Wed Jun 15 15:53:03 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.455122	102.613842	0.000000
1.780016	102.775296	0.005005
1.341059	112.045112	0.010010
1.936472	98.076126	0.015014
1.548567	93.606310	0.020019
1.245830	78.691875	0.025024
1.143842	69.369226	0.030029
0.563052	75.208631	0.035034
0.564830	48.678236	0.040038
0.436145	56.150297	0.045043
-0.027334	37.687209	0.050048
-0.021764	25.869372	0.055053
-0.763254	24.584223	0.060058
-0.979002	13.411153	0.065062
-0.937172	16.022221	0.070067
-1.716791	13.056912	0.075072
-1.672827	-6.425844	0.080077
-2.108424	10.231780	0.085082
-2.589314	-4.855060	0.090086
-3.251357	-7.265081	0.095091
-3.830529	0.939671	0.100096
-3.354630	-1.711385	0.105101
-3.956745	6.413509	0.110106
-3.790719	-12.292545	0.115110
-3.868527	-3.905590	0.120115
-3.863315	-8.147068	0.125120
-4.373206	-1.662028	0.130125
-5.109573	0.507863	0.135130
-5.272464	-5.075245	0.140134
-5.471425	-4.594313	0.145139
-5.552514	-4.340315	0.150144
-5.355191	3.051306	0.155149
-6.412301	2.134582	0.160154
-6.748022	-4.335501	0.165158
-6.874469	1.991174	0.170163
-7.292162	5.288508	0.175168
-7.257938	-13.504963	0.180173
-7.171467	12.885256	0.185178
-7.135077	-13.983385	0.190182
-7.184788	1.380432	0.195187
-8.061695	2.983940	0.200192
-8.068069	8.943538	0.205197
-8.615576	-0.437132	0.210202
-8.899149	-8.877811	0.215206
-9.397723	-0.657675	0.220211
-9.988093	-1.024931	0.225216
-9.971644	2.638842	0.230221
-10.047214	-8.341835	0.235226
-9.792043	-12.211391	0.240230
-9.943845	12.077775	0.245235
-10.211292	-5.768856	0.250240
-10.830484	-14.884050	0.255245
-11.355723	-4.930632	0.260250
-11.291390	-9.569165	0.265254
-11.465887	2.441469	0.270259
-11.787374	4.784578	0.275264
-12.277254	-18.373299	0.280269
-12.996991	-5.229178	0.285274
-13.076119	-8.899167	0.290278
-13.290037	-0.764546	0.295283
-13.653158	-9.489793	0.300288
-13.512543	-6.009211	0.305293
-13.235341	-2.353711	0.310298
-13.089953	-9.939879	0.315302
-13.556700	-26.909429	0.320307
-14.212528	-10.223127	0.325312
-14.372970	-19.182709	0.330317
-14.756195	-6.073684	0.335322
-14.973461	-12.361115	0.340326
-15.699589	2.492033	0.345331
-16.155468	-2.804521	0.350336
-16.159339	-2.553716	0.355341
-16.341703	3.165068	0.360346
-16.404754	-4.725209	0.365350
-16.367362	-5.625424	0.370355
-16.378229	-1.486791	0.375360
-16.857089	-2.645864	0.380365
-17.501569	-4.732562	0.385370
-17.536569	-7.179328	0.390374
-17.838893	-0.610117	0.395379
-18.236486	3.595389	0.400384
-18.654094	-3.103831	0.405389
-19.293631	-5.955559	0.410394
-18.886260	-3.289294	0.415398
-19.345288	-5.399538	0.420403
-19.637476	3.075329	0.425408
-19.638566	-7.279315	0.430413
-20.134040	-7.862703	0.435418
-19.709215	-9.270264	0.440422
-19.716546	-6.014314	0.445427
-20.687670	-2.194728	0.450432
-20.856472	-5.510454	0.455437
-21.660767	-9.940621	0.460442
-21.234224	-14.276489	0.465446
-21.248330	-5.230847	0.470451
-22.366911	-7.466275	0.475456
-22.428453	-0.699021	0.480461
-22.794370	-2.600726	0.485466
-22.975770	-10.795494	0.490470
-22.950027	-2.357785	0.495475
-23.071149	-1.843353	0.500480
-22.787309	3.237972	0.505485
-23.303246	-0.525751	0.510490
-23.854671	-2.295882	0.515494
-24.312996	0.621374	0.520499
-24.413346	-8.920491	0.525504
-24.167280	-22.679714	0.530509
-24.936307	3.537187	0.535514
-25.442628	-23.734873	0.540518
-25.905178	-8.656881	0.545523
-26.221476	-8.379991	0.550528
-25.909655	-12.781636	0.555533
-26.486246	-10.926790	0.560538
-26.611782	2.671554	0.565542
-26.173774	-0.835312	0.570547
-26.001162	2.410334	0.575552
-26.833948	-1.962054	0.580557
-27.643232	-6.460843	0.585562
-27.491791	3.930208	0.590566
-27.492606	-2.047143	0.595571
-28.637382	7.344880	0.600576
-28.515050	-12.949160	0.605581
-29.164868	4.944681	0.610586
-29.392470	-4.190250	0.615590
-29.493691	-9.531011	0.620595
-29.499187	11.719433	0.625600
-29.417924	-3.878864	0.630605
-29.625885	-0.265701	0.635610
-29.935661	-9.859959	0.640614
-30.488356	-4.558804	0.645619
-30.864266	-1.519530	0.650624
-30.889667	-16.907134	0.655629
-31.163723	-4.553040	0.660634
-31.443507	-7.171539	0.665638
-31.654967	-6.242166	0.670643
-31.946102	7.382169	0.675648
-32.296629	-12.053231	0.680653
-32.726850	-0.865270	0.685658
-33.271442	-10.385206	0.690662
-33.140717	-3.130850	0.695667
-33.305487	4.402489	0.700672
-32.917286	-4.525253	0.705677
-33.476156	-4.555213	0.710682
-33.698185	4.401686	0.715686
-34.090995	-7.850690	0.720691
-34.330610	-3.887627	0.725696
-34.424779	-6.166187	0.730701
-35.163193	-6.767822	0.735706
-35.541742	6.038975	0.740710
-35.988486	-7.902982	0.745715
-36.236453	10.955800	0.750720
-35.885455	0.218910	0.755725
-36.039983	6.619871	0.760730
-36.189169	-0.505965	0.765734
-35.987343	-7.661793	0.770739
-36.719787	13.062857	0.775744
-37.157896	-0.855083	0.780749
-37.370627	-5.978741	0.785754
-37.653435	3.351713	0.790758
-37.646608	7.208648	0.795763
-38.548132	8.319543	0.800768
-38.743606	5.175035	0.805773
-39.100962	-2.931961	0.810778
-39.211351	-2.042473	0.815782
-39.185802	4.128966	0.820787
-39.531668	6.098191	0.825792
-39.362651	-5.362575	0.830797
-39.480471	-0.564670	0.835802
-40.596059	-1.397837	0.840806
-40.749023	-8.227500	0.845811
-40.757884	4.698720	0.850816
-40.640178	-1.247711	0.855821
-40.795401	5.254575	0.860826
-41.193156	-11.624288	0.865830
-41.481333	8.726652	0.870835
-41.684628	17.118768	0.875840
-41.692704	-9.495512	0.880845
-42.800371	11.248040	0.885850
-43.333403	-0.395797	0.890854
-43.362996	-5.273315	0.895859
-43.785272	8.938333	0.900864
-43.766543	4.987501	0.905869
-43.834918	1.666818	0.910874
-43.947890	0.401504	0.915878
-43.965177	-8.101529	0.920883
-44.273774	8.043543	0.925888
-43.727330	1.877395	0.930893
-44.637144	-12.525055	0.935898
-45.464107	-2.571488	0.940902
-45.492647	-13.197107	0.945907
-45.777168	1.944099	0.950912
-45.901093	-2.536068	0.955917
-46.927138	2.914544	0.960922
-47.037883	-5.235673	0.965926
-46.851178	-0.684996	0.970931
-47.068510	-5.850312	0.975936
-47.040547	-5.895380	0.980941
-47.373859	-2.789062	0.985946
-47.500393	-1.397459	0.990950
-47.381354	-2.339085	0.995955
-48.375103	1.169760	1.000960
-48.584304	-0.332579	1.005965
-48.740640	0.834793	1.010970
-48.704323	-3.240278	1.015974
-48.726290	4.297474	1.020979
-49.970527	2.584041	1.025984
-50.258094	5.734984	1.030989
-50.281791	6.947121	1.035994
-50.438400	1.499897	1.040998
-50.376149	4.788641	1.046003
-50.507248	8.945568	1.051008
-50.329048	-1.745893	1.056013
-51.195438	1.838774	1.061018
-51.633052	-3.182907	1.066022
-51.739976	2.694559	1.071027
-52.207856	-0.246894	1.076032
-51.934904	3.998522	1.081037
-52.021099	9.147908	1.086042
-53.091500	3.568889	1.091046
-53.584604	12.007320	1.096051
-53.943592	2.267895	1.101056
-53.617745	-6.206519	1.106061
-53.775074	6.699453	1.111066
-53.858558	-12.070118	1.116070
-53.906706	2.860477	1.121075
-53.959318	2.823694	1.126080
-54.473212	7.294743	1.131085
-54.893964	-8.561695	1.136090
-55.414346	9.259361	1.141094
-55.294091	-3.120523	1.146099
-55.669170	-5.091539	1.151104
-56.259962	-9.366500	1.156109
-56.967989	-5.373569	1.161114
-56.919740	-10.913339	1.166118
-56.796836	0.492758	1.171123
-57.257590	-4.595826	1.176128
-56.888938	4.190548	1.181133
-56.903926	0.835097	1.186138
-57.179346	7.649045	1.191142
-57.962203	-1.198203	1.196147
-58.353057	5.723012	1.201152
-58.265209	-0.698399	1.206157
-58.490792	-0.687358	1.211162
-59.347713	-1.479620	1.216166
-59.660292	3.164032	1.221171
-60.083544	13.482860	1.226176
-60.005440	6.166853	1.231181
-60.281633	9.047204	1.236186
-60.367103	-1.275935	1.241190
-59.792231	-11.608866	1.246195
-60.115910	-11.236350	1.251200
-60.607672	-24.612212	1.256205
-61.374882	3.252861	1.261210
-61.741945	-7.326972	1.266214
-61.614006	-0.679128	1.271219
-61.929874	-9.579383	1.276224
-62.433581	-14.434865	1.281229
-62.991865	-4.658778	1.286234
-63.193298	-0.008047	1.291238
-63.367757	-16.416170	1.296243
-63.661034	-1.701647	1.301248
-63.438364	-0.226200	1.306253
-63.566847	-7.366204	1.311258
-63.624501	-9.983630	1.316262
-63.649606	4.546893	1.321267
-64.589969	-4.624515	1.326272
-64.777078	-5.697742	1.331277
-65.280386	-0.279268	1.336282
-65.158038	7.804513	1.341286
-65.256768	11.185760	1.346291
-65.654119	7.845462	1.351296
-66.273166	14.481920	1.356301
-66.345390	-5.042684	1.361306
-66.528642	-9.719410	1.366310
-66.495845	-9.743575	1.371315
-67.170261	-9.640203	1.376320
-66.643236	-4.708870	1.381325
-67.394232	-22.459766	1.386330
-68.249875	3.000719	1.391334
-67.776743	-8.514841	1.396339
-68.262884	-3.212649	1.401344
-68.599312	-10.658810	1.406349
-69.176151	-3.411908	1.411354
-69.366982	-0.116061	1.416358
-69.505493	0.595579	1.421363
-69.848371	9.955594	1.426368
-69.462998	-0.564231	1.431373
-69.891739	4.688131	1.436378
-69.715487	4.587974	1.441382
-70.285887	3.680095	1.446387
-71.224596	10.591831	1.451392
-71.266047	4.518703	1.456397
-71.461526	-8.465682	1.461402
-71.346862	9.977835	1.466406
-71.269725	14.343312	1.471411
-72.201649	-5.312158	1.476416
-72.955459	0.091588	1.481421
-73.023205	-5.443711	1.486426
-72.689603	10.065391	1.491430
-72.788171	0.425670	1.496435
-73.552433	14.321748	1.501440
-73.155848	-10.003426	1.506445
-73.229480	8.717825	1.511450
-74.138751	7.795421	1.516454
-74.328855	-5.977546	1.521459
-74.573772	-0.603060	1.526464
-74.755065	-4.720095	1.531469
-74.702843	-1.907244	1.536474
-75.498201	7.992179	1.541478
-75.643849	-6.675263	1.546483
-76.597281	6.932755	1.551488
-75.988542	2.079061	1.556493
-76.457742	0.599571	1.561498
-76.304025	-1.153135	1.566502
-76.278463	6.906097	1.571507
-77.019399	10.404434	1.576512
-77.270189	16.694646	1.581517
-77.683490	-1.417593	1.586522
-78.078672	-1.928869	1.591526
-77.909083	4.538376	1.596531
-77.726718	16.251112	1.601536
-78.182239	5.238136	1.606541
-78.943485	-8.404722	1.611546
-79.218514	-12.993082	1.616550
-79.462410	2.665909	1.621555
-79.761014	1.848651	1.626560
-79.462647	8.736155	1.631565
-79.917584	6.750026	1.636570
-80.522806	10.090492	1.641574
-80.517743	-8.304552	1.646579
-81.110845	1.918144	1.651584
-81.182119	-6.253291	1.656589
-81.284145	13.318156	1.661594
-81.314076	0.657486	1.666598
-81.980324	-3.855464	1.671603
-82.741504	-2.235760	1.676608
-82.763689	-5.225520	1.681613
-83.043598	-4.647358	1.686618
-82.748698	-3.378086	1.691622
-82.791730	-4.176226	1.696627
-83.018897	2.437680	1.701632
-82.910294	-7.650590	1.706637
-83.586029	-14.075314	1.711642
-84.019815	-12.944751	1.716646
-84.423048	-21.043951	1.721651
-84.343915	-3.416797	1.726656
-84.569296	-21.551092	1.731661
-85.449540	-18.434976	1.736666
-86.147937	-9.037816	1.741670
-85.840001	-20.819142	1.746675
-86.070879	-0.907297	1.751680
-86.262855	-21.726349	1.756685
-86.399957	-15.780277	1.761690
-86.481778	-17.232738	1.766694
-86.609615	-8.710961	1.771699
-86.554861	-7.183990	1.776704
-87.350016	-4.535608	1.781709
-87.686291	-9.278487	1.786714
-88.136394	2.850493	1.791718
-87.788340	-11.892226	1.796723
-88.127770	-1.629681	1.801728
-88.011598	-13.605612	1.806733
-88.899099	-4.258579	1.811738
-89.890689	0.822633	1.816742
-89.737369	-18.558210	1.821747
-89.942181	-8.740421	1.826752
-90.118593	-11.279523	1.831757
-89.881326	-16.957660	1.836762
-90.063387	-8.063014	1.841766
-89.757349	-5.478063	1.846771
-90.659278	-8.123154	1.851776
-90.974307	-9.902458	1.856781
-91.250705	-16.858891	1.861786
-91.471682	1.799301	1.866790
-91.981180	-7.883076	1.871795
-92.560819	-16.721379	1.876800
-92.746260	3.367429	1.881805
-92.892029	-14.606708	1.886810
-93.093804	2.756735	1.891814
-92.772829	-4.518714	1.896819
-93.026363	5.964517	1.901824
-92.816660	-6.198622	1.906829
-93.685701	-2.099665	1.911834
-94.090976	-10.902472	1.916838
-94.070112	-7.550466	1.921843
-94.504503	-10.255370	1.926848
-95.415451	-1.751536	1.931853
-95.602392	-11.014114	1.936858
-95.871228	7.644300	1.941862
-94.982562	-20.177226	1.946867
-95.401697	-4.460081	1.951872
-95.742764	-7.030665	1.956877
-96.190054	-12.548803	1.961882
-96.682402	-6.343169	1.966886
-97.226949	-20.403885	1.971891
-97.573889	-6.081991	1.976896
-97.458397	-6.815380	1.981901
-97.544790	-6.124290	1.986906
-97.716276	-9.405632	1.991910
-97.373893	-21.655991	1.996915
-98.544972	-0.608857	2.006912
-98.149767	-5.110656	2.016909
-97.679187	-5.456310	2.026906
-97.128625	2.568446	2.036902
-96.247176	8.280276	2.046899
-96.044493	-3.610796	2.056896
-95.873012	-13.649752	2.066893
-94.805256	-13.185398	2.076890
-94.364953	-6.989669	2.086886
-94.351326	-8.497617	2.096883
-93.830211	-8.301261	2.106880
-93.355217	-7.959791	2.116877
-92.444335	-4.908136	2.126874
-91.767791	-13.394498	2.136870
-92.031199	-6.219977	2.146867
-90.789761	-10.714071	2.156864
-90.553951	-6.568547	2.166861
-90.269304	-12.437654	2.176858
-89.433239	-7.327557	2.186854
-89.072443	-9.567403	2.196851
-88.795204	-12.847343	2.206848
-87.713906	-14.598918	2.216845
-87.427266	-12.924099	2.226842
-87.306082	-4.965870	2.236838
-86.449057	-13.995876	2.246835
-85.920500	-8.084875	2.256832
-85.771445	-3.004450	2.266829
-84.968891	-6.590587	2.276826
-84.313515	-6.953449	2.286822
-84.149688	-8.577981	2.296819
-83.573108	-13.354908	2.306816
-82.525647	-2.498485	2.316813
-82.369544	-3.293137	2.326810
-82.166877	-11.296903	2.336806
-81.751976	-4.955826	2.346803
-81.339334	-1.907259	2.356800
-80.547109	1.871323	2.366797
-79.668802	8.634717	2.376794
-79.295847	4.318236	2.386790
-79.368207	2.888404	2.396787
-78.713373	5.937837	2.406784
-77.921627	-1.056842	2.416781
-77.809114	3.093557	2.426778
-76.512737	-9.622371	2.436774
-76.509998	4.089590	2.446771
-76.183503	-0.525900	2.456768
-75.374123	-12.465976	2.466765
-74.606418	-10.206912	2.476762
-74.522063	-14.898535	2.486758
-74.408779	-5.514105	2.496755
-73.533276	0.106061	2.506752
-73.355515	6.179055	2.516749
-72.279563	-0.443010	2.526746
-71.584539	-6.095282	2.536742
-71.546477	-6.869930	2.546739
-71.271556	-2.436130	2.556736
-70.210380	-1.686415	2.566733
-70.070040	0.621619	2.576730
-69.678214	3.578412	2.586726
-69.143456	-9.424805	2.596723
-68.842305	-13.052722	2.606720
-67.805307	-10.200784	2.616717
-67.040338	-6.944156	2.626714
-67.138062	-10.586056	2.636710
-66.721515	2.276517	2.646707
-65.634926	2.318177	2.656704
-65.732397	2.131007	2.666701
-65.078856	-11.656242	2.676698
-64.383155	-11.252080	2.686694
-64.100691	0.007546	2.696691
-63.432396	-6.050511	2.706688
-62.609731	-15.951939	2.716685
-62.468196	-4.247364	2.726682
-62.333323	-10.922890	2.736678
-61.316460	-8.859681	2.746675
-61.064666	-3.913773	2.756672
-60.525473	-7.919922	2.766669
-59.549306	-6.891051	2.776666
-59.118307	-5.978809	2.786662
-58.833409	2.247305	2.796659
-58.774895	-3.595198	2.806656
-58.217944	-0.259542	2.816653
-57.355031	6.325053	2.826650
-57.029038	4.445157	2.836646
-56.216404	-3.651227	2.846643
-55.727153	-0.436144	2.856640
-55.875503	-3.533640	2.866637
-55.046279	-2.521077	2.876634
-54.198071	-0.189974	2.886630
-54.014957	9.322097	2.896627
-53.649820	3.496574	2.906624
-52.664602	11.988806	2.916621
-52.418173	5.565176	2.926618
-52.209944	4.863645	2.936614
-51.211787	3.683189	2.946611
-50.864737	6.393638	2.956608
-50.792996	8.670638	2.966605
-49.480723	4.815356	2.976602
-49.059883	-1.239833	2.986598
-48.977951	-4.801691	2.996595
-49.110163	-6.122364	3.006592
-47.740453	-0.349485	3.016589
-47.476651	1.152310	3.026586
-46.683446	-10.395930	3.036582
-45.873286	1.649638	3.046579
-46.069004	0.550932	3.056576
-46.070034	2.697726	3.066573
-44.702688	0.569571	3.076570
-44.495255	7.808616	3.086566
-44.119065	6.384953	3.096563
-43.406599	5.516524	3.106560
-43.221350	-4.189187	3.116557
-42.252066	-7.621529	3.126554
-41.617232	7.387558	3.136550
-41.371044	3.912337	3.146547
-41.367614	1.219811	3.156544
-40.270752	-7.020737	3.166541
-40.151260	0.352848	3.176538
-39.122170	-8.549635	3.186534
-38.646242	0.525764	3.196531
-38.370533	-5.113902	3.206528
-38.269871	-1.207092	3.216525
-37.254242	-9.856961	3.226522
-36.585387	-11.167300	3.236518
-36.566942	-7.808525	3.246515
-35.906129	-6.209567	3.256512
-35.087982	-5.547494	3.266509
-35.107804	0.430937	3.276506
-34.479418	-4.510417	3.286502
-33.751779	-2.867683	3.296499
-33.251831	-4.242163	3.306496
-33.336870	8.386752	3.316493
-32.422641	9.412433	3.326490
-31.796587	1.298682	3.336486
-31.716654	-0.823333	3.346483
-30.637762	8.017004	3.356480
-30.157606	1.122418	3.366477
-29.857638	0.029599	3.376474
-29.656467	-1.457095	3.386470
-28.615131	-7.378071	3.396467
-28.512128	4.189170	3.406464
-27.970868	-3.113271	3.416461
-26.900161	-3.917338	3.426458
-26.885026	-1.622884	3.436454
-26.858732	3.924587	3.446451
-25.820903	5.583322	3.456448
-25.783122	5.567986	3.466445
-24.144182	12.050808	3.476442
-24.335932	5.862767	3.486438
-23.540921	-2.820871	3.496435
-23.625926	3.348792	3.506432
-23.097220	8.050113	3.516429
-22.107744	4.598827	3.526426
-21.904484	2.201003	3.536422
-21.781214	2.588952	3.546419
-20.563797	10.618686	3.556416
-20.416504	6.292978	3.566413
-20.025337	-3.021155	3.576410
-19.108110	5.091375	3.586406
-18.714390	3.754700	3.596403
-18.742875	-0.187362	3.606400
-17.850085	0.476404	3.616397
-17.227367	-7.942788	3.626394
-17.006579	-7.126479	3.636390
-15.655758	-10.108847	3.646387
-15.746370	-2.170129	3.656384
-15.789967	1.421733	3.666381
-15.033649	-10.343834	3.676378
-14.016596	-4.302575	3.686374
-13.875623	-4.483816	3.696371
-13.505135	3.792954	3.706368
-12.479008	-7.420124	3.716365
-12.160518	7.316388	3.726362
-12.035717	3.476409	3.736358
-11.765594	3.803246	3.746355
-10.991611	9.466183	3.756352
-9.984625	-0.568143	3.766349
-9.840542	2.223460	3.776346
-9.289905	7.046106	3.786342
-9.187880	4.431218	3.796339
-7.981988	-0.665038	3.806336
-7.285657	6.816890	3.816333
-7.380513	-0.905499	3.826330
-7.141914	0.468206	3.836326
-6.355167	-1.655155	3.846323
-5.838324	-4.822683	3.856320
-5.692471	3.933913	3.866317
-4.711471	6.434699	3.876314
-4.243093	1.811366	3.886310
-3.993180	14.855291	3.896307
-3.417311	18.602974	3.906304
-3.329019	22.716988	3.916301
-2.622182	34.794781	3.926298
-2.024499	41.026168	3.936294
-1.485037	62.818076	3.946291
-1.207961	66.078319	3.956288
-0.812217	82.541684	3.966285
-0.164273	105.128729	3.976282
0.000000	107.869553	3.981286
0.065139	116.078863	3.986291
0.297590	129.711974	3.991296
0.649676	126.066574	3.996301
0.596892	148.321466	4.001306
0.724293	138.594686	4.006310
0.911782	128.289575	4.011315
0.749038	134.304659	4.016320
1.094269	136.252710	4.021325
0.747747	129.824207	4.026330
0.794208	140.442527	4.031334
0.861933	142.496911	4.036339
1.204358	152.532546	4.041344
1.212377	144.995637	4.046349
0.747231	136.413138	4.051354
1.108627	152.227658	4.056358
0.985496	148.089816	4.061363
1.217258	148.702882	4.066368
0.992894	132.681640	4.071373
0.950543	158.629660	4.076378
1.006238	153.337288	4.081382
1.224762	166.336852	4.086387
1.511026	163.008424	4.091392
1.256560	138.573570	4.096397
0.731527	139.535142	4.101402
1.253194	136.598610	4.106406
1.180300	160.552691	4.111411
1.242796	154.228327	4.116416
1.330451	138.551977	4.121421
0.910913	144.938691	4.126426
1.524359	156.062504	4.131430
1.140161	154.612743	4.136435
1.075288	153.948911	4.141440
1.443504	163.586983	4.146445
1.398542	161.522517	4.151450
1.382377	150.990717	4.156454
1.290388	138.346689	4.161459
0.976131	138.654316	4.166464
1.292375	149.357975	4.171469
1.380590	161.924109	4.176474
1.688211	155.965860	4.181478
1.262697	158.937502	4.186483
1.170091	166.088772	4.191488
1.307743	164.804910	4.196493
1.339334	172.060841	4.201498
1.112404	178.148007	4.206502
1.342415	178.218801	4.211507
1.313476	181.286987	4.216512
1.639067	178.469661	4.221517
1.290602	175.624540	4.226522
1.679898	168.987410	4.231526
1.847312	180.468763	4.236531
2.123092	165.216653	4.241536
1.627325	153.798648	4.246541
1.250724	161.935974	4.251546
1.358683	141.389687	4.256550
1.320514	177.303203	4.261555
1.419951	175.103597	4.266560
1.514079	183.505249	4.271565
1.571859	188.801170	4.276570
1.530626	173.735603	4.281574
1.578772	178.603403	4.286579
1.320072	173.688618	4.291584
1.950546	179.154462	4.296589
1.618188	187.704531	4.301594
1.863106	177.016713	4.306598
1.637918	174.390341	4.311603
1.568266	190.557481	4.316608
1.966260	178.733392	4.321613
1.860868	182.560976	4.326618
1.759710	169.742252	4.331622
1.872953	185.943380	4.336627
1.658393	176.805096	4.341632
1.789886	170.787955	4.346637
1.896339	172.663605	4.351642
1.843913	187.023333	4.356646
1.767424	175.827820	4.361651
1.746469	181.822844	4.366656
1.979842	176.161258	4.371661
1.277152	174.262508	4.376666
1.601035	167.320121	4.381670
1.990350	167.047732	4.386675
1.695994	160.855536	4.391680
1.684906	165.327581	4.396685
1.320986	176.627730	4.401690
1.872714	165.228473	4.406694
1.988174	183.185455	4.411699
1.794843	162.018325	4.416704
1.943550	174.673416	4.421709
2.001451	182.982802	4.426714
1.941876	176.528659	4.431718
2.004701	178.336055	4.436723
2.002196	166.285673	4.441728
2.059175	182.064907	4.446733
1.687103	191.331707	4.451738
1.616314	174.376790	4.456742
2.011498	194.941870	4.461747
1.641523	200.710673	4.466752
2.138271	194.936896	4.471757
2.015107	203.634703	4.476762
2.129865	201.875687	4.481766
2.166932	199.236353	4.486771
1.902696	209.421707	4.491776
2.452658	196.545270	4.496781
2.213891	191.475563	4.501786
2.243546	196.230513	4.506790
2.323322	183.862290	4.511795
2.130774	199.550691	4.516800
2.605167	180.978107	4.521805
2.012678	195.273008	4.526810
2.560174	182.296665	4.531814
2.039532	194.499311	4.536819
2.082484	187.737997	4.541824
2.143327	204.056514	4.546829
1.882818	210.512957	4.551834
2.162924	207.567206	4.556838
2.340878	184.220618	4.561843
2.057120	210.877652	4.566848
2.728527	191.407256	4.571853
2.457034	202.997069	4.576858
2.535955	192.564747	4.581862
2.516097	203.611745	4.586867
2.350534	197.271981	4.591872
2.553722	194.829914	4.596877
2.253528	185.654381	4.601882
2.450408	202.999139	4.606886
2.244194	203.270366	4.611891
2.036260	200.712757	4.616896
2.473265	200.109907	4.621901
1.979498	198.445836	4.626906
1.871557	203.257759	4.631910
2.293060	197.692231	4.636915
2.352534	198.822078	4.641920
2.540103	206.300249	4.646925
2.595285	200.828011	4.651930
2.429972	200.822183	4.656934
2.452762	209.585840	4.661939
2.743546	214.436142	4.666944
2.758511	216.834954	4.671949
2.368135	199.808530	4.676954
2.473715	205.243738	4.681958
2.812563	216.867152	4.686963
2.518077	224.616078	4.691968
3.053892	216.872939	4.696973
2.463632	213.083463	4.701978
2.859495	197.458316	4.706982
2.708525	200.655580	4.711987
2.671227	209.036154	4.716992
2.278348	190.369146	4.721997
2.325299	217.826518	4.727002
2.654051	218.533846	4.732006
2.688933	225.278459	4.737011
2.678902	224.950828	4.742016
3.131354	226.838752	4.747021
2.787938	233.600411	4.752026
2.978640	215.873916	4.757030
3.003174	217.519055	4.762035
2.713789	222.651883	4.767040
3.156659	224.032860	4.772045
2.490918	215.373672	4.777050
2.152117	215.145950	4.782054
2.657094	213.526941	4.787059
2.897334	232.305220	4.792064
2.846518	217.054256	4.797069
2.862388	219.360980	4.802074
2.910783	228.007858	4.807078
2.735973	211.703016	4.812083
2.789579	217.250498	4.817088
2.875066	221.483359	4.822093
2.597387	232.535599	4.827098
3.051739	211.084585	4.832102
3.217495	214.532851	4.837107
2.918010	234.329592	4.842112
2.860874	215.227273	4.847117
2.872850	229.187527	4.852122
2.803712	238.500374	4.857126
2.961258	226.255695	4.862131
3.022551	240.295507	4.867136
3.342150	257.429852	4.872141
2.887315	232.257420	4.877146
3.395703	239.220224	4.882150
3.024917	226.714335	4.887155
2.717562	246.288954	4.892160
3.162031	235.018055	4.897165
3.262393	253.794914	4.902170
3.233883	259.089138	4.907174
3.374214	255.986543	4.912179
3.144976	253.101185	4.917184
3.381469	254.861541	4.922189
3.091311	238.788616	4.927194
3.194627	229.753730	4.932198
3.328242	232.351244	4.937203
3.175114	244.251701	4.942208
3.288736	240.380221	4.947213
3.417831	251.425130	4.952218
3.437501	257.563218	4.957222
3.017628	239.514498	4.962227
3.099356	238.254670	4.967232
3.723062	232.885268	4.972237
3.214532	244.953861	4.977242
3.541721	236.843101	4.982246
3.236474	232.124407	4.987251
3.065681	225.077203	4.992256
3.400339	238.575143	4.997261
3.747528	242.359120	5.002266
3.613656	251.615296	5.007270
3.578952	238.484261	5.012275
3.214718	232.033782	5.017280
3.428511	237.180922	5.022285
3.367913	232.275106	5.027290
3.417662	244.625313	5.032294
3.397655	257.494799	5.037299
3.195703	255.143255	5.042304
3.648819	265.936046	5.047309
3.554554	257.697432	5.052314
3.712294	250.913963	5.057318
3.588281	254.183531	5.062323
3.419515	259.088980	5.067328
3.566136	256.685156	5.072333
3.481359	248.457112	5.077338
3.908811	254.020855	5.082342
3.702021	257.719314	5.087347
3.647910	259.607206	5.092352
3.765928	257.068127	5.097357
3.673388	253.887909	5.102362
3.845415	245.916528	5.107366
3.832134	244.120465	5.112371
3.502270	233.543775	5.117376
3.624297	231.002657	5.122381
3.591898	256.894648	5.127386
3.850361	246.786468	5.132390
3.793197	252.020909	5.137395
3.696311	252.229677	5.142400
3.823294	242.818771	5.147405
3.851281	257.454611	5.152410
3.733768	256.308797	5.157414
3.580721	252.741717	5.162419
3.799204	249.184067	5.167424
3.582223	248.505712	5.172429
3.551057	250.471590	5.177434
3.761338	258.703256	5.182438
3.671206	257.307777	5.187443
3.356397	270.274332	5.192448
4.001020	231.933558	5.197453
3.652116	257.877660	5.202458
3.910370	243.290199	5.207462
3.764242	255.452603	5.212467
3.942018	263.385215	5.217472
4.319232	245.332312	5.222477
3.991038	249.167336	5.227482
4.125506	260.383109	5.232486
4.169466	254.012542	5.237491
3.912186	253.016294	5.242496
3.985404	250.265325	5.247501
3.969970	256.207380	5.252506
3.952644	246.794277	5.257510
3.871543	261.445879	5.262515
3.911991	261.995273	5.267520
3.884410	250.538590	5.272525
3.759474	266.394832	5.277530
3.863199	275.600215	5.282534
4.343161	284.080312	5.287539
3.946263	305.061239	5.292544
4.132823	285.939175	5.297549
4.458217	295.576221	5.302554
4.391160	280.956860	5.307558
4.280135	272.217901	5.312563
4.065271	265.772613	5.317568
4.033165	258.934198	5.322573
4.178918	288.534975	5.327578
4.571142	281.624845	5.332582
4.348639	265.655834	5.337587
3.837670	252.647986	5.342592
4.113631	271.329357	5.347597
4.538022	287.926542	5.352602
4.671008	275.815802	5.357606
4.635528	264.499113	5.362611
3.909082	262.457192	5.367616
4.116857	249.232409	5.372621
4.126508	279.820342	5.377626
4.541636	266.018810	5.382630
4.453712	282.696316	5.387635
4.141632	286.410209	5.392640
4.472434	289.450433	5.397645
4.416263	276.877809	5.402650
4.412659	285.673986	5.407654
4.387660	282.771738	5.412659
4.154055	268.599268	5.417664
4.258701	277.049643	5.422669
4.055300	279.129320	5.427674
4.235860	284.762978	5.432678
4.306564	288.058872	5.437683
4.051928	282.415453	5.442688
4.279099	275.606491	5.447693
4.615860	284.641573	5.452698
4.345291	291.950456	5.457702
4.681214	292.347734	5.462707
4.485719	298.750361	5.467712
4.550713	282.247976	5.472717
4.432447	311.332994	5.477722
4.753648	314.216380	5.482726
4.767252	324.750784	5.487731
4.560140	311.993152	5.492736
4.846995	314.810793	5.497741
4.416490	304.875822	5.502746
4.602116	311.464063	5.507750
4.872583	316.733855	5.512755
4.732954	312.974645	5.517760
4.694545	299.383678	5.522765
4.459323	290.857007	5.527770
4.719079	317.790587	5.532774
4.903653	305.834067	5.537779
4.886495	309.591759	5.542784
4.832081	311.619197	5.547789
4.556181	294.399041	5.552794
4.759708	325.652173	5.557798
5.186413	323.081206	5.562803
4.711391	319.857841	5.567808
4.347161	296.136643	5.572813
4.755602	315.804164	5.577818
4.905219	311.738792	5.582822
4.955174	312.908891	5.587827
4.962290	307.380240	5.592832
4.899182	300.522268	5.597837
4.878422	313.893849	5.602842
4.699459	312.830595	5.607846
5.079441	325.430129	5.612851
4.738696	321.427050	5.617856
4.998757	325.202461	5.622861
4.802421	309.224147	5.627866
4.782218	318.235081	5.632870
4.696353	319.006989	5.637875
4.773944	314.105537	5.642880
4.720403	311.933462	5.647885
4.666341	323.657404	5.652890
4.993044	314.048704	5.657894
5.149196	313.189908	5.662899
4.828712	323.241198	5.667904
5.168109	319.334359	5.672909
5.374956	334.689555	5.677914
5.082879	314.806760	5.682918
5.135836	316.862227	5.687923
5.166360	306.875035	5.692928
5.254170	314.942400	5.697933
4.945194	313.631124	5.702938
4.712669	322.435362	5.707942
5.142811	326.166191	5.712947
5.197392	342.384184	5.717952
4.893388	338.015256	5.722957
5.207160	343.204408	5.727962
5.288098	334.832427	5.732966
5.444487	334.893095	5.737971
5.364264	351.729806	5.742976
5.754654	334.176545	5.747981
5.426908	335.730365	5.752986
4.926292	320.456859	5.757990
5.404952	325.797605	5.762995
5.568540	353.631329	5.768000
5.763454	320.575087	5.773005
5.406962	316.134639	5.778010
5.387817	324.822230	5.783014
5.204361	298.917455	5.788019
5.497265	315.587402	5.793024
5.461496	307.904645	5.798029
5.045200	316.396842	5.803034
5.140148	306.935750	5.808038
5.495374	321.562751	5.813043
5.642635	327.143330	5.818048
5.414569	330.150047	5.823053
5.332768	333.392926	5.828058
5.547636	330.521562	5.833062
5.703779	338.627463	5.838067
5.141630	339.863998	5.843072
5.820515	328.579840	5.848077
5.340300	335.459249	5.853082
5.947150	327.190159	5.858086
5.624347	311.024003	5.863091
5.669301	308.902139	5.868096
5.641157	317.158639	5.873101
5.531570	321.904086	5.878106
5.493518	325.992156	5.883110
5.574264	320.787625	5.888115
5.363978	319.871502	5.893120
5.454364	337.142367	5.898125
5.806504	342.060503	5.903130
5.534707	349.948981	5.908134
6.043359	339.898929	5.913139
5.729562	355.160944	5.918144
5.875662	335.328722	5.923149
5.503859	337.143449	5.928154
5.588039	343.358708	5.933158
5.748776	339.388955	5.938163
5.715184	345.670438	5.943168
5.848749	343.551386	5.948173
5.657189	343.671234	5.953178
5.671297	337.138258	5.958182
5.834363	337.952287	5.963187
5.821948	344.114752	5.968192
5.910142	344.886997	5.973197
5.588238	343.023252	5.978202
5.675494	352.890278	5.983206
5.760668	347.368837	5.988211
5.946944	340.508599	5.993216
5.851649	339.262135	5.998221
6.245019	335.737317	6.003226
5.823053	354.415655	6.008230
6.245884	333.743678	6.013235
5.957705	350.468854	6.018240
6.414022	336.601953	6.023245
5.538588	334.922318	6.028250
5.506117	316.807708	6.033254
5.729577	323.615705	6.038259
5.505452	349.419778	6.043264
5.844132	338.928841	6.048269
5.559303	344.825089	6.053274
5.638913	344.858986	6.058278
5.861909	348.532705	6.063283
5.583742	346.252240	6.068288
5.776078	349.390135	6.073293
5.608867	340.109273	6.078298
5.827910	349.771425	6.083302
6.107639	344.847902	6.088307
5.777804	360.434858	6.093312
6.037118	350.957722	6.098317
5.881001	341.809780	6.103322
5.873998	342.010501	6.108326
6.058143	353.082294	6.113331
5.668647	351.335864	6.118336
5.845377	349.987524	6.123341
5.810568	346.284673	6.128346
5.900174	345.876945	6.133350
6.046416	335.739901	6.138355
5.871072	350.927832	6.143360
6.098508	342.761093	6.148365
6.051280	341.890922	6.153370
6.036808	345.734990	6.158374
6.197091	332.224998	6.163379
6.100258	348.974878	6.168384
5.840718	330.939012	6.173389
5.623999	322.185826	6.178394
6.046653	339.821828	6.183398
6.063890	333.024057	6.188403
5.485964	328.115810	6.193408
5.634713	335.916628	6.198413
5.832000	339.223477	6.203418
5.670766	353.173109	6.208422
5.978054	344.852993	6.213427
5.642591	345.311608	6.218432
5.861975	353.179779	6.223437
5.932679	336.657550	6.228442
5.816346	348.427118	6.233446
6.174106	345.789905	6.238451
5.843061	352.981160	6.243456
6.225748	345.821024	6.248461
5.873769	355.639402	6.253466
5.518363	338.045731	6.258470
6.084623	345.562995	6.263475
5.874396	342.638076	6.268480
5.817752	343.248403	6.273485
5.583355	338.905163	6.278490
5.937834	349.869489	6.283494
6.049495	358.561032	6.288499
5.780064	357.429466	6.293504
5.753078	360.094877	6.298509
5.915797	361.755175	6.303514
5.788226	353.788957	6.308518
6.134671	351.672802	6.313523
5.832613	351.386326	6.318528
6.024009	344.120978	6.323533
5.875087	342.932110	6.328538
5.572212	337.810602	6.333542
5.978832	337.224016	6.338547
5.647846	347.522002	6.343552
5.836596	328.920190	6.348557
6.137443	355.612854	6.353562
5.967160	346.510852	6.358566
5.768309	319.316486	6.363571
5.604067	333.669380	6.368576
5.752233	335.640357	6.373581
5.648060	351.043122	6.378586
5.673193	354.658982	6.383590
5.954020	350.947472	6.388595
5.751334	373.038946	6.393600
6.013887	355.458747	6.398605
5.930553	353.352949	6.403610
5.867465	368.841869	6.408614
5.993099	347.731466	6.413619
5.682717	362.934722	6.418624
6.151270	354.820859	6.423629
6.033031	353.815436	6.428634
5.464559	348.007916	6.433638
5.945366	343.066354	6.438643
5.503169	348.923799	6.443648
5.736244	360.663254	6.448653
6.052716	352.811875	6.453658
6.083270	342.779671	6.458662
5.903873	346.526894	6.463667
5.846055	371.613670	6.468672
6.001842	347.013118	6.473677
5.750098	364.476987	6.478682
5.928988	360.495351	6.483686
5.985053	351.128948	6.488691
5.539913	357.290326	6.493696
5.493647	353.365631	6.498701
6.108484	351.535397	6.503706
5.499706	357.567854	6.508710
5.831164	343.314163	6.513715
5.695302	360.379769	6.518720
5.705432	345.808653	6.523725
6.318277	345.078386	6.528730
6.076879	355.817034	6.533734
5.932357	348.920013	6.538739
5.964897	356.337264	6.543744
6.018137	363.079398	6.548749
5.719550	358.173216	6.553754
5.449749	373.587690	6.558758
5.807982	369.592592	6.563763
5.663421	370.428558	6.568768
5.713364	367.781050	6.573773
5.852863	354.751835	6.578778
5.700122	371.497464	6.583782
6.117397	360.201570	6.588787
5.752020	370.500717	6.593792
5.612484	368.198029	6.598797
5.731010	356.578617	6.603802
5.707866	373.243050	6.608806
5.915816	368.386427	6.613811
5.761517	357.762584	6.618816
5.957456	356.399922	6.623821
5.644295	363.346832	6.628826
5.719155	372.493810	6.633830
6.132003	362.151200	6.638835
5.648770	370.406880	6.643840
5.730875	350.996285	6.648845
5.692974	355.495111	6.653850
5.655102	369.220660	6.658854
6.037861	352.360465	6.663859
6.002698	361.021918	6.668864
6.127425	347.360740	6.673869
6.015855	355.110183	6.678874
6.200264	359.708504	6.683878
5.841878	356.218543	6.688883
5.921595	353.852593	6.693888
6.236008	352.957676	6.698893
6.103133	353.668498	6.703898
5.991381	354.341598	6.708902
6.209499	345.906692	6.713907
5.697122	341.099574	6.718912
5.919939	330.338849	6.723917
6.306391	319.713069	6.728922
5.799690	315.893775	6.733926
5.854225	318.116389	6.738931
5.543460	311.842893	6.743936
5.575285	316.507259	6.748941
5.789276	330.948476	6.753946
6.034679	344.785716	6.758950
5.965158	338.055452	6.763955
5.678764	329.060447	6.768960
5.797618	336.763118	6.773965
6.134887	338.640202	6.778970
6.150227	330.240592	6.783974
5.882429	323.118518	6.788979
5.799647	302.914576	6.793984
5.637605	316.171302	6.798989
5.898297	314.836612	6.803994
5.883085	318.522661	6.808998
6.027433	318.926544	6.814003
5.527430	329.894948	6.819008
5.817847	320.923198	6.824013
5.894636	326.509208	6.829018
5.587725	328.461676	6.834022
5.935931	336.462835	6.839027
6.287989	367.718931	6.844032
6.253746	349.733312	6.849037
5.894215	341.904182	6.854042
5.628523	323.920047	6.859046
6.071971	324.434508	6.864051
5.742630	323.928906	6.869056
5.904328	322.659702	6.874061
6.033673	330.451097	6.879066
5.890571	336.108570	6.884070
5.930450	333.684098	6.889075
5.577360	329.524036	6.894080
5.689873	341.719132	6.899085
6.029681	328.240440	6.904090
5.790354	339.037824	6.909094
5.820015	327.800389	6.914099
5.847715	323.370630	6.919104
6.308736	329.866212	6.924109
6.248466	332.135224	6.929114
5.689220	335.685576	6.934118
5.577558	318.641960	6.939123
5.673815	328.294797	6.944128
5.902292	326.221323	6.949133
5.632892	333.036592	6.954138
5.681646	321.321013	6.959142
5.839919	318.527466	6.964147
5.338342	332.521488	6.969152
5.411425	335.090846	6.974157
5.721196	347.621702	6.979162
5.755826	361.462322	6.984166
5.967493	356.406607	6.989171
5.792520	350.894814	6.994176
5.835341	360.957016	6.999181
6.323381	354.005370	7.004186
6.102220	360.294576	7.009190
6.404034	345.884786	7.014195
5.988143	329.465472	7.019200
5.797874	328.908476	7.024205
5.998584	327.988551	7.029210
5.621875	336.278695	7.034214
6.082984	320.262252	7.039219
5.644272	330.751355	7.044224
5.897490	316.125297	7.049229
5.891158	324.578651	7.054234
5.679360	326.272427	7.059238
5.589337	323.753316	7.064243
5.572936	324.127930	7.069248
5.990807	333.665076	7.074253
6.002215	335.699001	7.079258
5.613872	343.074625	7.084262
5.725818	325.441220	7.089267
5.600537	348.531607	7.094272
5.742536	350.575915	7.099277
6.306809	353.112340	7.104282
6.114050	344.498616	7.109286
6.138759	331.173999	7.114291
5.950626	329.618818	7.119296
6.070916	326.835197	7.124301
5.982956	327.901424	7.129306
5.954648	321.062354	7.134310
5.903970	321.904604	7.139315
5.619922	339.725169	7.144320
5.569380	333.007160	7.149325
5.966087	316.112145	7.154330
5.689852	334.881695	7.159334
6.078603	314.376667	7.164339
6.069411	323.328076	7.169344
5.720734	301.292078	7.174349
5.912701	324.167525	7.179354
5.717296	314.450378	7.184358
5.747664	315.886909	7.189363
5.651245	324.018166	7.194368
5.468512	325.788130	7.199373
6.345661	313.635565	7.204378
5.723325	337.653992	7.209382
5.795698	316.685906	7.214387
5.625589	328.737899	7.219392
5.794680	331.291489	7.224397
5.768136	346.712791	7.229402
5.972021	349.294569	7.234406
5.948733	328.135804	7.239411
5.849282	336.064945	7.244416
5.479546	327.716052	7.249421
6.175202	350.798720	7.254426
5.908683	339.181891	7.259430
5.720785	318.090494	7.264435
6.060260	331.327980	7.269440
5.910106	315.064923	7.274445
5.804136	315.608724	7.279450
5.485635	333.524155	7.284454
6.174999	333.534228	7.289459
5.960450	338.756038	7.294464
6.001694	328.510377	7.299469
5.824672	330.258583	7.304474
5.911641	319.781143	7.309478
6.008201	331.214242	7.314483
5.872761	324.942643	7.319488
5.986441	325.780815	7.324493
5.808149	322.420022	7.329498
5.590577	318.158351	7.334502
5.565497	317.297346	7.339507
5.546016	333.206961	7.344512
5.975224	338.992799	7.349517
5.955800	341.708748	7.354522
6.009382	335.464504	7.359526
6.330766	322.409204	7.364531
6.100962	328.368859	7.369536
5.937841	331.432614	7.374541
6.114523	320.564989	7.379546
5.864915	326.482242	7.384550
5.788540	319.586797	7.389555
6.118947	330.260818	7.394560
5.845706	315.084298	7.399565
5.917556	323.997652	7.404570
5.728884	311.750143	7.409574
5.874015	333.343120	7.414579
5.845395	323.461579	7.419584
5.744175	327.996904	7.424589
5.739636	322.545738	7.429594
5.981696	309.481560	7.434598
6.107022	319.205842	7.439603
5.902770	322.573227	7.444608
5.770907	325.266815	7.449613
5.693678	321.584200	7.454618
5.786553	322.616399	7.459622
5.859987	320.499396	7.464627
5.982516	310.805076	7.469632
5.782791	322.977970	7.474637
5.833425	314.167485	7.479642
5.743387	324.137680	7.484646
5.820167	313.754362	7.489651
5.713549	317.518060	7.494656
5.468296	328.025007	7.499661
5.871334	310.807259	7.504666
5.789266	331.077418	7.509670
5.836730	311.407726	7.514675
5.739204	332.403338	7.519680
5.994358	319.959262	7.524685
5.886984	315.277683	7.529690
6.106718	325.491645	7.534694
6.337451	327.992530	7.539699
6.033346	326.971954	7.544704
5.943925	329.933266	7.549709
6.150579	315.851848	7.554714
6.049761	324.253538	7.559718
6.235271	307.682772	7.564723
6.181853	326.742904	7.569728
5.479957	303.801479	7.574733
5.706218	316.592041	7.579738
5.513521	321.314032	7.584742
6.144172	312.142723	7.589747
5.987774	320.363697	7.594752
5.657738	315.798033	7.599757
6.179374	308.770519	7.604762
5.648968	320.411496	7.609766
5.994392	312.807498	7.614771
5.807725	330.448301	7.619776
5.988286	321.696245	7.624781
5.618772	311.733137	7.629786
5.627746	328.644161	7.634790
5.885200	312.073634	7.639795
5.887348	331.014891	7.644800
5.791661	326.847902	7.649805
5.766237	316.279440	7.654810
5.824686	331.431081	7.659814
6.074515	314.587964	7.664819
5.712525	332.224203	7.669824
5.923728	332.985885	7.674829
5.923212	332.627972	7.679834
5.548924	324.783533	7.684838
5.936815	316.449026	7.689843
6.015418	332.392840	7.694848
5.907744	318.577336	7.699853
5.986111	318.895349	7.704858
5.658385	326.492475	7.709862
5.903807	304.178947	7.714867
6.003655	328.851118	7.719872
5.815829	319.796917	7.724877
5.966040	321.226664	7.729882
5.758706	323.190493	7.734886
5.933734	326.017344	7.739891
5.745791	332.485817	7.744896
5.585037	326.529737	7.749901
6.031398	323.907381	7.754906
5.507560	336.466492	7.759910
5.833294	317.457820	7.764915
5.790794	347.466659	7.769920
5.860119	321.205284	7.774925
6.187615	332.134301	7.779930
5.559816	332.785650	7.784934
6.084803	331.869055	7.789939
5.872590	327.797973	7.794944
5.804847	333.717530	7.799949
6.007840	336.049773	7.804954
5.533390	330.042248	7.809958
5.991120	327.775713	7.814963
5.816169	332.140528	7.819968
5.881248	322.542506	7.824973
6.035723	323.265816	7.829978
5.577574	326.762466	7.834982
5.852039	333.009112	7.839987
5.836232	342.072703	7.844992
5.695293	323.674836	7.849997
5.600115	335.999546	7.855002
5.712946	334.926442	7.860006
5.733410	328.352861	7.865011
5.688325	328.712189	7.870016
5.796613	325.571273	7.875021
5.985740	334.209850	7.880026
5.640986	327.010525	7.885030
5.842347	333.414168	7.890035
5.826851	330.498108	7.895040
5.879481	322.820563	7.900045
5.860066	326.162137	7.905050
5.458077	336.634818	7.910054
5.809559	325.284419	7.915059
6.164904	329.181501	7.920064
5.944960	317.964016	7.925069
6.011496	317.987545	7.930074
5.755829	329.248804	7.935078
6.149493	320.159863	7.940083
6.122042	333.759460	7.945088
5.949505	333.507514	7.950093
6.000857	322.969863	7.955098
5.814306	331.485854	7.960102
6.034325	325.923392	7.965107
5.919330	334.388395	7.970112
6.072760	340.209747	7.975117
6.128434	326.321664	7.980122
5.907401	334.145985	7.985139
6.018648	325.169538	7.990157
5.816023	325.910597	7.995174
5.857017	333.460021	8.000192
5.884899	319.744288	8.005210
5.765309	337.839773	8.010227
6.027850	335.900372	8.015245
6.173160	331.749291	8.020262
5.569474	338.161324	8.025280
5.946413	323.594231	8.030298
5.981991	328.509675	8.035315
5.886222	333.150259	8.040333
5.986402	319.577651	8.045350
5.513247	333.240334	8.050368
5.894452	314.440785	8.055386
5.911174	330.387672	8.060403
6.017430	330.566905	8.065421
6.051421	330.234118	8.070438
6.082545	319.578488	8.075456
6.116694	320.918914	8.080474
5.794626	321.205438	8.085491
6.057752	321.886941	8.090509
5.981165	323.611311	8.095526
5.562808	326.944277	8.100544
5.747425	318.398987	8.105562
5.922209	333.680176	8.110579
6.034502	323.435909	8.115597
5.819942	333.013217	8.120614
5.614764	325.505587	8.125632
6.076794	322.946478	8.130650
5.812817	329.916364	8.135667
5.648606	329.528561	8.140685
5.877762	330.982290	8.145702
5.756244	332.548779	8.150720
6.110870	328.512671	8.155738
5.545997	329.046841	8.160755
6.068003	337.647454	8.165773
6.281731	332.186324	8.170790
6.021688	338.296065	8.175808
6.397420	343.413591	8.180826
6.229193	324.559695	8.185843
6.400664	339.440568	8.190861
6.233076	330.139046	8.195878
5.934621	330.679469	8.200896
5.941907	323.298197	8.205914
6.096994	328.567208	8.210931
6.160829	333.076622	8.215949
6.006435	323.871812	8.220966
5.892247	323.898456	8.225984
6.003765	335.235628	8.231002
6.104179	335.339274	8.236019
5.844776	333.465960	8.241037
6.027673	339.642913	8.246054
5.825353	330.356282	8.251072
5.867760	348.200071	8.256090
6.172644	353.209068	8.261107
6.510224	365.754413	8.266125
6.668203	352.931359	8.271142
5.866106	339.515424	8.276160
6.188101	342.513502	8.281178
5.826327	334.087431	8.286195
6.148227	343.606296	8.291213
6.515627	346.999808	8.296230
6.376921	343.997905	8.301248
6.230683	336.466655	8.306266
5.712821	337.833073	8.311283
5.919404	343.515899	8.316301
6.190488	359.560208	8.321318
6.312497	357.553996	8.326336
6.534223	360.062986	8.331354
6.390148	353.716662	8.336371
5.769852	360.105374	8.341389
6.406962	349.908078	8.346406
6.316483	372.361623	8.351424
6.548860	352.992599	8.356442
6.042605	350.801716	8.361459
5.847394	351.148749	8.366477
6.400407	347.206782	8.371494
6.196945	363.245292	8.376512
6.299064	359.169925	8.381530
6.535522	361.995976	8.386547
6.220332	365.571570	8.391565
6.205818	358.060851	8.396582
5.950350	356.282919	8.401600
6.453580	361.448554	8.406618
6.511964	366.244624	8.411635
6.210167	365.789033	8.416653
6.356598	356.432746	8.421670
6.227038	369.546396	8.426688
6.377361	355.887047	8.431706
6.367605	359.341809	8.436723
6.221175	353.377262	8.441741
6.353747	357.047705	8.446758
6.300174	360.569534	8.451776
6.406479	352.703415	8.456794
6.364085	363.522104	8.461811
6.259210	360.277175	8.466829
6.596678	360.876729	8.471846
6.581799	366.673504	8.476864
6.408292	356.774000	8.481882
6.379532	359.369254	8.486899
6.146639	364.519378	8.491917
6.259459	360.810936	8.496934
6.129770	363.278720	8.501952
6.620836	373.482928	8.506970
6.396660	366.061563	8.511987
6.463848	359.433347	8.517005
6.746078	368.157634	8.522022
6.379800	373.251184	8.527040
6.387585	372.766373	8.532058
6.170992	366.292994	8.537075
6.397738	387.340091	8.542093
6.254795	367.164423	8.547110
6.345386	370.670695	8.552128
6.409479	371.281874	8.557146
6.327181	365.397348	8.562163
6.234093	378.730406	8.567181
6.329043	360.966214	8.572199
5.842843	384.827214	8.577216
6.172158	365.892518	8.582234
6.803578	380.260436	8.587251
6.257287	357.738737	8.592269
6.919723	369.116642	8.597287
6.625164	372.998583	8.602304
6.413714	369.571715	8.607322
6.546922	365.583702	8.612339
6.433128	384.461919	8.617357
6.790506	375.620111	8.622375
6.541675	384.829697	8.627392
6.595530	372.894060	8.632410
6.466753	373.022201	8.637427
6.292757	372.792860	8.642445
6.510788	363.362056	8.647463
6.655242	350.625861	8.652480
6.365328	371.384510	8.657498
6.294184	369.963308	8.662515
6.588225	377.053041	8.667533
6.566311	380.754531	8.672551
6.803466	408.352215	8.677568
6.718301	394.693472	8.682586
6.820526	367.820114	8.687603
6.872936	379.117494	8.692621
6.827801	374.000718	8.697639
6.316427	374.462188	8.702656
6.589493	378.896006	8.707674
6.814064	371.355707	8.712691
6.608473	378.501543	8.717709
6.800289	368.296549	8.722727
6.406350	373.530558	8.727744
6.425135	368.177693	8.732762
6.401390	368.914578	8.737779
6.698027	381.637324	8.742797
6.827785	378.093551	8.747815
6.668165	365.965901	8.752832
6.683021	359.870396	8.757850
6.750534	362.314937	8.762867
6.684195	370.512056	8.767885
6.440147	372.474874	8.772903
6.777279	382.829493	8.777920
6.922907	381.704753	8.782938
6.593446	372.466560	8.787955
7.046517	379.338138	8.792973
6.954561	361.303345	8.797991
6.595025	361.281781	8.803008
6.593418	361.317273	8.808026
6.819861	357.317592	8.813043
6.758378	370.273380	8.818061
6.698129	363.823461	8.823079
6.600975	361.634337	8.828096
6.710165	386.385639	8.833114
6.563118	381.353399	8.838131
6.742069	385.539166	8.843149
7.011116	392.876276	8.848167
6.872701	384.969405	8.853184
6.595461	401.510462	8.858202
6.835177	389.515168	8.863219
7.244851	385.935563	8.868237
6.830806	379.861438	8.873255
6.695692	373.967827	8.878272
6.793545	384.009335	8.883290
7.014757	397.820633	8.888307
6.893860	396.532320	8.893325
7.038121	384.087680	8.898343
6.734028	374.673886	8.903360
6.739248	369.468103	8.908378
6.819033	367.666252	8.913395
6.825198	385.898742	8.918413
7.005259	381.069162	8.923431
7.068743	400.458598	8.928448
6.706202	385.540265	8.933466
7.017971	383.945575	8.938483
6.907993	391.621623	8.943501
7.056706	384.548941	8.948519
6.589995	373.138187	8.953536
6.825137	381.784855	8.958554
7.109268	393.687469	8.963571
6.801366	392.596354	8.968589
6.805507	395.719786	8.973607
7.096765	384.390393	8.978624
7.088853	394.616171	8.983642
7.272538	395.136839	8.988659
6.570118	380.236208	8.993677
6.671822	388.588191	8.998695
6.985535	382.454012	9.003712
6.878380	392.867106	9.008730
7.181373	393.409384	9.013747
6.803580	399.687091	9.018765
6.959219	387.539893	9.023783
6.893490	394.175359	9.028800
6.637599	389.530685	9.033818
6.846550	390.669935	9.038835
6.896759	404.982889	9.043853
6.652001	398.455703	9.048871
6.998079	385.371285	9.053888
6.953614	401.558805	9.058906
6.845656	398.202795	9.063923
6.824170	397.429596	9.068941
7.070658	417.264364	9.073959
7.229435	428.421303	9.078976
6.977399	420.166662	9.083994
7.237348	437.461066	9.089011
7.131536	418.099734	9.094029
7.168158	402.301571	9.099047
7.012771	404.486681	9.104064
6.962600	410.506566	9.109082
7.611759	411.393394	9.114099
6.931712	412.651521	9.119117
7.172682	403.859044	9.124135
7.109477	400.929865	9.129152
6.936519	390.518680	9.134170
7.167521	410.857727	9.139187
7.529657	417.767474	9.144205
7.335895	396.786418	9.149223
7.511318	400.579577	9.154240
6.957295	400.611999	9.159258
7.184980	399.513154	9.164275
6.881210	393.117341	9.169293
7.223037	396.678627	9.174311
7.004341	389.562755	9.179328
6.920079	402.915039	9.184346
7.136878	411.932663	9.189363
6.846050	427.380238	9.194381
7.099351	421.904666	9.199399
7.364912	433.885949	9.204416
7.439466	433.314040	9.209434
7.711440	419.955012	9.214451
7.876107	424.102216	9.219469
7.422008	403.145088	9.224487
7.210066	399.188621	9.229504
7.079545	406.105196	9.234522
7.232468	392.971220	9.239539
7.303088	395.490428	9.244557
7.518488	391.641931	9.249575
7.286470	398.972310	9.254592
7.480135	397.126642	9.259610
7.513075	397.429379	9.264627
7.133270	406.754298	9.269645
6.975965	385.699929	9.274663
7.132535	395.099340	9.279680
7.041806	405.177144	9.284698
7.485620	404.393959	9.289715
7.357293	428.072983	9.294733
7.288279	422.786564	9.299751
7.797607	419.991931	9.304768
7.306709	402.181440	9.309786
7.508372	410.856584	9.314803
7.200053	407.844128	9.319821
7.248164	399.828395	9.324839
7.723869	412.904733	9.329856
7.317004	416.994070	9.334874
7.382711	400.174263	9.339891
7.230844	403.721497	9.344909
7.218606	411.573276	9.349927
7.662725	431.374318	9.354944
7.697975	429.452493	9.359962
7.432912	399.164475	9.364979
7.235800	402.071731	9.369997
7.402228	403.870483	9.375015
7.795725	411.410003	9.380032
7.243611	402.489809	9.385050
7.313970	408.275268	9.390067
7.602860	420.940387	9.395085
7.780973	416.511793	9.400103
7.736822	412.135282	9.405120
7.445108	404.689736	9.410138
7.481590	398.351831	9.415155
7.131437	391.447098	9.420173
7.354751	410.043911	9.425191
7.253791	408.519593	9.430208
7.130027	424.330488	9.435226
7.632022	420.528886	9.440243
7.530169	417.488015	9.445261
7.793891	423.966220	9.450279
7.880170	413.600933	9.455296
7.637822	419.362702	9.460314
7.479077	413.241846	9.465331
7.482029	412.747599	9.470349
7.300881	433.874959	9.475367
7.649372	418.731540	9.480384
7.547401	414.593653	9.485402
7.635469	418.736592	9.490419
7.536436	413.018054	9.495437
7.708867	420.388265	9.500455
7.949106	431.835595	9.505472
7.562800	426.457359	9.510490
7.407758	426.843609	9.515507
7.509547	433.791371	9.520525
7.835888	415.859679	9.525543
7.967854	426.189194	9.530560
7.441169	419.872719	9.535578
7.444619	424.681820	9.540595
7.296821	421.744972	9.545613
7.385398	434.044891	9.550631
7.579367	416.752717	9.555648
7.402491	439.060052	9.560666
7.831354	439.248848	9.565683
7.854475	433.703171	9.570701
7.830322	431.231379	9.575719
7.817952	421.747206	9.580736
7.535487	428.984585	9.585754
7.648873	436.856846	9.590771
7.775672	425.679959	9.595789
7.476764	432.004272	9.600807
7.840751	431.007668	9.605824
7.425014	423.987908	9.610842
7.720816	447.544229	9.615859
7.774522	448.587618	9.620877
7.799029	457.523596	9.625895
8.239886	449.426301	9.630912
7.955306	442.968651	9.635930
7.545507	428.227133	9.640947
8.004026	424.297614	9.645965
7.819196	432.509822	9.650983
7.870028	417.820206	9.656000
7.812991	443.808180	9.661018
8.179783	426.764028	9.666035
7.792696	426.395344	9.671053
7.643539	424.241569	9.676071
7.916551	425.890955	9.681088
7.685357	423.999487	9.686106
7.584035	423.023303	9.691123
8.012532	440.985921	9.696141
8.002398	449.158739	9.701159
8.162673	447.845209	9.706176
7.940059	436.141675	9.711194
7.716207	434.605488	9.716211
7.487256	430.273190	9.721229
7.435069	441.897758	9.726247
7.819821	451.528316	9.731264
8.089433	459.603151	9.736282
8.462856	454.195977	9.741299
8.120590	458.934702	9.746317
7.977300	458.093072	9.751335
8.439993	451.348286	9.756352
8.246827	441.897816	9.761370
7.933055	435.987065	9.766387
8.333969	432.291214	9.771405
7.762324	434.150546	9.776423
7.894965	422.411930	9.781440
7.749631	442.843618	9.786458
7.721226	431.190549	9.791475
8.245132	450.312476	9.796493
7.800885	451.413756	9.801511
8.246776	471.719339	9.806528
8.188755	453.603456	9.811546
8.047741	476.097878	9.816563
8.208545	458.995434	9.821581
7.762624	460.084298	9.826599
8.003844	462.392893	9.831616
7.982399	455.816969	9.836634
7.836741	463.985526	9.841651
7.982192	457.710669	9.846669
7.911741	462.890361	9.851687
8.221135	457.562647	9.856704
8.107814	455.317339	9.861722
8.028459	463.466279	9.866739
8.101826	463.736359	9.871757
7.838834	462.195912	9.876775
8.215471	459.251694	9.881792
8.359371	458.195522	9.886810
8.179126	453.402636	9.891827
8.251607	450.551882	9.896845
7.792035	458.292331	9.901863
8.242343	458.833586	9.906880
8.410547	448.693841	9.911898
8.180226	464.610258	9.916915
8.405015	451.959002	9.921933
7.876818	472.802233	9.926951
8.141857	456.240484	9.931968
8.367129	462.307461	9.936986
8.105941	457.394328	9.942003
8.631691	445.345224	9.947021
8.153092	458.318558	9.952039
8.075887	444.716805	9.957056
8.269298	459.199299	9.962074
8.266994	448.812318	9.967091
8.291100	457.718351	9.972109
8.078343	464.241076	9.977127
8.229139	453.375275	9.982144
8.082196	469.228915	9.987162
8.132739	461.992748	9.992179
8.742542	484.570916	9.997197
8.265991	474.670938	10.002215
8.194805	453.543008	10.007232
8.233754	462.279905	10.012250
8.569231	481.523734	10.017267
8.458844	454.743020	10.022285
8.328012	460.217258	10.027303
8.242697	471.018910	10.032320
8.482685	456.381830	10.037338
8.564931	463.607266	10.042355
8.500157	451.576343	10.047373
8.565227	465.694333	10.052391
8.448890	449.204868	10.057408
8.156977	463.105453	10.062426
8.160175	461.280924	10.067443
8.583800	463.351066	10.072461
8.451335	468.108649	10.077479
8.469210	463.179406	10.082496
8.630038	453.374939	10.087514
8.570733	453.463949	10.092531
8.577874	464.478404	10.097549
8.667802	449.542008	10.102567
8.513992	454.755645	10.107584
8.429941	441.322500	10.112602
8.082803	460.777020	10.117619
8.248111	455.982326	10.122637
8.340162	470.352188	10.127655
8.405363	471.516283	10.132672
8.660331	483.925717	10.137690
8.719925	484.658182	10.142707
8.505892	486.417978	10.147725
8.710232	485.936694	10.152743
8.629348	490.343433	10.157760
8.930358	486.560860	10.162778
8.475510	476.301292	10.167795
8.594030	477.031398	10.172813
8.430156	474.855250	10.177831
8.597755	476.474046	10.182848
8.759598	482.988303	10.187866
8.547405	476.220529	10.192883
8.571366	491.085388	10.197901
8.749349	491.958185	10.202919
9.002671	474.018811	10.207936
8.662510	480.668968	10.212954
8.420308	462.292844	10.217971
8.938926	468.703361	10.222989
8.653858	468.723905	10.228007
8.711377	468.455711	10.233024
8.640533	468.171732	10.238042
8.556669	483.470825	10.243059
9.062235	478.728720	10.248077
8.800456	470.246195	10.253095
8.323796	453.815978	10.258112
9.041735	470.705984	10.263130
8.717447	457.132361	10.268147
8.619437	470.907233	10.273165
8.904516	468.303841	10.278183
8.975665	483.732784	10.283200
8.641422	455.269265	10.288218
8.488027	471.014260	10.293235
8.751486	474.384339	10.298253
9.012892	494.259153	10.303271
8.833802	488.989721	10.308288
8.653729	500.515520	10.313306
8.805008	504.223250	10.318323
9.009297	496.805205	10.323341
8.945268	489.065662	10.328359
8.954770	502.242935	10.333376
9.126905	470.205128	10.338394
8.612087	474.602201	10.343411
8.599209	466.206955	10.348429
8.798501	493.781040	10.353447
8.861215	481.496018	10.358464
9.009483	477.648459	10.363482
8.885253	478.858030	10.368499
8.549534	487.067160	10.373517
8.948943	492.667303	10.378535
8.628763	489.769162	10.383552
9.227395	495.156805	10.388570
8.845067	491.719972	10.393587
8.970895	486.161435	10.398605
8.953471	504.102967	10.403623
8.702392	499.497611	10.408640
9.213218	492.524342	10.413658
8.876502	491.721269	10.418675
8.955872	493.738693	10.423693
9.104065	483.629095	10.428711
8.944265	492.815275	10.433728
9.149798	486.064758	10.438746
8.746361	499.943071	10.443763
8.740708	480.281425	10.448781
8.836449	499.902205	10.453799
8.704487	490.187526	10.458816
8.718307	500.329195	10.463834
8.710363	489.241245	10.468851
9.206403	510.411579	10.473869
9.099747	512.096266	10.478887
9.250136	521.934649	10.483904
9.395733	497.264609	10.488922
8.886388	497.831918	10.493939
8.911693	479.731359	10.498957
9.312191	497.712349	10.503975
9.100957	507.346976	10.508992
9.131901	503.021299	10.514010
9.163840	495.914336	10.519027
8.947707	495.115836	10.524045
9.163251	510.820367	10.529063
9.480884	500.028113	10.534080
9.334413	502.729140	10.539098
9.036111	496.973444	10.544115
9.202224	510.090501	10.549133
9.229765	501.037948	10.554151
9.105749	507.024319	10.559168
9.180335	513.738982	10.564186
9.055818	509.961686	10.569203
9.294318	507.466647	10.574221
9.349075	514.570996	10.579239
9.318712	524.377852	10.584256
9.459790	509.104589	10.589274
9.285576	527.376798	10.594291
9.110236	518.020356	10.599309
9.666071	510.452893	10.604327
9.094367	509.206207	10.609344
9.381926	498.702213	10.614362
9.349057	507.522638	10.619379
9.483633	505.608792	10.624397
9.090657	507.144098	10.629415
9.147187	504.866581	10.634432
9.439980	504.287630	10.639450
9.229781	503.426453	10.644467
9.479268	521.909757	10.649485
9.541476	507.521240	10.654503
9.498328	514.697561	10.659520
9.529573	521.713994	10.664538
9.457636	521.493465	10.669555
9.120265	518.493562	10.674573
9.405382	515.196154	10.679591
9.338326	511.724432	10.684608
9.427404	519.757697	10.689626
9.272183	506.701412	10.694643
9.401584	515.817475	10.699661
9.374607	501.362229	10.704679
9.509993	520.860571	10.709696
9.656962	503.677809	10.714714
9.406673	519.554976	10.719731
9.411360	511.967702	10.724749
9.695768	498.267175	10.729767
9.495766	514.797065	10.734784
9.414889	509.627899	10.739802
9.456057	515.320217	10.744819
9.448893	517.399177	10.749837
10.021066	516.006549	10.754855
9.517772	515.374763	10.759872
9.608075	522.510042	10.764890
9.331864	508.470581	10.769907
9.112372	519.776199	10.774925
9.409169	507.709979	10.779943
9.362709	516.078055	10.784960
9.614578	508.314143	10.789978
9.585594	524.321035	10.794995
9.315610	520.616189	10.800013
9.476889	508.853782	10.805031
9.091719	512.591918	10.810048
9.299698	519.671341	10.815066
9.748896	539.116566	10.820083
9.677320	538.667693	10.825101
9.865047	539.444519	10.830119
9.553021	543.639540	10.835136
9.917594	541.121889	10.840154
9.760046	545.940024	10.845171
9.776599	544.926146	10.850189
10.322384	543.340883	10.855207
9.896283	534.798693	10.860224
9.810662	516.728623	10.865242
9.760212	515.836223	10.870259
9.733700	518.850802	10.875277
9.813882	506.565824	10.880295
9.500749	513.712275	10.885312
9.672246	509.746039	10.890330
9.893161	524.647555	10.895347
9.716305	530.341274	10.900365
9.729986	532.404491	10.905383
9.674880	545.581262	10.910400
10.023825	541.871834	10.915418
9.926509	556.826662	10.920435
9.731735	550.449670	10.925453
9.796609	551.791139	10.930471
9.881349	555.238594	10.935488
10.066656	548.841985	10.940506
10.106339	559.016908	10.945523
9.886858	543.201886	10.950541
9.691840	536.236517	10.955559
9.951751	548.173365	10.960576
10.181195	540.588194	10.965594
10.000472	543.212332	10.970611
9.889354	534.757714	10.975629
10.106940	546.733043	10.980647
9.505465	547.545832	10.985664
9.792605	553.620333	10.990682
9.879147	542.539361	10.995699
9.773380	562.964573	11.000717
10.043818	551.618424	11.005735
10.122405	552.589420	11.010752
9.946491	548.247537	11.015770
9.979839	554.947188	11.020787
9.990010	561.051425	11.025805
10.254913	542.786524	11.030823
9.933886	554.241983	11.035840
10.289659	539.549380	11.040858
10.303048	550.982533	11.045875
10.034105	546.973949	11.050893
9.990210	544.122041	11.055911
10.234899	547.555951	11.060928
9.996450	539.754484	11.065946
10.035835	552.293767	11.070963
9.897565	535.874547	11.075981
10.101188	535.524643	11.080999
10.051291	539.214954	11.086016
9.865675	544.470679	11.091034
9.925189	549.788624	11.096051
10.238475	554.193018	11.101069
9.994725	556.336370	11.106087
9.965943	541.425800	11.111104
9.944012	551.849516	11.116122
9.976747	547.680476	11.121139
10.038669	555.727006	11.126157
10.190238	569.519662	11.131175
10.111761	568.046321	11.136192
10.511190	576.490307	11.141210
10.679527	571.254252	11.146227
10.285265	553.371723	11.151245
10.302840	562.288736	11.156263
10.384588	551.774636	11.161280
10.189069	550.351733	11.166298
10.256734	547.146047	11.171315
10.105044	556.799006	11.176333
10.540522	560.046410	11.181351
10.294074	554.798321	11.186368
10.408161	573.406201	11.191386
10.458260	544.205462	11.196403
10.116093	550.700510	11.201421
10.479253	557.978850	11.206439
10.306464	564.525123	11.211456
10.453758	573.952451	11.216474
10.463252	571.198477	11.221491
10.656953	566.115178	11.226509
10.690585	557.398697	11.231527
10.402295	553.369103	11.236544
10.006978	546.332333	11.241562
10.430921	554.940616	11.246579
10.314226	577.893246	11.251597
10.249949	574.354927	11.256615
10.502671	586.343668	11.261632
10.566354	569.721201	11.266650
10.677292	573.014174	11.271667
10.443434	580.575490	11.276685
10.839820	567.165564	11.281703
10.583791	574.838387	11.286720
10.390834	581.969339	11.291738
10.780285	564.079588	11.296755
10.568218	570.191530	11.301773
10.503776	550.641942	11.306791
10.561004	568.990193	11.311808
10.445538	566.165164	11.316826
10.513108	569.800449	11.321843
10.492568	570.143219	11.326861
10.723056	564.803318	11.331879
10.602681	571.011690	11.336896
10.676884	564.915447	11.341914
10.862388	551.525134	11.346931
10.479579	573.363587	11.351949
10.399455	559.081985	11.356967
10.521505	562.437177	11.361984
10.478759	572.510409	11.367002
10.733829	566.913560	11.372019
10.274740	574.552931	11.377037
10.475118	565.728990	11.382055
10.542420	564.986963	11.387072
10.792404	573.471684	11.392090
10.694883	560.039086	11.397107
10.542492	562.462930	11.402125
10.818823	572.162159	11.407143
10.753675	570.580837	11.412160
10.551122	568.017574	11.417178
10.803475	562.390868	11.422195
10.571056	576.061508	11.427213
10.775148	577.553940	11.432231
10.586924	598.239610	11.437248
10.879393	590.502009	11.442266
10.505548	600.354362	11.447283
10.674718	608.523217	11.452301
10.765366	590.901851	11.457319
11.004609	614.068474	11.462336
10.981737	601.363856	11.467354
11.029326	601.792290	11.472371
10.927972	605.327779	11.477389
10.861892	603.565456	11.482407
11.011055	596.132758	11.487424
11.080395	610.477281	11.492442
11.044714	598.687332	11.497459
10.794679	601.741130	11.502477
11.203870	602.411693	11.507495
11.085232	589.407445	11.512512
11.170933	607.022295	11.517530
11.399706	585.787932	11.522547
11.298274	583.701621	11.527565
10.783368	575.469082	11.532583
11.380201	567.010213	11.537600
10.932153	567.166028	11.542618
10.934056	567.304553	11.547635
10.705617	562.189865	11.552653
10.671729	584.670382	11.557671
11.091398	577.754746	11.562688
11.073396	605.183299	11.567706
11.257953	596.097950	11.572723
10.961043	596.198579	11.577741
10.865755	593.412424	11.582759
11.109802	589.849026	11.587776
10.887705	602.866781	11.592794
10.938723	583.433368	11.597811
10.975787	598.852413	11.602829
10.769385	590.959722	11.607847
11.196868	598.032918	11.612864
10.988715	590.560974	11.617882
11.259196	592.861999	11.622899
11.090005	613.724416	11.627917
11.000112	596.386947	11.632935
11.037537	609.026869	11.637952
11.350620	621.713445	11.642970
11.412111	624.035729	11.647987
11.211023	617.976301	11.653005
11.535501	615.310975	11.658023
11.353654	604.330302	11.663040
11.017376	602.220316	11.668058
11.296407	597.944631	11.673075
11.310716	618.505937	11.678093
11.374612	627.389847	11.683111
11.707804	617.898824	11.688128
11.359891	621.299322	11.693146
11.479205	617.322987	11.698163
11.397884	606.765246	11.703181
11.462815	613.442779	11.708199
11.387122	599.778942	11.713216
11.597384	604.041167	11.718234
11.480353	587.643571	11.723251
11.441525	601.985791	11.728269
11.284101	600.235710	11.733287
11.196174	597.775513	11.738304
11.248435	598.459405	11.743322
11.257132	604.883995	11.748339
11.507569	613.960828	11.753357
11.659565	621.686978	11.758375
11.731925	626.035664	11.763392
11.358783	618.239590	11.768410
11.165888	610.288373	11.773427
11.554298	608.009226	11.778445
11.530709	619.667184	11.783463
11.770721	615.523205	11.788480
11.649018	645.105893	11.793498
11.847571	612.584517	11.798515
11.119233	617.797120	11.803533
11.571670	619.267801	11.808551
11.825229	627.759145	11.813568
11.836048	625.867213	11.818586
11.623305	612.593632	11.823603
11.309586	602.768701	11.828621
11.621856	602.338554	11.833639
11.724737	618.158246	11.838656
11.530777	632.864230	11.843674
11.669450	640.689317	11.848691
11.688122	629.449465	11.853709
11.733470	636.781744	11.858727
11.638762	628.331938	11.863744
11.798270	624.358700	11.868762
11.913470	633.629206	11.873779
11.880675	626.076310	11.878797
11.601443	630.320547	11.883815
11.744167	630.093668	11.888832
11.648988	637.026448	11.893850
11.849934	635.633365	11.898867
11.764337	631.555001	11.903885
11.698021	641.629221	11.908903
11.902123	634.180440	11.913920
11.801805	633.274725	11.918938
11.704153	624.183454	11.923955
11.922407	644.715419	11.928973
11.722587	647.574461	11.933991
11.812358	619.167302	11.939008
12.007458	644.169712	11.944026
12.009989	633.152644	11.949043
12.116483	626.598503	11.954061
11.805980	636.770835	11.959079
11.891461	634.632766	11.964096
11.884191	633.044529	11.969114
11.955552	628.385256	11.974131
11.681425	632.229544	11.979149
11.941792	624.028360	11.984167
12.298872	630.639612	11.989184
11.918402	636.495136	11.994202
12.165680	621.022960	11.999219
12.027577	634.640083	12.004237
12.165335	632.372050	12.009255
12.101587	643.974081	12.014272
11.986015	646.092424	12.019290
11.885810	638.637844	12.024307
12.250061	643.948657	12.029325
11.760031	628.950689	12.034343
12.049791	638.394560	12.039360
11.808581	639.235489	12.044378
11.494012	630.698034	12.049395
11.938478	626.390967	12.054413
11.983654	649.608313	12.059431
12.341411	640.843238	12.064448
12.105638	652.897411	12.069466
12.192209	649.745355	12.074483
11.993582	646.014319	12.079501
12.019692	658.897918	12.084519
12.319620	653.254462	12.089536
12.003383	657.447554	12.094554
12.317636	671.870033	12.099571
12.461831	666.545833	12.104589
12.076414	671.606434	12.109607
12.351229	649.167545	12.114624
12.520310	671.503948	12.119642
12.282637	664.753782	12.124659
12.695812	663.537772	12.129677
12.318036	658.614419	12.134695
12.460000	636.582245	12.139712
12.317561	631.258983	12.144730
11.996695	631.623835	12.149747
12.217971	647.257992	12.154765
12.045232	671.581965	12.159783
12.561560	658.836897	12.164800
12.578052	665.888208	12.169818
12.483794	676.526468	12.174835
12.641939	677.169053	12.179853
12.313191	685.010403	12.184871
12.199072	660.692781	12.189888
12.350529	666.048412	12.194906
12.248084	678.887936	12.199923
12.523364	667.862372	12.204941
12.210010	674.699567	12.209959
12.524228	656.334181	12.214976
12.372071	679.126923	12.219994
12.498276	672.043266	12.225011
12.562863	681.473996	12.230029
12.559700	679.404297	12.235047
12.620002	672.687244	12.240064
12.546183	667.982580	12.245082
12.336857	660.371364	12.250099
12.582756	674.094111	12.255117
12.417546	664.370843	12.260135
12.524876	662.289675	12.265152
12.519131	674.653987	12.270170
12.553500	676.619833	12.275187
12.703310	671.077241	12.280205
12.475768	677.356405	12.285223
12.367373	674.339391	12.290240
12.593990	691.448698	12.295258
12.541878	680.956336	12.300275
12.989048	692.963505	12.305293
12.852951	697.799495	12.310311
12.765228	688.333021	12.315328
13.207687	700.144962	12.320346
12.875123	681.561028	12.325363
12.849415	676.979872	12.330381
12.542090	685.842214	12.335399
12.715995	667.071377	12.340416
12.903409	684.589902	12.345434
12.690303	674.414527	12.350451
12.909914	677.906829	12.355469
12.807048	669.062489	12.360487
12.961044	683.963904	12.365504
12.913914	671.981649	12.370522
12.885617	674.830357	12.375539
13.010185	670.227911	12.380557
12.670766	666.815138	12.385575
12.942536	673.544909	12.390592
12.977876	700.505390	12.395610
12.907370	682.488714	12.400627
13.287757	681.848443	12.405645
12.919848	683.654847	12.410663
12.847778	673.430581	12.415680
13.068548	681.224017	12.420698
12.949773	683.092075	12.425715
13.203620	653.523783	12.430733
12.842690	690.674117	12.435751
13.014943	678.232583	12.440768
13.419427	693.056793	12.445786
13.005140	671.705612	12.450803
12.781022	666.418271	12.455821
12.978388	679.381037	12.460839
12.906005	683.339596	12.465856
13.081728	681.902954	12.470874
13.121019	690.121852	12.475891
13.319046	682.313123	12.480909
13.184639	684.907885	12.485927
13.372656	681.744469	12.490944
13.348737	688.482178	12.495962
13.196797	680.972758	12.500979
13.027487	674.909826	12.505997
13.150089	681.575398	12.511015
13.088408	688.771985	12.516032
13.135797	688.228664	12.521050
13.141451	694.800803	12.526067
13.220729	674.001053	12.531085
12.958759	701.830336	12.536103
12.604294	679.124631	12.541120
12.958994	684.559839	12.546138
12.830261	694.501238	12.551155
12.971821	697.634297	12.556173
13.166757	705.668763	12.561191
13.284192	720.801788	12.566208
13.346324	713.227453	12.571226
13.115648	729.673691	12.576243
13.194767	715.173650	12.581261
13.066656	728.954910	12.586279
13.258393	728.762733	12.591296
13.489603	723.609222	12.596314
13.390577	726.484290	12.601331
13.711947	723.113345	12.606349
13.295777	715.136094	12.611367
13.524517	722.653699	12.616384
13.440406	704.524708	12.621402
13.305649	712.113598	12.626419
13.353525	717.529168	12.631437
13.433425	724.166785	12.636455
13.671426	725.305098	12.641472
13.521860	720.893670	12.646490
13.482719	715.939230	12.651507
13.648773	716.078476	12.656525
13.344129	714.500113	12.661543
13.532712	723.871510	12.666560
13.867937	733.943883	12.671578
13.557385	728.562073	12.676595
13.963705	721.793326	12.681613
13.868793	711.420192	12.686631
13.584851	715.781637	12.691648
13.981436	709.095289	12.696666
13.613087	727.828744	12.701683
13.968226	717.295818	12.706701
13.746470	710.341086	12.711719
13.932215	714.447102	12.716736
13.926600	700.467245	12.721754
13.695833	713.541827	12.726771
13.721685	703.540665	12.731789
13.939652	710.800959	12.736807
13.582815	711.773864	12.741824
13.716817	701.805802	12.746842
13.619523	711.623051	12.751859
13.489696	699.943243	12.756877
13.718316	710.830844	12.761895
13.886592	711.113189	12.766912
13.512368	708.775072	12.771930
13.643904	729.009556	12.776947
13.681109	731.142318	12.781965
13.700902	744.351653	12.786983
13.999437	733.170762	12.792000
14.222201	739.539367	12.797018
14.094132	742.095503	12.802035
14.333234	737.103142	12.807053
14.092667	743.661578	12.812071
14.114171	735.147736	12.817088
14.461092	721.442386	12.822106
13.755291	723.104884	12.827123
13.780469	703.921194	12.832141
14.092461	729.108605	12.837159
14.181807	743.755379	12.842176
14.493422	728.061395	12.847194
13.865348	727.385080	12.852211
13.989752	710.915374	12.857229
13.835727	723.462751	12.862247
13.895541	728.327972	12.867264
14.272184	732.088451	12.872282
14.101410	752.156742	12.877299
14.109367	733.557207	12.882317
14.157206	749.232725	12.887335
13.861437	743.771223	12.892352
14.391133	737.883124	12.897370
13.937858	744.990950	12.902387
14.294118	737.543343	12.907405
14.380960	731.430775	12.912423
14.248417	747.143580	12.917440
14.170346	738.994330	12.922458
13.844826	760.754210	12.927475
13.934736	742.340380	12.932493
13.923062	756.354029	12.937511
14.250297	733.255440	12.942528
14.118214	748.907950	12.947546
14.050228	757.366308	12.952563
14.601542	761.451872	12.957581
14.562993	773.456227	12.962599
14.249100	771.221880	12.967616
14.462423	760.965249	12.972634
14.571092	781.090717	12.977651
14.538975	777.611193	12.982669
14.498492	763.209591	12.987687
14.149245	753.637615	12.992704
14.213922	769.949084	12.997722
14.299441	773.493186	13.002739
14.647901	772.126783	13.007757
14.813998	786.551519	13.012775
14.633717	789.456755	13.017792
14.722136	781.910908	13.022810
14.912591	778.244443	13.027827
15.103446	766.956354	13.032845
14.995306	746.968380	13.037863
14.372697	754.272359	13.042880
14.520825	739.801922	13.047898
14.571593	749.126541	13.052915
14.441840	745.306068	13.057933
14.658929	730.938780	13.062951
14.409289	756.027566	13.067968
14.563313	739.320415	13.072986
14.888842	764.405772	13.078003
14.769816	762.188815	13.083021
14.966004	746.327519	13.088039
14.238535	753.075944	13.093056
14.758258	763.893630	13.098074
14.978712	775.997077	13.103091
14.648840	774.374760	13.108109
15.086961	769.489029	13.113127
14.600880	774.004928	13.118144
14.793270	760.710218	13.123162
15.040107	774.610118	13.128179
15.165445	758.001069	13.133197
14.929739	736.148261	13.138215
14.357165	745.763246	13.143232
14.639005	741.065219	13.148250
14.918080	772.125121	13.153267
14.845079	767.454043	13.158285
15.514552	770.443588	13.163303
14.881735	768.977019	13.168320
14.866936	772.100017	13.173338
14.996471	772.409430	13.178355
14.897938	782.507369	13.183373
14.923949	770.671078	13.188391
14.679473	784.428716	13.193408
14.779691	776.863210	13.198426
14.950883	769.857681	13.203443
14.866486	790.744210	13.208461
15.131767	778.611251	13.213479
14.929587	787.910588	13.218496
15.125411	774.515128	13.223514
15.236752	786.128577	13.228531
15.071537	770.669808	13.233549
15.291960	775.486558	13.238567
15.177767	777.424423	13.243584
14.955519	775.358248	13.248602
15.259758	766.059272	13.253619
15.026390	782.756046	13.258637
15.177148	771.634775	13.263655
14.762157	773.347914	13.268672
15.168985	771.233767	13.273690
15.322342	772.756842	13.278707
15.006399	781.598130	13.283725
15.346955	784.235152	13.288743
15.293738	805.709802	13.293760
15.444804	781.368139	13.298778
15.592146	796.470614	13.303795
15.160398	790.726822	13.308813
15.080601	786.147979	13.313831
15.277595	808.606216	13.318848
15.193518	806.049409	13.323866
15.366899	803.379502	13.328883
15.442900	808.910898	13.333901
15.892898	802.932528	13.338919
15.540136	802.189357	13.343936
15.538106	805.098496	13.348954
15.538141	794.674584	13.353971
15.345890	800.726761	13.358989
15.662479	796.632956	13.364007
15.372383	805.531290	13.369024
15.547541	795.068203	13.374042
15.635776	805.341735	13.379059
15.208456	803.092081	13.384077
15.382764	812.092561	13.389095
15.412219	801.096900	13.394112
15.545946	792.184656	13.399130
15.815113	807.329690	13.404147
15.909267	807.038806	13.409165
15.683965	798.120063	13.414183
15.684134	798.334054	13.419200
15.764144	796.835287	13.424218
15.753304	794.597002	13.429235
15.547352	792.711451	13.434253
15.687508	792.872001	13.439271
15.503212	794.524581	13.444288
15.661346	811.451000	13.449306
15.585797	788.637242	13.454323
15.691261	801.504305	13.459341
15.806554	802.028518	13.464359
15.450619	796.527838	13.469376
15.537886	793.599399	13.474394
15.739959	807.086657	13.479411
15.723065	819.442300	13.484429
15.912335	817.253401	13.489447
15.700827	827.610826	13.494464
15.819936	824.586394	13.499482
16.265250	829.851600	13.504499
15.865414	831.237322	13.509517
16.065275	822.247810	13.514535
16.070957	834.198065	13.519552
15.947422	830.521978	13.524570
16.268900	824.760655	13.529587
16.038721	842.043431	13.534605
16.252429	831.525732	13.539623
16.071472	818.870281	13.544640
15.750394	815.082393	13.549658
16.026356	804.943989	13.554675
15.646987	834.630241	13.559693
16.311760	820.510751	13.564711
15.906283	824.066243	13.569728
16.412485	826.680227	13.574746
16.375201	818.591205	13.579763
16.559464	833.874870	13.584781
16.427921	817.139060	13.589799
16.179014	819.431491	13.594816
16.233300	816.092462	13.599834
16.098547	802.307923	13.604851
16.147810	829.538112	13.609869
16.400601	816.882517	13.614887
16.295791	825.330073	13.619904
16.255529	823.348354	13.624922
16.732706	818.283166	13.629939
16.080924	821.628048	13.634957
16.313800	818.419503	13.639975
16.417744	821.791423	13.644992
16.395238	823.518522	13.650010
16.632432	825.246589	13.655027
16.385208	823.712551	13.660045
16.060043	810.172804	13.665063
16.105182	820.054456	13.670080
16.023817	830.606658	13.675098
16.656380	818.418579	13.680115
16.401283	831.683849	13.685133
16.482211	831.982206	13.690151
16.392611	818.660150	13.695168
16.460508	841.572042	13.700186
16.402803	825.522465	13.705203
16.408625	823.229861	13.710221
16.607913	840.620652	13.715239
16.364546	817.299288	13.720256
16.160174	828.323965	13.725274
16.615076	820.019188	13.730291
16.392113	845.181152	13.735309
16.589840	847.078203	13.740327
16.630856	848.221133	13.745344
16.857217	859.668226	13.750362
17.263946	847.188395	13.755379
16.848523	847.315105	13.760397
16.624908	829.142306	13.765415
16.704181	829.079119	13.770432
16.590809	830.409923	13.775450
16.838625	835.176507	13.780467
16.840357	852.156469	13.785485
16.799742	856.448024	13.790503
16.970500	856.480812	13.795520
16.596101	850.890963	13.800538
17.146732	844.226332	13.805555
16.934858	857.049059	13.810573
16.850459	832.338162	13.815591
16.721208	832.220089	13.820608
16.507126	847.432724	13.825626
17.186509	858.374644	13.830643
16.992706	855.297810	13.835661
16.998654	853.133987	13.840679
16.806690	865.765364	13.845696
16.930263	848.962684	13.850714
17.344791	854.002632	13.855731
17.235292	863.814591	13.860749
17.298163	856.077335	13.865767
17.357471	834.607314	13.870784
16.869986	832.951309	13.875802
17.046932	819.143877	13.880819
17.176527	844.874090	13.885837
17.201633	846.208480	13.890855
17.388075	840.014661	13.895872
17.053572	833.924256	13.900890
17.054553	828.126255	13.905907
17.050007	854.297541	13.910925
16.904934	847.538092	13.915943
17.231214	860.652302	13.920960
17.203732	866.409897	13.925978
17.219783	864.563712	13.930995
17.231776	853.559312	13.936013
17.148992	858.926859	13.941031
17.158719	851.354721	13.946048
17.207292	865.919666	13.951066
17.002229	842.276388	13.956083
17.199368	871.532752	13.961101
16.865781	848.749077	13.966119
17.299155	861.586083	13.971136
17.744072	867.138795	13.976154
17.375324	863.508046	13.981171
17.209474	861.443265	13.986189
17.527351	885.375651	13.991207
17.667048	878.581919	13.996224
17.583346	898.413626	14.001242
17.717771	858.154287	14.006259
17.468611	865.928628	14.011277
17.410376	869.494935	14.016295
17.750719	865.128848	14.021312
17.650346	878.011985	14.026330
17.599026	860.897410	14.031347
17.490588	871.334165	14.036365
17.434812	880.740334	14.041383
17.621748	882.090294	14.046400
17.872486	894.549468	14.051418
18.151411	881.522271	14.056435
17.801773	872.212718	14.061453
17.843419	862.834965	14.066471
17.925040	851.242827	14.071488
17.081083	858.135025	14.076506
17.438260	864.612710	14.081523
17.702499	878.936395	14.086541
18.022733	891.965039	14.091559
18.124769	887.387998	14.096576
17.941853	908.310845	14.101594
18.071311	879.402870	14.106611
18.037914	885.195029	14.111629
17.857443	868.293079	14.116647
18.262230	853.020198	14.121664
17.851254	845.449791	14.126682
17.803239	840.865286	14.131699
17.637363	850.318365	14.136717
17.754443	868.226656	14.141735
18.139863	869.542042	14.146752
17.894316	871.202588	14.151770
18.144171	873.841036	14.156787
18.157918	884.412785	14.161805
17.899055	875.957105	14.166823
18.247314	893.717037	14.171840
18.028288	883.256647	14.176858
18.216931	883.614842	14.181875
18.323625	877.401027	14.186893
18.129878	880.932758	14.191911
18.189002	864.843857	14.196928
18.141021	885.080663	14.201946
18.332349	875.949652	14.206963
18.186077	876.427648	14.211981
18.154024	884.327619	14.216999
18.462940	872.733596	14.222016
18.397331	882.689187	14.227034
18.396758	881.796592	14.232051
18.454528	853.727691	14.237069
18.163378	862.303749	14.242087
18.330688	841.733379	14.247104
18.455773	867.921815	14.252122
18.767550	856.138526	14.257139
18.711156	854.682172	14.262157
18.185057	838.187385	14.267175
18.427470	846.360007	14.272192
18.178846	849.175885	14.277210
18.346042	851.418349	14.282227
18.503486	865.248653	14.287245
18.443646	876.347880	14.292263
18.655031	888.486568	14.297280
18.527325	880.603747	14.302298
18.617760	872.238239	14.307315
18.348794	877.814174	14.312333
18.471516	873.463090	14.317351
18.813097	876.152308	14.322368
18.481180	866.457446	14.327386
18.211591	874.571918	14.332403
18.306826	879.661000	14.337421
17.857690	876.018145	14.342439
18.481095	868.468566	14.347456
18.196980	876.589474	14.352474
18.559458	894.170625	14.357491
18.944672	884.002503	14.362509
18.430991	907.043669	14.367527
18.905934	891.022799	14.372544
18.906893	904.707511	14.377562
19.117330	883.846047	14.382579
19.140855	911.171754	14.387597
18.894887	890.190481	14.392615
19.138855	910.678407	14.397632
19.279650	897.758746	14.402650
18.997348	880.489358	14.407667
19.220239	876.790547	14.412685
18.874745	860.562492	14.417703
19.312833	856.059320	14.422720
18.793399	866.771102	14.427738
18.858936	865.838259	14.432755
18.843015	857.905512	14.437773
18.680290	872.788285	14.442791
18.948843	880.577960	14.447808
18.976906	891.463214	14.452826
19.077792	893.729434	14.457843
19.383467	895.976671	14.462861
19.267350	904.335512	14.467879
19.270460	898.499248	14.472896
19.185503	896.315608	14.477914
19.163654	888.437232	14.482931
19.291436	896.827496	14.487949
19.172143	880.342973	14.492967
19.245991	889.138405	14.497984
19.146963	891.692915	14.503002
19.084380	894.511217	14.508019
19.704742	889.346279	14.513037
19.181066	906.483487	14.518055
19.546485	900.160485	14.523072
18.992909	903.290483	14.528090
19.127789	903.477392	14.533107
19.118101	894.073761	14.538125
19.060070	920.289424	14.543143
19.347702	894.709368	14.548160
18.988362	904.879616	14.553178
19.031195	912.837090	14.558195
19.622224	895.992408	14.563213
19.380933	919.582326	14.568231
18.959796	891.051273	14.573248
19.363006	927.596884	14.578266
19.594365	914.893484	14.583283
19.837092	926.102153	14.588301
19.542962	943.973029	14.593319
19.726080	925.600647	14.598336
19.552785	950.757528	14.603354
19.484967	934.404465	14.608371
19.612157	942.097386	14.613389
19.559516	941.333638	14.618407
19.796708	932.228667	14.623424
19.835913	940.261737	14.628442
19.614252	929.963817	14.633459
20.045129	930.012264	14.638477
19.760646	943.150531	14.643495
19.764071	930.459596	14.648512
19.557795	932.884334	14.653530
19.601586	930.461356	14.658547
19.765147	930.559885	14.663565
19.715186	930.837464	14.668583
19.975189	956.367716	14.673600
20.058858	931.788587	14.678618
19.940021	930.236863	14.683635
20.006247	926.027745	14.688653
19.724669	944.012856	14.693671
19.926164	921.712229	14.698688
19.907756	940.507471	14.703706
20.003364	938.335411	14.708723
20.064621	919.015600	14.713741
19.739072	943.356108	14.718759
20.116313	936.022921	14.723776
20.563175	950.756246	14.728794
20.125491	940.595569	14.733811
20.448857	926.883006	14.738829
20.150705	938.730247	14.743847
19.973762	929.553989	14.748864
19.937376	926.481728	14.753882
20.110424	935.802391	14.758899
20.505610	941.778995	14.763917
20.409607	946.127158	14.768935
20.130877	940.344934	14.773952
20.270481	944.216964	14.778970
20.397410	946.887352	14.783987
20.447285	948.637928	14.789005
20.492173	959.221310	14.794023
20.548457	945.841971	14.799040
20.557208	925.400989	14.804058
20.264059	914.360061	14.809075
20.341392	919.469827	14.814093
20.323218	932.489880	14.819111
20.245540	938.090509	14.824128
20.516334	945.996551	14.829146
20.280048	949.246423	14.834163
20.547666	956.863696	14.839181
20.143163	972.322242	14.844199
20.360090	956.295727	14.849216
20.723704	962.277164	14.854234
20.399281	969.603503	14.859251
20.666150	961.773513	14.864269
20.574951	952.465186	14.869287
20.370194	956.731350	14.874304
20.703331	949.260796	14.879322
20.348661	956.178843	14.884339
20.638937	958.163935	14.889357
20.300374	967.143877	14.894375
20.554096	976.364049	14.899392
20.725111	979.200933	14.904410
20.678482	983.994084	14.909427
20.732617	990.771475	14.914445
20.975288	996.645482	14.919463
20.815171	990.355173	14.924480
21.133874	984.665984	14.929498
20.867358	982.377920	14.934515
21.085923	985.236959	14.939533
20.738969	989.390149	14.944551
20.724779	990.953235	14.949568
20.847556	982.375779	14.954586
20.875880	987.762302	14.959603
21.172375	997.863981	14.964621
21.105234	984.948795	14.969639
21.058309	997.843077	14.974656
21.115763	981.415633	14.979674
21.213624	997.515907	14.984691
21.388393	980.954438	14.989709
21.278856	990.182302	14.994727
21.221067	990.838938	14.999744
21.273594	985.384537	15.004762
21.188884	984.419247	15.009779
21.362707	983.959425	15.014797
21.418179	988.073563	15.019815
21.219477	979.976002	15.024832
21.570121	980.420195	15.029850
21.602764	979.901736	15.034867
21.533493	982.966966	15.039885
21.498556	986.627753	15.044903
21.361691	981.775969	15.049920
21.571494	977.184438	15.054938
21.380877	986.174086	15.059955
21.585124	975.331259	15.064973
21.510202	991.742493	15.069991
21.043310	967.798255	15.075008
21.406675	987.232948	15.080026
21.457051	978.021947	15.085043
21.647520	976.895265	15.090061
21.471404	979.856822	15.095079
21.336901	969.194065	15.100096
21.765314	980.316984	15.105114
21.371381	960.942062	15.110131
21.423191	968.691144	15.115149
21.573992	971.862585	15.120167
21.501787	980.012389	15.125184
21.921413	972.878922	15.130202
21.377597	1003.301853	15.135219
21.676904	991.606007	15.140237
21.792765	1005.625377	15.145255
21.718999	1009.762158	15.150272
21.791751	1000.130618	15.155290
21.787537	1024.524423	15.160307
22.118130	1000.823348	15.165325
21.831685	1013.421973	15.170343
21.756775	1000.796767	15.175360
22.038407	1001.215367	15.180378
22.050029	1006.716244	15.185395
21.950724	1010.644797	15.190413
21.810324	1003.815823	15.195431
21.611830	1016.767051	15.200448
21.764269	1019.371242	15.205466
21.722908	1016.181999	15.210483
21.840704	1011.006792	15.215501
21.897617	1005.922238	15.220519
21.674631	1005.917760	15.225536
21.981954	1029.272926	15.230554
22.232271	1025.797445	15.235571
22.459867	1037.296423	15.240589
22.627092	1037.587706	15.245607
22.282825	1037.984281	15.250624
22.498585	1005.874087	15.255642
22.242735	1016.758821	15.260659
22.248720	1003.378495	15.265677
22.233192	1002.503911	15.270695
22.162869	997.914878	15.275712
22.644891	1003.070955	15.280730
22.222601	996.365223	15.285747
22.305229	1006.209016	15.290765
22.526547	1014.464821	15.295783
22.546253	1018.878803	15.300800
22.670777	1011.802451	15.305818
22.117093	1000.094255	15.310835
22.484243	1024.320120	15.315853
22.587435	1031.068757	15.320871
22.190762	1032.425732	15.325888
22.462099	1033.453565	15.330906
22.336059	1035.797162	15.335923
22.276348	1023.102906	15.340941
22.368431	1041.262150	15.345959
22.632879	1024.987906	15.350976
22.929091	1031.058540	15.355994
22.933509	1035.039233	15.361011
22.759993	1023.855650	15.366029
22.802301	1038.349200	15.371047
22.522798	1020.019209	15.376064
22.919270	1033.940964	15.381082
22.373823	1026.014434	15.386099
22.778052	1035.197468	15.391117
22.826973	1012.567186	15.396135
22.792543	1027.894371	15.401152
22.822192	1030.955661	15.406170
22.818762	1044.276547	15.411187
23.148858	1047.478202	15.416205
23.184777	1041.996316	15.421223
22.964648	1039.575017	15.426240
22.921516	1025.676438	15.431258
23.033672	1041.802638	15.436275
22.889385	1046.282500	15.441293
23.351620	1053.359612	15.446311
23.225527	1046.534354	15.451328
23.558217	1041.980847	15.456346
23.386842	1035.204406	15.461363
23.433200	1011.992602	15.466381
23.351903	1020.842679	15.471399
23.244083	1014.074244	15.476416
23.536470	1025.623318	15.481434
23.489449	1010.282732	15.486451
23.558483	1013.620906	15.491469
23.634331	1009.821788	15.496487
23.313213	1031.265849	15.501504
23.514840	1010.045815	15.506522
23.564014	1019.558219	15.511539
23.773417	1024.504693	15.516557
23.393724	1036.163761	15.521575
23.245331	1021.989836	15.526592
23.589391	1011.370373	15.531610
23.551847	1020.255040	15.536627
23.403913	1013.359704	15.541645
23.735755	1026.673385	15.546663
23.619814	1029.019543	15.551680
23.767810	1016.992569	15.556698
23.566208	1023.489383	15.561715
23.669432	1024.451123	15.566733
23.535602	1013.085736	15.571751
23.277912	1027.713676	15.576768
23.702151	1002.755394	15.581786
23.516260	1026.901735	15.586803
23.250985	1026.873151	15.591821
23.973294	1029.575640	15.596839
23.723466	1033.566172	15.601856
23.494146	1013.501048	15.606874
23.120053	1029.430888	15.611891
23.448714	1029.067002	15.616909
23.850398	1047.212677	15.621927
23.884542	1052.074076	15.626944
24.254857	1047.275332	15.631962
23.976498	1055.590021	15.636979
23.948972	1054.718008	15.641997
24.214606	1044.940123	15.647015
24.073606	1050.814580	15.652032
24.031356	1052.480810	15.657050
24.094930	1052.611116	15.662067
24.177970	1039.510473	15.667085
24.092990	1044.373549	15.672103
23.882569	1052.114447	15.677120
23.836896	1048.761678	15.682138
23.699968	1049.742541	15.687155
23.849448	1050.455751	15.692173
23.891766	1052.178363	15.697191
23.779469	1052.193575	15.702208
24.131301	1059.454840	15.707226
24.353091	1073.059027	15.712243
24.209276	1081.923800	15.717261
24.274441	1072.628330	15.722279
24.299215	1086.901648	15.727296
24.324932	1068.815577	15.732314
24.404661	1085.925000	15.737331
24.339563	1083.941152	15.742349
24.455285	1074.257692	15.747367
24.247847	1091.828064	15.752384
24.517081	1085.843541	15.757402
24.538692	1090.561782	15.762419
24.523210	1070.802502	15.767437
24.330387	1067.503764	15.772455
24.207796	1089.172811	15.777472
24.517074	1066.841566	15.782490
24.885893	1080.255850	15.787507
24.461075	1079.604573	15.792525
24.409155	1085.716920	15.797543
24.647256	1093.102286	15.802560
24.803434	1097.379394	15.807578
25.104436	1093.327940	15.812595
24.850906	1086.024139	15.817613
24.718873	1074.486403	15.822631
24.564765	1083.002469	15.827648
24.703149	1083.944626	15.832666
25.143231	1098.445216	15.837683
25.136555	1102.014864	15.842701
25.076568	1097.072110	15.847719
25.200881	1088.721846	15.852736
24.999502	1073.831113	15.857754
24.866581	1076.394108	15.862771
24.588892	1098.679014	15.867789
25.131452	1088.014787	15.872807
25.001029	1094.445649	15.877824
24.796407	1092.761367	15.882842
24.950500	1105.936815	15.887859
24.993867	1098.736761	15.892877
25.083829	1097.470614	15.897895
25.199692	1098.735513	15.902912
25.061822	1103.693154	15.907930
24.999026	1103.006354	15.912947
24.988463	1096.201539	15.917965
25.185950	1092.419199	15.922983
24.914743	1100.100400	15.928000
25.030431	1116.936361	15.933018
25.230550	1131.168541	15.938035
25.468700	1126.045140	15.943053
25.401277	1128.860053	15.948071
25.454028	1130.083625	15.953088
25.262238	1132.552347	15.958106
25.557897	1122.885368	15.963123
25.334015	1134.117969	15.968141
25.545264	1127.661138	15.973159
25.349528	1124.628653	15.978176
25.594183	1146.002892	15.983194
25.712670	1134.362701	15.988211
25.442264	1140.828720	15.993229
25.581026	1129.719210	15.998247
25.514117	1132.713131	16.003264
25.740604	1136.332719	16.008282
25.403497	1130.016890	16.013299
25.772124	1139.261370	16.018317
26.179205	1148.918793	16.023335
26.254202	1139.715139	16.028352
25.797360	1119.338149	16.033370
25.694808	1122.761382	16.038387
25.801086	1118.779199	16.043405
26.061842	1117.671396	16.048423
25.963279	1110.906308	16.053440
25.999544	1130.410492	16.058458
26.059084	1120.710702	16.063475
26.053894	1126.492485	16.068493
26.327509	1124.397945	16.073511
26.096042	1119.697547	16.078528
26.018035	1126.430021	16.083546
26.104975	1118.264713	16.088563
26.069986	1133.801594	16.093581
26.176312	1145.052352	16.098599
26.320898	1154.456869	16.103616
26.158077	1145.878597	16.108634
26.338290	1152.324962	16.113651
26.292190	1158.548062	16.118669
26.263236	1159.837883	16.123687
26.124251	1147.989698	16.128704
25.936174	1157.906272	16.133722
26.340108	1140.762299	16.138739
26.123348	1146.303724	16.143757
26.346927	1149.547998	16.148775
26.226309	1149.411668	16.153792
26.325156	1139.467827	16.158810
26.750075	1139.320162	16.163827
26.395309	1139.349762	16.168845
26.736101	1148.039824	16.173863
26.466813	1143.243429	16.178880
26.678823	1145.839667	16.183898
26.762507	1141.650729	16.188915
26.734781	1154.472892	16.193933
26.737587	1141.125640	16.198951
26.719892	1160.115181	16.203968
26.665249	1143.566357	16.208986
26.993750	1149.196076	16.214003
26.712034	1149.197367	16.219021
26.640969	1148.280981	16.224039
26.632539	1160.249863	16.229056
26.478613	1156.688339	16.234074
26.848882	1168.550067	16.239091
26.813164	1181.045499	16.244109
26.779024	1187.960765	16.249127
27.003976	1182.109479	16.254144
26.747608	1196.958668	16.259162
26.887049	1179.083147	16.264179
26.878162	1199.396369	16.269197
26.982720	1184.945603	16.274215
27.252027	1185.872428	16.279232
27.309767	1178.899140	16.284250
27.154003	1185.456443	16.289267
27.035174	1186.754427	16.294285
27.250310	1190.037104	16.299303
27.406093	1188.856310	16.304320
27.260747	1182.816768	16.309338
27.417708	1178.577433	16.314355
27.457540	1179.921816	16.319373
27.228638	1184.726260	16.324391
27.100153	1178.651461	16.329408
27.169203	1182.923704	16.334426
27.503574	1161.165108	16.339443
27.611183	1174.937531	16.344461
27.449793	1176.943764	16.349479
27.608725	1185.342618	16.354496
27.472476	1174.448465	16.359514
27.698336	1191.139066	16.364531
27.169917	1188.642342	16.369549
27.403562	1195.450184	16.374567
27.448159	1169.804543	16.379584
27.465147	1201.617817	16.384602
27.670422	1192.416120	16.389619
27.995406	1202.421614	16.394637
28.119189	1211.140589	16.399655
28.031861	1193.729299	16.404672
27.800155	1207.562648	16.409690
28.212064	1196.838166	16.414707
27.788281	1198.433046	16.419725
27.623232	1184.298231	16.424743
27.988968	1191.870575	16.429760
28.161488	1212.208645	16.434778
28.055930	1196.269221	16.439795
27.979073	1211.782202	16.444813
27.719683	1194.855147	16.449831
28.001865	1206.570475	16.454848
28.011337	1219.157955	16.459866
28.073723	1208.014859	16.464883
28.034473	1220.439958	16.469901
28.137325	1215.273154	16.474919
27.889290	1198.998104	16.479936
28.085336	1215.261179	16.484954
28.109635	1200.599600	16.489971
28.007530	1210.679026	16.494989
28.231958	1205.943309	16.500007
28.222446	1196.589846	16.505024
28.369123	1214.310351	16.510042
28.346356	1197.934211	16.515059
28.209339	1214.990741	16.520077
28.471241	1216.934700	16.525095
28.617391	1211.856389	16.530112
28.163662	1212.582109	16.535130
28.482810	1224.735138	16.540147
28.361500	1223.093262	16.545165
28.344348	1247.000498	16.550183
28.738706	1237.038951	16.555200
28.608939	1240.877245	16.560218
28.691551	1235.762488	16.565235
28.367965	1236.697751	16.570253
28.423467	1238.855999	16.575271
28.649830	1216.519542	16.580288
28.447446	1231.846445	16.585306
28.555959	1223.521843	16.590323
28.487093	1230.115285	16.595341
28.417888	1232.440564	16.600359
28.867742	1263.081204	16.605376
28.988425	1276.179859	16.610394
28.962878	1263.378304	16.615411
29.060223	1272.613576	16.620429
28.952206	1259.123647	16.625447
29.135544	1278.060037	16.630464
28.850510	1270.328479	16.635482
28.916223	1265.944982	16.640499
29.378010	1279.782759	16.645517
28.685345	1277.397888	16.650535
28.951301	1263.634980	16.655552
29.223365	1264.853512	16.660570
29.323465	1262.581376	16.665587
29.150192	1270.152502	16.670605
29.136494	1263.314773	16.675623
29.122906	1266.515903	16.680640
29.205407	1264.439348	16.685658
29.107682	1267.880610	16.690675
29.176527	1260.985255	16.695693
29.233397	1286.263865	16.700711
29.567796	1293.168853	16.705728
29.508512	1303.419865	16.710746
29.751565	1299.487654	16.715763
29.762547	1294.479182	16.720781
29.482155	1292.467614	16.725799
29.822462	1284.681807	16.730816
29.815434	1283.044753	16.735834
29.690654	1280.601360	16.740851
29.420978	1269.688155	16.745869
29.600788	1296.204548	16.750887
29.893840	1279.975000	16.755904
29.612859	1298.308282	16.760922
29.908456	1294.804790	16.765939
29.803060	1291.692199	16.770957
29.608934	1284.938892	16.775975
29.744103	1293.946715	16.780992
29.566405	1305.034339	16.786010
29.750347	1294.994365	16.791027
29.866475	1289.802414	16.796045
29.521228	1306.652173	16.801063
29.917032	1293.546367	16.806080
29.916962	1301.457897	16.811098
30.063793	1301.726873	16.816115
30.183020	1314.799725	16.821133
29.877536	1335.817508	16.826151
30.052008	1326.096135	16.831168
30.166016	1331.770423	16.836186
30.295554	1343.571305	16.841203
30.389681	1318.779048	16.846221
30.394519	1336.792465	16.851239
30.440202	1326.086299	16.856256
30.139603	1317.697986	16.861274
30.308956	1323.067127	16.866291
30.300743	1326.094781	16.871309
30.345008	1327.103677	16.876327
30.593067	1312.716459	16.881344
30.646291	1325.662069	16.886362
30.490481	1319.527964	16.891379
30.919861	1319.333705	16.896397
30.704876	1305.914353	16.901415
30.425108	1316.985593	16.906432
30.694469	1315.287902	16.911450
30.586041	1320.914516	16.916467
30.789001	1319.690097	16.921485
30.544619	1302.978307	16.926503
30.827100	1320.307283	16.931520
30.368144	1317.464487	16.936538
30.368695	1334.638541	16.941555
30.504702	1321.332393	16.946573
30.474076	1323.241657	16.951591
30.604410	1347.549976	16.956608
30.832249	1340.520557	16.961626
30.861721	1350.547825	16.966643
30.968241	1357.683177	16.971661
30.804642	1354.422057	16.976679
31.145565	1351.127944	16.981696
31.207948	1364.545886	16.986714
31.016872	1360.822479	16.991731
31.224724	1352.506582	16.996749
31.140464	1366.478171	17.001767
30.996027	1357.143463	17.006784
31.038903	1351.007803	17.011802
31.063768	1351.115775	17.016819
31.148338	1345.267454	17.021837
30.823389	1363.248217	17.026855
31.409717	1385.154583	17.031872
31.481398	1382.891160	17.036890
31.447910	1389.136378	17.041907
31.709422	1375.415926	17.046925
31.701447	1388.289142	17.051943
31.474042	1372.319879	17.056960
31.439721	1393.221389	17.061978
31.341093	1382.085194	17.066995
31.556434	1371.351746	17.072013
31.435774	1390.089355	17.077031
31.433696	1380.632900	17.082048
31.245417	1375.220714	17.087066
31.306647	1380.182147	17.092083
31.905859	1383.846769	17.097101
31.829265	1410.439190	17.102119
32.397541	1401.025837	17.107136
32.099123	1395.067500	17.112154
31.560092	1401.612560	17.117171
32.001399	1377.928919	17.122189
31.594580	1393.031950	17.127207
32.040716	1397.428215	17.132224
32.364126	1412.701568	17.137242
32.213228	1404.543727	17.142259
32.241946	1383.186729	17.147277
32.121398	1396.970685	17.152295
32.438433	1364.181534	17.157312
32.274088	1377.992981	17.162330
31.950134	1381.068200	17.167347
32.233540	1367.980218	17.172365
32.118978	1397.568099	17.177383
32.426176	1403.281042	17.182400
32.417406	1419.910394	17.187418
32.605196	1404.043509	17.192435
32.574925	1407.328608	17.197453
32.527217	1378.673232	17.202471
32.462570	1371.538134	17.207488
32.270338	1382.000301	17.212506
32.289475	1401.947329	17.217523
32.299824	1415.757198	17.222541
32.592816	1416.527106	17.227559
32.896971	1417.924068	17.232576
33.237043	1402.530927	17.237594
32.615638	1401.536121	17.242611
32.785982	1400.942541	17.247629
32.759074	1403.276798	17.252647
32.550621	1405.788564	17.257664
32.787186	1406.270124	17.262682
32.509040	1422.213937	17.267699
32.798855	1408.982371	17.272717
32.755667	1414.618213	17.277735
32.712454	1415.188225	17.282752
32.828195	1407.715491	17.287770
32.772975	1409.575987	17.292787
32.935563	1402.557226	17.297805
32.396440	1418.485515	17.302823
32.777200	1424.676853	17.307840
33.065039	1437.719878	17.312858
33.091180	1444.503277	17.317875
33.205794	1432.361442	17.322893
32.838303	1446.548772	17.327911
33.189306	1438.193821	17.332928
33.542525	1451.992523	17.337946
33.323694	1435.465892	17.342963
33.487645	1448.068770	17.347981
33.112630	1441.127420	17.352999
32.994176	1447.911000	17.358016
33.569485	1436.457235	17.363034
33.036772	1457.020617	17.368051
33.488075	1445.622369	17.373069
33.544165	1476.230597	17.378087
33.711437	1470.407628	17.383104
33.892379	1471.297215	17.388122
33.669246	1472.450880	17.393139
33.940213	1453.976555	17.398157
33.790644	1447.310674	17.403175
33.304695	1450.594332	17.408192
33.858962	1453.165846	17.413210
33.723488	1479.995825	17.418227
33.873053	1464.966318	17.423245
33.563257	1471.459945	17.428263
33.706869	1459.390248	17.433280
33.951390	1455.473598	17.438298
33.650133	1466.249741	17.443315
33.801848	1450.194422	17.448333
33.761494	1467.161257	17.453351
33.848474	1463.085443	17.458368
34.029419	1475.769769	17.463386
34.175823	1500.927956	17.468403
34.388354	1495.414261	17.473421
34.054107	1505.787112	17.478439
34.067184	1481.023338	17.483456
34.457808	1501.932215	17.488474
34.160276	1501.641790	17.493491
34.604577	1488.100828	17.498509
34.397664	1496.248075	17.503527
34.369418	1499.971055	17.508544
34.520569	1486.045856	17.513562
34.206141	1499.875917	17.518579
34.515072	1482.241662	17.523597
34.680397	1489.573415	17.528615
34.506848	1483.204431	17.533632
34.610396	1491.339042	17.538650
34.414688	1489.204223	17.543667
34.631189	1499.043037	17.548685
34.625658	1487.483296	17.553703
34.964720	1501.371471	17.558720
34.814307	1477.806226	17.563738
34.624956	1492.508630	17.568755
34.634920	1478.839201	17.573773
34.729834	1492.720383	17.578791
34.553440	1494.488143	17.583808
34.711113	1502.891316	17.588826
34.857041	1519.203736	17.593843
35.046977	1515.079503	17.598861
35.098199	1541.264493	17.603879
34.974256	1519.370644	17.608896
35.365325	1529.084191	17.613914
35.214486	1530.400877	17.618931
35.303266	1517.858603	17.623949
35.453293	1518.712661	17.628967
35.273281	1526.281484	17.633984
35.496469	1506.535437	17.639002
35.427484	1521.278201	17.644019
35.107466	1519.657420	17.649037
35.395695	1515.850731	17.654055
35.315741	1510.858397	17.659072
35.718830	1522.772446	17.664090
35.503974	1508.509173	17.669107
35.631749	1509.594518	17.674125
35.517642	1500.859307	17.679143
35.746551	1511.353223	17.684160
35.748168	1500.125490	17.689178
35.503912	1524.030933	17.694195
35.697212	1507.155762	17.699213
35.646677	1520.094672	17.704231
35.505132	1515.301551	17.709248
36.140823	1517.930276	17.714266
35.620711	1514.925536	17.719283
35.864696	1513.419577	17.724301
35.901346	1518.951436	17.729319
35.854268	1523.143577	17.734336
36.191634	1534.502079	17.739354
36.063025	1536.258404	17.744371
36.148152	1535.949024	17.749389
36.223527	1530.961716	17.754407
35.896434	1536.549954	17.759424
36.260959	1533.865554	17.764442
36.397897	1539.883104	17.769459
35.872843	1540.539145	17.774477
36.086265	1529.212917	17.779495
36.281522	1536.481195	17.784512
36.368226	1530.592695	17.789530
36.306573	1522.745762	17.794547
36.252840	1539.573481	17.799565
36.161754	1522.745290	17.804583
35.840455	1551.445974	17.809600
36.912116	1545.360746	17.814618
36.662058	1552.542717	17.819635
36.370823	1558.651699	17.824653
36.370281	1552.289816	17.829671
36.223252	1580.998362	17.834688
36.770185	1565.675674	17.839706
36.674262	1572.440432	17.844723
36.364250	1579.253858	17.849741
36.802743	1570.055905	17.854759
36.723275	1576.444400	17.859776
36.743403	1556.304572	17.864794
36.641878	1577.934713	17.869811
37.056504	1582.896361	17.874829
37.182766	1587.869354	17.879847
37.164671	1577.806789	17.884864
37.227933	1562.471534	17.889882
36.947449	1567.596761	17.894899
37.268747	1564.078137	17.899917
37.427761	1560.886467	17.904935
37.304999	1560.160255	17.909952
37.483463	1548.228007	17.914970
37.384342	1559.198716	17.919987
37.432317	1560.647967	17.925005
37.409411	1547.350368	17.930023
36.970325	1563.167904	17.935040
37.183242	1561.858374	17.940058
37.299667	1559.412567	17.945075
37.565469	1586.721876	17.950093
37.795867	1572.959254	17.955111
37.782530	1591.722179	17.960128
38.026893	1578.167240	17.965146
37.784445	1571.265327	17.970163
37.842324	1565.680925	17.975181
37.457336	1544.495987	17.980199
37.533799	1565.606641	17.985216
37.564652	1582.473469	17.990234
37.731601	1573.637450	17.995251
37.746684	1577.085724	18.000269
37.980087	1583.006363	18.005287
37.513313	1583.370548	18.010304
37.672567	1582.366084	18.015322
37.619037	1580.706768	18.020339
37.604710	1611.495865	18.025357
38.055009	1618.218692	18.030375
37.778344	1633.183641	18.035392
38.174655	1609.132352	18.040410
38.360631	1624.087950	18.045427
38.255613	1615.930287	18.050445
38.378985	1621.138366	18.055463
37.953638	1609.756748	18.060480
38.620707	1612.694020	18.065498
38.560476	1597.907378	18.070515
38.383725	1612.328737	18.075533
38.373957	1611.654307	18.080551
38.500939	1622.873268	18.085568
38.916432	1609.305372	18.090586
38.357309	1614.689414	18.095603
38.389244	1607.275700	18.100621
38.741688	1614.291609	18.105639
38.684927	1611.787227	18.110656
38.727341	1605.716883	18.115674
39.081189	1624.002421	18.120691
38.858838	1635.121870	18.125709
39.014874	1615.077492	18.130727
38.986957	1631.376546	18.135744
38.937749	1610.093614	18.140762
38.898807	1623.324435	18.145779
38.998502	1628.688171	18.150797
39.384027	1634.059288	18.155815
39.081891	1630.528050	18.160832
39.388149	1629.393504	18.165850
39.159339	1606.288663	18.170867
39.132494	1609.800850	18.175885
39.294604	1618.823012	18.180903
39.235545	1638.615784	18.185920
39.242403	1623.911416	18.190938
39.350177	1635.850936	18.195955
39.360845	1632.595891	18.200973
39.541776	1630.322742	18.205991
39.231517	1645.794729	18.211008
39.501984	1623.624668	18.216026
39.887164	1638.131990	18.221043
39.520945	1635.062629	18.226061
39.765252	1623.828944	18.231079
39.107858	1636.187571	18.236096
39.776599	1633.409385	18.241114
39.637030	1629.761635	18.246131
39.594956	1630.836187	18.251149
39.883857	1626.661225	18.256167
39.274591	1639.448133	18.261184
39.595730	1639.047297	18.266202
39.496979	1661.574850	18.271219
39.548432	1665.090150	18.276237
39.816309	1655.456459	18.281255
39.739389	1672.334111	18.286272
39.814552	1663.204707	18.291290
39.964885	1681.141543	18.296307
39.901008	1686.867993	18.301325
40.598956	1680.660552	18.306343
40.363054	1690.304227	18.311360
40.086210	1686.717921	18.316378
40.467830	1684.614511	18.321395
40.462866	1700.579792	18.326413
40.514925	1689.781883	18.331431
40.375269	1702.211566	18.336448
40.680350	1695.847434	18.341466
40.739350	1686.970835	18.346483
40.700537	1689.481772	18.351501
41.028723	1679.364571	18.356519
41.209298	1671.255333	18.361536
40.956051	1674.966630	18.366554
41.116586	1653.209792	18.371571
40.826744	1658.472788	18.376589
40.861001	1651.687381	18.381607
40.877797	1648.075683	18.386624
40.887433	1648.616895	18.391642
41.342986	1647.072909	18.396659
40.813922	1660.797669	18.401677
40.756223	1640.260240	18.406695
40.860387	1648.741024	18.411712
40.728561	1648.350194	18.416730
41.107879	1668.553042	18.421747
41.246811	1673.150422	18.426765
41.308086	1682.194894	18.431783
41.010013	1689.723280	18.436800
40.953984	1687.703118	18.441818
41.159831	1673.832280	18.446835
40.643916	1683.899807	18.451853
40.842959	1681.612046	18.456871
41.574064	1700.436984	18.461888
41.555766	1715.556423	18.466906
41.485880	1705.828646	18.471923
41.432009	1721.586817	18.476941
41.628995	1699.456246	18.481959
41.724318	1701.560743	18.486976
41.809094	1712.948426	18.491994
41.845758	1710.488026	18.497011
41.684967	1695.940698	18.502029
42.097243	1700.972839	18.507047
41.797005	1702.849162	18.512064
41.600152	1710.411510	18.517082
42.079929	1698.000301	18.522099
41.955308	1708.697532	18.527117
42.053798	1696.755062	18.532135
41.896169	1700.696087	18.537152
41.912797	1690.961599	18.542170
42.148937	1699.122825	18.547187
42.325273	1711.151348	18.552205
42.253327	1728.144260	18.557223
42.235426	1726.715607	18.562240
42.544553	1738.782334	18.567258
42.463731	1721.705917	18.572275
42.392757	1744.242089	18.577293
42.334243	1718.878858	18.582311
42.700303	1741.634675	18.587328
42.733399	1726.401368	18.592346
42.944452	1723.462136	18.597363
42.522610	1719.829326	18.602381
42.746643	1708.383420	18.607399
42.495411	1692.775269	18.612416
42.597279	1713.666321	18.617434
43.106986	1717.462822	18.622451
42.605732	1729.544983	18.627469
42.847241	1713.308243	18.632487
43.208919	1725.163657	18.637504
42.916300	1727.293890	18.642522
43.019269	1731.209275	18.647539
42.766405	1723.494212	18.652557
42.142427	1720.606871	18.657575
42.717125	1725.431112	18.662592
42.917022	1726.318763	18.667610
43.106689	1736.965354	18.672627
42.770275	1753.469031	18.677645
42.978328	1754.117489	18.682663
43.329244	1763.143861	18.687680
43.423260	1757.025173	18.692698
43.461578	1761.947218	18.697715
43.336506	1764.395371	18.702733
43.398831	1761.326213	18.707751
43.394402	1769.782399	18.712768
43.271581	1763.717846	18.717786
43.575026	1764.303599	18.722803
43.603107	1779.633407	18.727821
44.034362	1785.256419	18.732839
44.134580	1785.687705	18.737856
43.945122	1770.240492	18.742874
44.041012	1761.921228	18.747891
43.719348	1750.969330	18.752909
43.997937	1764.979626	18.757927
44.211833	1778.783640	18.762944
44.006361	1766.232322	18.767962
44.235396	1785.163067	18.772979
44.197443	1770.423354	18.777997
44.113147	1772.959928	18.783015
44.180330	1789.957470	18.788032
44.063019	1781.922593	18.793050
44.079869	1780.781345	18.798067
44.109833	1779.862986	18.803085
44.371606	1771.832777	18.808103
44.743934	1790.201370	18.813120
44.595802	1779.431167	18.818138
44.486017	1780.721899	18.823155
44.418673	1779.579706	18.828173
44.582860	1772.067398	18.833191
44.623355	1783.576603	18.838208
44.321487	1774.203102	18.843226
44.279715	1787.255925	18.848243
44.564752	1799.151910	18.853261
44.487934	1811.087531	18.858279
44.899160	1806.877643	18.863296
44.714425	1821.587472	18.868314
44.930734	1816.427105	18.873331
45.011721	1814.742188	18.878349
44.887206	1823.361824	18.883367
44.733932	1814.640976	18.888384
44.737070	1807.805535	18.893402
45.066550	1819.976914	18.898419
44.818589	1845.968508	18.903437
45.562575	1832.227059	18.908455
45.504941	1834.549434	18.913472
45.384257	1842.148266	18.918490
45.499113	1835.071853	18.923507
45.272238	1843.785272	18.928525
45.267342	1830.306434	18.933543
45.727940	1842.822925	18.938560
45.542468	1843.978462	18.943578
45.529165	1831.754911	18.948595
45.406180	1842.520258	18.953613
45.670423	1833.940795	18.958631
45.816925	1842.702036	18.963648
45.605178	1829.449572	18.968666
45.927060	1825.388375	18.973683
45.868875	1840.028105	18.978701
46.044025	1826.111818	18.983719
45.989003	1839.466523	18.988736
45.634575	1825.848442	18.993754
45.885715	1830.426145	18.998771
45.988175	1838.304279	19.003789
46.165920	1851.392913	19.008807
46.529321	1859.055625	19.013824
46.504789	1869.586455	19.018842
46.477703	1853.689570	19.023859
46.467254	1833.314515	19.028877
46.335510	1819.717797	19.033895
46.682880	1822.008864	19.038912
46.133459	1837.212554	19.043930
46.430920	1845.916474	19.048947
46.652204	1853.634160	19.053965
46.660237	1864.576062	19.058983
46.865192	1850.471791	19.064000
46.639975	1864.005009	19.069018
47.076184	1850.972058	19.074035
46.746961	1854.334014	19.079053
47.103407	1854.676706	19.084071
46.937820	1851.214861	19.089088
46.858069	1853.240951	19.094106
47.028074	1848.398601	19.099123
47.144288	1867.013017	19.104141
46.902416	1846.778925	19.109159
47.195514	1860.820271	19.114176
47.396387	1847.160886	19.119194
47.200856	1851.752678	19.124211
47.384794	1849.718818	19.129229
47.068196	1852.450261	19.134247
47.215494	1856.180334	19.139264
47.155168	1863.218714	19.144282
47.311786	1846.766083	19.149299
47.171350	1853.354694	19.154317
46.894550	1859.571920	19.159335
47.547903	1885.573854	19.164352
47.244461	1882.085679	19.169370
47.440678	1895.891343	19.174387
47.543396	1888.710238	19.179405
47.306445	1883.026833	19.184423
47.602880	1890.098475	19.189440
47.788711	1911.349770	19.194458
48.368688	1907.248459	19.199475
48.390233	1909.837729	19.204493
48.300302	1896.670863	19.209511
48.706002	1885.856493	19.214528
48.408978	1879.975180	19.219546
48.153878	1883.928915	19.224563
47.934388	1872.197883	19.229581
48.408114	1869.618684	19.234599
48.321635	1864.298142	19.239616
48.276033	1863.060635	19.244634
48.404358	1871.298912	19.249651
48.480795	1865.348213	19.254669
48.283764	1881.140736	19.259687
48.393927	1888.832323	19.264704
48.510109	1893.145294	19.269722
48.556506	1906.238657	19.274739
48.602572	1910.583985	19.279757
48.521935	1907.573554	19.284775
48.885931	1896.799822	19.289792
48.496482	1911.359546	19.294810
48.372153	1907.892247	19.299827
48.663942	1889.476251	19.304845
48.454157	1915.662995	19.309863
48.556117	1902.933617	19.314880
48.451693	1928.628846	19.319898
48.698858	1907.661024	19.324915
48.870284	1929.052100	19.329933
49.273586	1918.046308	19.334951
49.465128	1924.268924	19.339968
49.279102	1918.603266	19.344986
49.290160	1928.150973	19.350003
49.574473	1929.995277	19.355021
49.346255	1950.622460	19.360039
49.637970	1933.595739	19.365056
49.772404	1951.715703	19.370074
50.207444	1938.232658	19.375091
49.955633	1910.726743	19.380109
49.443667	1910.306618	19.385127
49.779220	1899.256435	19.390144
49.569791	1918.844147	19.395162
49.716707	1931.127856	19.400179
50.388617	1937.321674	19.405197
49.836802	1953.902002	19.410215
50.222574	1927.043707	19.415232
50.179538	1947.430282	19.420250
50.179214	1935.315409	19.425267
50.164080	1944.045556	19.430285
49.870158	1936.331464	19.435303
50.362869	1941.354033	19.440320
50.081147	1940.350091	19.445338
50.006234	1941.103477	19.450355
50.374383	1955.298127	19.455373
50.136257	1940.544587	19.460391
50.292824	1941.076682	19.465408
50.207779	1949.847515	19.470426
50.151063	1959.387941	19.475443
50.556783	1963.060573	19.480461
50.723121	1976.697262	19.485479
50.943680	1957.773659	19.490496
50.956850	1974.169122	19.495514
50.635948	1964.913196	19.500531
51.079218	1959.693822	19.505549
50.915269	1978.780777	19.510567
51.050101	1954.997710	19.515584
51.030150	1956.355092	19.520602
50.650070	1952.724574	19.525619
50.841901	1954.204607	19.530637
50.940813	1971.131862	19.535655
50.975168	1985.089135	19.540672
51.139780	2004.848467	19.545690
51.300663	1997.726979	19.550707
51.601114	1983.097250	19.555725
51.259710	1999.800799	19.560743
51.535246	1991.665169	19.565760
51.348934	1990.574898	19.570778
51.419603	1992.727007	19.575795
51.343219	1983.430464	19.580813
51.516287	2008.557720	19.585831
51.945740	2010.561875	19.590848
51.985039	2017.826929	19.595866
51.590031	2024.213926	19.600883
52.008382	2021.192850	19.605901
51.921459	2025.630450	19.610919
51.998284	2015.107403	19.615936
51.981653	2010.318578	19.620954
52.144232	2026.620717	19.625971
52.313916	2010.471309	19.630989
52.281696	2021.805733	19.636007
52.560195	2013.489221	19.641024
52.537143	2025.923908	19.646042
52.320589	2018.346666	19.651059
52.446918	2013.029776	19.656077
52.463443	2020.356557	19.661095
52.225568	2012.234612	19.666112
52.520048	2016.859136	19.671130
52.486485	2016.994187	19.676147
52.843495	2004.059909	19.681165
52.494704	2012.976313	19.686183
52.671177	2009.185611	19.691200
52.973356	2024.153198	19.696218
52.663937	2013.122035	19.701235
52.793034	2015.251895	19.706253
52.468347	2021.294848	19.711271
52.083687	2028.585587	19.716288
52.685680	2040.103750	19.721306
52.809506	2037.144923	19.726323
53.388899	2043.680395	19.731341
52.951471	2056.288783	19.736359
53.099189	2060.663901	19.741376
53.080144	2079.465367	19.746394
53.340570	2082.746658	19.751411
53.840027	2073.735051	19.756429
53.811563	2064.868063	19.761447
53.822754	2067.039852	19.766464
53.870891	2070.163342	19.771482
53.848320	2066.878370	19.776499
54.156903	2054.125644	19.781517
53.997293	2061.052591	19.786535
53.902452	2060.263384	19.791552
54.107283	2039.979720	19.796570
53.812131	2066.491404	19.801587
53.883343	2052.513658	19.806605
53.986242	2054.791725	19.811623
54.177736	2050.409558	19.816640
54.097641	2052.474011	19.821658
53.939466	2060.735528	19.826675
54.142352	2042.441206	19.831693
53.772360	2064.977568	19.836711
54.034812	2048.924777	19.841728
54.296626	2063.978193	19.846746
54.189021	2076.309296	19.851763
54.536658	2089.383048	19.856781
54.548194	2088.958970	19.861799
54.486555	2085.067465	19.866816
54.581927	2089.180914	19.871834
54.809721	2086.413621	19.876851
54.725882	2090.800936	19.881869
54.983096	2089.544268	19.886887
54.923031	2080.235621	19.891904
55.130078	2086.417361	19.896922
54.958895	2079.940767	19.901939
55.129027	2072.524065	19.906957
54.946501	2086.901556	19.911975
55.003106	2094.099821	19.916992
55.253117	2106.467306	19.922010
55.337040	2119.159047	19.927027
55.391859	2102.590902	19.932045
55.365409	2111.242319	19.937063
55.562365	2099.384921	19.942080
55.582393	2120.379702	19.947098
55.266860	2104.252418	19.952115
55.589115	2110.815651	19.957133
56.052294	2108.620867	19.962151
56.089679	2099.331728	19.967168
55.930540	2106.817479	19.972186
55.951278	2102.179509	19.977203
56.097324	2101.756918	19.982221
55.890873	2089.231279	19.987239
55.564458	2107.451498	19.992256
55.874660	2099.267472	19.997274
55.464290	2101.646998	20.002291
55.729120	2103.205420	20.007309
55.647658	2108.933752	20.012327
56.155681	2124.748569	20.017344
56.026542	2140.203028	20.022362
56.272412	2138.913690	20.027379
56.465078	2140.255142	20.032397
56.492232	2135.304934	20.037415
56.245984	2128.219175	20.042432
56.422669	2124.431263	20.047450
56.319344	2160.096368	20.052467
56.672000	2161.426341	20.057485
57.005417	2165.753285	20.062503
56.850998	2165.927696	20.067520
57.157692	2152.058754	20.072538
57.122557	2154.253858	20.077555
57.307027	2148.240618	20.082573
57.229563	2145.359319	20.087591
57.463329	2153.322591	20.092608
57.858089	2146.677455	20.097626
57.317275	2130.926487	20.102643
57.378463	2116.349654	20.107661
57.427589	2117.179089	20.112679
57.356660	2109.340474	20.117696
57.371904	2121.159466	20.122714
57.771871	2134.850586	20.127731
57.712375	2138.075918	20.132749
57.605963	2132.169996	20.137767
57.749545	2150.792043	20.142784
57.978177	2145.324562	20.147802
58.049385	2147.621953	20.152819
58.112581	2145.152769	20.157837
57.782583	2131.479205	20.162855
57.556138	2147.650224	20.167872
57.821971	2138.282962	20.172890
57.642048	2149.988584	20.177907
57.798268	2126.817558	20.182925
57.610950	2137.766647	20.187943
57.745940	2161.751428	20.192960
58.281780	2161.263830	20.197978
58.310329	2181.948284	20.202995
58.162087	2172.760237	20.208013
58.017508	2183.539134	20.213031
58.154488	2182.663193	20.218048
58.367494	2201.669433	20.223066
58.450885	2205.920010	20.228083
58.472439	2207.061436	20.233101
58.558946	2214.723735	20.238119
58.650195	2216.637375	20.243136
59.060879	2200.221108	20.248154
58.516786	2219.413695	20.253171
58.911013	2217.247611	20.258189
59.324100	2215.211459	20.263207
59.433307	2236.163122	20.268224
59.502212	2214.839363	20.273242
59.354102	2214.700578	20.278259
59.377735	2203.284470	20.283277
59.516850	2184.024204	20.288295
59.670952	2192.131742	20.293312
59.603231	2193.145818	20.298330
59.530513	2192.799528	20.303347
59.400110	2202.032058	20.308365
59.237459	2208.297577	20.313383
59.386560	2224.460544	20.318400
59.826206	2226.838770	20.323418
59.907679	2227.775839	20.328435
59.388212	2228.310134	20.333453
59.739598	2222.483419	20.338471
59.719410	2237.912886	20.343488
59.805319	2232.289659	20.348506
59.871080	2240.287826	20.353523
60.148154	2262.056923	20.358541
60.366917	2248.742102	20.363559
60.100584	2266.338506	20.368576
60.313118	2248.109560	20.373594
60.831242	2252.947060	20.378611
60.688737	2251.169817	20.383629
60.843891	2246.682397	20.388647
60.914904	2254.538388	20.393664
60.848340	2242.795479	20.398682
60.724531	2253.357837	20.403699
60.809301	2244.356992	20.408717
60.994999	2235.213707	20.413735
60.913210	2245.739397	20.418752
61.263542	2233.859698	20.423770
61.138636	2253.580202	20.428787
60.969768	2238.960574	20.433805
61.240573	2247.904426	20.438823
60.978299	2260.944197	20.443840
61.360882	2250.753569	20.448858
61.066883	2250.940812	20.453875
60.978167	2258.566352	20.458893
61.219838	2252.008074	20.463911
61.182924	2282.892000	20.468928
61.422494	2271.225427	20.473946
61.353373	2279.302588	20.478963
61.558334	2274.782720	20.483981
61.738671	2271.210670	20.488999
61.402167	2280.460184	20.494016
61.546935	2274.645353	20.499034
61.617664	2291.543668	20.504051
61.826908	2300.150338	20.509069
61.918327	2292.558969	20.514087
62.007020	2299.463590	20.519104
62.010317	2275.960383	20.524122
61.802599	2302.980284	20.529139
62.088454	2292.151780	20.534157
62.270442	2317.337507	20.539175
62.355238	2315.475260	20.544192
62.621435	2330.445551	20.549210
62.675565	2305.037346	20.554227
62.413651	2330.604671	20.559245
62.711229	2302.495434	20.564263
62.799182	2319.930218	20.569280
62.770662	2323.265413	20.574298
62.699478	2314.532584	20.579315
62.823299	2333.121116	20.584333
63.124490	2314.050208	20.589351
63.119340	2341.938725	20.594368
63.294364	2342.274213	20.599386
63.173789	2335.972386	20.604403
63.075293	2358.256960	20.609421
63.421478	2340.865134	20.614439
63.132738	2358.755458	20.619456
63.438425	2340.846193	20.624474
63.391912	2351.828062	20.629491
63.606459	2347.937004	20.634509
63.775859	2353.284259	20.639527
63.811549	2342.737968	20.644544
63.914541	2341.055360	20.649562
63.756598	2325.189353	20.654579
63.477467	2345.743405	20.659597
63.751058	2323.359649	20.664615
63.405060	2348.901536	20.669632
63.759267	2336.262377	20.674650
63.937590	2369.075758	20.679667
63.839611	2354.214617	20.684685
64.297099	2371.041036	20.689703
64.119101	2369.773307	20.694720
64.220598	2368.761313	20.699738
64.233522	2361.929815	20.704755
64.608516	2373.453760	20.709773
64.589213	2363.620371	20.714791
64.697685	2375.963636	20.719808
64.949618	2382.091629	20.724826
64.992457	2390.696326	20.729843
64.760749	2363.953384	20.734861
65.223208	2371.816979	20.739879
65.013139	2383.893845	20.744896
65.180401	2381.478872	20.749914
65.394864	2378.835267	20.754931
64.858212	2372.210314	20.759949
65.154311	2375.692435	20.764967
65.179769	2378.096815	20.769984
65.283860	2382.725064	20.775002
65.577736	2391.170775	20.780019
65.323727	2398.215524	20.785037
65.555106	2384.295838	20.790055
65.164498	2408.687695	20.795072
65.116860	2394.579301	20.800090
65.557563	2394.900212	20.805107
65.427089	2415.875196	20.810125
66.102660	2420.444642	20.815143
65.530163	2418.368217	20.820160
65.703399	2409.294988	20.825178
66.189546	2416.676221	20.830195
66.328438	2413.869731	20.835213
66.234509	2409.933979	20.840231
66.271028	2417.109046	20.845248
66.138631	2401.447172	20.850266
66.903306	2426.189202	20.855283
66.634742	2413.818619	20.860301
66.387890	2414.961706	20.865319
66.411687	2426.901942	20.870336
66.348102	2431.851375	20.875354
66.769745	2437.612616	20.880371
66.629242	2434.230339	20.885389
66.945773	2436.262857	20.890407
67.031230	2431.010443	20.895424
67.359197	2423.370472	20.900442
67.495740	2428.429724	20.905459
67.362432	2422.757824	20.910477
67.315403	2431.807448	20.915495
67.474130	2430.207339	20.920512
67.610511	2419.724068	20.925530
67.676404	2419.234411	20.930547
67.544830	2421.142189	20.935565
67.825028	2413.636083	20.940583
67.587695	2425.392733	20.945600
67.883987	2422.847983	20.950618
67.606020	2425.360181	20.955635
67.595731	2427.225676	20.960653
67.830050	2409.015377	20.965671
67.749316	2424.318050	20.970688
67.739089	2425.292526	20.975706
67.837183	2417.957041	20.980723
67.715332	2430.012477	20.985741
67.696538	2440.617050	20.990759
67.810812	2449.275910	20.995776
68.070089	2462.145619	21.000794
68.106046	2443.381729	21.005811
68.065215	2461.380592	21.010829
68.158942	2467.201742	21.015847
68.239334	2468.028785	21.020864
68.385001	2474.894349	21.025882
68.864735	2482.593951	21.030899
68.470557	2479.849560	21.035917
68.758230	2477.926803	21.040935
68.776589	2487.899376	21.045952
68.616936	2485.301044	21.050970
69.216608	2491.813875	21.055987
69.093743	2508.273819	21.061005
69.343034	2501.509679	21.066023
69.641336	2510.117298	21.071040
69.153522	2515.914901	21.076058
69.795384	2495.186521	21.081075
69.755892	2517.375958	21.086093
70.005764	2507.820980	21.091111
69.780546	2514.294374	21.096128
69.731971	2493.788346	21.101146
69.766364	2494.458843	21.106163
69.623747	2496.189544	21.111181
70.090469	2500.803762	21.116199
69.828775	2506.724994	21.121216
69.905021	2503.947735	21.126234
70.063246	2495.455395	21.131251
69.878574	2510.350588	21.136269
70.105463	2493.512282	21.141287
70.331411	2501.864570	21.146304
69.980752	2501.436466	21.151322
70.294424	2518.335625	21.156339
69.999496	2520.705780	21.161357
70.508428	2539.035083	21.166375
70.778145	2529.874983	21.171392
70.751938	2536.878804	21.176410
71.040948	2519.857788	21.181427
71.051277	2538.966827	21.186445
70.858745	2528.768314	21.191463
70.823805	2526.356816	21.196480
71.077662	2526.714316	21.201498
71.378933	2533.858676	21.206515
70.960754	2563.323311	21.211533
71.363074	2551.968757	21.216551
71.704641	2566.797117	21.221568
71.452336	2553.065659	21.226586
71.586989	2553.019296	21.231603
71.155926	2561.495935	21.236621
71.214309	2546.710919	21.241639
71.458926	2551.340403	21.246656
71.241003	2563.823178	21.251674
71.775597	2574.695595	21.256691
71.703301	2588.854087	21.261709
71.616733	2597.045699	21.266727
71.893222	2576.030986	21.271744
71.598453	2593.146505	21.276762
71.671287	2582.780893	21.281779
72.036058	2609.501046	21.286797
71.806605	2607.873937	21.291815
72.223184	2614.470613	21.296832
72.083066	2603.480623	21.301850
72.638067	2615.017124	21.306867
72.425961	2626.976620	21.311885
73.144273	2640.670500	21.316903
73.223903	2635.160156	21.321920
73.284160	2631.092386	21.326938
73.126549	2619.971435	21.331955
73.264185	2602.170729	21.336973
73.390546	2604.801546	21.341991
73.430731	2593.029117	21.347008
73.547335	2608.370611	21.352026
73.634942	2604.649067	21.357043
73.283953	2581.425564	21.362061
73.330151	2586.219719	21.367079
73.736848	2582.595822	21.372096
73.425948	2594.003981	21.377114
73.614383	2592.694377	21.382131
73.865501	2598.164416	21.387149
73.657211	2615.823467	21.392167
73.967640	2609.098383	21.397184
73.793899	2626.882231	21.402202
74.129124	2617.197742	21.407219
74.217624	2620.735876	21.412237
73.989305	2607.498171	21.417255
74.405806	2620.759101	21.422272
73.798526	2615.682313	21.427290
73.827467	2622.061002	21.432307
74.250515	2624.605399	21.437325
74.252228	2648.954651	21.442343
74.368524	2644.030094	21.447360
74.441924	2654.498532	21.452378
74.561487	2652.439581	21.457395
74.425126	2644.048589	21.462413
74.523820	2670.259153	21.467431
74.886626	2665.198590	21.472448
74.576559	2663.858579	21.477466
74.984555	2670.550386	21.482483
75.073940	2663.498469	21.487501
75.132779	2673.860876	21.492519
75.444284	2679.066275	21.497536
75.405790	2697.350619	21.502554
75.800528	2693.192720	21.507571
75.610257	2698.697552	21.512589
75.850027	2690.903937	21.517607
75.886665	2682.910657	21.522624
75.627634	2701.849282	21.527642
76.269332	2689.220981	21.532659
75.878144	2684.311582	21.537677
75.902736	2692.018795	21.542695
76.254372	2680.759716	21.547712
76.466090	2689.792714	21.552730
76.642958	2677.305599	21.557747
76.400705	2687.248149	21.562765
76.830066	2674.016059	21.567783
77.009674	2682.098778	21.572800
76.748290	2673.976822	21.577818
76.565255	2692.441522	21.582835
76.685905	2682.835949	21.587853
76.248163	2686.261284	21.592871
76.747588	2683.299117	21.597888
76.801186	2680.710977	21.602906
76.706144	2702.853962	21.607923
77.130689	2716.537999	21.612941
76.649033	2719.033517	21.617959
77.041990	2703.383719	21.622976
76.602741	2717.065638	21.627994
77.177024	2731.625613	21.633011
77.326744	2727.257440	21.638029
77.392981	2742.202130	21.643047
77.745419	2732.285423	21.648064
77.531391	2736.940565	21.653082
77.632801	2739.740666	21.658099
77.808981	2753.497270	21.663117
77.510413	2747.167215	21.668135
77.898829	2745.258679	21.673152
77.757741	2775.285921	21.678170
78.113433	2756.612298	21.683187
78.264964	2768.640732	21.688205
78.237870	2765.983049	21.693223
78.416553	2774.352744	21.698240
78.452249	2780.547139	21.703258
78.502823	2757.182414	21.708275
78.495077	2777.840994	21.713293
78.708217	2779.140543	21.718311
78.990089	2766.574397	21.723328
78.832593	2802.002729	21.728346
78.668225	2803.504213	21.733363
78.662689	2794.179627	21.738381
78.761197	2795.476864	21.743399
79.049833	2781.113948	21.748416
78.916840	2783.723294	21.753434
78.889856	2803.227754	21.758451
79.119525	2804.843628	21.763469
79.186428	2827.073204	21.768487
79.554084	2825.044680	21.773504
79.602129	2827.362928	21.778522
79.535154	2835.048342	21.783539
79.834612	2838.423728	21.788557
79.904127	2854.623342	21.793575
79.813270	2860.375353	21.798592
79.824325	2856.694348	21.803610
79.909094	2871.951219	21.808627
80.408685	2869.392287	21.813645
80.340768	2860.801307	21.818663
80.414096	2850.969030	21.823680
80.230096	2854.779583	21.828698
80.533775	2880.948365	21.833715
81.024782	2878.797494	21.838733
80.706392	2888.935411	21.843751
81.099968	2873.158385	21.848768
81.011991	2885.870113	21.853786
81.293360	2865.458655	21.858803
81.086275	2882.236815	21.863821
80.821650	2871.041252	21.868839
81.479084	2866.816671	21.873856
81.203975	2880.915650	21.878874
81.412783	2874.269442	21.883891
81.498376	2872.490648	21.888909
81.461823	2872.678851	21.893927
81.660428	2864.905926	21.898944
81.796194	2871.159599	21.903962
81.466019	2870.122462	21.908979
81.584258	2863.537479	21.913997
81.334253	2872.456554	21.919015
81.684091	2892.168902	21.924032
81.703640	2897.788523	21.929050
81.711730	2902.588877	21.934067
82.081083	2909.161993	21.939085
82.099444	2921.207238	21.944103
82.473769	2932.690185	21.949120
82.730084	2918.662563	21.954138
83.007228	2921.882422	21.959155
83.452912	2915.841070	21.964173
83.317693	2897.574544	21.969191
83.357243	2888.201707	21.974208
83.057445	2870.641265	21.979226
83.256958	2871.223476	21.984243
83.334415	2867.736982	21.989261
82.772805	2876.830963	21.994279
83.074688	2863.300918	21.999296
83.164908	2872.533804	22.004314
83.409716	2891.414005	22.009331
83.462604	2901.387635	22.014349
83.281226	2895.320992	22.019367
83.359357	2899.902513	22.024384
83.476654	2897.618340	22.029402
83.412560	2914.334328	22.034419
83.582985	2917.043538	22.039437
83.591678	2930.977174	22.044455
83.748281	2935.489445	22.049472
83.916557	2932.043237	22.054490
83.727265	2945.781875	22.059507
83.959553	2945.352884	22.064525
83.807494	2965.199637	22.069543
84.250456	2955.791588	22.074560
84.333205	2977.142682	22.079578
84.482954	2970.667394	22.084595
84.549794	2966.998205	22.089613
84.326315	2993.616455	22.094631
84.519419	2996.893717	22.099648
84.711731	3002.329726	22.104666
84.834685	2997.694277	22.109683
85.180980	3006.996923	22.114701
85.379858	3002.642594	22.119719
85.715325	2985.447462	22.124736
85.326404	3000.039320	22.129754
85.556224	3006.064734	22.134771
86.066710	3003.611055	22.139789
85.467444	3018.386294	22.144807
85.528693	3012.981007	22.149824
86.074430	3018.841634	22.154842
85.974927	3023.494076	22.159859
86.124904	3021.301325	22.164877
85.828183	3026.664235	22.169895
86.067831	3019.235199	22.174912
86.147517	3010.777206	22.179930
86.004114	3024.524470	22.184947
86.358824	3023.792602	22.189965
86.535418	3040.445333	22.194983
86.935155	3052.836079	22.200000
86.912034	3039.690062	22.205018
86.991571	3050.118980	22.210035
87.259898	3036.243777	22.215053
87.106136	3052.606269	22.220071
87.235729	3033.768319	22.225088
87.318926	3045.352013	22.230106
87.326055	3039.167361	22.235123
87.782573	3034.434266	22.240141
87.476887	3036.308889	22.245159
87.485698	3029.011685	22.250176
87.620364	3032.952083	22.255194
87.268788	3031.786398	22.260211
87.386509	3025.832071	22.265229
87.320547	3046.333524	22.270247
87.732472	3058.762807	22.275264
88.144421	3046.274731	22.280282
87.579084	3065.616939	22.285299
87.659332	3048.333611	22.290317
87.608887	3073.558003	22.295335
88.106940	3092.023413	22.300352
88.402764	3091.836058	22.305370
88.348789	3097.525572	22.310387
88.408703	3088.242940	22.315405
88.431972	3089.343405	22.320423
88.454859	3093.256428	22.325440
88.586393	3096.839327	22.330458
88.505155	3123.261282	22.335475
88.778871	3117.014043	22.340493
88.531554	3125.352565	22.345511
89.180883	3121.651840	22.350528
89.317286	3118.496065	22.355546
89.519707	3116.916221	22.360563
89.411795	3110.221276	22.365581
89.581021	3137.085673	22.370599
89.768592	3141.896792	22.375616
90.116574	3137.015477	22.380634
90.166126	3148.217446	22.385651
90.527891	3140.158786	22.390669
90.474766	3114.890579	22.395687
90.338000	3105.817387	22.400704
90.393445	3098.681520	22.405722
90.172217	3094.921926	22.410739
90.258423	3102.108981	22.415757
90.420856	3112.629941	22.420775
90.551173	3130.500132	22.425792
90.413821	3125.184312	22.430810
90.784293	3137.588229	22.435827
90.748846	3115.204005	22.440845
90.967290	3124.759321	22.445863
90.778624	3124.777606	22.450880
90.956354	3126.158619	22.455898
90.715241	3136.736440	22.460915
91.036585	3136.328354	22.465933
91.102086	3155.268624	22.470951
91.063386	3151.209983	22.475968
91.305995	3155.735663	22.480986
91.218147	3165.692765	22.486003
91.626095	3173.155392	22.491021
91.586555	3180.897264	22.496039
91.828814	3185.634997	22.501056
91.858067	3179.903279	22.506074
91.647658	3180.483761	22.511091
91.930198	3193.892903	22.516109
92.153313	3204.189351	22.521127
92.012804	3211.949105	22.526144
92.339855	3192.372300	22.531162
92.609391	3209.374583	22.536179
92.577082	3209.191652	22.541197
92.798858	3222.155984	22.546215
92.648233	3225.463918	22.551232
93.373096	3233.190511	22.556250
93.196546	3227.287884	22.561267
93.173386	3229.512852	22.566285
93.267021	3230.548948	22.571303
92.946585	3234.023121	22.576320
93.655587	3234.519185	22.581338
93.139679	3214.831084	22.586355
93.396601	3233.084370	22.591373
93.541595	3245.309317	22.596391
93.553055	3259.359907	22.601408
94.122369	3255.058456	22.606426
93.951975	3261.519953	22.611443
94.065555	3264.079381	22.616461
94.191296	3256.188785	22.621479
94.270654	3260.197037	22.626496
94.255314	3247.542030	22.631514
94.035139	3256.853996	22.636531
94.544440	3266.121596	22.641549
94.658250	3277.426810	22.646567
94.519848	3295.069969	22.651584
95.191633	3276.199996	22.656602
94.862435	3294.539582	22.661619
94.980375	3272.469121	22.666637
95.036311	3284.848960	22.671655
95.239915	3298.075979	22.676672
95.331444	3282.048480	22.681690
95.337505	3282.745935	22.686707
95.281588	3273.350062	22.691725
95.138667	3279.497803	22.696743
95.113331	3315.323347	22.701760
95.359784	3299.996145	22.706778
95.342080	3310.381864	22.711795
95.505010	3311.225233	22.716813
95.776051	3328.828328	22.721831
95.774187	3334.673083	22.726848
96.083301	3342.921346	22.731866
96.309882	3349.728856	22.736883
96.378977	3334.197092	22.741901
96.516025	3344.906246	22.746919
96.016936	3337.206256	22.751936
96.251109	3356.118309	22.756954
96.448411	3370.920897	22.761971
96.644641	3380.807770	22.766989
96.879648	3352.677831	22.772007
96.728690	3368.608737	22.777024
97.253067	3377.059025	22.782042
97.451346	3397.720804	22.787059
97.518292	3374.598283	22.792077
97.715949	3388.704829	22.797095
97.721616	3385.213548	22.802112
97.708062	3383.729205	22.807130
97.810492	3390.106895	22.812147
97.888161	3379.289792	22.817165
98.214473	3385.730671	22.822183
98.071312	3385.059999	22.827200
97.974336	3382.682041	22.832218
97.933335	3384.022853	22.837235
97.824564	3382.448348	22.842253
98.183547	3412.125514	22.847271
98.402351	3410.303388	22.852288
99.027397	3413.942199	22.857306
98.786908	3402.022243	22.862323
98.953246	3418.124763	22.867341
99.036170	3407.640208	22.872359
99.042700	3432.511510	22.877376
99.172161	3411.971493	22.882394
99.309005	3431.447116	22.887411
99.464070	3434.642380	22.892429
99.822661	3428.550465	22.897447
99.551237	3440.371781	22.902464
99.958342	3434.627919	22.907482
99.718561	3442.050876	22.912499
99.705226	3439.596101	22.917517
100.067375	3435.131411	22.922535
99.949206	3442.371294	22.927552
100.285127	3440.959696	22.932570
100.109975	3428.941331	22.937587
100.078774	3427.076665	22.942605
100.212346	3433.805496	22.947623
100.110806	3463.704519	22.952640
100.609933	3445.348068	22.957658
100.246177	3450.311606	22.962675
100.479591	3449.966465	22.967693
100.631240	3463.761615	22.972711
100.251305	3483.030794	22.977728
100.772670	3465.276501	22.982746
100.686081	3493.577181	22.987763
101.064851	3495.198016	22.992781
101.201357	3526.514203	22.997799
101.131708	3513.356182	23.002816
101.264575	3511.265394	23.007834
101.791516	3520.478859	23.012851
101.667234	3546.549820	23.017869
102.133334	3541.872662	23.022887
101.972911	3548.368257	23.027904
102.286705	3536.621542	23.032922
102.359277	3537.995957	23.037939
102.287624	3528.032691	23.042957
102.383634	3526.595381	23.047975
102.439392	3533.028083	23.052992
102.335590	3512.915425	23.058010
102.456779	3540.483486	23.063027
102.330623	3556.153813	23.068045
102.843546	3556.623046	23.073063
102.938239	3544.899343	23.078080
103.133110	3553.665576	23.083098
103.068981	3553.358382	23.088115
103.079459	3551.032715	23.093133
103.513907	3558.585829	23.098151
103.527693	3594.316191	23.103168
103.652763	3575.010648	23.108186
103.517022	3582.710355	23.113203
103.873131	3592.514453	23.118221
103.926935	3595.369227	23.123239
103.900781	3601.169675	23.128256
103.805309	3596.667379	23.133274
103.688954	3619.658445	23.138291
103.607490	3604.780377	23.143309
104.242389	3626.856620	23.148327
104.395761	3641.556106	23.153344
104.855166	3662.028642	23.158362
104.866034	3639.012624	23.163379
105.171207	3649.268451	23.168397
105.181581	3651.567262	23.173415
105.180411	3656.839033	23.178432
105.202614	3630.686138	23.183450
105.802638	3636.382731	23.188467
105.471676	3656.886268	23.193485
105.366476	3632.984581	23.198503
105.440203	3649.361093	23.203520
105.730679	3647.111574	23.208538
105.648302	3652.757367	23.213555
105.781219	3665.749747	23.218573
105.810516	3669.844128	23.223591
106.010083	3660.974659	23.228608
106.270910	3681.317842	23.233626
106.263186	3686.789511	23.238643
106.113574	3689.343097	23.243661
106.693601	3675.253227	23.248679
106.407014	3698.707550	23.253696
106.428893	3685.167944	23.258714
106.471029	3706.978501	23.263731
106.724807	3712.160526	23.268749
106.842823	3704.343218	23.273767
107.256211	3720.371177	23.278784
107.211474	3722.901532	23.283802
107.824447	3731.322220	23.288819
107.291461	3752.276562	23.293837
107.717314	3737.934965	23.298855
107.922632	3755.448233	23.303872
107.781285	3744.519438	23.308890
108.182246	3743.168912	23.313907
108.068966	3742.355303	23.318925
107.990439	3741.207626	23.323943
108.173509	3754.943319	23.328960
108.494597	3762.151904	23.333978
108.429566	3762.090902	23.338995
108.584734	3773.597506	23.344013
108.613599	3768.776404	23.349031
108.558974	3768.900679	23.354048
108.489392	3770.789126	23.359066
108.745714	3774.834603	23.364083
108.595606	3803.498882	23.369101
109.258827	3809.970286	23.374119
109.182684	3817.014630	23.379136
109.215663	3804.365749	23.384154
109.109457	3815.962423	23.389171
109.184878	3832.805553	23.394189
109.562698	3831.267517	23.399207
109.417202	3838.586702	23.404224
109.622595	3848.173363	23.409242
109.891654	3851.904963	23.414259
110.409272	3861.247135	23.419277
110.431626	3871.395917	23.424295
110.590948	3863.371124	23.429312
110.720510	3865.501068	23.434330
110.875466	3856.434934	23.439347
110.442325	3866.155073	23.444365
110.981489	3853.223698	23.449383
110.925189	3868.966258	23.454400
111.033791	3887.220420	23.459418
111.228439	3876.718660	23.464435
111.182561	3879.542126	23.469453
111.483625	3876.580236	23.474471
111.430419	3877.583755	23.479488
111.465456	3883.510606	23.484506
111.726159	3894.643188	23.489523
111.730048	3915.701149	23.494541
111.742097	3897.914981	23.499559
111.873374	3912.921115	23.504576
111.675154	3915.893378	23.509594
112.229582	3921.954877	23.514611
112.179898	3938.519992	23.519629
112.564002	3935.287689	23.524647
112.533999	3943.727937	23.529664
112.590324	3934.789466	23.534682
112.781803	3962.911399	23.539699
112.906916	3966.521545	23.544717
113.021085	3968.048566	23.549735
113.200499	3962.925768	23.554752
113.154996	3969.644662	23.559770
113.669746	3975.530859	23.564787
113.874347	3981.859235	23.569805
114.002848	3988.153340	23.574823
114.381687	3976.154218	23.579840
114.363699	3985.372779	23.584858
114.570382	3967.012270	23.589875
114.125067	3957.675602	23.594893
114.213709	3962.466124	23.599911
114.519585	3968.813191	23.604928
114.157909	3982.864290	23.609946
114.762287	3962.550365	23.614963
114.257887	3969.991515	23.619981
114.193119	3987.874071	23.624999
114.672357	3997.958460	23.630016
114.754079	4001.271075	23.635034
115.125329	3997.263361	23.640051
114.879762	4016.771025	23.645069
115.045121	4017.153818	23.650087
115.322273	4040.700139	23.655104
115.174407	4018.262125	23.660122
115.669488	4042.472797	23.665139
115.769753	4059.327422	23.670157
115.986861	4069.202036	23.675175
116.370590	4052.671143	23.680192
116.281714	4070.389281	23.685210
116.223509	4060.300030	23.690227
116.206669	4075.915812	23.695245
116.577713	4064.727324	23.700263
116.325521	4060.290750	23.705280
116.050530	4084.496462	23.710298
116.717819	4083.572745	23.715315
116.775452	4091.638370	23.720333
116.616372	4092.090919	23.725351
116.973856	4105.596930	23.730368
117.174744	4130.958279	23.735386
117.358821	4115.904348	23.740403
117.142946	4118.337068	23.745421
117.381911	4135.140117	23.750439
117.694564	4136.491448	23.755456
117.853971	4148.607056	23.760474
117.954330	4148.410065	23.765491
118.406832	4154.352678	23.770509
118.195645	4134.683909	23.775527
118.589692	4143.527796	23.780544
118.623566	4161.589520	23.785562
118.980926	4169.067883	23.790579
118.739874	4184.440520	23.795597
118.840608	4170.912851	23.800615
118.867408	4175.764444	23.805632
119.101426	4168.958208	23.810650
119.357630	4175.279317	23.815667
119.500638	4161.673414	23.820685
119.432022	4173.419256	23.825703
119.997577	4177.655071	23.830720
119.895765	4192.637004	23.835738
119.763954	4179.206808	23.840755
119.894179	4197.094390	23.845773
120.090320	4180.676640	23.850791
120.396021	4180.124863	23.855808
120.062646	4180.311738	23.860826
120.315427	4199.161318	23.865843
120.068127	4205.170773	23.870861
119.933246	4220.323152	23.875879
120.638237	4216.699195	23.880896
120.698392	4238.494334	23.885914
121.054332	4234.251303	23.890931
120.788009	4248.503019	23.895949
121.153992	4244.200060	23.900967
121.296715	4249.853360	23.905984
121.388522	4274.582596	23.911002
121.815908	4276.955106	23.916019
121.922619	4275.912208	23.921037
122.104620	4275.816682	23.926055
122.175615	4260.608468	23.931072
121.854604	4270.294581	23.936090
122.039465	4269.694268	23.941107
122.111732	4305.843760	23.946125
122.376622	4287.684664	23.951143
122.672180	4293.572560	23.956160
122.531124	4284.576350	23.961178
122.491202	4305.170833	23.966195
122.921819	4317.648045	23.971213
122.986769	4325.638963	23.976231
123.105233	4337.578813	23.981248
123.018135	4333.453058	23.986266
123.020175	4348.221135	23.991283
123.116678	4358.337510	23.996301
123.471159	4351.049096	24.001319
123.687001	4368.123141	24.006336
123.839433	4386.189551	24.011354
123.804046	4381.247777	24.016371
124.021942	4392.177560	24.021389
124.202954	4392.946350	24.026407
124.538960	4386.213716	24.031424
124.823931	4412.776170	24.036442
125.058180	4404.833991	24.041459
125.136526	4411.034590	24.046477
125.152669	4402.200914	24.051495
125.504725	4397.475421	24.056512
125.238171	4408.238423	24.061530
125.473705	4401.222785	24.066547
125.678647	4396.525932	24.071565
125.503408	4400.868868	24.076583
125.882650	4414.940046	24.081600
125.353780	4403.250823	24.086618
126.089669	4396.080067	24.091635
126.056844	4385.180916	24.096653
126.002021	4416.547449	24.101671
126.332373	4419.343489	24.106688
126.229493	4425.089011	24.111706
126.114908	4435.007252	24.116723
126.691435	4436.215403	24.121741
126.409017	4444.209060	24.126759
126.808556	4447.472796	24.131776
126.589060	4452.980517	24.136794
126.789395	4474.890223	24.141811
127.043288	4490.953016	24.146829
127.070350	4490.303180	24.151847
127.455860	4491.851556	24.156864
127.337363	4497.805982	24.161882
127.264298	4509.268566	24.166899
127.663424	4511.405236	24.171917
127.773181	4522.345107	24.176935
128.388385	4539.623424	24.181952
128.357673	4554.399077	24.186970
128.552506	4543.964552	24.191987
128.681490	4551.619420	24.197005
128.651635	4563.022148	24.202023
128.835778	4557.298381	24.207040
128.653653	4574.463218	24.212058
128.907941	4569.830206	24.217075
129.225480	4584.070788	24.222093
129.481499	4579.687878	24.227111
129.840703	4575.793031	24.232128
129.774795	4596.831954	24.237146
129.621895	4600.346458	24.242163
129.820488	4606.872144	24.247181
129.848633	4613.037419	24.252199
129.982427	4613.884102	24.257216
129.859522	4607.847672	24.262234
129.992008	4636.999071	24.267251
130.588734	4618.151690	24.272269
130.389752	4623.202542	24.277287
130.650541	4654.511890	24.282304
130.817434	4647.487405	24.287322
131.224687	4662.531339	24.292339
131.278754	4650.321982	24.297357
131.262160	4671.466636	24.302375
131.307589	4668.196448	24.307392
131.535403	4686.450356	24.312410
131.738296	4693.326154	24.317427
131.963751	4690.265976	24.322445
131.725240	4707.823741	24.327463
132.264855	4682.025109	24.332480
132.413747	4711.849920	24.337498
132.682333	4706.620805	24.342515
132.828361	4721.959143	24.347533
133.032047	4719.338383	24.352551
132.978840	4713.951023	24.357568
133.015075	4722.378780	24.362586
133.239484	4725.534114	24.367603
133.446345	4718.422678	24.372621
133.276939	4722.531668	24.377639
133.444092	4708.735077	24.382656
133.362482	4716.069314	24.387674
133.531876	4712.758160	24.392691
133.917129	4711.048341	24.397709
133.454978	4726.823401	24.402727
133.893177	4723.707984	24.407744
133.572104	4739.357382	24.412762
133.615044	4762.036022	24.417779
134.029548	4754.298132	24.422797
133.772620	4767.048768	24.427815
134.507754	4775.754767	24.432832
134.577058	4786.409382	24.437850
134.800515	4803.613752	24.442867
134.969398	4807.620801	24.447885
135.017900	4822.350549	24.452903
135.387872	4812.210528	24.457920
135.412657	4817.086276	24.462938
135.664160	4828.973024	24.467955
135.896121	4833.455093	24.472973
135.849501	4838.188315	24.477991
136.454055	4835.432003	24.483008
136.467743	4836.699728	24.488026
136.624261	4839.182049	24.493043
136.664226	4840.363542	24.498061
136.633575	4837.654318	24.503079
136.816892	4867.179249	24.508096
136.837721	4861.775667	24.513114
136.743816	4873.536453	24.518131
137.446256	4858.088272	24.523149
137.167125	4881.338026	24.528167
137.330661	4873.505326	24.533184
137.616600	4899.912155	24.538202
137.558287	4901.939429	24.543219
137.817976	4901.429090	24.548237
137.682927	4909.635644	24.553255
137.801626	4930.809082	24.558272
138.406593	4920.895911	24.563290
138.364356	4937.336056	24.568307
138.673079	4939.913322	24.573325
138.685400	4958.729937	24.578343
138.770156	4960.334359	24.583360
139.014165	4960.128189	24.588378
138.705727	4975.128090	24.593395
139.156228	4988.175008	24.598413
139.432959	4986.895697	24.603431
139.791043	4991.588864	24.608448
139.645445	4993.121116	24.613466
139.714040	5003.416936	24.618483
140.211214	4993.297512	24.623501
140.357879	5003.692639	24.628519
140.717563	5011.230477	24.633536
140.579491	5021.461639	24.638554
140.665813	5017.344447	24.643571
140.894972	5007.892934	24.648589
140.933763	5020.428374	24.653607
141.228767	5002.953246	24.658624
140.932405	5006.191148	24.663642
141.078719	5024.458134	24.668659
141.184607	5039.040806	24.673677
141.545852	5041.343658	24.678695
141.392000	5041.179214	24.683712
142.161166	5044.960753	24.688730
142.056012	5057.647570	24.693747
141.796216	5065.631900	24.698765
142.128216	5069.807344	24.703783
142.342584	5068.887158	24.708800
142.198878	5075.208182	24.713818
142.114678	5079.600042	24.718835
142.256330	5099.348233	24.723853
142.228301	5097.450754	24.728871
142.442849	5117.160544	24.733888
142.672477	5123.116739	24.738906
142.999909	5137.088472	24.743923
143.245207	5144.672836	24.748941
143.288241	5158.916392	24.753959
143.487705	5162.233816	24.758976
143.838085	5165.530241	24.763994
144.192190	5177.862913	24.769011
144.189242	5166.045655	24.774029
144.294047	5183.388165	24.779047
144.773518	5179.209904	24.784064
144.851057	5179.786379	24.789082
144.479751	5180.092130	24.794099
144.642516	5170.884961	24.799117
144.922824	5184.622391	24.804135
145.252949	5203.615141	24.809152
145.376506	5208.501857	24.814170
145.273951	5202.727982	24.819187
145.314779	5223.346953	24.824205
145.205735	5242.721778	24.829223
145.539080	5234.977770	24.834240
145.771496	5264.798502	24.839258
145.831597	5267.385409	24.844275
146.268790	5278.766211	24.849293
146.369401	5298.317099	24.854311
146.067550	5299.486209	24.859328
146.432039	5298.966023	24.864346
146.472718	5319.811926	24.869363
146.803904	5340.391734	24.874381
146.911976	5333.959360	24.879399
146.712420	5356.604918	24.884416
147.332230	5352.331371	24.889434
147.234006	5372.862883	24.894451
147.759598	5372.692073	24.899469
148.193659	5390.261127	24.904487
148.282546	5372.689718	24.909504
148.529067	5394.866723	24.914522
148.388549	5393.316943	24.919539
148.605490	5403.989713	24.924557
148.706397	5438.092924	24.929575
149.000376	5420.595844	24.934592
149.257328	5430.958859	24.939610
149.221355	5422.269442	24.944627
149.230889	5426.002576	24.949645
149.559418	5439.768879	24.954663
149.585585	5444.947759	24.959680
149.745424	5454.381518	24.964698
149.589168	5459.444477	24.969715
150.103095	5461.639876	24.974733
150.007783	5480.309545	24.979751
150.125519	5474.714532	24.984768
150.409831	5479.209399	24.989786
150.489452	5502.643722	24.994803
150.802139	5491.590242	24.999821
151.013939	5508.460689	25.004839
151.238535	5518.867299	25.009856
151.269860	5511.604973	25.014874
151.041714	5525.863751	25.019891
151.474346	5525.666173	25.024909
151.658862	5521.968079	25.029927
151.824768	5550.137272	25.034944
151.856235	5549.360673	25.039962
152.091931	5565.130719	25.044979
152.245701	5560.149046	25.049997
152.522785	5560.441368	25.055015
152.404266	5570.710999	25.060032
152.557971	5576.040905	25.065050
152.530600	5591.333552	25.070067
152.648345	5591.791976	25.075085
152.847168	5610.456900	25.080103
153.020333	5619.012131	25.085120
153.487688	5616.633890	25.090138
153.542907	5623.112432	25.095155
154.155102	5645.414814	25.100173
154.071836	5643.755149	25.105191
153.799211	5650.085502	25.110208
154.412478	5640.607541	25.115226
154.373343	5649.470719	25.120243
154.498286	5662.799967	25.125261
154.614831	5666.513901	25.130279
154.733522	5673.518228	25.135296
154.928136	5667.129689	25.140314
154.738660	5694.753106	25.145331
155.123920	5687.202672	25.150349
155.377281	5705.255906	25.155367
155.588894	5707.100090	25.160384
155.947214	5729.201614	25.165402
155.690570	5731.259798	25.170419
155.864575	5746.526410	25.175437
156.374212	5748.070943	25.180455
156.622338	5769.271382	25.185472
156.743903	5757.403966	25.190490
156.326274	5767.219968	25.195507
156.973326	5766.084143	25.200525
156.952077	5791.886510	25.205543
156.942801	5795.559450	25.210560
157.190904	5809.775621	25.215578
156.977649	5811.832158	25.220595
157.368521	5826.103892	25.225613
157.567103	5830.941002	25.230631
157.694679	5854.645902	25.235648
158.157207	5860.717452	25.240666
158.152924	5855.070020	25.245683
158.288209	5883.689788	25.250701
158.762028	5887.655786	25.255719
158.799505	5890.221730	25.260736
159.203178	5891.807412	25.265754
159.152941	5903.766891	25.270771
159.394932	5916.238370	25.275789
159.679809	5906.176670	25.280807
159.698980	5920.362655	25.285824
159.701015	5913.918428	25.290842
159.636290	5936.820127	25.295859
160.096446	5932.452326	25.300877
159.904995	5935.135245	25.305895
160.015593	5974.194704	25.310912
160.769126	5962.858189	25.315930
160.772223	5976.346826	25.320947
160.929884	5965.004039	25.325965
161.391878	5975.089815	25.330983
161.729686	5990.629623	25.336000
162.115386	5984.192449	25.341018
162.182124	5987.263457	25.346035
162.230162	5990.264716	25.351053
162.576421	5985.024311	25.356071
162.396781	5985.764976	25.361088
163.071981	5975.048137	25.366106
162.715287	5984.109659	25.371123
162.695804	5982.661483	25.376141
162.944495	5968.872749	25.381159
162.515637	5976.690580	25.386176
162.906794	5984.007534	25.391194
163.319718	5983.718714	25.396211
162.920972	5997.132813	25.401229
162.997483	5997.684290	25.406247
163.009944	6009.591361	25.411264
163.407189	6015.984808	25.416282
163.417186	6031.784746	25.421299
163.655127	6042.102881	25.426317
163.996655	6054.887185	25.431335
163.998510	6075.523172	25.436352
164.432600	6080.827000	25.441370
164.466537	6091.949416	25.446387
164.525057	6093.112977	25.451405
164.712737	6111.290536	25.456423
164.948919	6124.278148	25.461440
165.228066	6122.433733	25.466458
165.379282	6152.776318	25.471475
165.407730	6160.885638	25.476493
165.785405	6149.704017	25.481511
165.688234	6173.572534	25.486528
165.983144	6185.665766	25.491546
166.064939	6198.000934	25.496563
166.288133	6208.010169	25.501581
166.602001	6217.231913	25.506599
166.902875	6214.386166	25.511616
166.861145	6229.093566	25.516634
167.123451	6235.535781	25.521651
167.447547	6251.763614	25.526669
167.639348	6254.766367	25.531687
167.770832	6251.337520	25.536704
168.068875	6269.700591	25.541722
168.300279	6276.849573	25.546739
168.141249	6285.929005	25.551757
168.199823	6280.628942	25.556775
168.305647	6312.728723	25.561792
168.763950	6306.097907	25.566810
168.855745	6316.049388	25.571827
169.087337	6324.352415	25.576845
169.376395	6336.703843	25.581863
169.369255	6359.000914	25.586880
169.590192	6340.202931	25.591898
169.839799	6366.212303	25.596915
169.758551	6372.492816	25.601933
169.862549	6384.222825	25.606951
170.187890	6399.370571	25.611968
170.226461	6399.963374	25.616986
170.505607	6404.996036	25.622003
170.288441	6430.345162	25.627021
171.138254	6428.948995	25.632039
171.058874	6434.155093	25.637056
171.670225	6446.024961	25.642074
171.849861	6455.817512	25.647091
171.597250	6470.878130	25.652109
172.126068	6449.977734	25.657127
172.044299	6464.545892	25.662144
172.265222	6458.859848	25.667162
172.798482	6464.583297	25.672180
172.594127	6488.871230	25.677197
172.800132	6490.947170	25.682215
173.007353	6485.437022	25.687232
172.988045	6488.030560	25.692250
173.279255	6495.217797	25.697268
173.394306	6515.896690	25.702285
173.294991	6523.217769	25.707303
173.339836	6524.359603	25.712320
173.818010	6549.240443	25.717338
174.149722	6538.629199	25.722356
173.997761	6549.596415	25.727373
174.525148	6549.863937	25.732391
174.180096	6577.635105	25.737408
173.978887	6569.066852	25.742426
174.718499	6595.033831	25.747444
174.531961	6601.258991	25.752461
175.075313	6608.618029	25.757479
175.305129	6635.423339	25.762496
175.157810	6632.335002	25.767514
175.548498	6630.673303	25.772532
175.411094	6675.116688	25.777549
175.837301	6671.185451	25.782567
175.646200	6695.492776	25.787584
175.915126	6700.065353	25.792602
176.168832	6722.272983	25.797620
176.465741	6745.410634	25.802637
176.546944	6726.574246	25.807655
176.789113	6752.698889	25.812672
177.482457	6746.015272	25.817690
177.414982	6759.350475	25.822708
177.559353	6780.134729	25.827725
177.849503	6792.450113	25.832743
177.776127	6785.521860	25.837760
178.037905	6823.112205	25.842778
178.222911	6826.375282	25.847796
178.083743	6839.816901	25.852813
178.986391	6839.178610	25.857831
179.526070	6843.986056	25.862848
179.641894	6848.340635	25.867866
179.913178	6838.018740	25.872884
179.604191	6847.035467	25.877901
179.909765	6834.392243	25.882919
180.256751	6860.181593	25.887936
179.964012	6884.955279	25.892954
180.321431	6868.287557	25.897972
180.319398	6890.349074	25.902989
180.608121	6889.512971	25.908007
180.782407	6917.161518	25.913024
180.687830	6916.021768	25.918042
180.876762	6910.468031	25.923060
180.919390	6935.718738	25.928077
181.035571	6943.043780	25.933095
181.174457	6964.323743	25.938112
181.141861	6987.528010	25.943130
181.857046	6995.177388	25.948148
181.712309	7026.149785	25.953165
182.537989	7029.807115	25.958183
182.484343	7039.582271	25.963200
182.850591	7048.165052	25.968218
183.047382	7054.487310	25.973236
182.737962	7065.427746	25.978253
183.029659	7081.000278	25.983271
183.285125	7080.129891	25.988288
183.336311	7100.713793	25.993306
183.856467	7104.163318	25.998324
183.984459	7130.143259	26.003341
184.356728	7125.937316	26.008359
184.532649	7116.962300	26.013376
184.633877	7150.299783	26.018394
184.936950	7147.362941	26.023412
184.752489	7166.542338	26.028429
185.000638	7156.496147	26.033447
185.463906	7180.552767	26.038464
185.602114	7167.755800	26.043482
186.107140	7176.105451	26.048500
185.784615	7186.306288	26.053517
185.837500	7212.457068	26.058535
185.956902	7220.015209	26.063552
186.831849	7229.971746	26.068570
186.809999	7241.522372	26.073588
186.339016	7242.692002	26.078605
186.598117	7244.461585	26.083623
186.892057	7269.572469	26.088640
187.303809	7270.989220	26.093658
187.519136	7274.768725	26.098676
187.488727	7289.231507	26.103693
187.813925	7310.713869	26.108711
188.111833	7312.579426	26.113728
188.053108	7321.588542	26.118746
188.646327	7321.288421	26.123764
188.561074	7341.923535	26.128781
188.731355	7335.275698	26.133799
188.613949	7366.643921	26.138816
188.953058	7372.477360	26.143834
189.408562	7358.521325	26.148852
189.468209	7395.655021	26.153869
189.447006	7396.648751	26.158887
189.901974	7399.785437	26.163904
190.222064	7418.960526	26.168922
190.663324	7438.879527	26.173940
190.346371	7439.827623	26.178957
190.788156	7443.791836	26.183975
191.066050	7456.997324	26.188992
190.692525	7463.858943	26.194010
191.545856	7478.037268	26.199028
191.626445	7488.868664	26.204045
191.797541	7487.853113	26.209063
191.757062	7495.229894	26.214080
192.118328	7524.001573	26.219098
192.015482	7516.547457	26.224116
192.326677	7532.606280	26.229133
193.016743	7543.276367	26.234151
192.985335	7525.098295	26.239168
193.082283	7546.735251	26.244186
193.586139	7550.667184	26.249204
193.708632	7570.147597	26.254221
193.767048	7564.142671	26.259239
194.170287	7560.446549	26.264256
194.025759	7580.394794	26.269274
194.202752	7595.985217	26.274292
194.332271	7604.502676	26.279309
194.488558	7607.096523	26.284327
194.654038	7621.776108	26.289344
194.510709	7638.630747	26.294362
194.783466	7648.616177	26.299380
195.088147	7657.476445	26.304397
195.322522	7678.534866	26.309415
195.815027	7693.292790	26.314432
195.616543	7704.974536	26.319450
196.127079	7712.681712	26.324468
196.187692	7724.097784	26.329485
195.979772	7749.117523	26.334503
196.488597	7752.875425	26.339520
196.615569	7764.776719	26.344538
197.349592	7792.664305	26.349556
197.545925	7791.884770	26.354573
197.885016	7804.637045	26.359591
198.129742	7807.146220	26.364608
198.319019	7817.537754	26.369626
198.630041	7813.607156	26.374644
198.567189	7821.521749	26.379661
198.752308	7812.039996	26.384679
198.979130	7837.368431	26.389696
199.008078	7862.765830	26.394714
199.080581	7836.535561	26.399732
199.125144	7867.801626	26.404749
199.117116	7869.421681	26.409767
199.791238	7894.874764	26.414784
199.418271	7898.468105	26.419802
199.593430	7908.865182	26.424820
199.903021	7921.471215	26.429837
199.813531	7936.707501	26.434855
200.275372	7960.437928	26.439872
200.245933	7969.599300	26.444890
200.667730	7994.470487	26.449908
200.812555	8006.938424	26.454925
201.412109	8023.762083	26.459943
201.702774	8014.772324	26.464960
201.728781	8034.251928	26.469978
201.838002	8033.471811	26.474996
201.982682	8058.291229	26.480013
202.317963	8073.478725	26.485031
202.415559	8075.308956	26.490048
202.609845	8103.176804	26.495066
202.911334	8098.060843	26.500084
203.444047	8131.577194	26.505101
203.595943	8133.334665	26.510119
203.824559	8130.258733	26.515136
203.556977	8150.854151	26.520154
204.221820	8170.442587	26.525172
204.300533	8173.273017	26.530189
204.496845	8207.331834	26.535207
204.742923	8196.953755	26.540224
204.747298	8226.387396	26.545242
205.195078	8225.794691	26.550260
205.318514	8226.303841	26.555277
205.276287	8236.803211	26.560295
205.830115	8262.759552	26.565312
206.010194	8254.858249	26.570330
206.354191	8275.367740	26.575348
206.485541	8284.157768	26.580365
206.498238	8303.057094	26.585383
206.879931	8302.525710	26.590400
207.192603	8306.653243	26.595418
207.407742	8312.192486	26.600436
207.795403	8339.493246	26.605453
207.769327	8329.351431	26.610471
208.406433	8341.510682	26.615488
208.636350	8336.154445	26.620506
208.215653	8351.222971	26.625524
208.763498	8343.322289	26.630541
208.753588	8378.437832	26.635559
208.970119	8354.417280	26.640576
209.111576	8379.501578	26.645594
209.360192	8392.901710	26.650612
209.740021	8408.132575	26.655629
209.644270	8443.862587	26.660647
209.867904	8425.042770	26.665664
209.920552	8456.833988	26.670682
210.488380	8469.902636	26.675700
210.551748	8466.617667	26.680717
210.634104	8491.385845	26.685735
210.823029	8487.009792	26.690752
211.040768	8510.963317	26.695770
211.411218	8505.295544	26.700788
211.775214	8523.773223	26.705805
211.780346	8514.071122	26.710823
212.426754	8530.036985	26.715840
212.610790	8539.614705	26.720858
212.981331	8537.006702	26.725876
213.316651	8560.628201	26.730893
212.906508	8558.571337	26.735911
213.479701	8574.060247	26.740928
213.215326	8573.812028	26.745946
213.469322	8586.413604	26.750964
213.467796	8593.662384	26.755981
213.506642	8616.997438	26.760999
213.865660	8632.650173	26.766016
213.936873	8640.624934	26.771034
214.116998	8656.291498	26.776052
214.850918	8661.308817	26.781069
214.451118	8691.940312	26.786087
214.948283	8696.052429	26.791104
214.902189	8720.227862	26.796122
215.010214	8737.234315	26.801140
215.592759	8739.204236	26.806157
215.703592	8780.529080	26.811175
216.109785	8769.086897	26.816192
215.907722	8803.234089	26.821210
216.190903	8821.424604	26.826228
216.316553	8841.258126	26.831245
216.478676	8849.725978	26.836263
216.866338	8878.972275	26.841280
217.125616	8879.108516	26.846298
217.458879	8908.415050	26.851316
218.062787	8913.147553	26.856333
217.962720	8940.246400	26.861351
218.652878	8946.469000	26.866368
218.928905	8942.941653	26.871386
219.078532	8971.943124	26.876404
219.361163	8970.542024	26.881421
219.737900	8982.032791	26.886439
219.721759	8994.825037	26.891456
219.787923	9011.570913	26.896474
219.781634	9016.620076	26.901492
220.105327	9016.856730	26.906509
220.002729	9036.773893	26.911527
220.636396	9038.571582	26.916544
220.630863	9073.921867	26.921562
220.971218	9078.126943	26.926580
221.321692	9094.297438	26.931597
221.279452	9101.458664	26.936615
221.396264	9122.078468	26.941632
221.838940	9130.244139	26.946650
221.907648	9166.763009	26.951668
222.206676	9160.000984	26.956685
222.612257	9197.077821	26.961703
222.498509	9186.636468	26.966720
222.900439	9224.456703	26.971738
222.761279	9228.255084	26.976756
223.308412	9247.685521	26.981773
223.587647	9264.051477	26.986791
224.092488	9268.547629	26.991808
224.210176	9291.515429	26.996826
224.445283	9301.632576	27.001844
224.844360	9316.168024	27.006861
224.672125	9337.992110	27.011879
225.134552	9352.480893	27.016896
225.357108	9361.505343	27.021914
225.571551	9373.722629	27.026932
226.083759	9377.760768	27.031949
226.192122	9402.088938	27.036967
226.367473	9406.970377	27.041984
226.491518	9419.990271	27.047002
226.433361	9420.138799	27.052020
227.295618	9435.438234	27.057037
227.079329	9460.792079	27.062055
227.309738	9467.659527	27.067072
227.771618	9477.402208	27.072090
228.007361	9486.564750	27.077108
227.912096	9500.153390	27.082125
227.724787	9516.396634	27.087143
228.063808	9536.374566	27.092160
228.645648	9544.908917	27.097178
228.507453	9563.202202	27.102196
229.086016	9563.455040	27.107213
229.441448	9587.145638	27.112231
229.341345	9599.603318	27.117248
229.511417	9607.221970	27.122266
229.725193	9629.556870	27.127284
230.014552	9631.399706	27.132301
229.963527	9665.278050	27.137319
230.178991	9668.772983	27.142336
230.488463	9695.536077	27.147354
230.447615	9715.112286	27.152372
231.099148	9739.867139	27.157389
231.120576	9754.962397	27.162407
231.667881	9779.761313	27.167424
231.917152	9793.817067	27.172442
232.142815	9820.176761	27.177460
232.722055	9827.884657	27.182477
232.876566	9833.542362	27.187495
233.546727	9847.169449	27.192512
233.561244	9854.856456	27.197530
233.764397	9865.518789	27.202548
234.169857	9874.248658	27.207565
233.983568	9876.963285	27.212583
234.255992	9911.180965	27.217600
234.511676	9897.965401	27.222618
234.742121	9926.344829	27.227636
235.170601	9926.859559	27.232653
235.160924	9945.341567	27.237671
235.417249	9956.381918	27.242688
235.944828	9981.556186	27.247706
235.862929	9981.753539	27.252724
236.014526	9981.773682	27.257741
236.128141	10014.758351	27.262759
236.300488	10030.274754	27.267776
236.765925	10032.590288	27.272794
237.154400	10058.446152	27.277812
236.907278	10066.640426	27.282829
237.578388	10092.265332	27.287847
238.061586	10090.983806	27.292864
238.653064	10106.201032	27.297882
238.499237	10115.599230	27.302900
239.150897	10118.819762	27.307917
239.003863	10116.167846	27.312935
238.851500	10151.764551	27.317952
239.397004	10144.688851	27.322970
239.370833	10180.499497	27.327988
239.754187	10180.596349	27.333005
239.878172	10213.678964	27.338023
240.412387	10211.101151	27.343040
240.587620	10236.140273	27.348058
241.009998	10243.688399	27.353076
240.981368	10270.932097	27.358093
241.288215	10258.599433	27.363111
241.524336	10296.592979	27.368128
241.811430	10284.495924	27.373146
241.807599	10316.312016	27.378164
242.094145	10304.408018	27.383181
242.642795	10333.930509	27.388199
242.679649	10342.736507	27.393216
243.055452	10351.892950	27.398234
242.783792	10368.356584	27.403252
243.096237	10382.829346	27.408269
243.662605	10406.584777	27.413287
243.714581	10429.518608	27.418304
243.947154	10422.765454	27.423322
244.851958	10449.254226	27.428340
244.605144	10441.479085	27.433357
244.831449	10461.465780	27.438375
244.670834	10483.536063	27.443392
245.295024	10495.844051	27.448410
245.321067	10494.529328	27.453428
245.773515	10513.531134	27.458445
245.842704	10532.895609	27.463463
246.109708	10538.637380	27.468480
246.579146	10561.115669	27.473498
246.502285	10568.837023	27.478516
246.697445	10580.458992	27.483533
246.700886	10607.961844	27.488551
247.028746	10623.037228	27.493568
247.229924	10643.263823	27.498586
247.303570	10653.162750	27.503604
247.876989	10677.912284	27.508621
247.912180	10700.256928	27.513639
248.184291	10716.464871	27.518656
248.609008	10743.010613	27.523674
249.035345	10767.580573	27.528692
249.632132	10780.721187	27.533709
249.368401	10784.358559	27.538727
249.256579	10812.799271	27.543744
249.768398	10825.041010	27.548762
249.871540	10846.289962	27.553780
250.009399	10864.112980	27.558797
250.651526	10893.339853	27.563815
251.176161	10919.857565	27.568832
251.567448	10923.463152	27.573850
251.830780	10951.545947	27.578868
252.430557	10961.769321	27.583885
252.619237	10987.849547	27.588903
252.817133	10984.321272	27.593920
252.946848	10999.158778	27.598938
253.290424	11002.895149	27.603956
253.394080	11012.512065	27.608973
253.478948	11023.294759	27.613991
253.542177	11043.233508	27.619008
254.114956	11064.355528	27.624026
254.132000	11084.502827	27.629044
254.310277	11106.870087	27.634061
254.697819	11109.137212	27.639079
254.679169	11137.382720	27.644096
255.206595	11150.431122	27.649114
255.193395	11187.503026	27.654132
255.699338	11193.189014	27.659149
256.167103	11211.857492	27.664167
256.478937	11220.908424	27.669184
256.808263	11224.693678	27.674202
257.008113	11242.799123	27.679220
257.449367	11247.835704	27.684237
258.281088	11270.370934	27.689255
258.617213	11259.548250	27.694272
258.420828	11258.519136	27.699290
258.524218	11277.325093	27.704308
258.578022	11290.313223	27.709325
258.960384	11299.166643	27.714343
259.389859	11302.898346	27.719360
259.583016	11317.098634	27.724378
259.929397	11315.648204	27.729396
259.955571	11332.340901	27.734413
260.456241	11330.230067	27.739431
260.068829	11354.547821	27.744448
260.808789	11366.686903	27.749466
260.850838	11389.344109	27.754484
260.691960	11397.265319	27.759501
261.456635	11405.651524	27.764519
261.150232	11430.486153	27.769536
261.054119	11433.838387	27.774554
261.236696	11459.921180	27.779572
261.949812	11479.211922	27.784589
262.397501	11507.250268	27.789607
262.123911	11524.358204	27.794624
262.496243	11546.344261	27.799642
262.807459	11566.408903	27.804660
263.059426	11577.571625	27.809677
263.561866	11616.701990	27.814695
263.564290	11615.413134	27.819712
263.736717	11645.223150	27.824730
263.957086	11656.044540	27.829748
264.130491	11681.977963	27.834765
264.430797	11710.275766	27.839783
264.919165	11726.186685	27.844800
265.430395	11752.488216	27.849818
265.550186	11775.512819	27.854836
265.769673	11798.850265	27.859853
266.316375	11813.881166	27.864871
266.564833	11827.495346	27.869888
267.291899	11855.543288	27.874906
267.423784	11849.068494	27.879924
267.836309	11880.592037	27.884941
268.322562	11866.510397	27.889959
267.958884	11895.396400	27.894976
268.488696	11902.659732	27.899994
268.589422	11928.227438	27.905012
269.065779	11952.775206	27.910029
269.283966	11962.281603	27.915047
269.485413	11968.092230	27.920064
269.517342	11986.446835	27.925082
269.730630	12022.697066	27.930100
269.769139	12031.402099	27.935117
270.607578	12053.115690	27.940135
270.709096	12078.763858	27.945152
271.252917	12100.260712	27.950170
271.357401	12095.708563	27.955188
271.526479	12135.236378	27.960205
271.759326	12137.386626	27.965223
271.949742	12167.898910	27.970240
272.331799	12168.957867	27.975258
272.383045	12196.846287	27.980276
272.699548	12201.585525	27.985293
273.035536	12230.452638	27.990311
273.324675	12242.642457	27.995328
273.700474	12259.095590	28.000346
273.775965	12287.615897	28.005364
274.030933	12318.846496	28.010381
274.517516	12319.621925	28.015399
274.744562	12356.115636	28.020416
275.130610	12358.005056	28.025434
275.127151	12394.530636	28.030452
275.549960	12414.653532	28.035469
275.639871	12421.006628	28.040487
275.912492	12456.314512	28.045504
276.234360	12482.314509	28.050522
276.716287	12501.651776	28.055540
276.989091	12526.624798	28.060557
277.406473	12544.598090	28.065575
277.743527	12563.403188	28.070592
277.777400	12582.329301	28.075610
278.255729	12596.584445	28.080628
278.192861	12630.989400	28.085645
278.464048	12623.445877	28.090663
278.486939	12675.777197	28.095680
278.913755	12691.278565	28.100698
279.499341	12703.033735	28.105716
279.460785	12737.167047	28.110733
279.823442	12729.162469	28.115751
280.140232	12773.887408	28.120768
280.554281	12774.886764	28.125786
280.710812	12812.844293	28.130804
280.956397	12817.110145	28.135821
281.522649	12828.946594	28.140839
281.734263	12845.244685	28.145856
281.931717	12874.213838	28.150874
282.286966	12885.107524	28.155892
282.072181	12904.249204	28.160909
282.986558	12927.891021	28.165927
283.302975	12942.212615	28.170944
283.498430	12937.965049	28.175962
283.747235	12960.673821	28.180980
284.075958	12993.239126	28.185997
284.539285	12997.996097	28.191015
284.466114	13030.921733	28.196032
284.906855	13038.283810	28.201050
285.095799	13057.956920	28.206068
285.260065	13075.896997	28.211085
285.656754	13081.820729	28.216103
285.802849	13122.822473	28.221120
286.052778	13125.948504	28.226138
286.340309	13162.007842	28.231156
286.910545	13179.653280	28.236173
286.930146	13198.487937	28.241191
287.218619	13218.431567	28.246208
287.366517	13243.130118	28.251226
287.691233	13255.589780	28.256244
287.987426	13277.890955	28.261261
288.463997	13304.437897	28.266279
288.777094	13321.409053	28.271296
289.230932	13324.595185	28.276314
289.877122	13353.012062	28.281332
289.966755	13361.715672	28.286349
290.130053	13387.677155	28.291367
290.215577	13406.599643	28.296384
290.280168	13427.693728	28.301402
290.695719	13439.869874	28.306420
290.741472	13487.112223	28.311437
291.284415	13494.073160	28.316455
291.846084	13521.850395	28.321472
292.192746	13539.878241	28.326490
292.506116	13548.302332	28.331508
292.707967	13580.372965	28.336525
293.170938	13598.163428	28.341543
293.392096	13619.825142	28.346560
293.755327	13635.270173	28.351578
294.355886	13642.304380	28.356596
294.347233	13660.672327	28.361613
294.597241	13667.052250	28.366631
294.310287	13691.874544	28.371648
294.723992	13726.186552	28.376666
295.404031	13751.898586	28.381684
295.359545	13763.555371	28.386701
295.580315	13796.670359	28.391719
296.109727	13802.915935	28.396736
296.182893	13846.636262	28.401754
296.668812	13856.820434	28.406772
296.453550	13904.924921	28.411789
297.037153	13914.029385	28.416807
297.210103	13942.466401	28.421824
297.831757	13972.814739	28.426842
298.140849	13997.799018	28.431860
298.130027	14022.966976	28.436877
298.532243	14036.852288	28.441895
298.912464	14067.136695	28.446912
299.072247	14098.919858	28.451930
299.574229	14120.872266	28.456948
300.439862	14139.145157	28.461965
300.601626	14147.166009	28.466983
301.028689	14170.367816	28.472000
301.537891	14168.613699	28.477018
301.686348	14182.426033	28.482036
301.635408	14197.468886	28.487053
301.841663	14209.150745	28.492071
302.457717	14226.130316	28.497088
302.340157	14249.485247	28.502106
302.972904	14252.034559	28.507124
303.081882	14283.982479	28.512141
303.195752	14293.505128	28.517159
303.346091	14330.658891	28.522176
303.467488	14336.124331	28.527194
304.116489	14363.402468	28.532212
304.172519	14393.805655	28.537229
304.478509	14410.732648	28.542247
304.651042	14432.787184	28.547264
305.042188	14478.004081	28.552282
305.432366	14501.689916	28.557300
305.700735	14515.252660	28.562317
306.003684	14551.803408	28.567335
306.962883	14566.511104	28.572352
306.473108	14595.317187	28.577370
307.541591	14596.171512	28.582388
307.609008	14630.884598	28.587405
308.464271	14656.629007	28.592423
308.661448	14660.517282	28.597440
308.730627	14688.247891	28.602458
309.008281	14691.902266	28.607476
309.427098	14720.924042	28.612493
309.669995	14732.841323	28.617511
309.780137	14755.207582	28.622528
309.853667	14783.374131	28.627546
310.318926	14798.570203	28.632564
310.375034	14831.415112	28.637581
310.967772	14850.230276	28.642599
310.974315	14868.734177	28.647616
311.475319	14916.340405	28.652634
311.853623	14919.231269	28.657652
312.507681	14955.031562	28.662669
312.466127	14967.189836	28.667687
312.994153	14999.575770	28.672704
312.856373	15031.674662	28.677722
313.561750	15050.097980	28.682740
313.576850	15086.781010	28.687757
313.650064	15098.978727	28.692775
314.265116	15130.003210	28.697792
314.186400	15150.072136	28.702810
314.915340	15185.829050	28.707828
315.359180	15211.938575	28.712845
315.879345	15232.931380	28.717863
316.099519	15262.202834	28.722880
315.972524	15282.429605	28.727898
316.766574	15308.030733	28.732916
316.902323	15318.119252	28.737933
317.233181	15361.771149	28.742951
317.777332	15389.235380	28.747968
317.775702	15415.970382	28.752986
318.206256	15426.604362	28.758004
318.235689	15461.538239	28.763021
318.423736	15480.235045	28.768039
318.927068	15515.727394	28.773056
319.040309	15549.060713	28.778074
319.700508	15559.308571	28.783092
319.941861	15585.887093	28.788109
320.072657	15625.207574	28.793127
320.493580	15654.435536	28.798144
320.751163	15675.752803	28.803162
321.334248	15698.231330	28.808180
321.414603	15701.852345	28.813197
321.735376	15733.805947	28.818215
322.168907	15764.384139	28.823232
322.010670	15790.572003	28.828250
322.853884	15822.069129	28.833268
323.528068	15834.951332	28.838285
323.894087	15850.108055	28.843303
324.159236	15884.567371	28.848320
324.210951	15901.396100	28.853338
324.781489	15930.765311	28.858356
324.610054	15935.097739	28.863373
325.044795	15971.201260	28.868391
325.124705	15986.679588	28.873408
325.439567	16034.469557	28.878426
325.928791	16046.966444	28.883444
326.473822	16092.149805	28.888461
326.593036	16096.635974	28.893479
327.114486	16130.750890	28.898496
327.258018	16153.020575	28.903514
327.572592	16190.072658	28.908532
327.737984	16210.208146	28.913549
328.431206	16246.026878	28.918567
328.822082	16265.069302	28.923584
329.145582	16297.705942	28.928602
329.550873	16308.486510	28.933620
329.905897	16348.310663	28.938637
330.214330	16370.874896	28.943655
330.742284	16394.993030	28.948672
331.012376	16411.918586	28.953690
331.327542	16444.730253	28.958708
331.490642	16453.491152	28.963725
331.746934	16502.827155	28.968743
332.471135	16506.111887	28.973760
332.828801	16542.740021	28.978778
333.165247	16566.797067	28.983796
333.584740	16579.715637	28.988813
333.448344	16626.308507	28.993831
333.780791	16625.276773	28.998848
334.027853	16661.609827	29.003866
334.027831	16683.194761	29.008884
334.256473	16716.927459	29.013901
334.693331	16750.662075	29.018919
335.394752	16796.467705	29.023936
335.447623	16822.092810	29.028954
335.896401	16845.119918	29.033972
336.407549	16886.424667	29.038989
336.394204	16919.890443	29.044007
337.092100	16955.553937	29.049024
337.179214	16975.782102	29.054042
337.621567	17008.711001	29.059060
337.981109	17038.842035	29.064077
338.115074	17086.324548	29.069095
339.131850	17093.471174	29.074112
339.048795	17131.760493	29.079130
339.360928	17157.212480	29.084148
339.602403	17179.820413	29.089165
339.783998	17221.431042	29.094183
340.411654	17244.373999	29.099200
340.683350	17291.322139	29.104218
341.022041	17311.203403	29.109236
341.516040	17347.527128	29.114253
341.457466	17378.433932	29.119271
341.975378	17396.419649	29.124288
342.179593	17449.450338	29.129306
342.603396	17458.430331	29.134324
342.901105	17506.545799	29.139341
343.266542	17536.389931	29.144359
343.748658	17539.609278	29.149376
343.933696	17594.222820	29.154394
344.589705	17602.346549	29.159412
345.244701	17623.350108	29.164429
345.600205	17644.130512	29.169447
345.956151	17672.389353	29.174464
346.119306	17682.046113	29.179482
346.550330	17723.073060	29.184500
347.097791	17744.874702	29.189517
346.864478	17765.449930	29.194535
347.024581	17771.425510	29.199552
347.521831	17816.271640	29.204570
347.788591	17835.891184	29.209588
348.052812	17868.625861	29.214605
348.565106	17899.149330	29.219623
349.003757	17930.547151	29.224640
349.152592	17970.212300	29.229658
349.452730	18017.224014	29.234676
349.980786	18033.457697	29.239693
350.204936	18086.334266	29.244711
350.727087	18110.878291	29.249728
351.004342	18140.805864	29.254746
351.218974	18164.172975	29.259764
351.523099	18203.073828	29.264781
351.878560	18232.886200	29.269799
352.637469	18246.500254	29.274816
352.968800	18298.020084	29.279834
353.456918	18323.501546	29.284852
353.968197	18329.230177	29.289869
353.905511	18365.884547	29.294887
354.539878	18389.764231	29.299904
354.504505	18426.732605	29.304922
354.958602	18463.987441	29.309940
355.593254	18490.158951	29.314957
355.617203	18538.371528	29.319975
356.132428	18551.389326	29.324992
356.501641	18582.908620	29.330010
356.860930	18606.138976	29.335028
357.972740	18633.704024	29.340045
358.445685	18647.529578	29.345063
358.617377	18671.430944	29.350080
359.255513	18681.161134	29.355098
359.284509	18711.663507	29.360116
359.756766	18719.187682	29.365133
359.873664	18752.623061	29.370151
360.142301	18757.129408	29.375168
360.688834	18809.644531	29.380186
360.603864	18822.225798	29.385204
361.234611	18855.464584	29.390221
361.389131	18886.696809	29.395239
361.622769	18900.620431	29.400256
361.625071	18937.698787	29.405274
362.119426	18966.710901	29.410292
362.267346	19010.180501	29.415309
362.506176	19040.205901	29.420327
362.844056	19084.552210	29.425344
363.297918	19122.360248	29.430362
363.613313	19166.108376	29.435380
363.913164	19201.935512	29.440397
364.348427	19242.525780	29.445415
364.918832	19275.828974	29.450432
365.410552	19318.435557	29.455450
365.617820	19345.960514	29.460468
366.156853	19378.714263	29.465485
366.572212	19428.541893	29.470503
367.080667	19437.332448	29.475520
367.429711	19487.306768	29.480538
367.446988	19502.016936	29.485556
368.147368	19528.051562	29.490573
368.260596	19564.660613	29.495591
368.603865	19593.352012	29.500608
368.999555	19611.160164	29.505626
369.282715	19648.166916	29.510644
370.058758	19669.815129	29.515661
370.291785	19714.881890	29.520679
370.232586	19728.192554	29.525696
370.635206	19765.543952	29.530714
370.909395	19806.242604	29.535732
371.465295	19829.443778	29.540749
371.529608	19870.829842	29.545767
372.039004	19897.549186	29.550784
372.787338	19952.413223	29.555802
372.553131	19974.928610	29.560820
373.043209	20032.042391	29.565837
373.545086	20074.956624	29.570855
373.891000	20103.333208	29.575872
374.429994	20136.827755	29.580890
374.751816	20168.157711	29.585908
375.239881	20213.152166	29.590925
375.718104	20239.509929	29.595943
375.882331	20280.183773	29.600960
376.491067	20312.992487	29.605978
376.311715	20360.875094	29.610996
377.082431	20380.261505	29.616013
377.631312	20430.907125	29.621031
378.026248	20465.070857	29.626048
378.843160	20500.117060	29.631066
378.925301	20538.941857	29.636084
379.280681	20557.307833	29.641101
379.721277	20596.754531	29.646119
380.038907	20614.639713	29.651136
380.544262	20661.744848	29.656154
380.836443	20690.229047	29.661172
381.546428	20722.730217	29.666189
381.826487	20747.534124	29.671207
382.168189	20790.470363	29.676224
382.561910	20808.116185	29.681242
382.817865	20847.554572	29.686260
383.573104	20869.983375	29.691277
383.675122	20905.061837	29.696295
383.790082	20942.102414	29.701312
384.245453	20969.567008	29.706330
384.409615	21018.822967	29.711348
384.973925	21044.693293	29.716365
385.486652	21088.801686	29.721383
385.657727	21124.709424	29.726400
386.072679	21142.798217	29.731418
386.293344	21207.271925	29.736436
386.848931	21228.793077	29.741453
387.175724	21288.901814	29.746471
387.470207	21304.969221	29.751488
388.064390	21357.498733	29.756506
388.163152	21383.452801	29.761524
388.444055	21431.604533	29.766541
388.924049	21470.198670	29.771559
389.195753	21519.186110	29.776576
389.719306	21554.264085	29.781594
390.141959	21589.144405	29.786612
391.021427	21623.938296	29.791629
391.091486	21667.500229	29.796647
391.665666	21703.219653	29.801664
392.494322	21728.407329	29.806682
392.535554	21767.869177	29.811700
393.097394	21787.777295	29.816717
393.514597	21815.427731	29.821735
394.029587	21847.042654	29.826752
394.757594	21861.754153	29.831770
394.832874	21899.645248	29.836788
395.293784	21905.024017	29.841805
395.671561	21927.541830	29.846823
395.665032	21967.462913	29.851840
395.975738	21978.469349	29.856858
396.007811	22029.892557	29.861876
396.894396	22043.405111	29.866893
396.951421	22082.272330	29.871911
397.420749	22143.937093	29.876928
397.416434	22157.492868	29.881946
397.510299	22214.846700	29.886964
398.195185	22225.405239	29.891981
398.480390	22291.996027	29.896999
398.734502	22324.359653	29.902016
399.399289	22368.414778	29.907034
399.613466	22417.663444	29.912052
400.060617	22465.004000	29.917069
400.171280	22506.018460	29.922087
400.807089	22547.166981	29.927104
401.263342	22581.041141	29.932122
401.732900	22641.739701	29.937140
402.238890	22675.845472	29.942157
402.939908	22711.531909	29.947175
403.255534	22744.668156	29.952192
403.961777	22787.306515	29.957210
404.324716	22834.893783	29.962228
404.945069	22880.789567	29.967245
405.565170	22907.735094	29.972263
405.743788	22932.888508	29.977280
406.335178	22970.419283	29.982298
406.650082	22997.468977	29.987316
407.003969	23037.208514	29.992333
407.441234	23065.519868	29.997351
407.813417	23116.054625	30.002368
408.093644	23131.725690	30.007386
408.514126	23164.377195	30.012404
408.996849	23212.513319	30.017421
409.738563	23243.956263	30.022439
409.716661	23290.870546	30.027456
410.163311	23306.731853	30.032474
410.753740	23356.770910	30.037492
411.048349	23387.416116	30.042509
411.663200	23412.922294	30.047527
411.835497	23453.895776	30.052544
412.583774	23472.537453	30.057562
412.794134	23526.160408	30.062580
413.193731	23553.077182	30.067597
413.446825	23607.796981	30.072615
413.796172	23628.868117	30.077632
414.365785	23678.504796	30.082650
414.479834	23706.416551	30.087668
414.757265	23756.387101	30.092685
415.142885	23782.913965	30.097703
415.316077	23821.579970	30.102720
415.903438	23864.311653	30.107738
416.195791	23913.731526	30.112756
416.688792	23958.639071	30.117773
417.437071	24009.593689	30.122791
417.426840	24054.806934	30.127808
418.179130	24087.384920	30.132826
418.578056	24138.993627	30.137844
418.830093	24173.593748	30.142861
419.319189	24222.830661	30.147879
419.477541	24269.446695	30.152896
419.979099	24311.632381	30.157914
420.535186	24348.394748	30.162932
420.823579	24392.960417	30.167949
421.138145	24437.509266	30.172967
420.982223	24492.182822	30.177984
421.866235	24519.870968	30.183002
422.298939	24579.289687	30.188020
422.538006	24616.448735	30.193037
423.259476	24672.267697	30.198055
423.786053	24707.410103	30.203072
424.403399	24751.745780	30.208090
424.356097	24803.903257	30.213108
424.833727	24840.173518	30.218125
425.230664	24897.538444	30.223143
425.617847	24945.870318	30.228160
426.246230	24976.851155	30.233178
426.418206	25022.175639	30.238196
426.870569	25083.472390	30.243213
427.075080	25123.615213	30.248231
427.512877	25188.765248	30.253248
428.234139	25235.183727	30.258266
428.995084	25290.687580	30.263284
429.354464	25321.543193	30.268301
430.191724	25378.422309	30.273319
430.182569	25400.750097	30.278336
431.045411	25443.809239	30.283354
431.871831	25479.565976	30.288372
431.774448	25531.202573	30.293389
432.890913	25550.739708	30.298407
433.079555	25595.597807	30.303424
433.948435	25613.228537	30.308442
434.416991	25657.378293	30.313460
434.594522	25679.756027	30.318477
435.210943	25709.893423	30.323495
435.600638	25748.382993	30.328512
435.759132	25778.028496	30.333530
436.613881	25819.489436	30.338548
436.477921	25863.241307	30.343565
437.114609	25894.488938	30.348583
436.940978	25932.821265	30.353600
437.628742	25972.678119	30.358618
437.841265	26027.715195	30.363636
438.427118	26047.446210	30.368653
439.233622	26105.283694	30.373671
439.438481	26140.288262	30.378688
439.763359	26179.500686	30.383706
440.212000	26220.124563	30.388724
440.675813	26256.784895	30.393741
441.102110	26307.610392	30.398759
441.278303	26346.092430	30.403776
441.841093	26410.695088	30.408794
442.179756	26449.169442	30.413812
442.412727	26498.650809	30.418829
443.301112	26527.563625	30.423847
443.680876	26582.251597	30.428864
444.317789	26610.805561	30.433882
444.548969	26661.886691	30.438900
444.806603	26699.741074	30.443917
445.745094	26753.458948	30.448935
445.934020	26803.508285	30.453952
446.385621	26846.708303	30.458970
446.956816	26883.259204	30.463988
447.116154	26932.424409	30.469005
447.505142	26972.831277	30.474023
447.550581	27035.523764	30.479040
448.030225	27069.649058	30.484058
448.682263	27121.190320	30.489076
448.969948	27178.421709	30.494093
449.482128	27227.356008	30.499111
449.662813	27286.702810	30.504128
450.460819	27333.527507	30.509146
450.990558	27377.923929	30.514164
451.175971	27430.429474	30.519181
451.769340	27470.655517	30.524199
452.239936	27516.112348	30.529216
452.751983	27555.355360	30.534234
453.439460	27605.662164	30.539252
453.393270	27649.895801	30.544269
453.959776	27680.163205	30.549287
454.719031	27743.532028	30.554304
455.074250	27785.898746	30.559322
455.762181	27824.823148	30.564340
455.941176	27881.466105	30.569357
456.876098	27914.477034	30.574375
456.956868	27963.768569	30.579392
457.451157	28005.163477	30.584410
458.163299	28053.458364	30.589428
458.358499	28097.224319	30.594445
459.360707	28134.772784	30.599463
459.406085	28191.013028	30.604480
459.850409	28225.796211	30.609498
460.234415	28273.959831	30.614516
460.365014	28335.838693	30.619533
460.713813	28376.602466	30.624551
461.190957	28439.036360	30.629568
461.334110	28474.702499	30.634586
462.139497	28542.886237	30.639604
462.482939	28599.125889	30.644621
463.220509	28645.377472	30.649639
463.559454	28715.468387	30.654656
464.211850	28749.940687	30.659674
464.686379	28814.114354	30.664692
464.959395	28863.565962	30.669709
465.934326	28925.402093	30.674727
466.074514	28964.927398	30.679744
466.640736	29027.187841	30.684762
467.366091	29066.878521	30.689780
467.700026	29112.122423	30.694797
468.102143	29158.295163	30.699815
468.876724	29203.983822	30.704832
469.662993	29254.831140	30.709850
470.151454	29296.643334	30.714868
470.549535	29341.905631	30.719885
471.136077	29388.591069	30.724903
471.514955	29422.346547	30.729920
471.812651	29457.443486	30.734938
472.027767	29507.032676	30.739956
472.756142	29559.770459	30.744973
473.263078	29612.932971	30.749991
473.674623	29673.461150	30.755008
473.950114	29712.631447	30.760026
474.162518	29754.824719	30.765044
474.223375	29804.569574	30.770061
475.094181	29865.981504	30.775079
475.485596	29922.003038	30.780096
475.751462	29971.127780	30.785114
476.258752	30037.679035	30.790132
476.558129	30086.871122	30.795149
477.084969	30153.542617	30.800167
477.509513	30210.537502	30.805184
477.913363	30282.422108	30.810202
478.763924	30329.454477	30.815220
478.864943	30399.250829	30.820237
479.298903	30461.172356	30.825255
479.975615	30527.807915	30.830272
480.536177	30582.895131	30.835290
481.145015	30627.671717	30.840308
481.351221	30695.738952	30.845325
482.146766	30739.182141	30.850343
482.417974	30792.860400	30.855360
482.891337	30851.855651	30.860378
483.444494	30890.837630	30.865396
483.808018	30954.457116	30.870413
484.169840	31011.704741	30.875431
485.319213	31064.592076	30.880448
485.616070	31117.629860	30.885466
486.242132	31153.287993	30.890484
486.530622	31204.456707	30.895501
487.127566	31268.250145	30.900519
487.813639	31310.842154	30.905536
487.978326	31361.088525	30.910554
488.794516	31416.312819	30.915572
489.100907	31459.712423	30.920589
489.657056	31520.096959	30.925607
490.432115	31559.466515	30.930624
490.624936	31625.451156	30.935642
491.472221	31681.068651	30.940660
491.607116	31723.058668	30.945677
491.893152	31778.441088	30.950695
492.147778	31826.093332	30.955712
492.619691	31884.612791	30.960730
493.443874	31934.477405	30.965748
493.711249	32007.587347	30.970765
494.320032	32046.928684	30.975783
495.244035	32107.538422	30.980800
496.243769	32157.822664	30.985818
496.663443	32210.606868	30.990836
496.899653	32259.951184	30.995853
497.394673	32306.987689	31.000871
498.094842	32358.830022	31.005888
498.378550	32409.444642	31.010906
499.060753	32457.494901	31.015924
498.992920	32520.762280	31.020941
499.583184	32557.173757	31.025959
499.922144	32625.933288	31.030976
500.176364	32674.540697	31.035994
501.095934	32743.678023	31.041012
501.379175	32800.925561	31.046029
501.936854	32873.290759	31.051047
502.240053	32912.454207	31.056064
502.296778	32991.509178	31.061082
503.166829	33056.223145	31.066100
503.466342	33127.518318	31.071117
503.978627	33185.685246	31.076135
504.527697	33246.004340	31.081152
505.099866	33314.822696	31.086170
505.847142	33375.936119	31.091188
506.070346	33459.881287	31.096205
506.643450	33510.981330	31.101223
507.219026	33570.170790	31.106240
507.750758	33640.467376	31.111258
508.575098	33705.727656	31.116276
508.955970	33762.346946	31.121293
509.346369	33828.039044	31.126311
510.214393	33875.576597	31.131328
510.593172	33944.647065	31.136346
511.414452	33983.383406	31.141364
511.846032	34048.416401	31.146381
512.468267	34111.938355	31.151399
513.171458	34164.583786	31.156416
513.231121	34220.487734	31.161434
513.985757	34263.634072	31.166452
514.438609	34332.747462	31.171469
514.952717	34382.610305	31.176487
515.406503	34438.159557	31.181504
515.548810	34506.854791	31.186522
516.438909	34548.341866	31.191540
516.781374	34600.817847	31.196557
517.246609	34654.699898	31.201575
517.890969	34699.285400	31.206592
518.039979	34775.259851	31.211610
518.854489	34812.957879	31.216628
519.122886	34880.116023	31.221645
519.579170	34930.621030	31.226663
520.397179	34984.458434	31.231680
520.914291	35039.876056	31.236698
521.627957	35088.221749	31.241716
522.198969	35146.256069	31.246733
522.543457	35193.927829	31.251751
523.662111	35245.965127	31.256768
523.855191	35298.035559	31.261786
524.411850	35345.846228	31.266804
524.926566	35397.078124	31.271821
525.254290	35457.523375	31.276839
525.470541	35500.878416	31.281856
525.918342	35572.739559	31.286874
526.695108	35632.663158	31.291892
527.284175	35701.753076	31.296909
527.725544	35742.108525	31.301927
528.464359	35805.652010	31.306944
528.541291	35871.229913	31.311962
529.527725	35928.232584	31.316980
530.090627	35979.568644	31.321997
530.223510	36054.730793	31.327015
530.660349	36109.798970	31.332032
530.799777	36184.641874	31.337050
531.950420	36256.269771	31.342068
532.544074	36317.002195	31.347085
532.822095	36382.731788	31.352103
533.602523	36444.197449	31.357120
533.554167	36508.331030	31.362138
534.446995	36570.466486	31.367156
535.191859	36646.006540	31.372173
535.530293	36699.376120	31.377191
536.404944	36761.562580	31.382208
536.928965	36810.272473	31.387226
537.320624	36892.719730	31.392244
537.858988	36937.615527	31.397261
538.484206	37018.850867	31.402279
539.169129	37075.203289	31.407296
539.569233	37122.154673	31.412314
540.256892	37202.197133	31.417332
540.909378	37251.407707	31.422349
541.336786	37326.409791	31.427367
541.960564	37385.537743	31.432384
542.065911	37439.105819	31.437402
542.972325	37517.677673	31.442420
543.445659	37573.325000	31.447437
543.683050	37644.989398	31.452455
544.439486	37702.423897	31.457472
544.972228	37781.465732	31.462490
545.640966	37839.991301	31.467508
546.302233	37902.324273	31.472525
546.326646	37958.725458	31.477543
546.912995	38028.052045	31.482560
547.644025	38091.055820	31.487578
548.034313	38171.306363	31.492596
548.929355	38234.532868	31.497613
549.214244	38304.781352	31.502631
550.109785	38356.384884	31.507648
550.441862	38443.431545	31.512666
550.733602	38484.909862	31.517684
551.574038	38560.997651	31.522701
551.402078	38620.150646	31.527719
552.566836	38697.974892	31.532736
552.798421	38750.468759	31.537754
552.940555	38820.929039	31.542772
553.560458	38884.881822	31.547789
554.045049	38962.232533	31.552807
554.394106	39025.485723	31.557824
554.911119	39111.779166	31.562842
555.685077	39183.058071	31.567860
555.942416	39253.800838	31.572877
556.545953	39322.255324	31.577895
557.287760	39410.747594	31.582912
558.143953	39483.172401	31.587930
558.573447	39565.647750	31.592948
558.847172	39631.086939	31.597965
559.468120	39733.001852	31.602983
560.389132	39782.733642	31.608000
560.817279	39872.539301	31.613018
561.445312	39944.056775	31.618036
562.206554	40008.419434	31.623053
562.530586	40084.185468	31.628071
563.180117	40165.850766	31.633088
563.680160	40239.192771	31.638106
564.481977	40320.315981	31.643124
565.415087	40380.396893	31.648141
565.564534	40470.832305	31.653159
566.259728	40536.280893	31.658176
567.041292	40608.599428	31.663194
567.691098	40688.278535	31.668212
568.485087	40733.943282	31.673229
568.585978	40818.451325	31.678247
569.479119	40880.740489	31.683264
570.074501	40952.033752	31.688282
570.570866	41029.864798	31.693300
571.068088	41088.643853	31.698317
571.615916	41164.491052	31.703335
572.127350	41226.216315	31.708352
573.110430	41304.236438	31.713370
573.715370	41362.029549	31.718388
574.376860	41446.125944	31.723405
574.763780	41485.518437	31.728423
575.464260	41580.934509	31.733440
576.153238	41634.431221	31.738458
576.239410	41703.658784	31.743476
577.740510	41767.441453	31.748493
578.362617	41824.368301	31.753511
578.921022	41894.468708	31.758528
579.075838	41944.320343	31.763546
579.369760	42004.335423	31.768564
580.247066	42067.672930	31.773581
580.786289	42145.889913	31.778599
581.395070	42216.627181	31.783616
581.807868	42269.631587	31.788634
582.423465	42356.763799	31.793652
583.315527	42403.369835	31.798669
583.464369	42493.957409	31.803687
584.360263	42538.445034	31.808704
584.752291	42607.253003	31.813722
585.539662	42676.194803	31.818740
586.267759	42728.722304	31.823757
586.350177	42814.688386	31.828775
587.035795	42867.911467	31.833792
587.443992	42946.788008	31.838810
588.125339	43019.767144	31.843828
588.553203	43085.328996	31.848845
588.803264	43173.112614	31.853863
589.590956	43241.759746	31.858880
590.174642	43316.656580	31.863898
590.481121	43390.156839	31.868916
591.002609	43455.145787	31.873933
591.345962	43554.214109	31.878951
592.126268	43613.914188	31.883968
592.670175	43691.019444	31.888986
593.210612	43762.506342	31.894004
593.612822	43848.402325	31.899021
593.782012	43927.859212	31.904039
594.942061	44014.101173	31.909056
595.269516	44074.076425	31.914074
595.660817	44177.149477	31.919092
596.431801	44250.686931	31.924109
596.940620	44346.262663	31.929127
597.655476	44421.653745	31.934144
598.383277	44524.957284	31.939162
598.831038	44592.257556	31.944180
599.618795	44684.884501	31.949197
600.027683	44782.928853	31.954215
600.674654	44867.441073	31.959232
601.292635	44947.241780	31.964250
601.847964	45043.252257	31.969268
602.402453	45126.300250	31.974285
602.748194	45214.914383	31.979303
603.704885	45315.775628	31.984320
604.640980	45391.370896	31.989338
605.274149	45473.785485	31.994356
606.265170	45546.335110	31.999373
606.860291	45631.206658	32.004391
607.495437	45710.638415	32.009408
608.298311	45788.751502	32.014426
608.675103	45883.302433	32.019444
609.621826	45962.841665	32.024461
610.103503	46048.728387	32.029479
611.010828	46109.410066	32.034496
611.347609	46186.992449	32.039514
611.917035	46256.422450	32.044532
612.497453	46351.444131	32.049549
613.179082	46418.087229	32.054567
613.714710	46490.573667	32.059584
614.563547	46577.500934	32.064602
614.879422	46664.049340	32.069620
615.725933	46735.468705	32.074637
616.604222	46826.752618	32.079655
617.045885	46884.015324	32.084672
617.771730	46973.784315	32.089690
618.307446	47043.601697	32.094708
618.862138	47115.553798	32.099725
619.416400	47185.441266	32.104743
620.103220	47285.871479	32.109760
621.003838	47342.080963	32.114778
621.158596	47434.980832	32.119796
621.842067	47506.092210	32.124813
622.363715	47608.610130	32.129831
622.999748	47669.515342	32.134848
623.729302	47761.229376	32.139866
624.372810	47834.022101	32.144884
625.016171	47927.683616	32.149901
625.722250	48012.253974	32.154919
626.078249	48096.295216	32.159936
626.880803	48175.842397	32.164954
627.425947	48235.425618	32.169972
627.712660	48335.157050	32.174989
628.231771	48430.988793	32.180007
628.845963	48516.703879	32.185024
629.586590	48588.643534	32.190042
630.262371	48689.869324	32.195060
630.702060	48771.787239	32.200077
631.604295	48869.329412	32.205095
632.117091	48957.147353	32.210112
632.802840	49021.203323	32.215130
633.156861	49110.349200	32.220148
633.799882	49180.418873	32.225165
634.463553	49266.255495	32.230183
635.052588	49348.517544	32.235200
635.812227	49443.228395	32.240218
636.313824	49517.629967	32.245236
636.789295	49612.735962	32.250253
637.319475	49696.967121	32.255271
637.746551	49794.027272	32.260288
638.391054	49890.369898	32.265306
638.782374	49983.356896	32.270324
639.818296	50072.063081	32.275341
640.546053	50172.707139	32.280359
640.722555	50267.107873	32.285376
641.625548	50357.353172	32.290394
642.318752	50457.230733	32.295412
643.312786	50551.984186	32.300429
643.932886	50654.609704	32.305447
644.310246	50749.087022	32.310464
645.150463	50839.733414	32.315482
645.412086	50932.408547	32.320500
646.186873	51033.696789	32.325517
647.106110	51126.586377	32.330535
647.833192	51224.466425	32.335552
648.834735	51329.505388	32.340570
649.201799	51430.319867	32.345588
650.136974	51518.455683	32.350605
650.585581	51622.163233	32.355623
651.097932	51712.198371	32.360640
652.037822	51814.654124	32.365658
652.704621	51894.915151	32.370676
653.387400	51992.260061	32.375693
654.127514	52086.447193	32.380711
654.524332	52183.976109	32.385728
655.337679	52264.685063	32.390746
655.970238	52368.997925	32.395764
656.713628	52448.958051	32.400781
657.337907	52561.342873	32.405799
658.109954	52639.508271	32.410816
658.820534	52729.180645	32.415834
659.262590	52817.729179	32.420852
660.313289	52931.634408	32.425869
660.844447	52999.307738	32.430887
661.146975	53117.124581	32.435904
661.984425	53205.063178	32.440922
662.651015	53297.553330	32.445940
663.529321	53394.348724	32.450957
664.374521	53479.848937	32.455975
664.657849	53579.870445	32.460992
665.461186	53665.264685	32.466010
666.369979	53773.036010	32.471028
666.616201	53851.334218	32.476045
667.272989	53939.659752	32.481063
668.194214	54031.492274	32.486080
669.303994	54142.890114	32.491098
670.091396	54210.367428	32.496116
671.003569	54290.010387	32.501133
671.968432	54369.221712	32.506151
672.396937	54468.118294	32.511168
673.108176	54514.477783	32.516186
673.478107	54608.646745	32.521204
674.171389	54691.025020	32.526221
674.410158	54778.715859	32.531239
675.166349	54875.753607	32.536256
675.960894	54944.299942	32.541274
676.415077	55060.334636	32.546292
677.009319	55125.515862	32.551309
677.671028	55218.300261	32.556327
677.859854	55314.119839	32.561344
678.769946	55390.583574	32.566362
679.027441	55483.530756	32.571380
679.518439	55582.700646	32.576397
680.670182	55658.177865	32.581415
681.371423	55761.363595	32.586432
682.056721	55847.090159	32.591450
682.788653	55942.203975	32.596468
683.256194	56050.679925	32.601485
684.128626	56122.780798	32.606503
684.335027	56233.448962	32.611520
685.046073	56306.758613	32.616538
685.894445	56417.890406	32.621556
686.493783	56513.989224	32.626573
687.473320	56617.379900	32.631591
687.993190	56708.065609	32.636608
688.813543	56812.690351	32.641626
689.495892	56891.731113	32.646644
689.858592	56995.162468	32.651661
690.912754	57090.215991	32.656679
692.179979	57185.196877	32.661696
692.910949	57257.350551	32.666714
693.689536	57363.981682	32.671732
694.429516	57456.112958	32.676749
694.959965	57555.463204	32.681767
695.894524	57639.993851	32.686784
696.604693	57725.920371	32.691802
697.132208	57818.840316	32.696820
697.927169	57921.029910	32.701837
698.446299	58010.331672	32.706855
698.750065	58107.674945	32.711872
699.471977	58197.443223	32.716890
700.071616	58301.493095	32.721908
700.800495	58404.890308	32.726925
701.486948	58495.885283	32.731943
701.973176	58623.372412	32.736960
702.695300	58713.161946	32.741978
703.431440	58809.419944	32.746996
703.916328	58936.384848	32.752013
704.849972	59029.590925	32.757031
705.416991	59150.439676	32.762048
706.387422	59247.160288	32.767066
706.991635	59360.655335	32.772084
707.618851	59471.322664	32.777101
708.281082	59575.210891	32.782119
709.072022	59688.866536	32.787136
710.002928	59783.068676	32.792154
710.686963	59903.890029	32.797172
711.124275	60014.440074	32.802189
711.811753	60125.410713	32.807207
712.430056	60248.172339	32.812224
713.427026	60346.220924	32.817242
714.082571	60465.723340	32.822260
714.584074	60579.741492	32.827277
715.683875	60672.352745	32.832295
716.497138	60800.760304	32.837312
717.213956	60873.239089	32.842330
718.060095	60982.109193	32.847348
718.993997	61091.388797	32.852365
719.838408	61200.652177	32.857383
720.119591	61287.612821	32.862400
721.003361	61398.735031	32.867418
721.565942	61501.588018	32.872436
722.226828	61622.341387	32.877453
722.969882	61725.563848	32.882471
723.586797	61822.481673	32.887488
724.362958	61931.273672	32.892506
725.306412	62030.944522	32.897524
725.709693	62128.436275	32.902541
726.328807	62232.768798	32.907559
726.900840	62337.823776	32.912576
727.438865	62443.011313	32.917594
728.162795	62537.298467	32.922612
728.568497	62638.502057	32.927629
729.549300	62756.883636	32.932647
730.314285	62865.202186	32.937664
731.419893	62979.772457	32.942682
732.170408	63064.394340	32.947700
732.583709	63193.812221	32.952717
733.700713	63278.810561	32.957735
734.607433	63394.035388	32.962752
735.377092	63488.907188	32.967770
735.790467	63608.139541	32.972788
736.750786	63712.631892	32.977805
737.114599	63818.411505	32.982823
737.662746	63934.741457	32.987840
738.651394	64051.416470	32.992858
739.543714	64155.517817	32.997876
739.972453	64284.959037	33.002893
740.754248	64386.147128	33.007911
741.308352	64502.921764	33.012928
742.214329	64621.105323	33.017946
743.044718	64738.682630	33.022964
743.571072	64863.086524	33.027981
744.444392	64970.077357	33.032999
745.212539	65111.356896	33.038016
745.492471	65220.311633	33.043034
746.749046	65352.454568	33.048052
747.426980	65451.237895	33.053069
748.394883	65596.880740	33.058087
748.936506	65708.911025	33.063104
749.680579	65832.892940	33.068122
750.553105	65953.472677	33.073140
751.232804	66081.158154	33.078157
751.836440	66195.494325	33.083175
752.726785	66325.769755	33.088192
753.516386	66450.146087	33.093210
754.366771	66556.422027	33.098228
755.114300	66689.624737	33.103245
755.815184	66811.508387	33.108263
756.825243	66937.886676	33.113280
757.317641	67054.881931	33.118298
758.352823	67178.444566	33.123316
758.911831	67298.944855	33.128333
759.755371	67421.725130	33.133351
760.740542	67543.730491	33.138368
761.442846	67669.911205	33.143386
762.288765	67785.265501	33.148404
762.947021	67909.008514	33.153421
763.771063	68009.954542	33.158439
764.495291	68137.373497	33.163456
765.308373	68256.060995	33.168474
766.118394	68389.321175	33.173492
766.709102	68522.220153	33.178509
767.272727	68632.732733	33.183527
768.220155	68761.389313	33.188544
768.791226	68873.602502	33.193562
769.616718	69002.192192	33.198580
770.258756	69142.230356	33.203597
771.249383	69252.233156	33.208615
772.113191	69376.285972	33.213632
772.944319	69511.421118	33.218650
773.949743	69607.679244	33.223668
774.396978	69738.415870	33.228685
775.163852	69847.592612	33.233703
776.224438	69968.411107	33.238720
776.965627	70076.474255	33.243738
777.936225	70181.971179	33.248756
778.295039	70283.801591	33.253773
779.307680	70405.218480	33.258791
780.276251	70512.848010	33.263808
780.691650	70632.588259	33.268826
781.714261	70727.710641	33.273844
782.176712	70856.896376	33.278861
783.101567	70973.285724	33.283879
783.862434	71076.735338	33.288896
784.141692	71201.097744	33.293914
785.235522	71309.285994	33.298932
785.682823	71452.153584	33.303949
786.618936	71560.489290	33.308967
786.931430	71697.456474	33.313984
787.655009	71820.269622	33.319002
788.441112	71963.369221	33.324020
789.115477	72089.960421	33.329037
789.982811	72234.780878	33.334055
790.685939	72378.352211	33.339072
791.440994	72511.173279	33.344090
792.508779	72634.876397	33.349108
792.947472	72777.849143	33.354125
794.243794	72908.844473	33.359143
795.083427	73040.738024	33.364160
795.861890	73194.033624	33.369178
796.857956	73318.960261	33.374196
797.631624	73458.069362	33.379213
798.699885	73584.964791	33.384231
799.783484	73734.287129	33.389248
800.147722	73852.656466	33.394266
801.034460	73986.761217	33.399284
802.065186	74118.338960	33.404301
803.201418	74240.339046	33.409319
803.856069	74380.403312	33.414336
805.082402	74482.534180	33.419354
805.828490	74623.286834	33.424372
806.625420	74740.040322	33.429389
807.141159	74870.000326	33.434407
807.932826	74988.811204	33.439424
808.401233	75120.323500	33.444442
809.722958	75262.053958	33.449460
809.879825	75396.357552	33.454477
810.760341	75512.582854	33.459495
811.636055	75665.892615	33.464512
812.097271	75800.148447	33.469530
812.915709	75928.585018	33.474548
813.507898	76072.357390	33.479565
814.419828	76231.540127	33.484583
815.224889	76361.840725	33.489600
815.711195	76518.661082	33.494618
816.652065	76659.331529	33.499636
817.307321	76810.750565	33.504653
818.146139	76958.421692	33.509671
819.355122	77108.486506	33.514688
819.443495	77263.278256	33.519706
820.735729	77411.712376	33.524724
821.827032	77571.400172	33.529741
822.411130	77713.072317	33.534759
823.478842	77858.694213	33.539776
823.973082	78017.800804	33.544794
825.006168	78164.473990	33.549812
826.045216	78324.555361	33.554829
826.347398	78474.412423	33.559847
827.347019	78620.543925	33.564864
828.186037	78782.982821	33.569882
829.121839	78918.475954	33.574900
830.200648	79062.902262	33.579917
831.297202	79185.100991	33.584935
832.429410	79311.614416	33.589952
832.818844	79464.208782	33.594970
834.213700	79565.007340	33.599988
835.586831	79686.081592	33.605005
836.351011	79812.165295	33.610023
837.353101	79917.483146	33.615040
837.831157	80052.957601	33.620058
838.725317	80153.411405	33.625076
839.664370	80284.560650	33.630093
840.213341	80400.891851	33.635111
841.224812	80523.440907	33.640128
841.805324	80653.683766	33.645146
842.700098	80776.158601	33.650164
843.249336	80920.304907	33.655181
844.279501	81032.189115	33.660199
845.141375	81182.901849	33.665216
845.559865	81309.639365	33.670234
846.503771	81450.327136	33.675252
846.868721	81583.198131	33.680269
847.626744	81744.659918	33.685287
848.659270	81874.006578	33.690304
849.096605	82036.946684	33.695322
850.213692	82171.993180	33.700340
851.079170	82336.851031	33.705357
851.513690	82496.537160	33.710375
852.112931	82638.370986	33.715392
852.923586	82805.385773	33.720410
853.757190	82964.237548	33.725428
854.592082	83135.729533	33.730445
855.362387	83310.377518	33.735463
856.453709	83456.329372	33.740480
857.085066	83639.599968	33.745498
858.058010	83792.336156	33.750516
858.955998	83953.683064	33.755533
859.841516	84139.863736	33.760551
860.855591	84277.103379	33.765568
861.850855	84473.947453	33.770586
862.762617	84611.737418	33.775604
863.635042	84782.052583	33.780621
864.835080	84939.826439	33.785639
865.801147	85105.465932	33.790656
866.629042	85271.641892	33.795674
867.732919	85428.346822	33.800692
868.681911	85587.514164	33.805709
869.145715	85751.001616	33.810727
870.337646	85906.062978	33.815744
870.871168	86058.646446	33.820762
871.868927	86223.289135	33.825780
872.747636	86386.092555	33.830797
873.545118	86556.097924	33.835815
874.456439	86701.720585	33.840832
875.452978	86857.029396	33.845850
876.680531	87023.107709	33.850868
877.397291	87179.059622	33.855885
878.330121	87341.974722	33.860903
879.609992	87492.128676	33.865920
880.058510	87667.457712	33.870938
881.000335	87802.344946	33.875956
881.984111	87946.767610	33.880973
882.916562	88118.476844	33.885991
883.680282	88270.163687	33.891008
884.274318	88430.674669	33.896026
885.403705	88581.309746	33.901044
886.507416	88740.568116	33.906061
887.387540	88899.680989	33.911079
888.171991	89053.413294	33.916096
889.008386	89191.603664	33.921114
890.253167	89352.747523	33.926132
891.085021	89464.414606	33.931149
891.577270	89623.957119	33.936167
892.672411	89772.226269	33.941184
893.360956	89913.027037	33.946202
894.105168	90061.577429	33.951220
895.013232	90200.388353	33.956237
895.927295	90368.510187	33.961255
897.045827	90514.729888	33.966272
897.890815	90668.108374	33.971290
898.612614	90817.312680	33.976308
899.313727	90987.283905	33.981325
900.082836	91139.595865	33.986343
900.894105	91288.547892	33.991360
901.783012	91468.072454	33.996378
902.553197	91629.114035	34.001396
903.257272	91790.781469	34.006413
904.031408	91963.563727	34.011431
905.117004	92124.354067	34.016448
905.937854	92307.807160	34.021466
906.693290	92482.735287	34.026484
907.805963	92654.549009	34.031501
908.276361	92825.172649	34.036519
909.493802	93004.667175	34.041536
910.118015	93193.931260	34.046554
911.083813	93385.773197	34.051572
911.923389	93560.385178	34.056589
912.611440	93758.990812	34.061607
913.832215	93928.840181	34.066624
914.579202	94115.914096	34.071642
916.003863	94301.187721	34.076660
917.168611	94488.556293	34.081677
917.618317	94660.525441	34.086695
919.040142	94851.582210	34.091712
920.343973	95011.982392	34.096730
921.551492	95186.222570	34.101748
922.543938	95360.012155	34.106765
923.168299	95526.781250	34.111783
924.236884	95700.978431	34.116800
924.600735	95891.401568	34.121818
925.824318	96064.525069	34.126836
926.484835	96239.141586	34.131853
927.496647	96438.152398	34.136871
928.505350	96610.941801	34.141888
929.404979	96791.402970	34.146906
930.286448	96962.671423	34.151924
931.423404	97153.445108	34.156941
932.587278	97326.296208	34.161959
933.248658	97516.170110	34.166976
934.071100	97701.714562	34.171994
935.127833	97897.520514	34.177012
936.092830	98073.201181	34.182029
936.832936	98254.212122	34.187047
937.842110	98427.349669	34.192064
938.632664	98630.225404	34.197082
939.569916	98813.828544	34.202100
940.440983	99004.483160	34.207117
941.174962	99179.260265	34.212135
942.161161	99387.978020	34.217152
943.156452	99567.778948	34.222170
944.054178	99761.448195	34.227188
944.828209	99942.674710	34.232205
945.897824	100132.956983	34.237223
947.366166	100318.414297	34.242240
948.548385	100508.161720	34.247258
949.651340	100683.888642	34.252276
950.926662	100846.768711	34.257293
951.961424	100997.483933	34.262311
953.013175	101173.140425	34.267328
953.681934	101335.952875	34.272346
954.420839	101500.888284	34.277364
955.480245	101665.936454	34.282381
956.098641	101827.943701	34.287399
957.052131	102002.754843	34.292416
957.818446	102175.496199	34.297434
958.615481	102351.810702	34.302452
959.688567	102527.770624	34.307469
960.383876	102704.686828	34.312487
961.478201	102885.849915	34.317504
962.370700	103080.482484	34.322522
962.960716	103271.988175	34.327540
963.883935	103442.059400	34.332557
964.618318	103641.192254	34.337575
965.593100	103830.416280	34.342592
966.654002	104043.117225	34.347610
967.280906	104224.145352	34.352628
968.418144	104433.544534	34.357645
969.170927	104636.588635	34.362663
970.192218	104850.974337	34.367680
970.984874	105050.551686	34.372698
971.974265	105262.052468	34.377716
973.245001	105467.942854	34.382733
974.253085	105677.766009	34.387751
975.281056	105897.724983	34.392768
976.758456	106084.742339	34.397786
977.439238	106299.360860	34.402804
978.954214	106504.294650	34.407821
980.039821	106691.507688	34.412839
980.957497	106894.605530	34.417856
981.703137	107094.947176	34.422874
982.678735	107302.521823	34.427892
983.561998	107486.899104	34.432909
984.568580	107710.821886	34.437927
985.693368	107910.347265	34.442944
986.901157	108110.430372	34.447962
987.602072	108317.159161	34.452980
988.881562	108507.190080	34.457997
989.790599	108724.349068	34.463015
991.131276	108922.187300	34.468032
991.791917	109142.253078	34.473050
992.596305	109335.876696	34.478068
993.590907	109536.588382	34.483085
994.384117	109744.275629	34.488103
995.688764	109972.309985	34.493120
996.298773	110163.425875	34.498138
997.235581	110389.269988	34.503156
998.233300	110617.069194	34.508173
999.075046	110826.086761	34.513191
1000.281327	111041.062263	34.518208
1001.795506	111243.157578	34.523226
1002.313855	111473.905791	34.528244
1003.586839	111663.567569	34.533261
1004.588893	111899.306193	34.538279
1005.730243	112097.479444	34.543296
1006.968471	112317.792557	34.548314
1007.663285	112526.226856	34.553332
1009.067546	112739.143780	34.558349
1009.619834	112936.483040	34.563367
1010.689501	113152.295884	34.568384
1012.380134	113354.289130	34.573402
1013.177683	113577.548016	34.578420
1014.272912	113772.396848	34.583437
1015.507046	113974.242022	34.588455
1016.731185	114174.722211	34.593472
1018.325285	114356.407028	34.598490
1019.110331	114537.783243	34.603508
1020.381393	114723.602891	34.608525
1021.073780	114909.671347	34.613543
1021.903796	115092.639963	34.618560
1022.909211	115272.553115	34.623578
1023.813769	115456.575963	34.628596
1025.024367	115644.793433	34.633613
1025.532644	115826.059094	34.638631
1026.729440	116008.339769	34.643648
1027.678124	116209.766986	34.648666
1028.149869	116413.111373	34.653684
1029.162215	116609.222740	34.658701
1030.215172	116826.194571	34.663719
1031.210824	117018.181475	34.668736
1032.161563	117228.255988	34.673754
1033.217494	117440.835886	34.678772
1034.103019	117651.152372	34.683789
1034.913898	117862.432960	34.688807
1036.220024	118062.078751	34.693824
1037.012354	118302.847709	34.698842
1037.629753	118521.804960	34.703860
1038.879051	118743.256894	34.708877
1039.513984	118977.456581	34.713895
1040.917437	119192.551598	34.718912
1042.003808	119424.171764	34.723930
1043.142917	119655.240283	34.728948
1043.996796	119884.482550	34.733965
1045.150256	120123.192697	34.738983
1045.378127	120361.614172	34.744000
1046.542825	120591.418961	34.749018
1047.661847	120841.024852	34.754036
1048.732736	121066.502850	34.759053
1049.514931	121319.374216	34.764071
1050.816175	121574.278172	34.769088
1051.950450	121799.865462	34.774106
1053.157752	122075.113914	34.779124
1054.368306	122311.995393	34.784141
1055.186376	122555.570795	34.789159
1056.282055	122803.347389	34.794176
1057.725549	123038.979838	34.799194
1058.582180	123300.460227	34.804212
1060.022670	123537.871240	34.809229
1061.285963	123795.145174	34.814247
1062.116450	124022.941352	34.819264
1063.399513	124273.398584	34.824282
1064.344416	124508.060649	34.829300
1065.688478	124747.562916	34.834317
1066.731659	124991.324081	34.839335
1067.652604	125218.354170	34.844352
1069.312358	125454.578495	34.849370
1070.501808	125693.239488	34.854388
1072.003275	125921.408362	34.859405
1073.468595	126130.550029	34.864423
1074.388086	126350.301969	34.869440
1075.604763	126567.915373	34.874458
1076.783538	126785.359184	34.879476
1078.346258	127010.687411	34.884493
1079.313632	127216.192859	34.889511
1080.146797	127431.112992	34.894528
1081.299700	127632.687178	34.899546
1082.464340	127862.472568	34.904564
1083.299757	128075.533855	34.909581
1084.336935	128290.717897	34.914599
1084.768834	128505.737231	34.919616
1086.386794	128717.152934	34.924634
1087.222603	128943.540734	34.929652
1088.097369	129156.248195	34.934669
1089.296960	129380.348490	34.939687
1090.329958	129616.379274	34.944704
1092.105875	129802.820320	34.949722
1093.113650	129994.763360	34.954740
1094.299346	130200.899274	34.959757
1094.792930	130397.061667	34.964775
1095.899306	130628.144901	34.969792
1096.727774	130826.181313	34.974810
1097.310055	131051.118122	34.979828
1098.506783	131272.051167	34.984845
1099.682469	131504.257566	34.989863
1100.833756	131713.337191	34.994880
1102.198203	131944.628428	34.999898
1102.922873	132150.561841	35.004916
1104.044619	132385.661033	35.009933
1105.036316	132620.796129	35.014951
1105.816668	132853.939740	35.019968
1107.258242	133091.475865	35.024986
1108.153065	133327.278692	35.030004
1109.155622	133548.171078	35.035021
1110.546296	133781.258800	35.040039
1111.165464	134033.629457	35.045056
1112.297406	134271.922737	35.050074
1113.399603	134522.873832	35.055092
1114.256151	134760.151395	35.060109
1115.674147	135017.329141	35.065127
1116.431162	135267.709224	35.070144
1117.843279	135531.661458	35.075162
1118.977803	135785.710252	35.080180
1119.684040	136032.795972	35.085197
1121.191336	136295.534419	35.090215
1121.963210	136554.593219	35.095232
1123.117874	136817.026462	35.100250
1124.563339	137084.332679	35.105268
1125.496634	137346.299630	35.110285
1126.774789	137607.083436	35.115303
1127.919490	137874.318988	35.120320
1128.984200	138131.452962	35.125338
1130.023227	138402.069891	35.130356
1131.131398	138675.973932	35.135373
1132.223542	138941.426528	35.140391
1133.196683	139219.680628	35.145408
1134.740137	139472.486096	35.150426
1135.935219	139755.399053	35.155444
1137.085097	140015.791975	35.160461
1138.425885	140274.633968	35.165479
1139.253375	140564.131310	35.170496
1140.621261	140816.785754	35.175514
1141.670016	141101.217669	35.180532
1142.795402	141368.852174	35.185549
1144.099398	141642.583379	35.190567
1144.937064	141915.354072	35.195584
1146.215105	142194.888471	35.200602
1147.480870	142466.147460	35.205620
1148.145764	142733.006528	35.210637
1149.653766	143006.943266	35.215655
1150.490801	143279.763014	35.220672
1151.871052	143562.499722	35.225690
1153.002839	143841.196796	35.230708
1154.225701	144126.018275	35.235725
1155.743189	144392.825559	35.240743
1156.877030	144679.137191	35.245760
1158.151813	144948.283953	35.250778
1159.362855	145211.584909	35.255796
1160.367139	145462.304753	35.260813
1161.738122	145735.068361	35.265831
1163.054525	146012.192625	35.270848
1164.425363	146293.165089	35.275866
1165.553910	146535.743611	35.280884
1166.438293	146802.813279	35.285901
1167.888250	147026.180957	35.290919
1169.263629	147294.644299	35.295936
1170.484185	147531.152794	35.300954
1171.207259	147779.335833	35.305972
1172.203976	148032.421229	35.310989
1173.372324	148278.784177	35.316007
1174.228137	148553.493345	35.321024
1175.425918	148803.380556	35.326042
1176.620427	149079.115780	35.331060
1178.013808	149321.961196	35.336077
1179.549886	149569.984342	35.341095
1180.694609	149838.022856	35.346112
1182.109435	150082.480462	35.351130
1183.279446	150342.186265	35.356148
1184.101251	150618.578086	35.361165
1185.633678	150857.618742	35.366183
1186.788482	151127.643530	35.371200
1187.829737	151378.943983	35.376218
1189.260164	151650.537811	35.381236
1190.184880	151907.809339	35.386253
1191.483528	152166.314591	35.391271
1192.433065	152432.894974	35.396288
1193.682773	152706.885419	35.401306
1194.878518	152963.967315	35.406324
1195.695244	153245.998270	35.411341
1197.370306	153520.457159	35.416359
1198.037437	153806.093743	35.421376
1198.959840	154082.862541	35.426394
1200.084430	154353.308862	35.431412
1201.111862	154647.872404	35.436429
1202.714059	154930.204843	35.441447
1203.661362	155241.731924	35.446464
1204.584892	155514.845276	35.451482
1205.682050	155826.606061	35.456500
1206.755113	156140.999004	35.461517
1207.846312	156444.470233	35.466535
1209.099555	156737.655322	35.471552
1210.190623	157065.688663	35.476570
1211.455482	157374.795845	35.481588
1212.608457	157676.198889	35.486605
1214.095577	157986.606129	35.491623
1215.143328	158305.726848	35.496640
1216.243138	158608.224051	35.501658
1217.834367	158940.528833	35.506676
1219.254920	159244.665096	35.511693
1220.835992	159547.838469	35.516711
1221.695287	159867.142414	35.521728
1222.771505	160162.741739	35.526746
1224.520903	160468.266520	35.531764
1225.933486	160788.919961	35.536781
1227.143274	161089.007509	35.541799
1227.933268	161401.497369	35.546816
1229.810680	161712.110202	35.551834
1231.122604	162000.947751	35.556852
1232.049801	162313.701060	35.561869
1233.528742	162627.101492	35.566887
1234.642964	162933.536208	35.571904
1235.827705	163229.444395	35.576922
1236.833617	163534.150699	35.581940
1237.926445	163847.903239	35.586957
1239.305712	164157.639878	35.591975
1240.137043	164472.759716	35.596992
1241.159342	164796.705959	35.602010
1242.420360	165115.210572	35.607028
1243.697330	165426.191428	35.612045
1245.257149	165743.357360	35.617063
1246.671647	166063.607320	35.622080
1248.423838	166342.303091	35.627098
1249.896369	166639.900607	35.632116
1250.936863	166937.038620	35.637133
1252.222796	167229.659393	35.642151
1253.523445	167517.191892	35.647168
1254.613048	167810.737159	35.652186
1256.059891	168080.359275	35.657204
1256.876622	168391.742114	35.662221
1258.129027	168690.341686	35.667239
1259.155418	168992.317618	35.672256
1260.739227	169286.171881	35.677274
1262.009871	169579.927533	35.682292
1262.983693	169896.446617	35.687309
1264.025242	170194.152228	35.692327
1265.363847	170516.414219	35.697344
1266.498288	170822.508625	35.702362
1267.799800	171130.392056	35.707380
1268.893600	171447.562147	35.712397
1269.710514	171774.461931	35.717415
1270.887820	172102.675017	35.722432
1272.294604	172428.835004	35.727450
1273.724537	172750.311132	35.732468
1274.841337	173095.697345	35.737485
1276.451729	173413.823702	35.742503
1277.396537	173742.937115	35.747520
1278.858456	174093.844576	35.752538
1280.596942	174415.928555	35.757556
1281.892034	174753.150845	35.762573
1283.271354	175067.062852	35.767591
1284.467574	175410.270471	35.772608
1285.777440	175738.220943	35.777626
1287.290922	176078.513069	35.782644
1288.594193	176397.776364	35.787661
1289.863744	176749.991699	35.792679
1291.196092	177072.122730	35.797696
1291.989150	177421.934296	35.802714
1293.311400	177755.581936	35.807732
1294.743066	178105.343793	35.812749
1295.930130	178433.777105	35.817767
1297.968584	178765.409816	35.822784
1299.152292	179118.417961	35.827802
1300.613860	179434.096226	35.832820
1301.564428	179787.541053	35.837837
1303.190783	180121.852584	35.842855
1304.315982	180455.703341	35.847872
1305.396947	180780.933421	35.852890
1306.853199	181140.650071	35.857908
1307.814495	181475.664188	35.862925
1309.634438	181834.475393	35.867943
1310.874100	182147.948199	35.872960
1311.992394	182507.590677	35.877978
1313.502599	182846.584585	35.882996
1314.906757	183193.188074	35.888013
1316.416520	183528.239284	35.893031
1317.771994	183862.061581	35.898048
1319.106659	184212.122909	35.903066
1320.399549	184531.554020	35.908084
1321.546269	184894.825605	35.913101
1322.989487	185221.635783	35.918119
1324.969931	185565.570511	35.923136
1326.249404	185891.751799	35.928154
1327.676494	186232.786656	35.933172
1328.989478	186559.067995	35.938189
1330.349912	186889.303664	35.943207
1331.685161	187227.339010	35.948224
1332.809689	187544.175662	35.953242
1334.172278	187883.543315	35.958260
1335.288499	188210.666645	35.963277
1336.440664	188523.772540	35.968295
1337.972175	188837.566494	35.973312
1339.205820	189161.680387	35.978330
1340.363456	189469.522881	35.983348
1341.699509	189793.471185	35.988365
1343.176854	190107.319236	35.993383
1344.478355	190443.272478	35.998400
1345.594748	190759.658973	36.003418
1346.836413	191087.120999	36.008436
1348.194097	191428.871841	36.013453
1349.881585	191746.832399	36.018471
1351.219218	192078.498605	36.023488
1352.524108	192420.086255	36.028506
1354.186285	192740.544448	36.033524
1355.338622	193073.452800	36.038541
1356.503607	193410.765886	36.043559
1357.747076	193739.588018	36.048576
1358.710051	194087.753948	36.053594
1360.433732	194434.552266	36.058612
1361.719378	194794.703509	36.063629
1362.831971	195146.291085	36.068647
1364.382348	195494.368125	36.073664
1365.376739	195849.114856	36.078682
1366.843819	196219.540079	36.083700
1368.037016	196569.332459	36.088717
1368.724856	196939.573183	36.093735
1370.367146	197294.563962	36.098752
1371.158330	197678.756686	36.103770
1372.763034	198050.464882	36.108788
1373.955573	198448.890963	36.113805
1374.866451	198842.820999	36.118823
1376.487045	199230.720152	36.123840
1377.571394	199624.816724	36.128858
1378.901549	200033.843365	36.133876
1380.092517	200427.343134	36.138893
1381.151838	200832.839179	36.143911
1382.769766	201235.388892	36.148928
1383.833577	201665.392436	36.153946
1385.154758	202073.887076	36.158964
1386.473839	202505.199576	36.163981
1388.107911	202913.901499	36.168999
1389.462805	203345.149845	36.174016
1390.915695	203768.525586	36.179034
1392.587672	204191.156711	36.184052
1394.503238	204607.084446	36.189069
1395.930398	205028.884885	36.194087
1397.509340	205427.097615	36.199104
1398.866152	205847.873315	36.204122
1400.153060	206272.167312	36.209140
1401.899963	206681.799048	36.214157
1403.077108	207127.370761	36.219175
1404.542257	207529.067234	36.224192
1405.881860	207961.920003	36.229210
1407.241492	208365.009624	36.234228
1409.020781	208791.369744	36.239245
1410.613103	209200.748606	36.244263
1412.426120	209618.130678	36.249280
1413.624261	210028.302690	36.254298
1415.494866	210428.372869	36.259316
1416.919775	210830.575631	36.264333
1418.299921	211236.533617	36.269351
1420.098197	211631.212518	36.274368
1421.968870	212023.430706	36.279386
1423.508968	212421.939981	36.284404
1424.665834	212824.844417	36.289421
1425.877084	213222.446757	36.294439
1427.633536	213614.018308	36.299456
1428.635738	213990.833953	36.304474
1430.031878	214440.905503	36.309492
1431.631253	214825.626109	36.314509
1432.837892	215183.670632	36.319527
1434.235563	215574.954745	36.324544
1435.284058	215946.412523	36.329562
1437.080692	216331.335723	36.334580
1438.553799	216712.021870	36.339597
1439.897526	217087.372174	36.344615
1441.396921	217476.692198	36.349632
1442.369863	217870.824649	36.354650
1443.648301	218254.876365	36.359668
1445.422727	218673.617036	36.364685
1446.347666	219052.498441	36.369703
1448.046817	219451.267007	36.374720
1449.012903	219855.948908	36.379738
1450.315652	220259.891185	36.384756
1451.579683	220682.864662	36.389773
1452.983035	221112.903039	36.394791
1454.349070	221521.564056	36.399808
1455.765336	221954.804068	36.404826
1457.641996	222367.701932	36.409844
1459.118221	222804.745392	36.414861
1460.349089	223225.372804	36.419879
1461.942999	223659.149350	36.424896
1463.064649	224095.037499	36.429914
1464.457086	224513.128806	36.434932
1466.098447	224961.964341	36.439949
1467.484041	225401.776381	36.444967
1469.111950	225837.968852	36.449984
1471.401705	226268.923095	36.455002
1473.224038	226695.663574	36.460020
1475.242620	227111.502208	36.465037
1476.879049	227524.890806	36.470055
1478.979310	227953.393350	36.475072
1480.610911	228347.456358	36.480090
1482.320524	228746.257549	36.485108
1483.814857	229146.975152	36.490125
1485.278233	229564.615606	36.495143
1486.913336	229946.287851	36.500160
1488.356332	230349.303738	36.505178
1489.611019	230753.698166	36.510196
1490.814639	231144.995654	36.515213
1491.779228	231550.430998	36.520231
1493.804976	231973.726837	36.525248
1495.181291	232377.318659	36.530266
1496.648689	232814.704963	36.535284
1498.044490	233211.107570	36.540301
1499.318449	233640.958904	36.545319
1501.231798	234044.238229	36.550336
1502.579861	234461.709493	36.555354
1503.720272	234887.674744	36.560372
1505.402756	235282.968765	36.565389
1506.755884	235724.395931	36.570407
1508.191804	236138.224890	36.575424
1509.281020	236575.252757	36.580442
1510.822408	236999.227062	36.585460
1511.986360	237455.600818	36.590477
1513.452861	237879.411910	36.595495
1515.234359	238319.784720	36.600512
1516.691982	238761.507573	36.605530
1517.730319	239205.129636	36.610548
1519.121219	239655.654698	36.615565
1520.452475	240098.036703	36.620583
1521.908728	240559.069526	36.625600
1523.460983	241009.418779	36.630618
1525.039967	241476.834816	36.635636
1526.563945	241932.906279	36.640653
1527.636640	242385.903352	36.645671
1529.072365	242826.902459	36.650688
1530.465382	243287.951888	36.655706
1532.266137	243717.969589	36.660724
1533.449410	244185.279039	36.665741
1535.119345	244638.131362	36.670759
1536.230520	245102.736470	36.675776
1537.971432	245554.334074	36.680794
1539.271868	246022.110381	36.685812
1540.998721	246477.420704	36.690829
1542.160487	246949.641588	36.695847
1543.821578	247407.733206	36.700864
1545.947022	247881.854256	36.705882
1547.324247	248340.654660	36.710900
1549.672878	248791.674625	36.715917
1550.961315	249262.100118	36.720935
1552.587661	249732.216499	36.725952
1554.289800	250191.296166	36.730970
1555.708374	250666.985929	36.735988
1557.471214	251137.081652	36.741005
1558.411020	251611.810087	36.746023
1560.592389	252085.114865	36.751040
1562.023344	252559.458508	36.756058
1563.756221	253033.346388	36.761076
1565.531751	253517.160319	36.766093
1566.744056	253984.479420	36.771111
1568.668452	254457.905204	36.776128
1570.150956	254928.762374	36.781146
1571.688664	255421.736979	36.786164
1573.348488	255883.928530	36.791181
1574.888858	256378.986461	36.796199
1576.095392	256844.987691	36.801216
1577.766965	257352.929419	36.806234
1578.989732	257840.013192	36.811252
1580.681925	258332.125791	36.816269
1582.025462	258843.170762	36.821287
1583.436071	259339.597957	36.826304
1585.268131	259849.368697	36.831322
1586.827401	260342.570808	36.836340
1588.491385	260856.510226	36.841357
1589.759422	261369.803741	36.846375
1591.150336	261868.724135	36.851392
1592.916692	262401.470583	36.856410
1594.574259	262913.048581	36.861428
1596.267767	263430.234701	36.866445
1597.868362	263952.440491	36.871463
1599.760929	264483.260478	36.876480
1601.467568	264989.037920	36.881498
1602.929445	265510.224521	36.886516
1604.755729	266015.194275	36.891533
1605.974312	266526.716457	36.896551
1607.823111	267041.233538	36.901568
1609.245271	267553.788415	36.906586
1611.118099	268098.225762	36.911604
1613.039011	268595.735075	36.916621
1614.980669	269123.063836	36.921639
1616.745124	269627.736352	36.926656
1618.603586	270132.418268	36.931674
1620.233300	270647.222420	36.936692
1621.905365	271149.088862	36.941709
1623.453724	271649.527165	36.946727
1625.208889	272157.932673	36.951744
1626.870124	272659.773660	36.956762
1628.344611	273168.478168	36.961780
1630.101115	273670.556077	36.966797
1631.349636	274184.961229	36.971815
1632.840586	274677.656998	36.976832
1634.495419	275195.143440	36.981850
1635.841453	275711.689247	36.986868
1637.719663	276199.796968	36.991885
1639.013364	276706.086949	36.996903
1640.976190	277197.811528	37.001920
1642.275518	277684.030711	37.006938
1643.503466	278187.077182	37.011956
1645.275569	278685.257198	37.016973
1646.869944	279176.759285	37.021991
1648.785741	279689.189614	37.027008
1650.535311	280172.611443	37.032026
1652.175296	280689.809815	37.037044
1653.886336	281193.201866	37.042061
1655.594222	281692.757517	37.047079
1657.533263	282193.569313	37.052096
1659.221002	282714.895282	37.057114
1660.310022	283217.038618	37.062132
1662.210959	283735.126012	37.067149
1663.608550	284253.879248	37.072167
1664.703876	284782.384307	37.077184
1666.573667	285311.344246	37.082202
1668.233056	285833.199462	37.087220
1669.814130	286383.642595	37.092237
1671.491569	286902.570342	37.097255
1672.988462	287456.122729	37.102272
1674.753329	287980.290627	37.107290
1676.108162	288540.365335	37.112308
1677.784940	289083.721822	37.117325
1679.448240	289646.738845	37.122343
1681.035839	290200.875917	37.127360
1683.296275	290761.935830	37.132378
1684.587461	291325.337872	37.137396
1686.489672	291880.356246	37.142413
1688.386991	292437.532186	37.147431
1690.282486	293005.729812	37.152448
1691.841106	293551.298204	37.157466
1693.660661	294126.361486	37.162484
1695.602936	294666.578589	37.167501
1697.543013	295224.065583	37.172519
1699.184478	295780.100713	37.177536
1700.854563	296336.712736	37.182554
1702.285943	296905.375465	37.187572
1703.960560	297464.470528	37.192589
1705.595437	298042.237835	37.197607
1706.984193	298607.952820	37.202624
1709.009525	299174.829838	37.207642
1710.605324	299757.039467	37.212660
1712.009497	300339.709334	37.217677
1713.672591	300921.520522	37.222695
1715.103504	301512.256207	37.227712
1716.998325	302104.181869	37.232730
1718.321298	302702.471743	37.237748
1719.659322	303292.323429	37.242765
1721.591047	303898.582186	37.247783
1723.360794	304487.364909	37.252800
1725.444230	305084.549607	37.257818
1727.157154	305690.350540	37.262836
1729.119628	306280.614097	37.267853
1731.189497	306891.605465	37.272871
1733.155918	307476.806620	37.277888
1735.268597	308075.211458	37.282906
1737.262224	308660.120956	37.287924
1738.940469	309238.246950	37.292941
1740.878398	309814.980220	37.297959
1742.668357	310395.365608	37.302976
1744.663003	310961.821723	37.307994
1746.459686	311553.194318	37.313012
1747.906175	312118.767888	37.318029
1749.593977	312694.760539	37.323047
1751.481918	313271.782625	37.328064
1753.362538	313813.959948	37.333082
1755.042897	314381.434287	37.338100
1756.727124	314935.749480	37.343117
1758.244339	315481.047841	37.348135
1759.443828	316036.552365	37.353152
1761.430060	316593.243478	37.358170
1762.852174	317164.345575	37.363188
1764.660768	317718.162648	37.368205
1766.993779	318271.762033	37.373223
1768.266214	318839.853893	37.378240
1769.785981	319410.439734	37.383258
1771.687842	319983.954287	37.388276
1773.738200	320557.261901	37.393293
1775.000160	321132.167600	37.398311
1777.229878	321722.042545	37.403328
1778.941663	322292.547620	37.408346
1780.234154	322898.944713	37.413364
1782.017095	323485.475444	37.418381
1783.628349	324090.793413	37.423399
1784.720340	324696.394577	37.428416
1786.856201	325306.489775	37.433434
1788.486664	325920.648862	37.438452
1790.233199	326547.325656	37.443469
1792.427180	327147.897644	37.448487
1794.600379	327777.995569	37.453504
1796.286146	328389.252306	37.458522
1798.258998	329004.568639	37.463540
1800.032414	329621.561917	37.468557
1802.129566	330231.919777	37.473575
1803.557165	330863.606593	37.478592
1805.549074	331479.808317	37.483610
1806.945840	332110.344354	37.488628
1809.002240	332738.682931	37.493645
1810.974592	333357.559018	37.498663
1812.990268	333993.557516	37.503680
1814.763061	334626.974080	37.508698
1816.352949	335257.621135	37.513716
1818.340186	335898.019941	37.518733
1820.287538	336509.884095	37.523751
1821.758767	337173.682778	37.528768
1823.727348	337798.374039	37.533786
1825.507994	338444.640913	37.538804
1826.830392	339102.627109	37.543821
1828.669470	339743.766167	37.548839
1829.988087	340407.498898	37.553856
1831.844166	341058.874124	37.558874
1833.505750	341734.488968	37.563892
1835.291843	342408.043677	37.568909
1837.421631	343075.720070	37.573927
1838.698637	343768.707588	37.578944
1840.630101	344425.534988	37.583962
1842.482524	345109.068236	37.588980
1844.135573	345799.858507	37.593997
1846.246868	346484.497296	37.599015
1847.942909	347174.905486	37.604032
1849.955953	347852.662793	37.609050
1851.778701	348561.938225	37.614068
1853.899116	349241.586730	37.619085
1855.840870	349934.477322	37.624103
1857.487576	350620.604697	37.629120
1859.669460	351301.989288	37.634138
1861.367714	352009.455890	37.639156
1863.389387	352680.923401	37.644173
1865.559065	353374.180839	37.649191
1867.462577	354063.030439	37.654208
1869.327777	354754.159491	37.659226
1871.715615	355438.847430	37.664244
1873.322224	356105.484521	37.669261
1875.425628	356758.225249	37.674279
1877.254292	357409.757998	37.679296
1879.375896	358061.841448	37.684314
1881.369965	358696.808387	37.689332
1883.420886	359339.774443	37.694349
1885.761962	359972.736402	37.699367
1887.503884	360605.000975	37.704384
1889.606485	361253.181043	37.709402
1891.624260	361865.539404	37.714420
1893.229189	362531.896961	37.719437
1895.397817	363156.693828	37.724455
1897.101486	363807.233047	37.729472
1899.230749	364440.667855	37.734490
1900.835961	365066.212778	37.739508
1902.368947	365731.564740	37.744525
1904.626091	366364.871425	37.749543
1906.101693	367034.066795	37.754560
1907.866478	367691.990060	37.759578
1909.800567	368354.338902	37.764596
1911.542729	369025.079201	37.769613
1912.951482	369689.038908	37.774631
1914.841916	370372.312940	37.779648
1916.855178	371056.061583	37.784666
1918.646042	371745.871394	37.789684
1919.748177	372447.526045	37.794701
1921.831800	373142.106221	37.799719
1923.463194	373862.340290	37.804736
1925.345066	374552.868580	37.809754
1927.406888	375276.427627	37.814772
1929.133508	375994.549023	37.819789
1931.403139	376722.305463	37.824807
1933.015176	377438.666577	37.829824
1935.202104	378170.439307	37.834842
1937.710239	378896.310799	37.839860
1939.284479	379639.489941	37.844877
1941.992950	380347.317682	37.849895
1943.881264	381081.614121	37.854912
1945.650022	381798.670716	37.859930
1947.882479	382518.323601	37.864948
1949.726174	383253.062169	37.869965
1951.662684	383977.626581	37.874983
1953.514575	384716.337981	37.880000
1955.778209	385441.019340	37.885018
1958.329053	386172.280408	37.890036
1960.032949	386885.764483	37.895053
1962.307011	387616.531718	37.900071
1964.028022	388344.280531	37.905088
1965.495722	389090.435472	37.910106
1967.464685	389825.208550	37.915124
1969.295718	390565.387288	37.920141
1971.305710	391296.443470	37.925159
1973.087344	392050.056878	37.930176
1975.262958	392814.614300	37.935194
1976.666175	393548.683745	37.940212
1978.906885	394304.219985	37.945229
1980.956565	395050.288968	37.950247
1982.658764	395802.683170	37.955264
1984.534216	396572.215231	37.960282
1986.369736	397322.141704	37.965300
1987.977210	398106.708939	37.970317
1989.598146	398871.560411	37.975335
1991.388151	399666.599811	37.980352
1993.256074	400447.513965	37.985370
1995.549475	401245.494181	37.990388
1997.301120	402036.395435	37.995405
1999.443539	402836.738998	38.000423
2001.550142	403609.064796	38.005440
2003.373682	404416.461644	38.010458
2005.390432	405174.797605	38.015476
2007.358172	405957.471738	38.020493
2009.614525	406717.373778	38.025511
2011.686444	407493.273405	38.030528
2014.009920	408247.421899	38.035546
2015.710233	409012.699074	38.040564
2017.804003	409785.845345	38.045581
2020.058226	410561.856817	38.050599
2022.208168	411329.452646	38.055616
2024.568091	412093.749522	38.060634
2026.643211	412865.266092	38.065652
2028.769160	413628.291406	38.070669
2031.022113	414393.528432	38.075687
2032.803453	415168.345317	38.080704
2034.877094	415935.695153	38.085722
2036.950332	416720.423404	38.090740
2039.135199	417482.947914	38.095757
2041.683109	418229.611474	38.100775
2043.766947	419023.968883	38.105792
2045.753764	419780.304211	38.110810
2048.018363	420577.217730	38.115828
2050.058198	421334.080899	38.120845
2052.053902	422104.805957	38.125863
2053.929393	422900.090151	38.130880
2056.012041	423673.639717	38.135898
2057.606816	424462.463709	38.140916
2059.505891	425262.125503	38.145933
2061.647704	426062.632979	38.150951
2063.193698	426854.503222	38.155968
2065.103048	427643.097995	38.160986
2067.574155	428461.701642	38.166004
2069.111796	429288.482143	38.171021
2071.475361	430100.466095	38.176039
2073.382734	430937.812080	38.181056
2075.619578	431756.646395	38.186074
2078.590604	432557.460924	38.191092
2080.583509	433380.481428	38.196109
2082.790594	434189.517046	38.201127
2085.199998	435009.982102	38.206144
2087.077777	435817.142934	38.211162
2089.229866	436641.591860	38.216180
2091.208648	437464.875899	38.221197
2092.977209	438290.898283	38.226215
2095.149314	439117.735374	38.231232
2096.912087	439933.476098	38.236250
2099.118621	440773.608139	38.241268
2101.588004	441597.067164	38.246285
2103.794936	442428.484061	38.251303
2106.033209	443241.395446	38.256320
2108.274103	444086.508656	38.261338
2110.677937	444897.510661	38.266356
2112.545560	445737.157917	38.271373
2114.836546	446574.983123	38.276391
2117.154153	447386.109979	38.281408
2119.316598	448205.781950	38.286426
2121.517663	449027.187177	38.291444
2123.909853	449851.615409	38.296461
2125.725205	450668.418372	38.301479
2128.194365	451506.428065	38.306496
2130.147991	452335.284229	38.311514
2131.928181	453156.145262	38.316532
2133.495389	454006.293199	38.321549
2135.872846	454828.760784	38.326567
2137.744690	455670.142898	38.331584
2139.892859	456518.474749	38.336602
2141.812750	457342.991990	38.341620
2143.746345	458180.570708	38.346637
2146.281153	459011.543991	38.351655
2148.537806	459834.237271	38.356672
2150.221945	460660.783790	38.361690
2152.409803	461465.322031	38.366708
2154.142452	462298.214660	38.371725
2156.118125	463134.571550	38.376743
2158.220530	463952.219100	38.381760
2159.923857	464812.461751	38.386778
2162.073668	465635.643434	38.391796
2164.180977	466502.671218	38.396813
2165.871768	467360.227493	38.401831
2168.421448	468224.073913	38.406848
2170.017977	469106.233222	38.411866
2172.396332	469962.045865	38.416884
2174.266892	470840.543708	38.421901
2176.273739	471717.715811	38.426919
2178.523133	472606.176997	38.431936
2181.271108	473487.289358	38.436954
2183.579077	474384.854046	38.441972
2185.989720	475269.173035	38.446989
2188.095787	476175.426484	38.452007
2190.258295	477065.815016	38.457024
2192.657564	477971.933386	38.462042
2195.236643	478848.175658	38.467060
2197.543610	479758.010738	38.472077
2199.403541	480674.895342	38.477095
2201.922635	481554.857838	38.482112
2203.669726	482466.520135	38.487130
2205.917585	483379.266355	38.492148
2207.971978	484289.827265	38.497165
2209.984228	485227.515685	38.502183
2212.376773	486139.896910	38.507200
2214.261700	487080.640284	38.512218
2216.422806	488020.531313	38.517236
2218.378152	488947.331161	38.522253
2220.530575	489897.019301	38.527271
2223.413660	490840.579324	38.532288
2225.409896	491817.902647	38.537306
2227.584331	492738.964938	38.542324
2230.274517	493718.591137	38.547341
2232.333817	494659.001950	38.552359
2234.785964	495607.320787	38.557376
2236.830329	496567.816054	38.562394
2239.489611	497520.839437	38.567412
2241.838739	498471.035143	38.572429
2243.906156	499422.586424	38.577447
2246.310796	500377.509723	38.582464
2248.368355	501349.941687	38.587482
2250.938273	502295.950794	38.592500
2253.401756	503256.703552	38.597517
2255.225483	504199.196771	38.602535
2257.729819	505168.053891	38.607552
2260.128355	506130.063044	38.612570
2262.626201	507084.081900	38.617588
2265.133098	508030.529930	38.622605
2267.191278	508997.519963	38.627623
2269.581561	509939.489256	38.632640
2271.316056	510920.132756	38.637658
2273.782905	511868.581759	38.642676
2275.811549	512836.002224	38.647693
2278.129753	513806.088948	38.652711
2280.441393	514778.990838	38.657728
2282.394421	515761.116041	38.662746
2284.673687	516729.820671	38.667764
2287.397598	517689.723990	38.672781
2289.457512	518666.509694	38.677799
2292.099328	519638.048833	38.682816
2294.157900	520612.142836	38.687834
2296.606345	521567.519299	38.692852
2298.879188	522517.172423	38.697869
2300.932899	523465.493167	38.702887
2303.110166	524401.140933	38.707904
2304.967926	525358.746381	38.712922
2307.399825	526295.041756	38.717940
2309.617924	527260.174274	38.722957
2311.459553	528243.437736	38.727975
2313.960867	529185.182915	38.732992
2315.621243	530168.299745	38.738010
2318.038319	531132.646762	38.743028
2319.952239	532139.106510	38.748045
2321.761981	533120.795011	38.753063
2324.084492	534137.523293	38.758080
2326.008950	535152.938015	38.763098
2328.693869	536150.287670	38.768116
2331.229805	537196.114037	38.773133
2333.517396	538197.918722	38.778151
2336.385890	539239.063554	38.783168
2338.529485	540258.866002	38.788186
2340.720685	541296.249760	38.793204
2343.143095	542326.928957	38.798221
2344.970469	543373.429221	38.803239
2348.205089	544415.646032	38.808256
2350.194140	545473.484710	38.813274
2352.688796	546506.664736	38.818292
2355.507391	547553.546552	38.823309
2357.849738	548609.380389	38.828327
2360.578038	549644.200927	38.833344
2363.058823	550705.686002	38.838362
2365.372120	551741.675196	38.843380
2367.947428	552798.156620	38.848397
2370.102164	553858.145042	38.853415
2372.462664	554910.879083	38.858432
2374.722504	555966.162026	38.863450
2377.486686	557025.702612	38.868468
2380.028925	558088.664365	38.873485
2382.223883	559157.177454	38.878503
2384.546472	560219.654908	38.883520
2386.849079	561297.426069	38.888538
2389.144626	562369.132378	38.893556
2391.523099	563446.867221	38.898573
2393.795641	564527.997586	38.903591
2396.045261	565596.335002	38.908608
2398.457797	566703.783742	38.913626
2400.823239	567788.446756	38.918644
2403.391387	568880.116533	38.923661
2405.479493	569970.216880	38.928679
2408.203125	571070.111659	38.933696
2410.730861	572162.062727	38.938714
2413.102649	573281.856970	38.943732
2415.529047	574358.326502	38.948749
2418.062684	575472.179300	38.953767
2421.603817	576527.452085	38.958784
2424.316459	577621.563629	38.963802
2427.127151	578684.754943	38.968820
2430.186016	579762.565992	38.973837
2432.236291	580824.596940	38.978855
2434.893286	581894.413352	38.983872
2437.264182	582948.785440	38.988890
2439.403363	584041.474921	38.993908
2441.982707	585096.732401	38.998925
2444.145296	586166.560595	39.003943
2446.479384	587221.775656	39.008960
2448.698662	588309.808948	39.013978
2450.962190	589376.530844	39.018996
2453.308516	590466.856193	39.024013
2455.545015	591539.206481	39.029031
2457.869595	592612.098083	39.034048
2460.459247	593656.083306	39.039066
2462.359332	594717.529658	39.044084
2465.274365	595752.908804	39.049101
2467.963791	596798.205105	39.054119
2470.334917	597852.779633	39.059136
2472.666778	598890.635034	39.064154
2475.139313	599973.105140	39.069172
2477.642655	601009.141691	39.074189
2479.617530	602096.204930	39.079207
2481.827248	603144.319273	39.084224
2484.226537	604247.685838	39.089242
2486.480014	605334.599351	39.094260
2488.799473	606418.796060	39.099277
2490.818160	607542.484375	39.104295
2493.145084	608633.327690	39.109312
2495.457103	609764.806912	39.114330
2497.622335	610884.687887	39.119348
2500.030611	612028.085172	39.124365
2502.210085	613170.103288	39.129383
2504.498073	614333.098449	39.134400
2506.509202	615503.521488	39.139418
2508.881787	616692.868059	39.144436
2511.025396	617881.724918	39.149453
2513.487196	619074.401998	39.154471
2515.966207	620299.246878	39.159488
2518.341603	621513.323582	39.164506
2520.814609	622724.750115	39.169524
2523.357319	623962.371468	39.174541
2525.743259	625198.628271	39.179559
2528.894056	626439.265140	39.184576
2531.783901	627677.953581	39.189594
2534.036007	628917.803398	39.194612
2537.127700	630166.013273	39.199629
2539.361424	631417.515087	39.204647
2542.212026	632671.015263	39.209664
2544.975775	633911.997206	39.214682
2547.245762	635172.487265	39.219700
2550.253497	636427.063159	39.224717
2552.497352	637682.912585	39.229735
2555.243490	638954.849421	39.234752
2557.929060	640201.487978	39.239770
2560.538072	641462.609917	39.244788
2563.651197	642718.954364	39.249805
2566.231915	643980.521254	39.254823
2568.910523	645238.425029	39.259840
2571.477091	646509.459269	39.264858
2573.370752	647772.915438	39.269876
2576.331306	649028.858071	39.274893
2578.340797	650318.255346	39.279911
2581.218185	651581.272678	39.284928
2583.677732	652868.374325	39.289946
2586.260075	654146.668115	39.294964
2589.014306	655433.689357	39.299981
2591.209241	656716.101866	39.304999
2594.191521	658006.936560	39.310016
2597.148041	659292.824499	39.315034
2599.604534	660588.985991	39.320052
2602.205591	661868.667825	39.325069
2604.531078	663161.023750	39.330087
2607.374874	664433.954956	39.335104
2610.134187	665739.835759	39.340122
2612.676485	667020.241573	39.345140
2615.371808	668316.924087	39.350157
2617.551208	669610.082828	39.355175
2620.259356	670907.457001	39.360192
2622.935359	672195.755194	39.365210
2625.782661	673511.902616	39.370228
2628.458747	674798.652820	39.375245
2630.706905	676069.435527	39.380263
2633.693859	677308.701376	39.385280
2636.125582	678572.949219	39.390298
2638.664517	679830.496633	39.395316
2641.217525	681083.349018	39.400333
2643.852957	682337.558778	39.405351
2646.446815	683616.099479	39.410368
2648.896834	684873.323538	39.415386
2651.824891	686161.837404	39.420404
2654.455715	687441.080460	39.425421
2656.480927	688731.019198	39.430439
2659.037733	690024.956924	39.435456
2661.736853	691316.452240	39.440474
2664.089867	692623.057697	39.445492
2666.826163	693920.526602	39.450509
2669.265178	695235.174264	39.455527
2671.716838	696545.508330	39.460544
2675.056583	697874.651040	39.465562
2677.458792	699191.498132	39.470580
2680.716159	700535.084906	39.475597
2683.912622	701848.627324	39.480615
2686.426495	703181.321274	39.485632
2689.656690	704518.601448	39.490650
2691.712950	705838.771395	39.495668
2694.875079	707187.596910	39.500685
2697.724840	708510.549544	39.505703
2700.378825	709860.478601	39.510720
2703.008993	711190.139948	39.515738
2705.327814	712549.260967	39.520756
2707.781168	713871.552220	39.525773
2710.383612	715255.497413	39.530791
2713.168348	716628.742670	39.535808
2716.090838	717984.321512	39.540826
2718.537078	719362.374541	39.545844
2721.709250	720717.224598	39.550861
2724.377188	722096.375093	39.555879
2727.322564	723464.766767	39.560896
2730.154454	724837.946508	39.565914
2732.499619	726218.247004	39.570932
2735.462480	727621.152387	39.575949
2738.213367	728992.765138	39.580967
2740.602884	730391.486442	39.585984
2743.596447	731770.105576	39.591002
2746.509620	733182.047533	39.596020
2748.954550	734573.521345	39.601037
2751.631208	735983.631575	39.606055
2754.109523	737394.318093	39.611072
2757.265335	738791.514250	39.616090
2759.435203	740217.305800	39.621108
2762.187956	741636.825071	39.626125
2765.229296	743066.454298	39.631143
2767.811252	744470.545771	39.636160
2771.000939	745887.752650	39.641178
2774.074052	747329.972038	39.646196
2776.887166	748730.159895	39.651213
2780.080858	750171.540948	39.656231
2782.762646	751580.063624	39.661248
2785.674188	753008.201208	39.666266
2788.271540	754424.106109	39.671284
2790.951321	755857.077013	39.676301
2793.408373	757272.629876	39.681319
2796.061579	758716.842700	39.686336
2798.606100	760141.108349	39.691354
2800.985650	761606.186100	39.696372
2803.604350	763043.235491	39.701389
2806.279283	764493.878168	39.706407
2808.854354	765958.918142	39.711424
2811.311225	767409.478188	39.716442
2813.763402	768846.137106	39.721460
2816.093221	770292.618829	39.726477
2818.868933	771746.414421	39.731495
2821.210589	773207.122974	39.736512
2824.088195	774657.234615	39.741530
2826.838577	776120.984810	39.746548
2829.366601	777592.486145	39.751565
2831.773503	779065.430638	39.756583
2834.803300	780565.616671	39.761600
2838.088428	782041.300933	39.766618
2840.550649	783556.081530	39.771636
2843.380454	785053.899918	39.776653
2846.126667	786570.503338	39.781671
2849.105429	788086.257672	39.786688
2852.172411	789607.952866	39.791706
2855.016719	791150.832677	39.796724
2857.670826	792667.137672	39.801741
2860.451356	794205.540692	39.806759
2863.075896	795757.596995	39.811776
2866.397608	797301.065150	39.816794
2868.977107	798870.270236	39.821812
2871.600088	800424.525882	39.826829
2874.262061	802004.419910	39.831847
2876.900443	803584.594382	39.836864
2879.468064	805188.931432	39.841882
2882.288163	806791.043626	39.846900
2885.540884	808401.757891	39.851917
2888.681395	809999.253099	39.856935
2891.980875	811607.297080	39.861952
2894.783744	813215.384522	39.866970
2897.448578	814840.408249	39.871988
2900.238765	816448.119756	39.877005
2903.569414	818077.528268	39.882023
2906.388280	819737.870578	39.887040
2909.447216	821351.684830	39.892058
2912.638471	822993.876422	39.897076
2915.694995	824622.170145	39.902093
2918.386515	826271.095340	39.907111
2921.346955	827905.666631	39.912128
2924.468946	829540.096767	39.917146
2927.541837	831172.372097	39.922164
2930.702094	832823.178062	39.927181
2933.633979	834477.158117	39.932199
2936.573229	836115.714985	39.937216
2939.969029	837766.682516	39.942234
2942.612848	839411.655062	39.947252
2945.746392	841057.292489	39.952269
2948.432431	842704.817384	39.957287
2951.332126	844366.228353	39.962304
2954.298208	846002.248993	39.967322
2957.534947	847668.523879	39.972340
2959.913608	849321.377706	39.977357
2962.874865	850968.161539	39.982375
2965.714322	852653.195776	39.987392
2968.861496	854299.847332	39.992410
2971.658343	855988.744095	39.997428
2974.536119	857664.839322	40.002445
2977.939423	859321.663791	40.007463
2980.923725	861003.528503	40.012480
2985.493354	862623.471023	40.017498
2988.779577	864274.513971	40.022516
2991.808525	865923.794301	40.027533
2995.074274	867582.084279	40.032551
2997.583104	869213.788843	40.037568
3000.485853	870833.266988	40.042586
3003.318956	872503.446316	40.047604
3005.804232	874127.913001	40.052621
3008.814868	875770.238455	40.057639
3011.719236	877393.261476	40.062656
3014.599406	878989.341586	40.067674
3017.691482	880592.207908	40.072692
3020.664140	882199.587832	40.077709
3024.067803	883788.093936	40.082727
3026.496822	885396.136195	40.087744
3029.348900	886992.460701	40.092762
3032.429751	888616.216621	40.097780
3035.531534	890224.647160	40.102797
3038.407734	891849.170410	40.107815
3040.882788	893475.134575	40.112832
3043.986783	895127.735180	40.117850
3046.924088	896787.503606	40.122868
3049.512975	898436.435030	40.127885
3052.563271	900091.750791	40.132903
3054.823267	901793.343255	40.137920
3057.652105	903456.284994	40.142938
3060.773846	905177.710132	40.147956
3063.427890	906893.678593	40.152973
3066.734244	908611.129723	40.157991
3069.448414	910348.446227	40.163008
3072.765644	912087.427658	40.168026
3075.619208	913829.111303	40.173044
3078.538094	915590.992667	40.178061
3081.938607	917334.648185	40.183079
3084.776676	919107.998693	40.188096
3087.781367	920872.008421	40.193114
3090.285062	922664.610594	40.198132
3093.411540	924449.608994	40.203149
3096.940839	926250.640557	40.208167
3099.706081	928058.194812	40.213184
3102.679140	929863.955445	40.218202
3106.159538	931678.700147	40.223220
3109.269021	933501.220989	40.228237
3112.686342	935334.747167	40.233255
3116.001854	937154.157863	40.238272
3119.030213	938979.972885	40.243290
3122.023138	940801.045870	40.248308
3125.137118	942644.796593	40.253325
3128.927663	944453.086071	40.258343
3131.759803	946305.718601	40.263360
3134.951606	948133.844973	40.268378
3138.260159	949977.536928	40.273396
3141.193601	951822.538672	40.278413
3144.560471	953681.975894	40.283431
3147.670112	955523.228252	40.288448
3150.836137	957427.589988	40.293466
3153.748372	959316.010645	40.298484
3156.761684	961222.275581	40.303501
3160.158473	963121.103138	40.308519
3163.483187	965031.334649	40.313536
3166.774355	966925.505149	40.318554
3170.110079	968824.902971	40.323572
3173.566423	970740.246736	40.328589
3176.958162	972616.614102	40.333607
3180.362015	974525.238556	40.338624
3183.959296	976409.499776	40.343642
3187.260259	978303.132790	40.348660
3190.511509	980186.304849	40.353677
3194.291797	982070.815076	40.358695
3197.388144	983930.859373	40.363712
3200.552542	985810.340902	40.368730
3203.802467	987685.393224	40.373748
3207.048170	989558.856124	40.378765
3210.108829	991428.620569	40.383783
3213.143747	993298.455035	40.388800
3216.403200	995173.663107	40.393818
3219.284850	997040.929716	40.398836
3222.493322	998880.040186	40.403853
3225.742255	1000700.972357	40.408871
3228.445966	1002544.219399	40.413888
3231.531500	1004362.932348	40.418906
3234.760534	1006191.318891	40.423924
3237.675300	1008028.086721	40.428941
3240.594035	1009865.807082	40.433959
3243.381725	1011747.528103	40.438976
3246.499190	1013608.415979	40.443994
3249.821935	1015482.116108	40.449012
3252.780540	1017359.608403	40.454029
3256.402370	1019223.685923	40.459047
3259.567862	1021135.496372	40.464064
3263.019091	1023018.367562	40.469082
3266.530636	1024907.073771	40.474100
3269.559211	1026810.202905	40.479117
3272.431648	1028733.772479	40.484135
3275.589783	1030646.395202	40.489152
3278.547771	1032591.415508	40.494170
3281.541271	1034514.035883	40.499188
3284.453307	1036500.938600	40.504205
3287.417047	1038452.306512	40.509223
3290.089452	1040454.329662	40.514240
3292.910598	1042452.619518	40.519258
3295.844099	1044468.765976	40.524276
3298.438535	1046504.267578	40.529293
3301.631100	1048558.177533	40.534311
3304.891276	1050632.293875	40.539328
3307.922353	1052715.193983	40.544346
3311.431149	1054786.940859	40.549364
3314.578620	1056885.365951	40.554381
3318.294138	1058966.467619	40.559399
3322.271700	1061060.283624	40.564416
3325.998711	1063144.894782	40.569434
3329.516155	1065253.321240	40.574452
3332.648058	1067357.931717	40.579469
3336.021125	1069458.338601	40.584487
3339.512547	1071580.642513	40.589504
3342.686149	1073696.522193	40.594522
3346.147247	1075806.459077	40.599540
3349.211250	1077948.587866	40.604557
3352.231218	1080064.708888	40.609575
3355.214209	1082218.097273	40.614592
3358.014384	1084351.726941	40.619610
3361.301390	1086535.590533	40.624628
3364.351710	1088687.460398	40.629645
3367.533721	1090878.197334	40.634663
3370.904279	1093059.806441	40.639680
3373.822075	1095255.503005	40.644698
3377.249341	1097458.431137	40.649716
3380.681736	1099668.759042	40.654733
3384.219122	1101875.019397	40.659751
3388.156695	1104092.510239	40.664768
3391.550536	1106301.176880	40.669786
3395.018172	1108522.732597	40.674804
3398.563911	1110727.843766	40.679821
3402.129019	1112952.692752	40.684839
3405.466330	1115153.832802	40.689856
3408.351799	1117388.366590	40.694874
3411.970919	1119595.811268	40.699892
3414.949298	1121824.202305	40.704909
3418.512162	1124066.379562	40.709927
3422.442262	1126284.113523	40.714944
3425.532373	1128521.080267	40.719962
3429.402141	1130735.738738	40.724980
3432.536188	1132974.620288	40.729997
3436.092295	1135190.792869	40.735015
3439.543500	1137404.665013	40.740020
3442.504157	1139543.412602	40.745024
3445.725256	1141643.400202	40.750029
3449.240024	1143691.579838	40.755034
3452.172539	1145635.066406	40.760039
3455.591802	1147536.629280	40.765044
3458.266272	1149346.590770	40.770048
3461.413652	1151084.921023	40.775053
3463.940828	1152735.396978	40.780058
3466.455858	1154313.143801	40.785063
3469.617546	1155804.208984	40.790068
3471.830604	1157238.346808	40.795072
3474.650333	1158575.439722	40.800077
3476.741410	1159852.181485	40.805082
3479.069712	1161042.935456	40.810087
3481.275808	1162169.082500	40.815092
3483.321301	1163243.331305	40.820096
3485.505204	1164225.327329	40.825101
3487.305587	1165172.350526	40.830106
3489.235801	1166032.585710	40.835111
3491.050856	1166858.046667	40.840116
3492.426493	1167595.181030	40.845120
3494.251216	1168287.678433	40.850125
3495.618290	1168936.460935	40.855130
3497.225123	1169531.709780	40.860135
3498.772690	1170068.302627	40.865140
3500.032489	1170569.977574	40.870144
3501.539079	1171013.353746	40.875149
3502.566390	1171416.961242	40.880154
3504.125858	1171764.889579	40.885159
3505.056598	1172093.750414	40.890164
3506.027875	1172378.536926	40.895168
3507.405267	1172610.236204	40.900173
3507.942817	1172845.081431	40.905178
3508.853068	1173012.708003	40.910183
3509.779955	1173169.198468	40.915188
3510.408630	1173276.130207	40.920192
3511.608228	1173366.463012	40.925197
3511.712545	1173430.570645	40.930202
3512.904960	1173480.447713	40.935207
3513.558628	1173484.112321	40.940212
3514.117180	1173477.513974	40.945216
3514.817831	1173448.920399	40.950221
3515.465482	1173386.481458	40.955226
3515.865240	1173315.972611	40.960231
3516.305619	1173224.803610	40.965236
3516.999742	1173118.125095	40.970240
3517.596931	1172990.524004	40.975245
3517.573722	1172842.273633	40.980250
3518.018687	1172697.714480	40.985255
3519.128671	1172510.127826	40.990260
3519.210740	1172330.909579	40.995264
3519.535133	1172113.255543	41.000269
3519.889901	1171902.567688	41.005274
3520.046556	1171663.981725	41.010279
3520.189000	1171440.386664	41.015284
3520.137336	1171190.021307	41.020288
3520.804196	1170949.997908	41.025293
3520.761063	1170694.229695	41.030298
3520.861617	1170426.819697	41.035303
3521.364874	1170143.571651	41.040308
3521.165099	1169870.992869	41.045312
3521.997279	1169564.634267	41.050317
3522.041702	1169254.706798	41.055322
3522.074050	1168949.010083	41.060327
3522.341527	1168638.348645	41.065332
3522.377727	1168303.919892	41.070336
3522.569374	1167990.400642	41.075341
3522.570200	1167650.366382	41.080346
3522.544147	1167323.909562	41.085351
3523.129634	1166987.701157	41.090356
3522.816268	1166639.627490	41.095360
3523.198607	1166282.823011	41.100365
3523.262153	1165933.129382	41.105370
3523.187734	1165568.418812	41.110375
3523.486349	1165203.054691	41.115380
3523.395559	1164851.047397	41.120384
3523.839220	1164460.860281	41.125389
3523.331191	1164100.275152	41.130394
3523.520033	1163727.552045	41.135399
3523.520533	1163351.054150	41.140404
3523.630464	1162998.133369	41.145408
3523.827011	1162595.091993	41.150413
3524.120506	1162223.095089	41.155418
3523.871013	1161820.445616	41.160423
3524.048123	1161442.930949	41.165428
3523.989976	1161037.543367	41.170432
3524.020919	1160636.836333	41.175437
3524.188906	1160249.595088	41.180442
3524.384885	1159842.182509	41.185447
3524.328704	1159452.461176	41.190452
3524.377916	1159060.707796	41.195456
3524.133317	1158644.764465	41.200461
3524.049697	1158229.896558	41.205466
3524.279841	1157832.536419	41.210471
3524.398950	1157407.166148	41.215476
3524.337356	1157015.183826	41.220480
3524.731086	1156587.147847	41.225485
3524.353520	1156184.276109	41.230490
3524.130630	1155753.435456	41.235495
3524.554388	1155346.298904	41.240500
3524.184476	1154935.760107	41.245504
3524.288015	1154513.375765	41.250509
3523.935770	1154116.303800	41.255514
3524.287312	1153694.948701	41.260519
3524.410348	1153272.461549	41.265524
3524.409917	1152860.753346	41.270528
3524.506590	1152435.363236	41.275533
3524.548359	1152006.160353	41.280538
3524.449526	1151582.627305	41.285543
3524.610941	1151143.202140	41.290548
3524.207555	1150720.596980	41.295552
3524.454808	1150296.335294	41.300557
3524.529232	1149880.782614	41.305562
3524.446850	1149451.297373	41.310567
3524.377630	1149028.691010	41.315572
3524.195163	1148598.110642	41.320576
3524.353778	1148159.005718	41.325581
3524.333721	1147743.679266	41.330586
3523.697485	1147301.032874	41.335591
3524.447469	1146890.535346	41.340596
3523.973795	1146446.558424	41.345600
3523.954746	1146028.727247	41.350605
3524.080463	1145600.221426	41.355610
3523.776967	1145187.205424	41.360615
3524.341163	1144745.853714	41.365620
3524.180731	1144315.584173	41.370624
3524.389007	1143893.469290	41.375629
3523.747707	1143455.243034	41.380634
3523.957920	1143028.885876	41.385639
3524.053466	1142592.458586	41.390644
3523.826579	1142164.111781	41.395648
3523.947095	1141736.621799	41.400653
3523.934011	1141326.766663	41.405658
3523.909715	1140886.802877	41.410663
3523.839048	1140460.190200	41.415668
3523.484755	1140031.596951	41.420672
3524.089664	1139595.597961	41.425677
3523.891624	1139160.834365	41.430682
3523.968074	1138733.394019	41.435687
3523.876441	1138287.530018	41.440692
3523.746096	1137871.541084	41.445696
3523.665934	1137436.426790	41.450701
3523.867869	1137015.093843	41.455706
3523.826557	1136576.389280	41.460711
3524.116965	1136148.230564	41.465716
3523.686084	1135722.530579	41.470720
3524.000225	1135276.726644	41.475725
3523.382616	1134852.032469	41.480730
3523.502830	1134419.772678	41.485735
3523.612830	1133973.227969	41.490740
3523.137553	1133543.180171	41.495744
3523.433091	1133108.884537	41.500749
3523.328740	1132689.824541	41.505754
3523.381750	1132251.792581	41.510759
3523.207628	1131829.539951	41.515764
3522.968319	1131392.245739	41.520768
3523.298343	1130970.127041	41.525773
3523.440842	1130554.470575	41.530778
3523.321070	1130128.366238	41.535783
3523.573362	1129675.542370	41.540788
3523.308760	1129267.744679	41.545792
3522.927121	1128832.545865	41.550797
3523.104005	1128418.428839	41.555802
3522.953816	1127984.454155	41.560807
3522.937805	1127544.714565	41.565812
3522.749392	1127126.466969	41.570816
3522.565775	1126700.955169	41.575821
3522.470944	1126272.064640	41.580826
3522.496062	1125854.062671	41.585831
3522.706977	1125435.807030	41.590836
3522.626483	1125020.516865	41.595840
3522.543628	1124605.861014	41.600845
3522.775096	1124186.552338	41.605850
3522.715126	1123754.883783	41.610855
3522.716707	1123332.975770	41.615860
3522.694500	1122903.612192	41.620864
3522.879090	1122479.131226	41.625869
3522.655494	1122054.683776	41.630874
3522.477828	1121638.480052	41.635879
3522.747001	1121199.980014	41.640884
3522.451736	1120795.825229	41.645888
3522.347822	1120361.413412	41.650893
3522.554423	1119950.349154	41.655898
3522.731744	1119520.204675	41.660903
3522.575828	1119082.172667	41.665908
3522.352491	1118675.654533	41.670912
3522.232465	1118236.880470	41.675917
3522.105197	1117830.663520	41.680922
3522.241100	1117409.314235	41.685927
3522.255108	1116991.478456	41.690932
3522.131315	1116569.534033	41.695936
3522.266519	1116145.321200	41.700941
3522.230554	1115745.318053	41.705946
3521.962900	1115321.583066	41.710951
3522.204212	1114895.537723	41.715956
3521.954864	1114482.984726	41.720960
3522.101295	1114062.038103	41.725965
3521.891251	1113635.394846	41.730970
3521.986486	1113227.266412	41.735975
3522.022317	1112787.162105	41.740980
3521.758815	1112387.232195	41.745984
3521.976016	1111953.898118	41.750989
3521.525044	1111557.753395	41.755994
3521.400245	1111139.961648	41.760999
3521.893557	1110722.894430	41.766004
3521.804011	1110316.770014	41.771008
3521.899738	1109885.006872	41.776013
3521.745113	1109487.229119	41.781018
3521.825011	1109052.633828	41.786023
3521.561200	1108644.025434	41.791028
3521.692063	1108235.225531	41.796032
3521.626398	1107812.869436	41.801037
3521.470966	1107405.199348	41.806042
3521.266703	1106993.686826	41.811047
3521.402178	1106578.553492	41.816052
3521.356709	1106171.058341	41.821056
3521.515421	1105766.173066	41.826061
3521.250422	1105348.909669	41.831066
3521.260099	1104936.345046	41.836071
3521.756676	1104525.770398	41.841076
3521.338023	1104118.945789	41.846080
3521.093786	1103696.391818	41.851085
3521.136310	1103293.250891	41.856090
3520.799158	1102890.811309	41.861095
3520.866686	1102463.522387	41.866100
3520.715730	1102075.900305	41.871104
3521.075889	1101674.497663	41.876109
3520.725955	1101261.997927	41.881114
3520.546779	1100851.732919	41.886119
3520.674315	1100458.117275	41.891124
3520.645967	1100056.084690	41.896128
3520.363690	1099642.780829	41.901133
3520.591143	1099254.415769	41.906138
3520.733222	1098848.248912	41.911143
3520.580249	1098474.809436	41.916148
3520.245261	1098071.723321	41.921152
3520.386620	1097649.971559	41.926157
3520.580686	1097269.026174	41.931162
3520.272627	1096851.303980	41.936167
3520.507655	1096459.962559	41.941172
3520.118668	1096067.738784	41.946176
3520.376556	1095674.136066	41.951181
3520.209611	1095276.746811	41.956186
3520.079485	1094892.242417	41.961191
3520.021755	1094485.685210	41.966196
3519.776042	1094106.599630	41.971200
3520.119437	1093709.011294	41.976205
3519.981563	1093327.747509	41.981210
3519.927172	1092919.732007	41.986215
3520.262677	1092531.153794	41.991220
3519.910891	1092140.458622	41.996224
3520.064534	1091750.130852	42.001229
3520.058439	1091344.478620	42.006234
3519.645704	1090949.015075	42.011239
3519.861921	1090567.211541	42.016244
3519.745337	1090171.355203	42.021248
3520.008957	1089792.937762	42.026253
3519.794806	1089399.723468	42.031258
3519.262304	1089010.461264	42.036263
3519.828842	1088625.972515	42.041268
3519.503357	1088241.220195	42.046272
3519.514452	1087856.289360	42.051277
3519.614220	1087457.995540	42.056282
3519.364575	1087077.365077	42.061287
3519.331544	1086705.011132	42.066292
3519.198844	1086317.886364	42.071296
3519.265627	1085919.868718	42.076301
3519.234788	1085555.967504	42.081306
3519.319007	1085166.520076	42.086311
3519.412411	1084802.068601	42.091316
3519.050635	1084409.859893	42.096320
3518.779179	1084045.609634	42.101325
3519.084493	1083664.840733	42.106330
3518.804451	1083294.307970	42.111335
3519.011965	1082908.035464	42.116340
3518.948516	1082527.823311	42.121344
3519.182972	1082151.084931	42.126349
3518.689031	1081765.230653	42.131354
3518.831826	1081402.462226	42.136359
3518.686006	1081027.051976	42.141364
3518.544292	1080659.483532	42.146368
3518.707151	1080299.996884	42.151373
3518.385754	1079922.812217	42.156378
3518.451343	1079536.420111	42.161383
3518.688474	1079178.190961	42.166388
3518.539088	1078800.996386	42.171392
3518.486680	1078434.799130	42.176397
3518.440852	1078056.672113	42.181402
3518.139744	1077697.474428	42.186407
3518.498063	1077327.294951	42.191412
3518.225182	1076976.014304	42.196416
3518.417571	1076606.773536	42.201421
3518.312886	1076234.771791	42.206426
3518.113061	1075875.149479	42.211431
3518.360457	1075501.695297	42.216436
3518.411227	1075136.124290	42.221440
3518.381446	1074770.638167	42.226445
3518.022711	1074399.033621	42.231450
3518.012306	1074043.102204	42.236455
3518.166443	1073668.385330	42.241460
3517.870273	1073314.471216	42.246464
3517.713289	1072955.995026	42.251469
3517.974344	1072594.543595	42.256474
3517.617454	1072255.466001	42.261479
3517.659189	1071882.663542	42.266484
3517.416565	1071536.891067	42.271488
3517.737426	1071172.452454	42.276493
3517.878918	1070826.379621	42.281498
3517.460729	1070471.628905	42.286503
3517.696168	1070102.230338	42.291508
3517.470556	1069749.323955	42.296512
3517.582296	1069389.800873	42.301517
3517.334435	1069041.179457	42.306522
3517.039704	1068695.236222	42.311527
3517.358024	1068339.553039	42.316532
3517.176326	1068004.799704	42.321536
3517.114708	1067650.288543	42.326541
3517.308931	1067312.930305	42.331546
3517.289009	1066959.329538	42.336551
3517.074581	1066609.105096	42.341556
3516.700138	1066267.543381	42.346560
3516.734133	1065942.441908	42.351565
3516.690213	1065590.873650	42.356570
3516.676121	1065260.158962	42.361575
3516.757675	1064905.831879	42.366580
3516.834627	1064570.249079	42.371584
3516.572351	1064245.769652	42.376589
3516.474511	1063892.850450	42.381594
3516.145991	1063573.924733	42.386599
3516.021142	1063217.790219	42.391604
3516.177660	1062903.558792	42.396608
3516.004797	1062569.820346	42.401613
3516.380710	1062244.251210	42.406618
3516.534081	1061925.631914	42.411623
3516.358059	1061577.391173	42.416628
3516.112845	1061248.976754	42.421632
3516.350089	1060908.232965	42.426637
3516.411369	1060602.938190	42.431642
3516.085555	1060261.284028	42.436647
3516.106066	1059946.809840	42.441652
3515.933565	1059614.818480	42.446656
3516.351324	1059286.659425	42.451661
3516.387501	1058949.102759	42.456666
3516.222911	1058607.415777	42.461671
3516.344201	1058288.687633	42.466676
3516.131616	1057973.946526	42.471680
3516.088979	1057641.044018	42.476685
3516.461254	1057301.692999	42.481690
3516.270102	1056974.749340	42.486695
3516.403685	1056644.263267	42.491700
3515.917405	1056305.763390	42.496704
3515.913754	1055967.741572	42.501709
3516.102921	1055651.452292	42.506714
3516.000183	1055323.625056	42.511719
3516.139665	1055012.320100	42.516724
3515.981173	1054675.787133	42.521728
3516.009837	1054343.734401	42.526733
3516.122559	1054023.604205	42.531738
3515.708582	1053702.095789	42.536743
3516.191066	1053376.563670	42.541748
3516.079673	1053042.237795	42.546752
3515.954834	1052722.071301	42.551757
3515.772089	1052385.016957	42.556762
3515.644878	1052064.523406	42.561767
3515.684209	1051738.871363	42.566772
3515.498904	1051437.739855	42.571776
3515.539608	1051105.104620	42.576781
3515.449306	1050776.426584	42.581786
3515.215734	1050474.864676	42.586791
3515.381268	1050146.975458	42.591796
3515.427219	1049857.395052	42.596800
3515.466712	1049526.594995	42.601805
3515.162998	1049214.264362	42.606810
3514.921753	1048907.986027	42.611815
3515.078607	1048567.747734	42.616820
3515.113471	1048271.426490	42.621824
3514.888275	1047973.201672	42.626829
3515.054924	1047659.644055	42.631834
3515.119243	1047335.369762	42.636839
3515.335409	1047032.773916	42.641844
3515.209336	1046726.259398	42.646848
3515.081741	1046409.300264	42.651853
3514.995698	1046091.833357	42.656858
3515.116343	1045784.550201	42.661863
3515.222941	1045461.607797	42.666868
3514.884000	1045164.409381	42.671872
3515.013249	1044852.920395	42.676877
3515.224398	1044555.308992	42.681882
3514.706097	1044235.295719	42.686887
3514.771614	1043932.748679	42.691892
3514.692685	1043624.122929	42.696896
3514.556834	1043319.353739	42.701901
3514.705274	1043005.922342	42.706906
3514.420460	1042714.670442	42.711911
3514.617749	1042404.385476	42.716916
3514.508894	1042123.122509	42.721920
3514.646783	1041816.196498	42.726925
3514.668627	1041522.608965	42.731930
3514.751362	1041213.919250	42.736935
3514.844659	1040889.553223	42.741940
3514.376582	1040607.886097	42.746944
3514.646034	1040291.575239	42.751949
3514.432618	1039997.752569	42.756954
3514.151877	1039694.451639	42.761959
3514.023381	1039411.894592	42.766964
3514.299873	1039109.436739	42.771968
3514.376820	1038836.001366	42.776973
3514.389688	1038515.474219	42.781978
3514.105022	1038238.394728	42.786983
3514.236271	1037918.974083	42.791988
3514.182950	1037628.771272	42.796993
3514.442635	1037342.950555	42.801997
3514.462127	1037048.353427	42.807002
3514.153488	1036749.732397	42.812007
3514.167001	1036466.808935	42.817012
3514.048820	1036155.550043	42.822017
3514.260920	1035852.248652	42.827021
3514.134165	1035563.788329	42.832026
3513.606363	1035266.381508	42.837031
3513.727545	1034980.849370	42.842036
3513.941169	1034703.028056	42.847041
3513.949620	1034417.969443	42.852045
3513.839056	1034121.981028	42.857050
3513.568134	1033839.454825	42.862055
3513.649457	1033550.565694	42.867060
3513.717275	1033263.502707	42.872065
3513.785560	1032979.328519	42.877069
3513.746491	1032679.960978	42.882074
3513.501437	1032400.745391	42.887079
3513.657754	1032111.672589	42.892084
3513.679688	1031840.516469	42.897089
3513.746109	1031552.300775	42.902093
3513.965469	1031265.787735	42.907098
3513.506792	1030980.049431	42.912103
3513.971159	1030680.298054	42.917108
3513.515857	1030415.929307	42.922113
3513.472910	1030118.845838	42.927117
3513.772428	1029843.286125	42.932122
3513.767866	1029561.274122	42.937127
3513.571328	1029261.846032	42.942132
3513.433586	1028988.737514	42.947137
3513.460040	1028701.252973	42.952141
3513.405518	1028424.325527	42.957146
3513.539193	1028138.828615	42.962151
3513.772590	1027868.316644	42.967156
3513.343439	1027578.718122	42.972161
3513.533095	1027306.151642	42.977165
3513.361167	1027013.574884	42.982170
3513.146174	1026744.729578	42.987175
3513.263076	1026453.917005	42.992180
3513.227142	1026195.578062	42.997185
3513.406240	1025911.219736	43.002189
3513.401253	1025607.300270	43.007194
3512.899676	1025347.351289	43.012199
3513.188141	1025073.496727	43.017204
3513.135028	1024795.420111	43.022209
3513.085928	1024532.838593	43.027213
3513.184208	1024234.934499	43.032218
3512.957963	1023972.355879	43.037223
3513.064995	1023693.228713	43.042228
3513.019343	1023430.982768	43.047233
3512.783162	1023149.461197	43.052237
3512.926317	1022866.602475	43.057242
3512.873557	1022599.761512	43.062247
3512.632476	1022337.108690	43.067252
3512.712028	1022069.541885	43.072257
3512.402914	1021793.588894	43.077261
3512.527834	1021551.108179	43.082266
3512.273010	1021278.224440	43.087271
3512.379174	1021024.279090	43.092276
3512.516822	1020766.437068	43.097281
3512.376023	1020502.226772	43.102285
3512.559313	1020245.517348	43.107290
3512.144881	1019973.857552	43.112295
3512.255939	1019716.747784	43.117300
3512.184170	1019459.753375	43.122305
3512.302891	1019209.992835	43.127309
3512.589435	1018935.450571	43.132314
3512.529194	1018688.122083	43.137319
3512.358649	1018418.966818	43.142324
3512.144067	1018164.556735	43.147329
3512.165633	1017910.969674	43.152333
3512.147141	1017645.828377	43.157338
3512.011772	1017393.990796	43.162343
3512.171033	1017121.710243	43.167348
3512.197910	1016870.210715	43.172353
3511.927523	1016630.397464	43.177357
3511.953562	1016361.208294	43.182362
3511.916762	1016122.499810	43.187367
3511.989625	1015869.977156	43.192372
3511.760280	1015606.230626	43.197377
3511.986988	1015363.174589	43.202381
3511.868010	1015105.794557	43.207386
3511.935207	1014866.433038	43.212391
3511.825123	1014623.691829	43.217396
3511.959445	1014368.275557	43.222401
3511.571510	1014131.676831	43.227405
3511.548737	1013869.757134	43.232410
3511.724108	1013635.181368	43.237415
3511.899842	1013362.133324	43.242420
3511.577695	1013120.333466	43.247425
3511.545273	1012890.034680	43.252429
3511.843363	1012641.798278	43.257434
3511.723907	1012394.299722	43.262439
3511.732581	1012152.403805	43.267444
3511.713509	1011913.319499	43.272449
3511.706083	1011665.090378	43.277453
3511.625718	1011414.919108	43.282458
3511.548673	1011166.582330	43.287463
3511.695289	1010921.307203	43.292468
3511.745569	1010665.736814	43.297473
3511.848991	1010426.083357	43.302477
3511.818012	1010168.754610	43.307482
3511.289601	1009942.984620	43.312487
3511.700611	1009684.491919	43.317492
3511.704995	1009444.521481	43.322497
3511.180620	1009196.949164	43.327501
3511.411475	1008956.434659	43.332506
3511.676482	1008713.862913	43.337511
3511.515994	1008466.101370	43.342516
3511.413066	1008233.776851	43.347521
3511.359389	1007994.823681	43.352525
3511.530907	1007763.795695	43.357530
3510.973334	1007508.668465	43.362535
3511.070664	1007267.131669	43.367540
3511.233888	1007046.382354	43.372545
3511.151924	1006813.023531	43.377549
3511.211234	1006556.195792	43.382554
3511.043176	1006328.082337	43.387559
3510.874483	1006085.566327	43.392564
3510.979957	1005861.765373	43.397569
3510.850091	1005614.359886	43.402573
3511.013486	1005405.120472	43.407578
3510.674657	1005169.985298	43.412583
3511.000017	1004939.594584	43.417588
3510.728193	1004719.312346	43.422593
3510.597969	1004466.895563	43.427597
3510.608663	1004240.905845	43.432602
3510.336264	1004022.153086	43.437607
3510.566214	1003795.428428	43.442612
3510.453402	1003566.318727	43.447617
3510.116032	1003347.939766	43.452621
3510.404129	1003137.720184	43.457626
3510.235595	1002915.891094	43.462631
3510.466867	1002705.470197	43.467636
3510.358954	1002470.573932	43.472641
3510.367887	1002265.233681	43.477645
3510.325340	1002025.442225	43.482650
3510.043604	1001808.746483	43.487655
3510.288233	1001593.123710	43.492660
3510.293463	1001380.646848	43.497665
3509.967511	1001163.933699	43.502669
3510.270345	1000947.400709	43.507674
3510.172437	1000749.323668	43.512679
3510.305213	1000511.288746	43.517684
3510.299266	1000315.420408	43.522689
3510.070639	1000077.426778	43.527693
3510.196633	999869.935871	43.532698
3510.145374	999652.827556	43.537703
3510.277764	999435.972776	43.542708
3510.139938	999211.753986	43.547713
3510.161373	999018.854820	43.552717
3510.163836	998791.285547	43.557722
3509.526337	998583.094242	43.562727
3510.077180	998367.687777	43.567732
3509.753377	998173.550689	43.572737
3509.620044	997947.430740	43.577741
3510.064155	997740.101640	43.582746
3509.793269	997535.415135	43.587751
3509.565115	997312.402282	43.592756
3509.656733	997117.770998	43.597761
3509.619119	996905.815198	43.602765
3510.007730	996696.606299	43.607770
3509.846307	996501.605897	43.612775
3509.819929	996289.625226	43.617780
3509.520838	996095.315483	43.622785
3509.768955	995879.961851	43.627789
3509.941502	995656.525614	43.632794
3509.832565	995468.301320	43.637799
3509.549774	995251.257440	43.642804
3509.631441	995054.705685	43.647809
3509.392742	994847.675704	43.652813
3509.715600	994630.215987	43.657818
3509.415734	994441.989110	43.662823
3509.641421	994224.334953	43.667828
3509.936535	994035.509322	43.672833
3510.118434	993828.957687	43.677837
3509.820687	993621.502873	43.682842
3509.573305	993408.671283	43.687847
3509.445839	993208.971027	43.692852
3509.314066	993004.683001	43.697857
3509.205466	992820.854873	43.702861
3509.261152	992598.292375	43.707866
3509.479849	992407.573027	43.712871
3509.488130	992215.322078	43.717876
3509.363620	992002.320082	43.722881
3509.017070	991816.841257	43.727885
3509.268964	991602.299802	43.732890
3509.187175	991425.247258	43.737895
3509.057191	991225.770248	43.742900
3509.240188	991035.205772	43.747905
3509.323932	990831.584244	43.752909
3509.344454	990619.481713	43.757914
3508.892667	990446.360388	43.762919
3509.035978	990237.149030	43.767924
3509.091349	990057.885774	43.772929
3508.800191	989867.262750	43.777933
3509.097613	989676.243790	43.782938
3509.089818	989490.048066	43.787943
3508.759440	989284.976330	43.792948
3508.951616	989115.805195	43.797953
3508.674933	988924.172750	43.802957
3508.952143	988734.686298	43.807962
3508.787251	988560.972589	43.812967
3509.004497	988349.240819	43.817972
3509.011129	988165.048098	43.822977
3508.807865	987965.468857	43.827981
3508.922889	987783.099653	43.832986
3508.709442	987587.509108	43.837991
3509.027462	987418.559549	43.842996
3509.008407	987218.045618	43.848001
3509.018596	987045.135032	43.853005
3508.925877	986833.983486	43.858010
3508.837721	986651.221188	43.863015
3508.826991	986464.243909	43.868020
3508.740030	986267.904100	43.873025
3508.458780	986098.233367	43.878029
3508.638921	985903.496149	43.883034
3508.639838	985723.715027	43.888039
3508.775399	985545.858176	43.893044
3508.692217	985364.713109	43.898049
3508.520351	985187.188534	43.903053
3508.824813	984986.152357	43.908058
3508.558712	984808.241047	43.913063
3508.561337	984607.241235	43.918068
3508.652587	984438.338345	43.923073
3508.516729	984267.710567	43.928077
3508.912814	984078.537877	43.933082
3508.610978	983899.530171	43.938087
3508.845007	983707.149948	43.943092
3508.900476	983521.529840	43.948097
3508.508814	983335.782056	43.953101
3508.529426	983142.832106	43.958106
3508.552425	982976.338362	43.963111
3508.647783	982791.078532	43.968116
3508.548479	982609.848650	43.973121
3508.430304	982446.097063	43.978125
3508.621713	982247.033866	43.983130
3508.460133	982074.196179	43.988135
3508.542633	981873.770602	43.993140
3508.650088	981701.561006	43.998145
3508.454806	981515.721650	44.003149
3508.540775	981341.746605	44.008154
3508.453228	981155.780117	44.013159
3508.503190	980980.139420	44.018164
3508.715039	980805.345841	44.023169
3508.171913	980618.655416	44.028173
3508.270548	980437.910157	44.033178
3508.261225	980266.458092	44.038183
3508.246704	980094.708644	44.043188
3508.469694	979933.759813	44.048193
3508.186732	979768.004564	44.053197
3508.299136	979572.280863	44.058202
3508.077699	979418.230269	44.063207
3508.065754	979224.273927	44.068212
3508.001336	979064.715971	44.073217
3508.167057	978891.825824	44.078221
3508.299973	978703.593414	44.083226
3508.085156	978540.820766	44.088231
3508.144442	978362.166339	44.093236
3507.947197	978200.553857	44.098241
3507.776951	978021.242471	44.103245
3508.288017	977854.616834	44.108250
3507.891518	977675.234134	44.113255
3508.059825	977508.557141	44.118260
3508.117468	977338.276922	44.123265
3507.759087	977171.090377	44.128269
3507.923634	976997.361198	44.133274
3507.644987	976844.032709	44.138279
3507.478785	976655.000150	44.143284
3507.644535	976516.057797	44.148289
3507.776035	976349.255359	44.153293
3507.937129	976199.063342	44.158298
3507.815136	976014.304029	44.163303
3507.628568	975849.592570	44.168308
3507.608129	975672.431668	44.173313
3507.585672	975532.323161	44.178317
3507.685800	975365.986144	44.183322
3507.715133	975217.354567	44.188327
3507.558926	975034.427145	44.193332
3507.896367	974880.162308	44.198337
3507.706905	974712.973943	44.203341
3507.333336	974563.902825	44.208346
3507.503092	974389.800324	44.213351
3507.315780	974225.237875	44.218356
3507.256575	974055.172687	44.223361
3507.390686	973911.869105	44.228365
3507.526812	973733.155393	44.233370
3507.345086	973585.298716	44.238375
3507.476680	973428.485666	44.243380
3507.353888	973284.817479	44.248385
3507.191448	973116.893398	44.253389
3507.512668	972971.187860	44.258394
3507.276994	972807.668710	44.263399
3507.223697	972658.397451	44.268404
3507.428778	972506.927525	44.273409
3507.207482	972343.197107	44.278413
3507.356999	972181.455452	44.283418
3507.075998	972037.586412	44.288423
3507.496906	971873.541141	44.293428
3507.603142	971734.884048	44.298433
3507.485898	971558.296827	44.303437
3507.282949	971417.432563	44.308442
3507.139091	971257.963686	44.313447
3507.368037	971106.942132	44.318452
3507.171515	970943.265536	44.323457
3507.046439	970785.737548	44.328461
3507.273622	970649.480762	44.333466
3507.123175	970488.230105	44.338471
3507.460046	970333.843106	44.343476
3507.243800	970187.959717	44.348481
3507.150155	970034.124913	44.353485
3507.236487	969878.886119	44.358490
3506.968300	969734.565737	44.363495
3507.070220	969584.797464	44.368500
3507.160091	969422.890041	44.373505
3506.673362	969297.877206	44.378509
3507.137725	969132.376120	44.383514
3506.877968	968990.972242	44.388519
3507.066144	968829.815022	44.393524
3507.074093	968692.666916	44.398529
3506.740914	968539.614689	44.403533
3506.787674	968395.306677	44.408538
3506.866273	968265.185422	44.413543
3506.418024	968111.944953	44.418548
3507.070349	967974.771486	44.423553
3506.826987	967833.042693	44.428557
3506.881019	967678.043487	44.433562
3506.824421	967546.851225	44.438567
3506.855589	967392.827227	44.443572
3506.909302	967257.595656	44.448577
3506.886072	967110.818985	44.453581
3506.857675	966973.831699	44.458586
3506.718195	966812.965684	44.463591
3507.025466	966661.912325	44.468596
3506.822583	966524.551366	44.473601
3506.576697	966377.498863	44.478605
3506.882915	966249.938705	44.483610
3506.551039	966103.089220	44.488615
3506.675414	965950.676190	44.493620
3506.997659	965810.273477	44.498625
3506.534708	965666.568597	44.503629
3506.592518	965522.186667	44.508634
3506.487324	965388.798340	44.513639
3506.711914	965253.197659	44.518644
3506.690838	965114.597665	44.523649
3506.424012	964973.781805	44.528653
3506.571635	964844.649323	44.533658
3506.300166	964688.643593	44.538663
3506.351211	964567.259759	44.543668
3506.481726	964428.422349	44.548673
3506.246009	964303.553410	44.553677
3506.521161	964162.922350	44.558682
3506.292982	964045.590303	44.563687
3506.533184	963900.059953	44.568692
3506.939030	963743.133243	44.573697
3506.435742	963622.310687	44.578701
3506.504176	963472.290753	44.583706
3506.383334	963346.598283	44.588711
3506.396635	963207.554784	44.593716
3506.547773	963062.311906	44.598721
3506.199350	962932.042377	44.603725
3506.580624	962791.752339	44.608730
3506.135040	962670.116344	44.613735
3506.301183	962531.227343	44.618740
3506.394023	962404.695141	44.623745
3506.492774	962269.534952	44.628749
3506.499474	962144.089249	44.633754
3506.331269	961997.990105	44.638759
3506.334692	961866.070401	44.643764
3506.263514	961733.767919	44.648769
3506.119096	961607.845377	44.653773
3506.331593	961458.533406	44.658778
3506.177646	961341.820171	44.663783
3506.427150	961207.688464	44.668788
3506.440356	961064.868499	44.673793
3506.202943	960938.652589	44.678797
3506.246511	960818.465338	44.683802
3506.253209	960681.910713	44.688807
3506.178081	960556.247881	44.693812
3506.187330	960430.862516	44.698817
3506.295473	960286.046948	44.703821
3506.619251	960160.309789	44.708826
3506.074705	960019.320497	44.713831
3506.312299	959903.886243	44.718836
3506.427053	959761.801633	44.723841
3505.992391	959646.178816	44.728845
3506.233074	959511.028648	44.733850
3506.180595	959383.081390	44.738855
3506.342150	959236.759917	44.743860
3506.212505	959122.449123	44.748865
3506.121306	958995.970504	44.753869
3506.298249	958868.170161	44.758874
3506.078863	958741.118709	44.763879
3506.078107	958615.205227	44.768884
3506.339733	958476.104790	44.773889
3505.761109	958349.496155	44.778893
3505.995513	958207.843937	44.783898
3505.658065	958085.799164	44.788903
3506.027434	957967.460348	44.793908
3505.922403	957842.331795	44.798913
3505.910398	957720.716091	44.803917
3506.008074	957598.295103	44.808922
3506.049835	957474.311385	44.813927
3505.857025	957359.289491	44.818932
3505.940797	957217.735892	44.823937
3505.764752	957107.708742	44.828941
3505.937689	956973.883625	44.833946
3506.022621	956871.754501	44.838951
3505.887947	956729.440165	44.843956
3505.980455	956623.675824	44.848961
3505.733470	956493.342198	44.853965
3506.014063	956373.219548	44.858970
3506.038953	956237.537811	44.863975
3505.858348	956125.923030	44.868980
3506.028453	955990.505898	44.873985
3505.597324	955869.214582	44.878989
3505.685873	955761.276661	44.883994
3505.442657	955630.790460	44.888999
3505.743843	955519.340142	44.894004
3505.781550	955406.400763	44.899009
3505.974026	955277.941550	44.904013
3505.843269	955167.606597	44.909018
3505.592044	955045.334968	44.914023
3505.807943	954929.104124	44.919028
3505.766460	954827.641177	44.924033
3505.860313	954697.940299	44.929037
3505.868866	954591.586786	44.934042
3505.622090	954457.345091	44.939047
3505.762824	954353.355940	44.944052
3505.569813	954232.107313	44.949057
3505.555563	954120.104464	44.954061
3505.528649	954000.162071	44.959066
3505.448278	953893.234726	44.964071
3505.418111	953786.392527	44.969076
3505.788025	953682.256298	44.974081
3505.852415	953559.610073	44.979085
3505.596307	953461.407772	44.984090
3505.544069	953331.791896	44.989095
3505.886413	953203.734090	44.994100
3505.490426	953101.434197	44.999105
3505.181551	952984.480149	45.004109
3505.398899	952879.778673	45.009114
3505.487214	952774.809280	45.014119
3505.405199	952659.915306	45.019124
3505.158648	952566.191082	45.024129
3505.070029	952444.308739	45.029133
3505.417163	952322.064667	45.034138
3505.227322	952226.411196	45.039143
3505.200116	952117.045787	45.044148
3505.352727	952023.820012	45.049153
3505.318800	951910.910789	45.054157
3505.244226	951801.737834	45.059162
3505.165599	951707.204672	45.064167
3505.295296	951588.232561	45.069172
3505.246279	951494.264783	45.074177
3505.219518	951390.434367	45.079181
3505.100629	951295.134626	45.084186
3505.011841	951186.907953	45.089191
3505.360278	951065.303640	45.094196
3505.211729	950976.702397	45.099201
3505.061610	950870.871891	45.104205
3505.293574	950773.111884	45.109210
3505.263445	950655.101595	45.114215
3505.406718	950560.989338	45.119220
3505.316955	950445.089820	45.124225
3505.556146	950352.393732	45.129229
3505.601881	950237.424422	45.134234
3505.359556	950118.670978	45.139239
3505.482842	950022.159018	45.144244
3505.337369	949911.904544	45.149249
3504.993500	949810.391910	45.154253
3505.119274	949693.769833	45.159258
3504.981124	949605.430427	45.164263
3504.947917	949482.606985	45.169268
3505.172664	949389.895935	45.174273
3504.859477	949284.059612	45.179277
3505.070420	949181.868747	45.184282
3504.798928	949078.223405	45.189287
3505.054812	948996.510764	45.194292
3505.131370	948878.633634	45.199297
3504.775978	948794.912018	45.204301
3504.861142	948701.254070	45.209306
3504.843975	948587.790298	45.214311
3504.912557	948494.418586	45.219316
3505.149078	948406.092651	45.224321
3504.977286	948291.594503	45.229325
3505.043458	948202.527068	45.234330
3504.926171	948087.153557	45.239335
3504.986283	947999.424297	45.244340
3504.855416	947881.750079	45.249345
3504.695782	947800.470005	45.254349
3505.145448	947700.987763	45.259354
3504.895359	947592.041657	45.264359
3504.621955	947506.657492	45.269364
3505.135040	947403.902779	45.274369
3505.043362	947320.975779	45.279373
3505.028426	947213.611172	45.284378
3504.837001	947117.096667	45.289383
3504.667939	947015.787535	45.294388
3504.866381	946922.078659	45.299393
3504.660740	946811.480436	45.304397
3504.506643	946726.063721	45.309402
3504.833505	946636.160043	45.314407
3504.750926	946538.467332	45.319412
3504.622503	946441.929849	45.324417
3504.667521	946349.289603	45.329421
3504.855332	946270.706306	45.334426
3504.642081	946156.934057	45.339431
3504.375016	946089.727178	45.344436
3504.507877	945980.013431	45.349441
3504.453924	945888.626675	45.354445
3504.454636	945795.792221	45.359450
3504.464866	945714.355575	45.364455
3504.494509	945625.728814	45.369460
3504.566169	945525.404760	45.374465
3504.692755	945450.364098	45.379469
3504.747569	945369.681191	45.384474
3504.402895	945257.635484	45.389479
3504.602835	945173.093000	45.394484
3504.795272	945085.867458	45.399489
3504.352823	944989.929563	45.404493
3504.627464	944902.016650	45.409498
3504.409756	944801.534621	45.414503
3504.096145	944721.189789	45.419508
3504.529905	944614.751497	45.424513
3504.359618	944549.616911	45.429517
3504.449942	944447.160720	45.434522
3504.386403	944382.389776	45.439527
3504.183294	944281.032789	45.444532
3504.346507	944202.134723	45.449537
3504.482428	944118.831485	45.454541
3504.022103	944036.583500	45.459546
3504.049757	943959.141645	45.464551
3504.295450	943857.894164	45.469556
3504.276003	943781.224148	45.474561
3504.186551	943712.902956	45.479565
3504.466664	943606.565191	45.484570
3504.523215	943528.153706	45.489575
3504.312774	943441.829568	45.494580
3504.363658	943352.393740	45.499585
3503.860456	943265.827352	45.504589
3504.363273	943184.174063	45.509594
3504.261200	943115.367839	45.514599
3504.017170	943012.938483	45.519604
3504.511493	942934.350097	45.524609
3504.163500	942860.021229	45.529613
3504.230098	942769.326631	45.534618
3504.257204	942690.428083	45.539623
3504.075728	942603.030782	45.544628
3504.420533	942524.173254	45.549633
3504.357411	942455.831237	45.554637
3504.242174	942358.928097	45.559642
3504.260945	942293.638266	45.564647
3504.086293	942209.301081	45.569652
3504.128787	942124.735021	45.574657
3503.909343	942032.444886	45.579661
3504.065636	941961.088130	45.584666
3504.104880	941873.929889	45.589671
3504.080629	941796.368569	45.594676
3504.276636	941706.017695	45.599681
3503.973684	941635.019772	45.604685
3503.984013	941548.532038	45.609690
3504.060558	941485.907334	45.614695
3503.807774	941417.007648	45.619700
3504.056429	941315.518559	45.624705
3503.910724	941233.078598	45.629709
3504.315332	941160.998794	45.634714
3504.305533	941085.725926	45.639719
3504.190144	941002.126625	45.644724
3503.858271	940925.274304	45.649729
3503.698278	940831.802426	45.654733
3503.688015	940765.731111	45.659738
3503.434444	940708.809455	45.664743
3503.539617	940625.359601	45.669748
3504.142077	940565.610172	45.674753
3503.836212	940482.033935	45.679757
3503.601783	940401.993069	45.684762
3503.911192	940341.138496	45.689767
3503.530358	940273.107981	45.694772
3503.869028	940202.560363	45.699777
3503.775398	940135.343927	45.704781
3503.901621	940055.622002	45.709786
3503.721302	939974.318844	45.714791
3503.742916	939913.218971	45.719796
3503.865957	939825.245491	45.724801
3503.682570	939761.012409	45.729805
3503.742605	939688.105856	45.734810
3503.860079	939610.201037	45.739815
3503.509355	939544.266316	45.744820
3503.860080	939450.877514	45.749825
3503.484372	939319.524834	45.754829
3503.931292	939118.294080	45.759834
3504.095458	938877.482207	45.764839
3503.785356	938559.795439	45.769844
3503.908349	938183.971609	45.774849
3503.579765	937759.643355	45.779853
3503.553435	937237.830135	45.784858
3503.544497	936689.666000	45.789863
3503.425116	936052.294709	45.794868
3503.179802	935362.261394	45.799873
3502.925988	934610.597269	45.804877
3503.100709	933778.287314	45.809882
3503.114023	932879.413045	45.814887
3502.356650	931907.701387	45.819892
3502.464389	930855.637421	45.824897
3502.462040	929737.365069	45.829901
3502.595584	928536.077957	45.834906
3502.199688	927248.080900	45.839911
3502.136337	925918.657201	45.844916
3502.079930	924470.877390	45.849921
3501.583222	922967.359991	45.854925
3501.572712	921348.426343	45.859930
3501.467405	919690.130003	45.864935
3500.864296	917913.241815	45.869940
3500.954049	916061.383644	45.874945
3500.309157	914136.741043	45.879949
3500.062492	912102.514238	45.884954
3500.219859	910013.945053	45.889959
3499.529388	907805.186576	45.894964
3499.462959	905522.768207	45.899969
3499.032716	903178.258297	45.904973
3498.786302	900711.114796	45.909978
3498.156699	898190.670875	45.914983
3497.947515	895564.901191	45.919988
3497.609884	892880.869821	45.924993
3497.353175	890077.202034	45.929997
3496.775837	887200.956207	45.935002
3496.200010	884231.634363	45.940007
3495.736342	881196.324260	45.945012
3495.149687	878040.272643	45.950017
3494.782707	874849.411283	45.955021
3494.436259	871531.103778	45.960026
3494.181881	868158.291079	45.965031
3493.298070	864687.176363	45.970036
3492.861687	861136.101931	45.975041
3492.081943	857506.145187	45.980045
3491.651931	853779.249741	45.985050
3491.067824	849978.141756	45.990055
3490.520026	846075.375396	45.995060
3490.231992	842094.354197	46.000065
3489.275312	838053.995008	46.005069
3488.827032	833888.617850	46.010074
3488.101583	829665.676478	46.015079
3487.380708	825346.062183	46.020084
3486.704985	820935.918157	46.025089
3485.758301	816453.949467	46.030093
3485.137194	811887.105620	46.035098
3484.921564	807228.957274	46.040103
3483.834871	802509.985100	46.045108
3483.129748	797675.191985	46.050113
3482.334881	792784.105480	46.055117
3481.768058	787787.029677	46.060122
3480.930662	782717.620639	46.065127
3480.062001	777551.354408	46.070132
3479.192752	772294.667920	46.075137
3478.194431	766959.024332	46.080141
3477.151016	761517.789891	46.085146
3476.372494	756031.329906	46.090151
3475.434788	750432.856257	46.095156
3474.672566	744771.778667	46.100161
3473.582546	739009.598838	46.105165
3472.472075	733165.272863	46.110170
3471.638752	727248.646884	46.115175
3470.783727	721232.498197	46.120180
3469.731352	715133.184764	46.125185
3468.628163	708942.574520	46.130189
3467.716183	702659.010470	46.135194
3466.417241	696298.179580	46.140199
3465.347269	689847.595853	46.145204
3463.933109	683335.633670	46.150209
3462.679138	676728.114618	46.155213
3462.063904	670031.226257	46.160218
3460.853172	663266.585207	46.165223
3459.575110	656388.094999	46.170228
3458.262032	649449.642256	46.175233
3457.075269	642421.908951	46.180237
3456.059859	635316.616025	46.185242
3454.476324	628114.694234	46.190247
3452.962519	620850.182461	46.195252
3452.180371	613477.762414	46.200257
3450.433387	606034.149562	46.205261
3449.271751	598508.466091	46.210266
3447.492583	590906.698553	46.215271
3446.179994	583236.991003	46.220276
3445.146339	575461.178818	46.225281
3443.393348	567616.463848	46.230285
3441.693173	559696.980206	46.235290
3439.889018	551678.607455	46.240295
3438.287226	543611.443929	46.245300
3437.257064	535433.865232	46.250305
3435.473732	527207.549357	46.255309
3434.036732	518882.314264	46.260314
3432.300287	510488.182153	46.265319
3430.369642	502023.967550	46.270324
3429.107806	493458.610993	46.275329
3426.747942	484845.368024	46.280333
3424.941609	476132.754763	46.285338
3423.133061	467374.351078	46.290343
3420.924736	458522.477117	46.295348
3419.337135	449601.108191	46.300353
3417.119088	440628.909395	46.305357
3415.267935	431553.000530	46.310362
3413.177698	422439.987964	46.315367
3410.737854	413236.935257	46.320372
3408.722018	403977.324108	46.325377
3406.321902	394637.871825	46.330381
3404.442877	385255.797831	46.335386
3402.135307	375813.398276	46.340391
3399.856334	366291.706788	46.345396
3397.619824	356727.100625	46.350401
3394.754375	347093.311439	46.355405
3392.545874	337405.599165	46.360410
3390.251587	327648.929936	46.365415
3387.222921	317858.481768	46.370420
3384.422266	307990.848646	46.375425
3381.822987	298107.533841	46.380429
3378.954991	288143.780709	46.385434
3376.286428	278156.527851	46.390439
3373.021886	268111.407634	46.395444
3370.278554	258031.705774	46.400449
3367.250378	247909.655268	46.405453
3364.074132	237762.756000	46.410458
3360.741208	227549.353295	46.415463
3357.523742	217278.589004	46.420468
3354.229329	206982.155142	46.425473
3350.110875	196684.583359	46.430477
3346.722521	186399.362139	46.435482
3342.569483	176071.425264	46.440487
3338.708379	165745.059142	46.445492
3334.946757	155406.768260	46.450497
3330.273472	145055.920725	46.455501
3325.482854	134724.291305	46.460506
3320.481661	124368.548300	46.465511
3314.790563	114082.329631	46.470516
3309.124368	103797.997165	46.475521
3302.139266	93587.570972	46.480525
3291.146648	83548.678079	46.485530
3270.614329	73850.982135	46.490535
3245.982179	64480.655085	46.495540
3222.085167	55428.420851	46.500545
3196.589695	46858.572784	46.505549
3165.669462	38890.010464	46.510554
3128.901992	31683.003779	46.515559
3089.280074	25240.581292	46.520564
3051.068790	19549.160652	46.525569
3015.944196	14651.434139	46.530573
2985.114093	10482.271329	46.535578
2958.198070	7029.957307	46.540583
2934.888365	4246.463366	46.545588
2915.368629	2073.815064	46.550593
2894.083497	590.576675	46.555597
2848.997204	343.647861	46.560602
2821.608027	352.435859	46.565607
2820.690354	346.217205	46.570612
2836.189606	326.268444	46.575617
2855.844752	335.423129	46.580621
2872.981229	325.611192	46.585626
2883.226306	329.453401	46.590631
2886.144568	324.588811	46.595636
2885.979375	313.530459	46.600641
2881.610229	302.111079	46.605645
2877.194427	331.005672	46.610650
2873.297669	321.863023	46.615655
2869.920899	321.273283	46.620660
2867.825426	316.371460	46.625665
2865.587961	319.618783	46.630669
2863.039961	310.035870	46.635674
2860.612229	325.624506	46.640679
2858.062388	312.922926	46.645684
2855.957493	307.394056	46.650689
2852.849978	303.582468	46.655693
2849.431313	309.051125	46.660698
2846.477850	310.164672	46.665703
2843.009041	316.935515	46.670708
2840.320476	293.816736	46.675713
2836.885150	297.917972	46.680717
2833.599170	288.014202	46.685722
2830.864125	300.616992	46.690727
2827.806971	292.547310	46.695732
2824.712195	292.041221	46.700737
2821.534278	285.765405	46.705741
2817.957073	295.608464	46.710746
2814.957504	285.336573	46.715751
2811.465559	300.265659	46.720756
2808.044014	274.527531	46.725761
2804.917017	286.313783	46.730765
2801.670559	284.559518	46.735770
2798.850517	284.444086	46.740775
2794.911860	280.817010	46.745780
2791.755468	287.148455	46.750785
2788.358915	291.112603	46.755789
2785.064196	276.721178	46.760794
2781.906727	266.752460	46.765799
2778.337037	266.814692	46.770804
2774.917102	276.054223	46.775809
2771.359508	269.021441	46.780813
2768.323173	285.863526	46.785818
2765.456016	274.137024	46.790823
2761.479536	274.816313	46.795828
2758.039738	269.979231	46.800833
2754.494687	282.878051	46.805837
2751.192967	286.307869	46.810842
2747.975320	266.783076	46.815847
2744.060844	287.655624	46.820852
2740.946649	270.589527	46.825857
2737.805970	272.795663	46.830861
2734.491907	273.782944	46.835866
2730.773896	270.802291	46.840871
2727.340653	273.744860	46.845876
2724.219729	271.993115	46.850881
2720.227656	268.879097	46.855885
2716.573514	270.466123	46.860890
2713.831240	258.903250	46.865895
2710.099638	272.583471	46.870900
2706.820943	267.272173	46.875905
2703.574802	252.632594	46.880909
2700.094159	262.753438	46.885914
2697.063124	258.346885	46.890919
2693.364487	260.049576	46.895924
2689.992203	257.301385	46.900929
2685.644315	262.302393	46.905933
2682.455524	256.049659	46.910938
2679.274512	244.256888	46.915943
2675.512031	275.573316	46.920948
2672.667004	261.791476	46.925953
2668.903037	270.249330	46.930957
2665.338834	262.923027	46.935962
2662.221070	268.786946	46.940967
2657.958067	262.992991	46.945972
2654.606586	264.789198	46.950977
2651.803657	256.466194	46.955981
2647.795857	266.337580	46.960986
2644.603258	251.246955	46.965991
2641.130041	261.473925	46.970996
2638.072947	246.561424	46.976001
2634.567990	261.028715	46.981005
2630.547744	250.248888	46.986010
2626.731527	248.480333	46.991015
2622.884730	260.807827	46.996020
2620.180361	257.268252	47.001025
2616.877699	271.885395	47.006029
2613.930966	248.375029	47.011034
2610.645371	248.974507	47.016039
2606.697311	263.609774	47.021044
2603.428212	242.645490	47.026049
2599.416842	254.197205	47.031053
2596.322572	251.959608	47.036058
2592.378068	249.415322	47.041063
2588.891348	254.789826	47.046068
2585.675907	241.031149	47.051073
2581.961714	247.123064	47.056077
2578.696815	261.219911	47.061082
2575.553091	247.280123	47.066087
2571.794333	240.132757	47.071092
2568.381255	249.038857	47.076097
2564.632744	248.791119	47.081101
2561.186306	265.961684	47.086106
2557.950562	243.718345	47.091111
2554.460347	253.157260	47.096116
2550.705309	251.138145	47.101121
2547.415763	246.490767	47.106125
2543.692206	255.340647	47.111130
2540.156425	247.980434	47.116135
2536.841794	243.446504	47.121140
2534.207064	238.123815	47.126145
2530.536734	236.335792	47.131149
2526.657830	249.928180	47.136154
2523.051448	235.347437	47.141159
2519.353340	246.477678	47.146164
2515.773881	233.049873	47.151169
2512.344724	237.049189	47.156173
2508.716995	248.095420	47.161178
2505.790110	232.561936	47.166183
2501.934897	247.571684	47.171188
2498.681506	231.564858	47.176193
2495.159868	239.864719	47.181197
2491.837999	236.632716	47.186202
2488.370355	238.103166	47.191207
2484.054492	241.425381	47.196212
2481.259290	242.392805	47.201217
2477.957914	244.131003	47.206221
2474.039313	245.608546	47.211226
2470.785841	225.834779	47.216231
2466.846365	244.746844	47.221236
2463.220763	239.548622	47.226241
2459.923949	233.070152	47.231245
2456.609520	249.966808	47.236250
2453.649430	221.647001	47.241255
2449.857464	240.453946	47.246260
2446.495002	236.182173	47.251265
2442.848396	235.697798	47.256269
2439.213603	233.865093	47.261274
2436.201715	215.752553	47.266279
2432.243880	242.022642	47.271284
2428.669033	228.890974	47.276289
2425.178309	233.473440	47.281293
2421.627477	219.554736	47.286298
2418.230514	224.499670	47.291303
2414.518868	224.251156	47.296308
2411.216192	228.026235	47.301313
2407.990725	223.757443	47.306317
2404.648767	237.738485	47.311322
2401.017196	223.717387	47.316327
2397.361989	226.340366	47.321332
2393.583817	232.840172	47.326337
2390.235939	226.616690	47.331341
2386.890905	228.323355	47.336346
2383.551502	234.868790	47.341351
2379.934819	234.538535	47.346356
2376.464340	235.400630	47.351361
2372.665124	229.153434	47.356365
2369.127056	227.926410	47.361370
2366.071181	213.061642	47.366375
2362.375174	218.611713	47.371380
2359.327960	207.147289	47.376385
2355.697234	228.799564	47.381389
2352.064595	217.102787	47.386394
2348.789334	222.776039	47.391399
2344.913291	222.860095	47.396404
2341.421183	229.864002	47.401409
2338.082995	220.974204	47.406413
2334.353167	228.485317	47.411418
2330.986770	214.599490	47.416423
2327.170769	226.758919	47.421428
2323.787006	204.568618	47.426433
2320.536127	223.104330	47.431437
2316.904902	220.982449	47.436442
2313.554257	216.246621	47.441447
2309.977044	227.770136	47.446452
2306.533307	217.836188	47.451457
2303.016222	220.054159	47.456461
2299.302423	234.443905	47.461466
2295.947439	213.932432	47.466471
2292.149564	203.590591	47.471476
2289.084888	207.930595	47.476481
2285.372187	205.776989	47.481485
2282.176988	226.746998	47.486490
2278.742793	211.790489	47.491495
2274.865247	204.607066	47.496500
2271.622842	210.935486	47.501505
2267.921872	212.736323	47.506509
2264.509233	231.796922	47.511514
2261.406274	212.036661	47.516519
2257.316784	225.720289	47.521524
2254.107987	208.778374	47.526529
2250.505814	213.303133	47.531533
2246.730193	217.009491	47.536538
2243.462856	202.698187	47.541543
2239.987860	204.757912	47.546548
2236.579294	210.487026	47.551553
2233.039164	194.263215	47.556557
2229.323723	198.997451	47.561562
2226.236979	224.897578	47.566567
2222.548028	226.918517	47.571572
2219.427504	213.308673	47.576577
2215.915612	216.040385	47.581581
2212.285981	211.097590	47.586586
2208.690240	220.446487	47.591591
2204.843567	211.809134	47.596596
2201.288715	211.078904	47.601601
2197.855264	218.203701	47.606605
2194.573484	218.213884	47.611610
2191.390784	211.664256	47.616615
2187.560661	204.581579	47.621620
2184.462265	214.999004	47.626625
2180.772417	200.537343	47.631629
2177.067372	209.213331	47.636634
2173.513340	200.113600	47.641639
2169.691181	206.960007	47.646644
2166.339324	201.789905	47.651649
2163.019498	203.140226	47.656653
2159.680006	204.935252	47.661658
2156.402178	205.758073	47.666663
2152.522819	201.248641	47.671668
2149.103953	203.809662	47.676673
2145.632742	192.604119	47.681677
2141.580698	206.600536	47.686682
2138.611811	195.262316	47.691687
2134.995872	205.335697	47.696692
2131.553195	188.861687	47.701697
2128.121314	200.322406	47.706701
2124.486584	194.373781	47.711706
2121.175317	204.385860	47.716711
2117.572713	209.080819	47.721716
2113.964546	207.389203	47.726721
2110.800517	199.948197	47.731725
2106.805622	210.778008	47.736730
2103.558619	208.110755	47.741735
2100.055882	207.513737	47.746740
2096.667788	190.863828	47.751745
2093.120021	203.788998	47.756749
2089.493561	201.022759	47.761754
2086.155052	207.894581	47.766759
2082.822239	198.263089	47.771764
2079.212248	206.057682	47.776769
2075.516594	200.570654	47.781773
2071.921239	206.373164	47.786778
2068.586879	198.664723	47.791783
2065.024420	204.790215	47.796788
2061.749388	200.346382	47.801793
2058.239405	199.836702	47.806797
2054.572771	207.275941	47.811802
2050.910724	193.728514	47.816807
2047.293607	205.256223	47.821812
2044.066826	197.495028	47.826817
2040.349509	205.319081	47.831821
2036.875107	190.837077	47.836826
2033.623155	189.964625	47.841831
2030.082941	192.216422	47.846836
2026.620850	202.252033	47.851841
2023.384279	189.178886	47.856845
2019.337907	203.095296	47.861850
2016.240117	184.743588	47.866855
2012.437418	203.569558	47.871860
2008.909559	208.000677	47.876865
2005.775972	179.175403	47.881869
2001.707884	195.260363	47.886874
1998.817903	188.177787	47.891879
1994.917478	195.845615	47.896884
1991.714093	190.830754	47.901889
1988.224443	187.098810	47.906893
1984.254095	188.221908	47.911898
1980.952748	181.005865	47.916903
1977.401981	183.480698	47.921908
1974.239175	198.204509	47.926913
1970.877320	169.089223	47.931917
1967.117192	195.644286	47.936922
1963.939728	178.989815	47.941927
1960.182622	196.086932	47.946932
1956.760911	172.570732	47.951937
1953.003304	190.930940	47.956941
1949.527442	188.584646	47.961946
1946.161291	186.598772	47.966951
1942.635055	187.393416	47.971956
1939.122291	181.208736	47.976961
1935.723152	182.940008	47.981965
1932.002082	185.040764	47.986970
1928.390904	184.358436	47.991975
1924.721688	190.171710	47.996980
1921.302785	203.892302	48.001985
1918.409626	194.727688	48.006989
1914.651958	189.417606	48.011994
1911.510673	186.768914	48.016999
1907.596093	196.278935	48.022004
1904.137304	196.520389	48.027009
1900.611661	179.621335	48.032013
1896.720326	200.644291	48.037018
1893.191985	194.288281	48.042023
1889.999198	189.016219	48.047028
1886.162161	180.947392	48.052033
1883.199040	172.884135	48.057037
1879.848976	189.244678	48.062042
1875.735141	185.517226	48.067047
1872.515507	184.353531	48.072052
1868.810798	174.266413	48.077057
1865.380069	175.514020	48.082061
1862.089011	182.404724	48.087066
1858.742281	167.212031	48.092071
1855.195441	187.385693	48.097076
1851.628909	183.547929	48.102081
1848.120323	182.959992	48.107085
1844.505158	169.282167	48.112090
1840.853876	182.315245	48.117095
1837.620673	175.918766	48.122100
1833.787927	187.340755	48.127105
1830.480223	175.798970	48.132109
1826.313254	198.037606	48.137114
1823.357288	181.049540	48.142119
1819.906535	195.694926	48.147124
1816.558350	172.223123	48.152129
1812.920808	187.988120	48.157133
1809.451287	187.170414	48.162138
1806.379581	184.106913	48.167143
1802.603635	181.811786	48.172148
1799.344645	184.823353	48.177153
1795.661292	192.467587	48.182157
1791.930774	192.952118	48.187162
1788.358281	181.804940	48.192167
1784.917068	182.354100	48.197172
1781.458478	190.688104	48.202177
1778.090110	179.498474	48.207181
1774.339612	194.058183	48.212186
1770.857556	181.200110	48.217191
1767.383376	178.633643	48.222196
1764.244628	194.759889	48.227201
1760.276925	189.958367	48.232205
1756.477904	175.433542	48.237210
1753.348547	182.819954	48.242215
1750.066492	184.556061	48.247220
1746.644663	193.886196	48.252225
1742.788652	183.984716	48.257229
1739.114563	188.988372	48.262234
1736.167416	177.107970	48.267239
1732.727714	190.683872	48.272244
1729.295060	182.540522	48.277249
1725.502703	187.824430	48.282253
1721.920749	193.797414	48.287258
1718.379779	188.150314	48.292263
1714.815806	192.548650	48.297268
1711.647420	182.505020	48.302273
1708.354349	186.028716	48.307277
1704.264530	189.405697	48.312282
1701.053967	183.497022	48.317287
1697.137933	193.888906	48.322292
1693.639407	175.610840	48.327297
1690.705815	192.170056	48.332301
1686.761336	184.096293	48.337306
1683.617962	172.896529	48.342311
1679.906414	190.008312	48.347316
1676.773014	176.683375	48.352321
1673.274558	184.162885	48.357325
1669.373276	188.452453	48.362330
1665.303966	183.471051	48.367335
1661.981741	177.215921	48.372340
1658.701690	178.522711	48.377345
1655.582908	171.894956	48.382349
1651.614104	181.481999	48.387354
1648.479724	180.725671	48.392359
1644.826187	183.654931	48.397364
1641.472043	180.274100	48.402369
1638.000658	184.722199	48.407373
1634.137876	173.841439	48.412378
1630.946958	183.693241	48.417383
1627.447992	173.436286	48.422388
1624.185472	183.337689	48.427393
1620.670850	171.252389	48.432397
1616.928270	178.991406	48.437402
1613.358481	182.056709	48.442407
1609.622981	176.049548	48.447412
1605.980869	163.816119	48.452417
1602.874783	172.990607	48.457421
1599.405571	168.123697	48.462426
1596.177264	176.943591	48.467431
1592.205298	161.652026	48.472436
1588.814514	172.480300	48.477441
1585.534387	174.467321	48.482445
1581.482281	179.196939	48.487450
1578.336693	186.770176	48.492455
1574.586742	167.466407	48.497460
1571.284516	180.267171	48.502465
1568.304119	172.718519	48.507469
1564.411039	165.326514	48.512474
1560.995508	169.204704	48.517479
1557.467858	170.290091	48.522484
1553.587172	171.478136	48.527489
1550.314814	169.994399	48.532493
1546.435958	170.374406	48.537498
1543.374110	162.308482	48.542503
1539.637983	166.929937	48.547508
1536.105452	155.827345	48.552513
1532.824853	180.647518	48.557517
1528.957462	176.718418	48.562522
1525.819540	179.494572	48.567527
1522.460455	168.792478	48.572532
1518.876565	171.067999	48.577537
1515.806868	161.132601	48.582541
1511.977106	170.902833	48.587546
1508.024004	159.527551	48.592551
1504.848233	173.615845	48.597556
1501.198831	165.586341	48.602561
1497.973201	180.204823	48.607565
1494.234657	182.934413	48.612570
1490.768934	173.313276	48.617575
1487.229077	178.684556	48.622580
1483.550383	170.367795	48.627585
1480.374138	185.298055	48.632589
1476.545859	174.009316	48.637594
1473.441962	174.635341	48.642599
1469.827920	165.160926	48.647604
1466.047439	182.675790	48.652609
1462.790630	165.990843	48.657613
1459.110598	187.327572	48.662618
1456.084995	161.957082	48.667623
1452.427820	171.227608	48.672628
1448.765707	175.279526	48.677633
1445.356035	169.192447	48.682637
1441.578372	164.437895	48.687642
1437.893944	174.395973	48.692647
1434.346678	166.013653	48.697652
1431.057754	168.767120	48.702657
1428.038673	164.806090	48.707661
1423.942962	173.105500	48.712666
1420.838610	158.188375	48.717671
1417.067672	174.715477	48.722676
1413.643843	153.165641	48.727681
1410.315633	165.547236	48.732685
1406.940376	159.892011	48.737690
1403.488437	173.854072	48.742695
1399.913169	168.692552	48.747700
1396.124446	171.747728	48.752705
1392.810691	159.132434	48.757709
1388.916056	170.859477	48.762714
1385.957319	161.309508	48.767719
1382.174653	169.042615	48.772724
1378.550338	167.636980	48.777729
1375.155170	161.924587	48.782733
1371.163062	169.053615	48.787738
1368.042866	161.202408	48.792743
1364.523402	153.573665	48.797748
1361.155582	163.923727	48.802753
1357.921171	158.662763	48.807757
1354.188250	159.640672	48.812762
1350.448599	163.848672	48.817767
1347.286284	153.361132	48.822772
1343.752940	176.396376	48.827777
1339.980451	162.241947	48.832781
1336.585527	168.454619	48.837786
1333.372875	165.681653	48.842791
1329.612485	173.624388	48.847796
1326.034286	166.995398	48.852801
1322.926815	152.163494	48.857805
1319.042473	152.916439	48.862810
1315.400614	170.843207	48.867815
1312.019500	164.081368	48.872820
1308.554186	169.139641	48.877825
1305.400791	163.565832	48.882829
1301.393577	166.704178	48.887834
1298.308279	173.426775	48.892839
1294.700103	170.901814	48.897844
1291.098668	163.504655	48.902849
1287.807602	165.738561	48.907853
1284.209185	158.085312	48.912858
1280.815829	176.559517	48.917863
1276.788318	168.780984	48.922868
1273.217869	174.224688	48.927873
1269.819026	152.950602	48.932877
1266.291941	172.586868	48.937882
1263.563707	163.198874	48.942887
1259.739977	166.220439	48.947892
1255.765593	163.738295	48.952897
1252.443904	163.454425	48.957901
1249.037847	174.635355	48.962906
1245.573756	158.114599	48.967911
1242.057462	182.562576	48.972916
1238.335569	166.457759	48.977921
1235.341791	154.375522	48.982925
1231.729364	162.627699	48.987930
1227.988667	171.317948	48.992935
1224.573330	160.648605	48.997940
1220.665665	167.860642	49.002945
1217.539498	159.750266	49.007949
1213.818845	160.568682	49.012954
1210.633028	150.565029	49.017959
1207.012927	153.737477	49.022964
1203.515217	163.643418	49.027969
1200.054263	174.364649	49.032973
1196.601766	165.856736	49.037978
1192.902984	166.459458	49.042983
1189.503821	161.749704	49.047988
1186.132503	164.829303	49.052993
1182.557202	152.123950	49.057997
1178.961384	173.589983	49.063002
1175.765583	158.097001	49.068007
1171.888945	158.367745	49.073012
1168.763015	171.628141	49.078017
1164.949196	167.690714	49.083021
1161.132481	158.771216	49.088026
1157.883130	157.731146	49.093031
1154.794324	168.927996	49.098036
1150.853981	166.749757	49.103041
1147.134920	165.892791	49.108045
1143.732021	161.569100	49.113050
1140.401395	161.895621	49.118055
1136.958268	169.093354	49.123060
1133.486170	161.894926	49.128065
1130.203269	170.227207	49.133069
1126.546927	166.841393	49.138074
1123.249409	168.561592	49.143079
1119.552637	162.149798	49.148084
1115.962397	161.962911	49.153089
1112.155152	166.827255	49.158093
1108.520037	157.817635	49.163098
1105.411628	167.681837	49.168103
1102.217495	162.040973	49.173108
1098.662381	156.526495	49.178113
1095.025218	157.953663	49.183117
1091.007397	168.946709	49.188122
1087.854188	161.517204	49.193127
1084.211745	165.811686	49.198132
1080.836175	151.173253	49.203137
1077.621335	165.032351	49.208141
1073.819996	158.010249	49.213146
1070.742334	153.882879	49.218151
1067.357051	156.844387	49.223156
1063.373561	147.479673	49.228161
1059.903495	166.876829	49.233165
1056.239333	150.518276	49.238170
1052.612812	155.225749	49.243175
1049.292743	147.850062	49.248180
1045.557972	151.986478	49.253185
1042.117620	154.703859	49.258189
1038.691938	164.875967	49.263194
1035.295251	146.652316	49.268199
1032.102157	155.496781	49.273204
1028.467174	138.322553	49.278209
1025.311415	152.919856	49.283213
1021.540667	151.565230	49.288218
1018.060393	150.207926	49.293223
1014.210209	136.501226	49.298228
1010.674216	153.477285	49.303233
1007.331386	146.895950	49.308237
1003.445471	154.328135	49.313242
1000.030091	155.648792	49.318247
996.604700	163.717779	49.323252
993.075979	148.426091	49.328257
990.130842	150.239395	49.333261
986.435353	152.196720	49.338266
982.850005	157.596453	49.343271
979.552273	161.111270	49.348276
975.805720	148.840469	49.353281
972.041503	169.482929	49.358285
968.655194	157.244486	49.363290
965.218703	168.264815	49.368295
962.243473	154.344907	49.373300
958.626846	166.337666	49.378305
954.891004	145.582916	49.383309
951.309341	162.598805	49.388314
947.927227	146.696969	49.393319
944.257771	166.143852	49.398324
940.258748	150.608853	49.403329
936.796157	150.592166	49.408333
933.541569	162.826228	49.413338
930.360249	149.778688	49.418343
927.132298	159.109072	49.423348
923.196091	143.460732	49.428353
919.977325	140.840315	49.433357
916.398152	143.905824	49.438362
912.908384	129.865743	49.443367
909.114354	152.317106	49.448372
906.063177	148.067759	49.453377
902.359000	135.328646	49.458381
898.243239	148.388348	49.463386
895.293624	136.249507	49.468391
891.672150	146.334234	49.473396
888.010983	153.543904	49.478401
884.602317	151.925759	49.483405
880.940358	158.789704	49.488410
877.423324	140.867094	49.493415
874.140682	156.303490	49.498420
870.940101	151.821952	49.503425
867.449747	139.393904	49.508429
863.596349	151.603554	49.513434
859.940917	159.357720	49.518439
857.134606	144.193654	49.523444
853.655637	156.369004	49.528449
849.900935	158.094492	49.533453
846.030687	157.389326	49.538458
842.422443	139.808627	49.543463
838.948292	145.765675	49.548468
835.343294	160.743928	49.553473
832.392561	132.146422	49.558477
828.840346	149.893393	49.563482
825.769313	140.586117	49.568487
821.650831	152.608529	49.573492
817.923423	149.822875	49.578497
814.840125	143.651292	49.583501
810.777450	160.138002	49.588506
807.587996	141.910777	49.593511
804.340129	146.286528	49.598516
800.788003	143.400518	49.603521
797.499210	151.371954	49.608525
793.465961	161.770962	49.613530
790.002020	152.439013	49.618535
786.487436	157.330459	49.623540
782.560051	164.400169	49.628545
779.785924	153.081959	49.633549
776.291215	160.437323	49.638554
772.800191	148.347311	49.643559
769.317594	142.860221	49.648564
765.449077	145.432998	49.653569
762.049454	140.939803	49.658573
758.107737	135.079302	49.663578
754.936712	132.441518	49.668583
751.730556	142.027510	49.673588
747.896880	134.293501	49.678593
744.884050	147.774557	49.683597
741.475438	142.578805	49.688602
737.500785	144.470105	49.693607
734.370773	155.048563	49.698612
730.771061	145.844632	49.703617
727.144576	135.109376	49.708621
723.260188	145.807883	49.713626
719.688028	147.845110	49.718631
716.584052	159.096004	49.723636
713.044757	152.464122	49.728641
709.657757	142.424447	49.733645
705.915674	147.352317	49.738650
702.650725	152.218948	49.743655
699.157077	146.495882	49.748660
695.412906	125.402997	49.753665
692.224525	143.564315	49.758669
688.514907	142.066317	49.763674
684.911310	135.047529	49.768679
681.608632	134.456969	49.773684
678.096817	147.111120	49.778689
674.636449	126.044475	49.783693
670.946974	148.662227	49.788698
667.524428	133.395072	49.793703
664.251247	141.875372	49.798708
660.626779	145.419437	49.803713
656.918674	134.626091	49.808717
653.354303	133.974694	49.813722
649.847672	157.280325	49.818727
646.371624	147.187228	49.823732
642.710345	142.743729	49.828737
639.822994	140.001735	49.833741
636.252983	144.093983	49.838746
632.811072	138.511965	49.843751
629.095534	142.926269	49.848756
625.422056	150.939118	49.853761
621.821449	143.773971	49.858765
618.130623	136.281422	49.863770
614.951553	146.797981	49.868775
611.484268	146.297187	49.873780
608.094646	142.421148	49.878785
604.727362	136.715249	49.883789
600.777923	154.032997	49.888794
597.457146	127.149453	49.893799
593.936663	140.426348	49.898804
590.304457	132.412154	49.903809
586.993358	147.297356	49.908813
583.601588	136.655812	49.913818
579.977704	145.064058	49.918823
576.443974	139.178409	49.923828
572.855070	157.187922	49.928833
569.393700	138.254179	49.933837
565.762119	144.822241	49.938842
562.396929	139.111088	49.943847
558.914544	147.363685	49.948852
555.264430	143.383816	49.953857
551.961024	151.629938	49.958861
548.253247	142.089339	49.963866
544.687454	142.316006	49.968871
541.689458	138.143197	49.973876
537.895106	135.544267	49.978881
534.527610	146.329722	49.983885
530.848105	127.863145	49.988890
527.267164	140.683252	49.993895
524.062729	136.677925	49.998900
520.447845	132.849802	50.003905
517.382586	133.924349	50.008909
513.403524	140.938112	50.013914
509.362941	137.435417	50.018919
506.237407	144.699431	50.023924
502.691205	135.625515	50.028929
499.490919	136.922236	50.033933
495.609514	127.860493	50.038938
492.576816	145.017469	50.043943
488.937174	133.697691	50.048948
485.090364	135.083462	50.053953
481.993505	126.327660	50.058957
478.455553	144.610515	50.063962
474.943870	138.905954	50.068967
471.551964	130.354069	50.073972
467.342522	155.339219	50.078977
464.248070	144.701703	50.083981
460.417130	150.112958	50.088986
457.197242	150.566835	50.093991
453.818409	139.719724	50.098996
450.226802	149.635071	50.104001
447.202978	140.446680	50.109005
443.188833	138.165065	50.114010
439.704614	148.495149	50.119015
436.226808	138.799738	50.124020
432.152549	147.716704	50.129025
429.445943	137.100472	50.134029
425.808232	140.413446	50.139034
422.688400	140.843018	50.144039
418.889677	131.837509	50.149044
415.170134	137.401931	50.154049
411.714770	135.624352	50.159053
408.216927	147.051591	50.164058
404.592081	143.244910	50.169063
401.329443	127.068630	50.174068
397.926736	133.712206	50.179073
394.763131	139.395803	50.184077
390.672330	127.764820	50.189082
386.944216	135.381459	50.194087
383.858790	134.238148	50.199092
380.061172	140.555049	50.204097
376.695648	128.333705	50.209101
373.032174	144.017447	50.214106
369.876440	139.747574	50.219111
366.556017	152.705440	50.224116
362.729909	141.105809	50.229121
359.327254	137.772359	50.234125
355.481654	135.772119	50.239130
352.014215	152.343380	50.244135
348.902989	139.672320	50.249140
345.095422	145.736079	50.254145
341.600407	140.189542	50.259149
337.956548	141.213964	50.264154
334.725261	132.457961	50.269159
331.376348	137.246983	50.274164
327.605314	131.616734	50.279169
324.021114	143.091911	50.284173
320.658559	132.679409	50.289178
317.467750	129.053514	50.294183
313.939054	126.718910	50.299188
309.856051	124.919507	50.304193
307.001284	127.652859	50.309197
303.256832	134.110860	50.314202
299.783918	134.951690	50.319207
295.969968	133.602166	50.324212
292.903812	132.309028	50.329217
289.185315	116.234789	50.334221
285.540182	132.399292	50.339226
282.103204	121.916649	50.344231
278.529754	130.384664	50.349236
274.670538	128.864673	50.354241
271.692699	136.156363	50.359245
268.030254	125.971211	50.364250
264.853300	134.527812	50.369255
261.406416	118.075286	50.374260
257.743644	141.051181	50.379265
254.137117	130.781133	50.384269
250.701762	135.280147	50.389274
246.964108	123.853231	50.394279
243.529853	136.826981	50.399284
239.936926	139.693376	50.404289
236.347234	139.053104	50.409293
233.279955	138.836820	50.414298
229.004568	135.702987	50.419303
225.931476	137.614017	50.424308
222.584824	127.308945	50.429313
219.410207	137.279786	50.434317
215.784914	126.265809	50.439322
212.012049	139.585448	50.444327
208.641105	125.855902	50.449332
204.861283	138.274166	50.454337
201.746267	140.360329	50.459341
198.142770	126.329967	50.464346
194.529644	130.045625	50.469351
191.313589	131.111602	50.474356
187.453839	136.737881	50.479361
184.181738	123.092643	50.484365
180.378372	129.124912	50.489370
176.919597	123.515969	50.494375
173.574704	125.600472	50.499380
170.113619	119.063052	50.504385
166.914472	121.443092	50.509389
163.093232	123.305437	50.514394
159.405186	122.963495	50.519399
156.005500	122.049103	50.524404
152.566307	126.389778	50.529409
148.936671	135.946740	50.534413
145.662644	119.141775	50.539418
141.634790	134.714758	50.544423
138.617813	106.124243	50.549428
134.840607	133.556332	50.554433
131.251377	123.085431	50.559437
128.157662	129.958427	50.564442
124.400955	129.078582	50.569447
120.916297	136.580745	50.574452
117.071446	135.156928	50.579457
114.050689	135.346151	50.584461
110.473403	130.470939	50.589466
107.131419	138.918349	50.594471
103.650583	125.011813	50.599476
100.025871	138.118700	50.604481
96.952937	118.200075	50.609485
92.871512	130.813533	50.614490
89.465376	135.926417	50.619495
86.013100	140.377704	50.624500
82.014361	141.787537	50.629505
78.735007	141.725935	50.634509
75.570569	125.452862	50.639514
72.355256	120.480472	50.644519
68.831548	141.436333	50.649524
64.834366	122.075410	50.654529
61.242623	131.082404	50.659533
57.660877	128.256376	50.664538
54.081667	126.815237	50.669543
51.014517	123.697704	50.674548
47.453865	123.765668	50.679553
44.125155	137.312065	50.684557
40.453579	130.147089	50.689562
36.806264	125.987050	50.694567
33.128426	131.107770	50.699572
29.611331	136.400013	50.704577
26.474533	128.230728	50.709581
22.970088	121.277466	50.714586
19.633884	134.117906	50.719591
16.081418	123.419545	50.724596
12.324436	142.052262	50.729601
8.713159	131.194735	50.734605
5.500891	133.756561	50.739610
1.734505	129.595013	50.744615