Thu Jun 16 18:58:13 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.000477	96.651801	0.000000
-0.158988	92.441103	0.005005
0.103556	96.953193	0.010010
0.076377	92.738491	0.015014
0.355261	101.170501	0.020019
0.164604	98.653832	0.025024
0.178944	84.426290	0.030029
-0.055111	88.396647	0.035034
-0.382050	64.215699	0.040038
-0.511831	51.675620	0.045043
-0.949673	42.581955	0.050048
-1.498630	29.778402	0.055053
-2.089253	27.213502	0.060058
-1.967084	15.304146	0.065062
-2.557195	17.382434	0.070067
-3.232725	27.802365	0.075072
-3.311484	22.399429	0.080077
-3.510025	21.318019	0.085082
-3.429211	26.181831	0.090086
-3.499868	13.282578	0.095091
-4.215394	23.448569	0.100096
-4.595390	15.625206	0.105101
-4.586024	12.121015	0.110106
-4.922756	25.417163	0.115110
-4.569920	7.820047	0.120115
-5.420859	11.270609	0.125120
-5.804903	9.266755	0.130125
-6.245635	20.505285	0.135130
-6.203859	18.557634	0.140134
-6.264525	20.792499	0.145139
-6.500905	22.562539	0.150144
-7.109902	28.109190	0.155149
-7.539649	26.213909	0.160154
-8.047435	30.085057	0.165158
-7.890217	23.373735	0.170163
-7.877820	16.552081	0.175168
-8.054295	22.513027	0.180173
-7.843159	21.413538	0.185178
-8.252904	24.582933	0.190182
-8.890597	16.902192	0.195187
-9.409170	30.749587	0.200192
-9.555179	24.964131	0.205197
-9.622486	20.376064	0.210202
-9.689505	17.581390	0.215206
-9.694877	20.794550	0.220211
-10.862191	24.107489	0.225216
-11.375169	24.388865	0.230221
-11.221961	25.024220	0.235226
-11.634049	24.110298	0.240230
-11.452815	18.284873	0.245235
-11.483594	20.166056	0.250240
-11.421438	30.989514	0.255245
-11.618795	17.615063	0.260250
-12.448262	23.954728	0.265254
-12.386606	23.746622	0.270259
-12.943585	22.517964	0.275264
-12.873848	17.394542	0.280269
-13.392264	26.561345	0.285274
-14.140538	20.456041	0.290278
-14.306670	17.765450	0.295283
-14.575421	36.738692	0.300288
-14.755636	28.303798	0.305293
-14.583626	27.210676	0.310298
-14.742787	22.879886	0.315302
-14.469084	22.236397	0.320307
-15.331696	23.057777	0.325312
-15.415894	14.115428	0.330317
-16.022166	16.537436	0.335322
-16.075983	11.268104	0.340326
-16.110847	15.834940	0.345331
-17.324527	23.194653	0.350336
-17.355282	16.120176	0.355341
-17.519409	20.273210	0.360346
-17.537939	21.438406	0.365350
-17.654138	17.970552	0.370355
-17.502493	22.239313	0.375360
-17.704053	25.759648	0.380365
-17.957039	17.667575	0.385370
-18.878995	24.957178	0.390374
-18.954168	32.291823	0.395379
-19.094559	23.743114	0.400384
-19.300233	16.612601	0.405389
-19.999120	23.334973	0.410394
-20.428839	22.723974	0.415398
-20.408100	16.323478	0.420403
-20.608719	27.025211	0.425408
-20.955603	19.111435	0.430413
-20.740369	19.743050	0.435418
-20.823848	19.592471	0.440422
-20.957758	24.802825	0.445427
-21.673129	14.456751	0.450432
-22.146103	12.801343	0.455437
-22.323190	14.931931	0.460442
-22.493892	22.046081	0.465446
-22.185415	11.706808	0.470451
-23.122257	23.743951	0.475456
-23.461415	25.477802	0.480461
-24.011898	21.154858	0.485466
-24.337775	23.478243	0.490470
-23.963499	9.657235	0.495475
-24.414945	23.818891	0.500480
-24.154301	15.538942	0.505485
-24.306726	18.539633	0.510490
-24.431309	32.880203	0.515494
-25.044439	21.848252	0.520499
-25.580695	26.880731	0.525504
-25.691856	28.532903	0.530509
-25.607006	12.926919	0.535514
-26.320377	18.696807	0.540518
-26.820758	24.815757	0.545523
-27.214920	30.569595	0.550528
-27.458739	14.346287	0.555533
-27.390157	24.662974	0.560538
-27.877446	21.145164	0.565542
-27.480412	21.892940	0.570547
-27.339529	20.471116	0.575552
-27.646291	27.931537	0.580557
-28.371717	20.439225	0.585562
-29.050269	25.401892	0.590566
-28.955282	13.868368	0.595571
-29.094520	19.196308	0.600576
-29.057922	17.758472	0.605581
-29.811750	22.087983	0.610586
-30.484267	14.729289	0.615590
-30.058183	3.629395	0.620595
-30.555097	17.256354	0.625600
-30.430986	17.666257	0.630605
-30.188390	17.919942	0.635610
-31.346946	14.872762	0.640614
-31.521813	20.345101	0.645619
-31.674119	12.981432	0.650624
-31.964967	18.641933	0.655629
-31.816508	10.515486	0.660634
-32.727446	25.438728	0.665638
-33.017024	18.027994	0.670643
-33.167107	28.642254	0.675648
-33.627053	22.587661	0.680653
-33.380819	20.190393	0.685658
-33.152428	23.801763	0.690662
-33.578899	20.868592	0.695667
-34.661693	25.399959	0.700672
-35.053703	27.922605	0.705677
-35.182048	18.345903	0.710682
-35.200344	16.929470	0.715686
-35.327755	30.150579	0.720691
-35.385140	19.146456	0.725696
-35.657076	21.968997	0.730701
-35.364568	17.948714	0.735706
-36.184988	22.228460	0.740710
-36.645304	11.012628	0.745715
-36.726380	25.073319	0.750720
-37.006327	14.550419	0.755725
-36.871181	24.675567	0.760730
-37.470160	21.264216	0.765734
-37.991795	13.123810	0.770739
-38.276362	22.985065	0.775744
-38.354382	21.265176	0.780749
-38.812686	27.399765	0.785754
-38.735449	22.047114	0.790758
-38.773454	20.866072	0.795763
-38.772425	20.434568	0.800768
-38.972055	30.943664	0.805773
-39.864800	32.377838	0.810778
-39.951425	30.319406	0.815782
-39.882735	26.445615	0.820787
-40.547297	32.900293	0.825792
-41.161106	32.226588	0.830797
-41.497363	29.940281	0.835802
-41.352199	22.969519	0.840806
-41.571957	31.806690	0.845811
-41.594291	33.322838	0.850816
-41.299552	26.225247	0.855821
-41.848049	17.071954	0.860826
-42.661144	31.008271	0.865830
-42.791323	22.309600	0.870835
-43.136471	24.259606	0.875840
-43.204538	29.445661	0.880845
-43.304356	21.256062	0.885850
-43.928632	30.404451	0.890854
-44.702674	22.774659	0.895859
-44.763161	25.397109	0.900864
-44.707309	28.866617	0.905869
-45.153404	19.396490	0.910874
-44.829571	34.787712	0.915878
-44.781016	22.554899	0.920883
-44.940980	22.988762	0.925888
-45.349028	21.813826	0.930893
-45.557192	24.878186	0.935898
-46.413678	31.318017	0.940902
-46.079186	14.308261	0.945907
-47.360136	17.207285	0.950912
-47.678435	17.357146	0.955917
-47.513198	26.155549	0.960922
-47.461361	20.417213	0.965926
-47.633137	25.054228	0.970931
-47.725790	32.771383	0.975936
-47.910170	25.925126	0.980941
-48.172353	23.875484	0.985946
-49.287910	33.595872	0.990950
-49.377771	25.296993	0.995955
-49.843258	49.688308	1.000960
-49.731700	31.188696	1.005965
-49.613491	22.999468	1.010970
-49.928908	33.760031	1.015974
-49.648938	30.222856	1.020979
-50.002735	23.638706	1.025984
-51.463290	28.903060	1.030989
-51.155657	19.762674	1.035994
-51.334815	23.168024	1.040998
-51.379404	24.002595	1.046003
-51.178017	20.389225	1.051008
-52.037391	21.373051	1.056013
-52.505861	19.395188	1.061018
-52.966569	27.001113	1.066022
-53.063064	26.528606	1.071027
-53.011981	26.070678	1.076032
-53.085558	13.489977	1.081037
-52.806643	24.603754	1.086042
-53.850518	21.006174	1.091046
-54.235374	21.358621	1.096051
-54.459106	21.268710	1.101056
-54.256673	23.711071	1.106061
-54.583764	12.672803	1.111066
-55.177763	11.688617	1.116070
-55.368303	15.144088	1.121075
-55.489580	18.455621	1.126080
-55.665254	16.269846	1.131085
-55.602605	17.399428	1.136090
-56.293121	29.826396	1.141094
-57.092974	21.576193	1.146099
-57.549852	27.538888	1.151104
-56.932691	30.393059	1.156109
-57.078718	24.381298	1.161114
-57.675313	35.624383	1.166118
-57.386281	29.805213	1.171123
-57.800362	26.670319	1.176128
-58.288530	35.131187	1.181133
-58.526364	25.201340	1.186138
-59.190918	22.519428	1.191142
-59.265532	25.529557	1.196147
-59.470621	26.189989	1.201152
-59.311623	23.081237	1.206157
-59.134577	15.562216	1.211162
-60.265234	18.647821	1.216166
-60.544208	15.312629	1.221171
-60.878772	22.943874	1.226176
-60.840535	19.967843	1.231181
-60.613776	11.977919	1.236186
-60.771612	18.130426	1.241190
-61.239861	34.329613	1.246195
-61.757078	22.795451	1.251200
-62.220277	22.110571	1.256205
-62.401333	23.631541	1.261210
-62.653278	25.854018	1.266214
-62.871836	23.038614	1.271219
-63.528402	31.532243	1.276224
-63.722364	21.075339	1.281229
-63.779892	14.764930	1.286234
-63.557320	27.128302	1.291238
-63.640656	27.747995	1.296243
-63.934659	21.073464	1.301248
-64.720284	27.314435	1.306253
-65.378045	20.748658	1.311258
-65.512270	38.274795	1.316262
-65.322379	22.750793	1.321267
-65.669402	29.204982	1.326272
-66.002636	29.102981	1.331277
-65.859221	24.114378	1.336282
-65.735071	26.973371	1.341286
-66.118078	24.566247	1.346291
-67.069292	24.670358	1.351296
-67.298901	22.363865	1.356301
-67.404315	21.402618	1.361306
-67.639838	30.605539	1.366310
-67.342538	20.832315	1.371315
-67.883511	28.122197	1.376320
-68.667585	33.634055	1.381325
-68.868463	25.383615	1.386330
-69.264987	26.905469	1.391334
-69.192419	25.419957	1.396339
-69.023572	31.263457	1.401344
-69.121858	34.791489	1.406349
-69.404051	26.164506	1.411354
-70.236190	35.077431	1.416358
-70.462933	26.843005	1.421363
-70.500704	19.904155	1.426368
-70.722820	23.132516	1.431373
-70.915314	33.716198	1.436378
-71.474845	24.868881	1.441382
-71.874545	33.441405	1.446387
-72.370896	31.749415	1.451392
-72.547756	30.114425	1.456397
-72.173658	24.363279	1.461402
-72.135246	25.259504	1.466406
-72.376922	22.455517	1.471411
-72.668342	20.809274	1.476416
-73.480654	21.045219	1.481421
-73.548669	14.385433	1.486426
-73.658065	24.558982	1.491430
-73.730696	12.471500	1.496435
-74.848187	22.195556	1.501440
-75.267900	30.207970	1.506445
-74.509195	26.165193	1.511450
-75.054426	39.940737	1.516454
-75.128118	30.098301	1.521459
-75.371533	32.166159	1.526464
-75.498898	30.391878	1.531469
-76.233024	29.393363	1.536474
-77.039770	20.904080	1.541478
-77.001012	28.599216	1.546483
-76.750501	27.268977	1.551488
-77.314299	35.427242	1.556493
-77.414006	32.197873	1.561498
-77.505711	33.406535	1.566502
-77.459235	28.452006	1.571507
-77.910576	18.785048	1.576512
-78.645608	30.640864	1.581517
-78.521996	24.109816	1.586522
-79.086393	31.272853	1.591526
-78.779148	18.822478	1.596531
-78.930519	26.035046	1.601536
-79.919959	29.387855	1.606541
-80.399690	22.935212	1.611546
-80.651195	35.677539	1.616550
-80.626816	20.887656	1.621555
-80.566821	26.343082	1.626560
-80.912845	29.420657	1.631565
-80.583391	20.897498	1.636570
-80.937178	17.266277	1.641574
-81.098047	14.347620	1.646579
-81.640816	22.832994	1.651584
-81.904487	18.979902	1.656589
-81.739638	20.350575	1.661594
-83.048005	31.767623	1.666598
-83.612495	16.483534	1.671603
-83.434381	31.829868	1.676608
-83.753120	36.892107	1.681613
-83.241827	26.745227	1.686618
-83.638038	19.562552	1.691622
-83.502280	21.375564	1.696627
-84.026322	26.341111	1.701632
-85.021328	16.836124	1.706637
-84.846259	13.226119	1.711642
-85.206492	26.381715	1.716646
-85.085757	21.017635	1.721651
-85.184947	24.018210	1.726656
-85.995187	24.074954	1.731661
-86.318505	15.697860	1.736666
-86.784758	18.789484	1.741670
-86.771972	18.696494	1.746675
-86.667519	21.439566	1.751680
-86.866569	20.008316	1.756685
-86.823882	23.338724	1.761690
-87.715919	26.638835	1.766694
-87.977375	25.494526	1.771699
-87.997187	26.065935	1.776704
-88.247089	29.073070	1.781709
-88.448841	20.592519	1.786714
-89.516771	30.533915	1.791718
-89.823715	21.562877	1.796723
-89.754815	18.615420	1.801728
-90.077945	17.926631	1.806733
-89.418572	16.192901	1.811738
-90.211033	23.420066	1.816742
-90.549883	22.984161	1.821747
-90.338323	22.675809	1.826752
-90.615624	21.022991	1.831757
-90.700216	14.331417	1.836762
-91.327573	12.174518	1.841766
-91.763767	19.425079	1.846771
-91.919552	23.787362	1.851776
-92.064820	31.005434	1.856781
-92.038134	29.278402	1.861786
-93.275186	34.993180	1.866790
-93.475089	27.224212	1.871795
-93.459787	33.509705	1.876800
-93.440593	30.077485	1.881805
-93.272987	31.073703	1.886810
-93.633334	34.875305	1.891814
-93.473248	25.610334	1.896819
-93.976669	29.634666	1.901824
-94.481912	31.006974	1.906829
-94.570746	22.465241	1.911834
-95.291948	26.536713	1.916838
-95.969112	36.178535	1.921843
-96.447335	25.600210	1.926848
-96.264124	43.711784	1.931853
-95.639501	25.804656	1.936858
-96.224131	21.993068	1.941862
-96.412325	19.418495	1.946867
-96.552135	16.142978	1.951872
-97.577806	18.184147	1.956877
-97.827628	23.956352	1.961882
-97.642113	23.289650	1.966886
-98.103705	27.010019	1.971891
-98.081044	20.870151	1.976896
-98.473538	24.034527	1.981901
-98.149694	19.818858	1.986906
-98.590652	20.301234	1.991910
-99.534337	23.294483	1.996915
-99.679411	25.373613	2.006912
-98.810012	24.081123	2.016909
-98.632757	21.153273	2.026906
-98.495533	22.758123	2.036902
-97.316294	13.102969	2.046899
-97.284814	15.174993	2.056896
-96.846384	17.985119	2.066893
-95.860168	11.272589	2.076890
-95.533493	18.556736	2.086886
-95.435849	20.188031	2.096883
-94.254943	18.243917	2.106880
-94.367599	21.870618	2.116877
-93.873249	27.655176	2.126874
-92.881594	22.613410	2.136870
-92.697301	30.714403	2.146867
-92.336670	28.015940	2.156864
-91.289620	32.806250	2.166861
-91.204201	30.322927	2.176858
-90.786766	33.717654	2.186854
-89.750317	38.003071	2.196851
-89.772614	29.719310	2.206848
-89.506032	23.799395	2.216845
-88.476446	32.117188	2.226842
-88.299096	26.192954	2.236838
-87.088181	28.603273	2.246835
-86.959320	31.414484	2.256832
-86.726634	38.910997	2.266829
-86.421788	27.000614	2.276826
-85.564159	27.383022	2.286822
-85.151091	18.602310	2.296819
-84.554147	20.458541	2.306816
-83.621909	23.569389	2.316813
-83.385570	22.030460	2.326810
-83.499837	27.767928	2.336806
-82.876748	26.691632	2.346803
-82.192702	23.189825	2.356800
-81.618112	24.491788	2.366797
-80.622596	22.957633	2.376794
-80.756134	26.320831	2.386790
-80.395089	28.135051	2.396787
-79.636883	22.306455	2.406784
-79.201408	20.097974	2.416781
-78.300104	19.739619	2.426778
-77.747002	15.987363	2.436774
-77.585826	21.191182	2.446771
-77.366729	25.697077	2.456768
-76.576382	22.535931	2.466765
-76.002738	17.964055	2.476762
-75.699422	23.390002	2.486758
-74.754454	26.744713	2.496755
-74.552794	25.465727	2.506752
-74.390701	18.442216	2.516749
-73.511363	23.978084	2.526746
-73.007312	23.132952	2.536742
-72.875659	31.617175	2.546739
-71.811628	32.552627	2.556736
-71.220821	33.575474	2.566733
-71.107060	23.564766	2.576730
-71.087755	27.826256	2.586726
-70.195772	34.641324	2.596723
-69.507697	32.768586	2.606720
-68.511456	32.160184	2.616717
-68.331343	24.313615	2.626714
-68.445893	24.723636	2.636710
-67.644445	27.449176	2.646707
-66.845692	23.740828	2.656704
-66.718933	22.107152	2.666701
-66.269519	18.922142	2.676698
-65.213918	21.533025	2.686694
-65.328908	27.071718	2.696691
-64.566026	27.657126	2.706688
-63.935086	23.724127	2.716685
-63.674623	27.137043	2.726682
-62.711355	19.771808	2.736678
-62.158049	24.081362	2.746675
-62.042788	33.815206	2.756672
-61.930411	26.228708	2.766669
-60.904146	20.067126	2.776666
-60.672961	27.662221	2.786662
-60.274320	34.772142	2.796659
-59.139300	30.333003	2.806656
-58.902629	33.446398	2.816653
-58.882200	28.034345	2.826650
-58.096016	18.555673	2.836646
-57.528972	24.082109	2.846643
-57.140998	22.808338	2.856640
-56.337373	25.826750	2.866637
-55.713088	35.214506	2.876634
-55.948226	31.098661	2.886630
-55.086811	34.915799	2.896627
-54.549916	30.321347	2.906624
-54.008132	24.700447	2.916621
-52.867218	25.110721	2.926618
-52.735111	22.088835	2.936614
-52.932436	20.635553	2.946611
-52.431511	25.899196	2.956608
-51.188363	24.205485	2.966605
-50.904210	17.272041	2.976602
-50.676905	17.370069	2.986598
-49.757931	21.732099	2.996595
-49.601659	23.563764	3.006592
-49.319739	23.845439	3.016589
-48.357641	20.610225	3.026586
-48.014737	24.821150	3.036582
-47.682705	29.877905	3.046579
-46.552400	29.842407	3.056576
-46.387665	28.743576	3.066573
-46.224968	23.715384	3.076570
-45.556215	25.114548	3.086566
-44.925621	14.797803	3.096563
-44.735821	19.104311	3.106560
-43.631499	16.044539	3.116557
-43.300024	14.620922	3.126554
-43.116840	28.316897	3.136550
-42.762435	28.515075	3.146547
-41.967684	32.008859	3.156544
-41.580764	28.240058	3.166541
-40.707733	24.458687	3.176538
-40.055489	21.877738	3.186534
-40.023365	27.776328	3.196531
-40.030255	29.946810	3.206528
-39.053330	21.554665	3.216525
-38.601618	16.278237	3.226522
-37.770778	21.581545	3.236518
-37.183170	15.195675	3.246515
-37.020499	20.428045	3.256512
-36.669452	16.803272	3.266509
-35.838958	20.093733	3.276506
-35.351700	21.261122	3.286502
-35.213115	39.384722	3.296499
-34.254742	30.435156	3.306496
-33.853429	24.983568	3.316493
-33.370630	31.320847	3.326490
-33.250036	25.349686	3.336486
-32.854699	26.404791	3.346483
-32.007970	26.497506	3.356480
-30.986208	22.016340	3.366477
-31.088252	16.836859	3.376474
-30.713856	10.071545	3.386470
-29.807810	18.559167	3.396467
-29.360214	25.298916	3.406464
-29.272755	15.624954	3.416461
-28.237870	19.994996	3.426458
-27.964935	27.883341	3.436454
-27.745460	25.538086	3.446451
-26.737106	20.357398	3.456448
-26.478876	24.690483	3.466445
-26.046259	20.007078	3.476442
-24.934400	21.665216	3.486438
-24.570433	20.514791	3.496435
-24.659777	26.712265	3.506432
-24.124455	25.925978	3.516429
-23.075895	26.851746	3.526426
-22.838304	35.349487	3.536422
-22.900272	33.562032	3.546419
-22.255850	26.030837	3.556416
-21.221054	21.989069	3.566413
-20.748951	20.982725	3.576410
-19.928341	22.780022	3.586406
-19.858660	22.503891	3.596403
-19.648808	29.651681	3.606400
-19.386135	28.546296	3.616397
-18.274173	30.754926	3.626394
-17.949730	34.958436	3.636390
-17.196486	30.698857	3.646387
-16.544989	29.389886	3.656384
-16.468121	32.902640	3.666381
-16.366832	26.848728	3.676378
-15.237108	23.551046	3.686374
-15.007235	24.299518	3.696371
-14.562822	26.033979	3.706368
-13.593235	24.200565	3.716365
-13.306175	29.547269	3.726362
-13.313644	29.723808	3.736358
-12.227356	31.653822	3.746355
-11.924883	27.050105	3.756352
-11.533179	21.245039	3.766349
-10.694226	25.627907	3.776346
-10.234066	24.257208	3.786342
-10.146491	19.846908	3.796339
-9.235689	23.213499	3.806336
-8.330876	13.648846	3.816333
-8.014702	16.053637	3.826330
-8.146320	24.075762	3.836326
-8.205170	19.470218	3.846323
-7.384675	25.048076	3.856320
-6.136307	22.338734	3.866317
-5.400290	22.567397	3.876314
-5.377414	21.749926	3.886310
-5.167739	22.813193	3.896307
-4.069635	27.659884	3.906304
-3.927568	21.726761	3.916301
-3.733556	20.682065	3.926298
-3.082782	35.862803	3.936294
-2.691279	39.963269	3.946291
-2.151006	63.049906	3.956288
-1.986138	65.007437	3.966285
-1.465732	85.337200	3.976282
-0.871539	99.795877	3.986278
-0.335844	125.361343	3.996275
0.000000	137.637175	4.001280
-0.009984	139.235051	4.006285
0.442955	158.940182	4.011290
0.085420	177.293029	4.016294
0.472024	172.596657	4.021299
0.469752	177.484903	4.026304
0.500133	177.510548	4.031309
0.679873	184.804818	4.036314
0.694340	202.568807	4.041318
0.987285	199.895252	4.046323
0.840624	197.315062	4.051328
0.768844	204.276213	4.056333
0.728549	194.442448	4.061338
0.888190	203.510029	4.066342
1.166565	193.596670	4.071347
1.266236	197.935237	4.076352
0.940951	206.933493	4.081357
1.194088	200.208019	4.086362
1.046390	196.967402	4.091366
1.319970	201.648570	4.096371
1.184269	213.051013	4.101376
1.018450	220.697387	4.106381
1.195905	209.148902	4.111386
1.043993	212.611451	4.116390
0.932140	210.823829	4.121395
1.305475	207.753217	4.126400
1.198594	205.761148	4.131405
1.107418	208.014105	4.136410
0.971151	222.824513	4.141414
1.291654	203.888725	4.146419
1.049778	207.914864	4.151424
1.115899	210.191155	4.156429
1.403548	207.575891	4.161434
1.298240	221.045285	4.166438
1.342847	202.065809	4.171443
1.114435	207.997921	4.176448
0.864569	218.076332	4.181453
1.110485	199.348313	4.186458
1.115819	208.646502	4.191462
1.306691	203.534274	4.196467
1.432668	208.164957	4.201472
1.317049	202.523381	4.206477
1.464186	208.233116	4.211482
1.211266	210.828994	4.216486
1.377222	211.924058	4.221491
1.512106	209.431215	4.226496
1.118035	207.299654	4.231501
1.309073	205.123391	4.236506
1.230710	209.631671	4.241510
1.345418	199.790144	4.246515
1.264667	202.179693	4.251520
1.034496	208.546871	4.256525
1.588487	202.291199	4.261530
1.177434	218.239821	4.266534
1.510041	227.489364	4.271539
1.776485	232.468576	4.276544
1.668116	226.675541	4.281549
1.750328	225.920442	4.286554
1.392783	222.935093	4.291558
1.138534	211.294278	4.296563
1.727738	220.512856	4.301568
1.400687	226.132061	4.306573
1.448259	228.789272	4.311578
1.393584	249.665298	4.316582
1.536461	243.346829	4.321587
1.665642	243.761031	4.326592
1.358428	241.629021	4.331597
1.504474	236.882804	4.336602
1.603960	252.653271	4.341606
1.595599	240.001518	4.346611
1.641145	230.113687	4.351616
1.743773	238.257328	4.356621
1.597396	240.661477	4.361626
1.527256	233.985169	4.366630
1.957995	231.569710	4.371635
1.560567	228.787177	4.376640
1.425030	243.765002	4.381645
1.820312	235.802949	4.386650
1.713365	243.151529	4.391654
1.649277	239.412883	4.396659
1.585997	242.735796	4.401664
1.400133	244.425592	4.406669
1.991897	241.165466	4.411674
1.915925	259.257896	4.416678
1.986459	253.253463	4.421683
1.836030	247.776164	4.426688
1.493656	244.108366	4.431693
1.922620	260.952425	4.436698
1.994919	268.845082	4.441702
2.010739	280.417479	4.446707
2.152400	266.063758	4.451712
1.682383	256.954958	4.456717
2.293359	263.462253	4.461722
2.158395	253.035585	4.466726
2.124534	246.835309	4.471731
2.101267	253.262826	4.476736
1.867943	254.526280	4.481741
1.963527	250.080322	4.486746
1.902542	250.882789	4.491750
1.801556	239.320608	4.496755
2.007331	266.119634	4.501760
2.235827	274.108223	4.506765
2.278666	267.685422	4.511770
1.841017	268.803090	4.516774
2.255706	278.918224	4.521779
2.420042	269.084434	4.526784
2.200858	255.616106	4.531789
2.013291	250.006134	4.536794
1.939445	243.209186	4.541798
1.612502	252.487729	4.546803
1.923259	271.901000	4.551808
1.739566	278.904849	4.556813
2.172036	269.087718	4.561818
2.077288	277.071914	4.566822
2.014523	285.031096	4.571827
2.221526	277.786783	4.576832
1.743414	289.546177	4.581837
2.296370	279.444433	4.586842
2.173677	284.520625	4.591846
1.991545	284.697606	4.596851
2.396602	291.880207	4.601856
2.589203	302.315004	4.606861
2.503902	285.788180	4.611866
2.340643	299.431678	4.616870
2.088524	281.692711	4.621875
2.224305	295.686641	4.626880
2.445373	311.743207	4.631885
2.545867	300.496435	4.636890
2.666095	303.323475	4.641894
2.312907	306.159593	4.646899
2.269750	279.629362	4.651904
2.260106	311.621319	4.656909
2.697901	307.759170	4.661914
2.509839	296.526444	4.666918
2.268258	299.466648	4.671923
2.619780	295.354261	4.676928
2.116891	302.909775	4.681933
2.324740	299.801577	4.686938
2.382383	313.967273	4.691942
2.486503	300.730200	4.696947
2.458777	309.133379	4.701952
2.414111	309.108977	4.706957
2.725270	303.378585	4.711962
2.593093	310.395936	4.716966
2.506251	310.861328	4.721971
2.861070	303.031023	4.726976
2.401673	310.012671	4.731981
2.973704	296.186151	4.736986
2.560546	309.266292	4.741990
2.818198	307.175887	4.746995
2.611068	310.174329	4.752000
2.453154	309.664607	4.757005
2.937022	307.056560	4.762010
2.957402	317.773375	4.767014
2.739004	310.122638	4.772019
2.909257	311.720147	4.777024
2.795460	308.095063	4.782029
3.081682	309.241391	4.787034
2.549872	312.816367	4.792038
2.821539	300.962293	4.797043
3.051334	301.886004	4.802048
2.712273	312.951278	4.807053
2.873406	301.917645	4.812058
3.036635	300.454909	4.817062
3.028569	302.332175	4.822067
2.866848	300.260761	4.827072
2.784797	313.541017	4.832077
3.175979	300.644027	4.837082
2.930633	306.737614	4.842086
2.930391	310.463198	4.847091
2.842436	307.197097	4.852096
2.632051	317.040561	4.857101
2.943837	294.747839	4.862106
2.957494	308.004578	4.867110
2.822246	300.237108	4.872115
3.164627	302.010093	4.877120
2.852498	308.277105	4.882125
2.988092	305.030494	4.887130
3.100878	301.288649	4.892134
2.835709	303.640320	4.897139
2.807567	300.883565	4.902144
2.681987	313.518994	4.907149
3.120273	314.969508	4.912154
3.026775	311.499709	4.917158
2.532630	307.715800	4.922163
3.125920	308.841374	4.927168
2.771401	317.835351	4.932173
3.382160	327.226830	4.937178
3.258393	331.697760	4.942182
3.100773	324.686231	4.947187
3.209793	320.277592	4.952192
3.195980	333.411824	4.957197
3.311728	321.359550	4.962202
3.213531	317.678415	4.967206
3.161295	313.190569	4.972211
3.411693	311.894264	4.977216
3.046416	325.079565	4.982221
3.274908	324.789722	4.987226
3.087406	349.353217	4.992230
3.168234	338.586869	4.997235
3.250567	342.428745	5.002240
3.150554	335.126816	5.007245
3.303888	329.856190	5.012250
3.586574	342.734451	5.017254
3.355582	329.946864	5.022259
3.422666	330.127057	5.027264
3.413254	338.822800	5.032269
3.643282	329.197528	5.037274
3.331461	342.325570	5.042278
3.435576	338.338014	5.047283
3.459891	337.996377	5.052288
2.974507	340.693044	5.057293
3.009756	353.737300	5.062298
3.358238	338.620655	5.067302
2.990548	348.768938	5.072307
3.561377	331.350992	5.077312
3.147941	349.629227	5.082317
3.186948	344.551717	5.087322
3.331008	371.495595	5.092326
3.468804	370.010517	5.097331
3.681973	367.766843	5.102336
3.612346	371.463557	5.107341
3.851560	367.996477	5.112346
3.989360	359.814779	5.117350
3.570915	350.946509	5.122355
3.653629	346.246142	5.127360
3.352304	345.700628	5.132365
3.331502	350.943208	5.137370
3.350530	370.401460	5.142374
3.223701	375.050687	5.147379
3.548255	366.554782	5.152384
3.208356	377.613532	5.157389
3.300877	373.985415	5.162394
3.371319	377.362914	5.167398
3.752027	370.458532	5.172403
4.068777	387.490372	5.177408
3.657500	393.892488	5.182413
3.950889	375.577181	5.187418
3.803568	374.629741	5.192422
3.426291	385.918527	5.197427
3.944546	386.340850	5.202432
3.539605	389.515740	5.207437
3.670878	392.816005	5.212442
4.043595	401.208306	5.217446
4.229963	413.760302	5.222451
3.997586	394.147011	5.227456
3.994280	392.637005	5.232461
3.703766	374.434866	5.237466
4.011727	372.280299	5.242470
3.532469	388.317814	5.247475
4.032140	397.460532	5.252480
3.902669	404.200351	5.257485
4.354978	404.165939	5.262490
3.848236	394.926782	5.267494
3.625437	380.238556	5.272499
4.108800	395.609213	5.277504
3.946174	404.784826	5.282509
4.107895	404.971775	5.287514
4.177011	399.523748	5.292518
3.845685	415.435819	5.297523
4.302369	402.399074	5.302528
4.238534	403.056501	5.307533
4.264943	397.630034	5.312538
3.988855	383.382136	5.317542
3.694961	374.443744	5.322547
4.052657	392.848637	5.327552
3.953597	409.276771	5.332557
4.069887	392.578891	5.337562
3.991075	403.182818	5.342566
4.168883	400.982472	5.347571
4.067191	401.958996	5.352576
4.276123	403.904202	5.357581
4.411805	403.712370	5.362586
4.407650	402.849989	5.367590
3.899287	411.362545	5.372595
4.164341	410.805316	5.377600
4.200106	409.366002	5.382605
4.166847	408.307763	5.387610
4.379277	419.611984	5.392614
4.029291	417.591693	5.397619
4.167844	405.400523	5.402624
4.267117	416.399255	5.407629
4.085061	402.436606	5.412634
4.067375	405.823545	5.417638
3.975877	410.793203	5.422643
4.124871	409.551039	5.427648
4.274038	433.539011	5.432653
4.340780	422.129221	5.437658
4.208494	433.132984	5.442662
4.313124	436.015211	5.447667
4.255124	420.183210	5.452672
4.298048	434.345629	5.457677
4.320920	431.408756	5.462682
4.385092	433.133810	5.467686
4.184242	435.219647	5.472691
4.084343	434.754594	5.477696
4.252937	431.856484	5.482701
4.374141	440.853704	5.487706
4.851037	458.377996	5.492710
5.012625	450.481484	5.497715
5.062092	432.424649	5.502720
4.498013	435.491080	5.507725
4.772709	430.842327	5.512730
4.719159	435.035308	5.517734
4.597603	427.232461	5.522739
4.666965	428.422922	5.527744
4.677800	440.219624	5.532749
4.681983	437.558921	5.537754
4.785521	429.987321	5.542758
4.482305	434.534304	5.547763
4.563505	429.898191	5.552768
4.653943	441.216964	5.557773
4.934805	433.919133	5.562778
4.441315	432.958652	5.567782
4.248855	439.219457	5.572787
4.594034	439.945934	5.577792
4.316011	445.836809	5.582797
4.696838	454.370853	5.587802
4.866886	473.488278	5.592806
5.025835	469.272608	5.597811
5.163587	460.208276	5.602816
4.764223	453.973903	5.607821
4.612139	440.801838	5.612826
4.662967	444.582747	5.617830
4.634584	450.794935	5.622835
4.947901	463.470427	5.627840
4.582866	464.811011	5.632845
4.628817	468.014502	5.637850
4.577611	476.622124	5.642854
4.542145	477.952050	5.647859
4.709632	466.534359	5.652864
4.647141	478.538253	5.657869
4.806337	467.574572	5.662874
4.614239	467.551645	5.667878
4.370651	485.954003	5.672883
4.859471	501.026117	5.677888
4.554027	507.674896	5.682893
4.808505	495.420694	5.687898
4.875135	505.212975	5.692902
4.977762	500.296071	5.697907
5.240573	493.580117	5.702912
4.960372	502.131477	5.707917
4.951847	498.650751	5.712922
5.113609	508.016798	5.717926
4.850410	506.421574	5.722931
5.212507	501.911966	5.727936
5.013441	510.214525	5.732941
5.413864	515.826776	5.737946
5.117257	503.667781	5.742950
4.834941	508.730961	5.747955
5.134125	516.055275	5.752960
5.012636	529.818258	5.757965
5.388087	527.699183	5.762970
5.385067	530.535484	5.767974
5.476959	537.104507	5.772979
5.784596	530.983731	5.777984
5.175027	505.141521	5.782989
5.293148	512.438731	5.787994
5.523098	506.121452	5.792998
4.993914	507.617126	5.798003
5.185498	484.864418	5.803008
5.260883	499.235915	5.808013
4.983171	515.169320	5.813018
5.521472	526.970377	5.818022
5.289547	530.568654	5.823027
5.552867	539.335561	5.828032
5.753054	541.150916	5.833037
5.602954	518.598269	5.838042
5.178090	515.944427	5.843046
5.019878	514.607699	5.848051
5.156567	521.494487	5.853056
5.250147	540.800836	5.858061
5.294681	533.723247	5.863066
5.284589	545.362872	5.868070
5.544654	552.687157	5.873075
5.694896	540.314589	5.878080
5.458954	543.624762	5.883085
5.544920	552.162402	5.888090
5.565068	538.696007	5.893094
5.295314	540.338826	5.898099
5.463234	534.640505	5.903104
5.129579	534.321221	5.908109
5.402797	534.781873	5.913114
5.559370	530.660796	5.918118
5.353147	535.467035	5.923123
5.677903	536.231817	5.928128
5.740102	533.617745	5.933133
5.372903	530.904450	5.938138
5.550535	535.984270	5.943142
5.512547	555.792054	5.948147
5.826135	558.501356	5.953152
5.721581	576.558926	5.958157
5.861115	566.072180	5.963162
5.749125	553.971034	5.968166
5.835487	557.765436	5.973171
5.795871	553.273757	5.978176
5.556622	549.166587	5.983181
5.868214	554.581122	5.988186
5.653964	570.911258	5.993190
5.478391	563.056791	5.998195
5.644863	563.057185	6.003200
5.893403	567.768847	6.008205
6.009177	566.195045	6.013210
6.041368	554.238876	6.018214
5.841688	577.492202	6.023219
6.373512	563.101944	6.028224
6.030613	550.655476	6.033229
5.551598	547.515116	6.038234
5.798986	538.995463	6.043238
5.624744	536.770996	6.048243
5.932815	547.838612	6.053248
5.679958	542.999579	6.058253
5.674624	542.330953	6.063258
6.178123	541.222479	6.068262
5.615075	561.520550	6.073267
5.981504	540.570352	6.078272
5.912912	546.522749	6.083277
5.842152	543.331499	6.088282
6.108985	540.721395	6.093286
6.226989	540.231478	6.098291
5.905092	526.236281	6.103296
5.823960	539.078144	6.108301
5.766216	546.120496	6.113306
6.052012	531.986096	6.118310
5.996814	537.719525	6.123315
6.204592	528.671008	6.128320
5.860505	552.440166	6.133325
5.672251	530.976774	6.138330
5.973406	526.711246	6.143334
5.826292	535.006615	6.148339
5.783551	533.656722	6.153344
5.835051	546.297511	6.158349
5.787533	530.834124	6.163354
6.078882	533.461757	6.168358
5.734780	533.991374	6.173363
5.891676	525.876776	6.178368
5.581645	528.956886	6.183373
5.562022	535.597512	6.188378
5.854825	537.295451	6.193382
5.353849	530.466061	6.198387
5.481978	529.290575	6.203392
5.423727	534.551147	6.208397
5.458758	537.093279	6.213402
5.694262	545.624258	6.218406
5.883426	560.316393	6.223411
5.680356	548.554690	6.228416
5.577384	557.524403	6.233421
5.858073	561.962894	6.238426
6.141514	570.517042	6.243430
5.920251	562.738002	6.248435
5.876621	535.648511	6.253440
5.787321	547.164882	6.258445
5.638345	547.129106	6.263450
5.736530	537.789205	6.268454
5.767428	540.538214	6.273459
5.987246	545.750667	6.278464
5.733344	539.944666	6.283469
5.919479	547.118972	6.288474
5.823962	543.835523	6.293478
5.710941	546.043698	6.298483
5.985487	535.571658	6.303488
5.722158	542.137921	6.308493
5.770207	546.305461	6.313498
5.951798	543.474638	6.318502
5.518810	548.985381	6.323507
5.943067	550.354772	6.328512
5.833994	545.942549	6.333517
5.954368	544.091550	6.338522
5.972683	552.203415	6.343526
5.844790	547.627075	6.348531
6.047504	551.667934	6.353536
6.088466	551.914403	6.358541
5.763024	556.356966	6.363546
5.868708	558.279495	6.368550
5.976196	558.745337	6.373555
6.470422	547.150762	6.378560
6.185927	553.600461	6.383565
5.889976	546.818575	6.388570
6.137266	545.459624	6.393574
6.095166	551.103877	6.398579
5.902477	523.294666	6.403584
5.637677	513.606518	6.408589
5.717921	515.518842	6.413594
5.755211	530.251634	6.418598
5.826777	538.618502	6.423603
5.765849	542.837101	6.428608
5.841231	540.324539	6.433613
5.931546	547.689009	6.438618
5.946374	525.075553	6.443622
6.074468	525.229783	6.448627
6.020903	514.149098	6.453632
6.000176	504.937391	6.458637
5.908416	505.840062	6.463642
5.952007	505.608988	6.468646
5.588720	508.440596	6.473651
5.383223	509.279290	6.478656
5.733321	503.192945	6.483661
5.960394	508.565097	6.488666
5.759400	518.831957	6.493670
5.591683	507.677896	6.498675
5.712038	507.447653	6.503680
5.795360	525.407718	6.508685
5.725855	522.864447	6.513690
5.690465	529.177764	6.518694
5.872816	543.357791	6.523699
5.855679	550.693847	6.528704
6.176414	550.223604	6.533709
5.778234	542.189282	6.538714
5.797899	517.664825	6.543718
5.613052	524.178253	6.548723
5.683676	515.172535	6.553728
6.156350	537.825843	6.558733
5.639527	530.466912	6.563738
6.080932	528.480188	6.568742
5.628542	518.775978	6.573747
5.469601	518.542462	6.578752
5.740221	523.895978	6.583757
5.653672	533.794490	6.588762
5.804487	542.541021	6.593766
5.635990	548.499667	6.598771
6.116507	543.336700	6.603776
6.013981	558.639682	6.608781
5.770256	551.754748	6.613786
5.940494	552.104064	6.618790
5.770436	548.002134	6.623795
5.887172	551.025437	6.628800
5.680793	537.584342	6.633805
5.620321	537.287592	6.638810
5.892880	539.066915	6.643814
5.807998	534.966698	6.648819
5.731602	541.908539	6.653824
5.731552	548.848027	6.658829
6.028222	543.732409	6.663834
6.130134	550.732988	6.668838
5.875727	536.133202	6.673843
5.705402	520.007309	6.678848
5.536539	527.158879	6.683853
5.685729	540.916702	6.688858
6.092009	552.316847	6.693862
5.805997	542.583647	6.698867
6.068691	540.510433	6.703872
5.740803	528.263159	6.708877
5.679169	519.848747	6.713882
5.932129	520.095304	6.718886
5.495555	524.986371	6.723891
5.830783	532.828215	6.728896
5.839618	540.963542	6.733901
5.716691	541.291061	6.738906
6.108125	536.944608	6.743910
5.927084	543.109844	6.748915
5.690877	524.196009	6.753920
5.782863	536.995845	6.758925
5.552013	534.185234	6.763930
5.934592	536.881750	6.768934
6.115258	542.781904	6.773939
5.928028	534.742717	6.778944
5.639508	520.526048	6.783949
5.840563	527.718203	6.788954
5.818035	523.784084	6.793958
5.662759	540.939975	6.798963
5.575008	540.549964	6.803968
5.829456	542.684982	6.808973
5.932547	555.546829	6.813978
5.928594	551.829641	6.818982
5.924458	548.071344	6.823987
5.784054	546.837234	6.828992
5.860182	550.204460	6.833997
5.939189	546.979580	6.839002
5.642292	524.423559	6.844006
5.992509	526.443499	6.849011
5.986756	521.948009	6.854016
5.699858	519.612623	6.859021
5.584353	514.431547	6.864026
5.926630	526.887922	6.869030
5.698815	537.003742	6.874035
5.822615	536.652468	6.879040
5.814650	534.234975	6.884045
5.835334	546.723300	6.889050
6.199247	529.585477	6.894054
5.337793	528.168633	6.899059
5.753887	531.706882	6.904064
5.740423	539.213891	6.909069
5.600314	534.346759	6.914074
5.839234	542.482442	6.919078
5.314860	537.644477	6.924083
5.571805	546.190559	6.929088
5.820414	544.744670	6.934093
5.582844	547.016245	6.939098
6.029925	544.075842	6.944102
5.854760	554.721250	6.949107
5.828396	549.589559	6.954112
5.735852	542.758177	6.959117
5.456020	546.287521	6.964122
5.940334	544.292619	6.969126
5.831795	544.488617	6.974131
5.907214	551.161788	6.979136
6.085283	544.745431	6.984141
5.825417	547.657724	6.989146
5.725019	547.945806	6.994150
5.586438	555.103829	6.999155
5.884189	550.579879	7.004160
5.756958	546.912761	7.009165
5.614875	557.782676	7.014170
5.841491	549.189201	7.019174
6.038607	550.877204	7.024179
5.895154	552.032205	7.029184
5.778818	542.692431	7.034189
5.458011	546.484267	7.039194
5.880312	543.806838	7.044198
5.701255	553.019290	7.049203
5.770924	538.768372	7.054208
5.847937	550.993546	7.059213
6.105547	544.194965	7.064218
5.551044	547.402988	7.069222
5.816012	544.431710	7.074227
6.047054	543.473035	7.079232
5.727027	541.621611	7.084237
5.718240	549.052380	7.089242
6.058481	543.244186	7.094246
5.678865	553.608661	7.099251
5.921530	541.411919	7.104256
6.083447	563.609814	7.109261
5.766325	551.303027	7.114266
5.937860	547.457492	7.119270
5.729792	554.739861	7.124275
6.133832	560.611199	7.129280
6.109358	550.065833	7.134285
5.975211	562.293650	7.139290
6.082051	550.356915	7.144294
5.792086	548.526371	7.149299
6.085108	538.739217	7.154304
5.930772	531.528452	7.159309
5.801842	528.204553	7.164314
5.690086	514.793027	7.169318
5.483313	522.026332	7.174323
5.699072	533.706170	7.179328
6.314019	545.374016	7.184333
6.016058	536.537917	7.189338
5.468353	519.887572	7.194342
5.388379	528.745142	7.199347
5.780774	546.523435	7.204352
5.620323	539.335480	7.209357
5.766289	550.012662	7.214362
6.014681	552.082088	7.219366
5.657746	555.485264	7.224371
5.861532	556.308811	7.229376
5.787513	561.879021	7.234381
5.849418	553.337230	7.239386
6.144978	546.397907	7.244390
5.821341	559.257960	7.249395
5.969906	560.579482	7.254400
6.022279	555.327733	7.259405
6.030385	544.491570	7.264410
5.838053	522.514166	7.269414
5.944214	515.749308	7.274419
5.817473	520.580983	7.279424
5.801796	509.134137	7.284429
5.794057	507.010907	7.289434
5.933834	506.988778	7.294438
5.716697	521.958358	7.299443
5.689042	512.726481	7.304448
5.758834	515.178907	7.309453
5.582333	524.024505	7.314458
5.582689	533.217360	7.319462
5.618267	550.544168	7.324467
5.786119	550.684626	7.329472
5.896536	554.040068	7.334477
5.818011	560.065836	7.339482
6.009093	561.973858	7.344486
5.873072	556.010150	7.349491
6.230467	551.616439	7.354496
6.114851	540.547864	7.359501
5.666641	526.741555	7.364506
5.978883	520.017618	7.369510
5.748641	515.965994	7.374515
5.697005	512.160405	7.379520
5.770142	517.829209	7.384525
5.653443	523.378539	7.389530
5.714209	506.365226	7.394534
5.648271	519.130075	7.399539
5.464808	549.678588	7.404544
5.989443	539.806592	7.409549
5.990912	547.949553	7.414554
6.078368	541.802511	7.419558
5.675198	538.143210	7.424563
5.569863	524.562599	7.429568
6.201630	535.600194	7.434573
5.842922	532.447948	7.439578
5.683821	527.994964	7.444582
5.569041	529.681528	7.449587
5.661212	543.474329	7.454592
5.739702	560.790012	7.459597
5.881201	538.402151	7.464602
6.054671	548.832089	7.469606
5.848205	557.830251	7.474611
6.072442	549.017655	7.479616
5.831052	529.353885	7.484621
5.393548	531.192241	7.489626
5.542768	533.432452	7.494630
5.681922	553.155021	7.499635
5.732756	555.333357	7.504640
5.702129	552.516983	7.509645
5.788007	564.374089	7.514650
5.762184	559.059294	7.519654
6.019740	552.661468	7.524659
5.783857	554.925366	7.529664
6.026615	554.378427	7.534669
5.891124	551.436230	7.539674
6.030815	551.545726	7.544678
6.106807	540.779937	7.549683
6.226248	543.528028	7.554688
5.838007	523.303196	7.559693
5.586389	527.421497	7.564698
5.879330	526.998270	7.569702
5.362038	518.759395	7.574707
5.775564	527.145417	7.579712
5.819772	545.098552	7.584717
6.038730	555.437808	7.589722
6.097989	542.938601	7.594726
5.852951	527.208432	7.599731
5.966743	528.637315	7.604736
5.645563	522.480167	7.609741
5.453146	530.585507	7.614746
5.818255	520.557467	7.619750
5.759864	526.668193	7.624755
5.808992	540.034996	7.629760
6.121027	539.997917	7.634765
5.607274	533.724404	7.639770
5.797240	532.224770	7.644774
5.569504	533.936611	7.649779
5.628013	557.944889	7.654784
5.714900	560.306889	7.659789
5.972588	555.620558	7.664794
6.224208	555.986319	7.669798
5.993953	549.404506	7.674803
5.869736	533.203695	7.679808
6.120755	527.469545	7.684813
5.897538	530.617688	7.689818
5.995700	515.259681	7.694822
5.780629	518.812254	7.699827
5.737811	518.853943	7.704832
5.680228	511.631342	7.709837
5.420901	515.958686	7.714842
5.630037	523.651277	7.719846
5.753945	524.412055	7.724851
5.516540	536.631165	7.729856
5.899936	547.650027	7.734861
6.005304	548.458759	7.739866
6.059941	537.545752	7.744870
5.530865	547.159965	7.749875
5.790225	538.028530	7.754880
6.047879	538.492050	7.759885
5.492091	533.769775	7.764890
5.762358	532.330864	7.769894
5.765981	547.087981	7.774899
6.012486	542.137421	7.779904
6.232484	547.396313	7.784909
5.569973	534.847979	7.789914
5.787188	518.830301	7.794918
5.624839	520.892423	7.799923
5.685207	539.215609	7.804928
6.175124	543.390534	7.809933
6.046834	534.317045	7.814938
6.140912	519.091418	7.819942
5.735261	525.883145	7.824947
5.604410	517.504246	7.829952
5.559163	516.126060	7.834957
5.780318	515.170500	7.839962
6.077423	516.086850	7.844966
5.699265	519.461068	7.849971
5.752649	516.500688	7.854976
5.974437	518.090491	7.859981
5.587597	511.995894	7.864986
5.860310	511.629483	7.869990
6.058372	522.083062	7.874995
5.725601	511.498990	7.880000
5.600040	514.542003	7.885005
5.716180	528.028542	7.890010
5.867588	527.272352	7.895014
5.711204	533.361784	7.900019
5.731148	543.784631	7.905024
6.037311	551.371818	7.910029
5.682193	550.108865	7.915034
6.184861	543.886597	7.920038
5.829375	535.853609	7.925043
5.801111	528.182886	7.930048
5.387610	514.683991	7.935053
5.595238	541.233489	7.940058
5.981747	554.227563	7.945062
6.089403	554.438051	7.950067
5.466828	548.618386	7.955072
5.875979	542.921041	7.960077
5.701016	553.261858	7.965082
5.794538	562.459066	7.970086
6.052673	548.173640	7.975091
5.911884	551.983479	7.980096
5.614066	532.415651	7.985101
5.513773	550.709561	7.990106
6.330881	549.876410	7.995110
6.006351	549.748790	8.000115
5.812169	546.099052	8.005133
5.636251	522.618197	8.010150
5.351937	527.654648	8.015168
5.627339	537.416469	8.020186
5.774764	549.740098	8.025203
5.686133	538.625777	8.030221
5.827998	540.620824	8.035238
5.579347	551.058119	8.040256
6.028329	553.369470	8.045274
5.929238	555.562379	8.050291
5.824419	558.168458	8.055309
6.162254	554.705198	8.060326
5.690194	552.101819	8.065344
6.082577	560.389683	8.070362
6.224005	560.186999	8.075379
5.878741	560.626840	8.080397
6.166552	559.217417	8.085414
5.819088	562.671413	8.090432
6.022131	552.706092	8.095450
6.012722	554.418620	8.100467
6.110165	554.111809	8.105485
6.006910	521.292498	8.110502
5.575814	525.596364	8.115520
5.830578	526.897195	8.120538
5.882042	542.856150	8.125555
5.859918	548.260813	8.130573
6.008689	544.877313	8.135590
5.791953	554.952516	8.140608
5.865945	539.003782	8.145626
6.182337	556.269890	8.150643
6.051633	550.737721	8.155661
6.301517	535.595786	8.160678
5.963612	553.172339	8.165696
6.072467	545.428265	8.170714
5.805066	532.781982	8.175731
5.819570	546.258161	8.180749
5.904099	543.586619	8.185766
6.084334	546.246062	8.190784
5.777858	553.393356	8.195802
5.991195	552.940940	8.200819
5.749623	552.651775	8.205837
5.719431	559.472858	8.210854
5.930952	559.546429	8.215872
5.822234	546.764778	8.220890
6.050751	550.010813	8.225907
5.899653	559.803473	8.230925
5.764570	543.742069	8.235942
5.732736	562.903367	8.240960
6.056849	548.765001	8.245978
5.875807	553.071342	8.250995
5.731710	551.938472	8.256013
6.180791	564.271207	8.261030
6.115636	578.297287	8.266048
6.217453	588.526031	8.271066
6.256825	572.905658	8.276083
5.846386	568.475806	8.281101
5.921316	576.533320	8.286118
5.819993	587.510358	8.291136
5.837581	596.949538	8.296154
6.121440	580.231574	8.301171
6.292511	585.970495	8.306189
6.387536	587.739081	8.311206
6.230793	590.826196	8.316224
6.342443	582.661643	8.321242
6.417363	568.167566	8.326259
6.437498	564.212520	8.331277
5.981596	556.832781	8.336294
6.097194	559.213102	8.341312
5.836269	551.694176	8.346330
6.413040	563.174572	8.351347
6.412785	567.228348	8.356365
6.008726	562.348219	8.361382
6.052826	564.038522	8.366400
6.495490	569.249970	8.371418
6.506011	564.605011	8.376435
5.977699	561.410943	8.381453
6.083200	544.445577	8.386470
6.130598	560.525770	8.391488
6.116446	561.161927	8.396506
6.393219	564.715383	8.401523
6.201036	566.831274	8.406541
6.182303	575.042624	8.411558
6.316521	575.276186	8.416576
6.312927	572.309714	8.421594
6.414396	556.049393	8.426611
6.317023	559.451727	8.431629
6.242209	558.551356	8.436646
6.288337	554.944311	8.441664
5.934371	563.482164	8.446682
6.362315	567.475018	8.451699
6.204311	571.521209	8.456717
6.432989	578.338391	8.461734
6.124141	567.463748	8.466752
6.196819	576.073989	8.471770
6.691940	574.593009	8.476787
6.155913	571.644951	8.481805
6.306704	556.620336	8.486822
6.562921	592.275482	8.491840
6.121865	565.260907	8.496858
6.435907	557.800181	8.501875
6.224113	575.961512	8.506893
6.521229	580.160699	8.511910
6.285698	558.322400	8.516928
6.275367	566.516809	8.521946
6.467490	573.415507	8.526963
6.352863	577.851306	8.531981
6.252076	571.486882	8.536998
6.202582	578.629803	8.542016
6.122197	589.030362	8.547034
6.723962	590.930718	8.552051
6.247499	586.732695	8.557069
6.446785	578.010458	8.562087
6.497920	580.482916	8.567104
6.607403	583.866028	8.572122
6.348220	574.024511	8.577139
6.614772	584.166197	8.582157
6.292943	580.881124	8.587175
6.357018	581.547457	8.592192
6.298850	583.079204	8.597210
6.437756	577.480329	8.602227
6.030910	572.692864	8.607245
6.163259	570.988326	8.612263
6.025133	570.661400	8.617280
5.961333	582.951569	8.622298
6.359229	572.082056	8.627315
6.092080	582.256535	8.632333
6.681932	596.485746	8.637351
6.472594	584.861911	8.642368
6.360819	589.742826	8.647386
6.592083	605.357528	8.652403
6.361686	619.919419	8.657421
6.711373	616.936478	8.662439
6.496579	611.671383	8.667456
6.419287	612.936659	8.672474
6.832347	607.699674	8.677491
6.516670	606.534634	8.682509
6.150721	596.040597	8.687527
6.596329	602.195584	8.692544
6.572654	613.763042	8.697562
6.847587	604.849976	8.702579
6.537772	600.207166	8.707597
6.845452	602.067851	8.712615
6.663587	586.642656	8.717632
6.251636	582.278491	8.722650
6.388705	586.137367	8.727667
6.305016	601.227450	8.732685
6.727909	610.650438	8.737703
6.743742	603.041075	8.742720
6.485720	606.061776	8.747738
6.937856	617.901918	8.752755
6.517501	617.051069	8.757773
6.815656	606.645961	8.762791
6.733229	612.194249	8.767808
6.474619	595.127611	8.772826
6.448463	610.771573	8.777843
6.642022	612.634488	8.782861
6.775826	617.308128	8.787879
6.810646	604.770473	8.792896
6.527694	614.731386	8.797914
6.829417	618.627517	8.802931
6.641079	619.047331	8.807949
6.851600	618.095375	8.812967
6.828028	616.158085	8.817984
6.455574	612.338658	8.823002
6.611121	607.272945	8.828019
6.399556	613.008782	8.833037
6.791567	615.188738	8.838055
6.868706	613.861065	8.843072
6.822268	609.062052	8.848090
6.555927	611.018484	8.853107
6.530929	615.372959	8.858125
6.796535	615.189214	8.863143
6.632704	619.479937	8.868160
6.590926	623.831775	8.873178
6.780963	622.448246	8.878195
6.687793	611.218897	8.883213
6.561500	616.801103	8.888231
6.904668	617.020801	8.893248
6.784634	620.429058	8.898266
6.628557	627.593944	8.903283
6.667218	620.042698	8.908301
6.399312	619.603090	8.913319
6.789372	609.800294	8.918336
6.774341	623.209486	8.923354
6.537966	616.952277	8.928371
6.893345	621.554859	8.933389
6.330279	612.533075	8.938407
6.792201	631.159406	8.943424
6.796669	641.406634	8.948442
7.003274	642.890597	8.953459
6.987999	656.035341	8.958477
6.772802	652.015638	8.963495
7.353656	642.694090	8.968512
6.795123	627.437576	8.973530
6.951154	612.738652	8.978547
6.942945	619.942276	8.983565
6.847995	615.542248	8.988583
6.926783	610.762297	8.993600
6.791769	614.935876	8.998618
6.958309	614.827743	9.003635
6.832493	621.594590	9.008653
6.885353	637.346562	9.013671
7.217143	637.324879	9.018688
6.864430	629.339382	9.023706
6.788957	634.523900	9.028723
7.306198	637.354101	9.033741
7.093726	633.974581	9.038759
7.188996	616.301510	9.043776
6.902105	615.064993	9.048794
6.954490	613.737278	9.053811
6.851269	614.558006	9.058829
6.627814	614.787204	9.063847
7.162106	613.714532	9.068864
6.994199	625.453247	9.073882
7.115630	622.811117	9.078899
6.836153	617.018031	9.083917
6.955429	626.541489	9.088935
7.107225	620.482680	9.093952
6.774412	625.574511	9.098970
7.087932	632.892068	9.103987
7.214761	640.824821	9.109005
7.116558	635.312835	9.114023
7.265725	626.246951	9.119040
6.999041	623.953847	9.124058
6.910150	610.372560	9.129075
6.580560	626.473987	9.134093
6.908092	643.391173	9.139111
7.158096	631.248859	9.144128
7.054434	639.093051	9.149146
7.112924	632.330500	9.154163
6.969410	642.708660	9.159181
7.093940	636.006834	9.164199
7.106928	640.655770	9.169216
7.329466	647.242446	9.174234
6.934229	646.793471	9.179251
7.394072	639.965477	9.184269
7.269790	636.778528	9.189287
7.204412	633.659391	9.194304
6.687951	643.337022	9.199322
6.949246	637.924455	9.204339
7.261608	639.367816	9.209357
7.013646	647.486697	9.214375
7.065625	647.410683	9.219392
7.368220	639.496284	9.224410
7.197620	634.654506	9.229427
7.153248	642.616731	9.234445
7.086583	643.354762	9.239463
7.005708	637.651856	9.244480
6.870501	644.026048	9.249498
7.124914	642.366279	9.254515
7.129148	649.472111	9.259533
7.175040	657.664166	9.264551
7.101326	648.739412	9.269568
7.079754	654.895556	9.274586
7.294852	666.080351	9.279603
7.588462	667.967086	9.284621
7.375285	656.118677	9.289639
7.302477	651.542669	9.294656
7.168384	654.004417	9.299674
7.411460	662.211518	9.304691
7.223186	663.805809	9.309709
7.260624	675.908389	9.314727
7.356149	661.026540	9.319744
7.199488	670.345671	9.324762
7.067559	669.845113	9.329779
7.413902	675.428059	9.334797
7.200840	688.198012	9.339815
7.360535	686.382761	9.344832
7.536008	672.422163	9.349850
7.579293	679.161583	9.354867
7.610390	667.496083	9.359885
7.410924	672.381479	9.364903
7.425661	653.401544	9.369920
7.494818	653.679416	9.374938
6.914762	651.960338	9.379955
6.905400	669.177374	9.384973
7.013238	674.417226	9.389991
7.542614	683.654681	9.395008
7.527552	674.543481	9.400026
7.502094	677.687348	9.405043
7.699055	674.079656	9.410061
7.521255	687.139199	9.415079
7.471254	678.202341	9.420096
7.640186	677.649112	9.425114
7.452568	684.288331	9.430131
7.599074	667.811827	9.435149
7.638623	673.854944	9.440167
7.700294	671.170920	9.445184
7.437375	663.809425	9.450202
7.330739	660.268046	9.455219
7.685447	663.029853	9.460237
7.425004	669.714953	9.465255
7.651899	662.391489	9.470272
7.344796	661.264882	9.475290
7.360597	673.093528	9.480307
7.587272	662.288854	9.485325
7.236673	682.885203	9.490343
7.427929	674.570660	9.495360
7.541692	670.197925	9.500378
7.148704	675.557838	9.505395
7.370988	674.583466	9.510413
7.605311	675.076027	9.515431
7.490301	677.864682	9.520448
7.744088	680.333287	9.525466
7.615881	680.231843	9.530483
7.997940	674.292609	9.535501
7.516590	675.903056	9.540519
7.706165	684.121667	9.545536
7.516162	680.389570	9.550554
7.309816	679.805756	9.555571
8.095706	679.266101	9.560589
7.795871	680.476542	9.565607
7.824360	675.941650	9.570624
7.826349	665.470900	9.575642
7.632859	684.184348	9.580659
7.902752	668.925119	9.585677
7.594875	680.413533	9.590695
7.733671	681.022747	9.595712
8.000601	672.159579	9.600730
7.569916	676.786390	9.605747
7.805343	670.203009	9.610765
7.547491	670.420375	9.615783
7.485545	678.945459	9.620800
8.051329	671.483129	9.625818
7.738955	671.667485	9.630835
7.914825	659.331336	9.635853
7.544273	675.512306	9.640871
7.548648	674.775286	9.645888
7.747855	683.657044	9.650906
7.629479	677.878840	9.655923
7.786106	675.627170	9.660941
7.608798	683.807905	9.665959
7.581663	683.135726	9.670976
7.587612	676.200474	9.675994
7.495096	684.321732	9.681011
7.767447	670.104817	9.686029
7.564303	672.297224	9.691047
7.242202	683.089695	9.696064
7.945205	680.358927	9.701082
7.930341	687.158049	9.706099
7.868769	679.225478	9.711117
7.709594	675.826119	9.716135
7.635432	686.651129	9.721152
7.814160	692.868264	9.726170
7.903431	706.852507	9.731187
8.127904	702.881371	9.736205
8.325981	694.404893	9.741223
7.770248	676.807450	9.746240
7.981851	673.264747	9.751258
7.607309	671.653314	9.756275
7.735796	672.941566	9.761293
7.575077	691.588399	9.766311
7.933106	694.086031	9.771328
7.833335	698.895620	9.776346
7.698718	711.049392	9.781363
8.514187	702.250057	9.786381
8.411745	707.609399	9.791399
8.012165	698.797020	9.796416
8.278671	688.988121	9.801434
7.680737	681.297700	9.806451
8.114906	670.144616	9.811469
8.135385	686.646438	9.816487
7.756121	687.738829	9.821504
7.682959	676.705596	9.826522
7.669567	699.074251	9.831539
8.264161	706.764118	9.836557
8.281229	704.276302	9.841575
8.197451	702.971376	9.846592
7.975032	694.317778	9.851610
7.847231	698.687986	9.856627
8.182884	698.537244	9.861645
8.026373	698.728317	9.866663
7.621671	706.578009	9.871680
7.907239	703.804331	9.876698
7.871947	708.498267	9.881715
7.939626	711.651646	9.886733
8.082957	717.148789	9.891751
7.897666	710.725549	9.896768
8.008566	707.513301	9.901786
7.989806	701.462079	9.906803
8.054321	709.409297	9.911821
8.278275	707.813993	9.916839
8.116598	706.296587	9.921856
8.111716	695.428895	9.926874
7.939785	717.076767	9.931891
8.154476	714.577843	9.936909
8.140685	708.625384	9.941927
7.902356	706.279264	9.946944
8.185786	700.705960	9.951962
7.719045	714.508619	9.956979
8.408185	716.894166	9.961997
8.354266	731.058561	9.967015
8.155863	738.779804	9.972032
8.502207	734.191876	9.977050
8.212854	726.511942	9.982067
8.270955	720.339271	9.987085
8.603821	705.341892	9.992103
8.132811	710.989365	9.997120
8.542240	699.817517	10.002138
8.472226	704.675232	10.007155
8.574857	703.185002	10.012173
8.701456	701.296886	10.017191
8.234075	708.756321	10.022208
8.653470	700.600877	10.027226
8.643805	697.616785	10.032243
8.678468	710.109740	10.037261
8.450981	705.636526	10.042279
8.204042	713.156957	10.047296
8.660300	702.547934	10.052314
8.568355	703.763877	10.057331
8.286641	685.145434	10.062349
8.234855	682.726766	10.067367
8.138416	693.931181	10.072384
8.528456	692.428882	10.077402
8.512084	690.706199	10.082419
8.526877	706.604369	10.087437
8.593663	692.358128	10.092455
8.241932	678.431508	10.097472
8.411740	674.009360	10.102490
8.599862	673.623400	10.107507
8.383787	678.878206	10.112525
8.655279	654.842494	10.117543
8.407863	676.115059	10.122560
8.436362	668.705797	10.127578
8.172496	668.814827	10.132595
7.939989	682.121846	10.137613
8.088096	684.833661	10.142631
8.235496	704.827760	10.147648
8.628525	694.347576	10.152666
8.368471	706.162297	10.157683
8.609704	699.047529	10.162701
8.572191	703.292602	10.167719
8.780019	701.022233	10.172736
8.529757	699.272169	10.177754
8.412518	705.754617	10.182771
8.443535	705.336657	10.187789
8.627506	697.890371	10.192807
8.396431	702.987950	10.197824
8.715805	698.897115	10.202842
8.730640	699.476529	10.207859
8.278361	694.225066	10.212877
8.321907	703.429552	10.217895
8.459645	695.470530	10.222912
8.460749	687.611736	10.227930
8.437120	706.419953	10.232947
8.323529	705.150165	10.237965
8.470250	701.381902	10.242983
8.547169	722.320079	10.248000
8.922305	735.136936	10.253018
8.718105	711.591384	10.258035
8.703151	714.713743	10.263053
8.983128	698.163782	10.268071
8.701340	704.130705	10.273088
8.779182	691.249416	10.278106
8.658125	706.377858	10.283123
8.799661	701.882632	10.288141
8.563257	691.850006	10.293159
8.084310	710.159954	10.298176
8.414077	718.610488	10.303194
8.346382	723.133339	10.308211
8.434469	739.547386	10.313229
8.806431	742.551194	10.318247
8.873414	735.635057	10.323264
8.801000	733.322526	10.328282
9.187832	728.419008	10.333299
8.982361	742.080011	10.338317
8.898048	724.103482	10.343335
8.977439	728.265081	10.348352
8.800010	742.032158	10.353370
9.115532	738.057677	10.358387
8.789977	736.914236	10.363405
8.842871	739.265978	10.368423
8.658802	738.936602	10.373440
9.233457	726.620605	10.378458
9.277469	712.870933	10.383475
8.805648	710.843562	10.388493
8.932202	687.727945	10.393511
8.871923	701.357144	10.398528
8.399621	707.689251	10.403546
8.724098	709.218100	10.408563
8.665083	734.280667	10.413581
8.897342	731.227558	10.418599
8.905497	746.696236	10.423616
8.763014	731.989059	10.428634
8.687101	731.161976	10.433651
8.995395	732.735326	10.438669
9.024275	732.694914	10.443687
8.844617	730.130863	10.448704
9.025450	745.558801	10.453722
9.328373	733.021118	10.458739
8.979741	742.368081	10.463757
9.015611	728.874516	10.468775
9.145240	738.606826	10.473792
8.986896	734.263589	10.478810
9.262665	724.090309	10.483827
8.946159	736.889205	10.488845
9.103462	718.039639	10.493863
8.871646	741.422324	10.498880
9.098261	724.990581	10.503898
9.175783	727.216423	10.508915
8.875547	728.077391	10.513933
8.961598	730.093692	10.518951
8.703406	733.049202	10.523968
8.844716	726.671276	10.528986
8.863066	720.652588	10.534003
8.795659	734.909652	10.539021
9.140978	728.698861	10.544039
9.149331	738.145165	10.549056
8.931250	737.855656	10.554074
9.325817	736.490474	10.559091
8.744112	744.890502	10.564109
8.961365	741.053400	10.569127
9.041819	753.456652	10.574144
9.499546	766.054609	10.579162
9.568421	750.233939	10.584179
9.271346	750.435646	10.589197
9.125026	737.091748	10.594215
9.221086	733.479559	10.599232
9.003509	737.830663	10.604250
9.214441	741.663497	10.609267
9.089466	750.649546	10.614285
9.620252	754.265874	10.619303
9.360714	753.537233	10.624320
9.012812	744.295201	10.629338
9.473883	741.336834	10.634355
9.041280	743.777467	10.639373
9.604966	745.858513	10.644391
9.320372	743.678370	10.649408
9.375459	744.933688	10.654426
9.606525	736.378914	10.659443
9.168066	725.441932	10.664461
9.439387	729.954815	10.669479
9.568014	731.987600	10.674496
9.219544	728.691644	10.679514
9.058759	727.093296	10.684531
9.098356	726.388831	10.689549
9.407739	739.345374	10.694567
9.290308	749.933233	10.699584
9.168161	749.229517	10.704602
9.505609	756.217648	10.709619
9.389702	767.356645	10.714637
9.562545	762.786949	10.719655
9.320700	762.268928	10.724672
9.183522	772.898052	10.729690
9.379282	763.483799	10.734707
9.189482	770.564675	10.739725
9.327408	764.547563	10.744743
9.653164	768.908477	10.749760
9.625176	771.753327	10.754778
9.786942	764.579331	10.759795
9.152229	763.973407	10.764813
9.412566	759.382069	10.769831
9.538029	764.302758	10.774848
9.858831	759.005293	10.779866
9.653327	751.101981	10.784883
9.024045	765.789857	10.789901
9.299599	756.896086	10.794919
9.685484	758.514381	10.799936
9.159581	753.563299	10.804954
9.356158	760.393150	10.809971
9.295680	765.104648	10.814989
9.669371	743.878962	10.820007
9.337241	760.959709	10.825024
9.331974	757.350285	10.830042
9.655984	755.774164	10.835059
9.789178	762.013022	10.840077
9.617148	765.690880	10.845095
9.904552	757.278332	10.850112
9.457826	762.045295	10.855130
9.535119	755.400033	10.860147
9.506926	763.959344	10.865165
9.896020	777.562962	10.870183
9.550261	756.489806	10.875200
9.626534	768.872703	10.880218
9.820496	783.798599	10.885235
9.808961	785.554410	10.890253
9.674501	787.613556	10.895271
9.814581	788.187135	10.900288
9.903419	782.485850	10.905306
10.022994	765.177916	10.910323
9.725293	765.374511	10.915341
9.728582	765.011516	10.920359
9.906353	764.101276	10.925376
9.750469	775.099864	10.930394
9.913737	753.253937	10.935411
9.867257	766.635583	10.940429
9.696348	766.071495	10.945447
9.676167	756.769591	10.950464
9.848887	769.551534	10.955482
9.760336	758.949252	10.960499
9.597545	765.156921	10.965517
9.615450	776.659373	10.970535
9.932235	800.015748	10.975552
10.125478	800.456254	10.980570
10.241535	783.075961	10.985587
9.882436	776.809641	10.990605
9.697872	770.553549	10.995623
9.658609	767.596181	11.000640
9.807288	789.468386	11.005658
10.024272	783.498723	11.010675
9.852781	786.677373	11.015693
10.127521	789.825778	11.020711
10.070888	788.076083	11.025728
10.221216	796.643797	11.030746
10.218450	776.529501	11.035763
10.009587	772.760741	11.040781
9.562783	779.551770	11.045799
10.110418	781.797847	11.050816
9.961082	792.094900	11.055834
10.101482	780.739146	11.060851
10.201939	794.623016	11.065869
10.103467	793.330351	11.070887
10.433645	784.954117	11.075904
9.624788	779.930712	11.080922
9.942203	770.229568	11.085939
10.091376	787.858058	11.090957
10.018562	788.056262	11.095975
10.257142	793.547040	11.100992
9.733310	794.989747	11.106010
10.230133	800.482825	11.111027
10.372618	791.372582	11.116045
10.100363	784.164513	11.121063
10.065754	794.814983	11.126080
9.755924	805.442449	11.131098
9.946708	790.219201	11.136115
10.091358	794.040367	11.141133
9.987654	794.952606	11.146151
9.977701	791.132667	11.151168
9.886207	791.345374	11.156186
10.116908	787.795356	11.161203
10.123567	793.134632	11.166221
9.976301	795.207408	11.171239
10.337455	790.754098	11.176256
9.675543	792.896570	11.181274
10.227085	807.023568	11.186291
10.575512	806.279676	11.191309
10.335970	811.168982	11.196327
10.442272	792.357472	11.201344
10.149938	790.142387	11.206362
10.388680	792.209533	11.211379
10.270397	799.955059	11.216397
9.840962	799.180686	11.221415
10.682944	808.076550	11.226432
10.217482	818.340442	11.231450
10.217221	818.271485	11.236467
10.329429	814.350560	11.241485
10.308691	820.831575	11.246503
10.781736	817.218278	11.251520
10.587542	839.536419	11.256538
10.731761	815.404088	11.261555
10.412094	809.783880	11.266573
10.496529	810.119357	11.271591
10.712810	796.632822	11.276608
10.321446	802.380926	11.281626
10.384034	799.264521	11.286643
10.269565	803.455716	11.291661
10.674659	797.906457	11.296679
10.645223	788.958953	11.301696
10.408681	800.745259	11.306714
10.636609	786.140864	11.311731
10.586221	799.720886	11.316749
10.630457	787.221578	11.321767
10.758479	779.364200	11.326784
10.434175	797.299349	11.331802
10.606522	795.072225	11.336819
10.517368	791.422040	11.341837
10.434025	802.806326	11.346855
10.824757	788.502722	11.351872
10.404119	809.998847	11.356890
10.676655	792.648285	11.361907
10.636209	790.848088	11.366925
10.536768	807.868292	11.371943
10.638450	787.476039	11.376960
10.554686	800.450662	11.381978
10.243999	791.078950	11.386995
10.688044	798.348251	11.392013
10.575986	784.899945	11.397031
10.828170	798.705900	11.402048
10.883229	805.724384	11.407066
10.409408	794.325267	11.412083
10.732794	794.968635	11.417101
10.538477	813.977798	11.422119
10.833594	813.590588	11.427136
10.827620	813.911483	11.432154
11.095534	808.651772	11.437171
10.828088	794.790237	11.442189
10.628733	783.607536	11.447207
10.750554	780.379396	11.452224
10.418546	794.093928	11.457242
10.599579	801.591897	11.462259
10.807721	809.973423	11.467277
10.404042	827.705326	11.472295
10.948102	811.215915	11.477312
10.842494	825.502895	11.482330
10.867029	819.331302	11.487347
10.989050	810.078688	11.492365
10.851707	822.862416	11.497383
11.029397	815.402253	11.502400
10.903467	820.111201	11.507418
10.974878	813.797439	11.512435
10.943078	808.432756	11.517453
10.809713	821.227732	11.522471
11.036103	811.815080	11.527488
10.722949	807.452138	11.532506
10.670075	807.952604	11.537523
11.073254	802.126740	11.542541
10.525402	808.174279	11.547559
10.905633	803.107094	11.552576
10.868718	810.260344	11.557594
10.726342	805.240453	11.562611
10.960772	804.943474	11.567629
10.807132	811.904438	11.572647
10.767514	817.749510	11.577664
10.878515	820.425855	11.582682
10.820473	815.724250	11.587699
10.927131	826.570255	11.592717
11.248965	835.288161	11.597735
11.139296	836.338077	11.602752
11.458291	842.684232	11.607770
11.102088	820.583956	11.612787
10.890240	812.436231	11.617805
10.854046	834.388649	11.622823
11.396155	826.580316	11.627840
11.543123	827.525529	11.632858
11.336315	815.555591	11.637875
11.327465	812.606571	11.642893
11.219363	808.738686	11.647911
11.370380	804.820600	11.652928
11.416129	811.007504	11.657946
11.211792	806.736501	11.662963
11.260058	802.432711	11.667981
11.091577	810.902751	11.672999
11.231275	804.746281	11.678016
11.102162	810.462858	11.683034
11.248888	802.876147	11.688051
10.997153	800.808753	11.693069
10.776876	804.160696	11.698087
11.103999	818.215065	11.703104
11.225419	834.348261	11.708122
11.190740	840.019918	11.713139
11.738347	830.239266	11.718157
11.723147	832.461945	11.723175
11.624025	810.219513	11.728192
11.558987	806.899925	11.733210
11.027444	800.630799	11.738227
11.163781	795.116015	11.743245
11.211068	805.646875	11.748263
11.733506	821.285713	11.753280
11.382874	815.218829	11.758298
11.188350	807.522495	11.763315
11.504603	820.247302	11.768333
11.545601	841.579010	11.773351
11.518613	827.015227	11.778368
11.555013	819.076431	11.783386
11.444016	811.013499	11.788403
11.256068	807.339683	11.793421
11.167732	818.976730	11.798439
11.916801	830.708136	11.803456
11.786113	819.105275	11.808474
11.442653	809.481827	11.813491
11.654578	813.722121	11.818509
11.478921	813.992330	11.823527
11.343744	813.641097	11.828544
11.355245	811.642090	11.833562
11.634553	833.303041	11.838579
11.994994	825.485859	11.843597
11.740395	815.677182	11.848615
11.184367	817.263376	11.853632
11.473919	817.361154	11.858650
11.711888	832.045909	11.863667
11.906521	834.198486	11.868685
11.694220	840.403640	11.873703
11.404809	819.769826	11.878720
11.361348	831.754425	11.883738
11.358910	844.836687	11.888755
11.521008	842.883840	11.893773
11.732475	850.361551	11.898791
11.730390	847.017381	11.903808
12.001657	837.633019	11.908826
11.723468	841.635077	11.913843
11.787133	840.701374	11.918861
11.740417	841.405709	11.923879
11.734003	841.441097	11.928896
11.964630	843.728451	11.933914
11.658263	839.885449	11.938931
12.081995	841.066963	11.943949
11.804810	851.812667	11.948967
11.824331	841.794825	11.953984
11.663187	833.425066	11.959002
11.712301	843.096253	11.964019
11.937513	835.787155	11.969037
11.758583	837.837222	11.974055
11.956907	834.079195	11.979072
12.140920	836.747611	11.984090
11.815868	842.461940	11.989107
11.686759	846.900603	11.994125
11.765344	819.864558	11.999143
11.760630	842.752566	12.004160
11.641592	826.529285	12.009178
11.706092	836.409010	12.014195
11.866155	829.910739	12.019213
11.937968	836.338480	12.024231
12.078470	843.585831	12.029248
12.165494	834.913590	12.034266
11.919849	842.370495	12.039283
11.970402	833.650256	12.044301
12.042838	836.590609	12.049319
11.399338	837.843880	12.054336
12.154164	847.211767	12.059354
12.139660	869.675818	12.064371
12.369336	858.465856	12.069389
12.330562	858.580890	12.074407
12.116163	857.792332	12.079424
12.161785	841.920106	12.084442
11.891023	831.173900	12.089459
12.283219	844.855103	12.094477
12.536300	843.318445	12.099495
12.028159	839.412348	12.104512
12.116381	827.334404	12.109530
11.991170	836.356953	12.114547
12.527041	842.136160	12.119565
12.377576	835.777703	12.124583
12.014443	841.020455	12.129600
12.291822	829.687395	12.134618
12.097888	834.763528	12.139635
12.048785	830.503473	12.144653
12.266269	840.308715	12.149671
12.213340	860.599757	12.154688
12.476590	856.687517	12.159706
12.278935	861.998288	12.164723
12.351045	849.539689	12.169741
12.764386	853.435838	12.174759
12.021996	838.593976	12.179776
12.197931	831.887605	12.184794
12.459156	848.207912	12.189811
12.268635	846.205678	12.194829
12.215053	863.353284	12.199847
12.346085	856.024510	12.204864
12.602961	857.637762	12.209882
12.354334	864.209004	12.214899
12.505171	846.580512	12.219917
12.372872	859.348676	12.224935
12.251706	848.255941	12.229952
12.975798	851.431561	12.234970
12.521912	868.304438	12.239987
12.587547	860.890521	12.245005
12.738688	856.468158	12.250023
12.761330	836.319275	12.255040
12.614625	832.770601	12.260058
12.351845	833.768963	12.265075
12.414871	823.630675	12.270093
12.573033	822.239898	12.275111
12.177954	831.066237	12.280128
12.552878	836.907762	12.285146
12.634653	861.299646	12.290163
12.591983	866.682427	12.295181
12.818383	850.264363	12.300199
12.784548	860.379115	12.305216
12.659728	844.649599	12.310234
12.370312	858.033191	12.315251
12.529338	856.285342	12.320269
12.524006	861.039126	12.325287
12.457432	868.627545	12.330304
12.684031	853.180932	12.335322
12.576371	859.767749	12.340339
12.765103	859.101024	12.345357
12.597284	860.844586	12.350375
12.776708	859.977072	12.355392
12.755423	855.843296	12.360410
12.738461	860.735002	12.365427
12.590354	864.078967	12.370445
12.818130	870.052972	12.375463
12.373457	870.107152	12.380480
12.640427	862.467082	12.385498
12.454265	866.254859	12.390515
12.664615	874.791541	12.395533
12.930843	889.574124	12.400551
12.846635	894.638344	12.405568
13.436117	884.989985	12.410586
12.766687	867.036078	12.415603
13.042004	866.457388	12.420621
12.907136	868.813215	12.425639
12.712943	864.427153	12.430656
12.848495	863.281505	12.435674
13.088683	872.064097	12.440691
12.852044	879.860319	12.445709
13.152218	884.530559	12.450727
13.080221	884.125190	12.455744
13.044199	857.501946	12.460762
12.933453	868.447284	12.465779
12.463887	872.205433	12.470797
13.063543	886.555616	12.475815
12.891487	890.268246	12.480832
13.173315	902.710868	12.485850
13.346688	893.530806	12.490867
13.191776	910.362392	12.495885
13.369669	897.512321	12.500903
13.151266	897.385432	12.505920
13.163807	865.204408	12.510938
13.180213	865.945942	12.515955
12.963501	862.621393	12.520973
12.969341	873.332642	12.525991
12.926059	890.132079	12.531008
13.144660	888.392096	12.536026
13.153612	895.342957	12.541043
13.163114	899.552071	12.546061
13.088493	898.354356	12.551079
13.175646	899.659595	12.556096
13.287213	890.355914	12.561114
13.023453	901.734955	12.566131
13.155611	912.726389	12.571149
13.326624	892.818223	12.576167
13.252530	905.762699	12.581184
13.445548	894.788553	12.586202
13.161141	894.223436	12.591219
13.246944	901.386956	12.596237
13.264329	903.823613	12.601255
13.147224	906.603307	12.606272
13.280917	886.978434	12.611290
13.471009	892.200241	12.616307
12.982552	892.156556	12.621325
13.522532	895.530298	12.626343
13.202582	900.819665	12.631360
13.481179	890.822746	12.636378
13.252086	893.860077	12.641395
13.360246	903.704288	12.646413
13.912520	911.655344	12.651431
13.384782	906.920128	12.656448
13.492560	916.072401	12.661466
13.697787	892.003576	12.666483
13.527146	898.338952	12.671501
13.606296	893.969118	12.676519
13.411893	895.939087	12.681536
13.408821	895.677812	12.686554
13.690817	913.907619	12.691571
13.706849	919.030072	12.696589
13.595516	903.208617	12.701607
13.665121	902.494462	12.706624
13.672583	900.259144	12.711642
13.671577	907.992823	12.716659
13.413637	907.375505	12.721677
13.770301	899.882772	12.726695
13.712181	916.276590	12.731712
13.871914	919.500023	12.736730
13.829674	908.973533	12.741747
13.371298	902.130557	12.746765
13.933391	901.245268	12.751783
13.840387	918.999939	12.756800
13.771371	907.401875	12.761818
13.776074	903.625738	12.766835
13.762256	914.560995	12.771853
13.938170	906.299642	12.776871
13.797021	913.403838	12.781888
13.781340	906.817963	12.786906
13.958730	911.260512	12.791923
13.673992	908.334432	12.796941
14.119997	903.747304	12.801959
13.683161	902.093786	12.806976
13.814227	906.158031	12.811994
13.881910	899.454857	12.817011
13.940612	918.120518	12.822029
13.645480	916.321751	12.827047
13.929121	914.257093	12.832064
13.742601	919.539965	12.837082
13.895929	911.489393	12.842099
13.924109	908.377570	12.847117
14.055308	908.108277	12.852135
13.887360	910.997734	12.857152
13.889180	912.860882	12.862170
14.174186	914.770129	12.867187
14.015525	920.752019	12.872205
14.344743	909.710086	12.877223
14.328613	915.566863	12.882240
14.199225	906.120935	12.887258
14.119207	912.465353	12.892275
14.153069	911.233964	12.897293
14.384623	908.943112	12.902311
14.521431	913.526991	12.907328
14.005324	910.872373	12.912346
14.027086	890.785561	12.917363
13.943128	900.237969	12.922381
13.966764	907.506827	12.927399
14.065860	909.470415	12.932416
13.930052	908.481595	12.937434
14.270202	912.026924	12.942451
14.127112	913.171230	12.947469
14.362711	912.699086	12.952487
14.020307	909.095250	12.957504
14.038733	915.359435	12.962522
14.470048	912.688582	12.967539
14.238535	912.715015	12.972557
14.503389	914.961592	12.977575
14.670702	904.475856	12.982592
14.265988	907.550084	12.987610
14.576535	912.083406	12.992627
14.085249	914.733039	12.997645
14.485865	908.353913	13.002663
14.302053	909.850165	13.007680
14.101663	903.725451	13.012698
14.435466	908.940441	13.017715
14.353833	909.466821	13.022733
14.300980	910.568464	13.027751
14.415453	906.716716	13.032768
14.438500	907.250792	13.037786
14.253045	904.243159	13.042803
14.286175	924.782618	13.047821
14.782525	933.556766	13.052839
15.277187	924.546389	13.057856
14.747685	908.173665	13.062874
14.967478	907.493146	13.067891
14.584597	902.597008	13.072909
14.685357	901.086106	13.077927
14.724237	903.696543	13.082944
14.592681	901.032700	13.087962
14.671052	891.167868	13.092979
14.443438	909.126040	13.097997
14.841581	900.137925	13.103015
14.619361	902.930659	13.108032
14.479182	909.200190	13.113050
14.798880	895.418376	13.118067
14.550700	907.028469	13.123085
14.677575	902.505101	13.128103
14.638774	904.567250	13.133120
14.656255	903.679850	13.138138
14.623539	901.607837	13.143155
14.647168	911.750227	13.148173
14.936479	922.713336	13.153191
14.925605	924.738004	13.158208
14.947700	914.634860	13.163226
15.110836	901.260936	13.168243
15.207746	903.994241	13.173261
14.852588	903.820475	13.178279
15.070658	891.445578	13.183296
14.829367	896.749893	13.188314
14.986239	902.402121	13.193331
14.523898	898.701592	13.198349
14.796777	902.139944	13.203367
14.921932	896.407226	13.208384
14.907301	897.131158	13.213402
15.150057	899.801982	13.218419
14.834752	908.857267	13.223437
15.119309	923.845284	13.228455
15.015249	913.532319	13.233472
14.739061	930.705764	13.238490
15.186936	922.019208	13.243507
15.028467	931.524886	13.248525
15.064422	925.214871	13.253543
15.284168	927.150060	13.258560
15.210350	931.090912	13.263578
15.070541	924.084081	13.268595
15.137039	929.984679	13.273613
15.155806	936.050818	13.278631
15.204843	925.813906	13.283648
15.175569	934.737307	13.288666
15.614302	932.910949	13.293683
15.300869	928.957103	13.298701
15.221173	913.196343	13.303719
15.324669	928.838590	13.308736
14.904783	937.098319	13.313754
15.496211	932.460187	13.318771
15.356408	930.211805	13.323789
15.246240	931.059383	13.328807
15.632358	932.347104	13.333824
15.366053	941.538775	13.338842
15.113219	937.631596	13.343859
15.428538	937.161235	13.348877
15.102140	932.190213	13.353895
15.147788	936.623444	13.358912
15.099978	929.131997	13.363930
15.609635	940.316340	13.368947
15.105239	942.481022	13.373965
15.334677	935.452726	13.378983
15.408129	929.544908	13.384000
15.239765	936.877984	13.389018
15.499203	935.253668	13.394035
15.475772	930.556148	13.399053
15.533142	936.619254	13.404071
15.614961	932.339504	13.409088
15.428132	937.451005	13.414106
15.664934	938.019235	13.419123
15.710314	933.640996	13.424141
15.492542	943.995908	13.429159
15.804191	930.652525	13.434176
15.828499	937.539855	13.439194
15.490146	930.974030	13.444211
15.588238	937.003442	13.449229
15.290268	939.181247	13.454247
15.813075	938.388064	13.459264
15.562089	939.625387	13.464282
15.410148	929.703920	13.469299
15.461978	957.511553	13.474317
15.549937	962.364893	13.479335
15.685031	958.102509	13.484352
15.555379	968.128951	13.489370
16.043910	962.054512	13.494387
15.873106	962.593464	13.499405
16.256812	965.313239	13.504423
16.149677	964.425762	13.509440
16.019842	962.012567	13.514458
15.985172	948.597089	13.519475
15.968122	941.224549	13.524493
15.674749	937.390987	13.529511
15.968645	936.641537	13.534528
15.929975	957.259429	13.539546
15.958607	957.278103	13.544563
16.161317	948.153977	13.549581
16.089168	956.241506	13.554599
16.076343	937.381406	13.559616
15.760857	941.304333	13.564634
15.812605	937.766239	13.569651
15.770815	948.489249	13.574669
15.786702	957.647680	13.579687
16.049565	948.927521	13.584704
15.885547	957.938939	13.589722
15.955272	949.414055	13.594739
16.071535	949.526891	13.599757
16.167385	956.093009	13.604775
16.089015	955.805797	13.609792
15.806774	968.162583	13.614810
16.282818	956.215988	13.619827
16.261143	958.712249	13.624845
15.747252	960.956049	13.629863
16.164324	957.304241	13.634880
15.821920	955.603424	13.639898
15.790164	979.095511	13.644915
16.088223	976.806058	13.649933
15.885674	976.492524	13.654951
16.628590	983.594335	13.659968
16.531709	990.692629	13.664986
16.753656	976.898161	13.670003
16.711460	981.242395	13.675021
16.822859	978.554331	13.680039
16.671653	958.934131	13.685056
16.201097	951.144485	13.690074
16.315022	943.355877	13.695091
16.546529	953.856789	13.700109
16.433013	948.650419	13.705127
16.537604	941.337488	13.710144
16.454332	950.383582	13.715162
16.572016	944.848307	13.720179
16.548547	953.558590	13.725197
16.555536	956.490592	13.730215
16.426493	958.917210	13.735232
16.720954	954.135659	13.740250
16.657602	962.244962	13.745267
16.688518	960.074055	13.750285
16.444932	956.136607	13.755303
16.600287	952.329462	13.760320
16.451656	961.866401	13.765338
16.682896	975.950440	13.770355
16.964436	974.852497	13.775373
16.320636	966.357735	13.780391
16.750284	977.347487	13.785408
16.716719	981.647585	13.790426
16.613685	983.127741	13.795443
16.621531	986.033430	13.800461
16.467049	990.766830	13.805479
16.789671	978.918197	13.810496
16.706261	986.267371	13.815514
16.576665	993.663544	13.820531
16.579674	984.188800	13.825549
16.491709	993.036121	13.830567
16.710110	978.891704	13.835584
16.688856	987.108218	13.840602
16.701596	992.450888	13.845619
16.689834	986.284537	13.850637
16.583395	995.150658	13.855655
16.965428	999.135665	13.860672
17.074964	1012.303585	13.865690
16.964562	1014.457489	13.870707
17.182177	1014.538225	13.875725
17.044508	1010.008748	13.880743
17.169435	1002.398971	13.885760
16.649668	998.919683	13.890778
16.944552	1003.033248	13.895795
17.115582	1005.356553	13.900813
16.980165	1015.532576	13.905831
17.119760	1017.803804	13.910848
16.961025	1014.675807	13.915866
17.159636	1016.215155	13.920883
17.328392	1010.222278	13.925901
17.066485	1013.381374	13.930919
17.495050	1002.174557	13.935936
17.101241	1001.748951	13.940954
17.235727	1001.271470	13.945971
17.479210	1010.157123	13.950989
17.300040	1009.065835	13.956007
17.354516	1004.256025	13.961024
17.460239	1003.176113	13.966042
17.226352	1010.924317	13.971059
17.380634	1004.929700	13.976077
17.416511	1004.461035	13.981095
17.485169	1008.361633	13.986112
17.602640	1006.328557	13.991130
17.135184	988.116068	13.996147
17.552439	994.364173	14.001165
17.448548	1001.592546	14.006183
17.643178	1002.170700	14.011200
17.665998	987.473061	14.016218
17.279447	982.724527	14.021235
17.252967	976.607258	14.026253
17.310778	981.685039	14.031271
17.431850	991.996387	14.036288
17.383717	1010.739648	14.041306
17.484212	1004.229989	14.046323
17.563268	993.648560	14.051341
17.542914	1000.817269	14.056359
17.327162	1002.068850	14.061376
17.680741	1000.853310	14.066394
17.666046	1001.037779	14.071411
17.489877	995.716964	14.076429
17.445197	999.056856	14.081447
17.853022	976.998572	14.086464
17.913946	998.657367	14.091482
17.725752	1002.338248	14.096499
18.139506	994.184960	14.101517
17.559161	1009.376412	14.106535
17.902253	992.262646	14.111552
17.622561	1002.342049	14.116570
17.459587	999.278525	14.121587
17.678782	995.060885	14.126605
17.525383	998.786400	14.131623
17.711118	1000.444587	14.136640
17.662377	1002.309212	14.141658
17.554798	1004.953513	14.146675
18.117497	1013.979496	14.151693
17.770395	1025.111223	14.156711
18.226913	1037.353855	14.161728
18.271311	1028.108427	14.166746
18.140699	1006.207965	14.171763
17.658511	1007.454371	14.176781
17.877462	1008.054486	14.181799
17.804790	1011.212030	14.186816
18.105337	1020.100265	14.191834
17.943281	1030.267316	14.196851
18.177880	1019.874303	14.201869
18.321422	1036.829119	14.206887
18.115241	1020.398318	14.211904
17.999606	1028.254724	14.216922
18.139571	1026.152387	14.221939
18.222233	1028.544031	14.226957
18.169092	1037.073862	14.231975
18.384160	1030.209289	14.236992
18.455985	1023.272934	14.242010
18.082568	1015.150718	14.247027
18.616644	1007.469980	14.252045
18.306745	1008.006333	14.257063
18.173862	1007.983401	14.262080
18.405627	995.528808	14.267098
18.030005	1003.462214	14.272115
18.075366	1009.604487	14.277133
18.168033	1032.438010	14.282151
18.148052	1029.505746	14.287168
18.263810	1018.625171	14.292186
18.165224	1036.888298	14.297203
18.318427	1023.309447	14.302221
18.046721	1028.598954	14.307239
18.096883	1031.280175	14.312256
18.260925	1017.492287	14.317274
18.087748	1037.197627	14.322291
18.606413	1043.649037	14.327309
19.117261	1046.687722	14.332327
19.101418	1033.989809	14.337344
18.868915	1014.208197	14.342362
18.917673	1019.971627	14.347379
18.806123	1017.505212	14.352397
18.882337	1016.635064	14.357415
18.539168	1022.123356	14.362432
18.679453	1021.761433	14.367450
18.589877	1016.518608	14.372467
18.574078	1013.925759	14.377485
18.512789	1013.185009	14.382503
18.594465	1010.714022	14.387520
18.593567	1006.523695	14.392538
18.540896	1022.606935	14.397555
18.978729	1020.249896	14.402573
18.819343	1019.377743	14.407591
18.782806	1024.683890	14.412608
18.784727	1010.181975	14.417626
18.717612	1034.799494	14.422643
18.787643	1020.091267	14.427661
18.585420	1023.092888	14.432679
19.238564	1042.261944	14.437696
19.493043	1034.491592	14.442714
18.977457	1026.574134	14.447731
19.083498	1025.330021	14.452749
19.430393	1016.129084	14.457767
18.901983	1016.515947	14.462784
19.068202	1015.958234	14.467802
19.178522	1023.172278	14.472819
19.024525	1024.624842	14.477837
19.121059	1021.256857	14.482855
18.769483	1016.594643	14.487872
19.014287	1007.906958	14.492890
18.710469	1021.797221	14.497907
18.880582	1022.015904	14.502925
19.300073	1021.703298	14.507943
19.106032	1043.458612	14.512960
19.298593	1038.908801	14.517978
19.011644	1041.226311	14.522995
19.140319	1042.879762	14.528013
19.442078	1051.524153	14.533031
19.145334	1042.298286	14.538048
19.709599	1041.011711	14.543066
19.119528	1046.455394	14.548083
19.321810	1039.892291	14.553101
19.547591	1033.009021	14.558119
19.415434	1043.328595	14.563136
19.476192	1035.678036	14.568154
19.393511	1035.562767	14.573171
19.213475	1035.780267	14.578189
19.638662	1034.150200	14.583207
19.230628	1042.554853	14.588224
19.827609	1037.156446	14.593242
19.548809	1035.389016	14.598259
19.440779	1041.893996	14.603277
19.412182	1041.527506	14.608295
19.382930	1039.927070	14.613312
19.570008	1031.289456	14.618330
19.405469	1049.031692	14.623347
19.674851	1040.615277	14.628365
19.474141	1030.514236	14.633383
19.379605	1038.188646	14.638400
19.535388	1035.643017	14.643418
19.437755	1039.427819	14.648435
19.500444	1037.117420	14.653453
19.798994	1025.513045	14.658471
19.547858	1037.775390	14.663488
19.673375	1039.764741	14.668506
19.430742	1041.052849	14.673523
19.948976	1046.255319	14.678541
20.104989	1053.216787	14.683559
20.033307	1057.416530	14.688576
20.227211	1040.979424	14.693594
20.109882	1038.050649	14.698611
19.976236	1023.605961	14.703629
20.059418	1030.933531	14.708647
20.185159	1031.312868	14.713664
20.299989	1026.606839	14.718682
19.892511	1026.219509	14.723699
19.796805	1031.534845	14.728717
20.050337	1027.108799	14.733735
19.604501	1034.933962	14.738752
20.108358	1025.683659	14.743770
19.944944	1031.547696	14.748787
19.980593	1026.975598	14.753805
19.900179	1025.650701	14.758823
19.861631	1032.730321	14.763840
20.065602	1040.776005	14.768858
20.222176	1047.841101	14.773875
20.436617	1061.955353	14.778893
20.354209	1049.664820	14.783911
20.097596	1045.749775	14.788928
20.180781	1041.946660	14.793946
20.104240	1059.864888	14.798963
20.239343	1060.680798	14.803981
20.381663	1049.290381	14.808999
20.363635	1056.750614	14.814016
20.582112	1059.982476	14.819034
20.573688	1055.751261	14.824051
20.507401	1052.411357	14.829069
20.786579	1031.062727	14.834087
20.236875	1037.641678	14.839104
20.517783	1024.160010	14.844122
20.283691	1027.763849	14.849139
19.929008	1024.626703	14.854157
20.237208	1036.866093	14.859175
20.464820	1052.957762	14.864192
20.776314	1047.174316	14.869210
20.804143	1058.582440	14.874227
20.442774	1053.178055	14.879245
20.741207	1050.972374	14.884263
20.732470	1058.658005	14.889280
20.938193	1056.103333	14.894298
20.671863	1065.001033	14.899315
20.678429	1061.898458	14.904333
20.818002	1056.261314	14.909351
20.759983	1061.691673	14.914368
20.735940	1062.688779	14.919386
20.805060	1051.270306	14.924403
20.606738	1070.926112	14.929421
20.699008	1059.079859	14.934439
20.741986	1064.382130	14.939456
20.871014	1070.907585	14.944474
20.809640	1061.395212	14.949491
20.763693	1067.924584	14.954509
21.106199	1057.113187	14.959527
20.599403	1067.339790	14.964544
20.859570	1065.259113	14.969562
20.887985	1059.568301	14.974579
20.783587	1064.701847	14.979597
20.786228	1055.467042	14.984615
20.822023	1060.209367	14.989632
20.752895	1046.869763	14.994650
20.902198	1052.555182	14.999667
20.629775	1057.652329	15.004685
20.756933	1063.831294	15.009703
20.851437	1075.302811	15.014720
21.113496	1077.985828	15.019738
21.406762	1081.066381	15.024755
21.077810	1071.363217	15.029773
21.389462	1078.374752	15.034791
21.342367	1075.518800	15.039808
21.442815	1069.401382	15.044826
21.618560	1074.123537	15.049843
21.206515	1068.889109	15.054861
21.447462	1067.639822	15.059879
21.338193	1072.523231	15.064896
21.423057	1068.720817	15.069914
21.352999	1074.590503	15.074931
21.650057	1069.383358	15.079949
21.421468	1060.195815	15.084967
21.510528	1075.782733	15.089984
21.687039	1074.575979	15.095002
21.342692	1059.589199	15.100019
21.465069	1071.742808	15.105037
21.301196	1062.089130	15.110055
21.266699	1074.792991	15.115072
21.323514	1070.256156	15.120090
21.492990	1065.404492	15.125107
20.853768	1074.422077	15.130125
21.269258	1060.471752	15.135143
21.276611	1066.985230	15.140160
21.719261	1083.407676	15.145178
21.760884	1089.175067	15.150195
21.660161	1106.222679	15.155213
21.745922	1095.656408	15.160231
21.849883	1095.660075	15.165248
21.580736	1093.248033	15.170266
21.958899	1093.578376	15.175283
21.908609	1097.469524	15.180301
22.003369	1081.533919	15.185319
21.691044	1062.848531	15.190336
21.643565	1081.236512	15.195354
21.967401	1079.643067	15.200371
21.981372	1084.392746	15.205389
22.088223	1085.104682	15.210407
21.981133	1095.587051	15.215424
22.033211	1086.148223	15.220442
22.352246	1085.154886	15.225459
21.843043	1062.147998	15.230477
22.040621	1054.453564	15.235495
21.993571	1068.693304	15.240512
21.972064	1088.735793	15.245530
22.129527	1093.502504	15.250547
22.001692	1101.721537	15.255565
22.194571	1097.330883	15.260583
22.295577	1102.448409	15.265600
22.111131	1086.454624	15.270618
21.951221	1096.226938	15.275635
21.756985	1105.875227	15.280653
22.249387	1095.552928	15.285671
22.004291	1102.792087	15.290688
21.978715	1098.164938	15.295706
22.070789	1097.424033	15.300723
22.106842	1097.962265	15.305741
22.092967	1097.221745	15.310759
22.295713	1109.351672	15.315776
22.461366	1113.790315	15.320794
22.642809	1107.974409	15.325811
22.663777	1121.513302	15.330829
22.558493	1090.476888	15.335847
22.708393	1084.452851	15.340864
22.353142	1080.580863	15.345882
22.443575	1079.466274	15.350899
22.111271	1097.407916	15.355917
22.638078	1103.939293	15.360935
22.796842	1113.729615	15.365952
22.666287	1113.989719	15.370970
22.950043	1113.047085	15.375987
22.501206	1116.188085	15.381005
22.895012	1117.616262	15.386023
22.785899	1116.221899	15.391040
22.717527	1113.496798	15.396058
23.235194	1098.594463	15.401075
23.019485	1092.458426	15.406093
22.662820	1088.819311	15.411111
22.708121	1087.424233	15.416128
22.650228	1082.172017	15.421146
22.914947	1082.099913	15.426163
22.708320	1110.839370	15.431181
23.213888	1116.176615	15.436199
22.890991	1105.239944	15.441216
22.862696	1119.354998	15.446234
23.334528	1112.867184	15.451251
23.271735	1103.595729	15.456269
23.171462	1091.032568	15.461287
23.362084	1089.428465	15.466304
22.943728	1085.166574	15.471322
23.241252	1067.815804	15.476339
22.950416	1076.646509	15.481357
23.250953	1083.656144	15.486375
23.148283	1077.268597	15.491392
23.141149	1064.407040	15.496410
23.095336	1082.494401	15.501427
22.939021	1074.737592	15.506445
23.409092	1089.355011	15.511463
23.566868	1098.737677	15.516480
23.609746	1096.245730	15.521498
23.575297	1090.440117	15.526515
22.976797	1076.526850	15.531533
23.184006	1078.082301	15.536551
23.298315	1071.626227	15.541568
23.117458	1067.042265	15.546586
23.379991	1088.083909	15.551603
23.332509	1107.429251	15.556621
23.245993	1105.491475	15.561639
23.146872	1103.898249	15.566656
23.245849	1110.184039	15.571674
23.625359	1097.036353	15.576691
23.247212	1105.916340	15.581709
23.211196	1105.663064	15.586727
23.230848	1110.706845	15.591744
22.928209	1106.904885	15.596762
23.404057	1133.750978	15.601779
23.689052	1135.382346	15.606797
23.730869	1139.585398	15.611815
23.661875	1136.848783	15.616832
23.937775	1134.460426	15.621850
24.032055	1132.287487	15.626867
23.511163	1137.790231	15.631885
23.810428	1129.246604	15.636903
24.252264	1130.381851	15.641920
23.870221	1134.355976	15.646938
24.057735	1133.966564	15.651955
24.212515	1144.073853	15.656973
23.959244	1131.270039	15.661991
24.013021	1140.239078	15.667008
24.009879	1136.587389	15.672026
24.092200	1136.957569	15.677043
24.156057	1124.613085	15.682061
24.290515	1129.590664	15.687079
24.200507	1118.640298	15.692096
23.987542	1108.660897	15.697114
23.910429	1113.457522	15.702131
24.134118	1137.727000	15.707149
24.176114	1138.480360	15.712167
24.208545	1130.836796	15.717184
23.901495	1139.755440	15.722202
24.461616	1133.329984	15.727219
24.229701	1126.949603	15.732237
24.294301	1125.242324	15.737255
24.443452	1130.846709	15.742272
24.267410	1137.717835	15.747290
24.319748	1131.384165	15.752307
24.559891	1137.082159	15.757325
24.409831	1138.283136	15.762343
24.228586	1133.330181	15.767360
24.410081	1131.888580	15.772378
24.698079	1135.966514	15.777395
24.504652	1131.988060	15.782413
24.346770	1124.060644	15.787431
24.493118	1120.241365	15.792448
24.267005	1123.189876	15.797466
24.300846	1119.450596	15.802483
24.677921	1125.253694	15.807501
24.319663	1134.513816	15.812519
24.270290	1116.034674	15.817536
24.336179	1133.353360	15.822554
24.778402	1145.986571	15.827571
24.746916	1153.490604	15.832589
25.121108	1148.088235	15.837607
25.435912	1134.759112	15.842624
25.375319	1123.106351	15.847642
25.195147	1123.202437	15.852659
25.232906	1116.388384	15.857677
24.908169	1120.630551	15.862695
24.819591	1108.148895	15.867712
25.134105	1110.197954	15.872730
25.368932	1114.415948	15.877747
25.262744	1106.363679	15.882765
24.836716	1115.625935	15.887783
25.104274	1116.979518	15.892800
25.111810	1110.182664	15.897818
25.419727	1108.878023	15.902835
25.139455	1097.883337	15.907853
24.698301	1082.698982	15.912871
24.995986	1108.658083	15.917888
25.023700	1110.706119	15.922906
24.956529	1102.344893	15.927923
24.893504	1112.179344	15.932941
24.925655	1121.491263	15.937959
25.042887	1106.794244	15.942976
25.078552	1112.371319	15.947994
24.956108	1102.563745	15.953011
25.287898	1109.273785	15.958029
25.177582	1132.269918	15.963047
25.600242	1137.354574	15.968064
25.631103	1142.580737	15.973082
25.380424	1133.158451	15.978099
25.491991	1121.958860	15.983117
25.661832	1135.951634	15.988135
25.736233	1116.216008	15.993152
25.446803	1116.870026	15.998170
24.969436	1111.096660	16.003187
25.482127	1131.716966	16.008205
25.508074	1141.847118	16.013223
25.515262	1130.809236	16.018240
25.687908	1127.199158	16.023258
25.578154	1135.356963	16.028275
25.787141	1142.805704	16.033293
25.579020	1128.345866	16.038311
26.066285	1131.864573	16.043328
25.674082	1141.371413	16.048346
25.859467	1134.355031	16.053363
25.725563	1129.831193	16.058381
25.710940	1146.118872	16.063399
25.724702	1129.252456	16.068416
25.547632	1139.904860	16.073434
25.778918	1136.137673	16.078451
25.716744	1143.093512	16.083469
25.875456	1155.192568	16.088487
26.193616	1163.483579	16.093504
26.176819	1166.215646	16.098522
26.114115	1157.125220	16.103539
26.432965	1153.882451	16.108557
26.298049	1146.757404	16.113575
26.471438	1131.534035	16.118592
26.342290	1129.656836	16.123610
26.147777	1123.188399	16.128627
26.522118	1121.697020	16.133645
25.981239	1131.722047	16.138663
26.319834	1118.587992	16.143680
26.261754	1118.068916	16.148698
26.085422	1124.106356	16.153715
26.188167	1123.731149	16.158733
26.001137	1141.527595	16.163751
26.340445	1147.657168	16.168768
26.255993	1165.479401	16.173786
26.376361	1155.568882	16.178803
26.505126	1155.505861	16.183821
26.311004	1155.754623	16.188839
26.414898	1158.724776	16.193856
26.436892	1160.856428	16.198874
26.327129	1158.854584	16.203891
26.266532	1151.340343	16.208909
26.280363	1160.436842	16.213927
26.598497	1163.363719	16.218944
26.544702	1165.251637	16.223962
26.500163	1155.658876	16.228979
26.733069	1166.287243	16.233997
26.767195	1185.959106	16.239015
27.032805	1182.640104	16.244032
26.987482	1179.956253	16.249050
26.702174	1170.547737	16.254067
27.247581	1160.999194	16.259085
27.011922	1163.465505	16.264103
27.316331	1139.188593	16.269120
27.192853	1148.111940	16.274138
26.961323	1146.865737	16.279155
27.097547	1150.760717	16.284173
26.941042	1146.782259	16.289191
27.030271	1142.409114	16.294208
27.160180	1147.288843	16.299226
27.110463	1144.587618	16.304243
27.166981	1147.498088	16.309261
27.001179	1154.427560	16.314279
27.092223	1142.854237	16.319296
27.309649	1149.282256	16.324314
26.990187	1148.387737	16.329331
27.388254	1148.462075	16.334349
26.887094	1151.073622	16.339367
27.551207	1174.653938	16.344384
27.499346	1167.253188	16.349402
27.281472	1154.851119	16.354419
27.396921	1159.389003	16.359437
27.368456	1172.806603	16.364455
27.803093	1172.150403	16.369472
27.354441	1155.599903	16.374490
27.027034	1167.380544	16.379507
27.432884	1171.237271	16.384525
27.432743	1176.390825	16.389543
27.540737	1170.607305	16.394560
27.643158	1174.221700	16.399578
27.594614	1171.014448	16.404595
27.507054	1177.967019	16.409613
27.509997	1178.765214	16.414631
27.557737	1172.722400	16.419648
27.468665	1172.112001	16.424666
27.259379	1174.353911	16.429683
27.422005	1172.579452	16.434701
28.022628	1189.681903	16.439719
28.097182	1204.682658	16.444736
28.236292	1197.213333	16.449754
27.836423	1174.141365	16.454771
28.144032	1159.641935	16.459789
27.785905	1172.505837	16.464807
27.592362	1166.789468	16.469824
28.214757	1175.064261	16.474842
27.997473	1201.185968	16.479859
28.288553	1197.107552	16.484877
28.304109	1196.278515	16.489895
28.241228	1185.547797	16.494912
28.136781	1173.899292	16.499930
28.011463	1168.762110	16.504947
28.346925	1186.129995	16.509965
28.571121	1195.654477	16.514983
28.157978	1184.109725	16.520000
28.289116	1177.591386	16.525018
28.255998	1184.707378	16.530035
28.287288	1183.245326	16.535053
28.271555	1203.122075	16.540071
28.385468	1208.080440	16.545088
28.549121	1208.246461	16.550106
28.547825	1200.843637	16.555123
28.699709	1189.279712	16.560141
28.382171	1191.187401	16.565159
28.684519	1184.024915	16.570176
28.813555	1173.381173	16.575194
28.216876	1175.118486	16.580211
28.335737	1172.578936	16.585229
28.402820	1190.635763	16.590247
28.353170	1203.409547	16.595264
28.549728	1196.317285	16.600282
28.527149	1197.637141	16.605299
28.569125	1194.607809	16.610317
28.415126	1195.095967	16.615335
28.321507	1193.109165	16.620352
28.603144	1199.205973	16.625370
28.491765	1225.399183	16.630387
28.977746	1225.154710	16.635405
28.974555	1217.762229	16.640423
28.860955	1217.757761	16.645440
29.117095	1212.579177	16.650458
28.880108	1219.913887	16.655475
29.060472	1216.061211	16.660493
28.575961	1215.690344	16.665511
28.718213	1220.944773	16.670528
28.515263	1217.717364	16.675546
28.475569	1224.306784	16.680563
28.859847	1230.972579	16.685581
29.107449	1238.730884	16.690599
28.992491	1256.677734	16.695616
29.264735	1244.583912	16.700634
29.134252	1242.183966	16.705651
29.200446	1246.964823	16.710669
29.312692	1247.456616	16.715687
29.132710	1244.077594	16.720704
29.538047	1248.403254	16.725722
29.393119	1244.364795	16.730739
29.457652	1245.940888	16.735757
29.481412	1243.491047	16.740775
29.525398	1264.436390	16.745792
30.057432	1253.547677	16.750810
29.594690	1235.130994	16.755827
29.518781	1241.594536	16.760845
29.923780	1227.679253	16.765863
29.961743	1231.683588	16.770880
30.092449	1229.637470	16.775898
30.087595	1228.896830	16.780915
30.086126	1217.941012	16.785933
29.982511	1228.236902	16.790951
30.066155	1228.514949	16.795968
30.024314	1222.779395	16.800986
30.002160	1222.502570	16.806003
30.221186	1231.280403	16.811021
30.244370	1223.661940	16.816039
30.005802	1216.542967	16.821056
30.121074	1213.085440	16.826074
30.134656	1216.837736	16.831091
30.305902	1208.998582	16.836109
30.143665	1202.893029	16.841127
29.946710	1197.254563	16.846144
30.146825	1185.094373	16.851162
29.952536	1197.987710	16.856179
30.166426	1222.177064	16.861197
30.134578	1216.242647	16.866215
30.390501	1230.469670	16.871232
30.487529	1219.368853	16.876250
30.190596	1225.339070	16.881267
30.146433	1225.665989	16.886285
30.259776	1227.038571	16.891303
30.254433	1219.409670	16.896320
30.363465	1218.414616	16.901338
30.192815	1228.552121	16.906355
30.252127	1220.555107	16.911373
30.181031	1233.077971	16.916391
30.010603	1232.707752	16.921408
30.347372	1235.068459	16.926426
30.218258	1249.347514	16.931443
30.358784	1250.861058	16.936461
30.289191	1258.563734	16.941479
30.392082	1255.746733	16.946496
30.654658	1253.535928	16.951514
30.762946	1260.026707	16.956531
30.751624	1259.232025	16.961549
30.731568	1245.920353	16.966567
30.721013	1258.586753	16.971584
30.774793	1255.473975	16.976602
30.977320	1256.827492	16.981619
30.733141	1248.351757	16.986637
30.983679	1249.123605	16.991655
30.880887	1273.748781	16.996672
31.533733	1274.688563	17.001690
31.191080	1253.923218	17.006707
31.184321	1250.029026	17.011725
30.988917	1232.502282	17.016743
30.696514	1245.594522	17.021760
31.512448	1257.563599	17.026778
31.468400	1266.615403	17.031795
31.457744	1263.223157	17.036813
31.769481	1242.478212	17.041831
31.348458	1242.543047	17.046848
31.589294	1226.225331	17.051866
31.395660	1236.852591	17.056883
31.363407	1234.392128	17.061901
31.607017	1230.085363	17.066919
31.061345	1240.671995	17.071936
31.605328	1237.118228	17.076954
31.587587	1243.186782	17.081971
31.279305	1243.778575	17.086989
31.500035	1241.712855	17.092007
31.692137	1260.769623	17.097024
31.617491	1269.451344	17.102042
31.517810	1270.288940	17.107059
31.908244	1270.500152	17.112077
31.986104	1264.919382	17.117095
31.904896	1267.966594	17.122112
31.876349	1253.533451	17.127130
31.681246	1249.218087	17.132147
31.752108	1257.419917	17.137165
32.065661	1258.403367	17.142183
31.926107	1260.524333	17.147200
32.031036	1268.289500	17.152218
32.124711	1256.549540	17.157235
31.849489	1254.096750	17.162253
31.923625	1259.563009	17.167271
31.715754	1264.103967	17.172288
32.285982	1257.981470	17.177306
32.066029	1264.613685	17.182323
31.981603	1259.185307	17.187341
32.197241	1256.570508	17.192359
32.088310	1267.607548	17.197376
32.399334	1265.747344	17.202394
32.154453	1253.246327	17.207411
32.079419	1251.389497	17.212429
31.986128	1256.532687	17.217447
32.055244	1261.974584	17.222464
32.311947	1270.892058	17.227482
32.446172	1278.458323	17.232499
32.562418	1284.972597	17.237517
32.601650	1283.558034	17.242535
32.586015	1298.199430	17.247552
32.749581	1288.331286	17.252570
32.604309	1281.949119	17.257587
32.519499	1300.626955	17.262605
32.571892	1281.814110	17.267623
32.201981	1285.179073	17.272640
32.644297	1282.126278	17.277658
32.703539	1285.681113	17.282675
32.535640	1290.057622	17.287693
32.618383	1290.429900	17.292711
32.625250	1288.143450	17.297728
32.884319	1279.172390	17.302746
32.887309	1281.805749	17.307763
32.637011	1285.777431	17.312781
32.784165	1296.643255	17.317799
32.599377	1314.210626	17.322816
33.099538	1311.255929	17.327834
33.088111	1308.712496	17.332851
33.265129	1300.398592	17.337869
33.147434	1305.638534	17.342887
33.120651	1315.234679	17.347904
33.563022	1308.606004	17.352922
33.479787	1307.729910	17.357939
33.379678	1307.941684	17.362957
33.213964	1298.515294	17.367975
33.420680	1312.282285	17.372992
33.745711	1307.641419	17.378010
33.797380	1303.914501	17.383027
33.663553	1306.894246	17.388045
33.874336	1302.418304	17.393063
33.737181	1303.128453	17.398080
33.583725	1272.267519	17.403098
33.510576	1273.276690	17.408115
33.456624	1284.935471	17.413133
33.763771	1281.642452	17.418151
33.478161	1300.649294	17.423168
33.649470	1306.071170	17.428186
33.336960	1302.254258	17.433203
33.504358	1304.066472	17.438221
33.715793	1306.232775	17.443239
33.749701	1305.256232	17.448256
33.602438	1306.339651	17.453274
33.731120	1308.317886	17.458291
33.617415	1319.592726	17.463309
34.119479	1318.528388	17.468327
34.387623	1333.640959	17.473344
33.742245	1312.808450	17.478362
33.943604	1308.624573	17.483379
34.097708	1324.221464	17.488397
34.057249	1335.782398	17.493415
34.448054	1329.401769	17.498432
34.387040	1325.692482	17.503450
34.582610	1331.553405	17.508467
34.419623	1323.397234	17.513485
34.501969	1318.014494	17.518503
34.450368	1316.256919	17.523520
34.313764	1294.196035	17.528538
34.545823	1301.674895	17.533555
34.431557	1323.334757	17.538573
34.688248	1322.422762	17.543591
34.252164	1318.908313	17.548608
34.393963	1316.909950	17.553626
34.502453	1315.149538	17.558643
34.535661	1322.546127	17.563661
34.562758	1318.219612	17.568679
34.408386	1329.437016	17.573696
34.555105	1332.063559	17.578714
34.605881	1321.106907	17.583731
34.513017	1334.818714	17.588749
34.706122	1325.656982	17.593767
34.759943	1324.710804	17.598784
34.783760	1327.260622	17.603802
34.708511	1324.457300	17.608819
34.690773	1336.244368	17.613837
34.943882	1351.567286	17.618855
35.161157	1354.743709	17.623872
35.653450	1367.854392	17.628890
35.912633	1341.232799	17.633907
35.662755	1328.664642	17.638925
35.826211	1323.735949	17.643943
35.549546	1326.640891	17.648960
35.650942	1327.363975	17.653978
35.574079	1315.242367	17.658995
35.205494	1301.647541	17.664013
35.307577	1290.839496	17.669031
35.430623	1289.596882	17.674048
35.645888	1311.396536	17.679066
35.490211	1289.937740	17.684083
35.464581	1290.158069	17.689101
35.534800	1276.127814	17.694119
35.248951	1295.809788	17.699136
35.456160	1298.978022	17.704154
35.699141	1295.632818	17.709171
35.440992	1310.538875	17.714189
35.440288	1311.776397	17.719207
35.409713	1313.447336	17.724224
35.557825	1317.461243	17.729242
35.895290	1304.479951	17.734259
35.482338	1311.690655	17.739277
35.656713	1303.888135	17.744295
35.385808	1318.411718	17.749312
35.817001	1335.721636	17.754330
35.799718	1342.687074	17.759347
36.069350	1349.508462	17.764365
36.187326	1345.775497	17.769383
36.146913	1345.186377	17.774400
35.623397	1346.977750	17.779418
36.131677	1346.676842	17.784435
36.290633	1344.752401	17.789453
36.627836	1348.382560	17.794471
36.132777	1344.250970	17.799488
35.871692	1350.570576	17.804506
36.413358	1337.834015	17.809523
36.038137	1341.283321	17.814541
36.443580	1343.567351	17.819559
36.381638	1342.853264	17.824576
36.174052	1352.994002	17.829594
36.399418	1351.860245	17.834611
36.352820	1373.358229	17.839629
36.740859	1367.996403	17.844647
36.767994	1367.428399	17.849664
36.607514	1379.632341	17.854682
37.198398	1363.221206	17.859699
37.051528	1367.201207	17.864717
36.959751	1357.328370	17.869735
36.530507	1344.078523	17.874752
36.895407	1341.031621	17.879770
37.063484	1350.085424	17.884787
36.601390	1358.314561	17.889805
36.893718	1353.321459	17.894823
37.289233	1354.438004	17.899840
37.013611	1359.890847	17.904858
36.946590	1365.918585	17.909875
37.048037	1357.346899	17.914893
37.176157	1370.354205	17.919911
37.230748	1366.016834	17.924928
36.992368	1364.000789	17.929946
37.420317	1349.036869	17.934963
36.959107	1354.016709	17.939981
37.031391	1362.927709	17.944999
37.322608	1356.758577	17.950016
37.203545	1359.616814	17.955034
37.214150	1344.037709	17.960051
37.517023	1359.628554	17.965069
37.387246	1353.923031	17.970087
37.682691	1347.072787	17.975104
36.930088	1357.703142	17.980122
37.447537	1350.828414	17.985139
37.343963	1358.830219	17.990157
37.540668	1368.380412	17.995175
37.698058	1377.096477	18.000192
37.339306	1382.928763	18.005210
37.716359	1384.678786	18.010227
37.932953	1386.349041	18.015245
37.714494	1388.163619	18.020263
37.925610	1385.736331	18.025280
37.884149	1385.780366	18.030298
38.049735	1390.343887	18.035315
38.123368	1389.263544	18.040333
37.768469	1381.627177	18.045351
38.110046	1377.045359	18.050368
38.179751	1379.374051	18.055386
38.146717	1376.187220	18.060403
37.891711	1378.060192	18.065421
37.909742	1383.336779	18.070439
38.298341	1391.120083	18.075456
38.378451	1395.487327	18.080474
38.640905	1394.434434	18.085491
38.264532	1402.802361	18.090509
38.432960	1405.921915	18.095527
38.731491	1399.801156	18.100544
38.543572	1402.075193	18.105562
38.514568	1390.556360	18.110579
38.525646	1394.606316	18.115597
38.517925	1402.661389	18.120615
38.648049	1389.744796	18.125632
38.455707	1396.811618	18.130650
39.013566	1397.386253	18.135667
38.772821	1400.219927	18.140685
38.869233	1394.511258	18.145703
38.942835	1390.617135	18.150720
38.663051	1399.511150	18.155738
38.576258	1383.356842	18.160755
38.448416	1391.250091	18.165773
38.440373	1399.792944	18.170791
38.946468	1405.040256	18.175808
39.010511	1420.399014	18.180826
39.307646	1418.302537	18.185843
39.382660	1426.577187	18.190861
39.241369	1415.106611	18.195879
39.361217	1402.818785	18.200896
39.150374	1397.224266	18.205914
39.318544	1406.458377	18.210931
39.725933	1412.165447	18.215949
39.145071	1403.228009	18.220967
39.669137	1400.324849	18.225984
39.498735	1405.303690	18.231002
39.623711	1391.923443	18.236019
39.590305	1388.981716	18.241037
39.034431	1387.645999	18.246055
39.426574	1398.011830	18.251072
39.424955	1417.802874	18.256090
39.711987	1413.212739	18.261107
40.029073	1420.628401	18.266125
39.576383	1417.138717	18.271143
39.693371	1411.092042	18.276160
40.024507	1425.832730	18.281178
39.692083	1424.194570	18.286195
39.829841	1420.695491	18.291213
39.803736	1422.904410	18.296231
39.866286	1408.734375	18.301248
39.605498	1430.490442	18.306266
39.790883	1418.729889	18.311283
39.992707	1424.025324	18.316301
40.010826	1445.383795	18.321319
40.167410	1448.967458	18.326336
40.532562	1439.510728	18.331354
40.565934	1439.029867	18.336371
40.602417	1437.332515	18.341389
40.477409	1418.993049	18.346407
40.445263	1403.333754	18.351424
40.324499	1404.949932	18.356442
40.507798	1401.120541	18.361459
40.318799	1406.616755	18.366477
40.214662	1419.919928	18.371495
40.786073	1419.360589	18.376512
40.649235	1423.397010	18.381530
40.790736	1431.076109	18.386547
41.157530	1422.313315	18.391565
40.894050	1430.341778	18.396583
41.217760	1420.731299	18.401600
40.654806	1411.040607	18.406618
40.719449	1409.912935	18.411635
40.917547	1420.219717	18.416653
40.808354	1425.922996	18.421671
40.761616	1433.008090	18.426688
40.737228	1434.205841	18.431706
40.993013	1419.420085	18.436723
41.155307	1428.659707	18.441741
40.758578	1436.704091	18.446759
40.944304	1422.202708	18.451776
40.837848	1436.157174	18.456794
40.961485	1453.418260	18.461811
41.445184	1450.965402	18.466829
41.158109	1466.448951	18.471847
41.355740	1468.562645	18.476864
41.474830	1459.333547	18.481882
41.328411	1463.260355	18.486899
41.443031	1466.843280	18.491917
41.122712	1461.165465	18.496935
41.656930	1461.012218	18.501952
41.507728	1465.657697	18.506970
41.628967	1460.484594	18.511987
41.699761	1461.800851	18.517005
41.597177	1456.535619	18.522023
41.920111	1478.305712	18.527040
41.993800	1486.681190	18.532058
41.892579	1473.627779	18.537075
42.020981	1491.301254	18.542093
41.759309	1486.733079	18.547111
42.218672	1489.046405	18.552128
41.997711	1492.418094	18.557146
42.068818	1488.173814	18.562163
42.336026	1481.516932	18.567181
42.394776	1478.828231	18.572199
42.777130	1470.339377	18.577216
42.409723	1458.747690	18.582234
42.200482	1441.182054	18.587251
42.449919	1444.602754	18.592269
41.909810	1439.712937	18.597287
42.508693	1457.307643	18.602304
42.475491	1467.091139	18.607322
42.760364	1469.594693	18.612339
42.715118	1471.239338	18.617357
42.498468	1469.350379	18.622375
42.849524	1468.542254	18.627392
42.615681	1460.591984	18.632410
42.397129	1464.447063	18.637427
42.822890	1467.761672	18.642445
42.586891	1476.431202	18.647463
42.695229	1466.643714	18.652480
42.855137	1473.142587	18.657498
42.675855	1479.490455	18.662515
42.923208	1478.437296	18.667533
42.526958	1485.114682	18.672551
42.866428	1472.613562	18.677568
42.513167	1487.276486	18.682586
42.621816	1506.583934	18.687603
43.286918	1490.615459	18.692621
43.062858	1515.529924	18.697639
43.271845	1509.026136	18.702656
43.336403	1518.202643	18.707674
43.210693	1518.408219	18.712691
43.473070	1509.218003	18.717709
43.285543	1506.756978	18.722727
42.989702	1499.275141	18.727744
43.161572	1513.718653	18.732762
43.538064	1532.235513	18.737779
43.645150	1533.883925	18.742797
43.599738	1542.773146	18.747815
43.701188	1526.254749	18.752832
44.016272	1524.954205	18.757850
43.677905	1527.855799	18.762867
43.752443	1522.865960	18.767885
43.775607	1523.864742	18.772903
44.069760	1525.347022	18.777920
44.209841	1538.997489	18.782938
44.117483	1518.872422	18.787955
44.108775	1526.831476	18.792973
43.716573	1525.463582	18.797991
43.885961	1529.681286	18.803008
44.101550	1523.030751	18.808026
43.940068	1529.748090	18.813043
44.278887	1508.698154	18.818061
44.028486	1520.111070	18.823079
44.529987	1516.450890	18.828096
44.535704	1507.004899	18.833114
44.417894	1524.807473	18.838131
44.339433	1512.238394	18.843149
44.218853	1530.739373	18.848167
44.710237	1537.957611	18.853184
44.805476	1540.390361	18.858202
44.634363	1547.390956	18.863219
45.073547	1539.596323	18.868237
44.849067	1538.757334	18.873255
44.715462	1546.472307	18.878272
45.166133	1538.442342	18.883290
44.867778	1550.658968	18.888307
44.740882	1538.672208	18.893325
45.070272	1546.854500	18.898343
45.061185	1539.174686	18.903360
45.253704	1543.954641	18.908378
45.216927	1543.893388	18.913395
45.275644	1541.891405	18.918413
44.746854	1542.093126	18.923431
45.111834	1544.357303	18.928448
45.121943	1542.563326	18.933466
44.861266	1538.705509	18.938483
45.063365	1534.693081	18.943501
45.004714	1535.346178	18.948519
45.050082	1538.310330	18.953536
45.197410	1548.612204	18.958554
45.306898	1564.108655	18.963571
45.558236	1554.163444	18.968589
45.422665	1568.672180	18.973607
45.706257	1568.673917	18.978624
45.731534	1564.882802	18.983642
45.447642	1573.306788	18.988659
45.527411	1561.345497	18.993677
45.661783	1571.566664	18.998695
45.548361	1576.678252	19.003712
45.920312	1587.459307	19.008730
45.763834	1606.304259	19.013747
46.245236	1580.963673	19.018765
46.244461	1590.575375	19.023783
46.504258	1586.254814	19.028800
46.553297	1587.472919	19.033818
46.529628	1586.625936	19.038835
46.861159	1568.362011	19.043853
46.458997	1559.501040	19.048871
46.386696	1556.355696	19.053888
46.386486	1548.259700	19.058906
46.406263	1557.888456	19.063923
46.463691	1554.342983	19.068941
46.235245	1549.654548	19.073959
46.602320	1559.559139	19.078976
46.730803	1572.028435	19.083994
46.716830	1588.601479	19.089011
46.814721	1572.391850	19.094029
46.863347	1577.096590	19.099047
46.549334	1568.843017	19.104064
46.856581	1572.746650	19.109082
46.906517	1578.964763	19.114099
46.764869	1575.972983	19.119117
46.998545	1577.532379	19.124135
47.087138	1572.866931	19.129152
47.222011	1562.302852	19.134170
46.682191	1576.344606	19.139187
46.963199	1570.091654	19.144205
46.821770	1571.536483	19.149223
47.027288	1582.694403	19.154240
47.554711	1586.825009	19.159258
47.677781	1599.867394	19.164275
47.583230	1594.188043	19.169293
47.585671	1584.620514	19.174311
47.569986	1592.023147	19.179328
47.307223	1594.817784	19.184346
47.111340	1597.697026	19.189363
47.261297	1604.654826	19.194381
47.523328	1593.773489	19.199399
47.306336	1587.624277	19.204416
47.897837	1597.677217	19.209434
47.462882	1599.711430	19.214451
47.631732	1603.478710	19.219469
47.680764	1620.921976	19.224487
48.081272	1622.778965	19.229504
48.580451	1624.243908	19.234522
48.299145	1617.297931	19.239539
48.339597	1618.808760	19.244557
48.255741	1615.683224	19.249575
47.928404	1625.387293	19.254592
48.201545	1620.246705	19.259610
48.318463	1622.264125	19.264627
48.418262	1624.466242	19.269645
48.267776	1622.146697	19.274663
48.302509	1625.010864	19.279680
48.431537	1626.482847	19.284698
48.406308	1620.368658	19.289715
48.595303	1622.546981	19.294733
48.636143	1622.835259	19.299751
48.495391	1632.155196	19.304768
48.709943	1621.680652	19.309786
48.458280	1620.052547	19.314803
48.618977	1625.045634	19.319821
48.761458	1640.471561	19.324839
49.035032	1666.153342	19.329856
49.480225	1643.548231	19.334874
49.178545	1648.393744	19.339891
49.167327	1636.628707	19.344909
49.150638	1631.246871	19.349927
49.087555	1649.104120	19.354944
49.315226	1640.691122	19.359962
49.160043	1647.711962	19.364979
49.367745	1643.166164	19.369997
49.320388	1642.601996	19.375015
49.372422	1637.375120	19.380032
49.591025	1636.024573	19.385050
49.431893	1636.311058	19.390067
49.469672	1642.191089	19.395085
49.716438	1634.414428	19.400103
49.375629	1639.091426	19.405120
49.302422	1632.546631	19.410138
49.365233	1640.558878	19.415155
49.400603	1648.181420	19.420173
49.575449	1663.850811	19.425191
49.243465	1666.602378	19.430208
49.552775	1669.296392	19.435226
50.140583	1669.697607	19.440243
50.203544	1673.031471	19.445261
50.268940	1672.358720	19.450279
49.955551	1671.415531	19.455296
50.004308	1667.974012	19.460314
50.351876	1677.880328	19.465331
50.621000	1691.868423	19.470349
50.860234	1683.425344	19.475367
50.643762	1669.803873	19.480384
50.569069	1668.053616	19.485402
50.553905	1677.845879	19.490419
50.901618	1659.556143	19.495437
50.683982	1662.960386	19.500455
50.301858	1666.327842	19.505472
50.664887	1655.987972	19.510490
50.546140	1672.024550	19.515507
50.377793	1692.313719	19.520525
50.868680	1684.415402	19.525543
50.782403	1696.718934	19.530560
51.176570	1693.251823	19.535578
51.263628	1693.460426	19.540595
51.074896	1694.399954	19.545613
50.999321	1688.580244	19.550631
50.657272	1693.224199	19.555648
50.705295	1685.491180	19.560666
50.566686	1693.152729	19.565683
50.657408	1711.653256	19.570701
51.087926	1704.613822	19.575719
51.160235	1715.722600	19.580736
51.306039	1720.394398	19.585754
51.398236	1727.440135	19.590771
51.567772	1730.173988	19.595789
52.198239	1741.938889	19.600807
52.012942	1730.995564	19.605824
51.729206	1712.777831	19.610842
51.811382	1715.296814	19.615859
51.980427	1701.923777	19.620877
52.146040	1706.151995	19.625895
51.994176	1704.643396	19.630912
52.032954	1707.739560	19.635930
51.970678	1706.250405	19.640947
51.684491	1714.001895	19.645965
52.282558	1713.176953	19.650983
51.880183	1707.480325	19.656000
51.869841	1719.187340	19.661018
51.800796	1727.319835	19.666035
51.851967	1728.806465	19.671053
51.979556	1727.058401	19.676071
51.992756	1730.756955	19.681088
52.474141	1739.171093	19.686106
52.813330	1755.422405	19.691123
52.623197	1755.938989	19.696141
53.031870	1755.615761	19.701159
53.062436	1747.945825	19.706176
53.157604	1726.010962	19.711194
53.378920	1726.916784	19.716211
53.143753	1722.540001	19.721229
53.203064	1711.058493	19.726247
52.831239	1716.298251	19.731264
53.023378	1711.812478	19.736282
53.129452	1711.505794	19.741299
53.228934	1726.593481	19.746317
53.190350	1717.185584	19.751335
52.956801	1722.120440	19.756352
53.268738	1715.758197	19.761370
53.061522	1716.087467	19.766387
53.096288	1724.308502	19.771405
53.518034	1730.886447	19.776423
53.088392	1732.797766	19.781440
53.513467	1752.136885	19.786458
53.906853	1753.995658	19.791475
53.388308	1746.898493	19.796493
53.984514	1749.538027	19.801511
53.441345	1753.360214	19.806528
53.490152	1746.665695	19.811546
53.768924	1750.176094	19.816563
53.746481	1751.285565	19.821581
53.548001	1751.094751	19.826599
53.696440	1756.227883	19.831616
53.984037	1765.762715	19.836634
53.884381	1770.356600	19.841651
54.290193	1767.697692	19.846669
54.590969	1777.613184	19.851687
54.506838	1764.089825	19.856704
54.578922	1754.240241	19.861722
54.745985	1771.217965	19.866739
54.450552	1768.807205	19.871757
54.643824	1755.931241	19.876775
54.613373	1763.451345	19.881792
55.076128	1764.812492	19.886810
55.396968	1751.642845	19.891827
54.556783	1746.055553	19.896845
55.330991	1751.162433	19.901863
55.103062	1738.357858	19.906880
54.989011	1729.151378	19.911898
55.030249	1713.578055	19.916915
54.721729	1724.001629	19.921933
54.856120	1728.484000	19.926951
55.169079	1741.562246	19.931968
54.824646	1747.579681	19.936986
55.176891	1740.242177	19.942003
55.334695	1756.306560	19.947021
55.311992	1749.223902	19.952039
55.307139	1747.527442	19.957056
55.045066	1757.841407	19.962074
55.317840	1744.054584	19.967091
55.087315	1757.122664	19.972109
55.176208	1751.373181	19.977127
55.188332	1763.696919	19.982144
55.425230	1772.792349	19.987162
55.725114	1776.749215	19.992179
55.671001	1788.961885	19.997197
55.636623	1765.868584	20.002215
55.666081	1786.901283	20.007232
55.751070	1781.980885	20.012250
55.877733	1774.963877	20.017267
55.705831	1786.324652	20.022285
55.920956	1801.065583	20.027303
56.021712	1805.959395	20.032320
56.061626	1793.981283	20.037338
56.651852	1806.968103	20.042355
56.119657	1803.687901	20.047373
56.429478	1811.669064	20.052391
56.851349	1806.307993	20.057408
56.331834	1802.891261	20.062426
56.673652	1791.960187	20.067443
56.411456	1799.914819	20.072461
56.640509	1804.047355	20.077479
56.312889	1808.750173	20.082496
56.364202	1817.019109	20.087514
56.764161	1827.688434	20.092531
56.774138	1827.049044	20.097549
56.949633	1824.260488	20.102567
56.913990	1835.512374	20.107584
56.861545	1824.213602	20.112602
57.198498	1824.471256	20.117619
57.081149	1829.162954	20.122637
57.089269	1829.112389	20.127655
57.041694	1829.192667	20.132672
57.331063	1837.004211	20.137690
57.837583	1844.241745	20.142707
57.563387	1849.071953	20.147725
57.841868	1847.946902	20.152743
58.198411	1839.193834	20.157760
57.769207	1826.432878	20.162778
57.968709	1830.510861	20.167795
57.833990	1824.637690	20.172813
57.577942	1824.228067	20.177831
57.708967	1821.731474	20.182848
57.835285	1839.720424	20.187866
58.210708	1838.289228	20.192883
58.143769	1836.231208	20.197901
58.505602	1841.719418	20.202919
58.388865	1832.128520	20.207936
58.147011	1847.728587	20.212954
58.354702	1837.811466	20.217971
58.043579	1838.815908	20.222989
58.148008	1832.740635	20.228007
58.227308	1833.898253	20.233024
58.264856	1835.044465	20.238042
58.375005	1818.712092	20.243059
58.444688	1826.493799	20.248077
58.845927	1842.861512	20.253095
58.984734	1849.242982	20.258112
58.941127	1850.940540	20.263130
59.273928	1834.603834	20.268147
59.178925	1835.322196	20.273165
59.213323	1826.298389	20.278183
59.202749	1823.413232	20.283200
59.071435	1823.189273	20.288218
59.308911	1816.473585	20.293235
59.407192	1821.939205	20.298253
59.340687	1818.587753	20.303271
59.358368	1816.451389	20.308288
59.057626	1823.027123	20.313306
59.509219	1820.971204	20.318323
59.077976	1828.144819	20.323341
59.820307	1838.658965	20.328359
59.552990	1850.866763	20.333376
59.279629	1840.437268	20.338394
59.526523	1850.611093	20.343411
59.665275	1851.354404	20.348429
59.564052	1853.548045	20.353447
59.966660	1846.225985	20.358464
59.791890	1853.339910	20.363482
59.702935	1854.433217	20.368499
59.882484	1871.896338	20.373517
60.212917	1879.181685	20.378535
60.119392	1873.844150	20.383552
60.194369	1889.501931	20.388570
60.354469	1887.151886	20.393587
60.320086	1884.094097	20.398605
60.369559	1884.341784	20.403623
60.426814	1881.384391	20.408640
60.226874	1885.301057	20.413658
60.324913	1877.145548	20.418675
60.412671	1883.611837	20.423693
60.739331	1905.518718	20.428711
60.923696	1899.789030	20.433728
60.697974	1903.023617	20.438746
61.137753	1903.611686	20.443763
61.070078	1902.985322	20.448781
60.779518	1899.534277	20.453799
61.064283	1901.296267	20.458816
61.192669	1896.762123	20.463834
61.169725	1899.265242	20.468851
60.949584	1904.218018	20.473869
60.940379	1899.893598	20.478887
61.544139	1911.480189	20.483904
61.299293	1916.980892	20.488922
62.107697	1903.390032	20.493939
61.995863	1921.658564	20.498957
61.721624	1915.415344	20.503975
62.014993	1909.548755	20.508992
61.819641	1914.142553	20.514010
61.963801	1921.637423	20.519027
62.277787	1930.001975	20.524045
62.093997	1917.075993	20.529063
62.136574	1909.331557	20.534080
61.927497	1917.232791	20.539098
62.064348	1917.359948	20.544115
62.386348	1904.998361	20.549133
62.025113	1910.059483	20.554151
62.297726	1908.298850	20.559168
62.378479	1912.027029	20.564186
62.230234	1904.702867	20.569203
62.341779	1903.111552	20.574221
62.424083	1914.028881	20.579239
62.695593	1910.124952	20.584256
62.559649	1912.142468	20.589274
62.793110	1927.732174	20.594291
62.931906	1941.766244	20.599309
62.840772	1944.569388	20.604327
62.690592	1935.406153	20.609344
62.878052	1944.385655	20.614362
63.096163	1939.357784	20.619379
63.351764	1934.122560	20.624397
62.934031	1939.571730	20.629415
63.603938	1932.661121	20.634432
63.193168	1933.918034	20.639450
63.153370	1935.884236	20.644467
63.160109	1935.700645	20.649485
63.172361	1937.975142	20.654503
63.336644	1949.959548	20.659520
63.216956	1957.234085	20.664538
63.409931	1950.862273	20.669555
63.626345	1962.396190	20.674573
63.869097	1957.552608	20.679591
63.725658	1953.437147	20.684608
63.654791	1957.963148	20.689626
63.937077	1957.766501	20.694643
64.133496	1972.888013	20.699661
64.327850	1980.644472	20.704679
64.447443	1979.580703	20.709696
64.530296	1981.400475	20.714714
64.344456	1983.023332	20.719731
64.365939	1984.665272	20.724749
64.467071	1988.360183	20.729767
64.865633	1979.874081	20.734784
64.631716	1977.711364	20.739802
64.728429	1984.286442	20.744819
64.942868	1981.645344	20.749837
64.690255	1969.018654	20.754855
65.006879	1973.710723	20.759872
64.878214	1978.369497	20.764890
65.116824	1971.219936	20.769907
65.065176	1978.739908	20.774925
64.655388	1979.774637	20.779943
65.243897	1978.241098	20.784960
64.859440	1984.139267	20.789978
64.857806	1970.250948	20.794995
65.002776	1985.108167	20.800013
64.970501	2008.743829	20.805031
65.323894	2008.601960	20.810048
65.213291	2007.196345	20.815066
65.576560	2001.312659	20.820083
65.570522	2007.452212	20.825101
65.583826	2030.071813	20.830119
65.577824	2035.521082	20.835136
65.938903	2042.494977	20.840154
65.972973	2034.605638	20.845171
65.742668	2030.465145	20.850189
65.741274	2035.609352	20.855207
66.011346	2025.625706	20.860224
65.941137	2039.964455	20.865242
66.111713	2052.909226	20.870259
66.317312	2045.858778	20.875277
66.512605	2064.598725	20.880295
66.481569	2062.508759	20.885312
66.519827	2059.402321	20.890330
66.596927	2058.494767	20.895347
66.579140	2054.773240	20.900365
66.564218	2052.750685	20.905383
66.699863	2057.892332	20.910400
66.480183	2064.678766	20.915418
66.421064	2081.292474	20.920435
67.271809	2089.438311	20.925453
67.494889	2087.699818	20.930471
67.998592	2070.000496	20.935488
67.972123	2061.944786	20.940506
67.922170	2051.313679	20.945523
67.791848	2038.130160	20.950541
67.475638	2052.219638	20.955559
67.976251	2043.017689	20.960576
68.028597	2044.957656	20.965594
67.779685	2042.932236	20.970611
68.004248	2038.312284	20.975629
67.862189	2041.003203	20.980647
67.952844	2030.686441	20.985664
67.883009	2031.103044	20.990682
67.644807	2032.882773	20.995699
67.786018	2039.766042	21.000717
67.604825	2034.977926	21.005735
67.916444	2032.001305	21.010752
67.449890	2037.636118	21.015770
67.760401	2046.511889	21.020787
67.934067	2068.133290	21.025805
67.834555	2060.732503	21.030823
67.891789	2061.944174	21.035840
68.263574	2068.921429	21.040858
68.576121	2088.069155	21.045875
68.690335	2081.168228	21.050893
68.555550	2092.869322	21.055911
68.806933	2072.734361	21.060928
68.814249	2084.078533	21.065946
68.671136	2079.778946	21.070963
68.777380	2072.236094	21.075981
68.934965	2091.197245	21.080999
69.035678	2102.844078	21.086016
69.226871	2101.409645	21.091034
69.087921	2104.794289	21.096051
69.431665	2098.934854	21.101069
69.143373	2105.380315	21.106087
69.679647	2102.885997	21.111104
69.389137	2098.382043	21.116122
69.368526	2110.066645	21.121139
69.678643	2112.867879	21.126157
69.565889	2129.980222	21.131175
70.098948	2130.134225	21.136192
70.054347	2133.969187	21.141210
70.009512	2133.708100	21.146227
70.413262	2135.822667	21.151245
70.131594	2136.998621	21.156263
70.208448	2131.696223	21.161280
70.158460	2128.112861	21.166298
70.134880	2127.444558	21.171315
70.617360	2131.736665	21.176333
70.134353	2131.126959	21.181351
70.422968	2129.307363	21.186368
70.468895	2134.933109	21.191386
70.589412	2152.188606	21.196403
70.809442	2155.397023	21.201421
70.813287	2168.502699	21.206439
70.983374	2166.298784	21.211456
70.856134	2155.117236	21.216474
70.626575	2161.601435	21.221491
70.879650	2150.672767	21.226509
70.823869	2160.636206	21.231527
71.298331	2167.858918	21.236544
71.371154	2169.937631	21.241562
71.136316	2171.063530	21.246579
71.471140	2170.459022	21.251597
71.570690	2176.876443	21.256615
71.412583	2176.850196	21.261632
71.975341	2178.756423	21.266650
71.642828	2174.608962	21.271667
71.908740	2165.218973	21.276685
71.423405	2175.762414	21.281703
71.746460	2176.772308	21.286720
71.950774	2187.578929	21.291738
71.897696	2207.754854	21.296755
72.177889	2203.436854	21.301773
72.215301	2211.789788	21.306791
72.175205	2207.526681	21.311808
72.239971	2197.646333	21.316826
72.001959	2209.939326	21.321843
72.255497	2206.579980	21.326861
72.431845	2224.781960	21.331879
72.714045	2239.364406	21.336896
72.897401	2227.870480	21.341914
72.880560	2230.981452	21.346931
73.259372	2227.010505	21.351949
72.819050	2227.536755	21.356967
73.108746	2223.130966	21.361984
73.302829	2224.321611	21.367002
73.153200	2232.751719	21.372019
73.190822	2232.201437	21.377037
73.255344	2222.372487	21.382055
73.272893	2227.751403	21.387072
73.602581	2226.668844	21.392090
73.294921	2220.791818	21.397107
73.523350	2222.726725	21.402125
73.309545	2232.681484	21.407143
73.737156	2251.123054	21.412160
74.179853	2249.251805	21.417178
73.871832	2242.966596	21.422195
73.756834	2243.759731	21.427213
73.593111	2254.782911	21.432231
73.765715	2256.402270	21.437248
73.930630	2245.185175	21.442266
73.875446	2270.459731	21.447283
74.010650	2275.007477	21.452301
74.470475	2278.030047	21.457319
74.357724	2274.146417	21.462336
74.561037	2275.980174	21.467354
74.628262	2281.453648	21.472371
74.745368	2279.080729	21.477389
74.826407	2279.842850	21.482407
74.901025	2276.976797	21.487424
75.684565	2268.726898	21.492442
75.174523	2270.897609	21.497459
75.505252	2260.929574	21.502477
75.689169	2259.718948	21.507495
75.315059	2266.437690	21.512512
75.720094	2246.275145	21.517530
75.380738	2262.977479	21.522547
75.413357	2265.556311	21.527565
75.506390	2254.188108	21.532583
75.528557	2258.293345	21.537600
75.668922	2263.926169	21.542618
75.789204	2282.181179	21.547635
75.816879	2293.841014	21.552653
75.982304	2292.666509	21.557671
76.045428	2293.226096	21.562688
76.486150	2286.725025	21.567706
76.079536	2281.954398	21.572723
76.347472	2282.228388	21.577741
76.538993	2284.761086	21.582759
76.339670	2286.441316	21.587776
76.569309	2275.419590	21.592794
76.315292	2276.339430	21.597811
76.400147	2276.724376	21.602829
76.483635	2286.813494	21.607847
76.474329	2298.222180	21.612864
76.746448	2309.648538	21.617882
76.762173	2312.703361	21.622899
76.581260	2308.111752	21.627917
77.226545	2310.610020	21.632935
76.996892	2314.679134	21.637952
77.200939	2311.906638	21.642970
76.903619	2312.931266	21.647987
76.866651	2321.733524	21.653005
76.915568	2340.957999	21.658023
77.164557	2344.182732	21.663040
77.595846	2331.946434	21.668058
77.301980	2345.860255	21.673075
77.761609	2344.424353	21.678093
77.662236	2355.247222	21.683111
77.920917	2357.462361	21.688128
78.156943	2359.662939	21.693146
78.349478	2367.021892	21.698163
78.589208	2369.015575	21.703181
78.473074	2361.986654	21.708199
78.561871	2352.903357	21.713216
78.687711	2344.296387	21.718234
78.180350	2337.941331	21.723251
78.287409	2348.886568	21.728269
78.321909	2356.565506	21.733287
78.252442	2361.505929	21.738304
78.536756	2346.826572	21.743322
78.533487	2359.263164	21.748339
78.770859	2368.965517	21.753357
78.943993	2372.968285	21.758375
78.752772	2383.037313	21.763392
78.953084	2375.435465	21.768410
79.034886	2383.947089	21.773427
79.312103	2391.787891	21.778445
79.467682	2388.683652	21.783463
79.466201	2384.739288	21.788480
79.254556	2384.731729	21.793498
79.793640	2399.971828	21.798515
79.849532	2421.349228	21.803533
80.171307	2412.240192	21.808551
79.991406	2420.101036	21.813568
79.974841	2409.437198	21.818586
79.902634	2410.896451	21.823603
80.125067	2406.983777	21.828621
80.307166	2407.900256	21.833639
79.829979	2409.876986	21.838656
80.037067	2412.360483	21.843674
80.280078	2409.387451	21.848691
80.338900	2414.560020	21.853709
80.281919	2425.384003	21.858727
80.215661	2436.270940	21.863744
80.826898	2429.958941	21.868762
80.309062	2446.459485	21.873779
80.505570	2434.448308	21.878797
81.205308	2440.642065	21.883815
81.454582	2441.855101	21.888832
81.960749	2431.933552	21.893850
81.803121	2424.488064	21.898867
81.708596	2414.286876	21.903885
81.957250	2402.131880	21.908903
81.737266	2411.574230	21.913920
82.206163	2396.433057	21.918938
81.687743	2413.493465	21.923955
81.726648	2414.183623	21.928973
81.978801	2401.814482	21.933991
81.642867	2407.590036	21.939008
82.320713	2410.708093	21.944026
82.064184	2416.373095	21.949043
81.927659	2406.527647	21.954061
82.340696	2394.298647	21.959079
82.016941	2401.335086	21.964096
82.186925	2421.246298	21.969114
82.400269	2435.881054	21.974131
82.121912	2441.229222	21.979149
82.283313	2443.936597	21.984167
82.242782	2445.416011	21.989184
82.536516	2439.370041	21.994202
82.776994	2462.818622	21.999219
82.710530	2469.882651	22.004237
82.836455	2459.562924	22.009255
82.692500	2476.555224	22.014272
82.891909	2463.013924	22.019290
83.477298	2469.169309	22.024307
83.428172	2455.687390	22.029325
83.295797	2462.128689	22.034343
83.248758	2467.427619	22.039360
83.642338	2485.319424	22.044378
83.804972	2496.018787	22.049395
83.649288	2491.666835	22.054413
83.959253	2496.330444	22.059431
84.070733	2492.314437	22.064448
84.211413	2486.034112	22.069466
83.876601	2475.792870	22.074483
84.033118	2494.488177	22.079501
84.577982	2488.909909	22.084519
83.989623	2498.401963	22.089536
84.197258	2489.253676	22.094554
84.299591	2497.509625	22.099571
84.210797	2516.464574	22.104589
84.740913	2511.608964	22.109607
84.861456	2521.530312	22.114624
84.796193	2507.374877	22.119642
85.022534	2506.456021	22.124659
84.813996	2511.588162	22.129677
84.830569	2504.775224	22.134695
84.436622	2514.170009	22.139712
84.683080	2527.290424	22.144730
84.814611	2530.736954	22.149747
84.887538	2531.077227	22.154765
85.446940	2546.090113	22.159783
85.496284	2559.265369	22.164800
85.571166	2553.462396	22.169818
85.666719	2557.682153	22.174835
85.697363	2553.398206	22.179853
86.000064	2550.947534	22.184871
85.791682	2557.749245	22.189888
86.528655	2578.474196	22.194906
86.752833	2576.384505	22.199923
86.466411	2564.367600	22.204941
86.536937	2550.220591	22.209959
86.401611	2560.176568	22.214976
86.545292	2573.519307	22.219994
86.811215	2576.549964	22.225011
86.722594	2576.160680	22.230029
86.867473	2572.742837	22.235047
87.026468	2583.236379	22.240064
86.618143	2574.339815	22.245082
87.016939	2571.939792	22.250099
87.135760	2577.792617	22.255117
87.135604	2576.292324	22.260135
87.340907	2589.763863	22.265152
87.437839	2597.300132	22.270170
87.542147	2594.614930	22.275187
87.326235	2612.824316	22.280205
87.378762	2599.236109	22.285223
87.440146	2604.982301	22.290240
87.432896	2606.914470	22.295258
87.540122	2620.479009	22.300275
87.721223	2634.687221	22.305293
88.296004	2631.182187	22.310311
87.853891	2633.406677	22.315328
87.954477	2624.913758	22.320346
88.527404	2632.805617	22.325363
88.534924	2646.069349	22.330381
88.926407	2646.804992	22.335399
88.934594	2654.605546	22.340416
88.877867	2646.596458	22.345434
88.932760	2638.328392	22.350451
89.067921	2637.553329	22.355469
89.343029	2660.381759	22.360487
89.435322	2638.696061	22.365504
89.150709	2637.924618	22.370522
89.145242	2622.209088	22.375539
89.307409	2640.302886	22.380557
89.563950	2645.788511	22.385575
89.476991	2659.416272	22.390592
89.191204	2653.426023	22.395610
89.435486	2655.862274	22.400627
89.231243	2653.524093	22.405645
89.551710	2665.506278	22.410663
89.844931	2671.069311	22.415680
89.690973	2683.810970	22.420698
90.030283	2686.961012	22.425715
89.921832	2682.905515	22.430733
89.790172	2681.259628	22.435751
90.052107	2699.881468	22.440768
90.324565	2713.690031	22.445786
90.521912	2708.056911	22.450803
90.218515	2715.708206	22.455821
90.690897	2701.682441	22.460839
90.842163	2714.987437	22.465856
91.178579	2725.389163	22.470874
91.386332	2717.982758	22.475891
91.266109	2728.265070	22.480909
91.511287	2717.580208	22.485927
91.518099	2721.741055	22.490944
91.507567	2720.059796	22.495962
91.613732	2711.067114	22.500979
91.733009	2721.324806	22.505997
91.837479	2716.172361	22.511015
91.783728	2724.004837	22.516032
91.980121	2726.815923	22.521050
92.138353	2719.073230	22.526067
91.849218	2726.417858	22.531085
91.715737	2734.526099	22.536103
91.730491	2740.008406	22.541120
92.094615	2750.091019	22.546138
92.335321	2745.548698	22.551155
91.977963	2753.541981	22.556173
92.334237	2758.662365	22.561191
92.486846	2769.300389	22.566208
92.767015	2772.068114	22.571226
92.881922	2778.452345	22.576243
92.795651	2774.815973	22.581261
93.009733	2769.591069	22.586279
93.455613	2760.431206	22.591296
92.991612	2760.815721	22.596314
93.463568	2773.843772	22.601331
93.426112	2792.602986	22.606349
93.671295	2795.592234	22.611367
94.029598	2798.281308	22.616384
93.892889	2801.418304	22.621402
93.868590	2784.660494	22.626419
93.832506	2789.257955	22.631437
94.315204	2799.051335	22.636455
94.033375	2797.228291	22.641472
94.134705	2791.111424	22.646490
94.064578	2794.496459	22.651507
93.929308	2788.139569	22.656525
93.949459	2808.026237	22.661543
94.291612	2815.785860	22.666560
94.399307	2809.884853	22.671578
94.759133	2807.406200	22.676595
94.239243	2817.094012	22.681613
94.832600	2828.730458	22.686631
94.740273	2836.493384	22.691648
94.588741	2845.234166	22.696666
94.992880	2845.581524	22.701683
94.777919	2847.068540	22.706701
94.988896	2867.222951	22.711719
95.033259	2876.820319	22.716736
95.313226	2876.085093	22.721754
95.423135	2881.140720	22.726771
95.767610	2874.257296	22.731789
95.809427	2887.712017	22.736807
96.046741	2898.177084	22.741824
96.312450	2913.322714	22.746842
96.406361	2902.229273	22.751859
96.419489	2891.732237	22.756877
96.613047	2894.076912	22.761895
96.881929	2889.786576	22.766912
96.859536	2887.314377	22.771930
97.207414	2890.543751	22.776947
96.779476	2862.348698	22.781965
96.809773	2867.180478	22.786983
97.324343	2885.306878	22.792000
97.098489	2883.258835	22.797018
97.513090	2883.982404	22.802035
97.535343	2886.055791	22.807053
97.641605	2888.051912	22.812071
97.362342	2884.239539	22.817088
97.045724	2895.048882	22.822106
97.377270	2881.362356	22.827123
97.291553	2877.201087	22.832141
96.969070	2886.401617	22.837159
97.776985	2892.898932	22.842176
97.553535	2912.013815	22.847194
97.963251	2907.100620	22.852211
97.884200	2912.873674	22.857229
97.962114	2928.564504	22.862247
98.198700	2938.228175	22.867264
97.979072	2934.378377	22.872282
97.958170	2935.370360	22.877299
98.391028	2954.231576	22.882317
98.260420	2961.476500	22.887335
98.282790	2969.415415	22.892352
98.731849	2982.492700	22.897370
99.066999	2997.063571	22.902387
99.365940	2999.711311	22.907405
99.140760	3006.815196	22.912423
99.124934	2997.889749	22.917440
99.496224	2997.139427	22.922458
99.600088	3000.545755	22.927475
99.411551	3005.557828	22.932493
99.474911	3016.587135	22.937511
99.627828	3008.003471	22.942528
99.669504	3025.490091	22.947546
100.097624	3018.143190	22.952563
99.882781	3034.390753	22.957581
100.256144	3050.855301	22.962599
100.873405	3048.886811	22.967616
100.086282	3050.640431	22.972634
100.669790	3057.514258	22.977651
101.115703	3033.706645	22.982669
101.368819	3029.782250	22.987687
101.607878	3028.709694	22.992704
101.142213	3028.400023	22.997722
101.753566	3023.303084	23.002739
102.023991	3023.685535	23.007757
101.623054	3007.988899	23.012775
101.646362	2990.973008	23.017792
101.582999	3004.141284	23.022810
101.870522	2989.748575	23.027827
101.823238	2991.912204	23.032845
101.683005	2992.745962	23.037863
101.861223	2983.677439	23.042880
101.888360	3002.203801	23.047898
101.987208	3013.529594	23.052915
101.975576	3024.646099	23.057933
102.299292	3018.704988	23.062951
102.362215	3009.089378	23.067968
102.066944	3016.480430	23.072986
102.031949	3023.559196	23.078003
102.436717	3034.428955	23.083021
102.281726	3044.902255	23.088039
102.691873	3046.033248	23.093056
102.450925	3049.987493	23.098074
102.977767	3064.813360	23.103091
103.251378	3066.412572	23.108109
102.929205	3077.034381	23.113127
103.819032	3073.007128	23.118144
103.554324	3071.615067	23.123162
103.680988	3072.918098	23.128179
103.677117	3071.321918	23.133197
103.288119	3069.651978	23.138215
103.988403	3083.753949	23.143232
104.251870	3100.089863	23.148250
103.948191	3100.814417	23.153267
104.143721	3099.549842	23.158285
103.996257	3115.154090	23.163303
104.423280	3100.898066	23.168320
104.209020	3117.844026	23.173338
104.532783	3126.149744	23.178355
104.775661	3131.383870	23.183373
104.891637	3145.067500	23.188391
104.911031	3133.663380	23.193408
105.053463	3133.023309	23.198426
104.818359	3130.345281	23.203443
105.067561	3135.857097	23.208461
105.064163	3151.990712	23.213479
105.514866	3146.067544	23.218496
105.675030	3145.595798	23.223514
105.934583	3150.692927	23.228531
106.176062	3137.695058	23.233549
105.839226	3153.985738	23.238567
106.146748	3141.424187	23.243584
105.921959	3145.695463	23.248602
106.119900	3154.774331	23.253619
106.721651	3164.253398	23.258637
106.463101	3175.151368	23.263655
106.314928	3175.288826	23.268672
106.652619	3173.947212	23.273690
106.577679	3172.214343	23.278707
106.809483	3176.738520	23.283725
106.654826	3180.338783	23.288743
107.488102	3189.193007	23.293760
107.425320	3186.211697	23.298778
107.546013	3187.662178	23.303795
107.760002	3190.240920	23.308813
107.781126	3206.429200	23.313831
107.632479	3191.380833	23.318848
107.628878	3186.829935	23.323866
107.582492	3191.130011	23.328883
107.763646	3190.979198	23.333901
107.712963	3193.202076	23.338919
107.912379	3189.554619	23.343936
108.201080	3211.875331	23.348954
108.387560	3226.239101	23.353971
108.598422	3212.246642	23.358989
108.555754	3214.410326	23.364007
108.720519	3229.871366	23.369024
108.681518	3221.707873	23.374042
108.563583	3219.281722	23.379059
108.638146	3211.115217	23.384077
108.688279	3235.193852	23.389095
109.127213	3230.262737	23.394112
109.000328	3233.443864	23.399130
109.507481	3227.245595	23.404147
109.667721	3218.077153	23.409165
109.672294	3234.854406	23.414183
109.811162	3235.803079	23.419200
109.937590	3246.378436	23.424218
110.067518	3246.880170	23.429235
110.344494	3243.081305	23.434253
110.203470	3260.051932	23.439271
110.441050	3237.068183	23.444288
110.476066	3249.067283	23.449306
110.541458	3248.754892	23.454323
110.630598	3239.812354	23.459341
110.662230	3254.394253	23.464359
110.444183	3245.578848	23.469376
110.841558	3248.599336	23.474394
110.864682	3270.665990	23.479411
110.985586	3257.805265	23.484429
110.961263	3277.019188	23.489447
111.064770	3273.662358	23.494464
111.230405	3287.807586	23.499482
111.611118	3296.358312	23.504499
111.672047	3299.627708	23.509517
111.766570	3300.659696	23.514535
111.658544	3302.299161	23.519552
111.831143	3320.842812	23.524570
111.840252	3325.977051	23.529587
112.152714	3334.255222	23.534605
112.036169	3329.081614	23.539623
112.347473	3340.067820	23.544640
112.450465	3358.165936	23.549658
112.505467	3358.648953	23.554675
112.750552	3352.288429	23.559693
112.870570	3359.220081	23.564711
112.903127	3376.218058	23.569728
113.252491	3376.612278	23.574746
113.063877	3378.219003	23.579763
113.610073	3366.954435	23.584781
113.261377	3369.703741	23.589799
113.141257	3387.440337	23.594816
113.867850	3397.684346	23.599834
113.608460	3417.788459	23.604851
113.796770	3412.214452	23.609869
113.482820	3412.253321	23.614887
114.061594	3425.418603	23.619904
114.308782	3429.550551	23.624922
114.309451	3425.527615	23.629939
114.536122	3423.851572	23.634957
114.540141	3436.380344	23.639975
114.958114	3447.646636	23.644992
115.030153	3460.167337	23.650010
114.678827	3469.124552	23.655027
115.209429	3468.771507	23.660045
115.175517	3462.118852	23.665063
115.240420	3453.326653	23.670080
115.688950	3456.782035	23.675098
115.184254	3463.387434	23.680115
115.800682	3481.531563	23.685133
115.848469	3483.407111	23.690151
115.750959	3492.008620	23.695168
116.333026	3483.021894	23.700186
116.106119	3492.389271	23.705203
116.082888	3490.227744	23.710221
116.219276	3488.899289	23.715239
116.310007	3507.449211	23.720256
116.833638	3510.033535	23.725274
116.741604	3507.157784	23.730291
116.732700	3504.597038	23.735309
116.698419	3517.269999	23.740327
116.511606	3508.508731	23.745344
116.999945	3518.446521	23.750362
116.863556	3536.974164	23.755379
116.621167	3542.763418	23.760397
116.875312	3553.853709	23.765415
117.318638	3562.338725	23.770432
117.580173	3570.186460	23.775450
117.689707	3572.017169	23.780467
118.158591	3572.951490	23.785485
118.901424	3578.344891	23.790503
118.613513	3571.041637	23.795520
118.689627	3551.307343	23.800538
118.435885	3555.528396	23.805555
118.697330	3560.969838	23.810573
119.416350	3568.096308	23.815591
118.926597	3570.809902	23.820608
119.157279	3569.109953	23.825626
118.905225	3573.634276	23.830643
119.443216	3568.149284	23.835661
119.337683	3573.637195	23.840679
119.141698	3571.453808	23.845696
119.184181	3571.824333	23.850714
119.377337	3592.949961	23.855731
119.706031	3587.151513	23.860749
119.638138	3589.044613	23.865767
120.125363	3609.908680	23.870784
120.507719	3592.463902	23.875802
120.393377	3598.574146	23.880819
120.555212	3610.223434	23.885837
121.276608	3615.987715	23.890855
120.995193	3601.380182	23.895872
121.252670	3602.343925	23.900890
121.183490	3613.819576	23.905907
121.118331	3609.343293	23.910925
121.254761	3612.093190	23.915943
121.294416	3618.339415	23.920960
121.485731	3613.313268	23.925978
121.487099	3618.091007	23.930995
121.466485	3605.601807	23.936013
121.720495	3613.091750	23.941031
121.892569	3608.592804	23.946048
121.809491	3621.087691	23.951066
121.553059	3636.373851	23.956083
121.482698	3641.368963	23.961101
121.819723	3653.171226	23.966119
122.127760	3658.640437	23.971136
122.550438	3663.443850	23.976154
122.237169	3679.920557	23.981171
122.392496	3690.936329	23.986189
122.851580	3690.518326	23.991207
122.407144	3708.207300	23.996224
122.913393	3709.484280	24.001242
123.250086	3722.429972	24.006259
123.622602	3721.814458	24.011277
123.739833	3719.303701	24.016295
124.166132	3717.356056	24.021312
124.052960	3717.237731	24.026330
124.219131	3721.686692	24.031347
124.089135	3707.617431	24.036365
124.499173	3718.538772	24.041383
124.420394	3710.204427	24.046400
124.394724	3712.054344	24.051418
124.168401	3719.566620	24.056435
124.294828	3731.432876	24.061453
124.517518	3740.263508	24.066471
124.341489	3740.276830	24.071488
124.894781	3744.080326	24.076506
124.599872	3765.175416	24.081523
124.971755	3765.522619	24.086541
125.197164	3764.827867	24.091559
125.064772	3784.923279	24.096576
125.066868	3787.961157	24.101594
125.407224	3802.044125	24.106611
125.586692	3798.435651	24.111629
126.140136	3819.828045	24.116647
126.242326	3826.750647	24.121664
126.490959	3827.767443	24.126682
126.776219	3821.956794	24.131699
126.572035	3828.364262	24.136717
126.779759	3821.388450	24.141735
126.864278	3820.415395	24.146752
126.880577	3816.564974	24.151770
126.870418	3824.495135	24.156787
127.343305	3837.535351	24.161805
127.204409	3832.494011	24.166823
127.132593	3852.094451	24.171840
127.483915	3841.616877	24.176858
127.629447	3848.078380	24.181875
127.526294	3867.129676	24.186893
127.864531	3874.570395	24.191911
127.774374	3879.337353	24.196928
128.197681	3879.075655	24.201946
128.156545	3881.773836	24.206963
128.419120	3898.569019	24.211981
128.695079	3907.491734	24.216999
128.644364	3909.116673	24.222016
129.170457	3901.350012	24.227034
128.945400	3901.209226	24.232051
128.831010	3906.747932	24.237069
129.313427	3914.264455	24.242087
129.462661	3933.251293	24.247104
129.658932	3931.226668	24.252122
129.910859	3923.762785	24.257139
129.818344	3926.693485	24.262157
129.523017	3927.734025	24.267175
129.598176	3939.671906	24.272192
130.075031	3945.122379	24.277210
130.092547	3950.880649	24.282227
130.280808	3961.948260	24.287245
130.437229	3963.685440	24.292263
130.313488	3966.532328	24.297280
130.589564	3972.737268	24.302298
130.892019	3972.693181	24.307315
130.952032	3986.587593	24.312333
130.962282	3983.633434	24.317351
131.245297	3995.550004	24.322368
131.677090	4007.890440	24.327386
131.563182	4013.650764	24.332403
131.633740	4008.706257	24.337421
132.227643	4009.862478	24.342439
131.771964	4000.333127	24.347456
132.139074	4007.937649	24.352474
131.931436	4034.199947	24.357491
132.159034	4034.974949	24.362509
132.501792	4027.627901	24.367527
132.594121	4033.275019	24.372544
132.980777	4041.168069	24.377562
132.884401	4047.083782	24.382579
133.112006	4058.345754	24.387597
133.227006	4053.818708	24.392615
132.977952	4062.990867	24.397632
133.513529	4068.867130	24.402650
133.581539	4068.101912	24.407667
133.201739	4066.383094	24.412685
133.474529	4061.035458	24.417703
133.462059	4090.597213	24.422720
133.771108	4078.661450	24.427738
134.340577	4072.952966	24.432755
134.201216	4075.287476	24.437773
134.212004	4091.876038	24.442791
134.209539	4109.141637	24.447808
134.490091	4098.078318	24.452826
134.657615	4111.627112	24.457843
134.885183	4135.674281	24.462861
135.189114	4122.273132	24.467879
134.957170	4141.142492	24.472896
135.105528	4135.380728	24.477914
135.351637	4146.605060	24.482931
135.157832	4155.719717	24.487949
135.571984	4151.226680	24.492967
135.674458	4174.587464	24.497984
135.956003	4184.609856	24.503002
136.176638	4185.126162	24.508019
136.094519	4196.158692	24.513037
136.619689	4186.645117	24.518055
136.362601	4195.893487	24.523072
136.724226	4209.915829	24.528090
136.980063	4218.810945	24.533107
136.954745	4220.442744	24.538125
137.282873	4216.190291	24.543143
137.428489	4218.402928	24.548160
137.398519	4211.814264	24.553178
137.749522	4231.753998	24.558195
137.509355	4246.537257	24.563213
137.811699	4249.861062	24.568231
137.954839	4254.553363	24.573248
137.761499	4248.963771	24.578266
138.000360	4263.542298	24.583283
138.299285	4280.318895	24.588301
139.016507	4270.897164	24.593319
138.611482	4274.614248	24.598336
138.801145	4269.895266	24.603354
139.264668	4280.316411	24.608371
139.340171	4284.742718	24.613389
139.505973	4287.229996	24.618407
139.481889	4286.991428	24.623424
139.777643	4285.355458	24.628442
139.696790	4288.739833	24.633459
139.650557	4295.021782	24.638477
140.066779	4303.314038	24.643495
140.021097	4324.665174	24.648512
139.767099	4331.133050	24.653530
140.208171	4319.588697	24.658547
140.041594	4329.431670	24.663565
140.839389	4332.820093	24.668583
140.884985	4336.116258	24.673600
141.235932	4324.023379	24.678618
141.340812	4338.973739	24.683635
141.367680	4337.245571	24.688653
141.255059	4321.959040	24.693671
141.159968	4343.734136	24.698688
141.807871	4361.104767	24.703706
141.816137	4357.657924	24.708723
141.314231	4370.730518	24.713741
141.934295	4367.612922	24.718759
141.736725	4384.966972	24.723776
141.981861	4380.502192	24.728794
142.845600	4374.651664	24.733811
142.645883	4378.079322	24.738829
143.148358	4368.626871	24.743847
143.392628	4368.023077	24.748864
143.654069	4350.310803	24.753882
143.992568	4356.452037	24.758899
143.756046	4356.472597	24.763917
143.876868	4350.451903	24.768935
143.728513	4348.586930	24.773952
143.536959	4355.230728	24.778970
143.846681	4346.758222	24.783987
143.871942	4375.776067	24.789005
144.188527	4389.036286	24.794023
144.421869	4385.586895	24.799040
144.301854	4391.043232	24.804058
144.935058	4391.574058	24.809075
144.339218	4403.804672	24.814093
144.643751	4406.058405	24.819111
144.539109	4428.304514	24.824128
144.708221	4425.785466	24.829146
145.018741	4430.103293	24.834163
144.690815	4450.908684	24.839181
145.033474	4459.339171	24.844199
145.080439	4475.196530	24.849216
145.441259	4477.743353	24.854234
145.805759	4489.031841	24.859251
145.589507	4510.826402	24.864269
146.316135	4505.969409	24.869287
146.300102	4525.659911	24.874304
146.504191	4534.090893	24.879322
146.480780	4531.875310	24.884339
146.628359	4544.170609	24.889357
147.113369	4547.838731	24.894375
147.492089	4566.217914	24.899392
147.369972	4564.993898	24.904410
147.539266	4565.384834	24.909427
147.811690	4561.261580	24.914445
147.954417	4562.140403	24.919463
148.172891	4576.454071	24.924480
148.086829	4578.818828	24.929498
148.202622	4582.331021	24.934515
148.286636	4596.136573	24.939533
148.612359	4586.019448	24.944551
148.366885	4606.274377	24.949568
148.690626	4619.203666	24.954586
148.923613	4614.393164	24.959603
149.078624	4637.062449	24.964621
149.212226	4645.086998	24.969639
149.407473	4650.377152	24.974656
149.693133	4649.110950	24.979674
149.781171	4646.004038	24.984691
149.664482	4650.869716	24.989709
149.839943	4672.142264	24.994727
150.052584	4679.392297	24.999744
149.953640	4681.230025	25.004762
150.086900	4685.639029	25.009779
150.437657	4698.996630	25.014797
150.667871	4702.208821	25.019815
150.778993	4718.527909	25.024832
150.962811	4742.727350	25.029850
151.134275	4733.791615	25.034867
151.028688	4742.513268	25.039885
151.144930	4753.620116	25.044903
151.658453	4764.689677	25.049920
151.948104	4768.835443	25.054938
151.888624	4760.506008	25.059955
152.054604	4790.738873	25.064973
152.332706	4790.749603	25.069991
152.789381	4783.293216	25.075008
153.331583	4778.596546	25.080026
153.294537	4769.679888	25.085043
153.378671	4769.628172	25.090061
153.578800	4767.211827	25.095079
154.002561	4777.816270	25.100096
153.521356	4770.601084	25.105114
153.574290	4763.739806	25.110131
153.539037	4777.876668	25.115149
153.885797	4758.488678	25.120167
153.788969	4763.797601	25.125184
153.625299	4769.534139	25.130202
153.991070	4776.062010	25.135219
154.019870	4778.725560	25.140237
154.138055	4791.028274	25.145255
154.157977	4813.505945	25.150272
154.229263	4822.105889	25.155290
154.547701	4835.769367	25.160307
154.346153	4866.765133	25.165325
154.698712	4865.634330	25.170343
155.232115	4876.824320	25.175360
155.227964	4888.374028	25.180378
155.401170	4899.392821	25.185395
155.506551	4920.280402	25.190413
155.669735	4931.212676	25.195431
156.045306	4940.714856	25.200448
155.957101	4954.272384	25.205466
156.197214	4961.268380	25.210483
156.286630	4980.895571	25.215501
156.509432	4979.761789	25.220519
157.156614	4997.364376	25.225536
156.967641	5004.211191	25.230554
157.321560	5015.026961	25.235571
157.342959	5012.998413	25.240589
157.546258	5030.283005	25.245607
157.726878	5029.116420	25.250624
157.728217	5043.165971	25.255642
157.656324	5042.188368	25.260659
158.222930	5054.942050	25.265677
158.352614	5059.371044	25.270695
158.374515	5056.264348	25.275712
158.357565	5094.524877	25.280730
158.849676	5093.214292	25.285747
158.835470	5110.455375	25.290765
158.947971	5119.922778	25.295783
159.268440	5116.843123	25.300800
159.535203	5128.327377	25.305818
159.501255	5140.484619	25.310835
159.971753	5157.609049	25.315853
159.796186	5149.547826	25.320871
160.279377	5162.077166	25.325888
160.503032	5180.975660	25.330906
160.660852	5186.362742	25.335923
160.968958	5184.840401	25.340941
160.756346	5191.546305	25.345959
160.805497	5185.012275	25.350976
161.299368	5211.270492	25.355994
161.247657	5208.345238	25.361011
161.441622	5214.327210	25.366029
161.359085	5224.065117	25.371047
161.965772	5239.423637	25.376064
161.962311	5255.973660	25.381082
161.996730	5251.079619	25.386099
162.204852	5251.521646	25.391117
162.136900	5266.840466	25.396135
162.688384	5265.942939	25.401152
162.825557	5278.438196	25.406170
163.046268	5284.940638	25.411187
163.632952	5293.073355	25.416205
164.040667	5282.534316	25.421223
164.527286	5271.434941	25.426240
164.247357	5263.366884	25.431258
164.012106	5235.329010	25.436275
164.247554	5242.729492	25.441293
164.358456	5244.762953	25.446311
164.520740	5256.437024	25.451328
164.360722	5271.577339	25.456346
164.541922	5275.907715	25.461363
164.682756	5273.950354	25.466381
164.729578	5278.263953	25.471399
164.943732	5286.432627	25.476416
164.928603	5309.527107	25.481434
164.809635	5309.238445	25.486451
165.036513	5325.808757	25.491469
164.954482	5347.504736	25.496487
165.221837	5350.152199	25.501504
165.309769	5373.944395	25.506522
165.295715	5393.182459	25.511539
165.903130	5405.549720	25.516557
165.753654	5428.260619	25.521575
166.174085	5440.459566	25.526592
166.437780	5454.382662	25.531610
166.470505	5462.556993	25.536627
166.778734	5473.592075	25.541645
167.072921	5491.585872	25.546663
167.489689	5498.840754	25.551680
167.578836	5501.069599	25.556698
168.132498	5518.534666	25.561715
168.458382	5520.641317	25.566733
168.165400	5525.658457	25.571751
168.558394	5518.669786	25.576768
168.316677	5521.415960	25.581786
168.478740	5537.886168	25.586803
169.216252	5530.693305	25.591821
169.226196	5541.885608	25.596839
169.340877	5530.562036	25.601856
169.838720	5559.114966	25.606874
169.772542	5564.424608	25.611891
170.123120	5567.937212	25.616909
170.183059	5564.469360	25.621927
170.598475	5564.239660	25.626944
170.947662	5561.273301	25.631962
170.808001	5568.469346	25.636979
170.977454	5558.473493	25.641997
170.726075	5572.354618	25.647015
171.032296	5584.853295	25.652032
170.639841	5598.040334	25.657050
171.122631	5603.908583	25.662067
171.344049	5623.993574	25.667085
171.357030	5635.040148	25.672103
171.524151	5633.988364	25.677120
171.635856	5653.265425	25.682138
171.610548	5659.647233	25.687156
172.279750	5673.249551	25.692173
172.247165	5690.975872	25.697191
172.573927	5689.536634	25.702208
172.300094	5704.663884	25.707226
172.652086	5722.587364	25.712244
172.666726	5734.940217	25.717261
172.566637	5752.491908	25.722279
173.097778	5766.244696	25.727296
173.418127	5784.707017	25.732314
173.684171	5794.452258	25.737332
174.377293	5789.963462	25.742349
174.259619	5814.749494	25.747367
174.517556	5809.417895	25.752384
174.791318	5812.881034	25.757402
174.753116	5816.843028	25.762420
175.108887	5813.777488	25.767437
174.790192	5809.690153	25.772455
175.107243	5825.200667	25.777472
175.011950	5845.984036	25.782490
175.013544	5841.194857	25.787508
175.437937	5857.610638	25.792525
175.638233	5883.616085	25.797543
175.583809	5875.567153	25.802560
175.938661	5895.532005	25.807578
175.813500	5906.843364	25.812596
176.240042	5921.278240	25.817613
176.152344	5933.097679	25.822631
176.572415	5957.976217	25.827648
176.857189	5964.805024	25.832666
176.771784	5970.286903	25.837684
176.810622	5984.793772	25.842701
177.206968	6008.076058	25.847719
177.781662	6017.908652	25.852736
177.736900	6036.264640	25.857754
178.091356	6036.791191	25.862772
178.529089	6043.826293	25.867789
178.781601	6061.996164	25.872807
178.950454	6051.968990	25.877824
179.188186	6050.851567	25.882842
178.847594	6072.612138	25.887860
179.206085	6073.710558	25.892877
179.295365	6081.792389	25.897895
179.978344	6097.798708	25.902912
179.919237	6108.933129	25.907930
180.025847	6110.803999	25.912948
179.923743	6113.265353	25.917965
179.986881	6125.002525	25.922983
180.209262	6134.419309	25.928000
180.624516	6153.566501	25.933018
180.614072	6181.970652	25.938036
180.864245	6171.872476	25.943053
180.802984	6191.361484	25.948071
181.157091	6201.019581	25.953088
181.305955	6227.326271	25.958106
181.263199	6231.823073	25.963124
181.657819	6252.010194	25.968141
181.751923	6275.375891	25.973159
182.004009	6277.017985	25.978176
182.143013	6297.266300	25.983194
182.021806	6317.851388	25.988212
182.292326	6312.247415	25.993229
182.355542	6341.366584	25.998247
183.002280	6351.527704	26.003264
183.977597	6351.003482	26.008282
183.923896	6359.035838	26.013300
184.415298	6350.325508	26.018317
184.699906	6358.064129	26.023335
184.661955	6381.054092	26.028352
184.889295	6379.786368	26.033370
184.937255	6387.794066	26.038388
185.140633	6373.830343	26.043405
185.112517	6384.144729	26.048423
184.999341	6376.331273	26.053440
185.284605	6387.850805	26.058458
185.204605	6409.320706	26.063476
185.828193	6410.027255	26.068493
185.403342	6415.923708	26.073511
185.602727	6433.149067	26.078528
185.903092	6454.883017	26.083546
185.770561	6466.530703	26.088564
186.108887	6476.249856	26.093581
185.837979	6500.912652	26.098599
186.113912	6517.981334	26.103616
186.619120	6527.501259	26.108634
186.803430	6556.751241	26.113652
187.429051	6568.068972	26.118669
187.309041	6583.017680	26.123687
187.460309	6586.917848	26.128704
187.677805	6611.072475	26.133722
187.417645	6624.536995	26.138740
187.787815	6637.881629	26.143757
188.274591	6647.971715	26.148775
188.294095	6682.231258	26.153792
188.875670	6676.925439	26.158810
188.929314	6692.870962	26.163828
189.278084	6705.868725	26.168845
189.609531	6710.112457	26.173863
189.524964	6723.543324	26.178880
189.858553	6731.860770	26.183898
189.727644	6741.363856	26.188916
189.920297	6752.251580	26.193933
190.076918	6768.409346	26.198951
190.070715	6796.435085	26.203968
190.444986	6808.985320	26.208986
190.634185	6820.969954	26.214004
190.772443	6823.903623	26.219021
190.990852	6845.727260	26.224039
191.088356	6862.997487	26.229056
191.381708	6875.643840	26.234074
191.472042	6896.777533	26.239092
191.734043	6911.741404	26.244109
192.182282	6920.415679	26.249127
192.411684	6938.950302	26.254144
193.044446	6944.573759	26.259162
193.177030	6962.790476	26.264180
193.458962	6953.607229	26.269197
193.542713	6975.169768	26.274215
193.903661	6980.550684	26.279232
194.594339	6974.485632	26.284250
194.798670	6976.280605	26.289268
195.075159	6970.255637	26.294285
195.311557	6969.287223	26.299303
195.261359	6973.598023	26.304320
195.102601	6958.464213	26.309338
195.262101	6967.086987	26.314356
195.316128	6984.046350	26.319373
195.362571	6994.359054	26.324391
195.626862	7003.316580	26.329408
195.860337	7006.777979	26.334426
195.842263	7033.697193	26.339444
195.802803	7037.013887	26.344461
195.827687	7040.531022	26.349479
195.839828	7062.083460	26.354496
196.185444	7082.430961	26.359514
196.249662	7099.860525	26.364532
196.519630	7121.857170	26.369549
196.384945	7146.620541	26.374567
196.676306	7180.437730	26.379584
197.386480	7181.129226	26.384602
197.838875	7195.623224	26.389620
198.365226	7185.575644	26.394637
198.359570	7207.681743	26.399655
198.654518	7224.295187	26.404672
199.145576	7225.719904	26.409690
198.942324	7231.535939	26.414708
199.000552	7252.633672	26.419725
199.460615	7265.381171	26.424743
199.453758	7248.256161	26.429760
200.313513	7254.951152	26.434778
199.948203	7267.954738	26.439796
200.098463	7277.536918	26.444813
200.328552	7281.684140	26.449831
200.813499	7295.875931	26.454848
200.877824	7295.007600	26.459866
200.959324	7305.987319	26.464884
200.890891	7323.603654	26.469901
201.126175	7320.200169	26.474919
200.947786	7334.483479	26.479936
201.348193	7347.885940	26.484954
201.558598	7357.674032	26.489972
201.912747	7365.430013	26.494989
202.139398	7373.197613	26.500007
201.706435	7396.412627	26.505024
202.555293	7396.406251	26.510042
202.261929	7420.366142	26.515060
202.768073	7428.864949	26.520077
203.172281	7445.107730	26.525095
203.505359	7473.336945	26.530112
203.940925	7472.304092	26.535130
203.813211	7474.722631	26.540148
203.780140	7498.587652	26.545165
204.175356	7511.593372	26.550183
203.986358	7516.487237	26.555200
204.064116	7537.911341	26.560218
204.340096	7550.184633	26.565236
204.668606	7570.063027	26.570253
204.864327	7592.877528	26.575271
204.908730	7604.376315	26.580288
205.508652	7613.051903	26.585306
205.752218	7626.386003	26.590324
206.099850	7644.348233	26.595341
206.230012	7651.613667	26.600359
206.482104	7663.806719	26.605376
207.317922	7683.276155	26.610394
207.435731	7682.528135	26.615412
207.322506	7691.630339	26.620429
207.524378	7688.900977	26.625447
207.704552	7706.634973	26.630464
208.084016	7709.152477	26.635482
208.108904	7723.168630	26.640500
208.280707	7746.268482	26.645517
208.640908	7742.648153	26.650535
208.428339	7745.377683	26.655552
208.803216	7762.802333	26.660570
208.997753	7775.008132	26.665588
208.862135	7783.986495	26.670605
209.133854	7802.091404	26.675623
209.331656	7817.943360	26.680640
209.652599	7834.982404	26.685658
209.915018	7836.628471	26.690676
209.960967	7873.475128	26.695693
210.495189	7869.382588	26.700711
210.365503	7885.919604	26.705728
210.729801	7898.058068	26.710746
210.664956	7922.327513	26.715764
210.963192	7940.995288	26.720781
211.205831	7961.159306	26.725799
211.061955	7973.416445	26.730816
211.793446	7993.779342	26.735834
211.583839	8009.836637	26.740852
212.110854	8032.267020	26.745869
212.295415	8039.543334	26.750887
212.683574	8072.185476	26.755904
213.151237	8060.429222	26.760922
213.328383	8085.626931	26.765940
213.288444	8093.481465	26.770957
213.901177	8107.299229	26.775975
213.549648	8115.606947	26.780992
213.667881	8133.954982	26.786010
214.034920	8132.404910	26.791028
213.890510	8163.927004	26.796045
214.842759	8164.263502	26.801063
214.469864	8187.757234	26.806080
215.024571	8196.250797	26.811098
215.227568	8207.743509	26.816116
215.405698	8226.042372	26.821133
215.750814	8218.887149	26.826151
215.924236	8237.001709	26.831168
216.519867	8253.195580	26.836186
216.921877	8251.818512	26.841204
216.461407	8262.548967	26.846221
217.193198	8269.764904	26.851239
217.134349	8287.173578	26.856256
217.139340	8290.603699	26.861274
217.744403	8302.697969	26.866292
217.402890	8311.412920	26.871309
217.863426	8330.526137	26.876327
218.075816	8347.207176	26.881344
218.320820	8342.797623	26.886362
218.328945	8366.304279	26.891380
218.314323	8376.217611	26.896397
218.977801	8390.834576	26.901415
219.075631	8414.005122	26.906432
219.151080	8416.025556	26.911450
219.398716	8439.775514	26.916468
219.641307	8462.895434	26.921485
220.501927	8453.485749	26.926503
220.533412	8468.333229	26.931520
220.845364	8492.027743	26.936538
221.234593	8495.392061	26.941556
221.096187	8489.482328	26.946573
221.555064	8509.853915	26.951591
221.643140	8533.164873	26.956608
221.380622	8537.709666	26.961626
221.879571	8552.426429	26.966644
221.741992	8564.678257	26.971661
222.538903	8587.842251	26.976679
222.587804	8598.899141	26.981696
222.758680	8607.195629	26.986714
223.155063	8626.144156	26.991732
223.061784	8639.382746	26.996749
223.252043	8657.461135	27.001767
223.323473	8667.165091	27.006784
223.468772	8687.163379	27.011802
224.100047	8704.774339	27.016820
224.335767	8730.041373	27.021837
224.244371	8728.333052	27.026855
224.424820	8746.953500	27.031872
224.934009	8759.220707	27.036890
224.875763	8782.715315	27.041908
224.944005	8797.250626	27.046925
225.862783	8810.207147	27.051943
225.778557	8825.005550	27.056960
226.213547	8842.758580	27.061978
226.650977	8840.904588	27.066996
226.624064	8854.799546	27.072013
227.242373	8870.431060	27.077031
227.391066	8873.835202	27.082048
227.512706	8884.490376	27.087066
227.718755	8904.751434	27.092084
227.468336	8911.956662	27.097101
228.117610	8918.234238	27.102119
227.991178	8933.323277	27.107136
228.295628	8953.766634	27.112154
228.998541	8965.352164	27.117172
228.702519	8977.355589	27.122189
228.835464	8980.751328	27.127207
229.107138	9005.980566	27.132224
229.257937	9026.247757	27.137242
229.420250	9035.118525	27.142260
229.479987	9054.586339	27.147277
229.710669	9070.949258	27.152295
230.015925	9095.905279	27.157312
230.132485	9112.034250	27.162330
230.238901	9135.893652	27.167348
230.605036	9148.819668	27.172365
231.250993	9169.691304	27.177383
231.167380	9189.603591	27.182400
231.179311	9208.300470	27.187418
231.769829	9220.234010	27.192436
231.845930	9245.784234	27.197453
232.035090	9263.951715	27.202471
232.323160	9284.400566	27.207488
232.966754	9300.587587	27.212506
233.363501	9300.562981	27.217524
233.347636	9323.816653	27.222541
233.452920	9334.752887	27.227559
233.760486	9354.629106	27.232576
233.931122	9365.538022	27.237594
234.303356	9372.101012	27.242612
234.396178	9400.009440	27.247629
234.960129	9412.109779	27.252647
235.094989	9428.844149	27.257664
235.251121	9431.810798	27.262682
235.475881	9456.839762	27.267700
235.588875	9468.829542	27.272717
235.839772	9483.222661	27.277735
235.956457	9507.444052	27.282752
235.736785	9529.475314	27.287770
236.591268	9545.726205	27.292788
236.398854	9573.563907	27.297805
236.572586	9587.743799	27.302823
237.281976	9618.536143	27.307840
237.364556	9633.956019	27.312858
238.158712	9657.275637	27.317876
238.338165	9677.431006	27.322893
238.785575	9673.874608	27.327911
239.445746	9695.540962	27.332928
239.651202	9699.536926	27.337946
239.897495	9690.359570	27.342964
239.902456	9698.610784	27.347981
240.247682	9711.103535	27.352999
240.669938	9723.384277	27.358016
240.922664	9719.104620	27.363034
241.276796	9723.198121	27.368052
240.801582	9728.153341	27.373069
241.371013	9738.986385	27.378087
241.449277	9738.031335	27.383104
241.568632	9759.805246	27.388122
242.013965	9758.134959	27.393140
241.763586	9781.162584	27.398157
241.884667	9779.312703	27.403175
242.229743	9797.450307	27.408192
242.215209	9820.596566	27.413210
242.596307	9819.170837	27.418228
242.832798	9851.907076	27.423245
242.919022	9870.404981	27.428263
243.229136	9885.177813	27.433280
243.373498	9919.675787	27.438298
243.889312	9938.230405	27.443316
243.789172	9950.707913	27.448333
244.098322	9969.489704	27.453351
244.433741	9981.893700	27.458368
244.667447	10012.169878	27.463386
244.937735	10007.393338	27.468404
245.268500	10028.124399	27.473421
245.328997	10050.589814	27.478439
245.572494	10061.260304	27.483456
245.663619	10082.202752	27.488474
246.357687	10095.527516	27.493492
246.139729	10102.526255	27.498509
246.563639	10118.373873	27.503527
247.163337	10140.677071	27.508544
246.893771	10161.887177	27.513562
247.424820	10181.249351	27.518580
247.658737	10188.293994	27.523597
247.925231	10216.648585	27.528615
248.322804	10236.755233	27.533632
248.108839	10253.934878	27.538650
248.811045	10267.997341	27.543668
249.076112	10274.643007	27.548685
249.529953	10292.581237	27.553703
250.040671	10299.152455	27.558720
250.100594	10318.034913	27.563738
250.611112	10330.003777	27.568756
250.677575	10332.929480	27.573773
250.698348	10350.012153	27.578791
251.113248	10355.654722	27.583808
251.681731	10360.340806	27.588826
252.142844	10364.089099	27.593844
252.583786	10383.122950	27.598861
252.252153	10379.941673	27.603879
252.979976	10379.091171	27.608896
252.790831	10392.399831	27.613914
253.028323	10399.132818	27.618932
252.867074	10403.599960	27.623949
252.987075	10424.408896	27.628967
253.241585	10438.465127	27.633984
253.636190	10465.953742	27.639002
254.097945	10472.240867	27.644020
254.105559	10493.981462	27.649037
254.249288	10511.630079	27.654055
254.699446	10516.072651	27.659072
254.496928	10543.272480	27.664090
255.067333	10573.714664	27.669108
255.165076	10584.957074	27.674125
255.543997	10599.608916	27.679143
255.800725	10628.774875	27.684160
255.986929	10640.961408	27.689178
256.441093	10659.396285	27.694196
256.818839	10666.919179	27.699213
257.312461	10688.604950	27.704231
257.667763	10692.890724	27.709248
257.616560	10701.881200	27.714266
258.260234	10722.558315	27.719284
258.200274	10716.484331	27.724301
258.759833	10739.184941	27.729319
259.127590	10739.249421	27.734336
258.863378	10762.822720	27.739354
259.401291	10769.937136	27.744372
259.743508	10763.494188	27.749389
259.849113	10788.615826	27.754407
260.150307	10815.680116	27.759424
260.121737	10827.623406	27.764442
260.727301	10822.652587	27.769460
260.914268	10843.243034	27.774477
260.842572	10865.771610	27.779495
261.521584	10875.905121	27.784512
261.382720	10884.006612	27.789530
261.412384	10899.399427	27.794548
261.837547	10908.634302	27.799565
261.610555	10934.066354	27.804583
262.117135	10944.735722	27.809600
262.018530	10971.425964	27.814618
262.526012	10999.195413	27.819636
262.815560	11011.759830	27.824653
262.998765	11033.596614	27.829671
263.269689	11045.730070	27.834688
263.503751	11081.241413	27.839706
263.605933	11105.823697	27.844724
263.731707	11114.717416	27.849741
263.957404	11159.722277	27.854759
264.693384	11166.968794	27.859776
264.810696	11189.002593	27.864794
265.122496	11215.292990	27.869812
265.851004	11234.505653	27.874829
265.635284	11262.269784	27.879847
266.219301	11276.287280	27.884864
266.588755	11296.410149	27.889882
266.676245	11311.419605	27.894900
266.978436	11329.672388	27.899917
267.324063	11355.335071	27.904935
267.898807	11362.719396	27.909952
267.839665	11385.962730	27.914970
267.868462	11393.120574	27.919988
268.394681	11420.228274	27.925005
268.557935	11450.337619	27.930023
269.046921	11461.593209	27.935040
269.188633	11484.229986	27.940058
269.598861	11500.524767	27.945076
269.982398	11513.966626	27.950093
269.998310	11537.464843	27.955111
270.374305	11548.962110	27.960128
270.701710	11577.413824	27.965146
270.558962	11600.940710	27.970164
271.180478	11615.157138	27.975181
271.126042	11629.039357	27.980199
271.958905	11654.778007	27.985216
271.958092	11667.959706	27.990234
272.741891	11675.716147	27.995252
273.162102	11685.178391	28.000269
273.310015	11700.015939	28.005287
273.845493	11709.619867	28.010304
273.991336	11720.910273	28.015322
273.978904	11731.003367	28.020340
274.327138	11735.230718	28.025357
274.361407	11756.067362	28.030375
274.797130	11772.279427	28.035392
274.956715	11783.125644	28.040410
274.946333	11799.026197	28.045428
275.419123	11819.569887	28.050445
275.418479	11844.275856	28.055463
275.831113	11870.003922	28.060480
275.753678	11884.665373	28.065498
275.846680	11898.974097	28.070516
276.939354	11917.925736	28.075533
276.805147	11923.409844	28.080551
277.329317	11953.984404	28.085568
277.584357	11964.113812	28.090586
277.611191	11991.124572	28.095604
278.258792	11997.060954	28.100621
278.467885	12027.460815	28.105639
279.107206	12015.383398	28.110656
279.839112	12036.548693	28.115674
280.015634	12049.440637	28.120692
280.055321	12048.699023	28.125709
280.192405	12066.583645	28.130727
280.576302	12076.015092	28.135744
281.206621	12080.136845	28.140762
281.727118	12078.093874	28.145780
281.674256	12083.856094	28.150797
282.018849	12071.655581	28.155815
282.269614	12086.682117	28.160832
281.874433	12098.502567	28.165850
282.563051	12103.130722	28.170868
282.683898	12102.318973	28.175885
282.553325	12126.169200	28.180903
283.062182	12132.216792	28.185920
282.928557	12159.734920	28.190938
283.075872	12173.583489	28.195956
283.041042	12195.644591	28.200973
283.330148	12227.720725	28.205991
283.749000	12252.019245	28.211008
284.086172	12268.580560	28.216026
283.950789	12293.349657	28.221044
284.365917	12322.656395	28.226061
284.293806	12361.085731	28.231079
285.243752	12378.596902	28.236096
285.581119	12407.284792	28.241114
285.585399	12434.084938	28.246132
286.469608	12451.550325	28.251149
286.564924	12475.099031	28.256167
287.222794	12491.004102	28.261184
287.310956	12506.924526	28.266202
287.683554	12524.587967	28.271220
288.201183	12549.209391	28.276237
288.250616	12570.002038	28.281255
288.628443	12583.884571	28.286272
289.012204	12592.597825	28.291290
288.981967	12613.747194	28.296308
289.583865	12626.912040	28.301325
289.635167	12658.247555	28.306343
289.788404	12673.322265	28.311360
291.001010	12679.139561	28.316378
291.473534	12682.646227	28.321396
291.767216	12668.967779	28.326413
292.299484	12699.130370	28.331431
292.561688	12704.810032	28.336448
292.835615	12711.513551	28.341466
292.865261	12725.036164	28.346484
292.941691	12727.533638	28.351501
292.776749	12751.864757	28.356519
293.043459	12758.678212	28.361536
293.433054	12772.261153	28.366554
293.572780	12789.344098	28.371572
294.134849	12804.294662	28.376589
294.535514	12817.346368	28.381607
294.920614	12832.012626	28.386624
295.271275	12841.547710	28.391642
295.028299	12859.607878	28.396660
295.799957	12867.461454	28.401677
295.972940	12891.792105	28.406695
295.949207	12895.762131	28.411712
296.451217	12917.343959	28.416730
296.674429	12925.114839	28.421748
297.029351	12939.661698	28.426765
297.243514	12949.046066	28.431783
297.194018	12965.303256	28.436800
297.961972	12976.554795	28.441818
298.274310	13018.053965	28.446836
298.659228	13029.825788	28.451853
298.451396	13053.220573	28.456871
298.549331	13068.991816	28.461888
299.266124	13089.947484	28.466906
299.153818	13116.988628	28.471924
299.311512	13131.374425	28.476941
299.003263	13159.486436	28.481959
299.870768	13191.228626	28.486976
300.278499	13200.601646	28.491994
300.330189	13228.172127	28.497012
301.029844	13255.044693	28.502029
300.983850	13276.821536	28.507047
301.015415	13297.947407	28.512064
301.632354	13328.513190	28.517082
301.810875	13353.061077	28.522100
302.597583	13373.189310	28.527117
302.671986	13394.368109	28.532135
303.131475	13413.537223	28.537152
303.535634	13441.710091	28.542170
303.797392	13463.059728	28.547188
304.419260	13461.017179	28.552205
304.776607	13479.877058	28.557223
304.927693	13501.736677	28.562240
305.297716	13511.582543	28.567258
305.628943	13540.407404	28.572276
305.887650	13563.519418	28.577293
306.303971	13565.314793	28.582311
306.506336	13586.861926	28.587328
307.038274	13594.673523	28.592346
307.043952	13627.638376	28.597364
307.679667	13638.707373	28.602381
307.929192	13655.675394	28.607399
308.222862	13662.120766	28.612416
308.294742	13682.988350	28.617434
308.628880	13710.276617	28.622452
308.907137	13724.474411	28.627469
309.154090	13740.883532	28.632487
309.342073	13774.037603	28.637504
309.764830	13796.345969	28.642522
309.901466	13813.677910	28.647540
310.002028	13843.631887	28.652557
310.636370	13867.944515	28.657575
310.912576	13886.210004	28.662592
311.083530	13913.962078	28.667610
311.379790	13937.191336	28.672628
312.141895	13948.491799	28.677645
312.349817	13972.777331	28.682663
312.638257	13984.293170	28.687680
313.363295	14000.177608	28.692698
313.395223	14007.065048	28.697716
313.785099	14035.263370	28.702733
314.408011	14048.257294	28.707751
314.517554	14072.251938	28.712768
314.817755	14092.067480	28.717786
314.352569	14108.890883	28.722804
315.110296	14121.432387	28.727821
315.614961	14158.827550	28.732839
315.893068	14184.097744	28.737856
316.043154	14189.657778	28.742874
316.631135	14216.101272	28.747892
317.047614	14232.030611	28.752909
317.296969	14252.463033	28.757927
317.546166	14267.085285	28.762944
317.967031	14276.689990	28.767962
317.982351	14313.838572	28.772980
318.188814	14319.646204	28.777997
318.684343	14346.376234	28.783015
318.644215	14377.095098	28.788032
319.020207	14402.784404	28.793050
319.389379	14424.478438	28.798068
319.768944	14451.126942	28.803085
319.979236	14464.512425	28.808103
320.399592	14483.178685	28.813120
320.800363	14512.731300	28.818138
320.964787	14528.420487	28.823156
321.042265	14555.145857	28.828173
321.316583	14579.485938	28.833191
321.836598	14605.755340	28.838208
321.943837	14628.154797	28.843226
322.156854	14652.383769	28.848244
322.404291	14691.340249	28.853261
322.805555	14700.407908	28.858279
323.229999	14725.949463	28.863296
324.267698	14743.018495	28.868314
324.229771	14772.948208	28.873332
324.646504	14796.485008	28.878349
325.147680	14808.639205	28.883367
325.204756	14836.345477	28.888384
325.557014	14850.249942	28.893402
325.400231	14872.045647	28.898420
325.714984	14897.552012	28.903437
326.245532	14919.987526	28.908455
326.528219	14947.584222	28.913472
327.755075	14962.803610	28.918490
327.979367	14994.167061	28.923508
327.896809	15011.460845	28.928525
328.205718	15016.530023	28.933543
328.471199	15053.640539	28.938560
329.011047	15080.471619	28.943578
329.238646	15094.724684	28.948596
329.678238	15134.284008	28.953613
330.070892	15138.592389	28.958631
330.060829	15161.335027	28.963648
330.590671	15179.448175	28.968666
330.743894	15208.620594	28.973684
330.730210	15229.524782	28.978701
331.459922	15260.745361	28.983719
331.360827	15286.533459	28.988736
331.744225	15314.424604	28.993754
332.278725	15349.058054	28.998772
332.638409	15380.398304	29.003789
333.138591	15403.652703	29.008807
333.177120	15446.089007	29.013824
333.876283	15461.189590	29.018842
334.102575	15491.128976	29.023860
334.791804	15506.636270	29.028877
335.817210	15511.550989	29.033895
336.043565	15521.015208	29.038912
336.429685	15538.430697	29.043930
336.595373	15546.497594	29.048948
336.900970	15544.507049	29.053965
337.325156	15572.089306	29.058983
337.368375	15583.534895	29.064000
338.041263	15597.706958	29.069018
338.111761	15626.424142	29.074036
338.108753	15643.892997	29.079053
338.301351	15657.372216	29.084071
338.391016	15692.084611	29.089088
338.937218	15716.345225	29.094106
339.121405	15739.702740	29.099124
339.548797	15772.948985	29.104141
339.682935	15795.380272	29.109159
339.440859	15837.778843	29.114176
340.125932	15871.403515	29.119194
340.533885	15905.122894	29.124212
340.744506	15935.251654	29.129229
341.082856	15959.452406	29.134247
341.115586	16010.360718	29.139264
341.870935	16044.536782	29.144282
342.178129	16072.629359	29.149300
342.641696	16095.986933	29.154317
343.539745	16106.978036	29.159335
343.607324	16146.812459	29.164352
343.964402	16153.156939	29.169370
344.344339	16181.245566	29.174388
344.526260	16204.224289	29.179405
345.134673	16217.072625	29.184423
345.295969	16253.467058	29.189440
345.543517	16263.648465	29.194458
345.871299	16283.492062	29.199476
346.125428	16324.791781	29.204493
346.462733	16343.267429	29.209511
346.939081	16368.938524	29.214528
347.551849	16387.943981	29.219546
348.729195	16396.244494	29.224564
349.053975	16408.224140	29.229581
349.395983	16421.176539	29.234599
349.353006	16444.419707	29.239616
349.786024	16455.487871	29.244634
349.620547	16485.326732	29.249652
349.645409	16491.466173	29.254669
350.298841	16517.038899	29.259687
350.891237	16557.055553	29.264704
350.781843	16569.765847	29.269722
351.179066	16602.265389	29.274740
351.703628	16628.168493	29.279757
352.135750	16642.833580	29.284775
352.172054	16680.051840	29.289792
352.676922	16702.353775	29.294810
352.972567	16725.363301	29.299828
353.355725	16758.796954	29.304845
354.034099	16769.536371	29.309863
354.364816	16801.524027	29.314880
354.817283	16813.722445	29.319898
355.097930	16836.209759	29.324916
355.596100	16864.213827	29.329933
356.197257	16872.830430	29.334951
356.363922	16899.198149	29.339968
356.408546	16919.354082	29.344986
356.989573	16946.690513	29.350004
357.140424	16968.031540	29.355021
357.646193	16998.548506	29.360039
357.824214	17023.319504	29.365056
358.354930	17046.938437	29.370074
358.603289	17067.390307	29.375092
358.906734	17101.532903	29.380109
359.424813	17119.777816	29.385127
359.832921	17149.835202	29.390144
360.328230	17171.048662	29.395162
362.008576	17144.610198	29.400180
362.575056	17154.198856	29.405197
362.930843	17153.963537	29.410215
362.989636	17153.610208	29.415232
363.202500	17154.268531	29.420250
363.401139	17154.180535	29.425268
363.304981	17161.796577	29.430285
363.618514	17180.986362	29.435303
363.877848	17182.910537	29.440320
363.891695	17217.848311	29.445338
363.985071	17231.993015	29.450356
364.243427	17255.786488	29.455373
364.545102	17279.568110	29.460391
364.781538	17318.099215	29.465408
365.083070	17343.372000	29.470426
365.716468	17369.452164	29.475444
365.571481	17409.000071	29.480461
365.538498	17433.979924	29.485479
366.044077	17471.194953	29.490496
366.623713	17514.072078	29.495514
367.058922	17532.085257	29.500532
367.444735	17574.611546	29.505549
367.883086	17588.185731	29.510567
367.830607	17617.856661	29.515584
368.164373	17666.294613	29.520602
368.931113	17691.052900	29.525620
369.020522	17724.273818	29.530637
369.450834	17756.407651	29.535655
369.811365	17802.842958	29.540672
370.281826	17821.931909	29.545690
370.847607	17853.014287	29.550708
371.211506	17891.803088	29.555725
371.609009	17928.102308	29.560743
371.963799	17951.069101	29.565760
372.291256	17983.277111	29.570778
372.690543	18010.823449	29.575796
372.826575	18047.315866	29.580813
373.863859	18070.917214	29.585831
374.323099	18099.062220	29.590848
374.901877	18111.109911	29.595866
375.608562	18129.427246	29.600884
375.540163	18155.820044	29.605901
376.502789	18169.278153	29.610919
376.420241	18201.817553	29.615936
376.437435	18221.494125	29.620954
376.979419	18242.152723	29.625972
377.339531	18268.544268	29.630989
377.511538	18297.047584	29.636007
377.976034	18327.439850	29.641024
378.115751	18357.081932	29.646042
378.514287	18374.001862	29.651060
378.938861	18424.744141	29.656077
379.166572	18449.452327	29.661095
379.374023	18488.608847	29.666112
379.912486	18523.219970	29.671130
379.918102	18558.209223	29.676148
380.437461	18607.752620	29.681165
380.578873	18640.246426	29.686183
381.446703	18668.673265	29.691200
381.639402	18715.851345	29.696218
382.178628	18747.087964	29.701236
382.575611	18789.314461	29.706253
383.571057	18797.714046	29.711271
383.873058	18828.386285	29.716288
384.167562	18869.463450	29.721306
385.003409	18877.883137	29.726324
385.053038	18907.993487	29.731341
385.302641	18939.369740	29.736359
385.698808	18956.720992	29.741376
386.035987	18981.889512	29.746394
386.456396	19018.584574	29.751412
386.263647	19061.022679	29.756429
386.655172	19090.189408	29.761447
387.367989	19113.951467	29.766464
387.833952	19155.864847	29.771482
388.867966	19173.101499	29.776500
388.983434	19199.038395	29.781517
389.762270	19228.880690	29.786535
390.051299	19245.455467	29.791552
390.052942	19282.005906	29.796570
390.614141	19286.367942	29.801588
390.639714	19328.717069	29.806605
391.254146	19351.512078	29.811623
391.638974	19383.516291	29.816640
391.623884	19408.463060	29.821658
392.230901	19442.498866	29.826676
392.469966	19479.026281	29.831693
392.770459	19511.692559	29.836711
393.518052	19529.322124	29.841728
393.528697	19560.518333	29.846746
394.209475	19593.999993	29.851764
394.361301	19616.471387	29.856781
394.894098	19646.684542	29.861799
395.114126	19677.970917	29.866816
395.182996	19698.690575	29.871834
395.670901	19735.751252	29.876852
395.539575	19776.232614	29.881869
396.154997	19808.070287	29.886887
396.991709	19845.541778	29.891904
397.172222	19894.329992	29.896922
397.804194	19924.041736	29.901940
397.993761	19957.518570	29.906957
398.436241	19985.995869	29.911975
398.900963	20026.018375	29.916992
398.951023	20070.460400	29.922010
399.619295	20093.933280	29.927028
399.798996	20139.813843	29.932045
400.093334	20186.607267	29.937063
400.109240	20223.535758	29.942080
400.400407	20269.081400	29.947098
401.547282	20316.811065	29.952116
401.870470	20354.947090	29.957133
402.343912	20404.714674	29.962151
403.116107	20435.799330	29.967168
403.149782	20478.942995	29.972186
403.660484	20504.761458	29.977204
404.338538	20542.438868	29.982221
404.570334	20564.840001	29.987239
405.363537	20595.655061	29.992256
406.023795	20621.114787	29.997274
406.739816	20649.076668	30.002292
407.048026	20675.510565	30.007309
407.403256	20705.264690	30.012327
407.970317	20729.831924	30.017344
408.213225	20758.665114	30.022362
408.943274	20779.089290	30.027380
409.271318	20799.694983	30.032397
409.347026	20823.128047	30.037415
410.000163	20849.524159	30.042432
410.232380	20882.771941	30.047450
410.704644	20895.170325	30.052468
410.866069	20927.022075	30.057485
411.260876	20959.276754	30.062503
411.637475	20985.346707	30.067520
411.635470	21017.233508	30.072538
412.272890	21070.326074	30.077556
412.767291	21092.211579	30.082573
413.066098	21123.987407	30.087591
413.867194	21158.841254	30.092608
414.127821	21188.246113	30.097626
414.572422	21221.544616	30.102644
415.171508	21243.833961	30.107661
415.735132	21264.410770	30.112679
416.149095	21296.022862	30.117696
416.231093	21312.799432	30.122714
416.575825	21348.611924	30.127732
416.952107	21381.554697	30.132749
417.570515	21421.424307	30.137767
418.200745	21431.913021	30.142784
418.242592	21475.748434	30.147802
418.576451	21498.726742	30.152820
419.087016	21536.940140	30.157837
419.277975	21575.679389	30.162855
419.618910	21608.653672	30.167872
419.735400	21651.244337	30.172890
420.158233	21688.233387	30.177908
420.613178	21721.819689	30.182925
420.653731	21759.969343	30.187943
421.323081	21788.959314	30.192960
421.741217	21832.115476	30.197978
422.263361	21875.106369	30.202996
422.681302	21912.508212	30.208013
423.071009	21946.482546	30.213031
423.468651	21981.820976	30.218048
423.902452	22021.326781	30.223066
424.318846	22061.079929	30.228084
425.018235	22085.687209	30.233101
425.738829	22110.995768	30.238119
426.462514	22137.360188	30.243136
426.750851	22171.339110	30.248154
427.149973	22195.844797	30.253172
427.649979	22229.066778	30.258189
427.812009	22266.084415	30.263207
428.417932	22288.288885	30.268224
428.733162	22313.076628	30.273242
429.091690	22345.239062	30.278260
429.660086	22373.002754	30.283277
430.253036	22418.698314	30.288295
430.825856	22430.523098	30.293312
430.739259	22473.307056	30.298330
431.559798	22503.378519	30.303348
432.134541	22517.714652	30.308365
432.221185	22564.113866	30.313383
432.792495	22591.303535	30.318400
433.114194	22626.061463	30.323418
433.260075	22651.546184	30.328436
433.755111	22694.240931	30.333453
434.338876	22741.447756	30.338471
434.452439	22770.966395	30.343488
434.726091	22822.437550	30.348506
435.012678	22857.818238	30.353524
435.705976	22913.080073	30.358541
436.176580	22941.813178	30.363559
436.500661	22988.270515	30.368576
437.114138	23030.631209	30.373594
437.530681	23063.520173	30.378612
438.482398	23089.613493	30.383629
438.751726	23124.702748	30.388647
439.600121	23148.962171	30.393664
440.145777	23187.654421	30.398682
440.603866	23200.950856	30.403700
441.627204	23222.772267	30.408717
442.260119	23247.502601	30.413735
442.882922	23245.808797	30.418752
442.891868	23275.451239	30.423770
443.247214	23283.802766	30.428788
443.695439	23298.352826	30.433805
444.362466	23332.284149	30.438823
445.015769	23348.769710	30.443840
445.140190	23363.762766	30.448858
445.314454	23389.604984	30.453876
445.667752	23406.803963	30.458893
445.627187	23431.786147	30.463911
446.130781	23472.728120	30.468928
446.422240	23503.946762	30.473946
447.153804	23532.541587	30.478964
447.445784	23555.004567	30.483981
447.597678	23601.359585	30.488999
448.229170	23625.734364	30.494016
448.630839	23670.367492	30.499034
448.655774	23716.262885	30.504052
448.915784	23743.507414	30.509069
449.138499	23794.748699	30.514087
449.674824	23842.530924	30.519104
450.139093	23883.475656	30.524122
450.305003	23932.821992	30.529140
450.720347	23969.175536	30.534157
451.071695	24014.527436	30.539175
451.339474	24055.184951	30.544192
451.728876	24112.681615	30.549210
452.829205	24138.755167	30.554228
453.747062	24170.395066	30.559245
454.176641	24219.935205	30.564263
454.768463	24244.853545	30.569280
455.294547	24291.607493	30.574298
455.727164	24309.778222	30.579316
455.475557	24348.535442	30.584333
456.111630	24403.628690	30.589351
456.488243	24433.985069	30.594368
456.758672	24480.524743	30.599386
457.343616	24525.121962	30.604404
458.124666	24572.523646	30.609421
458.407015	24621.086402	30.614439
459.057937	24652.105865	30.619456
459.149779	24691.616058	30.624474
459.624369	24745.335265	30.629492
460.274222	24785.313286	30.634509
460.273174	24839.027782	30.639527
460.877856	24874.139377	30.644544
461.779779	24924.891851	30.649562
461.729955	24982.705272	30.654580
462.776235	25014.278228	30.659597
462.826017	25074.808249	30.664615
463.228671	25111.634669	30.669632
463.997303	25156.860768	30.674650
464.486155	25194.412694	30.679668
465.359020	25224.519785	30.684685
465.715053	25273.343457	30.689703
465.851931	25317.619385	30.694720
466.977854	25358.614494	30.699738
467.498235	25392.080591	30.704756
468.576860	25425.386734	30.709773
468.578075	25458.462488	30.714791
469.008952	25490.163213	30.719808
469.589064	25525.576673	30.724826
470.391518	25547.018117	30.729844
470.947493	25574.065306	30.734861
471.442560	25603.510084	30.739879
472.117808	25619.429693	30.744896
472.133891	25663.767473	30.749914
472.001922	25699.090759	30.754932
472.667680	25731.305067	30.759949
472.639830	25782.917001	30.764967
473.055296	25824.278167	30.769984
473.510805	25860.116606	30.775002
473.809819	25919.815240	30.780020
474.438155	25961.882753	30.785037
474.344763	26021.952493	30.790055
474.843463	26064.079518	30.795072
475.519447	26112.378068	30.800090
476.120800	26168.242863	30.805108
477.087877	26210.945758	30.810125
477.105642	26261.662173	30.815143
477.576467	26311.291466	30.820160
478.177982	26357.360509	30.825178
478.421023	26405.611547	30.830196
479.154385	26450.198749	30.835213
479.579089	26497.672533	30.840231
480.085366	26543.647417	30.845248
480.787784	26594.645983	30.850266
481.072264	26651.523529	30.855284
482.045687	26684.338553	30.860301
482.366390	26724.910105	30.865319
482.747963	26759.646095	30.870336
483.224076	26797.145297	30.875354
483.463729	26834.283068	30.880372
484.130602	26865.521558	30.885389
484.298071	26920.539475	30.890407
484.880505	26947.423608	30.895424
485.907176	26977.060504	30.900442
486.818102	27012.482330	30.905460
487.450790	27032.734612	30.910477
487.616467	27076.127169	30.915495
487.971973	27107.978971	30.920512
488.589156	27140.254424	30.925530
488.936102	27184.759119	30.930548
489.194023	27219.418685	30.935565
489.210744	27264.709901	30.940583
489.658121	27302.741703	30.945600
490.301121	27340.861136	30.950618
490.495902	27398.184940	30.955636
491.862001	27418.578335	30.960653
492.074936	27469.758134	30.965671
492.653336	27506.623763	30.970688
492.935063	27551.130716	30.975706
492.857669	27607.673765	30.980724
493.753964	27639.500310	30.985741
494.378612	27698.438479	30.990759
494.278005	27755.402209	30.995776
494.915572	27809.433732	31.000794
495.226974	27869.559768	31.005812
496.162700	27910.846337	31.010829
496.497987	27972.088562	31.015847
496.890712	28024.413712	31.020864
497.493969	28064.771418	31.025882
497.992415	28130.990021	31.030900
498.734289	28183.226438	31.035917
499.142488	28235.707390	31.040935
499.667433	28280.914171	31.045952
500.339529	28326.979989	31.050970
500.555331	28382.127069	31.055988
501.688331	28416.603492	31.061005
502.244845	28451.295072	31.066023
502.881782	28505.694790	31.071040
503.524433	28545.062937	31.076058
504.132991	28593.370133	31.081076
504.368572	28621.746285	31.086093
504.881947	28667.612110	31.091111
505.250534	28709.675629	31.096128
505.843520	28743.964313	31.101146
506.024088	28807.234973	31.106164
506.443678	28845.675384	31.111181
506.658257	28892.487028	31.116199
506.977629	28942.808206	31.121216
507.831600	29008.277456	31.126234
507.572312	29055.372852	31.131252
508.584329	29113.816543	31.136269
509.252595	29177.222504	31.141287
509.593588	29231.140267	31.146304
510.246636	29265.322273	31.151322
510.579300	29339.516031	31.156340
511.223476	29377.261220	31.161357
511.952044	29443.058818	31.166375
512.367958	29502.400389	31.171392
513.308027	29535.986621	31.176410
513.768152	29590.523050	31.181428
514.323427	29627.157274	31.186445
515.096991	29680.601192	31.191463
515.238478	29734.231698	31.196480
516.112557	29770.261506	31.201498
516.721074	29819.026392	31.206516
517.123604	29843.184440	31.211533
517.819091	29883.259852	31.216551
518.194791	29910.450898	31.221568
519.152200	29941.732149	31.226586
519.438891	29983.578836	31.231604
519.403540	30010.528774	31.236621
520.455578	30040.337110	31.241639
520.585312	30082.768341	31.246656
521.176986	30112.756946	31.251674
521.511895	30161.586914	31.256692
521.963580	30211.410395	31.261709
522.658431	30236.539680	31.266727
523.222955	30283.123757	31.271744
523.621310	30326.706855	31.276762
523.749308	30382.934781	31.281780
524.039572	30432.135676	31.286797
524.535056	30489.268601	31.291815
525.075340	30536.239085	31.296832
525.397299	30583.340400	31.301850
525.994019	30651.946867	31.306868
526.113922	30703.542764	31.311885
526.952875	30763.869307	31.316903
527.364951	30826.856681	31.321920
527.942298	30882.737524	31.326938
528.486919	30951.536753	31.331956
528.698323	31006.399475	31.336973
529.554855	31072.317750	31.341991
529.992424	31148.031987	31.347008
530.462491	31193.640305	31.352026
531.061634	31274.552909	31.357044
531.375752	31335.785234	31.362061
532.170095	31391.679185	31.367079
532.613795	31442.170028	31.372096
533.426989	31521.489876	31.377114
533.920842	31589.432384	31.382132
534.548041	31653.687045	31.387149
535.293872	31703.065509	31.392167
535.586737	31771.004056	31.397184
536.524896	31827.468782	31.402202
536.794716	31898.437283	31.407220
537.592807	31948.375709	31.412237
538.579118	32003.334409	31.417255
538.864770	32051.278597	31.422272
539.379260	32101.056068	31.427290
539.675419	32160.189811	31.432308
540.114719	32216.425833	31.437325
540.769853	32272.834622	31.442343
541.348202	32334.291812	31.447360
542.001812	32386.003273	31.452378
542.427794	32453.181018	31.457396
542.961733	32508.906989	31.462413
543.871334	32568.527636	31.467431
544.032623	32627.603191	31.472448
545.073730	32671.035472	31.477466
545.472052	32724.007984	31.482484
546.023547	32778.024960	31.487501
546.975321	32828.309660	31.492519
547.559425	32886.186688	31.497536
548.159193	32914.273018	31.502554
548.918291	32973.948294	31.507572
549.657699	33004.781983	31.512589
550.153577	33044.225544	31.517607
550.494527	33092.295950	31.522624
551.366415	33133.220514	31.527642
551.715280	33169.621741	31.532660
552.110485	33205.337010	31.537677
552.803935	33242.678534	31.542695
553.574146	33277.259220	31.547712
554.301548	33299.844385	31.552730
554.863337	33343.736129	31.557748
555.155018	33369.517078	31.562765
555.747193	33406.282483	31.567783
555.841201	33450.592526	31.572800
556.239547	33488.421898	31.577818
556.627164	33527.199718	31.582836
556.775678	33574.082113	31.587853
557.717536	33621.310053	31.592871
557.767627	33677.943173	31.597888
558.270819	33736.962809	31.602906
558.694358	33791.647712	31.607924
558.808836	33852.786076	31.612941
559.535399	33906.342146	31.617959
560.000542	33976.614643	31.622976
560.719904	34041.408668	31.627994
561.044309	34101.667567	31.633012
561.663203	34159.858560	31.638029
562.116371	34220.538355	31.643047
562.849955	34288.836624	31.648064
563.882855	34358.928508	31.653082
564.856140	34415.856421	31.658100
565.167812	34478.198157	31.663117
565.627543	34530.544302	31.668135
566.000532	34602.049359	31.673152
566.408698	34652.788763	31.678170
567.245601	34716.717006	31.683188
567.652964	34779.842341	31.688205
568.218854	34832.903926	31.693223
568.794578	34913.013474	31.698240
569.336841	34973.334011	31.703258
569.570507	35044.797589	31.708276
570.194682	35107.481205	31.713293
570.842519	35185.509998	31.718311
571.423687	35251.006556	31.723328
571.764074	35327.755080	31.728346
572.362447	35395.417245	31.733364
572.870987	35470.172642	31.738381
573.791311	35543.639095	31.743399
574.270368	35615.386305	31.748416
574.882771	35690.993284	31.753434
575.617057	35756.248662	31.758452
576.186007	35831.992799	31.763469
577.287398	35884.571447	31.768487
578.011382	35948.390216	31.773504
579.472165	35987.075044	31.778522
580.875883	36021.651122	31.783540
581.570207	36050.209636	31.788557
581.982159	36084.113362	31.793575
582.921787	36116.292154	31.798592
583.783803	36144.220370	31.803610
584.217510	36179.622834	31.808628
584.604910	36207.354985	31.813645
585.210864	36230.273213	31.818663
585.379721	36269.348758	31.823680
585.758097	36308.206747	31.828698
585.945299	36349.311774	31.833716
586.027257	36398.039804	31.838733
586.481306	36438.198397	31.843751
586.952512	36507.867637	31.848768
587.335218	36561.065600	31.853786
587.359895	36619.864541	31.858804
587.766926	36694.266269	31.863821
588.411563	36768.487047	31.868839
588.863190	36832.104634	31.873856
589.761001	36888.469065	31.878874
590.362810	36972.566281	31.883892
590.490713	37039.091021	31.888909
591.293450	37090.387580	31.893927
591.870247	37154.970290	31.898944
592.544921	37228.209660	31.903962
593.116635	37286.784724	31.908980
593.383795	37367.855670	31.913997
594.381615	37414.850881	31.919015
594.622849	37495.330198	31.924032
594.834131	37555.158637	31.929050
595.732241	37621.331083	31.934068
596.068954	37698.951952	31.939085
596.648072	37754.942511	31.944103
597.376986	37842.535488	31.949120
598.094820	37924.430826	31.954138
598.997954	37968.186038	31.959156
599.637594	38046.225470	31.964173
600.667179	38107.839503	31.969191
601.219073	38190.909127	31.974208
601.564104	38251.320602	31.979226
602.374810	38323.490955	31.984244
602.927361	38386.753337	31.989261
603.724771	38449.410543	31.994279
604.233931	38522.912904	31.999296
604.572923	38595.196966	32.004314
605.421849	38655.103635	32.009332
605.780420	38726.760058	32.014349
606.796033	38784.720639	32.019367
607.519137	38851.043275	32.024384
607.787093	38926.326202	32.029402
608.647802	38983.880597	32.034420
609.049779	39060.767426	32.039437
609.624251	39127.383904	32.044455
610.344970	39200.532128	32.049472
610.797475	39279.033879	32.054490
611.757757	39335.057908	32.059508
612.318215	39403.622015	32.064525
613.010318	39474.203646	32.069543
613.631965	39534.131817	32.074560
614.603503	39604.396355	32.079578
615.202549	39658.697689	32.084596
615.556599	39731.018503	32.089613
616.197237	39791.222148	32.094631
616.776528	39870.201066	32.099648
617.149574	39939.909208	32.104666
617.559418	40004.434962	32.109684
618.097440	40088.999089	32.114701
618.811975	40153.231999	32.119719
619.808853	40225.035107	32.124736
620.327961	40281.475815	32.129754
621.446691	40340.803722	32.134772
622.191129	40402.987157	32.139789
623.270904	40448.928750	32.144807
624.067574	40513.667035	32.149824
624.428205	40581.634113	32.154842
625.092987	40617.916190	32.159860
625.736108	40689.735361	32.164877
626.168590	40739.619820	32.169895
626.827823	40797.882422	32.174912
627.020956	40865.502584	32.179930
627.573001	40917.545834	32.184948
628.171881	40980.632812	32.189965
628.819772	41047.477770	32.194983
629.389319	41107.792196	32.200000
629.762620	41173.653900	32.205018
630.048777	41243.283504	32.210036
631.208966	41310.578289	32.215053
632.285971	41375.967796	32.220071
633.158860	41425.806642	32.225088
633.129041	41490.463913	32.230106
633.881770	41536.979956	32.235124
634.605970	41601.519401	32.240141
635.032043	41650.144707	32.245159
635.595750	41711.207071	32.250176
636.011730	41783.904578	32.255194
636.630073	41839.250932	32.260212
636.748223	41914.406754	32.265229
638.090484	41959.750044	32.270247
638.784026	42029.608927	32.275264
639.438710	42104.260217	32.280282
639.770391	42156.160278	32.285300
640.367282	42215.154275	32.290317
640.891564	42282.213552	32.295335
641.967729	42344.033102	32.300352
642.911488	42398.421378	32.305370
643.991098	42456.796604	32.310388
644.405237	42528.970159	32.315405
645.000201	42591.390898	32.320423
645.646775	42638.003025	32.325440
645.867326	42707.841574	32.330458
646.605038	42760.134031	32.335476
647.061917	42838.404069	32.340493
648.148325	42902.957710	32.345511
648.534262	42951.024828	32.350528
648.774018	43026.556557	32.355546
649.425679	43100.748304	32.360564
650.015017	43175.073763	32.365581
650.274909	43253.927408	32.370599
651.304760	43331.928113	32.375616
651.803678	43409.871608	32.380634
652.276120	43491.393580	32.385652
652.687777	43578.214026	32.390669
653.192314	43666.639119	32.395687
653.907539	43754.013254	32.400704
654.136468	43843.889614	32.405722
655.126754	43927.307483	32.410740
655.585436	44026.343477	32.415757
656.458509	44113.443820	32.420775
657.258973	44198.068715	32.425792
657.729324	44295.074154	32.430810
658.464404	44387.183761	32.435828
659.345412	44481.116696	32.440845
660.167392	44555.983874	32.445863
661.420735	44632.317690	32.450880
661.870042	44723.888912	32.455898
662.592891	44805.201638	32.460916
663.934338	44862.489837	32.465933
664.779536	44928.226985	32.470951
665.340463	44989.682653	32.475968
665.686959	45074.916931	32.480986
666.667900	45140.054620	32.486004
667.011158	45217.273632	32.491021
667.499986	45292.716593	32.496039
667.904379	45364.280771	32.501056
668.173589	45447.420391	32.506074
669.001773	45521.418983	32.511092
669.946459	45607.690400	32.516109
670.679257	45680.530820	32.521127
671.743397	45744.769642	32.526144
672.442362	45818.617091	32.531162
673.211325	45900.034317	32.536180
673.570707	45965.296475	32.541197
674.396562	46048.454186	32.546215
675.176384	46117.423784	32.551232
675.551426	46206.204357	32.556250
675.961467	46271.639191	32.561268
676.625237	46350.009793	32.566285
677.188479	46420.632928	32.571303
678.136849	46506.825778	32.576320
678.305993	46585.215896	32.581338
678.740092	46657.301098	32.586356
679.402793	46731.723334	32.591373
679.965958	46842.856879	32.596391
680.726332	46901.759786	32.601408
681.336419	46988.247529	32.606426
681.954115	47068.318067	32.611444
682.939383	47145.890525	32.616461
683.696395	47224.432513	32.621479
684.162220	47315.022139	32.626496
684.951576	47402.821039	32.631514
685.490846	47487.630235	32.636532
686.449101	47568.341351	32.641549
686.509571	47672.877878	32.646567
687.436372	47753.857073	32.651584
687.992997	47861.063114	32.656602
688.487865	47949.165806	32.661620
689.141824	48047.436053	32.666637
689.982055	48144.375021	32.671655
691.067146	48231.977352	32.676672
691.593836	48332.531111	32.681690
692.179983	48421.846174	32.686708
692.961076	48514.887353	32.691725
693.585773	48616.345375	32.696743
694.717614	48701.305301	32.701760
695.005720	48805.854684	32.706778
695.831868	48896.411308	32.711796
696.755148	48982.016417	32.716813
697.661971	49077.878601	32.721831
698.565026	49163.977357	32.726848
699.089103	49262.786933	32.731866
699.655302	49347.416826	32.736884
700.191006	49452.238352	32.741901
701.029964	49546.415072	32.746919
701.595848	49632.331611	32.751936
702.494202	49733.889346	32.756954
702.665200	49825.802868	32.761972
703.551541	49911.096121	32.766989
704.180901	50022.638426	32.772007
704.757778	50130.864506	32.777024
705.687261	50235.565291	32.782042
706.194950	50335.144236	32.787060
707.000994	50417.310606	32.792077
707.192959	50549.772378	32.797095
707.948244	50655.063227	32.802112
708.858933	50754.912572	32.807130
709.719532	50860.269269	32.812148
710.507432	50973.467967	32.817165
711.219458	51073.936062	32.822183
712.115413	51176.026115	32.827200
712.908893	51267.063631	32.832218
714.478220	51339.380197	32.837236
715.825643	51421.660437	32.842253
716.106909	51508.551468	32.847271
716.836732	51598.378768	32.852288
717.557414	51678.912787	32.857306
718.424872	51771.241736	32.862324
718.869992	51846.607398	32.867341
719.385773	51937.829756	32.872359
720.007157	52036.820733	32.877376
720.739440	52121.353307	32.882394
721.144328	52221.132699	32.887412
721.838460	52311.755679	32.892429
722.442629	52415.615552	32.897447
723.008586	52511.927043	32.902464
723.921769	52600.474778	32.907482
724.566725	52700.817124	32.912500
725.249995	52782.701156	32.917517
725.702618	52884.724999	32.922535
727.050874	52959.190942	32.927552
727.798164	53039.397734	32.932570
728.170496	53124.360528	32.937588
729.202976	53212.436512	32.942605
729.689111	53303.774430	32.947623
730.372662	53390.057856	32.952640
731.042427	53485.422062	32.957658
731.554507	53581.520328	32.962676
732.985246	53651.780526	32.967693
733.519677	53769.898733	32.972711
734.525407	53850.666356	32.977728
735.300156	53932.748604	32.982746
735.830677	54023.918313	32.987764
736.655141	54098.854178	32.992781
737.276285	54184.753421	32.997799
738.040799	54273.743975	33.002816
739.219670	54351.812709	33.007834
739.610563	54447.973162	33.012852
740.530495	54534.431102	33.017869
741.149118	54630.561163	33.022887
741.993518	54720.197607	33.027904
742.660442	54805.896166	33.032922
743.071311	54909.005209	33.037940
743.949296	54999.660881	33.042957
744.529494	55100.866552	33.047975
745.175651	55197.133840	33.052992
746.036394	55292.058338	33.058010
746.621912	55401.661299	33.063028
747.235789	55492.887261	33.068045
747.774293	55601.406074	33.073063
748.562189	55722.748020	33.078080
749.555939	55834.434144	33.083098
750.163959	55933.276510	33.088116
750.850272	56031.007069	33.093133
751.688058	56151.825324	33.098151
752.189154	56259.570473	33.103168
753.257920	56370.994518	33.108186
753.541510	56486.099780	33.113204
754.050348	56601.604486	33.118221
754.738359	56721.060904	33.123239
755.535424	56836.393015	33.128256
756.521287	56942.058869	33.133274
757.840042	57051.259258	33.138292
758.955007	57143.522167	33.143309
760.192847	57250.967815	33.148327
761.419361	57327.208097	33.153344
762.630319	57409.308650	33.158362
763.396952	57492.734019	33.163380
764.511168	57561.442904	33.168397
765.242546	57648.160484	33.173415
765.738012	57745.507671	33.178432
766.612897	57807.849689	33.183450
766.745749	57913.472018	33.188468
767.467434	57991.099896	33.193485
767.970897	58083.209081	33.198503
768.341962	58185.905786	33.203520
769.013886	58284.332278	33.208538
769.707145	58381.574083	33.213556
770.463380	58486.079147	33.218573
771.172430	58599.167498	33.223591
771.711079	58701.219912	33.228608
772.715375	58799.398167	33.233626
773.043041	58910.864057	33.238644
774.174037	59019.727112	33.243661
774.566600	59129.957584	33.248679
775.696570	59230.493229	33.253696
776.750611	59331.269411	33.258714
777.061843	59431.720090	33.263732
777.900447	59530.131509	33.268749
778.587328	59620.334322	33.273767
779.439774	59712.317549	33.278784
780.060349	59821.553620	33.283802
780.565926	59924.900571	33.288820
781.532732	60024.879431	33.293837
782.536073	60138.180649	33.298855
783.240113	60241.224713	33.303872
784.080351	60341.365076	33.308890
784.780130	60438.419875	33.313908
786.039829	60546.126103	33.318925
786.851086	60658.741527	33.323943
787.517916	60751.442682	33.328960
788.316670	60851.712506	33.333978
788.590600	60955.223067	33.338996
789.670986	61049.759558	33.344013
790.627623	61163.478716	33.349031
791.305427	61275.670906	33.354048
792.226881	61382.824423	33.359066
793.538256	61481.002983	33.364084
794.237294	61575.895623	33.369101
794.772140	61686.078657	33.374119
795.095217	61796.278297	33.379136
796.311558	61896.983627	33.384154
796.608445	62027.703847	33.389172
797.173335	62127.677317	33.394189
797.925330	62253.356194	33.399207
798.593278	62382.772344	33.404224
799.827850	62492.951649	33.409242
800.075061	62615.423255	33.414260
800.759598	62734.252387	33.419277
801.884542	62869.695296	33.424295
802.359324	62999.539119	33.429312
803.416221	63122.309852	33.434330
803.905757	63255.041313	33.439348
804.831650	63380.666815	33.444365
806.053365	63504.177410	33.449383
807.435283	63610.015138	33.454400
808.243537	63735.188195	33.459418
808.816821	63851.103083	33.464436
810.072162	63963.006114	33.469453
811.230001	64057.341520	33.474471
812.427472	64175.816209	33.479488
813.301212	64268.575056	33.484506
813.638334	64371.460434	33.489524
815.088548	64477.266079	33.494541
815.594857	64580.813542	33.499559
816.480683	64699.374313	33.504576
817.760705	64785.798026	33.509594
818.415146	64869.373494	33.514612
819.832344	64964.093742	33.519629
820.127282	65062.394148	33.524647
820.639214	65163.680670	33.529664
821.429988	65260.022777	33.534682
822.020306	65374.489569	33.539700
822.818257	65469.074185	33.544717
823.484855	65582.025088	33.549735
823.987174	65695.338759	33.554752
824.973212	65800.791674	33.559770
825.245077	65926.401635	33.564788
826.062688	66035.632101	33.569805
827.316384	66146.731799	33.574823
828.104284	66263.617253	33.579840
828.913573	66371.744612	33.584858
829.621958	66484.522848	33.589876
830.744605	66590.235362	33.594893
831.518156	66705.886653	33.599911
832.069707	66805.992518	33.604928
833.167079	66907.696610	33.609946
833.645525	67021.293280	33.614964
834.398791	67128.087305	33.619981
835.470728	67229.215569	33.624999
836.223151	67343.691725	33.630016
837.427528	67433.634900	33.635034
838.277628	67545.662148	33.640052
839.052499	67651.228848	33.645069
839.843942	67764.600863	33.650087
840.275058	67860.483366	33.655104
841.191554	67973.058265	33.660122
841.786005	68084.744972	33.665140
842.860746	68204.710665	33.670157
843.615745	68319.653236	33.675175
844.216447	68437.858819	33.680192
845.073260	68556.869941	33.685210
845.472209	68678.669543	33.690228
846.587342	68812.882179	33.695245
847.299071	68937.501908	33.700263
847.740577	69069.279546	33.705280
848.767773	69199.842249	33.710298
849.504521	69349.996110	33.715316
849.965991	69474.862649	33.720333
851.094786	69621.021172	33.725351
852.001131	69770.170034	33.730368
852.796497	69908.381339	33.735386
853.852692	70044.109967	33.740404
854.488274	70175.198578	33.745421
855.723989	70309.432420	33.750439
856.598808	70455.107530	33.755456
857.640448	70579.378962	33.760474
858.543230	70715.137213	33.765492
859.392941	70851.587955	33.770509
860.602818	70983.971420	33.775527
861.905564	71114.980955	33.780544
863.215831	71220.072423	33.785562
864.078251	71352.648331	33.790580
864.703493	71462.564703	33.795597
865.787463	71587.815091	33.800615
866.421079	71723.402899	33.805632
867.552031	71835.488696	33.810650
868.317097	71961.261837	33.815668
869.279781	72084.334709	33.820685
870.098714	72196.252604	33.825703
870.841863	72314.348749	33.830720
871.545526	72446.900738	33.835738
872.393112	72562.881679	33.840756
873.432607	72692.009407	33.845773
874.288551	72814.357934	33.850791
875.142345	72937.573820	33.855808
876.006393	73053.251163	33.860826
876.646576	73187.588763	33.865844
877.459448	73318.819126	33.870861
878.701699	73439.286241	33.875879
879.456541	73551.879420	33.880896
880.668612	73672.877680	33.885914
881.620905	73795.677490	33.890932
882.435297	73920.334642	33.895949
883.241903	74043.052409	33.900967
884.063793	74161.955110	33.905984
884.869184	74287.646637	33.911002
886.021129	74417.834843	33.916020
886.555781	74536.837616	33.921037
887.021400	74652.096032	33.926055
888.098345	74782.007903	33.931072
889.034153	74912.601550	33.936090
889.513253	75026.304019	33.941108
890.246399	75154.915216	33.946125
891.172428	75281.490585	33.951143
891.756534	75409.969792	33.956160
892.293010	75542.384932	33.961178
893.253101	75679.214798	33.966196
893.886158	75821.114652	33.971213
895.078962	75957.262760	33.976231
895.903601	76097.513754	33.981248
896.809071	76232.920476	33.986266
897.726757	76364.208823	33.991284
898.753717	76509.728906	33.996301
900.610784	76624.084934	34.001319
901.531799	76748.607831	34.006336
902.749923	76875.251700	34.011354
903.638859	76999.016040	34.016372
904.047110	77130.165391	34.021389
904.704123	77259.655333	34.026407
905.771136	77398.261817	34.031424
906.525636	77514.145358	34.036442
907.804823	77668.517720	34.041460
908.589599	77788.888304	34.046477
909.428698	77937.554321	34.051495
910.250492	78065.459536	34.056512
911.050958	78197.878691	34.061530
911.988217	78336.088704	34.066548
913.128577	78476.321676	34.071565
914.280905	78605.307608	34.076583
915.023632	78737.657291	34.081600
916.219677	78882.260595	34.086618
917.018657	79015.703217	34.091636
917.781463	79148.659245	34.096653
919.120831	79290.154833	34.101671
919.588436	79431.662424	34.106688
920.462997	79575.127824	34.111706
921.750257	79698.752908	34.116724
922.250140	79849.707911	34.121741
923.207015	79988.196927	34.126759
923.969681	80145.391704	34.131776
924.706305	80296.658531	34.136794
925.771987	80438.143316	34.141812
926.037994	80591.514015	34.146829
926.934884	80748.361919	34.151847
927.548923	80904.447927	34.156864
928.576296	81059.094085	34.161882
929.690745	81226.157109	34.166900
930.625505	81385.603098	34.171917
931.804752	81533.794059	34.176935
932.801361	81696.736571	34.181952
933.721285	81851.677914	34.186970
934.915482	82002.191108	34.191988
936.007723	82154.544039	34.197005
937.263379	82305.479272	34.202023
938.156842	82456.437353	34.207040
938.917221	82602.996411	34.212058
940.211787	82762.633082	34.217076
940.755500	82903.555228	34.222093
941.784286	83056.044881	34.227111
942.574802	83225.871129	34.232128
943.552138	83370.172427	34.237146
944.726167	83514.600324	34.242164
945.718024	83663.297946	34.247181
946.829364	83809.376612	34.252199
948.172320	83945.358754	34.257216
948.999945	84083.792930	34.262234
950.190866	84223.793904	34.267252
950.765007	84373.507771	34.272269
952.100994	84501.718891	34.277287
952.548973	84632.854779	34.282304
953.519441	84777.912633	34.287322
954.802920	84907.222890	34.292340
954.975837	85054.343841	34.297357
956.039152	85186.804830	34.302375
956.807770	85322.307872	34.307392
957.461312	85473.262181	34.312410
958.527842	85612.551883	34.317428
959.093684	85763.383370	34.322445
960.376189	85918.545461	34.327463
962.187555	86043.978676	34.332480
962.950074	86205.720173	34.337498
963.967944	86339.656843	34.342516
964.387112	86484.449445	34.347533
965.307282	86639.169998	34.352551
966.041206	86792.941594	34.357568
966.632914	86946.838921	34.362586
967.293742	87106.971009	34.367604
968.281354	87282.324729	34.372621
969.383766	87448.428978	34.377639
970.790069	87609.776537	34.382656
971.894155	87774.971662	34.387674
972.641682	87931.690837	34.392692
973.484257	88112.763270	34.397709
974.758750	88275.301468	34.402727
975.522859	88436.817696	34.407744
976.713759	88616.513997	34.412762
977.955342	88769.158006	34.417780
978.974821	88943.190027	34.422797
980.399398	89094.578317	34.427815
981.570818	89241.010264	34.432832
982.653624	89402.277993	34.437850
983.767904	89545.930602	34.442868
984.517285	89712.248339	34.447885
985.906032	89854.364070	34.452903
986.909541	89999.910853	34.457920
987.723359	90153.691233	34.462938
989.162563	90300.313335	34.467956
989.718912	90459.808334	34.472973
990.820321	90606.253944	34.477991
991.910514	90760.752022	34.483008
992.320757	90913.610381	34.488026
993.471073	91071.055920	34.493044
994.819005	91216.293808	34.498061
995.772063	91372.172785	34.503079
996.842456	91523.305944	34.508096
997.516594	91676.606583	34.513114
998.609898	91844.217755	34.518132
999.470045	92019.697223	34.523149
1000.596630	92168.407596	34.528167
1001.450540	92327.929204	34.533184
1002.032189	92495.224343	34.538202
1003.328814	92646.517084	34.543220
1003.957215	92825.027916	34.548237
1005.331220	92975.525157	34.553255
1006.424787	93141.708638	34.558272
1006.953580	93306.283984	34.563290
1008.069136	93462.839537	34.568308
1008.884699	93651.585044	34.573325
1009.861548	93805.785949	34.578343
1011.512667	93965.579155	34.583360
1012.710626	94140.948629	34.588378
1013.625298	94292.960300	34.593396
1014.386569	94464.220516	34.598413
1015.228551	94620.670457	34.603431
1016.770295	94785.063260	34.608448
1017.157171	94950.578265	34.613466
1018.453692	95097.113860	34.618484
1019.306315	95262.908539	34.623501
1020.211027	95421.119193	34.628519
1021.036416	95575.894303	34.633536
1022.062553	95740.948315	34.638554
1023.415105	95890.460688	34.643572
1024.193327	96056.273006	34.648589
1024.945736	96217.058496	34.653607
1026.002931	96382.440833	34.658624
1027.057924	96557.249865	34.663642
1027.828908	96712.946277	34.668660
1028.823312	96886.970071	34.673677
1030.104329	97056.193917	34.678695
1032.391693	97201.287134	34.683712
1033.545442	97347.777403	34.688730
1034.588266	97505.598815	34.693748
1035.769280	97661.347436	34.698765
1036.988402	97798.720438	34.703783
1037.979061	97936.125585	34.708800
1038.403515	98096.470989	34.713818
1039.700091	98264.320491	34.718836
1040.646849	98419.004713	34.723853
1041.267480	98568.926286	34.728871
1042.264164	98743.475452	34.733888
1043.173125	98920.104060	34.738906
1044.097826	99076.891385	34.743924
1044.813526	99262.587995	34.748941
1045.624633	99426.746072	34.753959
1046.920363	99609.893206	34.758976
1047.690112	99783.784361	34.763994
1049.196644	99953.414761	34.769012
1050.104520	100141.352536	34.774029
1050.701797	100332.964235	34.779047
1051.636565	100518.406015	34.784064
1052.759600	100711.984999	34.789082
1054.021926	100898.331456	34.794100
1054.894824	101095.645634	34.799117
1055.517774	101290.305558	34.804135
1056.742591	101483.449433	34.809152
1057.800701	101699.155017	34.814170
1058.649163	101886.817949	34.819188
1059.573316	102086.505550	34.824205
1060.201084	102300.615791	34.829223
1061.518896	102497.221555	34.834240
1062.654270	102713.821993	34.839258
1063.598632	102923.085924	34.844276
1064.370623	103135.001275	34.849293
1065.469488	103356.399804	34.854311
1066.911824	103570.145539	34.859328
1067.546975	103798.082700	34.864346
1069.065309	103996.224405	34.869364
1070.442440	104211.068933	34.874381
1071.437096	104420.526644	34.879399
1072.348512	104637.566429	34.884416
1073.359702	104848.392552	34.889434
1074.628882	105066.712898	34.894452
1075.724685	105281.036493	34.899469
1076.310479	105490.709610	34.904487
1077.913767	105708.587574	34.909504
1079.485656	105910.388672	34.914522
1081.457281	106107.186160	34.919540
1082.446152	106301.209162	34.924557
1083.751386	106502.146977	34.929575
1084.928940	106689.353394	34.934592
1085.891514	106881.497955	34.939610
1087.872746	107038.267036	34.944628
1088.769142	107232.628786	34.949645
1089.681737	107413.336226	34.954663
1090.853335	107587.720172	34.959680
1091.696996	107762.007418	34.964698
1092.255113	107928.921006	34.969716
1093.406441	108103.489003	34.974733
1093.835556	108296.580474	34.979751
1095.004268	108471.869955	34.984768
1096.086531	108652.228500	34.989786
1097.337795	108832.079061	34.994804
1098.574555	109014.238428	34.999821
1099.928737	109200.280786	35.004839
1101.068120	109376.239673	35.009856
1101.701842	109571.396477	35.014874
1102.647129	109751.506379	35.019892
1103.698890	109951.283455	35.024909
1104.995836	110137.709078	35.029927
1105.869227	110326.612556	35.034944
1107.038422	110531.403166	35.039962
1108.042443	110733.955245	35.044980
1109.599520	110913.566572	35.049997
1110.674185	111123.367995	35.055015
1112.072679	111318.297166	35.060032
1112.802495	111508.765293	35.065050
1113.825822	111711.093466	35.070068
1114.995040	111919.631366	35.075085
1115.833541	112118.446227	35.080103
1117.117843	112318.595032	35.085120
1117.809791	112530.953288	35.090138
1119.097556	112739.807227	35.095156
1120.280690	112940.610657	35.100173
1121.207218	113157.976810	35.105191
1122.793687	113365.126700	35.110208
1123.855326	113572.415457	35.115226
1125.077098	113793.158254	35.120244
1125.884171	114011.678315	35.125261
1126.486730	114244.954496	35.130279
1128.370044	114442.714206	35.135296
1130.241870	114625.426992	35.140314
1131.785816	114826.894000	35.145332
1133.241206	115026.198063	35.150349
1135.282445	115192.873353	35.155367
1136.617725	115383.749713	35.160384
1137.859782	115555.195902	35.165402
1138.874444	115729.797263	35.170420
1140.097749	115896.713123	35.175437
1140.857552	116081.671407	35.180455
1141.840515	116263.198703	35.185472
1142.575623	116444.932785	35.190490
1143.130493	116634.540179	35.195508
1144.454027	116825.238236	35.200525
1144.914962	117042.420121	35.205543
1146.139944	117232.326336	35.210560
1147.536843	117430.035383	35.215578
1148.482510	117653.096740	35.220596
1149.847552	117833.481435	35.225613
1150.691486	118050.481111	35.230631
1152.146831	118242.459287	35.235648
1153.240375	118462.892523	35.240666
1154.469112	118639.212323	35.245684
1155.762729	118842.903288	35.250701
1156.586296	119066.806757	35.255719
1158.089819	119253.588850	35.260736
1159.055008	119458.390059	35.265754
1159.835928	119677.946607	35.270772
1161.137280	119868.871405	35.275789
1161.832516	120092.449249	35.280807
1162.979279	120311.924884	35.285824
1164.283775	120525.344669	35.290842
1165.461245	120740.586311	35.295860
1166.893249	120935.019186	35.300877
1167.712751	121149.017793	35.305895
1169.080465	121336.836802	35.310912
1170.124055	121530.704193	35.315930
1171.079515	121739.007805	35.320948
1172.487924	121930.853516	35.325965
1173.522559	122139.767827	35.330983
1174.533937	122351.754079	35.336000
1175.466561	122562.525670	35.341018
1176.273018	122770.113543	35.346036
1178.005693	122988.156648	35.351053
1178.455791	123204.664294	35.356071
1179.790541	123418.569047	35.361088
1180.810485	123650.788402	35.366106
1182.198547	123865.283187	35.371124
1183.599226	124084.377629	35.376141
1184.887776	124321.284803	35.381159
1185.770013	124545.588027	35.386176
1187.331924	124757.880804	35.391194
1188.343766	124977.324792	35.396212
1190.420267	125179.460522	35.401229
1191.662499	125409.147580	35.406247
1193.160435	125619.999599	35.411264
1194.582734	125828.913870	35.416282
1195.660841	126039.939514	35.421300
1196.973874	126251.929071	35.426317
1197.951690	126471.795123	35.431335
1198.926978	126688.938320	35.436352
1199.929316	126903.695913	35.441370
1201.177307	127123.344653	35.446388
1202.384564	127353.331071	35.451405
1203.154910	127588.017413	35.456423
1204.336575	127810.368972	35.461440
1205.552000	128047.076623	35.466458
1206.194779	128275.718271	35.471476
1207.718352	128506.244162	35.476493
1208.700641	128754.200048	35.481511
1210.156023	128992.649820	35.486528
1211.248533	129236.003123	35.491546
1212.409609	129475.405111	35.496564
1213.768603	129716.956387	35.501581
1214.837266	129957.733579	35.506599
1216.213905	130207.334470	35.511616
1217.648280	130440.259750	35.516634
1218.695957	130679.410859	35.521652
1220.261867	130920.138750	35.526669
1221.621753	131164.616457	35.531687
1222.772039	131397.278854	35.536704
1223.679499	131650.682676	35.541722
1224.812496	131902.200621	35.546740
1226.349828	132125.475020	35.551757
1227.445997	132381.578898	35.556775
1228.555104	132629.303725	35.561792
1230.153744	132870.573491	35.566810
1231.179012	133128.609215	35.571828
1232.597529	133360.329048	35.576845
1233.938538	133600.759506	35.581863
1235.529876	133827.079313	35.586880
1236.881337	134054.758698	35.591898
1238.120225	134301.194705	35.596916
1239.703303	134532.249321	35.601933
1240.478975	134773.136817	35.606951
1241.355340	135019.384604	35.611968
1242.566069	135254.410407	35.616986
1243.639525	135504.926940	35.622004
1245.101212	135737.734312	35.627021
1246.063519	135990.275962	35.632039
1247.351874	136242.131865	35.637056
1248.699326	136481.505061	35.642074
1249.247098	136713.963126	35.647092
1250.691812	136956.239631	35.652109
1251.593243	137185.435142	35.657127
1252.936487	137429.646256	35.662144
1254.341856	137672.809310	35.667162
1255.173467	137924.537947	35.672180
1256.911398	138159.282012	35.677197
1258.227041	138411.111944	35.682215
1259.311766	138640.578870	35.687232
1260.792821	138900.512156	35.692250
1261.827349	139138.307987	35.697268
1263.265752	139376.406532	35.702285
1264.246399	139642.526691	35.707303
1265.310071	139908.609892	35.712320
1266.567508	140157.926750	35.717338
1268.114458	140402.075256	35.722356
1269.997419	140638.537117	35.727373
1271.664798	140897.149093	35.732391
1272.777587	141143.847083	35.737408
1274.236156	141381.195648	35.742426
1275.324090	141634.025528	35.747444
1276.647006	141877.181863	35.752461
1277.686207	142133.231453	35.757479
1278.888770	142374.065397	35.762496
1280.240884	142631.347724	35.767514
1281.980374	142878.766283	35.772532
1283.464726	143126.216043	35.777549
1284.842570	143369.411882	35.782567
1286.301620	143610.706640	35.787584
1287.792778	143851.756844	35.792602
1288.949713	144104.339808	35.797620
1290.081246	144360.339893	35.802637
1291.424696	144600.633439	35.807655
1292.390670	144851.008810	35.812672
1294.233480	145093.429778	35.817690
1295.399899	145346.945828	35.822708
1296.244491	145602.634563	35.827725
1297.503259	145851.320157	35.832743
1298.773071	146119.179811	35.837760
1299.829199	146371.630799	35.842778
1301.029092	146640.355566	35.847796
1302.062043	146898.470053	35.852813
1303.245374	147181.582543	35.857831
1304.096288	147444.435909	35.862848
1305.774775	147721.916310	35.867866
1306.821561	147999.503107	35.872884
1308.021573	148280.960140	35.877901
1309.761005	148553.338668	35.882919
1310.768466	148838.801325	35.887936
1312.311872	149115.972270	35.892954
1313.443649	149390.968460	35.897972
1314.844184	149676.829357	35.902989
1316.144304	149953.653635	35.908007
1317.462397	150225.860508	35.913024
1319.294299	150505.251857	35.918042
1320.155352	150795.687514	35.923060
1321.638475	151071.411911	35.928077
1323.262356	151342.371632	35.933095
1324.864147	151626.476788	35.938112
1326.297475	151899.843769	35.943130
1327.302200	152181.312082	35.948148
1328.847720	152434.244149	35.953165
1330.219810	152727.223267	35.958183
1331.482139	152996.466219	35.963200
1333.038874	153263.404784	35.968218
1334.262288	153540.686856	35.973236
1335.312946	153811.467219	35.978253
1336.561448	154085.704965	35.983271
1337.608239	154347.788510	35.988288
1339.338656	154603.127171	35.993306
1341.352200	154858.864752	35.998324
1342.688095	155103.502873	36.003341
1344.292348	155360.173868	36.008359
1345.274275	155622.061150	36.013376
1346.262652	155867.294203	36.018394
1347.570849	156131.211348	36.023412
1348.802196	156392.986544	36.028429
1349.712713	156665.674711	36.033447
1351.110418	156929.937650	36.038464
1352.391654	157196.149718	36.043482
1354.066475	157460.827150	36.048500
1355.997730	157714.935290	36.053517
1357.419722	157979.518383	36.058535
1358.598468	158261.179882	36.063552
1359.440802	158523.718427	36.068570
1360.746611	158812.441352	36.073588
1361.420919	159092.365238	36.078605
1363.243670	159367.648837	36.083623
1364.928803	159640.698952	36.088640
1366.227413	159922.136675	36.093658
1367.181557	160220.594414	36.098676
1368.541729	160497.750781	36.103693
1369.996917	160784.687099	36.108711
1371.377398	161074.555609	36.113728
1372.587134	161373.487052	36.118746
1373.844383	161678.591141	36.123764
1374.983655	161982.372183	36.128781
1376.612903	162262.566215	36.133799
1377.918825	162569.724086	36.138816
1379.661205	162874.528564	36.143834
1380.693590	163189.728860	36.148852
1381.969019	163491.049869	36.153869
1383.916526	163783.305018	36.158887
1384.791830	164103.308451	36.163904
1386.535464	164413.718958	36.168922
1387.771350	164714.839548	36.173940
1389.633544	165023.217650	36.178957
1390.747512	165317.930068	36.183975
1392.175710	165631.928658	36.188992
1393.711448	165940.684439	36.194010
1395.962147	166230.876313	36.199028
1397.925324	166511.944218	36.204045
1400.271708	166771.165401	36.209063
1401.884706	167060.630670	36.214080
1404.087804	167306.492764	36.219098
1405.452663	167572.529296	36.224116
1406.588279	167834.075547	36.229133
1408.100671	168096.830013	36.234151
1409.108988	168361.052276	36.239168
1410.024614	168621.827443	36.244186
1411.199433	168894.742436	36.249204
1412.356850	169166.862588	36.254221
1413.909647	169432.549389	36.259239
1414.757367	169712.565631	36.264256
1416.292518	169998.053301	36.269274
1417.403110	170279.856900	36.274292
1418.680032	170575.668938	36.279309
1420.280370	170863.473424	36.284327
1421.302350	171159.648570	36.289344
1422.620427	171456.017870	36.294362
1424.116011	171733.439882	36.299380
1425.103198	172036.998994	36.304397
1426.462081	172345.358873	36.309415
1427.889230	172639.141813	36.314432
1429.911410	172918.628601	36.319450
1431.528050	173218.969911	36.324468
1432.790004	173499.017092	36.329485
1434.201886	173775.779884	36.334503
1435.445809	174045.097589	36.339520
1436.844934	174323.109328	36.344538
1437.898596	174604.111147	36.349556
1438.833473	174904.499580	36.354573
1440.067797	175189.789737	36.359591
1441.338853	175499.707652	36.364608
1442.601807	175806.202468	36.369626
1444.234738	176121.458142	36.374644
1445.062835	176448.270299	36.379661
1446.581964	176760.871184	36.384679
1448.453397	177061.080443	36.389696
1450.214314	177383.874238	36.394714
1451.550155	177707.641367	36.399732
1453.001419	178024.944505	36.404749
1454.805282	178335.680925	36.409767
1455.788905	178671.137598	36.414784
1457.244093	179006.620239	36.419802
1458.440754	179314.429737	36.424820
1459.415144	179667.446840	36.429837
1460.977029	179998.108416	36.434855
1462.293651	180346.669806	36.439872
1463.727451	180673.447883	36.444890
1465.204937	181033.981135	36.449908
1466.516397	181390.990578	36.454925
1468.374917	181733.786000	36.459943
1469.212441	182106.070937	36.464960
1470.918329	182454.823524	36.469978
1472.508595	182815.426722	36.474996
1473.588977	183175.075764	36.480013
1475.128204	183546.734755	36.485031
1476.572249	183931.904235	36.490048
1478.150231	184301.759771	36.495066
1479.978167	184655.444168	36.500084
1481.966146	185014.587773	36.505101
1484.275186	185376.092434	36.510119
1485.792442	185722.752458	36.515136
1487.449608	186082.757380	36.520154
1489.599876	186408.640319	36.525172
1490.983372	186755.849371	36.530189
1492.824765	187093.249292	36.535207
1494.311166	187431.217577	36.540224
1495.746426	187770.897268	36.545242
1497.406035	188104.842607	36.550260
1498.123697	188462.682378	36.555277
1499.285938	188805.396350	36.560295
1500.870757	189146.925605	36.565312
1502.250393	189504.815016	36.570330
1503.522072	189868.995259	36.575348
1504.927438	190220.030158	36.580365
1506.328909	190577.871839	36.585383
1508.115698	190938.635253	36.590400
1509.528352	191298.916774	36.595418
1511.237992	191649.567299	36.600436
1512.873828	192005.462157	36.605453
1514.754094	192342.327924	36.610471
1517.052470	192683.341171	36.615488
1518.634967	193032.472071	36.620506
1520.600046	193354.946554	36.625524
1521.871420	193692.821663	36.630541
1523.530504	194031.332878	36.635559
1524.842063	194375.273233	36.640576
1525.835173	194708.655088	36.645594
1527.637811	195048.836624	36.650612
1528.521768	195396.725177	36.655629
1530.059303	195732.269696	36.660647
1531.408348	196076.314809	36.665664
1532.886132	196402.072046	36.670682
1534.481311	196737.003004	36.675700
1535.606338	197083.642289	36.680717
1537.765181	197390.668016	36.685735
1539.354058	197717.581586	36.690752
1540.864959	198046.566353	36.695770
1542.384494	198374.129439	36.700788
1543.277076	198717.375266	36.705805
1544.899763	199056.706361	36.710823
1546.662348	199405.956961	36.715840
1547.905527	199738.790394	36.720858
1549.294205	200092.067398	36.725876
1550.680668	200448.000089	36.730893
1551.932318	200804.325077	36.735911
1553.371552	201172.542689	36.740928
1554.713658	201546.478918	36.745946
1556.142916	201914.130801	36.750964
1557.470102	202294.028092	36.755981
1559.191750	202665.190670	36.760999
1560.719181	203039.764523	36.766016
1562.176734	203427.556340	36.771034
1564.375999	203803.953236	36.776052
1565.323138	204191.249356	36.781069
1566.685653	204574.657267	36.786087
1568.276232	204974.218065	36.791104
1569.865400	205375.546141	36.796122
1572.057234	205756.004652	36.801140
1573.971942	206142.300696	36.806157
1576.161619	206525.963141	36.811175
1577.550766	206907.309065	36.816192
1578.697790	207280.900733	36.821210
1580.853601	207662.377867	36.826228
1582.559966	208066.456205	36.831245
1584.140562	208431.830175	36.836263
1585.734363	208827.385642	36.841280
1587.486703	209201.788172	36.846298
1589.409492	209588.684202	36.851316
1590.294513	209975.766031	36.856333
1591.856650	210359.855597	36.861351
1593.185155	210745.128328	36.866368
1594.725653	211149.135343	36.871386
1596.345288	211549.728227	36.876404
1597.411114	211942.021038	36.881421
1598.804792	212353.207081	36.886439
1600.324333	212774.380466	36.891456
1601.677340	213200.764260	36.896474
1603.211359	213620.441016	36.901492
1605.223754	214046.339221	36.906509
1607.183642	214450.457761	36.911527
1609.164045	214847.133484	36.916544
1610.879397	215266.483386	36.921562
1613.091797	215665.410170	36.926580
1614.888760	216062.807225	36.931597
1616.410408	216461.241920	36.936615
1618.351701	216856.688386	36.941632
1619.277601	217266.526663	36.946650
1621.274292	217664.557933	36.951668
1622.664087	218069.573782	36.956685
1624.126655	218505.640875	36.961703
1625.371782	218943.650646	36.966720
1626.915477	219352.379941	36.971738
1628.492611	219755.187632	36.976756
1630.092606	220178.540362	36.981773
1631.428058	220608.237304	36.986791
1633.352872	221013.888048	36.991808
1635.294051	221419.512285	36.996826
1637.099165	221827.573419	37.001844
1638.806882	222234.712447	37.006861
1640.608466	222617.200647	37.011879
1642.232927	223001.217966	37.016896
1643.798819	223394.999533	37.021914
1645.467438	223781.298215	37.026932
1646.376571	224170.695257	37.031949
1647.881987	224555.017001	37.036967
1649.472390	224960.661508	37.041984
1650.612781	225367.854864	37.047002
1652.270686	225772.043310	37.052020
1654.545320	226177.655370	37.057037
1656.509703	226582.786606	37.062055
1658.470236	226969.784368	37.067072
1660.001086	227380.095165	37.072090
1662.577961	227755.462162	37.077108
1664.734925	228148.578013	37.082125
1666.649659	228535.842222	37.087143
1668.518577	228913.869485	37.092160
1670.248135	229296.467498	37.097178
1671.792466	229665.355595	37.102196
1673.351640	230061.166727	37.107213
1674.371609	230448.050809	37.112231
1676.177841	230842.197836	37.117248
1677.689541	231236.699393	37.122266
1679.096248	231639.169813	37.127284
1680.505384	232041.920385	37.132301
1681.781710	232464.582880	37.137319
1682.912639	232878.685069	37.142336
1684.431109	233310.835401	37.147354
1686.401746	233733.564774	37.152372
1688.373553	234168.055861	37.157389
1689.915350	234591.620378	37.162407
1691.985556	235007.529268	37.167424
1693.627825	235427.269241	37.172442
1695.447477	235848.860735	37.177460
1697.037706	236280.931165	37.182477
1698.435362	236721.289977	37.187495
1700.474411	237157.937069	37.192512
1701.465184	237612.691786	37.197530
1703.496365	238043.982608	37.202548
1705.471422	238473.607193	37.207565
1707.231195	238912.031934	37.212583
1709.179071	239347.581642	37.217600
1710.654537	239792.659807	37.222618
1712.678682	240241.484161	37.227636
1714.322529	240666.773712	37.232653
1715.754670	241129.872057	37.237671
1717.588410	241550.737512	37.242688
1719.202002	242003.646939	37.247706
1721.493845	242445.014361	37.252724
1722.786951	242897.343414	37.257741
1724.251593	243343.396057	37.262759
1726.483976	243786.376191	37.267776
1728.182435	244233.052366	37.272794
1729.650253	244672.857898	37.277812
1731.437601	245140.122453	37.282829
1732.762687	245593.721273	37.287847
1734.818708	246045.447471	37.292864
1736.855128	246496.390140	37.297882
1738.709479	246941.495510	37.302900
1740.949031	247383.210224	37.307917
1741.869334	247848.361381	37.312935
1744.235015	248284.518729	37.317952
1745.349613	248741.459377	37.322970
1746.806706	249186.887408	37.327988
1748.538052	249643.829081	37.333005
1750.064312	250111.296571	37.338023
1752.160620	250571.760955	37.343040
1754.020760	251029.470482	37.348058
1755.811801	251475.531890	37.353076
1757.461546	251907.848577	37.358093
1758.958031	252341.969158	37.363111
1760.768405	252783.989508	37.368128
1762.252778	253238.689372	37.373146
1764.380394	253671.208134	37.378164
1766.426337	254090.200785	37.383181
1768.800035	254529.233571	37.388199
1770.811165	254931.644211	37.393216
1772.603169	255370.036788	37.398234
1774.465146	255798.231363	37.403252
1776.214679	256220.932192	37.408269
1778.742053	256643.174643	37.413287
1780.821280	257050.909716	37.418304
1782.337721	257481.753144	37.423322
1784.006989	257903.908976	37.428340
1785.179575	258315.045617	37.433357
1786.902998	258765.542802	37.438375
1788.980537	259191.492868	37.443392
1790.409823	259636.678623	37.448410
1792.368940	260052.232966	37.453428
1794.396830	260488.276453	37.458445
1795.715502	260927.917191	37.463463
1797.721572	261373.388883	37.468480
1798.728203	261827.205271	37.473498
1800.532258	262281.982383	37.478516
1802.236937	262730.602798	37.483533
1803.723427	263201.258342	37.488551
1805.495233	263670.723524	37.493568
1807.025843	264153.234795	37.498586
1808.628723	264628.189168	37.503604
1810.308756	265122.792694	37.508621
1811.781688	265606.862364	37.513639
1813.866280	266109.273569	37.518656
1815.327065	266603.531294	37.523674
1817.326454	267098.639720	37.528692
1819.190998	267587.266787	37.533709
1820.634871	268105.074821	37.538727
1822.540157	268613.711926	37.543744
1824.581012	269121.437045	37.548762
1825.985880	269636.582611	37.553780
1828.144454	270139.257382	37.558797
1829.902984	270665.876356	37.563815
1831.858033	271176.814001	37.568832
1833.832814	271697.248399	37.573850
1835.743901	272220.740906	37.578868
1837.621485	272740.173699	37.583885
1839.138808	273270.054856	37.588903
1840.945554	273793.790728	37.593920
1842.815956	274323.256220	37.598938
1844.240245	274857.366833	37.603956
1846.131652	275387.157149	37.608973
1847.822239	275929.630046	37.613991
1850.352331	276452.047775	37.619008
1852.644606	276969.778809	37.624026
1854.913850	277488.173022	37.629044
1857.252837	278000.889887	37.634061
1858.759654	278522.125657	37.639079
1861.098339	279050.919881	37.644096
1862.841482	279570.742497	37.649114
1864.388285	280085.769836	37.654132
1866.306536	280599.972567	37.659149
1867.979253	281124.375293	37.664167
1869.798008	281633.181165	37.669184
1871.405954	282166.076021	37.674202
1873.368344	282691.798405	37.679220
1875.233024	283213.877558	37.684237
1876.973390	283725.256215	37.689255
1879.100541	284213.631975	37.694272
1881.643703	284724.367237	37.699290
1882.869319	285220.026640	37.704308
1884.932660	285710.135885	37.709325
1887.020717	286202.728893	37.714343
1888.724464	286688.931868	37.719360
1890.717413	287195.762110	37.724378
1892.400365	287681.177956	37.729396
1894.827671	288181.252788	37.734413
1896.952175	288671.571148	37.739431
1899.106524	289148.445928	37.744448
1901.436568	289629.227234	37.749466
1903.817028	290105.375668	37.754484
1905.579182	290581.421244	37.759501
1907.053274	291079.687215	37.764519
1908.821833	291560.732149	37.769536
1910.575240	292054.960530	37.774554
1912.460044	292558.969792	37.779572
1914.014829	293043.676688	37.784589
1915.620923	293564.720518	37.789607
1917.049263	294082.057699	37.794624
1919.110776	294595.478284	37.799642
1920.630530	295124.378175	37.804660
1922.323634	295654.237678	37.809677
1923.837467	296202.183268	37.814695
1925.786568	296743.476038	37.819712
1928.083176	297267.894681	37.824730
1929.949017	297816.104547	37.829748
1932.135112	298359.382261	37.834765
1933.653475	298917.498635	37.839783
1935.340903	299464.586603	37.844800
1937.055442	300028.531814	37.849818
1938.717748	300605.689679	37.854836
1940.177862	301174.318443	37.859853
1942.412732	301764.785475	37.864871
1944.807936	302325.964199	37.869888
1947.128635	302908.562258	37.874906
1949.206487	303483.399797	37.879924
1951.923825	304041.747048	37.884941
1953.641122	304617.881618	37.889959
1956.002966	305179.201368	37.894976
1958.393938	305727.103279	37.899994
1960.016661	306286.963483	37.905012
1962.614053	306852.221267	37.910029
1964.341008	307410.965121	37.915047
1966.247106	307970.742483	37.920064
1968.454042	308525.895277	37.925082
1970.006861	309094.231255	37.930100
1971.751039	309655.497192	37.935117
1973.932410	310220.699731	37.940135
1975.623484	310790.575823	37.945152
1977.864178	311364.801430	37.950170
1979.134625	311949.442570	37.955188
1981.726918	312510.396500	37.960205
1984.639766	313060.526188	37.965223
1987.310304	313616.659658	37.970240
1989.551887	314154.829863	37.975258
1991.194140	314687.559183	37.980276
1993.116901	315239.868022	37.985293
1995.068922	315788.384268	37.990311
1997.263247	316335.586792	37.995328
2000.883047	316853.931716	38.000346
2003.468704	317366.907766	38.005364
2005.616328	317872.943907	38.010381
2007.284703	318383.219926	38.015399
2008.914032	318903.274881	38.020416
2010.797660	319407.362918	38.025434
2011.855691	319923.035395	38.030452
2013.888749	320426.202607	38.035469
2015.812839	320942.714845	38.040487
2016.986005	321438.297220	38.045504
2019.125366	321955.959580	38.050522
2020.742719	322456.564828	38.055540
2022.598674	322975.053084	38.060557
2024.597701	323498.084000	38.065575
2026.801441	324007.467480	38.070592
2028.661648	324531.173073	38.075610
2030.172844	325077.783231	38.080628
2031.847067	325615.703741	38.085645
2033.721899	326173.162157	38.090663
2034.915728	326735.983549	38.095680
2036.853672	327295.808067	38.100698
2038.401405	327896.847684	38.105716
2039.900153	328470.190088	38.110733
2042.022996	329063.836591	38.115751
2043.575411	329675.774753	38.120768
2045.375943	330288.097242	38.125786
2046.902184	330915.792841	38.130804
2049.173197	331544.298147	38.135821
2051.811084	332157.097467	38.140839
2053.603407	332797.625375	38.145856
2055.616093	333425.137032	38.150874
2057.634330	334073.660734	38.155892
2059.969983	334719.966675	38.160909
2062.061772	335366.914494	38.165927
2063.875564	336012.123489	38.170944
2065.955663	336674.948999	38.175962
2068.346909	337335.988810	38.180980
2071.469265	337960.777474	38.185997
2073.836462	338627.491257	38.191015
2075.869696	339258.384003	38.196032
2078.478124	339873.385533	38.201050
2081.998767	340477.365154	38.206068
2084.437851	341102.558583	38.211085
2086.389899	341714.727089	38.216103
2088.394442	342329.062365	38.221120
2091.091242	342936.600389	38.226138
2092.987888	343556.674636	38.231156
2094.829048	344171.496225	38.236173
2097.343807	344764.269597	38.241191
2099.146974	345379.919729	38.246208
2101.385263	345983.637482	38.251226
2103.116263	346608.649141	38.256244
2105.005128	347212.662707	38.261261
2106.959789	347838.991695	38.266279
2109.203422	348458.006160	38.271296
2111.702737	349059.052680	38.276314
2113.659157	349675.255756	38.281332
2115.612784	350297.820920	38.286349
2117.762306	350921.994799	38.291367
2119.413531	351555.961802	38.296384
2121.506940	352192.689144	38.301402
2123.591084	352816.415974	38.306420
2125.794838	353451.305273	38.311437
2127.883185	354069.684591	38.316455
2129.719001	354711.188663	38.321472
2131.821938	355350.761396	38.326490
2133.780871	355994.839719	38.331508
2136.552194	356616.495482	38.336525
2138.895899	357249.757901	38.341543
2141.050433	357871.649154	38.346560
2143.205511	358509.262599	38.351578
2145.216473	359148.919872	38.356596
2147.341483	359793.572212	38.361613
2149.422410	360431.980122	38.366631
2151.465427	361045.037809	38.371648
2154.523931	361630.847384	38.376666
2157.007636	362235.416363	38.381684
2158.683209	362827.195782	38.386701
2160.531609	363429.035302	38.391719
2161.897621	364034.319424	38.396736
2163.712934	364649.870922	38.401754
2165.578025	365255.053904	38.406772
2167.462020	365897.516422	38.411789
2169.654305	366538.851948	38.416807
2171.195457	367186.144125	38.421824
2173.336877	367840.759004	38.426842
2175.795301	368484.960564	38.431860
2177.766919	369135.243277	38.436877
2179.838465	369784.407484	38.441895
2181.660966	370466.931970	38.446912
2184.055432	371131.593900	38.451930
2186.002510	371808.720970	38.456948
2188.354243	372481.609031	38.461965
2190.780741	373148.384990	38.466983
2192.603860	373848.550212	38.472000
2195.004179	374525.982946	38.477018
2197.422474	375210.653495	38.482036
2199.870887	375898.729717	38.487053
2202.236935	376587.719104	38.492071
2204.352118	377293.550573	38.497088
2206.640351	377972.076827	38.502106
2208.834928	378673.403747	38.507124
2210.733500	379362.136245	38.512141
2213.923020	380058.528602	38.517159
2216.023466	380761.096212	38.522176
2218.435993	381441.156135	38.527194
2220.407074	382139.861981	38.532212
2222.816174	382838.354218	38.537229
2225.393356	383533.127416	38.542247
2227.409597	384232.441109	38.547264
2229.628773	384939.211577	38.552282
2231.935932	385639.106522	38.557300
2233.833073	386350.387254	38.562317
2236.229963	387065.423649	38.567335
2238.035677	387775.876685	38.572352
2240.492913	388476.572607	38.577370
2242.757630	389202.484474	38.582388
2245.148778	389918.978880	38.587405
2247.279399	390637.756109	38.592423
2248.977647	391364.928253	38.597440
2251.480129	392085.106422	38.602458
2253.954587	392822.509619	38.607476
2256.543752	393549.939705	38.612493
2259.131500	394267.745961	38.617511
2261.141489	394980.383696	38.622528
2263.773620	395695.208566	38.627546
2266.706155	396409.536022	38.632564
2269.555463	397113.215147	38.637581
2271.862101	397816.840381	38.642599
2274.283234	398511.027378	38.647616
2276.605536	399220.876529	38.652634
2278.962892	399904.523585	38.657652
2281.150607	400604.249537	38.662669
2283.354992	401294.174001	38.667687
2285.529726	401988.850963	38.672704
2288.073357	402678.179492	38.677722
2290.661554	403371.411701	38.682740
2292.354596	404065.788172	38.687757
2294.666385	404762.148675	38.692775
2296.486080	405466.529190	38.697792
2298.458271	406169.371955	38.702810
2300.301522	406875.765387	38.707828
2302.917898	407578.238298	38.712845
2305.669593	408243.884124	38.717863
2307.669566	408925.091954	38.722880
2309.717098	409611.215124	38.727898
2311.602528	410293.750385	38.732916
2313.781939	410995.016917	38.737933
2315.471731	411689.328950	38.742951
2317.198419	412409.303051	38.747968
2319.293140	413137.834862	38.752986
2321.472448	413855.592817	38.758004
2323.316686	414595.372452	38.763021
2325.627618	415336.751378	38.768039
2327.291323	416095.363053	38.773056
2329.496929	416844.137678	38.778074
2331.589420	417619.755378	38.783092
2333.597268	418404.556954	38.788109
2336.188101	419187.972192	38.793127
2338.322131	419978.453515	38.798144
2340.973763	420760.670823	38.803162
2343.999259	421538.750702	38.808180
2346.434354	422342.048372	38.813197
2349.583594	423113.779266	38.818215
2352.187433	423890.716188	38.823232
2355.019813	424677.490971	38.828250
2357.412662	425449.932217	38.833268
2359.807110	426238.451015	38.838285
2362.253185	427013.872343	38.843303
2365.018918	427787.494769	38.848320
2367.496897	428563.367683	38.853338
2369.888740	429337.204676	38.858356
2371.976552	430136.633664	38.863373
2374.574753	430904.968845	38.868391
2377.333379	431682.010708	38.873408
2379.266231	432476.374810	38.878426
2381.720590	433248.403682	38.883444
2383.718225	434047.057403	38.888461
2386.332650	434842.038903	38.893479
2387.951900	435646.470527	38.898496
2390.293695	436458.448328	38.903514
2392.474682	437257.416738	38.908532
2394.742424	438079.623643	38.913549
2397.284183	438908.689059	38.918567
2399.529334	439741.619177	38.923584
2401.739582	440566.579426	38.928602
2404.007148	441398.230113	38.933620
2406.089286	442245.516104	38.938637
2408.907903	443076.406212	38.943655
2411.296538	443927.271258	38.948672
2413.549840	444767.045506	38.953690
2416.447013	445614.321036	38.958708
2418.928884	446462.087510	38.963725
2421.337840	447303.559923	38.968743
2424.612245	448135.295984	38.973760
2427.324122	448971.847699	38.978778
2430.367021	449788.635348	38.983796
2432.461754	450612.477729	38.988813
2435.129626	451446.107264	38.993831
2437.575705	452267.551409	38.998848
2440.289353	453093.724097	39.003866
2442.457367	453904.124752	39.008884
2444.743198	454723.880853	39.013901
2447.487742	455558.194172	39.018919
2449.699952	456384.470880	39.023936
2452.017911	457209.989150	39.028954
2454.457724	458032.066418	39.033972
2456.626666	458858.554137	39.038989
2459.140557	459702.192143	39.044007
2461.508621	460530.601411	39.049024
2463.460164	461360.410355	39.054042
2466.078238	462171.117814	39.059060
2467.925804	462991.170300	39.064077
2470.385049	463807.044325	39.069095
2472.909590	464621.408214	39.074112
2474.843186	465438.818136	39.079130
2477.665097	466262.567689	39.084148
2480.142651	467090.382657	39.089165
2482.379218	467930.786308	39.094183
2485.378370	468741.666471	39.099200
2487.585211	469573.968663	39.104218
2490.867124	470384.480648	39.109236
2493.600181	471235.927421	39.114253
2496.317944	472052.020199	39.119271
2498.753454	472883.938983	39.124288
2500.984772	473732.477054	39.129306
2503.883351	474551.211386	39.134324
2506.042696	475393.321053	39.139341
2508.281461	476225.933299	39.144359
2510.552448	477070.020339	39.149376
2513.617032	477900.300118	39.154394
2515.989808	478750.102894	39.159412
2518.430874	479605.916161	39.164429
2520.851064	480457.501162	39.169447
2523.705315	481314.277775	39.174464
2525.620040	482177.582539	39.179482
2528.326139	483054.047197	39.184500
2530.474004	483928.743621	39.189517
2532.715431	484802.978249	39.194535
2535.253091	485688.582749	39.199552
2537.608932	486585.836009	39.204570
2540.145042	487491.950208	39.209588
2542.426389	488387.054942	39.214605
2545.169942	489284.612609	39.219623
2547.888035	490203.228195	39.224640
2550.543433	491109.187298	39.229658
2553.355324	492012.095722	39.234676
2556.212449	492904.149324	39.239693
2558.766788	493818.109466	39.244711
2561.589541	494736.821470	39.249728
2564.072821	495654.581517	39.254746
2566.965272	496548.156068	39.259764
2569.102806	497474.200972	39.264781
2571.637417	498397.052242	39.269799
2574.066700	499312.202009	39.274816
2576.303128	500248.219179	39.279834
2579.081203	501175.771405	39.284852
2581.660952	502099.773853	39.289869
2584.121428	503044.222977	39.294887
2586.676406	503981.037227	39.299904
2588.796810	504920.895939	39.304922
2591.376408	505876.056979	39.309940
2593.977222	506841.244308	39.314957
2596.685987	507783.363064	39.319975
2598.956562	508747.382413	39.324992
2601.552451	509704.282485	39.330010
2604.335813	510678.084889	39.335028
2606.625564	511637.995677	39.340045
2608.949089	512603.841983	39.345063
2611.524295	513591.111760	39.350080
2615.113234	514550.834343	39.355098
2618.573249	515503.715786	39.360116
2621.529076	516458.537693	39.365133
2623.896988	517415.010932	39.370151
2627.212241	518353.733293	39.375168
2629.766135	519310.513009	39.380186
2632.457408	520246.452376	39.385204
2635.026932	521175.351952	39.390221
2637.622715	522106.810777	39.395239
2639.998100	523027.871863	39.400256
2642.373124	523938.802855	39.405274
2645.108358	524837.077811	39.410292
2647.624430	525745.862309	39.415309
2649.814824	526645.580302	39.420327
2652.327773	527558.839105	39.425344
2654.342950	528501.432481	39.430362
2656.468660	529428.791476	39.435380
2658.807289	530370.709832	39.440397
2661.388979	531340.370763	39.445415
2664.018429	532298.531934	39.450432
2666.270630	533274.312409	39.455450
2668.617802	534249.810957	39.460468
2670.917111	535229.681718	39.465485
2673.331695	536229.600009	39.470503
2676.322598	537230.964846	39.475520
2678.743964	538243.727408	39.480538
2681.702850	539245.460846	39.485556
2684.688765	540262.768452	39.490573
2687.312348	541275.686041	39.495591
2690.441584	542303.440526	39.500608
2693.346024	543327.535487	39.505626
2696.219814	544350.152752	39.510644
2699.231875	545359.896955	39.515661
2702.090053	546381.714937	39.520679
2705.832780	547392.751099	39.525696
2708.278472	548411.671891	39.530714
2710.942778	549422.587119	39.535732
2714.398341	550428.873228	39.540749
2717.140205	551445.610676	39.545767
2720.487318	552440.605752	39.550784
2723.134601	553452.886131	39.555802
2725.903773	554456.274617	39.560820
2728.498111	555452.329674	39.565837
2730.858388	556459.859054	39.570855
2734.216925	557447.549215	39.575872
2737.741494	558439.812622	39.580890
2740.468730	559441.730998	39.585908
2743.154048	560431.723494	39.590925
2746.310871	561422.669730	39.595943
2749.018030	562412.108772	39.600960
2751.588726	563418.273574	39.605978
2754.191088	564409.538780	39.610996
2756.779321	565414.693664	39.616013
2759.053988	566411.084429	39.621031
2762.122864	567421.529493	39.626048
2764.607356	568423.907822	39.631066
2767.407475	569428.315312	39.636084
2769.988851	570445.984763	39.641101
2772.557524	571460.663908	39.646119
2775.419919	572492.230833	39.651136
2777.540578	573530.411706	39.656154
2780.213963	574566.409029	39.661172
2782.876108	575590.730712	39.666189
2786.368272	576619.549315	39.671207
2790.190419	577622.789803	39.676224
2793.246127	578652.065474	39.681242
2795.708589	579663.142929	39.686260
2798.473707	580693.652302	39.691277
2800.717295	581722.807610	39.696295
2803.981203	582750.254485	39.701312
2806.574616	583768.899403	39.706330
2809.602015	584793.456041	39.711348
2813.008832	585800.013286	39.716365
2815.630857	586828.828313	39.721383
2818.299835	587843.059490	39.726400
2820.293291	588869.248098	39.731418
2823.177375	589897.207705	39.736436
2825.827836	590884.569159	39.741453
2828.261617	591904.511785	39.746471
2830.851577	592895.676576	39.751488
2832.982005	593904.974256	39.756506
2835.395894	594914.339836	39.761524
2837.780287	595961.350128	39.766541
2840.096863	597003.569593	39.771559
2842.587987	598046.319085	39.776576
2844.872757	599121.015605	39.781594
2847.547534	600190.891254	39.786612
2850.312072	601274.074667	39.791629
2852.886267	602376.115989	39.796647
2856.135955	603474.586319	39.801664
2858.208228	604592.620685	39.806682
2861.266567	605714.488478	39.811700
2864.321515	606842.903940	39.816717
2866.828745	607982.608977	39.821735
2869.786695	609119.322932	39.826752
2872.516059	610281.179885	39.831770
2875.139210	611426.973970	39.836788
2877.863041	612606.954099	39.841805
2880.163370	613788.480429	39.846823
2882.936971	614975.305616	39.851840
2886.450033	616173.235042	39.856858
2889.716012	617351.322908	39.861876
2893.872225	618524.388169	39.866893
2897.099690	619707.530585	39.871911
2900.049402	620887.141683	39.876928
2903.068315	622081.009767	39.881946
2905.737838	623273.005187	39.886964
2908.942024	624444.291974	39.891981
2911.468634	625645.295009	39.896999
2914.664196	626833.762888	39.902016
2918.476773	628010.407228	39.907034
2921.935657	629170.645912	39.912052
2925.642352	630340.606934	39.917069
2928.688337	631513.844070	39.922087
2931.715627	632667.429279	39.927104
2934.668350	633852.007303	39.932122
2936.936142	635019.939768	39.937140
2939.620223	636185.526937	39.942157
2942.680255	637372.834146	39.947175
2945.303314	638548.000185	39.952192
2948.302546	639737.442746	39.957210
2951.037337	640923.598636	39.962228
2954.134874	642111.853151	39.967245
2956.585539	643304.217179	39.972263
2959.704459	644498.028044	39.977280
2962.806940	645703.422056	39.982298
2965.403910	646893.696470	39.987316
2968.478369	648103.547320	39.992333
2971.387812	649307.297702	39.997351
2974.588954	650534.384895	40.002368
2977.282789	651732.496380	40.007386
2979.793752	652953.469356	40.012404
2982.874568	654177.088953	40.017421
2985.627644	655412.569679	40.022439
2988.590573	656654.985576	40.027456
2991.505782	657894.811931	40.032474
2994.239397	659139.193502	40.037492
2997.390562	660370.350367	40.042509
3000.378813	661602.872521	40.047527
3003.571546	662853.426840	40.052544
3006.739154	664098.596945	40.057562
3009.678631	665344.291165	40.062580
3012.873217	666591.275169	40.067597
3015.661791	667851.649276	40.072615
3018.611415	669079.390599	40.077632
3021.395476	670300.633215	40.082650
3024.000929	671528.164956	40.087668
3026.917295	672734.995231	40.092685
3030.144229	673953.107437	40.097703
3033.533985	675152.637589	40.102720
3037.017367	676352.396548	40.107738
3040.216669	677563.183326	40.112756
3043.464434	678758.843940	40.117773
3046.264377	679970.029304	40.122791
3049.506326	681186.896547	40.127808
3053.088915	682376.866774	40.132826
3055.905258	683593.684922	40.137844
3058.877423	684812.749791	40.142861
3061.552768	686029.317073	40.147879
3064.474277	687248.362872	40.152896
3067.173699	688503.526849	40.157914
3069.414280	689737.940484	40.162932
3072.669134	691002.644322	40.167949
3075.612654	692269.802378	40.172967
3078.328094	693532.700186	40.177984
3081.613346	694811.847779	40.183002
3084.753262	696090.885204	40.188020
3088.287785	697371.756592	40.193037
3091.139191	698659.597516	40.198055
3095.260734	699922.792920	40.203072
3099.211589	701195.800506	40.208090
3102.361347	702475.844037	40.213108
3105.680078	703730.195341	40.218125
3109.112144	704997.777627	40.223143
3112.428104	706274.757290	40.228160
3115.959156	707535.312118	40.233178
3119.410381	708783.856512	40.238196
3122.571891	710043.312394	40.243213
3125.479654	711298.068928	40.248231
3128.446365	712544.362443	40.253248
3131.774956	713815.316365	40.258266
3134.674332	715075.013153	40.263284
3138.151126	716331.655706	40.268301
3140.927209	717607.971253	40.273319
3143.795281	718891.598623	40.278336
3147.168703	720165.151077	40.283354
3149.909034	721435.151362	40.288372
3153.306482	722728.341060	40.293389
3156.261072	724009.287715	40.298407
3159.560504	725300.757274	40.303424
3163.559767	726562.151269	40.308442
3166.574401	727834.239220	40.313460
3169.857767	729104.405450	40.318477
3173.007868	730387.835654	40.323495
3175.884018	731685.534138	40.328512
3179.304778	732952.756262	40.333530
3182.139854	734251.286015	40.338548
3185.368443	735536.308947	40.343565
3188.150990	736829.494430	40.348583
3191.441009	738124.362471	40.353600
3195.510021	739399.842016	40.358618
3198.600481	740676.019015	40.363636
3201.981755	741962.649727	40.368653
3205.271026	743253.526536	40.373671
3208.135185	744540.563443	40.378688
3211.154657	745826.476958	40.383706
3214.187840	747140.725849	40.388724
3217.538481	748419.749990	40.393741
3220.537110	749726.569793	40.398759
3223.501765	751028.198474	40.403776
3226.553745	752328.559790	40.408794
3228.929237	753660.589668	40.413812
3232.042670	754955.670830	40.418829
3235.375383	756246.705728	40.423847
3238.593863	757508.786144	40.428864
3241.906721	758793.338416	40.433882
3244.939053	760085.399259	40.438900
3248.170367	761347.235871	40.443917
3251.377246	762639.571335	40.448935
3254.234963	763943.255637	40.453952
3257.191482	765234.794219	40.458970
3260.344297	766540.439270	40.463988
3263.559451	767868.760741	40.469005
3266.596858	769178.143857	40.474023
3269.551469	770507.119741	40.479040
3272.863595	771854.425094	40.484058
3276.003556	773185.199987	40.489076
3279.314442	774534.326216	40.494093
3282.726846	775893.699693	40.499111
3285.541254	777274.380614	40.504128
3289.002722	778641.486131	40.509146
3292.075438	780010.510110	40.514164
3295.871835	781393.734221	40.519181
3299.047156	782774.588146	40.524199
3301.776502	784183.462693	40.529216
3305.010755	785572.504088	40.534234
3307.978274	787001.879751	40.539252
3311.511124	788422.835069	40.544269
3314.885965	789850.886809	40.549287
3318.477923	791277.880609	40.554304
3322.062291	792706.793400	40.559322
3325.249913	794140.528834	40.564340
3328.437465	795578.723776	40.569357
3331.577553	797038.474309	40.574375
3334.481858	798498.252858	40.579392
3337.930696	799939.865920	40.584410
3341.393444	801424.199000	40.589428
3344.873543	802908.211212	40.594445
3348.284724	804385.898426	40.599463
3351.275786	805864.902817	40.604480
3355.069701	807339.739689	40.609498
3358.332618	808832.875549	40.614516
3361.549525	810331.557569	40.619533
3364.678495	811838.573391	40.624551
3367.718784	813327.435325	40.629568
3371.121703	814830.172675	40.634586
3374.171512	816363.985561	40.639604
3377.372337	817879.748212	40.644621
3381.180908	819402.486880	40.649639
3385.146609	820916.652833	40.654656
3388.932006	822422.891796	40.659674
3392.723792	823943.177348	40.664692
3395.897353	825443.511688	40.669709
3399.340336	826960.671208	40.674727
3402.507110	828475.624118	40.679744
3406.072528	829988.844436	40.684762
3409.418687	831515.246084	40.689780
3412.693070	833038.621658	40.694797
3416.263251	834559.057621	40.699815
3419.523281	836088.388845	40.704832
3423.220266	837595.379326	40.709850
3426.851857	839108.693784	40.714868
3430.389094	840640.689723	40.719885
3433.614893	842151.160052	40.724903
3436.961932	843691.548941	40.729920
3440.563494	845189.416142	40.734938
3444.043869	846711.349382	40.739956
3447.135814	848240.462381	40.744973
3450.835687	849745.004353	40.749991
3454.030378	851279.577186	40.755008
3457.603574	852772.491148	40.760013
3460.885027	854236.340013	40.765018
3464.004643	855647.411065	40.770023
3467.472896	856992.227263	40.775028
3470.431151	858274.474686	40.780032
3473.535098	859473.755243	40.785037
3476.524125	860623.904781	40.790042
3479.410529	861676.624990	40.795047
3482.795675	862658.892579	40.800052
3484.819176	863594.084094	40.805056
3487.651713	864439.004416	40.810061
3490.489453	865227.737111	40.815066
3492.543262	865963.057285	40.820071
3495.517421	866592.824687	40.825076
3497.915381	867172.301626	40.830080
3500.181838	867688.413316	40.835085
3501.812900	868153.108456	40.840090
3503.339981	868561.261156	40.845095
3504.790098	868909.576552	40.850100
3506.066441	869223.329494	40.855104
3507.569986	869473.133569	40.860109
3508.745625	869705.502968	40.865114
3509.683517	869880.614468	40.870119
3511.151740	870012.231422	40.875124
3511.859837	870137.271149	40.880128
3513.007345	870203.397441	40.885133
3513.698426	870243.091852	40.890138
3514.322304	870268.912848	40.895143
3515.082382	870252.961532	40.900148
3515.462680	870216.003493	40.905152
3515.938201	870161.552596	40.910157
3516.590294	870086.293719	40.915162
3517.217212	869986.278332	40.920167
3517.719786	869877.154472	40.925172
3517.724821	869744.223772	40.930176
3518.491575	869600.191997	40.935181
3518.913615	869445.240599	40.940186
3519.254477	869278.354236	40.945191
3519.333385	869071.302191	40.950196
3519.666165	868885.372291	40.955200
3520.082399	868660.672729	40.960205
3520.192024	868439.997291	40.965210
3520.566981	868214.608029	40.970215
3520.574787	867972.855926	40.975220
3520.078730	867720.783818	40.980224
3520.545343	867468.639742	40.985229
3520.929869	867216.692938	40.990234
3520.952257	866952.846316	40.995239
3521.001417	866658.867090	41.000244
3521.026579	866390.817978	41.005248
3521.320369	866097.742720	41.010253
3521.227276	865816.571048	41.015258
3521.299920	865527.099658	41.020263
3521.654307	865236.401945	41.025268
3521.585600	864935.556252	41.030272
3521.461018	864630.720318	41.035277
3521.624030	864318.726954	41.040282
3521.166526	864018.677336	41.045287
3521.204253	863698.022525	41.050292
3521.335989	863390.068946	41.055296
3521.379773	863066.755365	41.060301
3521.293028	862755.111719	41.065306
3521.307369	862433.713639	41.070311
3521.191061	862109.500644	41.075316
3520.919836	861793.171454	41.080320
3520.949628	861475.415010	41.085325
3521.157791	861155.959592	41.090330
3520.996130	860829.741315	41.095335
3521.190135	860497.514846	41.100340
3520.948548	860187.127068	41.105344
3520.711751	859853.186005	41.110349
3520.852509	859534.824164	41.115354
3520.714162	859220.868895	41.120359
3520.631120	858882.764320	41.125364
3520.488944	858574.613107	41.130368
3520.584764	858250.355243	41.135373
3520.276118	857927.508955	41.140378
3520.061440	857607.646388	41.145383
3520.525078	857284.055362	41.150388
3520.328287	856967.075575	41.155392
3520.097133	856644.149215	41.160397
3519.900663	856318.864660	41.165402
3519.669870	856000.283724	41.170407
3519.722018	855687.771247	41.175412
3519.383540	855371.024771	41.180416
3519.611065	855039.179176	41.185421
3519.367196	854728.029646	41.190426
3519.223960	854427.361190	41.195431
3519.778457	854100.376032	41.200436
3519.262418	853794.870776	41.205440
3519.160561	853471.270633	41.210445
3519.103386	853167.314015	41.215450
3519.126199	852845.802770	41.220455
3518.926108	852530.251484	41.225460
3518.514021	852229.228690	41.230464
3518.601056	851914.377907	41.235469
3518.347172	851614.175770	41.240474
3518.466053	851319.838797	41.245479
3518.454012	851013.334675	41.250484
3518.363464	850707.802460	41.255488
3518.382911	850417.140611	41.260493
3518.452626	850111.260589	41.265498
3518.171908	849809.027766	41.270503
3518.039253	849500.813193	41.275508
3517.606610	849213.677057	41.280512
3517.868593	848907.511658	41.285517
3517.220333	848619.214601	41.290522
3517.364768	848329.506987	41.295527
3517.135655	848037.411401	41.300532
3517.275473	847763.172141	41.305536
3517.270416	847458.149389	41.310541
3517.213415	847171.540059	41.315546
3516.878422	846892.565553	41.320551
3517.061313	846615.637649	41.325556
3516.857961	846322.970811	41.330560
3516.828278	846039.619467	41.335565
3516.879156	845763.260697	41.340570
3516.465267	845476.243067	41.345575
3516.673330	845202.075972	41.350580
3516.558131	844930.972506	41.355584
3516.450236	844637.724288	41.360589
3515.887538	844369.400367	41.365594
3515.884493	844092.294848	41.370599
3516.100477	843822.746917	41.375604
3516.041540	843552.111383	41.380608
3515.736627	843279.066842	41.385613
3515.894467	843022.659442	41.390618
3515.475448	842760.046238	41.395623
3515.582934	842490.313239	41.400628
3515.466758	842236.503775	41.405632
3515.388865	841973.899398	41.410637
3515.151209	841706.335813	41.415642
3514.878022	841457.739643	41.420647
3515.282133	841198.730636	41.425652
3514.606783	840937.840253	41.430656
3515.073881	840694.360281	41.435661
3514.701725	840428.374846	41.440666
3514.490462	840188.938580	41.445671
3514.515750	839925.452203	41.450676
3513.998713	839685.901070	41.455680
3514.382760	839455.169631	41.460685
3514.267306	839203.532265	41.465690
3514.095421	838957.554206	41.470695
3514.067094	838728.377032	41.475700
3514.055348	838483.037471	41.480704
3514.046840	838231.490647	41.485709
3513.775070	838000.473198	41.490714
3513.639516	837772.450670	41.495719
3513.946213	837533.122461	41.500724
3513.724788	837304.853439	41.505728
3513.765122	837078.046190	41.510733
3513.698940	836839.583260	41.515738
3513.386980	836606.569903	41.520743
3512.793762	836379.158990	41.525748
3512.964063	836164.647516	41.530752
3512.822162	835943.639072	41.535757
3513.064867	835705.620184	41.540762
3513.190683	835497.244754	41.545767
3513.044231	835269.769869	41.550772
3512.804620	835049.674435	41.555776
3512.807824	834832.851505	41.560781
3512.690143	834612.623427	41.565786
3512.425680	834390.751893	41.570791
3512.791823	834178.339288	41.575796
3512.398521	833951.591023	41.580800
3512.394368	833742.985041	41.585805
3512.605928	833525.595596	41.590810
3512.321932	833327.619190	41.595815
3512.486658	833102.165448	41.600820
3512.094454	832903.412502	41.605824
3511.945839	832674.332608	41.610829
3512.120245	832482.115646	41.615834
3512.013327	832272.795450	41.620839
3512.259790	832062.970691	41.625844
3511.980160	831861.969265	41.630848
3511.861029	831657.466996	41.635853
3512.084984	831447.528366	41.640858
3511.603044	831244.294081	41.645863
3511.525806	831037.909084	41.650868
3511.502454	830858.231665	41.655872
3511.355436	830651.992479	41.660877
3511.100480	830457.441289	41.665882
3511.051313	830265.391011	41.670887
3511.360602	830082.412757	41.675892
3511.109710	829882.518041	41.680896
3510.911718	829688.667426	41.685901
3511.300471	829494.616676	41.690906
3510.965343	829314.166208	41.695911
3511.120422	829118.481350	41.700916
3510.644972	828934.916041	41.705920
3510.706203	828751.403781	41.710925
3510.389287	828564.869793	41.715930
3510.495158	828382.805957	41.720935
3510.661743	828204.392571	41.725940
3510.179344	828022.562226	41.730944
3510.125258	827840.900660	41.735949
3510.087782	827673.992335	41.740954
3510.188409	827500.360620	41.745959
3510.337899	827314.447348	41.750964
3510.326479	827147.814612	41.755968
3509.940874	826969.556311	41.760973
3510.119088	826795.844280	41.765978
3509.813838	826617.709835	41.770983
3509.857580	826465.911826	41.775988
3509.684706	826285.008905	41.780992
3509.526641	826130.058665	41.785997
3509.847895	825961.532129	41.791002
3509.578517	825790.800661	41.796007
3509.654430	825625.777229	41.801012
3509.611452	825466.880985	41.806016
3509.572693	825299.961408	41.811021
3509.409687	825145.331049	41.816026
3509.202647	824978.235449	41.821031
3509.267561	824813.095665	41.826036
3508.873327	824665.191247	41.831040
3508.730788	824507.901960	41.836045
3509.123516	824354.090615	41.841050
3508.740078	824205.147152	41.846055
3508.974866	824028.320747	41.851060
3509.223556	823900.490845	41.856064
3508.953058	823751.176194	41.861069
3508.969734	823591.833678	41.866074
3508.828038	823443.371194	41.871079
3508.906158	823286.896830	41.876084
3508.836396	823131.763726	41.881088
3508.907160	822987.902584	41.886093
3508.928166	822840.084528	41.891098
3508.850377	822685.871645	41.896103
3508.734028	822524.422000	41.901108
3508.531929	822396.441619	41.906112
3508.499871	822249.352866	41.911117
3508.303061	822095.928533	41.916122
3508.299157	821958.318937	41.921127
3508.498261	821814.215485	41.926132
3508.504786	821669.602482	41.931136
3508.222113	821531.247191	41.936141
3508.347221	821386.021399	41.941146
3507.896863	821257.179283	41.946151
3507.845274	821106.447946	41.951156
3507.616374	820980.303844	41.956160
3507.956379	820842.663399	41.961165
3507.850610	820715.368639	41.966170
3507.739747	820585.038620	41.971175
3507.753558	820444.703587	41.976180
3507.526636	820317.029708	41.981184
3507.573763	820183.729883	41.986189
3507.629743	820063.246611	41.991194
3507.700941	819929.154784	41.996199
3507.507297	819805.967622	42.001204
3507.469824	819675.069400	42.006208
3507.551709	819551.342780	42.011213
3507.696824	819410.181314	42.016218
3507.136681	819299.426618	42.021223
3507.305538	819165.792739	42.026228
3507.115296	819050.323633	42.031232
3507.415723	818930.122203	42.036237
3507.322493	818796.866702	42.041242
3506.853681	818676.934247	42.046247
3507.247443	818551.522561	42.051252
3507.298053	818432.821678	42.056256
3506.923772	818305.378264	42.061261
3507.169194	818191.290941	42.066266
3507.065952	818079.070193	42.071271
3507.124363	817951.157166	42.076276
3506.773350	817846.462569	42.081280
3506.756412	817726.487568	42.086285
3506.857134	817609.085482	42.091290
3506.643679	817507.936411	42.096295
3506.499186	817391.256231	42.101300
3506.518401	817289.331230	42.106304
3506.654611	817178.279786	42.111309
3506.777623	817060.179037	42.116314
3506.443672	816950.327242	42.121319
3506.346343	816833.874367	42.126324
3506.470253	816734.616346	42.131328
3506.392652	816616.296029	42.136333
3506.474312	816525.169073	42.141338
3506.495489	816417.502198	42.146343
3506.174931	816301.860221	42.151348
3505.981206	816208.130403	42.156352
3506.152284	816094.264428	42.161357
3506.140029	815997.172296	42.166362
3506.043184	815909.151085	42.171367
3506.134891	815803.617175	42.176372
3506.091724	815712.793543	42.181376
3505.748688	815597.975559	42.186381
3505.790189	815500.083924	42.191386
3505.839755	815393.718075	42.196391
3505.780598	815296.819421	42.201396
3505.612398	815215.411650	42.206400
3505.548427	815116.846239	42.211405
3505.587127	815017.332028	42.216410
3505.393846	814940.528309	42.221415
3505.333757	814835.591866	42.226420
3505.493719	814755.838503	42.231424
3505.530257	814667.093446	42.236429
3505.653047	814576.374054	42.241434
3505.163422	814482.130193	42.246439
3505.606937	814402.374916	42.251444
3505.255373	814308.791541	42.256448
3505.333433	814223.609043	42.261453
3505.488737	814131.849807	42.266458
3505.111637	814052.519423	42.271463
3505.374584	813957.654487	42.276468
3505.308906	813866.074970	42.281472
3505.181327	813792.039142	42.286477
3505.022700	813703.460485	42.291482
3504.716702	813615.296786	42.296487
3505.085585	813537.992635	42.301492
3504.992357	813456.061438	42.306496
3505.026996	813388.117218	42.311501
3505.145187	813302.083774	42.316506
3504.661446	813225.161400	42.321511
3505.154649	813139.358017	42.326516
3505.082792	813057.467449	42.331520
3505.484993	812967.807066	42.336525
3505.294175	812879.614789	42.341530
3504.664300	812804.328238	42.346535
3504.910017	812717.482559	42.351540
3504.831286	812654.154453	42.356544
3504.919525	812566.255038	42.361549
3504.983719	812485.951760	42.366554
3504.800470	812402.748905	42.371559
3504.629808	812330.614756	42.376564
3504.974653	812247.371996	42.381568
3504.893563	812174.584550	42.386573
3504.774178	812088.623795	42.391578
3504.593372	812012.960508	42.396583
3504.955602	811927.163338	42.401588
3504.729970	811861.745308	42.406592
3504.683649	811789.388937	42.411597
3504.623369	811711.301714	42.416602
3504.670540	811647.992452	42.421607
3504.766558	811576.982233	42.426612
3504.330393	811502.923172	42.431616
3504.291874	811429.336767	42.436621
3504.468942	811366.346457	42.441626
3504.341158	811298.163023	42.446631
3504.440086	811217.202017	42.451636
3504.187597	811152.075549	42.456640
3503.864063	811083.971204	42.461645
3504.138286	811025.126659	42.466650
3503.810930	810966.723695	42.471655
3503.864339	810912.373553	42.476660
3504.119164	810840.398460	42.481664
3504.213688	810778.004300	42.486669
3504.350999	810710.898334	42.491674
3504.240374	810647.507726	42.496679
3504.066731	810572.562221	42.501684
3503.835951	810505.661867	42.506688
3503.948786	810446.152846	42.511693
3503.935476	810394.651775	42.516698
3503.933194	810327.418003	42.521703
3503.744489	810251.834380	42.526708
3503.725463	810204.106210	42.531712
3503.730106	810156.520825	42.536717
3503.683968	810098.064068	42.541722
3503.453618	810057.720629	42.546727
3504.055672	809988.472705	42.551732
3503.829448	809932.102484	42.556736
3503.528312	809864.766341	42.561741
3503.557338	809809.725287	42.566746
3503.590142	809764.435917	42.571751
3503.492326	809698.583911	42.576756
3503.784234	809640.312586	42.581760
3503.630047	809592.749420	42.586765
3503.956646	809523.297091	42.591770
3503.714645	809469.327148	42.596775
3504.003938	809401.006968	42.601780
3503.734333	809353.020036	42.606784
3503.492851	809303.802831	42.611789
3503.730120	809240.341803	42.616794
3503.763652	809198.675479	42.621799
3503.680536	809129.286622	42.626804
3503.777575	809078.394588	42.631808
3503.794303	809017.712583	42.636813
3503.894351	808951.183577	42.641818
3503.839435	808903.256142	42.646823
3503.710972	808839.851630	42.651828
3503.963830	808791.382561	42.656832
3503.702295	808725.303035	42.661837
3503.857608	808670.182960	42.666842
3503.666812	808615.854704	42.671847
3503.511949	808558.726104	42.676852
3503.494693	808500.986145	42.681856
3503.533268	808460.637963	42.686861
3503.832050	808393.090419	42.691866
3503.129550	808345.265730	42.696871
3503.754858	808299.427864	42.701876
3503.833655	808236.424779	42.706880
3503.550446	808175.000367	42.711885
3504.079662	808128.785025	42.716890
3503.633692	808064.543238	42.721895
3503.735201	808007.367794	42.726900
3503.792408	807943.189048	42.731904
3503.374369	807894.137814	42.736909
3503.805193	807839.946104	42.741914
3503.216707	807792.392891	42.746919
3503.409008	807736.131660	42.751924
3503.269157	807692.915956	42.756928
3503.201523	807646.991766	42.761933
3503.851979	807598.889965	42.766938
3503.419245	807553.858700	42.771943
3503.692637	807499.690228	42.776948
3503.772270	807445.357140	42.781952
3503.476824	807397.752910	42.786957
3503.830145	807324.302732	42.791962
3503.663736	807285.158007	42.796967
3503.415918	807216.708346	42.801972
3503.447116	807163.263484	42.806977
3503.402545	807104.388594	42.811981
3503.280327	807064.107683	42.816986
3503.072273	807018.496571	42.821991
3503.585489	806961.980005	42.826996
3503.476564	806911.007698	42.832001
3503.127782	806873.998917	42.837005
3503.465412	806812.754178	42.842010
3503.062583	806775.851828	42.847015
3502.946750	806721.986468	42.852020
3503.227304	806674.723605	42.857025
3503.121744	806639.830856	42.862029
3503.093360	806576.143700	42.867034
3503.002439	806539.924176	42.872039
3503.046175	806493.385517	42.877044
3503.369366	806451.899899	42.882049
3502.859662	806413.689320	42.887053
3503.375945	806367.022936	42.892058
3503.137587	806313.566813	42.897063
3503.385696	806272.288610	42.902068
3503.421571	806226.583012	42.907073
3503.186726	806175.135630	42.912077
3503.196405	806134.582355	42.917082
3502.955775	806078.378822	42.922087
3503.020370	806034.285373	42.927092
3503.013287	805992.900417	42.932097
3502.714403	805957.839896	42.937101
3502.960432	805914.010006	42.942106
3503.087777	805883.831573	42.947111
3502.911042	805844.533205	42.952116
3502.864337	805800.946958	42.957121
3502.935332	805761.656347	42.962125
3502.964977	805708.935965	42.967130
3502.868059	805682.618539	42.972135
3502.919067	805631.904606	42.977140
3502.954927	805589.480339	42.982145
3502.849005	805560.025448	42.987149
3503.106123	805501.675570	42.992154
3502.848765	805464.300837	42.997159
3502.822030	805416.687614	43.002164
3502.801347	805379.616716	43.007169
3502.908355	805336.590686	43.012173
3503.069394	805296.252731	43.017178
3502.645115	805261.552591	43.022183
3502.771742	805206.556491	43.027188
3502.748467	805179.930760	43.032193
3502.761750	805140.597062	43.037197
3502.827871	805108.365549	43.042202
3503.111124	805077.373222	43.047207
3503.224764	805017.130214	43.052212
3502.934652	805004.132591	43.057217
3502.762418	804949.379834	43.062221
3502.936640	804909.920221	43.067226
3502.689726	804863.565523	43.072231
3502.734971	804823.538133	43.077236
3502.692349	804788.429427	43.082241
3502.452202	804760.170282	43.087245
3502.344997	804700.402278	43.092250
3502.640906	804684.119593	43.097255
3502.623310	804638.951737	43.102260
3502.712325	804602.496171	43.107265
3502.344056	804566.998562	43.112269
3502.799304	804530.531337	43.117274
3502.407173	804504.797535	43.122279
3502.457879	804465.944280	43.127284
3502.876751	804433.111988	43.132289
3502.428777	804397.822822	43.137293
3502.720826	804362.951103	43.142298
3502.070599	804338.092994	43.147303
3502.203591	804304.080985	43.152308
3502.394591	804282.370318	43.157313
3502.376219	804252.552068	43.162317
3502.518640	804219.568103	43.167322
3502.214185	804192.788671	43.172327
3502.183111	804159.244410	43.177332
3502.274511	804129.113251	43.182337
3502.136258	804104.169965	43.187341
3502.343085	804074.608147	43.192346
3502.173141	804054.672948	43.197351
3502.229828	804020.279711	43.202356
3502.219610	803989.674182	43.207361
3502.349134	803962.871423	43.212365
3502.153283	803921.259842	43.217370
3501.615228	803905.652245	43.222375
3501.955083	803877.195835	43.227380
3502.509162	803851.450883	43.232385
3501.734183	803828.426366	43.237389
3502.111931	803796.480743	43.242394
3502.041059	803763.284470	43.247399
3501.929169	803749.715546	43.252404
3502.110608	803715.447395	43.257409
3502.022278	803697.950323	43.262413
3502.219421	803679.964714	43.267418
3502.297715	803648.999727	43.272423
3501.983255	803629.724785	43.277428
3502.127349	803599.582633	43.282433
3502.143062	803571.717938	43.287437
3501.953036	803540.992874	43.292442
3502.190806	803540.953694	43.297447
3502.145752	803503.827655	43.302452
3502.496847	803483.755928	43.307457
3502.089936	803448.160803	43.312461
3502.362133	803418.928787	43.317466
3502.337627	803405.246683	43.322471
3502.101833	803357.849874	43.327476
3502.112004	803327.630486	43.332481
3501.875414	803311.088893	43.337485
3501.995028	803292.133947	43.342490
3502.145394	803256.396984	43.347495
3502.060526	803235.120907	43.352500
3502.011043	803202.261799	43.357505
3501.738372	803183.371169	43.362509
3502.415913	803165.893764	43.367514
3502.308708	803132.357048	43.372519
3502.443830	803104.078348	43.377524
3502.559069	803075.459410	43.382529
3502.098198	803044.727692	43.387533
3502.408366	803011.563153	43.392538
3502.147211	802984.183204	43.397543
3502.104750	802973.593808	43.402548
3502.196380	802933.989323	43.407553
3501.888544	802920.156695	43.412557
3502.209407	802880.072625	43.417562
3502.038008	802866.904229	43.422567
3502.073281	802844.429764	43.427572
3501.949595	802822.668226	43.432577
3501.950417	802781.851367	43.437581
3502.007269	802760.893895	43.442586
3501.906732	802735.988505	43.447591
3501.977641	802709.533951	43.452596
3501.959247	802690.501969	43.457601
3501.796582	802676.644940	43.462605
3502.065401	802661.490323	43.467610
3502.032408	802636.230031	43.472615
3501.907450	802607.599661	43.477620
3501.730588	802582.019449	43.482625
3501.782874	802567.979616	43.487629
3502.203903	802541.810172	43.492634
3502.018131	802518.487969	43.497639
3501.941995	802506.627829	43.502644
3501.941812	802472.383431	43.507649
3501.529614	802454.740309	43.512653
3501.912853	802442.166599	43.517658
3501.724662	802419.089765	43.522663
3501.985654	802399.176920	43.527668
3501.892773	802379.616675	43.532673
3501.839080	802350.041330	43.537677
3502.131936	802329.583358	43.542682
3502.001908	802303.258471	43.547687
3502.275798	802285.796279	43.552692
3502.301698	802253.901489	43.557697
3501.791861	802239.855456	43.562701
3502.365941	802201.884501	43.567706
3501.880371	802189.355314	43.572711
3501.927922	802164.080031	43.577716
3501.789987	802143.545278	43.582721
3501.856366	802122.976810	43.587725
3502.042429	802082.027182	43.592730
3501.742529	802077.023006	43.597735
3501.850970	802037.852195	43.602740
3502.264500	802017.667809	43.607745
3502.166658	802003.504368	43.612749
3502.055613	801980.511491	43.617754
3502.059953	801957.008886	43.622759
3501.954395	801937.106026	43.627764
3502.035444	801903.434208	43.632769
3501.830998	801891.790408	43.637773
3501.989229	801864.336939	43.642778
3502.094902	801856.076560	43.647783
3502.176417	801816.810803	43.652788
3502.171942	801796.400233	43.657793
3501.885396	801767.743936	43.662797
3502.149475	801735.169668	43.667802
3501.965382	801724.945150	43.672807
3502.150376	801706.956417	43.677812
3502.191717	801671.867092	43.682817
3501.936376	801651.644616	43.687821
3502.134307	801624.968728	43.692826
3501.926299	801602.432168	43.697831
3501.965435	801579.805759	43.702836
3502.112889	801557.603040	43.707841
3501.815721	801536.405770	43.712845
3502.363146	801502.164508	43.717850
3502.224326	801483.296245	43.722855
3502.205011	801459.305169	43.727860
3502.090915	801435.722168	43.732865
3502.047524	801403.246055	43.737869
3502.321045	801370.864795	43.742874
3501.896818	801356.950065	43.747879
3501.969849	801330.538962	43.752884
3502.243794	801300.610753	43.757889
3502.175714	801280.454486	43.762893
3502.117382	801253.672173	43.767898
3501.892756	801236.927361	43.772903
3501.785559	801223.745257	43.777908
3501.822356	801179.085581	43.782913
3501.522206	801176.092661	43.787917
3501.889562	801147.178875	43.792922
3501.663564	801112.964950	43.797927
3501.563628	801114.846075	43.802932
3501.981581	801101.479097	43.807937
3501.850288	801074.953464	43.812941
3501.774085	801048.369584	43.817946
3501.726869	801043.519317	43.822951
3501.983851	801023.652258	43.827956
3502.046372	801007.301233	43.832961
3501.951832	800981.456186	43.837965
3501.932819	800961.732553	43.842970
3502.115123	800940.650767	43.847975
3501.885221	800918.704449	43.852980
3502.143672	800880.483828	43.857985
3501.897551	800871.544141	43.862989
3502.050847	800848.798399	43.867994
3501.789979	800837.603767	43.872999
3501.730878	800813.617010	43.878004
3501.909739	800781.297667	43.883009
3501.668093	800776.332020	43.888013
3502.188394	800739.686899	43.893018
3502.118413	800723.062591	43.898023
3501.953451	800709.103850	43.903028
3501.831234	800666.871665	43.908033
3501.880900	800664.458858	43.913037
3502.154447	800619.167699	43.918042
3502.392461	800607.350707	43.923047
3501.912606	800574.599088	43.928052
3501.968476	800555.941602	43.933057
3501.849448	800532.012818	43.938061
3502.319999	800509.655381	43.943066
3501.995617	800472.510013	43.948071
3501.898502	800465.066583	43.953076
3502.202070	800421.045141	43.958081
3502.027533	800420.779421	43.963085
3501.994591	800394.627590	43.968090
3502.135964	800363.392141	43.973095
3501.591939	800352.930426	43.978100
3501.997827	800319.884480	43.983105
3501.957618	800304.579320	43.988109
3502.111515	800278.641658	43.993114
3501.906204	800262.283919	43.998119
3501.752240	800233.942973	44.003124
3501.987267	800225.021351	44.008129
3501.799873	800195.851450	44.013133
3502.003471	800170.199659	44.018138
3502.032866	800156.305946	44.023143
3502.163303	800136.751662	44.028148
3502.156566	800099.404744	44.033153
3502.001311	800095.013309	44.038157
3502.062367	800056.280816	44.043162
3501.853927	800032.119647	44.048167
3501.909168	800019.791904	44.053172
3502.182505	799996.974525	44.058177
3501.793419	799965.333879	44.063181
3501.825594	799956.837956	44.068186
3501.926599	799933.656126	44.073191
3501.879093	799901.713532	44.078196
3501.896122	799883.747747	44.083201
3501.566744	799862.158024	44.088205
3501.572357	799842.917951	44.093210
3502.099575	799817.456953	44.098215
3501.687280	799814.629147	44.103220
3502.105222	799789.873163	44.108225
3502.006120	799762.306534	44.113229
3502.054643	799737.513053	44.118234
3501.685920	799723.242329	44.123239
3501.767947	799703.400319	44.128244
3501.710029	799669.151590	44.133249
3501.560667	799668.538126	44.138253
3501.734686	799638.177497	44.143258
3502.005799	799630.132628	44.148263
3501.746950	799609.364878	44.153268
3501.979590	799588.908761	44.158273
3501.873822	799568.999138	44.163277
3501.911120	799540.034881	44.168282
3501.748649	799543.644584	44.173287
3501.857289	799501.563616	44.178292
3502.270534	799491.580982	44.183297
3501.640254	799463.560760	44.188301
3501.824557	799439.774579	44.193306
3501.893066	799439.763279	44.198311
3501.466022	799412.691021	44.203316
3501.939824	799400.391404	44.208321
3501.410571	799391.987268	44.213325
3501.665444	799354.298762	44.218330
3501.722297	799342.460384	44.223335
3501.426181	799339.711410	44.228340
3501.874800	799304.150374	44.233345
3501.657856	799299.228678	44.238349
3501.540826	799284.817427	44.243354
3501.689768	799262.312634	44.248359
3501.552309	799250.996943	44.253364
3501.751373	799232.214154	44.258369
3501.381025	799230.017285	44.263373
3501.616811	799203.816711	44.268378
3501.697496	799187.311163	44.273383
3501.506710	799187.882498	44.278388
3501.727410	799157.659338	44.283393
3501.632827	799148.986972	44.288397
3501.496730	799138.701645	44.293402
3501.463024	799125.601620	44.298407
3501.330149	799094.307480	44.303412
3501.474747	799082.945056	44.308417
3501.539506	799093.340353	44.313421
3501.677037	799049.190333	44.318426
3501.426829	799045.795573	44.323431
3501.561526	799033.796594	44.328436
3501.900787	799012.584946	44.333441
3502.121954	799003.320450	44.338445
3501.848499	798984.320313	44.343450
3501.837406	798956.343310	44.348455
3501.818351	798937.497484	44.353460
3501.625727	798919.023798	44.358465
3501.553401	798900.088473	44.363469
3501.769104	798865.054426	44.368474
3501.847975	798866.121319	44.373479
3501.636392	798851.773832	44.378484
3501.597361	798828.169611	44.383489
3501.649911	798817.312783	44.388493
3501.555840	798799.067979	44.393498
3501.696183	798783.238865	44.398503
3501.468393	798776.993236	44.403508
3501.845618	798746.644339	44.408513
3501.593600	798729.701638	44.413517
3501.705426	798724.823555	44.418522
3501.563463	798701.923084	44.423527
3501.774415	798696.243252	44.428532
3501.599382	798666.917639	44.433537
3501.767122	798655.845235	44.438541
3501.742374	798635.036015	44.443546
3501.532244	798616.858939	44.448551
3501.011274	798619.693669	44.453556
3501.841143	798586.275143	44.458561
3501.449566	798585.456036	44.463565
3501.618149	798580.273973	44.468570
3501.801126	798550.348927	44.473575
3501.968454	798525.727920	44.478580
3501.997803	798524.446761	44.483585
3501.519046	798487.758012	44.488589
3501.840813	798477.249024	44.493594
3502.190611	798460.599251	44.498599
3501.842407	798439.351833	44.503604
3501.734085	798414.677659	44.508609
3501.682277	798392.350395	44.513613
3501.499507	798387.618781	44.518618
3501.681514	798377.083573	44.523623
3501.582873	798351.916684	44.528628
3501.751654	798326.558385	44.533633
3501.668619	798329.713816	44.538637
3501.427464	798290.284931	44.543642
3501.742552	798283.703985	44.548647
3501.290658	798269.198518	44.553652
3501.492613	798273.239753	44.558657
3501.572402	798251.086724	44.563661
3501.705785	798232.606609	44.568666
3501.797481	798231.511491	44.573671
3501.752008	798219.786245	44.578676
3501.446721	798180.269119	44.583681
3501.751062	798178.893511	44.588685
3501.852762	798158.405679	44.593690
3501.629227	798124.373001	44.598695
3501.554312	798119.623438	44.603700
3501.860728	798103.863612	44.608705
3501.578375	798069.349436	44.613709
3501.875371	798057.272955	44.618714
3501.585516	798039.500241	44.623719
3501.834644	798011.329308	44.628724
3501.971596	798000.800955	44.633729
3501.726380	797978.602410	44.638733
3501.892966	797968.461868	44.643738
3501.819443	797951.340593	44.648743
3501.776596	797920.811841	44.653748
3501.818428	797908.924412	44.658753
3501.348782	797897.857610	44.663757
3501.436051	797866.325324	44.668762
3501.514357	797858.801114	44.673767
3501.490775	797858.706795	44.678772
3501.535462	797834.349020	44.683777
3501.258441	797811.467870	44.688781
3501.283168	797809.696404	44.693786
3501.405409	797803.048587	44.698791
3501.244878	797805.186048	44.703796
3501.937933	797783.568742	44.708801
3501.591681	797779.403674	44.713805
3501.352741	797762.358276	44.718810
3501.624115	797749.352697	44.723815
3501.125370	797724.544013	44.728820
3501.565102	797713.032561	44.733825
3501.200169	797716.971119	44.738829
3501.213987	797720.650910	44.743834
3501.297224	797700.115681	44.748839
3501.436381	797689.341024	44.753844
3501.518996	797664.534557	44.758849
3501.286356	797669.875100	44.763853
3501.589138	797661.086333	44.768858
3501.533070	797629.085638	44.773863
3501.462093	797623.745948	44.778868
3501.367342	797599.852179	44.783873
3501.564817	797605.956543	44.788877
3501.316679	797579.878685	44.793882
3501.219556	797565.607885	44.798887
3501.226460	797547.343174	44.803892
3501.435863	797537.980487	44.808897
3501.401449	797550.063675	44.813901
3501.515414	797524.024155	44.818906
3501.477817	797510.627162	44.823911
3501.112785	797494.191029	44.828916
3501.436010	797499.391045	44.833921
3501.069673	797484.280695	44.838925
3501.600820	797461.167086	44.843930
3501.766889	797444.643356	44.848935
3501.096942	797455.554883	44.853940
3501.357825	797434.007686	44.858945
3501.462912	797420.930695	44.863949
3501.267521	797404.859180	44.868954
3501.477484	797406.051996	44.873959
3501.343236	797389.872183	44.878964
3501.712547	797388.780304	44.883969
3501.665693	797353.732830	44.888973
3501.460026	797350.624482	44.893978
3501.747212	797343.310798	44.898983
3501.440746	797314.541216	44.903988
3501.599183	797293.452337	44.908993
3501.472393	797296.762733	44.913997
3501.450698	797291.365573	44.919002
3501.816474	797267.934885	44.924007
3501.442290	797259.011635	44.929012
3501.497196	797244.420551	44.934017
3501.227481	797217.313839	44.939021
3501.593423	797202.916927	44.944026
3501.628732	797197.166619	44.949031
3501.390929	797199.415187	44.954036
3501.758848	797178.438751	44.959041
3501.648321	797159.063110	44.964045
3501.577690	797153.035625	44.969050
3501.661307	797131.762190	44.974055
3501.414755	797104.258436	44.979060
3501.767953	797097.768302	44.984065
3501.577293	797085.279485	44.989069
3501.513315	797055.977908	44.994074
3501.488661	797044.149060	44.999079
3501.531220	797048.266364	45.004084
3501.739809	797020.589114	45.009089
3501.818592	797008.104876	45.014093
3501.643390	796994.189466	45.019098
3501.668889	796975.281905	45.024103
3501.562255	796973.630065	45.029108
3501.608901	796945.488195	45.034113
3501.344122	796936.153711	45.039117
3501.764054	796897.786469	45.044122
3501.709891	796894.014658	45.049127
3501.459026	796895.037968	45.054132
3501.539485	796858.837739	45.059137
3501.589104	796847.045425	45.064141
3501.534812	796842.979004	45.069146
3501.583744	796834.181917	45.074151
3501.492635	796798.255138	45.079156
3501.793413	796794.621212	45.084161
3501.583720	796792.888102	45.089165
3501.265057	796762.399722	45.094170
3501.448283	796750.830745	45.099175
3501.285482	796750.219228	45.104180
3501.466168	796736.146482	45.109185
3501.567900	796723.265146	45.114189
3501.357180	796705.819708	45.119194
3501.408576	796689.705898	45.124199
3501.475512	796693.868497	45.129204
3501.555386	796666.211049	45.134209
3501.406744	796652.290582	45.139213
3501.412632	796653.811756	45.144218
3501.571033	796634.243059	45.149223
3501.179536	796625.812868	45.154228
3501.295907	796594.171851	45.159233
3501.099735	796595.087990	45.164237
3501.256130	796590.937616	45.169242
3501.549317	796583.327540	45.174247
3501.385799	796595.531846	45.179252
3501.812310	796554.362809	45.184257
3501.623735	796542.952936	45.189261
3501.420493	796538.125229	45.194266
3501.448481	796511.212256	45.199271
3501.388310	796503.021959	45.204276
3501.454878	796483.467967	45.209281
3501.441556	796490.148166	45.214285
3501.456664	796472.812258	45.219290
3501.614979	796449.462113	45.224295
3501.274901	796448.977976	45.229300
3501.732481	796434.859016	45.234305
3501.271663	796424.917793	45.239309
3501.468114	796403.574458	45.244314
3501.458314	796390.907297	45.249319
3501.457292	796391.005657	45.254324
3501.649070	796361.266215	45.259329
3501.473944	796340.720453	45.264333
3501.600643	796338.882715	45.269338
3501.969649	796314.466230	45.274343
3501.759017	796296.725131	45.279348
3501.855486	796289.048932	45.284353
3501.599156	796263.654974	45.289357
3501.655460	796239.289734	45.294362
3501.581788	796222.557089	45.299367
3500.955633	796232.775821	45.304372
3501.562865	796218.189833	45.309377
3501.542295	796193.984414	45.314381
3501.567674	796183.078868	45.319386
3501.676653	796177.462905	45.324391
3501.328842	796170.449018	45.329396
3501.592176	796142.906603	45.334401
3501.580551	796146.689624	45.339405
3501.154837	796145.630304	45.344410
3501.483282	796114.246822	45.349415
3501.153353	796097.408771	45.354420
3501.574770	796083.344169	45.359425
3501.463549	796076.585853	45.364429
3501.399371	796074.141110	45.369434
3501.649891	796045.323667	45.374439
3501.409555	796032.841151	45.379444
3501.429758	796036.618989	45.384449
3501.456814	796026.105773	45.389453
3501.266278	795998.932190	45.394458
3501.274406	795996.082657	45.399463
3501.406070	795988.351226	45.404468
3501.527012	795973.893939	45.409473
3501.301498	795956.547283	45.414477
3501.006248	795950.212012	45.419482
3501.093351	795935.711114	45.424487
3501.101597	795925.839236	45.429492
3501.354012	795930.315487	45.434497
3501.217421	795931.860287	45.439501
3501.508559	795929.307859	45.444506
3501.380034	795896.476359	45.449511
3501.473498	795893.514514	45.454516
3501.335363	795883.224722	45.459521
3501.330309	795886.663050	45.464525
3501.218346	795873.373387	45.469530
3501.444695	795837.192960	45.474535
3501.067419	795841.429235	45.479540
3501.469995	795831.148519	45.484545
3501.372384	795832.441381	45.489549
3501.458904	795825.502929	45.494554
3501.654687	795787.903158	45.499559
3501.390784	795791.089522	45.504564
3501.664583	795779.945999	45.509569
3501.374399	795759.417483	45.514573
3501.256127	795735.324789	45.519578
3501.595389	795724.857914	45.524583
3501.423401	795728.716683	45.529588
3501.337537	795705.207849	45.534593
3501.449631	795700.573163	45.539597
3501.525297	795688.087090	45.544602
3501.684272	795671.069264	45.549607
3501.376511	795669.352024	45.554612
3501.303784	795650.211525	45.559617
3501.519062	795636.671076	45.564621
3501.236853	795627.681475	45.569626
3501.585693	795621.436250	45.574631
3501.208372	795622.971659	45.579636
3501.595934	795579.396976	45.584641
3501.476328	795589.091214	45.589645
3501.113336	795572.011796	45.594650
3501.408449	795570.440776	45.599655
3500.993514	795558.428158	45.604660
3501.328642	795525.714989	45.609665
3501.358981	795530.915614	45.614669
3501.236538	795540.021070	45.619674
3501.158860	795522.354329	45.624679
3501.207920	795527.699202	45.629684
3501.183374	795496.321995	45.634689
3501.382510	795489.806653	45.639693
3500.945719	795483.052280	45.644698
3501.549891	795470.331437	45.649703
3501.143912	795478.796132	45.654708
3501.684211	795462.500754	45.659713
3501.313008	795443.850847	45.664717
3501.323499	795428.133761	45.669722
3501.397250	795419.527255	45.674727
3501.101164	795432.541184	45.679732
3501.604922	795403.679398	45.684737
3501.298398	795395.528385	45.689741
3501.544556	795376.089059	45.694746
3501.859969	795368.523123	45.699751
3501.561294	795367.049865	45.704756
3501.580723	795327.364909	45.709761
3501.619581	795335.461836	45.714765
3501.659354	795309.426313	45.719770
3501.835087	795294.221934	45.724775
3501.543292	795276.786289	45.729780
3501.334397	795278.244916	45.734785
3501.540428	795254.440935	45.739789
3501.518262	795242.264855	45.744794
3501.488645	795243.006394	45.749799
3501.403707	795219.397556	45.754804
3501.630104	795205.461551	45.759809
3501.723726	795173.916104	45.764813
3501.661432	795157.375492	45.769818
3501.513400	795068.898773	45.774823
3501.369786	794944.567172	45.779828
3501.281669	794758.142916	45.784833
3501.364005	794534.848183	45.789837
3501.044601	794236.362904	45.794842
3500.943829	793870.041781	45.799847
3500.891829	793470.387478	45.804852
3500.678532	792991.101872	45.809857
3500.428620	792472.484983	45.814861
3500.355474	791885.601619	45.819866
3500.267037	791239.459060	45.824871
3499.532215	790527.658045	45.829876
3499.078503	789775.534910	45.834881
3498.827170	788947.943867	45.839885
3498.523686	788071.005547	45.844890
3498.220380	787120.011000	45.849895
3497.694802	786125.751152	45.854900
3497.233519	785066.176678	45.859905
3496.994692	783942.413550	45.864909
3496.237824	782758.293190	45.869914
3495.803709	781500.066894	45.874919
3495.326920	780183.850322	45.879924
3494.804468	778800.654231	45.884929
3494.224306	777383.233413	45.889933
3493.416934	775858.715119	45.894938
3492.564710	774297.931178	45.899943
3492.008758	772675.136029	45.904948
3491.361162	770977.344878	45.909953
3490.713133	769229.087819	45.914957
3489.851759	767421.491901	45.919962
3489.183497	765524.121355	45.924967
3488.173057	763600.234351	45.929972
3487.544697	761579.435070	45.934977
3486.653882	759515.252869	45.939981
3485.806742	757387.216524	45.944986
3484.897086	755189.762602	45.949991
3483.847117	752962.758554	45.954996
3482.678863	750645.800643	45.960001
3481.635056	748260.864907	45.965005
3480.536299	745840.998047	45.970010
3480.088973	743353.365909	45.975015
3478.464026	740804.345004	45.980020
3477.639300	738194.842021	45.985025
3476.484451	735506.623546	45.990029
3475.123889	732782.629603	45.995034
3474.289392	729987.141760	46.000039
3472.927238	727137.214558	46.005044
3471.531237	724227.263943	46.010049
3470.509939	721250.571200	46.015053
3469.131830	718225.250635	46.020058
3468.107347	715144.590264	46.025063
3466.532234	712004.815122	46.030068
3465.057445	708804.321564	46.035073
3463.832894	705542.132540	46.040077
3462.425545	702235.903804	46.045082
3460.833395	698855.963408	46.050087
3459.148120	695431.618572	46.055092
3457.797110	691958.281174	46.060097
3456.428776	688416.700542	46.065101
3454.935551	684813.400522	46.070106
3452.962845	681164.022802	46.075111
3451.245262	677460.033098	46.080116
3449.662519	673688.138793	46.085121
3448.092123	669885.452675	46.090125
3446.367286	666009.219003	46.095130
3444.923912	662088.894916	46.100135
3442.743061	658112.726924	46.105140
3441.319747	654090.660193	46.110145
3439.633449	650001.634640	46.115149
3437.420060	645874.230963	46.120154
3435.809112	641675.423074	46.125159
3433.914713	637439.417956	46.130164
3431.913916	633145.387096	46.135169
3429.977474	628797.810933	46.140173
3427.867340	624399.141162	46.145178
3426.197784	619943.924857	46.150183
3424.217560	615443.673963	46.155188
3422.082987	610877.214313	46.160193
3419.572506	606287.987199	46.165197
3417.539713	601639.503527	46.170202
3416.067206	596939.842210	46.175207
3413.748756	592188.699513	46.180212
3411.312836	587385.520823	46.185217
3409.114831	582553.396875	46.190221
3406.810145	577667.379932	46.195226
3405.117939	572704.070102	46.200231
3402.450502	567719.753998	46.205236
3399.996346	562685.890496	46.210241
3397.730161	557600.294594	46.215245
3395.545469	552474.602661	46.220250
3393.138946	547298.720872	46.225255
3391.016939	542080.818378	46.230260
3388.457406	536810.308333	46.235265
3386.131372	531504.475183	46.240269
3383.423781	526146.859476	46.245274
3381.357176	520755.108247	46.250279
3378.768037	515301.222973	46.255284
3375.976577	509830.670930	46.260289
3373.644259	504288.506953	46.265293
3371.028963	498711.040766	46.270298
3368.698150	493093.331255	46.275303
3365.622727	487435.453148	46.280308
3363.001729	481744.456866	46.285313
3360.473034	475993.930606	46.290317
3357.632097	470218.890601	46.295322
3355.057339	464405.129941	46.300327
3351.973702	458547.925774	46.305332
3348.954408	452669.050988	46.310337
3346.440013	446743.867436	46.315341
3343.287095	440791.450685	46.320346
3340.660530	434791.240139	46.325351
3337.754790	428765.009085	46.330356
3335.006112	422696.093175	46.335361
3332.236688	416602.879413	46.340365
3328.824632	410471.642443	46.345370
3326.197091	404301.238555	46.350375
3322.718984	398107.545555	46.355380
3319.690189	391880.583645	46.360385
3316.746943	385615.902392	46.365389
3313.472181	379340.330075	46.370394
3310.634520	373025.035496	46.375399
3307.285693	366690.740437	46.380404
3304.393893	360308.925355	46.385409
3300.896560	353910.437538	46.390413
3297.646769	347479.239734	46.395418
3294.432311	341015.418550	46.400423
3290.881099	334545.252539	46.405428
3287.811847	328047.213399	46.410433
3284.662544	321521.579035	46.415437
3281.244113	314982.722776	46.420442
3277.562743	308408.480998	46.425447
3274.280564	301826.585487	46.430452
3270.395419	295233.780946	46.435457
3266.954585	288617.077241	46.440461
3263.211486	281976.741013	46.445466
3259.725237	275321.000348	46.450471
3256.300120	268670.409058	46.455476
3252.570089	261985.318221	46.460481
3248.872585	255311.714502	46.465485
3245.111574	248607.205885	46.470490
3241.668400	241903.460220	46.475495
3238.121072	235171.920076	46.480500
3234.234194	228450.364740	46.485505
3230.172308	221709.887798	46.490509
3226.119093	214988.017146	46.495514
3222.725598	208133.293513	46.500519
3218.479522	201378.415042	46.505524
3214.438310	194628.347054	46.510529
3210.515663	187861.861720	46.515533
3206.657501	181101.139214	46.520538
3202.610002	174350.111979	46.525543
3198.326678	167584.461018	46.530548
3194.219184	160826.649932	46.535553
3190.072125	154075.807465	46.540557
3185.463993	147329.062299	46.545562
3181.436841	140598.647041	46.550567
3176.495916	133884.848761	46.555572
3172.202488	127169.800516	46.560577
3168.030443	120482.375463	46.565581
3162.996318	113803.384979	46.570586
3158.295514	107149.791641	46.575591
3153.153452	100531.571872	46.580596
3148.328121	93916.151206	46.585601
3143.242784	87343.007495	46.590605
3137.804860	80815.725296	46.595610
3132.655751	74299.277276	46.600615
3126.495894	67866.174435	46.605620
3120.638332	61451.354361	46.610625
3114.459800	55107.030899	46.615629
3106.109253	48871.889985	46.620634
3091.082010	42896.459776	46.625639
3073.150528	37142.701891	46.630644
3055.698206	31602.257489	46.635649
3038.256364	26343.772284	46.640653
3021.345043	21358.561133	46.645658
3005.684322	16672.425814	46.650663
2989.795929	12318.907038	46.655668
2974.445776	8249.068921	46.660673
2958.747092	4537.042609	46.665677
2940.055444	1199.664276	46.670682
2847.102808	313.922852	46.675687
2754.722489	338.787068	46.680692
2714.672292	318.048200	46.685697
2718.495013	305.497029	46.690701
2746.218060	282.039727	46.695706
2779.804468	281.461983	46.700711
2805.637427	290.523878	46.705716
2820.195213	290.735590	46.710721
2824.863693	300.625778	46.715725
2822.954721	296.449401	46.720730
2818.045193	276.619154	46.725735
2811.807076	273.126983	46.730740
2806.488934	284.411462	46.735745
2802.615740	284.755680	46.740749
2799.603832	283.660244	46.745754
2797.581107	282.501475	46.750759
2795.589907	273.836358	46.755764
2793.496428	275.214831	46.760769
2791.109348	268.410679	46.765773
2787.604543	277.436254	46.770778
2784.497111	277.543540	46.775783
2781.474478	273.312323	46.780788
2778.402488	273.691790	46.785793
2775.696846	273.670881	46.790797
2772.274297	272.526541	46.795802
2769.107554	275.080392	46.800807
2765.682297	271.585456	46.805812
2762.880426	269.232726	46.810817
2759.646698	257.643115	46.815821
2756.453853	258.719710	46.820826
2753.048714	264.339233	46.825831
2749.322952	264.197743	46.830836
2745.840085	260.099644	46.835841
2743.190945	245.171937	46.840845
2739.768771	260.056171	46.845850
2736.691351	246.559286	46.850855
2733.485220	252.178362	46.855860
2729.460168	252.204517	46.860865
2726.438303	255.842633	46.865869
2722.845202	259.625048	46.870874
2719.780991	238.956360	46.875879
2716.269090	251.772009	46.880884
2712.846026	244.236663	46.885889
2709.109953	252.639170	46.890893
2705.529976	258.478143	46.895898
2702.904372	247.993032	46.900903
2699.648201	252.122137	46.905908
2695.932842	241.753266	46.910913
2692.688510	247.340472	46.915917
2689.150470	254.098351	46.920922
2686.257837	244.270342	46.925927
2682.405938	248.471134	46.930932
2678.687396	244.174853	46.935937
2675.220932	242.737286	46.940941
2671.287498	249.215844	46.945946
2668.575898	246.293019	46.950951
2665.692205	238.689588	46.955956
2661.991848	241.353752	46.960961
2658.076213	247.205759	46.965965
2654.322190	236.302543	46.970970
2651.771696	236.320324	46.975975
2647.917581	243.218826	46.980980
2644.004315	234.484938	46.985985
2640.927259	231.203577	46.990989
2637.548094	247.720346	46.995994
2634.504184	233.923703	47.000999
2631.269140	234.979878	47.006004
2627.232476	227.676775	47.011009
2623.807028	228.576995	47.016013
2620.554340	230.489086	47.021018
2616.801827	232.313898	47.026023
2612.952595	228.177426	47.031028
2609.400868	234.758223	47.036033
2606.467775	222.902892	47.041037
2603.532387	229.553336	47.046042
2599.614546	230.745193	47.051047
2596.400197	231.842859	47.056052
2592.776068	229.957668	47.061057
2589.626989	222.647645	47.066061
2585.757378	232.213392	47.071066
2581.977662	214.068196	47.076071
2578.981254	227.457909	47.081076
2575.351391	218.607986	47.086081
2572.449743	224.352910	47.091085
2568.530080	231.763631	47.096090
2564.632871	230.335875	47.101095
2561.169548	226.469364	47.106100
2557.832285	231.357945	47.111105
2554.245106	229.350757	47.116109
2550.879348	233.993841	47.121114
2547.824733	217.636961	47.126119
2544.117909	229.164935	47.131124
2540.453891	223.389138	47.136129
2537.307460	215.555028	47.141133
2533.672077	217.234380	47.146138
2529.541697	219.404196	47.151143
2526.591955	210.767434	47.156148
2523.182545	231.597320	47.161153
2520.026458	218.593228	47.166157
2516.234363	224.753056	47.171162
2512.686101	221.772027	47.176167
2509.172479	224.794773	47.181172
2505.568848	220.251741	47.186177
2502.800962	210.031527	47.191181
2498.648464	218.736292	47.196186
2495.407309	214.432924	47.201191
2491.384983	219.258980	47.206196
2488.135948	213.170113	47.211201
2484.711526	220.421851	47.216205
2481.539000	217.727440	47.221210
2478.539580	207.186894	47.226215
2474.878900	215.451549	47.231220
2471.072157	215.836277	47.236225
2467.403319	205.013171	47.241229
2463.222247	219.109507	47.246234
2460.105348	219.984962	47.251239
2457.068349	217.547909	47.256244
2453.547168	220.656869	47.261249
2449.995255	211.639865	47.266253
2446.279851	212.024637	47.271258
2443.098173	215.613133	47.276263
2439.919707	213.165774	47.281268
2435.915718	217.320323	47.286273
2432.659994	206.629092	47.291277
2428.741575	207.622825	47.296282
2425.736045	210.085395	47.301287
2422.144472	209.346363	47.306292
2418.245967	204.071919	47.311297
2415.250904	209.651650	47.316301
2411.370701	215.959930	47.321306
2408.145938	197.804059	47.326311
2404.843188	203.845148	47.331316
2401.188988	206.579951	47.336321
2397.715929	203.365390	47.341325
2394.081633	207.533181	47.346330
2390.668427	220.014163	47.351335
2386.879030	216.603251	47.356340
2383.539268	204.932813	47.361345
2380.324350	202.853569	47.366349
2376.920847	198.847655	47.371354
2373.132811	221.503222	47.376359
2369.365545	219.254021	47.381364
2365.988645	209.425843	47.386369
2362.869105	209.130108	47.391373
2358.833469	205.841808	47.396378
2355.563341	208.404374	47.401383
2352.068043	211.010390	47.406388
2348.745476	212.243407	47.411393
2345.625131	194.798456	47.416397
2342.171927	210.330237	47.421402
2338.584510	206.550014	47.426407
2334.898049	202.572730	47.431412
2330.873094	210.759986	47.436417
2327.469206	213.644939	47.441421
2323.492290	209.501473	47.446426
2321.152230	208.843481	47.451431
2317.593862	204.322093	47.456436
2313.590779	206.048375	47.461441
2310.547389	200.321107	47.466445
2306.511402	208.079450	47.471450
2302.915541	198.432947	47.476455
2299.620769	198.578332	47.481460
2296.051498	203.999646	47.486465
2293.115998	199.628900	47.491469
2289.358022	211.096526	47.496474
2285.998318	199.036087	47.501479
2282.370512	196.268573	47.506484
2279.070318	203.366507	47.511489
2275.584390	188.955750	47.516493
2271.646654	200.891952	47.521498
2268.092428	200.684622	47.526503
2264.955621	205.806822	47.531508
2261.248504	209.016872	47.536513
2257.620791	203.663723	47.541517
2253.891197	212.043617	47.546522
2250.762427	203.531033	47.551527
2247.570396	202.566463	47.556532
2243.833056	199.408293	47.561537
2240.677375	195.619071	47.566541
2236.703313	201.664195	47.571546
2233.250272	189.414670	47.576551
2229.787767	192.028055	47.581556
2226.118287	196.822476	47.586561
2222.933397	198.119855	47.591565
2219.379494	196.374515	47.596570
2215.972439	198.331959	47.601575
2212.746725	186.511311	47.606580
2208.733151	190.068888	47.611585
2205.198159	194.074268	47.616589
2201.622569	202.174930	47.621594
2198.169900	201.479396	47.626599
2194.955813	193.776299	47.631604
2191.264729	199.227415	47.636609
2187.648426	195.510838	47.641613
2184.482675	199.858047	47.646618
2180.600793	194.410914	47.651623
2177.665688	204.349014	47.656628
2173.934494	195.054428	47.661633
2170.192935	183.795012	47.666637
2166.777158	198.683430	47.671642
2163.690877	193.390102	47.676647
2160.203931	196.133536	47.681652
2155.995291	199.149620	47.686657
2152.667720	197.400722	47.691661
2149.638252	201.661535	47.696666
2145.928983	187.903917	47.701671
2142.350928	184.417442	47.706676
2138.321962	190.554438	47.711681
2135.286264	195.462689	47.716685
2132.138100	185.526190	47.721690
2128.651359	191.090132	47.726695
2124.840393	182.534370	47.731700
2121.196680	191.480546	47.736705
2117.909382	184.106558	47.741709
2114.168981	189.369609	47.746714
2110.676385	189.044158	47.751719
2107.622792	184.147598	47.756724
2103.757576	184.395945	47.761729
2100.470067	183.182984	47.766733
2096.740495	206.081225	47.771738
2093.197240	185.781088	47.776743
2089.708679	183.580780	47.781748
2086.205827	190.276041	47.786753
2083.324667	186.487685	47.791757
2079.401317	195.299956	47.796762
2075.962097	193.719472	47.801767
2071.977488	178.690049	47.806772
2068.394907	189.525717	47.811777
2065.563507	186.711397	47.816781
2061.514765	181.088727	47.821786
2058.505726	186.078536	47.826791
2055.430269	184.380737	47.831796
2051.490836	189.895372	47.836801
2048.101228	190.767440	47.841805
2044.147824	179.845635	47.846810
2040.808131	186.868970	47.851815
2037.254010	181.467404	47.856820
2033.555768	179.449602	47.861825
2030.340184	186.685102	47.866829
2026.832866	188.177817	47.871834
2023.415241	181.379933	47.876839
2019.954217	169.351087	47.881844
2016.059969	187.962881	47.886849
2012.928742	179.880394	47.891853
2008.975135	182.882306	47.896858
2005.930867	176.040899	47.901863
2002.616381	184.819943	47.906868
1999.019313	174.265690	47.911873
1995.243456	182.843322	47.916877
1991.688993	177.583019	47.921882
1988.096431	182.207000	47.926887
1984.647786	185.846218	47.931892
1981.078045	194.703395	47.936897
1977.948289	183.373954	47.941901
1974.355938	192.040901	47.946906
1970.877457	185.283174	47.951911
1967.462204	185.558683	47.956916
1963.488310	185.472034	47.961921
1960.636874	177.592628	47.966925
1956.848334	179.486540	47.971930
1953.185766	173.922667	47.976935
1950.031519	178.401447	47.981940
1946.433320	186.012053	47.986945
1942.916035	180.456574	47.991949
1939.304111	171.735796	47.996954
1935.351355	174.717477	48.001959
1932.357577	186.743242	48.006964
1928.868429	186.258076	48.011969
1925.278450	174.237533	48.016973
1921.765347	182.988600	48.021978
1918.127235	181.765885	48.026983
1914.925731	172.099458	48.031988
1911.163337	182.629211	48.036993
1907.885404	170.550000	48.041997
1904.114306	187.765046	48.047002
1900.761184	170.719192	48.052007
1897.413897	169.574199	48.057012
1893.778503	180.038314	48.062017
1890.498387	158.176210	48.067021
1886.858755	183.246080	48.072026
1883.206620	161.009286	48.077031
1879.736201	170.874759	48.082036
1876.040648	182.268985	48.087041
1872.460658	171.529279	48.092045
1868.918107	168.997426	48.097050
1865.837124	177.316527	48.102055
1862.500500	175.655391	48.107060
1858.582374	185.002602	48.112065
1855.358216	181.675629	48.117069
1851.607223	177.254252	48.122074
1847.988657	168.370459	48.127079
1845.147687	171.398926	48.132084
1841.408625	186.664858	48.137089
1838.340906	172.137052	48.142093
1834.588828	182.539149	48.147098
1830.663690	172.433953	48.152103
1827.067753	174.102883	48.157108
1823.594058	184.048443	48.162113
1820.367978	173.233112	48.167117
1816.713716	177.686904	48.172122
1813.193009	181.237454	48.177127
1809.733166	170.197185	48.182132
1805.615084	178.748488	48.187137
1802.955243	175.450078	48.192141
1799.217608	183.601010	48.197146
1795.499647	173.168839	48.202151
1792.206381	178.384404	48.207156
1788.644992	185.059056	48.212161
1785.323145	180.002392	48.217165
1781.914806	175.130088	48.222170
1778.316782	173.149062	48.227175
1774.907572	180.342508	48.232180
1771.031130	179.885409	48.237185
1767.921501	186.822547	48.242189
1764.233377	177.639504	48.247194
1760.576048	182.111883	48.252199
1757.300066	173.539904	48.257204
1753.703764	179.034369	48.262209
1750.144024	166.100220	48.267213
1746.438287	180.698395	48.272218
1743.254971	177.288772	48.277223
1740.145469	173.254309	48.282228
1736.331571	182.174158	48.287233
1732.764530	178.654513	48.292237
1729.287435	181.062655	48.297242
1725.709689	176.273087	48.302247
1722.196590	177.840298	48.307252
1718.381775	174.005293	48.312257
1715.380286	173.281422	48.317261
1711.796178	177.587638	48.322266
1708.047529	186.958353	48.327271
1704.619233	162.739823	48.332276
1700.957063	171.565488	48.337281
1697.708803	173.652935	48.342285
1694.234715	182.673795	48.347290
1690.356869	167.442351	48.352295
1687.173433	174.335654	48.357300
1683.373722	182.856385	48.362305
1680.262258	168.572079	48.367309
1676.730518	175.444820	48.372314
1673.181188	174.804459	48.377319
1669.637488	160.433243	48.382324
1666.230831	173.406436	48.387329
1662.750416	178.140212	48.392333
1659.036724	172.540447	48.397338
1655.448361	167.952552	48.402343
1652.051376	174.000885	48.407348
1648.593302	183.427265	48.412353
1644.928148	164.006993	48.417357
1641.651556	180.325117	48.422362
1638.150498	171.301697	48.427367
1634.767028	173.695517	48.432372
1631.511364	173.947810	48.437377
1627.861018	173.721039	48.442381
1624.099359	165.743681	48.447386
1620.539225	175.019783	48.452391
1617.042216	169.094631	48.457396
1613.405467	177.262733	48.462401
1610.071007	168.351143	48.467405
1606.425182	187.913488	48.472410
1602.838789	174.628854	48.477415
1599.478010	179.924106	48.482420
1595.718069	179.741877	48.487425
1593.065608	166.298109	48.492429
1589.237444	162.752773	48.497434
1585.518917	155.627038	48.502439
1582.085334	168.413106	48.507444
1578.416250	173.109387	48.512449
1574.925042	165.679470	48.517453
1571.457829	167.100370	48.522458
1568.063632	162.746956	48.527463
1564.727335	159.677977	48.532468
1560.916157	167.336806	48.537473
1557.804259	168.134757	48.542477
1554.132638	162.804552	48.547482
1550.423241	172.299865	48.552487
1546.818465	166.319333	48.557492
1543.179109	174.180182	48.562497
1539.929409	168.256682	48.567501
1536.550899	162.188207	48.572506
1533.255424	175.890524	48.577511
1530.027524	167.756473	48.582516
1526.270941	167.284366	48.587521
1522.541500	164.308996	48.592525
1518.860035	179.097995	48.597530
1515.343557	169.861134	48.602535
1511.792692	175.783285	48.607540
1508.359514	162.141359	48.612545
1505.100615	168.874334	48.617549
1501.814042	164.827775	48.622554
1497.899504	168.003056	48.627559
1494.174241	162.656581	48.632564
1490.472103	171.970080	48.637569
1487.294959	157.865243	48.642573
1484.393162	160.334134	48.647578
1480.850545	164.258807	48.652583
1477.141666	165.005161	48.657588
1473.296348	157.815770	48.662593
1469.879921	163.156067	48.667597
1466.321962	157.985528	48.672602
1462.618340	162.717453	48.677607
1459.515303	154.391473	48.682612
1455.924587	154.336184	48.687617
1452.471929	162.779111	48.692621
1448.977405	152.969722	48.697626
1445.635309	166.182819	48.702631
1442.116456	152.469154	48.707636
1438.458563	163.151434	48.712641
1435.238327	164.424298	48.717645
1431.847554	161.328662	48.722650
1427.809486	160.019002	48.727655
1424.181276	161.360388	48.732660
1420.607226	167.826056	48.737665
1417.312172	170.497012	48.742669
1413.576626	161.778509	48.747674
1410.363395	156.819256	48.752679
1406.832858	159.788449	48.757684
1403.416247	153.135779	48.762689
1399.831281	154.290583	48.767693
1396.521185	164.116555	48.772698
1393.054073	168.264597	48.777703
1389.473066	156.189850	48.782708
1385.787658	171.101481	48.787713
1382.479638	161.796657	48.792717
1379.168034	155.607323	48.797722
1375.205451	170.242689	48.802727
1372.228378	162.994900	48.807732
1367.849137	163.531024	48.812737
1364.533820	158.888559	48.817741
1361.269173	156.582314	48.822746
1357.887125	161.213167	48.827751
1354.790682	151.392985	48.832756
1350.844037	158.447400	48.837761
1347.207805	160.531456	48.842765
1343.720509	144.541673	48.847770
1340.220802	155.330868	48.852775
1336.660281	158.007199	48.857780
1333.387005	158.641082	48.862785
1330.390790	155.454725	48.867789
1326.254226	161.109189	48.872794
1322.884926	152.742781	48.877799
1319.260561	150.887994	48.882804
1315.894997	165.643856	48.887809
1312.203718	146.100401	48.892813
1308.768828	156.764272	48.897818
1305.265805	156.932447	48.902823
1301.811481	147.798727	48.907828
1298.607329	149.515320	48.912833
1295.198094	157.510342	48.917837
1291.088030	151.879150	48.922842
1287.358579	158.538438	48.927847
1284.338930	158.659493	48.932852
1280.830641	164.013061	48.937857
1277.309820	172.088375	48.942861
1273.899027	159.954921	48.947866
1270.313210	159.975871	48.952871
1266.991790	155.973269	48.957876
1263.195814	166.290794	48.962881
1259.710411	166.180239	48.967885
1256.236623	162.216998	48.972890
1252.872679	156.763276	48.977895
1249.505858	147.099662	48.982900
1245.357716	161.947232	48.987905
1242.047788	155.372443	48.992909
1238.710578	152.675520	48.997914
1235.209911	150.591997	49.002919
1231.730745	145.887172	49.007924
1228.363516	157.196958	49.012929
1225.092461	154.635726	49.017933
1221.453963	162.334673	49.022938
1217.453405	159.812177	49.027943
1214.241604	152.828453	49.032948
1210.707088	150.140635	49.037953
1207.221445	152.297672	49.042957
1203.812800	151.337275	49.047962
1200.111550	154.821519	49.052967
1196.731616	150.682109	49.057972
1193.118333	159.736097	49.062977
1189.831182	155.607616	49.067981
1186.480045	149.691191	49.072986
1182.897725	152.902361	49.077991
1179.565750	159.386183	49.082996
1175.441933	158.013185	49.088001
1171.974632	153.336720	49.093005
1168.651372	159.603839	49.098010
1165.035778	164.054510	49.103015
1161.877323	144.438701	49.108020
1157.847373	152.584192	49.113025
1154.563238	150.347170	49.118029
1151.503453	156.363621	49.123034
1147.879082	151.712508	49.128039
1144.323519	142.689914	49.133044
1140.553702	157.660644	49.138049
1137.131948	157.040541	49.143053
1133.373289	159.189311	49.148058
1130.053637	164.150921	49.153063
1127.014902	150.952117	49.158068
1123.178049	170.867156	49.163073
1120.010603	146.300292	49.168077
1115.926035	159.600256	49.173082
1112.403758	152.291271	49.178087
1109.300782	160.080723	49.183092
1105.577782	150.802843	49.188097
1102.192129	148.644268	49.193101
1098.531224	156.322796	49.198106
1094.580004	167.022569	49.203111
1091.686606	152.475819	49.208116
1087.907416	159.796519	49.213121
1084.524422	144.188561	49.218125
1081.393097	142.769961	49.223130
1077.576006	153.500766	49.228135
1074.090564	152.005274	49.233140
1070.618249	151.410916	49.238145
1067.009440	143.689461	49.243149
1063.890310	146.396149	49.248154
1060.096002	154.130260	49.253159
1056.679359	135.178794	49.258164
1053.171426	154.128441	49.263169
1049.400256	148.320901	49.268173
1045.856167	142.280140	49.273178
1042.603490	147.522256	49.278183
1038.896054	146.487953	49.283188
1035.343342	155.920516	49.288193
1031.994683	160.215895	49.293197
1028.845643	149.883673	49.298202
1025.425580	155.963008	49.303207
1021.982299	154.364985	49.308212
1017.895027	156.811061	49.313217
1014.600685	147.918854	49.318221
1011.184600	153.844719	49.323226
1007.310268	159.236451	49.328231
1003.901742	151.363378	49.333236
1000.528533	162.682428	49.338241
996.982671	157.315412	49.343245
993.476019	154.993073	49.348250
989.548457	158.941478	49.353255
987.024671	151.136227	49.358260
983.102044	145.906902	49.363265
979.678033	145.393407	49.368269
976.234091	154.827569	49.373274
972.636069	151.209481	49.378279
969.060259	138.885451	49.383284
965.287371	149.831969	49.388289
962.173852	142.481141	49.393293
958.551803	142.862118	49.398298
954.687439	154.962636	49.403303
951.862896	153.234372	49.408308
947.833077	152.527810	49.413313
944.317729	155.596729	49.418317
940.744802	157.418472	49.423322
937.218026	153.828596	49.428327
934.220860	158.072789	49.433332
930.715696	150.615965	49.438337
926.984413	147.210314	49.443341
923.270349	146.992663	49.448346
919.944698	160.557693	49.453351
916.566320	155.910984	49.458356
913.137265	152.220931	49.463361
909.496175	158.980447	49.468365
906.149680	152.629520	49.473370
902.488667	150.716986	49.478375
898.799807	144.663910	49.483380
895.475078	156.102553	49.488385
891.921347	151.991808	49.493389
888.331393	138.970102	49.498394
884.827828	147.162097	49.503399
881.763290	141.629748	49.508404
878.031093	143.134694	49.513409
874.444458	136.735344	49.518413
871.159743	135.820164	49.523418
867.319188	147.472633	49.528423
863.871446	141.872258	49.533428
860.150668	134.989356	49.538433
856.750016	143.610688	49.543437
853.449194	141.670079	49.548442
849.772215	150.913100	49.553447
846.321971	140.509872	49.558452
842.824498	148.128871	49.563457
839.527322	145.072062	49.568461
835.853182	143.258812	49.573466
832.586200	151.496807	49.578471
828.945944	146.760503	49.583476
825.249737	148.623873	49.588481
821.809406	149.403479	49.593485
818.701474	145.200024	49.598490
814.414194	148.349021	49.603495
811.556124	144.389131	49.608500
807.954741	144.665653	49.613505
804.139834	150.005252	49.618509
800.708820	145.953222	49.623514
797.153278	143.389860	49.628519
794.136656	144.303729	49.633524
790.547068	142.148412	49.638529
786.858574	129.095307	49.643533
783.636878	137.994132	49.648538
779.677852	150.591403	49.653543
776.210741	132.986843	49.658548
772.540388	139.491093	49.663553
769.303538	140.068027	49.668557
766.049187	141.164020	49.673562
762.202977	146.049071	49.678567
758.690502	132.897657	49.683572
755.085364	148.065483	49.688577
751.568252	135.759532	49.693581
748.530573	137.144232	49.698586
744.858455	143.219042	49.703591
741.707810	133.832487	49.708596
737.841367	140.916382	49.713601
734.301927	150.016282	49.718605
731.084221	142.202430	49.723610
727.014256	146.308565	49.728615
723.615607	134.759098	49.733620
720.033089	142.371871	49.738625
716.451794	140.562298	49.743629
713.202796	137.470077	49.748634
709.908261	134.186783	49.753639
706.598904	136.817308	49.758644
702.645665	136.938504	49.763649
698.721078	132.822036	49.768653
695.826885	135.004078	49.773658
692.167693	136.163217	49.778663
688.911553	137.870815	49.783668
685.378111	148.532258	49.788673
681.829018	137.745609	49.793677
678.746365	130.763751	49.798682
674.460169	129.892621	49.803687
671.411793	133.721151	49.808692
667.469624	132.219031	49.813697
664.392591	139.348591	49.818701
660.701695	127.663344	49.823706
657.108043	137.343540	49.828711
653.796999	131.443392	49.833716
649.851784	127.496205	49.838721
646.679870	130.761007	49.843725
643.379194	136.329088	49.848730
639.788540	137.540470	49.853735
636.052426	130.084687	49.858740
632.616752	139.638372	49.863745
629.352980	138.957615	49.868749
625.684455	138.505899	49.873754
622.132697	136.518854	49.878759
618.484411	133.621375	49.883764
615.326672	137.721539	49.888769
611.613647	131.912964	49.893773
608.165680	143.089805	49.898778
604.342192	141.789801	49.903783
601.191966	121.631029	49.908788
597.787208	142.968305	49.913793
594.109328	140.611034	49.918797
590.495769	142.285864	49.923802
587.155443	134.749448	49.928807
584.052400	137.754785	49.933812
580.263561	141.533895	49.938817
576.800913	140.102389	49.943821
573.069197	144.544507	49.948826
569.370180	145.287649	49.953831
566.231602	137.560467	49.958836
562.500855	137.368564	49.963841
559.177176	140.773309	49.968845
555.929079	125.349144	49.973850
551.738615	138.525077	49.978855
548.479405	127.368531	49.983860
545.301969	137.223907	49.988865
541.472514	143.748926	49.993869
538.284969	133.955709	49.998874
534.707456	137.796029	50.003879
531.052717	136.009249	50.008884
527.729220	135.275170	50.013889
523.899337	137.295151	50.018893
520.863684	135.356495	50.023898
516.613792	133.443883	50.028903
513.575837	133.593070	50.033908
510.277416	132.138617	50.038913
506.583238	144.242690	50.043917
503.027207	130.607734	50.048922
499.205451	137.778585	50.053927
495.876510	133.134411	50.058932
492.419930	136.302760	50.063937
489.106158	135.721886	50.068941
485.940927	130.683382	50.073946
482.039559	136.347797	50.078951
478.542008	121.810569	50.083956
475.283116	128.605509	50.088961
471.746678	132.297405	50.093965
468.113919	122.910643	50.098970
464.193206	127.511595	50.103975
460.965899	135.436656	50.108980
457.223179	124.941020	50.113985
453.871710	137.788105	50.118989
450.610262	130.641948	50.123994
447.076921	132.979198	50.128999
443.462535	132.660114	50.134004
440.079527	121.183925	50.139009
436.733492	137.174273	50.144013
433.745278	135.052020	50.149018
429.568909	134.951662	50.154023
425.909728	129.275487	50.159028
422.394356	130.085846	50.164033
418.545712	122.930756	50.169037
415.229448	126.401329	50.174042
411.825238	126.824655	50.179047
408.795640	119.396056	50.184052
404.977907	124.330059	50.189057
401.510779	118.184443	50.194061
398.061187	122.945661	50.199066
394.134161	137.017945	50.204071
390.863760	126.980622	50.209076
387.404180	131.874512	50.214081
383.774158	134.825322	50.219085
380.727722	125.248726	50.224090
377.029227	129.328816	50.229095
373.556032	135.160316	50.234100
369.901876	144.790953	50.239105
366.092847	140.424951	50.244109
362.894577	133.693712	50.249114
359.506435	140.109615	50.254119
356.103435	140.082604	50.259124
352.510619	141.009285	50.264129
348.836431	138.573907	50.269133
345.532016	136.383278	50.274138
341.822676	136.351438	50.279143
338.218734	137.992356	50.284148
335.060526	133.944558	50.289153
331.181757	147.360839	50.294157
328.186882	136.772814	50.299162
324.600215	138.224920	50.304167
320.880450	137.765565	50.309172
317.243400	125.441548	50.314177
314.038639	128.356372	50.319181
310.060595	133.300734	50.324186
306.489628	131.661153	50.329191
303.466840	139.772100	50.334196
299.838178	131.910772	50.339201
296.538310	129.716952	50.344205
292.676943	129.281797	50.349210
289.209299	136.999503	50.354215
286.034021	129.248359	50.359220
282.674373	124.520395	50.364225
278.706510	128.568779	50.369229
275.240376	129.965383	50.374234
271.656103	136.522841	50.379239
268.483751	136.651333	50.384244
264.979956	124.897764	50.389249
261.045523	135.736421	50.394253
257.788743	127.498083	50.399258
253.959924	129.839855	50.404263
250.603496	129.503320	50.409268
247.255363	126.912718	50.414273
243.832942	130.395093	50.419277
240.265730	121.690511	50.424282
236.416372	132.784451	50.429287
234.021239	125.488485	50.434292
230.331222	123.202201	50.439297
226.316168	130.748545	50.444301
222.899462	131.005729	50.449306
219.090975	153.842018	50.454311
215.664521	131.125031	50.459316
212.070953	130.400618	50.464321
208.531621	144.291637	50.469325
205.319241	129.670086	50.474330
201.312595	137.825834	50.479335
198.258518	130.492252	50.484340
195.331429	136.605736	50.489345
191.508924	126.758709	50.494349
187.864667	136.312122	50.499354
183.813652	137.679035	50.504359
180.677977	127.183031	50.509364
177.549192	129.306186	50.514369
173.779131	123.549246	50.519373
170.289953	127.106615	50.524378
166.431882	128.317353	50.529383
163.323614	133.246830	50.534388
159.521477	129.371820	50.539393
155.858264	126.282438	50.544397
152.737571	127.372333	50.549402
149.131612	121.000408	50.554407
146.042763	130.165014	50.559412
142.202831	128.978108	50.564417
138.677606	122.134200	50.569421
135.562080	122.260669	50.574426
132.211973	131.572433	50.579431
128.484494	127.587242	50.584436
124.643367	127.547116	50.589441
120.933205	140.629107	50.594445
117.579769	140.442203	50.599450
113.966922	126.845325	50.604455
110.830117	127.388392	50.609460
107.259970	137.641001	50.614465
103.567249	139.548190	50.619469
100.215545	134.078015	50.624474
96.484093	136.559073	50.629479
92.896659	121.499495	50.634484
89.964842	130.876822	50.639489
86.375061	130.745859	50.644493
82.900537	130.170254	50.649498
78.975976	127.430627	50.654503
75.578052	135.675272	50.659508
72.022508	137.058741	50.664513
68.519465	132.968131	50.669517
65.133673	124.748466	50.674522
61.419284	134.763691	50.679527
58.240288	124.866064	50.684532
54.790158	126.152014	50.689537
50.718153	126.606662	50.694541
47.421413	125.530718	50.699546
43.862190	121.608344	50.704551
40.837554	129.499987	50.709556
37.174918	124.390223	50.714561
33.772089	131.799001	50.719565
30.615974	124.369615	50.724570
26.639980	130.996660	50.729575
23.113368	130.283390	50.734580
19.670070	121.686037	50.739585
15.867885	124.129895	50.744589
12.846633	116.192854	50.749594
8.686540	136.951907	50.754599
5.556159	128.219880	50.759604
2.265844	122.591639	50.764609