Wed Jun 15 15:46:58 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.703415	84.970493	0.000000
0.728695	76.960638	0.005005
0.656819	81.358706	0.010010
0.686422	77.524466	0.015014
0.627010	80.007015	0.020019
0.472847	73.642755	0.025024
0.601391	66.062416	0.030029
0.340589	63.423635	0.035034
-0.153807	53.868541	0.040038
-0.041669	37.685059	0.045043
-0.595957	29.385493	0.050048
-0.473374	14.666301	0.055053
-0.943324	11.460544	0.060058
-1.536508	5.107284	0.065062
-1.662196	-15.420404	0.070067
-2.021244	-9.595332	0.075072
-2.432052	-19.637894	0.080077
-2.471575	-21.995192	0.085082
-3.251796	-7.335865	0.090086
-3.024031	-24.857788	0.095091
-3.454929	1.145095	0.100096
-3.711698	-22.002188	0.105101
-4.584969	-3.705376	0.110106
-4.850592	-17.278130	0.115110
-4.951295	-30.032332	0.120115
-5.223480	-14.452254	0.125120
-5.192955	-12.160964	0.130125
-5.049069	-27.464664	0.135130
-5.521482	-22.118041	0.140134
-5.398795	-35.558742	0.145139
-6.287396	-16.272354	0.150144
-6.663564	-25.156113	0.155149
-6.706119	-36.204849	0.160154
-6.831097	-23.382700	0.165158
-6.461699	-24.823378	0.170163
-7.418405	-16.961136	0.175168
-8.015288	-29.682564	0.180173
-7.954861	-26.912850	0.185178
-8.218240	-23.867472	0.190182
-8.181706	-24.598621	0.195187
-8.400896	-26.713150	0.200192
-9.153622	-24.217353	0.205197
-9.442754	-31.773602	0.210202
-10.020707	-41.469306	0.215206
-9.971112	-32.054555	0.220211
-9.797042	-20.741299	0.225216
-10.032491	-23.350221	0.230221
-9.824504	-23.084570	0.235226
-10.199279	-8.773194	0.240230
-10.729866	-30.041074	0.245235
-11.427163	-17.064758	0.250240
-11.662992	-17.334115	0.255245
-11.456658	-25.772369	0.260250
-11.701318	-12.821823	0.265254
-11.968500	-20.012766	0.270259
-12.777804	-18.373538	0.275264
-13.190345	-31.352413	0.280269
-13.376109	-22.632002	0.285274
-13.223911	-30.370287	0.290278
-13.187127	-27.639577	0.295283
-13.334505	-18.170269	0.300288
-13.324998	-32.540360	0.305293
-13.661484	-19.242600	0.310298
-14.796082	-32.968561	0.315302
-14.501648	-21.381921	0.320307
-14.806945	-37.889936	0.325312
-15.279334	-20.212110	0.330317
-15.758615	-20.104653	0.335322
-16.124697	-19.265597	0.340326
-15.975053	-16.413655	0.345331
-16.154159	-11.853771	0.350336
-16.495161	-26.441955	0.355341
-16.187864	-15.781854	0.360346
-16.675099	-22.347115	0.365350
-17.082855	-27.035737	0.370355
-17.327725	-23.838147	0.375360
-17.583874	-11.716405	0.380365
-17.538016	-20.494909	0.385370
-17.817827	-14.940401	0.390374
-18.762580	-21.730530	0.395379
-19.194595	-9.504160	0.400384
-19.276988	-17.012407	0.405389
-19.262332	-24.136382	0.410394
-19.415597	-11.503094	0.415398
-19.498065	-21.778858	0.420403
-19.768164	-16.528702	0.425408
-20.133287	-10.406884	0.430413
-20.749519	-18.232938	0.435418
-21.266624	-25.142272	0.440422
-20.796245	-25.642175	0.445427
-21.043015	-29.482800	0.450432
-20.961676	-26.071887	0.455437
-21.236256	-37.238828	0.460442
-22.092266	-21.750297	0.465446
-22.299038	-27.605877	0.470451
-22.526958	-24.949995	0.475456
-22.762038	-18.967061	0.480461
-23.036936	-26.766459	0.485466
-22.943398	-24.231668	0.490470
-23.307238	-24.045036	0.495475
-23.981221	-18.465636	0.500480
-23.956235	-30.196925	0.505485
-24.014977	-16.711963	0.510490
-24.557339	-7.426654	0.515494
-24.354844	-15.834190	0.520499
-25.364239	-16.666530	0.525504
-25.700016	-18.014643	0.530509
-25.739537	-21.647144	0.535514
-26.000055	-11.529770	0.540518
-25.964288	-23.269751	0.545523
-25.825385	-19.683289	0.550528
-26.152104	-16.346496	0.555533
-26.063526	-20.706082	0.560538
-26.649212	-10.434350	0.565542
-27.274875	-28.747142	0.570547
-27.041160	-4.588807	0.575552
-28.162783	-20.231551	0.580557
-27.777712	-22.760228	0.585562
-28.480288	-11.605530	0.590566
-28.546786	-7.334940	0.595571
-29.003180	-17.038513	0.600576
-29.045855	-21.012205	0.605581
-28.820731	-23.697832	0.610586
-28.877619	-24.382864	0.615590
-29.266927	-18.563448	0.620595
-30.103694	-24.167734	0.625600
-30.224809	-14.455360	0.630605
-30.082680	-22.643884	0.635610
-30.732729	-12.953101	0.640614
-31.364005	-28.178509	0.645619
-31.507201	-17.820989	0.650624
-31.908705	-23.765329	0.655629
-31.738077	-26.478449	0.660634
-31.990823	-8.755132	0.665638
-31.831014	-13.643992	0.670643
-32.229559	-8.704158	0.675648
-32.346546	-11.965673	0.680653
-33.063781	-2.902813	0.685658
-33.597596	-21.409538	0.690662
-33.429975	-15.888628	0.695667
-33.574067	-20.335833	0.700672
-33.816446	-26.320772	0.705677
-34.262752	-35.279738	0.710682
-35.060073	-20.905154	0.715686
-34.939391	-24.615919	0.720691
-35.119794	-19.502121	0.725696
-35.428373	-18.814914	0.730701
-35.061077	-21.805476	0.735706
-35.442557	-6.536614	0.740710
-35.228067	-24.653545	0.745715
-36.038897	-7.091321	0.750720
-36.451963	-17.748764	0.755725
-36.777442	-24.102127	0.760730
-36.806444	-11.335982	0.765734
-37.326925	-26.659406	0.770739
-37.576514	-14.829661	0.775744
-38.145368	-12.877406	0.780749
-38.051811	-25.750322	0.785754
-38.398478	-12.961964	0.790758
-38.193593	-14.610531	0.795763
-38.773621	-15.891742	0.800768
-39.050482	-20.836477	0.805773
-39.136345	-9.627836	0.810778
-39.780802	-14.438036	0.815782
-39.862265	-19.018406	0.820787
-40.101564	-7.407674	0.825792
-39.983302	-9.698518	0.830797
-40.128033	-19.730691	0.835802
-40.611296	-14.604522	0.840806
-40.805703	-24.755342	0.845811
-41.622974	-12.118465	0.850816
-41.664069	-23.762977	0.855821
-41.454952	-13.584620	0.860826
-41.879550	-20.992412	0.865830
-42.546123	-19.488733	0.870835
-42.925106	-24.304626	0.875840
-43.212394	-23.843287	0.880845
-43.314405	-20.815106	0.885850
-43.720576	-13.883523	0.890854
-43.317156	-18.178146	0.895859
-43.424334	-10.841312	0.900864
-43.366820	-15.202277	0.905869
-43.368729	-28.439103	0.910874
-44.360623	-6.804619	0.915878
-44.492929	-16.130959	0.920883
-44.908940	-22.455649	0.925888
-45.848359	-11.013515	0.930893
-45.860658	-26.433154	0.935898
-46.353144	-17.392352	0.940902
-46.235795	-25.187421	0.945907
-46.409005	-15.748371	0.950912
-46.760969	-16.515245	0.955917
-46.384891	-20.045968	0.960922
-46.905669	-7.346222	0.965926
-46.849117	-25.936003	0.970931
-47.152527	-11.441600	0.975936
-47.832891	-11.737716	0.980941
-47.904604	-12.517661	0.985946
-48.318106	-7.106882	0.990950
-48.472938	-10.145613	0.995955
-48.608150	-7.543028	1.000960
-49.231174	-1.081461	1.005965
-49.639647	-3.285650	1.010970
-49.626469	-2.730732	1.015974
-49.839546	-11.465656	1.020979
-49.963835	-13.727561	1.025984
-50.209718	-3.004150	1.030989
-50.047003	-8.639852	1.035994
-50.873795	-5.997846	1.040998
-51.226710	-16.672330	1.046003
-51.245593	-10.913637	1.051008
-51.577010	-12.068332	1.056013
-51.142976	-11.080855	1.061018
-51.919181	-14.657703	1.066022
-52.097044	-18.168004	1.071027
-52.588657	-4.499040	1.076032
-52.664368	-16.824415	1.081037
-52.802895	-16.876454	1.086042
-53.035325	-13.086770	1.091046
-53.753593	-14.971045	1.096051
-54.158312	-22.526538	1.101056
-54.589736	-22.584427	1.106061
-54.151461	-15.711414	1.111066
-55.001738	-10.903983	1.116070
-54.316066	-14.142977	1.121075
-54.380687	-8.540675	1.126080
-55.066030	-6.370492	1.131085
-55.470212	-13.453463	1.136090
-56.064531	-0.995277	1.141094
-56.181441	-24.033370	1.146099
-56.166211	-6.744192	1.151104
-56.034906	-11.047511	1.156109
-56.576954	-13.129299	1.161114
-57.480330	-2.748041	1.166118
-57.645871	4.528997	1.171123
-57.664602	1.737077	1.176128
-57.893215	-8.728601	1.181133
-57.690745	-14.915992	1.186138
-57.972213	-10.593897	1.191142
-58.236339	-15.262850	1.196147
-58.778995	-21.372274	1.201152
-59.262092	-7.776042	1.206157
-58.873384	-12.559200	1.211162
-59.523494	-5.012386	1.216166
-59.989990	-8.403370	1.221171
-60.442831	3.364587	1.226176
-60.604120	-6.199343	1.231181
-60.752141	-4.017538	1.236186
-60.958758	4.046978	1.241190
-60.924819	-12.612904	1.246195
-60.837726	-1.786589	1.251200
-61.361332	-14.022851	1.256205
-61.909358	-9.262017	1.261210
-62.484931	-0.208362	1.266214
-62.480595	-12.502972	1.271219
-62.448697	0.494602	1.276224
-62.718277	-10.623855	1.281229
-62.595319	-20.851095	1.286234
-62.999458	-10.688975	1.291238
-63.688140	-28.372531	1.296243
-64.226293	-13.113299	1.301248
-64.185425	-16.268023	1.306253
-64.113121	-20.802877	1.311258
-64.194956	-1.756148	1.316262
-64.585010	-16.130350	1.321267
-65.080886	-14.513419	1.326272
-65.511336	-6.084804	1.331277
-65.765599	-9.356974	1.336282
-65.800655	-17.178154	1.341286
-65.745763	-7.494867	1.346291
-65.980678	-9.194848	1.351296
-66.784840	-2.797453	1.356301
-67.092629	-17.143128	1.361306
-67.661537	-11.921124	1.366310
-67.215365	-0.741021	1.371315
-67.115210	-16.430011	1.376320
-67.215784	-12.357695	1.381325
-67.731413	-16.967029	1.386330
-68.895451	-13.864935	1.391334
-68.766813	-26.784581	1.396339
-68.711816	-17.423004	1.401344
-69.070226	-19.074459	1.406349
-68.468138	-18.657709	1.411354
-69.456497	-22.325461	1.416358
-69.969476	-21.018019	1.421363
-69.819454	-9.689248	1.426368
-70.559508	-10.143294	1.431373
-70.453320	-11.453963	1.436378
-70.540268	-8.820488	1.441382
-71.285457	-17.011126	1.446387
-71.764089	-11.248662	1.451392
-71.856992	-7.752623	1.456397
-71.790898	-5.603345	1.461402
-71.989684	-9.223928	1.466406
-72.073207	-16.898894	1.471411
-72.203921	-16.442320	1.476416
-72.886671	4.310087	1.481421
-72.953622	-16.471638	1.486426
-73.428897	-10.827117	1.491430
-73.647718	-16.894176	1.496435
-73.528147	-11.119499	1.501440
-73.881976	-20.498300	1.506445
-74.531164	-15.541015	1.511450
-75.236652	-8.809341	1.516454
-75.153942	-23.677856	1.521459
-75.291895	-10.009146	1.526464
-75.422551	-17.957267	1.531469
-75.390145	-28.456991	1.536474
-75.610202	-12.164627	1.541478
-75.566611	-20.407890	1.546483
-75.854861	-14.567097	1.551488
-76.780301	-7.568337	1.556493
-76.641277	-16.071031	1.561498
-76.905078	-13.026172	1.566502
-77.537995	-18.303884	1.571507
-78.212389	-26.981593	1.576512
-78.389176	-22.158020	1.581517
-78.249867	-25.653262	1.586522
-78.515936	-25.088890	1.591526
-78.680035	-9.245439	1.596531
-78.564549	-14.730097	1.601536
-78.719778	-13.766571	1.606541
-78.790085	-19.698464	1.611546
-79.314500	-9.662859	1.616550
-79.684772	-15.710609	1.621555
-79.596975	-18.126630	1.626560
-80.690401	-10.359667	1.631565
-80.780903	-8.254449	1.636570
-81.386472	-7.740900	1.641574
-81.177105	-16.418677	1.646579
-81.440465	-16.271928	1.651584
-81.525640	-7.676254	1.656589
-81.558968	-30.591419	1.661594
-81.960661	-12.706281	1.666598
-81.985458	-17.663374	1.671603
-82.893970	-2.501053	1.676608
-83.058433	-4.341313	1.681613
-82.956732	-18.385523	1.686618
-83.496221	-10.294413	1.691622
-83.605611	-18.450738	1.696627
-83.312957	-7.392354	1.701632
-83.961022	-8.083951	1.706637
-84.501223	-7.228643	1.711642
-84.969513	-13.078783	1.716646
-84.708302	-20.468613	1.721651
-84.679842	-17.310770	1.726656
-85.453287	-19.078594	1.731661
-85.816099	-11.767975	1.736666
-86.228455	-17.074543	1.741670
-86.134700	-14.282321	1.746675
-86.159658	-18.195707	1.751680
-86.562933	-18.380469	1.756685
-86.543541	-21.964503	1.761690
-87.392945	-10.556481	1.766694
-87.666814	-16.875459	1.771699
-88.149238	-15.857759	1.776704
-88.023058	-10.832705	1.781709
-87.980626	-11.725525	1.786714
-88.726884	-10.019861	1.791718
-88.249533	-17.843552	1.796723
-88.042976	-18.916004	1.801728
-89.086350	-15.699098	1.806733
-89.578680	-29.748996	1.811738
-89.860090	-11.995010	1.816742
-89.747030	-19.575110	1.821747
-89.657909	-26.565289	1.826752
-90.321367	-25.018618	1.831757
-90.810274	-14.966294	1.836762
-91.242001	-12.186267	1.841766
-91.323077	-16.674070	1.846771
-91.683393	-2.406418	1.851776
-91.724631	-4.532402	1.856781
-91.327598	-8.438588	1.861786
-91.526741	-0.283077	1.866790
-92.058985	-8.248285	1.871795
-92.268864	-22.706705	1.876800
-92.828464	-3.139383	1.881805
-92.629053	-20.112181	1.886810
-93.708717	-3.949316	1.891814
-94.087498	-12.738428	1.896819
-94.015079	-16.826827	1.901824
-94.538390	-15.433530	1.906829
-94.592128	-15.579781	1.911834
-94.737840	-17.652687	1.916838
-94.804577	-16.022435	1.921843
-94.716300	-12.138772	1.926848
-95.043494	-7.083770	1.931853
-95.376231	-14.110871	1.936858
-96.241368	-4.559632	1.941862
-96.346774	-4.179745	1.946867
-96.008868	-3.956580	1.951872
-96.322197	3.132692	1.956877
-96.741272	-14.676121	1.961882
-97.597718	-10.441691	1.966886
-97.933992	-7.461699	1.971891
-97.820035	-11.607866	1.976896
-97.712469	-5.752189	1.981901
-97.488245	-18.249153	1.986906
-98.006883	-7.120610	1.991910
-98.696185	-15.807103	1.996915
-99.051083	-15.345600	2.006912
-98.763124	-15.022716	2.016909
-98.328226	-12.405919	2.026906
-97.356015	-17.425156	2.036902
-96.610531	-13.259965	2.046899
-96.495385	-18.957268	2.056896
-96.416628	-21.588180	2.066893
-95.823774	-16.056035	2.076890
-94.967720	-10.072140	2.086886
-94.801719	-6.629805	2.096883
-93.955032	-18.006059	2.106880
-93.516478	-23.634234	2.116877
-93.424309	-19.187823	2.126874
-92.574066	-8.386409	2.136870
-92.371046	-10.723762	2.146867
-91.414649	-5.669603	2.156864
-90.830690	-20.118126	2.166861
-90.786313	-19.839337	2.176858
-90.091794	-17.075014	2.186854
-89.411305	-6.187266	2.196851
-89.109136	-11.990055	2.206848
-88.905001	-5.115245	2.216845
-87.851641	-13.326503	2.226842
-87.777839	-8.122429	2.236838
-86.459097	-17.557189	2.246835
-86.679672	-17.494384	2.256832
-86.043486	-18.285031	2.266829
-85.717475	-14.060291	2.276826
-84.925474	-7.721090	2.286822
-84.503469	-10.509678	2.296819
-84.481853	-9.707681	2.306816
-83.043486	-9.533834	2.316813
-82.974671	-16.156589	2.326810
-82.662136	-18.262046	2.336806
-82.409823	-11.471946	2.346803
-81.319509	-10.563983	2.356800
-81.322542	-11.667981	2.366797
-80.646193	-22.973904	2.376794
-80.155105	-20.506847	2.386790
-79.441079	-18.393103	2.396787
-78.628472	-17.115466	2.406784
-78.318387	-14.694451	2.416781
-78.201366	-20.491627	2.426778
-78.067184	-13.194758	2.436774
-77.090424	-10.511549	2.446771
-76.515427	-8.265781	2.456768
-75.378758	-10.722372	2.466765
-75.172528	-13.084454	2.476762
-75.111327	-13.454321	2.486758
-75.205179	-8.500287	2.496755
-74.026228	-7.871089	2.506752
-73.725997	-11.657702	2.516749
-72.588543	-3.578318	2.526746
-72.131276	-6.233168	2.536742
-72.292403	-7.983583	2.546739
-71.910583	-13.450275	2.556736
-70.462878	-9.479460	2.566733
-70.275086	-2.164974	2.576730
-70.573080	-12.855423	2.586726
-69.690932	-5.837731	2.596723
-69.130361	-1.084695	2.606720
-68.272873	-6.203698	2.616717
-67.529626	-10.313917	2.626714
-67.245033	-16.668113	2.636710
-67.237779	-25.347118	2.646707
-67.144753	-18.491976	2.656704
-66.084190	-12.577729	2.666701
-65.435359	-17.672022	2.676698
-64.352464	-13.692080	2.686694
-64.762188	-8.456887	2.696691
-64.331409	-9.884748	2.706688
-63.338924	-16.647315	2.716685
-62.644789	-8.326455	2.726682
-62.689167	-10.882200	2.736678
-62.372475	-6.569884	2.746675
-61.342054	-8.301700	2.756672
-61.295111	-4.047824	2.766669
-60.427760	-5.784100	2.776666
-59.648818	-9.605577	2.786662
-59.718152	-7.520403	2.796659
-59.099199	-15.539956	2.806656
-58.049271	-12.346722	2.816653
-58.178186	-15.652503	2.826650
-57.472724	-7.636450	2.836646
-56.789342	-8.946243	2.846643
-56.436928	-7.463747	2.856640
-56.429637	-6.103586	2.866637
-55.390238	-5.199945	2.876634
-55.326320	-0.861458	2.886630
-54.159624	-4.212460	2.896627
-53.634355	-13.358049	2.906624
-53.562611	-12.062471	2.916621
-53.388474	-11.912986	2.926618
-52.699965	-15.516933	2.936614
-51.822831	-12.460882	2.946611
-51.194588	-14.163073	2.956608
-50.760816	-15.746105	2.966605
-50.336845	-16.579214	2.976602
-50.161416	-11.812212	2.986598
-49.483932	-15.037617	2.996595
-48.824317	-11.217069	3.006592
-48.905290	-13.297397	3.016589
-47.759113	-17.062517	3.026586
-47.072234	-10.791376	3.036582
-47.058580	-7.214123	3.046579
-46.889227	-10.541444	3.056576
-45.878406	-12.403066	3.066573
-45.518408	-15.165798	3.076570
-44.737996	-19.349518	3.086566
-44.140332	-16.347732	3.096563
-43.933750	-17.104813	3.106560
-43.739269	-14.911326	3.116557
-42.928307	-11.364202	3.126554
-42.341717	-11.925102	3.136550
-42.154647	-12.763507	3.146547
-41.233001	-12.163095	3.156544
-40.886039	-12.147957	3.166541
-40.690504	-13.788710	3.176538
-39.645602	-3.450495	3.186534
-39.309613	-15.009927	3.196531
-39.380058	-3.882402	3.206528
-38.864792	-8.059049	3.216525
-37.698591	-11.292524	3.226522
-37.248485	-23.791076	3.236518
-36.415353	-11.639562	3.246515
-36.135891	-7.897529	3.256512
-36.166310	-4.850416	3.266509
-35.912216	-7.546952	3.276506
-34.802727	-14.088343	3.286502
-34.343880	-14.978774	3.296499
-34.024956	-4.192161	3.306496
-33.194567	-16.709216	3.316493
-33.009176	-11.941785	3.326490
-32.715233	-18.274315	3.336486
-31.673946	-8.473518	3.346483
-31.204699	-10.364362	3.356480
-31.269905	-8.620043	3.366477
-30.279795	-12.940451	3.376474
-29.709200	-23.018436	3.386470
-29.836096	-23.646424	3.396467
-29.283362	-18.520312	3.406464
-28.404553	-20.063301	3.416461
-27.347030	-12.225633	3.426458
-27.073728	-20.284660	3.436454
-26.944808	-11.523595	3.446451
-26.746877	-11.162025	3.456448
-25.957544	-8.058963	3.466445
-25.212359	-10.982939	3.476442
-24.851488	-14.042529	3.486438
-24.605787	-6.241078	3.496435
-23.915690	-18.006596	3.506432
-23.668660	-17.825301	3.516429
-22.721117	-22.975969	3.526426
-22.003703	-17.619570	3.536422
-21.748777	-26.833175	3.546419
-21.839395	-15.442254	3.556416
-20.420758	-15.672669	3.566413
-20.217809	-11.522703	3.576410
-20.349784	-9.275758	3.586406
-19.327465	-14.698755	3.596403
-18.627873	-6.358934	3.606400
-18.512872	-17.210782	3.616397
-17.776658	-25.246646	3.626394
-17.124964	-23.664856	3.636390
-16.912789	-20.025295	3.646387
-16.742229	-16.161752	3.656384
-15.622189	-11.896064	3.666381
-15.234519	-20.748075	3.676378
-15.162215	-14.186808	3.686374
-14.323522	-21.357962	3.696371
-13.926713	-22.093733	3.706368
-13.742337	-22.489585	3.716365
-12.663392	-21.645809	3.726362
-12.383141	-16.156616	3.736358
-11.901709	-16.554247	3.746355
-10.704477	-19.082667	3.756352
-10.860176	-19.689005	3.766349
-10.576980	-8.879399	3.776346
-10.192416	-9.963989	3.786342
-9.207188	-22.731337	3.796339
-9.157442	-8.113681	3.806336
-8.097452	-15.533671	3.816333
-7.399584	-4.033421	3.826330
-7.439609	-17.375102	3.836326
-7.334911	-15.168652	3.846323
-6.158626	-10.756294	3.856320
-5.899410	-10.887456	3.866317
-5.607283	-14.397745	3.876314
-5.084180	-19.719374	3.886310
-4.432212	-5.014161	3.896307
-3.495753	0.378351	3.906304
-3.553005	5.281600	3.916301
-3.182994	7.678399	3.926298
-2.780915	19.993931	3.936294
-2.162836	38.611957	3.946291
-1.724780	38.900462	3.956288
-1.349583	59.732405	3.966285
-0.813734	83.529729	3.976282
-0.466677	98.752187	3.986278
-0.403705	119.623760	3.996275
0.000000	136.046810	4.001280
0.601350	149.155206	4.006285
0.866487	168.671007	4.011290
1.063257	178.907275	4.016294
0.937738	167.886207	4.021299
0.894981	180.034295	4.026304
1.051795	184.853116	4.031309
1.139558	187.031299	4.036314
1.417790	197.753078	4.041318
1.659517	200.229384	4.046323
1.391890	218.174525	4.051328
1.333066	209.520910	4.056333
1.753027	229.152664	4.061338
1.455886	213.849493	4.066342
1.403819	222.493891	4.071347
1.388849	217.354567	4.076352
1.843662	216.838587	4.081357
1.636276	219.713667	4.086362
1.586195	217.344267	4.091366
1.915235	201.675223	4.096371
1.525128	200.436392	4.101376
1.576251	188.810704	4.106381
1.681378	177.807743	4.111386
1.194318	195.875437	4.116390
1.477212	186.085564	4.121395
1.909530	205.725308	4.126400
1.772990	208.039801	4.131405
1.724188	198.449057	4.136410
1.419906	212.857899	4.141414
1.993963	203.130187	4.146419
1.811612	204.574579	4.151424
1.908477	185.918878	4.156429
1.825386	190.177764	4.161434
1.233453	193.282216	4.166438
1.799269	192.677161	4.171443
1.524083	208.948301	4.176448
1.848056	215.684650	4.181453
2.010392	223.023918	4.186458
1.813822	220.235893	4.191462
1.976950	232.779217	4.196467
1.793845	210.711147	4.201472
1.932367	206.744246	4.206477
1.635614	204.141962	4.211482
1.271378	213.975454	4.216486
1.408082	223.967659	4.221491
1.603563	224.152321	4.226496
1.840655	229.488518	4.231501
2.072032	234.841149	4.236506
1.877873	236.245174	4.241510
2.108090	229.426485	4.246515
2.152398	219.801005	4.251520
2.048676	227.624312	4.256525
1.556442	222.310627	4.261530
1.605997	224.907380	4.266534
2.207669	208.559856	4.271539
1.981575	223.770126	4.276544
1.954246	211.100864	4.281549
2.123192	210.505954	4.286554
1.826524	210.335725	4.291558
2.104553	220.246075	4.296563
1.941639	221.697318	4.301568
1.609347	229.715939	4.306573
1.811001	230.954327	4.311578
2.030937	255.721651	4.316582
2.131462	258.576534	4.321587
2.332027	258.583282	4.326592
2.449534	259.401526	4.331597
2.215825	236.520731	4.336602
1.829523	226.314343	4.341606
2.353979	233.626722	4.346611
2.153434	242.625449	4.351616
2.294470	244.455881	4.356621
2.536837	245.163424	4.361626
2.205237	235.963575	4.366630
2.437314	224.085505	4.371635
1.905311	237.881713	4.376640
2.615735	247.913384	4.381645
2.062611	238.478661	4.386650
2.003037	247.929481	4.391654
2.169595	243.588894	4.396659
2.461681	261.819215	4.401664
2.307524	257.525410	4.406669
2.661754	258.124599	4.411674
2.440830	262.619166	4.416678
2.730654	244.732926	4.421683
2.377296	251.209024	4.426688
2.261737	234.380611	4.431693
2.259089	226.741377	4.436698
2.016843	243.850946	4.441702
2.784885	251.912167	4.446707
2.769338	254.051103	4.451712
2.480653	242.424512	4.456717
2.421299	235.052609	4.461722
1.969030	244.586967	4.466726
2.271883	250.986978	4.471731
2.463474	255.465558	4.476736
2.422957	248.369020	4.481741
2.664317	259.247671	4.486746
2.508837	258.239568	4.491750
2.886840	254.998196	4.496755
2.445362	256.347208	4.501760
2.315779	260.607484	4.506765
2.488349	262.206210	4.511770
2.470861	281.373971	4.516774
2.475579	262.253184	4.521779
2.531172	272.351949	4.526784
2.335521	257.605504	4.531789
2.575887	268.869153	4.536794
2.198151	261.051776	4.541798
2.748247	250.331054	4.546803
2.502297	261.365309	4.551808
2.320045	263.938326	4.556813
2.890575	279.090694	4.561818
2.987917	293.974032	4.566822
2.729722	275.852187	4.571827
2.657926	291.494755	4.576832
3.050959	282.770274	4.581837
2.961945	268.946612	4.586842
2.290789	265.766553	4.591846
2.944019	278.406884	4.596851
2.889837	294.737775	4.601856
2.773489	290.470364	4.606861
3.067757	280.421868	4.611866
2.814226	292.215512	4.616870
3.352485	281.501952	4.621875
2.904908	274.158575	4.626880
2.862593	256.660048	4.631885
3.012162	252.926290	4.636890
2.747236	255.408598	4.641894
2.949647	242.373438	4.646899
2.784037	258.473814	4.651904
2.809817	271.799757	4.656909
2.983315	272.314578	4.661914
3.029206	280.622608	4.666918
3.145017	259.038069	4.671923
3.103092	283.372931	4.676928
3.098236	272.513558	4.681933
2.987013	256.319799	4.686938
2.768420	277.934321	4.691942
3.299414	262.857864	4.696947
3.123756	273.851707	4.701952
3.296963	270.803788	4.706957
2.925386	265.818969	4.711962
3.172693	277.774681	4.716966
3.198588	288.044093	4.721971
3.017092	278.585714	4.726976
3.069052	280.100595	4.731981
3.156305	295.701889	4.736986
2.755919	285.058014	4.741990
3.364951	296.949327	4.746995
3.567072	291.077545	4.752000
2.964746	293.269951	4.757005
3.486826	285.456274	4.762010
3.158577	285.904461	4.767014
3.356446	279.752336	4.772019
2.871177	295.418648	4.777024
3.178102	273.235967	4.782029
3.330014	292.688858	4.787034
2.972164	282.755130	4.792038
3.142926	296.219807	4.797043
3.006513	290.336790	4.802048
3.062553	297.676198	4.807053
3.354754	284.837370	4.812058
3.007488	294.407677	4.817062
3.595444	281.719542	4.822067
3.047743	286.475773	4.827072
3.226287	286.388794	4.832077
3.428113	283.205928	4.837082
3.307814	297.093766	4.842086
3.415995	306.920373	4.847091
3.470463	306.236259	4.852096
3.488950	305.477396	4.857101
3.520699	312.640299	4.862106
3.227580	290.117965	4.867110
3.598952	308.932360	4.872115
3.615094	305.163423	4.877120
3.716591	306.706226	4.882125
3.926468	303.172709	4.887130
3.226802	306.680506	4.892134
3.662212	292.826782	4.897139
3.370506	296.821465	4.902144
3.911368	311.463429	4.907149
3.630629	299.800558	4.912154
3.320168	303.234072	4.917158
3.725326	305.598944	4.922163
3.590691	317.672259	4.927168
3.414154	318.308556	4.932173
3.900612	312.601083	4.937178
3.663407	305.100009	4.942182
3.613350	319.181744	4.947187
3.752321	317.417765	4.952192
3.634352	296.555738	4.957197
3.929666	308.618762	4.962202
3.539500	299.617958	4.967206
3.879400	309.764861	4.972211
3.900399	307.920349	4.977216
3.834240	311.978976	4.982221
4.111466	313.346049	4.987226
3.762201	293.123119	4.992230
3.651129	284.704495	4.997235
3.347170	302.139411	5.002240
3.568706	291.666999	5.007245
4.204339	303.921584	5.012250
3.873849	294.795305	5.017254
3.811907	310.556418	5.022259
3.652719	310.200499	5.027264
3.665860	313.859023	5.032269
3.709582	308.645749	5.037274
3.329072	307.427322	5.042278
3.669033	301.312573	5.047283
3.775242	323.893313	5.052288
3.743752	313.525737	5.057293
3.914890	319.539434	5.062298
4.005766	334.453475	5.067302
4.284900	339.814035	5.072307
3.871118	341.458468	5.077312
4.239437	337.844997	5.082317
4.105423	326.243092	5.087322
4.016454	325.639503	5.092326
4.088985	318.879682	5.097331
3.970396	310.802821	5.102336
3.966004	327.899221	5.107341
4.191555	336.479457	5.112346
4.125981	343.173795	5.117350
4.427314	322.263552	5.122355
4.182483	328.235704	5.127360
3.914583	306.725359	5.132365
3.913330	317.624514	5.137370
4.107488	341.590770	5.142374
4.160582	344.748961	5.147379
3.916197	351.328332	5.152384
4.042978	349.464558	5.157389
4.179345	338.038443	5.162394
4.122980	359.276855	5.167398
4.445001	344.163333	5.172403
4.332152	341.638358	5.177408
4.015973	350.691377	5.182413
4.419692	347.074323	5.187418
4.403511	334.323309	5.192422
4.532257	334.765919	5.197427
4.435902	343.590537	5.202432
4.234827	348.426529	5.207437
4.354532	341.754888	5.212442
4.224974	345.814037	5.217446
4.781564	326.865165	5.222451
4.380426	360.579954	5.227456
4.335596	348.972566	5.232461
4.474005	346.140506	5.237466
4.469680	353.209064	5.242470
4.685171	345.972610	5.247475
4.478101	351.886741	5.252480
4.274827	351.407693	5.257485
4.032048	350.429302	5.262490
4.382765	353.154369	5.267494
4.769389	345.981871	5.272499
4.564000	346.625305	5.277504
3.889670	346.802678	5.282509
4.060525	345.079792	5.287514
4.229646	347.104964	5.292518
4.636166	343.726868	5.297523
4.339435	346.527263	5.302528
4.176774	363.761528	5.307533
4.453895	371.211917	5.312538
4.749954	370.460649	5.317542
4.764738	360.903786	5.322547
4.923119	373.598845	5.327552
4.902125	364.938891	5.332557
4.727048	363.841586	5.337562
4.502797	357.522923	5.342566
4.947766	358.968426	5.347571
4.579179	358.893635	5.352576
4.676822	375.882666	5.357581
4.834160	367.745971	5.362586
4.494303	375.211313	5.367590
5.314421	375.310213	5.372595
4.769897	355.713237	5.377600
4.422081	353.463650	5.382605
4.627233	354.689238	5.387610
4.729026	363.471061	5.392614
4.908865	371.030257	5.397619
4.951748	372.371545	5.402624
5.045907	368.544912	5.407629
5.224008	370.093510	5.412634
4.853993	360.012782	5.417638
4.860731	345.676135	5.422643
4.745851	347.988746	5.427648
4.660826	342.529299	5.432653
4.711197	372.548395	5.437658
5.156963	375.988354	5.442662
4.865885	370.382125	5.447667
5.011043	372.693496	5.452672
4.959654	369.101926	5.457677
4.791586	366.190884	5.462682
4.755706	369.679560	5.467686
4.743497	374.124279	5.472691
4.870710	372.246028	5.477696
5.087047	382.621352	5.482701
5.035179	365.986572	5.487706
5.049045	373.030233	5.492710
4.962473	372.795489	5.497715
5.329322	373.494305	5.502720
4.738018	372.585050	5.507725
5.081863	366.190752	5.512730
4.944636	368.421728	5.517734
4.967797	375.630176	5.522739
5.022290	360.820196	5.527744
4.849460	374.570785	5.532749
4.952364	387.911508	5.537754
4.635641	391.223751	5.542758
5.420134	390.708725	5.547763
5.249157	411.896307	5.552768
5.117090	418.795907	5.557773
5.321664	409.210511	5.562778
5.266186	404.129411	5.567782
5.530461	407.032335	5.572787
5.248220	407.726352	5.577792
5.274065	411.188757	5.582797
5.502527	399.671021	5.587802
5.119210	399.178417	5.592806
5.205438	410.730545	5.597811
5.318518	400.810364	5.602816
5.676189	403.568424	5.607821
5.716704	394.728414	5.612826
5.141171	388.012426	5.617830
5.150537	377.539306	5.622835
5.220171	381.573933	5.627840
5.396268	391.601664	5.632845
5.731191	395.848053	5.637850
5.590047	407.855434	5.642854
5.373914	404.283089	5.647859
5.558594	389.460941	5.652864
5.293947	399.840689	5.657869
5.630066	393.787503	5.662874
5.653935	407.767926	5.667878
5.564352	386.799279	5.672883
5.423287	379.156305	5.677888
5.258514	384.699641	5.682893
5.888940	394.446806	5.687898
5.590154	399.237700	5.692902
5.622778	389.706184	5.697907
5.289790	379.396279	5.702912
5.259704	392.677202	5.707917
5.357834	398.843571	5.712922
5.144131	405.839818	5.717926
5.581632	417.482269	5.722931
5.579031	407.369401	5.727936
5.427956	407.207071	5.732941
5.640195	413.866776	5.737946
5.421143	411.996319	5.742950
5.554809	403.384968	5.747955
5.525929	411.795888	5.752960
5.320906	405.960764	5.757965
5.692861	416.373826	5.762970
5.830489	417.930004	5.767974
5.857193	422.490928	5.772979
5.655486	427.000322	5.777984
5.805845	430.078236	5.782989
5.807816	422.964336	5.787994
5.795830	438.439232	5.792998
6.175563	422.020630	5.798003
5.613754	419.162216	5.803008
5.532499	417.755920	5.808013
5.666394	425.287321	5.813018
5.717241	426.408789	5.818022
5.931773	425.750798	5.823027
6.162629	429.019911	5.828032
5.775895	436.903114	5.833037
5.753035	430.589713	5.838042
5.712047	434.133109	5.843046
6.005654	433.897785	5.848051
6.108496	437.889452	5.853056
5.809260	427.830722	5.858061
6.041849	427.672465	5.863066
5.680653	430.163410	5.868070
5.759718	427.593388	5.873075
5.696131	421.510161	5.878080
5.628926	431.314730	5.883085
5.756268	427.002671	5.888090
5.959735	453.036244	5.893094
6.364236	456.566104	5.898099
6.251246	453.291988	5.903104
6.064630	437.176690	5.908109
6.210682	435.414487	5.913114
6.024226	432.824517	5.918118
6.073636	435.162572	5.923123
6.274556	443.284173	5.928128
6.020048	449.185466	5.933133
6.160440	432.624691	5.938138
5.714910	461.232457	5.943142
6.430229	456.987573	5.948147
6.726818	470.168116	5.953152
6.314564	450.917221	5.958157
6.338354	431.397385	5.963162
6.077159	436.864042	5.968166
6.177658	435.120219	5.973171
6.404847	432.417105	5.978176
6.551231	429.671016	5.983181
6.414996	436.321039	5.988186
6.182032	440.800088	5.993190
6.190535	433.714008	5.998195
5.902534	436.891494	6.003200
6.201334	442.397308	6.008205
6.641092	456.868589	6.013210
6.457080	461.622383	6.018214
6.494890	449.356488	6.023219
6.376047	431.895759	6.028224
6.006498	437.276148	6.033229
6.356470	443.857074	6.038234
6.393117	462.972119	6.043238
6.398575	437.767165	6.048243
6.225360	453.858350	6.053248
6.470499	443.009925	6.058253
5.982509	444.374532	6.063258
6.616223	453.308123	6.068262
6.629496	449.722718	6.073267
6.366222	434.964290	6.078272
6.359419	431.539356	6.083277
6.325588	434.804365	6.088282
6.227402	425.589702	6.093286
6.450094	433.703063	6.098291
6.492631	420.999491	6.103296
6.282408	411.993842	6.108301
6.394191	414.125274	6.113306
6.323078	421.365797	6.118310
6.728157	419.538200	6.123315
6.454123	424.125640	6.128320
6.305259	432.139308	6.133325
6.611694	435.843800	6.138330
6.220882	428.612799	6.143334
6.341517	422.456215	6.148339
6.188374	432.950244	6.153344
6.314699	418.331655	6.158349
6.362052	420.423917	6.163354
6.197769	426.825930	6.168358
6.323294	429.587831	6.173363
5.990257	432.320055	6.178368
5.943091	432.414305	6.183373
6.436179	424.677068	6.188378
6.113360	428.895928	6.193382
6.184578	428.450535	6.198387
6.317428	435.323528	6.203392
6.202992	446.728809	6.208397
6.647580	456.921942	6.213402
6.332743	438.961380	6.218406
6.434182	435.632398	6.223411
6.538639	432.373946	6.228416
6.273679	433.138110	6.233421
6.215213	422.657722	6.238426
5.916100	441.870941	6.243430
6.169971	442.287155	6.248435
6.304169	446.477158	6.253440
6.316322	465.402308	6.258445
6.971975	455.504298	6.263450
6.133016	446.067949	6.268454
6.201829	438.379507	6.273459
6.558129	444.178675	6.278464
6.201067	444.725740	6.283469
6.501945	431.395855	6.288474
6.438987	436.046376	6.293478
6.515940	436.837099	6.298483
6.424246	424.189248	6.303488
6.312233	434.644518	6.308493
6.259386	429.577971	6.313498
6.185279	430.629627	6.318502
6.421553	440.897917	6.323507
6.210233	432.434319	6.328512
6.135353	443.781171	6.333517
6.242147	437.141413	6.338522
6.369330	442.195855	6.343526
6.469749	443.133832	6.348531
6.531777	443.004649	6.353536
6.330926	433.248293	6.358541
6.604938	427.482466	6.363546
6.440555	430.192639	6.368550
6.530789	429.112155	6.373555
6.670403	433.423188	6.378560
6.436049	432.962492	6.383565
6.781868	432.868981	6.388570
6.262883	434.605980	6.393574
6.373455	429.445740	6.398579
6.501647	431.850582	6.403584
6.451912	418.708769	6.408589
6.701615	419.836638	6.413594
6.737027	425.773566	6.418598
6.653819	413.716710	6.423603
6.237515	407.647286	6.428608
6.171860	407.258053	6.433613
6.131817	408.568261	6.438618
6.207111	416.515481	6.443622
6.394401	420.793871	6.448627
6.609901	419.951740	6.453632
6.322769	421.651310	6.458637
6.211578	401.562713	6.463642
5.945989	418.170955	6.468646
6.093658	425.004601	6.473651
6.202968	424.479122	6.478656
6.530804	433.221163	6.483661
6.499223	431.796102	6.488666
6.405720	414.845467	6.493670
6.235063	427.380976	6.498675
6.617758	422.326899	6.503680
6.421573	432.555866	6.508685
6.582608	405.210804	6.513690
6.351885	425.185322	6.518694
5.910717	407.959206	6.523699
6.093356	415.601912	6.528704
6.066879	426.134588	6.533709
6.649258	436.001688	6.538714
6.467245	433.083072	6.543718
6.461851	433.606352	6.548723
6.224494	431.452932	6.553728
6.386067	427.946904	6.558733
6.311454	426.722998	6.563738
6.400980	426.233935	6.568742
6.180814	431.174025	6.573747
6.670260	428.314422	6.578752
6.252829	426.193721	6.583757
6.176389	415.889930	6.588762
6.082176	432.515738	6.593766
6.243133	432.824783	6.598771
6.243006	426.487008	6.603776
6.173012	432.193056	6.608781
6.515285	430.907853	6.613786
6.224884	427.153735	6.618790
6.112139	436.476137	6.623795
6.521540	429.060909	6.628800
6.057321	448.521016	6.633805
6.229153	425.148528	6.638810
6.331171	445.916571	6.643814
6.529945	426.872024	6.648819
6.408131	425.600575	6.653824
5.908873	446.599187	6.658829
6.319810	425.648197	6.663834
6.292868	438.166278	6.668838
5.992520	440.358520	6.673843
6.179022	427.259737	6.678848
5.929879	434.638694	6.683853
6.174447	421.613777	6.688858
6.134460	431.484186	6.693862
6.326156	439.652196	6.698867
6.480627	430.416789	6.703872
6.385229	432.506895	6.708877
6.509436	436.146601	6.713882
6.296028	440.453530	6.718886
6.335919	435.921035	6.723891
6.163471	431.318273	6.728896
6.080081	452.358360	6.733901
6.335257	440.391071	6.738906
6.565740	427.414941	6.743910
6.590143	425.857612	6.748915
6.702453	438.397271	6.753920
6.603861	440.203697	6.758925
6.710117	431.657136	6.763930
6.003052	431.469786	6.768934
6.171779	430.893746	6.773939
6.534642	429.309785	6.778944
6.606690	429.527474	6.783949
6.393845	417.771414	6.788954
6.049162	425.340766	6.793958
5.994670	419.084386	6.798963
6.473889	428.037279	6.803968
6.184945	427.039284	6.808973
6.604150	428.622820	6.813978
6.569367	424.684897	6.818982
6.406643	430.965512	6.823987
6.534580	435.197584	6.828992
6.345454	422.883683	6.833997
6.448555	436.569591	6.839002
6.497579	431.006574	6.844006
6.569385	427.268657	6.849011
6.726853	431.744937	6.854016
6.267971	429.509452	6.859021
6.664116	421.526025	6.864026
6.135339	409.923296	6.869030
5.997110	411.749784	6.874035
6.133154	423.870294	6.879040
6.098088	435.409732	6.884045
6.580854	426.981778	6.889050
6.385586	435.021958	6.894054
6.415826	422.218611	6.899059
6.418088	431.474949	6.904064
6.393146	431.998204	6.909069
6.637135	429.777078	6.914074
6.186979	417.201788	6.919078
6.376921	413.300126	6.924083
6.404893	417.860444	6.929088
6.251402	399.905326	6.934093
6.261915	412.669345	6.939098
6.289406	417.480016	6.944102
6.336405	424.912133	6.949107
6.106718	426.987240	6.954112
5.980353	426.687452	6.959117
6.305477	419.846384	6.964122
6.142765	443.878879	6.969126
6.295935	433.572447	6.974131
6.273711	440.383963	6.979136
6.240678	452.525434	6.984141
6.884784	438.670335	6.989146
6.492355	446.215625	6.994150
6.211212	439.161130	6.999155
6.430944	436.710014	7.004160
6.365354	433.820892	7.009165
6.481069	425.192669	7.014170
6.450750	433.701697	7.019174
6.327440	430.534848	7.024179
6.527388	425.880313	7.029184
6.312527	419.098788	7.034189
6.291698	410.509512	7.039194
5.975604	412.384531	7.044198
6.326842	427.612847	7.049203
6.661464	421.109859	7.054208
6.229240	438.201024	7.059213
6.403739	429.359965	7.064218
6.367945	431.755603	7.069222
6.185351	435.002678	7.074227
6.414451	423.480972	7.079232
6.084369	425.576320	7.084237
6.499680	423.774357	7.089242
6.302779	423.883092	7.094246
6.505606	432.797218	7.099251
6.415553	431.430750	7.104256
6.019648	424.713373	7.109261
6.282908	434.117863	7.114266
6.278618	426.083610	7.119270
6.776893	437.704688	7.124275
6.416286	427.773492	7.129280
6.163315	416.617736	7.134285
6.184262	411.011719	7.139290
6.510605	432.902000	7.144294
6.319032	417.253071	7.149299
6.195124	414.670820	7.154304
5.987838	425.871736	7.159309
6.106517	427.479780	7.164314
6.164210	431.837200	7.169318
6.080701	437.366731	7.174323
6.060550	441.518511	7.179328
6.342849	435.203904	7.184333
6.587394	433.580403	7.189338
6.598308	442.374428	7.194342
6.288307	440.940625	7.199347
6.535742	440.383048	7.204352
6.448018	441.733299	7.209357
6.649132	434.990552	7.214362
6.548785	439.456662	7.219366
6.093509	434.961209	7.224371
6.482188	427.882742	7.229376
5.918693	435.743562	7.234381
6.376572	436.524409	7.239386
6.207664	423.197292	7.244390
6.195903	443.133479	7.249395
6.220193	437.903741	7.254400
6.063624	446.545905	7.259405
6.476330	435.242444	7.264410
6.150165	442.610261	7.269414
6.332640	433.691130	7.274419
6.743146	441.730843	7.279424
6.262765	450.457596	7.284429
6.626887	430.156348	7.289434
6.403172	439.992706	7.294438
6.208931	430.948398	7.299443
6.151154	436.073257	7.304448
6.166107	440.188062	7.309453
6.348984	424.255876	7.314458
6.064840	440.640018	7.319462
6.193742	419.554525	7.324467
6.406348	438.948346	7.329472
6.332996	429.248660	7.334477
6.508844	428.769994	7.339482
6.607344	435.336833	7.344486
6.532535	433.608268	7.349491
6.847384	437.053796	7.354496
6.553888	437.186780	7.359501
6.326072	435.786848	7.364506
6.082486	431.383572	7.369510
6.001663	444.531661	7.374515
6.374802	428.498776	7.379520
6.311812	448.727942	7.384525
6.478220	441.738482	7.389530
6.128415	440.736930	7.394534
6.228481	439.329178	7.399539
6.142722	442.664130	7.404544
6.111272	444.082424	7.409549
6.370662	421.247615	7.414554
6.220286	432.833728	7.419558
6.303461	437.485355	7.424563
6.472105	432.552473	7.429568
6.045676	444.225944	7.434573
6.108809	422.089648	7.439578
6.293343	434.545157	7.444582
6.285710	428.534264	7.449587
6.349703	429.909358	7.454592
6.142587	435.408904	7.459597
6.295083	430.287411	7.464602
6.139974	431.913571	7.469606
6.224900	430.870760	7.474611
6.351512	432.306534	7.479616
6.128234	443.562884	7.484621
6.415034	433.630743	7.489626
6.535288	431.892928	7.494630
6.227084	436.380957	7.499635
6.329473	428.251141	7.504640
5.934116	437.833626	7.509645
6.344130	431.888863	7.514650
6.333260	437.027674	7.519654
6.494059	447.982516	7.524659
6.488137	446.424179	7.529664
6.385898	443.190411	7.534669
6.455192	434.452262	7.539674
6.313029	426.710600	7.544678
6.286544	434.054340	7.549683
6.210405	427.457446	7.554688
5.996586	436.548941	7.559693
5.890529	441.341933	7.564698
6.483203	445.854024	7.569702
6.693600	466.994147	7.574707
6.741666	448.153923	7.579712
6.255160	439.904585	7.584717
6.341988	436.139422	7.589722
6.336406	444.952157	7.594726
6.588558	436.126078	7.599731
6.655435	428.330140	7.604736
6.530926	446.190932	7.609741
6.583981	440.925067	7.614746
6.495002	441.295047	7.619750
6.154876	443.079437	7.624755
6.494631	442.566976	7.629760
6.445071	433.962804	7.634765
6.644988	422.791195	7.639770
6.709770	439.941989	7.644774
6.671688	426.112235	7.649779
6.301472	424.338179	7.654784
6.185671	432.206794	7.659789
6.522572	419.047945	7.664794
6.723700	422.211777	7.669798
6.454211	409.826527	7.674803
6.445801	403.232753	7.679808
6.279940	418.749237	7.684813
6.379020	406.825824	7.689818
6.200196	414.447174	7.694822
6.120185	410.193948	7.699827
5.898356	409.328990	7.704832
5.980278	422.122352	7.709837
6.448548	431.974865	7.714842
6.466324	428.771086	7.719846
6.338625	434.976269	7.724851
6.575524	425.886562	7.729856
6.354902	422.551320	7.734861
6.398172	408.736153	7.739866
6.120921	409.714443	7.744870
6.254976	425.328556	7.749875
6.625464	419.075834	7.754880
6.403362	426.628382	7.759885
5.962473	403.376518	7.764890
6.155435	413.308155	7.769894
6.365336	428.795304	7.774899
6.847177	424.971870	7.779904
6.252942	431.376276	7.784909
6.343190	415.866336	7.789914
6.312428	416.883009	7.794918
5.982221	429.093694	7.799923
6.129500	423.711643	7.804928
6.155996	438.674404	7.809933
6.385378	434.410292	7.814938
6.626434	434.231201	7.819942
6.438450	450.926587	7.824947
6.589208	445.717182	7.829952
6.135096	423.126748	7.834957
5.972438	429.467233	7.839962
5.953345	442.582034	7.844966
6.355461	436.917061	7.849971
6.347897	428.720182	7.854976
5.891346	435.923588	7.859981
6.321170	433.263638	7.864986
6.118615	422.888447	7.869990
6.229889	432.994393	7.874995
6.573727	430.299034	7.880000
6.462760	441.249355	7.885005
6.349223	442.486577	7.890010
6.508073	439.744346	7.895014
6.387953	439.588540	7.900019
6.463835	424.551819	7.905024
6.294282	445.181055	7.910029
6.446153	430.918991	7.915034
6.505816	440.777181	7.920038
6.171831	432.296762	7.925043
5.848029	437.686954	7.930048
5.836731	435.467667	7.935053
6.265733	441.738003	7.940058
6.304354	438.330026	7.945062
6.264933	433.415053	7.950067
6.410502	434.945160	7.955072
6.418318	432.103985	7.960077
6.285265	430.250784	7.965082
6.092536	435.884287	7.970086
6.046803	439.411698	7.975091
6.327161	446.285182	7.980096
6.398311	442.419814	7.985101
6.009222	435.781310	7.990106
6.305025	446.148381	7.995110
6.324108	453.932667	8.000115
6.502247	436.474462	8.005133
5.996068	443.010198	8.010150
6.471566	459.880119	8.015168
6.511051	462.369400	8.020186
6.238003	448.308226	8.025203
6.538396	439.535154	8.030221
6.157938	438.588208	8.035238
6.243642	432.049223	8.040256
6.515720	452.444990	8.045274
6.469756	445.952161	8.050291
6.668134	426.309508	8.055309
6.558128	434.609870	8.060326
6.304892	426.141822	8.065344
6.602291	431.965096	8.070362
6.416485	442.853259	8.075379
6.691781	425.795601	8.080397
6.415680	435.362930	8.085414
6.419554	430.169186	8.090432
6.272629	431.650580	8.095450
6.123496	434.560780	8.100467
6.059118	429.459986	8.105485
6.079976	446.118784	8.110502
6.403285	457.557293	8.115520
6.857874	466.984409	8.120538
6.609386	459.785482	8.125555
6.583159	447.660139	8.130573
6.317934	447.615646	8.135590
6.099021	428.661856	8.140608
6.439502	453.045602	8.145626
6.148230	459.570823	8.150643
6.391957	463.356891	8.155661
6.274202	464.876074	8.160678
6.443618	471.068940	8.165696
6.846139	472.995809	8.170714
6.561074	466.441823	8.175731
6.472653	463.595648	8.180749
6.452138	462.140031	8.185766
6.553256	467.857605	8.190784
6.899322	472.604151	8.195802
6.562351	478.903532	8.200819
6.736752	472.594096	8.205837
6.741734	480.093119	8.210854
6.738735	465.352141	8.215872
6.561525	448.682832	8.220890
6.514514	448.087755	8.225907
6.775081	441.053068	8.230925
6.418280	431.726389	8.235942
6.340103	443.221789	8.240960
6.483567	461.589391	8.245978
6.962313	461.882062	8.250995
6.925136	457.725812	8.256013
6.566769	448.856342	8.261030
6.385871	448.794174	8.266048
6.972332	446.529689	8.271066
6.481304	445.278171	8.276083
6.516510	444.509513	8.281101
6.606819	443.769829	8.286118
6.446482	439.862316	8.291136
6.498748	431.929344	8.296154
6.600424	449.098857	8.301171
6.980102	441.401455	8.306189
6.753478	437.962252	8.311206
6.772022	446.950140	8.316224
6.538492	441.838917	8.321242
6.685573	433.487533	8.326259
6.579402	438.692357	8.331277
6.471638	433.535854	8.336294
6.291464	445.472307	8.341312
6.837982	459.492103	8.346330
6.976159	480.602757	8.351347
6.955817	455.409165	8.356365
6.405743	434.553351	8.361382
6.535802	439.856305	8.366400
6.933600	451.493959	8.371418
6.372069	442.727533	8.376435
6.638160	453.671109	8.381453
6.629605	465.391963	8.386470
6.723992	466.458389	8.391488
6.970165	461.589059	8.396506
6.634534	465.380244	8.401523
7.050479	469.643619	8.406541
6.813866	464.890479	8.411558
6.675236	474.882137	8.416576
6.826490	466.756360	8.421594
7.154493	467.252240	8.426611
6.649859	455.794075	8.431629
6.541392	446.592346	8.436646
6.575155	462.222738	8.441664
7.087576	463.073862	8.446682
7.149864	456.564122	8.451699
6.658603	436.501514	8.456717
6.614132	436.848965	8.461734
6.784373	451.694013	8.466752
7.059742	450.495912	8.471770
6.602883	455.121274	8.476787
6.765815	458.524443	8.481805
7.048180	462.695553	8.486822
6.815311	460.732855	8.491840
6.908007	449.031830	8.496858
6.680028	453.554425	8.501875
6.943464	449.356862	8.506893
7.002931	457.182702	8.511910
6.677772	449.257579	8.516928
6.711035	449.677594	8.521946
6.951094	477.227692	8.526963
6.936422	471.069449	8.531981
7.075373	475.356461	8.536998
6.667926	471.545570	8.542016
6.789222	456.592085	8.547034
6.372426	469.819871	8.552051
6.821515	469.216707	8.557069
6.775654	473.746603	8.562087
6.874158	470.331299	8.567104
6.989874	467.825303	8.572122
6.817009	455.271850	8.577139
7.119418	472.988863	8.582157
7.319722	468.314264	8.587175
6.758262	462.791707	8.592192
7.188104	461.328675	8.597210
6.751777	467.101904	8.602227
6.991391	457.478770	8.607245
7.105766	462.594316	8.612263
7.083280	469.553338	8.617280
7.291716	455.751275	8.622298
7.003583	469.814549	8.627315
7.157882	476.876902	8.632333
7.182178	473.476321	8.637351
7.018156	469.880939	8.642368
6.902734	460.837493	8.647386
6.649400	487.487919	8.652403
6.974715	463.311702	8.657421
6.765434	463.456630	8.662439
6.840378	470.188684	8.667456
7.084880	458.749592	8.672474
6.800454	469.271893	8.677491
7.101929	459.021284	8.682509
6.996980	461.096071	8.687527
6.852800	467.838653	8.692544
7.009144	458.867292	8.697562
6.813079	472.684218	8.702579
6.891242	465.434948	8.707597
6.854713	475.627391	8.712615
6.860058	469.481191	8.717632
7.309003	494.808034	8.722650
7.016384	505.287140	8.727667
7.131336	510.167238	8.732685
7.215360	488.129890	8.737703
7.000119	488.681695	8.742720
7.710278	483.761659	8.747738
7.199893	479.257834	8.752755
6.954016	469.538593	8.757773
7.308053	462.845832	8.762791
7.272634	464.968365	8.767808
7.121573	453.392536	8.772826
7.140012	466.051976	8.777843
7.196603	456.358132	8.782861
7.229916	469.476307	8.787879
7.178823	464.526904	8.792896
7.062361	459.933092	8.797914
6.943796	481.201891	8.802931
7.009130	466.882473	8.807949
7.150456	487.213992	8.812967
7.126572	498.366497	8.817984
7.358553	479.232256	8.823002
7.382050	494.928435	8.828019
7.415187	493.622370	8.833037
7.104610	477.495103	8.838055
7.061045	475.032942	8.843072
7.407499	487.814129	8.848090
7.186041	498.743942	8.853107
7.065268	490.141793	8.858125
7.403359	495.316024	8.863143
7.303483	500.722824	8.868160
7.376332	490.827901	8.873178
7.254044	497.456082	8.878195
7.262461	496.077844	8.883213
7.492554	495.772609	8.888231
7.234022	498.040845	8.893248
7.523400	491.107251	8.898266
6.890374	485.268650	8.903283
6.847439	497.022268	8.908301
7.151870	493.470792	8.913319
7.179790	502.943151	8.918336
7.306974	485.936568	8.923354
7.373693	491.556025	8.928371
7.564372	490.926588	8.933389
7.683212	496.941555	8.938407
7.393399	493.907654	8.943424
7.315758	490.536116	8.948442
7.400867	495.439739	8.953459
7.427826	503.015827	8.958477
7.233721	507.793103	8.963495
7.187541	497.795044	8.968512
7.244115	501.539727	8.973530
7.226477	497.480799	8.978547
7.318595	493.362211	8.983565
7.597838	487.094483	8.988583
7.230432	503.734260	8.993600
7.324498	489.638357	8.998618
7.198448	492.704356	9.003635
7.076681	495.988978	9.008653
7.236984	487.087301	9.013671
7.178768	498.360114	9.018688
7.531613	513.436489	9.023706
7.820294	524.488063	9.028723
7.466957	510.549124	9.033741
7.527268	500.327321	9.038759
7.470373	492.512329	9.043776
7.398312	481.165385	9.048794
7.840807	494.708643	9.053811
7.304244	490.424436	9.058829
7.396739	493.559507	9.063847
7.330820	504.046805	9.068864
7.502590	513.543516	9.073882
7.579952	512.299314	9.078899
7.680991	511.910809	9.083917
7.934660	505.268859	9.088935
7.363580	489.407403	9.093952
7.368627	494.411929	9.098970
7.545657	489.232057	9.103987
7.346023	497.754198	9.109005
7.757461	498.469199	9.114023
7.713954	513.643742	9.119040
7.526850	519.629574	9.124058
7.705582	500.213340	9.129075
7.619016	495.034912	9.134093
7.495737	491.507280	9.139111
7.691198	503.753055	9.144128
7.496552	499.927752	9.149146
7.661667	505.134900	9.154163
7.551269	507.161788	9.159181
7.655363	517.474878	9.164199
7.651376	530.577918	9.169216
7.618434	521.761783	9.174234
7.736787	531.867070	9.179251
7.712514	526.203959	9.184269
7.745859	500.630361	9.189287
7.646100	507.934854	9.194304
7.545348	504.450236	9.199322
7.542571	505.818962	9.204339
7.888748	533.235711	9.209357
7.877608	512.303718	9.214375
7.618550	511.695269	9.219392
7.402713	516.823092	9.224410
7.721550	526.416931	9.229427
7.681556	542.815982	9.234445
7.781081	528.593683	9.239463
7.771517	544.078505	9.244480
7.916071	531.893188	9.249498
8.306922	530.747238	9.254515
7.753527	514.437580	9.259533
7.985383	492.458253	9.264551
7.512590	489.602778	9.269568
7.699586	484.013893	9.274586
7.809790	491.137166	9.279603
7.593067	499.522899	9.284621
7.545495	492.911450	9.289639
7.598338	506.779669	9.294656
7.512917	513.760820	9.299674
8.085771	522.696803	9.304691
7.820400	535.804372	9.309709
8.025048	530.777557	9.314727
8.005005	531.958639	9.319744
8.145842	523.010467	9.324762
7.811487	503.305007	9.329779
7.737997	499.873447	9.334797
8.052703	508.701926	9.339815
7.852220	508.927858	9.344832
8.064342	484.112914	9.349850
8.015345	488.283687	9.354867
7.768709	499.034345	9.359885
7.654622	490.841805	9.364903
7.851637	513.987398	9.369920
7.649623	520.685836	9.374938
8.042680	513.961809	9.379955
7.880867	519.792814	9.384973
7.975066	524.657947	9.389991
8.139889	529.828547	9.395008
7.908741	514.718544	9.400026
8.049570	511.849531	9.405043
7.766521	508.306872	9.410061
7.989097	513.482486	9.415079
8.101108	521.701338	9.420096
7.918440	508.989564	9.425114
7.920278	504.483837	9.430131
7.694697	529.803243	9.435149
8.044143	528.792446	9.440167
7.916822	515.579331	9.445184
7.659075	532.147686	9.450202
7.833381	528.538396	9.455219
7.556126	529.311811	9.460237
7.896660	520.245427	9.465255
8.133491	528.256698	9.470272
7.820113	516.052508	9.475290
7.826046	522.270346	9.480307
7.854778	523.327159	9.485325
7.826740	503.886247	9.490343
7.904453	524.786049	9.495360
7.897319	530.841724	9.500378
8.040440	535.199600	9.505395
8.114911	553.189054	9.510413
8.518292	560.045564	9.515431
8.008933	545.201132	9.520448
7.839077	528.886132	9.525466
8.298917	540.582971	9.530483
7.899575	551.954114	9.535501
8.071327	551.736451	9.540519
8.371892	552.289020	9.545536
8.249552	561.549302	9.550554
8.256881	539.143555	9.555571
8.067213	536.238529	9.560589
8.236934	550.597374	9.565607
7.942104	535.838923	9.570624
8.088979	540.737568	9.575642
8.527155	548.372165	9.580659
8.050886	547.267766	9.585677
8.485574	529.684082	9.590695
8.103338	531.265478	9.595712
7.950860	522.313922	9.600730
8.585604	537.445774	9.605747
8.267698	544.397366	9.610765
8.417963	531.704353	9.615783
8.140263	522.610149	9.620800
7.952257	533.955210	9.625818
8.367686	523.834604	9.630835
8.200851	551.966012	9.635853
8.463098	537.597259	9.640871
8.293855	529.933751	9.645888
8.218613	532.829103	9.650906
8.321522	527.690790	9.655923
8.123315	528.461178	9.660941
8.210318	549.339603	9.665959
8.520401	545.053028	9.670976
8.460096	564.121766	9.675994
8.489640	539.834702	9.681011
7.962986	541.293843	9.686029
8.313584	550.036121	9.691047
8.299494	550.821250	9.696064
8.294960	552.777317	9.701082
8.376359	551.326103	9.706099
8.406914	547.704747	9.711117
8.654702	547.739605	9.716135
8.482979	539.360947	9.721152
8.268050	535.445705	9.726170
8.430965	526.262843	9.731187
8.082164	542.816343	9.736205
8.307840	531.479002	9.741223
8.551077	542.561715	9.746240
8.512728	551.356954	9.751258
8.640586	550.896612	9.756275
8.522950	551.433077	9.761293
8.292755	540.785170	9.766311
8.737938	542.274996	9.771328
8.233649	529.488732	9.776346
8.727542	546.921303	9.781363
8.311973	529.699722	9.786381
8.512310	523.380469	9.791399
8.610172	508.483647	9.796416
8.212393	523.393309	9.801434
8.673519	531.067991	9.806451
8.543579	521.023735	9.811469
8.679716	544.588182	9.816487
8.562885	522.187037	9.821504
8.216569	521.082516	9.826522
8.237629	537.276644	9.831539
8.511751	541.005360	9.836557
8.299733	545.136374	9.841575
8.386174	558.562100	9.846592
8.531443	552.639232	9.851610
8.903194	544.345024	9.856627
8.752646	576.064152	9.861645
8.740712	554.100720	9.866663
8.947190	557.799488	9.871680
8.515988	552.445872	9.876698
8.811231	546.691477	9.881715
8.532734	545.829911	9.886733
8.382642	535.978885	9.891751
9.046055	538.335847	9.896768
8.520999	545.037496	9.901786
8.502792	535.293185	9.906803
8.847517	534.729701	9.911821
8.617879	528.507577	9.916839
8.750854	526.840615	9.921856
8.531046	513.709008	9.926874
8.706874	540.053531	9.931891
8.730756	550.056463	9.936909
8.795358	542.596660	9.941927
8.683452	538.603385	9.946944
8.404331	542.681036	9.951962
8.733374	538.092986	9.956979
8.690535	548.103794	9.961997
8.591926	544.404106	9.967015
8.559801	549.678304	9.972032
8.610158	546.875108	9.977050
8.427332	550.528494	9.982067
8.748814	548.453906	9.987085
8.428024	555.942350	9.992103
8.962295	551.640176	9.997120
8.508945	551.419643	10.002138
8.887736	543.635058	10.007155
8.785877	549.490902	10.012173
8.735009	549.149737	10.017191
8.701316	536.999481	10.022208
8.495083	556.316672	10.027226
8.894420	538.961988	10.032243
8.740015	538.038785	10.037261
8.579278	553.258618	10.042279
9.013656	548.285147	10.047296
8.674989	554.273113	10.052314
8.783876	550.458545	10.057331
8.891335	559.824808	10.062349
9.018764	567.999515	10.067367
9.046363	549.853428	10.072384
8.568219	547.276410	10.077402
9.066391	571.640877	10.082419
9.121691	557.355701	10.087437
8.668377	547.657209	10.092455
8.999518	550.431387	10.097472
9.186432	566.207396	10.102490
9.084467	554.018225	10.107507
9.057210	554.791065	10.112525
8.847304	550.610198	10.117543
9.039779	534.006440	10.122560
8.645752	544.507644	10.127578
8.733643	557.333587	10.132595
9.238734	559.558589	10.137613
9.205744	575.086477	10.142631
9.161312	535.292496	10.147648
9.100371	561.870619	10.152666
9.165220	546.371702	10.157683
9.203522	546.503169	10.162701
8.994248	548.229460	10.167719
9.343163	550.422707	10.172736
9.089153	556.375331	10.177754
8.943723	543.131631	10.182771
8.726596	551.967238	10.187789
8.790477	547.036200	10.192807
8.854023	543.892333	10.197824
8.923479	557.662800	10.202842
9.131926	560.933504	10.207859
9.122372	568.100417	10.212877
9.249430	582.107186	10.217895
9.326520	567.702683	10.222912
8.743923	561.938569	10.227930
9.170253	578.261187	10.232947
9.522457	585.531175	10.237965
9.177510	576.601357	10.242983
9.086759	567.702057	10.248000
8.900245	562.251717	10.253018
8.957780	569.012866	10.258035
8.846795	570.651577	10.263053
9.163191	578.199749	10.268071
8.955482	576.277354	10.273088
9.205980	585.621472	10.278106
9.100650	577.892372	10.283123
9.469398	581.653873	10.288141
9.241590	581.920237	10.293159
9.424919	580.293164	10.298176
9.277935	581.859796	10.303194
9.285097	583.499943	10.308211
9.455512	582.276865	10.313229
8.988917	582.799561	10.318247
9.174455	587.726370	10.323264
9.122669	587.338616	10.328282
9.328475	585.029762	10.333299
9.345359	576.413180	10.338317
8.924257	582.583139	10.343335
9.333704	573.704888	10.348352
9.357355	577.828846	10.353370
8.944295	575.328544	10.358387
9.092666	578.439245	10.363405
8.984580	583.030821	10.368423
9.488641	594.002967	10.373440
9.433908	598.560146	10.378458
9.342973	595.209478	10.383475
9.554284	589.512037	10.388493
9.110582	589.201841	10.393511
9.477531	602.556748	10.398528
9.448913	610.502313	10.403546
9.544064	593.325361	10.408563
9.816729	579.304360	10.413581
9.449306	584.625912	10.418599
9.901317	576.413377	10.423616
9.553328	575.922842	10.428634
9.346576	556.901744	10.433651
9.878517	573.701161	10.438669
9.568836	579.684149	10.443687
9.774008	572.747608	10.448704
9.593878	580.300887	10.453722
9.671904	581.087128	10.458739
9.562242	581.518170	10.463757
9.638302	574.583876	10.468775
9.983409	571.529560	10.473792
9.883851	583.957286	10.478810
9.737870	554.779757	10.483827
9.718483	541.872514	10.488845
9.414333	549.377097	10.493863
9.489175	546.524198	10.498880
9.397172	544.152783	10.503898
8.975322	547.782202	10.508915
9.799824	542.414923	10.513933
9.580146	572.839327	10.518951
9.605576	568.359988	10.523968
9.763297	571.838336	10.528986
9.630107	574.861350	10.534003
10.065623	566.888688	10.539021
9.386167	563.994339	10.544039
9.356017	553.821594	10.549056
9.661035	561.044560	10.554074
9.350109	571.629267	10.559091
9.447071	578.217217	10.564109
9.670743	578.064281	10.569127
9.967710	584.551877	10.574144
9.834319	578.936495	10.579162
9.701231	578.929499	10.584179
10.175473	579.992200	10.589197
9.731462	577.593935	10.594215
9.789308	577.176354	10.599232
9.736743	576.691708	10.604250
9.699790	582.254434	10.609267
9.880275	575.834826	10.614285
9.540519	580.755945	10.619303
9.691291	574.322257	10.624320
9.883214	572.450720	10.629338
9.548431	596.345462	10.634355
10.061597	576.437563	10.639373
9.531633	589.613208	10.644391
9.458822	572.854580	10.649408
9.694646	570.896085	10.654426
9.090402	577.329415	10.659443
9.357581	578.484880	10.664461
9.574045	576.157341	10.669479
9.667145	582.530438	10.674496
9.967348	592.578064	10.679514
9.582776	608.391880	10.684531
9.918531	606.732038	10.689549
9.970735	604.963290	10.694567
10.055194	611.811716	10.699584
10.126569	602.873402	10.704602
9.984039	597.530711	10.709619
10.144993	609.206639	10.714637
9.797881	587.584004	10.719655
9.805833	589.625587	10.724672
9.733215	597.166912	10.729690
9.951609	595.749340	10.734707
10.249495	592.381059	10.739725
9.914342	613.801846	10.744743
9.844781	594.035487	10.749760
9.587910	595.697719	10.754778
9.431598	595.108005	10.759795
9.951447	596.534823	10.764813
9.833438	610.091205	10.769831
9.652281	600.994972	10.774848
10.163947	595.816836	10.779866
9.854180	603.206263	10.784883
10.168942	605.408114	10.789901
10.101327	595.149136	10.794919
9.845358	589.535901	10.799936
9.994151	591.849898	10.804954
9.935290	600.266177	10.809971
10.079465	596.163067	10.814989
10.110758	604.359190	10.820007
10.217582	590.735958	10.825024
10.286771	596.288626	10.830042
10.456838	602.299991	10.835059
10.316667	599.931018	10.840077
10.339303	609.586059	10.845095
10.039628	601.365778	10.850112
10.387938	595.854596	10.855130
10.255957	605.029021	10.860147
10.156298	594.456132	10.865165
9.980864	610.063092	10.870183
10.008544	603.931450	10.875200
10.148530	590.685805	10.880218
9.989742	606.622599	10.885235
10.163047	596.390816	10.890253
10.029001	598.633673	10.895271
10.324890	610.747713	10.900288
10.518324	618.403799	10.905306
10.721542	604.848855	10.910323
10.516691	593.325400	10.915341
10.320543	599.116748	10.920359
10.288932	592.752551	10.925376
10.404482	595.132558	10.930394
10.512702	584.185355	10.935411
10.606929	590.607468	10.940429
10.352687	596.268295	10.945447
10.073512	586.371263	10.950464
10.427223	589.764779	10.955482
10.281215	591.927253	10.960499
10.342178	597.966190	10.965517
10.432057	593.249483	10.970535
10.017395	589.499187	10.975552
10.463714	595.501305	10.980570
10.234290	600.928172	10.985587
10.173322	598.483528	10.990605
10.393686	593.123672	10.995623
10.693311	582.331601	11.000640
10.512491	598.113900	11.005658
10.366399	592.098554	11.010675
10.568489	583.766434	11.015693
10.346428	600.394499	11.020711
10.704054	592.107322	11.025728
10.646448	598.142829	11.030746
10.412149	599.777618	11.035763
10.422824	594.498464	11.040781
10.386236	596.634491	11.045799
10.263072	608.739356	11.050816
10.465589	589.537523	11.055834
10.476432	607.480387	11.060851
10.507044	610.320278	11.065869
10.463913	624.286627	11.070887
10.195623	621.689282	11.075904
10.639609	620.688736	11.080922
10.336993	640.079327	11.085939
10.447350	627.171924	11.090957
10.625015	637.640511	11.095975
10.926975	628.261034	11.100992
11.028111	629.645662	11.106010
10.753952	638.335962	11.111027
11.081294	626.270520	11.116045
10.651267	613.698033	11.121063
10.503477	604.347434	11.126080
10.664467	596.966532	11.131098
10.650011	602.935576	11.136115
10.985781	610.358941	11.141133
10.613671	600.262157	11.146151
10.309666	591.415403	11.151168
10.847474	601.085671	11.156186
10.439356	630.375696	11.161203
10.884789	624.308931	11.166221
10.937793	628.992765	11.171239
10.789325	628.334941	11.176256
10.993870	623.149592	11.181274
10.600862	622.038019	11.186291
10.816414	621.893903	11.191309
10.730633	625.265396	11.196327
10.853139	635.630135	11.201344
10.845829	626.462354	11.206362
10.748186	627.844210	11.211379
10.636208	619.487418	11.216397
10.985546	610.343660	11.221415
10.677372	630.809085	11.226432
10.822736	627.619996	11.231450
10.757037	630.427296	11.236467
10.882350	628.394365	11.241485
11.002315	630.153241	11.246503
11.034586	628.883813	11.251520
11.101230	625.197239	11.256538
10.795765	631.815701	11.261555
10.842679	634.070479	11.266573
10.981775	621.055799	11.271591
10.991851	639.202611	11.276608
11.156718	613.489601	11.281626
10.916611	639.733588	11.286643
11.113214	626.140851	11.291661
11.068512	627.634693	11.296679
11.184275	624.742840	11.301696
11.177165	618.304327	11.306714
10.874278	607.442659	11.311731
10.804768	615.704842	11.316749
11.156868	610.203065	11.321767
11.106352	622.901876	11.326784
11.310775	616.624320	11.331802
11.142704	608.777753	11.336819
10.999682	598.269885	11.341837
11.199572	614.830401	11.346855
11.099109	604.675342	11.351872
11.194590	604.088298	11.356890
10.978206	601.732804	11.361907
10.850290	616.724600	11.366925
10.969359	610.260516	11.371943
10.935281	610.190517	11.376960
11.267692	611.363938	11.381978
11.024330	614.114004	11.386995
11.053021	620.982474	11.392013
11.331175	613.979538	11.397031
10.937794	622.056333	11.402048
11.185447	614.155331	11.407066
11.175343	629.501488	11.412083
11.431215	627.513893	11.417101
11.544028	617.592504	11.422119
11.053025	634.168225	11.427136
11.269260	621.492969	11.432154
11.349655	622.683438	11.437171
11.158523	638.278752	11.442189
11.209821	616.804156	11.447207
11.424186	631.873521	11.452224
11.570680	617.391082	11.457242
11.293716	613.243321	11.462259
11.038372	614.984022	11.467277
11.014099	621.934749	11.472295
11.089802	616.022074	11.477312
11.137066	633.236208	11.482330
11.186357	625.820223	11.487347
10.899658	629.397019	11.492365
11.177438	618.965917	11.497383
10.755315	639.612740	11.502400
11.076214	635.552541	11.507418
11.296479	652.061514	11.512435
10.997937	645.317012	11.517453
11.412151	648.865559	11.522471
11.283277	661.795503	11.527488
11.590760	651.075982	11.532506
11.475482	656.820335	11.537523
11.394961	646.312438	11.542541
11.801174	640.267597	11.547559
11.588109	660.350216	11.552576
11.616903	646.462246	11.557594
11.688938	653.771284	11.562611
11.445887	657.806303	11.567629
11.897644	639.924770	11.572647
11.770335	653.677459	11.577664
11.672254	650.771642	11.582682
11.719057	655.749739	11.587699
11.458340	653.652579	11.592717
11.633178	648.924964	11.597735
11.829814	648.060051	11.602752
11.548900	649.096999	11.607770
11.874658	650.293957	11.612787
11.509667	646.972921	11.617805
11.686107	647.961447	11.622823
11.384498	652.409086	11.627840
11.627579	640.737280	11.632858
11.775991	647.305245	11.637875
11.564428	656.487539	11.642893
11.740369	662.385290	11.647911
11.511732	651.606177	11.652928
11.462311	643.162578	11.657946
11.445586	657.203115	11.662963
11.646944	652.056364	11.667981
11.797407	637.150723	11.672999
11.584301	648.992112	11.678016
11.320576	649.377375	11.683034
11.625498	646.211606	11.688051
11.159975	653.404021	11.693069
11.722082	664.270293	11.698087
11.837509	681.210195	11.703104
12.241626	670.836507	11.708122
12.184041	675.560967	11.713139
11.887375	669.003792	11.718157
11.969271	649.236735	11.723175
11.683280	665.950711	11.728192
11.821890	650.959637	11.733210
11.835160	644.464315	11.738227
11.710378	654.706786	11.743245
12.112170	667.177681	11.748263
12.020219	671.433337	11.753280
11.969221	644.459733	11.758298
11.925895	647.061817	11.763315
11.702721	656.111616	11.768333
12.071579	659.875677	11.773351
11.951452	669.452505	11.778368
12.122973	683.005483	11.783386
11.922657	662.053282	11.788403
11.973492	666.829883	11.793421
12.030634	664.765999	11.798439
11.925308	661.020063	11.803456
11.991709	669.680965	11.808474
12.474057	673.162859	11.813491
11.966392	655.573975	11.818509
12.174158	645.191228	11.823527
11.963222	639.529500	11.828544
11.601159	642.631776	11.833562
12.059096	656.429251	11.838579
12.001368	667.280172	11.843597
12.050896	671.801251	11.848615
12.064106	669.549106	11.853632
12.193645	676.924618	11.858650
12.401441	673.524369	11.863667
12.171420	672.984323	11.868685
12.523319	672.103492	11.873703
12.280681	683.335578	11.878720
11.900084	676.351046	11.883738
12.282149	680.705491	11.888755
12.243544	662.741230	11.893773
12.267295	666.555533	11.898791
12.295043	672.936712	11.903808
12.291151	672.322398	11.908826
12.417249	679.801897	11.913843
12.309045	673.710394	11.918861
12.502477	669.874445	11.923879
11.996341	665.299900	11.928896
12.036269	665.204191	11.933914
12.265905	668.635744	11.938931
12.116892	679.499594	11.943949
12.394610	669.965281	11.948967
12.368675	677.837425	11.953984
12.192647	672.303936	11.959002
12.487696	675.476223	11.964019
12.084520	684.656743	11.969037
12.421643	668.155084	11.974055
12.473355	677.672229	11.979072
12.343175	674.854269	11.984090
12.294004	678.329340	11.989107
12.122609	686.376668	11.994125
12.572215	668.563648	11.999143
12.426710	683.854598	12.004160
12.348075	674.321411	12.009178
12.499688	682.585760	12.014195
12.131278	679.013969	12.019213
12.292817	669.205822	12.024231
12.601205	676.439897	12.029248
12.396950	673.591276	12.034266
12.559240	672.386163	12.039283
12.342898	676.193701	12.044301
12.574787	681.162671	12.049319
12.788838	677.387372	12.054336
12.583689	688.507979	12.059354
12.708870	675.658601	12.064371
12.424000	671.988088	12.069389
12.856584	677.892240	12.074407
13.067275	682.401646	12.079424
12.820213	679.734363	12.084442
12.789821	676.952654	12.089459
12.533213	678.689143	12.094477
12.620412	662.065645	12.099495
12.731527	689.212546	12.104512
12.449592	675.505786	12.109530
12.896602	671.209341	12.114547
12.261343	680.062362	12.119565
12.449912	668.104346	12.124583
12.735394	669.164889	12.129600
12.567277	690.130142	12.134618
12.939655	667.803017	12.139635
12.648377	702.267489	12.144653
13.005531	689.752797	12.149671
12.804929	680.089899	12.154688
12.473504	682.280959	12.159706
12.645942	673.046449	12.164723
12.756569	695.344221	12.169741
13.101640	698.102643	12.174759
13.307882	704.085045	12.179776
12.799829	687.558609	12.184794
12.687211	679.529953	12.189811
12.988274	698.823712	12.194829
12.964677	699.000932	12.199847
12.943198	684.471010	12.204864
12.803988	699.805905	12.209882
13.071978	688.722607	12.214899
12.957690	697.597884	12.219917
12.719049	686.642886	12.224935
13.065278	697.547120	12.229952
13.046579	704.676346	12.234970
12.957235	698.592737	12.239987
12.849313	700.057084	12.245005
12.819593	707.276790	12.250023
13.179244	688.423179	12.255040
12.879778	700.799511	12.260058
13.217257	696.217794	12.265075
13.029297	706.524761	12.270093
12.922777	702.192944	12.275111
13.023753	692.002668	12.280128
12.885273	712.618361	12.285146
13.275813	684.013168	12.290163
13.157333	707.862597	12.295181
12.955202	701.953392	12.300199
12.991921	692.986903	12.305216
12.702043	710.797938	12.310234
13.328465	690.816760	12.315251
13.162599	709.329847	12.320269
13.093046	698.332433	12.325287
13.212154	697.558458	12.330304
13.079848	703.550164	12.335322
13.111026	691.161861	12.340339
13.173981	694.663671	12.345357
12.994411	696.092134	12.350375
13.259738	690.163050	12.355392
13.380910	697.121559	12.360410
13.277394	695.743596	12.365427
13.274061	692.844155	12.370445
13.245766	692.634752	12.375463
13.353122	695.934787	12.380480
13.173558	715.239998	12.385498
13.724726	708.195346	12.390515
13.643061	712.354949	12.395533
13.394994	707.377306	12.400551
13.550376	697.635889	12.405568
13.456483	702.756906	12.410586
13.206417	693.779949	12.415603
13.430561	700.264870	12.420621
13.297576	705.687841	12.425639
13.437433	703.341554	12.430656
13.208557	702.981586	12.435674
13.480355	715.833259	12.440691
13.692882	722.193370	12.445709
13.535229	726.186545	12.450727
13.645920	688.501804	12.455744
13.440059	688.563316	12.460762
13.716941	702.177128	12.465779
13.472454	690.176810	12.470797
13.636456	688.296589	12.475815
13.658765	687.748005	12.480832
13.273059	689.458302	12.485850
13.660665	699.314338	12.490867
13.751713	693.628270	12.495885
13.365180	699.624890	12.500903
13.910518	694.068912	12.505920
13.603219	698.988543	12.510938
13.744442	695.529328	12.515955
13.874892	681.884694	12.520973
13.591237	685.951817	12.525991
13.465831	686.279094	12.531008
13.459735	692.199559	12.536026
14.022248	710.605367	12.541043
13.717489	708.800444	12.546061
13.608495	699.751070	12.551079
13.700417	707.432636	12.556096
13.857364	722.947982	12.561114
13.910411	724.375399	12.566131
13.591445	715.830277	12.571149
13.671193	726.785261	12.576167
14.123763	723.651656	12.581184
14.088835	725.187583	12.586202
13.765344	708.965478	12.591219
13.676579	705.357505	12.596237
13.471979	717.561325	12.601255
13.916661	721.267804	12.606272
13.689092	727.230687	12.611290
13.871835	720.909833	12.616307
13.933471	727.367795	12.621325
13.938538	720.366151	12.626343
13.879916	722.190172	12.631360
13.788380	725.815328	12.636378
13.545204	715.821046	12.641395
13.740591	724.355966	12.646413
13.509041	729.964088	12.651431
13.909089	726.240007	12.656448
13.836299	721.903004	12.661466
13.845086	728.747949	12.666483
14.223980	740.948054	12.671501
13.740125	748.278842	12.676519
14.055979	743.407945	12.681536
13.813446	750.004939	12.686554
13.990661	739.123467	12.691571
14.333041	737.180602	12.696589
13.954671	756.199903	12.701607
14.490886	750.894658	12.706624
14.269238	753.154966	12.711642
14.404504	756.967297	12.716659
14.382195	755.353426	12.721677
14.127667	751.697461	12.726695
14.495304	747.897452	12.731712
14.328880	730.044959	12.736730
14.251793	710.499616	12.741747
14.313564	708.289526	12.746765
13.910906	716.359933	12.751783
14.062809	714.765690	12.756800
14.029043	727.636086	12.761818
14.324850	733.816538	12.766835
14.634845	741.975829	12.771853
14.443357	744.052457	12.776871
14.618777	741.960456	12.781888
14.623086	726.844689	12.786906
14.532494	712.909672	12.791923
14.578006	724.955070	12.796941
14.237863	722.943055	12.801959
14.352526	705.750354	12.806976
14.453878	719.744869	12.811994
14.432625	704.234141	12.817011
14.241883	708.055660	12.822029
14.364750	723.787509	12.827047
14.330067	701.156342	12.832064
14.248110	706.237208	12.837082
14.488560	714.208325	12.842099
14.816835	719.264207	12.847117
14.465518	721.566504	12.852135
14.872140	704.850224	12.857152
14.897535	707.772274	12.862170
14.518429	707.941331	12.867187
14.482198	699.793376	12.872205
14.272738	708.820277	12.877223
14.482331	704.136593	12.882240
14.480842	720.163524	12.887258
14.465577	711.229624	12.892275
14.805855	724.290403	12.897293
14.694813	732.556364	12.902311
14.657461	719.718950	12.907328
14.681579	712.597853	12.912346
14.468005	731.370164	12.917363
14.819718	731.257075	12.922381
14.739031	737.447298	12.927399
14.754061	724.611260	12.932416
14.628733	731.047083	12.937434
14.693666	747.043287	12.942451
14.955560	731.627731	12.947469
14.698337	736.047789	12.952487
14.830332	738.267661	12.957504
14.657454	754.149077	12.962522
14.645969	735.814791	12.967539
14.623369	746.938238	12.972557
14.666057	740.425418	12.977575
14.888819	739.743830	12.982592
14.815575	739.767978	12.987610
14.492881	738.305986	12.992627
15.302964	741.888815	12.997645
14.886936	756.477491	13.002663
14.624548	744.928399	13.007680
14.844282	747.557975	13.012698
15.207666	736.150691	13.017715
14.830425	736.367951	13.022733
15.071353	742.498534	13.027751
15.064828	739.646154	13.032768
15.075327	740.384425	13.037786
15.076016	735.703274	13.042803
15.120888	741.532876	13.047821
14.997514	762.414181	13.052839
15.010397	743.410675	13.057856
15.472626	737.463598	13.062874
15.146446	751.183803	13.067891
15.209405	735.357138	13.072909
14.940421	761.109974	13.077927
15.038263	747.524692	13.082944
14.861113	746.241843	13.087962
14.953914	738.060737	13.092979
15.057081	737.807863	13.097997
14.918882	746.656910	13.103015
15.160618	745.015937	13.108032
14.882494	740.539873	13.113050
14.632363	762.481129	13.118067
15.275381	761.761777	13.123085
15.476132	777.982454	13.128103
15.367257	772.585235	13.133120
15.694029	767.623769	13.138138
15.555741	772.614877	13.143155
15.501041	748.214665	13.148173
15.332543	739.411458	13.153191
15.279283	736.144273	13.158208
15.187897	741.297557	13.163226
15.521361	760.212317	13.168243
15.528989	748.691712	13.173261
15.443321	734.161624	13.178279
15.232472	732.834949	13.183296
15.502701	742.638873	13.188314
15.147525	734.656669	13.193331
15.543465	745.625538	13.198349
15.491565	768.085181	13.203367
15.444811	776.359632	13.208384
15.820454	772.251483	13.213402
15.381317	763.402949	13.218419
15.596304	750.230577	13.223437
15.685407	766.975370	13.228455
15.519240	750.967613	13.233472
15.598311	760.713595	13.238490
15.493956	757.250670	13.243507
15.844891	754.646223	13.248525
15.723160	750.042370	13.253543
15.545484	739.334772	13.258560
15.654235	741.480356	13.263578
15.521693	746.070118	13.268595
15.841852	757.997241	13.273613
15.896076	746.142643	13.278631
15.739063	737.185511	13.283648
15.779823	727.685400	13.288666
15.204413	732.557738	13.293683
15.690668	743.707890	13.298701
15.831831	759.346815	13.303719
15.623623	755.934213	13.308736
16.041832	764.466085	13.313754
15.904842	753.276284	13.318771
15.850813	762.353593	13.323789
15.789042	762.719261	13.328807
16.057490	771.071311	13.333824
15.745004	757.972422	13.338842
15.926896	762.684887	13.343859
15.893791	761.617640	13.348877
16.050879	769.577075	13.353895
16.116173	759.954023	13.358912
16.079171	729.658039	13.363930
15.732372	741.559673	13.368947
15.667282	740.405316	13.373965
15.820224	755.605198	13.378983
15.921649	758.950704	13.384000
16.259854	762.700176	13.389018
15.962743	760.799912	13.394035
15.984678	757.783516	13.399053
15.735846	756.035174	13.404071
15.769718	755.694859	13.409088
15.688861	753.358667	13.414106
15.486198	761.824776	13.419123
15.737791	751.638697	13.424141
15.564257	770.427070	13.429159
15.945639	789.563417	13.434176
16.236784	781.093178	13.439194
16.181771	793.098465	13.444211
16.480200	786.208999	13.449229
16.282436	800.985509	13.454247
16.250291	790.318573	13.459264
16.524705	792.666946	13.464282
16.320291	798.037597	13.469299
16.424494	787.432853	13.474317
16.100097	787.587360	13.479335
16.200399	799.023423	13.484352
16.458474	780.772752	13.489370
16.301723	803.038115	13.494387
16.532416	787.948148	13.499405
16.437604	766.671261	13.504423
16.118689	766.984861	13.509440
16.214466	770.743500	13.514458
16.202625	778.979119	13.519475
16.518723	771.189824	13.524493
16.104964	781.538191	13.529511
16.336114	787.474788	13.534528
16.544135	786.614972	13.539546
16.261719	792.791518	13.544563
16.378815	780.218613	13.549581
15.930410	786.529253	13.554599
16.370889	795.655144	13.559616
16.084977	788.922660	13.564634
16.119112	795.210831	13.569651
16.317733	810.508606	13.574669
16.531541	832.180995	13.579687
16.713794	825.648544	13.584704
16.777314	826.698743	13.589722
16.784449	832.693213	13.594739
16.733060	823.715747	13.599757
16.839669	830.866513	13.604775
16.804473	802.943725	13.609792
16.446418	796.763278	13.614810
15.989981	792.884534	13.619827
16.752909	810.594127	13.624845
17.164562	827.944867	13.629863
16.766685	819.178929	13.634880
17.091171	812.096906	13.639898
16.894012	824.199015	13.644915
17.124636	812.728694	13.649933
16.953594	794.523631	13.654951
16.458319	791.678209	13.659968
16.646126	787.748303	13.664986
16.641395	809.007701	13.670003
17.053966	814.746063	13.675021
16.980292	804.401156	13.680039
16.847204	817.641692	13.685056
17.432957	800.373101	13.690074
17.035976	792.325155	13.695091
16.836611	783.496421	13.700109
16.965559	781.072909	13.705127
16.779465	785.832416	13.710144
17.111975	795.020134	13.715162
17.177984	810.346121	13.720179
17.311865	780.805555	13.725197
17.011848	781.230175	13.730215
16.608076	786.027327	13.735232
17.300776	792.287650	13.740250
17.148673	809.425409	13.745267
16.938174	785.046555	13.750285
17.328801	795.929255	13.755303
17.257825	798.582478	13.760320
17.112197	777.323420	13.765338
16.873269	794.581783	13.770355
17.152039	801.351247	13.775373
17.235814	809.401933	13.780391
17.228279	809.038349	13.785408
17.520547	817.234459	13.790426
17.060134	818.259556	13.795443
17.009558	809.487399	13.800461
17.155056	808.658282	13.805479
17.087384	815.728840	13.810496
17.573971	798.756096	13.815514
17.320346	808.737455	13.820531
17.509648	806.057374	13.825549
17.242868	808.344041	13.830567
17.141372	817.793702	13.835584
17.444192	806.489461	13.840602
17.559210	812.398420	13.845619
17.177563	801.557303	13.850637
17.228822	814.477878	13.855655
17.279893	811.394075	13.860672
17.406853	801.923068	13.865690
17.560552	808.791825	13.870707
17.671304	812.540030	13.875725
17.793014	797.927002	13.880743
17.213339	817.077454	13.885760
17.510924	805.879859	13.890778
17.546227	806.883454	13.895795
17.395547	801.742774	13.900813
17.476728	802.225629	13.905831
17.242259	811.130967	13.910848
17.640129	808.325498	13.915866
17.456355	817.075058	13.920883
17.477609	832.179756	13.925901
17.725751	829.302003	13.930919
17.536211	845.669118	13.935936
18.015821	837.832695	13.940954
17.813130	831.646042	13.945971
17.741016	840.495539	13.950989
18.110891	833.794097	13.956007
17.694607	818.897632	13.961024
17.787191	817.116184	13.966042
17.587043	819.692552	13.971059
17.459758	826.855229	13.976077
18.133409	828.127159	13.981095
17.957716	825.750244	13.986112
18.283302	835.848818	13.991130
18.127153	825.259347	13.996147
17.642031	820.918918	14.001165
18.186179	822.136480	14.006183
18.009311	822.018540	14.011200
18.096187	818.984020	14.016218
17.569863	809.678924	14.021235
18.145327	821.578962	14.026253
17.979219	815.378989	14.031271
18.025702	825.155292	14.036288
18.068320	823.062496	14.041306
18.057246	833.808384	14.046323
18.034474	822.993677	14.051341
18.130482	826.084646	14.056359
17.859096	838.382426	14.061376
18.445044	833.441480	14.066394
18.192878	821.885941	14.071411
18.169507	832.739543	14.076429
18.627139	832.494314	14.081447
17.944854	837.986261	14.086464
18.288012	826.410962	14.091482
17.998996	831.244932	14.096499
18.350646	827.884862	14.101517
18.200894	827.723966	14.106535
18.273129	827.389610	14.111552
18.539703	825.490848	14.116570
18.541810	834.792009	14.121587
18.504821	831.144553	14.126605
18.360187	821.952928	14.131623
18.044192	828.057891	14.136640
18.368599	827.485947	14.141658
18.296821	829.278280	14.146675
17.998141	812.981435	14.151693
18.310604	827.473311	14.156711
17.896847	830.945665	14.161728
18.063895	830.364892	14.166746
18.292465	825.043476	14.171763
17.864578	835.551137	14.176781
18.619133	842.163274	14.181799
18.673614	860.424043	14.186816
18.865425	866.402006	14.191834
18.686625	853.241090	14.196851
18.456745	824.847410	14.201869
18.591234	846.290174	14.206887
18.497980	861.139016	14.211904
18.661183	854.725591	14.216922
18.886060	864.902746	14.221939
18.777767	856.222657	14.226957
18.899795	833.625323	14.231975
18.604377	832.984787	14.236992
18.706243	838.539032	14.242010
18.743086	830.503310	14.247027
19.044917	842.262508	14.252045
18.743694	836.842735	14.257063
18.560037	837.747313	14.262080
18.498653	838.323987	14.267098
18.685510	859.952678	14.272115
18.516699	870.303037	14.277133
18.838813	858.037343	14.282151
18.735746	870.824356	14.287168
18.879528	864.292809	14.292186
18.876938	861.227605	14.297203
18.831270	862.106331	14.302221
18.805975	859.425394	14.307239
18.826839	852.443416	14.312256
18.833661	854.441729	14.317274
18.808644	855.011902	14.322291
18.749100	872.923708	14.327309
19.072009	883.727526	14.332327
18.724712	879.764598	14.337344
19.300887	881.969539	14.342362
19.577067	889.474524	14.347379
19.428665	869.700959	14.352397
19.110981	854.885754	14.357415
19.139972	870.565273	14.362432
18.894278	851.118953	14.367450
19.162372	861.133294	14.372467
18.990917	876.288799	14.377485
19.479449	883.525972	14.382503
19.412365	899.764963	14.387520
19.599159	894.980783	14.392538
19.678043	859.498659	14.397555
19.160356	873.510595	14.402573
19.333162	855.583199	14.407591
19.039735	858.474127	14.412608
19.330841	855.181891	14.417626
19.110950	863.235259	14.422643
19.372244	875.408265	14.427661
19.614141	872.094539	14.432679
19.724906	875.345046	14.437696
19.206371	871.957624	14.442714
19.515674	864.251471	14.447731
19.405865	881.823649	14.452749
19.736968	871.590304	14.457767
19.754382	876.702825	14.462784
19.202590	872.598933	14.467802
19.555677	863.392511	14.472819
19.386151	881.373473	14.477837
19.633824	872.822595	14.482855
19.512912	877.513105	14.487872
19.564831	883.685902	14.492890
19.950701	874.156222	14.497907
19.627586	892.322184	14.502925
19.999265	873.471966	14.507943
19.718479	881.161681	14.512960
19.676919	891.626523	14.517978
19.713327	889.521164	14.522995
19.663160	882.522670	14.528013
19.648878	895.095671	14.533031
19.485666	885.304840	14.538048
19.844037	894.442392	14.543066
19.726604	886.356859	14.548083
19.608339	892.784596	14.553101
19.792395	883.525898	14.558119
19.855151	888.130267	14.563136
19.585646	872.022068	14.568154
20.058565	873.373225	14.573171
19.439408	876.154836	14.578189
19.577088	886.376918	14.583207
19.661160	894.617710	14.588224
19.906851	909.830562	14.593242
20.178188	913.178133	14.598259
19.902301	929.574171	14.603277
20.244451	926.879733	14.608295
20.124190	925.951945	14.613312
19.976547	919.240736	14.618330
20.111028	902.209262	14.623347
20.041578	912.290634	14.628365
20.385948	909.267174	14.633383
20.088041	913.831668	14.638400
20.108251	920.457935	14.643418
20.281134	911.198214	14.648435
20.088185	923.625216	14.653453
20.329125	905.793661	14.658471
20.090923	907.413087	14.663488
20.136058	902.144861	14.668506
20.385246	901.521089	14.673523
19.784485	910.924013	14.678541
20.248108	906.876960	14.683559
20.110684	917.102213	14.688576
20.285853	910.926197	14.693594
20.457760	907.458716	14.698611
20.034820	909.186210	14.703629
20.344671	911.351329	14.708647
20.492391	916.583043	14.713664
20.545241	950.891329	14.718682
20.577012	928.182226	14.723699
20.297029	941.202125	14.728717
20.304187	937.899821	14.733735
20.337263	937.807604	14.738752
20.468850	944.007603	14.743770
20.578554	930.820691	14.748787
20.692378	939.819297	14.753805
20.911285	946.747206	14.758823
20.841961	945.617739	14.763840
20.665570	954.834449	14.768858
20.840711	940.399615	14.773875
20.396235	946.487284	14.778893
20.762233	942.475739	14.783911
20.819925	934.792729	14.788928
20.646180	955.012411	14.793946
20.874194	937.281849	14.798963
20.856899	943.081851	14.803981
20.868546	941.601193	14.808999
20.926494	928.418703	14.814016
20.655669	948.324578	14.819034
20.828529	930.795610	14.824051
20.669354	942.993185	14.829069
20.798214	945.180444	14.834087
20.747110	926.826400	14.839104
20.611976	925.274845	14.844122
20.581657	934.038670	14.849139
20.966504	942.991113	14.854157
21.010356	945.897366	14.859175
20.848702	952.906764	14.864192
20.969744	954.642573	14.869210
21.064742	961.980634	14.874227
21.109338	958.168718	14.879245
21.072834	960.014203	14.884263
21.063728	965.224913	14.889280
21.188062	971.234535	14.894298
21.276428	969.297898	14.899315
21.244239	980.576113	14.904333
21.306156	962.337765	14.909351
21.504113	969.868312	14.914368
21.226070	970.683698	14.919386
21.543921	970.153965	14.924403
21.248301	965.980948	14.929421
21.232057	967.312286	14.934439
21.513800	961.603461	14.939456
21.491081	960.129563	14.944474
21.521008	956.025261	14.949491
21.273865	958.732421	14.954509
21.196375	954.644886	14.959527
21.424811	958.315228	14.964544
21.526955	955.785319	14.969562
21.436211	961.238005	14.974579
21.503352	964.471829	14.979597
21.234286	960.309383	14.984615
22.000466	957.316774	14.989632
21.685910	969.535323	14.994650
21.719850	952.803706	14.999667
21.656815	964.982950	15.004685
21.671758	952.280167	15.009703
21.550466	956.586016	15.014720
21.870753	959.711683	15.019738
21.427091	958.015391	15.024755
21.797628	964.537930	15.029773
21.630081	957.159585	15.034791
21.465268	960.649992	15.039808
21.397195	968.165755	15.044826
21.711036	965.087993	15.049843
21.834250	959.699389	15.054861
21.718320	963.388067	15.059879
21.645483	952.568627	15.064896
21.617626	965.906244	15.069914
21.400342	963.297753	15.074931
21.736714	963.611998	15.079949
21.810498	983.131917	15.084967
22.298744	988.579266	15.089984
22.040515	979.174656	15.095002
21.954562	959.482071	15.100019
21.636820	961.356221	15.105037
21.830264	976.682472	15.110055
22.100701	985.868952	15.115072
21.593205	993.851933	15.120090
22.262989	990.308160	15.125107
21.956248	980.143937	15.130125
22.045071	999.714332	15.135143
22.467932	989.085622	15.140160
22.271284	997.210397	15.145178
22.151118	986.234621	15.150195
22.464903	993.784317	15.155213
22.278897	992.972679	15.160231
22.398611	1002.470228	15.165248
22.130686	998.493857	15.170266
22.418575	986.508749	15.175283
22.622123	999.304929	15.180301
22.444673	1005.810982	15.185319
22.338019	990.013067	15.190336
22.110935	991.072531	15.195354
22.239077	988.280606	15.200371
22.539964	983.272279	15.205389
22.344838	992.604284	15.210407
22.299791	991.741997	15.215424
22.430820	992.081221	15.220442
22.238312	993.775270	15.225459
22.457007	982.662809	15.230477
22.081266	982.658519	15.235495
22.496740	979.547624	15.240512
22.191680	997.340443	15.245530
22.735258	1012.380381	15.250547
22.510697	1023.031521	15.255565
22.646329	1017.675581	15.260583
22.783755	1021.577462	15.265600
23.073148	1024.563695	15.270618
22.748429	1011.931655	15.275635
22.750833	1006.250280	15.280653
22.669345	1015.725588	15.285671
22.824211	1024.984819	15.290688
22.730102	1015.571565	15.295706
22.635226	1018.660168	15.300723
22.990116	1025.736663	15.305741
22.859381	1016.560115	15.310759
22.972195	997.705783	15.315776
22.808969	1025.620982	15.320794
22.769776	1016.367609	15.325811
22.813410	1014.492873	15.330829
22.821863	1013.860859	15.335847
22.715213	1015.623478	15.340864
22.692752	1028.292503	15.345882
22.716630	1010.994215	15.350899
22.810227	1025.088890	15.355917
23.057822	1034.072137	15.360935
23.547732	1040.197808	15.365952
23.499583	1029.342155	15.370970
23.037152	1033.559453	15.375987
23.163121	1023.040200	15.381005
23.045127	1027.618096	15.386023
23.171660	1021.834037	15.391040
22.998191	1034.923597	15.396058
23.411968	1043.491488	15.401075
23.467413	1047.358411	15.406093
23.396251	1054.442742	15.411111
23.500813	1040.105973	15.416128
23.312089	1034.785227	15.421146
23.143013	1026.526996	15.426163
23.489247	1035.860687	15.431181
23.266425	1044.194291	15.436199
23.410937	1053.971565	15.441216
23.534702	1042.320845	15.446234
23.359030	1052.520036	15.451251
23.425296	1047.816439	15.456269
23.261598	1038.117006	15.461287
23.785061	1029.498818	15.466304
23.534084	1050.786353	15.471322
23.273433	1046.006891	15.476339
23.656492	1042.985178	15.481357
23.506349	1046.444743	15.486375
23.437689	1044.148311	15.491392
23.580914	1052.201895	15.496410
23.873542	1048.850621	15.501427
23.469267	1051.192222	15.506445
23.493234	1045.258214	15.511463
23.603857	1040.264877	15.516480
23.636362	1058.447447	15.521498
23.750174	1073.376028	15.526515
24.457904	1069.045443	15.531533
24.187825	1064.974551	15.536551
23.659654	1055.563826	15.541568
23.833847	1043.047101	15.546586
23.516605	1058.053001	15.551603
23.852953	1063.680265	15.556621
23.910963	1065.098923	15.561639
24.128796	1062.960805	15.566656
24.219287	1065.632065	15.571674
23.881201	1080.117933	15.576691
24.238382	1088.998379	15.581709
23.714633	1070.011707	15.586727
23.862801	1066.104419	15.591744
23.835365	1072.576262	15.596762
23.694274	1066.472029	15.601779
24.097835	1066.085769	15.606797
23.960631	1072.938068	15.611815
24.201062	1067.863639	15.616832
24.486971	1077.569345	15.621850
24.134078	1088.776257	15.626867
24.210116	1074.378240	15.631885
24.140991	1086.999822	15.636903
24.218817	1100.237040	15.641920
24.544836	1099.636875	15.646938
24.363216	1095.210786	15.651955
24.619982	1091.578489	15.656973
24.538127	1105.279987	15.661991
24.692556	1099.074261	15.667008
24.508575	1096.149097	15.672026
24.283823	1106.767066	15.677043
24.811967	1094.734102	15.682061
24.681869	1097.847140	15.687079
25.086922	1083.704218	15.692096
24.470009	1081.620202	15.697114
24.286699	1078.796777	15.702131
24.713175	1072.120122	15.707149
24.442640	1100.360303	15.712167
24.951926	1093.744346	15.717184
25.007904	1099.360095	15.722202
24.822535	1109.556203	15.727219
25.215905	1095.388436	15.732237
24.828845	1094.639636	15.737255
24.650703	1068.811915	15.742272
24.742050	1063.160692	15.747290
24.807691	1091.346680	15.752307
24.919126	1097.261163	15.757325
25.017812	1102.527908	15.762343
25.177496	1101.457512	15.767360
24.866995	1085.643983	15.772378
24.533068	1101.012244	15.777395
24.888345	1102.717923	15.782413
24.860944	1094.283621	15.787431
24.918121	1093.131074	15.792448
24.894555	1093.258600	15.797466
24.612268	1093.949527	15.802483
24.747164	1082.202667	15.807501
24.719688	1101.671082	15.812519
25.204887	1108.234071	15.817536
25.227494	1112.667526	15.822554
24.952845	1123.343642	15.827571
25.382628	1124.594988	15.832589
25.262637	1125.808673	15.837607
25.515912	1133.057191	15.842624
25.574247	1131.268869	15.847642
25.545649	1127.043416	15.852659
25.535696	1124.113203	15.857677
25.433754	1098.618035	15.862695
25.127401	1094.566019	15.867712
25.334091	1094.460462	15.872730
25.176758	1114.082013	15.877747
25.487273	1119.727540	15.882765
25.472816	1118.670963	15.887783
25.709017	1113.940347	15.892800
25.396427	1118.538718	15.897818
25.043650	1123.817787	15.902835
25.326618	1117.698365	15.907853
24.805031	1126.734482	15.912871
25.174181	1112.850065	15.917888
25.597147	1135.292193	15.922906
25.669289	1148.678586	15.927923
25.914324	1153.720324	15.932941
25.789873	1158.015829	15.937959
25.708022	1152.387388	15.942976
25.919282	1144.560911	15.947994
25.891615	1158.727409	15.953011
25.944441	1142.607775	15.958029
26.073172	1148.190460	15.963047
25.895165	1154.736619	15.968064
26.069921	1147.439773	15.973082
25.887040	1162.489206	15.978099
25.903973	1148.208736	15.983117
25.887838	1150.812415	15.988135
26.209172	1149.011823	15.993152
26.023386	1143.866891	15.998170
26.002679	1154.834845	16.003187
26.294664	1141.445524	16.008205
26.114193	1139.906655	16.013223
25.943600	1145.280202	16.018240
26.414239	1136.060293	16.023258
25.868911	1155.188171	16.028275
26.257418	1133.539830	16.033293
26.058558	1149.483022	16.038311
26.078892	1150.651674	16.043328
26.470842	1142.792387	16.048346
25.872286	1136.364504	16.053363
26.272723	1143.752843	16.058381
26.329453	1144.556213	16.063399
25.992353	1138.856500	16.068416
26.412468	1145.018348	16.073434
26.304780	1161.128334	16.078451
26.574723	1172.032231	16.083469
26.549544	1174.923859	16.088487
26.747859	1164.193386	16.093504
26.925256	1156.889309	16.098522
26.300123	1160.062516	16.103539
26.782022	1154.225586	16.108557
26.760091	1156.667171	16.113575
26.724962	1153.392079	16.118592
26.636610	1137.968951	16.123610
26.872136	1164.288449	16.128627
26.821457	1154.230285	16.133645
26.827663	1147.737392	16.138663
26.512543	1141.632859	16.143680
26.248939	1148.507457	16.148698
26.949415	1168.920376	16.153715
27.265196	1165.474031	16.158733
26.894771	1168.898782	16.163751
27.076029	1168.041892	16.168768
27.249314	1163.135382	16.173786
26.978727	1162.063365	16.178803
27.004640	1168.514625	16.183821
27.027126	1161.471032	16.188839
26.849365	1171.157379	16.193856
26.981498	1170.467626	16.198874
26.655357	1170.839597	16.203891
26.890826	1163.068152	16.208909
27.147463	1156.442750	16.213927
26.920672	1161.839170	16.218944
26.789611	1174.393714	16.223962
26.885243	1175.986144	16.228979
26.858283	1163.847463	16.233997
27.151339	1180.618441	16.239015
27.278756	1187.714102	16.244032
27.538739	1200.295759	16.249050
27.051773	1204.458510	16.254067
27.297309	1194.051339	16.259085
27.332451	1202.968439	16.264103
27.548920	1204.182028	16.269120
27.532736	1198.076289	16.274138
27.065891	1206.887609	16.279155
27.579882	1192.196687	16.284173
27.554124	1206.666191	16.289191
27.451865	1205.444335	16.294208
27.544977	1190.892143	16.299226
27.396569	1196.190207	16.304243
27.526353	1199.060266	16.309261
27.762979	1192.252569	16.314279
27.519224	1193.325035	16.319296
27.500514	1187.692543	16.324314
27.541415	1185.488884	16.329331
27.798816	1192.082272	16.334349
27.711716	1184.183159	16.339367
27.481667	1208.729602	16.344384
27.988193	1200.718901	16.349402
28.054943	1224.990785	16.354419
28.152633	1210.370017	16.359437
27.997691	1207.040025	16.364455
28.033574	1200.462500	16.369472
27.812386	1186.188281	16.374490
27.898988	1200.665289	16.379507
28.131704	1225.494751	16.384525
28.172619	1224.708087	16.389543
28.086727	1217.533495	16.394560
28.410755	1221.877318	16.399578
28.257403	1226.359663	16.404595
27.950174	1218.357078	16.409613
28.629634	1224.625182	16.414631
28.121659	1216.853955	16.419648
28.481662	1194.481072	16.424666
28.444917	1196.370612	16.429683
28.149920	1197.621882	16.434701
28.154117	1199.285218	16.439719
28.302564	1212.529067	16.444736
28.623663	1208.056378	16.449754
28.598601	1213.804038	16.454771
28.737322	1206.649209	16.459789
28.460918	1196.499116	16.464807
28.296922	1207.844840	16.469824
28.657731	1211.082537	16.474842
28.482125	1214.944584	16.479859
28.422356	1218.499956	16.484877
28.771913	1214.030927	16.489895
28.815294	1212.541652	16.494912
28.804785	1218.917868	16.499930
28.565344	1213.612526	16.504947
28.588766	1214.894721	16.509965
29.127671	1209.416869	16.514983
28.489773	1206.524873	16.520000
28.329837	1204.055059	16.525018
28.873593	1227.959112	16.530035
28.327064	1209.127867	16.535053
28.957381	1212.718181	16.540071
28.545841	1225.409254	16.545088
28.758175	1227.140242	16.550106
28.661746	1211.655298	16.555123
28.499456	1219.777663	16.560141
28.691095	1221.881081	16.565159
28.706811	1236.595868	16.570176
29.150045	1230.578431	16.575194
29.057033	1230.995915	16.580211
29.193226	1240.768287	16.585229
29.044096	1238.213826	16.590247
29.248076	1236.791887	16.595264
28.870297	1236.979228	16.600282
28.959413	1230.558210	16.605299
29.150840	1237.774783	16.610317
29.179766	1232.793802	16.615335
28.641811	1230.357718	16.620352
29.055592	1252.356361	16.625370
29.558819	1254.941540	16.630387
29.749165	1255.491194	16.635405
29.817428	1268.529002	16.640423
29.685663	1271.285835	16.645440
29.743562	1244.445996	16.650458
29.313449	1237.363309	16.655475
29.513459	1232.055009	16.660493
29.911667	1242.994343	16.665511
29.730239	1247.051804	16.670528
29.512591	1229.806761	16.675546
29.652987	1229.376998	16.680563
29.387952	1241.127840	16.685581
29.798663	1251.489456	16.690599
29.620043	1243.467474	16.695616
30.085315	1249.100662	16.700634
29.971020	1254.135687	16.705651
29.866439	1258.507446	16.710669
29.897488	1259.892495	16.715687
29.740787	1268.009632	16.720704
29.898088	1261.133731	16.725722
29.890368	1258.653023	16.730739
29.770549	1261.516320	16.735757
30.177712	1241.000907	16.740775
29.636105	1273.160723	16.745792
29.926324	1265.330485	16.750810
30.057964	1250.538457	16.755827
29.687582	1254.048140	16.760845
29.996522	1259.537421	16.765863
29.782226	1256.537627	16.770880
29.973111	1258.987554	16.775898
30.030024	1282.673097	16.780915
30.148270	1278.753479	16.785933
30.464391	1272.404847	16.790951
30.389510	1279.848577	16.795968
30.370895	1279.182746	16.800986
30.693866	1278.426519	16.806003
30.354879	1282.440455	16.811021
30.446416	1288.005033	16.816039
30.482870	1283.915605	16.821056
30.564432	1277.122178	16.826074
30.762193	1289.438070	16.831091
30.665514	1286.787059	16.836109
30.786464	1277.652996	16.841127
30.331256	1278.082708	16.846144
30.450555	1275.921186	16.851162
30.768871	1283.177036	16.856179
30.363673	1280.982628	16.861197
30.660972	1273.606528	16.866215
30.132673	1284.481526	16.871232
29.855549	1288.195246	16.876250
30.353415	1296.031827	16.881267
30.637576	1309.679616	16.886285
30.974331	1299.060887	16.891303
30.857736	1323.870101	16.896320
30.827660	1311.181940	16.901338
30.745170	1303.801868	16.906355
30.817402	1297.251653	16.911373
30.885671	1312.356067	16.916391
31.005836	1302.493933	16.921408
30.656570	1307.387923	16.926426
31.191995	1321.406512	16.931443
31.133191	1327.489738	16.936461
31.083226	1325.929874	16.941479
31.458378	1329.165718	16.946496
31.739687	1328.450716	16.951514
31.500617	1321.140399	16.956531
31.265540	1302.667815	16.961549
31.226172	1303.418683	16.966567
31.138107	1297.778817	16.971584
31.503812	1303.189063	16.976602
31.710298	1323.529820	16.981619
31.271801	1324.030377	16.986637
31.482799	1313.736093	16.991655
31.738282	1330.909715	16.996672
31.531077	1320.037630	17.001690
31.764516	1315.032076	17.006707
31.564269	1319.331688	17.011725
31.744652	1315.496161	17.016743
31.822276	1324.731831	17.021760
31.666773	1310.429323	17.026778
31.762413	1307.381844	17.031795
31.639057	1318.956020	17.036813
31.961567	1325.291517	17.041831
32.119047	1326.292571	17.046848
31.797448	1310.504456	17.051866
32.016779	1305.952121	17.056883
31.795181	1307.144233	17.061901
32.021569	1308.828823	17.066919
31.821413	1320.815801	17.071936
31.846437	1318.873548	17.076954
32.039845	1313.670422	17.081971
32.208172	1324.907982	17.086989
32.444519	1311.184770	17.092007
32.329695	1317.976898	17.097024
32.263982	1325.584355	17.102042
32.293581	1320.702818	17.107059
32.337317	1316.600960	17.112077
32.157282	1307.363993	17.117095
32.340059	1315.714362	17.122112
32.376586	1319.659956	17.127130
32.572618	1311.759943	17.132147
32.289467	1311.504575	17.137165
32.348282	1314.102096	17.142183
32.459459	1328.401087	17.147200
32.274746	1324.655511	17.152218
32.313958	1314.471879	17.157235
32.476546	1334.883868	17.162253
32.391085	1333.601266	17.167271
32.446028	1320.664846	17.172288
32.148938	1317.252733	17.177306
32.651434	1316.008376	17.182323
32.259249	1319.164768	17.187341
32.511661	1331.251141	17.192359
32.660308	1335.892522	17.197376
32.640744	1362.696841	17.202394
33.128893	1350.451339	17.207411
32.910049	1349.225219	17.212429
32.811538	1348.549758	17.217447
32.797502	1350.049330	17.222464
32.916517	1348.159932	17.227482
33.382657	1347.381125	17.232499
33.269892	1347.859344	17.237517
33.042223	1340.837916	17.242535
33.005585	1329.148244	17.247552
32.986933	1331.411794	17.252570
32.891468	1345.446098	17.257587
32.802624	1346.573469	17.262605
32.925248	1340.495807	17.267623
32.800737	1345.832780	17.272640
32.900401	1351.063926	17.277658
33.035614	1344.756279	17.282675
32.720729	1362.235956	17.287693
33.361971	1372.774571	17.292711
33.425618	1377.156252	17.297728
33.393000	1383.651519	17.302746
33.405874	1377.917893	17.307763
33.408168	1392.046493	17.312781
33.591744	1382.258358	17.317799
33.593823	1375.790849	17.322816
33.532002	1388.520995	17.327834
33.943556	1371.108445	17.332851
33.458960	1384.429599	17.337869
33.576249	1380.045155	17.342887
33.629197	1367.735759	17.347904
33.588113	1384.503234	17.352922
33.684705	1363.723005	17.357939
33.745836	1373.833878	17.362957
33.808362	1374.644175	17.367975
33.788753	1365.421008	17.372992
33.921038	1367.863810	17.378010
34.052559	1365.074605	17.383027
33.901381	1378.714197	17.388045
34.054935	1371.610373	17.393063
34.123078	1369.659414	17.398080
33.995373	1367.377315	17.403098
34.174667	1365.834766	17.408115
33.883589	1365.287858	17.413133
33.653365	1388.170903	17.418151
34.275753	1398.532573	17.423168
34.015152	1415.374538	17.428186
34.200084	1408.164351	17.433203
34.296676	1401.919646	17.438221
34.317090	1400.892023	17.443239
34.485745	1408.921125	17.448256
34.719675	1396.788546	17.453274
34.792554	1402.835182	17.458291
34.814083	1400.599465	17.463309
34.547408	1396.454708	17.468327
34.689535	1399.160005	17.473344
34.174489	1393.610540	17.478362
34.902444	1388.888321	17.483379
34.645021	1399.155866	17.488397
34.796685	1385.973339	17.493415
34.849093	1401.473684	17.498432
34.758331	1410.297955	17.503450
34.924185	1397.655772	17.508467
34.682040	1402.025309	17.513485
34.977381	1402.097875	17.518503
34.890930	1402.154809	17.523520
34.770843	1407.655604	17.528538
35.154127	1395.387936	17.533555
34.940500	1393.919663	17.538573
34.937598	1393.242374	17.543591
35.315545	1389.381070	17.548608
34.996289	1395.427261	17.553626
35.038379	1400.529287	17.558643
34.841691	1395.597836	17.563661
34.957412	1397.423335	17.568679
34.753008	1388.530038	17.573696
34.393684	1403.221939	17.578714
34.639592	1398.016309	17.583731
35.195221	1419.453679	17.588749
35.073244	1423.985117	17.593767
35.333588	1410.644285	17.598784
35.106793	1424.496076	17.603802
35.535207	1417.319847	17.608819
35.431935	1420.500351	17.613837
35.367874	1408.034509	17.618855
35.366411	1417.635099	17.623872
35.331542	1425.462755	17.628890
35.536953	1432.107251	17.633907
35.864136	1446.705922	17.638925
35.875127	1443.505904	17.643943
36.079554	1429.279801	17.648960
35.565997	1435.683342	17.653978
35.689761	1421.330940	17.658995
35.991112	1442.168865	17.664013
35.976176	1438.161986	17.669031
36.244456	1408.327192	17.674048
35.600928	1415.842324	17.679066
35.863197	1413.640429	17.684083
36.144881	1434.887905	17.689101
35.933667	1449.247862	17.694119
36.519369	1429.440038	17.699136
36.198682	1433.340186	17.704154
36.049268	1418.429121	17.709171
35.891986	1415.280829	17.714189
35.988208	1440.583396	17.719207
36.332691	1439.513239	17.724224
36.339011	1440.674979	17.729242
36.595868	1444.278748	17.734259
36.320719	1437.957495	17.739277
36.127295	1437.180811	17.744295
36.560938	1435.662450	17.749312
36.290515	1440.866416	17.754330
36.586610	1431.018523	17.759347
36.609706	1439.343980	17.764365
36.396012	1444.523222	17.769383
36.523949	1438.224612	17.774400
36.424363	1444.444221	17.779418
36.283733	1436.827682	17.784435
36.407299	1445.136736	17.789453
36.283338	1440.694918	17.794471
36.711075	1453.074886	17.799488
36.828234	1459.912680	17.804506
36.774533	1467.046471	17.809523
36.740757	1454.211195	17.814541
36.825398	1460.007045	17.819559
36.980139	1461.969677	17.824576
36.961024	1471.961915	17.829594
36.862542	1465.010598	17.834611
37.147148	1468.418096	17.839629
36.953550	1464.069946	17.844647
37.006549	1462.706787	17.849664
37.108465	1464.688776	17.854682
36.933024	1458.385381	17.859699
37.111021	1460.410396	17.864717
37.094955	1471.372496	17.869735
37.553599	1474.462319	17.874752
37.658026	1474.397671	17.879770
37.963878	1473.247398	17.884787
37.421633	1456.664961	17.889805
37.380158	1461.245496	17.894823
37.787171	1454.719106	17.899840
37.663514	1465.148016	17.904858
38.041211	1454.325998	17.909875
37.832142	1452.975249	17.914893
37.658716	1455.437488	17.919911
37.693663	1448.363757	17.924928
37.687211	1441.724536	17.929946
37.760948	1445.354334	17.934963
37.916186	1446.885477	17.939981
37.910896	1448.388238	17.944999
37.778457	1451.518068	17.950016
37.579306	1442.966022	17.955034
37.894202	1451.751328	17.960051
38.046485	1457.280147	17.965069
37.705641	1463.445656	17.970087
37.651180	1464.224513	17.975104
37.757323	1461.239428	17.980122
37.892211	1486.256606	17.985139
38.021863	1479.916267	17.990157
38.032947	1497.658110	17.995175
38.213677	1489.313679	18.000192
38.085144	1481.574179	18.005210
38.127123	1481.573579	18.010227
38.181061	1485.336454	18.015245
38.295640	1484.584149	18.020263
38.039541	1465.046857	18.025280
38.095833	1484.408332	18.030298
38.195340	1500.742256	18.035315
38.586207	1505.267399	18.040333
38.236961	1518.251604	18.045351
38.662659	1518.078857	18.050368
38.788449	1510.881544	18.055386
38.560929	1503.624338	18.060403
38.794193	1489.474105	18.065421
38.632688	1499.587706	18.070439
38.969782	1494.227633	18.075456
39.000036	1494.105473	18.080474
39.028185	1493.977460	18.085491
38.820454	1493.631296	18.090509
38.678672	1495.264074	18.095527
39.040576	1498.632630	18.100544
39.018663	1494.816121	18.105562
38.957821	1490.086652	18.110579
39.134027	1489.716797	18.115597
39.112364	1500.375281	18.120615
39.112620	1485.650102	18.125632
39.101167	1494.733601	18.130650
38.868215	1501.775598	18.135667
39.218036	1485.278935	18.140685
39.315833	1504.684354	18.145703
39.553123	1516.380148	18.150720
39.599319	1524.366470	18.155738
39.395651	1515.306967	18.160755
39.577205	1514.820997	18.165773
39.479899	1525.410617	18.170791
39.995618	1506.401007	18.175808
39.427374	1507.957046	18.180826
39.531732	1508.797142	18.185843
39.883535	1507.987331	18.190861
39.714133	1539.008762	18.195879
39.587330	1521.618680	18.200896
39.667892	1526.089322	18.205914
39.476816	1515.361449	18.210931
39.736011	1512.396525	18.215949
39.705199	1523.020225	18.220967
39.849788	1523.757532	18.225984
39.564628	1525.568798	18.231002
39.028682	1521.476278	18.236019
40.000399	1527.264315	18.241037
39.878526	1541.695305	18.246055
39.799061	1547.134133	18.251072
40.058732	1547.122456	18.256090
40.181743	1555.637329	18.261107
40.212277	1540.395879	18.266125
40.049707	1549.406372	18.271143
40.151710	1543.592417	18.276160
40.390341	1550.063990	18.281178
40.061354	1551.834479	18.286195
40.305428	1544.468029	18.291213
40.237962	1558.080663	18.296231
40.712890	1564.621538	18.301248
40.843514	1561.922191	18.306266
40.633281	1553.863842	18.311283
40.428504	1541.851863	18.316301
40.553954	1559.289996	18.321319
40.771719	1563.357050	18.326336
40.957761	1573.322636	18.331354
41.054351	1567.086425	18.336371
41.175265	1561.850027	18.341389
40.892366	1541.384972	18.346407
40.922601	1548.158840	18.351424
40.810106	1541.831231	18.356442
40.691088	1565.192420	18.361459
41.003585	1569.793808	18.366477
41.095675	1586.667719	18.371495
41.129702	1582.426478	18.376512
41.189225	1581.241328	18.381530
41.038068	1570.243094	18.386547
41.161958	1570.718326	18.391565
41.234129	1570.494868	18.396583
41.148473	1572.057270	18.401600
41.239783	1580.530554	18.406618
41.249574	1570.842263	18.411635
41.475647	1561.365135	18.416653
41.320669	1562.223881	18.421671
41.294076	1571.087434	18.426688
41.726975	1574.549667	18.431706
41.270584	1582.317066	18.436723
41.547942	1566.052227	18.441741
41.877726	1591.421544	18.446759
41.731832	1588.580032	18.451776
41.822631	1590.639351	18.456794
41.768928	1581.162587	18.461811
41.914652	1584.974480	18.466829
41.795560	1574.106645	18.471847
42.140787	1579.912617	18.476864
42.063431	1586.947146	18.481882
42.032309	1580.151049	18.486899
42.232790	1580.540707	18.491917
42.170249	1583.176434	18.496935
42.351793	1582.710734	18.501952
42.360556	1586.720127	18.506970
42.327452	1592.031649	18.511987
42.343856	1561.143716	18.517005
42.481500	1567.935860	18.522023
42.196207	1565.149664	18.527040
42.876854	1556.448625	18.532058
42.510010	1568.133881	18.537075
42.314034	1559.553889	18.542093
42.375232	1553.755234	18.547111
42.374171	1559.073849	18.552128
42.251930	1559.204302	18.557146
42.362350	1574.182742	18.562163
42.841298	1573.522749	18.567181
42.426722	1588.209000	18.572199
42.631150	1576.229452	18.577216
42.816487	1574.808792	18.582234
42.375525	1592.895863	18.587251
42.577928	1575.360982	18.592269
42.632136	1590.056267	18.597287
42.629276	1590.113755	18.602304
42.691184	1610.391501	18.607322
42.631194	1603.891739	18.612339
42.525004	1603.341822	18.617357
42.619697	1615.314550	18.622375
42.887631	1609.497063	18.627392
43.315043	1615.209858	18.632410
42.891569	1615.104321	18.637427
43.464471	1617.601294	18.642445
43.472986	1626.138669	18.647463
43.470387	1633.786724	18.652480
43.642966	1632.051400	18.657498
43.391139	1633.181615	18.662515
43.696571	1630.128435	18.667533
43.423519	1615.820267	18.672551
43.819725	1623.294563	18.677568
43.773903	1615.131862	18.682586
43.469379	1600.272033	18.687603
43.580104	1616.066441	18.692621
43.664530	1624.429394	18.697639
43.787858	1634.545316	18.702656
43.611238	1637.843968	18.707674
43.810219	1638.752277	18.712691
43.939192	1634.724419	18.717709
43.940377	1630.890086	18.722727
44.098349	1618.862877	18.727744
44.273265	1624.927870	18.732762
43.819234	1625.755247	18.737779
44.069732	1622.719412	18.742797
44.023517	1627.291923	18.747815
44.087763	1623.265613	18.752832
44.194000	1621.902007	18.757850
43.743775	1626.228252	18.762867
44.427906	1626.792761	18.767885
44.404828	1644.067384	18.772903
44.386377	1656.246206	18.777920
44.350446	1654.660371	18.782938
44.429728	1662.193454	18.787955
44.779863	1660.091746	18.792973
44.875054	1661.888787	18.797991
44.745062	1654.914545	18.803008
44.991954	1661.656006	18.808026
44.872627	1660.883794	18.813043
45.031072	1651.496019	18.818061
44.911376	1638.025900	18.823079
44.525658	1657.854850	18.828096
44.841087	1651.317434	18.833114
45.004254	1653.941363	18.838131
44.947043	1647.701898	18.843149
45.215549	1662.586008	18.848167
44.723079	1667.664472	18.853184
45.118641	1654.236727	18.858202
45.095553	1657.789484	18.863219
44.739875	1658.936765	18.868237
45.170774	1656.976995	18.873255
44.981102	1654.173800	18.878272
45.178310	1658.570197	18.883290
45.240674	1673.846678	18.888307
45.227076	1686.021474	18.893325
45.645115	1682.303542	18.898343
45.011545	1680.586981	18.903360
45.477381	1682.874144	18.908378
45.317703	1690.530866	18.913395
45.297266	1696.294868	18.918413
45.555142	1687.035691	18.923431
45.698841	1696.157536	18.928448
45.846522	1710.745776	18.933466
46.073831	1706.271812	18.938483
45.801172	1691.682067	18.943501
45.998231	1707.645338	18.948519
45.555438	1711.085807	18.953536
45.931006	1704.154549	18.958554
46.117993	1708.385851	18.963571
45.881497	1702.094707	18.968589
46.127709	1705.077486	18.973607
46.031128	1707.056882	18.978624
46.128425	1700.551950	18.983642
46.089979	1698.784180	18.988659
46.360649	1704.322851	18.993677
46.667564	1685.133000	18.998695
46.122905	1686.860616	19.003712
46.474185	1692.613181	19.008730
46.313253	1694.820982	19.013747
46.506458	1695.220013	19.018765
46.665948	1696.709247	19.023783
46.670843	1708.018575	19.028800
46.730534	1693.962474	19.033818
46.525486	1699.600519	19.038835
46.808126	1719.907570	19.043853
47.121541	1730.642707	19.048871
46.980729	1727.121917	19.053888
46.995727	1717.850898	19.058906
46.931124	1729.998240	19.063923
46.734266	1721.788604	19.068941
47.156856	1725.875289	19.073959
46.970882	1738.551749	19.078976
47.149786	1726.119697	19.083994
47.267680	1722.589417	19.089011
47.005695	1722.651643	19.094029
47.223138	1724.024434	19.099047
47.057134	1718.100597	19.104064
47.232828	1722.192851	19.109082
47.229304	1706.804629	19.114099
47.478778	1714.751555	19.119117
47.781325	1718.635678	19.124135
47.236000	1722.325527	19.129152
47.697973	1737.344735	19.134170
47.619771	1746.455356	19.139187
47.591655	1753.471786	19.144205
47.570772	1749.051616	19.149223
47.741729	1762.237902	19.154240
47.975884	1748.353473	19.159258
47.755981	1755.572922	19.164275
48.001182	1766.480448	19.169293
48.313481	1748.242891	19.174311
47.983869	1749.021275	19.179328
48.245831	1741.722923	19.184346
47.988829	1740.301047	19.189363
47.923855	1730.168700	19.194381
47.951373	1747.290815	19.199399
48.057259	1753.011428	19.204416
48.167506	1738.067770	19.209434
48.381653	1744.757014	19.214451
48.370283	1768.569826	19.219469
48.668171	1770.251314	19.224487
48.668556	1768.426145	19.229504
48.513237	1772.347170	19.234522
48.756144	1768.524719	19.239539
48.554736	1777.428891	19.244557
49.056857	1765.485123	19.249575
48.848674	1765.645229	19.254592
48.976961	1757.231381	19.259610
48.953487	1747.631727	19.264627
48.741613	1739.329109	19.269645
49.162380	1740.435276	19.274663
48.715975	1744.224903	19.279680
49.046394	1758.593166	19.284698
49.079738	1767.527818	19.289715
49.226091	1757.457756	19.294733
49.283774	1757.148321	19.299751
49.290999	1767.323273	19.304768
49.249754	1781.773934	19.309786
49.015885	1766.064238	19.314803
49.049641	1777.410278	19.319821
49.150574	1773.385148	19.324839
49.303760	1759.511826	19.329856
49.507278	1750.361869	19.334874
49.433407	1758.978766	19.339891
49.306373	1751.349688	19.344909
49.734987	1760.375877	19.349927
49.524967	1766.993026	19.354944
49.501093	1765.825482	19.359962
50.089000	1790.983906	19.364979
49.921971	1784.374910	19.369997
49.927011	1786.198671	19.375015
49.756330	1799.018689	19.380032
50.134503	1804.128686	19.385050
50.117852	1784.988833	19.390067
50.063826	1794.684746	19.395085
50.427695	1783.452952	19.400103
49.963145	1785.499462	19.405120
49.843651	1794.238857	19.410138
49.975889	1783.992798	19.415155
49.708207	1787.089937	19.420173
50.348386	1780.490045	19.425191
49.948317	1795.849460	19.430208
50.394837	1818.798448	19.435226
50.731010	1803.528273	19.440243
50.341211	1824.251841	19.445261
50.820380	1810.992196	19.450279
50.570384	1816.680715	19.455296
50.371875	1814.638651	19.460314
50.637728	1804.805554	19.465331
50.407119	1806.835058	19.470349
50.794270	1815.116601	19.475367
50.654545	1819.367578	19.480384
50.785152	1827.247804	19.485402
51.021065	1842.172606	19.490419
51.049731	1837.750225	19.495437
51.027782	1833.825095	19.500455
51.340622	1839.854392	19.505472
51.359897	1841.034983	19.510490
51.189735	1839.169989	19.515507
50.999243	1838.398210	19.520525
51.427114	1848.556943	19.525543
51.280524	1836.213917	19.530560
51.504861	1833.380162	19.535578
51.934893	1825.890937	19.540595
51.506045	1847.313181	19.545613
51.578161	1835.678267	19.550631
51.471649	1828.739920	19.555648
51.517113	1826.659015	19.560666
51.908995	1840.394578	19.565683
51.919246	1851.735109	19.570701
52.335233	1850.352969	19.575719
52.214524	1838.088425	19.580736
51.961443	1847.489176	19.585754
52.210636	1833.032115	19.590771
51.688241	1835.820140	19.595789
52.022174	1848.547268	19.600807
52.338317	1846.857966	19.605824
51.909112	1868.340032	19.610842
52.347460	1861.510613	19.615859
52.081133	1864.784381	19.620877
52.010175	1855.889227	19.625895
52.478879	1858.172991	19.630912
52.446493	1846.260510	19.635930
52.628362	1849.151705	19.640947
52.513343	1849.990481	19.645965
52.456193	1851.481382	19.650983
52.471943	1844.744732	19.656000
52.506811	1859.199127	19.661018
52.745823	1856.653243	19.666035
52.567711	1876.096952	19.671053
52.856643	1871.551253	19.676071
52.861401	1884.665028	19.681088
52.921174	1882.629380	19.686106
53.051129	1879.999465	19.691123
52.838697	1874.130770	19.696141
53.103134	1873.155885	19.701159
53.235728	1879.946148	19.706176
53.098515	1877.513012	19.711194
52.987227	1881.963011	19.716211
53.056682	1874.839885	19.721229
53.540289	1903.745853	19.726247
53.719092	1895.470208	19.731264
53.479044	1906.525823	19.736282
54.056727	1902.790807	19.741299
53.763340	1901.535923	19.746317
53.971453	1896.771724	19.751335
53.967472	1883.193012	19.756352
53.587855	1880.810954	19.761370
53.851454	1878.073243	19.766387
53.766874	1896.045096	19.771405
53.950279	1884.152723	19.776423
54.179615	1896.270715	19.781440
54.031682	1899.377315	19.786458
54.214006	1889.761178	19.791475
54.062402	1887.087452	19.796493
54.083079	1891.415664	19.801511
54.117865	1899.764829	19.806528
54.307799	1885.327056	19.811546
54.432164	1898.036601	19.816563
54.078839	1891.917216	19.821581
54.266927	1902.000373	19.826599
54.483624	1896.371036	19.831616
54.334737	1914.818905	19.836634
54.685340	1919.387237	19.841651
54.613468	1920.020300	19.846669
54.632939	1924.419083	19.851687
54.812991	1922.879306	19.856704
54.702009	1921.911347	19.861722
54.661410	1908.706609	19.866739
54.763933	1928.473037	19.871757
54.670535	1914.759986	19.876775
54.876386	1918.695960	19.881792
54.928500	1939.446934	19.886810
55.152978	1936.406284	19.891827
55.063087	1928.080454	19.896845
55.446859	1928.239574	19.901863
55.600632	1929.458565	19.906880
55.533018	1930.029420	19.911898
55.534588	1921.297310	19.916915
55.849885	1930.006363	19.921933
55.963769	1918.983565	19.926951
55.767436	1935.519174	19.931968
55.837048	1924.646772	19.936986
55.827949	1918.502575	19.942003
55.605834	1932.251706	19.947021
55.382040	1926.022729	19.952039
55.585190	1925.428275	19.957056
55.688309	1925.284427	19.962074
55.807690	1920.789070	19.967091
55.682280	1923.790889	19.972109
55.566770	1915.626357	19.977127
55.857719	1951.641220	19.982144
55.890439	1959.286849	19.987162
56.215090	1956.218915	19.992179
56.252590	1966.845411	19.997197
56.249015	1965.431332	20.002215
56.342080	1955.603271	20.007232
56.402184	1957.378886	20.012250
56.786390	1955.766500	20.017267
56.338732	1950.562617	20.022285
56.060843	1960.004439	20.027303
56.498068	1970.704721	20.032320
56.910486	1971.871823	20.037338
57.225826	1971.893165	20.042355
56.885491	1982.182179	20.047373
57.096878	1989.395023	20.052391
56.993017	1984.504921	20.057408
56.650615	1980.355788	20.062426
56.809087	1978.610259	20.067443
56.882017	1991.622326	20.072461
56.944890	1975.786620	20.077479
57.050298	1972.016362	20.082496
56.935085	1989.278454	20.087514
57.466857	1991.228941	20.092531
57.201315	2006.558463	20.097549
57.376362	2012.766182	20.102567
57.464734	2006.375863	20.107584
57.451572	2022.999190	20.112602
57.606478	2009.726041	20.117619
57.734741	2009.985249	20.122637
57.846389	2013.693549	20.127655
58.124848	1998.354288	20.132672
57.948311	2004.060849	20.137690
57.945227	1998.547503	20.142707
58.075396	2004.065217	20.147725
58.163551	1996.567061	20.152743
58.340373	2002.002866	20.157760
58.091099	2010.732339	20.162778
58.154630	2008.755097	20.167795
57.955344	2005.961496	20.172813
58.055001	2019.531275	20.177831
57.908918	2035.644096	20.182848
58.350952	2020.536398	20.187866
58.385952	2043.259191	20.192883
58.527234	2032.897909	20.197901
58.725412	2026.102791	20.202919
58.795996	2031.330413	20.207936
58.494089	2022.047515	20.212954
58.730974	2027.210260	20.217971
58.582226	2036.657162	20.222989
59.064722	2040.914416	20.228007
59.729833	2047.069017	20.233024
59.521222	2033.960230	20.238042
59.100911	2019.097575	20.243059
58.870995	2028.207650	20.248077
58.822219	2031.064369	20.253095
59.477757	2047.727984	20.258112
59.203444	2053.182361	20.263130
59.228302	2052.134279	20.268147
59.326949	2048.228628	20.273165
59.415536	2037.680119	20.278183
59.540130	2034.554202	20.283200
59.321425	2039.775900	20.288218
59.865652	2035.804888	20.293235
60.004563	2036.226285	20.298253
59.749209	2039.789269	20.303271
60.477006	2038.665770	20.308288
60.090427	2039.142217	20.313306
59.984439	2038.110641	20.318323
59.910565	2034.106949	20.323341
59.864245	2034.359383	20.328359
59.766453	2037.522084	20.333376
59.921006	2045.232746	20.338394
60.004778	2050.766214	20.343411
59.930250	2063.727623	20.348429
59.724065	2079.849535	20.353447
60.083260	2069.499061	20.358464
60.229213	2063.724195	20.363482
60.582011	2070.576957	20.368499
60.759029	2065.495459	20.373517
60.836358	2075.680386	20.378535
60.916899	2066.301196	20.383552
60.461642	2064.287453	20.388570
60.715633	2094.173885	20.393587
60.932465	2089.470972	20.398605
60.981203	2107.352647	20.403623
61.145013	2085.704277	20.408640
60.971510	2102.623629	20.413658
61.153244	2091.357152	20.418675
61.129309	2089.480166	20.423693
61.096847	2101.003501	20.428711
61.693606	2096.518661	20.433728
61.403548	2102.820495	20.438746
61.461688	2091.920249	20.443763
61.774238	2099.535649	20.448781
61.687686	2090.459601	20.453799
61.504216	2091.970415	20.458816
61.554610	2081.144870	20.463834
61.661558	2091.020634	20.468851
61.486137	2094.553200	20.473869
61.540577	2118.171361	20.478887
61.897096	2114.119654	20.483904
61.722452	2116.952215	20.488922
61.963499	2125.241143	20.493939
62.187270	2122.965012	20.498957
61.900621	2119.627357	20.503975
61.941261	2124.539737	20.508992
62.083198	2128.047424	20.514010
62.385354	2155.886201	20.519027
62.450975	2147.549020	20.524045
62.345600	2156.289436	20.529063
62.665471	2150.897737	20.534080
62.609796	2151.106353	20.539098
62.334600	2148.625120	20.544115
62.716965	2154.774331	20.549133
62.436621	2152.424833	20.554151
62.733689	2143.564646	20.559168
62.870847	2155.431780	20.564186
63.012201	2165.733922	20.569203
63.063523	2171.076174	20.574221
62.721136	2165.925971	20.579239
63.313950	2172.380121	20.584256
63.304589	2167.590369	20.589274
63.557528	2167.609230	20.594291
63.631330	2164.129928	20.599309
63.370870	2162.481357	20.604327
63.873477	2172.709046	20.609344
63.542772	2165.353338	20.614362
63.583055	2175.120112	20.619379
63.628677	2158.747984	20.624397
63.604313	2164.069872	20.629415
63.823226	2174.270832	20.634432
63.575649	2156.456260	20.639450
63.930259	2161.052246	20.644467
63.887436	2164.151765	20.649485
63.568914	2157.825570	20.654503
63.918301	2177.684280	20.659520
64.213662	2184.033283	20.664538
63.832770	2193.292202	20.669555
63.941318	2192.279978	20.674573
63.778608	2193.800558	20.679591
64.288702	2190.450697	20.684608
64.136924	2192.659909	20.689626
64.609145	2197.492926	20.694643
64.911196	2207.287911	20.699661
64.700681	2211.749775	20.704679
65.106320	2206.765273	20.709696
65.061137	2195.069758	20.714714
64.748907	2191.026587	20.719731
64.706758	2196.618704	20.724749
64.918872	2215.365883	20.729767
65.081961	2198.808186	20.734784
65.148468	2195.680026	20.739802
65.295665	2205.278784	20.744819
65.425931	2197.718954	20.749837
65.331558	2207.359009	20.754855
65.398820	2195.258755	20.759872
65.512028	2205.558096	20.764890
65.497653	2204.691163	20.769907
65.551256	2198.909856	20.774925
65.426071	2209.707573	20.779943
65.431329	2196.665552	20.784960
65.956809	2201.800153	20.789978
65.695011	2190.831269	20.794995
65.678748	2203.528387	20.800013
65.292598	2235.124748	20.805031
65.681931	2241.749342	20.810048
65.793360	2240.686646	20.815066
65.888456	2242.484657	20.820083
65.948803	2240.225084	20.825101
66.083231	2253.835381	20.830119
66.233458	2267.789677	20.835136
66.256399	2262.301164	20.840154
66.321883	2270.148390	20.845171
66.885706	2257.287794	20.850189
66.354278	2264.749283	20.855207
66.812566	2251.885267	20.860224
66.945709	2261.692649	20.865242
66.706526	2261.665293	20.870259
66.955617	2252.983417	20.875277
66.581589	2265.730848	20.880295
66.819749	2265.785808	20.885312
67.321611	2288.020464	20.890330
67.569710	2276.849759	20.895347
67.584425	2276.796587	20.900365
67.405628	2276.008977	20.905383
67.452873	2259.733898	20.910400
67.561163	2263.108812	20.915418
67.278790	2262.863432	20.920435
67.513771	2274.923517	20.925453
67.605714	2285.494689	20.930471
67.611951	2278.638279	20.935488
67.700890	2278.265803	20.940506
67.906433	2280.615163	20.945523
68.175240	2272.097315	20.950541
67.977723	2282.738558	20.955559
67.876009	2278.258671	20.960576
68.234024	2288.253482	20.965594
68.013714	2262.822680	20.970611
68.025141	2282.126839	20.975629
68.082771	2273.440571	20.980647
68.157105	2277.306259	20.985664
68.320970	2277.468757	20.990682
67.971679	2295.863992	20.995699
68.344609	2295.560121	21.000717
68.395170	2305.572092	21.005735
68.082815	2302.827332	21.010752
68.355220	2289.816863	21.015770
68.188191	2304.745325	21.020787
68.548681	2306.837034	21.025805
68.690808	2326.677636	21.030823
69.238914	2319.430925	21.035840
69.271853	2319.402099	21.040858
69.275091	2325.554983	21.045875
69.654993	2311.975832	21.050893
68.994982	2311.367330	21.055911
68.890684	2315.913232	21.060928
69.508281	2316.161161	21.065946
69.145455	2325.346910	21.070963
69.275958	2321.425395	21.075981
69.705084	2338.061004	21.080999
69.809027	2335.244691	21.086016
69.867349	2344.520085	21.091034
69.609236	2340.898180	21.096051
70.347093	2334.183012	21.101069
69.837538	2334.046224	21.106087
69.974528	2343.461350	21.111104
70.141192	2330.918448	21.116122
69.930892	2323.704946	21.121139
70.236466	2334.085560	21.126157
70.076265	2340.422716	21.131175
70.203857	2324.459046	21.136192
70.308177	2332.095194	21.141210
70.337123	2350.097728	21.146227
70.542036	2354.365021	21.151245
70.691730	2367.376924	21.156263
70.547188	2358.454176	21.161280
70.858612	2362.210639	21.166298
70.827193	2358.411527	21.171315
70.790220	2366.703424	21.176333
70.893669	2370.865656	21.181351
70.671533	2370.720146	21.186368
71.089115	2362.678572	21.191386
71.163201	2396.634080	21.196403
71.109390	2376.601930	21.201421
70.910007	2386.392304	21.206439
70.892342	2381.243084	21.211456
71.384183	2391.364645	21.216474
71.480241	2389.633517	21.221491
71.600565	2397.782527	21.226509
71.670152	2416.830234	21.231527
71.892977	2413.930886	21.236544
72.130443	2401.467748	21.241562
72.215633	2410.772793	21.246579
72.190454	2399.596376	21.251597
72.558565	2413.318571	21.256615
72.315252	2412.666006	21.261632
72.798266	2404.856672	21.266650
72.247665	2395.331809	21.271667
72.509665	2381.640014	21.276685
72.579672	2379.923427	21.281703
72.207086	2391.106589	21.286720
72.710937	2397.413159	21.291738
72.390411	2404.640879	21.296755
72.640315	2397.137548	21.301773
72.432769	2398.046162	21.306791
72.473932	2398.336008	21.311808
72.661804	2399.992938	21.316826
72.485159	2424.692120	21.321843
72.642714	2428.350619	21.326861
72.705468	2422.446474	21.331879
73.008243	2438.515166	21.336896
73.263614	2436.787427	21.341914
72.946205	2438.650674	21.346931
73.508359	2423.719457	21.351949
73.420513	2422.663894	21.356967
73.436632	2448.280530	21.361984
73.617234	2448.173571	21.367002
73.573851	2456.590180	21.372019
73.527791	2451.330686	21.377037
73.808596	2451.326049	21.382055
74.095597	2436.980956	21.387072
74.090342	2439.228974	21.392090
74.114989	2453.681287	21.397107
74.052624	2462.902888	21.402125
74.039186	2451.029122	21.407143
74.014048	2447.778083	21.412160
74.246954	2458.683509	21.417178
74.530583	2469.257577	21.422195
74.451820	2487.987614	21.427213
74.439895	2486.443783	21.432231
74.267451	2488.959164	21.437248
74.834230	2475.013212	21.442266
74.678987	2470.956621	21.447283
75.078532	2476.997824	21.452301
75.002074	2472.266892	21.457319
74.868097	2466.340326	21.462336
75.151893	2464.362647	21.467354
75.031603	2481.951084	21.472371
75.147431	2489.728695	21.477389
75.481979	2493.126696	21.482407
75.646396	2506.203204	21.487424
75.697086	2506.118499	21.492442
75.430719	2506.043870	21.497459
75.564369	2506.786675	21.502477
76.219538	2502.063755	21.507495
75.895615	2504.683490	21.512512
75.838677	2498.971314	21.517530
75.641515	2510.181274	21.522547
75.899609	2499.699997	21.527565
75.896301	2485.418970	21.532583
75.963369	2501.097014	21.537600
76.013097	2494.003826	21.542618
76.054770	2516.847263	21.547635
76.016644	2524.007509	21.552653
76.483855	2523.062751	21.557671
76.344876	2522.318147	21.562688
76.521779	2528.779572	21.567706
76.472605	2521.846198	21.572723
76.527470	2512.721535	21.577741
76.934792	2539.575659	21.582759
76.877911	2553.745516	21.587776
77.112366	2552.406207	21.592794
77.351492	2554.533359	21.597811
77.411510	2552.617053	21.602829
77.311818	2542.988261	21.607847
77.472222	2549.845476	21.612864
77.667198	2533.398079	21.617882
77.556093	2546.173938	21.622899
77.547595	2538.316838	21.627917
77.723592	2534.650707	21.632935
77.356089	2536.198273	21.637952
77.679845	2520.808394	21.642970
77.673116	2541.744193	21.647987
77.711389	2524.210652	21.653005
77.758580	2539.652684	21.658023
77.577559	2534.070629	21.663040
77.820832	2550.843071	21.668058
77.920678	2572.294493	21.673075
77.633562	2570.102522	21.678093
78.163152	2566.511598	21.683111
77.966795	2577.135926	21.688128
78.431317	2581.073612	21.693146
78.556759	2592.179741	21.698163
78.581199	2602.953402	21.703181
78.557128	2599.680897	21.708199
78.723590	2599.120431	21.713216
78.643737	2595.855373	21.718234
78.736588	2600.587845	21.723251
78.902604	2592.554065	21.728269
79.168144	2601.153728	21.733287
79.282873	2611.558390	21.738304
79.389896	2614.947959	21.743322
79.632737	2626.787170	21.748339
79.281935	2617.082716	21.753357
79.477482	2614.950136	21.758375
79.529212	2617.765260	21.763392
79.882595	2618.040718	21.768410
79.801076	2615.541772	21.773427
79.906283	2615.292174	21.778445
80.146777	2608.962972	21.783463
79.967641	2621.609013	21.788480
80.127928	2608.039519	21.793498
80.171392	2611.237058	21.798515
80.131318	2612.242796	21.803533
80.273061	2614.309090	21.808551
80.175911	2624.309265	21.813568
80.434544	2629.158230	21.818586
80.526724	2637.625165	21.823603
80.565958	2662.727973	21.828621
80.638459	2651.326796	21.833639
80.351610	2645.527180	21.838656
80.447432	2647.357792	21.843674
80.586782	2640.749070	21.848691
80.663519	2658.554133	21.853709
80.564993	2647.315651	21.858727
80.714981	2661.812399	21.863744
81.135349	2651.663212	21.868762
81.200922	2660.663423	21.873779
81.109683	2682.955326	21.878797
81.637000	2678.510927	21.883815
82.063770	2677.834619	21.888832
81.885190	2676.057318	21.893850
81.730365	2679.664162	21.898867
81.651372	2688.513892	21.903885
81.820475	2674.689372	21.908903
81.837111	2687.862492	21.913920
82.303135	2674.202070	21.918938
82.079714	2680.773602	21.923955
82.180706	2677.167660	21.928973
82.515135	2673.419812	21.933991
82.241333	2683.474804	21.939008
82.180173	2693.102589	21.944026
82.385782	2707.520907	21.949043
82.642086	2706.638348	21.954061
82.734215	2701.763558	21.959079
82.717236	2708.034093	21.964096
82.849278	2701.797174	21.969114
82.722593	2697.434858	21.974131
82.679658	2717.312450	21.979149
82.941942	2716.315137	21.984167
83.093335	2724.853034	21.989184
83.218112	2723.392678	21.994202
83.541642	2732.167455	21.999219
83.542305	2719.376506	22.004237
83.640954	2728.748408	22.009255
83.621972	2724.473983	22.014272
83.360092	2732.759743	22.019290
83.225155	2726.999946	22.024307
83.583205	2744.499601	22.029325
83.936595	2742.221842	22.034343
84.155848	2757.699629	22.039360
84.093952	2759.016227	22.044378
84.480186	2757.619737	22.049395
84.159409	2758.803742	22.054413
84.556557	2761.163046	22.059431
84.623480	2752.622001	22.064448
84.604770	2761.995602	22.069466
84.978863	2749.121861	22.074483
84.575182	2748.745551	22.079501
84.710905	2748.595423	22.084519
84.737113	2753.017736	22.089536
84.471337	2743.878015	22.094554
84.654961	2758.061658	22.099571
84.857276	2784.505852	22.104589
84.942058	2776.065767	22.109607
85.129253	2779.247858	22.114624
85.070727	2781.049864	22.119642
85.225187	2786.540818	22.124659
85.171425	2795.342547	22.129677
85.537784	2797.383953	22.134695
85.625569	2811.075474	22.139712
85.628232	2803.402592	22.144730
85.672805	2801.089054	22.149747
85.641116	2807.599826	22.154765
86.107853	2817.479589	22.159783
86.277784	2828.768081	22.164800
86.367102	2826.077308	22.169818
86.463822	2821.918563	22.174835
86.699670	2824.399204	22.179853
86.773994	2826.854574	22.184871
86.846736	2826.113745	22.189888
86.844194	2829.842097	22.194906
86.899519	2816.190367	22.199923
86.945101	2820.175692	22.204941
87.129067	2828.094559	22.209959
87.384792	2815.157656	22.214976
87.589059	2814.524212	22.219994
87.477038	2810.944187	22.225011
87.432257	2818.120038	22.230029
87.641389	2812.353938	22.235047
87.419874	2818.102873	22.240064
87.534321	2816.323192	22.245082
87.756306	2804.822407	22.250099
87.600129	2825.328224	22.255117
87.578038	2817.616320	22.260135
87.589289	2808.434523	22.265152
87.502816	2826.216164	22.270170
87.657869	2822.025736	22.275187
87.852470	2842.430113	22.280205
87.946205	2836.882458	22.285223
87.703730	2841.797368	22.290240
87.595280	2867.796266	22.295258
87.986526	2857.381119	22.300275
87.718058	2878.832026	22.305293
88.304700	2874.320493	22.310311
88.612994	2900.923141	22.315328
88.727884	2894.638000	22.320346
89.087411	2898.255364	22.325363
89.062134	2908.790830	22.330381
89.471297	2895.039818	22.335399
89.182521	2894.694708	22.340416
89.221808	2891.762614	22.345434
89.630777	2886.932248	22.350451
89.599257	2885.838610	22.355469
89.788239	2881.847849	22.360487
89.682518	2876.867523	22.365504
89.701557	2878.093011	22.370522
89.849153	2875.139087	22.375539
89.802926	2888.978200	22.380557
89.876329	2883.244737	22.385575
89.953429	2880.855742	22.390592
89.812436	2882.027959	22.395610
90.062907	2899.425700	22.400627
90.262147	2905.615120	22.405645
90.057182	2902.261235	22.410663
90.212362	2910.662208	22.415680
90.192541	2917.723758	22.420698
90.332964	2918.608558	22.425715
90.416436	2928.295062	22.430733
90.588816	2941.950282	22.435751
90.872154	2949.813033	22.440768
90.864272	2945.495969	22.445786
90.767078	2939.737531	22.450803
90.883370	2958.970690	22.455821
91.335056	2982.250355	22.460839
91.512464	2972.791623	22.465856
91.463739	2979.550925	22.470874
91.612344	2961.329044	22.475891
91.465397	2966.886993	22.480909
91.566021	2951.863835	22.485927
91.818444	2951.129328	22.490944
91.923380	2979.742066	22.495962
92.242548	2982.209753	22.500979
92.281079	2992.885306	22.505997
92.524003	2992.646801	22.511015
92.434977	2981.540348	22.516032
92.555165	2986.245196	22.521050
92.878798	2979.234070	22.526067
92.675840	2972.354050	22.531085
92.871150	2975.557083	22.536103
93.059366	2976.405843	22.541120
92.951652	2978.277213	22.546138
93.074352	2979.176953	22.551155
93.083620	2967.886963	22.556173
93.103072	2960.659603	22.561191
93.256613	2974.263641	22.566208
92.886581	2974.320691	22.571226
93.354059	2965.053769	22.576243
93.171400	2977.585342	22.581261
93.347493	2992.169614	22.586279
93.627120	3004.065236	22.591296
93.544265	3007.254010	22.596314
93.568051	2994.258640	22.601331
93.708812	3015.725374	22.606349
93.746303	3018.870841	22.611367
93.900697	3021.279354	22.616384
93.778778	3025.179628	22.621402
93.881797	3021.708296	22.626419
93.742986	3037.622853	22.631437
94.413366	3038.398242	22.636455
94.466209	3056.629715	22.641472
94.265481	3044.131393	22.646490
94.714815	3049.738659	22.651507
94.982760	3061.601810	22.656525
95.129958	3066.926760	22.661543
95.608718	3067.735980	22.666560
95.289891	3068.809854	22.671578
95.932970	3061.907895	22.676595
95.566234	3045.938359	22.681613
95.369472	3042.447865	22.686631
95.642839	3025.486258	22.691648
95.779993	3065.841967	22.696666
95.974955	3072.292568	22.701683
95.854739	3052.520877	22.706701
96.143485	3058.754028	22.711719
96.454418	3056.775729	22.716736
95.972249	3056.726715	22.721754
96.206739	3063.841181	22.726771
96.212870	3056.664987	22.731789
96.318281	3067.147474	22.736807
96.544800	3045.118338	22.741824
96.184258	3055.070790	22.746842
96.081599	3062.221283	22.751859
96.130076	3063.582851	22.756877
96.484552	3090.854109	22.761895
96.838849	3085.643781	22.766912
96.736225	3089.865455	22.771930
96.976177	3096.694418	22.776947
96.902012	3101.415474	22.781965
96.575132	3122.515188	22.786983
96.785012	3121.543044	22.792000
97.118495	3142.599014	22.797018
97.612658	3138.133196	22.802035
97.801564	3152.644644	22.807053
97.605024	3147.695772	22.812071
97.897014	3146.301241	22.817088
97.801990	3143.161395	22.822106
98.317624	3153.300002	22.827123
98.570368	3167.273803	22.832141
98.245835	3163.404237	22.837159
98.648713	3160.645651	22.842176
98.476729	3180.322351	22.847194
98.768223	3171.692593	22.852211
98.525107	3182.189446	22.857229
98.670804	3171.898513	22.862247
98.853248	3168.880316	22.867264
98.687186	3175.749832	22.872282
98.816975	3185.246381	22.877299
99.171896	3195.715676	22.882317
99.215014	3195.451135	22.887335
99.252338	3193.099567	22.892352
99.252794	3200.754884	22.897370
99.405013	3185.055913	22.902387
99.397227	3210.310677	22.907405
99.612722	3221.446863	22.912423
99.880975	3212.563271	22.917440
99.571374	3213.386834	22.922458
99.914575	3224.199981	22.927475
100.020268	3221.635950	22.932493
99.888891	3248.169738	22.937511
100.425735	3249.989352	22.942528
100.214025	3242.935871	22.947546
100.534355	3248.779862	22.952563
100.721808	3251.117206	22.957581
100.478127	3251.281712	22.962599
101.084815	3267.912020	22.967616
100.790022	3279.050884	22.972634
100.747953	3275.721568	22.977651
101.323500	3267.476867	22.982669
101.239480	3277.698700	22.987687
101.799882	3260.608311	22.992704
102.004842	3258.471529	22.997722
102.108403	3257.701967	23.002739
102.016543	3252.958774	23.007757
101.846932	3265.360876	23.012775
102.332925	3258.755236	23.017792
101.693504	3275.808172	23.022810
101.949740	3253.021931	23.027827
102.173032	3240.207541	23.032845
101.913856	3278.544455	23.037863
102.140777	3282.760542	23.042880
102.122005	3282.638891	23.047898
102.435454	3300.671699	23.052915
102.742666	3275.427619	23.057933
102.474943	3295.716490	23.062951
103.178658	3305.954620	23.067968
102.630013	3318.560132	23.072986
102.701903	3323.754517	23.078003
103.070512	3317.811498	23.083021
102.855321	3324.814186	23.088039
103.063996	3314.655062	23.093056
103.299460	3331.333199	23.098074
103.607269	3340.019395	23.103091
103.847108	3354.065571	23.108109
103.634960	3346.709188	23.113127
103.995164	3342.318790	23.118144
104.235114	3335.107177	23.123162
104.069121	3338.827427	23.128179
103.871948	3348.726893	23.133197
104.183422	3346.589820	23.138215
104.146479	3374.159112	23.143232
104.322329	3362.447248	23.148250
104.515586	3359.032970	23.153267
105.017911	3353.099729	23.158285
104.979056	3367.587800	23.163303
104.943613	3357.252273	23.168320
105.147163	3377.231311	23.173338
105.208563	3376.271877	23.178355
105.729898	3375.571650	23.183373
105.731609	3384.040954	23.188391
105.904072	3364.999371	23.193408
106.000183	3385.588052	23.198426
105.785340	3385.666108	23.203443
106.082448	3376.698723	23.208461
105.976103	3379.520621	23.213479
105.921183	3389.588126	23.218496
106.023311	3379.009004	23.223514
106.157299	3380.396231	23.228531
106.180207	3372.087491	23.233549
106.060278	3366.248996	23.238567
106.446165	3395.973659	23.243584
106.531807	3392.318911	23.248602
106.404444	3388.636374	23.253619
106.666457	3388.585441	23.258637
106.416799	3398.750479	23.263655
106.747256	3405.246344	23.268672
106.848089	3426.669859	23.273690
106.610111	3420.256608	23.278707
106.923237	3434.796611	23.283725
107.349305	3457.332669	23.288743
107.982246	3457.392281	23.293760
107.967978	3456.836061	23.298778
107.611129	3463.394147	23.303795
107.852359	3439.229515	23.308813
107.931038	3454.114747	23.313831
107.693653	3473.964425	23.318848
107.757411	3478.062656	23.323866
108.081777	3485.801392	23.328883
108.371979	3487.143920	23.333901
108.319882	3491.975809	23.338919
108.742300	3496.877311	23.343936
108.879121	3512.668865	23.348954
108.739264	3515.291419	23.353971
109.083658	3504.194068	23.358989
108.830122	3505.209941	23.364007
108.939619	3508.873884	23.369024
109.148862	3504.416463	23.374042
108.972241	3517.202573	23.379059
109.587867	3528.166967	23.384077
109.447385	3542.121445	23.389095
109.617951	3529.795020	23.394112
109.728746	3542.038813	23.399130
109.661331	3543.874264	23.404147
109.906849	3547.091756	23.409165
110.119323	3556.275091	23.414183
110.389927	3561.111549	23.419200
110.440423	3566.930175	23.424218
110.251781	3563.254178	23.429235
110.689777	3559.900197	23.434253
110.533973	3558.239885	23.439271
110.395548	3557.092412	23.444288
110.737026	3562.721036	23.449306
110.671936	3587.396952	23.454323
110.886945	3588.267893	23.459341
111.016943	3583.402118	23.464359
111.330582	3598.295708	23.469376
111.518321	3605.971851	23.474394
111.811963	3608.342685	23.479411
111.967069	3611.294836	23.484429
112.010736	3620.109477	23.489447
112.030805	3609.712052	23.494464
112.021356	3613.839344	23.499482
112.127469	3618.158944	23.504499
112.324539	3603.708545	23.509517
112.256039	3595.521671	23.514535
111.988754	3613.687614	23.519552
112.344634	3620.349830	23.524570
112.503307	3629.402936	23.529587
112.640020	3621.076044	23.534605
112.556435	3640.537162	23.539623
112.958981	3644.085986	23.544640
113.081781	3667.386784	23.549658
113.131627	3676.905901	23.554675
113.664573	3662.964673	23.559693
113.210185	3671.721690	23.564711
113.728548	3657.344914	23.569728
113.517256	3667.688815	23.574746
113.624622	3694.560468	23.579763
113.859070	3700.817025	23.584781
113.770936	3693.935622	23.589799
113.856315	3706.342593	23.594816
114.047324	3713.542099	23.599834
114.356767	3719.144580	23.604851
114.620357	3728.705964	23.609869
114.785910	3724.302154	23.614887
114.593767	3721.129422	23.619904
114.511781	3720.591468	23.624922
115.004752	3738.940379	23.629939
115.165783	3731.481206	23.634957
114.916509	3750.634231	23.639975
115.081368	3753.036013	23.644992
115.399996	3739.129933	23.650010
115.271392	3741.632563	23.655027
115.583142	3769.468347	23.660045
115.518667	3782.184572	23.665063
115.744561	3780.153704	23.670080
116.235943	3779.505259	23.675098
116.438464	3766.550174	23.680115
116.484385	3766.518611	23.685133
116.138898	3775.329144	23.690151
116.472881	3780.985069	23.695168
116.901904	3793.009166	23.700186
116.434751	3805.754549	23.705203
116.683557	3790.262417	23.710221
116.689835	3802.199297	23.715239
116.772690	3813.001944	23.720256
117.324743	3777.477422	23.725274
117.263624	3803.643882	23.730291
117.139041	3806.124205	23.735309
117.768570	3808.053962	23.740327
117.681860	3817.067020	23.745344
117.780632	3824.685733	23.750362
117.602294	3814.174507	23.755379
117.899659	3806.446328	23.760397
118.056931	3817.149679	23.765415
117.853293	3814.450847	23.770432
118.307544	3829.482441	23.775450
118.083541	3838.941796	23.780467
118.350027	3836.295585	23.785485
118.299687	3855.877654	23.790503
118.423051	3843.333594	23.795520
118.637255	3860.300840	23.800538
118.761571	3872.361175	23.805555
118.999845	3861.966894	23.810573
119.035241	3879.161727	23.815591
118.803496	3872.866541	23.820608
119.138910	3895.539079	23.825626
119.381770	3902.164781	23.830643
119.451509	3897.048052	23.835661
120.161717	3906.983363	23.840679
120.004090	3921.654365	23.845696
120.392468	3917.774676	23.850714
120.163650	3923.819304	23.855731
120.503224	3917.341907	23.860749
120.649860	3919.396349	23.865767
120.549547	3914.182917	23.870784
120.886271	3919.055804	23.875802
120.629384	3912.019519	23.880819
120.633633	3918.081537	23.885837
120.832047	3937.084049	23.890855
121.053935	3930.269024	23.895872
121.543370	3943.937897	23.900890
121.162122	3946.831895	23.905907
121.370310	3942.077294	23.910925
121.505049	3953.371048	23.915943
121.424506	3969.657231	23.920960
121.922531	3965.678314	23.925978
121.788290	3976.714183	23.930995
122.052334	3978.095327	23.936013
122.103561	3986.806177	23.941031
122.143463	4008.841523	23.946048
122.402508	4000.859355	23.951066
122.198521	4014.660193	23.956083
122.396557	4016.340818	23.961101
122.747216	4016.406138	23.966119
122.713132	4040.279262	23.971136
123.127707	4032.510739	23.976154
123.173415	4027.691625	23.981171
122.880754	4039.376916	23.986189
123.561175	4051.800600	23.991207
123.647091	4053.015918	23.996224
123.880651	4051.690805	24.001242
123.627176	4049.864696	24.006259
123.740315	4049.944068	24.011277
124.036009	4054.031292	24.016295
124.055421	4076.111849	24.021312
124.405003	4077.493829	24.026330
124.368260	4084.462255	24.031347
124.435815	4073.229541	24.036365
124.413584	4097.361021	24.041383
124.547617	4099.181359	24.046400
124.807786	4104.042940	24.051418
124.723197	4108.718586	24.056435
125.170173	4112.109200	24.061453
125.068224	4102.978803	24.066471
124.981307	4129.717770	24.071488
125.536975	4131.902679	24.076506
125.484530	4134.057366	24.081523
125.773480	4126.155230	24.086541
125.959766	4130.144809	24.091559
125.746739	4118.644657	24.096576
126.144823	4152.972131	24.101594
126.121032	4153.898902	24.106611
126.455810	4156.783282	24.111629
126.674411	4160.711232	24.116647
126.590268	4159.596474	24.121664
127.117281	4167.012710	24.126682
126.966303	4155.619596	24.131699
127.041049	4173.442483	24.136717
127.262946	4174.935725	24.141735
127.454729	4176.670155	24.146752
127.256311	4177.869869	24.151770
127.299689	4186.330955	24.156787
127.678243	4174.987726	24.161805
127.968040	4192.495583	24.166823
127.796858	4195.734430	24.171840
127.977007	4202.152914	24.176858
128.193809	4214.722233	24.181875
128.411681	4198.505302	24.186893
128.380153	4201.245893	24.191911
128.363833	4202.199778	24.196928
128.918453	4203.590409	24.201946
128.977975	4225.624002	24.206963
128.491104	4214.023363	24.211981
128.821666	4214.833321	24.216999
128.867413	4225.297910	24.222016
129.153870	4249.788056	24.227034
129.315714	4259.334693	24.232051
129.617151	4260.169544	24.237069
129.716363	4251.792017	24.242087
129.972641	4281.098869	24.247104
130.456390	4277.215931	24.252122
130.413837	4283.396452	24.257139
130.110236	4296.138438	24.262157
130.450367	4278.780385	24.267175
130.563270	4274.748888	24.272192
130.780174	4284.930913	24.277210
130.793667	4273.153460	24.282227
130.732319	4286.397520	24.287245
131.186477	4302.742154	24.292263
131.021080	4302.004188	24.297280
131.157654	4306.853579	24.302298
131.103826	4317.813806	24.307315
130.972061	4333.716325	24.312333
131.726274	4333.623630	24.317351
131.434325	4347.565672	24.322368
131.370894	4342.711346	24.327386
131.642685	4355.070517	24.332403
131.960953	4358.376945	24.337421
132.148303	4359.806230	24.342439
132.032717	4374.686062	24.347456
132.148418	4393.424068	24.352474
132.497740	4396.343097	24.357491
132.690697	4412.609356	24.362509
133.097602	4429.442631	24.367527
133.387910	4426.854983	24.372544
133.426543	4419.495626	24.377562
133.868812	4414.391579	24.382579
133.822803	4402.316779	24.387597
134.564944	4407.109841	24.392615
134.240248	4395.710216	24.397632
134.493783	4401.057230	24.402650
134.376903	4395.683383	24.407667
134.404887	4405.736077	24.412685
134.495885	4398.621221	24.417703
134.489797	4398.134480	24.422720
134.309732	4408.908547	24.427738
134.758484	4403.253838	24.432755
134.589180	4395.327680	24.437773
134.680702	4396.366906	24.442791
134.582304	4425.635394	24.447808
135.050570	4432.605569	24.452826
134.914132	4430.334493	24.457843
135.221824	4437.049317	24.462861
135.170910	4447.267828	24.467879
135.528154	4457.210246	24.472896
135.575946	4462.983003	24.477914
135.809097	4466.616900	24.482931
135.949630	4483.054097	24.487949
136.222395	4476.209167	24.492967
135.636727	4491.053794	24.497984
135.731317	4511.099349	24.503002
136.238030	4519.589569	24.508019
136.438639	4540.570388	24.513037
136.686263	4548.327853	24.518055
136.847410	4550.311086	24.523072
137.316241	4557.874131	24.528090
137.710187	4562.716903	24.533107
137.754762	4568.409917	24.538125
138.123904	4554.260908	24.543143
137.969255	4557.204975	24.548160
138.534173	4562.378941	24.553178
138.754937	4552.025675	24.558195
138.677941	4562.287154	24.563213
139.050425	4548.992313	24.568231
138.630902	4543.975505	24.573248
138.862198	4544.514879	24.578266
138.843332	4551.241586	24.583283
138.814042	4545.475659	24.588301
139.038745	4552.646762	24.593319
139.203656	4569.707970	24.598336
139.118802	4585.962441	24.603354
139.435305	4579.818107	24.608371
139.324753	4590.580027	24.613389
139.596034	4596.059608	24.618407
139.863179	4620.433060	24.623424
139.587847	4619.884502	24.628442
140.342150	4626.905140	24.633459
139.948596	4630.961131	24.638477
140.411272	4637.794135	24.643495
140.518485	4649.744910	24.648512
140.266364	4650.623219	24.653530
140.659815	4656.705861	24.658547
140.431962	4667.481310	24.663565
140.987334	4674.184447	24.668583
140.974560	4675.676357	24.673600
141.431355	4703.889855	24.678618
141.802245	4683.269972	24.683635
141.708369	4710.474867	24.688653
142.089245	4682.716723	24.693671
141.837457	4697.629606	24.698688
142.051996	4708.702457	24.703706
142.344862	4703.699382	24.708723
142.142233	4701.823454	24.713741
142.903678	4712.103579	24.718759
142.713872	4707.258997	24.723776
142.636703	4719.698166	24.728794
143.120519	4739.740334	24.733811
143.027688	4738.830119	24.738829
143.488248	4733.380427	24.743847
143.445727	4733.594973	24.748864
143.371423	4737.058475	24.753882
143.539277	4742.155198	24.758899
143.505892	4754.897792	24.763917
143.940585	4758.755937	24.768935
143.766013	4770.941556	24.773952
143.808386	4782.210625	24.778970
144.308802	4781.740969	24.783987
144.297035	4806.318280	24.789005
144.456573	4797.007258	24.794023
144.615097	4806.173677	24.799040
144.540782	4816.045507	24.804058
144.804489	4813.516523	24.809075
144.813253	4816.416314	24.814093
145.065928	4821.972673	24.819111
145.188665	4845.247497	24.824128
145.583847	4850.483466	24.829146
145.793497	4843.079114	24.834163
145.529772	4874.792321	24.839181
146.052315	4856.787731	24.844199
146.377962	4869.571095	24.849216
146.567889	4865.522389	24.854234
146.820629	4865.390902	24.859251
146.626728	4878.091614	24.864269
146.803424	4887.057044	24.869287
147.022440	4899.025759	24.874304
147.196946	4894.529194	24.879322
147.493051	4889.267254	24.884339
147.682030	4905.035862	24.889357
147.714152	4911.062166	24.894375
147.915107	4923.229162	24.899392
148.052526	4931.453460	24.904410
148.111898	4929.275154	24.909427
148.165698	4921.314225	24.914445
148.229384	4926.983740	24.919463
148.153602	4929.486099	24.924480
148.675238	4934.123636	24.929498
149.064041	4945.040302	24.934515
148.902197	4937.615397	24.939533
149.020285	4945.404308	24.944551
149.019318	4949.941189	24.949568
149.052272	4971.168801	24.954586
149.588372	4960.288349	24.959603
149.512599	4978.439399	24.964621
149.655390	4988.595943	24.969639
149.900964	4992.616108	24.974656
149.981683	5000.448229	24.979674
150.368731	4993.251507	24.984691
150.563273	5016.259600	24.989709
150.885376	5024.836903	24.994727
150.806444	5027.155543	24.999744
150.809852	5019.950543	25.004762
151.216379	5020.003492	25.009779
151.115591	5026.669530	25.014797
151.332835	5026.628555	25.019815
151.573409	5044.301811	25.024832
151.807274	5036.819743	25.029850
152.231897	5038.226029	25.034867
152.151680	5036.896381	25.039885
152.097987	5033.099701	25.044903
152.396063	5036.371029	25.049920
152.383487	5042.994939	25.054938
152.537278	5061.421940	25.059955
152.661934	5064.697126	25.064973
152.587493	5074.436067	25.069991
152.804588	5076.062085	25.075008
152.455970	5080.555658	25.080026
152.922008	5092.096295	25.085043
153.154096	5113.040404	25.090061
152.968235	5099.804280	25.095079
153.046218	5134.478559	25.100096
153.046502	5131.687137	25.105114
153.477264	5145.374646	25.110131
153.598769	5159.658557	25.115149
153.960918	5169.741573	25.120167
154.153596	5179.917953	25.125184
154.022945	5204.016308	25.130202
154.412880	5190.382989	25.135219
154.639034	5220.161567	25.140237
154.903547	5210.522708	25.145255
155.053545	5221.754233	25.150272
155.186728	5246.794919	25.155290
155.856226	5250.394700	25.160307
155.711415	5253.112460	25.165325
155.900451	5260.337818	25.170343
156.487295	5253.319389	25.175360
156.336799	5256.978674	25.180378
156.270571	5259.863772	25.185395
156.371812	5279.441880	25.190413
156.639688	5282.611555	25.195431
157.143301	5270.642516	25.200448
156.538748	5292.894439	25.205466
157.110822	5297.869435	25.210483
157.325480	5297.762743	25.215501
157.304463	5309.343861	25.220519
157.627440	5298.236963	25.225536
157.692268	5308.574322	25.230554
157.691010	5325.221673	25.235571
157.968344	5337.399997	25.240589
157.785742	5342.711523	25.245607
158.225838	5356.659498	25.250624
158.125480	5362.027917	25.255642
158.206856	5381.336983	25.260659
158.374069	5386.309609	25.265677
158.678291	5400.265900	25.270695
158.822409	5416.575928	25.275712
158.897441	5423.600897	25.280730
159.345555	5419.810976	25.285747
159.560809	5434.469431	25.290765
160.041436	5448.390712	25.295783
160.076598	5456.527455	25.300800
160.288117	5456.387815	25.305818
160.554768	5437.767326	25.310835
160.602420	5452.234189	25.315853
160.407385	5463.592981	25.320871
160.834305	5468.425079	25.325888
160.887469	5481.733129	25.330906
160.995875	5463.606890	25.335923
161.069694	5491.651230	25.340941
160.942728	5496.734314	25.345959
161.717683	5500.579735	25.350976
161.549996	5510.939111	25.355994
161.716334	5519.319580	25.361011
161.685836	5530.402402	25.366029
161.773484	5518.953897	25.371047
162.166884	5539.575453	25.376064
162.465741	5546.166230	25.381082
162.578045	5554.262323	25.386099
162.881652	5575.394854	25.391117
163.024979	5579.962411	25.396135
163.132633	5583.277132	25.401152
163.533091	5586.176523	25.406170
163.478822	5590.918079	25.411187
163.328332	5600.152955	25.416205
163.705577	5617.605057	25.421223
164.067625	5614.450213	25.426240
164.007892	5629.866928	25.431258
164.007769	5616.184690	25.436275
164.380487	5643.854308	25.441293
164.532558	5642.368502	25.446311
164.703883	5643.358011	25.451328
164.426037	5642.720452	25.456346
164.616102	5666.143656	25.461363
164.930466	5677.857045	25.466381
164.970051	5671.782452	25.471399
165.466202	5690.336711	25.476416
165.152545	5691.848903	25.481434
165.650528	5714.982706	25.486451
166.277310	5718.310899	25.491469
166.250322	5729.668497	25.496487
166.239540	5722.385591	25.501504
166.290510	5751.168079	25.506522
166.602569	5751.034661	25.511539
166.842644	5761.826074	25.516557
166.667519	5777.054112	25.521575
166.997192	5779.962480	25.526592
167.367383	5798.845576	25.531610
167.622174	5781.269232	25.536627
167.630085	5805.601936	25.541645
167.818589	5825.163555	25.546663
168.130744	5822.491358	25.551680
168.003603	5825.913434	25.556698
168.219176	5845.699363	25.561715
168.725984	5852.119286	25.566733
168.645753	5852.717270	25.571751
168.942198	5856.906040	25.576768
169.042326	5885.056197	25.581786
169.084170	5890.745421	25.586803
169.128452	5876.755202	25.591821
169.202967	5904.871829	25.596839
169.581706	5906.494063	25.601856
169.708619	5910.205309	25.606874
169.876014	5938.096396	25.611891
170.309584	5949.353645	25.616909
170.401782	5958.670296	25.621927
170.494467	5948.068351	25.626944
170.611054	5967.905832	25.631962
171.187692	5962.521191	25.636979
171.045355	5973.460195	25.641997
171.084727	5990.086974	25.647015
171.294325	5995.596537	25.652032
171.698099	6001.494527	25.657050
171.654740	6014.955998	25.662067
171.922304	6014.639758	25.667085
172.140495	6033.025374	25.672103
172.353007	6024.212000	25.677120
172.597730	6040.761985	25.682138
172.485593	6053.574168	25.687156
172.471992	6044.806410	25.692173
173.000706	6066.967465	25.697191
173.311184	6060.296339	25.702208
173.604100	6078.157413	25.707226
173.399223	6086.823558	25.712244
173.887133	6085.294428	25.717261
173.701835	6103.936576	25.722279
174.004506	6103.821245	25.727296
174.329165	6116.108905	25.732314
174.220454	6109.342832	25.737332
174.581930	6116.358584	25.742349
174.699989	6136.048384	25.747367
174.755817	6130.780845	25.752384
174.734936	6141.995595	25.757402
174.917470	6161.182602	25.762420
175.305373	6162.048950	25.767437
175.327863	6163.495014	25.772455
175.656081	6179.505712	25.777472
175.316394	6206.041163	25.782490
175.421295	6213.220230	25.787508
175.893320	6219.304288	25.792525
175.973815	6238.045607	25.797543
176.136174	6247.361863	25.802560
176.496015	6257.021122	25.807578
176.673193	6264.187088	25.812596
176.996012	6272.875606	25.817613
177.312642	6286.946402	25.822631
177.636131	6287.268620	25.827648
177.698084	6280.235667	25.832666
177.991485	6313.679608	25.837684
178.570084	6302.165161	25.842701
178.545115	6313.017679	25.847719
178.767729	6294.184530	25.852736
178.906826	6321.647469	25.857754
178.946199	6313.019643	25.862772
179.000957	6308.416856	25.867789
179.087697	6326.650898	25.872807
179.430499	6328.727195	25.877824
179.524550	6333.646064	25.882842
179.740183	6331.466157	25.887860
180.078733	6353.094415	25.892877
179.861636	6353.409094	25.897895
180.252393	6360.677625	25.902912
180.595413	6373.137670	25.907930
180.173607	6382.772204	25.912948
180.516682	6388.275997	25.917965
180.373451	6397.679846	25.922983
181.196968	6403.214509	25.928000
181.027156	6419.321523	25.933018
181.072765	6420.270036	25.938036
181.234031	6449.633683	25.943053
181.295134	6452.521980	25.948071
181.713662	6466.953310	25.953088
182.311838	6473.272560	25.958106
182.124924	6482.521455	25.963124
182.269086	6488.567261	25.968141
182.484253	6513.473585	25.973159
182.668445	6517.375928	25.978176
182.774231	6528.335353	25.983194
183.105434	6545.439367	25.988212
183.450530	6551.246462	25.993229
183.811030	6565.526429	25.998247
184.261517	6580.621954	26.003264
183.956142	6572.888842	26.008282
184.346704	6573.274009	26.013300
184.554763	6588.333605	26.018317
184.595623	6587.687446	26.023335
184.948210	6601.171018	26.028352
184.906432	6598.965881	26.033370
184.984072	6617.883739	26.038388
185.649451	6615.755482	26.043405
185.458664	6618.558249	26.048423
185.533206	6639.772988	26.053440
185.668741	6651.380026	26.058458
185.853727	6654.883405	26.063476
186.056516	6666.421854	26.068493
185.896521	6681.075757	26.073511
186.432715	6692.128769	26.078528
186.763484	6703.508288	26.083546
186.324160	6721.758047	26.088564
187.160655	6721.901801	26.093581
187.206072	6733.054438	26.098599
187.321499	6750.671556	26.103616
187.497330	6749.025009	26.108634
187.548506	6756.408110	26.113652
187.904418	6764.065315	26.118669
188.055382	6791.624375	26.123687
188.373559	6786.758604	26.128704
188.311384	6801.228324	26.133722
188.532542	6822.506499	26.138740
188.555713	6821.486037	26.143757
188.703058	6836.624416	26.148775
188.844466	6837.259447	26.153792
189.104915	6858.475660	26.158810
189.153536	6870.689428	26.163828
189.738307	6877.696981	26.168845
190.073247	6878.290588	26.173863
190.405091	6887.093328	26.178880
190.662992	6888.833680	26.183898
190.661863	6913.920493	26.188916
191.015562	6909.114572	26.193933
191.392145	6906.565032	26.198951
191.204016	6917.159454	26.203968
191.671875	6926.585503	26.208986
191.710688	6937.355858	26.214004
191.886165	6942.646954	26.219021
192.141895	6949.119450	26.224039
192.193947	6973.241923	26.229056
192.434180	6969.463145	26.234074
192.412109	6979.440716	26.239092
192.841343	6993.838870	26.244109
193.018771	6985.466251	26.249127
193.199245	7006.209193	26.254144
193.801139	7017.987123	26.259162
193.289759	7031.881573	26.264180
193.720474	7028.214638	26.269197
193.912413	7045.814721	26.274215
194.229586	7058.153187	26.279232
194.950612	7065.288729	26.284250
194.537864	7067.860491	26.289268
194.897053	7063.220965	26.294285
195.247869	7084.697792	26.299303
195.197604	7091.351241	26.304320
195.480564	7091.424231	26.309338
195.522169	7094.128832	26.314356
195.517989	7109.450802	26.319373
195.758890	7122.731985	26.324391
195.605567	7125.985414	26.329408
196.498308	7132.102699	26.334426
196.425683	7150.412070	26.339444
196.465478	7171.045775	26.344461
196.477518	7184.015163	26.349479
196.802919	7186.451595	26.354496
196.991100	7221.742709	26.359514
197.440122	7219.606810	26.364532
197.629097	7230.675835	26.369549
197.713077	7246.712625	26.374567
197.838375	7253.863204	26.379584
198.425124	7248.646568	26.384602
198.361014	7268.441525	26.389620
198.383561	7271.566697	26.394637
198.847933	7287.425698	26.399655
198.978869	7301.222134	26.404672
199.437417	7292.175635	26.409690
199.688892	7310.387541	26.414708
200.292092	7312.869448	26.419725
200.529715	7314.342288	26.424743
200.552763	7327.579312	26.429760
200.701495	7323.046936	26.434778
200.632242	7319.138865	26.439796
201.028098	7314.759394	26.444813
201.084693	7307.383503	26.449831
200.954987	7312.416041	26.454848
201.368415	7317.224174	26.459866
201.264900	7326.379063	26.464884
201.441091	7327.725811	26.469901
201.561111	7345.436556	26.474919
201.641337	7369.242330	26.479936
202.145805	7374.244136	26.484954
201.788740	7393.780515	26.489972
202.157214	7397.158846	26.494989
202.296890	7423.618330	26.500007
202.749426	7435.524421	26.505024
203.181424	7439.701068	26.510042
203.253938	7469.598309	26.515060
203.318840	7465.304192	26.520077
203.507621	7481.792492	26.525095
203.714224	7496.698844	26.530112
204.079829	7497.555962	26.535130
204.135871	7530.508553	26.540148
204.444863	7526.333961	26.545165
204.732344	7545.480518	26.550183
204.903756	7551.197372	26.555200
204.997650	7568.206257	26.560218
205.265012	7591.299434	26.565236
205.199644	7589.974594	26.570253
205.190388	7611.070608	26.575271
205.527422	7631.080110	26.580288
205.834606	7650.753559	26.585306
206.055773	7683.566568	26.590324
206.414266	7687.213591	26.595341
206.777763	7692.232491	26.600359
207.003971	7712.932977	26.605376
207.694393	7709.924686	26.610394
207.702982	7715.333005	26.615412
208.083344	7733.813926	26.620429
208.287486	7735.509704	26.625447
208.071601	7744.804684	26.630464
208.541912	7742.274573	26.635482
208.664843	7751.744331	26.640500
208.854212	7761.594531	26.645517
209.031094	7771.980764	26.650535
209.153272	7790.586317	26.655552
209.569069	7799.189443	26.660570
209.534651	7812.044165	26.665588
209.791801	7808.091494	26.670605
209.957991	7823.807355	26.675623
210.012767	7821.588455	26.680640
210.670523	7840.433201	26.685658
210.763482	7853.907984	26.690676
210.800473	7854.336645	26.695693
211.307476	7866.891678	26.700711
211.348818	7882.471500	26.705728
211.549277	7884.476627	26.710746
211.514839	7910.950734	26.715764
211.767501	7921.637208	26.720781
212.136932	7933.352643	26.725799
212.218822	7955.606742	26.730816
212.417432	7944.266902	26.735834
212.441557	7974.102215	26.740852
212.735365	7978.568825	26.745869
213.440559	7988.548160	26.750887
213.235792	8009.285590	26.755904
213.417742	7998.728944	26.760922
213.624420	8033.366718	26.765940
213.828061	8043.666015	26.770957
214.104396	8036.236938	26.775975
214.042162	8065.653529	26.780992
214.599861	8068.724306	26.786010
214.542836	8086.091040	26.791028
214.668087	8089.654622	26.796045
215.321574	8092.131500	26.801063
215.368462	8108.743923	26.806080
215.467447	8122.845636	26.811098
215.767306	8129.982738	26.816116
215.576453	8152.820091	26.821133
215.924141	8164.874798	26.826151
216.029910	8189.483282	26.831168
216.587365	8196.131297	26.836186
216.497993	8211.983491	26.841204
216.975801	8226.270794	26.846221
217.093719	8243.505624	26.851239
217.390358	8261.122061	26.856256
217.855019	8266.072451	26.861274
218.164596	8289.350272	26.866292
218.064300	8282.262112	26.871309
218.738825	8299.731099	26.876327
218.731558	8313.656005	26.881344
219.238797	8295.510615	26.886362
219.512363	8307.480019	26.891380
219.120774	8336.741247	26.896397
219.808296	8338.361165	26.901415
219.589560	8336.604015	26.906432
219.960712	8348.935367	26.911450
220.117737	8370.717688	26.916468
220.248077	8400.793799	26.921485
220.406806	8395.690828	26.926503
220.649738	8427.218023	26.931520
220.918709	8432.082661	26.936538
220.980203	8442.875895	26.941556
220.986438	8473.118352	26.946573
221.750234	8487.257829	26.951591
221.866044	8508.971542	26.956608
222.151394	8505.332227	26.961626
222.294052	8531.777327	26.966644
222.031724	8540.740207	26.971661
222.402558	8565.074717	26.976679
222.742240	8575.369999	26.981696
222.901423	8606.359285	26.986714
223.766804	8626.809661	26.991732
223.726331	8629.647803	26.996749
224.298048	8645.904720	27.001767
224.377822	8660.021902	27.006784
224.844618	8654.412716	27.011802
224.969803	8665.123119	27.016820
225.405697	8686.189553	27.021837
225.849715	8684.076344	27.026855
225.784521	8688.552853	27.031872
225.688096	8686.143799	27.036890
226.113715	8702.314649	27.041908
226.357479	8712.286413	27.046925
226.365409	8706.704191	27.051943
226.261025	8736.980394	27.056960
226.786411	8737.263802	27.061978
227.010356	8752.801712	27.066996
227.187955	8776.841619	27.072013
227.494794	8764.800458	27.077031
227.865789	8789.548780	27.082048
227.957240	8805.005456	27.087066
227.929715	8807.250785	27.092084
228.182143	8834.961269	27.097101
228.450403	8836.764716	27.102119
228.509853	8857.054771	27.107136
228.640306	8859.629218	27.112154
228.971064	8872.752114	27.117172
229.239537	8898.060209	27.122189
229.648675	8902.438719	27.127207
229.650578	8916.221658	27.132224
229.679216	8936.827226	27.137242
229.806854	8948.783422	27.142260
229.830365	8960.528422	27.147277
230.403603	8977.390319	27.152295
230.611371	8993.780976	27.157312
231.184150	9024.616109	27.162330
231.548945	9036.704889	27.167348
231.458968	9045.788437	27.172365
232.199773	9051.661438	27.177383
232.204817	9074.596924	27.182400
232.348265	9080.831696	27.187418
232.718428	9088.308897	27.192436
232.825584	9087.330334	27.197453
233.195336	9107.904182	27.202471
233.622307	9107.985688	27.207488
233.914994	9108.130337	27.212506
234.132640	9125.390608	27.217524
234.253941	9131.924418	27.222541
234.537621	9140.601307	27.227559
234.724976	9156.746616	27.232576
234.464536	9160.422997	27.237594
234.910886	9165.844550	27.242612
234.948046	9203.122299	27.247629
235.207764	9198.536396	27.252647
235.158671	9220.826520	27.257664
235.617016	9251.251746	27.262682
236.193037	9254.653689	27.267700
235.888539	9284.785209	27.272717
236.462544	9292.201262	27.277735
237.034753	9301.064495	27.282752
237.291702	9336.817621	27.287770
237.707381	9321.720942	27.292788
238.024208	9329.595373	27.297805
238.218855	9343.014458	27.302823
238.519279	9340.883933	27.307840
238.534011	9339.226719	27.312858
239.138382	9352.778177	27.317876
238.884351	9377.116361	27.322893
239.124445	9356.217794	27.327911
239.575611	9388.903407	27.332928
239.824716	9388.254234	27.337946
240.254321	9398.121690	27.342964
240.109864	9397.795885	27.347981
240.597588	9416.830506	27.352999
240.777830	9430.011815	27.358016
241.163302	9429.354288	27.363034
241.241934	9446.654419	27.368052
241.154074	9464.675986	27.373069
241.249091	9464.987197	27.378087
241.547787	9486.430231	27.383104
242.122131	9492.884614	27.388122
242.620612	9514.979138	27.393140
242.486338	9540.318571	27.398157
242.670366	9547.607779	27.403175
242.857501	9569.858576	27.408192
243.058039	9573.560496	27.413210
243.584020	9577.020401	27.418228
243.580441	9595.112470	27.423245
243.802699	9613.882431	27.428263
244.340188	9625.335855	27.433280
243.947303	9632.808635	27.438298
244.427936	9648.212861	27.443316
244.611194	9669.305019	27.448333
245.142768	9678.050730	27.453351
245.442056	9688.853574	27.458368
245.203743	9696.877406	27.463386
245.751987	9716.348988	27.468404
245.962022	9731.574309	27.473421
246.150230	9742.931146	27.478439
246.343593	9751.913149	27.483456
246.431020	9761.010329	27.488474
246.789516	9776.937384	27.493492
246.578273	9782.484337	27.498509
246.980172	9815.966627	27.503527
247.174233	9825.972512	27.508544
247.044396	9847.462417	27.513562
247.632589	9863.824992	27.518580
247.819434	9894.360899	27.523597
247.774683	9915.505234	27.528615
248.261050	9938.710592	27.533632
248.419198	9961.872541	27.538650
249.378020	9983.116601	27.543668
249.445515	9999.547228	27.548685
249.850406	10005.958930	27.553703
250.312813	10032.371825	27.558720
250.335899	10040.128157	27.563738
250.785539	10059.820458	27.568756
251.155756	10077.993888	27.573773
251.455371	10077.283570	27.578791
251.480035	10092.723392	27.583808
251.656977	10113.803006	27.588826
252.198432	10131.439369	27.593844
252.231076	10137.348652	27.598861
252.599849	10143.960145	27.603879
252.937864	10160.554978	27.608896
252.792826	10173.087253	27.613914
253.550864	10181.939974	27.618932
253.364965	10194.651518	27.623949
253.752603	10210.585221	27.628967
253.899789	10227.657478	27.633984
254.358528	10251.170327	27.639002
254.533566	10269.221049	27.644020
254.563674	10285.530545	27.649037
254.856012	10284.179461	27.654055
255.093099	10304.013520	27.659072
255.496426	10328.647845	27.664090
255.673009	10336.684583	27.669108
255.848709	10355.494620	27.674125
256.200602	10370.263892	27.679143
256.738537	10374.545918	27.684160
256.864302	10396.410233	27.689178
257.110017	10402.376570	27.694196
257.419271	10408.026790	27.699213
257.627130	10429.130859	27.704231
258.141713	10439.375620	27.709248
258.295003	10478.710371	27.714266
258.323627	10478.077104	27.719284
258.921857	10497.845438	27.724301
258.488909	10520.069257	27.729319
259.088870	10524.901127	27.734336
258.887651	10555.858455	27.739354
259.098008	10563.265873	27.744372
259.608017	10589.402439	27.749389
259.813533	10598.707445	27.754407
260.247857	10609.980917	27.759424
260.370933	10648.718492	27.764442
260.637761	10663.803778	27.769460
261.078294	10683.104509	27.774477
261.186322	10710.738939	27.779495
261.428319	10726.506599	27.784512
261.803007	10743.379555	27.789530
262.189203	10746.335055	27.794548
262.346749	10771.232018	27.799565
262.782129	10782.834699	27.804583
263.329419	10779.851077	27.809600
263.327094	10796.684764	27.814618
263.742533	10800.279786	27.819636
263.956510	10816.285325	27.824653
263.953651	10833.607518	27.829671
264.219842	10837.192547	27.834688
264.629103	10857.829096	27.839706
265.031370	10870.031244	27.844724
265.094974	10879.254307	27.849741
265.107301	10896.119550	27.854759
265.761084	10904.043862	27.859776
265.626764	10924.310281	27.864794
265.816989	10928.486063	27.869812
266.218272	10955.459627	27.874829
266.004433	10961.862873	27.879847
266.686589	10986.299335	27.884864
266.828816	11020.660467	27.889882
267.284518	11042.271864	27.894900
267.594865	11047.575537	27.899917
267.743751	11071.686681	27.904935
268.612610	11085.784357	27.909952
268.706062	11098.725381	27.914970
268.942527	11113.455335	27.919988
269.048460	11126.040632	27.925005
269.148422	11159.187289	27.930023
269.502185	11167.806447	27.935040
269.619802	11190.037124	27.940058
269.767763	11215.714637	27.945076
270.004946	11223.440899	27.950093
270.398309	11258.751225	27.955111
270.691579	11264.506797	27.960128
270.918827	11302.801799	27.965146
271.507984	11310.477830	27.970164
271.842892	11323.201905	27.975181
272.097250	11349.054260	27.980199
272.504158	11349.614107	27.985216
272.921001	11365.511848	27.990234
273.661141	11362.915334	27.995252
274.048999	11371.551815	28.000269
274.388122	11382.057769	28.005287
274.573842	11389.716205	28.010304
274.376702	11402.632226	28.015322
274.640124	11397.802462	28.020340
275.058352	11414.647669	28.025357
275.203399	11432.751929	28.030375
275.115867	11452.811989	28.035392
275.375523	11458.969418	28.040410
275.325916	11467.790873	28.045428
275.687371	11483.809741	28.050445
275.732785	11522.359817	28.055463
276.242699	11542.161372	28.060480
276.517883	11571.178159	28.065498
276.313786	11596.070772	28.070516
276.798780	11615.088002	28.075533
276.885036	11651.735537	28.080551
276.839534	11667.932109	28.085568
277.185701	11690.805550	28.090586
277.991519	11706.125754	28.095604
278.461751	11746.236827	28.100621
278.978416	11760.943144	28.105639
279.398159	11767.832062	28.110656
279.827439	11793.543588	28.115674
280.442549	11797.610803	28.120692
280.686903	11798.975039	28.125709
280.517130	11827.995694	28.130727
280.805122	11816.504417	28.135744
280.847952	11847.935966	28.140762
281.064450	11854.077833	28.145780
281.549612	11859.105540	28.150797
281.617651	11890.410118	28.155815
282.035170	11886.924664	28.160832
282.292672	11917.955364	28.165850
282.428752	11923.743447	28.170868
282.764502	11930.268188	28.175885
282.994142	11955.050312	28.180903
283.517666	11976.339030	28.185920
283.640595	11987.659412	28.190938
283.712915	12012.159600	28.195956
283.792397	12020.369207	28.200973
283.774316	12044.921405	28.205991
284.405992	12072.537061	28.211008
284.578245	12089.581960	28.216026
284.800009	12120.702460	28.221044
285.315633	12137.814362	28.226061
285.487483	12177.544113	28.231079
285.675598	12184.952810	28.236096
286.199408	12196.224441	28.241114
286.669455	12218.418016	28.246132
287.336316	12232.089238	28.251149
287.390682	12250.524515	28.256167
288.041332	12253.092352	28.261184
288.412589	12286.292629	28.266202
288.449062	12301.287539	28.271220
288.968368	12313.479337	28.276237
289.189421	12326.652363	28.281255
289.497384	12338.988597	28.286272
289.730564	12347.065053	28.291290
289.942638	12373.843816	28.296308
290.261998	12369.715103	28.301325
290.499226	12396.293590	28.306343
290.577415	12393.510861	28.311360
291.078171	12426.139373	28.316378
291.058543	12440.719064	28.321396
291.266895	12450.106613	28.326413
291.242538	12476.010774	28.331431
291.751065	12495.749143	28.336448
292.024203	12520.708510	28.341466
292.214811	12556.822507	28.346484
292.698689	12578.400606	28.351501
292.636603	12620.999858	28.356519
293.284402	12637.034812	28.361536
293.399414	12658.442347	28.366554
293.811493	12686.597958	28.371572
294.229722	12705.276946	28.376589
294.654163	12734.540609	28.381607
295.306223	12729.095570	28.386624
295.441291	12758.189650	28.391642
295.462618	12774.860008	28.396660
296.062901	12786.284861	28.401677
296.161896	12807.648761	28.406695
296.674971	12816.040027	28.411712
297.071885	12831.194105	28.416730
296.891157	12859.354995	28.421748
297.478916	12868.966869	28.426765
297.533344	12893.393364	28.431783
297.816755	12908.081764	28.436800
297.937383	12928.663895	28.441818
298.580817	12971.019889	28.446836
298.832321	12972.628845	28.451853
298.879124	13008.128697	28.456871
299.175074	13005.421757	28.461888
299.615038	13037.899266	28.466906
299.716601	13068.174075	28.471924
300.214106	13076.338009	28.476941
300.711168	13104.852951	28.481959
301.265715	13102.418400	28.486976
301.296359	13122.252248	28.491994
301.501932	13123.712031	28.497012
301.831012	13143.920449	28.502029
301.921245	13164.009999	28.507047
302.166208	13177.134868	28.512064
302.486888	13195.996774	28.517082
302.832591	13226.695576	28.522100
303.122131	13234.190420	28.527117
303.343411	13252.008401	28.532135
303.422827	13278.410371	28.537152
303.785226	13301.571775	28.542170
304.079254	13325.305443	28.547188
304.470704	13352.284672	28.552205
304.653929	13381.852500	28.557223
305.359785	13392.700198	28.562240
305.547339	13408.831658	28.567258
306.143720	13426.542955	28.572276
306.734897	13434.545848	28.577293
306.821184	13455.979673	28.582311
307.440254	13456.598307	28.587328
307.841286	13484.268683	28.592346
307.717456	13487.954989	28.597364
308.159698	13497.980476	28.602381
308.620538	13522.700824	28.607399
309.048951	13546.963318	28.612416
309.045741	13549.303774	28.617434
308.981248	13580.666626	28.622452
309.350084	13575.537541	28.627469
309.747514	13600.354360	28.632487
309.765977	13628.887061	28.637504
309.975431	13647.039115	28.642522
309.972750	13680.573494	28.647540
310.752817	13696.598689	28.652557
310.770620	13735.890544	28.657575
311.318764	13761.126271	28.662592
311.881189	13773.847010	28.667610
312.096271	13804.753639	28.672628
312.224371	13827.469978	28.677645
312.550734	13857.267931	28.682663
312.996637	13885.122244	28.687680
313.381884	13913.213528	28.692698
313.499922	13941.579061	28.697716
313.957606	13948.546958	28.702733
314.123540	13980.814011	28.707751
314.361160	14006.374022	28.712768
315.049009	14026.650335	28.717786
315.140364	14062.328718	28.722804
315.410237	14074.218769	28.727821
315.448937	14106.648908	28.732839
316.042525	14153.444856	28.737856
316.144806	14159.931080	28.742874
316.585314	14189.736001	28.747892
317.107512	14211.278448	28.752909
317.505355	14231.979534	28.757927
317.369470	14265.439434	28.762944
317.713087	14288.788935	28.767962
317.722775	14303.103103	28.772980
318.196100	14353.425553	28.777997
318.511839	14372.782078	28.783015
318.664245	14406.835978	28.788032
319.630064	14438.094095	28.793050
319.792625	14464.281781	28.798068
320.547091	14483.810203	28.803085
320.776724	14499.088824	28.808103
321.192708	14510.713964	28.813120
321.860190	14522.217200	28.818138
321.754098	14557.246981	28.823156
322.279645	14550.702653	28.828173
322.438055	14583.663917	28.833191
323.004281	14593.081839	28.838208
323.224208	14601.951874	28.843226
323.295206	14631.046521	28.848244
323.859996	14647.765334	28.853261
323.999895	14657.419182	28.858279
324.036566	14675.008439	28.863296
324.648434	14686.636013	28.868314
324.855356	14718.733883	28.873332
325.047288	14738.026207	28.878349
325.540281	14749.623040	28.883367
326.028498	14777.577480	28.888384
326.275014	14790.965777	28.893402
326.270413	14821.652209	28.898420
326.768840	14844.699596	28.903437
327.018281	14855.418045	28.908455
327.307552	14887.863505	28.913472
327.558001	14897.696210	28.918490
327.761818	14935.304065	28.923508
328.322065	14965.648474	28.928525
328.493915	14986.096334	28.933543
328.735836	15012.692540	28.938560
329.269284	15036.128370	28.943578
329.425828	15052.729099	28.948596
329.579800	15080.105797	28.953613
329.893785	15110.954456	28.958631
330.415028	15136.088044	28.963648
331.134097	15172.842320	28.968666
331.107448	15185.735558	28.973684
331.943550	15216.529680	28.978701
332.386334	15237.352272	28.983719
332.344778	15267.711571	28.988736
333.092412	15278.158896	28.993754
333.157023	15301.579589	28.998772
333.280465	15322.420377	29.003789
333.684793	15352.234993	29.008807
333.974633	15371.518198	29.013824
334.361871	15394.910940	29.018842
334.306194	15427.625632	29.023860
334.942520	15444.814091	29.028877
335.128900	15481.817807	29.033895
335.402520	15512.240533	29.038912
336.190462	15551.077047	29.043930
336.124131	15561.532955	29.048948
336.933819	15582.465571	29.053965
337.140280	15615.288618	29.058983
337.049305	15652.363756	29.064000
337.598115	15660.404704	29.069018
338.019577	15699.796945	29.074036
338.453670	15731.093403	29.079053
338.820171	15737.599645	29.084071
338.936416	15763.431470	29.089088
339.898310	15786.099483	29.094106
340.122641	15814.252167	29.099124
340.395225	15821.137991	29.104141
340.425250	15843.203597	29.109159
340.933632	15868.034719	29.114176
341.276458	15897.939291	29.119194
341.137015	15938.045680	29.124212
341.932684	15942.815365	29.129229
342.420642	15957.318308	29.134247
342.372553	15993.254053	29.139264
342.883902	16015.358570	29.144282
343.030862	16051.142449	29.149300
343.351321	16077.341320	29.154317
344.190285	16106.455146	29.159335
344.347904	16126.728711	29.164352
344.749668	16139.510956	29.169370
344.741212	16172.039683	29.174388
344.987880	16179.640688	29.179405
345.295376	16205.966407	29.184423
345.232133	16240.061348	29.189440
346.434428	16239.364769	29.194458
346.782950	16256.177707	29.199476
347.265595	16290.111655	29.204493
347.513050	16305.006076	29.209511
347.852115	16322.230392	29.214528
347.954422	16343.110650	29.219546
348.197210	16367.477378	29.224564
348.210770	16391.932442	29.229581
348.441396	16421.126842	29.234599
349.084176	16458.862695	29.239616
349.784914	16468.472247	29.244634
349.721858	16514.122708	29.249652
350.125698	16531.618642	29.254669
350.671055	16555.358862	29.259687
350.948548	16596.597304	29.264704
351.666963	16622.159229	29.269722
351.706357	16649.076818	29.274740
352.147243	16665.975784	29.279757
352.531426	16693.742678	29.284775
352.846720	16726.036209	29.289792
353.196224	16737.062449	29.294810
353.851730	16775.227177	29.299828
354.039036	16798.541494	29.304845
354.616128	16821.104316	29.309863
354.311231	16844.011450	29.314880
354.717002	16884.203451	29.319898
355.007577	16907.551295	29.324916
355.501688	16939.193185	29.329933
355.527270	16961.435971	29.334951
355.955776	17002.229694	29.339968
356.527673	17028.032375	29.344986
356.773443	17057.023678	29.350004
357.044810	17095.399184	29.355021
357.891561	17122.742089	29.360039
357.923363	17160.845271	29.365056
358.297005	17187.962269	29.370074
359.005729	17214.815920	29.375092
359.243783	17233.900272	29.380109
359.713452	17265.789541	29.385127
360.029941	17297.255005	29.390144
360.777185	17305.281328	29.395162
361.021718	17327.516811	29.400180
361.683918	17363.108121	29.405197
362.057067	17357.859733	29.410215
362.287464	17380.871464	29.415232
362.866368	17418.495579	29.420250
362.786708	17426.089609	29.425268
363.212000	17460.739962	29.430285
363.778216	17490.388322	29.435303
363.897592	17496.305671	29.440320
364.530065	17520.305562	29.445338
364.540316	17549.617185	29.450356
364.594616	17571.079053	29.455373
365.166930	17593.416778	29.460391
365.322796	17628.061558	29.465408
365.390058	17662.211975	29.470426
365.715123	17690.302391	29.475444
366.183724	17741.761413	29.480461
366.670496	17777.694670	29.485479
366.615728	17803.100901	29.490496
367.333814	17840.788101	29.495514
367.860048	17870.385439	29.500532
368.201606	17895.420577	29.505549
368.612069	17924.876376	29.510567
368.887486	17943.863969	29.515584
369.296135	17974.470714	29.520602
369.465587	17994.620126	29.525620
369.624117	18036.918927	29.530637
370.292979	18051.746901	29.535655
370.514361	18092.917996	29.540672
370.830933	18114.529533	29.545690
371.339362	18143.274470	29.550708
371.828146	18174.741524	29.555725
372.545942	18178.497110	29.560743
372.859576	18216.248836	29.565760
373.343637	18232.313244	29.570778
373.768226	18268.232630	29.575796
374.039385	18280.562135	29.580813
374.648875	18309.676823	29.585831
374.876625	18330.326110	29.590848
375.096482	18353.653022	29.595866
375.477398	18373.810521	29.600884
375.587102	18404.637677	29.605901
376.277687	18428.840504	29.610919
376.143207	18470.351886	29.615936
376.623837	18502.993577	29.620954
377.120680	18527.075667	29.625972
377.484909	18556.519746	29.630989
377.989483	18582.175229	29.636007
378.145595	18621.430775	29.641024
378.493974	18663.531172	29.646042
378.660171	18697.429390	29.651060
378.943810	18738.235597	29.656077
379.667817	18771.516951	29.661095
379.603348	18812.097133	29.666112
380.189394	18838.355846	29.671130
380.460886	18886.687593	29.676148
380.798103	18920.739280	29.681165
381.407787	18949.921270	29.686183
381.691660	18989.898978	29.691200
382.383414	19022.453231	29.696218
382.955852	19058.622601	29.701236
383.256584	19087.945717	29.706253
384.062349	19115.976496	29.711271
384.374215	19138.996143	29.716288
384.811698	19161.987190	29.721306
385.194026	19196.684551	29.726324
385.406262	19232.381041	29.731341
385.877196	19253.186764	29.736359
386.245735	19294.377531	29.741376
386.443118	19325.210836	29.746394
387.054529	19343.164119	29.751412
387.116283	19387.597684	29.756429
387.596311	19416.719955	29.761447
387.915527	19441.419089	29.766464
388.425299	19484.536820	29.771482
388.784684	19498.312274	29.776500
389.120073	19526.999943	29.781517
389.498480	19548.927856	29.786535
389.809168	19591.675232	29.791552
390.103220	19627.299160	29.796570
390.933674	19655.106102	29.801588
390.830878	19687.011092	29.806605
391.337019	19713.878655	29.811623
391.622713	19752.246953	29.816640
392.037118	19789.746036	29.821658
392.789862	19822.791476	29.826676
392.781178	19855.031178	29.831693
393.396262	19888.742615	29.836711
393.367629	19917.757489	29.841728
394.044407	19957.072061	29.846746
394.587800	19980.811257	29.851764
394.661046	20009.919803	29.856781
395.337608	20045.408932	29.861799
395.250142	20057.764332	29.866816
395.999629	20094.966002	29.871834
396.292108	20120.986788	29.876852
396.480404	20155.045125	29.881869
397.386310	20191.987880	29.886887
397.543870	20214.995107	29.891904
397.839894	20258.217945	29.896922
398.542692	20282.946397	29.901940
398.477496	20312.297452	29.906957
399.266582	20336.902964	29.911975
399.750953	20375.025501	29.916992
400.286819	20412.118149	29.922010
400.898185	20440.943091	29.927028
400.936686	20467.318492	29.932045
401.395720	20492.457967	29.937063
401.536260	20523.332842	29.942080
401.985096	20561.204731	29.947098
402.782899	20595.196389	29.952116
403.023128	20621.169842	29.957133
403.380987	20654.594295	29.962151
403.623948	20676.109423	29.967168
403.684044	20715.065789	29.972186
404.585438	20750.419977	29.977204
404.822656	20795.846664	29.982221
405.149540	20818.583994	29.987239
405.767234	20864.260139	29.992256
405.634048	20905.383304	29.997274
406.546105	20933.243548	30.002292
406.821913	20980.070503	30.007309
407.499493	21001.288833	30.012327
407.599148	21044.658078	30.017344
408.172669	21077.723016	30.022362
408.778091	21099.751052	30.027380
409.118886	21148.804668	30.032397
409.900895	21162.919986	30.037415
410.401693	21200.374881	30.042432
410.609387	21227.798653	30.047450
410.848905	21235.499344	30.052468
411.228698	21279.097220	30.057485
411.581934	21311.869540	30.062503
412.250934	21341.156300	30.067520
412.463497	21369.211649	30.072538
413.125219	21401.526468	30.077556
413.031094	21440.606168	30.082573
413.688734	21467.583967	30.087591
414.202077	21507.179864	30.092608
414.369359	21549.099955	30.097626
414.904121	21574.173381	30.102644
415.313244	21612.085752	30.107661
416.006555	21642.338546	30.112679
416.099966	21664.122430	30.117696
416.465854	21718.243472	30.122714
417.201460	21727.161450	30.127732
417.128867	21775.716092	30.132749
417.495307	21818.278689	30.137767
418.210064	21838.782534	30.142784
418.389399	21883.739343	30.147802
418.699727	21908.071565	30.152820
419.311624	21949.644906	30.157837
419.808060	21985.108029	30.162855
420.086167	22027.208072	30.167872
420.608120	22051.387307	30.172890
421.110045	22091.987553	30.177908
421.044361	22126.711440	30.182925
421.733403	22170.033541	30.187943
422.185834	22193.901282	30.192960
422.664628	22225.372953	30.197978
423.292285	22259.258963	30.202996
423.576885	22291.850634	30.208013
423.524150	22321.360813	30.213031
423.867796	22366.465194	30.218048
423.931784	22393.296619	30.223066
424.660662	22432.950545	30.228084
424.881403	22482.098850	30.233101
425.367446	22516.688262	30.238119
425.956889	22573.910881	30.243136
425.696067	22614.535915	30.248154
426.004164	22662.281378	30.253172
426.318976	22733.792502	30.258189
426.708026	22788.556413	30.263207
427.480273	22830.078652	30.268224
427.647261	22902.243964	30.273242
428.205851	22952.436710	30.278260
428.918706	22993.666462	30.283277
429.715319	23049.194759	30.288295
430.384620	23098.791047	30.293312
430.239481	23137.030187	30.298330
431.318617	23177.384784	30.303348
431.574538	23223.675798	30.308365
432.101546	23277.395296	30.313383
432.368852	23308.998533	30.318400
433.121040	23359.021773	30.323418
433.750099	23401.571810	30.328436
434.273093	23448.096810	30.333453
434.727681	23471.792587	30.338471
435.700971	23495.175680	30.343488
436.418626	23540.869429	30.348506
436.717719	23568.190490	30.353524
437.053590	23596.301723	30.358541
437.625050	23622.562523	30.363559
437.763245	23658.004799	30.368576
437.973023	23681.687706	30.373594
437.974824	23729.746943	30.378612
438.820258	23755.560647	30.383629
438.897186	23790.653845	30.388647
439.295097	23841.646775	30.393664
439.647305	23888.401440	30.398682
440.255350	23932.572377	30.403700
440.405185	23976.798623	30.408717
440.825274	24025.734037	30.413735
441.422010	24061.749432	30.418752
441.777936	24121.770361	30.423770
442.276353	24166.988024	30.428788
443.102155	24200.487313	30.433805
443.282922	24238.358197	30.438823
443.850926	24275.972841	30.443840
444.049771	24313.992272	30.448858
444.204689	24378.381688	30.453876
444.978478	24407.768451	30.458893
445.424494	24441.616341	30.463911
446.137239	24487.291394	30.468928
446.795882	24528.325736	30.473946
447.537327	24550.058345	30.478964
447.970708	24584.167192	30.483981
448.308564	24620.836741	30.488999
449.012958	24644.439296	30.494016
449.140676	24686.324863	30.499034
449.271789	24716.983539	30.504052
450.033062	24748.719163	30.509069
450.517096	24800.077604	30.514087
450.733929	24842.398212	30.519104
450.960120	24873.582294	30.524122
451.225558	24893.177050	30.529140
451.775978	24944.827702	30.534157
452.447280	24982.887274	30.539175
452.561302	25007.423546	30.544192
452.825827	25061.707688	30.549210
453.284166	25086.045288	30.554228
453.780331	25128.325199	30.559245
454.212824	25186.222789	30.564263
454.883636	25214.153669	30.569280
455.264180	25263.342022	30.574298
455.738403	25306.053313	30.579316
456.211030	25350.225096	30.584333
456.370110	25391.358242	30.589351
457.188172	25419.560001	30.594368
457.690932	25465.638203	30.599386
458.319476	25510.716548	30.604404
458.524545	25534.692963	30.609421
458.747878	25599.206590	30.614439
459.554101	25637.519715	30.619456
460.089966	25680.045160	30.624474
460.546835	25695.271349	30.629492
461.101260	25752.272431	30.634509
461.312995	25788.571128	30.639527
461.820596	25829.414391	30.644544
462.396716	25872.126044	30.649562
462.472946	25919.988396	30.654580
463.370881	25959.800883	30.659597
463.571611	26007.813218	30.664615
464.527582	26036.242369	30.669632
464.815886	26095.683824	30.674650
465.229324	26128.376732	30.679668
465.576648	26180.380068	30.684685
466.152193	26227.987350	30.689703
466.773798	26261.373073	30.694720
467.315196	26316.369240	30.699738
467.625271	26333.384795	30.704756
468.226689	26386.475845	30.709773
468.377887	26425.319979	30.714791
469.095265	26465.251782	30.719808
469.582553	26520.418390	30.724826
469.910276	26552.014547	30.729844
470.055423	26599.228770	30.734861
470.446039	26647.306155	30.739879
471.313507	26683.547329	30.744896
471.933761	26727.337187	30.749914
472.463785	26757.638762	30.754932
472.547167	26805.562341	30.759949
473.072489	26841.710558	30.764967
473.780272	26892.529010	30.769984
474.415873	26942.384979	30.775002
474.818992	26986.268139	30.780020
475.505130	27014.325607	30.785037
475.891481	27061.359339	30.790055
476.214382	27106.047692	30.795072
476.599636	27146.099029	30.800090
477.113381	27184.113863	30.805108
477.357109	27223.535892	30.810125
477.666425	27273.919818	30.815143
478.300509	27298.393986	30.820160
478.631749	27367.446076	30.825178
479.057839	27411.130984	30.830196
479.473301	27465.796831	30.835213
479.761374	27523.231037	30.840231
480.521134	27563.562124	30.845248
480.878280	27619.953881	30.850266
481.930828	27660.908643	30.855284
482.028561	27706.957298	30.860301
482.642606	27751.731714	30.865319
483.367876	27779.162627	30.870336
483.673033	27830.419396	30.875354
483.981869	27868.097416	30.880372
484.524224	27903.317766	30.885389
484.465890	27951.061364	30.890407
485.534318	28003.703383	30.895424
485.976528	28036.606515	30.900442
485.931777	28080.424522	30.905460
486.543946	28128.543592	30.910477
486.993662	28181.786708	30.915495
487.528508	28226.638529	30.920512
488.361843	28267.971601	30.925530
488.834784	28315.820858	30.930548
489.568972	28366.774953	30.935565
490.339544	28397.681574	30.940583
490.645541	28439.199942	30.945600
490.647200	28484.768190	30.950618
491.167482	28524.317852	30.955636
491.687481	28571.507130	30.960653
491.965625	28626.565241	30.965671
492.968993	28679.043444	30.970688
493.164834	28715.789411	30.975706
493.542493	28773.017434	30.980724
493.878884	28814.620006	30.985741
494.144376	28864.350289	30.990759
494.783281	28935.430205	30.995776
495.487587	28996.468996	31.000794
495.743596	29047.598720	31.005812
496.337681	29098.833623	31.010829
496.885471	29147.183823	31.015847
497.337828	29214.889052	31.020864
497.940329	29279.005349	31.025882
498.703914	29310.309057	31.030900
499.293279	29366.308585	31.035917
499.742498	29417.158296	31.040935
500.353771	29471.681462	31.045952
500.895657	29514.103456	31.050970
501.308093	29574.085315	31.055988
501.948543	29615.321000	31.061005
502.574483	29659.647339	31.066023
503.035833	29703.502582	31.071040
503.659702	29758.661764	31.076058
503.567380	29799.917984	31.081076
504.624253	29854.245732	31.086093
504.641857	29907.530851	31.091111
505.354294	29951.991912	31.096128
505.768021	30008.593487	31.101146
506.462227	30061.786249	31.106164
507.038906	30100.535281	31.111181
507.334243	30162.260866	31.116199
508.251173	30205.225116	31.121216
508.221271	30252.169131	31.126234
508.814968	30311.111004	31.131252
509.573586	30352.899897	31.136269
509.516173	30406.290419	31.141287
510.142846	30462.044431	31.146304
510.702480	30511.743481	31.151322
511.498312	30573.403632	31.156340
512.115940	30611.320546	31.161357
512.270707	30680.866148	31.166375
513.170030	30728.768380	31.171392
513.363118	30778.055548	31.176410
513.685310	30828.744261	31.181428
514.532935	30862.727787	31.186445
515.050322	30929.369020	31.191463
515.642273	30978.341657	31.196480
515.997143	31010.599254	31.201498
516.358953	31078.793605	31.206516
517.204462	31113.923114	31.211533
517.372704	31164.023073	31.216551
518.007118	31215.784406	31.221568
518.558618	31253.022768	31.226586
519.047240	31310.568931	31.231604
519.741730	31344.679646	31.236621
520.038924	31392.257278	31.241639
520.879735	31444.464717	31.246656
520.993531	31494.893247	31.251674
521.836860	31533.522565	31.256692
522.282404	31575.142126	31.261709
522.607485	31618.119299	31.266727
523.078054	31673.404527	31.271744
523.720396	31713.509171	31.276762
524.141385	31769.115213	31.281780
524.578705	31828.491869	31.286797
525.099453	31872.472123	31.291815
525.773683	31929.469128	31.296832
526.091794	31980.934794	31.301850
526.473470	32049.022392	31.306868
527.328287	32102.005577	31.311885
527.652291	32161.846915	31.316903
527.844156	32216.381716	31.321920
528.612443	32283.545091	31.326938
528.916202	32333.698581	31.331956
529.730127	32396.598912	31.336973
530.332614	32460.127515	31.341991
530.494060	32522.631284	31.347008
531.104744	32593.768686	31.352026
531.591710	32652.603599	31.357044
532.095446	32717.108547	31.362061
532.917671	32780.753455	31.367079
533.493078	32832.308478	31.372096
533.745267	32880.676870	31.377114
534.306437	32950.602919	31.382132
534.815197	33020.326516	31.387149
535.525484	33077.542154	31.392167
536.391613	33139.732960	31.397184
536.870046	33190.216566	31.402202
537.224915	33256.189936	31.407220
538.258441	33313.548567	31.412237
538.908565	33376.880162	31.417255
539.216199	33422.634797	31.422272
539.969132	33479.507107	31.427290
540.215069	33542.170921	31.432308
540.863965	33591.195106	31.437325
541.286799	33648.882868	31.442343
542.083463	33703.590576	31.447360
542.548156	33756.816732	31.452378
542.997530	33831.812976	31.457396
543.630435	33866.954742	31.462413
543.823649	33932.774347	31.467431
544.390836	33988.514723	31.472448
545.039579	34049.810719	31.477466
545.439237	34102.581692	31.482484
546.039142	34165.630984	31.487501
547.330946	34209.350911	31.492519
547.756818	34247.884789	31.497536
548.311384	34307.228373	31.502554
549.119634	34369.587692	31.507572
549.662426	34386.059996	31.512589
550.177195	34460.372885	31.517607
550.406946	34512.661994	31.522624
551.131406	34555.880142	31.527642
551.065578	34627.938944	31.532660
551.798673	34667.852345	31.537677
552.232444	34735.610427	31.542695
552.730367	34786.758002	31.547712
553.253685	34838.841820	31.552730
553.623251	34888.856039	31.557748
554.181807	34939.943556	31.562765
554.751320	34999.103982	31.567783
555.131276	35065.262979	31.572800
555.631190	35110.043615	31.577818
556.418158	35163.690932	31.582836
556.891733	35241.655225	31.587853
557.312625	35292.501443	31.592871
557.887006	35352.315414	31.597888
558.456923	35419.697061	31.602906
558.660746	35484.536185	31.607924
559.618798	35547.673242	31.612941
560.024791	35611.570665	31.617959
560.345054	35674.466412	31.622976
560.935638	35743.234285	31.627994
561.545496	35813.403440	31.633012
561.909523	35873.282308	31.638029
562.223410	35953.696381	31.643047
562.909036	36037.571008	31.648064
563.755871	36099.582932	31.653082
564.023794	36168.572985	31.658100
565.048687	36241.679382	31.663117
565.853241	36313.935749	31.668135
566.293244	36387.215081	31.673152
566.850935	36447.534078	31.678170
567.582940	36519.812729	31.683188
568.294232	36575.250272	31.688205
568.609043	36639.545119	31.693223
569.080662	36718.450274	31.698240
569.674091	36775.107058	31.703258
570.348021	36849.675036	31.708276
571.788008	36893.493882	31.713293
572.124009	36954.854720	31.718311
572.487717	37014.134730	31.723328
573.453392	37069.853677	31.728346
573.921867	37131.433076	31.733364
574.488699	37193.646527	31.738381
574.625877	37255.987962	31.743399
575.051108	37324.129684	31.748416
576.306956	37382.461997	31.753434
576.558748	37441.638831	31.758452
577.254059	37506.290512	31.763469
577.954110	37563.604370	31.768487
578.296036	37622.899459	31.773504
579.014375	37681.034343	31.778522
579.736557	37748.734155	31.783540
580.263450	37804.193341	31.788557
580.632032	37863.008286	31.793575
580.927846	37926.641846	31.798592
581.874424	37991.023395	31.803610
582.171436	38044.675095	31.808628
583.021742	38112.320402	31.813645
583.711809	38172.462396	31.818663
584.336795	38242.281967	31.823680
585.311511	38295.948723	31.828698
585.397684	38355.948064	31.833716
585.808812	38409.449455	31.838733
586.388351	38482.120986	31.843751
586.651139	38541.488983	31.848768
587.346129	38609.739359	31.853786
587.678390	38673.776664	31.858804
588.147068	38746.013104	31.863821
588.975097	38815.892888	31.868839
589.518289	38888.527876	31.873856
589.981285	38963.612881	31.878874
590.640201	39036.387154	31.883892
591.167525	39105.831691	31.888909
591.975277	39169.280936	31.893927
592.106209	39232.782222	31.898944
593.402810	39289.185621	31.903962
593.470595	39350.131825	31.908980
594.271607	39411.632547	31.913997
594.977096	39480.212720	31.919015
595.535557	39546.412441	31.924032
596.481728	39600.968370	31.929050
596.850355	39672.275029	31.934068
597.737453	39733.014612	31.939085
597.987811	39796.343497	31.944103
598.441664	39857.596921	31.949120
599.177031	39921.802473	31.954138
599.585639	39986.709250	31.959156
600.119902	40067.484077	31.964173
601.022412	40125.091426	31.969191
601.154876	40199.907899	31.974208
601.772432	40254.810451	31.979226
602.357818	40338.106224	31.984244
602.852154	40417.210049	31.989261
603.538713	40497.545003	31.994279
603.894849	40561.042150	31.999296
604.668283	40644.374552	32.004314
605.226301	40726.846505	32.009332
605.859235	40809.596845	32.014349
606.449634	40882.598169	32.019367
607.067900	40966.746772	32.024384
608.042907	41037.014872	32.029402
608.540986	41112.077724	32.034420
609.410835	41175.492169	32.039437
610.091951	41250.976735	32.044455
610.649915	41314.648345	32.049472
611.205889	41385.024872	32.054490
611.782619	41472.197108	32.059508
612.421009	41538.870672	32.064525
613.276529	41603.993489	32.069543
613.775542	41691.612051	32.074560
614.426404	41751.261043	32.079578
615.231382	41828.552023	32.084596
616.060592	41900.065959	32.089613
616.902376	41965.997262	32.094631
616.913329	42040.794001	32.099648
617.566287	42101.453900	32.104666
617.889235	42174.577162	32.109684
618.775639	42241.515362	32.114701
619.876476	42311.969613	32.119719
620.232060	42385.659679	32.124736
620.818306	42444.040000	32.129754
621.466408	42517.050950	32.134772
621.972008	42595.373180	32.139789
622.921983	42652.096806	32.144807
623.618587	42727.607003	32.149824
624.312550	42792.375613	32.154842
625.090039	42851.609529	32.159860
625.461283	42916.176179	32.164877
626.467814	42970.186118	32.169895
627.207346	43033.650627	32.174912
628.208506	43084.356658	32.179930
628.431914	43145.002561	32.184948
628.650035	43205.728457	32.189965
629.355734	43271.743752	32.194983
629.624276	43347.197762	32.200000
630.384862	43408.838604	32.205018
631.054133	43468.910001	32.210036
631.049320	43544.280532	32.215053
632.218963	43610.551889	32.220071
632.379886	43683.013398	32.225088
632.942225	43757.170440	32.230106
633.805549	43817.851773	32.235124
633.946381	43896.555471	32.240141
634.781199	43959.000377	32.245159
635.030689	44040.897336	32.250176
635.952432	44117.433622	32.255194
636.450081	44187.918915	32.260212
636.841873	44268.843135	32.265229
637.794493	44339.086545	32.270247
638.130839	44419.389182	32.275264
638.817093	44488.644811	32.280282
639.408799	44557.133372	32.285300
640.149863	44651.952481	32.290317
640.835894	44723.643105	32.295335
641.316009	44802.686094	32.300352
642.060165	44886.503517	32.305370
642.390643	44972.186026	32.310388
643.027515	45061.789973	32.315405
643.932775	45139.968592	32.320423
644.133813	45231.021840	32.325440
644.802155	45322.247773	32.330458
645.631054	45423.326425	32.335476
645.995122	45521.126303	32.340493
646.852643	45606.099566	32.345511
647.525817	45700.442714	32.350528
648.805795	45779.588232	32.355546
649.382790	45852.551482	32.360564
650.056387	45936.811519	32.365581
651.078987	46011.198339	32.370599
651.857314	46111.603951	32.375616
652.052547	46172.116011	32.380634
652.834580	46259.861044	32.385652
653.451931	46350.333203	32.390669
654.006223	46419.649390	32.395687
654.474003	46509.351370	32.400704
654.956652	46596.165487	32.405722
655.514640	46690.668429	32.410740
656.044891	46785.520584	32.415757
656.785693	46867.314101	32.420775
657.673126	46973.026565	32.425792
658.430962	47057.078820	32.430810
659.353077	47151.779704	32.435828
659.485903	47237.928351	32.440845
660.325262	47322.719813	32.445863
661.095496	47419.508974	32.450880
661.642660	47498.463890	32.455898
662.347574	47590.667369	32.460916
663.380361	47672.747718	32.465933
664.099528	47765.492799	32.470951
664.777495	47861.266948	32.475968
665.963456	47931.330634	32.480986
666.837904	48012.469234	32.486004
667.271853	48101.148710	32.491021
668.266786	48157.663856	32.496039
669.184801	48236.860600	32.501056
669.945379	48316.443651	32.506074
670.196838	48387.759077	32.511092
670.539392	48439.693668	32.516109
671.527976	48519.006250	32.521127
671.781514	48593.028250	32.526144
672.481321	48680.135053	32.531162
673.018011	48748.648046	32.536180
673.377890	48828.934136	32.541197
674.340636	48925.298205	32.546215
675.093145	48998.225745	32.551232
675.604411	49087.478111	32.556250
676.445998	49167.663980	32.561268
677.165052	49252.976611	32.566285
677.745641	49319.296054	32.571303
678.191492	49403.378719	32.576320
678.692619	49487.326314	32.581338
679.523821	49560.344073	32.586356
680.227132	49634.179021	32.591373
680.902182	49714.202074	32.596391
681.206467	49791.848793	32.601408
681.461097	49883.563084	32.606426
682.535980	49947.428334	32.611444
683.037544	50051.901754	32.616461
683.540188	50125.478060	32.621479
684.110890	50235.675926	32.626496
684.805193	50336.980048	32.631514
685.741394	50411.780639	32.636532
686.391763	50520.176402	32.641549
687.765632	50577.558339	32.646567
688.406654	50669.023117	32.651584
689.167823	50757.796769	32.656602
689.748304	50839.981340	32.661620
690.024801	50919.194173	32.666637
690.788101	51013.729021	32.671655
691.370375	51121.589934	32.676672
691.750058	51196.712894	32.681690
692.993629	51298.935700	32.686708
693.149525	51411.681688	32.691725
694.137519	51495.554563	32.696743
694.617442	51599.686304	32.701760
695.518847	51701.159263	32.706778
696.085276	51801.386886	32.711796
696.452607	51884.741791	32.716813
697.476205	51980.767018	32.721831
698.322034	52089.903692	32.726848
698.795224	52201.051198	32.731866
699.570826	52300.185689	32.736884
700.275396	52401.919098	32.741901
701.174278	52498.046465	32.746919
701.623568	52595.950920	32.751936
702.237535	52714.146564	32.756954
703.566473	52801.007204	32.761972
704.247014	52888.341690	32.766989
705.210006	52983.905014	32.772007
706.254936	53078.886759	32.777024
706.987524	53170.689447	32.782042
707.478574	53251.932617	32.787060
707.948336	53346.590587	32.792077
708.822530	53427.272179	32.797095
710.453066	53522.870063	32.802112
710.721641	53598.352389	32.807130
711.626306	53685.328138	32.812148
712.257745	53773.025330	32.817165
713.310363	53848.972964	32.822183
713.288876	53933.443257	32.827200
713.831592	54027.366031	32.832218
714.577490	54106.113308	32.837236
714.874206	54217.791140	32.842253
715.680309	54310.850545	32.847271
716.249343	54410.216332	32.852288
716.411552	54506.149995	32.857306
717.295445	54609.495277	32.862324
718.125739	54726.944138	32.867341
718.896678	54814.130234	32.872359
719.865538	54923.635309	32.877376
720.650617	55024.453164	32.882394
721.727954	55125.741316	32.887412
722.734032	55205.745178	32.892429
723.341651	55306.429539	32.897447
724.041858	55384.551456	32.902464
724.450254	55474.839163	32.907482
725.382046	55563.417204	32.912500
726.101580	55654.690462	32.917517
726.719148	55727.090899	32.922535
727.508551	55823.736134	32.927552
727.813660	55907.346045	32.932570
728.832432	55986.940353	32.937588
729.187300	56078.642244	32.942605
730.386995	56170.571487	32.947623
731.133953	56253.528662	32.952640
731.483533	56343.065615	32.957658
732.401498	56437.020151	32.962676
732.858443	56533.818558	32.967693
733.781854	56633.648888	32.972711
734.422542	56738.991549	32.977728
734.939171	56832.780485	32.982746
735.640950	56918.224626	32.987764
735.926374	57041.229903	32.992781
736.863882	57130.395350	32.997799
737.524242	57238.030940	33.002816
737.933944	57364.170508	33.007834
738.565380	57460.862518	33.012852
739.278895	57584.286994	33.017869
740.348757	57694.934487	33.022887
741.120653	57811.798582	33.027904
741.722741	57929.961419	33.032922
742.645756	58025.742414	33.037940
743.660521	58147.003962	33.042957
744.184589	58269.832148	33.047975
744.960646	58370.959314	33.052992
745.606314	58472.759347	33.058010
746.286808	58592.132681	33.063028
747.122104	58723.821607	33.068045
748.293330	58828.620207	33.073063
748.991867	58927.892664	33.078080
749.628839	59065.031792	33.083098
750.400951	59158.543126	33.088116
751.007808	59296.086906	33.093133
751.519272	59401.882122	33.098151
753.064415	59513.326965	33.103168
753.743837	59634.697202	33.108186
754.549877	59718.701789	33.113204
755.178598	59841.029507	33.118221
755.531597	59962.613617	33.123239
756.865650	60072.567220	33.128256
757.301272	60188.799390	33.133274
758.381499	60299.573416	33.138292
759.308047	60398.095146	33.143309
759.880098	60501.086752	33.148327
761.034401	60608.734856	33.153344
761.474815	60715.319709	33.158362
762.685436	60821.152322	33.163380
763.135447	60945.045581	33.168397
763.703769	61042.801790	33.173415
764.535394	61155.176180	33.178432
765.384368	61262.044036	33.183450
766.154528	61371.390098	33.188468
766.741184	61474.270529	33.193485
767.667303	61590.524606	33.198503
768.548208	61701.257126	33.203520
769.262448	61825.409191	33.208538
770.480955	61894.440319	33.213556
771.872381	61994.182328	33.218573
772.733032	62101.709963	33.223591
773.354169	62204.525226	33.228608
773.600665	62300.571133	33.233626
774.380652	62385.545473	33.238644
775.132005	62492.973160	33.243661
775.455214	62600.415237	33.248679
776.057997	62699.292408	33.253696
777.081832	62805.627643	33.258714
777.603955	62904.879375	33.263732
778.027071	62999.407900	33.268749
778.743933	63114.043116	33.273767
779.410941	63223.921836	33.278784
779.744863	63341.459305	33.283802
780.691739	63453.176457	33.288820
781.244504	63584.394020	33.293837
781.969050	63699.442080	33.298855
782.691982	63822.637934	33.303872
783.601024	63944.217392	33.308890
784.642564	64063.835338	33.313908
785.533643	64184.332087	33.318925
785.846376	64310.171032	33.323943
787.208751	64416.838010	33.328960
787.744868	64547.166998	33.333978
788.658734	64657.714257	33.338996
789.746181	64788.048546	33.344013
790.163750	64907.483716	33.349031
791.049485	65029.067152	33.354048
791.598088	65169.460562	33.359066
792.550768	65283.247317	33.364084
793.053369	65418.580776	33.369101
794.111680	65535.429716	33.374119
795.249351	65657.676883	33.379136
795.632315	65796.034996	33.384154
796.355548	65930.109127	33.389172
797.163068	66054.732960	33.394189
798.054250	66191.233602	33.399207
799.272612	66313.452372	33.404224
799.713469	66451.798999	33.409242
800.668793	66581.875696	33.414260
801.899440	66705.649763	33.419277
802.598087	66829.847444	33.424295
803.414885	66950.574946	33.429312
804.024940	67086.103869	33.434330
805.332590	67203.483674	33.439348
806.406007	67331.592283	33.444365
807.082524	67460.791292	33.449383
807.987745	67567.044363	33.454400
808.513811	67684.239873	33.459418
809.331960	67814.764172	33.464436
809.829194	67930.562450	33.469453
810.467607	68068.337248	33.474471
811.468011	68184.452110	33.479488
812.158750	68330.570895	33.484506
812.962429	68460.583247	33.489524
813.957946	68585.652718	33.494541
814.599976	68717.735293	33.499559
815.825106	68835.277003	33.504576
816.864708	68972.770254	33.509594
817.584106	69097.490101	33.514612
818.535432	69225.131069	33.519629
819.309424	69349.868689	33.524647
820.278475	69459.016321	33.529664
821.096608	69577.305857	33.534682
822.035110	69708.283609	33.539700
822.824246	69807.214630	33.544717
823.458499	69944.882336	33.549735
824.722112	70043.540133	33.554752
825.313658	70170.342174	33.559770
826.037136	70288.221423	33.564788
827.108248	70421.489346	33.569805
828.040298	70532.931014	33.574823
828.892968	70647.503315	33.579840
829.563310	70767.120022	33.584858
830.186785	70875.345758	33.589876
831.076714	70997.835840	33.594893
831.816952	71107.858039	33.599911
832.634655	71215.661446	33.604928
833.215114	71330.023165	33.609946
833.820381	71436.971289	33.614964
834.886312	71559.878141	33.619981
835.498812	71670.803201	33.624999
836.184178	71792.338987	33.630016
836.746360	71931.043147	33.635034
837.369479	72070.990065	33.640052
838.365575	72178.655091	33.645069
838.785449	72320.660517	33.650087
839.819572	72463.728880	33.655104
840.510563	72590.895695	33.660122
841.463182	72725.386364	33.665140
842.419657	72859.339784	33.670157
843.325365	72998.961585	33.675175
844.631151	73121.920039	33.680192
845.247705	73267.693150	33.685210
846.055672	73392.607015	33.690228
847.075702	73525.004920	33.695245
847.367199	73673.616687	33.700263
848.228956	73800.509553	33.705280
848.955489	73949.803869	33.710298
849.949632	74101.793068	33.715316
851.146642	74263.974869	33.720333
851.498384	74403.260950	33.725351
852.660111	74540.915506	33.730368
853.690891	74682.133767	33.735386
854.550868	74820.124490	33.740404
855.625804	74958.422077	33.745421
856.313354	75098.782803	33.750439
857.208392	75234.316783	33.755456
858.214235	75374.120837	33.760474
859.622981	75518.557866	33.765492
860.413649	75636.575642	33.770509
861.161359	75782.849992	33.775527
861.940272	75911.950680	33.780544
862.775407	76054.588806	33.785562
863.470262	76213.788347	33.790580
864.168903	76340.210794	33.795597
865.023197	76480.888089	33.800615
865.599918	76625.109374	33.805632
866.679936	76776.053332	33.810650
867.702312	76918.754732	33.815668
868.850917	77061.872594	33.820685
869.626213	77212.408208	33.825703
870.412414	77344.659348	33.830720
871.304295	77511.753897	33.835738
871.936113	77634.817630	33.840756
873.050798	77780.741188	33.845773
873.554564	77933.135379	33.850791
874.528336	78071.374544	33.855808
875.460511	78215.661440	33.860826
876.738718	78361.239294	33.865844
877.760999	78514.785199	33.870861
878.748450	78665.169234	33.875879
879.744133	78794.902559	33.880896
880.376833	78937.877477	33.885914
881.018186	79094.475617	33.890932
882.539807	79206.351687	33.895949
883.851533	79339.040342	33.900967
884.496537	79484.350653	33.905984
885.381422	79599.565901	33.911002
886.415353	79728.887259	33.916020
887.614370	79862.464186	33.921037
888.392540	79997.800208	33.926055
889.174680	80122.630328	33.931072
889.916930	80246.740338	33.936090
890.296974	80384.162176	33.941108
891.281879	80505.779379	33.946125
891.531024	80639.011780	33.951143
892.406065	80768.403362	33.956160
893.130320	80904.070051	33.961178
893.490520	81053.833751	33.966196
894.129612	81186.815266	33.971213
895.358708	81354.465040	33.976231
896.194575	81486.973061	33.981248
896.988942	81640.464311	33.986266
897.786102	81790.211384	33.991284
898.819682	81930.229512	33.996301
899.668674	82075.794996	34.001319
900.565485	82243.961723	34.006336
901.470089	82409.402002	34.011354
902.119249	82558.330962	34.016372
903.383270	82722.214969	34.021389
903.788360	82893.516796	34.026407
904.897352	83065.526074	34.031424
905.831543	83218.290141	34.036442
906.264892	83393.911756	34.041460
907.758105	83545.035838	34.046477
908.438617	83722.131121	34.051495
909.453219	83908.117879	34.056512
910.157687	84053.024059	34.061530
910.880860	84249.715128	34.066548
912.127346	84397.811033	34.071565
912.928376	84586.862586	34.076583
914.084771	84744.718269	34.081600
915.199312	84924.496904	34.086618
915.611421	85097.825982	34.091636
916.368284	85267.923502	34.096653
917.331027	85455.576332	34.101671
918.338471	85631.550579	34.106688
919.071787	85808.684940	34.111706
920.123245	85999.079689	34.116724
921.399683	86165.339955	34.121741
922.139687	86354.283277	34.126759
923.138592	86524.539930	34.131776
924.565551	86697.460417	34.136794
925.444521	86864.234231	34.141812
926.541931	87052.516856	34.146829
927.815281	87217.114854	34.151847
928.505684	87394.711360	34.156864
929.768930	87557.541835	34.161882
930.771044	87725.022810	34.166900
931.919362	87875.416123	34.171917
932.705362	88028.236654	34.176935
933.680194	88188.746416	34.181952
935.261349	88344.981073	34.186970
936.264610	88507.487801	34.191988
937.312605	88664.053067	34.197005
938.148795	88810.890938	34.202023
939.000512	88966.649071	34.207040
939.843182	89110.507455	34.212058
940.613137	89261.687188	34.217076
941.747871	89426.032591	34.222093
942.688573	89575.553603	34.227111
943.253122	89734.452189	34.232128
944.388885	89890.764367	34.237146
945.251958	90055.228625	34.242164
946.076203	90210.195892	34.247181
946.819254	90363.165289	34.252199
947.583002	90542.918735	34.257216
948.590697	90706.224606	34.262234
949.478337	90868.355413	34.267252
950.432137	91029.584138	34.272269
950.956718	91197.776223	34.277287
951.815745	91365.540914	34.282304
953.137610	91522.326749	34.287322
953.588576	91676.719751	34.292340
954.649813	91845.049301	34.297357
955.814921	92000.718735	34.302375
956.718066	92164.880912	34.307392
957.725133	92323.451660	34.312410
958.220525	92497.929273	34.317428
959.069283	92654.256407	34.322445
960.373695	92829.552152	34.327463
960.963139	93016.934738	34.332480
962.418604	93175.399124	34.337498
962.571842	93346.319372	34.342516
963.870783	93532.361058	34.347533
965.055328	93711.935992	34.352551
965.719189	93883.851654	34.357568
966.828138	94067.561831	34.362586
967.852532	94241.426792	34.367604
968.671988	94423.605222	34.372621
969.761435	94607.423985	34.377639
970.894848	94784.312808	34.382656
971.936640	94970.730810	34.387674
972.628254	95149.074994	34.392692
973.595112	95341.109578	34.397709
974.578997	95512.091521	34.402727
975.676812	95713.417857	34.407744
976.539735	95900.081375	34.412762
977.364281	96075.429229	34.417780
979.000356	96275.000347	34.422797
979.909650	96453.761193	34.427815
980.885946	96643.215660	34.432832
981.878394	96828.206509	34.437850
982.565585	97017.585001	34.442868
983.789112	97196.236075	34.447885
984.956697	97383.841698	34.452903
985.498698	97562.633266	34.457920
986.930228	97760.617119	34.462938
988.068404	97951.213295	34.467956
989.149590	98122.229002	34.472973
990.375725	98302.071357	34.477991
991.278005	98497.673438	34.483008
992.554318	98678.383791	34.488026
993.441147	98846.733611	34.493044
994.012225	99027.145138	34.498061
995.356690	99211.222121	34.503079
996.370846	99395.601879	34.508096
997.131325	99574.536452	34.513114
997.977871	99769.505694	34.518132
999.397836	99959.811190	34.523149
1000.351881	100148.238927	34.528167
1001.256739	100335.213840	34.533184
1002.496479	100513.392294	34.538202
1003.351294	100686.241850	34.543220
1004.231764	100877.985472	34.548237
1005.163604	101064.600502	34.553255
1005.877133	101248.954879	34.558272
1007.222120	101437.865844	34.563290
1008.108471	101643.067332	34.568308
1009.175046	101817.086207	34.573325
1010.280414	102009.136820	34.578343
1011.148965	102199.404649	34.583360
1012.473734	102370.662354	34.588378
1013.634454	102558.092631	34.593396
1014.686928	102739.559213	34.598413
1015.792843	102921.043589	34.603431
1016.721810	103107.066318	34.608448
1017.793440	103282.278322	34.613466
1018.786328	103444.253042	34.618484
1019.961613	103605.514887	34.623501
1021.216841	103778.218076	34.628519
1021.854575	103937.430735	34.633536
1023.009917	104115.768686	34.638554
1024.122909	104272.726925	34.643572
1025.407395	104435.780443	34.648589
1026.065689	104602.110512	34.653607
1026.901067	104776.586592	34.658624
1027.741145	104944.832678	34.663642
1028.594448	105122.290362	34.668660
1029.352671	105304.266862	34.673677
1030.033164	105479.893979	34.678695
1031.095935	105685.427956	34.683712
1031.813156	105867.364517	34.688730
1032.710011	106087.175900	34.693748
1033.781608	106256.310400	34.698765
1034.435634	106463.475675	34.703783
1035.497093	106674.463253	34.708800
1036.557448	106881.311473	34.713818
1037.178616	107105.381496	34.718836
1038.380455	107312.361734	34.723853
1039.280360	107539.910194	34.728871
1040.123752	107750.410509	34.733888
1041.136362	107980.882399	34.738906
1042.002065	108196.043262	34.743924
1043.282995	108423.979722	34.748941
1044.896443	108641.781757	34.753959
1046.010378	108863.290322	34.758976
1047.303794	109070.433875	34.763994
1048.433551	109290.537534	34.769012
1049.600389	109488.700074	34.774029
1051.499234	109699.168286	34.779047
1052.484437	109915.805243	34.784064
1053.472498	110103.856565	34.789082
1054.422827	110322.491118	34.794100
1055.296867	110520.203006	34.799117
1056.650902	110731.326590	34.804135
1057.098696	110940.764831	34.809152
1058.370889	111148.434642	34.814170
1059.439429	111370.098132	34.819188
1060.396515	111586.031214	34.824205
1061.488987	111789.137656	34.829223
1062.343218	112020.506537	34.834240
1063.277989	112234.561124	34.839258
1064.167004	112465.839392	34.844276
1065.010232	112699.964616	34.849293
1066.261407	112927.450224	34.854311
1066.841783	113151.868973	34.859328
1067.854714	113377.649575	34.864346
1069.318484	113623.511646	34.869364
1069.846630	113854.962594	34.874381
1071.661359	114095.070520	34.879399
1072.620568	114320.171023	34.884416
1074.013294	114543.719649	34.889434
1074.660846	114774.056502	34.894452
1076.305521	114999.556114	34.899469
1077.603849	115233.703827	34.904487
1078.696748	115461.679928	34.909504
1079.944148	115676.343167	34.914522
1080.835957	115904.799498	34.919540
1082.104493	116123.833360	34.924557
1083.499386	116337.083792	34.929575
1084.393711	116551.355985	34.934592
1085.481173	116779.571809	34.939610
1086.632569	116986.760950	34.944628
1087.953680	117192.960749	34.949645
1089.498691	117403.521331	34.954663
1090.425619	117613.742098	34.959680
1091.470366	117803.027741	34.964698
1092.720278	118008.586460	34.969716
1093.703778	118192.842358	34.974733
1095.087056	118392.591845	34.979751
1096.031506	118574.069337	34.984768
1096.984890	118771.396515	34.989786
1098.155670	118968.765196	34.994804
1098.920685	119166.227570	34.999821
1099.915422	119360.245126	35.004839
1100.806724	119575.237619	35.009856
1101.793247	119774.086699	35.014874
1103.070582	119980.428044	35.019892
1103.636893	120195.263448	35.024909
1104.973782	120404.676946	35.029927
1105.894771	120628.351796	35.034944
1107.113176	120830.312248	35.039962
1108.010922	121055.426048	35.044980
1108.815844	121287.918763	35.049997
1110.252195	121514.341034	35.055015
1111.158414	121742.081693	35.060032
1112.069911	121982.532560	35.065050
1113.052981	122202.407948	35.070068
1113.855006	122446.048561	35.075085
1115.176003	122668.672081	35.080103
1116.009891	122917.189924	35.085120
1117.426030	123162.851310	35.090138
1118.407513	123396.282095	35.095156
1119.609695	123648.508893	35.100173
1121.140200	123884.729472	35.105191
1122.031131	124124.288935	35.110208
1123.250100	124355.749276	35.115226
1124.903190	124624.751489	35.120244
1125.517567	124861.283175	35.125261
1126.796198	125104.930488	35.130279
1127.682897	125358.313791	35.135296
1128.962973	125601.610096	35.140314
1129.824769	125847.968245	35.145332
1130.855057	126114.146606	35.150349
1132.189700	126354.842056	35.155367
1133.077976	126628.842418	35.160384
1134.043505	126872.226310	35.165402
1135.325877	127131.667857	35.170420
1136.175715	127406.619472	35.175437
1137.544400	127663.263143	35.180455
1138.816217	127912.257323	35.185472
1139.737984	128176.583397	35.190490
1141.238027	128431.830423	35.195508
1143.193248	128674.951354	35.200525
1144.716628	128905.585352	35.205543
1145.716282	129168.500323	35.210560
1146.817961	129419.233248	35.215578
1147.863666	129657.543740	35.220596
1148.993087	129906.831165	35.225613
1150.344132	130151.635190	35.230631
1151.418918	130396.296635	35.235648
1152.451495	130651.816727	35.240666
1153.580426	130886.105003	35.245684
1154.447947	131145.496941	35.250701
1155.592693	131407.266249	35.255719
1156.599839	131649.426352	35.260736
1157.950916	131921.268163	35.265754
1158.816457	132164.849929	35.270772
1159.955590	132421.127457	35.275789
1161.308693	132671.616960	35.280807
1162.324405	132926.993650	35.285824
1163.607828	133188.691550	35.290842
1164.950854	133444.411348	35.295860
1165.913457	133700.208681	35.300877
1167.137025	133935.087185	35.305895
1168.368380	134179.410025	35.310912
1169.266940	134410.656864	35.315930
1170.711519	134656.405953	35.320948
1171.602833	134895.478928	35.325965
1172.902295	135136.945600	35.330983
1173.785542	135394.252778	35.336000
1174.863628	135631.538318	35.341018
1176.169526	135898.439582	35.346036
1177.021028	136144.171169	35.351053
1178.549251	136404.878826	35.356071
1179.605938	136658.960101	35.361088
1180.608921	136921.647529	35.366106
1182.072526	137182.169246	35.371124
1183.121327	137444.219441	35.376141
1184.281000	137698.570723	35.381159
1185.459305	137973.560428	35.386176
1186.429569	138216.283369	35.391194
1188.015158	138488.218155	35.396212
1188.886983	138766.523326	35.401229
1189.900822	139034.981749	35.406247
1191.234260	139296.239000	35.411264
1192.358187	139574.090951	35.416282
1193.824049	139835.077007	35.421300
1194.939904	140118.475358	35.426317
1196.355926	140391.962479	35.431335
1197.575860	140662.022867	35.436352
1198.573183	140939.881702	35.441370
1199.743725	141215.076988	35.446388
1200.594200	141500.394620	35.451405
1201.998867	141771.549169	35.456423
1203.231601	142057.518436	35.461440
1204.300482	142330.774260	35.466458
1205.653463	142615.992960	35.471476
1206.866229	142911.114679	35.476493
1208.383392	143190.110689	35.481511
1209.712251	143476.266164	35.486528
1210.712075	143747.617344	35.491546
1212.344713	144020.945746	35.496564
1213.244076	144312.910469	35.501581
1214.692407	144596.240495	35.506599
1216.167597	144876.702622	35.511616
1217.229541	145159.657200	35.516634
1218.296943	145430.414399	35.521652
1219.395160	145721.216848	35.526669
1220.654901	146014.645342	35.531687
1222.180038	146291.116095	35.536704
1223.139036	146575.798332	35.541722
1225.019622	146845.899603	35.546740
1226.255206	147123.680098	35.551757
1227.406964	147397.126903	35.556775
1228.664135	147680.944506	35.561792
1230.078119	147962.519214	35.566810
1231.229258	148235.947185	35.571828
1232.303546	148525.013823	35.576845
1233.528244	148799.537255	35.581863
1234.816136	149070.057539	35.586880
1235.803826	149353.197287	35.591898
1237.083510	149642.378474	35.596916
1238.196632	149918.311163	35.601933
1239.629041	150196.108273	35.606951
1241.062191	150477.369677	35.611968
1241.910208	150763.904289	35.616986
1243.149709	151051.708197	35.622004
1244.223869	151338.882146	35.627021
1245.090833	151617.556995	35.632039
1246.408424	151923.250267	35.637056
1247.538158	152212.704753	35.642074
1248.758775	152503.414803	35.647092
1249.647479	152775.283920	35.652109
1250.488078	153069.041651	35.657127
1251.995857	153361.017354	35.662144
1252.873752	153645.717493	35.667162
1254.320540	153943.795867	35.672180
1255.301563	154260.509729	35.677197
1256.381697	154563.321106	35.682215
1257.621820	154862.531626	35.687232
1258.431863	155185.953156	35.692250
1259.663308	155492.729721	35.697268
1261.001898	155811.858173	35.702285
1261.996315	156132.555514	35.707303
1263.546169	156451.489500	35.712320
1265.258009	156778.124264	35.717338
1266.469607	157097.626781	35.722356
1267.951370	157418.723661	35.727373
1269.335259	157727.294019	35.732391
1270.556839	158043.073280	35.737408
1272.214838	158372.317999	35.742426
1273.662329	158682.369514	35.747444
1274.799600	158994.669212	35.752461
1276.319717	159311.398797	35.757479
1277.695580	159619.160725	35.762496
1279.150001	159947.285064	35.767514
1280.146934	160248.949204	35.772532
1281.498501	160571.551999	35.777549
1283.011394	160881.292665	35.782567
1284.019460	161195.102417	35.787584
1285.297762	161530.195251	35.792602
1286.762557	161836.487864	35.797620
1287.809972	162169.645028	35.802637
1289.053321	162494.057037	35.807655
1291.311263	162809.093786	35.812672
1292.596562	163109.526340	35.817690
1293.880926	163413.868717	35.822708
1295.032253	163738.508688	35.827725
1296.609326	164038.506530	35.832743
1297.773090	164371.839863	35.837760
1298.813793	164681.319176	35.842778
1300.033704	165010.854901	35.847796
1301.376538	165332.341906	35.852813
1302.494303	165653.386384	35.857831
1303.981826	165969.842859	35.862848
1304.929478	166301.425485	35.867866
1306.227647	166632.673707	35.872884
1307.437955	166946.924781	35.877901
1308.716067	167293.749222	35.882919
1309.770747	167617.737044	35.887936
1311.207079	167957.105587	35.892954
1312.786118	168278.245815	35.897972
1314.145395	168615.957383	35.902989
1315.608215	168964.439511	35.908007
1317.282589	169283.630074	35.913024
1318.208897	169601.931334	35.918042
1319.646760	169943.662366	35.923060
1321.169032	170264.915283	35.928077
1322.681695	170596.386548	35.933095
1324.278181	170914.992634	35.938112
1325.491688	171255.831764	35.943130
1326.895858	171564.170771	35.948148
1328.429422	171879.000042	35.953165
1329.533821	172212.733110	35.958183
1331.039170	172517.470852	35.963200
1331.933309	172862.003892	35.968218
1332.950376	173184.299949	35.973236
1333.987288	173529.867656	35.978253
1335.100777	173856.885707	35.983271
1336.717194	174175.879275	35.988288
1337.531909	174511.351854	35.993306
1338.530318	174833.852793	35.998324
1339.811292	175167.717639	36.003341
1340.664375	175500.957513	36.008359
1342.305653	175837.153369	36.013376
1343.699590	176185.321299	36.018394
1344.779261	176533.937039	36.023412
1345.956013	176879.544344	36.028429
1347.014610	177231.683894	36.033447
1348.328766	177580.585789	36.038464
1349.664633	177940.959051	36.043482
1350.948357	178305.950363	36.048500
1352.674222	178670.109974	36.053517
1353.574063	179035.665024	36.058535
1355.225721	179401.492129	36.063552
1356.958157	179760.264976	36.068570
1358.267757	180126.090417	36.073588
1359.674976	180491.610522	36.078605
1360.991524	180855.815644	36.083623
1362.778322	181231.660126	36.088640
1363.897321	181605.409254	36.093658
1365.223157	181963.795324	36.098676
1366.657609	182339.249230	36.103693
1368.216809	182696.891167	36.108711
1369.850207	183052.962216	36.113728
1371.037561	183431.688627	36.118746
1372.761432	183788.384390	36.123764
1374.113951	184167.342722	36.128781
1375.649142	184536.297408	36.133799
1377.738638	184883.979429	36.138816
1378.376034	185265.348301	36.143834
1380.101360	185615.062548	36.148852
1381.547280	185984.130853	36.153869
1382.500210	186358.867893	36.158887
1384.336588	186719.931074	36.163904
1385.923700	187091.369896	36.168922
1387.029842	187457.851460	36.173940
1388.638770	187816.484270	36.178957
1389.840890	188189.720326	36.183975
1391.563116	188546.270167	36.188992
1393.045955	188923.006257	36.194010
1394.417233	189291.131704	36.199028
1396.018111	189639.660845	36.204045
1397.026250	190022.892893	36.209063
1398.548081	190398.350329	36.214080
1399.937833	190769.655753	36.219098
1401.609186	191131.764787	36.224116
1403.095984	191504.556810	36.229133
1404.455068	191859.816392	36.234151
1406.062002	192225.700321	36.239168
1407.112332	192586.956131	36.244186
1408.746571	192951.139036	36.249204
1410.022575	193315.167491	36.254221
1411.466555	193688.145434	36.259239
1412.847543	194052.224520	36.264256
1414.123061	194416.132790	36.269274
1415.506570	194778.629006	36.274292
1416.926346	195150.375881	36.279309
1418.080273	195521.115211	36.284327
1419.526526	195891.808527	36.289344
1421.166633	196278.163093	36.294362
1422.192093	196640.551611	36.299380
1423.559619	197033.976208	36.304397
1424.852244	197407.712613	36.309415
1426.217969	197793.347355	36.314432
1427.260369	198181.056348	36.319450
1428.491421	198569.510972	36.324468
1430.063018	198943.870466	36.329485
1431.177948	199327.029361	36.334503
1432.593489	199692.087630	36.339520
1434.024961	200082.295583	36.344538
1434.984917	200459.176851	36.349556
1436.737411	200847.838216	36.354573
1438.120223	201232.119250	36.359591
1439.758680	201627.088444	36.364608
1441.224496	202019.104836	36.369626
1442.408061	202418.952820	36.374644
1443.949337	202804.511579	36.379661
1445.127894	203206.701062	36.384679
1446.698345	203599.534418	36.389696
1448.418937	204013.268998	36.394714
1449.535760	204424.515536	36.399732
1451.070754	204819.786560	36.404749
1452.307333	205223.158715	36.409767
1453.732090	205638.145006	36.414784
1455.110270	206050.779735	36.419802
1456.789942	206479.390541	36.424820
1458.321013	206887.459232	36.429837
1459.548351	207315.895575	36.434855
1460.915109	207730.484180	36.439872
1462.521021	208159.002512	36.444890
1463.938678	208593.153816	36.449908
1465.715190	209011.198911	36.454925
1466.581805	209457.229141	36.459943
1468.182599	209929.983255	36.464960
1469.621541	210371.073790	36.469978
1471.296566	210807.086852	36.474996
1472.794789	211232.592370	36.480013
1474.384443	211671.785927	36.485031
1476.318997	212096.398612	36.490048
1477.665597	212532.894160	36.495066
1479.155957	212976.948966	36.500084
1480.693031	213407.436916	36.505101
1481.939646	213841.784418	36.510119
1483.554044	214279.628925	36.515136
1485.376961	214730.368046	36.520154
1486.592211	215159.470302	36.525172
1488.181767	215602.912823	36.530189
1489.509687	216044.876927	36.535207
1491.391336	216478.040685	36.540224
1492.597851	216929.553032	36.545242
1493.982382	217363.006223	36.550260
1495.703194	217797.879006	36.555277
1497.290233	218248.725491	36.560295
1498.894073	218692.358459	36.565312
1500.028173	219137.823452	36.570330
1501.560047	219574.386441	36.575348
1503.483011	220017.109349	36.580365
1505.151126	220455.736434	36.585383
1506.931026	220895.845506	36.590400
1508.626272	221328.325610	36.595418
1510.215706	221769.231880	36.600436
1511.761561	222199.657675	36.605453
1513.476856	222627.238062	36.610471
1515.356031	223031.350186	36.615488
1517.173572	223463.971441	36.620506
1518.931145	223884.793870	36.625524
1520.378307	224297.820881	36.630541
1521.533780	224730.861247	36.635559
1523.218429	225136.435696	36.640576
1524.640597	225552.163832	36.645594
1525.827952	225983.019455	36.650612
1527.177725	226396.654479	36.655629
1528.583441	226828.772608	36.660647
1530.019873	227251.387804	36.665664
1531.350517	227659.417127	36.670682
1532.822740	228066.840281	36.675700
1534.123491	228474.343895	36.680717
1535.441586	228905.721967	36.685735
1536.797537	229320.102649	36.690752
1538.234652	229737.671717	36.695770
1539.770796	230166.020902	36.700788
1541.317448	230597.519407	36.705805
1542.496953	231039.824277	36.710823
1543.870769	231472.268568	36.715840
1545.553160	231921.148286	36.720858
1546.850331	232370.423245	36.725876
1548.679440	232808.130756	36.730893
1549.838755	233265.534155	36.735911
1551.348560	233720.214085	36.740928
1553.044179	234175.677602	36.745946
1554.372751	234641.134885	36.750964
1556.125339	235086.355156	36.755981
1557.568243	235560.610570	36.760999
1559.523952	236017.078128	36.766016
1561.453967	236471.849347	36.771034
1562.912925	236926.826576	36.776052
1564.943200	237384.098530	36.781069
1566.536346	237853.280976	36.786087
1568.109971	238296.405874	36.791104
1569.801989	238757.445945	36.796122
1571.568429	239218.703544	36.801140
1573.174105	239667.694369	36.806157
1574.815604	240126.891918	36.811175
1576.411418	240580.966931	36.816192
1578.307401	241042.233046	36.821210
1579.898121	241480.790377	36.826228
1582.008345	241930.262049	36.831245
1583.376036	242377.698034	36.836263
1585.009212	242825.065759	36.841280
1586.676643	243278.169665	36.846298
1588.602518	243730.723809	36.851316
1590.234377	244163.615138	36.856333
1591.592602	244612.987774	36.861351
1593.249901	245064.191689	36.866368
1595.131821	245500.194081	36.871386
1596.224081	245956.522538	36.876404
1597.512561	246406.443372	36.881421
1599.120776	246863.551957	36.886439
1600.499480	247321.308832	36.891456
1602.191305	247779.395822	36.896474
1603.446346	248251.044453	36.901492
1605.124238	248703.368736	36.906509
1606.457011	249199.367258	36.911527
1608.076305	249658.688333	36.916544
1609.527467	250153.246182	36.921562
1610.761479	250638.365258	36.926580
1612.726410	251087.063542	36.931597
1614.448718	251594.559496	36.936615
1615.882348	252082.568794	36.941632
1617.792251	252561.329568	36.946650
1619.488274	253036.899953	36.951668
1621.368246	253522.296871	36.956685
1622.828728	253994.376026	36.961703
1624.252652	254474.692253	36.966720
1625.677309	254961.181736	36.971738
1627.362571	255456.316501	36.976756
1629.109354	255948.113671	36.981773
1630.347787	256432.475700	36.986791
1631.847124	256927.134102	36.991808
1634.054063	257407.831270	36.996826
1635.271248	257923.977114	37.001844
1636.849798	258397.665516	37.006861
1638.726880	258881.847207	37.011879
1640.358585	259341.275931	37.016896
1642.073141	259817.076235	37.021914
1643.521284	260277.195954	37.026932
1645.295546	260737.363554	37.031949
1646.696189	261229.016738	37.036967
1648.198017	261711.965324	37.041984
1649.871926	262193.488336	37.047002
1651.235294	262677.653692	37.052020
1653.308287	263147.984129	37.057037
1654.797503	263639.470137	37.062055
1656.575797	264128.520427	37.067072
1658.007033	264613.334680	37.072090
1659.423309	265125.358138	37.077108
1661.337813	265602.649127	37.082125
1662.688812	266112.117172	37.087143
1664.344478	266623.135074	37.092160
1666.179070	267136.307817	37.097178
1667.655119	267642.324856	37.102196
1669.321785	268143.026213	37.107213
1671.023311	268665.237897	37.112231
1672.360826	269173.232610	37.117248
1674.298247	269697.360464	37.122266
1675.714859	270234.808710	37.127284
1677.193640	270763.075594	37.132301
1679.121933	271287.025392	37.137319
1680.334022	271825.496203	37.142336
1682.371735	272362.788559	37.147354
1684.038408	272898.540994	37.152372
1685.561497	273440.743259	37.157389
1687.244194	273990.158156	37.162407
1688.945661	274535.936447	37.167424
1690.935953	275076.179158	37.172442
1692.183158	275640.853897	37.177460
1694.099680	276184.790167	37.182477
1696.292398	276739.806163	37.187495
1697.567727	277293.219599	37.192512
1699.830136	277837.171704	37.197530
1701.654870	278395.648836	37.202548
1703.394372	278940.650091	37.207565
1705.204571	279486.730727	37.212583
1706.641188	280047.579609	37.217600
1708.475663	280598.302169	37.222618
1709.849028	281146.355970	37.227636
1711.638649	281684.458264	37.232653
1713.494804	282261.387817	37.237671
1714.952415	282818.898173	37.242688
1716.747756	283393.065618	37.247706
1718.325974	283961.323121	37.252724
1720.109628	284517.885596	37.257741
1721.856217	285085.375147	37.262759
1723.540032	285662.271775	37.267776
1725.237684	286225.218779	37.272794
1727.055168	286795.713714	37.277812
1728.898372	287361.172956	37.282829
1730.858936	287938.904994	37.287847
1732.497929	288524.943288	37.292864
1734.321690	289083.744400	37.297882
1736.056505	289650.483167	37.302900
1737.684340	290204.867206	37.307917
1739.618599	290785.208844	37.312935
1741.161276	291360.380167	37.317952
1743.168091	291914.644134	37.322970
1744.477557	292508.696237	37.327988
1746.483691	293081.421543	37.333005
1748.054607	293657.035542	37.338023
1749.429008	294232.526969	37.343040
1751.461510	294794.394442	37.348058
1753.232583	295352.238519	37.353076
1754.787229	295910.420533	37.358093
1756.654269	296470.961359	37.363111
1758.154645	297034.836525	37.368128
1760.156402	297587.475933	37.373146
1761.406091	298155.425436	37.378164
1762.935325	298724.418102	37.383181
1764.747153	299299.456954	37.388199
1766.171320	299865.540147	37.393216
1768.274623	300453.478136	37.398234
1769.721991	301028.948796	37.403252
1771.700398	301615.300754	37.408269
1773.518605	302187.401984	37.413287
1775.079716	302780.089418	37.418304
1777.174327	303377.460114	37.423322
1778.585594	303978.241607	37.428340
1780.414387	304574.251930	37.433357
1782.041274	305177.606293	37.438375
1783.572984	305790.140895	37.443392
1785.299563	306391.134415	37.448410
1787.013363	307008.862667	37.453428
1788.764574	307639.050318	37.458445
1790.530426	308248.304313	37.463463
1792.264658	308893.393600	37.468480
1794.257150	309502.855398	37.473498
1796.091110	310146.928376	37.478516
1797.826368	310785.578011	37.483533
1799.799401	311417.225117	37.488551
1801.460269	312046.023783	37.493568
1803.367409	312688.541162	37.498586
1805.015804	313320.404765	37.503604
1806.469391	313975.531715	37.508621
1808.160304	314622.894062	37.513639
1809.738519	315284.972919	37.518656
1812.118438	315943.460167	37.523674
1813.957353	316608.607928	37.528692
1815.812155	317270.318968	37.533709
1817.723712	317933.284360	37.538727
1819.348531	318592.608979	37.543744
1821.444711	319252.814719	37.548762
1823.180037	319910.559956	37.553780
1824.982745	320589.312926	37.558797
1827.199764	321246.407466	37.563815
1828.761352	321918.229641	37.568832
1831.268499	322585.394835	37.573850
1833.043560	323259.377517	37.578868
1834.766665	323912.388728	37.583885
1836.716538	324577.340595	37.588903
1838.564039	325247.964677	37.593920
1840.446476	325920.937309	37.598938
1842.448372	326572.860007	37.603956
1844.215101	327244.288840	37.608973
1845.960934	327901.140203	37.613991
1847.524982	328581.804430	37.619008
1849.675927	329255.610749	37.624026
1851.281938	329940.289696	37.629044
1853.415803	330609.056671	37.634061
1855.483570	331272.140026	37.639079
1857.584827	331946.964991	37.644096
1859.178901	332615.239596	37.649114
1861.266647	333278.322145	37.654132
1862.769381	333942.585125	37.659149
1864.915164	334619.757640	37.664167
1866.656969	335287.443284	37.669184
1868.662913	335948.324597	37.674202
1870.429760	336629.520703	37.679220
1872.052857	337288.976592	37.684237
1873.825449	337958.960021	37.689255
1875.599071	338638.809620	37.694272
1877.608484	339285.687800	37.699290
1878.860466	339944.715109	37.704308
1880.595714	340601.395202	37.709325
1882.320223	341258.551016	37.714343
1883.562612	341939.384402	37.719360
1885.356487	342602.501933	37.724378
1886.991476	343297.086014	37.729396
1888.878496	343989.689822	37.734413
1890.842132	344688.159915	37.739431
1892.373261	345382.122747	37.744448
1894.144274	346097.610124	37.749466
1896.114433	346809.754559	37.754484
1897.775276	347525.822633	37.759501
1899.682952	348242.727504	37.764519
1901.355392	348972.730781	37.769536
1903.477327	349701.912514	37.774554
1905.611419	350429.938719	37.779572
1907.200178	351158.474775	37.784589
1909.305819	351897.065137	37.789607
1911.192530	352637.202198	37.794624
1913.435322	353388.104362	37.799642
1915.364491	354137.294580	37.804660
1917.022757	354889.435031	37.809677
1919.183928	355630.923239	37.814695
1921.158293	356385.548692	37.819712
1923.022938	357134.190518	37.824730
1925.164521	357884.346766	37.829748
1926.764123	358635.162736	37.834765
1929.377593	359394.628096	37.839783
1931.236292	360164.835476	37.844800
1933.283848	360915.206676	37.849818
1934.899135	361680.731944	37.854836
1936.519237	362449.743344	37.859853
1938.767012	363213.511602	37.864871
1940.910420	363992.352782	37.869888
1942.561984	364753.906589	37.874906
1945.010001	365521.783660	37.879924
1947.019285	366289.844916	37.884941
1949.027563	367057.459924	37.889959
1950.925105	367839.918403	37.894976
1952.979896	368605.693745	37.899994
1955.422309	369384.631468	37.905012
1957.246222	370162.741963	37.910029
1959.238116	370919.069795	37.915047
1961.079511	371691.311398	37.920064
1963.351827	372470.136858	37.925082
1965.912586	373227.921707	37.930100
1967.828343	374005.657293	37.935117
1970.286217	374752.470075	37.940135
1971.765627	375519.668447	37.945152
1973.876163	376255.829410	37.950170
1975.769998	377023.485053	37.955188
1977.599022	377778.403275	37.960205
1979.842680	378542.341407	37.965223
1981.351057	379314.017507	37.970240
1983.382265	380072.327041	37.975258
1985.708362	380842.312507	37.980276
1987.207371	381622.966202	37.985293
1989.260155	382373.714959	37.990311
1991.274213	383150.368692	37.995328
1993.188211	383920.554935	38.000346
1995.775555	384691.601203	38.005364
1997.204928	385471.416052	38.010381
1999.513308	386223.607903	38.015399
2001.023589	387005.249196	38.020416
2003.465293	387780.861317	38.025434
2005.563259	388538.510678	38.030452
2007.103276	389297.451091	38.035469
2009.236171	390047.630608	38.040487
2011.134253	390795.473410	38.045504
2012.894506	391539.797425	38.050522
2014.999301	392294.541937	38.055540
2016.869225	393057.697623	38.060557
2018.680873	393811.845214	38.065575
2020.708404	394574.329040	38.070592
2022.857466	395334.086965	38.075610
2024.797201	396080.274388	38.080628
2026.637724	396857.078325	38.085645
2028.553683	397625.637718	38.090663
2030.619701	398418.357242	38.095680
2032.201808	399204.038990	38.100698
2034.400504	399976.799549	38.105716
2036.208323	400779.205036	38.110733
2038.546069	401583.097669	38.115751
2040.583712	402383.165613	38.120768
2042.246401	403192.928164	38.125786
2044.440448	404006.001196	38.130804
2046.558807	404807.331337	38.135821
2048.830756	405603.089661	38.140839
2050.921142	406419.987508	38.145856
2052.904845	407243.466901	38.150874
2054.964522	408060.904688	38.155892
2057.249961	408883.931072	38.160909
2059.413248	409699.453857	38.165927
2061.413206	410535.804199	38.170944
2063.483656	411359.703825	38.175962
2065.807413	412181.206041	38.180980
2067.564210	413024.688969	38.185997
2069.451593	413858.649967	38.191015
2071.506127	414679.942771	38.196032
2073.866008	415521.600845	38.201050
2075.928570	416355.353180	38.206068
2077.893260	417209.003012	38.211085
2079.850121	418043.909414	38.216103
2082.149279	418902.995197	38.221120
2083.869066	419740.165369	38.226138
2086.403455	420597.661608	38.231156
2088.784067	421444.746304	38.236173
2091.120562	422288.366095	38.241191
2093.447683	423130.237352	38.246208
2095.534587	423985.540322	38.251226
2097.999234	424808.949234	38.256244
2099.945400	425669.053871	38.261261
2102.654449	426500.899004	38.266279
2104.864478	427334.925011	38.271296
2107.028051	428156.879363	38.276314
2109.467769	428968.887130	38.281332
2111.569620	429805.681801	38.286349
2113.536946	430639.887552	38.291367
2115.575347	431471.470603	38.296384
2117.834382	432304.253942	38.301402
2120.090497	433114.987312	38.306420
2121.969965	433962.455824	38.311437
2123.734335	434795.030518	38.316455
2125.901106	435626.243794	38.321472
2127.626694	436460.385304	38.326490
2129.727510	437311.694487	38.331508
2131.644901	438165.381300	38.336525
2133.463573	438996.986351	38.341543
2135.820444	439856.661556	38.346560
2137.730234	440723.311135	38.351578
2139.986439	441570.235635	38.356596
2141.925990	442425.074586	38.361613
2144.233714	443292.622314	38.366631
2146.505724	444130.187425	38.371648
2148.116618	444972.687294	38.376666
2150.152818	445806.888442	38.381684
2151.964442	446650.910113	38.386701
2154.186034	447500.346107	38.391719
2156.067848	448352.385075	38.396736
2157.863584	449207.187072	38.401754
2160.548742	450057.053504	38.406772
2162.043366	450931.969718	38.411789
2164.441554	451791.071476	38.416807
2165.916000	452661.519501	38.421824
2168.351295	453538.651830	38.426842
2170.628189	454426.647443	38.431860
2172.710912	455309.276760	38.436877
2174.607501	456203.328487	38.441895
2176.854143	457089.749312	38.446912
2179.502507	458005.697871	38.451930
2181.701773	458891.189521	38.456948
2183.734750	459797.198530	38.461965
2185.877451	460699.711154	38.466983
2188.193787	461610.042011	38.472000
2190.149551	462531.058480	38.477018
2192.342225	463442.540334	38.482036
2194.764904	464363.547388	38.487053
2196.748613	465302.781626	38.492071
2198.802192	466224.117212	38.497088
2201.367650	467164.077026	38.502106
2203.859323	468086.061989	38.507124
2206.041831	469021.750455	38.512141
2208.350535	469943.425163	38.517159
2210.647678	470874.103511	38.522176
2212.760113	471815.277952	38.527194
2214.620397	472753.517189	38.532212
2216.862574	473710.342173	38.537229
2219.287923	474649.102381	38.542247
2221.835661	475597.293900	38.547264
2224.089408	476561.248069	38.552282
2226.214603	477505.321103	38.557300
2228.492070	478454.675785	38.562317
2230.636181	479414.257750	38.567335
2233.104459	480369.039273	38.572352
2235.042123	481333.050893	38.577370
2237.297963	482285.798246	38.582388
2239.633204	483249.643433	38.587405
2242.221895	484219.354497	38.592423
2244.968223	485157.276740	38.597440
2246.659435	486117.490356	38.602458
2249.448769	487080.450451	38.607476
2251.384738	488066.723368	38.612493
2253.572507	489036.593732	38.617511
2256.107069	490008.272114	38.622528
2258.161393	490984.973532	38.627546
2260.385561	491942.159445	38.632564
2262.784068	492917.737347	38.637581
2265.037060	493878.193986	38.642599
2267.618370	494849.545172	38.647616
2269.805057	495817.626565	38.652634
2272.154363	496777.653669	38.657652
2274.521094	497752.004828	38.662669
2276.746091	498713.911479	38.667687
2279.049796	499670.503508	38.672704
2281.270957	500648.395459	38.677722
2283.855041	501608.615086	38.682740
2285.794403	502595.016198	38.687757
2287.963067	503555.444760	38.692775
2290.338108	504530.158773	38.697792
2292.251947	505508.421914	38.702810
2294.354564	506491.992152	38.707828
2296.324185	507468.465259	38.712845
2298.472255	508422.814238	38.717863
2300.880151	509389.872021	38.722880
2302.800945	510359.977674	38.727898
2305.264688	511314.003607	38.732916
2307.091767	512287.689170	38.737933
2309.195348	513248.667121	38.742951
2311.545350	514224.870724	38.747968
2313.674494	515220.960845	38.752986
2316.469255	516193.895207	38.758004
2319.092309	517183.227887	38.763021
2320.622347	518173.232799	38.768039
2323.000834	519166.411469	38.773056
2325.369963	520167.036366	38.778074
2327.522733	521186.375994	38.783092
2330.129360	522191.567169	38.788109
2332.205864	523201.011958	38.793127
2335.128169	524204.155317	38.798144
2337.299799	525233.600706	38.803162
2339.779713	526253.002827	38.808180
2342.308332	527271.774270	38.813197
2344.780414	528282.780760	38.818215
2347.222429	529303.443479	38.823232
2349.574286	530334.374351	38.828250
2351.707548	531357.213614	38.833268
2354.304258	532399.290229	38.838285
2357.185948	533415.167651	38.843303
2359.564716	534445.656987	38.848320
2361.831254	535480.622870	38.853338
2364.636622	536497.004179	38.858356
2366.718413	537536.334410	38.863373
2368.860336	538574.573686	38.868391
2371.385939	539597.225682	38.873408
2373.534387	540647.593562	38.878426
2375.895942	541696.239199	38.883444
2378.523411	542740.487378	38.888461
2380.890367	543782.236668	38.893479
2383.486039	544828.952466	38.898496
2385.737885	545885.103983	38.903514
2388.361718	546919.788546	38.908532
2391.090472	547973.742555	38.913549
2392.653505	549031.077961	38.918567
2395.454557	550092.202009	38.923584
2397.788985	551153.925006	38.928602
2400.148772	552205.506330	38.933620
2402.885988	553273.636137	38.938637
2405.315669	554324.691430	38.943655
2407.899978	555379.862602	38.948672
2410.004613	556443.826886	38.953690
2412.677430	557511.131952	38.958708
2415.367698	558568.298581	38.963725
2417.373281	559628.359149	38.968743
2419.840005	560697.354414	38.973760
2422.298369	561753.151844	38.978778
2424.786197	562821.621176	38.983796
2427.285188	563903.415086	38.988813
2429.773282	564954.129514	38.993831
2432.225257	566021.541576	38.998848
2434.844268	567107.069831	39.003866
2436.709226	568170.083839	39.008884
2439.446428	569247.931352	39.013901
2441.842007	570327.151244	39.018919
2443.941516	571414.111492	39.023936
2446.701840	572480.689684	39.028954
2449.084147	573567.922651	39.033972
2451.459157	574643.419243	39.038989
2453.593345	575723.030140	39.044007
2456.398924	576813.980723	39.049024
2458.817922	577885.982624	39.054042
2460.936090	578945.800009	39.059060
2463.618097	579989.881416	39.064077
2465.743229	581041.392048	39.069095
2468.061120	582100.958601	39.074112
2470.891233	583152.976678	39.079130
2473.072491	584201.400893	39.084148
2475.714827	585263.501308	39.089165
2477.696728	586337.402921	39.094183
2479.911441	587395.026095	39.099200
2482.092426	588496.032044	39.104218
2484.519071	589580.454019	39.109236
2487.270281	590662.419292	39.114253
2489.210967	591769.883835	39.119271
2491.578891	592866.450288	39.124288
2494.049288	593975.077119	39.129306
2496.010104	595087.593380	39.134324
2498.777976	596220.315228	39.139341
2500.718881	597367.994790	39.144359
2503.667598	598495.208110	39.149376
2506.112301	599653.702848	39.154394
2508.001699	600803.860276	39.159412
2510.790398	601953.155071	39.164429
2513.172109	603127.340851	39.169447
2515.864158	604299.303499	39.174464
2518.313471	605473.440014	39.179482
2520.819686	606660.412753	39.184500
2523.091561	607846.550252	39.189517
2524.928941	609047.751041	39.194535
2527.871038	610241.236242	39.199552
2530.901166	611465.655332	39.204570
2533.248662	612679.346881	39.209588
2535.998997	613875.831411	39.214605
2538.407403	615096.055304	39.219623
2541.106369	616308.245149	39.224640
2543.414743	617532.370021	39.229658
2546.188269	618748.281930	39.234676
2548.502623	619988.335874	39.239693
2551.182085	621218.590731	39.244711
2553.822974	622468.759495	39.249728
2556.253867	623712.621688	39.254746
2558.815419	624953.671214	39.259764
2561.491588	626198.857265	39.264781
2563.809195	627444.208584	39.269799
2567.018745	628692.915773	39.274816
2569.323578	629948.220545	39.279834
2572.299160	631188.082686	39.284852
2575.038646	632443.471344	39.289869
2577.349889	633699.381099	39.294887
2580.158888	634947.020506	39.299904
2582.770224	636207.275429	39.304922
2585.164899	637471.258302	39.309940
2587.845022	638723.561133	39.314957
2590.339863	639991.614226	39.319975
2592.709022	641245.810186	39.324992
2595.503837	642530.768410	39.330010
2597.944971	643795.070418	39.335028
2600.564014	645071.059261	39.340045
2602.647960	646346.528085	39.345063
2605.581004	647634.114791	39.350080
2607.991767	648916.687660	39.355098
2610.417604	650200.690744	39.360116
2613.336422	651486.592470	39.365133
2616.149089	652783.910809	39.370151
2618.948784	654052.605493	39.375168
2621.649436	655329.078183	39.380186
2624.156633	656612.842602	39.385204
2627.146817	657878.974092	39.390221
2629.653104	659171.771934	39.395239
2632.075513	660421.580496	39.400256
2634.829249	661665.995746	39.405274
2637.245221	662904.780895	39.410292
2639.934341	664150.184008	39.415309
2642.409125	665396.159316	39.420327
2644.697024	666645.588414	39.425344
2647.224484	667897.652599	39.430362
2649.518976	669162.579373	39.435380
2652.017527	670426.459332	39.440397
2654.509067	671717.285264	39.445415
2657.055876	672988.278955	39.450432
2659.929885	674272.078354	39.455450
2662.522124	675555.301858	39.460468
2665.550472	676856.376535	39.465485
2667.955611	678156.925737	39.470503
2670.541674	679447.024324	39.475520
2673.475720	680761.040681	39.480538
2675.805302	682079.045164	39.485556
2678.761473	683394.174675	39.490573
2681.066887	684725.418675	39.495591
2684.057187	686034.849007	39.500608
2686.760081	687376.867697	39.505626
2689.219381	688716.097033	39.510644
2692.397650	690042.200797	39.515661
2694.900942	691397.808002	39.520679
2697.695681	692723.382655	39.525696
2700.299200	694077.576983	39.530714
2703.414886	695408.309716	39.535732
2706.026878	696771.472562	39.540749
2708.647653	698130.357409	39.545767
2711.062203	699496.705763	39.550784
2714.024395	700848.272399	39.555802
2716.715499	702225.656825	39.560820
2719.602779	703577.708259	39.565837
2722.174299	704969.304908	39.570855
2724.720751	706340.810552	39.575872
2727.393583	707710.691215	39.580890
2730.579174	709121.836342	39.585908
2733.108797	710500.611782	39.590925
2735.406306	711904.412953	39.595943
2738.631840	713298.273961	39.600960
2741.378259	714682.282151	39.605978
2743.866101	716092.244545	39.610996
2746.616977	717484.160702	39.616013
2748.918103	718895.765071	39.621031
2752.154232	720307.621669	39.626048
2755.188406	721728.870624	39.631066
2757.373600	723151.303621	39.636084
2760.470044	724562.760728	39.641101
2762.789379	725995.662984	39.646119
2765.793186	727412.978202	39.651136
2768.506811	728845.419485	39.656154
2771.304894	730285.701364	39.661172
2773.793608	731710.019265	39.666189
2776.935025	733156.408412	39.671207
2779.209296	734604.016505	39.676224
2782.361225	736047.221177	39.681242
2784.966787	737491.393304	39.686260
2787.711754	738938.343675	39.691277
2790.537853	740389.905592	39.696295
2793.506180	741821.786917	39.701312
2797.075441	743271.763908	39.706330
2799.778505	744716.981586	39.711348
2803.101678	746139.885473	39.716365
2805.992720	747583.363396	39.721383
2809.101066	749020.229443	39.726400
2811.871723	750438.254548	39.731418
2814.638821	751857.550163	39.736436
2817.190790	753241.341146	39.741453
2819.662370	754636.475762	39.746471
2822.283560	756031.974001	39.751488
2825.271692	757400.958580	39.756506
2827.776213	758795.235444	39.761524
2830.390395	760176.932385	39.766541
2833.369718	761595.677896	39.771559
2836.178890	762980.328399	39.776576
2838.540606	764394.616733	39.781594
2841.163261	765792.805821	39.786612
2843.869756	767224.708064	39.791629
2846.982258	768649.041252	39.796647
2849.305727	770090.097013	39.801664
2852.163858	771540.371498	39.806682
2854.641952	772986.690254	39.811700
2857.160657	774442.792861	39.816717
2860.251824	775916.592636	39.821735
2862.990013	777386.078439	39.826752
2865.858291	778876.806374	39.831770
2868.467377	780377.534141	39.836788
2871.250943	781868.351804	39.841805
2874.072786	783364.059027	39.846823
2876.851354	784879.581446	39.851840
2880.480904	786382.577048	39.856858
2882.676981	787920.513285	39.861876
2885.320346	789428.476985	39.866893
2887.722397	790973.616985	39.871911
2890.766271	792522.628740	39.876928
2893.563531	794091.482964	39.881946
2896.621309	795655.781335	39.886964
2899.462122	797217.759461	39.891981
2902.347295	798783.887696	39.896999
2905.112146	800372.695870	39.902016
2908.273144	801952.216652	39.907034
2910.926648	803543.059720	39.912052
2913.520299	805139.124328	39.917069
2916.533257	806745.169079	39.922087
2919.497006	808337.398033	39.927104
2922.748608	809946.859083	39.932122
2925.530017	811559.537191	39.937140
2928.672737	813167.961418	39.942157
2931.917965	814783.901626	39.947175
2934.486314	816414.855007	39.952192
2937.070632	818029.197716	39.957210
2940.305052	819671.653884	39.962228
2943.542506	821295.011704	39.967245
2946.223032	822931.191891	39.972263
2949.125821	824552.247503	39.977280
2951.999403	826208.563717	39.982298
2954.958296	827862.011379	39.987316
2957.636134	829498.806813	39.992333
2960.688875	831163.593029	39.997351
2963.649590	832809.113072	40.002368
2966.972348	834460.489145	40.007386
2969.782057	836138.799936	40.012404
2972.689905	837787.007916	40.017421
2975.856639	839465.901935	40.022439
2978.370874	841138.186171	40.027456
2981.839476	842783.118506	40.032474
2984.354907	844463.578426	40.037492
2987.694174	846127.995153	40.042509
2990.937637	847808.808158	40.047527
2993.709606	849470.394468	40.052544
2997.086296	851145.919148	40.057562
2999.992917	852804.266643	40.062580
3003.031699	854473.125124	40.067597
3005.919324	856142.919236	40.072615
3008.797588	857795.763460	40.077632
3011.916226	859438.421299	40.082650
3015.117663	861062.873215	40.087668
3018.116801	862679.459687	40.092685
3021.147162	864303.563786	40.097703
3024.484533	865917.490329	40.102720
3027.798796	867519.362060	40.107738
3030.193205	869134.815250	40.112756
3033.416735	870760.449978	40.117773
3036.914255	872369.331865	40.122791
3039.551870	873983.924915	40.127808
3042.966365	875613.050612	40.132826
3045.587922	877239.828853	40.137844
3048.700020	878868.884907	40.142861
3052.026108	880497.553226	40.147879
3054.837660	882134.459687	40.152896
3057.791591	883782.097035	40.157914
3060.737453	885439.803009	40.162932
3063.773625	887067.949183	40.167949
3066.967207	888748.240113	40.172967
3069.592617	890407.864961	40.177984
3072.736432	892067.409899	40.183002
3075.820548	893757.938167	40.188020
3078.949887	895430.888974	40.193037
3081.839389	897124.698915	40.198055
3084.671148	898818.496756	40.203072
3087.610186	900526.419017	40.208090
3090.396967	902245.603746	40.213108
3093.391359	903957.199938	40.218125
3096.545324	905679.609201	40.223143
3099.230801	907419.082823	40.228160
3102.681225	909158.754404	40.233178
3105.490943	910913.184861	40.238196
3108.341323	912665.418866	40.243213
3111.836510	914426.315076	40.248231
3114.625655	916193.394920	40.253248
3117.631708	917978.602197	40.258266
3120.715284	919755.627505	40.263284
3123.484323	921535.293174	40.268301
3127.159763	923348.006997	40.273319
3129.932332	925143.761461	40.278336
3132.951872	926948.947195	40.283354
3135.707349	928755.199903	40.288372
3138.725609	930584.088917	40.293389
3142.081416	932402.523421	40.298407
3145.078190	934233.611881	40.303424
3148.349154	936064.884142	40.308442
3151.684973	937904.602720	40.313460
3154.669596	939749.954644	40.318477
3157.900236	941589.643414	40.323495
3161.355549	943432.567232	40.328512
3164.488126	945266.003762	40.333530
3167.803778	947126.276949	40.338548
3171.117229	948971.460244	40.343565
3174.371953	950807.018297	40.348583
3177.518748	952670.663539	40.353600
3180.913951	954503.251952	40.358618
3184.351481	956377.150018	40.363636
3187.717644	958258.294161	40.368653
3190.954100	960142.171582	40.373671
3194.056586	962049.895101	40.378688
3197.540787	963923.795644	40.383706
3200.499358	965810.263847	40.388724
3204.295477	967692.069153	40.393741
3207.529528	969561.440247	40.398759
3210.985429	971449.197862	40.403776
3214.031973	973328.791848	40.408794
3217.447666	975203.124843	40.413812
3220.538444	977060.322868	40.418829
3224.190565	978877.350371	40.423847
3226.450873	980694.809336	40.428864
3230.146590	982510.966849	40.433882
3233.344890	984321.564905	40.438900
3236.396001	986133.267453	40.443917
3239.655907	987945.040998	40.448935
3242.369186	989776.174318	40.453952
3245.360904	991604.241249	40.458970
3248.861129	993438.733880	40.463988
3251.603154	995291.905482	40.469005
3254.905337	997148.266154	40.474023
3257.633927	999005.084920	40.479040
3261.102122	1000864.571745	40.484058
3263.895631	1002751.124715	40.489076
3267.068824	1004638.150343	40.494093
3270.653591	1006533.789869	40.499111
3273.607571	1008435.587439	40.504128
3276.841869	1010353.757778	40.509146
3279.792454	1012262.601186	40.514164
3282.736684	1014193.271548	40.519181
3286.349422	1016130.819098	40.524199
3289.323982	1018075.838223	40.529216
3292.606287	1020035.518762	40.534234
3296.153464	1021999.501288	40.539252
3298.840414	1023959.262941	40.544269
3302.129637	1025944.145492	40.549287
3305.065858	1027933.600082	40.554304
3308.151808	1029911.310326	40.559322
3311.904411	1031930.214058	40.564340
3315.185832	1033921.341429	40.569357
3318.792580	1035930.616188	40.574375
3322.039563	1037960.541933	40.579392
3325.514583	1039977.251410	40.584410
3328.863664	1042002.888499	40.589428
3332.292333	1044035.674340	40.594445
3335.729466	1046069.832940	40.599463
3339.078076	1048102.874520	40.604480
3342.180899	1050147.914359	40.609498
3345.511269	1052195.528088	40.614516
3348.752527	1054234.415630	40.619533
3352.367759	1056283.448319	40.624551
3355.264592	1058350.770050	40.629568
3359.067812	1060404.774712	40.634586
3362.180130	1062482.037968	40.639604
3365.816632	1064549.791103	40.644621
3368.954000	1066617.807870	40.649639
3372.152943	1068705.274542	40.654656
3375.587412	1070777.429480	40.659674
3378.953064	1072849.578777	40.664692
3382.623608	1074938.426701	40.669709
3386.176933	1077022.281837	40.674727
3389.135067	1079109.843924	40.679744
3392.803998	1081192.853748	40.684762
3396.481822	1083288.363465	40.689780
3399.392930	1085373.534757	40.694797
3403.237310	1087461.863617	40.699815
3406.718744	1089559.387400	40.704832
3410.752709	1091638.339224	40.709850
3414.534301	1093732.289993	40.714868
3417.472888	1095801.423169	40.719885
3421.083901	1097885.492357	40.724903
3424.575597	1099972.592832	40.729920
3428.214443	1102044.562739	40.734938
3431.435805	1104126.955670	40.739956
3434.517855	1106216.188088	40.744973
3438.467057	1108284.375271	40.749991
3441.443539	1110360.494447	40.755008
3445.200648	1112417.961523	40.760013
3448.497107	1114419.258032	40.765018
3451.650987	1116377.126894	40.770023
3455.009139	1118259.063976	40.775028
3457.804878	1120067.751359	40.780032
3460.820057	1121805.990642	40.785037
3463.579826	1123470.024939	40.790042
3466.585200	1125065.550594	40.795047
3469.561636	1126568.507791	40.800052
3471.991302	1128007.784649	40.805056
3474.601137	1129359.159468	40.810061
3477.600060	1130650.234349	40.815066
3479.120150	1131864.442142	40.820071
3481.791629	1132996.270768	40.825076
3484.075765	1134071.297984	40.830080
3486.426596	1135078.084631	40.835085
3488.129225	1135989.719825	40.840090
3490.068312	1136867.639611	40.845095
3491.934055	1137675.643540	40.850100
3493.598214	1138427.264623	40.855104
3495.524073	1139110.206176	40.860109
3496.835903	1139744.379383	40.865114
3498.244881	1140328.640779	40.870119
3499.845735	1140863.560560	40.875124
3501.325608	1141355.846572	40.880128
3502.710858	1141778.658363	40.885133
3503.870036	1142180.509067	40.890138
3504.920645	1142529.417727	40.895143
3506.187206	1142832.455168	40.900148
3507.076346	1143108.696146	40.905152
3508.181870	1143348.562948	40.910157
3509.256323	1143552.006436	40.915162
3510.103938	1143722.856441	40.920167
3511.119331	1143856.309528	40.925172
3511.768996	1143957.672066	40.930176
3512.549884	1144027.243379	40.935181
3513.493473	1144092.330065	40.940186
3513.915519	1144115.114089	40.945191
3514.603252	1144095.276696	40.950196
3515.067220	1144095.484807	40.955200
3515.751733	1144031.078400	40.960205
3516.427394	1143972.552138	40.965210
3516.968062	1143893.563893	40.970215
3517.731032	1143771.862865	40.975220
3518.254866	1143658.449142	40.980224
3518.494793	1143513.403837	40.985229
3519.252964	1143348.542256	40.990234
3519.517919	1143174.746562	40.995239
3519.752527	1142979.135186	41.000244
3519.775925	1142794.364415	41.005248
3520.792867	1142569.205091	41.010253
3520.816460	1142339.267110	41.015258
3521.195218	1142109.640103	41.020263
3521.550153	1141833.901207	41.025268
3521.688867	1141583.799313	41.030272
3522.152137	1141303.745694	41.035277
3522.517283	1141028.911992	41.040282
3522.622780	1140739.399170	41.045287
3523.198308	1140422.558692	41.050292
3523.409802	1140124.739072	41.055296
3523.390330	1139793.344498	41.060301
3523.498083	1139465.040306	41.065306
3523.440653	1139140.065069	41.070311
3523.928182	1138794.761631	41.075316
3524.017801	1138458.234709	41.080320
3524.030592	1138095.971665	41.085325
3523.915188	1137748.136130	41.090330
3523.991458	1137400.720957	41.095335
3524.660891	1137037.233049	41.100340
3524.518993	1136667.966302	41.105344
3524.641578	1136300.814554	41.110349
3525.034341	1135924.855300	41.115354
3524.761667	1135543.470127	41.120359
3524.989377	1135156.560838	41.125364
3525.257759	1134765.341901	41.130368
3525.206766	1134361.511485	41.135373
3525.347166	1133974.245471	41.140378
3525.005215	1133581.234698	41.145383
3525.471606	1133171.337635	41.150388
3525.582695	1132777.717730	41.155392
3525.734772	1132355.075423	41.160397
3525.880385	1131932.400599	41.165402
3525.589537	1131522.881390	41.170407
3526.018696	1131115.683643	41.175412
3526.172261	1130685.874039	41.180416
3525.978696	1130270.443285	41.185421
3526.023770	1129841.914467	41.190426
3525.862204	1129403.876131	41.195431
3525.931194	1128978.411888	41.200436
3525.819563	1128559.695929	41.205440
3525.925254	1128119.891200	41.210445
3526.174699	1127691.536193	41.215450
3525.953979	1127248.479198	41.220455
3525.956817	1126816.479592	41.225460
3526.036849	1126382.148808	41.230464
3526.074314	1125953.689116	41.235469
3526.367475	1125505.930564	41.240474
3526.417379	1125065.502464	41.245479
3526.351759	1124620.964479	41.250484
3526.214056	1124178.876131	41.255488
3526.158567	1123746.827961	41.260493
3526.271968	1123276.351556	41.265498
3526.388012	1122836.585509	41.270503
3526.264406	1122377.398704	41.275508
3526.421449	1121929.553116	41.280512
3526.642044	1121467.946123	41.285517
3526.479794	1121008.362384	41.290522
3526.228640	1120561.326589	41.295527
3526.782330	1120103.642670	41.300532
3526.523790	1119658.628303	41.305536
3526.453658	1119195.063023	41.310541
3526.475557	1118723.057709	41.315546
3526.259713	1118280.494310	41.320551
3526.278873	1117807.074658	41.325556
3526.137749	1117357.084739	41.330560
3526.401810	1116892.502635	41.335565
3526.360451	1116432.506010	41.340570
3526.605427	1115969.658178	41.345575
3526.585005	1115498.901018	41.350580
3526.323623	1115049.690549	41.355584
3526.280457	1114569.511594	41.360589
3526.685877	1114116.394308	41.365594
3526.235951	1113644.686876	41.370599
3526.380352	1113164.255907	41.375604
3526.196205	1112705.775359	41.380608
3526.032214	1112235.423195	41.385613
3526.250985	1111770.691082	41.390618
3526.047994	1111311.617591	41.395623
3526.175275	1110840.427423	41.400628
3526.259834	1110381.895101	41.405632
3525.996320	1109914.314426	41.410637
3526.369940	1109437.329887	41.415642
3525.990980	1108977.322431	41.420647
3526.116799	1108519.483592	41.425652
3525.887459	1108046.961811	41.430656
3525.918161	1107581.612119	41.435661
3526.239049	1107120.662309	41.440666
3525.805624	1106649.197276	41.445671
3525.992947	1106183.318957	41.450676
3525.801225	1105725.199249	41.455680
3525.993609	1105258.858110	41.460685
3525.875149	1104780.777800	41.465690
3525.805289	1104327.964367	41.470695
3525.637607	1103858.313113	41.475700
3525.694103	1103400.719292	41.480704
3525.593426	1102921.897901	41.485709
3525.464753	1102457.660826	41.490714
3525.449144	1102010.091324	41.495719
3525.563269	1101537.228661	41.500724
3525.481806	1101079.078330	41.505728
3525.326764	1100608.950934	41.510733
3525.442603	1100160.346019	41.515738
3525.503304	1099681.975518	41.520743
3525.513685	1099217.628170	41.525748
3525.154736	1098755.501368	41.530752
3525.400439	1098293.522400	41.535757
3525.497095	1097836.980659	41.540762
3525.168546	1097381.522666	41.545767
3525.294306	1096893.328706	41.550772
3525.321733	1096446.056465	41.555776
3524.884782	1095973.754444	41.560781
3524.926162	1095515.494956	41.565786
3525.287763	1095054.751427	41.570791
3525.256282	1094580.155633	41.575796
3525.488923	1094127.489752	41.580800
3525.338886	1093655.033935	41.585805
3525.135952	1093196.905697	41.590810
3525.136692	1092714.099517	41.595815
3524.961504	1092252.248670	41.600820
3525.265116	1091801.100322	41.605824
3525.001217	1091332.195378	41.610829
3524.966205	1090864.265725	41.615834
3524.182344	1090404.464821	41.620839
3524.628060	1089943.656114	41.625844
3524.746144	1089491.005187	41.630848
3524.897355	1089032.371038	41.635853
3524.866165	1088579.285482	41.640858
3524.666285	1088117.853303	41.645863
3525.110920	1087641.326071	41.650868
3524.703441	1087185.311298	41.655872
3524.571994	1086714.835622	41.660877
3524.488448	1086245.461620	41.665882
3524.549097	1085811.397252	41.670887
3524.725466	1085350.339218	41.675892
3524.365824	1084884.728149	41.680896
3524.405590	1084432.531705	41.685901
3524.634191	1083961.758606	41.690906
3524.352098	1083513.566490	41.695911
3524.200838	1083064.932283	41.700916
3524.210665	1082595.228031	41.705920
3524.093179	1082148.143404	41.710925
3524.511783	1081684.528673	41.715930
3524.069879	1081224.374303	41.720935
3523.889326	1080760.203973	41.725940
3524.490774	1080326.380852	41.730944
3524.322804	1079854.934361	41.735949
3524.289915	1079406.075415	41.740954
3524.079210	1078937.819914	41.745959
3524.100127	1078481.773192	41.750964
3524.198399	1078032.299692	41.755968
3524.006253	1077572.276053	41.760973
3524.025063	1077124.661111	41.765978
3523.668802	1076664.107918	41.770983
3523.936300	1076208.406877	41.775988
3523.675369	1075773.691744	41.780992
3523.560499	1075318.075485	41.785997
3523.789855	1074856.312996	41.791002
3523.612482	1074407.643296	41.796007
3523.499904	1073954.122493	41.801012
3523.499798	1073509.961441	41.806016
3523.564159	1073062.102370	41.811021
3523.840201	1072600.333947	41.816026
3523.471744	1072159.583434	41.821031
3523.386661	1071692.896647	41.826036
3523.465182	1071263.533839	41.831040
3523.221595	1070817.944898	41.836045
3523.507277	1070371.367326	41.841050
3523.212023	1069929.079345	41.846055
3523.225132	1069474.397554	41.851060
3523.253152	1069041.984458	41.856064
3523.130790	1068583.981745	41.861069
3523.177788	1068137.550022	41.866074
3522.890769	1067695.561366	41.871079
3523.126009	1067252.392997	41.876084
3522.867773	1066828.028663	41.881088
3522.667277	1066379.378311	41.886093
3522.997946	1065943.881220	41.891098
3522.746288	1065496.129256	41.896103
3522.976623	1065052.206778	41.901108
3523.078326	1064623.090001	41.906112
3522.657777	1064179.107947	41.911117
3522.835497	1063734.028968	41.916122
3522.361553	1063296.625778	41.921127
3522.854556	1062853.541308	41.926132
3522.565632	1062424.606041	41.931136
3522.409767	1061989.549631	41.936141
3522.722178	1061551.589286	41.941146
3522.554675	1061115.502786	41.946151
3522.663614	1060675.098776	41.951156
3522.474457	1060233.841817	41.956160
3522.364249	1059793.788658	41.961165
3522.421642	1059351.264526	41.966170
3522.343046	1058925.200692	41.971175
3522.631487	1058491.143308	41.976180
3522.460097	1058042.289405	41.981184
3522.221559	1057615.283476	41.986189
3522.349481	1057192.616958	41.991194
3522.096555	1056745.501853	41.996199
3521.853056	1056310.300264	42.001204
3521.690138	1055887.581636	42.006208
3521.746222	1055456.215276	42.011213
3521.816071	1055024.620127	42.016218
3521.522531	1054614.165162	42.021223
3521.753558	1054174.764135	42.026228
3521.465179	1053756.820332	42.031232
3521.674926	1053337.219923	42.036237
3521.825042	1052919.236964	42.041242
3521.333146	1052494.673210	42.046247
3521.598815	1052077.764954	42.051252
3521.560628	1051656.630946	42.056256
3521.365910	1051237.902392	42.061261
3521.641701	1050818.099862	42.066266
3521.282367	1050388.818087	42.071271
3521.552675	1049965.864276	42.076276
3521.591957	1049552.759143	42.081280
3521.250808	1049122.121595	42.086285
3521.071036	1048709.568647	42.091290
3521.162643	1048296.747217	42.096295
3521.461653	1047870.250315	42.101300
3521.200622	1047463.602704	42.106304
3521.132487	1047029.571747	42.111309
3521.069230	1046632.677991	42.116314
3520.855918	1046199.571437	42.121319
3520.991013	1045787.328315	42.126324
3520.892222	1045382.722265	42.131328
3520.729670	1044966.024786	42.136333
3521.049282	1044544.000906	42.141338
3520.844092	1044141.156953	42.146343
3520.907790	1043735.921044	42.151348
3520.828307	1043326.621598	42.156352
3520.225308	1042911.967746	42.161357
3520.732700	1042495.843942	42.166362
3520.479839	1042097.787254	42.171367
3520.593937	1041683.310051	42.176372
3520.383486	1041280.259323	42.181376
3520.357056	1040873.089721	42.186381
3520.591286	1040468.457113	42.191386
3520.562203	1040070.218283	42.196391
3520.687886	1039658.488086	42.201396
3520.246126	1039251.654801	42.206400
3520.024913	1038849.202968	42.211405
3520.398333	1038442.562981	42.216410
3520.037311	1038044.040327	42.221415
3520.094808	1037634.782449	42.226420
3520.194631	1037239.317591	42.231424
3520.139133	1036841.819089	42.236429
3519.821614	1036448.107734	42.241434
3519.786577	1036052.677529	42.246439
3519.584270	1035655.311973	42.251444
3519.661445	1035271.900505	42.256448
3519.671409	1034882.281428	42.261453
3519.908025	1034477.309455	42.266458
3519.836133	1034075.842547	42.271463
3520.006224	1033694.726498	42.276468
3519.559504	1033295.103834	42.281472
3519.651047	1032897.783603	42.286477
3519.558417	1032497.948709	42.291482
3519.658613	1032119.930835	42.296487
3519.878673	1031703.047001	42.301492
3519.757881	1031323.946702	42.306496
3519.908516	1030940.225269	42.311501
3519.885870	1030533.557314	42.316506
3519.535381	1030135.144892	42.321511
3519.633812	1029744.087085	42.326516
3519.523741	1029350.711831	42.331520
3519.376274	1028968.163062	42.336525
3519.453493	1028576.833340	42.341530
3518.883508	1028179.673692	42.346535
3519.437283	1027779.685033	42.351540
3519.329180	1027406.904458	42.356544
3519.159923	1027015.796717	42.361549
3519.354995	1026624.989214	42.366554
3518.965171	1026242.972156	42.371559
3518.968580	1025864.934508	42.376564
3519.083777	1025484.817643	42.381568
3518.648084	1025104.862624	42.386573
3518.995174	1024717.483074	42.391578
3518.732055	1024340.258733	42.396583
3519.041705	1023950.021085	42.401588
3518.787959	1023588.061695	42.406592
3518.323907	1023196.735596	42.411597
3518.552847	1022821.073129	42.416602
3518.612954	1022459.280016	42.421607
3518.670558	1022075.741250	42.426612
3518.713160	1021707.405064	42.431616
3518.543239	1021328.119881	42.436621
3518.882641	1020949.113145	42.441626
3518.190668	1020568.213618	42.446631
3518.755751	1020186.111088	42.451636
3518.224663	1019819.103515	42.456640
3518.345992	1019446.725290	42.461645
3518.415114	1019069.964681	42.466650
3518.504163	1018712.776558	42.471655
3518.515519	1018325.980959	42.476660
3518.389095	1017967.228245	42.481664
3518.191389	1017588.471235	42.486669
3518.361007	1017215.937131	42.491674
3518.143116	1016843.539222	42.496679
3518.127073	1016476.325354	42.501684
3518.105342	1016120.349668	42.506688
3517.884019	1015736.132317	42.511693
3518.083339	1015376.869311	42.516698
3517.790174	1015012.129852	42.521703
3517.978554	1014648.161370	42.526708
3517.776798	1014293.556269	42.531712
3517.682143	1013920.070416	42.536717
3517.679109	1013578.983986	42.541722
3517.205469	1013203.861922	42.546727
3517.780505	1012843.986792	42.551732
3517.317336	1012501.453818	42.556736
3517.123576	1012142.923356	42.561741
3517.178862	1011788.118069	42.566746
3517.034442	1011437.987025	42.571751
3517.435789	1011083.954844	42.576756
3517.387505	1010738.428487	42.581760
3517.098808	1010398.362526	42.586765
3516.916961	1010027.353820	42.591770
3516.957219	1009701.866521	42.596775
3516.901170	1009340.608113	42.601780
3517.088181	1009008.836071	42.606784
3517.140056	1008657.236331	42.611789
3517.220109	1008300.263251	42.616794
3517.126638	1007962.643022	42.621799
3517.321741	1007601.912452	42.626804
3517.361461	1007255.963765	42.631808
3517.013328	1006908.404706	42.636813
3516.819183	1006552.435864	42.641818
3516.549496	1006214.351108	42.646823
3516.993980	1005854.537584	42.651828
3516.681169	1005516.320892	42.656832
3516.538119	1005169.690922	42.661837
3516.872119	1004837.163141	42.666842
3516.164129	1004495.351275	42.671847
3516.703244	1004146.016889	42.676852
3516.658645	1003821.761035	42.681856
3516.408318	1003472.028579	42.686861
3516.601162	1003134.364429	42.691866
3516.519144	1002804.607428	42.696871
3516.647353	1002468.957696	42.701876
3516.384761	1002125.372131	42.706880
3516.597578	1001801.639314	42.711885
3516.542326	1001447.369866	42.716890
3516.148746	1001129.733096	42.721895
3516.212386	1000774.720605	42.726900
3516.155280	1000454.362237	42.731904
3516.065397	1000117.538142	42.736909
3516.386078	999779.652786	42.741914
3516.162318	999458.097186	42.746919
3516.217392	999131.121943	42.751924
3515.751300	998797.981491	42.756928
3515.696702	998471.862674	42.761933
3515.988490	998152.874830	42.766938
3515.325142	997816.787515	42.771943
3515.864394	997487.202829	42.776948
3515.692949	997177.392036	42.781952
3515.754743	996845.803204	42.786957
3515.943490	996520.895858	42.791962
3515.458489	996199.393241	42.796967
3515.494071	995876.422667	42.801972
3515.334800	995556.681115	42.806977
3515.233100	995231.552918	42.811981
3515.741915	994918.291231	42.816986
3515.413664	994602.518988	42.821991
3515.452317	994289.300044	42.826996
3515.424001	993972.468812	42.832001
3515.294136	993641.893890	42.837005
3515.601270	993326.823264	42.842010
3514.964986	993021.443311	42.847015
3515.275638	992696.784419	42.852020
3515.436495	992380.418148	42.857025
3515.113366	992057.874402	42.862029
3515.245482	991763.122041	42.867034
3515.589343	991432.340566	42.872039
3515.295991	991125.242165	42.877044
3514.966434	990817.353023	42.882049
3514.713325	990502.315649	42.887053
3515.030549	990176.536589	42.892058
3514.667295	989886.644864	42.897063
3514.911555	989566.012006	42.902068
3514.835195	989269.604200	42.907073
3514.578837	988963.748596	42.912077
3514.785815	988657.702693	42.917082
3514.610201	988360.776159	42.922087
3515.029827	988047.443227	42.927092
3514.348077	987753.690392	42.932097
3514.026560	987446.398069	42.937101
3514.335803	987157.915349	42.942106
3513.851758	986860.863839	42.947111
3514.189439	986558.098999	42.952116
3514.294677	986285.414920	42.957121
3514.537004	985982.440034	42.962125
3514.509664	985684.764016	42.967130
3514.457055	985398.203902	42.972135
3514.531181	985084.276937	42.977140
3514.252816	984807.192763	42.982145
3514.290774	984499.291858	42.987149
3514.649951	984196.690986	42.992154
3513.941642	983920.610838	42.997159
3514.139754	983605.410482	43.002164
3514.124471	983325.477137	43.007169
3513.714775	983042.470291	43.012173
3513.855027	982736.703342	43.017178
3513.851732	982453.991000	43.022183
3513.889898	982173.601742	43.027188
3513.665533	981876.247772	43.032193
3513.983351	981589.826055	43.037197
3513.925679	981310.289262	43.042202
3513.763385	981027.239457	43.047207
3513.755605	980730.376265	43.052212
3513.776401	980440.624498	43.057217
3513.290488	980169.015484	43.062221
3513.679735	979890.898805	43.067226
3513.451115	979601.634100	43.072231
3513.753683	979319.986491	43.077236
3513.280084	979049.690224	43.082241
3513.564883	978753.067032	43.087245
3513.572165	978486.085170	43.092250
3513.530195	978199.455122	43.097255
3513.681538	977937.114990	43.102260
3513.544478	977644.315477	43.107265
3513.416355	977380.529759	43.112269
3513.427840	977088.850298	43.117274
3512.963478	976818.642581	43.122279
3512.993815	976538.662486	43.127284
3512.958036	976269.824660	43.132289
3513.107060	975999.868326	43.137293
3512.827917	975727.916560	43.142298
3512.728212	975467.557843	43.147303
3512.861144	975205.291122	43.152308
3512.852642	974932.768122	43.157313
3513.141338	974674.754073	43.162317
3513.194658	974406.107483	43.167322
3512.854852	974141.620653	43.172327
3513.090571	973850.619552	43.177332
3513.119030	973591.817189	43.182337
3512.650317	973323.303646	43.187341
3512.967051	973044.083749	43.192346
3512.661231	972795.864930	43.197351
3512.914730	972529.640846	43.202356
3512.756396	972259.265463	43.207361
3512.898059	972002.427210	43.212365
3513.125796	971722.864169	43.217370
3512.648980	971454.851523	43.222375
3512.780038	971207.861878	43.227380
3512.828826	970922.516177	43.232385
3512.516982	970676.555169	43.237389
3512.580054	970413.102185	43.242394
3512.523336	970142.610342	43.247399
3512.637509	969883.235098	43.252404
3512.384769	969618.427460	43.257409
3512.549948	969369.493458	43.262413
3512.609520	969107.743042	43.267418
3512.219971	968840.083367	43.272423
3512.404209	968592.385136	43.277428
3512.623549	968337.328038	43.282433
3512.050695	968088.166391	43.287437
3512.071971	967823.230876	43.292442
3511.791315	967567.340795	43.297447
3512.040406	967308.120830	43.302452
3512.064598	967064.299780	43.307457
3511.762637	966806.323006	43.312461
3512.030262	966556.662765	43.317466
3511.938351	966315.277317	43.322471
3511.920000	966066.524311	43.327476
3512.054466	965814.699184	43.332481
3512.025266	965567.983194	43.337485
3512.133021	965316.042703	43.342490
3511.990782	965060.899858	43.347495
3511.693114	964814.097814	43.352500
3511.876156	964570.830644	43.357505
3511.573074	964334.197062	43.362509
3511.611303	964087.112593	43.367514
3511.851365	963847.136485	43.372519
3511.846351	963597.490777	43.377524
3511.584543	963347.092674	43.382529
3511.643958	963119.951899	43.387533
3511.840205	962860.932286	43.392538
3511.536666	962633.832128	43.397543
3511.407572	962388.564288	43.402548
3511.694408	962145.471603	43.407553
3511.716661	961909.174824	43.412557
3511.618520	961676.906693	43.417562
3511.532700	961443.647012	43.422567
3511.468902	961192.730608	43.427572
3511.393323	960967.193578	43.432577
3511.455637	960724.862180	43.437581
3511.560977	960486.728914	43.442586
3511.288198	960253.942065	43.447591
3511.351806	960011.286369	43.452596
3511.154172	959767.094782	43.457601
3511.051971	959542.290780	43.462605
3511.150875	959316.856583	43.467610
3511.131103	959085.647812	43.472615
3511.184472	958856.869238	43.477620
3511.260483	958621.605638	43.482625
3510.876086	958392.978846	43.487629
3510.789628	958167.236083	43.492634
3510.834662	957940.285928	43.497639
3510.955775	957716.550950	43.502644
3510.917747	957486.163848	43.507649
3510.897266	957250.467949	43.512653
3511.319436	957026.852853	43.517658
3510.913391	956796.008386	43.522663
3510.442373	956574.582897	43.527668
3510.922637	956358.191678	43.532673
3510.757102	956144.253279	43.537677
3510.876438	955905.536304	43.542682
3510.857831	955687.948989	43.547687
3511.176183	955458.306824	43.552692
3510.738700	955240.732404	43.557697
3510.117674	955034.176681	43.562701
3510.541788	954797.793013	43.567706
3510.505568	954608.529633	43.572711
3510.384987	954390.962351	43.577716
3510.382150	954177.957533	43.582721
3510.686485	953962.023646	43.587725
3510.654668	953753.979848	43.592730
3510.708696	953547.444003	43.597735
3510.717841	953325.122543	43.602740
3510.728529	953111.592686	43.607745
3510.621037	952911.180521	43.612749
3510.207816	952690.240425	43.617754
3510.234044	952468.548637	43.622759
3510.075139	952258.646968	43.627764
3510.348331	952050.292230	43.632769
3510.050437	951854.271700	43.637773
3510.030258	951649.872378	43.642778
3509.930613	951447.391991	43.647783
3510.206356	951239.099560	43.652788
3510.214818	951029.598499	43.657793
3509.956720	950834.489498	43.662797
3509.941294	950629.761611	43.667802
3510.073587	950432.945896	43.672807
3510.263069	950228.359702	43.677812
3510.153528	950023.527439	43.682817
3509.650744	949814.252464	43.687821
3509.806690	949615.965623	43.692826
3509.757001	949429.767940	43.697831
3509.932128	949223.037905	43.702836
3510.012014	949016.602496	43.707841
3510.026385	948822.042460	43.712845
3510.218624	948623.424184	43.717850
3509.779366	948420.018707	43.722855
3510.202309	948221.729989	43.727860
3509.961448	948010.327603	43.732865
3509.963626	947821.477653	43.737869
3510.053450	947615.367592	43.742874
3509.832185	947425.007609	43.747879
3509.916418	947227.694261	43.752884
3509.715680	947023.907143	43.757889
3509.482343	946828.929651	43.762893
3509.577499	946636.668592	43.767898
3509.527472	946441.167347	43.772903
3509.364868	946249.317527	43.777908
3509.335754	946061.079007	43.782913
3509.508576	945868.968253	43.787917
3509.524238	945687.510829	43.792922
3509.259650	945505.518352	43.797927
3509.210556	945289.949154	43.802932
3509.542156	945113.210307	43.807937
3509.096599	944920.016445	43.812941
3509.444174	944732.817524	43.817946
3509.397317	944552.480599	43.822951
3509.068373	944368.829787	43.827956
3509.028270	944187.424936	43.832961
3509.254193	943995.044418	43.837965
3509.066433	943818.730439	43.842970
3509.100956	943643.715695	43.847975
3508.934458	943460.389418	43.852980
3509.185690	943268.936372	43.857985
3508.665916	943084.121410	43.862989
3508.668297	942911.004429	43.867994
3508.985200	942745.402921	43.872999
3509.083450	942551.072872	43.878004
3509.128160	942377.643620	43.883009
3508.955740	942211.147070	43.888013
3509.172087	942012.655071	43.893018
3508.613890	941837.293799	43.898023
3508.923597	941652.483227	43.903028
3508.664375	941482.334248	43.908033
3508.658603	941311.754434	43.913037
3508.808473	941118.417327	43.918042
3508.714824	940964.142073	43.923047
3508.809949	940787.966718	43.928052
3508.705728	940616.325573	43.933057
3508.753367	940438.132364	43.938061
3509.146925	940268.315893	43.943066
3508.640308	940079.939785	43.948071
3508.459085	939915.002027	43.953076
3508.716970	939744.231793	43.958081
3508.241424	939571.946175	43.963085
3508.786155	939400.541994	43.968090
3508.364436	939234.087671	43.973095
3508.634414	939060.703216	43.978100
3508.236753	938891.835860	43.983105
3508.336993	938726.238778	43.988109
3508.748759	938545.522930	43.993114
3508.218786	938394.505805	43.998119
3508.279479	938206.352741	44.003124
3508.418383	938049.266989	44.008129
3508.498413	937878.945146	44.013133
3508.290573	937712.119519	44.018138
3508.077971	937557.091987	44.023143
3507.988520	937388.605355	44.028148
3508.135699	937212.109497	44.033153
3508.097891	937070.761447	44.038157
3508.625873	936899.854338	44.043162
3508.026261	936749.953094	44.048167
3508.167971	936570.941436	44.053172
3508.297415	936420.334898	44.058177
3508.113180	936266.512427	44.063181
3508.536484	936090.893369	44.068186
3507.917719	935937.612796	44.073191
3507.733288	935768.706114	44.078196
3508.014655	935612.100213	44.083201
3507.563728	935456.858212	44.088205
3507.719703	935293.543930	44.093210
3507.853759	935143.476217	44.098215
3507.974092	934985.726295	44.103220
3507.948725	934828.475698	44.108225
3507.691790	934670.586510	44.113229
3507.953908	934518.271786	44.118234
3507.813770	934365.058798	44.123239
3507.838059	934204.901085	44.128244
3507.767790	934050.227232	44.133249
3507.454664	933898.277495	44.138253
3507.766491	933743.627787	44.143258
3507.816984	933608.894383	44.148263
3507.878932	933434.879209	44.153268
3507.818648	933292.569580	44.158273
3507.487817	933137.335823	44.163277
3507.457343	932981.279744	44.168282
3507.340009	932845.882345	44.173287
3507.618721	932695.913612	44.178292
3507.640966	932548.672204	44.183297
3507.286714	932399.471689	44.188301
3507.548462	932252.951041	44.193306
3507.461268	932106.579888	44.198311
3507.446127	931960.673128	44.203316
3507.651543	931808.193950	44.208321
3507.366673	931666.454140	44.213325
3507.103425	931516.829631	44.218330
3507.278909	931373.373082	44.223335
3507.179880	931230.534312	44.228340
3507.216945	931094.874783	44.233345
3507.242674	930956.427479	44.238349
3507.623018	930807.926046	44.243354
3507.291658	930666.263364	44.248359
3507.561441	930529.494239	44.253364
3507.382861	930381.841677	44.258369
3507.196767	930240.335932	44.263373
3507.341924	930092.429867	44.268378
3506.889190	929954.996303	44.273383
3507.258241	929805.604019	44.278388
3507.349939	929663.748958	44.283393
3506.654493	929538.645294	44.288397
3506.954625	929400.400756	44.293402
3507.202677	929266.774314	44.298407
3507.002719	929104.385739	44.303412
3507.152759	928977.880281	44.308417
3506.959521	928831.821200	44.313421
3507.019920	928710.225984	44.318426
3507.118803	928580.067148	44.323431
3507.005927	928427.447755	44.328436
3506.981512	928306.722440	44.333441
3506.881595	928159.668429	44.338445
3507.052509	928026.408259	44.343450
3506.727929	927903.608485	44.348455
3506.731815	927745.567142	44.353460
3506.756847	927631.740078	44.358465
3506.720118	927510.037507	44.363469
3506.563354	927365.662942	44.368474
3506.466549	927243.675806	44.373479
3506.552178	927115.598750	44.378484
3506.697322	926976.548090	44.383489
3506.658022	926854.158052	44.388493
3506.698446	926709.156470	44.393498
3506.413833	926594.204601	44.398503
3506.529623	926461.010826	44.403508
3506.790390	926346.733090	44.408513
3506.587777	926206.373580	44.413517
3506.790362	926070.944159	44.418522
3506.355430	925951.387474	44.423527
3506.209021	925821.106010	44.428532
3506.731467	925694.558028	44.433537
3506.398915	925584.497148	44.438541
3506.548002	925452.234655	44.443546
3506.299338	925326.670613	44.448551
3506.109345	925202.536662	44.453556
3506.512586	925084.457719	44.458561
3506.439800	924972.225570	44.463565
3506.237010	924834.427277	44.468570
3506.117794	924718.253894	44.473575
3505.881227	924593.344095	44.478580
3506.346843	924476.973005	44.483585
3506.096038	924357.927792	44.488589
3506.509065	924246.947259	44.493594
3506.132228	924143.116974	44.498599
3506.277842	924007.933733	44.503604
3506.139743	923892.226692	44.508609
3506.037467	923773.625149	44.513613
3506.150353	923636.321517	44.518618
3506.040230	923526.663057	44.523623
3506.102237	923415.723286	44.528628
3506.422270	923294.443995	44.533633
3505.830989	923179.758479	44.538637
3506.135015	923063.094948	44.543642
3506.260461	922947.997821	44.548647
3506.332004	922829.154512	44.553652
3506.293368	922717.543467	44.558657
3506.079807	922588.542199	44.563661
3506.065739	922486.833544	44.568666
3505.620728	922371.433220	44.573671
3505.823505	922265.161923	44.578676
3506.041722	922150.225038	44.583681
3505.815644	922037.572304	44.588685
3505.781036	921935.567989	44.593690
3505.949993	921819.669850	44.598695
3506.034233	921697.623769	44.603700
3506.071194	921587.324388	44.608705
3505.946462	921481.476665	44.613709
3506.015828	921359.714176	44.618714
3505.824464	921255.990466	44.623719
3505.954318	921144.030555	44.628724
3505.993053	921023.516839	44.633729
3505.693113	920920.670889	44.638733
3505.894308	920804.360766	44.643738
3505.902436	920701.748704	44.648743
3505.956426	920585.939452	44.653748
3505.998091	920469.167138	44.658753
3505.682606	920363.040266	44.663757
3505.889335	920254.707446	44.668762
3505.794369	920140.742321	44.673767
3505.903678	920034.057725	44.678772
3505.855285	919918.251133	44.683777
3505.688883	919815.651116	44.688781
3505.659605	919699.355352	44.693786
3505.701458	919599.316421	44.698791
3505.771753	919482.036839	44.703796
3505.782998	919383.539475	44.708801
3505.557451	919292.011755	44.713805
3506.178461	919183.011703	44.718810
3505.689533	919078.525224	44.723815
3505.381808	918967.844385	44.728820
3505.688570	918861.104320	44.733825
3505.453162	918748.192418	44.738829
3505.504987	918653.334329	44.743834
3505.667444	918542.374831	44.748839
3505.793390	918446.152782	44.753844
3505.473098	918325.060734	44.758849
3505.501544	918239.444163	44.763853
3505.940899	918125.541532	44.768858
3505.493700	918031.140053	44.773863
3505.689499	917905.331021	44.778868
3505.672210	917808.832424	44.783873
3505.455362	917716.891629	44.788877
3505.710263	917595.784999	44.793882
3505.585363	917501.321286	44.798887
3505.781988	917395.533910	44.803892
3505.613553	917283.254933	44.808897
3505.314906	917189.585009	44.813901
3505.455282	917083.608231	44.818906
3505.183578	916985.114245	44.823911
3505.463201	916894.619053	44.828916
3505.397641	916792.716251	44.833921
3505.233762	916684.662665	44.838925
3505.400129	916580.213145	44.843930
3505.125260	916495.678906	44.848935
3505.538722	916390.896087	44.853940
3505.398912	916287.936452	44.858945
3505.441026	916203.538174	44.863949
3505.496232	916093.413757	44.868954
3505.439573	915997.660466	44.873959
3505.338067	915892.952963	44.878964
3505.465219	915787.049659	44.883969
3505.398080	915692.448914	44.888973
3505.375522	915590.516701	44.893978
3505.661245	915501.250070	44.898983
3505.463055	915385.950289	44.903988
3505.210306	915288.193529	44.908993
3504.800029	915198.073070	44.913997
3505.320736	915112.422933	44.919002
3505.022895	915013.608788	44.924007
3504.926708	914915.241455	44.929012
3505.307574	914822.864606	44.934017
3505.021465	914723.946962	44.939021
3505.262335	914628.024439	44.944026
3505.308962	914545.623635	44.949031
3505.138091	914449.476718	44.954036
3505.570668	914353.035988	44.959041
3505.396475	914250.140209	44.964045
3505.579819	914148.436479	44.969050
3505.188673	914065.329603	44.974055
3505.150432	913961.635038	44.979060
3505.115211	913878.563097	44.984065
3504.837813	913800.156036	44.989069
3505.032668	913692.466432	44.994074
3505.313481	913601.145790	44.999079
3505.207008	913501.019990	45.004084
3505.444397	913405.462310	45.009089
3504.913580	913318.318918	45.014093
3504.961419	913219.030080	45.019098
3505.333556	913130.385534	45.024103
3505.131043	913040.291923	45.029108
3505.079723	912954.124127	45.034113
3504.933533	912859.198541	45.039117
3504.843373	912758.574602	45.044122
3504.869934	912685.307131	45.049127
3505.192333	912593.480981	45.054132
3505.360305	912496.087384	45.059137
3505.138339	912400.780791	45.064141
3505.050423	912310.174373	45.069146
3505.390155	912209.758856	45.074151
3505.157524	912121.776197	45.079156
3504.941730	912034.464240	45.084161
3504.870582	911940.378210	45.089165
3504.990601	911847.898133	45.094170
3504.908703	911766.826811	45.099175
3505.150743	911664.874852	45.104180
3505.243380	911574.612319	45.109185
3505.001202	911486.042609	45.114189
3505.298484	911380.894452	45.119194
3505.235536	911289.110137	45.124199
3504.876686	911194.383850	45.129204
3505.464159	911100.175065	45.134209
3504.994019	911023.206742	45.139213
3505.154205	910927.136827	45.144218
3504.759087	910839.256975	45.149223
3504.955014	910756.775068	45.154228
3505.062823	910653.669424	45.159233
3504.900214	910572.497485	45.164237
3505.099125	910493.675755	45.169242
3504.965041	910404.299450	45.174247
3505.113571	910297.419350	45.179252
3504.833349	910210.860790	45.184257
3504.663999	910129.104819	45.189261
3505.078531	910019.089342	45.194266
3504.468051	909941.068203	45.199271
3504.929344	909868.849246	45.204276
3504.907521	909775.297038	45.209281
3504.814905	909695.740401	45.214285
3504.526124	909611.681648	45.219290
3504.453158	909520.351989	45.224295
3504.674115	909429.068874	45.229300
3504.579906	909355.198535	45.234305
3504.538082	909275.916896	45.239309
3504.930790	909195.694415	45.244314
3504.639644	909115.872800	45.249319
3504.685082	909032.329007	45.254324
3505.131688	908946.692131	45.259329
3504.600841	908857.645691	45.264333
3504.732596	908773.890871	45.269338
3504.585369	908700.502909	45.274343
3504.653255	908605.855101	45.279348
3504.426937	908522.059001	45.284353
3504.432657	908449.607259	45.289357
3504.692566	908369.008857	45.294362
3504.341673	908288.413417	45.299367
3504.782545	908208.844129	45.304372
3504.806444	908124.229014	45.309377
3504.739389	908049.468568	45.314381
3505.047755	907950.428419	45.319386
3504.582827	907885.861887	45.324391
3504.383905	907798.191072	45.329396
3504.834985	907717.551770	45.334401
3504.876203	907635.820967	45.339405
3504.770376	907536.359254	45.344410
3504.699732	907460.819599	45.349415
3504.339359	907387.063490	45.354420
3504.636406	907313.680586	45.359425
3504.457656	907232.752053	45.364429
3504.755258	907132.348247	45.369434
3504.401166	907065.438057	45.374439
3504.389751	906989.496282	45.379444
3504.636682	906911.870428	45.384449
3504.358053	906845.813673	45.389453
3504.586039	906747.151430	45.394458
3504.503550	906677.779295	45.399463
3504.243399	906582.089651	45.404468
3504.572810	906518.245004	45.409473
3504.687584	906436.002001	45.414477
3504.738839	906354.443816	45.419482
3504.524391	906282.772291	45.424487
3504.802069	906188.338474	45.429492
3504.835529	906104.945852	45.434497
3504.714652	906032.869660	45.439501
3504.897555	905946.554618	45.444506
3504.435724	905859.958369	45.449511
3504.518563	905789.775849	45.454516
3504.466149	905704.943628	45.459521
3504.510371	905623.568996	45.464525
3504.378922	905540.677743	45.469530
3504.588988	905472.111186	45.474535
3504.415225	905391.155181	45.479540
3504.578904	905308.115352	45.484545
3504.339054	905216.356633	45.489549
3504.596926	905146.040695	45.494554
3504.632360	905072.092322	45.499559
3504.546958	904992.081313	45.504564
3504.618859	904905.092790	45.509569
3504.297004	904835.158045	45.514573
3504.311965	904757.540547	45.519578
3504.265296	904683.310962	45.524583
3504.219812	904620.375296	45.529588
3504.250921	904532.036160	45.534593
3504.219825	904467.262134	45.539597
3504.651146	904394.301584	45.544602
3504.262462	904324.178391	45.549607
3504.135408	904254.590500	45.554612
3503.966368	904175.643628	45.559617
3504.086536	904094.717047	45.564621
3504.305638	904023.910706	45.569626
3504.196959	903967.060739	45.574631
3504.225948	903887.497899	45.579636
3504.259338	903811.409120	45.584641
3503.922894	903735.766445	45.589645
3504.015914	903678.301009	45.594650
3504.039236	903605.687097	45.599655
3503.900253	903550.575928	45.604660
3504.208182	903470.188780	45.609665
3503.834511	903412.990620	45.614669
3504.182866	903335.491688	45.619674
3504.041855	903284.433816	45.624679
3504.064076	903199.744569	45.629684
3504.258108	903138.780698	45.634689
3503.933160	903066.989715	45.639693
3504.095944	902984.977929	45.644698
3504.111071	902920.854446	45.649703
3504.166958	902862.710823	45.654708
3504.356517	902785.616761	45.659713
3504.334800	902731.830249	45.664717
3504.140880	902637.897272	45.669722
3503.864700	902573.045225	45.674727
3504.009715	902495.375085	45.679732
3504.383480	902433.697955	45.684737
3504.134705	902370.191133	45.689741
3504.223790	902281.710539	45.694746
3504.353128	902210.123547	45.699751
3503.885231	902139.599833	45.704756
3504.045985	902076.698325	45.709761
3503.773940	902006.237267	45.714765
3504.313400	901930.426061	45.719770
3503.997736	901871.077802	45.724775
3504.071413	901799.398182	45.729780
3504.230306	901734.078473	45.734785
3503.951801	901651.154090	45.739789
3504.114063	901585.638929	45.744794
3504.113302	901533.479588	45.749799
3504.009462	901468.972825	45.754804
3503.917150	901397.798413	45.759809
3503.735043	901338.325957	45.764813
3504.136169	901245.334332	45.769818
3504.071534	901120.443655	45.774823
3503.856161	900931.721216	45.779828
3503.928103	900679.088470	45.784833
3503.760526	900383.588435	45.789837
3503.907924	900014.012135	45.794842
3503.893973	899590.135147	45.799847
3503.481422	899094.783609	45.804852
3503.677845	898526.903076	45.809857
3503.531425	897914.658335	45.814861
3503.436260	897220.174084	45.819866
3503.101110	896467.831320	45.824871
3502.692147	895652.261841	45.829876
3502.864115	894755.923615	45.834881
3502.791668	893797.969480	45.839885
3502.706823	892762.271652	45.844890
3502.641534	891642.300302	45.849895
3501.898547	890469.962107	45.854900
3501.994104	889196.285336	45.859905
3501.730247	887865.746274	45.864909
3501.709177	886427.169275	45.869914
3501.580906	884933.425115	45.874919
3501.097679	883338.777632	45.879924
3501.050161	881667.731603	45.884929
3501.133913	879925.412248	45.889933
3500.531830	878071.450237	45.894938
3500.150053	876147.116589	45.899943
3499.620565	874137.072296	45.904948
3499.477301	872035.611781	45.909953
3499.108916	869861.680895	45.914957
3499.122452	867594.993576	45.919962
3498.446399	865225.031985	45.924967
3498.232069	862794.855480	45.929972
3498.003002	860260.411641	45.934977
3497.484145	857652.373125	45.939981
3497.152053	854944.288103	45.944986
3496.704674	852165.204518	45.949991
3496.312201	849283.337499	45.954996
3496.003959	846317.071834	45.960001
3495.297845	843284.957645	45.965005
3494.997752	840120.273701	45.970010
3494.120900	836900.712916	45.975015
3493.782413	833603.895167	45.980020
3493.460252	830214.993988	45.985025
3492.960206	826743.005154	45.990029
3492.141990	823176.729375	45.995034
3491.239515	819555.980141	46.000039
3490.942996	815814.408034	46.005044
3490.654911	812007.445867	46.010049
3489.587474	808109.538489	46.015053
3489.343879	804116.557248	46.020058
3488.888207	800057.342576	46.025063
3487.943286	795888.035205	46.030068
3487.546272	791652.767997	46.035073
3486.603811	787325.860204	46.040077
3485.667519	782916.774142	46.045082
3485.270555	778426.234691	46.050087
3484.131417	773857.632674	46.055092
3483.684317	769179.954377	46.060097
3482.595097	764449.283660	46.065101
3482.028314	759604.502326	46.070106
3481.151118	754706.218059	46.075111
3480.050678	749724.747280	46.080116
3479.725894	744622.218850	46.085121
3478.529629	739468.982048	46.090125
3478.020852	734215.749855	46.095130
3476.233746	728879.196507	46.100135
3475.684869	723462.013616	46.105140
3474.733185	717960.393047	46.110145
3473.636176	712381.227145	46.115149
3473.013915	706694.703380	46.120154
3472.121306	700932.704719	46.125159
3470.942643	695097.480208	46.130164
3469.726063	689174.069412	46.135169
3468.913449	683159.946243	46.140173
3468.057621	677064.341357	46.145178
3466.901953	670891.941926	46.150183
3465.523342	664621.740928	46.155188
3464.604737	658264.493715	46.160193
3463.233330	651828.201622	46.165197
3462.200428	645313.057720	46.170202
3460.942093	638730.091048	46.175207
3459.613296	632043.276119	46.180212
3458.510087	625281.310555	46.185217
3457.267036	618447.408477	46.190221
3456.034834	611511.350244	46.195226
3454.420793	604512.156692	46.200231
3453.106198	597430.507929	46.205236
3451.946117	590251.952124	46.210241
3450.233198	583014.499789	46.215245
3448.929973	575684.732010	46.220250
3447.338288	568285.767433	46.225255
3446.094095	560802.429348	46.230260
3444.590165	553226.672170	46.235265
3442.910046	545579.977267	46.240269
3441.528004	537851.874484	46.245274
3439.705382	530037.175368	46.250279
3437.852985	522172.218997	46.255284
3436.498919	514206.684521	46.260289
3434.575523	506195.182183	46.265293
3433.252915	498082.041498	46.270298
3431.205950	489906.340731	46.275303
3429.764783	481658.293393	46.280308
3428.025483	473321.681344	46.285313
3425.988454	464910.978201	46.290317
3424.273685	456423.349722	46.295322
3422.333298	447878.168606	46.300327
3420.275801	439250.542511	46.305332
3418.254311	430566.196696	46.310337
3415.979132	421807.814219	46.315341
3413.760514	412978.913527	46.320346
3411.777523	404083.478574	46.325351
3409.580722	395113.410921	46.330356
3407.389528	386103.992861	46.335361
3404.998570	377015.054499	46.340365
3403.059500	367865.278810	46.345370
3400.644097	358655.726275	46.350375
3398.127915	349384.909327	46.355380
3395.745010	340060.607509	46.360385
3392.834528	330672.077575	46.365389
3390.257453	321243.863606	46.370394
3387.794794	311764.630753	46.375399
3385.280406	302217.459064	46.380404
3382.862207	292630.883946	46.385409
3379.887333	283002.519141	46.390413
3377.315362	273296.660203	46.395418
3374.358822	263569.350290	46.400423
3371.140453	253797.871748	46.405428
3368.517646	243970.240652	46.410433
3364.947238	234108.314258	46.415437
3361.832763	224216.761289	46.420442
3358.512019	214228.309133	46.425447
3355.198407	204241.210244	46.430452
3351.780307	194248.739420	46.435457
3348.375132	184245.271131	46.440461
3344.631516	174199.156636	46.445466
3340.808139	164163.147196	46.450471
3336.846624	154074.689459	46.455476
3332.940383	143998.574554	46.460481
3328.195049	133922.700188	46.465485
3323.827610	123834.542154	46.470490
3319.451509	113757.495338	46.475495
3314.225155	103704.085371	46.480500
3309.128892	93657.449918	46.485505
3303.747463	83641.256989	46.490509
3298.078847	73644.297758	46.495514
3291.575490	63707.665436	46.500519
3284.715209	53830.014179	46.505524
3276.935870	44047.927446	46.510529
3266.366085	34403.857848	46.515533
3239.632376	25336.776728	46.520538
3188.847913	17216.976044	46.525543
3134.444047	9811.014792	46.530548
3079.320899	3297.324172	46.535553
2932.113149	395.506107	46.540557
2749.012224	366.340992	46.545562
2670.363585	364.697066	46.550567
2684.996891	378.436409	46.555572
2753.196035	352.501916	46.560577
2831.435981	341.092317	46.565581
2893.111293	345.110942	46.570586
2926.672081	334.137030	46.575591
2935.215953	344.722178	46.580596
2928.601139	332.751598	46.585601
2916.485482	332.485380	46.590605
2904.922102	320.394775	46.595610
2896.853128	317.069787	46.600615
2891.704365	319.779070	46.605620
2889.255130	306.687197	46.610625
2888.144309	331.539040	46.615629
2886.895372	321.712166	46.620634
2885.763434	297.587945	46.625639
2883.578175	309.929085	46.630644
2881.170757	294.294094	46.635649
2877.617680	309.401594	46.640653
2874.390371	312.549510	46.645658
2871.380483	302.976349	46.650663
2868.323814	302.233032	46.655668
2865.330583	292.119483	46.660673
2862.138212	300.693009	46.665677
2858.864835	311.096961	46.670682
2855.984458	304.367008	46.675687
2852.711192	310.693273	46.680692
2849.773315	299.514929	46.685697
2846.366468	298.314289	46.690701
2843.167123	298.085789	46.695706
2840.031974	292.861445	46.700711
2836.014788	289.407996	46.705716
2833.521095	284.907372	46.710721
2829.620909	288.596350	46.715725
2826.920309	274.009573	46.720730
2823.343574	282.394609	46.725735
2819.910414	280.142750	46.730740
2816.821112	293.651109	46.735745
2813.397301	296.102701	46.740749
2810.142900	296.389374	46.745754
2806.588492	274.826244	46.750759
2803.049029	283.713889	46.755764
2800.109175	276.180791	46.760769
2796.584704	283.989778	46.765773
2793.278697	284.865333	46.770778
2790.312162	280.431829	46.775783
2786.505371	275.915578	46.780788
2783.219089	270.409477	46.785793
2779.499291	279.448891	46.790797
2776.137374	274.127210	46.795802
2772.847644	275.898311	46.800807
2769.308240	288.065333	46.805812
2766.133160	278.832396	46.810817
2762.490770	275.103324	46.815821
2759.505728	264.966298	46.820826
2756.247004	269.919029	46.825831
2752.318498	266.530031	46.830836
2748.855696	267.698800	46.835841
2745.157642	267.865682	46.840845
2742.186321	270.985346	46.845850
2738.744275	272.018307	46.850855
2735.293157	269.988357	46.855860
2732.299302	276.441620	46.860865
2728.469189	283.960379	46.865869
2724.871975	265.989665	46.870874
2721.548805	270.994073	46.875879
2717.715665	277.571016	46.880884
2714.151127	262.393272	46.885889
2711.648901	275.468251	46.890893
2708.074404	255.887080	46.895898
2703.912934	267.366078	46.900903
2700.755058	267.326130	46.905908
2697.392977	267.247639	46.910913
2693.497824	266.473452	46.915917
2690.798333	263.318190	46.920922
2686.910994	268.615397	46.925927
2683.192130	264.248371	46.930932
2679.923839	253.794168	46.935937
2676.159822	244.614204	46.940941
2672.993198	248.767103	46.945946
2669.899902	247.003049	46.950951
2666.580096	257.923918	46.955956
2663.278497	243.942227	46.960961
2659.264217	263.396693	46.965965
2655.611367	254.519614	46.970970
2652.869817	243.119333	46.975975
2648.792612	257.531063	46.980980
2645.214572	250.119847	46.985985
2641.859632	249.941947	46.990989
2638.687744	250.089208	46.995994
2635.165114	255.488285	47.000999
2631.188012	257.338150	47.006004
2628.158672	244.305203	47.011009
2624.783405	252.961220	47.016013
2621.154151	255.609436	47.021018
2617.813684	255.735866	47.026023
2613.826317	248.021429	47.031028
2610.636858	257.137605	47.036033
2607.097808	254.734517	47.041037
2603.683491	242.403236	47.046042
2600.525804	244.394426	47.051047
2596.461429	256.952379	47.056052
2593.302580	251.952063	47.061057
2589.793751	248.411684	47.066061
2586.041240	244.273905	47.071066
2583.053978	242.610095	47.076071
2579.524107	245.091301	47.081076
2576.195175	237.440075	47.086081
2571.960140	253.127565	47.091085
2568.627792	244.681183	47.096090
2565.420768	257.187059	47.101095
2561.416535	245.821891	47.106100
2558.827806	247.311261	47.111105
2555.192035	248.562891	47.116109
2551.736756	244.491246	47.121114
2548.440632	237.377501	47.126119
2544.419131	239.886910	47.131124
2540.905078	242.202256	47.136129
2537.475122	232.133794	47.141133
2533.977081	240.252999	47.146138
2530.305853	231.815664	47.151143
2526.900940	238.959246	47.156148
2523.832499	241.234168	47.161153
2519.781432	248.576643	47.166157
2516.335345	245.503129	47.171162
2513.277306	235.031821	47.176167
2509.598448	263.103230	47.181172
2506.364019	246.226586	47.186177
2502.985477	247.817504	47.191181
2499.045534	250.576295	47.196186
2495.688804	238.302765	47.201191
2492.364527	242.355551	47.206196
2488.997945	247.783801	47.211201
2485.029358	242.928903	47.216205
2481.501255	249.351951	47.221210
2478.286375	231.813523	47.226215
2474.681640	248.721102	47.231220
2471.397940	232.253735	47.236225
2467.568263	240.296840	47.241229
2464.299608	233.675515	47.246234
2460.965548	225.138230	47.251239
2457.009484	226.692605	47.256244
2453.932433	228.129256	47.261249
2450.349007	242.974480	47.266253
2447.255034	230.780672	47.271258
2443.727845	230.542774	47.276263
2439.866462	225.315974	47.281268
2436.280852	241.597620	47.286273
2432.423570	227.301175	47.291277
2429.198780	233.819138	47.296282
2425.890535	230.741290	47.301287
2422.436669	232.926506	47.306292
2418.793926	240.381329	47.311297
2415.235004	230.774581	47.316301
2412.052824	238.551905	47.321306
2408.810770	227.944182	47.326311
2404.562443	235.123806	47.331316
2401.524205	221.856397	47.336321
2397.767671	221.607807	47.341325
2394.480870	228.392399	47.346330
2391.256641	219.780614	47.351335
2387.368374	229.154737	47.356340
2384.217170	218.925077	47.361345
2380.260656	225.835903	47.366349
2376.919903	233.557014	47.371354
2373.510042	232.370411	47.376359
2370.009459	233.296185	47.381364
2366.939370	220.626150	47.386369
2362.907131	231.791453	47.391373
2358.893309	223.615816	47.396378
2355.441558	214.214192	47.401383
2352.622250	215.715017	47.406388
2349.592615	204.698229	47.411393
2345.510527	221.968753	47.416397
2342.084193	230.049069	47.421402
2338.266506	219.951939	47.426407
2334.534297	235.087296	47.431412
2331.528918	226.432442	47.436417
2327.970684	223.117083	47.441421
2324.668807	215.726019	47.446426
2321.177744	219.152320	47.451431
2317.414054	220.954220	47.456436
2314.014854	212.443351	47.461441
2310.618695	220.334911	47.466445
2306.947886	208.847077	47.471450
2303.514557	221.360727	47.476455
2300.145711	221.795722	47.481460
2296.656702	208.524397	47.486465
2293.139164	229.901294	47.491469
2289.445303	219.400121	47.496474
2286.295539	219.661766	47.501479
2282.333623	230.700280	47.506484
2279.136444	217.622619	47.511489
2275.430713	214.089823	47.516493
2272.241476	221.985843	47.521498
2268.618159	219.261808	47.526503
2264.853960	214.737752	47.531508
2261.484178	218.115270	47.536513
2257.761429	222.490355	47.541517
2254.650769	211.064750	47.546522
2251.285472	208.408167	47.551527
2247.229599	217.106508	47.556532
2244.122568	213.249864	47.561537
2240.521077	229.005408	47.566541
2237.240502	220.979707	47.571546
2233.789015	213.797252	47.576551
2230.250217	219.465603	47.581556
2226.675915	205.120177	47.586561
2222.835559	208.818002	47.591565
2219.512745	203.668535	47.596570
2216.174127	204.238468	47.601575
2212.761893	208.096528	47.606580
2209.150649	205.413843	47.611585
2205.721370	215.193743	47.616589
2201.938188	210.289203	47.621594
2198.658842	212.677458	47.626599
2194.606757	218.635677	47.631604
2191.700584	210.169139	47.636609
2188.050782	217.416859	47.641613
2184.175611	201.726270	47.646618
2181.318466	207.448233	47.651623
2177.790375	211.178330	47.656628
2174.371939	201.255182	47.661633
2170.316408	210.872623	47.666637
2167.082174	208.120080	47.671642
2163.769477	212.132210	47.676647
2159.719303	211.870518	47.681652
2156.806052	208.054362	47.686657
2153.346324	203.756273	47.691661
2149.485217	208.503743	47.696666
2146.017358	207.978598	47.701671
2142.601390	198.105079	47.706676
2139.229436	196.401921	47.711681
2135.450675	197.509330	47.716685
2131.859775	199.530527	47.721690
2128.345433	195.569968	47.726695
2124.995597	215.494122	47.731700
2121.956941	205.034145	47.736705
2118.101604	197.475041	47.741709
2114.491112	206.273891	47.746714
2111.099239	198.417958	47.751719
2107.405273	205.288156	47.756724
2104.123964	210.219388	47.761729
2100.516677	210.761083	47.766733
2097.290380	199.899295	47.771738
2093.637797	201.407148	47.776743
2089.965096	206.131854	47.781748
2086.352566	202.638638	47.786753
2083.184051	203.065446	47.791757
2079.704147	206.280770	47.796762
2076.155490	208.822114	47.801767
2072.470742	216.687673	47.806772
2069.076071	196.972882	47.811777
2065.613087	204.580978	47.816781
2062.191781	216.746261	47.821786
2058.259701	208.620867	47.826791
2054.638563	224.920310	47.831796
2051.676637	211.332626	47.836801
2048.432364	212.543095	47.841805
2044.745977	208.817134	47.846810
2041.265407	206.021235	47.851815
2037.541533	212.189078	47.856820
2034.003798	204.161029	47.861825
2030.264463	203.210654	47.866829
2026.942885	206.831775	47.871834
2023.575477	203.320156	47.876839
2019.660225	209.373079	47.881844
2016.915278	191.095619	47.886849
2013.316023	198.836800	47.891853
2009.428541	200.697643	47.896858
2005.618817	197.134011	47.901863
2002.077231	204.191905	47.906868
1998.990071	196.254988	47.911873
1995.456461	208.981191	47.916877
1992.034468	212.947694	47.921882
1988.754713	207.399597	47.926887
1985.353744	212.962148	47.931892
1982.027452	204.128099	47.936897
1978.012488	216.489008	47.941901
1974.512592	210.778749	47.946906
1971.012760	197.057601	47.951911
1967.254958	195.640239	47.956916
1964.257394	193.957084	47.961921
1960.722577	191.535281	47.966925
1956.943072	189.650452	47.971930
1953.663352	191.779124	47.976935
1949.855990	206.259712	47.981940
1946.735097	198.304710	47.986945
1942.949483	194.612047	47.991949
1939.322764	200.800697	47.996954
1936.083439	196.566196	48.001959
1932.485654	193.908763	48.006964
1929.210305	194.593770	48.011969
1925.656745	203.286920	48.016973
1922.100240	198.421699	48.021978
1918.724385	199.801906	48.026983
1915.007532	208.359526	48.031988
1911.728828	195.011531	48.036993
1907.948992	208.597083	48.041997
1904.791951	199.033459	48.047002
1901.404310	198.115494	48.052007
1897.212129	203.112338	48.057012
1893.659544	193.896613	48.062017
1890.301788	197.714940	48.067021
1886.762719	204.945400	48.072026
1883.686645	197.050513	48.077031
1879.870951	199.493649	48.082036
1876.559821	191.483063	48.087041
1872.966069	192.056078	48.092045
1869.813170	189.165171	48.097050
1866.702858	196.728179	48.102055
1862.493426	195.475944	48.107060
1859.076072	205.275896	48.112065
1855.124097	194.693095	48.117069
1851.934432	193.291858	48.122074
1848.831792	181.513685	48.127079
1845.022713	185.042966	48.132084
1841.480412	194.750381	48.137089
1838.068001	194.850951	48.142093
1834.070734	189.035994	48.147098
1830.779785	190.013255	48.152103
1827.537912	202.400361	48.157108
1824.083781	188.469936	48.162113
1820.563003	196.289596	48.167117
1816.831592	196.061230	48.172122
1813.437921	188.465507	48.177127
1809.935385	190.822778	48.182132
1806.479410	193.768016	48.187137
1802.851244	189.544961	48.192141
1799.478465	200.044009	48.197146
1796.251360	195.648635	48.202151
1792.211770	204.665991	48.207156
1789.407619	187.669342	48.212161
1785.425498	201.519741	48.217165
1782.013527	191.879969	48.222170
1778.212485	201.997377	48.227175
1774.955416	193.235683	48.232180
1771.462857	180.361767	48.237185
1767.942658	188.932864	48.242189
1764.164275	191.951146	48.247194
1760.809460	191.611839	48.252199
1757.146046	187.501858	48.257204
1754.159786	189.287034	48.262209
1750.581496	193.128490	48.267213
1747.158545	191.882200	48.272218
1743.632945	190.903419	48.277223
1740.090943	184.648892	48.282228
1736.518762	184.333625	48.287233
1733.041114	177.405265	48.292237
1729.244605	187.665768	48.297242
1725.902831	184.810829	48.302247
1722.132920	183.118293	48.307252
1718.915245	187.203706	48.312257
1715.548956	179.668140	48.317261
1711.834191	179.314855	48.322266
1708.383335	173.670060	48.327271
1704.836180	189.215329	48.332276
1701.475830	182.725956	48.337281
1697.807588	186.576062	48.342285
1694.433228	179.123225	48.347290
1691.353736	190.064101	48.352295
1687.306624	191.488289	48.357300
1683.780094	190.978377	48.362305
1680.360102	204.430548	48.367309
1676.877696	195.643939	48.372314
1673.501866	185.200194	48.377319
1669.963322	186.748625	48.382324
1666.386838	179.933286	48.387329
1662.975867	186.403610	48.392333
1659.357342	175.240818	48.397338
1655.794222	182.724915	48.402343
1652.303167	186.493323	48.407348
1648.646238	178.152237	48.412353
1645.562497	180.424100	48.417357
1641.795716	187.253337	48.422362
1638.651113	178.973717	48.427367
1634.685128	185.893241	48.432372
1631.445389	185.179474	48.437377
1627.855759	187.821402	48.442381
1624.405760	193.029549	48.447386
1621.147494	179.139546	48.452391
1617.076562	180.676317	48.457396
1614.004277	177.273259	48.462401
1609.992184	182.180949	48.467405
1606.527006	172.486836	48.472410
1603.378293	174.092109	48.477415
1599.570209	178.493802	48.482420
1596.369306	173.561307	48.487425
1592.865111	179.799430	48.492429
1588.721549	174.211400	48.497434
1586.260727	179.093848	48.502439
1582.519610	189.008584	48.507444
1579.045206	187.798588	48.512449
1575.145351	192.219091	48.517453
1571.570291	192.381747	48.522458
1568.522037	185.050264	48.527463
1564.618329	183.179437	48.532468
1561.528146	179.593404	48.537473
1557.881553	176.914928	48.542477
1554.526455	179.989238	48.547482
1550.824573	182.717499	48.552487
1546.921544	191.085609	48.557492
1543.473736	181.751888	48.562497
1540.131094	177.867483	48.567501
1536.608822	177.710405	48.572506
1533.494314	180.418687	48.577511
1529.883060	182.341819	48.582516
1526.423778	179.059788	48.587521
1522.865584	172.854722	48.592525
1519.512871	175.715176	48.597530
1515.955928	173.559173	48.602535
1511.980895	176.530422	48.607540
1508.706001	176.100015	48.612545
1505.086981	181.239724	48.617549
1501.489422	178.480382	48.622554
1498.365931	179.508977	48.627559
1494.626113	175.458318	48.632564
1491.434305	183.922353	48.637569
1487.806243	183.430479	48.642573
1483.683487	180.459902	48.647578
1480.985566	163.603371	48.652583
1477.231884	188.158510	48.657588
1474.401730	181.106466	48.662593
1470.320233	168.085889	48.667597
1466.619983	177.619151	48.672602
1462.652070	177.090748	48.677607
1459.854234	179.410798	48.682612
1456.537454	172.595043	48.687617
1452.701850	168.581330	48.692621
1449.041346	171.009329	48.697626
1445.832161	173.602167	48.702631
1442.240425	168.981273	48.707636
1438.669418	159.328313	48.712641
1434.900084	163.746871	48.717645
1431.605542	176.173852	48.722650
1428.261902	163.264639	48.727655
1424.481246	178.465572	48.732660
1421.662414	176.029663	48.737665
1417.900587	174.183548	48.742669
1414.486460	173.692708	48.747674
1410.647293	164.170635	48.752679
1406.848108	168.925300	48.757684
1403.665484	164.587309	48.762689
1400.034912	176.234794	48.767693
1396.534338	160.309851	48.772698
1393.148533	163.289562	48.777703
1389.146382	176.995436	48.782708
1386.002395	163.552948	48.787713
1382.469473	171.555111	48.792717
1379.063703	175.978209	48.797722
1375.955252	171.515725	48.802727
1371.922483	177.892876	48.807732
1368.811595	166.941353	48.812737
1365.505845	167.759382	48.817741
1361.849377	175.931205	48.822746
1358.443754	163.008296	48.827751
1354.401599	167.294553	48.832756
1350.998568	161.907136	48.837761
1347.562432	169.551914	48.842765
1344.107130	171.874376	48.847770
1340.569188	163.465313	48.852775
1337.180084	166.765910	48.857780
1333.469007	175.890928	48.862785
1329.922652	170.401992	48.867789
1326.318740	155.647959	48.872794
1323.274511	163.390137	48.877799
1319.845566	166.111934	48.882804
1315.951431	159.934920	48.887809
1312.451559	163.501519	48.892813
1309.200783	162.306543	48.897818
1306.417174	155.812860	48.902823
1302.185463	169.626006	48.907828
1298.417839	146.510095	48.912833
1294.592318	168.661493	48.917837
1291.362927	159.496582	48.922842
1288.058944	159.907331	48.927847
1284.536338	151.524087	48.932852
1281.295435	166.038747	48.937857
1277.711732	160.528386	48.942861
1273.630562	176.029843	48.947866
1270.607479	169.631732	48.952871
1266.573005	181.417464	48.957876
1263.430280	170.242978	48.962881
1260.245638	169.333943	48.967885
1256.448992	174.704526	48.972890
1253.182790	170.265282	48.977895
1249.905046	169.577698	48.982900
1246.413286	163.806738	48.987905
1242.598404	167.620596	48.992909
1238.915637	172.138409	48.997914
1235.625706	174.587519	49.002919
1231.827597	187.146038	49.007924
1228.591173	173.041075	49.012929
1225.164727	175.950431	49.017933
1221.263602	178.645947	49.022938
1217.953450	151.969498	49.027943
1214.057668	171.145629	49.032948
1211.033968	162.756816	49.037953
1207.796255	161.122322	49.042957
1204.015480	149.063368	49.047962
1200.327470	165.935780	49.052967
1197.216277	164.054204	49.057972
1193.471696	159.665552	49.062977
1190.077716	161.613753	49.067981
1186.253533	155.648716	49.072986
1183.051283	156.718663	49.077991
1179.233553	172.427532	49.082996
1175.596445	169.142096	49.088001
1172.778540	174.449504	49.093005
1169.053506	173.884629	49.098010
1165.318430	177.733001	49.103015
1161.759531	167.846975	49.108020
1158.487056	163.776878	49.113025
1154.802747	166.291129	49.118029
1151.095466	163.075989	49.123034
1147.822506	161.524191	49.128039
1144.414241	164.821626	49.133044
1140.932811	160.078819	49.138049
1137.673422	159.552511	49.143053
1133.701789	169.177769	49.148058
1130.857424	165.332957	49.153063
1127.259207	163.325737	49.158068
1123.650077	153.712022	49.163073
1119.787342	147.592597	49.168077
1116.423035	163.468316	49.173082
1112.912450	163.642267	49.178087
1109.360732	160.754338	49.183092
1106.047152	160.436163	49.188097
1102.206194	172.435653	49.193101
1098.755936	168.775030	49.198106
1095.374069	168.636725	49.203111
1091.771575	164.595793	49.208116
1088.526372	168.042718	49.213121
1085.056505	165.737227	49.218125
1081.635224	167.718003	49.223130
1077.949950	163.156857	49.228135
1074.213814	163.693310	49.233140
1070.794148	157.579682	49.238145
1067.296652	155.938527	49.243149
1063.740271	172.914548	49.248154
1060.256137	155.824940	49.253159
1056.393832	166.978603	49.258164
1053.107866	168.893944	49.263169
1049.670054	169.542744	49.268173
1046.352368	167.204355	49.273178
1043.271587	162.558819	49.278183
1039.323007	162.945793	49.283188
1035.856782	154.546386	49.288193
1032.589115	168.193982	49.293197
1028.987128	173.100162	49.298202
1025.388656	159.021672	49.303207
1021.956354	156.393153	49.308212
1018.422155	157.778217	49.313217
1014.984603	157.830660	49.318221
1011.418888	168.694871	49.323226
1007.814621	157.651396	49.328231
1003.841630	163.359988	49.333236
1000.673522	160.512660	49.338241
997.044216	156.098386	49.343245
993.548020	161.503441	49.348250
990.400934	156.702953	49.353255
986.812769	171.650207	49.358260
983.315330	161.774275	49.363265
980.046676	157.593550	49.368269
976.216298	168.294705	49.373274
973.116885	154.666757	49.378279
969.334908	165.179394	49.383284
965.592732	158.248007	49.388289
961.891999	157.374904	49.393293
958.547808	166.908288	49.398298
955.258586	152.484423	49.403303
951.470799	160.298601	49.408308
948.320629	165.234587	49.413313
944.861033	146.640374	49.418317
941.335719	155.455611	49.423322
937.962994	153.757621	49.428327
934.208745	166.675487	49.433332
930.873494	169.077666	49.438337
927.170429	161.721276	49.443341
923.526567	176.226535	49.448346
920.398585	150.702448	49.453351
917.021693	163.480868	49.458356
913.055337	160.170142	49.463361
909.633578	150.538057	49.468365
906.071410	162.253059	49.473370
902.906540	149.475960	49.478375
899.058247	156.508596	49.483380
895.782859	149.174739	49.488385
892.361253	146.812061	49.493389
888.626145	160.333371	49.498394
885.073868	131.790614	49.503399
881.546288	161.507223	49.508404
878.266141	142.644307	49.513409
874.576683	163.546375	49.518413
871.026415	149.357840	49.523418
868.037373	146.391638	49.528423
864.022343	164.744332	49.533428
860.750675	164.010854	49.538433
857.431602	164.086824	49.543437
853.293745	155.583771	49.548442
849.960255	150.446278	49.553447
846.409346	166.528003	49.558452
843.128282	158.319404	49.563457
839.762811	148.923802	49.568461
835.948749	154.567565	49.573466
832.715699	155.135114	49.578471
829.035701	154.760587	49.583476
825.808695	149.416809	49.588481
822.353827	165.225899	49.593485
818.519926	144.314776	49.598490
815.516426	160.328405	49.603495
811.709238	165.028067	49.608500
807.938473	169.990535	49.613505
804.765019	161.846262	49.618509
800.941603	157.307405	49.623514
797.683824	155.537236	49.628519
793.817303	156.232102	49.633524
790.804982	149.252614	49.638529
787.387487	160.118083	49.643533
783.410638	160.752748	49.648538
780.096344	156.655331	49.653543
776.694236	157.864813	49.658548
772.734748	151.934122	49.663553
769.340241	155.185659	49.668557
766.005080	151.346605	49.673562
762.800714	153.067979	49.678567
759.203243	159.116283	49.683572
755.766415	153.404706	49.688577
752.099784	167.103485	49.693581
748.401406	160.285648	49.698586
744.835485	161.256046	49.703591
741.110208	164.636012	49.708596
738.127090	180.277865	49.713601
734.383169	155.208986	49.718605
730.952278	142.194487	49.723610
727.765897	158.215849	49.728615
723.992240	147.590599	49.733620
720.488416	146.122523	49.738625
716.988318	154.705419	49.743629
713.294078	158.322258	49.748634
710.352920	151.279663	49.753639
706.692466	154.706650	49.758644
703.116232	152.801492	49.763649
699.813579	146.520194	49.768653
695.817624	152.073618	49.773658
692.438929	148.302562	49.778663
688.850651	154.233172	49.783668
685.456923	154.877442	49.788673
682.195827	144.952222	49.793677
678.301593	147.251215	49.798682
674.796526	147.991416	49.803687
671.067256	155.633096	49.808692
668.102811	135.442179	49.813697
664.514444	160.976813	49.818701
660.934820	147.179383	49.823706
657.557648	141.307577	49.828711
653.983872	147.466348	49.833716
650.593771	148.932073	49.838721
647.214999	145.301826	49.843725
643.414044	171.973792	49.848730
640.010375	143.769109	49.853735
636.393210	165.834318	49.858740
633.015426	150.514767	49.863745
629.716424	154.423182	49.868749
626.052191	150.596628	49.873754
622.232319	143.637952	49.878759
618.886622	158.033202	49.883764
615.415765	152.662830	49.888769
611.916160	150.309734	49.893773
608.327250	151.800325	49.898778
604.775098	146.703722	49.903783
600.945030	153.482140	49.908788
598.111453	143.058228	49.913793
594.805526	143.989610	49.918797
590.809313	153.204564	49.923802
587.756565	146.293419	49.928807
583.736576	163.504994	49.933812
580.369835	151.615434	49.938817
576.916787	151.493490	49.943821
573.022638	153.162857	49.948826
569.722490	140.428440	49.953831
566.457452	140.604046	49.958836
563.053160	129.578464	49.963841
559.642286	141.473397	49.968845
555.751578	149.750553	49.973850
552.359570	141.948640	49.978855
548.724965	148.023793	49.983860
545.157301	149.302761	49.988865
542.076209	157.951872	49.993869
538.375668	149.272348	49.998874
534.990621	148.290820	50.003879
531.229246	152.202357	50.008884
527.588657	144.239386	50.013889
524.450568	132.932607	50.018893
520.849367	147.715650	50.023898
517.455206	146.766020	50.028903
513.284411	146.505194	50.033908
510.004391	138.693984	50.038913
506.925200	149.890084	50.043917
502.982193	150.706955	50.048922
500.188908	135.414964	50.053927
496.559232	139.186384	50.058932
492.881114	129.613984	50.063937
489.706076	139.430537	50.068941
485.632361	153.937208	50.073946
482.522662	144.258581	50.078951
478.897579	148.204947	50.083956
475.343141	140.260730	50.088961
472.191165	137.607420	50.093965
468.188694	137.885157	50.098970
464.857749	140.450698	50.103975
461.212064	142.298185	50.108980
457.539032	154.874924	50.113985
454.095358	147.173541	50.118989
450.772090	150.872375	50.123994
447.199305	146.875059	50.128999
443.607944	148.180290	50.134004
440.222702	150.103045	50.139009
436.669808	134.910726	50.144013
433.391081	148.659678	50.149018
430.084412	142.085425	50.154023
426.620091	149.796505	50.159028
422.690220	150.938470	50.164033
419.363689	148.929190	50.169037
415.499695	153.689147	50.174042
411.984746	149.162717	50.179047
408.487316	152.701233	50.184052
405.100298	137.002398	50.189057
402.139404	141.194215	50.194061
398.131132	151.242172	50.199066
394.609771	155.196406	50.204071
391.293572	142.994000	50.209076
387.510273	152.539673	50.214081
384.347210	136.510773	50.219085
380.558327	144.956850	50.224090
377.427813	130.020932	50.229095
373.860280	138.946471	50.234100
370.380505	146.088462	50.239105
367.015490	135.394186	50.244109
363.049412	152.355644	50.249114
359.525165	142.181406	50.254119
356.141533	153.113562	50.259124
352.909180	144.277605	50.264129
349.196216	151.497986	50.269133
345.319414	149.940999	50.274138
342.204762	134.066605	50.279143
338.560083	149.970838	50.284148
335.347802	134.957003	50.289153
331.801204	141.371670	50.294157
328.011857	144.708872	50.299162
324.643475	132.336883	50.304167
320.711519	131.612242	50.309172
317.159325	146.316637	50.314177
314.004651	134.913287	50.319181
310.526621	139.934381	50.324186
307.305941	146.450884	50.329191
303.649935	138.601095	50.334196
300.242872	151.715192	50.339201
296.561265	143.592137	50.344205
293.043493	134.628177	50.349210
289.501513	139.519273	50.354215
286.239662	149.352621	50.359220
282.345668	154.158744	50.364225
279.196767	144.906756	50.369229
275.569541	156.240935	50.374234
272.205815	148.617705	50.379239
268.753053	147.404537	50.384244
265.024327	145.144635	50.389249
261.545000	144.314471	50.394253
257.812029	159.303280	50.399258
254.547815	137.540788	50.404263
251.085229	151.584955	50.409268
247.777697	145.147085	50.414273
244.250910	143.004961	50.419277
240.587188	138.597918	50.424282
237.099484	147.194070	50.429287
233.352257	142.416002	50.434292
229.974454	148.064453	50.439297
226.435978	151.996148	50.444301
222.893481	155.238566	50.449306
219.949133	152.831831	50.454311
216.137831	152.248510	50.459316
212.519263	152.295767	50.464321
209.119229	142.232209	50.469325
205.600544	151.123421	50.474330
202.121811	134.048259	50.479335
198.488462	146.354960	50.484340
195.167965	145.376957	50.489345
191.720197	139.881098	50.494349
187.617357	133.384383	50.499354
184.346152	141.052909	50.504359
180.825997	142.515502	50.509364
177.252565	137.950640	50.514369
173.976711	144.144662	50.519373
170.635568	142.952072	50.524378
167.094008	145.539835	50.529383
163.510468	152.873381	50.534388
160.340677	148.743851	50.539393
156.572891	138.374518	50.544397
152.851470	152.737016	50.549402
149.659722	133.461188	50.554407
145.836865	155.134072	50.559412
141.904421	139.172383	50.564417
138.548458	141.024260	50.569421
135.568377	145.585934	50.574426
132.589251	143.972199	50.579431
128.409624	141.557136	50.584436
124.540753	152.913552	50.589441
121.532311	138.652694	50.594445
117.903164	157.244974	50.599450
114.487627	140.010863	50.604455
110.841175	150.604385	50.609460
107.565664	150.334290	50.614465
104.376627	143.440605	50.619469
100.346561	139.869458	50.624474
97.049356	136.730036	50.629479
93.489170	133.302025	50.634484
89.688300	136.350942	50.639489
86.281603	130.119161	50.644493
82.726643	132.564268	50.649498
79.378554	144.247385	50.654503
75.623471	136.371602	50.659508
72.196836	138.026354	50.664513
69.048319	145.043214	50.669517
65.545402	155.815764	50.674522
62.265180	133.878106	50.679527
58.056609	140.427056	50.684532
54.657039	146.282894	50.689537
51.235777	139.467964	50.694541
47.883605	141.288187	50.699546
44.706369	131.322184	50.704551
40.837812	146.642542	50.709556
37.424876	139.318012	50.714561
33.911165	137.475515	50.719565
30.083098	133.445864	50.724570
27.172487	137.098310	50.729575
23.415333	143.855112	50.734580
19.888570	135.962649	50.739585
16.385634	132.585004	50.744589
12.693595	131.656858	50.749594
9.233737	135.756787	50.754599
5.836524	127.654215	50.759604
2.174404	134.886387	50.764609