131467	646.890277	7.884979
6.371004	644.781106	7.889984
5.978794	629.170924	7.894989
6.224691	616.150755	7.899994
6.034907	625.577632	7.904998
6.024682	617.569808	7.910003
6.315923	619.021656	7.915008
5.973249	623.003484	7.920013
5.790584	611.766062	7.925018
5.964111	633.507337	7.930022
6.310283	639.365968	7.935027
6.421343	643.899696	7.940032
5.845502	631.498144	7.945037
6.374985	623.160402	7.950042
5.966679	619.190154	7.955046
5.821349	624.362143	7.960051
6.079283	624.013750	7.965056
6.161676	642.025515	7.970061
6.368210	642.438776	7.975066
6.174242	622.194306	7.980070
6.016124	611.686156	7.985075
5.989442	618.733961	7.990080
5.879120	628.862588	7.995085
6.200833	621.110682	8.000090
6.141697	629.849041	8.005094
5.871511	628.207689	8.010099
6.321072	630.064217	8.015104
6.310628	634.816720	8.020109
6.049925	615.114486	8.025126
6.076685	621.374612	8.030144
5.914950	620.799654	8.035162
6.032372	622.878847	8.040179
6.315585	627.734646	8.045197
6.435176	625.575001	8.050214
5.951111	619.413715	8.055232
6.060520	634.589227	8.060250
5.782564	613.346695	8.065267
6.060829	640.320932	8.070285
6.411353	641.728161	8.075302
6.248387	628.395054	8.080320
5.911301	627.130901	8.085338
6.421419	634.983285	8.090355
6.142016	638.818489	8.095373
5.795849	637.963929	8.100390
5.827051	631.455529	8.105408
6.252668	657.674677	8.110426
6.203695	658.211780	8.115443
6.243011	666.427067	8.120461
6.070414	658.151387	8.125478
6.354767	658.100336	8.130496
6.339856	668.377355	8.135514
6.414372	650.914498	8.140531
6.291981	656.523132	8.145549
6.221600	647.221206	8.150566
6.139881	637.932574	8.155584
6.353851	660.289396	8.160602
6.311372	645.900335	8.165619
5.854441	652.030503	8.170637
6.504098	646.806449	8.175654
6.325134	652.627346	8.180672
6.213394	653.223237	8.185690
6.389161	643.189229	8.190707
6.239453	644.733444	8.195725
6.232794	644.096153	8.200742
6.358770	635.758844	8.205760
5.877582	635.729006	8.210778
6.269487	642.460984	8.215795
6.127501	657.734450	8.220813
6.530658	652.187909	8.225830
6.596933	660.243648	8.230848
6.472324	659.677019	8.235866
6.462870	639.433588	8.240883
6.440736	632.999147	8.245901
6.402789	633.042491	8.250918
6.126942	626.404356	8.255936
5.714010	632.302878	8.260954
6.491341	642.152952	8.265971
6.196350	666.428490	8.270989
6.378881	655.999826	8.276006
6.248566	647.868416	8.281024
6.392999	654.159297	8.286042
6.521163	653.949445	8.291059
6.446768	654.861449	8.296077
6.649480	655.178253	8.301094
6.561091	642.964195	8.306112
6.277959	623.522759	8.311130
6.549080	625.722294	8.316147
6.439283	631.002619	8.321165
6.232499	608.091062	8.326182
6.419064	621.430237	8.331200
6.391140	627.899955	8.336218
6.332709	616.702234	8.341235
6.309718	636.678653	8.346253
6.458318	641.423754	8.351270
6.574332	656.445666	8.356288
6.449514	660.328053	8.361306
6.499472	636.527136	8.366323
6.170891	640.176311	8.371341
6.546952	648.982080	8.376358
6.318919	646.822704	8.381376
6.598561	660.586312	8.386394
6.500012	659.949641	8.391411
6.718375	656.579205	8.396429
6.273292	643.801470	8.401446
6.349564	636.392578	8.406464
6.400637	657.945958	8.411482
6.144943	641.434463	8.416499
6.317419	658.002466	8.421517
6.344851	658.794708	8.426534
6.363456	645.626034	8.431552
6.358341	658.541883	8.436570
6.758646	648.416445	8.441587
6.422374	653.863805	8.446605
6.117116	659.048019	8.451622
6.425351	653.011549	8.456640
6.153443	667.105339	8.461658
6.434183	657.590785	8.466675
6.137462	654.288739	8.471693
6.510919	684.205929	8.476710
6.530567	698.063904	8.481728
6.234204	695.492169	8.486746
6.438295	699.441549	8.491763
6.582305	687.302515	8.496781
6.745771	695.590001	8.501798
6.361829	686.487380	8.506816
6.479613	695.011211	8.511834
6.727079	688.233037	8.516851
6.304381	691.124887	8.521869
6.528506	689.513702	8.526886
6.506507	687.642260	8.531904
6.341661	692.097604	8.536922
6.726974	686.569253	8.541939
6.813650	683.422701	8.546957
6.500448	697.144671	8.551974
6.741833	691.632132	8.556992
6.665354	693.157953	8.562010
6.654280	696.984453	8.567027
6.531872	695.309197	8.572045
6.707151	695.551711	8.577063
6.895940	702.025601	8.582080
6.556269	693.550388	8.587098
6.599443	689.881101	8.592115
6.792404	697.661836	8.597133
6.695358	689.345805	8.602151
6.852215	700.334975	8.607168
6.549558	690.452327	8.612186
6.378355	694.683664	8.617203
6.448521	697.162829	8.622221
6.542261	706.199208	8.627239
6.762353	693.851470	8.632256
6.636746	706.240520	8.637274
6.973432	705.095684	8.642291
6.950478	701.174082	8.647309
6.354234	701.914597	8.652327
6.600497	696.958727	8.657344
6.788985	718.191310	8.662362
7.060913	722.983366	8.667379
7.024596	716.104957	8.672397
6.802820	708.278832	8.677415
6.839496	694.111051	8.682432
6.597146	692.345597	8.687450
6.600121	689.826248	8.692467
6.865527	707.677036	8.697485
6.706261	719.571061	8.702503
7.121655	715.510691	8.707520
6.451681	709.079358	8.712538
6.789434	728.884394	8.717555
7.152455	728.208249	8.722573
7.232097	722.369341	8.727591
6.842619	700.355103	8.732608
6.523569	691.151910	8.737626
6.630506	693.860486	8.742643
6.985267	704.426868	8.747661
6.670771	719.156369	8.752679
7.030708	719.972098	8.757696
6.660164	719.812283	8.762714
7.116532	729.957929	8.767731
7.143147	724.996033	8.772749
6.416805	715.603878	8.777767
6.629366	717.210949	8.782784
6.761808	719.420325	8.787802
6.797176	713.592477	8.792819
6.869328	718.148205	8.797837
6.589979	712.682840	8.802855
6.730560	714.320601	8.807872
6.729331	728.024207	8.812890
6.986012	714.913555	8.817907
7.057736	718.210231	8.822925
6.942252	719.074805	8.827943
7.036773	717.074085	8.832960
7.050300	732.896528	8.837978
6.526785	732.150684	8.842995
7.131761	717.070710	8.848013
6.880836	721.939427	8.853031
6.781690	736.193771	8.858048
6.998085	732.308579	8.863066
6.783994	725.870296	8.868083
6.990472	729.065291	8.873101
7.093057	728.196891	8.878119
7.275000	731.057911	8.883136
7.118320	727.906791	8.888154
7.304544	722.055584	8.893171
7.114353	728.992730	8.898189
6.931181	717.664986	8.903207
7.271153	722.984972	8.908224
7.128626	729.857461	8.913242
7.183836	726.072220	8.918259
7.191913	732.667899	8.923277
7.104586	725.837081	8.928295
7.088172	733.939490	8.933312
6.824380	728.741775	8.938330
6.967139	737.570699	8.943347
7.123436	721.437806	8.948365
6.738974	736.643762	8.953383
7.061934	740.402772	8.958400
6.912458	737.779596	8.963418
6.847486	728.227362	8.968435
7.036659	733.802250	8.973453
6.886385	748.280961	8.978471
7.160501	744.353851	8.983488
7.492130	749.283957	8.988506
7.288807	754.818614	8.993523
7.351225	754.097968	8.998541
7.166061	742.608259	9.003559
7.340447	731.808418	9.008576
7.237967	735.221566	9.013594
7.098171	739.864383	9.018611
7.415777	732.663353	9.023629
6.984701	733.625250	9.028647
7.171877	738.728606	9.033664
7.168617	736.438586	9.038682
7.362830	748.680741	9.043699
7.406841	733.889874	9.048717
7.143889	739.180685	9.053735
7.150089	731.137577	9.058752
7.261746	744.179450	9.063770
6.897544	739.812549	9.068787
7.298713	739.506213	9.073805
7.174863	754.318494	9.078823
7.379040	748.602967	9.083840
7.070296	752.073134	9.088858
7.002015	748.169639	9.093875
7.617761	745.064854	9.098893
7.269941	757.834404	9.103911
7.163454	757.465430	9.108928
7.491893	748.790326	9.113946
7.062000	752.728367	9.118963
7.526009	749.391910	9.123981
7.444701	753.465323	9.128999
7.255020	754.541830	9.134016
7.070108	756.975476	9.139034
7.068099	754.059963	9.144051
7.113371	740.537553	9.149069
7.194101	754.665060	9.154087
7.192063	751.157829	9.159104
7.267223	744.163561	9.164122
7.192367	751.494084	9.169139
7.232492	736.869377	9.174157
7.287003	743.361441	9.179175
7.331730	754.187026	9.184192
7.552285	746.225789	9.189210
6.964315	753.497923	9.194227
6.938564	754.132355	9.199245
7.220564	769.729596	9.204263
7.565536	777.328488	9.209280
7.553606	772.279754	9.214298
7.686117	790.280333	9.219315
7.856601	771.405860	9.224333
7.445720	762.428196	9.229351
7.444567	752.495191	9.234368
7.273619	748.074998	9.239386
7.340501	757.119093	9.244403
7.668111	778.627928	9.249421
7.617234	768.062889	9.254439
7.689903	759.756661	9.259456
7.510401	762.893717	9.264474
7.424703	753.592487	9.269491
7.789366	755.833265	9.274509
7.418978	758.295691	9.279527
7.516071	751.762870	9.284544
7.992814	757.106026	9.289562
7.388193	760.361554	9.294579
7.480074	750.281704	9.299597
7.460306	747.573520	9.304615
7.500864	740.876160	9.309632
7.650656	744.770757	9.314650
7.398451	750.625246	9.319667
7.553657	739.959549	9.324685
7.553380	751.585144	9.329703
7.223802	744.343644	9.334720
7.659868	757.280943	9.339738
7.636255	779.152687	9.344755
7.616776	771.873410	9.349773
7.612469	769.260780	9.354791
7.375125	771.352860	9.359808
7.672213	783.796803	9.364826
7.495800	787.339975	9.369843
7.710840	776.927409	9.374861
7.718177	793.544890	9.379879
7.668155	780.732065	9.384896
7.852720	786.296516	9.389914
7.695329	783.585975	9.394931
7.912031	786.231161	9.399949
7.627093	771.748312	9.404967
7.761100	765.865765	9.409984
7.547211	758.482819	9.415002
7.634626	765.978231	9.420019
7.575866	768.628883	9.425037
7.610092	783.287040	9.430055
7.756757	780.476065	9.435072
7.965211	784.811194	9.440090
7.670068	789.604773	9.445107
7.830281	777.075559	9.450125
7.856956	786.009309	9.455143
7.835055	782.398875	9.460160
7.879099	751.982999	9.465178
7.493208	757.591225	9.470195
7.642952	773.002389	9.475213
7.933837	771.324859	9.480231
7.678887	780.382690	9.485248
7.805441	778.163616	9.490266
7.512489	784.723645	9.495283
7.719928	773.749838	9.500301
7.852747	786.196327	9.505319
7.847585	790.284229	9.510336
7.870697	783.954039	9.515354
7.792903	797.006992	9.520371
7.994305	783.418887	9.525389
8.054619	780.482837	9.530407
7.682654	785.014749	9.535424
7.907331	783.523718	9.540442
7.573289	789.402570	9.545459
7.925318	792.667801	9.550477
7.946835	791.615585	9.555495
7.994116	792.215513	9.560512
7.888986	786.926610	9.565530
7.957037	794.835498	9.570547
8.177437	795.376115	9.575565
8.268693	788.469604	9.580583
7.684133	783.577000	9.585600
8.119268	779.489536	9.590618
7.680003	781.731303	9.595635
7.698009	798.077487	9.600653
7.922006	793.484356	9.605671
7.967852	788.310735	9.610688
7.815756	788.703200	9.615706
7.712365	800.487383	9.620723
7.755279	791.810530	9.625741
7.684383	782.649920	9.630759
7.601945	791.297526	9.635776
7.869422	783.445719	9.640794
7.928167	783.521896	9.645811
7.994727	779.068152	9.650829
7.795115	792.647048	9.655847
7.804172	788.859480	9.660864
7.795631	797.430322	9.665882
7.899733	809.203643	9.670899
8.002938	813.119438	9.675917
8.111607	826.238632	9.680935
7.903957	833.877900	9.685952
8.361059	818.759283	9.690970
7.971243	830.947649	9.695987
8.153195	816.950497	9.701005
8.381007	817.702254	9.706023
8.271968	814.840927	9.711040
8.324713	797.942230	9.716058
8.098616	804.288204	9.721075
7.981142	798.314056	9.726093
8.059475	783.968177	9.731111
7.786205	793.129616	9.736128
8.129716	810.254553	9.741146
8.105886	821.647422	9.746163
8.225310	818.154447	9.751181
8.274611	821.732165	9.756199
8.291830	824.013640	9.761216
8.413045	802.865286	9.766234
7.861676	807.442696	9.771251
8.051907	803.469503	9.776269
8.371942	819.292653	9.781287
8.146459	827.887258	9.786304
8.480701	820.277899	9.791322
8.038011	800.370272	9.796339
8.254168	807.020557	9.801357
8.115946	803.555795	9.806375
7.889010	820.709275	9.811392
8.205070	822.528052	9.816410
8.193906	817.908826	9.821427
8.326328	829.687225	9.826445
8.782851	817.035699	9.831463
8.050736	831.002476	9.836480
8.280912	821.816003	9.841498
8.076548	825.748579	9.846515
8.010169	825.001780	9.851533
8.616231	819.093655	9.856551
8.310589	835.023759	9.861568
8.462088	817.898226	9.866586
7.930509	831.906458	9.871603
8.169290	825.573971	9.876621
8.465813	815.673708	9.881639
8.212132	821.853411	9.886656
8.377708	825.675157	9.891674
8.296845	824.942462	9.896691
7.933823	825.142068	9.901709
8.491413	824.650952	9.906727
8.082731	817.106599	9.911744
8.287559	820.896369	9.916762
8.431556	824.990138	9.921779
7.814772	826.327550	9.926797
8.032015	811.624300	9.931815
8.038507	830.477594	9.936832
8.248610	850.114642	9.941850
8.190137	843.429765	9.946867
8.428737	846.590741	9.951885
8.592580	846.999785	9.956903
8.124345	853.397897	9.961920
8.655108	853.821491	9.966938
8.584714	859.476320	9.971955
8.693507	852.700226	9.976973
8.654136	842.184899	9.981991
8.671797	849.200822	9.987008
8.640932	847.093662	9.992026
8.463470	856.355132	9.997043
8.530632	855.759069	10.002061
8.473284	848.640712	10.007079
8.414041	863.465547	10.012096
8.702016	851.258113	10.017114
8.610883	857.186106	10.022131
8.677850	857.201091	10.027149
8.821676	859.965008	10.032167
8.638708	863.583185	10.037184
8.517858	843.333489	10.042202
8.480704	837.405590	10.047219
8.276308	857.913959	10.052237
8.518645	852.235978	10.057255
8.554873	850.191832	10.062272
8.466086	856.061081	10.067290
8.525111	863.976909	10.072307
8.572284	855.839676	10.077325
8.681607	847.624669	10.082343
8.367568	842.902659	10.087360
8.496160	846.815447	10.092378
8.473425	847.648169	10.097395
8.317319	869.373165	10.102413
8.353727	851.480528	10.107431
8.351415	855.698957	10.112448
8.631757	859.826395	10.117466
8.398646	859.315084	10.122483
8.669197	875.098347	10.127501
8.904376	887.259151	10.132519
8.880485	886.664159	10.137536
8.708747	879.307157	10.142554
8.636270	883.668170	10.147571
8.677908	891.863413	10.152589
9.053429	883.697197	10.157607
8.833799	878.970497	10.162624
9.119557	861.541575	10.167642
8.914688	867.827089	10.172659
8.473669	850.471342	10.177677
8.869775	857.524122	10.182695
8.371227	856.131539	10.187712
8.914285	856.362484	10.192730
8.700809	867.424780	10.197747
8.936977	875.543191	10.202765
8.869390	877.581153	10.207783
8.645960	869.396029	10.212800
8.669288	885.943656	10.217818
8.827177	881.386617	10.222835
8.482475	889.746079	10.227853
8.741978	885.076987	10.232871
8.866708	891.663888	10.237888
9.003316	871.033970	10.242906
9.160484	888.867724	10.247923
8.888033	886.296040	10.252941
8.857047	890.411854	10.257959
8.596460	899.107361	10.262976
8.519350	889.191446	10.267994
9.033083	889.672176	10.273011
8.618301	891.050905	10.278029
8.493887	900.039998	10.283047
8.472858	889.706026	10.288064
8.902286	890.136722	10.293082
8.808167	902.812901	10.298099
8.943535	913.941775	10.303117
9.498606	906.783496	10.308135
9.192394	907.046438	10.313152
9.179039	896.210097	10.318170
9.275045	895.458897	10.323187
9.107999	892.752687	10.328205
8.786962	888.140954	10.333223
8.893829	908.441680	10.338240
8.875869	897.272297	10.343258
8.955989	893.571467	10.348275
9.023837	890.661901	10.353293
8.961721	885.682634	10.358311
8.681411	895.653230	10.363328
8.744733	901.191998	10.368346
9.172352	914.218508	10.373363
9.072389	927.484944	10.378381
9.068360	929.218955	10.383399
9.056588	920.116691	10.388416
9.185421	923.983699	10.393434
9.581615	914.693372	10.398451
9.115916	931.549972	10.403469
9.562707	915.212893	10.408487
9.135053	910.027139	10.413504
9.091306	897.240834	10.418522
9.124592	893.932127	10.423539
9.103938	908.458846	10.428557
9.201674	915.575918	10.433575
9.006754	917.594777	10.438592
8.938397	919.527575	10.443610
9.000833	922.593487	10.448627
9.195297	933.824402	10.453645
9.159571	918.739302	10.458663
9.199830	937.925279	10.463680
9.139420	934.491913	10.468698
9.426275	913.813097	10.473715
9.041493	934.263203	10.478733
9.382689	925.020730	10.483751
9.522632	924.133747	10.488768
9.515571	924.739511	10.493786
9.662698	918.689804	10.498803
9.397190	926.575450	10.503821
9.421659	900.389171	10.508839
9.464495	900.729842	10.513856
8.803510	896.240217	10.518874
9.208536	902.175394	10.523891
9.314380	921.801225	10.528909
9.206148	923.437711	10.533927
9.593900	923.759763	10.538944
9.620387	920.263820	10.543962
9.926860	910.231756	10.548979
9.212274	910.027824	10.553997
9.075081	904.048332	10.559015
9.255691	902.893059	10.564032
8.950293	915.591173	10.569050
9.495282	930.065574	10.574067
9.350511	915.543092	10.579085
9.434026	921.001574	10.584103
9.563587	932.348117	10.589120
9.475085	921.254339	10.594138
9.933959	909.816220	10.599155
9.510715	933.229859	10.604173
9.694855	931.496145	10.609191
9.524904	917.614920	10.614208
9.298153	923.995002	10.619226
9.638700	913.829176	10.624243
9.210131	914.797853	10.629261
9.710608	922.969445	10.634279
9.913943	905.501348	10.639296
9.405269	908.002100	10.644314
9.544117	894.152923	10.649331
9.306462	897.345573	10.654349
9.680518	904.752156	10.659367
9.557890	913.577013	10.664384
9.313285	917.447474	10.669402
9.520252	919.588471	10.674419
9.260536	914.565483	10.679437
9.250383	910.956916	10.684455
9.192464	907.247206	10.689472
9.361417	918.667727	10.694490
9.615553	908.783463	10.699507
9.537627	913.769690	10.704525
9.582606	925.804501	10.709543
9.602719	912.257559	10.714560
9.598543	915.487011	10.719578
9.607942	925.802402	10.724595
9.479612	932.141227	10.729613
9.480833	921.471722	10.734631
9.941516	939.079029	10.739648
9.752709	937.238272	10.744666
9.953759	931.815370	10.749683
9.661020	922.152156	10.754701
9.436793	922.483426	10.759719
9.602793	921.214247	10.764736
9.732457	945.119902	10.769754
9.989362	944.391512	10.774771
9.796133	933.355577	10.779789
9.789167	924.600686	10.784807
9.810757	931.385130	10.789824
9.373682	933.796705	10.794842
9.775722	924.551264	10.799859
9.776403	949.347779	10.804877
9.807980	948.628677	10.809895
9.784472	940.779313	10.814912
9.714182	957.719788	10.819930
9.935995	950.717331	10.824947
9.925142	968.195344	10.829965
9.821760	961.846129	10.834983
9.808426	950.979042	10.840000
9.712412	956.352263	10.845018
9.781880	943.044144	10.850035
9.728495	947.403596	10.855053
9.412292	951.995227	10.860071
10.053593	938.476493	10.865088
9.988178	950.890137	10.870106
10.215077	941.270349	10.875123
10.312024	941.636522	10.880141
10.218555	947.603906	10.885159
10.334249	945.314075	10.890176
10.009157	945.253617	10.895194
10.094827	944.905631	10.900211
10.155309	940.126325	10.905229
10.054713	926.694381	10.910247
10.355478	926.901303	10.915264
9.972912	921.103864	10.920282
10.035491	912.194205	10.925299
10.094023	912.594083	10.930317
9.765761	915.747979	10.935335
9.810560	918.200570	10.940352
9.792330	922.062751	10.945370
9.922753	934.964405	10.950387
10.339632	944.560218	10.955405
10.276580	944.812107	10.960423
10.447712	947.529605	10.965440
10.022799	938.504459	10.970458
10.026510	922.154387	10.975475
10.071210	925.711141	10.980493
9.772540	932.664828	10.985511
10.098233	940.238646	10.990528
10.232942	947.599581	10.995546
10.106028	950.839285	11.000563
10.039899	960.204151	11.005581
9.648749	960.738765	11.010599
10.082635	958.869894	11.015616
10.158856	947.407594	11.020634
10.285795	959.867792	11.025651
10.272628	941.752670	11.030669
9.977197	959.690625	11.035687
10.107332	950.460579	11.040704
10.202350	950.252363	11.045722
10.089228	948.806903	11.050739
10.104148	950.121516	11.055757
9.961517	946.660009	11.060775
10.347929	956.643675	11.065792
9.965663	946.578577	11.070810
9.580318	957.071801	11.075827
10.352477	974.152951	11.080845
10.427334	989.871050	11.085863
10.696757	979.077866	11.090880
10.656170	985.343168	11.095898
10.296060	978.897023	11.100915
10.509145	955.558143	11.105933
10.487437	959.603359	11.110951
10.465455	953.890588	11.115968
10.361261	956.719324	11.120986
10.311949	943.145841	11.126003
10.271933	949.817462	11.131021
10.107167	943.973395	11.136039
10.565827	965.283601	11.141056
10.228455	972.385608	11.146074
10.267153	978.044005	11.151091
10.511069	985.552828	11.156109
10.386854	987.245497	11.161127
10.489686	988.548931	11.166144
10.828384	985.958310	11.171162
10.432396	997.634623	11.176179
10.671931	970.776173	11.181197
10.599426	959.283923	11.186215
10.481433	953.774783	11.191232
10.134272	958.862200	11.196250
10.290340	968.510181	11.201267
10.553418	980.679439	11.206285
10.472121	987.277596	11.211303
10.449936	972.018778	11.216320
10.395916	993.869379	11.221338
10.392150	990.437858	11.226355
10.603115	987.794340	11.231373
10.789412	994.555924	11.236391
10.475597	993.301080	11.241408
10.438633	990.580442	11.246426
10.399093	994.307013	11.251443
10.720850	988.455746	11.256461
10.619567	991.322583	11.261479
10.698196	985.749644	11.266496
10.680290	991.663030	11.271514
10.443384	979.096144	11.276531
10.562205	985.418948	11.281549
10.359475	981.467446	11.286567
10.573757	991.917106	11.291584
10.522738	987.923212	11.296602
10.597972	994.487043	11.301619
10.452739	1000.053619	11.306637
10.486213	1001.546243	11.311655
10.876919	1013.610591	11.316672
11.021485	1019.070632	11.321690
10.653015	1016.072542	11.326707
10.962085	1009.100710	11.331725
10.703044	1017.992060	11.336743
10.862826	1009.298528	11.341760
10.713544	1011.143939	11.346778
10.879082	1010.259807	11.351795
10.921969	1010.523319	11.356813
10.805763	1002.306037	11.361831
11.025250	1009.638821	11.366848
10.700686	1004.326568	11.371866
10.314682	1011.048306	11.376883
10.755180	1010.926676	11.381901
10.526128	1004.260470	11.386919
10.807854	1010.745900	11.391936
10.929915	1013.750017	11.396954
10.816551	1002.180249	11.401971
10.924951	1004.902416	11.406989
10.781709	1015.397396	11.412007
10.742844	1024.140376	11.417024
10.707823	1009.893518	11.422042
10.663375	1010.882961	11.427059
10.751820	1002.834190	11.432077
10.832982	1021.078033	11.437095
10.959234	1046.022036	11.442112
11.200329	1040.006943	11.447130
11.109090	1041.006089	11.452147
11.248459	1028.594073	11.457165
10.813425	1022.502757	11.462183
10.973407	1023.997505	11.467200
11.008426	1029.825202	11.472218
10.602703	1038.131256	11.477235
10.874556	1044.318773	11.482253
10.888130	1054.030704	11.487271
11.060467	1049.519645	11.492288
11.133655	1042.337016	11.497306
10.964476	1058.116767	11.502323
11.366389	1050.341118	11.507341
11.015737	1047.046226	11.512359
11.011007	1044.120284	11.517376
11.265543	1046.984031	11.522394
11.070850	1039.119606	11.527411
11.391732	1041.588984	11.532429
11.087276	1049.040451	11.537447
11.317202	1040.875381	11.542464
11.292851	1049.241823	11.547482
11.016558	1055.663605	11.552499
11.149237	1051.162642	11.557517
11.527727	1054.717408	11.562535
11.457652	1043.676393	11.567552
11.430782	1047.912219	11.572570
11.259230	1046.943654	11.577587
11.594923	1033.650311	11.582605
11.667864	1047.820412	11.587623
11.349787	1044.120989	11.592640
11.412443	1028.737875	11.597658
11.258481	1029.407677	11.602675
11.447518	1014.217044	11.607693
11.439906	1018.837609	11.612711
11.180073	1011.127837	11.617728
11.363674	1019.748829	11.622746
11.242305	1034.293491	11.627763
11.742121	1040.298084	11.632781
11.221412	1025.740196	11.637799
10.957865	1033.193948	11.642816
11.322912	1033.594351	11.647834
11.560401	1040.988337	11.652851
11.289611	1050.515404	11.657869
11.330022	1040.227271	11.662887
11.692776	1038.062912	11.667904
11.552368	1046.488879	11.672922
11.097804	1045.511580	11.677939
11.451323	1039.856588	11.682957
11.402394	1046.046337	11.687975
11.276485	1032.502753	11.692992
11.371740	1032.573587	11.698010
11.340256	1036.808597	11.703027
11.446247	1033.962572	11.708045
11.775464	1041.606516	11.713063
11.457780	1038.582905	11.718080
11.527183	1035.226671	11.723098
11.387026	1030.875508	11.728115
11.732509	1041.846544	11.733133
11.514152	1050.125775	11.738151
11.601637	1047.664438	11.743168
11.807580	1036.739601	11.748186
11.676343	1054.792242	11.753203
11.749692	1038.782057	11.758221
11.395427	1042.549233	11.763239
11.125921	1044.727261	11.768256
11.487041	1036.774137	11.773274
11.435414	1050.865038	11.778291
11.650022	1061.141294	11.783309
11.786599	1066.946712	11.788327
11.711405	1077.012643	11.793344
11.914087	1072.617607	11.798362
11.398772	1078.812798	11.803379
11.632274	1076.355275	11.808397
11.713926	1071.606086	11.813415
11.750311	1076.636457	11.818432
11.723964	1070.862760	11.823450
11.799608	1076.169867	11.828467
11.895959	1083.163642	11.833485
12.081021	1087.028485	11.838503
11.996855	1076.039374	11.843520
12.021957	1074.006189	11.848538
11.899970	1067.870996	11.853555
11.699223	1068.858914	11.858573
11.843075	1056.648465	11.863591
11.718393	1076.531057	11.868608
12.195395	1066.243779	11.873626
11.831951	1077.875804	11.878643
11.767766	1066.175242	11.883661
11.895328	1067.520653	11.888679
11.456714	1078.931279	11.893696
11.531646	1066.879827	11.898714
11.695481	1073.981128	11.903731
11.762150	1074.450914	11.908749
11.931783	1082.619990	11.913767
11.713643	1076.266074	11.918784
11.876092	1076.566710	11.923802
11.876645	1078.034669	11.928819
11.870962	1085.454297	11.933837
11.937795	1083.449445	11.938855
11.490436	1081.725401	11.943872
12.006529	1096.446822	11.948890
12.286362	1099.447125	11.953907
11.968136	1101.375968	11.958925
12.353539	1114.485991	11.963943
12.269445	1099.890522	11.968960
12.351129	1099.226115	11.973978
12.441355	1086.890667	11.978995
12.156774	1082.979038	11.984013
12.465309	1066.015537	11.989031
12.142490	1066.001546	11.994048
12.369608	1066.543424	11.999066
12.255443	1066.039512	12.004083
12.329902	1075.367832	12.009101
12.538477	1069.992646	12.014119
12.483436	1075.587645	12.019136
12.303300	1069.822633	12.024154
12.213776	1077.123062	12.029171
12.322139	1077.042147	12.034189
12.442448	1066.171985	12.039207
12.197597	1074.539845	12.044224
12.172172	1076.588187	12.049242
12.212636	1075.755423	12.054259
12.236720	1069.543342	12.059277
12.300727	1061.966811	12.064295
12.315321	1080.305570	12.069312
12.287847	1067.974826	12.074330
12.348880	1061.089622	12.079347
12.221760	1061.141701	12.084365
12.094485	1057.615239	12.089383
12.092598	1078.037885	12.094400
12.178594	1060.985396	12.099418
12.160844	1083.827414	12.104435
12.141283	1074.446468	12.109453
12.382700	1072.395448	12.114471
12.441321	1094.595826	12.119488
12.474839	1100.156714	12.124506
12.407384	1079.104406	12.129523
12.390757	1103.106517	12.134541
12.586320	1107.591777	12.139559
12.277464	1112.804586	12.144576
12.538702	1105.199180	12.149594
12.641507	1114.175846	12.154611
12.613800	1094.886161	12.159629
12.615359	1097.053846	12.164647
12.410680	1096.687509	12.169664
12.411902	1087.922118	12.174682
12.574240	1112.550275	12.179699
12.633934	1110.555260	12.184717
12.520606	1106.877293	12.189735
12.470388	1109.297198	12.194752
12.711404	1104.357910	12.199770
12.782573	1103.095531	12.204787
12.487017	1104.686429	12.209805
12.615297	1107.487993	12.214823
12.310791	1109.289393	12.219840
12.614371	1103.966202	12.224858
12.247289	1101.083989	12.229875
12.008165	1111.264419	12.234893
12.528232	1113.290918	12.239911
12.713561	1111.984677	12.244928
12.704240	1107.433159	12.249946
12.777745	1108.989837	12.254963
12.453437	1111.865996	12.259981
12.962739	1109.862027	12.264999
12.456613	1108.804281	12.270016
12.824658	1122.786139	12.275034
12.618437	1135.245047	12.280051
12.553022	1137.168923	12.285069
13.047006	1135.168269	12.290087
12.680137	1139.272538	12.295104
12.918729	1139.914870	12.300122
13.052070	1135.047294	12.305139
12.692124	1135.338407	12.310157
12.982628	1143.470024	12.315175
12.820936	1139.004297	12.320192
13.132164	1137.351708	12.325210
13.097507	1133.043310	12.330227
13.222067	1133.215977	12.335245
13.111115	1114.810756	12.340263
12.882343	1104.536556	12.345280
12.822487	1102.805748	12.350298
13.008636	1110.429871	12.355315
12.871528	1127.203648	12.360333
13.030098	1138.150728	12.365351
12.734598	1141.564175	12.370368
12.916425	1138.889429	12.375386
13.220633	1135.476460	12.380403
13.144364	1138.905048	12.385421
13.263208	1125.805901	12.390439
12.964828	1124.044833	12.395456
12.965141	1130.326069	12.400474
13.072425	1131.563042	12.405491
13.141295	1135.055427	12.410509
13.343083	1138.375870	12.415527
13.011955	1139.505202	12.420544
13.281801	1134.435569	12.425562
13.389496	1132.188758	12.430579
13.159267	1139.379615	12.435597
13.220471	1127.786219	12.440615
13.078424	1135.831265	12.445632
12.897353	1131.164838	12.450650
13.076915	1130.650371	12.455667
12.926836	1130.839687	12.460685
13.100307	1131.924406	12.465703
13.249320	1124.292268	12.470720
13.186139	1135.546225	12.475738
13.644360	1126.066021	12.480755
13.519308	1120.757956	12.485773
13.753079	1129.977318	12.490791
13.755862	1129.655819	12.495808
13.589004	1119.664836	12.500826
13.473149	1112.501014	12.505843
13.267565	1096.656923	12.510861
13.494548	1086.915003	12.515879
13.479193	1089.597605	12.520896
13.032905	1092.603350	12.525914
13.236478	1093.218598	12.530931
13.116356	1089.342379	12.535949
13.433916	1095.262759	12.540967
13.369243	1117.677019	12.545984
13.535332	1128.358915	12.551002
13.939798	1116.724941	12.556019
13.585706	1114.500319	12.561037
13.221200	1107.711199	12.566055
13.195294	1107.308038	12.571072
13.273860	1131.713098	12.576090
13.475600	1121.118963	12.581107
13.443752	1129.719526	12.586125
13.757298	1120.107352	12.591143
13.595989	1126.184425	12.596160
13.513200	1131.544303	12.601178
13.685140	1118.737523	12.606195
13.691486	1130.182711	12.611213
13.750895	1123.534522	12.616231
13.239863	1128.636478	12.621248
13.481487	1123.095994	12.626266
13.741064	1123.413253	12.631283
13.700580	1125.070843	12.636301
13.734780	1126.419878	12.641319
13.846582	1128.122764	12.646336
13.764185	1127.484290	12.651354
13.539830	1121.325250	12.656371
13.609363	1125.085591	12.661389
13.600858	1134.873060	12.666407
13.702639	1129.189962	12.671424
13.906842	1127.262585	12.676442
13.885801	1123.303066	12.681459
13.710066	1122.310388	12.686477
13.998955	1123.673822	12.691495
13.690595	1130.674468	12.696512
14.023055	1125.146725	12.701530
14.028452	1126.269649	12.706547
13.948708	1120.339822	12.711565
14.067737	1118.404085	12.716583
13.986212	1118.987128	12.721600
13.836475	1116.430750	12.726618
14.006830	1120.013824	12.731635
13.793082	1124.484458	12.736653
14.043769	1115.385156	12.741671
14.232751	1122.215830	12.746688
13.912634	1126.050600	12.751706
14.152014	1116.918328	12.756723
14.357585	1118.322888	12.761741
14.158223	1113.710858	12.766759
14.174350	1092.853544	12.771776
13.858013	1090.324308	12.776794
13.705463	1087.897710	12.781811
13.746069	1105.925163	12.786829
14.130450	1120.272176	12.791847
14.010247	1119.697027	12.796864
13.841408	1127.964573	12.801882
13.718106	1125.408352	12.806899
13.951796	1122.354230	12.811917
13.690451	1120.107392	12.816935
14.216908	1117.545948	12.821952
13.777330	1127.229675	12.826970
14.134090	1119.850763	12.831987
13.945617	1119.084958	12.837005
14.135765	1119.063351	12.842023
14.191519	1123.674854	12.847040
14.075266	1126.013956	12.852058
14.462733	1128.693571	12.857075
14.124789	1130.293051	12.862093
14.121999	1129.196411	12.867111
14.112059	1137.661292	12.872128
14.109743	1153.330706	12.877146
14.457028	1159.991164	12.882163
14.392339	1159.860314	12.887181
14.286170	1159.319257	12.892199
14.159857	1158.782512	12.897216
14.705756	1168.408121	12.902234
14.296988	1158.109701	12.907251
14.245468	1164.091690	12.912269
14.269409	1164.453597	12.917287
14.298514	1161.442132	12.922304
14.205165	1154.510362	12.927322
14.134512	1149.746363	12.932339
14.191277	1162.043938	12.937357
14.125056	1155.015376	12.942375
14.469756	1151.924796	12.947392
14.238323	1164.116872	12.952410
14.308505	1161.489701	12.957427
14.318979	1163.184537	12.962445
14.328656	1167.039609	12.967463
14.633802	1171.110383	12.972480
14.534139	1179.467101	12.977498
14.593856	1181.253196	12.982515
14.873041	1189.055655	12.987533
14.632315	1166.692101	12.992551
14.749628	1157.502430	12.997568
14.465065	1166.909619	13.002586
14.488173	1148.507003	13.007603
14.581532	1166.394727	13.012621
14.725590	1177.716028	13.017639
14.750932	1162.287183	13.022656
14.397041	1185.503158	13.027674
14.309623	1185.478411	13.032691
14.641088	1183.368801	13.037709
14.616183	1188.123553	13.042727
14.855863	1184.259692	13.047744
14.673620	1186.768543	13.052762
14.581348	1171.210920	13.057779
15.022914	1179.659864	13.062797
14.835371	1187.020434	13.067815
14.551063	1186.186421	13.072832
14.410330	1189.695741	13.077850
14.779801	1183.722360	13.082867
14.955102	1188.078335	13.087885
14.638624	1182.581837	13.092903
14.989577	1172.243676	13.097920
14.920401	1186.538949	13.102938
14.920454	1187.491920	13.107955
15.064091	1185.784553	13.112973
14.971375	1185.202301	13.117991
14.855618	1183.929276	13.123008
14.609917	1188.811447	13.128026
14.864393	1189.867431	13.133043
14.951017	1193.800530	13.138061
14.986339	1191.859721	13.143079
15.231935	1191.112720	13.148096
14.713203	1185.939364	13.153114
15.038468	1193.858995	13.158131
15.367861	1199.022849	13.163149
14.885831	1200.227902	13.168167
15.011751	1198.978117	13.173184
14.988744	1199.904196	13.178202
15.084066	1216.723704	13.183219
15.061971	1232.161855	13.188237
15.120168	1219.085445	13.193255
15.366399	1215.152787	13.198272
15.307450	1219.674825	13.203290
15.153962	1207.224460	13.208307
15.348465	1212.049442	13.213325
15.203801	1211.659998	13.218343
15.306820	1194.565972	13.223360
15.116894	1195.999483	13.228378
15.415414	1196.761619	13.233395
15.381200	1202.587833	13.238413
15.106693	1199.617282	13.243431
15.235236	1189.943525	13.248448
15.563171	1210.669073	13.253466
15.146571	1203.650365	13.258483
15.185686	1203.590930	13.263501
15.274385	1222.499613	13.268519
15.486227	1221.716265	13.273536
15.464918	1222.612345	13.278554
15.665361	1206.677229	13.283571
15.695892	1207.227783	13.288589
15.353827	1194.720809	13.293607
15.565552	1181.399210	13.298624
15.353034	1176.374634	13.303642
15.111450	1187.732903	13.308659
15.753433	1194.830824	13.313677
15.744701	1209.413330	13.318695
15.420029	1199.162983	13.323712
15.300783	1184.102250	13.328730
15.468157	1207.463579	13.333747
15.469424	1208.166979	13.338765
15.259039	1218.983778	13.343783
15.812587	1219.886815	13.348800
15.528190	1221.092275	13.353818
15.365681	1207.368984	13.358835
15.570172	1217.087454	13.363853
15.594062	1206.720653	13.368871
15.574475	1211.682573	13.373888
15.648103	1217.504946	13.378906
15.307663	1216.842191	13.383923
15.742744	1207.781841	13.388941
15.349515	1223.524782	13.393959
15.387903	1214.395750	13.398976
15.457429	1216.260924	13.403994
15.336147	1227.173027	13.409011
15.954424	1227.911651	13.414029
15.713687	1232.581038	13.419047
15.866867	1232.626161	13.424064
15.581681	1234.072859	13.429082
15.591663	1239.691026	13.434099
15.746944	1228.924797	13.439117
15.787552	1230.736886	13.444135
15.940626	1241.114166	13.449152
15.716901	1233.360329	13.454170
15.516669	1228.791905	13.459187
16.041103	1233.756242	13.464205
15.873424	1243.441560	13.469223
15.988559	1224.838239	13.474240
16.258756	1227.190846	13.479258
15.733970	1231.821949	13.484275
16.158380	1229.395838	13.489293
16.070598	1229.920872	13.494311
16.114739	1233.054427	13.499328
15.944199	1234.360544	13.504346
15.962075	1224.522009	13.509363
16.273045	1228.038374	13.514381
15.959235	1246.150933	13.519399
16.150202	1228.997854	13.524416
16.122661	1240.289102	13.529434
16.189663	1239.303147	13.534451
16.326276	1241.881148	13.539469
16.144922	1244.312903	13.544487
16.317389	1235.162096	13.549504
16.296193	1240.973183	13.554522
16.033194	1248.537956	13.559539
16.065801	1232.910625	13.564557
15.912192	1243.529897	13.569575
16.437966	1235.974596	13.574592
16.190723	1229.201865	13.579610
16.213595	1247.714824	13.584627
16.165813	1238.813372	13.589645
16.018772	1241.071175	13.594663
16.340778	1254.886771	13.599680
16.230228	1262.571809	13.604698
16.519522	1272.864601	13.609715
16.605331	1269.767378	13.614733
16.407193	1255.986357	13.619751
16.650863	1253.074240	13.624768
16.343310	1253.440739	13.629786
16.356049	1245.662975	13.634803
16.519006	1253.466370	13.639821
16.309754	1253.026583	13.644839
16.432581	1261.551273	13.649856
16.432593	1273.692985	13.654874
16.271199	1275.762641	13.659891
16.440493	1275.872218	13.664909
16.455641	1271.437457	13.669927
16.423455	1268.151101	13.674944
16.490216	1274.207077	13.679962
16.427698	1276.824288	13.684979
16.677076	1266.217655	13.689997
16.476979	1279.563530	13.695015
16.366553	1279.111741	13.700032
16.840194	1264.082857	13.705050
16.146250	1273.562486	13.710067
16.553422	1269.281809	13.715085
16.924835	1264.189838	13.720103
16.691311	1271.914491	13.725120
16.962531	1270.494845	13.730138
16.679776	1269.209061	13.735155
16.633909	1261.538006	13.740173
16.666752	1273.526284	13.745191
16.517027	1271.902026	13.750208
16.911007	1279.982173	13.755226
16.890366	1293.215936	13.760243
16.969577	1294.394775	13.765261
16.982623	1296.324600	13.770279
17.029113	1279.689954	13.775296
16.936593	1273.723208	13.780314
16.708898	1272.617077	13.785331
16.809463	1277.680012	13.790349
16.681978	1281.141304	13.795367
16.994121	1296.552433	13.800384
17.260234	1293.650967	13.805402
17.061453	1293.557430	13.810419
17.006782	1298.590128	13.815437
16.909367	1296.226226	13.820455
17.274362	1297.362170	13.825472
17.264267	1293.029394	13.830490
17.094814	1283.466822	13.835507
17.046260	1274.463326	13.840525
16.927318	1262.436870	13.845543
16.900068	1282.824810	13.850560
16.893295	1286.173453	13.855578
16.950686	1302.611583	13.860595
17.247655	1298.734684	13.865613
17.074052	1296.732141	13.870631
17.312191	1298.069140	13.875648
17.150154	1300.794914	13.880666
17.085220	1297.853482	13.885683
17.506582	1290.195544	13.890701
17.334833	1297.144954	13.895719
16.963292	1292.101546	13.900736
17.211263	1294.754054	13.905754
17.131883	1295.264121	13.910771
17.248750	1290.886354	13.915789
17.221184	1299.673088	13.920807
17.108087	1299.452416	13.925824
17.348634	1288.241408	13.930842
17.046915	1297.886124	13.935859
17.243852	1296.165410	13.940877
17.157900	1294.870720	13.945895
17.367124	1320.310242	13.950912
17.591203	1313.706206	13.955930
17.625767	1327.856335	13.960947
17.620202	1321.745299	13.965965
17.490119	1313.883243	13.970983
17.694967	1311.621927	13.976000
17.934663	1284.534590	13.981018
17.425817	1299.971959	13.986035
17.510862	1281.186168	13.991053
17.883433	1274.977234	13.996071
17.555535	1279.463824	14.001088
17.782099	1278.313920	14.006106
17.385581	1288.223866	14.011123
17.479585	1273.665130	14.016141
17.572982	1292.451289	14.021159
17.936930	1312.657908	14.026176
17.777467	1308.303558	14.031194
17.487742	1303.907162	14.036211
17.972758	1310.749424	14.041229
17.911164	1301.156617	14.046247
17.788431	1296.144916	14.051264
17.765385	1286.004094	14.056282
17.500817	1292.762767	14.061299
18.029537	1302.051585	14.066317
17.994739	1315.118833	14.071335
17.836227	1306.462577	14.076352
18.030733	1297.301005	14.081370
17.752931	1297.090427	14.086387
17.901623	1307.435410	14.091405
17.868469	1311.655617	14.096423
17.748355	1319.841602	14.101440
17.849155	1327.410656	14.106458
17.747757	1324.406160	14.111475
17.757163	1319.770394	14.116493
17.847562	1311.310567	14.121511
17.891333	1314.688653	14.126528
17.826618	1322.541318	14.131546
18.030542	1316.276785	14.136563
18.042831	1314.585401	14.141581
18.160174	1313.302384	14.146599
17.880572	1315.500619	14.151616
18.194030	1318.750097	14.156634
18.129739	1317.060346	14.161651
17.910446	1321.976181	14.166669
18.099825	1319.947899	14.171687
17.691530	1320.044474	14.176704
18.300635	1323.249427	14.181722
18.166185	1343.620129	14.186739
18.296382	1345.749664	14.191757
18.266618	1339.110607	14.196775
18.074206	1332.543307	14.201792
18.391638	1334.540930	14.206810
18.281049	1338.150012	14.211827
18.310267	1342.279616	14.216845
18.724075	1341.939199	14.221863
18.455300	1345.215615	14.226880
18.562797	1344.229260	14.231898
18.552234	1340.604520	14.236915
18.869270	1332.712656	14.241933
18.813808	1321.141346	14.246951
18.314109	1315.722315	14.251968
18.521394	1315.173541	14.256986
18.335366	1317.371665	14.262003
18.348191	1317.093574	14.267021
18.129327	1305.147367	14.272039
18.178243	1333.155362	14.277056
18.453859	1339.064660	14.282074
18.408314	1346.165063	14.287091
18.587888	1352.316387	14.292109
18.707134	1347.515435	14.297127
18.590797	1346.163369	14.302144
18.761827	1346.823763	14.307162
18.721985	1350.368212	14.312179
18.698313	1339.903880	14.317197
18.462575	1340.489781	14.322215
18.735267	1345.743358	14.327232
19.174889	1340.308248	14.332250
18.895208	1341.988462	14.337267
18.924403	1336.616256	14.342285
19.029524	1342.090409	14.347303
18.581853	1339.538352	14.352320
19.109936	1349.160722	14.357338
18.719324	1339.626591	14.362355
18.540597	1346.021152	14.367373
18.983433	1330.310776	14.372391
18.712561	1336.128911	14.377408
18.905619	1334.566489	14.382426
19.085055	1337.114007	14.387443
19.237098	1336.980013	14.392461
19.137167	1330.478915	14.397479
19.070819	1337.627037	14.402496
19.062717	1320.419166	14.407514
18.971047	1328.421938	14.412531
19.179090	1344.210108	14.417549
18.855414	1336.255837	14.422567
18.469897	1349.203537	14.427584
19.233684	1332.941372	14.432602
19.200656	1330.612684	14.437619
19.001851	1338.180670	14.442637
19.212706	1327.455575	14.447655
19.013333	1331.751870	14.452672
18.982309	1327.976993	14.457690
19.151824	1329.662098	14.462707
19.149801	1330.582356	14.467725
19.334853	1320.170935	14.472743
19.045616	1338.871583	14.477760
19.111308	1340.190436	14.482778
19.084065	1343.083089	14.487795
19.082163	1332.376026	14.492813
19.529997	1359.957372	14.497831
19.257338	1370.389346	14.502848
19.553486	1358.226514	14.507866
19.175422	1363.057591	14.512883
19.062031	1375.996559	14.517901
19.177165	1351.358094	14.522919
19.300245	1369.357859	14.527936
19.216816	1357.880894	14.532954
19.466646	1368.849076	14.537971
19.267064	1371.871972	14.542989
19.514593	1354.219710	14.548007
19.557666	1363.424669	14.553024
19.597859	1364.276740	14.558042
19.573537	1358.929116	14.563059
19.468566	1369.918928	14.568077
19.422546	1372.016178	14.573095
19.505709	1377.063717	14.578112
19.374745	1361.314094	14.583130
19.568112	1359.286526	14.588147
19.383827	1378.232244	14.593165
19.687061	1373.454022	14.598183
19.942604	1397.065009	14.603200
19.974852	1385.478762	14.608218
19.680883	1375.426346	14.613235
19.513263	1371.029238	14.618253
19.904613	1377.700420	14.623271
19.852787	1397.177149	14.628288
20.029716	1394.624215	14.633306
20.218361	1382.584429	14.638323
19.749142	1378.343443	14.643341
19.852259	1370.324531	14.648359
19.976717	1360.169913	14.653376
19.907593	1362.304833	14.658394
19.867759	1366.153966	14.663411
19.647870	1376.420553	14.668429
19.679179	1388.191683	14.673447
19.773922	1381.096857	14.678464
19.895592	1398.373760	14.683482
20.187403	1386.425372	14.688499
19.974367	1395.845090	14.693517
20.279217	1397.837321	14.698535
20.025971	1396.656083	14.703552
20.099630	1401.798495	14.708570
20.346710	1398.178994	14.713587
19.965687	1406.537257	14.718605
20.223522	1398.702183	14.723623
20.081051	1402.613162	14.728640
20.319780	1407.513761	14.733658
20.211532	1393.586874	14.738675
20.121134	1402.839500	14.743693
19.967327	1398.176751	14.748711
19.720276	1399.689200	14.753728
20.133423	1395.270119	14.758746
20.328556	1406.778987	14.763763
19.804403	1422.828963	14.768781
20.562868	1420.043724	14.773799
20.548861	1429.584685	14.778816
20.782738	1418.314064	14.783834
20.894369	1410.429139	14.788851
20.677701	1399.918914	14.793869
20.524197	1382.080761	14.798887
20.421227	1378.910985	14.803904
20.744697	1383.210252	14.808922
20.913286	1386.936968	14.813939
20.593431	1384.314773	14.818957
20.854439	1384.388331	14.823975
20.826841	1387.819167	14.828992
20.414937	1396.871016	14.834010
20.781777	1397.447683	14.839027
20.283946	1387.600774	14.844045
20.372373	1391.984154	14.849063
20.422785	1385.302108	14.854080
20.484997	1380.449949	14.859098
20.627545	1384.848395	14.864115
20.352923	1399.841111	14.869133
20.487420	1412.941284	14.874151
20.703673	1413.114942	14.879168
20.458021	1422.678433	14.884186
20.853882	1418.066756	14.889203
20.702440	1427.940622	14.894221
20.812100	1417.638038	14.899239
20.699455	1425.311693	14.904256
20.926667	1427.000659	14.909274
20.891580	1415.711502	14.914291
20.585199	1418.422179	14.919309
20.802137	1419.147421	14.924327
20.878774	1422.004028	14.929344
20.956394	1419.873745	14.934362
21.163712	1420.233894	14.939379
20.909302	1423.038725	14.944397
21.122709	1426.570865	14.949415
21.103770	1415.610098	14.954432
21.241930	1413.307235	14.959450
21.137531	1415.482043	14.964467
20.882795	1426.409647	14.969485
21.121106	1425.587078	14.974503
20.967500	1427.930627	14.979520
21.052406	1437.649120	14.984538
21.346228	1444.274055	14.989555
21.117725	1451.695449	14.994573
21.223492	1450.787906	14.999591
21.475359	1444.369158	15.004608
21.300619	1455.207983	15.009626
21.493462	1446.346952	15.014643
21.260448	1454.880756	15.019661
21.306941	1440.784180	15.024679
21.178753	1451.027593	15.029696
21.042021	1445.604826	15.034714
21.845822	1435.492994	15.039731
21.476652	1443.688316	15.044749
21.456393	1444.900335	15.049767
21.480117	1438.917071	15.054784
21.737388	1448.788559	15.059802
21.878758	1439.079853	15.064819
21.368432	1450.067032	15.069837
21.625474	1434.853332	15.074855
21.733901	1434.048093	15.079872
21.515615	1447.286503	15.084890
21.792057	1441.145351	15.089907
21.691238	1443.617562	15.094925
21.791763	1445.567197	15.099943
21.897124	1437.963374	15.104960
21.551753	1444.115274	15.109978
21.636965	1433.662803	15.114995
21.569917	1450.134054	15.120013
21.532961	1446.443778	15.125031
21.654513	1441.648911	15.130048
21.465878	1445.883628	15.135066
21.710793	1432.195748	15.140083
21.595399	1439.585061	15.145101
21.257574	1442.251141	15.150119
21.589929	1448.668359	15.155136
21.727721	1465.043777	15.160154
21.750846	1457.743456	15.165171
22.045423	1476.896149	15.170189
21.891016	1483.311744	15.175207
22.283929	1478.723170	15.180224
22.131502	1471.012345	15.185242
22.506470	1467.228603	15.190259
22.209274	1478.906076	15.195277
22.030727	1453.231870	15.200295
21.963806	1459.657208	15.205312
21.901461	1476.315283	15.210330
22.351668	1469.477579	15.215347
22.329518	1474.826178	15.220365
22.102125	1473.567836	15.225383
22.394993	1470.833154	15.230400
22.147053	1466.056430	15.235418
22.268173	1478.765222	15.240435
22.154510	1476.217781	15.245453
22.328880	1470.870941	15.250471
22.475990	1469.313146	15.255488
22.460469	1477.016244	15.260506
22.444586	1460.788901	15.265523
22.151635	1463.492052	15.270541
22.351084	1466.876725	15.275559
22.724173	1461.171108	15.280576
22.354652	1473.393726	15.285594
22.454946	1464.249790	15.290611
22.295253	1467.229896	15.295629
22.193384	1475.424758	15.300647
22.339597	1463.146678	15.305664
22.146361	1473.715381	15.310682
22.597052	1463.603425	15.315699
22.604607	1470.038504	15.320717
22.323327	1468.409787	15.325735
22.569328	1463.568957	15.330752
22.308958	1451.876903	15.335770
22.447960	1460.379939	15.340787
22.438302	1464.920474	15.345805
22.363321	1473.701562	15.350823
22.736915	1475.814906	15.355840
22.814862	1490.675835	15.360858
22.915155	1479.625643	15.365875
22.492885	1488.163381	15.370893
22.712324	1492.414524	15.375911
23.031637	1472.183082	15.380928
22.999960	1489.741693	15.385946
22.891238	1480.661811	15.390963
23.000899	1484.982661	15.395981
22.942856	1484.948334	15.400999
23.127563	1475.065931	15.406016
23.087591	1479.760673	15.411034
23.180419	1472.709029	15.416051
23.496079	1474.863833	15.421069
22.968467	1480.561083	15.426087
23.275257	1485.981099	15.431104
23.112669	1485.717231	15.436122
22.949463	1488.297187	15.441139
23.238824	1472.121739	15.446157
23.302096	1479.018025	15.451175
23.561738	1473.220930	15.456192
23.303151	1478.532823	15.461210
23.456363	1469.640538	15.466227
23.170730	1462.206419	15.471245
23.069155	1465.503846	15.476263
23.423607	1477.231093	15.481280
23.065098	1482.621303	15.486298
23.489282	1473.254372	15.491315
23.269589	1473.043046	15.496333
23.035447	1480.420706	15.501351
23.049329	1475.044290	15.506368
23.353733	1483.761903	15.511386
23.189939	1480.557085	15.516403
23.365774	1480.302835	15.521421
23.262523	1487.411067	15.526439
23.679701	1476.898789	15.531456
23.358298	1483.923203	15.536474
23.365623	1478.946439	15.541491
23.640704	1479.639441	15.546509
23.402455	1477.978813	15.551527
23.536625	1483.632445	15.556544
23.451248	1502.124232	15.561562
23.791761	1513.355056	15.566579
23.644519	1504.144535	15.571597
24.005508	1509.146600	15.576615
24.109157	1503.821276	15.581632
23.889480	1482.923081	15.586650
23.552102	1471.552948	15.591667
23.833101	1479.494608	15.596685
23.732311	1498.132620	15.601703
24.218830	1488.102118	15.606720
23.733303	1492.021784	15.611738
23.993665	1497.851589	15.616755
23.971195	1486.517388	15.621773
23.671656	1495.701296	15.626791
24.054983	1495.787512	15.631808
23.906069	1498.647355	15.636826
23.931405	1503.255731	15.641843
24.224373	1500.692659	15.646861
23.969063	1507.078487	15.651879
24.492813	1499.133681	15.656896
24.293203	1508.229636	15.661914
24.296453	1491.304701	15.666931
24.268615	1471.574466	15.671949
24.107069	1467.186364	15.676967
24.046574	1461.965925	15.681984
24.292438	1477.682244	15.687002
24.313339	1495.687429	15.692019
24.002992	1480.554849	15.697037
24.008876	1500.967914	15.702055
24.186149	1490.906634	15.707072
23.638329	1501.786674	15.712090
23.988599	1509.678128	15.717107
24.108408	1504.346985	15.722125
23.981671	1495.857592	15.727143
24.373771	1508.721209	15.732160
24.588437	1520.525716	15.737178
24.550895	1532.345337	15.742195
24.825458	1531.602785	15.747213
24.571960	1529.201459	15.752231
24.863573	1518.837444	15.757248
24.708521	1501.430652	15.762266
24.683004	1499.482144	15.767283
24.968158	1499.539510	15.772301
24.670884	1494.481204	15.777319
24.766222	1496.345493	15.782336
24.633206	1497.368499	15.787354
24.471874	1493.927278	15.792371
24.556004	1488.613649	15.797389
24.632157	1510.326163	15.802407
24.599586	1503.487132	15.807424
24.657844	1526.882527	15.812442
24.718618	1531.841112	15.817459
24.920394	1525.663649	15.822477
24.729740	1531.680384	15.827495
25.188178	1533.366187	15.832512
25.115793	1529.946279	15.837530
24.765455	1528.673215	15.842547
24.805005	1524.779751	15.847565
24.734344	1528.922170	15.852583
24.874273	1536.024093	15.857600
25.041730	1529.391729	15.862618
24.968470	1521.576271	15.867635
24.822151	1530.675637	15.872653
24.729900	1536.375365	15.877671
24.625609	1534.885876	15.882688
24.909072	1549.903624	15.887706
24.987913	1568.179991	15.892723
25.217281	1562.161516	15.897741
25.252504	1558.784245	15.902759
25.644325	1558.405337	15.907776
26.048271	1562.863972	15.912794
25.650679	1544.806747	15.917811
25.799768	1519.274130	15.922829
25.716300	1515.161854	15.927847
25.606435	1503.679111	15.932864
25.536662	1509.653818	15.937882
25.623694	1513.295039	15.942899
25.675347	1512.364353	15.947917
25.581859	1521.527218	15.952935
25.586515	1519.321588	15.957952
25.469815	1514.695974	15.962970
25.679047	1522.338139	15.967987
25.825388	1517.183489	15.973005
25.601476	1511.280680	15.978023
25.576472	1512.686967	15.983040
25.385935	1512.801881	15.988058
25.296404	1511.520165	15.993075
25.708535	1515.973103	15.998093
25.761118	1508.546253	16.003111
25.508391	1505.292748	16.008128
26.094693	1506.215979	16.013146
25.538691	1511.363083	16.018163
26.063944	1513.545848	16.023181
25.714579	1488.859134	16.028199
25.778159	1504.509356	16.033216
25.720333	1511.138106	16.038234
25.606342	1514.807627	16.043251
26.166490	1531.516025	16.048269
25.968389	1551.038968	16.053287
25.965337	1538.577055	16.058304
26.263623	1541.949349	16.063322
26.125045	1542.178496	16.068339
26.389720	1540.843165	16.073357
26.219310	1543.206041	16.078375
26.197918	1523.563245	16.083392
26.148671	1521.962903	16.088410
26.219333	1524.656561	16.093427
26.085351	1519.194342	16.098445
25.952853	1520.066889	16.103463
26.108479	1543.125788	16.108480
26.421030	1536.010250	16.113498
25.725103	1536.352756	16.118515
25.796243	1545.316602	16.123533
25.715487	1539.320253	16.128551
25.803826	1541.617342	16.133568
26.097874	1555.860217	16.138586
25.964780	1575.757833	16.143603
26.356515	1573.604162	16.148621
26.337016	1583.200056	16.153639
26.361742	1568.387956	16.158656
26.474682	1574.420082	16.163674
26.248992	1577.886647	16.168691
26.463877	1573.468195	16.173709
26.506078	1588.765387	16.178727
26.643043	1602.586485	16.183744
27.227616	1599.140469	16.188762
26.913043	1591.039697	16.193779
26.935262	1572.713286	16.198797
26.590442	1578.333521	16.203815
26.702040	1581.312317	16.208832
26.977502	1571.582156	16.213850
26.508740	1572.341201	16.218867
26.452615	1575.440613	16.223885
26.613919	1592.121297	16.228903
26.621420	1589.420761	16.233920
27.037555	1595.760229	16.238938
26.954276	1601.534276	16.243955
27.246729	1587.677791	16.248973
27.150209	1596.982720	16.253991
26.791834	1592.938093	16.259008
26.910630	1602.497172	16.264026
26.492493	1603.167547	16.269043
26.596337	1596.912746	16.274061
26.813334	1593.746738	16.279079
27.092288	1596.210933	16.284096
27.581373	1595.024318	16.289114
27.540768	1609.259166	16.294131
27.420606	1596.843721	16.299149
27.392171	1593.592695	16.304167
27.531242	1596.910809	16.309184
27.955902	1586.522992	16.314202
27.601338	1600.862266	16.319219
27.775124	1597.361117	16.324237
27.440903	1598.681519	16.329255
27.478657	1595.921461	16.334272
27.309534	1593.789808	16.339290
27.443706	1604.213168	16.344307
27.526841	1605.176253	16.349325
27.557528	1588.962926	16.354343
27.674892	1594.016301	16.359360
27.740596	1590.552697	16.364378
27.265458	1597.154197	16.369395
27.301875	1599.280764	16.374413
27.268430	1599.488602	16.379431
27.486640	1601.478644	16.384448
27.574244	1602.664978	16.389466
27.626726	1600.478989	16.394483
27.617194	1604.828427	16.399501
27.736386	1609.338068	16.404519
27.579811	1613.943668	16.409536
27.873582	1616.849655	16.414554
27.896482	1621.653721	16.419571
27.875791	1620.976095	16.424589
27.908979	1621.637433	16.429607
27.809934	1615.691906	16.434624
28.015596	1612.535443	16.439642
27.387314	1625.774050	16.444659
27.684643	1617.248761	16.449677
28.130699	1613.863620	16.454695
28.054720	1609.847510	16.459712
28.233327	1600.632094	16.464730
27.912007	1605.293850	16.469747
28.239074	1610.207275	16.474765
28.362808	1594.482245	16.479783
28.102335	1611.861115	16.484800
28.329228	1602.922919	16.489818
27.764830	1611.877470	16.494835
28.308129	1619.792195	16.499853
28.771362	1625.353710	16.504871
28.668636	1637.065694	16.509888
28.406983	1613.949133	16.514906
28.280003	1623.625208	16.519923
28.407442	1623.906251	16.524941
28.461615	1634.417055	16.529959
28.508218	1647.815187	16.534976
28.609750	1644.431663	16.539994
28.517973	1638.282785	16.545011
28.720236	1641.548739	16.550029
28.672505	1632.244934	16.555047
28.770400	1633.736029	16.560064
28.739546	1632.560339	16.565082
28.790622	1630.597386	16.570099
28.771713	1636.438949	16.575117
28.705918	1620.170479	16.580135
28.524777	1624.483919	16.585152
28.647413	1622.185756	16.590170
28.979872	1633.556368	16.595187
28.993157	1638.940698	16.600205
29.308228	1624.519291	16.605223
28.783961	1634.339951	16.610240
29.235251	1622.074512	16.615258
29.071463	1601.365911	16.620275
28.777110	1598.545786	16.625293
29.066169	1610.184348	16.630311
29.048760	1633.779788	16.635328
29.333381	1606.999974	16.640346
29.114929	1624.925193	16.645363
29.061164	1637.799613	16.650381
29.198423	1621.611156	16.655399
28.852034	1633.734027	16.660416
29.252996	1616.339345	16.665434
29.081008	1634.758804	16.670451
29.061189	1634.984270	16.675469
29.301800	1628.471255	16.680487
28.785277	1634.504679	16.685504
29.088453	1623.164787	16.690522
29.080483	1637.227359	16.695539
29.204535	1630.560594	16.700557
29.573304	1632.377550	16.705575
29.355051	1664.624670	16.710592
29.546829	1664.067819	16.715610
29.639492	1658.863731	16.720627
29.636929	1666.005598	16.725645
29.839119	1660.800534	16.730663
29.762453	1653.056627	16.735680
29.808326	1651.346863	16.740698
30.140097	1639.600707	16.745715
29.599927	1620.422209	16.750733
29.586090	1616.035047	16.755751
29.471214	1624.220131	16.760768
29.957751	1640.574125	16.765786
30.326560	1639.790013	16.770803
30.159561	1636.661273	16.775821
30.229348	1614.933269	16.780839
29.646365	1622.789654	16.785856
29.616392	1614.557598	16.790874
30.021885	1608.102570	16.795891
29.853294	1611.202073	16.800909
30.227993	1618.024126	16.805927
30.141569	1628.242647	16.810944
30.273199	1623.447830	16.815962
30.175765	1623.960498	16.820979
30.060340	1612.631329	16.825997
30.221215	1623.927938	16.831015
30.199357	1619.929651	16.836032
30.292168	1645.338365	16.841050
30.334541	1638.123547	16.846067
30.364842	1659.055558	16.851085
30.578286	1643.794927	16.856103
30.464875	1626.551170	16.861120
30.327532	1616.637849	16.866138
30.300653	1617.705718	16.871155
30.211146	1638.636439	16.876173
30.552899	1635.610614	16.881191
30.481323	1645.904046	16.886208
30.397193	1646.289334	16.891226
30.356067	1640.965449	16.896243
30.179083	1648.515022	16.901261
30.449219	1635.736265	16.906279
30.502437	1639.430146	16.911296
30.349248	1647.168676	16.916314
30.534175	1643.005519	16.921331
30.246190	1636.573552	16.926349
30.952067	1660.130996	16.931367
30.568255	1655.510901	16.936384
30.410445	1663.256698	16.941402
30.662615	1670.387374	16.946419
30.434047	1672.163691	16.951437
30.956700	1680.217867	16.956455
31.092238	1678.086048	16.961472
31.195772	1675.802646	16.966490
31.344858	1669.356504	16.971507
31.166858	1677.172368	16.976525
31.255411	1661.345813	16.981543
31.194764	1665.253375	16.986560
30.866892	1664.891437	16.991578
31.395186	1672.346913	16.996595
30.937555	1664.169360	17.001613
31.367836	1662.763548	17.006631
31.439716	1673.471626	17.011648
31.192715	1664.389685	17.016666
31.398229	1672.907435	17.021683
31.213437	1674.799535	17.026701
31.240679	1659.038619	17.031719
31.242895	1668.478241	17.036736
31.388334	1667.239169	17.041754
31.497212	1663.536748	17.046771
31.198992	1672.608549	17.051789
31.448699	1651.365268	17.056807
31.442846	1663.491921	17.061824
31.230555	1662.859929	17.066842
31.323026	1661.443806	17.071859
31.153696	1678.376048	17.076877
31.349816	1687.139424	17.081895
31.502584	1692.600908	17.086912
31.770750	1690.440085	17.091930
31.703517	1686.840965	17.096947
31.503521	1699.370944	17.101965
31.699103	1680.336309	17.106983
32.020733	1694.135437	17.112000
31.734800	1689.358819	17.117018
31.946061	1689.806109	17.122035
31.815308	1683.258780	17.127053
31.938450	1687.828021	17.132071
31.802894	1711.766098	17.137088
31.922103	1718.480236	17.142106
32.392843	1717.133671	17.147123
32.668088	1724.279060	17.152141
32.545285	1700.598344	17.157159
32.667810	1681.942666	17.162176
32.449005	1684.500153	17.167194
32.487955	1685.652806	17.172211
32.190223	1684.763705	17.177229
32.395750	1679.275046	17.182247
32.334951	1676.736157	17.187264
32.410839	1677.239671	17.192282
32.406388	1681.519992	17.197299
32.363979	1670.828637	17.202317
32.482876	1678.650749	17.207335
32.762397	1682.495804	17.212352
32.380027	1685.540305	17.217370
32.638133	1673.826175	17.222387
32.626655	1678.899492	17.227405
32.597216	1676.850440	17.232423
32.295901	1670.897770	17.237440
32.425225	1666.737299	17.242458
32.438177	1671.672931	17.247475
32.268186	1678.797594	17.252493
32.233519	1693.252379	17.257511
32.801169	1696.404034	17.262528
32.940001	1705.179446	17.267546
33.118526	1685.922255	17.272563
32.953054	1697.325006	17.277581
32.996345	1691.581296	17.282599
33.140982	1700.780893	17.287616
33.315826	1696.003712	17.292634
33.344527	1703.147909	17.297651
32.880659	1711.723545	17.302669
33.142928	1704.195226	17.307687
33.400884	1693.981914	17.312704
33.185567	1701.427427	17.317722
33.133367	1697.621513	17.322739
33.554030	1698.716010	17.327757
33.054058	1691.733686	17.332775
33.251805	1676.417158	17.337792
32.993978	1699.630234	17.342810
33.149013	1694.664814	17.347827
32.923093	1710.228061	17.352845
33.039889	1696.119438	17.357863
33.081383	1695.005598	17.362880
33.366777	1707.122342	17.367898
33.469771	1701.209135	17.372915
33.348677	1701.325171	17.377933
33.430735	1713.145638	17.382951
33.602735	1725.076827	17.387968
33.357797	1730.667818	17.392986
33.834923	1733.958245	17.398003
33.471787	1745.370469	17.403021
33.672177	1734.315954	17.408039
33.996730	1727.478038	17.413056
33.722168	1736.305640	17.418074
33.998731	1732.236556	17.423091
33.606669	1723.574372	17.428109
33.822463	1735.596352	17.433127
34.055054	1725.349027	17.438144
33.585146	1738.941240	17.443162
34.239327	1726.078673	17.448179
34.186297	1727.980498	17.453197
34.112184	1728.128531	17.458215
34.090056	1717.862877	17.463232
33.946065	1732.323954	17.468250
33.882470	1727.026190	17.473267
34.021669	1729.842008	17.478285
33.922510	1732.647614	17.483303
33.936302	1739.808069	17.488320
33.761128	1761.458938	17.493338
34.379909	1758.679010	17.498355
34.441829	1765.086136	17.503373
34.177279	1765.419558	17.508391
34.320826	1752.110112	17.513408
34.080959	1763.368531	17.518426
34.303666	1760.784550	17.523443
34.365381	1761.780905	17.528461
34.445985	1768.173529	17.533479
34.756567	1779.327614	17.538496
34.801913	1788.274212	17.543514
34.679508	1773.207913	17.548531
34.683442	1753.974764	17.553549
34.497749	1771.533363	17.558567
34.762832	1776.276790	17.563584
35.031082	1788.304316	17.568602
35.176264	1790.004122	17.573619
35.221173	1769.411382	17.578637
35.220808	1750.014990	17.583655
35.322607	1745.596676	17.588672
35.365656	1750.076426	17.593690
35.723488	1735.422088	17.598707
35.644703	1731.837463	17.603725
35.343782	1732.593185	17.608743
35.576822	1707.043628	17.613760
35.237457	1699.919024	17.618778
35.265457	1698.269289	17.623795
35.392795	1691.079574	17.628813
35.217137	1694.069251	17.633831
35.466279	1692.764424	17.638848
35.424034	1703.123905	17.643866
35.049380	1703.686716	17.648883
35.066187	1697.377564	17.653901
35.106691	1689.817993	17.658919
35.309887	1708.849282	17.663936
35.311922	1728.101215	17.668954
35.411242	1728.075133	17.673971
35.496311	1722.935066	17.678989
35.634346	1727.515636	17.684007
35.840144	1716.536805	17.689024
35.455409	1726.650374	17.694042
35.596270	1724.406265	17.699059
35.805340	1728.181290	17.704077
35.571017	1725.632882	17.709095
35.858410	1728.686189	17.714112
35.622072	1725.374226	17.719130
35.280212	1734.747926	17.724147
35.742963	1729.942841	17.729165
35.540145	1734.660044	17.734183
35.999549	1734.608706	17.739200
36.156437	1752.591129	17.744218
36.067768	1748.721552	17.749235
36.451033	1743.223970	17.754253
36.046024	1756.393513	17.759271
36.416548	1743.494351	17.764288
35.976989	1730.168892	17.769306
35.955294	1737.686154	17.774323
36.145558	1738.799045	17.779341
36.044558	1752.341527	17.784359
36.333988	1748.176229	17.789376
36.153129	1754.593552	17.794394
35.981838	1753.506604	17.799411
36.625056	1752.501571	17.804429
36.377152	1751.451493	17.809447
36.341822	1759.281220	17.814464
35.913845	1752.252132	17.819482
36.173469	1762.091154	17.824499
36.411946	1774.721946	17.829517
36.747431	1792.976642	17.834535
37.076653	1783.205972	17.839552
36.923277	1780.409166	17.844570
37.027435	1785.452780	17.849587
37.228752	1769.501979	17.854605
37.121903	1768.060719	17.859623
36.959173	1742.557805	17.864640
37.010079	1748.804165	17.869658
36.980158	1751.935105	17.874675
37.119933	1740.210167	17.879693
36.775261	1744.620144	17.884711
37.385504	1743.983511	17.889728
37.239999	1752.151286	17.894746
36.643840	1747.822916	17.899763
36.931924	1743.791881	17.904781
37.050942	1768.604803	17.909799
37.209142	1770.612658	17.914816
36.995714	1780.911513	17.919834
36.693307	1776.919196	17.924851
36.786854	1772.606556	17.929869
36.639367	1781.233087	17.934887
37.432933	1777.841661	17.939904
37.237897	1798.742012	17.944922
37.127725	1805.514564	17.949939
37.071428	1806.325328	17.954957
37.037598	1825.870680	17.959975
36.894097	1805.568052	17.964992
37.223880	1817.202797	17.970010
37.190557	1837.570628	17.975027
37.361113	1848.834507	17.980045
37.523789	1851.372678	17.985063
37.835771	1834.980340	17.990080
37.859059	1839.833814	17.995098
38.074738	1836.144213	18.000115
38.187347	1826.476232	18.005133
37.679463	1832.096736	18.010151
38.079066	1840.955104	18.015168
38.281867	1832.614197	18.020186
38.485225	1827.881077	18.025203
38.503600	1824.283525	18.030221
38.113710	1844.423310	18.035239
38.570771	1826.949640	18.040256
38.064543	1810.029616	18.045274
38.046137	1809.703535	18.050291
38.112291	1824.321683	18.055309
38.328889	1824.961579	18.060327
38.296010	1825.898577	18.065344
38.422305	1832.057128	18.070362
38.188221	1844.081692	18.075379
38.522419	1828.684007	18.080397
38.529186	1832.501149	18.085415
38.418690	1838.173691	18.090432
38.475061	1822.470386	18.095450
38.272342	1834.344303	18.100467
38.667482	1828.665024	18.105485
38.609400	1832.498393	18.110503
38.614225	1830.990647	18.115520
38.464351	1832.105426	18.120538
38.371476	1832.062683	18.125555
38.564939	1847.725843	18.130573
38.461279	1859.256083	18.135591
38.692337	1860.241978	18.140608
38.785054	1860.367167	18.145626
38.857567	1868.214361	18.150643
39.140560	1850.918035	18.155661
38.942784	1860.070975	18.160679
38.944599	1858.356265	18.165696
39.212371	1856.810576	18.170714
38.864719	1854.599738	18.175731
38.855873	1859.500060	18.180749
38.621654	1864.735231	18.185767
39.017697	1884.713703	18.190784
39.167650	1887.774006	18.195802
38.902890	1886.187981	18.200819
39.147923	1886.031531	18.205837
39.208429	1887.907333	18.210855
39.267681	1888.821828	18.215872
39.652267	1891.190869	18.220890
39.510228	1892.830878	18.225907
39.539692	1889.601124	18.230925
39.511767	1907.192068	18.235943
39.667873	1908.561377	18.240960
40.145146	1912.612371	18.245978
39.929521	1907.792967	18.250995
40.195350	1893.298156	18.256013
39.966692	1878.023547	18.261031
39.532644	1879.859037	18.266048
39.543983	1879.290662	18.271066
39.554809	1883.315982	18.276083
40.236508	1893.654573	18.281101
39.808181	1909.711459	18.286119
40.075845	1907.379053	18.291136
40.365698	1915.937720	18.296154
39.961436	1913.655134	18.301171
40.352032	1904.057102	18.306189
40.559992	1900.939370	18.311207
40.456894	1906.211150	18.316224
40.364982	1882.451238	18.321242
40.419772	1887.584924	18.326259
40.381561	1865.123705	18.331277
40.445267	1878.049183	18.336295
40.510622	1864.948209	18.341312
40.291891	1870.876615	18.346330
40.289509	1881.560106	18.351347
40.715395	1899.249654	18.356365
40.426335	1901.413316	18.361383
40.568438	1899.518349	18.366400
40.569325	1896.983598	18.371418
40.549693	1902.328386	18.376435
40.606956	1907.211500	18.381453
40.574811	1894.953101	18.386471
40.380221	1909.768536	18.391488
40.741284	1906.449735	18.396506
40.378056	1906.533548	18.401523
40.746768	1920.875043	18.406541
41.227152	1924.030735	18.411559
41.166051	1939.748652	18.416576
41.281205	1927.182648	18.421594
41.128662	1935.198549	18.426611
41.329124	1930.089537	18.431629
41.277279	1942.274004	18.436647
41.507231	1934.450944	18.441664
41.587875	1919.805429	18.446682
41.176078	1914.945022	18.451699
41.435969	1904.681454	18.456717
41.699086	1907.015851	18.461735
41.504548	1906.170701	18.466752
41.159615	1889.659323	18.471770
41.108843	1915.162674	18.476787
41.519860	1927.405275	18.481805
41.535568	1927.531183	18.486823
41.363031	1931.821241	18.491840
41.595808	1927.666044	18.496858
41.344174	1938.298252	18.501875
41.353851	1931.029454	18.506893
41.674154	1935.740580	18.511911
41.470055	1936.982426	18.516928
41.858718	1949.394863	18.521946
41.304153	1946.560395	18.526963
41.586329	1954.673153	18.531981
41.822110	1953.598246	18.536999
42.004650	1954.659875	18.542016
42.223001	1959.329594	18.547034
41.785930	1960.013149	18.552051
41.894162	1956.663682	18.557069
41.840709	1962.063681	18.562087
42.229082	1980.640732	18.567104
42.209655	1986.310483	18.572122
42.225155	1985.480222	18.577139
42.754151	1988.432048	18.582157
42.863207	1978.113050	18.587175
42.984573	1978.390970	18.592192
43.102402	1956.367566	18.597210
42.819871	1937.505313	18.602227
42.858114	1926.060371	18.607245
42.964724	1916.903116	18.612263
43.142268	1929.988548	18.617280
43.235323	1923.881642	18.622298
42.953761	1931.529728	18.627315
43.111549	1918.272898	18.632333
42.804586	1897.003759	18.637351
42.710439	1904.926145	18.642368
43.105313	1899.030371	18.647386
42.845016	1916.744362	18.652403
42.837311	1919.278420	18.657421
42.783353	1913.044843	18.662439
42.915514	1928.761321	18.667456
43.075510	1922.333544	18.672474
43.001463	1926.825216	18.677491
43.197994	1926.402990	18.682509
43.200632	1922.486788	18.687527
43.316372	1930.971490	18.692544
43.187875	1920.356780	18.697562
43.057482	1922.152922	18.702579
42.941504	1918.957824	18.707597
42.974407	1928.003795	18.712615
42.889328	1944.124456	18.717632
42.786119	1953.058695	18.722650
43.178576	1948.281890	18.727667
43.340593	1967.089028	18.732685
43.914750	1973.475565	18.737703
43.667928	1990.164681	18.742720
44.079688	1981.580523	18.747738
43.898577	1977.555708	18.752755
43.784679	1983.926238	18.757773
43.846011	1993.137413	18.762791
44.088138	1985.313497	18.767808
44.036710	1978.425603	18.772826
43.693976	1987.188046	18.777843
44.034147	1979.926220	18.782861
44.343035	1975.869052	18.787879
43.875333	1987.346170	18.792896
44.367070	1973.950849	18.797914
44.272755	1981.171796	18.802931
44.062022	1979.743549	18.807949
44.245165	1980.213801	18.812967
43.924332	1985.997918	18.817984
44.496852	1981.831640	18.823002
44.140503	1988.967164	18.828019
44.070080	1989.875144	18.833037
44.570393	2007.044497	18.838055
44.336508	2013.350819	18.843072
44.768013	2008.871451	18.848090
44.523217	2006.592417	18.853107
44.604931	2015.126681	18.858125
44.906465	2005.046108	18.863143
44.700514	2007.497990	18.868160
44.765730	2018.138124	18.873178
45.008584	2018.434746	18.878195
44.355586	2004.481981	18.883213
44.944483	2004.120888	18.888231
44.545173	2012.439982	18.893248
44.844061	2015.905974	18.898266
45.265660	2025.484170	18.903283
45.268424	2024.238137	18.908301
45.181676	2029.213191	18.913319
45.272602	2026.334635	18.918336
45.358638	2030.230056	18.923354
45.372664	2020.821529	18.928371
45.338103	2021.124823	18.933389
45.734690	2014.552017	18.938407
45.550313	2018.970421	18.943424
45.501385	2019.739430	18.948442
45.829229	2017.806867	18.953459
45.788057	2022.085280	18.958477
45.848042	2019.666912	18.963495
45.914430	2026.624931	18.968512
45.729713	2020.747926	18.973530
45.805279	2006.168713	18.978547
45.306349	2024.575937	18.983565
45.885279	2027.237854	18.988583
45.735225	2024.164890	18.993600
45.941810	2021.868739	18.998618
45.803658	2027.150093	19.003635
45.479863	2038.053324	19.008653
46.088088	2028.123808	19.013671
45.962803	2026.310803	19.018688
45.856410	2025.123159	19.023706
45.976711	2041.325523	19.028723
45.973215	2057.513522	19.033741
46.418834	2052.004347	19.038759
46.461635	2061.315861	19.043776
46.389729	2046.029158	19.048794
46.754806	2053.180722	19.053811
46.538469	2057.694370	19.058829
46.527583	2048.515906	19.063847
46.505972	2049.863025	19.068864
46.492723	2054.120299	19.073882
46.700411	2051.426952	19.078899
46.692952	2050.409554	19.083917
47.000230	2053.568685	19.088935
46.696955	2061.355646	19.093952
46.377931	2046.586702	19.098970
47.054432	2048.627832	19.103987
46.670333	2055.514059	19.109005
46.827579	2042.129862	19.114023
46.772386	2046.668252	19.119040
47.004214	2056.997444	19.124058
47.405807	2049.522305	19.129075
46.956491	2067.467094	19.134093
47.436402	2062.465783	19.139111
47.223212	2072.701019	19.144128
46.980977	2062.720697	19.149146
47.236740	2062.222544	19.154163
47.052817	2075.170801	19.159181
47.562319	2071.755198	19.164199
47.021567	2066.085618	19.169216
47.247276	2066.293153	19.174234
47.507430	2071.859458	19.179251
47.565035	2098.485254	19.184269
47.876824	2097.038164	19.189287
48.251861	2090.375982	19.194304
48.041416	2091.682662	19.199322
48.080495	2091.054188	19.204339
48.063425	2097.921512	19.209357
48.177627	2063.276090	19.214375
48.207855	2067.156140	19.219392
48.032344	2054.322148	19.224410
48.269184	2052.292622	19.229427
47.844700	2065.039504	19.234445
48.002552	2057.734547	19.239463
48.082834	2077.980783	19.244480
48.037618	2094.744167	19.249498
48.133565	2090.936902	19.254515
48.024722	2091.870723	19.259533
47.911678	2095.353036	19.264551
48.139843	2085.481170	19.269568
47.890589	2094.717551	19.274586
48.301459	2114.205727	19.279603
48.346833	2124.706314	19.284621
48.546983	2108.636666	19.289639
48.600487	2113.497044	19.294656
48.482823	2111.261153	19.299674
48.860138	2107.827626	19.304691
48.432212	2125.787253	19.309709
48.805779	2113.407706	19.314727
48.777077	2119.139860	19.319744
48.793362	2130.791808	19.324762
49.215316	2134.124509	19.329779
49.021313	2148.671201	19.334797
49.330272	2147.065140	19.339815
49.243985	2136.712573	19.344832
49.553362	2127.797056	19.349850
49.571469	2122.700006	19.354867
49.306756	2119.427288	19.359885
49.362058	2104.394088	19.364903
49.636037	2098.875271	19.369920
49.315908	2100.079025	19.374938
49.635898	2104.651291	19.379955
49.228205	2105.941752	19.384973
49.411764	2123.915479	19.389991
49.503046	2125.905111	19.395008
49.421542	2130.881495	19.400026
49.919805	2136.874971	19.405043
49.595761	2128.111561	19.410061
49.650266	2122.553419	19.415079
49.949386	2131.722431	19.420096
49.783579	2129.618695	19.425114
50.315505	2130.076982	19.430131
49.759442	2130.421576	19.435149
49.932298	2130.910264	19.440167
49.981030	2136.323356	19.445184
49.869568	2153.304622	19.450202
50.189814	2156.856282	19.455219
50.071390	2157.678117	19.460237
50.277463	2157.436970	19.465255
50.450985	2154.055020	19.470272
50.158512	2156.594839	19.475290
50.635238	2144.351357	19.480307
50.383248	2159.634546	19.485325
50.136505	2148.210551	19.490343
50.512040	2151.930027	19.495360
50.385671	2176.236171	19.500378
50.695188	2182.054573	19.505395
50.337352	2187.606317	19.510413
50.938200	2183.795314	19.515431
51.118596	2180.809039	19.520448
51.254178	2183.722774	19.525466
51.265903	2168.899057	19.530483
50.969412	2187.063000	19.535501
51.051940	2173.066681	19.540519
51.032155	2180.868071	19.545536
50.666647	2188.187271	19.550554
51.073658	2183.007827	19.555571
50.788885	2178.330856	19.560589
51.576266	2196.497579	19.565607
51.481218	2189.879572	19.570624
51.506223	2198.812449	19.575642
51.558246	2193.199579	19.580659
51.226420	2205.124639	19.585677
51.454987	2209.595126	19.590695
51.899452	2194.729400	19.595712
51.570591	2204.068167	19.600730
51.500465	2212.471149	19.605747
51.528143	2218.626073	19.610765
51.795508	2202.784571	19.615783
52.030867	2220.494754	19.620800
51.796177	2214.014173	19.625818
52.051315	2199.847979	19.630835
51.935509	2203.696687	19.635853
52.020065	2204.434200	19.640871
52.209502	2202.058580	19.645888
51.897135	2213.432447	19.650906
52.413088	2221.569310	19.655923
52.298075	2204.183843	19.660941
52.209104	2213.793775	19.665959
52.139409	2225.358633	19.670976
52.259960	2232.923098	19.675994
52.374205	2231.283855	19.681011
52.435547	2226.814219	19.686029
52.478468	2228.632540	19.691047
52.634152	2233.521736	19.696064
52.263134	2230.106338	19.701082
52.527870	2226.199697	19.706099
52.720927	2232.012364	19.711117
52.710081	2258.383825	19.716135
52.981257	2251.714525	19.721152
53.081865	2254.839745	19.726170
53.080438	2257.719053	19.731187
53.090553	2259.961662	19.736205
53.074622	2267.645146	19.741223
53.596684	2249.997476	19.746240
53.755915	2257.780740	19.751258
53.333134	2246.940637	19.756275
53.581132	2238.191289	19.761293
53.193433	2230.476049	19.766311
53.376108	2228.810146	19.771328
53.407712	2252.546256	19.776346
53.743578	2249.293353	19.781363
53.404720	2244.205057	19.786381
53.351083	2244.792390	19.791399
53.717119	2237.797211	19.796416
53.461088	2249.021451	19.801434
53.583445	2250.672527	19.806451
53.854519	2254.653167	19.811469
53.272603	2236.283881	19.816487
53.594246	2269.524062	19.821504
53.701475	2273.746923	19.826522
53.866498	2279.114079	19.831539
54.177876	2281.488391	19.836557
54.066874	2289.819042	19.841575
54.384907	2276.068533	19.846592
54.005085	2285.668506	19.851610
53.997742	2287.972070	19.856627
54.160924	2282.137665	19.861645
54.429028	2290.301939	19.866663
54.239209	2296.274938	19.871680
54.336943	2308.842819	19.876698
54.313530	2304.335399	19.881715
54.436927	2303.456781	19.886733
53.979183	2309.023897	19.891751
54.172751	2318.835219	19.896768
54.986517	2314.219178	19.901786
55.835179	2305.384510	19.906803
55.865809	2306.114208	19.911821
55.834837	2289.211767	19.916839
56.043519	2266.588308	19.921856
55.967807	2273.912018	19.926874
55.726364	2262.710666	19.931891
55.873206	2247.932847	19.936909
55.550569	2240.517258	19.941927
55.534111	2246.138586	19.946944
55.761491	2241.923769	19.951962
55.445062	2242.908633	19.956979
55.844262	2242.905825	19.961997
55.839625	2250.012481	19.967015
55.798178	2241.031456	19.972032
55.543649	2235.031860	19.977050
55.663719	2243.329420	19.982067
55.708391	2230.414413	19.987085
55.727144	2249.139672	19.992103
55.599945	2245.444433	19.997120
55.603643	2242.147806	20.002138
55.694385	2242.418786	20.007155
56.126443	2240.008974	20.012173
55.835864	2235.210906	20.017191
55.900295	2230.514399	20.022208
55.962683	2252.759524	20.027226
56.144826	2253.812973	20.032243
56.060917	2261.154960	20.037261
55.683353	2268.282504	20.042279
56.091584	2266.361625	20.047296
56.001950	2265.209576	20.052314
56.432058	2281.970006	20.057331
56.672125	2286.198279	20.062349
56.619029	2293.595421	20.067367
56.768127	2282.714134	20.072384
56.740047	2288.138004	20.077402
56.717837	2298.976230	20.082419
56.733189	2285.335764	20.087437
56.544597	2291.352650	20.092455
56.947390	2287.498568	20.097472
56.679845	2287.863200	20.102490
57.124638	2289.054928	20.107507
57.148089	2286.035714	20.112525
56.915053	2296.434404	20.117543
57.414704	2311.807105	20.122560
57.045285	2322.486597	20.127578
56.874551	2322.112846	20.132595
57.524436	2324.803050	20.137613
57.323465	2320.004124	20.142631
57.712040	2311.304728	20.147648
57.522439	2320.438480	20.152666
57.212250	2315.462146	20.157683
57.383119	2307.842149	20.162701
57.483491	2326.910878	20.167719
58.066299	2345.702483	20.172736
57.788042	2343.852715	20.177754
57.995832	2347.702903	20.182771
58.185005	2332.065710	20.187789
57.893611	2336.129082	20.192807
58.299925	2333.941800	20.197824
58.395788	2339.173173	20.202842
58.331652	2342.629548	20.207859
58.447649	2337.069238	20.212877
58.304053	2348.676122	20.217895
58.515430	2331.830627	20.222912
58.539371	2344.604024	20.227930
58.569592	2341.820867	20.232947
58.323959	2335.371764	20.237965
58.266172	2331.433556	20.242983
58.593342	2328.652903	20.248000
58.408636	2332.594322	20.253018
58.474924	2346.389581	20.258035
58.308062	2355.408778	20.263053
58.553519	2370.552499	20.268071
58.746841	2360.395292	20.273088
58.814903	2359.737020	20.278106
58.679188	2367.033291	20.283123
58.968123	2380.531573	20.288141
58.887130	2400.307083	20.293159
59.105922	2400.526397	20.298176
59.093472	2403.254217	20.303194
59.116454	2391.407348	20.308211
59.448973	2398.013115	20.313229
59.679459	2394.188858	20.318247
59.520145	2393.360495	20.323264
59.506811	2394.883626	20.328282
59.283391	2396.112165	20.333299
59.809960	2383.747866	20.338317
59.647929	2404.842584	20.343335
59.329398	2415.995586	20.348352
59.762332	2411.636922	20.353370
59.776290	2418.868330	20.358387
60.237577	2419.884128	20.363405
59.912869	2413.049662	20.368423
60.300700	2417.569477	20.373440
60.800714	2414.601204	20.378458
60.491610	2413.376165	20.383475
60.618335	2405.237272	20.388493
60.569332	2423.601328	20.393511
60.834314	2410.120669	20.398528
60.797760	2413.755953	20.403546
60.860432	2417.133520	20.408563
60.936390	2404.830871	20.413581
60.577833	2400.949038	20.418599
61.013436	2403.362286	20.423616
61.094912	2383.970667	20.428634
60.658042	2388.089781	20.433651
61.001207	2393.196455	20.438669
61.173068	2399.978564	20.443687
61.156993	2411.378216	20.448704
61.097241	2407.554281	20.453722
60.669094	2420.396541	20.458739
60.892980	2412.900794	20.463757
61.332087	2415.094780	20.468775
61.272090	2420.862923	20.473792
61.037306	2401.784941	20.478810
60.653881	2413.323441	20.483827
61.124854	2420.653334	20.488845
60.957970	2441.150323	20.493863
61.505954	2443.089134	20.498880
61.503523	2437.949314	20.503898
61.334062	2438.501663	20.508915
61.741066	2460.719470	20.513933
62.062995	2461.756527	20.518951
61.965430	2468.482604	20.523968
61.911646	2468.015513	20.528986
61.905658	2468.265279	20.534003
62.318353	2466.282029	20.539021
62.382037	2463.674411	20.544039
62.254194	2476.528900	20.549056
62.114537	2466.581164	20.554074
62.239078	2470.657527	20.559091
62.016561	2466.696114	20.564109
62.170553	2471.618931	20.569127
62.361229	2489.326178	20.574144
62.741687	2498.348317	20.579162
62.793121	2497.768176	20.584179
62.519215	2498.533246	20.589197
62.591641	2489.994647	20.594215
62.667431	2503.068445	20.599232
62.981274	2495.372372	20.604250
62.611872	2494.877519	20.609267
63.023605	2494.673245	20.614285
63.169308	2502.935806	20.619303
63.034044	2507.634599	20.624320
63.655816	2509.395882	20.629338
63.483161	2510.013718	20.634355
63.695100	2497.731632	20.639373
63.508387	2482.764629	20.644391
63.499299	2473.084270	20.649408
63.702752	2470.480128	20.654426
63.314544	2480.671330	20.659443
63.701530	2494.433609	20.664461
63.630774	2505.372515	20.669479
63.542609	2515.978893	20.674496
63.678798	2498.590756	20.679514
63.553467	2516.859274	20.684531
63.628781	2511.575095	20.689549
63.585264	2510.816168	20.694567
63.551052	2520.122772	20.699584
64.111699	2530.235753	20.704602
64.326460	2549.291955	20.709619
64.169371	2539.044513	20.714637
64.309312	2543.318731	20.719655
64.124191	2548.516297	20.724672
64.492914	2541.619941	20.729690
64.192935	2545.000379	20.734707
64.540644	2542.279677	20.739725
64.725717	2546.856655	20.744743
64.689207	2561.236184	20.749760
65.008535	2569.402181	20.754778
65.011043	2567.273918	20.759795
65.172750	2569.732846	20.764813
65.223035	2569.938671	20.769831
64.997937	2582.284941	20.774848
65.432090	2559.884607	20.779866
65.040560	2570.650201	20.784883
65.272722	2565.887690	20.789901
65.428885	2568.161325	20.794919
65.192283	2563.912862	20.799936
65.032741	2564.376181	20.804954
65.055960	2566.480457	20.809971
65.128761	2560.871500	20.814989
64.951321	2570.646657	20.820007
65.192186	2598.804750	20.825024
65.438882	2590.463662	20.830042
65.217750	2589.486852	20.835059
65.565559	2620.641701	20.840077
66.022289	2616.186140	20.845095
66.018660	2618.902306	20.850112
66.519688	2612.834794	20.855130
66.463411	2618.370127	20.860147
66.524079	2617.790817	20.865165
66.671315	2599.249430	20.870183
66.725501	2610.399246	20.875200
66.597166	2607.458394	20.880218
66.578826	2617.202173	20.885235
66.621178	2608.123627	20.890253
66.495848	2599.358211	20.895271
66.349314	2610.318768	20.900288
66.543162	2606.373552	20.905306
66.627692	2606.525690	20.910323
66.636512	2602.781906	20.915341
66.991205	2605.387680	20.920359
66.816872	2628.258451	20.925376
67.008228	2631.586850	20.930394
66.977246	2642.360234	20.935411
66.935642	2635.838710	20.940429
67.361225	2636.287227	20.945447
66.856864	2642.793805	20.950464
67.184601	2636.953333	20.955482
67.159921	2650.896763	20.960499
67.618584	2648.606502	20.965517
67.916473	2651.106717	20.970535
67.532315	2653.873564	20.975552
68.000733	2652.385977	20.980570
68.020329	2662.841192	20.985587
67.724718	2663.091578	20.990605
68.288171	2660.070259	20.995623
67.911320	2663.530744	21.000640
67.988083	2655.101568	21.005658
68.031873	2654.974233	21.010675
67.679458	2651.301546	21.015693
68.307084	2653.758691	21.020711
68.089074	2654.085618	21.025728
68.202979	2648.526527	21.030746
68.377896	2674.539870	21.035763
68.393273	2689.162505	21.040781
68.962169	2675.671551	21.045799
68.341913	2684.146798	21.050816
68.478642	2680.256669	21.055834
68.619302	2695.212525	21.060851
68.778938	2684.915799	21.065869
68.821994	2682.722948	21.070887
68.644741	2692.206827	21.075904
68.994657	2698.559273	21.080922
68.961022	2698.723852	21.085939
69.183774	2719.038326	21.090957
69.432601	2696.666845	21.095975
69.347789	2707.275950	21.100992
69.379530	2695.196900	21.106010
69.453702	2710.409808	21.111027
69.293213	2695.447320	21.116045
69.703059	2699.716744	21.121063
69.486863	2699.837871	21.126080
69.778586	2704.372078	21.131098
69.893136	2723.275379	21.136115
70.102116	2731.389227	21.141133
70.153693	2713.104443	21.146151
70.116631	2730.226599	21.151168
70.264306	2710.707102	21.156186
70.307319	2725.750380	21.161203
70.173616	2730.938722	21.166221
70.301448	2729.401508	21.171239
70.452666	2724.865305	21.176256
70.308553	2722.613224	21.181274
70.634164	2728.908678	21.186291
70.542735	2705.977297	21.191309
70.831862	2718.581599	21.196327
70.616990	2733.230118	21.201344
70.466755	2726.579664	21.206362
70.920928	2732.696009	21.211379
70.559050	2752.254814	21.216397
70.812984	2740.273259	21.221415
70.986585	2752.385286	21.226432
70.817895	2752.709971	21.231450
71.015240	2751.105759	21.236467
71.009593	2767.056286	21.241485
71.324526	2770.770575	21.246503
71.236783	2777.869750	21.251520
71.587088	2782.368711	21.256538
71.623975	2784.751848	21.261555
71.855142	2784.691183	21.266573
71.773724	2783.795992	21.271591
71.571390	2780.717736	21.276608
71.815827	2784.717680	21.281626
72.104879	2775.816371	21.286643
72.023871	2777.797354	21.291661
72.090625	2774.678177	21.296679
72.072199	2790.910748	21.301696
72.331512	2803.855070	21.306714
72.380914	2812.081153	21.311731
72.482066	2808.675983	21.316749
72.587009	2797.938633	21.321767
72.634903	2808.131802	21.326784
72.104195	2802.379974	21.331802
72.395029	2800.636298	21.336819
72.358046	2807.144843	21.341837
72.616602	2810.105893	21.346855
72.637964	2806.439511	21.351872
72.818346	2828.950009	21.356890
73.042902	2826.188588	21.361907
73.165875	2828.836628	21.366925
73.455572	2840.584674	21.371943
73.240338	2830.971815	21.376960
73.304759	2826.299932	21.381978
73.645698	2834.820751	21.386995
73.377191	2837.873624	21.392013
73.436260	2821.594868	21.397031
73.471691	2831.273205	21.402048
73.492568	2828.342299	21.407066
73.877069	2823.965542	21.412083
73.512447	2840.677006	21.417101
73.899797	2824.988067	21.422119
73.903588	2830.772987	21.427136
73.939054	2851.210705	21.432154
74.151682	2849.034296	21.437171
73.985058	2853.535629	21.442189
74.096881	2846.048940	21.447207
74.475505	2841.674724	21.452224
74.537645	2849.999505	21.457242
74.222195	2835.454203	21.462259
74.430913	2849.696238	21.467277
74.413209	2843.846632	21.472295
74.613128	2846.935484	21.477312
74.913309	2861.247452	21.482330
74.618663	2872.736977	21.487347
74.735803	2875.319850	21.492365
74.991457	2871.554898	21.497383
75.048891	2870.473772	21.502400
74.956355	2873.066490	21.507418
74.599947	2873.830841	21.512435
75.161990	2887.927916	21.517453
75.467698	2901.498880	21.522471
75.524978	2893.336956	21.527488
75.566102	2898.842514	21.532506
76.029948	2891.278737	21.537523
76.063818	2906.186699	21.542541
76.479255	2900.420217	21.547559
75.951445	2895.030459	21.552576
75.882421	2896.341393	21.557594
76.068991	2904.075980	21.562611
75.837522	2905.064166	21.567629
75.959485	2903.204295	21.572647
75.938596	2903.134101	21.577664
76.058351	2903.983151	21.582682
76.074176	2895.987124	21.587699
76.155816	2900.208086	21.592717
76.064458	2907.056747	21.597735
76.304617	2916.913111	21.602752
76.463340	2931.860306	21.607770
76.438621	2923.920176	21.612787
76.110675	2935.614455	21.617805
76.561323	2950.277218	21.622823
76.775376	2954.850711	21.627840
76.592909	2967.134338	21.632858
76.803420	2950.363903	21.637875
76.857558	2971.131753	21.642893
77.259050	2971.233488	21.647911
77.423030	2975.992814	21.652928
77.517219	2974.239096	21.657946
77.711466	2973.523925	21.662963
77.797327	2977.711928	21.667981
78.243413	2956.997575	21.672999
78.390159	2972.287328	21.678016
77.972997	2946.157167	21.683034
78.193683	2939.093767	21.688051
77.984628	2932.829307	21.693069
78.158915	2933.419749	21.698087
77.820956	2933.251167	21.703104
77.979123	2938.549218	21.708122
78.518362	2946.828678	21.713139
78.514462	2967.764376	21.718157
78.476010	2953.918833	21.723175
78.376946	2960.992011	21.728192
78.237907	2965.669520	21.733210
77.896097	2964.021311	21.738227
78.247679	2963.744693	21.743245
78.604317	2975.206987	21.748263
78.744235	2994.800892	21.753280
78.550987	2991.616371	21.758298
78.767345	2980.616398	21.763315
78.667265	3002.587292	21.768333
78.728065	2997.361643	21.773351
79.127310	3006.600064	21.778368
78.978678	3027.083789	21.783386
79.259084	3021.441935	21.788403
79.519611	3024.931425	21.793421
79.732524	3019.472766	21.798439
80.068949	3013.546076	21.803456
79.803678	3019.312143	21.808474
80.136376	3007.901994	21.813491
80.110578	3010.499454	21.818509
80.063286	3003.685811	21.823527
80.248491	3002.047754	21.828544
80.007632	3009.623109	21.833562
80.251547	3004.256967	21.838579
80.172018	3016.393707	21.843597
80.342089	3024.330287	21.848615
80.308161	3024.300042	21.853632
80.121542	3038.735526	21.858650
80.262211	3028.888936	21.863667
80.253871	3040.652525	21.868685
80.393677	3051.195222	21.873703
80.854149	3067.208402	21.878720
80.488418	3067.132594	21.883738
80.819448	3061.751250	21.888755
81.277969	3068.002047	21.893773
81.321880	3050.843296	21.898791
81.461032	3052.838327	21.903808
81.123363	3051.583507	21.908826
81.491754	3054.787472	21.913843
81.689262	3071.401179	21.918861
81.802438	3065.687733	21.923879
81.920245	3067.268982	21.928896
82.281969	3069.766198	21.933914
82.491670	3056.775989	21.938931
82.023142	3040.084592	21.943949
81.943265	3051.793084	21.948967
82.172033	3045.213719	21.953984
81.977966	3055.029722	21.959002
81.988728	3057.249506	21.964019
82.134359	3073.279679	21.969037
82.246492	3072.645394	21.974055
82.520666	3064.687296	21.979072
82.495554	3067.834637	21.984090
82.127534	3078.536068	21.989107
82.576460	3079.932292	21.994125
82.534790	3097.036718	21.999143
82.640073	3103.601404	22.004160
82.727267	3104.817646	22.009178
83.165773	3096.244993	22.014195
83.155400	3102.183925	22.019213
83.560516	3108.584505	22.024231
83.379445	3092.347900	22.029248
83.003569	3104.135657	22.034266
83.033933	3095.419033	22.039283
83.452480	3107.228273	22.044301
83.450870	3118.016819	22.049319
83.592505	3118.478810	22.054336
83.797831	3121.979018	22.059354
83.701310	3113.745938	22.064371
83.996151	3117.729373	22.069389
83.700833	3112.403480	22.074407
83.832130	3109.766078	22.079424
84.113345	3137.893684	22.084442
84.062715	3139.951975	22.089459
84.503789	3144.030148	22.094477
84.617001	3146.533403	22.099495
84.624559	3139.297260	22.104512
84.192922	3154.791425	22.109530
84.461343	3136.791956	22.114547
84.649188	3136.568375	22.119565
84.720604	3142.293025	22.124583
85.613945	3139.777723	22.129600
85.328080	3135.390395	22.134618
85.370081	3126.850173	22.139635
85.399193	3133.069199	22.144653
85.410302	3122.042413	22.149671
85.640648	3115.304101	22.154688
85.622210	3128.056408	22.159706
85.567649	3112.854363	22.164723
85.666643	3130.858788	22.169741
85.612217	3142.167483	22.174759
85.694350	3140.241726	22.179776
85.727901	3149.593809	22.184794
86.006590	3151.658707	22.189811
86.085427	3149.957111	22.194829
85.876738	3163.476694	22.199847
86.082459	3150.163450	22.204864
86.006185	3171.994433	22.209882
86.113486	3179.002509	22.214899
86.224331	3187.639497	22.219917
86.339199	3193.995161	22.224935
86.658489	3198.786766	22.229952
86.573314	3192.761173	22.234970
86.530597	3193.641810	22.239987
86.964301	3200.627850	22.245005
86.898559	3214.451409	22.250023
87.144178	3203.974386	22.255040
87.149196	3202.812137	22.260058
87.323252	3216.170885	22.265075
87.003401	3211.753718	22.270093
87.355065	3200.569818	22.275111
87.440416	3213.805035	22.280128
87.482660	3229.067823	22.285146
87.625247	3232.862671	22.290163
87.546279	3236.512243	22.295181
87.974928	3239.077561	22.300199
88.096309	3227.934449	22.305216
87.983676	3227.573514	22.310234
87.887334	3242.917875	22.315251
87.986557	3235.455127	22.320269
88.177402	3250.408740	22.325287
88.325632	3256.149480	22.330304
88.374834	3268.820648	22.335322
88.523325	3261.763914	22.340339
88.780503	3259.856067	22.345357
88.354980	3251.758773	22.350375
88.765977	3257.856086	22.355392
88.946474	3261.458853	22.360410
89.107398	3279.133537	22.365427
89.032106	3280.392784	22.370445
89.119124	3293.649054	22.375463
89.408288	3292.255596	22.380480
89.357977	3300.187789	22.385498
89.456396	3287.583488	22.390515
89.636197	3283.336884	22.395533
89.275048	3294.733774	22.400551
89.689794	3286.249980	22.405568
89.617010	3276.394017	22.410586
89.318976	3280.574672	22.415603
89.665972	3293.962391	22.420621
90.006330	3311.367307	22.425639
90.228894	3302.117634	22.430656
89.793667	3304.583587	22.435674
90.181078	3301.580215	22.440691
90.289283	3301.182393	22.445709
90.293659	3308.625640	22.450727
90.888997	3312.113021	22.455744
90.830998	3323.107088	22.460762
90.604726	3319.687406	22.465779
91.248360	3326.328977	22.470797
91.179346	3327.297430	22.475815
91.114303	3325.430615	22.480832
91.245205	3320.537364	22.485850
91.243210	3329.047015	22.490867
91.193021	3331.389113	22.495885
91.034782	3330.474300	22.500903
91.405983	3329.455862	22.505920
91.547801	3333.150470	22.510938
91.447020	3359.987285	22.515955
91.826503	3354.691141	22.520973
91.736907	3361.083416	22.525991
91.519588	3365.405873	22.531008
91.623359	3361.231259	22.536026
91.681850	3368.099062	22.541043
92.214094	3391.817187	22.546061
92.240840	3392.718247	22.551079
92.096987	3395.449057	22.556096
92.417277	3400.014183	22.561114
92.251767	3384.671938	22.566131
92.889640	3401.641972	22.571149
92.656359	3412.336721	22.576167
92.546861	3415.490202	22.581184
92.880843	3421.892431	22.586202
92.986856	3417.502078	22.591219
93.123588	3407.595664	22.596237
93.007082	3421.365197	22.601255
92.829837	3436.524694	22.606272
93.127004	3433.827939	22.611290
93.142505	3437.456043	22.616307
93.454761	3438.295361	22.621325
93.717005	3444.625596	22.626343
93.924546	3458.146342	22.631360
94.194916	3464.885870	22.636378
93.973407	3468.555901	22.641395
94.213189	3472.663880	22.646413
94.330170	3457.699687	22.651431
94.122795	3454.264649	22.656448
94.521667	3452.994387	22.661466
94.598858	3449.022960	22.666483
94.690790	3446.886886	22.671501
94.539753	3471.948742	22.676519
94.616795	3472.337559	22.681536
94.917397	3456.808775	22.686554
94.533259	3467.082034	22.691571
95.181389	3472.659936	22.696589
94.989921	3479.469879	22.701607
95.238006	3477.678470	22.706624
95.744771	3474.502588	22.711642
94.842292	3479.809155	22.716659
95.372303	3474.487311	22.721677
95.629074	3484.343655	22.726695
95.658493	3483.102943	22.731712
95.461247	3479.584729	22.736730
95.439796	3491.176812	22.741747
95.575358	3497.674851	22.746765
95.803490	3496.856815	22.751783
95.966208	3508.009029	22.756800
96.143054	3498.390810	22.761818
95.773005	3518.163344	22.766835
96.262643	3534.261167	22.771853
96.168319	3530.957825	22.776871
96.283563	3536.119472	22.781888
96.433938	3539.893818	22.786906
96.472347	3568.605241	22.791923
96.553364	3554.702807	22.796941
96.713616	3575.634641	22.801959
96.776826	3577.264335	22.806976
97.065262	3570.632370	22.811994
97.146523	3584.986301	22.817011
97.425297	3591.405203	22.822029
97.613061	3582.739070	22.827047
97.967380	3591.102585	22.832064
98.013800	3587.639360	22.837082
98.080325	3578.202314	22.842099
98.088048	3573.896269	22.847117
98.120085	3583.638630	22.852135
98.090186	3575.271854	22.857152
98.628566	3571.914350	22.862170
98.587662	3583.400660	22.867187
98.621329	3590.038017	22.872205
98.528027	3587.410088	22.877223
98.424685	3578.685759	22.882240
98.696398	3590.081047	22.887258
98.283782	3595.782695	22.892275
98.565323	3599.603098	22.897293
98.749871	3614.259283	22.902311
98.485920	3610.663084	22.907328
98.827192	3621.623671	22.912346
98.834203	3637.478906	22.917363
99.113544	3643.996950	22.922381
98.934731	3646.256412	22.927399
99.089489	3653.890331	22.932416
99.089567	3665.301425	22.937434
99.401757	3680.570839	22.942451
99.445622	3675.891074	22.947469
99.784987	3689.425279	22.952487
99.645928	3707.463015	22.957504
100.211285	3711.265289	22.962522
99.833453	3718.327000	22.967539
100.255415	3703.084614	22.972557
100.400808	3709.323634	22.977575
100.390310	3725.309807	22.982592
100.597321	3728.197662	22.987610
100.920834	3735.857675	22.992627
100.743172	3736.370084	22.997645
100.757340	3740.109504	23.002663
100.799144	3735.372186	23.007680
100.954318	3721.068368	23.012698
101.341992	3750.466520	23.017715
101.253289	3770.446432	23.022733
101.227951	3774.568772	23.027751
101.377125	3767.447522	23.032768
101.392135	3763.549676	23.037786
101.219095	3765.010156	23.042803
101.528661	3776.310349	23.047821
101.854898	3788.750335	23.052839
101.858155	3784.532373	23.057856
102.085708	3790.965728	23.062874
101.980575	3784.315239	23.067891
102.307985	3788.618276	23.072909
102.640896	3786.495881	23.077927
102.486829	3788.150476	23.082944
102.568392	3803.321502	23.087962
102.535702	3825.897791	23.092979
102.842418	3819.892240	23.097997
103.262843	3817.168361	23.103015
103.081158	3819.954710	23.108032
103.141408	3814.941481	23.113050
103.273236	3809.931780	23.118067
103.403823	3813.801196	23.123085
103.532912	3805.945044	23.128103
103.339975	3812.104181	23.133120
103.667409	3823.054992	23.138138
103.463605	3831.684092	23.143155
103.716482	3835.055344	23.148173
104.313164	3831.811777	23.153191
103.851219	3834.308211	23.158208
104.068091	3828.622627	23.163226
103.808439	3844.582374	23.168243
103.938793	3857.710702	23.173261
104.494828	3858.484172	23.178279
104.470885	3862.081884	23.183296
104.170126	3861.763042	23.188314
104.297810	3873.848101	23.193331
104.636119	3880.728558	23.198349
105.081170	3888.089817	23.203367
104.858706	3881.414578	23.208384
105.155104	3883.734137	23.213402
105.176414	3897.644708	23.218419
105.443857	3909.803948	23.223437
106.023889	3907.941893	23.228455
105.875882	3915.038552	23.233472
105.619999	3902.382452	23.238490
105.675079	3913.791333	23.243507
105.795403	3910.630793	23.248525
106.197258	3900.113707	23.253543
106.008598	3923.960035	23.258560
106.295712	3936.530624	23.263578
106.584088	3928.426824	23.268595
106.844411	3935.473738	23.273613
106.800785	3933.588350	23.278631
106.546338	3943.244805	23.283648
106.805771	3930.329512	23.288666
106.681172	3933.765915	23.293683
106.767418	3936.439113	23.298701
106.981131	3957.491766	23.303719
107.121000	3966.385422	23.308736
107.098159	3960.680343	23.313754
107.228131	3965.803873	23.318771
106.982657	3976.493935	23.323789
107.601933	3985.789504	23.328807
107.702342	3997.856331	23.333824
107.882848	3996.071306	23.338842
107.704194	4003.799861	23.343859
107.567737	4009.299329	23.348877
108.064500	4022.290084	23.353895
107.931711	4027.320039	23.358912
108.442451	4028.995127	23.363930
108.554189	4023.897730	23.368947
108.342369	4031.941238	23.373965
108.826065	4035.790553	23.378983
108.631318	4054.860368	23.384000
108.792899	4048.988952	23.389018
108.912312	4043.395381	23.394035
108.965159	4053.100344	23.399053
108.979491	4040.053800	23.404071
109.244131	4057.740580	23.409088
109.395659	4073.464502	23.414106
109.681988	4074.830601	23.419123
109.305684	4088.131429	23.424141
109.502957	4080.026462	23.429159
109.673132	4081.173950	23.434176
109.654401	4080.691175	23.439194
109.887643	4094.744076	23.444211
109.796176	4111.590906	23.449229
110.324141	4115.166381	23.454247
110.079552	4113.377565	23.459264
110.117201	4115.892282	23.464282
110.676729	4134.625741	23.469299
110.783006	4149.574509	23.474317
110.735851	4141.265794	23.479335
111.085235	4146.017682	23.484352
111.298310	4141.647233	23.489370
110.925405	4140.885956	23.494387
111.049782	4162.761949	23.499405
111.638214	4175.874700	23.504423
111.285768	4170.196447	23.509440
111.463294	4165.615714	23.514458
111.751703	4169.243384	23.519475
111.951691	4177.068915	23.524493
112.486593	4173.325624	23.529511
112.641220	4177.678187	23.534528
112.950133	4163.283991	23.539546
112.654102	4152.278090	23.544563
112.322297	4141.721827	23.549581
112.869390	4147.818661	23.554599
112.754081	4170.251220	23.559616
112.688353	4180.859751	23.564634
113.064804	4158.602488	23.569651
112.938513	4177.000483	23.574669
112.917248	4171.767921	23.579687
113.012577	4167.044858	23.584704
112.815265	4185.542004	23.589722
113.220957	4199.135777	23.594739
113.037367	4203.202486	23.599757
113.233118	4204.089841	23.604775
113.590350	4231.311553	23.609792
113.575657	4231.388761	23.614810
114.001410	4234.311438	23.619827
113.939887	4227.095260	23.624845
113.970140	4237.638755	23.629863
114.234606	4245.106406	23.634880
114.596467	4252.912315	23.639898
114.589886	4248.968307	23.644915
114.466197	4243.700674	23.649933
114.703590	4259.427132	23.654951
114.804386	4277.276281	23.659968
114.898683	4276.346456	23.664986
114.994295	4269.288161	23.670003
115.337417	4285.768473	23.675021
115.739151	4274.196380	23.680039
115.660246	4276.459109	23.685056
115.816466	4289.854408	23.690074
115.846858	4285.873178	23.695091
116.059204	4304.881150	23.700109
116.254787	4292.033592	23.705127
116.026271	4294.823431	23.710144
116.068206	4300.707325	23.715162
116.727445	4288.630051	23.720179
117.047768	4266.183474	23.725197
117.617424	4264.199859	23.730215
117.527121	4270.052440	23.735232
117.404514	4241.513432	23.740250
117.162885	4237.449203	23.745267
117.412505	4221.296557	23.750285
117.540297	4234.189002	23.755303
117.481765	4232.937172	23.760320
117.386899	4239.024364	23.765338
117.360575	4230.322378	23.770355
117.378940	4246.791741	23.775373
117.585460	4246.956813	23.780391
117.755660	4255.394027	23.785408
117.638800	4265.223625	23.790426
117.774600	4265.983088	23.795443
117.775486	4281.262011	23.800461
117.777318	4295.106468	23.805479
117.943444	4303.356971	23.810496
117.860908	4307.301492	23.815514
118.628344	4327.558391	23.820531
118.451394	4331.098812	23.825549
118.549024	4324.166543	23.830567
118.360721	4323.277111	23.835584
118.475361	4352.282125	23.840602
118.907997	4351.473565	23.845619
118.960435	4354.168957	23.850637
119.434640	4372.128965	23.855655
119.751229	4386.519165	23.860672
119.801097	4375.614621	23.865690
119.771065	4392.570902	23.870707
119.835529	4377.681043	23.875725
120.217955	4385.519843	23.880743
120.279139	4380.371625	23.885760
120.261086	4400.170975	23.890778
120.214159	4404.236810	23.895795
120.400137	4418.991948	23.900813
120.350832	4407.256476	23.905831
120.605716	4424.486204	23.910848
120.533117	4435.003518	23.915866
120.745058	4445.410827	23.920883
120.747612	4443.848475	23.925901
120.878749	4451.358729	23.930919
121.332109	4470.374327	23.935936
121.115618	4478.471201	23.940954
121.392526	4473.784976	23.945971
121.377081	4495.359323	23.950989
121.486797	4503.516883	23.956007
121.661086	4503.858161	23.961024
121.773780	4517.047055	23.966042
122.385776	4532.687482	23.971059
122.461669	4535.154606	23.976077
122.673257	4534.332559	23.981095
123.079935	4534.383060	23.986112
123.063450	4536.855605	23.991130
123.416499	4520.826515	23.996147
123.028909	4535.275330	24.001165
123.040152	4530.408954	24.006183
123.480315	4535.073910	24.011200
123.188438	4534.285837	24.016218
123.651499	4524.934282	24.021235
123.505466	4545.240821	24.026253
123.772950	4553.566841	24.031271
124.032259	4553.922420	24.036288
123.786635	4556.851362	24.041306
123.925774	4562.420455	24.046323
124.119748	4550.116294	24.051341
123.983400	4578.014698	24.056359
124.292523	4588.143429	24.061376
124.200755	4594.938564	24.066394
124.572245	4585.645019	24.071411
124.410003	4582.157780	24.076429
124.580174	4598.603218	24.081447
124.965136	4604.525435	24.086464
124.801055	4609.551298	24.091482
125.094379	4612.129369	24.096499
125.114014	4624.448628	24.101517
125.578417	4629.932107	24.106535
125.991647	4643.923086	24.111552
125.864627	4638.281432	24.116570
126.012238	4630.699778	24.121587
126.096520	4635.727921	24.126605
126.240867	4640.089007	24.131623
126.791040	4618.686702	24.136640
126.436292	4629.171234	24.141658
126.586958	4620.459078	24.146675
126.630601	4630.439957	24.151693
126.961454	4653.459772	24.156711
126.836663	4636.488578	24.161728
126.911095	4648.488543	24.166746
127.181756	4644.693916	24.171763
127.071072	4649.609386	24.176781
127.044219	4660.792177	24.181799
127.374355	4675.356797	24.186816
127.260250	4675.593752	24.191834
127.367146	4682.942364	24.196851
127.350077	4705.704367	24.201869
127.312265	4714.406140	24.206887
127.841227	4721.646838	24.211904
128.289912	4728.053888	24.216922
128.352938	4728.389538	24.221939
128.642758	4734.378711	24.226957
128.685334	4736.433230	24.231975
128.917731	4755.308901	24.236992
128.747815	4764.715656	24.242010
128.921617	4761.034256	24.247027
128.959530	4756.158678	24.252045
129.222234	4766.333388	24.257063
129.355718	4781.114474	24.262080
129.662286	4800.220089	24.267098
129.527109	4798.026468	24.272115
129.576101	4794.814540	24.277133
130.021293	4805.566652	24.282151
130.324009	4810.470169	24.287168
130.319360	4816.640324	24.292186
130.285123	4811.336063	24.297203
130.510648	4818.359206	24.302221
130.468333	4824.339115	24.307239
130.855749	4823.383661	24.312256
130.934634	4848.364064	24.317274
131.137327	4850.537429	24.322291
131.360030	4851.339654	24.327309
131.157888	4843.403054	24.332327
131.547597	4843.429982	24.337344
131.834466	4849.444492	24.342362
131.821686	4838.031429	24.347379
131.818736	4849.263165	24.352397
131.915385	4862.916066	24.357415
132.057123	4865.512139	24.362432
131.997597	4866.711816	24.367450
132.153838	4867.375798	24.372467
132.421432	4888.281425	24.377485
132.412035	4891.465911	24.382503
132.702967	4896.098543	24.387520
132.785287	4900.607365	24.392538
132.519051	4911.523957	24.397555
132.941743	4923.293739	24.402573
132.757537	4943.211397	24.407591
133.090631	4934.226382	24.412608
133.160548	4955.617953	24.417626
133.406206	4965.544404	24.422643
133.358760	4969.437227	24.427661
133.579790	4962.599651	24.432679
133.637080	4979.901229	24.437696
133.949561	4993.243358	24.442714
134.170358	4996.622529	24.447731
134.296052	4991.401240	24.452749
134.480450	5001.259089	24.457767
134.790540	5006.136644	24.462784
134.950816	5013.097027	24.467802
135.004443	5020.361284	24.472819
135.207013	5012.867618	24.477837
135.067268	5016.633169	24.482855
135.364231	5020.725814	24.487872
135.709029	5039.504510	24.492890
135.774866	5040.357863	24.497907
135.909743	5044.448948	24.502925
135.935363	5039.748952	24.507943
135.733458	5040.352422	24.512960
135.789375	5060.371905	24.517978
136.193259	5063.113691	24.522995
136.483346	5063.629963	24.528013
135.929341	5081.088964	24.533031
136.550362	5088.546143	24.538048
136.592412	5094.900444	24.543066
136.707983	5085.932384	24.548083
137.077512	5083.470664	24.553101
136.690077	5114.496862	24.558119
137.055251	5132.311574	24.563136
137.027388	5123.710142	24.568154
136.754363	5154.764371	24.573171
137.669465	5146.432753	24.578189
137.509201	5173.968809	24.583207
137.802976	5174.943974	24.588224
138.078773	5188.844753	24.593242
138.184098	5189.994772	24.598259
138.403455	5204.472275	24.603277
138.423807	5211.573202	24.608295
138.883039	5214.767732	24.613312
138.845530	5219.508280	24.618330
138.888226	5226.794519	24.623347
139.505878	5241.281057	24.628365
139.383529	5248.906029	24.633383
139.574038	5242.833696	24.638400
139.765692	5243.298121	24.643418
139.337041	5246.734256	24.648435
140.155826	5254.244675	24.653453
139.899369	5255.099320	24.658471
140.269374	5264.968798	24.663488
140.560129	5266.710301	24.668506
140.509887	5259.565412	24.673523
141.074531	5273.890640	24.678541
141.181643	5293.333395	24.683559
141.037563	5291.888110	24.688576
141.274042	5303.016430	24.693594
141.122385	5307.644355	24.698611
141.388094	5303.752739	24.703629
141.605910	5314.845564	24.708647
141.490558	5299.459281	24.713664
141.518865	5313.914116	24.718682
141.398360	5329.877584	24.723699
141.606485	5320.023524	24.728717
141.348359	5343.763402	24.733735
141.907451	5355.370406	24.738752
142.111856	5359.424491	24.743770
142.084439	5381.639122	24.748787
142.464209	5391.356655	24.753805
142.548882	5396.442860	24.758823
142.713702	5401.619380	24.763840
142.680384	5418.143011	24.768858
142.627600	5426.301129	24.773875
143.609074	5422.440055	24.778893
143.937824	5429.931517	24.783911
144.194143	5416.413472	24.788928
144.357050	5431.491530	24.793946
144.387380	5427.294245	24.798963
144.798948	5417.154116	24.803981
145.033888	5417.579107	24.808999
144.683082	5406.124226	24.814016
144.698058	5395.283799	24.819034
144.977983	5414.401657	24.824051
145.011205	5418.228893	24.829069
144.720793	5420.571227	24.834087
144.834546	5436.636272	24.839104
144.889519	5430.094862	24.844122
144.960470	5442.293280	24.849139
145.217215	5450.720780	24.854157
145.144096	5462.647707	24.859175
145.265099	5475.363537	24.864192
145.790604	5483.160353	24.869210
145.784827	5493.266892	24.874227
145.936266	5506.315556	24.879245
146.021440	5521.143912	24.884263
146.519697	5527.916774	24.889280
146.752508	5536.662489	24.894298
146.588713	5544.720492	24.899315
146.800422	5534.853105	24.904333
147.125157	5561.800585	24.909351
147.056222	5578.521239	24.914368
147.123633	5571.270535	24.919386
147.230370	5591.604391	24.924403
147.543174	5594.318009	24.929421
147.540580	5612.963430	24.934439
147.353670	5618.183570	24.939456
147.834961	5632.535107	24.944474
147.835499	5649.935004	24.949491
148.012408	5642.213751	24.954509
148.377575	5668.668840	24.959527
148.902391	5653.028777	24.964544
149.300678	5683.707740	24.969562
149.283676	5692.051449	24.974579
149.516875	5697.668407	24.979597
149.716302	5703.872525	24.984615
149.803146	5692.629806	24.989632
150.321691	5684.907603	24.994650
149.914564	5696.093721	24.999667
150.277124	5681.010828	25.004685
150.738140	5686.963814	25.009703
149.921204	5679.593790	25.014720
150.805857	5695.238376	25.019738
150.365623	5700.909512	25.024755
150.744358	5700.771700	25.029773
150.867887	5709.348140	25.034791
151.101622	5727.519155	25.039808
151.480573	5721.965579	25.044826
151.534910	5742.798516	25.049843
151.920431	5731.428454	25.054861
151.674321	5737.256531	25.059879
151.706889	5733.169441	25.064896
152.188909	5729.254973	25.069914
151.978742	5763.979678	25.074931
152.414299	5756.972434	25.079949
152.498247	5757.120766	25.084967
152.261055	5761.525126	25.089984
152.709128	5755.917198	25.095002
152.945491	5770.430217	25.100019
152.955977	5787.073788	25.105037
153.098168	5791.875775	25.110055
153.079885	5788.479455	25.115072
153.474010	5789.529825	25.120090
153.432272	5785.401841	25.125107
153.708280	5797.115014	25.130125
153.647753	5809.681950	25.135143
154.041050	5800.536078	25.140160
154.166569	5798.465406	25.145178
154.273154	5819.038987	25.150195
154.328205	5829.247127	25.155213
154.717518	5843.320312	25.160231
154.464711	5834.155174	25.165248
154.702583	5854.020392	25.170266
154.699212	5862.072526	25.175283
154.887927	5864.788977	25.180301
155.704511	5869.708333	25.185319
155.583557	5897.473451	25.190336
155.862595	5882.649479	25.195354
156.027911	5895.050014	25.200371
156.260203	5896.012547	25.205389
156.429098	5887.719575	25.210407
156.462520	5904.929254	25.215424
156.505553	5919.347957	25.220442
156.412200	5919.928009	25.225459
156.267458	5919.465997	25.230477
156.666663	5940.830101	25.235495
156.809452	5958.093432	25.240512
156.997674	5961.878652	25.245530
157.171135	5983.258062	25.250547
157.290702	5977.164880	25.255565
157.315572	5993.969706	25.260583
157.411460	6009.438194	25.265600
157.572105	6021.919141	25.270618
157.984433	6040.267342	25.275635
157.992858	6042.853744	25.280653
158.246667	6050.353163	25.285671
158.260229	6067.747433	25.290688
158.827563	6073.319162	25.295706
159.099080	6089.623419	25.300723
159.199892	6102.723078	25.305741
159.661441	6106.634067	25.310759
159.548320	6101.845635	25.315776
159.302721	6106.246755	25.320794
159.539875	6130.075305	25.325811
159.636701	6139.350603	25.330829
159.942029	6135.927909	25.335847
160.344333	6165.972794	25.340864
160.676306	6154.634903	25.345882
160.826251	6164.243230	25.350899
160.554219	6168.283318	25.355917
161.147606	6175.437663	25.360935
161.323344	6192.101218	25.365952
161.818220	6193.251132	25.370970
161.551621	6186.830268	25.375987
161.647281	6188.647821	25.381005
161.922503	6199.664062	25.386023
161.482921	6210.984275	25.391040
161.992203	6221.488547	25.396058
161.953450	6217.287109	25.401075
162.331610	6237.150897	25.406093
162.728682	6238.861951	25.411111
162.607347	6253.197863	25.416128
162.975590	6248.954370	25.421146
162.824365	6254.488958	25.426163
163.018939	6282.705859	25.431181
163.305824	6285.281732	25.436199
163.216079	6285.162652	25.441216
163.280995	6293.791231	25.446234
163.984395	6322.315539	25.451251
163.765058	6318.414038	25.456269
163.858242	6307.439959	25.461287
164.167019	6333.484942	25.466304
164.481697	6331.180547	25.471322
164.332264	6337.497686	25.476339
164.400879	6351.976350	25.481357
164.979598	6364.831093	25.486375
164.934256	6367.431946	25.491392
165.211382	6365.709447	25.496410
165.468937	6390.139855	25.501427
165.438757	6402.221059	25.506445
165.719528	6396.885476	25.511463
165.506850	6418.209572	25.516480
165.828591	6427.479381	25.521498
166.142135	6438.352424	25.526515
166.420128	6427.365840	25.531533
166.646600	6445.759401	25.536551
166.836562	6454.562719	25.541568
166.890155	6451.077593	25.546586
167.158716	6469.019262	25.551603
167.354821	6475.197458	25.556621
167.425956	6479.817266	25.561639
167.349785	6494.126245	25.566656
167.701880	6503.865978	25.571674
167.879188	6515.934250	25.576691
167.978611	6517.465338	25.581709
168.504946	6526.664387	25.586727
168.368116	6545.380347	25.591744
168.423929	6547.122620	25.596762
168.632915	6546.197340	25.601779
168.679460	6563.892280	25.606797
168.725225	6569.087283	25.611815
168.874586	6581.501235	25.616832
169.412599	6593.691894	25.621850
169.817390	6596.779151	25.626867
169.806045	6607.684728	25.631885
170.145005	6625.244003	25.636903
169.910673	6638.957863	25.641920
170.056426	6636.158397	25.646938
170.592934	6645.226675	25.651955
171.003396	6653.408516	25.656973
171.491439	6650.637548	25.661991
171.593973	6640.457916	25.667008
172.166051	6630.322780	25.672026
172.458705	6625.454542	25.677044
172.317817	6636.950949	25.682061
172.254318	6621.239384	25.687079
172.321060	6632.834579	25.692096
172.301126	6630.345224	25.697114
172.656165	6626.413323	25.702132
172.635411	6634.074946	25.707149
172.588518	6633.931457	25.712167
172.734536	6655.552584	25.717184
172.900765	6666.279226	25.722202
173.275655	6654.864580	25.727220
173.082474	6678.770578	25.732237
173.065365	6695.545286	25.737255
172.996216	6705.894225	25.742272
173.387023	6706.955055	25.747290
173.709211	6730.208933	25.752308
173.568348	6734.347989	25.757325
174.091697	6750.005687	25.762343
174.009890	6769.987102	25.767360
174.421909	6783.459620	25.772378
174.485280	6791.573658	25.777396
174.394103	6806.658791	25.782413
174.933508	6814.860365	25.787431
175.312298	6822.679734	25.792448
175.064299	6838.000301	25.797466
175.519572	6840.032587	25.802484
175.331331	6856.769586	25.807501
176.273488	6851.683705	25.812519
175.886247	6867.964516	25.817536
176.254798	6875.390242	25.822554
176.468903	6888.360790	25.827572
176.386237	6896.914849	25.832589
176.640664	6895.248025	25.837607
176.812780	6912.335080	25.842624
176.862406	6916.457674	25.847642
177.180251	6941.211333	25.852660
177.056064	6950.943405	25.857677
177.421919	6951.958757	25.862695
177.660096	6972.370342	25.867712
178.009750	6982.024930	25.872730
178.057339	6996.870733	25.877748
178.014707	7008.088124	25.882765
178.513433	7019.709888	25.887783
178.580037	7034.065074	25.892800
178.794747	7040.077391	25.897818
178.900075	7047.627811	25.902836
179.092088	7060.028792	25.907853
179.657994	7057.693024	25.912871
180.188316	7070.454747	25.917888
180.472339	7078.050477	25.922906
180.892969	7076.909842	25.927924
180.607089	7084.061032	25.932941
181.178358	7071.699258	25.937959
180.990650	7077.753664	25.942976
180.762779	7090.248460	25.947994
181.133818	7080.875555	25.953012
181.055210	7091.550793	25.958029
181.279749	7113.224157	25.963047
181.058455	7123.389010	25.968064
181.259359	7122.959636	25.973082
181.922246	7139.162515	25.978100
181.672106	7171.395558	25.983117
182.175481	7178.855071	25.988135
182.141121	7181.037610	25.993152
182.343950	7192.966720	25.998170
183.072244	7210.630866	26.003188
182.928684	7206.114906	26.008205
183.279768	7231.440044	26.013223
183.657098	7240.547570	26.018240
183.688860	7234.507790	26.023258
183.664067	7242.241258	26.028276
183.656420	7258.363665	26.033293
183.973203	7264.064644	26.038311
184.099883	7284.773862	26.043328
184.204425	7302.111933	26.048346
184.596309	7301.263504	26.053364
184.630493	7310.964905	26.058381
184.778922	7324.496403	26.063399
184.591188	7338.858448	26.068416
185.032073	7356.686021	26.073434
185.473616	7373.519561	26.078452
185.545087	7375.096307	26.083469
185.930136	7396.701009	26.088487
185.976753	7402.204097	26.093504
186.019547	7406.180667	26.098522
186.243797	7415.892471	26.103540
186.529894	7427.363009	26.108557
187.247607	7409.218647	26.113575
187.477297	7435.511650	26.118592
187.626206	7431.453728	26.123610
188.048732	7438.288768	26.128628
188.048216	7439.470226	26.133645
188.126268	7437.122073	26.138663
188.363106	7429.039171	26.143680
188.031199	7445.129496	26.148698
188.307274	7449.514103	26.153716
188.488441	7469.455315	26.158733
188.639828	7471.509541	26.163751
188.890147	7473.550573	26.168768
188.775783	7495.436402	26.173786
189.021970	7500.237876	26.178804
189.013519	7508.030994	26.183821
188.979585	7522.930930	26.188839
189.320711	7542.998601	26.193856
189.144305	7555.782187	26.198874
189.560208	7575.839908	26.203892
189.827060	7600.884991	26.208909
189.882113	7610.473650	26.213927
190.596633	7641.104581	26.218944
190.826780	7645.711060	26.223962
191.193531	7645.733924	26.228980
191.477694	7668.422879	26.233997
191.728236	7667.587547	26.239015
192.317327	7673.150745	26.244032
192.169703	7686.235274	26.249050
192.472368	7685.984400	26.254068
192.388155	7694.005933	26.259085
192.400584	7700.396111	26.264103
192.804758	7703.868046	26.269120
192.725158	7720.493495	26.274138
193.133369	7714.350379	26.279156
193.228938	7735.429205	26.284173
193.456594	7752.724588	26.289191
193.887499	7741.795317	26.294208
193.701186	7769.264206	26.299226
193.968571	7769.327118	26.304244
194.233211	7792.008449	26.309261
194.476075	7785.627198	26.314279
194.785887	7796.512038	26.319296
194.746147	7815.116582	26.324314
195.012906	7814.857462	26.329332
194.999706	7841.621310	26.334349
195.425353	7832.936772	26.339367
195.847920	7847.378018	26.344384
195.910683	7857.063218	26.349402
196.315033	7840.552469	26.354420
196.490628	7859.722441	26.359437
196.464722	7860.864805	26.364455
196.766550	7871.760468	26.369472
196.628712	7880.832190	26.374490
197.186382	7888.522509	26.379508
197.241324	7897.329253	26.384525
197.160390	7908.971050	26.389543
197.520519	7921.913597	26.394560
197.619305	7949.897270	26.399578
198.024181	7940.233150	26.404596
198.252203	7963.350032	26.409613
198.281753	7957.484407	26.414631
198.884566	7967.434090	26.419648
198.819279	7976.689998	26.424666
199.114294	7998.869617	26.429684
199.208295	8002.280236	26.434701
198.950558	8000.477385	26.439719
199.229655	8033.727418	26.444736
199.205258	8038.947887	26.449754
199.517477	8046.518948	26.454772
200.052555	8060.449533	26.459789
200.274717	8074.946153	26.464807
200.695659	8091.868929	26.469824
200.619734	8094.327830	26.474842
200.460518	8096.642180	26.479860
200.863356	8116.490875	26.484877
201.105984	8134.351297	26.489895
201.451222	8131.361871	26.494912
202.065949	8152.876104	26.499930
202.163581	8154.606920	26.504948
202.411467	8158.137861	26.509965
202.101366	8162.469865	26.514983
202.560768	8177.139256	26.520000
202.899799	8185.149393	26.525018
202.904965	8187.269618	26.530036
203.199798	8197.960301	26.535053
203.225638	8212.355586	26.540071
203.453087	8216.303426	26.545088
203.260514	8240.193565	26.550106
203.849801	8237.567068	26.555124
203.668294	8258.374951	26.560141
203.648084	8277.937732	26.565159
204.182294	8288.748818	26.570176
204.117269	8306.196345	26.575194
204.922980	8339.426962	26.580212
204.810778	8353.565568	26.585229
204.578692	8367.304968	26.590247
205.053020	8381.011942	26.595264
205.642566	8407.600758	26.600282
205.523827	8408.730145	26.605300
205.947077	8423.132424	26.610317
206.287068	8442.111320	26.615335
206.432784	8458.194644	26.620352
206.448263	8484.152224	26.625370
206.627955	8483.765703	26.630388
207.197199	8505.160330	26.635405
207.164170	8514.549061	26.640423
207.644133	8531.823302	26.645440
207.723234	8549.861653	26.650458
207.924318	8576.261310	26.655476
207.749353	8582.693043	26.660493
208.076966	8603.565340	26.665511
208.163887	8606.573192	26.670528
208.527454	8639.487600	26.675546
208.611684	8649.754180	26.680564
209.017701	8651.769643	26.685581
209.420105	8686.314487	26.690599
209.439318	8700.250527	26.695616
209.791972	8716.285744	26.700634
210.024994	8741.721026	26.705652
210.322120	8755.323701	26.710669
210.467391	8765.084829	26.715687
210.546778	8783.010762	26.720704
210.771817	8781.077644	26.725722
210.790554	8806.556311	26.730740
211.360791	8809.602498	26.735757
211.676720	8824.955472	26.740775
212.919564	8807.956249	26.745792
214.013400	8786.310016	26.750810
214.118275	8782.806454	26.755828
214.396235	8755.441131	26.760845
214.214163	8758.626571	26.765863
214.406524	8750.196687	26.770880
214.725469	8723.432724	26.775898
214.574137	8722.373877	26.780916
214.667709	8712.763875	26.785933
214.291668	8726.260351	26.790951
214.729751	8700.081668	26.795968
214.403572	8718.552647	26.800986
214.351009	8716.477938	26.806004
214.775999	8719.367731	26.811021
214.667496	8742.852479	26.816039
214.887138	8748.467652	26.821056
214.753288	8764.206008	26.826074
214.796111	8781.836306	26.831092
215.209596	8784.653971	26.836109
215.127662	8820.078611	26.841127
215.388432	8832.765000	26.846144
215.331242	8849.795153	26.851162
215.747263	8870.733538	26.856180
215.663241	8895.636211	26.861197
215.596463	8928.466361	26.866215
215.979193	8967.700148	26.871232
216.471804	8983.039051	26.876250
216.761815	9007.441365	26.881268
217.373514	9020.902499	26.886285
218.053776	9032.016064	26.891303
218.205451	9036.859617	26.896320
218.658684	9056.490854	26.901338
218.669218	9059.071888	26.906356
218.840978	9071.995300	26.911373
218.818724	9092.427445	26.916391
219.180055	9101.395334	26.921408
219.552329	9111.927332	26.926426
219.188065	9136.208728	26.931444
219.605905	9146.767879	26.936461
219.879625	9166.261135	26.941479
220.005948	9196.151802	26.946496
220.336544	9207.132641	26.951514
220.248871	9236.289958	26.956532
220.622094	9240.295890	26.961549
221.015831	9278.150958	26.966567
221.378609	9296.711213	26.971584
221.715718	9303.557241	26.976602
221.653418	9315.595560	26.981620
222.306626	9328.258468	26.986637
222.260662	9344.827282	26.991655
222.322606	9348.131636	26.996672
222.592680	9375.385322	27.001690
223.141587	9392.670379	27.006708
223.581225	9380.722420	27.011725
223.939664	9403.000650	27.016743
224.257630	9412.123967	27.021760
224.372826	9422.274865	27.026778
224.408282	9425.927048	27.031796
224.569990	9414.941862	27.036813
224.974124	9440.242077	27.041831
225.233569	9442.547315	27.046848
225.156469	9460.775560	27.051866
225.527027	9481.885317	27.056884
225.618045	9479.017991	27.061901
225.617285	9494.572811	27.066919
226.018149	9510.189687	27.071936
226.145916	9516.575718	27.076954
226.134650	9537.227173	27.081972
227.187902	9545.694235	27.086989
227.955902	9525.154002	27.092007
228.089090	9541.470502	27.097024
228.225131	9543.915086	27.102042
228.082474	9558.022771	27.107060
228.357465	9560.334122	27.112077
228.340282	9565.442046	27.117095
228.561577	9559.670184	27.122112
228.678796	9587.450468	27.127130
228.864123	9593.522966	27.132148
228.984003	9597.855996	27.137165
228.859812	9608.492406	27.142183
229.150303	9633.157120	27.147200
229.166192	9640.358058	27.152218
229.081747	9658.571201	27.157236
229.425555	9664.523017	27.162253
229.676673	9698.235666	27.167271
229.510436	9717.509258	27.172288
229.903773	9742.955890	27.177306
230.255756	9774.400752	27.182324
230.813690	9783.779242	27.187341
230.828119	9811.972332	27.192359
231.261711	9822.902709	27.197376
231.809224	9832.796542	27.202394
231.868464	9848.478857	27.207412
232.278588	9848.499296	27.212429
232.391197	9877.539620	27.217447
232.594025	9884.795644	27.222464
233.048696	9908.040970	27.227482
233.060345	9928.351212	27.232500
233.500452	9933.558576	27.237517
233.490235	9946.254392	27.242535
233.920793	9965.931461	27.247552
234.380138	9972.551988	27.252570
234.434544	9997.789561	27.257588
234.649068	10006.426167	27.262605
235.135182	10013.235281	27.267623
235.706378	10029.282982	27.272640
235.764491	10030.124101	27.277658
235.667330	10041.815825	27.282676
236.031846	10048.881363	27.287693
235.827035	10065.156563	27.292711
236.371587	10085.290735	27.297728
236.528968	10085.972089	27.302746
236.441815	10112.102097	27.307764
236.931006	10118.713815	27.312781
237.249040	10144.006530	27.317799
237.356497	10163.989301	27.322816
237.557366	10179.951820	27.327834
237.531839	10202.794819	27.332852
237.777145	10219.550375	27.337869
238.505753	10240.306580	27.342887
238.666128	10253.643244	27.347904
239.407022	10245.287373	27.352922
239.241828	10273.153320	27.357940
239.813158	10282.654356	27.362957
239.835093	10299.477622	27.367975
240.004983	10304.766777	27.372992
240.579280	10326.647489	27.378010
240.497336	10322.600192	27.383028
240.597147	10339.528008	27.388045
240.623563	10364.524221	27.393063
241.090895	10388.039927	27.398080
241.010008	10393.213782	27.403098
241.655320	10424.646124	27.408116
241.742114	10429.147123	27.413133
242.021963	10449.600413	27.418151
242.016512	10461.441143	27.423168
242.244431	10477.175769	27.428186
242.041505	10499.815327	27.433204
242.450763	10524.424772	27.438221
242.645608	10556.847953	27.443239
243.082871	10577.227346	27.448256
243.521282	10597.141799	27.453274
243.612453	10618.569420	27.458292
243.922438	10638.569739	27.463309
244.268879	10657.134279	27.468327
244.553460	10689.206529	27.473344
244.973103	10697.136874	27.478362
245.011242	10711.055788	27.483380
245.391298	10723.259198	27.488397
245.620857	10726.965476	27.493415
245.746217	10751.028202	27.498432
246.404818	10749.622709	27.503450
246.078818	10767.411453	27.508468
246.399477	10788.755697	27.513485
247.096827	10796.130526	27.518503
247.218304	10825.124627	27.523520
247.383285	10841.364727	27.528538
247.808737	10847.825789	27.533556
247.899612	10870.024232	27.538573
248.123192	10865.605699	27.543591
248.219693	10885.645537	27.548608
248.564248	10899.442303	27.553626
248.830456	10920.527089	27.558644
249.172959	10926.611153	27.563661
249.636286	10948.593768	27.568679
249.655825	10966.502105	27.573696
250.058569	10960.582386	27.578714
250.724916	10974.844407	27.583732
250.907734	10965.975359	27.588749
251.617341	10966.586786	27.593767
251.631667	10959.923771	27.598784
251.815676	10989.682220	27.603802
252.201886	10990.994629	27.608820
252.285147	10998.628564	27.613837
252.637606	10990.911562	27.618855
252.492095	11007.400860	27.623872
252.553716	11017.898792	27.628890
252.713264	11041.425346	27.633908
252.873645	11063.371513	27.638925
253.027984	11069.960175	27.643943
253.093045	11091.481761	27.648960
253.230023	11104.955347	27.653978
253.087645	11139.300884	27.658996
253.362438	11167.763731	27.664013
253.729075	11191.096370	27.669031
253.864620	11225.207893	27.674048
254.317217	11249.142464	27.679066
254.770705	11276.823645	27.684084
255.105401	11300.167234	27.689101
255.234955	11321.071087	27.694119
255.737331	11354.273040	27.699136
256.089184	11339.527291	27.704154
256.607040	11377.292775	27.709172
256.518118	11385.717138	27.714189
257.169595	11395.170936	27.719207
256.872728	11422.588742	27.724224
257.367550	11422.354921	27.729242
257.716552	11461.598045	27.734260
257.641090	11479.233528	27.739277
257.937927	11497.868687	27.744295
258.204754	11519.951513	27.749312
258.986703	11548.536075	27.754330
259.047844	11564.222119	27.759348
259.054700	11573.653323	27.764365
259.351259	11610.223793	27.769383
259.577545	11622.739269	27.774400
259.724009	11647.637290	27.779418
260.202963	11662.862863	27.784436
260.188051	11680.761931	27.789453
260.822028	11698.608174	27.794471
260.934092	11734.241977	27.799488
261.335699	11738.045329	27.804506
261.750764	11765.712430	27.809524
261.919249	11787.493595	27.814541
262.062445	11790.283982	27.819559
262.049969	11811.497126	27.824576
262.287691	11834.391127	27.829594
262.579618	11842.967881	27.834612
262.531184	11874.090688	27.839629
263.271947	11882.016628	27.844647
263.380214	11897.936284	27.849664
263.913479	11916.532080	27.854682
264.832309	11912.550661	27.859700
265.303886	11922.741169	27.864717
265.885941	11931.733277	27.869735
266.284648	11933.900852	27.874752
266.133607	11927.869803	27.879770
266.461005	11933.973293	27.884788
266.174990	11923.911995	27.889805
266.635760	11952.072921	27.894823
266.810576	11951.535081	27.899840
266.982623	11954.872993	27.904858
267.213371	11977.838467	27.909876
267.069771	11985.047112	27.914893
267.682163	12008.576686	27.919911
267.326796	12015.717913	27.924928
267.607774	12039.625293	27.929946
268.156272	12063.816248	27.934964
268.145022	12098.453358	27.939981
268.289534	12097.985121	27.944999
268.799843	12143.746179	27.950016
268.915277	12144.355772	27.955034
269.054166	12170.237490	27.960052
269.282731	12206.384877	27.965069
269.800948	12222.340332	27.970087
270.101595	12245.744494	27.975104
270.354598	12264.606803	27.980122
270.970651	12281.335566	27.985140
270.853170	12298.952100	27.990157
271.617590	12325.216820	27.995175
271.871338	12347.729953	28.000192
272.349218	12370.052460	28.005210
272.626550	12375.936703	28.010228
272.484548	12401.094689	28.015245
272.928668	12415.350593	28.020263
273.272751	12423.575542	28.025280
273.488065	12434.917999	28.030298
273.872262	12453.367296	28.035316
273.826103	12485.496986	28.040333
274.332473	12481.855384	28.045351
274.403147	12505.075743	28.050368
274.620411	12545.305238	28.055386
275.020347	12543.732768	28.060404
275.079722	12572.293567	28.065421
275.027242	12603.813164	28.070439
275.780009	12612.741211	28.075456
276.025525	12636.912965	28.080474
276.645428	12651.979892	28.085492
276.739129	12662.920311	28.090509
277.394419	12693.150822	28.095527
277.516776	12690.921429	28.100544
277.654211	12721.885167	28.105562
278.026969	12726.796525	28.110580
278.100369	12748.119619	28.115597
278.420502	12756.990013	28.120615
278.688791	12793.467782	28.125632
278.500373	12808.389495	28.130650
279.110027	12824.036568	28.135668
279.294675	12856.380981	28.140685
279.629345	12867.108397	28.145703
280.140868	12890.073693	28.150720
280.662346	12888.723775	28.155738
281.312391	12894.129852	28.160756
281.205861	12905.968594	28.165773
282.284658	12892.517921	28.170791
282.559078	12891.378999	28.175808
282.825347	12901.315690	28.180826
283.241652	12898.535046	28.185844
282.760323	12901.611589	28.190861
282.986605	12905.587579	28.195879
282.951524	12919.020202	28.200896
283.216371	12935.253798	28.205914
283.821765	12950.057102	28.210932
283.548050	12970.984023	28.215949
283.576683	12981.810925	28.220967
283.801028	13007.830352	28.225984
284.007669	13032.652026	28.231002
284.100809	13054.957106	28.236020
284.287482	13081.378389	28.241037
284.353891	13119.985998	28.246055
284.937341	13146.393836	28.251072
284.953535	13181.163459	28.256090
285.446773	13204.155860	28.261108
285.818833	13229.259356	28.266125
286.397619	13256.692394	28.271143
286.935787	13274.663372	28.276160
287.262246	13300.721552	28.281178
287.806134	13295.702649	28.286196
288.274731	13339.805246	28.291213
288.651612	13331.503214	28.296231
288.932319	13364.477266	28.301248
288.861134	13374.659093	28.306266
289.564671	13388.223780	28.311284
289.681020	13408.486450	28.316301
289.797315	13429.466137	28.321319
290.066510	13440.401726	28.326336
290.082888	13464.387235	28.331354
290.153034	13471.543893	28.336372
290.761657	13500.283474	28.341389
291.291029	13514.727971	28.346407
292.078533	13512.536703	28.351424
292.339394	13543.747933	28.356442
292.868408	13547.280119	28.361460
292.706391	13556.247943	28.366477
292.884908	13578.802798	28.371495
293.201750	13581.878395	28.376512
293.176579	13607.360113	28.381530
293.703588	13626.987922	28.386548
293.628428	13649.559572	28.391565
293.922619	13667.530323	28.396583
294.252552	13692.806960	28.401600
294.530880	13717.937731	28.406618
295.026345	13732.827677	28.411636
295.825954	13759.768101	28.416653
295.830549	13760.211697	28.421671
295.757052	13786.629838	28.426688
296.076938	13804.525585	28.431706
296.516832	13813.819583	28.436724
296.257978	13833.534926	28.441741
296.660061	13857.131099	28.446759
297.007954	13890.550536	28.451776
297.295139	13909.594280	28.456794
297.598840	13936.413643	28.461812
297.693107	13969.443365	28.466829
298.257260	13984.085819	28.471847
298.619397	14017.581957	28.476864
298.585697	14045.796709	28.481882
299.035261	14064.334751	28.486900
299.498024	14092.809526	28.491917
299.515742	14107.441511	28.496935
299.955218	14132.989118	28.501952
300.277091	14166.675014	28.506970
300.402773	14179.495902	28.511988
301.202546	14201.454167	28.517005
301.206507	14215.913602	28.522023
301.854224	14237.711085	28.527040
301.959998	14267.004710	28.532058
302.434896	14267.551847	28.537076
302.706825	14300.809758	28.542093
302.946626	14310.460153	28.547111
303.201984	14329.976106	28.552128
303.271393	14367.875468	28.557146
303.441402	14396.971185	28.562164
303.943104	14406.592552	28.567181
303.859277	14430.506216	28.572199
304.307099	14459.349707	28.577216
304.704910	14482.444788	28.582234
305.136220	14508.285873	28.587252
305.446885	14536.041155	28.592269
305.743093	14558.634660	28.597287
306.469493	14570.474112	28.602304
306.503879	14594.565475	28.607322
307.084322	14613.235385	28.612340
307.463682	14633.405703	28.617357
307.489271	14658.089576	28.622375
307.791524	14675.987622	28.627392
308.168067	14705.525693	28.632410
308.466496	14710.749364	28.637428
308.760163	14740.704624	28.642445
308.604436	14754.131904	28.647463
309.540325	14784.241173	28.652480
309.813371	14805.316510	28.657498
310.056404	14826.327491	28.662516
310.731052	14847.183672	28.667533
310.738742	14864.911535	28.672551
311.207257	14875.807285	28.677568
311.598696	14910.813313	28.682586
311.775426	14921.779362	28.687604
312.151454	14936.507340	28.692621
312.369768	14956.123144	28.697639
312.877833	14979.394556	28.702656
313.048571	15002.943937	28.707674
313.395901	15015.298634	28.712692
313.711472	15031.188698	28.717709
313.856771	15059.208584	28.722727
314.163572	15074.056863	28.727744
313.874568	15105.335139	28.732762
314.534787	15118.459294	28.737780
314.772176	15145.803791	28.742797
315.089942	15173.339930	28.747815
315.683811	15185.409754	28.752832
316.164220	15206.649924	28.757850
316.420742	15230.168125	28.762868
317.139848	15246.125691	28.767885
317.439948	15278.780502	28.772903
318.023932	15272.717394	28.777920
317.919243	15291.925206	28.782938
318.443188	15314.092872	28.787956
318.770012	15317.088355	28.792973
318.861895	15344.200340	28.797991
319.417114	15347.969723	28.803008
319.400864	15380.314526	28.808026
319.581981	15391.335326	28.813044
320.100756	15402.237312	28.818061
319.936757	15413.212701	28.823079
320.568310	15438.596670	28.828096
320.915263	15467.791144	28.833114
321.002399	15469.292820	28.838132
321.501555	15506.104169	28.843149
321.498050	15521.688099	28.848167
322.571428	15541.696034	28.853184
323.093200	15539.471190	28.858202
323.318532	15564.402386	28.863220
323.610340	15571.100983	28.868237
323.715472	15586.741099	28.873255
323.733470	15592.676453	28.878272
323.875859	15618.749848	28.883290
324.402835	15652.280430	28.888308
324.300961	15645.559827	28.893325
324.325253	15690.686226	28.898343
324.679039	15713.680006	28.903360
324.921386	15743.729115	28.908378
325.128077	15771.428030	28.913396
325.241174	15812.265945	28.918413
325.844149	15842.763137	28.923431
326.129480	15872.660388	28.928448
326.549257	15907.785227	28.933466
326.812406	15933.391581	28.938484
327.491553	15962.826778	28.943501
327.837675	15990.436836	28.948519
328.547148	16015.336019	28.953536
328.663694	16044.582196	28.958554
329.083545	16061.768878	28.963572
329.587201	16087.025261	28.968589
329.764449	16113.481392	28.973607
330.250516	16146.598941	28.978624
330.453839	16163.807317	28.983642
330.767833	16183.730304	28.988660
331.184360	16203.732517	28.993677
331.640278	16224.569860	28.998695
332.185398	16223.961257	29.003712
332.395923	16260.836173	29.008730
332.546481	16290.471184	29.013748
332.765799	16291.093722	29.018765
333.086165	16322.710220	29.023783
333.752418	16354.205020	29.028800
334.153901	16368.346941	29.033818
334.377894	16391.509691	29.038836
334.776240	16420.281292	29.043853
334.802915	16438.869837	29.048871
335.323203	16460.930917	29.053888
335.831094	16493.497087	29.058906
335.672429	16506.879004	29.063924
336.102533	16526.397086	29.068941
336.225901	16553.598860	29.073959
336.793185	16580.585495	29.078976
336.720939	16609.865444	29.083994
336.904345	16649.618932	29.089012
337.621891	16671.264717	29.094029
337.648169	16706.063824	29.099047
338.178441	16734.672333	29.104064
338.328401	16771.911449	29.109082
338.398298	16796.999439	29.114100
338.844964	16835.072305	29.119117
339.287852	16862.625291	29.124135
340.262134	16881.663021	29.129152
341.019086	16893.954625	29.134170
341.279759	16933.543152	29.139188
342.033079	16930.958347	29.144205
341.912560	16967.440341	29.149223
342.442885	16983.886300	29.154240
342.781196	16995.988655	29.159258
342.754270	17020.941673	29.164276
343.260134	17041.644139	29.169293
343.612124	17073.795898	29.174311
343.902043	17078.317204	29.179328
344.585643	17085.828033	29.184346
345.409208	17097.240334	29.189364
345.967774	17093.210835	29.194381
346.012896	17097.870307	29.199399
346.358964	17087.719509	29.204416
346.834407	17107.389984	29.209434
346.902194	17130.584310	29.214452
347.662817	17131.944935	29.219469
347.163267	17133.988157	29.224487
347.343442	17162.730904	29.229504
347.674513	17167.344734	29.234522
347.720943	17195.822775	29.239540
348.181631	17205.682697	29.244557
347.973268	17248.478127	29.249575
348.221797	17267.943552	29.254592
348.528345	17298.566505	29.259610
348.409004	17350.459275	29.264628
348.735367	17376.224512	29.269645
348.609269	17420.516765	29.274663
349.308369	17462.229743	29.279680
350.220792	17496.723362	29.284698
350.071096	17552.559077	29.289716
350.741512	17584.545745	29.294733
351.341763	17612.311996	29.299751
352.632304	17629.145279	29.304768
353.099358	17646.264355	29.309786
353.385257	17675.378274	29.314804
353.811636	17693.605880	29.319821
354.105660	17729.524576	29.324839
353.981586	17755.773053	29.329856
354.663996	17775.663907	29.334874
354.600025	17796.855512	29.339892
355.266439	17820.281343	29.344909
355.088439	17855.605248	29.349927
355.295310	17881.502926	29.354944
355.605431	17910.876487	29.359962
355.708784	17961.103000	29.364980
356.334567	17996.721580	29.369997
356.582213	18037.295323	29.375015
356.850014	18073.135557	29.380032
357.102958	18105.365588	29.385050
357.499750	18148.367590	29.390068
357.937580	18185.258127	29.395085
358.212544	18226.496149	29.400103
358.585073	18269.948552	29.405120
359.216666	18307.295992	29.410138
359.806632	18340.501678	29.415156
360.644243	18370.890723	29.420173
361.025461	18395.135277	29.425191
361.456430	18412.491246	29.430208
362.038747	18433.725070	29.435226
362.212611	18465.686715	29.440244
362.443138	18480.287444	29.445261
362.881734	18507.120382	29.450279
362.728833	18535.304217	29.455296
363.304854	18565.128390	29.460314
363.557907	18601.670498	29.465332
363.734534	18636.456717	29.470349
363.886087	18676.422114	29.475367
364.216251	18713.044730	29.480384
364.706686	18739.708699	29.485402
364.989933	18785.618890	29.490420
365.417201	18820.706148	29.495437
365.568477	18855.678290	29.500455
366.038066	18894.819284	29.505472
366.558212	18933.182777	29.510490
366.794916	18963.919662	29.515508
367.228028	18993.984171	29.520525
367.734774	19032.584980	29.525543
368.273692	19059.719082	29.530560
369.241683	19077.089497	29.535578
369.029546	19108.682655	29.540596
369.187752	19114.682814	29.545613
369.648100	19155.099626	29.550631
369.847817	19185.814658	29.555648
370.554019	19205.124790	29.560666
371.004101	19253.138352	29.565684
371.347731	19266.515185	29.570701
371.922409	19297.149566	29.575719
372.373514	19318.768763	29.580736
372.955386	19341.056831	29.585754
373.211958	19363.051867	29.590772
373.891613	19377.049538	29.595789
374.013631	19413.674982	29.600807
374.511251	19425.358716	29.605824
374.485326	19449.746161	29.610842
374.709306	19470.789871	29.615860
375.054577	19503.355746	29.620877
375.731643	19535.307261	29.625895
375.876111	19560.538455	29.630912
376.253240	19589.762050	29.635930
376.403121	19630.370028	29.640948
376.817339	19650.551787	29.645965
377.229194	19683.873138	29.650983
377.494047	19720.412606	29.656000
377.938736	19750.184941	29.661018
378.714596	19786.668515	29.666036
378.722304	19810.116129	29.671053
379.003315	19837.790674	29.676071
379.186573	19875.940857	29.681088
379.930705	19914.627461	29.686106
380.133325	19954.346304	29.691124
380.617077	19973.690929	29.696141
381.305980	19995.071521	29.701159
381.761549	20034.501272	29.706176
381.977427	20060.189623	29.711194
382.608816	20096.079784	29.716212
382.907475	20119.645295	29.721229
383.512292	20147.372486	29.726247
383.909367	20172.528196	29.731264
384.060372	20195.197568	29.736282
384.712634	20231.016786	29.741300
385.036615	20255.092224	29.746317
385.728255	20288.603458	29.751335
385.748261	20308.713986	29.756352
385.990633	20340.469286	29.761370
386.056323	20371.331608	29.766388
386.233725	20396.385217	29.771405
386.939293	20425.688447	29.776423
387.568979	20465.144054	29.781440
388.057680	20486.581998	29.786458
388.227393	20517.235078	29.791476
388.587064	20548.739657	29.796493
389.140816	20568.481716	29.801511
389.956361	20600.678828	29.806528
390.876347	20602.407561	29.811546
391.214110	20599.886135	29.816564
391.650020	20616.255148	29.821581
392.244160	20631.533917	29.826599
392.481149	20647.245323	29.831616
392.633576	20661.080515	29.836634
392.814170	20681.945322	29.841652
392.709520	20699.436307	29.846669
393.231871	20718.026593	29.851687
393.529892	20754.698426	29.856704
393.800333	20777.399307	29.861722
394.181217	20803.548681	29.866740
394.289144	20830.324913	29.871757
394.861514	20860.760765	29.876775
395.013999	20890.126223	29.881792
394.987204	20919.653775	29.886810
395.519091	20955.669427	29.891828
395.793813	20995.150242	29.896845
396.017560	21026.471653	29.901863
396.318457	21065.804847	29.906880
396.887386	21104.333975	29.911898
397.134892	21146.179693	29.916916
397.855124	21187.115019	29.921933
398.354479	21210.622116	29.926951
398.632246	21257.924218	29.931968
398.684342	21291.232536	29.936986
399.233535	21320.484343	29.942004
399.609168	21361.938948	29.947021
400.676953	21395.363469	29.952039
400.623445	21434.776569	29.957056
401.206496	21464.995769	29.962074
401.790354	21492.083848	29.967092
401.827048	21537.578836	29.972109
402.791298	21567.618586	29.977127
402.909372	21604.205339	29.982144
403.706302	21626.478286	29.987162
404.070228	21678.039844	29.992180
404.252304	21699.548916	29.997197
405.153876	21721.334884	30.002215
405.280530	21759.263803	30.007232
406.093145	21782.007341	30.012250
407.068850	21788.674327	30.017268
407.383239	21827.674422	30.022285
407.925782	21816.701587	30.027303
408.267728	21854.420156	30.032320
408.685007	21868.179486	30.037338
409.197470	21882.394506	30.042356
409.255851	21897.264735	30.047373
409.502646	21915.365831	30.052391
409.730227	21940.910091	30.057408
410.463945	21962.136030	30.062426
410.919536	21987.962747	30.067444
410.807142	22015.895078	30.072461
410.980278	22042.995137	30.077479
411.411490	22080.904428	30.082496
411.655036	22110.944385	30.087514
412.153068	22155.004218	30.092532
412.475348	22185.570506	30.097549
412.936817	22206.323018	30.102567
413.446829	22257.412886	30.107584
413.324791	22289.758671	30.112602
413.571390	22323.462596	30.117620
414.262901	22362.778451	30.122637
415.076399	22390.944734	30.127655
414.892084	22435.113286	30.132672
415.332034	22470.634971	30.137690
415.689449	22523.819417	30.142708
416.220341	22558.266753	30.147725
416.624704	22600.869053	30.152743
416.738829	22655.566704	30.157760
417.649821	22689.956252	30.162778
418.146543	22716.910920	30.167796
418.397399	22770.309253	30.172813
418.748227	22807.672162	30.177831
419.123999	22846.442166	30.182848
419.423026	22888.042476	30.187866
420.462986	22918.258193	30.192884
420.721211	22951.892079	30.197901
421.840261	22963.948655	30.202919
422.307496	22997.995889	30.207936
422.612275	23020.374062	30.212954
423.099547	23032.670645	30.217972
423.432549	23082.718522	30.222989
423.789753	23092.912812	30.228007
423.945031	23128.290549	30.233024
423.999888	23160.301322	30.238042
424.351901	23190.471920	30.243060
424.634972	23231.087110	30.248077
424.645834	23270.799753	30.253095
425.063669	23314.059122	30.258112
425.522524	23351.577254	30.263130
426.957324	23378.612956	30.268148
427.146184	23426.853497	30.273165
427.725424	23449.614198	30.278183
427.976884	23493.834940	30.283200
428.369539	23521.719444	30.288218
428.602474	23549.712368	30.293236
428.788276	23602.271054	30.298253
429.022220	23630.010086	30.303271
429.535552	23682.846038	30.308288
430.435534	23710.128295	30.313306
431.349448	23741.804322	30.318324
431.833181	23777.988499	30.323341
432.420406	23794.412883	30.328359
432.664999	23833.753961	30.333376
433.048589	23863.915815	30.338394
433.681314	23900.646437	30.343412
433.811578	23930.277882	30.348429
434.281432	23959.774445	30.353447
434.630519	24002.063013	30.358464
434.829492	24025.754541	30.363482
435.453599	24063.760990	30.368500
435.629600	24102.499071	30.373517
436.708453	24138.647210	30.378535
436.878174	24171.924439	30.383552
436.987160	24209.577953	30.388570
437.534157	24246.823336	30.393588
438.276857	24282.048108	30.398605
438.885861	24308.855895	30.403623
439.254220	24342.677762	30.408640
439.238509	24381.861276	30.413658
439.882371	24418.009332	30.418676
440.307284	24464.950792	30.423693
440.833642	24491.414579	30.428711
441.033609	24529.548900	30.433728
441.175735	24572.134831	30.438746
441.648385	24612.409801	30.443764
441.969902	24655.701119	30.448781
442.147297	24701.902001	30.453799
442.697810	24745.322868	30.458816
442.953678	24808.085463	30.463834
443.749953	24844.724887	30.468852
444.005312	24892.644811	30.473869
444.683691	24950.470329	30.478887
445.273069	24975.817491	30.483904
445.594251	25040.345721	30.488922
446.225832	25066.455569	30.493940
446.407195	25120.676995	30.498957
447.082886	25167.293551	30.503975
448.099748	25199.953480	30.508992
448.282972	25256.776920	30.514010
448.688459	25272.947341	30.519028
449.347613	25321.047767	30.524045
449.893466	25343.838607	30.529063
450.211279	25372.687818	30.534080
450.479478	25424.439028	30.539098
450.995524	25442.354347	30.544116
451.502798	25470.696198	30.549133
451.541182	25517.486792	30.554151
452.197312	25550.106056	30.559168
452.412251	25580.879127	30.564186
452.778442	25630.466985	30.569204
452.937774	25667.082506	30.574221
453.561721	25703.529896	30.579239
454.216904	25741.741545	30.584256
454.642084	25792.165376	30.589274
455.011255	25830.553778	30.594292
455.363915	25873.240645	30.599309
455.648843	25915.276479	30.604327
456.336139	25964.452717	30.609344
456.494145	26018.702929	30.614362
457.129502	26042.665807	30.619380
457.478689	26089.665251	30.624397
458.454021	26127.657721	30.629415
458.845644	26179.854464	30.634432
458.865634	26228.381577	30.639450
459.620874	26276.317431	30.644468
459.932687	26324.809230	30.649485
460.448389	26359.869211	30.654503
461.216640	26415.518037	30.659520
461.454679	26465.820217	30.664538
461.802258	26494.234302	30.669556
462.414584	26534.955960	30.674573
462.913719	26587.798537	30.679591
463.589519	26610.771465	30.684608
464.189215	26668.407629	30.689626
465.017830	26680.439159	30.694644
465.707801	26709.367933	30.699661
466.116666	26753.640521	30.704679
466.749946	26775.072036	30.709696
467.054058	26813.258910	30.714714
467.797231	26842.242202	30.719732
467.897033	26874.722486	30.724749
468.541345	26900.489242	30.729767
468.938730	26932.838475	30.734784
469.623920	26966.487042	30.739802
470.214061	26998.151654	30.744820
470.526301	27017.658859	30.749837
471.236600	27051.527391	30.754855
471.714693	27067.758488	30.759872
471.943317	27090.272874	30.764890
472.513265	27128.318760	30.769908
473.081186	27162.106940	30.774925
473.188683	27201.743375	30.779943
473.578567	27238.462953	30.784960
473.529343	27268.814293	30.789978
474.052779	27306.253189	30.794996
474.348578	27344.944134	30.800013
474.460735	27401.111423	30.805031
474.953414	27439.249615	30.810048
475.155098	27508.009872	30.815066
475.903429	27563.028557	30.820084
476.443116	27599.765167	30.825101
477.113658	27656.295266	30.830119
477.615881	27697.201890	30.835136
478.017684	27730.864068	30.840154
478.380603	27789.331670	30.845172
478.564294	27835.946863	30.850189
478.969391	27882.475142	30.855207
479.918617	27941.095602	30.860224
480.353217	27968.113009	30.865242
480.687941	28029.141074	30.870260
481.235366	28080.639674	30.875277
482.338680	28104.111769	30.880295
483.871743	28127.784186	30.885312
484.536120	28166.286767	30.890330
484.978421	28176.553643	30.895348
484.998722	28202.942739	30.900365
485.269421	28234.744407	30.905383
486.082038	28248.546132	30.910400
485.885725	28279.544953	30.915418
486.509617	28309.900497	30.920436
486.550929	28337.929759	30.925453
486.398080	28385.646124	30.930471
487.083474	28418.464742	30.935488
487.684151	28476.986877	30.940506
487.957379	28523.456651	30.945524
488.240975	28560.594058	30.950541
488.098709	28615.864148	30.955559
488.759459	28684.439700	30.960576
488.938041	28735.947552	30.965594
489.718376	28797.415745	30.970612
490.348866	28857.013067	30.975629
490.475762	28919.245755	30.980647
491.120108	28980.172405	30.985664
491.289222	29039.654138	30.990682
491.822291	29095.110729	30.995700
492.702457	29158.058954	31.000717
493.086487	29234.013515	31.005735
493.995301	29290.869222	31.010752
494.607865	29344.496457	31.015770
495.099154	29407.159661	31.020788
495.914445	29450.782131	31.025805
496.397990	29504.140948	31.030823
497.111304	29543.824638	31.035840
498.009722	29594.468498	31.040858
498.748080	29636.072574	31.045876
499.705636	29671.097856	31.050893
500.286580	29710.494639	31.055911
500.627654	29730.725712	31.060928
500.876928	29772.713745	31.065946
501.480233	29798.324412	31.070964
501.813558	29837.633043	31.075981
501.930488	29882.463460	31.080999
502.707293	29920.683227	31.086016
503.191214	29965.535262	31.091034
503.528245	30013.900755	31.096052
504.385638	30055.656529	31.101069
504.423785	30098.696031	31.106087
505.105700	30132.761424	31.111104
504.897218	30175.469597	31.116122
505.730261	30222.883042	31.121140
506.732140	30270.530571	31.126157
506.517812	30319.861844	31.131175
507.183892	30365.498744	31.136192
507.856134	30418.065747	31.141210
508.113164	30470.322919	31.146228
508.889537	30517.853789	31.151245
508.944635	30580.489156	31.156263
509.491097	30621.805498	31.161280
510.088710	30682.556544	31.166298
510.518378	30738.858858	31.171316
510.858717	30786.064973	31.176333
510.811223	30848.541574	31.181351
511.518138	30908.862070	31.186368
512.085305	30983.869638	31.191386
512.499232	31031.505941	31.196404
513.058601	31085.491203	31.201421
513.473467	31168.380365	31.206439
514.237965	31216.088616	31.211456
514.888878	31280.931154	31.216474
515.246791	31340.427407	31.221492
515.636945	31393.166978	31.226509
516.564323	31463.870565	31.231527
516.740102	31500.230691	31.236544
517.391882	31560.906430	31.241562
517.973797	31607.544824	31.246580
518.595018	31654.899340	31.251597
519.076708	31715.644723	31.256615
519.649501	31761.127151	31.261632
519.758945	31815.091170	31.266650
520.506836	31873.979002	31.271668
521.651906	31912.729140	31.276685
522.387887	31970.543400	31.281703
522.884636	31998.604278	31.286720
523.515494	32052.754238	31.291738
523.717847	32086.173835	31.296756
524.402365	32131.411604	31.301773
524.914885	32194.582953	31.306791
525.426305	32218.287753	31.311808
525.847860	32277.063619	31.316826
526.372591	32330.351694	31.321844
526.783972	32379.673747	31.326861
527.055891	32434.616155	31.331879
527.846958	32486.179031	31.336896
528.304588	32537.822374	31.341914
528.695596	32599.526020	31.346932
529.299921	32646.078281	31.351949
530.008429	32681.794396	31.356967
530.757757	32733.797150	31.361984
531.166590	32783.808583	31.367002
531.678401	32829.912799	31.372020
532.524997	32874.232790	31.377037
532.576851	32937.659582	31.382055
533.211313	32988.003487	31.387072
533.888124	33038.924258	31.392090
534.184979	33099.159090	31.397108
534.995505	33147.126872	31.402125
535.668518	33190.738002	31.407143
536.154201	33241.053563	31.412160
537.442284	33268.032874	31.417178
537.874375	33311.535798	31.422196
538.522908	33337.084228	31.427213
538.985117	33387.262096	31.432231
539.206122	33422.432330	31.437248
539.909769	33474.511075	31.442266
540.287007	33522.999497	31.447284
541.033694	33556.436098	31.452301
541.515422	33592.040060	31.457319
541.911389	33632.886646	31.462336
542.465642	33684.264957	31.467354
542.625408	33734.730415	31.472372
543.707937	33771.210509	31.477389
544.257599	33820.942878	31.482407
544.597211	33861.395412	31.487424
545.315450	33902.883575	31.492442
545.462178	33952.698642	31.497460
546.228864	34004.667564	31.502477
546.485690	34045.219387	31.507495
546.749452	34108.593284	31.512512
547.164513	34170.124890	31.517530
547.390632	34224.995229	31.522548
547.896132	34278.989709	31.527565
548.604476	34350.324813	31.532583
549.086679	34423.676036	31.537600
549.434239	34480.489810	31.542618
549.542878	34542.732813	31.547636
550.006224	34610.534250	31.552653
550.637068	34681.779352	31.557671
550.873281	34757.722241	31.562688
551.639443	34832.375661	31.567706
551.772073	34895.906553	31.572724
552.704518	34955.758710	31.577741
552.958957	35030.405967	31.582759
553.116787	35093.232861	31.587776
554.517066	35171.301453	31.592794
555.098448	35240.493193	31.597812
556.276158	35272.432346	31.602829
557.273603	35327.134505	31.607847
558.225244	35382.033737	31.612864
558.919896	35430.171995	31.617882
558.910911	35465.876540	31.622900
559.651618	35532.591151	31.627917
560.015612	35574.271109	31.632935
559.943854	35653.891396	31.637952
560.798426	35683.650430	31.642970
561.097782	35762.509341	31.647988
562.106620	35797.765583	31.653005
562.466296	35872.790288	31.658023
562.398435	35934.385655	31.663040
563.154694	35994.787942	31.668058
563.535796	36069.409152	31.673076
564.125340	36141.279120	31.678093
564.683184	36208.392525	31.683111
565.323306	36284.016414	31.688128
565.967542	36347.827726	31.693146
566.428549	36433.129153	31.698164
567.116711	36485.736824	31.703181
567.858819	36547.998947	31.708199
568.414058	36618.282789	31.713216
569.202469	36683.605234	31.718234
569.974330	36744.023249	31.723252
570.810778	36795.584832	31.728269
572.438009	36828.759074	31.733287
573.404664	36873.810851	31.738304
574.718050	36890.026716	31.743322
575.230545	36941.856827	31.748340
575.651177	36965.087489	31.753357
576.283082	37001.872712	31.758375
576.563047	37027.544129	31.763392
577.257042	37062.289956	31.768410
577.427046	37093.799182	31.773428
577.891815	37126.881939	31.778445
578.584020	37162.593977	31.783463
578.657465	37209.457311	31.788480
578.923572	37265.223510	31.793498
579.283926	37302.761137	31.798516
579.776639	37355.877038	31.803533
580.001905	37421.052164	31.808551
579.981027	37489.610397	31.813568
580.504111	37542.172684	31.818586
580.746252	37625.164676	31.823604
581.535436	37698.980427	31.828621
582.127112	37770.758723	31.833639
582.171135	37855.346746	31.838656
582.970226	37915.600084	31.843674
583.420116	37999.484217	31.848692
584.075869	38073.399283	31.853709
584.754440	38159.001188	31.858727
585.379672	38234.348524	31.863744
586.409759	38296.663819	31.868762
586.949601	38369.327308	31.873780
587.766907	38429.295297	31.878797
588.565301	38500.060776	31.883815
588.743231	38556.107486	31.888832
589.728256	38629.787383	31.893850
590.188520	38701.177612	31.898868
590.562845	38756.349792	31.903885
591.339202	38824.317442	31.908903
592.113981	38895.798523	31.913920
592.822602	38939.594550	31.918938
593.383453	38998.009708	31.923956
594.032977	39053.673908	31.928973
594.720555	39091.243268	31.933991
595.094765	39140.227144	31.939008
595.734007	39208.768077	31.944026
596.139456	39277.420478	31.949044
596.636387	39328.218417	31.954061
597.343976	39387.330237	31.959079
597.715835	39455.837354	31.964096
598.627445	39509.076615	31.969114
599.050654	39578.588907	31.974132
599.678128	39637.389664	31.979149
600.657558	39688.067888	31.984167
601.501260	39759.361071	31.989184
601.914033	39815.344470	31.994202
602.568972	39856.796888	31.999220
603.996211	39893.260944	32.004237
605.026797	39925.974450	32.009255
605.921880	39980.231039	32.014272
606.311907	40016.778266	32.019290
606.537693	40058.898593	32.024308
607.161847	40100.123073	32.029325
607.917875	40147.332639	32.034343
608.310118	40182.762440	32.039360
608.705626	40236.218486	32.044378
608.890789	40287.250513	32.049396
609.594987	40349.989683	32.054413
609.854870	40395.334266	32.059431
609.648903	40479.679072	32.064448
610.362227	40543.591630	32.069466
610.574462	40631.460214	32.074484
611.114318	40712.213854	32.079501
611.669195	40774.360453	32.084519
612.011462	40878.506198	32.089536
612.512659	40955.147929	32.094554
613.121707	41053.597111	32.099572
613.597834	41125.792844	32.104589
614.630403	41220.688041	32.109607
615.063871	41303.125415	32.114624
615.915040	41389.389529	32.119642
616.722932	41477.258489	32.124660
617.330528	41560.545825	32.129677
618.013433	41637.741233	32.134695
618.114776	41714.644733	32.139712
619.286341	41799.210036	32.144730
620.416959	41862.231203	32.149748
621.898750	41914.884542	32.154765
623.242147	41977.337467	32.159783
623.777902	42040.444863	32.164800
624.617219	42094.644328	32.169818
624.719214	42143.927440	32.174836
625.572136	42187.890526	32.179853
626.332826	42245.566461	32.184871
626.810311	42292.634994	32.189888
627.348429	42348.671725	32.194906
627.831787	42413.490598	32.199924
627.877638	42473.334109	32.204941
628.601886	42526.890907	32.209959
628.877249	42600.846090	32.214976
629.389859	42668.259152	32.219994
629.650542	42740.048520	32.225012
630.030918	42821.784840	32.230029
630.963780	42899.597741	32.235047
631.607886	42978.393119	32.240064
632.445946	43043.019871	32.245082
632.851553	43109.514594	32.250100
633.156815	43182.696861	32.255117
633.952927	43242.924072	32.260135
634.792596	43314.386428	32.265152
635.496134	43384.053093	32.270170
636.265355	43455.524471	32.275188
636.529827	43522.391260	32.280205
637.520387	43579.537739	32.285223
637.564368	43661.210194	32.290240
637.946489	43734.432457	32.295258
638.204058	43814.475980	32.300276
638.386623	43901.736779	32.305293
639.352921	43992.470841	32.310311
640.075488	44084.240102	32.315328
640.840299	44176.949988	32.320346
641.273677	44266.346361	32.325364
641.398221	44362.222219	32.330381
642.348819	44444.225117	32.335399
643.006160	44553.785727	32.340416
643.279343	44648.003061	32.345434
644.420876	44743.741339	32.350452
645.249833	44829.927294	32.355469
646.252859	44917.739321	32.360487
647.163287	45010.069373	32.365504
648.094560	45084.068193	32.370522
648.824601	45173.353615	32.375540
648.940367	45269.459751	32.380557
650.018964	45335.996523	32.385575
650.580343	45423.776517	32.390592
651.400219	45505.423626	32.395610
651.902188	45584.294561	32.400628
653.052979	45656.848037	32.405645
654.278858	45711.231036	32.410663
655.205211	45783.174797	32.415680
655.794343	45856.383829	32.420698
656.516754	45921.383840	32.425716
656.745273	45995.868594	32.430733
657.629017	46054.521164	32.435751
657.855791	46137.876139	32.440768
658.202793	46211.413875	32.445786
658.810680	46289.256722	32.450804
659.219004	46381.910117	32.455821
659.921457	46459.302310	32.460839
660.142128	46543.771548	32.465856
660.584429	46633.622969	32.470874
661.294223	46731.659335	32.475892
661.915081	46817.636194	32.480909
663.090497	46909.009813	32.485927
664.069538	46986.424806	32.490944
664.843297	47074.224803	32.495962
665.925077	47148.077449	32.500980
666.629270	47226.710314	32.505997
667.390608	47296.805145	32.511015
667.680168	47374.266127	32.516032
668.055014	47459.591846	32.521050
668.740382	47543.464635	32.526068
669.611214	47617.957084	32.531085
670.412467	47699.253654	32.536103
671.007120	47777.117460	32.541120
671.955027	47846.722486	32.546138
672.664202	47912.745205	32.551156
672.983266	47999.143587	32.556173
673.758163	48067.255933	32.561191
674.192285	48155.679136	32.566208
675.153311	48239.591589	32.571226
676.142323	48310.476777	32.576244
676.963178	48376.488985	32.581261
677.616721	48431.078579	32.586279
678.588498	48502.883118	32.591296
678.860648	48566.062394	32.596314
679.619041	48631.615278	32.601332
680.086519	48704.798608	32.606349
680.487157	48758.758273	32.611367
680.864750	48846.199276	32.616384
681.333632	48926.040181	32.621402
682.331529	48983.842986	32.626420
682.873921	49062.118600	32.631437
683.618918	49147.520257	32.636455
685.175224	49205.335732	32.641472
685.866983	49262.248856	32.646490
686.868911	49325.957530	32.651508
687.038955	49403.730752	32.656525
687.835434	49453.297342	32.661543
688.509368	49527.498210	32.666560
689.014675	49593.844666	32.671578
690.014526	49663.444617	32.676596
690.091688	49736.870063	32.681613
690.807536	49819.724645	32.686631
691.505325	49895.631542	32.691648
691.514981	49969.826979	32.696666
692.055403	50046.032060	32.701684
692.753176	50138.251756	32.706701
693.644492	50230.120958	32.711719
694.155767	50331.186856	32.716736
694.492359	50411.055814	32.721754
695.390642	50511.379736	32.726772
695.413179	50627.352609	32.731789
696.429930	50718.979204	32.736807
697.235791	50815.858530	32.741824
697.899639	50914.505173	32.746842
698.577360	51012.249914	32.751860
698.998329	51122.475025	32.756877
700.296211	51216.284184	32.761895
700.760931	51315.297392	32.766912
701.337480	51423.012906	32.771930
702.523829	51518.875952	32.776948
703.243136	51606.958495	32.781965
703.954068	51711.087590	32.786983
704.394037	51808.512415	32.792000
705.025166	51913.366427	32.797018
705.790960	52010.526848	32.802036
706.264732	52120.117246	32.807053
707.268019	52218.528155	32.812071
707.938087	52329.211747	32.817088
708.483118	52435.241984	32.822106
709.315234	52537.138222	32.827124
709.581809	52643.815709	32.832141
710.709584	52744.400783	32.837159
711.696343	52859.280248	32.842176
712.286468	52967.087400	32.847194
713.155385	53069.447834	32.852212
713.499832	53177.555734	32.857229
714.450582	53277.901163	32.862247
715.116018	53383.202833	32.867264
716.228428	53484.305986	32.872282
717.280452	53566.284092	32.877300
717.696279	53676.088683	32.882317
718.962107	53760.281322	32.887335
719.807622	53848.511146	32.892352
720.836094	53936.679570	32.897370
721.498013	54017.182511	32.902388
721.882914	54102.981469	32.907405
722.340857	54197.367059	32.912423
723.280117	54285.671827	32.917440
724.583671	54351.887012	32.922458
725.949414	54412.974802	32.927476
726.825778	54483.260094	32.932493
727.571693	54553.718809	32.937511
728.207614	54601.338206	32.942528
728.988487	54672.960367	32.947546
729.478672	54733.056542	32.952564
730.147587	54800.622664	32.957581
729.985714	54867.157408	32.962599
730.922207	54932.266374	32.967616
731.293610	55025.785747	32.972634
732.035362	55099.551382	32.977652
732.512447	55186.376008	32.982669
732.892808	55276.546574	32.987687
733.569684	55359.535540	32.992704
734.544345	55458.169721	32.997722
736.011793	55507.227201	33.002740
737.959310	55565.429935	33.007757
739.074836	55636.197955	33.012775
739.782914	55685.204375	33.017792
740.061086	55768.020819	33.022810
740.856311	55817.032131	33.027828
741.679528	55869.621353	33.032845
742.544000	55939.060876	33.037863
743.096828	55988.453827	33.042880
743.273062	56072.135025	33.047898
744.301414	56132.942714	33.052916
744.749829	56215.208508	33.057933
744.853148	56290.101286	33.062951
745.678068	56365.210058	33.067968
745.896479	56463.228595	33.072986
746.414304	56544.599725	33.078004
747.249719	56634.315938	33.083021
748.118697	56737.213644	33.088039
748.557083	56836.771003	33.093056
749.532256	56923.919098	33.098074
750.649325	57013.394645	33.103092
750.892894	57114.344059	33.108109
751.280623	57217.058348	33.113127
751.759826	57324.882488	33.118144
752.337643	57426.201641	33.123162
753.152420	57544.365793	33.128180
753.855627	57650.669811	33.133197
755.040270	57744.314195	33.138215
756.690076	57836.877516	33.143232
758.224526	57904.488269	33.148250
759.556243	57981.490959	33.153268
760.208765	58066.112940	33.158285
760.807747	58145.954386	33.163303
761.987725	58214.970660	33.168320
762.495955	58298.031402	33.173338
762.876132	58377.107398	33.178356
763.336108	58459.191016	33.183373
764.026607	58553.685411	33.188391
764.449258	58635.162970	33.193408
765.025553	58726.568060	33.198426
766.115518	58810.975627	33.203444
766.474854	58903.599029	33.208461
766.929549	59013.344736	33.213479
767.527291	59105.007102	33.218496
768.141945	59218.955075	33.223514
768.784969	59312.279193	33.228532
769.894308	59421.508281	33.233549
770.355156	59514.282045	33.238567
771.431304	59616.010295	33.243584
771.925138	59719.497223	33.248602
772.636059	59831.499040	33.253620
773.748778	59936.129817	33.258637
774.391937	60051.164757	33.263655
775.475266	60160.901404	33.268672
775.773340	60255.677167	33.273690
776.331247	60351.377368	33.278708
777.620966	60449.933728	33.283725
778.632149	60535.827719	33.288743
779.165632	60636.930302	33.293760
779.995996	60734.900342	33.298778
780.770879	60820.158353	33.303796
781.608267	60918.039645	33.308813
781.810291	61024.855110	33.313831
782.605966	61119.988828	33.318848
783.379081	61232.221989	33.323866
783.698813	61339.247191	33.328884
784.828117	61449.059089	33.333901
785.206622	61564.778347	33.338919
785.723767	61686.043309	33.343936
786.227682	61808.031666	33.348954
787.159596	61916.538838	33.353972
788.408479	62035.264460	33.358989
789.030696	62164.244447	33.364007
790.400158	62264.641971	33.369024
791.145539	62391.650120	33.374042
792.045304	62494.452188	33.379060
793.119448	62599.773063	33.384077
793.830455	62716.436254	33.389095
795.254167	62815.038881	33.394112
796.507130	62907.400341	33.399130
797.192667	63010.132939	33.404148
797.565838	63114.662081	33.409165
798.131573	63231.055138	33.414183
799.143191	63337.742735	33.419200
799.327032	63441.647475	33.424218
799.744134	63559.324734	33.429236
800.712809	63678.706650	33.434253
801.443823	63813.190682	33.439271
802.698701	63910.556017	33.444288
803.839160	64028.122842	33.449306
804.618330	64142.216681	33.454324
805.830378	64239.028098	33.459341
806.549436	64353.651343	33.464359
807.285978	64465.269922	33.469376
808.354852	64561.651397	33.474394
809.084874	64675.174784	33.479412
809.691540	64787.126279	33.484429
810.444432	64898.434777	33.489447
810.969391	65001.614720	33.494464
811.743810	65119.450495	33.499482
812.394636	65235.910383	33.504500
813.293876	65339.226164	33.509517
813.891265	65474.684958	33.514535
814.266741	65595.440176	33.519552
815.057522	65721.898835	33.524570
816.032768	65855.919693	33.529588
817.210561	65970.109524	33.534605
817.603521	66107.837643	33.539623
819.491903	66195.690306	33.544640
820.710082	66306.076153	33.549658
821.216680	66424.835934	33.554676
822.312392	66528.308522	33.559693
823.054348	66630.088972	33.564711
823.935209	66749.528427	33.569728
825.043709	66844.200843	33.574746
825.235378	66964.741502	33.579764
825.884023	67073.897920	33.584781
826.951091	67191.589665	33.589799
827.533451	67301.984632	33.594816
828.380291	67416.142222	33.599834
829.001220	67530.729690	33.604852
829.719984	67642.621167	33.609869
830.358758	67772.834625	33.614887
831.438285	67870.740641	33.619904
832.669918	67980.861289	33.624922
833.600624	68079.981384	33.629940
834.943147	68154.390773	33.634957
836.045981	68260.165655	33.639975
836.850489	68335.492710	33.644992
837.567588	68438.942449	33.650010
838.012079	68540.383021	33.655028
838.891629	68633.988650	33.660045
839.377022	68736.409668	33.665063
840.295834	68840.194759	33.670080
840.785384	68952.301763	33.675098
841.432607	69056.050573	33.680116
842.240611	69175.971091	33.685133
842.744891	69291.491512	33.690151
843.400683	69419.335151	33.695168
844.065337	69540.147573	33.700186
844.934157	69683.137760	33.705204
845.993019	69803.406086	33.710221
846.367910	69934.934658	33.715239
846.795410	70071.431223	33.720256
847.312334	70203.608200	33.725274
847.996180	70358.640133	33.730292
848.824807	70501.054463	33.735309
850.051445	70656.188623	33.740327
850.895860	70801.061904	33.745344
852.053055	70947.680211	33.750362
852.617192	71097.508308	33.755380
853.891461	71231.811241	33.760397
854.455132	71395.299015	33.765415
855.344944	71526.872534	33.770432
856.350090	71672.882306	33.775450
857.590999	71809.047031	33.780468
858.985291	71941.475621	33.785485
860.586943	72080.263516	33.790503
861.610594	72197.332682	33.795520
862.824752	72324.241610	33.800538
863.523556	72446.019677	33.805556
864.235940	72560.650849	33.810573
864.890615	72679.794383	33.815591
865.991479	72793.527971	33.820608
867.688228	72896.679555	33.825626
868.908054	73001.333156	33.830644
870.643609	73086.482741	33.835661
871.741355	73174.001785	33.840679
872.369675	73264.577070	33.845696
873.386337	73354.804056	33.850714
874.189018	73463.247024	33.855732
875.011742	73531.260440	33.860749
875.257413	73644.735018	33.865767
876.291743	73743.858061	33.870784
876.501796	73839.873606	33.875802
876.825575	73943.990449	33.880820
877.806825	74067.305643	33.885837
878.701221	74177.286366	33.890855
879.635051	74280.102577	33.895872
880.177530	74383.338028	33.900890
880.936744	74514.869160	33.905908
881.330602	74642.104232	33.910925
881.855638	74765.226789	33.915943
882.686185	74903.591013	33.920960
883.596991	75033.342179	33.925978
884.359692	75164.731210	33.930996
885.318290	75293.040466	33.936013
885.911050	75438.542999	33.941031
886.678108	75585.086510	33.946048
887.506124	75730.046204	33.951066
888.226699	75867.764330	33.956084
888.904473	75990.432202	33.961101
889.810914	76125.578888	33.966119
890.335446	76261.181577	33.971136
891.661033	76399.087744	33.976154
892.458120	76541.091753	33.981172
893.599097	76680.978109	33.986189
894.624274	76804.712611	33.991207
895.949892	76928.404527	33.996224
897.351578	77046.816177	34.001242
898.373959	77182.177906	34.006260
899.427833	77296.682770	34.011277
899.830794	77407.652664	34.016295
900.649113	77544.087560	34.021312
902.015045	77662.717140	34.026330
902.512822	77783.628487	34.031348
903.616654	77915.344490	34.036365
904.292983	78052.141182	34.041383
905.279145	78166.535236	34.046400
906.376412	78284.573691	34.051418
907.219416	78418.985915	34.056436
908.180330	78552.165076	34.061453
909.269110	78676.702840	34.066471
910.095017	78803.479519	34.071488
911.453684	78917.423782	34.076506
912.263834	79045.716154	34.081524
913.302814	79161.200867	34.086541
914.286990	79301.711601	34.091559
914.957840	79421.793655	34.096576
915.819496	79552.635855	34.101594
916.972703	79687.213254	34.106612
917.501193	79807.706732	34.111629
918.448622	79932.009181	34.116647
919.027781	80080.277085	34.121664
919.814987	80216.385605	34.126682
920.669609	80364.964139	34.131700
921.191366	80492.483777	34.136717
922.386394	80643.044789	34.141735
923.234075	80786.977919	34.146752
924.261130	80924.164444	34.151770
925.011279	81078.900888	34.156788
925.998813	81214.925445	34.161805
927.406899	81356.195087	34.166823
928.160546	81511.092064	34.171840
929.211642	81637.803311	34.176858
930.655696	81778.652149	34.181876
931.810270	81911.015898	34.186893
932.610711	82048.120150	34.191911
933.598752	82174.022428	34.196928
934.758804	82290.287665	34.201946
935.502720	82426.258513	34.206964
936.444943	82561.824190	34.211981
937.808941	82676.684955	34.216999
938.589630	82809.077718	34.222016
940.021309	82933.164918	34.227034
941.311247	83059.091847	34.232052
942.076142	83162.527449	34.237069
942.852961	83295.062855	34.242087
943.580781	83411.841710	34.247104
944.359136	83536.147608	34.252122
944.839376	83671.555757	34.257140
945.624436	83792.907478	34.262157
947.444100	83914.202906	34.267175
948.124962	84047.808724	34.272192
949.596894	84154.048635	34.277210
950.678776	84278.947442	34.282228
951.014701	84400.433474	34.287245
952.064063	84522.181961	34.292263
952.704468	84647.415056	34.297280
954.049290	84753.501580	34.302298
954.710488	84875.062951	34.307316
955.653438	84992.288847	34.312333
956.421965	85110.480514	34.317351
957.038987	85230.722410	34.322368
957.722046	85359.950941	34.327386
958.007613	85504.683652	34.332404
959.026162	85631.947565	34.337421
959.713687	85775.369183	34.342439
960.288304	85935.102606	34.347456
961.025251	86073.361322	34.352474
961.642928	86239.170109	34.357492
962.247589	86405.678223	34.362509
963.984917	86549.861408	34.367527
965.893444	86685.386779	34.372544
967.063934	86820.914572	34.377562
968.619974	86962.605640	34.382580
969.920713	87099.246150	34.387597
971.168864	87225.879786	34.392615
972.055124	87361.204549	34.397632
972.974239	87486.571478	34.402650
974.228220	87619.761602	34.407668
974.597429	87764.462917	34.412685
975.794838	87888.248447	34.417703
976.640592	88032.543704	34.422720
977.141802	88161.457131	34.427738
977.810566	88305.776960	34.432756
978.199238	88473.132755	34.437773
978.968972	88619.102044	34.442791
979.233722	88798.490825	34.447808
980.592418	88957.153608	34.452826
981.262387	89142.369394	34.457844
982.058573	89312.726601	34.462861
983.125601	89486.881450	34.467879
983.633781	89662.041092	34.472896
984.820581	89851.587789	34.477914
986.069947	90041.499036	34.482932
988.114669	90180.736760	34.487949
990.173178	90332.547323	34.492967
991.173040	90495.500622	34.497984
992.128331	90652.115041	34.503002
993.202879	90798.996693	34.508020
993.605874	90961.355592	34.513037
994.450883	91129.490148	34.518055
994.993882	91287.942454	34.523072
995.861796	91452.569490	34.528090
996.677542	91637.236372	34.533108
997.665377	91803.769925	34.538125
998.843807	91981.867379	34.543143
999.547754	92168.835146	34.548160
1000.479506	92345.210290	34.553178
1001.790412	92536.283039	34.558196
1002.521101	92707.384110	34.563213
1003.470368	92881.241378	34.568231
1004.635759	93071.171529	34.573248
1005.018193	93253.707187	34.578266
1005.952545	93445.710045	34.583284
1007.085456	93631.308187	34.588301
1008.556266	93820.573534	34.593319
1009.943549	93994.714584	34.598336
1010.776469	94174.600460	34.603354
1012.072553	94373.880257	34.608372
1013.065377	94531.260546	34.613389
1014.566652	94692.209989	34.618407
1015.380374	94876.756343	34.623424
1016.251972	95041.432500	34.628442
1017.711741	95215.418392	34.633460
1018.501034	95381.186447	34.638477
1019.696806	95542.546379	34.643495
1020.331149	95704.468455	34.648512
1020.867613	95869.946075	34.653530
1022.107184	96033.751606	34.658548
1023.202678	96200.582346	34.663565
1024.088294	96374.804160	34.668583
1024.505989	96552.471963	34.673600
1025.644579	96727.452069	34.678618
1026.330646	96900.780031	34.683636
1027.557238	97085.122861	34.688653
1029.048368	97244.394232	34.693671
1030.107098	97440.617335	34.698688
1030.841345	97604.801553	34.703706
1031.808545	97791.287737	34.708724
1032.681548	97975.106835	34.713741
1034.001705	98151.333056	34.718759
1036.035223	98317.016657	34.723776
1037.635282	98480.614254	34.728794
1038.943127	98641.488432	34.733812
1039.650753	98820.802133	34.738829
1040.682701	98974.703495	34.743847
1041.785332	99148.851932	34.748864
1042.649118	99316.976285	34.753882
1043.765819	99474.949964	34.758900
1044.610904	99642.313571	34.763917
1045.387400	99810.107440	34.768935
1046.402401	100003.186157	34.773952
1047.766081	100158.128888	34.778970
1049.539368	100316.208362	34.783988
1051.169337	100460.143943	34.789005
1052.488283	100609.500317	34.794023
1053.492115	100776.383072	34.799040
1054.374151	100910.884921	34.804058
1055.514273	101070.783007	34.809076
1056.201795	101229.015767	34.814093
1056.898176	101399.587414	34.819111
1058.200413	101561.380152	34.824128
1058.523173	101729.160326	34.829146
1059.975400	101875.216237	34.834164
1060.714486	102053.427019	34.839181
1061.611427	102224.129347	34.844199
1063.142064	102389.017300	34.849216
1064.238351	102549.362420	34.854234
1065.316654	102713.769972	34.859252
1065.861141	102896.007550	34.864269
1067.863345	103037.312984	34.869287
1069.261319	103189.071058	34.874304
1070.153547	103365.556143	34.879322
1071.583059	103524.440383	34.884340
1072.235047	103684.315068	34.889357
1073.828982	103833.942466	34.894375
1075.039822	103977.162912	34.899392
1075.886124	104142.327030	34.904410
1077.167658	104287.101474	34.909428
1077.801075	104449.073451	34.914445
1078.649449	104613.043498	34.919463
1080.445300	104754.449380	34.924480
1081.264830	104923.744987	34.929498
1082.348662	105062.686633	34.934516
1083.461568	105229.111708	34.939533
1084.628678	105378.064951	34.944551
1085.503733	105533.994616	34.949568
1086.036382	105713.334821	34.954586
1087.292498	105856.273183	34.959604
1088.098828	106028.668248	34.964621
1088.656498	106190.277259	34.969639
1089.341367	106367.342505	34.974656
1089.829032	106563.020718	34.979674
1090.963081	106719.902524	34.984692
1091.688171	106917.013292	34.989709
1092.107947	107101.156272	34.994727
1092.978960	107291.925895	34.999744
1094.042803	107478.890825	35.004762
1095.103054	107673.710158	35.009780
1096.194638	107872.755993	35.014797
1097.507386	108069.563013	35.019815
1098.568417	108270.440700	35.024832
1099.213156	108480.862559	35.029850
1100.370463	108691.594102	35.034868
1100.927177	108923.223856	35.039885
1101.588705	109127.910382	35.044903
1102.967990	109349.123240	35.049920
1104.502995	109577.341962	35.054938
1105.968642	109783.129365	35.059956
1106.993074	110011.714717	35.064973
1108.039209	110245.517031	35.069991
1109.270095	110465.382910	35.075008
1110.137175	110697.166695	35.080026
1111.274035	110933.417326	35.085044
1112.352814	111146.296410	35.090061
1113.190158	111385.716487	35.095079
1114.397351	111615.944590	35.100096
1115.679241	111847.923059	35.105114
1116.802494	112076.851512	35.110132
1118.121427	112314.034117	35.115149
1119.879410	112543.634416	35.120167
1121.496373	112757.425298	35.125184
1122.881815	112967.683748	35.130202
1124.605184	113173.631613	35.135220
1125.614255	113380.408338	35.140237
1126.910492	113593.523920	35.145255
1128.024443	113809.154199	35.150272
1129.131941	114018.250395	35.155290
1130.055596	114216.369710	35.160308
1131.006245	114446.423166	35.165325
1132.290161	114647.070451	35.170343
1133.394495	114865.814326	35.175360
1134.206311	115089.054938	35.180378
1135.903193	115292.603193	35.185396
1137.264251	115486.237910	35.190413
1139.168447	115687.373059	35.195431
1140.960875	115871.412128	35.200448
1142.283896	116055.200492	35.205466
1143.814826	116235.649058	35.210484
1144.841357	116418.424521	35.215501
1146.055705	116588.602084	35.220519
1146.572096	116772.629640	35.225536
1147.942862	116971.556181	35.230554
1149.029231	117153.515672	35.235572
1149.511729	117345.534454	35.240589
1150.390102	117542.354413	35.245607
1151.328886	117733.933076	35.250624
1152.045108	117943.541218	35.255642
1153.169458	118152.044582	35.260660
1154.543470	118364.879487	35.265677
1155.375235	118574.739269	35.270695
1156.632546	118776.167874	35.275712
1157.580151	119001.190813	35.280730
1158.588521	119211.317527	35.285748
1159.436868	119423.626209	35.290765
1160.709132	119644.077153	35.295783
1161.791201	119874.647206	35.300800
1162.645576	120106.827889	35.305818
1163.876969	120327.455520	35.310836
1164.911359	120555.061161	35.315853
1165.496682	120787.494447	35.320871
1166.561763	121010.562269	35.325888
1168.518426	121212.830116	35.330906
1170.635605	121403.110920	35.335924
1172.037080	121587.720166	35.340941
1173.104278	121806.054532	35.345959
1174.842593	121991.218968	35.350976
1175.473441	122180.039479	35.355994
1176.830949	122387.787244	35.361012
1177.490236	122593.091969	35.366029
1178.495985	122792.841220	35.371047
1179.731052	123001.868071	35.376064
1180.332899	123223.939383	35.381082
1181.295748	123443.088801	35.386100
1182.136062	123674.831218	35.391117
1183.100874	123899.673654	35.396135
1184.633770	124129.835273	35.401152
1186.229146	124355.020611	35.406170
1187.382035	124570.978767	35.411188
1188.776630	124799.723673	35.416205
1189.967603	125036.627403	35.421223
1190.891866	125262.627374	35.426240
1192.432298	125486.943175	35.431258
1193.840750	125707.898637	35.436276
1195.090220	125940.300778	35.441293
1196.238094	126167.170445	35.446311
1197.485969	126397.219076	35.451328
1198.510204	126625.544714	35.456346
1199.588548	126858.527123	35.461364
1201.094630	127091.795587	35.466381
1201.846866	127330.678142	35.471399
1202.896656	127563.569265	35.476416
1203.844484	127808.443502	35.481434
1205.462090	128051.193917	35.486452
1207.158109	128286.138512	35.491469
1207.893098	128532.790064	35.496487
1208.890915	128767.954982	35.501504
1210.064960	129003.548894	35.506522
1211.449292	129246.904933	35.511540
1212.433232	129504.575635	35.516557
1213.883592	129753.298939	35.521575
1214.713888	130009.503532	35.526592
1215.968665	130244.561186	35.531610
1217.682501	130494.818658	35.536628
1219.271640	130743.146695	35.541645
1220.998521	130981.224781	35.546663
1222.481705	131205.490401	35.551680
1223.616061	131452.707610	35.556698
1225.281444	131668.250888	35.561716
1226.622581	131886.473078	35.566733
1227.474348	132125.642284	35.571751
1229.181879	132344.339550	35.576768
1230.275068	132581.621636	35.581786
1231.254943	132800.175948	35.586804
1232.370576	133027.823674	35.591821
1233.386693	133281.019887	35.596839
1234.975554	133513.055088	35.601856
1235.672124	133733.754189	35.606874
1236.724585	133965.716408	35.611892
1239.694075	134173.227173	35.616909
1241.423137	134351.989944	35.621927
1243.659164	134551.498317	35.626944
1244.824476	134749.511280	35.631962
1246.355605	134949.075074	35.636980
1247.603540	135141.105863	35.641997
1248.313092	135334.545090	35.647015
1249.648959	135524.395817	35.652032
1250.629232	135716.765768	35.657050
1251.167554	135905.533321	35.662068
1252.244807	136106.675086	35.667085
1253.078930	136301.062986	35.672103
1254.062927	136490.711182	35.677120
1254.620958	136694.008727	35.682138
1255.438384	136921.568260	35.687156
1256.174917	137143.551721	35.692173
1256.909160	137376.541630	35.697191
1258.102441	137606.351264	35.702208
1258.725390	137854.526007	35.707226
1259.804789	138117.384885	35.712244
1261.074668	138376.309435	35.717261
1262.019607	138645.888912	35.722279
1263.073127	138905.068814	35.727296
1264.369170	139169.092020	35.732314
1265.097048	139447.360700	35.737332
1266.382404	139732.411677	35.742349
1267.448463	140016.220673	35.747367
1269.739274	140270.300083	35.752384
1272.023529	140545.899225	35.757402
1273.352883	140810.360884	35.762420
1274.944006	141077.291933	35.767437
1275.751523	141356.425374	35.772455
1277.119281	141605.050065	35.777472
1278.434027	141883.229191	35.782490
1279.582025	142162.389086	35.787508
1280.961328	142427.222729	35.792525
1281.904716	142716.514155	35.797543
1283.200217	142977.942233	35.802560
1284.706723	143241.556509	35.807578
1286.369361	143515.443486	35.812596
1287.982411	143776.774452	35.817613
1289.391318	144044.785692	35.822631
1291.658805	144295.310130	35.827648
1293.187760	144535.940461	35.832666
1294.764259	144780.343487	35.837684
1296.075401	145036.039993	35.842701
1297.421034	145284.999039	35.847719
1298.810311	145527.295056	35.852736
1299.767641	145766.493725	35.857754
1300.846609	146027.942261	35.862772
1301.670084	146277.856791	35.867789
1302.999993	146545.595720	35.872807
1303.755236	146818.795804	35.877824
1304.612657	147083.002491	35.882842
1306.190454	147350.313394	35.887860
1307.641672	147619.232407	35.892877
1309.034202	147895.214273	35.897895
1310.285815	148162.153846	35.902912
1311.516869	148435.744216	35.907930
1312.533326	148711.287082	35.912948
1313.936569	148989.380756	35.917965
1315.233575	149277.830259	35.922983
1316.509654	149554.579519	35.928000
1317.968875	149827.724142	35.933018
1318.757188	150110.087710	35.938036
1320.364091	150404.531886	35.943053
1321.637444	150692.856878	35.948071
1322.720358	150967.505208	35.953088
1324.163179	151269.123867	35.958106
1325.179035	151553.578952	35.963124
1326.561014	151846.460907	35.968141
1327.893091	152152.150945	35.973159
1329.245773	152438.180630	35.978176
1330.679822	152738.772520	35.983194
1331.569358	153034.243664	35.988212
1333.581694	153324.750011	35.993229
1335.015382	153618.905573	35.998247
1335.906876	153911.136135	36.003264
1337.558189	154173.854494	36.008282
1339.120077	154450.770323	36.013300
1340.521456	154703.893592	36.018317
1341.975566	154984.687071	36.023335
1343.484740	155250.670762	36.028352
1345.135082	155499.445454	36.033370
1347.227794	155754.047076	36.038388
1349.345240	155982.756849	36.043405
1350.633784	156237.735366	36.048423
1351.800008	156498.469286	36.053440
1353.292982	156724.559226	36.058458
1354.107002	156998.039516	36.063476
1355.566234	157238.104176	36.068493
1356.694714	157486.444870	36.073511
1357.895579	157745.100968	36.078528
1359.266908	158002.119584	36.083546
1360.457327	158254.197039	36.088564
1361.867905	158513.660767	36.093581
1363.281158	158779.430472	36.098599
1364.710088	159039.021437	36.103616
1366.113679	159300.559182	36.108634
1366.998434	159564.531130	36.113652
1368.415114	159831.601182	36.118669
1369.831816	160117.093056	36.123687
1371.159701	160380.641988	36.128704
1372.719234	160648.784847	36.133722
1373.207149	160935.234972	36.138740
1374.582117	161220.475054	36.143757
1375.891638	161518.972553	36.148775
1376.817236	161813.260219	36.153792
1377.966823	162112.689154	36.158810
1378.977215	162430.018798	36.163828
1380.273271	162741.049125	36.168845
1381.348657	163057.002648	36.173863
1382.886392	163379.111571	36.178880
1385.154195	163675.220815	36.183898
1386.298370	163989.051262	36.188916
1387.931205	164308.474611	36.193933
1389.722053	164614.006994	36.198951
1390.789591	164937.880142	36.203968
1391.834489	165251.901250	36.208986
1393.325413	165567.195946	36.214004
1394.661874	165875.096118	36.219021
1396.924117	166178.709476	36.224039
1398.478196	166489.306005	36.229056
1399.909223	166771.123284	36.234074
1401.121810	167087.794567	36.239092
1402.614395	167402.328389	36.244109
1403.820226	167705.784173	36.249127
1405.239605	168015.677879	36.254144
1406.560508	168334.421182	36.259162
1407.928781	168644.987540	36.264180
1410.375115	168931.193627	36.269197
1412.457647	169224.059726	36.274215
1413.745780	169510.701760	36.279232
1415.558891	169804.326696	36.284250
1416.505521	170104.301445	36.289268
1417.785237	170406.481872	36.294285
1419.110305	170681.096050	36.299303
1420.307218	170996.604968	36.304320
1421.405273	171290.256041	36.309338
1422.576979	171606.547383	36.314356
1423.726518	171908.974979	36.319373
1425.086520	172220.468236	36.324391
1425.855733	172548.024653	36.329408
1427.346872	172870.934014	36.334426
1428.526793	173188.008902	36.339444
1429.432761	173521.196566	36.344461
1431.019963	173830.277406	36.349479
1432.246372	174147.769884	36.354496
1433.488188	174473.688220	36.359514
1434.718305	174784.877353	36.364532
1436.095877	175116.348713	36.369549
1437.738676	175442.905484	36.374567
1438.673108	175788.718662	36.379584
1440.761603	176102.135144	36.384602
1441.822678	176450.876387	36.389620
1443.208775	176792.637339	36.394637
1444.624521	177132.720601	36.399655
1445.842127	177475.453261	36.404672
1447.462679	177821.941819	36.409690
1449.158861	178174.880115	36.414708
1450.369507	178514.587964	36.419725
1452.181390	178849.376221	36.424743
1453.524924	179219.944891	36.429760
1456.725533	179516.104298	36.434778
1458.819583	179826.878343	36.439796
1460.492589	180146.810987	36.444813
1462.122271	180477.159998	36.449831
1463.736474	180792.334324	36.454848
1464.898802	181106.645963	36.459866
1467.085358	181408.809314	36.464884
1468.746771	181717.102495	36.469901
1469.998043	182025.680960	36.474919
1470.937470	182334.693482	36.479936
1472.800583	182631.561241	36.484954
1473.888036	182954.451001	36.489972
1475.215926	183265.638757	36.494989
1476.730016	183588.360459	36.500007
1477.855660	183900.676875	36.505024
1479.321321	184227.040515	36.510042
1480.970258	184555.343270	36.515060
1482.251341	184875.394968	36.520077
1483.906988	185210.910111	36.525095
1484.753672	185565.308288	36.530112
1486.654333	185895.240416	36.535130
1487.861849	186234.034454	36.540148
1489.930426	186544.636598	36.545165
1492.067358	186853.185602	36.550183
1494.075762	187184.377007	36.555200
1495.980720	187485.605690	36.560218
1497.131142	187799.933210	36.565236
1498.400628	188119.980314	36.570253
1500.184475	188411.472638	36.575271
1501.006062	188752.325864	36.580288
1502.336043	189058.824157	36.585306
1503.813503	189392.096374	36.590324
1505.307396	189714.933448	36.595341
1507.351476	190025.089149	36.600359
1509.014570	190329.558994	36.605376
1510.558214	190650.184318	36.610394
1511.703972	190970.648564	36.615412
1513.199658	191308.308262	36.620429
1514.386091	191621.089334	36.625447
1516.015438	191949.222617	36.630464
1517.487769	192265.539716	36.635482
1519.022258	192585.339219	36.640500
1520.189104	192915.762965	36.645517
1521.812798	193240.210129	36.650535
1523.150890	193588.242134	36.655552
1524.386132	193920.995892	36.660570
1526.152638	194245.602568	36.665588
1527.840865	194572.508956	36.670605
1529.642763	194890.892681	36.675623
1531.161944	195225.828239	36.680640
1532.341313	195543.619794	36.685658
1533.949509	195869.619446	36.690676
1535.038265	196178.148984	36.695693
1536.536325	196499.764810	36.700711
1537.735043	196830.597702	36.705728
1539.189154	197148.478911	36.710746
1539.987649	197485.640059	36.715764
1541.231694	197839.639926	36.720781
1542.976088	198167.342686	36.725799
1543.868017	198538.302318	36.730816
1545.627676	198892.438620	36.735834
1546.776104	199248.721701	36.740852
1548.131904	199622.226198	36.745869
1549.475572	199984.524234	36.750887
1550.549885	200387.597564	36.755904
1551.957873	200773.249936	36.760922
1553.749492	201164.744910	36.765940
1554.716522	201561.507464	36.770957
1556.815175	201960.916848	36.775975
1558.089162	202366.495389	36.780992
1560.050276	202760.510665	36.786010
1561.642855	203169.659756	36.791028
1562.969746	203564.571333	36.796045
1564.801732	203974.015637	36.801063
1566.449360	204386.197094	36.806080
1568.206122	204781.603052	36.811098
1569.819371	205184.944996	36.816116
1571.772479	205596.321039	36.821133
1574.164707	205967.847067	36.826151
1576.728419	206343.333534	36.831168
1578.474825	206729.508076	36.836186
1580.355677	207094.762757	36.841204
1581.691927	207483.967253	36.846221
1583.105233	207850.750169	36.851239
1584.437025	208247.476079	36.856256
1585.888391	208630.077369	36.861274
1587.705847	209013.204201	36.866292
1588.899782	209404.651115	36.871309
1590.390545	209796.101758	36.876327
1591.911566	210192.780775	36.881344
1593.273947	210591.138618	36.886362
1595.078022	210991.000055	36.891380
1596.669559	211395.863382	36.896397
1598.305118	211790.728111	36.901415
1599.963983	212175.914952	36.906432
1601.995458	212571.073561	36.911450
1603.841788	212966.086777	36.916468
1605.521638	213363.973677	36.921485
1607.114352	213741.153213	36.926503
1608.489495	214148.592277	36.931520
1610.217618	214526.489350	36.936538
1611.909274	214920.495658	36.941556
1613.425076	215324.335946	36.946573
1615.740477	215701.429960	36.951591
1617.272495	216087.188245	36.956608
1619.191780	216472.808058	36.961626
1621.612845	216833.812798	36.966644
1623.470691	217203.267635	36.971661
1625.160381	217552.332001	36.976679
1627.275975	217917.175531	36.981696
1628.315468	218290.045914	36.986714
1629.991875	218703.804834	36.991732
1631.229806	219074.791436	36.996749
1632.464010	219449.437373	37.001767
1633.422688	219833.222727	37.006784
1635.057595	220210.243626	37.011802
1636.404503	220597.320401	37.016820
1637.652467	220986.523037	37.021837
1639.251511	221370.589500	37.026855
1640.233356	221762.150216	37.031872
1642.012007	222144.716756	37.036890
1643.895244	222514.745788	37.041908
1645.101464	222915.036319	37.046925
1646.789490	223280.121988	37.051943
1649.800324	223636.888309	37.056960
1652.089634	223992.835056	37.061978
1654.115547	224336.634751	37.066996
1655.602798	224696.856137	37.072013
1657.260088	225057.710990	37.077031
1658.641282	225406.192173	37.082048
1660.410152	225774.625298	37.087066
1661.969970	226134.051792	37.092084
1663.571121	226505.080228	37.097101
1665.490062	226860.639697	37.102119
1667.589953	227209.566386	37.107136
1669.444397	227577.965522	37.112154
1671.046037	227930.075247	37.117172
1672.537927	228306.918359	37.122189
1674.010762	228652.345725	37.127207
1675.485117	229027.619047	37.132224
1676.891570	229398.103998	37.137242
1678.666239	229767.741831	37.142260
1679.977380	230157.726729	37.147277
1680.956239	230548.758198	37.152295
1682.256378	230939.788581	37.157312
1683.358964	231354.526091	37.162330
1684.899250	231762.664620	37.167348
1686.075590	232196.442997	37.172365
1687.626960	232631.608652	37.177383
1688.845963	233062.309059	37.182400
1690.053190	233512.317452	37.187418
1691.990766	233968.633171	37.192436
1693.090763	234419.398558	37.197453
1695.237263	234878.019388	37.202471
1697.792848	235317.421429	37.207488
1699.815511	235766.031691	37.212506
1701.841567	236222.720282	37.217524
1703.611593	236669.774360	37.222541
1705.358764	237113.581967	37.227559
1707.591870	237564.651616	37.232576
1708.969008	238002.248290	37.237594
1710.780969	238449.528571	37.242612
1712.827781	238879.675732	37.247629
1715.422729	239298.480390	37.252647
1717.355336	239740.866655	37.257664
1719.029070	240162.619368	37.262682
1720.951898	240576.279411	37.267700
1722.958710	241003.795996	37.272717
1724.689484	241411.773910	37.277735
1726.550769	241841.195954	37.282752
1727.534797	242268.502764	37.287770
1729.046207	242699.965570	37.292788
1730.533159	243139.511175	37.297805
1731.650223	243582.776573	37.302823
1733.184224	244030.698856	37.307840
1734.335164	244491.284791	37.312858
1736.061801	244949.947594	37.317876
1737.398565	245419.497026	37.322893
1738.863559	245897.485197	37.327911
1740.419431	246365.552140	37.332928
1741.591378	246854.030766	37.337946
1743.658919	247334.309757	37.342964
1745.311040	247820.780101	37.347981
1747.132451	248312.913488	37.352999
1749.100849	248802.610072	37.358016
1750.745165	249303.461883	37.363034
1752.715005	249770.246119	37.368052
1754.354358	250263.783985	37.373069
1756.294892	250709.083252	37.378087
1758.790630	251156.704688	37.383104
1761.786814	251589.332423	37.388122
1764.108758	252025.526617	37.393140
1765.687191	252454.603975	37.398157
1767.578485	252881.775654	37.403175
1769.621863	253311.996363	37.408192
1771.592780	253734.608400	37.413210
1773.806723	254125.426658	37.418228
1775.531225	254539.849259	37.423245
1777.108172	254960.012176	37.428263
1779.421524	255380.434894	37.433280
1780.757111	255797.615100	37.438298
1782.597939	256213.365783	37.443316
1783.788052	256646.320390	37.448333
1785.182099	257076.497976	37.453351
1787.051246	257518.308252	37.458368
1788.581141	257967.135136	37.463386
1790.147195	258404.321469	37.468404
1790.964138	258870.311804	37.473421
1792.470904	259321.987978	37.478439
1793.925072	259805.604843	37.483456
1795.400346	260288.735601	37.488474
1796.746529	260781.261486	37.493492
1798.531818	261283.393574	37.498509
1799.898608	261797.635816	37.503527
1801.993329	262299.462691	37.508544
1803.472019	262818.233459	37.513562
1805.465615	263317.917475	37.518580
1807.596669	263826.800029	37.523597
1809.800593	264331.986876	37.528615
1811.470751	264844.374444	37.533632
1814.010720	265330.783153	37.538650
1816.313795	265838.543961	37.543668
1818.135292	266344.377019	37.548685
1820.163731	266851.445731	37.553703
1822.077098	267357.110446	37.558720
1823.385638	267878.573643	37.563738
1825.110862	268382.033012	37.568756
1826.535746	268901.469170	37.573773
1828.086410	269408.334910	37.578791
1829.744255	269948.866825	37.583808
1831.595328	270481.364243	37.588826
1833.503283	271007.627857	37.593844
1835.434787	271541.583958	37.598861
1837.200365	272075.998506	37.603879
1839.234793	272606.963911	37.608896
1841.051851	273139.793338	37.613914
1844.033208	273656.680107	37.618932
1846.456333	274163.624022	37.623949
1848.448545	274662.687119	37.628967
1850.748502	275168.912934	37.633984
1852.552332	275680.376392	37.639002
1855.480719	276165.844390	37.644020
1857.635836	276643.615071	37.649037
1859.561484	277129.526080	37.654055
1861.570275	277592.585657	37.659072
1862.662946	278078.124117	37.664090
1864.846439	278554.463809	37.669108
1867.337052	279023.994841	37.674125
1869.176387	279500.821120	37.679143
1871.625521	279941.322317	37.684160
1873.775572	280389.238525	37.689178
1875.546273	280845.065554	37.694196
1877.430395	281295.614631	37.699213
1878.989405	281758.078989	37.704231
1880.731315	282200.698627	37.709248
1881.802482	282644.012106	37.714266
1884.034122	283075.346696	37.719284
1885.297175	283515.984624	37.724301
1886.903931	283964.794878	37.729319
1888.655470	284401.107942	37.734336
1890.054246	284863.565378	37.739354
1891.727612	285334.384101	37.744372
1893.223997	285795.451163	37.749389
1894.428488	286284.709627	37.754407
1896.381341	286759.847096	37.759424
1898.180593	287241.358719	37.764442
1900.483686	287717.045088	37.769460
1903.046452	288200.917011	37.774477
1904.819977	288685.552549	37.779495
1906.634900	289170.636849	37.784512
1908.094101	289668.478501	37.789530
1909.792827	290158.049088	37.794548
1911.623174	290674.241320	37.799565
1912.692132	291191.573185	37.804583
1914.475050	291714.703535	37.809600
1917.097839	292205.155633	37.814618
1919.315024	292727.473661	37.819636
1921.285219	293246.502877	37.824653
1922.433760	293794.570500	37.829671
1924.303256	294320.774572	37.834688
1925.838226	294861.306121	37.839706
1927.874726	295407.162581	37.844724
1929.936790	295960.606694	37.849741
1931.602295	296508.551114	37.854759
1933.703565	297059.595901	37.859776
1935.433670	297634.345673	37.864794
1937.533118	298197.678218	37.869812
1939.165661	298755.776505	37.874829
1941.404637	299322.407374	37.879847
1943.367843	299881.918304	37.884864
1945.122849	300466.808094	37.889882
1946.869973	301030.996308	37.894900
1949.026900	301621.578530	37.899917
1950.423249	302205.145881	37.904935
1952.344584	302783.899180	37.909952
1954.246661	303390.005383	37.914970
1956.108765	303995.352395	37.919988
1958.403447	304588.128702	37.925005
1960.384224	305183.848255	37.930023
1962.271550	305781.814266	37.935040
1964.543677	306376.462054	37.940058
1966.682057	306975.419950	37.945076
1969.117693	307556.445655	37.950093
1971.042937	308160.941586	37.955111
1972.812552	308762.868521	37.960128
1974.917253	309355.771157	37.965146
1976.705326	309965.381384	37.970164
1979.234548	310574.153787	37.975181
1981.111062	311161.265512	37.980199
1983.703993	311738.553851	37.985216
1986.247969	312312.316180	37.990234
1988.903536	312887.452634	37.995252
1991.424650	313427.333939	38.000269
1993.575540	313997.136346	38.005287
1995.829786	314555.490052	38.010304
1997.928048	315102.590407	38.015322
1998.929824	315667.363958	38.020340
2001.182579	316220.271186	38.025357
2002.688447	316804.480578	38.030375
2004.478421	317366.851002	38.035392
2005.962745	317939.983292	38.040410
2007.727677	318503.009114	38.045428
2009.462339	319084.673612	38.050445
2011.001219	319656.691032	38.055463
2013.147289	320218.395895	38.060480
2015.075264	320789.882637	38.065498
2016.786885	321366.630941	38.070516
2018.555796	321930.237397	38.075533
2020.070874	322507.363738	38.080551
2022.534777	323074.857638	38.085568
2025.061344	323649.978921	38.090586
2027.046103	324228.307496	38.095604
2029.202412	324801.499072	38.100621
2031.177112	325375.020103	38.105639
2033.355048	325962.314529	38.110656
2035.989133	326532.186997	38.115674
2038.747987	327094.696060	38.120692
2041.277277	327659.827523	38.125709
2043.272014	328212.931317	38.130727
2045.614578	328783.414771	38.135744
2047.575182	329338.925745	38.140762
2049.682360	329893.975734	38.145780
2052.155299	330462.466614	38.150797
2053.933417	331014.919882	38.155815
2055.645664	331584.363032	38.160832
2057.862201	332149.401514	38.165850
2059.722097	332725.612744	38.170868
2061.951094	333281.346217	38.175885
2063.677072	333868.179517	38.180903
2065.606894	334453.018258	38.185920
2067.636518	335027.349910	38.190938
2069.296595	335605.645886	38.195956
2071.223294	336202.829297	38.200973
2072.960332	336793.310290	38.205991
2074.873777	337402.438958	38.211008
2076.985473	338004.141009	38.216026
2079.310425	338599.911844	38.221044
2082.277945	339199.250589	38.226061
2084.532381	339796.948522	38.231079
2086.548266	340393.815810	38.236096
2088.378054	341002.053072	38.241114
2089.699727	341612.828964	38.246132
2091.778190	342230.833556	38.251149
2093.026108	342868.232553	38.256167
2094.652944	343516.195854	38.261184
2096.590905	344152.779134	38.266202
2098.006015	344813.044834	38.271220
2099.895315	345467.715675	38.276237
2101.727065	346146.219350	38.281255
2103.416933	346837.985172	38.286272
2105.559732	347526.544454	38.291290
2106.620102	348224.205660	38.296308
2110.338660	348904.972432	38.301325
2114.371386	349551.771497	38.306343
2117.126727	350202.883353	38.311360
2119.275953	350871.926494	38.316378
2121.269219	351536.671251	38.321396
2123.354410	352186.088559	38.326413
2125.726707	352849.964542	38.331431
2127.320240	353512.766274	38.336448
2129.195956	354175.359188	38.341466
2130.835991	354841.508086	38.346484
2133.041368	355503.188940	38.351501
2135.244528	356193.558869	38.356519
2137.179540	356859.983012	38.361536
2139.009194	357535.777035	38.366554
2141.200821	358227.257485	38.371572
2143.889588	358901.441472	38.376589
2145.872507	359585.220290	38.381607
2147.521809	360267.368179	38.386624
2150.146191	360935.998245	38.391642
2152.323820	361600.403177	38.396660
2154.630490	362243.819354	38.401677
2156.746195	362893.929169	38.406695
2159.387979	363533.387571	38.411712
2162.731576	364138.242237	38.416730
2165.694245	364753.399677	38.421748
2168.779639	365350.261444	38.426765
2171.281226	365943.658688	38.431783
2172.937012	366551.012018	38.436800
2174.955504	367143.404967	38.441818
2177.158921	367747.401917	38.446836
2179.594183	368335.293642	38.451853
2181.541480	368946.517953	38.456871
2183.019712	369548.906095	38.461888
2184.968546	370155.265456	38.466906
2187.123849	370779.641072	38.471924
2189.657221	371378.299732	38.476941
2191.450913	372004.768766	38.481959
2193.593399	372616.838772	38.486976
2195.334110	373258.538836	38.491994
2197.171755	373903.813095	38.497012
2198.799971	374551.773384	38.502029
2200.676520	375214.010688	38.507047
2202.292171	375878.865565	38.512064
2204.377399	376554.941656	38.517082
2205.825638	377262.151473	38.522100
2208.335468	377940.286427	38.527117
2210.420739	378637.041543	38.532135
2212.441580	379356.160128	38.537152
2214.334578	380065.420114	38.542170
2216.274814	380792.991558	38.547188
2218.788472	381500.572338	38.552205
2221.208113	382236.071989	38.557223
2223.805314	382960.496040	38.562240
2226.034484	383672.134804	38.567258
2228.281549	384414.207260	38.572276
2230.540849	385138.689949	38.577293
2233.009815	385872.350972	38.582311
2235.361082	386609.107972	38.587328
2237.375753	387358.402777	38.592346
2239.440098	388094.209637	38.597364
2242.216325	388821.693412	38.602381
2244.494389	389563.363387	38.607399
2246.624237	390307.550075	38.612416
2249.101206	391046.465042	38.617434
2251.634827	391796.912570	38.622452
2253.460001	392540.082160	38.627469
2255.519624	393294.855421	38.632487
2257.278390	394064.209304	38.637504
2259.562368	394831.074506	38.642522
2261.047264	395603.450835	38.647540
2263.033836	396381.478118	38.652557
2265.623994	397174.111169	38.657575
2266.868760	397981.239211	38.662592
2269.249905	398768.364354	38.667610
2271.151618	399586.009859	38.672628
2273.618031	400382.859992	38.677645
2276.071100	401194.920808	38.682663
2278.156644	402017.839974	38.687680
2280.555189	402822.591018	38.692698
2282.744921	403649.829945	38.697716
2285.768662	404456.408173	38.702733
2288.231873	405266.527075	38.707751
2290.501452	406074.627524	38.712768
2293.556704	406880.016021	38.717786
2296.204213	407666.775837	38.722804
2298.726687	408451.836378	38.727821
2301.399893	409244.373923	38.732839
2303.776144	410006.080992	38.737856
2306.198357	410754.864622	38.742874
2308.201888	411516.185348	38.747892
2310.725943	412252.801728	38.752909
2314.053570	412979.994213	38.757927
2316.900467	413701.977404	38.762944
2319.750563	414419.887661	38.767962
2322.256806	415138.620253	38.772980
2324.910415	415843.910272	38.777997
2327.109299	416542.569769	38.783015
2329.069630	417253.913212	38.788032
2331.108132	417986.472784	38.793050
2332.978744	418689.281924	38.798068
2335.111517	419422.671404	38.803085
2337.433420	420148.664694	38.808103
2339.605901	420891.451140	38.813120
2341.441893	421620.901004	38.818138
2345.000625	422341.638875	38.823156
2348.218562	423043.598696	38.828173
2350.753911	423767.376097	38.833191
2352.814705	424491.134686	38.838208
2354.841978	425205.357750	38.843226
2356.751956	425955.581682	38.848244
2358.650762	426704.670527	38.853261
2360.459272	427456.991763	38.858279
2362.021756	428224.114604	38.863296
2364.011447	429010.280685	38.868314
2367.181126	429761.293162	38.873332
2370.269156	430518.826350	38.878349
2372.870319	431289.527562	38.883367
2374.670556	432052.084205	38.888384
2377.269790	432830.885879	38.893402
2379.557660	433613.560194	38.898420
2382.352566	434377.649099	38.903437
2384.823632	435162.569715	38.908455
2386.900393	435936.494748	38.913472
2389.206727	436721.794543	38.918490
2391.445044	437516.340588	38.923508
2393.090134	438333.174429	38.928525
2395.496406	439124.650832	38.933543
2397.472177	439940.360216	38.938560
2399.621156	440759.149007	38.943578
2401.944086	441585.469601	38.948596
2403.986914	442416.663461	38.953613
2406.010741	443245.957262	38.958631
2407.897025	444116.023463	38.963648
2410.864386	444967.916049	38.968666
2413.183033	445817.757610	38.973684
2415.846501	446664.777353	38.978701
2418.443064	447521.741056	38.983719
2420.909759	448394.019935	38.988736
2423.158558	449253.299184	38.993754
2425.559758	450109.230990	38.998772
2428.023822	450978.370153	39.003789
2430.366899	451845.116498	39.008807
2433.077807	452733.919037	39.013824
2435.671029	453581.839536	39.018842
2438.614937	454467.900353	39.023860
2440.624724	455334.608091	39.028877
2443.582366	456197.128500	39.033895
2445.669957	457066.987211	39.038912
2448.133629	457939.426985	39.043930
2450.406353	458811.810487	39.048948
2452.560732	459693.984626	39.053965
2454.942527	460566.628751	39.058983
2457.318346	461458.649178	39.064000
2460.047622	462338.995220	39.069018
2462.475897	463214.650972	39.074036
2465.088160	464068.148375	39.079053
2468.206999	464894.432880	39.084071
2472.036277	465688.116468	39.089088
2475.336944	466485.443645	39.094106
2478.366644	467282.530340	39.099124
2480.567707	468090.030797	39.104141
2482.878165	468880.550218	39.109159
2484.823983	469687.470385	39.114176
2487.064703	470496.582102	39.119194
2489.862363	471304.708930	39.124212
2492.180120	472104.695329	39.129229
2494.749007	472912.033949	39.134247
2496.595982	473727.793541	39.139264
2498.725211	474552.262036	39.144282
2501.172430	475367.245583	39.149300
2503.730572	476206.726379	39.154317
2506.799199	477025.526099	39.159335
2509.207146	477856.723604	39.164352
2511.408540	478695.645865	39.169370
2514.597629	479516.386623	39.174388
2517.587931	480349.749784	39.179405
2520.190579	481167.836635	39.184423
2522.250476	481999.207419	39.189440
2524.865840	482843.881131	39.194458
2527.422665	483675.497214	39.199476
2530.148371	484508.763912	39.204493
2532.973491	485337.178948	39.209511
2534.947815	486189.021704	39.214528
2537.056697	487039.589945	39.219546
2539.249436	487902.068331	39.224564
2541.553348	488763.022417	39.229581
2544.392687	489614.053302	39.234599
2547.145517	490483.985880	39.239616
2549.508376	491354.141390	39.244634
2551.960929	492232.717868	39.249652
2554.279898	493124.848013	39.254669
2556.933077	494003.049317	39.259687
2559.302015	494883.018935	39.264704
2561.721843	495795.078679	39.269722
2564.613199	496674.920567	39.274740
2566.686902	497579.978695	39.279757
2569.660633	498479.693966	39.284775
2572.461503	499374.849283	39.289792
2574.910706	500295.541409	39.294810
2577.880172	501176.800706	39.299828
2580.467467	502084.407286	39.304845
2583.240071	502987.041175	39.309863
2585.694197	503886.299134	39.314880
2587.876607	504805.827296	39.319898
2589.996991	505723.902196	39.324916
2592.119827	506647.774902	39.329933
2595.187409	507571.086587	39.334951
2597.810851	508500.015905	39.339968
2600.747748	509418.907604	39.344986
2603.349917	510348.087108	39.350004
2605.455726	511290.200590	39.355021
2607.742019	512218.517151	39.360039
2610.196928	513171.552474	39.365056
2612.502378	514131.259058	39.370074
2615.205198	515079.703155	39.375092
2617.602043	516041.597011	39.380109
2620.300055	517007.111535	39.385127
2623.069666	517969.682258	39.390144
2625.184883	518926.607365	39.395162
2627.916436	519899.898492	39.400180
2630.066743	520871.511104	39.405197
2633.047433	521853.606008	39.410215
2635.939414	522813.436590	39.415232
2638.700793	523767.838426	39.420250
2641.260670	524695.970711	39.425268
2643.574433	525636.477067	39.430285
2646.188018	526587.804431	39.435303
2648.560306	527553.413884	39.440320
2650.644322	528501.333171	39.445338
2653.058364	529471.142746	39.450356
2655.372018	530440.452507	39.455373
2658.236523	531428.639514	39.460391
2660.970977	532394.529650	39.465408
2663.886367	533367.726680	39.470426
2667.484316	534321.014211	39.475444
2670.161378	535298.098790	39.480461
2672.945882	536284.008627	39.485479
2675.939337	537267.300594	39.490496
2678.686598	538239.343916	39.495514
2682.020400	539189.033441	39.500532
2685.531021	540158.808193	39.505549
2688.681163	541106.589296	39.510567
2691.450357	542074.594964	39.515584
2693.648190	543031.158707	39.520602
2696.396153	543990.836796	39.525620
2698.949674	544946.004810	39.530637
2702.498223	545897.724810	39.535655
2705.286276	546864.945488	39.540672
2707.297091	547822.923495	39.545690
2709.802507	548795.286720	39.550708
2712.032832	549778.085824	39.555725
2714.110520	550774.314908	39.560743
2716.781451	551766.904977	39.565760
2719.205676	552763.133604	39.570778
2721.577614	553773.976446	39.575796
2724.078888	554793.016451	39.580813
2727.067307	555812.301580	39.585831
2730.107762	556838.888899	39.590848
2732.070057	557865.625786	39.595866
2735.420636	558896.225864	39.600884
2737.843514	559936.797573	39.605901
2741.059643	560977.659543	39.610919
2743.522528	562025.798066	39.615936
2747.013573	563054.293850	39.620954
2750.828603	564062.564008	39.625972
2753.393371	565098.486290	39.630989
2756.040583	566131.701310	39.636007
2758.585305	567168.969047	39.641024
2761.154899	568217.648629	39.646042
2764.097476	569250.466080	39.651060
2766.767253	570292.634066	39.656077
2769.392127	571333.770983	39.661095
2771.589282	572386.489179	39.666112
2774.122069	573448.250412	39.671130
2776.704007	574517.643823	39.676148
2779.074339	575590.896097	39.681165
2781.567071	576659.721315	39.686183
2784.412399	577744.453765	39.691200
2786.587825	578848.819653	39.696218
2789.313290	579964.234489	39.701236
2791.943556	581060.252288	39.706253
2794.739011	582166.077104	39.711271
2797.257500	583271.296711	39.716288
2799.871240	584407.995063	39.721306
2802.825154	585517.203154	39.726324
2805.704231	586656.256118	39.731341
2808.302411	587798.206563	39.736359
2810.982296	588927.453140	39.741376
2813.882107	590061.119181	39.746394
2817.228759	591202.674084	39.751412
2819.760551	592320.349079	39.756429
2822.632286	593423.080482	39.761447
2826.136000	594523.801597	39.766464
2828.591875	595613.570633	39.771482
2831.446185	596708.383564	39.776500
2834.032345	597805.643447	39.781517
2837.093266	598898.014109	39.786535
2840.048687	599989.799182	39.791552
2843.167767	601080.052696	39.796570
2846.080700	602169.586772	39.801588
2849.094564	603259.251905	39.806605
2851.605385	604370.725065	39.811623
2854.371556	605470.735094	39.816640
2857.399949	606582.559312	39.821658
2860.762206	607696.572477	39.826676
2863.734782	608793.975744	39.831693
2866.719862	609904.431228	39.836711
2870.124654	611007.303095	39.841728
2873.083344	612102.935982	39.846746
2876.407398	613192.898800	39.851764
2879.797905	614286.395873	39.856781
2883.281997	615358.513452	39.861799
2886.966648	616422.992787	39.866816
2889.478500	617512.566085	39.871834
2892.267591	618585.285687	39.876852
2894.922209	619673.721648	39.881869
2897.460920	620756.369617	39.886887
2900.422964	621859.234976	39.891904
2903.016679	622961.049710	39.896922
2905.895797	624057.158212	39.901940
2909.013170	625143.571907	39.906957
2911.691636	626269.621497	39.911975
2914.358706	627382.265445	39.916992
2916.505640	628504.071374	39.922010
2919.629276	629630.143988	39.927028
2922.822763	630758.183621	39.932045
2925.015763	631898.203720	39.937063
2928.227645	633033.239196	39.942080
2930.724906	634200.823702	39.947098
2933.169496	635353.559767	39.952116
2936.075966	636535.793754	39.957133
2937.955236	637711.225101	39.962151
2941.103905	638895.596960	39.967168
2944.265120	640105.130873	39.972186
2947.091654	641299.410300	39.977204
2950.205924	642490.909487	39.982221
2953.675805	643681.762686	39.987239
2957.872204	644852.456376	39.992256
2961.093553	646026.916518	39.997274
2964.275063	647207.929362	40.002292
2967.302538	648390.175959	40.007309
2969.958991	649572.295252	40.012327
2973.098434	650749.360679	40.017344
2975.816090	651948.287914	40.022362
2979.048258	653113.546269	40.027380
2982.505973	654300.058134	40.032397
2985.686023	655486.872423	40.037415
2988.629817	656634.874152	40.042432
2991.365128	657821.680296	40.047450
2994.120939	659005.550530	40.052468
2996.932537	660183.242578	40.057485
2999.484154	661382.645408	40.062503
3002.620473	662571.099535	40.067520
3006.064226	663760.153865	40.072538
3009.509012	664929.151238	40.077556
3012.615969	666097.664270	40.082573
3015.871819	667275.316502	40.087591
3018.786799	668438.101896	40.092608
3021.309989	669619.069165	40.097626
3023.811541	670768.255077	40.102644
3026.565819	671918.802061	40.107661
3028.590814	673075.446479	40.112679
3031.520311	674247.016624	40.117696
3034.028839	675420.001712	40.122714
3036.566561	676603.772458	40.127732
3039.215650	677802.983356	40.132749
3041.819964	679015.516466	40.137767
3045.350803	680217.053896	40.142784
3048.262254	681433.444062	40.147802
3051.284755	682651.692450	40.152820
3054.272925	683882.849809	40.157837
3057.283977	685098.738467	40.162855
3060.346692	686352.994949	40.167872
3063.769131	687600.762711	40.172890
3066.901740	688833.164387	40.177908
3070.568934	690074.245631	40.182925
3074.064531	691324.565335	40.187943
3077.430561	692548.627844	40.192960
3080.813713	693780.112366	40.197978
3084.700908	695006.829032	40.202996
3088.822835	696215.727068	40.208013
3092.137746	697431.587116	40.213031
3095.426925	698647.333871	40.218048
3098.761906	699857.202888	40.223066
3102.548599	701053.642460	40.228084
3106.197004	702242.852363	40.233101
3109.405858	703432.022391	40.238119
3112.409936	704612.836768	40.243136
3115.814360	705792.582246	40.248154
3119.012738	706971.408197	40.253172
3122.270895	708156.255909	40.258189
3125.728526	709320.153098	40.263207
3128.746838	710485.995449	40.268224
3131.973773	711656.101445	40.273242
3135.008746	712835.684221	40.278260
3138.497752	713995.374597	40.283277
3141.026239	715175.260590	40.288295
3144.353240	716361.581506	40.293312
3146.880365	717551.182903	40.298330
3149.416904	718749.471205	40.303348
3152.359082	719943.167973	40.308365
3154.601887	721183.850214	40.313383
3157.471220	722399.565590	40.318400
3160.469138	723632.043235	40.323418
3162.995369	724881.275111	40.328436
3165.743616	726126.524494	40.333453
3168.952637	727388.660967	40.338471
3171.900511	728668.042140	40.343488
3175.155572	729955.226870	40.348506
3178.067706	731235.793150	40.353524
3181.245318	732529.302896	40.358541
3184.055723	733826.519112	40.363559
3187.167160	735125.156542	40.368576
3191.191278	736418.250274	40.373594
3194.483680	737719.549614	40.378612
3198.083203	739010.024693	40.383629
3200.687705	740329.274510	40.388647
3203.796867	741630.706873	40.393664
3206.872407	742948.161554	40.398682
3209.995489	744259.568818	40.403700
3213.294206	745581.923692	40.408717
3216.133798	746920.600348	40.413735
3219.267064	748253.774337	40.418752
3222.557106	749578.463548	40.423770
3225.096064	750924.045229	40.428788
3228.301599	752246.568973	40.433805
3231.938911	753582.047852	40.438823
3235.001543	754877.000009	40.443840
3238.591246	756178.788345	40.448858
3241.723661	757470.976991	40.453876
3245.875165	758737.572797	40.458893
3249.234488	760043.565791	40.463911
3252.004361	761319.607282	40.468928
3255.225483	762622.177206	40.473946
3258.082988	763912.036989	40.478964
3260.822154	765215.124220	40.483981
3263.832965	766527.383423	40.488999
3266.614186	767851.350220	40.494016
3269.619143	769191.367695	40.499034
3272.629290	770547.659021	40.504052
3275.673179	771894.654143	40.509069
3278.353634	773275.810290	40.514087
3281.238477	774659.179635	40.519104
3284.137570	776055.155233	40.524122
3287.078529	777465.885225	40.529140
3289.908062	778895.411508	40.534157
3293.051027	780338.252317	40.539175
3296.333996	781782.550132	40.544192
3299.607628	783243.244754	40.549210
3302.675992	784716.236518	40.554228
3306.322765	786180.983307	40.559245
3309.614467	787670.400977	40.564263
3312.769062	789156.490812	40.569280
3316.683244	790638.959047	40.574298
3320.771431	792121.137804	40.579316
3325.017080	793578.431845	40.584333
3328.829080	795045.979389	40.589351
3332.203669	796519.365642	40.594368
3335.800268	797986.284404	40.599386
3339.102157	799464.742077	40.604404
3342.744122	800925.747191	40.609421
3345.730350	802421.297299	40.614439
3348.762006	803886.622828	40.619456
3352.202834	805388.304716	40.624474
3354.873025	806881.275866	40.629492
3358.335166	808377.898114	40.634509
3361.430050	809875.572469	40.639527
3364.273707	811393.338160	40.644544
3368.078431	812898.146210	40.649562
3370.844393	814428.973984	40.654580
3374.878783	815927.499517	40.659597
3378.473077	817439.972069	40.664615
3381.800649	818964.985629	40.669632
3386.263599	820464.230819	40.674650
3390.036548	821961.202149	40.679668
3394.186114	823455.724380	40.684685
3397.760416	824942.979924	40.689703
3401.149418	826427.053163	40.694720
3404.867737	827902.546502	40.699738
3408.586045	829378.389536	40.704756
3411.592992	830859.912093	40.709773
3414.923252	832323.602918	40.714791
3418.156258	833824.483650	40.719808
3421.223638	835279.804960	40.724826
3424.779894	836783.109540	40.729844
3427.836667	838267.600133	40.734861
3431.293342	839756.692907	40.739879
3434.188474	841256.623105	40.744896
3437.554948	842759.186419	40.749914
3440.829457	844262.478796	40.754932
3444.010905	845766.693173	40.759949
3447.698026	847283.005212	40.764967
3450.752531	848778.841166	40.769984
3454.811675	850300.193782	40.775002
3457.611423	851802.592149	40.780007
3461.129021	853246.083179	40.785012
3464.888850	854624.271851	40.790016
3468.138156	855966.423732	40.795021
3471.498889	857208.143230	40.800026
3474.392250	858409.317237	40.805031
3477.486144	859537.956282	40.810036
3481.386183	860557.143148	40.815040
3483.968486	861533.886583	40.820045
3486.933438	862416.012144	40.825050
3489.475663	863260.558496	40.830055
3492.236850	863995.512771	40.835060
3494.594472	864684.185917	40.840064
3496.559447	865309.683847	40.845069
3498.787008	865868.323087	40.850074
3500.477164	866363.265657	40.855079
3502.402690	866791.679735	40.860084
3503.677666	867188.308030	40.865088
3504.692355	867552.703981	40.870093
3506.018783	867851.851763	40.875098
3507.171663	868135.958630	40.880103
3508.556005	868358.146804	40.885108
3509.694622	868538.411422	40.890112
3510.645183	868690.731738	40.895117
3511.554358	868804.402971	40.900122
3512.462691	868901.756991	40.905127
3513.212436	868948.345324	40.910132
3514.097632	868989.181322	40.915136
3514.642385	868980.351396	40.920141
3515.171677	868963.657823	40.925146
3515.723204	868920.448453	40.930151
3515.910158	868863.799849	40.935156
3516.616766	868783.465906	40.940160
3516.961420	868679.202415	40.945165
3517.343809	868574.153946	40.950170
3517.444522	868451.959532	40.955175
3517.796260	868319.037685	40.960180
3518.242235	868162.301483	40.965184
3518.313290	867997.367001	40.970189
3518.957368	867809.701909	40.975194
3518.582586	867634.826335	40.980199
3519.055984	867434.258732	40.985204
3519.192617	867227.328605	40.990208
3519.277258	867021.274251	40.995213
3519.681190	866803.405354	41.000218
3519.841459	866581.196909	41.005223
3519.667125	866339.895773	41.010228
3520.153839	866106.443202	41.015232
3520.150390	865851.006285	41.020237
3520.131829	865602.168469	41.025242
3520.036645	865343.615890	41.030247
3520.282884	865065.463675	41.035252
3520.484325	864804.992915	41.040256
3520.354365	864538.831671	41.045261
3520.631899	864257.916105	41.050266
3519.986558	863991.038211	41.055271
3520.348650	863691.518573	41.060276
3520.225430	863407.324950	41.065280
3520.388996	863126.667476	41.070285
3520.615030	862835.779544	41.075290
3520.455931	862551.843516	41.080295
3520.431116	862258.052823	41.085300
3520.510769	861960.147286	41.090304
3520.564786	861668.162481	41.095309
3520.389018	861351.795513	41.100314
3520.651580	861056.732823	41.105319
3520.523333	860757.344242	41.110324
3520.211722	860455.150963	41.115328
3520.283698	860160.076403	41.120333
3520.631024	859847.727393	41.125338
3520.551620	859538.545206	41.130343
3520.385194	859226.930028	41.135348
3520.248074	858919.476978	41.140352
3520.050261	858614.353216	41.145357
3519.934500	858305.503995	41.150362
3520.132655	857989.388182	41.155367
3520.062697	857674.370514	41.160372
3520.042554	857365.361035	41.165376
3519.725975	857053.757678	41.170381
3520.276726	856740.536074	41.175386
3519.622639	856448.808624	41.180391
3519.443112	856136.844404	41.185396
3519.537596	855839.612357	41.190400
3519.311855	855533.464624	41.195405
3519.473676	855222.857931	41.200410
3519.551820	854926.265984	41.205415
3519.416112	854602.341950	41.210420
3519.083408	854311.920794	41.215424
3519.244321	854000.084742	41.220429
3519.472170	853687.540489	41.225434
3518.914589	853387.474756	41.230439
3518.851357	853088.676212	41.235444
3518.906062	852786.533267	41.240448
3518.744723	852493.954005	41.245453
3519.098429	852180.728963	41.250458
3518.566267	851888.766598	41.255463
3518.573830	851585.696639	41.260468
3518.420462	851290.819554	41.265472
3518.158256	850998.868409	41.270477
3518.528223	850707.286490	41.275482
3518.358537	850396.395672	41.280487
3518.204798	850109.255453	41.285492
3518.127553	849816.049585	41.290496
3517.888847	849524.999841	41.295501
3517.929741	849237.592696	41.300506
3517.634616	848933.274765	41.305511
3517.543569	848655.118546	41.310516
3517.354186	848363.324641	41.315520
3517.226422	848089.631609	41.320525
3517.145469	847811.826105	41.325530
3517.403296	847528.495167	41.330535
3517.154711	847250.789916	41.335540
3516.899996	846968.687648	41.340544
3516.614303	846693.108027	41.345549
3516.800184	846400.478888	41.350554
3516.594542	846127.785440	41.355559
3516.496111	845857.889409	41.360564
3516.304588	845591.506533	41.365568
3516.128277	845332.713863	41.370573
3516.281105	845058.550324	41.375578
3516.128623	844799.829379	41.380583
3516.003867	844534.950843	41.385588
3516.223789	844258.206562	41.390592
3515.959060	844013.122346	41.395597
3515.751940	843733.549003	41.400602
3515.542485	843491.409576	41.405607
3515.383500	843208.977215	41.410612
3515.635068	842961.524322	41.415616
3515.564745	842707.385436	41.420621
3515.437519	842447.881539	41.425626
3515.255095	842198.032090	41.430631
3515.115514	841951.384534	41.435636
3515.213571	841696.982408	41.440640
3514.925139	841463.703770	41.445645
3514.933167	841192.859766	41.450650
3514.734283	840952.963008	41.455655
3514.800582	840697.794524	41.460660
3515.067747	840458.973101	41.465664
3514.665754	840211.667211	41.470669
3514.407004	839954.278512	41.475674
3514.430790	839714.639977	41.480679
3514.507980	839471.324533	41.485684
3514.434923	839233.391490	41.490688
3513.980541	838994.097432	41.495693
3514.103262	838762.945507	41.500698
3513.761054	838530.983494	41.505703
3513.698234	838315.021333	41.510708
3513.540249	838070.520215	41.515712
3513.571938	837861.603055	41.520717
3513.669146	837625.436624	41.525722
3513.654859	837413.828319	41.530727
3513.400083	837176.824879	41.535732
3513.706841	836950.360245	41.540736
3513.352823	836724.240515	41.545741
3513.639023	836505.133769	41.550746
3513.089348	836289.818179	41.555751
3513.294328	836069.440843	41.560756
3513.392339	835839.066321	41.565760
3513.105584	835626.565368	41.570765
3513.203867	835412.724683	41.575770
3513.054002	835189.983564	41.580775
3512.914365	834972.115318	41.585780
3512.756543	834751.655026	41.590784
3512.517130	834539.940462	41.595789
3512.607472	834332.754413	41.600794
3512.197063	834131.308350	41.605799
3512.339478	833919.364064	41.610804
3512.486491	833707.949227	41.615808
3512.088827	833516.687803	41.620813
3512.264314	833297.490329	41.625818
3512.256284	833096.775956	41.630823
3512.202711	832900.702491	41.635828
3512.016517	832689.016231	41.640832
3511.990835	832480.666671	41.645837
3511.917335	832285.457019	41.650842
3511.724426	832101.544176	41.655847
3511.638829	831895.823285	41.660852
3511.762469	831702.712844	41.665856
3511.257200	831517.418331	41.670861
3511.271277	831336.820283	41.675866
3511.204454	831131.169782	41.680871
3511.137412	830956.974085	41.685876
3511.294064	830753.766334	41.690880
3510.820507	830581.044304	41.695885
3510.835243	830392.114460	41.700890
3510.967654	830222.703104	41.705895
3510.829294	830033.055190	41.710900
3510.942250	829849.125975	41.715904
3510.555043	829669.085227	41.720909
3510.750426	829491.435601	41.725914
3510.594047	829314.425461	41.730919
3510.541678	829146.678003	41.735924
3510.697156	828961.055298	41.740928
3510.337869	828797.209968	41.745933
3510.243046	828619.486687	41.750938
3510.291081	828461.088180	41.755943
3510.108908	828272.324884	41.760948
3510.546947	828115.955317	41.765952
3510.199840	827951.255920	41.770957
3510.023206	827777.726518	41.775962
3509.917144	827628.277645	41.780967
3509.931713	827448.402797	41.785972
3510.054440	827279.649917	41.790976
3509.864558	827127.172843	41.795981
3509.784265	826957.907426	41.800986
3509.841404	826789.788220	41.805991
3509.554036	826626.316661	41.810996
3509.919199	826466.791118	41.816000
3509.493598	826315.116180	41.821005
3509.556170	826140.721860	41.826010
3509.738920	825995.245983	41.831015
3509.261717	825820.247609	41.836020
3509.312260	825669.457162	41.841024
3509.556860	825512.715189	41.846029
3509.378927	825348.167044	41.851034
3509.269471	825202.721774	41.856039
3509.065913	825047.998385	41.861044
3508.999838	824896.133700	41.866048
3508.895132	824754.736289	41.871053
3509.074957	824601.308437	41.876058
3508.936100	824445.826747	41.881063
3508.668274	824317.601285	41.886068
3508.745125	824166.380881	41.891072
3508.653786	824029.171406	41.896077
3509.004472	823892.717666	41.901082
3508.852589	823745.242106	41.906087
3508.698450	823596.296395	41.911092
3508.492711	823451.072890	41.916096
3508.460309	823313.203020	41.921101
3508.584579	823172.418733	41.926106
3508.336178	823033.502571	41.931111
3508.355884	822886.908920	41.936116
3508.540824	822757.991650	41.941120
3508.065800	822618.810623	41.946125
3508.355946	822496.034198	41.951130
3508.302702	822362.207957	41.956135
3508.384394	822223.856349	41.961140
3508.355270	822083.465515	41.966144
3507.935897	821958.056534	41.971149
3507.978775	821809.918718	41.976154
3508.030834	821691.863018	41.981159
3507.810308	821558.781936	41.986164
3507.971694	821439.969907	41.991168
3507.573408	821299.721135	41.996173
3507.523129	821182.260322	42.001178
3507.745499	821048.117541	42.006183
3507.547306	820937.086121	42.011188
3507.747922	820802.012337	42.016192
3507.433385	820676.953299	42.021197
3507.571954	820566.643089	42.026202
3507.511001	820437.819102	42.031207
3507.440378	820329.349859	42.036212
3507.833640	820198.929547	42.041216
3507.227420	820086.483146	42.046221
3507.588564	819964.969443	42.051226
3507.327624	819833.817850	42.056231
3507.173133	819722.563214	42.061236
3507.002973	819597.900536	42.066240
3506.979861	819492.884376	42.071245
3506.828777	819376.142345	42.076250
3506.706743	819260.519096	42.081255
3506.801160	819159.099851	42.086260
3507.086076	819047.663693	42.091264
3506.659988	818942.215824	42.096269
3506.981892	818830.623125	42.101274
3506.818114	818727.086360	42.106279
3506.409551	818609.100782	42.111284
3506.648491	818513.717029	42.116288
3506.437997	818412.532445	42.121293
3506.711849	818306.127157	42.126298
3507.064031	818209.105168	42.131303
3506.286874	818094.646470	42.136308
3506.690693	817994.822821	42.141312
3506.532411	817878.887922	42.146317
3506.942511	817781.115940	42.151322
3506.771915	817667.382173	42.156327
3506.099854	817571.449717	42.161332
3506.158043	817471.479384	42.166336
3506.577478	817376.832935	42.171341
3506.529112	817266.254190	42.176346
3506.611959	817160.694374	42.181351
3506.325087	817072.426200	42.186356
3506.653702	816956.688863	42.191360
3506.296398	816859.617313	42.196365
3506.461000	816760.206326	42.201370
3506.205006	816654.155805	42.206375
3506.038792	816569.141359	42.211380
3506.481102	816461.014392	42.216384
3506.404980	816367.561408	42.221389
3506.220375	816266.095304	42.226394
3505.922773	816173.557405	42.231399
3505.920719	816082.095695	42.236404
3505.934708	815983.922089	42.241408
3505.809966	815893.751075	42.246413
3505.918918	815797.517672	42.251418
3505.757256	815698.928147	42.256423
3505.775804	815614.213931	42.261428
3505.774706	815518.533289	42.266432
3505.524850	815445.711158	42.271437
3505.474026	815349.448689	42.276442
3505.610416	815263.290564	42.281447
3505.672605	815174.205388	42.286452
3505.746651	815080.513886	42.291456
3505.550459	814994.162244	42.296461
3505.501176	814907.295581	42.301466
3505.357928	814831.804783	42.306471
3505.249228	814736.228682	42.311476
3505.290130	814670.598217	42.316480
3505.144664	814590.158784	42.321485
3505.218442	814500.132278	42.326490
3505.128028	814429.476730	42.331495
3505.136695	814359.244898	42.336500
3505.127544	814271.530843	42.341504
3505.246531	814202.454632	42.346509
3504.881202	814115.433907	42.351514
3504.819709	814045.602182	42.356519
3504.733762	813958.729326	42.361524
3504.939676	813876.068445	42.366528
3504.619910	813818.423670	42.371533
3504.838792	813730.126240	42.376538
3504.855812	813689.763784	42.381543
3505.241862	813602.024908	42.386548
3505.076942	813543.568584	42.391552
3504.831147	813462.642409	42.396557
3504.728734	813395.504701	42.401562
3504.721188	813320.023601	42.406567
3504.699782	813234.747233	42.411572
3504.686086	813173.960571	42.416576
3504.378424	813094.068832	42.421581
3504.507247	813033.061489	42.426586
3504.874548	812958.249382	42.431591
3504.526774	812907.361443	42.436596
3504.959817	812826.462790	42.441600
3504.481241	812765.700041	42.446605
3504.696544	812696.347626	42.451610
3504.639808	812623.218246	42.456615
3504.585152	812541.073835	42.461620
3504.961678	812477.375297	42.466624
3504.555837	812416.548439	42.471629
3504.564051	812342.768465	42.476634
3504.617818	812278.337377	42.481639
3504.654691	812212.781666	42.486644
3504.701251	812142.324577	42.491648
3504.390098	812079.617415	42.496653
3504.418454	812007.741158	42.501658
3504.498630	811947.123980	42.506663
3504.422945	811885.111125	42.511668
3504.739580	811809.510781	42.516672
3504.683658	811749.649162	42.521677
3504.789155	811673.151182	42.526682
3504.891470	811602.777290	42.531687
3504.611951	811538.247074	42.536692
3504.735433	811460.077869	42.541696
3504.425654	811394.963316	42.546701
3504.449375	811326.363389	42.551706
3504.523764	811268.974928	42.556711
3504.274637	811206.298461	42.561716
3504.541626	811142.703427	42.566720
3504.517978	811072.393779	42.571725
3504.382766	811014.547699	42.576730
3504.645706	810947.962529	42.581735
3504.304030	810891.423409	42.586740
3504.286116	810808.516936	42.591744
3504.368972	810743.674466	42.596749
3504.259048	810684.498364	42.601754
3504.347066	810633.668556	42.606759
3504.013615	810573.793271	42.611764
3504.101788	810501.058151	42.616768
3504.086775	810446.666670	42.621773
3503.694879	810404.146815	42.626778
3504.014113	810335.684221	42.631783
3503.779254	810304.506919	42.636788
3504.062144	810233.108992	42.641792
3503.626265	810190.104989	42.646797
3503.931437	810132.031837	42.651802
3503.918293	810068.129849	42.656807
3503.810130	810018.993979	42.661812
3504.148960	809957.336295	42.666816
3504.122588	809905.980810	42.671821
3504.080841	809852.667149	42.676826
3504.277059	809803.430578	42.681831
3503.966844	809730.997885	42.686836
3504.104238	809680.299846	42.691840
3503.950674	809630.874596	42.696845
3504.084174	809562.777890	42.701850
3504.013789	809522.552045	42.706855
3503.708865	809457.418111	42.711860
3504.179530	809398.037162	42.716864
3503.719363	809360.227101	42.721869
3503.693910	809296.074834	42.726874
3503.791397	809234.156287	42.731879
3503.442528	809184.122800	42.736884
3503.758123	809138.929828	42.741888
3503.594007	809080.238826	42.746893
3503.573333	809032.796902	42.751898
3503.696900	808982.193975	42.756903
3503.688749	808931.906457	42.761908
3503.656433	808876.034836	42.766912
3503.362298	808841.968704	42.771917
3503.399780	808802.210991	42.776922
3503.524288	808755.233378	42.781927
3503.591892	808698.510573	42.786932
3503.738342	808650.058132	42.791937
3503.415707	808599.868982	42.796941
3503.397718	808555.364315	42.801946
3503.397343	808505.513528	42.806951
3503.424261	808457.324496	42.811956
3503.651182	808416.307881	42.816961
3503.695095	808371.693783	42.821965
3503.549737	808336.718284	42.826970
3503.647394	808273.075324	42.831975
3503.243006	808229.122369	42.836980
3503.082382	808175.079870	42.841985
3503.190137	808145.502925	42.846989
3503.622982	808092.587529	42.851994
3503.500299	808050.302744	42.856999
3503.126240	808005.853144	42.862004
3503.293124	807963.912298	42.867009
3503.497511	807915.003906	42.872013
3503.501902	807888.237124	42.877018
3503.444418	807831.723813	42.882023
3503.317355	807802.429175	42.887028
3503.193644	807736.121424	42.892033
3503.387556	807698.684636	42.897037
3503.438594	807652.888108	42.902042
3503.352154	807600.005412	42.907047
3503.016291	807580.450999	42.912052
3503.165548	807523.018644	42.917057
3503.227094	807477.268233	42.922061
3502.822458	807441.840606	42.927066
3503.361085	807403.953224	42.932071
3503.044279	807373.609437	42.937076
3503.193529	807326.127666	42.942081
3503.288485	807292.479969	42.947085
3503.026328	807253.792155	42.952090
3503.210217	807206.450928	42.957095
3502.950581	807165.408901	42.962100
3502.796846	807133.027066	42.967105
3502.940607	807098.585936	42.972109
3503.006497	807058.960485	42.977114
3502.881323	807021.915750	42.982119
3502.842426	806987.259005	42.987124
3503.101718	806963.829593	42.992129
3502.884032	806929.937438	42.997133
3503.288777	806889.127524	43.002138
3503.119208	806837.723507	43.007143
3503.167686	806809.817563	43.012148
3503.219376	806772.644287	43.017153
3503.103578	806716.670702	43.022157
3503.061657	806683.336741	43.027162
3503.159227	806640.026341	43.032167
3502.949075	806603.679775	43.037172
3503.030789	806562.725002	43.042177
3502.801176	806519.369668	43.047181
3502.728226	806493.296617	43.052186
3503.294359	806452.506556	43.057191
3503.101696	806425.178121	43.062196
3503.119792	806383.350169	43.067201
3503.113414	806344.713150	43.072205
3502.919378	806306.106824	43.077210
3503.191363	806276.641857	43.082215
3502.976919	806246.472343	43.087220
3503.164475	806180.539558	43.092225
3503.111957	806160.493100	43.097229
3503.003906	806114.124073	43.102234
3503.168066	806081.684904	43.107239
3502.595169	806045.738373	43.112244
3503.001374	806007.276672	43.117249
3503.049607	805973.875377	43.122253
3502.738851	805948.378817	43.127258
3503.031036	805897.431086	43.132263
3502.795464	805861.477061	43.137268
3503.019401	805816.669550	43.142273
3503.119382	805794.145053	43.147277
3503.034131	805747.769795	43.152282
3503.125848	805722.451289	43.157287
3503.031863	805682.304804	43.162292
3503.243680	805633.378908	43.167297
3503.172157	805609.705137	43.172301
3503.128509	805556.015000	43.177306
3503.254490	805525.541047	43.182311
3502.899158	805491.174056	43.187316
3503.119647	805449.797470	43.192321
3502.827787	805410.172382	43.197325
3502.966156	805379.989983	43.202330
3502.855431	805338.814405	43.207335
3502.646231	805321.880847	43.212340
3503.262154	805273.425273	43.217345
3502.935779	805231.352795	43.222349
3502.800761	805204.500411	43.227354
3502.944853	805164.017434	43.232359
3502.813354	805126.620209	43.237364
3503.066359	805097.888946	43.242369
3502.977453	805062.102744	43.247373
3502.651582	805031.161560	43.252378
3503.126970	804983.511776	43.257383
3503.145196	804957.614044	43.262388
3503.067688	804908.632562	43.267393
3503.271329	804871.767270	43.272397
3503.004015	804830.957748	43.277402
3503.043690	804793.579561	43.282407
3502.888720	804759.323037	43.287412
3503.213147	804728.763823	43.292417
3502.912285	804705.222801	43.297421
3502.726742	804671.019917	43.302426
3503.209060	804631.115682	43.307431
3502.758715	804589.353964	43.312436
3503.058586	804565.860653	43.317441
3502.586008	804521.944168	43.322445
3502.670433	804488.284462	43.327450
3502.985470	804444.581078	43.332455
3502.738278	804427.700619	43.337460
3502.678427	804375.916763	43.342465
3502.453079	804358.198732	43.347469
3502.456897	804327.249121	43.352474
3502.585161	804296.573160	43.357479
3502.486334	804274.517865	43.362484
3502.493868	804255.044531	43.367489
3502.701246	804207.139236	43.372493
3502.664672	804195.030259	43.377498
3502.397412	804151.371880	43.382503
3502.571021	804127.260237	43.387508
3503.018147	804090.007315	43.392513
3502.658178	804059.410717	43.397517
3502.541678	804039.368610	43.402522
3502.972920	803992.945492	43.407527
3502.691186	803971.704155	43.412532
3502.740290	803927.697947	43.417537
3502.668771	803913.141709	43.422541
3502.321276	803883.523284	43.427546
3502.477710	803850.731517	43.432551
3502.485836	803836.554406	43.437556
3502.526349	803796.276655	43.442561
3502.510192	803772.783648	43.447565
3502.610836	803739.804337	43.452570
3502.413187	803705.696754	43.457575
3502.423892	803687.447593	43.462580
3502.671337	803655.081375	43.467585
3502.492920	803633.380504	43.472589
3502.492734	803605.077146	43.477594
3502.779139	803578.198053	43.482599
3502.305785	803546.538687	43.487604
3502.430868	803511.395920	43.492609
3502.737764	803495.991617	43.497613
3502.529256	803461.394078	43.502618
3502.999881	803437.574480	43.507623
3502.740802	803409.705395	43.512628
3502.802561	803367.214205	43.517633
3502.628326	803346.345666	43.522637
3502.498293	803310.802409	43.527642
3502.460808	803275.636165	43.532647
3502.431447	803256.509473	43.537652
3502.549090	803225.143725	43.542657
3502.432191	803183.710996	43.547661
3502.186413	803161.921624	43.552666
3502.580379	803130.755213	43.557671
3502.456915	803127.292540	43.562676
3502.595019	803102.398270	43.567681
3502.395724	803069.808556	43.572685
3502.327841	803042.249888	43.577690
3502.569461	803013.658992	43.582695
3502.126472	802998.229927	43.587700
3502.163618	802955.396857	43.592705
3502.357304	802945.504396	43.597709
3502.034250	802910.138040	43.602714
3502.081425	802882.412610	43.607719
3501.999863	802868.248282	43.612724
3502.037887	802862.207862	43.617729
3502.257591	802833.423599	43.622733
3502.240905	802816.108753	43.627738
3502.266335	802788.582761	43.632743
3502.068581	802768.648459	43.637748
3502.403941	802758.339926	43.642753
3502.233345	802727.559043	43.647757
3501.853720	802699.216352	43.652762
3502.180468	802670.511897	43.657767
3502.013927	802666.173019	43.662772
3502.151338	802651.775942	43.667777
3502.371982	802612.442805	43.672781
3502.251201	802598.235324	43.677786
3501.923692	802573.366782	43.682791
3501.937296	802553.495165	43.687796
3502.188812	802541.188652	43.692801
3502.410642	802514.070760	43.697805
3502.008612	802500.449069	43.702810
3502.358441	802470.660652	43.707815
3502.183958	802446.747663	43.712820
3502.077949	802421.400541	43.717825
3502.214311	802413.969820	43.722829
3502.259169	802388.941157	43.727834
3502.179825	802356.917057	43.732839
3501.958950	802341.548057	43.737844
3502.060941	802322.004649	43.742849
3502.113777	802301.340856	43.747853
3501.925495	802291.657564	43.752858
3501.905700	802266.344734	43.757863
3502.016014	802246.897867	43.762868
3502.160778	802238.140890	43.767873
3501.925589	802210.410212	43.772877
3501.872285	802202.470816	43.777882
3501.924731	802179.304526	43.782887
3501.850687	802165.480960	43.787892
3501.779429	802142.874616	43.792897
3501.928166	802132.007136	43.797901
3502.120318	802112.055779	43.802906
3501.888320	802089.917309	43.807911
3501.954303	802088.925145	43.812916
3501.957416	802067.680083	43.817921
3502.200893	802045.070643	43.822925
3501.740685	802036.020547	43.827930
3501.913521	802008.516235	43.832935
3501.813102	802010.053735	43.837940
3501.909051	801972.945386	43.842945
3502.171703	801979.771098	43.847949
3501.807187	801948.086462	43.852954
3501.942438	801920.833315	43.857959
3501.968187	801925.244868	43.862964
3502.215391	801887.865826	43.867969
3502.053334	801883.574780	43.872973
3501.969702	801851.205591	43.877978
3502.077514	801826.262654	43.882983
3501.953460	801818.481667	43.887988
3501.836765	801801.180753	43.892993
3501.798218	801792.551538	43.897997
3501.747822	801770.431197	43.903002
3501.860152	801761.777092	43.908007
3501.564692	801741.463393	43.913012
3501.752823	801725.485927	43.918017
3501.749245	801709.490936	43.923021
3501.681826	801712.347852	43.928026
3501.922897	801684.585685	43.933031
3501.736398	801671.711915	43.938036
3501.724387	801656.601386	43.943041
3502.156488	801658.885381	43.948045
3502.002001	801634.328424	43.953050
3502.301906	801606.703454	43.958055
3502.027923	801610.870176	43.963060
3501.974545	801565.246598	43.968065
3502.002562	801553.514887	43.973069
3501.907334	801522.912495	43.978074
3502.090101	801506.101260	43.983079
3502.274115	801506.463466	43.988084
3502.017562	801478.193626	43.993089
3502.165835	801468.355608	43.998093
3502.138239	801445.739796	44.003098
3502.051683	801413.565315	44.008103
3502.281969	801410.779534	44.013108
3502.228969	801389.345362	44.018113
3502.245010	801384.681190	44.023117
3501.664535	801349.643658	44.028122
3501.994028	801324.760541	44.033127
3501.875663	801313.248810	44.038132
3501.426008	801291.634324	44.043137
3501.773462	801278.475597	44.048141
3501.726978	801266.068701	44.053146
3502.200720	801242.731749	44.058151
3501.804890	801240.736003	44.063156
3501.902540	801220.110674	44.068161
3502.254142	801200.179501	44.073165
3501.965697	801195.467216	44.078170
3502.156099	801166.435506	44.083175
3501.845914	801164.523771	44.088180
3501.957481	801130.794172	44.093185
3501.665590	801123.972383	44.098189
3501.683928	801120.877906	44.103194
3501.726363	801110.271688	44.108199
3501.641855	801101.551042	44.113204
3502.085456	801060.994684	44.118209
3502.191197	801051.408435	44.123213
3501.786369	801036.164973	44.128218
3502.228006	801002.331312	44.133223
3502.083740	801009.372224	44.138228
3501.786361	800975.022232	44.143233
3502.067861	800966.486486	44.148237
3501.721007	800955.453438	44.153242
3502.099383	800936.498530	44.158247
3501.962553	800917.284930	44.163252
3502.150348	800898.557597	44.168257
3501.986253	800884.648161	44.173261
3501.746760	800859.857100	44.178266
3501.888780	800839.615909	44.183271
3501.857292	800829.414017	44.188276
3501.981702	800803.434148	44.193281
3502.060862	800788.993728	44.198285
3502.085904	800779.812978	44.203290
3502.298447	800756.173908	44.208295
3502.037326	800743.948651	44.213300
3501.775816	800724.656906	44.218305
3502.220456	800694.256372	44.223309
3502.149277	800695.642124	44.228314
3502.252281	800659.899641	44.233319
3502.005272	800646.984858	44.238324
3502.205415	800627.469581	44.243329
3502.271751	800602.970743	44.248333
3502.092995	800590.584427	44.253338
3502.144506	800556.125817	44.258343
3501.956776	800561.898408	44.263348
3501.834258	800543.319380	44.268353
3502.073065	800514.424196	44.273357
3501.979211	800506.342310	44.278362
3502.451480	800491.100400	44.283367
3502.072897	800466.232691	44.288372
3502.196989	800459.145426	44.293377
3502.428647	800425.441696	44.298381
3502.065116	800421.919054	44.303386
3502.129670	800380.243353	44.308391
3502.101201	800375.242306	44.313396
3501.986086	800347.239008	44.318401
3502.100770	800307.321342	44.323405
3501.853480	800303.141503	44.328410
3502.210183	800289.979386	44.333415
3501.831771	800261.920961	44.338420
3502.047703	800249.763483	44.343425
3501.950458	800234.762049	44.348429
3501.750886	800209.765781	44.353434
3502.263662	800199.620545	44.358439
3502.112406	800182.713898	44.363444
3501.915280	800167.532463	44.368449
3502.149005	800157.089590	44.373453
3501.990059	800128.700014	44.378458
3501.817955	800106.398103	44.383463
3501.791064	800098.844565	44.388468
3501.614558	800078.162848	44.393473
3502.077140	800058.210127	44.398477
3501.918267	800054.310040	44.403482
3502.312478	800041.828367	44.408487
3502.105133	800011.826712	44.413492
3502.049591	799989.357992	44.418497
3502.018369	799972.725531	44.423501
3501.668101	799941.127523	44.428506
3502.168736	799938.296629	44.433511
3501.998809	799914.815855	44.438516
3501.808337	799916.761278	44.443521
3501.842382	799899.479867	44.448525
3501.432075	799883.743977	44.453530
3502.026789	799867.400797	44.458535
3502.051846	799857.384480	44.463540
3501.458004	799849.286026	44.468545
3502.006567	799823.527107	44.473549
3501.827514	799810.452333	44.478554
3501.766166	799791.566739	44.483559
3501.729528	799793.241459	44.488564
3501.549835	799766.473450	44.493569
3501.761411	799758.634864	44.498573
3501.768414	799755.443486	44.503578
3502.164505	799735.549874	44.508583
3502.019044	799711.818984	44.513588
3501.870670	799695.106996	44.518593
3501.955020	799694.307790	44.523597
3501.932087	799655.341577	44.528602
3501.988200	799633.785850	44.533607
3501.787823	799643.733153	44.538612
3501.731087	799613.950376	44.543617
3501.816716	799593.616687	44.548621
3501.765970	799587.342632	44.553626
3501.981779	799577.000005	44.558631
3501.592854	799556.400804	44.563636
3501.470409	799555.144830	44.568641
3501.946272	799542.599735	44.573645
3501.687053	799535.967320	44.578650
3501.923652	799524.590479	44.583655
3502.186332	799496.668771	44.588660
3501.961285	799502.939201	44.593665
3501.861410	799456.082376	44.598669
3501.566756	799449.701126	44.603674
3501.871397	799437.380374	44.608679
3501.605840	799444.099270	44.613684
3501.787264	799423.945635	44.618689
3501.792522	799402.544815	44.623693
3501.979796	799394.218999	44.628698
3501.963384	799381.214792	44.633703
3501.792412	799351.007962	44.638708
3501.872373	799338.773127	44.643713
3502.022272	799332.171295	44.648717
3501.767262	799308.898820	44.653722
3501.760232	799290.150168	44.658727
3501.633771	799294.490299	44.663732
3501.357133	799287.369682	44.668737
3501.819606	799252.591507	44.673741
3501.857101	799247.676950	44.678746
3502.047928	799237.877855	44.683751
3501.998014	799226.105967	44.688756
3501.783327	799192.567955	44.693761
3502.198401	799183.664443	44.698765
3502.107430	799175.286029	44.703770
3501.807091	799152.756759	44.708775
3502.034501	799135.588855	44.713780
3501.800784	799123.552562	44.718785
3501.890576	799095.608641	44.723789
3501.771046	799094.008510	44.728794
3501.928508	799086.374422	44.733799
3501.854325	799058.751870	44.738804
3501.791822	799045.852798	44.743809
3501.892123	799032.288780	44.748813
3501.524356	799017.918300	44.753818
3501.580497	798994.691693	44.758823
3501.659878	798990.015482	44.763828
3501.392407	798974.057658	44.768833
3501.784917	798965.452098	44.773837
3501.649056	798962.529317	44.778842
3501.858291	798938.197422	44.783847
3501.781400	798940.418920	44.788852
3501.849344	798937.757073	44.793857
3501.903589	798915.610401	44.798861
3501.578919	798899.318226	44.803866
3501.717331	798889.429103	44.808871
3501.515450	798887.646145	44.813876
3501.564886	798877.673489	44.818881
3501.800489	798864.872238	44.823885
3501.726413	798848.980445	44.828890
3502.127726	798842.189480	44.833895
3501.658142	798824.055713	44.838900
3501.747044	798799.252289	44.843905
3501.949472	798782.627586	44.848909
3501.710269	798782.814221	44.853914
3501.710341	798766.664592	44.858919
3501.741848	798757.627370	44.863924
3501.520166	798738.274458	44.868929
3501.602723	798735.953737	44.873933
3501.346896	798732.167048	44.878938
3501.596486	798728.149847	44.883943
3501.463252	798709.027720	44.888948
3501.295481	798685.051566	44.893953
3501.574595	798682.894802	44.898957
3501.532947	798676.520251	44.903962
3501.645721	798690.000726	44.908967
3501.657019	798674.438084	44.913972
3501.610199	798637.777230	44.918977
3501.552632	798640.044728	44.923981
3501.457124	798628.279339	44.928986
3501.494461	798626.211470	44.933991
3501.674451	798626.476325	44.938996
3501.468889	798618.214291	44.944001
3501.422800	798581.749373	44.949005
3501.261481	798587.911949	44.954010
3501.420266	798580.228003	44.959015
3501.353430	798559.720058	44.964020
3501.301334	798552.070816	44.969025
3501.974107	798562.612165	44.974029
3501.471750	798555.037090	44.979034
3501.479986	798542.321788	44.984039
3501.396005	798534.432336	44.989044
3501.226694	798526.311486	44.994049
3501.384455	798522.947446	44.999053
3501.147334	798525.195468	45.004058
3501.841954	798522.184797	45.009063
3501.688740	798518.184734	45.014068
3501.324048	798493.454936	45.019073
3501.645341	798468.121169	45.024077
3501.563496	798472.798083	45.029082
3501.592247	798464.840895	45.034087
3501.542486	798460.332868	45.039092
3501.490748	798458.819601	45.044097
3501.789219	798441.834644	45.049101
3501.708716	798421.181275	45.054106
3501.914145	798419.232926	45.059111
3501.705559	798411.805663	45.064116
3501.634092	798397.826900	45.069121
3501.825421	798381.399429	45.074125
3501.504983	798374.825075	45.079130
3501.700452	798369.883879	45.084135
3501.809203	798353.617214	45.089140
3501.618750	798341.523351	45.094145
3501.715982	798326.093048	45.099149
3501.559611	798320.522509	45.104154
3501.899409	798318.306549	45.109159
3502.172663	798286.254686	45.114164
3501.821944	798263.976288	45.119169
3501.689115	798261.347254	45.124173
3501.912912	798237.108700	45.129178
3502.226168	798224.440759	45.134183
3502.174254	798216.840210	45.139188
3502.021217	798181.618088	45.144193
3502.216431	798175.596793	45.149197
3501.690950	798161.839613	45.154202
3501.921421	798153.554296	45.159207
3501.955126	798135.974021	45.164212
3501.713768	798134.050094	45.169217
3501.977244	798088.302417	45.174221
3501.724108	798094.775100	45.179226
3501.670728	798081.087272	45.184231
3501.700341	798087.464298	45.189236
3501.355871	798050.505742	45.194241
3501.584695	798032.009410	45.199245
3501.594586	798030.633175	45.204250
3501.777314	798010.131600	45.209255
3501.789801	798015.087836	45.214260
3501.448991	797987.897696	45.219265
3501.644888	797979.863331	45.224269
3501.504088	797967.318807	45.229274
3501.775631	797976.307084	45.234279
3501.722613	797967.773688	45.239284
3501.467477	797948.276812	45.244289
3501.599566	797931.514393	45.249293
3501.649378	797933.028040	45.254298
3501.773493	797928.834679	45.259303
3501.856923	797911.343834	45.264308
3501.491662	797883.568199	45.269313
3501.796186	797874.190305	45.274317
3501.662902	797876.814174	45.279322
3501.531878	797878.455806	45.284327
3501.833717	797853.761229	45.289332
3501.368056	797837.833443	45.294337
3501.628238	797822.817030	45.299341
3501.396454	797819.909566	45.304346
3501.615866	797813.393039	45.309351
3501.884262	797802.548190	45.314356
3501.527292	797785.669601	45.319361
3502.055758	797778.463917	45.324365
3501.805582	797776.541342	45.329370
3501.653247	797755.406894	45.334375
3501.784444	797745.861002	45.339380
3501.722399	797731.290221	45.344385
3501.830457	797720.471655	45.349389
3501.383158	797706.700695	45.354394
3501.170251	797681.059312	45.359399
3501.288391	797686.243852	45.364404
3501.390646	797685.195997	45.369409
3501.640284	797675.728690	45.374413
3501.793681	797682.723926	45.379418
3501.308768	797660.612986	45.384423
3501.637439	797660.755202	45.389428
3501.747842	797646.057649	45.394433
3501.745752	797630.740361	45.399437
3501.698110	797619.112670	45.404442
3501.274032	797622.128197	45.409447
3501.806265	797609.864932	45.414452
3501.664304	797586.371699	45.419457
3501.658128	797571.054953	45.424461
3501.592270	797584.419702	45.429466
3501.889868	797575.435312	45.434471
3501.703566	797545.812327	45.439476
3501.551647	797529.586680	45.444481
3501.522009	797513.488142	45.449485
3501.653328	797527.704245	45.454490
3501.645633	797502.470266	45.459495
3501.555292	797489.229229	45.464500
3501.560715	797482.894930	45.469505
3501.714849	797473.295793	45.474509
3501.418678	797468.729520	45.479514
3501.554893	797474.549489	45.484519
3501.693084	797442.025044	45.489524
3501.585684	797437.034887	45.494529
3501.481334	797426.447238	45.499533
3501.599580	797429.029844	45.504538
3501.730985	797414.279248	45.509543
3501.951600	797404.472680	45.514548
3501.576118	797382.244638	45.519553
3501.971857	797383.406846	45.524557
3501.672700	797370.494559	45.529562
3501.893568	797358.674917	45.534567
3502.055840	797350.105304	45.539572
3501.789690	797339.151399	45.544577
3501.686125	797314.178016	45.549581
3501.591144	797299.169884	45.554586
3501.907965	797302.603579	45.559591
3501.764886	797301.006911	45.564596
3501.364034	797283.496069	45.569601
3501.892785	797255.816165	45.574605
3501.989040	797250.988720	45.579610
3502.054180	797232.860921	45.584615
3501.915625	797207.303748	45.589620
3501.594469	797193.020013	45.594625
3501.850343	797191.210312	45.599629
3501.977197	797195.411821	45.604634
3501.942280	797157.661080	45.609639
3501.933252	797143.080340	45.614644
3501.627285	797134.783983	45.619649
3501.762040	797118.215570	45.624653
3501.787605	797097.491717	45.629658
3501.834942	797099.496940	45.634663
3501.591642	797085.691148	45.639668
3501.143027	797066.911061	45.644673
3501.734372	797040.349271	45.649677
3501.822767	797049.221615	45.654682
3501.871330	797047.740620	45.659687
3501.802046	797034.200657	45.664692
3501.781763	797018.590430	45.669697
3502.097309	796992.024787	45.674701
3501.669252	796984.288454	45.679706
3501.608550	796970.943354	45.684711
3501.607351	796942.220212	45.689716
3501.516368	796949.501936	45.694721
3501.582963	796930.636620	45.699725
3501.564045	796943.749361	45.704730
3501.794630	796933.498595	45.709735
3502.044444	796894.275637	45.714740
3501.624529	796904.508495	45.719745
3501.516012	796892.251321	45.724749
3501.616483	796862.136300	45.729754
3501.211908	796856.458171	45.734759
3501.647467	796836.058815	45.739764
3501.245031	796845.061366	45.744769
3501.636999	796826.682281	45.749773
3501.748001	796845.616774	45.754778
3501.413503	796816.358809	45.759783
3501.818404	796781.970642	45.764788
3501.358198	796780.426089	45.769793
3501.664099	796788.673727	45.774797
3501.580307	796786.527065	45.779802
3501.351857	796776.940890	45.784807
3501.627504	796754.456295	45.789812
3501.691570	796679.958955	45.794817
3501.634496	796559.619225	45.799821
3501.425075	796379.789059	45.804826
3501.739342	796133.428659	45.809831
3501.547959	795851.490995	45.814836
3501.356860	795482.126683	45.819841
3501.011663	795069.450881	45.824845
3501.108098	794604.762531	45.829850
3500.609755	794070.440711	45.834855
3500.513418	793488.755075	45.839860
3499.934297	792855.270782	45.844865
3499.796675	792136.411117	45.849869
3499.374954	791387.452472	45.854874
3498.901819	790574.830855	45.859879
3499.247219	789683.242977	45.864884
3498.413857	788751.429069	45.869889
3498.109949	787751.658894	45.874893
3497.626056	786684.611157	45.879898
3497.109184	785568.821458	45.884903
3496.806043	784365.910385	45.889908
3495.975149	783137.844803	45.894913
3495.848116	781803.173645	45.899917
3495.076796	780446.757754	45.904922
3494.457227	779001.511144	45.909927
3493.845109	777500.195168	45.914932
3492.877463	775935.991192	45.919937
3492.323255	774320.751628	45.924941
3491.582992	772627.594462	45.929946
3490.779380	770879.607936	45.934951
3490.175802	769068.184428	45.939956
3488.781669	767221.347623	45.944961
3488.554054	765270.696721	45.949965
3487.477477	763282.091463	45.954970
3486.657402	761231.638383	45.959975
3485.960946	759109.243472	45.964980
3485.018073	756931.695978	45.969985
3483.761613	754690.518503	45.974989
3482.779632	752399.344079	45.979994
3481.650905	750019.955685	45.984999
3480.965063	747607.885422	45.990004
3479.547155	745134.326860	45.995009
3478.467223	742585.893914	46.000013
3477.014387	739996.824533	46.005018
3475.952116	737339.836720	46.010023
3474.872998	734636.125769	46.015028
3473.587549	731865.475302	46.020033
3472.555058	729025.617172	46.025037
3471.414637	726157.185551	46.030042
3469.857953	723198.582770	46.035047
3468.933725	720195.225540	46.040052
3467.030870	717134.340306	46.045057
3465.915235	714019.899895	46.050061
3464.472623	710851.045014	46.055066
3462.838189	707638.132984	46.060071
3461.395513	704335.397438	46.065076
3459.733826	701008.975291	46.070081
3458.425226	697622.654785	46.075085
3456.860825	694173.145895	46.080090
3455.077318	690659.584983	46.085095
3454.035718	687104.304031	46.090100
3451.794754	683493.791256	46.095105
3450.769048	679818.578873	46.100109
3449.058559	676111.515781	46.105114
3447.483171	672316.944622	46.110119
3445.541640	668494.270947	46.115124
3443.536069	664616.728318	46.120129
3441.842393	660668.878305	46.125133
3440.324599	656692.030331	46.130138
3438.747582	652647.632623	46.135143
3437.034176	648543.382211	46.140148
3434.741105	644384.999293	46.145153
3432.858393	640180.629299	46.150157
3431.042322	635927.541084	46.155162
3428.871939	631622.561767	46.160167
3427.225121	627266.858029	46.165172
3425.033583	622870.438648	46.170177
3422.709165	618396.264453	46.175181
3420.951247	613904.580763	46.180186
3418.259333	609335.986668	46.185191
3416.518054	604744.611387	46.190196
3414.345099	600081.325158	46.195201
3412.276188	595394.051782	46.200205
3409.855448	590642.514719	46.205210
3407.874556	585854.687806	46.210215
3405.834165	581008.814330	46.215220
3403.170569	576114.508579	46.220225
3400.822310	571196.000859	46.225229
3398.428977	566221.232047	46.230234
3396.114829	561192.466932	46.235239
3393.727588	556137.214603	46.240244
3391.284278	551018.629832	46.245249
3388.913367	545860.406325	46.250253
3386.566767	540660.072748	46.255258
3384.161911	535414.706911	46.260263
3381.558995	530126.946005	46.265268
3378.958483	524795.487942	46.270273
3376.501520	519431.770076	46.275277
3374.072021	514011.915978	46.280282
3371.124516	508574.670377	46.285287
3368.964091	503070.893076	46.290292
3365.793249	497541.172599	46.295297
3363.186406	491963.458808	46.300301
3360.523601	486353.745949	46.305306
3357.810502	480697.769753	46.310311
3355.407619	475013.606179	46.315316
3352.148374	469293.970645	46.320321
3349.643647	463530.099769	46.325325
3346.551854	457724.962138	46.330330
3343.510976	451907.927821	46.335335
3340.930733	446030.530936	46.340340
3338.174922	440124.536775	46.345345
3335.341246	434187.776446	46.350349
3332.095788	428206.933214	46.355354
3328.965772	422223.092278	46.360359
3326.267166	416180.974104	46.365364
3323.016384	410122.077841	46.370369
3319.994135	404020.813684	46.375373
3316.861284	397886.769432	46.380378
3313.766321	391733.757414	46.385383
3310.623717	385542.316193	46.390388
3307.239969	379345.438403	46.395393
3303.696505	373108.202430	46.400397
3300.644316	366847.172803	46.405402
3297.333098	360578.267408	46.410407
3294.585013	354272.329189	46.415412
3291.352983	347926.039199	46.420417
3287.848042	341546.991991	46.425421
3284.575209	335172.898849	46.430426
3281.286695	328754.435173	46.435431
3277.958777	322322.355146	46.440436
3274.437646	315891.358521	46.445441
3271.102072	309413.302174	46.450445
3267.617428	302924.707708	46.455450
3263.567650	296437.574619	46.460455
3260.562525	289906.146905	46.465460
3257.000597	283385.986761	46.470465
3253.207430	276826.200380	46.475469
3249.760537	270263.966534	46.480474
3245.942258	263675.353977	46.485479
3242.505687	257088.220862	46.490484
3238.529388	250492.397943	46.495489
3234.886788	243881.775912	46.500493
3231.027700	237262.883639	46.505498
3227.295412	230634.590295	46.510503
3223.611725	223998.610892	46.515508
3219.482583	217379.849191	46.520513
3215.629277	210665.514233	46.525517
3211.852683	203987.125625	46.530522
3207.916187	197343.576897	46.535527
3203.826357	190678.842585	46.540532
3199.789463	184022.452314	46.545537
3195.893848	177376.242326	46.550541
3191.719218	170717.832804	46.555546
3187.121269	164072.777620	46.560551
3183.229210	157434.229389	46.565556
3178.985328	150798.426091	46.570561
3174.761492	144169.026018	46.575565
3170.445631	137553.552067	46.580570
3165.864619	130953.240275	46.585575
3161.133221	124368.527835	46.590580
3156.723264	117784.040741	46.595585
3151.944988	111225.883474	46.600589
3147.349581	104694.372731	46.605594
3142.511670	98169.142058	46.610599
3137.642973	91704.844991	46.615604
3132.014605	85248.598781	46.620609
3126.481387	78834.041197	46.625613
3120.844486	72481.637266	46.630618
3113.604342	66171.706885	46.635623
3102.618191	60062.688040	46.640628
3085.158440	54212.041836	46.645633
3068.469729	48542.055957	46.650637
3051.496115	43120.620945	46.655642
3035.143880	37951.423055	46.660647
3019.550111	33042.449213	46.665652
3004.406881	28440.227320	46.670657
2990.019334	24119.375913	46.675661
2976.389339	20083.318413	46.680666
2962.751125	16338.349523	46.685671
2950.260611	12839.644799	46.690676
2937.842974	9638.105188	46.695681
2926.002657	6663.648032	46.700685
2913.749618	3971.999709	46.705690
2900.690451	1547.785131	46.710695
2855.031479	268.492875	46.715700
2780.739328	297.824436	46.720705
2742.366689	292.084826	46.725709
2736.163121	275.969961	46.730714
2750.149334	282.908748	46.735719
2771.877183	287.232253	46.740724
2790.555143	283.722409	46.745729
2802.827323	273.034059	46.750733
2807.606461	280.415632	46.755738
2806.507533	262.207783	46.760743
2802.744035	269.816624	46.765748
2797.545651	267.889435	46.770753
2792.812707	286.101680	46.775757
2790.053143	276.106706	46.780762
2787.241901	262.647361	46.785767
2784.914355	259.286745	46.790772
2782.252638	271.097576	46.795777
2779.441134	267.600188	46.800781
2777.013100	265.135292	46.805786
2773.821943	273.468462	46.810791
2771.013302	254.656444	46.815796
2768.053391	272.819966	46.820801
2764.914952	275.392620	46.825805
2761.875638	255.557358	46.830810
2758.408986	269.467173	46.835815
2755.804037	260.734631	46.840820
2752.291962	264.171973	46.845825
2748.928027	251.136652	46.850829
2745.718262	249.464724	46.855834
2742.306058	263.379373	46.860839
2739.427874	250.804429	46.865844
2736.079403	257.171910	46.870849
2732.570601	259.122618	46.875853
2729.578641	241.561669	46.880858
2726.027693	252.213452	46.885863
2722.592416	239.976230	46.890868
2719.438313	248.827569	46.895873
2715.864296	247.797302	46.900877
2712.804170	240.722720	46.905882
2709.462285	252.031244	46.910887
2705.999054	241.553092	46.915892
2702.390888	247.511244	46.920897
2698.938023	244.986749	46.925901
2695.765886	237.070141	46.930906
2691.973329	238.440178	46.935911
2689.234607	239.248147	46.940916
2685.417782	234.471598	46.945921
2682.236926	244.523596	46.950925
2679.217601	233.896999	46.955930
2675.353938	234.190461	46.960935
2671.674138	233.791117	46.965940
2668.631515	231.789080	46.970945
2665.694095	229.644303	46.975949
2662.241888	224.522924	46.980954
2658.384777	232.124450	46.985959
2655.030482	225.046411	46.990964
2651.027206	236.694753	46.995969
2647.822959	235.639069	47.000973
2644.365558	232.134978	47.005978
2640.869524	235.344774	47.010983
2637.317139	232.041037	47.015988
2634.206771	240.774394	47.020993
2631.040472	234.940728	47.025997
2627.549238	231.295914	47.031002
2623.581498	237.704069	47.036007
2620.527317	230.952155	47.041012
2616.761689	238.028650	47.046017
2613.549411	228.767673	47.051021
2610.759960	232.940600	47.056026
2606.679909	241.062930	47.061031
2603.197443	236.671214	47.066036
2599.709059	226.588559	47.071041
2595.970877	225.908526	47.076045
2592.382687	226.689858	47.081050
2589.185707	237.417095	47.086055
2586.017660	239.556846	47.091060
2582.460146	221.559163	47.096065
2578.638182	235.848524	47.101069
2576.067927	219.265715	47.106074
2572.311276	241.669643	47.111079
2568.556311	221.254040	47.116084
2565.130147	229.807340	47.121089
2561.636142	231.185038	47.126093
2558.162728	229.999050	47.131098
2554.284682	231.234964	47.136103
2551.141218	239.427530	47.141108
2547.691668	229.985405	47.146113
2544.140633	234.811755	47.151117
2540.512035	219.039429	47.156122
2536.946078	227.849313	47.161127
2534.009413	227.789714	47.166132
2530.417886	232.855187	47.171137
2526.955652	230.729028	47.176141
2523.467871	214.752261	47.181146
2519.939870	219.647038	47.186151
2516.407524	212.840740	47.191156
2513.044091	227.008532	47.196161
2509.121868	219.388068	47.201165
2506.223437	211.122666	47.206170
2502.376874	212.082004	47.211175
2499.224636	214.494041	47.216180
2495.462851	213.811636	47.221185
2491.725358	217.752607	47.226189
2488.517135	210.155604	47.231194
2484.793377	224.608451	47.236199
2481.488576	208.198129	47.241204
2478.328599	215.622414	47.246209
2475.114099	209.343248	47.251213
2471.561456	210.225621	47.256218
2467.502385	215.590490	47.261223
2463.972418	202.536582	47.266228
2460.406079	211.971550	47.271233
2457.121543	204.683520	47.276237
2453.955496	204.785890	47.281242
2450.161634	210.796260	47.286247
2446.513512	202.966376	47.291252
2442.931299	213.512888	47.296257
2439.217896	213.985913	47.301261
2436.309406	199.759984	47.306266
2432.555417	217.782551	47.311271
2429.285526	193.901628	47.316276
2425.865660	195.478090	47.321281
2422.362826	209.888888	47.326285
2418.770301	208.880760	47.331290
2415.445232	205.123513	47.336295
2411.861852	200.458391	47.341300
2408.243853	214.347246	47.346305
2404.708717	203.676530	47.351309
2401.679886	209.235878	47.356314
2398.060408	201.780442	47.361319
2394.234033	196.904022	47.366324
2390.808352	197.775459	47.371329
2387.113591	206.764284	47.376333
2383.973245	203.866981	47.381338
2380.482149	204.844810	47.386343
2376.769056	209.104518	47.391348
2373.466449	214.918675	47.396353
2369.929036	212.263753	47.401357
2366.754316	213.832962	47.406362
2362.917724	205.073075	47.411367
2359.417860	207.132373	47.416372
2356.019063	205.373403	47.421377
2352.329710	209.454582	47.426381
2348.794070	206.686316	47.431386
2345.103390	200.622685	47.436391
2342.102716	205.233544	47.441396
2338.911785	197.716249	47.446401
2334.820222	204.461931	47.451405
2331.761686	195.710099	47.456410
2327.327666	209.387066	47.461415
2324.413508	201.856195	47.466420
2320.827250	195.028811	47.471425
2317.325034	197.377188	47.476429
2314.298106	201.735776	47.481434
2310.579085	213.633332	47.486439
2307.308722	202.296473	47.491444
2303.557741	201.429668	47.496449
2299.805995	203.387280	47.501453
2296.545977	195.960328	47.506458
2292.870003	195.971648	47.511463
2289.645189	189.576189	47.516468
2286.080307	194.912811	47.521473
2282.813074	194.777896	47.526477
2278.942174	191.381556	47.531482
2275.453411	195.468061	47.536487
2272.313349	190.158277	47.541492
2268.773840	191.490529	47.546497
2264.688767	191.613631	47.551501
2261.709779	187.741965	47.556506
2257.725948	197.774268	47.561511
2254.641390	178.030837	47.566516
2251.291564	193.745757	47.571521
2247.503309	198.468883	47.576525
2244.294491	185.534512	47.581530
2240.417251	200.664270	47.586535
2236.946971	195.234930	47.591540
2233.656336	189.560003	47.596545
2229.731619	198.712010	47.601549
2226.764436	190.292147	47.606554
2223.092975	186.376462	47.611559
2219.702359	183.896402	47.616564
2216.267112	186.457828	47.621569
2212.586774	184.476324	47.626573
2208.865955	193.046169	47.631578
2205.725431	191.004244	47.636583
2202.068886	183.041132	47.641588
2198.421039	191.417117	47.646593
2195.175434	186.778388	47.651597
2191.704123	178.365534	47.656602
2187.985480	190.552814	47.661607
2184.524948	182.936130	47.666612
2181.344591	191.037699	47.671617
2177.425321	185.487699	47.676621
2173.749959	186.525611	47.681626
2170.179413	187.292982	47.686631
2167.194478	177.270721	47.691636
2163.857475	191.443695	47.696641
2159.885844	178.660848	47.701645
2156.865607	185.440042	47.706650
2153.202080	191.352972	47.711655
2150.084433	182.556628	47.716660
2145.951737	180.324004	47.721665
2142.422080	200.819693	47.726669
2139.278892	188.717981	47.731674
2135.710761	193.119628	47.736679
2132.004393	183.774782	47.741684
2128.541897	192.237724	47.746689
2124.877081	187.577607	47.751693
2121.404582	176.440650	47.756698
2117.767185	179.850080	47.761703
2114.663312	188.724964	47.766708
2111.304128	177.073269	47.771713
2107.567008	186.006335	47.776717
2104.076208	172.819831	47.781722
2100.536818	182.071999	47.786727
2097.416983	179.611658	47.791732
2093.862485	170.705779	47.796737
2090.104589	182.834450	47.801741
2086.682120	169.025307	47.806746
2082.980955	187.418769	47.811751
2079.930426	186.914043	47.816756
2076.355756	174.219881	47.821761
2072.067699	174.658240	47.826765
2069.058893	175.229407	47.831770
2065.368665	174.932714	47.836775
2061.877177	178.207604	47.841780
2058.543957	183.275443	47.846785
2054.787821	176.185987	47.851789
2051.670861	187.166532	47.856794
2048.133408	183.094760	47.861799
2044.767927	182.104712	47.866804
2041.646534	181.723571	47.871809
2037.585713	186.326006	47.876813
2034.564206	180.123365	47.881818
2030.580250	188.767862	47.886823
2027.127191	168.804395	47.891828
2023.684873	170.227573	47.896833
2019.855693	178.547310	47.901837
2016.797603	169.585339	47.906842
2012.969274	179.978723	47.911847
2009.394842	174.004442	47.916852
2006.079356	173.366069	47.921857
2002.205428	176.587756	47.926861
1998.982721	166.335378	47.931866
1995.473423	169.395989	47.936871
1992.136648	173.799781	47.941876
1988.514586	174.816461	47.946881
1985.221340	181.957834	47.951885
1981.780312	171.149136	47.956890
1978.168934	177.404064	47.961895
1974.425400	172.358542	47.966900
1970.942846	179.737540	47.971905
1967.399917	177.367575	47.976909
1964.102320	172.182690	47.981914
1960.565584	172.315935	47.986919
1957.090321	168.970831	47.991924
1953.605268	168.232102	47.996929
1949.998561	173.980157	48.001933
1946.595238	170.185840	48.006938
1942.963944	170.014846	48.011943
1939.557673	180.716493	48.016948
1936.475046	174.131918	48.021953
1932.485774	181.407175	48.026957
1929.415119	173.262133	48.031962
1925.379216	175.298965	48.036967
1921.743275	175.604869	48.041972
1918.362155	173.453992	48.046977
1915.155634	174.172873	48.051981
1912.030325	175.375889	48.056986
1908.308653	176.942285	48.061991
1904.435222	169.090114	48.066996
1901.058637	164.063222	48.072001
1897.188342	174.087393	48.077005
1894.041140	170.150316	48.082010
1890.391657	170.507108	48.087015
1887.236964	173.792809	48.092020
1883.739087	175.479458	48.097025
1879.869441	180.168919	48.102029
1876.940266	171.113139	48.107034
1872.988477	181.452365	48.112039
1869.318362	172.239430	48.117044
1866.010123	174.461095	48.122049
1862.117177	172.994130	48.127053
1859.105269	185.363666	48.132058
1855.411636	182.338771	48.137063
1852.289349	170.948955	48.142068
1848.677100	176.001644	48.147073
1844.723818	176.898218	48.152077
1841.579940	167.665964	48.157082
1837.853395	169.800775	48.162087
1834.541022	161.366645	48.167092
1831.547773	167.499525	48.172097
1827.221008	171.488782	48.177101
1824.420307	168.588190	48.182106
1820.759028	178.327222	48.187111
1816.987108	164.283680	48.192116
1813.605040	167.514481	48.197121
1809.793180	181.045106	48.202125
1806.475637	165.369787	48.207130
1802.582497	174.763302	48.212135
1799.314963	167.483384	48.217140
1796.167856	161.127852	48.222145
1792.716972	173.023360	48.227149
1789.222373	164.716793	48.232154
1785.223574	167.576102	48.237159
1782.019201	174.789801	48.242164
1778.640875	171.255650	48.247169
1774.902992	170.009398	48.252173
1771.490647	152.140323	48.257178
1768.068478	171.388474	48.262183
1764.413308	166.124175	48.267188
1761.113086	162.584745	48.272193
1757.062302	170.387687	48.277197
1753.840726	164.993053	48.282202
1750.282822	180.114776	48.287207
1747.106079	159.849414	48.292212
1743.370751	169.972233	48.297217
1740.012046	179.902198	48.302221
1736.430774	173.225670	48.307226
1732.812672	175.705503	48.312231
1729.511694	183.285991	48.317236
1726.284047	173.757141	48.322241
1722.403742	176.556681	48.327245
1718.882459	176.885401	48.332250
1715.174729	180.201157	48.337255
1711.882214	172.633477	48.342260
1708.179817	169.777335	48.347265
1705.008877	172.834537	48.352269
1701.967851	162.180213	48.357274
1697.997532	168.604192	48.362279
1694.418289	160.048727	48.367284
1691.181319	150.161351	48.372289
1687.481777	167.041933	48.377293
1684.154131	150.886234	48.382298
1680.290610	164.072720	48.387303
1676.838483	163.446392	48.392308
1673.176850	162.836385	48.397313
1669.735690	175.726280	48.402317
1666.411957	162.270484	48.407322
1662.809790	167.366775	48.412327
1659.380849	169.527251	48.417332
1656.016939	163.907438	48.422337
1652.102643	174.188084	48.427341
1648.808644	162.588859	48.432346
1645.428163	167.741907	48.437351
1642.220452	166.909817	48.442356
1638.265116	164.546612	48.447361
1634.823553	168.931931	48.452365
1631.319443	145.935785	48.457370
1627.976264	165.122492	48.462375
1624.483211	155.577423	48.467380
1621.057672	160.133047	48.472385
1617.324590	158.452688	48.477389
1614.119990	160.589582	48.482394
1610.183942	162.597969	48.487399
1606.592833	160.942036	48.492404
1603.542809	153.842002	48.497409
1599.773098	164.794733	48.502413
1596.343365	160.019766	48.507418
1592.897428	157.060400	48.512423
1589.383415	166.888969	48.517428
1585.948711	161.506901	48.522433
1582.147965	165.210696	48.527437
1578.834191	161.175868	48.532442
1575.272250	174.175010	48.537447
1571.604176	162.445672	48.542452
1568.138017	159.979291	48.547457
1564.695553	168.424334	48.552461
1561.600802	164.500074	48.557466
1557.532038	158.802080	48.562471
1554.301142	172.506949	48.567476
1551.159264	168.231160	48.572481
1547.013636	157.246586	48.577485
1543.937825	157.488757	48.582490
1540.154894	158.549864	48.587495
1536.630167	157.732649	48.592500
1533.206580	157.791690	48.597505
1529.651897	145.742480	48.602509
1526.739131	141.343267	48.607514
1523.188975	155.587592	48.612519
1519.397543	147.452313	48.617524
1515.732840	154.471257	48.622529
1512.088731	157.005110	48.627533
1508.810504	151.325760	48.632538
1505.176247	160.044282	48.637543
1502.069501	149.426276	48.642548
1498.384398	152.454464	48.647553
1494.518838	143.481605	48.652557
1490.936111	161.680660	48.657562
1487.701864	152.962823	48.662567
1484.524112	145.848021	48.667572
1481.079499	154.778837	48.672577
1477.241389	166.663774	48.677581
1473.942293	163.128445	48.682586
1470.429725	166.453940	48.687591
1466.438852	159.045952	48.692596
1463.190671	151.309601	48.697601
1459.538457	153.538092	48.702605
1456.237173	157.112361	48.707610
1452.742669	150.634392	48.712615
1449.105548	148.237627	48.717620
1445.767900	157.874751	48.722625
1442.037977	169.688180	48.727629
1438.531599	154.149341	48.732634
1435.296332	157.911518	48.737639
1431.806990	162.395574	48.742644
1428.205456	151.238518	48.747649
1424.383895	157.696678	48.752653
1421.482671	157.796435	48.757658
1417.908858	154.120114	48.762663
1414.211061	167.147256	48.767668
1410.593144	154.688272	48.772673
1406.937218	168.765814	48.777677
1403.559529	167.823373	48.782682
1400.156579	162.681427	48.787687
1396.780526	154.957631	48.792692
1393.172827	157.118825	48.797697
1389.599145	151.059045	48.802701
1386.477605	158.632335	48.807706
1382.421404	154.457619	48.812711
1379.127713	147.103723	48.817716
1375.563285	149.541422	48.822721
1371.898820	164.162305	48.827725
1368.703337	151.735344	48.832730
1365.144301	155.718013	48.837735
1361.573119	152.033890	48.842740
1358.122439	153.628447	48.847745
1354.529687	160.356785	48.852749
1351.271661	144.883474	48.857754
1347.551981	160.257941	48.862759
1344.171374	159.679563	48.867764
1340.750169	143.627538	48.872769
1336.884828	156.017704	48.877773
1333.507698	151.606530	48.882778
1330.145276	151.181233	48.887783
1326.546352	153.353146	48.892788
1323.683114	157.910207	48.897793
1319.851350	161.903089	48.902797
1316.534594	150.166254	48.907802
1312.902047	150.717563	48.912807
1308.638381	156.462851	48.917812
1305.451821	147.193747	48.922817
1301.749359	145.810300	48.927821
1298.498372	146.044201	48.932826
1294.762222	142.784835	48.937831
1291.223862	148.367988	48.942836
1288.075036	138.917259	48.947841
1284.594024	157.347312	48.952845
1281.103788	139.129173	48.957850
1277.503450	155.079256	48.962855
1274.261604	150.489807	48.967860
1271.128914	138.241083	48.972865
1266.918875	149.987214	48.977869
1263.814379	144.017190	48.982874
1260.474183	151.747469	48.987879
1256.433282	155.922493	48.992884
1252.548461	148.307823	48.997889
1249.155430	152.790662	49.002893
1246.010788	148.578626	49.007898
1242.496980	150.711275	49.012903
1239.013772	151.044012	49.017908
1235.812018	140.395180	49.022913
1232.025404	152.064924	49.027917
1228.325784	150.329337	49.032922
1225.122915	154.183924	49.037927
1221.756024	145.060656	49.042932
1218.384689	136.350120	49.047937
1214.449066	151.623633	49.052941
1210.708164	151.218153	49.057946
1207.680943	153.235178	49.062951
1204.192974	156.215086	49.067956
1200.456225	144.715077	49.072961
1196.714034	148.480824	49.077965
1193.279543	146.498850	49.082970
1190.095929	148.143421	49.087975
1186.677196	155.857001	49.092980
1183.142186	143.141794	49.097985
1179.270164	137.373593	49.102989
1175.896291	144.501244	49.107994
1172.798754	135.088287	49.112999
1169.122661	160.247294	49.118004
1165.430290	150.345813	49.123009
1161.882848	154.233828	49.128013
1158.272136	150.461437	49.133018
1155.124282	143.645936	49.138023
1151.519188	150.983136	49.143028
1147.892402	144.298693	49.148033
1143.967494	146.699626	49.153037
1140.375928	143.673975	49.158042
1137.283007	147.793197	49.163047
1133.902465	145.239709	49.168052
1130.749032	149.790978	49.173057
1126.849241	142.948285	49.178061
1123.607988	140.571786	49.183066
1120.321372	138.052524	49.188071
1116.436387	141.849481	49.193076
1113.209086	141.881258	49.198081
1109.400325	132.587428	49.203085
1105.854103	149.182231	49.208090
1102.532267	142.960783	49.213095
1098.602392	141.924773	49.218100
1095.627436	136.653646	49.223105
1091.860276	145.253299	49.228109
1088.160301	143.903892	49.233114
1084.634104	137.225772	49.238119
1081.209966	148.718435	49.243124
1078.194080	133.114868	49.248129
1074.481166	141.069336	49.253133
1070.797965	144.528057	49.258138
1067.559809	136.956119	49.263143
1063.787804	142.593436	49.268148
1060.604198	134.657530	49.273153
1056.792746	144.656653	49.278157
1053.348589	134.883571	49.283162
1049.826220	155.058158	49.288167
1046.235024	143.835026	49.293172
1043.004201	138.832286	49.298177
1039.432473	144.976892	49.303181
1035.581499	134.762609	49.308186
1032.186520	138.484433	49.313191
1028.880320	149.178061	49.318196
1025.465574	121.171788	49.323201
1021.888820	153.109281	49.328205
1018.435949	151.499013	49.333210
1014.705362	136.549183	49.338215
1011.067375	148.595520	49.343220
1007.747051	145.555152	49.348225
1004.094051	145.950373	49.353229
1000.882886	143.926597	49.358234
997.683903	140.045873	49.363239
994.065726	142.971906	49.368244
990.781584	139.133462	49.373249
986.726923	141.725000	49.378253
983.307876	139.929613	49.383258
979.740316	147.067128	49.388263
976.028491	137.165341	49.393268
972.649593	136.074150	49.398273
969.584602	140.210335	49.403277
966.064869	149.504779	49.408282
962.278967	142.840505	49.413287
958.538525	150.586576	49.418292
955.117322	146.971742	49.423297
951.936799	138.994245	49.428301
948.260712	143.466634	49.433306
944.773646	150.065135	49.438311
941.246340	144.039893	49.443316
937.912286	139.317568	49.448321
934.057558	152.955833	49.453325
930.637438	136.418523	49.458330
926.892387	139.688539	49.463335
923.220045	150.985864	49.468340
920.327659	151.250116	49.473345
916.846551	150.956300	49.478349
913.283495	148.697462	49.483354
909.949765	142.541423	49.488359
906.175575	141.461274	49.493364
903.103023	134.167722	49.498369
899.260485	145.247305	49.503373
895.749492	140.261209	49.508378
892.196694	137.377380	49.513383
888.053493	143.075681	49.518388
885.035091	140.398205	49.523393
881.805951	139.169174	49.528397
878.208134	141.666596	49.533402
875.077620	137.424499	49.538407
871.317275	144.870330	49.543412
868.157917	129.908865	49.548417
864.028869	143.864740	49.553421
860.845115	132.439300	49.558426
856.952329	137.321421	49.563431
853.336935	145.776455	49.568436
850.191437	135.617073	49.573441
846.594483	134.923727	49.578445
843.009638	140.496113	49.583450
839.629510	138.966568	49.588455
836.082927	126.336879	49.593460
832.791890	125.169988	49.598465
828.764992	138.388619	49.603469
825.599699	132.324291	49.608474
822.359015	131.702058	49.613479
818.943629	130.732301	49.618484
815.356333	125.359792	49.623489
811.703492	145.126139	49.628493
807.919421	129.456917	49.633498
804.720303	135.682756	49.638503
801.169432	142.329246	49.643508
797.984414	128.342053	49.648513
794.024871	132.787133	49.653517
790.893505	133.598885	49.658522
787.076092	134.888462	49.663527
783.127045	136.138218	49.668532
780.058022	138.514627	49.673537
776.461698	125.163236	49.678541
773.270215	135.431347	49.683546
769.867831	143.131545	49.688551
766.082344	131.647977	49.693556
762.594093	137.298764	49.698561
759.020537	138.981879	49.703565
755.554420	134.359008	49.708570
752.024079	126.004622	49.713575
748.569310	132.410227	49.718580
745.246950	130.670428	49.723585
741.385457	126.347661	49.728589
737.831445	127.575418	49.733594
734.599136	128.294752	49.738599
730.901736	131.434074	49.743604
727.624527	126.291579	49.748609
723.827379	137.253442	49.753613
720.623060	128.448538	49.758618
717.550650	129.009965	49.763623
713.478204	130.680781	49.768628
710.031803	137.743652	49.773633
706.372476	134.721251	49.778637
702.824033	120.449833	49.783642
699.823222	129.330847	49.788647
695.872229	132.733748	49.793652
692.576690	131.582173	49.798657
688.857638	140.103528	49.803661
685.548818	132.562025	49.808666
682.300308	131.967001	49.813671
678.391504	138.291550	49.818676
675.131252	124.497798	49.823681
671.357901	129.001479	49.828685
668.000421	129.634870	49.833690
664.465554	129.276863	49.838695
660.899594	135.990429	49.843700
657.650129	121.877137	49.848705
653.940831	125.565906	49.853709
650.633309	133.080105	49.858714
647.063006	126.816393	49.863719
643.447250	130.195231	49.868724
640.093754	125.465138	49.873729
636.235966	134.962050	49.878733
632.758508	123.946934	49.883738
629.291690	134.500799	49.888743
625.929862	141.375712	49.893748
622.569411	119.557982	49.898753
619.287474	122.171080	49.903757
615.327308	116.706177	49.908762
611.974544	137.129988	49.913767
607.922010	126.514121	49.918772
604.843231	130.201382	49.923777
601.474207	130.801197	49.928781
597.973140	128.489682	49.933786
594.504827	134.064544	49.938791
590.858449	128.445323	49.943796
587.673324	125.682964	49.948801
584.045661	140.695238	49.953805
580.376137	119.962008	49.958810
576.984332	134.226876	49.963815
573.167614	131.621818	49.968820
569.707679	126.706212	49.973825
566.498804	135.748908	49.978829
562.849725	132.094290	49.983834
559.548575	125.913345	49.988839
555.886178	137.069183	49.993844
552.359253	123.723257	49.998849
549.035691	125.272847	50.003853
545.396913	132.955652	50.008858
541.684408	128.739912	50.013863
538.296662	133.544605	50.018868
535.023122	124.935533	50.023873
531.364868	132.211055	50.028877
527.953589	123.115181	50.033882
524.629880	134.879636	50.038887
520.743616	129.306789	50.043892
517.498733	120.945654	50.048897
513.976931	128.858553	50.053901
510.391478	121.768523	50.058906
506.867242	117.289770	50.063911
503.107177	134.952821	50.068916
499.868550	130.728976	50.073921
495.984340	124.182074	50.078925
492.713458	119.814890	50.083930
489.147186	126.851584	50.088935
485.546283	127.988168	50.093940
482.199280	119.098061	50.098945
479.112588	126.876062	50.103949
475.499383	129.717384	50.108954
472.135544	134.493298	50.113959
468.314006	139.408255	50.118964
464.653985	131.405964	50.123969
461.296607	126.398600	50.128973
457.579110	121.992641	50.133978
454.521578	128.767045	50.138983
450.720227	131.495521	50.143988
447.369558	124.730589	50.148993
443.851937	121.165319	50.153997
440.217848	125.795481	50.159002
436.936812	126.306952	50.164007
433.092054	134.698149	50.169012
429.837915	121.181955	50.174017
426.260339	127.221953	50.179021
422.939661	119.839826	50.184026
419.564966	113.893387	50.189031
415.736097	121.809301	50.194036
412.372452	105.090312	50.199041
408.615589	130.015793	50.204045
404.805783	117.728910	50.209050
401.694200	114.248719	50.214055
398.008152	130.619719	50.219060
395.094744	118.055329	50.224065
391.235459	125.304141	50.229069
387.657801	121.525760	50.234074
384.279521	123.358832	50.239079
380.622681	128.629311	50.244084
377.536925	117.033296	50.249089
373.782255	128.627093	50.254093
369.895196	129.830645	50.259098
366.705845	122.517323	50.264103
363.005059	119.898375	50.269108
359.839036	116.400463	50.274113
356.079165	125.612099	50.279117
352.741097	119.527940	50.284122
349.257749	113.005388	50.289127
345.408580	127.909017	50.294132
342.168845	119.085329	50.299137
338.476462	125.627254	50.304141
335.055821	115.862589	50.309146
332.003923	116.498744	50.314151
328.273970	124.425592	50.319156
324.788619	112.126706	50.324161
321.448471	121.309564	50.329165
317.711598	115.171445	50.334170
314.359527	115.813100	50.339175
310.271194	124.267875	50.344180
306.877510	112.521817	50.349185
303.830600	125.210602	50.354189
300.263186	116.067665	50.359194
296.721104	104.093381	50.364199
292.892075	119.666923	50.369204
289.773046	111.765589	50.374209
285.926997	119.209577	50.379213
282.595024	124.197060	50.384218
279.174797	110.741956	50.389223
275.354442	131.331999	50.394228
272.081298	115.489005	50.399233
268.534255	123.742698	50.404237
264.725227	120.194895	50.409242
261.721591	119.219958	50.414247
257.936823	123.831304	50.419252
254.963563	112.759979	50.424257
251.210486	122.565533	50.429261
247.558769	118.704269	50.434266
244.316333	110.772642	50.439271
240.446551	121.604162	50.444276
236.867389	115.072252	50.449281
233.079270	114.441810	50.454285
229.715806	122.140145	50.459290
227.284998	111.940710	50.464295
223.249294	119.487986	50.469300
219.927151	114.655680	50.474305
216.049523	121.316075	50.479309
212.098649	119.118264	50.484314
208.925342	122.031082	50.489319
205.466483	123.766374	50.494324
202.214851	120.155719	50.499329
198.602268	120.515998	50.504333
194.915830	122.824989	50.509338
191.421147	113.556753	50.514343
187.898980	119.562355	50.519348
184.741709	114.824471	50.524353
181.457727	119.047580	50.529357
177.723666	112.419560	50.534362
174.108756	108.494254	50.539367
170.051772	118.642868	50.544372
166.910579	118.125972	50.549377
163.665265	118.837868	50.554381
160.023016	117.243183	50.559386
156.479816	118.159586	50.564391
152.745406	113.225553	50.569396
149.533329	111.200987	50.574401
145.854610	119.719974	50.579405
142.453315	125.516210	50.584410
139.151600	118.318862	50.589415
135.324189	117.106393	50.594420
132.158264	108.171001	50.599425
128.611576	108.890389	50.604429
125.147359	111.374118	50.609434
121.548360	117.273962	50.614439
117.554648	122.778508	50.619444
114.620269	123.231974	50.624449
110.879080	112.770836	50.629453
107.478154	125.464319	50.634458
104.472876	115.309946	50.639463
100.364509	116.588997	50.644468
96.844924	107.239801	50.649473
93.355163	117.222808	50.654477
89.663759	126.111314	50.659482
86.539499	112.434788	50.664487
82.829543	125.748289	50.669492
79.232249	113.550246	50.674497
76.357987	110.021244	50.679501
72.345949	112.411334	50.684506
69.093478	109.539427	50.689511
65.298066	108.825252	50.694516
61.885280	120.174360	50.699521
58.444035	108.441261	50.704525
54.844620	116.834719	50.709530
51.520665	116.320754	50.714535
47.478948	123.786844	50.719540
44.252710	112.823348	50.724545
40.820868	117.678475	50.729549
37.078632	111.639294	50.734554
34.012022	117.933038	50.739559
30.539260	118.176387	50.744564
27.224143	119.350939	50.749569
23.780808	116.973486	50.754573
19.839756	121.454913	50.759578
16.509663	115.047725	50.764583
12.532667	124.853700	50.769588
9.517433	126.013234	50.774593
5.836638	113.356088	50.779597
2.395157	128.919587	50.784602