Thu Jun 16 19:04:14 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.768924	110.934135	0.000000
-0.323284	114.136204	0.005005
-0.413346	107.487971	0.010010
-0.516712	109.525574	0.015014
-0.629027	93.255728	0.020019
-0.923410	88.991827	0.025024
-1.003722	74.264710	0.030029
-1.379214	63.197356	0.035034
-1.837924	58.722269	0.040038
-1.930464	49.137909	0.045043
-2.020987	44.784296	0.050048
-2.241308	22.951766	0.055053
-3.023254	7.933415	0.060058
-2.786311	7.715854	0.065062
-3.542781	-0.965870	0.070067
-3.839732	-4.836478	0.075072
-3.919205	-1.713988	0.080077
-4.465127	0.090806	0.085082
-4.984793	-15.895158	0.090086
-5.119203	-1.231966	0.095091
-5.631852	-7.772529	0.100096
-5.583408	-3.125460	0.105101
-5.421023	-0.318184	0.110106
-5.712883	-7.117601	0.115110
-6.439470	-2.105091	0.120115
-6.925607	1.537327	0.125120
-7.049525	5.724049	0.130125
-7.284498	1.322005	0.135130
-7.208800	-4.098882	0.140134
-7.152718	-7.519857	0.145139
-7.693801	0.671229	0.150144
-7.915487	0.994023	0.155149
-8.639763	6.979973	0.160154
-8.581202	5.535524	0.165158
-8.766622	14.005537	0.170163
-9.138776	8.105203	0.175168
-8.952311	-1.677554	0.180173
-9.585662	13.445754	0.185178
-9.916083	-2.150242	0.190182
-10.035284	0.308653	0.195187
-10.316589	-2.394794	0.200192
-10.223084	-3.251511	0.205197
-11.095175	-1.758330	0.210202
-11.382877	-2.732884	0.215206
-11.789890	11.373182	0.220211
-11.857834	2.450904	0.225216
-11.875852	-6.600077	0.230221
-11.912293	3.341603	0.235226
-11.926325	-2.188268	0.240230
-11.708220	-0.648540	0.245235
-12.725751	-4.695636	0.250240
-12.923182	0.629670	0.255245
-13.164474	-1.831779	0.260250
-13.304841	-1.076209	0.265254
-14.245364	2.482270	0.270259
-14.841888	18.554768	0.275264
-14.539221	3.807248	0.280269
-14.769116	2.562002	0.285274
-14.888216	1.049246	0.290278
-15.140441	2.730726	0.295283
-15.254668	-0.748232	0.300288
-15.111602	-2.459693	0.305293
-15.444576	5.586412	0.310298
-16.033033	-2.665612	0.315302
-16.261798	-1.159174	0.320307
-16.600160	7.086809	0.325312
-16.349608	0.877680	0.330317
-16.912480	1.980785	0.335322
-17.958971	0.118642	0.340326
-17.603180	-12.284337	0.345331
-18.229233	3.302121	0.350336
-18.035545	-11.705679	0.355341
-18.358556	1.008390	0.360346
-18.320823	0.847525	0.365350
-18.033400	-0.691569	0.370355
-18.792097	4.939882	0.375360
-19.070147	-3.627931	0.380365
-19.233491	5.821520	0.385370
-20.179651	2.994726	0.390374
-20.715408	5.092129	0.395379
-21.363776	2.889243	0.400384
-20.305889	-0.172645	0.405389
-20.908385	3.314682	0.410394
-21.030341	9.642378	0.415398
-20.959014	-6.053152	0.420403
-21.747003	-3.494489	0.425408
-21.709097	-9.016662	0.430413
-22.003717	0.837556	0.435418
-22.793026	2.215247	0.440422
-22.811264	-2.355597	0.445427
-22.981125	4.546585	0.450432
-22.709702	-10.039291	0.455437
-22.860913	5.566168	0.460442
-23.510876	0.056645	0.465446
-24.013688	-3.776390	0.470451
-24.510392	2.572784	0.475456
-24.518585	0.624589	0.480461
-24.694805	-2.908446	0.485466
-25.010032	1.853476	0.490470
-24.344733	-5.099283	0.495475
-24.918923	2.677500	0.500480
-25.478167	-0.079852	0.505485
-25.981995	-3.639545	0.510490
-26.030807	9.756301	0.515494
-26.161423	-3.926550	0.520499
-26.695365	3.096176	0.525504
-27.240373	1.716746	0.530509
-27.441512	3.128153	0.535514
-27.805501	-2.014673	0.540518
-27.687878	-2.789349	0.545523
-28.037229	0.794062	0.550528
-27.838519	-7.501030	0.555533
-28.056835	-7.145250	0.560538
-28.088396	-13.513643	0.565542
-28.526269	-7.709395	0.570547
-29.104402	1.602412	0.575552
-28.829242	-9.102618	0.580557
-29.588149	-1.485812	0.585562
-30.494882	5.495724	0.590566
-30.329251	1.754958	0.595571
-30.752035	-3.824267	0.600576
-30.792871	-13.981136	0.605581
-31.100836	-2.363832	0.610586
-31.051840	2.389594	0.615590
-30.972936	1.336402	0.620595
-31.055666	0.173088	0.625600
-31.853148	-4.479211	0.630605
-32.411260	-0.951965	0.635610
-32.751305	4.795475	0.640614
-32.472526	4.847429	0.645619
-32.712655	2.897509	0.650624
-32.658929	-8.118290	0.655629
-33.467051	1.450933	0.660634
-33.883627	-5.238193	0.665638
-33.849239	1.255741	0.670643
-34.335207	4.445605	0.675648
-34.157562	-8.582112	0.680653
-34.077466	5.440980	0.685658
-34.865856	3.603172	0.690662
-35.135199	-1.868326	0.695667
-35.694211	14.827186	0.700672
-35.546152	10.940254	0.705677
-35.762959	11.255436	0.710682
-35.823912	-4.421290	0.715686
-36.375411	-0.698419	0.720691
-37.075532	9.974564	0.725696
-37.215662	13.270452	0.730701
-37.470901	12.878910	0.735706
-37.536518	9.049093	0.740710
-37.514201	2.292168	0.745715
-37.544152	11.965030	0.750720
-38.109570	6.838324	0.755725
-38.643713	3.708842	0.760730
-39.113642	-0.813893	0.765734
-38.989483	2.195724	0.770739
-39.377298	10.570535	0.775744
-39.161122	1.916113	0.780749
-39.715175	6.339362	0.785754
-39.748756	8.770001	0.790758
-39.491569	7.111006	0.795763
-39.919815	11.117466	0.800768
-40.305471	6.028927	0.805773
-40.608107	3.546935	0.810778
-41.465347	6.356875	0.815782
-41.809650	1.698741	0.820787
-42.132464	14.818356	0.825792
-41.881647	0.504612	0.830797
-41.926767	2.895425	0.835802
-41.866416	-4.463162	0.840806
-42.043456	6.017912	0.845811
-42.692326	2.472423	0.850816
-43.162218	2.051736	0.855821
-43.250737	6.483288	0.860826
-43.694588	10.573421	0.865830
-44.021713	-0.034940	0.870835
-45.002280	2.654403	0.875840
-44.597858	7.277567	0.880845
-44.911725	1.753446	0.885850
-45.293588	1.449520	0.890854
-45.225062	8.780621	0.895859
-45.332130	12.965447	0.900864
-45.389759	15.196635	0.905869
-45.238024	15.603037	0.910874
-45.792904	12.389475	0.915878
-46.251787	12.186870	0.920883
-46.824219	19.325273	0.925888
-46.886537	5.087051	0.930893
-47.118294	7.368718	0.935898
-47.397060	11.745192	0.940902
-47.709596	-5.982812	0.945907
-48.756619	10.141238	0.950912
-48.717869	6.199664	0.955917
-48.747592	2.468195	0.960922
-48.285282	-3.854948	0.965926
-48.476551	0.160390	0.970931
-49.066324	-2.095386	0.975936
-48.885220	7.328414	0.980941
-49.450067	7.766522	0.985946
-50.183901	10.986696	0.990950
-50.114781	4.671605	0.995955
-50.081835	7.611750	1.000960
-50.259717	16.515484	1.005965
-51.357549	6.112030	1.010970
-51.891605	8.650041	1.015974
-52.011459	6.409340	1.020979
-52.088897	1.704342	1.025984
-51.645024	-6.962054	1.030989
-51.815083	-2.264178	1.035994
-52.079858	3.545503	1.040998
-51.966815	-2.740638	1.046003
-52.874291	4.597363	1.051008
-52.987207	-1.465177	1.056013
-53.540770	1.011340	1.061018
-53.673226	14.044248	1.066022
-53.399203	4.045568	1.071027
-54.483551	-3.819161	1.076032
-55.083435	0.038972	1.081037
-55.093108	7.342645	1.086042
-55.248348	-2.443027	1.091046
-55.198923	-7.589354	1.096051
-55.281056	5.652072	1.101056
-55.083663	-3.244300	1.106061
-55.221463	-2.500696	1.111066
-56.259237	7.326089	1.116070
-56.075356	8.069904	1.121075
-56.528734	0.523830	1.126080
-57.030084	7.051747	1.131085
-57.719222	14.274745	1.136090
-57.929485	5.674815	1.141094
-58.091228	2.560348	1.146099
-58.208540	6.986891	1.151104
-58.150928	5.680815	1.156109
-58.161637	2.450132	1.161114
-58.120772	0.396753	1.166118
-58.312708	-7.618809	1.171123
-59.085888	6.854577	1.176128
-59.529542	8.480188	1.181133
-59.587773	1.754729	1.186138
-59.739757	4.562852	1.191142
-60.281653	3.730740	1.196147
-61.051005	12.099942	1.201152
-61.298481	12.107459	1.206157
-61.085765	8.014802	1.211162
-61.267184	5.093694	1.216166
-61.482527	2.921653	1.221171
-62.002522	8.415004	1.226176
-61.528556	1.259359	1.231181
-61.349396	-1.365098	1.236186
-62.046962	16.106045	1.241190
-62.733027	3.096460	1.246195
-63.340016	6.296856	1.251200
-63.248330	10.698923	1.256205
-63.303885	8.204116	1.261210
-63.780457	20.860903	1.266214
-64.131726	6.122606	1.271219
-64.976807	9.806296	1.276224
-64.827509	1.135799	1.281229
-64.909004	10.232746	1.286234
-64.653021	5.241498	1.291238
-64.941523	1.797559	1.296243
-64.921798	12.660269	1.301248
-65.383567	5.124263	1.306253
-65.894089	4.563790	1.311258
-66.270688	6.551432	1.316262
-66.118493	-1.413768	1.321267
-66.584416	4.995136	1.326272
-66.815834	11.901081	1.331277
-67.289085	-0.527671	1.336282
-67.493023	8.700496	1.341286
-67.488820	3.582752	1.346291
-68.189966	8.360114	1.351296
-67.783810	6.765288	1.356301
-68.934678	-0.506778	1.361306
-69.454580	3.926218	1.366310
-68.898718	-1.526668	1.371315
-69.430204	5.485788	1.376320
-69.699848	7.245817	1.381325
-69.378737	13.458656	1.386330
-69.444181	14.484294	1.391334
-69.544378	-4.460779	1.396339
-70.623029	19.338202	1.401344
-70.900019	15.350054	1.406349
-70.740921	4.246298	1.411354
-71.142225	23.932213	1.416358
-71.371197	15.675335	1.421363
-72.355543	9.045412	1.426368
-72.485837	20.415439	1.431373
-72.301856	15.883486	1.436378
-72.519670	10.152791	1.441382
-72.628789	8.232620	1.446387
-73.024301	12.141922	1.451392
-72.738063	11.937423	1.456397
-72.991420	11.963571	1.461402
-73.901668	0.739495	1.466406
-74.048655	4.596674	1.471411
-74.475810	5.491193	1.476416
-74.712900	1.896795	1.481421
-74.346182	7.795081	1.486426
-74.924620	11.119997	1.491430
-74.969152	5.307096	1.496435
-75.764792	12.519283	1.501440
-76.098798	7.020984	1.506445
-76.164321	5.621213	1.511450
-76.185801	8.519447	1.516454
-75.745535	9.999668	1.521459
-77.009630	14.151765	1.526464
-77.384535	7.240586	1.531469
-77.747846	9.836901	1.536474
-78.033103	9.792949	1.541478
-77.532560	10.077480	1.546483
-77.710426	5.302461	1.551488
-77.465358	10.768719	1.556493
-77.902615	4.049765	1.561498
-78.847572	11.375220	1.566502
-78.849503	0.898689	1.571507
-79.452885	9.872639	1.576512
-79.454584	-3.185618	1.581517
-79.428512	14.619246	1.586522
-80.343860	16.910007	1.591526
-80.208336	5.837375	1.596531
-80.481529	9.817323	1.601536
-80.628970	6.407292	1.606541
-80.563684	0.788055	1.611546
-81.040700	-1.734172	1.616550
-81.708219	-15.650871	1.621555
-82.633582	-0.713823	1.626560
-82.375428	-4.894388	1.631565
-82.500081	-5.562728	1.636570
-82.764000	2.525333	1.641574
-82.278593	-1.990234	1.646579
-82.527588	-3.137315	1.651584
-82.839252	-5.519452	1.656589
-83.489858	-4.281485	1.661594
-83.991038	-1.073912	1.666598
-84.299371	-13.596202	1.671603
-84.219497	2.315062	1.676608
-84.222372	-2.908451	1.681613
-84.225302	-8.685504	1.686618
-84.934968	-3.314218	1.691622
-85.396312	-2.808666	1.696627
-85.934209	-6.069322	1.701632
-85.703120	-8.425634	1.706637
-85.748441	0.021410	1.711642
-86.028507	12.517561	1.716646
-86.672753	3.819377	1.721651
-87.191674	-1.431810	1.726656
-87.037855	8.817596	1.731661
-87.012531	11.190256	1.736666
-87.160732	3.845911	1.741670
-87.554043	4.153762	1.746675
-88.492176	-0.368934	1.751680
-88.782373	5.507496	1.756685
-88.896191	0.213429	1.761690
-89.152556	11.203549	1.766694
-89.321805	-1.829878	1.771699
-89.291740	-2.499815	1.776704
-89.012619	0.710502	1.781709
-88.936106	3.875283	1.786714
-89.458521	6.157929	1.791718
-90.011167	-6.266867	1.796723
-90.538585	4.875183	1.801728
-90.513271	3.123495	1.806733
-91.446876	-3.458275	1.811738
-91.843644	-1.080180	1.816742
-91.554047	-6.423947	1.821747
-91.835369	5.441608	1.826752
-91.978359	0.717752	1.831757
-92.267428	11.264300	1.836762
-92.355151	12.298355	1.841766
-92.355597	6.261228	1.846771
-93.138535	20.150822	1.851776
-93.225797	5.200300	1.856781
-93.365142	8.014425	1.861786
-93.661252	-1.661737	1.866790
-93.589895	-7.251094	1.871795
-94.605602	18.867995	1.876800
-95.046673	3.666370	1.881805
-95.250952	10.276994	1.886810
-95.559461	-2.582178	1.891814
-95.394913	3.820394	1.896819
-94.931609	5.030142	1.901824
-95.266073	1.877237	1.906829
-95.401394	14.838595	1.911834
-96.254870	-3.230725	1.916838
-96.775216	2.002136	1.921843
-96.853640	9.652792	1.926848
-96.896924	8.010898	1.931853
-97.106462	-7.981221	1.936858
-97.732939	10.924832	1.941862
-97.979480	1.635884	1.946867
-98.436057	-3.435103	1.951872
-98.345777	-0.116922	1.956877
-98.652762	1.602615	1.961882
-99.014314	5.745048	1.966886
-98.543048	-9.264028	1.971891
-98.656101	8.497720	1.976896
-99.487809	5.242312	1.981901
-99.747099	12.726736	1.986906
-100.122223	7.500419	1.991910
-100.140400	7.628085	1.996915
-100.146715	19.497100	2.006912
-100.444988	17.610957	2.016909
-100.254755	14.728577	2.026906
-99.672537	4.355171	2.036902
-98.764264	7.625617	2.046899
-97.701929	7.393073	2.056896
-97.627646	9.275288	2.066893
-97.599575	15.485371	2.076890
-97.342953	14.382126	2.086886
-96.455283	16.043184	2.096883
-95.329657	14.010666	2.106880
-94.985552	12.066316	2.116877
-94.377487	4.014187	2.126874
-94.068882	8.343890	2.136870
-94.371441	9.745338	2.146867
-93.637161	1.480518	2.156864
-93.075966	3.860870	2.166861
-92.019826	8.605483	2.176858
-91.651732	-4.164365	2.186854
-91.451806	-4.495552	2.196851
-90.391868	5.671547	2.206848
-90.258475	8.566078	2.216845
-90.053467	7.871525	2.226842
-88.960902	11.988344	2.236838
-88.897395	13.622129	2.246835
-88.427660	4.398947	2.256832
-87.255365	6.361909	2.266829
-86.862011	4.447204	2.276826
-86.865397	-3.545948	2.286822
-86.430751	0.860667	2.296819
-85.587952	-3.708371	2.306816
-85.518178	-2.639958	2.316813
-84.964242	-4.845390	2.326810
-84.146025	-5.005829	2.336806
-83.991659	3.431875	2.346803
-82.734699	1.539359	2.356800
-82.294777	-1.393174	2.366797
-82.379322	-0.591302	2.376794
-82.298131	5.505193	2.386790
-81.321420	4.411604	2.396787
-80.922792	0.904472	2.406784
-79.995702	3.567025	2.416781
-79.254042	4.626785	2.426778
-79.023215	2.466553	2.436774
-79.132932	2.178835	2.446771
-78.210485	12.847602	2.456768
-77.725651	6.944566	2.466765
-77.394546	9.125230	2.476762
-76.512366	7.467174	2.486758
-76.249696	10.325426	2.496755
-75.791789	11.742006	2.506752
-75.067084	10.454375	2.516749
-74.363388	4.325905	2.526746
-74.583244	13.041100	2.536742
-73.831469	14.758601	2.546739
-73.089829	11.425876	2.556736
-72.819587	15.258092	2.566733
-71.681148	10.003944	2.576730
-71.397203	2.326222	2.586726
-71.378692	1.660417	2.596723
-71.091535	-5.778930	2.606720
-70.112359	2.887408	2.616717
-69.947125	5.404768	2.626714
-69.228520	11.483196	2.636710
-68.685300	5.823588	2.646707
-68.247428	7.009715	2.656704
-67.094044	8.500820	2.666701
-67.105223	10.400321	2.676698
-66.897612	16.331214	2.686694
-66.425505	6.477613	2.696691
-65.765921	8.874109	2.706688
-65.414767	10.375504	2.716685
-63.994562	5.034787	2.726682
-64.126004	2.883849	2.736678
-63.831696	-1.018946	2.746675
-63.516009	12.125137	2.756672
-62.405639	13.771672	2.766669
-62.177531	10.025121	2.776666
-61.948980	9.755042	2.786662
-61.105029	11.920741	2.796659
-60.682301	4.826251	2.806656
-60.285581	3.327500	2.816653
-59.479247	7.323158	2.826650
-59.138804	1.151052	2.836646
-58.581193	5.313216	2.846643
-57.717221	10.660993	2.856640
-57.626955	19.294566	2.866637
-57.500446	10.013269	2.876634
-56.892921	11.281105	2.886630
-56.001304	12.713580	2.896627
-56.039659	7.305072	2.906624
-54.710714	10.857467	2.916621
-54.346994	10.899472	2.926618
-54.174859	16.061787	2.936614
-54.141940	10.793127	2.946611
-53.033933	13.244920	2.956608
-52.711832	12.236453	2.966605
-52.014034	10.722518	2.976602
-51.238053	16.429783	2.986598
-51.136000	17.098580	2.996595
-51.111878	12.718377	3.006592
-50.080881	9.396115	3.016589
-49.747023	9.083542	3.026586
-49.240040	6.748911	3.036582
-48.106859	4.920617	3.046579
-48.419134	12.941445	3.056576
-47.914895	7.433634	3.066573
-46.609646	9.030678	3.076570
-46.369234	7.727070	3.086566
-46.334940	8.670415	3.096563
-45.755947	13.037328	3.106560
-44.867446	13.859410	3.116557
-44.594582	22.722109	3.126554
-44.424518	17.959803	3.136550
-43.696609	13.940352	3.146547
-43.479971	15.489366	3.156544
-42.502606	14.707624	3.166541
-41.812429	8.856443	3.176538
-41.762474	15.739020	3.186534
-41.292356	9.006531	3.196531
-40.632922	14.015020	3.206528
-40.227843	9.495304	3.216525
-39.225386	10.281416	3.226522
-38.552057	9.561774	3.236518
-38.745356	14.014682	3.246515
-38.468349	8.002116	3.256512
-37.868404	8.739470	3.266509
-36.896850	6.604107	3.276506
-36.961533	13.963577	3.286502
-35.917744	9.576073	3.296499
-35.778019	16.024144	3.306496
-34.817871	13.006231	3.316493
-34.166801	2.653106	3.326490
-34.006253	12.644313	3.336486
-33.924840	9.829802	3.346483
-33.351991	14.959433	3.356480
-32.268742	10.153146	3.366477
-32.027237	5.949497	3.376474
-31.977791	-1.704387	3.386470
-30.764412	-1.406338	3.396467
-30.659268	7.995262	3.406464
-30.312829	4.312381	3.416461
-29.290478	7.585669	3.426458
-29.148810	4.399565	3.436454
-28.853833	8.190898	3.446451
-27.760514	9.227470	3.456448
-27.681777	14.618440	3.466445
-27.271780	15.137220	3.476442
-26.158319	8.322270	3.486438
-25.987151	13.400634	3.496435
-25.965870	13.330218	3.506432
-24.859951	10.619231	3.516429
-24.375852	10.532438	3.526426
-24.404075	10.178354	3.536422
-22.932427	10.374010	3.546419
-22.976213	6.163721	3.556416
-22.735929	10.528775	3.566413
-22.285632	6.792626	3.576410
-21.383538	8.905457	3.586406
-20.893801	9.862143	3.596403
-21.243187	7.995703	3.606400
-19.941304	13.096575	3.616397
-19.390240	4.727988	3.626394
-19.203273	5.978104	3.636390
-18.290613	7.420147	3.646387
-17.815759	2.546874	3.656384
-17.888060	7.400146	3.666381
-17.199389	8.133261	3.676378
-16.604123	3.633236	3.686374
-16.168315	-1.095784	3.696371
-15.076935	2.686329	3.706368
-14.929048	7.642742	3.716365
-14.845579	-0.506819	3.726362
-13.980654	7.573878	3.736358
-13.278898	-0.327779	3.746355
-13.204246	1.373361	3.756352
-13.020735	5.636570	3.766349
-12.028319	1.785792	3.776346
-11.504148	0.702840	3.786342
-10.611528	5.454391	3.796339
-10.144592	5.271259	3.806336
-10.198077	3.627567	3.816333
-10.002165	6.335101	3.826330
-8.904823	-2.681475	3.836326
-8.589557	4.243935	3.846323
-8.092596	0.056402	3.856320
-6.953285	6.914683	3.866317
-6.835296	5.174742	3.876314
-6.702877	1.353523	3.886310
-6.526630	0.043628	3.896307
-5.682213	6.080432	3.906304
-5.089227	-1.921835	3.916301
-4.265561	-1.125040	3.926298
-4.010050	1.269289	3.936294
-4.045013	4.103237	3.946291
-3.538702	20.547124	3.956288
-2.931629	38.433919	3.966285
-2.396181	43.281156	3.976282
-1.813402	61.291468	3.986278
-1.415165	75.895595	3.996275
-0.863050	97.296749	4.006272
-0.711950	115.910796	4.016269
0.000000	130.491669	4.021274
0.189513	139.049551	4.026278
0.202263	151.891068	4.031283
0.575017	154.953655	4.036288
0.332523	143.767877	4.041293
0.564494	154.277358	4.046298
0.422041	166.462629	4.051302
0.561996	148.772521	4.056307
0.476277	164.860500	4.061312
0.613722	179.335198	4.066317
0.956907	170.794652	4.071322
0.640835	182.181596	4.076326
0.955320	180.480657	4.081331
0.832236	175.745064	4.086336
0.534284	181.027752	4.091341
0.816264	174.083998	4.096346
0.663629	170.784587	4.101350
0.859654	181.585043	4.106355
0.845301	183.551218	4.111360
1.048587	184.306833	4.116365
1.183730	183.787040	4.121370
1.186446	189.844313	4.126374
1.200891	176.538065	4.131379
0.808152	180.760379	4.136384
0.907063	179.051459	4.141389
1.130727	172.513347	4.146394
1.196080	187.233780	4.151398
1.156922	184.080368	4.156403
1.098043	189.456539	4.161408
0.880644	182.947309	4.166413
1.236274	174.672259	4.171418
0.995830	196.069049	4.176422
1.168032	176.365639	4.181427
1.343388	185.024048	4.186432
0.998482	170.307219	4.191437
0.865276	165.294896	4.196442
0.995999	171.789757	4.201446
1.389247	173.440257	4.206451
0.981819	179.523375	4.211456
0.844673	184.621838	4.216461
1.229722	162.364788	4.221466
0.698531	194.084607	4.226470
0.960146	190.273475	4.231475
1.069216	175.402991	4.236480
1.307980	180.403422	4.241485
1.331902	175.681124	4.246490
1.212857	174.068402	4.251494
1.035076	168.715979	4.256499
0.953430	184.686202	4.261504
1.016567	182.689298	4.266509
1.208102	178.624070	4.271514
1.111714	182.197585	4.276518
1.387705	193.571047	4.281523
1.437961	194.836350	4.286528
1.117098	192.448099	4.291533
1.531333	209.462854	4.296538
1.285758	202.305367	4.301542
1.844167	196.538663	4.306547
1.570266	200.112216	4.311552
1.336034	189.151948	4.316557
1.247387	184.819985	4.321562
1.038321	189.903500	4.326566
1.482049	190.593139	4.331571
1.468933	200.881124	4.336576
1.546595	197.269978	4.341581
1.633612	205.935401	4.346586
1.320150	199.980108	4.351590
1.522640	201.306283	4.356595
1.511122	192.920431	4.361600
1.600965	214.193903	4.366605
1.239463	200.083858	4.371610
1.430037	210.541617	4.376614
1.351070	211.937588	4.381619
1.378047	214.696839	4.386624
1.353421	213.106591	4.391629
1.606882	207.949261	4.396634
1.443064	221.273339	4.401638
1.530054	216.914315	4.406643
1.759248	212.513738	4.411648
1.487687	221.464940	4.416653
1.625533	210.796457	4.421658
1.290511	223.485663	4.426662
1.579803	216.300652	4.431667
1.464767	217.854120	4.436672
1.536215	225.251043	4.441677
1.883631	234.204934	4.446682
1.782996	239.112796	4.451686
1.786223	224.639187	4.456691
1.734491	233.526839	4.461696
1.899886	240.707677	4.466701
2.050818	230.925415	4.471706
1.712431	219.075886	4.476710
1.644115	210.706810	4.481715
1.820987	220.574707	4.486720
1.891367	233.734012	4.491725
2.352582	218.767408	4.496730
1.803140	222.367361	4.501734
1.677938	215.104639	4.506739
1.725003	209.734184	4.511744
1.772467	221.922742	4.516749
2.306769	233.565202	4.521754
1.646376	230.959677	4.526758
2.344633	226.496282	4.531763
1.859325	221.831879	4.536768
1.872734	229.215705	4.541773
2.140813	221.667985	4.546778
1.702537	228.279590	4.551782
1.813518	213.701959	4.556787
2.092514	244.423670	4.561792
1.835658	233.642619	4.566797
2.152435	230.066535	4.571802
2.026627	247.940291	4.576806
2.343853	227.111847	4.581811
2.365021	231.343713	4.586816
1.988083	229.148322	4.591821
2.475360	229.186246	4.596826
1.874347	227.112826	4.601830
2.154323	227.989449	4.606835
2.080666	237.909512	4.611840
2.315889	235.212611	4.616845
2.231704	224.118606	4.621850
1.754297	222.142951	4.626854
2.064700	236.507927	4.631859
1.981715	236.661892	4.636864
2.273895	243.266445	4.641869
2.640862	240.445959	4.646874
2.554553	240.537432	4.651878
2.625491	234.687402	4.656883
2.018152	217.341106	4.661888
2.169838	222.986845	4.666893
2.126949	234.089935	4.671898
2.183261	237.335946	4.676902
2.542200	229.788599	4.681907
2.611216	241.508941	4.686912
2.253402	233.598793	4.691917
2.379952	233.354288	4.696922
2.126496	243.551299	4.701926
2.419292	243.486992	4.706931
2.414682	242.799195	4.711936
2.392212	236.031019	4.716941
2.308138	231.142162	4.721946
2.374522	245.895334	4.726950
2.425171	228.402110	4.731955
2.588530	240.899365	4.736960
2.153455	252.538361	4.741965
2.194139	236.123016	4.746970
2.360754	245.599480	4.751974
2.626631	244.895101	4.756979
2.592554	246.789960	4.761984
2.069850	247.160431	4.766989
2.438954	245.561546	4.771994
2.046321	259.498733	4.776998
2.426356	246.436068	4.782003
2.336409	254.271072	4.787008
2.684810	274.481499	4.792013
2.771905	272.512293	4.797018
2.747164	263.447958	4.802022
2.796135	251.684941	4.807027
2.595590	242.899468	4.812032
2.356500	252.998710	4.817037
2.715487	259.401725	4.822042
2.817302	268.272310	4.827046
2.846116	256.138319	4.832051
2.557302	258.085338	4.837056
2.674694	265.024224	4.842061
3.120562	269.170625	4.847066
2.798092	253.915094	4.852070
2.566693	253.955861	4.857075
2.996630	241.131397	4.862080
2.414660	243.025342	4.867085
2.900485	253.868722	4.872090
2.636316	260.858624	4.877094
2.735504	257.776158	4.882099
2.664427	275.578649	4.887104
2.396930	271.040133	4.892109
2.693496	271.955748	4.897114
2.611438	274.529106	4.902118
2.751580	270.579389	4.907123
2.596550	275.686954	4.912128
2.578224	280.165588	4.917133
2.622385	279.832095	4.922138
2.479115	274.132483	4.927142
3.020344	294.721284	4.932147
3.200333	304.012468	4.937152
2.845814	302.579231	4.942157
2.906313	293.426701	4.947162
3.117818	305.634388	4.952166
3.172569	301.684864	4.957171
3.279722	299.599969	4.962176
2.662959	288.562062	4.967181
3.010314	297.611204	4.972186
3.008238	301.689080	4.977190
3.464828	301.063580	4.982195
3.208546	293.233503	4.987200
2.788796	284.199705	4.992205
3.386614	302.223176	4.997210
3.298384	301.400520	5.002214
2.981322	295.477650	5.007219
3.018508	302.844559	5.012224
3.173992	306.243096	5.017229
3.511109	315.191337	5.022234
2.924573	300.100449	5.027238
3.121044	296.209588	5.032243
3.236108	303.489044	5.037248
3.228677	316.635923	5.042253
2.973873	314.851958	5.047258
3.208186	311.304183	5.052262
3.164752	310.167006	5.057267
2.924510	310.858592	5.062272
2.821283	317.780981	5.067277
3.173197	306.220322	5.072282
3.309789	321.353433	5.077286
3.116573	309.429332	5.082291
2.891866	311.438769	5.087296
2.981440	305.713985	5.092301
3.203940	312.735660	5.097306
3.141965	330.130738	5.102310
3.440170	325.061080	5.107315
3.454933	341.545813	5.112320
3.200977	335.928399	5.117325
3.452614	335.131955	5.122330
3.154171	339.557056	5.127334
3.634126	334.761420	5.132339
3.444198	344.622137	5.137344
3.496420	335.582136	5.142349
3.643812	348.373055	5.147354
3.690482	339.459757	5.152358
3.593246	332.524141	5.157363
3.651657	340.873930	5.162368
3.359029	342.862631	5.167373
3.720581	339.326084	5.172378
3.525727	338.487305	5.177382
3.884684	340.795414	5.182387
3.798425	342.402938	5.187392
3.512247	341.947141	5.192397
3.603239	335.350282	5.197402
3.576746	342.961452	5.202406
3.605211	336.136472	5.207411
3.679088	345.911567	5.212416
3.719795	352.723466	5.217421
3.604299	344.455739	5.222426
3.209468	347.695428	5.227430
3.676995	342.609918	5.232435
3.878475	341.647535	5.237440
3.595689	346.568267	5.242445
3.979149	342.663266	5.247450
3.787941	351.594951	5.252454
3.776374	336.272273	5.257459
4.120787	334.487150	5.262464
3.735051	341.472021	5.267469
3.981293	337.379163	5.272474
4.030146	342.046790	5.277478
3.807774	337.967146	5.282483
3.676419	336.519127	5.287488
3.543923	332.657857	5.292493
3.798898	338.595662	5.297498
3.473214	351.790033	5.302502
4.030927	346.451460	5.307507
4.141550	346.121189	5.312512
3.993058	348.330445	5.317517
4.248056	345.630455	5.322522
3.850684	340.927214	5.327526
3.884801	346.253246	5.332531
4.310246	347.887494	5.337536
3.926805	348.526780	5.342541
3.868410	357.310338	5.347546
3.510363	352.936522	5.352550
3.961920	346.236960	5.357555
3.892483	352.311351	5.362560
3.931093	349.555269	5.367565
4.142266	337.411401	5.372570
4.043712	344.900307	5.377574
3.979099	346.215485	5.382579
4.124557	346.960736	5.387584
3.732553	337.311143	5.392589
4.248119	343.252551	5.397594
3.850389	355.663460	5.402598
3.773118	335.048640	5.407603
3.952426	345.691460	5.412608
4.039652	344.481485	5.417613
3.991241	345.148574	5.422618
3.934429	370.017379	5.427622
4.052937	368.574928	5.432627
4.077360	379.984083	5.437632
3.992675	380.799628	5.442637
4.396504	384.912559	5.447642
4.022537	377.570014	5.452646
4.111875	378.896357	5.457651
4.341033	379.974951	5.462656
4.203182	385.500881	5.467661
4.419902	374.513610	5.472666
4.163053	382.835608	5.477670
4.609796	381.520639	5.482675
4.237015	382.259782	5.487680
4.194417	377.943240	5.492685
4.334667	378.612992	5.497690
4.148939	381.790904	5.502694
4.252768	383.149579	5.507699
4.244226	377.584923	5.512704
4.134047	389.302828	5.517709
4.162625	379.119524	5.522714
4.050577	399.724869	5.527718
4.696911	408.300838	5.532723
4.607096	410.196739	5.537728
4.630258	422.242276	5.542733
4.754493	402.881148	5.547738
4.571976	397.370293	5.552742
4.440787	392.801224	5.557747
4.362566	388.602837	5.562752
4.568464	386.683537	5.567757
4.499125	396.114340	5.572762
4.427272	402.662605	5.577766
4.682752	410.706586	5.582771
4.584620	412.775624	5.587776
4.659111	424.169237	5.592781
4.623944	413.055058	5.597786
4.324098	425.339648	5.602790
4.464884	421.371830	5.607795
4.548393	419.740408	5.612800
4.400375	420.912018	5.617805
4.389707	415.062086	5.622810
4.327960	420.957650	5.627814
4.385768	407.278807	5.632819
4.843694	412.601617	5.637824
4.396896	421.597975	5.642829
4.655084	404.186078	5.647834
4.280894	413.434241	5.652838
4.697471	428.825054	5.657843
4.616139	440.175961	5.662848
4.575621	444.180809	5.667853
4.727352	433.190917	5.672858
4.779316	444.936430	5.677862
4.839682	445.546282	5.682867
4.758890	452.253897	5.687872
4.918182	451.798179	5.692877
5.050260	445.410543	5.697882
5.111867	453.380330	5.702886
4.983016	447.500489	5.707891
4.934299	446.081226	5.712896
4.873960	454.304589	5.717901
4.991973	446.283635	5.722906
4.932234	456.784900	5.727910
4.868618	448.302744	5.732915
4.906974	443.701300	5.737920
4.833740	449.473972	5.742925
5.331379	449.759098	5.747930
5.284592	449.877289	5.752934
5.133668	435.692962	5.757939
5.009017	436.832397	5.762944
4.911203	443.200875	5.767949
5.115370	441.354465	5.772954
5.009809	435.241205	5.777958
5.354823	430.955996	5.782963
5.013873	447.517186	5.787968
4.590733	433.413659	5.792973
4.788106	442.499708	5.797978
4.664712	450.339649	5.802982
4.874474	445.115468	5.807987
5.154078	444.013393	5.812992
4.543013	440.903433	5.817997
4.786049	447.724066	5.823002
5.169794	473.665944	5.828006
4.778578	463.456555	5.833011
5.160396	485.306951	5.838016
5.122827	476.237704	5.843021
5.459986	475.888246	5.848026
5.036574	484.184549	5.853030
5.097635	474.180699	5.858035
5.261110	482.683289	5.863040
5.119317	491.949724	5.868045
5.376120	476.000379	5.873050
5.596046	483.421331	5.878054
5.314296	476.570600	5.883059
5.240450	483.906911	5.888064
5.127627	481.466772	5.893069
5.273062	470.138019	5.898074
5.326815	484.591713	5.903078
5.447756	475.320169	5.908083
5.377423	484.026550	5.913088
5.100419	482.413360	5.918093
5.345084	485.812196	5.923098
5.418724	480.012632	5.928102
5.467484	479.085936	5.933107
5.614577	469.389693	5.938112
5.156372	486.106154	5.943117
5.346527	474.898657	5.948122
5.108974	483.938806	5.953126
5.495499	496.109336	5.958131
5.529005	508.416943	5.963136
5.756696	512.995380	5.968141
5.957164	501.460392	5.973146
5.428083	500.003496	5.978150
6.031891	488.890516	5.983155
5.772227	481.079943	5.988160
5.312722	480.963359	5.993165
5.041632	475.487042	5.998170
5.388385	491.193518	6.003174
5.550111	506.171218	6.008179
5.603621	497.729466	6.013184
5.591814	502.528910	6.018189
6.022467	504.246667	6.023194
5.790746	502.855864	6.028198
5.819882	507.762000	6.033203
6.040333	505.465578	6.038208
5.949558	504.034415	6.043213
5.794470	488.829422	6.048218
5.194813	477.671148	6.053222
5.131175	477.189523	6.058227
5.231709	512.541273	6.063232
5.429569	508.780062	6.068237
5.429617	507.726844	6.073242
5.844284	521.875076	6.078246
5.514571	500.694314	6.083251
6.034433	509.059690	6.088256
5.795456	508.783933	6.093261
5.890474	512.659258	6.098266
5.560123	508.379182	6.103270
5.530529	515.590793	6.108275
5.889715	515.965592	6.113280
5.555447	515.709330	6.118285
5.822772	499.753585	6.123290
5.688915	508.147373	6.128294
5.741511	512.563743	6.133299
5.864337	509.361003	6.138304
5.482413	506.420541	6.143309
5.929044	508.467543	6.148314
5.810391	518.364047	6.153318
5.537585	516.443333	6.158323
5.781891	504.771264	6.163328
5.199711	516.847356	6.168333
5.764115	496.919686	6.173338
5.912019	513.400459	6.178342
5.971287	509.619628	6.183347
5.995068	506.068124	6.188352
5.810573	504.825297	6.193357
5.683338	482.155010	6.198362
5.449972	482.937218	6.203366
5.628033	492.286056	6.208371
5.946484	498.612800	6.213376
5.669385	494.910941	6.218381
5.541711	484.059826	6.223386
5.581247	492.328366	6.228390
5.368886	503.352217	6.233395
5.872458	515.047030	6.238400
5.693511	518.782647	6.243405
5.666978	508.926832	6.248410
5.720121	505.820848	6.253414
5.816444	507.082512	6.258419
5.829619	507.491404	6.263424
5.718494	481.125399	6.268429
5.901944	484.856862	6.273434
5.586993	478.276710	6.278438
5.165122	475.634290	6.283443
5.622766	488.717582	6.288448
5.695398	494.007309	6.293453
6.042566	494.109036	6.298458
6.066043	498.984533	6.303462
5.639518	476.940663	6.308467
6.004545	478.982993	6.313472
5.596427	483.862820	6.318477
5.698121	474.436802	6.323482
5.487202	482.318551	6.328486
5.580560	487.434468	6.333491
5.319317	482.972794	6.338496
5.317530	492.666762	6.343501
6.031223	501.168906	6.348506
5.664350	512.391541	6.353510
5.834455	500.013409	6.358515
5.817089	485.192032	6.363520
5.439346	481.972077	6.368525
5.740257	485.237803	6.373530
5.564705	480.005363	6.378534
5.700157	492.088830	6.383539
6.031847	490.467197	6.388544
5.681942	490.319084	6.393549
5.915251	473.959064	6.398554
5.863711	476.498308	6.403558
5.464175	479.210490	6.408563
5.931262	473.845611	6.413568
5.282811	479.254691	6.418573
5.608532	476.476298	6.423578
5.316155	471.067826	6.428582
5.546298	493.602035	6.433587
5.789299	494.742181	6.438592
5.559140	513.611484	6.443597
5.937734	502.744964	6.448602
5.903966	497.478532	6.453606
5.847784	482.831882	6.458611
5.600937	473.128026	6.463616
5.576130	485.833765	6.468621
5.865014	474.177931	6.473626
5.720201	469.855070	6.478630
5.426165	477.795145	6.483635
5.784325	476.856092	6.488640
5.542627	475.605061	6.493645
5.644380	475.648192	6.498650
5.387034	490.458746	6.503654
5.697984	494.127212	6.508659
5.863339	493.727318	6.513664
5.734705	503.770390	6.518669
5.409260	486.321068	6.523674
5.559044	507.282654	6.528678
5.882442	505.158347	6.533683
6.058912	499.389928	6.538688
5.150069	496.841001	6.543693
5.716139	494.785610	6.548698
5.774983	509.491741	6.553702
5.677966	514.970618	6.558707
6.086984	518.557375	6.563712
5.881440	489.931414	6.568717
6.204466	478.492112	6.573722
5.875107	484.499998	6.578726
5.716677	489.017039	6.583731
5.954521	486.499218	6.588736
5.299333	480.127914	6.593741
5.702900	479.542740	6.598746
5.821911	491.362153	6.603750
5.791798	478.008154	6.608755
5.766358	467.771465	6.613760
5.815143	466.487625	6.618765
5.787618	473.750176	6.623770
5.982144	467.075872	6.628774
5.789823	471.954761	6.633779
5.714796	466.739060	6.638784
5.660601	478.719189	6.643789
5.864392	465.336216	6.648794
5.893443	473.875813	6.653798
5.909215	469.394411	6.658803
5.695448	450.360092	6.663808
5.512097	444.516784	6.668813
5.629376	451.311437	6.673818
5.687827	451.955247	6.678822
5.850611	465.010885	6.683827
5.665931	440.146735	6.688832
5.720508	446.979373	6.693837
5.835680	442.307718	6.698842
5.790023	438.163328	6.703846
5.737521	447.896232	6.708851
5.861558	439.035205	6.713856
5.253940	455.235088	6.718861
5.153197	445.643944	6.723866
5.540364	464.171927	6.728870
5.858672	483.781253	6.733875
5.710235	470.289849	6.738880
5.918792	482.827188	6.743885
5.754788	464.878543	6.748890
5.844356	467.132631	6.753894
5.458024	458.760724	6.758899
5.588161	450.854575	6.763904
5.653234	465.364785	6.768909
5.470326	478.926158	6.773914
5.754828	481.559140	6.778918
5.487459	482.555530	6.783923
5.799911	479.805967	6.788928
5.706516	481.071355	6.793933
5.708440	480.679822	6.798938
5.717240	475.926684	6.803942
5.592140	474.878463	6.808947
5.683688	463.296585	6.813952
5.240883	482.492819	6.818957
5.362334	483.283776	6.823962
5.626832	479.259391	6.828966
5.487684	481.330974	6.833971
5.562036	473.495890	6.838976
5.342886	481.103250	6.843981
5.803941	473.086367	6.848986
5.664404	477.021359	6.853990
5.924652	474.974579	6.858995
5.871564	470.617618	6.864000
5.989726	473.844776	6.869005
5.619991	477.610728	6.874010
5.581012	467.492890	6.879014
5.396545	481.185342	6.884019
5.793547	485.132204	6.889024
5.821741	487.959969	6.894029
5.707230	470.230052	6.899034
6.037886	476.866824	6.904038
5.857117	469.977703	6.909043
5.888492	474.997605	6.914048
5.789470	480.644124	6.919053
5.618520	473.220826	6.924058
5.755459	474.446079	6.929062
5.595727	480.936386	6.934067
5.770326	469.717553	6.939072
5.460390	485.494265	6.944077
5.599972	477.299250	6.949082
6.045908	467.652478	6.954086
5.731499	473.635001	6.959091
5.604899	475.814315	6.964096
5.904951	473.052399	6.969101
5.549207	455.939312	6.974106
5.390109	471.349136	6.979110
5.606368	468.709787	6.984115
5.990576	466.865489	6.989120
5.852557	478.062218	6.994125
5.812681	455.598034	6.999130
5.654272	460.403439	7.004134
5.232283	452.201792	7.009139
5.681977	469.046415	7.014144
5.656395	471.134253	7.019149
5.667040	475.057154	7.024154
5.615445	472.262188	7.029158
5.781294	478.125293	7.034163
6.103245	476.281811	7.039168
5.727754	473.472691	7.044173
5.800296	449.578542	7.049178
5.642708	454.414493	7.054182
5.600681	444.770335	7.059187
5.714084	454.570735	7.064192
5.493366	454.673766	7.069197
5.802419	446.876369	7.074202
5.848751	453.453567	7.079206
5.703049	448.883228	7.084211
5.854397	437.201611	7.089216
5.136346	444.176527	7.094221
5.692670	440.316731	7.099226
5.733263	455.270398	7.104230
5.524566	463.927711	7.109235
5.832734	456.516701	7.114240
5.701917	474.965142	7.119245
5.811284	461.560878	7.124250
5.450660	453.436303	7.129254
5.347044	459.033752	7.134259
5.524440	472.257461	7.139264
5.631977	477.877737	7.144269
5.901408	473.072552	7.149274
5.664542	475.652781	7.154278
5.646365	482.135679	7.159283
5.896496	484.264775	7.164288
5.594675	475.636886	7.169293
5.855180	479.573549	7.174298
5.651414	477.573357	7.179302
5.566248	480.710697	7.184307
5.862133	482.031132	7.189312
5.769204	472.709494	7.194317
5.806898	467.837437	7.199322
5.647552	460.675839	7.204326
5.749442	461.150969	7.209331
5.675701	455.580386	7.214336
5.512427	455.966049	7.219341
5.457438	449.070852	7.224346
5.449316	464.221507	7.229350
5.635610	474.160524	7.234355
5.932192	475.061943	7.239360
5.555243	478.606614	7.244365
5.653436	481.813593	7.249370
6.109185	480.881400	7.254374
5.400651	468.017380	7.259379
5.841761	473.331052	7.264384
5.663257	481.493650	7.269389
5.638336	469.195226	7.274394
5.868416	471.749000	7.279398
5.414792	475.468436	7.284403
5.922052	465.960603	7.289408
5.726551	469.283892	7.294413
5.744354	450.250669	7.299418
5.798151	450.934810	7.304422
5.556284	444.202501	7.309427
5.546216	443.817193	7.314432
5.436618	451.149630	7.319437
5.734114	467.236851	7.324442
5.586025	463.734082	7.329446
5.868084	472.300435	7.334451
5.931358	467.865544	7.339456
5.543298	452.234311	7.344461
5.684668	452.802067	7.349466
5.746723	448.939991	7.354470
5.505271	454.964316	7.359475
5.917146	457.089766	7.364480
5.385480	460.824363	7.369485
5.701075	455.862976	7.374490
5.734621	469.384920	7.379494
5.602431	473.340797	7.384499
5.847633	484.532311	7.389504
5.625592	477.716306	7.394509
5.926330	468.496643	7.399514
5.331529	456.990307	7.404518
5.473173	468.296890	7.409523
6.208160	470.031537	7.414528
5.678973	457.261111	7.419533
5.489348	444.989332	7.424538
5.607264	448.269308	7.429542
5.827997	470.402811	7.434547
5.712945	453.811017	7.439552
5.401157	454.866738	7.444557
5.759739	474.322299	7.449562
5.948085	475.735386	7.454566
5.594477	470.045597	7.459571
5.704644	446.507013	7.464576
5.372764	458.247697	7.469581
5.688859	481.209176	7.474586
5.765602	478.357287	7.479590
5.712747	482.569687	7.484595
5.818398	475.114688	7.489600
5.445962	471.183919	7.494605
5.812882	483.422991	7.499610
5.586259	478.770416	7.504614
5.409391	488.916160	7.509619
5.551314	470.161927	7.514624
5.733209	497.601970	7.519629
5.908195	483.566582	7.524634
6.163702	480.099914	7.529638
5.681507	470.701229	7.534643
5.685396	453.311668	7.539648
4.853112	456.502617	7.544653
5.350570	470.128343	7.549658
5.662067	482.211617	7.554662
5.715511	465.903132	7.559667
5.890018	464.382554	7.564672
5.769550	475.755938	7.569677
5.512360	478.537335	7.574682
5.712585	474.699380	7.579686
5.177440	484.979998	7.584691
5.623360	482.367514	7.589696
5.656246	494.977006	7.594701
6.223324	483.429296	7.599706
5.749761	491.225704	7.604710
5.749604	495.900885	7.609715
5.585714	481.283775	7.614720
5.903956	483.466730	7.619725
5.649773	472.130513	7.624730
5.986835	485.313938	7.629734
5.786578	482.140719	7.634739
5.869104	472.757332	7.639744
5.430274	477.006088	7.644749
5.933121	470.678717	7.649754
5.932114	468.673926	7.654758
5.374695	455.659550	7.659763
5.794788	454.893766	7.664768
5.505835	468.516458	7.669773
5.687350	476.454406	7.674778
5.663267	466.710880	7.679782
5.830147	493.319544	7.684787
5.562606	460.158131	7.689792
5.612967	470.510096	7.694797
5.523816	474.267070	7.699802
5.523346	487.701124	7.704806
5.348881	486.877614	7.709811
5.839683	480.953569	7.714816
5.244716	485.633809	7.719821
5.704171	483.546117	7.724826
5.930493	480.958280	7.729830
5.719954	476.153779	7.734835
6.000949	480.914597	7.739840
5.810028	476.023291	7.744845
6.020340	477.935211	7.749850
6.051709	465.118218	7.754854
5.258831	457.994722	7.759859
5.827075	448.502374	7.764864
5.841095	454.323572	7.769869
5.948945	453.097849	7.774874
5.996006	455.383327	7.779878
5.637742	458.340262	7.784883
5.484289	447.349984	7.789888
5.450941	453.875630	7.794893
5.676490	440.029635	7.799898
5.659722	441.829610	7.804902
5.303909	455.095938	7.809907
5.804361	442.837490	7.814912
5.562502	445.015524	7.819917
5.372253	449.623348	7.824922
5.721336	471.042376	7.829926
5.573210	475.563630	7.834931
5.644355	475.456039	7.839936
5.483153	481.943828	7.844941
5.522050	486.401325	7.849946
5.562020	477.759968	7.854950
5.636218	477.489581	7.859955
5.863138	480.050094	7.864960
5.655573	493.366838	7.869965
5.551006	486.381752	7.874970
5.686906	484.403072	7.879974
5.800048	485.355425	7.884979
5.782015	480.148948	7.889984
5.796110	485.537038	7.894989
5.899387	486.141773	7.899994
5.765062	482.497420	7.904998
5.744145	478.155463	7.910003
5.781570	470.502587	7.915008
5.842099	482.019603	7.920013
5.348188	473.164088	7.925018
5.352619	483.953996	7.930022
5.408126	488.420392	7.935027
5.630199	483.345603	7.940032
5.723468	482.860937	7.945037
5.791077	479.189134	7.950042
5.993756	477.368519	7.955046
5.749397	479.510763	7.960051
5.489292	484.159541	7.965056
5.727262	476.351481	7.970061
5.578508	486.285200	7.975066
5.633877	481.081193	7.980070
5.278084	473.924035	7.985075
5.881977	475.110204	7.990080
5.781933	486.447367	7.995085
5.870450	491.569907	8.000090
5.936167	480.565684	8.005094
5.691112	493.960150	8.010099
5.922175	486.739352	8.015104
5.816635	483.459912	8.020109
5.517841	462.625850	8.025126
5.309902	465.196586	8.030144
5.807701	491.288791	8.035162
6.000527	473.103250	8.040179
5.742389	490.702184	8.045197
5.884790	476.444288	8.050214
6.000036	456.284969	8.055232
5.588144	450.327218	8.060250
5.551872	445.500369	8.065267
5.587405	455.527518	8.070285
5.483512	447.623870	8.075302
5.727140	456.406634	8.080320
5.447897	476.739900	8.085338
5.715341	465.012328	8.090355
5.847525	482.445590	8.095373
5.663624	482.607413	8.100390
5.750387	478.585947	8.105408
5.704345	494.919368	8.110426
5.755526	483.779775	8.115443
5.596584	492.532254	8.120461
5.471770	488.991824	8.125478
5.614415	490.891657	8.130496
5.646364	488.549197	8.135514
5.741675	495.733385	8.140531
5.608450	482.685569	8.145549
5.729029	482.736556	8.150566
5.961924	489.981551	8.155584
5.545289	494.707331	8.160602
6.013211	481.516777	8.165619
5.808864	480.551787	8.170637
5.894333	490.887180	8.175654
5.778967	484.475375	8.180672
5.453983	488.607675	8.185690
5.872532	474.253566	8.190707
5.797524	485.840039	8.195725
5.489121	484.239418	8.200742
5.868414	485.500163	8.205760
5.820302	507.829524	8.210778
5.988257	506.665239	8.215795
5.906622	504.771482	8.220813
5.884130	506.719667	8.225830
5.754441	483.864310	8.230848
5.940331	507.655790	8.235866
6.079433	518.420443	8.240883
6.248250	498.468710	8.245901
5.844583	503.569146	8.250918
6.134065	488.967605	8.255936
5.777151	488.711649	8.260954
6.046690	484.618450	8.265971
5.794934	485.555806	8.270989
5.680779	483.347508	8.276006
6.105294	482.840986	8.281024
5.975774	486.431242	8.286042
5.945255	483.058561	8.291059
6.062379	481.033556	8.296077
5.860739	493.131318	8.301094
6.185030	483.958405	8.306112
6.056162	486.241131	8.311130
5.942280	495.062233	8.316147
6.005000	490.597383	8.321165
5.849159	491.790884	8.326182
6.230398	494.554263	8.331200
5.901829	499.349334	8.336218
6.157068	489.904222	8.341235
5.488117	486.904609	8.346253
5.701133	484.852834	8.351270
6.144042	496.847529	8.356288
6.135125	506.199217	8.361306
6.231710	504.461308	8.366323
5.942146	495.612031	8.371341
5.987664	507.992126	8.376358
6.186531	489.235895	8.381376
6.011062	492.514123	8.386394
5.955855	488.722079	8.391411
5.989267	478.757145	8.396429
6.051257	506.231768	8.401446
6.131924	505.725386	8.406464
6.107507	500.419587	8.411482
6.114723	509.485398	8.416499
6.103291	510.568339	8.421517
5.797782	521.746560	8.426534
5.887313	521.160971	8.431552
6.031563	524.444234	8.436570
6.145254	509.185241	8.441587
6.149038	514.867731	8.446605
5.829222	514.983229	8.451622
5.838089	512.647925	8.456640
5.953615	525.122547	8.461658
5.787292	518.040342	8.466675
6.038913	508.037657	8.471693
6.080182	522.723630	8.476710
6.428475	507.064524	8.481728
6.406130	510.697299	8.486746
6.254988	510.491279	8.491763
6.087128	514.955524	8.496781
5.723029	513.824350	8.501798
6.314767	511.701032	8.506816
5.933606	512.900672	8.511834
5.990419	513.253282	8.516851
6.306220	504.865073	8.521869
6.231996	521.620521	8.526886
6.548159	514.274270	8.531904
6.207462	519.643091	8.536922
6.221889	523.505081	8.541939
6.363003	515.329360	8.546957
6.036556	525.492146	8.551974
6.539400	515.017709	8.556992
6.217950	519.197161	8.562010
6.089553	518.540716	8.567027
6.361613	517.939725	8.572045
6.092998	519.625886	8.577063
6.337000	510.995946	8.582080
5.836654	513.818909	8.587098
6.230497	517.193083	8.592115
6.247215	519.172873	8.597133
6.076998	516.082177	8.602151
6.456968	522.040233	8.607168
6.419376	528.748464	8.612186
6.359691	514.575197	8.617203
6.003831	507.319142	8.622221
5.710554	529.843645	8.627239
6.291823	529.914349	8.632256
6.415139	545.844713	8.637274
6.385635	552.695192	8.642291
6.397088	548.029782	8.647309
6.426699	538.104310	8.652327
6.581341	543.443733	8.657344
6.537760	551.914338	8.662362
6.466920	543.199624	8.667379
6.650736	536.440775	8.672397
6.220242	519.568485	8.677415
6.517416	513.657085	8.682432
6.488581	513.453388	8.687450
6.073652	516.864482	8.692467
6.365950	527.875722	8.697485
6.365260	542.245382	8.702503
6.601999	536.673819	8.707520
6.549459	534.243266	8.712538
6.277325	532.042470	8.717555
6.406002	517.282471	8.722573
6.380734	539.329810	8.727591
6.667830	539.469202	8.732608
6.220437	529.763774	8.737626
6.370706	525.835718	8.742643
6.549820	530.969754	8.747661
6.101610	535.535146	8.752679
6.773173	538.342567	8.757696
6.689018	531.684292	8.762714
6.728619	519.336681	8.767731
6.651520	516.607984	8.772749
6.517106	505.997571	8.777767
6.355491	507.356167	8.782784
6.543865	508.630456	8.787802
6.292140	514.287368	8.792819
6.470031	515.233434	8.797837
6.257196	516.639071	8.802855
6.291859	538.156033	8.807872
6.743765	545.738413	8.812890
6.505711	557.381209	8.817907
6.500066	545.883020	8.822925
6.417052	556.248858	8.827943
6.528783	550.317705	8.832960
6.698657	544.339354	8.837978
6.038916	555.036575	8.842995
6.343998	547.631620	8.848013
6.656448	555.447443	8.853031
6.701493	550.743614	8.858048
6.708987	551.442303	8.863066
6.474909	556.743034	8.868083
6.771308	549.145161	8.873101
6.461627	548.524085	8.878119
6.613380	545.526703	8.883136
6.427820	552.650266	8.888154
6.223439	546.651101	8.893171
6.339122	542.040895	8.898189
6.511483	558.360631	8.903207
6.715947	553.374107	8.908224
6.791790	540.152546	8.913242
6.585196	559.438287	8.918259
6.775456	553.405491	8.923277
6.441872	552.764157	8.928295
6.671802	553.377278	8.933312
6.742535	545.989795	8.938330
6.733972	550.038234	8.943347
6.984910	547.746666	8.948365
6.443032	544.517716	8.953383
6.287648	548.832595	8.958400
6.680195	549.721147	8.963418
6.454946	546.411925	8.968435
6.722357	567.477651	8.973453
6.718170	571.571525	8.978471
6.818854	578.562873	8.983488
6.835558	578.338955	8.988506
6.740539	587.503975	8.993523
6.972635	573.075980	8.998541
6.576446	575.426512	9.003559
6.746058	573.341847	9.008576
7.042003	583.915895	9.013594
6.818978	570.243693	9.018611
6.725852	556.515496	9.023629
6.717230	555.248818	9.028647
6.923083	552.927403	9.033664
7.196289	555.995502	9.038682
6.786545	558.858509	9.043699
6.908628	543.916736	9.048717
6.735019	552.322724	9.053735
6.503560	551.747175	9.058752
6.603198	549.198774	9.063770
6.741103	556.057803	9.068787
6.806119	569.729262	9.073805
6.952614	578.513486	9.078823
7.078760	581.256154	9.083840
6.907799	558.312840	9.088858
6.713401	568.655369	9.093875
6.665081	561.419614	9.098893
7.069410	577.517213	9.103911
6.832735	577.215899	9.108928
6.727744	570.975932	9.113946
6.621947	591.386178	9.118963
6.763406	583.641975	9.123981
6.911293	583.323657	9.128999
7.087159	587.974776	9.134016
6.783235	580.538089	9.139034
6.677609	583.841697	9.144051
6.948103	574.171712	9.149069
6.641753	592.343288	9.154087
6.992184	580.440331	9.159104
6.982023	586.909354	9.164122
6.929879	594.685565	9.169139
6.956213	575.420538	9.174157
6.966444	574.832405	9.179175
6.678382	582.778576	9.184192
7.156690	573.245969	9.189210
6.756860	586.833760	9.194227
7.150313	583.172925	9.199245
7.072616	571.815831	9.204263
7.218366	580.774358	9.209280
7.499040	578.885865	9.214298
7.126266	582.948741	9.219315
7.553322	575.737355	9.224333
7.078041	592.389305	9.229351
7.285773	583.725464	9.234368
7.214968	578.136610	9.239386
6.677192	571.232475	9.244403
7.011096	572.926927	9.249421
6.978209	574.094506	9.254439
6.908542	575.999225	9.259456
7.387756	575.903660	9.264474
7.010988	589.513523	9.269491
7.090904	571.073840	9.274509
6.901026	584.420674	9.279527
7.024950	580.358598	9.284544
7.361628	580.711311	9.289562
7.098948	582.620766	9.294579
7.344141	566.467218	9.299597
7.309029	583.403931	9.304615
7.231450	577.905747	9.309632
7.171719	578.106784	9.314650
6.954040	578.267400	9.319667
7.155662	572.186173	9.324685
7.030689	577.465831	9.329703
6.831329	587.380435	9.334720
7.158032	574.555397	9.339738
7.108334	587.526674	9.344755
7.050350	583.490426	9.349773
7.082129	579.498784	9.354791
7.220366	589.351991	9.359808
7.240157	585.403462	9.364826
6.817474	580.851706	9.369843
7.206080	576.269506	9.374861
7.059016	580.691659	9.379879
7.072913	584.721536	9.384896
7.331215	584.942543	9.389914
6.911061	581.961529	9.394931
7.355932	582.406185	9.399949
7.303197	579.634482	9.404967
7.002472	584.831888	9.409984
7.356310	570.310956	9.415002
7.276476	589.526879	9.420019
7.470064	581.949719	9.425037
7.200371	582.086751	9.430055
7.018116	579.752515	9.435072
7.456153	589.915364	9.440090
7.259866	605.026131	9.445107
7.405114	611.885153	9.450125
7.561843	608.024696	9.455143
7.318090	594.288391	9.460160
7.238478	588.057115	9.465178
6.990625	601.195867	9.470195
7.263166	608.450801	9.475213
7.421285	615.198860	9.480231
7.386698	620.213544	9.485248
7.831937	612.473349	9.490266
6.955688	607.271181	9.495283
6.893084	611.189321	9.500301
7.243823	609.310207	9.505319
7.398329	616.763160	9.510336
7.726567	607.654766	9.515354
7.552569	615.376827	9.520371
7.495526	613.729439	9.525389
7.589580	617.416415	9.530407
7.225374	623.754626	9.535424
7.403370	616.596188	9.540442
7.465725	622.222197	9.545459
7.425891	626.922455	9.550477
7.434364	626.137600	9.555495
7.337736	618.669590	9.560512
7.327851	619.633507	9.565530
7.295913	619.682144	9.570547
7.200539	615.399555	9.575565
7.157138	612.472691	9.580583
7.378473	620.071168	9.585600
7.453544	611.515536	9.590618
7.459733	624.045012	9.595635
7.239687	634.466514	9.600653
7.494280	618.693078	9.605671
7.494878	631.428564	9.610688
7.914745	642.105281	9.615706
7.300884	625.873200	9.620723
7.512743	631.936428	9.625741
7.880724	626.820614	9.630759
7.440691	635.837794	9.635776
7.456243	622.102601	9.640794
7.570611	637.288122	9.645811
7.547849	649.815711	9.650829
7.493479	650.158455	9.655847
7.543475	645.583873	9.660864
7.760718	653.661104	9.665882
7.837253	648.290745	9.670899
7.467997	645.113350	9.675917
7.912786	640.281241	9.680935
7.725294	647.468837	9.685952
7.702480	621.613094	9.690970
7.619673	615.772320	9.695987
7.474855	618.379787	9.701005
7.852147	623.951096	9.706023
7.432694	628.486964	9.711040
7.762878	620.881111	9.716058
7.657208	637.919093	9.721075
7.581137	643.804654	9.726093
7.832951	643.049356	9.731111
7.798781	644.890748	9.736128
7.886058	636.913883	9.741146
7.711954	637.802694	9.746163
7.664610	635.127512	9.751181
7.874892	645.487947	9.756199
7.638902	649.232522	9.761216
7.866210	644.604332	9.766234
7.601945	649.866982	9.771251
7.601961	650.770417	9.776269
7.977024	642.235358	9.781287
7.485779	645.881884	9.786304
7.742671	653.963289	9.791322
8.139138	653.368009	9.796339
7.994161	642.548557	9.801357
8.136668	649.746274	9.806375
7.532424	630.067959	9.811392
7.735190	637.193421	9.816410
7.650358	639.188137	9.821427
7.602191	641.575540	9.826445
7.768825	644.322256	9.831463
7.558324	654.586318	9.836480
7.749050	637.041659	9.841498
7.626736	654.185934	9.846515
7.562466	646.006690	9.851533
7.972055	630.614541	9.856551
7.443997	644.901597	9.861568
7.817683	644.810481	9.866586
7.768840	642.817704	9.871603
7.604536	651.108941	9.876621
8.074484	654.566222	9.881639
7.783849	651.785502	9.886656
8.297707	672.312903	9.891674
8.297298	664.005696	9.896691
7.966018	658.278296	9.901709
8.066401	645.384517	9.906727
7.823637	660.982360	9.911744
8.181788	650.735445	9.916762
8.197754	653.219713	9.921779
7.899248	659.184943	9.926797
7.952040	648.465851	9.931815
8.016296	659.158144	9.936832
7.947482	656.273456	9.941850
8.136748	653.656398	9.946867
7.736857	665.108539	9.951885
8.039983	655.585937	9.956903
7.934315	651.642280	9.961920
8.176688	650.253423	9.966938
8.117124	645.432526	9.971955
7.878526	651.538514	9.976973
8.015252	647.153006	9.981991
8.035493	646.656408	9.987008
8.095448	641.613535	9.992026
8.150722	649.703949	9.997043
8.088285	647.645714	10.002061
8.208822	650.941582	10.007079
8.001617	655.892301	10.012096
8.429493	656.662149	10.017114
8.220905	654.807461	10.022131
7.445458	664.706213	10.027149
8.077580	678.011268	10.032167
8.034108	680.913653	10.037184
8.254109	679.410402	10.042202
8.353331	675.267851	10.047219
8.146564	680.190755	10.052237
8.345054	672.816837	10.057255
8.519774	678.888287	10.062272
8.387488	664.415126	10.067290
8.227951	649.907119	10.072307
7.976659	658.399217	10.077325
7.938938	656.402140	10.082343
8.181425	671.052149	10.087360
8.107840	686.521882	10.092378
8.503329	684.230418	10.097395
8.161298	687.164626	10.102413
8.541702	682.301025	10.107431
7.846681	686.680222	10.112448
8.114549	690.211056	10.117466
8.594348	682.240450	10.122483
8.176294	690.377320	10.127501
8.318642	686.692319	10.132519
8.303187	688.467544	10.137536
8.179253	696.940093	10.142554
8.630341	686.381197	10.147571
8.111780	704.711081	10.152589
8.371082	690.069758	10.157607
8.562444	682.689633	10.162624
8.488133	684.953433	10.167642
8.658478	677.311970	10.172659
8.102872	672.621059	10.177677
8.099755	668.099629	10.182695
8.426117	671.053179	10.187712
8.429539	690.636601	10.192730
8.682571	679.137683	10.197747
8.240533	674.025716	10.202765
8.205276	682.916004	10.207783
8.285699	690.092312	10.212800
8.425978	688.907493	10.217818
8.569163	684.271543	10.222835
8.507662	695.736475	10.227853
8.621809	686.781404	10.232871
8.344104	689.837438	10.237888
8.273678	696.068873	10.242906
8.354837	681.786465	10.247923
8.419682	693.175802	10.252941
8.231595	688.548933	10.257959
8.701300	685.383846	10.262976
8.401446	680.676156	10.267994
8.458438	680.441742	10.273011
8.545335	680.987675	10.278029
8.824338	675.276031	10.283047
8.867470	685.869687	10.288064
8.562921	680.328379	10.293082
8.818956	681.126920	10.298099
8.480158	685.836156	10.303117
8.787686	682.361414	10.308135
8.725466	681.246470	10.313152
8.225336	685.320479	10.318170
8.410971	676.126280	10.323187
8.316773	678.960486	10.328205
8.736487	678.747908	10.333223
8.738378	683.484489	10.338240
8.562790	683.441433	10.343258
8.569590	676.609826	10.348275
8.617476	691.125606	10.353293
8.576428	683.996249	10.358311
8.449067	672.868211	10.363328
8.153692	682.988571	10.368346
8.561585	673.666224	10.373363
8.270277	677.942588	10.378381
8.562187	682.874013	10.383399
8.690025	674.154242	10.388416
8.834087	692.349222	10.393434
8.620369	680.465511	10.398451
8.208309	689.374279	10.403469
8.785954	699.081925	10.408487
8.729999	697.056563	10.413504
8.870292	701.254328	10.418522
9.100757	705.194029	10.423539
8.788151	704.865798	10.428557
8.694726	687.456310	10.433575
8.608855	681.488383	10.438592
8.643583	695.279211	10.443610
8.865222	696.380332	10.448627
8.851936	696.776907	10.453645
8.383385	703.861493	10.458663
8.679687	707.224276	10.463680
8.764809	691.069594	10.468698
8.791361	694.362109	10.473715
8.511204	707.489462	10.478733
8.400612	704.966034	10.483751
8.632175	702.472663	10.488768
8.719358	714.983120	10.493786
8.325221	700.549851	10.498803
8.714233	718.563366	10.503821
8.793809	730.201530	10.508839
9.266254	742.278529	10.513856
8.876832	740.088325	10.518874
8.909962	746.763806	10.523891
8.866692	746.817269	10.528909
8.932860	744.440479	10.533927
9.025665	742.075032	10.538944
9.055492	745.808965	10.543962
9.548212	728.437880	10.548979
9.214275	721.011594	10.553997
9.011599	709.244519	10.559015
8.921115	713.125272	10.564032
8.921315	705.803591	10.569050
9.123705	711.275904	10.574067
8.759576	720.671071	10.579085
8.781434	705.008533	10.584103
9.296311	708.739847	10.589120
8.885030	716.782911	10.594138
9.001037	702.784633	10.599155
8.914361	708.844971	10.604173
8.895551	709.663544	10.609191
9.187972	721.768505	10.614208
9.265428	742.976768	10.619226
9.213367	721.065737	10.624243
8.878640	712.929871	10.629261
9.100808	733.891314	10.634279
9.093956	721.360012	10.639296
9.220096	731.425902	10.644314
8.874178	720.855704	10.649331
9.074051	735.229402	10.654349
8.859532	739.815674	10.659367
8.909136	735.517262	10.664384
8.862909	747.679189	10.669402
8.965937	736.499552	10.674419
8.862853	735.950607	10.679437
8.735869	740.461204	10.684455
9.105559	741.978631	10.689472
8.925017	737.362507	10.694490
9.262773	739.584889	10.699507
9.188140	754.099128	10.704525
8.971689	762.884882	10.709543
9.501047	761.522494	10.714560
9.254962	777.380997	10.719578
9.350626	770.047445	10.724595
9.275919	770.051684	10.729613
9.247125	760.567336	10.734631
9.596708	754.725418	10.739648
9.208594	754.048507	10.744666
9.414337	737.912222	10.749683
9.078744	739.671373	10.754701
9.113208	738.603428	10.759719
9.432336	741.396602	10.764736
9.258406	758.547949	10.769754
9.621148	750.252029	10.774771
9.522803	748.242620	10.779789
9.176471	743.702405	10.784807
9.469564	741.439466	10.789824
9.267454	745.025049	10.794842
9.352770	728.260070	10.799859
9.306739	737.581719	10.804877
9.159395	767.854392	10.809895
9.334810	762.703537	10.814912
9.362062	754.127781	10.819930
9.437378	754.420558	10.824947
9.484817	758.488237	10.829965
9.080639	745.597059	10.834983
9.320977	773.041505	10.840000
9.532439	774.305604	10.845018
9.708528	757.326416	10.850035
9.496352	758.363133	10.855053
9.586569	762.462713	10.860071
9.476586	759.014339	10.865088
9.280840	762.810746	10.870106
9.794246	765.912507	10.875123
9.755094	766.719389	10.880141
9.243303	762.071398	10.885159
9.667021	767.556951	10.890176
9.568275	772.194757	10.895194
9.832577	775.411491	10.900211
9.689188	771.399837	10.905229
9.487074	778.806506	10.910247
9.575937	763.977766	10.915264
9.489401	772.684291	10.920282
9.666596	766.109179	10.925299
9.937369	762.699244	10.930317
9.591504	763.807848	10.935335
9.299693	755.492654	10.940352
9.372052	769.484379	10.945370
9.686765	763.390883	10.950387
9.605821	768.711846	10.955405
9.365796	767.122529	10.960423
9.602015	762.665242	10.965440
9.447227	772.428136	10.970458
9.666071	765.052582	10.975475
9.265431	773.499356	10.980493
9.379975	768.395363	10.985511
9.523618	758.935267	10.990528
9.550848	779.001198	10.995546
9.740565	786.192653	11.000563
9.918690	800.142916	11.005581
9.612770	805.256821	11.010599
9.939318	806.979872	11.015616
9.829801	807.276132	11.020634
9.770932	802.990608	11.025651
9.889181	806.576995	11.030669
9.450906	809.106927	11.035687
9.722051	811.173034	11.040704
9.635379	807.371547	11.045722
9.504630	807.097104	11.050739
9.787865	803.241969	11.055757
9.659663	817.226336	11.060775
9.760209	806.629043	11.065792
9.657448	807.815370	11.070810
9.753910	806.583856	11.075827
9.818268	805.997594	11.080845
9.837882	799.458449	11.085863
9.670355	799.915056	11.090880
9.875867	802.566316	11.095898
9.843896	806.478459	11.100915
9.956086	795.404431	11.105933
9.864199	805.861947	11.110951
10.382726	804.703279	11.115968
10.194617	810.278046	11.120986
9.933445	807.669759	11.126003
10.127364	792.921743	11.131021
9.588422	800.483180	11.136039
9.791194	798.067865	11.141056
9.756838	806.547321	11.146074
10.002436	826.024962	11.151091
10.136617	825.497227	11.156109
10.139356	836.897131	11.161127
10.117118	825.744427	11.166144
10.130442	823.967298	11.171162
10.093349	823.242218	11.176179
10.038330	810.262780	11.181197
9.538237	806.326300	11.186215
9.940173	831.146173	11.191232
10.096117	826.889994	11.196250
10.139457	833.990228	11.201267
10.120788	831.734315	11.206285
10.059924	833.968361	11.211303
10.071439	826.031473	11.216320
10.129641	825.870859	11.221338
10.065313	829.538694	11.226355
10.544250	830.830730	11.231373
10.145697	825.623549	11.236391
10.266209	824.509396	11.241408
10.390801	835.650522	11.246426
10.088053	821.653140	11.251443
10.390976	824.207710	11.256461
10.398625	824.671289	11.261479
10.277217	832.175847	11.266496
10.230816	829.660586	11.271514
10.440348	832.896913	11.276531
10.538208	838.768764	11.281549
10.085994	833.807415	11.286567
10.319072	828.387998	11.291584
10.505146	826.479977	11.296602
10.210633	830.519848	11.301619
10.505721	813.794015	11.306637
10.391563	820.486192	11.311655
10.356590	806.694627	11.316672
10.303557	801.831467	11.321690
10.079207	798.105874	11.326707
10.347031	802.980207	11.331725
10.337580	817.274421	11.336743
10.601891	828.106380	11.341760
10.510829	824.598279	11.346778
10.210706	829.510875	11.351795
10.504255	825.923668	11.356813
10.456550	834.285877	11.361831
10.660653	832.397510	11.366848
10.427151	823.466547	11.371866
10.398704	832.846361	11.376883
10.349118	825.302969	11.381901
10.090911	830.598925	11.386919
10.085855	836.643561	11.391936
10.108836	830.088101	11.396954
10.299808	828.069348	11.401971
10.572366	827.043632	11.406989
10.465324	842.342802	11.412007
10.181825	834.464403	11.417024
10.605840	827.425028	11.422042
10.342392	842.886339	11.427059
10.525217	834.138398	11.432077
10.349413	820.116201	11.437095
10.296658	827.546628	11.442112
10.822688	838.862320	11.447130
10.410795	840.834155	11.452147
10.743007	845.738307	11.457165
10.823401	852.325132	11.462183
10.534325	831.916737	11.467200
11.070464	834.274136	11.472218
10.387574	837.104983	11.477235
10.579058	820.006568	11.482253
10.366907	842.298965	11.487271
10.805801	852.450038	11.492288
10.737014	854.608244	11.497306
10.357356	856.692057	11.502323
11.014635	845.886023	11.507341
10.844369	857.165738	11.512359
10.524759	851.868645	11.517376
10.855241	846.680820	11.522394
10.521970	863.671343	11.527411
11.080583	857.407213	11.532429
10.822193	853.125615	11.537447
10.705202	856.162308	11.542464
10.903140	852.489829	11.547482
10.679777	852.989616	11.552499
10.809742	862.984499	11.557517
10.640894	867.031167	11.562535
10.637671	854.087023	11.567552
11.120528	845.309963	11.572570
10.497311	861.034745	11.577587
10.803125	864.932120	11.582605
10.864389	864.583827	11.587623
10.918862	869.437542	11.592640
10.926567	862.506310	11.597658
10.643743	860.596848	11.602675
10.761654	872.960451	11.607693
10.766628	866.987183	11.612711
10.677513	868.158171	11.617728
11.049282	856.360709	11.622746
10.759877	863.786370	11.627763
10.564256	863.576771	11.632781
10.708508	864.003015	11.637799
10.757603	867.788903	11.642816
11.319410	863.044260	11.647834
10.915224	872.090981	11.652851
11.117245	856.193926	11.657869
10.846177	863.491775	11.662887
10.931476	871.864993	11.667904
11.169405	877.215863	11.672922
11.164520	885.227283	11.677939
11.126342	878.198526	11.682957
10.985922	869.370835	11.687975
10.812086	871.120294	11.692992
11.349530	886.125339	11.698010
11.374332	890.161071	11.703027
11.382143	870.671708	11.708045
11.134434	860.377162	11.713063
11.107779	851.465338	11.718080
11.057803	861.995775	11.723098
10.962754	857.535044	11.728115
11.219075	862.674441	11.733133
11.436447	881.054051	11.738151
11.138795	865.691057	11.743168
11.421449	863.038456	11.748186
11.052482	869.900200	11.753203
11.338668	856.810213	11.758221
11.203363	843.409246	11.763239
11.192530	855.029085	11.768256
11.232424	843.828017	11.773274
11.167222	861.216190	11.778291
11.442338	869.984541	11.783309
11.398814	864.699290	11.788327
11.319288	865.008998	11.793344
11.547331	853.235092	11.798362
11.193805	864.038096	11.803379
11.319088	863.961853	11.808397
11.410307	857.325824	11.813415
11.117979	854.557451	11.818432
11.551955	854.361506	11.823450
11.227266	864.703721	11.828467
11.067934	861.643138	11.833485
11.459047	865.676195	11.838503
11.514633	881.559546	11.843520
11.469717	880.609022	11.848538
11.404508	884.656085	11.853555
11.203297	881.154660	11.858573
11.583231	888.458505	11.863591
11.360313	892.732581	11.868608
11.875713	889.961606	11.873626
11.510827	875.063376	11.878643
11.383626	858.285253	11.883661
11.408069	867.951770	11.888679
11.701265	882.386648	11.893696
11.795315	862.242602	11.898714
11.303573	872.346724	11.903731
11.520898	869.500031	11.908749
11.586602	880.544148	11.913767
11.443207	894.341659	11.918784
11.511904	883.684824	11.923802
11.471477	894.050346	11.928819
11.387314	892.485349	11.933837
11.573640	893.694666	11.938855
11.857042	894.996191	11.943872
11.651754	882.730187	11.948890
11.524978	895.505047	11.953907
11.899280	900.534621	11.958925
11.740857	890.373307	11.963943
11.544195	903.184128	11.968960
11.775486	889.031515	11.973978
11.349646	898.143236	11.978995
11.677941	900.086840	11.984013
11.641045	893.659534	11.989031
11.431381	897.241774	11.994048
11.453412	887.040604	11.999066
11.603065	897.404831	12.004083
11.687772	887.920937	12.009101
11.675430	878.302914	12.014119
11.443854	883.298179	12.019136
11.346734	883.246683	12.024154
11.584418	899.141291	12.029171
11.971878	910.619185	12.034189
11.925951	906.431574	12.039207
12.082082	915.563257	12.044224
11.832769	917.233477	12.049242
11.939933	915.048573	12.054259
11.834467	913.972249	12.059277
11.944892	913.840400	12.064295
11.689038	912.705281	12.069312
12.116535	913.428167	12.074330
12.095479	915.742246	12.079347
12.175027	911.214464	12.084365
11.949741	904.454567	12.089383
11.675628	896.335846	12.094400
12.216369	903.489129	12.099418
12.058836	908.508184	12.104435
11.927633	907.965159	12.109453
12.100764	896.425257	12.114471
11.852135	905.323281	12.119488
11.941226	913.991711	12.124506
11.968339	913.256016	12.129523
11.862976	908.845982	12.134541
12.060068	913.133124	12.139559
11.879983	909.726413	12.144576
11.936378	902.769600	12.149594
11.845294	917.412281	12.154611
12.099697	914.016236	12.159629
12.219621	915.703970	12.164647
11.868170	918.910500	12.169664
12.042150	921.660972	12.174682
12.099553	914.447337	12.179699
12.080606	922.784865	12.184717
12.521430	923.978699	12.189735
12.136802	922.142538	12.194752
12.025913	924.832427	12.199770
12.212170	920.424388	12.204787
11.850804	921.489411	12.209805
12.273771	926.215528	12.214823
12.040017	918.933096	12.219840
11.993829	917.684405	12.224858
12.287435	917.512443	12.229875
12.124571	917.258855	12.234893
12.374839	919.493261	12.239911
12.168586	934.754890	12.244928
12.347003	946.675949	12.249946
12.498673	941.587905	12.254963
12.342102	940.062620	12.259981
12.187594	937.318692	12.264999
12.316887	948.651513	12.270016
12.481758	945.176768	12.275034
12.331496	942.675208	12.280051
12.353487	958.283528	12.285069
12.466045	945.065098	12.290087
12.448538	953.762975	12.295104
12.338557	948.083430	12.300122
12.623110	941.603771	12.305139
12.496910	936.339637	12.310157
12.547434	935.098778	12.315175
12.314934	932.910563	12.320192
12.568044	929.567278	12.325210
12.312103	941.914974	12.330227
11.870897	942.837706	12.335245
12.326782	936.786551	12.340263
12.272681	942.759623	12.345280
12.322945	938.734228	12.350298
12.874874	944.196985	12.355315
12.308355	931.223835	12.360333
12.415556	940.108935	12.365351
12.528936	938.996642	12.370368
12.444875	939.500769	12.375386
12.964573	937.535831	12.380403
12.850688	949.214889	12.385421
12.788304	938.490519	12.390439
12.554082	933.505611	12.395456
12.825133	932.544201	12.400474
13.189831	933.692161	12.405491
12.840495	932.420938	12.410509
12.953160	936.206769	12.415527
12.760837	931.949265	12.420544
12.366421	929.684084	12.425562
12.473886	928.951249	12.430579
12.838558	935.542206	12.435597
13.103928	930.790633	12.440615
12.917357	944.838788	12.445632
12.635780	947.073699	12.450650
12.972050	946.155440	12.455667
12.761106	949.450746	12.460685
12.975174	945.502200	12.465703
12.831883	951.511862	12.470720
12.895419	949.628208	12.475738
12.795265	943.682321	12.480755
12.607438	945.964131	12.485773
13.137971	931.079662	12.490791
12.824455	945.150369	12.495808
12.531802	939.691927	12.500826
13.040332	939.706066	12.505843
12.779472	937.889405	12.510861
13.012638	938.700302	12.515879
12.832127	947.063755	12.520896
12.514278	932.416512	12.525914
12.635407	947.535879	12.530931
12.796626	956.906470	12.535949
13.047901	963.656509	12.540967
12.848367	973.187102	12.545984
13.207914	976.101375	12.551002
13.500191	976.357516	12.556019
13.113348	968.018645	12.561037
13.212117	947.401935	12.566055
12.761456	945.163169	12.571072
12.882892	955.048713	12.576090
13.343632	947.051797	12.581107
13.252036	973.912091	12.586125
13.239837	963.443146	12.591143
12.936957	949.318721	12.596160
12.811436	957.012375	12.601178
13.018115	966.485480	12.606195
13.334191	966.919351	12.611213
13.600150	956.508759	12.616231
13.078005	957.994383	12.621248
13.202907	966.127090	12.626266
13.320643	968.905564	12.631283
13.268111	968.048601	12.636301
13.242159	966.654852	12.641319
13.176089	973.912972	12.646336
13.285129	966.661454	12.651354
13.320202	966.261984	12.656371
13.326893	968.178046	12.661389
13.063781	959.283388	12.666407
12.949620	962.478663	12.671424
13.245181	974.289652	12.676442
13.666218	968.912047	12.681459
13.497138	976.802641	12.686477
13.525275	971.654306	12.691495
13.633246	978.737825	12.696512
13.262566	966.889573	12.701530
13.627614	974.502955	12.706547
13.135918	970.224845	12.711565
13.195528	981.920132	12.716583
13.128623	975.185597	12.721600
13.178059	961.289114	12.726618
13.516566	965.247439	12.731635
13.040302	967.786726	12.736653
13.265469	969.273048	12.741671
13.614678	990.395314	12.746688
13.886892	983.541951	12.751706
13.596420	975.092482	12.756723
13.314875	980.138744	12.761741
13.405404	983.450961	12.766759
13.732082	991.982748	12.771776
13.656533	996.437782	12.776794
13.844860	993.982410	12.781811
13.859702	993.719332	12.786829
13.607794	977.701330	12.791847
13.733469	977.351838	12.796864
13.263449	969.157006	12.801882
13.568775	972.848617	12.806899
13.721097	992.521381	12.811917
13.681026	991.857798	12.816935
13.780622	991.922982	12.821952
13.560495	991.327533	12.826970
13.963268	989.784405	12.831987
13.547270	999.551933	12.837005
13.674468	993.397224	12.842023
13.712575	993.488118	12.847040
13.573963	995.584862	12.852058
13.669189	996.230989	12.857075
13.520836	995.922450	12.862093
13.496002	998.874268	12.867111
13.668905	988.636093	12.872128
13.644210	998.369857	12.877146
13.750315	996.202634	12.882163
13.638306	1002.813347	12.887181
14.012222	1004.938567	12.892199
13.989972	1019.868544	12.897216
13.687105	1023.841943	12.902234
13.939024	1010.546696	12.907251
14.109279	1013.539690	12.912269
14.007357	1026.482571	12.917287
14.154478	1021.613525	12.922304
13.996406	1024.902866	12.927322
14.542473	1009.375699	12.932339
14.071069	996.917005	12.937357
13.841449	996.719517	12.942375
14.057365	991.880247	12.947392
13.673312	991.392387	12.952410
14.066866	1007.948050	12.957427
13.935186	1015.118229	12.962445
13.989407	1020.038360	12.967463
14.396417	1017.481503	12.972480
14.201061	1012.731249	12.977498
14.355174	1010.301801	12.982515
14.457097	1023.688082	12.987533
13.999452	1007.548955	12.992551
13.897586	1011.506651	12.997568
14.244429	1017.459551	13.002586
14.187707	1019.772454	13.007603
14.018659	1036.514018	13.012621
13.826603	1024.540352	13.017639
14.077911	1024.248826	13.022656
13.843105	1033.180460	13.027674
13.909339	1022.441862	13.032691
14.019474	1026.883540	13.037709
13.841885	1027.001615	13.042727
14.059715	1041.833485	13.047744
14.464304	1045.803939	13.052762
14.771866	1048.971660	13.057779
14.768846	1048.752274	13.062797
14.965884	1029.287140	13.067815
15.042454	1028.000637	13.072832
14.418686	1017.519351	13.077850
14.766646	1012.562796	13.082867
14.748393	1008.404241	13.087885
14.570897	1013.150689	13.092903
14.594274	1003.452484	13.097920
14.512860	1004.077416	13.102938
14.635121	996.187385	13.107955
14.755057	1007.394453	13.112973
14.851530	1011.556934	13.117991
14.668261	992.624104	13.123008
14.586681	985.554447	13.128026
14.590136	979.022028	13.133043
14.367264	978.452030	13.138061
14.472654	981.499234	13.143079
14.619312	985.279853	13.148096
14.819550	1013.415201	13.153114
14.678092	1005.519343	13.158131
14.673871	996.629511	13.163149
14.787259	974.843607	13.168167
15.013465	981.118938	13.173184
14.506501	984.708603	13.178202
14.760090	975.876556	13.183219
14.534457	977.900882	13.188237
14.429129	980.428668	13.193255
14.958547	984.089942	13.198272
14.620567	996.439626	13.203290
14.924789	1001.490065	13.208307
14.983452	1001.905265	13.213325
14.804456	986.670942	13.218343
14.710182	972.449041	13.223360
14.607502	993.216530	13.228378
15.021584	989.799986	13.233395
14.827109	1010.415371	13.238413
14.652629	1012.498954	13.243431
15.025977	1002.138093	13.248448
14.653253	1010.547515	13.253466
14.745673	1012.266177	13.258483
14.709690	1010.812676	13.263501
14.737526	1015.974726	13.268519
14.772578	1010.840194	13.273536
14.417324	1020.755547	13.278554
14.835523	1017.457982	13.283571
14.741463	1020.077204	13.288589
14.567492	1022.660624	13.293607
14.918826	1027.851491	13.298624
15.006412	1044.843521	13.303642
15.210373	1040.000504	13.308659
15.617027	1037.351590	13.313677
14.962347	1036.826770	13.318695
15.412721	1026.742094	13.323712
15.282156	1027.134637	13.328730
15.296326	1012.950281	13.333747
15.153031	1011.333439	13.338765
14.833701	1002.418523	13.343783
15.022418	1006.049504	13.348800
15.095798	1021.359482	13.353818
15.440716	1024.831211	13.358835
15.404591	1028.995927	13.363853
14.979295	1011.520757	13.368871
15.606987	1015.372458	13.373888
15.546789	1016.911650	13.378906
15.508564	1003.595862	13.383923
15.410644	1002.526552	13.388941
14.972662	1006.497671	13.393959
15.328758	1003.521936	13.398976
15.177876	1014.035890	13.403994
15.149283	1019.504660	13.409011
15.448630	1019.861980	13.414029
15.489886	1037.750886	13.419047
15.156159	1022.358662	13.424064
14.856070	1028.158672	13.429082
15.317799	1027.890041	13.434099
15.438816	1033.964307	13.439117
14.996991	1037.081875	13.444135
15.544021	1032.816319	13.449152
15.344279	1042.021843	13.454170
15.340259	1033.781460	13.459187
15.593233	1037.646476	13.464205
15.475895	1043.427707	13.469223
15.549607	1046.473467	13.474240
15.443075	1044.465962	13.479258
15.566006	1042.554966	13.484275
15.583749	1042.029638	13.489293
15.364058	1046.174701	13.494311
16.080754	1041.693536	13.499328
15.791059	1040.644695	13.504346
15.469174	1044.817667	13.509363
15.931941	1033.441577	13.514381
15.542560	1036.250920	13.519399
15.846517	1029.625915	13.524416
15.776728	1043.153760	13.529434
15.450570	1045.854247	13.534451
16.101819	1041.037693	13.539469
15.685631	1040.277035	13.544487
16.074996	1029.491923	13.549504
16.061080	1035.927213	13.554522
15.322883	1044.006756	13.559539
15.727266	1033.352997	13.564557
15.443255	1040.222821	13.569575
15.627296	1037.907695	13.574592
15.398071	1037.742420	13.579610
15.752523	1055.378244	13.584627
15.616369	1069.961599	13.589645
15.829322	1081.376938	13.594663
16.105410	1075.970108	13.599680
16.228612	1073.012967	13.604698
16.192574	1069.733771	13.609715
16.065142	1067.603555	13.614733
16.300955	1046.609002	13.619751
16.059963	1034.072641	13.624768
16.333569	1040.374213	13.629786
16.224579	1037.321809	13.634803
16.637623	1031.034231	13.639821
16.048858	1041.257630	13.644839
16.494581	1033.454853	13.649856
16.297661	1027.575112	13.654874
16.265844	1031.251399	13.659891
16.538877	1028.884763	13.664909
16.037130	1032.828244	13.669927
16.103657	1023.554717	13.674944
15.897902	1031.696439	13.679962
15.961875	1030.108523	13.684979
16.321168	1027.377295	13.689997
15.978340	1033.082614	13.695015
16.099725	1026.837921	13.700032
16.140434	1028.709203	13.705050
15.872249	1040.208546	13.710067
16.005916	1038.560300	13.715085
16.003113	1031.973391	13.720103
16.152900	1036.418163	13.725120
16.378422	1046.910483	13.730138
16.587576	1044.692961	13.735155
16.701513	1035.746382	13.740173
16.186476	1043.613090	13.745191
16.109640	1043.659209	13.750208
16.341980	1048.270826	13.755226
16.311482	1067.114978	13.760243
16.554404	1067.456824	13.765261
16.408603	1063.595666	13.770279
16.540562	1059.448882	13.775296
16.490072	1058.041073	13.780314
16.491939	1059.318675	13.785331
16.506371	1048.232770	13.790349
16.666467	1063.761494	13.795367
16.655194	1058.245489	13.800384
16.600659	1062.647668	13.805402
16.823123	1057.112523	13.810419
16.850779	1053.011319	13.815437
16.489671	1026.330526	13.820455
16.320503	1031.171847	13.825472
16.675104	1044.452032	13.830490
16.820203	1067.762910	13.835507
16.563505	1056.134102	13.840525
16.173950	1061.111442	13.845543
16.430400	1061.937393	13.850560
16.579856	1055.122785	13.855578
16.674447	1063.726818	13.860595
16.638109	1065.670473	13.865613
16.209009	1068.895770	13.870631
16.769188	1066.965655	13.875648
16.635317	1070.458257	13.880666
16.613723	1061.507096	13.885683
16.401904	1052.132328	13.890701
16.740666	1075.742856	13.895719
16.900655	1089.209152	13.900736
17.178047	1092.320264	13.905754
17.015748	1095.016513	13.910771
16.895161	1087.281508	13.915789
16.931343	1089.018330	13.920807
16.890298	1089.829083	13.925824
17.045514	1090.500925	13.930842
17.067886	1090.591467	13.935859
17.046438	1089.365835	13.940877
16.836090	1073.629600	13.945895
17.079566	1088.710190	13.950912
17.155594	1097.147848	13.955930
17.089761	1094.191041	13.960947
17.220835	1088.208854	13.965965
17.196226	1092.725960	13.970983
16.660743	1082.931505	13.976000
17.204647	1091.357580	13.981018
17.084847	1094.828771	13.986035
17.319004	1087.472478	13.991053
17.087421	1089.287401	13.996071
17.453308	1088.967098	14.001088
17.393606	1091.661154	14.006106
17.017091	1100.719772	14.011123
17.312666	1093.764680	14.016141
17.070270	1090.029499	14.021159
17.211075	1095.687002	14.026176
17.351728	1084.092297	14.031194
17.144317	1090.608397	14.036211
17.273843	1092.693320	14.041229
17.430255	1082.968948	14.046247
17.157915	1085.820169	14.051264
17.478447	1093.185298	14.056282
17.214753	1091.201199	14.061299
17.203201	1096.281218	14.066317
17.243431	1095.062516	14.071335
17.375615	1079.769199	14.076352
17.657319	1085.884638	14.081370
17.385984	1099.292122	14.086387
17.334251	1092.455241	14.091405
17.004351	1103.998880	14.096423
16.792805	1090.715005	14.101440
17.656644	1119.517929	14.106458
17.585505	1124.599340	14.111475
18.083332	1122.736208	14.116493
18.060112	1120.380134	14.121511
17.846242	1110.933437	14.126528
17.989412	1101.564140	14.131546
17.445161	1091.699879	14.136563
17.629447	1090.923244	14.141581
17.727906	1090.807542	14.146599
17.687113	1097.276036	14.151616
17.776638	1087.490481	14.156634
18.041149	1086.277034	14.161651
18.066084	1075.174219	14.166669
17.985273	1081.240918	14.171687
17.591667	1085.039789	14.176704
18.222619	1078.882693	14.181722
17.833165	1086.561570	14.186739
17.834099	1088.617554	14.191757
18.150087	1085.702753	14.196775
17.971383	1079.558212	14.201792
17.991378	1082.932098	14.206810
17.882427	1088.720620	14.211827
17.677593	1087.834103	14.216845
17.596906	1082.586803	14.221863
17.466670	1089.790828	14.226880
17.846079	1081.381364	14.231898
17.627349	1087.563165	14.236915
17.812374	1079.627685	14.241933
18.174414	1097.536081	14.246951
17.825726	1103.530735	14.251968
18.020433	1106.039861	14.256986
17.954572	1129.826374	14.262003
18.085262	1116.161956	14.267021
18.296139	1113.880567	14.272039
18.195215	1123.717545	14.277056
18.141085	1111.611587	14.282074
17.825516	1108.433291	14.287091
17.988332	1111.895769	14.292109
18.128596	1113.924795	14.297127
17.979926	1115.043645	14.302144
18.064495	1105.455718	14.307162
17.948229	1118.510873	14.312179
18.028312	1124.939524	14.317197
17.902908	1116.554810	14.322215
17.785612	1106.376912	14.327232
18.476981	1115.808394	14.332250
18.257732	1132.630198	14.337267
18.528396	1140.534414	14.342285
18.640484	1128.034299	14.347303
18.411918	1118.916944	14.352320
18.895535	1125.871339	14.357338
18.599413	1114.207078	14.362355
18.462893	1116.943553	14.367373
18.489165	1105.402964	14.372391
18.262463	1109.674970	14.377408
18.451770	1107.968712	14.382426
18.613917	1108.313278	14.387443
18.637406	1097.810396	14.392461
18.863586	1102.860578	14.397479
18.682231	1107.089072	14.402496
18.707495	1099.937149	14.407514
18.393949	1117.217166	14.412531
18.391917	1107.870679	14.417549
18.815153	1105.540815	14.422567
18.324306	1117.752497	14.427584
18.897256	1122.234043	14.432602
18.776173	1126.375625	14.437619
18.692163	1123.936501	14.442637
19.087330	1123.763304	14.447655
18.422405	1123.799929	14.452672
18.538788	1114.329162	14.457690
18.726528	1124.851790	14.462707
19.053923	1124.365827	14.467725
18.910819	1130.084036	14.472743
18.596873	1141.292046	14.477760
18.935222	1124.528615	14.482778
19.130914	1138.579515	14.487795
18.666864	1137.846049	14.492813
18.903246	1135.068195	14.497831
19.295523	1139.909867	14.502848
19.314431	1133.806653	14.507866
18.869104	1131.724434	14.512883
18.694035	1135.646825	14.517901
18.809250	1129.216722	14.522919
18.651137	1137.331142	14.527936
18.770658	1126.920031	14.532954
18.658525	1121.633630	14.537971
18.438921	1135.178243	14.542989
18.904450	1121.537609	14.548007
18.628837	1146.509815	14.553024
19.237087	1148.688050	14.558042
19.017394	1149.013840	14.563059
19.467840	1156.956259	14.568077
19.397935	1153.173861	14.573095
19.173920	1163.545694	14.578112
19.376414	1157.754798	14.583130
19.614924	1154.296967	14.588147
19.187310	1141.271160	14.593165
19.528814	1124.177336	14.598183
19.426744	1119.857037	14.603200
19.118784	1117.226414	14.608218
19.264652	1131.429219	14.613235
19.209980	1118.234339	14.618253
19.515706	1138.185830	14.623271
19.144141	1159.764395	14.628288
19.533374	1154.914541	14.633306
19.756767	1148.613184	14.638323
19.562387	1138.241539	14.643341
19.373194	1125.414892	14.648359
19.401228	1140.134740	14.653376
19.435857	1140.727510	14.658394
19.907198	1148.484807	14.663411
19.556292	1143.530134	14.668429
19.502189	1137.739332	14.673447
19.797497	1155.991646	14.678464
19.991345	1135.963210	14.683482
19.887801	1131.331191	14.688499
19.631647	1130.632652	14.693517
19.893563	1126.998151	14.698535
19.503557	1120.567301	14.703552
19.540474	1127.231594	14.708570
19.517107	1113.654634	14.713587
19.626159	1109.569881	14.718605
19.426750	1126.527944	14.723623
19.365791	1140.025877	14.728640
19.686601	1142.844434	14.733658
19.760774	1151.234601	14.738675
19.543644	1150.537485	14.743693
19.857484	1141.027970	14.748711
19.863849	1162.511610	14.753728
19.782209	1152.030590	14.758746
19.702595	1147.698897	14.763763
19.485241	1153.063299	14.768781
19.936681	1145.834039	14.773799
19.829618	1152.891962	14.778816
20.009949	1157.794054	14.783834
19.906498	1166.372219	14.788851
19.953096	1165.679742	14.793869
20.649456	1168.835003	14.798887
20.025765	1172.190691	14.803904
20.019249	1153.744715	14.808922
20.122961	1147.896535	14.813939
19.913829	1155.742666	14.818957
20.226567	1169.520944	14.823975
20.020184	1187.191143	14.828992
20.072142	1187.914103	14.834010
20.183268	1182.912983	14.839027
19.902725	1191.191539	14.844045
20.620306	1184.765005	14.849063
20.576154	1182.652306	14.854080
20.425985	1187.626540	14.859098
20.446797	1172.598742	14.864115
20.158235	1178.403005	14.869133
20.209138	1188.990212	14.874151
20.536892	1183.833627	14.879168
20.494606	1182.708463	14.884186
20.406499	1181.070871	14.889203
20.193087	1186.502339	14.894221
20.371628	1189.665627	14.899239
20.289467	1179.657045	14.904256
20.281248	1169.513632	14.909274
20.697713	1173.951771	14.914291
20.567726	1179.502502	14.919309
20.678818	1172.328095	14.924327
20.606178	1171.416972	14.929344
20.592199	1178.901191	14.934362
20.903983	1175.689475	14.939379
20.645014	1166.219295	14.944397
20.677533	1166.514035	14.949415
20.739242	1170.583697	14.954432
20.637645	1171.265703	14.959450
20.919153	1169.421385	14.964467
20.670055	1173.605785	14.969485
20.664044	1169.335730	14.974503
20.787206	1169.622774	14.979520
20.563189	1172.047585	14.984538
20.880482	1168.117943	14.989555
20.948136	1163.496988	14.994573
20.934769	1164.014436	14.999591
20.953002	1179.596637	15.004608
20.846599	1164.672338	15.009626
21.185595	1165.690331	15.014643
20.925671	1171.336142	15.019661
20.868180	1169.089252	15.024679
20.887509	1171.566158	15.029696
21.079720	1174.683293	15.034714
20.876730	1164.320532	15.039731
20.845114	1170.235654	15.044749
21.118674	1177.572568	15.049767
20.719618	1170.225810	15.054784
21.045372	1173.823557	15.059802
21.086478	1173.186113	15.064819
21.050104	1166.919213	15.069837
20.993207	1173.307341	15.074855
21.027547	1159.716277	15.079872
20.871110	1164.652372	15.084890
21.208840	1162.500778	15.089907
20.878785	1166.639705	15.094925
21.232959	1183.762022	15.099943
21.466657	1194.593591	15.104960
21.733318	1183.456657	15.109978
21.670546	1174.587617	15.114995
21.130739	1162.420166	15.120013
21.310203	1161.008988	15.125031
21.170653	1154.345425	15.130048
21.237019	1166.618193	15.135066
21.431332	1189.121047	15.140083
21.599952	1186.020966	15.145101
21.812785	1179.829200	15.150119
21.861035	1176.316007	15.155136
21.220379	1164.677741	15.160154
21.632821	1152.962688	15.165171
21.405607	1164.997791	15.170189
21.185440	1164.765476	15.175207
21.267375	1174.748227	15.180224
21.698324	1184.903000	15.185242
21.976966	1182.635005	15.190259
21.807710	1190.778653	15.195277
21.825293	1191.131759	15.200295
21.832013	1189.190153	15.205312
21.647842	1196.408060	15.210330
22.183386	1185.736261	15.215347
21.261926	1174.528782	15.220365
21.513575	1178.824499	15.225383
21.787411	1191.467665	15.230400
21.703861	1195.641641	15.235418
21.940543	1192.416353	15.240435
21.971057	1196.066239	15.245453
21.821307	1186.736045	15.250471
22.140800	1199.505118	15.255488
21.539460	1193.463831	15.260506
22.387707	1193.476747	15.265523
22.053778	1201.574592	15.270541
22.211751	1190.764819	15.275559
21.740499	1193.299770	15.280576
21.868322	1192.884377	15.285594
21.957642	1193.266567	15.290611
21.651533	1189.413760	15.295629
21.650596	1192.397684	15.300647
21.819026	1194.670651	15.305664
21.677404	1190.827468	15.310682
22.110391	1179.457767	15.315699
22.038862	1194.664324	15.320717
22.113636	1204.054075	15.325735
22.249186	1214.819213	15.330752
22.445249	1219.413455	15.335770
22.469137	1206.400371	15.340787
22.233015	1206.816265	15.345805
22.649186	1200.900685	15.350823
22.589048	1192.171730	15.355840
22.314793	1190.281672	15.360858
22.407471	1194.796352	15.365875
22.199862	1190.476350	15.370893
22.464798	1178.139491	15.375911
22.467660	1182.996716	15.380928
22.575708	1195.377168	15.385946
22.367697	1190.076080	15.390963
22.452681	1188.763571	15.395981
22.565588	1213.174315	15.400999
22.516180	1205.355845	15.406016
22.667511	1213.510494	15.411034
22.748334	1206.740621	15.416051
22.774303	1213.780918	15.421069
22.632533	1205.709837	15.426087
22.710600	1194.214749	15.431104
22.784962	1200.730978	15.436122
22.768338	1192.831321	15.441139
22.570244	1193.485383	15.446157
22.874758	1196.526296	15.451175
22.629177	1203.642166	15.456192
22.395925	1214.969553	15.461210
22.581680	1209.432154	15.466227
22.824233	1212.890139	15.471245
22.974531	1212.120689	15.476263
22.641929	1213.119569	15.481280
22.785511	1218.391479	15.486298
23.242571	1207.746412	15.491315
22.921977	1210.260800	15.496333
22.843700	1204.854225	15.501351
22.969959	1213.804239	15.506368
22.679220	1208.277874	15.511386
23.051928	1203.681682	15.516403
22.889647	1210.474585	15.521421
22.623231	1216.734977	15.526439
23.086445	1205.347075	15.531456
22.772108	1242.251629	15.536474
22.965989	1237.755441	15.541491
23.368048	1238.281593	15.546509
23.388984	1242.775470	15.551527
23.318094	1241.117312	15.556544
23.106142	1240.198108	15.561562
22.971413	1246.572361	15.566579
23.180751	1250.446019	15.571597
22.955648	1254.193271	15.576615
23.264871	1234.522555	15.581632
23.372370	1240.742029	15.586650
23.655790	1237.279317	15.591667
23.515645	1237.872041	15.596685
23.640428	1237.932080	15.601703
23.296070	1236.395086	15.606720
23.282782	1246.010604	15.611738
23.070400	1239.701707	15.616755
23.297164	1237.837101	15.621773
23.313995	1238.059840	15.626791
23.109653	1234.827709	15.631808
23.263622	1251.702715	15.636826
23.753655	1257.860361	15.641843
23.730056	1264.978351	15.646861
23.826175	1267.460101	15.651879
24.144328	1266.687120	15.656896
23.949349	1258.168571	15.661914
23.724633	1227.312538	15.666931
23.540495	1244.650633	15.671949
23.235618	1238.925244	15.676967
23.585105	1244.083622	15.681984
23.644965	1252.227033	15.687002
23.853153	1258.481640	15.692019
23.925480	1256.638420	15.697037
23.706665	1257.849962	15.702055
23.878916	1255.927049	15.707072
23.727040	1259.033355	15.712090
23.767075	1259.385902	15.717107
23.927776	1266.061292	15.722125
23.851879	1265.950586	15.727143
23.976795	1255.953397	15.732160
23.844115	1259.223633	15.737178
23.832099	1264.368735	15.742195
23.996079	1262.897320	15.747213
24.378093	1281.719033	15.752231
25.172494	1264.472468	15.757248
24.827459	1260.140909	15.762266
24.961222	1246.914976	15.767283
24.688604	1242.538586	15.772301
24.498037	1234.009677	15.777319
24.557569	1216.583072	15.782336
24.548310	1222.956854	15.787354
24.662749	1215.801162	15.792371
24.577537	1226.623456	15.797389
24.604201	1214.173405	15.802407
24.759711	1210.912321	15.807424
24.566623	1224.325485	15.812442
24.383285	1215.653287	15.817459
24.553512	1210.757138	15.822477
24.376308	1223.627402	15.827495
24.578024	1210.760098	15.832512
24.369415	1222.574881	15.837530
24.610370	1218.604109	15.842547
24.523445	1216.443953	15.847565
24.278361	1211.996693	15.852583
24.334380	1211.654377	15.857600
24.165856	1208.195499	15.862618
24.179349	1218.560794	15.867635
24.582907	1219.046152	15.872653
24.558992	1234.910138	15.877671
25.029047	1231.286487	15.882688
25.033861	1234.775103	15.887706
25.004868	1232.581556	15.892723
24.918427	1214.746461	15.897741
24.566573	1214.389865	15.902759
24.949553	1219.351389	15.907776
25.044898	1236.676750	15.912794
25.111822	1228.396589	15.917811
24.572197	1218.162638	15.922829
24.806300	1229.976895	15.927847
25.301584	1228.820760	15.932864
25.167090	1228.796498	15.937882
24.763076	1232.762258	15.942899
24.960346	1232.989820	15.947917
24.802219	1242.705441	15.952935
24.667378	1236.213086	15.957952
24.849271	1232.399490	15.962970
24.928407	1242.492968	15.967987
24.954522	1232.462522	15.973005
24.819188	1246.110416	15.978023
25.124637	1235.342374	15.983040
25.010042	1253.171078	15.988058
24.939124	1266.814447	15.993075
25.338859	1271.188658	15.998093
25.140761	1273.752094	16.003111
25.398475	1278.723119	16.008128
25.453183	1272.739112	16.013146
25.412868	1277.844610	16.018163
25.431659	1261.110021	16.023181
25.161763	1271.999278	16.028199
25.544010	1268.219090	16.033216
25.737382	1264.499245	16.038234
25.303579	1266.547773	16.043251
25.742751	1266.802477	16.048269
25.467656	1264.269925	16.053287
25.818524	1253.672292	16.058304
25.778637	1262.262641	16.063322
25.322540	1258.669213	16.068339
25.841088	1252.467247	16.073357
25.967343	1251.254393	16.078375
25.760603	1259.279682	16.083392
25.585583	1256.760117	16.088410
25.958165	1260.948289	16.093427
26.009595	1245.943111	16.098445
25.862317	1274.824061	16.103463
26.088674	1260.866185	16.108480
26.141456	1266.066515	16.113498
26.311831	1263.811086	16.118515
26.115339	1255.673245	16.123533
25.948764	1252.754902	16.128551
26.123818	1255.490102	16.133568
26.279622	1252.423224	16.138586
25.828059	1251.177527	16.143603
26.244789	1249.195123	16.148621
25.860436	1273.597598	16.153639
25.978311	1252.653745	16.158656
26.079330	1255.660394	16.163674
26.074243	1264.612853	16.168691
26.018278	1259.414943	16.173709
25.993045	1257.881306	16.178727
25.987395	1256.561134	16.183744
26.006507	1263.818501	16.188762
25.592680	1254.355749	16.193779
25.909234	1257.600560	16.198797
25.769695	1284.294148	16.203815
26.122737	1279.940717	16.208832
26.482137	1292.024630	16.213850
26.293250	1293.663844	16.218867
26.354425	1286.463779	16.223885
26.193136	1291.749486	16.228903
26.437075	1302.017709	16.233920
26.537982	1280.715452	16.238938
26.487160	1290.296065	16.243955
26.203631	1291.002629	16.248973
26.453346	1298.240800	16.253991
26.432370	1297.570506	16.259008
26.665644	1302.697524	16.264026
26.832791	1323.773576	16.269043
26.874480	1315.261942	16.274061
26.502307	1291.958219	16.279079
26.744076	1300.745909	16.284096
26.705578	1310.092837	16.289114
26.724044	1316.103268	16.294131
27.347846	1314.475166	16.299149
27.106461	1296.785052	16.304167
26.879542	1283.246696	16.309184
27.169990	1282.179320	16.314202
26.667608	1280.676504	16.319219
26.700016	1278.597000	16.324237
26.953373	1300.982796	16.329255
27.186614	1317.924489	16.334272
27.095581	1306.727694	16.339290
27.171554	1311.124320	16.344307
27.394313	1301.030433	16.349325
27.142981	1279.656286	16.354343
27.056527	1285.682075	16.359360
27.011993	1285.735453	16.364378
27.330839	1300.453651	16.369395
27.350006	1296.183140	16.374413
27.481266	1298.832685	16.379431
27.449084	1288.753970	16.384448
26.961604	1292.329265	16.389466
27.059306	1290.825893	16.394483
27.724176	1297.550248	16.399501
27.582411	1306.314128	16.404519
27.298531	1304.370535	16.409536
27.617987	1300.997510	16.414554
27.692514	1306.631403	16.419571
27.314900	1296.974281	16.424589
27.591298	1294.305910	16.429607
27.593524	1300.126330	16.434624
27.751672	1306.543929	16.439642
27.663367	1305.519261	16.444659
27.438757	1291.024353	16.449677
27.426163	1305.630027	16.454695
27.492549	1306.431109	16.459712
27.755109	1302.476034	16.464730
27.442793	1311.191732	16.469747
27.756984	1308.166180	16.474765
27.608612	1313.588716	16.479783
27.334392	1310.043556	16.484800
27.502429	1311.968624	16.489818
27.265077	1310.739484	16.494835
27.722730	1321.150528	16.499853
28.073819	1326.438178	16.504871
28.103026	1340.654355	16.509888
28.023006	1331.527283	16.514906
28.076645	1330.979087	16.519923
27.967116	1312.836911	16.524941
28.029592	1324.650079	16.529959
27.545782	1333.470300	16.534976
27.920351	1322.257765	16.539994
27.817573	1329.808692	16.545011
28.333724	1323.118383	16.550029
28.227796	1327.813933	16.555047
28.045118	1329.897338	16.560064
28.241918	1324.484630	16.565082
28.251399	1331.393276	16.570099
28.561876	1326.051533	16.575117
28.627866	1327.771056	16.580135
28.182686	1333.693371	16.585152
28.288502	1337.699103	16.590170
28.290153	1327.859816	16.595187
28.209735	1329.509059	16.600205
28.072496	1329.507885	16.605223
28.173407	1357.158575	16.610240
28.368838	1353.502926	16.615258
28.560360	1363.716672	16.620275
28.706223	1357.912621	16.625293
28.876906	1369.500294	16.630311
28.679696	1353.862373	16.635328
28.910400	1362.253754	16.640346
28.691768	1359.044428	16.645363
28.838002	1358.082559	16.650381
29.179092	1354.998624	16.655399
29.017763	1350.802603	16.660416
28.981410	1332.737274	16.665434
28.443918	1335.146402	16.670451
28.599252	1333.748643	16.675469
29.275663	1344.932693	16.680487
29.077195	1361.401558	16.685504
29.573750	1351.345453	16.690522
28.988301	1337.399431	16.695539
29.057334	1325.288894	16.700557
28.908003	1319.764315	16.705575
29.000495	1330.606325	16.710592
29.042609	1340.526877	16.715610
29.068216	1338.579965	16.720627
28.565783	1352.723202	16.725645
28.962817	1356.752459	16.730663
28.589703	1347.265404	16.735680
29.077620	1345.527292	16.740698
28.702808	1354.189769	16.745715
28.974605	1355.635949	16.750733
29.278726	1369.462675	16.755751
29.260869	1372.014254	16.760768
29.636764	1361.657850	16.765786
29.846830	1381.928180	16.770803
29.987733	1372.195167	16.775821
29.668656	1347.910868	16.780839
29.339584	1352.123096	16.785856
29.747598	1341.426996	16.790874
29.731252	1344.547925	16.795891
29.769101	1348.850679	16.800909
29.691546	1333.761430	16.805927
29.312567	1346.511618	16.810944
29.421670	1328.372265	16.815962
29.616645	1361.968199	16.820979
29.946976	1352.935881	16.825997
29.909070	1359.158766	16.831015
29.348267	1375.900484	16.836032
29.886749	1364.631308	16.841050
29.983555	1368.937709	16.846067
29.692327	1377.167547	16.851085
29.624117	1358.410697	16.856103
29.737408	1373.346963	16.861120
29.714537	1373.003115	16.866138
30.000462	1369.259289	16.871155
29.599944	1372.995798	16.876173
29.659681	1371.157007	16.881191
29.803886	1383.761723	16.886208
30.297764	1390.481112	16.891226
29.977928	1408.356114	16.896243
30.387143	1408.241413	16.901261
30.629241	1400.961995	16.906279
30.165228	1392.492356	16.911296
30.119496	1375.284120	16.916314
29.990237	1384.170763	16.921331
30.012964	1389.130465	16.926349
30.319399	1395.640313	16.931367
30.135762	1399.173098	16.936384
30.302336	1403.638036	16.941402
30.281237	1399.018883	16.946419
30.462127	1396.416272	16.951437
30.582044	1396.227543	16.956455
30.334557	1399.856498	16.961472
30.328129	1393.356241	16.966490
30.194503	1401.547648	16.971507
30.032761	1392.888707	16.976525
30.492044	1407.836916	16.981543
30.375958	1430.145387	16.986560
30.736741	1429.974919	16.991578
31.040538	1422.044239	16.996595
31.033450	1416.542963	17.001613
31.143925	1422.076876	17.006631
30.679142	1414.453891	17.011648
31.266926	1405.109153	17.016666
31.255898	1410.028186	17.021683
30.904198	1404.012679	17.026701
30.942508	1399.987564	17.031719
30.907605	1407.700321	17.036736
31.205122	1415.325281	17.041754
31.325489	1424.310835	17.046771
31.232377	1409.266203	17.051789
30.931354	1405.629204	17.056807
30.971166	1409.818083	17.061824
31.220082	1410.967106	17.066842
31.017761	1418.010974	17.071859
30.926176	1428.629766	17.076877
31.185694	1410.216479	17.081895
30.822722	1421.597732	17.086912
31.413897	1416.018063	17.091930
31.461951	1415.667218	17.096947
31.382077	1420.304560	17.101965
31.689903	1414.219231	17.106983
31.138728	1429.082306	17.112000
31.474039	1421.726460	17.117018
31.439163	1417.954544	17.122035
31.428004	1418.621615	17.127053
31.583175	1415.567603	17.132071
31.336576	1415.305994	17.137088
31.636961	1417.950050	17.142106
31.647212	1418.607088	17.147123
31.356250	1428.017852	17.152141
31.408713	1431.797221	17.157159
31.965856	1443.129578	17.162176
31.970966	1445.852547	17.167194
31.861082	1440.641441	17.172211
31.749655	1443.173853	17.177229
32.069515	1454.780240	17.182247
31.798906	1444.481015	17.187264
31.784223	1435.862701	17.192282
31.842427	1445.567894	17.197299
31.971976	1447.635936	17.202317
32.242336	1445.861529	17.207335
31.993987	1450.793418	17.212352
32.374361	1453.054036	17.217370
31.997617	1453.188293	17.222387
32.002633	1440.793795	17.227405
31.993537	1435.792383	17.232423
32.144332	1450.814443	17.237440
31.930996	1444.661307	17.242458
31.958865	1444.373434	17.247475
31.979984	1449.227333	17.252493
32.353270	1444.107226	17.257511
32.370525	1465.624919	17.262528
32.350534	1472.361553	17.267546
32.726414	1465.218441	17.272563
32.702876	1475.740599	17.277581
33.040257	1455.716765	17.282599
32.535512	1444.413849	17.287616
32.375955	1430.533960	17.292634
32.547408	1429.516352	17.297651
32.758980	1446.238963	17.302669
32.648735	1428.221948	17.307687
32.662848	1436.696596	17.312704
32.814453	1450.491717	17.317722
33.162411	1456.089731	17.322739
32.802749	1454.502101	17.327757
32.856526	1443.891431	17.332775
32.674915	1433.223026	17.337792
32.576538	1443.958684	17.342810
32.933750	1441.257056	17.347827
32.711535	1447.602744	17.352845
32.940941	1453.835620	17.357863
33.247550	1453.096228	17.362880
33.066625	1456.648457	17.367898
33.261274	1455.457745	17.372915
33.087793	1457.587082	17.377933
33.179443	1453.177598	17.382951
33.090791	1459.667537	17.387968
33.125107	1465.827159	17.392986
33.093538	1451.956215	17.398003
32.860529	1467.024196	17.403021
33.181180	1463.130338	17.408039
33.090862	1457.203883	17.413056
33.067254	1471.009671	17.418074
33.108758	1480.585577	17.423091
33.318392	1479.261893	17.428109
33.260998	1490.530897	17.433127
33.545275	1483.252343	17.438144
33.843329	1479.580887	17.443162
33.608443	1489.226288	17.448179
33.519782	1484.921384	17.453197
33.763443	1469.557297	17.458215
33.752929	1486.415260	17.463232
33.718840	1489.397043	17.468250
33.778490	1479.107778	17.473267
33.749899	1475.984725	17.478285
34.018083	1484.507756	17.483303
33.644991	1480.375036	17.488320
33.644866	1482.126563	17.493338
33.905472	1474.789531	17.498355
33.859139	1479.155832	17.503373
34.036130	1478.015275	17.508391
34.199630	1484.598971	17.513408
34.070794	1483.620945	17.518426
34.394056	1480.543473	17.523443
33.649515	1486.345258	17.528461
33.934139	1485.535490	17.533479
34.142961	1490.214112	17.538496
34.174484	1503.148727	17.543514
34.478915	1501.260233	17.548531
34.593300	1518.041890	17.553549
34.326025	1493.463600	17.558567
34.270200	1486.777397	17.563584
34.258255	1492.450054	17.568602
34.519999	1492.609690	17.573619
34.444922	1505.873102	17.578637
34.905792	1489.185866	17.583655
34.724762	1495.120096	17.588672
34.447628	1470.220483	17.593690
34.979552	1469.229908	17.598707
34.873898	1470.958720	17.603725
34.653585	1462.019299	17.608743
34.637940	1457.084112	17.613760
34.496868	1468.604102	17.618778
34.521084	1468.448311	17.623795
34.228645	1476.593766	17.628813
34.661871	1496.703766	17.633831
34.783629	1496.591297	17.638848
34.793104	1509.549833	17.643866
34.901416	1503.741501	17.648883
34.973236	1510.302568	17.653901
34.740888	1502.111080	17.658919
35.296477	1490.065662	17.663936
34.881312	1504.530005	17.668954
35.098581	1495.775899	17.673971
34.702608	1501.190801	17.678989
34.906509	1504.424364	17.684007
35.067713	1497.638324	17.689024
35.220357	1505.730322	17.694042
35.463939	1510.201263	17.699059
35.938311	1507.715666	17.704077
35.693575	1489.678486	17.709095
35.491121	1483.245619	17.714112
35.703794	1489.721598	17.719130
35.826086	1493.251679	17.724147
35.482984	1488.182232	17.729165
35.405216	1476.591440	17.734183
35.801991	1486.442259	17.739200
35.488283	1481.664179	17.744218
35.658972	1481.808944	17.749235
35.444020	1495.265715	17.754253
35.550160	1484.482606	17.759271
35.506277	1476.867980	17.764288
35.580934	1479.450345	17.769306
35.701927	1484.313142	17.774323
35.438040	1501.969782	17.779341
36.029202	1513.919522	17.784359
35.863783	1507.326214	17.789376
35.868810	1526.707706	17.794394
36.283049	1518.047596	17.799411
36.151079	1516.093045	17.804429
36.059827	1507.446010	17.809447
36.175009	1514.754738	17.814464
35.970445	1511.517664	17.819482
36.040762	1519.402632	17.824499
36.222064	1507.601311	17.829517
36.507528	1520.151107	17.834535
36.219616	1514.120291	17.839552
35.864177	1521.700467	17.844570
36.381078	1521.543959	17.849587
36.139381	1516.704564	17.854605
35.833873	1520.484258	17.859623
36.145343	1523.197949	17.864640
36.295368	1530.807580	17.869658
36.629402	1533.351620	17.874675
36.302454	1542.591454	17.879693
36.532519	1541.158299	17.884711
36.895580	1533.422862	17.889728
36.526692	1534.992252	17.894746
36.527991	1541.581716	17.899763
36.673303	1530.898388	17.904781
36.723792	1544.665427	17.909799
36.807170	1533.717366	17.914816
36.746736	1544.822170	17.919834
36.817628	1528.946287	17.924851
36.571955	1545.073784	17.929869
36.876173	1544.470001	17.934887
36.568354	1541.574943	17.939904
36.641596	1546.618856	17.944922
36.853721	1553.293157	17.949939
36.819432	1573.743669	17.954957
36.842833	1578.320298	17.959975
37.139424	1558.116677	17.964992
36.957889	1567.037455	17.970010
37.093115	1560.192499	17.975027
37.335007	1569.772154	17.980045
37.408512	1567.106167	17.985063
37.498823	1555.190924	17.990080
37.164822	1559.536880	17.995098
37.351761	1556.999375	18.000115
37.272878	1564.899771	18.005133
37.271670	1555.894762	18.010151
37.487030	1568.476652	18.015168
37.652475	1576.253422	18.020186
38.001881	1560.279127	18.025203
37.997162	1561.998158	18.030221
37.932258	1551.261376	18.035239
38.338061	1545.536332	18.040256
37.717287	1547.230014	18.045274
38.032121	1546.441429	18.050291
37.954206	1543.019268	18.055309
37.758174	1547.832910	18.060327
37.939454	1554.507585	18.065344
37.803599	1545.720673	18.070362
38.072855	1546.269177	18.075379
37.586400	1538.070060	18.080397
37.452414	1546.797953	18.085415
37.927378	1558.684262	18.090432
38.036598	1569.307366	18.095450
38.034138	1571.736566	18.100467
38.364995	1574.012077	18.105485
38.187376	1581.767597	18.110503
38.810733	1570.386424	18.115520
38.194360	1564.773993	18.120538
38.540485	1568.397993	18.125555
38.548114	1568.895255	18.130573
38.084391	1577.436344	18.135591
38.237721	1574.002928	18.140608
38.453842	1567.311510	18.145626
38.517206	1565.387068	18.150643
38.515714	1565.077473	18.155661
38.426079	1577.186213	18.160679
38.466016	1564.021176	18.165696
38.237229	1577.133301	18.170714
38.402173	1585.351048	18.175731
38.680646	1595.464567	18.180749
38.653319	1593.286440	18.185767
39.267137	1588.413118	18.190784
38.869154	1594.633206	18.195802
39.127660	1585.721662	18.200819
39.371614	1587.095114	18.205837
39.186330	1587.704166	18.210855
39.575920	1585.882880	18.215872
39.335377	1566.570074	18.220890
39.124411	1559.355608	18.225907
39.087845	1550.192686	18.230925
39.166773	1562.519789	18.235943
39.456626	1556.346047	18.240960
39.224817	1559.728187	18.245978
39.147954	1569.971069	18.250995
39.216859	1570.142496	18.256013
39.236082	1585.819423	18.261031
39.679540	1590.764973	18.266048
39.465054	1592.380500	18.271066
39.182462	1593.222534	18.276083
39.739262	1589.855496	18.281101
39.340263	1593.162135	18.286119
39.611869	1596.195773	18.291136
39.541004	1599.577505	18.296154
39.634731	1584.395540	18.301171
39.625159	1586.791474	18.306189
39.712691	1596.256709	18.311207
39.709783	1582.831446	18.316224
39.703636	1594.345373	18.321242
39.611888	1597.890575	18.326259
39.892810	1588.718074	18.331277
39.567889	1595.194166	18.336295
39.724733	1600.744888	18.341312
40.229747	1608.123870	18.346330
40.459262	1619.296155	18.351347
40.583269	1611.331316	18.356365
40.186709	1602.990160	18.361383
40.204048	1580.191247	18.366400
40.298884	1587.809830	18.371418
40.553794	1589.118093	18.376435
40.386921	1579.316335	18.381453
40.176392	1583.836554	18.386471
40.494317	1582.504414	18.391488
40.612531	1604.618339	18.396506
40.286029	1601.724387	18.401523
40.738665	1596.265962	18.406541
40.507444	1600.979346	18.411559
40.935285	1606.383529	18.416576
40.713465	1611.796262	18.421594
40.770307	1600.360079	18.426611
40.764051	1595.187301	18.431629
40.516812	1600.325525	18.436647
40.652563	1603.499514	18.441664
40.834613	1607.422256	18.446682
40.591642	1595.920476	18.451699
40.760859	1601.801003	18.456717
40.815124	1599.356273	18.461735
40.701128	1599.412076	18.466752
40.390037	1596.696463	18.471770
40.721587	1617.323559	18.476787
41.063827	1627.796990	18.481805
41.194641	1629.230081	18.486823
41.618284	1633.685673	18.491840
41.388679	1628.317930	18.496858
41.091329	1627.670853	18.501875
41.505913	1638.856068	18.506893
41.225350	1634.712543	18.511911
41.540356	1614.595754	18.516928
41.643869	1622.741203	18.521946
41.455169	1632.020049	18.526963
41.743825	1624.485224	18.531981
42.001848	1623.625325	18.536999
41.551907	1627.167329	18.542016
41.766696	1629.495489	18.547034
41.646795	1620.694089	18.552051
41.885223	1625.041325	18.557069
41.808487	1631.592744	18.562087
41.858203	1618.872447	18.567104
41.852661	1622.157179	18.572122
41.712445	1630.145687	18.577139
41.833727	1615.819074	18.582157
41.664659	1628.733995	18.587175
42.045270	1628.762390	18.592192
42.044315	1623.189169	18.597210
41.831900	1625.476912	18.602227
42.098455	1627.903394	18.607245
42.160843	1650.987124	18.612263
42.070488	1645.743197	18.617280
42.125691	1649.191498	18.622298
42.212690	1645.159258	18.627315
42.529049	1643.662627	18.632333
42.275786	1651.883187	18.637351
42.592884	1648.948811	18.642368
42.335222	1644.122446	18.647386
42.471464	1652.594548	18.652403
42.504756	1656.175000	18.657421
42.435666	1656.547360	18.662439
42.373255	1644.891508	18.667456
42.690928	1651.896597	18.672474
42.283635	1649.955245	18.677491
42.624926	1656.782832	18.682509
42.610635	1673.640246	18.687527
43.076007	1682.278818	18.692544
43.139575	1676.549853	18.697562
42.935145	1674.050431	18.702579
42.888589	1671.119457	18.707597
43.085097	1678.256575	18.712615
43.284506	1669.871814	18.717632
43.371850	1670.405507	18.722650
43.245860	1672.417196	18.727667
43.524183	1663.057700	18.732685
43.320162	1673.290565	18.737703
43.420029	1685.371618	18.742720
43.495273	1681.346428	18.747738
43.434545	1674.770389	18.752755
43.445261	1682.035443	18.757773
43.312476	1681.942991	18.762791
43.456586	1686.445185	18.767808
43.343117	1686.652852	18.772826
43.343530	1677.416428	18.777843
43.331767	1672.321691	18.782861
43.540738	1674.884847	18.787879
43.110542	1670.759739	18.792896
43.238713	1678.109700	18.797914
43.228992	1701.078270	18.802931
43.614928	1697.812861	18.807949
43.534279	1696.304084	18.812967
43.753262	1702.773797	18.817984
43.859972	1709.892505	18.823002
43.906039	1722.413727	18.828019
44.261139	1726.129971	18.833037
44.036929	1734.521345	18.838055
44.398250	1735.805738	18.843072
44.480545	1736.678418	18.848090
44.609631	1736.601937	18.853107
44.557721	1707.761426	18.858125
44.314253	1702.408545	18.863143
44.454160	1704.377283	18.868160
45.109950	1702.711775	18.873178
44.335644	1709.343661	18.878195
44.602617	1703.512775	18.883213
44.774174	1698.859531	18.888231
44.469141	1692.994053	18.893248
44.702532	1685.266189	18.898266
44.425447	1697.781744	18.903283
44.800688	1709.134517	18.908301
44.648667	1729.283272	18.913319
44.738140	1723.412427	18.918336
44.825024	1712.880540	18.923354
44.938532	1721.463315	18.928371
44.954978	1721.954204	18.933389
45.008348	1719.914675	18.938407
45.098234	1734.720923	18.943424
44.924612	1724.963490	18.948442
44.942239	1722.710207	18.953459
44.953488	1729.804348	18.958477
44.978483	1719.886159	18.963495
44.668315	1723.707022	18.968512
45.288645	1728.713537	18.973530
45.195691	1754.431849	18.978547
45.275127	1762.497304	18.983565
45.322581	1744.621163	18.988583
45.440337	1762.029624	18.993600
45.777917	1754.143186	18.998618
45.696743	1762.647931	19.003635
45.666325	1750.843028	19.008653
45.463071	1748.782326	19.013671
45.760905	1752.470643	19.018688
45.767314	1747.184907	19.023706
45.619071	1749.208943	19.028723
45.689057	1745.838862	19.033741
45.820109	1745.646519	19.038759
45.846763	1746.885440	19.043776
45.882384	1745.349177	19.048794
45.479328	1750.329558	19.053811
46.072681	1760.606681	19.058829
46.490169	1780.764531	19.063847
46.290828	1768.003583	19.068864
46.646643	1755.065878	19.073882
46.567455	1752.928972	19.078899
46.383062	1741.364850	19.083917
46.408576	1739.881630	19.088935
46.212057	1743.193419	19.093952
46.295861	1735.102301	19.098970
46.273510	1747.957845	19.103987
46.515911	1757.105299	19.109005
46.930698	1771.183363	19.114023
46.597549	1765.624437	19.119040
47.002468	1774.306708	19.124058
46.924063	1776.706960	19.129075
46.586541	1774.594040	19.134093
46.723339	1760.609179	19.139111
46.423086	1757.669329	19.144128
46.872985	1757.019815	19.149146
46.697189	1768.039327	19.154163
46.655366	1765.248088	19.159181
46.890798	1760.792319	19.164199
46.660456	1769.564800	19.169216
47.248932	1768.160578	19.174234
46.818328	1783.716194	19.179251
47.312469	1785.347698	19.184269
47.222379	1788.283484	19.189287
47.287465	1789.478267	19.194304
47.831281	1780.071484	19.199322
47.499544	1780.954125	19.204339
47.588794	1785.597879	19.209357
47.537434	1782.313189	19.214375
47.279075	1786.478419	19.219392
47.408549	1770.874465	19.224410
47.261191	1774.416300	19.229427
47.362391	1776.214298	19.234445
47.743478	1772.681398	19.239463
47.375847	1788.205355	19.244480
47.693815	1796.050329	19.249498
47.526072	1813.944364	19.254515
47.554577	1799.025301	19.259533
48.224158	1800.648285	19.264551
47.700742	1811.838842	19.269568
48.033212	1805.024169	19.274586
48.044291	1802.520016	19.279603
47.915661	1809.161180	19.284621
48.296759	1817.694870	19.289639
48.014022	1826.046953	19.294656
48.316341	1829.624323	19.299674
48.497638	1828.660373	19.304691
48.192916	1827.399216	19.309709
48.512047	1820.129311	19.314727
48.384962	1834.604619	19.319744
48.529148	1829.141183	19.324762
48.492993	1824.756256	19.329779
48.374919	1822.716503	19.334797
48.491615	1817.253678	19.339815
48.197135	1828.453064	19.344832
48.336146	1820.020728	19.349850
48.712181	1848.308261	19.354867
48.932717	1861.975445	19.359885
48.953815	1860.188645	19.364903
48.751120	1860.452590	19.369920
49.161890	1856.463239	19.374938
49.282585	1857.977346	19.379955
49.044740	1867.939186	19.384973
49.650769	1844.722164	19.389991
49.421421	1851.030223	19.395008
49.376843	1855.591005	19.400026
49.198884	1848.899830	19.405043
49.204008	1855.418725	19.410061
49.694973	1839.298322	19.415079
49.378215	1847.367094	19.420096
49.482151	1848.837518	19.425114
49.599973	1846.121251	19.430131
49.424165	1850.795243	19.435149
49.794146	1847.245069	19.440167
49.595214	1844.667946	19.445184
49.974183	1841.171794	19.450202
49.686606	1856.534182	19.455219
49.880701	1849.536276	19.460237
49.863206	1841.678944	19.465255
49.816242	1864.481490	19.470272
50.076738	1864.979294	19.475290
50.131496	1868.151369	19.480307
50.420694	1871.584869	19.485325
50.424734	1872.113636	19.490343
50.136850	1866.002566	19.495360
50.118993	1868.231426	19.500378
50.114410	1871.333985	19.505395
50.137033	1867.871518	19.510413
50.335835	1865.189696	19.515431
50.365623	1873.128191	19.520448
50.180589	1873.338435	19.525466
50.450966	1872.539074	19.530483
49.861163	1878.745308	19.535501
50.475295	1891.901855	19.540519
50.575739	1905.660962	19.545536
50.767085	1911.414145	19.550554
50.968247	1915.966617	19.555571
50.977057	1903.545532	19.560589
51.366354	1896.805869	19.565607
51.139371	1900.480169	19.570624
51.050231	1893.388706	19.575642
50.929495	1892.517570	19.580659
51.018715	1892.123301	19.585677
51.210185	1896.735435	19.590695
51.163858	1896.632828	19.595712
51.367187	1883.277149	19.600730
51.339432	1897.960292	19.605747
51.081227	1905.699373	19.610765
51.051519	1885.187077	19.615783
51.272307	1898.158260	19.620800
51.582365	1912.912354	19.625818
51.829196	1914.406018	19.630835
51.869300	1932.786854	19.635853
51.884079	1913.866416	19.640871
51.483422	1908.830155	19.645888
51.691079	1919.123290	19.650906
51.921040	1923.285219	19.655923
51.480664	1922.786946	19.660941
52.030415	1916.172911	19.665959
51.975929	1920.166116	19.670976
51.898613	1914.235761	19.675994
51.757646	1913.175270	19.681011
52.011143	1911.882487	19.686029
52.121309	1912.184094	19.691047
52.143423	1911.400954	19.696064
51.945175	1908.419025	19.701082
52.029470	1932.021156	19.706099
52.206936	1941.319593	19.711117
52.458665	1941.117344	19.716135
52.183250	1944.723877	19.721152
52.560446	1942.013941	19.726170
52.822649	1951.061988	19.731187
52.544010	1935.705603	19.736205
52.672886	1928.008471	19.741223
52.595958	1938.658850	19.746240
52.448722	1944.552632	19.751258
52.674807	1943.460616	19.756275
52.845870	1968.820334	19.761293
52.994031	1955.750651	19.766311
52.616887	1973.588931	19.771328
52.727954	1975.704385	19.776346
53.013961	1967.126824	19.781363
52.454592	1974.901927	19.786381
52.878245	1973.345415	19.791399
52.988543	1986.801421	19.796416
53.224466	1989.563503	19.801434
53.378171	1993.531182	19.806451
53.306359	1993.886678	19.811469
53.508546	1985.762089	19.816487
53.736496	1990.114310	19.821504
53.809570	1998.287230	19.826522
53.775180	1988.999683	19.831539
53.800426	1996.190837	19.836557
53.865677	1987.918616	19.841575
53.911141	1989.911855	19.846592
54.070355	1991.574517	19.851610
53.887385	1988.652246	19.856627
53.856227	1989.730875	19.861645
53.930846	1972.352097	19.866663
54.172118	1988.950521	19.871680
53.832003	1995.831023	19.876698
53.918937	2002.080974	19.881715
54.148884	2011.992768	19.886733
54.601812	2013.781094	19.891751
54.498984	2023.292417	19.896768
54.740175	2021.574140	19.901786
54.814624	2015.581269	19.906803
54.667328	2022.834409	19.911821
54.802600	2012.762782	19.916839
54.468136	2007.580327	19.921856
54.415417	2028.290566	19.926874
54.744950	2015.136536	19.931891
54.529958	2020.031403	19.936909
54.590316	2018.218808	19.941927
54.772099	2016.847915	19.946944
54.685348	2020.758887	19.951962
54.964063	2015.922897	19.956979
54.464185	2020.033423	19.961997
54.975856	2031.705394	19.967015
55.168627	2047.389936	19.972032
55.035117	2047.745787	19.977050
55.138733	2045.891398	19.982067
55.182717	2039.317387	19.987085
55.301706	2034.838265	19.992103
55.361525	2039.249185	19.997120
55.425230	2036.817196	20.002138
55.751067	2034.034439	20.007155
55.420211	2043.097871	20.012173
55.670426	2043.288945	20.017191
55.721400	2030.258090	20.022208
55.717588	2030.601760	20.027226
55.906467	2035.014776	20.032243
56.135705	2033.922627	20.037261
55.954817	2032.611859	20.042279
56.031159	2030.427955	20.047296
56.152263	2038.326055	20.052314
56.382147	2040.071327	20.057331
56.233863	2055.178436	20.062349
56.097594	2031.412993	20.067367
56.712268	2040.923468	20.072384
56.399396	2028.776087	20.077402
56.383023	2016.355135	20.082419
56.580750	2038.205779	20.087437
56.555487	2035.121231	20.092455
57.072663	2046.729121	20.097472
56.547060	2034.482452	20.102490
56.862958	2027.049220	20.107507
56.686114	2026.286157	20.112525
56.670722	2034.319398	20.117543
56.728246	2048.885257	20.122560
56.620636	2047.197255	20.127578
56.846100	2054.685636	20.132595
56.559703	2065.063067	20.137613
56.805590	2060.050812	20.142631
56.887986	2055.373025	20.147648
56.937870	2062.754216	20.152666
56.913157	2076.324728	20.157683
57.376582	2079.708424	20.162701
57.495328	2085.138660	20.167719
57.342317	2083.240460	20.172736
57.492264	2087.184968	20.177754
57.721270	2070.548215	20.182771
57.425087	2083.669347	20.187789
57.491640	2072.471739	20.192807
57.553012	2071.986210	20.197824
57.706772	2068.881520	20.202842
58.049867	2066.666523	20.207859
57.888523	2073.895632	20.212877
57.876380	2078.596186	20.217895
57.974545	2073.875044	20.222912
57.922225	2080.306882	20.227930
58.005085	2077.470379	20.232947
58.081785	2092.234666	20.237965
57.907953	2099.943367	20.242983
58.642454	2107.879106	20.248000
58.093603	2103.185154	20.253018
58.436101	2096.471641	20.258035
58.447378	2104.796154	20.263053
58.241476	2095.275885	20.268071
58.504696	2094.211578	20.273088
58.517383	2101.671762	20.278106
58.804204	2087.742515	20.283123
58.775850	2100.470419	20.288141
58.454394	2101.640329	20.293159
58.757185	2106.439427	20.298176
58.441779	2121.973197	20.303194
59.020552	2125.478382	20.308211
59.016144	2128.632927	20.313229
59.172163	2121.789602	20.318247
59.177505	2119.074357	20.323264
59.103752	2128.408711	20.328282
59.330146	2130.677359	20.333299
59.323914	2128.647428	20.338317
58.945993	2132.378020	20.343335
59.457766	2126.428185	20.348352
59.030524	2131.119008	20.353370
59.179944	2126.960983	20.358387
59.217677	2115.869475	20.363405
59.297766	2128.043900	20.368423
59.743526	2135.308729	20.373440
59.678589	2137.644808	20.378458
59.596653	2128.214654	20.383475
60.050403	2131.007494	20.388493
59.774623	2137.690435	20.393511
59.965392	2133.841296	20.398528
59.942771	2140.426899	20.403546
59.845589	2126.115639	20.408563
60.185943	2155.089100	20.413581
60.320745	2162.586610	20.418599
60.839891	2161.371750	20.423616
60.745631	2166.162074	20.428634
60.715302	2145.632606	20.433651
60.319138	2138.525038	20.438669
60.467049	2149.691511	20.443687
60.643658	2146.948550	20.448704
60.450161	2164.415590	20.453722
60.831960	2161.757410	20.458739
60.728733	2158.512114	20.463757
60.501955	2159.313657	20.468775
61.150257	2158.916753	20.473792
60.934610	2161.611963	20.478810
60.946330	2154.638544	20.483827
60.928822	2151.885930	20.488845
61.238574	2153.141090	20.493863
61.311948	2148.782062	20.498880
61.136850	2165.718354	20.503898
61.012869	2169.116663	20.508915
61.291574	2178.301672	20.513933
61.214627	2181.344013	20.518951
61.523501	2186.474780	20.523968
60.814373	2209.659672	20.528986
61.275700	2190.483821	20.534003
61.700517	2199.598049	20.539021
61.466262	2219.993100	20.544039
61.873223	2214.192036	20.549056
61.977087	2212.604493	20.554074
62.216030	2210.811180	20.559091
62.458787	2215.639916	20.564109
62.178377	2214.388291	20.569127
62.541766	2205.288603	20.574144
62.432421	2190.961183	20.579162
62.205968	2197.307090	20.584179
62.768785	2203.703665	20.589197
62.418562	2196.300313	20.594215
62.456373	2195.902525	20.599232
62.397772	2203.263327	20.604250
62.554178	2199.017325	20.609267
62.300137	2195.652072	20.614285
62.381046	2201.816886	20.619303
62.455688	2198.716781	20.624320
62.217692	2198.703910	20.629338
62.810252	2222.677185	20.634355
62.904705	2224.220073	20.639373
62.870035	2223.940158	20.644391
63.048361	2222.097416	20.649408
63.093633	2230.744896	20.654426
62.920084	2222.754312	20.659443
63.086828	2219.699806	20.664461
62.975080	2229.999082	20.669479
63.185927	2223.716291	20.674496
63.117308	2241.167900	20.679514
63.499834	2259.040610	20.684531
63.627913	2252.562445	20.689549
63.337174	2260.598000	20.694567
63.476818	2259.810381	20.699584
63.430753	2253.900122	20.704602
63.436281	2255.038056	20.709619
64.202929	2244.830454	20.714637
63.993852	2251.555764	20.719655
63.851279	2248.778724	20.724672
63.752404	2256.108217	20.729690
64.304141	2277.392279	20.734707
64.418001	2276.243397	20.739725
64.151407	2290.938037	20.744743
64.462745	2283.122198	20.749760
64.502805	2293.945011	20.754778
64.853174	2287.407858	20.759795
65.013066	2283.290774	20.764813
64.825666	2295.010162	20.769831
64.768664	2287.546503	20.774848
64.635747	2288.899034	20.779866
64.857139	2293.353402	20.784883
64.994988	2285.111148	20.789901
64.749514	2289.110222	20.794919
65.154448	2287.345373	20.799936
65.003443	2281.762263	20.804954
65.059229	2283.383981	20.809971
65.028674	2272.734713	20.814989
64.756280	2286.041833	20.820007
64.887592	2273.394318	20.825024
64.715183	2289.111696	20.830042
65.296939	2299.578486	20.835059
65.098418	2297.939926	20.840077
65.446327	2298.630569	20.845095
65.603246	2300.925485	20.850112
65.474432	2304.328362	20.855130
65.760479	2295.087280	20.860147
65.938729	2310.536122	20.865165
65.533617	2332.229732	20.870183
65.766754	2315.391851	20.875200
66.075236	2331.305378	20.880218
65.789241	2333.417601	20.885235
65.892619	2329.390547	20.890253
65.783079	2344.291550	20.895271
66.076063	2335.670708	20.900288
66.401307	2354.170861	20.905306
66.312588	2366.459976	20.910323
66.987109	2365.167463	20.915341
66.684603	2362.086145	20.920359
67.011392	2360.438524	20.925376
66.973820	2355.332866	20.930394
66.773641	2360.972975	20.935411
67.392473	2343.575107	20.940429
66.816235	2338.994654	20.945447
66.821553	2332.818216	20.950464
66.930526	2350.841149	20.955482
66.765671	2344.617045	20.960499
66.904880	2343.539358	20.965517
66.845926	2352.068509	20.970535
66.840920	2339.275761	20.975552
67.238890	2352.522752	20.980570
67.003242	2379.151051	20.985587
67.587374	2367.586030	20.990605
67.432215	2374.969758	20.995623
67.704985	2370.906435	21.000640
68.096890	2376.492015	21.005658
67.960648	2366.978569	21.010675
68.489699	2360.650228	21.015693
68.019176	2363.786378	21.020711
68.283849	2344.326912	21.025728
68.166824	2332.408128	21.030746
68.114173	2336.793037	21.035763
68.232803	2328.420678	21.040781
68.011312	2330.417132	21.045799
68.257980	2348.094695	21.050816
68.626257	2354.185513	21.055834
68.246161	2362.134515	21.060851
68.303528	2338.467300	21.065869
68.213460	2355.662170	21.070887
68.269185	2355.154142	21.075904
68.428348	2353.735584	21.080922
68.385915	2369.031595	21.085939
68.696674	2364.966720	21.090957
68.788673	2391.220843	21.095975
68.720507	2391.447015	21.100992
69.034084	2399.013517	21.106010
68.708055	2391.817868	21.111027
69.083859	2382.372349	21.116045
68.814752	2391.324212	21.121063
68.851955	2398.846232	21.126080
69.110519	2408.041202	21.131098
69.167177	2412.797413	21.136115
69.501532	2410.507046	21.141133
69.462905	2419.399976	21.146151
69.544332	2407.296383	21.151168
69.840994	2414.417688	21.156186
69.960231	2417.529422	21.161203
69.719373	2416.112790	21.166221
69.700229	2418.698413	21.171239
70.062831	2431.484813	21.176256
70.452669	2428.763651	21.181274
71.120003	2410.720927	21.186291
71.495248	2380.505907	21.191309
71.234199	2371.836644	21.196327
71.337591	2367.157656	21.201344
71.246352	2344.784776	21.206362
71.044267	2348.217879	21.211379
71.361070	2329.914690	21.216397
71.416182	2330.018136	21.221415
71.297349	2338.006625	21.226432
71.047250	2308.931812	21.231450
70.993068	2308.639963	21.236467
70.892319	2301.948034	21.241485
70.972463	2300.692723	21.246503
71.291066	2308.919126	21.251520
71.265396	2301.677628	21.256538
70.984668	2304.699734	21.261555
71.088672	2323.259832	21.266573
71.326849	2325.191942	21.271591
71.133738	2337.604183	21.276608
71.423824	2337.841032	21.281626
71.181892	2345.362698	21.286643
71.536594	2341.822221	21.291661
71.508336	2339.137487	21.296679
71.378524	2348.814678	21.301696
71.622883	2358.552871	21.306714
71.350681	2366.463379	21.311731
71.540964	2363.053405	21.316749
71.755902	2371.575888	21.321767
71.595381	2386.761716	21.326784
71.839365	2397.702666	21.331802
71.503256	2398.776796	21.336819
72.100681	2399.530537	21.341837
71.894312	2406.272789	21.346855
72.087869	2427.475902	21.351872
72.231896	2425.146712	21.356890
72.035568	2441.796480	21.361907
72.256917	2428.205677	21.366925
72.521655	2451.904369	21.371943
72.467266	2470.685686	21.376960
72.941184	2456.648622	21.381978
72.846421	2472.050227	21.386995
73.002072	2467.691882	21.392013
73.038748	2469.653764	21.397031
72.775012	2461.235665	21.402048
72.919153	2462.550696	21.407066
72.837503	2472.074936	21.412083
72.709136	2480.833921	21.417101
73.483891	2483.529298	21.422119
73.509410	2475.048238	21.427136
73.384277	2482.722115	21.432154
73.413935	2497.862257	21.437171
74.083721	2497.426760	21.442189
74.218136	2517.931154	21.447207
74.178902	2512.160406	21.452224
74.356128	2505.324431	21.457242
74.173141	2484.585304	21.462259
74.043915	2477.154352	21.467277
73.956859	2489.781065	21.472295
73.852915	2515.275702	21.477312
74.202222	2506.562196	21.482330
74.134894	2512.511882	21.487347
74.190343	2515.286757	21.492365
74.511014	2522.613974	21.497383
74.338504	2525.749728	21.502400
74.840953	2534.000791	21.507418
74.479866	2532.841598	21.512435
74.884908	2539.536022	21.517453
74.983413	2527.636588	21.522471
75.145604	2530.861515	21.527488
75.355169	2519.230725	21.532506
75.083810	2538.575897	21.537523
75.002732	2522.746544	21.542541
75.124560	2540.064272	21.547559
75.287585	2557.290177	21.552576
75.542849	2566.732033	21.557594
75.555230	2556.213655	21.562611
75.984139	2567.455447	21.567629
76.052048	2555.168158	21.572647
75.829882	2562.304795	21.577664
76.252296	2552.540663	21.582682
76.052177	2560.298815	21.587699
76.381433	2561.938757	21.592717
76.177333	2546.791084	21.597735
76.300446	2555.485133	21.602752
76.587545	2544.042681	21.607770
76.320824	2547.453046	21.612787
76.189904	2547.037267	21.617805
76.341786	2541.080213	21.622823
76.436190	2557.019900	21.627840
76.418873	2546.661151	21.632858
76.326175	2558.612712	21.637875
76.551897	2561.301195	21.642893
76.927970	2568.647231	21.647911
76.702582	2575.257273	21.652928
76.563479	2566.570505	21.657946
76.642431	2559.493280	21.662963
76.641580	2580.472050	21.667981
76.879387	2597.287242	21.672999
76.916858	2607.267837	21.678016
77.051476	2605.209452	21.683034
77.317191	2592.778429	21.688051
77.226761	2596.522251	21.693069
77.507339	2606.410710	21.698087
77.323892	2628.975928	21.703104
77.885036	2627.491906	21.708122
78.083420	2615.952650	21.713139
78.288862	2621.705345	21.718157
78.305228	2609.602109	21.723175
78.257732	2607.125417	21.728192
78.458114	2599.237602	21.733210
78.141100	2608.247307	21.738227
78.523614	2608.066352	21.743245
78.290406	2609.985451	21.748263
78.383693	2612.037204	21.753280
78.460442	2601.940811	21.758298
78.533982	2610.061619	21.763315
78.612593	2605.727973	21.768333
78.744395	2612.071540	21.773351
78.538473	2619.714939	21.778368
78.701974	2624.458482	21.783386
79.032060	2638.841284	21.788403
78.991774	2656.287893	21.793421
79.227471	2641.005648	21.798439
79.388575	2641.750600	21.803456
79.327733	2650.908540	21.808474
79.239278	2641.164205	21.813491
79.456722	2643.044273	21.818509
79.490788	2629.563370	21.823527
79.325806	2646.408167	21.828544
79.549554	2659.725942	21.833562
79.358257	2662.697513	21.838579
79.676304	2658.752218	21.843597
79.894045	2651.596902	21.848615
79.743056	2668.228792	21.853632
79.855656	2672.820139	21.858650
79.899995	2690.205955	21.863667
80.058798	2702.388101	21.868685
80.282231	2699.328857	21.873703
79.926335	2700.782045	21.878720
80.240549	2706.143589	21.883738
80.311634	2721.165691	21.888755
80.448452	2719.593123	21.893773
80.647744	2721.947831	21.898791
80.406720	2731.253302	21.903808
80.590709	2712.590722	21.908826
80.746279	2747.163266	21.913843
80.930949	2754.182768	21.918861
81.333862	2746.000796	21.923879
81.401624	2744.751038	21.928896
81.616565	2749.792404	21.933914
81.780133	2746.170236	21.938931
81.742624	2744.143424	21.943949
82.136943	2746.441107	21.948967
81.619791	2733.987372	21.953984
81.779024	2738.205302	21.959002
81.824335	2737.581666	21.964019
81.632242	2738.894410	21.969037
82.071420	2744.459717	21.974055
81.531403	2747.567663	21.979072
82.052064	2758.787742	21.984090
82.284451	2767.926036	21.989107
82.020464	2770.677367	21.994125
82.441574	2784.538988	21.999143
82.325905	2772.138954	22.004160
82.430297	2769.770990	22.009178
82.615848	2774.821944	22.014195
82.092856	2774.711091	22.019213
82.635406	2786.478729	22.024231
82.717713	2793.404144	22.029248
82.909650	2807.225706	22.034266
83.127257	2799.961687	22.039283
82.851152	2800.083254	22.044301
83.254401	2794.579427	22.049319
83.221376	2792.434944	22.054336
83.248236	2784.150532	22.059354
83.452647	2787.975989	22.064371
83.341418	2801.922835	22.069389
83.838391	2802.610328	22.074407
83.760924	2811.197119	22.079424
83.666155	2816.421173	22.084442
83.992512	2821.523676	22.089459
83.861257	2822.560243	22.094477
84.398054	2809.978746	22.099495
84.373876	2816.374154	22.104512
84.317745	2833.656660	22.109530
84.445304	2817.497266	22.114547
84.009250	2831.306482	22.119565
84.722015	2823.060671	22.124583
84.507932	2828.428062	22.129600
84.373574	2824.625194	22.134618
84.464608	2822.463357	22.139635
84.382708	2826.317237	22.144653
84.415402	2837.814060	22.149671
84.439296	2835.930627	22.154688
84.553245	2850.569017	22.159706
84.959155	2851.852244	22.164723
84.983200	2870.093548	22.169741
85.223811	2868.368781	22.174759
85.235702	2878.311654	22.179776
85.698985	2867.722101	22.184794
85.756822	2876.743245	22.189811
85.839131	2876.670947	22.194829
85.790469	2873.413727	22.199847
85.517094	2872.254186	22.204864
85.591121	2870.738434	22.209882
85.976151	2885.215926	22.214899
85.757305	2897.479920	22.219917
86.278848	2888.621209	22.224935
86.249470	2899.078376	22.229952
86.093896	2902.294080	22.234970
86.327414	2904.321912	22.239987
86.395483	2891.479233	22.245005
86.681181	2905.721199	22.250023
86.541900	2913.508843	22.255040
86.627249	2923.777784	22.260058
87.396705	2923.791147	22.265075
86.761400	2932.272158	22.270093
86.945431	2920.868901	22.275111
86.997556	2919.464240	22.280128
87.089735	2921.612670	22.285146
87.191521	2914.292542	22.290163
87.512133	2926.201680	22.295181
87.285764	2921.238052	22.300199
87.283462	2932.968279	22.305216
87.229987	2944.635713	22.310234
87.514199	2945.864651	22.315251
87.416324	2950.385745	22.320269
87.479818	2954.653412	22.325287
87.660004	2966.887744	22.330304
87.438031	2971.165186	22.335322
87.885987	2975.539010	22.340339
88.258090	2980.353307	22.345357
88.831163	2972.937560	22.350375
88.702094	2962.388345	22.355392
89.045070	2961.406862	22.360410
89.222244	2954.037646	22.365427
89.139948	2952.126865	22.370445
89.740657	2950.546516	22.375463
89.481484	2964.750230	22.380480
89.279538	2932.955552	22.385498
89.236857	2919.997689	22.390515
88.945572	2925.612506	22.395533
89.193893	2918.256353	22.400551
89.568623	2933.724533	22.405568
89.469259	2944.953504	22.410586
89.526700	2947.897413	22.415603
89.422438	2952.553023	22.420621
89.846621	2949.385758	22.425639
89.664781	2956.138367	22.430656
89.462728	2950.264837	22.435674
89.611684	2943.670734	22.440691
89.493761	2947.716810	22.445709
89.435563	2967.811912	22.450727
90.045885	2973.294694	22.455744
89.951238	2984.690232	22.460762
90.142199	2985.691676	22.465779
90.036654	2993.563153	22.470797
90.370250	3001.709697	22.475815
90.331880	3001.620334	22.480832
90.493669	3004.523784	22.485850
90.752210	2998.542238	22.490867
90.574672	3009.588510	22.495885
91.068555	3020.399045	22.500903
91.422541	3030.731538	22.505920
91.141667	3034.558114	22.510938
91.380755	3023.068915	22.515955
91.608490	3028.145658	22.520973
91.655290	3027.178468	22.525991
92.002298	3025.821918	22.531008
91.601295	3023.384674	22.536026
91.867574	3010.770553	22.541043
91.681232	3030.383777	22.546061
91.572205	3013.634157	22.551079
91.683692	3021.197353	22.556096
91.497879	3037.147619	22.561114
91.972154	3049.049177	22.566131
92.428925	3060.439872	22.571149
92.086405	3058.759473	22.576167
92.307544	3057.611509	22.581184
92.122348	3076.124238	22.586202
92.285355	3077.820841	22.591219
92.287525	3090.090984	22.596237
92.706324	3075.054428	22.601255
92.715225	3079.669724	22.606272
93.034422	3103.917096	22.611290
93.091173	3108.227257	22.616307
92.928455	3111.444578	22.621325
93.563287	3112.569926	22.626343
93.754533	3102.651527	22.631360
93.679584	3111.230982	22.636378
94.018748	3097.913032	22.641395
93.534797	3103.791633	22.646413
93.475652	3115.778629	22.651431
93.429097	3102.328352	22.656448
93.323229	3121.498483	22.661466
93.860578	3128.165004	22.666483
93.944492	3131.073473	22.671501
94.195015	3132.478462	22.676519
94.160936	3128.429820	22.681536
94.003265	3145.308595	22.686554
94.550778	3154.705277	22.691571
94.623868	3170.198340	22.696589
94.436495	3173.559115	22.701607
94.513626	3157.486439	22.706624
94.457575	3166.056502	22.711642
94.833755	3167.898202	22.716659
94.774798	3186.276819	22.721677
94.996354	3198.178520	22.726695
95.238387	3186.370610	22.731712
95.303340	3194.156142	22.736730
95.585516	3174.955927	22.741747
95.796089	3178.058038	22.746765
95.630645	3181.267162	22.751783
95.712193	3182.673700	22.756800
95.507327	3173.417941	22.761818
95.687928	3192.670742	22.766835
95.814984	3202.729437	22.771853
95.542454	3212.349451	22.776871
96.188712	3204.129391	22.781888
95.947940	3213.655183	22.786906
96.092787	3224.107795	22.791923
96.280077	3241.496986	22.796941
96.744453	3241.702101	22.801959
97.067262	3249.674577	22.806976
96.675119	3240.156816	22.811994
97.114648	3240.799493	22.817011
97.244739	3234.810737	22.822029
97.175740	3240.734206	22.827047
97.517632	3234.425417	22.832064
97.155082	3252.262556	22.837082
97.287536	3248.736750	22.842099
97.357947	3228.536438	22.847117
97.111569	3254.821562	22.852135
97.350508	3261.700046	22.857152
97.635207	3259.991180	22.862170
97.711015	3256.102691	22.867187
97.578115	3259.933610	22.872205
97.871118	3274.904620	22.877223
98.381315	3284.884311	22.882240
98.093792	3292.407274	22.887258
98.006871	3293.680638	22.892275
98.460808	3285.856483	22.897293
98.201920	3283.387841	22.902311
98.514627	3302.854774	22.907328
98.014151	3318.803385	22.912346
98.550596	3317.957235	22.917363
98.916226	3307.808712	22.922381
98.857478	3322.371755	22.927399
99.387767	3337.217791	22.932416
99.055324	3347.915887	22.937434
99.089084	3347.944916	22.942451
99.203175	3354.433052	22.947469
99.491862	3348.278283	22.952487
99.852234	3340.056968	22.957504
99.749048	3345.934158	22.962522
99.708469	3348.234505	22.967539
99.723902	3348.361443	22.972557
99.548920	3376.511336	22.977575
99.886824	3362.576050	22.982592
99.958328	3368.391313	22.987610
99.806896	3390.437785	22.992627
100.039507	3400.867353	22.997645
100.062249	3397.234053	23.002663
100.379177	3396.953302	23.007680
100.897995	3427.915792	23.012698
100.898389	3419.659429	23.017715
101.272406	3420.028690	23.022733
101.328320	3417.341868	23.027751
101.153838	3415.473033	23.032768
101.494560	3426.852073	23.037786
101.564868	3422.075873	23.042803
101.798685	3405.871932	23.047821
101.510891	3419.522918	23.052839
101.567077	3417.377387	23.057856
101.438642	3404.260849	23.062874
101.470521	3403.959877	23.067891
101.758248	3409.124077	23.072909
101.366328	3415.788763	23.077927
101.860810	3431.467574	23.082944
101.885344	3440.068960	23.087962
102.192440	3453.735458	23.092979
102.163295	3455.567396	23.097997
102.413485	3469.264176	23.103015
102.756276	3478.148822	23.108032
102.466896	3471.297792	23.113050
102.742761	3473.446262	23.118067
102.897993	3467.539876	23.123085
102.772170	3480.996042	23.128103
103.296682	3468.357385	23.133120
103.111313	3477.889931	23.138138
102.982436	3489.931258	23.143155
103.484165	3488.912490	23.148173
103.345694	3493.862102	23.153191
103.666846	3488.781048	23.158208
103.503749	3506.233551	23.163226
103.643673	3510.480868	23.168243
104.046285	3527.648187	23.173261
104.292910	3516.216434	23.178279
104.469076	3527.255809	23.183296
104.567792	3529.056393	23.188314
104.805719	3526.353256	23.193331
104.747575	3516.461236	23.198349
104.669298	3519.580436	23.203367
104.729661	3513.653094	23.208384
104.576721	3524.302752	23.213402
104.816224	3516.348167	23.218419
104.837097	3513.958458	23.223437
104.683204	3531.141358	23.228455
104.901734	3532.699309	23.233472
104.945971	3541.028597	23.238490
104.931886	3539.760017	23.243507
105.454959	3561.435828	23.248525
105.598511	3567.503830	23.253543
105.508603	3566.298958	23.258560
105.461751	3575.874818	23.263578
105.443346	3590.059002	23.268595
105.925843	3598.152124	23.273613
106.020816	3604.672264	23.278631
106.464034	3609.623435	23.283648
106.589043	3606.256655	23.288666
106.462718	3602.977468	23.293683
106.404995	3604.532254	23.298701
106.571088	3624.476970	23.303719
106.669871	3621.725155	23.308736
106.965649	3627.745979	23.313754
106.677054	3632.417683	23.318771
106.890427	3635.750922	23.323789
106.878207	3650.423120	23.328807
107.085156	3657.764946	23.333824
107.459535	3663.651929	23.338842
107.512921	3653.347687	23.343859
107.703208	3650.632322	23.348877
107.994633	3661.343296	23.353895
107.907685	3669.327790	23.358912
108.370998	3672.466980	23.363930
108.269180	3686.124872	23.368947
108.687260	3666.196074	23.373965
108.702981	3668.113539	23.378983
108.644026	3675.670572	23.384000
108.860747	3672.343348	23.389018
108.498737	3671.832649	23.394035
109.042025	3671.802683	23.399053
109.051536	3671.361306	23.404071
108.917547	3657.425777	23.409088
109.039345	3657.337110	23.414106
109.025312	3660.761080	23.419123
109.354795	3654.843547	23.424141
109.274497	3651.161859	23.429159
109.687443	3657.145223	23.434176
109.482477	3650.877415	23.439194
109.563199	3663.087788	23.444211
109.610004	3680.886516	23.449229
109.723686	3681.644869	23.454247
110.063987	3685.102029	23.459264
109.820975	3682.405499	23.464282
109.806182	3690.798559	23.469299
110.319163	3691.846056	23.474317
110.255226	3714.902559	23.479335
110.052027	3706.272986	23.484352
110.467025	3717.102164	23.489370
110.611115	3738.266033	23.494387
110.916604	3741.989593	23.499405
110.860433	3731.967186	23.504423
110.758631	3751.960663	23.509440
110.927277	3743.551521	23.514458
110.682612	3768.485239	23.519475
111.215688	3757.222124	23.524493
111.407308	3758.217606	23.529511
111.397353	3769.139873	23.534528
111.635709	3785.202709	23.539546
111.867740	3786.040726	23.544563
111.998173	3781.141094	23.549581
111.756167	3796.319911	23.554599
112.027753	3795.751366	23.559616
112.325594	3809.157890	23.564634
112.178772	3829.612458	23.569651
112.566435	3826.203805	23.574669
112.841208	3818.899158	23.579687
112.967253	3827.012322	23.584704
113.230269	3832.116179	23.589722
112.928105	3850.968455	23.594739
112.935737	3847.331247	23.599757
113.318768	3855.077939	23.604775
113.561784	3852.953054	23.609792
113.911749	3858.319330	23.614810
113.335019	3852.642409	23.619827
113.722449	3844.183676	23.624845
113.519988	3853.513759	23.629863
113.533640	3865.247172	23.634880
113.979102	3867.783827	23.639898
113.805595	3872.050750	23.644915
114.071867	3882.401063	23.649933
114.605653	3903.795262	23.654951
114.552426	3902.350832	23.659968
114.662531	3888.177120	23.664986
114.477359	3908.208196	23.670003
114.835990	3908.080787	23.675021
114.988197	3903.275553	23.680039
115.021979	3926.495754	23.685056
115.249810	3929.886119	23.690074
115.367190	3925.366561	23.695091
115.637955	3918.734989	23.700109
115.736512	3931.919424	23.705127
115.498196	3938.317212	23.710144
115.989030	3926.192033	23.715162
115.635806	3930.475281	23.720179
115.877319	3936.038644	23.725197
116.045203	3945.015059	23.730215
115.719776	3950.440603	23.735232
116.353309	3954.306079	23.740250
116.363403	3946.301778	23.745267
116.489393	3948.775483	23.750285
116.311918	3961.912243	23.755303
116.652305	3972.894878	23.760320
116.747330	3973.618532	23.765338
116.724267	3977.046032	23.770355
116.735773	3983.125385	23.775373
117.165528	4007.884266	23.780391
117.054561	4011.539692	23.785408
117.146910	4009.002658	23.790426
117.195117	4020.865523	23.795443
117.659040	4036.797250	23.800461
117.704465	4037.287755	23.805479
117.730482	4033.786448	23.810496
118.258552	4025.370523	23.815514
118.497309	4027.482682	23.820531
118.284708	4033.082138	23.825549
118.536337	4040.502199	23.830567
118.486416	4041.681317	23.835584
119.001912	4048.503825	23.840602
118.884419	4059.501941	23.845619
118.874819	4053.663910	23.850637
119.366085	4052.031067	23.855655
118.852674	4053.764741	23.860672
119.379137	4053.832837	23.865690
119.389355	4071.087644	23.870707
119.392586	4061.395379	23.875725
119.387557	4076.304595	23.880743
119.289228	4085.620760	23.885760
119.829132	4086.319730	23.890778
119.429424	4100.584708	23.895795
119.784329	4096.258540	23.900813
120.017089	4114.458944	23.905831
120.570631	4126.625808	23.910848
120.501324	4129.820816	23.915866
120.554051	4130.064044	23.920883
120.868163	4129.339637	23.925901
121.067214	4129.589397	23.930919
120.833848	4121.796108	23.935936
120.950294	4122.513473	23.940954
121.093364	4145.237577	23.945971
121.197948	4148.342436	23.950989
121.503842	4159.435238	23.956007
121.253022	4166.634825	23.961024
121.301874	4164.478198	23.966042
121.328367	4181.568619	23.971059
121.629884	4191.022725	23.976077
121.918520	4190.411190	23.981095
121.740357	4211.580524	23.986112
122.285037	4216.507253	23.991130
122.312995	4220.243320	23.996147
122.433520	4210.329210	24.001165
122.625523	4216.491040	24.006183
122.640583	4244.222891	24.011200
122.962200	4238.813550	24.016218
122.721305	4249.420752	24.021235
123.209125	4246.665965	24.026253
123.334136	4236.635344	24.031271
123.529021	4265.151732	24.036288
123.851738	4279.708940	24.041306
124.165240	4278.009775	24.046323
124.272904	4272.314498	24.051341
124.408921	4277.419014	24.056359
124.580074	4265.870044	24.061376
124.634023	4228.635676	24.066394
124.455319	4242.031155	24.071411
124.294913	4233.111527	24.076429
124.566064	4240.868632	24.081447
124.494516	4254.772425	24.086464
124.687721	4275.020991	24.091482
124.671922	4264.896290	24.096499
124.446080	4267.325026	24.101517
124.754953	4284.410636	24.106535
124.637510	4292.146145	24.111552
124.723177	4305.466103	24.116570
124.976589	4305.110004	24.121587
125.024953	4315.783635	24.126605
125.282620	4325.840769	24.131623
125.303995	4344.005894	24.136640
125.280744	4351.216785	24.141658
125.748985	4351.417740	24.146675
125.841563	4375.579735	24.151693
126.431386	4378.294602	24.156711
126.261730	4392.291505	24.161728
126.764409	4376.901236	24.166746
127.017083	4378.940274	24.171763
126.862614	4380.423717	24.176781
127.243135	4393.933628	24.181799
127.329222	4413.300022	24.186816
127.460493	4402.377656	24.191834
127.777878	4416.755155	24.196851
127.461438	4410.118822	24.201869
127.710195	4404.416720	24.206887
127.383267	4405.083730	24.211904
127.617450	4413.828190	24.216922
127.631659	4440.626224	24.221939
127.529739	4437.562132	24.226957
128.258242	4442.022707	24.231975
128.452664	4460.434588	24.236992
128.215562	4467.510385	24.242010
128.486837	4471.271667	24.247027
128.700784	4469.962970	24.252045
128.847016	4482.181666	24.257063
128.982685	4490.364851	24.262080
129.173033	4488.228896	24.267098
129.392907	4489.074474	24.272115
129.461509	4490.718719	24.277133
129.839567	4490.791655	24.282151
129.931440	4496.939036	24.287168
129.959179	4491.466742	24.292186
130.042914	4508.991400	24.297203
130.274632	4500.800973	24.302221
130.797234	4492.140806	24.307239
130.612901	4508.329354	24.312256
130.376328	4495.830589	24.317274
130.656620	4500.251454	24.322291
130.162311	4505.435784	24.327309
130.493087	4517.664175	24.332327
130.704686	4525.005644	24.337344
130.828666	4535.314546	24.342362
131.025265	4550.750385	24.347379
130.861198	4561.999480	24.352397
131.265941	4564.909147	24.357415
131.214584	4600.070045	24.362432
131.810446	4593.345493	24.367450
131.523207	4600.031574	24.372467
131.887982	4606.559133	24.377485
132.125296	4614.386981	24.382503
132.218909	4614.719926	24.387520
132.197820	4617.381438	24.392538
132.680692	4616.758268	24.397555
132.659476	4631.062771	24.402573
132.914571	4635.810696	24.407591
133.279391	4651.817703	24.412608
133.240397	4650.431879	24.417626
133.753248	4645.109707	24.422643
133.844784	4651.453282	24.427661
133.768229	4649.398812	24.432679
133.845351	4650.860944	24.437696
134.209365	4665.865662	24.442714
134.050827	4650.918263	24.447731
133.961763	4638.866304	24.452749
134.326032	4642.669747	24.457767
134.187011	4640.778760	24.462784
133.971920	4641.213898	24.467802
134.638184	4655.719026	24.472819
134.370349	4668.309063	24.477837
134.728550	4662.220254	24.482855
134.473754	4675.412912	24.487872
134.683828	4689.845406	24.492890
135.272249	4688.369690	24.497907
134.953061	4706.871452	24.502925
135.496415	4707.512400	24.507943
135.164237	4723.107441	24.512960
135.369680	4731.833598	24.517978
135.459897	4732.543120	24.522995
135.714772	4751.945830	24.528013
136.338811	4756.317845	24.533031
135.967779	4761.110993	24.538048
136.335992	4761.490308	24.543066
136.622319	4769.507002	24.548083
136.705493	4780.570508	24.553101
137.071513	4778.866944	24.558119
136.929210	4773.356501	24.563136
136.765523	4773.205148	24.568154
137.409945	4789.963408	24.573171
137.234213	4803.925458	24.578189
137.427502	4802.120500	24.583207
137.681085	4806.626188	24.588224
137.589209	4822.373370	24.593242
137.868196	4822.109106	24.598259
138.030625	4845.749221	24.603277
138.059895	4837.323148	24.608295
138.411522	4846.297286	24.613312
138.241252	4868.524170	24.618330
138.724845	4867.789445	24.623347
138.493446	4874.473504	24.628365
139.161470	4877.114512	24.633383
139.041876	4890.320447	24.638400
139.347936	4890.398197	24.643418
139.476925	4883.902253	24.648435
139.243654	4893.102601	24.653453
139.654544	4908.361642	24.658471
139.972708	4910.461197	24.663488
140.099711	4922.245186	24.668506
140.537071	4921.899630	24.673523
140.236786	4924.787657	24.678541
140.508646	4914.650834	24.683559
140.503403	4920.341551	24.688576
140.370334	4918.968492	24.693594
140.552321	4926.976521	24.698611
140.185918	4930.151090	24.703629
140.674932	4931.709773	24.708647
140.672357	4954.992242	24.713664
140.751353	4951.392597	24.718682
141.245326	4972.163292	24.723699
141.332095	4991.145214	24.728717
141.644314	4989.214274	24.733735
141.882319	4992.837073	24.738752
141.703488	4994.626202	24.743770
142.239469	4997.564272	24.748787
142.351412	5013.081493	24.753805
142.991354	5027.754720	24.758823
143.221135	5016.162829	24.763840
142.948858	5028.145169	24.768858
143.270681	5017.712200	24.773875
143.148580	5022.621791	24.778893
143.141522	5017.701967	24.783911
143.439403	5017.774769	24.788928
143.205850	5015.305204	24.793946
143.456233	5015.765812	24.798963
143.389543	5035.659452	24.803981
143.834908	5039.105465	24.808999
143.920132	5043.887884	24.814016
143.723366	5053.124030	24.819034
144.364375	5057.597670	24.824051
144.456484	5070.719560	24.829069
144.282444	5064.927614	24.834087
144.688500	5072.261623	24.839104
144.671177	5072.712525	24.844122
144.721049	5087.156107	24.849139
144.918806	5090.048102	24.854157
144.936732	5098.810567	24.859175
145.494944	5111.667269	24.864192
145.592891	5121.352055	24.869210
145.773611	5127.153080	24.874227
145.895363	5136.085045	24.879245
146.190707	5136.191736	24.884263
146.257687	5142.530512	24.889280
146.203290	5155.888515	24.894298
146.521413	5146.616432	24.899315
146.342846	5150.225018	24.904333
146.782295	5176.644177	24.909351
146.814602	5175.389060	24.914368
146.935611	5181.947690	24.919386
147.098674	5186.825965	24.924403
147.467976	5185.911272	24.929421
147.583949	5206.781749	24.934439
147.638902	5217.982526	24.939456
147.980766	5217.282230	24.944474
148.040404	5206.750316	24.949491
148.306122	5213.256305	24.954509
148.500598	5214.763280	24.959527
148.272482	5221.860375	24.964544
148.472077	5236.927854	24.969562
148.818829	5236.460634	24.974579
148.820006	5233.378563	24.979597
148.723705	5235.142663	24.984615
149.197387	5248.836372	24.989632
148.728395	5256.935989	24.994650
148.845922	5248.411245	24.999667
149.234818	5279.216981	25.004685
149.351388	5282.959137	25.009703
149.636112	5311.574810	25.014720
149.747742	5328.528389	25.019738
149.922726	5333.802425	25.024755
149.816759	5350.210417	25.029773
150.224487	5353.123679	25.034791
150.798217	5353.630885	25.039808
150.874610	5370.526151	25.044826
151.185383	5363.178221	25.049843
151.759170	5371.239866	25.054861
152.041543	5366.519383	25.059879
151.661556	5349.830920	25.064896
152.032020	5367.532814	25.069914
152.094877	5365.170140	25.074931
152.429024	5360.270218	25.079949
152.311985	5362.273220	25.084967
152.283320	5360.501329	25.089984
152.446227	5359.260843	25.095002
152.694302	5358.785513	25.100019
152.395168	5356.396421	25.105037
152.416449	5357.533161	25.110055
152.915343	5359.767503	25.115072
152.614248	5380.075159	25.120090
152.936391	5381.274407	25.125107
152.782572	5382.054994	25.130125
152.925265	5407.942405	25.135143
153.231289	5418.930167	25.140160
153.237680	5438.492125	25.145178
153.688561	5445.392473	25.150195
153.821547	5451.627938	25.155213
153.531895	5463.185079	25.160231
153.971303	5479.834239	25.165248
154.110557	5480.391975	25.170266
154.078117	5498.974078	25.175283
154.653044	5510.732539	25.180301
154.821359	5512.119440	25.185319
155.635211	5522.349658	25.190336
156.247964	5524.848320	25.195354
156.474603	5516.452664	25.200371
156.722778	5500.245365	25.205389
156.612398	5483.245642	25.210407
156.828254	5485.463375	25.215424
156.867370	5484.712685	25.220442
157.067635	5473.645086	25.225459
157.126772	5473.740015	25.230477
156.886359	5473.044174	25.235495
157.117563	5467.278439	25.240512
157.102186	5471.460211	25.245530
156.886254	5469.943293	25.250547
156.921146	5471.137248	25.255565
156.969226	5498.166568	25.260583
157.171267	5484.091196	25.265600
157.418532	5517.623118	25.270618
157.450362	5528.230222	25.275635
157.771470	5537.057814	25.280653
157.806844	5560.430596	25.285671
157.829811	5568.239609	25.290688
158.106844	5584.351855	25.295706
158.134654	5598.186087	25.300723
158.336155	5598.294114	25.305741
158.489565	5626.088639	25.310759
158.431918	5621.775097	25.315776
158.942253	5649.973352	25.320794
159.508939	5659.927921	25.325811
159.831290	5664.333114	25.330829
159.828058	5666.976103	25.335847
159.587589	5671.130938	25.340864
159.701944	5697.331820	25.345882
159.968769	5699.006835	25.350899
160.406335	5708.928825	25.355917
160.338439	5724.279982	25.360935
160.814808	5720.909820	25.365952
161.094713	5716.768857	25.370970
161.034019	5722.479660	25.375987
161.773363	5726.015858	25.381005
161.511912	5734.912648	25.386023
161.789717	5746.047843	25.391040
161.790425	5737.948886	25.396058
162.229801	5735.272728	25.401075
162.326044	5730.373806	25.406093
162.038999	5742.731230	25.411111
162.449923	5766.938853	25.416128
162.365348	5775.742259	25.421146
162.154591	5780.372203	25.426163
162.603653	5774.475464	25.431181
162.471729	5795.521171	25.436199
162.820867	5800.392518	25.441216
162.882086	5804.017548	25.446234
163.402514	5816.627102	25.451251
164.240951	5803.990617	25.456269
163.808593	5803.928927	25.461287
164.373309	5810.847643	25.466304
164.557414	5802.007223	25.471322
164.261708	5801.708748	25.476339
164.507943	5799.594492	25.481357
164.772596	5822.391118	25.486375
164.849021	5818.567650	25.491392
164.990866	5835.894796	25.496410
165.162401	5836.874441	25.501427
165.337485	5820.384750	25.506445
165.051342	5839.641160	25.511463
165.168178	5862.406354	25.516480
165.504519	5867.267237	25.521498
165.635559	5887.284822	25.526515
166.103879	5901.542676	25.531533
165.851411	5903.819343	25.536551
166.010684	5903.332289	25.541568
166.011359	5922.328778	25.546586
165.955842	5940.238340	25.551603
166.782978	5947.607537	25.556621
166.565731	5959.835076	25.561639
167.298268	5974.042252	25.566656
167.274419	5978.968196	25.571674
167.231480	6000.728330	25.576691
167.566015	6004.514579	25.581709
167.758082	6015.116801	25.586727
167.778519	6011.807342	25.591744
168.396821	6026.330339	25.596762
168.502488	6045.658506	25.601779
168.491786	6048.484319	25.606797
168.479296	6063.246242	25.611815
169.010344	6070.929818	25.616832
169.251727	6083.495128	25.621850
168.968848	6095.250071	25.626867
169.122117	6086.682347	25.631885
169.527207	6106.711634	25.636903
169.707444	6111.377089	25.641920
169.763768	6116.377246	25.646938
170.076688	6137.966942	25.651955
170.184632	6146.529262	25.656973
170.296491	6152.022701	25.661991
170.804934	6173.283240	25.667008
170.797709	6172.749659	25.672026
170.830614	6178.232526	25.677044
171.028542	6174.550341	25.682061
170.973772	6188.779118	25.687079
171.455975	6198.253812	25.692096
171.625389	6200.229278	25.697114
171.774788	6209.621148	25.702132
172.244152	6223.914563	25.707149
172.407430	6238.689349	25.712167
172.623157	6232.542361	25.717184
172.465255	6233.117328	25.722202
172.704115	6254.286275	25.727220
173.038794	6256.917240	25.732237
172.811196	6263.496909	25.737255
173.106633	6255.582888	25.742272
173.350679	6274.623859	25.747290
173.251125	6280.976830	25.752308
173.584067	6295.785853	25.757325
173.647018	6309.521188	25.762343
173.797073	6315.375368	25.767360
174.088373	6319.460229	25.772378
174.350322	6333.332815	25.777396
174.539855	6339.513613	25.782413
175.095824	6346.060718	25.787431
174.888356	6348.546588	25.792448
175.130073	6337.709371	25.797466
175.444659	6349.154725	25.802484
175.460768	6353.676473	25.807501
175.581216	6371.618881	25.812519
175.444619	6368.546356	25.817536
175.937902	6372.390734	25.822554
175.966551	6391.324889	25.827572
176.597613	6387.198580	25.832589
176.321735	6390.872355	25.837607
176.726473	6398.098922	25.842624
176.894960	6411.351468	25.847642
176.863595	6431.483210	25.852660
177.157756	6418.831423	25.857677
176.957081	6431.384209	25.862695
176.976114	6440.704826	25.867712
177.664447	6440.181532	25.872730
177.706885	6467.497758	25.877748
178.369081	6471.895464	25.882765
178.288728	6474.608430	25.887783
178.393362	6480.556807	25.892800
178.627383	6498.571164	25.897818
178.584138	6505.836359	25.902836
178.878539	6506.509077	25.907853
178.922386	6516.098920	25.912871
179.054250	6510.065700	25.917888
179.373982	6540.455735	25.922906
179.313611	6544.075824	25.927924
179.771735	6558.887251	25.932941
180.114673	6574.800614	25.937959
180.194944	6578.207672	25.942976
180.370935	6583.596160	25.947994
180.277481	6599.157945	25.953012
180.981565	6610.428876	25.958029
180.831586	6626.989201	25.963047
181.011607	6633.910418	25.968064
181.134581	6649.941319	25.973082
181.240933	6663.472902	25.978100
181.701916	6657.413599	25.983117
181.901411	6683.834784	25.988135
182.052457	6699.655544	25.993152
182.417835	6701.943649	25.998170
182.441743	6703.243078	26.003188
182.745109	6715.162303	26.008205
182.798806	6714.284711	26.013223
183.055007	6717.159478	26.018240
183.333384	6718.256988	26.023258
183.196628	6739.600484	26.028276
183.206197	6739.395674	26.033293
183.736962	6754.899367	26.038311
183.708096	6760.105970	26.043328
184.399677	6754.386562	26.048346
184.260599	6755.379784	26.053364
184.336331	6785.078959	26.058381
184.651263	6782.343646	26.063399
184.758980	6797.629030	26.068416
185.316725	6790.719656	26.073434
185.464288	6813.733173	26.078452
185.915987	6811.257995	26.083469
185.963498	6814.344464	26.088487
185.958048	6815.257331	26.093504
186.326829	6802.537778	26.098522
186.178027	6808.397418	26.103540
186.428932	6827.895503	26.108557
186.325396	6833.588584	26.113575
186.494777	6841.684342	26.118592
186.780813	6847.096479	26.123610
186.696214	6861.963999	26.128628
186.898953	6880.296627	26.133645
186.677052	6876.625365	26.138663
187.090921	6909.834244	26.143680
187.730710	6904.643926	26.148698
187.990286	6916.100357	26.153716
188.262158	6921.338444	26.158733
188.311603	6934.543369	26.163751
188.336278	6933.090905	26.168768
188.561123	6932.252754	26.173786
188.816046	6958.717223	26.178804
189.121930	6953.474948	26.183821
189.341267	6967.985983	26.188839
189.192544	6983.587207	26.193856
189.671908	6984.717685	26.198874
189.594548	6996.570866	26.203892
189.698610	7016.445494	26.208909
190.193239	7032.317719	26.213927
190.209581	7032.352786	26.218944
190.223630	7045.727468	26.223962
190.315597	7064.197537	26.228980
190.862549	7078.762443	26.233997
191.416173	7089.902640	26.239015
191.317064	7095.883339	26.244032
191.198336	7098.813823	26.249050
191.254277	7117.134752	26.254068
191.588985	7131.871815	26.259085
191.679612	7142.828645	26.264103
191.959339	7157.814242	26.269120
192.650480	7163.951867	26.274138
192.603364	7182.486796	26.279156
192.851410	7178.329060	26.284173
193.210461	7192.150132	26.289191
193.341204	7198.334682	26.294208
193.725217	7188.973727	26.299226
193.443500	7212.270614	26.304244
193.750599	7211.564563	26.309261
194.094581	7225.624431	26.314279
194.213810	7247.983263	26.319296
194.531681	7255.145033	26.324314
194.689042	7253.142144	26.329332
194.781010	7268.751924	26.334349
195.143617	7278.781809	26.339367
195.463290	7292.763844	26.344384
195.764103	7289.812615	26.349402
195.357919	7311.066720	26.354420
196.003300	7312.410011	26.359437
195.969326	7304.349845	26.364455
196.358060	7328.579690	26.369472
196.388727	7336.189047	26.374490
196.533393	7355.334382	26.379508
196.713957	7353.504068	26.384525
196.915049	7365.124071	26.389543
196.887607	7376.443963	26.394560
197.369749	7391.538894	26.399578
197.447763	7396.150738	26.404596
197.840560	7407.230310	26.409613
198.118380	7410.482832	26.414631
198.134803	7433.627609	26.419648
198.532034	7430.035071	26.424666
198.613230	7435.237100	26.429684
198.817453	7454.846063	26.434701
199.275292	7456.172309	26.439719
199.094296	7454.463154	26.444736
199.635689	7466.357799	26.449754
199.790015	7485.509572	26.454772
199.631476	7487.010907	26.459789
199.997988	7490.821378	26.464807
200.012552	7488.460853	26.469824
200.708599	7488.808923	26.474842
200.372595	7503.004228	26.479860
200.805120	7504.501633	26.484877
201.268598	7502.701744	26.489895
200.730377	7535.906215	26.494912
201.030378	7526.562880	26.499930
201.394228	7551.916366	26.504948
201.218481	7561.028819	26.509965
201.780391	7571.762374	26.514983
201.815830	7592.829688	26.520000
202.028900	7601.906278	26.525018
202.528911	7616.365236	26.530036
202.321527	7635.538360	26.535053
202.884167	7632.442208	26.540071
202.832054	7641.360219	26.545088
203.198425	7659.717913	26.550106
203.235154	7678.193889	26.555124
203.369086	7684.651404	26.560141
203.976094	7686.579964	26.565159
203.972239	7718.492269	26.570176
204.350642	7717.668877	26.575194
204.398111	7734.514359	26.580212
204.417365	7746.370254	26.585229
204.956355	7743.155121	26.590247
204.861946	7776.374980	26.595264
205.129637	7779.716678	26.600282
205.604132	7793.386884	26.605300
205.833441	7807.146446	26.610317
206.100928	7812.072084	26.615335
206.396335	7827.209313	26.620352
206.641565	7829.895495	26.625370
206.880062	7849.149582	26.630388
206.960802	7846.774919	26.635405
207.120140	7858.344688	26.640423
207.261148	7871.272203	26.645440
207.464047	7886.857964	26.650458
207.845330	7903.644536	26.655476
207.433579	7911.010642	26.660493
207.921758	7911.278077	26.665511
208.105399	7937.904038	26.670528
208.418699	7945.348848	26.675546
208.537530	7964.192015	26.680564
208.684444	7971.672992	26.685581
209.574230	7988.206298	26.690599
209.348845	7991.992604	26.695616
209.320139	7994.405085	26.700634
209.828892	8014.430703	26.705652
210.010053	8025.084915	26.710669
210.280867	8016.705448	26.715687
210.355205	8048.859116	26.720704
210.578877	8057.164702	26.725722
210.776914	8061.983749	26.730740
210.893352	8089.864737	26.735757
211.340496	8085.486414	26.740775
211.170989	8098.176356	26.745792
211.741493	8110.582579	26.750810
212.054221	8099.173208	26.755828
212.167242	8122.048627	26.760845
212.279462	8136.590250	26.765863
212.426136	8151.761028	26.770880
212.927721	8157.837426	26.775898
213.292466	8157.051713	26.780916
213.172434	8175.300550	26.785933
213.431339	8163.966975	26.790951
213.488114	8185.176477	26.795968
213.436979	8191.971955	26.800986
214.512850	8199.676836	26.806004
214.070586	8213.465006	26.811021
214.338287	8220.633931	26.816039
214.443397	8225.262020	26.821056
214.467742	8237.046553	26.826074
214.568170	8250.678143	26.831092
214.866950	8270.277221	26.836109
215.066267	8283.985442	26.841127
215.315702	8296.870973	26.846144
215.414502	8311.697738	26.851162
215.666003	8327.183750	26.856180
215.750972	8339.732597	26.861197
216.466537	8358.988823	26.866215
216.684192	8371.968670	26.871232
216.852778	8395.641065	26.876250
217.358664	8398.404790	26.881268
217.219779	8416.251380	26.886285
217.912410	8402.154582	26.891303
218.033546	8422.607078	26.896320
218.213364	8443.587081	26.901338
218.582076	8440.309365	26.906356
218.349065	8452.767486	26.911373
218.854767	8464.093799	26.916391
219.241054	8464.108705	26.921408
218.987255	8473.688264	26.926426
219.288580	8496.444894	26.931444
219.683778	8503.013171	26.936461
219.841537	8510.311451	26.941479
220.152068	8523.260324	26.946496
220.096488	8525.964819	26.951514
220.547048	8542.549225	26.956532
220.745817	8562.191180	26.961549
220.794468	8559.429461	26.966567
221.195826	8579.268749	26.971584
221.127019	8589.918957	26.976602
221.242367	8605.460030	26.981620
221.333941	8618.508169	26.986637
221.889033	8628.858409	26.991655
222.433132	8644.409024	26.996672
222.601329	8663.905713	27.001690
223.197434	8669.731972	27.006708
222.956139	8674.043285	27.011725
223.388185	8675.721261	27.016743
223.775574	8696.364056	27.021760
223.736910	8703.992614	27.026778
224.067552	8713.537194	27.031796
224.079053	8735.554389	27.036813
224.191411	8732.710437	27.041831
224.979630	8738.067827	27.046848
225.438803	8748.625396	27.051866
225.613651	8744.362773	27.056884
225.772125	8743.585121	27.061901
226.356278	8738.571970	27.066919
226.011759	8744.583596	27.071936
226.132068	8761.844262	27.076954
226.513121	8775.227509	27.081972
226.408500	8766.929368	27.086989
226.565545	8782.959956	27.092007
226.774455	8805.073810	27.097024
227.172424	8803.968299	27.102042
227.299928	8823.379751	27.107060
227.149374	8835.976568	27.112077
227.126077	8859.154407	27.117095
227.443124	8865.434857	27.122112
227.286570	8886.804994	27.127130
227.544139	8912.223905	27.132148
228.145204	8934.753628	27.137165
228.363221	8951.984967	27.142183
228.605645	8970.750623	27.147200
228.622591	8994.704172	27.152218
229.013987	9010.250445	27.157236
229.178711	9021.015167	27.162253
229.443353	9057.048682	27.167271
229.874289	9063.617590	27.172288
229.795682	9086.883666	27.177306
230.118386	9091.286227	27.182324
230.418564	9111.995170	27.187341
231.003206	9133.005299	27.192359
231.235888	9142.666358	27.197376
231.282416	9141.534608	27.202394
231.651764	9163.122274	27.207412
232.005972	9170.089081	27.212429
232.379698	9182.181290	27.217447
232.492754	9191.022470	27.222464
232.609882	9195.922972	27.227482
233.363149	9218.648506	27.232500
233.364883	9230.637585	27.237517
233.460293	9235.340039	27.242535
233.553658	9246.323866	27.247552
233.519865	9268.851040	27.252570
234.055344	9273.648577	27.257588
234.195912	9305.424419	27.262605
234.391782	9308.796427	27.267623
234.525641	9337.368321	27.272640
234.857365	9355.811690	27.277658
234.670781	9367.602765	27.282676
235.199278	9385.213359	27.287693
235.360844	9397.271468	27.292711
236.118764	9408.193660	27.297728
236.209883	9422.901426	27.302746
236.331002	9439.584523	27.307764
236.481287	9453.457033	27.312781
237.097234	9477.683350	27.317799
237.051846	9493.266814	27.322816
237.419030	9509.560379	27.327834
237.533530	9514.308599	27.332852
237.930288	9529.403929	27.337869
237.842881	9553.902533	27.342887
238.393044	9563.212855	27.347904
237.850116	9584.588684	27.352922
238.325393	9593.402538	27.357940
238.729506	9613.272597	27.362957
239.069228	9647.306871	27.367975
239.473100	9650.356285	27.372992
239.488277	9666.489185	27.378010
239.984823	9680.965574	27.383028
240.396557	9695.343346	27.388045
240.739178	9706.527349	27.393063
241.340140	9713.692305	27.398080
241.119876	9723.341904	27.403098
241.568150	9731.701060	27.408116
241.848354	9730.182493	27.413133
242.315945	9738.246220	27.418151
242.697527	9755.980751	27.423168
242.450182	9767.823121	27.428186
242.793991	9759.704807	27.433204
243.260177	9772.447022	27.438221
242.774290	9802.235971	27.443239
243.437689	9790.573680	27.448256
243.624087	9806.722545	27.453274
243.883291	9826.841312	27.458292
243.627284	9832.386570	27.463309
243.798753	9845.051500	27.468327
244.296825	9864.558178	27.473344
244.501947	9876.851284	27.478362
244.538624	9893.834750	27.483380
244.826919	9906.168490	27.488397
244.927792	9932.527100	27.493415
245.193530	9941.794837	27.498432
245.347924	9959.960204	27.503450
245.750759	9979.567045	27.508468
245.913627	9995.716838	27.513485
246.106729	10019.222176	27.518503
246.446402	10024.386290	27.523520
246.580801	10064.253841	27.528538
246.956085	10063.214229	27.533556
247.422754	10084.475912	27.538573
248.145874	10076.266413	27.543591
248.683211	10098.378218	27.548608
249.315711	10102.369886	27.553626
249.503281	10102.427872	27.558644
249.604920	10101.846239	27.563661
249.701420	10098.862874	27.568679
249.815163	10088.219127	27.573696
249.812662	10090.390489	27.578714
250.002330	10114.329787	27.583732
250.716892	10120.376487	27.588749
250.400232	10132.807199	27.593767
250.578562	10138.272138	27.598784
250.869206	10147.063240	27.603802
251.090049	10175.024374	27.608820
251.318949	10198.418506	27.613837
251.199488	10208.123426	27.618855
251.762054	10215.264233	27.623872
251.493953	10240.070237	27.628890
251.966586	10266.960359	27.633908
252.414176	10284.360812	27.638925
252.471676	10295.584459	27.643943
253.065379	10316.359910	27.648960
253.017423	10322.458618	27.653978
253.298568	10348.515573	27.658996
253.809358	10352.936253	27.664013
253.943726	10385.859075	27.669031
254.206820	10399.790970	27.674048
254.374017	10411.625984	27.679066
254.525351	10432.850427	27.684084
255.008645	10449.967087	27.689101
255.443791	10464.906503	27.694119
255.790514	10469.287363	27.699136
256.285473	10498.980940	27.704154
256.362684	10505.809766	27.709172
256.563047	10508.145394	27.714189
256.992266	10533.025706	27.719207
257.311045	10545.050044	27.724224
257.431928	10541.104660	27.729242
257.534034	10551.919363	27.734260
257.829118	10557.823630	27.739277
257.769020	10591.232749	27.744295
258.045904	10585.872768	27.749312
258.244510	10612.204536	27.754330
258.670896	10625.466053	27.759348
259.147358	10647.859667	27.764365
259.093073	10662.272767	27.769383
259.620870	10681.386382	27.774400
259.960456	10688.953397	27.779418
260.120738	10701.085965	27.784436
261.004992	10715.292850	27.789453
260.769765	10721.150084	27.794471
261.054741	10724.548637	27.799488
261.055742	10743.382263	27.804506
261.158972	10751.860410	27.809524
261.797279	10769.096752	27.814541
261.930170	10774.341752	27.819559
262.274010	10785.977703	27.824576
262.354758	10808.463702	27.829594
262.294649	10807.504643	27.834612
262.965668	10827.713400	27.839629
262.627989	10842.027745	27.844647
262.827598	10870.033778	27.849664
262.953963	10889.306133	27.854682
263.167216	10921.471793	27.859700
263.684538	10935.782825	27.864717
263.609433	10952.130455	27.869735
264.260880	10970.802530	27.874752
264.448859	11005.289378	27.879770
264.714528	11028.718826	27.884788
265.391170	11044.564220	27.889805
265.663667	11072.613710	27.894823
266.122453	11071.518489	27.899840
266.684154	11089.602092	27.904858
266.812716	11100.456910	27.909876
267.161692	11103.054039	27.914893
267.125347	11118.936159	27.919911
267.800135	11135.694990	27.924928
267.609980	11135.329325	27.929946
267.750512	11173.578157	27.934964
267.984907	11176.268280	27.939981
268.043324	11198.528482	27.944999
268.490907	11216.010307	27.950016
268.673082	11237.010928	27.955034
268.889602	11263.921407	27.960052
269.279006	11270.220793	27.965069
269.575947	11306.773989	27.970087
269.887462	11321.246990	27.975104
270.385839	11332.774302	27.980122
270.669034	11359.275302	27.985140
270.983496	11365.146731	27.990157
271.080516	11375.404285	27.995175
271.658631	11393.797487	28.000192
271.980978	11410.966190	28.005210
272.200052	11421.914988	28.010228
272.488029	11422.072988	28.015245
272.485801	11453.441038	28.020263
272.804209	11455.249175	28.025280
273.132195	11482.027374	28.030298
273.268748	11497.340085	28.035316
273.594670	11513.874916	28.040333
273.915825	11542.090505	28.045351
273.869347	11565.044478	28.050368
274.092262	11573.680543	28.055386
274.192031	11599.197552	28.060404
274.758349	11612.874791	28.065421
275.033521	11641.993099	28.070439
275.727510	11642.446416	28.075456
275.785791	11658.867265	28.080474
275.916168	11691.819424	28.085492
276.513384	11700.402385	28.090509
276.637895	11708.812134	28.095527
277.440761	11733.121292	28.100544
277.972920	11726.295185	28.105562
277.923982	11732.599422	28.110580
278.276190	11743.389365	28.115597
278.415893	11766.035557	28.120615
278.575426	11765.322190	28.125632
279.107111	11763.360106	28.130650
279.106430	11800.026620	28.135668
279.279233	11803.726762	28.140685
279.573440	11833.626148	28.145703
279.534723	11842.911413	28.150720
280.059303	11867.638601	28.155738
279.841097	11887.147127	28.160756
280.313108	11890.592236	28.165773
280.529975	11921.140333	28.170791
280.729912	11937.541214	28.175808
281.100661	11963.870396	28.180826
281.308804	11972.932964	28.185844
281.703759	11988.697419	28.190861
281.390811	12011.333653	28.195879
281.927605	12037.306211	28.200896
282.693971	12059.963521	28.205914
282.432164	12080.892847	28.210932
283.020995	12101.579249	28.215949
282.888495	12122.090199	28.220967
283.530874	12144.752356	28.225984
284.178098	12151.798117	28.231002
284.416351	12175.425211	28.236020
284.547292	12198.620215	28.241037
284.750930	12212.285404	28.246055
285.471795	12227.167448	28.251072
286.027911	12225.159519	28.256090
286.294637	12246.725763	28.261108
286.500970	12269.048883	28.266125
286.898153	12258.213488	28.271143
287.099501	12290.955826	28.276160
287.406146	12305.218591	28.281178
287.553634	12310.668886	28.286196
288.054153	12320.309681	28.291213
288.350245	12325.409264	28.296231
288.125756	12346.141322	28.301248
288.887921	12341.138631	28.306266
288.729375	12371.176054	28.311284
289.431370	12384.106723	28.316301
289.554044	12398.180944	28.321319
289.395618	12425.806858	28.326336
289.588945	12444.914810	28.331354
290.014470	12464.386226	28.336372
290.456628	12479.992886	28.341389
290.988583	12509.203487	28.346407
290.671848	12531.819802	28.351424
290.976604	12550.547059	28.356442
291.441079	12579.789421	28.361460
291.757967	12590.325778	28.366477
292.190097	12613.173023	28.371495
292.425386	12636.533412	28.376512
293.024014	12637.337360	28.381530
292.850461	12664.952000	28.386548
293.341862	12685.247928	28.391565
292.989352	12703.789289	28.396583
293.537126	12726.879160	28.401600
294.433101	12761.817702	28.406618
294.207178	12783.755986	28.411636
294.782768	12789.544618	28.416653
295.096462	12818.304938	28.421671
295.502540	12847.839489	28.426688
296.093655	12848.898382	28.431706
295.893634	12877.125990	28.436724
296.418655	12908.591761	28.441741
296.602882	12926.535740	28.446759
296.797177	12951.835215	28.451776
297.698925	12950.033250	28.456794
297.794647	12980.433974	28.461812
298.296058	12988.452007	28.466829
298.530931	13004.178511	28.471847
298.469275	13017.005793	28.476864
299.154417	13034.518898	28.481882
299.356223	13043.984145	28.486900
299.374599	13054.010731	28.491917
299.782023	13066.875588	28.496935
300.093251	13093.974386	28.501952
300.130096	13098.946076	28.506970
300.205859	13117.237519	28.511988
300.713991	13137.693557	28.517005
301.297411	13155.218872	28.522023
300.897306	13178.974956	28.527040
301.043910	13189.286140	28.532058
301.505087	13218.158323	28.537076
301.954807	13241.780406	28.542093
302.075354	13269.601188	28.547111
302.449132	13289.190878	28.552128
302.927166	13311.632858	28.557146
303.369052	13347.449759	28.562164
303.844405	13364.406964	28.567181
304.151246	13382.879565	28.572199
304.364338	13417.291000	28.577216
304.744626	13425.431689	28.582234
304.825037	13459.294697	28.587252
305.277032	13479.802989	28.592269
305.654671	13484.636554	28.597287
305.432407	13522.345786	28.602304
305.880006	13542.193048	28.607322
306.220857	13565.827288	28.612340
306.747940	13577.344382	28.617357
307.495414	13581.677230	28.622375
307.715720	13625.227577	28.627392
308.122852	13623.280341	28.632410
308.486130	13649.882971	28.637428
308.667970	13649.173719	28.642445
308.895024	13672.949828	28.647463
308.867613	13693.756630	28.652480
309.338969	13706.601980	28.657498
309.606549	13725.662936	28.662516
309.862847	13755.130915	28.667533
310.517433	13774.430550	28.672551
310.705156	13783.282412	28.677568
311.026573	13818.225188	28.682586
311.652482	13833.211868	28.687604
311.336057	13858.803566	28.692621
311.599860	13870.854449	28.697639
311.813081	13897.761199	28.702656
312.381253	13923.800950	28.707674
312.472127	13957.105422	28.712692
313.047605	13972.396820	28.717709
313.363542	13992.721805	28.722727
313.639718	14010.870838	28.727744
314.296732	14037.980277	28.732762
314.443062	14054.141604	28.737780
314.967750	14067.736415	28.742797
315.828862	14076.700961	28.747815
316.002497	14093.212383	28.752832
316.329479	14094.901221	28.757850
316.398276	14112.295125	28.762868
316.218106	14138.116889	28.767885
316.934280	14149.174522	28.772903
317.065002	14168.605296	28.777920
317.365982	14192.176123	28.782938
317.480628	14196.473434	28.787956
317.706271	14223.362913	28.792973
318.172794	14256.947904	28.797991
318.178106	14276.264001	28.803008
318.509251	14307.956779	28.808026
318.383162	14331.454956	28.813044
318.640875	14364.534140	28.818061
319.271433	14399.912468	28.823079
319.625593	14431.133647	28.828096
320.234461	14458.615774	28.833114
320.466390	14477.897823	28.838132
320.764445	14492.854180	28.843149
321.108987	14507.123660	28.848167
321.556808	14537.530593	28.853184
322.519693	14530.891402	28.858202
323.100860	14551.950187	28.863220
323.285497	14562.952508	28.868237
323.819665	14557.451015	28.873255
323.673154	14576.850858	28.878272
323.894445	14581.365462	28.883290
324.401678	14596.930325	28.888308
324.329932	14621.211045	28.893325
324.706873	14620.482129	28.898343
324.606233	14653.506061	28.903360
324.726321	14677.594431	28.908378
325.101133	14694.742991	28.913396
324.984216	14728.541959	28.918413
325.518584	14756.506520	28.923431
325.721145	14790.040089	28.928448
326.159954	14825.203601	28.933466
326.496275	14850.036586	28.938484
326.476373	14894.498350	28.943501
327.226877	14913.170462	28.948519
327.496211	14951.915973	28.953536
328.246422	14973.905548	28.958554
328.707913	15009.748093	28.963572
329.251033	15032.752196	28.968589
329.723551	15044.249409	28.973607
329.698473	15077.442948	28.978624
330.038038	15101.513022	28.983642
330.887407	15109.920625	28.988660
330.722534	15143.118480	28.993677
331.420121	15152.816672	28.998695
331.719319	15168.619750	29.003712
332.142931	15184.793127	29.008730
332.817877	15209.056956	29.013748
332.973263	15219.487753	29.018765
333.315839	15234.546178	29.023783
333.417925	15259.803019	29.028800
333.622287	15265.463186	29.033818
334.225942	15294.236727	29.038836
333.974407	15315.725620	29.043853
334.636699	15327.642412	29.048871
334.755368	15354.847714	29.053888
334.952347	15383.163796	29.058906
335.050233	15406.821940	29.063924
335.267084	15441.021126	29.068941
335.760753	15463.178247	29.073959
335.999203	15503.512459	29.078976
336.258593	15538.237505	29.083994
336.994755	15547.812938	29.089012
337.005060	15587.595625	29.094029
337.703844	15615.908012	29.099047
337.846144	15642.668609	29.104064
338.301461	15672.302604	29.109082
338.645908	15696.011843	29.114100
338.955884	15727.996138	29.119117
339.530533	15745.327129	29.124135
339.922544	15774.692814	29.129152
340.046759	15801.784470	29.134170
341.032318	15814.787677	29.139188
341.211849	15824.321268	29.144205
341.384298	15854.141013	29.149223
342.047924	15876.505448	29.154240
342.354489	15897.422217	29.159258
342.992806	15906.219709	29.164276
343.052672	15927.929038	29.169293
343.383583	15946.681111	29.174311
343.694752	15960.626413	29.179328
343.847567	15977.835063	29.184346
343.930247	15980.267373	29.189364
344.639088	15994.979156	29.194381
344.925696	16005.051505	29.199399
345.491723	16029.109176	29.204416
345.523238	16041.217378	29.209434
346.274198	16049.140550	29.214452
346.274830	16080.648664	29.219469
346.375794	16088.825806	29.224487
346.852164	16107.305019	29.229504
346.644423	16135.036779	29.234522
347.191136	16136.126886	29.239540
347.732665	16169.282622	29.244557
348.703290	16190.967928	29.249575
348.574449	16202.040478	29.254592
348.887175	16230.524881	29.259610
349.498892	16255.773143	29.264628
349.535716	16277.359080	29.269645
349.711544	16310.674807	29.274663
349.977992	16340.158391	29.279680
350.338224	16365.473585	29.284698
350.525986	16389.628949	29.289716
350.665066	16407.270587	29.294733
351.280145	16429.347497	29.299751
351.659536	16461.317030	29.304768
351.813887	16491.818640	29.309786
352.600357	16527.213655	29.314804
352.835793	16554.954867	29.319821
353.182883	16577.894240	29.324839
353.566746	16602.775623	29.329856
353.446775	16640.539766	29.334874
353.809347	16660.729557	29.339892
354.364430	16705.876692	29.344909
354.897007	16747.538165	29.349927
355.139797	16761.911539	29.354944
355.266456	16799.972593	29.359962
355.989158	16829.756799	29.364980
355.980903	16870.272251	29.369997
356.585824	16887.701903	29.375015
357.150681	16915.507513	29.380032
357.245675	16946.120644	29.385050
357.598383	16979.039693	29.390068
357.920448	17024.303427	29.395085
357.689317	17040.626208	29.400103
358.282809	17069.650431	29.405120
358.845702	17117.960720	29.410138
359.710680	17144.999995	29.415156
360.113216	17182.709011	29.420173
360.282535	17210.933521	29.425191
360.963620	17241.689956	29.430208
361.163829	17272.172828	29.435226
361.532894	17294.338830	29.440244
362.058541	17328.060645	29.445261
362.377544	17338.795181	29.450279
362.567229	17385.226072	29.455296
362.603997	17411.682294	29.460314
363.162407	17446.421875	29.465332
363.685809	17468.899917	29.470349
364.008287	17502.088227	29.475367
364.579346	17509.706108	29.480384
364.697966	17542.759525	29.485402
365.441285	17563.354079	29.490420
365.807465	17587.038820	29.495437
366.179076	17605.365224	29.500455
366.668042	17641.804790	29.505472
366.881022	17669.833730	29.510490
367.641316	17673.325467	29.515508
368.058973	17713.323416	29.520525
368.079792	17719.027364	29.525543
368.317703	17737.000865	29.530560
368.486386	17754.418389	29.535578
368.612270	17783.796956	29.540596
368.862228	17807.094550	29.545613
369.145968	17829.224929	29.550631
369.662854	17857.145664	29.555648
369.650305	17892.700836	29.560666
370.258388	17920.073850	29.565684
370.808555	17946.000047	29.570701
371.368677	17982.332462	29.575719
371.945020	18006.195877	29.580736
371.978004	18044.123959	29.585754
372.620782	18069.918411	29.590772
372.677360	18100.451760	29.595789
372.828506	18121.508949	29.600807
373.118548	18157.678302	29.605824
373.633126	18187.522994	29.610842
373.954250	18208.140814	29.615860
373.968225	18257.349007	29.620877
374.600212	18279.753474	29.625895
375.144952	18321.251411	29.630912
375.303733	18363.558783	29.635930
375.837036	18392.443960	29.640948
376.034379	18429.530844	29.645965
376.759746	18457.971426	29.650983
377.424691	18486.847633	29.656000
377.525917	18519.508655	29.661018
377.992501	18559.330331	29.666036
378.502839	18574.915811	29.671053
378.841078	18609.760417	29.676071
379.273027	18639.621152	29.681088
379.295098	18684.210748	29.686106
380.014120	18707.632315	29.691124
380.556193	18734.722818	29.696141
380.794493	18761.696459	29.701159
381.564167	18798.229344	29.706176
381.679645	18832.879501	29.711194
381.885266	18839.593670	29.716212
382.269279	18890.801274	29.721229
382.310451	18921.745370	29.726247
383.282336	18954.906560	29.731264
383.228645	18986.846918	29.736282
383.827261	19013.670020	29.741300
384.706601	19042.415626	29.746317
384.413560	19066.143603	29.751335
385.487748	19091.200022	29.756352
385.625825	19120.927316	29.761370
386.051635	19140.362516	29.766388
386.620251	19159.129427	29.771405
386.875709	19194.849619	29.776423
387.722810	19209.062246	29.781440
387.710447	19245.611808	29.786458
387.903462	19270.481452	29.791476
388.483705	19294.264115	29.796493
388.274321	19319.632227	29.801511
388.719280	19352.123032	29.806528
388.974496	19395.224198	29.811546
389.329515	19443.551980	29.816564
389.744241	19473.743371	29.821581
390.141951	19514.106800	29.826599
390.454052	19543.348954	29.831616
390.787701	19589.331891	29.836634
391.163631	19629.880483	29.841652
391.832906	19662.803026	29.846669
392.401247	19686.161017	29.851687
393.421336	19687.483733	29.856704
393.957590	19728.240963	29.861722
394.600256	19733.948499	29.866740
394.990840	19749.121361	29.871757
394.957241	19766.229185	29.876775
395.441953	19779.620963	29.881792
395.480096	19799.549756	29.886810
395.732839	19831.439538	29.891828
396.052326	19846.960008	29.896845
396.192363	19877.238495	29.901863
396.589687	19901.641821	29.906880
396.877575	19933.497618	29.911898
397.115691	19965.568208	29.916916
397.538282	19997.256845	29.921933
397.759624	20028.934647	29.926951
398.434528	20062.293721	29.931968
398.648672	20103.286368	29.936986
398.920861	20140.134547	29.942004
399.528237	20184.046619	29.947021
399.776841	20215.209507	29.952039
400.375249	20266.341790	29.957056
400.769194	20290.784080	29.962074
401.183365	20319.950832	29.967092
402.071692	20347.972053	29.972109
402.095572	20378.680515	29.977127
402.515674	20411.612596	29.982144
402.911676	20462.898728	29.987162
402.998255	20495.477766	29.992180
403.644190	20523.692241	29.997197
403.649008	20563.845658	30.002215
404.019897	20610.805826	30.007232
404.580710	20655.515069	30.012250
404.566859	20695.594638	30.017268
405.213871	20750.546501	30.022285
405.625378	20794.284438	30.027303
405.975059	20844.707593	30.032320
406.151704	20888.044728	30.037338
406.727902	20935.585153	30.042356
407.568815	20980.685688	30.047373
407.787209	21020.357190	30.052391
408.432623	21052.578568	30.057408
408.712450	21096.045813	30.062426
409.008270	21151.290331	30.067444
409.722845	21181.019080	30.072461
409.831422	21226.799344	30.077479
410.607727	21273.260854	30.082496
410.772551	21315.398149	30.087514
411.356206	21344.975396	30.092532
412.147057	21387.253825	30.097549
412.395091	21419.949879	30.102567
413.435024	21447.484400	30.107584
413.937846	21467.622200	30.112602
414.065748	21513.125732	30.117620
414.685058	21521.841097	30.122637
415.024605	21560.563693	30.127655
415.453715	21578.946475	30.132672
415.679475	21615.442963	30.137690
415.967089	21649.681119	30.142708
416.590362	21676.941153	30.147725
417.757898	21695.055462	30.152743
418.347220	21698.558979	30.157760
419.007577	21732.742040	30.162778
418.849396	21741.023112	30.167796
419.770906	21760.666427	30.172813
419.609708	21779.254147	30.177831
420.051546	21801.633292	30.182848
420.429579	21818.074536	30.187866
420.665115	21858.891370	30.192884
421.406759	21872.543521	30.197901
421.457169	21895.887686	30.202919
422.152059	21908.361988	30.207936
421.948630	21937.393939	30.212954
421.945098	21961.204319	30.217972
422.630952	21992.471713	30.222989
422.484369	22030.979295	30.228007
423.056581	22062.024369	30.233024
423.485426	22099.962496	30.238042
423.575422	22128.342461	30.243060
424.346313	22158.571316	30.248077
424.409734	22215.106409	30.253095
424.785002	22252.960710	30.258112
425.031441	22298.303314	30.263130
425.386257	22344.202033	30.268148
425.954386	22385.594284	30.273165
426.360284	22434.731120	30.278183
426.940349	22466.010564	30.283200
427.318808	22518.798968	30.288218
427.929671	22570.347733	30.293236
428.852877	22603.756002	30.298253
428.807282	22641.899853	30.303271
429.444488	22675.852158	30.308288
430.502893	22699.790886	30.313306
430.767735	22734.156416	30.318324
431.753251	22754.449377	30.323341
431.942015	22791.265132	30.328359
432.513804	22820.774415	30.333376
432.861809	22843.238246	30.338394
433.020880	22881.065027	30.343412
433.509691	22911.688705	30.348429
433.854968	22950.080871	30.353447
434.091944	22985.881579	30.358464
434.417416	23017.631389	30.363482
434.418600	23054.376218	30.368500
435.030437	23102.899179	30.373517
435.325483	23157.486618	30.378535
435.489486	23193.900549	30.383552
436.297459	23241.019763	30.388570
436.417982	23293.276116	30.393588
437.368824	23334.605903	30.398605
437.411437	23374.554808	30.403623
437.506981	23424.819547	30.408640
438.396392	23481.151483	30.413658
438.342066	23534.754045	30.418676
438.479327	23579.500037	30.423693
438.946659	23639.189750	30.428711
439.738280	23686.891580	30.433728
440.329929	23750.736421	30.438746
440.723583	23810.833102	30.443764
441.824721	23842.491023	30.448781
442.166221	23885.679342	30.453799
442.556805	23931.950164	30.458816
443.273379	23969.400312	30.463834
443.967998	24000.280519	30.468852
445.081662	24023.830422	30.473869
445.411390	24071.798850	30.478887
445.726168	24089.190956	30.483904
446.389803	24117.629301	30.488922
446.298651	24145.749289	30.493940
446.822426	24175.096999	30.498957
446.905838	24221.763096	30.503975
447.211809	24251.865942	30.508992
448.268259	24287.554538	30.514010
448.238771	24336.350960	30.519028
448.647632	24364.833381	30.524045
448.820725	24405.666681	30.529063
449.273582	24460.881904	30.534080
449.873055	24495.717667	30.539098
450.240480	24551.289469	30.544116
450.509973	24577.068905	30.549133
450.605981	24618.997166	30.554151
451.101132	24657.631780	30.559168
451.858243	24699.066284	30.564186
452.098132	24743.566593	30.569204
452.784580	24777.005659	30.574221
453.300674	24823.444248	30.579239
453.803614	24863.676989	30.584256
454.491930	24895.253693	30.589274
454.361149	24952.812389	30.594292
454.979875	24982.095350	30.599309
455.778227	25022.908847	30.604327
456.084234	25057.447322	30.609344
456.658698	25104.077301	30.614362
456.676673	25152.043502	30.619380
456.840731	25201.162079	30.624397
457.259479	25240.520243	30.629415
457.395020	25294.596865	30.634432
458.262789	25343.093421	30.639450
458.646779	25401.650365	30.644468
459.079684	25452.078254	30.649485
459.420771	25501.371875	30.654503
459.765861	25571.378045	30.659520
460.546808	25622.345029	30.664538
460.558383	25678.734641	30.669556
461.381505	25719.678180	30.674573
461.900235	25788.306686	30.679591
462.399035	25836.132305	30.684608
463.215728	25875.992331	30.689626
463.433421	25938.533614	30.694644
464.087974	25983.397597	30.699661
464.777883	26028.249550	30.704679
465.195088	26099.942801	30.709696
466.059255	26134.518993	30.714714
466.109368	26182.886485	30.719732
466.853167	26228.026536	30.724749
467.486748	26261.016764	30.729767
467.580874	26313.468096	30.734784
467.934122	26344.047814	30.739802
468.827806	26396.086621	30.744820
469.632871	26424.926527	30.749837
470.207200	26477.895155	30.754855
470.538038	26519.805059	30.759872
471.070862	26555.969704	30.764890
471.593347	26605.572450	30.769908
471.807339	26651.744197	30.774925
472.349845	26691.736576	30.779943
472.799757	26723.789732	30.784960
473.161637	26763.622869	30.789978
473.495491	26818.187238	30.794996
474.463475	26850.148748	30.800013
475.365434	26882.054987	30.805031
475.572701	26920.254961	30.810048
475.864730	26960.093783	30.815066
476.323710	26995.319005	30.820084
476.831294	27031.182870	30.825101
477.220202	27074.074938	30.830119
477.319230	27114.327650	30.835136
477.761520	27162.734055	30.840154
477.933901	27199.918462	30.845172
478.395593	27260.055471	30.850189
479.371008	27299.611874	30.855207
479.311286	27346.079878	30.860224
480.111344	27395.020832	30.865242
480.759373	27441.271253	30.870260
481.482801	27459.679616	30.875277
481.932183	27506.284755	30.880295
482.270704	27551.577243	30.885312
482.659780	27579.569922	30.890330
482.983309	27618.569192	30.895348
483.326208	27670.302252	30.900365
484.192792	27698.500134	30.905383
484.001379	27745.561889	30.910400
484.695193	27788.458996	30.915418
484.979365	27835.767331	30.920436
485.249853	27887.232270	30.925453
485.932917	27921.558097	30.930471
486.339768	27981.933794	30.935488
486.860263	28032.717545	30.940506
487.420194	28088.153887	30.945524
487.477961	28136.418355	30.950541
488.410313	28182.327294	30.955559
488.633631	28240.232806	30.960576
488.936871	28299.790821	30.965594
489.433144	28353.175567	30.970612
489.842484	28402.461505	30.975629
490.632142	28460.230047	30.980647
490.899068	28525.715657	30.985664
491.556642	28576.702328	30.990682
492.354149	28624.186693	30.995700
493.081205	28689.467589	31.000717
493.639592	28738.351332	31.005735
493.732080	28782.157773	31.010752
494.546902	28833.075064	31.015770
495.199379	28881.924744	31.020788
495.894955	28930.836842	31.025805
496.652914	28955.698349	31.030823
497.025320	29004.222404	31.035840
497.914777	29031.674230	31.040858
498.288587	29084.772318	31.045876
498.456587	29123.532538	31.050893
499.072928	29169.767588	31.055911
499.367821	29219.368127	31.060928
499.993347	29249.460082	31.065946
500.341640	29317.313772	31.070964
500.841468	29360.268905	31.075981
501.059606	29405.008843	31.080999
501.453435	29469.874532	31.086016
502.038341	29511.465822	31.091034
502.312179	29568.745970	31.096052
502.979518	29634.664900	31.101069
503.734940	29680.319970	31.106087
504.051234	29742.786194	31.111104
504.333870	29791.204245	31.116122
505.065134	29843.182492	31.121140
505.875072	29885.649204	31.126157
506.562193	29938.199712	31.131175
507.153907	29979.071731	31.136192
507.428622	30015.585953	31.141210
508.298870	30048.957605	31.146228
508.560095	30111.655077	31.151245
509.165644	30160.273194	31.156263
509.695058	30192.562567	31.161280
509.843864	30253.730151	31.166298
510.288231	30303.280697	31.171316
510.678967	30351.187154	31.176333
511.385406	30404.792720	31.181351
511.666897	30461.664420	31.186368
512.485541	30511.718441	31.191386
513.077865	30557.440610	31.196404
513.571151	30613.239897	31.201421
514.325984	30644.243576	31.206439
514.259845	30706.483022	31.211456
514.903725	30746.802443	31.216474
515.691166	30800.474717	31.221492
515.704017	30856.231095	31.226509
516.533790	30882.121445	31.231527
516.852770	30929.400907	31.236544
517.811503	30971.321985	31.241562
518.457646	31015.250813	31.246580
518.486305	31062.682699	31.251597
519.048498	31103.391867	31.256615
519.588587	31156.229030	31.261632
520.248433	31197.584816	31.266650
521.005951	31241.148776	31.271668
520.819695	31284.805631	31.276685
521.534446	31332.585543	31.281703
522.004304	31373.222252	31.286720
522.330532	31440.788123	31.291738
522.874136	31480.027878	31.296756
523.297965	31537.157198	31.301773
523.603205	31586.781686	31.306791
523.989157	31659.209808	31.311808
524.335339	31707.711010	31.316826
524.951059	31773.861081	31.321844
525.311158	31850.070801	31.326861
526.157233	31906.506887	31.331879
526.802771	31960.654169	31.336896
527.315218	32024.803019	31.341914
528.371091	32081.640413	31.346932
528.990335	32129.719072	31.351949
529.391883	32195.123647	31.356967
529.637114	32249.587190	31.361984
530.396165	32301.423023	31.367002
530.980282	32372.442575	31.372020
531.307617	32415.402157	31.377037
532.026697	32472.643508	31.382055
532.246381	32533.930385	31.387072
532.831233	32597.469886	31.392090
534.044974	32632.348387	31.397108
534.523545	32707.040393	31.402125
535.001871	32739.693128	31.407143
535.688456	32794.530337	31.412160
536.236603	32840.991451	31.417178
536.758223	32903.409784	31.422196
537.355786	32966.532029	31.427213
537.842427	33007.646182	31.432231
538.302908	33064.162292	31.437248
538.132527	33118.501538	31.442266
538.979265	33174.361017	31.447284
539.413526	33234.570495	31.452301
539.589735	33288.076821	31.457319
540.311551	33355.584698	31.462336
540.840940	33414.545360	31.467354
542.489305	33460.422506	31.472372
542.829074	33509.456662	31.477389
543.807906	33558.164529	31.482407
544.424434	33609.816345	31.487424
544.835367	33647.031879	31.492442
545.936235	33689.936219	31.497460
546.043359	33730.761339	31.502477
546.400536	33780.064730	31.507495
546.936519	33824.921206	31.512512
547.040165	33867.350144	31.517530
547.653530	33916.958694	31.522548
548.054288	33978.056587	31.527565
548.961314	34011.063689	31.532583
549.483162	34064.912855	31.537600
549.852825	34123.854929	31.542618
550.417379	34176.630847	31.547636
551.194027	34217.270774	31.552653
551.980198	34266.930648	31.557671
552.220549	34317.684247	31.562688
552.723066	34360.332474	31.567706
553.383250	34401.550577	31.572724
553.768569	34442.369251	31.577741
554.221664	34482.242801	31.582759
554.621048	34527.110993	31.587776
555.085555	34579.838368	31.592794
555.998307	34613.322130	31.597812
556.545549	34668.759310	31.602829
557.169203	34699.167018	31.607847
557.572681	34746.136667	31.612864
558.174638	34805.598009	31.617882
558.876349	34844.374202	31.622900
558.572388	34897.904732	31.627917
559.220449	34956.731008	31.632935
559.617580	35017.631117	31.637952
560.382324	35075.261481	31.642970
560.618725	35124.048942	31.647988
561.023547	35196.904969	31.653005
561.684222	35260.876972	31.658023
562.209878	35329.276774	31.663040
562.682342	35386.890151	31.668058
563.547915	35451.415946	31.673076
563.963087	35516.098412	31.678093
564.414455	35580.484811	31.683111
565.401435	35639.541374	31.688128
565.648664	35705.426180	31.693146
566.510929	35766.378249	31.698164
566.880763	35841.874550	31.703181
567.921069	35893.362024	31.708199
569.035556	35943.947475	31.713216
569.656602	35997.681961	31.718234
570.243531	36049.683417	31.723252
570.922343	36097.561033	31.728269
571.311336	36152.019111	31.733287
571.801933	36210.272771	31.738304
572.281868	36269.052244	31.743322
572.789191	36317.757190	31.748340
573.194266	36374.333993	31.753357
573.618777	36437.030078	31.758375
574.162649	36490.494764	31.763392
574.449742	36551.509790	31.768410
574.960094	36628.652487	31.773428
575.598566	36693.980837	31.778445
576.258425	36764.550981	31.783463
577.213798	36823.282148	31.788480
577.415456	36890.939829	31.793498
578.276654	36949.301941	31.798516
578.551194	37023.607080	31.803533
579.280718	37074.136225	31.808551
579.859849	37137.052223	31.813568
580.079360	37211.319885	31.818586
581.177605	37276.280910	31.823604
581.693580	37333.934386	31.828621
582.122307	37400.489754	31.833639
582.757135	37472.023076	31.838656
583.577276	37545.107244	31.843674
584.005799	37596.347179	31.848692
584.319137	37659.577163	31.853709
584.967788	37730.440146	31.858727
585.752718	37793.886226	31.863744
585.866634	37868.814716	31.868762
586.626871	37944.640409	31.873780
587.030541	38006.913017	31.878797
587.111690	38084.117052	31.883815
588.073972	38150.350352	31.888832
588.442808	38238.292036	31.893850
589.264587	38305.909412	31.898868
589.699667	38386.480713	31.903885
590.312155	38457.141054	31.908903
590.998738	38530.705759	31.913920
591.192604	38607.650381	31.918938
592.119413	38663.545362	31.923956
592.742640	38742.035627	31.928973
593.383007	38809.713252	31.933991
594.456052	38880.778930	31.939008
594.784006	38945.188275	31.944026
595.609953	38995.697406	31.949044
596.317790	39043.638029	31.954061
597.035680	39105.382761	31.959079
597.854052	39164.674438	31.964096
598.566811	39229.418933	31.969114
599.510488	39280.083010	31.974132
600.217562	39333.832172	31.979149
600.678291	39386.438549	31.984167
601.466803	39443.305681	31.989184
601.705954	39493.294467	31.994202
602.003844	39541.386177	31.999220
602.435685	39610.174393	32.004237
602.983718	39675.837785	32.009255
603.416069	39723.917239	32.014272
603.815411	39804.305036	32.019290
604.659684	39872.584228	32.024308
605.091097	39937.885896	32.029325
606.190420	39998.453285	32.034343
607.104527	40060.011030	32.039360
607.469259	40120.586515	32.044378
608.100313	40190.186797	32.049396
608.832709	40246.948918	32.054413
609.059729	40315.338026	32.059431
609.729058	40378.165153	32.064448
610.239102	40449.263660	32.069466
610.957260	40515.646918	32.074484
611.133554	40595.172264	32.079501
611.839674	40665.285947	32.084519
612.319252	40740.279507	32.089536
612.751381	40831.171510	32.094554
613.103228	40903.475318	32.099572
613.992705	40983.430655	32.104589
614.256589	41066.014971	32.109607
614.951343	41149.065128	32.114624
615.259051	41249.168764	32.119642
615.924036	41322.129599	32.124660
616.500737	41410.004903	32.129677
617.330727	41494.770472	32.134695
618.417042	41564.493350	32.139712
619.146182	41642.536657	32.144730
619.430297	41724.956443	32.149748
620.277006	41812.173511	32.154765
620.874754	41886.214678	32.159783
621.769539	41961.706561	32.164800
622.294834	42051.563258	32.169818
622.480217	42125.319928	32.174836
623.756940	42204.310619	32.179853
624.013220	42279.299987	32.184871
625.024861	42355.023575	32.189888
625.877577	42441.803831	32.194906
627.703423	42471.097951	32.199924
628.728962	42522.448855	32.204941
629.247343	42575.910388	32.209959
629.929812	42624.230792	32.214976
630.119648	42676.098972	32.219994
630.664451	42725.114798	32.225012
631.415860	42777.963871	32.230029
631.730783	42842.941537	32.235047
632.355433	42898.788887	32.240064
632.803288	42958.128789	32.245082
633.061628	43006.409745	32.250100
633.735083	43067.616393	32.255117
633.988615	43142.489754	32.260135
634.659246	43192.824605	32.265152
635.310584	43259.629746	32.270170
635.507263	43329.701967	32.275188
636.012734	43399.887621	32.280205
636.493236	43477.114725	32.285223
636.922473	43564.045957	32.290240
637.407579	43626.482085	32.295258
637.808909	43714.056357	32.300276
638.246648	43791.942193	32.305293
638.543057	43893.132282	32.310311
640.144171	43960.626043	32.315328
641.116961	44033.944561	32.320346
641.744364	44107.538254	32.325364
643.003545	44176.014317	32.330381
643.552351	44249.990943	32.335399
643.973848	44315.492885	32.340416
644.903245	44394.439795	32.345434
645.513996	44465.044623	32.350452
646.337487	44531.178679	32.355469
646.674031	44616.425236	32.360487
647.613122	44685.495927	32.365504
648.092597	44754.443874	32.370522
648.425273	44831.514736	32.375540
649.538659	44902.202388	32.380557
650.028005	44978.862796	32.385575
650.507338	45047.240375	32.390592
651.184863	45133.515939	32.395610
651.574357	45207.169051	32.400628
652.594529	45299.924494	32.405645
653.068689	45380.459977	32.410663
653.733515	45451.208002	32.415680
654.607046	45522.815369	32.420698
655.507361	45601.083875	32.425716
656.069713	45669.926789	32.430733
656.104133	45746.210802	32.435751
656.925223	45824.846960	32.440768
657.806125	45905.421722	32.445786
658.344023	45991.383293	32.450804
659.178342	46066.750296	32.455821
659.693353	46151.491275	32.460839
660.437809	46237.754556	32.465856
660.998803	46304.853918	32.470874
661.459599	46394.988532	32.475892
662.487635	46464.600518	32.480909
663.226603	46543.401654	32.485927
663.824578	46620.395008	32.490944
664.715379	46699.916914	32.495962
665.102173	46778.515115	32.500980
665.831034	46860.202142	32.505997
666.437519	46933.412543	32.511015
667.246453	47010.925240	32.516032
667.361962	47086.759224	32.521050
667.919803	47199.850476	32.526068
669.065051	47276.740343	32.531085
669.282392	47371.122716	32.536103
670.020433	47461.753453	32.541120
670.557737	47535.277597	32.546138
671.301445	47624.354574	32.551156
672.233326	47717.190209	32.556173
673.428388	47784.884833	32.561191
674.260283	47848.730337	32.566208
675.195984	47937.082368	32.571226
675.574300	48022.185894	32.576244
676.482144	48089.556420	32.581261
676.560940	48177.141631	32.586279
677.158121	48242.653513	32.591296
678.248540	48309.356783	32.596314
678.162550	48388.068171	32.601332
678.524068	48460.014419	32.606349
679.341733	48547.858264	32.611367
680.098007	48613.013571	32.616384
680.837677	48710.515314	32.621402
680.970681	48801.839753	32.626420
681.539241	48880.258763	32.631437
682.001435	48981.625687	32.636455
682.636811	49081.868729	32.641472
683.253380	49156.826108	32.646490
684.040726	49261.598837	32.651508
684.973699	49358.487742	32.656525
685.445840	49461.399853	32.661543
686.286925	49560.581915	32.666560
687.205893	49643.916998	32.671578
687.769510	49751.091608	32.676596
689.279271	49823.061810	32.681613
689.991396	49910.973584	32.686631
690.583488	49994.013625	32.691648
691.738354	50078.139079	32.696666
692.594841	50161.540428	32.701684
693.241088	50220.005135	32.706701
694.265865	50304.936299	32.711719
695.200687	50367.516298	32.716736
696.194262	50424.563088	32.721754
696.659052	50518.399087	32.726772
697.348211	50574.122766	32.731789
697.533002	50663.628401	32.736807
698.249460	50751.420145	32.741824
698.932607	50816.424505	32.746842
699.446818	50906.584323	32.751860
699.684328	50985.493006	32.756877
700.472179	51066.809356	32.761895
701.251411	51158.158331	32.766912
702.140008	51228.587754	32.771930
702.652008	51324.829710	32.776948
703.419596	51409.574516	32.781965
703.975823	51493.884000	32.786983
704.436207	51610.077966	32.792000
705.096370	51684.567431	32.797018
705.561198	51794.034341	32.802036
706.202646	51886.353894	32.807053
707.142344	51972.146623	32.812071
707.823525	52076.266867	32.817088
708.524536	52167.267156	32.822106
708.723478	52277.181839	32.827124
709.482734	52400.302040	32.832141
710.051076	52487.680796	32.837159
710.807748	52592.697855	32.842176
711.497218	52695.300788	32.847194
711.971089	52813.448596	32.852212
712.503740	52924.429982	32.857229
713.534539	53030.130621	32.862247
714.608482	53155.079876	32.867264
715.306992	53252.156610	32.872282
715.811704	53373.562480	32.877300
716.615679	53478.311186	32.882317
717.657458	53579.552902	32.887335
718.480705	53683.054989	32.892352
719.404588	53760.999294	32.897370
720.196834	53871.576797	32.902388
720.851377	53958.202458	32.907405
721.564709	54064.795064	32.912423
722.146171	54170.045418	32.917440
723.127007	54261.350455	32.922458
723.741727	54367.784104	32.927476
724.394261	54460.350968	32.932493
725.356385	54545.386912	32.937511
725.716873	54635.362007	32.942528
726.728728	54716.903062	32.947546
727.541883	54798.894248	32.952564
728.337341	54896.051599	32.957581
729.357803	54969.366411	32.962599
729.840453	55065.047324	32.967616
730.520466	55152.103685	32.972634
730.855911	55232.147506	32.977652
731.588901	55333.297669	32.982669
732.578181	55433.616274	32.987687
732.693009	55509.148659	32.992704
733.721946	55598.885106	32.997722
734.298649	55716.370079	33.002740
734.766301	55822.987543	33.007757
735.617829	55914.599634	33.012775
736.283616	56028.678882	33.017792
737.480942	56137.294162	33.022810
738.066167	56227.201520	33.027828
738.792665	56333.134530	33.032845
739.680545	56437.240722	33.037863
740.492279	56544.165410	33.042880
741.377830	56646.225925	33.047898
742.177763	56747.574482	33.052916
742.837377	56845.029258	33.057933
744.103639	56913.300152	33.062951
744.458022	57012.600618	33.067968
745.572558	57104.010513	33.072986
746.067753	57209.190269	33.078004
746.554529	57323.616161	33.083021
748.195703	57391.510863	33.088039
749.220116	57471.178283	33.093056
750.164454	57557.057918	33.098074
750.969899	57647.093327	33.103092
751.828502	57721.898418	33.108109
752.469450	57795.008381	33.113127
753.295011	57888.592730	33.118144
754.313878	57973.362381	33.123162
754.654079	58061.776722	33.128180
755.169617	58156.620434	33.133197
755.982433	58225.627896	33.138215
756.120141	58320.022943	33.143232
756.820205	58417.921084	33.148250
757.575596	58518.382415	33.153268
758.336236	58608.979328	33.158285
759.386272	58701.026488	33.163303
759.774348	58809.537270	33.168320
760.816818	58894.060493	33.173338
761.606719	58990.809160	33.178356
761.942258	59089.029870	33.183373
762.861618	59191.319036	33.188391
763.258348	59299.508763	33.193408
764.145426	59395.630368	33.198426
764.648871	59503.740381	33.203444
765.396027	59613.706545	33.208461
766.180932	59716.304964	33.213479
766.684985	59821.907783	33.218496
767.457802	59938.999823	33.223514
768.239429	60050.416165	33.228532
768.835189	60164.473791	33.233549
769.896780	60279.049180	33.238567
770.655029	60395.084589	33.243584
771.273393	60496.469521	33.248602
772.219090	60610.844746	33.253620
772.893935	60736.053122	33.258637
774.670585	60800.006180	33.263655
775.537129	60913.290235	33.268672
776.603751	60989.653129	33.273690
777.302748	61088.518755	33.278708
778.287409	61176.334802	33.283725
778.806187	61256.656929	33.288743
779.292621	61332.649252	33.293760
780.024650	61426.682661	33.298778
780.742148	61511.276867	33.303796
781.348547	61607.379530	33.308813
782.078781	61684.344114	33.313831
782.195832	61796.353828	33.318848
783.178676	61912.683178	33.323866
783.610812	62014.112783	33.328884
783.846438	62113.198964	33.333901
784.998890	62234.962770	33.338919
785.806886	62352.884600	33.343936
786.510366	62457.324280	33.348954
787.314540	62571.626496	33.353972
788.000221	62684.678531	33.358989
789.217767	62798.901122	33.364007
789.805096	62925.388884	33.369024
790.773911	63029.673913	33.374042
791.860596	63143.199509	33.379060
792.565063	63261.042556	33.384077
793.454273	63357.555533	33.389095
793.785513	63485.732388	33.394112
794.592091	63597.890950	33.399130
795.152712	63726.069355	33.404148
795.563218	63861.447340	33.409165
796.526185	63974.011942	33.414183
797.109497	64119.571079	33.419200
797.785793	64253.624641	33.424218
798.592598	64372.342085	33.429236
799.106379	64523.439989	33.434253
800.029831	64652.468144	33.439271
800.770454	64790.661116	33.444288
801.656316	64938.325215	33.449306
802.838789	65062.894768	33.454324
803.828131	65208.565218	33.459341
804.737249	65336.196728	33.464359
805.229195	65468.822119	33.469376
806.167840	65606.994173	33.474394
807.900134	65721.647392	33.479412
809.122145	65825.999610	33.484429
810.331448	65932.528990	33.489447
811.092403	66059.803825	33.494464
812.160297	66166.888755	33.499482
813.115909	66264.087089	33.504500
813.736326	66380.849271	33.509517
814.309639	66482.410352	33.514535
814.970498	66604.357061	33.519552
815.879559	66715.725440	33.524570
816.737100	66824.656462	33.529588
817.361655	66931.660495	33.534605
818.682829	67048.658399	33.539623
819.184809	67151.460924	33.544640
819.633365	67263.647908	33.549658
820.700927	67384.267674	33.554676
821.523261	67494.029834	33.559693
822.254282	67601.095578	33.564711
822.943637	67728.006788	33.569728
823.483345	67840.124915	33.574746
824.250327	67962.049381	33.579764
824.669556	68095.373620	33.584781
825.807410	68223.288508	33.589799
826.374518	68347.264942	33.594816
826.996902	68485.419776	33.599834
828.122454	68598.134323	33.604852
828.758923	68726.621869	33.609869
829.972825	68859.174870	33.614887
830.246817	68971.355548	33.619904
830.923948	69096.241273	33.624922
831.917415	69210.713215	33.629940
832.493031	69327.429665	33.634957
833.527304	69461.407030	33.639975
834.407253	69583.992409	33.644992
835.325268	69712.654430	33.650010
836.743579	69821.868785	33.655028
837.820586	69929.167430	33.660045
838.705950	70038.154775	33.665063
839.163206	70162.501425	33.670080
839.942334	70278.133636	33.675098
840.824830	70403.309295	33.680116
841.425939	70533.059218	33.685133
842.465838	70646.146579	33.690151
843.303826	70773.437243	33.695168
843.642366	70907.848440	33.700186
844.596315	71022.735031	33.705204
845.150346	71162.967225	33.710221
846.142413	71291.051192	33.715239
847.117386	71435.300289	33.720256
847.587490	71566.266851	33.725274
848.505128	71695.307661	33.730292
849.486839	71837.680411	33.735309
850.504074	71977.525308	33.740327
851.470646	72101.634761	33.745344
852.474801	72239.750978	33.750362
854.144365	72350.233077	33.755380
854.889372	72480.938523	33.760397
856.059428	72600.363321	33.765415
856.690833	72722.976171	33.770432
857.620329	72846.760915	33.775450
858.359180	72962.534442	33.780468
859.078531	73096.675165	33.785485
859.556166	73211.342287	33.790503
860.741270	73341.417498	33.795520
861.173702	73491.505444	33.800538
862.147005	73600.730390	33.805556
862.536505	73757.713694	33.810573
863.134866	73903.913343	33.815591
864.119626	74048.209968	33.820608
864.703854	74188.671907	33.825626
865.833780	74330.669878	33.830644
866.778730	74480.983596	33.835661
867.600171	74615.186434	33.840679
868.711070	74766.872314	33.845696
869.516692	74913.714880	33.850714
870.260725	75061.042908	33.855732
870.965300	75214.949174	33.860749
871.918663	75347.294432	33.865767
872.987579	75509.749758	33.870784
873.316244	75644.223697	33.875802
874.956448	75774.775898	33.880820
875.939077	75924.821406	33.885837
876.888834	76052.453607	33.890855
877.940069	76205.639229	33.895872
878.647782	76340.946595	33.900890
880.041789	76470.670829	33.905908
880.640575	76610.273170	33.910925
881.614517	76745.254467	33.915943
882.394517	76882.450592	33.920960
883.384566	77025.007782	33.925978
884.501878	77154.535077	33.930996
885.423796	77289.914107	33.936013
886.294353	77409.952346	33.941031
887.498157	77540.150697	33.946048
888.598741	77659.911974	33.951066
889.386723	77777.720545	33.956084
890.350507	77904.210049	33.961101
890.821420	78014.045982	33.966119
891.807793	78116.871559	33.971136
892.335897	78252.093806	33.976154
893.397894	78359.575844	33.981172
894.097372	78494.214672	33.986189
895.158952	78611.299396	33.991207
896.576862	78729.173468	33.996224
896.719948	78858.043000	34.001242
898.482437	78942.907392	34.006260
899.968879	79053.365110	34.011277
901.232044	79139.179246	34.016295
902.281504	79241.778234	34.021312
902.945876	79346.882831	34.026330
903.988097	79442.247827	34.031348
904.882323	79560.313972	34.036365
905.479155	79648.378050	34.041383
906.053303	79768.256590	34.046400
906.453498	79892.940190	34.051418
907.575756	80002.931406	34.056436
907.756798	80124.983137	34.061453
908.377019	80254.667513	34.066471
909.130964	80387.607201	34.071488
909.825142	80535.669415	34.076506
910.408761	80669.518153	34.081524
911.097332	80829.601957	34.086541
912.129706	80982.810993	34.091559
912.983035	81126.157121	34.096576
913.530348	81294.895908	34.101594
914.553611	81438.121073	34.106612
915.329976	81594.046042	34.111629
916.197144	81750.501126	34.116647
917.250256	81908.470132	34.121664
917.782368	82079.488312	34.126682
918.854768	82240.859860	34.131700
920.012529	82411.492570	34.136717
920.464031	82588.297324	34.141735
921.341079	82761.800488	34.146752
922.143194	82937.594806	34.151770
923.314242	83095.970133	34.156788
923.460921	83276.841445	34.161805
924.613287	83449.633791	34.166823
925.872636	83616.678001	34.171840
927.149247	83795.468918	34.176858
928.126196	83969.211497	34.181876
929.374951	84143.562157	34.186893
930.533089	84305.762941	34.191911
932.037165	84465.440343	34.196928
933.535219	84623.715312	34.201946
934.678388	84768.839637	34.206964
935.475635	84915.198780	34.211981
936.147669	85060.086385	34.216999
937.236222	85221.811623	34.222016
937.924357	85361.181397	34.227034
938.896279	85500.131866	34.232052
940.289180	85652.692690	34.237069
941.179646	85795.663390	34.242087
942.374325	85942.608786	34.247104
943.164843	86092.355167	34.252122
944.147273	86233.820181	34.257140
945.228749	86368.151580	34.262157
945.885487	86517.422940	34.267175
947.148010	86650.840265	34.272192
947.980582	86801.337221	34.277210
948.779677	86942.773543	34.282228
949.530818	87084.130057	34.287245
950.725075	87234.215756	34.292263
951.661050	87370.684003	34.297280
952.263133	87514.560763	34.302298
953.382539	87647.950474	34.307316
954.127831	87770.867255	34.312333
954.630694	87920.242590	34.317351
955.839239	88052.740348	34.322368
956.254814	88207.434515	34.327386
957.254676	88368.031952	34.332404
958.561356	88501.205764	34.337421
959.050401	88664.667464	34.342439
960.261794	88805.857124	34.347456
960.789209	88980.584634	34.352474
961.666559	89125.874905	34.357492
962.485944	89288.330863	34.362509
963.588225	89450.026161	34.367527
964.349388	89620.448372	34.372544
965.378491	89779.519186	34.377562
966.898548	89941.427303	34.382580
968.208700	90098.890798	34.387597
968.951073	90258.328572	34.392615
969.818204	90412.943631	34.397632
970.781093	90583.814074	34.402650
971.789264	90747.008249	34.407668
973.286961	90890.447612	34.412685
974.283663	91062.410721	34.417703
975.409421	91217.773032	34.422720
976.454150	91371.516960	34.427738
977.593847	91531.688715	34.432756
978.350204	91682.647036	34.437773
979.131485	91835.184363	34.442791
980.098528	91993.622006	34.447808
981.212457	92144.429265	34.452826
981.809877	92308.043646	34.457844
982.819831	92469.932870	34.462861
983.434177	92648.849935	34.467879
984.276082	92822.313180	34.472896
985.419690	92989.607731	34.477914
986.275557	93163.843259	34.482932
987.609265	93332.096123	34.487949
988.599844	93509.172638	34.492967
989.854037	93673.681504	34.497984
990.676797	93851.743929	34.503002
991.254904	94021.176967	34.508020
992.499634	94185.026285	34.513037
993.312236	94361.872565	34.518055
994.362849	94533.288194	34.523072
995.655902	94723.431777	34.528090
996.541792	94888.737542	34.533108
997.455651	95062.369461	34.538125
997.978785	95237.257076	34.543143
999.458560	95416.254163	34.548160
1000.842706	95602.306931	34.553178
1001.772172	95762.731226	34.558196
1003.250568	95935.877353	34.563213
1003.899723	96111.775807	34.568231
1005.378817	96285.816782	34.573248
1006.311516	96438.028811	34.578266
1007.123812	96607.466379	34.583284
1008.470787	96757.029372	34.588301
1009.281835	96942.610847	34.593319
1010.181820	97106.682170	34.598336
1011.294527	97280.328541	34.603354
1011.990658	97445.727100	34.608372
1013.349339	97607.529450	34.613389
1014.452834	97781.415061	34.618407
1015.265103	97949.367865	34.623424
1016.626859	98104.798365	34.628442
1019.103178	98222.627202	34.633460
1020.525161	98349.714732	34.638477
1021.627036	98490.947226	34.643495
1022.863071	98596.866207	34.648512
1023.861540	98724.614293	34.653530
1024.452679	98853.246910	34.658548
1025.707180	98959.373284	34.663565
1026.086153	99087.497705	34.668583
1026.952950	99225.557231	34.673600
1027.716335	99356.196108	34.678618
1028.284152	99501.795633	34.683636
1029.173885	99653.591250	34.688653
1029.654633	99802.998976	34.693671
1030.693391	99950.872051	34.698688
1031.122472	100121.466622	34.703706
1031.510337	100291.967854	34.708724
1032.516835	100461.228543	34.713741
1033.201277	100646.421531	34.718759
1034.015023	100838.375015	34.723776
1034.594478	101021.891368	34.728794
1035.697807	101222.030291	34.733812
1036.613734	101414.192840	34.738829
1037.666141	101626.727050	34.743847
1038.978617	101832.825546	34.748864
1039.799404	102021.203299	34.753882
1040.931066	102225.188503	34.758900
1042.118139	102430.014589	34.763917
1042.926143	102636.829647	34.768935
1044.349636	102834.927609	34.773952
1045.614319	103050.825936	34.778970
1046.341815	103240.798261	34.783988
1047.334501	103448.266831	34.789005
1048.458957	103666.941396	34.794023
1049.934535	103857.877482	34.799040
1051.041551	104067.814190	34.804058
1051.935968	104275.444915	34.809076
1053.508832	104479.812020	34.814093
1054.710144	104683.703855	34.819111
1055.565501	104875.680616	34.824128
1056.986819	105084.623855	34.829146
1057.967630	105287.163767	34.834164
1059.379829	105481.642883	34.839181
1060.133513	105672.686137	34.844199
1061.315244	105862.494992	34.849216
1062.776577	106055.374539	34.854234
1063.235246	106257.463575	34.859252
1064.823963	106452.237367	34.864269
1065.910316	106646.943556	34.869287
1066.650619	106848.078763	34.874304
1067.747995	107044.343850	34.879322
1068.805260	107241.718880	34.884340
1070.072096	107433.728737	34.889357
1071.713253	107635.721770	34.894375
1072.814320	107820.694562	34.899392
1073.947432	108002.408326	34.904410
1075.024386	108194.341043	34.909428
1076.026027	108384.235741	34.914445
1076.985462	108570.567020	34.919463
1078.034312	108764.636325	34.924480
1079.146949	108949.754370	34.929498
1079.954418	109159.800120	34.934516
1080.799615	109353.172683	34.939533
1081.609619	109553.632854	34.944551
1082.524385	109753.139920	34.949568
1083.691458	109969.123794	34.954586
1084.283050	110178.592486	34.959604
1085.607572	110380.379854	34.964621
1086.708929	110593.402922	34.969639
1087.581887	110810.544078	34.974656
1088.762507	111005.266458	34.979674
1089.418883	111221.585308	34.984692
1090.723716	111392.311367	34.989709
1091.921342	111613.154794	34.994727
1093.086995	111806.605999	34.999744
1094.321757	112007.698246	35.004762
1095.306510	112198.749961	35.009780
1096.854537	112380.019370	35.014797
1098.444944	112570.074304	35.019815
1099.703172	112772.967101	35.024832
1101.384951	112934.405817	35.029850
1102.482024	113120.821677	35.034868
1103.409510	113300.147408	35.039885
1104.767997	113485.787844	35.044903
1105.941303	113672.283527	35.049920
1107.148905	113845.878579	35.054938
1107.570359	114038.834945	35.059956
1108.821731	114218.151171	35.064973
1109.828991	114409.822588	35.069991
1110.482459	114609.585586	35.075008
1111.891471	114800.395258	35.080026
1112.579811	114996.468704	35.085044
1113.807211	115194.088817	35.090061
1114.639725	115407.636981	35.095079
1116.115130	115597.300941	35.100096
1117.072313	115787.305113	35.105114
1118.082899	116029.726805	35.110132
1119.226627	116225.835038	35.115149
1120.393073	116430.910800	35.120167
1120.946498	116634.606921	35.125184
1122.455804	116849.029866	35.130202
1123.142734	117067.010997	35.135220
1124.502288	117280.929813	35.140237
1125.530907	117504.115849	35.145255
1126.085137	117731.436332	35.150272
1127.366423	117953.228503	35.155290
1128.184240	118187.414291	35.160308
1129.139680	118416.042382	35.165325
1130.404187	118651.615319	35.170343
1131.562241	118901.081927	35.175360
1132.741448	119130.198272	35.180378
1133.762421	119370.986912	35.185396
1134.970090	119608.388992	35.190413
1136.305537	119849.725250	35.195431
1137.374734	120092.881416	35.200448
1138.673076	120323.723508	35.205466
1139.579728	120571.003284	35.210484
1140.645957	120805.410120	35.215501
1141.950144	121045.050870	35.220519
1142.739108	121293.800758	35.225536
1144.367443	121530.566246	35.230554
1145.323314	121777.125852	35.235572
1146.511115	122021.254274	35.240589
1148.506903	122248.486388	35.245607
1149.815585	122483.829731	35.250624
1151.348462	122717.275146	35.255642
1152.686580	122934.952294	35.260660
1153.892699	123158.786237	35.265677
1155.104015	123390.287829	35.270695
1155.904853	123609.161127	35.275712
1157.143780	123827.672255	35.280730
1158.457034	124061.494015	35.285748
1159.126022	124271.573754	35.290765
1160.231832	124509.957463	35.295783
1161.346979	124758.543295	35.300800
1162.566388	124969.398847	35.305818
1163.731506	125210.819890	35.310836
1164.711719	125441.361693	35.315853
1165.874291	125668.896916	35.320871
1166.629476	125894.283245	35.325888
1168.089807	126112.406966	35.330906
1168.958966	126351.161180	35.335924
1170.258131	126575.600984	35.340941
1171.264357	126790.496695	35.345959
1172.568149	127020.287389	35.350976
1173.484709	127232.095903	35.355994
1174.301094	127479.777542	35.361012
1175.267630	127711.948484	35.366029
1176.566773	127951.721582	35.371047
1177.889062	128200.314142	35.376064
1178.866404	128436.646003	35.381082
1180.142350	128697.848725	35.386100
1180.996540	128928.982738	35.391117
1182.280016	129170.162138	35.396135
1183.258898	129432.548166	35.401152
1185.082043	129679.396875	35.406170
1186.571307	129928.267306	35.411188
1187.928157	130165.791892	35.416205
1189.061565	130412.354660	35.421223
1190.280504	130658.398238	35.426240
1191.612763	130887.439825	35.431258
1192.873774	131137.346258	35.436276
1193.844340	131387.150511	35.441293
1195.027450	131637.745591	35.446311
1196.321471	131886.042687	35.451328
1197.501141	132137.719758	35.456346
1198.561402	132383.942448	35.461364
1199.755972	132641.097146	35.466381
1201.347999	132892.395232	35.471399
1202.252430	133141.134069	35.476416
1203.578429	133380.475331	35.481434
1205.140954	133626.257100	35.486452
1206.680112	133870.155781	35.491469
1208.674967	134089.172571	35.496487
1210.305729	134314.120355	35.501504
1211.671496	134532.394649	35.506522
1213.065134	134762.430142	35.511540
1214.528015	134979.816713	35.516557
1216.228506	135187.454757	35.521575
1217.251242	135410.038469	35.526592
1218.491277	135609.920630	35.531610
1219.551050	135840.792201	35.536628
1220.456253	136049.150181	35.541645
1221.595188	136269.489331	35.546663
1222.171768	136489.872074	35.551680
1223.654792	136717.561247	35.556698
1224.668867	136939.738440	35.561716
1225.177550	137181.017564	35.566733
1226.577516	137417.523832	35.571751
1227.265380	137660.881452	35.576768
1228.249433	137901.681670	35.581786
1229.582383	138169.304226	35.586804
1230.483727	138414.204253	35.591821
1231.854243	138677.475975	35.596839
1232.663689	138928.861027	35.601856
1234.279228	139197.472163	35.606874
1235.437335	139451.884536	35.611892
1236.655010	139703.030506	35.616909
1238.132757	139963.454538	35.621927
1239.213944	140219.939419	35.626944
1240.311906	140483.536541	35.631962
1241.528700	140746.012995	35.636980
1242.483248	141003.488337	35.641997
1243.488876	141269.274983	35.647015
1244.330259	141546.705374	35.652032
1245.873134	141819.901308	35.657050
1246.905388	142097.444134	35.662068
1248.228725	142365.012745	35.667085
1249.353846	142618.008725	35.672103
1250.091504	142894.237148	35.677120
1252.026583	143154.115494	35.682138
1253.068161	143412.799148	35.687156
1254.437586	143686.558383	35.692173
1256.078618	143932.466518	35.697191
1257.252287	144193.860486	35.702208
1259.086367	144456.973430	35.707226
1260.272009	144711.800674	35.712244
1261.545194	144978.979204	35.717261
1262.928408	145231.812064	35.722279
1263.509072	145506.375106	35.727296
1264.769756	145761.463851	35.732314
1266.796014	146023.187198	35.737332
1268.016457	146296.357267	35.742349
1269.508522	146555.940780	35.747367
1270.507152	146819.665723	35.752384
1272.000482	147092.112034	35.757402
1273.354006	147355.642847	35.762420
1274.472951	147619.594764	35.767437
1276.129157	147873.783616	35.772455
1277.648918	148135.111397	35.777472
1278.922078	148379.982327	35.782490
1280.940552	148628.967752	35.787508
1282.188533	148880.872156	35.792525
1283.762233	149125.140478	35.797543
1284.843302	149385.243363	35.802560
1286.030995	149636.820501	35.807578
1287.342092	149884.409329	35.812596
1288.175370	150133.220131	35.817613
1289.474324	150393.471746	35.822631
1291.082498	150646.356123	35.827648
1292.147267	150910.416846	35.832666
1294.022130	151154.877219	35.837684
1294.972827	151418.440371	35.842701
1296.496739	151666.576727	35.847719
1297.415142	151929.425868	35.852736
1298.591604	152202.190749	35.857754
1300.266135	152438.334199	35.862772
1301.376135	152707.042303	35.867789
1302.315289	152970.389948	35.872807
1303.862382	153247.299515	35.877824
1304.753885	153493.459456	35.882842
1306.402333	153769.392127	35.887860
1307.078801	154050.548148	35.892877
1308.373120	154312.806370	35.897895
1309.727773	154597.761190	35.902912
1310.482894	154888.613806	35.907930
1312.070771	155152.744641	35.912948
1313.327458	155468.887674	35.917965
1314.529911	155738.540459	35.922983
1315.607935	156040.815316	35.928000
1316.807532	156330.692090	35.933018
1318.321121	156630.730527	35.938036
1319.299810	156922.183011	35.943053
1320.916773	157209.866324	35.948071
1322.279175	157507.310592	35.953088
1323.477030	157806.648989	35.958106
1324.740603	158096.819966	35.963124
1326.019683	158399.891609	35.968141
1327.556842	158691.937273	35.973159
1328.871969	158992.039041	35.978176
1330.506611	159276.664463	35.983194
1331.884209	159570.303200	35.988212
1333.208039	159867.860212	35.993229
1335.067811	160147.545171	35.998247
1337.455342	160410.247083	36.003264
1339.150227	160651.828359	36.008282
1340.895025	160887.211944	36.013300
1342.106222	161143.985273	36.018317
1343.379970	161377.165881	36.023335
1344.650447	161629.263872	36.028352
1345.734614	161869.709847	36.033370
1347.138064	162093.231332	36.038388
1347.988053	162362.263702	36.043405
1349.171418	162622.273246	36.048423
1350.713281	162879.205778	36.053440
1351.518131	163145.738664	36.058458
1352.616318	163406.541054	36.063476
1353.861381	163685.653671	36.068493
1354.821467	163954.322877	36.073511
1356.393210	164230.035772	36.078528
1357.399303	164512.618857	36.083546
1358.668442	164792.990860	36.088564
1359.612662	165091.764475	36.093581
1360.659949	165389.876101	36.098599
1362.292741	165683.718922	36.103616
1363.270287	166001.448790	36.108634
1364.780935	166297.181061	36.113652
1366.445452	166593.765429	36.118669
1368.732332	166882.547472	36.123687
1370.008001	167191.659754	36.128704
1371.281650	167490.865056	36.133722
1372.346884	167773.548564	36.138740
1373.879605	168082.155238	36.143757
1375.169576	168378.889656	36.148775
1376.290718	168678.229703	36.153792
1377.693214	169004.742487	36.158810
1379.425640	169289.647594	36.163828
1380.501907	169618.959477	36.168845
1381.825906	169938.462427	36.173863
1383.351025	170233.178208	36.178880
1384.610700	170555.513104	36.183898
1386.128243	170874.419725	36.188916
1387.008903	171194.131597	36.193933
1388.440269	171516.191180	36.198951
1390.066993	171839.286701	36.203968
1391.461921	172148.464260	36.208986
1393.484819	172464.735269	36.214004
1395.178276	172779.882665	36.219021
1396.818656	173075.270270	36.224039
1398.298341	173384.962366	36.229056
1399.079895	173700.799452	36.234074
1401.118858	173995.860602	36.239092
1402.770249	174317.801777	36.244109
1403.878692	174623.350171	36.249127
1405.276627	174930.832441	36.254144
1406.258872	175251.722871	36.259162
1407.556729	175559.428751	36.264180
1408.788448	175885.827983	36.269197
1410.256169	176206.149743	36.274215
1411.687275	176512.621420	36.279232
1412.995089	176845.169557	36.284250
1414.744111	177159.232698	36.289268
1416.125528	177477.000822	36.294285
1417.566946	177799.050670	36.299303
1419.471391	178116.165513	36.304320
1420.751381	178425.719958	36.309338
1421.971779	178739.068164	36.314356
1423.255438	179063.868193	36.319373
1424.890487	179359.980462	36.324391
1426.720075	179678.488270	36.329408
1428.087616	179988.037925	36.334426
1430.062679	180270.938256	36.339444
1431.577096	180575.060608	36.344461
1433.406808	180868.814300	36.349479
1435.163749	181123.071876	36.354496
1436.034093	181411.783330	36.359514
1437.471824	181693.790229	36.364532
1438.480565	181971.541459	36.369549
1439.768356	182256.076499	36.374567
1440.887422	182549.449337	36.379584
1442.287504	182858.185889	36.384602
1443.378883	183132.515426	36.389620
1444.367794	183437.896294	36.394637
1445.736739	183757.457204	36.399655
1446.821562	184079.935446	36.404672
1448.062369	184404.585725	36.409690
1449.128511	184725.167039	36.414708
1450.475341	185064.197377	36.419725
1451.659655	185399.994583	36.424743
1453.126916	185764.623703	36.429760
1454.066936	186109.071437	36.434778
1455.095794	186486.140753	36.439796
1456.434827	186837.800380	36.444813
1457.578039	187215.909342	36.449831
1459.102575	187582.241933	36.454848
1460.593450	187975.302267	36.459866
1462.672742	188328.588136	36.464884
1464.719522	188690.678278	36.469901
1466.864973	189048.159316	36.474919
1469.081491	189396.262836	36.479936
1470.546056	189750.509456	36.484954
1472.404337	190079.153035	36.489972
1474.495160	190429.504980	36.494989
1475.795955	190768.412376	36.500007
1477.142606	191111.972931	36.505024
1478.048870	191468.137396	36.510042
1479.667873	191799.089697	36.515060
1481.063508	192153.197209	36.520077
1482.517491	192512.527316	36.525095
1484.022714	192858.978842	36.530112
1484.841458	193230.554054	36.535130
1486.494174	193579.054588	36.540148
1488.148806	193937.915735	36.545165
1489.727798	194314.754684	36.550183
1491.056517	194655.621718	36.555200
1492.770256	195013.171795	36.560218
1494.880459	195359.575704	36.565236
1496.207237	195713.969098	36.570253
1497.721603	196068.219273	36.575271
1499.293975	196427.501884	36.580288
1500.447385	196788.175973	36.585306
1502.138476	197147.087571	36.590324
1503.923123	197501.059878	36.595341
1505.293710	197856.283132	36.600359
1506.706292	198213.202607	36.605376
1508.200331	198581.663675	36.610394
1509.635295	198944.029883	36.615412
1511.015539	199293.216119	36.620429
1512.368902	199654.672866	36.625447
1514.051990	200010.452834	36.630464
1515.052054	200401.655090	36.635482
1516.401561	200774.633786	36.640500
1518.069161	201158.290308	36.645517
1519.188060	201539.741488	36.650535
1520.575599	201913.811961	36.655552
1522.113574	202295.375886	36.660570
1523.302073	202687.524924	36.665588
1524.612994	203071.200043	36.670605
1526.206151	203480.833314	36.675623
1528.267512	203843.363173	36.680640
1529.951902	204237.914757	36.685658
1531.917369	204592.566823	36.690676
1533.544961	204941.651651	36.695693
1534.703376	205318.964646	36.700711
1536.643653	205664.623919	36.705728
1538.094089	206017.818792	36.710746
1539.441073	206388.884537	36.715764
1540.786777	206750.277071	36.720781
1541.846271	207126.713984	36.725799
1543.857854	207489.587302	36.730816
1545.135281	207874.334042	36.735834
1546.444675	208239.955100	36.740852
1548.064486	208625.652152	36.745869
1549.549071	209018.217382	36.750887
1551.320194	209397.239720	36.755904
1552.647430	209780.298770	36.760922
1554.443071	210162.279232	36.765940
1556.031090	210551.914423	36.770957
1557.458242	210939.267005	36.775975
1559.027700	211324.337700	36.780992
1560.831558	211723.288471	36.786010
1562.159593	212114.675445	36.791028
1564.750632	212470.478984	36.796045
1566.474147	212868.000843	36.801063
1568.024751	213250.416830	36.806080
1569.998885	213634.974120	36.811098
1571.493104	214024.793203	36.816116
1572.889391	214398.808016	36.821133
1574.247266	214784.818047	36.826151
1575.556781	215176.221876	36.831168
1577.163558	215565.267223	36.836186
1578.275537	215965.062683	36.841204
1580.260544	216342.442433	36.846221
1581.859388	216742.872058	36.851239
1583.899184	217139.573406	36.856256
1585.229005	217522.272514	36.861274
1586.736395	217907.889995	36.866292
1587.965709	218381.431286	36.871309
1589.215940	218795.768874	36.876327
1591.037087	219194.343434	36.881344
1592.382516	219614.510304	36.886362
1593.761754	220029.390528	36.891380
1595.373682	220453.352066	36.896397
1596.841756	220869.821162	36.901415
1598.244418	221299.052802	36.906432
1599.772365	221730.094239	36.911450
1601.200708	222151.451549	36.916468
1603.160486	222585.549260	36.921485
1604.360582	223014.668874	36.926503
1606.172091	223450.801031	36.931520
1607.985161	223887.976020	36.936538
1609.768605	224320.865135	36.941556
1611.484201	224743.556565	36.946573
1613.601162	225171.898210	36.951591
1615.610130	225581.514405	36.956608
1617.622538	225998.725951	36.961626
1618.892274	226421.370044	36.966644
1620.578102	226833.304456	36.971661
1622.509860	227245.733087	36.976679
1624.325436	227661.382668	36.981696
1625.813081	228069.569327	36.986714
1627.399072	228490.314147	36.991732
1629.200387	228893.066874	36.996749
1631.007944	229295.870625	37.001767
1632.737631	229686.064480	37.006784
1634.482695	230094.824670	37.011802
1635.960964	230489.532832	37.016820
1637.804698	230899.727003	37.021837
1639.148955	231301.622580	37.026855
1640.880838	231672.669661	37.031872
1642.698837	232058.283565	37.036890
1644.072884	232434.471826	37.041908
1645.560972	232821.209031	37.046925
1647.036037	233214.375851	37.051943
1648.426242	233596.584442	37.056960
1650.417205	233995.713634	37.061978
1651.172264	234386.995589	37.066996
1652.549321	234790.317701	37.072013
1654.230557	235207.688386	37.077031
1655.408233	235622.298273	37.082048
1656.728304	236049.637244	37.087066
1657.839748	236484.251161	37.092084
1659.579756	236928.719904	37.097101
1661.062102	237359.362994	37.102119
1662.421542	237803.033087	37.107136
1664.222311	238259.129134	37.112154
1665.367115	238715.740966	37.117172
1667.246915	239175.026852	37.122189
1668.665743	239656.591208	37.127207
1670.251679	240132.261307	37.132224
1672.235351	240590.720503	37.137242
1673.533812	241065.449533	37.142260
1675.654899	241533.185319	37.147277
1677.666113	242019.026650	37.152295
1679.435289	242477.449085	37.157312
1681.905792	242949.448609	37.162330
1683.487899	243411.891939	37.167348
1685.762276	243865.991554	37.172365
1687.446971	244338.606108	37.177383
1689.135296	244788.003016	37.182400
1690.972204	245266.284334	37.187418
1692.405272	245726.597257	37.192436
1694.613385	246190.237841	37.197453
1696.572895	246656.612878	37.202471
1697.766430	247103.148456	37.207488
1700.044818	247570.971066	37.212506
1702.015239	248027.845750	37.217524
1704.175568	248472.064515	37.222541
1705.849488	248919.996721	37.227559
1707.695046	249370.822514	37.232576
1709.345877	249810.910132	37.237594
1710.943075	250254.690535	37.242612
1713.283124	250692.963437	37.247629
1714.818014	251132.411157	37.252647
1716.531868	251583.667621	37.257664
1718.125961	252029.152381	37.262682
1720.188589	252455.736548	37.267700
1721.891268	252898.079590	37.272717
1723.750931	253338.796697	37.277735
1725.544718	253775.968567	37.282752
1727.503442	254222.690541	37.287770
1728.821411	254665.962081	37.292788
1730.466864	255102.346406	37.297805
1732.052786	255544.481933	37.302823
1733.655577	255991.898788	37.307840
1735.194359	256427.945761	37.312858
1736.546874	256897.454354	37.317876
1738.443732	257336.160772	37.322893
1740.378441	257787.257897	37.327911
1741.836350	258237.290666	37.332928
1744.204503	258677.088269	37.337946
1745.854075	259137.174727	37.342964
1747.647989	259575.009547	37.347981
1749.302763	260034.993646	37.352999
1750.465137	260490.460999	37.358016
1752.472883	260944.899772	37.363034
1754.117228	261390.405702	37.368052
1755.523546	261828.685509	37.373069
1757.340907	262258.234917	37.378087
1758.632475	262707.710956	37.383104
1760.372324	263142.709267	37.388122
1761.838815	263604.273573	37.393140
1763.679898	264042.328701	37.398157
1765.408672	264501.842539	37.403175
1766.948454	264967.484125	37.408192
1768.529716	265422.500077	37.413210
1769.479774	265908.865864	37.418228
1771.574885	266379.521082	37.423245
1772.893516	266864.402841	37.428263
1774.378735	267363.914372	37.433280
1776.300013	267850.423348	37.438298
1778.022522	268341.867488	37.443316
1779.478377	268858.275583	37.448333
1781.416318	269356.542024	37.453351
1782.954041	269866.025879	37.458368
1784.764795	270380.544695	37.463386
1786.361095	270913.134355	37.468404
1788.102337	271432.743883	37.473421
1790.547449	271954.319608	37.478439
1792.118286	272485.133016	37.483456
1794.226899	273009.658594	37.488474
1795.527603	273519.582992	37.493492
1797.249310	274070.106886	37.498509
1799.727600	274590.174152	37.503527
1801.708592	275132.702246	37.508544
1803.390216	275664.507970	37.513562
1805.025454	276206.303491	37.518580
1806.461201	276738.630260	37.523597
1808.614408	277283.157724	37.528615
1810.219500	277828.130018	37.533632
1812.421857	278368.658728	37.538650
1814.195284	278913.676907	37.543668
1816.380419	279456.644456	37.548685
1818.964798	279981.102834	37.553703
1820.745266	280511.890613	37.558720
1823.236563	281022.111146	37.563738
1825.244400	281554.331984	37.568756
1827.128437	282068.612669	37.573773
1829.314474	282586.576199	37.578791
1831.275278	283111.332286	37.583808
1833.071877	283626.537516	37.588826
1835.432972	284132.859179	37.593844
1837.957235	284619.263072	37.598861
1840.271120	285118.527986	37.603879
1842.058399	285604.542558	37.608896
1844.402168	286090.514682	37.613914
1845.870473	286578.458623	37.618932
1847.480869	287059.544705	37.623949
1849.261926	287549.669295	37.628967
1850.798890	288042.982273	37.633984
1852.815713	288522.904402	37.639002
1854.276001	289019.325653	37.644020
1855.692638	289519.054470	37.649037
1857.239563	290025.618179	37.654055
1858.608089	290528.881993	37.659072
1860.582442	291040.248339	37.664090
1861.897009	291565.056720	37.669108
1863.923273	292086.138778	37.674125
1865.535614	292606.804411	37.679143
1867.447808	293128.840847	37.684160
1869.181806	293652.047492	37.689178
1871.150802	294186.008053	37.694196
1872.941772	294719.792428	37.699213
1875.312306	295231.330406	37.704231
1877.001075	295760.097836	37.709248
1879.305302	296256.605787	37.714266
1881.164199	296746.708235	37.719284
1883.011426	297250.068805	37.724301
1885.163930	297730.238258	37.729319
1886.710596	298223.306575	37.734336
1888.729041	298719.495068	37.739354
1890.258613	299225.057795	37.744372
1891.868930	299722.553447	37.749389
1893.384054	300228.672478	37.754407
1895.162424	300755.876947	37.759424
1897.170356	301272.576779	37.764442
1899.000057	301803.399229	37.769460
1900.708762	302323.470092	37.774477
1902.939668	302853.103182	37.779495
1904.784117	303400.473819	37.784512
1906.701791	303928.070025	37.789530
1908.073882	304456.845344	37.794548
1909.967817	305007.373116	37.799565
1912.030727	305560.003057	37.804583
1913.601905	306109.256766	37.809600
1915.671163	306666.755054	37.814618
1917.547684	307217.754713	37.819636
1919.270429	307788.864771	37.824653
1921.374507	308354.778122	37.829671
1922.674013	308925.950420	37.834688
1924.507935	309502.135260	37.839706
1926.577486	310082.543716	37.844724
1928.351249	310667.669633	37.849741
1930.101369	311255.512537	37.854759
1931.667861	311859.177181	37.859776
1934.388691	312445.149747	37.864794
1936.104408	313037.860959	37.869812
1938.031372	313639.039967	37.874829
1940.425511	314226.297306	37.879847
1942.654103	314823.633480	37.884864
1944.890483	315418.297256	37.889882
1946.917760	316011.137020	37.894900
1949.005269	316599.899104	37.899917
1951.211426	317194.578885	37.904935
1952.913272	317788.803676	37.909952
1954.744528	318373.936905	37.914970
1956.769843	318975.919392	37.919988
1958.997039	319578.168096	37.925005
1961.085701	320160.552283	37.930023
1962.736782	320757.832617	37.935040
1964.990610	321352.976922	37.940058
1967.165083	321957.168424	37.945076
1968.765199	322541.770883	37.950093
1970.964413	323143.738405	37.955111
1972.719853	323752.045097	37.960128
1974.306601	324342.727396	37.965146
1976.118480	324949.464604	37.970164
1978.240854	325572.369078	37.975181
1980.735952	326152.017692	37.980199
1982.238866	326776.408761	37.985216
1983.939998	327387.634493	37.990234
1986.129217	327992.527870	37.995252
1988.113427	328610.854328	38.000269
1989.901389	329238.702108	38.005287
1991.883631	329853.943974	38.010304
1994.103977	330479.041478	38.015322
1996.101997	331092.845989	38.020340
1997.654962	331724.996398	38.025357
1999.967447	332337.644093	38.030375
2001.918583	332960.778818	38.035392
2004.018784	333591.853476	38.040410
2006.133990	334211.976983	38.045428
2007.617846	334826.333475	38.050445
2009.916292	335431.485996	38.055463
2011.982554	336045.123467	38.060480
2013.383457	336642.566362	38.065498
2015.443467	337240.833130	38.070516
2017.458583	337857.504464	38.075533
2019.939183	338464.293436	38.080551
2021.877708	339066.697169	38.085568
2023.404811	339683.782831	38.090586
2025.535414	340303.223762	38.095604
2027.636044	340910.072066	38.100621
2030.142233	341536.924072	38.105639
2031.712872	342148.337673	38.110656
2033.806421	342766.993014	38.115674
2035.889888	343382.621844	38.120692
2037.798652	344022.739646	38.125709
2040.148631	344647.268331	38.130727
2041.967074	345274.896957	38.135744
2043.859738	345908.596496	38.140762
2045.954153	346551.974988	38.145780
2047.609609	347193.589781	38.150797
2049.578492	347855.295501	38.155815
2051.270456	348520.362182	38.160832
2053.438312	349170.544964	38.165850
2055.645933	349831.903897	38.170868
2057.121825	350512.610518	38.175885
2059.309412	351178.318191	38.180903
2061.120375	351865.065172	38.185920
2062.781633	352560.632065	38.190938
2065.307585	353231.531685	38.195956
2067.203064	353931.301591	38.200973
2069.311285	354626.000788	38.205991
2071.361457	355330.188779	38.211008
2073.458545	356035.321738	38.216026
2075.371830	356743.239169	38.221044
2077.413488	357455.589423	38.226061
2079.589733	358161.079900	38.231079
2081.415736	358886.407293	38.236096
2083.862305	359597.969103	38.241114
2086.308463	360316.902001	38.246132
2088.304761	361029.984779	38.251149
2091.203051	361738.085686	38.256167
2093.643356	362440.262108	38.261184
2095.796435	363141.281141	38.266202
2098.584036	363825.844817	38.271220
2100.604362	364528.028182	38.276237
2102.609906	365222.032516	38.281255
2104.569183	365926.078106	38.286272
2106.927315	366620.836410	38.291290
2109.279241	367306.780530	38.296308
2111.190215	368006.407286	38.301325
2113.482445	368691.220092	38.306343
2115.404764	369399.291698	38.311360
2117.454320	370086.833246	38.316378
2120.084144	370770.157171	38.321396
2122.849151	371468.944155	38.326413
2125.068955	372138.765378	38.331431
2127.497007	372803.822239	38.336448
2129.425736	373495.200539	38.341466
2131.602643	374170.951708	38.346484
2133.871335	374841.171299	38.351501
2136.323797	375495.090833	38.356519
2138.601061	376150.523511	38.361536
2140.730420	376807.794376	38.366554
2143.183211	377477.781357	38.371572
2145.258877	378143.151342	38.376589
2147.359291	378797.117920	38.381607
2149.364741	379460.622806	38.386624
2151.057379	380120.311872	38.391642
2153.222019	380750.849716	38.396660
2154.900343	381401.311171	38.401677
2156.662905	382039.245004	38.406695
2158.408590	382692.637129	38.411712
2159.940953	383359.236898	38.416730
2162.053305	384013.277900	38.421748
2163.941067	384694.422409	38.426765
2165.957858	385372.818513	38.431783
2167.884827	386055.221269	38.436800
2169.642972	386747.956441	38.441818
2171.971413	387430.213235	38.446836
2174.014280	388135.573457	38.451853
2176.120366	388840.400595	38.456871
2178.348766	389540.755377	38.461888
2180.683427	390244.651545	38.466906
2183.667894	390938.538113	38.471924
2185.874705	391641.764782	38.476941
2187.855579	392350.741669	38.481959
2190.311431	393063.629006	38.486976
2192.624528	393769.096342	38.491994
2195.589948	394469.116829	38.497012
2197.764677	395182.178431	38.502029
2199.701420	395897.239432	38.507047
2201.702534	396606.468637	38.512064
2203.635241	397325.906318	38.517082
2206.062474	398039.517190	38.522100
2208.292503	398751.495995	38.527117
2210.588487	399478.652577	38.532135
2212.651327	400204.537046	38.537152
2214.442150	400946.084200	38.542170
2216.549061	401684.443252	38.547188
2218.390436	402429.441034	38.552205
2220.731892	403169.471699	38.557223
2223.463294	403904.072241	38.562240
2225.224092	404672.919520	38.567258
2228.287471	405414.774208	38.572276
2230.160053	406175.833867	38.577293
2232.632803	406912.172007	38.582311
2234.982437	407674.910863	38.587328
2236.407706	408436.640974	38.592346
2238.815651	409193.526371	38.597364
2240.823181	409969.634450	38.602381
2243.482794	410729.855696	38.607399
2246.019656	411495.167582	38.612416
2247.718093	412258.949376	38.617434
2249.833355	413047.110222	38.622452
2252.243745	413819.063792	38.627469
2254.060229	414604.061403	38.632487
2256.349863	415386.576711	38.637504
2258.394438	416180.810506	38.642522
2261.252591	416961.285322	38.647540
2263.410966	417751.400039	38.652557
2265.301257	418551.006501	38.657575
2267.899077	419344.114888	38.662592
2270.283122	420131.561330	38.667610
2272.213540	420922.299528	38.672628
2274.498391	421743.898440	38.677645
2276.631713	422541.288149	38.682663
2279.232795	423338.195512	38.687680
2281.245691	424171.179210	38.692698
2283.135097	424968.733960	38.697716
2285.254714	425787.846696	38.702733
2287.305274	426617.829920	38.707751
2289.661897	427438.164825	38.712768
2291.588378	428274.542407	38.717786
2293.845315	429087.546987	38.722804
2296.114444	429924.114601	38.727821
2298.713507	430762.724845	38.732839
2301.600140	431556.101313	38.737856
2303.478214	432363.741191	38.742874
2305.840546	433177.348052	38.747892
2307.905896	433983.888999	38.752909
2310.239693	434787.472640	38.757927
2312.224772	435586.631824	38.762944
2314.156253	436411.079130	38.767962
2316.915176	437224.681362	38.772980
2319.375810	438043.466121	38.777997
2322.013336	438846.149470	38.783015
2325.254480	439644.909417	38.788032
2328.043954	440445.284341	38.793050
2330.404863	441254.253348	38.798068
2332.859726	442045.113030	38.803085
2335.103867	442847.313656	38.808103
2337.858962	443630.528161	38.813120
2340.491264	444437.464546	38.818138
2342.975339	445217.833983	38.823156
2345.656334	445993.741635	38.828173
2347.908747	446792.710921	38.833191
2350.317179	447587.476839	38.838208
2352.355585	448382.578070	38.843226
2354.710948	449198.185629	38.848244
2357.006436	449979.173435	38.853261
2359.162533	450789.947785	38.858279
2361.362567	451601.088589	38.863296
2363.758724	452412.469425	38.868314
2365.535224	453239.194826	38.873332
2367.933729	454077.315732	38.878349
2369.880659	454900.255600	38.883367
2372.256010	455737.605551	38.888384
2374.150415	456581.220650	38.893402
2376.470713	457441.316247	38.898420
2379.403016	458280.898144	38.903437
2381.619531	459138.108058	38.908455
2384.146772	459988.455788	38.913472
2385.944278	460852.336093	38.918490
2388.862564	461709.169801	38.923508
2391.015917	462585.606087	38.928525
2393.065639	463457.977050	38.933543
2395.246308	464332.765006	38.938560
2397.432853	465232.482692	38.943578
2400.483851	466102.247046	38.948596
2402.665606	466986.166482	38.953613
2405.122591	467885.313693	38.958631
2407.748104	468771.858651	38.963648
2409.926951	469659.093624	38.968666
2412.098954	470569.028030	38.973684
2414.378240	471479.255348	38.978701
2416.554916	472408.706845	38.983719
2418.780591	473322.492974	38.988736
2420.821102	474248.946488	38.993754
2423.312273	475184.474688	38.998772
2425.782154	476115.211252	39.003789
2428.058132	477049.014816	39.008807
2430.786562	477964.765376	39.013824
2433.817072	478904.210621	39.018842
2436.295049	479842.537485	39.023860
2439.484256	480739.892066	39.028877
2441.925492	481668.434790	39.033895
2444.302598	482599.617198	39.038912
2446.848484	483510.929477	39.043930
2449.795303	484418.898087	39.048948
2452.620721	485322.094708	39.053965
2455.100031	486231.613917	39.058983
2457.432379	487141.716816	39.064000
2460.033114	488035.725607	39.069018
2462.303523	488918.082595	39.074036
2464.781187	489801.168894	39.079053
2466.587627	490670.390088	39.084071
2469.106596	491531.475819	39.089088
2471.755701	492432.016188	39.094106
2473.799997	493307.880104	39.099124
2476.175430	494180.061981	39.104141
2478.224678	495070.016450	39.109159
2480.606620	495976.067681	39.114176
2482.828317	496870.895651	39.119194
2484.858273	497787.353386	39.124212
2487.640133	498684.768441	39.129229
2490.368313	499611.607198	39.134247
2493.352839	500516.155996	39.139264
2496.155692	501409.335945	39.144282
2498.420179	502320.513962	39.149300
2501.067202	503228.956148	39.154317
2503.257571	504151.797969	39.159335
2506.210632	505077.589255	39.164352
2508.710606	505991.047651	39.169370
2511.132668	506917.326858	39.174388
2513.898430	507846.875194	39.179405
2516.028717	508778.491919	39.184423
2518.832384	509702.784523	39.189440
2521.634206	510641.191207	39.194458
2524.219527	511566.420961	39.199476
2527.176374	512488.914598	39.204493
2529.517485	513429.854814	39.209511
2532.286017	514361.394436	39.214528
2534.757203	515287.938461	39.219546
2536.901078	516222.394392	39.224564
2539.572850	517150.962599	39.229581
2542.365155	518107.322487	39.234599
2545.052543	519032.601371	39.239616
2547.777243	519975.504320	39.244634
2550.937237	520916.968001	39.249652
2553.569279	521837.200872	39.254669
2555.601495	522789.567316	39.259687
2558.291535	523715.622107	39.264704
2561.286667	524646.909521	39.269722
2563.500084	525598.465884	39.274740
2566.192992	526534.975491	39.279757
2568.510443	527498.532558	39.284775
2570.693686	528445.280717	39.289792
2573.217219	529399.768098	39.294810
2575.633484	530364.735369	39.299828
2578.143158	531330.278976	39.304845
2580.752824	532295.239551	39.309863
2583.521193	533257.845341	39.314880
2586.580174	534227.991422	39.319898
2588.636464	535188.876103	39.324916
2591.201545	536154.747303	39.329933
2593.526554	537146.462341	39.334951
2596.043956	538120.011109	39.339968
2598.389638	539102.932401	39.344986
2600.628772	540085.753590	39.350004
2602.916411	541102.863749	39.355021
2605.204168	542111.298143	39.360039
2607.863658	543117.939445	39.365056
2610.332491	544141.945406	39.370074
2612.667072	545167.659503	39.375092
2614.780984	546209.882312	39.380109
2617.557475	547232.555699	39.385127
2620.666258	548263.245900	39.390144
2623.281951	549297.812681	39.395162
2625.801960	550343.932644	39.400180
2628.774665	551379.792784	39.405197
2631.608617	552417.558188	39.410215
2633.754061	553446.158927	39.415232
2636.779414	554460.412238	39.420250
2638.988344	555456.981769	39.425268
2642.055586	556447.807914	39.430285
2644.561209	557456.192562	39.435303
2646.912970	558459.903712	39.440320
2649.725370	559456.278258	39.445338
2652.067050	560472.753166	39.450356
2654.667973	561475.693602	39.455373
2657.001018	562504.674398	39.460391
2659.632022	563547.238970	39.465408
2662.649856	564568.511215	39.470426
2665.265984	565600.819168	39.475444
2668.126258	566621.253752	39.480461
2670.880170	567651.769303	39.485479
2673.591264	568690.745880	39.490496
2676.828546	569724.832541	39.495514
2679.255109	570763.236946	39.500532
2682.174551	571790.883849	39.505549
2684.894589	572840.215525	39.510567
2687.824706	573868.947961	39.515584
2690.561723	574917.001009	39.520602
2693.129211	575967.403831	39.525620
2695.935409	576999.113479	39.530637
2699.042602	578052.564840	39.535655
2701.594009	579093.727251	39.540672
2705.177315	580128.512274	39.545690
2707.911758	581172.480437	39.550708
2710.993413	582204.666644	39.555725
2714.031994	583238.428600	39.560743
2716.477830	584274.006652	39.565760
2719.632776	585310.132437	39.570778
2721.742036	586340.476101	39.575796
2724.139639	587382.416963	39.580813
2726.983058	588438.783304	39.585831
2729.901587	589495.395785	39.590848
2732.794320	590530.216284	39.595866
2735.220008	591591.086502	39.600884
2738.069104	592654.849827	39.605901
2740.758713	593690.633061	39.610919
2743.102615	594761.306753	39.615936
2745.909806	595820.985380	39.620954
2748.430659	596895.394568	39.625972
2751.342696	597963.429681	39.630989
2754.042133	599030.550993	39.636007
2757.233827	600101.500310	39.641024
2759.821545	601189.176795	39.646042
2762.277719	602251.535836	39.651060
2765.102404	603349.285563	39.656077
2768.091520	604432.585224	39.661095
2770.797959	605513.126052	39.666112
2773.808252	606601.923988	39.671130
2776.703324	607680.476815	39.676148
2779.756892	608760.552680	39.681165
2782.880604	609831.056353	39.686183
2785.894933	610915.636687	39.691200
2789.239162	611973.441656	39.696218
2791.837796	613035.672064	39.701236
2794.657621	614100.716392	39.706253
2797.671739	615172.779323	39.711271
2800.105574	616232.381474	39.716288
2803.040175	617305.701700	39.721306
2805.649097	618370.920878	39.726324
2808.153323	619439.504017	39.731341
2810.774342	620514.562818	39.736359
2813.508720	621592.896384	39.741376
2816.188246	622662.185409	39.746394
2819.272025	623761.239161	39.751412
2822.030243	624821.706155	39.756429
2824.567492	625861.818455	39.761447
2826.869483	626904.017407	39.766464
2829.891669	627945.147143	39.771482
2832.300080	629005.109035	39.776500
2834.647174	630060.130689	39.781517
2837.111517	631135.205372	39.786535
2839.278917	632220.656980	39.791552
2842.179061	633298.735892	39.796570
2844.311220	634402.443927	39.801588
2847.374620	635503.186639	39.806605
2850.236540	636627.657217	39.811623
2852.715933	637743.884064	39.816640
2855.659565	638878.130368	39.821658
2858.326788	640012.497659	39.826676
2861.233409	641164.014575	39.831693
2863.963552	642304.905035	39.836711
2866.307316	643480.401748	39.841728
2869.064546	644631.753635	39.846746
2871.684598	645825.589300	39.851764
2874.538312	646995.758955	39.856781
2877.682430	648188.581828	39.861799
2880.660440	649399.737398	39.866816
2883.687086	650580.381085	39.871834
2886.622258	651790.607258	39.876852
2889.452395	652994.773533	39.881869
2892.472650	654203.895438	39.886887
2895.332371	655432.427791	39.891904
2898.373048	656649.369263	39.896922
2901.087413	657870.199251	39.901940
2903.986241	659099.712635	39.906957
2906.942880	660329.510288	39.911975
2909.869870	661553.331969	39.916992
2913.201282	662804.166660	39.922010
2916.214728	664036.174694	39.927028
2919.028627	665287.719401	39.932045
2922.557918	666534.355090	39.937063
2924.980791	667773.696151	39.942080
2928.075418	669033.613272	39.947098
2930.946020	670283.898781	39.952116
2933.624588	671545.541723	39.957133
2936.983967	672790.143551	39.962151
2939.352758	674064.929692	39.967168
2942.673468	675330.784280	39.972186
2945.834711	676583.767045	39.977204
2948.778859	677861.123746	39.982221
2952.003623	679115.942884	39.987239
2954.773482	680399.887832	39.992256
2958.013656	681651.528249	39.997274
2960.771712	682924.093267	40.002292
2963.908470	684182.659784	40.007309
2967.249166	685457.161593	40.012327
2970.017679	686730.089829	40.017344
2973.117751	688021.603937	40.022362
2976.108278	689271.199369	40.027380
2978.955468	690553.556646	40.032397
2981.890840	691814.523686	40.037415
2984.894964	693100.561627	40.042432
2987.787993	694379.734511	40.047450
2990.878766	695666.926753	40.052468
2994.058290	696927.032525	40.057485
2997.357938	698212.332898	40.062503
3000.177734	699486.913016	40.067520
3003.585654	700735.131167	40.072538
3006.748115	702015.436251	40.077556
3009.707468	703279.031542	40.082573
3013.193915	704539.928305	40.087591
3015.995155	705793.123662	40.092608
3019.160569	707044.492198	40.097626
3022.168084	708253.893855	40.102644
3025.190809	709482.985737	40.107661
3028.005877	710680.982205	40.112679
3030.778436	711896.000971	40.117696
3033.671014	713082.753701	40.122714
3036.493650	714313.510681	40.127732
3039.413180	715535.163491	40.132749
3042.825170	716770.762346	40.137767
3045.429168	717994.041348	40.142784
3048.401145	719221.979751	40.147802
3051.464575	720450.860863	40.152820
3054.251197	721691.279629	40.157837
3057.247425	722933.704501	40.162855
3060.208441	724202.848060	40.167872
3063.258018	725451.067539	40.172890
3066.050188	726730.677731	40.177908
3068.661125	728000.975366	40.182925
3072.224147	729287.967806	40.187943
3074.917590	730579.693434	40.192960
3077.982129	731867.744562	40.197978
3081.289279	733163.306064	40.202996
3083.970341	734462.763572	40.208013
3087.090023	735775.271264	40.213031
3089.972129	737106.906980	40.218048
3093.376949	738421.008921	40.223066
3096.418376	739757.607251	40.228084
3099.581246	741080.243979	40.233101
3102.316746	742417.531553	40.238119
3105.026784	743768.853037	40.243136
3108.239880	745112.709239	40.248154
3111.785533	746467.819723	40.253172
3115.188846	747813.352332	40.258189
3119.128042	749154.966771	40.263207
3122.571353	750517.230018	40.268224
3126.071732	751842.633161	40.273242
3129.499381	753186.592409	40.278260
3132.972404	754516.764136	40.283277
3136.218259	755845.512215	40.288295
3139.219541	757187.021149	40.293312
3142.205237	758523.718798	40.298330
3145.089158	759864.875323	40.303348
3147.692859	761215.832300	40.308365
3150.849506	762575.905191	40.313383
3154.009644	763932.436481	40.318400
3156.704423	765298.342878	40.323418
3159.903368	766662.983406	40.328436
3162.801974	768034.308646	40.333453
3166.673645	769395.684185	40.338471
3169.886829	770758.295372	40.343488
3172.968802	772126.476858	40.348506
3176.043052	773507.132408	40.353524
3178.999447	774890.791081	40.358541
3182.544965	776258.473164	40.363559
3185.817936	777652.659093	40.368576
3188.899058	779026.333083	40.373594
3191.861151	780412.235984	40.378612
3194.743251	781800.046912	40.383629
3198.212896	783182.146264	40.388647
3201.291058	784586.760138	40.393664
3204.336916	785976.193576	40.398682
3207.578479	787371.504635	40.403700
3210.726198	788787.446085	40.408717
3214.278183	790166.371246	40.413735
3217.362327	791585.442732	40.418752
3220.551609	792967.852729	40.423770
3223.939443	794364.363124	40.428788
3226.750261	795783.174558	40.433805
3229.988530	797165.584436	40.438823
3233.098063	798545.196130	40.443840
3236.120106	799897.967266	40.448858
3239.616392	801239.237667	40.453876
3242.839763	802610.828844	40.458893
3246.469057	803952.432208	40.463911
3249.711867	805311.887874	40.468928
3252.731393	806684.853851	40.473946
3255.794610	808042.379620	40.478964
3258.998952	809405.967517	40.483981
3262.118584	810775.650238	40.488999
3265.308850	812149.785046	40.494016
3268.207200	813537.661980	40.499034
3271.630476	814910.268813	40.504052
3275.170960	816318.080493	40.509069
3278.638080	817704.418199	40.514087
3281.701403	819092.341252	40.519104
3284.809710	820489.826843	40.524122
3288.000951	821906.425689	40.529140
3291.119964	823341.515931	40.534157
3294.423280	824745.877691	40.539175
3297.368144	826179.160066	40.544192
3300.602217	827633.338486	40.549210
3303.661082	829068.993213	40.554228
3306.350546	830532.901094	40.559245
3309.296338	832001.942952	40.564263
3312.520116	833483.757976	40.569280
3315.316137	834980.741307	40.574298
3318.641449	836475.731972	40.579316
3321.627372	838003.968109	40.584333
3324.973359	839509.151876	40.589351
3327.928106	841036.814586	40.594368
3331.149124	842592.618751	40.599386
3334.698868	844134.906371	40.604404
3337.932175	845696.413870	40.609421
3341.530833	847261.848884	40.614439
3344.710384	848820.160120	40.619456
3347.466961	850393.893346	40.624474
3351.255203	851962.591845	40.629492
3355.383828	853528.314002	40.634509
3359.022384	855088.187768	40.639527
3363.040830	856646.634870	40.644544
3366.757859	858211.239084	40.649562
3370.429048	859773.027125	40.654580
3374.835310	861314.413297	40.659597
3378.408380	862842.166518	40.664615
3382.399832	864364.814248	40.669632
3385.806638	865903.748620	40.674650
3389.774391	867410.031412	40.679668
3392.876655	868927.413847	40.684685
3396.474056	870430.483350	40.689703
3399.911101	871945.982236	40.694720
3403.272402	873469.820575	40.699738
3406.058371	874975.364971	40.704756
3409.106705	876507.379237	40.709773
3412.346638	878042.157239	40.714791
3415.278227	879568.368024	40.719808
3418.416485	881118.219247	40.724826
3421.701355	882661.355101	40.729844
3425.224915	884216.701211	40.734861
3428.639102	885770.394673	40.739879
3431.948445	887307.273968	40.744896
3435.536099	888881.832720	40.749914
3438.850463	890451.374603	40.754932
3441.847570	892017.163860	40.759949
3444.913346	893594.089874	40.764967
3448.565135	895172.509882	40.769984
3452.423346	896758.171579	40.775002
3455.963840	898329.226036	40.780007
3459.135495	899855.093885	40.785012
3462.541626	901310.977446	40.790016
3465.679335	902719.412360	40.795021
3468.526033	904077.444567	40.800026
3471.577621	905336.003245	40.805031
3474.624739	906550.282331	40.810036
3477.644993	907686.743893	40.815040
3480.787810	908755.923065	40.820045
3483.254792	909745.936003	40.825050
3485.914693	910681.652745	40.830055
3488.069154	911527.355395	40.835060
3490.084502	912333.241209	40.840064
3492.280605	913070.652495	40.845069
3494.203293	913768.984663	40.850074
3496.155140	914378.197961	40.855079
3497.775842	914965.047760	40.860084
3499.079729	915475.209354	40.865088
3500.652774	915965.148126	40.870093
3501.558907	916391.201295	40.875098
3503.160971	916764.523496	40.880103
3504.366686	917099.172712	40.885108
3505.609780	917396.432743	40.890112
3506.549275	917652.032753	40.895117
3507.426877	917899.061476	40.900122
3508.705066	918080.925843	40.905127
3509.432714	918238.323310	40.910132
3510.256696	918370.379233	40.915136
3511.516396	918470.107651	40.920141
3512.105856	918540.580753	40.925146
3512.872520	918578.579314	40.930151
3513.416123	918613.244759	40.935156
3513.877062	918596.802203	40.940160
3514.510070	918583.700865	40.945165
3514.762461	918550.733281	40.950170
3515.537495	918488.700367	40.955175
3515.828553	918405.950534	40.960180
3516.124592	918307.505112	40.965184
3516.608954	918198.532246	40.970189
3516.585420	918071.828434	40.975194
3517.145051	917925.094441	40.980199
3517.603689	917801.963822	40.985204
3517.848765	917631.105327	40.990208
3518.300072	917443.452285	40.995213
3518.219946	917276.006557	41.000218
3518.831290	917071.462288	41.005223
3518.525392	916875.439953	41.010228
3518.745660	916650.238811	41.015232
3518.868674	916433.519916	41.020237
3518.854184	916224.327747	41.025242
3519.201529	915977.406836	41.030247
3519.350348	915750.928306	41.035252
3519.677074	915508.516911	41.040256
3519.727107	915255.351077	41.045261
3519.558104	915007.411861	41.050266
3519.750211	914749.575090	41.055271
3519.849518	914476.518729	41.060276
3520.141994	914213.630237	41.065280
3520.213589	913943.442496	41.070285
3520.071736	913657.955240	41.075290
3519.999682	913377.549074	41.080295
3519.829821	913093.097153	41.085300
3519.941552	912804.150864	41.090304
3520.235282	912523.062696	41.095309
3520.022829	912243.489364	41.100314
3520.204435	911925.280528	41.105319
3519.785499	911648.217222	41.110324
3520.037520	911346.543572	41.115328
3519.994199	911049.336814	41.120333
3520.001134	910743.139495	41.125338
3520.182319	910437.957123	41.130343
3520.078917	910141.482839	41.135348
3519.810215	909843.477069	41.140352
3519.952729	909527.451002	41.145357
3519.629160	909234.339617	41.150362
3519.868320	908919.227373	41.155367
3519.921577	908634.123501	41.160372
3519.856527	908312.468431	41.165376
3519.913710	908000.227679	41.170381
3519.731185	907698.137712	41.175386
3519.450526	907393.153405	41.180391
3519.374372	907075.287453	41.185396
3519.524733	906765.952887	41.190400
3519.470493	906455.959458	41.195405
3519.228698	906160.549942	41.200410
3519.021116	905846.881260	41.205415
3519.115655	905546.173010	41.210420
3518.881879	905248.397881	41.215424
3519.379515	904939.677025	41.220429
3518.662527	904644.169110	41.225434
3518.810948	904321.476600	41.230439
3518.775936	904037.117539	41.235444
3518.479144	903731.163723	41.240448
3518.577661	903446.270044	41.245453
3517.941017	903131.071789	41.250458
3518.344861	902833.739128	41.255463
3518.282230	902544.288442	41.260468
3518.199707	902234.452186	41.265472
3518.527826	901935.153316	41.270477
3517.824279	901640.160943	41.275482
3517.809594	901359.236074	41.280487
3517.796559	901068.639024	41.285492
3517.681275	900771.282950	41.290496
3517.950105	900485.535235	41.295501
3517.532133	900192.062062	41.300506
3517.527795	899896.766725	41.305511
3517.299373	899615.017446	41.310516
3517.068675	899329.873194	41.315520
3517.511392	899039.483124	41.320525
3517.346942	898765.120250	41.325530
3517.192875	898466.876399	41.330535
3517.313501	898182.389494	41.335540
3516.957018	897904.634598	41.340544
3516.927773	897600.140080	41.345549
3516.744411	897330.639471	41.350554
3516.386997	897048.107312	41.355559
3516.284968	896765.229083	41.360564
3516.543262	896490.879937	41.365568
3516.804930	896212.070565	41.370573
3516.471395	895949.102225	41.375578
3516.290974	895663.088809	41.380583
3516.433193	895404.560525	41.385588
3515.939575	895126.305810	41.390592
3516.004239	894847.075401	41.395597
3515.718974	894587.903729	41.400602
3515.785960	894317.542472	41.405607
3515.796582	894038.378128	41.410612
3515.631218	893780.407169	41.415616
3515.632911	893507.600795	41.420621
3515.283376	893253.891573	41.425626
3515.389047	892998.258521	41.430631
3515.118211	892738.420370	41.435636
3514.915866	892487.264413	41.440640
3514.978462	892219.319642	41.445645
3515.194311	891976.681373	41.450650
3515.119576	891713.088605	41.455655
3514.967077	891459.751241	41.460660
3514.663407	891217.069718	41.465664
3514.655190	890964.170481	41.470669
3514.261061	890712.194484	41.475674
3514.352565	890459.450152	41.480679
3513.968864	890228.834999	41.485684
3514.061552	889989.616659	41.490688
3514.495540	889743.074350	41.495693
3513.991114	889515.450440	41.500698
3514.166448	889270.962834	41.505703
3514.033324	889023.805753	41.510708
3513.861043	888775.676670	41.515712
3514.092044	888535.504197	41.520717
3513.990007	888313.283722	41.525722
3513.755885	888070.845478	41.530727
3513.747616	887824.874959	41.535732
3513.649346	887590.428879	41.540736
3513.680914	887366.891567	41.545741
3513.339004	887130.337155	41.550746
3513.315177	886902.724840	41.555751
3513.399972	886672.858785	41.560756
3513.131476	886453.499049	41.565760
3513.107373	886220.437750	41.570765
3512.427363	886000.063527	41.575770
3512.894164	885773.875480	41.580775
3512.920342	885561.115289	41.585780
3512.447883	885340.488184	41.590784
3512.706383	885116.342620	41.595789
3512.762367	884905.684218	41.600794
3512.637715	884671.124608	41.605799
3512.646336	884460.845344	41.610804
3512.327241	884242.863440	41.615808
3512.416884	884026.840261	41.620813
3512.157190	883820.553625	41.625818
3512.195767	883611.498113	41.630823
3512.100400	883409.819817	41.635828
3511.845193	883195.760215	41.640832
3511.988097	882984.436829	41.645837
3511.370292	882795.321369	41.650842
3511.358898	882579.842631	41.655847
3511.711208	882387.938166	41.660852
3511.440451	882195.161068	41.665856
3511.751048	881991.816648	41.670861
3511.372935	881808.831431	41.675866
3511.565693	881592.701322	41.680871
3511.190718	881411.156770	41.685876
3511.289751	881203.071251	41.690880
3511.034663	881013.935412	41.695885
3511.089546	880822.222513	41.700890
3511.179677	880630.885240	41.705895
3511.115825	880442.087170	41.710900
3510.685149	880255.960534	41.715904
3511.450368	880048.596745	41.720909
3511.080479	879873.692135	41.725914
3510.905953	879666.469662	41.730919
3510.596647	879485.824155	41.735924
3510.673650	879303.946139	41.740928
3510.702854	879126.045230	41.745933
3510.283497	878950.151840	41.750938
3510.524239	878745.737079	41.755943
3510.157111	878574.477653	41.760948
3510.078552	878402.099167	41.765952
3510.292909	878221.037750	41.770957
3510.205410	878045.256628	41.775962
3510.081009	877856.288660	41.780967
3509.958084	877692.139059	41.785972
3509.908470	877521.863468	41.790976
3509.980569	877356.217805	41.795981
3509.734638	877180.921941	41.800986
3509.735473	877016.345269	41.805991
3509.817286	876850.974803	41.810996
3509.723170	876683.591953	41.816000
3509.952846	876496.267976	41.821005
3509.515521	876340.764819	41.826010
3509.396699	876170.073751	41.831015
3509.816030	876006.661037	41.836020
3509.718762	875830.039703	41.841024
3509.486010	875671.284226	41.846029
3509.763565	875502.351731	41.851034
3509.470452	875351.940244	41.856039
3509.331347	875186.559727	41.861044
3509.317438	875029.982326	41.866048
3509.365474	874853.210973	41.871053
3509.105244	874694.045814	41.876058
3509.232456	874546.261253	41.881063
3508.971687	874372.922269	41.886068
3509.105086	874218.045674	41.891072
3508.937620	874068.260186	41.896077
3508.981356	873909.412081	41.901082
3508.722225	873763.903481	41.906087
3509.021882	873611.021453	41.911092
3508.560460	873456.514134	41.916096
3508.606516	873307.838831	41.921101
3508.631482	873157.222391	41.926106
3508.534891	873013.803692	41.931111
3508.554587	872858.134090	41.936116
3508.149249	872721.649771	41.941120
3508.689375	872563.266346	41.946125
3508.453247	872418.109323	41.951130
3508.701478	872281.216112	41.956135
3508.274618	872123.562658	41.961140
3508.302788	871990.581514	41.966144
3508.363101	871848.662006	41.971149
3508.047779	871700.297387	41.976154
3508.039518	871555.373076	41.981159
3507.844357	871416.591672	41.986164
3507.612385	871294.801345	41.991168
3507.991375	871149.803428	41.996173
3507.855928	871035.272755	42.001178
3507.701918	870893.462971	42.006183
3507.693290	870750.072534	42.011188
3507.174879	870628.801258	42.016192
3507.552724	870503.787638	42.021197
3507.302690	870367.321069	42.026202
3507.566837	870246.398613	42.031207
3507.281548	870105.659825	42.036212
3507.202107	869984.497398	42.041216
3507.505817	869857.734788	42.046221
3507.113808	869735.939133	42.051226
3507.004543	869607.491448	42.056231
3507.159766	869479.191661	42.061236
3507.112449	869380.734257	42.066240
3507.264361	869247.671854	42.071245
3507.116108	869121.259474	42.076250
3506.941914	869018.835500	42.081255
3506.982379	868882.870008	42.086260
3506.733338	868769.674396	42.091264
3506.765638	868649.340682	42.096269
3506.468096	868528.476168	42.101274
3506.631121	868409.864298	42.106279
3506.491416	868306.354166	42.111284
3506.479911	868208.065913	42.116288
3506.522263	868082.280184	42.121293
3506.485516	867986.712044	42.126298
3506.325937	867858.235284	42.131303
3506.736531	867756.276289	42.136308
3506.126278	867638.262258	42.141312
3506.298214	867527.985131	42.146317
3506.321032	867434.729701	42.151322
3506.100617	867314.993786	42.156327
3506.200255	867225.608062	42.161332
3505.944407	867125.011004	42.166336
3506.246521	867003.919994	42.171341
3506.191508	866910.280701	42.176346
3506.168677	866810.902930	42.181351
3506.262065	866687.314107	42.186356
3506.550927	866600.316709	42.191360
3506.543554	866477.517402	42.196365
3506.422322	866376.982864	42.201370
3506.554276	866260.471264	42.206375
3506.058264	866148.627305	42.211380
3505.923433	866046.534973	42.216384
3506.252391	865936.591576	42.221389
3506.068956	865837.418579	42.226394
3506.015908	865747.647491	42.231399
3505.863799	865643.705072	42.236404
3505.662403	865559.688461	42.241408
3505.937628	865444.789414	42.246413
3505.534939	865356.138978	42.251418
3505.518573	865244.685157	42.256423
3505.612895	865154.881008	42.261428
3505.573054	865057.809426	42.266432
3505.763905	864962.544667	42.271437
3505.468509	864885.045075	42.276442
3505.495781	864790.581988	42.281447
3505.464561	864690.879241	42.286452
3505.516115	864599.713368	42.291456
3505.703631	864508.523731	42.296461
3505.445485	864416.628638	42.301466
3505.135875	864312.106202	42.306471
3505.448824	864229.347062	42.311476
3505.119313	864139.986456	42.316480
3505.389313	864048.970713	42.321485
3505.154214	863957.356446	42.326490
3505.147982	863869.007734	42.331495
3505.291796	863784.715276	42.336500
3505.058882	863700.872491	42.341504
3505.222553	863599.856157	42.346509
3505.019479	863532.724411	42.351514
3504.849249	863441.577684	42.356519
3505.023599	863358.926726	42.361524
3504.778506	863289.952357	42.366528
3505.228134	863190.437395	42.371533
3504.990530	863121.848710	42.376538
3504.773075	863028.273390	42.381543
3504.974176	862953.000359	42.386548
3504.897381	862867.273379	42.391552
3505.176711	862777.111972	42.396557
3504.980407	862712.108729	42.401562
3504.725838	862616.102845	42.406567
3504.927546	862535.672154	42.411572
3504.652973	862468.346006	42.416576
3504.784887	862391.327517	42.421581
3504.795529	862306.744870	42.426586
3504.503292	862232.613618	42.431591
3504.589221	862151.613603	42.436596
3504.580613	862090.656156	42.441600
3504.486057	861987.516692	42.446605
3504.443136	861926.077126	42.451610
3504.329524	861835.188703	42.456615
3504.634211	861781.565856	42.461620
3504.414521	861707.999644	42.466624
3504.363791	861640.141329	42.471629
3504.464690	861574.590846	42.476634
3504.383472	861499.151906	42.481639
3504.351898	861427.690454	42.486644
3504.134741	861351.591442	42.491648
3504.168646	861290.424529	42.496653
3504.285723	861212.421242	42.501658
3504.187584	861138.828150	42.506663
3504.247537	861076.001742	42.511668
3504.194134	860999.482412	42.516672
3504.241716	860936.170401	42.521677
3504.055193	860864.825128	42.526682
3504.254456	860794.290677	42.531687
3504.403911	860727.847917	42.536692
3503.718622	860661.639171	42.541696
3503.975026	860603.929605	42.546701
3504.301260	860540.470353	42.551706
3504.466779	860465.658751	42.556711
3504.487611	860398.552855	42.561716
3504.423500	860321.637806	42.566720
3504.727780	860254.289139	42.571725
3504.395497	860177.610955	42.576730
3504.523958	860110.386919	42.581735
3504.175210	860043.338002	42.586740
3503.982010	859985.696664	42.591744
3504.280960	859894.808687	42.596749
3504.231763	859842.880531	42.601754
3503.897173	859769.698948	42.606759
3504.315658	859700.088390	42.611764
3504.100179	859638.070680	42.616768
3504.196183	859559.077167	42.621773
3504.306625	859486.888805	42.626778
3503.768140	859424.435809	42.631783
3503.975285	859353.688940	42.636788
3503.880346	859292.523281	42.641792
3504.215711	859242.277519	42.646797
3503.657161	859187.412372	42.651802
3503.684241	859113.774304	42.656807
3503.984947	859068.785453	42.661812
3503.810489	858991.871885	42.666816
3503.539195	858936.859907	42.671821
3503.490956	858880.546127	42.676826
3503.443835	858817.325088	42.681831
3503.743440	858764.552144	42.686836
3503.609613	858710.488257	42.691840
3503.726811	858649.573079	42.696845
3503.574426	858597.554096	42.701850
3503.344958	858550.216798	42.706855
3503.748188	858471.450521	42.711860
3503.657683	858428.661603	42.716864
3503.689746	858370.287002	42.721869
3503.454984	858309.134572	42.726874
3503.286529	858262.563275	42.731879
3503.383575	858196.004428	42.736884
3503.276626	858156.621309	42.741888
3503.384105	858109.127826	42.746893
3502.997339	858060.256071	42.751898
3503.171410	857996.601003	42.756903
3503.108780	857951.663824	42.761908
3503.484108	857897.898079	42.766912
3503.451981	857845.852923	42.771917
3503.372900	857795.858187	42.776922
3503.283758	857734.384177	42.781927
3503.539210	857690.171038	42.786932
3503.406561	857639.210917	42.791937
3503.090983	857604.042270	42.796941
3503.435374	857542.397640	42.801946
3503.052923	857496.439560	42.806951
3503.141605	857429.192721	42.811956
3502.911023	857394.300766	42.816961
3503.023964	857345.049122	42.821965
3502.948587	857302.152573	42.826970
3503.028551	857253.002925	42.831975
3503.293926	857203.530442	42.836980
3502.983296	857154.347040	42.841985
3503.057523	857100.526631	42.846989
3502.951414	857066.390736	42.851994
3503.250894	857019.343738	42.856999
3503.180319	856956.788562	42.862004
3503.267939	856926.998707	42.867009
3503.557314	856874.405857	42.872013
3503.264113	856826.190025	42.877018
3503.029746	856783.997204	42.882023
3503.161148	856721.114445	42.887028
3503.008643	856695.352676	42.892033
3502.950462	856640.090419	42.897037
3503.039079	856591.517931	42.902042
3503.012805	856544.618280	42.907047
3503.296702	856500.975797	42.912052
3502.845493	856457.843336	42.917057
3502.656778	856402.211197	42.922061
3502.818610	856356.446896	42.927066
3502.945929	856329.080475	42.932071
3503.014378	856276.518919	42.937076
3502.819234	856235.191721	42.942081
3502.960483	856169.771496	42.947085
3502.894186	856139.516604	42.952090
3502.244408	856104.589069	42.957095
3502.596990	856059.861654	42.962100
3502.508840	856037.298064	42.967105
3503.031679	855989.135912	42.972109
3502.623433	855946.090113	42.977114
3502.398623	855918.098624	42.982119
3502.817421	855873.748242	42.987124
3502.739215	855838.725055	42.992129
3503.236064	855789.203113	42.997133
3502.936573	855735.529676	43.002138
3502.698936	855698.293496	43.007143
3503.013110	855664.177939	43.012148
3502.947606	855618.056312	43.017153
3502.783056	855569.809464	43.022157
3502.996893	855533.568524	43.027162
3502.791865	855495.157819	43.032167
3503.199361	855447.399762	43.037172
3503.123692	855404.295405	43.042177
3503.098484	855366.535588	43.047181
3502.947482	855316.337929	43.052186
3502.537578	855271.243748	43.057191
3502.622394	855230.058371	43.062196
3502.441281	855203.321761	43.067201
3502.495042	855157.371717	43.072205
3502.904635	855120.122779	43.077210
3502.350772	855088.483037	43.082215
3502.456101	855051.089131	43.087220
3502.586928	855008.629347	43.092225
3502.666334	854963.257652	43.097229
3502.817539	854951.844344	43.102234
3502.520867	854904.003407	43.107239
3502.764876	854863.762746	43.112244
3502.366813	854828.105150	43.117249
3502.508397	854793.137176	43.122253
3502.513473	854745.342650	43.127258
3502.256381	854718.032417	43.132263
3502.496160	854680.614128	43.137268
3502.502120	854640.605907	43.142273
3502.494846	854606.634813	43.147277
3502.363931	854582.710167	43.152282
3502.100167	854539.436078	43.157287
3502.451897	854510.661848	43.162292
3502.037027	854486.783601	43.167297
3502.196350	854455.899242	43.172301
3502.462405	854436.678518	43.177306
3502.320374	854399.613455	43.182311
3502.684380	854368.208221	43.187316
3502.224452	854317.761304	43.192321
3502.216375	854295.762247	43.197325
3502.307149	854260.215553	43.202330
3502.020663	854229.208800	43.207335
3502.074155	854192.791729	43.212340
3502.023320	854165.834479	43.217345
3502.310080	854135.122231	43.222349
3502.366363	854096.757149	43.227354
3502.249853	854084.899592	43.232359
3502.590211	854050.868193	43.237364
3502.528490	854015.637267	43.242369
3502.478830	853977.775655	43.247373
3501.991956	853951.862812	43.252378
3502.123050	853910.953099	43.257383
3502.408685	853885.204796	43.262388
3502.184634	853864.213313	43.267393
3502.095504	853827.817591	43.272397
3502.330324	853793.023328	43.277402
3502.099829	853774.953245	43.282407
3502.496979	853725.918018	43.287412
3502.160029	853695.111613	43.292417
3502.387636	853665.380348	43.297421
3502.575567	853625.043530	43.302426
3502.063898	853601.177806	43.307431
3502.454413	853556.328715	43.312436
3502.521914	853536.164325	43.317441
3502.154025	853503.025450	43.322445
3502.262929	853472.923378	43.327450
3502.125801	853449.287458	43.332455
3502.727123	853408.978507	43.337460
3502.255120	853384.326527	43.342465
3502.234916	853355.608209	43.347469
3502.022768	853328.965975	43.352474
3502.263877	853304.196220	43.357479
3502.464535	853260.544615	43.362484
3502.323175	853238.758488	43.367489
3502.461047	853197.356140	43.372493
3502.506577	853166.484109	43.377498
3502.097403	853139.191961	43.382503
3502.040066	853108.726046	43.387508
3502.052539	853072.211790	43.392513
3502.186031	853049.503433	43.397517
3502.166266	853023.704499	43.402522
3502.315576	852987.459308	43.407527
3502.381896	852944.314446	43.412532
3502.291259	852929.432007	43.417537
3502.257326	852890.879595	43.422541
3502.054897	852861.896901	43.427546
3502.193302	852834.026370	43.432551
3502.140182	852803.363524	43.437556
3502.098634	852780.585645	43.442561
3502.100505	852752.639868	43.447565
3502.028696	852731.716844	43.452570
3502.020738	852704.648812	43.457575
3502.143226	852669.282531	43.462580
3502.072971	852642.419234	43.467585
3501.936591	852623.843429	43.472589
3502.439302	852598.346164	43.477594
3502.104941	852568.507470	43.482599
3502.181350	852532.563758	43.487604
3501.876316	852504.570041	43.492609
3501.968712	852462.001787	43.497613
3501.916551	852443.898451	43.502618
3501.792239	852417.140459	43.507623
3501.964333	852406.011166	43.512628
3502.015944	852379.613544	43.517633
3501.755512	852362.907552	43.522637
3501.894532	852323.349362	43.527642
3501.854022	852317.902839	43.532647
3501.770937	852278.867838	43.537652
3501.799472	852262.990388	43.542657
3502.175955	852238.096715	43.547661
3502.275176	852213.540749	43.552666
3501.777151	852181.390043	43.557671
3501.984773	852149.999367	43.562676
3502.105602	852129.529490	43.567681
3501.894263	852097.428510	43.572685
3501.853237	852075.816540	43.577690
3501.590484	852043.236840	43.582695
3501.853316	852024.496107	43.587700
3501.603594	852014.701566	43.592705
3501.467506	851991.936370	43.597709
3502.065069	851969.537168	43.602714
3501.738604	851963.260984	43.607719
3501.719556	851930.835321	43.612724
3501.664082	851912.049295	43.617729
3501.903104	851878.217473	43.622733
3501.964300	851856.198364	43.627738
3501.885425	851846.959727	43.632743
3501.882220	851818.231507	43.637748
3501.683934	851800.734681	43.642753
3501.839785	851788.633103	43.647757
3501.888924	851754.247567	43.652762
3501.895605	851738.567153	43.657767
3502.475128	851701.951456	43.662772
3502.089814	851690.328373	43.667777
3502.198612	851650.283948	43.672781
3502.124966	851616.502206	43.677786
3502.164688	851583.675501	43.682791
3502.216201	851552.210139	43.687796
3501.819475	851544.192084	43.692801
3501.899596	851519.733920	43.697805
3501.676960	851485.196883	43.702810
3501.733905	851483.142257	43.707815
3502.026150	851441.508021	43.712820
3501.813154	851433.264777	43.717825
3501.926002	851403.541612	43.722829
3502.370494	851382.821189	43.727834
3502.162105	851359.286449	43.732839
3502.459056	851315.410561	43.737844
3502.175790	851293.543595	43.742849
3502.104255	851260.636120	43.747853
3502.085249	851226.843266	43.752858
3501.794566	851206.438139	43.757863
3501.705533	851178.208081	43.762868
3501.747897	851151.806779	43.767873
3501.943910	851130.834260	43.772877
3501.820751	851116.342423	43.777882
3502.018035	851096.051355	43.782887
3502.430138	851052.057253	43.787892
3502.141332	851034.183590	43.792897
3501.871989	851013.871715	43.797901
3502.329295	850990.031136	43.802906
3502.020329	850970.115239	43.807911
3502.049456	850932.319503	43.812916
3502.045393	850894.626405	43.817921
3502.100524	850880.981256	43.822925
3502.068917	850848.357230	43.827930
3501.889880	850828.419479	43.832935
3502.087402	850799.945708	43.837940
3501.815643	850776.614007	43.842945
3501.979799	850747.366276	43.847949
3501.887841	850718.842414	43.852954
3501.677357	850708.260125	43.857959
3501.755506	850677.175574	43.862964
3501.652016	850656.348197	43.867969
3501.584037	850633.859031	43.872973
3502.111991	850620.622456	43.877978
3501.955907	850600.290577	43.882983
3501.792482	850568.758253	43.887988
3501.884942	850549.067105	43.892993
3501.669176	850524.653777	43.897997
3502.032941	850505.989272	43.903002
3501.675625	850488.612358	43.908007
3502.105887	850462.728691	43.913012
3501.864022	850436.468586	43.918017
3501.720706	850411.945476	43.923021
3501.925652	850375.481117	43.928026
3501.821921	850369.848486	43.933031
3502.014227	850336.892682	43.938036
3501.780335	850324.462829	43.943041
3501.880072	850307.107536	43.948045
3501.823080	850273.023545	43.953050
3501.452033	850261.298025	43.958055
3501.626366	850232.435849	43.963060
3501.676503	850216.744453	43.968065
3501.629477	850202.919828	43.973069
3502.004841	850176.946611	43.978074
3501.681926	850160.732051	43.983079
3501.868498	850140.537058	43.988084
3501.815554	850125.739119	43.993089
3501.665163	850101.508191	43.998093
3501.870772	850071.860823	44.003098
3501.430541	850067.354886	44.008103
3501.794045	850038.655483	44.013108
3501.556361	850023.498076	44.018113
3501.751823	849996.189949	44.023117
3502.022463	849976.370236	44.028122
3501.643574	849968.542032	44.033127
3501.876213	849925.641125	44.038132
3501.586089	849921.500018	44.043137
3501.647399	849891.485902	44.048141
3501.779843	849877.533581	44.053146
3501.461752	849862.973524	44.058151
3501.497432	849837.736763	44.063156
3501.798435	849822.100473	44.068161
3501.257826	849805.920846	44.073165
3501.378002	849789.534922	44.078170
3501.531120	849776.358310	44.083175
3501.515279	849750.155506	44.088180
3501.320392	849748.531463	44.093185
3501.553652	849722.287513	44.098189
3501.341398	849708.196753	44.103194
3501.297781	849698.169775	44.108199
3501.717758	849689.819963	44.113204
3501.724383	849657.767935	44.118209
3501.311532	849642.248776	44.123213
3501.758945	849637.304061	44.128218
3501.480372	849596.433494	44.133223
3501.606966	849591.833847	44.138228
3501.394176	849578.717088	44.143233
3501.113480	849549.049922	44.148237
3501.298271	849548.337500	44.153242
3501.450142	849544.707866	44.158247
3501.698161	849528.689888	44.163252
3501.542215	849510.595129	44.168257
3501.676401	849487.484007	44.173261
3501.561692	849460.029786	44.178266
3501.221256	849456.676035	44.183271
3501.268485	849439.034716	44.188276
3501.394892	849437.649939	44.193281
3501.360043	849396.250805	44.198285
3501.277329	849399.674212	44.203290
3501.108724	849386.257500	44.208295
3501.351613	849384.366407	44.213300
3501.163396	849364.328066	44.218305
3501.029396	849366.590851	44.223309
3501.772775	849349.419161	44.228314
3501.287051	849345.894431	44.233319
3501.193885	849322.625299	44.238324
3501.129462	849310.555209	44.243329
3501.364550	849293.272237	44.248333
3501.264787	849291.729830	44.253338
3501.269683	849274.192445	44.258343
3501.271259	849254.025065	44.263348
3501.107848	849244.796496	44.268353
3501.126644	849229.010360	44.273357
3501.185104	849230.364658	44.278362
3501.233644	849239.904372	44.283367
3501.360136	849200.913018	44.288372
3501.139289	849182.243439	44.293377
3501.104210	849180.300644	44.298381
3501.370378	849170.514075	44.303386
3500.900368	849180.334144	44.308391
3501.309948	849150.259110	44.313396
3501.274119	849149.777837	44.318401
3501.110204	849136.749526	44.323405
3501.535193	849128.300718	44.328410
3501.340938	849110.893105	44.333415
3501.273621	849084.306280	44.338420
3501.379237	849078.248288	44.343425
3501.169926	849070.780734	44.348429
3501.548302	849054.252931	44.353434
3501.083249	849040.104873	44.358439
3501.224542	849019.913726	44.363444
3501.189371	849024.790946	44.368449
3501.230753	849017.964042	44.373453
3500.984974	849017.517340	44.378458
3500.957516	848989.851826	44.383463
3501.139478	848966.048903	44.388468
3501.420192	848967.464082	44.393473
3501.274255	848951.801810	44.398477
3501.112056	848955.238551	44.403482
3501.107519	848941.891292	44.408487
3501.323661	848917.303110	44.413492
3501.267158	848916.045778	44.418497
3501.455216	848923.906666	44.423501
3501.535879	848898.951005	44.428506
3501.229644	848894.129845	44.433511
3501.222805	848871.721700	44.438516
3501.149347	848868.615949	44.443521
3501.170011	848850.977350	44.448525
3501.549489	848836.202567	44.453530
3501.443702	848815.272001	44.458535
3501.256371	848805.949292	44.463540
3501.673273	848807.634374	44.468545
3501.702082	848767.876955	44.473549
3501.450233	848755.934100	44.478554
3501.295757	848759.564542	44.483559
3501.378285	848721.844084	44.488564
3501.524126	848714.804777	44.493569
3501.482278	848716.273143	44.498573
3501.131431	848693.336417	44.503578
3501.303533	848675.185208	44.508583
3501.135664	848672.874388	44.513588
3501.194772	848666.239051	44.518593
3501.219777	848665.650286	44.523597
3501.493552	848623.805473	44.528602
3501.250398	848623.455744	44.533607
3501.224070	848610.208803	44.538612
3501.406588	848603.650508	44.543617
3501.401843	848593.225614	44.548621
3501.509660	848561.346180	44.553626
3501.086063	848567.651843	44.558631
3501.219109	848553.111858	44.563636
3501.243770	848533.328102	44.568641
3501.253850	848544.434200	44.573645
3501.390007	848525.996170	44.578650
3501.078911	848530.821785	44.583655
3501.451337	848527.544986	44.588660
3501.433933	848493.444781	44.593665
3500.979124	848471.108989	44.598669
3501.362334	848480.010109	44.603674
3501.334320	848472.901729	44.608679
3501.339058	848451.367115	44.613684
3501.275861	848438.905390	44.618689
3501.338126	848419.992028	44.623693
3501.572287	848420.732931	44.628698
3501.456937	848393.761333	44.633703
3501.689203	848364.296376	44.638708
3501.524751	848360.718162	44.643713
3501.473731	848338.607708	44.648717
3501.390537	848320.107763	44.653722
3501.239865	848321.886466	44.658727
3501.184589	848311.274546	44.663732
3501.462402	848285.309567	44.668737
3501.363824	848274.314954	44.673741
3501.528194	848261.523071	44.678746
3501.217367	848251.927553	44.683751
3501.112865	848237.036198	44.688756
3501.221217	848213.145104	44.693761
3501.282156	848227.361524	44.698765
3501.445551	848211.159241	44.703770
3501.266146	848205.634564	44.708775
3501.343292	848174.927522	44.713780
3501.520979	848172.267271	44.718785
3501.392734	848170.047179	44.723789
3501.728189	848130.722427	44.728794
3501.115652	848133.259359	44.733799
3501.275042	848115.303512	44.738804
3501.619440	848102.676541	44.743809
3501.583976	848081.926829	44.748813
3501.451788	848076.881480	44.753818
3501.439061	848075.616767	44.758823
3501.336707	848039.871541	44.763828
3501.318253	848026.914404	44.768833
3501.053144	848029.686486	44.773837
3501.147773	848015.833698	44.778842
3501.467288	848005.549308	44.783847
3501.265099	847978.980010	44.788852
3501.309033	847967.961386	44.793857
3501.394176	847964.244388	44.798861
3501.224834	847947.219218	44.803866
3501.118723	847924.336810	44.808871
3501.313336	847930.248942	44.813876
3501.753977	847918.287872	44.818881
3501.326301	847888.734491	44.823885
3501.752048	847882.720065	44.828890
3501.597272	847866.764195	44.833895
3501.322027	847857.844341	44.838900
3501.142320	847832.245192	44.843905
3501.350009	847817.203971	44.848909
3501.306389	847804.737761	44.853914
3500.859219	847821.669893	44.858919
3501.197598	847791.112843	44.863924
3501.583910	847783.253299	44.868929
3501.428125	847758.234598	44.873933
3501.633038	847751.964076	44.878938
3501.398783	847738.457195	44.883943
3501.522347	847715.633644	44.888948
3501.740324	847712.869115	44.893953
3501.390265	847694.606181	44.898957
3501.552298	847675.089443	44.903962
3501.592300	847666.117391	44.908967
3501.236354	847641.131193	44.913972
3501.526723	847631.825501	44.918977
3501.317523	847625.330709	44.923981
3501.555585	847609.406931	44.928986
3501.367616	847582.638709	44.933991
3501.378342	847574.353509	44.938996
3501.667397	847573.721151	44.944001
3501.409693	847549.303116	44.949005
3501.759507	847533.848000	44.954010
3501.421727	847523.865993	44.959015
3501.257111	847493.000534	44.964020
3501.595518	847485.051057	44.969025
3501.458512	847479.811113	44.974029
3501.378789	847464.036763	44.979034
3501.218879	847440.869092	44.984039
3501.353469	847433.440390	44.989044
3501.360535	847423.693786	44.994049
3501.259357	847413.380270	44.999053
3501.431064	847390.937429	45.004058
3501.300702	847383.942127	45.009063
3501.317684	847373.511628	45.014068
3501.424670	847374.176153	45.019073
3501.364412	847356.936504	45.024077
3501.430439	847336.070156	45.029082
3501.588738	847330.683993	45.034087
3501.269307	847299.745628	45.039092
3501.511388	847281.968695	45.044097
3501.236127	847285.619878	45.049101
3501.458794	847272.816383	45.054106
3501.332190	847252.956052	45.059111
3501.359773	847230.536378	45.064116
3501.286151	847240.878912	45.069121
3501.432231	847214.736298	45.074125
3500.891344	847194.261817	45.079130
3501.178378	847184.468728	45.084135
3501.343172	847178.204244	45.089140
3501.411567	847178.680231	45.094145
3501.355688	847167.189354	45.099149
3501.412048	847142.230714	45.104154
3501.231199	847135.145992	45.109159
3501.162522	847134.085222	45.114164
3501.472265	847121.169619	45.119169
3501.229069	847099.866126	45.124173
3501.383834	847080.933498	45.129178
3501.606816	847085.087487	45.134183
3501.124850	847065.772392	45.139188
3501.381317	847045.750851	45.144193
3501.383153	847034.152764	45.149197
3501.283454	847032.025025	45.154202
3501.217359	847021.022864	45.159207
3501.297493	847007.949928	45.164212
3501.586663	846980.418325	45.169217
3501.154549	846976.493560	45.174221
3501.448564	846972.254269	45.179226
3501.639283	846957.506175	45.184231
3501.223095	846936.620466	45.189236
3501.761572	846936.434275	45.194241
3501.082020	846913.740097	45.199245
3501.388356	846896.536266	45.204250
3501.450057	846895.259056	45.209255
3501.363093	846872.369661	45.214260
3501.419515	846856.278972	45.219265
3501.350556	846843.425177	45.224269
3501.374830	846843.128752	45.229274
3501.124783	846837.419574	45.234279
3501.331459	846799.959517	45.239284
3501.523240	846778.875681	45.244289
3501.146051	846798.625489	45.249293
3501.337178	846773.155869	45.254298
3500.939404	846752.071584	45.259303
3500.911128	846731.511158	45.264308
3501.242432	846732.041340	45.269313
3501.136086	846729.719663	45.274317
3501.209413	846733.313747	45.279322
3501.282309	846736.420576	45.284327
3500.902029	846706.756353	45.289332
3501.170572	846680.493886	45.294337
3501.178301	846688.972079	45.299341
3500.966533	846677.895846	45.304346
3501.007498	846687.343224	45.309351
3501.141353	846678.256840	45.314356
3501.162057	846657.298241	45.319361
3501.333347	846640.700751	45.324365
3501.272199	846639.638657	45.329370
3501.078363	846624.368326	45.334375
3501.037882	846631.100140	45.339380
3501.536789	846605.481682	45.344385
3501.182459	846590.432637	45.349389
3501.302807	846581.933141	45.354394
3501.143272	846572.699995	45.359399
3501.432672	846562.905553	45.364404
3501.448782	846546.138440	45.369409
3501.252740	846535.839108	45.374413
3501.532621	846520.100626	45.379418
3501.175867	846508.560634	45.384423
3501.360876	846488.938968	45.389428
3501.410353	846473.920601	45.394433
3501.114181	846476.016191	45.399437
3501.179612	846468.110400	45.404442
3501.047785	846470.178922	45.409447
3501.357249	846446.930277	45.414452
3501.252408	846433.204330	45.419457
3501.041351	846443.863218	45.424461
3501.423191	846426.645669	45.429466
3501.368115	846407.258233	45.434471
3501.196772	846387.889887	45.439476
3501.503530	846387.644383	45.444481
3501.353896	846370.416751	45.449485
3501.158860	846357.290317	45.454490
3501.404388	846341.946932	45.459495
3501.301076	846339.917023	45.464500
3501.305181	846332.703459	45.469505
3501.125571	846310.217163	45.474509
3501.391270	846291.361362	45.479514
3501.318252	846281.723652	45.484519
3501.248546	846271.792965	45.489524
3501.898113	846264.765425	45.494529
3501.166848	846240.420301	45.499533
3501.142654	846238.767217	45.504538
3501.494954	846229.156844	45.509543
3501.324041	846209.787879	45.514548
3501.539219	846184.214446	45.519553
3501.066873	846187.313880	45.524557
3501.292024	846179.381420	45.529562
3501.093564	846175.027767	45.534567
3501.069000	846159.923374	45.539572
3501.064803	846153.880657	45.544577
3500.927003	846137.625175	45.549581
3501.071134	846146.861424	45.554586
3501.219523	846144.595045	45.559591
3501.191480	846132.805272	45.564596
3501.059392	846111.480127	45.569601
3500.734790	846105.977510	45.574605
3501.063449	846075.316267	45.579610
3501.051015	846091.694055	45.584615
3501.256150	846089.320836	45.589620
3501.415603	846080.229374	45.594625
3501.267264	846064.950190	45.599629
3501.023811	846053.488174	45.604634
3501.213997	846052.092157	45.609639
3501.372943	846047.192170	45.614644
3501.117094	846043.920109	45.619649
3501.118803	846021.597867	45.624653
3501.243276	845999.840182	45.629658
3501.124303	845986.505494	45.634663
3501.028414	845984.961628	45.639668
3501.400311	845987.044816	45.644673
3501.153190	845958.817276	45.649677
3501.320494	845949.236950	45.654682
3501.172712	845943.705066	45.659687
3500.942639	845953.685573	45.664692
3501.151786	845935.617840	45.669697
3501.050120	845949.671242	45.674701
3500.962270	845901.239453	45.679706
3501.081935	845895.565998	45.684711
3501.012785	845894.407617	45.689716
3501.031163	845882.512252	45.694721
3501.137647	845879.375379	45.699725
3501.238819	845877.116683	45.704730
3501.161061	845874.497545	45.709735
3501.139287	845855.980230	45.714740
3501.207967	845837.447961	45.719745
3501.140302	845858.319469	45.724749
3501.261817	845842.020512	45.729754
3501.399418	845834.102039	45.734759
3500.875145	845803.774922	45.739764
3501.298620	845792.397538	45.744769
3501.180275	845791.637159	45.749773
3501.157419	845780.625707	45.754778
3501.001625	845791.958948	45.759783
3501.419069	845776.195955	45.764788
3501.195357	845750.303135	45.769793
3500.723167	845744.044669	45.774797
3501.131149	845741.150509	45.779802
3501.009530	845738.343578	45.784807
3500.855569	845718.385428	45.789812
3500.822125	845637.871487	45.794817
3500.608572	845525.216713	45.799821
3500.899828	845360.419451	45.804826
3500.665625	845131.751605	45.809831
3500.558817	844833.249050	45.814836
3500.570928	844497.468162	45.819841
3500.264219	844089.275677	45.824845
3500.070145	843610.634300	45.829850
3499.839061	843102.365346	45.834855
3499.333799	842513.687929	45.839860
3499.321815	841890.492108	45.844865
3498.782482	841180.405301	45.849869
3498.773412	840444.932318	45.854874
3498.531404	839629.305070	45.859879
3497.987296	838761.902362	45.864884
3498.220657	837814.562672	45.869889
3497.619572	836831.785708	45.874893
3496.816073	835768.247517	45.879898
3496.426764	834648.414667	45.884903
3496.059014	833461.384241	45.889908
3495.482364	832208.964953	45.894913
3494.864794	830908.092770	45.899917
3494.597990	829536.539759	45.904922
3493.842675	828111.701873	45.909927
3493.110074	826599.681340	45.914932
3492.268304	825046.012755	45.919937
3491.486175	823421.392618	45.924941
3491.000465	821739.673581	45.929946
3490.163299	819997.446193	45.934951
3489.640044	818192.792924	45.939956
3488.767220	816320.388724	45.944961
3487.765715	814395.031006	45.949965
3487.031022	812390.304170	45.954970
3486.194813	810334.966644	45.959975
3484.960677	808221.328078	45.964980
3484.537379	806027.709800	45.969985
3483.457884	803792.589422	45.974989
3482.386914	801486.281953	45.979994
3481.536643	799124.686811	45.984999
3480.125719	796706.555012	45.990004
3479.228028	794206.604985	45.995009
3478.248770	791686.617287	46.000013
3477.072994	789071.536195	46.005018
3476.344612	786410.181887	46.010023
3474.742875	783678.130774	46.015028
3473.713837	780898.740794	46.020033
3472.638976	778052.669908	46.025037
3471.335424	775153.618025	46.030042
3470.036184	772197.944358	46.035047
3468.549554	769172.509887	46.040052
3467.744234	766096.029901	46.045057
3466.132797	762969.139861	46.050061
3464.585473	759775.505630	46.055066
3463.334188	756509.485462	46.060071
3461.675633	753209.343678	46.065076
3460.297903	749841.135086	46.070081
3458.489440	746434.166453	46.075085
3457.228644	742962.767713	46.080090
3455.662953	739426.611610	46.085095
3453.936954	735864.114031	46.090100
3452.506353	732213.076051	46.095105
3450.884769	728537.239374	46.100109
3449.260461	724781.632649	46.105114
3447.667718	720988.260718	46.110119
3445.971126	717134.337996	46.115124
3444.013499	713213.470816	46.120129
3442.420442	709255.228049	46.125133
3440.443553	705234.411163	46.130138
3438.831030	701170.811193	46.135143
3436.829258	697042.134393	46.140148
3435.413676	692849.592541	46.145153
3433.333225	688622.293851	46.150157
3431.364751	684342.404788	46.155162
3429.407340	679989.114690	46.160167
3427.420446	675611.001454	46.165172
3425.542676	671168.983412	46.170177
3423.553462	666685.684241	46.175181
3421.097466	662130.431335	46.180186
3419.218813	657543.979969	46.185191
3417.048501	652914.566042	46.190196
3415.197487	648227.210932	46.195201
3412.896057	643492.342246	46.200205
3410.730743	638696.318061	46.205210
3408.661117	633851.555537	46.210215
3406.294373	628977.565361	46.215220
3404.309533	624038.303882	46.220225
3401.773283	619049.909503	46.225229
3399.290092	614040.133084	46.230234
3397.572128	608958.541230	46.235239
3394.965211	603843.644292	46.240244
3392.951499	598660.591045	46.245249
3390.359898	593465.739376	46.250253
3387.770368	588191.717377	46.255258
3385.511946	582902.467325	46.260263
3383.055640	577545.428443	46.265268
3380.764536	572160.605025	46.270273
3378.099045	566714.007917	46.275277
3375.597357	561234.274161	46.280282
3372.740989	555717.309868	46.285287
3370.134456	550164.728455	46.290292
3367.677212	544563.891073	46.295297
3365.026095	538935.830204	46.300301
3362.593210	533233.455331	46.305306
3359.823962	527513.367561	46.310311
3356.965259	521755.604410	46.315316
3354.549491	515946.089549	46.320321
3351.541072	510114.303753	46.325325
3348.745340	504225.555870	46.330330
3346.167783	498304.520667	46.335335
3343.061115	492345.066662	46.340340
3340.489147	486345.666711	46.345345
3337.553472	480332.762917	46.350349
3334.330069	474261.863781	46.355354
3331.390558	468170.166405	46.360359
3328.064308	462054.930623	46.365364
3325.863738	455878.123528	46.370369
3322.762200	449708.849434	46.375373
3319.873715	443480.538905	46.380378
3316.815475	437222.391028	46.385383
3313.374972	430946.253084	46.390388
3310.564932	424618.803902	46.395393
3307.120593	418269.525335	46.400397
3304.337354	411894.137510	46.405402
3300.861790	405496.491260	46.410407
3297.340646	399062.885733	46.415412
3294.184877	392622.724546	46.420417
3291.031813	386149.313019	46.425421
3287.908338	379646.939560	46.430426
3284.436483	373131.534333	46.435431
3280.798491	366576.474824	46.440436
3277.772543	359989.745216	46.445441
3274.313984	353410.752064	46.450445
3270.996826	346792.656027	46.455450
3267.493091	340162.337255	46.460455
3263.657547	333520.548242	46.465460
3260.536641	326844.860782	46.470465
3256.545716	320169.837308	46.475469
3253.405872	313475.536336	46.480474
3249.567036	306768.163160	46.485479
3245.910340	300037.941777	46.490484
3242.463475	293302.329934	46.495489
3238.740562	286547.577028	46.500493
3234.985194	279785.353956	46.505498
3231.420167	273004.696700	46.510503
3227.600986	266226.204183	46.515508
3223.861009	259433.801747	46.520513
3220.244709	252640.470803	46.525517
3216.083701	245822.433083	46.530522
3212.131640	239016.875810	46.535527
3208.299586	232192.413808	46.540532
3204.254389	225380.528833	46.545537
3200.626522	218568.766463	46.550541
3196.514458	211679.925794	46.555546
3192.475683	204821.053788	46.560551
3188.581465	198002.647006	46.565556
3184.791273	191171.160272	46.570561
3180.016207	184355.067335	46.575565
3175.655392	177535.417322	46.580570
3171.793799	170730.098719	46.585575
3166.975647	163922.963575	46.590580
3162.773624	157136.888438	46.595585
3158.217916	150377.096943	46.600589
3153.781528	143612.248926	46.605594
3149.529232	136858.898702	46.610599
3144.983345	130147.782197	46.615604
3140.212126	123428.752187	46.620609
3135.353744	116730.674978	46.625613
3130.546539	110072.382832	46.630618
3126.016942	103427.926986	46.635623
3120.841675	96822.190598	46.640628
3115.788297	90237.362808	46.645633
3110.530756	83698.352523	46.650637
3105.290719	77193.234506	46.655642
3099.793281	70728.769460	46.660647
3093.690889	64317.518500	46.665652
3087.361714	57956.396904	46.670657
3078.105197	51731.115436	46.675661
3060.745834	45837.222537	46.680666
3042.026072	40118.509034	46.685671
3023.939233	34673.631450	46.690676
3007.025170	29471.512582	46.695681
2990.604270	24578.080154	46.700685
2974.878644	19982.437105	46.705690
2959.646029	15679.460099	46.710695
2945.051754	11715.176542	46.715700
2930.835678	8024.593878	46.720705
2916.484449	4650.353016	46.725709
2901.415923	1619.567136	46.730714
2836.684419	278.202933	46.735719
2747.537867	294.125411	46.740724
2703.114107	281.924264	46.745729
2699.070169	294.497255	46.750733
2719.474492	293.103777	46.755738
2748.609060	275.111540	46.760743
2773.333691	288.137013	46.765748
2789.146483	270.220703	46.770753
2794.694956	264.515546	46.775757
2792.730365	281.415333	46.780762
2788.337910	282.985242	46.785767
2782.979218	284.015052	46.790772
2778.309757	269.567125	46.795777
2774.534117	253.065566	46.800781
2771.652986	255.478085	46.805786
2769.306777	257.898116	46.810791
2766.722335	274.218451	46.815796
2764.524399	261.272038	46.820801
2762.293495	262.790260	46.825805
2759.072679	256.577272	46.830810
2756.603844	246.524813	46.835815
2753.152537	265.027734	46.840820
2749.594643	246.620906	46.845825
2746.584044	262.818613	46.850829
2743.708706	257.429405	46.855834
2740.726680	252.001160	46.860839
2737.008767	253.162034	46.865844
2734.345889	244.483143	46.870849
2731.231888	255.814568	46.875853
2727.416779	253.789293	46.880858
2724.529749	248.355556	46.885863
2721.367272	249.640433	46.890868
2718.096321	249.744489	46.895873
2714.591726	245.203228	46.900877
2710.957184	253.230357	46.905882
2708.174644	238.806858	46.910887
2704.321429	243.656419	46.915892
2701.247331	226.672559	46.920897
2697.971366	235.796650	46.925901
2694.979334	234.136486	46.930906
2691.387349	237.799327	46.935911
2687.585696	237.973530	46.940916
2684.491228	234.636975	46.945921
2681.335803	242.320217	46.950925
2677.833436	234.074856	46.955930
2674.549485	239.943149	46.960935
2670.679059	234.994882	46.965940
2667.574942	246.136052	46.970945
2663.897196	227.100679	46.975949
2660.774991	234.882039	46.980954
2657.536577	241.646546	46.985959
2653.639575	233.014899	46.990964
2651.031132	228.828884	46.995969
2647.656641	239.550345	47.000973
2643.874463	231.987981	47.005978
2640.580628	232.305591	47.010983
2637.133259	231.981287	47.015988
2633.138023	231.839464	47.020993
2629.805296	235.005952	47.025997
2626.206284	231.806282	47.031002
2623.174867	223.636819	47.036007
2619.420603	228.309482	47.041012
2616.160155	233.238534	47.046017
2612.915905	242.133669	47.051021
2609.161760	225.833226	47.056026
2606.070954	220.335971	47.061031
2601.797497	222.698615	47.066036
2598.379551	217.571605	47.071041
2595.337314	220.298531	47.076045
2591.988937	232.111403	47.081050
2588.820652	224.778852	47.086055
2585.364047	230.158670	47.091060
2582.343839	217.213777	47.096065
2578.566300	215.993068	47.101069
2574.880072	221.980405	47.106074
2571.118001	211.782464	47.111079
2567.249027	231.174310	47.116084
2564.537110	213.249506	47.121089
2561.162476	220.616711	47.126093
2557.394124	227.633684	47.131098
2554.332485	221.525977	47.136103
2550.327589	211.230164	47.141108
2546.876643	221.001738	47.146113
2543.903293	201.180142	47.151117
2539.825202	217.901342	47.156122
2536.731387	215.358655	47.161127
2532.851440	219.885443	47.166132
2529.776162	227.298308	47.171137
2526.028592	210.417628	47.176141
2522.534179	219.567428	47.181146
2519.377350	216.315918	47.186151
2515.778381	212.129814	47.191156
2512.258395	211.707932	47.196161
2509.075169	214.046533	47.201165
2505.279817	212.011609	47.206170
2502.257129	213.207222	47.211175
2498.540708	222.626377	47.216180
2494.900430	218.409209	47.221185
2491.469225	213.082683	47.226189
2487.752186	221.684951	47.231194
2484.638741	220.383688	47.236199
2480.740099	231.210769	47.241204
2477.621515	219.168699	47.246209
2473.915415	212.002147	47.251213
2469.965893	217.118575	47.256218
2467.219116	207.394558	47.261223
2463.609784	209.156439	47.266228
2460.157970	209.857617	47.271233
2456.811994	208.753848	47.276237
2453.131781	205.997714	47.281242
2449.776468	193.239092	47.286247
2446.082049	214.360557	47.291252
2442.423983	202.971907	47.296257
2439.381092	200.484601	47.301261
2435.272961	213.629387	47.306266
2432.109813	193.428057	47.311271
2428.535312	213.329571	47.316276
2425.063977	195.244382	47.321281
2422.043393	196.853254	47.326285
2418.255176	205.051829	47.331290
2415.219978	204.113187	47.336295
2411.480429	212.711103	47.341300
2407.451184	195.372134	47.346305
2404.272717	200.642118	47.351309
2400.768534	207.255086	47.356314
2397.688329	203.504906	47.361319
2393.946695	206.350990	47.366324
2390.276855	208.414715	47.371329
2386.911016	206.008904	47.376333
2383.266581	208.031938	47.381338
2379.956857	200.549584	47.386343
2375.907717	211.282036	47.391348
2372.833873	194.193390	47.396353
2369.355588	198.588400	47.401357
2365.571765	213.930919	47.406362
2362.309317	207.733692	47.411367
2358.997339	212.110656	47.416372
2355.498082	206.799864	47.421377
2351.959916	192.309712	47.426381
2348.322843	213.497020	47.431386
2345.193890	193.160173	47.436391
2341.715711	196.954742	47.441396
2338.230718	202.412239	47.446401
2334.320111	192.486781	47.451405
2330.409698	192.665975	47.456410
2327.480176	204.161016	47.461415
2323.558196	194.035288	47.466420
2320.444594	192.704230	47.471425
2317.445713	193.591033	47.476429
2313.609590	195.080992	47.481434
2310.155152	190.908557	47.486439
2306.229723	197.696792	47.491444
2302.844993	198.690745	47.496449
2299.373050	190.804646	47.501453
2296.167939	198.306370	47.506458
2292.599442	198.531996	47.511463
2288.838697	196.358094	47.516468
2285.635158	187.947667	47.521473
2282.265544	186.073115	47.526477
2278.733707	197.544079	47.531482
2275.154717	181.937691	47.536487
2271.565139	190.681695	47.541492
2267.995599	181.126238	47.546497
2264.576327	189.849457	47.551501
2260.926388	194.583497	47.556506
2257.616733	190.025627	47.561511
2253.983708	179.853183	47.566516
2250.358188	178.544334	47.571521
2246.941895	185.691890	47.576525
2243.352177	184.549396	47.581530
2240.218899	176.322852	47.586535
2236.186125	179.656250	47.591540
2232.694324	186.518318	47.596545
2229.444666	182.882395	47.601549
2226.003091	179.967353	47.606554
2223.007570	183.493138	47.611559
2219.330773	185.129220	47.616564
2216.162105	181.988726	47.621569
2212.483976	182.583399	47.626573
2208.547117	192.664006	47.631578
2204.987053	178.753734	47.636583
2201.253973	189.912312	47.641588
2197.803563	179.484941	47.646593
2194.713324	177.079153	47.651597
2190.855304	184.090925	47.656602
2187.383074	177.756241	47.661607
2183.916718	188.861855	47.666612
2180.532960	182.050269	47.671617
2177.287789	176.974112	47.676621
2173.662206	182.672695	47.681626
2170.342412	181.017682	47.686631
2166.792470	180.429338	47.691636
2162.969765	173.849104	47.696641
2159.476045	186.662864	47.701645
2156.030213	175.699544	47.706650
2152.710311	184.432456	47.711655
2149.449224	177.101347	47.716660
2145.749270	192.755558	47.721665
2142.303599	181.356640	47.726669
2138.651781	180.392061	47.731674
2135.178171	169.812581	47.736679
2131.284746	183.558888	47.741684
2127.509110	175.461935	47.746689
2124.908232	174.657874	47.751693
2121.049987	183.962525	47.756698
2117.600876	173.846848	47.761703
2114.354657	184.435017	47.766708
2110.613192	184.711754	47.771713
2107.388793	178.797657	47.776717
2103.830642	191.638839	47.781722
2100.382699	175.249216	47.786727
2096.629008	176.502521	47.791732
2092.795596	183.275668	47.796737
2089.868490	182.767734	47.801741
2086.077304	190.726500	47.806746
2082.758335	181.045762	47.811751
2078.692910	168.910923	47.816756
2075.496541	187.739867	47.821761
2072.268560	181.666847	47.826765
2068.535741	180.030682	47.831770
2065.196312	167.613509	47.836775
2061.507039	173.219052	47.841780
2058.009111	180.497054	47.846785
2054.465001	171.668884	47.851789
2050.831092	172.117530	47.856794
2047.863313	180.570511	47.861799
2044.609821	171.412147	47.866804
2040.752533	180.170305	47.871809
2037.191284	167.715351	47.876813
2033.792403	171.449116	47.881818
2030.407764	178.445024	47.886823
2026.708792	185.871930	47.891828
2022.853220	176.908197	47.896833
2019.313549	174.044069	47.901837
2015.821620	181.602767	47.906842
2012.577058	168.288467	47.911847
2008.850471	171.521450	47.916852
2005.223084	185.757758	47.921857
2001.893359	160.850424	47.926861
1998.684730	178.455081	47.931866
1995.403895	171.487907	47.936871
1991.971022	171.418121	47.941876
1988.186682	173.225072	47.946881
1984.806723	166.884258	47.951885
1981.075043	167.941211	47.956890
1977.569313	168.474706	47.961895
1974.104734	161.275232	47.966900
1970.351477	161.232757	47.971905
1967.546370	173.908999	47.976909
1963.525496	171.596459	47.981914
1959.836690	174.227044	47.986919
1956.694607	168.393271	47.991924
1953.170032	177.650245	47.996929
1949.871169	175.077917	48.001933
1946.302518	171.232820	48.006938
1942.402427	164.039207	48.011943
1938.984948	192.238670	48.016948
1935.458227	178.321687	48.021953
1932.434578	177.205338	48.026957
1928.415405	180.547106	48.031962
1925.070867	173.710642	48.036967
1921.955031	178.689586	48.041972
1917.931923	175.820912	48.046977
1914.506816	177.207252	48.051981
1910.976195	183.618672	48.056986
1907.816501	173.616181	48.061991
1903.914672	183.688173	48.066996
1900.415813	178.414464	48.072001
1897.253777	172.643205	48.077005
1893.581542	179.319310	48.082010
1890.309654	166.481570	48.087015
1886.587023	165.039263	48.092020
1883.071648	173.057774	48.097025
1879.844519	166.868696	48.102029
1875.869617	165.109492	48.107034
1872.394883	158.175168	48.112039
1869.461022	172.371875	48.117044
1866.022140	157.770381	48.122049
1862.073576	169.636781	48.127053
1857.980284	173.505509	48.132058
1854.786833	159.892922	48.137063
1851.373325	165.894848	48.142068
1847.872201	164.472745	48.147073
1844.623961	164.494310	48.152077
1840.845963	157.785055	48.157082
1837.788686	176.570276	48.162087
1834.193287	167.255832	48.167092
1830.614221	169.698484	48.172097
1827.310039	163.566740	48.177101
1823.635727	168.099582	48.182106
1819.820273	173.241740	48.187111
1816.354774	169.092107	48.192116
1813.097864	176.349777	48.197121
1809.938234	161.490128	48.202125
1806.001035	174.019828	48.207130
1802.796568	167.711917	48.212135
1798.900096	167.313129	48.217140
1795.204933	165.516005	48.222145
1792.174315	165.123337	48.227149
1788.342431	175.079750	48.232154
1784.729875	164.284850	48.237159
1781.397954	172.162440	48.242164
1778.118256	168.540671	48.247169
1775.024154	157.557935	48.252173
1770.973179	170.658901	48.257178
1767.765816	156.085766	48.262183
1763.818987	162.792232	48.267188
1760.277167	179.015274	48.272193
1756.903405	157.452680	48.277197
1753.580107	166.648792	48.282202
1750.113730	166.574684	48.287207
1746.937906	167.072896	48.292212
1742.987424	161.255607	48.297217
1739.566474	167.264036	48.302221
1736.094244	167.856739	48.307226
1732.648598	158.611475	48.312231
1728.849468	156.753899	48.317236
1725.227539	170.832426	48.322241
1722.119568	163.983581	48.327245
1718.334075	165.541253	48.332250
1715.001963	160.206101	48.337255
1711.366159	166.924316	48.342260
1707.864803	158.567691	48.347265
1704.830190	157.855872	48.352269
1701.108070	162.751233	48.357274
1697.709172	157.476933	48.362279
1694.302514	164.541219	48.367284
1690.419124	164.547393	48.372289
1686.838506	157.918624	48.377293
1683.052798	168.736827	48.382298
1679.584185	155.614695	48.387303
1676.129839	165.467615	48.392308
1673.159306	159.707790	48.397313
1669.634785	161.358769	48.402317
1665.857706	162.469247	48.407322
1662.291191	160.396036	48.412327
1659.056575	150.902306	48.417332
1655.378942	167.216643	48.422337
1652.168374	154.294352	48.427341
1648.562290	165.454372	48.432346
1644.741099	149.782143	48.437351
1641.206939	150.078879	48.442356
1637.655349	156.622808	48.447361
1634.218588	143.390686	48.452365
1630.733660	155.626993	48.457370
1627.644869	150.520383	48.462375
1623.902606	151.135304	48.467380
1620.486097	138.824173	48.472385
1617.097564	148.563542	48.477389
1613.337526	153.846705	48.482394
1609.824758	145.915564	48.487399
1606.652864	153.001815	48.492404
1602.765009	167.972323	48.497409
1599.579409	146.400115	48.502413
1595.836469	148.773629	48.507418
1592.338075	148.534895	48.512423
1588.981683	152.678662	48.517428
1585.242474	145.232411	48.522433
1582.170602	151.067076	48.527437
1578.085342	147.064540	48.532442
1574.720985	147.846108	48.537447
1571.132764	154.169001	48.542452
1567.564401	156.725143	48.547457
1564.653752	143.695606	48.552461
1560.901551	150.762011	48.557466
1557.444803	147.634053	48.562471
1554.073824	151.080171	48.567476
1550.154180	150.032432	48.572481
1546.860229	143.815297	48.577485
1543.333958	142.740630	48.582490
1539.950550	134.877472	48.587495
1536.457554	142.354635	48.592500
1532.876454	147.499191	48.597505
1529.265537	139.090123	48.602509
1525.684082	146.519441	48.607514
1522.188742	148.970223	48.612519
1518.738799	138.684085	48.617524
1515.557344	144.149233	48.622529
1512.042195	149.748773	48.627533
1508.242128	154.588026	48.632538
1504.994241	165.352370	48.637543
1501.184504	153.165783	48.642548
1497.400123	150.986056	48.647553
1494.567521	143.927923	48.652557
1490.712971	145.814981	48.657562
1487.618794	151.998663	48.662567
1484.024247	142.927889	48.667572
1480.234944	151.572850	48.672577
1476.788493	137.396408	48.677581
1473.345977	143.233480	48.682586
1469.509832	134.487119	48.687591
1466.472896	135.818581	48.692596
1463.164194	141.937042	48.697601
1459.594501	130.351269	48.702605
1455.265274	131.239350	48.707610
1451.992642	134.846270	48.712615
1448.644055	138.013286	48.717620
1444.781329	133.876834	48.722625
1441.772123	139.952879	48.727629
1438.041474	139.991007	48.732634
1434.815623	132.249399	48.737639
1431.525720	136.809245	48.742644
1427.893744	141.753879	48.747649
1424.402834	132.784037	48.752653
1420.879160	137.251847	48.757658
1417.242886	144.700617	48.762663
1413.931975	137.888396	48.767668
1410.024469	135.116776	48.772673
1406.492204	139.379127	48.777677
1403.038650	147.225722	48.782682
1399.573326	154.210423	48.787687
1396.387636	142.105705	48.792692
1392.570682	143.762954	48.797697
1389.501615	146.626962	48.802701
1385.861399	143.357022	48.807706
1382.575112	141.410855	48.812711
1378.842323	140.161106	48.817716
1375.127717	145.935691	48.822721
1371.678364	136.619541	48.827725
1367.927436	155.976507	48.832730
1364.566901	151.390996	48.837735
1361.406898	135.376137	48.842740
1357.530593	140.737013	48.847745
1354.173376	136.245380	48.852749
1350.731079	137.577794	48.857754
1347.150552	136.626329	48.862759
1343.836699	142.690737	48.867764
1340.229112	143.927019	48.872769
1336.855940	138.896993	48.877773
1333.233598	146.809557	48.882778
1329.503796	134.910811	48.887783
1325.949036	146.796283	48.892788
1322.400361	146.840446	48.897793
1319.453236	139.890094	48.902797
1315.611867	141.725543	48.907802
1312.344457	147.525891	48.912807
1309.079529	142.912202	48.917812
1304.934764	138.360868	48.922817
1301.765723	144.251729	48.927821
1298.004367	133.330872	48.932826
1294.681461	135.248866	48.937831
1291.139668	131.762858	48.942836
1287.735851	128.196167	48.947841
1284.424661	135.934659	48.952845
1280.485454	139.316936	48.957850
1277.126037	139.905645	48.962855
1273.345006	132.147242	48.967860
1269.531822	139.358607	48.972865
1266.556434	137.089084	48.977869
1263.081345	132.757839	48.982874
1259.807821	148.177366	48.987879
1256.720036	135.555596	48.992884
1252.801834	143.847727	48.997889
1249.100588	139.427537	49.002893
1245.308624	145.780355	49.007898
1241.874395	139.243118	49.012903
1238.574868	129.978088	49.017908
1234.937971	151.454555	49.022913
1231.940156	125.635040	49.027917
1228.179967	134.157602	49.032922
1224.622678	142.706168	49.037927
1221.158194	139.616466	49.042932
1217.602902	133.960995	49.047937
1213.728738	140.078090	49.052941
1210.578606	132.169609	49.057946
1207.219576	135.645574	49.062951
1203.805194	130.177584	49.067956
1199.710317	144.633082	49.072961
1196.328167	140.293633	49.077965
1192.928658	142.135627	49.082970
1189.454117	142.078830	49.087975
1186.464721	135.336982	49.092980
1182.646324	133.572674	49.097985
1178.829723	129.535713	49.102989
1175.373762	142.342957	49.107994
1171.746606	145.427140	49.112999
1168.345505	138.535132	49.118004
1164.957712	146.070953	49.123009
1161.646633	142.553341	49.128013
1158.204343	139.812115	49.133018
1154.421014	147.453784	49.138023
1151.211166	136.036698	49.143028
1147.221691	139.110657	49.148033
1143.878606	139.522309	49.153037
1140.332517	140.752486	49.158042
1136.910978	145.866245	49.163047
1133.477543	137.987109	49.168052
1129.977011	141.086911	49.173057
1126.688918	137.110617	49.178061
1122.769411	129.813108	49.183066
1119.285713	133.716060	49.188071
1116.234525	135.654196	49.193076
1112.627659	128.141312	49.198081
1109.073520	143.173117	49.203085
1105.644017	129.045527	49.208090
1101.993381	135.261427	49.213095
1098.649517	141.854165	49.218100
1094.796504	137.400224	49.223105
1091.889927	121.171852	49.228109
1088.050909	130.697705	49.233114
1084.303233	136.653790	49.238119
1080.499537	131.239781	49.243124
1077.036304	128.023573	49.248129
1074.024137	134.494078	49.253133
1070.733171	127.173637	49.258138
1066.947369	128.607096	49.263143
1063.537132	122.305940	49.268148
1059.833373	147.335556	49.273153
1056.356294	128.846746	49.278157
1052.761025	143.322034	49.283162
1049.526411	137.002243	49.288167
1046.213119	132.307791	49.293172
1042.399361	134.104002	49.298177
1038.728427	122.262534	49.303181
1035.503538	134.629945	49.308186
1031.808982	143.249992	49.313191
1028.294355	134.894987	49.318196
1024.720936	130.768149	49.323201
1021.360247	139.133791	49.328205
1017.795924	131.860777	49.333210
1014.001375	139.639028	49.338215
1010.903239	134.561405	49.343220
1007.302511	137.732661	49.348225
1004.168482	139.616942	49.353229
1000.949338	130.785595	49.358234
997.185643	138.532713	49.363239
993.527704	123.679513	49.368244
989.747664	136.081772	49.373249
986.154802	134.250547	49.378253
982.525748	136.566009	49.383258
979.141738	138.073962	49.388263
975.927693	131.036546	49.393268
972.122582	122.231822	49.398273
968.715629	131.247077	49.403277
965.366112	136.508447	49.408282
962.136934	129.230744	49.413287
958.682588	128.949939	49.418292
954.861464	127.516121	49.423297
951.413673	128.419001	49.428301
947.999568	130.782651	49.433306
944.018243	130.493462	49.438311
940.880110	131.197433	49.443316
937.258352	130.304197	49.448321
933.988398	125.844852	49.453325
930.328765	122.797399	49.458330
926.692536	118.691646	49.463335
923.420665	127.854401	49.468340
919.416033	123.206195	49.473345
916.180094	129.237392	49.478349
912.655137	125.195256	49.483354
909.272611	128.128383	49.488359
906.470454	121.008400	49.493364
902.434568	123.624004	49.498369
898.760712	112.864689	49.503373
894.954458	134.958375	49.508378
891.291393	132.919185	49.513383
888.458889	125.613023	49.518388
885.014312	136.626497	49.523393
881.485075	126.260423	49.528397
877.815239	129.467719	49.533402
874.146565	132.153130	49.538407
870.733196	127.385028	49.543412
867.081265	125.110002	49.548417
863.580206	125.777350	49.553421
859.714937	130.841376	49.558426
856.289764	137.505355	49.563431
853.436915	130.348185	49.568436
849.832733	124.182172	49.573441
846.388561	128.862747	49.578445
842.561679	127.429847	49.583450
839.072771	137.343836	49.588455
835.916595	125.360872	49.593460
832.366825	140.106937	49.598465
828.782120	126.393768	49.603469
825.289783	134.079386	49.608474
821.646986	127.911675	49.613479
818.250744	128.071319	49.618484
814.208400	137.835294	49.623489
811.188212	131.838253	49.628493
807.578798	135.900823	49.633498
804.461348	134.001750	49.638503
801.112428	123.011056	49.643508
797.197419	126.316493	49.648513
793.378165	130.353640	49.653517
790.183210	124.933112	49.658522
786.661048	131.770492	49.663527
783.409112	127.875230	49.668532
779.501137	135.060555	49.673537
775.750407	110.939194	49.678541
772.556558	128.192640	49.683546
768.878987	137.191995	49.688551
766.093842	116.566988	49.693556
761.999033	123.810793	49.698561
758.794010	123.327517	49.703565
755.376678	124.994984	49.708570
751.497789	124.607603	49.713575
748.090706	116.567295	49.718580
744.201631	135.063205	49.723585
741.052058	123.725408	49.728589
737.841542	118.395088	49.733594
734.022258	124.796661	49.738599
731.020779	126.679793	49.743604
727.278772	129.841075	49.748609
723.607640	115.512735	49.753613
719.815579	126.592236	49.758618
716.263112	126.007424	49.763623
713.343404	116.634309	49.768628
709.544055	123.898112	49.773633
706.088568	121.181906	49.778637
702.954841	121.139517	49.783642
699.261332	122.948516	49.788647
695.440086	121.464063	49.793652
692.070734	134.743948	49.798657
688.580877	125.122170	49.803661
684.928527	126.312020	49.808666
681.369506	146.514076	49.813671
678.284534	132.959392	49.818676
674.650729	136.619693	49.823681
670.989992	131.931129	49.828685
667.526135	136.517174	49.833690
663.703527	132.413939	49.838695
660.533267	133.874118	49.843700
657.037604	124.109578	49.848705
653.728706	122.114932	49.853709
650.245651	126.408086	49.858714
646.362697	123.953311	49.863719
643.267107	116.730781	49.868724
639.626906	136.647910	49.873729
636.070582	124.598659	49.878733
632.404391	123.991437	49.883738
628.910316	124.688436	49.888743
625.555358	119.100961	49.893748
621.848916	119.849809	49.898753
618.241984	123.633260	49.903757
614.968866	129.655728	49.908762
611.583043	121.675720	49.913767
608.061191	120.490720	49.918772
604.628578	116.771802	49.923777
601.449367	128.659846	49.928781
597.960582	116.387659	49.933786
594.158237	128.557289	49.938791
590.703878	118.397268	49.943796
586.423269	131.939965	49.948801
583.097834	129.097376	49.953805
579.854830	124.889291	49.958810
576.236154	121.431678	49.963815
572.988056	117.946997	49.968820
569.355704	118.965004	49.973825
566.165205	115.377879	49.978829
562.408355	122.678243	49.983834
558.774356	119.340671	49.988839
555.521225	129.581943	49.993844
551.632492	121.090338	49.998849
548.396532	121.187045	50.003853
544.979102	121.703122	50.008858
541.339671	121.405158	50.013863
538.074266	113.342860	50.018868
534.432686	119.082897	50.023873
531.044384	115.851955	50.028877
527.483368	112.917690	50.033882
524.190618	114.405661	50.038887
520.422816	118.447376	50.043892
516.584391	114.863709	50.048897
513.145703	109.881574	50.053901
509.774631	121.143696	50.058906
506.563518	118.044013	50.063911
503.198467	111.751113	50.068916
499.444938	124.277845	50.073921
495.408887	108.902834	50.078925
492.510676	116.966668	50.083930
488.913959	117.575429	50.088935
485.561260	116.109010	50.093940
481.680729	118.395140	50.098945
478.202331	113.293402	50.103949
475.239687	109.813221	50.108954
471.673166	112.840779	50.113959
467.785086	100.843600	50.118964
464.021064	106.486196	50.123969
460.594143	115.649384	50.128973
457.256314	119.664603	50.133978
454.056078	107.663810	50.138983
450.421585	111.147445	50.143988
446.734656	111.761166	50.148993
443.376267	127.210739	50.153997
439.866947	109.765879	50.159002
436.070651	119.241865	50.164007
432.634304	121.496480	50.169012
429.155488	116.959545	50.174017
425.923503	114.574957	50.179021
422.416697	109.526189	50.184026
418.701662	127.772382	50.189031
415.681483	111.776790	50.194036
411.730586	116.724871	50.199041
408.368490	114.882194	50.204045
405.078175	117.464703	50.209050
401.433667	115.994936	50.214055
397.794156	109.309505	50.219060
394.033611	125.458995	50.224065
390.564753	118.537703	50.229069
387.267339	116.431103	50.234074
383.938238	112.925869	50.239079
380.318881	113.964425	50.244084
377.055159	109.980373	50.249089
373.125194	124.824132	50.254093
369.370273	108.689202	50.259098
366.127985	123.010729	50.264103
362.635063	104.237784	50.269108
359.237797	117.565995	50.274113
355.687742	109.252200	50.279117
352.661604	108.149318	50.284122
348.527055	105.871157	50.289127
345.348190	113.157533	50.294132
341.519327	112.282962	50.299137
338.113776	105.917632	50.304141
334.988139	105.974614	50.309146
331.237697	119.149665	50.314151
327.465965	120.964686	50.319156
323.971372	121.908078	50.324161
320.509303	120.296836	50.329165
317.121556	111.545744	50.334170
313.449505	119.888330	50.339175
310.419580	95.024997	50.344180
306.789127	112.713944	50.349185
303.451856	108.993261	50.354189
300.152765	115.843829	50.359194
296.638229	107.638448	50.364199
292.867980	112.531592	50.369204
289.143993	125.668655	50.374209
285.274897	123.209942	50.379213
282.261984	112.927271	50.384218
278.408878	110.421626	50.389223
275.177835	107.478968	50.394228
271.441984	125.460013	50.399233
267.966047	122.242609	50.404237
264.656494	110.249141	50.409242
261.092199	123.346513	50.414247
258.022738	108.119309	50.419252
254.140650	119.731244	50.424257
250.710046	123.371410	50.429261
246.987908	114.694647	50.434266
243.502795	125.509868	50.439271
239.976205	125.239701	50.444276
236.636411	120.971832	50.449281
233.527294	120.875585	50.454285
230.083058	125.067032	50.459290
226.046971	124.320194	50.464295
222.584779	114.148783	50.469300
218.802042	118.143800	50.474305
215.534577	115.010766	50.479309
212.516077	110.626295	50.484314
208.582802	122.577502	50.489319
205.053198	119.691705	50.494324
201.460527	117.715576	50.499329
197.906627	116.455596	50.504333
194.907009	128.611560	50.509338
190.989436	121.223796	50.514343
187.555424	110.291461	50.519348
184.075830	109.189492	50.524353
180.506535	125.116769	50.529357
177.417098	103.479919	50.534362
173.468151	120.006805	50.539367
170.108396	113.543933	50.544372
166.356085	116.936790	50.549377
162.964857	117.225776	50.554381
159.866330	113.365294	50.559386
156.152756	124.440867	50.564391
152.877627	115.635455	50.569396
148.987252	120.843606	50.574401
145.521387	123.758811	50.579405
142.136373	113.679868	50.584410
138.212800	123.319786	50.589415
135.067712	124.364365	50.594420
131.489263	125.125786	50.599425
127.988738	119.236892	50.604429
124.556035	118.809311	50.609434
120.880090	116.153244	50.614439
117.388185	116.995378	50.619444
113.730380	106.864849	50.624449
110.254402	112.500190	50.629453
107.169883	105.798911	50.634458
103.639152	112.333371	50.639463
100.429461	103.834955	50.644468
96.691483	110.203392	50.649473
93.170544	118.496451	50.654477
89.434366	108.992328	50.659482
85.898516	116.516664	50.664487
82.325855	110.744098	50.669492
79.347451	109.196813	50.674497
75.467629	104.518487	50.679501
71.993286	103.464351	50.684506
68.063015	108.534803	50.689511
64.621791	97.066474	50.694516
61.345270	100.430487	50.699521
57.677991	117.681080	50.704525
54.899026	104.070227	50.709530
51.075325	116.910536	50.714535
47.453427	109.414235	50.719540
43.951415	113.238456	50.724545
40.364973	112.498728	50.729549
37.019108	105.949688	50.734554
33.483140	122.668943	50.739559
29.532137	113.357023	50.744564
26.427395	111.837250	50.749569
23.018047	114.253649	50.754573
19.682971	118.978053	50.759578
15.745557	110.609510	50.764583
12.138344	112.625713	50.769588
8.886876	117.202824	50.774593
5.292944	113.024342	50.779597
2.084147	110.193976	50.784602