Thu Jun 16 19:01:19 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.356422	84.064734	0.000000
0.660723	95.003862	0.005005
0.821794	94.807892	0.010010
0.499666	100.536296	0.015014
0.477076	92.787360	0.020019
0.712205	79.799681	0.025024
0.297016	90.149562	0.030029
0.323134	70.099982	0.035034
-0.164370	70.845813	0.040038
-0.751288	55.888216	0.045043
-0.695913	50.777369	0.050048
-1.128947	46.747103	0.055053
-1.362654	26.209460	0.060058
-1.789457	26.122775	0.065062
-1.719642	32.909072	0.070067
-2.081104	21.131379	0.075072
-2.517609	15.035967	0.080077
-3.112374	10.387533	0.085082
-3.249950	11.807156	0.090086
-3.614139	5.439152	0.095091
-3.356921	8.682470	0.100096
-3.804523	15.582481	0.105101
-4.494370	10.662083	0.110106
-4.570710	16.486179	0.115110
-4.654537	9.436013	0.120115
-4.693519	11.231988	0.125120
-5.002148	15.958957	0.130125
-5.180907	14.778046	0.135130
-6.002341	17.104160	0.140134
-6.483855	10.396145	0.145139
-6.280204	9.718413	0.150144
-6.703652	14.765056	0.155149
-6.451448	18.269355	0.160154
-6.839527	23.575043	0.165158
-7.390763	23.732572	0.170163
-7.815438	18.853391	0.175168
-8.101643	18.290450	0.180173
-8.113079	10.213561	0.185178
-8.305863	21.045563	0.190182
-8.424586	16.847839	0.195187
-7.950653	4.935457	0.200192
-8.722980	10.624873	0.205197
-9.136852	7.224616	0.210202
-9.837639	23.056129	0.215206
-9.653166	16.064322	0.220211
-9.588358	3.985445	0.225216
-10.670323	13.640443	0.230221
-11.060890	6.162201	0.235226
-10.882838	13.675542	0.240230
-11.051994	15.477934	0.245235
-11.324367	6.074747	0.250240
-11.478021	14.339602	0.255245
-11.470886	11.262415	0.260250
-11.377196	19.146039	0.265254
-12.155143	12.344456	0.270259
-12.475928	24.359862	0.275264
-12.875420	17.346963	0.280269
-12.830860	13.004266	0.285274
-13.077296	17.517039	0.290278
-13.508298	14.916049	0.295283
-14.117778	18.286714	0.300288
-14.776984	19.258524	0.305293
-14.332788	15.735305	0.310298
-14.585621	17.835455	0.315302
-14.633552	19.491635	0.320307
-14.630395	9.696931	0.325312
-14.946435	21.221138	0.330317
-15.291902	12.014412	0.335322
-15.733801	5.224087	0.340326
-16.277961	4.901678	0.345331
-16.129393	11.836052	0.350336
-16.306013	11.255002	0.355341
-16.425932	10.471120	0.360346
-17.315251	14.420271	0.365350
-17.665626	22.216870	0.370355
-18.110623	18.217989	0.375360
-17.955639	21.481163	0.380365
-17.751334	20.429126	0.385370
-17.408034	18.425780	0.390374
-18.255145	13.869561	0.395379
-18.949587	5.808176	0.400384
-19.014100	18.253583	0.405389
-18.798472	12.788733	0.410394
-19.348309	4.833478	0.415398
-20.596958	15.438740	0.420403
-20.233623	12.062956	0.425408
-20.348499	11.288797	0.430413
-20.651439	2.023947	0.435418
-20.694976	9.771509	0.440422
-20.924976	9.150743	0.445427
-20.740261	-2.688482	0.450432
-21.526361	12.170673	0.455437
-22.085096	3.373887	0.460442
-22.241662	19.570649	0.465446
-22.451261	8.115038	0.470451
-22.229332	-0.213307	0.475456
-22.480235	17.458931	0.480461
-22.916460	20.897941	0.485466
-23.559796	16.676521	0.490470
-24.329932	22.658683	0.495475
-24.283813	15.631929	0.500480
-24.378213	16.015056	0.505485
-23.866439	21.572373	0.510490
-24.086302	7.192761	0.515494
-24.052600	20.252043	0.520499
-24.827313	12.464863	0.525504
-25.382776	22.941860	0.530509
-25.356504	9.983333	0.535514
-25.935045	6.366319	0.540518
-25.575361	-4.237859	0.545523
-26.482352	13.816565	0.550528
-27.016729	6.690315	0.555533
-27.158696	8.419451	0.560538
-27.358401	6.196266	0.565542
-27.289266	11.764479	0.570547
-27.035614	5.380401	0.575552
-27.288452	14.526649	0.580557
-27.925484	5.239270	0.585562
-28.204629	4.545532	0.590566
-28.625971	8.076197	0.595571
-28.609521	4.902665	0.600576
-29.087166	5.811915	0.605581
-28.811219	10.883951	0.610586
-29.401571	22.313106	0.615590
-29.822133	17.339625	0.620595
-29.811321	5.823323	0.625600
-30.219013	16.076612	0.630605
-30.781800	6.456830	0.635610
-31.350583	7.517187	0.640614
-31.611391	16.960815	0.645619
-31.678644	21.775949	0.650624
-32.016149	23.179879	0.655629
-31.725774	22.630863	0.660634
-32.024415	21.220662	0.665638
-31.967536	17.640401	0.670643
-31.934018	15.365255	0.675648
-32.601385	23.713729	0.680653
-32.984709	21.269121	0.685658
-32.819362	14.544772	0.690662
-33.419902	21.679800	0.695667
-33.763467	14.749115	0.700672
-34.728650	17.820252	0.705677
-34.660101	9.298928	0.710682
-35.133050	14.588746	0.715686
-35.103292	14.188559	0.720691
-34.884373	12.943999	0.725696
-35.281261	21.183647	0.730701
-35.188246	3.945809	0.735706
-34.998205	21.606245	0.740710
-36.109873	13.120539	0.745715
-36.083990	16.041504	0.750720
-36.783242	19.522207	0.755725
-36.731070	8.097920	0.760730
-37.059264	19.621963	0.765734
-37.351981	28.364900	0.770739
-37.923799	14.942782	0.775744
-38.557313	19.502458	0.780749
-38.525785	21.514376	0.785754
-38.449170	25.937655	0.790758
-38.491751	27.780692	0.795763
-38.441905	31.348228	0.800768
-38.705407	25.775212	0.805773
-38.814290	19.763677	0.810778
-39.568878	22.684389	0.815782
-39.922959	26.290955	0.820787
-40.087235	18.831546	0.825792
-39.822736	24.017944	0.830797
-40.766200	18.446514	0.835802
-41.217693	16.739665	0.840806
-41.316428	22.112861	0.845811
-41.293939	19.025736	0.850816
-41.609427	15.451572	0.855821
-41.660705	20.599195	0.860826
-41.312968	11.479858	0.865830
-42.188156	9.510565	0.870835
-42.543896	7.355293	0.875840
-43.156975	18.251224	0.880845
-42.838374	7.399103	0.885850
-43.066742	17.413117	0.890854
-44.055490	22.185205	0.895859
-44.283407	6.989772	0.900864
-44.282043	24.122710	0.905869
-44.623028	24.466975	0.910874
-44.618502	20.243852	0.915878
-44.438508	24.757777	0.920883
-44.733439	7.886524	0.925888
-44.780749	21.676213	0.930893
-45.519978	18.569458	0.935898
-45.767012	23.739962	0.940902
-45.964496	25.830669	0.945907
-46.089896	24.145498	0.950912
-46.702202	19.871993	0.955917
-47.263211	27.074876	0.960922
-47.521842	16.055625	0.965926
-47.919510	22.653791	0.970931
-47.632227	9.228115	0.975936
-47.693090	15.519935	0.980941
-47.891158	13.721089	0.985946
-47.724302	17.748448	0.990950
-48.582509	28.965767	0.995955
-49.166477	17.765583	1.000960
-49.545001	25.309149	1.005965
-49.596926	12.008390	1.010970
-49.913843	10.304952	1.015974
-50.001478	21.167125	1.020979
-49.825786	12.121898	1.025984
-49.822080	22.202431	1.030989
-50.228492	19.758779	1.035994
-50.940153	19.515157	1.040998
-51.087428	21.355271	1.046003
-51.273648	15.944599	1.051008
-51.418497	25.258476	1.056013
-51.886232	23.676051	1.061018
-52.400416	19.843396	1.066022
-52.669000	25.828403	1.071027
-52.877070	18.804887	1.076032
-53.004118	16.439075	1.081037
-52.870193	30.217465	1.086042
-53.171367	1.804180	1.091046
-53.258335	29.496003	1.096051
-53.584500	16.333792	1.101056
-54.027919	17.417532	1.106061
-54.348221	15.441182	1.111066
-54.512660	13.985522	1.116070
-54.901903	17.718947	1.121075
-55.182595	11.474376	1.126080
-55.996081	12.645319	1.131085
-56.076924	9.716745	1.136090
-55.939968	13.165404	1.141094
-56.224636	16.452695	1.146099
-55.920803	14.879197	1.151104
-56.071080	25.095278	1.156109
-56.258198	23.602423	1.161114
-57.218196	7.867980	1.166118
-57.719360	23.195918	1.171123
-57.406596	18.279713	1.176128
-57.835923	20.006126	1.181133
-58.048000	21.612089	1.186138
-58.798673	18.415084	1.191142
-59.110722	31.023934	1.196147
-59.017134	17.677616	1.201152
-59.488418	26.283533	1.206157
-59.547693	19.345427	1.211162
-59.469430	10.425908	1.216166
-59.702130	25.763247	1.221171
-59.498701	17.042348	1.226176
-60.561842	19.371616	1.231181
-60.381514	11.567684	1.236186
-60.630520	6.063707	1.241190
-61.088892	19.638485	1.246195
-61.038095	6.784235	1.251200
-62.065546	23.535128	1.256205
-62.259293	13.622618	1.261210
-62.215278	11.360437	1.266214
-62.723194	18.148481	1.271219
-62.212708	10.505348	1.276224
-62.487610	13.343824	1.281229
-62.842874	11.809602	1.286234
-63.603471	9.347834	1.291238
-64.365174	19.079049	1.296243
-64.087865	14.670166	1.301248
-64.393296	20.132570	1.306253
-64.341215	14.886435	1.311258
-64.097562	17.834844	1.316262
-64.459058	22.243217	1.321267
-64.707066	1.539683	1.326272
-65.640956	18.625923	1.331277
-65.751476	20.217667	1.336282
-65.641876	16.051073	1.341286
-65.835032	24.677911	1.346291
-66.085482	13.411663	1.351296
-67.111043	17.790384	1.356301
-67.114721	11.663997	1.361306
-67.204760	4.521243	1.366310
-67.117417	8.913936	1.371315
-67.119292	13.432657	1.376320
-68.297283	13.394160	1.381325
-68.501688	11.040543	1.386330
-68.696777	14.957341	1.391334
-68.755385	10.837293	1.396339
-68.685036	-3.615520	1.401344
-68.952766	14.809163	1.406349
-68.943008	14.125887	1.411354
-69.613594	9.418666	1.416358
-70.273609	13.544203	1.421363
-70.339442	6.357394	1.426368
-70.375457	14.508885	1.431373
-70.715032	15.345993	1.436378
-70.493425	4.861115	1.441382
-71.219669	23.341559	1.446387
-71.636067	8.400042	1.451392
-72.308438	23.614112	1.456397
-72.387007	15.022394	1.461402
-72.317276	14.562129	1.466406
-72.474892	16.173199	1.471411
-72.324240	18.278684	1.476416
-72.476718	17.518731	1.481421
-72.619748	15.183777	1.486426
-73.353251	17.604380	1.491430
-73.788975	16.663840	1.496435
-73.687159	2.943166	1.501440
-73.872554	12.565616	1.506445
-74.432077	17.017074	1.511450
-74.938683	10.091835	1.516454
-75.443227	14.059086	1.521459
-75.082886	3.572690	1.526464
-75.353873	13.888620	1.531469
-75.583150	13.561924	1.536474
-75.461074	4.815313	1.541478
-76.187361	30.080529	1.546483
-76.596890	13.349365	1.551488
-77.034012	10.719107	1.556493
-77.139917	0.870816	1.561498
-77.145036	1.705626	1.566502
-77.478316	8.313467	1.571507
-77.207003	0.853705	1.576512
-77.340719	6.390424	1.581517
-78.464820	7.300463	1.586522
-78.570889	8.849641	1.591526
-78.630288	8.162898	1.596531
-78.533848	1.946669	1.601536
-78.989499	14.338915	1.606541
-80.079088	8.519163	1.611546
-80.311720	12.649537	1.616550
-80.485599	15.661820	1.621555
-79.869843	18.829896	1.626560
-80.146831	8.312289	1.631565
-80.494346	5.284839	1.636570
-80.459504	9.271662	1.641574
-81.147441	10.860279	1.646579
-81.359404	-4.858667	1.651584
-81.747971	16.736512	1.656589
-81.897327	8.393860	1.661594
-81.915940	8.972130	1.666598
-82.334182	12.152654	1.671603
-83.048059	6.877732	1.676608
-83.028374	15.036788	1.681613
-83.399874	13.326785	1.686618
-83.142769	14.640929	1.691622
-83.824071	22.118516	1.696627
-83.365962	11.567517	1.701632
-84.185354	14.570070	1.706637
-84.573705	8.778265	1.711642
-84.631231	8.759201	1.716646
-85.111016	20.163371	1.721651
-84.988931	15.850580	1.726656
-85.146977	24.500026	1.731661
-85.883506	20.123443	1.736666
-85.873089	20.986762	1.741670
-86.463681	20.980821	1.746675
-86.737096	8.888987	1.751680
-86.705560	22.658735	1.756685
-86.673192	3.639561	1.761690
-86.571634	5.904493	1.766694
-87.847779	22.943912	1.771699
-87.715805	6.830616	1.776704
-88.229851	15.698615	1.781709
-87.955776	5.938562	1.786714
-88.308663	4.706622	1.791718
-88.440114	13.193129	1.796723
-89.142126	6.859955	1.801728
-89.405078	17.774575	1.806733
-89.933388	13.230990	1.811738
-89.537694	7.731551	1.816742
-89.958690	18.298984	1.821747
-89.916167	14.147127	1.826752
-90.252111	13.365407	1.831757
-90.888129	16.604615	1.836762
-91.096045	16.429178	1.841766
-91.425593	20.290558	1.846771
-91.582024	8.987569	1.851776
-91.717057	17.809898	1.856781
-91.837002	10.141819	1.861786
-91.326260	12.803294	1.866790
-92.732586	8.356777	1.871795
-92.928676	1.411894	1.876800
-93.051787	16.376347	1.881805
-93.276015	14.486723	1.886810
-92.973846	6.096382	1.891814
-93.530518	16.835698	1.896819
-93.548808	17.245610	1.901824
-94.263974	16.225077	1.906829
-94.173886	11.658213	1.911834
-94.344784	13.360859	1.916838
-95.727073	24.760782	1.921843
-95.908252	17.203645	1.926848
-95.862557	13.656608	1.931853
-95.670558	12.953276	1.936858
-96.037040	11.644757	1.941862
-96.097549	26.025000	1.946867
-95.752852	20.385706	1.951872
-96.265318	17.025527	1.956877
-97.187529	23.051373	1.961882
-97.347688	18.996842	1.966886
-97.763743	19.560395	1.971891
-97.822855	5.391396	1.976896
-97.902933	12.163776	1.981901
-98.134644	16.526922	1.986906
-98.202491	14.957039	1.991910
-99.043450	19.222089	1.996915
-99.106763	17.563413	2.006912
-98.837276	19.482368	2.016909
-98.350489	26.009093	2.026906
-97.716033	26.900221	2.036902
-96.735133	18.806432	2.046899
-96.437238	11.169533	2.056896
-96.499305	10.999149	2.066893
-96.004611	13.845970	2.076890
-95.387923	18.396205	2.086886
-94.659797	17.684001	2.096883
-93.890921	11.674662	2.106880
-93.713214	17.782320	2.116877
-93.497170	15.867635	2.126874
-92.582618	19.372340	2.136870
-92.427404	21.618032	2.146867
-91.497724	22.618960	2.156864
-91.263343	26.408354	2.166861
-91.103651	26.653192	2.176858
-89.885391	25.056598	2.186854
-89.441214	22.521945	2.196851
-89.278034	27.051664	2.206848
-88.864433	21.101829	2.216845
-88.037472	22.790505	2.226842
-88.151936	16.226107	2.236838
-87.151539	21.088691	2.246835
-86.391182	11.458569	2.256832
-86.373430	15.030192	2.266829
-85.585856	14.550522	2.276826
-84.797836	19.459367	2.286822
-84.768569	11.644063	2.296819
-84.314261	21.843590	2.306816
-83.410801	16.082469	2.316813
-83.114799	17.727321	2.326810
-83.072405	21.910969	2.336806
-81.977788	11.621855	2.346803
-81.733631	17.201859	2.356800
-81.523821	13.913720	2.366797
-80.493275	5.366233	2.376794
-80.391648	19.620318	2.386790
-79.481807	12.196800	2.396787
-78.804830	10.001807	2.406784
-78.622145	17.521752	2.416781
-78.577245	13.446568	2.426778
-77.659469	19.846649	2.436774
-77.402822	19.905808	2.446771
-76.629821	15.421456	2.456768
-75.781394	20.078110	2.466765
-75.701877	19.362171	2.476762
-75.004897	16.541652	2.486758
-74.156020	19.891460	2.496755
-74.300715	9.047988	2.506752
-73.914198	12.936798	2.516749
-73.134560	20.745358	2.526746
-72.634882	22.844676	2.536742
-72.340620	11.847309	2.546739
-71.394492	16.164803	2.556736
-70.922498	10.147682	2.566733
-70.892675	20.945594	2.576730
-70.219153	15.428088	2.586726
-69.430224	23.856791	2.596723
-69.364666	14.635911	2.606720
-68.552363	16.676597	2.616717
-67.925220	21.168903	2.626714
-67.986129	12.211876	2.636710
-66.917974	15.058559	2.646707
-66.323393	17.868428	2.656704
-66.236109	7.623407	2.666701
-65.962861	14.449317	2.676698
-65.083351	15.468666	2.686694
-64.812199	20.370477	2.696691
-63.945772	5.819103	2.706688
-63.359017	15.399858	2.716685
-63.070061	16.932130	2.726682
-62.807090	20.520225	2.736678
-62.180784	18.659090	2.746675
-61.786226	17.742865	2.756672
-60.759539	14.591568	2.766669
-60.232291	17.393353	2.776666
-60.068681	14.938113	2.786662
-60.126250	19.095757	2.796659
-59.213181	15.879421	2.806656
-58.793894	22.795786	2.816653
-57.402633	13.317584	2.826650
-57.826011	15.175365	2.836646
-57.163970	20.754421	2.846643
-56.843613	19.377645	2.856640
-56.027310	18.002326	2.866637
-55.845328	20.567547	2.876634
-54.965166	16.215041	2.886630
-54.315511	15.062899	2.896627
-53.889478	11.458143	2.906624
-53.943669	14.002928	2.916621
-53.061947	14.320027	2.926618
-52.630462	21.915568	2.936614
-52.290006	20.718807	2.946611
-51.267563	20.577026	2.956608
-51.065125	10.974654	2.966605
-50.817840	15.394656	2.976602
-49.696785	12.256757	2.986598
-49.460513	8.485653	2.996595
-49.430924	8.802569	3.006592
-48.118443	7.807546	3.016589
-47.989233	19.214267	3.026586
-47.956070	13.159083	3.036582
-47.342528	16.687958	3.046579
-46.452079	11.808240	3.056576
-46.099109	3.790430	3.066573
-45.194164	9.173711	3.076570
-45.163852	6.481350	3.086566
-44.561395	3.537670	3.096563
-44.132266	5.168869	3.106560
-43.075965	15.364087	3.116557
-42.738035	13.559255	3.126554
-42.633022	10.919150	3.136550
-42.772200	11.448628	3.146547
-41.713751	17.127632	3.156544
-41.153157	16.067950	3.166541
-40.026443	18.489835	3.176538
-39.763896	17.354797	3.186534
-39.763899	24.233232	3.196531
-39.259434	17.637319	3.206528
-38.566942	18.022785	3.216525
-38.113674	19.148487	3.226522
-37.587036	18.518730	3.236518
-36.729013	14.363841	3.246515
-36.566582	16.280587	3.256512
-36.155814	11.313154	3.266509
-35.423861	12.536081	3.276506
-34.774363	15.245901	3.286502
-34.707338	14.029727	3.296499
-33.983847	14.685619	3.306496
-33.081479	23.116277	3.316493
-32.983750	22.908963	3.326490
-33.027993	16.751885	3.336486
-32.412348	12.394003	3.346483
-31.655148	8.243874	3.356480
-30.688227	9.482103	3.366477
-30.412393	12.161414	3.376474
-30.472305	15.707547	3.386470
-29.281968	22.325057	3.396467
-28.843259	12.372822	3.406464
-28.901473	11.430718	3.416461
-27.873062	6.613649	3.426458
-27.537729	19.953676	3.436454
-27.328883	19.187471	3.446451
-26.209332	18.569970	3.456448
-25.932262	18.749330	3.466445
-25.755104	19.422808	3.476442
-24.529620	27.071317	3.486438
-24.377040	26.705434	3.496435
-24.118070	19.223823	3.506432
-23.918867	21.271750	3.516429
-23.074805	18.598856	3.526426
-22.580477	7.979502	3.536422
-21.836157	11.928514	3.546419
-21.121149	15.951865	3.556416
-20.885145	15.202163	3.566413
-20.809161	17.647301	3.576410
-19.822380	14.730047	3.586406
-19.368119	12.196251	3.596403
-19.154045	4.480251	3.606400
-18.583586	13.474924	3.616397
-17.849298	17.018619	3.626394
-17.621673	14.614637	3.636390
-17.117560	9.293849	3.646387
-16.176971	13.550135	3.656384
-15.981814	9.620022	3.666381
-15.499103	23.334329	3.676378
-14.691075	14.069818	3.686374
-14.362787	15.794538	3.696371
-14.094008	12.297610	3.706368
-13.725688	10.157039	3.716365
-13.043879	10.938507	3.726362
-12.664174	11.968894	3.736358
-11.435285	12.691315	3.746355
-11.193170	21.205801	3.756352
-11.124851	14.534191	3.766349
-11.018985	15.417605	3.776346
-9.853148	11.195206	3.786342
-9.401815	11.225504	3.796339
-9.279491	10.463670	3.806336
-8.362967	9.137633	3.816333
-7.771704	8.999253	3.826330
-7.584420	17.968696	3.836326
-6.709292	18.761335	3.846323
-6.582058	16.624056	3.856320
-6.199897	9.808964	3.866317
-5.064295	13.801186	3.876314
-4.917023	12.890960	3.886310
-4.893812	21.287970	3.896307
-3.961660	17.057909	3.906304
-3.543273	13.749624	3.916301
-3.196532	16.263813	3.926298
-2.548006	37.549601	3.936294
-2.231953	47.639887	3.946291
-1.741285	49.997338	3.956288
-1.337175	60.033865	3.966285
-0.757860	70.379672	3.976282
-0.471854	82.928969	3.986278
-0.235542	107.599656	3.996275
0.000000	106.849483	4.001280
0.362996	130.823812	4.006285
0.915034	136.035245	4.011290
1.062441	147.620289	4.016294
1.209976	150.089856	4.021299
1.276870	151.107618	4.026304
1.306932	153.442005	4.031309
1.205393	143.272262	4.036314
1.267582	149.824282	4.041318
1.258638	157.089303	4.046323
1.067546	151.321462	4.051328
1.123159	169.113306	4.056333
1.209921	172.210108	4.061338
1.518053	191.369047	4.066342
1.475661	190.362701	4.071347
1.653107	178.740789	4.076352
1.389834	183.874470	4.081357
1.574799	190.494614	4.086362
1.616053	180.652166	4.091366
1.443541	162.026730	4.096371
1.545230	168.000719	4.101376
1.370875	159.497253	4.106381
1.809341	171.732993	4.111386
1.469952	160.274049	4.116390
1.306716	161.690230	4.121395
1.832769	158.162529	4.126400
1.116396	162.805983	4.131405
1.256664	174.374074	4.136410
1.806366	184.403655	4.141414
1.482197	191.946115	4.146419
2.075944	184.952399	4.151424
1.862305	179.887544	4.156429
1.752225	155.252456	4.161434
1.493287	157.642988	4.166438
1.351828	162.070087	4.171443
1.401848	162.207968	4.176448
1.548260	186.135798	4.181453
1.707319	181.022967	4.186458
1.663459	185.108084	4.191462
1.600839	190.213640	4.196467
1.922619	182.003261	4.201472
1.499408	188.568723	4.206477
1.871212	180.721320	4.211482
1.877893	186.935064	4.216486
2.002404	199.116653	4.221491
1.890592	191.445650	4.226496
1.678326	190.355994	4.231501
2.230146	194.310906	4.236506
1.682782	204.806815	4.241510
1.750019	192.240620	4.246515
1.516106	186.985453	4.251520
1.679504	186.451596	4.256525
1.691820	191.775129	4.261530
1.610662	197.884514	4.266534
1.372143	192.279286	4.271539
2.275059	182.075822	4.276544
1.496925	185.653747	4.281549
1.743742	192.561216	4.286554
1.932854	192.579725	4.291558
1.959189	194.825155	4.296563
2.177309	193.910619	4.301568
1.910185	201.055052	4.306573
1.848299	191.346845	4.311578
1.727944	193.113866	4.316582
1.931235	219.127596	4.321587
2.164223	212.574593	4.326592
2.168485	225.321444	4.331597
2.247752	206.000456	4.336602
2.281913	218.057294	4.341606
1.812899	211.488300	4.346611
2.052279	209.271644	4.351616
2.239728	221.050594	4.356621
2.130134	222.127420	4.361626
2.394886	222.891303	4.366630
2.005473	227.955377	4.371635
2.184954	222.810843	4.376640
1.958291	213.262249	4.381645
2.177754	221.145911	4.386650
2.277882	225.661949	4.391654
2.006497	224.922225	4.396659
2.108280	224.062824	4.401664
2.334450	230.069442	4.406669
2.305258	226.587904	4.411674
2.285940	227.584501	4.416678
2.065789	228.880855	4.421683
2.601920	230.798561	4.426688
2.335785	231.663101	4.431693
2.509721	231.415774	4.436698
2.552661	224.116666	4.441702
2.268704	221.395051	4.446707
2.630491	218.847892	4.451712
2.153404	224.829549	4.456717
1.930150	228.596759	4.461722
2.383477	221.823346	4.466726
2.456898	215.182665	4.471731
2.438858	213.923976	4.476736
2.097487	222.033900	4.481741
2.068514	226.187699	4.486746
2.244274	233.372312	4.491750
2.284629	229.033800	4.496755
2.056720	235.074122	4.501760
2.092512	246.253169	4.506765
2.490344	257.284788	4.511770
2.761179	259.031072	4.516774
2.487972	266.785840	4.521779
2.659312	267.604428	4.526784
2.337595	258.682688	4.531789
2.598828	253.945599	4.536794
2.552467	266.598741	4.541798
2.787720	267.768046	4.546803
2.738430	250.445118	4.551808
2.786851	250.775150	4.556813
2.381374	246.717388	4.561818
2.466613	254.991828	4.566822
2.696576	253.023757	4.571827
2.682798	246.262807	4.576832
2.385328	250.630178	4.581837
2.321476	258.876971	4.586842
2.553082	247.727400	4.591846
2.334022	256.609930	4.596851
2.575681	248.708724	4.601856
2.745210	258.643627	4.606861
2.558648	247.603709	4.611866
2.786833	260.756156	4.616870
2.900569	271.739334	4.621875
3.026102	260.388168	4.626880
2.755382	261.824784	4.631885
2.715770	257.880489	4.636890
2.882781	258.566408	4.641894
2.843566	261.986132	4.646899
2.824689	259.445246	4.651904
2.873305	261.073264	4.656909
3.041477	261.273999	4.661914
2.949679	260.559941	4.666918
2.788672	253.817400	4.671923
3.125493	255.641766	4.676928
2.804747	254.806609	4.681933
3.139284	263.914837	4.686938
2.838843	255.576784	4.691942
2.532408	254.408370	4.696947
3.040430	247.296988	4.701952
2.618336	263.318578	4.706957
2.749724	266.356230	4.711962
2.933430	283.491002	4.716966
3.068053	290.867914	4.721971
3.262308	287.875965	4.726976
3.302421	295.377020	4.731981
3.371068	287.048299	4.736986
3.282746	265.452293	4.741990
2.993667	264.435209	4.746995
2.992257	249.449426	4.752000
3.287223	245.862323	4.757005
3.163935	254.303126	4.762010
3.120783	258.590292	4.767014
2.879824	259.227612	4.772019
2.975830	261.384981	4.777024
2.961771	277.993838	4.782029
3.239916	282.366822	4.787034
3.163694	289.599023	4.792038
3.052217	297.350856	4.797043
3.539217	292.778099	4.802048
3.426362	279.675012	4.807053
3.175259	287.397330	4.812058
3.080381	282.746113	4.817062
3.373206	293.237408	4.822067
3.584687	290.275957	4.827072
3.285423	282.700407	4.832077
3.416981	291.537544	4.837082
3.390406	297.792148	4.842086
3.283989	289.592195	4.847091
3.782517	279.026044	4.852096
3.513796	277.113349	4.857101
3.236979	263.569839	4.862106
3.226673	260.152554	4.867110
3.077476	275.028648	4.872115
3.574134	283.863456	4.877120
3.342800	301.782094	4.882125
3.364204	293.653950	4.887130
3.455658	285.822141	4.892134
3.062289	293.370067	4.897139
3.163715	291.140780	4.902144
3.215901	285.127579	4.907149
3.198861	285.858812	4.912154
3.476961	290.619328	4.917158
3.309504	292.691692	4.922163
3.125043	290.257582	4.927168
3.260279	297.026180	4.932173
3.741436	307.042112	4.937178
3.953691	318.522943	4.942182
3.479453	314.127085	4.947187
3.399680	312.079965	4.952192
3.682569	319.464947	4.957197
3.839679	323.044226	4.962202
3.665092	323.173548	4.967206
3.780347	328.988790	4.972211
4.323507	316.442305	4.977216
3.713787	302.547507	4.982221
3.622448	290.940727	4.987226
3.658177	293.930659	4.992230
3.646557	300.469290	4.997235
3.485236	291.015313	5.002240
3.458689	297.546939	5.007245
3.784139	328.391403	5.012250
3.735218	312.103152	5.017254
3.941629	327.339820	5.022259
3.888737	308.464568	5.027264
3.578066	315.303509	5.032269
3.814383	312.950607	5.037274
4.179539	320.919654	5.042278
3.573602	310.853576	5.047283
3.611500	315.337995	5.052288
3.807529	316.350608	5.057293
3.915816	315.197906	5.062298
4.304568	320.555170	5.067302
3.803160	328.964086	5.072307
4.030309	313.735560	5.077312
3.857094	320.708750	5.082317
3.940693	334.017649	5.087322
4.201652	322.690426	5.092326
4.078566	324.451205	5.097331
4.101702	312.106976	5.102336
3.633471	311.354494	5.107341
3.703908	299.676973	5.112346
3.970316	309.726619	5.117350
3.853422	328.552759	5.122355
4.067534	317.463250	5.127360
3.678764	325.370331	5.132365
3.855578	313.116922	5.137370
4.428647	318.666098	5.142374
3.871729	321.002309	5.147379
3.888209	318.424493	5.152384
3.716412	315.281511	5.157389
3.692481	324.222597	5.162394
3.916231	323.385457	5.167398
4.045897	354.845586	5.172403
4.236627	340.625798	5.177408
4.329453	358.119194	5.182413
4.188397	348.549067	5.187418
4.492664	350.311542	5.192422
4.294118	343.085531	5.197427
4.217834	337.983324	5.202432
4.184732	346.799362	5.207437
4.352790	346.219940	5.212442
4.321050	351.696624	5.217446
4.039101	352.937594	5.222451
4.370881	350.932953	5.227456
4.414416	358.027896	5.232461
4.352717	356.320221	5.237466
4.485710	345.457097	5.242470
4.567483	354.205222	5.247475
4.389047	322.244657	5.252480
4.258603	316.352191	5.257485
4.128489	335.135142	5.262490
4.299531	337.362204	5.267494
4.101583	355.042261	5.272499
4.066772	353.701290	5.277504
4.248747	356.570875	5.282509
4.025024	367.098452	5.287514
4.436672	357.204942	5.292518
4.101944	355.881667	5.297523
4.326357	364.874474	5.302528
4.140258	357.590362	5.307533
4.487896	368.841087	5.312538
4.563073	380.891473	5.317542
4.569945	379.805249	5.322547
4.819274	382.595635	5.327552
4.608051	373.863537	5.332557
4.155020	360.274971	5.337562
4.491672	370.327551	5.342566
4.492458	380.693826	5.347571
4.693237	397.454461	5.352576
4.699161	394.938359	5.357581
4.648191	393.224567	5.362586
4.975246	392.645308	5.367590
4.683214	395.459651	5.372595
4.938431	390.602364	5.377600
4.633894	376.673443	5.382605
4.435241	378.213688	5.387610
4.656098	384.310332	5.392614
4.962583	383.349415	5.397619
4.850730	384.660343	5.402624
4.565773	390.138831	5.407629
4.779287	383.462002	5.412634
4.877300	389.272718	5.417638
4.612495	401.817538	5.422643
4.602900	395.411490	5.427648
4.573618	387.285358	5.432653
4.816953	393.101953	5.437658
4.997406	382.028121	5.442662
4.848038	396.204489	5.447667
5.223184	388.085516	5.452672
4.815484	392.166687	5.457677
4.863789	390.442014	5.462682
5.078470	388.052818	5.467686
4.718431	392.255552	5.472691
4.970722	385.458464	5.477696
5.082892	388.620467	5.482701
4.885190	386.487460	5.487706
5.088979	388.492369	5.492710
4.931643	393.709440	5.497715
4.602731	386.122263	5.502720
4.783161	395.477817	5.507725
4.863750	386.262805	5.512730
4.810039	389.658415	5.517734
4.813346	394.930923	5.522739
5.017469	392.604935	5.527744
4.818874	387.682353	5.532749
4.637316	386.263816	5.537754
4.859792	395.325133	5.542758
4.431522	399.346466	5.547763
4.930222	406.050017	5.552768
4.921275	411.087779	5.557773
4.740634	404.456050	5.562778
5.211467	406.221983	5.567782
4.887351	416.221991	5.572787
4.925259	404.439960	5.577792
5.017605	416.606517	5.582797
4.957990	413.652354	5.587802
5.073578	421.194568	5.592806
5.050114	433.570685	5.597811
5.103584	447.601209	5.602816
5.121853	449.959986	5.607821
5.212129	447.099533	5.612826
5.745080	433.458853	5.617830
5.286954	435.870803	5.622835
5.482959	442.340357	5.627840
5.392286	450.116650	5.632845
5.096359	440.349390	5.637850
5.551317	444.182552	5.642854
5.282066	446.574931	5.647859
5.392892	443.806781	5.652864
5.404486	439.072611	5.657869
5.318985	439.330758	5.662874
5.514519	437.910672	5.667878
5.364871	443.907559	5.672883
5.372198	438.946689	5.677888
5.725169	439.571796	5.682893
5.498292	445.633241	5.687898
5.446325	432.684719	5.692902
5.284931	443.094510	5.697907
5.434390	444.884749	5.702912
5.367566	446.479773	5.707917
5.225715	453.089714	5.712922
5.499196	435.856882	5.717926
5.466751	447.501077	5.722931
5.509238	445.351455	5.727936
5.927697	449.361228	5.732941
5.440613	446.574187	5.737946
5.485530	445.203655	5.742950
5.654927	437.179529	5.747955
5.853481	441.700478	5.752960
5.882711	442.428808	5.757965
5.709745	429.583551	5.762970
5.769874	436.711995	5.767974
5.569393	449.622897	5.772979
5.797664	441.301158	5.777984
5.673529	445.923677	5.782989
5.845364	444.721791	5.787994
5.650242	434.536143	5.792998
5.502703	453.270619	5.798003
5.668754	439.800767	5.803008
5.637068	437.866440	5.808013
5.580114	446.493701	5.813018
5.912084	442.294189	5.818022
5.594361	452.484165	5.823027
5.812203	443.712692	5.828032
5.587330	446.420248	5.833037
5.540619	442.713954	5.838042
5.562935	443.722134	5.843046
5.528753	450.987321	5.848051
5.664754	438.436594	5.853056
5.671232	456.749020	5.858061
5.752039	481.301603	5.863066
5.603142	470.863227	5.868070
5.698838	481.460727	5.873075
5.785175	487.118320	5.878080
5.885887	483.422578	5.883085
5.811657	476.801153	5.888090
6.248309	475.552443	5.893094
5.846072	477.725587	5.898099
5.986669	479.879860	5.903104
5.839000	488.613493	5.908109
5.886828	471.997426	5.913114
6.339097	476.086069	5.918118
6.008093	478.036117	5.923123
6.060271	466.620659	5.928128
6.205640	480.026126	5.933133
5.850535	474.519480	5.938138
6.450991	479.691954	5.943142
6.143825	482.807352	5.948147
6.111599	478.504540	5.953152
5.961224	482.415548	5.958157
5.869046	476.219047	5.963162
6.217365	474.654136	5.968166
5.799821	479.307790	5.973171
6.052432	483.818634	5.978176
6.013632	483.421575	5.983181
6.363060	471.254352	5.988186
6.114705	477.992697	5.993190
6.065755	477.040986	5.998195
6.086109	481.659370	6.003200
6.261827	482.541670	6.008205
6.226814	502.855961	6.013210
6.446948	492.206528	6.018214
6.066185	490.203995	6.023219
6.042215	496.015967	6.028224
6.163395	502.735183	6.033229
6.287049	525.781062	6.038234
6.370099	501.048487	6.043238
6.081902	508.245577	6.048243
6.660846	504.587709	6.053248
6.236347	486.954383	6.058253
5.981784	488.122468	6.063258
6.461778	498.957576	6.068262
6.149058	487.225433	6.073267
6.191102	481.923968	6.078272
6.092795	492.024435	6.083277
6.271372	508.968713	6.088282
6.580674	510.437657	6.093286
6.112996	496.408319	6.098291
6.248233	478.961013	6.103296
6.251157	480.353217	6.108301
6.179888	487.725082	6.113306
6.004388	490.190571	6.118310
5.688701	514.183930	6.123315
6.331086	507.768553	6.128320
6.222240	508.663053	6.133325
6.089847	513.687804	6.138330
6.400137	519.714474	6.143334
6.123105	511.586599	6.148339
6.012482	517.405006	6.153344
6.150019	519.735402	6.158349
5.922588	515.801261	6.163354
6.199076	510.903721	6.168358
6.435020	519.955585	6.173363
6.112613	513.342008	6.178368
6.590081	516.533448	6.183373
6.348586	522.117468	6.188378
6.395782	520.481163	6.193382
5.929970	515.415546	6.198387
6.249377	511.451417	6.203392
5.943712	507.830521	6.208397
6.209364	516.164277	6.213402
6.402565	515.731936	6.218406
6.030522	520.910341	6.223411
6.072649	525.042802	6.228416
6.177914	516.680083	6.233421
6.359466	525.611895	6.238426
6.281744	520.774662	6.243430
6.048162	526.160159	6.248435
6.186250	525.743930	6.253440
6.188838	519.040831	6.258445
6.236285	530.407384	6.263450
6.065885	513.036100	6.268454
6.100781	525.891989	6.273459
6.013973	527.174421	6.278464
6.112948	519.101709	6.283469
6.279770	519.759456	6.288474
6.689627	518.961006	6.293478
6.288973	532.436428	6.298483
6.251562	523.563051	6.303488
6.401754	523.288863	6.308493
6.405656	517.781673	6.313498
6.502511	511.965224	6.318502
6.137130	526.487094	6.323507
6.263822	521.668172	6.328512
6.169833	524.908767	6.333517
6.102167	514.394586	6.338522
6.637304	502.226938	6.343526
6.139393	517.752938	6.348531
6.127451	513.307854	6.353536
6.328280	514.382729	6.358541
6.115148	506.309017	6.363546
6.481670	507.436916	6.368550
6.106797	513.398634	6.373555
6.428345	513.838133	6.378560
6.284139	514.774587	6.383565
6.342883	527.505976	6.388570
6.165022	515.065559	6.393574
6.146772	522.409440	6.398579
6.337558	513.844548	6.403584
6.164158	518.226318	6.408589
6.265436	511.443870	6.413594
6.433222	516.378566	6.418598
6.247630	517.244905	6.423603
6.308978	514.558714	6.428608
6.464735	513.182685	6.433613
6.217804	513.938404	6.438618
6.392827	509.819565	6.443622
6.148605	517.305464	6.448627
6.350370	526.522016	6.453632
6.800716	514.406354	6.458637
6.615422	524.699097	6.463642
6.508477	492.440651	6.468646
5.979465	492.313925	6.473651
5.932470	476.292545	6.478656
6.487459	505.742202	6.483661
6.135881	497.440191	6.488666
6.185430	488.732316	6.493670
6.255903	501.219246	6.498675
6.089164	512.397524	6.503680
6.269825	513.118986	6.508685
6.166244	516.553349	6.513690
6.301431	510.016185	6.518694
6.203946	513.772447	6.523699
6.317726	504.617882	6.528704
6.150677	516.265233	6.533709
5.983975	503.169669	6.538714
6.344165	504.329988	6.543718
6.273972	512.940827	6.548723
6.075012	512.393144	6.553728
6.306566	512.483074	6.558733
6.231711	517.642555	6.563738
6.445187	507.202478	6.568742
6.292057	519.429119	6.573747
6.207595	514.925379	6.578752
6.416004	514.393644	6.583757
6.323047	521.487145	6.588762
6.504964	511.703324	6.593766
5.909893	506.509012	6.598771
6.210058	512.579282	6.603776
6.426788	514.736962	6.608781
6.350725	506.748332	6.613786
6.453057	489.127191	6.618790
6.034513	490.196981	6.623795
6.087075	485.527455	6.628800
6.472362	503.473767	6.633805
6.070572	503.056781	6.638810
6.005754	497.469006	6.643814
6.437725	517.973212	6.648819
6.238163	503.040645	6.653824
6.235679	502.110654	6.658829
6.248087	509.208245	6.663834
6.522209	511.401626	6.668838
6.214003	487.093437	6.673843
5.953933	484.813956	6.678848
6.419087	496.146676	6.683853
6.148457	496.801438	6.688858
6.327585	483.276209	6.693862
6.061053	491.425209	6.698867
6.275554	507.156177	6.703872
6.302703	506.258680	6.708877
6.224150	520.843839	6.713882
6.175001	509.997380	6.718886
6.155653	507.213339	6.723891
6.355298	509.444481	6.728896
6.182117	514.449729	6.733901
6.306062	522.716240	6.738906
6.614418	503.950150	6.743910
6.292733	509.943034	6.748915
5.859553	495.586272	6.753920
5.964224	499.595033	6.758925
6.222105	516.198177	6.763930
6.171728	515.178724	6.768934
6.348460	512.931633	6.773939
6.155710	514.765606	6.778944
6.295005	517.936472	6.783949
5.976318	521.301610	6.788954
6.432725	516.252394	6.793958
5.978220	516.997329	6.798963
6.185727	516.239027	6.803968
6.210306	513.817396	6.808973
5.766497	516.204103	6.813978
6.315536	514.517424	6.818982
6.213502	519.430609	6.823987
6.192148	507.258827	6.828992
6.341306	516.836374	6.833997
6.248322	520.147540	6.839002
6.386739	524.967913	6.844006
6.197546	517.905723	6.849011
6.347237	520.303763	6.854016
6.372053	523.895974	6.859021
6.114601	518.923783	6.864026
6.227030	511.816585	6.869030
6.581563	519.000894	6.874035
6.116356	521.303234	6.879040
6.754786	518.652003	6.884045
6.279807	520.783110	6.889050
6.810560	514.620785	6.894054
6.274607	515.450115	6.899059
6.704828	500.685376	6.904064
6.280562	491.622299	6.909069
6.124269	487.609914	6.914074
6.115872	498.187137	6.919078
5.983981	489.706562	6.924083
6.132294	490.048604	6.929088
6.163556	487.379623	6.934093
6.163361	486.805507	6.939098
6.325797	494.110341	6.944102
6.071376	489.006839	6.949107
5.771955	494.727196	6.954112
6.264933	505.008765	6.959117
6.243928	523.856591	6.964122
6.677160	527.791134	6.969126
6.583637	524.589792	6.974131
6.331630	502.443848	6.979136
6.346122	489.813219	6.984141
5.986211	491.905969	6.989146
6.018524	487.008633	6.994150
5.864764	500.189973	6.999155
6.178622	512.917668	7.004160
6.564609	523.749386	7.009165
6.305241	522.953596	7.014170
6.491430	511.795851	7.019174
6.337679	497.877616	7.024179
6.260765	490.540275	7.029184
6.275788	484.435861	7.034189
5.940129	491.208173	7.039194
6.272362	499.357872	7.044198
6.318934	499.304240	7.049203
6.163317	496.178870	7.054208
6.241109	481.006826	7.059213
6.300476	489.288924	7.064218
6.351573	500.223619	7.069222
6.218354	497.259504	7.074227
6.176415	490.146552	7.079232
6.160702	492.372633	7.084237
5.946632	499.103446	7.089242
6.460563	507.912937	7.094246
6.273411	518.151918	7.099251
6.437778	511.379072	7.104256
6.627755	494.480711	7.109261
6.007609	487.446047	7.114266
5.892324	477.703764	7.119270
5.817345	498.983902	7.124275
6.131579	511.779608	7.129280
6.474478	517.151621	7.134285
6.659417	519.678504	7.139290
6.418522	509.375964	7.144294
6.350586	499.272254	7.149299
5.856337	481.209165	7.154304
6.485323	496.051782	7.159309
6.173813	496.825572	7.164314
6.190261	484.418774	7.169318
6.179109	489.929496	7.174323
6.125663	496.747023	7.179328
6.400174	497.394471	7.184333
6.381500	499.007885	7.189338
6.444472	490.992933	7.194342
6.472071	491.007846	7.199347
6.150044	492.738872	7.204352
6.053414	480.224088	7.209357
5.959913	480.175747	7.214362
6.107757	497.798034	7.219366
6.124709	499.923415	7.224371
6.391536	519.223568	7.229376
6.459412	505.372883	7.234381
6.034536	489.266837	7.239386
6.492146	492.592670	7.244390
6.252726	490.253443	7.249395
6.289098	496.413077	7.254400
6.113116	495.146428	7.259405
6.001200	482.848157	7.264410
6.224177	496.251369	7.269414
6.451340	505.544808	7.274419
6.105351	501.838431	7.279424
6.127094	494.153789	7.284429
6.245191	515.104688	7.289434
6.299801	508.289208	7.294438
6.335507	514.501741	7.299443
6.229165	507.459309	7.304448
6.221460	508.385635	7.309453
6.153163	513.167652	7.314458
6.636744	519.207713	7.319462
6.231120	500.699709	7.324467
6.019240	488.816924	7.329472
6.383414	497.008502	7.334477
6.096301	490.452933	7.339482
6.117985	496.240885	7.344486
6.304967	511.923919	7.349491
6.229298	531.062455	7.354496
6.283751	517.472856	7.359501
6.680131	514.469462	7.364506
6.490980	498.103557	7.369510
5.942089	491.770213	7.374515
5.914583	489.237719	7.379520
6.424395	490.903793	7.384525
6.310620	497.355010	7.389530
6.153424	491.841993	7.394534
5.652126	497.525173	7.399539
6.070856	515.146617	7.404544
6.657743	519.210461	7.409549
6.742203	518.154618	7.414554
6.433500	499.059963	7.419558
6.214446	500.277725	7.424563
6.058370	492.113001	7.429568
6.299897	486.970063	7.434573
6.184415	490.272608	7.439578
6.443233	482.512883	7.444582
6.503061	486.910461	7.449587
6.049817	488.294487	7.454592
6.277337	490.353992	7.459597
6.079118	479.760581	7.464602
6.201566	484.876693	7.469606
6.542412	484.757362	7.474611
6.273966	496.760935	7.479616
6.354077	486.042007	7.484621
6.324399	488.394802	7.489626
6.274971	487.212114	7.494630
6.263708	496.715626	7.499635
6.091109	488.091326	7.504640
6.531260	488.235378	7.509645
5.878195	493.795354	7.514650
6.346281	490.489370	7.519654
6.258656	488.229241	7.524659
6.185488	504.534872	7.529664
5.998155	482.226830	7.534669
5.922774	495.192767	7.539674
6.018251	492.738903	7.544678
6.076926	508.443137	7.549683
6.231920	522.881082	7.554688
6.299251	515.592800	7.559693
6.232947	527.869818	7.564698
6.344554	518.502503	7.569702
6.713461	516.656070	7.574707
6.092444	495.963078	7.579712
6.200357	489.005512	7.584717
5.872739	504.627369	7.589722
6.350174	511.691621	7.594726
6.380143	516.718843	7.599731
6.181474	514.136888	7.604736
6.613251	495.740109	7.609741
6.122471	498.550121	7.614746
6.117203	497.694880	7.619750
5.981810	495.475002	7.624755
6.233853	509.133582	7.629760
6.329543	523.882135	7.634765
6.271143	524.184246	7.639770
6.288438	518.459868	7.644774
6.370038	490.826124	7.649779
6.155828	494.265150	7.654784
6.461381	492.492034	7.659789
6.109097	482.389449	7.664794
6.016019	482.019119	7.669798
6.165696	501.963703	7.674803
6.248670	509.530195	7.679808
6.771768	507.956820	7.684813
6.244341	504.152861	7.689818
6.396308	497.365101	7.694822
6.111579	497.714282	7.699827
6.256547	485.598497	7.704832
6.237246	487.205009	7.709837
6.048302	496.018374	7.714842
5.982564	491.823996	7.719846
6.366347	506.631671	7.724851
6.224789	503.555378	7.729856
6.242835	498.604162	7.734861
6.083721	501.734066	7.739866
6.282876	516.179604	7.744870
6.573224	516.093875	7.749875
6.378441	498.700789	7.754880
6.069124	502.208216	7.759885
6.189837	486.691665	7.764890
6.069262	488.467930	7.769894
6.081471	495.229224	7.774899
6.142460	512.527190	7.779904
6.390929	506.745474	7.784909
6.049895	528.990984	7.789914
6.005352	515.626802	7.794918
6.355126	511.539759	7.799923
6.131227	520.097767	7.804928
6.230979	516.584003	7.809933
6.060259	533.474745	7.814938
5.764432	524.508221	7.819942
6.280309	524.951024	7.824947
6.064850	531.556687	7.829952
6.508155	536.162414	7.834957
6.197447	527.117842	7.839962
6.441453	524.591874	7.844966
6.281566	533.355077	7.849971
6.024023	527.883098	7.854976
6.307789	521.199039	7.859981
6.076246	530.505157	7.864986
6.075035	524.460829	7.869990
5.913996	523.177995	7.874995
6.141870	532.347715	7.880000
6.310203	517.653764	7.885005
6.275060	524.462261	7.890010
6.448038	527.265390	7.895014
6.385581	530.528202	7.900019
6.216542	527.026889	7.905024
6.421194	526.771029	7.910029
6.256514	525.268395	7.915034
6.522967	526.335485	7.920038
6.312491	527.620103	7.925043
6.298338	531.625028	7.930048
6.397398	529.795661	7.935053
6.452944	524.748856	7.940058
6.657507	529.089872	7.945062
6.521622	523.471212	7.950067
6.010407	517.092070	7.955072
6.038626	513.617850	7.960077
5.933953	514.245187	7.965082
6.307647	522.669615	7.970086
6.473325	524.743587	7.975091
6.000463	525.897336	7.980096
6.278307	516.077631	7.985101
6.224432	538.839925	7.990106
6.788910	525.235687	7.995110
6.351961	513.720185	8.000115
6.040750	509.783325	8.005133
6.203506	487.348351	8.010150
5.923803	508.512330	8.015168
6.035980	518.848310	8.020186
6.261266	531.669255	8.025203
6.346939	536.393590	8.030221
6.423448	527.350153	8.035238
6.319771	543.396313	8.040256
6.560944	531.510457	8.045274
6.585183	524.109399	8.050291
6.161981	518.590891	8.055309
6.267245	499.352478	8.060326
6.214469	507.566919	8.065344
6.607670	507.534354	8.070362
6.313205	491.626922	8.075379
5.943572	504.747792	8.080397
6.281694	503.938853	8.085414
6.355012	529.924968	8.090432
6.389855	528.388737	8.095450
6.501488	527.153831	8.100467
6.339658	524.514594	8.105485
6.392031	506.588793	8.110502
6.282510	509.874501	8.115520
6.223238	516.170119	8.120538
6.385654	521.902729	8.125555
6.411153	530.074429	8.130573
6.641489	525.708403	8.135590
6.509637	515.153741	8.140608
6.110938	498.254767	8.145626
6.244067	502.273157	8.150643
6.196636	522.093809	8.155661
6.296317	510.362034	8.160678
6.357045	535.081982	8.165696
6.480230	529.693311	8.170714
6.688339	537.709961	8.175731
6.361339	551.710072	8.180749
6.448874	531.045689	8.185766
6.551219	544.201369	8.190784
6.504478	527.378722	8.195802
6.671913	522.645802	8.200819
6.240556	518.358030	8.205837
6.411754	514.917055	8.210854
6.270115	534.446657	8.215872
6.440479	524.004318	8.220890
6.705010	529.808721	8.225907
6.343708	528.715933	8.230925
6.493065	518.953021	8.235942
6.331423	526.834940	8.240960
6.469673	524.366641	8.245978
6.524280	520.537727	8.250995
6.679281	532.101341	8.256013
6.607891	513.213203	8.261030
6.444743	528.779311	8.266048
6.474222	529.014293	8.271066
6.512474	524.218879	8.276083
6.291787	530.340723	8.281101
6.459801	534.583824	8.286118
6.691191	528.305099	8.291136
6.655795	524.805268	8.296154
7.091028	524.977724	8.301171
6.536384	520.592041	8.306189
6.222414	508.811818	8.311206
6.239918	518.289598	8.316224
6.433806	527.828769	8.321242
6.657446	534.561898	8.326259
6.344985	535.750951	8.331277
6.339939	541.254402	8.336294
6.259175	535.614351	8.341312
6.313094	540.773772	8.346330
6.347679	524.054202	8.351347
6.310884	536.024540	8.356365
6.172519	519.127198	8.361382
5.964383	538.334985	8.366400
6.578632	556.191870	8.371418
6.841032	554.099627	8.376435
6.608745	557.136788	8.381453
6.791966	569.488626	8.386470
6.750345	560.801241	8.391488
6.728040	558.125853	8.396506
7.016105	558.470042	8.401523
6.923444	568.312941	8.406541
6.579137	551.004112	8.411558
6.551060	541.818433	8.416576
6.415306	547.664783	8.421594
7.001524	547.603077	8.426611
6.717362	562.171794	8.431629
6.568382	549.279837	8.436646
6.563206	548.622884	8.441664
6.606685	546.080005	8.446682
6.873807	545.734776	8.451699
6.593351	555.324602	8.456717
6.915302	558.040787	8.461734
6.696927	559.388177	8.466752
6.809563	561.083151	8.471770
6.533915	553.852479	8.476787
6.492414	560.239451	8.481805
6.689144	563.566375	8.486822
6.782681	559.236231	8.491840
6.574576	561.232193	8.496858
6.897747	558.285679	8.501875
6.526216	560.294772	8.506893
6.581425	552.693049	8.511910
6.704277	561.477101	8.516928
6.706903	556.627339	8.521946
6.696529	556.535605	8.526963
6.769324	561.702247	8.531981
6.661335	551.860900	8.536998
6.992260	554.011438	8.542016
6.596980	554.497977	8.547034
6.953064	555.081567	8.552051
6.823477	567.156813	8.557069
6.872752	562.824831	8.562087
6.875532	558.059870	8.567104
6.841985	557.163066	8.572122
7.014513	569.189077	8.577139
6.903918	567.108973	8.582157
7.081855	554.730299	8.587175
6.924572	563.634253	8.592192
6.899380	572.644410	8.597210
7.176142	558.964804	8.602227
6.823294	562.225098	8.607245
6.928736	572.277636	8.612263
7.129866	561.945618	8.617280
6.754852	560.965998	8.622298
6.758250	562.258534	8.627315
6.769737	563.371421	8.632333
6.944240	555.875942	8.637351
6.980090	568.389115	8.642368
6.531665	567.393482	8.647386
7.122325	558.694900	8.652403
6.955607	554.243034	8.657421
6.891645	557.154266	8.662439
6.765573	558.501065	8.667456
6.676236	560.130124	8.672474
7.106248	555.180902	8.677491
6.817039	551.968927	8.682509
6.722448	552.022778	8.687527
6.909972	553.086498	8.692544
7.132717	545.604112	8.697562
7.072668	554.983040	8.702579
6.993465	560.963920	8.707597
6.776474	565.298797	8.712615
6.957449	554.989500	8.717632
6.822125	561.137498	8.722650
7.035292	556.086834	8.727667
6.924662	555.967385	8.732685
6.855071	555.329836	8.737703
7.050224	546.425215	8.742720
6.947203	573.237537	8.747738
7.229856	568.749291	8.752755
7.091707	571.230253	8.757773
6.670897	557.633451	8.762791
6.902389	565.821513	8.767808
6.909735	583.697834	8.772826
6.840030	583.233694	8.777843
7.157110	594.602492	8.782861
6.950086	599.409855	8.787879
7.006341	589.588085	8.792896
6.694681	596.236604	8.797914
7.348403	586.392269	8.802931
6.855888	589.899032	8.807949
6.945707	587.388440	8.812967
6.960245	588.330090	8.817984
6.812225	589.237984	8.823002
7.256035	581.183914	8.828019
7.140768	583.005020	8.833037
7.125966	588.986388	8.838055
7.139422	593.792247	8.843072
7.140335	588.994816	8.848090
7.335121	587.638802	8.853107
7.129186	600.013939	8.858125
6.988084	592.348101	8.863143
7.069008	588.058215	8.868160
7.004784	590.413796	8.873178
7.136981	593.938559	8.878195
7.190720	613.356856	8.883213
7.270772	622.149392	8.888231
7.665471	610.633699	8.893248
6.999868	606.223324	8.898266
6.738240	595.231970	8.903283
7.410229	619.055815	8.908301
7.376093	631.764331	8.913319
7.201616	615.863315	8.918336
7.279231	610.548965	8.923354
7.472957	616.838241	8.928371
7.126922	606.595631	8.933389
6.894418	607.735557	8.938407
7.187358	608.958205	8.943424
7.233013	623.142814	8.948442
7.591792	621.552452	8.953459
7.279017	622.260550	8.958477
7.066374	630.813228	8.963495
7.430169	622.895268	8.968512
7.355071	622.655107	8.973530
7.157526	636.938273	8.978547
7.263819	628.220601	8.983565
7.209030	632.809053	8.988583
7.467335	631.839019	8.993600
7.247964	626.428888	8.998618
7.302454	633.267065	9.003635
7.234409	615.665803	9.008653
7.456579	619.542958	9.013671
7.585290	600.697812	9.018688
7.408890	616.635715	9.023706
7.617778	609.170151	9.028723
7.432182	614.248729	9.033741
7.577379	613.016437	9.038759
7.499806	620.023058	9.043776
7.200722	619.693557	9.048794
7.295946	614.715209	9.053811
7.845515	626.323807	9.058829
7.162743	628.854826	9.063847
7.650038	612.128150	9.068864
7.391276	619.043181	9.073882
7.342470	625.689901	9.078899
7.199462	617.733377	9.083917
7.188711	622.662908	9.088935
7.747387	614.433765	9.093952
7.368823	636.631979	9.098970
7.604626	633.520887	9.103987
7.640813	620.413658	9.109005
7.544107	622.081435	9.114023
7.617971	619.271465	9.119040
7.443323	619.839731	9.124058
7.533147	615.097369	9.129075
7.673828	618.165114	9.134093
7.495325	607.092311	9.139111
7.732978	600.542789	9.144128
7.392607	603.013186	9.149146
7.600942	590.982935	9.154163
7.524279	585.168697	9.159181
7.597165	596.872678	9.164199
7.298499	587.326844	9.169216
7.643986	604.287728	9.174234
7.500733	620.858423	9.179251
7.497651	617.028785	9.184269
7.519282	633.922377	9.189287
7.384946	632.849249	9.194304
7.425771	627.654436	9.199322
7.447798	638.543188	9.204339
7.559247	631.867686	9.209357
7.385367	628.411874	9.214375
7.579760	621.931489	9.219392
7.643936	627.124277	9.224410
7.541281	625.092549	9.229427
7.628847	623.453125	9.234445
7.696619	624.153051	9.239463
7.495406	625.558721	9.244480
7.556342	618.815208	9.249498
7.302255	620.870834	9.254515
7.376247	620.409221	9.259533
7.383202	624.576127	9.264551
7.629360	620.078350	9.269568
7.521723	629.409489	9.274586
7.432206	650.380649	9.279603
8.034664	640.976068	9.284621
7.720675	656.871015	9.289639
8.058528	652.979515	9.294656
7.498716	646.247546	9.299674
7.297612	640.496363	9.304691
7.798628	652.882251	9.309709
7.862576	665.732332	9.314727
7.819103	658.579363	9.319744
7.710313	678.556195	9.324762
7.719301	672.331189	9.329779
7.958338	674.173662	9.334797
7.775892	661.446855	9.339815
7.769213	657.346493	9.344832
7.847554	663.328735	9.349850
7.764688	650.384042	9.354867
7.777771	664.336615	9.359885
7.566565	658.950315	9.364903
7.669763	659.689852	9.369920
7.965382	658.761575	9.374938
7.697199	651.661292	9.379955
7.894347	654.355705	9.384973
7.617103	663.525853	9.389991
8.021565	664.237943	9.395008
8.098054	658.721930	9.400026
8.051988	656.768035	9.405043
8.050626	664.953398	9.410061
7.606086	647.576492	9.415079
7.754912	651.653043	9.420096
7.857958	669.469366	9.425114
8.011484	662.928209	9.430131
7.632125	660.582526	9.435149
7.663601	662.242212	9.440167
7.786378	666.373358	9.445184
7.854697	659.568087	9.450202
7.751372	661.094567	9.455219
8.133153	658.982188	9.460237
7.725681	656.323001	9.465255
7.886064	671.176855	9.470272
7.901343	661.140887	9.475290
8.038450	665.809821	9.480307
8.099045	661.492079	9.485325
7.859518	662.781469	9.490343
7.890349	664.781849	9.495360
8.166768	661.477951	9.500378
7.824996	664.161641	9.505395
8.019410	658.603802	9.510413
7.629556	663.578577	9.515431
7.980072	656.074530	9.520448
7.866863	654.458048	9.525466
7.618286	664.374600	9.530483
8.055656	656.864269	9.535501
7.769006	667.888977	9.540519
8.015547	658.998925	9.545536
7.957938	665.633931	9.550554
8.070687	692.905594	9.555571
8.021167	690.463674	9.560589
8.081346	699.171070	9.565607
7.916011	694.527926	9.570624
8.084034	694.311059	9.575642
8.121063	690.734076	9.580659
8.318457	689.879105	9.585677
8.232828	689.383938	9.590695
8.056098	685.795834	9.595712
8.321608	687.260380	9.600730
7.899386	680.884427	9.605747
8.110836	669.856467	9.610765
7.941600	680.978886	9.615783
8.102560	687.647454	9.620800
8.202245	690.214699	9.625818
8.111795	697.978759	9.630835
8.188722	692.752077	9.635853
8.030919	699.901005	9.640871
8.075420	699.623561	9.645888
8.292175	704.714896	9.650906
7.835104	705.052132	9.655923
8.496574	689.832923	9.660941
8.142066	695.604082	9.665959
8.122770	701.084458	9.670976
8.498085	693.514791	9.675994
8.140490	691.883976	9.681011
8.594486	690.014338	9.686029
8.524384	699.686989	9.691047
8.420753	688.642987	9.696064
8.344958	686.915122	9.701082
8.007846	689.214257	9.706099
8.376474	682.557836	9.711117
8.420620	688.540326	9.716135
8.414182	692.338666	9.721152
8.328626	676.794379	9.726170
7.996922	670.580703	9.731187
8.231231	673.550422	9.736205
8.186869	692.216471	9.741223
7.989275	691.634610	9.746240
8.239957	679.649251	9.751258
8.209624	695.177735	9.756275
8.451211	694.747370	9.761293
8.774386	689.257891	9.766311
8.260656	708.691654	9.771328
8.416876	688.216462	9.776346
8.092872	701.486032	9.781363
8.380697	682.489514	9.786381
8.170928	701.942710	9.791399
8.300817	690.213974	9.796416
8.551664	686.560229	9.801434
8.278215	695.381998	9.806451
8.639740	697.899184	9.811469
8.634925	692.564576	9.816487
8.275308	696.539566	9.821504
8.608157	687.199390	9.826522
8.256492	708.050102	9.831539
8.292366	693.192887	9.836557
8.189625	694.150578	9.841575
8.119004	700.794047	9.846592
8.110825	691.973821	9.851610
8.304957	688.114821	9.856627
8.340194	696.152839	9.861645
8.550100	698.590080	9.866663
8.334407	695.233469	9.871680
8.198371	717.397329	9.876698
8.216926	727.190755	9.881715
8.456928	729.798488	9.886733
8.641485	725.825630	9.891751
8.459301	738.764370	9.896768
8.345339	734.155925	9.901786
8.227926	742.405381	9.906803
8.369787	732.561107	9.911821
8.725280	734.683894	9.916839
8.643725	734.689832	9.921856
8.608192	729.809026	9.926874
8.212318	730.869482	9.931891
8.511871	722.394080	9.936909
8.445742	729.859505	9.941927
8.391283	730.767692	9.946944
8.649316	732.438559	9.951962
8.475987	728.145974	9.956979
8.488906	735.990492	9.961997
8.402154	721.939101	9.967015
8.514494	748.241518	9.972032
8.680155	755.737340	9.977050
8.646784	768.239481	9.982067
8.818339	757.903362	9.987085
8.733322	760.614212	9.992103
8.411646	763.997228	9.997120
8.816408	758.854512	10.002138
8.788327	763.659416	10.007155
8.763520	762.551055	10.012173
8.821672	762.251968	10.017191
9.148819	768.227971	10.022208
9.119515	738.014740	10.027226
8.730294	729.948183	10.032243
8.777868	740.273339	10.037261
8.700868	730.517784	10.042279
8.657751	726.956104	10.047296
8.900390	726.839582	10.052314
8.898493	735.200137	10.057331
8.799304	735.861529	10.062349
8.866647	728.312330	10.067367
8.884442	716.689386	10.072384
8.764763	733.139103	10.077402
8.660547	727.432102	10.082419
8.768919	726.054733	10.087437
9.106715	720.345740	10.092455
8.818445	724.287199	10.097472
8.946000	731.034620	10.102490
8.685611	733.735378	10.107507
8.926158	736.470952	10.112525
8.817241	721.357963	10.117543
9.005728	726.688480	10.122560
8.935807	726.550002	10.127578
8.877308	730.084267	10.132595
8.842568	739.575246	10.137613
8.729126	735.449600	10.142631
8.310613	751.423815	10.147648
9.011465	743.286245	10.152666
8.998783	750.187830	10.157683
8.985689	759.938976	10.162701
9.040412	743.857457	10.167719
8.772194	731.720450	10.172736
9.137044	734.287772	10.177754
8.807142	746.956102	10.182771
9.078369	754.699883	10.187789
9.131459	737.595497	10.192807
8.428026	744.404967	10.197824
8.803089	748.979298	10.202842
8.781174	756.202137	10.207859
9.204810	760.286936	10.212877
9.126976	756.880959	10.217895
8.595637	772.797182	10.222912
8.910573	763.900589	10.227930
9.016294	766.539868	10.232947
8.796994	770.236518	10.237965
9.098799	762.800104	10.242983
8.744540	770.098438	10.248000
9.013358	765.917191	10.253018
8.558120	755.527203	10.258035
8.960996	761.823995	10.263053
9.354086	770.552683	10.268071
8.730524	777.764248	10.273088
9.212635	785.109283	10.278106
9.275610	803.248665	10.283123
9.309536	785.622288	10.288141
9.308799	772.835641	10.293159
9.011082	772.337043	10.298176
9.336234	773.389648	10.303194
9.260062	760.790840	10.308211
8.886538	763.585680	10.313229
9.076726	766.975135	10.318247
8.921264	773.753501	10.323264
9.219106	787.577843	10.328282
9.069429	800.528682	10.333299
9.327092	796.403788	10.338317
8.938351	798.733318	10.343335
8.997274	801.080881	10.348352
9.376862	789.264555	10.353370
9.310156	793.154360	10.358387
9.219876	800.342069	10.363405
9.343527	797.746438	10.368423
9.214595	814.230540	10.373440
9.603456	798.536287	10.378458
9.465295	806.753975	10.383475
9.419335	811.630636	10.388493
9.645755	798.902869	10.393511
8.944777	800.081847	10.398528
9.427006	791.992091	10.403546
9.350203	799.419853	10.408563
9.360942	808.660291	10.413581
9.444222	811.292264	10.418599
9.131353	804.825464	10.423616
9.417708	800.456795	10.428634
9.251459	800.373893	10.433651
9.272470	809.943678	10.438669
9.258170	799.271774	10.443687
8.993646	798.383998	10.448704
9.053064	801.251663	10.453722
9.160996	803.084622	10.458739
9.026389	801.468315	10.463757
9.365213	802.148058	10.468775
9.236534	797.587589	10.473792
9.280215	795.376466	10.478810
9.263875	798.920608	10.483827
9.315174	803.601402	10.488845
9.624108	815.879032	10.493863
9.587635	813.373726	10.498880
9.526939	814.515388	10.503898
9.416076	803.620209	10.508915
9.314755	806.240470	10.513933
9.616102	816.027272	10.518951
9.339876	823.014953	10.523968
9.572419	827.072698	10.528986
9.810060	827.221424	10.534003
9.688359	824.484181	10.539021
9.317755	803.464412	10.544039
9.337090	824.790786	10.549056
9.450809	825.800888	10.554074
9.769041	832.890990	10.559091
9.523899	830.605271	10.564109
9.666317	831.996980	10.569127
9.833509	826.049357	10.574144
9.630952	828.533623	10.579162
9.776234	814.461712	10.584179
9.503152	810.963503	10.589197
9.549758	824.980159	10.594215
9.608484	823.175628	10.599232
9.786583	827.719649	10.604250
9.814207	819.322394	10.609267
9.455373	821.153764	10.614285
9.761849	818.401364	10.619303
9.315947	827.555394	10.624320
9.553827	844.506379	10.629338
9.941893	824.296675	10.634355
9.874174	831.628282	10.639373
9.773082	826.271651	10.644391
9.735298	826.707386	10.649408
9.501716	830.110005	10.654426
9.682164	824.738241	10.659443
9.598547	820.239893	10.664461
9.907874	823.974865	10.669479
9.826615	821.307894	10.674496
9.583626	830.700393	10.679514
9.857021	825.625616	10.684531
9.737214	834.004431	10.689549
9.955937	831.031335	10.694567
9.722666	834.916202	10.699584
9.896927	832.243611	10.704602
10.044791	824.747877	10.709619
9.805007	839.771548	10.714637
9.911012	826.726118	10.719655
9.617445	828.519838	10.724672
9.668693	821.199985	10.729690
9.736569	816.974189	10.734707
9.705413	826.121480	10.739725
9.980232	825.564873	10.744743
9.933275	822.734387	10.749760
9.773404	824.430730	10.754778
9.578781	823.792969	10.759795
9.464970	835.801755	10.764813
9.962176	828.861470	10.769831
10.074823	839.126833	10.774848
9.901822	822.574685	10.779866
10.142096	825.409515	10.784883
10.018014	832.319016	10.789901
10.040827	831.210850	10.794919
9.611729	825.709738	10.799936
9.711665	828.852061	10.804954
9.882133	836.375961	10.809971
9.551171	841.428447	10.814989
9.833288	842.847063	10.820007
10.049249	858.045099	10.825024
9.990844	861.117254	10.830042
10.053160	846.881496	10.835059
9.876289	859.713868	10.840077
10.552366	859.564786	10.845095
10.193217	868.545673	10.850112
10.375421	858.605592	10.855130
10.381175	850.606158	10.860147
10.019955	844.289433	10.865165
10.138899	830.074937	10.870183
10.009653	833.365942	10.875200
10.103175	845.907402	10.880218
10.392684	832.311653	10.885235
10.044765	843.667324	10.890253
9.940147	834.435566	10.895271
10.305990	850.442048	10.900288
10.300821	866.302314	10.905306
10.225952	838.060942	10.910323
10.155789	836.380448	10.915341
9.927620	839.845451	10.920359
10.145365	859.968620	10.925376
10.078151	859.860692	10.930394
10.376302	857.645888	10.935411
10.102970	870.734522	10.940429
10.129449	873.291261	10.945447
10.317547	868.406422	10.950464
10.299457	861.570861	10.955482
10.510246	857.588516	10.960499
10.403325	865.195272	10.965517
10.331758	853.246795	10.970535
10.220987	853.336977	10.975552
10.190345	855.983158	10.980570
10.017922	860.804467	10.985587
9.889312	868.853414	10.990605
9.680057	866.228056	10.995623
9.919669	866.251380	11.000640
9.999241	861.469797	11.005658
10.271027	864.237430	11.010675
10.083061	875.444763	11.015693
10.361470	877.713849	11.020711
10.449775	890.215565	11.025728
10.221439	892.661490	11.030746
10.588855	890.391442	11.035763
10.564726	893.023860	11.040781
10.477395	894.470271	11.045799
10.645073	891.601252	11.050816
10.550361	891.833736	11.055834
10.665356	872.160350	11.060851
10.542322	863.811980	11.065869
10.421924	863.549876	11.070887
10.333748	856.742038	11.075904
10.366219	863.250549	11.080922
10.307887	868.755346	11.085939
10.347010	878.535530	11.090957
10.550794	878.492543	11.095975
10.776727	900.832440	11.100992
10.397414	892.367377	11.106010
10.757986	893.158373	11.111027
10.713763	898.263967	11.116045
10.415578	878.444717	11.121063
10.559285	876.295288	11.126080
10.477031	887.850551	11.131098
10.633462	887.083034	11.136115
10.734943	903.777341	11.141133
10.423456	893.622809	11.146151
10.861941	895.878238	11.151168
10.547425	901.120021	11.156186
10.779129	898.188067	11.161203
10.664660	898.477940	11.166221
10.651048	893.756719	11.171239
10.711258	892.883076	11.176256
10.503539	900.961449	11.181274
10.541722	888.962825	11.186291
10.818852	897.620803	11.191309
10.866350	897.890602	11.196327
10.707909	885.659164	11.201344
10.663681	894.268885	11.206362
10.450317	888.967197	11.211379
10.480957	896.661551	11.216397
10.496185	893.696683	11.221415
10.801943	890.447623	11.226432
10.339796	906.727878	11.231450
10.499046	893.743659	11.236467
10.388176	906.380647	11.241485
10.327699	902.420386	11.246503
10.707156	912.104199	11.251520
10.576051	925.202934	11.256538
10.207012	928.826647	11.261555
10.344332	936.989728	11.266573
10.262314	938.332921	11.271591
10.219204	923.316911	11.276608
10.129865	949.736845	11.281626
11.085441	945.676962	11.286643
11.249261	956.919413	11.291661
10.884894	954.414441	11.296679
11.221024	954.732787	11.301696
10.850748	956.413333	11.306714
10.782145	953.004508	11.311731
11.177152	955.658405	11.316749
10.950557	966.271795	11.321767
11.212609	955.500678	11.326784
10.982208	962.027184	11.331802
11.232492	960.824145	11.336819
10.911991	951.294190	11.341837
11.014412	946.858057	11.346855
11.021579	940.849350	11.351872
10.812360	935.307040	11.356890
11.027155	948.141186	11.361907
10.891470	949.426724	11.366925
10.880286	952.151288	11.371943
11.370113	965.617052	11.376960
11.084794	966.034947	11.381978
11.255880	953.871026	11.386995
11.235715	953.356667	11.392013
10.980183	953.777512	11.397031
11.589685	951.840026	11.402048
10.761425	948.785441	11.407066
11.066205	934.304352	11.412083
11.284872	947.948550	11.417101
10.782796	930.322213	11.422119
11.219556	940.596474	11.427136
11.318121	958.530289	11.432154
11.092422	952.846035	11.437171
11.286109	943.309644	11.442189
11.151683	953.811747	11.447207
11.232167	944.471591	11.452224
11.108216	938.465855	11.457242
11.354021	946.909979	11.462259
11.514395	955.744936	11.467277
11.070871	946.348287	11.472295
11.231353	936.582978	11.477312
11.043851	959.800004	11.482330
11.379268	945.625601	11.487347
11.372472	947.104173	11.492365
11.099613	955.342724	11.497383
11.301576	955.835579	11.502400
11.436153	954.170836	11.507418
11.506181	946.368569	11.512435
11.231232	945.060037	11.517453
11.274328	957.083926	11.522471
11.558860	952.623208	11.527488
11.341138	954.877263	11.532506
11.305848	960.432901	11.537523
11.495066	948.132153	11.542541
11.107272	957.918381	11.547559
11.220262	949.865353	11.552576
11.340444	963.018246	11.557594
11.487169	953.119002	11.562611
11.449377	958.969689	11.567629
11.534944	955.594432	11.572647
11.531573	956.970488	11.577664
11.158877	963.269960	11.582682
11.148351	955.462697	11.587699
11.342514	950.926574	11.592717
11.332436	951.022455	11.597735
11.459549	955.263673	11.602752
11.086543	955.674999	11.607770
11.229354	964.420752	11.612787
11.396082	958.543123	11.617805
11.276997	969.004125	11.622823
11.764759	978.289633	11.627840
11.209592	1000.417078	11.632858
11.484094	995.257726	11.637875
11.783070	981.308370	11.642893
11.589015	995.382369	11.647911
11.388092	1001.107694	11.652928
11.444292	1001.224310	11.657946
11.601612	997.523261	11.662963
11.675768	999.041798	11.667981
11.660928	999.676371	11.672999
11.839240	983.876196	11.678016
11.587748	992.796162	11.683034
10.997644	985.534195	11.688051
11.555387	984.144737	11.693069
11.467334	991.769201	11.698087
11.337855	996.682848	11.703104
11.583429	991.809925	11.708122
11.692852	996.470938	11.713139
11.696107	1000.840493	11.718157
11.694936	1009.371915	11.723175
11.981086	1012.632495	11.728192
11.963901	1018.409339	11.733210
11.863268	1007.270435	11.738227
11.885098	995.573397	11.743245
11.456121	989.881587	11.748263
11.890557	999.228864	11.753280
12.296038	1007.949342	11.758298
11.759989	994.432013	11.763315
12.179602	977.289819	11.768333
11.628964	984.606142	11.773351
11.606640	988.634504	11.778368
11.717290	981.267364	11.783386
11.958913	1000.498630	11.788403
12.368673	999.238530	11.793421
11.892738	997.306818	11.798439
12.014879	986.197246	11.803456
11.741625	986.450182	11.808474
11.743731	998.280516	11.813491
11.910623	986.752198	11.818509
11.745684	995.805870	11.823527
12.125188	1008.920082	11.828544
12.210009	1021.297894	11.833562
12.460690	1007.733994	11.838579
11.839423	996.190860	11.843597
11.606791	987.343296	11.848615
11.947970	991.457234	11.853632
12.342041	1003.479449	11.858650
12.044966	1012.170384	11.863667
11.708089	1001.386812	11.868685
11.928224	1015.350066	11.873703
12.031420	1011.964601	11.878720
12.138869	1015.168112	11.883738
11.917633	1024.017163	11.888755
12.189461	1023.230175	11.893773
11.733674	1024.147820	11.898791
11.896809	1026.256676	11.903808
11.883012	1022.132987	11.908826
12.057972	1034.297914	11.913843
12.663428	1013.067945	11.918861
12.260188	1022.731393	11.923879
12.294423	1021.164904	11.928896
12.286079	1016.408332	11.933914
12.000014	1020.495048	11.938931
12.295092	1024.532376	11.943949
12.207020	1027.417666	11.948967
11.954123	1023.844628	11.953984
12.139379	1010.873332	11.959002
12.196933	1021.018021	11.964019
12.227215	1016.539665	11.969037
11.935539	1025.315331	11.974055
12.153350	1027.544068	11.979072
12.259711	1031.125261	11.984090
12.042330	1046.527947	11.989107
12.438442	1048.148772	11.994125
12.355507	1049.289206	11.999143
12.542038	1046.783519	12.004160
12.314991	1049.496930	12.009178
12.173285	1049.730489	12.014195
12.546452	1051.788305	12.019213
12.081164	1054.385009	12.024231
12.288322	1057.497654	12.029248
12.465163	1049.012239	12.034266
12.084996	1051.052246	12.039283
12.366037	1041.074656	12.044301
12.304983	1052.609415	12.049319
12.303679	1045.133404	12.054336
12.341350	1050.439064	12.059354
12.520609	1040.833354	12.064371
12.473135	1034.653944	12.069389
12.416989	1050.194727	12.074407
12.168610	1035.007052	12.079424
12.336816	1045.963062	12.084442
12.362659	1074.911406	12.089459
12.632666	1066.713688	12.094477
12.720589	1083.291354	12.099495
12.792157	1073.792383	12.104512
12.967546	1067.508425	12.109530
12.300480	1060.193206	12.114547
12.568627	1056.720442	12.119565
12.520073	1061.713439	12.124583
12.381604	1072.617211	12.129600
12.744691	1075.961532	12.134618
12.731061	1085.254186	12.139635
12.670176	1084.772139	12.144653
12.857189	1080.899851	12.149671
12.164459	1070.513763	12.154688
12.991629	1076.031232	12.159706
12.825987	1078.202497	12.164723
12.951968	1071.446857	12.169741
12.983067	1078.128985	12.174759
12.834659	1077.072912	12.179776
12.930516	1060.970389	12.184794
12.362824	1051.210792	12.189811
12.827429	1071.429740	12.194829
12.634451	1084.187906	12.199847
12.336327	1091.287970	12.204864
12.511158	1077.267129	12.209882
12.607286	1084.274484	12.214899
12.875998	1080.899638	12.219917
12.858194	1083.801275	12.224935
12.818444	1091.346164	12.229952
13.178213	1076.198281	12.234970
13.076966	1087.601936	12.239987
13.110981	1078.739973	12.245005
13.301047	1088.361903	12.250023
13.057398	1079.991228	12.255040
13.043766	1081.340452	12.260058
12.938287	1086.759136	12.265075
12.975521	1071.113267	12.270093
12.804795	1070.180943	12.275111
12.689172	1082.705099	12.280128
12.858777	1070.881238	12.285146
12.664087	1077.332807	12.290163
12.702064	1076.136108	12.295181
12.971939	1085.938124	12.300199
13.064265	1085.038497	12.305216
12.616941	1074.400861	12.310234
12.533378	1093.340170	12.315251
13.015709	1102.278477	12.320269
13.185035	1110.266112	12.325287
13.315846	1105.410150	12.330304
13.527876	1102.097414	12.335322
13.384416	1093.862710	12.340339
13.435673	1082.081032	12.345357
13.454626	1080.465102	12.350375
13.242773	1080.497886	12.355392
13.118059	1063.885440	12.360410
12.924184	1071.961811	12.365427
13.324522	1071.315173	12.370445
13.671310	1070.113892	12.375463
13.358644	1071.909319	12.380480
13.684791	1064.158748	12.385498
13.437975	1071.711275	12.390515
13.329566	1067.266255	12.395533
13.554637	1066.443496	12.400551
13.301833	1075.121639	12.405568
13.591041	1063.898589	12.410586
13.550242	1065.086973	12.415603
13.485730	1065.014910	12.420621
13.342135	1077.327380	12.425639
13.375199	1074.356380	12.430656
13.301949	1070.040370	12.435674
13.411478	1071.048228	12.440691
13.722614	1065.061866	12.445709
13.555926	1065.002161	12.450727
13.258471	1057.101143	12.455744
13.556538	1044.533353	12.460762
13.042283	1063.149374	12.465779
13.171086	1065.785480	12.470797
13.218487	1055.397152	12.475815
13.032903	1055.679098	12.480832
13.435061	1063.399135	12.485850
13.327943	1064.308367	12.490867
13.493206	1063.831462	12.495885
13.607167	1073.063857	12.500903
13.207711	1068.089466	12.505920
13.369759	1061.994890	12.510938
13.291662	1070.107827	12.515955
13.044344	1063.483750	12.520973
13.878880	1078.509124	12.525991
13.531898	1089.703625	12.531008
13.521369	1105.422329	12.536026
13.497423	1106.504404	12.541043
13.501904	1108.062022	12.546061
13.728228	1096.759394	12.551079
13.358929	1103.943065	12.556096
13.928590	1098.812843	12.561114
13.753431	1106.819024	12.566131
13.583010	1105.741591	12.571149
13.838041	1117.694957	12.576167
13.430740	1106.170311	12.581184
13.771366	1103.498818	12.586202
13.597037	1104.527607	12.591219
13.600265	1104.805907	12.596237
13.977977	1093.940986	12.601255
13.416757	1104.885710	12.606272
13.825186	1096.112038	12.611290
13.766253	1102.526422	12.616307
13.598553	1101.138942	12.621325
13.763420	1106.665886	12.626343
14.061203	1101.842166	12.631360
14.063761	1089.466459	12.636378
14.279679	1107.282644	12.641395
14.080580	1099.431285	12.646413
14.128945	1103.793021	12.651431
14.018232	1107.924394	12.656448
13.839964	1094.259480	12.661466
13.664586	1100.691728	12.666483
13.827057	1092.684378	12.671501
14.116439	1094.548597	12.676519
14.015638	1096.694585	12.681536
14.076041	1092.669819	12.686554
13.976509	1086.215964	12.691571
13.856301	1092.019505	12.696589
13.887565	1093.047383	12.701607
13.696814	1086.853840	12.706624
13.926553	1098.349436	12.711642
14.016946	1092.113957	12.716659
14.037413	1088.205026	12.721677
14.255298	1077.294100	12.726695
14.387594	1080.041621	12.731712
14.420553	1084.860157	12.736730
14.209784	1092.783843	12.741747
13.674867	1087.712952	12.746765
13.972375	1088.389794	12.751783
13.788393	1098.639793	12.756800
14.086281	1094.610027	12.761818
14.249326	1111.163501	12.766835
14.109469	1120.990146	12.771853
14.441660	1120.930072	12.776871
14.336717	1118.861458	12.781888
14.146726	1098.800456	12.786906
13.994241	1096.928451	12.791923
14.227622	1122.295507	12.796941
14.642179	1120.770473	12.801959
14.460944	1126.857100	12.806976
14.613624	1102.535984	12.811994
14.449389	1093.354665	12.817011
14.454554	1101.823093	12.822029
14.523888	1093.167851	12.827047
14.495712	1086.989561	12.832064
14.398006	1096.841700	12.837082
14.705526	1096.337152	12.842099
14.489128	1094.353877	12.847117
14.735968	1091.383958	12.852135
14.344845	1094.122522	12.857152
14.341650	1100.001202	12.862170
14.293162	1083.913652	12.867187
14.115229	1097.076364	12.872205
14.394167	1095.693804	12.877223
13.709302	1097.220084	12.882240
13.861150	1097.044363	12.887258
14.303675	1107.496496	12.892275
14.071969	1127.754221	12.897293
14.320312	1112.651483	12.902311
14.581889	1127.084492	12.907328
14.651305	1120.847154	12.912346
14.801601	1119.210105	12.917363
14.256198	1129.388178	12.922381
14.402351	1113.366842	12.927399
14.093906	1127.201243	12.932416
14.589638	1135.549848	12.937434
14.969398	1144.155381	12.942451
14.898365	1145.379274	12.947469
15.111766	1129.818980	12.952487
14.664715	1133.062976	12.957504
14.845303	1127.804353	12.962522
14.650205	1120.249127	12.967539
14.665281	1127.050442	12.972557
14.948268	1121.442865	12.977575
14.861033	1121.149985	12.982592
14.969445	1122.261952	12.987610
14.962443	1118.967694	12.992627
14.873393	1121.743535	12.997645
14.668709	1118.858658	13.002663
14.707275	1124.399002	13.007680
14.855202	1124.762231	13.012698
14.932705	1110.403758	13.017715
15.022122	1118.681332	13.022733
14.921892	1116.463536	13.027751
15.100700	1115.173690	13.032768
14.975214	1120.391197	13.037786
15.124232	1119.418430	13.042803
15.059048	1126.402470	13.047821
15.158708	1120.431352	13.052839
14.876568	1131.914727	13.057856
14.901444	1121.644430	13.062874
15.286533	1113.592603	13.067891
14.950939	1123.740331	13.072909
14.849470	1124.035932	13.077927
14.771892	1122.779794	13.082944
14.731617	1116.816254	13.087962
14.911397	1119.458116	13.092979
14.791776	1127.230756	13.097997
15.152415	1132.067388	13.103015
15.159566	1146.427517	13.108032
15.068463	1144.684317	13.113050
15.427864	1154.576882	13.118067
15.446454	1135.393232	13.123085
15.280567	1123.628708	13.128103
15.196678	1133.523265	13.133120
15.061888	1117.236392	13.138138
15.375362	1126.149280	13.143155
15.159128	1119.782600	13.148173
15.349514	1121.931054	13.153191
15.204734	1122.050180	13.158208
15.153341	1115.132326	13.163226
15.186807	1115.685507	13.168243
15.025757	1130.921120	13.173261
14.998094	1123.967063	13.178279
15.288857	1145.674650	13.183296
15.397394	1150.411436	13.188314
15.653754	1153.681299	13.193331
15.358738	1152.567768	13.198349
15.363798	1165.644598	13.203367
15.437449	1167.295696	13.208384
15.471901	1156.819493	13.213402
15.551702	1152.329371	13.218419
15.537720	1165.651831	13.223437
15.480182	1145.474800	13.228455
15.573932	1140.194899	13.233472
15.236528	1132.422079	13.238490
15.167940	1125.172862	13.243507
15.287842	1149.562217	13.248525
15.474509	1150.988763	13.253543
15.283110	1154.673119	13.258560
15.107292	1156.683503	13.263578
15.462916	1146.869673	13.268595
15.487324	1155.744140	13.273613
15.215577	1141.306957	13.278631
15.325039	1150.682838	13.283648
15.055815	1152.767309	13.288666
15.349060	1161.814840	13.293683
15.435399	1179.523802	13.298701
15.902513	1175.613075	13.303719
16.154620	1170.705163	13.308736
15.796930	1179.681954	13.313754
16.300801	1170.620658	13.318771
15.825694	1158.197867	13.323789
15.425453	1147.412854	13.328807
15.884074	1136.662466	13.333824
15.838225	1135.647502	13.338842
15.528260	1143.832845	13.343859
15.653366	1159.066072	13.348877
15.826395	1159.858946	13.353895
16.014096	1173.069355	13.358912
15.884942	1170.492805	13.363930
16.264217	1171.572217	13.368947
16.098598	1157.492030	13.373965
15.928295	1151.781227	13.378983
15.817081	1155.079358	13.384000
15.677737	1155.544777	13.389018
15.716848	1142.777416	13.394035
15.724660	1161.221270	13.399053
15.893653	1174.486733	13.404071
15.902449	1177.771728	13.409088
15.652002	1177.788256	13.414106
15.568000	1176.092494	13.419123
15.837746	1181.013444	13.424141
15.625301	1186.705510	13.429159
15.792703	1176.953076	13.434176
15.602913	1180.742274	13.439194
16.192320	1179.399135	13.444211
16.252540	1200.129106	13.449229
16.781689	1190.914235	13.454247
16.297407	1178.723223	13.459264
16.024430	1174.412831	13.464282
16.179296	1177.295989	13.469299
16.278386	1175.687276	13.474317
16.311300	1176.123639	13.479335
16.274403	1179.662211	13.484352
15.944825	1170.520569	13.489370
16.217536	1167.135006	13.494387
15.977500	1174.579392	13.499405
15.963892	1170.488305	13.504423
16.136174	1168.280578	13.509440
16.108350	1182.231229	13.514458
16.285677	1195.584689	13.519475
16.523294	1196.421607	13.524493
16.590473	1205.016831	13.529511
16.520749	1195.992444	13.534528
15.810845	1196.345687	13.539546
16.223419	1201.009610	13.544563
16.367269	1215.180309	13.549581
16.468707	1218.278179	13.554599
16.627545	1207.833346	13.559616
16.364546	1213.833928	13.564634
16.634819	1210.964429	13.569651
16.322512	1205.531169	13.574669
16.611803	1213.581305	13.579687
16.382607	1201.422913	13.584704
16.689307	1211.703104	13.589722
16.456100	1199.264119	13.594739
16.389056	1214.786400	13.599757
16.517822	1201.590456	13.604775
16.788751	1206.945209	13.609792
16.454697	1204.582013	13.614810
16.435233	1196.966037	13.619827
16.532568	1205.009313	13.624845
16.603968	1210.388576	13.629863
16.627625	1200.692553	13.634880
16.261588	1201.970516	13.639898
16.499696	1203.651912	13.644915
16.543677	1201.306155	13.649933
16.500009	1210.018701	13.654951
16.540059	1200.597684	13.659968
16.422289	1204.610778	13.664986
16.820552	1219.516487	13.670003
17.087512	1239.150694	13.675021
16.912477	1221.535518	13.680039
16.985682	1203.519946	13.685056
17.261108	1217.956459	13.690074
17.034514	1205.350457	13.695091
17.339756	1205.444617	13.700109
17.063188	1198.944589	13.705127
17.239447	1199.930997	13.710144
16.752274	1193.072132	13.715162
16.908802	1191.531866	13.720179
16.782259	1195.486377	13.725197
16.811550	1196.008366	13.730215
16.976247	1199.573463	13.735232
16.902162	1205.421188	13.740250
16.960985	1200.930582	13.745267
16.934687	1200.489659	13.750285
16.799982	1199.327982	13.755303
17.380253	1193.397670	13.760320
16.747217	1188.213255	13.765338
16.696849	1192.773194	13.770355
16.994801	1189.925696	13.775373
17.025397	1209.450128	13.780391
17.227455	1200.909290	13.785408
16.837172	1211.584341	13.790426
17.162365	1211.647257	13.795443
17.790716	1214.880263	13.800461
17.332138	1210.147647	13.805479
17.213272	1195.477896	13.810496
16.902938	1191.821607	13.815514
16.932377	1193.391248	13.820531
17.262778	1203.045759	13.825549
17.620703	1212.638847	13.830567
17.775806	1204.993428	13.835584
17.489142	1200.756934	13.840602
17.588723	1208.257401	13.845619
17.454861	1195.010389	13.850637
17.603860	1188.032620	13.855655
17.721377	1193.152523	13.860672
17.412843	1198.847088	13.865690
17.492973	1188.775261	13.870707
17.608397	1193.251512	13.875725
17.317565	1208.043757	13.880743
17.442048	1195.298262	13.885760
17.331778	1195.892519	13.890778
17.227147	1200.023304	13.895795
17.292894	1191.082620	13.900813
17.189761	1199.936069	13.905831
17.605435	1195.141649	13.910848
17.675776	1201.490427	13.915866
17.578949	1191.572231	13.920883
17.634733	1196.137264	13.925901
17.288504	1193.145862	13.930919
17.779223	1198.615842	13.935936
17.608355	1203.612171	13.940954
17.394066	1194.294793	13.945971
17.630730	1201.981825	13.950989
17.318134	1194.439878	13.956007
17.612629	1200.329826	13.961024
17.688407	1215.287248	13.966042
17.564851	1223.297952	13.971059
18.048108	1219.731739	13.976077
17.622183	1227.508203	13.981095
18.028332	1220.299567	13.986112
17.924048	1227.399939	13.991130
17.556681	1215.431077	13.996147
17.893732	1224.547772	14.001165
17.753419	1216.623656	14.006183
17.820291	1230.772056	14.011200
17.863380	1220.878547	14.016218
17.606363	1217.177029	14.021235
18.009804	1226.149506	14.026253
17.785456	1224.442684	14.031271
17.961441	1215.993534	14.036288
17.837953	1220.086109	14.041306
17.876930	1216.421491	14.046323
18.147623	1216.099574	14.051341
17.908647	1222.888198	14.056359
17.900560	1210.430306	14.061376
17.940591	1214.387606	14.066394
17.763623	1221.949921	14.071411
17.993103	1208.735753	14.076429
17.836255	1209.971864	14.081447
18.018194	1209.984055	14.086464
18.046517	1217.694698	14.091482
17.998324	1208.468153	14.096499
18.342529	1218.190855	14.101517
18.013993	1235.435253	14.106535
18.204054	1231.723030	14.111552
18.503790	1250.334072	14.116570
17.806834	1234.552316	14.121587
18.292286	1241.646171	14.126605
17.917126	1257.059002	14.131623
18.577175	1256.136402	14.136640
18.351784	1254.737579	14.141658
18.420506	1249.554086	14.146675
18.654448	1243.884501	14.151693
17.881596	1255.679932	14.156711
18.627104	1244.794081	14.161728
18.399620	1249.427394	14.166746
18.366265	1249.188590	14.171763
18.739175	1244.346309	14.176781
18.516731	1235.621112	14.181799
18.442250	1241.749190	14.186816
18.209365	1241.851384	14.191834
18.447584	1254.494346	14.196851
18.719559	1243.966038	14.201869
18.352710	1258.864384	14.206887
18.715260	1239.838102	14.211904
18.584902	1249.252690	14.216922
18.513433	1256.858012	14.221939
18.514548	1260.654456	14.226957
18.505456	1254.805573	14.231975
18.563388	1260.884222	14.236992
18.210644	1256.319901	14.242010
18.381296	1261.989035	14.247027
18.727415	1257.051192	14.252045
18.324915	1256.034340	14.257063
18.255688	1247.527088	14.262080
18.578906	1254.718615	14.267098
18.572951	1253.651978	14.272115
18.523980	1257.365767	14.277133
18.473201	1273.037168	14.282151
18.869953	1274.666179	14.287168
18.723546	1285.511186	14.292186
18.160108	1283.578938	14.297203
19.373205	1274.987893	14.302221
19.101868	1279.629447	14.307239
19.110337	1273.555443	14.312256
19.375566	1283.420943	14.317274
19.322258	1272.090785	14.322291
19.167895	1249.215840	14.327309
19.171556	1248.837868	14.332327
19.340394	1244.224951	14.337344
19.438915	1246.341957	14.342362
19.321833	1240.091499	14.347379
19.637207	1240.415645	14.352397
19.259471	1243.515551	14.357415
19.320933	1236.300294	14.362432
19.413457	1241.781181	14.367450
19.244751	1219.658933	14.372467
19.171275	1201.693582	14.377485
18.886466	1207.039203	14.382503
19.092899	1195.370160	14.387520
19.167078	1212.753267	14.392538
18.923635	1225.353378	14.397555
19.241097	1232.368706	14.402573
19.168340	1232.069495	14.407591
19.274055	1223.920493	14.412608
19.225259	1228.005057	14.417626
19.094871	1229.200976	14.422643
19.232147	1221.550229	14.427661
18.951678	1235.576925	14.432679
19.118787	1226.589749	14.437696
19.061407	1233.508975	14.442714
18.898994	1239.042617	14.447731
19.180857	1239.280385	14.452749
19.227912	1235.139891	14.457767
19.133231	1258.204450	14.462784
19.373394	1258.051136	14.467802
19.603906	1276.017446	14.472819
19.535939	1264.964676	14.477837
19.484651	1277.592122	14.482855
19.472457	1278.986395	14.487872
19.661148	1275.445426	14.492890
19.076270	1277.066600	14.497907
19.392687	1270.723433	14.502925
19.700346	1262.712077	14.507943
19.712438	1256.553438	14.512960
19.564835	1265.077118	14.517978
19.303605	1266.799903	14.522995
19.602002	1262.332870	14.528013
19.461155	1258.076395	14.533031
19.505958	1266.247658	14.538048
19.499221	1258.102263	14.543066
19.156251	1268.604599	14.548083
19.258228	1281.377168	14.553101
19.511525	1298.197187	14.558119
19.676635	1284.293496	14.563136
19.551206	1294.186361	14.568154
19.656688	1300.378016	14.573171
20.036169	1297.027332	14.578189
19.777748	1293.857840	14.583207
19.815612	1297.920622	14.588224
20.235390	1286.282190	14.593242
19.623277	1306.277666	14.598259
19.891464	1293.226494	14.603277
19.871188	1306.230279	14.608295
19.749583	1303.970523	14.613312
20.110032	1306.569572	14.618330
20.065164	1309.789065	14.623347
20.249024	1299.900388	14.628365
20.164733	1308.175081	14.633383
19.922643	1306.963631	14.638400
19.930178	1308.980541	14.643418
20.038155	1306.941863	14.648435
20.069179	1310.560764	14.653453
20.413357	1324.462863	14.658471
19.875539	1303.730043	14.663488
20.341998	1311.956829	14.668506
20.551077	1331.882569	14.673523
20.361227	1313.185835	14.678541
20.152088	1308.456646	14.683559
20.594967	1290.108464	14.688576
20.265390	1296.526715	14.693594
20.135992	1298.763665	14.698611
20.167510	1297.501883	14.703629
20.572380	1303.047300	14.708647
20.526213	1307.916181	14.713664
20.680227	1299.701095	14.718682
20.268510	1299.926530	14.723699
20.266669	1293.579852	14.728717
20.130126	1292.021088	14.733735
20.033346	1305.867908	14.738752
20.610809	1305.480926	14.743770
20.822757	1322.968735	14.748787
21.000760	1318.777449	14.753805
20.779141	1297.988448	14.758823
20.550421	1292.729111	14.763840
20.390934	1292.238355	14.768858
20.405751	1294.983679	14.773875
20.798492	1301.742343	14.778893
20.667924	1303.845254	14.783911
20.568734	1300.999397	14.788928
20.811795	1306.312143	14.793946
20.894896	1301.595481	14.798963
20.494240	1297.775968	14.803981
20.635657	1296.249014	14.808999
20.820315	1314.397528	14.814016
20.999083	1315.403604	14.819034
20.934533	1304.258522	14.824051
20.994889	1297.766348	14.829069
21.072268	1288.685515	14.834087
21.004121	1289.347016	14.839104
21.282826	1286.112186	14.844122
20.829081	1286.438253	14.849139
20.936898	1282.100921	14.854157
20.951415	1284.028695	14.859175
20.560703	1285.803780	14.864192
20.664482	1279.636673	14.869210
20.754951	1288.551276	14.874227
20.971209	1304.911546	14.879245
21.155826	1308.818406	14.884263
20.952978	1314.900216	14.889280
21.093014	1306.247539	14.894298
20.821570	1312.318049	14.899315
21.084297	1322.482960	14.904333
21.188499	1321.715000	14.909351
20.806819	1328.241466	14.914368
20.971503	1321.978462	14.919386
20.744640	1325.984225	14.924403
20.757573	1327.768389	14.929421
21.083868	1319.815529	14.934439
20.912680	1323.384200	14.939456
21.078977	1318.174915	14.944474
21.080990	1341.909350	14.949491
21.330813	1350.327839	14.954509
21.614434	1353.631621	14.959527
21.275027	1356.820281	14.964544
21.600076	1350.757899	14.969562
21.811867	1350.047344	14.974579
21.213406	1335.999944	14.979597
21.313058	1318.602416	14.984615
21.400392	1347.207891	14.989632
21.532872	1347.143425	14.994650
21.605224	1347.587643	14.999667
21.324621	1353.546313	15.004685
21.594286	1356.062551	15.009703
21.566933	1357.536097	15.014720
21.572553	1350.375284	15.019738
21.647179	1361.996697	15.024755
21.369546	1356.144915	15.029773
21.902826	1341.967565	15.034791
21.853264	1351.979604	15.039808
21.592822	1342.014540	15.044826
21.963275	1344.719605	15.049843
21.705564	1336.336941	15.054861
22.312951	1333.215479	15.059879
21.868686	1327.757531	15.064896
21.745632	1315.611228	15.069914
21.849687	1309.027194	15.074931
21.608801	1316.159629	15.079949
21.643139	1309.672142	15.084967
21.710546	1320.150982	15.089984
21.711333	1330.803217	15.095002
21.858067	1335.526465	15.100019
22.017484	1342.649643	15.105037
22.101718	1341.939108	15.110055
22.216536	1345.431981	15.115072
21.633287	1344.252105	15.120090
21.923728	1351.526839	15.125107
21.549450	1352.557785	15.130125
22.049901	1347.752064	15.135143
21.797952	1354.481087	15.140160
22.163287	1342.054675	15.145178
21.973365	1345.397541	15.150195
21.947323	1349.334893	15.155213
22.432601	1329.057094	15.160231
22.049126	1346.882071	15.165248
21.648934	1342.037614	15.170266
21.677090	1339.193931	15.175283
21.874629	1354.675188	15.180301
22.341730	1348.587758	15.185319
22.370518	1357.501572	15.190336
22.360935	1349.217642	15.195354
22.514012	1349.417254	15.200371
22.392117	1359.356420	15.205389
22.699527	1360.948834	15.210407
22.541210	1353.596441	15.215424
22.078904	1350.994019	15.220442
22.529091	1330.800352	15.225459
22.219691	1355.276723	15.230477
22.294148	1367.472300	15.235495
22.344595	1355.967476	15.240512
22.277939	1354.687864	15.245530
22.588640	1354.153653	15.250547
22.591265	1355.981840	15.255565
22.710485	1346.129796	15.260583
22.447047	1350.554740	15.265600
22.531262	1349.555469	15.270618
22.869555	1357.760552	15.275635
22.611187	1359.589749	15.280653
22.742795	1351.629878	15.285671
22.464274	1355.384576	15.290688
22.387072	1353.236947	15.295706
22.538573	1353.599788	15.300723
22.329853	1366.985307	15.305741
22.512663	1355.513131	15.310759
22.683397	1369.648038	15.315776
23.094609	1375.768338	15.320794
23.278020	1367.200178	15.325811
22.806043	1369.075894	15.330829
23.040996	1364.109347	15.335847
23.198362	1355.269356	15.340864
22.830848	1359.397963	15.345882
22.869507	1346.998762	15.350899
22.739533	1349.470427	15.355917
22.933283	1365.289873	15.360935
23.127167	1377.091364	15.365952
22.914690	1385.361695	15.370970
23.300162	1374.534660	15.375987
23.439032	1375.599886	15.381005
23.652160	1357.927888	15.386023
23.164314	1351.740229	15.391040
22.949364	1359.942657	15.396058
23.405590	1344.905915	15.401075
23.088801	1352.920079	15.406093
23.036274	1333.728646	15.411111
22.797468	1343.109841	15.416128
23.235823	1357.374700	15.421146
23.628416	1365.958753	15.426163
23.188802	1383.328153	15.431181
23.469934	1378.644874	15.436199
23.255597	1383.375254	15.441216
23.234313	1385.508338	15.446234
23.398307	1377.433865	15.451251
23.221013	1381.030916	15.456269
23.380482	1365.507835	15.461287
23.423678	1378.022716	15.466304
23.340155	1381.000025	15.471322
23.044363	1362.286491	15.476339
23.256858	1383.400347	15.481357
23.486013	1372.915243	15.486375
23.504206	1378.493292	15.491392
23.414672	1378.180514	15.496410
23.651171	1379.136706	15.501427
23.770178	1392.178170	15.506445
23.498955	1392.502025	15.511463
23.401755	1392.043093	15.516480
23.678238	1395.677939	15.521498
23.842344	1397.605216	15.526515
23.629384	1403.110071	15.531533
24.047428	1397.609192	15.536551
24.284889	1402.832555	15.541568
23.956797	1399.995377	15.546586
24.315684	1385.266767	15.551603
23.681877	1386.930482	15.556621
23.602163	1376.188979	15.561639
24.237532	1382.178748	15.566656
23.813196	1377.351260	15.571674
23.938478	1375.163277	15.576691
23.956974	1385.367213	15.581709
23.799103	1374.793527	15.586727
23.863910	1386.672254	15.591744
24.024772	1402.099196	15.596762
24.137621	1406.351359	15.601779
24.177998	1414.555121	15.606797
24.265058	1408.611364	15.611815
24.227989	1409.229550	15.616832
24.114160	1403.766963	15.621850
24.434047	1399.175292	15.626867
24.312010	1402.651618	15.631885
24.278704	1395.026022	15.636903
24.502799	1396.341106	15.641920
23.945040	1390.860558	15.646938
24.217668	1396.521550	15.651955
24.029206	1417.992815	15.656973
24.328600	1406.304708	15.661991
24.300863	1407.724786	15.667008
24.115836	1416.043936	15.672026
24.437592	1401.309638	15.677043
24.183758	1405.802096	15.682061
24.395408	1400.861039	15.687079
24.681902	1404.906185	15.692096
24.219225	1400.314128	15.697114
24.601147	1396.141478	15.702131
24.527439	1398.234022	15.707149
24.722966	1392.291635	15.712167
24.419110	1402.322308	15.717184
24.414968	1401.368732	15.722202
24.767388	1393.579605	15.727219
24.687152	1396.979543	15.732237
24.259245	1399.149907	15.737255
24.734316	1412.148489	15.742272
24.410250	1430.548311	15.747290
24.666355	1420.238619	15.752307
24.719452	1431.104493	15.757325
24.588357	1435.908128	15.762343
24.454484	1427.117995	15.767360
24.497145	1435.358196	15.772378
24.797572	1434.187775	15.777395
24.732497	1441.636246	15.782413
24.695045	1440.291572	15.787431
25.074982	1447.712368	15.792448
24.812810	1454.346483	15.797466
25.230626	1452.693140	15.802483
25.201523	1463.810778	15.807501
25.175623	1441.784871	15.812519
25.353468	1442.606882	15.817536
25.319212	1438.964351	15.822554
25.219954	1420.323569	15.827571
25.359278	1427.696530	15.832589
25.442836	1419.746336	15.837607
25.814478	1400.956116	15.842624
25.304601	1421.145841	15.847642
25.382496	1405.882820	15.852659
25.268555	1418.072371	15.857677
25.447518	1415.929244	15.862695
25.496936	1414.885725	15.867712
25.587072	1416.996662	15.872730
25.680764	1411.813121	15.877747
25.878276	1420.032055	15.882765
25.155389	1425.050789	15.887783
25.558168	1415.666142	15.892800
25.503073	1427.702098	15.897818
25.623729	1419.491477	15.902835
25.265632	1420.469760	15.907853
25.696878	1418.179052	15.912871
25.655533	1414.466841	15.917888
25.827406	1412.259738	15.922906
25.557625	1411.665370	15.927923
25.381029	1420.878087	15.932941
25.511256	1417.874824	15.937959
25.386172	1412.297574	15.942976
25.170184	1417.618904	15.947994
24.937001	1417.203109	15.953011
25.402369	1427.423962	15.958029
25.318005	1444.071231	15.963047
25.712617	1440.384203	15.968064
25.399942	1454.555574	15.973082
25.778381	1443.268298	15.978099
25.945897	1449.887302	15.983117
25.770134	1452.750160	15.988135
25.935203	1437.963778	15.993152
26.047875	1447.574317	15.998170
26.028163	1434.926852	16.003187
25.722464	1442.023802	16.008205
25.911043	1442.159879	16.013223
25.944080	1447.499508	16.018240
25.665813	1451.497856	16.023258
26.053368	1455.007880	16.028275
26.032166	1472.592648	16.033293
26.487270	1479.931558	16.038311
26.515661	1465.289177	16.043328
26.605793	1466.453987	16.048346
26.356353	1451.250918	16.053363
26.245141	1429.104303	16.058381
26.178712	1437.014548	16.063399
26.477794	1438.521744	16.068416
26.542831	1437.336882	16.073434
26.383400	1436.752817	16.078451
26.371443	1434.289514	16.083469
26.274272	1444.591332	16.088487
26.317645	1435.223749	16.093504
26.391691	1460.125831	16.098522
26.546051	1468.877640	16.103539
26.633806	1470.464243	16.108557
26.607399	1466.690308	16.113575
26.798644	1466.921207	16.118592
26.563505	1455.162165	16.123610
26.547543	1455.270634	16.128627
26.633049	1462.490322	16.133645
26.478636	1460.660711	16.138663
26.824280	1461.872852	16.143680
26.629986	1470.877920	16.148698
26.874581	1473.244602	16.153715
26.986845	1472.664647	16.158733
26.655165	1463.493652	16.163751
26.703682	1458.730105	16.168768
26.613788	1473.265216	16.173786
26.750164	1460.310871	16.178803
26.666361	1458.624492	16.183821
26.583906	1465.067321	16.188839
26.729664	1465.236652	16.193856
26.945042	1472.452991	16.198874
26.759125	1472.263014	16.203891
26.967649	1469.837669	16.208909
26.666331	1474.108497	16.213927
27.053594	1485.376214	16.218944
26.954604	1496.844947	16.223962
27.265266	1493.523702	16.228979
27.491934	1501.438688	16.233997
27.256276	1508.901013	16.239015
27.211574	1494.380708	16.244032
27.021484	1492.247186	16.249050
27.237707	1489.919569	16.254067
26.962107	1489.237786	16.259085
26.841228	1493.181005	16.264103
27.186869	1484.545032	16.269120
27.223301	1489.190505	16.274138
27.326351	1484.771239	16.279155
27.370981	1485.897119	16.284173
27.560674	1500.242568	16.289191
27.528289	1484.544209	16.294208
27.329593	1491.316255	16.299226
27.297529	1490.390514	16.304243
27.516070	1492.498940	16.309261
27.227313	1499.353580	16.314279
27.558896	1495.804891	16.319296
27.531846	1512.078047	16.324314
27.586089	1511.354942	16.329331
27.582801	1510.379174	16.334349
27.640269	1518.439043	16.339367
27.896230	1513.441225	16.344384
27.905723	1518.531652	16.349402
28.007399	1522.551473	16.354419
28.532481	1514.152922	16.359437
28.008823	1504.348163	16.364455
28.194268	1484.441320	16.369472
27.753839	1486.815904	16.374490
28.015568	1487.065467	16.379507
28.106549	1479.633435	16.384525
28.103888	1483.112490	16.389543
27.982763	1474.395016	16.394560
28.146158	1474.547065	16.399578
28.191684	1472.090593	16.404595
28.181890	1468.257620	16.409613
28.300914	1479.052602	16.414631
28.047150	1469.125519	16.419648
28.119652	1480.154538	16.424666
27.898438	1480.672269	16.429683
28.237768	1484.461494	16.434701
27.971618	1489.168779	16.439719
28.362887	1481.973502	16.444736
27.865874	1489.654378	16.449754
27.828990	1510.971607	16.454771
28.318628	1516.220454	16.459789
28.258021	1515.944226	16.464807
28.457872	1512.993801	16.469824
28.449767	1516.774118	16.474842
28.465879	1519.148844	16.479859
28.610033	1513.803407	16.484877
28.482037	1509.137902	16.489895
28.290323	1511.687306	16.494912
28.340866	1511.166755	16.499930
28.504246	1508.479215	16.504947
28.874923	1511.505884	16.509965
28.608959	1516.564676	16.514983
28.781425	1511.873924	16.520000
28.849920	1516.259810	16.525018
28.514062	1517.864656	16.530035
28.924877	1503.945160	16.535053
28.495217	1517.018547	16.540071
28.667487	1509.129031	16.545088
28.613586	1512.997022	16.550106
28.795161	1532.968508	16.555123
28.880096	1546.459967	16.560141
28.809200	1543.335015	16.565159
29.206560	1527.868313	16.570176
29.310030	1529.807399	16.575194
29.232910	1535.159160	16.580211
29.184723	1517.017630	16.585229
28.737890	1507.791633	16.590247
29.132672	1513.078001	16.595264
29.650798	1518.403626	16.600282
29.269668	1516.120199	16.605299
29.402934	1496.437092	16.610317
29.182390	1504.838527	16.615335
29.014799	1491.817276	16.620352
29.403157	1503.023810	16.625370
28.719864	1499.209618	16.630387
29.565503	1497.538322	16.635405
29.371147	1525.705900	16.640423
29.568870	1527.571937	16.645440
29.784746	1525.457337	16.650458
29.485007	1523.512972	16.655475
29.698602	1507.369859	16.660493
29.357802	1496.114206	16.665511
29.266200	1496.069252	16.670528
29.425233	1510.461504	16.675546
29.336077	1518.789469	16.680563
29.519590	1524.064500	16.685581
29.458080	1536.282680	16.690599
29.360103	1529.047577	16.695616
29.428568	1524.260243	16.700634
29.516463	1530.406479	16.705651
29.595217	1517.024657	16.710669
29.327905	1532.389039	16.715687
29.368698	1539.010324	16.720704
29.643274	1549.999504	16.725722
29.247237	1559.493810	16.730739
29.685073	1554.227568	16.735757
29.756257	1558.672068	16.740775
29.541774	1554.392645	16.745792
29.407055	1551.328625	16.750810
29.844144	1578.030905	16.755827
30.272796	1573.648740	16.760845
30.198270	1590.645285	16.765863
30.709882	1576.917505	16.770880
30.474817	1568.851208	16.775898
29.843280	1561.000216	16.780915
30.105967	1553.128605	16.785933
30.661536	1561.489995	16.790951
30.341340	1556.525570	16.795968
30.361017	1547.140184	16.800986
30.324420	1557.849731	16.806003
30.471078	1544.898340	16.811021
30.342166	1547.022858	16.816039
30.400742	1544.502808	16.821056
30.546485	1549.151690	16.826074
30.395185	1546.413205	16.831091
30.598479	1540.794240	16.836109
30.421238	1545.888766	16.841127
30.223889	1550.296351	16.846144
30.380013	1547.798759	16.851162
30.680906	1569.779845	16.856179
30.724071	1566.768109	16.861197
30.772216	1579.101453	16.866215
30.886606	1560.681069	16.871232
31.138879	1557.464919	16.876250
30.869303	1558.453578	16.881267
30.922051	1537.426023	16.886285
30.801295	1536.410224	16.891303
30.668428	1544.845217	16.896320
31.070180	1544.346735	16.901338
30.834020	1542.072414	16.906355
30.866545	1537.063485	16.911373
30.556349	1539.834022	16.916391
30.597725	1553.202387	16.921408
30.700440	1568.684178	16.926426
30.936792	1572.106041	16.931443
30.981153	1568.554215	16.936461
30.875322	1587.524777	16.941479
30.655823	1575.264892	16.946496
30.834978	1568.708292	16.951514
30.786850	1582.900623	16.956531
31.083189	1584.127023	16.961549
31.053346	1601.450603	16.966567
31.225339	1600.341940	16.971584
31.624145	1596.045400	16.976602
31.382343	1615.986576	16.981619
31.394989	1607.082965	16.986637
31.932585	1601.993307	16.991655
31.714013	1587.690205	16.996672
31.616149	1577.103708	17.001690
31.458135	1568.960118	17.006707
31.672420	1568.624488	17.011725
31.534619	1560.372261	17.016743
31.222188	1567.481796	17.021760
31.525651	1575.398695	17.026778
31.639377	1588.821269	17.031795
31.692861	1583.846258	17.036813
31.657244	1600.700182	17.041831
31.569652	1589.489811	17.046848
31.945204	1593.407313	17.051866
31.883863	1607.274135	17.056883
32.046886	1599.729168	17.061901
31.744252	1607.570673	17.066919
31.589370	1603.582728	17.071936
32.102353	1593.186775	17.076954
31.968078	1591.355001	17.081971
31.922073	1598.835236	17.086989
32.312533	1604.006617	17.092007
31.673831	1603.820800	17.097024
31.761640	1591.660887	17.102042
31.824151	1600.029967	17.107059
32.284895	1601.073905	17.112077
32.378479	1604.959274	17.117095
31.706340	1599.486135	17.122112
32.001432	1593.383930	17.127130
31.915526	1605.369808	17.132147
32.481038	1607.577980	17.137165
32.251176	1618.646632	17.142183
32.183759	1628.685617	17.147200
32.489283	1622.038239	17.152218
32.695517	1621.503963	17.157235
32.656719	1625.058501	17.162253
32.634968	1616.451478	17.167271
32.405943	1615.126046	17.172288
32.530574	1603.443051	17.177306
32.598916	1612.195968	17.182323
32.399941	1626.058586	17.187341
32.293929	1617.008062	17.192359
32.348572	1622.355991	17.197376
32.568836	1613.915644	17.202394
32.614305	1635.072997	17.207411
32.615937	1619.648372	17.212429
32.997426	1621.885185	17.217447
32.529357	1630.831467	17.222464
33.107902	1619.017749	17.227482
33.047221	1627.116292	17.232499
32.703714	1629.169996	17.237517
33.002410	1627.782747	17.242535
32.632128	1620.813242	17.247552
32.757336	1626.376255	17.252570
32.877211	1627.623947	17.257587
32.726610	1638.763954	17.262605
33.195615	1645.415692	17.267623
33.021519	1651.782020	17.272640
33.404615	1649.676971	17.277658
33.532764	1666.362779	17.282675
33.210535	1656.839361	17.287693
33.258559	1652.189208	17.292711
33.012553	1650.840401	17.297728
33.442646	1647.466124	17.302746
33.321388	1655.474113	17.307763
33.163253	1642.743656	17.312781
33.474523	1643.287952	17.317799
33.302152	1649.582744	17.322816
33.301516	1648.722263	17.327834
33.014044	1652.342504	17.332851
33.122493	1648.648589	17.337869
33.319352	1655.326211	17.342887
33.194646	1674.280512	17.347904
33.398117	1683.022162	17.352922
33.527739	1679.674108	17.357939
33.849980	1678.537068	17.362957
33.903520	1678.246304	17.367975
33.623142	1676.838813	17.372992
33.678412	1670.747667	17.378010
33.752932	1672.366397	17.383027
33.492337	1669.278081	17.388045
33.743199	1666.297548	17.393063
33.859093	1674.213214	17.398080
33.884641	1675.642226	17.403098
33.965868	1689.987471	17.408115
34.289572	1700.306515	17.413133
34.266749	1693.642704	17.418151
34.278045	1688.372502	17.423168
34.370703	1667.596609	17.428186
34.042768	1660.040235	17.433203
34.315767	1662.622108	17.438221
34.300602	1651.667408	17.443239
33.825098	1656.613449	17.448256
34.625340	1676.398251	17.453274
34.675311	1680.560697	17.458291
34.595289	1678.542605	17.463309
35.021929	1667.373564	17.468327
34.509547	1662.386342	17.473344
34.326712	1655.286250	17.478362
34.499355	1654.152282	17.483379
34.351037	1647.843835	17.488397
34.453923	1645.903974	17.493415
34.391750	1657.216367	17.498432
34.779835	1678.076049	17.503450
34.750941	1681.564011	17.508467
34.439987	1683.564907	17.513485
35.011890	1682.461404	17.518503
35.122654	1693.699582	17.523520
34.935843	1689.762751	17.528538
34.802192	1680.623264	17.533555
34.779700	1683.311838	17.538573
34.784254	1681.900366	17.543591
34.666197	1676.155736	17.548608
34.750835	1674.841844	17.553626
34.918467	1680.665355	17.558643
34.816256	1689.695880	17.563661
35.198583	1687.173089	17.568679
34.820953	1688.148513	17.573696
34.906465	1682.650326	17.578714
34.907335	1682.687716	17.583731
35.086835	1690.556664	17.588749
35.229798	1678.123230	17.593767
34.996143	1691.117726	17.598784
35.352825	1691.846622	17.603802
35.379461	1706.570349	17.608819
35.711794	1706.043773	17.613837
35.864106	1693.752072	17.618855
35.758435	1693.082153	17.623872
35.825233	1678.427514	17.628890
35.917048	1669.419456	17.633907
35.401997	1682.777730	17.638925
35.493412	1670.562245	17.643943
35.563663	1667.523182	17.648960
35.629429	1677.320138	17.653978
35.740634	1676.763773	17.658995
35.483362	1678.174174	17.664013
35.721193	1674.914330	17.669031
35.864944	1684.812957	17.674048
35.826304	1686.536401	17.679066
35.884669	1685.293378	17.684083
35.865219	1700.222919	17.689101
35.930170	1699.809811	17.694119
35.590417	1710.155240	17.699136
35.969352	1707.369257	17.704154
35.851284	1704.501447	17.709171
35.814669	1702.521253	17.714189
35.939563	1699.982149	17.719207
35.722790	1711.874592	17.724224
35.808759	1707.274248	17.729242
35.810650	1707.034927	17.734259
35.984103	1723.114758	17.739277
36.504514	1734.547839	17.744295
36.635827	1727.371001	17.749312
36.996557	1735.005716	17.754330
36.851266	1713.617385	17.759347
36.517924	1700.892017	17.764365
36.703255	1694.843338	17.769383
36.726952	1692.084175	17.774400
36.809763	1691.633080	17.779418
36.746355	1683.515720	17.784435
36.456727	1687.214466	17.789453
36.375266	1681.016596	17.794471
36.345015	1679.567180	17.799488
36.351818	1679.515805	17.804506
36.594993	1709.170876	17.809523
36.488823	1715.933243	17.814541
36.973121	1711.509958	17.819559
36.615007	1717.244005	17.824576
36.774246	1717.347733	17.829594
36.998448	1728.382960	17.834611
36.816245	1733.991892	17.839629
36.890782	1724.460340	17.844647
37.195697	1723.517476	17.849664
37.070806	1728.124924	17.854682
37.053059	1724.260528	17.859699
36.686273	1727.556531	17.864717
36.854406	1725.628119	17.869735
36.797381	1745.034065	17.874752
37.048060	1752.831250	17.879770
37.251583	1759.275363	17.884787
37.374957	1755.861207	17.889805
36.908607	1754.870419	17.894823
36.835658	1754.215364	17.899840
36.882434	1752.412110	17.904858
37.496123	1765.260345	17.909875
37.446376	1776.501095	17.914893
37.897287	1780.069419	17.919911
37.949259	1773.889811	17.924928
37.625130	1761.826968	17.929946
37.967932	1735.272898	17.934963
37.753384	1748.559919	17.939981
37.899121	1731.927055	17.944999
38.110287	1734.740196	17.950016
37.766189	1749.117007	17.955034
38.027354	1734.670326	17.960051
37.515812	1746.516438	17.965069
37.397108	1745.881738	17.970087
38.012325	1751.967888	17.975104
37.981862	1762.918465	17.980122
38.253208	1765.154803	17.985139
38.347044	1774.705871	17.990157
38.157412	1759.458956	17.995175
38.142134	1744.541668	18.000192
37.764876	1734.134484	18.005210
38.377649	1751.556348	18.010227
38.122419	1757.176175	18.015245
38.341825	1762.447522	18.020263
38.285430	1770.406471	18.025280
37.973196	1757.169161	18.030298
38.186565	1763.639401	18.035315
38.353609	1762.409905	18.040333
38.108842	1763.940084	18.045351
38.291649	1761.718528	18.050368
38.371473	1765.793789	18.055386
38.606438	1757.981965	18.060403
38.593507	1763.350951	18.065421
38.517831	1769.051335	18.070439
38.684964	1788.035297	18.075456
38.869901	1790.851602	18.080474
38.967207	1790.059171	18.085491
38.840584	1792.837798	18.090509
38.988118	1793.512295	18.095527
39.203929	1795.965271	18.100544
38.819805	1777.200480	18.105562
38.949215	1774.180948	18.110579
38.979336	1799.837998	18.115597
39.098768	1786.821817	18.120615
39.320944	1791.075113	18.125632
38.975814	1797.793351	18.130650
39.251224	1785.290508	18.135667
39.381063	1791.794641	18.140685
39.229296	1789.433903	18.145703
39.553647	1788.297490	18.150720
39.168907	1780.320177	18.155738
39.216534	1781.678038	18.160755
39.171666	1784.571092	18.165773
39.167594	1774.292742	18.170791
39.563165	1782.874964	18.175808
39.088910	1776.050113	18.180826
39.466589	1776.452549	18.185843
39.555883	1772.856641	18.190861
39.516225	1786.931632	18.195879
39.461618	1776.921247	18.200896
39.325179	1778.359323	18.205914
39.745989	1789.392809	18.210931
39.754496	1809.332434	18.215949
39.859891	1817.902200	18.220967
40.015084	1814.602642	18.225984
40.046585	1821.956607	18.231002
40.145452	1807.989973	18.236019
39.845638	1803.268922	18.241037
39.721582	1810.106324	18.246055
39.598418	1803.826920	18.251072
39.493196	1818.686901	18.256090
39.778577	1820.962064	18.261107
39.838217	1813.974569	18.266125
39.738220	1816.467533	18.271143
39.634454	1824.352654	18.276160
39.940096	1836.304123	18.281178
40.085427	1840.636463	18.286195
40.353660	1849.819623	18.291213
40.635441	1835.614493	18.296231
40.430748	1830.467720	18.301248
40.414451	1831.717658	18.306266
40.669104	1824.598927	18.311283
40.779718	1820.175952	18.316301
41.031411	1823.900816	18.321319
40.676202	1827.764746	18.326336
40.434052	1833.908366	18.331354
40.881568	1823.875599	18.336371
41.010353	1837.700188	18.341389
40.795110	1818.971408	18.346407
40.698361	1821.310899	18.351424
40.747432	1827.157994	18.356442
40.969486	1828.421688	18.361459
40.849065	1825.615458	18.366477
40.655273	1830.974596	18.371495
41.132180	1824.098438	18.376512
41.020154	1823.515775	18.381530
41.070921	1809.626962	18.386547
40.933379	1822.270683	18.391565
40.544794	1823.611862	18.396583
41.346271	1827.270281	18.401600
41.200974	1853.570515	18.406618
41.386092	1855.163312	18.411635
41.466374	1859.502273	18.416653
40.777877	1861.270140	18.421671
41.633148	1853.047922	18.426688
41.398509	1858.619112	18.431706
41.574997	1865.975907	18.436723
41.442061	1859.560315	18.441741
41.138855	1855.206501	18.446759
41.556530	1856.691584	18.451776
41.274208	1861.387679	18.456794
41.178333	1857.951469	18.461811
41.461253	1876.358396	18.466829
41.330504	1886.339321	18.471847
42.037082	1884.369151	18.476864
41.837061	1893.122879	18.481882
41.966597	1893.730875	18.486899
42.017617	1881.048129	18.491917
41.613904	1896.404510	18.496935
42.065898	1880.546775	18.501952
42.029606	1890.791396	18.506970
42.282965	1879.914391	18.511987
42.116211	1890.084123	18.517005
41.943188	1884.000701	18.522023
42.457110	1873.186144	18.527040
42.268533	1876.680657	18.532058
42.365055	1872.627280	18.537075
42.122118	1867.242353	18.542093
42.331298	1882.610814	18.547111
42.714317	1901.956641	18.552128
42.710529	1898.241847	18.557146
42.636955	1870.552736	18.562163
42.660337	1880.670572	18.567181
42.461994	1874.164218	18.572199
42.900822	1879.847330	18.577216
43.114686	1870.634163	18.582234
42.691068	1872.590912	18.587251
42.951498	1868.170723	18.592269
42.561943	1868.748368	18.597287
42.711435	1868.050448	18.602304
42.618976	1883.280192	18.607322
42.777081	1890.516626	18.612339
43.058543	1903.505696	18.617357
42.891371	1907.313181	18.622375
43.030284	1907.703115	18.627392
42.836093	1919.702998	18.632410
42.789535	1903.853813	18.637427
42.779211	1899.231926	18.642445
42.546917	1905.062167	18.647463
43.115413	1903.759825	18.652480
43.039187	1925.233325	18.657498
43.127925	1921.529218	18.662515
43.623347	1929.531693	18.667533
43.433022	1936.625156	18.672551
43.823558	1918.199455	18.677568
43.855612	1928.847921	18.682586
43.778976	1935.364386	18.687603
44.101764	1927.388963	18.692621
43.609499	1913.496692	18.697639
43.762392	1895.249448	18.702656
43.821979	1904.239781	18.707674
43.732854	1908.378035	18.712691
43.987061	1903.532924	18.717709
43.638188	1920.993630	18.722727
44.273140	1913.111299	18.727744
44.310426	1918.377563	18.732762
44.118952	1898.598803	18.737779
44.352804	1892.166872	18.742797
43.971330	1876.045142	18.747815
44.029110	1872.514254	18.752832
44.030866	1885.832178	18.757850
43.877096	1910.343350	18.762867
44.034974	1908.387480	18.767885
44.034921	1908.868087	18.772903
44.118333	1913.871241	18.777920
44.461511	1914.745083	18.782938
44.191027	1923.434102	18.787955
44.292777	1912.415216	18.792973
44.420760	1920.783690	18.797991
44.268139	1907.310249	18.803008
44.659667	1918.858458	18.808026
44.744727	1929.312161	18.813043
44.953219	1932.693439	18.818061
44.668101	1939.710648	18.823079
45.023415	1937.458002	18.828096
45.158221	1926.904264	18.833114
44.707099	1920.294204	18.838131
44.987336	1919.884880	18.843149
44.771346	1935.661807	18.848167
44.639768	1929.091449	18.853184
44.453666	1941.866114	18.858202
44.472180	1932.973548	18.863219
45.109553	1941.774339	18.868237
44.912730	1953.306227	18.873255
45.261966	1961.217140	18.878272
45.398310	1957.236680	18.883290
44.984537	1965.567944	18.888307
45.414595	1963.567877	18.893325
45.503035	1972.398772	18.898343
45.235824	1955.461503	18.903360
45.555794	1967.657139	18.908378
45.485918	1954.391615	18.913395
45.732356	1957.824890	18.918413
45.743620	1955.465726	18.923431
45.766536	1965.337066	18.928448
45.798480	1952.945573	18.933466
45.786456	1962.661875	18.938483
45.982872	1957.001774	18.943501
45.598644	1957.127602	18.948519
45.867884	1959.711329	18.953536
45.372035	1957.600318	18.958554
45.474579	1961.911616	18.963571
46.081733	1957.053043	18.968589
45.493700	1948.366791	18.973607
45.872064	1962.060297	18.978624
46.147699	1979.436568	18.983642
45.992781	1981.522139	18.988659
46.213752	1982.848421	18.993677
46.052079	1994.532980	18.998695
45.871394	1990.196279	19.003712
46.130151	1983.231900	19.008730
46.152675	1993.379279	19.013747
46.265185	1982.273535	19.018765
46.251967	1988.712423	19.023783
46.594019	2004.016533	19.028800
46.792792	2006.548335	19.033818
46.758610	2020.270700	19.038835
46.710584	2015.228672	19.043853
46.838891	2021.836294	19.048871
47.108425	2015.395463	19.053888
47.077358	2017.721571	19.058906
47.072907	2019.780315	19.063923
46.836960	1985.990667	19.068941
46.984475	1994.017404	19.073959
46.932427	1999.202010	19.078976
47.324335	1998.420132	19.083994
46.931259	2011.628230	19.089011
47.450095	2015.012174	19.094029
47.163153	2005.392362	19.099047
47.106975	2011.747423	19.104064
47.476837	2008.443253	19.109082
47.467229	2004.962049	19.114099
47.299809	1990.699130	19.119117
47.361054	2005.128475	19.124135
47.343398	2002.712475	19.129152
47.469337	2002.418795	19.134170
47.555663	2011.593533	19.139187
47.961114	2003.646730	19.144205
47.754344	2001.950299	19.149223
47.740576	2001.910785	19.154240
47.688301	2000.126429	19.159258
47.431626	2006.962017	19.164275
47.712617	2007.324538	19.169293
47.764029	2001.998983	19.174311
47.715422	1995.611323	19.179328
47.703764	2008.588492	19.184346
47.891508	2033.238681	19.189363
47.872809	2028.905907	19.194381
47.940948	2038.932010	19.199399
47.975848	2036.368357	19.204416
47.870465	2027.937900	19.209434
48.059571	2039.079337	19.214451
48.236586	2040.562479	19.219469
48.366143	2031.289140	19.224487
48.089449	2036.344165	19.229504
48.209394	2047.992856	19.234522
48.270497	2049.603411	19.239539
48.545286	2045.694727	19.244557
48.565249	2060.040993	19.249575
48.490063	2047.505922	19.254592
48.306901	2051.052134	19.259610
48.735542	2053.118047	19.264627
48.594709	2056.114994	19.269645
48.707460	2059.271002	19.274663
48.549804	2071.223827	19.279680
49.202575	2068.164599	19.284698
48.935087	2086.928849	19.289715
49.096539	2075.749601	19.294733
49.230053	2070.974378	19.299751
48.897584	2088.044605	19.304768
49.412773	2079.158258	19.309786
49.275750	2081.786307	19.314803
49.385895	2079.035425	19.319821
49.466837	2074.114966	19.324839
49.347797	2066.980719	19.329856
49.419342	2074.072896	19.334874
49.537213	2079.645947	19.339891
49.460352	2065.515421	19.344909
49.594618	2065.006014	19.349927
49.613909	2070.832731	19.354944
50.017550	2060.867293	19.359962
49.561223	2070.389785	19.364979
49.692303	2066.758362	19.369997
49.916180	2063.689898	19.375015
49.413741	2067.092239	19.380032
49.693218	2068.801736	19.385050
49.631502	2076.869784	19.390067
49.637809	2061.037683	19.395085
49.621714	2070.882863	19.400103
49.869992	2085.526629	19.405120
50.091551	2083.743662	19.410138
49.904488	2102.736154	19.415155
50.285372	2099.909233	19.420173
50.223369	2089.655008	19.425191
50.363726	2106.623305	19.430208
50.510883	2102.798684	19.435226
50.093976	2103.459982	19.440243
50.820641	2091.143127	19.445261
50.760131	2089.433736	19.450279
50.295441	2091.912606	19.455296
50.524618	2100.525848	19.460314
50.481980	2104.486409	19.465331
50.715655	2105.331906	19.470349
50.816088	2118.252263	19.475367
50.747403	2119.391403	19.480384
50.748742	2121.896998	19.485402
50.907795	2125.483518	19.490419
51.045549	2117.784024	19.495437
51.019470	2121.771575	19.500455
50.982966	2123.432516	19.505472
51.220937	2125.081956	19.510490
50.826786	2127.507052	19.515507
51.152436	2127.934435	19.520525
51.445679	2122.779683	19.525543
51.268116	2123.877963	19.530560
51.566809	2117.778303	19.535578
51.251135	2120.839584	19.540595
51.526979	2116.612429	19.545613
51.533761	2119.455086	19.550631
51.709002	2126.175262	19.555648
51.854024	2120.499581	19.560666
51.761574	2119.813287	19.565683
51.612126	2120.280008	19.570701
51.891467	2126.969598	19.575719
51.790917	2145.867145	19.580736
51.777232	2135.208878	19.585754
51.818975	2143.899373	19.590771
51.830352	2146.138966	19.595789
51.803420	2148.239628	19.600807
51.898838	2145.549824	19.605824
51.819134	2136.996571	19.610842
52.097194	2142.448891	19.615859
51.679029	2131.656302	19.620877
52.024789	2155.983555	19.625895
52.090880	2179.606338	19.630912
52.225607	2168.227914	19.635930
52.242171	2182.956910	19.640947
52.340306	2179.330709	19.645965
52.547674	2160.901723	19.650983
52.504056	2171.751428	19.656000
52.883870	2163.561557	19.661018
52.713554	2172.435130	19.666035
52.507060	2172.854001	19.671053
53.109754	2165.890575	19.676071
52.969418	2169.718491	19.681088
52.990430	2158.948577	19.686106
52.953262	2173.379777	19.691123
52.797971	2166.165064	19.696141
53.192946	2169.659464	19.701159
52.978669	2183.460155	19.706176
53.163466	2184.606621	19.711194
53.504732	2188.087855	19.716211
53.513684	2199.088918	19.721229
53.282220	2171.525939	19.726247
53.434394	2192.215480	19.731264
53.511102	2186.716601	19.736282
53.369354	2199.041667	19.741299
53.480774	2195.636082	19.746317
53.821877	2188.872749	19.751335
53.416541	2189.794321	19.756352
53.723905	2184.551593	19.761370
53.674602	2189.071693	19.766387
53.621977	2193.856298	19.771405
53.954233	2186.190175	19.776423
53.827463	2197.440416	19.781440
53.607060	2183.004593	19.786458
53.621084	2190.454134	19.791475
53.728365	2201.268885	19.796493
54.110835	2204.637614	19.801511
54.464291	2221.763524	19.806528
54.212121	2219.213226	19.811546
54.113914	2214.211706	19.816563
54.384271	2209.402214	19.821581
54.477862	2214.570306	19.826599
54.506030	2215.532439	19.831616
54.955620	2207.184767	19.836634
54.872217	2206.459182	19.841651
54.572166	2212.866041	19.846669
54.970611	2207.613569	19.851687
54.604870	2197.500401	19.856704
54.807241	2209.222398	19.861722
54.899990	2215.348028	19.866739
54.983846	2206.015213	19.871757
54.982126	2201.391814	19.876775
54.780527	2206.153603	19.881792
54.702402	2200.293526	19.886810
54.867908	2203.644963	19.891827
54.579171	2201.812854	19.896845
55.161992	2222.110039	19.901863
55.310079	2224.511486	19.906880
55.119764	2228.073879	19.911898
55.431550	2233.941884	19.916915
55.308846	2224.722515	19.921933
55.034541	2223.912539	19.926951
55.017779	2232.859779	19.931968
55.317160	2214.917452	19.936986
55.440669	2234.212297	19.942003
55.291510	2245.682200	19.947021
55.903603	2254.697569	19.952039
55.536222	2257.240299	19.957056
56.062847	2252.043002	19.962074
56.134053	2247.570517	19.967091
55.933131	2245.900452	19.972109
56.280447	2255.485320	19.977127
55.872151	2253.569033	19.982144
56.007312	2245.353215	19.987162
56.217869	2256.437529	19.992179
55.794726	2250.628345	19.997197
56.083507	2247.158797	20.002215
55.937126	2255.372020	20.007232
55.993776	2254.831736	20.012250
56.600288	2270.718147	20.017267
56.452818	2268.181245	20.022285
56.974937	2265.999800	20.027303
56.790229	2270.283068	20.032320
56.930202	2276.080276	20.037338
57.079515	2265.499897	20.042355
56.906073	2249.533342	20.047373
56.961231	2235.038944	20.052391
56.867589	2239.968124	20.057408
57.050995	2247.362343	20.062426
57.319587	2236.968357	20.067443
56.930513	2244.713846	20.072461
56.976537	2251.053495	20.077479
57.026256	2262.922401	20.082496
57.159568	2279.765095	20.087514
57.251725	2273.436927	20.092531
56.960344	2267.654384	20.097549
57.294085	2265.380652	20.102567
57.181293	2269.119009	20.107584
57.365715	2263.527702	20.112602
57.200192	2266.086876	20.117619
57.392423	2285.227330	20.122637
58.005206	2282.400636	20.127655
57.790288	2296.209210	20.132672
57.343861	2300.236349	20.137690
57.815126	2289.263999	20.142707
57.928149	2290.747702	20.147725
57.918622	2290.003015	20.152743
58.059162	2292.716326	20.157760
58.236632	2283.988220	20.162778
58.003293	2294.230633	20.167795
57.890188	2296.535697	20.172813
58.413931	2284.589006	20.177831
58.079534	2285.476027	20.182848
58.427042	2314.808554	20.187866
58.667056	2309.246034	20.192883
58.783727	2311.878259	20.197901
58.741944	2306.909113	20.202919
58.721484	2301.746697	20.207936
58.359085	2294.506704	20.212954
58.320062	2298.710005	20.217971
58.797991	2314.211049	20.222989
59.037412	2313.044544	20.228007
59.052985	2323.552513	20.233024
58.961432	2324.361615	20.238042
59.270756	2313.940967	20.243059
59.253289	2327.134309	20.248077
59.225471	2311.816803	20.253095
59.030546	2309.003309	20.258112
58.774364	2324.283573	20.263130
59.266224	2316.453031	20.268147
59.016444	2320.126838	20.273165
59.058848	2312.874664	20.278183
59.296379	2329.516346	20.283200
59.071476	2338.420489	20.288218
59.407351	2332.601587	20.293235
59.317633	2343.029929	20.298253
59.590529	2338.520546	20.303271
59.768404	2346.668621	20.308288
59.580197	2350.526932	20.313306
59.975225	2337.433055	20.318323
59.617488	2336.160715	20.323341
59.789318	2351.242532	20.328359
60.218545	2369.319399	20.333376
59.808396	2374.328087	20.338394
60.725004	2367.437690	20.343411
60.443133	2366.632302	20.348429
60.550713	2354.107919	20.353447
60.498544	2343.254111	20.358464
60.364599	2345.337249	20.363482
60.701803	2340.687130	20.368499
60.407969	2354.191892	20.373517
60.586161	2362.179108	20.378535
60.715138	2352.846622	20.383552
60.477519	2360.029386	20.388570
60.994358	2354.421893	20.393587
60.644798	2351.885106	20.398605
60.496748	2356.897521	20.403623
60.772025	2350.691806	20.408640
60.358889	2357.682132	20.413658
60.690198	2356.876593	20.418675
60.590435	2382.842670	20.423693
60.690586	2397.471647	20.428711
60.959408	2390.872128	20.433728
61.112401	2402.065265	20.438746
61.107817	2393.196526	20.443763
61.263569	2401.798450	20.448781
61.302642	2404.681882	20.453799
61.394562	2417.474772	20.458816
61.346267	2411.243374	20.463834
61.845224	2401.574740	20.468851
61.748067	2409.282504	20.473869
61.739313	2410.547186	20.478887
61.727647	2404.776830	20.483904
61.848800	2406.026933	20.488922
61.824717	2404.445140	20.493939
61.718918	2413.164302	20.498957
62.122338	2427.743981	20.503975
62.351338	2428.067077	20.508992
62.480690	2437.245982	20.514010
62.044189	2437.341475	20.519027
62.300553	2441.671975	20.524045
62.368100	2435.753094	20.529063
62.680390	2425.933611	20.534080
62.137978	2442.148038	20.539098
62.680639	2432.082229	20.544115
62.641359	2429.996287	20.549133
63.015497	2427.262739	20.554151
63.213503	2415.725853	20.559168
62.760318	2419.159496	20.564186
62.838243	2420.408674	20.569203
62.947213	2413.092307	20.574221
62.799324	2425.172522	20.579239
62.994956	2425.181273	20.584256
63.104170	2437.209762	20.589274
63.396447	2443.724333	20.594291
63.156556	2452.755025	20.599309
63.205516	2454.965816	20.604327
63.650755	2452.929522	20.609344
63.543434	2452.825354	20.614362
63.540538	2448.075509	20.619379
63.558089	2454.316016	20.624397
63.388490	2455.091765	20.629415
63.566043	2451.651181	20.634432
63.534351	2454.602415	20.639450
63.877841	2458.244357	20.644467
63.697948	2445.364479	20.649485
63.906608	2441.214673	20.654503
63.776500	2452.107014	20.659520
63.627962	2457.536640	20.664538
64.092825	2460.108597	20.669555
64.027079	2467.281316	20.674573
63.994764	2469.267760	20.679591
64.232445	2469.159925	20.684608
64.172694	2476.787531	20.689626
64.167232	2481.013287	20.694643
64.116135	2478.707849	20.699661
64.485142	2498.697448	20.704679
64.697181	2501.511768	20.709696
65.053861	2500.752617	20.714714
64.773658	2502.177903	20.719731
64.834654	2500.144864	20.724749
64.978619	2507.216219	20.729767
65.193161	2502.743398	20.734784
65.011862	2500.258108	20.739802
65.148703	2502.226052	20.744819
65.041902	2496.244232	20.749837
64.966278	2501.529550	20.754855
65.207435	2504.107184	20.759872
64.877012	2518.029131	20.764890
65.243627	2502.854511	20.769907
65.366326	2511.941849	20.774925
65.414539	2527.369441	20.779943
65.578567	2531.069597	20.784960
65.469274	2536.177037	20.789978
65.734562	2548.298515	20.794995
65.742589	2525.408814	20.800013
65.769690	2520.359324	20.805031
65.829108	2525.168427	20.810048
65.664455	2524.170050	20.815066
65.816933	2511.668040	20.820083
65.990933	2539.687824	20.825101
66.097749	2546.768091	20.830119
66.685598	2542.340455	20.835136
66.428033	2548.888847	20.840154
66.548981	2553.000039	20.845171
67.182395	2546.309894	20.850189
66.421761	2556.416399	20.855207
66.697933	2546.006782	20.860224
66.489118	2546.100279	20.865242
66.751900	2559.794128	20.870259
66.849801	2540.637354	20.875277
66.868087	2556.258491	20.880295
66.861003	2544.498918	20.885312
66.765512	2552.221636	20.890330
66.901853	2553.042300	20.895347
66.889843	2539.206903	20.900365
66.880407	2554.224390	20.905383
66.818858	2567.435654	20.910400
67.214036	2576.715784	20.915418
67.051369	2574.297477	20.920435
67.183774	2566.136665	20.925453
67.429417	2582.907588	20.930471
67.522727	2582.153177	20.935488
67.352272	2582.947773	20.940506
67.340718	2595.132356	20.945523
68.076746	2606.900124	20.950541
67.545858	2600.857838	20.955559
68.053025	2602.306557	20.960576
67.925757	2599.988689	20.965594
68.086797	2591.368435	20.970611
68.174711	2601.015871	20.975629
68.091651	2614.704716	20.980647
68.362876	2594.943283	20.985664
67.916701	2599.498181	20.990682
68.038073	2597.562824	20.995699
68.218905	2601.562564	21.000717
68.563522	2618.458108	21.005735
68.689607	2623.690058	21.010752
68.687871	2629.901344	21.015770
68.624421	2626.595818	21.020787
68.942105	2619.116525	21.025805
68.930515	2632.307778	21.030823
68.975769	2625.828958	21.035840
68.910733	2625.244797	21.040858
69.306655	2623.548697	21.045875
68.693299	2625.121560	21.050893
68.968766	2621.192346	21.055911
69.010376	2623.095142	21.060928
68.938465	2623.389232	21.065946
69.201081	2633.525506	21.070963
69.292182	2648.839052	21.075981
69.142472	2656.356226	21.080999
69.588761	2647.028999	21.086016
69.543413	2659.540852	21.091034
69.582118	2657.578993	21.096051
69.618686	2653.131011	21.101069
69.605270	2665.593107	21.106087
69.743409	2661.783421	21.111104
70.148023	2676.493643	21.116122
70.005411	2682.793975	21.121139
70.256534	2672.825791	21.126157
70.146841	2679.487984	21.131175
70.227236	2671.276265	21.136192
70.215230	2671.426606	21.141210
70.170582	2673.338151	21.146227
70.655986	2664.847317	21.151245
70.178589	2670.275457	21.156263
70.642336	2676.792894	21.161280
70.600671	2692.944913	21.166298
71.018644	2704.586583	21.171315
71.122990	2690.295233	21.176333
70.804881	2713.205589	21.181351
70.893892	2697.346376	21.186368
70.974147	2699.206183	21.191386
71.117663	2688.524313	21.196403
71.051963	2694.985947	21.201421
71.301518	2704.884675	21.206439
71.365695	2711.071717	21.211456
71.074634	2699.360528	21.216474
71.353461	2700.202928	21.221491
71.369429	2706.935702	21.226509
71.379336	2725.714529	21.231527
71.482387	2720.379997	21.236544
71.736705	2724.653045	21.241562
71.532030	2717.510010	21.246579
72.191698	2719.085501	21.251597
71.771183	2723.856656	21.256615
72.185624	2721.141791	21.261632
71.795905	2731.718978	21.266650
72.023058	2741.538759	21.271667
72.598486	2746.106371	21.276685
72.221221	2752.120719	21.281703
72.085400	2750.036907	21.286720
72.211564	2745.932738	21.291738
72.617253	2748.212373	21.296755
72.353974	2745.596895	21.301773
72.334962	2747.458546	21.306791
72.370599	2753.008227	21.311808
72.531024	2773.308226	21.316826
72.621369	2785.000946	21.321843
73.231136	2775.064373	21.326861
72.865081	2782.217770	21.331879
73.545334	2784.091822	21.336896
73.369107	2782.811101	21.341914
72.896457	2780.398711	21.346931
73.372706	2772.754174	21.351949
73.237583	2770.883619	21.356967
73.294563	2766.671984	21.361984
73.310487	2761.706936	21.367002
73.184375	2778.298569	21.372019
73.510395	2789.679920	21.377037
73.741820	2793.349319	21.382055
73.825412	2794.605071	21.387072
74.278073	2786.137692	21.392090
73.946855	2787.246644	21.397107
73.971817	2783.850887	21.402125
73.770613	2795.610295	21.407143
73.845374	2777.177885	21.412160
74.083123	2785.573963	21.417178
73.927383	2810.170150	21.422195
74.449102	2813.450261	21.427213
74.265985	2823.560713	21.432231
74.374692	2819.198790	21.437248
74.634759	2805.865416	21.442266
74.138306	2818.526740	21.447283
74.634426	2826.887233	21.452301
74.693776	2823.220049	21.457319
74.785701	2826.477880	21.462336
75.007496	2834.247123	21.467354
74.767652	2838.728626	21.472371
75.165000	2849.202605	21.477389
75.105582	2848.052571	21.482407
75.108740	2844.940706	21.487424
75.507500	2846.917972	21.492442
75.328261	2874.047167	21.497459
75.832576	2866.181420	21.502477
75.994518	2853.979920	21.507495
76.490523	2859.344909	21.512512
76.540667	2830.831107	21.517530
76.205212	2833.583998	21.522547
76.147811	2814.112799	21.527565
76.199206	2823.134547	21.532583
76.199583	2814.061999	21.537600
76.525343	2816.944196	21.542618
76.217219	2818.668992	21.547635
76.367563	2813.866745	21.552653
76.432527	2820.772173	21.557671
76.415216	2816.239351	21.562688
76.246274	2809.003758	21.567706
75.908645	2821.729388	21.572723
76.503123	2824.481753	21.577741
76.757859	2848.485392	21.582759
76.681578	2847.127524	21.587776
76.946733	2852.482235	21.592794
76.801945	2852.213199	21.597811
77.269538	2843.074059	21.602829
76.846655	2851.095895	21.607847
77.100024	2844.418428	21.612864
76.932007	2845.956302	21.617882
77.037500	2873.177810	21.622899
77.153141	2879.617035	21.627917
77.311481	2884.323293	21.632935
77.330646	2874.129934	21.637952
77.361938	2870.047708	21.642970
77.259399	2900.205487	21.647987
77.818330	2903.721585	21.653005
77.890019	2905.845814	21.658023
77.773128	2906.552444	21.663040
78.187693	2903.671392	21.668058
77.918479	2911.307251	21.673075
78.485920	2906.704153	21.678093
78.470108	2902.125391	21.683111
78.004066	2905.577404	21.688128
78.310741	2901.131960	21.693146
78.367920	2898.211544	21.698163
78.451058	2896.660406	21.703181
78.626945	2901.175194	21.708199
78.883980	2910.889756	21.713216
79.149243	2907.182620	21.718234
79.296145	2903.463943	21.723251
79.173498	2889.996895	21.728269
79.402331	2877.888649	21.733287
79.242867	2889.677844	21.738304
79.326792	2879.939903	21.743322
78.941290	2893.325049	21.748339
79.321921	2894.164418	21.753357
79.439648	2917.479810	21.758375
79.343064	2913.810813	21.763392
79.807394	2919.166098	21.768410
79.386556	2920.581589	21.773427
79.323971	2909.600566	21.778445
79.480690	2907.225882	21.783463
79.362422	2920.510990	21.788480
79.706974	2925.457740	21.793498
79.913190	2948.574311	21.798515
79.847201	2941.477937	21.803533
79.846241	2955.098401	21.808551
79.776341	2962.832054	21.813568
80.130430	2959.053538	21.818586
80.052604	2977.204671	21.823603
80.209890	2984.466557	21.828621
80.331534	2986.902217	21.833639
80.371430	2986.319599	21.838656
80.733513	2994.281088	21.843674
80.992784	3003.155209	21.848691
81.317878	2998.475205	21.853709
81.176784	2990.059375	21.858727
81.132419	3002.667403	21.863744
81.503311	3000.781313	21.868762
81.359671	2992.089139	21.873779
81.658669	2986.881973	21.878797
81.799468	2986.372443	21.883815
81.624174	2986.526148	21.888832
81.761635	2979.944544	21.893850
81.546477	2994.071287	21.898867
81.928157	2996.829715	21.903885
81.765663	2995.397106	21.908903
81.768931	2994.661885	21.913920
81.951497	2978.569609	21.918938
81.682774	2984.498002	21.923955
81.898601	2988.922361	21.928973
81.958209	2997.904667	21.933991
82.124116	3006.733983	21.939008
82.401233	3004.155538	21.944026
82.057376	3017.392575	21.949043
82.442471	3009.573621	21.954061
82.631808	3007.071489	21.959079
82.616911	3017.005456	21.964096
82.594456	3027.898916	21.969114
82.952497	3037.538208	21.974131
82.624901	3037.904082	21.979149
83.091641	3039.304016	21.984167
82.999340	3041.861649	21.989184
82.989398	3037.292506	21.994202
82.930062	3042.055647	21.999219
83.315640	3052.268726	22.004237
83.406622	3063.641877	22.009255
83.411829	3081.912085	22.014272
83.732392	3067.886619	22.019290
83.598216	3075.061280	22.024307
83.743600	3062.200954	22.029325
83.807685	3064.718970	22.034343
83.540778	3061.850107	22.039360
84.113268	3064.253799	22.044378
84.091585	3071.113816	22.049395
83.826252	3067.449440	22.054413
84.021406	3068.537571	22.059431
84.057139	3084.758704	22.064448
84.538139	3079.822999	22.069466
84.578819	3087.593558	22.074483
84.381687	3084.578913	22.079501
84.596916	3092.141896	22.084519
84.602011	3076.872917	22.089536
85.115003	3074.983415	22.094554
85.027178	3077.435987	22.099571
85.237522	3065.688120	22.104589
85.288376	3079.669019	22.109607
84.842744	3084.921584	22.114624
85.603486	3094.027845	22.119642
85.387123	3103.295572	22.124659
85.545424	3107.436959	22.129677
85.980616	3113.083734	22.134695
85.773992	3111.409200	22.139712
86.011368	3110.222701	22.144730
85.700653	3108.215377	22.149747
85.593804	3120.411002	22.154765
85.568217	3114.105490	22.159783
85.475982	3109.883774	22.164800
85.815271	3111.376427	22.169818
85.914314	3132.479934	22.174835
85.914807	3142.946858	22.179853
86.077831	3138.025491	22.184871
86.190924	3142.611748	22.189888
86.330232	3153.906509	22.194906
86.561312	3153.673781	22.199923
86.495784	3161.139493	22.204941
87.177696	3158.042569	22.209959
86.661040	3155.781480	22.214976
87.144661	3152.292924	22.219994
87.311679	3156.585637	22.225011
86.822905	3148.648815	22.230029
86.997446	3142.814934	22.235047
87.366391	3159.481466	22.240064
87.426427	3173.225504	22.245082
87.624240	3170.929028	22.250099
87.648225	3177.283918	22.255117
87.996804	3167.887883	22.260135
87.733986	3175.985402	22.265152
88.217632	3185.501278	22.270170
88.393005	3173.320535	22.275187
88.409670	3176.774338	22.280205
88.283710	3171.495209	22.285223
88.196402	3183.656553	22.290240
88.313856	3182.273334	22.295258
88.456481	3163.105644	22.300275
88.207400	3180.916425	22.305293
88.557742	3174.574753	22.310311
88.310288	3174.020714	22.315328
88.427073	3174.922595	22.320346
89.003806	3189.368258	22.325363
88.508036	3206.652915	22.330381
88.580191	3212.212081	22.335399
88.832183	3202.877653	22.340416
88.846959	3205.695961	22.345434
88.770237	3210.720683	22.350451
88.961965	3228.141361	22.355469
89.285523	3232.172011	22.360487
89.097362	3229.230264	22.365504
89.534642	3239.042017	22.370522
89.522068	3233.690195	22.375539
89.476151	3231.474141	22.380557
89.553759	3251.349878	22.385575
89.587545	3255.259129	22.390592
89.404207	3255.185822	22.395610
89.883448	3255.166019	22.400627
89.946431	3275.576479	22.405645
90.901535	3259.270037	22.410663
90.915485	3273.835152	22.415680
90.909924	3253.404456	22.420698
91.584174	3238.412534	22.425715
91.205829	3226.916543	22.430733
91.287224	3222.930273	22.435751
91.073543	3218.899064	22.440768
91.059257	3213.915241	22.445786
91.337314	3220.428162	22.450803
91.154026	3214.871095	22.455821
91.212660	3211.342911	22.460839
91.235952	3224.791105	22.465856
91.240353	3215.979856	22.470874
91.410039	3221.642985	22.475891
91.387923	3217.708860	22.480909
91.422603	3234.892116	22.485927
91.608529	3261.744331	22.490944
91.612612	3261.365650	22.495962
91.585275	3257.074115	22.500979
91.837117	3270.553085	22.505997
91.765035	3262.186331	22.511015
91.728692	3282.034482	22.516032
91.599366	3292.028478	22.521050
92.096863	3292.023768	22.526067
91.927026	3314.740435	22.531085
92.859552	3325.664881	22.536103
92.397706	3323.652581	22.541120
92.581974	3327.257459	22.546138
92.795705	3336.787715	22.551155
92.511483	3326.421360	22.556173
92.803684	3334.724096	22.561191
92.933287	3356.599227	22.566208
92.899914	3351.594498	22.571226
93.394967	3347.667401	22.576243
92.901637	3354.557053	22.581261
92.773377	3363.887147	22.586279
93.197481	3374.279111	22.591296
93.492936	3392.600149	22.596314
93.535368	3374.187331	22.601331
93.585557	3394.268174	22.606349
93.932589	3402.181575	22.611367
94.483174	3401.575184	22.616384
94.226690	3406.419833	22.621402
94.343445	3410.555175	22.626419
94.331524	3417.252315	22.631437
94.629803	3406.173909	22.636455
94.962021	3412.366940	22.641472
94.601827	3414.381897	22.646490
94.808343	3399.865926	22.651507
95.081006	3417.107302	22.656525
94.993768	3421.842100	22.661543
94.995684	3418.704735	22.666560
94.679658	3416.131322	22.671578
94.978148	3419.362626	22.676595
95.241245	3432.652083	22.681613
95.183568	3449.207140	22.686631
95.262039	3436.296144	22.691648
95.162874	3436.840814	22.696666
95.137656	3429.655196	22.701683
95.375358	3442.305948	22.706701
95.454328	3458.215604	22.711719
95.683470	3457.122172	22.716736
95.268960	3457.793753	22.721754
96.018202	3448.143943	22.726771
96.062294	3472.693986	22.731789
96.162506	3477.726171	22.736807
96.465671	3480.876402	22.741824
96.786687	3473.517410	22.746842
96.837179	3470.879487	22.751859
96.810141	3480.127176	22.756877
97.098195	3482.639748	22.761895
96.988498	3464.792904	22.766912
97.122965	3470.718243	22.771930
97.091617	3464.551336	22.776947
97.178237	3477.775899	22.781965
97.052336	3481.937577	22.786983
97.231432	3466.355605	22.792000
97.020797	3493.635165	22.797018
97.590995	3494.494820	22.802035
97.344456	3510.025640	22.807053
97.430014	3515.953566	22.812071
97.809512	3497.905771	22.817088
97.556143	3507.245206	22.822106
97.605003	3519.801635	22.827123
97.772846	3526.995890	22.832141
97.861463	3532.105599	22.837159
97.954441	3518.207098	22.842176
98.157828	3548.827397	22.847194
98.528361	3543.409407	22.852211
98.476078	3555.923917	22.857229
98.398010	3554.713132	22.862247
98.673380	3551.006144	22.867264
98.450774	3560.166905	22.872282
98.745591	3568.655950	22.877299
98.689681	3591.754196	22.882317
99.035692	3587.873321	22.887335
99.435995	3580.605116	22.892352
99.465009	3595.882613	22.897370
99.953601	3593.187632	22.902387
99.786672	3593.677756	22.907405
100.407177	3580.981800	22.912423
100.834392	3571.105992	22.917440
100.704277	3563.202604	22.922458
100.731010	3552.676052	22.927475
100.574386	3556.632590	22.932493
100.665198	3557.466739	22.937511
100.785234	3550.276748	22.942528
100.398282	3554.969772	22.947546
100.722030	3550.479592	22.952563
100.894710	3547.805323	22.957581
100.837479	3549.687952	22.962599
101.149277	3530.865083	22.967616
100.475315	3550.616968	22.972634
101.051251	3542.482749	22.977651
100.795184	3547.635640	22.982669
100.790615	3541.919396	22.987687
101.065136	3564.629537	22.992704
100.626639	3568.548403	22.997722
100.737933	3572.695321	23.002739
101.060995	3593.734486	23.007757
101.148256	3606.309837	23.012775
101.502348	3619.134810	23.017792
101.445015	3612.583552	23.022810
101.600894	3620.418808	23.027827
101.846686	3639.273150	23.032845
101.823472	3636.047374	23.037863
101.892891	3641.626043	23.042880
102.115218	3656.279527	23.047898
102.423204	3660.092390	23.052915
102.524137	3670.080470	23.057933
102.731389	3674.182819	23.062951
103.289576	3662.102613	23.067968
102.629513	3681.456300	23.072986
102.944554	3665.357565	23.078003
103.217610	3675.344767	23.083021
102.928215	3669.607823	23.088039
103.275878	3663.874670	23.093056
103.318029	3680.874113	23.098074
103.045451	3684.957719	23.103091
103.187536	3691.433464	23.108109
103.138602	3695.054916	23.113127
103.616265	3693.987727	23.118144
103.684753	3722.288507	23.123162
103.954223	3726.897918	23.128179
104.246533	3717.257305	23.133197
104.212478	3720.914888	23.138215
104.621924	3715.714427	23.143232
104.047029	3719.237753	23.148250
104.660664	3711.886597	23.153267
104.728225	3730.143329	23.158285
104.588172	3740.472066	23.163303
104.807644	3731.468686	23.168320
104.770372	3746.362004	23.173338
105.035393	3744.676001	23.178355
105.317368	3730.659465	23.183373
105.306903	3732.287535	23.188391
105.668936	3738.501756	23.193408
105.400122	3741.011110	23.198426
105.613758	3752.620408	23.203443
105.453603	3760.329213	23.208461
105.505007	3771.579106	23.213479
105.766145	3770.689425	23.218496
105.804437	3768.730644	23.223514
105.940180	3780.683154	23.228531
106.286690	3792.926837	23.233549
106.344467	3807.880100	23.238567
106.313167	3792.414064	23.243584
106.460529	3802.983939	23.248602
106.364282	3782.876986	23.253619
106.568308	3790.920911	23.258637
106.375548	3808.910115	23.263655
106.977827	3817.505975	23.268672
107.131224	3817.979396	23.273690
107.308155	3821.595840	23.278707
107.215917	3821.175973	23.283725
107.286355	3816.626784	23.288743
107.760970	3830.375343	23.293760
107.820013	3839.594454	23.298778
107.674299	3838.778297	23.303795
108.086556	3847.142182	23.308813
107.864023	3847.903711	23.313831
108.223836	3834.908494	23.318848
108.009875	3843.354198	23.323866
108.272800	3847.395817	23.328883
108.555443	3843.189123	23.333901
108.145744	3845.109162	23.338919
108.423498	3860.713543	23.343936
108.432495	3879.605731	23.348954
108.480330	3877.818985	23.353971
108.569376	3871.793837	23.358989
107.684032	3880.370973	23.364007
108.515849	3892.314853	23.369024
108.947509	3908.495046	23.374042
108.866056	3906.998958	23.379059
109.374090	3917.509314	23.384077
109.487853	3936.689385	23.389095
109.877834	3922.835938	23.394112
109.523619	3930.056013	23.399130
110.063446	3923.884309	23.404147
110.215529	3924.125661	23.409165
110.156746	3917.540655	23.414183
110.371523	3925.521849	23.419200
110.550667	3910.207148	23.424218
110.749638	3911.605349	23.429235
110.809630	3908.255921	23.434253
110.508068	3912.344375	23.439271
110.801026	3899.513305	23.444288
110.486063	3916.273188	23.449306
110.983411	3922.307640	23.454323
111.193934	3917.018326	23.459341
110.976668	3928.875735	23.464359
111.364374	3928.969095	23.469376
111.489409	3929.801940	23.474394
111.044749	3932.838425	23.479411
111.261491	3952.792073	23.484429
111.387397	3964.391223	23.489447
111.668651	3968.976318	23.494464
111.564425	3973.040448	23.499482
111.742395	3972.227887	23.504499
111.779516	3997.489380	23.509517
112.024370	3996.479540	23.514535
111.941044	3990.821027	23.519552
112.145042	4012.276509	23.524570
112.065206	4023.276608	23.529587
112.815835	4030.407477	23.534605
113.027051	4019.935561	23.539623
112.724101	4020.714323	23.544640
112.934136	4045.109106	23.549658
113.037147	4045.918037	23.554675
113.434310	4056.498778	23.559693
113.354158	4058.752984	23.564711
113.562682	4044.091982	23.569728
113.821084	4050.866385	23.574746
113.835751	4045.583800	23.579763
113.802517	4051.175249	23.584781
114.014568	4075.381550	23.589799
113.892706	4076.266224	23.594816
114.188936	4086.792401	23.599834
114.179882	4086.600523	23.604851
114.632165	4083.007490	23.609869
114.511322	4091.890321	23.614887
114.250165	4091.999164	23.619904
114.522252	4106.983446	23.624922
114.509661	4112.468352	23.629939
114.837758	4108.745828	23.634957
114.777670	4114.313782	23.639975
115.453393	4118.228600	23.644992
115.510857	4137.160731	23.650010
115.433119	4145.614406	23.655027
115.863486	4133.249434	23.660045
115.604094	4140.542524	23.665063
115.468362	4126.181646	23.670080
115.633938	4125.706571	23.675098
115.667081	4140.457129	23.680115
116.050186	4154.856162	23.685133
115.931934	4166.807630	23.690151
116.424732	4169.584922	23.695168
115.994063	4172.712058	23.700186
116.232795	4191.165071	23.705203
116.580214	4198.248466	23.710221
116.445660	4198.004879	23.715239
116.657277	4189.476176	23.720256
117.055002	4195.085446	23.725274
116.742492	4216.699394	23.730291
117.250220	4219.759280	23.735309
116.990315	4227.507240	23.740327
117.410130	4228.909925	23.745344
117.611464	4224.195281	23.750362
117.419013	4237.246121	23.755379
117.835834	4242.231357	23.760397
118.067188	4267.096609	23.765415
118.022205	4260.909197	23.770432
118.174036	4262.180567	23.775450
118.074330	4262.887960	23.780467
118.012342	4246.523352	23.785485
118.458192	4260.010104	23.790503
118.742693	4266.692095	23.795520
119.173493	4267.361438	23.800538
118.919817	4265.348471	23.805555
119.042093	4262.417831	23.810573
118.961906	4266.630040	23.815591
119.189095	4269.183116	23.820608
119.370273	4281.652152	23.825626
119.234908	4296.310617	23.830643
119.696834	4283.854088	23.835661
119.642110	4304.510556	23.840679
119.706561	4296.637246	23.845696
120.093370	4296.213804	23.850714
120.004730	4320.866255	23.855731
120.077247	4319.854555	23.860749
120.252389	4322.705231	23.865767
120.239759	4324.114023	23.870784
120.466593	4322.117719	23.875802
120.350904	4338.133672	23.880819
120.332232	4348.378185	23.885837
120.484360	4360.653254	23.890855
120.867285	4360.391879	23.895872
121.211491	4366.314795	23.900890
121.114432	4365.235043	23.905907
121.489991	4372.320168	23.910925
121.638541	4368.707570	23.915943
121.434162	4367.697917	23.920960
122.045502	4387.779451	23.925978
121.957864	4390.236134	23.930995
122.138722	4389.200621	23.936013
122.592194	4384.476159	23.941031
122.199119	4392.642683	23.946048
123.018930	4378.359915	23.951066
123.050998	4375.341398	23.956083
123.060392	4373.914116	23.961101
122.995311	4374.001979	23.966119
123.034225	4375.241227	23.971136
123.244852	4371.406155	23.976154
122.876431	4382.294340	23.981171
123.574351	4372.985537	23.986189
123.414222	4378.403571	23.991207
123.357832	4394.267256	23.996224
123.724351	4398.517113	24.001242
123.633320	4410.249297	24.006259
123.571235	4397.526094	24.011277
123.736934	4402.604061	24.016295
123.395127	4412.607111	24.021312
123.763792	4427.282421	24.026330
123.906933	4439.183425	24.031347
124.333803	4444.873802	24.036365
124.416306	4464.678231	24.041383
124.280281	4472.378281	24.046400
124.657922	4469.958590	24.051418
124.467599	4471.821586	24.056435
124.555474	4483.168729	24.061453
124.743117	4504.301194	24.066471
124.946475	4504.485262	24.071488
125.125138	4516.323365	24.076506
125.381744	4523.938090	24.081523
125.646903	4529.409534	24.086541
125.703707	4516.584300	24.091559
126.098734	4529.496182	24.096576
126.101844	4504.509753	24.101594
126.145775	4535.682787	24.106611
126.332050	4544.576942	24.111629
126.459570	4552.794545	24.116647
126.372971	4548.267548	24.121664
126.689096	4553.815625	24.126682
126.676513	4557.695461	24.131699
126.610382	4566.686851	24.136717
126.880899	4578.040107	24.141735
127.029641	4582.095669	24.146752
127.351038	4571.068528	24.151770
127.362838	4577.129134	24.156787
127.596677	4594.116011	24.161805
128.055478	4608.696278	24.166823
127.608902	4606.295819	24.171840
128.166963	4597.717524	24.176858
128.002215	4610.762129	24.181875
128.240398	4595.722849	24.186893
128.507669	4600.863237	24.191911
128.261219	4624.779199	24.196928
128.775555	4624.878811	24.201946
128.658605	4625.620961	24.206963
128.738035	4627.818957	24.211981
128.872499	4617.885740	24.216999
128.806537	4635.526574	24.222016
129.328590	4644.930305	24.227034
129.525243	4649.557931	24.232051
129.848928	4643.023603	24.237069
130.242009	4644.584693	24.242087
130.016306	4638.651811	24.247104
130.270474	4641.383575	24.252122
130.165662	4634.547585	24.257139
130.099774	4630.764046	24.262157
130.624070	4631.369529	24.267175
130.229084	4639.857386	24.272192
130.490292	4649.100269	24.277210
130.666295	4658.297784	24.282227
130.528452	4663.655537	24.287245
130.779536	4664.382156	24.292263
130.591387	4680.753372	24.297280
130.826244	4685.072311	24.302298
131.122904	4693.723887	24.307315
131.066852	4710.980068	24.312333
131.381388	4718.313249	24.317351
131.362401	4720.762577	24.322368
131.916825	4720.575624	24.327386
131.840413	4733.055299	24.332403
131.953054	4754.598952	24.337421
132.620646	4747.722299	24.342439
132.679758	4752.080140	24.347456
132.665064	4757.885724	24.352474
132.337369	4753.158722	24.357491
132.448625	4754.216741	24.362509
132.763482	4763.294517	24.367527
132.921103	4771.400954	24.372544
133.106708	4776.867912	24.377562
132.969266	4779.071054	24.382579
133.205461	4784.548555	24.387597
133.685089	4789.546429	24.392615
133.389227	4801.794680	24.397632
133.898508	4799.398862	24.402650
134.039766	4803.034817	24.407667
133.705432	4811.543849	24.412685
133.873778	4807.536509	24.417703
134.065181	4816.627233	24.422720
134.391501	4820.746043	24.427738
134.608731	4830.786919	24.432755
134.306171	4829.323732	24.437773
135.000449	4834.196775	24.442791
134.810020	4855.922547	24.447808
135.172393	4851.862268	24.452826
135.301813	4859.439113	24.457843
134.885372	4856.837948	24.462861
135.712986	4869.000624	24.467879
135.754373	4875.723050	24.472896
136.424582	4861.404324	24.477914
136.548451	4873.576585	24.482931
136.426886	4876.212981	24.487949
136.662772	4871.032158	24.492967
136.625746	4874.410556	24.497984
136.413519	4871.268122	24.503002
136.377640	4870.999556	24.508019
136.651077	4871.909122	24.513037
136.610125	4876.146118	24.518055
136.768347	4894.163229	24.523072
136.725215	4902.339130	24.528090
136.905407	4901.065484	24.533107
136.683775	4931.575252	24.538125
137.495421	4924.047497	24.543143
137.182199	4939.685252	24.548160
137.362662	4952.315981	24.553178
137.684828	4961.467081	24.558195
137.574661	4963.691728	24.563213
137.950373	4978.237248	24.568231
138.124985	4989.236538	24.573248
138.549268	4981.407767	24.578266
139.295316	4997.575736	24.583283
139.405202	5003.897099	24.588301
139.725470	4986.664145	24.593319
140.126142	4974.851502	24.598336
140.241096	4956.000777	24.603354
139.859993	4951.371523	24.608371
140.088045	4951.388904	24.613389
140.313441	4950.022739	24.618407
140.216427	4948.857497	24.623424
140.068371	4943.275875	24.628442
140.412136	4951.838702	24.633459
140.297049	4954.833916	24.638477
140.124299	4948.175171	24.643495
140.182878	4970.204871	24.648512
140.111390	4974.581204	24.653530
140.708182	4969.414344	24.658547
140.811200	4990.915816	24.663565
141.058781	4995.066582	24.668583
141.044733	5013.888748	24.673600
141.196580	5002.444789	24.678618
141.087542	5013.453167	24.683635
141.018245	5050.774480	24.688653
141.577634	5034.525685	24.693671
141.271104	5058.462474	24.698688
141.577216	5057.594037	24.703706
141.687304	5067.111770	24.708723
141.459123	5091.947566	24.713741
141.966535	5097.512661	24.718759
142.107534	5109.504698	24.723776
142.447651	5128.690178	24.728794
142.636569	5125.656230	24.733811
142.973807	5132.664957	24.738829
143.171521	5139.527431	24.743847
143.134454	5141.693563	24.748864
143.401812	5162.646802	24.753882
143.481762	5163.749791	24.758899
143.474344	5171.573044	24.763917
144.246980	5174.212147	24.768935
143.942289	5172.769754	24.773952
143.802204	5177.054711	24.778970
144.090841	5185.173577	24.783987
144.360881	5188.704870	24.789005
144.550544	5171.502744	24.794023
144.670630	5193.869877	24.799040
145.141807	5189.772240	24.804058
145.143198	5207.471495	24.809075
144.985263	5208.579144	24.814093
145.606973	5207.359307	24.819111
145.333632	5202.630666	24.824128
145.492863	5211.498173	24.829146
145.866790	5219.233239	24.834163
145.733209	5230.839983	24.839181
146.001764	5224.854740	24.844199
145.780581	5234.625366	24.849216
146.074936	5256.036525	24.854234
146.278191	5259.281987	24.859251
146.237724	5260.872254	24.864269
146.441524	5266.154469	24.869287
146.368320	5297.621636	24.874304
146.664581	5301.195085	24.879322
147.146029	5306.994099	24.884339
146.991156	5313.640075	24.889357
147.660557	5322.884818	24.894375
147.594841	5321.055246	24.899392
147.702944	5319.272553	24.904410
148.017959	5328.792416	24.909427
148.082198	5333.025542	24.914445
148.317179	5356.601625	24.919463
148.298620	5345.357247	24.924480
148.516452	5352.606301	24.929498
148.544480	5363.667481	24.934515
148.721424	5376.559797	24.939533
148.739403	5376.761121	24.944551
149.060581	5385.216882	24.949568
148.942546	5408.259176	24.954586
149.477910	5402.048262	24.959603
149.614126	5411.116559	24.964621
149.750199	5402.586686	24.969639
150.040886	5424.796023	24.974656
149.687161	5434.322892	24.979674
150.372059	5424.558089	24.984691
150.239711	5429.518690	24.989709
150.416503	5424.510856	24.994727
151.268410	5438.481607	24.999744
151.412737	5441.307656	25.004762
151.983488	5438.436570	25.009779
151.811043	5419.844612	25.014797
151.916819	5410.773611	25.019815
152.158046	5396.263045	25.024832
151.686857	5406.877546	25.029850
151.818302	5391.046774	25.034867
151.660164	5403.904310	25.039885
151.937959	5430.381657	25.044903
152.270789	5425.328353	25.049920
152.043337	5429.950688	25.054938
152.437686	5432.854337	25.059955
152.623038	5452.420163	25.064973
152.769600	5455.997120	25.069991
152.976966	5464.795785	25.075008
152.865387	5473.599119	25.080026
153.238446	5469.631416	25.085043
153.054831	5475.915234	25.090061
152.953709	5467.918281	25.095079
153.092163	5485.053403	25.100096
153.076644	5498.789140	25.105114
153.536765	5509.252977	25.110131
153.067308	5535.370838	25.115149
153.595594	5545.313135	25.120167
153.741396	5558.950606	25.125184
153.887914	5578.184379	25.130202
154.437511	5586.700552	25.135219
154.508812	5606.961883	25.140237
154.674699	5600.667827	25.145255
154.895965	5616.407335	25.150272
155.073814	5623.167780	25.155290
155.846316	5612.414239	25.160307
155.768148	5610.676466	25.165325
155.631977	5619.832416	25.170343
156.302826	5639.027272	25.175360
155.827039	5643.864741	25.180378
156.216059	5641.494183	25.185395
156.328429	5644.388945	25.190413
156.252662	5663.827684	25.195431
156.164518	5668.616073	25.200448
156.307879	5687.547704	25.205466
156.645782	5694.546336	25.210483
156.652148	5702.800314	25.215501
157.006563	5725.822893	25.220519
157.287368	5725.164144	25.225536
157.065515	5735.292328	25.230554
157.531089	5730.831254	25.235571
158.144594	5743.706471	25.240589
158.140459	5745.282516	25.245607
158.444855	5753.425457	25.250624
158.300826	5746.168626	25.255642
158.738426	5758.327539	25.260659
158.702384	5776.115916	25.265677
158.567192	5778.375525	25.270695
159.108439	5787.160550	25.275712
158.910063	5813.889689	25.280730
159.426169	5816.863070	25.285747
159.739990	5819.319400	25.290765
159.970581	5812.985825	25.295783
159.865996	5820.093853	25.300800
160.087118	5830.016995	25.305818
160.388995	5836.572759	25.310835
160.506416	5840.727146	25.315853
160.558357	5842.285666	25.320871
160.718587	5832.164718	25.325888
160.867240	5858.673184	25.330906
160.995392	5865.340355	25.335923
161.080839	5871.173513	25.340941
161.071961	5876.753713	25.345959
161.440822	5888.084982	25.350976
161.317679	5909.310075	25.355994
162.041491	5906.197835	25.361011
161.482921	5915.859250	25.366029
161.483349	5926.428462	25.371047
161.932046	5929.105081	25.376064
161.957051	5939.979738	25.381082
162.422796	5953.415059	25.386099
162.809297	5960.931061	25.391117
162.877779	5964.789582	25.396135
163.498758	5974.960971	25.401152
163.056146	5982.634454	25.406170
163.466017	5982.739138	25.411187
163.538258	5987.267229	25.416205
163.535899	5982.335283	25.421223
163.932744	5985.634750	25.426240
164.068280	6003.707290	25.431258
164.527104	6008.866110	25.436275
164.317617	6002.787879	25.441293
164.668830	5997.918787	25.446311
165.139460	5992.510198	25.451328
164.710923	5997.621902	25.456346
165.171782	6012.744964	25.461363
165.187750	6034.450472	25.466381
165.058638	6035.126968	25.471399
165.048818	6027.181583	25.476416
165.392556	6049.229867	25.481434
165.692629	6041.035602	25.486451
166.138740	6027.920360	25.491469
165.977042	6040.426192	25.496487
166.300898	6058.876407	25.501504
166.240244	6072.274378	25.506522
166.819819	6069.476539	25.511539
166.682642	6077.279944	25.516557
166.760840	6087.737186	25.521575
166.982454	6095.339562	25.526592
166.707691	6111.164676	25.531610
167.161805	6143.834421	25.536627
167.311380	6145.729654	25.541645
167.333450	6156.598645	25.546663
167.395423	6159.823537	25.551680
167.787960	6181.755265	25.556698
167.917284	6205.108704	25.561715
167.989363	6206.704097	25.566733
167.976073	6233.605371	25.571751
168.340471	6248.540627	25.576768
168.599085	6250.673806	25.581786
169.011230	6256.900450	25.586803
169.277810	6253.964498	25.591821
169.281197	6276.915156	25.596839
169.665384	6281.279958	25.601856
169.865874	6291.940791	25.606874
169.799482	6294.941207	25.611891
170.282055	6300.731747	25.616909
170.878922	6315.664096	25.621927
171.709428	6292.226597	25.626944
171.380652	6292.517123	25.631962
171.646212	6293.997077	25.636979
172.056702	6286.516066	25.641997
172.048263	6297.477613	25.647015
172.507050	6281.410724	25.652032
172.235070	6266.914456	25.657050
172.210812	6253.164022	25.662067
172.246400	6248.006000	25.667085
172.400483	6274.896229	25.672103
172.505063	6272.112259	25.677120
172.837566	6290.844046	25.682138
172.533357	6281.907619	25.687156
172.676614	6283.520398	25.692173
172.703873	6294.164966	25.697191
172.695391	6309.645441	25.702208
172.473018	6318.303351	25.707226
172.775108	6354.798547	25.712244
173.094440	6367.078675	25.717261
172.790590	6385.915719	25.722279
173.241577	6392.169076	25.727296
173.578258	6416.665163	25.732314
173.833523	6428.021105	25.737332
174.116200	6444.297857	25.742349
174.360438	6455.500495	25.747367
174.715523	6446.387310	25.752384
174.661994	6466.485696	25.757402
174.885781	6478.447777	25.762420
174.950455	6483.311970	25.767437
175.221504	6494.938633	25.772455
175.954859	6497.506103	25.777472
175.866642	6514.162380	25.782490
175.637114	6517.426060	25.787508
176.437333	6516.369194	25.792525
176.187982	6531.531350	25.797543
176.492031	6534.843118	25.802560
176.383450	6539.715478	25.807578
176.798120	6560.283974	25.812596
176.992924	6561.755169	25.817613
177.250205	6571.657056	25.822631
177.410308	6561.114320	25.827648
177.127628	6579.046345	25.832666
177.594364	6600.910484	25.837684
177.752342	6597.408046	25.842701
177.786415	6611.412206	25.847719
178.148342	6627.898146	25.852736
178.096879	6630.228310	25.857754
178.385793	6650.431011	25.862772
178.490274	6651.620228	25.867789
178.710110	6667.668965	25.872807
179.098471	6670.198172	25.877824
178.801960	6684.261744	25.882842
179.110604	6698.755369	25.887860
179.767309	6716.303158	25.892877
179.855048	6725.996100	25.897895
180.292925	6732.098973	25.902912
180.340787	6732.528890	25.907930
180.396435	6750.435924	25.912948
180.651587	6751.799508	25.917965
180.613509	6775.212168	25.922983
181.089276	6770.999567	25.928000
180.896805	6788.426272	25.933018
181.035184	6797.442247	25.938036
181.591421	6816.402316	25.943053
181.675419	6819.356719	25.948071
181.942405	6822.520309	25.953088
182.504394	6842.634034	25.958106
182.371062	6847.774415	25.963124
182.552465	6834.241515	25.968141
182.592709	6856.397784	25.973159
182.839738	6865.300550	25.978176
182.900394	6877.211919	25.983194
183.013460	6885.126378	25.988212
183.323039	6893.760502	25.993229
183.024981	6898.066513	25.998247
183.290981	6917.045518	26.003264
184.104060	6909.289778	26.008282
184.556939	6899.678181	26.013300
184.931193	6891.464919	26.018317
184.984756	6907.124748	26.023335
185.327603	6912.452671	26.028352
185.753326	6918.218182	26.033370
185.961311	6913.418156	26.038388
186.077126	6901.579078	26.043405
186.108893	6902.533032	26.048423
186.401364	6880.776032	26.053440
186.095454	6902.062589	26.058458
186.145981	6905.776245	26.063476
185.988294	6912.493452	26.068493
186.306187	6930.176219	26.073511
186.289545	6930.655390	26.078528
186.325602	6940.066389	26.083546
186.263401	6958.979961	26.088564
186.506554	6963.581692	26.093581
186.711836	6984.197153	26.098599
186.855876	6984.961657	26.103616
187.008616	7011.681675	26.108634
186.874552	7025.245376	26.113652
187.557005	7043.604421	26.118669
187.577363	7050.708898	26.123687
187.625075	7060.596891	26.128704
187.715974	7083.012098	26.133722
188.243904	7096.212880	26.138740
188.700334	7109.240404	26.143757
188.882798	7120.838851	26.148775
189.397134	7112.958317	26.153792
190.133933	7120.268935	26.158810
190.087594	7131.059330	26.163828
189.820375	7117.894868	26.168845
190.169303	7121.660870	26.173863
190.660375	7142.669578	26.178880
190.986053	7149.845729	26.183898
190.679507	7155.216450	26.188916
190.990316	7153.099989	26.193933
191.048756	7156.918721	26.198951
191.123035	7166.651175	26.203968
191.691172	7185.137174	26.208986
191.502881	7188.575321	26.214004
191.938842	7183.625709	26.219021
192.055904	7205.225554	26.224039
191.833059	7219.649959	26.229056
192.233667	7214.172194	26.234074
192.117986	7240.925136	26.239092
192.680557	7243.028710	26.244109
192.743724	7254.961215	26.249127
192.630763	7268.046720	26.254144
193.064134	7277.527739	26.259162
193.038105	7294.455735	26.264180
193.232400	7296.092478	26.269197
193.556662	7314.649639	26.274215
193.729818	7326.676651	26.279232
194.118699	7331.654509	26.284250
194.188234	7360.987924	26.289268
194.322691	7361.007391	26.294285
194.555862	7385.525240	26.299303
194.522042	7402.164802	26.304320
194.886563	7409.051119	26.309338
194.484666	7434.459995	26.314356
195.049600	7442.224464	26.319373
195.450855	7465.055194	26.324391
195.882663	7476.598528	26.329408
196.363820	7489.744361	26.334426
196.200610	7501.633333	26.339444
196.453539	7511.175023	26.344461
196.566367	7523.283824	26.349479
196.792962	7522.130291	26.354496
197.173383	7544.392779	26.359514
197.327770	7550.177365	26.364532
197.883720	7540.701935	26.369549
197.910273	7571.836217	26.374567
198.269197	7577.985547	26.379584
198.622951	7592.607224	26.384602
198.399850	7587.994786	26.389620
198.649204	7592.138866	26.394637
198.728493	7608.923779	26.399655
199.161464	7608.536351	26.404672
199.413896	7605.154342	26.409690
199.176567	7629.098169	26.414708
200.066426	7639.739741	26.419725
199.965853	7640.729782	26.424743
200.147116	7651.304139	26.429760
200.017355	7646.558121	26.434778
200.176392	7649.757043	26.439796
200.688889	7674.310313	26.444813
200.455324	7680.139355	26.449831
200.388077	7690.462595	26.454848
201.279992	7691.633630	26.459866
200.762944	7702.143823	26.464884
201.028219	7727.995052	26.469901
201.344153	7727.372560	26.474919
201.316034	7748.420603	26.479936
202.054122	7758.636030	26.484954
202.304956	7778.685797	26.489972
202.093002	7787.089174	26.494989
202.490569	7783.394092	26.500007
202.629052	7802.782741	26.505024
203.150642	7810.389156	26.510042
203.162955	7810.910827	26.515060
203.602400	7835.417346	26.520077
203.901451	7849.563127	26.525095
203.887370	7844.567951	26.530112
204.074802	7845.484428	26.535130
204.010043	7875.267875	26.540148
204.378436	7885.549194	26.545165
204.514734	7893.611543	26.550183
205.026045	7897.070511	26.555200
205.045289	7897.275203	26.560218
205.384000	7929.619595	26.565236
205.558487	7927.557851	26.570253
205.615805	7944.540506	26.575271
205.761367	7963.074397	26.580288
206.073750	7963.071557	26.585306
206.312901	7985.875478	26.590324
206.556976	7996.764191	26.595341
206.875505	7990.315190	26.600359
206.966490	8003.388872	26.605376
207.503444	8005.242382	26.610394
207.302759	8014.383598	26.615412
207.223959	8031.387261	26.620429
207.878959	8047.874312	26.625447
208.073276	8040.594387	26.630464
208.574940	8072.689249	26.635482
208.778442	8076.316471	26.640500
208.829531	8084.600931	26.645517
209.222557	8084.628087	26.650535
209.216135	8109.716721	26.655552
209.506647	8108.491940	26.660570
209.470513	8106.039651	26.665588
209.884839	8120.578560	26.670605
210.109206	8125.374343	26.675623
210.003546	8123.242291	26.680640
210.239884	8147.135418	26.685658
210.517721	8163.208388	26.690676
210.286619	8173.557439	26.695693
210.628283	8196.353390	26.700711
210.909883	8209.591082	26.705728
211.266375	8229.335689	26.710746
211.553234	8237.788424	26.715764
212.030186	8247.512510	26.720781
212.238816	8261.516860	26.725799
212.059942	8262.107941	26.730816
212.505146	8269.653950	26.735834
212.783966	8293.789961	26.740852
212.737062	8310.201860	26.745869
213.260498	8307.423157	26.750887
213.348520	8311.306593	26.755904
213.872705	8313.761647	26.760922
214.088512	8321.032101	26.765940
214.270126	8340.330004	26.770957
214.662215	8342.750965	26.775975
214.598189	8348.185985	26.780992
214.852585	8337.090891	26.786010
214.638452	8345.908436	26.791028
215.199310	8349.772044	26.796045
215.250501	8363.952150	26.801063
215.227447	8356.637894	26.806080
215.290700	8368.772074	26.811098
215.551822	8386.952620	26.816116
215.777198	8393.413401	26.821133
216.103696	8406.106665	26.826151
216.105130	8427.250758	26.831168
216.625083	8440.268103	26.836186
216.235782	8457.653549	26.841204
216.459046	8473.044294	26.846221
216.925360	8489.679555	26.851239
216.975902	8506.435514	26.856256
217.531727	8528.438839	26.861274
217.737596	8541.545181	26.866292
217.648605	8565.391083	26.871309
218.043422	8571.329295	26.876327
218.449029	8597.839293	26.881344
218.465556	8605.981657	26.886362
219.045169	8624.414677	26.891380
218.912907	8637.120123	26.896397
219.142199	8647.839230	26.901415
219.558027	8668.733227	26.906432
219.857600	8681.497325	26.911450
220.334626	8691.465060	26.916468
220.371380	8701.105413	26.921485
220.681448	8708.473106	26.926503
220.678404	8719.852901	26.931520
221.202528	8730.710816	26.936538
221.425331	8741.082911	26.941556
221.592856	8743.229910	26.946573
222.083579	8771.281771	26.951591
222.004782	8788.271278	26.956608
221.985310	8781.894345	26.961626
222.067666	8799.462952	26.966644
222.331737	8810.964089	26.971661
222.759511	8830.957600	26.976679
222.685214	8847.175299	26.981696
223.188700	8862.578411	26.986714
223.294575	8870.931422	26.991732
223.666803	8893.611479	26.996749
224.087069	8880.747062	27.001767
224.339103	8905.715485	27.006784
224.362680	8918.772702	27.011802
224.672702	8929.723628	27.016820
224.721621	8943.213837	27.021837
225.081739	8962.604306	27.026855
225.354294	8969.215851	27.031872
225.402355	8989.417230	27.036890
225.599912	9007.176555	27.041908
225.831597	9013.329354	27.046925
226.396842	9004.558859	27.051943
226.664934	9022.709051	27.056960
226.978876	9038.866739	27.061978
227.286166	9042.823615	27.066996
227.455790	9041.163460	27.072013
227.324003	9050.592417	27.077031
227.594697	9071.486507	27.082048
228.135288	9066.022793	27.087066
228.366007	9073.963808	27.092084
228.376231	9101.206350	27.097101
228.485018	9107.379491	27.102119
228.243071	9112.162035	27.107136
228.620564	9137.705582	27.112154
229.008668	9146.216118	27.117172
228.717948	9172.379753	27.122189
229.384508	9178.807348	27.127207
229.683816	9194.864426	27.132224
229.708334	9205.542913	27.137242
229.960113	9223.592842	27.142260
229.720937	9240.087880	27.147277
230.024348	9243.245944	27.152295
230.325778	9286.327579	27.157312
230.618832	9302.633922	27.162330
230.851132	9314.870076	27.167348
231.353484	9340.624901	27.172365
231.689712	9343.399470	27.177383
231.994443	9359.523561	27.182400
232.349377	9361.968938	27.187418
232.898497	9378.618234	27.192436
232.858255	9395.112859	27.197453
233.278769	9405.780405	27.202471
233.211471	9405.977360	27.207488
233.413371	9420.673080	27.212506
233.785663	9429.288782	27.217524
233.692169	9452.306522	27.222541
233.824851	9470.660769	27.227559
234.100919	9480.884337	27.232576
234.030706	9502.366227	27.237594
234.519770	9509.437691	27.242612
235.054694	9532.966128	27.247629
235.817059	9538.464308	27.252647
235.804233	9551.615494	27.257664
235.802834	9564.958578	27.262682
236.199089	9579.290710	27.267700
236.111428	9596.332955	27.272717
236.848018	9604.605777	27.277735
237.211144	9609.932056	27.282752
237.176561	9614.032207	27.287770
237.051785	9637.655616	27.292788
237.621096	9643.471667	27.297805
237.639615	9664.197094	27.302823
237.718675	9681.043315	27.307840
237.883992	9695.156125	27.312858
238.584306	9699.518495	27.317876
238.540511	9720.440191	27.322893
239.363676	9726.468762	27.327911
239.462832	9738.333384	27.332928
239.683361	9751.553309	27.337946
240.356426	9756.788257	27.342964
240.390731	9753.277204	27.347981
240.895666	9754.792778	27.352999
240.913671	9760.063485	27.358016
241.379612	9770.687537	27.363034
241.565362	9773.264122	27.368052
241.460168	9769.758783	27.373069
241.723088	9774.777136	27.378087
241.816544	9803.237536	27.383104
242.345315	9806.523113	27.388122
242.622575	9817.190973	27.393140
242.424374	9821.869612	27.398157
242.478293	9821.745637	27.403175
242.740136	9838.901332	27.408192
242.251559	9862.735634	27.413210
242.962997	9869.052119	27.418228
242.883183	9898.709504	27.423245
243.193353	9918.085761	27.428263
243.501514	9934.139761	27.433280
243.431469	9963.638108	27.438298
243.988275	9978.568739	27.443316
244.115958	10015.970840	27.448333
244.525830	10035.485949	27.453351
244.828642	10049.781167	27.458368
244.720816	10066.812278	27.463386
245.187666	10076.077553	27.468404
245.260491	10105.560433	27.473421
245.393353	10106.787763	27.478439
246.161342	10135.352361	27.483456
246.138510	10156.342059	27.488474
246.589644	10156.956731	27.493492
246.687160	10188.184452	27.498509
246.976019	10200.071642	27.503527
247.167097	10221.323848	27.508544
247.507039	10244.624812	27.513562
248.632025	10259.123896	27.518580
248.573874	10256.592987	27.523597
248.819628	10268.857586	27.528615
249.427079	10286.343442	27.533632
249.601315	10276.775072	27.538650
250.222630	10287.903949	27.543668
249.867342	10286.421769	27.548685
249.891241	10306.956508	27.553703
250.259390	10318.406094	27.558720
250.282994	10330.794095	27.563738
250.825016	10331.870342	27.568756
251.061980	10330.401380	27.573773
251.286536	10352.824329	27.578791
251.902294	10365.379205	27.583808
251.967204	10367.069159	27.588826
252.306458	10377.739757	27.593844
252.392512	10400.555895	27.598861
252.011334	10402.959990	27.603879
252.815997	10422.800283	27.608896
253.082990	10430.270425	27.613914
253.294649	10448.363820	27.618932
253.385759	10455.562901	27.623949
253.697580	10470.875566	27.628967
253.650646	10492.730697	27.633984
253.892911	10509.974638	27.639002
254.358294	10527.232939	27.644020
254.187758	10545.043765	27.649037
254.321650	10572.416482	27.654055
254.999669	10588.064998	27.659072
255.222434	10602.069863	27.664090
255.344797	10630.995674	27.669108
255.721790	10642.115537	27.674125
255.981083	10657.440211	27.679143
256.310176	10670.786334	27.684160
256.374009	10695.122210	27.689178
256.987032	10711.214066	27.694196
257.125990	10722.318956	27.699213
257.703935	10726.622269	27.704231
258.643713	10724.833915	27.709248
258.885673	10724.724556	27.714266
259.277713	10735.025878	27.719284
259.608540	10758.169971	27.724301
259.394679	10764.259202	27.729319
259.856381	10772.156602	27.734336
259.953543	10766.689167	27.739354
260.051607	10774.180290	27.744372
259.806006	10790.794574	27.749389
260.275947	10808.495937	27.754407
260.561955	10811.368083	27.759424
260.087660	10825.262219	27.764442
260.810293	10846.571597	27.769460
260.787726	10856.653174	27.774477
260.780806	10871.996827	27.779495
261.223220	10897.027509	27.784512
261.498189	10918.857609	27.789530
261.884565	10931.701343	27.794548
262.091490	10945.844622	27.799565
262.220119	10956.053322	27.804583
262.884144	10982.768020	27.809600
262.811481	10992.984002	27.814618
263.336139	11019.479153	27.819636
263.581227	11031.514418	27.824653
263.883307	11047.610719	27.829671
263.947750	11055.428154	27.834688
263.995160	11086.188513	27.839706
264.151182	11101.375481	27.844724
264.645573	11115.477720	27.849741
264.815239	11152.332759	27.854759
265.411485	11154.417135	27.859776
265.114405	11190.760114	27.864794
265.505806	11203.007670	27.869812
266.264646	11235.712410	27.874829
266.321798	11249.486021	27.879847
266.801589	11263.115767	27.884864
266.734446	11282.475662	27.889882
267.285251	11293.251360	27.894900
267.812066	11317.138277	27.899917
267.875877	11338.332638	27.904935
268.278434	11345.466484	27.909952
268.449760	11356.572769	27.914970
268.915509	11363.790718	27.919988
269.014217	11377.637929	27.925005
269.708573	11386.774998	27.930023
270.362429	11389.785000	27.935040
270.691170	11391.930936	27.940058
270.868848	11393.418024	27.945076
270.903803	11392.752017	27.950093
271.244356	11416.479210	27.955111
271.767378	11428.620901	27.960128
271.407254	11444.264520	27.965146
271.696037	11446.465908	27.970164
271.950526	11453.827517	27.975181
272.048419	11474.643012	27.980199
272.059796	11490.280445	27.985216
271.986501	11514.184083	27.990234
272.362593	11526.729842	27.995252
272.806060	11547.349685	28.000269
272.766221	11578.187636	28.005287
273.262913	11597.439790	28.010304
273.140530	11630.452425	28.015322
273.497777	11653.726586	28.020340
274.028459	11680.380971	28.025357
274.379245	11700.713017	28.030375
274.865733	11715.694711	28.035392
275.464731	11730.858722	28.040410
276.485036	11729.472140	28.045428
277.049257	11729.203970	28.050445
277.324939	11741.718431	28.055463
277.560925	11735.740076	28.060480
277.569749	11737.735659	28.065498
277.641957	11736.344212	28.070516
278.565190	11745.790312	28.075533
278.025215	11768.065030	28.080551
278.508010	11763.823982	28.085568
278.246151	11770.647885	28.090586
278.321354	11795.283707	28.095604
278.695984	11806.882976	28.100621
278.873250	11812.508561	28.105639
278.699788	11830.896398	28.110656
279.251259	11860.783208	28.115674
278.939197	11864.710764	28.120692
279.328206	11890.502611	28.125709
279.515417	11922.771417	28.130727
279.903226	11942.424067	28.135744
280.563407	11957.883072	28.140762
280.972303	11983.161275	28.145780
281.285186	11999.177177	28.150797
281.396668	12020.745081	28.155815
281.856732	12016.893758	28.160832
282.278254	12049.154044	28.165850
282.511911	12059.768368	28.170868
282.991978	12060.636751	28.175885
283.124411	12088.031990	28.180903
283.255894	12087.257831	28.185920
283.549737	12116.528268	28.190938
283.686726	12132.882981	28.195956
284.065234	12144.038305	28.200973
284.083269	12168.695961	28.205991
284.485931	12182.098944	28.211008
284.678081	12209.759477	28.216026
284.637115	12235.615824	28.221044
285.238418	12244.477262	28.226061
285.155524	12279.097401	28.231079
285.731857	12290.452555	28.236096
286.161259	12317.157821	28.241114
286.553628	12334.703515	28.246132
286.909712	12369.975350	28.251149
287.021376	12384.587070	28.256167
287.733086	12405.120367	28.261184
287.930408	12415.079141	28.266202
288.044991	12437.368754	28.271220
288.469055	12455.614466	28.276237
288.768713	12458.579198	28.281255
289.257468	12481.654779	28.286272
289.205203	12504.252523	28.291290
289.165169	12524.557213	28.296308
289.723707	12536.468552	28.301325
289.702205	12566.265402	28.306343
290.052854	12587.176875	28.311360
290.317217	12619.105794	28.316378
290.677600	12635.777068	28.321396
291.106028	12661.431279	28.326413
291.442816	12686.473537	28.331431
292.276756	12693.779378	28.336448
292.460763	12700.678914	28.341466
292.909897	12726.490531	28.346484
293.214936	12736.278864	28.351501
293.598611	12760.654840	28.356519
293.978542	12771.919878	28.361536
294.215524	12785.483885	28.366554
294.517723	12799.260883	28.371572
294.713749	12811.196076	28.376589
294.702487	12829.936426	28.381607
295.100615	12841.017298	28.386624
295.325435	12853.905808	28.391642
295.325972	12869.415584	28.396660
295.834602	12888.837493	28.401677
295.948875	12905.557586	28.406695
296.364042	12921.712719	28.411712
296.586866	12940.493311	28.416730
296.674840	12963.308041	28.421748
297.084938	12987.783994	28.426765
297.329764	13007.619929	28.431783
297.626175	13026.991975	28.436800
298.136712	13049.585744	28.441818
298.396623	13066.946909	28.446836
298.957627	13087.907794	28.451853
299.223235	13108.102843	28.456871
299.412407	13120.562547	28.461888
299.853701	13135.993458	28.466906
299.875419	13164.945967	28.471924
300.145884	13172.052028	28.476941
300.438439	13193.452917	28.481959
300.787034	13205.412044	28.486976
301.072238	13230.310818	28.491994
301.030626	13239.947149	28.497012
301.947381	13247.950236	28.502029
301.940566	13273.325930	28.507047
302.091228	13288.732516	28.512064
302.555427	13290.168509	28.517082
302.871166	13318.800109	28.522100
303.222154	13338.604730	28.527117
303.405893	13360.895223	28.532135
303.909169	13363.312781	28.537152
304.038071	13386.217467	28.542170
304.034733	13416.197247	28.547188
304.672963	13420.486612	28.552205
304.788920	13446.129087	28.557223
304.873168	13457.719217	28.562240
305.216956	13489.397214	28.567258
305.684072	13507.761492	28.572276
305.893916	13533.810907	28.577293
306.009180	13559.548222	28.582311
306.289221	13595.151243	28.587328
306.681972	13617.607686	28.592346
306.885464	13643.094187	28.597364
307.593500	13679.518593	28.602381
307.517261	13686.527729	28.607399
308.102223	13724.100849	28.612416
308.422430	13754.259446	28.617434
308.655550	13768.294510	28.622452
309.387525	13786.930513	28.627469
309.391620	13809.150448	28.632487
309.783037	13825.042520	28.637504
310.176343	13845.716929	28.642522
310.258354	13870.892934	28.647540
310.832568	13888.781386	28.652557
311.620439	13902.671341	28.657575
311.788269	13914.689222	28.662592
312.270435	13933.845719	28.667610
312.594699	13961.055642	28.672628
312.974866	13965.345242	28.677645
313.385567	13974.960863	28.682663
313.807984	13978.926742	28.687680
314.868545	13987.929166	28.692698
314.708419	13996.884276	28.697716
315.128792	13994.399002	28.702733
315.388151	13990.667050	28.707751
315.456355	14012.882976	28.712768
315.504098	14029.159801	28.717786
315.591392	14036.781865	28.722804
316.253298	14043.163364	28.727821
316.423594	14047.950957	28.732839
316.293606	14078.751837	28.737856
316.701781	14083.927197	28.742874
317.229656	14123.655408	28.747892
316.888115	14130.420184	28.752909
317.163536	14163.180798	28.757927
317.789632	14183.385395	28.762944
317.766374	14209.792729	28.767962
317.823500	14234.782731	28.772980
318.241470	14263.975879	28.777997
318.781299	14281.460721	28.783015
318.729007	14320.966934	28.788032
319.018992	14338.036110	28.793050
319.218274	14383.301709	28.798068
319.779591	14401.990255	28.803085
320.277507	14430.759190	28.808103
320.604585	14473.476210	28.813120
321.121905	14486.862957	28.818138
321.331320	14514.868120	28.823156
321.803168	14538.556150	28.828173
321.842527	14552.571900	28.833191
322.014497	14578.397591	28.838208
322.655549	14596.672910	28.843226
322.762631	14629.096664	28.848244
323.200102	14657.106945	28.853261
323.385285	14673.424744	28.858279
323.679513	14699.046048	28.863296
324.104423	14721.571199	28.868314
324.557985	14746.862105	28.873332
324.949763	14758.124997	28.878349
325.451276	14792.296216	28.883367
325.329655	14805.634342	28.888384
326.200493	14818.130875	28.893402
327.077470	14823.881457	28.898420
327.752193	14825.246569	28.903437
328.273990	14843.349606	28.908455
328.058044	14864.565648	28.913472
328.637038	14861.614359	28.918490
328.635984	14884.634031	28.923508
328.797384	14892.091388	28.928525
329.095912	14907.073222	28.933543
328.869068	14929.194155	28.938560
329.445963	14949.173023	28.943578
329.298455	14971.154832	28.948596
329.677975	15001.008093	28.953613
330.087677	15031.948550	28.958631
330.052795	15061.315651	28.963648
330.499065	15084.944090	28.968666
330.657768	15120.058313	28.973684
331.119044	15143.564586	28.978701
331.561156	15179.547746	28.983719
331.722505	15213.520741	28.988736
332.273618	15231.176522	28.993754
332.855216	15266.662466	28.998772
333.111799	15276.734561	29.003789
334.022068	15301.848443	29.008807
333.893730	15343.189937	29.013824
334.481313	15355.602875	29.018842
335.005717	15378.388294	29.023860
335.382337	15401.508627	29.028877
335.870089	15411.038302	29.033895
335.959459	15436.871119	29.038912
336.592416	15450.297870	29.043930
336.788197	15458.227330	29.048948
337.503154	15463.669226	29.053965
337.674245	15486.076617	29.058983
337.912038	15492.779340	29.064000
337.951699	15519.722115	29.069018
338.352627	15537.235985	29.074036
339.078109	15543.940115	29.079053
339.243189	15561.125767	29.084071
339.427378	15592.356702	29.089088
339.882603	15596.085893	29.094106
339.963727	15630.596240	29.099124
340.094831	15649.894710	29.104141
340.526850	15669.357828	29.109159
340.408764	15705.989448	29.114176
341.043348	15723.348294	29.119194
340.888178	15748.325252	29.124212
341.201210	15787.230936	29.129229
341.574944	15819.206390	29.134247
341.883981	15850.789133	29.139264
342.546556	15870.337332	29.144282
342.892533	15912.523879	29.149300
343.131890	15933.431260	29.154317
343.347169	15969.798785	29.159335
344.126526	15982.498880	29.164352
344.567967	16006.496668	29.169370
344.747215	16025.158790	29.174388
344.828081	16043.501488	29.179405
345.455394	16057.251186	29.184423
345.403481	16082.801034	29.189440
345.661952	16117.752770	29.194458
345.898891	16143.923239	29.199476
346.276487	16168.790759	29.204493
347.057469	16201.345862	29.209511
347.557584	16228.826821	29.214528
348.073542	16241.223900	29.219546
348.504370	16258.386873	29.224564
349.034185	16288.652651	29.229581
349.250677	16299.625628	29.234599
349.131515	16317.174245	29.239616
350.225986	16333.442781	29.244634
350.588552	16352.431183	29.249652
350.462764	16374.285199	29.254669
351.060433	16402.087612	29.259687
350.943527	16425.454836	29.264704
351.580117	16453.216233	29.269722
351.817181	16475.070331	29.274740
351.874537	16505.151355	29.279757
352.266381	16523.741097	29.284775
352.204724	16565.643623	29.289792
352.887200	16584.409227	29.294810
353.342560	16614.112634	29.299828
353.611302	16656.457279	29.304845
353.996043	16664.157520	29.309863
354.076269	16708.642263	29.314880
354.512777	16750.031110	29.319898
354.916758	16770.947038	29.324916
355.372320	16807.680209	29.329933
355.716752	16836.005907	29.334951
355.431630	16873.110611	29.339968
356.584892	16893.698020	29.344986
357.095350	16919.252408	29.350004
357.465787	16947.999557	29.355021
357.961046	16973.651109	29.360039
358.012828	17011.545273	29.365056
358.474818	17026.446882	29.370074
359.260669	17057.770349	29.375092
358.927765	17084.443098	29.380109
359.813325	17106.447816	29.385127
360.265575	17108.401539	29.390144
360.639076	17145.260928	29.395162
361.369923	17162.783507	29.400180
361.302708	17193.354483	29.405197
361.703758	17213.004235	29.410215
362.031656	17240.283645	29.415232
362.602890	17242.584972	29.420250
362.782827	17263.738712	29.425268
363.287834	17299.493903	29.430285
363.824892	17308.986598	29.435303
363.477075	17344.862282	29.440320
363.866206	17369.518511	29.445338
364.480548	17388.382982	29.450356
364.736590	17427.703892	29.455373
364.836060	17457.694586	29.460391
364.768720	17487.180143	29.465408
365.520282	17525.907170	29.470426
365.989651	17555.146567	29.475444
366.153051	17583.842339	29.480461
366.626602	17608.023157	29.485479
367.651329	17615.783623	29.490496
368.340469	17643.984416	29.495514
369.014708	17649.533082	29.500532
369.214706	17656.231904	29.505549
369.677444	17678.332460	29.510567
369.606605	17691.773296	29.515584
369.796204	17689.699163	29.520602
370.211996	17717.945240	29.525620
370.332146	17728.397604	29.530637
371.058616	17742.105546	29.535655
371.280124	17769.735988	29.540672
371.209897	17789.257799	29.545690
371.694837	17804.168934	29.550708
371.497936	17832.443916	29.555725
372.032718	17859.444286	29.560743
372.174172	17905.154742	29.565760
372.343149	17938.154860	29.570778
372.425368	17979.956824	29.575796
372.633015	18020.946907	29.580813
373.087850	18063.319594	29.585831
373.594536	18109.961732	29.590848
373.727062	18142.761791	29.595866
374.904831	18181.531866	29.600884
375.004611	18231.133972	29.605901
375.620346	18253.050823	29.610919
376.087684	18292.742409	29.615936
376.262234	18321.445501	29.620954
376.956975	18354.917591	29.625972
376.989667	18394.670188	29.630989
377.560807	18426.186205	29.636007
377.969398	18466.332419	29.641024
378.564833	18501.821499	29.646042
378.833367	18532.765081	29.651060
378.753796	18568.031640	29.656077
379.118474	18604.310945	29.661095
379.649061	18642.805980	29.666112
380.290666	18686.402559	29.671130
380.992529	18715.801066	29.676148
380.935318	18751.913945	29.681165
381.601572	18791.624308	29.686183
382.118388	18807.669175	29.691200
382.651159	18832.037466	29.696218
383.581524	18848.482220	29.701236
383.281416	18890.702733	29.706253
383.695397	18914.102421	29.711271
384.406907	18948.023768	29.716288
384.531855	18976.709392	29.721306
385.385614	18998.688798	29.726324
385.230561	19025.341593	29.731341
385.690079	19050.800513	29.736359
386.188376	19077.720628	29.741376
386.365259	19115.334123	29.746394
387.080056	19137.601494	29.751412
386.808002	19170.760467	29.756429
387.332046	19206.146202	29.761447
387.742067	19240.978635	29.766464
388.440095	19281.974375	29.771482
388.749437	19305.595251	29.776500
389.102232	19347.489955	29.781517
389.588512	19365.233413	29.786535
390.063819	19390.048669	29.791552
390.360141	19413.329779	29.796570
391.032824	19438.900683	29.801588
391.738484	19477.911006	29.806605
391.981961	19488.870616	29.811623
392.205122	19507.352870	29.816640
392.326731	19560.543160	29.821658
392.505839	19572.493964	29.826676
392.902171	19602.600290	29.831693
393.729462	19628.748124	29.836711
394.661534	19644.298007	29.841728
394.579324	19663.481927	29.846746
395.131257	19671.625725	29.851764
395.056890	19701.548307	29.856781
395.443170	19722.998993	29.861799
395.807892	19741.111316	29.866816
395.751723	19782.013762	29.871834
396.331439	19802.551390	29.876852
396.518405	19837.013634	29.881869
396.994160	19863.412230	29.886887
397.871891	19891.547873	29.891904
398.150969	19921.224871	29.896922
398.693744	19941.352603	29.901940
398.927042	19976.989790	29.906957
399.323911	20000.253537	29.911975
399.602091	20021.736653	29.916992
399.960628	20052.102264	29.922010
400.451722	20086.819034	29.927028
400.616488	20125.294389	29.932045
400.932398	20157.800142	29.937063
401.516255	20185.794081	29.942080
401.595099	20229.872329	29.947098
401.946144	20267.454928	29.952116
402.375208	20308.224906	29.957133
403.004577	20338.005579	29.962151
404.035892	20356.211819	29.967168
404.500316	20392.801726	29.972186
405.019381	20424.989102	29.977204
405.078295	20454.340833	29.982221
405.276098	20481.322321	29.987239
405.592543	20509.846531	29.992256
406.026582	20552.016184	29.997274
406.453792	20575.857440	30.002292
406.819272	20617.713832	30.007309
407.209613	20644.846649	30.012327
407.821165	20675.841604	30.017344
408.016197	20722.958753	30.022362
408.604736	20749.953377	30.027380
409.037707	20782.283360	30.032397
409.270130	20812.579752	30.037415
410.036506	20851.811859	30.042432
410.071995	20888.300292	30.047450
410.800544	20918.254798	30.052468
410.933284	20945.686052	30.057485
411.258182	20988.823893	30.062503
411.869986	21021.053853	30.067520
411.886930	21060.788613	30.072538
412.525488	21091.999014	30.077556
412.690230	21136.905747	30.082573
412.652765	21177.822704	30.087591
413.171898	21219.508602	30.092608
413.666484	21265.568815	30.097626
414.402335	21307.747273	30.102644
414.666668	21370.326959	30.107661
414.908401	21390.674862	30.112679
415.780799	21425.768132	30.117696
415.818886	21482.222874	30.122714
416.677365	21512.921613	30.127732
416.865148	21551.602974	30.132749
417.569448	21596.997253	30.137767
418.443633	21626.537984	30.142784
419.117157	21651.653368	30.147802
419.614860	21674.538604	30.152820
420.191638	21695.200449	30.157837
420.195318	21726.993036	30.162855
420.748505	21743.569194	30.167872
421.098814	21773.412714	30.172890
421.509191	21799.240260	30.177908
421.707110	21832.134526	30.182925
421.900680	21840.070570	30.187943
422.642542	21868.738084	30.192960
423.359795	21897.414443	30.197978
423.536594	21923.115222	30.202996
424.002238	21942.971171	30.208013
424.175305	21972.733962	30.213031
424.258542	21985.641985	30.218048
424.702175	22015.587188	30.223066
425.180305	22053.496505	30.228084
425.217816	22100.632508	30.233101
425.543321	22134.294596	30.238119
426.285470	22165.740570	30.243136
426.323866	22207.713298	30.248154
426.652427	22241.846507	30.253172
426.953847	22290.016282	30.258189
427.551648	22332.086108	30.263207
428.124638	22365.862288	30.268224
428.339293	22428.543989	30.273242
428.712341	22459.652593	30.278260
429.303324	22500.590358	30.283277
429.513332	22544.501660	30.288295
430.171160	22591.878703	30.293312
430.335113	22644.067453	30.298330
430.889097	22684.986552	30.303348
431.137344	22736.612983	30.308365
431.659181	22784.813982	30.313383
432.993769	22815.456958	30.318400
433.626061	22845.457616	30.323418
434.096167	22874.532800	30.328436
434.768763	22899.563489	30.333453
434.731221	22929.441594	30.338471
435.655023	22971.908526	30.343488
435.746402	23008.821188	30.348506
436.150881	23035.678039	30.353524
436.676513	23079.429804	30.358541
436.998605	23118.619198	30.363559
437.625067	23146.961081	30.368576
437.679691	23189.529567	30.373594
438.157283	23225.128568	30.378612
438.991128	23245.212198	30.383629
439.480842	23285.397582	30.388647
440.442277	23312.000469	30.393664
440.372302	23333.650980	30.398682
440.713693	23366.557652	30.403700
441.039724	23397.242152	30.408717
441.515915	23428.923629	30.413735
442.089293	23460.278494	30.418752
441.839316	23493.637865	30.423770
442.379639	23540.019982	30.428788
442.909212	23585.163098	30.433805
443.122919	23628.920509	30.438823
443.692992	23656.049000	30.443840
444.094760	23717.321756	30.448858
444.976559	23738.418221	30.453876
445.149309	23797.065937	30.458893
445.414490	23835.503235	30.463911
445.979491	23863.954235	30.468928
446.597880	23898.526990	30.473946
447.494360	23932.459431	30.478964
448.234700	23960.112160	30.483981
448.585038	24001.162695	30.488999
448.889040	24021.903996	30.494016
449.152682	24046.428413	30.499034
449.641758	24080.936177	30.504052
450.100680	24109.501299	30.509069
450.382936	24153.633480	30.514087
450.759966	24167.636248	30.519104
450.949987	24222.119812	30.524122
451.407600	24252.035140	30.529140
451.999502	24283.426316	30.534157
452.315996	24326.686042	30.539175
452.303991	24355.477589	30.544192
452.841379	24406.362819	30.549210
453.296350	24435.509415	30.554228
454.217498	24477.703050	30.559245
454.073290	24524.808018	30.564263
454.781699	24552.760282	30.569280
455.406780	24587.126771	30.574298
456.003104	24617.578034	30.579316
456.315472	24658.496091	30.584333
456.548681	24701.420468	30.589351
457.404809	24736.018736	30.594368
458.531469	24768.713267	30.599386
458.992129	24793.409634	30.604404
460.332002	24805.235498	30.609421
461.161356	24804.570193	30.614439
461.946368	24808.940837	30.619456
461.882040	24832.224381	30.624474
462.557657	24847.119780	30.629492
462.790662	24844.149832	30.634509
462.789016	24869.040940	30.639527
462.880969	24883.758407	30.644544
463.057446	24915.757088	30.649562
463.450222	24948.659920	30.654580
463.762460	24967.166580	30.659597
464.184506	24997.478588	30.664615
464.452168	25028.383830	30.669632
464.854098	25085.671976	30.674650
464.992089	25131.043155	30.679668
465.423165	25154.054502	30.684685
465.513592	25207.423884	30.689703
466.211164	25251.234854	30.694720
466.358528	25302.169844	30.699738
467.001007	25359.334022	30.704756
467.399594	25400.660658	30.709773
467.952458	25470.573648	30.714791
468.383756	25510.792876	30.719808
469.082010	25559.010469	30.724826
469.384303	25599.934029	30.729844
469.859907	25644.432374	30.734861
470.421398	25695.867831	30.739879
471.313005	25738.026899	30.744896
471.182321	25792.037025	30.749914
471.993805	25831.919819	30.754932
472.486845	25871.051056	30.759949
472.671673	25920.379505	30.764967
473.542740	25968.497169	30.769984
473.890968	26012.834584	30.775002
474.665876	26045.677989	30.780020
475.272676	26094.158209	30.785037
475.813513	26147.591747	30.790055
476.272856	26177.229470	30.795072
476.671279	26219.480654	30.800090
477.061324	26254.980615	30.805108
478.271978	26293.234170	30.810125
478.784359	26330.187000	30.815143
479.203009	26356.144715	30.820160
479.551905	26389.607949	30.825178
479.524322	26422.877959	30.830196
480.287328	26459.133631	30.835213
480.712143	26494.246707	30.840231
480.845748	26533.855165	30.845248
481.228371	26580.298428	30.850266
481.424213	26623.795229	30.855284
481.759845	26670.032020	30.860301
482.026808	26728.502354	30.865319
482.570218	26780.306777	30.870336
483.438037	26802.188430	30.875354
483.953597	26848.058491	30.880372
484.703925	26886.342100	30.885389
485.068903	26935.306221	30.890407
485.530915	26968.594194	30.895424
485.975839	27000.039885	30.900442
486.545917	27042.700015	30.905460
487.372359	27071.518501	30.910477
487.444159	27112.967909	30.915495
487.878519	27156.921865	30.920512
488.476101	27200.000501	30.925530
488.492826	27255.082221	30.930548
489.254445	27293.506812	30.935565
489.377380	27347.382155	30.940583
490.181556	27386.049105	30.945600
490.747618	27424.298112	30.950618
490.834735	27478.886326	30.955636
491.487876	27535.677500	30.960653
491.668748	27579.560853	30.965671
492.029929	27631.435793	30.970688
492.793758	27698.738113	30.975706
493.093659	27750.692927	30.980724
493.541603	27792.898796	30.985741
494.364983	27856.381525	30.990759
494.927892	27910.589703	30.995776
495.607021	27955.129818	31.000794
495.980907	28013.911749	31.005812
496.820125	28056.287053	31.010829
497.189725	28107.859219	31.015847
497.878151	28148.531080	31.020864
498.546035	28189.405155	31.025882
498.710026	28237.201212	31.030900
499.236884	28288.987675	31.035917
500.143134	28330.573452	31.040935
500.443859	28377.476703	31.045952
501.298600	28423.468428	31.050970
501.115302	28469.492941	31.055988
501.591947	28505.551035	31.061005
502.335756	28559.261362	31.066023
502.764223	28608.702374	31.071040
503.526246	28665.431965	31.076058
503.881069	28711.361927	31.081076
504.649632	28769.349403	31.086093
505.471550	28800.385965	31.091111
505.565549	28836.593124	31.096128
506.188770	28879.192240	31.101146
506.444674	28923.243262	31.106164
507.472920	28960.829446	31.111181
508.086524	29000.474690	31.116199
508.472229	29049.368832	31.121216
508.966750	29085.478809	31.126234
509.169508	29139.598911	31.131252
509.734094	29173.495640	31.136269
510.385964	29217.349515	31.141287
510.922354	29268.146808	31.146304
511.327191	29299.224767	31.151322
512.264707	29349.340904	31.156340
512.681598	29386.710384	31.161357
513.677475	29418.561594	31.166375
514.258552	29448.219541	31.171392
514.485596	29480.860319	31.176410
514.953481	29520.051324	31.181428
515.393329	29549.114471	31.186445
515.664199	29587.095257	31.191463
515.638598	29635.535322	31.196480
516.453726	29666.741756	31.201498
516.539859	29720.939716	31.206516
516.770759	29771.656446	31.211533
517.396626	29811.269972	31.216551
517.748043	29857.948028	31.221568
518.280373	29906.646858	31.226586
518.733717	29971.075461	31.231604
518.725807	30015.668110	31.236621
519.413484	30059.852595	31.241639
520.019495	30112.669324	31.246656
520.586191	30170.530782	31.251674
520.476556	30225.447217	31.256692
521.275752	30288.485420	31.261709
522.248130	30341.993157	31.266727
522.992125	30393.980334	31.271744
523.831484	30439.869534	31.276762
524.219561	30482.681781	31.281780
524.738118	30530.280461	31.286797
525.057625	30592.490419	31.291815
526.028914	30636.522259	31.296832
526.941128	30664.843587	31.301850
527.624749	30717.778678	31.306868
527.806701	30751.807936	31.311885
528.467944	30803.579701	31.316903
528.421950	30866.974125	31.321920
529.255647	30901.079005	31.326938
529.799338	30961.006997	31.331956
530.384312	30992.187574	31.336973
530.823702	31033.172340	31.341991
531.117824	31090.176421	31.347008
531.880514	31137.818460	31.352026
532.133045	31201.082758	31.357044
532.850478	31239.813655	31.362061
533.170209	31296.290463	31.367079
533.260747	31358.499949	31.372096
533.876327	31419.543945	31.377114
534.338411	31475.906325	31.382132
534.946160	31536.384131	31.387149
535.607543	31609.356435	31.392167
535.740246	31668.272574	31.397184
536.555877	31725.347175	31.402202
536.772193	31797.573475	31.407220
537.456202	31861.469296	31.412237
538.362241	31914.554260	31.417255
538.523148	31986.232047	31.422272
539.037475	32037.444888	31.427290
539.649317	32116.305335	31.432308
540.336765	32172.459199	31.437325
541.439239	32239.830426	31.442343
542.122087	32288.296481	31.447360
542.907867	32315.707463	31.452378
543.828734	32378.903474	31.457396
544.481271	32421.967048	31.462413
545.320561	32457.613737	31.467431
545.339415	32514.601648	31.472448
546.044882	32545.405403	31.477466
546.167061	32592.220109	31.482484
547.071439	32641.202699	31.487501
547.608081	32683.206991	31.492519
547.516868	32716.568953	31.497536
548.489829	32780.925218	31.502554
548.625300	32825.463462	31.507572
548.905769	32883.119270	31.512589
549.860947	32922.130134	31.517607
551.162861	32951.170137	31.522624
552.555359	32989.682967	31.527642
553.295781	33004.888671	31.532660
553.918155	33043.961085	31.537677
554.434856	33078.898750	31.542695
554.905900	33093.716757	31.547712
555.374712	33112.554921	31.552730
555.904456	33132.840764	31.557748
556.447878	33139.263374	31.562765
557.063774	33151.650053	31.567783
557.145312	33185.268340	31.572800
557.643186	33199.473041	31.577818
557.713672	33241.066594	31.582836
557.784584	33277.229953	31.587853
558.485316	33318.003345	31.592871
558.336999	33368.830971	31.597888
558.440805	33416.392390	31.602906
559.079158	33470.513871	31.607924
559.232540	33546.616667	31.612941
560.045212	33596.241812	31.617959
559.957294	33682.810249	31.622976
560.322132	33731.951246	31.627994
561.025224	33802.338356	31.633012
561.452161	33878.113409	31.638029
562.122435	33952.942998	31.643047
562.124928	34026.753562	31.648064
563.274864	34104.417003	31.653082
563.879881	34191.378336	31.658100
564.056104	34279.449059	31.663117
564.546441	34336.364960	31.668135
565.384973	34421.007452	31.673152
565.989518	34499.289665	31.678170
566.601830	34587.494993	31.683188
567.344387	34665.272350	31.688205
568.445791	34732.801574	31.693223
568.554668	34814.316258	31.698240
569.504423	34881.501896	31.703258
570.232114	34956.468227	31.708276
570.560029	35020.128191	31.713293
571.441350	35086.240386	31.718311
571.926783	35155.886220	31.723328
572.243109	35227.541984	31.728346
573.050626	35294.812630	31.733364
573.516563	35370.562352	31.738381
574.646702	35437.524645	31.743399
574.920446	35513.581258	31.748416
575.897998	35576.987596	31.753434
576.615927	35632.980149	31.758452
577.099092	35693.489587	31.763469
577.967341	35753.468583	31.768487
578.473670	35809.827988	31.773504
579.232881	35866.130026	31.778522
579.978834	35920.036070	31.783540
580.533843	35980.001292	31.788557
580.940899	36034.313942	31.793575
581.623245	36095.132664	31.798592
582.445138	36138.464469	31.803610
583.220063	36186.935442	31.808628
583.215694	36243.721388	31.813645
584.229811	36291.998506	31.818663
584.588602	36355.497181	31.823680
585.175454	36404.403750	31.828698
585.958375	36452.902526	31.833716
586.107861	36518.213078	31.838733
586.920935	36566.489428	31.843751
587.424054	36624.568712	31.848768
588.309117	36675.269791	31.853786
589.001426	36722.001194	31.858804
588.926913	36789.208541	31.863821
590.045371	36827.146954	31.868839
590.399099	36893.075252	31.873856
590.875707	36939.502008	31.878874
591.285849	36996.998228	31.883892
591.695184	37065.288074	31.888909
592.130260	37116.749560	31.893927
592.786521	37177.292224	31.898944
593.076316	37232.754545	31.903962
594.006597	37292.352888	31.908980
594.208877	37343.881876	31.913997
595.025424	37400.040398	31.919015
595.482202	37463.296413	31.924032
596.161434	37525.742685	31.929050
596.831569	37582.197375	31.934068
597.442353	37647.552609	31.939085
598.201755	37705.782418	31.944103
598.405283	37774.569726	31.949120
599.062981	37839.356128	31.954138
599.786198	37900.742306	31.959156
600.298810	37969.706546	31.964173
600.782457	38028.326955	31.969191
601.172830	38099.707366	31.974208
601.734018	38173.559504	31.979226
602.288244	38242.331700	31.984244
603.157698	38303.732969	31.989261
604.132936	38372.035292	31.994279
604.695068	38440.645972	31.999296
605.019507	38514.478636	32.004314
605.818136	38574.743668	32.009332
606.318105	38648.699386	32.014349
607.151117	38712.550973	32.019367
607.862129	38783.076284	32.024384
608.422155	38846.765118	32.029402
608.788766	38912.067406	32.034420
609.366039	38984.244219	32.039437
610.339111	39064.502326	32.044455
610.447557	39118.977745	32.049472
610.867813	39213.556406	32.054490
611.796467	39275.146882	32.059508
612.137237	39351.858822	32.064525
612.871439	39423.654796	32.069543
613.703047	39505.961438	32.074560
614.246059	39565.470263	32.079578
615.279270	39637.132475	32.084596
616.282037	39692.396197	32.089613
617.419364	39747.827248	32.094631
618.068216	39798.544548	32.099648
619.038366	39858.428842	32.104666
620.421744	39887.106874	32.109684
620.929122	39932.841817	32.114701
621.286969	39970.312746	32.119719
621.785486	40009.218799	32.124736
622.100077	40054.799658	32.129754
622.790492	40104.311492	32.134772
622.842913	40156.586583	32.139789
623.726744	40211.536940	32.144807
624.150959	40267.791249	32.149824
624.327219	40327.861863	32.154842
624.975082	40378.527282	32.159860
625.256573	40444.597219	32.164877
625.986563	40522.711276	32.169895
626.477715	40582.213047	32.174912
626.597866	40663.487121	32.179930
627.220308	40733.539037	32.184948
627.491023	40816.581859	32.189965
628.047373	40895.682632	32.194983
628.610330	40974.350200	32.200000
629.126906	41056.605385	32.205018
629.911512	41134.801419	32.210036
630.402719	41227.582664	32.215053
631.201349	41307.832106	32.220071
632.034696	41392.284033	32.225088
632.825531	41475.262876	32.230106
633.533354	41540.275146	32.235124
634.100580	41614.740010	32.240141
634.499053	41678.932604	32.245159
635.238421	41764.765477	32.250176
635.478203	41846.198648	32.255194
636.365617	41900.301158	32.260212
636.580850	41991.970144	32.265229
637.333640	42050.303334	32.270247
637.993922	42144.301903	32.275264
638.543382	42221.938448	32.280282
639.436352	42306.419452	32.285300
640.155579	42388.505069	32.290317
640.900987	42466.665890	32.295335
641.595396	42542.966588	32.300352
641.973422	42620.301648	32.305370
643.030330	42710.591381	32.310388
643.221287	42791.193891	32.315405
644.450314	42864.351716	32.320423
644.866936	42938.265923	32.325440
645.252365	43039.818527	32.330458
646.260522	43092.319796	32.335476
647.088215	43173.977426	32.340493
648.086822	43239.689562	32.345511
648.811841	43323.593655	32.350528
649.590556	43388.692289	32.355546
650.463639	43449.633529	32.360564
651.089125	43511.556662	32.365581
651.949934	43573.554792	32.370599
652.612216	43626.967110	32.375616
653.292558	43690.356133	32.380634
653.920634	43763.212658	32.385652
654.303049	43830.117852	32.390669
654.690057	43909.373175	32.395687
655.260133	43981.558198	32.400704
655.779447	44067.949565	32.405722
656.432449	44136.086660	32.410740
656.968915	44222.984217	32.415757
657.399143	44302.347735	32.420775
657.948189	44370.670188	32.425792
658.652001	44456.300418	32.430810
659.809567	44523.029572	32.435828
661.118799	44598.214252	32.440845
662.211099	44651.678474	32.445863
663.119983	44719.920682	32.450880
663.481265	44782.340013	32.455898
664.458757	44841.588913	32.460916
664.664592	44895.389671	32.465933
665.580731	44961.598274	32.470951
666.200045	45015.255317	32.475968
666.402945	45092.017074	32.480986
667.192644	45152.737715	32.486004
667.536961	45234.973616	32.491021
667.958665	45296.661656	32.496039
668.813633	45369.730110	32.501056
669.190578	45465.408864	32.506074
669.729410	45518.793322	32.511092
670.310286	45595.289491	32.516109
670.445473	45687.046759	32.521127
671.559462	45753.070778	32.526144
671.846857	45853.426670	32.531162
672.657042	45923.208305	32.536180
673.547574	46016.957941	32.541197
673.953372	46097.027758	32.546215
674.988697	46178.547442	32.551232
675.090223	46267.057719	32.556250
675.905373	46352.002533	32.561268
676.685001	46441.623609	32.566285
677.442390	46512.761271	32.571303
678.211666	46604.036234	32.576320
678.932644	46675.455234	32.581338
679.346118	46745.194925	32.586356
679.853122	46818.771711	32.591373
680.707246	46901.997991	32.596391
681.869966	46968.352948	32.601408
682.318170	47050.118624	32.606426
683.005783	47125.678204	32.611444
683.514510	47195.545924	32.616461
683.798273	47293.946022	32.621479
684.341215	47373.739687	32.626496
685.067776	47478.398812	32.631514
686.035912	47557.459912	32.636532
686.500573	47649.263900	32.641549
687.149012	47725.476529	32.646567
688.456780	47808.821357	32.651584
689.248579	47888.879244	32.656602
689.993274	47960.194983	32.661620
691.467066	48033.661050	32.666637
692.118221	48100.363413	32.671655
693.336022	48171.652343	32.676672
694.024079	48231.294469	32.681690
694.543879	48285.081486	32.686708
695.259376	48353.270936	32.691725
695.855726	48418.764534	32.696743
696.319631	48486.225490	32.701760
697.137418	48559.530357	32.706778
698.006748	48636.625965	32.711796
698.984321	48694.011196	32.716813
700.177153	48754.212665	32.721831
701.073852	48798.165096	32.726848
701.572392	48867.601715	32.731866
702.203223	48924.940695	32.736884
702.564765	48979.614781	32.741901
702.984692	49055.163107	32.746919
703.720184	49117.699213	32.751936
703.862362	49195.255076	32.756954
703.831754	49279.705321	32.761972
704.820075	49355.337819	32.766989
705.309992	49451.106518	32.772007
705.953745	49526.082877	32.777024
706.340671	49628.504559	32.782042
707.004541	49710.517676	32.787060
707.827465	49801.666540	32.792077
708.168145	49900.740251	32.797095
708.772879	49993.034561	32.802112
709.529750	50109.097726	32.807130
710.232753	50217.079246	32.812148
711.358415	50304.643357	32.817165
711.466294	50401.620010	32.822183
712.565829	50493.029675	32.827200
713.598735	50599.206055	32.832218
714.217679	50685.649142	32.837236
714.937696	50783.688872	32.842253
715.342571	50894.869075	32.847271
716.226342	50979.456894	32.852288
716.812794	51074.601897	32.857306
717.296173	51169.805449	32.862324
718.900524	51261.830242	32.867341
719.616597	51355.824542	32.872359
720.503277	51442.267875	32.877376
721.189520	51531.505129	32.882394
722.424411	51615.564003	32.887412
723.487203	51692.845277	32.892429
723.712105	51776.477861	32.897447
724.578286	51861.931557	32.902464
725.144407	51940.679243	32.907482
725.578265	52023.956229	32.912500
726.143952	52088.042974	32.917517
727.399993	52160.550172	32.922535
728.151898	52239.906413	32.927552
728.582922	52306.258659	32.932570
729.936198	52380.892102	32.937588
731.265526	52427.014504	32.942605
731.897162	52489.550325	32.947623
732.583524	52550.750717	32.952640
733.169020	52628.765221	32.957658
733.401235	52697.672178	32.962676
734.112905	52760.448344	32.967693
734.379379	52850.885468	32.972711
734.945482	52920.938350	32.977728
735.507804	53007.739162	32.982746
736.078185	53095.423450	32.987764
736.882612	53183.391668	32.992781
737.801418	53278.947483	32.997799
738.403576	53363.039477	33.002816
739.973369	53433.200107	33.007834
740.644243	53506.428086	33.012852
741.370279	53598.258439	33.017869
741.628686	53682.421215	33.022887
742.677326	53769.214608	33.027904
743.330785	53844.897929	33.032922
743.783326	53953.276520	33.037940
744.651038	54017.585099	33.042957
744.964635	54121.754787	33.047975
745.835773	54205.471165	33.052992
746.323697	54307.509277	33.058010
747.055009	54417.253250	33.063028
747.892803	54505.367233	33.068045
748.359763	54622.257157	33.073063
749.361069	54700.211295	33.078080
749.927070	54812.657217	33.083098
750.515403	54921.126148	33.088116
751.607044	55020.136783	33.093133
752.085074	55131.929363	33.098151
753.378954	55214.165027	33.103168
754.141028	55316.472702	33.108186
754.874267	55417.130345	33.113204
755.839178	55507.982510	33.118221
756.537546	55605.923792	33.123239
757.953347	55678.164991	33.128256
759.199155	55769.603793	33.133274
759.762490	55862.836357	33.138292
760.628788	55939.326623	33.143309
761.018703	56030.750021	33.148327
761.590340	56112.691712	33.153344
762.321460	56204.160661	33.158362
762.928995	56299.422481	33.163380
763.633625	56396.229359	33.168397
763.899455	56499.231687	33.173415
764.429702	56582.907083	33.178432
765.363986	56692.794520	33.183450
765.918159	56810.643440	33.188468
766.749604	56907.741487	33.193485
767.273056	57027.277495	33.198503
767.966307	57144.233473	33.203520
768.548215	57244.028183	33.208538
769.509647	57350.824981	33.213556
770.354303	57465.622145	33.218573
771.136983	57583.949741	33.223591
772.187727	57691.182252	33.228608
772.915334	57793.805428	33.233626
773.361301	57912.291680	33.238644
774.512675	58013.190476	33.243661
775.179514	58126.624351	33.248679
775.842519	58226.069378	33.253696
777.012392	58332.982366	33.258714
777.697171	58422.605103	33.263732
779.347979	58487.197053	33.268749
781.189216	58555.043667	33.273767
782.173190	58611.998998	33.278784
782.797870	58697.538147	33.283802
783.286044	58765.539402	33.288820
784.116339	58826.040463	33.293837
784.557781	58898.738679	33.298855
785.051616	58980.528116	33.303872
785.749434	59067.377477	33.308890
786.075681	59155.084796	33.313908
786.936250	59232.820952	33.318925
787.552603	59331.166996	33.323943
788.435302	59417.387015	33.328960
789.687941	59512.589291	33.333978
790.491081	59588.415231	33.338996
791.876177	59658.464231	33.344013
792.578956	59752.538804	33.349031
793.263315	59835.399846	33.354048
793.770599	59924.963829	33.359066
794.481099	60010.867263	33.364084
795.325329	60088.836938	33.369101
795.776063	60188.073983	33.374119
796.282645	60279.674557	33.379136
797.039850	60372.289538	33.384154
797.164445	60498.061150	33.389172
797.803436	60588.206700	33.394189
798.435809	60700.681282	33.399207
799.309154	60824.327937	33.404224
799.715663	60945.075814	33.409242
800.616351	61067.234289	33.414260
801.413944	61181.422216	33.419277
802.006333	61304.991806	33.424295
802.834782	61422.430747	33.429312
804.191145	61542.254306	33.434330
804.702977	61674.339819	33.439348
805.743582	61786.272701	33.444365
806.974913	61899.445044	33.449383
807.025995	62025.295155	33.454400
808.090639	62151.301006	33.459418
808.652592	62277.586571	33.464436
809.869719	62391.554026	33.469453
810.305550	62528.138684	33.474471
811.153074	62644.380684	33.479488
812.070396	62762.526888	33.484506
812.901188	62900.142239	33.489524
813.615484	63019.410563	33.494541
814.373178	63135.221441	33.499559
815.457361	63264.448065	33.504576
816.489204	63380.828154	33.509594
817.023948	63509.736218	33.514612
818.522129	63628.120182	33.519629
820.248731	63732.675442	33.524647
821.098472	63830.789873	33.529664
822.261628	63926.210963	33.534682
823.042626	64036.492467	33.539700
823.729834	64140.172192	33.544717
824.340334	64235.806073	33.549735
824.702981	64346.455397	33.554752
825.523986	64452.687187	33.559770
825.931626	64564.177249	33.564788
826.858475	64687.358101	33.569805
827.224436	64789.482300	33.574823
827.936285	64915.601347	33.579840
828.731977	65030.342064	33.584858
829.653514	65155.530363	33.589876
830.494804	65273.400163	33.594893
831.311562	65378.449051	33.599911
831.952666	65497.731197	33.604928
833.150377	65611.214051	33.609946
834.003251	65721.309380	33.614964
834.746567	65813.540443	33.619981
835.833311	65938.794699	33.624999
836.582251	66031.145907	33.630016
837.808015	66120.390849	33.635034
838.627954	66249.117226	33.640052
839.618089	66347.941085	33.645069
839.903672	66450.333281	33.650087
840.992508	66565.286954	33.655104
841.701841	66679.026973	33.660122
842.788845	66779.044303	33.665140
843.478360	66899.021879	33.670157
845.345047	66982.664885	33.675175
846.427886	67070.818578	33.680192
847.769244	67158.538012	33.685210
848.681512	67256.253779	33.690228
849.357029	67336.453580	33.695245
849.894064	67432.209168	33.700263
850.597525	67526.154964	33.705280
851.153898	67629.203631	33.710298
851.668076	67748.898949	33.715316
852.665355	67836.709656	33.720333
853.285036	67951.211070	33.725351
853.756665	68061.893796	33.730368
854.597197	68172.497226	33.735386
855.411746	68299.947447	33.740404
855.706291	68407.506534	33.745421
856.443209	68550.498117	33.750439
857.100451	68681.289414	33.755456
857.983927	68804.343733	33.760474
858.189493	68940.800042	33.765492
859.110403	69087.672032	33.770509
859.933402	69227.284218	33.775527
860.880410	69380.805023	33.780544
862.201263	69513.369647	33.785562
863.478618	69641.238386	33.790580
864.328706	69769.083611	33.795597
865.183091	69908.322086	33.800615
866.089644	70048.254667	33.805632
867.160334	70171.501002	33.810650
867.833055	70303.203910	33.815668
868.368431	70434.335981	33.820685
869.906056	70559.081816	33.825703
871.024623	70682.531863	33.830720
872.661269	70803.968632	33.835738
873.380222	70925.740983	33.840756
874.192993	71033.518692	33.845773
875.340317	71153.071840	33.850791
875.589616	71272.849811	33.855808
876.791412	71378.118054	33.860826
877.451326	71510.918096	33.865844
877.821526	71637.829465	33.870861
878.761558	71754.960548	33.875879
879.425844	71891.537105	33.880896
880.831918	72006.126598	33.885914
881.883151	72145.593794	33.890932
882.828847	72268.563055	33.895949
884.044802	72395.611163	33.900967
884.967535	72485.799375	33.905984
887.121407	72583.151350	33.911002
888.075258	72689.181517	33.916020
888.642277	72787.030393	33.921037
889.640006	72880.926027	33.926055
889.952847	72973.986641	33.931072
890.771864	73071.320944	33.936090
891.366122	73178.253914	33.941108
892.084539	73281.644712	33.946125
892.656579	73380.380746	33.951143
893.118473	73504.739607	33.956160
893.790884	73600.823140	33.961178
894.721946	73724.827562	33.966196
895.302845	73846.753105	33.971213
896.603565	73964.260352	33.976231
896.886228	74082.454879	33.981248
897.680885	74214.041514	33.986266
898.642481	74346.954683	33.991284
898.880693	74483.605361	33.996301
899.890078	74624.189519	34.001319
900.528170	74767.846093	34.006336
901.593256	74912.748505	34.011354
902.535752	75053.226323	34.016372
902.862085	75203.242310	34.021389
904.327020	75349.163022	34.026407
904.985651	75507.758665	34.031424
906.481214	75638.789169	34.036442
907.911455	75764.291207	34.041460
909.413707	75895.777494	34.046477
910.656837	76009.630891	34.051495
912.002589	76122.241014	34.056512
912.906751	76233.318235	34.061530
914.116352	76347.830339	34.066548
915.110083	76474.572215	34.071565
916.593370	76552.269888	34.076583
917.480851	76676.197110	34.081600
918.286695	76774.543104	34.086618
918.894376	76882.889769	34.091636
919.476104	77009.146193	34.096653
920.516769	77112.780243	34.101671
921.177814	77233.629947	34.106688
921.636522	77348.100475	34.111706
922.510580	77481.863030	34.116724
923.088656	77609.040577	34.121741
923.777568	77740.431853	34.126759
924.558794	77892.275886	34.131776
925.079522	78029.154994	34.136794
926.199914	78175.726935	34.141812
927.017569	78331.856272	34.146829
928.073394	78468.706669	34.151847
928.946849	78617.030052	34.156864
930.299689	78747.602944	34.161882
930.490868	78898.071206	34.166900
931.442508	79045.600220	34.171917
932.701113	79202.459838	34.176935
933.281344	79345.460045	34.181952
933.845851	79507.971020	34.186970
935.262722	79658.444449	34.191988
936.279701	79812.204544	34.197005
937.104334	79972.076205	34.202023
938.175898	80117.802399	34.207040
938.875368	80261.604761	34.212058
940.709617	80406.542729	34.217076
941.659128	80553.405206	34.222093
943.066689	80689.641835	34.227111
943.407450	80831.229836	34.232128
944.140568	80981.957879	34.237146
945.476027	81123.408790	34.242164
946.033418	81264.331167	34.247181
947.128190	81416.235936	34.252199
947.867049	81565.809302	34.257216
948.864657	81708.129373	34.262234
950.162522	81852.254276	34.267252
950.724427	82000.752688	34.272269
951.666824	82146.665157	34.277287
952.436732	82295.751112	34.282304
953.365968	82431.406660	34.287322
954.658623	82549.593400	34.292340
955.216041	82701.722032	34.297357
956.411500	82828.112383	34.302375
958.664048	82945.181112	34.307392
959.985595	83058.348993	34.312410
961.101219	83177.219835	34.317428
961.897672	83294.157513	34.322445
962.964909	83394.115301	34.327463
963.645144	83523.922267	34.332480
964.299585	83646.610621	34.337498
964.963587	83781.837190	34.342516
965.817469	83902.444199	34.347533
966.587922	84031.796293	34.352551
967.564874	84172.831912	34.357568
968.357902	84296.772517	34.362586
969.725555	84437.099937	34.367604
970.407846	84579.989813	34.372621
971.804991	84711.475605	34.377639
972.747454	84848.541533	34.382656
973.369311	84979.732962	34.387674
974.240583	85118.995012	34.392692
975.224677	85258.561949	34.397709
976.036767	85406.446435	34.402727
977.183609	85555.908966	34.407744
978.303307	85703.820494	34.412762
979.195290	85837.009499	34.417780
979.676570	86000.403113	34.422797
980.652130	86149.119517	34.427815
981.437722	86314.015250	34.432832
982.189595	86467.009846	34.437850
983.367188	86620.960182	34.442868
984.278862	86793.760264	34.447885
985.321855	86953.081615	34.452903
986.247411	87110.942827	34.457920
986.756908	87271.278233	34.462938
988.143391	87438.341622	34.467956
989.093685	87607.680207	34.472973
990.036909	87776.065716	34.477991
991.037285	87940.538844	34.483008
991.665281	88109.567263	34.488026
993.403356	88277.274635	34.493044
994.024724	88453.324077	34.498061
994.850403	88625.240673	34.503079
996.176642	88788.394044	34.508096
997.302249	88962.756767	34.513114
998.487574	89127.087427	34.518132
999.301013	89290.404867	34.523149
1000.387830	89454.494619	34.528167
1001.525933	89637.959997	34.533184
1002.193558	89801.070894	34.538202
1003.242660	89965.569086	34.543220
1004.070384	90141.666644	34.548237
1005.085277	90314.519839	34.553255
1006.078330	90486.732408	34.558272
1007.347425	90662.900178	34.563290
1008.509604	90817.488026	34.568308
1009.511621	91004.460714	34.573325
1010.764518	91146.524353	34.578343
1012.463009	91305.140342	34.583360
1013.634494	91438.492103	34.588378
1015.045017	91599.265000	34.593396
1016.097903	91740.099463	34.598413
1017.039931	91890.420780	34.603431
1018.086905	92034.156487	34.608448
1018.882042	92176.757480	34.613466
1020.499206	92326.628312	34.618484
1020.464171	92469.361765	34.623501
1021.683127	92597.737656	34.628519
1023.598573	92720.505749	34.633536
1025.022880	92821.830821	34.638554
1026.732515	92955.007223	34.643572
1026.964480	93072.415923	34.648589
1028.245167	93177.873726	34.653607
1028.789916	93301.997639	34.658624
1029.482979	93433.964771	34.663642
1030.417246	93560.987723	34.668660
1031.045499	93706.713919	34.673677
1031.387498	93845.513459	34.678695
1032.479950	94001.911784	34.683712
1032.804832	94147.937548	34.688730
1033.705608	94300.628830	34.693748
1034.389038	94475.218583	34.698765
1035.436863	94661.041107	34.703783
1036.402013	94825.947157	34.708800
1036.822853	95007.343929	34.713818
1037.898761	95178.956012	34.718836
1038.963041	95371.718406	34.723853
1039.967408	95565.055545	34.728871
1041.173251	95746.815572	34.733888
1041.893630	95938.582130	34.738906
1042.912001	96133.927960	34.743924
1043.629567	96328.850258	34.748941
1045.173575	96532.550156	34.753959
1046.030448	96729.807344	34.758976
1047.088748	96937.483684	34.763994
1047.952702	97124.190731	34.769012
1049.136937	97341.192819	34.774029
1050.420591	97527.548759	34.779047
1051.923304	97710.584558	34.784064
1053.349208	97918.360341	34.789082
1054.793418	98104.497859	34.794100
1056.065724	98281.568439	34.799117
1057.452253	98456.120915	34.804135
1058.609640	98635.055116	34.809152
1059.291700	98827.432713	34.814170
1060.666150	98996.496093	34.819188
1061.370395	99165.354728	34.824205
1062.556142	99352.240560	34.829223
1063.718233	99540.429473	34.834240
1064.365814	99725.096227	34.839258
1065.393774	99907.441458	34.844276
1066.252465	100094.937568	34.849293
1067.024033	100295.421364	34.854311
1068.214969	100484.916713	34.859328
1069.007414	100685.621733	34.864346
1070.180630	100887.113835	34.869364
1071.106743	101087.850617	34.874381
1072.289960	101293.415155	34.879399
1073.348317	101467.232268	34.884416
1074.577158	101688.170811	34.889434
1075.835584	101871.979944	34.894452
1077.071643	102069.216428	34.899469
1078.317297	102260.571034	34.904487
1079.612798	102448.094683	34.909504
1080.681042	102635.492604	34.914522
1081.795095	102823.093268	34.919540
1083.145542	103011.890925	34.924557
1084.999170	103168.550175	34.929575
1086.764398	103331.980794	34.934592
1087.768186	103500.476832	34.939610
1088.819648	103668.434239	34.944628
1090.015388	103829.644626	34.949645
1090.999197	103982.526745	34.954663
1092.216586	104138.163530	34.959680
1092.570881	104303.232540	34.964698
1093.913587	104460.547506	34.969716
1094.880248	104611.929178	34.974733
1095.875202	104760.615981	34.979751
1097.166152	104919.588578	34.984768
1097.396877	105089.330655	34.989786
1098.444295	105241.760106	34.994804
1099.606286	105417.904277	34.999821
1100.432598	105596.536597	35.004839
1101.426421	105763.478577	35.009856
1101.984636	105960.774298	35.014874
1103.096510	106133.208195	35.019892
1103.796559	106328.279627	35.024909
1104.753801	106540.762088	35.029927
1105.572535	106722.924124	35.034944
1106.412765	106945.814346	35.039962
1107.544522	107136.983013	35.044980
1108.609088	107354.279689	35.049997
1109.769146	107567.724812	35.055015
1111.059189	107776.590666	35.060032
1111.728112	107990.563552	35.065050
1112.480723	108205.765568	35.070068
1114.105867	108440.799043	35.075085
1115.074854	108641.517330	35.080103
1116.878258	108856.956443	35.085120
1117.864718	109079.080459	35.090138
1119.380447	109282.183165	35.095156
1120.470779	109494.185952	35.100173
1121.632713	109715.982287	35.105191
1122.478043	109920.416449	35.110208
1123.276081	110154.423517	35.115226
1124.442733	110370.068548	35.120244
1125.895775	110589.037361	35.125261
1126.949359	110815.825962	35.130279
1127.880427	111034.605874	35.135296
1129.404318	111271.276825	35.140314
1130.638084	111490.301779	35.145332
1132.384531	111701.744881	35.150349
1133.256443	111922.023757	35.155367
1134.449720	112130.103320	35.160384
1135.508203	112353.091031	35.165402
1136.818581	112564.954821	35.170420
1138.754817	112767.127490	35.175437
1139.546189	112981.613712	35.180455
1141.100362	113177.873275	35.185472
1142.470103	113376.698278	35.190490
1143.568032	113579.547357	35.195508
1144.432317	113788.922593	35.200525
1145.522275	114001.631918	35.205543
1146.669733	114200.220837	35.210560
1147.122133	114415.369556	35.215578
1148.278607	114636.332597	35.220596
1149.737058	114842.032499	35.225613
1151.227599	115043.953341	35.230631
1152.296062	115252.495103	35.235648
1153.166045	115470.129466	35.240666
1154.690575	115676.470726	35.245684
1155.766525	115883.153606	35.250701
1157.140775	116096.009348	35.255719
1158.353141	116311.972068	35.260736
1159.480126	116500.280571	35.265754
1160.789375	116701.863200	35.270772
1162.503191	116900.225765	35.275789
1163.501820	117095.768417	35.280807
1165.680446	117270.427950	35.285824
1167.444344	117440.697246	35.290842
1168.525553	117612.663992	35.295860
1170.289574	117785.038538	35.300877
1170.834829	117946.719075	35.305895
1172.346011	118087.753523	35.310912
1173.808050	118237.792600	35.315930
1174.626710	118388.192074	35.320948
1175.894904	118530.675220	35.325965
1176.798206	118693.251157	35.330983
1177.675681	118843.896727	35.336000
1178.145316	119009.092799	35.341018
1179.737667	119172.622039	35.346036
1180.621905	119336.902631	35.351053
1181.247979	119510.995907	35.356071
1182.598264	119689.924977	35.361088
1183.420721	119865.229717	35.366106
1184.045823	120065.631272	35.371124
1184.870106	120254.673411	35.376141
1185.736756	120455.899429	35.381159
1186.490237	120673.782856	35.386176
1187.030409	120894.820276	35.391194
1188.187710	121119.191465	35.396212
1189.273735	121358.870689	35.401229
1190.004089	121586.369786	35.406247
1191.079597	121819.110466	35.411264
1192.014623	122065.701161	35.416282
1192.926803	122326.262191	35.421300
1194.140950	122572.975807	35.426317
1195.117686	122847.026540	35.431335
1196.382745	123105.014446	35.436352
1197.707057	123368.190508	35.441370
1199.188369	123628.238227	35.446388
1200.560971	123875.291387	35.451405
1201.660451	124138.929592	35.456423
1203.214022	124401.481349	35.461440
1204.549832	124643.173667	35.466458
1205.786847	124902.791267	35.471476
1207.585077	125153.878155	35.476493
1209.190212	125407.736444	35.481511
1210.910784	125640.121807	35.486528
1212.453867	125873.400057	35.491546
1214.154504	126101.939540	35.496564
1215.618431	126323.574662	35.501581
1216.772454	126549.432223	35.506599
1217.851807	126771.222815	35.511616
1218.471546	127001.303598	35.516634
1219.608014	127228.335105	35.521652
1221.505187	127442.986865	35.526669
1222.022161	127686.435629	35.531687
1223.279572	127922.755214	35.536704
1224.415502	128165.395858	35.541722
1225.564562	128405.932282	35.546740
1227.179592	128633.896505	35.551757
1228.452776	128871.209401	35.556775
1229.694845	129114.207570	35.561792
1231.038070	129348.888889	35.566810
1232.546579	129594.686030	35.571828
1233.845278	129813.914718	35.576845
1235.175460	130041.353275	35.581863
1236.412146	130262.167081	35.586880
1237.690730	130484.699383	35.591898
1239.124456	130716.105833	35.596916
1240.303673	130931.635514	35.601933
1241.243265	131169.908294	35.606951
1242.230514	131398.287939	35.611968
1243.258102	131632.024458	35.616986
1244.420775	131864.346060	35.622004
1246.009815	132094.532806	35.627021
1247.558691	132323.295457	35.632039
1248.568234	132551.438912	35.637056
1249.847318	132781.871952	35.642074
1250.845722	133001.933007	35.647092
1252.990935	133193.119472	35.652109
1254.048007	133409.053806	35.657127
1255.491203	133614.188770	35.662144
1256.543281	133813.532969	35.667162
1257.441150	134039.271564	35.672180
1258.709455	134249.155219	35.677197
1259.385815	134466.313101	35.682215
1260.644393	134691.122017	35.687232
1262.101116	134927.600787	35.692250
1262.645971	135146.851318	35.697268
1264.298764	135379.421795	35.702285
1265.200103	135615.198576	35.707303
1266.137510	135857.208439	35.712320
1267.135148	136096.230921	35.717338
1268.786553	136335.628997	35.722356
1270.677404	136573.163704	35.727373
1271.987451	136810.491727	35.732391
1272.894762	137055.241152	35.737408
1274.300698	137299.656534	35.742426
1275.478326	137547.040062	35.747444
1276.665227	137793.523755	35.752461
1277.745714	138053.554632	35.757479
1278.693730	138319.352744	35.762496
1280.150728	138575.243099	35.767514
1281.062917	138838.959309	35.772532
1282.374111	139101.293154	35.777549
1283.193751	139369.567808	35.782567
1284.671894	139638.991133	35.787584
1286.114871	139906.127514	35.792602
1287.402509	140190.446535	35.797620
1288.881663	140456.643043	35.802637
1289.729076	140734.648953	35.807655
1291.861399	141001.819680	35.812672
1293.666819	141259.511441	35.817690
1295.107586	141515.236592	35.822708
1296.660682	141777.107470	35.827725
1297.902108	142037.066417	35.832743
1299.061046	142297.053626	35.837760
1300.631388	142554.248691	35.842778
1301.299115	142815.424047	35.847796
1302.765510	143087.235063	35.852813
1304.154348	143343.274016	35.857831
1306.778284	143568.969689	35.862848
1308.779626	143799.436004	35.867866
1309.910854	144053.316300	35.872884
1311.122619	144289.495624	35.877901
1312.448191	144534.318708	35.882919
1314.203194	144753.901173	35.887936
1315.618103	145002.973539	35.892954
1316.395250	145228.591624	35.897972
1317.534075	145461.443078	35.902989
1319.092983	145712.715876	35.908007
1320.318799	145938.302481	35.913024
1321.846108	146169.877073	35.918042
1323.266236	146412.440291	35.923060
1324.864393	146625.491284	35.928077
1325.965313	146863.316644	35.933095
1327.190336	147096.925470	35.938112
1328.273684	147335.124629	35.943130
1329.498865	147568.685771	35.948148
1330.880576	147815.246918	35.953165
1331.881603	148056.267134	35.958183
1332.654690	148302.285270	35.963200
1333.843280	148557.532531	35.968218
1334.768144	148802.768076	35.973236
1336.078784	149055.170539	35.978253
1337.445264	149316.417874	35.983271
1338.673430	149568.977003	35.988288
1339.864880	149825.259937	35.993306
1340.719279	150063.058177	35.998324
1341.915294	150320.624758	36.003341
1342.797105	150579.893765	36.008359
1343.905384	150846.698939	36.013376
1345.146114	151121.499863	36.018394
1346.000537	151410.279994	36.023412
1347.236676	151693.190429	36.028429
1349.064940	151949.382939	36.033447
1350.559875	152242.820038	36.038464
1351.913016	152524.334939	36.043482
1353.530359	152798.718190	36.048500
1355.082057	153078.669737	36.053517
1356.489653	153358.203201	36.058535
1357.662354	153654.190467	36.063552
1358.971740	153924.370890	36.068570
1360.484985	154220.521974	36.073588
1361.609542	154518.020601	36.078605
1362.980473	154810.013938	36.083623
1364.095436	155107.176227	36.088640
1365.819491	155406.181005	36.093658
1366.724562	155711.399171	36.098676
1367.865092	156010.745918	36.103693
1369.470015	156312.403061	36.108711
1370.787863	156621.150022	36.113728
1372.841983	156927.355070	36.118746
1374.236840	157212.842408	36.123764
1376.372217	157506.290054	36.128781
1377.858743	157795.445177	36.133799
1379.381317	158098.372756	36.138816
1380.633565	158387.393259	36.143834
1381.889261	158678.660628	36.148852
1383.468477	158965.728524	36.153869
1385.366711	159249.663194	36.158887
1387.139102	159522.076551	36.163904
1389.267054	159780.973338	36.168922
1390.968113	160049.558204	36.173940
1392.602814	160311.064295	36.178957
1394.175214	160569.601109	36.183975
1395.348985	160832.962682	36.188992
1396.439718	161082.676513	36.194010
1397.657313	161360.547375	36.199028
1398.939573	161627.993855	36.204045
1400.157748	161902.696666	36.209063
1400.921595	162192.433825	36.214080
1402.257409	162468.808302	36.219098
1403.324999	162756.799252	36.224116
1404.000612	163052.875000	36.229133
1405.344219	163346.267144	36.234151
1406.271993	163661.602492	36.239168
1407.253501	163982.031581	36.244186
1408.761074	164302.249411	36.249204
1409.915075	164617.326191	36.254221
1411.663550	164935.504441	36.259239
1412.403011	165258.051166	36.264256
1414.492155	165586.099717	36.269274
1415.570970	165901.490193	36.274292
1417.098604	166238.593941	36.279309
1419.118210	166539.585371	36.284327
1421.172284	166848.122579	36.289344
1422.893813	167160.840495	36.294362
1424.416655	167459.547595	36.299380
1425.573257	167771.931712	36.304397
1426.697981	168082.762638	36.309415
1428.008316	168395.481083	36.314432
1429.572427	168702.462693	36.319450
1431.168517	169001.586876	36.324468
1433.156441	169304.378892	36.329485
1434.601839	169584.854043	36.334503
1435.582723	169865.585251	36.339520
1437.417778	170151.290907	36.344538
1438.934472	170427.242274	36.349556
1440.779708	170693.256277	36.354573
1442.182191	170969.915011	36.359591
1443.710819	171257.771933	36.364608
1445.772363	171529.224210	36.369626
1447.783229	171778.073897	36.374644
1448.760653	172050.241121	36.379661
1450.581662	172304.556096	36.384679
1451.567978	172579.478611	36.389696
1453.160562	172846.523908	36.394714
1454.373482	173119.661045	36.399732
1455.594479	173408.242021	36.404749
1457.171373	173683.010140	36.409767
1458.094019	173977.976140	36.414784
1459.373325	174260.537659	36.419802
1460.087708	174550.871649	36.424820
1461.284793	174854.833239	36.429837
1462.568006	175154.137891	36.434855
1463.898266	175479.693140	36.439872
1465.686099	175789.223118	36.444890
1466.825512	176115.042595	36.449908
1468.162264	176428.420222	36.454925
1469.746082	176759.158134	36.459943
1471.008350	177085.027306	36.464960
1473.124989	177392.533489	36.469978
1474.627046	177719.319132	36.474996
1475.775478	178045.226158	36.480013
1477.082846	178374.548413	36.485031
1478.782973	178701.891659	36.490048
1479.938846	179053.072379	36.495066
1481.231623	179387.480273	36.500084
1482.223461	179730.100698	36.505101
1484.364671	180068.967439	36.510119
1485.454921	180432.390619	36.515136
1486.655132	180779.527376	36.520154
1488.225464	181136.479686	36.525172
1489.318689	181499.376894	36.530189
1490.917838	181855.948676	36.535207
1492.323988	182220.791956	36.540224
1493.925558	182586.582843	36.545242
1495.548864	182950.913084	36.550260
1497.214344	183310.809241	36.555277
1498.757759	183675.284595	36.560295
1500.013094	184051.144461	36.565312
1501.656560	184416.725330	36.570330
1503.500424	184787.048097	36.575348
1504.952736	185158.275751	36.580365
1506.844228	185520.434194	36.585383
1508.198311	185889.982209	36.590400
1510.082746	186246.536330	36.595418
1512.146088	186590.522388	36.600436
1513.766779	186947.111875	36.605453
1515.375149	187284.856088	36.610471
1516.897586	187644.690369	36.615488
1518.080916	187998.591591	36.620506
1519.829528	188347.908235	36.625524
1521.238892	188695.670924	36.630541
1522.750229	189045.069100	36.635559
1524.196306	189390.684735	36.640576
1526.590248	189738.138982	36.645594
1528.726675	190069.795763	36.650612
1529.934142	190404.375031	36.655629
1531.482937	190728.935032	36.660647
1532.685230	191062.566870	36.665664
1534.304560	191383.399465	36.670682
1535.789798	191708.698939	36.675700
1537.242795	192015.636756	36.680717
1538.896676	192322.149480	36.685735
1540.351579	192639.969327	36.690752
1541.974654	192954.221318	36.695770
1543.394913	193256.220004	36.700788
1544.421565	193590.961302	36.705805
1545.855860	193905.833327	36.710823
1547.327926	194231.542128	36.715840
1548.526944	194566.184140	36.720858
1550.412423	194902.568155	36.725876
1551.622114	195252.293737	36.730893
1553.563826	195579.607864	36.735911
1554.867462	195924.649893	36.740928
1556.323724	196268.995773	36.745946
1557.683115	196611.048955	36.750964
1558.761634	196975.303766	36.755981
1560.467651	197332.246078	36.760999
1562.104954	197701.694104	36.766016
1563.278613	198065.253800	36.771034
1565.104911	198430.142439	36.776052
1566.348894	198795.687801	36.781069
1568.493763	199150.053871	36.786087
1570.405210	199508.332588	36.791104
1571.850794	199882.674294	36.796122
1573.469786	200249.016367	36.801140
1575.055171	200621.447392	36.806157
1576.816874	200974.337367	36.811175
1578.051202	201352.111899	36.816192
1579.504162	201728.646274	36.821210
1581.046718	202106.450240	36.826228
1582.634752	202484.794689	36.831245
1584.677422	202847.195536	36.836263
1586.064020	203229.767060	36.841280
1587.295641	203604.392723	36.846298
1589.227168	203975.502142	36.851316
1590.526746	204369.203707	36.856333
1592.299940	204753.141573	36.861351
1594.276813	205141.771090	36.866368
1595.603165	205519.222391	36.871386
1597.491508	205890.843826	36.876404
1599.292016	206289.158190	36.881421
1600.591825	206652.081418	36.886439
1602.109436	207047.983211	36.891456
1603.877844	207430.894444	36.896474
1606.005908	207818.738298	36.901492
1607.364659	208189.099722	36.906509
1609.159825	208575.478589	36.911527
1610.498855	208961.642572	36.916544
1611.890006	209348.244254	36.921562
1613.717329	209726.128736	36.926580
1616.112007	210097.877271	36.931597
1617.977227	210460.407407	36.936615
1619.625970	210840.307405	36.941632
1621.644271	211214.764280	36.946650
1624.117134	211564.742403	36.951668
1625.185034	211911.982479	36.956685
1626.822360	212268.932927	36.961703
1628.601271	212630.712193	36.966720
1629.758847	212986.398812	36.971738
1631.763306	213345.121722	36.976756
1632.876598	213711.510525	36.981773
1634.690821	214070.242418	36.986791
1636.247299	214432.650033	36.991808
1637.031543	214810.094483	36.996826
1638.987046	215167.283695	37.001844
1640.463670	215522.140618	37.006861
1641.719181	215873.556002	37.011879
1643.435179	216225.938044	37.016896
1644.070470	216602.170051	37.021914
1645.705001	216973.337006	37.026932
1647.292150	217352.335687	37.031949
1649.913572	217700.307116	37.036967
1651.668789	218064.397900	37.041984
1652.830701	218442.251978	37.047002
1654.571842	218849.244969	37.052020
1655.564132	219255.067902	37.057037
1657.201957	219633.178220	37.062055
1658.586858	220026.062670	37.067072
1659.983510	220410.641457	37.072090
1661.634766	220810.799717	37.077108
1663.145751	221203.667901	37.082125
1664.895683	221604.854291	37.087143
1666.036426	222012.238415	37.092160
1667.492651	222433.389004	37.097178
1669.254389	222842.070771	37.102196
1670.858808	223277.956973	37.107213
1672.442024	223698.862928	37.112231
1674.250273	224132.331357	37.117248
1675.541595	224570.915808	37.122266
1677.555769	225004.023413	37.127284
1679.232760	225435.308717	37.132301
1680.782124	225877.944890	37.137319
1682.133057	226320.031269	37.142336
1683.629862	226775.861897	37.147354
1685.373985	227208.666547	37.152372
1687.096119	227670.406911	37.157389
1690.157828	228103.708511	37.162407
1692.636142	228520.572362	37.167424
1694.826228	228948.788227	37.172442
1697.035285	229367.426462	37.177460
1698.644718	229784.742541	37.182477
1700.211998	230208.772605	37.187495
1702.033752	230614.473627	37.192512
1703.677319	231046.266284	37.197530
1705.274242	231458.484043	37.202548
1706.851939	231887.572292	37.207565
1708.489199	232302.427529	37.212583
1710.363421	232736.752764	37.217600
1711.637013	233160.509956	37.222618
1713.515837	233593.312880	37.227636
1715.410343	234014.683938	37.232653
1718.099164	234413.851454	37.237671
1720.689327	234818.548339	37.242688
1721.899230	235224.972650	37.247706
1723.687075	235629.473731	37.252724
1725.479381	236036.007189	37.257741
1727.028367	236441.083088	37.262759
1728.600656	236849.839338	37.267776
1729.899585	237276.930831	37.272794
1731.604487	237683.152392	37.277812
1732.758097	238103.208174	37.282829
1734.224408	238529.970216	37.287847
1736.026131	238951.292703	37.292864
1737.539798	239373.679725	37.297882
1739.157346	239816.803952	37.302900
1741.047968	240247.335512	37.307917
1742.687275	240673.946725	37.312935
1744.428321	241108.162679	37.317952
1746.431081	241553.360904	37.322970
1748.344995	241973.299467	37.327988
1750.487371	242402.117344	37.333005
1752.117495	242821.164435	37.338023
1754.635455	243242.047200	37.343040
1756.721951	243638.412341	37.348058
1759.162825	244011.501809	37.353076
1761.139285	244380.807274	37.358093
1762.626733	244758.424375	37.363111
1765.733298	245105.317222	37.368128
1767.801412	245454.769685	37.373146
1769.350809	245816.653857	37.378164
1770.937930	246176.728685	37.383181
1772.124487	246538.165587	37.388199
1773.666802	246892.736310	37.393216
1774.621003	247275.728561	37.398234
1775.944858	247659.447788	37.403252
1777.393753	248048.074999	37.408269
1778.535570	248462.486426	37.413287
1780.214384	248862.355523	37.418304
1781.577844	249278.204729	37.423322
1782.658300	249698.699030	37.428340
1784.329130	250128.825743	37.433357
1785.300194	250570.855359	37.438375
1787.179237	251017.613041	37.443392
1788.416831	251482.005115	37.448410
1790.205579	251954.740562	37.453428
1791.843443	252413.707479	37.458445
1793.479257	252886.621469	37.463463
1795.604533	253359.531336	37.468480
1797.351422	253842.233431	37.473498
1799.146108	254319.618751	37.478516
1801.084608	254796.015367	37.483533
1803.240407	255281.648629	37.488551
1805.255892	255766.467031	37.493568
1806.948501	256255.454294	37.498586
1808.616819	256735.427652	37.503604
1810.867048	257224.247178	37.508621
1812.350192	257720.230147	37.513639
1814.348084	258209.650526	37.518656
1815.827253	258706.091709	37.523674
1817.704556	259201.552802	37.528692
1819.711870	259707.966752	37.533709
1821.452469	260208.124728	37.538727
1823.383144	260711.299761	37.543744
1824.813571	261223.397653	37.548762
1826.777435	261724.230044	37.553780
1828.587763	262233.750212	37.558797
1830.331981	262749.225543	37.563815
1832.353663	263268.567061	37.568832
1833.769948	263783.080027	37.573850
1835.712125	264308.937493	37.578868
1838.290172	264830.142623	37.583885
1839.794670	265346.113670	37.588903
1842.105279	265860.325614	37.593920
1843.571076	266374.270121	37.598938
1845.495704	266905.311106	37.603956
1847.975305	267420.357720	37.608973
1849.110049	267934.787429	37.613991
1851.039862	268455.283858	37.619008
1852.882416	268987.200135	37.624026
1854.600754	269501.023936	37.629044
1856.618179	270022.520335	37.634061
1858.460579	270558.931124	37.639079
1860.442235	271076.342221	37.644096
1863.503542	271568.069988	37.649114
1866.192397	272070.603961	37.654132
1868.369424	272567.912450	37.659149
1870.505062	273051.839750	37.664167
1872.702917	273535.705260	37.669184
1874.576995	274011.189721	37.674202
1876.388000	274481.146049	37.679220
1877.853910	274955.959646	37.684237
1879.771340	275435.143421	37.689255
1881.557443	275904.644237	37.694272
1883.138665	276363.686774	37.699290
1884.390406	276820.522020	37.704308
1886.420571	277273.824100	37.709325
1887.719824	277750.514484	37.714343
1889.347780	278232.585783	37.719360
1890.975095	278712.242962	37.724378
1892.461720	279208.560773	37.729396
1894.031422	279699.376884	37.734413
1895.439897	280215.366533	37.739431
1897.114984	280714.037534	37.744448
1898.514428	281237.773710	37.749466
1900.467670	281766.700736	37.754484
1902.183558	282295.132018	37.759501
1903.917196	282842.584793	37.764519
1906.013082	283377.757966	37.769536
1908.087443	283926.091113	37.774554
1910.014214	284468.401316	37.779572
1912.794716	285001.475254	37.784589
1914.936194	285535.338728	37.789607
1917.264180	286062.336746	37.794624
1919.404072	286603.055290	37.799642
1921.462510	287127.731905	37.804660
1923.247363	287657.176438	37.809677
1925.087354	288184.476334	37.814695
1926.757294	288730.980016	37.819712
1928.753459	289269.147185	37.824730
1930.110492	289823.902744	37.829748
1932.872464	290358.078527	37.834765
1934.810060	290907.222050	37.839783
1936.952638	291440.962318	37.844800
1939.214727	291977.042934	37.849818
1941.397078	292516.106298	37.854836
1943.613535	293053.383756	37.859853
1945.604669	293586.708292	37.864871
1947.551286	294116.735892	37.869888
1949.594283	294652.841203	37.874906
1951.284207	295187.351373	37.879924
1953.359608	295721.871732	37.884941
1955.032313	296264.609230	37.889959
1956.491638	296819.824950	37.894976
1958.909555	297373.381269	37.899994
1960.631430	297922.604810	37.905012
1962.410310	298468.920716	37.910029
1964.258617	299023.603961	37.915047
1966.137227	299575.155281	37.920064
1968.065875	300145.185483	37.925082
1970.227522	300701.840001	37.930100
1972.732904	301238.065463	37.935117
1975.016109	301793.779570	37.940135
1977.384900	302341.450711	37.945152
1979.271217	302888.791992	37.950170
1980.908823	303431.396440	37.955188
1983.122929	303979.388547	37.960205
1985.145754	304537.440925	37.965223
1986.785131	305093.851582	37.970240
1989.087489	305636.943082	37.975258
1991.481938	306192.968503	37.980276
1993.615317	306733.059028	37.985293
1995.038672	307286.875878	37.990311
1996.691543	307824.626270	37.995328
1999.051638	308370.281852	38.000346
2000.940534	308932.138124	38.005364
2002.883023	309461.703695	38.010381
2004.588976	310035.264832	38.015399
2006.804425	310587.939030	38.020416
2008.849553	311146.072169	38.025434
2010.148229	311702.699268	38.030452
2012.010087	312252.957033	38.035469
2013.523180	312792.958194	38.040487
2015.609118	313337.609931	38.045504
2017.667654	313877.869106	38.050522
2019.394111	314443.929009	38.055540
2021.446305	314990.834615	38.060557
2023.326046	315559.679585	38.065575
2025.482354	316113.339939	38.070592
2027.345464	316666.485816	38.075610
2029.475349	317231.848441	38.080628
2031.620802	317805.710739	38.085645
2033.632429	318378.270052	38.090663
2035.514235	318952.928325	38.095680
2037.657081	319533.988499	38.100698
2039.667868	320113.999093	38.105716
2041.720084	320690.671581	38.110733
2043.667075	321284.749909	38.115751
2045.013298	321888.520082	38.120768
2046.978405	322474.688055	38.125786
2048.777256	323077.128550	38.130804
2051.098849	323699.307541	38.135821
2053.484521	324301.487535	38.140839
2055.430801	324908.609280	38.145856
2057.708530	325525.978942	38.150874
2059.197356	326145.554611	38.155892
2061.166865	326765.958852	38.160909
2063.421665	327398.902923	38.165927
2065.445315	328033.148001	38.170944
2067.595316	328658.733370	38.175962
2069.449217	329294.135639	38.180980
2071.616387	329935.775732	38.185997
2073.600262	330576.652016	38.191015
2075.363970	331225.884735	38.196032
2077.647599	331863.371554	38.201050
2080.186124	332515.635332	38.206068
2083.085788	333152.853775	38.211085
2085.153030	333788.704459	38.216103
2087.508222	334412.365733	38.221120
2089.974878	335043.236588	38.226138
2091.894154	335683.710087	38.231156
2094.699071	336302.198497	38.236173
2097.279855	336930.946966	38.241191
2099.400760	337556.920766	38.246208
2101.686127	338143.717077	38.251226
2104.148105	338749.262056	38.256244
2106.633785	339349.110078	38.261261
2109.003405	339942.522830	38.266279
2111.033493	340551.570104	38.271296
2113.030324	341145.461887	38.276314
2115.090417	341750.326999	38.281332
2116.943141	342348.137311	38.286349
2119.320125	342961.641687	38.291367
2121.229066	343563.895338	38.296384
2122.991227	344160.454961	38.301402
2125.280115	344764.458635	38.306420
2128.190517	345345.814027	38.311437
2131.344492	345904.584235	38.316455
2133.812802	346488.359053	38.321472
2135.981233	347062.734779	38.326490
2137.520373	347644.364346	38.331508
2139.394396	348224.053381	38.336525
2141.290182	348805.305094	38.341543
2143.438319	349373.767750	38.346560
2145.024178	349963.710083	38.351578
2147.176150	350554.668052	38.356596
2148.886473	351157.466406	38.361613
2150.879368	351760.057813	38.366631
2152.732463	352366.419944	38.371648
2154.374510	352929.439794	38.376666
2156.065443	353543.070275	38.381684
2158.161701	354123.255848	38.386701
2160.090866	354707.445224	38.391719
2161.773181	355318.311523	38.396736
2163.457070	355928.077754	38.401754
2165.181361	356557.646178	38.406772
2167.363368	357183.272894	38.411789
2169.010341	357827.298461	38.416807
2170.512780	358468.927480	38.421824
2172.613200	359118.694226	38.426842
2174.569317	359796.079972	38.431860
2176.302126	360474.252526	38.436877
2178.596776	361152.727088	38.441895
2180.534899	361851.799860	38.446912
2182.934275	362530.031008	38.451930
2185.240106	363227.699838	38.456948
2187.783088	363925.596353	38.461965
2190.301855	364613.564987	38.466983
2192.109820	365329.417918	38.472000
2194.925749	366021.726916	38.477018
2196.888960	366738.669780	38.482036
2199.362428	367443.084912	38.487053
2202.456075	368132.519530	38.492071
2204.990872	368834.336627	38.497088
2207.521216	369516.685387	38.502106
2210.005682	370202.884853	38.507124
2212.511012	370881.839053	38.512141
2215.282264	371556.703877	38.517159
2217.747248	372243.730983	38.522176
2220.188048	372909.164377	38.527194
2222.448759	373572.459338	38.532212
2224.487897	374238.999721	38.537229
2227.052129	374916.220189	38.542247
2228.987103	375595.509769	38.547264
2231.792021	376265.740926	38.552282
2233.796442	376943.319219	38.557300
2235.602442	377618.786802	38.562317
2237.954464	378309.062963	38.567335
2239.646568	378988.504158	38.572352
2241.568657	379692.086565	38.577370
2243.150658	380399.920072	38.582388
2245.209115	381098.835655	38.587405
2247.549771	381801.367062	38.592423
2249.457979	382508.620745	38.597440
2251.285826	383229.691929	38.602458
2253.673467	383975.301015	38.607476
2255.861898	384704.216943	38.612493
2257.711596	385431.220188	38.617511
2259.923145	386178.177309	38.622528
2262.243437	386898.959733	38.627546
2264.969845	387649.727690	38.632564
2267.251252	388410.337417	38.637581
2269.730673	389140.803732	38.642599
2271.812769	389881.636619	38.647616
2274.616629	390629.025584	38.652634
2276.918027	391359.571076	38.657652
2279.768311	392097.208109	38.662669
2282.477056	392831.352730	38.667687
2284.434311	393562.967506	38.672704
2286.693942	394287.848489	38.677722
2289.020028	395035.817650	38.682740
2290.728416	395780.118888	38.687757
2293.204482	396510.791191	38.692775
2295.369564	397261.088651	38.697792
2297.606638	398007.224152	38.702810
2299.795494	398746.049751	38.707828
2301.878652	399466.525750	38.712845
2304.698738	400192.083048	38.717863
2306.497663	400914.774932	38.722880
2308.970276	401620.257653	38.727898
2311.146367	402351.872858	38.732916
2313.260376	403063.790419	38.737933
2315.436462	403787.260052	38.742951
2317.625537	404516.308937	38.747968
2319.983036	405237.709782	38.752986
2321.952000	405976.765644	38.758004
2324.266514	406721.243035	38.763021
2326.707220	407466.313061	38.768039
2328.740361	408212.367602	38.773056
2331.109849	408959.385158	38.778074
2333.777095	409729.969801	38.783092
2335.954530	410478.953451	38.788109
2338.621630	411221.198506	38.793127
2340.509079	411988.402197	38.798144
2343.361974	412758.059172	38.803162
2345.724048	413512.728600	38.808180
2347.683342	414289.201141	38.813197
2350.443903	415045.508884	38.818215
2352.826726	415804.187312	38.823232
2355.795130	416561.683404	38.828250
2358.016844	417339.010032	38.833268
2360.767948	418109.691926	38.838285
2362.806152	418871.908373	38.843303
2365.007410	419635.569396	38.848320
2367.074961	420427.440133	38.853338
2369.777495	421210.014580	38.858356
2371.515722	422010.727733	38.863373
2374.165674	422804.225728	38.868391
2376.011453	423600.717639	38.873408
2378.037841	424404.420989	38.878426
2380.549680	425199.738943	38.883444
2383.251395	426007.304429	38.888461
2386.364512	426801.357370	38.893479
2388.495242	427625.115854	38.898496
2390.935064	428428.289893	38.903514
2393.377792	429246.372337	38.908532
2395.681159	430054.780045	38.913549
2398.660781	430848.873695	38.918567
2401.096976	431672.240510	38.923584
2403.792508	432476.552568	38.928602
2405.980878	433275.403136	38.933620
2408.142248	434093.921668	38.938637
2410.678155	434913.665782	38.943655
2412.888546	435729.689100	38.948672
2415.148936	436558.936089	38.953690
2417.164735	437386.169046	38.958708
2419.232957	438214.274449	38.963725
2421.764498	439043.639784	38.968743
2424.340031	439892.046014	38.973760
2426.643152	440728.168455	38.978778
2429.438078	441564.279892	38.983796
2432.062979	442404.942118	38.988813
2434.604483	443226.864896	38.993831
2437.469572	444075.317620	38.998848
2440.030236	444890.243632	39.003866
2442.886040	445724.214784	39.008884
2444.988244	446545.276494	39.013901
2447.614628	447365.613718	39.018919
2449.580685	448199.788381	39.023936
2452.288051	449023.236272	39.028954
2454.816366	449863.576819	39.033972
2456.835352	450684.241648	39.038989
2458.923464	451537.436358	39.044007
2461.608684	452369.963954	39.049024
2464.893045	453181.775811	39.054042
2467.584809	453977.773963	39.059060
2469.520798	454771.792962	39.064077
2472.195624	455562.929111	39.069095
2474.487538	456368.863858	39.074112
2477.033764	457141.250872	39.079130
2479.427317	457943.871022	39.084148
2481.724254	458736.262191	39.089165
2483.852537	459534.565827	39.094183
2485.939362	460358.123674	39.099200
2488.403263	461166.065274	39.104218
2490.713328	461992.906787	39.109236
2492.783127	462826.376024	39.114253
2495.458208	463655.565641	39.119271
2497.456495	464510.156312	39.124288
2499.549941	465363.279145	39.129306
2502.023908	466236.064482	39.134324
2503.854583	467111.696768	39.139341
2506.066425	467974.289229	39.144359
2508.439532	468874.061747	39.149376
2511.068605	469784.210680	39.154394
2513.358276	470693.311451	39.159412
2515.658101	471600.902167	39.164429
2518.511523	472518.969018	39.169447
2521.517781	473433.025519	39.174464
2524.257229	474354.811646	39.179482
2526.928428	475247.667192	39.184500
2529.602846	476177.558802	39.189517
2532.366082	477093.043577	39.194535
2534.627987	478006.949603	39.199552
2537.124827	478938.449949	39.204570
2539.893780	479863.696644	39.209588
2542.174195	480794.835714	39.214605
2545.141214	481726.874729	39.219623
2547.749546	482658.319189	39.224640
2550.530205	483588.071527	39.229658
2553.107873	484526.494316	39.234676
2556.138528	485452.473706	39.239693
2558.696505	486386.258292	39.244711
2561.446479	487305.927345	39.249728
2564.017200	488234.059428	39.254746
2567.433136	489147.717540	39.259764
2570.314297	490077.619695	39.264781
2573.212300	490981.777996	39.269799
2576.223833	491892.936888	39.274816
2579.049696	492790.199467	39.279834
2581.799231	493683.087969	39.284852
2584.778859	494576.649294	39.289869
2586.829736	495466.027989	39.294887
2589.506129	496362.473041	39.299904
2591.635091	497259.364853	39.304922
2594.651226	498163.076156	39.309940
2596.925263	499069.888577	39.314957
2599.025000	499970.627117	39.319975
2601.394521	500877.830806	39.324992
2603.828582	501798.644689	39.330010
2606.820595	502707.109156	39.335028
2609.162346	503620.422615	39.340045
2611.641609	504537.697703	39.345063
2614.141851	505471.661578	39.350080
2616.407545	506395.878135	39.355098
2619.513211	507308.810195	39.360116
2621.801350	508241.995076	39.365133
2624.313741	509171.358159	39.370151
2626.754777	510106.376668	39.375168
2629.313336	511039.960251	39.380186
2632.107928	511980.911419	39.385204
2634.505001	512933.567394	39.390221
2636.708425	513858.979228	39.395239
2639.366062	514787.487877	39.400256
2641.906848	515685.771737	39.405274
2644.642499	516600.653472	39.410292
2646.559853	517517.178842	39.415309
2649.544784	518445.417026	39.420327
2651.928323	519378.939225	39.425344
2654.296614	520315.027665	39.430362
2656.991059	521251.458978	39.435380
2659.398627	522190.903231	39.440397
2661.760744	523145.863354	39.445415
2664.134945	524104.892229	39.450432
2667.112839	525063.257382	39.455450
2669.943726	526031.004505	39.460468
2672.130834	527020.199737	39.465485
2674.741392	527985.389754	39.470503
2678.050522	528969.185173	39.475520
2680.477344	529944.350083	39.480538
2683.097136	530934.372923	39.485556
2685.658386	531940.349176	39.490573
2688.464368	532939.520885	39.495591
2691.475007	533939.597646	39.500608
2694.698210	534931.366279	39.505626
2698.420024	535917.247342	39.510644
2700.800551	536907.711446	39.515661
2703.486930	537906.713267	39.520679
2706.107675	538916.727434	39.525696
2708.149325	539923.193390	39.530714
2710.784939	540941.314569	39.535732
2713.330663	541954.397008	39.540749
2715.449529	542988.707225	39.545767
2718.287123	544021.616034	39.550784
2720.940332	545063.382578	39.555802
2723.935961	546103.154371	39.560820
2726.548876	547151.662778	39.565837
2729.293538	548207.312081	39.570855
2732.475329	549227.710141	39.575872
2734.910611	550297.481674	39.580890
2737.671069	551351.882501	39.585908
2740.287751	552419.799736	39.590925
2743.247987	553480.187268	39.595943
2746.397415	554527.190902	39.600960
2750.752297	555544.411393	39.605978
2754.980780	556558.208793	39.610996
2757.890221	557578.479218	39.616013
2760.542612	558592.935600	39.621031
2763.713671	559602.054091	39.626048
2766.351618	560610.279591	39.631066
2769.911334	561587.580568	39.636084
2772.680886	562581.165504	39.641101
2775.467449	563575.275490	39.646119
2778.773887	564536.174725	39.651136
2781.610561	565511.746228	39.656154
2784.777280	566471.521643	39.661172
2787.298701	567446.749020	39.666189
2789.694852	568421.773004	39.671207
2792.470946	569396.158665	39.676224
2794.791263	570367.734185	39.681242
2797.046070	571339.949741	39.686260
2799.375292	572330.852967	39.691277
2802.159885	573314.777772	39.696295
2804.832900	574327.905273	39.701312
2806.973428	575327.138042	39.706330
2809.471345	576336.821082	39.711348
2812.039775	577354.138750	39.716365
2814.001885	578397.062159	39.721383
2816.872627	579429.112866	39.726400
2819.385338	580475.433989	39.731418
2821.821072	581520.024211	39.736436
2824.397861	582537.217751	39.741453
2826.892502	583562.615965	39.746471
2830.117791	584578.179649	39.751488
2832.233498	585619.615898	39.756506
2834.858716	586666.043615	39.761524
2837.430138	587707.326412	39.766541
2840.223448	588752.343191	39.771559
2842.899662	589824.206764	39.776576
2845.501976	590902.452735	39.781594
2848.200462	591959.686827	39.786612
2851.307877	593046.727588	39.791629
2854.022943	594146.361054	39.796647
2856.618102	595239.699469	39.801664
2859.222445	596342.353878	39.806682
2862.193821	597473.598738	39.811700
2865.403238	598570.584355	39.816717
2868.726849	599672.556909	39.821735
2872.487636	600785.621235	39.826752
2875.493105	601894.497016	39.831770
2878.535560	602992.445226	39.836788
2882.152760	604095.250841	39.841805
2885.021462	605190.414656	39.846823
2888.301114	606293.064640	39.851840
2891.049978	607395.345229	39.856858
2893.997144	608492.381612	39.861876
2897.753233	609572.064300	39.866893
2900.696204	610672.292931	39.871911
2904.135747	611754.120619	39.876928
2907.378005	612831.924401	39.881946
2910.430487	613909.205428	39.886964
2913.515107	614979.674742	39.891981
2916.435985	616066.822211	39.896999
2919.108605	617156.854382	39.902016
2921.540923	618248.218651	39.907034
2924.477223	619340.141644	39.912052
2927.107740	620444.204604	39.917069
2929.375336	621554.014488	39.922087
2932.010214	622677.546022	39.927104
2934.821574	623804.030875	39.932122
2937.085027	624931.038509	39.937140
2939.809718	626072.592684	39.942157
2942.319102	627218.857481	39.947175
2945.105315	628394.827840	39.952192
2947.408547	629573.945160	39.957210
2950.193390	630746.509511	39.962228
2952.960388	631944.915698	39.967245
2955.368851	633155.778467	39.972263
2958.276805	634359.929135	39.977280
2961.271730	635595.827571	39.982298
2964.010920	636816.198030	39.987316
2966.892619	638047.332493	39.992333
2969.717617	639296.295931	39.997351
2972.785465	640535.039080	40.002368
2975.715872	641789.072790	40.007386
2979.067362	643035.301384	40.012404
2982.719272	644262.374335	40.017421
2985.601463	645523.091548	40.022439
2988.741454	646763.612954	40.027456
2991.537171	648007.030911	40.032474
2994.258796	649277.279823	40.037492
2998.039613	650507.513791	40.042509
3001.340589	651751.332893	40.047527
3005.023232	652996.977567	40.052544
3007.954892	654233.620592	40.057562
3011.014466	655461.418945	40.062580
3014.317064	656690.668814	40.067597
3016.799075	657921.345122	40.072615
3020.229671	659127.505230	40.077632
3023.879287	660297.325818	40.082650
3027.567133	661459.929070	40.087668
3030.667497	662623.585479	40.092685
3033.713896	663770.284719	40.097703
3036.877427	664931.313530	40.102720
3039.805246	666071.885198	40.107738
3042.157831	667246.853183	40.112756
3045.245725	668388.964175	40.117773
3047.579104	669570.516413	40.122791
3050.942063	670731.505659	40.127808
3054.689849	671888.907060	40.132826
3057.354319	673047.489155	40.137844
3060.606485	674213.539844	40.142861
3063.512250	675397.949618	40.147879
3066.570598	676572.340894	40.152896
3069.290662	677765.728469	40.157914
3072.537216	678938.001242	40.162932
3075.984828	680122.467188	40.167949
3078.959382	681336.275808	40.172967
3081.863940	682527.230954	40.177984
3084.838747	683726.614352	40.183002
3087.331797	684934.413794	40.188020
3090.099128	686163.562422	40.193037
3092.656141	687400.574575	40.198055
3095.306949	688635.615326	40.203072
3097.887886	689915.177897	40.208090
3100.934401	691197.162584	40.213108
3103.825229	692467.128780	40.218125
3106.688027	693776.269694	40.223143
3109.344765	695072.204044	40.228160
3112.547825	696390.133333	40.233178
3115.269796	697701.894895	40.238196
3118.800394	699028.652647	40.243213
3122.025508	700370.780973	40.248231
3125.288689	701691.032626	40.253248
3128.285760	703033.435332	40.258266
3130.842521	704392.109004	40.263284
3134.159514	705742.912829	40.268301
3137.533954	707109.450503	40.273319
3141.101075	708464.544382	40.278336
3144.463350	709818.022167	40.283354
3147.830597	711181.784347	40.288372
3151.296924	712527.239549	40.293389
3154.468290	713899.264682	40.298407
3157.916595	715244.094841	40.303424
3161.568682	716597.190140	40.308442
3164.600732	717947.993155	40.313460
3167.815629	719304.387019	40.318477
3170.656822	720669.230109	40.323495
3173.648168	722027.247238	40.328512
3177.122938	723387.138917	40.333530
3180.167983	724756.816413	40.338548
3183.332460	726121.798111	40.343565
3186.124122	727516.369821	40.348583
3188.905380	728889.505998	40.353600
3192.049361	730284.932275	40.358618
3194.823512	731680.575912	40.363636
3198.357492	733054.368838	40.368653
3201.706708	734445.638835	40.373671
3204.968146	735832.486581	40.378688
3208.946758	737214.040402	40.383706
3212.416762	738603.781638	40.388724
3215.752894	739971.983956	40.393741
3219.077608	741345.134096	40.398759
3222.480851	742716.899200	40.403776
3226.192761	744094.541317	40.408794
3229.191467	745470.482249	40.413812
3232.433423	746812.366680	40.418829
3235.811560	748136.744223	40.423847
3238.599146	749455.375438	40.428864
3242.637238	750754.751465	40.433882
3246.449350	752029.999830	40.438900
3250.203254	753315.886389	40.443917
3253.569678	754605.513997	40.448935
3256.205194	755890.514950	40.453952
3260.014529	757159.546977	40.458970
3262.642066	758455.395538	40.463988
3265.842250	759740.690845	40.469005
3268.735523	761043.389954	40.474023
3271.101768	762355.203301	40.479040
3274.295896	763676.148256	40.484058
3277.307535	765026.062033	40.489076
3280.302031	766343.964522	40.494093
3283.568881	767695.323315	40.499111
3286.688141	769039.480579	40.504128
3290.000619	770383.805784	40.509146
3292.843284	771764.087661	40.514164
3296.161197	773147.669990	40.519181
3299.098764	774537.294747	40.524199
3301.923231	775942.246183	40.529216
3304.779711	777343.927463	40.534234
3307.939251	778768.317736	40.539252
3311.355723	780196.707090	40.544269
3314.465388	781634.436642	40.549287
3317.515169	783073.902371	40.554304
3321.259881	784525.673129	40.559322
3324.318381	785984.179959	40.564340
3328.903011	787419.579921	40.569357
3333.645884	788852.164796	40.574375
3336.870184	790294.858935	40.579392
3340.703187	791728.680738	40.584410
3344.172058	793165.604076	40.589428
3347.518641	794587.116611	40.594445
3350.748290	796031.529182	40.599463
3354.416829	797457.501527	40.604480
3357.564251	798890.710814	40.609498
3360.814764	800339.811040	40.614516
3364.255109	801790.143719	40.619533
3367.414676	803243.350331	40.624551
3370.666865	804680.092031	40.629568
3374.188200	806129.450445	40.634586
3377.133184	807579.330951	40.639604
3380.837797	809029.316616	40.644621
3384.020345	810497.262573	40.649639
3387.000070	811957.252454	40.654656
3390.321520	813430.844515	40.659674
3393.591360	814908.714977	40.664692
3396.682191	816376.962670	40.669709
3400.124722	817877.690404	40.674727
3402.918366	819361.347293	40.679744
3406.297937	820859.316024	40.684762
3409.700199	822360.895432	40.689780
3412.799375	823875.794207	40.694797
3416.286285	825401.937453	40.699815
3419.215338	826909.924251	40.704832
3422.953291	828423.768268	40.709850
3426.478643	829956.937302	40.714868
3430.305795	831479.415066	40.719885
3434.214019	832976.873794	40.724903
3437.496689	834507.985637	40.729920
3441.107940	836005.716908	40.734938
3444.670162	837525.743272	40.739956
3447.752423	839044.125758	40.744973
3451.099130	840560.839055	40.749991
3454.100311	842113.779924	40.755008
3457.648693	843599.876370	40.760013
3461.029062	845075.210776	40.765018
3464.589197	846467.614830	40.770023
3467.754905	847815.924201	40.775028
3470.769126	849100.640741	40.780032
3473.617313	850296.868316	40.785037
3476.947963	851439.611488	40.790042
3479.928699	852512.774532	40.795047
3482.763296	853511.102037	40.800052
3484.956436	854457.587361	40.805056
3487.643965	855305.640028	40.810061
3490.025125	856114.018221	40.815066
3492.086656	856853.255600	40.820071
3494.276103	857521.259957	40.825076
3495.814440	858125.381900	40.830080
3497.714780	858693.489409	40.835085
3499.083824	859197.823152	40.840090
3501.235156	859646.255278	40.845095
3502.927125	860050.965043	40.850100
3504.433732	860408.706707	40.855104
3506.432338	860712.083502	40.860109
3507.155156	860978.606445	40.865114
3508.788889	861205.392022	40.870119
3510.046297	861386.433623	40.875124
3511.065834	861519.865094	40.880128
3512.102169	861638.609011	40.885133
3512.869281	861709.655277	40.890138
3513.497648	861747.471250	40.895143
3514.243792	861771.752789	40.900148
3515.234587	861763.325076	40.905152
3516.190833	861724.470246	40.910157
3516.370882	861679.909201	40.915162
3516.623479	861596.151647	40.920167
3517.451350	861512.589891	40.925172
3517.712144	861405.006239	40.930176
3518.513333	861259.214890	40.935181
3518.652919	861119.849594	40.940186
3519.195294	860962.716807	40.945191
3519.509111	860773.818683	40.950196
3519.522648	860601.204537	40.955200
3519.851092	860397.316249	40.960205
3520.227883	860194.483002	40.965210
3520.320152	859974.280845	40.970215
3520.572279	859751.418396	40.975220
3520.294707	859506.556006	40.980224
3520.841650	859255.809169	40.985229
3520.998452	859014.746350	40.990234
3521.300198	858749.622852	40.995239
3521.414175	858487.729113	41.000244
3521.040263	858205.669225	41.005248
3521.498515	857939.706724	41.010253
3521.655782	857652.961375	41.015258
3521.718298	857374.196768	41.020263
3521.855077	857066.021726	41.025268
3521.692956	856775.298675	41.030272
3522.000681	856476.018317	41.035277
3521.581643	856175.967291	41.040282
3521.877245	855859.531127	41.045287
3521.878830	855546.630974	41.050292
3521.700352	855251.361774	41.055296
3521.957629	854920.965374	41.060301
3521.644896	854606.512031	41.065306
3521.967534	854299.628488	41.070311
3521.897831	853977.412759	41.075316
3521.778587	853644.868575	41.080320
3521.945640	853317.224900	41.085325
3521.516237	853002.904163	41.090330
3521.505819	852670.387227	41.095335
3521.197630	852351.339678	41.100340
3521.150860	852035.446331	41.105344
3521.436782	851707.600871	41.110349
3521.536519	851385.807182	41.115354
3521.010473	851066.047910	41.120359
3521.344261	850733.468253	41.125364
3521.102920	850416.453478	41.130368
3521.200739	850092.353024	41.135373
3521.101730	849768.268186	41.140378
3520.825293	849441.857627	41.145383
3520.978514	849106.493309	41.150388
3520.484799	848795.770777	41.155392
3520.893401	848464.227342	41.160397
3520.674889	848141.637021	41.165402
3520.736511	847814.696250	41.170407
3520.742199	847481.900468	41.175412
3520.425961	847164.635991	41.180416
3520.339905	846843.419055	41.185421
3520.185456	846524.146354	41.190426
3520.189135	846195.376506	41.195431
3520.294939	845876.125567	41.200436
3519.875670	845557.237401	41.205440
3519.947642	845240.689403	41.210445
3519.802371	844932.935686	41.215450
3519.790740	844612.372760	41.220455
3520.072030	844294.475409	41.225460
3519.555530	843981.471366	41.230464
3519.310255	843670.113632	41.235469
3519.659777	843344.648893	41.240474
3519.309495	843041.176450	41.245479
3519.513563	842727.845497	41.250484
3519.147384	842410.984333	41.255488
3519.487349	842116.619493	41.260493
3519.019465	841794.818761	41.265498
3519.052647	841476.430867	41.270503
3519.308332	841172.232815	41.275508
3518.988890	840857.237531	41.280512
3519.353733	840537.235941	41.285517
3519.004805	840226.994823	41.290522
3518.817250	839919.931841	41.295527
3518.744949	839617.323532	41.300532
3518.348281	839318.803848	41.305536
3518.244357	839007.731283	41.310541
3518.335467	838717.105029	41.315546
3518.287045	838419.217903	41.320551
3518.248238	838113.605145	41.325556
3517.882418	837827.503261	41.330560
3517.532288	837519.424603	41.335565
3517.686055	837222.180590	41.340570
3517.479730	836939.819672	41.345575
3517.470443	836645.699526	41.350580
3517.187476	836357.907760	41.355584
3516.998199	836069.599539	41.360589
3517.013646	835800.575961	41.365594
3516.871023	835513.602010	41.370599
3517.036368	835225.539315	41.375604
3516.711769	834964.494599	41.380608
3516.571929	834681.779548	41.385613
3516.462239	834406.664139	41.390618
3516.335991	834126.656842	41.395623
3516.021623	833852.723447	41.400628
3516.095130	833605.230875	41.405632
3516.159223	833326.866739	41.410637
3516.070401	833059.894856	41.415642
3516.212659	832802.250991	41.420647
3516.036516	832530.876182	41.425652
3515.646420	832268.707739	41.430656
3515.960778	831999.281298	41.435661
3515.971220	831752.509873	41.440666
3515.532658	831479.864309	41.445671
3515.763927	831227.809744	41.450676
3515.211706	830972.747888	41.455680
3515.610939	830716.151379	41.460685
3515.550406	830459.278493	41.465690
3515.426409	830190.533300	41.470695
3515.331537	829933.547620	41.475700
3514.883606	829688.141488	41.480704
3514.953056	829438.487442	41.485709
3515.145680	829187.142111	41.490714
3514.854375	828946.226822	41.495719
3514.739265	828693.349404	41.500724
3514.522990	828450.693040	41.505728
3514.663198	828200.393568	41.510733
3514.735494	827958.648891	41.515738
3514.631639	827725.380034	41.520743
3514.458055	827478.330526	41.525748
3514.419936	827252.512467	41.530752
3514.464627	826991.331036	41.535757
3513.963905	826753.253579	41.540762
3513.855133	826522.875798	41.545767
3514.182685	826294.715788	41.550772
3513.990132	826067.611315	41.555776
3514.178925	825823.373175	41.560781
3513.791493	825601.027125	41.565786
3513.482859	825365.850207	41.570791
3513.683229	825129.652013	41.575796
3513.375861	824916.022071	41.580800
3513.561816	824693.844321	41.585805
3513.437950	824466.624387	41.590810
3513.101479	824236.644173	41.595815
3513.148610	824025.861171	41.600820
3513.108550	823803.641765	41.605824
3512.850132	823576.951328	41.610829
3513.061427	823368.027699	41.615834
3512.839436	823162.886069	41.620839
3512.720459	822934.292008	41.625844
3512.490799	822729.040359	41.630848
3512.783990	822517.581766	41.635853
3512.768320	822302.400668	41.640858
3512.485613	822091.659263	41.645863
3512.376913	821879.268122	41.650868
3512.640934	821683.980375	41.655872
3512.569196	821470.983011	41.660877
3512.414912	821271.446764	41.665882
3512.366506	821047.374933	41.670887
3512.356099	820843.447666	41.675892
3512.324443	820643.529864	41.680896
3512.001434	820432.595630	41.685901
3512.074284	820224.721188	41.690906
3512.015108	820039.616325	41.695911
3511.867107	819835.289343	41.700916
3511.548420	819636.220457	41.705920
3511.583338	819436.451179	41.710925
3511.680650	819246.257841	41.715930
3511.480913	819057.429419	41.720935
3511.583477	818858.953113	41.725940
3511.529713	818677.382338	41.730944
3511.240766	818478.714495	41.735949
3511.342101	818295.786273	41.740954
3511.009439	818115.127193	41.745959
3511.281722	817922.958368	41.750964
3511.076192	817745.841679	41.755968
3511.258653	817560.726153	41.760973
3511.103235	817373.996745	41.765978
3510.632384	817195.146855	41.770983
3511.044409	816999.305845	41.775988
3510.618494	816833.999770	41.780992
3510.635657	816656.083211	41.785997
3511.052028	816488.524657	41.791002
3510.964374	816290.688942	41.796007
3511.102087	816108.527328	41.801012
3510.506613	815923.641622	41.806016
3510.096526	815750.814736	41.811021
3510.506241	815583.724357	41.816026
3510.333705	815409.086757	41.821031
3510.371537	815235.536259	41.826036
3510.267457	815070.084761	41.831040
3510.104930	814897.391037	41.836045
3510.306083	814742.605973	41.841050
3509.759479	814563.845367	41.846055
3509.925283	814395.982097	41.851060
3509.647423	814243.419372	41.856064
3509.620570	814067.351628	41.861069
3509.548938	813923.612632	41.866074
3509.594074	813767.018654	41.871079
3509.666686	813598.122301	41.876084
3509.325751	813455.593237	41.881088
3509.249789	813300.820725	41.886093
3509.374845	813132.785792	41.891098
3509.015257	812999.459225	41.896103
3509.326122	812842.995995	41.901108
3509.168301	812700.812734	41.906112
3509.323978	812536.725929	41.911117
3509.454956	812379.105874	41.916122
3509.086921	812234.791890	41.921127
3508.814103	812085.510959	41.926132
3508.875202	811938.131457	41.931136
3509.121071	811776.852976	41.936141
3509.018417	811645.417170	41.941146
3508.799522	811495.085448	41.946151
3508.898000	811354.448573	41.951156
3508.402708	811209.398744	41.956160
3508.692571	811068.626424	41.961165
3508.344843	810929.230214	41.966170
3508.262937	810789.983361	41.971175
3508.282353	810653.951114	41.976180
3508.486315	810521.953017	41.981184
3508.318826	810386.926276	41.986189
3508.302833	810251.920903	41.991194
3508.108914	810123.705003	41.996199
3508.324278	809981.109202	42.001204
3508.235663	809854.635141	42.006208
3507.917901	809717.414494	42.011213
3507.984398	809583.362447	42.016218
3507.776036	809460.576536	42.021223
3507.715599	809324.971962	42.026228
3507.957188	809202.107279	42.031232
3507.797765	809071.807345	42.036237
3507.740686	808955.065098	42.041242
3507.754574	808832.133225	42.046247
3507.688660	808708.575069	42.051252
3507.555947	808594.829107	42.056256
3507.616975	808471.343779	42.061261
3507.635499	808345.951483	42.066266
3507.723946	808220.349287	42.071271
3507.593414	808104.928128	42.076276
3507.719595	807982.109511	42.081280
3507.453492	807860.627885	42.086285
3507.534479	807741.930275	42.091290
3507.563261	807626.572841	42.096295
3507.664144	807492.719178	42.101300
3507.509404	807365.915712	42.106304
3507.792797	807252.373015	42.111309
3507.427778	807131.041798	42.116314
3507.249868	807030.710793	42.121319
3507.502724	806906.086973	42.126324
3507.326856	806786.532573	42.131328
3507.486217	806658.732699	42.136333
3507.394990	806542.249046	42.141338
3507.271781	806436.261661	42.146343
3507.501370	806307.953355	42.151348
3507.000332	806184.176090	42.156352
3507.277270	806077.479802	42.161357
3507.205199	805962.601306	42.166362
3506.975043	805844.657608	42.171367
3507.168018	805728.162353	42.176372
3507.320275	805628.393928	42.181376
3507.091762	805508.776884	42.186381
3506.744287	805405.998071	42.191386
3506.515159	805298.392238	42.196391
3506.926376	805182.440271	42.201396
3506.734469	805079.532866	42.206400
3506.827765	804981.775500	42.211405
3506.926287	804865.183091	42.216410
3506.579190	804774.704755	42.221415
3506.810721	804670.495371	42.226420
3506.771466	804560.149224	42.231424
3506.746670	804442.883329	42.236429
3506.673404	804341.711029	42.241434
3506.287683	804233.182419	42.246439
3506.617102	804128.262032	42.251444
3506.502296	804032.193127	42.256448
3506.445639	803925.567456	42.261453
3506.477909	803836.044354	42.266458
3506.117993	803732.408714	42.271463
3506.528361	803635.659156	42.276468
3506.189852	803538.688221	42.281472
3506.231556	803436.012090	42.286477
3506.290927	803334.263562	42.291482
3506.087079	803237.560541	42.296487
3506.338021	803138.966179	42.301492
3506.123875	803045.647034	42.306496
3506.109715	802957.395656	42.311501
3506.147253	802854.515335	42.316506
3505.942248	802775.368809	42.321511
3505.861459	802679.079224	42.326516
3505.797476	802579.645687	42.331520
3505.845448	802481.320676	42.336525
3505.997937	802399.608863	42.341530
3505.242467	802320.694983	42.346535
3505.924515	802241.101857	42.351540
3505.778780	802148.887769	42.356544
3505.772071	802059.936823	42.361549
3505.737297	801970.498714	42.366554
3505.654247	801886.758939	42.371559
3505.845065	801801.550139	42.376564
3505.794867	801709.903253	42.381568
3506.010186	801623.412506	42.386573
3505.693560	801531.414608	42.391578
3505.534428	801452.981406	42.396583
3505.629991	801360.422663	42.401588
3505.350035	801273.469373	42.406592
3505.542284	801185.603022	42.411597
3505.399504	801114.327501	42.416602
3505.147126	801025.992591	42.421607
3505.409835	800941.497445	42.426612
3505.435854	800871.222127	42.431616
3505.422484	800784.218790	42.436621
3505.326218	800712.195383	42.441626
3505.481685	800639.491805	42.446631
3505.187471	800558.666121	42.451636
3505.210970	800478.523287	42.456640
3505.412639	800400.656730	42.461645
3505.653611	800315.863103	42.466650
3505.397392	800234.978316	42.471655
3505.519741	800150.545748	42.476660
3505.068809	800077.298166	42.481664
3504.991495	799994.319842	42.486669
3505.095944	799924.463731	42.491674
3504.559387	799870.172477	42.496679
3504.888555	799768.228972	42.501684
3504.843530	799710.616230	42.506688
3504.512897	799635.773606	42.511693
3504.699970	799573.017082	42.516698
3504.459518	799501.642933	42.521703
3504.703768	799430.777202	42.526708
3504.642813	799360.157353	42.531712
3504.885397	799297.192869	42.536717
3504.944550	799221.839838	42.541722
3504.842530	799162.121341	42.546727
3505.038797	799088.854909	42.551732
3504.451778	799027.448092	42.556736
3504.290159	798965.823406	42.561741
3504.815482	798888.917421	42.566746
3504.815643	798829.473758	42.571751
3504.745980	798751.682533	42.576756
3504.544864	798686.527610	42.581760
3504.728413	798624.057646	42.586765
3504.991313	798543.018593	42.591770
3504.589424	798487.516235	42.596775
3504.569746	798417.076385	42.601780
3504.349784	798358.646755	42.606784
3504.595937	798286.689107	42.611789
3504.566345	798220.028859	42.616794
3504.600763	798159.346571	42.621799
3504.648027	798085.554141	42.626804
3504.242502	798009.822727	42.631808
3504.747457	797960.843359	42.636813
3504.580224	797894.202673	42.641818
3504.392817	797831.737629	42.646823
3504.429658	797770.315157	42.651828
3504.259294	797701.414821	42.656832
3504.200248	797639.957902	42.661837
3504.208627	797582.073298	42.666842
3504.461327	797530.334033	42.671847
3504.266801	797461.386213	42.676852
3504.194947	797411.516086	42.681856
3504.353290	797354.979604	42.686861
3504.163241	797285.440148	42.691866
3504.127229	797235.513764	42.696871
3504.035946	797171.259462	42.701876
3504.194267	797122.085831	42.706880
3504.181702	797056.835540	42.711885
3504.194733	797012.103979	42.716890
3503.870363	796957.755068	42.721895
3504.546107	796890.622263	42.726900
3504.307974	796823.884849	42.731904
3504.067584	796767.409298	42.736909
3504.297333	796710.855852	42.741914
3503.997049	796657.482671	42.746919
3504.526893	796593.759081	42.751924
3503.961743	796547.450309	42.756928
3503.732766	796473.195341	42.761933
3503.991312	796427.584853	42.766938
3503.775187	796384.360130	42.771943
3503.967475	796320.051306	42.776948
3504.162389	796275.874334	42.781952
3503.926273	796222.536371	42.786957
3504.147169	796163.917566	42.791962
3504.185937	796108.863881	42.796967
3504.259794	796043.000643	42.801972
3504.139635	795985.516860	42.806977
3503.811897	795937.249788	42.811981
3503.958104	795884.926632	42.816986
3503.894818	795838.530503	42.821991
3504.153166	795771.062882	42.826996
3503.861517	795729.859991	42.832001
3503.838166	795691.215420	42.837005
3503.669600	795619.593322	42.842010
3503.589815	795584.837079	42.847015
3503.634190	795528.943060	42.852020
3503.461503	795488.652241	42.857025
3503.780956	795433.841687	42.862029
3503.951262	795378.564164	42.867034
3503.716607	795330.670470	42.872039
3503.840060	795286.106153	42.877044
3503.794164	795233.073112	42.882049
3503.419293	795180.142969	42.887053
3503.643178	795133.449318	42.892058
3503.345358	795082.863150	42.897063
3503.838637	795028.757499	42.902068
3503.742026	794996.849683	42.907073
3503.467918	794953.183668	42.912077
3503.511258	794915.800804	42.917082
3503.364034	794870.001469	42.922087
3503.672872	794816.121021	42.927092
3503.639741	794776.981885	42.932097
3503.777291	794733.050236	42.937101
3503.947790	794675.851661	42.942106
3503.551767	794630.533788	42.947111
3503.612023	794573.549005	42.952116
3503.514574	794541.933960	42.957121
3503.479514	794487.960297	42.962125
3503.852731	794438.192181	42.967130
3503.505186	794396.155673	42.972135
3503.641832	794339.745826	42.977140
3503.694426	794297.790175	42.982145
3503.673633	794248.429446	42.987149
3503.825077	794195.012241	42.992154
3503.400896	794152.446589	42.997159
3503.432181	794103.027144	43.002164
3503.479353	794085.090605	43.007169
3503.384102	794036.624813	43.012173
3503.880518	793984.278951	43.017178
3503.668592	793949.683751	43.022183
3503.789718	793897.890272	43.027188
3503.622258	793850.171907	43.032193
3503.163866	793813.013194	43.037197
3503.526114	793757.543960	43.042202
3503.301804	793712.388374	43.047207
3503.715095	793667.716948	43.052212
3503.583934	793624.461242	43.057217
3503.414306	793566.179853	43.062221
3503.304812	793529.846397	43.067226
3503.221131	793495.129592	43.072231
3503.286558	793440.247118	43.077236
3503.418117	793410.603369	43.082241
3503.373838	793359.520924	43.087245
3503.326577	793319.147891	43.092250
3503.216473	793291.557579	43.097255
3503.225563	793243.511274	43.102260
3503.280328	793209.507143	43.107265
3503.218131	793153.317060	43.112269
3503.315657	793127.018314	43.117274
3503.162153	793090.247704	43.122279
3503.112769	793038.918145	43.127284
3503.334749	793010.584255	43.132289
3502.837539	792971.315018	43.137293
3502.800715	792926.369153	43.142298
3502.902123	792897.121238	43.147303
3503.241978	792859.776882	43.152308
3503.298610	792830.437810	43.157313
3503.041743	792788.671540	43.162317
3503.171951	792761.727376	43.167322
3502.694915	792725.941610	43.172327
3502.940985	792678.048939	43.177332
3503.215445	792648.722363	43.182337
3502.776347	792603.349405	43.187341
3503.041327	792569.651479	43.192346
3503.017736	792541.798333	43.197351
3503.091196	792509.605585	43.202356
3502.962001	792471.845133	43.207361
3503.004822	792431.501318	43.212365
3503.262408	792409.005778	43.217370
3503.027738	792370.426923	43.222375
3503.025194	792326.159438	43.227380
3503.000133	792297.765120	43.232385
3502.889273	792262.850202	43.237389
3502.894804	792225.410169	43.242394
3502.910620	792201.872875	43.247399
3503.165383	792165.570663	43.252404
3503.056678	792117.290436	43.257409
3502.813850	792093.353181	43.262413
3502.970503	792047.681988	43.267418
3502.800669	792007.960392	43.272423
3502.816967	791988.254779	43.277428
3503.091364	791952.341316	43.282433
3502.787757	791914.115266	43.287437
3503.227655	791884.512601	43.292442
3502.739907	791841.501246	43.297447
3503.029310	791807.451723	43.302452
3503.029283	791791.138610	43.307457
3502.801425	791748.919192	43.312461
3502.841224	791706.311480	43.317466
3502.584449	791674.021916	43.322471
3502.704873	791643.979503	43.327476
3502.753058	791611.148052	43.332481
3502.739502	791586.335986	43.337485
3503.011405	791556.808762	43.342490
3502.760351	791527.416692	43.347495
3502.924067	791497.759629	43.352500
3503.092861	791464.317979	43.357505
3502.684449	791428.170363	43.362509
3502.783274	791385.403583	43.367514
3502.587990	791369.907879	43.372519
3502.966196	791338.150994	43.377524
3502.936136	791318.795127	43.382529
3502.436115	791298.779529	43.387533
3502.705381	791251.905316	43.392538
3502.520659	791233.115224	43.397543
3502.479131	791206.537408	43.402548
3502.848623	791169.572380	43.407553
3502.612295	791154.033824	43.412557
3502.788778	791112.038847	43.417562
3503.058209	791088.210374	43.422567
3502.652758	791030.634885	43.427572
3502.306608	791024.450926	43.432577
3502.439909	790993.469955	43.437581
3502.690926	790970.823513	43.442586
3502.285182	790935.360921	43.447591
3502.256584	790916.396847	43.452596
3502.709115	790890.621020	43.457601
3502.426143	790868.701055	43.462605
3502.538023	790844.111440	43.467610
3502.440158	790815.084318	43.472615
3502.914544	790796.921641	43.477620
3502.894618	790764.982059	43.482625
3502.738916	790726.332089	43.487629
3503.031681	790708.690535	43.492634
3502.462096	790672.221603	43.497639
3502.593295	790651.756195	43.502644
3502.683324	790618.569251	43.507649
3502.439584	790598.460311	43.512653
3502.507656	790550.484293	43.517658
3502.780398	790541.839038	43.522663
3502.598081	790509.630188	43.527668
3502.655930	790487.407181	43.532673
3502.457766	790460.311776	43.537677
3502.553241	790431.742689	43.542682
3502.266077	790409.821994	43.547687
3502.395413	790384.195859	43.552692
3502.734583	790350.327732	43.557697
3502.573439	790332.956596	43.562701
3502.869821	790299.734173	43.567706
3502.679504	790276.224436	43.572711
3502.757781	790237.385824	43.577716
3503.088533	790220.670588	43.582721
3502.796909	790189.215488	43.587725
3503.153674	790140.255357	43.592730
3502.716625	790114.918134	43.597735
3502.851179	790080.246919	43.602740
3502.795513	790045.115389	43.607745
3502.532234	790022.845528	43.612749
3502.729898	789993.717221	43.617754
3502.689818	789971.951066	43.622759
3502.730240	789937.196363	43.627764
3502.827962	789912.065220	43.632769
3502.723148	789893.405861	43.637773
3503.045603	789858.309423	43.642778
3502.772707	789840.021653	43.647783
3502.882266	789795.326705	43.652788
3502.803448	789766.439607	43.657793
3502.256356	789734.827974	43.662797
3502.503309	789701.070247	43.667802
3502.645740	789682.320458	43.672807
3502.718997	789657.929703	43.677812
3502.805537	789624.001432	43.682817
3502.349561	789599.648499	43.687821
3502.691118	789574.869209	43.692826
3502.508556	789545.801698	43.697831
3502.538319	789518.075338	43.702836
3502.401336	789498.633816	43.707841
3502.448168	789478.277232	43.712845
3502.576823	789437.066664	43.717850
3502.363992	789427.959370	43.722855
3502.504498	789392.251628	43.727860
3502.283053	789372.086386	43.732865
3502.368774	789355.851857	43.737869
3502.459128	789317.448605	43.742874
3502.430980	789311.161608	43.747879
3502.210307	789286.080699	43.752884
3502.416310	789247.412255	43.757889
3501.996877	789251.266092	43.762893
3502.423239	789198.994750	43.767898
3502.317214	789193.900165	43.772903
3502.448641	789164.779378	43.777908
3502.500285	789151.794156	43.782913
3502.190849	789134.297051	43.787917
3502.713516	789096.411249	43.792922
3502.246491	789082.774019	43.797927
3502.531844	789057.461490	43.802932
3502.370525	789047.362128	43.807937
3502.272422	789014.788546	43.812941
3502.503041	788998.283560	43.817946
3502.091149	788972.790647	43.822951
3502.322031	788958.005959	43.827956
3502.440233	788928.886386	43.832961
3502.448941	788904.552839	43.837965
3502.500921	788882.424097	43.842970
3502.402274	788862.728743	43.847975
3502.298323	788852.373874	43.852980
3502.324107	788819.434899	43.857985
3502.371356	788794.701378	43.862989
3502.650547	788778.237039	43.867994
3502.507284	788747.783409	43.872999
3502.646210	788726.524684	43.878004
3502.313048	788688.286115	43.883009
3502.222893	788697.591617	43.888013
3502.136622	788653.118386	43.893018
3502.177345	788647.556821	43.898023
3502.442241	788620.820545	43.903028
3502.432247	788586.215024	43.908033
3502.254931	788558.322405	43.913037
3502.281343	788538.605555	43.918042
3502.764305	788519.010084	43.923047
3502.370996	788482.304226	43.928052
3502.447549	788476.539991	43.933057
3502.331247	788459.648476	43.938061
3502.531113	788426.531536	43.943066
3502.328877	788419.780836	43.948071
3502.376107	788380.248979	43.953076
3502.375034	788349.721067	43.958081
3502.272391	788334.940867	43.963085
3502.449975	788305.120731	43.968090
3502.367537	788295.892187	43.973095
3502.301538	788267.783455	43.978100
3502.524875	788252.211988	43.983105
3502.258576	788222.464621	43.988109
3502.432323	788211.817278	43.993114
3502.389811	788185.916578	43.998119
3502.367448	788171.516101	44.003124
3502.579549	788136.478529	44.008129
3502.363374	788116.800472	44.013133
3502.176979	788098.592294	44.018138
3502.303992	788066.223103	44.023143
3502.247870	788053.450279	44.028148
3502.094827	788033.417461	44.033153
3501.919985	788003.408307	44.038157
3502.081195	787992.369406	44.043162
3501.756035	787993.160336	44.048167
3501.823706	787962.570282	44.053172
3501.955251	787948.094841	44.058177
3502.037963	787948.474456	44.063181
3502.300230	787923.604173	44.068186
3502.194131	787901.842565	44.073191
3502.117469	787889.564458	44.078196
3502.116609	787876.143098	44.083201
3501.896464	787851.892818	44.088205
3501.720562	787834.567172	44.093210
3501.902309	787831.833203	44.098215
3502.232815	787826.075777	44.103220
3502.136658	787797.232711	44.108225
3501.928805	787789.056599	44.113229
3502.133009	787771.520699	44.118234
3502.076766	787748.668814	44.123239
3502.180644	787731.640979	44.128244
3502.104868	787718.182499	44.133249
3501.784140	787688.638526	44.138253
3502.259168	787681.873897	44.143258
3502.448452	787671.469011	44.148263
3502.076109	787628.413111	44.153268
3502.091337	787620.101731	44.158273
3502.209565	787612.609174	44.163277
3502.302798	787581.570797	44.168282
3501.845170	787580.416994	44.173287
3502.215259	787557.690933	44.178292
3502.244104	787532.169428	44.183297
3501.710125	787521.588467	44.188301
3501.567502	787501.896597	44.193306
3501.901761	787512.117042	44.198311
3502.455523	787467.186838	44.203316
3502.233807	787459.651785	44.208321
3501.963792	787435.211640	44.213325
3502.348927	787411.843482	44.218330
3502.084728	787420.294326	44.223335
3502.291121	787390.318131	44.228340
3502.311794	787364.797374	44.233345
3502.253097	787364.561151	44.238349
3502.242240	787331.424679	44.243354
3502.444879	787315.608751	44.248359
3502.051604	787285.534225	44.253364
3502.324702	787262.823206	44.258369
3502.320353	787272.608099	44.263373
3502.323986	787235.437102	44.268378
3502.357703	787223.385504	44.273383
3502.273039	787201.077389	44.278388
3502.441969	787179.317445	44.283393
3502.088116	787165.264548	44.288397
3502.411254	787132.711322	44.293402
3502.455020	787105.759967	44.298407
3502.331828	787083.506999	44.303412
3502.253317	787074.030386	44.308417
3502.425897	787043.320782	44.313421
3502.474545	787019.072566	44.318426
3502.433709	787021.095150	44.323431
3502.120682	786983.630823	44.328436
3502.719484	786953.538994	44.333441
3502.478629	786940.302916	44.338445
3502.524558	786905.188346	44.343450
3502.332469	786894.304286	44.348455
3502.437170	786865.276866	44.353460
3502.629189	786848.773280	44.358465
3502.395696	786825.849300	44.363469
3502.320206	786789.967443	44.368474
3502.114106	786773.922624	44.373479
3502.136898	786745.842449	44.378484
3502.588820	786736.130504	44.383489
3502.531600	786705.309791	44.388493
3502.831038	786681.461662	44.393498
3502.701486	786674.058109	44.398503
3502.470925	786630.726985	44.403508
3502.571343	786613.402032	44.408513
3502.124162	786581.759933	44.413517
3502.383068	786555.951192	44.418522
3502.607139	786545.293083	44.423527
3502.158883	786511.044732	44.428532
3502.453295	786490.737195	44.433537
3502.053584	786468.134481	44.438541
3502.338617	786445.910634	44.443546
3502.146870	786449.335071	44.448551
3501.996557	786412.135983	44.453556
3502.417175	786405.379123	44.458561
3502.228236	786392.330169	44.463565
3502.177730	786352.803200	44.468570
3501.865539	786361.804099	44.473575
3502.291792	786333.803372	44.478580
3502.327712	786303.752364	44.483585
3502.214042	786301.607386	44.488589
3502.076561	786271.683153	44.493594
3501.975266	786251.440118	44.498599
3502.024858	786241.400386	44.503604
3502.315391	786217.847227	44.508609
3502.007261	786182.738260	44.513613
3502.216698	786184.965728	44.518618
3501.994941	786148.662180	44.523623
3501.845763	786152.423968	44.528628
3502.136103	786126.067582	44.533633
3501.936669	786134.460094	44.538637
3502.008514	786101.943581	44.543642
3501.999616	786074.800321	44.548647
3501.823521	786073.894938	44.553652
3502.190141	786058.540981	44.558657
3502.031820	786044.552018	44.563661
3501.914200	786014.672614	44.568666
3501.692645	786005.267322	44.573671
3501.738729	785995.817932	44.578676
3502.036373	785971.426806	44.583681
3501.616911	785967.512588	44.588685
3502.048196	785965.769506	44.593690
3502.108392	785947.318522	44.598695
3501.894084	785922.372266	44.603700
3502.143852	785909.594404	44.608705
3501.858892	785914.804796	44.613709
3502.265294	785876.478524	44.618714
3501.870265	785877.084474	44.623719
3501.511562	785861.259449	44.628724
3501.945867	785849.237909	44.633729
3501.960929	785845.252050	44.638733
3502.342817	785822.075960	44.643738
3502.038550	785820.699886	44.648743
3502.059146	785783.567737	44.653748
3502.330344	785755.098523	44.658753
3502.102151	785754.447567	44.663757
3502.219196	785741.740445	44.668762
3502.144256	785711.705216	44.673767
3501.979342	785711.289721	44.678772
3501.977335	785679.570302	44.683777
3501.820395	785672.612824	44.688781
3501.887110	785663.995626	44.693786
3501.972808	785662.456931	44.698791
3501.985639	785633.341299	44.703796
3502.231725	785613.924453	44.708801
3501.860527	785613.936357	44.713805
3501.934358	785580.040157	44.718810
3502.036203	785553.220933	44.723815
3501.812267	785550.356210	44.728820
3502.019350	785544.420581	44.733825
3501.928407	785528.206462	44.738829
3502.054215	785505.317427	44.743834
3501.904914	785505.194422	44.748839
3501.840704	785488.385661	44.753844
3501.941034	785448.386248	44.758849
3501.913553	785450.702152	44.763853
3501.599885	785439.786723	44.768858
3501.810180	785447.719109	44.773863
3501.843341	785427.549960	44.778868
3502.109301	785404.735878	44.783873
3501.739739	785404.550792	44.788877
3501.731355	785391.126014	44.793882
3501.747750	785384.631504	44.798887
3501.856765	785366.170985	44.803892
3502.018603	785346.521393	44.808897
3501.770035	785348.234403	44.813901
3501.720150	785331.226194	44.818906
3501.775801	785299.298876	44.823911
3501.847440	785306.516550	44.828916
3502.027439	785292.421211	44.833921
3501.663140	785280.677810	44.838925
3501.892010	785281.967929	44.843930
3502.098297	785263.392763	44.848935
3501.844983	785260.729485	44.853940
3501.805052	785236.784917	44.858945
3501.737523	785229.566376	44.863949
3502.009441	785188.602814	44.868954
3501.890463	785191.081416	44.873959
3501.516753	785174.863894	44.878964
3502.169878	785175.838244	44.883969
3501.888080	785165.507324	44.888973
3501.793121	785127.358004	44.893978
3501.912355	785136.584459	44.898983
3501.995453	785131.652546	44.903988
3502.254006	785093.346453	44.908993
3501.764566	785094.459833	44.913997
3501.642505	785072.938161	44.919002
3501.875326	785073.293208	44.924007
3501.735309	785033.527803	44.929012
3501.965295	785032.801308	44.934017
3501.530852	785022.101865	44.939021
3501.647806	785013.278881	44.944026
3502.050444	785024.475281	44.949031
3501.925148	784992.379675	44.954036
3501.524410	784972.477448	44.959041
3501.563898	784982.307430	44.964045
3501.894365	784969.760521	44.969050
3501.743632	784972.785438	44.974055
3501.864423	784954.076008	44.979060
3502.093689	784930.331993	44.984065
3501.703001	784932.019326	44.989069
3501.960184	784917.615441	44.994074
3501.815585	784901.408745	44.999079
3501.494890	784884.690001	45.004084
3502.004015	784884.901180	45.009089
3501.790295	784874.214342	45.014093
3501.718627	784854.208400	45.019098
3501.911625	784837.847586	45.024103
3502.019821	784819.976004	45.029108
3502.011840	784813.435810	45.034113
3502.113022	784796.253899	45.039117
3501.907396	784783.893338	45.044122
3501.768185	784780.374955	45.049127
3501.884946	784773.961730	45.054132
3501.983893	784759.190120	45.059137
3501.878387	784728.713156	45.064141
3501.913579	784719.313067	45.069146
3501.971420	784719.254295	45.074151
3501.938789	784703.471369	45.079156
3502.039362	784683.141473	45.084161
3501.515590	784671.275784	45.089165
3501.749255	784662.531517	45.094170
3501.587281	784668.902984	45.099175
3501.906783	784648.045079	45.104180
3502.091366	784622.930230	45.109185
3501.856104	784621.099885	45.114189
3501.951069	784599.491862	45.119194
3501.931624	784595.658550	45.124199
3501.973811	784580.059771	45.129204
3502.249423	784563.635540	45.134209
3502.069249	784546.105892	45.139213
3501.920424	784535.161931	45.144218
3501.745417	784501.006516	45.149223
3501.620483	784498.174247	45.154228
3501.910989	784496.650756	45.159233
3501.658273	784480.214987	45.164237
3501.371167	784456.751210	45.169242
3501.612187	784458.039479	45.174247
3501.554075	784469.460200	45.179252
3501.749722	784454.622851	45.184257
3501.920745	784465.366413	45.189261
3501.859245	784441.521122	45.194266
3501.654119	784420.257109	45.199271
3501.668419	784410.909245	45.204276
3501.894482	784402.116727	45.209281
3501.858803	784407.729822	45.214285
3501.685039	784384.886566	45.219290
3501.838438	784360.267806	45.224295
3501.273071	784362.229975	45.229300
3501.753818	784354.772684	45.234305
3501.694982	784349.371744	45.239309
3501.521229	784359.582011	45.244314
3501.425000	784353.006747	45.249319
3501.468162	784338.046714	45.254324
3501.545549	784305.767095	45.259329
3501.846381	784303.258116	45.264333
3501.584313	784301.481292	45.269338
3501.595757	784301.184223	45.274343
3501.630797	784294.784032	45.279348
3501.882815	784293.906275	45.284353
3501.903298	784274.375415	45.289357
3501.830169	784251.859473	45.294362
3501.885069	784245.505156	45.299367
3501.528391	784250.236680	45.304372
3501.681868	784229.896790	45.309377
3502.012873	784202.198588	45.314381
3501.717950	784193.835949	45.319386
3501.921465	784194.933692	45.324391
3501.500499	784191.510618	45.329396
3502.192892	784174.524970	45.334401
3501.582489	784156.917673	45.339405
3501.712390	784140.368915	45.344410
3501.933095	784144.907026	45.349415
3501.842534	784127.951857	45.354420
3502.118893	784110.395136	45.359425
3502.034013	784102.588056	45.364429
3502.089663	784092.003249	45.369434
3502.091393	784072.376553	45.374439
3502.070826	784049.556187	45.379444
3501.813522	784052.451475	45.384449
3501.589708	784059.177989	45.389453
3501.591313	784026.220954	45.394458
3501.802701	784014.085514	45.399463
3501.627857	784010.474243	45.404468
3502.160154	783997.892402	45.409473
3501.661536	783993.203097	45.414477
3501.953670	783973.085591	45.419482
3501.808621	783964.402859	45.424487
3501.924947	783954.250562	45.429492
3501.828454	783939.115946	45.434497
3502.006345	783925.116660	45.439501
3501.381401	783916.021017	45.444506
3502.069670	783895.346144	45.449511
3501.637596	783901.910348	45.454516
3501.470164	783895.051252	45.459521
3501.635307	783897.434306	45.464525
3501.708834	783880.451526	45.469530
3501.713293	783854.084722	45.474535
3501.503240	783851.364598	45.479540
3501.746260	783840.010701	45.484545
3501.861622	783853.961729	45.489549
3501.273528	783840.186829	45.494554
3501.694189	783835.149237	45.499559
3501.052262	783822.465362	45.504564
3501.573142	783796.554380	45.509569
3501.654294	783796.688525	45.514573
3501.664166	783784.438320	45.519578
3501.855391	783777.765990	45.524583
3501.699372	783774.790981	45.529588
3501.832479	783783.033071	45.534593
3502.001680	783764.607724	45.539597
3501.674534	783735.835556	45.544602
3501.287094	783735.210636	45.549607
3501.349321	783725.411267	45.554612
3501.549006	783734.429507	45.559617
3501.655630	783724.967163	45.564621
3501.743490	783710.539569	45.569626
3501.961507	783692.597911	45.574631
3501.722429	783680.585301	45.579636
3501.827885	783677.616374	45.584641
3501.921712	783675.977536	45.589645
3501.886865	783658.175826	45.594650
3501.684364	783632.285026	45.599655
3501.542009	783637.276796	45.604660
3501.985068	783624.856583	45.609665
3501.580557	783643.419310	45.614669
3501.508260	783615.244176	45.619674
3501.804629	783590.500854	45.624679
3501.669875	783570.944465	45.629684
3502.028940	783571.918300	45.634689
3501.851096	783563.240486	45.639693
3501.798396	783553.754968	45.644698
3501.756542	783537.774236	45.649703
3501.655411	783523.475783	45.654708
3501.650757	783518.409644	45.659713
3501.569754	783524.276855	45.664717
3501.596708	783525.403786	45.669722
3501.623892	783523.087194	45.674727
3501.418511	783491.785166	45.679732
3501.604061	783472.372522	45.684737
3501.785432	783476.720764	45.689741
3501.647564	783478.661940	45.694746
3501.655935	783462.820347	45.699751
3501.923664	783459.480251	45.704756
3502.022971	783443.672831	45.709761
3501.674034	783436.351262	45.714765
3501.672548	783427.299881	45.719770
3501.893161	783427.902996	45.724775
3501.514562	783434.409619	45.729780
3501.583545	783396.617665	45.734785
3501.446343	783388.916816	45.739789
3501.268152	783373.597693	45.744794
3501.601434	783373.887092	45.749799
3501.323608	783373.342470	45.754804
3501.724437	783369.193310	45.759809
3501.570489	783367.152471	45.764813
3501.614784	783339.399798	45.769818
3502.247758	783267.619579	45.774823
3501.484118	783144.167891	45.779828
3501.717209	782956.447115	45.784833
3501.512231	782733.125117	45.789837
3501.272379	782438.511425	45.794842
3501.597125	782091.392337	45.799847
3501.154620	781675.397546	45.804852
3500.967377	781214.901773	45.809857
3500.602752	780685.312679	45.814861
3500.214024	780105.095123	45.819866
3500.402182	779460.750139	45.824871
3499.771285	778754.853529	45.829876
3499.824599	777997.330499	45.834881
3498.695063	777175.622178	45.839885
3498.663799	776311.194538	45.844890
3498.432388	775367.704793	45.849895
3497.848483	774386.866389	45.854900
3498.116271	773311.076774	45.859905
3497.383853	772190.066181	45.864909
3496.921459	771003.648030	45.869914
3496.498207	769755.328730	45.874919
3495.775248	768439.711180	45.879924
3495.528509	767040.116068	45.884929
3494.738941	765602.624504	45.889933
3494.094570	764104.463280	45.894938
3493.592852	762525.864566	45.899943
3492.795545	760886.786131	45.904948
3492.227507	759187.843956	45.909953
3491.311894	757424.947795	45.914957
3490.910050	755592.333496	45.919962
3490.225197	753691.763584	45.924967
3489.323792	751743.088092	45.929972
3488.359293	749725.542788	45.934977
3487.691388	747644.009628	45.939981
3486.630651	745505.574620	45.944986
3485.995431	743289.733215	45.949991
3485.067955	741017.715000	45.954996
3484.249882	738688.122568	45.960001
3483.084733	736289.995818	45.965005
3481.797532	733830.122912	45.970010
3481.184772	731303.268739	45.975015
3480.211951	728736.697045	45.980020
3479.322605	726094.023813	45.985025
3477.995883	723378.985408	45.990029
3476.532013	720623.802418	45.995034
3475.740937	717789.264513	46.000039
3474.382390	714921.060699	46.005044
3473.463337	711971.637003	46.010049
3472.122962	708976.070393	46.015053
3470.296524	705897.170814	46.020058
3469.480845	702789.875083	46.025063
3467.726863	699616.699357	46.030068
3466.602871	696382.047912	46.035073
3465.488808	693094.821537	46.040077
3463.871746	689744.456048	46.045082
3463.098591	686334.902192	46.050087
3461.444666	682861.657469	46.055092
3459.971184	679327.277120	46.060097
3458.404359	675736.135623	46.065101
3456.763685	672085.734365	46.070106
3455.311508	668384.455950	46.075111
3453.571390	664638.821932	46.080116
3452.279443	660820.367319	46.085121
3450.611267	656958.175748	46.090125
3448.420990	653035.148558	46.095130
3447.053545	649058.956690	46.100135
3445.267449	645032.709833	46.105140
3443.689402	640943.207587	46.110145
3441.842431	636802.282685	46.115149
3439.820371	632606.473938	46.120154
3438.361626	628350.005469	46.125159
3436.214577	624058.585385	46.130164
3434.529003	619691.354388	46.135169
3432.704859	615274.318197	46.140173
3430.696843	610812.013555	46.145178
3428.594203	606296.668119	46.150183
3426.632691	601728.807796	46.155188
3424.685057	597111.631808	46.160193
3422.624632	592436.739100	46.165197
3420.574983	587732.216485	46.170202
3419.025404	582944.878731	46.175207
3416.687267	578125.575706	46.180212
3414.455068	573241.997636	46.185217
3412.415407	568320.919137	46.190221
3410.165048	563333.841513	46.195226
3408.107205	558330.279908	46.200231
3406.177243	553246.254351	46.205236
3403.998727	548108.391612	46.210241
3401.569618	542937.548424	46.215245
3399.193128	537709.204896	46.220250
3397.145176	532429.246257	46.225255
3394.643027	527123.231751	46.230260
3392.228878	521751.181970	46.235265
3389.703145	516335.382626	46.240269
3387.133318	510877.537005	46.245274
3385.163826	505371.319176	46.250279
3382.529580	499834.027253	46.255284
3379.929219	494233.988434	46.260289
3377.263776	488594.787219	46.265293
3374.820516	482930.053930	46.270298
3372.549720	477189.379698	46.275303
3369.548292	471436.669244	46.280308
3366.935930	465623.332514	46.285313
3363.982300	459785.727626	46.290317
3361.432211	453894.962467	46.295322
3358.709265	447972.439502	46.300327
3355.752003	442014.238147	46.305332
3353.246951	436004.691529	46.310337
3350.503003	429971.945472	46.315341
3347.685418	423897.809452	46.320346
3344.965643	417786.876465	46.325351
3341.829160	411636.595343	46.330356
3339.248585	405444.397928	46.335361
3336.400281	399224.984453	46.340365
3333.143963	392960.783521	46.345370
3330.474323	386670.397834	46.350375
3326.992627	380358.731208	46.355380
3324.182777	373988.184866	46.360385
3321.399985	367607.091335	46.365389
3317.875513	361197.220137	46.370394
3314.881991	354752.688441	46.375399
3311.781986	348270.343643	46.380404
3308.923345	341749.186717	46.385409
3305.458384	335211.450287	46.390413
3302.267300	328641.881413	46.395418
3298.748477	322067.748976	46.400423
3295.527399	315450.295430	46.405428
3292.389882	308815.050341	46.410433
3288.923482	302166.961264	46.415437
3285.696795	295483.340313	46.420442
3282.052027	288785.295100	46.425447
3278.660032	282073.677678	46.430452
3275.325421	275326.435722	46.435457
3271.966179	268572.484445	46.440461
3268.255658	261800.313591	46.445466
3265.180039	254999.776176	46.450471
3261.128228	248179.237168	46.455476
3257.629795	241354.108852	46.460481
3253.716897	234524.603314	46.465485
3250.248265	227680.522369	46.470490
3246.727515	220809.551260	46.475495
3242.856045	213950.881568	46.480500
3239.455562	206979.588232	46.485505
3235.711016	200074.358005	46.490509
3231.732297	193177.364218	46.495514
3228.089192	186250.223096	46.500519
3223.670039	179351.702302	46.505524
3219.905037	172425.632836	46.510529
3215.887150	165499.695166	46.515533
3211.543504	158586.154362	46.520538
3207.595754	151663.070354	46.525543
3203.399217	144757.194748	46.530548
3198.861433	137845.887667	46.535553
3194.808587	130953.332549	46.540557
3190.094153	124056.168659	46.545562
3185.702135	117179.735941	46.550567
3181.165427	110311.567615	46.555572
3176.625362	103470.879672	46.560577
3171.819459	96647.956774	46.565581
3166.684323	89849.028992	46.570586
3161.909691	83072.595638	46.575591
3156.695024	76327.147563	46.580596
3151.649525	69612.114465	46.585601
3146.119843	62939.907733	46.590605
3140.051559	56309.392754	46.595610
3133.977812	49716.810585	46.600615
3126.580421	43236.977869	46.605620
3112.804216	36980.348307	46.610625
3093.383704	31012.493650	46.615629
3073.844609	25278.993202	46.620634
3055.149669	19807.495267	46.625639
3035.529299	14687.265296	46.630644
3013.194255	9996.652785	46.635649
2979.531547	6022.242163	46.640653
2940.605862	2690.832962	46.645658
2886.367383	465.728242	46.650663
2788.774636	303.209012	46.655668
2733.939311	306.575095	46.660673
2726.873610	301.368041	46.665677
2750.480684	304.644315	46.670682
2785.165816	276.398360	46.675687
2815.448972	280.872554	46.680692
2834.369026	286.704642	46.685697
2842.138498	273.674906	46.690701
2841.075421	280.746577	46.695706
2836.584163	281.082422	46.700711
2830.459030	283.738652	46.705716
2824.934212	276.557860	46.710721
2820.797510	269.586082	46.715725
2817.183761	278.402357	46.720730
2815.038908	274.671008	46.725735
2812.784249	281.208256	46.730740
2810.742275	268.750613	46.735745
2808.572591	264.710218	46.740749
2805.610616	263.383041	46.745754
2802.559616	265.728526	46.750759
2799.231778	262.350265	46.755764
2796.283199	264.583858	46.760769
2793.272934	251.975782	46.765773
2789.824110	257.262471	46.770778
2787.377027	246.644939	46.775783
2783.768678	261.848398	46.780788
2779.924410	256.263240	46.785793
2776.972104	247.687189	46.790797
2773.872624	255.891252	46.795802
2770.953107	240.589348	46.800807
2767.498273	241.522228	46.805812
2764.186399	243.789185	46.810817
2761.236923	251.289450	46.815821
2757.715455	249.389968	46.820826
2754.626915	264.723211	46.825831
2750.932578	240.024024	46.830836
2747.661891	249.270729	46.835841
2744.675167	248.545729	46.840845
2740.879614	242.540270	46.845850
2737.953506	253.137737	46.850855
2734.301406	247.715875	46.855860
2730.391089	250.375515	46.860865
2727.392154	241.465917	46.865869
2723.667838	238.291580	46.870874
2720.662558	253.641974	46.875879
2717.254492	236.288631	46.880884
2713.828413	237.344358	46.885889
2710.292549	230.778640	46.890893
2707.137594	240.367561	46.895898
2703.937046	232.354387	46.900903
2700.437612	229.120888	46.905908
2696.569767	232.611250	46.910913
2693.392809	234.996776	46.915917
2689.451483	227.249000	46.920922
2687.001443	231.963783	46.925927
2683.265877	229.905774	46.930932
2679.455190	230.116872	46.935937
2676.365133	226.566875	46.940941
2672.655830	240.606836	46.945946
2668.774698	237.437862	46.950951
2665.915143	243.979063	46.955956
2662.437395	241.521310	46.960961
2659.045860	238.871562	46.965965
2655.455572	232.430276	46.970970
2652.334525	223.666156	46.975975
2649.422558	237.903290	46.980980
2645.257820	235.460257	46.985985
2641.655227	235.007226	46.990989
2638.108053	230.992753	46.995994
2635.038489	227.189393	47.000999
2631.120903	223.875999	47.006004
2627.734833	226.626239	47.011009
2624.673749	229.761335	47.016013
2621.071214	228.287681	47.021018
2618.032491	217.397626	47.026023
2614.251564	226.692875	47.031028
2610.654812	219.995285	47.036033
2607.439798	219.433574	47.041037
2603.064737	232.551454	47.046042
2600.014048	219.865325	47.051047
2597.065730	225.813635	47.056052
2593.213089	222.974855	47.061057
2589.956823	230.760555	47.066061
2586.197118	228.894421	47.071066
2582.866705	222.647306	47.076071
2579.148607	230.593217	47.081076
2575.656471	221.713922	47.086081
2572.793507	210.563561	47.091085
2568.606292	219.474257	47.096090
2565.307184	211.299040	47.101095
2562.117124	219.829551	47.106100
2558.601190	219.847375	47.111105
2555.170019	211.776418	47.116109
2551.400148	217.852315	47.121114
2548.074126	227.560644	47.126119
2544.566603	224.937181	47.131124
2540.757174	221.077882	47.136129
2537.605470	222.363009	47.141133
2534.016841	231.431338	47.146138
2530.955954	218.743673	47.151143
2527.312888	227.363105	47.156148
2523.606561	231.524429	47.161153
2520.357681	213.882555	47.166157
2516.876246	226.955322	47.171162
2513.902602	233.391067	47.176167
2510.312194	226.899368	47.181172
2506.287496	220.682030	47.186177
2502.849279	212.391662	47.191181
2498.885934	226.108424	47.196186
2495.540404	221.810576	47.201191
2492.191039	224.969777	47.206196
2488.836714	225.918957	47.211201
2485.315462	220.788014	47.216205
2481.818604	217.379475	47.221210
2478.475052	228.550075	47.226215
2475.053334	212.364518	47.231220
2471.153995	220.170661	47.236225
2468.293729	220.996943	47.241229
2464.568753	224.279163	47.246234
2461.371212	214.509700	47.251239
2457.880529	214.125517	47.256244
2453.672982	216.386981	47.261249
2450.594721	207.805339	47.266253
2446.733965	205.272636	47.271258
2443.400374	199.806118	47.276263
2439.829947	206.051418	47.281268
2436.344488	214.969079	47.286273
2432.975024	216.075575	47.291277
2429.375947	230.169253	47.296282
2425.780654	215.593941	47.301287
2422.760923	213.684496	47.306292
2419.059039	219.028933	47.311297
2415.826075	204.820288	47.316301
2412.287835	204.135070	47.321306
2408.644977	206.323067	47.326311
2404.974809	204.890864	47.331316
2401.355409	201.071934	47.336321
2398.445749	201.164772	47.341325
2394.840643	214.709916	47.346330
2391.065881	208.629809	47.351335
2387.661704	208.405328	47.356340
2383.695035	203.699220	47.361345
2380.697485	204.131737	47.366349
2377.187770	197.174862	47.371354
2373.954279	207.430132	47.376359
2370.266481	203.222340	47.381364
2366.419160	194.854199	47.386369
2363.336768	199.414959	47.391373
2359.622748	200.963570	47.396378
2356.129148	201.628159	47.401383
2352.892559	206.842215	47.406388
2348.866425	200.254065	47.411393
2345.731876	183.782606	47.416397
2342.052063	203.941590	47.421402
2338.779155	189.431482	47.426407
2335.361410	202.461029	47.431412
2331.578937	203.323724	47.436417
2328.019618	198.069018	47.441421
2324.686983	195.268148	47.446426
2321.224461	202.729616	47.451431
2317.890825	192.676058	47.456436
2314.230715	202.354407	47.461441
2310.992519	198.274353	47.466445
2307.023519	198.748131	47.471450
2303.666862	201.832640	47.476455
2300.118463	191.654588	47.481460
2296.754553	196.829873	47.486465
2293.565560	189.114155	47.491469
2289.542684	208.458983	47.496474
2285.998644	205.197533	47.501479
2282.595801	195.143174	47.506484
2279.278723	202.930808	47.511489
2276.215884	193.425843	47.516493
2272.338621	209.441221	47.521498
2268.601620	194.651634	47.526503
2265.094482	200.877389	47.531508
2261.735131	201.205457	47.536513
2258.406509	196.096343	47.541517
2254.547788	197.134832	47.546522
2251.700007	200.502145	47.551527
2248.104478	196.261049	47.556532
2244.370231	204.215073	47.561537
2240.987511	201.420628	47.566541
2237.058492	197.223096	47.571546
2233.671074	195.498489	47.576551
2230.106062	199.800204	47.581556
2226.469911	202.336723	47.586561
2223.699570	190.354483	47.591565
2219.788590	204.132840	47.596570
2216.403040	197.864530	47.601575
2212.750976	191.642748	47.606580
2209.166426	197.320914	47.611585
2205.707914	186.486719	47.616589
2201.766192	205.609031	47.621594
2198.737105	194.613734	47.626599
2195.449437	188.788646	47.631604
2191.714684	188.648870	47.636609
2188.291743	194.988233	47.641613
2184.409774	186.924558	47.646618
2181.454623	184.779628	47.651623
2178.309532	183.460815	47.656628
2174.456097	190.363293	47.661633
2170.978590	183.091340	47.666637
2167.275313	179.658018	47.671642
2163.570774	182.645858	47.676647
2160.165514	185.418296	47.681652
2156.842579	190.466217	47.686657
2153.548059	193.625877	47.691661
2149.808593	194.525866	47.696666
2146.219803	183.012034	47.701671
2142.769808	185.904130	47.706676
2139.221299	194.259284	47.711681
2136.284604	185.240592	47.716685
2132.364150	188.820197	47.721690
2128.681061	187.962580	47.726695
2125.250710	188.710469	47.731700
2121.639015	184.329747	47.736705
2118.509067	171.749829	47.741709
2114.509966	180.563779	47.746714
2111.434792	173.276111	47.751719
2108.102489	181.706992	47.756724
2104.087217	182.952713	47.761729
2100.738483	183.060871	47.766733
2097.156656	186.814311	47.771738
2093.459560	187.820795	47.776743
2090.226451	181.265476	47.781748
2086.824136	186.064680	47.786753
2083.712208	186.236387	47.791757
2079.975657	186.161881	47.796762
2076.130735	191.699252	47.801767
2072.894175	191.445292	47.806772
2069.389297	185.817010	47.811777
2065.663769	188.876039	47.816781
2062.025230	183.510929	47.821786
2058.693624	177.501668	47.826791
2055.257092	172.605216	47.831796
2051.885828	182.154318	47.836801
2048.304823	175.279045	47.841805
2044.364223	184.564828	47.846810
2041.397993	182.076877	47.851815
2037.596309	181.936972	47.856820
2034.453466	181.702496	47.861825
2031.035884	173.856219	47.866829
2027.411716	179.849692	47.871834
2023.854090	181.968557	47.876839
2020.457432	172.502821	47.881844
2016.421555	184.087469	47.886849
2013.202024	175.561632	47.891853
2009.546674	178.445336	47.896858
2006.346749	177.953518	47.901863
2003.259926	161.035488	47.906868
1999.129953	182.354624	47.911873
1996.144878	177.024020	47.916877
1991.854331	179.862658	47.921882
1988.610671	168.993554	47.926887
1985.335780	165.361903	47.931892
1982.015198	170.774730	47.936897
1978.298563	178.830920	47.941901
1974.545019	164.362063	47.946906
1971.364874	171.823340	47.951911
1967.841806	167.283354	47.956916
1964.108137	178.747330	47.961921
1960.967604	176.098944	47.966925
1957.380462	178.389044	47.971930
1953.709530	173.273422	47.976935
1950.221971	165.725635	47.981940
1946.534644	166.174643	47.986945
1943.183805	173.435599	47.991949
1939.442774	173.823622	47.996954
1936.323717	180.452624	48.001959
1932.571667	165.848880	48.006964
1928.785278	167.587120	48.011969
1925.740811	173.128549	48.016973
1922.424956	173.438446	48.021978
1919.069231	160.022187	48.026983
1915.474822	164.352262	48.031988
1911.805843	184.875178	48.036993
1908.460368	169.033602	48.041997
1904.810312	174.592568	48.047002
1901.185225	177.709786	48.052007
1897.862237	170.059797	48.057012
1893.744795	174.136594	48.062017
1890.552563	166.625258	48.067021
1887.353967	175.447138	48.072026
1883.791811	167.665247	48.077031
1880.194309	166.993519	48.082036
1876.593959	165.431484	48.087041
1873.354577	168.135043	48.092045
1869.759063	175.558236	48.097050
1866.444264	159.844133	48.102055
1863.054278	171.737033	48.107060
1858.946627	174.019132	48.112065
1855.404155	173.499544	48.117069
1851.961489	176.708333	48.122074
1848.558206	162.780725	48.127079
1845.425574	159.825845	48.132084
1842.006649	174.455255	48.137089
1838.407642	166.461142	48.142093
1834.668832	179.498912	48.147098
1830.932069	170.953441	48.152103
1827.657649	184.512859	48.157108
1823.861811	173.512671	48.162113
1820.791064	175.342836	48.167117
1817.349195	174.241854	48.172122
1813.825001	175.365864	48.177127
1810.560204	166.444296	48.182132
1806.671112	172.267288	48.187137
1803.242051	175.435081	48.192141
1799.421501	176.739504	48.197146
1796.238772	170.572138	48.202151
1792.545492	165.858576	48.207156
1788.792934	186.519727	48.212161
1785.838222	164.290307	48.217165
1782.249725	177.815821	48.222170
1778.692448	166.201627	48.227175
1775.190679	159.529107	48.232180
1771.335870	174.289356	48.237185
1768.138540	165.486021	48.242189
1764.746958	174.310877	48.247194
1761.354936	171.744626	48.252199
1757.876862	178.698317	48.257204
1754.136130	179.477167	48.262209
1750.526225	172.478380	48.267213
1746.932302	180.566611	48.272218
1743.585276	171.335542	48.277223
1740.099317	166.214088	48.282228
1736.181990	170.779253	48.287233
1733.122904	169.284750	48.292237
1729.718136	161.673113	48.297242
1726.306715	169.711404	48.302247
1722.477375	163.644555	48.307252
1719.050359	169.531438	48.312257
1716.065313	171.680572	48.317261
1712.316462	169.429240	48.322266
1708.361469	169.791715	48.327271
1705.322263	155.148946	48.332276
1701.570292	169.552374	48.337281
1698.027867	164.739586	48.342285
1694.330315	170.615476	48.347290
1690.749379	156.389744	48.352295
1687.710607	164.553613	48.357300
1684.002273	165.366418	48.362305
1680.791464	161.174626	48.367309
1677.457686	165.202432	48.372314
1673.509901	163.615354	48.377319
1670.392440	161.376376	48.382324
1666.566047	174.701347	48.387329
1662.838424	155.374493	48.392333
1659.604730	161.740246	48.397338
1655.783394	160.433810	48.402343
1652.812613	155.679740	48.407348
1648.984361	174.564555	48.412353
1645.770480	164.478809	48.417357
1642.052914	162.826729	48.422362
1638.192884	169.406441	48.427367
1635.063116	163.184447	48.432372
1631.197219	172.368104	48.437377
1628.096214	163.605777	48.442381
1624.439801	173.678597	48.447386
1621.091213	172.226983	48.452391
1617.686206	157.361775	48.457396
1614.240441	169.288529	48.462401
1611.013588	158.741456	48.467405
1607.020296	168.748128	48.472410
1603.458972	165.424288	48.477415
1600.143113	148.752873	48.482420
1596.464045	158.398993	48.487425
1593.360242	151.096392	48.492429
1589.461151	155.177565	48.497434
1585.814219	150.396987	48.502439
1582.380589	143.101172	48.507444
1578.739245	146.717070	48.512449
1575.439716	145.960908	48.517453
1572.103396	148.705055	48.522458
1568.370450	148.971179	48.527463
1565.014867	151.518235	48.532468
1561.163507	158.502127	48.537473
1558.107309	156.858945	48.542477
1554.664932	161.457796	48.547482
1550.422861	163.337922	48.552487
1547.588374	156.109089	48.557492
1543.872000	168.137351	48.562497
1540.406160	152.357228	48.567501
1537.160758	164.233577	48.572506
1533.489986	156.608729	48.577511
1530.227476	154.409244	48.582516
1526.353629	168.476203	48.587521
1522.706153	164.152134	48.592525
1518.904633	162.594578	48.597530
1515.918326	163.935109	48.602535
1513.053461	156.956567	48.607540
1509.128735	165.498255	48.612545
1505.689592	162.698892	48.617549
1501.923081	162.091653	48.622554
1497.946861	162.960603	48.627559
1494.779972	155.975383	48.632564
1490.903916	159.453070	48.637569
1488.176801	164.394736	48.642573
1484.571423	158.790079	48.647578
1480.763314	152.545945	48.652583
1477.733101	151.798460	48.657588
1473.911089	158.485920	48.662593
1470.336735	151.151137	48.667597
1467.004965	158.751365	48.672602
1463.367787	164.138711	48.677607
1459.913710	156.147743	48.682612
1456.353193	164.351726	48.687617
1453.061496	153.251129	48.692621
1449.223638	165.231996	48.697626
1445.944112	162.885497	48.702631
1442.558289	148.963070	48.707636
1438.143453	164.179513	48.712641
1435.163687	148.193257	48.717645
1432.105907	154.570413	48.722650
1428.459079	149.156036	48.727655
1425.394528	147.973542	48.732660
1421.072015	149.909244	48.737665
1417.951672	151.199719	48.742669
1414.584530	144.649132	48.747674
1410.903060	142.312365	48.752679
1407.680034	143.471511	48.757684
1403.468689	148.064252	48.762689
1400.314549	135.816308	48.767693
1396.564623	150.107421	48.772698
1392.957444	157.213875	48.777703
1389.998649	143.220217	48.782708
1386.432523	150.168555	48.787713
1382.815185	142.383056	48.792717
1379.349579	148.549328	48.797722
1375.732340	154.244979	48.802727
1372.296812	139.301521	48.807732
1368.732418	147.380385	48.812737
1365.477506	149.998817	48.817741
1361.838679	136.639316	48.822746
1357.985101	157.449731	48.827751
1354.702130	149.886676	48.832756
1351.523880	166.019407	48.837761
1348.162038	150.954677	48.842765
1344.366117	151.821675	48.847770
1340.598381	157.320304	48.852775
1337.318249	148.838493	48.857780
1333.479337	156.589370	48.862785
1330.243221	149.217488	48.867789
1326.964466	149.058145	48.872794
1323.605273	153.975248	48.877799
1319.786218	151.359448	48.882804
1315.843713	163.956291	48.887809
1312.847173	156.939893	48.892813
1309.473387	160.773989	48.897818
1305.937890	161.191557	48.902823
1302.291336	151.296313	48.907828
1298.576326	154.850908	48.912833
1295.266023	156.186802	48.917837
1291.808828	159.763466	48.922842
1287.721465	156.807900	48.927847
1284.591120	152.752887	48.932852
1281.032200	156.348911	48.937857
1278.055851	152.389929	48.942861
1274.691735	152.697437	48.947866
1271.112768	155.832102	48.952871
1267.588812	143.464633	48.957876
1263.656435	150.995474	48.962881
1260.266835	134.315850	48.967885
1256.518886	148.037440	48.972890
1252.681061	148.145336	48.977895
1250.030965	143.325010	48.982900
1246.124629	150.836368	48.987905
1242.717452	141.241922	48.992909
1239.339717	148.447600	48.997914
1235.484188	145.618063	49.002919
1231.975544	149.333374	49.007924
1228.505395	149.071696	49.012929
1225.221556	151.791946	49.017933
1221.896335	148.623303	49.022938
1218.113410	160.414752	49.027943
1214.794853	150.722224	49.032948
1211.477952	149.849829	49.037953
1207.714993	150.342879	49.042957
1204.186066	141.186957	49.047962
1200.270414	149.117487	49.052967
1197.060320	142.470360	49.057972
1193.663283	155.866892	49.062977
1190.336138	147.216133	49.067981
1186.798908	148.605026	49.072986
1182.925001	146.017501	49.077991
1179.718717	147.236930	49.082996
1176.094295	148.063278	49.088001
1172.807187	145.195093	49.093005
1169.213055	141.092000	49.098010
1165.525218	135.502433	49.103015
1162.218034	140.254151	49.108020
1158.477552	149.204800	49.113025
1154.948439	151.303585	49.118029
1151.588058	153.706694	49.123034
1147.654146	154.194454	49.128039
1144.610953	153.740199	49.133044
1141.136272	147.254674	49.138049
1137.977775	139.144765	49.143053
1134.362037	148.977736	49.148058
1130.560806	137.961164	49.153063
1127.131306	143.957616	49.158068
1123.568113	143.320968	49.163073
1119.840411	141.218807	49.168077
1116.454217	145.428451	49.173082
1113.084937	149.768688	49.178087
1109.883350	137.957804	49.183092
1106.359269	139.375643	49.188097
1102.750659	140.202970	49.193101
1099.020254	148.001647	49.198106
1095.309155	146.554501	49.203111
1092.027768	145.664661	49.208116
1088.134094	151.843819	49.213121
1085.104967	140.632228	49.218125
1081.688361	153.942942	49.223130
1078.140345	149.838204	49.228135
1074.690455	140.029428	49.233140
1070.945468	147.584574	49.238145
1067.660296	153.606655	49.243149
1064.231559	147.816122	49.248154
1060.853059	153.390027	49.253159
1057.106930	147.895481	49.258164
1053.309175	152.448846	49.263169
1050.126826	140.093294	49.268173
1046.436698	142.117789	49.273178
1042.757823	140.037800	49.278183
1039.602970	141.138996	49.283188
1035.913161	140.454338	49.288193
1032.420038	138.112339	49.293197
1029.095157	138.881022	49.298202
1025.333339	143.770212	49.303207
1021.772461	138.138459	49.308212
1018.218594	142.510988	49.313217
1015.109038	146.340953	49.318221
1012.030529	128.378910	49.323226
1008.035977	140.420642	49.328231
1004.700206	142.368304	49.333236
1000.804362	141.497087	49.338241
997.228838	134.619073	49.343245
993.775019	134.645659	49.348250
990.639533	139.004272	49.353255
986.961541	130.487830	49.358260
983.308033	144.286769	49.363265
980.151019	136.518845	49.368269
976.699974	137.506486	49.373274
972.934107	153.297016	49.378279
969.468350	141.698927	49.383284
965.934600	147.661659	49.388289
962.369905	137.324859	49.393293
959.293143	132.562089	49.398298
955.241569	150.642649	49.403303
951.809626	140.103097	49.408308
948.417656	138.796710	49.413313
944.795122	134.774008	49.418317
941.559905	135.532368	49.423322
937.375145	136.869564	49.428327
934.293300	135.675551	49.433332
930.607866	132.722418	49.438337
927.607894	129.256253	49.443341
923.962837	130.382109	49.448346
920.011721	133.028973	49.453351
916.816680	129.845215	49.458356
913.501804	147.171465	49.463361
910.274896	131.263152	49.468365
906.950825	138.201427	49.473370
902.898954	143.047610	49.478375
899.340273	129.417406	49.483380
895.710851	126.659659	49.488385
892.275253	144.595613	49.493389
889.067457	131.565119	49.498394
885.122312	138.546071	49.503399
881.851983	128.214688	49.508404
878.270358	133.831974	49.513409
875.161493	137.380909	49.518413
871.640001	133.295197	49.523418
867.784401	135.243421	49.528423
864.562962	137.652133	49.533428
861.063089	135.408814	49.538433
857.142588	133.563577	49.543437
853.877662	138.750531	49.548442
850.075741	144.357743	49.553447
846.991459	135.609670	49.558452
842.993079	141.444172	49.563457
839.895177	140.074878	49.568461
836.103622	132.204342	49.573466
832.618878	133.693664	49.578471
829.554499	129.686990	49.583476
826.047324	137.345043	49.588481
822.088606	145.782168	49.593485
818.959522	137.472833	49.598490
815.396868	137.620677	49.603495
812.011479	128.008104	49.608500
808.306760	137.906315	49.613505
804.854482	131.077621	49.618509
801.481077	136.280438	49.623514
797.423762	145.128087	49.628519
794.333725	125.882010	49.633524
790.772154	142.288811	49.638529
787.444999	142.823383	49.643533
783.926728	137.379383	49.648538
780.085308	132.986658	49.653543
776.701042	127.530402	49.658548
773.315763	133.314205	49.663553
769.733635	138.472481	49.668557
766.345053	126.580916	49.673562
762.501623	134.633605	49.678567
759.149576	124.418987	49.683572
755.834780	141.086639	49.688577
752.059615	132.163553	49.693581
748.526248	136.449165	49.698586
745.418227	134.908151	49.703591
742.123903	129.919292	49.708596
738.550648	129.020411	49.713601
734.475277	134.032757	49.718605
731.247048	127.790712	49.723610
727.475026	125.488823	49.728615
724.125039	128.874015	49.733620
720.377465	130.729601	49.738625
717.037089	132.884153	49.743629
713.854975	125.111156	49.748634
710.277842	136.741753	49.753639
706.952440	133.947321	49.758644
703.287885	130.260621	49.763649
699.407418	136.092990	49.768653
696.010154	136.749779	49.773658
692.501552	136.460397	49.778663
689.419386	129.762238	49.783668
685.674479	137.848319	49.788673
682.239320	137.143310	49.793677
678.618457	138.766080	49.798682
674.907368	129.563331	49.803687
671.610174	130.499968	49.808692
668.067705	134.455342	49.813697
664.778429	122.955979	49.818701
661.316560	118.572569	49.823706
657.477366	129.052726	49.828711
654.143512	129.264386	49.833716
650.493093	127.149242	49.838721
647.142200	138.829121	49.843725
643.854747	130.457550	49.848730
640.185003	127.729201	49.853735
637.067608	126.742756	49.858740
633.080790	126.627590	49.863745
629.192053	133.171585	49.868749
625.960532	132.054628	49.873754
622.337443	127.984755	49.878759
619.253089	118.528878	49.883764
615.917892	129.582567	49.888769
612.330589	129.502059	49.893773
608.865854	121.798689	49.898778
605.042387	139.976866	49.903783
601.330500	137.608686	49.908788
598.127976	130.772408	49.913793
594.715157	130.070169	49.918797
591.231566	128.936163	49.923802
587.269150	133.764489	49.928807
583.855411	123.912174	49.933812
580.437690	136.827040	49.938817
577.150788	130.532322	49.943821
573.582134	121.977078	49.948826
569.978093	124.147428	49.953831
566.695607	115.946949	49.958836
563.140977	114.770630	49.963841
559.783900	120.355317	49.968845
556.252789	120.530055	49.973850
552.135199	127.681328	49.978855
548.936148	116.989238	49.983860
545.481541	120.516198	49.988865
542.031049	131.340841	49.993869
538.623447	121.082264	49.998874
535.085408	132.740116	50.003879
531.520495	122.254869	50.008884
527.633203	123.089070	50.013889
524.328217	121.451066	50.018893
521.360522	119.653664	50.023898
517.508468	120.829122	50.028903
514.141755	119.045443	50.033908
510.775328	133.229551	50.038913
506.933933	131.722480	50.043917
503.548196	123.602820	50.048922
499.998160	130.893894	50.053927
496.445466	133.374165	50.058932
492.928722	116.653640	50.063937
489.377390	121.771347	50.068941
486.092740	117.934914	50.073946
482.184926	122.038628	50.078951
479.071334	123.833625	50.083956
475.387738	120.480409	50.088961
471.514227	136.894058	50.093965
468.607304	123.348480	50.098970
465.102490	129.372365	50.103975
461.657862	128.991741	50.108980
458.027983	127.898941	50.113985
454.427734	126.442438	50.118989
450.962788	132.253258	50.123994
447.246247	131.818015	50.128999
444.007864	124.934180	50.134004
440.414576	130.636079	50.139009
436.763251	126.627216	50.144013
433.394885	127.860842	50.149018
429.949412	122.071380	50.154023
426.791658	117.479822	50.159028
423.122965	119.466085	50.164033
419.361849	128.077744	50.169037
416.133518	121.469094	50.174042
412.488512	129.763046	50.179047
409.060149	124.889154	50.184052
405.209609	119.015777	50.189057
401.777400	125.623084	50.194061
398.206160	115.569015	50.199066
394.680716	124.396876	50.204071
391.137293	121.929470	50.209076
387.922244	130.190685	50.214081
384.355371	128.016611	50.219085
380.941614	122.638857	50.224090
377.226356	132.812674	50.229095
374.049041	126.777588	50.234100
370.446901	129.302693	50.239105
366.940873	125.237018	50.244109
363.580029	129.639736	50.249114
359.982675	132.915418	50.254119
356.321691	127.337010	50.259124
352.669125	128.922276	50.264129
349.237694	143.950930	50.269133
345.584672	129.218134	50.274138
342.000920	141.522814	50.279143
339.056123	117.543833	50.284148
335.253811	123.399982	50.289153
331.923215	132.099399	50.294157
328.463061	127.430977	50.299162
324.889014	123.985960	50.304167
321.231303	120.990924	50.309172
317.745323	129.287554	50.314177
314.033157	119.006432	50.319181
310.730876	125.984373	50.324186
307.431519	122.563340	50.329191
304.237253	121.544574	50.334196
300.637478	125.300349	50.339201
296.917297	129.971121	50.344205
293.273131	118.867239	50.349210
289.428906	125.634022	50.354215
286.261783	129.972314	50.359220
282.539802	123.807362	50.364225
278.893476	120.280197	50.369229
275.888618	116.532419	50.374234
272.531273	133.067454	50.379239
269.358355	121.135356	50.384244
265.216072	115.955579	50.389249
261.526148	113.949398	50.394253
258.213940	115.827329	50.399258
254.865754	119.977223	50.404263
251.309741	116.793866	50.409268
247.922141	119.917648	50.414273
244.360237	120.456552	50.419277
241.026289	118.451453	50.424282
236.808067	115.471237	50.429287
233.611521	109.093429	50.434292
230.259530	119.433505	50.439297
226.432748	126.843632	50.444301
223.050946	126.730078	50.449306
219.683702	130.187816	50.454311
216.074339	124.096345	50.459316
212.684244	112.296361	50.464321
209.477723	119.179302	50.469325
206.322377	118.168066	50.474330
202.507916	125.604089	50.479335
198.778607	116.133968	50.484340
195.020697	114.076217	50.489345
191.466096	114.506705	50.494349
188.359628	96.099406	50.499354
184.457027	122.539173	50.504359
180.991871	107.730788	50.509364
177.834487	102.008916	50.514369
174.095822	123.499988	50.519373
170.354243	108.382319	50.524378
166.883136	123.130984	50.529383
163.933894	116.309442	50.534388
160.316591	123.434702	50.539393
156.492129	130.707748	50.544397
153.020698	119.907988	50.549402
149.584048	123.817527	50.554407
146.065837	115.224533	50.559412
142.733764	118.769133	50.564417
138.736970	121.462371	50.569421
135.500947	121.293600	50.574426
132.275104	101.970015	50.579431
128.796869	112.767735	50.584436
125.213075	110.774881	50.589441
122.072986	111.061148	50.594445
118.615261	111.831912	50.599450
114.780373	123.593444	50.604455
111.192935	119.605993	50.609460
107.548904	108.693024	50.614465
103.787782	114.293777	50.619469
100.566783	115.984464	50.624474
96.989682	112.740163	50.629479
93.491383	115.197350	50.634484
89.664728	108.981853	50.639489
86.418549	127.556231	50.644493
83.319134	118.014463	50.649498
79.464946	114.656828	50.654503
76.245398	106.571639	50.659508
72.686870	118.697334	50.664513
69.029000	121.106517	50.669517
65.828896	110.325619	50.674522
62.018245	127.047208	50.679527
58.526470	113.083056	50.684532
55.270289	110.115752	50.689537
51.374649	111.261986	50.694541
47.944475	115.862471	50.699546
44.501384	108.585132	50.704551
41.071265	104.073918	50.709556
37.399524	111.662438	50.714561
33.733927	115.161478	50.719565
30.715985	116.569145	50.724570
26.863764	121.639728	50.729575
23.628855	118.934011	50.734580
20.309954	121.207295	50.739585
16.533744	118.234394	50.744589
12.952130	114.688116	50.749594
9.455765	128.364298	50.754599
6.228706	127.344592	50.759604
2.680764	102.433716	50.764609