Wed Jun 15 15:50:00 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.005283	87.834679	0.000000
0.356311	87.037876	0.005005
0.426958	86.157588	0.010010
0.276069	95.024831	0.015014
0.025571	63.712517	0.020019
-0.172811	71.615825	0.025024
-0.897908	47.602444	0.030029
-1.362171	47.372053	0.035034
-1.557202	47.482287	0.040038
-1.375304	40.833196	0.045043
-1.814197	37.346721	0.050048
-2.022280	33.567300	0.055053
-1.988551	30.412674	0.060058
-2.786518	12.713735	0.065062
-3.122139	12.356435	0.070067
-3.254899	16.466561	0.075072
-3.722483	21.437273	0.080077
-4.173157	15.341178	0.085082
-4.732382	7.088459	0.090086
-4.817133	4.344972	0.095091
-4.832976	9.454005	0.100096
-5.147177	8.470607	0.105101
-5.053752	5.537077	0.110106
-5.356032	20.872892	0.115110
-5.282263	8.701984	0.120115
-5.488124	17.872530	0.125120
-5.970181	3.204401	0.130125
-6.411010	9.066497	0.135130
-6.650024	13.621124	0.140134
-6.384818	-0.764067	0.145139
-7.066330	3.731595	0.150144
-8.058532	10.277083	0.155149
-8.272845	6.833604	0.160154
-8.434498	15.069762	0.165158
-8.357603	12.714171	0.170163
-8.462887	4.944580	0.175168
-8.648778	20.642527	0.180173
-8.491864	20.974066	0.185178
-8.772785	26.663746	0.190182
-9.254887	12.878010	0.195187
-9.762829	16.977238	0.200192
-10.006655	8.682361	0.205197
-10.109443	24.956584	0.210202
-9.988225	11.730403	0.215206
-10.524046	20.655790	0.220211
-11.140960	13.331693	0.225216
-11.305296	13.805497	0.230221
-11.103330	7.277302	0.235226
-11.644096	10.429125	0.240230
-11.871475	8.878169	0.245235
-12.059331	10.608968	0.250240
-12.638921	7.666803	0.255245
-12.781476	6.002197	0.260250
-12.823252	15.386224	0.265254
-12.734673	12.273464	0.270259
-13.599888	8.116515	0.275264
-14.065071	13.330090	0.280269
-14.088716	3.717903	0.285274
-14.499823	12.709583	0.290278
-14.357743	11.683631	0.295283
-14.475842	8.785649	0.300288
-14.546221	19.452569	0.305293
-15.267067	13.718372	0.310298
-15.761326	20.139552	0.315302
-15.866431	9.228626	0.320307
-15.874928	22.876188	0.325312
-16.324413	19.186284	0.330317
-16.061253	3.400646	0.335322
-16.501703	9.687451	0.340326
-16.947883	6.747508	0.345331
-17.448809	15.122793	0.350336
-17.936840	9.078155	0.355341
-17.468368	1.214932	0.360346
-17.840465	14.272789	0.365350
-17.722869	13.563297	0.370355
-18.526624	4.907970	0.375360
-19.033130	27.981147	0.380365
-18.891867	17.794605	0.385370
-19.009546	27.215744	0.390374
-19.120378	13.632634	0.395379
-20.097798	14.197304	0.400384
-20.883253	9.013483	0.405389
-20.356674	11.433144	0.410394
-20.317817	23.848873	0.415398
-20.880211	2.251273	0.420403
-21.077242	16.939140	0.425408
-21.183143	12.194549	0.430413
-20.735153	0.652431	0.435418
-21.453630	17.592947	0.440422
-22.225764	13.501309	0.445427
-22.332742	18.864425	0.450432
-22.750872	22.857071	0.455437
-22.627026	10.114025	0.460442
-22.769907	21.427915	0.465446
-22.868324	13.181611	0.470451
-23.559145	25.487488	0.475456
-24.100881	7.302110	0.480461
-24.366535	7.487446	0.485466
-24.452465	13.101985	0.490470
-24.295296	10.787187	0.495475
-24.080498	24.927974	0.500480
-24.777086	15.439815	0.505485
-25.316716	15.335523	0.510490
-25.690179	10.022850	0.515494
-25.841289	24.695736	0.520499
-25.530097	1.669983	0.525504
-26.132705	21.202330	0.530509
-26.850687	11.363173	0.535514
-27.311351	5.627317	0.540518
-27.460930	17.981848	0.545523
-27.339755	-1.912527	0.550528
-27.634785	26.001598	0.555533
-27.437773	19.277022	0.560538
-27.655238	21.125271	0.565542
-27.355227	6.082368	0.570547
-28.347669	12.050718	0.575552
-28.922616	20.546158	0.580557
-28.834894	15.043036	0.585562
-28.999714	11.797746	0.590566
-29.628056	20.613832	0.595571
-30.416769	19.793886	0.600576
-30.662717	18.435696	0.605581
-29.900525	-3.448761	0.610586
-30.574095	13.142321	0.615590
-30.884430	20.603225	0.620595
-30.920715	2.486240	0.625600
-31.237020	13.397105	0.630605
-31.152761	11.060028	0.635610
-31.444261	12.368682	0.640614
-32.120512	19.439143	0.645619
-32.369364	5.857938	0.650624
-32.526270	19.407896	0.655629
-32.467033	2.219568	0.660634
-33.058207	-0.173584	0.665638
-33.511428	3.943725	0.670643
-33.579561	-1.251998	0.675648
-34.028943	10.481966	0.680653
-34.221561	2.197375	0.685658
-34.375835	9.843094	0.690662
-34.145758	15.843400	0.695667
-34.047177	3.955067	0.700672
-35.092611	12.890091	0.705677
-35.179793	8.417435	0.710682
-35.435512	8.606161	0.715686
-35.961037	10.845353	0.720691
-36.038292	1.246271	0.725696
-36.263033	7.419793	0.730701
-36.603712	4.753720	0.735706
-37.251371	-0.449218	0.740710
-37.158858	-7.142110	0.745715
-37.105508	2.013109	0.750720
-37.199417	-2.817307	0.755725
-37.258860	4.403945	0.760730
-37.983858	15.340823	0.765734
-38.242315	12.808637	0.770739
-38.107594	7.554528	0.775744
-38.593357	19.908290	0.780749
-38.512864	9.202362	0.785754
-39.802067	18.361454	0.790758
-40.260774	11.473772	0.795763
-39.852517	4.580429	0.800768
-40.303690	18.572319	0.805773
-39.872687	9.190504	0.810778
-40.414952	2.920352	0.815782
-40.442565	13.717119	0.820787
-40.665780	6.237015	0.825792
-41.467962	15.989179	0.830797
-41.708226	2.207786	0.835802
-42.091741	13.939351	0.840806
-42.345336	6.927512	0.845811
-41.972493	12.755464	0.850816
-42.236598	27.263443	0.855821
-42.400746	7.991914	0.860826
-43.250892	7.613997	0.865830
-43.045116	8.686187	0.870835
-43.113118	7.934862	0.875840
-44.110716	0.113378	0.880845
-44.476352	10.822079	0.885850
-44.581578	10.036164	0.890854
-45.040928	1.903477	0.895859
-45.018585	0.320231	0.900864
-45.111915	3.892132	0.905869
-44.881045	4.352906	0.910874
-45.306100	17.801179	0.915878
-45.414206	3.952765	0.920883
-45.346572	8.249357	0.925888
-46.397044	8.614704	0.930893
-46.721095	12.281163	0.935898
-47.132724	20.423092	0.940902
-47.169346	16.093600	0.945907
-46.858124	5.755968	0.950912
-47.567890	18.615023	0.955917
-47.881641	12.274353	0.960922
-48.303382	21.991170	0.965926
-48.475043	14.433787	0.970931
-48.143203	2.269958	0.975936
-48.579184	10.542766	0.980941
-49.110787	-1.127873	0.985946
-49.750525	7.161048	0.990950
-49.888271	0.815463	0.995955
-49.960057	12.355727	1.000960
-50.257201	7.717223	1.005965
-50.178039	7.014772	1.010970
-50.332928	5.701020	1.015974
-50.454773	25.144151	1.020979
-50.886297	2.053718	1.025984
-51.578541	19.884425	1.030989
-51.273188	0.681313	1.035994
-51.952520	16.695181	1.040998
-52.055478	8.962201	1.046003
-51.919243	9.391856	1.051008
-52.665318	9.512663	1.056013
-53.065891	-2.911783	1.061018
-53.481223	22.054134	1.066022
-53.734154	12.303853	1.071027
-53.590862	16.107437	1.076032
-54.038252	29.857718	1.081037
-53.625120	7.854653	1.086042
-53.445078	18.644626	1.091046
-54.122780	20.052422	1.096051
-54.486472	4.828400	1.101056
-55.003971	12.261586	1.106061
-55.470305	5.162882	1.111066
-56.156830	4.283733	1.116070
-56.333366	10.200107	1.121075
-55.884939	6.330153	1.126080
-55.947713	12.533532	1.131085
-56.287702	2.007486	1.136090
-56.541692	8.576482	1.141094
-57.033177	0.903868	1.146099
-57.716138	1.349742	1.151104
-58.171854	4.711241	1.156109
-57.982547	12.325924	1.161114
-58.342889	10.582684	1.166118
-58.339339	0.064479	1.171123
-58.161661	4.516501	1.176128
-58.686766	3.028957	1.181133
-58.690235	3.784545	1.186138
-59.366201	4.512280	1.191142
-59.835316	11.236488	1.196147
-59.878079	-0.728508	1.201152
-60.032502	11.014220	1.206157
-59.961153	-0.877991	1.211162
-60.436318	6.063644	1.216166
-61.087527	-0.974613	1.221171
-61.327256	9.574286	1.226176
-61.755421	23.321384	1.231181
-61.628996	11.106365	1.236186
-61.958526	24.076696	1.241190
-61.819961	14.889205	1.246195
-61.755661	11.438451	1.251200
-62.531083	26.036158	1.256205
-62.955797	0.029499	1.261210
-62.962492	6.951618	1.266214
-63.233526	3.231541	1.271219
-63.071591	6.590301	1.276224
-64.212175	26.482048	1.281229
-64.303157	13.402610	1.286234
-64.710923	19.272465	1.291238
-64.783533	17.044274	1.296243
-64.495106	12.901565	1.301248
-64.762810	11.494197	1.306253
-64.464298	1.024215	1.311258
-65.294299	4.020628	1.316262
-65.746625	4.194003	1.321267
-65.864706	5.321588	1.326272
-66.898408	20.275078	1.331277
-66.595698	-3.594560	1.336282
-66.914737	-2.029708	1.341286
-67.857790	0.593072	1.346291
-67.786846	1.139464	1.351296
-67.845352	5.995905	1.356301
-67.574702	3.523953	1.361306
-67.953628	17.501237	1.366310
-67.863310	6.596989	1.371315
-67.948811	13.991433	1.376320
-68.947635	22.156224	1.381325
-68.802989	11.740468	1.386330
-69.340713	14.075887	1.391334
-69.610550	13.035048	1.396339
-69.730715	6.772084	1.401344
-70.858213	17.772425	1.406349
-70.906566	20.037622	1.411354
-70.422015	15.725677	1.416358
-70.828987	16.898541	1.421363
-71.123473	8.127985	1.426368
-71.145694	29.623172	1.431373
-71.292081	7.145856	1.436378
-71.956772	19.639967	1.441382
-72.645630	3.535704	1.446387
-72.754935	18.547129	1.451392
-73.008249	9.741950	1.456397
-72.938289	16.890523	1.461402
-73.174850	21.067226	1.466406
-73.514105	15.875960	1.471411
-73.016624	6.030275	1.476416
-73.316411	16.487103	1.481421
-73.914252	-1.642515	1.486426
-74.181206	18.214435	1.491430
-74.745325	22.846567	1.496435
-74.694140	10.806456	1.501440
-75.184344	11.503591	1.506445
-75.113063	4.821012	1.511450
-75.923213	10.428279	1.516454
-76.414514	9.277453	1.521459
-76.334620	4.570031	1.526464
-76.536775	-3.096435	1.531469
-76.439264	2.586723	1.536474
-76.783521	10.420488	1.541478
-76.485717	9.622518	1.546483
-77.603515	4.396566	1.551488
-77.697074	4.505618	1.556493
-77.810455	14.828453	1.561498
-78.012015	4.664648	1.566502
-78.070732	6.649624	1.571507
-78.565480	3.377778	1.576512
-79.378052	2.769335	1.581517
-79.517859	-6.008920	1.586522
-79.703739	9.944400	1.591526
-79.946593	11.200921	1.596531
-79.856328	1.007336	1.601536
-79.810821	15.151322	1.606541
-79.678371	11.052345	1.611546
-80.243210	-2.060136	1.616550
-81.042910	16.523240	1.621555
-81.079302	-3.166926	1.626560
-81.542374	12.074504	1.631565
-81.446595	-2.319373	1.636570
-81.265920	13.858065	1.641574
-82.175033	3.219811	1.646579
-82.607242	10.383899	1.651584
-82.850808	14.644522	1.656589
-82.980253	1.998198	1.661594
-82.817735	14.355692	1.666598
-83.290679	5.562252	1.671603
-83.699520	7.054448	1.676608
-84.483794	12.198832	1.681613
-84.501731	-2.525656	1.686618
-84.742050	5.450637	1.691622
-84.976404	18.455147	1.696627
-84.806422	8.630736	1.701632
-85.156953	14.807687	1.706637
-85.071286	17.649617	1.711642
-85.051976	14.261639	1.716646
-85.806928	21.340375	1.721651
-86.208893	5.711920	1.726656
-86.873656	18.722358	1.731661
-86.550332	7.682928	1.736666
-86.599878	4.728638	1.741670
-87.011480	1.467319	1.746675
-87.262195	4.740979	1.751680
-88.505263	4.656966	1.756685
-88.303462	5.756149	1.761690
-88.290704	4.941858	1.766694
-88.373909	-4.234023	1.771699
-88.048563	-3.317039	1.776704
-88.107948	14.390916	1.781709
-88.777579	9.214303	1.786714
-89.391748	1.844296	1.791718
-89.701152	9.014821	1.796723
-89.460071	2.701923	1.801728
-90.447006	17.659223	1.806733
-90.857864	6.251944	1.811738
-91.287418	10.067729	1.816742
-91.094100	12.186840	1.821747
-91.168436	11.632573	1.826752
-91.305945	16.968573	1.831757
-91.304123	11.626635	1.836762
-91.351754	7.690989	1.841766
-91.700876	13.990324	1.846771
-92.121713	14.191050	1.851776
-93.048789	3.686276	1.856781
-92.878810	14.314052	1.861786
-92.823925	-1.739994	1.866790
-93.632256	18.180187	1.871795
-93.856116	15.623149	1.876800
-94.698760	16.576418	1.881805
-94.202658	3.292145	1.886810
-94.464192	5.393306	1.891814
-94.389349	4.170716	1.896819
-94.641058	9.287949	1.901824
-94.784259	13.342681	1.906829
-95.533697	-3.850281	1.911834
-95.852212	6.274137	1.916838
-96.584739	12.052553	1.921843
-95.884436	-1.529639	1.926848
-96.320681	7.648390	1.931853
-96.238726	-8.186294	1.936858
-96.634024	15.347597	1.941862
-97.768260	9.338053	1.946867
-97.871338	5.667757	1.951872
-98.121246	13.816494	1.956877
-98.088763	27.227526	1.961882
-98.222673	14.332554	1.966886
-98.026342	13.793235	1.971891
-97.655488	13.816655	1.976896
-98.870155	18.124528	1.981901
-99.130452	10.051576	1.986906
-99.126454	22.508961	1.991910
-99.648891	15.893725	1.996915
-99.665206	18.498452	2.006912
-99.671463	16.400511	2.016909
-99.725947	12.800897	2.026906
-98.852394	20.940057	2.036902
-98.281480	13.941822	2.046899
-97.183502	5.637329	2.056896
-96.599894	9.178527	2.066893
-96.539445	6.510310	2.076890
-96.721703	15.350916	2.086886
-95.645258	6.400550	2.096883
-95.158647	6.804655	2.106880
-94.734678	9.625020	2.116877
-93.982285	6.457233	2.126874
-93.818894	7.532086	2.136870
-93.012828	20.029491	2.146867
-92.218135	19.037393	2.156864
-91.876520	20.857962	2.166861
-91.822414	19.481161	2.176858
-91.312633	15.202567	2.186854
-90.587368	9.630982	2.196851
-90.476273	15.370433	2.206848
-89.282322	13.282940	2.216845
-88.891970	12.966307	2.226842
-88.877399	12.597992	2.236838
-88.219323	9.620027	2.246835
-87.531431	10.760900	2.256832
-87.476197	16.478964	2.266829
-86.478050	10.220059	2.276826
-85.920470	12.444178	2.286822
-85.660561	11.488313	2.296819
-84.539252	16.289194	2.306816
-84.236838	7.269107	2.316813
-84.076346	8.269176	2.326810
-83.889980	11.037743	2.336806
-83.414115	8.728952	2.346803
-82.672247	12.781420	2.356800
-81.807365	0.742629	2.366797
-81.143139	9.612829	2.376794
-81.064309	3.589226	2.386790
-80.983464	10.037530	2.396787
-80.047694	15.761982	2.406784
-79.534110	10.415816	2.416781
-79.122585	13.423341	2.426778
-78.661031	13.933522	2.436774
-77.908404	24.282765	2.446771
-77.685975	14.192453	2.456768
-77.003479	15.092028	2.466765
-76.434649	11.519878	2.476762
-76.443230	10.699849	2.486758
-75.384151	10.968947	2.496755
-74.805037	3.187575	2.506752
-74.300063	5.469380	2.516749
-74.410244	9.260066	2.526746
-73.450532	5.972677	2.536742
-72.845264	4.188913	2.546739
-72.751905	5.446218	2.556736
-71.842877	-3.461063	2.566733
-71.436085	-5.578077	2.576730
-71.431753	-0.834592	2.586726
-70.626611	4.260337	2.596723
-69.848711	6.301565	2.606720
-69.639683	0.365885	2.616717
-68.916084	-0.301349	2.626714
-68.323172	0.335085	2.636710
-68.137429	-1.210148	2.646707
-67.854685	1.371120	2.656704
-66.666935	6.037358	2.666701
-66.640946	10.459812	2.676698
-66.167546	-5.486920	2.686694
-65.391070	9.627123	2.696691
-65.250530	7.430645	2.706688
-64.505498	-0.553863	2.716685
-63.692672	19.678516	2.726682
-63.405552	12.759185	2.736678
-63.806633	9.762373	2.746675
-62.352139	11.914914	2.756672
-62.133932	11.931939	2.766669
-61.474676	12.283315	2.776666
-60.722742	16.754699	2.786662
-60.634747	12.865146	2.796659
-60.108177	17.543072	2.806656
-59.360434	21.171432	2.816653
-59.221181	20.133079	2.826650
-58.427429	11.039492	2.836646
-57.586340	15.705738	2.846643
-57.623858	11.349089	2.856640
-57.242699	6.502080	2.866637
-56.195291	6.706439	2.876634
-55.887034	4.435227	2.886630
-55.615001	8.549443	2.896627
-55.354725	11.427880	2.906624
-54.340073	12.778381	2.916621
-53.896214	16.188497	2.926618
-53.686664	7.410242	2.936614
-52.850677	11.679078	2.946611
-52.329613	5.847889	2.956608
-52.307695	9.718283	2.966605
-51.423370	8.949519	2.976602
-51.079038	12.859379	2.986598
-50.631087	11.043931	2.996595
-49.631622	13.037089	3.006592
-49.195766	11.304041	3.016589
-48.896987	15.567826	3.026586
-48.853367	10.889497	3.036582
-48.037151	18.737281	3.046579
-47.505290	14.177092	3.056576
-46.845784	10.871659	3.066573
-46.023587	12.713655	3.076570
-45.904892	14.666482	3.086566
-45.893012	6.372879	3.096563
-45.117603	6.596708	3.106560
-44.406966	15.639707	3.116557
-44.095017	20.452964	3.126554
-42.973120	8.609240	3.136550
-43.002376	11.738901	3.146547
-42.611393	16.548874	3.156544
-42.146497	6.700786	3.166541
-41.183826	5.125633	3.176538
-40.964939	10.717781	3.186534
-40.736960	6.695852	3.196531
-40.088476	1.401180	3.206528
-39.757084	-0.660011	3.216525
-38.505217	6.568769	3.226522
-37.999279	5.151671	3.236518
-38.036614	15.557882	3.246515
-38.013136	10.503593	3.256512
-37.459978	9.260828	3.266509
-36.264419	10.901755	3.276506
-35.611106	10.642712	3.286502
-35.434741	7.992180	3.296499
-34.533414	16.493803	3.306496
-34.617585	9.653612	3.316493
-34.380787	4.930222	3.326490
-33.514012	2.235031	3.336486
-32.896031	7.817228	3.346483
-31.837535	8.418209	3.356480
-32.082454	6.435566	3.366477
-31.749298	5.245062	3.376474
-31.014350	12.118351	3.386470
-30.303984	17.019951	3.396467
-30.049442	14.076477	3.406464
-29.365364	13.346438	3.416461
-28.191628	20.602462	3.426458
-28.571645	21.745195	3.436454
-28.125903	15.999739	3.446451
-27.676035	13.611686	3.456448
-26.938010	7.203761	3.466445
-26.544605	5.838548	3.476442
-25.906844	11.908874	3.486438
-25.164620	8.115959	3.496435
-24.857144	11.435225	3.506432
-24.572933	1.974162	3.516429
-23.526536	2.893611	3.526426
-23.506203	7.569661	3.536422
-23.303923	14.984250	3.546419
-22.003259	10.260861	3.556416
-21.327683	-3.795093	3.566413
-21.173376	14.509918	3.576410
-21.324576	7.872424	3.586406
-20.846763	0.473649	3.596403
-19.994206	5.015327	3.606400
-19.646929	10.644338	3.616397
-18.388356	4.095078	3.626394
-18.496417	9.582925	3.636390
-18.449389	10.797614	3.646387
-17.192059	9.987361	3.656384
-17.089731	9.389911	3.666381
-16.146463	10.209556	3.676378
-15.395695	8.905393	3.686374
-15.567795	16.634514	3.696371
-15.198753	14.597818	3.706368
-14.536724	17.423695	3.716365
-13.704721	14.090646	3.726362
-13.713986	9.337691	3.736358
-12.709392	18.455981	3.746355
-12.149286	11.293694	3.756352
-12.131555	6.145830	3.766349
-11.693150	9.339154	3.776346
-10.719946	8.396684	3.786342
-10.400235	10.189072	3.796339
-9.591677	16.949454	3.806336
-9.105466	16.730573	3.816333
-8.978861	15.700929	3.826330
-8.777012	16.429454	3.836326
-7.870885	15.470412	3.846323
-7.568326	21.642661	3.856320
-6.934054	20.458598	3.866317
-6.107706	11.338093	3.876314
-5.908558	10.239174	3.886310
-5.620304	21.758786	3.896307
-4.840954	27.336255	3.906304
-4.704536	22.332042	3.916301
-4.116828	38.554644	3.926298
-3.511692	60.718802	3.936294
-3.153041	56.210883	3.946291
-2.556679	67.976230	3.956288
-1.997977	71.956716	3.966285
-1.704761	80.612511	3.976282
-1.423197	90.432058	3.986278
-0.818333	101.653859	3.996275
0.000000	123.062825	4.001280
-0.144603	128.323292	4.006285
0.309617	126.932051	4.011290
-0.227541	125.364998	4.016294
0.236177	119.336848	4.021299
0.130324	135.128719	4.026304
0.228177	123.091650	4.031309
0.623187	139.450150	4.036314
0.635879	134.588557	4.041318
0.129893	132.644746	4.046323
0.657159	135.558244	4.051328
0.271268	129.800707	4.056333
0.560810	131.809040	4.061338
0.079672	134.274904	4.066342
0.425911	137.053182	4.071347
0.636994	159.590893	4.076352
0.466192	144.257603	4.081357
0.767686	148.146452	4.086362
0.627509	147.979991	4.091366
0.721914	137.648601	4.096371
0.863097	131.763615	4.101376
0.253951	128.284045	4.106381
0.249756	126.938077	4.111386
0.322909	129.777168	4.116390
0.596289	148.597597	4.121395
0.749332	147.771066	4.126400
0.526310	159.745332	4.131405
0.847048	151.588210	4.136410
0.738236	152.033310	4.141414
0.496171	142.487315	4.146419
0.705293	152.482518	4.151424
0.928598	155.381932	4.156429
0.894399	139.848408	4.161434
0.356513	144.498236	4.166438
0.576309	149.355198	4.171443
1.174534	152.543050	4.176448
0.682094	153.741488	4.181453
0.782064	133.219586	4.186458
0.417300	156.378442	4.191462
0.748564	144.746894	4.196467
1.087887	160.564956	4.201472
0.655649	158.502120	4.206477
0.984323	154.632980	4.211482
1.139310	156.779068	4.216486
1.186272	133.414123	4.221491
1.120513	135.154254	4.226496
0.624387	131.701975	4.231501
0.949620	132.887609	4.236506
0.607196	134.671585	4.241510
0.799795	131.641344	4.246515
0.943349	132.558198	4.251520
0.710411	131.250919	4.256525
0.968261	123.547920	4.261530
0.905152	136.786148	4.266534
1.432923	144.215447	4.271539
1.234541	124.452925	4.276544
0.668267	135.491505	4.281549
0.979080	115.507826	4.286554
0.604651	129.322299	4.291558
1.092255	138.440861	4.296563
1.196937	141.004745	4.301568
0.890414	150.120979	4.306573
1.342407	137.714635	4.311578
0.979084	148.294120	4.316582
1.204277	137.458731	4.321587
1.021297	135.778496	4.326592
0.834731	134.414723	4.331597
1.217338	150.057724	4.336602
1.373883	157.359762	4.341606
1.186510	155.938115	4.346611
0.983346	150.458253	4.351616
1.207199	155.246085	4.356621
1.649693	157.233584	4.361626
0.867214	144.993455	4.366630
1.207897	142.919690	4.371635
1.301202	148.168371	4.376640
1.154162	156.641115	4.381645
1.470436	151.091196	4.386650
1.374656	156.738096	4.391654
0.953557	149.630953	4.396659
0.986276	148.967640	4.401664
1.311490	164.894380	4.406669
1.165330	158.280216	4.411674
1.139903	144.007433	4.416678
1.404540	153.208031	4.421683
1.324538	161.495882	4.426688
1.385817	160.097166	4.431693
1.573839	145.134188	4.436698
1.220082	151.613785	4.441702
1.210370	145.034294	4.446707
1.674583	154.254392	4.451712
1.191676	154.918656	4.456717
1.413367	155.627474	4.461722
1.203321	166.169804	4.466726
1.209927	147.500525	4.471731
1.463220	157.418195	4.476736
1.539016	155.612231	4.481741
1.386819	149.509569	4.486746
1.140357	169.332268	4.491750
1.547378	167.335333	4.496755
1.493040	163.765549	4.501760
1.526387	154.953153	4.506765
1.375740	160.094772	4.511770
1.391281	170.425417	4.516774
1.812669	183.602856	4.521779
1.813092	178.139453	4.526784
1.289994	171.253554	4.531789
1.799988	185.949337	4.536794
1.517978	188.308810	4.541798
1.749320	184.788979	4.546803
2.145528	188.623616	4.551808
1.606216	171.439797	4.556813
1.590171	162.303609	4.561818
1.360426	168.631223	4.566822
1.813500	164.663295	4.571827
2.008916	165.362546	4.576832
2.078440	174.500896	4.581837
1.885021	142.098995	4.586842
1.670123	153.117302	4.591846
1.856585	148.192560	4.596851
1.778333	149.031540	4.601856
1.544880	149.942335	4.606861
1.859377	136.051182	4.611866
1.656895	164.718835	4.616870
1.679481	157.819019	4.621875
1.890482	164.969022	4.626880
2.015115	170.728757	4.631885
2.059648	161.918848	4.636890
1.653840	154.989601	4.641894
2.018724	176.060483	4.646899
1.878157	164.329426	4.651904
1.946173	184.387535	4.656909
2.293000	173.486741	4.661914
2.017313	160.186928	4.666918
1.638909	161.471482	4.671923
1.966759	163.011225	4.676928
1.891507	171.138487	4.681933
2.216843	180.326703	4.686938
1.567063	169.959745	4.691942
2.389914	171.040460	4.696947
2.254160	177.602419	4.701952
1.907574	158.663884	4.706957
1.884983	160.403691	4.711962
1.886041	165.012306	4.716966
1.804452	171.866878	4.721971
2.196056	172.121164	4.726976
1.852615	182.959198	4.731981
2.257880	181.706554	4.736986
2.147982	178.040592	4.741990
2.039562	176.772315	4.746995
2.248314	177.095094	4.752000
2.041612	187.209445	4.757005
2.363243	173.384457	4.762010
2.250192	184.409730	4.767014
2.191836	181.329899	4.772019
2.453811	176.814979	4.777024
1.991815	176.977026	4.782029
2.428776	181.433015	4.787034
1.949252	175.210126	4.792038
2.093270	170.947410	4.797043
2.152958	187.792763	4.802048
2.073066	179.601211	4.807053
2.194073	178.380745	4.812058
1.906772	198.189414	4.817062
2.043566	178.806667	4.822067
2.320540	208.817176	4.827072
2.352287	201.789951	4.832077
2.666736	203.006671	4.837082
2.287057	191.667872	4.842086
2.419648	196.563824	4.847091
2.374045	188.232933	4.852096
2.333553	201.424667	4.857101
2.808436	210.313355	4.862106
2.469654	192.181908	4.867110
2.232021	197.664636	4.872115
2.497077	195.838144	4.877120
2.463587	209.455380	4.882125
2.601029	210.198543	4.887130
2.495822	216.856290	4.892134
2.467978	205.125415	4.897139
2.790948	207.665075	4.902144
2.457677	197.494978	4.907149
2.806513	205.780842	4.912154
2.709222	202.841700	4.917158
2.687286	191.915121	4.922163
2.324839	196.686707	4.927168
2.209357	196.842195	4.932173
2.527268	200.650315	4.937178
2.573588	213.280512	4.942182
2.601584	210.018901	4.947187
2.593382	234.574896	4.952192
2.774927	221.429517	4.957197
2.997595	225.458767	4.962202
2.757065	219.978248	4.967206
2.838112	228.929071	4.972211
3.045125	220.054200	4.977216
2.593317	218.691044	4.982221
2.825788	201.629624	4.987226
2.624102	226.529899	4.992230
3.023414	225.984259	4.997235
2.819367	216.720381	5.002240
2.613986	221.791951	5.007245
2.868809	215.002492	5.012250
2.905405	223.976047	5.017254
2.777573	221.413654	5.022259
3.064667	223.619305	5.027264
2.619824	224.015962	5.032269
2.880025	219.472025	5.037274
2.894354	223.803533	5.042278
2.690078	220.805023	5.047283
2.605878	218.501277	5.052288
2.598146	219.156072	5.057293
2.682568	205.081907	5.062298
2.680387	220.355701	5.067302
2.795356	220.767571	5.072307
3.083658	199.712733	5.077312
2.707299	216.446888	5.082317
2.796984	209.110492	5.087322
2.521532	236.553490	5.092326
3.055504	234.274743	5.097331
3.354444	252.115644	5.102336
3.263192	238.747206	5.107341
3.577215	231.176134	5.112346
3.262141	222.218949	5.117350
2.949023	214.455087	5.122355
3.130725	220.424408	5.127360
2.734128	217.605653	5.132365
2.570803	226.762685	5.137370
2.784825	232.215968	5.142374
3.135061	257.731505	5.147379
3.388162	242.517863	5.152384
3.042246	255.342933	5.157389
3.504771	252.894576	5.162394
3.273530	246.612081	5.167398
3.398345	245.059128	5.172403
3.281249	246.060988	5.177408
3.134287	241.458356	5.182413
3.726869	240.575658	5.187418
3.251612	237.157096	5.192422
3.153259	219.835244	5.197427
3.000474	224.855508	5.202432
3.090680	246.316357	5.207437
3.622235	242.904343	5.212442
3.359175	252.049166	5.217446
3.260016	254.178965	5.222451
3.350848	247.185361	5.227456
3.108134	257.327117	5.232461
3.362736	255.350131	5.237466
3.322716	250.073616	5.242470
3.421472	263.377441	5.247475
3.453240	258.877259	5.252480
3.437242	256.065838	5.257485
3.544011	260.585888	5.262490
3.436709	257.942361	5.267494
3.487995	260.171597	5.272499
3.563145	254.229606	5.277504
3.406876	252.054366	5.282509
3.706598	249.040828	5.287514
3.568389	259.642673	5.292518
3.446838	252.520408	5.297523
3.588440	260.077307	5.302528
3.605182	250.997006	5.307533
3.481374	259.929121	5.312538
3.688017	257.053779	5.317542
3.627315	245.693203	5.322547
3.554556	258.996661	5.327552
3.290804	260.395550	5.332557
3.402756	257.382557	5.337562
3.504267	259.314946	5.342566
3.171365	259.299105	5.347571
3.380494	243.382067	5.352576
3.489896	256.707013	5.357581
3.440570	243.621568	5.362586
3.497334	250.984236	5.367590
3.843283	260.928686	5.372595
3.990281	256.151694	5.377600
3.747253	264.370360	5.382605
4.039742	264.160512	5.387610
3.955698	247.865954	5.392614
3.631068	255.465075	5.397619
3.715852	252.676361	5.402624
3.768422	241.766535	5.407629
3.874336	246.143682	5.412634
3.908244	250.394720	5.417638
4.001577	248.407985	5.422643
3.872602	232.703188	5.427648
3.577548	254.501365	5.432653
4.032376	250.123143	5.437658
4.071797	259.615733	5.442662
3.741580	255.528434	5.447667
3.875228	249.869467	5.452672
3.686430	262.118023	5.457677
3.821866	274.378707	5.462682
3.851427	268.425798	5.467686
3.882814	269.460930	5.472691
3.864106	267.715356	5.477696
3.707030	273.479955	5.482701
4.235011	268.450794	5.487706
3.720328	271.352822	5.492710
3.982883	266.762709	5.497715
4.107018	266.721059	5.502720
4.042935	267.839147	5.507725
4.075983	259.480522	5.512730
4.038084	282.495783	5.517734
4.063383	268.286613	5.522739
4.092491	270.375883	5.527744
4.076348	266.822846	5.532749
4.160656	258.200744	5.537754
4.040799	256.507105	5.542758
3.809964	278.075605	5.547763
4.047381	265.195099	5.552768
3.847995	266.459449	5.557773
4.079111	262.327526	5.562778
4.140562	261.469069	5.567782
4.442630	271.534617	5.572787
4.216723	273.321254	5.577792
3.936526	283.482341	5.582797
4.384267	282.167426	5.587802
4.709598	290.089262	5.592806
4.576347	277.346453	5.597811
4.473574	266.719062	5.602816
4.166889	272.715052	5.607821
4.240712	252.951378	5.612826
4.242552	271.408528	5.617830
4.094807	257.436408	5.622835
4.358201	265.168407	5.627840
4.303961	268.004999	5.632845
4.331104	284.905951	5.637850
4.330876	284.586342	5.642854
4.313872	303.288727	5.647859
4.527905	286.179061	5.652864
4.358132	306.223060	5.657869
4.850927	291.019577	5.662874
4.798056	287.622551	5.667878
4.361382	278.834781	5.672883
4.442238	260.570278	5.677888
3.925057	269.974625	5.682893
4.289877	286.510118	5.687898
4.752441	288.646138	5.692902
4.600291	293.820802	5.697907
4.578969	295.077727	5.702912
4.387620	300.955034	5.707917
4.857882	303.261531	5.712922
4.850973	296.432818	5.717926
4.813023	299.693970	5.722931
4.564533	276.045976	5.727936
4.019109	281.545170	5.732941
4.210217	287.016959	5.737946
4.588418	279.921594	5.742950
4.820432	293.140782	5.747955
4.572494	284.488437	5.752960
4.748632	301.767862	5.757965
4.973844	296.188943	5.762970
4.778177	298.052858	5.767974
4.965607	298.224088	5.772979
5.104598	297.104616	5.777984
4.874564	301.942839	5.782989
4.995969	284.930163	5.787994
4.715183	268.794661	5.792998
4.622472	272.028850	5.798003
4.586845	266.492158	5.803008
4.669214	291.672321	5.808013
4.847789	290.707796	5.813018
4.751561	303.747242	5.818022
4.447610	294.245117	5.823027
5.026733	300.487651	5.828032
4.620621	305.362668	5.833037
4.768162	295.766398	5.838042
4.406170	314.554219	5.843046
4.242303	307.898919	5.848051
4.320896	305.375103	5.853056
4.755998	327.689597	5.858061
5.120070	320.893283	5.863066
5.090630	325.494853	5.868070
4.831868	330.682314	5.873075
5.210534	328.641412	5.878080
5.008401	334.225553	5.883085
5.180032	316.915501	5.888090
5.139134	328.001954	5.893094
5.029216	315.406585	5.898099
5.085937	320.755876	5.903104
5.026410	335.120350	5.908109
5.150127	335.874075	5.913114
4.980910	323.248743	5.918118
5.079181	329.293253	5.923123
5.604837	332.910224	5.928128
4.945965	310.393723	5.933133
4.865688	294.147719	5.938138
5.055540	324.552748	5.943142
5.219958	320.410523	5.948147
5.752568	321.167603	5.953152
5.192547	314.394280	5.958157
5.249783	304.731050	5.963162
5.142978	290.937791	5.968166
5.100361	301.430645	5.973171
5.265263	278.482804	5.978176
4.652742	312.237722	5.983181
5.005968	311.160186	5.988186
5.488435	317.204533	5.993190
5.416919	321.427734	5.998195
5.471666	310.257856	6.003200
5.427758	327.663839	6.008205
5.526545	308.298849	6.013210
5.422498	331.105720	6.018214
5.150639	308.801384	6.023219
5.077010	307.749700	6.028224
5.107887	317.713403	6.033229
5.426300	315.970020	6.038234
5.589088	311.419859	6.043238
5.275763	318.516699	6.048243
5.205617	314.108217	6.053248
5.426424	330.875212	6.058253
5.370783	305.448926	6.063258
5.347163	311.305326	6.068262
5.015112	304.557370	6.073267
5.344817	299.617194	6.078272
5.394960	321.650716	6.083277
5.476754	301.164837	6.088282
4.967757	300.404692	6.093286
5.055852	316.908608	6.098291
5.371631	319.796521	6.103296
5.281360	323.650127	6.108301
5.450125	319.158066	6.113306
5.360751	320.213158	6.118310
5.327002	333.261739	6.123315
5.521300	331.023327	6.128320
5.282174	319.093680	6.133325
5.219481	302.912236	6.138330
5.202463	311.719699	6.143334
5.220621	327.042622	6.148339
5.336443	326.004317	6.153344
5.067937	332.041964	6.158349
5.327702	317.928460	6.163354
5.354820	330.069868	6.168358
5.303876	330.790308	6.173363
5.593827	321.156381	6.178368
5.344961	313.107311	6.183373
5.423034	321.448933	6.188378
5.079590	301.417562	6.193382
5.316975	337.364628	6.198387
5.604503	322.126770	6.203392
4.935935	313.821813	6.208397
4.997206	307.799921	6.213402
5.151279	316.293131	6.218406
5.077200	318.962447	6.223411
5.487774	325.508864	6.228416
5.355376	319.146475	6.233421
5.629639	323.368369	6.238426
5.296418	322.069063	6.243430
5.125985	318.004962	6.248435
5.531511	318.286348	6.253440
5.167888	324.831474	6.258445
5.559577	324.968457	6.263450
5.383508	318.567709	6.268454
5.201995	310.181082	6.273459
5.474404	310.652859	6.278464
4.969916	306.259433	6.283469
5.130297	301.356215	6.288474
5.327771	317.654822	6.293478
4.982755	315.677678	6.298483
5.429459	327.131121	6.303488
5.123583	328.220216	6.308493
5.524849	319.125458	6.313498
5.278000	328.491678	6.318502
5.470805	316.681637	6.323507
5.656240	327.711057	6.328512
5.211915	330.192768	6.333517
5.043528	314.073072	6.338522
5.209608	327.081818	6.343526
5.296585	340.802968	6.348531
5.566025	322.424755	6.353536
5.301878	343.447900	6.358541
5.394461	326.445859	6.363546
5.150709	322.483348	6.368550
5.295630	339.246814	6.373555
5.533980	322.396382	6.378560
4.916224	338.974647	6.383565
5.179808	324.831798	6.388570
5.444707	331.246229	6.393574
5.152782	334.065388	6.398579
5.173745	324.348359	6.403584
5.127132	333.538353	6.408589
5.388158	329.668313	6.413594
5.595966	330.149089	6.418598
5.222394	340.893171	6.423603
5.434703	333.114827	6.428608
5.180300	334.576101	6.433613
5.478333	322.611151	6.438618
5.286450	332.175748	6.443622
5.227939	338.443369	6.448627
5.748555	322.189778	6.453632
4.961851	330.079560	6.458637
5.269509	327.518775	6.463642
5.358327	337.331059	6.468646
5.453291	338.469826	6.473651
5.117457	319.382131	6.478656
5.074530	327.786072	6.483661
5.559605	324.601610	6.488666
5.434092	328.277850	6.493670
5.349275	336.503456	6.498675
5.579863	325.977491	6.503680
5.189018	313.635709	6.508685
5.189446	305.446403	6.513690
5.166336	303.334087	6.518694
5.238673	319.566071	6.523699
5.174785	323.267443	6.528704
5.170510	342.513892	6.533709
5.388714	335.237582	6.538714
5.350725	335.040618	6.543718
5.326618	341.155470	6.548723
5.345640	331.980535	6.553728
5.343129	335.919967	6.558733
5.343183	336.133409	6.563738
5.490251	337.808402	6.568742
5.016491	329.395777	6.573747
5.743738	327.745234	6.578752
5.289728	315.955174	6.583757
5.285204	304.872534	6.588762
5.196515	305.690460	6.593766
4.900546	309.521332	6.598771
5.157363	316.026566	6.603776
5.213285	321.146631	6.608781
5.374122	340.180332	6.613786
5.339399	327.998294	6.618790
5.338500	348.046205	6.623795
5.521211	328.181081	6.628800
5.271304	337.222666	6.633805
5.371829	319.701119	6.638810
5.275174	322.674157	6.643814
5.262079	319.140630	6.648819
5.467446	332.915504	6.653824
5.165652	324.141426	6.658829
5.349465	326.275770	6.663834
5.275145	330.429396	6.668838
5.147005	330.570207	6.673843
5.250910	329.997520	6.678848
5.601249	343.530630	6.683853
5.760349	320.099221	6.688858
5.164221	323.416218	6.693862
4.901847	309.608895	6.698867
5.319532	308.418902	6.703872
5.285657	321.978789	6.708877
5.637174	306.699889	6.713882
5.462328	314.118422	6.718886
5.065947	300.410297	6.723891
5.354671	294.393734	6.728896
5.132439	310.120773	6.733901
5.205889	303.397451	6.738906
5.395414	299.434766	6.743910
5.285099	307.751875	6.748915
5.374271	302.154495	6.753920
5.027202	315.441678	6.758925
5.621815	318.685604	6.763930
5.228829	314.867812	6.768934
5.090465	306.191033	6.773939
5.334922	316.550436	6.778944
5.150392	320.891849	6.783949
5.399809	337.008567	6.788954
5.830798	326.698276	6.793958
5.189669	314.878766	6.798963
5.043502	303.954091	6.803968
5.277181	306.654030	6.808973
5.250504	298.113086	6.813978
5.011547	314.233836	6.818982
5.320559	316.179293	6.823987
5.657102	327.746433	6.828992
5.532498	343.479667	6.833997
5.425059	310.015846	6.839002
5.314677	307.238954	6.844006
5.066995	306.034323	6.849011
5.078375	293.725526	6.854016
5.065408	312.707417	6.859021
5.211429	318.207186	6.864026
5.289273	320.338523	6.869030
5.187862	322.839623	6.874035
5.587746	318.077051	6.879040
5.739451	327.279450	6.884045
5.375645	299.717354	6.889050
5.275827	298.366556	6.894054
5.302525	282.037680	6.899059
5.099159	296.047472	6.904064
5.108966	292.517566	6.909069
5.392218	307.746449	6.914074
5.537321	307.281288	6.919078
5.090950	292.073983	6.924083
5.222559	295.901964	6.929088
5.161056	304.783659	6.934093
5.625603	322.948070	6.939098
5.367151	300.797592	6.944102
5.035255	310.767083	6.949107
5.476910	290.689737	6.954112
4.864225	295.268219	6.959117
5.041479	318.533763	6.964122
5.226888	312.171635	6.969126
5.460537	329.790705	6.974131
6.072193	321.927333	6.979136
5.107166	317.099109	6.984141
5.138655	313.183253	6.989146
5.249106	305.889053	6.994150
5.305197	325.786648	6.999155
5.296984	317.575186	7.004160
5.378907	332.236692	7.009165
5.470231	327.377136	7.014170
5.617245	300.508962	7.019174
4.942727	294.343599	7.024179
5.216686	288.948202	7.029184
5.343773	293.390917	7.034189
5.096659	294.363561	7.039194
5.346306	313.011930	7.044198
5.559153	307.296744	7.049203
5.018371	315.515219	7.054208
5.030940	303.802746	7.059213
5.585300	324.377196	7.064218
5.429869	307.976584	7.069222
5.447258	316.146816	7.074227
5.021898	299.491225	7.079232
5.051912	309.322482	7.084237
5.154067	311.081348	7.089242
5.479867	320.533950	7.094246
5.378148	323.182482	7.099251
5.452486	310.635093	7.104256
5.400885	325.944090	7.109261
5.580570	313.062233	7.114266
5.114965	299.491129	7.119270
5.004754	296.775471	7.124275
5.431285	311.288365	7.129280
5.052817	322.095194	7.134285
5.164358	323.384718	7.139290
5.450975	319.601997	7.144294
5.231011	337.009661	7.149299
5.369096	322.868810	7.154304
5.065439	335.310322	7.159309
5.351564	338.348647	7.164314
5.353800	333.815935	7.169318
5.164493	332.280652	7.174323
5.413318	329.625021	7.179328
5.034340	334.488855	7.184333
5.199875	330.251641	7.189338
5.555572	330.388554	7.194342
5.468450	333.950037	7.199347
5.637856	335.842311	7.204352
5.481946	336.159952	7.209357
5.595774	315.273573	7.214362
5.132605	300.411347	7.219366
4.867336	307.462162	7.224371
5.362135	307.454749	7.229376
5.465684	321.972986	7.234381
5.401074	315.732966	7.239386
5.183929	296.565707	7.244390
4.980628	298.642781	7.249395
5.415270	312.379550	7.254400
5.320396	323.688100	7.259405
5.253274	328.131549	7.264410
5.351319	323.002164	7.269414
5.451516	337.482102	7.274419
5.409310	319.685828	7.279424
5.252581	320.765467	7.284429
5.216951	302.439863	7.289434
5.375620	318.042013	7.294438
4.926054	313.754138	7.299443
5.038501	317.509924	7.304448
5.405881	321.054201	7.309453
5.491580	319.119325	7.314458
5.490991	336.139546	7.319462
5.314109	329.370968	7.324467
5.314131	319.877684	7.329472
5.099687	320.127164	7.334477
5.206607	326.658555	7.339482
5.660401	319.695200	7.344486
4.953054	322.331355	7.349491
5.287557	311.239346	7.354496
5.216961	332.780456	7.359501
5.485217	318.275985	7.364506
5.649548	329.776586	7.369510
5.334104	326.172079	7.374515
5.365202	300.938234	7.379520
4.926665	308.726077	7.384525
5.125461	312.305118	7.389530
5.303343	316.708075	7.394534
5.128263	327.679285	7.399539
5.609559	330.860752	7.404544
5.458010	327.448654	7.409549
5.403461	315.720627	7.414554
5.330995	312.906591	7.419558
5.253026	317.952600	7.424563
5.150806	297.531760	7.429568
5.133455	314.840413	7.434573
5.483670	327.920831	7.439578
5.476755	330.377215	7.444582
5.443138	318.437875	7.449587
5.537727	299.194730	7.454592
5.294358	309.686337	7.459597
5.072012	287.685579	7.464602
5.465735	307.289118	7.469606
5.447176	301.639205	7.474611
5.463533	295.542763	7.479616
5.158109	306.502253	7.484621
5.338728	303.239767	7.489626
5.730632	298.892350	7.494630
5.145790	314.217443	7.499635
5.656637	301.729918	7.504640
5.423859	305.449429	7.509645
5.109036	315.616556	7.514650
5.131859	299.242529	7.519654
5.260062	313.509174	7.524659
5.735289	311.011949	7.529664
5.498939	308.630147	7.534669
5.031570	307.486778	7.539674
5.217174	306.745416	7.544678
5.059557	310.770452	7.549683
5.430745	301.827365	7.554688
5.219212	315.737213	7.559693
5.239996	299.093916	7.564698
5.419268	296.753425	7.569702
5.209362	304.359950	7.574707
5.393679	303.009548	7.579712
5.052739	312.129593	7.584717
5.233548	300.742185	7.589722
5.495412	297.521615	7.594726
5.188655	294.669354	7.599731
5.152669	297.833111	7.604736
5.177499	307.363162	7.609741
5.125152	303.014088	7.614746
5.492989	303.307423	7.619750
5.442057	318.721364	7.624755
5.594766	298.576734	7.629760
5.574802	317.285840	7.634765
5.574308	301.857462	7.639770
5.474632	311.325226	7.644774
5.338716	302.299125	7.649779
5.288762	297.521424	7.654784
5.336768	313.356614	7.659789
5.508131	295.172110	7.664794
5.124844	306.564414	7.669798
5.077187	305.822930	7.674803
5.314177	300.467869	7.679808
5.489707	301.558497	7.684813
5.289204	294.437717	7.689818
5.548675	302.518909	7.694822
5.339202	303.871641	7.699827
5.791449	298.771429	7.704832
5.312377	292.171283	7.709837
4.983694	276.002355	7.714842
5.200929	291.464583	7.719846
5.133270	294.162231	7.724851
5.414302	301.879398	7.729856
5.180240	296.349938	7.734861
5.342934	301.694830	7.739866
5.474942	291.645868	7.744870
5.497083	301.572433	7.749875
5.300665	292.260095	7.754880
5.278959	288.340803	7.759885
5.161819	300.121693	7.764890
5.302006	298.309610	7.769894
5.176982	303.964553	7.774899
5.296737	296.647611	7.779904
5.420132	315.959837	7.784909
5.475260	306.931363	7.789914
5.352368	297.041813	7.794918
5.454005	308.380617	7.799923
5.317612	281.525375	7.804928
4.953134	280.891393	7.809933
5.201392	296.205262	7.814938
5.260483	305.480266	7.819942
5.510696	303.280956	7.824947
5.550424	311.028830	7.829952
5.297064	312.988796	7.834957
5.284062	292.523822	7.839962
5.188501	278.006511	7.844966
5.432512	294.159196	7.849971
5.356233	278.091496	7.854976
5.397610	286.859109	7.859981
4.986407	277.060918	7.864986
5.083835	280.223636	7.869990
5.426299	298.329471	7.874995
5.703217	293.729183	7.880000
5.158161	284.595605	7.885005
5.407007	268.953518	7.890010
5.242095	277.473477	7.895014
4.591888	282.293431	7.900019
5.381081	280.493858	7.905024
5.655885	302.444946	7.910029
5.134842	297.387592	7.915034
5.407531	304.472027	7.920038
5.426067	318.581699	7.925043
5.436777	291.614826	7.930048
5.160119	295.931997	7.935053
4.874614	299.421885	7.940058
5.337414	302.158736	7.945062
5.107174	307.470508	7.950067
5.330314	303.110237	7.955072
5.656442	299.272063	7.960077
5.509761	290.884820	7.965082
5.233426	300.469568	7.970086
5.050292	295.978451	7.975091
5.695389	301.411524	7.980096
5.629643	297.373435	7.985101
5.285884	275.580683	7.990106
5.590516	260.973184	7.995110
4.756465	269.918207	8.000115
5.184713	253.703478	8.005133
4.881418	283.175935	8.010150
5.427214	280.881039	8.015168
5.253868	300.410423	8.020186
5.225123	304.706136	8.025203
5.125801	289.602577	8.030221
5.432201	300.853479	8.035238
5.207398	302.001504	8.040256
5.563065	304.804281	8.045274
5.130026	312.323773	8.050291
5.281066	300.556795	8.055309
5.083491	316.280771	8.060326
5.274046	302.546604	8.065344
5.276792	305.547131	8.070362
5.007208	312.016186	8.075379
5.383910	303.364649	8.080397
5.160435	308.721775	8.085414
5.231212	301.003219	8.090432
5.508784	304.092051	8.095450
5.252206	311.432818	8.100467
5.540290	300.188115	8.105485
5.228265	306.677760	8.110502
5.297652	298.512811	8.115520
5.586567	292.071710	8.120538
5.427151	297.194196	8.125555
5.322730	302.577499	8.130573
5.468378	295.470310	8.135590
5.076250	307.682077	8.140608
5.135892	308.219775	8.145626
5.147616	316.599950	8.150643
5.513461	329.981774	8.155661
5.652352	333.272809	8.160678
5.494067	331.896882	8.165696
5.359532	329.787909	8.170714
5.394334	341.165294	8.175731
5.546041	333.172891	8.180749
5.722880	329.373954	8.185766
5.595120	324.975639	8.190784
5.541819	321.973672	8.195802
5.401357	308.586540	8.200819
5.492709	324.407913	8.205837
5.499985	324.372936	8.210854
5.682636	320.381757	8.215872
5.542500	328.034986	8.220890
5.413880	308.191744	8.225907
5.314078	325.557953	8.230925
5.689927	334.629422	8.235942
5.642918	324.167723	8.240960
5.512095	340.202844	8.245978
5.661272	333.490710	8.250995
5.460841	331.051090	8.256013
5.777524	328.635924	8.261030
5.384275	320.372467	8.266048
5.585655	322.616954	8.271066
5.648978	336.083117	8.276083
5.649593	329.391500	8.281101
5.749052	333.088543	8.286118
5.482984	317.321666	8.291136
5.619955	296.882246	8.296154
5.166741	319.657375	8.301171
5.435956	314.031985	8.306189
5.865108	335.817766	8.311206
5.655364	331.536216	8.316224
5.841596	338.547791	8.321242
5.582556	338.612123	8.326259
5.822148	332.250297	8.331277
5.671663	327.350764	8.336294
5.522157	308.046253	8.341312
5.886100	317.292268	8.346330
5.615072	318.610878	8.351347
5.527888	308.085673	8.356365
5.560372	313.563545	8.361382
5.766831	326.139562	8.366400
6.012600	320.946858	8.371418
5.331639	317.761886	8.376435
5.503330	327.186387	8.381453
5.687505	317.534376	8.386470
5.664608	325.730568	8.391488
5.944432	330.831842	8.396506
5.526663	338.024212	8.401523
5.624659	330.698667	8.406541
6.138687	338.095808	8.411558
5.979156	337.172123	8.416576
5.701022	305.710074	8.421594
5.746835	308.857870	8.426611
5.574347	307.467663	8.431629
5.707924	305.410520	8.436646
5.530450	324.813686	8.441664
5.890640	325.548989	8.446682
5.971071	315.965290	8.451699
5.609228	325.037632	8.456717
5.724679	329.069828	8.461734
5.581609	321.070255	8.466752
5.864949	332.966441	8.471770
5.949417	333.536444	8.476787
5.955617	319.818657	8.481805
5.949637	315.622696	8.486822
5.476277	313.570111	8.491840
5.765276	309.871409	8.496858
5.908273	336.931029	8.501875
5.684656	321.127515	8.506893
5.854732	311.623170	8.511910
5.880713	334.612060	8.516928
6.276544	331.594219	8.521946
5.746445	328.094142	8.526963
5.700579	309.838436	8.531981
5.971476	310.758328	8.536998
5.657800	319.908313	8.542016
6.051357	320.652861	8.547034
6.052776	328.217756	8.552051
5.773876	325.989275	8.557069
5.891460	318.973500	8.562087
5.881424	323.476401	8.567104
5.791075	313.119974	8.572122
5.869619	318.039411	8.577139
5.912860	331.146197	8.582157
6.258048	313.936765	8.587175
5.955491	316.288243	8.592192
5.703705	306.477051	8.597210
5.735569	302.686630	8.602227
5.935643	318.554776	8.607245
6.107846	314.442919	8.612263
5.944465	321.424885	8.617280
6.177956	318.405831	8.622298
6.012758	322.398897	8.627315
5.855874	302.151297	8.632333
5.922067	306.642679	8.637351
6.004544	321.235161	8.642368
6.307942	319.649218	8.647386
6.327631	311.654634	8.652403
5.764296	295.662770	8.657421
5.553406	297.424459	8.662439
5.684982	313.713152	8.667456
6.318178	316.816720	8.672474
6.246130	334.881695	8.677491
5.902509	326.712267	8.682509
6.180490	323.280366	8.687527
5.974346	313.862496	8.692544
6.102102	308.821149	8.697562
6.122183	302.783913	8.702579
5.705765	302.188328	8.707597
5.818011	308.363541	8.712615
5.986194	317.359901	8.717632
6.092375	312.627543	8.722650
5.969784	326.079649	8.727667
6.203148	316.394320	8.732685
6.206719	310.647227	8.737703
6.211477	329.900437	8.742720
5.915743	314.417126	8.747738
6.000464	320.027667	8.752755
5.749661	320.370478	8.757773
6.464609	334.398940	8.762791
6.298787	315.409231	8.767808
6.229021	330.174968	8.772826
6.154668	317.116570	8.777843
6.159993	332.640545	8.782861
6.293122	327.913470	8.787879
6.208659	324.111764	8.792896
6.123873	318.885522	8.797914
6.311234	314.456684	8.802931
6.159646	317.449067	8.807949
5.839618	311.817735	8.812967
5.994270	326.001558	8.817984
6.347913	312.092738	8.823002
6.321004	324.134943	8.828019
6.220435	313.632117	8.833037
6.570949	306.537905	8.838055
6.291891	320.021079	8.843072
6.224907	303.614994	8.848090
6.209085	307.949801	8.853107
6.043681	319.273568	8.858125
6.388385	316.836062	8.863143
5.984408	335.033131	8.868160
6.032016	325.571647	8.873178
6.237090	320.146956	8.878195
6.002635	335.281154	8.883213
6.221284	312.956998	8.888231
6.293201	324.567244	8.893248
6.218792	327.864401	8.898266
6.242551	327.740308	8.903283
6.135406	332.784011	8.908301
6.243591	321.824066	8.913319
6.363381	329.332304	8.918336
6.396082	325.228936	8.923354
5.996922	321.931567	8.928371
5.800040	335.647855	8.933389
6.092076	318.735505	8.938407
5.928114	325.641803	8.943424
6.162783	323.867964	8.948442
6.239795	343.233034	8.953459
6.303681	345.158317	8.958477
6.544277	350.037799	8.963495
6.733810	359.067750	8.968512
6.338963	338.706714	8.973530
6.382786	319.666907	8.978547
6.220966	340.395667	8.983565
6.287251	309.653834	8.988583
6.234628	341.514497	8.993600
6.707276	345.732186	8.998618
6.827351	328.562300	9.003635
6.426827	321.109163	9.008653
6.588633	320.468107	9.013671
6.618979	312.117433	9.018688
6.194098	311.581202	9.023706
6.554874	308.080127	9.028723
6.536953	299.644353	9.033741
6.580644	312.867944	9.038759
6.403757	320.533245	9.043776
6.728649	310.309815	9.048794
6.486714	316.994514	9.053811
6.335385	316.563920	9.058829
6.453930	308.412194	9.063847
6.349541	329.537435	9.068864
6.366672	313.773452	9.073882
6.527886	315.145006	9.078899
6.317265	315.221902	9.083917
6.483847	326.006206	9.088935
6.445392	323.160500	9.093952
6.470516	313.789721	9.098970
6.165238	320.901405	9.103987
6.231158	325.009876	9.109005
6.474552	339.048670	9.114023
6.531791	338.442998	9.119040
6.691948	361.515336	9.124058
7.086046	353.629477	9.129075
6.856540	354.244085	9.134093
6.631321	326.192060	9.139111
6.506255	341.158919	9.144128
6.400050	326.434108	9.149146
6.840048	321.259980	9.154163
6.660513	326.876015	9.159181
6.700699	311.433525	9.164199
6.359639	322.193480	9.169216
6.415346	328.057074	9.174234
6.488401	316.249935	9.179251
6.256468	323.095536	9.184269
6.519418	344.671463	9.189287
6.819462	347.212159	9.194304
6.983744	359.089272	9.199322
6.547225	345.876881	9.204339
6.685748	355.628443	9.209357
6.798146	347.060410	9.214375
6.681825	335.059912	9.219392
6.546594	322.360485	9.224410
6.806817	346.951749	9.229427
6.673990	355.334382	9.234445
6.774061	333.220388	9.239463
6.773963	340.211195	9.244480
6.521505	325.037265	9.249498
6.925490	328.010455	9.254515
6.887775	338.080712	9.259533
6.896091	327.695966	9.264551
6.573288	328.500154	9.269568
6.336792	341.940299	9.274586
6.461922	332.265171	9.279603
6.689219	364.633009	9.284621
7.012031	354.210442	9.289639
6.919680	365.710306	9.294656
7.063668	351.868666	9.299674
7.084113	347.512763	9.304691
6.699608	333.812594	9.309709
6.794571	319.119882	9.314727
6.812644	321.547866	9.319744
6.785100	328.809663	9.324762
6.554737	314.134704	9.329779
6.560992	332.874826	9.334797
6.459677	331.954115	9.339815
6.964660	346.519997	9.344832
6.787539	357.730210	9.349850
6.840172	348.791059	9.354867
6.710495	352.401500	9.359885
6.907701	345.658595	9.364903
6.974059	340.968723	9.369920
6.661945	354.766947	9.374938
6.781676	338.597905	9.379955
6.721200	355.717068	9.384973
6.855225	353.940080	9.389991
7.087009	356.061275	9.395008
7.027449	349.300974	9.400026
6.799177	344.377686	9.405043
6.679068	354.228467	9.410061
7.014862	338.812078	9.415079
6.912970	353.442044	9.420096
6.455463	341.402380	9.425114
6.612901	351.366204	9.430131
6.659709	350.774949	9.435149
6.886707	348.342229	9.440167
7.104681	364.369130	9.445184
6.785515	355.673353	9.450202
6.795416	357.404172	9.455219
7.076852	369.955240	9.460237
7.245376	370.460187	9.465255
6.980331	360.957166	9.470272
7.104903	354.998875	9.475290
6.819694	353.555265	9.480307
7.069705	360.441284	9.485325
7.224845	356.021990	9.490343
7.007656	364.294490	9.495360
6.713524	350.051274	9.500378
7.269815	359.776996	9.505395
6.985112	360.277336	9.510413
6.877200	357.389081	9.515431
6.946066	365.966770	9.520448
6.870626	382.469911	9.525466
7.440301	369.524564	9.530483
7.449662	385.632504	9.535501
7.207989	372.619617	9.540519
7.332732	357.150020	9.545536
6.743148	362.901528	9.550554
7.051586	352.724280	9.555571
6.870985	363.144352	9.560589
7.110733	380.475667	9.565607
7.128919	379.384756	9.570624
7.183840	393.138300	9.575642
7.344615	371.888184	9.580659
6.983719	387.976627	9.585677
7.034109	382.116387	9.590695
7.176062	383.480602	9.595712
7.193196	385.737245	9.600730
7.205926	371.378847	9.605747
7.740135	380.586825	9.610765
7.262005	373.470805	9.615783
7.200224	348.861907	9.620800
7.039212	349.063637	9.625818
6.952862	359.445304	9.630835
7.123663	359.852068	9.635853
7.408883	373.049179	9.640871
7.561945	370.662818	9.645888
7.028763	352.847431	9.650906
7.142026	366.735954	9.655923
7.519899	362.695972	9.660941
7.236459	378.989458	9.665959
7.483871	362.536077	9.670976
7.086889	363.432620	9.675994
7.131228	361.317797	9.681011
7.495682	384.468679	9.686029
7.326283	380.948439	9.691047
6.986990	360.157840	9.696064
6.811594	372.103691	9.701082
7.421720	370.129455	9.706099
7.205968	381.646968	9.711117
7.239485	375.830157	9.716135
7.373026	379.732149	9.721152
7.135108	378.415821	9.726170
7.599625	376.772646	9.731187
7.226102	385.033307	9.736205
7.257016	375.982112	9.741223
7.128424	383.372511	9.746240
7.061267	380.625113	9.751258
7.328836	360.271280	9.756275
7.308484	382.157781	9.761293
7.010343	363.938288	9.766311
7.248034	374.814784	9.771328
7.008177	384.413895	9.776346
7.578900	401.943715	9.781363
7.889917	411.468634	9.786381
7.677653	397.283281	9.791399
7.678911	394.882249	9.796416
7.304643	381.461270	9.801434
7.294021	387.010644	9.806451
7.260670	385.842644	9.811469
7.556107	402.223412	9.816487
7.553136	392.671552	9.821504
7.203141	394.954525	9.826522
7.602370	399.872062	9.831539
7.609281	407.090024	9.836557
7.105427	403.857563	9.841575
7.705078	416.319971	9.846592
7.674134	416.290424	9.851610
7.660126	411.018113	9.856627
7.597162	396.495676	9.861645
7.488488	416.933750	9.866663
7.826110	395.400806	9.871680
7.526878	385.372959	9.876698
7.618760	384.280201	9.881715
7.566882	380.237337	9.886733
7.617903	382.195548	9.891751
7.807316	372.745926	9.896768
7.713299	364.118025	9.901786
7.780279	394.854919	9.906803
7.397081	380.449277	9.911821
7.266666	383.900542	9.916839
7.595327	373.550105	9.921856
7.761931	386.856076	9.926874
7.903515	389.099927	9.931891
7.548187	370.748972	9.936909
7.377658	379.149853	9.941927
7.670491	380.972167	9.946944
7.566212	398.581158	9.951962
7.787911	401.148487	9.956979
8.348616	404.828068	9.961997
7.693752	388.252385	9.967015
7.709789	381.641933	9.972032
7.556637	387.481026	9.977050
7.679185	379.485348	9.982067
7.730581	377.685014	9.987085
7.429363	389.649606	9.992103
7.725249	386.368429	9.997120
7.770499	413.500522	10.002138
7.731794	418.370881	10.007155
7.989234	413.523168	10.012173
7.611220	411.997672	10.017191
7.914131	412.589929	10.022208
7.935408	407.772092	10.027226
7.707550	404.931300	10.032243
7.915126	389.816284	10.037261
7.854819	399.979660	10.042279
8.010630	396.140591	10.047296
7.680054	395.320148	10.052314
7.702637	377.357196	10.057331
7.900230	371.944449	10.062349
7.840251	385.758695	10.067367
7.978590	375.052416	10.072384
7.649296	389.835712	10.077402
7.817278	396.588297	10.082419
8.051598	408.587007	10.087437
8.058497	390.300641	10.092455
7.898928	384.645816	10.097472
7.218990	391.545999	10.102490
7.420552	394.156703	10.107507
7.789118	399.752247	10.112525
7.779665	415.174643	10.117543
7.831653	408.649453	10.122560
7.647801	417.614604	10.127578
7.716113	417.461204	10.132595
7.848989	422.849218	10.137613
7.685952	413.676061	10.142631
7.694873	417.529386	10.147648
7.806700	429.286713	10.152666
8.289856	423.970713	10.157683
8.245707	416.191783	10.162701
7.951710	416.575288	10.167719
8.250345	413.916803	10.172736
7.931068	407.779548	10.177754
8.027862	397.331229	10.182771
8.136740	403.029712	10.187789
8.276683	415.417540	10.192807
8.456694	409.686121	10.197824
8.062532	405.668327	10.202842
8.025222	417.996399	10.207859
8.296275	416.771007	10.212877
7.965572	407.527163	10.217895
8.226527	412.348985	10.222912
8.260828	406.780289	10.227930
7.804040	417.096082	10.232947
8.039698	407.128113	10.237965
8.214657	414.155951	10.242983
8.354438	406.689742	10.248000
8.224263	410.732835	10.253018
7.988353	401.587864	10.258035
8.295575	397.403097	10.263053
8.231038	406.319103	10.268071
8.228415	399.270217	10.273088
8.095386	394.399068	10.278106
7.975382	414.297235	10.283123
8.360127	398.573076	10.288141
8.249210	413.157360	10.293159
8.141380	411.259945	10.298176
8.315691	402.520672	10.303194
8.203406	412.638330	10.308211
8.466859	414.953260	10.313229
8.097907	417.083704	10.318247
8.084741	420.265768	10.323264
8.324793	398.855608	10.328282
7.989522	409.932098	10.333299
8.177271	416.883436	10.338317
8.164354	412.988609	10.343335
8.445901	417.876400	10.348352
8.421478	406.849456	10.353370
8.239923	419.671803	10.358387
8.540773	406.158818	10.363405
8.110573	417.184386	10.368423
8.123834	412.069236	10.373440
8.383839	411.471479	10.378458
8.334423	424.435137	10.383475
8.402635	407.524551	10.388493
8.585032	423.702037	10.393511
8.459047	413.262284	10.398528
8.426771	415.250894	10.403546
7.985296	410.818103	10.408563
8.475106	401.002867	10.413581
8.268773	408.776100	10.418599
8.034378	414.881707	10.423616
8.286837	422.528257	10.428634
8.205240	429.057607	10.433651
8.771563	427.577769	10.438669
8.369434	436.906077	10.443687
8.852491	432.539333	10.448704
8.289381	427.841480	10.453722
8.114292	413.318862	10.458739
8.554395	421.391655	10.463757
8.578895	434.502021	10.468775
8.609112	423.157066	10.473792
8.400918	419.553195	10.478810
8.298757	419.754844	10.483827
8.816337	422.579494	10.488845
8.489878	434.021471	10.493863
8.493061	433.169978	10.498880
8.763081	411.178138	10.503898
8.277014	420.072891	10.508915
8.497506	417.930624	10.513933
8.595700	424.821882	10.518951
8.595253	433.298595	10.523968
8.762102	425.656888	10.528986
8.797699	430.407720	10.534003
8.474429	404.157576	10.539021
8.650515	404.214845	10.544039
8.677270	404.975440	10.549056
8.462858	403.613997	10.554074
8.166046	412.250665	10.559091
8.674555	438.867099	10.564109
8.554261	432.884399	10.569127
8.408385	447.477838	10.574144
8.782078	418.352041	10.579162
8.547642	443.820160	10.584179
8.710712	429.781157	10.589197
8.737492	434.809650	10.594215
8.913704	438.664262	10.599232
8.805746	430.261892	10.604250
8.675902	437.791659	10.609267
9.151145	433.619558	10.614285
8.849941	431.681872	10.619303
8.819384	431.703231	10.624320
8.815078	425.449271	10.629338
8.430214	427.760150	10.634355
8.810818	445.110179	10.639373
8.804523	447.452766	10.644391
8.710181	442.506822	10.649408
8.911538	443.673876	10.654426
8.571090	441.537810	10.659443
8.833783	448.193884	10.664461
8.839130	439.597637	10.669479
8.791107	452.364393	10.674496
8.844495	436.539977	10.679514
8.932603	452.652981	10.684531
8.858858	431.652601	10.689549
8.689125	443.150944	10.694567
8.675843	434.227163	10.699584
8.918245	431.907796	10.704602
8.655360	439.067631	10.709619
8.896051	442.212277	10.714637
8.714940	445.428104	10.719655
8.794815	445.620727	10.724672
9.126460	444.791507	10.729690
8.790898	439.876767	10.734707
9.046880	445.694813	10.739725
9.001259	442.379927	10.744743
8.890643	449.649507	10.749760
9.095904	428.472548	10.754778
8.641509	447.761441	10.759795
8.972725	437.052568	10.764813
8.823203	438.825780	10.769831
8.953424	436.593436	10.774848
9.214022	433.185342	10.779866
8.565538	424.802732	10.784883
8.775793	435.618568	10.789901
9.023002	429.685834	10.794919
8.945283	438.793846	10.799936
9.019715	436.227019	10.804954
8.998456	436.676741	10.809971
8.549091	444.835038	10.814989
8.812996	459.066659	10.820007
9.084612	466.082288	10.825024
9.666371	465.943913	10.830042
9.673587	461.853674	10.835059
9.216093	449.624112	10.840077
9.251724	444.752134	10.845095
9.089809	435.791120	10.850112
9.428380	442.493789	10.855130
9.026196	442.332731	10.860147
9.080084	430.695062	10.865165
9.288376	444.965676	10.870183
8.847780	438.879452	10.875200
9.171223	430.696359	10.880218
9.312409	436.576668	10.885235
9.010756	422.397010	10.890253
9.103661	434.111814	10.895271
8.838585	440.284393	10.900288
9.054667	448.334003	10.905306
9.188316	471.055672	10.910323
9.339765	464.894525	10.915341
9.198146	464.423848	10.920359
9.563761	471.784083	10.925376
9.821487	458.532633	10.930394
9.431439	452.105171	10.935411
9.065082	438.018353	10.940429
9.348117	424.222449	10.945447
9.019699	434.485455	10.950464
9.508432	443.533316	10.955482
9.466516	441.623332	10.960499
9.305939	433.028039	10.965517
9.460995	430.972545	10.970535
9.065345	433.513097	10.975552
9.412632	437.697311	10.980570
9.296189	456.985076	10.985587
9.459586	461.593769	10.990605
9.473191	451.810752	10.995623
9.497314	462.620072	11.000640
9.648144	450.696660	11.005658
9.667113	435.179817	11.010675
9.283921	442.292033	11.015693
9.380211	443.934295	11.020711
9.389758	439.980351	11.025728
9.670793	434.480093	11.030746
9.224953	434.583953	11.035763
9.396577	430.395411	11.040781
9.626731	433.076277	11.045799
9.040537	436.711603	11.050816
9.417546	442.441261	11.055834
9.467289	472.815220	11.060851
9.729275	453.905387	11.065869
9.806761	464.897372	11.070887
9.372352	472.883773	11.075904
9.777350	461.570529	11.080922
9.477833	468.719409	11.085939
9.618677	457.410660	11.090957
9.483723	467.418156	11.095975
9.559336	470.879084	11.100992
9.793185	460.783362	11.106010
9.506472	452.520136	11.111027
9.225010	439.650637	11.116045
9.600086	461.389645	11.121063
9.544509	462.313609	11.126080
9.678225	478.234314	11.131098
9.526055	471.416252	11.136115
9.666915	477.151591	11.141133
9.939111	472.921523	11.146151
9.666928	475.822380	11.151168
9.935447	471.580620	11.156186
9.700421	468.590745	11.161203
9.679490	485.929935	11.166221
9.832097	460.468625	11.171239
9.737069	482.241957	11.176256
9.845872	459.820908	11.181274
9.738877	474.205053	11.186291
9.725014	471.106112	11.191309
9.739478	469.113499	11.196327
9.574805	476.931838	11.201344
9.778277	476.652784	11.206362
9.724722	474.831014	11.211379
9.662545	483.519277	11.216397
9.683846	467.339402	11.221415
9.507330	480.342417	11.226432
9.739169	461.966247	11.231450
9.590523	475.171778	11.236467
9.450215	470.160902	11.241485
9.575061	468.576800	11.246503
9.493320	469.102248	11.251520
9.542035	469.132056	11.256538
9.603407	484.757524	11.261555
9.654879	492.095096	11.266573
9.863582	490.428748	11.271591
9.827518	504.856696	11.276608
9.799050	481.294940	11.281626
9.996728	501.757186	11.286643
9.950435	491.324479	11.291661
10.367197	497.282563	11.296679
9.918906	494.238681	11.301696
10.130632	502.669250	11.306714
10.150310	489.585226	11.311731
9.992860	493.319745	11.316749
9.974251	491.348636	11.321767
10.052622	494.778608	11.326784
10.301728	491.398378	11.331802
10.597682	490.412991	11.336819
9.892891	493.800089	11.341837
10.081851	460.794202	11.346855
9.466834	453.223044	11.351872
10.136085	469.352301	11.356890
10.207794	473.145377	11.361907
9.977455	493.361699	11.366925
10.088090	474.705529	11.371943
9.991024	490.953673	11.376960
10.315600	468.934332	11.381978
10.091784	483.095634	11.386995
10.222414	481.839324	11.392013
10.161217	477.398478	11.397031
10.044726	479.052586	11.402048
10.455068	489.632498	11.407066
10.389546	485.045457	11.412083
10.189339	483.853462	11.417101
10.262505	479.696823	11.422119
10.399808	480.772525	11.427136
10.155685	471.146719	11.432154
10.280676	469.978916	11.437171
10.227675	484.227312	11.442189
10.173632	471.180972	11.447207
10.197340	488.362040	11.452224
10.111492	481.391813	11.457242
10.434833	495.061732	11.462259
10.300584	488.366946	11.467277
10.727964	473.932156	11.472295
10.307780	475.994718	11.477312
10.367927	466.040657	11.482330
10.475115	450.374022	11.487347
9.955498	462.240645	11.492365
10.402026	468.561708	11.497383
10.211073	482.857894	11.502400
10.140980	497.480382	11.507418
10.398728	480.367180	11.512435
10.275215	492.339580	11.517453
10.446849	482.076125	11.522471
10.309040	486.997520	11.527488
10.402050	490.898170	11.532506
10.272735	490.606216	11.537523
10.167225	497.794781	11.542541
10.437379	485.971077	11.547559
10.187224	482.135510	11.552576
10.095960	493.579794	11.557594
10.495648	488.240863	11.562611
10.148647	489.169398	11.567629
10.433271	481.743372	11.572647
10.415499	494.455866	11.577664
10.383289	476.883145	11.582682
10.466561	488.838099	11.587699
10.505607	505.112374	11.592717
11.065385	507.976610	11.597735
10.782649	493.365137	11.602752
10.444270	483.623440	11.607770
10.717002	477.305572	11.612787
10.653728	490.688392	11.617805
10.660643	479.236746	11.622823
10.231151	492.371903	11.627840
10.211868	490.306148	11.632858
10.674735	504.572532	11.637875
10.159235	517.059311	11.642893
10.891576	523.422511	11.647911
11.147276	524.887890	11.652928
10.815909	522.065755	11.657946
11.210444	503.161607	11.662963
10.619040	494.742564	11.667981
10.705079	487.192408	11.672999
10.795431	476.776784	11.678016
10.783028	484.386253	11.683034
10.905776	485.979966	11.688051
10.348884	490.673948	11.693069
10.525044	483.603252	11.698087
10.438909	484.884139	11.703104
10.669656	509.957669	11.708122
10.755488	516.281387	11.713139
10.658840	520.569784	11.718157
11.056268	519.932980	11.723175
10.995991	511.066512	11.728192
10.802187	514.687785	11.733210
10.924426	521.042191	11.738227
11.126824	523.667341	11.743245
11.039762	518.856057	11.748263
10.910158	502.091901	11.753280
10.633359	492.363342	11.758298
10.721421	499.454288	11.763315
10.774232	525.022670	11.768333
11.145012	525.518897	11.773351
11.123698	529.082346	11.778368
10.772428	520.206988	11.783386
11.080480	509.827492	11.788403
11.056936	522.033032	11.793421
11.062922	515.817579	11.798439
10.906616	498.356064	11.803456
10.953141	520.049083	11.808474
11.287351	514.700202	11.813491
10.803126	508.829566	11.818509
10.664822	499.824860	11.823527
10.938318	515.799844	11.828544
10.813760	507.980822	11.833562
10.776371	514.844051	11.838579
10.810845	517.786930	11.843597
11.218525	514.219116	11.848615
11.061644	521.077199	11.853632
10.848680	516.242344	11.858650
11.365840	521.787007	11.863667
10.740659	529.292011	11.868685
11.161584	512.195988	11.873703
10.997350	520.464053	11.878720
11.051698	511.002029	11.883738
10.766273	513.066040	11.888755
10.709550	514.609023	11.893773
11.029104	527.796462	11.898791
11.162577	545.364266	11.903808
11.296479	538.832372	11.908826
11.539895	531.153951	11.913843
11.634345	552.654502	11.918861
11.688345	521.546361	11.923879
11.967787	505.703999	11.928896
11.487111	508.172318	11.933914
11.604979	498.497892	11.938931
11.204507	495.258166	11.943949
11.547340	498.060739	11.948967
11.513808	508.971032	11.953984
11.434845	502.414701	11.959002
11.409761	492.707519	11.964019
11.535776	506.581468	11.969037
11.523060	484.516495	11.974055
11.545023	514.709646	11.979072
11.179841	494.849265	11.984090
11.546245	498.309375	11.989107
11.336806	500.574843	11.994125
11.715003	498.769000	11.999143
11.460230	479.433157	12.004160
11.043893	475.027778	12.009178
11.536577	488.945222	12.014195
11.759475	492.255274	12.019213
11.623406	478.107437	12.024231
11.526113	469.814374	12.029248
11.187526	460.225044	12.034266
11.342010	476.266690	12.039283
11.315891	475.944005	12.044301
11.356006	497.138977	12.049319
11.750524	489.907130	12.054336
11.469901	499.687903	12.059354
11.782380	495.204980	12.064371
11.401881	490.254453	12.069389
11.737903	487.585251	12.074407
11.830038	501.428386	12.079424
11.787812	500.625326	12.084442
11.919293	492.658419	12.089459
11.373409	478.116130	12.094477
11.721925	472.787431	12.099495
11.331567	475.757016	12.104512
11.361865	493.322524	12.109530
11.473551	487.910747	12.114547
11.471673	503.341034	12.119565
11.631955	508.364905	12.124583
11.904461	493.299769	12.129600
11.689429	508.186310	12.134618
11.363419	508.254428	12.139635
11.510832	506.774438	12.144653
11.543935	497.599123	12.149671
11.792003	502.811481	12.154688
11.488148	509.190738	12.159706
11.506328	501.567854	12.164723
11.432068	509.102935	12.169741
11.497053	498.199990	12.174759
11.939111	520.549889	12.179776
12.015052	520.803679	12.184794
12.291286	516.522355	12.189811
12.045595	505.439312	12.194829
11.892587	521.264372	12.199847
11.914424	498.689476	12.204864
11.567844	514.608901	12.209882
11.625283	495.677814	12.214899
11.777744	511.434770	12.219917
12.053848	521.387755	12.224935
11.913244	530.222729	12.229952
11.915455	526.854460	12.234970
11.934892	511.106817	12.239987
11.590409	534.218333	12.245005
11.530457	531.400445	12.250023
11.732530	527.659280	12.255040
11.999199	535.157320	12.260058
11.917423	522.336621	12.265075
11.899996	531.974341	12.270093
11.981953	527.100290	12.275111
11.935791	525.082365	12.280128
11.995568	541.213429	12.285146
12.104426	528.601313	12.290163
11.972877	534.563629	12.295181
11.777718	522.529370	12.300199
12.177251	528.436490	12.305216
11.950608	530.287105	12.310234
12.311253	530.032555	12.315251
12.252466	540.604323	12.320269
12.175051	533.138128	12.325287
12.215847	522.834079	12.330304
12.069604	533.353187	12.335322
12.379254	536.666427	12.340339
12.282644	525.263145	12.345357
12.035298	535.989756	12.350375
12.241503	531.413294	12.355392
12.020660	536.599933	12.360410
12.717756	548.041306	12.365427
12.358892	544.284989	12.370445
12.503138	535.483009	12.375463
12.573553	529.752437	12.380480
12.176495	531.703930	12.385498
12.456721	534.296050	12.390515
12.645921	525.176396	12.395533
12.351221	540.812252	12.400551
12.484620	520.208996	12.405568
12.241379	538.752181	12.410586
12.506306	519.699399	12.415603
12.359382	519.924091	12.420621
12.077729	535.254227	12.425639
12.332512	523.593916	12.430656
12.368926	529.660524	12.435674
12.129307	528.678821	12.440691
12.279925	526.332494	12.445709
12.116879	529.928417	12.450727
12.811284	544.808958	12.455744
12.454461	547.851930	12.460762
12.885735	532.308771	12.465779
12.726126	531.334904	12.470797
12.488771	526.444447	12.475815
12.505778	515.334023	12.480832
12.209163	529.883475	12.485850
12.395058	533.429017	12.490867
12.475534	536.223392	12.495885
12.581045	558.831073	12.500903
13.068825	552.908032	12.505920
12.846153	547.464110	12.510938
12.287600	531.375367	12.515955
12.460422	534.788166	12.520973
12.576671	538.894380	12.525991
12.879214	553.774350	12.531008
13.010528	549.889896	12.536026
12.824633	531.315328	12.541043
12.631644	525.882351	12.546061
12.483866	524.848080	12.551079
12.675498	526.879603	12.556096
12.679556	539.059046	12.561114
12.788681	532.901718	12.566131
12.635506	536.855265	12.571149
12.721281	560.652205	12.576167
13.137097	552.420230	12.581184
12.673825	554.675895	12.586202
12.542116	562.156536	12.591219
13.110105	556.737519	12.596237
12.820328	551.831609	12.601255
13.104647	538.173641	12.606272
12.542884	543.856363	12.611290
13.004944	547.869616	12.616307
13.347248	554.829424	12.621325
13.138642	542.269857	12.626343
12.917726	524.276027	12.631360
12.740962	523.452199	12.636378
12.958020	518.384218	12.641395
12.961631	526.774311	12.646413
12.734562	521.772441	12.651431
13.223754	518.973324	12.656448
12.873654	523.154337	12.661466
12.678493	523.724408	12.666483
13.008105	538.426906	12.671501
13.111413	547.306401	12.676519
13.115183	547.797549	12.681536
13.149391	557.525545	12.686554
12.809063	544.188060	12.691571
13.065433	547.353949	12.696589
13.043875	563.410804	12.701607
13.047630	551.801302	12.706624
12.864787	557.316224	12.711642
13.090508	544.068710	12.716659
13.074922	561.285775	12.721677
13.066702	557.293803	12.726695
13.393255	553.981644	12.731712
13.338842	557.285681	12.736730
13.079600	556.204294	12.741747
13.161373	557.991055	12.746765
12.909757	567.369646	12.751783
13.211096	559.029847	12.756800
13.530995	567.553767	12.761818
13.263639	557.391144	12.766835
13.471793	562.145973	12.771853
13.052861	571.714475	12.776871
13.459706	553.626514	12.781888
13.380033	556.121560	12.786906
13.078667	553.300758	12.791923
13.267655	545.779906	12.796941
13.089282	547.073975	12.801959
13.298504	557.071294	12.806976
13.217372	551.726388	12.811994
13.128705	557.959603	12.817011
13.044037	549.199281	12.822029
13.086814	557.747441	12.827047
13.205477	556.282923	12.832064
13.488361	568.727056	12.837082
13.624651	572.299008	12.842099
13.964195	545.955026	12.847117
13.279819	553.644481	12.852135
13.380637	545.079531	12.857152
13.341566	544.600170	12.862170
13.234900	544.284693	12.867187
13.936432	570.867002	12.872205
13.442895	555.804807	12.877223
13.506956	551.567392	12.882240
14.016591	563.739368	12.887258
13.880130	555.607512	12.892275
13.795172	547.604218	12.897293
13.712891	546.393813	12.902311
13.653202	545.249537	12.907328
13.761968	540.276097	12.912346
13.719943	542.198342	12.917363
14.030233	549.332191	12.922381
13.285408	536.468042	12.927399
13.619869	536.009116	12.932416
13.544862	537.815485	12.937434
13.688228	530.027550	12.942451
13.821702	535.473168	12.947469
13.674723	542.799870	12.952487
13.802157	546.229520	12.957504
13.562468	538.651889	12.962522
13.499710	555.398231	12.967539
13.886484	536.138041	12.972557
13.888609	558.105112	12.977575
13.857874	550.579043	12.982592
14.173577	542.969554	12.987610
13.625912	545.951863	12.992627
13.683834	541.444476	12.997645
14.087986	548.814517	13.002663
14.244142	549.405743	13.007680
13.933225	541.272811	13.012698
13.527985	549.556513	13.017715
13.890201	533.048062	13.022733
13.995556	563.870466	13.027751
13.934229	566.325090	13.032768
14.173733	553.092708	13.037786
13.795329	566.177667	13.042803
14.173840	543.964416	13.047821
14.182085	560.009159	13.052839
13.762410	557.779209	13.057856
14.240836	550.718949	13.062874
14.057997	555.587096	13.067891
14.107477	541.856643	13.072909
13.917337	553.161842	13.077927
14.245345	557.058803	13.082944
14.417293	556.853739	13.087962
13.879981	551.805516	13.092979
14.180127	556.601721	13.097997
14.086797	560.167829	13.103015
13.928662	571.953743	13.108032
13.985141	566.282138	13.113050
14.120858	570.243548	13.118067
14.253823	564.815731	13.123085
14.657553	572.828100	13.128103
14.614295	564.335360	13.133120
14.301351	557.997445	13.138138
14.176531	545.945148	13.143155
14.354719	542.985077	13.148173
13.904303	540.752831	13.153191
14.444907	562.632989	13.158208
14.397071	566.819855	13.163226
14.273587	553.859900	13.168243
14.528545	565.549008	13.173261
14.539960	562.114858	13.178279
14.665286	561.403169	13.183296
14.263335	551.459884	13.188314
14.023775	548.789948	13.193331
14.484256	557.913493	13.198349
14.358809	572.652947	13.203367
14.370485	556.221292	13.208384
14.237415	563.209773	13.213402
14.329822	570.420965	13.218419
14.544289	568.005927	13.223437
14.407851	572.279956	13.228455
14.728472	566.314867	13.233472
14.635310	567.552347	13.238490
14.499363	564.223826	13.243507
14.266925	567.830537	13.248525
14.513902	573.586260	13.253543
14.791578	571.751659	13.258560
14.718930	555.466286	13.263578
14.443086	568.688193	13.268595
14.473090	546.182429	13.273613
14.099567	568.939052	13.278631
14.438405	557.863580	13.283648
14.747106	565.651459	13.288666
14.287650	557.173676	13.293683
14.577670	555.619736	13.298701
14.712488	568.600895	13.303719
14.672308	582.882884	13.308736
14.975504	575.082879	13.313754
14.772188	581.943547	13.318771
14.901328	560.457615	13.323789
14.822581	564.102001	13.328807
14.592720	577.682261	13.333824
14.906062	576.684944	13.338842
14.840662	594.720591	13.343859
15.068989	596.033259	13.348877
15.033773	580.300972	13.353895
14.748989	572.611418	13.358912
14.837771	564.736350	13.363930
14.775568	592.286705	13.368947
15.327279	591.599901	13.373965
15.062658	573.938737	13.378983
14.711232	562.575962	13.384000
14.716439	577.161779	13.389018
15.047833	582.152478	13.394035
14.868948	586.931423	13.399053
15.024803	587.022343	13.404071
14.952197	599.705710	13.409088
15.371675	585.773463	13.414106
14.776814	590.866458	13.419123
14.858592	591.052669	13.424141
15.159928	578.254612	13.429159
15.067069	598.175592	13.434176
15.080741	579.358299	13.439194
14.609867	582.754483	13.444211
14.895990	583.435916	13.449229
14.905879	584.707733	13.454247
14.866478	592.863303	13.459264
15.331895	585.896392	13.464282
15.007896	585.459195	13.469299
15.288777	588.660107	13.474317
15.079374	597.405237	13.479335
15.202297	594.590768	13.484352
15.228510	600.002967	13.489370
15.054010	603.401740	13.494387
15.308181	613.094799	13.499405
15.596374	613.511986	13.504423
15.308364	619.004063	13.509440
15.691913	605.113356	13.514458
15.514488	605.606504	13.519475
15.601040	585.157515	13.524493
15.680903	577.557463	13.529511
15.512667	588.533860	13.534528
15.866953	578.941739	13.539546
15.711185	569.909667	13.544563
15.732152	581.992872	13.549581
15.672322	569.895180	13.554599
15.409790	578.419121	13.559616
15.700155	574.749551	13.564634
15.576964	583.517522	13.569651
15.627683	570.782535	13.574669
15.781385	582.271027	13.579687
15.647156	578.093826	13.584704
15.753744	569.241863	13.589722
15.465539	557.322532	13.594739
15.561040	574.521944	13.599757
15.807669	584.477283	13.604775
15.580573	577.276681	13.609792
15.722461	577.791646	13.614810
15.548605	582.607839	13.619827
15.783429	576.151155	13.624845
16.319208	575.520120	13.629863
15.439057	562.695235	13.634880
15.415865	561.765438	13.639898
15.313848	575.461344	13.644915
15.471250	573.528442	13.649933
15.712042	587.220843	13.654951
15.437021	580.370882	13.659968
15.724878	578.107351	13.664986
15.645398	598.654889	13.670003
15.543346	579.063134	13.675021
16.126664	582.495682	13.680039
15.789598	584.945497	13.685056
16.079235	574.243202	13.690074
15.991504	577.460747	13.695091
15.863859	578.779890	13.700109
15.909154	563.892646	13.705127
15.787953	590.065427	13.710144
16.224494	569.424702	13.715162
16.029722	573.547981	13.720179
15.611319	585.177167	13.725197
15.857614	574.899539	13.730215
16.083023	587.334588	13.735232
15.863058	586.716562	13.740250
15.975554	581.198151	13.745267
15.885535	599.048159	13.750285
15.987734	611.523071	13.755303
15.783808	623.294845	13.760320
16.316664	608.429814	13.765338
16.352519	613.109321	13.770355
16.097891	618.111366	13.775373
16.444267	607.425256	13.780391
16.152417	623.040257	13.785408
16.153747	610.160389	13.790426
16.293999	620.654549	13.795443
16.138179	615.847807	13.800461
16.441757	607.633365	13.805479
16.212689	622.402487	13.810496
16.440428	615.356270	13.815514
16.460218	601.306938	13.820531
16.097208	602.067698	13.825549
16.501257	612.314081	13.830567
16.460884	605.511038	13.835584
16.311893	592.750488	13.840602
15.987776	598.870602	13.845619
16.057105	593.032931	13.850637
16.416271	607.314779	13.855655
16.174466	601.662344	13.860672
16.370108	603.525149	13.865690
16.008316	609.779018	13.870707
16.020340	608.134533	13.875725
16.356239	601.995101	13.880743
16.131882	605.001335	13.885760
15.890111	617.961129	13.890778
16.371591	624.626487	13.895795
16.672491	648.387327	13.900813
16.802876	628.207145	13.905831
16.550361	642.449496	13.910848
16.688649	636.934773	13.915866
16.773516	629.091216	13.920883
16.865577	628.852218	13.925901
17.033208	629.289132	13.930919
16.735378	620.144619	13.935936
16.618710	601.958811	13.940954
16.970341	609.952160	13.945971
16.783454	606.434266	13.950989
16.891510	589.298348	13.956007
16.626871	603.564216	13.961024
16.882599	600.053473	13.966042
16.678723	592.286284	13.971059
16.578114	602.252966	13.976077
16.729389	591.099144	13.981095
16.749115	607.775335	13.986112
17.006695	623.154010	13.991130
17.164766	618.294904	13.996147
16.979270	610.594630	14.001165
16.966422	591.758777	14.006183
17.016453	606.546508	14.011200
16.781524	601.321660	14.016218
17.030462	605.865389	14.021235
16.983602	597.724115	14.026253
17.015085	592.280193	14.031271
16.798477	607.950543	14.036288
16.983249	604.749575	14.041306
17.306434	624.735660	14.046323
17.220672	606.144551	14.051341
17.407727	605.387826	14.056359
16.811542	602.427596	14.061376
16.977513	601.071466	14.066394
17.028021	594.557855	14.071411
17.047443	602.920975	14.076429
17.188123	624.731324	14.081447
17.441972	629.013098	14.086464
17.395698	609.934387	14.091482
17.235569	600.649149	14.096499
17.242554	607.915508	14.101517
17.311083	586.381795	14.106535
16.715629	614.697198	14.111552
16.960600	609.777683	14.116570
17.160213	628.438688	14.121587
16.977365	636.825707	14.126605
17.439795	625.778075	14.131623
17.418857	636.748075	14.136640
17.617221	630.661175	14.141658
17.595865	614.505611	14.146675
17.333839	629.437428	14.151693
17.536400	627.680472	14.156711
17.151933	623.459692	14.161728
17.321704	624.003704	14.166746
17.394457	623.826642	14.171763
17.601725	622.275054	14.176781
17.723814	622.163146	14.181799
17.480956	637.724410	14.186816
17.448900	632.996495	14.191834
17.731488	633.456625	14.196851
17.433021	633.092253	14.201869
17.421162	638.122770	14.206887
17.528134	629.009657	14.211904
17.477632	633.725680	14.216922
17.667779	626.529116	14.221939
17.212413	642.631273	14.226957
17.619359	614.513708	14.231975
17.446855	637.537232	14.236992
17.451462	630.060780	14.242010
17.649200	632.580351	14.247027
17.684592	620.574630	14.252045
17.757204	628.906539	14.257063
17.574755	622.172231	14.262080
17.711339	624.345013	14.267098
18.059443	629.390333	14.272115
17.805340	622.426985	14.277133
17.633725	622.407794	14.282151
17.885196	631.889655	14.287168
18.136113	635.511658	14.292186
18.033342	639.659702	14.297203
17.873270	622.311334	14.302221
18.318419	621.976793	14.307239
17.799408	629.062734	14.312256
17.993653	618.847700	14.317274
17.989819	618.099395	14.322291
17.761060	638.938710	14.327309
18.111978	635.253216	14.332327
18.112422	637.434919	14.337344
18.040363	637.324099	14.342362
18.147413	635.273460	14.347379
18.070061	622.762788	14.352397
17.896786	623.184304	14.357415
18.082772	638.245189	14.362432
18.384800	639.083895	14.367450
18.490700	639.413424	14.372467
18.064931	625.983321	14.377485
18.099985	629.645521	14.382503
18.048514	627.692813	14.387520
18.193020	637.326078	14.392538
18.355544	622.212177	14.397555
18.238679	632.719118	14.402573
18.425792	630.280448	14.407591
18.363982	647.502199	14.412608
18.404331	640.588681	14.417626
18.678680	631.999040	14.422643
18.111721	632.927622	14.427661
18.542785	628.251390	14.432679
18.964898	629.162746	14.437696
18.353224	630.520160	14.442714
18.741159	620.841174	14.447731
18.083423	620.362991	14.452749
18.204545	622.195802	14.457767
18.365311	624.421856	14.462784
18.434946	645.559612	14.467802
19.012808	639.885459	14.472819
18.392052	621.660816	14.477837
18.581783	626.582052	14.482855
18.523033	633.425543	14.487872
18.248723	636.178691	14.492890
18.569836	637.134683	14.497907
18.663207	637.623622	14.502925
18.775581	638.673050	14.507943
18.638107	627.124319	14.512960
18.630395	642.461739	14.517978
18.531479	640.450451	14.522995
18.460637	641.047312	14.528013
18.621180	634.836970	14.533031
18.650246	622.685776	14.538048
18.782783	639.765884	14.543066
18.945892	631.583991	14.548083
18.658024	635.735365	14.553101
18.442680	637.843111	14.558119
18.456858	637.242576	14.563136
18.526088	626.609434	14.568154
18.770678	623.069531	14.573171
18.762472	638.516252	14.578189
18.783714	652.576598	14.583207
19.145758	658.040084	14.588224
19.084643	668.785803	14.593242
19.080591	663.741325	14.598259
19.010233	664.082860	14.603277
19.387576	656.257277	14.608295
19.348416	634.853467	14.613312
18.833528	636.963482	14.618330
19.013238	633.619584	14.623347
18.984076	631.365039	14.628365
19.088387	649.576294	14.633383
19.154467	641.802943	14.638400
19.113679	661.311965	14.643418
19.583945	655.470499	14.648435
19.540775	645.087846	14.653453
19.333658	636.960635	14.658471
19.687428	624.333355	14.663488
19.197273	632.040445	14.668506
19.175788	633.468689	14.673523
19.248047	616.811660	14.678541
19.073068	628.428105	14.683559
19.466706	619.203863	14.688576
19.173985	633.739584	14.693594
19.460547	632.649962	14.698611
19.332426	618.254880	14.703629
19.481388	627.838795	14.708647
19.436928	627.068470	14.713664
19.020041	622.829432	14.718682
19.551377	634.368718	14.723699
19.663375	651.143752	14.728717
19.457353	645.346742	14.733735
19.918224	645.126009	14.738752
19.440256	634.207896	14.743770
19.413513	633.870944	14.748787
19.418112	629.597874	14.753805
19.214863	653.259011	14.758823
19.678940	652.807002	14.763840
19.461898	668.331559	14.768858
19.950914	666.784477	14.773875
19.616370	660.936475	14.778893
19.525428	670.131532	14.783911
19.803133	659.332357	14.788928
19.551912	657.728220	14.793946
19.845516	662.400376	14.798963
19.621411	662.146419	14.803981
19.540431	655.292008	14.808999
19.931875	664.866280	14.814016
19.834134	662.190600	14.819034
19.815888	645.470268	14.824051
19.784102	661.868296	14.829069
19.678143	646.757410	14.834087
19.770798	665.081407	14.839104
19.772257	644.668540	14.844122
19.659163	667.328449	14.849139
19.622485	655.563387	14.854157
20.056667	675.680764	14.859175
20.221208	690.694865	14.864192
19.697594	661.195568	14.869210
20.272092	670.674256	14.874227
20.569269	684.293075	14.879245
20.077924	675.135145	14.884263
20.047170	654.713320	14.889280
19.703948	665.840902	14.894298
20.221228	663.425500	14.899315
20.475124	676.578360	14.904333
19.993509	671.820814	14.909351
20.261754	663.867822	14.914368
20.085691	684.942719	14.919386
19.955662	683.329081	14.924403
20.223807	692.758140	14.929421
20.253199	682.665654	14.934439
20.164924	686.064760	14.939456
20.369649	682.787761	14.944474
20.458028	677.600478	14.949491
20.320531	666.245175	14.954509
20.474569	678.667492	14.959527
20.731348	664.319854	14.964544
20.353766	673.426785	14.969562
20.737461	669.381728	14.974579
20.264193	683.561903	14.979597
20.326628	674.772181	14.984615
20.351182	676.157004	14.989632
20.182920	672.331077	14.994650
20.535112	676.772059	14.999667
20.491093	686.340964	15.004685
20.361889	675.818807	15.009703
20.536349	680.271055	15.014720
20.416372	675.231462	15.019738
20.526083	665.162910	15.024755
20.331708	684.628660	15.029773
20.640205	678.225195	15.034791
20.918040	686.851383	15.039808
20.728337	678.341354	15.044826
21.112352	678.757763	15.049843
20.706280	678.385490	15.054861
20.780805	676.163693	15.059879
20.864613	667.533687	15.064896
20.997828	674.656022	15.069914
20.751241	672.888858	15.074931
20.961277	673.051119	15.079949
20.534456	670.776971	15.084967
21.332173	676.419583	15.089984
20.685219	686.071101	15.095002
21.042280	677.553963	15.100019
21.221366	691.110533	15.105037
21.100030	685.737587	15.110055
21.125324	674.195969	15.115072
20.866296	674.209623	15.120090
20.965334	682.704375	15.125107
21.100182	691.341699	15.130125
21.085273	697.642091	15.135143
21.302245	697.983573	15.140160
20.967738	695.585337	15.145178
21.202211	704.506224	15.150195
21.578406	707.679504	15.155213
21.230192	682.815216	15.160231
21.167418	680.599183	15.165248
20.850020	688.490098	15.170266
21.205680	687.679529	15.175283
21.158726	695.951038	15.180301
21.234859	696.078159	15.185319
21.178208	684.425108	15.190336
21.320744	705.024167	15.195354
21.371255	698.985584	15.200371
21.456014	692.744348	15.205389
21.186074	702.908423	15.210407
21.398663	699.204249	15.215424
21.181248	698.701219	15.220442
21.504924	694.187361	15.225459
21.744835	695.508258	15.230477
21.161724	689.626931	15.235495
21.379727	700.689839	15.240512
21.290681	692.494872	15.245530
21.432524	701.541075	15.250547
21.846715	688.303521	15.255565
21.526930	693.110014	15.260583
21.566025	697.988074	15.265600
21.505495	690.297318	15.270618
21.720173	712.940226	15.275635
22.136077	717.847535	15.280653
21.760005	709.027135	15.285671
21.744753	696.544908	15.290688
21.720636	708.181747	15.295706
21.955432	700.983084	15.300723
21.857228	707.619897	15.305741
21.480570	696.020210	15.310759
21.897036	709.645808	15.315776
21.803190	722.761514	15.320794
21.950586	723.874040	15.325811
22.071919	720.125803	15.330829
21.860430	720.533957	15.335847
22.375737	723.351563	15.340864
22.318963	715.073318	15.345882
22.037601	701.384603	15.350899
22.017128	694.259023	15.355917
21.854395	679.021598	15.360935
22.089756	707.977528	15.365952
22.204943	702.853702	15.370970
22.215673	712.103224	15.375987
22.416613	703.556571	15.381005
21.955992	694.899325	15.386023
22.626415	697.359589	15.391040
21.888773	698.123714	15.396058
22.096168	710.266740	15.401075
22.106458	710.451875	15.406093
22.193912	724.215988	15.411111
22.265794	704.942875	15.416128
22.738578	720.023556	15.421146
22.494049	721.356615	15.426163
22.746547	720.518320	15.431181
22.411829	709.660316	15.436199
22.269676	704.080820	15.441216
22.320180	696.777117	15.446234
22.427354	718.949640	15.451251
22.652509	712.639538	15.456269
22.151154	716.245163	15.461287
22.439540	708.731224	15.466304
22.577523	710.385223	15.471322
22.256207	721.178308	15.476339
22.743262	727.718020	15.481357
22.472717	722.843709	15.486375
22.528495	716.324453	15.491392
22.709319	708.585143	15.496410
22.549275	713.201312	15.501427
22.409993	710.928742	15.506445
22.536880	709.295178	15.511463
22.551178	709.789020	15.516480
22.586699	722.315778	15.521498
22.482826	715.207908	15.526515
23.087650	726.769953	15.531533
22.523159	743.717789	15.536551
22.759052	738.527068	15.541568
22.932219	746.697089	15.546586
22.861118	740.664613	15.551603
23.257009	733.942135	15.556621
23.350445	750.129456	15.561639
23.281194	728.212807	15.566656
23.205957	725.255417	15.571674
23.179996	706.026712	15.576691
23.234111	708.248559	15.581709
23.393234	706.110291	15.586727
23.424519	706.391439	15.591744
23.329304	709.615561	15.596762
22.918891	709.432735	15.601779
23.287592	702.748712	15.606797
23.316910	715.900048	15.611815
23.267710	704.761166	15.616832
22.988598	708.876673	15.621850
22.863025	714.069374	15.626867
22.989172	700.794786	15.631885
23.083278	714.372406	15.636903
23.063676	724.273925	15.641920
23.102192	710.247375	15.646938
23.169239	733.237066	15.651955
23.840523	737.429618	15.656973
23.532003	727.714416	15.661991
23.300725	737.842015	15.667008
23.454851	723.334362	15.672026
23.509639	743.362300	15.677043
23.657391	726.387735	15.682061
23.494776	736.015630	15.687079
23.516772	728.515199	15.692096
24.031501	727.269688	15.697114
23.360948	726.879226	15.702131
23.809817	718.695622	15.707149
23.874950	739.959417	15.712167
23.464929	716.207168	15.717184
23.811368	720.283067	15.722202
23.462413	726.207191	15.727219
23.877508	726.602131	15.732237
23.825238	734.950898	15.737255
23.728086	728.666794	15.742272
23.788577	739.734112	15.747290
23.739561	736.133577	15.752307
23.827366	721.290223	15.757325
23.850619	732.943164	15.762343
23.853209	730.436572	15.767360
23.895174	730.489341	15.772378
23.754493	730.653374	15.777395
23.935068	731.747429	15.782413
24.188993	740.396886	15.787431
24.053913	737.018688	15.792448
24.142130	728.091836	15.797466
23.847998	739.330717	15.802483
24.089861	742.643595	15.807501
23.853834	730.773265	15.812519
23.908473	742.092470	15.817536
24.331225	733.919078	15.822554
23.860847	723.126778	15.827571
24.062470	728.383987	15.832589
23.995149	742.148797	15.837607
24.359874	737.823663	15.842624
24.598503	748.431542	15.847642
24.107229	735.320060	15.852659
24.380081	744.006735	15.857677
24.549505	738.067943	15.862695
24.234342	734.747549	15.867712
24.187740	730.838527	15.872730
24.037502	757.128765	15.877747
24.604753	753.359671	15.882765
24.376504	764.798949	15.887783
24.557250	751.277954	15.892800
24.856178	748.375332	15.897818
24.449754	752.512479	15.902835
24.383635	749.938518	15.907853
24.581468	750.250200	15.912871
24.782494	765.667493	15.917888
24.831561	746.981312	15.922906
24.538523	776.660649	15.927923
24.620534	750.974953	15.932941
24.637301	771.020231	15.937959
24.495427	762.780033	15.942976
24.648350	755.201865	15.947994
24.375821	756.200075	15.953011
24.539195	754.164221	15.958029
24.646698	748.880176	15.963047
24.544442	750.007785	15.968064
25.038748	765.035657	15.973082
25.041727	767.523671	15.978099
25.164549	775.082501	15.983117
24.897714	755.328330	15.988135
25.055870	755.615081	15.993152
25.257116	758.095816	15.998170
24.759357	757.679750	16.003187
25.105808	765.091117	16.008205
25.415614	781.920790	16.013223
25.345564	769.189259	16.018240
25.527307	750.330008	16.023258
25.195177	751.975598	16.028275
24.933841	750.849082	16.033293
24.952824	746.956770	16.038311
25.136462	751.868328	16.043328
25.125340	771.733913	16.048346
25.349941	774.562374	16.053363
25.344752	778.419400	16.058381
25.762314	776.041616	16.063399
25.158394	779.971803	16.068416
25.663730	767.281278	16.073434
25.329156	778.530414	16.078451
25.644706	769.907516	16.083469
25.788809	763.411134	16.088487
25.494567	753.115554	16.093504
25.612510	734.725506	16.098522
25.090187	736.906232	16.103539
25.714536	757.984358	16.108557
25.526966	764.898298	16.113575
25.570412	772.598065	16.118592
25.914085	767.150903	16.123610
25.823751	773.028175	16.128627
25.761013	757.832792	16.133645
25.879207	768.575617	16.138663
25.535177	774.529450	16.143680
25.428363	765.334291	16.148698
25.795067	773.329467	16.153715
25.994104	765.280112	16.158733
25.990432	764.923995	16.163751
25.726212	764.178368	16.168768
26.132900	772.214168	16.173786
25.821577	771.844242	16.178803
26.095278	770.635213	16.183821
25.984497	768.406927	16.188839
25.938987	769.224648	16.193856
25.787939	770.416902	16.198874
25.873971	774.851712	16.203891
25.796703	778.480357	16.208909
25.985274	769.058476	16.213927
25.856992	770.534394	16.218944
26.377163	769.988391	16.223962
25.898490	782.605288	16.228979
25.934052	769.067137	16.233997
26.160985	772.991289	16.239015
25.898082	783.011771	16.244032
26.404915	790.868967	16.249050
26.476777	796.036942	16.254067
26.431749	789.581938	16.259085
26.587789	793.875297	16.264103
26.499527	794.379201	16.269120
26.379687	773.650761	16.274138
26.152364	780.013841	16.279155
26.508303	779.913866	16.284173
26.772954	790.663303	16.289191
26.636318	785.811812	16.294208
26.991078	778.086528	16.299226
26.995367	776.675724	16.304243
26.419062	775.611587	16.309261
26.315322	762.874215	16.314279
26.312511	776.847631	16.319296
26.843212	779.493260	16.324314
27.089329	782.590440	16.329331
26.991565	774.358493	16.334349
26.942896	757.467127	16.339367
26.727330	762.607510	16.344384
26.809175	754.882270	16.349402
26.741612	748.751594	16.354419
26.618409	761.354897	16.359437
26.838307	763.975328	16.364455
27.014997	790.583354	16.369472
27.088965	775.011713	16.374490
26.943115	795.765316	16.379507
26.800899	792.507644	16.384525
27.205405	777.851111	16.389543
26.960852	805.532649	16.394560
27.118328	782.603113	16.399578
27.226364	782.098057	16.404595
27.032739	785.101707	16.409613
26.909044	774.522189	16.414631
27.045496	798.763177	16.419648
27.421368	785.533151	16.424666
26.953786	793.465666	16.429683
26.809517	794.914707	16.434701
27.018856	787.368922	16.439719
27.086077	781.701071	16.444736
27.078400	793.634591	16.449754
27.562026	802.199483	16.454771
27.371549	818.143218	16.459789
27.406762	811.675535	16.464807
27.409468	813.142308	16.469824
27.757344	819.997801	16.474842
27.512948	822.552977	16.479859
27.233844	825.052192	16.484877
27.715857	818.194905	16.489895
27.591256	824.300932	16.494912
27.752905	813.556350	16.499930
27.548891	811.242015	16.504947
28.030121	816.579984	16.509965
28.181354	799.921021	16.514983
27.470014	810.573554	16.520000
27.575084	805.947598	16.525018
27.913487	801.631223	16.530035
27.568833	815.384169	16.535053
27.701617	809.128061	16.540071
27.616870	806.219952	16.545088
27.602781	809.043681	16.550106
28.098060	793.574403	16.555123
27.945834	811.863473	16.560141
27.914205	793.722816	16.565159
28.109959	816.016635	16.570176
28.161095	807.598491	16.575194
28.086443	808.697534	16.580211
27.998230	806.095529	16.585229
27.971357	808.666614	16.590247
27.717264	801.186974	16.595264
28.099666	815.875409	16.600282
28.380919	807.217715	16.605299
27.931589	806.953250	16.610317
28.238471	822.000342	16.615335
28.028615	834.918342	16.620352
28.330096	839.165244	16.625370
28.804998	844.202574	16.630387
28.446156	838.769241	16.635405
28.775370	836.412640	16.640423
28.579158	813.502243	16.645440
28.193099	817.400472	16.650458
28.352079	802.882692	16.655475
28.663108	829.993846	16.660493
28.650550	820.448517	16.665511
28.637492	825.060011	16.670528
28.654465	831.232977	16.675546
28.936901	825.569397	16.680563
28.470842	821.297297	16.685581
28.715788	831.595313	16.690599
28.783593	826.637700	16.695616
28.708392	822.506371	16.700634
28.780273	817.435124	16.705651
28.295420	823.133577	16.710669
28.891549	823.172408	16.715687
28.888448	824.982968	16.720704
28.974622	831.119603	16.725722
29.166557	827.614234	16.730739
28.572263	837.521349	16.735757
29.074810	825.241861	16.740775
28.711171	827.873225	16.745792
28.768179	834.809165	16.750810
28.785311	825.904334	16.755827
28.909752	832.769991	16.760845
29.221231	830.324317	16.765863
28.935922	830.255623	16.770880
28.884907	847.389617	16.775898
29.021488	849.740144	16.780915
28.961781	864.090149	16.785933
29.396031	856.701308	16.790951
29.568661	851.017513	16.795968
29.458677	858.586295	16.800986
29.658464	853.075329	16.806003
29.238202	860.454108	16.811021
29.679417	840.916618	16.816039
29.420906	854.645204	16.821056
29.212589	847.521788	16.826074
29.801958	850.309960	16.831091
29.718385	855.192376	16.836109
29.973819	848.326787	16.841127
29.402886	833.364976	16.846144
29.531473	846.711187	16.851162
30.147039	848.096761	16.856179
29.709153	842.612725	16.861197
29.750905	825.599577	16.866215
29.531295	830.640479	16.871232
29.381464	846.575854	16.876250
29.743057	847.011620	16.881267
29.835072	856.423417	16.886285
29.898779	845.711356	16.891303
29.920672	835.973954	16.896320
30.249420	858.577639	16.901338
29.949405	840.904522	16.906355
29.767277	846.586415	16.911373
29.768650	850.710417	16.916391
30.051421	844.064149	16.921408
29.767274	858.185656	16.926426
29.997985	846.023619	16.931443
29.861745	850.299857	16.936461
29.641637	851.627022	16.941479
29.962312	842.111040	16.946496
29.796664	856.324450	16.951514
30.198634	857.006925	16.956531
30.592791	873.516440	16.961549
30.546182	871.371016	16.966567
30.465294	866.601602	16.971584
30.291332	852.410699	16.976602
30.533068	843.328226	16.981619
30.526985	853.644197	16.986637
30.148257	830.794069	16.991655
30.409245	852.685922	16.996672
30.546370	853.577058	17.001690
30.625763	858.980561	17.006707
30.689715	860.340784	17.011725
30.690146	858.075314	17.016743
30.961440	862.280077	17.021760
30.789060	857.498332	17.026778
30.882971	854.785338	17.031795
30.589894	838.721793	17.036813
30.491811	847.881237	17.041831
31.059463	851.832352	17.046848
30.655266	854.647518	17.051866
31.105014	859.997397	17.056883
31.115563	858.834405	17.061901
31.321855	854.477856	17.066919
31.235219	834.168369	17.071936
31.036962	832.377553	17.076954
30.833065	808.503421	17.081971
30.516627	836.770371	17.086989
30.725147	828.877348	17.092007
30.804454	853.717064	17.097024
30.919828	849.754012	17.102042
31.170791	851.738481	17.107059
31.286157	853.530623	17.112077
31.068535	851.249551	17.117095
31.392537	853.766474	17.122112
31.106647	862.868402	17.127130
31.234652	859.071599	17.132147
31.136740	852.336921	17.137165
31.063711	864.694454	17.142183
31.082521	853.726069	17.147200
31.251103	874.599822	17.152218
31.662325	881.528418	17.157235
31.679798	884.232407	17.162253
31.623476	886.753267	17.167271
31.449668	901.522776	17.172288
31.470263	889.924699	17.177306
31.764902	889.549886	17.182323
31.965727	884.224788	17.187341
31.747089	887.309344	17.192359
32.054379	891.856407	17.197376
31.932357	885.117211	17.202394
31.796561	872.286251	17.207411
31.731901	866.858709	17.212429
31.948799	865.259750	17.217447
31.955357	861.686705	17.222464
31.920373	866.336668	17.227482
31.865482	859.827865	17.232499
31.671897	870.741348	17.237517
31.750550	882.851273	17.242535
32.008248	879.898073	17.247552
32.156435	887.003274	17.252570
32.181732	873.227122	17.257587
32.132055	872.856759	17.262605
32.198734	885.400841	17.267623
32.579531	870.310944	17.272640
32.294083	876.186844	17.277658
32.318293	869.321843	17.282675
32.085839	878.182626	17.287693
32.340854	880.412430	17.292711
32.302843	886.457925	17.297728
32.321182	880.350097	17.302746
32.427182	881.179588	17.307763
32.349277	873.005708	17.312781
32.243331	885.462892	17.317799
32.413401	871.856470	17.322816
32.361090	884.890372	17.327834
32.233615	876.839810	17.332851
32.335374	864.152526	17.337869
32.250146	868.670376	17.342887
32.668106	879.912227	17.347904
32.101208	896.951750	17.352922
32.992121	896.276188	17.357939
32.992426	907.922329	17.362957
33.021752	906.387720	17.367975
33.387181	900.384790	17.372992
32.894073	901.659754	17.378010
32.839735	908.032677	17.383027
32.788655	909.629479	17.388045
32.916608	903.998385	17.393063
33.641174	906.012052	17.398080
32.951108	893.332002	17.403098
32.856999	896.468110	17.408115
33.281341	900.275638	17.413133
33.110391	888.856225	17.418151
33.150171	894.455118	17.423168
33.029185	904.333065	17.428186
33.077589	904.682137	17.433203
33.170483	912.447506	17.438221
33.004002	913.880451	17.443239
33.250326	894.978959	17.448256
32.949913	914.593397	17.453274
32.894296	901.047762	17.458291
33.449732	923.361611	17.463309
33.549236	930.204570	17.468327
34.056320	923.037855	17.473344
33.656332	917.231170	17.478362
33.857773	915.602977	17.483379
33.563881	896.141407	17.488397
33.354798	888.414779	17.493415
33.640639	900.098256	17.498432
33.471835	918.610807	17.503450
33.640955	924.314881	17.508467
33.892316	927.297078	17.513485
33.747612	927.321753	17.518503
33.888371	921.115155	17.523520
33.818228	919.527118	17.528538
34.166125	915.044125	17.533555
34.016815	920.132775	17.538573
33.996642	921.484963	17.543591
34.437989	915.964536	17.548608
33.931635	918.159572	17.553626
33.849907	915.618568	17.558643
34.202190	927.143190	17.563661
33.925466	916.127852	17.568679
33.933214	924.154185	17.573696
34.204436	913.000282	17.578714
34.075507	927.731700	17.583731
34.241509	919.971609	17.588749
34.028762	928.963876	17.593767
34.272300	916.519491	17.598784
34.290752	925.718470	17.603802
34.144220	920.695287	17.608819
34.155057	928.188172	17.613837
34.503250	943.678939	17.618855
34.553020	932.068629	17.623872
34.400378	945.554979	17.628890
34.561261	938.852158	17.633907
34.763223	934.361000	17.638925
34.750309	935.882420	17.643943
34.702979	927.488354	17.648960
34.981582	930.519974	17.653978
34.866590	934.823229	17.658995
34.880378	927.794511	17.664013
34.523008	930.960846	17.669031
34.425861	928.966741	17.674048
34.800051	918.787995	17.679066
34.652499	932.859273	17.684083
34.853733	922.771590	17.689101
34.947211	925.504650	17.694119
34.732596	940.037891	17.699136
34.859704	919.894174	17.704154
34.601689	940.995955	17.709171
34.866518	947.347838	17.714189
35.102733	950.467550	17.719207
35.307669	958.063676	17.724224
35.287069	951.128995	17.729242
35.398167	953.809456	17.734259
35.869601	957.589439	17.739277
35.431037	955.981098	17.744295
35.527618	952.098937	17.749312
35.353914	969.258557	17.754330
35.475745	950.890436	17.759347
35.646108	950.724103	17.764365
35.346439	957.719335	17.769383
35.702964	963.300647	17.774400
35.591857	957.568718	17.779418
35.597208	959.973519	17.784435
35.716316	949.559020	17.789453
35.574129	965.551607	17.794471
35.762595	952.635211	17.799488
35.643610	958.200830	17.804506
35.755343	954.175844	17.809523
35.759210	962.499026	17.814541
35.807022	955.929618	17.819559
35.836316	961.782962	17.824576
35.824804	944.746207	17.829594
35.944957	951.416809	17.834611
36.093772	954.544667	17.839629
36.059271	954.472311	17.844647
35.968500	954.143572	17.849664
35.971010	959.895068	17.854682
36.126695	966.972302	17.859699
36.451279	982.184107	17.864717
36.461214	982.269328	17.869735
36.769040	966.713165	17.874752
36.330185	964.905413	17.879770
36.164696	942.653754	17.884787
36.495307	955.592557	17.889805
36.055273	946.957249	17.894823
36.417161	963.239869	17.899840
36.618105	975.292660	17.904858
36.463970	976.520963	17.909875
36.575657	983.415265	17.914893
36.613846	968.610769	17.919911
36.732257	982.547810	17.924928
36.561343	975.216505	17.929946
36.274725	985.887436	17.934963
36.416405	982.435502	17.939981
36.564287	976.767829	17.944999
36.665261	975.802925	17.950016
36.794940	972.187269	17.955034
36.585312	977.885661	17.960051
36.887513	973.563512	17.965069
36.824386	972.032956	17.970087
37.021450	972.733751	17.975104
37.053967	983.117748	17.980122
37.175395	989.929952	17.985139
37.674584	979.585761	17.990157
36.918551	976.529852	17.995175
37.084284	959.290015	18.000192
37.268496	972.285890	18.005210
37.253189	986.048229	18.010227
37.751884	989.852645	18.015245
37.350178	971.320385	18.020263
36.823553	970.713460	18.025280
37.332252	983.768491	18.030298
37.518933	991.428070	18.035315
37.674571	995.228562	18.040333
37.628174	991.322686	18.045351
37.556273	999.734473	18.050368
37.804715	994.705135	18.055386
37.126466	993.609708	18.060403
37.685735	1005.669338	18.065421
37.670603	987.896304	18.070439
37.305555	999.335927	18.075456
37.758805	988.078285	18.080474
37.542938	997.643409	18.085491
37.732642	992.265991	18.090509
37.652269	995.487032	18.095527
37.908087	1017.092447	18.100544
38.086823	1015.890138	18.105562
37.952087	1018.676377	18.110579
38.224959	1012.210862	18.115597
38.140898	1006.818358	18.120615
38.066886	1014.759750	18.125632
38.402220	1016.719081	18.130650
38.070697	1007.355151	18.135667
38.325721	1019.636287	18.140685
38.452565	1004.682590	18.145703
38.366366	1019.281967	18.150720
38.470589	1011.801265	18.155738
38.536716	1021.836413	18.160755
38.221478	1007.739633	18.165773
38.264382	1010.043869	18.170791
38.474332	1008.773229	18.175808
38.963511	1007.218610	18.180826
38.384531	1011.103306	18.185843
38.550603	1012.019901	18.190861
38.236451	997.395815	18.195879
38.231475	998.536199	18.200896
38.682004	1004.646643	18.205914
38.505039	1019.243602	18.210931
38.732559	1016.400947	18.215949
39.047239	1043.912865	18.220967
39.095025	1035.788288	18.225984
39.133538	1016.666028	18.231002
38.833897	1007.495404	18.236019
39.188222	1021.527126	18.241037
38.854960	1004.584015	18.246055
39.217399	1026.104321	18.251072
39.116704	1027.407929	18.256090
38.927175	1045.247449	18.261107
39.119954	1040.479006	18.266125
39.116962	1047.866781	18.271143
39.204025	1034.316146	18.276160
39.379654	1042.770890	18.281178
39.237414	1037.619431	18.286195
39.257633	1032.175344	18.291213
39.521748	1043.925596	18.296231
39.325539	1034.391982	18.301248
39.560806	1041.191006	18.306266
39.545416	1036.252978	18.311283
39.402457	1037.934447	18.316301
39.442094	1044.231873	18.321319
39.267016	1029.166371	18.326336
39.624202	1037.427173	18.331354
39.391720	1042.009063	18.336371
39.865722	1056.911772	18.341389
39.826607	1068.935426	18.346407
39.848225	1073.656493	18.351424
40.229437	1055.568239	18.356442
40.149956	1056.797200	18.361459
39.908436	1068.051737	18.366477
40.263314	1060.507844	18.371495
40.109835	1057.066981	18.376512
40.081335	1059.389026	18.381530
39.844410	1044.375846	18.386547
40.233007	1050.836520	18.391565
40.127497	1050.659686	18.396583
40.054145	1055.365937	18.401600
40.380003	1050.629325	18.406618
40.489200	1064.012388	18.411635
40.425591	1042.946709	18.416653
40.404542	1060.941040	18.421671
40.419914	1047.844851	18.426688
40.744407	1052.515369	18.431706
40.275361	1060.059674	18.436723
40.335416	1061.744990	18.441741
40.594927	1059.734342	18.446759
40.343973	1068.529214	18.451776
40.586194	1073.729452	18.456794
40.568132	1081.135478	18.461811
40.449138	1083.998734	18.466829
40.920892	1093.856788	18.471847
40.903258	1084.022044	18.476864
40.908851	1088.772923	18.481882
40.729515	1089.888103	18.486899
40.891635	1072.542757	18.491917
41.092512	1091.246926	18.496935
40.764623	1082.113299	18.501952
40.990674	1075.117335	18.506970
40.921037	1087.436923	18.511987
41.295648	1100.572663	18.517005
41.403968	1101.405424	18.522023
41.475454	1099.971973	18.527040
41.542579	1103.549675	18.532058
41.338513	1081.027286	18.537075
41.756263	1081.294665	18.542093
41.445888	1076.732752	18.547111
41.256507	1076.633443	18.552128
41.733912	1084.953816	18.557146
41.047848	1097.430873	18.562163
41.416290	1111.139259	18.567181
41.838856	1096.131882	18.572199
41.528696	1108.475489	18.577216
41.836813	1102.542469	18.582234
41.873120	1097.452900	18.587251
41.948161	1110.099008	18.592269
41.897437	1101.419451	18.597287
41.787996	1098.421884	18.602304
42.160377	1095.634687	18.607322
41.968518	1095.779136	18.612339
41.985226	1106.183935	18.617357
42.076848	1091.153908	18.622375
41.829348	1097.743924	18.627392
41.889147	1087.375049	18.632410
42.083792	1089.197243	18.637427
42.066508	1090.638022	18.642445
42.242257	1090.457219	18.647463
41.986988	1082.971828	18.652480
42.568211	1096.732322	18.657498
42.400148	1099.591488	18.662515
42.695544	1120.114681	18.667533
42.615662	1094.826824	18.672551
42.832155	1103.753870	18.677568
42.701961	1091.833099	18.682586
42.729487	1093.506476	18.687603
42.611579	1081.799479	18.692621
42.740889	1085.291131	18.697639
42.388029	1093.246465	18.702656
43.081000	1114.471979	18.707674
43.082019	1126.950257	18.712691
42.844632	1125.396526	18.717709
43.132901	1114.280104	18.722727
42.971858	1135.857942	18.727744
42.981402	1119.146866	18.732762
43.381621	1119.017039	18.737779
43.061724	1105.107018	18.742797
43.407144	1107.115765	18.747815
43.110031	1104.952268	18.752832
43.343363	1120.276020	18.757850
43.292672	1121.117936	18.762867
43.247470	1111.091025	18.767885
43.297761	1114.809963	18.772903
43.062073	1118.975574	18.777920
43.138802	1110.557463	18.782938
43.067361	1108.535667	18.787955
43.160814	1112.112268	18.792973
43.667375	1098.759218	18.797991
43.293937	1126.881435	18.803008
43.070256	1122.748189	18.808026
43.577658	1136.201799	18.813043
43.023339	1146.096011	18.818061
43.500842	1137.520832	18.823079
43.265167	1140.391178	18.828096
44.080560	1156.744405	18.833114
44.106757	1159.474653	18.838131
44.078433	1158.176560	18.843149
44.427914	1130.902486	18.848167
44.434912	1146.766894	18.853184
44.192242	1135.344092	18.858202
44.100222	1145.995081	18.863219
44.070087	1125.424329	18.868237
44.212999	1133.677197	18.873255
44.076234	1134.904019	18.878272
44.219629	1142.903230	18.883290
44.319239	1153.584846	18.888307
44.716876	1163.754532	18.893325
44.796147	1162.173957	18.898343
44.386225	1153.671613	18.903360
44.582450	1151.189043	18.908378
44.605905	1149.298868	18.913395
44.291413	1159.424654	18.918413
44.739491	1147.574778	18.923431
44.743153	1158.282486	18.928448
44.620875	1148.886155	18.933466
44.778871	1154.706497	18.938483
44.670506	1163.637863	18.943501
44.645020	1155.169803	18.948519
44.352719	1156.879407	18.953536
44.705921	1161.141864	18.958554
44.679161	1162.899890	18.963571
44.843334	1171.648559	18.968589
44.844984	1182.533545	18.973607
45.146379	1185.678058	18.978624
45.112914	1181.639416	18.983642
45.450138	1179.160307	18.988659
45.332211	1181.837326	18.993677
45.523178	1161.636391	18.998695
45.488215	1178.056261	19.003712
45.480433	1182.491146	19.008730
45.884051	1176.581972	19.013747
45.673907	1180.333336	19.018765
45.971782	1167.752140	19.023783
45.513783	1178.162124	19.028800
45.631862	1185.909989	19.033818
45.864811	1179.641803	19.038835
45.817705	1170.105409	19.043853
45.911089	1170.596823	19.048871
45.571895	1174.587472	19.053888
45.757649	1164.360193	19.058906
45.609154	1172.188216	19.063923
45.743909	1179.559000	19.068941
45.984411	1169.187171	19.073959
45.711495	1176.304233	19.078976
46.133691	1176.073061	19.083994
46.257100	1166.811275	19.089011
46.075481	1177.281271	19.094029
46.283248	1194.489597	19.099047
45.989196	1212.091721	19.104064
46.151665	1202.363230	19.109082
46.403186	1204.333878	19.114099
46.075991	1209.129454	19.119117
46.255774	1209.544993	19.124135
46.671003	1223.860373	19.129152
46.487151	1208.993244	19.134170
46.535383	1205.620763	19.139187
46.099830	1213.769212	19.144205
46.630959	1215.059057	19.149223
46.938871	1234.021341	19.154240
46.797737	1235.162101	19.159258
47.081868	1225.220326	19.164275
46.577150	1228.390405	19.169293
46.837200	1231.480553	19.174311
46.841917	1217.136755	19.179328
46.785818	1233.033033	19.184346
47.057786	1223.330126	19.189363
46.917565	1228.352528	19.194381
47.430355	1233.022492	19.199399
47.079984	1217.247356	19.204416
46.917502	1234.299932	19.209434
47.188233	1220.090282	19.214451
47.235659	1249.370554	19.219469
47.355934	1253.633052	19.224487
47.570281	1247.791045	19.229504
47.693285	1263.716308	19.234522
47.651789	1245.998599	19.239539
47.647734	1251.326976	19.244557
48.102340	1246.511562	19.249575
48.005977	1241.242930	19.254592
48.019681	1237.055763	19.259610
48.066825	1226.876341	19.264627
48.110623	1223.202099	19.269645
48.052017	1210.348061	19.274663
47.628745	1215.838003	19.279680
47.483784	1221.180896	19.284698
47.785064	1233.441671	19.289715
47.763029	1241.441308	19.294733
48.299893	1264.844309	19.299751
48.047137	1253.855959	19.304768
48.153822	1258.128577	19.309786
48.336433	1246.285789	19.314803
48.225584	1253.871466	19.319821
48.514098	1251.970247	19.324839
48.211129	1256.113064	19.329856
47.973132	1247.014865	19.334874
48.501829	1240.032973	19.339891
48.236934	1256.532153	19.344909
48.471790	1261.101434	19.349927
48.488206	1266.206503	19.354944
48.274886	1279.551634	19.359962
48.442360	1270.219822	19.364979
48.540336	1280.667597	19.369997
48.647170	1290.299334	19.375015
48.765704	1272.632100	19.380032
48.387677	1278.811872	19.385050
48.880985	1279.181212	19.390067
48.720647	1304.151620	19.395085
49.263260	1287.574663	19.400103
49.164901	1297.776314	19.405120
49.221487	1300.574384	19.410138
49.301709	1302.661718	19.415155
49.342625	1308.780046	19.420173
49.561493	1297.049115	19.425191
49.526042	1299.687629	19.430208
49.451363	1292.995830	19.435226
49.727429	1304.375100	19.440243
49.570658	1294.262394	19.445261
49.320075	1305.347872	19.450279
49.808103	1293.936262	19.455296
49.482385	1304.303315	19.460314
49.752976	1295.895379	19.465331
49.408002	1301.613895	19.470349
49.407312	1313.491265	19.475367
49.690018	1313.213965	19.480384
49.821862	1338.243405	19.485402
50.032793	1328.168121	19.490419
50.020247	1329.609321	19.495437
50.094207	1330.654715	19.500455
50.089666	1330.019065	19.505472
50.007540	1348.650854	19.510490
50.037578	1326.097094	19.515507
50.012951	1333.078043	19.520525
50.010471	1330.117763	19.525543
50.317439	1344.776369	19.530560
50.283662	1372.002737	19.535578
50.527040	1346.271958	19.540595
50.484805	1359.829287	19.545613
50.713503	1363.999605	19.550631
50.938916	1352.566401	19.555648
50.699711	1349.281339	19.560666
51.017405	1359.018993	19.565683
50.832644	1351.265575	19.570701
50.954384	1359.217013	19.575719
51.274202	1350.578128	19.580736
50.861820	1350.565163	19.585754
51.073897	1340.191618	19.590771
51.112919	1348.382851	19.595789
51.064706	1358.391651	19.600807
50.924209	1352.976861	19.605824
51.014485	1350.842207	19.610842
50.954463	1357.681509	19.615859
51.177884	1349.585505	19.620877
51.107160	1355.888012	19.625895
51.163277	1352.855853	19.630912
51.260863	1376.502345	19.635930
51.422917	1372.834209	19.640947
51.590443	1381.139234	19.645965
51.653120	1381.251561	19.650983
51.555483	1382.856892	19.656000
51.522272	1383.059065	19.661018
51.796062	1384.009742	19.666035
51.557496	1386.615708	19.671053
51.616162	1385.466670	19.676071
51.618653	1363.006857	19.681088
51.583477	1383.578634	19.686106
51.963136	1399.313430	19.691123
51.902213	1401.134794	19.696141
52.047087	1414.084703	19.701159
52.101514	1398.297004	19.706176
51.876305	1408.586212	19.711194
51.952307	1420.739807	19.716211
51.756244	1398.995283	19.721229
52.128208	1419.530827	19.726247
52.599234	1416.658980	19.731264
52.511195	1439.940660	19.736282
52.671781	1431.158394	19.741299
52.724300	1435.494823	19.746317
52.593725	1451.423512	19.751335
52.699741	1435.494109	19.756352
52.645775	1439.379437	19.761370
52.973426	1434.195657	19.766387
52.625351	1432.156946	19.771405
52.726162	1432.409299	19.776423
52.800462	1427.198210	19.781440
52.689147	1430.219873	19.786458
52.828044	1431.005187	19.791475
52.970421	1429.071021	19.796493
53.164646	1459.152947	19.801511
53.514699	1454.652321	19.806528
52.891702	1460.375113	19.811546
53.302667	1468.251949	19.816563
53.331847	1462.315683	19.821581
53.508422	1471.592972	19.826599
53.945191	1463.191534	19.831616
53.382592	1468.667096	19.836634
53.651336	1466.258399	19.841651
53.556665	1457.304662	19.846669
53.540191	1467.409153	19.851687
53.872274	1463.330204	19.856704
53.575915	1466.698429	19.861722
53.626668	1475.784057	19.866739
53.837896	1465.584645	19.871757
54.040506	1489.824753	19.876775
54.219202	1481.847465	19.881792
54.147607	1492.178751	19.886810
54.148853	1498.729900	19.891827
54.339095	1494.161694	19.896845
54.205915	1491.857887	19.901863
54.404102	1496.631681	19.906880
54.134518	1489.426547	19.911898
54.000699	1487.932124	19.916915
54.364160	1494.231036	19.921933
54.307669	1488.060740	19.926951
54.746951	1493.725698	19.931968
54.356711	1483.128132	19.936986
54.417303	1500.920552	19.942003
54.699031	1501.340017	19.947021
54.422824	1530.974145	19.952039
54.732406	1521.262079	19.957056
54.829119	1526.449418	19.962074
54.655556	1522.944066	19.967091
54.809346	1526.377160	19.972109
54.524617	1519.620091	19.977127
54.633358	1521.581803	19.982144
55.023695	1546.200539	19.987162
55.192763	1540.685227	19.992179
55.403156	1561.112649	19.997197
55.202165	1549.062895	20.002215
55.585110	1548.184995	20.007232
55.396189	1551.831977	20.012250
55.526684	1544.129791	20.017267
55.635747	1543.530368	20.022285
55.582087	1542.642939	20.027303
55.561658	1545.975326	20.032320
55.671923	1558.394475	20.037338
55.531261	1547.799609	20.042355
55.670932	1537.203200	20.047373
55.433303	1549.231596	20.052391
55.680779	1555.118193	20.057408
55.962558	1566.791044	20.062426
55.727796	1575.113449	20.067443
56.213196	1568.190129	20.072461
56.177057	1583.198318	20.077479
56.256491	1580.581172	20.082496
56.288296	1582.476684	20.087514
56.282679	1579.002609	20.092531
56.473440	1568.705449	20.097549
56.557216	1566.370699	20.102567
56.461888	1562.239740	20.107584
56.506240	1562.356376	20.112602
56.281053	1567.497829	20.117619
56.714928	1577.852907	20.122637
56.625171	1588.895580	20.127655
57.075635	1585.126497	20.132672
57.056776	1596.290896	20.137690
57.310042	1595.483428	20.142707
57.269928	1583.644711	20.147725
57.040622	1569.177576	20.152743
57.248496	1571.404745	20.157760
56.729230	1578.541839	20.162778
56.741778	1578.979513	20.167795
57.231265	1584.058472	20.172813
57.255477	1589.001665	20.177831
57.433032	1581.640136	20.182848
57.582102	1586.324555	20.187866
57.447819	1604.037411	20.192883
57.857114	1590.847421	20.197901
57.635906	1596.977493	20.202919
57.455322	1595.809620	20.207936
57.458945	1593.652841	20.212954
57.321864	1603.000344	20.217971
57.821186	1598.763927	20.222989
57.531473	1619.975107	20.228007
57.799721	1615.774902	20.233024
57.964844	1628.049046	20.238042
57.849200	1618.318916	20.243059
58.100262	1620.532165	20.248077
58.063346	1621.239477	20.253095
58.102872	1618.297786	20.258112
58.214242	1617.556177	20.263130
58.067168	1618.108892	20.268147
58.664873	1631.394211	20.273165
58.610746	1647.328774	20.278183
58.874798	1646.935185	20.283200
58.578864	1644.061321	20.288218
58.732422	1635.245855	20.293235
59.158050	1627.789778	20.298253
58.707553	1608.428556	20.303271
59.029998	1615.936513	20.308288
58.848342	1602.347907	20.313306
58.887665	1622.692285	20.318323
58.871531	1611.855779	20.323341
58.571280	1612.012926	20.328359
58.889950	1620.613218	20.333376
58.917585	1628.987548	20.338394
58.927692	1643.812894	20.343411
59.298499	1636.126747	20.348429
58.948615	1638.564081	20.353447
58.952530	1646.816086	20.358464
59.458670	1653.637834	20.363482
59.436392	1668.867198	20.368499
59.565338	1670.057435	20.373517
59.504116	1667.222817	20.378535
59.768228	1675.996001	20.383552
59.641561	1678.974589	20.388570
59.836934	1675.098061	20.393587
59.803920	1674.679560	20.398605
59.762145	1673.334443	20.403623
59.848215	1658.112591	20.408640
59.885173	1665.126025	20.413658
59.731002	1666.218391	20.418675
60.040490	1684.425710	20.423693
60.177357	1685.582854	20.428711
60.619741	1687.208604	20.433728
60.483529	1688.693398	20.438746
60.332975	1680.314893	20.443763
60.711636	1678.126340	20.448781
60.565157	1679.849495	20.453799
60.218590	1684.914705	20.458816
60.447362	1681.813604	20.463834
60.350912	1680.017179	20.468851
60.562345	1684.997267	20.473869
60.794227	1707.022493	20.478887
60.335538	1701.663505	20.483904
60.755770	1720.737728	20.488922
60.746008	1711.418010	20.493939
60.965023	1724.856030	20.498957
60.773021	1723.109536	20.503975
61.173161	1735.289922	20.508992
61.417303	1728.848535	20.514010
61.301139	1742.880337	20.519027
61.634623	1728.882345	20.524045
61.489115	1735.515413	20.529063
61.700395	1727.804410	20.534080
61.917775	1731.595573	20.539098
61.727611	1722.754096	20.544115
62.453752	1723.523276	20.549133
62.126567	1711.663013	20.554151
61.611694	1691.060109	20.559168
61.802522	1701.411939	20.564186
62.101959	1708.366963	20.569203
62.175556	1717.629043	20.574221
62.343228	1731.154179	20.579239
61.801977	1727.060058	20.584256
61.743880	1727.307777	20.589274
61.891683	1731.684243	20.594291
62.093125	1731.380215	20.599309
62.099000	1725.813375	20.604327
62.044826	1737.827741	20.609344
62.125019	1732.789261	20.614362
62.285344	1767.019600	20.619379
62.662655	1763.212180	20.624397
62.306543	1758.640102	20.629415
62.404488	1774.255137	20.634432
62.409444	1757.633476	20.639450
62.336826	1782.434192	20.644467
62.820585	1780.579371	20.649485
62.987247	1785.423906	20.654503
63.006526	1783.481105	20.659520
63.178570	1786.873552	20.664538
63.194426	1794.426159	20.669555
63.300481	1788.976181	20.674573
63.326410	1786.532081	20.679591
63.440728	1777.340709	20.684608
63.386087	1779.371570	20.689626
63.540911	1773.431446	20.694643
63.462301	1776.356352	20.699661
63.589966	1785.555514	20.704679
63.466310	1787.161447	20.709696
63.800165	1800.373312	20.714714
63.518388	1797.098336	20.719731
63.703761	1815.719258	20.724749
63.930697	1814.449781	20.729767
63.728594	1813.960909	20.734784
64.113381	1801.066368	20.739802
63.856093	1810.471157	20.744819
63.985755	1813.294639	20.749837
64.413416	1801.340668	20.754855
64.073415	1813.999653	20.759872
64.667830	1813.473139	20.764890
64.580765	1834.153485	20.769907
65.074432	1834.528589	20.774925
64.984038	1820.680365	20.779943
64.705141	1812.401624	20.784960
64.776771	1797.839277	20.789978
64.649424	1807.587778	20.794995
65.081940	1808.225990	20.800013
64.890378	1817.135466	20.805031
64.987684	1826.540812	20.810048
65.078709	1819.292957	20.815066
65.039685	1828.298176	20.820083
65.220328	1832.547121	20.825101
65.377317	1836.092925	20.830119
65.109017	1836.491007	20.835136
65.370781	1820.750487	20.840154
65.411591	1823.204966	20.845171
65.254601	1829.198952	20.850189
65.266564	1834.991136	20.855207
65.398856	1833.193108	20.860224
65.763808	1849.080672	20.865242
65.666806	1855.933982	20.870259
65.901063	1858.893704	20.875277
65.773018	1850.550848	20.880295
65.773067	1857.161688	20.885312
65.856294	1849.282843	20.890330
66.005273	1860.978750	20.895347
65.858345	1848.853795	20.900365
66.017422	1856.578202	20.905383
65.960928	1881.361750	20.910400
66.337642	1871.928967	20.915418
66.083799	1885.843321	20.920435
66.183955	1886.303430	20.925453
66.544649	1879.442598	20.930471
66.277139	1881.671119	20.935488
66.882389	1884.207009	20.940506
66.941759	1890.295655	20.945523
67.205353	1885.670241	20.950541
67.271148	1881.865065	20.955559
67.251617	1881.759035	20.960576
67.223132	1872.721396	20.965594
67.030015	1870.101905	20.970611
67.228070	1868.715860	20.975629
67.567916	1869.192158	20.980647
67.251064	1873.893530	20.985664
67.401405	1862.623802	20.990682
67.271007	1879.863587	20.995699
67.534923	1870.442752	21.000717
67.549788	1884.284263	21.005735
67.735386	1899.061373	21.010752
67.936494	1905.336407	21.015770
67.816935	1906.952894	21.020787
68.093906	1897.220099	21.025805
67.993261	1898.580947	21.030823
67.731513	1895.905875	21.035840
68.296068	1899.310933	21.040858
68.081724	1913.053855	21.045875
67.529290	1906.727395	21.050893
67.878927	1910.082355	21.055911
67.643222	1899.223474	21.060928
68.121820	1908.401327	21.065946
68.338463	1937.576717	21.070963
68.558105	1920.877679	21.075981
68.365429	1922.853331	21.080999
68.382116	1937.285918	21.086016
68.616252	1932.616646	21.091034
68.532538	1927.951777	21.096051
68.571390	1925.235688	21.101069
68.962845	1944.858941	21.106087
68.957357	1956.827252	21.111104
69.255562	1964.072013	21.116122
69.138086	1951.519745	21.121139
69.075466	1962.445820	21.126157
68.997970	1955.381725	21.131175
68.946725	1952.424167	21.136192
69.623026	1959.181524	21.141210
69.424513	1944.147039	21.146227
69.687448	1947.546546	21.151245
69.748947	1956.794237	21.156263
69.243222	1946.549427	21.161280
69.697618	1955.542660	21.166298
69.754026	1965.322598	21.171315
70.049646	1974.412245	21.176333
70.588390	1948.161164	21.181351
70.114378	1968.212449	21.186368
70.464209	1960.110785	21.191386
70.421597	1960.668293	21.196403
70.218450	1959.196695	21.201421
70.447913	1947.727741	21.206439
70.627200	1964.731737	21.211456
70.392996	1964.678402	21.216474
70.696074	1962.149607	21.221491
70.390669	1960.349692	21.226509
70.672056	1957.016457	21.231527
70.185611	1967.660666	21.236544
70.403000	1964.592586	21.241562
70.676863	1977.446670	21.246579
71.046361	1990.611775	21.251597
71.183689	1977.359918	21.256615
71.017651	2014.448964	21.261632
71.064996	1989.930592	21.266650
71.192029	2000.256460	21.271667
70.921421	1994.881050	21.276685
71.270253	1996.434416	21.281703
71.084364	1988.281227	21.286720
71.392051	1996.484306	21.291738
71.720847	2007.810809	21.296755
71.411721	2017.869255	21.301773
71.913133	2016.113539	21.306791
71.643442	2029.293961	21.311808
71.691619	2014.046626	21.316826
71.974459	2012.344545	21.321843
71.818362	2015.220895	21.326861
72.168985	1992.202033	21.331879
72.093627	2013.650431	21.336896
72.268043	2016.334001	21.341914
72.189563	1990.332256	21.346931
71.959176	2017.045406	21.351949
72.292415	2019.088568	21.356967
72.397512	2048.291064	21.361984
72.671604	2042.133328	21.367002
72.759293	2028.934110	21.372019
72.643839	2044.750797	21.377037
72.932449	2040.851784	21.382055
73.265579	2043.702307	21.387072
72.999217	2041.302235	21.392090
73.168541	2029.682458	21.397107
72.989743	2035.356562	21.402125
72.961773	2023.780511	21.407143
72.876123	2038.322410	21.412160
72.916113	2021.597545	21.417178
73.378088	2035.239249	21.422195
73.151251	2040.455233	21.427213
73.815636	2051.568074	21.432231
73.817223	2041.326657	21.437248
73.757866	2046.349642	21.442266
74.176320	2048.701702	21.447283
74.156833	2050.602894	21.452301
74.094367	2048.208689	21.457319
74.176855	2049.593215	21.462336
74.235398	2049.279731	21.467354
74.165744	2044.372388	21.472371
73.819442	2036.867619	21.477389
74.213318	2043.586463	21.482407
74.082396	2033.049778	21.487424
74.124436	2045.931108	21.492442
74.480405	2062.372547	21.497459
74.545076	2066.656664	21.502477
74.492030	2074.086565	21.507495
74.446693	2072.865995	21.512512
74.576865	2073.812207	21.517530
74.467232	2076.659339	21.522547
74.613701	2083.391823	21.527565
75.047391	2084.683286	21.532583
75.384691	2110.583721	21.537600
75.223840	2100.870202	21.542618
75.508763	2102.086266	21.547635
75.520333	2097.941926	21.552653
75.754374	2108.591367	21.557671
75.627569	2099.315652	21.562688
75.713494	2091.184706	21.567706
75.787548	2083.648439	21.572723
75.853514	2093.950609	21.577741
76.144530	2083.541771	21.582759
75.895495	2100.841853	21.587776
75.597831	2089.213288	21.592794
75.994806	2083.423155	21.597811
75.712177	2094.814051	21.602829
75.954281	2083.192343	21.607847
75.924775	2085.433031	21.612864
76.029513	2113.588253	21.617882
76.439675	2107.447468	21.622899
76.503970	2130.494330	21.627917
76.209929	2129.333846	21.632935
76.187648	2125.255515	21.637952
76.616130	2127.422695	21.642970
76.576107	2125.809478	21.647987
76.599387	2147.649176	21.653005
76.852824	2152.848521	21.658023
76.713976	2142.190356	21.663040
77.034342	2156.091946	21.668058
77.185359	2143.012262	21.673075
77.070641	2144.145574	21.678093
77.226524	2133.585931	21.683111
77.128755	2141.752266	21.688128
77.191970	2150.320082	21.693146
77.523662	2157.115677	21.698163
77.605609	2175.281371	21.703181
77.838217	2170.233308	21.708199
77.794200	2165.735400	21.713216
77.885724	2181.518222	21.718234
78.329403	2161.623172	21.723251
78.113153	2168.820288	21.728269
78.137204	2171.299341	21.733287
78.236372	2166.723648	21.738304
78.261949	2166.571784	21.743322
78.514320	2157.113908	21.748339
78.294148	2156.687941	21.753357
78.616442	2173.578100	21.758375
78.230969	2163.492081	21.763392
78.242006	2165.264150	21.768410
78.742154	2179.177188	21.773427
78.771494	2191.196512	21.778445
78.747948	2191.429080	21.783463
78.913188	2187.121748	21.788480
78.992812	2205.296915	21.793498
79.240052	2186.379414	21.798515
79.136149	2193.464291	21.803533
79.353959	2187.701659	21.808551
79.310176	2187.636441	21.813568
79.114926	2181.523434	21.818586
79.740205	2183.304815	21.823603
79.448028	2190.799676	21.828621
79.341739	2209.161252	21.833639
79.410808	2219.870703	21.838656
79.543044	2216.259057	21.843674
79.595719	2211.434382	21.848691
79.734940	2225.327392	21.853709
79.871369	2238.501701	21.858727
80.298911	2245.458831	21.863744
80.287661	2244.932010	21.868762
80.195160	2253.891697	21.873779
80.036150	2252.393783	21.878797
80.219227	2239.254398	21.883815
80.330340	2246.264407	21.888832
80.342995	2256.436049	21.893850
80.609197	2269.272455	21.898867
80.486066	2279.797206	21.903885
80.805343	2278.445614	21.908903
80.824792	2272.418334	21.913920
81.141528	2280.980545	21.918938
81.301319	2272.484992	21.923955
80.984258	2293.903063	21.928973
80.920837	2288.642108	21.933991
81.484921	2289.637282	21.939008
81.317816	2298.645341	21.944026
81.563390	2287.045541	21.949043
81.939323	2305.977248	21.954061
81.582288	2285.186364	21.959079
81.761106	2295.259523	21.964096
81.732433	2290.331551	21.969114
81.651614	2304.569802	21.974131
81.949817	2302.275973	21.979149
82.384685	2301.173937	21.984167
82.366840	2305.214217	21.989184
82.388771	2314.417195	21.994202
82.844535	2297.773006	21.999219
82.529365	2291.265861	22.004237
82.268034	2281.381262	22.009255
82.468824	2294.389496	22.014272
82.496319	2299.311513	22.019290
82.775635	2314.786123	22.024307
82.667647	2314.971239	22.029325
83.011023	2307.592788	22.034343
83.428854	2307.890001	22.039360
83.259327	2294.873981	22.044378
83.249157	2312.659255	22.049395
83.557477	2305.095486	22.054413
83.331314	2310.225537	22.059431
83.586426	2297.742401	22.064448
83.305802	2309.587088	22.069466
83.444124	2307.611364	22.074483
83.293042	2303.351348	22.079501
83.502116	2301.258044	22.084519
83.626952	2314.448308	22.089536
83.566376	2340.941962	22.094554
83.746342	2333.958948	22.099571
83.636595	2325.478972	22.104589
83.792482	2343.328560	22.109607
83.882983	2347.102955	22.114624
83.928161	2368.638804	22.119642
84.142490	2369.754959	22.124659
84.370704	2357.334478	22.129677
84.456197	2370.929852	22.134695
84.619380	2372.939166	22.139712
84.612795	2386.569451	22.144730
84.765217	2395.626523	22.149747
85.225173	2394.664605	22.154765
85.137946	2391.639100	22.159783
85.380859	2387.269475	22.164800
85.294784	2403.244052	22.169818
85.301664	2386.259636	22.174835
85.602510	2388.110004	22.179853
85.329749	2391.068782	22.184871
85.616041	2380.021153	22.189888
85.822558	2390.104559	22.194906
85.335583	2381.378862	22.199923
85.408363	2384.235469	22.204941
85.832405	2404.654791	22.209959
86.127217	2406.075514	22.214976
85.688354	2413.660657	22.219994
85.985850	2411.331698	22.225011
85.889553	2420.291913	22.230029
85.739394	2419.737850	22.235047
86.277349	2422.683321	22.240064
86.490629	2436.882938	22.245082
86.725298	2434.156347	22.250099
86.850374	2446.029754	22.255117
86.646636	2443.669065	22.260135
86.759171	2438.157757	22.265152
86.663034	2438.896148	22.270170
86.498563	2429.863036	22.275187
86.937355	2440.386565	22.280205
86.975719	2480.389273	22.285223
87.250324	2462.956064	22.290240
87.529915	2472.598772	22.295258
87.718570	2457.882132	22.300275
87.904533	2462.565448	22.305293
87.463885	2456.570823	22.310311
87.463686	2456.375585	22.315328
87.626983	2474.973204	22.320346
87.692655	2457.480839	22.325363
87.687163	2473.126471	22.330381
87.834976	2479.437119	22.335399
87.992155	2485.919229	22.340416
88.077508	2489.038306	22.345434
87.932698	2485.483203	22.350451
88.458508	2473.167172	22.355469
88.246141	2490.898478	22.360487
88.328994	2479.133520	22.365504
88.421283	2495.204292	22.370522
88.387134	2511.497519	22.375539
88.941431	2511.399800	22.380557
88.947256	2510.536338	22.385575
89.070286	2513.861566	22.390592
89.270862	2498.960659	22.395610
89.107765	2508.109103	22.400627
89.249917	2505.922515	22.405645
89.248987	2509.389073	22.410663
89.488771	2509.291364	22.415680
89.214459	2519.377744	22.420698
89.712208	2529.954182	22.425715
89.834293	2522.104788	22.430733
89.887711	2531.320209	22.435751
90.035393	2529.693057	22.440768
90.144745	2538.584127	22.445786
89.824087	2528.720588	22.450803
89.934146	2514.196973	22.455821
89.833767	2541.467911	22.460839
90.167708	2531.170068	22.465856
90.336612	2547.022752	22.470874
90.669429	2548.322855	22.475891
90.602574	2541.398443	22.480909
90.384987	2562.567018	22.485927
90.657959	2549.690625	22.490944
91.148291	2549.965826	22.495962
90.999486	2561.875132	22.500979
91.240866	2556.809157	22.505997
90.916238	2556.470507	22.511015
91.427565	2572.654571	22.516032
91.161524	2578.342995	22.521050
91.299465	2576.316126	22.526067
91.554786	2570.556010	22.531085
91.346650	2579.636949	22.536103
91.513665	2568.828746	22.541120
91.409198	2578.991613	22.546138
91.556369	2590.749095	22.551155
91.874840	2609.321630	22.556173
91.944508	2599.183142	22.561191
92.370312	2586.316105	22.566208
92.637024	2588.195363	22.571226
92.422278	2587.660430	22.576243
92.621556	2585.742896	22.581261
92.745491	2583.712436	22.586279
92.963969	2588.293975	22.591296
92.802399	2584.910295	22.596314
92.883808	2589.699498	22.601331
93.017258	2585.382152	22.606349
93.233801	2613.802061	22.611367
93.398667	2608.485362	22.616384
93.441899	2610.154932	22.621402
93.306292	2612.757866	22.626419
93.547343	2603.088429	22.631437
93.591042	2607.879145	22.636455
93.511748	2591.869436	22.641472
93.717542	2589.496360	22.646490
93.564393	2600.325067	22.651507
93.585557	2608.139759	22.656525
93.585410	2609.940102	22.661543
94.027708	2622.521163	22.666560
94.612659	2634.416153	22.671578
94.322695	2624.317984	22.676595
94.881632	2628.868077	22.681613
94.741293	2638.319685	22.686631
94.647766	2619.934865	22.691648
94.660388	2622.339512	22.696666
94.703763	2639.272337	22.701683
94.843549	2625.995111	22.706701
94.916044	2640.939933	22.711719
95.182714	2635.069074	22.716736
94.956922	2634.667049	22.721754
94.789506	2639.659960	22.726771
95.175838	2628.995963	22.731789
94.898186	2635.830264	22.736807
95.001230	2633.057091	22.741824
95.303901	2647.330506	22.746842
95.089745	2665.207171	22.751859
95.545308	2653.546809	22.756877
95.610024	2654.903033	22.761895
95.754843	2666.079347	22.766912
96.025034	2683.922450	22.771930
95.887363	2680.392103	22.776947
95.894410	2684.061883	22.781965
95.853233	2694.085644	22.786983
95.856503	2683.049138	22.792000
96.079625	2714.274269	22.797018
96.196127	2712.337331	22.802035
96.621702	2707.494971	22.807053
96.485288	2726.638615	22.812071
96.607404	2724.653903	22.817088
96.870859	2753.183822	22.822106
96.888627	2735.023947	22.827123
97.256696	2735.120168	22.832141
97.289960	2739.604028	22.837159
97.209380	2730.327968	22.842176
97.420705	2746.714133	22.847194
97.756147	2758.102685	22.852211
98.381344	2754.046905	22.857229
97.938676	2764.636991	22.862247
98.060601	2760.549621	22.867264
98.178066	2760.347926	22.872282
98.032229	2757.059234	22.877299
98.354242	2759.431871	22.882317
98.315322	2757.735345	22.887335
98.163327	2761.064345	22.892352
98.488249	2758.550118	22.897370
98.513452	2740.614766	22.902387
98.784039	2754.193475	22.907405
98.685431	2754.196951	22.912423
98.669039	2760.182137	22.917440
98.899902	2777.930287	22.922458
99.022384	2779.704087	22.927475
99.103481	2787.046230	22.932493
98.945386	2790.038294	22.937511
98.889881	2784.583759	22.942528
99.393042	2803.124436	22.947546
99.279351	2813.690309	22.952563
99.543090	2797.268039	22.957581
99.643143	2817.065744	22.962599
99.537279	2818.006523	22.967616
99.721713	2814.014112	22.972634
99.861570	2853.623114	22.977651
100.187814	2851.025199	22.982669
100.282573	2851.234685	22.987687
100.444443	2840.732421	22.992704
100.621246	2828.672179	22.997722
100.506703	2842.761598	23.002739
100.632246	2839.581176	23.007757
100.695739	2840.877586	23.012775
100.886690	2852.867770	23.017792
101.328729	2853.421398	23.022810
100.910409	2861.104139	23.027827
101.275910	2863.509956	23.032845
101.584462	2856.281470	23.037863
101.535678	2866.497325	23.042880
101.464295	2852.060454	23.047898
101.490739	2855.707387	23.052915
101.482149	2846.360117	23.057933
101.570665	2858.424114	23.062951
101.364086	2848.369885	23.067968
101.542855	2849.610638	23.072986
101.365153	2877.679301	23.078003
101.960115	2880.032836	23.083021
101.854748	2894.583525	23.088039
102.098014	2898.652264	23.093056
102.388262	2884.047746	23.098074
102.427523	2905.940007	23.103091
102.576130	2908.992622	23.108109
102.899565	2897.732803	23.113127
102.970797	2909.171030	23.118144
103.068380	2908.614000	23.123162
103.162435	2917.711730	23.128179
103.036803	2903.274918	23.133197
103.021181	2915.115644	23.138215
103.231885	2917.610230	23.143232
103.726388	2918.164836	23.148250
103.395008	2922.114388	23.153267
103.736874	2927.459997	23.158285
103.792454	2918.243205	23.163303
103.758989	2920.570682	23.168320
103.921964	2919.571597	23.173338
103.775906	2948.370310	23.178355
104.037794	2945.137813	23.183373
104.380756	2946.430568	23.188391
104.624399	2952.965509	23.193408
104.658856	2958.358186	23.198426
104.311089	2958.403619	23.203443
104.589477	2980.128337	23.208461
104.771327	2979.739643	23.213479
104.816606	2992.357284	23.218496
105.163981	2986.646364	23.223514
105.153570	2987.718214	23.228531
105.205459	2981.223144	23.233549
105.522005	2983.120199	23.238567
105.259879	2999.603761	23.243584
105.824275	3004.557155	23.248602
105.607360	2996.908795	23.253619
105.848561	2995.176388	23.258637
106.139187	3001.554785	23.263655
105.839761	3009.910986	23.268672
106.161521	3001.197738	23.273690
106.035121	3010.263848	23.278707
106.425321	3022.985526	23.283725
106.497219	3030.225773	23.288743
106.732298	3036.654106	23.293760
107.073236	3034.159234	23.298778
107.066919	3036.050596	23.303795
106.927587	3029.438498	23.308813
106.643360	3031.042550	23.313831
106.692028	3031.663155	23.318848
107.007359	3029.659271	23.323866
107.074063	3055.623140	23.328883
107.174272	3054.282488	23.333901
107.564702	3063.628150	23.338919
107.105457	3067.696690	23.343936
107.482936	3056.760860	23.348954
107.526665	3076.675478	23.353971
107.921931	3078.693971	23.358989
108.221161	3087.842733	23.364007
107.938116	3076.322013	23.369024
108.205466	3081.262318	23.374042
108.164318	3079.586595	23.379059
108.362220	3076.269772	23.384077
108.579270	3083.364025	23.389095
108.430070	3098.883662	23.394112
108.670106	3092.857994	23.399130
108.528275	3102.159557	23.404147
108.635047	3108.753398	23.409165
108.778449	3109.485307	23.414183
109.205979	3136.522050	23.419200
109.426457	3125.017885	23.424218
109.547883	3134.788120	23.429235
109.289206	3129.756167	23.434253
109.227265	3127.662659	23.439271
109.050414	3140.864313	23.444288
109.528567	3156.640740	23.449306
109.721110	3160.808472	23.454323
110.045678	3172.431389	23.459341
110.465270	3177.662875	23.464359
110.392944	3176.619790	23.469376
110.557464	3181.429889	23.474394
110.980004	3188.741392	23.479411
111.068972	3185.603160	23.484429
111.462870	3178.852301	23.489447
111.172577	3178.783523	23.494464
111.434502	3176.947486	23.499482
111.186328	3177.544712	23.504499
111.341442	3173.623977	23.509517
111.291583	3181.473724	23.514535
111.353321	3170.114051	23.519552
111.497411	3170.445496	23.524570
111.310298	3171.260365	23.529587
111.369942	3186.057461	23.534605
111.812222	3189.797753	23.539623
111.745327	3204.626798	23.544640
111.903709	3202.298271	23.549658
111.770527	3214.293482	23.554675
111.572781	3220.363926	23.559693
112.209664	3223.579009	23.564711
111.980378	3239.608034	23.569728
112.395862	3254.105081	23.574746
112.515557	3258.999179	23.579763
112.751457	3268.186463	23.584781
113.123309	3259.730910	23.589799
112.990295	3268.596709	23.594816
113.569558	3289.530683	23.599834
113.750609	3294.198138	23.604851
113.187912	3309.099760	23.609869
114.056842	3291.137532	23.614887
113.754930	3305.953544	23.619904
113.867352	3291.860264	23.624922
114.074811	3286.363871	23.629939
114.378757	3296.363670	23.634957
114.741913	3293.109447	23.639975
114.415690	3290.808035	23.644992
114.546173	3290.052266	23.650010
114.624548	3291.634024	23.655027
114.436972	3291.549453	23.660045
114.838728	3274.660211	23.665063
114.679613	3287.316985	23.670080
114.963874	3304.958503	23.675098
114.859432	3297.027063	23.680115
115.114943	3315.612824	23.685133
115.291158	3300.794297	23.690151
115.209116	3316.064887	23.695168
115.568197	3335.426595	23.700186
115.713833	3342.200909	23.705203
115.404801	3342.740093	23.710221
116.026196	3336.082076	23.715239
115.784905	3344.915617	23.720256
115.698610	3332.313864	23.725274
115.940240	3328.996454	23.730291
115.798939	3354.404304	23.735309
116.573583	3349.392660	23.740327
116.338031	3363.415745	23.745344
116.564190	3358.320532	23.750362
116.629368	3346.220857	23.755379
116.797103	3382.081473	23.760397
117.109394	3385.351801	23.765415
116.831455	3385.384908	23.770432
117.119453	3390.984442	23.775450
117.213796	3385.612404	23.780467
117.101747	3384.576262	23.785485
117.396708	3407.081453	23.790503
117.381288	3413.348007	23.795520
117.617034	3404.104896	23.800538
118.129859	3402.660407	23.805555
117.823120	3424.140144	23.810573
118.320355	3415.832081	23.815591
118.493321	3427.968193	23.820608
118.698042	3427.426903	23.825626
118.847761	3424.027621	23.830643
118.876824	3425.626792	23.835661
119.059856	3423.789000	23.840679
118.634196	3431.512994	23.845696
118.788928	3440.311859	23.850714
119.040345	3429.992610	23.855731
119.145067	3451.993717	23.860749
119.157111	3462.777229	23.865767
119.571381	3458.230971	23.870784
119.556839	3469.232249	23.875802
119.882151	3463.315762	23.880819
119.689247	3490.608587	23.885837
119.856904	3491.318398	23.890855
120.413041	3490.183453	23.895872
120.234239	3480.625360	23.900890
120.662400	3473.071731	23.905907
120.369469	3487.830926	23.910925
120.733928	3484.057199	23.915943
120.493508	3482.142137	23.920960
120.702897	3500.710154	23.925978
121.136836	3505.474065	23.930995
121.198622	3499.792235	23.936013
121.582317	3503.268489	23.941031
121.722771	3503.056294	23.946048
121.548446	3503.154164	23.951066
121.780266	3506.572449	23.956083
121.726998	3500.430140	23.961101
121.761971	3524.199428	23.966119
122.059909	3526.884212	23.971136
122.000591	3529.748294	23.976154
122.234303	3536.684701	23.981171
122.211905	3531.177387	23.986189
122.419974	3530.198764	23.991207
122.122485	3536.853485	23.996224
122.318750	3554.237803	24.001242
123.173361	3545.590129	24.006259
122.763863	3557.224798	24.011277
123.121914	3555.665331	24.016295
123.051086	3551.226758	24.021312
123.177870	3576.836917	24.026330
123.410019	3587.741616	24.031347
123.509267	3575.101132	24.036365
123.689492	3588.379983	24.041383
123.489367	3569.143008	24.046400
123.551228	3578.990881	24.051418
124.112032	3589.320054	24.056435
124.241693	3599.877944	24.061453
124.254235	3596.819772	24.066471
124.419127	3599.808618	24.071488
124.485315	3605.336622	24.076506
124.920038	3598.711898	24.081523
124.528984	3600.271853	24.086541
124.739498	3596.549912	24.091559
124.861013	3618.174690	24.096576
124.791296	3625.778750	24.101594
125.224109	3632.265205	24.106611
125.225782	3618.059426	24.111629
125.414604	3624.859403	24.116647
125.352327	3639.068460	24.121664
125.258812	3656.710800	24.126682
125.765249	3649.018570	24.131699
125.908691	3651.469080	24.136717
126.066039	3641.627800	24.141735
126.651225	3661.477522	24.146752
126.481133	3685.323065	24.151770
126.450129	3686.948329	24.156787
126.407175	3692.949288	24.161805
126.678391	3690.001889	24.166823
126.928685	3685.872200	24.171840
126.960986	3694.059199	24.176858
127.498064	3697.733563	24.181875
127.346134	3704.754829	24.186893
127.576914	3694.116593	24.191911
128.069328	3700.658776	24.196928
128.164646	3696.052954	24.201946
128.042457	3698.874703	24.206963
127.736930	3717.215486	24.211981
127.747103	3708.329327	24.216999
127.910116	3705.869457	24.222016
128.239394	3735.950453	24.227034
128.124504	3729.789300	24.232051
128.426179	3729.061716	24.237069
128.349828	3725.485564	24.242087
128.585797	3753.599071	24.247104
128.454811	3750.595094	24.252122
128.707690	3760.590249	24.257139
128.536540	3773.105716	24.262157
128.940468	3792.883201	24.267175
129.204915	3792.694410	24.272192
129.156005	3813.466769	24.277210
129.515374	3816.954594	24.282227
129.631824	3814.970680	24.287245
129.910040	3822.975587	24.292263
130.003960	3837.569623	24.297280
130.162419	3837.704626	24.302298
130.428335	3832.420219	24.307315
130.789614	3839.243760	24.312333
130.590321	3827.831859	24.317351
130.843902	3841.716881	24.322368
130.635670	3868.112167	24.327386
131.139380	3864.096259	24.332403
131.075942	3872.080482	24.337421
131.466080	3859.444848	24.342439
131.437831	3863.598273	24.347456
131.796387	3879.019438	24.352474
132.189943	3877.490095	24.357491
131.949790	3898.133547	24.362509
131.987600	3897.496797	24.367527
132.079484	3892.189948	24.372544
132.332996	3893.253682	24.377562
132.493248	3887.801687	24.382579
132.644438	3882.351584	24.387597
132.468903	3893.204578	24.392615
132.777500	3884.555016	24.397632
132.575745	3886.128992	24.402650
133.013069	3899.379014	24.407667
133.365132	3908.042592	24.412685
133.187529	3911.173126	24.417703
133.412614	3903.588872	24.422720
133.132299	3917.237394	24.427738
133.329139	3911.423458	24.432755
133.532528	3934.636049	24.437773
133.693588	3928.121362	24.442791
133.651434	3937.698083	24.447808
133.492249	3966.558140	24.452826
134.129892	3974.811594	24.457843
134.009591	3977.640562	24.462861
134.053613	4002.392505	24.467879
134.513653	4004.855913	24.472896
134.138515	4011.160298	24.477914
134.906236	4027.939134	24.482931
135.038340	4021.558321	24.487949
134.518791	4032.597777	24.492967
135.401263	4021.418780	24.497984
135.929931	4038.994574	24.503002
136.350624	4047.125261	24.508019
136.315962	4046.308756	24.513037
136.369902	4036.078819	24.518055
136.354149	4044.444212	24.523072
136.348957	4049.100547	24.528090
136.614416	4043.405138	24.533107
136.542041	4041.462239	24.538125
136.481107	4052.673557	24.543143
136.710804	4049.121757	24.548160
136.677048	4064.013075	24.553178
136.905062	4071.792558	24.558195
137.010287	4071.657632	24.563213
137.009742	4096.731250	24.568231
137.364936	4084.859050	24.573248
137.371259	4104.952623	24.578266
137.833665	4111.508798	24.583283
137.766573	4112.254673	24.588301
137.979047	4123.148041	24.593319
138.479373	4130.678630	24.598336
138.373929	4147.708562	24.603354
138.402098	4136.779301	24.608371
138.691068	4127.872228	24.613389
138.535087	4133.034587	24.618407
138.878018	4132.404889	24.623424
138.965060	4163.494619	24.628442
139.330503	4155.576431	24.633459
139.455027	4148.235044	24.638477
139.301683	4156.423632	24.643495
139.668832	4153.265617	24.648512
139.014177	4159.704039	24.653530
139.232817	4183.606584	24.658547
139.849780	4181.881249	24.663565
139.558386	4209.906154	24.668583
140.135128	4202.234910	24.673600
140.675553	4219.260560	24.678618
140.534649	4213.069656	24.683635
140.868239	4216.541755	24.688653
141.044966	4236.266014	24.693671
141.213239	4233.678622	24.698688
141.211549	4249.471090	24.703706
141.498541	4234.949105	24.708723
141.882493	4242.257252	24.713741
141.381623	4240.128838	24.718759
141.444972	4236.558421	24.723776
141.652867	4243.063797	24.728794
141.832093	4239.206917	24.733811
142.052916	4265.874889	24.738829
141.869593	4266.801781	24.743847
141.943722	4260.947363	24.748864
141.996158	4272.157035	24.753882
142.025664	4305.975374	24.758899
142.797207	4294.668060	24.763917
142.620348	4299.689046	24.768935
142.761193	4310.246361	24.773952
142.916894	4324.635378	24.778970
143.214190	4330.103604	24.783987
143.527828	4324.063922	24.789005
143.478024	4335.010619	24.794023
143.809913	4356.076681	24.799040
144.287560	4345.152924	24.804058
144.195689	4346.721386	24.809075
144.325129	4350.135912	24.814093
144.269074	4336.229950	24.819111
144.722011	4343.113766	24.824128
144.538720	4363.623246	24.829146
144.877989	4369.837683	24.834163
145.069656	4374.914728	24.839181
144.750265	4378.776247	24.844199
145.252276	4372.768017	24.849216
145.487953	4398.489296	24.854234
145.316376	4398.696555	24.859251
145.637655	4409.980407	24.864269
145.637682	4398.585936	24.869287
146.202169	4397.221210	24.874304
146.404987	4419.729521	24.879322
146.322567	4440.021651	24.884339
146.460668	4428.400018	24.889357
146.466092	4439.959305	24.894375
146.875687	4427.908567	24.899392
146.984755	4442.077844	24.904410
146.827499	4443.093745	24.909427
146.965357	4453.072922	24.914445
147.019837	4458.792729	24.919463
147.112382	4457.605583	24.924480
147.303499	4488.744515	24.929498
147.489037	4484.433784	24.934515
147.784747	4492.158987	24.939533
147.852875	4508.650013	24.944551
148.439418	4508.361540	24.949568
148.202099	4521.325938	24.954586
148.180720	4511.233722	24.959603
148.743579	4517.458125	24.964621
148.758213	4543.160656	24.969639
149.061226	4542.219039	24.974656
149.256123	4536.821328	24.979674
149.348943	4539.689985	24.984691
149.360355	4522.380626	24.989709
149.543015	4547.338088	24.994727
149.835781	4561.125550	24.999744
150.033037	4562.533665	25.004762
149.749743	4569.958518	25.009779
149.958264	4554.296852	25.014797
150.069892	4576.723608	25.019815
150.131710	4586.972519	25.024832
150.579965	4590.435993	25.029850
150.276419	4592.783937	25.034867
150.717256	4609.881592	25.039885
150.915581	4618.291842	25.044903
151.098293	4615.714600	25.049920
151.292526	4622.980655	25.054938
151.620597	4643.787898	25.059955
151.796131	4646.659443	25.064973
151.740145	4656.593221	25.069991
152.119998	4639.814189	25.075008
152.168736	4643.060619	25.080026
152.100649	4645.785017	25.085043
152.261081	4634.180406	25.090061
152.473552	4667.937806	25.095079
152.656888	4667.929732	25.100096
152.636002	4667.147926	25.105114
152.641520	4664.036964	25.110131
152.474375	4678.910361	25.115149
152.757212	4685.718106	25.120167
153.089512	4702.198760	25.125184
153.445353	4724.997976	25.130202
153.705042	4716.910366	25.135219
154.088891	4730.964032	25.140237
153.910478	4734.968879	25.145255
154.202313	4749.700758	25.150272
154.584450	4746.392511	25.155290
154.299900	4765.607047	25.160307
154.573839	4752.374929	25.165325
154.566513	4768.246415	25.170343
154.810058	4771.529581	25.175360
155.125248	4782.329277	25.180378
155.056805	4785.589980	25.185395
155.584866	4771.611524	25.190413
155.224591	4797.153981	25.195431
155.496661	4806.871838	25.200448
155.923496	4808.486924	25.205466
156.153535	4826.010596	25.210483
156.315873	4825.414256	25.215501
156.487701	4833.268761	25.220519
156.360555	4847.882166	25.225536
156.526898	4845.048140	25.230554
156.623536	4866.245893	25.235571
156.975268	4871.336811	25.240589
157.370905	4876.001574	25.245607
157.140032	4876.466669	25.250624
157.445782	4872.996213	25.255642
157.631402	4880.871298	25.260659
157.832118	4878.645766	25.265677
157.981066	4896.104174	25.270695
158.123559	4892.848486	25.275712
158.546551	4908.757676	25.280730
158.338861	4914.965856	25.285747
158.736187	4912.288143	25.290765
158.767636	4925.128939	25.295783
158.400057	4926.285529	25.300800
158.994295	4941.535741	25.305818
158.807837	4945.749061	25.310835
158.927716	4955.524049	25.315853
159.285063	4978.137559	25.320871
159.672161	4969.725612	25.325888
159.904168	4986.030616	25.330906
159.759288	4997.335227	25.335923
160.130984	5003.160304	25.340941
160.217211	4994.473248	25.345959
160.070892	5026.796197	25.350976
160.660715	5019.048772	25.355994
160.722188	5025.676310	25.361011
161.287701	5039.596301	25.366029
161.427256	5049.418885	25.371047
161.403171	5061.144931	25.376064
162.111597	5056.193697	25.381082
161.644953	5064.064443	25.386099
161.663638	5053.456977	25.391117
161.958943	5068.059842	25.396135
161.976381	5085.526807	25.401152
162.519865	5083.338313	25.406170
162.135278	5098.755924	25.411187
162.558526	5089.385949	25.416205
162.541389	5117.408511	25.421223
162.678961	5106.926251	25.426240
162.572760	5115.183539	25.431258
162.660094	5123.820281	25.436275
163.001946	5145.017268	25.441293
163.269868	5161.837403	25.446311
163.828980	5165.831919	25.451328
164.050022	5166.350308	25.456346
163.829976	5183.286527	25.461363
163.814420	5186.560230	25.466381
164.049964	5195.919396	25.471399
164.325032	5203.671988	25.476416
164.420058	5201.932786	25.481434
164.526573	5221.106889	25.486451
164.956043	5233.292785	25.491469
165.013792	5248.917387	25.496487
165.081882	5245.202644	25.501504
165.766667	5255.656160	25.506522
165.853996	5270.371141	25.511539
166.044803	5265.771126	25.516557
166.022370	5271.321651	25.521575
166.083039	5273.741410	25.526592
166.649061	5285.642572	25.531610
166.877512	5285.637282	25.536627
166.881270	5293.815864	25.541645
166.932570	5302.449210	25.546663
167.128359	5293.176541	25.551680
167.029762	5310.503869	25.556698
167.079969	5325.104953	25.561715
167.359033	5317.707952	25.566733
167.614530	5325.903620	25.571751
167.570188	5347.246193	25.576768
168.313449	5334.897885	25.581786
168.179622	5349.402622	25.586803
168.187360	5367.836898	25.591821
168.280074	5364.813755	25.596839
168.395266	5374.675611	25.601856
168.886456	5391.077592	25.606874
169.003424	5393.140021	25.611891
169.436594	5403.250156	25.616909
169.628283	5402.429646	25.621927
169.521740	5421.737235	25.626944
169.772104	5424.141029	25.631962
169.827323	5436.098359	25.636979
170.273234	5446.546983	25.641997
170.409375	5441.275998	25.647015
170.603819	5463.745077	25.652032
170.697222	5464.789708	25.657050
170.808315	5462.343064	25.662067
170.929034	5464.952153	25.667085
171.195794	5477.005276	25.672103
170.930293	5482.646434	25.677120
171.430191	5486.823268	25.682138
172.000911	5485.406243	25.687156
171.913599	5516.129829	25.692173
172.221667	5527.549363	25.697191
172.082381	5518.227195	25.702208
172.312859	5525.061679	25.707226
172.165537	5539.890887	25.712244
172.309709	5555.504273	25.717261
172.604024	5558.384710	25.722279
172.520956	5567.348688	25.727296
173.233371	5589.476446	25.732314
173.165356	5590.161515	25.737332
173.172594	5611.590027	25.742349
173.697191	5603.422754	25.747367
173.513098	5621.751616	25.752384
173.894980	5606.601620	25.757402
174.339157	5641.089425	25.762420
173.875238	5635.837201	25.767437
174.153759	5633.752260	25.772455
174.287459	5653.259824	25.777472
174.828723	5664.234999	25.782490
174.720561	5671.460166	25.787508
175.096123	5691.436902	25.792525
175.397104	5686.779188	25.797543
175.800714	5704.979545	25.802560
176.076251	5705.343665	25.807578
175.990553	5706.793125	25.812596
175.696017	5735.498104	25.817613
176.256578	5732.410583	25.822631
176.050824	5742.038674	25.827648
176.746162	5760.204675	25.832666
176.737204	5761.303643	25.837684
176.841348	5766.198349	25.842701
176.616815	5773.942430	25.847719
177.184865	5790.009671	25.852736
177.467430	5784.199775	25.857754
177.784852	5812.919540	25.862772
177.747958	5817.864339	25.867789
178.095463	5818.409103	25.872807
177.831688	5830.679696	25.877824
178.343466	5833.175017	25.882842
178.483025	5844.610027	25.887860
178.719790	5865.245004	25.892877
179.105589	5875.632979	25.897895
178.854202	5885.737237	25.902912
179.268757	5873.794026	25.907930
179.368064	5902.147996	25.912948
179.641520	5911.901753	25.917965
179.711312	5906.254930	25.922983
179.668065	5917.950531	25.928000
180.208599	5925.906098	25.933018
180.390000	5934.782491	25.938036
180.729170	5958.982050	25.943053
180.871392	5960.157636	25.948071
180.886145	5950.242391	25.953088
181.208337	5959.448319	25.958106
181.460818	5969.052416	25.963124
181.476632	5970.941070	25.968141
181.828525	5994.548377	25.973159
181.993336	5985.292229	25.978176
182.024311	6007.962344	25.983194
182.446584	6014.834652	25.988212
182.553000	6014.695184	25.993229
183.291979	6002.227761	25.998247
183.155857	6012.528034	26.003264
183.315500	6033.140146	26.008282
183.524281	6028.003036	26.013300
183.200627	6034.060332	26.018317
183.666871	6037.867257	26.023335
183.566623	6045.707482	26.028352
183.760470	6056.970278	26.033370
183.898641	6063.330840	26.038388
184.140474	6095.460754	26.043405
184.448345	6088.851614	26.048423
184.331034	6115.838097	26.053440
184.794370	6113.516240	26.058458
185.074643	6125.569602	26.063476
185.118843	6150.078847	26.068493
185.398644	6137.459213	26.073511
185.286872	6157.170579	26.078528
185.858956	6155.834382	26.083546
185.949297	6156.900828	26.088564
185.903267	6175.526060	26.093581
186.234091	6176.140925	26.098599
186.275130	6202.246197	26.103616
186.712455	6193.515032	26.108634
186.747432	6180.262130	26.113652
186.556253	6214.415983	26.118669
187.271768	6213.095064	26.123687
187.204917	6239.474154	26.128704
187.162856	6244.421910	26.133722
187.640540	6250.073238	26.138740
187.719032	6264.942995	26.143757
187.949921	6257.294826	26.148775
188.100000	6277.873798	26.153792
188.444341	6284.841393	26.158810
188.408240	6292.095889	26.163828
188.215895	6302.463915	26.168845
188.709594	6320.103595	26.173863
188.905165	6332.756604	26.178880
189.015291	6352.232319	26.183898
189.638144	6359.743362	26.188916
189.766568	6380.080745	26.193933
189.889338	6378.802626	26.198951
190.027596	6402.763993	26.203968
190.132797	6411.180363	26.208986
190.682288	6421.744435	26.214004
190.394439	6439.321235	26.219021
190.574892	6442.467135	26.224039
190.883053	6461.624014	26.229056
191.125227	6476.646081	26.234074
191.466033	6478.440149	26.239092
191.421859	6506.229485	26.244109
191.924414	6498.170129	26.249127
192.037978	6527.132000	26.254144
192.529299	6537.694344	26.259162
193.358932	6517.126749	26.264180
193.278043	6539.382603	26.269197
193.742899	6499.184852	26.274215
193.584563	6531.632990	26.279232
193.599769	6518.314951	26.284250
193.709795	6530.922800	26.289268
193.789596	6553.074555	26.294285
194.106384	6543.680750	26.299303
194.199254	6553.378123	26.304320
194.284335	6551.721133	26.309338
194.345544	6582.242724	26.314356
194.402494	6580.252938	26.319373
194.862727	6607.107830	26.324391
194.805899	6608.396285	26.329408
194.821366	6627.419816	26.334426
195.174960	6626.458307	26.339444
195.162414	6649.759846	26.344461
195.833639	6683.822630	26.349479
196.200127	6676.262103	26.354496
196.194540	6680.716508	26.359514
196.463318	6697.600766	26.364532
196.600205	6700.012485	26.369549
196.818713	6710.503078	26.374567
197.107129	6732.288687	26.379584
197.103936	6735.989072	26.384602
197.776989	6740.785361	26.389620
197.544956	6740.687633	26.394637
197.682274	6761.131142	26.399655
198.112512	6757.273518	26.404672
197.885745	6761.332544	26.409690
198.352755	6771.547050	26.414708
198.611148	6784.689717	26.419725
198.914903	6790.264062	26.424743
198.689626	6811.865723	26.429760
198.643106	6814.781842	26.434778
199.217724	6814.943800	26.439796
199.547304	6842.235306	26.444813
199.768661	6831.648273	26.449831
199.736479	6856.435846	26.454848
199.928405	6859.139718	26.459866
200.209234	6871.509356	26.464884
200.428353	6868.943845	26.469901
200.769364	6897.923947	26.474919
200.800168	6898.184027	26.479936
200.836415	6898.659773	26.484954
201.304021	6925.071019	26.489972
201.750876	6925.274564	26.494989
201.710344	6933.489278	26.500007
202.234818	6948.319466	26.505024
202.172337	6961.842904	26.510042
202.585721	6962.777674	26.515060
202.369524	6993.930235	26.520077
202.783974	6980.156414	26.525095
203.042915	7006.212847	26.530112
203.058431	7003.924691	26.535130
203.446469	7030.650092	26.540148
203.860420	7023.863562	26.545165
203.679970	7043.332627	26.550183
204.173739	7046.403651	26.555200
204.279400	7060.206524	26.560218
204.654830	7051.102380	26.565236
204.239653	7073.598896	26.570253
204.691112	7079.934885	26.575271
204.658799	7088.630678	26.580288
204.721486	7104.781988	26.585306
205.265680	7119.931571	26.590324
205.297640	7142.714993	26.595341
205.476202	7142.680937	26.600359
205.697628	7167.454662	26.605376
206.023176	7190.494418	26.610394
206.618268	7195.128506	26.615412
206.591161	7203.122605	26.620429
207.001727	7222.557243	26.625447
207.378566	7225.382226	26.630464
207.718250	7227.807772	26.635482
207.961057	7236.639322	26.640500
207.614782	7248.313529	26.645517
208.001070	7253.752338	26.650535
208.264178	7256.099974	26.655552
208.321206	7276.836601	26.660570
208.624035	7285.917358	26.665588
208.441519	7311.703875	26.670605
208.971799	7309.784635	26.675623
209.356460	7338.134615	26.680640
209.284958	7343.760922	26.685658
209.368955	7355.098718	26.690676
209.564687	7361.316418	26.695693
209.964788	7373.460412	26.700711
210.403198	7401.347218	26.705728
210.459873	7390.679521	26.710746
210.806453	7410.615600	26.715764
210.383210	7428.541520	26.720781
210.580434	7444.797744	26.725799
211.281327	7452.850458	26.730816
211.223421	7463.111588	26.735834
211.765993	7460.787867	26.740852
212.267088	7479.627452	26.745869
212.204856	7484.622245	26.750887
212.664290	7481.461715	26.755904
212.788942	7506.426011	26.760922
212.834689	7500.656975	26.765940
213.154233	7514.769065	26.770957
213.241771	7510.203573	26.775975
213.510725	7528.940602	26.780992
213.127884	7531.957311	26.786010
213.643604	7538.226955	26.791028
214.439125	7566.785105	26.796045
214.427233	7570.569816	26.801063
214.405599	7569.950615	26.806080
214.607979	7594.373766	26.811098
214.907083	7589.151922	26.816116
215.105375	7606.353980	26.821133
215.511366	7616.941787	26.826151
215.609938	7616.900471	26.831168
215.484672	7637.385750	26.836186
215.889577	7642.912187	26.841204
216.117037	7661.121484	26.846221
216.088265	7669.718569	26.851239
216.588240	7687.559977	26.856256
216.679308	7690.425961	26.861274
216.836425	7693.833893	26.866292
217.059671	7721.943469	26.871309
217.268084	7714.231366	26.876327
217.721028	7741.048455	26.881344
217.844455	7748.070533	26.886362
217.969451	7762.296895	26.891380
218.228747	7774.757435	26.896397
218.319897	7784.527127	26.901415
219.265696	7800.400934	26.906432
219.175194	7820.913784	26.911450
219.239178	7806.202858	26.916468
219.469834	7827.561257	26.921485
219.336312	7834.358057	26.926503
220.014109	7851.586691	26.931520
219.894085	7862.208019	26.936538
220.060271	7878.075254	26.941556
220.566037	7902.173111	26.946573
220.833415	7911.657808	26.951591
221.119195	7922.008938	26.956608
221.223744	7935.278009	26.961626
221.331663	7951.744042	26.966644
222.125743	7956.988923	26.971661
221.576632	7971.846643	26.976679
221.909087	7976.964610	26.981696
222.156261	8000.452452	26.986714
222.126892	8007.399082	26.991732
222.338092	8019.431451	26.996749
222.611500	8036.713714	27.001767
223.196087	8058.791279	27.006784
223.255689	8070.686495	27.011802
223.857063	8076.435798	27.016820
223.932296	8097.550106	27.021837
223.978644	8108.443389	27.026855
224.722915	8136.626710	27.031872
224.876240	8133.333912	27.036890
225.101714	8136.682605	27.041908
225.382703	8162.449849	27.046925
225.112494	8162.796306	27.051943
225.778899	8166.655747	27.056960
225.648845	8179.211652	27.061978
225.956636	8195.837085	27.066996
226.034311	8205.106003	27.072013
226.155195	8221.261446	27.077031
226.634902	8227.692471	27.082048
226.900584	8260.364732	27.087066
226.977974	8253.774262	27.092084
227.247282	8271.531582	27.097101
227.276253	8296.456233	27.102119
227.554088	8297.940770	27.107136
227.490556	8320.229746	27.112154
228.092737	8327.176920	27.117172
228.389678	8336.928705	27.122189
227.980399	8359.028346	27.127207
228.392777	8364.938934	27.132224
228.516561	8380.056811	27.137242
228.823635	8395.540576	27.142260
229.407483	8413.180718	27.147277
229.525980	8428.004958	27.152295
229.834179	8446.579079	27.157312
230.275881	8453.747359	27.162330
230.331224	8480.564456	27.167348
230.917165	8478.590993	27.172365
230.547733	8495.411329	27.177383
230.947652	8503.437920	27.182400
231.322514	8533.297548	27.187418
231.493932	8545.088801	27.192436
231.565813	8557.550997	27.197453
232.052556	8576.185558	27.202471
232.379690	8584.925175	27.207488
232.157833	8608.468575	27.212506
232.347006	8632.810458	27.217524
232.693830	8635.357124	27.222541
232.462017	8666.318274	27.227559
233.371332	8677.856182	27.232576
233.571130	8706.388027	27.237594
233.731573	8714.045527	27.242612
234.628025	8704.831513	27.247629
234.604595	8719.867713	27.252647
234.941680	8736.698379	27.257664
235.143321	8725.862485	27.262682
235.025538	8745.052358	27.267700
235.597921	8751.346998	27.272717
235.424503	8772.411928	27.277735
235.956210	8779.960076	27.282752
236.300776	8795.842081	27.287770
236.077977	8821.284870	27.292788
236.365405	8833.332833	27.297805
236.467011	8858.264484	27.302823
236.942412	8861.041980	27.307840
237.207206	8878.634545	27.312858
237.348499	8891.193439	27.317876
237.919642	8900.976669	27.322893
237.843824	8908.971803	27.327911
238.632813	8915.500084	27.332928
238.713695	8936.212898	27.337946
238.731970	8952.430148	27.342964
239.171816	8950.787149	27.347981
239.438744	8979.207581	27.352999
239.787105	8981.525644	27.358016
239.875056	8978.909006	27.363034
240.132787	9011.043830	27.368052
240.500992	9008.535258	27.373069
240.558241	9020.970308	27.378087
240.748096	9037.266413	27.383104
240.899776	9040.641669	27.388122
240.982112	9058.513467	27.393140
241.477881	9066.390615	27.398157
241.464948	9091.717252	27.403175
241.845681	9094.190657	27.408192
242.292331	9118.191452	27.413210
242.304616	9124.637065	27.418228
242.763476	9140.999886	27.423245
242.517909	9144.860600	27.428263
243.216044	9167.679443	27.433280
243.208021	9183.329459	27.438298
243.100560	9186.074930	27.443316
243.958946	9203.143679	27.448333
243.842224	9232.537660	27.453351
244.207673	9230.541467	27.458368
244.475698	9228.082492	27.463386
244.592377	9263.089980	27.468404
244.878325	9283.952886	27.473421
244.927028	9286.815921	27.478439
245.137066	9301.132800	27.483456
245.589421	9327.843995	27.488474
245.658652	9325.321759	27.493492
245.883350	9343.785499	27.498509
246.095426	9352.620953	27.503527
246.628312	9387.507967	27.508544
246.895109	9389.630843	27.513562
246.794063	9396.549755	27.518580
247.214087	9415.546042	27.523597
247.454017	9439.687022	27.528615
247.767876	9456.606570	27.533632
247.872338	9470.192789	27.538650
247.700795	9474.182339	27.543668
248.725858	9505.355706	27.548685
248.654916	9524.008700	27.553703
249.524640	9542.632325	27.558720
249.498494	9550.918880	27.563738
249.367039	9571.001260	27.568756
249.884303	9587.402154	27.573773
250.252324	9589.198001	27.578791
250.431069	9618.830584	27.583808
250.729718	9626.695686	27.588826
250.940294	9650.433048	27.593844
251.187267	9657.042528	27.598861
251.054414	9677.645121	27.603879
251.517538	9694.933301	27.608896
251.995233	9716.186490	27.613914
251.917028	9729.546335	27.618932
252.319197	9732.963847	27.623949
252.827109	9751.248944	27.628967
253.015054	9751.611891	27.633984
253.166287	9783.316915	27.639002
253.075553	9797.289320	27.644020
253.580551	9810.567058	27.649037
253.976087	9830.112158	27.654055
253.994441	9843.817681	27.659072
254.361788	9868.373050	27.664090
254.383598	9890.421712	27.669108
254.994868	9896.365394	27.674125
255.049729	9925.047044	27.679143
255.386137	9937.216934	27.684160
255.605443	9959.239363	27.689178
255.733337	9970.238604	27.694196
256.574876	9980.184989	27.699213
256.658964	9999.728981	27.704231
256.940183	10009.898712	27.709248
257.204417	10027.910898	27.714266
257.104962	10041.993656	27.719284
257.571821	10061.956538	27.724301
257.783726	10072.352793	27.729319
258.051805	10080.865910	27.734336
258.610913	10104.040685	27.739354
258.720221	10100.550747	27.744372
259.375039	10130.158404	27.749389
259.453381	10129.814811	27.754407
259.770261	10142.511099	27.759424
260.168133	10152.308771	27.764442
259.984139	10164.760157	27.769460
260.484326	10164.591834	27.774477
260.875115	10185.921451	27.779495
260.948024	10190.457610	27.784512
261.387249	10204.858742	27.789530
261.480890	10222.394434	27.794548
261.776916	10228.672314	27.799565
261.847546	10231.229430	27.804583
262.113210	10243.572718	27.809600
262.213858	10254.805083	27.814618
262.212546	10274.666779	27.819636
262.416429	10277.096338	27.824653
262.912685	10311.651162	27.829671
262.645503	10311.152764	27.834688
263.248405	10331.897732	27.839706
263.215953	10356.605766	27.844724
263.764691	10372.513912	27.849741
263.646193	10401.066737	27.854759
264.105035	10424.578346	27.859776
264.458709	10437.774486	27.864794
264.634033	10465.107592	27.869812
265.057168	10496.394176	27.874829
265.280213	10517.084778	27.879847
265.272440	10543.061144	27.884864
265.822558	10556.569149	27.889882
266.020693	10573.466474	27.894900
266.532482	10598.083391	27.899917
266.698175	10619.403517	27.904935
266.921613	10640.620395	27.909952
267.413181	10655.140108	27.914970
267.441239	10667.567092	27.919988
267.706029	10686.360542	27.925005
268.328860	10702.659292	27.930023
268.415655	10728.657359	27.935040
268.983382	10744.576920	27.940058
269.391216	10773.183664	27.945076
269.811748	10768.814287	27.950093
269.944794	10776.018868	27.955111
270.344700	10787.564512	27.960128
270.796086	10775.111345	27.965146
270.919688	10812.923750	27.970164
270.947439	10815.111522	27.975181
271.465226	10829.065429	27.980199
271.295205	10848.925780	27.985216
271.772644	10853.719042	27.990234
271.692448	10884.781554	27.995252
272.289387	10889.369185	28.000269
272.449732	10910.014729	28.005287
272.726308	10929.975481	28.010304
273.041049	10945.792890	28.015322
273.033016	10957.465132	28.020340
273.091600	10967.737640	28.025357
273.251287	11011.268864	28.030375
273.884058	11006.149114	28.035392
274.250649	11049.334324	28.040410
274.528003	11064.765745	28.045428
274.661539	11087.690877	28.050445
274.990768	11111.917321	28.055463
275.291257	11115.305460	28.060480
275.631616	11138.647071	28.065498
275.815421	11176.795414	28.070516
276.125017	11185.398367	28.075533
276.424982	11203.163363	28.080551
276.855161	11226.860495	28.085568
277.354725	11242.571254	28.090586
277.139117	11261.833887	28.095604
277.485505	11277.006762	28.100621
278.259932	11297.735682	28.105639
278.667305	11304.228762	28.110656
279.020585	11303.530931	28.115674
279.257073	11314.748692	28.120692
279.624695	11329.068935	28.125709
279.815265	11346.270818	28.130727
279.991816	11352.919424	28.135744
280.413576	11351.360316	28.140762
280.362116	11367.639600	28.145780
280.729447	11383.363680	28.150797
280.947559	11377.690010	28.155815
281.132992	11399.960288	28.160832
281.404577	11402.582072	28.165850
281.297741	11439.971633	28.170868
281.619998	11438.673941	28.175885
281.868737	11457.218089	28.180903
281.970393	11479.723673	28.185920
282.131207	11508.143316	28.190938
282.073355	11533.785325	28.195956
282.182691	11555.840735	28.200973
282.843182	11597.926450	28.205991
282.693352	11628.877447	28.211008
282.959425	11649.760922	28.216026
283.230457	11695.564806	28.221044
283.768630	11715.119382	28.226061
284.306118	11752.649788	28.231079
284.483347	11778.091073	28.236096
284.906868	11800.086247	28.241114
285.317797	11838.126171	28.246132
285.769040	11843.525121	28.251149
286.262556	11866.684155	28.256167
286.540013	11885.985029	28.261184
286.805093	11894.960453	28.266202
287.253439	11912.744263	28.271220
287.381504	11932.312504	28.276237
287.963311	11941.219872	28.281255
288.239445	11960.292604	28.286272
288.578277	11966.017395	28.291290
288.665018	11994.193327	28.296308
289.096059	12021.267851	28.301325
289.779263	12026.267746	28.306343
289.751528	12061.241428	28.311360
289.809223	12062.323125	28.316378
289.911990	12087.149353	28.321396
290.250013	12097.780545	28.326413
290.931986	12110.884447	28.331431
291.263908	12127.885782	28.336448
291.640671	12151.727821	28.341466
291.862976	12160.333119	28.346484
291.945763	12181.720232	28.351501
292.402356	12196.618173	28.356519
292.941370	12213.985575	28.361536
293.122879	12230.719605	28.366554
293.332539	12240.272365	28.371572
293.592694	12251.773624	28.376589
293.597388	12274.201810	28.381607
293.583930	12302.881685	28.386624
293.870103	12329.609621	28.391642
294.211385	12354.648159	28.396660
294.448438	12384.537002	28.401677
294.704799	12398.114012	28.406695
294.677089	12420.265729	28.411712
295.046023	12455.182614	28.416730
295.804405	12469.989199	28.421748
296.322055	12505.202253	28.426765
296.483241	12518.379924	28.431783
296.667451	12547.645206	28.436800
297.383185	12556.134535	28.441818
297.797297	12575.019768	28.446836
297.943109	12595.355559	28.451853
298.313671	12601.451902	28.456871
298.474997	12624.487298	28.461888
298.564152	12641.503288	28.466906
299.261235	12659.249987	28.471924
299.134679	12687.196099	28.476941
299.845153	12698.876954	28.481959
300.155512	12703.198132	28.486976
300.334669	12722.389419	28.491994
300.260564	12730.625671	28.497012
300.489238	12750.533587	28.502029
300.947919	12769.973388	28.507047
301.076053	12788.494098	28.512064
301.144467	12799.228596	28.517082
301.615197	12842.440829	28.522100
301.814357	12858.652647	28.527117
302.032973	12879.421880	28.532135
302.585682	12902.452888	28.537152
302.857670	12943.027556	28.542170
302.938184	12950.610492	28.547188
303.208850	12984.559212	28.552205
303.881231	12994.221112	28.557223
303.986791	13028.892841	28.562240
304.241711	13045.475362	28.567258
304.664388	13065.312225	28.572276
304.924014	13099.054240	28.577293
305.178623	13122.501935	28.582311
305.527043	13150.186030	28.587328
306.113930	13177.220216	28.592346
306.621585	13203.179553	28.597364
306.205047	13211.866535	28.602381
307.031650	13251.383695	28.607399
307.035246	13267.009790	28.612416
307.367225	13300.754455	28.617434
307.741745	13318.143141	28.622452
307.800703	13353.437773	28.627469
308.645699	13374.367297	28.632487
308.718066	13411.397796	28.637504
309.187920	13424.330622	28.642522
309.223374	13448.096254	28.647540
309.281157	13493.960192	28.652557
310.035075	13508.599094	28.657575
310.523239	13528.313837	28.662592
310.584971	13555.730857	28.667610
310.902609	13576.218340	28.672628
311.040869	13609.133756	28.677645
311.749187	13624.800554	28.682663
311.978635	13651.869377	28.687680
312.095805	13676.631074	28.692698
312.468670	13705.493067	28.697716
312.677776	13722.636923	28.702733
313.432487	13749.040852	28.707751
314.038138	13771.820127	28.712768
314.087749	13785.164598	28.717786
314.292372	13813.257273	28.722804
314.510350	13835.657911	28.727821
315.165920	13849.606668	28.732839
315.141715	13864.049062	28.737856
315.362743	13881.191116	28.742874
316.080827	13919.003228	28.747892
316.264766	13937.049627	28.752909
316.832521	13965.005365	28.757927
317.335833	13992.322600	28.762944
317.333543	13996.253002	28.767962
317.737398	14023.244788	28.772980
317.933216	14034.802074	28.777997
318.577087	14057.069631	28.783015
318.875451	14052.610048	28.788032
318.991329	14088.604385	28.793050
319.293303	14076.758746	28.798068
319.585183	14107.535169	28.803085
319.867776	14126.014565	28.808103
320.053478	14152.264194	28.813120
320.339240	14168.979866	28.818138
320.969901	14190.020712	28.823156
320.825917	14204.078232	28.828173
320.815143	14229.492210	28.833191
321.422078	14241.577358	28.838208
321.425165	14268.683036	28.843226
322.156049	14285.544321	28.848244
322.179849	14310.352353	28.853261
322.837380	14326.489923	28.858279
323.251540	14353.553044	28.863296
323.652790	14378.601370	28.868314
324.052166	14377.246592	28.873332
324.121880	14417.669294	28.878349
324.304800	14434.717383	28.883367
324.438460	14454.485524	28.888384
324.691214	14484.786944	28.893402
325.178220	14499.131268	28.898420
325.299253	14536.912675	28.903437
325.702631	14573.609087	28.908455
326.074014	14590.860997	28.913472
326.240546	14618.359415	28.918490
326.707079	14637.839572	28.923508
326.956138	14677.741649	28.928525
327.457612	14699.420636	28.933543
328.250164	14723.572834	28.938560
328.256484	14741.466683	28.943578
329.026142	14765.310718	28.948596
329.198504	14794.529244	28.953613
329.900662	14795.674057	28.958631
330.039932	14830.443357	28.963648
330.582052	14851.603698	28.968666
330.754575	14862.840809	28.973684
330.506253	14882.664697	28.978701
330.937263	14898.451038	28.983719
331.314363	14916.808570	28.988736
331.647358	14953.727054	28.993754
332.048043	14972.793023	28.998772
332.425122	15003.172574	29.003789
332.621398	15029.885170	29.008807
333.066386	15056.626058	29.013824
333.060906	15078.973936	29.018842
333.686944	15113.965986	29.023860
333.939864	15130.933908	29.028877
334.219006	15155.480433	29.033895
334.551104	15167.395791	29.038912
334.622539	15201.705917	29.043930
335.169731	15220.160185	29.048948
335.440252	15260.008146	29.053965
335.879307	15269.058357	29.058983
336.237271	15306.999396	29.064000
336.586080	15341.229325	29.069018
337.069546	15360.832047	29.074036
337.474496	15395.990451	29.079053
337.700272	15426.444642	29.084071
338.031318	15446.677779	29.089088
338.424953	15476.289612	29.094106
338.790223	15498.214368	29.099124
338.940185	15531.019868	29.104141
339.258821	15562.229574	29.109159
340.095791	15571.592428	29.114176
340.136222	15607.011644	29.119194
340.170661	15638.722300	29.124212
340.510501	15657.466614	29.129229
341.340319	15694.777472	29.134247
341.721459	15711.207927	29.139264
341.719667	15741.233838	29.144282
342.338514	15752.809140	29.149300
342.519104	15777.256269	29.154317
342.931113	15813.088892	29.159335
343.023031	15818.608438	29.164352
343.458355	15866.267608	29.169370
343.466483	15871.355033	29.174388
343.824593	15893.116035	29.179405
344.157078	15936.283731	29.184423
344.789363	15956.601690	29.189440
344.771976	16001.786219	29.194458
345.264495	16003.712745	29.199476
345.729841	16035.464876	29.204493
345.775314	16068.202044	29.209511
346.016571	16091.041636	29.214528
346.341109	16127.875931	29.219546
346.986811	16159.366848	29.224564
347.148791	16203.387631	29.229581
347.378580	16220.109937	29.234599
347.799541	16266.374793	29.239616
348.044495	16284.257705	29.244634
348.664904	16324.832138	29.249652
349.100749	16353.185714	29.254669
349.438795	16373.398361	29.259687
350.137401	16409.946136	29.264704
350.041820	16438.542096	29.269722
350.613632	16465.007469	29.274740
351.287307	16479.875874	29.279757
351.510640	16503.672463	29.284775
351.870752	16533.616405	29.289792
351.937958	16574.828135	29.294810
352.580759	16582.456991	29.299828
352.875671	16610.011638	29.304845
353.185784	16641.710220	29.309863
353.560291	16657.203443	29.314880
354.070350	16699.248516	29.319898
354.287356	16720.490219	29.324916
354.676487	16752.030971	29.329933
354.742234	16780.909771	29.334951
355.042538	16801.261567	29.339968
355.297252	16845.133223	29.344986
355.933514	16871.000761	29.350004
356.392757	16903.575112	29.355021
356.418009	16940.102928	29.360039
356.938583	16972.624732	29.365056
357.351362	17006.549725	29.370074
357.455567	17037.261833	29.375092
358.436783	17064.147535	29.380109
358.172465	17105.271949	29.385127
358.906146	17132.052085	29.390144
359.179011	17159.461578	29.395162
359.222016	17206.336838	29.400180
359.633320	17225.561298	29.405197
360.038249	17276.027066	29.410215
360.491024	17294.601731	29.415232
360.938092	17340.208104	29.420250
361.279733	17372.276416	29.425268
361.867337	17394.857304	29.430285
361.990163	17418.941332	29.435303
362.564879	17460.733393	29.440320
362.816526	17492.487411	29.445338
363.122015	17515.236426	29.450356
363.798772	17544.217370	29.455373
363.541668	17585.907602	29.460391
364.323399	17597.309164	29.465408
364.785334	17639.110854	29.470426
365.333069	17674.480686	29.475444
365.603933	17699.664414	29.480461
365.586734	17729.220541	29.485479
366.174114	17739.855234	29.490496
366.445209	17786.751211	29.495514
366.659494	17820.294592	29.500532
367.345397	17833.360742	29.505549
367.740669	17870.994237	29.510567
368.384037	17891.765121	29.515584
368.442230	17905.083178	29.520602
368.729767	17945.297380	29.525620
368.849148	17961.182304	29.530637
369.169731	17991.293054	29.535655
369.397796	18028.900945	29.540672
369.899895	18050.154015	29.545690
370.049705	18087.076748	29.550708
370.825544	18110.169712	29.555725
370.842533	18156.186690	29.560743
371.476448	18169.717198	29.565760
371.966340	18215.391431	29.570778
372.262354	18225.827123	29.575796
372.836495	18265.988458	29.580813
372.806084	18299.735582	29.585831
373.440349	18339.605037	29.590848
373.377879	18367.574733	29.595866
374.136604	18407.031330	29.600884
374.842311	18441.615439	29.605901
375.619326	18454.168972	29.610919
375.893663	18487.706946	29.615936
376.003351	18504.858075	29.620954
376.024225	18535.556801	29.625972
376.648772	18571.147572	29.630989
376.631499	18602.573032	29.636007
377.143396	18620.526305	29.641024
377.534939	18657.771327	29.646042
377.911174	18681.282595	29.651060
378.440597	18724.165034	29.656077
378.396000	18764.536979	29.661095
379.329502	18787.972104	29.666112
379.619722	18832.944957	29.671130
379.937810	18856.957853	29.676148
380.250857	18887.170787	29.681165
380.540899	18919.466580	29.686183
381.341543	18958.769415	29.691200
381.336881	18993.629654	29.696218
381.775951	19015.794399	29.701236
382.570127	19054.994502	29.706253
382.524474	19078.582336	29.711271
383.307379	19109.605467	29.716288
383.476074	19138.879641	29.721306
383.734625	19165.182032	29.726324
384.287079	19196.698924	29.731341
384.551832	19229.432964	29.736359
385.330110	19251.653903	29.741376
385.810724	19288.110129	29.746394
385.963711	19325.519013	29.751412
386.270752	19347.423868	29.756429
386.389781	19379.690492	29.761447
386.787886	19414.543404	29.766464
387.115946	19456.721752	29.771482
387.338410	19484.632082	29.776500
387.577480	19526.391839	29.781517
388.266333	19556.545493	29.786535
388.663408	19592.645771	29.791552
389.213797	19619.963077	29.796570
389.531173	19668.265939	29.801588
390.097026	19683.030550	29.806605
390.493415	19731.208628	29.811623
390.980124	19758.133156	29.816640
391.103494	19791.022493	29.821658
391.552556	19823.030544	29.826676
392.136380	19850.546049	29.831693
392.251190	19890.011686	29.836711
392.553609	19925.173095	29.841728
392.873650	19953.301387	29.846746
393.430631	19989.038787	29.851764
393.908538	20029.474098	29.856781
394.077564	20056.505185	29.861799
394.134242	20091.959750	29.866816
394.698861	20127.642593	29.871834
395.025146	20157.029673	29.876852
395.501982	20189.661219	29.881869
395.833893	20228.912098	29.886887
396.155779	20269.124708	29.891904
396.728229	20294.552622	29.896922
396.867226	20350.618829	29.901940
397.392624	20374.913374	29.906957
397.799279	20412.522410	29.911975
398.280787	20448.161347	29.916992
399.054418	20483.759987	29.922010
399.231865	20525.701109	29.927028
399.719186	20556.536182	29.932045
399.816991	20589.639402	29.937063
400.579588	20623.419474	29.942080
401.313617	20668.672373	29.947098
401.147957	20699.003949	29.952116
401.708645	20735.245206	29.957133
401.901724	20772.534078	29.962151
402.786073	20796.618614	29.967168
403.145186	20842.006432	29.972186
403.269578	20866.807750	29.977204
404.037118	20909.911892	29.982221
404.402593	20945.504857	29.987239
404.893565	20977.547623	29.992256
405.451015	21008.001497	29.997274
405.384699	21024.515917	30.002292
405.739343	21067.729661	30.007309
406.013243	21109.047829	30.012327
406.244397	21141.100725	30.017344
406.767136	21189.777648	30.022362
406.898208	21241.397951	30.027380
407.596074	21287.123551	30.032397
407.995387	21336.218549	30.037415
408.183856	21368.512245	30.042432
408.529444	21426.097575	30.047450
408.821856	21446.888351	30.052468
409.635265	21502.243251	30.057485
409.728951	21563.504367	30.062503
410.660281	21596.899115	30.067520
411.186228	21625.868001	30.072538
411.749669	21682.136570	30.077556
412.360228	21690.523542	30.082573
412.670876	21734.863993	30.087591
413.244076	21776.355076	30.092608
413.808668	21795.072410	30.097626
413.414833	21832.596181	30.102644
414.271973	21867.460389	30.107661
414.601195	21909.247495	30.112679
414.919730	21941.965381	30.117696
415.655748	21978.068450	30.122714
415.751110	22030.081752	30.127732
416.063194	22046.671828	30.132749
416.456867	22103.545281	30.137767
416.790447	22141.455636	30.142784
417.339745	22180.968434	30.147802
417.679655	22220.804414	30.152820
417.905249	22256.670794	30.157837
418.713116	22289.472486	30.162855
418.900003	22342.732852	30.167872
419.292437	22368.713927	30.172890
419.571717	22415.829739	30.177908
420.545846	22465.377003	30.182925
420.797089	22495.490044	30.187943
421.096211	22513.824797	30.192960
421.386959	22550.606471	30.197978
421.597369	22593.816457	30.202996
422.251057	22623.423392	30.208013
422.623492	22669.165544	30.213031
422.687699	22713.861454	30.218048
423.288390	22735.982396	30.223066
423.365868	22789.035227	30.228084
424.117024	22826.249105	30.233101
424.193554	22879.141568	30.238119
425.051045	22925.554742	30.243136
425.362859	22962.411091	30.248154
425.613716	23023.184911	30.253172
426.276508	23050.057298	30.258189
426.409787	23103.160236	30.263207
427.216573	23152.377713	30.268224
427.501931	23190.306289	30.273242
427.627045	23244.109455	30.278260
428.411627	23272.447243	30.283277
428.730839	23341.921688	30.288295
429.075565	23376.578860	30.293312
429.510872	23426.552216	30.298330
430.013909	23482.972400	30.303348
430.705655	23513.337708	30.308365
431.172247	23557.337160	30.313383
431.416692	23609.450548	30.318400
431.986694	23630.623874	30.323418
432.380808	23687.852635	30.328436
432.831737	23726.965936	30.333453
433.513162	23771.230023	30.338471
433.676089	23814.925562	30.343488
434.339781	23870.871160	30.348506
434.974722	23900.655303	30.353524
435.382905	23944.895610	30.358541
435.628413	23985.014671	30.363559
436.000223	24031.112229	30.368576
436.695460	24069.662511	30.373594
437.091917	24103.849090	30.378612
437.309664	24154.529058	30.383629
437.739222	24188.461224	30.388647
438.427672	24236.665533	30.393664
439.335125	24264.270454	30.398682
439.171342	24322.411832	30.403700
439.591440	24356.292290	30.408717
440.489568	24387.799736	30.413735
440.683734	24451.506564	30.418752
441.125530	24473.786912	30.423770
441.533658	24525.171295	30.428788
442.282677	24561.276200	30.433805
442.732732	24600.156737	30.438823
442.765156	24648.565192	30.443840
443.237432	24685.447682	30.448858
443.282639	24720.726297	30.453876
443.827870	24767.979776	30.458893
444.820010	24808.217125	30.463911
444.775335	24862.770916	30.468928
445.226602	24895.188806	30.473946
445.498919	24948.928937	30.478964
446.153249	24993.066681	30.483981
446.943749	25025.528121	30.488999
447.073524	25082.694896	30.494016
448.063120	25111.303082	30.499034
448.851197	25163.284158	30.504052
449.409024	25188.603669	30.509069
449.977315	25213.905721	30.514087
450.284084	25249.845479	30.519104
450.826110	25281.840728	30.524122
451.030270	25296.520264	30.529140
451.305802	25326.374177	30.534157
451.623624	25353.568976	30.539175
451.858869	25393.604771	30.544192
452.312103	25434.747840	30.549210
452.983660	25461.141702	30.554228
453.113899	25512.016790	30.559245
453.486260	25533.672971	30.564263
453.739141	25587.136083	30.569280
453.899664	25629.233072	30.574298
453.976886	25668.152417	30.579316
454.388140	25731.326760	30.584333
455.306742	25765.365796	30.589351
455.090840	25840.719591	30.594368
455.818004	25893.559734	30.599386
456.211017	25940.554638	30.604404
456.307880	26006.497282	30.609421
457.009495	26051.513013	30.614439
457.467232	26135.118964	30.619456
457.944127	26163.950809	30.624474
457.932146	26233.904966	30.629492
458.690724	26294.188788	30.634509
459.400897	26347.367448	30.639527
459.879656	26414.010225	30.644544
460.326526	26482.106131	30.649562
460.590962	26518.880284	30.654580
461.401810	26587.640290	30.659597
462.229276	26645.781986	30.664615
462.336658	26699.152775	30.669632
463.064411	26759.788683	30.674650
463.612061	26817.879417	30.679668
464.134582	26853.905193	30.684685
464.819132	26920.831344	30.689703
464.874412	26957.016519	30.694720
465.939806	27016.342314	30.699738
466.408364	27058.644261	30.704756
466.861153	27111.883588	30.709773
467.507310	27152.383923	30.714791
467.968558	27201.928874	30.719808
468.396805	27242.774504	30.724826
468.923036	27287.918666	30.729844
469.263507	27328.838926	30.734861
469.856218	27371.474384	30.739879
470.089388	27435.812000	30.744896
470.156441	27477.197258	30.749914
471.099208	27530.426341	30.754932
471.341780	27593.318459	30.759949
472.132246	27631.619819	30.764967
472.422454	27687.442553	30.769984
472.918628	27731.760185	30.775002
473.419235	27784.880161	30.780020
473.602535	27837.768849	30.785037
474.690125	27863.074223	30.790055
475.153836	27923.158598	30.795072
475.356303	27967.004929	30.800090
476.209818	28009.144707	30.805108
476.455662	28060.055593	30.810125
477.089907	28113.864187	30.815143
477.276566	28162.151467	30.820160
477.716921	28209.324572	30.825178
478.179157	28244.142584	30.830196
478.549440	28303.590814	30.835213
479.165258	28365.017355	30.840231
479.243655	28413.376843	30.845248
480.037348	28463.485588	30.850266
480.571803	28506.947270	30.855284
480.963200	28541.291841	30.860301
481.098737	28609.135359	30.865319
481.315608	28649.407337	30.870336
482.094995	28703.931889	30.875354
482.448551	28767.462894	30.880372
482.971225	28796.313695	30.885389
483.935930	28837.535028	30.890407
484.230540	28904.000259	30.895424
484.842258	28932.641017	30.900442
485.503126	28973.518580	30.905460
485.893843	29043.627430	30.910477
486.449594	29092.285333	30.915495
486.734875	29119.463107	30.920512
487.525944	29163.205798	30.925530
488.286104	29197.796734	30.930548
488.318756	29243.327224	30.935565
488.908598	29291.377583	30.940583
489.222007	29351.772505	30.945600
489.474879	29407.424031	30.950618
489.973203	29449.367353	30.955636
490.246819	29498.388439	30.960653
490.971356	29547.297330	30.965671
491.375400	29612.113244	30.970688
491.716602	29672.479459	30.975706
492.322680	29721.865799	30.980724
492.578527	29774.779989	30.985741
493.589746	29833.282238	30.990759
493.827505	29891.048127	30.995776
494.087173	29956.573691	31.000794
494.724336	29993.911985	31.005812
495.178053	30071.310856	31.010829
495.734696	30126.028108	31.015847
495.965024	30180.660635	31.020864
496.759971	30245.635165	31.025882
497.302453	30310.298334	31.030900
497.257125	30379.115558	31.035917
498.086963	30431.712971	31.040935
498.602893	30499.977405	31.045952
499.289248	30561.841744	31.050970
499.811267	30615.127779	31.055988
500.309434	30676.077238	31.061005
501.129552	30745.825520	31.066023
501.326252	30790.465460	31.071040
501.909366	30860.625593	31.076058
502.580512	30907.638602	31.081076
502.662761	30974.184706	31.086093
503.308777	31024.880488	31.091111
504.198187	31085.659502	31.096128
504.432496	31145.799278	31.101146
505.094895	31202.562451	31.106164
505.913881	31252.145117	31.111181
506.646954	31299.912392	31.116199
507.305535	31352.714391	31.121216
507.749402	31401.097560	31.126234
508.106158	31442.434988	31.131252
508.219202	31490.327283	31.136269
508.914574	31560.673597	31.141287
509.474853	31592.677590	31.146304
509.650544	31672.527115	31.151322
510.212125	31707.682711	31.156340
510.835061	31781.076765	31.161357
511.406552	31824.423928	31.166375
511.540332	31886.980503	31.171392
511.494467	31959.170221	31.176410
512.773759	31994.564342	31.181428
512.727196	32085.093670	31.186445
513.375790	32138.186785	31.191463
514.094808	32205.222357	31.196480
514.389925	32265.094090	31.201498
514.963348	32328.093867	31.206516
515.412680	32385.990825	31.211533
515.743741	32436.206400	31.216551
516.317377	32510.252101	31.221568
516.824310	32562.802019	31.226586
517.495446	32628.809153	31.231604
517.899253	32683.853091	31.236621
518.373950	32734.853462	31.241639
518.774415	32788.885541	31.246656
519.167224	32850.998937	31.251674
519.814623	32923.065494	31.256692
520.709312	32989.589183	31.261709
521.297976	33038.331564	31.266727
522.017472	33098.139199	31.271744
522.693311	33166.494913	31.276762
523.577301	33201.890523	31.281780
523.769704	33252.929562	31.286797
524.256237	33305.384112	31.291815
524.756010	33370.103526	31.296832
525.314185	33416.422592	31.301850
525.755706	33485.241028	31.306868
526.081691	33538.382205	31.311885
526.522429	33599.591126	31.316903
526.838334	33662.246992	31.321920
527.009595	33720.844235	31.326938
528.071931	33794.562219	31.331956
528.118232	33846.318085	31.336973
528.910655	33922.889273	31.341991
529.599629	33992.511247	31.347008
529.886204	34056.413343	31.352026
530.866330	34112.947311	31.357044
531.177739	34181.789957	31.362061
531.956716	34236.833580	31.367079
532.118975	34303.959654	31.372096
532.998680	34370.569922	31.377114
533.437689	34425.468349	31.382132
534.131617	34497.057220	31.387149
534.531708	34571.881746	31.392167
535.152294	34610.103501	31.397184
535.290407	34688.537268	31.402202
535.926488	34750.172277	31.407220
536.538754	34826.291220	31.412237
537.164146	34894.529441	31.417255
537.772810	34964.111712	31.422272
538.232463	35028.717619	31.427290
538.878943	35079.096881	31.432308
539.362171	35159.517254	31.437325
540.040181	35221.178530	31.442343
540.717006	35283.840481	31.447360
541.170291	35362.909896	31.452378
541.911450	35408.598123	31.457396
542.154027	35495.032993	31.462413
542.612009	35545.069216	31.467431
543.437138	35614.927521	31.472448
544.005192	35697.109690	31.477466
544.566319	35758.905737	31.482484
545.283460	35809.322735	31.487501
545.572090	35876.399175	31.492519
546.257692	35930.441100	31.497536
546.526378	35990.932536	31.502554
547.321582	36062.794997	31.507572
547.347192	36127.990944	31.512589
547.835974	36201.958846	31.517607
548.801473	36273.462694	31.522624
549.466029	36340.210565	31.527642
550.223023	36387.571160	31.532660
550.897036	36447.520703	31.537677
551.057529	36515.917671	31.542695
551.772617	36569.170913	31.547712
551.741247	36647.085914	31.552730
552.642595	36679.153262	31.557748
552.786715	36750.756823	31.562765
553.308221	36796.775218	31.567783
554.160640	36863.140580	31.572800
554.789768	36934.630058	31.577818
555.268737	36986.692822	31.582836
555.672522	37057.929686	31.587853
556.114051	37119.832252	31.592871
557.035511	37179.560351	31.597888
557.634401	37258.472114	31.602906
558.493041	37294.962529	31.607924
558.792672	37376.780207	31.612941
559.248062	37423.937749	31.617959
560.191838	37479.649005	31.622976
560.080387	37556.946875	31.627994
560.761863	37612.215872	31.633012
561.377757	37696.434844	31.638029
561.828296	37750.312816	31.643047
562.375403	37808.643689	31.648064
562.804035	37881.154686	31.653082
563.323560	37949.911246	31.658100
564.115108	38030.486137	31.663117
564.811845	38096.910189	31.668135
565.506863	38159.541361	31.673152
566.130133	38228.613224	31.678170
566.499852	38302.054024	31.683188
566.911099	38364.912669	31.688205
567.300907	38436.728540	31.693223
567.859231	38510.584030	31.698240
568.202727	38594.154726	31.703258
568.956137	38651.084558	31.708276
569.613905	38752.577517	31.713293
569.708070	38832.516892	31.718311
570.644259	38905.582547	31.723328
571.047779	38990.410739	31.728346
571.944971	39057.111363	31.733364
572.839421	39118.210640	31.738381
572.930935	39196.409906	31.743399
573.795051	39278.029371	31.748416
574.575672	39348.351448	31.753434
575.047029	39419.406604	31.758452
575.942379	39505.579398	31.763469
576.251414	39568.244497	31.768487
577.428393	39644.360098	31.773504
577.556207	39716.704069	31.778522
578.503101	39768.820692	31.783540
578.849396	39844.667185	31.788557
579.351434	39915.034320	31.793575
579.843601	39976.670063	31.798592
580.271503	40058.368251	31.803610
580.684010	40138.904689	31.808628
581.381653	40200.068534	31.813645
581.791957	40285.867492	31.818663
582.773545	40360.367636	31.823680
583.048618	40453.064139	31.828698
583.636942	40515.809478	31.833716
584.490951	40588.504118	31.838733
584.783251	40672.872477	31.843751
585.640526	40737.265965	31.848768
585.923304	40831.743313	31.853786
586.436089	40886.343165	31.858804
587.306981	40961.814132	31.863821
588.170673	41039.237266	31.868839
588.839143	41104.155638	31.873856
589.171696	41166.446749	31.878874
589.973252	41246.147347	31.883892
590.523398	41304.668910	31.888909
590.973887	41381.167456	31.893927
591.795569	41432.308934	31.898944
591.970490	41506.937534	31.903962
592.652744	41567.805495	31.908980
593.582484	41625.239527	31.913997
593.948856	41703.378922	31.919015
594.994803	41754.758882	31.924032
595.586682	41808.985432	31.929050
595.684004	41886.737600	31.934068
596.260862	41939.076235	31.939085
596.586109	42029.430282	31.944103
597.232498	42080.637250	31.949120
597.394530	42161.839527	31.954138
597.864768	42240.942610	31.959156
598.514165	42324.258966	31.964173
598.640848	42425.083604	31.969191
599.320402	42490.888935	31.974208
600.374438	42594.421281	31.979226
600.785589	42672.936216	31.984244
601.395303	42763.089057	31.989261
601.720686	42852.455923	31.994279
602.625166	42945.525144	31.999296
603.105651	43042.266726	32.004314
603.583655	43137.487660	32.009332
604.801468	43216.083190	32.014349
604.592956	43309.142349	32.019367
605.790882	43406.676515	32.024384
606.670866	43488.230124	32.029402
607.442609	43569.536795	32.034420
608.202228	43640.402920	32.039437
608.594944	43718.868536	32.044455
609.594590	43813.173391	32.049472
610.307897	43879.940968	32.054490
610.590761	43967.164094	32.059508
611.435409	44026.251824	32.064525
612.375180	44117.007104	32.069543
613.256132	44182.261166	32.074560
613.772525	44248.184962	32.079578
614.175557	44346.104779	32.084596
615.133205	44392.989065	32.089613
615.631034	44477.123125	32.094631
615.855148	44539.866615	32.099648
616.830711	44615.818343	32.104666
617.414128	44695.001662	32.109684
617.965223	44759.601904	32.114701
618.355421	44854.729377	32.119719
618.846616	44920.754440	32.124736
619.546531	45008.999628	32.129754
619.703443	45079.591957	32.134772
620.450828	45166.845037	32.139789
620.687258	45251.606689	32.144807
620.921349	45354.481705	32.149824
621.936686	45439.544945	32.154842
622.648557	45522.344478	32.159860
623.403815	45604.736249	32.164877
623.462466	45720.946699	32.169895
624.271598	45814.421808	32.174912
624.806230	45898.720399	32.179930
625.388997	46010.959522	32.184948
626.419160	46074.885331	32.189965
626.935099	46177.910933	32.194983
627.707729	46263.475828	32.200000
628.248347	46364.180917	32.205018
628.939570	46447.411049	32.210036
629.686204	46523.863034	32.215053
630.144852	46634.775056	32.220071
630.843115	46717.279030	32.225088
631.781798	46793.053134	32.230106
632.106986	46874.978467	32.235124
632.786798	46951.506384	32.240141
633.847163	47039.878465	32.245159
633.776383	47124.200472	32.250176
634.822976	47188.935688	32.255194
635.489389	47278.419078	32.260212
636.189624	47350.284809	32.265229
636.681437	47439.961994	32.270247
637.305959	47513.826928	32.275264
638.240542	47581.622690	32.280282
639.161538	47660.724946	32.285300
639.698405	47736.755521	32.290317
640.214727	47796.840919	32.295335
640.865229	47886.127746	32.300352
641.471479	47963.846559	32.305370
641.933224	48048.826796	32.310388
642.779650	48133.342867	32.315405
643.001955	48223.393530	32.320423
643.655939	48309.025240	32.325440
644.547244	48391.529948	32.330458
644.439552	48488.223266	32.335476
645.307650	48568.907441	32.340493
646.240691	48661.530012	32.345511
646.645731	48769.520485	32.350528
647.356315	48847.882515	32.355546
648.047358	48957.459379	32.360564
648.722259	49029.206231	32.365581
649.275963	49131.982841	32.370599
649.850152	49241.356443	32.375616
650.861225	49326.605377	32.380634
651.388710	49424.922746	32.385652
651.624530	49510.051069	32.390669
653.219604	49591.383745	32.395687
653.823111	49689.348879	32.400704
654.392494	49776.084353	32.405722
654.722626	49868.695557	32.410740
655.839393	49958.635166	32.415757
656.224702	50044.356990	32.420775
656.681573	50142.080248	32.425792
657.285130	50224.937312	32.430810
657.501034	50341.058683	32.435828
658.287954	50414.977601	32.440845
659.018602	50529.483477	32.445863
659.656177	50643.127477	32.450880
660.272713	50729.878456	32.455898
661.096812	50860.230642	32.460916
662.035251	50944.822998	32.465933
662.526283	51047.667676	32.470951
662.940624	51148.043286	32.475968
664.021545	51235.534664	32.480986
664.578073	51354.779869	32.486004
665.420058	51429.562115	32.491021
665.847277	51533.822170	32.496039
666.491437	51623.440274	32.501056
667.290532	51727.668392	32.506074
668.387212	51823.039612	32.511092
669.472619	51908.114115	32.516109
669.968170	51999.186046	32.521127
670.725334	52079.369677	32.526144
671.600623	52163.639912	32.531162
672.102538	52255.811094	32.536180
672.550090	52332.815967	32.541197
673.684667	52428.319743	32.546215
674.177337	52491.266376	32.551232
675.014842	52595.657094	32.556250
675.282870	52669.528284	32.561268
675.969827	52763.073652	32.566285
676.465664	52864.796564	32.571303
677.071606	52934.232254	32.576320
677.769931	53021.937088	32.581338
678.672600	53104.504526	32.586356
679.258216	53188.413329	32.591373
680.062093	53261.955091	32.596391
680.362400	53341.549829	32.601408
680.980155	53435.874239	32.606426
681.342545	53522.471338	32.611444
681.992016	53601.421998	32.616461
682.693202	53712.695271	32.621479
683.501659	53795.183303	32.626496
684.197861	53890.634054	32.631514
684.463094	53983.023128	32.636532
684.987177	54080.594224	32.641549
685.719493	54191.012277	32.646567
686.054787	54300.744769	32.651584
687.382957	54389.624714	32.656602
688.281237	54502.152378	32.661620
688.917075	54599.562325	32.666637
689.533514	54693.532976	32.671655
690.048947	54794.147755	32.676672
691.023363	54907.309568	32.681690
691.355615	55006.294197	32.686708
692.293482	55111.736921	32.691725
692.946745	55216.247993	32.696743
693.759668	55309.190987	32.701760
694.812796	55401.639885	32.706778
695.489813	55519.832664	32.711796
695.925753	55598.523447	32.716813
696.326631	55715.764816	32.721831
697.145271	55821.218425	32.726848
697.773173	55926.546158	32.731866
698.611601	56048.000729	32.736884
698.667101	56163.633902	32.741901
699.532606	56254.803699	32.746919
700.107516	56386.456769	32.751936
701.109250	56506.383536	32.756954
701.757837	56611.793665	32.761972
702.406673	56739.576580	32.766989
703.192393	56843.859644	32.772007
703.587608	56962.025514	32.777024
704.378141	57073.442179	32.782042
705.222891	57189.702906	32.787060
705.670544	57331.107040	32.792077
706.572909	57432.328557	32.797095
707.279124	57545.935308	32.802112
708.269718	57659.426247	32.807130
708.926183	57776.656644	32.812148
709.528366	57898.603935	32.817165
710.889357	58007.107323	32.822183
711.536823	58121.971825	32.827200
712.398939	58208.456572	32.832218
713.166908	58327.219857	32.837236
713.649427	58423.208180	32.842253
714.597922	58542.075631	32.847271
715.043812	58641.824334	32.852288
716.042472	58756.950452	32.857306
716.758100	58858.285925	32.862324
717.215536	58964.100333	32.867341
718.099364	59085.502908	32.872359
718.738300	59192.514408	32.877376
719.515094	59282.417465	32.882394
720.124724	59403.241689	32.887412
720.425085	59510.443506	32.892429
721.475749	59619.563025	32.897447
721.661981	59737.723074	32.902464
722.809271	59831.662150	32.907482
723.421735	59957.506588	32.912500
724.243591	60066.805358	32.917517
724.707780	60161.945684	32.922535
725.337869	60285.128908	32.927552
726.498218	60376.787163	32.932570
726.963864	60489.755343	32.937588
727.946970	60599.409547	32.942605
728.714491	60685.332975	32.947623
729.315510	60801.800419	32.952640
729.827552	60911.616273	32.957658
730.466240	61013.474615	32.962676
731.058946	61147.355455	32.967693
731.804259	61225.214904	32.972711
732.520017	61362.678965	32.977728
733.356237	61468.235515	32.982746
734.098212	61585.695351	32.987764
734.990422	61711.055892	32.992781
735.904513	61821.214771	32.997799
736.308110	61936.760792	33.002816
737.220808	62054.650186	33.007834
737.490167	62170.270267	33.012852
738.363715	62283.882649	33.017869
739.555467	62398.447979	33.022887
740.073187	62528.558449	33.027904
740.632902	62646.635982	33.032922
741.047849	62767.917054	33.037940
741.818890	62887.863405	33.042957
742.942759	63014.476731	33.047975
743.528226	63145.787101	33.052992
744.233313	63267.623653	33.058010
745.160607	63397.122204	33.063028
745.505243	63524.973420	33.068045
745.951640	63656.790389	33.073063
746.934596	63786.250621	33.078080
747.943308	63927.330510	33.083098
748.444557	64060.973929	33.088116
749.519012	64180.492250	33.093133
750.556085	64327.979122	33.098151
751.364457	64442.556077	33.103168
752.022740	64580.885730	33.108186
753.139444	64696.519285	33.113204
753.642152	64831.185107	33.118221
755.005342	64934.390908	33.123239
755.413011	65062.601607	33.128256
756.465978	65184.467993	33.133274
757.059510	65293.390216	33.138292
757.593530	65418.933878	33.143309
758.460581	65540.005051	33.148327
759.108188	65663.635201	33.153344
759.746583	65791.932442	33.158362
760.837205	65911.755268	33.163380
761.381682	66062.180371	33.168397
762.068333	66163.689943	33.173415
762.880152	66308.074043	33.178432
763.878849	66423.148939	33.183450
764.375165	66544.325157	33.188468
764.892322	66688.090529	33.193485
765.910509	66800.098532	33.198503
766.657554	66935.129668	33.203520
767.162440	67060.321486	33.208538
768.216574	67187.117479	33.213556
768.890916	67327.997768	33.218573
769.568052	67433.080392	33.223591
770.465046	67569.146566	33.228608
771.314917	67700.018827	33.233626
772.055939	67824.348141	33.238644
772.859803	67957.954198	33.243661
773.656482	68088.350923	33.248679
774.406028	68205.550333	33.253696
775.077268	68324.893738	33.258714
775.820940	68439.788022	33.263732
776.651697	68565.371277	33.268749
777.746690	68679.241637	33.273767
778.421395	68802.171647	33.278784
779.070764	68909.327211	33.283802
779.964722	69023.959657	33.288820
780.384439	69154.064931	33.293837
781.171817	69268.166304	33.298855
781.881147	69408.536455	33.303872
782.489587	69528.687342	33.308890
783.311656	69663.805932	33.313908
783.836666	69783.282944	33.318925
785.249308	69923.679482	33.323943
785.721341	70055.159925	33.328960
786.295475	70181.636081	33.333978
786.994150	70326.970750	33.338996
787.666992	70451.668310	33.344013
788.565611	70597.464965	33.349031
788.974467	70742.464686	33.354048
789.909242	70889.907534	33.359066
790.944961	71024.335702	33.364084
791.845560	71164.597440	33.369101
792.290425	71309.708903	33.374119
793.274826	71445.463311	33.379136
793.934398	71595.763754	33.384154
795.338723	71729.673972	33.389172
795.612300	71884.933967	33.394189
796.741068	72030.866865	33.399207
797.725573	72161.940648	33.404224
798.614707	72296.476947	33.409242
799.569961	72434.063464	33.414260
800.432243	72580.290723	33.419277
801.352411	72703.974287	33.424295
802.315639	72832.792076	33.429312
803.055075	72976.114768	33.434330
803.940207	73099.212037	33.439348
804.561579	73240.304968	33.444365
805.955319	73363.073165	33.449383
806.944687	73493.123632	33.454400
807.550206	73626.197555	33.459418
808.827354	73740.602529	33.464436
809.384829	73871.947002	33.469453
810.145541	74001.361707	33.474471
810.995477	74115.175264	33.479488
811.330742	74259.496479	33.484506
812.228520	74370.881608	33.489524
812.703094	74520.695639	33.494541
813.582585	74640.887525	33.499559
814.292607	74788.470261	33.504576
814.889544	74919.688126	33.509594
815.928424	75078.284906	33.514612
816.475494	75207.324754	33.519629
816.993588	75349.732262	33.524647
818.238871	75481.200602	33.529664
818.616472	75626.409274	33.534682
819.815691	75762.528626	33.539700
820.508685	75930.908565	33.544717
821.709689	76063.545022	33.549735
822.223553	76204.858461	33.554752
822.928830	76349.195727	33.559770
823.638262	76491.572793	33.564788
824.848309	76642.848400	33.569805
825.514008	76788.820412	33.574823
826.549556	76936.711811	33.579840
827.212642	77091.464299	33.584858
828.332635	77232.943598	33.589876
828.680668	77371.136130	33.594893
829.791347	77506.224816	33.599911
830.359937	77620.375137	33.604928
831.019584	77774.355108	33.609946
831.737978	77908.986117	33.614964
832.608393	78060.498356	33.619981
833.459824	78195.330508	33.624999
834.040121	78338.019169	33.630016
834.897601	78482.857644	33.635034
835.873152	78610.411123	33.640052
836.352701	78771.574719	33.645069
837.511177	78914.171634	33.650087
838.516988	79070.854784	33.655104
839.046693	79212.071107	33.660122
840.202686	79366.960590	33.665140
840.489748	79517.099110	33.670157
841.633113	79686.249380	33.675175
842.896419	79816.374524	33.680192
843.169959	79968.814323	33.685210
844.091386	80118.415727	33.690228
845.208398	80281.521724	33.695245
846.066063	80421.211485	33.700263
846.629013	80584.411184	33.705280
847.359862	80746.306640	33.710298
848.735502	80887.159875	33.715316
849.413886	81049.199020	33.720333
850.296731	81197.833593	33.725351
851.062488	81354.407990	33.730368
851.964149	81521.847277	33.735386
852.857032	81675.259134	33.740404
853.578994	81845.058313	33.745421
854.575348	81990.586166	33.750439
855.552567	82157.581243	33.755456
856.170432	82317.406554	33.760474
857.522204	82462.398013	33.765492
858.387595	82639.397231	33.770509
858.937865	82786.212114	33.775527
859.965041	82950.756695	33.780544
860.709572	83110.066951	33.785562
861.625754	83274.119806	33.790580
862.448957	83432.900608	33.795597
863.528491	83599.130313	33.800615
864.661281	83746.974958	33.805632
865.513981	83907.272484	33.810650
866.572520	84063.735081	33.815668
867.400761	84217.731570	33.820685
868.389597	84359.720523	33.825703
869.081371	84526.394281	33.830720
869.841831	84680.645490	33.835738
871.158672	84813.004917	33.840756
871.584264	84977.461047	33.845773
872.463734	85120.832985	33.850791
873.380953	85288.158335	33.855808
874.327790	85435.152574	33.860826
875.272869	85597.167543	33.865844
876.157450	85748.463547	33.870861
877.089358	85909.204897	33.875879
877.887230	86053.342689	33.880896
878.635735	86207.739001	33.885914
879.947873	86361.853477	33.890932
880.879380	86513.937621	33.895949
881.605893	86667.923068	33.900967
882.923025	86815.953218	33.905984
883.458082	86970.573357	33.911002
884.267027	87114.905758	33.916020
885.379064	87273.589544	33.921037
886.059225	87424.468402	33.926055
886.849891	87571.742469	33.931072
887.651330	87718.737292	33.936090
888.353471	87866.401149	33.941108
888.801973	87997.435324	33.946125
890.197386	88156.540245	33.951143
891.195281	88304.683219	33.956160
891.542737	88465.583095	33.961178
892.556613	88613.023040	33.966196
893.598104	88760.250548	33.971213
894.176335	88899.557428	33.976231
895.040467	89071.430419	33.981248
895.553891	89227.866147	33.986266
896.364733	89392.043204	33.991284
897.139326	89555.417444	33.996301
898.152134	89722.176818	34.001319
899.702495	89891.392408	34.006336
900.424986	90071.667825	34.011354
901.265005	90219.747716	34.016372
902.367935	90381.118143	34.021389
902.896757	90537.604323	34.026407
903.937963	90696.683702	34.031424
904.339044	90880.321596	34.036442
905.564519	91043.150753	34.041460
906.635618	91212.784002	34.046477
907.355443	91394.506433	34.051495
908.247422	91564.969129	34.056512
909.019369	91734.377050	34.061530
910.093586	91910.070967	34.066548
911.371711	92075.885496	34.071565
912.513844	92246.545918	34.076583
913.448064	92423.070442	34.081600
914.162630	92607.682456	34.086618
915.373917	92769.437245	34.091636
915.828452	92954.506223	34.096653
916.327271	93127.260006	34.101671
917.629796	93309.761494	34.106688
918.243015	93495.099558	34.111706
919.145751	93681.289941	34.116724
920.254775	93853.606430	34.121741
920.759598	94052.257332	34.126759
922.211835	94212.102347	34.131776
922.858166	94407.296168	34.136794
924.470113	94578.155063	34.141812
925.527468	94757.195344	34.146829
925.736387	94948.085989	34.151847
927.338433	95125.652968	34.156864
928.285342	95285.265708	34.161882
928.993686	95453.197607	34.166900
930.037749	95652.108027	34.171917
930.937980	95820.871569	34.176935
931.951655	95996.466001	34.181952
933.010927	96185.839793	34.186970
934.127087	96351.596489	34.191988
934.820099	96537.590208	34.197005
935.780383	96715.755766	34.202023
937.192364	96896.310283	34.207040
937.567209	97058.744480	34.212058
938.296567	97236.939284	34.217076
939.169207	97415.263636	34.222093
939.899571	97605.424275	34.227111
940.945398	97790.875486	34.232128
941.627443	97976.052662	34.237146
942.760580	98167.043645	34.242164
943.729996	98346.055035	34.247181
944.478511	98553.671903	34.252199
945.647719	98726.462215	34.257216
946.686306	98919.177407	34.262234
947.741656	99113.619480	34.267252
948.831875	99281.071304	34.272269
949.745429	99473.469591	34.277287
950.607051	99630.573431	34.282304
951.569700	99812.938922	34.287322
952.245824	99980.856290	34.292340
953.180769	100146.174529	34.297357
953.815210	100340.360120	34.302375
955.309448	100512.387444	34.307392
956.009051	100684.388876	34.312410
956.731450	100863.250178	34.317428
957.980882	101056.472457	34.322445
958.644590	101239.480085	34.327463
959.692713	101416.689847	34.332480
960.241209	101615.432319	34.337498
961.285446	101805.927618	34.342516
962.484513	101996.740659	34.347533
963.155526	102190.776168	34.352551
964.854110	102347.841071	34.357568
966.304277	102546.536935	34.362586
967.002994	102734.247247	34.367604
968.020021	102912.612194	34.372621
968.680220	103101.895374	34.377639
970.246312	103288.269952	34.382656
971.222646	103462.378170	34.387674
972.071034	103647.272030	34.392692
973.180807	103833.833552	34.397709
974.038318	104011.099166	34.402727
975.375448	104190.173609	34.407744
976.166158	104376.247235	34.412762
976.912930	104557.333828	34.417780
978.152057	104748.059478	34.422797
978.841054	104922.908841	34.427815
979.564950	105114.608697	34.432832
980.851301	105302.658650	34.437850
981.816879	105499.513514	34.442868
982.702415	105690.962999	34.447885
983.497231	105885.803787	34.452903
984.115772	106073.089437	34.457920
985.180876	106278.690881	34.462938
986.137008	106485.489701	34.467956
987.218345	106699.336133	34.472973
988.221716	106888.020482	34.477991
989.363913	107094.248830	34.483008
990.375218	107287.303974	34.488026
991.032550	107494.096766	34.493044
992.275947	107707.506730	34.498061
992.990577	107912.874904	34.503079
994.287561	108115.970165	34.508096
995.289040	108310.807524	34.513114
996.565246	108513.238026	34.518132
997.881300	108712.281886	34.523149
998.881665	108897.612181	34.528167
1000.062069	109096.314027	34.533184
1000.723458	109282.108260	34.538202
1001.757354	109492.654150	34.543220
1003.296226	109680.522773	34.548237
1003.626345	109871.948704	34.553255
1005.248375	110067.380448	34.558272
1006.259191	110283.256042	34.563290
1006.644948	110460.529132	34.568308
1007.758243	110666.156735	34.573325
1008.752140	110867.891760	34.578343
1009.872081	111069.493493	34.583360
1010.867798	111271.383238	34.588378
1011.511341	111470.976665	34.593396
1012.716115	111660.839626	34.598413
1013.656319	111884.276350	34.603431
1014.704025	112079.500865	34.608448
1015.752318	112272.484649	34.613466
1016.687930	112481.081462	34.618484
1017.643486	112672.310020	34.623501
1018.325612	112874.808169	34.628519
1019.320233	113053.492461	34.633536
1020.320414	113257.790364	34.638554
1021.293589	113472.278876	34.643572
1022.150583	113664.822738	34.648589
1023.088827	113858.342613	34.653607
1024.009412	114068.917514	34.658624
1025.077505	114273.579142	34.663642
1025.403526	114496.669934	34.668660
1026.684631	114713.916915	34.673677
1027.511871	114924.868473	34.678695
1028.817579	115143.229563	34.683712
1029.773205	115377.979630	34.688730
1030.793003	115589.829252	34.693748
1031.872176	115818.393130	34.698765
1032.601256	116043.444131	34.703783
1033.986195	116269.845577	34.708800
1034.873303	116503.324242	34.713818
1035.927004	116729.518053	34.718836
1036.918656	116954.064293	34.723853
1037.814485	117188.484739	34.728871
1038.844035	117429.713791	34.733888
1040.224176	117670.380258	34.738906
1041.320010	117903.671411	34.743924
1042.774237	118114.796941	34.748941
1043.767886	118354.532154	34.753959
1045.006986	118572.183482	34.758976
1046.471456	118802.279089	34.763994
1047.275583	119031.978776	34.769012
1048.404359	119240.163634	34.774029
1049.168076	119471.710697	34.779047
1050.184790	119696.958763	34.784064
1051.553569	119920.972138	34.789082
1052.140021	120160.815122	34.794100
1053.601198	120387.984512	34.799117
1054.682890	120610.593554	34.804135
1055.890351	120847.590217	34.809152
1057.122206	121058.318093	34.814170
1058.140590	121291.561031	34.819188
1059.345221	121500.700089	34.824205
1060.480616	121732.558791	34.829223
1061.726094	121961.157332	34.834240
1062.814901	122177.416295	34.839258
1063.937884	122407.331044	34.844276
1065.358204	122612.134205	34.849293
1066.118234	122833.280168	34.854311
1067.295058	123051.659919	34.859328
1068.405815	123267.961354	34.864346
1069.142222	123483.502508	34.869364
1070.437173	123707.582677	34.874381
1071.596480	123924.058337	34.879399
1072.616036	124149.505231	34.884416
1073.890085	124366.687513	34.889434
1074.606339	124586.155797	34.894452
1075.656098	124804.569524	34.899469
1076.946810	125032.994438	34.904487
1077.430999	125254.470223	34.909504
1078.842955	125490.051367	34.914522
1080.171806	125698.870320	34.919540
1081.189007	125916.017620	34.924557
1082.027387	126158.123911	34.929575
1082.816849	126383.955226	34.934592
1084.333266	126603.610422	34.939610
1085.430255	126824.198250	34.944628
1086.249308	127062.551039	34.949645
1087.309362	127288.623289	34.954663
1088.291438	127499.577795	34.959680
1089.701663	127723.973271	34.964698
1090.187943	127947.737157	34.969716
1091.204010	128168.081997	34.974733
1092.253207	128393.961499	34.979751
1093.012574	128601.411705	34.984768
1094.274182	128826.562272	34.989786
1095.451380	129054.770257	34.994804
1096.911447	129280.677211	34.999821
1098.125135	129503.331143	35.004839
1098.938896	129724.848626	35.009856
1100.252363	129949.872135	35.014874
1101.352831	130188.583134	35.019892
1102.578209	130402.014427	35.024909
1104.034102	130617.411775	35.029927
1105.134262	130845.151421	35.034944
1106.250818	131065.728602	35.039962
1107.351404	131294.054523	35.044980
1108.770405	131522.621085	35.049997
1110.393868	131724.233092	35.055015
1110.989862	131938.311193	35.060032
1111.889240	132172.114515	35.065050
1112.939212	132384.688387	35.070068
1114.410188	132625.169512	35.075085
1115.011617	132837.224727	35.080103
1115.376840	133087.170605	35.085120
1116.708076	133313.445003	35.090138
1118.033903	133550.826170	35.095156
1118.852900	133791.816761	35.100173
1119.815148	134037.729284	35.105191
1120.883783	134298.406817	35.110208
1122.132452	134537.595459	35.115226
1122.951969	134792.132019	35.120244
1124.038774	135053.585983	35.125261
1125.176259	135309.177032	35.130279
1126.390775	135556.644185	35.135296
1127.422091	135830.258086	35.140314
1128.406842	136093.968497	35.145332
1129.422427	136350.082322	35.150349
1130.635351	136607.167101	35.155367
1131.716757	136886.613214	35.160384
1132.887057	137138.600233	35.165402
1134.270539	137408.442115	35.170420
1135.325198	137667.741933	35.175437
1136.746716	137935.566125	35.180455
1137.758150	138196.778932	35.185472
1139.259686	138456.645107	35.190490
1140.562351	138729.845507	35.195508
1141.665265	138977.306312	35.200525
1143.395120	139232.881022	35.205543
1144.121386	139494.379366	35.210560
1145.363139	139748.618633	35.215578
1146.823019	139994.937740	35.220596
1147.998809	140255.987495	35.225613
1148.956667	140494.329495	35.230631
1150.145847	140758.170286	35.235648
1151.147855	141000.084036	35.240666
1152.246815	141278.803574	35.245684
1153.348719	141536.211209	35.250701
1154.469232	141784.792950	35.255719
1155.596777	142050.847532	35.260736
1156.891965	142299.543683	35.265754
1157.836520	142574.926621	35.270772
1158.515714	142839.755377	35.275789
1160.024456	143096.346877	35.280807
1161.171197	143372.425606	35.285824
1162.291927	143633.548485	35.290842
1163.422181	143911.903977	35.295860
1164.474993	144162.859984	35.300877
1165.715185	144420.063604	35.305895
1166.835729	144675.741880	35.310912
1167.831763	144930.910011	35.315930
1168.468952	145175.601725	35.320948
1169.531807	145451.888402	35.325965
1170.561988	145701.540456	35.330983
1171.533075	145993.989113	35.336000
1173.078694	146251.713768	35.341018
1174.061495	146546.282793	35.346036
1175.117799	146824.369360	35.351053
1176.569429	147109.443616	35.356071
1177.733048	147378.158072	35.361088
1179.197571	147644.060340	35.366106
1179.695786	147940.103192	35.371124
1180.956950	148216.594315	35.376141
1182.357155	148501.992548	35.381159
1183.205708	148799.151380	35.386176
1184.669061	149072.457940	35.391194
1186.145472	149372.117648	35.396212
1187.137112	149659.469416	35.401229
1188.368248	149936.650831	35.406247
1189.541459	150233.082996	35.411264
1190.826350	150531.566370	35.416282
1191.822984	150817.632834	35.421300
1193.236630	151113.043203	35.426317
1194.777858	151391.199060	35.431335
1195.807124	151705.841228	35.436352
1196.861520	151991.780445	35.441370
1198.172308	152293.431866	35.446388
1199.339631	152579.674044	35.451405
1200.926347	152872.330323	35.456423
1202.027774	153172.399959	35.461440
1203.458058	153458.909863	35.466458
1204.809904	153764.815326	35.471476
1205.649783	154047.102075	35.476493
1207.330093	154346.705011	35.481511
1208.192136	154636.894460	35.486528
1209.209697	154946.492220	35.491546
1210.579062	155224.616103	35.496564
1212.275426	155517.059134	35.501581
1213.325203	155818.350545	35.506599
1214.322041	156110.190558	35.511616
1215.966242	156409.498518	35.516634
1216.968889	156711.933603	35.521652
1218.215612	157001.303672	35.526669
1219.873022	157290.430522	35.531687
1220.751664	157596.419300	35.536704
1222.069263	157879.302258	35.541722
1223.673973	158175.180027	35.546740
1224.752644	158457.700670	35.551757
1226.364367	158729.137318	35.556775
1227.579316	159032.506674	35.561792
1228.960939	159318.649504	35.566810
1230.070195	159610.141864	35.571828
1230.997208	159888.029488	35.576845
1232.183954	160185.856025	35.581863
1233.572958	160469.646359	35.586880
1234.640936	160767.243096	35.591898
1236.384329	161058.222681	35.596916
1237.288874	161346.031773	35.601933
1238.734775	161632.535689	35.606951
1239.857781	161922.926142	35.611968
1241.002953	162192.966249	35.616986
1242.044764	162482.765141	35.622004
1242.935532	162787.408763	35.627021
1244.457749	163081.737760	35.632039
1245.814228	163385.661922	35.637056
1246.872147	163664.010443	35.642074
1248.387820	163946.459228	35.647092
1249.183702	164229.815320	35.652109
1250.391426	164507.713399	35.657127
1251.387010	164800.834729	35.662144
1252.549999	165078.388734	35.667162
1253.899185	165364.871008	35.672180
1255.152133	165649.823258	35.677197
1256.553605	165946.539495	35.682215
1257.491481	166233.691835	35.687232
1258.640416	166535.592286	35.692250
1260.403759	166826.012630	35.697268
1261.336953	167125.364562	35.702285
1262.711177	167426.447454	35.707303
1263.722383	167747.081007	35.712320
1264.794177	168033.639617	35.717338
1265.955861	168349.355209	35.722356
1267.034332	168677.026410	35.727373
1268.505432	168974.373699	35.732391
1269.633979	169308.956468	35.737408
1270.723066	169622.840706	35.742426
1272.151514	169941.505499	35.747444
1273.470014	170270.595421	35.752461
1274.624223	170586.137933	35.757479
1275.780099	170918.863078	35.762496
1277.148842	171231.608563	35.767514
1278.601517	171562.703371	35.772532
1280.168686	171889.721193	35.777549
1281.567671	172215.474833	35.782567
1282.920195	172546.732936	35.787584
1283.796303	172871.892342	35.792602
1285.332836	173198.429718	35.797620
1286.436679	173523.315046	35.802637
1287.760275	173861.820453	35.807655
1288.884204	174197.785267	35.812672
1290.135614	174541.713372	35.817690
1291.888674	174868.011038	35.822708
1292.976570	175197.847062	35.827725
1294.330485	175544.900035	35.832743
1295.850182	175871.078195	35.837760
1297.027520	176211.084061	35.842778
1298.667458	176543.173350	35.847796
1299.970861	176872.338229	35.852813
1301.089263	177220.254460	35.857831
1302.812859	177556.309090	35.862848
1304.017753	177884.887986	35.867866
1305.422965	178218.144334	35.872884
1306.252315	178558.389160	35.877901
1307.979289	178886.850561	35.882919
1308.857304	179231.698846	35.887936
1310.370323	179575.759411	35.892954
1312.420987	179899.414935	35.897972
1313.319146	180240.281853	35.902989
1314.863700	180557.742967	35.908007
1316.364103	180901.319786	35.913024
1317.435587	181236.593288	35.918042
1318.493307	181584.131434	35.923060
1319.701103	181910.401185	35.928077
1321.131562	182255.344038	35.933095
1322.329217	182595.466626	35.938112
1323.498371	182926.724452	35.943130
1325.089076	183271.609585	35.948148
1325.903127	183626.753542	35.953165
1327.300492	183958.335658	35.958183
1328.918824	184316.994237	35.963200
1330.012231	184653.948998	35.968218
1331.531617	184995.074898	35.973236
1332.336714	185331.726158	35.978253
1334.198359	185667.443609	35.983271
1335.513780	186010.932421	35.988288
1336.640622	186334.666435	35.993306
1338.293809	186666.616674	35.998324
1339.800225	186998.301226	36.003341
1341.156659	187315.720173	36.008359
1342.140236	187635.322245	36.013376
1343.324908	187991.627107	36.018394
1344.603340	188308.785401	36.023412
1345.574619	188658.440409	36.028429
1346.789866	189004.858597	36.033447
1348.325164	189348.217742	36.038464
1349.278386	189715.183577	36.043482
1350.722679	190065.822839	36.048500
1352.158814	190420.121408	36.053517
1353.244225	190782.197904	36.058535
1354.561529	191127.101630	36.063552
1355.829035	191505.375432	36.068570
1357.509794	191854.653710	36.073588
1358.489198	192240.850158	36.078605
1359.982388	192611.375836	36.083623
1361.392572	192959.461308	36.088640
1362.537343	193361.531069	36.093658
1364.268565	193743.220984	36.098676
1365.467618	194120.431115	36.103693
1366.842643	194501.448340	36.108711
1368.703277	194862.926827	36.113728
1369.824701	195243.203478	36.118746
1372.105819	195600.541904	36.123764
1373.389703	195976.137261	36.128781
1375.183989	196329.967579	36.133799
1377.172449	196670.031784	36.138816
1378.457427	197028.799629	36.143834
1379.775892	197389.696786	36.148852
1381.044425	197754.717513	36.153869
1382.274280	198108.257404	36.158887
1383.852223	198474.526104	36.163904
1384.751641	198832.809126	36.168922
1385.997062	199184.295674	36.173940
1387.320363	199546.689518	36.178957
1389.019983	199917.529389	36.183975
1390.673946	200287.210867	36.188992
1391.559493	200668.637926	36.194010
1393.017980	201034.420093	36.199028
1394.096720	201404.355031	36.204045
1395.692880	201786.674143	36.209063
1397.337264	202146.718413	36.214080
1398.327431	202536.111908	36.219098
1399.634424	202909.343736	36.224116
1401.471277	203295.173782	36.229133
1402.290194	203680.170930	36.234151
1404.130614	204058.640669	36.239168
1405.388177	204435.735820	36.244186
1406.750472	204818.529163	36.249204
1408.259307	205200.640139	36.254221
1409.568246	205588.372698	36.259239
1411.040838	205960.399740	36.264256
1412.539912	206356.408726	36.269274
1413.634526	206743.395565	36.274292
1415.183810	207126.995465	36.279309
1416.435567	207528.117627	36.284327
1417.926870	207913.305555	36.289344
1419.032427	208308.082012	36.294362
1420.657566	208704.476200	36.299380
1421.913524	209106.494794	36.304397
1423.425411	209494.544170	36.309415
1425.068545	209886.281477	36.314432
1425.755694	210302.265736	36.319450
1427.214757	210672.032470	36.324468
1428.866965	211067.392930	36.329485
1429.993605	211449.344375	36.334503
1431.895611	211826.319110	36.339520
1433.113763	212215.420595	36.344538
1434.469937	212603.904338	36.349556
1435.764133	213002.710873	36.354573
1437.022838	213392.585752	36.359591
1438.357709	213838.194465	36.364608
1439.609864	214246.765941	36.369626
1441.363998	214642.329742	36.374644
1443.092863	215042.013757	36.379661
1444.221250	215433.138433	36.384679
1445.700040	215842.873641	36.389696
1447.424028	216247.135340	36.394714
1448.857108	216642.507124	36.399732
1450.868715	217044.845561	36.404749
1451.983949	217459.524354	36.409767
1453.588218	217855.152505	36.414784
1454.530520	218260.517204	36.419802
1455.943448	218674.390360	36.424820
1457.319660	219074.683634	36.429837
1458.658747	219500.306281	36.434855
1460.107778	219920.248930	36.439872
1461.883794	220343.720543	36.444890
1463.057201	220765.337762	36.449908
1465.156959	221174.231790	36.454925
1466.310255	221610.510645	36.459943
1468.125613	222025.550638	36.464960
1469.288675	222446.109829	36.469978
1470.785545	222866.387050	36.474996
1472.586236	223299.213581	36.480013
1473.753985	223724.323484	36.485031
1475.379380	224165.792653	36.490048
1476.911979	224593.715848	36.495066
1478.316787	225021.026817	36.500084
1479.372193	225432.293979	36.505101
1481.205939	225874.980152	36.510119
1482.689087	226316.074938	36.515136
1483.660169	226761.167434	36.520154
1485.164691	227204.090832	36.525172
1486.906120	227649.491365	36.530189
1488.193411	228104.036221	36.535207
1489.792985	228539.100331	36.540224
1491.084546	228993.038190	36.545242
1492.847364	229435.952505	36.550260
1494.583431	229884.257620	36.555277
1496.136876	230332.289635	36.560295
1497.784082	230761.994081	36.565312
1499.211517	231215.231576	36.570330
1500.892818	231648.540123	36.575348
1502.448495	232100.337004	36.580365
1503.792041	232549.960512	36.585383
1505.764444	232983.123617	36.590400
1507.107245	233439.151070	36.595418
1508.748898	233874.378113	36.600436
1510.287201	234329.487065	36.605453
1511.398497	234768.385791	36.610471
1513.099864	235210.160353	36.615488
1514.393447	235680.529017	36.620506
1516.223452	236097.493306	36.625524
1517.637721	236548.539676	36.630541
1519.589598	236997.822098	36.635559
1520.924617	237431.585621	36.640576
1522.344653	237887.740394	36.645594
1524.149056	238325.010366	36.650612
1525.443396	238760.892301	36.655629
1526.647316	239219.245356	36.660647
1528.384214	239645.225941	36.665664
1530.035308	240085.141880	36.670682
1531.475766	240499.412270	36.675700
1533.015241	240917.934743	36.680717
1534.094876	241358.455927	36.685735
1535.721339	241780.725365	36.690752
1537.645295	242210.465616	36.695770
1538.904765	242645.092003	36.700788
1540.585595	243071.597239	36.705805
1541.393455	243509.906995	36.710823
1543.405337	243955.563430	36.715840
1544.380318	244397.810088	36.720858
1545.430871	244855.870815	36.725876
1547.383958	245301.844325	36.730893
1548.677556	245776.124248	36.735911
1549.918643	246238.804741	36.740928
1551.663356	246701.504556	36.745946
1553.089862	247175.129998	36.750964
1554.677126	247658.941597	36.755981
1556.207586	248130.874895	36.760999
1557.985832	248596.950814	36.766016
1559.439894	249083.962033	36.771034
1560.767251	249553.720956	36.776052
1562.366714	250040.938225	36.781069
1564.034344	250522.632492	36.786087
1565.910248	251006.706311	36.791104
1567.422090	251497.115352	36.796122
1569.116207	251981.017152	36.801140
1570.875782	252468.973197	36.806157
1572.089382	252960.144445	36.811175
1573.681286	253441.371986	36.816192
1575.065762	253942.397851	36.821210
1576.641041	254446.263266	36.826228
1578.032250	254940.963560	36.831245
1579.594162	255453.570743	36.836263
1580.892858	255957.559267	36.841280
1582.713820	256465.374074	36.846298
1584.517816	256971.083543	36.851316
1586.378370	257485.395681	36.856333
1587.876462	257990.749740	36.861351
1589.730918	258491.498048	36.866368
1591.081633	259006.555510	36.871386
1592.806149	259501.559080	36.876404
1594.455760	260017.355043	36.881421
1596.049732	260542.864360	36.886439
1597.698310	261051.319128	36.891456
1599.153938	261582.643349	36.896474
1600.853474	262103.435771	36.901492
1602.373925	262617.246403	36.906509
1604.104529	263144.562264	36.911527
1605.767144	263652.277902	36.916544
1607.413818	264156.871444	36.921562
1609.298337	264684.059916	36.926580
1611.109953	265191.826713	36.931597
1612.125984	265701.553593	36.936615
1614.041158	266228.964946	36.941632
1615.623803	266736.133677	36.946650
1616.989449	267262.999984	36.951668
1619.065677	267781.162394	36.956685
1620.426497	268300.534781	36.961703
1622.109302	268815.789104	36.966720
1623.875175	269346.448960	36.971738
1625.178318	269871.799181	36.976756
1626.828880	270379.665020	36.981773
1628.510770	270918.288235	36.986791
1629.795693	271435.307522	36.991808
1632.217242	271969.158640	36.996826
1633.900441	272466.728439	37.001844
1635.713854	272970.906264	37.006861
1637.113697	273487.472022	37.011879
1638.742466	273978.393177	37.016896
1640.526082	274468.881617	37.021914
1641.457615	274981.229254	37.026932
1643.123109	275476.460525	37.031949
1644.597136	275983.331584	37.036967
1646.305395	276488.867568	37.041984
1647.711850	277009.338336	37.047002
1649.479946	277515.370592	37.052020
1651.262790	278027.318203	37.057037
1652.863301	278534.011147	37.062055
1654.967591	279039.121177	37.067072
1656.797558	279557.484594	37.072090
1658.238059	280076.190519	37.077108
1659.956744	280582.783294	37.082125
1661.415716	281108.189916	37.087143
1663.182783	281629.784892	37.092160
1665.058362	282158.574810	37.097178
1666.262673	282686.280188	37.102196
1667.891726	283209.087706	37.107213
1669.218818	283740.072183	37.112231
1670.882517	284286.037430	37.117248
1672.897781	284812.231348	37.122266
1674.301801	285349.625035	37.127284
1676.363862	285887.238707	37.132301
1678.278658	286432.317580	37.137319
1679.772291	286972.510881	37.142336
1681.496926	287517.998530	37.147354
1682.881123	288063.311857	37.152372
1685.310515	288594.734254	37.157389
1686.785707	289155.116923	37.162407
1688.280488	289697.434229	37.167424
1690.084965	290253.948267	37.172442
1691.335656	290804.175936	37.177460
1693.067351	291361.916868	37.182477
1694.512353	291915.613365	37.187495
1695.937130	292485.109965	37.192512
1697.717520	293056.120270	37.197530
1699.058281	293631.417030	37.202548
1700.993676	294215.426914	37.207565
1702.590611	294798.423128	37.212583
1704.334811	295369.759192	37.217600
1706.345733	295960.047516	37.222618
1708.027625	296522.727102	37.227636
1710.011879	297113.928455	37.232653
1711.499888	297696.522095	37.237671
1713.241649	298284.074516	37.242688
1715.352094	298847.687942	37.247706
1717.214363	299436.738318	37.252724
1719.034240	300010.451637	37.257741
1720.754121	300607.087919	37.262759
1722.246131	301191.033773	37.267776
1724.277665	301762.975511	37.272794
1725.630446	302351.230060	37.277812
1727.271595	302922.340719	37.282829
1728.749765	303528.549453	37.287847
1730.608825	304103.173014	37.292864
1732.781126	304678.427208	37.297882
1734.516542	305273.585380	37.302900
1736.568288	305858.935043	37.307917
1737.836908	306443.699081	37.312935
1739.606345	307041.075219	37.317952
1741.280412	307634.552031	37.322970
1742.857645	308216.104461	37.327988
1744.718904	308822.139128	37.333005
1746.301863	309412.419010	37.338023
1747.916100	310013.635369	37.343040
1749.747284	310603.993018	37.348058
1751.262984	311187.948032	37.353076
1753.186138	311756.111867	37.358093
1754.807701	312323.991362	37.363111
1756.677269	312914.199092	37.368128
1758.294216	313470.313274	37.373146
1759.464366	314073.477627	37.378164
1761.502103	314646.553959	37.383181
1763.058963	315242.839674	37.388199
1764.310909	315834.600073	37.393216
1766.331107	316446.747453	37.398234
1767.628993	317052.381190	37.403252
1769.536947	317672.866138	37.408269
1771.330273	318280.541070	37.413287
1772.760803	318906.858525	37.418304
1775.035766	319502.686632	37.423322
1776.697327	320136.573012	37.428340
1778.219696	320751.584602	37.433357
1780.637327	321378.986811	37.438375
1782.398609	322005.374293	37.443392
1784.315997	322631.704838	37.448410
1785.635270	323259.880216	37.453428
1787.795100	323891.084898	37.458445
1790.222128	324504.034046	37.463463
1792.251942	325135.425892	37.468480
1794.544530	325740.108102	37.473498
1796.366463	326358.699946	37.478516
1798.374211	326969.790396	37.483533
1800.512585	327598.372309	37.488551
1801.619991	328203.251721	37.493568
1803.776131	328841.821523	37.498586
1805.198908	329464.383552	37.503604
1807.455891	330080.606675	37.508621
1808.902101	330698.988264	37.513639
1810.290994	331327.731256	37.518656
1812.343057	331954.860221	37.523674
1814.506226	332581.887926	37.528692
1815.973019	333229.917527	37.533709
1817.823511	333868.153205	37.538727
1819.395219	334503.660505	37.543744
1821.270962	335144.695492	37.548762
1823.253650	335793.067460	37.553780
1825.065901	336415.312370	37.558797
1827.532103	337058.817056	37.563815
1829.007613	337707.478434	37.568832
1830.721395	338344.034771	37.573850
1832.384562	338994.629618	37.578868
1833.749335	339641.584929	37.583885
1836.124592	340283.847188	37.588903
1837.709999	340943.416631	37.593920
1839.976471	341573.318906	37.598938
1841.844587	342237.394105	37.603956
1843.850461	342887.477320	37.608973
1845.801401	343519.463460	37.613991
1847.414649	344171.092341	37.619008
1849.584186	344815.513962	37.624026
1851.210622	345463.011729	37.629044
1853.160006	346133.798292	37.634061
1855.269481	346770.488080	37.639079
1856.898573	347425.979451	37.644096
1858.612650	348060.179224	37.649114
1860.303856	348722.977279	37.654132
1862.272240	349380.847394	37.659149
1863.726933	350024.834453	37.664167
1865.405164	350693.925963	37.669184
1867.011938	351363.958491	37.674202
1869.054553	352038.756449	37.679220
1870.506787	352710.647152	37.684237
1872.800197	353353.027609	37.689255
1874.709892	354030.279098	37.694272
1876.568346	354661.901808	37.699290
1878.131818	355320.538858	37.704308
1879.875890	355971.244320	37.709325
1881.909010	356633.311205	37.714343
1883.112634	357281.472380	37.719360
1885.609183	357939.230388	37.724378
1887.703036	358604.732967	37.729396
1889.404637	359256.638653	37.734413
1891.371870	359916.914303	37.739431
1893.094568	360590.362960	37.744448
1894.925052	361249.447370	37.749466
1896.716599	361930.119250	37.754484
1898.492025	362619.358021	37.759501
1900.207255	363295.883974	37.764519
1901.786563	363990.002904	37.769536
1903.908988	364685.593122	37.774554
1905.365541	365380.215410	37.779572
1906.642304	366083.252369	37.784589
1909.186067	366791.166855	37.789607
1910.496130	367525.502949	37.794624
1912.509420	368250.424354	37.799642
1914.650278	368976.325679	37.804660
1916.587716	369704.073112	37.809677
1918.597543	370417.360990	37.814695
1920.596035	371162.725250	37.819712
1922.688494	371884.190088	37.824730
1924.486694	372618.295824	37.829748
1926.421087	373371.159561	37.834765
1928.609023	374080.263703	37.839783
1930.529596	374841.088961	37.844800
1932.992689	375572.894846	37.849818
1934.937078	376297.416192	37.854836
1937.256840	377034.998351	37.859853
1939.184082	377763.804067	37.864871
1941.060865	378499.272885	37.869888
1942.952674	379236.727181	37.874906
1945.011663	379973.225252	37.879924
1947.013679	380724.323906	37.884941
1949.068212	381462.591256	37.889959
1950.708554	382214.604296	37.894976
1952.693351	382942.200491	37.899994
1954.576136	383696.270502	37.905012
1955.882304	384440.960617	37.910029
1958.176737	385204.918984	37.915047
1960.187555	385952.704382	37.920064
1961.874881	386722.432542	37.925082
1964.414641	387471.110115	37.930100
1966.552361	388236.722125	37.935117
1968.672426	388987.715535	37.940135
1970.660325	389748.524454	37.945152
1972.946603	390497.553450	37.950170
1975.225408	391245.450467	37.955188
1977.026054	391988.439835	37.960205
1979.390235	392741.712046	37.965223
1980.958554	393500.699434	37.970240
1983.037221	394246.149193	37.975258
1985.215744	394983.782519	37.980276
1986.953692	395741.723286	37.985293
1989.006492	396491.228749	37.990311
1990.798471	397237.007377	37.995328
1992.802658	397997.838413	38.000346
1994.715025	398744.066532	38.005364
1996.441209	399515.524120	38.010381
1998.425225	400273.867071	38.015399
2000.430149	401035.228125	38.020416
2002.219619	401794.602808	38.025434
2004.591914	402536.553179	38.030452
2006.480763	403279.527165	38.035469
2008.272447	404032.051243	38.040487
2009.989349	404760.773907	38.045504
2012.182482	405513.344679	38.050522
2014.207793	406243.194622	38.055540
2016.058645	406997.606574	38.060557
2018.215756	407735.047913	38.065575
2019.894305	408493.907122	38.070592
2021.304674	409251.370966	38.075610
2023.772429	410012.490489	38.080628
2025.363394	410776.545558	38.085645
2027.100237	411545.875174	38.090663
2029.241803	412323.324014	38.095680
2031.244500	413110.652818	38.100698
2033.702258	413895.375670	38.105716
2035.089422	414690.688170	38.110733
2037.011824	415479.454822	38.115751
2039.128741	416279.006633	38.120768
2041.380259	417085.046578	38.125786
2043.426619	417894.185435	38.130804
2045.184164	418698.484027	38.135821
2047.629078	419502.441635	38.140839
2049.713982	420324.844776	38.145856
2051.276907	421148.497807	38.150874
2053.773673	421953.256203	38.155892
2056.024181	422801.635087	38.160909
2058.439838	423586.172751	38.165927
2060.294464	424417.925957	38.170944
2062.932045	425225.417587	38.175962
2065.185588	426051.758468	38.180980
2066.924367	426869.472367	38.185997
2069.334109	427679.048041	38.191015
2071.198659	428507.016105	38.196032
2073.224823	429332.093950	38.201050
2075.362618	430160.365565	38.206068
2076.864742	431005.167673	38.211085
2078.898900	431836.385628	38.216103
2080.905079	432686.209065	38.221120
2082.687595	433534.672115	38.226138
2085.180265	434390.074473	38.231156
2086.800450	435249.993401	38.236173
2089.032703	436105.072332	38.241191
2090.902776	436961.849835	38.246208
2093.069492	437833.022123	38.251226
2095.117465	438691.983625	38.256244
2096.942176	439570.282596	38.261261
2099.293819	440445.272523	38.266279
2101.534905	441315.692387	38.271296
2103.485337	442199.334164	38.276314
2105.560425	443074.470099	38.281332
2107.780252	443949.800868	38.286349
2109.864641	444834.480072	38.291367
2111.797931	445714.645780	38.296384
2113.943783	446610.981799	38.301402
2116.500839	447480.298574	38.306420
2118.709528	448391.323919	38.311437
2121.175573	449265.795002	38.316455
2123.935448	450147.972341	38.321472
2125.558847	451025.141349	38.326490
2127.773240	451900.861792	38.331508
2130.133176	452772.526429	38.336525
2132.158713	453643.906862	38.341543
2134.447496	454530.784954	38.346560
2136.333517	455406.313078	38.351578
2138.751401	456275.395444	38.356596
2141.072673	457152.042691	38.361613
2143.684464	458011.311147	38.366631
2145.836329	458872.490476	38.371648
2147.888892	459717.318396	38.376666
2150.128678	460533.362269	38.381684
2151.800623	461393.503200	38.386701
2153.970276	462208.227304	38.391719
2155.868720	463059.513738	38.396736
2157.786129	463898.122982	38.401754
2159.966427	464731.244865	38.406772
2161.903985	465594.245506	38.411789
2163.888361	466449.265224	38.416807
2166.056811	467310.535426	38.421824
2168.033067	468178.774204	38.426842
2170.327195	469032.720661	38.431860
2171.893996	469921.316523	38.436877
2174.462312	470788.583278	38.441895
2177.054130	471655.251349	38.446912
2179.442674	472538.639145	38.451930
2181.941089	473395.441273	38.456948
2183.587388	474297.666249	38.461965
2185.690082	475174.764466	38.466983
2188.003726	476051.079918	38.472000
2189.596507	476950.913689	38.477018
2191.822264	477856.510182	38.482036
2193.737577	478766.154948	38.487053
2196.210508	479674.956093	38.492071
2198.057968	480603.816840	38.497088
2200.027132	481523.822770	38.502106
2202.386068	482452.606770	38.507124
2204.267409	483381.321287	38.512141
2206.183146	484317.658336	38.517159
2208.685728	485264.100668	38.522176
2210.497478	486223.280772	38.527194
2212.850294	487163.033400	38.532212
2214.713314	488131.342452	38.537229
2217.404623	489079.167624	38.542247
2219.713867	490066.380546	38.547264
2221.925060	491046.840739	38.552282
2224.414489	492000.044372	38.557300
2226.681858	492973.018056	38.562317
2228.964513	493935.840814	38.567335
2231.503026	494910.023984	38.572352
2233.704106	495868.614281	38.577370
2236.110262	496847.402881	38.582388
2238.628825	497816.933470	38.587405
2240.861700	498791.299762	38.592423
2242.946514	499756.754794	38.597440
2245.078488	500730.420704	38.602458
2247.523637	501713.260907	38.607476
2250.155754	502685.368903	38.612493
2252.654763	503642.259381	38.617511
2255.311660	504608.702446	38.622528
2257.748912	505581.328831	38.627546
2259.678328	506541.272575	38.632564
2262.370611	507496.243593	38.637581
2264.621802	508465.552679	38.642599
2266.925084	509412.962077	38.647616
2268.839700	510370.968533	38.652634
2271.564647	511345.371939	38.657652
2273.789834	512310.169548	38.662669
2275.838401	513262.184076	38.667687
2278.126894	514218.739838	38.672704
2280.097225	515187.942260	38.677722
2282.592283	516152.412231	38.682740
2285.045338	517112.143012	38.687757
2287.127106	518083.265906	38.692775
2289.211988	519036.942427	38.697792
2291.581025	520017.522753	38.702810
2294.227904	520977.135230	38.707828
2296.056567	521937.729976	38.712845
2298.326975	522890.886832	38.717863
2300.475611	523819.168509	38.722880
2302.762779	524770.694323	38.727898
2304.939737	525703.289679	38.732916
2306.897382	526653.089785	38.737933
2309.142460	527610.790867	38.742951
2311.432645	528552.660421	38.747968
2313.610054	529523.344892	38.752986
2315.721048	530485.618341	38.758004
2318.249422	531448.818212	38.763021
2320.243006	532417.682796	38.768039
2322.516235	533404.511770	38.773056
2324.759939	534384.986764	38.778074
2326.991466	535374.912248	38.783092
2329.040580	536368.827592	38.788109
2331.032602	537373.052852	38.793127
2333.718258	538381.271490	38.798144
2335.843780	539388.958577	38.803162
2338.243583	540402.065249	38.808180
2340.810623	541418.796293	38.813197
2343.322085	542444.369719	38.818215
2346.157929	543463.124511	38.823232
2347.956371	544496.063009	38.828250
2350.441446	545529.466730	38.833268
2352.685856	546550.007942	38.838285
2354.931796	547602.462592	38.843303
2357.695001	548625.633739	38.848320
2359.621321	549666.217004	38.853338
2362.321153	550721.126781	38.858356
2364.851749	551753.056009	38.863373
2367.254997	552805.240582	38.868391
2369.690029	553862.617775	38.873408
2371.719423	554921.588559	38.878426
2374.227954	555968.635928	38.883444
2376.315350	557042.360405	38.888461
2378.545664	558112.558454	38.893479
2381.284883	559178.567205	38.898496
2383.586480	560251.196138	38.903514
2386.032759	561344.365646	38.908532
2388.580214	562415.825094	38.913549
2390.807502	563482.226985	38.918567
2393.233982	564579.553591	38.923584
2395.776333	565663.358537	38.928602
2398.131633	566757.099242	38.933620
2400.164354	567840.004152	38.938637
2402.245635	568947.868510	38.943655
2405.156103	570025.575369	38.948672
2407.463932	571145.214579	38.953690
2410.058242	572242.770398	38.958708
2412.539269	573337.439692	38.963725
2414.569653	574462.356435	38.968743
2417.543051	575560.016078	38.973760
2419.886324	576668.775403	38.978778
2422.173709	577778.701012	38.983796
2424.734250	578880.455322	38.988813
2426.981338	580007.200225	38.993831
2429.192427	581113.230443	38.998848
2431.891695	582223.245296	39.003866
2434.523605	583331.566669	39.008884
2437.104356	584456.899435	39.013901
2439.440368	585572.089486	39.018919
2441.460822	586678.304227	39.023936
2443.998406	587812.412015	39.028954
2446.294745	588922.639366	39.033972
2448.980653	590054.307215	39.038989
2451.158523	591186.052956	39.044007
2453.871359	592304.472155	39.049024
2456.351250	593413.152789	39.054042
2458.724767	594523.000817	39.059060
2461.429705	595611.845897	39.064077
2463.487355	596703.152728	39.069095
2465.762244	597788.311140	39.074112
2468.563467	598904.090443	39.079130
2470.718106	599988.163875	39.084148
2473.169218	601103.891493	39.089165
2475.579121	602186.366400	39.094183
2478.174161	603299.706227	39.099200
2480.508690	604410.328165	39.104218
2482.868228	605524.293512	39.109236
2485.202533	606638.805819	39.114253
2487.430615	607765.240467	39.119271
2490.202169	608894.827720	39.124288
2492.313719	610046.281392	39.129306
2494.663892	611168.004921	39.134324
2497.388561	612325.130402	39.139341
2499.651012	613484.464440	39.144359
2502.210741	614633.324486	39.149376
2504.402075	615812.389066	39.154394
2506.793959	616971.790128	39.159412
2509.119415	618155.735499	39.164429
2511.690293	619338.763575	39.169447
2514.450531	620522.033377	39.174464
2516.908506	621725.072633	39.179482
2519.440199	622902.573813	39.184500
2521.896718	624101.502423	39.189517
2524.931186	625315.746073	39.194535
2528.030247	626493.514014	39.199552
2530.264985	627696.428375	39.204570
2532.911023	628898.740609	39.209588
2535.914913	630097.811646	39.214605
2538.301180	631304.991331	39.219623
2541.012380	632514.877081	39.224640
2543.364810	633720.638897	39.229658
2545.818243	634931.838679	39.234676
2548.550368	636128.774055	39.239693
2551.306021	637340.095595	39.244711
2554.079432	638550.225561	39.249728
2556.792681	639765.515055	39.254746
2559.080544	640974.594311	39.259764
2561.906840	642182.545291	39.264781
2564.425642	643393.897681	39.269799
2567.063809	644608.679195	39.274816
2569.669472	645832.748954	39.279834
2571.843788	647070.607515	39.284852
2574.482066	648267.647254	39.289869
2576.773889	649520.097735	39.294887
2579.448583	650739.325935	39.299904
2582.154406	651975.050622	39.304922
2584.557528	653197.115700	39.309940
2587.257635	654429.198762	39.314957
2589.505143	655680.438331	39.319975
2592.229196	656919.882423	39.324992
2594.928982	658172.028029	39.330010
2597.506280	659417.509412	39.335028
2600.212686	660677.005884	39.340045
2602.592178	661914.383208	39.345063
2605.173914	663161.030681	39.350080
2608.067267	664422.850628	39.355098
2610.279543	665678.495584	39.360116
2613.041705	666941.402227	39.365133
2615.482958	668201.110438	39.370151
2617.742322	669473.720083	39.375168
2620.530336	670746.073071	39.380186
2622.998392	672030.795024	39.385204
2625.550081	673273.398846	39.390221
2628.413932	674546.473163	39.395239
2630.898299	675782.740057	39.400256
2633.200915	677016.587082	39.405274
2635.664325	678262.872156	39.410292
2638.738666	679496.761676	39.415309
2641.053294	680755.810558	39.420327
2643.904565	681978.771194	39.425344
2646.329424	683240.992021	39.430362
2648.685213	684502.653804	39.435380
2651.655599	685749.685415	39.440397
2654.079592	687012.828241	39.445415
2656.604642	688284.370480	39.450432
2659.296603	689542.748097	39.455450
2661.468230	690838.866335	39.460468
2664.473952	692110.090220	39.465485
2666.687937	693408.065761	39.470503
2669.143520	694691.025772	39.475520
2672.232462	696005.054985	39.480538
2674.349118	697313.792050	39.485556
2677.176934	698636.504382	39.490573
2679.597496	699953.085207	39.495591
2682.080000	701287.707321	39.500608
2684.663108	702609.219577	39.505626
2687.413150	703975.516228	39.510644
2690.284835	705320.216921	39.515661
2693.356905	706698.969733	39.520679
2695.810273	708043.317761	39.525696
2698.569711	709407.965631	39.530714
2701.486200	710764.247995	39.535732
2704.257188	712129.947864	39.540749
2706.762040	713499.236844	39.545767
2709.749450	714875.306159	39.550784
2712.596082	716243.404118	39.555802
2715.080776	717614.310247	39.560820
2717.600960	718994.835326	39.565837
2720.918350	720385.590427	39.570855
2723.669824	721760.971673	39.575872
2726.371044	723169.421532	39.580890
2728.988788	724562.415654	39.585908
2732.163143	725953.996381	39.590925
2734.944898	727332.455504	39.595943
2737.339676	728740.700569	39.600960
2740.428073	730122.447448	39.605978
2742.894932	731532.869586	39.610996
2745.716560	732915.126887	39.616013
2748.692661	734337.971828	39.621031
2751.254516	735721.967121	39.626048
2753.999618	737154.577197	39.631066
2756.742751	738552.770529	39.636084
2759.726088	739956.652914	39.641101
2763.264185	741359.851850	39.646119
2765.578452	742775.439257	39.651136
2769.260913	744164.106687	39.656154
2772.101595	745564.605472	39.661172
2775.007604	746962.033876	39.666189
2777.797397	748356.718423	39.671207
2780.650096	749752.327514	39.676224
2783.143767	751132.121902	39.681242
2785.566856	752525.087525	39.686260
2788.367821	753923.062113	39.691277
2791.179732	755320.634439	39.696295
2793.776977	756724.293187	39.701312
2796.435805	758138.026647	39.706330
2799.039317	759547.323322	39.711348
2802.161657	760954.059190	39.716365
2804.695922	762369.736986	39.721383
2807.163451	763778.616968	39.726400
2809.980269	765206.511776	39.731418
2812.677699	766607.347710	39.736436
2815.607277	768000.064540	39.741453
2817.743774	769400.717000	39.746471
2820.318156	770782.648074	39.751488
2823.410618	772183.406524	39.756506
2825.820385	773575.855149	39.761524
2828.745297	774982.500230	39.766541
2831.365900	776395.018371	39.771559
2833.717840	777809.568474	39.776576
2836.640893	779225.519023	39.781594
2839.366636	780645.695119	39.786612
2842.440611	782083.698481	39.791629
2845.048658	783521.100880	39.796647
2847.933479	784968.132377	39.801664
2850.881384	786402.549689	39.806682
2853.544197	787859.632361	39.811700
2856.444069	789305.150035	39.816717
2859.564918	790782.500030	39.821735
2862.219143	792243.493664	39.826752
2865.182798	793731.627821	39.831770
2867.812340	795204.069955	39.836788
2870.758413	796701.036875	39.841805
2873.538483	798189.826982	39.846823
2876.347452	799681.086598	39.851840
2879.374366	801204.105390	39.856858
2881.951769	802695.785553	39.861876
2884.465813	804220.674052	39.866893
2887.537743	805740.828843	39.871911
2890.170750	807276.616337	39.876928
2893.085760	808808.883997	39.881946
2895.711103	810360.558307	39.886964
2898.919601	811898.048588	39.891981
2901.606400	813468.799352	39.896999
2903.997418	815026.580903	39.902016
2907.276502	816588.643197	39.907034
2910.121837	818172.730540	39.912052
2913.221597	819746.881446	39.917069
2915.758656	821352.138455	39.922087
2919.177985	822934.660115	39.927104
2922.050389	824515.430759	39.932122
2924.684805	826114.591959	39.937140
2927.636893	827706.193424	39.942157
2930.963304	829322.112656	39.947175
2933.575678	830942.331916	39.952192
2936.936174	832533.861684	39.957210
2939.517935	834166.878134	39.962228
2942.389626	835790.522746	39.967245
2945.877881	837401.192881	39.972263
2948.733606	839010.590435	39.977280
2952.167508	840607.663130	39.982298
2954.913294	842249.600014	39.987316
2958.173024	843849.100925	39.992333
2961.007428	845472.437065	39.997351
2963.854017	847078.728108	40.002368
2967.146369	848709.518568	40.007386
2970.288701	850317.364474	40.012404
2973.467980	851943.834139	40.017421
2976.607038	853548.129292	40.022439
2979.413787	855175.079574	40.027456
2982.623236	856775.422021	40.032474
2985.556775	858388.400914	40.037492
2988.218077	859999.643883	40.042509
2991.671879	861614.892644	40.047527
2994.214479	863243.927008	40.052544
2997.240119	864845.009114	40.057562
3000.341965	866449.146344	40.062580
3003.367754	868068.472525	40.067597
3006.668549	869681.409798	40.072615
3009.566215	871290.204145	40.077632
3012.705380	872852.632852	40.082650
3015.794204	874426.083914	40.087668
3018.361828	875969.302616	40.092685
3022.050726	877542.024560	40.097703
3024.582031	879097.883426	40.102720
3027.715505	880645.497467	40.107738
3030.704531	882218.539744	40.112756
3033.657888	883781.984967	40.117773
3036.988609	885333.355854	40.122791
3039.463251	886906.961466	40.127808
3042.592934	888481.771509	40.132826
3045.444931	890069.135895	40.137844
3048.089798	891662.661271	40.142861
3051.111253	893262.244871	40.147879
3053.795661	894882.948975	40.152896
3056.643695	896493.041690	40.157914
3059.303286	898124.884284	40.162932
3062.272207	899770.375116	40.167949
3065.295096	901400.926882	40.172967
3067.946113	903058.135657	40.177984
3071.328514	904713.677016	40.183002
3074.067566	906405.320152	40.188020
3076.964271	908083.722778	40.193037
3079.862246	909770.086084	40.198055
3082.554219	911472.225432	40.203072
3085.550331	913173.503170	40.208090
3088.646077	914899.038344	40.213108
3091.510120	916624.935284	40.218125
3094.856109	918359.527049	40.223143
3097.706138	920129.371283	40.228160
3100.437177	921864.486156	40.233178
3103.773152	923639.731056	40.238196
3106.755057	925403.803259	40.243213
3109.825056	927171.886870	40.248231
3112.571421	928948.070039	40.253248
3115.517046	930739.827466	40.258266
3119.144531	932534.703008	40.263284
3122.276296	934349.070430	40.268301
3125.427283	936138.687317	40.273319
3128.500141	937964.461530	40.278336
3131.947754	939761.986833	40.283354
3134.823033	941594.089897	40.288372
3137.826799	943394.744353	40.293389
3141.013800	945214.816289	40.298407
3144.645740	947031.883609	40.303424
3147.867849	948862.228207	40.308442
3150.794269	950676.123141	40.313460
3153.656109	952520.596154	40.318477
3157.186216	954351.605733	40.323495
3160.365837	956192.851977	40.328512
3163.515099	958087.406378	40.333530
3166.656900	959971.267780	40.338548
3169.420886	961865.036660	40.343565
3172.428544	963771.043399	40.348583
3175.623625	965673.262234	40.353600
3179.263484	967584.935967	40.358618
3181.788167	969485.223049	40.363636
3184.965548	971387.018800	40.368653
3188.486566	973308.909348	40.373671
3191.956428	975215.339054	40.378688
3195.331717	977139.187602	40.383706
3198.370655	979029.890521	40.388724
3201.960849	980956.416106	40.393741
3205.158706	982846.999376	40.398759
3208.012051	984774.403751	40.403776
3211.525023	986680.315251	40.408794
3214.692664	988590.414171	40.413812
3217.620684	990479.679022	40.418829
3220.979742	992353.464849	40.423847
3224.099817	994212.285351	40.428864
3226.971244	996071.412995	40.433882
3230.076176	997917.944139	40.438900
3233.089621	999793.120211	40.443917
3236.515509	1001657.608181	40.448935
3239.758606	1003548.685834	40.453952
3242.900855	1005409.945522	40.458970
3246.349417	1007310.596353	40.463988
3248.969993	1009203.763020	40.469005
3252.291133	1011082.416242	40.474023
3255.231636	1013001.973477	40.479040
3258.561165	1014921.974396	40.484058
3261.753309	1016835.242833	40.489076
3264.485214	1018760.421305	40.494093
3267.779868	1020701.779005	40.499111
3270.761327	1022649.577024	40.504128
3273.981008	1024612.612196	40.509146
3277.315271	1026572.620624	40.514164
3280.267705	1028548.527023	40.519181
3283.922041	1030520.528590	40.524199
3287.027516	1032509.592776	40.529216
3290.562563	1034480.504184	40.534234
3294.227496	1036477.712046	40.539252
3297.348735	1038472.364137	40.544269
3300.408966	1040486.268394	40.549287
3303.537096	1042500.106385	40.554304
3306.795371	1044520.610889	40.559322
3310.015490	1046538.459612	40.564340
3313.153835	1048590.726163	40.569357
3316.635015	1050622.735974	40.574375
3319.526068	1052690.460102	40.579392
3322.862620	1054736.565788	40.584410
3326.287991	1056809.295033	40.589428
3329.461794	1058862.068326	40.594445
3332.810958	1060941.712126	40.599463
3335.628635	1063023.538340	40.604480
3338.965362	1065098.540016	40.609498
3342.519905	1067212.731830	40.614516
3345.091521	1069323.201966	40.619533
3348.700964	1071426.265387	40.624551
3351.816892	1073556.394858	40.629568
3355.188085	1075698.010968	40.634586
3358.738398	1077810.987925	40.639604
3361.594597	1079970.261680	40.644621
3365.351422	1082113.701235	40.649639
3369.113697	1084256.583675	40.654656
3371.876685	1086411.790054	40.659674
3375.617104	1088552.601302	40.664692
3378.684601	1090709.780322	40.669709
3382.483460	1092865.790452	40.674727
3386.466666	1095018.908105	40.679744
3389.658145	1097184.086352	40.684762
3392.881926	1099333.417799	40.689780
3395.915882	1101496.894747	40.694797
3399.375276	1103662.007941	40.699815
3402.627680	1105847.054261	40.704832
3405.491805	1108029.564234	40.709850
3409.313255	1110205.986460	40.714868
3412.556148	1112399.416102	40.719885
3415.963763	1114585.455154	40.724903
3419.071759	1116784.628566	40.729920
3422.160927	1118979.861558	40.734938
3425.921105	1121174.368869	40.739956
3428.795580	1123400.976230	40.744973
3432.160209	1125597.530429	40.749991
3435.672007	1127819.532115	40.755008
3438.875574	1130005.310462	40.760013
3442.377779	1132167.286264	40.765018
3445.334848	1134251.994722	40.770023
3448.946837	1136294.086515	40.775028
3451.849095	1138239.057976	40.780032
3454.950760	1140128.336640	40.785037
3458.485718	1141929.118596	40.790042
3461.291694	1143659.893306	40.795047
3464.258418	1145285.598614	40.800052
3467.669595	1146857.275463	40.805056
3470.071560	1148314.000923	40.810061
3473.120087	1149717.644138	40.815066
3475.059112	1151038.799306	40.820071
3477.774189	1152283.087984	40.825076
3480.295741	1153453.942431	40.830080
3482.359616	1154547.196111	40.835085
3484.649257	1155574.896374	40.840090
3486.251822	1156533.258406	40.845095
3488.642131	1157427.847110	40.850100
3490.389791	1158244.649785	40.855104
3491.734003	1159025.931864	40.860109
3494.025662	1159724.307665	40.865114
3495.364930	1160397.317323	40.870119
3497.072498	1160964.501822	40.875124
3498.835240	1161522.069823	40.880128
3499.881386	1162012.691950	40.885133
3501.592157	1162447.499372	40.890138
3502.521180	1162870.210120	40.895143
3504.103772	1163229.002551	40.900148
3505.300395	1163544.373931	40.905152
3506.316122	1163821.683342	40.910157
3507.158538	1164056.306585	40.915162
3508.149955	1164255.942526	40.920167
3508.859632	1164425.672631	40.925172
3510.160627	1164563.655747	40.930176
3510.999646	1164681.402836	40.935181
3511.853726	1164758.339630	40.940186
3512.628417	1164798.828466	40.945191
3513.203052	1164824.048155	40.950196
3513.843634	1164825.265207	40.955200
3514.536446	1164782.362745	40.960205
3515.589503	1164735.527863	40.965210
3515.672665	1164664.765450	40.970215
3516.572000	1164558.634077	40.975220
3517.208934	1164452.827160	40.980224
3517.653308	1164317.765849	40.985229
3518.112772	1164164.749789	40.990234
3518.456524	1163989.736715	40.995239
3519.209035	1163810.588104	41.000244
3519.556937	1163598.527410	41.005248
3519.786478	1163386.477628	41.010253
3520.419751	1163166.132547	41.015258
3520.672976	1162917.871853	41.020263
3520.977507	1162658.629588	41.025268
3521.241611	1162392.577208	41.030272
3521.473685	1162132.186850	41.035277
3521.864398	1161824.502828	41.040282
3521.892555	1161538.315366	41.045287
3522.245471	1161224.742462	41.050292
3522.886486	1160927.550883	41.055296
3522.982988	1160590.823445	41.060301
3522.889545	1160250.324156	41.065306
3523.109039	1159938.965289	41.070311
3523.436561	1159570.934868	41.075316
3523.729800	1159221.795632	41.080320
3523.802796	1158864.726169	41.085325
3524.195949	1158478.735950	41.090330
3524.161386	1158124.943843	41.095335
3524.452222	1157730.687362	41.100340
3524.401977	1157353.862089	41.105344
3524.406526	1156956.189393	41.110349
3524.792885	1156566.748912	41.115354
3524.615114	1156168.479014	41.120359
3524.831373	1155770.397904	41.125364
3525.283973	1155361.744259	41.130368
3525.178451	1154961.667783	41.135373
3525.292939	1154544.678622	41.140378
3525.727709	1154127.698315	41.145383
3525.660262	1153708.874571	41.150388
3525.436333	1153282.375538	41.155392
3525.410548	1152857.040036	41.160397
3526.158807	1152407.494253	41.165402
3525.842033	1151992.740926	41.170407
3525.903041	1151543.234581	41.175412
3525.948156	1151115.189988	41.180416
3525.541362	1150659.150799	41.185421
3526.139801	1150217.682700	41.190426
3526.032610	1149776.293861	41.195431
3525.976641	1149316.196938	41.200436
3525.989714	1148864.385882	41.205440
3526.039202	1148411.393126	41.210445
3526.245682	1147958.430389	41.215450
3525.999468	1147512.042271	41.220455
3526.290638	1147048.563133	41.225460
3526.537390	1146600.026443	41.230464
3526.366317	1146130.761101	41.235469
3526.505163	1145674.580254	41.240474
3526.307951	1145208.270882	41.245479
3526.442031	1144742.624337	41.250484
3526.496145	1144278.372326	41.255488
3526.263172	1143801.134642	41.260493
3526.589931	1143319.398963	41.265498
3526.388005	1142854.020827	41.270503
3526.440508	1142372.908100	41.275508
3526.782962	1141901.095799	41.280512
3526.488957	1141428.966771	41.285517
3526.433678	1140957.040975	41.290522
3526.311893	1140482.806646	41.295527
3526.355718	1140020.080568	41.300532
3526.700806	1139526.608551	41.305536
3526.472175	1139057.199553	41.310541
3526.479080	1138567.300839	41.315546
3526.375151	1138092.849691	41.320551
3526.466797	1137622.786273	41.325556
3526.503224	1137142.150537	41.330560
3526.351267	1136650.486742	41.335565
3526.639076	1136165.922726	41.340570
3526.480377	1135699.528991	41.345575
3526.645597	1135193.906124	41.350580
3526.599957	1134717.528791	41.355584
3526.150973	1134221.414129	41.360589
3526.594326	1133729.571832	41.365594
3526.311854	1133254.717591	41.370599
3526.141641	1132776.001201	41.375604
3526.565128	1132283.173101	41.380608
3526.624907	1131798.248276	41.385613
3526.528793	1131303.133803	41.390618
3526.381438	1130827.089961	41.395623
3526.260813	1130319.054071	41.400628
3526.610532	1129830.669663	41.405632
3526.166157	1129347.220958	41.410637
3526.763929	1128851.764210	41.415642
3526.148382	1128361.977597	41.420647
3526.010126	1127858.084897	41.425652
3525.926116	1127380.961596	41.430656
3526.194081	1126898.980835	41.435661
3526.072141	1126398.182084	41.440666
3525.874027	1125910.384909	41.445671
3526.174009	1125428.646642	41.450676
3525.986045	1124922.200808	41.455680
3525.785864	1124444.738813	41.460685
3525.761219	1123961.113158	41.465690
3525.758476	1123469.824338	41.470695
3525.822962	1122986.286132	41.475700
3525.977313	1122495.833933	41.480704
3525.969945	1122016.790129	41.485709
3526.010101	1121523.982217	41.490714
3525.656572	1121035.765261	41.495719
3525.552062	1120544.890988	41.500724
3526.099209	1120051.197124	41.505728
3525.757809	1119559.985726	41.510733
3525.713748	1119063.249561	41.515738
3525.450846	1118598.709363	41.520743
3525.272811	1118095.235573	41.525748
3525.598055	1117618.411277	41.530752
3525.044709	1117128.345865	41.535757
3525.505941	1116644.740827	41.540762
3525.544586	1116165.356154	41.545767
3525.143101	1115669.984691	41.550772
3525.500660	1115181.497946	41.555776
3525.495313	1114694.170726	41.560781
3525.328121	1114215.503816	41.565786
3525.179758	1113719.433685	41.570791
3525.377850	1113224.882089	41.575796
3525.461019	1112748.713744	41.580800
3525.190312	1112253.482168	41.585805
3525.338525	1111760.234847	41.590810
3525.419873	1111281.265352	41.595815
3525.245930	1110787.313877	41.600820
3525.189478	1110293.011356	41.605824
3524.807765	1109820.381830	41.610829
3524.726349	1109321.699324	41.615834
3524.582003	1108858.491016	41.620839
3524.949071	1108360.504655	41.625844
3525.003697	1107885.055619	41.630848
3524.611055	1107407.728595	41.635853
3524.991988	1106908.364335	41.640858
3524.900576	1106429.086597	41.645863
3524.373332	1105953.180780	41.650868
3524.769806	1105467.242536	41.655872
3524.557800	1104991.390873	41.660877
3524.839072	1104513.791877	41.665882
3524.512487	1104022.110397	41.670887
3524.581083	1103547.422653	41.675892
3524.407142	1103058.399143	41.680896
3524.438836	1102585.639595	41.685901
3524.609000	1102092.840312	41.690906
3524.291331	1101626.266748	41.695911
3524.324832	1101134.740698	41.700916
3524.485401	1100664.659489	41.705920
3524.255840	1100195.462115	41.710925
3524.254998	1099705.915118	41.715930
3523.979741	1099228.418039	41.720935
3524.260909	1098750.978399	41.725940
3524.297987	1098271.050047	41.730944
3524.286950	1097798.260987	41.735949
3524.484006	1097314.777929	41.740954
3524.321448	1096828.153785	41.745959
3524.257414	1096356.491156	41.750964
3524.203916	1095865.265582	41.755968
3524.108778	1095403.763553	41.760973
3524.242861	1094897.586528	41.765978
3524.169296	1094442.985461	41.770983
3524.004560	1093936.767866	41.775988
3524.067679	1093476.607100	41.780992
3523.808929	1092986.877372	41.785997
3523.877694	1092504.421928	41.791002
3523.917409	1092029.014197	41.796007
3523.718803	1091557.434568	41.801012
3523.892213	1091062.671719	41.806016
3523.673347	1090601.834562	41.811021
3523.904607	1090121.822282	41.816026
3523.520281	1089649.628485	41.821031
3523.644095	1089170.795178	41.826036
3523.644300	1088700.946488	41.831040
3523.359072	1088235.320321	41.836045
3523.712521	1087760.253553	41.841050
3523.161160	1087289.894525	41.846055
3523.540507	1086817.137029	41.851060
3523.622493	1086348.029898	41.856064
3523.478075	1085872.880207	41.861069
3523.569504	1085399.279984	41.866074
3523.565621	1084928.434754	41.871079
3523.278524	1084448.965482	41.876084
3523.709742	1083979.404824	41.881088
3523.170112	1083506.990520	41.886093
3523.281442	1083032.030178	41.891098
3523.064936	1082571.566574	41.896103
3523.181655	1082083.861035	41.901108
3523.137655	1081610.337218	41.906112
3523.025593	1081155.205208	41.911117
3523.196050	1080679.646303	41.916122
3523.037854	1080203.140425	41.921127
3523.034825	1079735.588675	41.926132
3522.961464	1079267.624519	41.931136
3522.691051	1078807.715653	41.936141
3523.019722	1078345.653451	41.941146
3522.892303	1077877.483009	41.946151
3522.686920	1077418.502433	41.951156
3522.958278	1076946.442026	41.956160
3522.830960	1076492.843972	41.961165
3522.758271	1076005.874550	41.966170
3522.523206	1075556.538178	41.971175
3522.646132	1075096.732203	41.976180
3522.805626	1074623.721172	41.981184
3522.438118	1074163.725398	41.986189
3522.461185	1073696.228644	41.991194
3522.271830	1073250.922684	41.996199
3522.022065	1072778.396007	42.001204
3522.391542	1072331.385697	42.006208
3522.212749	1071862.227902	42.011213
3522.311344	1071406.248482	42.016218
3522.051206	1070950.097934	42.021223
3521.980847	1070486.764246	42.026228
3522.442596	1070032.437223	42.031232
3521.967939	1069585.630298	42.036237
3522.104333	1069125.705035	42.041242
3522.089461	1068669.901237	42.046247
3522.124459	1068217.705944	42.051252
3522.221971	1067749.304557	42.056256
3521.960404	1067306.124057	42.061261
3522.095909	1066836.099434	42.066266
3522.020324	1066400.318587	42.071271
3521.675076	1065934.432778	42.076276
3521.926004	1065491.694873	42.081280
3521.488287	1065037.679655	42.086285
3521.721255	1064575.047559	42.091290
3521.779544	1064129.440725	42.096295
3521.770090	1063693.241712	42.101300
3521.524476	1063241.934062	42.106304
3521.611402	1062799.391308	42.111309
3521.649283	1062332.366797	42.116314
3521.744270	1061896.585728	42.121319
3521.476178	1061435.505103	42.126324
3521.221792	1060973.613180	42.131328
3521.454108	1060533.560641	42.136333
3521.307525	1060085.637434	42.141338
3521.224515	1059651.634258	42.146343
3520.899154	1059205.691717	42.151348
3521.156639	1058762.507255	42.156352
3521.064155	1058321.271731	42.161357
3521.280220	1057873.783368	42.166362
3521.255049	1057434.585586	42.171367
3520.970478	1056990.962519	42.176372
3521.452386	1056549.586970	42.181376
3521.071997	1056113.426564	42.186381
3521.014407	1055661.851988	42.191386
3520.683164	1055230.722546	42.196391
3520.834149	1054783.379777	42.201396
3520.992548	1054345.737599	42.206400
3520.883225	1053900.583760	42.211405
3520.778396	1053464.650748	42.216410
3520.883654	1053022.476615	42.221415
3520.801315	1052570.460381	42.226420
3520.829689	1052143.370775	42.231424
3520.482632	1051711.679817	42.236429
3520.895427	1051278.190012	42.241434
3520.578782	1050833.787938	42.246439
3520.377990	1050386.243538	42.251444
3520.424827	1049954.736486	42.256448
3520.453593	1049532.945298	42.261453
3520.616478	1049092.763397	42.266458
3520.592438	1048683.269166	42.271463
3520.202975	1048254.017742	42.276468
3520.490505	1047822.883997	42.281472
3520.253548	1047377.805115	42.286477
3520.246437	1046956.402779	42.291482
3520.087130	1046517.324325	42.296487
3520.444583	1046084.595521	42.301492
3520.048506	1045663.738323	42.306496
3519.806369	1045239.926566	42.311501
3520.001281	1044800.943552	42.316506
3519.960064	1044377.902077	42.321511
3519.564180	1043966.575036	42.326516
3519.823030	1043527.867155	42.331520
3519.706114	1043110.924264	42.336525
3519.666983	1042695.193296	42.341530
3519.328519	1042274.069407	42.346535
3519.380006	1041851.883012	42.351540
3519.695727	1041425.465430	42.356544
3519.505174	1041013.789120	42.361549
3519.497722	1040589.970164	42.366554
3519.616121	1040197.900317	42.371559
3519.370688	1039769.611516	42.376564
3519.282428	1039363.886369	42.381568
3519.318061	1038941.191425	42.386573
3519.237811	1038533.470687	42.391578
3519.046407	1038112.297219	42.396583
3519.405194	1037700.768590	42.401588
3519.483338	1037286.934639	42.406592
3519.026983	1036896.274129	42.411597
3519.329002	1036464.448907	42.416602
3519.223358	1036056.937828	42.421607
3519.377171	1035638.035392	42.426612
3519.263165	1035218.661823	42.431616
3518.779744	1034817.991523	42.436621
3518.742793	1034402.897896	42.441626
3518.861063	1033990.747684	42.446631
3518.676222	1033597.585342	42.451636
3518.778513	1033183.152189	42.456640
3518.855873	1032767.240471	42.461645
3518.870524	1032364.569533	42.466650
3518.666759	1031956.581183	42.471655
3518.630610	1031544.856501	42.476660
3518.755667	1031134.527200	42.481664
3518.138429	1030756.727049	42.486669
3518.572817	1030342.512354	42.491674
3518.503718	1029953.237979	42.496679
3518.518072	1029545.134299	42.501684
3518.787110	1029142.673294	42.506688
3518.470938	1028752.581114	42.511693
3518.287616	1028343.066138	42.516698
3518.539800	1027944.880749	42.521703
3518.282937	1027545.394493	42.526708
3518.323686	1027142.439551	42.531712
3518.239936	1026743.642626	42.536717
3518.263284	1026349.063370	42.541722
3518.269028	1025951.067339	42.546727
3517.900035	1025551.069468	42.551732
3517.756270	1025159.147507	42.556736
3517.999366	1024777.021295	42.561741
3518.015958	1024362.917031	42.566746
3518.117303	1023969.223477	42.571751
3517.779261	1023585.463629	42.576756
3517.904934	1023194.814078	42.581760
3517.870288	1022819.096210	42.586765
3517.977970	1022414.820249	42.591770
3517.623304	1022018.640468	42.596775
3517.704932	1021632.253280	42.601780
3517.736775	1021251.958127	42.606784
3517.449879	1020867.906766	42.611789
3517.375212	1020481.854059	42.616794
3517.497245	1020093.123085	42.621799
3517.269066	1019726.736980	42.626804
3517.714098	1019338.579677	42.631808
3517.519126	1018965.055600	42.636813
3517.296047	1018574.917894	42.641818
3517.097841	1018200.081967	42.646823
3517.046503	1017813.356653	42.651828
3517.157025	1017433.566189	42.656832
3516.947468	1017067.100507	42.661837
3517.222737	1016691.503559	42.666842
3517.371882	1016304.544315	42.671847
3516.851349	1015936.308733	42.676852
3516.810095	1015550.008496	42.681856
3516.365777	1015186.662836	42.686861
3516.699493	1014815.397357	42.691866
3516.692037	1014451.155413	42.696871
3516.898382	1014088.408518	42.701876
3516.846644	1013706.547817	42.706880
3516.650890	1013348.287041	42.711885
3516.883690	1012976.528369	42.716890
3516.618783	1012606.284238	42.721895
3516.219103	1012247.598440	42.726900
3516.400152	1011871.500883	42.731904
3516.197889	1011518.856815	42.736909
3516.183409	1011161.009970	42.741914
3516.395510	1010791.831152	42.746919
3515.713129	1010437.935270	42.751924
3516.148361	1010068.866711	42.756928
3515.902856	1009727.779794	42.761933
3515.977176	1009368.832644	42.766938
3515.727722	1009009.527165	42.771943
3515.771054	1008647.817561	42.776948
3516.060297	1008293.238179	42.781952
3515.726481	1007959.058312	42.786957
3515.868133	1007597.848537	42.791962
3515.706284	1007250.375499	42.796967
3515.866859	1006893.201306	42.801972
3515.814084	1006542.360598	42.806977
3516.019597	1006196.901618	42.811981
3515.733407	1005833.412659	42.816986
3515.890872	1005480.623486	42.821991
3516.011285	1005150.287599	42.826996
3515.820322	1004786.423785	42.832001
3515.697319	1004446.164737	42.837005
3515.856930	1004096.012655	42.842010
3515.743425	1003754.445675	42.847015
3515.500829	1003403.733208	42.852020
3515.530402	1003035.731117	42.857025
3515.381978	1002696.052069	42.862029
3515.294580	1002348.946464	42.867034
3515.496420	1001999.241521	42.872039
3515.523397	1001662.975204	42.877044
3515.545755	1001316.372165	42.882049
3515.281195	1000952.176410	42.887053
3515.533866	1000622.917055	42.892058
3515.063869	1000276.623496	42.897063
3515.223383	999932.833763	42.902068
3516.010493	999584.635753	42.907073
3515.313854	999257.303306	42.912077
3515.862954	998907.350223	42.917082
3515.694565	998560.317803	42.922087
3515.435002	998208.507117	42.927092
3515.534703	997857.881552	42.932097
3515.265300	997514.113131	42.937101
3515.022847	997173.339022	42.942106
3515.064401	996829.380471	42.947111
3514.958126	996496.823314	42.952116
3514.967005	996162.474073	42.957121
3514.927062	995827.528598	42.962125
3514.905741	995487.591095	42.967130
3514.845584	995149.588452	42.972135
3514.753628	994817.904959	42.977140
3514.987699	994481.178319	42.982145
3514.592770	994145.120066	42.987149
3514.846845	993815.367650	42.992154
3514.867765	993475.205249	42.997159
3514.502998	993150.682072	43.002164
3514.398691	992824.635246	43.007169
3514.542613	992499.893640	43.012173
3514.041440	992176.994587	43.017178
3514.352646	991862.718157	43.022183
3514.285525	991532.983713	43.027188
3514.330510	991195.606003	43.032193
3514.178504	990895.393665	43.037197
3514.334080	990562.153270	43.042202
3514.344066	990246.081779	43.047207
3514.142609	989927.589294	43.052212
3514.334829	989598.675316	43.057217
3514.422274	989274.148973	43.062221
3514.199808	988967.213660	43.067226
3514.130825	988628.531947	43.072231
3514.168056	988316.641147	43.077236
3514.266757	987987.161691	43.082241
3514.114954	987681.413758	43.087245
3513.933716	987351.260645	43.092250
3514.105690	987037.326117	43.097255
3513.634442	986726.993310	43.102260
3514.093391	986394.239675	43.107265
3514.137792	986096.669626	43.112269
3513.920174	985771.603582	43.117274
3514.018004	985449.004837	43.122279
3514.122587	985141.028628	43.127284
3514.133452	984813.820493	43.132289
3513.637094	984521.919179	43.137293
3514.007808	984186.805960	43.142298
3513.953785	983868.633777	43.147303
3513.516886	983569.058433	43.152308
3513.562962	983244.097822	43.157313
3513.775913	982952.780561	43.162317
3513.507946	982619.633529	43.167322
3513.846761	982312.247316	43.172327
3513.522560	982020.482661	43.177332
3514.395866	981686.507235	43.182337
3513.840409	981380.487907	43.187341
3513.827554	981063.715457	43.192346
3514.114258	980744.043166	43.197351
3513.549935	980419.413119	43.202356
3513.541398	980120.954005	43.207361
3513.616977	979800.677543	43.212365
3513.142177	979486.922601	43.217370
3513.657282	979184.517703	43.222375
3513.443168	978890.132204	43.227380
3513.612422	978565.276036	43.232385
3513.374412	978270.471682	43.237389
3513.298760	977966.438296	43.242394
3513.433061	977668.707296	43.247399
3513.254123	977357.328039	43.252404
3513.237981	977047.175789	43.257409
3513.083690	976733.119242	43.262413
3513.191463	976436.012795	43.267418
3513.076024	976129.151055	43.272423
3513.037717	975848.658485	43.277428
3513.350039	975528.103862	43.282433
3513.033553	975248.214370	43.287437
3513.095443	974941.162000	43.292442
3513.182429	974635.653718	43.297447
3512.841011	974361.494741	43.302452
3512.849974	974050.589304	43.307457
3512.893832	973761.374440	43.312461
3512.773657	973455.152714	43.317466
3512.823351	973160.037827	43.322471
3513.146951	972883.546658	43.327476
3513.050482	972585.882936	43.332481
3512.805651	972281.477788	43.337485
3512.908505	971972.205188	43.342490
3512.838327	971656.291112	43.347495
3512.634112	971376.683295	43.352500
3512.990509	971072.408525	43.357505
3512.847528	970791.587889	43.362509
3512.708500	970479.926140	43.367514
3512.887418	970195.696003	43.372519
3512.749094	969919.921088	43.377524
3512.797919	969611.411054	43.382529
3513.116853	969330.540770	43.387533
3512.716108	969016.787195	43.392538
3512.823325	968733.279618	43.397543
3512.663345	968434.725834	43.402548
3512.697798	968137.201448	43.407553
3512.088787	967846.327466	43.412557
3512.340232	967561.759274	43.417562
3512.493638	967271.709770	43.422567
3512.627535	966993.889150	43.427572
3512.756786	966687.461125	43.432577
3512.600471	966396.439224	43.437581
3512.156651	966124.743585	43.442586
3512.314169	965839.909809	43.447591
3512.225676	965562.546404	43.452596
3512.515428	965261.794867	43.457601
3512.217995	964991.980659	43.462605
3512.100963	964704.882939	43.467610
3512.513915	964410.728015	43.472615
3512.098381	964147.849290	43.477620
3511.869061	963849.068868	43.482625
3511.959083	963578.536744	43.487629
3512.142827	963297.786035	43.492634
3512.269156	963034.375294	43.497639
3511.948751	962744.763611	43.502644
3512.073387	962444.676114	43.507649
3511.969691	962182.832332	43.512653
3511.646699	961886.023609	43.517658
3511.894486	961622.038270	43.522663
3511.741270	961346.932816	43.527668
3511.654310	961076.410402	43.532673
3511.287295	960805.431286	43.537677
3511.481026	960547.483367	43.542682
3511.773273	960280.880491	43.547687
3511.632318	960006.493366	43.552692
3511.755892	959726.657104	43.557697
3511.676104	959450.174487	43.562701
3511.646362	959182.887568	43.567706
3511.555136	958925.698531	43.572711
3511.187997	958650.009385	43.577716
3511.590531	958372.611200	43.582721
3511.617959	958113.208911	43.587725
3511.242280	957855.038295	43.592730
3511.446304	957570.376529	43.597735
3511.430997	957322.421400	43.602740
3511.388003	957049.054591	43.607745
3511.480332	956793.996476	43.612749
3511.480611	956531.584762	43.617754
3511.045172	956258.343280	43.622759
3510.845832	956019.780607	43.627764
3511.312942	955736.751141	43.632769
3511.213469	955489.447604	43.637773
3510.933869	955234.169600	43.642778
3511.172667	954991.321482	43.647783
3510.971133	954729.597842	43.652788
3511.187351	954474.200086	43.657793
3511.036534	954230.136504	43.662797
3510.766709	953965.611088	43.667802
3510.952265	953724.624478	43.672807
3510.801122	953471.245841	43.677812
3510.879034	953221.356595	43.682817
3511.081733	952974.017720	43.687821
3510.701217	952717.960701	43.692826
3511.103435	952460.326720	43.697831
3510.755023	952238.685621	43.702836
3510.730492	951978.227102	43.707841
3510.440423	951737.512268	43.712845
3510.435330	951491.092920	43.717850
3510.452287	951260.640661	43.722855
3510.246299	951017.772699	43.727860
3510.449109	950783.344351	43.732865
3510.263641	950540.450425	43.737869
3510.376639	950302.473383	43.742874
3510.326022	950071.404547	43.747879
3510.387010	949843.561774	43.752884
3510.288110	949591.801570	43.757889
3510.564172	949366.391353	43.762893
3510.266336	949119.140532	43.767898
3510.157153	948885.251512	43.772903
3510.076455	948655.943295	43.777908
3510.291983	948413.361666	43.782913
3510.260804	948188.812360	43.787917
3510.112728	947947.800905	43.792922
3510.095849	947711.066231	43.797927
3509.912865	947480.764935	43.802932
3510.355003	947254.851993	43.807937
3510.159747	947012.080639	43.812941
3510.025264	946779.249744	43.817946
3510.107818	946550.779027	43.822951
3509.798614	946314.220122	43.827956
3509.958785	946097.307879	43.832961
3509.998530	945866.993851	43.837965
3510.031570	945643.568883	43.842970
3510.048541	945409.501765	43.847975
3509.883390	945184.556666	43.852980
3509.818750	944954.794221	43.857985
3509.636040	944724.082804	43.862989
3509.597046	944499.278882	43.867994
3510.041830	944278.506388	43.872999
3509.540387	944073.597677	43.878004
3509.605776	943832.551241	43.883009
3509.604579	943607.702547	43.888013
3509.380417	943398.600208	43.893018
3509.685729	943161.892276	43.898023
3509.050345	942955.236210	43.903028
3509.293919	942725.420369	43.908033
3509.089444	942520.497464	43.913037
3508.884526	942307.417671	43.918042
3509.145291	942094.060728	43.923047
3509.384019	941891.532834	43.928052
3509.558548	941663.982682	43.933057
3509.130691	941453.205899	43.938061
3509.228421	941231.498562	43.943066
3509.460597	941031.047970	43.948071
3509.405825	940817.403206	43.953076
3509.636616	940590.276553	43.958081
3509.167333	940391.259608	43.963085
3509.218108	940171.049557	43.968090
3509.327184	939947.847352	43.973095
3509.146977	939739.838143	43.978100
3509.400642	939529.063446	43.983105
3509.263446	939305.586709	43.988109
3508.962047	939096.133065	43.993114
3509.260630	938890.217665	43.998119
3509.030554	938688.122769	44.003124
3508.893563	938473.820431	44.008129
3509.160916	938259.634644	44.013133
3508.858299	938056.280132	44.018138
3509.068952	937851.489903	44.023143
3508.816071	937645.040868	44.028148
3508.634316	937437.420515	44.033153
3508.622698	937226.405268	44.038157
3508.815641	937034.061283	44.043162
3508.848086	936830.508273	44.048167
3508.318658	936635.005737	44.053172
3508.549903	936430.732742	44.058177
3508.547949	936239.735572	44.063181
3508.808148	936034.098736	44.068186
3508.743958	935844.537287	44.073191
3508.228276	935624.614137	44.078196
3508.304378	935430.119136	44.083201
3508.393097	935218.143113	44.088205
3508.215081	935036.251340	44.093210
3508.256239	934834.540019	44.098215
3507.878172	934662.460946	44.103220
3508.155584	934453.303484	44.108225
3508.277404	934267.687428	44.113229
3508.245963	934080.169723	44.118234
3508.475631	933884.824507	44.123239
3508.325515	933704.802877	44.128244
3508.373392	933498.142233	44.133249
3508.255959	933311.763888	44.138253
3508.130974	933110.014313	44.143258
3507.784478	932931.631433	44.148263
3507.867493	932742.030741	44.153268
3508.137156	932558.347474	44.158273
3508.026536	932371.454781	44.163277
3507.987745	932190.499030	44.168282
3507.991271	931991.855621	44.173287
3507.554985	931818.733339	44.178292
3508.185307	931631.692628	44.183297
3508.017268	931451.693690	44.188301
3507.997347	931246.397701	44.193306
3507.944765	931079.144569	44.198311
3507.721536	930894.812585	44.203316
3508.007562	930727.204414	44.208321
3507.804192	930534.689892	44.213325
3507.676440	930361.661622	44.218330
3507.766621	930162.839696	44.223335
3507.756660	929981.035463	44.228340
3507.771634	929791.533180	44.233345
3507.468144	929620.912286	44.238349
3507.804592	929440.666320	44.243354
3508.022466	929255.340164	44.248359
3507.720548	929083.644696	44.253364
3507.583443	928901.248038	44.258369
3507.997817	928720.965007	44.263373
3507.759742	928542.129048	44.268378
3507.760457	928358.537775	44.273383
3507.450344	928180.951220	44.278388
3507.543566	927995.505885	44.283393
3507.462868	927823.445198	44.288397
3507.229452	927662.075170	44.293402
3507.480895	927479.181582	44.298407
3507.333840	927319.709806	44.303412
3506.783441	927127.899026	44.308417
3507.254045	926971.295662	44.313421
3507.160841	926816.222858	44.318426
3507.389554	926641.284972	44.323431
3507.116337	926474.501221	44.328436
3507.292257	926303.695781	44.333441
3507.136402	926118.322834	44.338445
3507.217953	925950.887442	44.343450
3507.358616	925783.148603	44.348455
3506.814666	925633.886091	44.353460
3507.054309	925447.944069	44.358465
3506.938284	925304.564786	44.363469
3506.958356	925131.535771	44.368474
3507.293501	924967.971475	44.373479
3506.999780	924798.253689	44.378484
3507.000450	924639.255281	44.383489
3507.160562	924479.648776	44.388493
3506.864947	924317.707745	44.393498
3507.241773	924151.803185	44.398503
3506.953870	923993.218081	44.403508
3507.093253	923823.494525	44.408513
3506.895542	923667.867336	44.413517
3506.923912	923502.866121	44.418522
3507.212002	923338.009522	44.423527
3506.815230	923175.666089	44.428532
3506.909237	922995.244122	44.433537
3506.864235	922849.863624	44.438541
3506.876418	922695.328552	44.443546
3506.872576	922529.436967	44.448551
3506.760372	922361.633560	44.453556
3506.468835	922207.904453	44.458561
3506.821137	922041.554355	44.463565
3506.604859	921894.444208	44.468570
3506.876705	921729.348889	44.473575
3506.652960	921597.149241	44.478580
3507.206640	921414.385381	44.483585
3506.864277	921260.830313	44.488589
3506.851425	921095.185121	44.493594
3506.599892	920937.082088	44.498599
3506.464577	920773.564876	44.503604
3506.567042	920628.389358	44.508609
3506.545136	920467.635824	44.513613
3506.527200	920332.579883	44.518618
3506.523008	920155.449022	44.523623
3506.314118	920005.976091	44.528628
3506.462864	919851.818994	44.533633
3506.602474	919712.485663	44.538637
3506.243774	919554.263833	44.543642
3506.414870	919402.208489	44.548647
3506.214335	919253.483799	44.553652
3506.220111	919116.179256	44.558657
3506.297285	918963.549434	44.563661
3506.307703	918822.481434	44.568666
3506.500587	918666.839197	44.573671
3506.281785	918532.060626	44.578676
3506.129134	918374.541024	44.583681
3506.152549	918233.070461	44.588685
3506.190024	918086.971268	44.593690
3506.499842	917930.710980	44.598695
3506.124046	917779.759936	44.603700
3506.370689	917622.441833	44.608705
3506.116073	917494.192883	44.613709
3506.011424	917342.414587	44.618714
3506.424752	917201.623680	44.623719
3506.147638	917059.401706	44.628724
3506.201347	916911.919948	44.633729
3506.270124	916755.665834	44.638733
3506.038742	916616.411017	44.643738
3506.275002	916464.359586	44.648743
3506.253667	916340.669230	44.653748
3505.606678	916181.144877	44.658753
3506.099216	916048.500119	44.663757
3505.690358	915912.339573	44.668762
3505.619555	915762.246139	44.673767
3505.576055	915637.483780	44.678772
3505.795374	915503.907393	44.683777
3505.967528	915374.767768	44.688781
3505.825391	915234.017883	44.693786
3505.947077	915094.377235	44.698791
3505.936434	914945.986043	44.703796
3505.991410	914818.490786	44.708801
3505.590048	914675.552962	44.713805
3505.426583	914553.387625	44.718810
3505.850653	914388.141849	44.723815
3505.627622	914280.050294	44.728820
3505.982393	914134.468205	44.733825
3505.876322	913999.559659	44.738829
3505.926768	913863.561859	44.743834
3505.782507	913717.858204	44.748839
3505.739376	913596.133731	44.753844
3505.800034	913452.509764	44.758849
3505.597367	913318.467943	44.763853
3505.426796	913192.032484	44.768858
3505.614256	913047.220392	44.773863
3505.419318	912935.145700	44.778868
3505.716151	912803.129798	44.783873
3505.545615	912660.294487	44.788877
3505.492550	912544.139675	44.793882
3505.728645	912405.086889	44.798887
3505.381090	912277.406381	44.803892
3505.624637	912155.506529	44.808897
3505.497899	912018.239145	44.813901
3505.131534	911885.057210	44.818906
3505.585497	911742.191737	44.823911
3505.206994	911634.266809	44.828916
3505.109926	911507.298612	44.833921
3505.263348	911366.979897	44.838925
3505.101123	911254.383636	44.843930
3505.250916	911115.312670	44.848935
3505.017903	911013.523024	44.853940
3505.142250	910879.657507	44.858945
3504.943238	910763.296501	44.863949
3505.214090	910645.794873	44.868954
3505.039825	910528.556947	44.873959
3505.080026	910409.063109	44.878964
3505.060967	910278.003445	44.883969
3505.417764	910162.695601	44.888973
3504.853270	910055.735003	44.893978
3505.373809	909917.923207	44.898983
3505.120005	909815.922116	44.903988
3504.975197	909670.401323	44.908993
3504.798252	909567.032669	44.913997
3504.823756	909446.266636	44.919002
3505.137984	909319.277084	44.924007
3505.136872	909211.049924	44.929012
3504.857140	909080.004943	44.934017
3505.035560	908981.582932	44.939021
3505.004804	908852.227937	44.944026
3505.180258	908740.972089	44.949031
3504.894336	908629.114717	44.954036
3505.066463	908513.417228	44.959041
3505.148280	908388.084755	44.964045
3504.926518	908277.753353	44.969050
3505.280520	908139.539063	44.974055
3504.797363	908021.816763	44.979060
3505.074424	907920.079404	44.984065
3504.960787	907797.949789	44.989069
3504.908135	907687.385879	44.994074
3505.099709	907560.858897	44.999079
3504.670881	907465.115335	45.004084
3505.165763	907327.919139	45.009089
3505.355268	907231.008294	45.014093
3505.107812	907105.990739	45.019098
3505.052555	906973.218803	45.024103
3504.755491	906860.266294	45.029108
3504.785711	906742.818454	45.034113
3504.721639	906630.594951	45.039117
3504.596131	906512.395880	45.044122
3504.507711	906407.313425	45.049127
3504.328577	906303.016023	45.054132
3504.776301	906187.900531	45.059137
3504.724415	906084.350197	45.064141
3504.228933	905969.289049	45.069146
3504.742888	905853.866235	45.074151
3504.456586	905769.073223	45.079156
3504.325307	905648.829944	45.084161
3504.360573	905555.776363	45.089165
3504.272344	905455.309136	45.094170
3504.365403	905339.752012	45.099175
3504.226494	905262.456175	45.104180
3504.043163	905137.384062	45.109185
3504.386867	905038.961907	45.114189
3504.403575	904933.158751	45.119194
3504.674422	904817.947733	45.124199
3504.794745	904716.660633	45.129204
3504.249762	904612.198935	45.134209
3504.482865	904519.192113	45.139213
3504.274489	904408.202897	45.144218
3504.653541	904290.549654	45.149223
3504.421432	904188.055980	45.154228
3504.501103	904100.956877	45.159233
3504.614675	903982.761628	45.164237
3504.378016	903888.470034	45.169242
3504.561809	903767.844895	45.174247
3504.509650	903664.056817	45.179252
3504.709800	903569.977604	45.184257
3504.703872	903462.509000	45.189261
3504.351640	903354.033207	45.194266
3504.434156	903251.180946	45.199271
3504.322128	903146.234419	45.204276
3504.437236	903037.482419	45.209281
3504.541095	902934.331154	45.214285
3504.264010	902833.944716	45.219290
3504.356343	902717.850948	45.224295
3504.189895	902637.819513	45.229300
3504.557062	902520.517529	45.234305
3504.627999	902421.804788	45.239309
3504.506481	902309.987248	45.244314
3504.516612	902199.111618	45.249319
3504.362758	902094.442134	45.254324
3504.207399	901988.129014	45.259329
3504.299019	901881.290277	45.264333
3503.937953	901793.069036	45.269338
3504.410456	901700.555762	45.274343
3504.558873	901580.565762	45.279348
3504.268455	901504.305740	45.284353
3504.044838	901397.123393	45.289357
3504.297088	901297.008788	45.294362
3504.376102	901206.001182	45.299367
3504.012019	901098.160111	45.304372
3503.944904	901005.917551	45.309377
3504.167466	900905.994116	45.314381
3503.993279	900809.901860	45.319386
3504.098846	900717.239729	45.324391
3503.979058	900611.957521	45.329396
3503.965737	900518.635461	45.334401
3504.193582	900415.610980	45.339405
3503.815163	900325.244216	45.344410
3503.930060	900222.041591	45.349415
3503.828385	900151.432508	45.354420
3503.980202	900062.906545	45.359425
3504.147953	899962.009302	45.364429
3503.719617	899866.522604	45.369434
3504.038953	899764.147555	45.374439
3504.047406	899676.412152	45.379444
3503.760257	899588.337576	45.384449
3503.814714	899489.093214	45.389453
3503.948684	899410.609256	45.394458
3503.758983	899312.851458	45.399463
3503.618810	899247.938655	45.404468
3503.761304	899136.594665	45.409473
3504.002224	899057.894946	45.414477
3503.722627	898964.591154	45.419482
3504.022115	898859.593874	45.424487
3503.931119	898761.037206	45.429492
3503.736116	898687.332786	45.434497
3503.731370	898594.750773	45.439501
3503.638784	898505.467624	45.444506
3504.092215	898412.420600	45.449511
3503.499727	898317.514730	45.454516
3503.565087	898241.635397	45.459521
3503.785755	898158.963968	45.464525
3503.575339	898084.094457	45.469530
3503.849899	897977.635223	45.474535
3503.315403	897905.039756	45.479540
3503.810534	897805.693400	45.484545
3503.717434	897724.710495	45.489549
3503.847472	897630.930700	45.494554
3503.777456	897544.721839	45.499559
3503.558704	897459.599452	45.504564
3503.479605	897357.729989	45.509569
3503.290338	897277.626536	45.514573
3503.330564	897197.000824	45.519578
3503.780848	897114.276407	45.524583
3503.548871	897040.363392	45.529588
3503.669846	896952.470733	45.534593
3503.701803	896870.971736	45.539597
3503.417951	896785.753328	45.544602
3503.621169	896709.250827	45.549607
3503.425550	896607.387142	45.554612
3503.514046	896530.127723	45.559617
3503.542309	896438.858697	45.564621
3503.206638	896370.368110	45.569626
3503.443470	896283.799592	45.574631
3503.202371	896200.499032	45.579636
3503.683318	896128.197066	45.584641
3503.675573	896044.082312	45.589645
3503.465092	895964.737393	45.594650
3503.706460	895871.297070	45.599655
3502.860699	895791.377555	45.604660
3502.985270	895712.747469	45.609665
3502.991905	895633.652263	45.614669
3503.123897	895570.586543	45.619674
3503.223759	895494.084788	45.624679
3503.173813	895410.161041	45.629684
3503.104155	895350.220400	45.634689
3503.334614	895259.576110	45.639693
3503.063932	895191.350769	45.644698
3503.497816	895109.276924	45.649703
3503.394174	895040.345357	45.654708
3503.460991	894955.718789	45.659713
3503.484739	894878.157586	45.664717
3503.489440	894805.917353	45.669722
3503.867109	894716.497408	45.674727
3503.186282	894642.337145	45.679732
3503.415566	894552.165396	45.684737
3503.455620	894480.302078	45.689741
3503.340954	894404.207939	45.694746
3503.585994	894314.029848	45.699751
3503.285001	894250.537326	45.704756
3503.218661	894168.242245	45.709761
3503.474039	894080.380001	45.714765
3503.524314	893995.645254	45.719770
3503.191787	893924.029768	45.724775
3503.215555	893840.554479	45.729780
3503.415020	893775.620138	45.734785
3503.545131	893696.768007	45.739789
3503.397755	893615.639050	45.744794
3503.675555	893534.342186	45.749799
3503.576547	893449.237043	45.754804
3503.254537	893380.321468	45.759809
3503.522275	893288.769290	45.764813
3503.390503	893179.095421	45.769818
3503.220809	893042.532968	45.774823
3503.307081	892852.911898	45.779828
3503.254654	892609.614764	45.784833
3503.427245	892281.034594	45.789837
3502.751575	891912.034880	45.794842
3502.936792	891462.653526	45.799847
3502.838173	890966.349855	45.804852
3502.737828	890405.644764	45.809857
3503.272390	889767.928577	45.814861
3502.861361	889069.892843	45.819866
3502.943371	888300.241806	45.824871
3502.559435	887456.877987	45.829876
3502.386639	886548.277162	45.834881
3502.413269	885559.494260	45.839885
3502.184513	884511.102167	45.844890
3501.958121	883372.503885	45.849895
3501.936535	882155.050295	45.854900
3501.658097	880866.814980	45.859905
3501.564899	879477.718059	45.864909
3501.364266	878040.885927	45.869914
3500.961195	876496.929966	45.874919
3500.820401	874885.767838	45.879924
3500.656260	873167.790987	45.884929
3500.576754	871380.758113	45.889933
3500.314590	869502.411993	45.894938
3500.326801	867534.925860	45.899943
3499.977036	865468.989940	45.904948
3499.543930	863327.988919	45.909953
3499.275985	861106.748676	45.914957
3499.130563	858778.339096	45.919962
3498.792344	856360.604221	45.924967
3498.477517	853856.134895	45.929972
3498.260962	851266.864982	45.934977
3497.475779	848577.211967	45.939981
3497.127240	845820.914763	45.944986
3496.948434	842944.435589	45.949991
3496.913308	840007.835231	45.954996
3496.038357	836966.046190	45.960001
3495.668343	833856.753737	45.965005
3495.271047	830642.088824	45.970010
3495.012034	827336.595053	45.975015
3494.431379	823930.831585	45.980020
3493.879862	820461.695333	45.985025
3493.362413	816896.881004	45.990029
3492.790030	813240.185247	45.995034
3492.340280	809503.308689	46.000039
3491.519771	805680.185340	46.005044
3490.892999	801776.681874	46.010049
3490.961166	797772.614829	46.015053
3490.230301	793696.574759	46.020058
3489.806724	789531.168991	46.025063
3488.970640	785252.968733	46.030068
3488.467608	780917.932031	46.035073
3488.274937	776450.292232	46.040077
3487.335726	771931.270819	46.045082
3486.486893	767297.647940	46.050087
3486.080359	762597.833894	46.055092
3485.050792	757794.539808	46.060097
3484.625853	752931.667866	46.065101
3483.547451	747980.430527	46.070106
3483.220244	742912.518195	46.075111
3482.174914	737789.564275	46.080116
3481.138767	732562.994817	46.085121
3480.729450	727251.632803	46.090125
3479.759851	721857.539146	46.095130
3478.902787	716360.391215	46.100135
3478.234648	710773.482739	46.105140
3477.373638	705092.479854	46.110145
3476.581041	699357.635147	46.115149
3475.602094	693507.741485	46.120154
3474.879530	687586.423421	46.125159
3473.796744	681575.718479	46.130164
3472.697411	675457.660672	46.135169
3471.910518	669286.129695	46.140173
3470.827941	663001.636597	46.145178
3469.817804	656641.885682	46.150183
3469.081449	650194.126097	46.155188
3467.834314	643649.090991	46.160193
3466.688460	637024.639467	46.165197
3465.331672	630320.603424	46.170202
3464.387795	623533.306237	46.175207
3463.460517	616647.601061	46.180212
3461.941278	609686.876166	46.185217
3461.385190	602640.236676	46.190221
3459.846821	595509.499626	46.195226
3458.512149	588303.564632	46.200231
3457.513337	580992.602494	46.205236
3456.434056	573613.137506	46.210241
3455.031375	566134.935782	46.215245
3453.273251	558586.360340	46.220250
3452.373695	550945.227531	46.225255
3451.158310	543236.057043	46.230260
3449.522477	535428.394294	46.235265
3448.185745	527522.087010	46.240269
3446.739488	519561.380465	46.245274
3445.103268	511484.721189	46.250279
3443.715891	503359.762017	46.255284
3442.045619	495142.185656	46.260289
3440.489075	486844.388425	46.265293
3438.914066	478487.797385	46.270298
3437.516218	470020.467971	46.275303
3435.994995	461486.859044	46.280308
3433.664788	452889.337254	46.285313
3432.304541	444195.530053	46.290317
3430.732740	435437.908010	46.295322
3429.052106	426605.432598	46.300327
3427.205923	417693.024110	46.305332
3425.174106	408684.497463	46.310337
3423.481426	399624.927677	46.315341
3421.037500	390486.470323	46.320346
3419.030060	381273.142072	46.325351
3417.050660	372002.815519	46.330356
3414.698678	362663.016740	46.335361
3412.515089	353259.125038	46.340365
3410.528518	343806.134015	46.345370
3408.149374	334269.043198	46.350375
3406.234122	324677.407950	46.355380
3403.370316	315028.112831	46.360385
3401.293325	305309.534008	46.365389
3398.738099	295528.854428	46.370394
3396.028118	285706.732958	46.375399
3393.488156	275825.257150	46.380404
3390.846911	265892.110550	46.385409
3388.073638	255920.650329	46.390413
3384.849947	245886.977226	46.395418
3382.075587	235818.112509	46.400423
3379.065724	225721.401127	46.405428
3375.790846	215487.747907	46.410433
3373.214428	205284.369505	46.415437
3369.403763	195065.060253	46.420442
3365.908350	184808.316091	46.425447
3362.308416	174538.651219	46.430452
3358.534987	164252.395788	46.435457
3354.780997	153938.353396	46.440461
3350.524030	143611.992573	46.445466
3346.597064	133291.480168	46.450471
3341.909538	122962.437505	46.455476
3336.650631	112641.118213	46.460481
3331.572787	102341.095660	46.465485
3325.646272	92076.378887	46.470490
3318.912476	81861.052850	46.475495
3310.985283	71726.801552	46.480500
3299.577214	61727.502520	46.485505
3270.955130	52360.972530	46.490509
3226.549908	43731.251548	46.495514
3179.403898	35733.025005	46.500519
3131.459457	28538.341649	46.505524
3086.698413	22186.912901	46.510529
3046.554724	16732.958218	46.515533
3010.874600	12129.943621	46.520538
2980.099726	8379.720701	46.525543
2955.183784	5389.100715	46.530548
2933.776542	3091.774292	46.535553
2915.752303	1406.970147	46.540557
2894.866915	421.496104	46.545562
2862.255820	336.777601	46.550567
2850.136479	336.277930	46.555572
2856.366991	331.200828	46.560577
2872.210763	332.310545	46.565581
2888.233008	337.278148	46.570586
2895.380982	472.741189	46.575591
2897.209335	629.074464	46.580596
2897.899805	725.922390	46.585601
2898.701484	794.662013	46.590605
2898.815735	834.033278	46.595610
2898.721985	809.806728	46.600615
2898.181961	767.786642	46.605620
2897.599993	702.556399	46.610625
2897.147856	606.670416	46.615629
2895.710579	482.761923	46.620634
2893.711794	362.146601	46.625639
2888.306253	281.099254	46.630644
2879.977224	295.467139	46.635649
2874.419387	290.770553	46.640653
2870.739025	305.321536	46.645658
2868.175266	295.291824	46.650663
2865.453999	304.323484	46.655668
2862.995546	288.364923	46.660673
2860.834448	293.349691	46.665677
2857.885614	296.608292	46.670682
2854.871534	288.490409	46.675687
2851.567215	300.445540	46.680692
2848.431132	293.934185	46.685697
2845.148161	293.041080	46.690701
2841.269040	301.282336	46.695706
2838.269867	300.046987	46.700711
2835.312595	290.785649	46.705716
2832.138325	296.241496	46.710721
2828.951077	286.358493	46.715725
2825.605585	288.439390	46.720730
2822.185097	287.134012	46.725735
2818.868702	277.466063	46.730740
2815.633758	284.959397	46.735745
2812.530963	279.895909	46.740749
2809.115746	292.555745	46.745754
2805.372884	277.983909	46.750759
2802.000802	284.918701	46.755764
2798.800726	288.730840	46.760769
2795.212985	278.802508	46.765773
2791.936492	287.654125	46.770778
2788.792001	278.464722	46.775783
2785.463215	279.672479	46.780788
2781.942451	267.533196	46.785793
2778.880115	275.224683	46.790797
2775.356740	281.514485	46.795802
2772.179515	266.799313	46.800807
2768.367764	272.772141	46.805812
2764.679619	277.979185	46.810817
2761.477249	266.398074	46.815821
2758.057845	273.455904	46.820826
2754.673368	272.499272	46.825831
2751.596900	272.546443	46.830836
2747.569186	268.002263	46.835841
2744.195978	260.317052	46.840845
2740.926780	267.708520	46.845850
2737.325277	261.923682	46.850855
2734.285234	263.373198	46.855860
2730.936148	265.273501	46.860865
2727.817650	261.071801	46.865869
2724.079909	264.841894	46.870874
2720.390963	253.068860	46.875879
2716.691097	254.701650	46.880884
2712.778425	272.240424	46.885889
2709.985980	245.529716	46.890893
2706.713673	261.272417	46.895898
2703.379048	254.812824	46.900903
2700.226944	257.082763	46.905908
2695.903878	259.212324	46.910913
2692.709738	251.021432	46.915917
2688.928208	261.470531	46.920922
2686.310329	260.184908	46.925927
2682.769392	253.289959	46.930932
2678.407472	264.897130	46.935937
2674.980612	250.108555	46.940941
2671.662942	252.067035	46.945946
2668.229498	255.876456	46.950951
2665.193462	254.373995	46.955956
2661.774628	258.781105	46.960961
2658.958974	248.407421	46.965965
2654.998353	256.964731	46.970970
2651.403160	262.564316	46.975975
2648.119612	251.250787	46.980980
2644.251726	264.382850	46.985985
2640.697713	253.977411	46.990989
2637.084539	254.450211	46.995994
2634.031024	260.869755	47.000999
2631.165776	252.918446	47.006004
2627.031220	269.196470	47.011009
2623.757098	243.423506	47.016013
2619.807970	264.385974	47.021018
2616.298584	252.114212	47.026023
2613.416565	255.698963	47.031028
2609.367532	257.031173	47.036033
2606.247251	249.443728	47.041037
2602.753871	251.748272	47.046042
2598.871726	256.560899	47.051047
2595.611116	247.226505	47.056052
2592.098497	252.045780	47.061057
2588.642063	253.268746	47.066061
2585.487052	254.367827	47.071066
2581.579233	254.327813	47.076071
2578.533676	248.084512	47.081076
2574.471703	263.005574	47.086081
2571.299919	239.428126	47.091085
2567.762600	250.880031	47.096090
2564.280501	243.808136	47.101095
2561.175608	245.815231	47.106100
2557.438217	242.625717	47.111105
2554.167247	239.521281	47.116109
2550.239500	248.994905	47.121114
2546.998096	240.528658	47.126119
2543.588546	232.123587	47.131124
2539.897018	240.083924	47.136129
2537.013573	247.577085	47.141133
2532.775787	245.196757	47.146138
2529.196050	245.454460	47.151143
2525.873596	239.844509	47.156148
2522.543500	246.792094	47.161153
2519.378442	232.095416	47.166157
2515.217593	259.844477	47.171162
2511.586613	255.382399	47.176167
2508.661586	246.826709	47.181172
2505.269966	249.834468	47.186177
2501.886459	251.099507	47.191181
2498.019611	234.383365	47.196186
2494.756558	239.962566	47.201191
2491.196044	239.985682	47.206196
2487.631242	240.608022	47.211201
2483.945620	236.722908	47.216205
2480.701901	237.612524	47.221210
2477.402819	231.434365	47.226215
2473.639767	237.031605	47.231220
2470.008004	253.199036	47.236225
2466.371916	235.736844	47.241229
2463.642021	239.386625	47.246234
2459.585574	233.995017	47.251239
2456.190495	235.625214	47.256244
2452.281918	240.267650	47.261249
2449.498982	247.102441	47.266253
2445.758750	235.253402	47.271258
2442.109130	237.540865	47.276263
2438.965582	219.359613	47.281268
2435.493628	238.907287	47.286273
2431.866216	220.488866	47.291277
2428.482660	230.291954	47.296282
2424.685273	224.791849	47.301287
2421.727033	220.047731	47.306292
2417.783492	216.018051	47.311297
2414.429725	227.581680	47.316301
2410.839795	219.190551	47.321306
2407.123329	222.973842	47.326311
2404.090163	225.370181	47.331316
2400.349701	222.683392	47.336321
2396.818021	216.706510	47.341325
2392.904692	228.132767	47.346330
2389.578671	222.469023	47.351335
2386.337679	233.905749	47.356340
2382.993585	224.037837	47.361345
2379.732444	225.664328	47.366349
2375.930729	219.857176	47.371354
2372.269452	220.131557	47.376359
2369.158070	209.178012	47.381364
2365.234805	226.801361	47.386369
2361.809116	217.422023	47.391373
2358.519827	218.664383	47.396378
2354.903602	224.260737	47.401383
2351.802994	232.331253	47.406388
2347.911071	230.067128	47.411393
2344.610996	224.607576	47.416397
2341.031769	227.527762	47.421402
2337.438506	223.627497	47.426407
2334.196011	221.115405	47.431412
2330.129856	222.405300	47.436417
2326.843131	219.302783	47.441421
2323.372510	206.403145	47.446426
2319.553875	221.797606	47.451431
2316.704881	221.925916	47.456436
2312.907555	224.595898	47.461441
2309.645531	215.784164	47.466445
2305.939396	227.416891	47.471450
2302.394951	222.317981	47.476455
2298.974468	214.636384	47.481460
2295.412981	243.819451	47.486465
2292.256685	217.400508	47.491469
2288.684434	229.071240	47.496474
2284.869750	220.752468	47.501479
2281.317659	230.593859	47.506484
2277.873009	219.215188	47.511489
2274.638908	221.733403	47.516493
2271.040272	223.842757	47.521498
2267.710503	221.931763	47.526503
2264.284639	230.483896	47.531508
2260.861057	225.227850	47.536513
2257.262342	207.128207	47.541517
2252.947518	211.044286	47.546522
2249.545461	217.371577	47.551527
2247.066726	218.704727	47.556532
2243.132607	219.853721	47.561537
2239.470999	214.414887	47.566541
2235.563001	224.073595	47.571546
2232.492378	215.910824	47.576551
2229.134267	219.764222	47.581556
2225.355867	223.632587	47.586561
2221.839634	207.234597	47.591565
2218.707207	222.059656	47.596570
2214.993873	214.602201	47.601575
2211.812227	217.881556	47.606580
2207.897640	225.523768	47.611585
2204.557594	202.591337	47.616589
2201.016683	204.504850	47.621594
2197.220541	212.072477	47.626599
2193.987184	199.051810	47.631604
2190.240502	219.067354	47.636609
2187.162012	211.080812	47.641613
2183.720914	208.919598	47.646618
2180.056604	212.973665	47.651623
2176.766036	202.589399	47.656628
2173.090345	213.734350	47.661633
2169.427735	202.254484	47.666637
2166.077177	219.275280	47.671642
2162.494418	211.485078	47.676647
2158.857155	202.378113	47.681652
2155.610965	216.524294	47.686657
2151.969067	201.048253	47.691661
2148.276534	218.539002	47.696666
2145.051574	213.661335	47.701671
2141.862025	197.778241	47.706676
2138.157199	209.677847	47.711681
2134.618007	196.403722	47.716685
2131.113195	211.489293	47.721690
2127.399857	203.109812	47.726695
2124.004971	200.479717	47.731700
2120.354996	210.555122	47.736705
2117.249158	195.584167	47.741709
2113.573912	205.150660	47.746714
2109.643334	204.448857	47.751719
2106.394032	196.847653	47.756724
2102.994035	206.706723	47.761729
2099.635499	196.230528	47.766733
2096.138930	208.837251	47.771738
2092.725353	205.010076	47.776743
2089.253075	200.503517	47.781748
2085.301794	222.600227	47.786753
2082.013350	191.224403	47.791757
2078.665581	205.615135	47.796762
2074.912576	191.981917	47.801767
2071.538930	206.299578	47.806772
2067.728926	201.350852	47.811777
2064.778032	196.536437	47.816781
2061.219118	205.992708	47.821786
2057.865758	195.812225	47.826791
2053.962421	197.588980	47.831796
2050.506392	202.110973	47.836801
2047.210553	200.061015	47.841805
2043.304748	195.685086	47.846810
2040.013020	209.476168	47.851815
2036.527999	192.687149	47.856820
2032.660486	200.183354	47.861825
2029.370018	202.280554	47.866829
2026.318203	191.660582	47.871834
2022.791402	204.479577	47.876839
2019.401363	202.887617	47.881844
2015.748258	200.623447	47.886849
2012.277385	197.779936	47.891853
2008.595080	208.636499	47.896858
2004.707313	198.977768	47.901863
2001.385074	196.798517	47.906868
1998.159616	197.533403	47.911873
1994.718741	198.047435	47.916877
1990.876503	206.683338	47.921882
1987.215171	204.393708	47.926887
1983.708550	200.125979	47.931892
1980.274648	203.375023	47.936897
1976.901000	199.102921	47.941901
1973.769719	196.724279	47.946906
1970.415521	201.846660	47.951911
1966.653725	192.355599	47.956916
1962.874565	197.325534	47.961921
1959.574298	197.950156	47.966925
1956.124421	189.904065	47.971930
1952.359957	197.020569	47.976935
1949.250499	185.364168	47.981940
1945.315727	205.444040	47.986945
1941.710949	200.386556	47.991949
1938.190999	200.561775	47.996954
1934.879075	184.232790	48.001959
1931.899307	201.304625	48.006964
1928.009076	185.934728	48.011969
1924.666321	180.266008	48.016973
1921.198137	203.285323	48.021978
1917.326873	190.959102	48.026983
1914.249075	188.395575	48.031988
1910.240958	205.031955	48.036993
1907.025180	198.793301	48.041997
1903.798387	193.125383	48.047002
1899.699982	201.035103	48.052007
1896.440653	197.138190	48.057012
1892.894204	207.613397	48.062017
1889.338812	195.337476	48.067021
1885.996402	203.718226	48.072026
1882.592680	214.886289	48.077031
1879.396835	200.932108	48.082036
1875.546070	210.244136	48.087041
1871.772141	198.019077	48.092045
1868.051007	196.920511	48.097050
1865.022186	198.412112	48.102055
1861.599725	194.643543	48.107060
1857.907908	204.357492	48.112065
1854.589933	195.661985	48.117069
1851.163495	212.592487	48.122074
1847.446997	201.482475	48.127079
1844.084511	201.515749	48.132084
1840.336192	197.695002	48.137089
1836.820028	193.075958	48.142093
1833.614256	208.897140	48.147098
1829.809114	204.286511	48.152103
1826.696712	184.404358	48.157108
1823.114146	203.238513	48.162113
1819.401631	194.241242	48.167117
1815.837908	189.747549	48.172122
1812.415034	197.739996	48.177127
1808.855051	206.948140	48.182132
1805.328103	202.817233	48.187137
1801.987489	195.751337	48.192141
1798.497329	199.283001	48.197146
1794.810966	199.087399	48.202151
1791.820268	197.035950	48.207156
1787.932732	194.193429	48.212161
1784.307605	186.095953	48.217165
1781.254292	200.087783	48.222170
1777.269658	193.355943	48.227175
1773.957776	203.503840	48.232180
1770.342929	195.934124	48.237185
1766.782501	203.634496	48.242189
1763.524039	171.232696	48.247194
1759.897669	189.822330	48.252199
1756.522702	186.356135	48.257204
1752.696210	194.715095	48.262209
1749.366258	190.557340	48.267213
1746.025415	181.109425	48.272218
1742.390589	193.048228	48.277223
1739.052468	182.342774	48.282228
1735.147852	185.219749	48.287233
1731.810909	181.589257	48.292237
1728.287723	187.994243	48.297242
1724.625785	180.271729	48.302247
1721.483815	191.251827	48.307252
1718.057906	191.388257	48.312257
1714.570424	187.898227	48.317261
1711.144204	188.304519	48.322266
1707.645350	187.636565	48.327271
1703.884011	176.767469	48.332276
1700.050365	188.876901	48.337281
1697.041520	181.090737	48.342285
1693.337939	188.418774	48.347290
1689.599018	188.914851	48.352295
1686.253124	195.986083	48.357300
1682.939962	191.390841	48.362305
1679.343368	192.344058	48.367309
1675.925446	186.284590	48.372314
1672.403279	187.572775	48.377319
1668.955965	189.517159	48.382324
1665.264454	187.154059	48.387329
1661.645023	196.938314	48.392333
1658.402735	198.686692	48.397338
1654.665252	190.819138	48.402343
1651.565794	197.941067	48.407348
1647.672061	199.140729	48.412353
1644.326487	191.449709	48.417357
1640.847333	191.775885	48.422362
1637.151737	201.121399	48.427367
1633.853458	179.559368	48.432372
1630.488533	200.543635	48.437377
1626.955641	186.743787	48.442381
1623.435343	197.237759	48.447386
1619.679672	205.424398	48.452391
1616.629376	188.842017	48.457396
1612.830788	198.581868	48.462401
1609.151407	184.739619	48.467405
1605.717746	193.725943	48.472410
1602.218182	187.785641	48.477415
1598.633153	186.945811	48.482420
1595.089679	188.804982	48.487425
1591.584318	173.279094	48.492429
1588.367558	189.982682	48.497434
1584.561368	188.410778	48.502439
1581.793095	186.118021	48.507444
1577.772391	184.602336	48.512449
1574.318175	182.359544	48.517453
1571.087997	179.257640	48.522458
1567.445460	174.635827	48.527463
1564.090054	169.349584	48.532468
1560.111325	182.305057	48.537473
1556.695790	176.330004	48.542477
1553.054982	177.087461	48.547482
1549.581118	181.833385	48.552487
1546.475907	181.131528	48.557492
1542.669481	182.874009	48.562497
1539.439371	181.848678	48.567501
1535.800788	184.858040	48.572506
1532.107408	183.657805	48.577511
1528.657160	187.522356	48.582516
1525.071538	190.214507	48.587521
1521.674449	194.546471	48.592525
1518.574463	181.043612	48.597530
1514.511212	191.348443	48.602535
1511.459960	173.141744	48.607540
1507.900812	180.991357	48.612545
1504.295900	182.968435	48.617549
1500.685249	187.056968	48.622554
1497.320302	179.341413	48.627559
1493.773536	178.001091	48.632564
1489.846345	193.245540	48.637569
1486.387657	185.227019	48.642573
1483.094423	187.705008	48.647578
1479.824349	186.143530	48.652583
1476.546520	193.760584	48.657588
1472.688944	179.636008	48.662593
1468.981484	185.827062	48.667597
1465.613813	191.312731	48.672602
1462.001194	182.614288	48.677607
1459.077899	178.221278	48.682612
1455.327802	181.392418	48.687617
1452.137789	187.303150	48.692621
1448.298821	174.150182	48.697626
1444.397491	183.698707	48.702631
1441.270973	166.167013	48.707636
1437.328260	185.222780	48.712641
1433.953999	182.437909	48.717645
1430.647111	185.602306	48.722650
1426.937093	186.327252	48.727655
1424.035490	193.774013	48.732660
1420.163214	177.178471	48.737665
1416.597078	185.991305	48.742669
1413.094396	171.509594	48.747674
1409.609612	179.861529	48.752679
1405.960624	178.474100	48.757684
1402.649034	168.781748	48.762689
1399.209483	174.465849	48.767693
1395.990547	175.566998	48.772698
1392.092861	180.049015	48.777703
1388.783641	170.455519	48.782708
1385.079330	193.568669	48.787713
1381.557002	182.380856	48.792717
1378.143918	178.184832	48.797722
1374.407207	188.750029	48.802727
1371.162888	161.611639	48.807732
1367.700996	189.360249	48.812737
1364.002644	178.231393	48.817741
1360.676688	181.036925	48.822746
1356.812267	182.922450	48.827751
1353.867366	169.885769	48.832756
1349.967769	180.531126	48.837761
1346.706194	176.983590	48.842765
1343.250350	179.637341	48.847770
1339.696538	187.659079	48.852775
1336.293445	166.139239	48.857780
1332.321724	192.377153	48.862785
1328.866223	176.962868	48.867789
1325.457210	168.510088	48.872794
1321.867093	175.799235	48.877799
1318.706299	166.172110	48.882804
1314.867587	175.778225	48.887809
1311.504738	164.561580	48.892813
1308.281450	159.637612	48.897818
1304.247792	174.804790	48.902823
1301.196867	157.903416	48.907828
1297.496250	176.881284	48.912833
1294.063947	156.650720	48.917837
1290.723360	166.057226	48.922842
1287.072040	162.498590	48.927847
1283.732796	164.547540	48.932852
1279.483852	179.380336	48.937857
1276.620415	178.325284	48.942861
1273.020994	153.101089	48.947866
1269.226289	176.628105	48.952871
1266.066168	155.744758	48.957876
1262.831489	167.139129	48.962881
1258.818087	158.428358	48.967885
1255.717909	156.924281	48.972890
1251.710093	165.759967	48.977895
1248.535734	167.481527	48.982900
1244.867714	162.982686	48.987905
1241.447685	160.266734	48.992909
1238.056893	154.013835	48.997914
1234.273527	182.003450	49.002919
1231.247003	166.247837	49.007924
1227.935295	161.881765	49.012929
1223.917562	173.151985	49.017933
1220.495229	163.338632	49.022938
1216.702714	174.429426	49.027943
1213.394625	167.965783	49.032948
1209.999904	169.193992	49.037953
1206.378251	165.353300	49.042957
1203.196885	171.417773	49.047962
1199.471919	179.332278	49.052967
1196.043838	169.998529	49.057972
1192.181968	168.617159	49.062977
1188.768771	180.172039	49.067981
1185.435291	165.386534	49.072986
1181.880939	181.152463	49.077991
1178.803260	161.656867	49.082996
1175.083085	178.292631	49.088001
1171.373063	171.852053	49.093005
1167.941925	177.866722	49.098010
1164.122249	179.955579	49.103015
1160.687480	167.052162	49.108020
1157.335778	177.126145	49.113025
1153.910157	167.140836	49.118029
1150.868489	170.997591	49.123034
1146.767007	165.777424	49.128039
1143.398745	164.880446	49.133044
1139.792754	160.755664	49.138049
1136.389858	168.432846	49.143053
1132.610049	162.720105	49.148058
1129.240455	160.864488	49.153063
1125.956782	157.596639	49.158068
1122.756862	163.595940	49.163073
1119.146581	162.821004	49.168077
1115.595409	159.018252	49.173082
1111.776158	166.740700	49.178087
1108.478747	159.910552	49.183092
1104.709239	168.451370	49.188097
1101.446022	160.618833	49.193101
1098.047696	168.669944	49.198106
1094.298629	160.893550	49.203111
1091.097081	153.803630	49.208116
1086.913217	172.099676	49.213121
1083.719072	154.316392	49.218125
1080.416614	167.986892	49.223130
1076.686352	176.927484	49.228135
1073.756090	166.344214	49.233140
1069.834033	171.580938	49.238145
1066.209800	160.422693	49.243149
1063.217298	158.248762	49.248154
1059.135370	174.957507	49.253159
1055.722572	154.189517	49.258164
1051.998722	169.561445	49.263169
1048.611293	169.121463	49.268173
1045.586412	160.873757	49.273178
1041.775991	156.035224	49.278183
1038.414217	158.280471	49.283188
1034.629643	168.561703	49.288193
1030.963616	164.386718	49.293197
1027.788180	158.706846	49.298202
1024.237351	165.101599	49.303207
1020.952376	159.333965	49.308212
1017.503128	160.003547	49.313217
1014.014410	167.497947	49.318221
1010.703623	161.478487	49.323226
1006.862193	163.420975	49.328231
1003.137990	162.937576	49.333236
999.564883	165.954639	49.338241
995.972052	155.223439	49.343245
992.916007	153.494975	49.348250
989.307863	167.294204	49.353255
986.094499	159.901367	49.358260
982.446842	161.089174	49.363265
978.613107	161.461104	49.368269
975.233819	160.049311	49.373274
971.318784	175.457478	49.378279
968.079908	147.154174	49.383284
964.829266	157.992434	49.388289
961.015436	163.192304	49.393293
957.982412	158.287319	49.398298
954.121839	179.381784	49.403303
950.589700	157.351335	49.408308
947.251351	148.902609	49.413313
943.706983	165.386105	49.418317
940.280209	153.325166	49.423322
936.570003	162.124098	49.428327
933.346461	151.584309	49.433332
929.813338	155.549919	49.438337
926.159738	154.954383	49.443341
922.951847	150.086084	49.448346
919.222222	166.751210	49.453351
915.359007	149.799541	49.458356
912.287048	168.178215	49.463361
908.578627	153.376879	49.468365
905.566071	144.537205	49.473370
901.749761	162.416409	49.478375
898.534256	154.965083	49.483380
894.777776	154.268568	49.488385
890.952473	160.968641	49.493389
887.626583	165.401880	49.498394
883.915493	158.644408	49.503399
881.041427	156.216815	49.508404
877.313734	155.296359	49.513409
873.280669	155.126439	49.518413
870.121821	152.052673	49.523418
866.270245	160.315051	49.528423
863.078777	156.716044	49.533428
859.786142	156.793108	49.538433
856.125435	165.137521	49.543437
852.905491	160.045736	49.548442
849.304981	142.398580	49.553447
845.466502	146.366412	49.558452
841.956548	160.141685	49.563457
838.250702	146.409923	49.568461
834.655490	160.073007	49.573466
831.021168	167.227814	49.578471
828.626925	152.812959	49.583476
825.085314	161.233900	49.588481
821.046796	169.925418	49.593485
817.645911	163.132446	49.598490
813.689557	161.821553	49.603495
810.640098	162.107474	49.608500
806.980888	153.096839	49.613505
803.591705	163.203676	49.618509
800.304935	151.736458	49.623514
796.845770	165.419218	49.628519
793.330946	152.694311	49.633524
789.341830	157.833246	49.638529
785.722866	164.493084	49.643533
782.650053	160.578676	49.648538
779.179946	163.736185	49.653543
775.288388	163.858926	49.658548
772.281215	158.665164	49.663553
768.357088	166.764671	49.668557
765.208105	151.831003	49.673562
761.275923	161.935389	49.678567
758.146206	171.005321	49.683572
754.271683	161.760764	49.688577
750.799325	151.346814	49.693581
747.402112	165.137148	49.698586
744.141124	169.036108	49.703591
740.719036	162.253095	49.708596
737.571192	166.580645	49.713601
733.372772	162.036129	49.718605
730.211925	154.950834	49.723610
725.985132	165.560437	49.728615
723.172265	152.990540	49.733620
719.510475	163.170249	49.738625
715.855580	167.836058	49.743629
712.706160	164.467531	49.748634
708.739584	160.860179	49.753639
705.505082	160.395413	49.758644
702.148538	153.866670	49.763649
698.493687	161.903588	49.768653
694.876511	161.297725	49.773658
691.480219	160.716449	49.778663
688.008427	153.576089	49.783668
684.570230	164.512513	49.788673
681.069117	158.820912	49.793677
677.891638	166.481973	49.798682
673.859088	162.892246	49.803687
670.538038	169.482125	49.808692
666.838779	163.127588	49.813697
663.288402	163.591402	49.818701
660.163191	153.222672	49.823706
655.912287	159.898056	49.828711
653.078267	161.180527	49.833716
649.484600	151.412699	49.838721
645.751407	161.836944	49.843725
642.445998	156.608654	49.848730
638.736588	156.262210	49.853735
635.706986	162.356892	49.858740
632.344014	147.372536	49.863745
628.326625	161.400190	49.868749
625.143456	143.181065	49.873754
621.274606	170.238211	49.878759
617.953716	152.736902	49.883764
614.175544	156.260650	49.888769
610.891017	146.455899	49.893773
607.563388	153.265588	49.898778
603.826194	148.638872	49.903783
600.183007	143.228362	49.908788
596.854570	146.114952	49.913793
593.461117	159.034639	49.918797
589.981204	141.474297	49.923802
586.545580	145.323051	49.928807
582.837232	147.732200	49.933812
579.388096	146.915951	49.938817
575.816651	156.797974	49.943821
572.191180	154.150152	49.948826
568.903371	159.017708	49.953831
565.475545	157.616021	49.958836
562.049634	156.302309	49.963841
558.275422	158.063085	49.968845
554.803057	134.783983	49.973850
551.217369	151.767965	49.978855
547.502153	130.105779	49.983860
544.232092	143.596979	49.988865
540.609042	136.991613	49.993869
537.454909	145.703608	49.998874
533.768468	148.580110	50.003879
530.563813	148.373498	50.008884
527.463708	143.348615	50.013889
523.563995	142.318178	50.018893
519.686096	142.852050	50.023898
516.156049	149.437445	50.028903
512.895773	136.962988	50.033908
509.347363	159.873132	50.038913
505.492507	152.435500	50.043917
501.997292	144.047678	50.048922
498.701143	152.330060	50.053927
495.403474	143.765092	50.058932
492.095259	148.067640	50.063937
488.350522	162.788901	50.068941
484.858154	145.959992	50.073946
481.051108	163.599692	50.078951
477.776181	149.789210	50.083956
474.927417	145.720464	50.088961
470.988575	166.314549	50.093965
467.614476	141.906226	50.098970
463.314536	161.987797	50.103975
460.084268	151.246387	50.108980
456.506357	156.185984	50.113985
453.180813	161.249428	50.118989
449.873540	140.488741	50.123994
446.254504	146.813344	50.128999
442.596377	145.467130	50.134004
438.978173	142.745386	50.139009
435.449570	133.270404	50.144013
432.360266	148.918122	50.149018
428.726006	141.670110	50.154023
425.345719	138.789117	50.159028
422.291977	138.657856	50.164033
418.159173	145.401265	50.169037
414.758337	144.473645	50.174042
410.764523	151.199032	50.179047
407.284192	142.386401	50.184052
404.183489	133.587518	50.189057
400.639951	148.297070	50.194061
397.412220	134.201658	50.199066
393.787454	148.139592	50.204071
390.221476	140.113436	50.209076
386.686671	148.112117	50.214081
382.783933	153.086865	50.219085
379.750142	152.069921	50.224090
375.953709	147.497329	50.229095
372.523856	144.033257	50.234100
369.064334	151.811562	50.239105
365.774645	145.630462	50.244109
362.471469	145.557600	50.249114
358.803497	140.014708	50.254119
355.199480	145.367954	50.259124
351.711822	148.551655	50.264129
347.690312	145.443601	50.269133
344.545670	154.046286	50.274138
340.882056	146.482374	50.279143
338.129219	155.896229	50.284148
334.224661	146.221405	50.289153
330.608965	160.113683	50.294157
327.284186	143.642227	50.299162
323.399441	157.508322	50.304167
320.143613	149.884649	50.309172
316.614858	150.882414	50.314177
313.187260	160.685647	50.319181
309.991321	143.352142	50.324186
306.177130	145.741539	50.329191
302.307665	147.425664	50.334196
299.076298	146.594108	50.339201
295.480063	155.338009	50.344205
292.155205	144.341645	50.349210
288.616358	152.848585	50.354215
284.808916	149.572621	50.359220
281.743890	150.594905	50.364225
278.031733	153.736027	50.369229
274.594529	138.890259	50.374234
270.776670	153.629406	50.379239
267.637123	147.342369	50.384244
264.463281	146.498664	50.389249
260.448107	155.770015	50.394253
257.365874	145.085267	50.399258
253.802502	147.151615	50.404263
249.898039	149.837797	50.409268
246.776265	139.938317	50.414273
243.063138	160.422290	50.419277
239.277633	153.297339	50.424282
235.838910	150.896161	50.429287
232.575849	149.054297	50.434292
229.316068	146.979973	50.439297
225.300522	161.096984	50.444301
221.982053	133.510222	50.449306
218.424030	154.199996	50.454311
214.867765	139.355297	50.459316
211.539599	136.372886	50.464321
208.116008	154.634141	50.469325
205.051268	132.476971	50.474330
201.075664	145.848609	50.479335
197.532212	133.268736	50.484340
194.088074	147.382489	50.489345
190.106212	157.971536	50.494349
187.345873	144.455625	50.499354
183.589780	155.138276	50.504359
179.905353	148.604633	50.509364
176.320894	133.028813	50.514369
172.825024	156.056937	50.519373
169.415646	143.061909	50.524378
165.719295	146.253059	50.529383
162.304632	150.926115	50.534388
158.958659	140.296451	50.539393
155.387781	154.585255	50.544397
152.105299	147.834482	50.549402
148.613478	152.028239	50.554407
144.938067	149.456793	50.559412
141.752262	139.286515	50.564417
137.858168	157.323975	50.569421
134.272773	152.183573	50.574426
130.805667	143.324542	50.579431
127.141576	152.186370	50.584436
124.216305	144.470413	50.589441
120.619428	143.878786	50.594445
117.162462	132.877639	50.599450
113.391509	139.119192	50.604455
109.742554	135.691872	50.609460
106.274116	139.847061	50.614465
102.608388	142.223387	50.619469
99.437414	128.536866	50.624474
95.773292	137.182866	50.629479
92.618790	140.650008	50.634484
89.410977	134.264563	50.639489
85.461109	155.734426	50.644493
81.574436	127.025457	50.649498
77.793288	150.382578	50.654503
74.863210	137.951007	50.659508
71.645457	158.650209	50.664513
68.016569	136.567513	50.669517
64.715339	155.326399	50.674522
60.746036	145.198532	50.679527
56.966064	133.555828	50.684532
53.993222	144.393800	50.689537
50.394555	143.953834	50.694541
46.909804	147.936355	50.699546
43.264677	153.658593	50.704551
39.993198	139.898939	50.709556
36.507206	133.287129	50.714561
32.630702	132.773823	50.719565
29.206716	153.033996	50.724570
25.736710	156.922351	50.729575
22.330094	147.554925	50.734580
19.075688	136.524510	50.739585
15.394442	144.138571	50.744589
12.028272	146.886867	50.749594
8.237783	134.428642	50.754599
4.575387	142.300712	50.759604
1.317773	135.845024	50.764609