Wed Jun 15 15:56:06 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.218113	94.574937	0.000000
0.886583	111.636198	0.005005
0.703054	91.138886	0.010010
0.422586	84.858433	0.015014
0.284171	83.274662	0.020019
0.456223	82.472657	0.025024
0.144891	88.112967	0.030029
0.314134	76.862252	0.035034
-0.429944	60.172956	0.040038
-0.203606	51.279434	0.045043
-0.783899	37.050868	0.050048
-1.075102	39.366600	0.055053
-1.093764	27.042034	0.060058
-1.495358	29.434800	0.065062
-1.586709	8.331474	0.070067
-1.845335	27.780365	0.075072
-2.493478	16.628868	0.080077
-3.086886	7.898588	0.085082
-3.851680	21.981400	0.090086
-3.851490	28.722890	0.095091
-3.709916	18.472036	0.100096
-3.881080	14.090250	0.105101
-3.562310	27.847606	0.110106
-4.362746	23.055370	0.115110
-4.823373	19.648500	0.120115
-4.864977	15.232281	0.125120
-5.026871	7.675312	0.130125
-5.138104	9.027806	0.135130
-5.649533	12.272974	0.140134
-6.317840	11.558358	0.145139
-6.764618	4.755962	0.150144
-6.919361	28.561766	0.155149
-6.952676	18.620661	0.160154
-7.479183	24.262080	0.165158
-6.989354	12.491045	0.170163
-7.270958	25.213478	0.175168
-7.028684	17.413627	0.180173
-7.006660	19.519856	0.185178
-8.150276	28.720327	0.190182
-8.011655	10.792110	0.195187
-8.655100	15.574503	0.200192
-9.713981	-0.030167	0.205197
-9.503030	1.265925	0.210202
-9.964361	15.889177	0.215206
-9.798547	5.342924	0.220211
-9.838893	4.137936	0.225216
-10.334632	10.483434	0.230221
-9.916133	8.963989	0.235226
-10.195507	20.232297	0.240230
-10.638959	19.275435	0.245235
-11.454453	36.710459	0.250240
-11.778195	12.601893	0.255245
-11.532138	10.248086	0.260250
-11.422861	23.991918	0.265254
-11.865737	7.463714	0.270259
-12.538442	16.965552	0.275264
-12.685758	5.232838	0.280269
-12.841100	7.896530	0.285274
-13.218354	17.885291	0.290278
-13.447271	-1.900352	0.295283
-13.870196	13.679733	0.300288
-14.085993	28.994672	0.305293
-14.252561	13.830162	0.310298
-14.780576	33.298127	0.315302
-14.617741	11.917322	0.320307
-14.463722	19.235721	0.325312
-15.192570	4.504869	0.330317
-15.310139	7.475717	0.335322
-15.951984	23.619947	0.340326
-16.185299	21.371798	0.345331
-16.034145	18.964818	0.350336
-16.464904	27.247754	0.355341
-16.321252	17.030197	0.360346
-17.426438	31.064706	0.365350
-17.439723	4.522631	0.370355
-17.661574	17.830217	0.375360
-17.720369	23.486180	0.380365
-17.536168	17.993305	0.385370
-17.994617	15.496190	0.390374
-18.538138	15.324914	0.395379
-19.203641	0.211109	0.400384
-19.329509	7.131157	0.405389
-19.118760	4.559654	0.410394
-19.283567	1.758913	0.415398
-19.432189	11.190709	0.420403
-19.480845	18.106387	0.425408
-20.321668	17.729341	0.430413
-20.727870	11.831633	0.435418
-20.902160	29.793697	0.440422
-20.821240	17.772989	0.445427
-21.023528	22.540876	0.450432
-21.424195	14.973055	0.455437
-21.880282	21.379381	0.460442
-22.621887	18.673270	0.465446
-22.695246	24.664967	0.470451
-22.947857	22.582182	0.475456
-22.704002	21.302011	0.480461
-22.637081	15.788764	0.485466
-22.985161	25.393807	0.490470
-22.939779	23.109662	0.495475
-23.553508	24.185438	0.500480
-24.173647	11.963347	0.505485
-24.081156	23.958287	0.510490
-24.257778	16.693178	0.515494
-24.476504	15.050577	0.520499
-25.339400	14.275788	0.525504
-25.771592	13.577394	0.530509
-25.337154	12.142715	0.535514
-25.709245	22.340446	0.540518
-25.822128	15.346144	0.545523
-25.632646	2.796419	0.550528
-26.684653	20.406841	0.555533
-27.175434	-7.213519	0.560538
-27.889914	17.415835	0.565542
-27.501983	-5.930483	0.570547
-27.230177	5.402977	0.575552
-27.480422	27.872808	0.580557
-27.232443	1.158535	0.585562
-28.076030	13.977186	0.590566
-28.490881	5.872316	0.595571
-28.685672	25.183198	0.600576
-29.074095	24.980471	0.605581
-29.057935	11.677610	0.610586
-29.254890	10.298547	0.615590
-30.121485	14.206820	0.620595
-30.762837	21.058768	0.625600
-31.080182	7.771372	0.630605
-30.348048	17.410175	0.635610
-30.560480	17.111184	0.640614
-30.690465	0.557720	0.645619
-30.973303	20.640258	0.650624
-31.043314	18.049059	0.655629
-31.647997	-0.930291	0.660634
-32.304749	16.480547	0.665638
-32.206312	12.109944	0.670643
-32.565396	11.250414	0.675648
-32.704230	-0.841781	0.680653
-32.591228	19.380324	0.685658
-33.230756	19.328790	0.690662
-33.750946	19.358055	0.695667
-33.870800	18.460369	0.700672
-34.160169	33.744558	0.705677
-33.863125	20.885839	0.710682
-34.344067	35.597973	0.715686
-34.958975	9.758645	0.720691
-35.172943	34.806235	0.725696
-35.533343	19.971373	0.730701
-35.377916	20.653492	0.735706
-35.602678	21.466904	0.740710
-35.729093	29.553941	0.745715
-36.603237	20.980934	0.750720
-37.105000	15.478612	0.755725
-36.754468	7.539145	0.760730
-37.313691	11.116267	0.765734
-37.219856	11.157893	0.770739
-37.087090	12.614580	0.775744
-37.374009	30.587758	0.780749
-38.074866	8.432585	0.785754
-38.831651	21.485683	0.790758
-38.700081	23.795071	0.795763
-38.816594	9.211514	0.800768
-39.180433	18.135733	0.805773
-38.583750	22.660206	0.810778
-38.902609	31.184189	0.815782
-39.677216	25.545150	0.820787
-39.738558	17.813431	0.825792
-40.080876	33.761776	0.830797
-40.194926	21.838791	0.835802
-41.445927	14.157786	0.840806
-41.871665	5.022876	0.845811
-41.428255	28.921291	0.850816
-41.615431	16.262162	0.855821
-41.748042	20.000206	0.860826
-42.258101	15.266922	0.865830
-42.063187	34.726978	0.870835
-41.753694	25.036700	0.875840
-42.719302	14.157761	0.880845
-43.243809	8.309105	0.885850
-43.470762	4.789540	0.890854
-43.486017	33.331978	0.895859
-43.360861	15.951502	0.900864
-44.012562	29.611968	0.905869
-44.315045	17.494622	0.910874
-44.705171	14.813488	0.915878
-44.857481	11.971420	0.920883
-45.014381	18.639134	0.925888
-45.308257	12.979050	0.930893
-45.122449	19.385927	0.935898
-45.697036	19.761159	0.940902
-46.293428	4.919544	0.945907
-46.449046	15.720328	0.950912
-46.994620	13.047030	0.955917
-46.531073	12.164694	0.960922
-46.784581	11.497044	0.965926
-47.203248	8.606171	0.970931
-47.816009	11.224223	0.975936
-48.068037	18.861865	0.980941
-48.192797	10.074362	0.985946
-48.197073	14.312541	0.990950
-48.575809	11.963246	0.995955
-48.352896	16.154508	1.000960
-49.061851	16.246439	1.005965
-49.470229	-0.307277	1.010970
-49.862630	15.815446	1.015974
-50.056717	16.200300	1.020979
-50.200620	11.811448	1.025984
-50.432277	16.073001	1.030989
-50.389947	9.134633	1.035994
-50.115800	24.214603	1.040998
-50.938227	15.051929	1.046003
-51.325658	15.021375	1.051008
-51.874632	11.772347	1.056013
-51.568354	16.194276	1.061018
-51.839761	23.162847	1.066022
-52.161740	17.598063	1.071027
-52.963093	13.909548	1.076032
-53.508454	23.409186	1.081037
-53.078948	0.578719	1.086042
-53.972860	17.620750	1.091046
-53.713495	4.599292	1.096051
-53.594761	10.999494	1.101056
-53.662424	17.008001	1.106061
-53.527740	7.549935	1.111066
-54.542759	13.161307	1.116070
-54.701412	11.314644	1.121075
-55.000341	19.725730	1.126080
-55.432691	10.116634	1.131085
-55.389469	19.721713	1.136090
-55.940595	21.351206	1.141094
-56.335625	32.852499	1.146099
-56.536626	26.147291	1.151104
-56.869550	26.954411	1.156109
-56.749717	28.810190	1.161114
-56.680536	22.090813	1.166118
-56.989067	26.203195	1.171123
-57.561863	18.812387	1.176128
-58.197415	15.117581	1.181133
-58.161912	23.633994	1.186138
-58.643976	14.266509	1.191142
-58.806132	12.940095	1.196147
-58.441662	6.503670	1.201152
-58.720220	-0.280449	1.206157
-59.373375	11.838004	1.211162
-59.922309	5.691925	1.216166
-59.860409	6.487554	1.221171
-59.774946	0.659429	1.226176
-60.079788	18.365162	1.231181
-60.050807	4.488734	1.236186
-61.277727	12.311660	1.241190
-61.703516	12.279357	1.246195
-61.684703	9.972970	1.251200
-61.681756	21.801291	1.256205
-61.717683	29.898724	1.261210
-61.718698	22.166899	1.266214
-62.106741	38.439755	1.271219
-62.636298	2.628469	1.276224
-63.077748	21.536493	1.281229
-62.907165	13.596579	1.286234
-63.079313	23.581629	1.291238
-63.528893	23.492886	1.296243
-63.380089	19.472932	1.301248
-64.574199	22.995178	1.306253
-64.687403	11.736054	1.311258
-65.054276	18.311017	1.316262
-65.209441	16.308311	1.321267
-65.147368	25.146656	1.326272
-64.952723	25.162052	1.331277
-64.871124	15.918038	1.336282
-65.295653	16.547247	1.341286
-66.183812	25.609124	1.346291
-66.122984	9.172881	1.351296
-66.081794	36.868976	1.356301
-66.794614	17.050248	1.361306
-67.777052	16.233371	1.366310
-68.046264	22.152769	1.371315
-67.871416	13.813717	1.376320
-68.183953	11.884568	1.381325
-68.194645	23.288202	1.386330
-68.229830	25.471063	1.391334
-67.849505	17.667733	1.396339
-67.924822	12.595272	1.401344
-69.078486	21.986510	1.406349
-69.256915	-0.679851	1.411354
-69.743793	22.858150	1.416358
-69.568866	22.065339	1.421363
-70.404810	15.955446	1.426368
-70.808017	26.795675	1.431373
-71.096053	28.651881	1.436378
-71.240363	12.126526	1.441382
-71.131214	33.989669	1.446387
-71.083815	27.672028	1.451392
-71.558838	20.155959	1.456397
-71.117651	17.264437	1.461402
-72.111339	36.726202	1.466406
-72.650717	18.722118	1.471411
-72.863353	36.706598	1.476416
-72.836140	17.519028	1.481421
-72.606492	22.639609	1.486426
-72.984892	30.410302	1.491430
-73.972279	34.911190	1.496435
-74.332669	16.675500	1.501440
-74.856465	27.794507	1.506445
-74.603358	10.147167	1.511450
-74.701245	30.969474	1.516454
-74.955799	18.530910	1.521459
-74.736404	29.276232	1.526464
-74.702526	16.924061	1.531469
-75.220419	22.294851	1.536474
-75.855059	9.652273	1.541478
-76.161158	22.274970	1.546483
-76.160827	3.876494	1.551488
-76.316473	23.385883	1.556493
-77.172497	20.272735	1.561498
-77.710867	18.019864	1.566502
-77.801214	9.207047	1.571507
-77.827251	11.270216	1.576512
-77.908904	18.680630	1.581517
-77.853336	13.083144	1.586522
-78.273001	15.338130	1.591526
-78.164824	25.885302	1.596531
-78.535625	16.729967	1.601536
-79.470606	28.783738	1.606541
-79.448573	2.426927	1.611546
-79.554187	20.581619	1.616550
-79.399757	0.667132	1.621555
-80.206636	18.328482	1.626560
-80.781653	17.619467	1.631565
-80.904954	13.688582	1.636570
-81.269600	19.818184	1.641574
-81.104118	24.692593	1.646579
-80.992986	28.841859	1.651584
-81.118912	19.304242	1.656589
-81.738166	29.391599	1.661594
-82.202437	26.397680	1.666598
-82.793092	25.749944	1.671603
-82.530126	24.139600	1.676608
-82.941398	18.488760	1.681613
-82.634567	13.359356	1.686618
-83.316063	4.656574	1.691622
-83.804295	22.638444	1.696627
-83.698778	5.578281	1.701632
-84.259077	20.608231	1.706637
-84.207086	5.731871	1.711642
-84.545629	22.803849	1.716646
-85.153475	14.347836	1.721651
-85.278307	11.464730	1.726656
-85.900402	22.046079	1.731661
-85.789090	24.639463	1.736666
-85.829611	33.953670	1.741670
-86.145538	23.473121	1.746675
-85.810446	10.022366	1.751680
-86.635504	17.253489	1.756685
-87.188469	13.198296	1.761690
-87.505339	14.694571	1.766694
-87.828294	10.394108	1.771699
-87.685611	23.283949	1.776704
-87.585991	9.725621	1.781709
-87.632736	18.885282	1.786714
-88.056727	16.229971	1.791718
-89.033293	20.443783	1.796723
-89.328478	18.162460	1.801728
-89.444448	27.096224	1.806733
-89.097317	3.381001	1.811738
-89.117084	7.448908	1.816742
-89.463559	28.886317	1.821747
-90.066565	9.290451	1.826752
-90.724936	26.299085	1.831757
-90.923729	8.646435	1.836762
-90.883531	15.468504	1.841766
-91.075893	10.437289	1.846771
-91.187445	14.275330	1.851776
-91.708602	17.002147	1.856781
-92.081703	16.168612	1.861786
-92.030734	29.993888	1.866790
-92.710489	22.227063	1.871795
-92.359671	14.959724	1.876800
-92.621447	19.896164	1.881805
-93.214378	14.445318	1.886810
-93.841222	16.611731	1.891814
-94.036826	20.968834	1.896819
-94.047309	18.958197	1.901824
-93.983210	16.722947	1.906829
-93.814903	15.699411	1.911834
-94.363869	22.555132	1.916838
-95.064437	23.013436	1.921843
-95.259779	17.392115	1.926848
-95.424254	35.608143	1.931853
-95.411540	32.954441	1.936858
-95.481262	15.909520	1.941862
-96.373943	31.106969	1.946867
-96.760555	17.535185	1.951872
-97.445069	27.870275	1.956877
-97.043549	16.928262	1.961882
-97.168159	26.181784	1.966886
-97.338288	18.463611	1.971891
-97.213049	14.640111	1.976896
-97.544110	16.581161	1.981901
-98.182966	21.317622	1.986906
-98.614380	16.531790	1.991910
-99.241574	16.063910	1.996915
-99.045223	17.637815	2.006912
-98.336729	15.435463	2.016909
-97.930105	17.016708	2.026906
-97.909668	14.182045	2.036902
-97.423538	10.780403	2.046899
-96.565356	16.267457	2.056896
-96.183825	8.212539	2.066893
-95.461311	19.332896	2.076890
-94.624105	25.266614	2.086886
-94.535234	24.308778	2.096883
-94.185212	22.414677	2.106880
-93.876217	6.229816	2.116877
-93.007468	13.006081	2.126874
-92.667416	21.744436	2.136870
-92.433209	23.228836	2.146867
-91.776140	22.849833	2.156864
-91.242326	8.967046	2.166861
-90.042273	10.594060	2.176858
-89.869151	20.822827	2.186854
-89.753798	10.774614	2.196851
-89.623239	14.795637	2.206848
-88.636352	17.915966	2.216845
-88.214591	27.308030	2.226842
-87.257449	11.207265	2.236838
-86.912535	16.115497	2.246835
-86.641941	11.745848	2.256832
-86.466789	16.986259	2.266829
-85.334667	8.021847	2.276826
-85.347474	3.092675	2.286822
-84.623481	20.360004	2.296819
-83.951852	15.241358	2.306816
-83.841405	15.190443	2.316813
-82.858747	13.892184	2.326810
-82.555526	15.761750	2.336806
-82.045877	17.421582	2.346803
-81.802444	20.305252	2.356800
-80.856841	13.423865	2.366797
-80.515703	17.353885	2.376794
-80.247330	25.642427	2.386790
-79.400276	25.725593	2.396787
-78.617622	21.017368	2.406784
-78.788980	12.853908	2.416781
-78.397534	14.148951	2.426778
-77.554832	20.839744	2.436774
-77.334587	21.755052	2.446771
-76.236211	24.022230	2.456768
-76.020228	26.279281	2.466765
-75.657193	24.241587	2.476762
-75.036181	16.204867	2.486758
-74.136259	24.205314	2.496755
-73.930514	13.503691	2.506752
-73.730037	13.664976	2.516749
-73.431990	15.720498	2.526746
-72.552375	26.667039	2.536742
-72.155420	19.637395	2.546739
-71.236964	16.855514	2.556736
-70.988920	13.735017	2.566733
-70.616148	13.278054	2.576730
-70.109628	23.250525	2.586726
-69.367555	24.421739	2.596723
-69.321625	16.237478	2.606720
-68.782573	26.196672	2.616717
-67.519139	20.976068	2.626714
-67.726926	20.638859	2.636710
-67.370923	15.844100	2.646707
-66.744119	5.796601	2.656704
-66.152925	17.710082	2.666701
-65.198055	20.274579	2.676698
-65.185917	15.940829	2.686694
-64.772394	14.227064	2.696691
-63.569433	20.369395	2.706688
-63.052777	12.777511	2.716685
-63.221924	15.317190	2.726682
-63.008752	19.618807	2.736678
-61.892600	22.286733	2.746675
-61.729936	16.090241	2.756672
-61.207718	7.758916	2.766669
-60.199508	15.614247	2.776666
-60.168441	16.834717	2.786662
-59.648682	25.354427	2.796659
-58.471856	11.956323	2.806656
-58.421500	24.586303	2.816653
-58.141192	15.804646	2.826650
-57.882809	18.165512	2.836646
-56.763457	25.635836	2.846643
-56.765122	10.218311	2.856640
-55.828081	8.519763	2.866637
-55.108185	22.907768	2.876634
-55.164609	20.706888	2.886630
-54.953655	22.943633	2.896627
-53.870118	17.515215	2.906624
-53.520627	12.711064	2.916621
-53.139142	3.907457	2.926618
-52.199293	15.582465	2.936614
-52.107918	20.140081	2.946611
-51.610744	33.158777	2.956608
-50.730490	6.512600	2.966605
-50.243130	17.448901	2.976602
-50.347964	17.877747	2.986598
-49.906946	24.475315	2.996595
-48.655932	12.045567	3.006592
-48.365469	21.178522	3.016589
-47.959388	22.161892	3.026586
-46.918310	17.775433	3.036582
-47.023919	5.296591	3.046579
-46.984160	12.870364	3.056576
-46.343669	21.872281	3.066573
-45.577512	17.746977	3.076570
-44.620227	28.026123	3.086566
-44.252267	25.025668	3.096563
-44.087801	23.803172	3.106560
-43.846297	21.370226	3.116557
-42.642963	22.371280	3.126554
-42.181928	17.870395	3.136550
-42.036001	21.700030	3.146547
-41.800684	7.207067	3.156544
-40.911344	10.387972	3.166541
-40.809573	12.324417	3.176538
-40.105313	13.700021	3.186534
-39.387503	17.271575	3.196531
-39.076956	21.278562	3.206528
-38.049103	19.410328	3.216525
-37.783888	9.225928	3.226522
-37.389545	19.712879	3.236518
-37.422355	14.041765	3.246515
-36.193754	19.707929	3.256512
-35.994838	14.299282	3.266509
-35.659530	8.958374	3.276506
-34.617496	11.876102	3.286502
-34.464118	19.146241	3.296499
-34.264780	17.581760	3.306496
-33.314610	13.936702	3.316493
-32.581513	12.629221	3.326490
-32.804216	8.906078	3.336486
-32.155458	11.864404	3.346483
-31.105078	8.569036	3.356480
-31.047409	6.932752	3.366477
-30.580775	17.036271	3.376474
-29.511811	18.558830	3.386470
-29.340691	16.555029	3.396467
-29.428715	12.935859	3.406464
-28.322331	16.337114	3.416461
-27.430674	18.672540	3.426458
-27.536778	15.884567	3.436454
-27.318292	17.640033	3.446451
-26.385141	19.198372	3.456448
-26.035927	15.537462	3.466445
-25.644068	24.390337	3.476442
-24.645806	13.395156	3.486438
-24.484266	18.873592	3.496435
-23.986828	13.373237	3.506432
-23.053885	19.115131	3.516429
-22.718984	22.429649	3.526426
-22.798137	22.644161	3.536422
-22.013800	24.095036	3.546419
-21.262597	11.748779	3.556416
-21.151918	11.726372	3.566413
-19.953161	9.022628	3.576410
-19.749966	10.279053	3.586406
-19.333813	6.346322	3.596403
-19.393555	18.432975	3.606400
-18.583683	12.582396	3.616397
-18.003252	13.855298	3.626394
-17.177733	18.551658	3.636390
-16.506905	17.283804	3.646387
-16.155645	23.353059	3.656384
-16.121149	10.428504	3.666381
-16.078126	12.427699	3.676378
-15.014507	17.705497	3.686374
-14.489159	17.325454	3.696371
-13.588637	21.061498	3.706368
-13.220521	24.644227	3.716365
-13.244746	13.638356	3.726362
-12.583110	15.439904	3.736358
-12.153964	15.849842	3.746355
-10.958317	14.752855	3.756352
-10.682285	4.881951	3.766349
-10.503529	8.938868	3.776346
-10.037192	21.178403	3.786342
-9.567231	18.326933	3.796339
-8.919389	12.563976	3.806336
-8.394368	16.868089	3.816333
-7.270362	13.297721	3.826330
-7.237676	19.120539	3.836326
-6.704300	20.374551	3.846323
-6.726701	20.366038	3.856320
-6.087787	21.745434	3.866317
-5.088585	18.459710	3.876314
-4.958451	19.701937	3.886310
-4.811359	21.813821	3.896307
-3.933500	21.556869	3.906304
-3.693716	17.334444	3.916301
-2.750707	31.356094	3.926298
-2.517192	44.317042	3.936294
-2.668761	50.537363	3.946291
-1.959262	73.339944	3.956288
-1.279775	87.528662	3.966285
-0.800652	98.676482	3.976282
-0.207554	125.019895	3.986278
0.000000	136.649950	3.991283
0.254344	131.353193	3.996288
0.408671	158.362101	4.001293
0.532005	164.883935	4.006298
0.844626	174.858917	4.011302
0.657845	158.652332	4.016307
0.734710	177.723196	4.021312
0.840018	166.483079	4.026317
0.611833	185.519233	4.031322
0.928768	161.468305	4.036326
0.741027	182.198945	4.041331
0.272397	168.844662	4.046336
0.609811	173.859990	4.051341
0.615836	166.006377	4.056346
1.225075	187.833181	4.061350
1.260540	181.404888	4.066355
1.116979	175.152378	4.071360
0.817289	165.073490	4.076365
0.767747	165.331371	4.081370
1.109282	174.973375	4.086374
1.108247	173.340750	4.091379
1.051817	182.755246	4.096384
0.954873	162.132651	4.101389
0.974021	180.106923	4.106394
1.373726	193.355152	4.111398
1.192288	180.559882	4.116403
1.271098	184.216466	4.121408
1.208249	169.155206	4.126413
0.797503	173.265480	4.131418
1.199857	169.713098	4.136422
1.048568	182.522638	4.141427
1.268349	181.646942	4.146432
1.181522	187.249989	4.151437
1.083575	178.057444	4.156442
1.443514	194.338062	4.161446
1.030269	175.702299	4.166451
1.426513	192.596717	4.171456
1.142002	174.862628	4.176461
1.015819	192.148696	4.181466
1.400671	185.705869	4.186470
1.424349	207.045378	4.191475
1.366115	199.054987	4.196480
1.554849	172.656402	4.201485
1.216636	179.070046	4.206490
1.681235	161.444884	4.211494
1.117193	180.129614	4.216499
1.177056	168.379403	4.221504
1.262299	182.108509	4.226509
1.231310	207.959033	4.231514
1.537361	204.236607	4.236518
1.295018	179.511881	4.241523
1.547540	193.919571	4.246528
1.289880	205.507004	4.251533
1.131160	197.290942	4.256538
1.622243	204.428939	4.261542
1.273381	209.074911	4.266547
1.484794	216.402763	4.271552
1.585946	208.904323	4.276557
1.278920	212.816447	4.281562
1.703618	211.533208	4.286566
1.574264	199.738679	4.291571
1.581269	202.226715	4.296576
1.387063	200.464820	4.301581
1.420228	213.183925	4.306586
1.685237	196.206185	4.311590
1.537262	213.902208	4.316595
1.487573	204.473796	4.321600
1.421307	211.849606	4.326605
1.489571	204.954506	4.331610
1.512817	219.914362	4.336614
1.634320	201.080992	4.341619
1.578134	216.839602	4.346624
1.999614	195.499547	4.351629
1.646806	179.271941	4.356634
1.321232	195.623923	4.361638
1.247435	200.026746	4.366643
1.359075	190.701007	4.371648
1.884310	225.053031	4.376653
1.865994	233.619598	4.381658
1.908055	226.786922	4.386662
1.610943	212.160898	4.391667
2.052863	224.422902	4.396672
2.007612	207.630879	4.401677
1.491739	202.238736	4.406682
1.965085	200.770878	4.411686
1.983554	204.109633	4.416691
2.068383	206.958585	4.421696
2.131837	190.407468	4.426701
1.816262	204.076170	4.431706
2.135484	208.208167	4.436710
1.986179	193.396840	4.441715
2.029491	199.053357	4.446720
2.080796	199.311343	4.451725
1.573536	198.132796	4.456730
1.921390	196.284182	4.461734
2.015313	203.254412	4.466739
1.874911	195.412256	4.471744
1.661669	203.312988	4.476749
1.497133	226.923129	4.481754
2.529055	210.575558	4.486758
2.437670	223.085208	4.491763
2.234090	212.509595	4.496768
2.280474	221.502570	4.501773
1.878605	209.601941	4.506778
2.046890	212.589118	4.511782
1.565825	205.604867	4.516787
1.874861	203.752802	4.521792
2.366083	210.364987	4.526797
2.245167	220.308360	4.531802
2.334919	211.542008	4.536806
2.055613	217.884870	4.541811
2.106508	205.659545	4.546816
2.052668	202.199317	4.551821
1.663716	207.170546	4.556826
1.840107	220.571615	4.561830
2.030444	237.137778	4.566835
2.440605	230.391451	4.571840
2.396216	232.111726	4.576845
2.360420	231.040819	4.581850
2.463209	226.497096	4.586854
2.522082	241.821508	4.591859
2.371614	240.279764	4.596864
2.744077	243.981845	4.601869
2.281104	237.712647	4.606874
2.291728	212.981179	4.611878
2.246515	223.941039	4.616883
2.313591	237.386034	4.621888
2.379044	236.985181	4.626893
2.193298	253.093046	4.631898
2.626640	231.044957	4.636902
2.725605	249.556674	4.641907
2.534984	226.058397	4.646912
2.078160	218.784844	4.651917
2.258455	217.001798	4.656922
2.719219	232.042069	4.661926
2.388307	223.872994	4.666931
2.348145	239.328004	4.671936
2.590536	232.007059	4.676941
2.462038	236.815102	4.681946
2.581587	230.852321	4.686950
2.616856	243.899404	4.691955
2.310686	246.512893	4.696960
2.578325	229.068273	4.701965
2.303709	236.935267	4.706970
2.372117	234.936717	4.711974
2.521826	230.906298	4.716979
2.535492	233.210740	4.721984
2.784749	248.732658	4.726989
2.317170	251.680801	4.731994
2.759032	224.395375	4.736998
2.735666	242.531820	4.742003
2.672498	234.345226	4.747008
2.745584	229.093582	4.752013
2.763268	241.293718	4.757018
2.628834	227.605276	4.762022
2.537942	244.482693	4.767027
2.231070	231.216252	4.772032
2.474753	239.519736	4.777037
2.441754	244.121412	4.782042
2.558503	236.965549	4.787046
2.557481	261.205321	4.792051
2.606560	253.329849	4.797056
2.794017	256.358555	4.802061
2.511015	264.785296	4.807066
2.667615	260.863131	4.812070
2.687914	262.389431	4.817075
2.905195	257.950581	4.822080
2.959573	264.421902	4.827085
2.590440	259.500899	4.832090
2.518922	262.687329	4.837094
2.576397	262.227519	4.842099
2.777957	260.511094	4.847104
3.013968	264.456504	4.852109
2.704109	268.182370	4.857114
2.856641	270.743536	4.862118
3.150505	287.727190	4.867123
2.982508	287.810411	4.872128
2.968055	277.097155	4.877133
2.915263	277.164790	4.882138
3.121235	283.788634	4.887142
3.065943	286.363925	4.892147
3.494821	280.352471	4.897152
3.334753	273.535619	4.902157
2.985689	283.597135	4.907162
2.998735	258.071570	4.912166
3.156799	279.743217	4.917171
2.669746	252.098085	4.922176
2.954222	272.117883	4.927181
2.732918	292.551863	4.932186
3.292571	294.579739	4.937190
3.184802	294.511248	4.942195
3.107682	301.390919	4.947200
3.764374	292.889612	4.952205
3.211705	304.882388	4.957210
2.999489	277.021624	4.962214
3.296210	271.775722	4.967219
3.335620	287.819976	4.972224
3.621372	269.146614	4.977229
2.930411	275.858308	4.982234
3.324406	270.913386	4.987238
3.356554	262.477624	4.992243
3.141229	271.294189	4.997248
3.414871	264.573960	5.002253
3.366309	297.870639	5.007258
3.360152	278.425245	5.012262
3.299598	279.383772	5.017267
3.389704	292.138516	5.022272
3.671363	271.354163	5.027277
3.243118	277.995905	5.032282
3.296582	261.558426	5.037286
3.479311	282.939725	5.042291
3.430277	285.624468	5.047296
3.555495	286.097132	5.052301
3.275420	279.538542	5.057306
3.688988	281.700057	5.062310
3.400023	284.134129	5.067315
2.871617	306.677371	5.072320
3.614034	288.163892	5.077325
3.318895	306.666525	5.082330
3.339837	289.956005	5.087334
3.748908	305.004594	5.092339
3.414571	303.621275	5.097344
3.483579	286.328189	5.102349
3.292779	300.500672	5.107354
3.305251	297.262470	5.112358
3.302961	297.211766	5.117363
3.302648	298.319853	5.122368
3.432439	307.847087	5.127373
2.875808	304.428296	5.132378
3.342161	315.159062	5.137382
3.806340	311.602942	5.142387
3.809467	313.254408	5.147392
4.127674	330.437598	5.152397
3.676382	330.120956	5.157402
3.865971	326.404825	5.162406
3.803107	325.748663	5.167411
3.507720	321.610756	5.172416
3.722835	332.922760	5.177421
3.751319	326.203165	5.182426
3.843652	335.264573	5.187430
3.817602	326.140455	5.192435
3.696348	327.003857	5.197440
4.196902	312.130397	5.202445
3.660620	332.538749	5.207450
3.953190	319.518930	5.212454
3.842824	331.376582	5.217459
3.869137	325.389121	5.222464
3.873859	323.983702	5.227469
4.065893	330.628218	5.232474
3.909779	315.261619	5.237478
3.918107	315.425496	5.242483
3.718773	314.079055	5.247488
3.725408	333.111013	5.252493
3.672952	324.357148	5.257498
3.879542	326.209578	5.262502
3.643337	337.571310	5.267507
4.220508	315.299469	5.272512
4.051335	316.202455	5.277517
4.014936	337.143571	5.282522
4.208376	310.651241	5.287526
4.313069	329.436449	5.292531
4.248527	320.452660	5.297536
4.505832	334.013486	5.302541
3.970780	337.852544	5.307546
3.963542	321.323227	5.312550
3.847712	331.869561	5.317555
3.893866	343.449210	5.322560
4.227102	323.158385	5.327565
3.885638	333.211476	5.332570
4.311084	319.615589	5.337574
4.239508	331.518918	5.342579
4.133949	323.626152	5.347584
4.212522	313.898878	5.352589
4.158860	308.249884	5.357594
4.200586	318.548114	5.362598
4.137697	343.183758	5.367603
4.361974	328.786541	5.372608
4.516382	348.647802	5.377613
4.353436	340.435222	5.382618
4.178124	334.657560	5.387622
4.425571	337.580580	5.392627
4.182645	338.026781	5.397632
4.465915	327.270307	5.402637
4.103051	337.461001	5.407642
3.943515	322.484227	5.412646
4.236065	341.781662	5.417651
4.152058	327.446245	5.422656
4.357082	323.041957	5.427661
4.029352	340.415559	5.432666
4.131643	314.889553	5.437670
4.071007	330.037591	5.442675
4.179171	348.038881	5.447680
4.644924	350.413347	5.452685
4.278204	363.567509	5.457690
4.689766	363.017514	5.462694
4.383631	366.851302	5.467699
4.537430	361.422517	5.472704
4.825451	363.287044	5.477709
4.492851	355.432966	5.482714
4.610373	336.878672	5.487718
4.516484	336.239376	5.492723
4.274258	341.378666	5.497728
4.620005	351.361706	5.502733
4.268447	348.895896	5.507738
4.363313	354.120156	5.512742
4.870290	373.951398	5.517747
4.565845	367.551184	5.522752
4.656196	362.355436	5.527757
4.582628	368.006274	5.532762
4.536170	366.468044	5.537766
4.813070	364.085115	5.542771
4.489978	366.439114	5.547776
4.872020	354.355453	5.552781
4.800731	366.783178	5.557786
4.772411	355.343047	5.562790
4.753784	370.135460	5.567795
4.575978	366.857366	5.572800
4.622686	375.360982	5.577805
4.748995	355.641156	5.582810
4.796846	349.306138	5.587814
4.899442	357.202993	5.592819
4.868039	353.632383	5.597824
5.119893	359.150323	5.602829
5.305044	356.406706	5.607834
4.936825	358.723079	5.612838
4.652226	333.762508	5.617843
4.790151	356.220664	5.622848
4.983622	369.001697	5.627853
4.740906	368.170067	5.632858
4.905337	371.885250	5.637862
5.037904	357.388631	5.642867
4.758447	370.349429	5.647872
4.973952	360.613801	5.652877
4.711203	372.872322	5.657882
4.794056	365.611218	5.662886
4.877350	365.992756	5.667891
4.764581	388.204038	5.672896
4.890000	368.553792	5.677901
4.791863	375.308134	5.682906
4.945951	374.876056	5.687910
4.625240	363.391904	5.692915
4.442561	376.127283	5.697920
4.954624	362.680110	5.702925
5.313377	398.030641	5.707930
5.130375	385.681253	5.712934
5.068236	372.737765	5.717939
4.738449	371.488935	5.722944
5.126221	378.855689	5.727949
5.189628	373.245625	5.732954
5.419563	387.360792	5.737958
5.533179	386.233812	5.742963
5.063805	369.514463	5.747968
5.105983	363.463006	5.752973
4.907482	358.613505	5.757978
5.044380	374.956825	5.762982
5.256252	384.472021	5.767987
4.972977	379.880680	5.772992
5.188170	386.601792	5.777997
4.871729	382.712983	5.783002
5.173239	399.624569	5.788006
5.265922	392.813246	5.793011
5.107678	404.009139	5.798016
5.263766	388.717932	5.803021
5.223833	393.915849	5.808026
5.165038	394.125445	5.813030
5.452404	405.936367	5.818035
5.264744	388.497162	5.823040
5.618633	397.972423	5.828045
5.293256	387.164375	5.833050
5.115936	393.377503	5.838054
5.629622	383.226694	5.843059
5.246722	402.993433	5.848064
5.624622	379.924298	5.853069
5.296397	392.291417	5.858074
5.529441	374.843963	5.863078
5.378402	393.342420	5.868083
5.415833	386.812600	5.873088
5.810851	368.816336	5.878093
5.484516	381.195957	5.883098
5.441834	377.132778	5.888102
5.345936	386.568720	5.893107
5.136694	393.837437	5.898112
5.553146	401.544240	5.903117
5.625452	424.009591	5.908122
5.770291	413.936389	5.913126
6.237547	420.751503	5.918131
5.759596	403.917917	5.923136
5.883747	381.394811	5.928141
5.476982	384.893650	5.933146
5.235816	383.949499	5.938150
5.408150	383.364361	5.943155
5.501355	388.867689	5.948160
5.862098	395.312112	5.953165
5.548507	411.398852	5.958170
5.938987	410.509041	5.963174
5.793714	413.239305	5.968179
5.796535	401.927958	5.973184
5.882020	401.867286	5.978189
5.557749	386.184811	5.983194
5.673959	400.947769	5.988198
5.858236	403.364617	5.993203
5.834146	409.491759	5.998208
5.948150	399.785210	6.003213
5.760810	397.204161	6.008218
6.100066	384.419840	6.013222
5.881353	386.217180	6.018227
5.669825	388.317269	6.023232
5.775034	398.650046	6.028237
5.615896	398.413265	6.033242
5.671976	379.930235	6.038246
5.704383	382.610808	6.043251
5.650964	405.363557	6.048256
6.158460	397.881132	6.053261
5.770667	398.845999	6.058266
5.671163	396.802375	6.063270
5.698900	378.747924	6.068275
5.684087	397.670554	6.073280
5.868752	401.097601	6.078285
6.038987	399.217253	6.083290
5.911597	391.475737	6.088294
5.422427	395.797215	6.093299
5.696144	403.993231	6.098304
6.052832	407.312439	6.103309
5.781903	402.873238	6.108314
5.528958	397.719808	6.113318
5.988990	401.414065	6.118323
5.718251	407.556418	6.123328
6.137796	413.775484	6.128333
5.855994	401.197366	6.133338
5.865284	384.559202	6.138342
6.083698	377.769526	6.143347
5.603276	382.263177	6.148352
5.711597	381.806700	6.153357
5.398876	387.626002	6.158362
5.311703	395.350133	6.163366
5.866022	399.716688	6.168371
5.568343	413.112024	6.173376
6.162842	417.978309	6.178381
6.005636	416.410334	6.183386
5.666039	420.753071	6.188390
6.134050	405.326349	6.193395
5.769527	408.433875	6.198400
5.794213	380.297211	6.203405
5.547166	378.673849	6.208410
5.555402	382.814277	6.213414
5.992161	395.557002	6.218419
6.263427	407.787772	6.223424
6.090141	382.314001	6.228429
6.105895	398.717911	6.233434
5.800934	393.098182	6.238438
5.685323	396.917755	6.243443
5.468405	386.088134	6.248448
5.703344	391.980787	6.253453
5.611448	394.074129	6.258458
5.631239	384.542380	6.263462
5.743119	389.242678	6.268467
5.614294	376.002522	6.273472
5.840809	383.791410	6.278477
5.948775	397.619057	6.283482
5.991412	398.544754	6.288486
5.937609	389.593085	6.293491
5.482100	400.134340	6.298496
5.774704	380.672885	6.303501
5.624532	405.212173	6.308506
5.775104	404.672655	6.313510
6.035604	410.838295	6.318515
5.530698	399.362458	6.323520
5.762096	383.449456	6.328525
5.557726	400.599129	6.333530
5.989682	408.790897	6.338534
6.155609	409.602207	6.343539
5.741794	400.766159	6.348544
6.285929	407.777303	6.353549
5.913692	380.377541	6.358554
5.927757	393.586883	6.363558
6.201469	373.340355	6.368563
5.653461	384.015855	6.373568
6.088950	386.536890	6.378573
5.644031	391.262321	6.383578
5.953350	380.039236	6.388582
6.179933	391.882092	6.393587
5.457347	373.611997	6.398592
6.108997	390.663402	6.403597
6.118397	378.654228	6.408602
6.232854	398.949207	6.413606
6.035512	372.842846	6.418611
5.873731	377.888357	6.423616
5.999103	357.032843	6.428621
5.360105	381.221089	6.433626
5.661092	377.187531	6.438630
5.876683	355.495956	6.443635
5.759862	369.140739	6.448640
5.570249	359.455290	6.453645
5.894433	372.703036	6.458650
5.873562	380.345274	6.463654
5.787878	375.903978	6.468659
5.673069	373.712841	6.473664
5.845305	395.334071	6.478669
5.721221	390.893296	6.483674
5.778532	396.438170	6.488678
5.919103	398.904955	6.493683
5.575625	385.153650	6.498688
5.922695	395.691203	6.503693
6.010297	388.267914	6.508698
5.620583	372.004671	6.513702
5.886848	369.754406	6.518707
5.578218	370.013182	6.523712
6.008200	381.835142	6.528717
5.653680	375.544117	6.533722
5.776482	380.957417	6.538726
5.914010	365.657857	6.543731
5.654758	371.659103	6.548736
5.651177	377.718721	6.553741
5.851871	393.941919	6.558746
5.792375	388.820250	6.563750
5.952754	394.840941	6.568755
5.610694	382.137550	6.573760
5.970503	389.356616	6.578765
5.801986	393.740029	6.583770
5.674914	365.056506	6.588774
5.798794	378.746949	6.593779
5.932267	380.779862	6.598784
5.780614	378.152077	6.603789
5.714144	358.344939	6.608794
5.590963	376.511356	6.613798
5.862240	376.896356	6.618803
5.921822	395.304764	6.623808
6.051245	374.702872	6.628813
5.838599	372.104306	6.633818
5.617145	366.228407	6.638822
5.652771	358.916218	6.643827
5.769077	379.608421	6.648832
5.677287	372.909274	6.653837
6.004573	395.840586	6.658842
6.000051	369.761455	6.663846
6.106907	365.132675	6.668851
5.805575	373.513675	6.673856
5.987839	358.521220	6.678861
5.781193	376.881860	6.683866
5.542813	370.438764	6.688870
5.922895	367.400525	6.693875
5.637295	374.003149	6.698880
5.980135	360.900902	6.703885
5.699495	367.980656	6.708890
5.701610	368.926662	6.713894
5.632129	351.762238	6.718899
5.532333	366.145746	6.723904
5.547274	362.044440	6.728909
5.886934	381.570502	6.733914
5.882793	386.242326	6.738918
5.489862	382.525969	6.743923
5.687638	395.498679	6.748928
6.133243	387.166663	6.753933
5.836155	391.674213	6.758938
5.843768	381.412996	6.763942
6.036017	379.104921	6.768947
5.981980	373.064132	6.773952
5.715575	363.690376	6.778957
5.955082	363.942122	6.783962
5.702727	362.369852	6.788966
6.039984	364.119504	6.793971
5.481966	363.431822	6.798976
5.774453	363.006271	6.803981
6.010639	361.896819	6.808986
5.413357	374.026251	6.813990
5.540243	363.662569	6.818995
5.542454	374.053191	6.824000
5.868417	390.038951	6.829005
6.116554	393.836687	6.834010
5.680954	381.886253	6.839014
6.121243	362.748152	6.844019
5.827429	379.877760	6.849024
5.891071	367.838322	6.854029
5.852727	385.653352	6.859034
5.671720	372.518596	6.864038
5.834402	378.563957	6.869043
5.709093	367.669787	6.874048
5.800253	381.067128	6.879053
5.703392	363.830565	6.884058
5.611310	374.197311	6.889062
5.603858	365.984669	6.894067
5.561281	367.834283	6.899072
6.080262	377.473923	6.904077
5.985030	386.858162	6.909082
5.479923	365.460678	6.914086
5.870031	380.157340	6.919091
5.570884	371.802804	6.924096
5.587135	378.821760	6.929101
5.759286	378.833083	6.934106
5.795604	395.088478	6.939110
6.103947	386.303067	6.944115
6.005340	381.941935	6.949120
6.020513	377.169577	6.954125
5.972741	365.792631	6.959130
5.988277	382.846458	6.964134
5.958664	368.890787	6.969139
5.588545	378.881563	6.974144
5.853752	382.709818	6.979149
5.684064	371.604274	6.984154
5.643515	373.259118	6.989158
5.525823	366.808114	6.994163
5.386962	372.290400	6.999168
6.009419	378.907113	7.004173
5.955960	371.672775	7.009178
5.500292	374.784604	7.014182
5.755100	386.055462	7.019187
5.769644	387.670128	7.024192
5.989066	386.065662	7.029197
5.935343	384.026904	7.034202
5.791359	371.377401	7.039206
5.572895	373.758206	7.044211
5.613965	382.813711	7.049216
5.883160	404.572724	7.054221
5.839579	392.281478	7.059226
5.805263	396.640346	7.064230
6.112966	388.505530	7.069235
5.575794	379.247834	7.074240
5.790653	379.123461	7.079245
5.618150	364.931173	7.084250
5.889669	387.645684	7.089254
6.120664	386.409338	7.094259
5.845628	382.758830	7.099264
6.277133	369.258968	7.104269
5.820477	377.063190	7.109274
5.633576	376.374945	7.114278
5.569216	364.558498	7.119283
5.451095	374.739352	7.124288
5.567933	378.960480	7.129293
5.798377	375.041373	7.134298
5.762612	396.620033	7.139302
5.883468	383.243708	7.144307
5.519094	375.261300	7.149312
6.053471	399.931508	7.154317
5.906127	382.783271	7.159322
5.713800	393.194118	7.164326
5.990541	378.266628	7.169331
5.714624	381.706453	7.174336
5.624262	371.566101	7.179341
5.623480	378.500074	7.184346
5.647044	390.104603	7.189350
5.878129	401.836335	7.194355
5.587896	402.992538	7.199360
6.043113	393.521606	7.204365
6.091764	406.433539	7.209370
5.624012	401.641247	7.214374
5.722404	393.852158	7.219379
5.840161	383.893839	7.224384
5.706054	402.951314	7.229389
6.083359	386.219776	7.234394
5.848602	393.787177	7.239398
5.754820	363.254310	7.244403
5.742375	384.663961	7.249408
5.987361	360.949461	7.254413
5.876049	375.518071	7.259418
5.703277	364.610636	7.264422
5.717983	373.332029	7.269427
5.896694	367.239855	7.274432
5.875771	375.600854	7.279437
5.715222	367.911393	7.284442
5.530287	374.793820	7.289446
5.601336	374.228775	7.294451
5.768675	383.128363	7.299456
5.892069	391.480910	7.304461
5.851345	382.213579	7.309466
5.821134	378.114896	7.314470
5.912669	378.157101	7.319475
5.426940	380.144173	7.324480
5.979048	382.425651	7.329485
5.995054	387.579202	7.334490
5.859015	382.071840	7.339494
6.078540	364.328615	7.344499
5.635629	377.522016	7.349504
5.684288	366.766109	7.354509
5.808368	382.071007	7.359514
6.063223	368.976289	7.364518
6.066206	381.075484	7.369523
5.703598	364.981391	7.374528
5.845961	382.633278	7.379533
5.736933	364.652151	7.384538
5.637194	369.679021	7.389542
5.746983	368.915604	7.394547
5.535923	372.546741	7.399552
5.878195	367.656504	7.404557
5.656819	382.121183	7.409562
5.570864	366.902256	7.414566
5.843398	373.053166	7.419571
5.789156	391.939985	7.424576
6.033931	374.618640	7.429581
5.635967	384.603170	7.434586
5.471037	371.403511	7.439590
5.853462	376.322488	7.444595
5.621592	402.851997	7.449600
5.948236	403.740033	7.454605
5.945259	405.049417	7.459610
5.624264	404.864343	7.464614
6.178692	377.096589	7.469619
5.458533	392.554433	7.474624
5.777185	381.255719	7.479629
5.785032	388.223094	7.484634
5.963557	391.043476	7.489638
5.795496	376.513754	7.494643
5.626398	375.384961	7.499648
5.747381	381.637274	7.504653
6.330419	379.890347	7.509658
5.935585	391.524364	7.514662
6.125345	371.568225	7.519667
5.898814	370.508606	7.524672
5.791539	368.092292	7.529677
5.768260	372.350483	7.534682
5.484718	367.844224	7.539686
5.930977	373.224290	7.544691
5.596899	372.084486	7.549696
5.962848	380.229634	7.554701
5.722768	374.444509	7.559706
5.870143	371.715715	7.564710
6.230301	363.701079	7.569715
5.642384	372.511801	7.574720
5.543043	368.943635	7.579725
5.646672	358.333725	7.584730
5.569284	375.846721	7.589734
6.001317	367.938188	7.594739
5.989307	384.531539	7.599744
5.931977	359.506634	7.604749
5.823831	377.589873	7.609754
5.700909	370.110923	7.614758
5.852277	378.595272	7.619763
5.600435	366.017658	7.624768
5.821363	374.277723	7.629773
5.789908	375.260943	7.634778
5.616622	370.248053	7.639782
5.615864	377.465933	7.644787
5.725405	378.356107	7.649792
5.654433	372.403448	7.654797
5.759966	371.055648	7.659802
5.611633	379.062346	7.664806
5.805875	366.699066	7.669811
5.732342	388.601408	7.674816
6.065297	369.376961	7.679821
5.834318	375.056973	7.684826
5.565533	393.264538	7.689830
6.075253	371.860429	7.694835
5.664315	390.953576	7.699840
5.630406	374.875489	7.704845
5.991245	373.501576	7.709850
5.560360	378.384002	7.714854
5.680860	378.333623	7.719859
5.578919	387.016986	7.724864
5.809922	392.160065	7.729869
5.841143	398.234262	7.734874
5.700130	383.002714	7.739878
6.083146	400.133150	7.744883
5.586502	382.536964	7.749888
5.900502	392.991393	7.754893
5.743992	377.904269	7.759898
5.646274	371.875532	7.764902
5.793708	377.370092	7.769907
5.892235	390.792958	7.774912
5.866646	388.003073	7.779917
5.653491	376.586172	7.784922
6.016972	393.586258	7.789926
6.092894	387.234648	7.794931
5.991052	374.029987	7.799936
5.739232	381.557586	7.804941
5.808373	372.695307	7.809946
5.411386	382.158216	7.814950
5.556949	374.823610	7.819955
5.284628	383.365747	7.824960
5.878784	395.458407	7.829965
5.889269	402.902912	7.834970
5.984107	412.325895	7.839974
6.307515	403.413687	7.844979
5.778807	394.757426	7.849984
5.567118	375.046082	7.854989
5.795462	391.891325	7.859994
5.875331	378.280779	7.864998
5.930285	386.758179	7.870003
5.703845	380.764917	7.875008
5.742045	391.930507	7.880013
5.922168	377.304278	7.885018
5.650691	388.723470	7.890022
6.115921	368.237150	7.895027
5.817609	382.591824	7.900032
5.585111	371.393474	7.905037
5.892002	373.439555	7.910042
5.379197	375.535076	7.915046
5.662896	373.079502	7.920051
5.906778	376.291371	7.925056
6.154286	379.763369	7.930061
5.648034	363.616563	7.935066
5.571957	377.226801	7.940070
5.691922	360.724857	7.945075
6.059379	388.642526	7.950080
5.686269	361.288518	7.955085
5.964073	373.521337	7.960090
5.656279	369.637416	7.965094
5.647518	376.514406	7.970099
5.717236	374.767866	7.975104
5.871560	389.002169	7.980109
5.602633	386.007652	7.985114
5.894612	383.156507	7.990118
6.021247	398.774986	7.995136
5.706895	380.852140	8.000154
5.591281	376.839343	8.005171
6.049241	383.491882	8.010189
5.872588	381.089897	8.015206
5.954406	357.252093	8.020224
5.835428	374.597828	8.025242
5.633682	371.952818	8.030259
6.002587	368.458600	8.035277
5.800382	370.652934	8.040294
5.928738	380.251734	8.045312
5.710170	367.062610	8.050330
5.983069	387.867691	8.055347
6.185426	380.043375	8.060365
5.695331	365.024757	8.065382
5.820812	376.428043	8.070400
5.796924	376.920453	8.075418
5.755616	368.732884	8.080435
5.833992	375.937674	8.085453
5.621262	377.499382	8.090470
5.923746	396.205005	8.095488
6.038031	402.890536	8.100506
6.047288	400.671346	8.105523
5.796558	379.776918	8.110541
5.981890	396.152473	8.115558
5.767373	368.535478	8.120576
5.845699	386.658232	8.125594
5.933717	378.616659	8.130611
6.251798	387.402443	8.135629
5.842680	382.016605	8.140646
5.658848	375.822890	8.145664
5.638005	383.818566	8.150682
6.096767	386.067699	8.155699
5.993527	402.206188	8.160717
5.685261	401.208629	8.165734
5.905388	401.532404	8.170752
6.034874	393.156504	8.175770
6.001079	415.354838	8.180787
6.326891	395.209163	8.185805
5.967540	407.203768	8.190822
6.353745	398.544170	8.195840
6.116078	389.421598	8.200858
5.734161	387.780492	8.205875
5.878447	377.705393	8.210893
5.914386	404.889191	8.215910
6.106685	392.214460	8.220928
5.984446	409.080890	8.225946
5.791478	420.874830	8.230963
5.987683	402.283006	8.235981
5.741889	420.462512	8.240998
6.103971	398.609350	8.246016
5.867632	408.520827	8.251034
5.905722	405.342122	8.256051
5.842721	410.253725	8.261069
5.949789	404.915705	8.266086
6.440761	409.379068	8.271104
6.022642	399.455444	8.276122
5.786383	397.766355	8.281139
6.033942	401.804719	8.286157
5.877057	409.307092	8.291174
5.924550	394.432116	8.296192
6.506324	402.251070	8.301210
6.152787	402.247327	8.306227
6.108129	404.238219	8.311245
5.719849	395.975435	8.316262
6.190651	406.128313	8.321280
6.118083	394.925590	8.326298
6.005293	404.170077	8.331315
6.423022	405.458946	8.336333
5.854007	413.083940	8.341350
6.231525	407.700241	8.346368
6.039925	414.870358	8.351386
6.257434	419.161261	8.356403
6.393366	405.802920	8.361421
6.112039	413.091575	8.366438
6.089408	398.925133	8.371456
6.212210	391.429322	8.376474
6.063577	410.661452	8.381491
6.469167	402.282426	8.386509
6.301559	407.856802	8.391526
6.004174	396.111178	8.396544
5.784224	393.944825	8.401562
6.268663	405.118091	8.406579
6.457626	414.079516	8.411597
6.078363	402.676164	8.416614
6.172626	402.073370	8.421632
6.232373	397.647936	8.426650
5.873635	403.932149	8.431667
6.509024	428.084191	8.436685
6.532374	428.108296	8.441702
6.509726	422.895713	8.446720
6.566598	404.013910	8.451738
6.305724	410.285692	8.456755
6.670482	406.061156	8.461773
6.186777	401.447953	8.466790
6.411389	417.934821	8.471808
6.427273	399.298707	8.476826
5.880916	401.291135	8.481843
6.392953	405.403574	8.486861
6.260329	392.726946	8.491878
6.115049	402.414374	8.496896
6.374993	402.036097	8.501914
5.759320	411.164932	8.506931
6.422224	409.888506	8.511949
6.099035	420.659970	8.516966
6.086253	425.050824	8.521984
6.580450	413.787683	8.527002
6.754250	438.708052	8.532019
6.394174	396.000715	8.537037
6.235329	420.501851	8.542054
6.070937	404.623100	8.547072
6.292770	415.435851	8.552090
6.255954	439.024189	8.557107
6.578074	434.356523	8.562125
6.313092	448.126891	8.567143
6.521828	437.334018	8.572160
6.530898	424.877087	8.577178
6.445967	438.782311	8.582195
6.665082	430.118821	8.587213
6.312646	410.272759	8.592231
6.363899	399.266536	8.597248
6.601067	418.093086	8.602266
6.288533	407.936222	8.607283
6.288992	419.368072	8.612301
6.484988	437.123802	8.617319
6.498365	421.648112	8.622336
6.552245	437.272621	8.627354
6.178836	429.753804	8.632371
6.484635	433.553877	8.637389
6.570252	431.064262	8.642407
6.689678	432.190974	8.647424
6.555575	447.582557	8.652442
6.373181	433.470136	8.657459
6.574710	432.958146	8.662477
6.731980	438.923109	8.667495
6.454943	434.928019	8.672512
6.910978	411.657836	8.677530
6.264111	417.668894	8.682547
6.422722	416.818032	8.687565
6.482173	427.509342	8.692583
6.614308	413.844523	8.697600
6.524473	411.267011	8.702618
6.718194	427.048860	8.707635
6.735766	421.160035	8.712653
6.403340	409.577432	8.717671
6.057346	417.914967	8.722688
6.424812	403.848179	8.727706
6.417407	440.585321	8.732723
6.847617	425.196014	8.737741
6.882865	441.949077	8.742759
6.628258	439.680403	8.747776
6.799759	425.995686	8.752794
6.587656	451.477838	8.757811
6.701004	422.594897	8.762829
6.695235	418.272089	8.767847
6.246146	421.154980	8.772864
6.478550	429.662609	8.777882
6.561402	434.868727	8.782899
6.482702	450.813204	8.787917
6.665732	434.964582	8.792935
6.614018	442.544052	8.797952
6.764098	437.083788	8.802970
6.495061	444.881502	8.807987
6.590405	424.783913	8.813005
6.886833	437.043390	8.818023
6.675533	425.914343	8.823040
6.877146	423.362364	8.828058
6.500743	430.901812	8.833075
6.486891	417.464208	8.838093
6.838464	443.421047	8.843111
6.853090	434.024536	8.848128
7.106147	438.023922	8.853146
6.722253	433.316283	8.858163
6.688653	444.698382	8.863181
6.641480	435.193515	8.868199
6.751136	453.993852	8.873216
6.611805	436.173380	8.878234
6.747510	433.361402	8.883251
6.832795	448.274138	8.888269
6.918488	430.682651	8.893287
6.622173	432.939679	8.898304
6.601590	436.395967	8.903322
6.728712	425.862090	8.908339
7.170449	437.330053	8.913357
6.894324	430.039972	8.918375
6.511559	430.956451	8.923392
6.930585	446.861079	8.928410
6.693537	436.800846	8.933427
6.867094	449.335486	8.938445
6.941319	437.323163	8.943463
6.712656	440.384924	8.948480
6.773250	431.170037	8.953498
7.195534	442.777302	8.958515
6.888675	439.645757	8.963533
7.016738	429.281359	8.968551
6.607532	441.882192	8.973568
6.986560	433.892568	8.978586
6.677855	445.994843	8.983603
6.718920	432.888411	8.988621
6.389521	437.443765	8.993639
6.455265	449.440965	8.998656
6.637345	436.627475	9.003674
6.779392	451.627854	9.008691
6.820868	438.217103	9.013709
7.092599	441.345242	9.018727
6.848153	448.232554	9.023744
7.111338	448.684315	9.028762
6.672816	448.308799	9.033779
6.793310	445.904534	9.038797
7.080174	460.857868	9.043815
7.122454	468.549734	9.048832
7.222214	451.647436	9.053850
6.936286	438.483946	9.058867
6.684607	433.692172	9.063885
6.841270	450.142973	9.068903
6.787446	441.149393	9.073920
7.201185	459.325630	9.078938
6.948994	459.773610	9.083955
7.233440	477.116061	9.088973
7.448377	459.159478	9.093991
6.880021	450.477728	9.099008
7.112240	435.669699	9.104026
6.772960	431.920951	9.109043
6.717054	443.937859	9.114061
7.173317	447.106742	9.119079
7.296928	469.952577	9.124096
7.243593	451.928457	9.129114
7.231815	455.116046	9.134131
6.944427	426.628659	9.139149
6.635317	445.082952	9.144167
6.887628	459.139197	9.149184
7.214979	456.751518	9.154202
7.371852	459.172763	9.159219
7.127496	466.881101	9.164237
7.202536	455.227188	9.169255
7.102902	452.509202	9.174272
7.285340	456.372765	9.179290
7.146133	449.523500	9.184307
6.920976	434.520366	9.189325
7.192495	448.490770	9.194343
6.916562	461.315392	9.199360
7.185729	460.994333	9.204378
7.142009	461.243832	9.209395
7.018546	466.889947	9.214413
7.258162	456.818623	9.219431
7.087344	472.356615	9.224448
6.967620	459.903425	9.229466
6.900006	463.513513	9.234483
6.897979	457.029263	9.239501
7.476353	461.074963	9.244519
7.226033	445.613111	9.249536
7.207584	462.416201	9.254554
7.494939	457.814592	9.259571
7.192745	465.788419	9.264589
7.417219	452.513212	9.269607
7.339295	463.454450	9.274624
7.181158	456.909999	9.279642
7.524140	471.015424	9.284659
6.890728	465.884278	9.289677
7.351908	461.921176	9.294695
7.187493	479.875651	9.299712
7.645609	456.322949	9.304730
7.592464	457.141859	9.309747
7.413914	470.684835	9.314765
7.568039	453.993272	9.319783
7.402130	460.819398	9.324800
7.361593	449.549842	9.329818
7.452708	439.049263	9.334835
6.953210	426.476137	9.339853
7.489499	453.472932	9.344871
7.023020	451.453384	9.349888
7.559377	466.869190	9.354906
7.594798	460.721567	9.359923
7.180271	467.351643	9.364941
7.353563	452.231278	9.369959
7.315071	460.500898	9.374976
7.546188	459.480812	9.379994
7.492889	448.736055	9.385011
7.441869	455.582255	9.390029
7.714077	443.001237	9.395047
6.985250	441.503160	9.400064
7.404828	442.224464	9.405082
7.613887	442.739288	9.410099
7.279397	440.659357	9.415117
7.469388	447.426069	9.420135
7.652325	450.213767	9.425152
7.400348	453.845367	9.430170
7.180129	457.185579	9.435187
7.305063	455.069277	9.440205
7.883054	459.378551	9.445223
7.682697	465.148561	9.450240
7.752746	445.113670	9.455258
7.474960	436.513502	9.460275
7.227609	442.382092	9.465293
7.443829	435.873000	9.470311
7.458340	435.579167	9.475328
7.364895	455.369395	9.480346
7.563685	450.399854	9.485363
7.505003	466.941464	9.490381
7.721265	456.542497	9.495399
7.603445	469.582464	9.500416
7.705353	448.149091	9.505434
7.671969	436.882202	9.510451
7.282421	424.160334	9.515469
7.468962	422.764260	9.520487
7.161287	442.868539	9.525504
6.946567	457.966554	9.530522
7.579938	455.527909	9.535539
7.562426	459.432389	9.540557
7.941120	469.170040	9.545575
7.585774	465.526962	9.550592
7.182504	483.162942	9.555610
7.482051	460.086808	9.560627
7.463683	469.115491	9.565645
7.259244	459.068745	9.570663
7.848955	470.809046	9.575680
7.288356	464.403227	9.580698
7.671872	469.384915	9.585715
7.745377	462.289824	9.590733
7.663909	467.758180	9.595751
7.485263	469.331091	9.600768
7.617118	448.119083	9.605786
7.861457	457.038025	9.610803
7.696534	461.094488	9.615821
7.829200	446.944450	9.620839
7.676244	469.854784	9.625856
7.597530	454.252784	9.630874
7.856889	450.618722	9.635891
7.924583	437.979504	9.640909
7.928901	444.519787	9.645927
7.596906	448.542751	9.650944
7.667464	443.361203	9.655962
8.167634	463.229473	9.660979
7.713633	458.562341	9.665997
7.743171	467.705022	9.671015
7.750141	460.980275	9.676032
7.764647	448.896434	9.681050
7.944379	453.033399	9.686067
7.636951	459.690643	9.691085
7.748225	465.198779	9.696103
7.344710	466.624651	9.701120
7.889451	480.498570	9.706138
8.447839	477.842752	9.711155
7.966445	470.040467	9.716173
7.848441	462.631746	9.721191
7.951753	455.332868	9.726208
7.656537	466.126506	9.731226
7.640632	462.813643	9.736243
7.753462	467.877651	9.741261
7.700266	462.077552	9.746279
8.040293	466.631115	9.751296
7.843219	483.687207	9.756314
8.266516	473.354972	9.761331
8.102392	474.604706	9.766349
8.070604	457.412712	9.771367
8.149015	453.725899	9.776384
7.841123	456.302077	9.781402
8.057129	451.713441	9.786419
8.005138	460.668762	9.791437
7.893280	456.063953	9.796455
8.127393	462.303744	9.801472
7.871089	459.096634	9.806490
8.109060	465.868120	9.811507
7.995819	462.084569	9.816525
8.054570	466.501791	9.821543
8.255396	465.144287	9.826560
7.899290	458.188187	9.831578
8.098600	455.620150	9.836595
7.887046	454.121012	9.841613
7.804669	458.098792	9.846631
8.084066	464.917648	9.851648
7.658933	463.703342	9.856666
7.734302	454.102445	9.861683
8.065141	477.997010	9.866701
8.165218	466.990935	9.871719
8.169311	453.466400	9.876736
7.906825	465.365144	9.881754
8.198705	445.617814	9.886771
8.210179	460.129787	9.891789
7.947298	460.192436	9.896807
8.067619	450.717146	9.901824
8.059506	454.091183	9.906842
8.249227	482.952378	9.911859
8.136944	460.817090	9.916877
8.038419	470.128926	9.921895
8.208436	460.607632	9.926912
8.077982	483.542015	9.931930
8.362151	490.783009	9.936947
8.302747	475.576406	9.941965
8.125274	473.456845	9.946983
8.448124	460.353314	9.952000
7.775473	459.509053	9.957018
8.255514	455.350960	9.962035
8.266581	469.522946	9.967053
8.235901	462.449401	9.972071
8.307695	463.367217	9.977088
8.259311	443.580283	9.982106
8.368113	456.341416	9.987123
7.955369	453.893321	9.992141
8.349080	469.257134	9.997159
8.769936	470.277260	10.002176
8.036801	465.416853	10.007194
8.122937	464.373889	10.012211
8.167197	463.965033	10.017229
7.996355	484.958211	10.022247
8.542390	493.686509	10.027264
8.530165	502.653389	10.032282
8.457250	476.669524	10.037299
8.283746	470.129770	10.042317
8.072960	474.162918	10.047335
8.339760	458.617170	10.052352
8.409460	494.594073	10.057370
8.529524	469.566737	10.062387
8.085252	479.494222	10.067405
8.396497	489.074772	10.072423
8.478107	474.164366	10.077440
8.051361	491.336058	10.082458
8.458853	471.152678	10.087475
7.887387	492.686744	10.092493
8.576700	480.422582	10.097511
8.728144	500.956928	10.102528
8.344139	491.631571	10.107546
8.599486	496.945585	10.112563
8.481439	504.589379	10.117581
8.377591	506.978836	10.122599
8.404013	502.668397	10.127616
8.510425	493.861137	10.132634
8.689822	506.479288	10.137651
8.511453	484.671431	10.142669
8.286317	484.939202	10.147687
8.654642	478.821572	10.152704
8.166426	495.703906	10.157722
8.600929	470.306975	10.162739
8.368221	489.061699	10.167757
8.510902	489.712164	10.172775
8.337571	485.460619	10.177792
8.185871	491.801572	10.182810
8.431815	486.492232	10.187827
8.491091	487.244546	10.192845
8.367919	486.071650	10.197863
8.756690	478.950624	10.202880
8.663323	487.779763	10.207898
8.538235	498.120329	10.212915
8.820169	498.225978	10.217933
8.451718	502.320415	10.222951
8.680122	485.644289	10.227968
8.466294	503.852167	10.232986
8.563143	489.446269	10.238003
8.652635	510.102744	10.243021
8.237218	506.282627	10.248039
8.527976	486.003588	10.253056
8.192187	490.353182	10.258074
8.097011	498.736689	10.263091
8.554584	500.242542	10.268109
8.847217	526.546965	10.273127
9.175617	504.079508	10.278144
8.900406	474.993625	10.283162
8.902597	482.843164	10.288179
9.146050	478.439991	10.293197
8.730126	487.502405	10.298215
9.015877	470.985671	10.303232
8.456540	488.169825	10.308250
8.608679	471.939172	10.313267
8.754898	478.387535	10.318285
8.932836	484.605918	10.323303
8.960869	478.492374	10.328320
8.565013	490.629160	10.333338
8.846814	475.632436	10.338355
8.941867	473.195472	10.343373
8.583239	482.813218	10.348391
8.883443	480.746668	10.353408
9.106755	479.119083	10.358426
8.862701	494.019774	10.363443
9.305235	479.414674	10.368461
8.869449	490.510418	10.373479
9.106123	485.218747	10.378496
9.013478	488.809461	10.383514
8.891570	487.315972	10.388531
8.999004	487.802034	10.393549
8.586406	494.695510	10.398567
8.969065	478.021552	10.403584
8.785796	496.799604	10.408602
8.994694	488.313408	10.413619
8.980594	497.252453	10.418637
8.427269	482.371593	10.423655
8.554605	506.270708	10.428672
8.821764	487.629858	10.433690
8.599750	488.906183	10.438707
8.874191	501.322454	10.443725
8.660634	505.727422	10.448743
9.021328	497.780942	10.453760
9.056313	491.336510	10.458778
9.000755	481.781341	10.463795
9.008250	488.292188	10.468813
8.561400	474.382738	10.473831
8.910957	473.427208	10.478848
9.056136	485.277489	10.483866
9.002075	481.425410	10.488883
9.205409	480.733545	10.493901
8.879407	488.427736	10.498919
8.906024	486.690176	10.503936
9.073810	504.146794	10.508954
9.227076	519.049940	10.513971
9.291336	490.250944	10.518989
8.936603	504.807341	10.524007
9.276334	489.086363	10.529024
8.951565	495.231080	10.534042
9.090808	491.843076	10.539059
9.337760	495.531665	10.544077
8.970858	495.682843	10.549095
9.218584	496.602681	10.554112
9.296905	495.284803	10.559130
9.188928	488.945472	10.564147
8.882781	504.818866	10.569165
8.722137	488.041034	10.574183
9.254155	514.501197	10.579200
9.238353	521.235140	10.584218
9.203801	501.535190	10.589235
9.439563	510.379125	10.594253
9.334021	502.581128	10.599271
8.910666	499.308040	10.604288
9.089481	501.327941	10.609306
9.061461	514.776512	10.614323
9.295640	493.176964	10.619341
9.122259	517.060456	10.624359
9.218158	492.935546	10.629376
9.419805	511.059716	10.634394
9.413408	493.659111	10.639411
9.424285	515.452584	10.644429
9.167007	505.429102	10.649447
9.495217	495.367515	10.654464
9.336960	507.814953	10.659482
9.223378	511.879771	10.664499
9.396412	506.716983	10.669517
9.118330	524.388015	10.674535
9.390661	504.608712	10.679552
9.393748	522.899431	10.684570
9.177578	501.928868	10.689587
9.644672	508.144247	10.694605
9.248257	510.285483	10.699623
9.440861	514.371629	10.704640
9.637083	510.107122	10.709658
8.901929	507.344291	10.714675
9.405974	497.111754	10.719693
9.446293	501.718202	10.724711
9.338022	488.170287	10.729728
9.747464	502.023981	10.734746
9.383418	500.399096	10.739763
9.349757	498.478932	10.744781
9.464995	513.925610	10.749799
9.450438	489.438454	10.754816
9.274914	502.858553	10.759834
9.363408	501.113029	10.764851
9.342625	508.060723	10.769869
9.375412	509.091061	10.774887
9.101202	518.027249	10.779904
9.124565	512.291917	10.784922
9.457729	510.985452	10.789939
9.312729	520.245271	10.794957
9.581185	526.744398	10.799975
9.808968	523.765458	10.804992
9.725879	522.762165	10.810010
9.279742	516.698431	10.815027
9.513386	515.996930	10.820045
9.430974	525.446551	10.825063
9.630755	544.167950	10.830080
9.720971	531.205039	10.835098
9.665001	542.679664	10.840115
9.858822	518.138840	10.845133
9.852487	526.472059	10.850151
9.824576	504.043314	10.855168
9.858904	488.390912	10.860186
9.615202	502.436576	10.865203
9.511051	497.634177	10.870221
9.357505	505.494311	10.875239
9.410107	502.649020	10.880256
9.607011	510.742992	10.885274
9.857368	546.258786	10.890291
10.171174	524.543308	10.895309
9.967115	530.816770	10.900327
9.983708	500.264798	10.905344
10.036903	498.115674	10.910362
9.615572	494.324481	10.915379
9.848312	508.703997	10.920397
9.667528	498.525200	10.925415
9.780585	482.202300	10.930432
9.659878	493.237908	10.935450
9.457446	504.061306	10.940467
9.547204	494.343174	10.945485
9.549288	503.949540	10.950503
9.938983	527.953124	10.955520
10.328667	531.250419	10.960538
9.830399	510.107626	10.965555
9.739846	511.803838	10.970573
9.616049	506.794701	10.975591
9.902843	531.743584	10.980608
10.152150	533.459302	10.985626
9.950298	525.865740	10.990643
9.837547	510.815417	10.995661
10.027545	511.199080	11.000679
9.937101	502.845592	11.005696
10.028554	505.545789	11.010714
9.918610	505.054079	11.015731
10.462200	494.217437	11.020749
10.156778	501.655254	11.025767
9.964339	496.063141	11.030784
10.118193	508.163118	11.035802
10.067879	512.344118	11.040819
10.031650	498.692287	11.045837
9.949039	504.297520	11.050855
9.718543	498.334733	11.055872
9.959121	476.926027	11.060890
9.780668	502.116761	11.065907
9.773623	471.348440	11.070925
9.987143	504.966328	11.075943
9.974100	501.461599	11.080960
10.334326	521.968849	11.085978
10.102132	517.940053	11.090995
10.420358	499.093169	11.096013
10.147328	511.020947	11.101031
10.038642	504.479913	11.106048
10.153612	502.795842	11.111066
9.747358	510.915201	11.116083
9.930894	502.595252	11.121101
10.032204	530.217164	11.126119
10.254209	527.702436	11.131136
10.305244	529.782128	11.136154
10.148630	544.841795	11.141171
10.352372	517.067345	11.146189
10.085495	516.484278	11.151207
9.979610	518.771839	11.156224
10.479494	524.732071	11.161242
10.197919	523.459596	11.166259
10.330154	515.705051	11.171277
9.965603	513.568579	11.176295
9.909476	523.687586	11.181312
10.351552	531.143382	11.186330
10.202292	527.407487	11.191347
10.276466	530.778570	11.196365
10.331561	531.171243	11.201383
10.401624	532.161377	11.206400
10.594372	535.394000	11.211418
10.495567	543.853110	11.216435
10.313540	525.354146	11.221453
10.310760	525.749988	11.226471
10.095832	519.156053	11.231488
10.242464	534.866781	11.236506
10.470130	533.978032	11.241523
10.609777	531.573738	11.246541
10.322303	527.760515	11.251559
10.260581	525.631461	11.256576
10.378009	538.717232	11.261594
10.478562	538.470578	11.266611
10.679746	538.167837	11.271629
10.666817	533.215152	11.276647
10.427326	535.139861	11.281664
10.209993	511.463724	11.286682
10.131011	524.963235	11.291699
10.277430	534.300655	11.296717
10.681894	533.378163	11.301735
10.313131	530.288512	11.306752
10.495139	540.865186	11.311770
10.406149	544.338313	11.316787
10.613881	516.896085	11.321805
10.600604	530.007877	11.326823
10.440331	518.404809	11.331840
10.337326	517.284861	11.336858
10.704525	515.111590	11.341875
10.444255	535.766763	11.346893
10.385975	521.087245	11.351911
10.330655	544.970161	11.356928
10.433471	535.873199	11.361946
10.183617	528.630388	11.366963
10.349360	529.093826	11.371981
10.470817	513.118032	11.376999
10.093577	532.757777	11.382016
10.738951	546.583442	11.387034
10.657126	563.751743	11.392051
10.806049	575.671732	11.397069
10.559365	553.420959	11.402087
10.791711	572.225570	11.407104
11.135940	550.650559	11.412122
10.935547	562.210171	11.417139
10.551534	534.395949	11.422157
10.678076	539.732246	11.427175
10.755688	534.705560	11.432192
10.791360	525.626194	11.437210
10.774911	529.833286	11.442227
10.607047	529.412646	11.447245
10.502739	537.919598	11.452263
10.658323	554.096652	11.457280
10.990636	549.937856	11.462298
11.048616	554.888059	11.467315
10.672624	542.661255	11.472333
10.809797	545.281286	11.477351
10.683874	557.203681	11.482368
11.206408	542.558536	11.487386
10.786481	550.984521	11.492403
10.734055	537.002058	11.497421
10.879436	540.896956	11.502439
10.890070	549.666043	11.507456
10.922012	554.528153	11.512474
10.984002	548.300435	11.517491
10.894000	556.815169	11.522509
10.935769	549.658173	11.527527
10.841837	554.240379	11.532544
10.986900	555.747798	11.537562
10.867662	562.642613	11.542579
10.991137	563.377828	11.547597
11.110361	546.322053	11.552615
10.935740	549.442996	11.557632
11.006827	543.461544	11.562650
11.176850	560.719288	11.567667
10.954978	556.035904	11.572685
11.184099	541.146514	11.577703
11.010437	557.163081	11.582720
11.506099	551.029987	11.587738
10.944099	542.268220	11.592755
10.594273	531.529900	11.597773
11.119291	535.122164	11.602791
10.927091	559.458806	11.607808
11.016017	550.044730	11.612826
11.222635	556.494854	11.617843
11.127812	555.732901	11.622861
11.242538	549.955102	11.627879
11.208037	559.831157	11.632896
11.327717	546.228793	11.637914
11.101485	557.079284	11.642931
11.120935	544.519484	11.647949
11.599850	551.644587	11.652967
10.993160	540.443336	11.657984
11.087053	544.230635	11.663002
11.323905	552.383167	11.668019
11.299244	561.379096	11.673037
11.296100	575.400125	11.678055
11.018421	564.078361	11.683072
11.212727	545.818968	11.688090
11.300599	559.365717	11.693107
11.461323	542.247297	11.698125
11.442553	550.926092	11.703143
11.173134	545.264619	11.708160
11.201954	551.032015	11.713178
11.460054	550.905152	11.718195
11.265568	541.397208	11.723213
11.434536	548.137035	11.728231
11.010185	545.727940	11.733248
11.354729	548.865224	11.738266
11.301599	543.602632	11.743283
11.116126	554.237584	11.748301
11.217485	540.652718	11.753319
11.137622	549.109684	11.758336
11.045577	556.254559	11.763354
11.214421	547.558180	11.768371
11.176283	571.871743	11.773389
11.557909	543.697279	11.778407
11.439314	547.384199	11.783424
11.419632	556.807925	11.788442
11.470234	549.978907	11.793459
11.359258	551.052194	11.798477
11.514305	540.302166	11.803495
11.368786	558.636281	11.808512
11.639686	548.363324	11.813530
11.640330	562.703313	11.818547
11.759045	559.172172	11.823565
11.904268	563.626989	11.828583
11.179569	558.403150	11.833600
11.403812	543.890445	11.838618
11.642451	549.335352	11.843635
11.181080	559.013519	11.848653
11.723647	550.687641	11.853671
11.536310	571.798496	11.858688
11.705646	573.836110	11.863706
12.206210	562.191793	11.868723
11.618036	558.327889	11.873741
11.825721	554.872966	11.878759
11.548130	550.113185	11.883776
11.722967	546.366923	11.888794
11.947213	546.198226	11.893811
11.559795	546.180008	11.898829
11.828374	539.105384	11.903847
11.874223	553.826568	11.908864
11.763195	531.380818	11.913882
11.609928	547.426081	11.918899
11.328384	542.279366	11.923917
11.419741	554.690413	11.928935
11.724886	561.405184	11.933952
11.912227	571.238188	11.938970
11.919372	573.175573	11.943987
11.788645	575.476202	11.949005
12.107208	561.223803	11.954023
11.721076	564.996169	11.959040
11.702655	553.057906	11.964058
11.987304	568.827237	11.969075
11.896601	571.387812	11.974093
11.923094	564.098922	11.979111
11.769354	556.944811	11.984128
11.760257	579.028308	11.989146
12.216661	567.331951	11.994163
11.861344	569.693507	11.999181
12.338530	579.122415	12.004199
11.963028	548.931912	12.009216
11.921201	543.121736	12.014234
12.191930	548.414726	12.019251
11.982274	534.786701	12.024269
11.700204	539.683185	12.029287
11.629604	545.583512	12.034304
12.037995	546.368662	12.039322
12.188645	573.530654	12.044339
12.376986	566.224266	12.049357
12.034858	552.745445	12.054375
12.108076	548.001391	12.059392
11.969062	547.551284	12.064410
11.912057	548.796311	12.069427
12.005954	561.504402	12.074445
12.257775	577.270507	12.079463
12.219493	575.656132	12.084480
12.216511	572.212797	12.089498
12.346250	569.518186	12.094515
12.279661	565.832284	12.099533
12.433247	542.310884	12.104551
11.970746	558.481750	12.109568
11.870157	548.916465	12.114586
12.280316	541.603541	12.119603
11.839086	551.691549	12.124621
12.032416	568.711558	12.129639
11.845236	572.367113	12.134656
11.827724	571.488573	12.139674
11.894494	573.642323	12.144691
11.990437	572.728798	12.149709
12.123974	586.598643	12.154727
12.183346	579.875023	12.159744
12.230644	587.617779	12.164762
12.335421	580.335526	12.169779
12.034964	591.725035	12.174797
12.271249	573.635985	12.179815
12.660142	593.123318	12.184832
12.151624	598.662295	12.189850
12.498277	595.100955	12.194867
12.325298	581.384173	12.199885
12.392660	577.858267	12.204903
12.035814	583.174098	12.209920
12.570981	602.963264	12.214938
12.956323	598.815765	12.219955
12.556156	589.731834	12.224973
12.621827	576.652008	12.229991
12.399392	580.791904	12.235008
12.209709	585.687401	12.240026
12.443970	584.056422	12.245043
12.241258	583.504175	12.250061
12.753941	595.907619	12.255079
12.527606	590.969126	12.260096
12.617366	599.744058	12.265114
12.724476	582.867066	12.270131
12.389023	580.957995	12.275149
12.541894	575.738297	12.280167
12.710522	585.864580	12.285184
12.672962	580.923232	12.290202
12.472978	568.902000	12.295219
12.762382	583.526777	12.300237
12.648471	577.565651	12.305255
12.738685	580.231135	12.310272
12.463254	569.326304	12.315290
12.890897	569.642652	12.320307
12.761898	570.280258	12.325325
12.319279	566.209671	12.330343
12.808242	577.247117	12.335360
12.763825	578.869687	12.340378
12.948427	572.126359	12.345395
12.420550	568.413370	12.350413
12.919235	591.823807	12.355431
12.759285	581.961110	12.360448
12.921310	597.629017	12.365466
13.020698	573.639194	12.370483
12.717677	578.391751	12.375501
12.524055	589.254588	12.380519
12.973977	568.887342	12.385536
12.743180	581.232096	12.390554
12.838792	586.879738	12.395571
12.780536	591.933095	12.400589
13.059616	596.371114	12.405607
13.186226	562.386407	12.410624
12.626313	577.877125	12.415642
12.830239	550.464395	12.420659
13.129046	581.452832	12.425677
12.787497	570.285674	12.430695
12.715932	579.241839	12.435712
12.948853	588.251401	12.440730
13.081078	591.674206	12.445747
12.925868	603.327930	12.450765
13.097854	590.191263	12.455783
13.469033	599.532120	12.460800
13.055663	578.565308	12.465818
12.827139	575.986677	12.470835
12.911815	569.187542	12.475853
13.142775	579.573820	12.480871
13.176927	563.232879	12.485888
12.816235	570.547024	12.490906
13.244124	579.417993	12.495923
13.276964	579.732577	12.500941
13.012231	569.837513	12.505959
13.131562	565.055034	12.510976
13.094206	569.691264	12.515994
13.272333	568.295289	12.521011
13.210534	566.280089	12.526029
13.123418	570.100455	12.531047
13.293586	555.892658	12.536064
12.721471	576.159579	12.541082
13.373548	575.377119	12.546099
13.368097	581.415079	12.551117
13.360371	592.492504	12.556135
13.237396	574.436552	12.561152
12.683177	576.835702	12.566170
13.241354	592.693184	12.571187
13.216863	597.604682	12.576205
13.327606	603.604163	12.581223
13.327162	578.139305	12.586240
13.035260	577.841987	12.591258
13.249233	586.863045	12.596275
13.068975	581.622925	12.601293
13.424945	597.746541	12.606311
13.496043	594.620004	12.611328
13.375788	598.589024	12.616346
13.469124	588.552513	12.621363
13.515583	602.350370	12.626381
13.387874	601.032289	12.631399
13.277192	589.541116	12.636416
13.557968	596.513601	12.641434
13.398000	603.576441	12.646451
13.441865	591.650781	12.651469
13.340173	610.859170	12.656487
13.715515	586.153137	12.661504
13.456276	602.050170	12.666522
13.708246	601.969091	12.671539
13.621908	601.421128	12.676557
13.446811	601.433847	12.681575
13.718110	587.052854	12.686592
13.543642	594.722155	12.691610
13.541812	590.172035	12.696627
13.588887	588.687116	12.701645
12.881371	595.045182	12.706663
13.584915	577.187881	12.711680
13.567972	590.751193	12.716698
13.630691	600.002021	12.721715
13.657950	590.278316	12.726733
13.293204	605.326487	12.731751
13.867296	620.988606	12.736768
13.630768	639.783703	12.741786
13.868831	621.871912	12.746803
13.949718	633.886534	12.751821
13.943667	617.236811	12.756839
13.738111	607.916628	12.761856
13.542853	596.704512	12.766874
13.657346	621.575156	12.771891
13.901313	617.037740	12.776909
13.682132	620.390608	12.781927
14.115359	612.888061	12.786944
13.700086	618.078359	12.791962
13.802687	622.384669	12.796979
14.045044	617.418698	12.801997
13.999305	631.246773	12.807015
14.031980	610.128863	12.812032
13.822642	609.726981	12.817050
13.687183	609.947363	12.822067
13.952655	600.250310	12.827085
14.100647	622.194260	12.832103
14.033369	607.753778	12.837120
14.265490	601.079533	12.842138
14.015965	588.546928	12.847155
13.963430	592.901990	12.852173
13.813145	585.293481	12.857191
14.179491	592.075099	12.862208
13.883140	581.935124	12.867226
13.967923	612.600528	12.872243
14.324631	612.301997	12.877261
13.969545	623.873838	12.882279
14.338018	603.517941	12.887296
13.897687	604.267317	12.892314
14.034783	604.456532	12.897331
14.224910	605.606308	12.902349
13.803358	626.687754	12.907367
14.148740	614.533261	12.912384
14.059275	620.318952	12.917402
14.113128	616.854112	12.922419
14.272802	610.576672	12.927437
14.227342	625.576821	12.932455
14.551966	618.728465	12.937472
13.994316	617.710408	12.942490
14.103905	636.936852	12.947507
14.304370	606.480331	12.952525
13.943607	619.957711	12.957543
14.240733	626.391431	12.962560
14.044182	634.675851	12.967578
14.362272	632.944521	12.972595
14.338432	626.984431	12.977613
14.243525	617.737664	12.982631
14.132888	623.395886	12.987648
14.492398	620.127317	12.992666
14.189263	619.309161	12.997683
14.434189	619.379009	13.002701
14.106887	616.594905	13.007719
14.547738	621.456371	13.012736
14.527688	621.234666	13.017754
14.440066	624.545228	13.022771
14.395253	607.315661	13.027789
14.305352	620.138404	13.032807
14.302290	619.685803	13.037824
14.659917	622.141596	13.042842
14.473929	635.146426	13.047859
14.898551	622.827297	13.052877
14.498675	624.458234	13.057895
14.567886	618.769701	13.062912
14.368135	607.986452	13.067930
14.638911	629.795094	13.072947
14.853394	613.493865	13.077965
14.639520	625.384306	13.082983
14.671624	616.610709	13.088000
14.770703	598.829758	13.093018
14.312957	616.716562	13.098035
14.685398	612.351467	13.103053
14.788626	640.579299	13.108071
15.028004	623.228262	13.113088
14.879428	623.551671	13.118106
14.745558	607.013903	13.123123
14.936899	612.385274	13.128141
14.513861	612.438869	13.133159
14.731547	619.982270	13.138176
14.882571	613.737549	13.143194
14.707079	619.130479	13.148211
14.693609	617.228020	13.153229
14.985352	611.414155	13.158247
14.957606	620.300127	13.163264
14.754077	618.430454	13.168282
14.654454	627.807412	13.173299
14.863229	615.371540	13.178317
14.470302	621.779176	13.183335
15.092341	625.064070	13.188352
15.276164	641.826255	13.193370
15.128295	626.729764	13.198387
14.862491	618.770842	13.203405
14.424584	619.990656	13.208423
15.005869	626.353506	13.213440
15.170784	645.297663	13.218458
14.933024	651.606460	13.223475
15.060756	657.375361	13.228493
15.020320	646.588093	13.233511
15.091050	655.179834	13.238528
14.877286	643.626543	13.243546
14.920822	662.810407	13.248563
15.049565	653.654577	13.253581
15.119168	662.679563	13.258599
15.128688	648.264825	13.263616
15.043902	660.351816	13.268634
14.959978	652.000120	13.273651
15.159673	662.250911	13.278669
14.753630	656.642674	13.283687
14.972768	668.046051	13.288704
15.061953	648.994279	13.293722
14.915851	658.323932	13.298739
15.443571	641.898191	13.303757
15.209675	647.772507	13.308775
15.444989	640.407449	13.313792
15.291222	653.378533	13.318810
15.457518	645.038822	13.323827
15.391543	651.583529	13.328845
15.411947	647.462280	13.333863
15.156062	636.273242	13.338880
15.390529	651.236701	13.343898
15.393926	650.243510	13.348915
15.265182	641.883187	13.353933
15.267088	644.745118	13.358951
15.678251	656.328900	13.363968
15.852905	652.863669	13.368986
15.644846	653.391542	13.374003
15.834882	651.812833	13.379021
15.439238	642.562615	13.384039
15.488719	639.985262	13.389056
15.867622	643.051847	13.394074
15.334235	650.545021	13.399091
15.539147	637.585598	13.404109
15.227653	642.414555	13.409127
15.234788	659.036810	13.414144
15.433651	641.212555	13.419162
15.365444	661.022398	13.424179
15.576568	671.814273	13.429197
15.652308	667.713787	13.434215
15.714187	678.876006	13.439232
15.939316	678.014728	13.444250
15.764777	665.060722	13.449267
16.140592	654.312505	13.454285
15.979673	649.101933	13.459303
15.569622	649.564788	13.464320
15.845204	627.741928	13.469338
15.496809	657.550616	13.474355
15.803447	646.387671	13.479373
15.856896	630.464419	13.484391
15.603326	643.507780	13.489408
16.001927	633.629004	13.494426
15.632890	644.650657	13.499443
15.555384	624.981162	13.504461
15.834544	637.276225	13.509479
15.598682	633.056324	13.514496
15.746861	657.588773	13.519514
15.692220	670.237469	13.524531
16.241547	672.095008	13.529549
15.674718	672.860077	13.534567
16.016765	680.749493	13.539584
15.946767	657.994494	13.544602
15.774660	678.983818	13.549619
16.003798	661.843626	13.554637
15.972153	684.610447	13.559655
16.294231	670.461866	13.564672
16.131443	676.693635	13.569690
16.071774	674.957324	13.574707
16.144062	685.016743	13.579725
15.982836	662.732597	13.584743
16.052933	673.241660	13.589760
16.110673	668.353315	13.594778
15.989844	685.944624	13.599795
15.995771	664.538912	13.604813
16.003763	681.138319	13.609831
16.093630	668.068784	13.614848
16.296367	669.567273	13.619866
15.701142	687.528341	13.624883
16.166905	673.781588	13.629901
15.974782	682.369847	13.634919
15.921197	670.140532	13.639936
16.178801	672.687350	13.644954
16.148777	683.432002	13.649971
16.480979	683.281576	13.654989
16.138478	696.824393	13.660007
16.386294	685.823364	13.665024
16.305774	681.242041	13.670042
16.148693	692.218269	13.675059
16.434074	698.596201	13.680077
16.321628	686.267870	13.685095
16.535902	693.243419	13.690112
16.727405	684.979815	13.695130
16.500466	700.399197	13.700147
16.479570	665.745611	13.705165
16.640292	673.187458	13.710183
16.316573	658.591722	13.715200
16.678631	664.224486	13.720218
16.417124	678.450862	13.725235
16.486382	678.113636	13.730253
16.517345	663.733716	13.735271
16.553534	678.744335	13.740288
16.880749	670.846102	13.745306
16.473167	681.274900	13.750323
16.612183	661.339815	13.755341
17.106301	688.816216	13.760359
16.522015	672.023668	13.765376
16.700135	669.367783	13.770394
16.568674	665.440578	13.775411
16.496445	667.747788	13.780429
16.924394	669.846784	13.785447
16.722249	683.413528	13.790464
16.742855	661.768449	13.795482
16.575515	677.765105	13.800499
16.806678	677.328505	13.805517
16.749941	680.078315	13.810535
16.514491	689.900480	13.815552
17.222331	684.685561	13.820570
17.063518	682.979115	13.825587
16.920119	670.354416	13.830605
16.988158	674.733363	13.835623
16.910821	658.633224	13.840640
16.791997	656.285893	13.845658
16.629802	653.963736	13.850675
17.075227	674.863795	13.855693
17.103954	662.277175	13.860711
16.875839	681.074278	13.865728
16.937184	657.969216	13.870746
17.057472	682.990635	13.875763
17.052895	671.122512	13.880781
17.379248	684.619630	13.885799
16.857688	672.911134	13.890816
16.908640	666.192410	13.895834
16.649816	664.872965	13.900851
16.958972	686.568779	13.905869
16.797869	673.027267	13.910887
16.828568	690.297556	13.915904
17.347037	696.823434	13.920922
17.041545	675.335152	13.925939
16.954250	690.584242	13.930957
17.084117	673.349939	13.935975
17.120074	692.538931	13.940992
17.315516	680.858061	13.946010
17.285889	678.563487	13.951027
16.876014	684.813855	13.956045
16.781416	674.458339	13.961063
16.853494	693.126341	13.966080
17.233091	691.318519	13.971098
17.335337	718.166609	13.976115
17.371869	707.147641	13.981133
17.703206	710.862974	13.986151
17.425803	731.314603	13.991168
17.395307	712.161992	13.996186
17.145584	718.417689	14.001203
17.453578	712.858120	14.006221
17.596424	703.700618	14.011239
17.315522	707.134551	14.016256
17.419323	707.073629	14.021274
17.590159	704.614166	14.026291
17.168420	719.589999	14.031309
17.527272	700.109842	14.036327
17.422219	701.450101	14.041344
17.947111	701.115904	14.046362
17.471472	700.183769	14.051379
17.580532	712.881411	14.056397
17.461553	698.332391	14.061415
17.419978	714.779635	14.066432
17.194655	700.327104	14.071450
17.081653	707.333424	14.076467
17.252327	713.410324	14.081485
17.899200	720.535499	14.086503
18.010971	743.156397	14.091520
18.005453	733.032808	14.096538
17.778445	727.509691	14.101555
17.577936	717.232067	14.106573
17.889234	707.624493	14.111591
17.763023	700.844111	14.116608
17.916909	718.644618	14.121626
17.717226	706.796705	14.126643
17.776272	733.093643	14.131661
17.821973	714.878975	14.136679
18.109891	730.810391	14.141696
17.922943	725.814078	14.146714
18.064853	709.786384	14.151731
17.794607	715.567153	14.156749
18.016283	709.099553	14.161767
17.673413	704.383967	14.166784
17.849379	712.645538	14.171802
17.935337	733.880502	14.176819
17.866293	723.070750	14.181837
18.213060	737.208270	14.186855
18.006025	726.933292	14.191872
18.253215	724.855495	14.196890
18.264487	728.195492	14.201907
18.280836	738.829002	14.206925
18.168559	730.067294	14.211943
18.084586	748.572914	14.216960
18.353824	738.919037	14.221978
18.272687	725.385518	14.226995
18.275127	713.089445	14.232013
18.061391	719.344017	14.237031
18.121311	716.894420	14.242048
18.333228	726.488191	14.247066
18.091156	735.817711	14.252083
18.234543	729.987975	14.257101
18.467679	738.363702	14.262119
18.397870	742.105287	14.267136
18.077194	739.473372	14.272154
18.361462	740.528783	14.277171
18.600926	746.012393	14.282189
18.721493	743.190758	14.287207
18.537257	734.083256	14.292224
18.343935	707.495143	14.297242
18.427260	726.979911	14.302259
18.306475	723.455938	14.307277
18.501811	727.243836	14.312295
18.508992	727.532947	14.317312
18.583432	734.014141	14.322330
18.480562	733.958738	14.327347
18.671723	737.057155	14.332365
18.436076	721.982259	14.337383
18.630177	725.408153	14.342400
18.712007	728.026242	14.347418
18.408241	721.138221	14.352435
18.192080	732.980317	14.357453
18.858476	724.561559	14.362471
18.594474	736.186229	14.367488
18.599883	726.725724	14.372506
18.693397	735.874819	14.377523
18.449487	737.783948	14.382541
18.580363	723.167538	14.387559
18.675074	745.172130	14.392576
18.574088	729.825333	14.397594
18.760475	735.054984	14.402611
18.414582	736.192197	14.407629
18.704697	735.404308	14.412647
18.605291	735.201619	14.417664
18.647609	763.884806	14.422682
19.101833	756.792195	14.427699
18.878789	755.146539	14.432717
18.896176	748.263587	14.437735
19.162191	750.827528	14.442752
19.099730	761.293318	14.447770
19.117173	753.688003	14.452787
18.964589	767.731543	14.457805
18.938923	757.204484	14.462823
19.045858	773.761466	14.467840
19.263599	770.388571	14.472858
19.376757	755.195189	14.477875
19.010550	749.163416	14.482893
18.922976	741.238246	14.487911
18.956846	753.704022	14.492928
19.292792	757.454816	14.497946
19.402460	764.769059	14.502963
18.842722	742.339292	14.507981
19.252257	749.385918	14.512999
18.987020	743.749164	14.518016
19.291399	762.803849	14.523034
19.639199	740.623413	14.528051
19.243485	756.976905	14.533069
19.145903	751.778855	14.538087
19.314861	749.934300	14.543104
19.348295	764.336956	14.548122
19.436798	750.466897	14.553139
19.184055	760.657520	14.558157
19.234198	760.584899	14.563175
19.459544	755.255451	14.568192
19.090727	765.933248	14.573210
19.469188	768.723034	14.578227
19.089310	764.273025	14.583245
19.522717	768.314526	14.588263
19.677855	756.797994	14.593280
19.809478	754.444388	14.598298
19.658288	759.679651	14.603315
19.536138	766.832748	14.608333
19.403513	764.665489	14.613351
19.226500	751.311528	14.618368
19.112177	754.577330	14.623386
19.558075	755.318115	14.628403
19.438825	755.526276	14.633421
19.551155	750.197204	14.638439
19.270306	773.635295	14.643456
19.537144	772.402844	14.648474
19.900000	786.083340	14.653491
19.912947	794.219278	14.658509
19.885809	790.704512	14.663527
20.241176	798.194745	14.668544
19.681578	782.564426	14.673562
19.721941	767.654744	14.678579
19.409777	774.445056	14.683597
20.062674	779.152271	14.688615
19.837829	776.088380	14.693632
19.921975	786.039437	14.698650
20.063995	786.426805	14.703667
19.959537	785.269783	14.708685
19.751149	791.709181	14.713703
19.889429	772.252789	14.718720
20.089596	782.434703	14.723738
19.965470	790.987973	14.728755
19.653676	774.256651	14.733773
20.060364	793.273409	14.738791
19.762680	791.834226	14.743808
19.719627	780.227823	14.748826
19.870876	795.650534	14.753843
19.670969	779.992953	14.758861
19.801823	800.486725	14.763879
20.109304	800.812606	14.768896
20.157354	816.348725	14.773914
20.367983	804.939197	14.778931
20.315498	820.059467	14.783949
20.468730	813.982071	14.788967
20.602091	825.896366	14.793984
20.363555	799.251408	14.799002
20.244381	780.849396	14.804019
20.137577	789.942084	14.809037
20.208536	810.307221	14.814055
20.866414	805.557586	14.819072
20.324034	808.799282	14.824090
20.672990	785.825289	14.829107
20.256296	776.885869	14.834125
20.439455	783.819173	14.839143
20.371714	778.367724	14.844160
20.376661	791.929269	14.849178
20.433821	780.268520	14.854195
20.734809	814.349578	14.859213
20.679184	791.815864	14.864231
20.650768	792.150120	14.869248
20.372004	772.567519	14.874266
20.786048	783.628814	14.879283
20.550961	778.862330	14.884301
20.571415	774.666451	14.889319
20.940105	773.772391	14.894336
20.482467	777.122781	14.899354
20.480707	778.842725	14.904371
20.768000	799.872408	14.909389
20.758478	806.338775	14.914407
20.984128	787.795737	14.919424
20.780830	801.508899	14.924442
20.659242	783.575371	14.929459
20.807551	789.741311	14.934477
21.004717	794.266331	14.939495
20.889900	798.918482	14.944512
20.618058	818.909781	14.949530
20.882186	809.030483	14.954547
20.903501	800.661117	14.959565
20.759514	808.692814	14.964583
20.753334	799.572282	14.969600
21.110063	812.655150	14.974618
21.291821	792.056306	14.979635
20.997736	810.991308	14.984653
20.833872	810.875038	14.989671
21.163964	807.556876	14.994688
20.844118	808.763491	14.999706
20.946050	810.580840	15.004723
21.265785	797.443981	15.009741
21.136274	817.662382	15.014759
21.356366	801.163620	15.019776
21.202479	807.933302	15.024794
21.439339	801.424088	15.029811
21.325557	814.710469	15.034829
21.088139	814.431694	15.039847
21.285462	812.661065	15.044864
21.155474	817.976976	15.049882
21.347395	810.679622	15.054899
21.129802	804.279063	15.059917
21.227000	807.848122	15.064935
21.416565	797.423817	15.069952
21.186198	807.826465	15.074970
21.136819	795.918220	15.079987
21.035119	807.161686	15.085005
21.136586	813.192204	15.090023
21.635464	825.822667	15.095040
21.307772	842.423308	15.100058
21.208973	832.369878	15.105075
21.307122	841.833151	15.110093
21.469992	845.707919	15.115111
21.719696	845.250538	15.120128
21.673711	845.418844	15.125146
21.758307	837.470190	15.130163
21.789117	859.356995	15.135181
21.721685	843.870715	15.140199
21.748391	845.507832	15.145216
21.499289	831.044445	15.150234
21.770917	834.994225	15.155251
21.712924	847.618038	15.160269
21.520078	841.348281	15.165287
21.797189	834.759782	15.170304
21.841190	836.341003	15.175322
21.651176	829.606629	15.180339
21.688919	831.742285	15.185357
21.829786	836.111310	15.190375
22.046429	828.666296	15.195392
21.792526	840.927205	15.200410
21.890704	835.359363	15.205427
21.932685	831.709968	15.210445
21.690858	834.921188	15.215463
22.061720	830.101291	15.220480
21.866452	840.893828	15.225498
21.869513	828.612024	15.230515
21.725056	839.906171	15.235533
21.536100	843.686659	15.240551
21.911018	860.461784	15.245568
21.922304	859.316035	15.250586
22.120646	873.541973	15.255603
22.379098	860.787436	15.260621
22.320642	879.850470	15.265639
22.512881	876.856278	15.270656
22.509353	880.936536	15.275674
22.516148	869.056565	15.280691
22.652210	864.444806	15.285709
22.128295	874.457047	15.290727
22.585137	850.335197	15.295744
22.389801	844.648675	15.300762
22.255241	848.919063	15.305779
22.455932	841.090065	15.310797
21.981246	861.975254	15.315815
22.491537	844.880398	15.320832
22.404874	871.605586	15.325850
22.790332	856.151706	15.330867
22.703068	866.566563	15.335885
22.291613	864.988735	15.340903
22.523969	869.132073	15.345920
22.559547	864.024648	15.350938
22.742231	866.261522	15.355955
22.549414	858.351715	15.360973
22.460111	871.855992	15.365991
22.598366	871.892893	15.371008
22.730239	871.395550	15.376026
22.737517	866.118928	15.381043
22.852954	861.825066	15.386061
22.682367	876.674923	15.391079
22.687923	862.526025	15.396096
22.681707	874.824750	15.401114
22.469697	873.992405	15.406131
22.632808	876.547199	15.411149
22.475007	873.301090	15.416167
22.621390	873.140831	15.421184
22.535958	874.402684	15.426202
22.700989	870.859586	15.431219
22.791282	878.833908	15.436237
23.003943	891.455021	15.441255
22.742800	891.724222	15.446272
22.981262	911.489416	15.451290
23.018182	897.333630	15.456307
23.380254	895.632395	15.461325
23.289670	891.944869	15.466343
23.217964	880.699235	15.471360
23.130966	884.972106	15.476378
22.964108	883.010535	15.481395
23.464374	880.791018	15.486413
23.170289	891.749490	15.491431
23.349219	891.702424	15.496448
22.991882	887.525454	15.501466
22.987174	894.030915	15.506483
23.466544	903.062323	15.511501
23.087602	888.890447	15.516519
23.041842	883.615499	15.521536
23.085090	894.310601	15.526554
22.973860	898.627431	15.531571
23.245498	897.145715	15.536589
22.978398	897.191449	15.541607
23.000502	890.178453	15.546624
23.109637	904.042878	15.551642
23.310979	907.984810	15.556659
23.695739	915.913735	15.561677
23.406872	918.008520	15.566695
23.698428	918.555484	15.571712
23.378820	920.669715	15.576730
23.589918	907.279819	15.581747
23.817459	911.387458	15.586765
23.563406	925.785918	15.591783
23.776691	924.388136	15.596800
23.909450	915.215939	15.601818
23.642951	932.845381	15.606835
23.802896	907.035242	15.611853
23.853321	931.729426	15.616871
23.738805	905.628017	15.621888
24.030891	923.868014	15.626906
23.739493	914.808913	15.631923
23.889552	921.516804	15.636941
23.861248	921.361894	15.641959
24.063194	921.520126	15.646976
23.875233	923.789626	15.651994
23.912701	919.325804	15.657011
24.211341	939.435825	15.662029
23.693234	925.336409	15.667047
23.852537	903.368634	15.672064
23.965253	920.418594	15.677082
23.841741	909.221747	15.682099
24.004546	906.503015	15.687117
23.856676	926.473573	15.692135
24.008102	915.803585	15.697152
23.858923	906.825586	15.702170
23.898132	914.392625	15.707187
23.898146	900.031472	15.712205
23.791275	926.761867	15.717223
24.056029	933.480231	15.722240
24.290795	950.239551	15.727258
24.220411	953.892328	15.732275
24.469684	958.557470	15.737293
24.270767	959.886794	15.742311
24.405343	957.845878	15.747328
24.398532	950.956010	15.752346
24.257792	958.210373	15.757363
24.715151	939.690853	15.762381
24.413588	951.133553	15.767399
24.605470	951.235196	15.772416
24.668771	943.345110	15.777434
24.483469	940.310075	15.782451
24.934518	944.426347	15.787469
24.557156	949.538264	15.792487
24.629070	955.705776	15.797504
24.791962	943.927060	15.802522
24.466341	950.365923	15.807539
24.591013	942.923752	15.812557
24.538509	952.329530	15.817575
24.461431	946.673610	15.822592
24.585244	948.504777	15.827610
24.856377	937.906602	15.832627
24.924047	952.415954	15.837645
24.848183	955.442725	15.842663
24.930168	948.902463	15.847680
25.154325	940.920065	15.852698
24.824640	954.790535	15.857715
24.868364	949.778366	15.862733
24.766935	954.229778	15.867751
24.609018	960.722997	15.872768
24.399345	954.751373	15.877786
24.373449	953.180569	15.882803
24.530437	946.520952	15.887821
24.631038	976.506687	15.892839
25.004414	977.452335	15.897856
25.311881	980.683414	15.902874
25.007474	973.473317	15.907891
25.296283	988.710735	15.912909
25.105012	977.816204	15.917927
25.008907	985.999982	15.922944
25.504621	969.958616	15.927962
25.259710	977.515468	15.932979
25.594352	973.693690	15.937997
25.507175	965.480909	15.943015
25.239696	980.127247	15.948032
25.431639	974.715372	15.953050
25.196052	977.713241	15.958067
25.470446	958.987279	15.963085
25.494242	970.137407	15.968103
25.216512	977.992918	15.973120
25.536277	960.676923	15.978138
25.318806	983.739203	15.983155
25.646285	965.897745	15.988173
25.576731	966.378828	15.993191
25.363375	966.624093	15.998208
25.577458	967.848560	16.003226
25.189337	968.213727	16.008243
25.264064	986.062461	16.013261
25.493321	975.775436	16.018279
25.596761	982.008007	16.023296
25.677447	972.971023	16.028314
25.500131	987.808127	16.033331
25.903909	991.164695	16.038349
26.064884	995.047195	16.043367
25.816478	994.825336	16.048384
25.943030	977.200587	16.053402
25.309373	981.277083	16.058419
25.746860	997.973139	16.063437
25.871671	997.656640	16.068455
25.963890	993.466849	16.073472
25.904363	993.104847	16.078490
26.015024	999.240193	16.083507
26.266215	1000.365050	16.088525
26.033233	997.500342	16.093543
26.307963	982.731499	16.098560
26.370021	990.438465	16.103578
26.138641	986.740924	16.108595
26.028102	990.325560	16.113613
26.056471	990.083351	16.118631
26.020543	985.854026	16.123648
26.419319	992.325421	16.128666
26.155814	989.150679	16.133683
25.931652	975.791817	16.138701
26.131130	989.259692	16.143719
26.148237	993.324786	16.148736
26.272514	988.716217	16.153754
26.204094	1000.553096	16.158771
26.125108	998.422990	16.163789
26.503785	989.748265	16.168807
26.233782	982.705861	16.173824
26.568001	1000.892148	16.178842
26.345274	1012.145728	16.183859
26.672538	1014.722028	16.188877
26.548220	1014.947955	16.193895
26.485817	1032.655960	16.198912
26.927494	1017.177376	16.203930
26.728057	1019.929870	16.208947
26.741903	985.567383	16.213965
26.492750	999.230144	16.218983
26.342927	1007.169723	16.224000
26.717652	1005.758342	16.229018
26.559672	1029.563334	16.234035
26.633984	1022.211317	16.239053
26.968601	1027.359402	16.244071
26.746495	1017.262956	16.249088
26.860157	1024.592013	16.254106
26.705436	1028.789916	16.259123
26.623056	1021.597619	16.264141
26.805208	1031.980956	16.269159
26.631014	1025.505039	16.274176
26.761289	1024.881116	16.279194
26.825319	1029.282279	16.284211
26.775170	1036.395952	16.289229
26.994789	1042.307847	16.294247
26.923769	1044.053435	16.299264
27.280492	1049.510890	16.304282
27.071559	1050.705098	16.309299
27.302724	1043.908112	16.314317
27.321073	1055.976304	16.319335
27.426488	1049.014708	16.324352
27.719541	1036.143804	16.329370
27.416782	1036.634103	16.334387
27.184645	1021.326793	16.339405
27.437341	1019.854789	16.344423
27.043934	1036.195798	16.349440
27.505708	1036.508191	16.354458
27.430831	1033.573265	16.359475
27.578027	1051.639277	16.364493
27.830423	1049.027929	16.369511
27.443503	1053.307212	16.374528
27.374015	1032.641423	16.379546
27.354012	1046.375189	16.384563
27.689491	1049.263350	16.389581
27.674793	1041.248145	16.394599
27.296262	1053.225857	16.399616
27.712184	1045.841681	16.404634
27.444281	1047.413163	16.409651
27.576990	1043.421441	16.414669
27.693944	1038.748631	16.419687
27.606446	1048.239365	16.424704
27.442729	1040.237176	16.429722
27.445664	1048.236945	16.434739
27.462465	1049.257661	16.439757
27.863253	1059.064465	16.444775
27.898337	1076.710064	16.449792
28.142001	1068.514485	16.454810
28.060926	1076.883775	16.459827
28.176804	1076.072806	16.464845
27.991378	1073.855974	16.469863
28.099980	1077.054304	16.474880
28.538377	1059.535762	16.479898
27.959885	1053.679663	16.484915
27.875160	1038.558849	16.489933
28.363444	1061.211871	16.494951
28.259285	1067.565279	16.499968
28.300055	1068.623069	16.504986
28.280577	1054.138350	16.510003
27.927965	1050.441442	16.515021
28.558562	1055.498902	16.520039
28.406846	1075.869013	16.525056
28.490907	1066.185607	16.530074
28.340202	1068.442476	16.535091
28.439507	1041.399811	16.540109
28.575608	1042.794713	16.545127
28.335276	1035.117415	16.550144
28.386343	1043.533337	16.555162
28.605064	1058.144470	16.560179
28.509624	1067.231016	16.565197
28.693283	1077.247491	16.570215
28.614532	1072.529176	16.575232
28.307546	1080.698654	16.580250
28.591167	1062.985758	16.585267
28.436261	1079.580242	16.590285
28.646768	1058.165066	16.595303
28.488744	1082.034994	16.600320
28.572195	1055.735495	16.605338
28.533290	1074.192437	16.610355
28.467724	1060.019193	16.615373
28.364196	1057.763540	16.620391
28.423887	1073.204515	16.625408
28.645507	1073.855639	16.630426
28.902010	1074.591036	16.635443
29.069462	1085.565478	16.640461
28.963625	1071.501314	16.645479
29.080266	1081.970985	16.650496
29.018955	1081.759732	16.655514
29.088190	1088.162035	16.660531
28.849136	1077.589526	16.665549
29.193950	1087.702870	16.670567
29.532819	1080.038272	16.675584
29.435358	1084.852070	16.680602
29.084468	1078.861323	16.685619
29.198529	1099.618643	16.690637
29.395325	1084.948189	16.695655
29.301299	1097.632087	16.700672
29.433138	1089.540193	16.705690
29.671489	1087.803589	16.710707
29.323079	1100.695925	16.715725
29.512473	1091.500291	16.720743
29.314006	1095.648466	16.725760
29.434923	1081.781213	16.730778
29.504206	1096.401433	16.735795
28.995494	1098.338327	16.740813
29.371699	1088.314374	16.745831
29.001080	1092.445143	16.750848
28.952514	1100.348652	16.755866
29.546291	1121.976106	16.760883
29.630140	1115.164368	16.765901
29.934337	1125.592447	16.770919
29.761730	1119.258320	16.775936
29.974399	1112.108736	16.780954
30.044042	1098.121331	16.785971
29.531602	1109.530215	16.790989
30.067092	1106.267002	16.796007
30.224870	1111.172159	16.801024
30.075149	1103.963990	16.806042
29.876855	1114.864183	16.811059
29.727469	1113.208086	16.816077
29.916683	1108.430716	16.821095
29.884720	1109.354402	16.826112
29.741285	1099.638409	16.831130
29.754790	1106.290816	16.836147
29.692313	1092.858292	16.841165
29.713269	1110.545626	16.846183
30.045351	1115.716005	16.851200
30.145612	1121.348119	16.856218
30.295020	1129.370171	16.861235
30.090643	1130.990697	16.866253
30.137845	1146.220277	16.871271
30.432513	1141.431670	16.876288
30.823785	1142.387360	16.881306
30.685041	1123.329072	16.886323
30.551487	1131.486940	16.891341
30.723786	1102.912383	16.896359
30.344513	1107.713226	16.901376
30.288909	1095.664865	16.906394
30.670548	1108.983087	16.911411
30.710872	1104.658962	16.916429
30.592065	1090.791956	16.921447
30.315806	1083.969877	16.926464
30.564188	1121.249612	16.931482
30.613321	1115.697054	16.936499
30.632832	1116.119929	16.941517
30.905507	1119.143846	16.946535
30.726248	1131.814993	16.951552
30.719933	1115.881039	16.956570
30.865401	1133.381326	16.961587
30.694209	1132.553538	16.966605
31.019106	1135.857933	16.971623
30.839657	1122.987007	16.976640
30.800183	1136.884960	16.981658
31.115435	1122.594505	16.986675
30.782934	1138.165992	16.991693
30.798116	1133.349182	16.996711
30.859927	1121.024274	17.001728
30.970119	1141.267548	17.006746
31.174649	1126.998832	17.011763
30.979407	1134.548930	17.016781
31.092808	1120.910488	17.021799
31.026420	1129.985579	17.026816
30.786212	1134.870215	17.031834
31.208942	1145.564972	17.036851
31.260663	1164.792000	17.041869
31.500652	1155.793922	17.046887
31.606346	1165.632635	17.051904
31.567462	1156.952133	17.056922
31.487067	1162.693823	17.061939
31.438636	1150.618649	17.066957
31.517698	1158.396298	17.071975
31.654754	1138.894870	17.076992
31.396264	1145.967253	17.082010
31.876856	1146.166920	17.087027
31.700307	1141.656236	17.092045
31.653446	1152.395339	17.097063
31.514961	1153.352769	17.102080
31.817109	1148.714758	17.107098
31.965922	1151.261432	17.112115
31.889726	1152.236613	17.117133
31.683664	1142.056349	17.122151
31.683915	1146.787400	17.127168
31.626196	1145.916357	17.132186
32.063800	1139.179877	17.137203
31.621615	1152.558213	17.142221
31.487789	1145.181393	17.147239
31.692356	1155.094389	17.152256
31.717799	1151.313726	17.157274
31.888105	1173.593578	17.162291
31.764396	1178.951775	17.167309
31.982227	1192.046705	17.172327
32.054939	1173.729806	17.177344
31.728714	1201.154158	17.182362
32.226243	1183.984479	17.187379
32.279702	1185.909762	17.192397
32.379983	1190.875419	17.197415
32.510326	1187.604750	17.202432
32.284180	1177.558262	17.207450
32.386428	1192.618888	17.212467
32.310409	1185.990293	17.217485
32.493287	1193.050769	17.222503
32.602680	1177.194654	17.227520
32.346021	1193.927407	17.232538
32.624297	1183.366554	17.237555
32.360685	1186.079202	17.242573
32.579816	1180.943602	17.247591
32.521704	1170.461867	17.252608
32.240785	1175.160277	17.257626
32.895200	1171.260612	17.262643
32.513459	1187.128112	17.267661
32.567957	1194.813897	17.272679
32.561298	1198.534136	17.277696
32.889476	1219.196700	17.282714
33.081268	1193.298453	17.287731
32.841237	1216.088300	17.292749
33.250814	1208.450036	17.297767
33.426021	1212.784367	17.302784
33.099052	1195.092024	17.307802
33.124434	1184.388655	17.312819
33.047667	1182.081328	17.317837
32.896879	1178.398761	17.322855
33.011476	1178.896258	17.327872
33.109963	1190.088620	17.332890
33.387606	1193.244180	17.337907
33.343580	1194.904832	17.342925
33.162859	1184.914106	17.347943
33.310537	1189.819580	17.352960
33.321805	1202.094916	17.357978
33.561319	1202.431054	17.362995
33.132184	1199.858211	17.368013
33.728701	1198.541332	17.373031
33.788036	1187.736112	17.378048
33.135185	1180.990491	17.383066
33.546994	1178.581957	17.388083
33.411396	1194.616319	17.393101
33.581043	1192.705471	17.398119
33.680650	1204.433558	17.403136
33.292173	1196.701938	17.408154
33.797291	1195.466290	17.413171
33.446415	1194.542433	17.418189
33.918918	1188.191413	17.423207
33.540195	1198.208602	17.428224
33.334090	1197.658269	17.433242
33.769574	1201.155083	17.438259
34.079261	1199.449386	17.443277
33.839236	1207.878865	17.448295
34.420387	1192.534598	17.453312
33.749430	1219.596561	17.458330
33.800353	1199.213924	17.463347
33.712769	1201.815615	17.468365
33.886290	1203.921013	17.473383
33.814827	1198.041879	17.478400
33.724302	1224.232323	17.483418
33.959930	1223.442493	17.488435
34.014591	1237.258854	17.493453
34.115909	1219.289258	17.498471
34.464769	1228.709863	17.503488
34.345217	1222.344588	17.508506
34.461170	1225.889686	17.513523
34.067803	1220.144529	17.518541
34.392249	1205.644160	17.523559
34.608898	1221.812323	17.528576
34.575463	1215.716416	17.533594
34.561486	1205.970105	17.538611
34.680670	1219.289777	17.543629
34.379542	1224.945653	17.548647
34.779175	1213.246281	17.553664
34.724116	1216.634051	17.558682
34.701326	1219.283093	17.563699
34.682394	1206.520480	17.568717
34.804207	1223.829845	17.573735
34.987868	1210.254695	17.578752
34.990432	1223.281707	17.583770
34.937600	1218.830852	17.588787
34.993098	1212.563985	17.593805
34.838303	1220.052829	17.598823
35.020644	1201.461145	17.603840
35.008778	1199.996731	17.608858
35.019824	1214.204344	17.613875
34.785864	1205.468769	17.618893
34.759477	1220.265018	17.623911
34.935043	1207.474395	17.628928
34.851060	1217.056462	17.633946
34.884830	1214.052870	17.638963
35.242742	1233.996335	17.643981
35.078351	1241.036484	17.648999
35.355918	1258.343766	17.654016
35.086754	1254.473408	17.659034
35.594685	1255.360626	17.664051
35.362237	1243.376798	17.669069
35.167545	1261.886378	17.674087
35.524813	1249.959190	17.679104
35.511857	1249.190266	17.684122
35.589035	1239.414798	17.689139
35.598482	1249.665837	17.694157
35.624653	1241.593195	17.699175
35.809275	1243.146988	17.704192
35.547102	1241.119545	17.709210
35.765454	1240.996787	17.714227
35.778233	1236.312989	17.719245
35.565957	1244.152308	17.724263
35.698268	1231.206154	17.729280
35.612124	1242.467245	17.734298
35.779336	1232.767729	17.739315
36.118495	1237.756314	17.744333
35.820451	1235.228026	17.749351
35.926126	1235.533539	17.754368
35.595819	1238.517689	17.759386
36.019100	1253.815907	17.764403
36.279548	1265.810701	17.769421
35.877753	1281.757482	17.774439
36.429984	1258.579641	17.779456
36.126678	1276.141462	17.784474
35.861644	1262.184613	17.789491
35.815670	1262.650098	17.794509
35.956912	1262.959771	17.799527
35.791017	1276.423236	17.804544
36.057137	1278.228957	17.809562
36.161637	1295.940682	17.814579
36.516787	1291.691025	17.819597
36.334972	1305.676025	17.824615
36.879951	1292.531042	17.829632
36.763984	1309.113337	17.834650
36.615085	1298.738523	17.839667
36.805603	1307.941207	17.844685
36.854077	1293.822899	17.849703
36.960739	1303.475363	17.854720
36.933895	1278.463404	17.859738
36.902453	1274.129934	17.864755
37.132466	1254.746529	17.869773
36.896273	1269.480964	17.874791
36.982612	1247.421233	17.879808
36.793312	1260.947003	17.884826
36.732838	1255.636178	17.889843
36.806496	1259.804865	17.894861
36.718997	1284.599167	17.899879
37.379198	1282.799816	17.904896
37.222993	1280.941527	17.909914
36.923106	1287.580365	17.914931
37.305183	1289.414454	17.919949
37.163538	1287.818757	17.924967
37.219553	1292.569274	17.929984
37.300960	1292.014033	17.935002
37.285840	1298.987620	17.940019
37.035328	1287.581220	17.945037
37.567036	1294.865826	17.950055
37.601297	1285.699155	17.955072
37.159915	1288.910581	17.960090
37.345251	1274.075145	17.965107
37.527434	1280.602630	17.970125
37.202266	1290.146173	17.975143
37.450993	1278.764537	17.980160
37.536639	1287.731151	17.985178
37.491136	1288.438926	17.990195
37.671046	1276.404148	17.995213
37.490466	1297.127670	18.000231
37.780395	1301.449563	18.005248
37.853493	1302.960388	18.010266
37.810388	1325.866346	18.015283
37.893582	1315.268267	18.020301
37.729312	1318.613490	18.025319
38.050375	1314.671459	18.030336
38.101290	1323.323334	18.035354
38.051787	1308.086517	18.040371
37.895239	1314.400565	18.045389
37.958630	1310.526898	18.050407
38.059013	1321.722291	18.055424
38.203841	1306.078838	18.060442
37.870759	1317.407066	18.065459
37.838839	1314.435368	18.070477
38.141403	1333.101291	18.075495
38.504019	1338.913113	18.080512
38.427237	1351.932288	18.085530
38.303441	1338.280303	18.090547
38.642702	1345.992613	18.095565
38.655439	1354.129474	18.100583
38.567599	1351.693566	18.105600
38.457077	1339.295605	18.110618
38.631616	1346.243776	18.115635
39.041308	1334.306187	18.120653
38.743836	1336.963151	18.125671
38.957355	1332.688375	18.130688
38.970440	1343.486588	18.135706
38.939167	1350.377848	18.140723
39.039667	1339.710470	18.145741
38.691604	1324.622952	18.150759
38.747504	1341.668405	18.155776
38.764040	1326.828045	18.160794
38.749569	1343.342434	18.165811
39.071088	1329.781692	18.170829
38.785396	1342.016077	18.175847
38.717609	1334.710517	18.180864
38.873259	1331.371575	18.185882
38.618454	1333.800966	18.190899
39.223018	1346.788625	18.195917
38.971930	1362.082278	18.200935
39.291765	1368.933827	18.205952
39.482856	1360.690593	18.210970
39.119158	1371.204907	18.215987
39.563705	1360.035482	18.221005
39.191331	1365.517201	18.226023
39.395802	1362.513218	18.231040
39.574978	1374.555183	18.236058
39.221588	1358.926997	18.241075
39.466170	1370.412995	18.246093
39.527854	1361.792020	18.251111
39.560522	1372.578850	18.256128
39.860604	1379.064458	18.261146
39.685472	1402.690030	18.266163
40.261182	1384.138510	18.271181
40.013920	1378.325752	18.276199
39.963027	1364.555814	18.281216
39.816103	1338.745572	18.286234
39.743021	1370.713794	18.291251
39.928367	1352.040642	18.296269
40.014115	1385.411958	18.301287
40.197776	1373.757601	18.306304
40.358462	1389.897600	18.311322
40.206179	1397.082736	18.316339
40.373201	1393.735701	18.321357
40.241477	1394.644696	18.326375
40.222995	1396.506910	18.331392
40.537531	1401.504243	18.336410
40.555207	1387.808367	18.341427
40.433473	1365.607398	18.346445
40.306406	1383.697182	18.351463
40.367598	1371.038881	18.356480
40.763067	1389.905024	18.361498
40.298709	1377.210366	18.366515
40.486576	1376.085288	18.371533
40.396939	1378.603803	18.376551
40.304374	1383.005951	18.381568
40.508245	1378.044621	18.386586
40.125761	1373.965252	18.391603
40.400045	1377.125048	18.396621
40.601568	1401.552161	18.401639
41.251085	1407.032702	18.406656
41.003503	1416.373091	18.411674
40.811348	1412.531591	18.416691
41.170791	1422.202186	18.421709
41.060266	1405.660779	18.426727
40.874969	1410.881333	18.431744
41.052026	1401.260971	18.436762
41.075222	1429.270860	18.441779
41.290360	1411.064658	18.446797
41.196158	1413.164339	18.451815
40.820554	1414.923599	18.456832
41.106679	1396.635423	18.461850
40.916827	1405.250673	18.466867
41.652957	1423.969736	18.471885
41.809178	1443.687216	18.476903
41.337863	1428.134144	18.481920
41.870008	1438.922911	18.486938
41.648178	1419.129131	18.491955
41.787333	1433.770501	18.496973
41.743661	1422.453315	18.501991
41.487897	1425.692743	18.507008
41.932678	1425.339301	18.512026
41.792994	1436.393878	18.517043
42.030232	1447.212295	18.522061
42.185403	1433.760528	18.527079
41.974002	1430.375354	18.532096
41.748452	1410.795441	18.537114
41.934799	1422.182562	18.542131
42.043794	1436.277955	18.547149
41.892899	1439.762991	18.552167
42.125857	1442.714715	18.557184
42.134938	1434.067164	18.562202
42.006658	1445.383487	18.567219
41.858948	1441.808887	18.572237
42.120661	1437.230709	18.577255
42.161470	1435.682879	18.582272
42.441798	1440.215015	18.587290
41.910891	1435.539130	18.592307
42.092361	1440.602058	18.597325
42.394460	1435.427176	18.602343
42.562866	1458.051483	18.607360
42.830919	1445.144612	18.612378
42.351273	1446.036416	18.617395
42.549371	1448.868339	18.622413
42.733570	1460.002453	18.627431
42.530718	1447.170939	18.632448
42.830754	1451.501045	18.637466
42.711777	1451.590592	18.642483
42.982001	1440.178715	18.647501
42.677906	1447.119827	18.652519
42.472706	1457.937760	18.657536
42.872309	1431.959797	18.662554
42.781180	1445.665921	18.667571
42.916417	1452.531679	18.672589
43.115913	1463.450714	18.677607
42.955836	1466.494848	18.682624
43.202649	1471.098856	18.687642
43.368575	1483.769242	18.692659
43.358172	1474.984366	18.697677
43.477957	1475.922457	18.702695
43.270233	1466.963939	18.707712
43.629329	1466.324523	18.712730
43.511343	1466.507489	18.717747
43.493734	1480.759446	18.722765
43.714924	1487.192895	18.727783
43.648475	1476.899000	18.732800
43.729396	1472.938555	18.737818
43.543413	1471.541660	18.742835
43.732710	1473.358133	18.747853
43.974559	1474.962421	18.752871
43.587497	1471.749150	18.757888
44.024709	1469.796118	18.762906
43.690616	1484.871671	18.767923
43.809426	1471.341548	18.772941
43.984651	1465.140208	18.777959
43.811061	1481.641089	18.782976
44.151468	1457.017463	18.787994
43.746617	1482.669867	18.793011
43.542860	1466.742787	18.798029
44.017293	1485.572284	18.803047
44.188961	1486.355180	18.808064
44.157527	1497.954785	18.813082
44.081754	1480.738108	18.818099
44.071153	1495.215152	18.823117
44.512551	1499.360922	18.828135
44.055428	1496.098409	18.833152
44.352536	1500.085385	18.838170
44.404153	1489.817433	18.843187
44.683626	1508.724246	18.848205
44.859222	1512.486279	18.853223
44.629906	1510.087305	18.858240
44.756656	1512.593798	18.863258
44.778557	1523.431126	18.868275
45.047878	1514.665834	18.873293
44.962966	1515.442717	18.878311
44.850990	1518.636950	18.883328
44.998853	1516.580087	18.888346
44.905520	1531.710270	18.893363
45.098216	1529.017487	18.898381
45.377237	1526.924385	18.903399
45.413036	1535.840142	18.908416
45.740204	1508.954921	18.913434
45.280697	1480.279191	18.918451
45.239306	1478.898255	18.923469
45.411261	1483.712429	18.928487
44.950443	1476.796289	18.933504
45.099618	1480.406315	18.938522
45.320885	1488.641043	18.943539
44.972662	1504.393020	18.948557
45.387593	1508.138428	18.953575
45.393386	1522.652938	18.958592
45.774466	1508.165558	18.963610
45.530466	1514.300185	18.968627
45.027913	1509.704416	18.973645
45.551881	1511.532207	18.978663
45.534659	1507.975586	18.983680
45.533698	1524.111344	18.988698
45.700118	1536.674235	18.993715
45.724465	1553.054214	18.998733
46.031780	1542.856252	19.003751
45.877706	1554.341549	19.008768
46.224679	1544.970422	19.013786
46.040795	1547.085531	19.018803
46.036847	1545.741109	19.023821
45.992975	1553.860566	19.028839
46.105316	1543.755244	19.033856
46.291392	1557.792155	19.038874
46.312905	1539.876208	19.043891
46.032840	1542.929853	19.048909
46.462173	1543.038020	19.053927
46.481216	1558.523793	19.058944
46.780132	1568.389190	19.063962
46.386861	1556.395479	19.068979
46.715301	1561.073212	19.073997
46.901113	1561.478064	19.079015
46.670452	1557.605693	19.084032
47.249117	1555.021528	19.089050
46.641398	1541.050399	19.094067
46.883202	1551.658928	19.099085
47.078289	1555.870314	19.104103
46.794681	1563.652306	19.109120
47.096659	1549.424267	19.114138
47.161495	1558.037073	19.119155
47.168700	1552.869652	19.124173
47.394537	1548.444091	19.129191
47.025033	1571.238444	19.134208
47.220372	1555.614731	19.139226
47.166432	1561.446371	19.144243
47.182296	1553.366510	19.149261
47.451687	1554.069001	19.154279
47.150874	1553.793306	19.159296
47.451542	1562.918505	19.164314
47.326232	1548.359782	19.169331
46.931393	1559.470488	19.174349
46.925766	1545.680606	19.179367
47.434346	1560.945257	19.184384
47.277485	1583.667783	19.189402
47.641306	1575.243461	19.194419
47.373428	1586.298370	19.199437
47.688403	1577.574701	19.204455
47.844405	1594.444673	19.209472
47.613256	1590.034887	19.214490
48.081547	1595.543970	19.219507
47.940179	1607.548852	19.224525
48.191397	1602.619971	19.229543
48.155302	1619.047206	19.234560
48.393578	1620.971327	19.239578
48.855585	1611.767332	19.244595
48.501373	1599.905194	19.249613
48.400506	1570.955505	19.254631
48.322351	1570.740829	19.259648
48.314839	1571.925702	19.264666
48.448429	1569.492923	19.269683
48.304248	1568.856472	19.274701
48.570516	1580.991075	19.279719
48.212159	1574.135895	19.284736
48.681025	1589.301156	19.289754
48.768618	1590.224794	19.294771
48.156322	1603.590991	19.299789
49.004126	1606.877470	19.304807
48.955608	1615.975383	19.309824
48.970545	1600.049614	19.314842
48.987730	1607.827680	19.319859
49.174782	1608.271593	19.324877
49.141878	1599.453068	19.329895
48.920523	1605.715163	19.334912
48.740386	1596.088858	19.339930
49.105460	1609.053045	19.344947
48.760189	1605.330875	19.349965
49.179496	1594.488613	19.354983
49.204124	1605.659240	19.360000
49.426542	1601.313445	19.365018
49.524133	1600.164990	19.370035
49.112688	1605.812272	19.375053
49.275085	1597.685342	19.380071
49.353388	1606.943948	19.385088
49.622100	1614.741660	19.390106
49.709008	1623.081323	19.395123
49.621903	1626.220101	19.400141
49.823553	1626.553258	19.405159
49.917877	1627.166203	19.410176
49.623157	1628.176246	19.415194
49.842340	1623.948770	19.420211
49.618290	1630.146766	19.425229
49.681026	1622.169534	19.430247
49.715193	1625.905173	19.435264
49.315901	1630.997025	19.440282
50.055873	1635.975794	19.445299
50.018065	1648.619859	19.450317
50.272675	1643.977256	19.455335
50.400419	1659.016612	19.460352
50.504847	1657.395956	19.465370
50.462876	1643.816970	19.470387
50.014177	1654.238951	19.475405
50.220873	1649.478010	19.480423
50.216799	1649.918869	19.485440
50.577224	1651.433025	19.490458
50.659911	1677.013650	19.495475
50.693641	1680.136013	19.500493
51.165278	1671.020727	19.505511
51.478871	1660.891616	19.510528
51.270156	1641.140548	19.515546
51.566682	1630.240418	19.520563
51.194510	1627.404004	19.525581
51.549410	1638.090439	19.530599
51.495369	1638.492616	19.535616
50.924018	1633.181651	19.540634
51.409253	1628.182010	19.545651
51.221687	1619.443057	19.550669
51.178732	1632.230450	19.555687
51.207280	1627.894938	19.560704
51.150042	1643.507356	19.565722
51.372207	1616.267326	19.570739
51.152248	1634.442624	19.575757
51.491086	1619.870897	19.580775
51.584991	1629.571631	19.585792
51.083018	1614.024024	19.590810
51.777134	1610.672991	19.595827
51.431690	1626.501390	19.600845
51.584775	1641.576494	19.605863
51.706851	1645.590761	19.610880
51.456291	1667.234333	19.615898
51.451432	1648.930668	19.620915
51.921525	1661.932160	19.625933
51.608544	1642.924651	19.630951
51.624652	1665.410686	19.635968
51.498053	1658.541967	19.640986
51.997599	1670.451220	19.646003
52.013375	1685.627192	19.651021
52.357002	1683.577024	19.656039
52.504145	1684.214505	19.661056
52.043533	1677.117172	19.666074
52.520896	1693.935330	19.671091
52.502034	1685.367535	19.676109
52.586738	1680.785078	19.681127
52.784180	1665.331934	19.686144
52.531590	1678.567410	19.691162
52.908280	1670.435043	19.696179
52.565218	1682.969475	19.701197
52.788622	1665.814545	19.706215
52.781519	1676.267876	19.711232
52.535824	1677.142582	19.716250
52.689871	1670.987760	19.721267
52.722272	1677.240228	19.726285
53.215812	1696.819631	19.731303
53.355021	1707.248805	19.736320
53.048400	1713.205609	19.741338
53.158816	1714.953174	19.746355
53.123927	1702.123900	19.751373
52.982746	1697.254028	19.756391
53.303081	1709.606132	19.761408
53.547426	1696.285236	19.766426
53.198560	1712.669001	19.771443
53.397191	1704.823273	19.776461
53.385632	1709.111755	19.781479
53.750784	1693.745807	19.786496
53.127607	1716.874560	19.791514
53.525564	1706.343267	19.796531
53.772693	1739.675500	19.801549
54.040456	1747.962318	19.806567
54.088936	1726.025553	19.811584
53.825236	1735.361615	19.816602
54.164712	1723.338694	19.821619
54.236091	1746.920222	19.826637
54.424422	1728.211382	19.831655
54.138012	1734.320434	19.836672
53.757826	1727.829449	19.841690
54.307384	1746.898085	19.846707
53.933779	1730.595726	19.851725
53.734367	1737.407880	19.856743
54.078418	1754.813378	19.861760
53.907841	1761.470610	19.866778
54.255692	1775.351878	19.871795
54.853759	1762.226360	19.876813
54.807935	1768.675122	19.881831
55.079270	1761.346972	19.886848
54.806727	1770.204492	19.891866
55.226110	1750.656909	19.896883
55.125091	1757.491190	19.901901
55.307640	1755.198786	19.906919
55.406014	1757.335082	19.911936
55.184362	1752.553082	19.916954
55.381949	1751.077620	19.921971
55.128248	1746.375411	19.926989
55.088683	1752.430787	19.932007
55.293885	1750.102757	19.937024
55.184288	1761.800305	19.942042
55.139244	1752.875156	19.947059
54.924869	1752.058208	19.952077
55.052155	1746.746100	19.957095
55.238265	1756.600739	19.962112
55.187718	1755.853057	19.967130
55.411489	1761.748112	19.972147
55.481975	1769.299975	19.977165
55.449444	1789.257123	19.982183
55.609265	1791.261541	19.987200
55.323474	1795.791193	19.992218
55.716142	1790.568948	19.997235
55.795293	1781.166163	20.002253
55.721622	1783.560573	20.007271
56.205980	1785.969835	20.012288
56.072709	1789.203856	20.017306
56.198774	1816.521402	20.022323
56.473538	1805.276484	20.027341
56.360957	1810.013496	20.032359
56.609037	1793.750827	20.037376
56.047807	1800.508944	20.042394
56.389475	1791.390267	20.047411
56.407418	1811.098598	20.052429
56.187981	1795.144047	20.057447
56.624818	1785.834385	20.062464
56.686859	1806.660600	20.067482
56.627678	1791.405711	20.072499
56.663580	1797.777016	20.077517
56.564920	1798.165216	20.082535
56.730694	1796.733878	20.087552
56.748816	1826.375825	20.092570
57.143176	1820.029981	20.097587
57.207774	1816.412336	20.102605
57.161761	1831.438753	20.107623
57.576951	1821.441636	20.112640
57.220509	1830.633466	20.117658
57.364791	1834.815832	20.122675
57.526593	1826.326153	20.127693
57.429551	1833.990854	20.132711
57.819658	1819.737963	20.137728
57.466851	1831.873415	20.142746
57.692901	1823.316734	20.147763
57.555194	1830.240362	20.152781
57.408973	1812.430246	20.157799
57.772492	1822.835421	20.162816
57.420851	1811.674823	20.167834
57.794829	1827.442012	20.172851
57.939852	1807.857329	20.177869
57.524205	1826.059286	20.182887
57.979512	1802.482845	20.187904
57.797417	1842.693590	20.192922
57.862135	1832.834780	20.197939
58.054662	1853.701787	20.202957
58.052633	1846.737510	20.207975
58.030042	1847.964653	20.212992
58.041734	1847.801550	20.218010
58.081214	1841.893995	20.223027
58.216973	1852.612169	20.228045
58.316851	1873.681092	20.233063
58.525905	1878.756633	20.238080
58.699098	1879.164367	20.243098
58.551772	1878.175831	20.248115
58.682528	1882.600164	20.253133
58.615629	1876.487480	20.258151
58.757701	1882.902287	20.263168
58.897106	1890.648589	20.268186
58.838315	1899.999601	20.273203
59.198992	1910.248739	20.278221
59.027914	1906.974391	20.283239
59.237129	1916.911421	20.288256
59.282647	1904.407309	20.293274
59.345039	1908.597913	20.298291
59.617219	1909.728820	20.303309
59.419128	1896.827945	20.308327
59.623266	1891.175097	20.313344
59.496441	1910.792835	20.318362
59.673106	1900.679108	20.323379
59.833555	1895.518132	20.328397
59.862967	1901.198752	20.333415
59.980180	1902.861078	20.338432
60.085340	1896.472459	20.343450
59.841106	1904.047760	20.348467
60.007417	1891.122492	20.353485
59.914278	1904.831818	20.358503
60.084723	1891.223907	20.363520
60.043595	1891.832678	20.368538
60.194649	1894.210044	20.373555
60.232831	1875.438058	20.378573
59.832359	1887.065681	20.383591
59.828394	1877.134940	20.388608
60.027784	1892.711009	20.393626
59.966208	1916.486194	20.398643
60.356950	1909.253280	20.403661
60.302492	1927.188130	20.408679
60.656073	1929.375960	20.413696
60.665094	1923.372343	20.418714
60.812198	1930.299236	20.423731
60.812944	1923.597509	20.428749
60.768135	1945.728931	20.433767
61.341413	1936.387676	20.438784
61.019875	1956.313780	20.443802
61.243948	1952.194639	20.448819
61.388715	1949.585969	20.453837
61.214649	1958.171661	20.458855
61.377375	1938.400258	20.463872
61.328079	1945.960488	20.468890
61.329574	1943.225916	20.473907
61.553196	1946.329452	20.478925
61.203272	1948.822580	20.483943
61.366466	1949.073533	20.488960
61.097881	1956.225304	20.493978
61.075592	1964.331079	20.498995
61.478514	1952.043407	20.504013
61.659736	1981.912396	20.509031
61.685833	1996.762620	20.514048
61.555195	1972.239725	20.519066
61.821599	1982.923707	20.524083
61.957387	1975.422418	20.529101
61.937985	1993.026905	20.534119
62.169156	1989.796973	20.539136
62.507520	1998.302239	20.544154
62.639217	1992.057004	20.549171
62.577570	1991.538072	20.554189
62.298914	1996.244032	20.559207
62.524606	1996.691806	20.564224
62.898658	2006.463490	20.569242
62.698679	1995.780362	20.574259
62.918908	1994.139945	20.579277
62.667555	2014.090443	20.584295
62.655339	1992.580774	20.589312
62.883128	1982.355906	20.594330
62.709358	1997.187790	20.599347
62.832271	1978.894993	20.604365
62.586334	1989.523610	20.609383
62.988844	2025.869318	20.614400
63.194403	2017.112606	20.619418
62.976719	2049.680446	20.624435
63.518034	2030.410142	20.629453
63.550196	2018.050147	20.634471
63.787555	2002.416674	20.639488
63.557460	2014.238441	20.644506
63.546351	2017.204926	20.649523
63.978769	2019.243251	20.654541
63.776767	2013.536628	20.659559
63.729287	2020.417975	20.664576
63.732072	2009.988287	20.669594
63.613332	2020.062044	20.674611
64.214860	2010.671400	20.679629
64.004247	2012.748674	20.684647
63.915555	2024.183367	20.689664
64.049608	2017.718283	20.694682
63.842782	2018.522717	20.699699
64.178186	2028.328848	20.704717
64.215784	2010.761305	20.709735
64.171355	2003.611183	20.714752
64.197588	2008.367926	20.719770
64.238754	2032.281403	20.724787
64.333432	2035.558895	20.729805
64.415411	2049.465552	20.734823
64.319197	2041.676151	20.739840
64.224598	2053.767436	20.744858
64.229564	2044.019233	20.749875
64.567266	2056.723311	20.754893
64.750074	2064.419623	20.759911
65.052815	2057.374086	20.764928
65.085888	2059.900578	20.769946
64.876706	2053.110278	20.774963
65.168443	2057.634415	20.779981
65.318273	2065.539783	20.784999
65.386368	2073.532075	20.790016
65.728059	2088.967723	20.795034
65.676049	2081.022696	20.800051
65.681029	2078.749058	20.805069
65.820457	2084.873690	20.810087
65.793372	2079.512679	20.815104
66.101073	2094.777799	20.820122
65.909932	2076.597994	20.825139
65.998131	2077.891773	20.830157
65.950442	2073.606719	20.835175
66.205184	2100.217504	20.840192
66.186046	2080.103694	20.845210
66.099489	2101.378413	20.850227
66.225249	2087.704694	20.855245
66.112670	2081.744727	20.860263
66.189475	2092.009506	20.865280
66.234993	2070.257845	20.870298
65.910873	2085.947978	20.875315
66.257318	2076.478602	20.880333
66.259282	2096.956244	20.885351
66.446868	2103.157458	20.890368
66.769027	2123.630050	20.895386
66.719367	2125.679757	20.900403
66.941248	2121.065644	20.905421
66.777645	2126.067931	20.910439
67.073568	2119.789896	20.915456
67.266764	2130.090969	20.920474
66.564344	2128.085476	20.925491
67.021409	2119.743956	20.930509
66.972330	2134.309345	20.935527
66.815505	2151.370874	20.940544
67.262032	2155.487242	20.945562
67.154189	2145.059703	20.950579
67.283070	2152.336697	20.955597
67.249785	2155.729538	20.960615
67.503657	2172.179220	20.965632
67.781174	2174.652740	20.970650
67.863471	2172.290832	20.975667
68.137249	2179.951701	20.980685
68.441662	2158.899331	20.985703
67.937949	2165.688251	20.990720
68.211041	2138.026254	20.995738
67.958955	2157.003406	21.000755
68.277024	2175.065437	21.005773
68.492605	2171.068192	21.010791
68.370948	2164.505463	21.015808
68.680433	2169.420336	21.020826
68.235542	2159.965456	21.025843
68.659143	2168.363834	21.030861
68.477256	2164.068357	21.035879
68.700905	2177.351722	21.040896
68.938537	2170.246629	21.045914
68.684087	2180.842341	21.050931
68.608844	2167.589202	21.055949
68.818530	2180.817801	21.060967
68.729127	2176.101200	21.065984
68.806243	2187.331774	21.071002
68.730862	2186.089045	21.076019
68.661626	2185.105297	21.081037
68.716232	2183.076846	21.086055
68.874436	2202.063012	21.091072
68.901240	2186.178860	21.096090
69.058439	2220.883073	21.101107
69.274858	2221.358563	21.106125
69.590502	2217.102291	21.111143
69.259157	2220.286569	21.116160
69.540161	2223.381860	21.121178
69.817525	2232.790103	21.126195
69.927787	2251.214857	21.131213
70.201929	2244.933089	21.136231
69.788168	2251.301933	21.141248
70.488278	2232.284323	21.146266
70.266504	2251.260911	21.151283
70.111737	2236.013897	21.156301
70.364847	2232.733151	21.161319
70.553868	2228.473592	21.166336
70.509192	2221.215160	21.171354
70.354453	2221.555756	21.176371
70.270112	2240.266944	21.181389
70.494196	2222.592763	21.186407
70.532509	2265.505930	21.191424
70.808382	2251.338339	21.196442
70.732756	2266.574274	21.201459
70.965337	2261.225990	21.206477
70.924568	2275.478969	21.211495
70.736973	2269.621075	21.216512
71.120137	2273.269874	21.221530
71.047691	2272.204184	21.226547
71.039210	2264.010569	21.231565
71.263137	2293.305581	21.236583
71.487016	2285.991127	21.241600
71.750758	2301.211560	21.246618
72.084540	2285.906989	21.251635
71.665289	2287.669423	21.256653
71.882951	2271.117132	21.261671
71.932398	2281.211783	21.266688
72.074442	2285.454672	21.271706
72.096842	2269.545969	21.276723
71.976561	2281.468377	21.281741
72.302657	2269.677323	21.286759
71.989631	2270.773881	21.291776
72.437025	2278.540930	21.296794
72.089914	2274.186912	21.301811
72.336805	2282.245519	21.306829
72.592050	2273.660540	21.311847
72.367800	2291.600156	21.316864
72.514353	2270.511328	21.321882
72.617783	2280.152051	21.326899
72.678216	2283.649493	21.331917
72.837928	2272.925528	21.336935
72.565989	2275.562686	21.341952
72.541556	2307.646946	21.346970
73.089229	2302.869511	21.351987
72.953560	2317.373410	21.357005
73.094803	2302.895001	21.362023
72.782298	2325.847855	21.367040
73.161794	2302.844999	21.372058
73.045021	2316.627779	21.377075
73.310141	2329.924302	21.382093
73.469129	2321.891929	21.387111
73.341242	2339.915267	21.392128
73.467801	2338.595659	21.397146
73.460996	2354.495989	21.402163
73.570795	2331.203064	21.407181
73.768158	2347.802211	21.412199
73.519908	2357.286367	21.417216
73.800270	2352.752665	21.422234
73.919561	2371.376039	21.427251
73.799385	2359.374258	21.432269
74.271464	2365.792403	21.437287
73.980080	2342.705694	21.442304
74.519116	2373.349946	21.447322
74.402696	2372.242704	21.452339
74.764176	2388.503603	21.457357
74.969886	2364.069164	21.462375
74.970971	2395.448122	21.467392
75.047961	2377.528821	21.472410
75.048961	2384.794386	21.477427
75.143231	2378.331887	21.482445
75.494922	2384.067483	21.487463
75.157895	2378.619023	21.492480
75.198229	2369.031083	21.497498
75.123732	2367.242215	21.502515
75.521158	2379.440510	21.507533
75.648962	2365.071333	21.512551
75.184000	2394.293397	21.517568
75.487672	2383.313319	21.522586
75.446497	2401.530636	21.527603
75.677647	2380.018490	21.532621
75.610162	2389.613323	21.537639
75.574426	2391.775118	21.542656
75.678363	2376.727105	21.547674
75.663363	2401.695552	21.552691
75.819841	2394.599633	21.557709
75.906189	2411.625203	21.562727
75.856087	2395.041841	21.567744
76.075773	2404.616587	21.572762
76.283694	2409.528442	21.577779
75.963037	2418.031248	21.582797
76.253104	2430.058180	21.587815
76.234420	2432.857616	21.592832
76.030061	2441.545122	21.597850
76.708923	2445.191156	21.602867
76.550863	2467.300317	21.607885
76.823087	2455.646942	21.612903
76.981482	2478.981195	21.617920
77.218473	2450.056484	21.622938
77.440756	2461.759063	21.627955
77.396704	2462.803903	21.632973
77.530108	2470.734535	21.637991
77.787766	2461.694789	21.643008
77.771067	2454.469216	21.648026
77.466024	2449.675583	21.653043
77.875791	2461.683941	21.658061
78.087199	2447.600630	21.663079
77.890863	2458.642964	21.668096
77.878065	2451.247088	21.673114
78.345560	2464.628182	21.678131
77.686853	2452.621042	21.683149
77.964933	2453.309350	21.688167
77.964331	2451.519873	21.693184
78.478938	2441.684445	21.698202
78.050454	2459.326362	21.703219
77.750373	2449.406887	21.708237
77.987177	2444.372755	21.713255
78.112571	2453.275421	21.718272
78.274548	2464.963365	21.723290
78.194759	2490.330793	21.728307
78.269646	2489.474959	21.733325
78.605098	2478.676345	21.738343
78.664165	2508.329276	21.743360
78.729344	2518.355744	21.748378
78.813865	2513.908484	21.753395
79.233763	2520.461480	21.758413
79.419547	2507.404445	21.763431
79.236130	2506.525162	21.768448
79.277709	2490.426671	21.773466
79.067882	2508.031527	21.778483
79.179741	2505.864261	21.783501
79.844943	2530.065294	21.788519
79.765583	2521.926162	21.793536
79.770657	2544.550130	21.798554
79.777222	2532.060606	21.803571
79.751576	2536.954413	21.808589
79.865926	2533.246009	21.813607
79.966779	2534.677874	21.818624
79.930460	2538.198841	21.823642
80.082815	2521.087273	21.828659
79.953841	2546.969739	21.833677
80.261222	2563.237991	21.838695
80.084919	2558.755680	21.843712
80.531779	2562.101349	21.848730
80.429231	2557.674164	21.853747
80.230580	2554.675847	21.858765
80.666098	2575.206973	21.863783
80.510189	2586.715288	21.868800
80.653816	2585.858127	21.873818
81.104093	2576.692010	21.878835
80.955286	2590.040232	21.883853
80.911097	2577.574410	21.888871
80.766687	2604.673918	21.893888
81.376939	2613.257022	21.898906
81.660039	2625.009115	21.903923
81.538818	2623.832579	21.908941
81.815697	2632.092292	21.913959
81.465827	2617.692578	21.918976
81.774763	2626.026310	21.923994
81.806220	2611.388416	21.929011
81.549731	2618.824772	21.934029
81.945023	2646.719692	21.939047
82.087222	2640.532392	21.944064
81.998391	2662.211553	21.949082
81.967255	2653.095420	21.954099
81.982882	2647.289220	21.959117
82.334302	2640.539663	21.964135
82.123200	2650.500864	21.969152
82.411297	2655.640068	21.974170
82.968176	2657.696689	21.979187
83.119906	2662.429550	21.984205
83.198850	2660.056116	21.989223
83.264706	2663.477168	21.994240
83.195231	2656.943987	21.999258
83.505238	2637.024335	22.004275
83.077861	2645.154206	22.009293
83.165448	2631.440157	22.014311
83.331024	2649.803893	22.019328
83.321811	2657.073242	22.024346
83.646445	2660.926860	22.029363
83.222745	2662.368656	22.034381
83.559362	2656.358643	22.039399
83.725535	2663.293543	22.044416
83.569597	2661.604111	22.049434
83.730234	2655.554290	22.054451
83.715691	2662.285816	22.059469
84.087894	2684.021088	22.064487
83.710286	2671.927369	22.069504
83.855930	2694.814708	22.074522
84.277912	2679.567013	22.079539
84.176746	2687.874662	22.084557
84.204340	2689.298769	22.089575
84.456395	2698.172577	22.094592
84.502062	2704.590669	22.099610
84.837997	2715.887114	22.104627
85.091816	2714.434845	22.109645
85.047301	2715.698057	22.114663
85.384315	2710.847450	22.119680
85.028710	2708.475550	22.124698
84.832367	2714.412841	22.129715
85.136608	2712.006303	22.134733
85.238989	2708.733241	22.139751
85.407182	2707.824973	22.144768
85.192684	2706.657743	22.149786
85.416906	2726.603794	22.154803
85.372182	2734.244944	22.159821
85.634857	2744.895925	22.164839
85.742199	2740.487343	22.169856
85.708406	2751.982097	22.174874
85.976589	2731.957044	22.179891
86.191368	2753.772359	22.184909
86.196849	2759.671199	22.189927
86.414072	2767.574552	22.194944
86.310748	2770.856480	22.199962
86.613379	2749.999046	22.204979
86.253643	2764.090253	22.209997
86.229474	2768.819148	22.215015
86.724105	2767.276891	22.220032
86.681406	2777.592777	22.225050
86.972824	2777.392986	22.230067
86.931443	2788.102902	22.235085
87.041436	2791.483031	22.240103
87.110264	2789.444868	22.245120
87.067261	2788.418365	22.250138
87.312249	2786.793359	22.255155
87.086272	2799.983671	22.260173
87.530833	2784.670338	22.265191
87.753946	2790.351754	22.270208
87.422182	2792.842014	22.275226
87.633319	2800.079545	22.280243
87.675883	2813.912414	22.285261
87.750854	2798.420408	22.290279
88.214934	2806.010779	22.295296
88.097794	2827.035287	22.300314
88.252242	2810.750115	22.305331
88.288585	2824.438567	22.310349
87.937091	2806.897015	22.315367
88.428858	2828.682214	22.320384
88.547720	2837.765097	22.325402
88.936342	2844.050010	22.330419
89.176516	2848.765756	22.335437
88.960886	2846.595873	22.340455
88.911255	2808.875841	22.345472
88.757379	2827.819283	22.350490
89.013400	2825.112860	22.355507
88.811091	2844.070427	22.360525
89.110201	2838.760747	22.365543
89.292073	2842.014458	22.370560
89.081964	2846.312545	22.375578
89.099871	2838.488430	22.380595
88.979636	2856.225710	22.385613
89.450022	2865.751445	22.390631
89.557992	2875.706122	22.395648
89.914145	2864.519614	22.400666
89.990460	2869.322869	22.405683
89.771604	2857.843636	22.410701
89.963096	2866.937957	22.415719
90.254152	2882.767372	22.420736
90.071359	2882.041487	22.425754
90.461676	2892.781702	22.430771
90.134227	2885.695258	22.435789
89.866049	2898.064185	22.440807
90.718205	2893.474417	22.445824
90.724861	2923.911518	22.450842
91.010800	2906.662896	22.455859
91.015437	2918.945817	22.460877
91.021717	2912.311043	22.465895
91.172997	2924.275677	22.470912
90.837053	2924.635406	22.475930
91.038461	2908.340403	22.480947
91.285718	2923.383491	22.485965
91.602089	2938.342937	22.490983
91.510816	2942.820603	22.496000
91.410851	2952.971286	22.501018
91.663666	2952.097835	22.506035
91.660118	2960.991791	22.511053
91.394410	2961.638698	22.516071
91.557627	2964.769942	22.521088
91.589760	2991.536660	22.526106
91.952869	2979.547240	22.531123
92.216319	2995.100065	22.536141
92.156055	2983.696882	22.541159
92.582988	2993.356633	22.546176
92.489888	2998.528436	22.551194
92.546754	2974.902379	22.556211
92.478600	2989.489443	22.561229
93.085502	2992.845176	22.566247
93.201979	2988.957001	22.571264
92.949335	3000.432599	22.576282
93.198933	2994.547453	22.581299
93.328968	2994.202694	22.586317
93.209972	2994.267942	22.591335
93.595446	3022.406872	22.596352
93.490422	3022.833550	22.601370
93.790909	3030.763629	22.606387
93.796423	3029.116760	22.611405
93.773521	3030.009735	22.616423
93.841498	3017.622649	22.621440
93.950551	3015.094989	22.626458
93.761847	3021.245874	22.631475
93.916056	3028.458082	22.636493
93.995495	3051.979657	22.641511
94.052392	3043.937601	22.646528
94.106703	3058.795800	22.651546
94.632435	3051.159679	22.656563
94.673857	3058.749160	22.661581
94.676657	3051.644874	22.666599
94.837086	3056.292965	22.671616
94.562346	3053.390578	22.676634
95.024944	3073.623047	22.681651
95.114790	3077.228985	22.686669
95.072460	3087.620993	22.691687
95.518787	3079.711199	22.696704
95.242529	3067.941524	22.701722
95.104987	3068.191117	22.706739
95.543524	3078.783942	22.711757
95.017841	3074.236982	22.716775
95.721421	3076.913051	22.721792
95.584054	3086.627138	22.726810
95.967571	3086.953799	22.731827
96.395651	3093.774952	22.736845
96.046090	3094.492014	22.741863
96.404025	3087.963210	22.746880
96.248116	3095.621928	22.751898
96.220233	3087.792853	22.756915
96.354396	3085.184663	22.761933
96.025122	3119.765212	22.766951
96.388080	3128.593977	22.771968
96.572079	3124.968597	22.776986
96.545431	3138.076067	22.782003
97.153522	3122.105721	22.787021
96.877698	3138.545947	22.792039
97.163071	3150.402584	22.797056
97.126476	3144.447560	22.802074
97.506200	3153.079101	22.807091
97.900883	3152.924245	22.812109
97.597065	3167.913374	22.817127
97.828791	3142.858900	22.822144
98.039088	3145.806239	22.827162
97.890835	3152.551807	22.832179
97.688845	3143.414605	22.837197
97.923433	3163.153625	22.842215
97.924093	3164.553489	22.847232
98.220000	3184.060969	22.852250
97.907022	3174.963544	22.857267
98.250649	3175.284399	22.862285
98.017890	3176.877150	22.867303
98.236013	3178.016496	22.872320
98.473376	3195.306728	22.877338
98.536695	3206.089387	22.882355
99.036709	3187.672711	22.887373
98.862285	3222.743400	22.892391
99.208106	3210.012244	22.897408
99.055541	3228.551474	22.902426
99.491717	3226.946793	22.907443
99.546460	3232.539475	22.912461
99.601572	3231.512672	22.917479
99.813312	3227.970668	22.922496
99.900899	3227.665592	22.927514
99.817922	3247.002910	22.932531
99.781570	3217.549743	22.937549
99.791845	3249.045640	22.942567
100.261707	3246.490405	22.947584
100.283667	3260.600871	22.952602
100.841061	3252.075254	22.957619
100.856762	3245.362213	22.962637
100.679254	3255.593618	22.967655
100.740241	3247.739345	22.972672
100.923109	3247.588193	22.977690
100.808420	3261.057723	22.982707
101.055272	3248.662938	22.987725
100.801374	3252.290683	22.992743
100.923823	3253.080527	22.997760
101.076195	3264.839950	23.002778
101.126679	3278.641616	23.007795
101.294424	3273.810538	23.012813
101.338808	3291.589809	23.017831
101.750311	3282.234428	23.022848
101.557838	3282.277963	23.027866
101.438814	3289.873994	23.032883
101.332777	3292.787027	23.037901
101.265631	3305.842676	23.042919
101.831108	3300.068785	23.047936
101.802946	3315.469943	23.052954
101.722362	3342.186808	23.057971
102.317731	3333.396627	23.062989
102.183186	3345.685566	23.068007
102.454257	3350.194608	23.073024
102.747484	3358.620303	23.078042
102.830063	3375.955801	23.083059
103.265007	3371.924362	23.088077
103.010787	3384.010095	23.093095
102.969421	3359.758007	23.098112
103.338374	3377.073347	23.103130
103.282114	3367.093304	23.108147
103.843348	3366.643823	23.113165
103.323808	3367.584439	23.118183
103.642530	3374.392099	23.123200
103.774270	3377.058789	23.128218
103.803782	3389.777502	23.133235
104.028557	3381.328823	23.138253
103.950600	3390.664418	23.143271
104.150466	3392.041227	23.148288
103.972148	3378.450368	23.153306
104.003672	3395.299487	23.158323
104.436576	3424.191876	23.163341
104.447044	3424.132592	23.168359
104.390324	3409.266210	23.173376
104.595609	3417.587976	23.178394
104.533778	3431.042226	23.183411
105.096133	3437.833276	23.188429
105.153261	3438.059956	23.193447
105.432290	3440.249798	23.198464
105.701111	3426.003368	23.203482
105.389124	3442.341633	23.208499
105.658610	3432.031760	23.213517
105.761802	3443.022741	23.218535
105.939631	3426.427375	23.223552
105.821777	3435.914459	23.228570
105.781325	3453.347140	23.233587
106.197211	3451.083641	23.238605
106.160990	3450.779731	23.243623
105.950974	3470.856764	23.248640
106.164765	3454.488082	23.253658
106.379268	3474.847698	23.258675
106.684317	3495.839963	23.263693
106.438571	3492.685084	23.268711
106.550656	3476.484157	23.273728
106.766599	3490.993453	23.278746
106.951082	3486.330789	23.283763
106.978260	3508.171086	23.288781
107.229164	3519.160546	23.293799
107.575587	3509.050687	23.298816
107.278523	3522.553926	23.303834
107.413822	3513.612521	23.308851
107.792675	3515.623294	23.313869
107.627258	3517.893478	23.318887
107.748458	3529.356900	23.323904
107.973059	3555.635349	23.328922
107.787153	3558.479156	23.333939
107.908223	3549.083818	23.338957
108.244423	3558.773092	23.343975
108.236979	3540.549096	23.348992
108.722597	3569.031503	23.354010
108.756290	3571.906933	23.359027
108.883055	3580.203773	23.364045
108.667147	3579.692956	23.369063
108.645709	3582.671389	23.374080
109.220327	3571.061294	23.379098
108.849914	3563.931443	23.384115
109.180602	3569.373538	23.389133
109.363419	3577.608363	23.394151
109.482174	3591.981856	23.399168
109.732202	3589.468404	23.404186
109.597458	3585.140132	23.409203
109.658218	3593.905726	23.414221
109.536134	3580.765008	23.419239
109.880869	3595.713518	23.424256
109.945910	3607.404175	23.429274
110.105641	3613.769745	23.434291
110.464483	3608.462334	23.439309
110.588718	3618.041407	23.444327
110.575745	3608.194989	23.449344
110.735363	3625.899112	23.454362
110.597523	3632.482746	23.459379
110.684169	3632.177032	23.464397
110.743788	3661.493727	23.469415
111.304383	3648.809394	23.474432
111.361912	3661.352847	23.479450
111.178855	3664.022986	23.484467
111.361930	3648.420933	23.489485
111.210519	3676.204333	23.494503
111.408909	3670.259485	23.499520
111.828150	3678.886368	23.504538
111.774308	3668.269555	23.509555
111.786382	3692.736243	23.514573
111.947838	3693.140950	23.519591
112.128221	3704.429970	23.524608
112.209682	3704.962849	23.529626
112.358550	3723.803034	23.534643
112.384098	3705.520837	23.539661
112.658445	3725.350457	23.544679
112.330665	3740.394291	23.549696
113.047991	3740.219186	23.554714
112.986433	3749.108419	23.559731
113.373590	3734.090233	23.564749
113.204271	3735.563312	23.569767
113.185707	3751.097167	23.574784
113.467272	3765.415377	23.579802
113.244119	3764.545537	23.584819
113.226971	3759.747814	23.589837
113.508801	3781.322613	23.594855
113.495764	3788.641942	23.599872
114.387688	3794.325608	23.604890
114.362209	3793.377043	23.609907
114.570776	3797.701676	23.614925
114.619931	3787.680321	23.619943
114.456269	3803.072861	23.624960
114.738478	3786.269716	23.629978
114.936518	3807.662347	23.634995
114.957418	3831.997095	23.640013
115.425806	3821.368287	23.645031
115.344737	3822.489804	23.650048
115.471584	3802.593999	23.655066
115.742238	3814.627192	23.660083
115.918352	3799.848134	23.665101
115.625878	3816.585118	23.670119
115.369550	3822.584119	23.675136
115.697123	3813.463140	23.680154
115.697980	3813.767625	23.685171
115.901184	3818.243928	23.690189
115.955198	3808.838255	23.695207
115.925964	3838.144378	23.700224
116.262461	3827.148407	23.705242
116.010225	3842.261152	23.710259
116.171332	3833.948331	23.715277
116.534928	3859.583894	23.720295
116.385962	3857.334940	23.725312
116.438219	3848.676340	23.730330
116.796147	3865.671236	23.735347
117.154453	3885.126186	23.740365
117.430987	3882.830539	23.745383
116.949127	3884.685966	23.750400
117.488708	3891.906155	23.755418
117.268513	3889.417800	23.760435
117.357478	3902.352294	23.765453
117.731414	3912.325697	23.770471
117.932001	3920.452262	23.775488
118.415202	3917.861450	23.780506
117.820720	3933.535140	23.785523
118.160150	3927.513151	23.790541
118.196127	3936.184220	23.795559
118.193924	3951.016397	23.800576
118.499774	3962.054964	23.805594
118.644233	3949.775353	23.810611
118.812314	3972.696705	23.815629
118.992442	3967.154545	23.820647
119.288526	3979.591124	23.825664
119.854201	3973.927775	23.830682
119.684971	3977.170456	23.835699
119.728754	3981.353481	23.840717
119.908204	3963.280575	23.845735
119.622410	3984.722300	23.850752
119.736769	3965.086212	23.855770
119.492641	3993.591174	23.860787
119.691843	3992.970412	23.865805
120.066917	4001.227628	23.870823
120.192425	4007.932070	23.875840
120.208738	4006.835254	23.880858
120.247373	4027.271900	23.885875
120.335432	4028.820581	23.890893
120.625256	4036.707275	23.895911
120.747035	4059.911591	23.900928
121.066822	4060.050000	23.905946
121.185315	4060.314579	23.910963
121.285420	4067.063400	23.915981
121.865176	4054.751539	23.920999
121.364604	4061.966528	23.926016
121.942312	4064.245682	23.931034
121.914312	4078.440934	23.936051
122.260622	4081.468927	23.941069
122.305994	4073.673112	23.946087
122.275408	4085.087032	23.951104
122.360475	4070.430236	23.956122
122.822761	4077.852647	23.961139
122.669260	4076.563030	23.966157
122.808589	4081.473567	23.971175
122.945294	4079.673024	23.976192
122.929593	4078.741722	23.981210
122.802765	4098.937312	23.986227
122.963462	4103.060895	23.991245
123.141297	4101.318904	23.996263
122.964433	4108.465070	24.001280
123.356658	4129.194195	24.006298
123.539684	4136.497826	24.011315
123.537198	4124.799029	24.016333
123.848550	4136.928106	24.021351
123.966481	4138.047470	24.026368
123.833070	4141.253952	24.031386
123.871119	4148.542176	24.036403
124.193267	4181.167523	24.041421
124.714557	4153.758340	24.046439
124.778767	4170.864703	24.051456
124.934068	4158.757932	24.056474
124.942688	4156.872249	24.061491
124.966183	4158.932774	24.066509
125.213669	4167.962314	24.071527
124.792750	4188.325903	24.076544
125.114231	4179.686802	24.081562
125.223802	4192.677581	24.086579
125.528929	4199.247312	24.091597
125.515578	4192.681963	24.096615
125.391809	4214.141717	24.101632
125.771822	4207.276331	24.106650
125.589438	4222.783793	24.111667
125.638443	4243.625296	24.116685
126.461761	4251.890466	24.121703
126.394739	4259.479559	24.126720
126.125138	4250.786520	24.131738
126.787889	4282.656216	24.136755
126.811943	4267.756175	24.141773
127.054223	4278.457847	24.146791
127.055744	4286.211999	24.151808
127.140529	4276.771825	24.156826
127.099890	4285.229378	24.161843
127.135101	4304.476048	24.166861
127.549094	4298.938825	24.171879
127.413758	4311.918993	24.176896
127.738833	4316.347744	24.181914
128.048895	4330.283828	24.186931
128.217712	4338.544993	24.191949
128.457080	4321.912124	24.196967
128.307905	4336.395343	24.201984
128.739101	4327.451425	24.207002
128.702618	4341.576275	24.212019
128.902410	4355.394385	24.217037
129.347416	4352.012198	24.222055
129.390264	4368.623504	24.227072
129.508833	4351.392863	24.232090
129.802212	4353.278112	24.237107
129.528563	4346.881690	24.242125
130.008699	4340.369375	24.247143
129.466024	4341.143988	24.252160
129.982975	4333.253978	24.257178
130.184476	4341.932961	24.262195
129.776738	4339.593629	24.267213
130.202123	4366.104050	24.272231
130.120126	4363.834901	24.277248
130.267956	4371.191308	24.282266
130.396644	4380.588232	24.287283
130.349738	4403.165441	24.292301
130.687515	4391.549190	24.297319
130.670529	4399.425352	24.302336
130.746125	4416.195073	24.307354
131.278112	4425.256097	24.312371
131.254583	4433.952238	24.317389
131.459029	4434.660092	24.322407
131.600809	4445.600529	24.327424
131.555812	4455.075016	24.332442
131.820307	4466.746750	24.337459
132.083509	4469.689736	24.342477
132.220354	4471.037884	24.347495
132.306602	4463.853218	24.352512
131.979514	4483.375719	24.357530
132.246751	4476.855616	24.362547
132.430454	4505.962464	24.367565
132.871707	4495.995939	24.372583
132.273727	4510.991269	24.377600
132.726597	4523.149233	24.382618
132.649774	4533.937274	24.387635
132.830067	4547.472168	24.392653
133.420083	4556.848480	24.397671
133.489214	4553.740956	24.402688
133.809921	4560.020476	24.407706
133.924272	4562.905400	24.412723
133.621397	4553.874779	24.417741
134.137080	4584.460755	24.422759
134.199570	4589.981389	24.427776
134.468259	4573.128054	24.432794
134.503584	4586.941265	24.437811
134.461500	4588.969770	24.442829
134.742076	4595.907502	24.447847
134.971250	4594.256186	24.452864
135.036426	4607.831414	24.457882
135.088539	4593.974444	24.462899
135.122415	4611.259925	24.467917
135.255659	4617.907842	24.472935
135.463140	4631.095800	24.477952
135.465368	4634.269735	24.482970
135.725722	4639.622259	24.487987
135.858757	4647.385570	24.493005
136.265047	4663.282809	24.498023
136.091254	4671.500372	24.503040
136.313830	4651.129397	24.508058
136.465037	4663.907788	24.513075
136.510030	4678.388769	24.518093
136.642331	4689.499841	24.523111
136.899630	4704.907965	24.528128
137.251917	4700.363865	24.533146
137.626606	4697.775899	24.538163
137.469789	4705.796975	24.543181
137.695919	4718.654368	24.548199
137.518156	4716.930123	24.553216
138.003834	4698.545921	24.558234
137.964715	4707.885733	24.563251
137.973006	4696.927241	24.568269
138.180847	4731.434438	24.573287
138.442408	4732.411608	24.578304
138.417826	4742.541163	24.583322
138.837580	4728.157184	24.588339
138.543458	4743.024968	24.593357
138.635208	4747.930194	24.598375
138.858960	4770.933292	24.603392
138.981305	4766.976774	24.608410
139.168009	4774.159626	24.613427
139.068584	4792.544501	24.618445
139.583700	4798.967585	24.623463
139.987850	4797.700328	24.628480
139.848349	4816.498153	24.633498
140.274039	4811.951735	24.638515
140.244858	4835.432550	24.643533
140.669555	4837.498131	24.648551
140.792350	4839.243123	24.653568
140.552715	4823.243596	24.658586
140.588704	4836.531719	24.663603
141.010362	4832.193836	24.668621
140.992123	4840.690510	24.673639
141.292435	4853.800720	24.678656
141.110203	4855.331154	24.683674
141.507407	4858.691052	24.688691
141.472528	4853.628990	24.693709
141.653610	4873.161317	24.698727
141.880634	4885.312003	24.703744
141.843295	4889.561434	24.708762
141.968080	4890.206882	24.713779
142.099217	4885.376828	24.718797
142.438552	4901.271596	24.723815
142.540449	4900.856250	24.728832
142.626625	4924.581921	24.733850
142.887809	4914.972053	24.738867
142.968333	4904.499515	24.743885
142.946007	4896.372738	24.748903
143.160658	4925.836680	24.753920
142.977255	4942.061964	24.758938
143.462786	4932.699663	24.763955
143.334233	4955.646681	24.768973
143.259690	4954.358115	24.773991
143.725479	4961.665807	24.779008
143.658044	4968.434437	24.784026
144.319250	4989.829334	24.789043
144.499912	4997.240063	24.794061
144.687344	4985.298603	24.799079
145.041297	5006.656103	24.804096
145.120184	5002.175990	24.809114
144.951661	4983.726320	24.814131
144.885741	4991.072672	24.819149
145.194031	5013.484986	24.824167
145.565011	5026.117121	24.829184
145.353226	5017.531422	24.834202
145.617423	5016.925473	24.839219
145.774470	5017.835285	24.844237
145.545166	5044.090867	24.849255
146.005566	5053.988122	24.854272
145.897150	5038.124961	24.859290
146.077205	5074.858811	24.864307
146.461182	5085.671882	24.869325
146.459307	5097.774335	24.874343
146.780548	5111.579351	24.879360
146.893503	5111.168472	24.884378
147.157610	5115.327602	24.889395
147.260562	5106.139441	24.894413
146.991121	5123.319308	24.899431
147.260289	5140.554293	24.904448
147.417324	5151.378925	24.909466
147.772436	5158.063643	24.914483
148.107783	5165.178413	24.919501
147.989175	5179.593978	24.924519
148.457728	5165.501542	24.929536
148.325525	5176.422410	24.934554
148.927050	5189.665421	24.939571
148.912325	5197.622324	24.944589
148.998474	5205.279091	24.949607
149.315782	5198.882307	24.954624
149.225733	5183.269514	24.959642
149.500798	5203.222959	24.964659
149.495481	5217.828901	24.969677
149.454966	5230.876452	24.974695
149.768555	5225.968505	24.979712
149.643120	5228.866009	24.984730
150.190168	5237.855731	24.989747
149.969209	5246.512506	24.994765
150.023058	5251.570221	24.999783
150.198970	5262.676859	25.004800
150.680502	5266.425682	25.009818
151.134293	5265.775798	25.014835
151.292354	5265.796453	25.019853
151.320200	5301.318940	25.024871
151.895811	5293.845149	25.029888
151.720361	5299.124633	25.034906
151.801305	5300.787221	25.039923
152.077948	5294.102619	25.044941
152.266524	5291.450031	25.049959
152.466632	5283.611506	25.054976
152.144100	5294.100112	25.059994
152.294553	5293.362155	25.065011
152.800247	5315.239514	25.070029
152.468384	5329.653446	25.075047
152.832361	5310.476794	25.080064
152.597190	5336.512963	25.085082
152.872758	5323.321596	25.090099
153.069455	5354.638991	25.095117
152.935599	5355.453578	25.100135
153.083680	5366.449531	25.105152
153.233416	5382.755664	25.110170
153.405877	5400.373073	25.115187
153.789432	5391.906126	25.120205
153.806907	5414.102100	25.125223
154.085691	5415.030012	25.130240
153.841363	5429.726435	25.135258
154.351807	5440.584214	25.140275
154.712587	5458.967851	25.145293
154.717869	5466.291243	25.150311
155.210089	5478.915526	25.155328
155.198676	5485.365661	25.160346
155.347867	5482.556155	25.165363
155.687373	5486.743480	25.170381
155.670291	5482.634615	25.175399
156.093183	5501.056860	25.180416
156.302221	5501.714793	25.185434
156.143703	5506.543496	25.190451
156.279575	5506.523328	25.195469
156.420346	5515.196073	25.200487
156.508732	5536.700551	25.205504
156.574659	5550.429241	25.210522
156.547128	5554.811885	25.215539
157.063543	5572.592745	25.220557
156.970502	5572.037143	25.225575
157.164672	5589.638974	25.230592
157.175248	5604.737166	25.235610
157.676758	5605.371581	25.240627
158.203944	5603.168529	25.245645
158.021879	5619.256886	25.250663
158.545067	5616.570608	25.255680
158.311202	5617.637574	25.260698
158.653242	5635.548506	25.265715
158.660577	5639.121430	25.270733
158.858503	5652.471293	25.275751
159.188386	5649.549219	25.280768
158.937430	5651.299364	25.285786
159.192400	5663.427931	25.290803
159.563138	5681.102270	25.295821
159.529856	5686.857635	25.300839
159.441350	5702.087261	25.305856
159.656380	5724.788074	25.310874
159.906296	5725.906613	25.315891
160.130735	5734.831421	25.320909
160.119779	5743.779774	25.325927
160.349951	5747.687579	25.330944
160.924556	5776.253049	25.335962
160.877518	5776.043405	25.340979
161.015295	5770.748171	25.345997
161.358934	5803.318647	25.351015
161.529092	5794.119764	25.356032
161.678087	5809.009443	25.361050
161.646651	5800.158061	25.366067
161.998089	5814.211485	25.371085
161.950653	5842.529837	25.376103
162.390924	5822.357994	25.381120
162.486957	5839.941676	25.386138
163.003407	5824.666638	25.391155
163.079544	5820.535981	25.396173
163.011935	5854.843922	25.401191
163.547587	5844.466035	25.406208
163.357106	5867.872688	25.411226
163.634314	5857.489462	25.416243
163.729146	5855.351910	25.421261
163.911083	5855.276883	25.426279
164.017199	5854.075722	25.431296
164.238091	5847.957617	25.436314
164.343118	5861.171424	25.441331
164.468448	5859.739512	25.446349
164.025831	5886.185703	25.451367
164.583778	5870.434438	25.456384
164.435119	5904.036143	25.461402
164.622547	5901.069446	25.466419
164.725822	5921.405767	25.471437
164.905620	5944.840729	25.476455
165.359897	5950.692415	25.481472
165.194602	5949.181342	25.486490
165.295163	5967.567236	25.491507
165.573242	5985.547411	25.496525
166.116344	6001.074965	25.501543
165.859027	6018.989302	25.506560
166.170679	6025.040975	25.511578
166.177611	6033.533745	25.516595
166.764823	6033.293713	25.521613
166.904164	6048.136392	25.526631
167.361393	6057.981661	25.531648
167.527036	6058.506226	25.536666
167.587552	6072.780409	25.541683
168.029944	6061.225563	25.546701
167.910423	6076.526038	25.551719
168.200238	6071.466627	25.556736
168.146190	6092.565841	25.561754
168.007257	6091.640212	25.566771
168.471217	6104.217702	25.571789
168.755792	6116.035404	25.576807
168.952558	6135.947859	25.581824
168.806927	6138.626800	25.586842
169.022192	6150.139811	25.591859
169.348137	6147.469500	25.596877
169.374767	6158.670742	25.601895
169.757979	6158.756962	25.606912
170.053861	6161.424771	25.611930
170.138031	6178.479250	25.616947
170.407564	6167.133615	25.621965
170.319371	6178.530237	25.626983
170.630987	6182.254207	25.632000
170.954593	6201.802844	25.637018
171.093304	6210.105023	25.642035
171.078121	6198.487876	25.647053
170.808625	6214.578297	25.652071
171.370751	6220.455970	25.657088
171.591709	6236.753197	25.662106
171.296163	6266.618966	25.667123
171.912711	6262.172894	25.672141
171.778568	6268.824357	25.677159
171.817611	6295.689730	25.682176
172.442131	6303.263592	25.687194
172.508696	6314.439841	25.692212
172.881162	6298.262452	25.697229
173.096544	6322.692987	25.702247
173.247295	6317.701361	25.707264
173.718490	6328.116204	25.712282
173.563707	6310.664762	25.717300
173.940002	6322.202478	25.722317
173.555740	6343.815301	25.727335
173.938894	6341.129993	25.732352
174.445183	6357.579432	25.737370
174.507982	6348.292048	25.742388
174.776813	6355.414025	25.747405
174.792993	6362.982518	25.752423
174.829163	6393.085086	25.757440
174.928338	6397.941176	25.762458
174.902160	6391.013202	25.767476
175.046116	6391.374415	25.772493
174.960519	6418.142865	25.777511
175.194995	6424.019237	25.782528
175.434993	6450.572902	25.787546
175.448056	6448.342471	25.792564
175.687429	6470.736770	25.797581
175.851143	6471.802673	25.802599
175.892743	6506.124707	25.807616
176.310044	6507.086499	25.812634
176.545953	6514.464805	25.817652
176.765229	6534.596515	25.822669
176.942681	6546.765746	25.827687
177.273949	6555.521780	25.832704
177.495048	6559.330491	25.837722
177.401017	6574.459504	25.842740
177.844440	6587.074246	25.847757
177.964996	6585.869068	25.852775
177.807385	6608.123230	25.857792
178.437048	6626.450823	25.862810
178.553658	6634.895479	25.867828
179.368065	6640.460335	25.872845
179.316246	6665.999071	25.877863
179.427219	6667.346569	25.882880
179.613780	6664.122361	25.887898
179.646311	6656.491571	25.892916
179.755024	6678.339185	25.897933
180.018248	6676.734397	25.902951
180.145538	6683.521994	25.907968
180.407996	6686.431273	25.912986
180.288073	6714.935641	25.918004
181.043468	6700.926735	25.923021
180.733234	6726.850042	25.928039
180.865420	6730.848706	25.933056
181.355920	6744.442535	25.938074
181.610121	6751.726187	25.943092
181.716527	6760.632497	25.948109
181.613056	6767.561029	25.953127
181.879249	6793.539615	25.958144
182.029915	6780.550757	25.963162
182.186643	6811.361074	25.968180
182.477093	6800.428904	25.973197
182.623457	6829.547441	25.978215
182.795947	6831.210422	25.983232
183.217125	6847.707911	25.988250
183.067389	6833.446029	25.993268
183.368710	6863.498207	25.998285
183.542012	6868.080349	26.003303
183.891444	6876.307114	26.008320
184.177880	6882.951950	26.013338
184.120680	6899.405292	26.018356
184.002893	6901.369428	26.023373
184.594747	6913.501185	26.028391
184.575500	6921.923950	26.033408
185.015049	6924.798107	26.038426
185.199025	6926.456838	26.043444
185.429229	6949.519966	26.048461
185.328179	6956.447393	26.053479
185.669899	6965.192087	26.058496
185.878238	6963.771955	26.063514
185.846714	6974.837306	26.068532
186.299356	6995.062563	26.073549
186.184920	6995.299140	26.078567
186.213671	7001.855483	26.083584
186.951910	7021.382311	26.088602
186.469637	7040.317408	26.093620
186.875400	7043.479100	26.098637
187.196788	7051.116410	26.103655
187.054589	7064.849318	26.108672
187.600718	7054.671299	26.113690
187.592813	7074.315179	26.118708
187.805776	7085.842647	26.123725
188.095488	7082.904899	26.128743
188.018514	7118.785497	26.133760
188.895477	7102.093544	26.138778
188.550393	7124.304599	26.143796
188.991531	7125.423541	26.148813
189.169736	7142.856112	26.153831
189.351574	7131.961740	26.158848
189.760787	7146.664399	26.163866
189.497450	7170.615035	26.168884
189.938307	7163.865102	26.173901
190.111217	7183.735187	26.178919
190.193932	7189.126609	26.183936
190.353615	7201.746598	26.188954
190.419214	7215.356313	26.193972
191.025563	7210.030424	26.198989
191.274422	7240.432205	26.204007
191.411833	7231.417842	26.209024
191.704932	7245.702703	26.214042
191.819432	7254.805233	26.219060
191.733329	7269.084257	26.224077
192.303437	7258.027203	26.229095
192.275453	7285.591677	26.234112
192.545548	7283.181628	26.239130
192.750561	7282.504657	26.244148
193.040445	7292.406710	26.249165
192.783624	7313.181169	26.254183
193.014200	7322.609497	26.259200
193.347417	7323.834491	26.264218
193.597426	7339.571676	26.269236
193.872950	7353.996571	26.274253
194.349977	7356.620875	26.279271
194.071003	7370.098650	26.284288
194.153079	7379.175108	26.289306
194.439832	7389.036000	26.294324
194.243441	7391.821982	26.299341
194.523422	7413.062302	26.304359
194.767399	7420.066805	26.309376
195.237169	7435.126721	26.314394
195.511984	7470.419983	26.319412
195.707386	7471.543328	26.324429
195.638217	7489.368400	26.329447
196.068416	7497.673896	26.334464
196.182675	7517.361935	26.339482
196.315877	7507.550332	26.344500
196.603185	7529.664555	26.349517
196.922088	7527.210178	26.354535
196.555241	7569.761342	26.359552
197.318339	7565.258408	26.364570
197.242700	7594.960813	26.369588
197.329891	7580.167677	26.374605
198.011091	7597.292405	26.379623
198.201792	7610.649465	26.384640
198.919943	7596.052903	26.389658
198.761951	7628.273369	26.394676
198.730394	7613.528961	26.399693
199.219088	7634.408263	26.404711
198.907788	7628.381734	26.409728
199.276783	7658.728248	26.414746
199.434788	7653.955121	26.419764
199.671337	7664.562413	26.424781
199.811201	7660.142741	26.429799
199.645937	7692.049520	26.434816
200.422123	7692.954849	26.439834
199.928388	7714.514791	26.444852
200.137277	7721.864661	26.449869
200.527443	7734.822659	26.454887
200.480516	7752.782174	26.459904
200.974120	7759.367559	26.464922
200.926589	7784.305712	26.469940
201.160663	7788.294111	26.474957
201.240931	7804.263785	26.479975
201.492461	7828.408355	26.484992
201.624522	7834.217125	26.490010
201.533939	7855.754750	26.495028
202.380085	7880.914758	26.500045
202.726968	7882.051696	26.505063
203.084363	7902.215107	26.510080
203.432285	7918.218640	26.515098
203.731050	7913.416665	26.520116
203.627381	7927.966170	26.525133
203.940589	7924.425053	26.530151
204.176823	7942.861726	26.535168
204.639796	7939.053291	26.540186
204.767267	7945.595292	26.545204
204.646218	7964.131189	26.550221
204.897561	7962.870828	26.555239
204.918576	7982.750482	26.560256
205.371540	7985.330043	26.565274
205.406659	8007.144804	26.570292
205.428058	8005.373500	26.575309
206.290354	8025.566267	26.580327
206.343155	8023.622021	26.585344
206.682323	8029.755773	26.590362
206.750739	8054.590926	26.595380
206.643784	8070.445317	26.600397
206.983715	8060.100683	26.605415
206.894925	8089.772328	26.610432
207.180890	8090.965813	26.615450
207.549102	8111.195436	26.620468
207.549677	8121.823913	26.625485
208.077837	8120.454796	26.630503
207.879669	8162.461466	26.635520
208.274480	8149.893052	26.640538
208.502635	8178.187800	26.645556
208.544150	8185.682103	26.650573
209.334181	8199.512416	26.655591
209.196020	8221.624668	26.660608
209.222761	8233.149883	26.665626
209.533886	8240.761118	26.670644
209.665630	8278.343325	26.675661
209.832954	8264.412882	26.680679
210.328024	8291.483940	26.685696
210.334824	8285.817290	26.690714
210.589752	8315.049803	26.695732
210.714824	8320.924489	26.700749
210.994967	8341.005929	26.705767
210.841657	8350.473889	26.710784
211.228170	8374.273297	26.715802
211.548958	8380.337766	26.720820
211.790274	8400.190210	26.725837
212.427639	8391.563555	26.730855
212.839928	8403.448124	26.735872
213.229330	8401.807354	26.740890
213.667554	8394.351661	26.745908
213.351058	8399.509388	26.750925
213.694825	8417.052269	26.755943
213.879703	8437.504774	26.760960
213.685491	8444.775883	26.765978
214.126865	8439.094868	26.770996
214.148696	8439.863409	26.776013
214.497236	8454.487536	26.781031
214.497387	8471.184677	26.786048
214.640264	8462.537300	26.791066
214.745934	8478.020669	26.796084
214.955725	8492.331456	26.801101
215.181801	8507.509852	26.806119
215.486506	8505.709796	26.811136
215.626572	8531.809757	26.816154
215.926850	8528.578591	26.821172
215.960500	8545.440395	26.826189
216.028088	8547.432387	26.831207
216.009909	8576.579770	26.836224
216.306707	8588.359909	26.841242
216.727055	8598.264071	26.846260
216.719127	8623.212757	26.851277
217.206525	8630.174432	26.856295
217.239101	8657.124061	26.861312
217.372856	8677.304151	26.866330
217.574050	8696.985601	26.871348
217.937099	8729.703472	26.876365
218.126659	8736.045731	26.881383
218.536699	8764.289425	26.886400
218.504850	8786.853524	26.891418
219.027123	8782.963420	26.896436
219.142834	8815.003252	26.901453
219.630343	8814.146438	26.906471
219.705671	8851.025760	26.911488
219.986531	8859.827644	26.916506
220.157955	8881.839259	26.921524
220.357839	8889.623561	26.926541
221.078030	8894.106878	26.931559
221.205380	8902.448196	26.936576
221.195178	8910.569661	26.941594
221.665225	8921.652743	26.946612
221.875351	8946.805345	26.951629
222.100473	8960.409112	26.956647
222.371349	8971.733855	26.961664
222.591881	8967.872297	26.966682
222.928986	8988.515383	26.971700
223.017894	8991.093831	26.976717
223.666099	9005.214504	26.981735
223.255492	9021.561082	26.986752
223.782086	9000.292282	26.991770
224.010632	9024.836289	26.996788
223.841785	9030.212410	27.001805
224.333024	9046.072906	27.006823
224.437789	9054.477895	27.011840
224.103798	9078.767592	27.016858
224.681529	9090.647399	27.021876
224.755006	9109.104452	27.026893
225.206353	9126.826465	27.031911
225.390999	9136.796690	27.036928
225.469317	9158.295580	27.041946
225.481777	9160.653551	27.046964
225.874983	9191.604697	27.051981
226.531095	9196.316862	27.056999
226.782539	9201.975666	27.062016
226.848273	9219.236150	27.067034
227.181932	9225.799750	27.072052
226.966975	9249.633697	27.077069
227.297226	9259.124693	27.082087
227.552611	9284.675982	27.087104
227.932988	9289.577082	27.092122
228.151470	9307.029810	27.097140
228.345172	9340.158137	27.102157
228.493686	9343.898790	27.107175
228.709017	9347.608712	27.112192
228.600712	9366.766374	27.117210
229.461163	9370.303552	27.122228
229.444934	9391.387544	27.127245
229.899171	9401.240144	27.132263
229.661633	9393.991729	27.137280
229.819874	9403.907413	27.142298
230.534774	9428.441788	27.147316
230.354803	9446.992307	27.152333
230.561602	9453.735276	27.157351
230.925637	9489.633458	27.162368
231.299772	9491.553655	27.167386
231.811736	9506.696802	27.172404
231.741614	9522.594606	27.177421
232.236553	9537.832751	27.182439
232.772687	9522.585555	27.187456
232.721161	9551.014824	27.192474
233.119544	9545.733554	27.197492
232.964175	9560.846026	27.202509
233.440512	9568.038362	27.207527
233.442044	9591.106120	27.212544
233.634221	9607.239496	27.217562
234.050946	9612.643510	27.222580
234.123235	9621.412544	27.227597
234.093390	9657.859800	27.232615
234.052776	9665.603092	27.237632
234.124344	9694.303708	27.242650
234.832540	9703.800265	27.247668
234.660616	9714.941142	27.252685
235.054061	9742.689955	27.257703
235.632921	9785.004962	27.262720
235.546696	9795.604796	27.267738
236.018915	9812.720000	27.272756
236.374084	9831.739421	27.277773
236.650776	9843.866449	27.282791
236.888528	9868.856844	27.287808
236.896930	9874.491458	27.292826
237.303562	9885.463611	27.297844
237.889953	9907.438808	27.302861
238.077658	9911.678797	27.307879
238.402119	9927.422806	27.312896
238.589137	9938.450185	27.317914
238.806537	9955.489496	27.322932
238.801312	9974.108639	27.327949
239.063471	9971.224540	27.332967
239.486532	10003.128562	27.337984
239.451152	10016.829839	27.343002
239.955053	10037.683822	27.348020
240.168938	10051.269904	27.353037
240.439336	10075.817288	27.358055
240.874678	10086.884083	27.363072
240.549444	10080.936892	27.368090
240.882841	10125.295615	27.373108
240.823915	10127.097614	27.378125
241.193665	10147.029489	27.383143
241.669876	10159.877596	27.388160
241.685612	10169.725934	27.393178
242.254330	10199.983681	27.398196
242.472412	10202.747355	27.403213
242.725742	10224.263671	27.408231
243.387080	10243.510262	27.413248
243.257546	10260.653694	27.418266
243.679023	10264.164362	27.423284
243.661307	10289.894722	27.428301
243.936017	10296.901731	27.433319
244.377428	10320.499655	27.438336
243.975908	10337.529785	27.443354
244.585518	10354.696130	27.448372
244.816881	10355.860219	27.453389
244.645816	10390.269548	27.458407
245.300894	10388.997433	27.463424
245.311665	10424.409444	27.468442
245.566309	10419.836924	27.473460
246.097219	10446.892362	27.478477
246.289104	10452.475598	27.483495
246.805849	10470.823975	27.488512
246.748915	10471.679672	27.493530
247.315706	10487.324334	27.498548
247.630801	10504.196069	27.503565
247.505524	10510.256292	27.508583
247.579536	10525.844565	27.513600
247.657418	10533.971998	27.518618
248.393736	10575.347014	27.523636
248.374763	10581.109281	27.528653
248.772100	10595.989630	27.533671
248.823047	10614.274923	27.538688
248.725155	10632.963710	27.543706
249.488309	10646.138958	27.548724
249.615298	10660.329902	27.553741
249.945959	10689.864637	27.558759
250.447211	10691.471745	27.563776
250.472071	10726.294477	27.568794
250.978466	10723.783434	27.573812
251.196960	10752.601894	27.578829
251.265098	10767.672279	27.583847
251.847695	10788.928579	27.588864
251.919705	10792.386038	27.593882
252.118779	10804.169796	27.598900
252.641872	10809.733882	27.603917
252.762939	10846.313314	27.608935
252.949091	10844.149766	27.613952
253.343286	10874.184779	27.618970
253.659577	10867.548394	27.623988
253.680753	10895.341824	27.629005
253.848354	10899.893394	27.634023
254.246161	10914.718824	27.639040
254.577635	10935.054230	27.644058
254.747272	10935.245500	27.649076
254.924488	10965.623742	27.654093
255.347261	10968.652275	27.659111
255.783726	11001.228003	27.664128
255.861115	10994.142656	27.669146
256.004388	11027.416742	27.674164
256.347020	11043.783514	27.679181
256.675228	11045.922601	27.684199
256.991687	11076.403295	27.689216
256.825427	11079.726098	27.694234
257.528858	11098.824985	27.699252
257.520537	11099.304819	27.704269
257.464483	11127.400504	27.709287
257.777430	11138.137722	27.714304
257.933682	11151.269511	27.719322
258.035790	11176.824749	27.724340
258.684321	11201.996714	27.729357
258.808834	11228.572372	27.734375
259.171729	11227.020779	27.739392
259.543538	11264.972132	27.744410
260.088922	11267.613385	27.749428
260.323413	11289.616342	27.754445
260.452364	11286.476738	27.759463
261.123910	11312.398143	27.764480
261.064695	11320.216207	27.769498
261.499354	11324.098319	27.774516
261.402226	11344.494033	27.779533
261.588633	11356.328344	27.784551
262.113124	11376.106219	27.789568
262.313994	11381.993938	27.794586
262.567180	11398.668101	27.799604
262.933165	11407.933919	27.804621
262.744212	11420.404552	27.809639
263.312858	11421.505907	27.814656
263.824178	11454.861080	27.819674
264.063049	11450.596515	27.824692
264.057208	11464.561984	27.829709
264.034482	11489.899663	27.834727
264.086940	11495.366873	27.839744
264.580194	11507.719346	27.844762
264.899618	11528.302487	27.849780
265.097618	11554.351364	27.854797
265.273883	11577.087483	27.859815
265.538135	11600.633863	27.864832
265.679312	11619.852267	27.869850
265.840202	11644.170448	27.874868
266.384379	11641.805847	27.879885
266.510022	11678.495136	27.884903
266.966002	11688.574958	27.889920
266.821017	11715.054157	27.894938
267.003965	11731.020270	27.899956
267.689527	11748.839647	27.904973
267.941641	11793.975833	27.909991
267.982181	11796.744700	27.915008
268.406418	11837.842125	27.920026
268.624364	11844.375516	27.925044
268.928025	11874.963044	27.930061
269.445483	11893.776934	27.935079
269.777038	11920.903264	27.940096
269.716549	11939.108439	27.945114
270.043957	11963.097880	27.950132
270.741388	11973.172651	27.955149
270.932810	12007.922601	27.960167
271.375012	12013.190100	27.965184
271.364534	12034.501148	27.970202
271.781176	12043.208319	27.975220
272.267265	12060.703357	27.980237
272.586816	12085.268560	27.985255
273.276474	12090.530651	27.990272
273.183381	12110.870741	27.995290
273.221030	12116.743947	28.000308
273.831586	12130.567193	28.005325
273.838564	12152.414347	28.010343
274.165100	12155.223468	28.015360
274.451343	12170.382032	28.020378
274.579741	12187.258035	28.025396
274.761612	12190.020952	28.030413
275.012532	12219.259733	28.035431
275.618892	12232.742656	28.040448
275.958164	12271.029487	28.045466
275.969282	12270.158259	28.050484
276.114630	12294.567438	28.055501
276.408970	12321.255501	28.060519
276.815850	12333.756808	28.065536
276.873480	12347.680261	28.070554
276.928771	12364.032051	28.075572
277.678106	12395.148017	28.080589
277.148676	12408.977084	28.085607
278.046935	12433.056469	28.090624
278.361295	12438.199491	28.095642
278.627572	12459.348786	28.100660
279.145792	12482.961644	28.105677
279.253565	12488.939205	28.110695
279.364408	12507.509035	28.115712
279.566492	12525.004237	28.120730
280.179823	12550.465386	28.125748
280.699487	12553.854783	28.130765
280.581652	12578.303936	28.135783
281.274479	12582.647104	28.140800
281.430970	12596.249564	28.145818
281.390591	12615.916689	28.150836
281.892846	12619.979387	28.155853
281.780338	12625.657793	28.160871
282.276341	12655.483174	28.165888
282.210191	12674.116314	28.170906
282.330300	12704.998876	28.175924
282.687079	12717.741161	28.180941
282.820040	12734.899806	28.185959
283.406196	12766.264824	28.190976
283.463989	12780.265042	28.195994
283.639711	12811.840551	28.201012
284.284025	12820.562527	28.206029
284.367099	12864.765384	28.211047
284.438584	12878.461695	28.216064
285.110123	12910.132737	28.221082
285.621418	12914.888864	28.226100
285.739903	12944.404521	28.231117
286.066574	12958.381741	28.236135
286.702394	12976.156350	28.241152
287.264525	12983.419577	28.246170
287.241274	13008.752649	28.251188
287.458221	13032.806846	28.256205
287.721360	13048.514438	28.261223
288.059480	13055.850159	28.266240
288.432686	13083.804295	28.271258
288.567124	13087.075466	28.276276
288.586814	13108.828070	28.281293
288.716232	13124.337240	28.286311
289.058910	13152.077524	28.291328
289.660702	13177.191785	28.296346
289.888294	13204.604533	28.301364
290.467243	13214.828872	28.306381
290.657531	13240.476033	28.311399
290.696062	13260.510638	28.316416
290.970765	13269.404221	28.321434
291.196890	13311.977509	28.326452
291.909944	13319.916333	28.331469
291.806141	13327.563903	28.336487
292.591592	13359.638500	28.341504
292.835764	13363.692820	28.346522
292.790032	13391.307822	28.351540
293.716126	13416.621772	28.356557
293.614899	13415.894309	28.361575
293.839758	13450.011588	28.366592
294.622548	13453.873738	28.371610
294.715043	13477.585182	28.376628
294.927608	13511.966972	28.381645
295.169609	13515.642741	28.386663
295.448181	13548.389185	28.391680
295.427000	13548.386695	28.396698
295.686831	13590.206703	28.401716
295.921064	13600.065170	28.406733
296.255111	13637.393377	28.411751
296.599487	13654.760729	28.416768
297.208428	13667.967117	28.421786
297.358127	13690.766554	28.426804
297.606924	13683.353111	28.431821
297.717330	13727.678298	28.436839
298.022889	13734.235015	28.441856
298.946273	13767.213357	28.446874
299.031503	13769.036854	28.451892
299.058599	13792.827321	28.456909
299.209187	13827.217659	28.461927
299.299334	13832.131881	28.466944
299.600207	13855.694427	28.471962
300.136492	13886.215838	28.476980
300.083692	13904.575595	28.481997
300.298770	13920.628393	28.487015
300.806866	13962.562768	28.492032
301.044806	13971.127187	28.497050
301.222715	14001.656026	28.502068
301.985807	14017.051121	28.507085
302.338151	14037.217627	28.512103
302.594214	14069.271589	28.517120
302.810374	14083.531193	28.522138
302.813811	14127.676606	28.527156
303.177327	14129.001932	28.532173
303.358873	14162.968724	28.537191
303.606040	14192.214862	28.542208
304.137042	14193.548764	28.547226
304.414429	14240.093197	28.552244
304.930698	14256.567715	28.557261
305.002767	14289.038568	28.562279
305.280509	14308.376288	28.567296
306.027511	14312.562866	28.572314
306.464472	14348.273176	28.577332
306.651588	14367.098061	28.582349
306.616925	14398.061434	28.587367
306.988059	14414.687729	28.592384
307.420723	14440.621361	28.597402
307.695459	14463.722687	28.602420
308.265482	14486.288348	28.607437
308.598317	14493.871422	28.612455
308.986197	14526.656153	28.617472
309.188038	14537.549525	28.622490
309.337658	14575.658861	28.627508
309.830722	14592.498410	28.632525
310.244202	14610.618051	28.637543
310.101161	14629.307118	28.642560
310.664203	14658.631127	28.647578
310.505586	14682.872743	28.652596
310.919688	14720.655083	28.657613
311.319864	14736.096644	28.662631
311.716845	14776.026595	28.667648
311.879225	14790.814144	28.672666
312.189374	14827.988317	28.677684
312.745514	14838.711475	28.682701
313.216321	14863.575817	28.687719
313.536283	14891.317329	28.692736
313.970186	14909.172347	28.697754
314.151093	14942.529466	28.702772
314.432383	14937.828360	28.707789
314.546082	14968.881769	28.712807
314.703409	14992.926675	28.717824
315.254290	15025.846221	28.722842
315.324379	15041.520675	28.727860
315.961315	15080.296051	28.732877
316.434207	15099.619811	28.737895
316.410139	15122.675317	28.742912
317.138246	15162.754796	28.747930
317.243035	15187.346029	28.752948
317.784484	15205.182030	28.757965
318.251751	15210.037519	28.762983
318.531861	15236.043328	28.768000
318.907278	15253.889479	28.773018
319.290170	15275.902522	28.778036
319.239163	15292.177135	28.783053
319.882897	15304.704659	28.788071
320.025387	15344.050866	28.793088
320.578572	15329.424146	28.798106
320.693641	15366.715304	28.803124
320.740593	15363.461604	28.808141
321.299036	15391.823279	28.813159
321.569118	15416.102320	28.818176
321.772254	15444.384112	28.823194
322.082562	15454.673960	28.828212
322.383005	15479.592608	28.833229
322.518147	15482.796389	28.838247
322.534395	15506.101068	28.843264
322.879067	15539.716013	28.848282
323.238460	15569.078467	28.853300
323.698526	15602.277358	28.858317
323.750100	15620.932260	28.863335
324.023923	15634.758217	28.868352
324.918306	15668.455958	28.873370
324.863657	15691.684366	28.878388
325.377839	15719.086332	28.883405
326.128708	15738.316077	28.888423
326.542219	15756.930250	28.893440
326.976965	15780.429356	28.898458
327.205882	15794.576471	28.903476
327.615336	15819.981917	28.908493
327.589411	15821.091218	28.913511
327.928096	15855.008801	28.918528
328.528149	15849.914378	28.923546
328.443094	15897.647059	28.928564
328.729077	15902.483855	28.933581
329.411807	15943.515152	28.938599
329.497252	15955.419953	28.943616
330.090171	15993.246629	28.948634
330.214339	16001.588229	28.953652
330.469815	16031.567534	28.958669
330.892348	16046.592186	28.963687
330.963340	16084.549427	28.968704
331.453969	16097.351856	28.973722
331.931421	16136.829023	28.978740
331.756453	16162.976111	28.983757
332.440607	16168.484740	28.988775
332.624461	16209.231934	28.993792
332.845982	16235.236413	28.998810
333.094834	16277.495395	29.003828
333.473963	16303.505463	29.008845
334.097925	16323.552721	29.013863
334.193471	16364.403144	29.018880
334.601998	16372.070728	29.023898
334.957264	16418.906390	29.028916
335.424308	16445.258327	29.033933
335.710743	16474.188471	29.038951
335.813669	16505.297021	29.043968
336.103521	16522.181605	29.048986
336.404801	16568.394653	29.054004
336.867039	16587.978828	29.059021
337.428372	16636.965368	29.064039
337.624429	16659.551711	29.069056
338.429141	16688.499050	29.074074
338.877205	16701.611576	29.079092
338.894398	16732.274535	29.084109
339.625040	16729.690878	29.089127
340.041176	16770.738359	29.094144
340.470552	16768.243867	29.099162
340.550377	16810.557367	29.104180
341.067436	16811.791365	29.109197
341.305694	16847.119205	29.114215
341.689907	16866.414014	29.119232
341.904253	16874.556771	29.124250
341.985798	16903.242573	29.129268
341.950477	16938.552767	29.134285
342.667448	16951.592702	29.139303
342.944871	16988.925361	29.144320
343.419281	17012.457516	29.149338
343.613189	17026.011023	29.154356
343.931563	17055.613030	29.159373
343.857853	17075.924620	29.164391
344.281310	17109.091653	29.169408
344.945301	17131.331843	29.174426
345.049673	17160.099429	29.179444
345.496160	17186.812141	29.184461
346.047924	17189.640106	29.189479
346.105198	17238.491078	29.194496
346.467467	17245.843631	29.199514
346.635505	17272.400752	29.204532
346.975317	17315.377094	29.209549
347.476255	17336.274921	29.214567
347.441931	17379.340032	29.219584
348.257326	17390.256884	29.224602
348.296044	17442.463784	29.229620
348.259522	17495.887389	29.234637
349.080669	17500.812769	29.239655
349.344935	17553.944157	29.244672
349.525900	17568.267795	29.249690
350.373428	17622.691562	29.254708
350.616727	17646.091018	29.259725
351.012294	17684.959752	29.264743
351.406006	17705.073542	29.269760
351.782299	17726.501533	29.274778
352.221344	17743.110558	29.279796
352.740708	17766.628492	29.284813
353.127581	17809.891506	29.289831
353.311051	17822.503320	29.294848
353.478905	17858.776440	29.299866
353.834073	17893.526131	29.304884
354.321767	17921.743136	29.309901
354.779922	17962.447800	29.314919
354.734656	17985.985251	29.319936
355.084369	18018.461788	29.324954
355.307826	18053.564560	29.329972
355.620151	18087.894614	29.334989
356.147075	18131.765784	29.340007
356.821771	18155.115187	29.345024
357.199275	18190.381936	29.350042
357.246034	18217.950429	29.355060
357.717691	18277.192063	29.360077
358.393966	18287.613955	29.365095
358.550571	18326.241556	29.370112
358.859844	18331.975204	29.375130
359.198218	18377.971293	29.380148
360.036154	18394.286540	29.385165
360.461046	18429.498689	29.390183
360.880073	18452.829284	29.395200
361.189581	18456.137242	29.400218
361.586427	18493.907526	29.405236
362.084402	18513.932580	29.410253
362.789428	18537.056855	29.415271
363.206741	18555.325260	29.420288
363.565282	18577.009480	29.425306
363.872071	18591.954722	29.430324
363.738313	18604.023754	29.435341
364.172422	18635.669538	29.440359
364.117541	18652.044273	29.445376
364.246811	18690.240645	29.450394
365.166253	18708.196146	29.455412
365.522936	18749.958222	29.460429
365.994815	18762.568821	29.465447
366.044115	18802.748890	29.470464
366.559323	18815.056048	29.475482
366.992002	18862.940367	29.480500
367.056750	18884.028866	29.485517
367.315548	18905.871854	29.490535
367.662527	18942.852276	29.495552
368.029410	18964.374856	29.500570
368.260285	18984.433576	29.505588
368.589984	19024.911474	29.510605
368.844433	19060.217754	29.515623
368.937912	19079.634128	29.520640
369.483156	19109.396230	29.525658
370.010148	19116.968303	29.530676
370.424250	19158.822806	29.535693
370.641430	19185.256681	29.540711
370.903120	19227.651961	29.545728
371.215148	19256.087846	29.550746
371.847886	19307.155906	29.555764
371.755241	19330.417803	29.560781
372.346789	19382.066648	29.565799
372.525682	19412.031680	29.570816
373.137126	19458.304071	29.575834
373.891966	19476.486213	29.580852
373.938942	19525.783865	29.585869
374.652228	19539.986601	29.590887
374.657327	19584.989751	29.595904
375.389106	19607.127527	29.600922
376.424176	19651.941792	29.605940
376.302842	19688.790029	29.610957
376.644246	19709.004759	29.615975
377.002510	19734.670629	29.620992
377.153604	19762.665820	29.626010
378.123757	19782.508803	29.631028
378.230311	19832.292474	29.636045
378.870220	19844.258243	29.641063
379.296639	19884.903541	29.646080
379.565667	19919.878227	29.651098
380.372646	19923.496798	29.656116
380.343991	19971.551966	29.661133
380.865705	19973.910926	29.666151
380.945508	20020.130850	29.671168
381.375939	20050.872007	29.676186
381.959127	20080.249703	29.681204
382.123723	20101.056861	29.686221
382.647440	20108.379302	29.691239
383.163888	20141.576492	29.696256
383.776690	20158.529686	29.701274
384.343785	20191.532605	29.706292
384.291168	20204.309772	29.711309
384.441044	20244.547658	29.716327
384.760286	20262.094862	29.721344
385.152330	20316.178744	29.726362
386.175727	20326.366468	29.731380
386.242755	20367.181086	29.736397
386.550968	20386.584011	29.741415
387.033684	20415.145019	29.746432
387.104762	20441.675970	29.751450
387.740642	20474.338634	29.756468
387.721451	20505.336191	29.761485
388.087673	20535.120978	29.766503
388.683413	20568.846612	29.771520
388.979429	20600.506362	29.776538
389.461720	20634.994912	29.781556
389.662207	20665.988004	29.786573
390.081578	20685.878928	29.791591
390.617023	20726.122068	29.796608
391.199921	20764.938733	29.801626
391.433590	20776.819382	29.806644
391.830690	20818.795964	29.811661
392.315727	20844.184085	29.816679
392.714509	20878.500923	29.821696
392.783720	20906.905665	29.826714
393.349336	20929.893961	29.831732
394.132229	20967.393307	29.836749
394.213751	20971.713648	29.841767
394.516452	20994.698175	29.846784
395.027532	21036.725839	29.851802
395.491754	21044.290256	29.856820
395.581114	21084.194940	29.861837
396.287531	21103.193994	29.866855
396.276299	21129.325045	29.871872
396.378923	21160.158668	29.876890
397.131071	21196.005229	29.881908
397.242378	21225.987853	29.886925
397.384767	21252.183575	29.891943
398.107509	21293.120722	29.896960
398.182948	21338.301438	29.901978
398.765972	21374.572005	29.906996
399.267884	21403.027497	29.912013
399.430612	21442.353402	29.917031
400.057909	21482.021987	29.922048
400.362998	21517.544255	29.927066
400.699615	21569.858413	29.932084
400.982589	21607.410259	29.937101
401.215552	21640.196951	29.942119
402.034049	21686.611609	29.947136
402.272304	21730.079679	29.952154
403.150978	21757.395237	29.957172
403.040400	21802.532267	29.962189
403.375268	21821.549382	29.967207
404.424066	21876.680662	29.972224
404.551119	21909.981969	29.977242
405.156636	21943.849084	29.982260
405.872994	21983.166781	29.987277
406.421937	21993.293614	29.992295
406.864264	22040.952187	29.997312
407.324650	22061.730275	30.002330
407.806474	22093.814620	30.007348
407.669371	22120.967513	30.012365
407.845674	22162.432178	30.017383
408.483186	22180.601996	30.022400
408.492992	22236.222978	30.027418
409.028520	22274.838159	30.032436
409.437866	22306.479273	30.037453
409.925799	22352.810081	30.042471
410.260913	22403.597872	30.047488
410.484235	22437.270574	30.052506
411.217968	22463.083578	30.057524
411.541690	22529.858079	30.062541
412.266607	22544.745696	30.067559
413.127237	22579.986111	30.072576
413.342012	22609.036576	30.077594
414.313815	22614.719025	30.082612
414.271420	22655.625105	30.087629
414.577239	22673.782463	30.092647
415.121767	22717.491012	30.097664
415.344530	22746.428460	30.102682
415.999990	22773.886611	30.107700
416.209155	22810.963041	30.112717
416.713659	22851.396148	30.117735
417.408844	22885.636617	30.122752
417.176084	22907.487238	30.127770
417.622424	22945.756088	30.132788
418.232013	22986.952567	30.137805
418.580835	22987.592106	30.142823
418.630272	23041.024069	30.147840
418.932028	23071.903994	30.152858
419.356677	23126.584390	30.157876
419.506751	23146.760802	30.162893
420.007987	23204.788524	30.167911
420.903903	23220.350084	30.172928
421.087544	23275.811781	30.177946
421.320586	23312.202702	30.182964
421.857108	23355.611527	30.187981
422.457851	23383.387156	30.192999
422.750274	23421.865404	30.198016
423.267058	23459.548322	30.203034
423.494051	23495.358864	30.208052
423.561159	23530.331901	30.213069
423.768439	23575.394385	30.218087
424.813861	23613.468040	30.223104
424.813604	23674.113881	30.228122
425.552693	23705.017322	30.233140
425.520045	23752.729264	30.238157
425.991797	23795.364751	30.243175
426.588148	23831.096071	30.248192
426.805767	23898.860028	30.253210
427.413573	23926.670075	30.258228
428.379233	23978.867335	30.263245
428.508605	24027.707414	30.268263
429.106893	24062.117650	30.273280
429.475200	24121.174833	30.278298
429.846543	24157.413868	30.283316
430.253456	24201.612554	30.288333
430.704675	24245.811921	30.293351
431.410432	24273.557484	30.298368
431.515259	24320.272341	30.303386
432.063958	24361.427060	30.308404
432.445894	24403.361519	30.313421
432.405842	24454.780362	30.318439
433.289520	24497.139872	30.323456
433.628155	24553.061063	30.328474
434.005243	24604.904969	30.333492
434.549554	24631.143630	30.338509
434.918690	24696.478084	30.343527
435.708242	24721.320380	30.348544
435.801174	24786.543133	30.353562
436.832446	24819.483238	30.358580
437.199836	24853.107012	30.363597
437.937167	24896.511860	30.368615
438.430134	24922.563939	30.373632
439.017878	24965.334589	30.378650
438.916006	24981.909337	30.383668
440.098954	25020.349765	30.388685
440.266297	25050.995351	30.393703
440.629800	25086.523395	30.398720
440.813580	25137.180440	30.403738
441.358281	25161.425235	30.408756
441.794723	25198.332187	30.413773
442.228152	25246.199981	30.418791
442.950527	25269.783289	30.423808
443.254003	25325.941475	30.428826
443.490974	25353.394128	30.433844
443.991935	25403.004610	30.438861
444.489557	25435.140023	30.443879
445.059511	25455.347595	30.448896
445.239958	25499.714804	30.453914
445.530242	25537.345166	30.458932
445.976059	25597.790179	30.463949
446.267136	25627.828212	30.468967
446.863364	25675.690823	30.473984
447.015455	25717.787920	30.479002
447.460255	25752.446132	30.484020
447.892438	25795.353375	30.489037
448.344950	25861.168939	30.494055
448.985736	25883.091969	30.499072
448.954460	25950.463726	30.504090
449.398382	25991.575063	30.509108
450.441300	26041.528368	30.514125
450.585766	26090.070711	30.519143
451.388953	26121.704386	30.524160
451.811546	26160.455926	30.529178
451.855781	26198.297120	30.534196
452.454015	26234.681305	30.539213
452.871061	26276.726555	30.544231
453.384973	26326.422745	30.549248
453.370106	26366.694602	30.554266
453.839223	26416.327494	30.559284
454.313154	26458.510447	30.564301
454.362724	26506.333237	30.569319
455.322211	26549.909039	30.574336
455.801504	26607.472668	30.579354
456.151445	26649.058423	30.584372
456.991187	26696.323873	30.589389
457.099701	26755.548251	30.594407
457.275350	26792.501744	30.599424
458.283526	26840.182888	30.604442
458.378255	26882.249757	30.609460
458.886210	26944.676230	30.614477
459.281076	26990.781235	30.619495
460.193513	27039.989473	30.624512
460.348992	27096.797686	30.629530
460.867380	27136.234212	30.634548
461.740463	27189.931117	30.639565
462.209916	27241.651106	30.644583
462.796776	27274.866518	30.649600
462.999216	27347.491205	30.654618
463.242212	27369.857184	30.659636
464.194886	27411.209610	30.664653
464.626190	27464.791115	30.669671
465.302193	27501.874805	30.674688
465.871560	27551.380891	30.679706
466.133898	27599.600534	30.684724
466.563368	27628.313467	30.689741
466.576280	27679.413155	30.694759
467.498580	27729.407103	30.699776
467.846849	27790.992526	30.704794
468.133031	27823.233604	30.709812
468.898549	27878.344532	30.714829
469.151487	27924.828752	30.719847
469.508544	27977.581987	30.724864
469.923522	28019.154020	30.729882
470.019537	28069.515699	30.734900
470.926124	28116.330884	30.739917
471.170599	28161.094998	30.744935
471.598580	28228.535482	30.749952
472.121746	28272.938438	30.754970
472.614746	28338.750542	30.759988
473.303463	28376.606792	30.765005
474.039101	28434.023821	30.770023
474.398311	28481.454012	30.775040
474.659427	28528.831146	30.780058
475.149021	28579.192387	30.785076
476.578862	28619.822302	30.790093
476.815484	28645.483984	30.795111
477.652500	28682.657184	30.800128
478.097313	28734.054550	30.805146
478.507384	28766.948784	30.810164
479.006050	28811.256242	30.815181
479.655287	28838.947623	30.820199
479.848590	28888.043393	30.825216
480.364848	28934.161956	30.830234
480.769723	28967.423326	30.835252
481.050645	29012.467517	30.840269
481.608307	29043.662981	30.845287
482.101572	29096.649490	30.850304
483.101039	29114.117192	30.855322
483.009684	29167.638936	30.860340
483.673323	29191.918706	30.865357
484.046786	29216.508251	30.870375
484.140697	29248.171825	30.875392
484.489664	29285.417483	30.880410
484.545951	29321.806274	30.885428
485.514580	29372.749962	30.890445
485.785514	29423.348513	30.895463
486.251386	29478.208093	30.900480
486.822694	29501.386909	30.905498
487.409120	29554.901987	30.910516
488.065078	29589.728658	30.915533
488.186868	29643.588883	30.920551
488.850364	29675.152844	30.925568
489.643424	29728.176939	30.930586
489.711886	29783.216691	30.935604
490.026128	29811.378200	30.940621
490.525661	29880.330601	30.945639
491.090129	29909.737945	30.950656
491.498943	29979.923340	30.955674
491.752577	30033.406545	30.960692
492.330786	30081.653509	30.965709
492.806597	30140.832016	30.970727
493.168079	30203.594184	30.975744
493.775018	30243.654107	30.980762
494.262929	30321.121018	30.985780
495.182930	30363.649962	30.990797
495.418823	30428.673398	30.995815
496.190579	30466.539449	31.000832
496.692686	30518.831701	31.005850
497.207063	30573.961186	31.010868
497.974709	30588.806236	31.015885
498.503386	30641.782164	31.020903
498.887324	30695.006138	31.025920
499.452303	30748.307625	31.030938
499.891706	30802.242011	31.035956
500.670557	30850.817598	31.040973
500.750991	30911.392130	31.045991
501.237761	30950.167523	31.051008
501.647899	30997.763398	31.056026
502.288955	31057.176413	31.061044
502.988679	31109.251676	31.066061
503.304316	31162.523063	31.071079
503.828340	31213.943099	31.076096
504.746275	31252.490212	31.081114
504.771038	31317.148044	31.086132
505.468405	31340.671292	31.091149
506.242373	31404.521126	31.096167
506.774635	31442.195418	31.101184
507.467750	31488.004488	31.106202
507.629115	31533.100212	31.111220
508.331400	31576.693380	31.116237
508.673433	31626.125662	31.121255
508.997566	31683.652993	31.126272
509.482425	31714.489879	31.131290
509.677885	31779.887837	31.136308
510.386548	31819.268933	31.141325
510.619406	31893.567093	31.146343
511.263335	31934.612256	31.151360
511.954727	31983.060328	31.156378
511.888400	32053.335724	31.161396
512.870866	32102.117781	31.166413
513.273717	32161.920939	31.171431
513.388023	32223.958278	31.176448
514.265573	32275.805741	31.181466
514.948310	32327.953702	31.186484
515.562800	32370.613739	31.191501
515.581117	32422.818097	31.196519
515.990981	32481.920804	31.201536
516.813538	32527.720687	31.206554
517.139493	32585.074007	31.211572
517.501147	32643.667816	31.216589
518.284400	32692.900879	31.221607
518.481890	32756.522762	31.226624
519.547120	32811.577794	31.231642
519.432702	32861.325583	31.236660
520.072766	32912.598942	31.241677
520.626058	32987.883646	31.246695
521.045991	33044.544620	31.251712
521.630449	33093.404651	31.256730
522.109588	33157.274879	31.261748
522.973811	33197.084552	31.266765
523.112188	33260.885241	31.271783
523.958923	33340.634698	31.276800
524.392507	33376.307065	31.281818
525.000719	33439.409248	31.286836
525.542233	33486.510624	31.291853
526.069794	33555.554947	31.296871
526.507434	33606.519863	31.301888
527.344569	33667.897073	31.306906
527.779885	33718.711252	31.311924
528.408921	33770.913389	31.316941
528.912803	33838.107513	31.321959
529.163078	33885.904868	31.326976
529.755186	33969.438091	31.331994
529.952550	34030.076653	31.337012
530.843373	34083.703635	31.342029
531.582597	34150.651834	31.347047
531.798423	34205.551794	31.352064
532.712760	34276.024313	31.357082
533.258863	34320.211733	31.362100
533.704437	34379.497920	31.367117
534.314998	34439.097822	31.372135
534.614234	34506.126355	31.377152
535.516421	34548.491738	31.382170
535.776179	34612.485513	31.387188
536.240356	34686.618428	31.392205
536.921008	34734.236555	31.397223
537.576562	34812.528633	31.402240
538.321575	34848.203023	31.407258
538.653598	34921.383755	31.412276
539.142615	34959.814246	31.417293
539.877350	35041.300088	31.422311
540.397801	35086.967215	31.427328
541.102095	35146.610815	31.432346
541.448066	35196.109275	31.437364
541.960184	35260.167834	31.442381
542.461658	35313.165516	31.447399
543.228836	35366.472877	31.452416
543.910440	35427.247653	31.457434
544.106145	35486.272740	31.462452
544.416675	35551.094552	31.467469
545.417353	35606.497150	31.472487
545.712337	35676.963953	31.477504
546.252054	35722.579047	31.482522
546.407893	35795.789328	31.487540
546.908403	35855.068221	31.492557
547.868888	35915.413632	31.497575
547.837098	35979.735022	31.502592
548.509972	36040.014763	31.507610
548.952828	36125.400390	31.512628
549.262223	36189.397959	31.517645
550.042072	36254.106945	31.522663
550.838183	36330.650089	31.527680
551.029744	36387.492025	31.532698
551.694971	36457.458976	31.537716
552.080147	36511.732217	31.542733
552.541940	36577.239637	31.547751
553.296187	36656.132571	31.552768
553.973871	36715.877344	31.557786
554.479294	36769.352060	31.562804
554.632785	36851.573333	31.567821
555.523818	36912.612066	31.572839
556.111752	36964.719946	31.577856
556.760913	37031.870607	31.582874
557.474586	37096.293786	31.587892
557.832205	37162.751497	31.592909
558.480115	37214.212740	31.597927
558.822411	37290.134379	31.602944
559.270765	37353.482013	31.607962
559.960673	37428.336976	31.612980
560.420512	37477.807185	31.617997
561.068610	37565.791411	31.623015
561.643222	37640.836719	31.628032
562.249266	37706.008863	31.633050
562.425559	37776.251081	31.638068
563.297990	37845.548603	31.643085
563.960837	37950.715920	31.648103
564.353641	38004.676839	31.653120
565.316758	38072.233989	31.658138
565.757967	38144.677733	31.663156
565.853950	38212.798372	31.668173
566.553466	38285.938505	31.673191
567.309122	38350.804243	31.678208
568.350208	38428.707667	31.683226
569.076163	38478.120898	31.688244
569.412696	38549.217026	31.693261
570.195174	38612.655933	31.698279
570.650627	38692.333057	31.703296
571.256677	38745.235275	31.708314
571.802362	38828.653754	31.713332
572.140334	38911.175895	31.718349
572.728488	38952.328579	31.723367
573.182805	39034.699514	31.728384
573.885844	39102.073095	31.733402
574.531806	39188.263489	31.738420
575.069191	39247.323429	31.743437
576.302245	39321.913508	31.748455
576.177089	39394.285388	31.753472
577.071472	39457.475230	31.758490
577.254520	39526.631127	31.763508
578.079507	39604.591106	31.768525
578.874583	39666.926982	31.773543
579.121595	39738.036262	31.778560
579.724867	39793.116620	31.783578
580.341497	39870.676604	31.788596
580.667971	39941.855620	31.793613
581.743484	39992.528251	31.798631
582.444096	40084.275164	31.803648
583.029849	40133.444646	31.808666
583.803954	40211.434579	31.813684
583.979865	40298.777871	31.818701
584.815201	40359.351431	31.823719
584.953525	40415.978153	31.828736
585.531795	40476.818661	31.833754
585.933245	40548.322239	31.838772
586.367316	40631.196162	31.843789
587.367035	40695.657556	31.848807
587.884495	40789.455191	31.853824
588.510314	40843.543914	31.858842
589.071783	40933.061284	31.863860
589.889454	40985.726773	31.868877
590.483855	41064.551774	31.873895
591.090795	41123.742061	31.878912
591.805297	41190.190363	31.883930
592.524404	41246.786871	31.888948
592.486191	41316.203915	31.893965
593.532744	41368.801145	31.898983
594.080683	41438.210222	31.904000
594.687189	41486.720231	31.909018
595.352671	41564.430882	31.914036
595.714656	41618.174075	31.919053
596.359661	41679.398986	31.924071
596.698334	41751.189112	31.929088
597.492495	41805.136093	31.934106
598.001332	41874.935229	31.939124
598.386228	41955.572665	31.944141
599.329394	42019.120052	31.949159
599.438460	42096.580797	31.954176
600.271963	42161.497814	31.959194
600.729524	42246.123947	31.964212
601.061963	42330.414436	31.969229
601.699964	42387.406670	31.974247
601.913086	42476.487228	31.979264
602.876515	42546.646303	31.984282
603.453027	42640.014372	31.989300
603.995220	42719.625361	31.994317
604.983962	42796.729113	31.999335
605.694862	42879.453862	32.004352
606.340383	42939.641179	32.009370
606.940577	43029.948438	32.014388
607.550841	43099.561861	32.019405
608.178262	43167.183943	32.024423
608.798994	43254.865631	32.029440
609.385142	43313.668677	32.034458
610.391069	43392.628292	32.039476
610.931251	43462.844989	32.044493
611.771507	43524.504708	32.049511
612.187550	43620.088787	32.054528
612.978519	43675.471853	32.059546
613.743828	43746.539527	32.064564
614.057193	43813.054120	32.069581
614.924184	43891.034928	32.074599
615.245632	43964.348698	32.079616
616.096493	44036.217842	32.084634
616.577389	44104.284277	32.089652
616.851275	44187.102859	32.094669
617.705150	44259.698473	32.099687
618.122061	44328.871768	32.104704
618.565404	44422.804391	32.109722
619.522673	44482.771623	32.114740
619.468188	44575.404473	32.119757
620.422037	44631.281256	32.124775
621.218707	44728.336199	32.129792
621.935663	44796.078898	32.134810
622.656103	44880.310640	32.139828
622.760073	44958.166246	32.144845
623.895816	45029.070325	32.149863
624.520118	45110.161894	32.154880
625.337866	45189.873776	32.159898
625.973837	45252.333865	32.164916
626.587423	45343.594196	32.169933
627.375778	45403.690178	32.174951
627.590695	45480.674057	32.179968
628.568278	45548.351198	32.184986
629.043339	45633.321463	32.190004
629.503797	45708.734489	32.195021
630.185691	45771.090862	32.200039
630.575804	45857.238035	32.205056
631.276222	45926.900873	32.210074
632.434713	45997.997486	32.215092
632.565422	46092.163827	32.220109
633.520050	46148.900672	32.225127
633.572131	46232.737443	32.230144
634.129150	46299.653248	32.235162
634.487333	46367.782971	32.240180
634.983787	46457.656778	32.245197
635.826865	46542.283081	32.250215
636.023061	46606.045392	32.255232
636.715186	46707.996574	32.260250
637.642422	46776.829462	32.265268
637.857570	46884.856270	32.270285
638.868300	46955.219998	32.275303
639.204485	47040.535339	32.280320
640.054141	47132.674766	32.285338
640.631241	47206.009594	32.290356
641.111812	47310.537594	32.295373
641.920257	47393.117941	32.300391
642.684782	47491.518716	32.305408
643.660172	47572.746127	32.310426
644.485317	47663.013479	32.315444
645.053421	47739.600986	32.320461
645.920275	47826.218417	32.325479
646.921354	47900.562664	32.330496
647.373026	47987.451493	32.335514
647.688697	48052.345189	32.340532
648.056188	48136.192045	32.345549
648.927860	48216.975198	32.350567
649.647101	48318.744343	32.355584
650.167974	48401.146102	32.360602
651.071855	48488.041493	32.365620
651.585616	48569.864151	32.370637
652.188764	48655.013252	32.375655
653.150539	48737.915208	32.380672
653.816360	48829.427025	32.385690
654.353649	48906.984314	32.390708
654.811567	48982.685635	32.395725
655.435421	49076.014973	32.400743
656.305021	49165.284315	32.405760
656.906454	49253.862600	32.410778
657.570192	49349.195061	32.415796
657.605135	49427.333224	32.420813
658.412589	49507.867244	32.425831
659.238142	49608.842624	32.430848
659.928155	49706.474624	32.435866
661.213224	49788.901475	32.440884
661.815194	49893.502665	32.445901
662.639912	49968.721024	32.450919
663.207671	50039.693641	32.455936
663.888184	50140.064212	32.460954
664.734686	50184.054011	32.465972
665.286169	50295.865902	32.470989
666.045090	50374.447349	32.476007
666.608051	50467.275669	32.481024
666.760902	50539.158702	32.486042
667.421583	50639.509915	32.491060
668.113985	50730.060141	32.496077
668.652522	50799.562447	32.501095
669.247126	50912.169818	32.506112
669.546667	50997.894330	32.511130
670.527272	51108.294761	32.516148
670.881587	51202.430674	32.521165
671.654538	51304.775409	32.526183
672.113587	51399.975083	32.531200
672.518335	51507.021048	32.536218
673.181618	51608.753884	32.541236
674.076255	51717.387644	32.546253
674.637423	51810.418589	32.551271
675.811434	51940.448701	32.556288
676.245210	52027.700033	32.561306
676.667786	52126.961390	32.566324
677.303450	52231.190811	32.571341
678.074518	52309.708717	32.576359
678.866955	52415.242893	32.581376
679.452514	52511.046213	32.586394
680.593838	52598.773893	32.591412
681.273367	52699.638114	32.596429
681.616429	52790.056783	32.601447
682.611193	52867.917821	32.606464
683.253561	52971.954323	32.611482
684.131489	53052.529534	32.616500
684.506888	53160.075941	32.621517
684.954205	53249.102458	32.626535
685.746519	53357.440211	32.631552
686.478645	53451.644754	32.636570
687.326187	53543.550249	32.641588
687.573186	53654.677096	32.646605
688.650204	53747.082609	32.651623
689.152769	53861.276443	32.656640
689.505139	53964.674451	32.661658
690.492420	54062.756469	32.666676
691.265459	54181.133719	32.671693
691.708426	54299.515665	32.676711
692.996897	54381.832191	32.681728
693.212437	54499.659088	32.686746
694.177259	54587.942966	32.691764
694.442443	54700.513151	32.696781
695.073525	54792.592977	32.701799
695.841514	54920.900251	32.706816
696.519384	55026.625518	32.711834
697.420351	55143.812442	32.716852
698.016559	55239.602219	32.721869
698.493380	55363.077003	32.726887
699.937813	55468.046303	32.731904
700.261009	55567.022647	32.736922
701.291571	55672.958510	32.741940
702.094175	55785.370383	32.746957
703.094997	55896.682461	32.751975
703.956512	55988.691965	32.756992
704.166829	56081.801347	32.762010
705.287288	56200.304058	32.767028
705.836666	56297.932621	32.772045
706.880278	56406.568050	32.777063
707.785156	56495.028399	32.782080
708.184863	56588.898657	32.787098
709.123884	56679.755045	32.792116
709.898591	56773.178852	32.797133
710.353454	56880.511523	32.802151
711.384684	56963.285776	32.807168
711.732738	57074.112113	32.812186
712.670218	57152.606293	32.817204
713.380569	57260.151566	32.822221
713.764172	57359.872519	32.827239
714.797662	57443.899435	32.832256
715.414217	57572.691350	32.837274
716.394608	57650.087355	32.842292
716.913618	57763.372442	32.847309
717.474576	57845.444585	32.852327
718.527980	57943.686774	32.857344
719.068664	58043.517923	32.862362
719.739794	58129.357818	32.867380
720.767662	58246.940360	32.872397
721.302933	58340.575413	32.877415
722.147328	58422.975938	32.882432
722.486132	58508.632251	32.887450
723.208304	58615.310973	32.892468
724.192051	58691.699515	32.897485
724.825451	58799.834548	32.902503
726.228364	58862.247034	32.907520
726.975604	58953.227697	32.912538
727.876743	59034.724128	32.917556
728.383755	59102.201343	32.922573
729.009457	59192.084741	32.927591
730.087670	59256.700497	32.932608
730.306488	59334.273085	32.937626
731.085196	59433.970816	32.942644
731.682754	59513.509927	32.947661
731.851478	59604.538554	32.952679
732.618791	59680.840261	32.957696
733.461361	59797.805406	32.962714
734.042944	59894.839767	32.967732
734.390691	59986.845302	32.972749
735.042260	60096.981208	32.977767
735.904220	60195.158720	32.982784
736.421057	60297.431671	32.987802
737.244127	60401.379719	32.992820
737.935432	60516.023294	32.997837
738.432556	60611.665883	33.002855
739.435841	60735.624382	33.007872
739.722781	60849.963803	33.012890
740.761460	60955.376808	33.017908
741.425687	61062.071854	33.022925
741.674143	61180.280681	33.027943
742.387798	61300.486176	33.032960
743.467776	61420.701410	33.037978
744.056916	61550.705298	33.042996
744.975423	61665.772921	33.048013
745.569504	61792.624063	33.053031
746.379013	61914.315150	33.058048
747.201138	62030.348724	33.063066
748.253991	62159.205600	33.068084
748.968349	62275.353175	33.073101
749.547529	62382.208287	33.078119
750.334791	62501.928475	33.083136
750.984770	62628.996830	33.088154
751.709341	62745.385571	33.093172
752.572855	62880.749946	33.098189
753.349044	62998.054334	33.103207
754.368804	63112.418263	33.108224
755.043472	63240.541822	33.113242
756.107452	63346.538261	33.118260
756.689359	63491.585114	33.123277
757.344661	63607.269731	33.128295
758.412793	63731.823683	33.133312
759.226417	63835.215822	33.138330
759.612350	63962.671093	33.143348
760.853485	64081.371263	33.148365
761.400363	64189.195584	33.153383
762.540115	64310.821218	33.158400
763.152499	64419.021483	33.163418
764.123729	64543.754405	33.168436
765.008571	64638.106835	33.173453
765.577465	64763.046587	33.178471
766.384149	64859.075256	33.183488
767.222142	64968.214541	33.188506
768.170990	65091.823102	33.193524
768.675850	65196.884889	33.198541
769.026504	65319.215688	33.203559
769.739048	65420.167435	33.208576
770.763574	65567.519885	33.213594
771.381642	65667.641457	33.218612
771.986257	65797.119978	33.223629
772.386370	65909.553911	33.228647
773.543992	66046.995552	33.233664
774.111447	66162.797596	33.238682
774.939747	66300.624003	33.243700
775.745825	66391.723186	33.248717
776.270194	66512.755521	33.253735
777.658100	66619.910095	33.258752
778.521029	66724.199925	33.263770
779.235176	66829.519923	33.268788
780.138497	66932.849632	33.273805
780.572184	67046.826590	33.278823
781.386254	67158.857607	33.283840
782.189934	67275.265320	33.288858
782.983240	67389.456593	33.293876
783.882627	67504.067154	33.298893
784.541429	67618.800255	33.303911
785.957920	67722.320976	33.308928
786.461848	67840.424942	33.313946
787.130618	67938.791744	33.318964
788.149974	68061.483478	33.323981
788.518734	68163.346149	33.328999
789.732301	68289.736912	33.334016
790.200727	68406.067237	33.339034
790.757597	68525.032409	33.344052
791.566912	68636.022756	33.349069
792.007604	68763.308947	33.354087
793.310013	68894.335224	33.359104
793.532418	69015.653246	33.364122
794.205020	69144.464961	33.369140
795.324323	69283.995284	33.374157
795.666170	69424.261832	33.379175
796.568138	69544.851138	33.384192
797.404837	69684.563554	33.389210
798.121835	69825.592700	33.394228
799.127803	69955.549220	33.399245
799.728746	70104.388302	33.404263
800.267698	70215.798337	33.409280
800.779533	70375.344955	33.414298
801.901806	70498.919078	33.419316
803.209667	70648.410264	33.424333
804.187070	70778.926621	33.429351
805.187992	70921.718096	33.434368
806.154937	71038.783614	33.439386
806.525223	71180.220476	33.444404
807.800120	71294.170128	33.449421
808.445147	71439.072370	33.454439
809.032054	71546.599415	33.459456
809.831448	71693.121785	33.464474
810.456380	71839.168156	33.469492
811.408604	71964.972898	33.474509
812.014134	72113.351131	33.479527
813.100935	72252.027550	33.484544
814.114704	72376.408243	33.489562
814.707003	72508.484701	33.494580
815.641029	72635.308074	33.499597
816.580335	72790.989506	33.504615
817.150638	72921.162600	33.509632
818.022119	73056.901650	33.514650
818.386858	73213.205847	33.519668
819.776614	73332.718118	33.524685
820.401746	73497.435461	33.529703
821.403590	73615.527410	33.534720
822.198142	73769.810802	33.539738
823.111160	73887.362464	33.544756
824.167026	74024.006715	33.549773
824.735237	74165.247273	33.554791
825.662363	74305.025684	33.559808
826.459382	74437.503884	33.564826
826.592681	74577.282349	33.569844
827.769713	74706.145623	33.574861
828.762914	74848.863429	33.579879
829.551946	74991.065734	33.584896
830.331562	75115.494634	33.589914
831.236182	75249.692736	33.594932
831.996512	75369.870414	33.599949
832.995652	75498.666605	33.604967
834.513128	75615.539750	33.609984
835.042489	75730.787036	33.615002
835.940402	75852.437102	33.620020
837.015950	75974.140729	33.625037
837.810287	76096.195023	33.630055
838.545242	76220.580718	33.635072
839.038025	76335.350297	33.640090
839.588231	76469.993902	33.645108
840.826004	76595.108189	33.650125
841.513994	76737.958374	33.655143
842.193137	76848.070593	33.660160
843.061407	77009.732559	33.665178
843.367408	77140.733590	33.670196
844.527787	77287.816195	33.675213
845.317139	77428.541829	33.680231
846.045505	77570.340935	33.685248
846.634249	77715.060606	33.690266
847.130738	77861.434504	33.695284
848.050571	77991.327335	33.700301
848.790936	78150.381500	33.705319
849.844749	78312.370273	33.710336
851.198336	78455.874364	33.715354
851.993165	78616.883545	33.720372
852.899635	78762.101556	33.725389
853.674262	78898.127085	33.730407
854.539301	79058.381566	33.735424
855.829181	79184.058584	33.740442
856.834950	79342.957342	33.745460
857.784759	79478.805716	33.750477
858.513944	79615.614800	33.755495
859.153778	79774.830076	33.760512
859.889312	79914.530491	33.765530
860.457130	80068.288575	33.770548
861.155467	80212.114649	33.775565
862.353224	80375.214292	33.780583
863.385427	80524.901321	33.785600
864.389282	80668.350979	33.790618
865.023863	80822.906553	33.795636
866.283910	80963.311272	33.800653
866.974025	81118.517558	33.805671
868.362813	81266.778063	33.810688
868.973202	81387.500385	33.815706
869.853465	81568.581273	33.820724
870.486224	81708.626154	33.825741
871.408390	81874.793212	33.830759
871.834784	82019.011061	33.835776
872.701575	82163.157114	33.840794
873.230895	82338.786137	33.845812
874.283871	82468.335193	33.850829
875.031100	82650.376642	33.855847
875.961882	82804.175788	33.860864
876.873392	82966.348366	33.865882
877.719223	83115.691226	33.870900
878.924611	83287.148388	33.875917
879.806625	83440.188135	33.880935
880.636142	83611.070877	33.885952
881.415133	83754.336938	33.890970
882.213660	83926.188742	33.895988
883.371572	84074.910700	33.901005
884.418467	84239.107068	33.906023
885.020493	84399.373509	33.911040
886.496436	84550.956174	33.916058
887.331154	84725.718162	33.921076
888.365796	84855.309178	33.926093
889.273115	85002.313481	33.931111
889.618232	85149.392578	33.936128
891.015736	85279.318326	33.941146
891.598810	85421.861689	33.946164
892.742815	85561.390404	33.951181
893.558276	85699.829087	33.956199
894.297433	85858.754494	33.961216
895.161538	85982.489855	33.966234
895.802926	86132.639096	33.971252
896.692798	86276.895953	33.976269
897.648228	86428.665556	33.981287
898.323213	86584.911313	33.986304
899.415207	86731.111638	33.991322
900.108717	86904.825270	33.996340
901.009151	87056.924431	34.001357
901.995758	87210.870529	34.006375
902.753115	87371.302863	34.011392
903.680690	87514.042696	34.016410
904.055968	87697.716856	34.021428
905.335472	87865.570488	34.026445
905.977175	88021.806112	34.031463
906.992251	88195.748379	34.036480
907.892709	88363.585931	34.041498
908.850326	88532.433973	34.046516
910.116256	88713.463400	34.051533
911.083536	88860.798698	34.056551
911.862673	89040.405075	34.061568
912.743710	89192.508726	34.066586
913.822645	89385.109508	34.071604
914.906840	89527.753532	34.076621
916.065814	89706.998563	34.081639
916.802240	89864.952001	34.086656
917.607132	90038.689541	34.091674
918.218571	90204.474479	34.096692
919.471359	90368.667616	34.101709
920.395001	90542.218402	34.106727
920.995175	90718.918284	34.111744
922.346618	90869.619875	34.116762
922.716273	91051.802459	34.121780
924.123158	91207.021660	34.126797
925.040373	91384.262674	34.131815
925.763067	91561.733305	34.136832
926.920039	91745.265697	34.141850
927.940097	91908.678917	34.146868
928.880914	92097.173177	34.151885
930.079448	92244.466079	34.156903
930.352890	92430.573423	34.161920
931.621980	92591.387155	34.166938
932.610927	92767.278624	34.171956
933.289144	92949.829787	34.176973
934.306078	93104.657407	34.181991
934.885145	93306.941504	34.187008
936.101757	93469.725370	34.192026
937.276659	93657.003440	34.197044
937.849771	93824.718521	34.202061
938.950545	93995.663997	34.207079
939.635104	94184.527076	34.212096
940.962773	94361.728672	34.217114
941.972267	94533.281621	34.222132
942.959813	94711.003953	34.227149
944.182159	94877.068508	34.232167
944.838545	95053.341689	34.237184
945.619215	95217.766288	34.242202
946.716204	95398.064235	34.247220
947.526533	95563.505288	34.252237
948.499680	95745.946581	34.257255
949.162323	95909.724424	34.262272
950.097911	96102.751036	34.267290
951.100502	96257.923981	34.272308
951.860066	96450.533005	34.277325
952.638270	96594.782350	34.282343
953.458393	96786.966264	34.287360
954.651280	96960.518836	34.292378
955.961115	97118.045447	34.297396
957.004232	97291.973222	34.302413
957.974663	97464.034272	34.307431
958.635246	97648.883357	34.312448
959.736198	97801.840691	34.317466
960.505994	97994.814585	34.322484
961.227904	98162.129759	34.327501
961.894481	98350.110110	34.332519
962.773574	98557.502836	34.337536
963.861947	98743.118700	34.342554
964.837823	98922.076177	34.347572
966.044133	99116.164134	34.352589
966.524352	99303.581091	34.357607
967.459685	99509.117687	34.362624
968.358789	99682.718847	34.367642
969.385848	99888.572600	34.372660
970.382782	100074.492007	34.377677
971.815533	100284.542444	34.382695
972.884604	100466.711506	34.387712
973.885196	100661.959603	34.392730
974.969347	100856.986507	34.397748
975.966338	101040.393445	34.402765
977.544012	101221.711653	34.407783
978.527357	101413.632109	34.412800
979.393575	101598.837324	34.417818
980.194712	101776.008058	34.422836
981.099874	101972.067076	34.427853
982.236707	102151.426167	34.432871
983.302905	102350.576373	34.437888
984.378098	102522.958789	34.442906
985.408843	102720.117116	34.447924
987.019444	102901.897750	34.452941
988.077111	103089.247484	34.457959
988.774863	103259.303990	34.462976
989.994548	103457.570117	34.467994
991.088584	103627.861218	34.473012
991.656327	103818.095638	34.478029
992.710332	103984.501898	34.483047
993.690893	104174.385885	34.488064
994.769983	104356.137967	34.493082
995.808459	104526.057970	34.498100
996.406357	104715.705209	34.503117
997.927950	104900.363938	34.508135
998.524219	105106.286727	34.513152
999.639538	105274.343771	34.518170
1000.252850	105467.609417	34.523188
1001.009271	105659.301568	34.528205
1002.004245	105857.509275	34.533223
1002.930255	106055.077687	34.538240
1004.295015	106256.513669	34.543258
1005.172331	106441.346721	34.548276
1006.104146	106651.405502	34.553293
1007.290472	106840.527852	34.558311
1008.284809	107041.372500	34.563328
1008.571992	107234.787401	34.568346
1010.155441	107431.143195	34.573364
1010.765215	107640.832476	34.578381
1011.955990	107832.418190	34.583399
1013.032569	108056.040953	34.588416
1014.005093	108268.182983	34.593434
1014.907573	108463.506387	34.598452
1015.817440	108670.266664	34.603469
1016.980020	108850.655739	34.608487
1017.929618	109065.974262	34.613504
1018.853641	109244.657580	34.618522
1020.173080	109437.348229	34.623540
1021.087491	109626.446775	34.628557
1022.935054	109790.035840	34.633575
1024.512388	109967.336912	34.638592
1025.637841	110130.768637	34.643610
1026.550810	110307.827008	34.648628
1027.524298	110488.410383	34.653645
1028.714447	110665.349358	34.658663
1029.563414	110824.385154	34.663680
1030.293779	111024.277565	34.668698
1031.111564	111195.037023	34.673716
1032.085087	111397.273337	34.678733
1032.923810	111566.727045	34.683751
1033.807968	111761.279580	34.688768
1034.799326	111942.376420	34.693786
1035.751297	112163.026774	34.698804
1036.082003	112362.881066	34.703821
1036.928804	112559.117528	34.708839
1038.050933	112774.019265	34.713856
1038.747824	112981.544583	34.718874
1039.741944	113213.863001	34.723892
1040.886383	113420.747742	34.728909
1041.868089	113645.344757	34.733927
1043.378166	113872.313901	34.738944
1044.458926	114092.857259	34.743962
1045.529718	114298.595354	34.748980
1046.507194	114527.646687	34.753997
1047.980051	114729.255220	34.759015
1049.085825	114955.273937	34.764032
1049.914809	115168.519963	34.769050
1051.175442	115379.821459	34.774068
1052.320120	115608.144716	34.779085
1053.209312	115831.761335	34.784103
1054.547678	116034.757106	34.789120
1055.400266	116256.976969	34.794138
1056.314011	116466.608379	34.799156
1057.270746	116699.925116	34.804173
1058.399575	116912.463547	34.809191
1059.647480	117147.978363	34.814208
1060.233234	117364.410609	34.819226
1061.561760	117597.179332	34.824244
1062.141179	117819.291975	34.829261
1062.856061	118059.602769	34.834279
1063.956941	118300.840113	34.839296
1065.106972	118528.514784	34.844314
1066.459690	118766.901842	34.849332
1067.566639	119011.020282	34.854349
1069.177208	119217.883757	34.859367
1070.338939	119446.830860	34.864384
1071.273566	119681.620264	34.869402
1072.392860	119904.686380	34.874420
1073.688143	120138.571083	34.879437
1074.880532	120379.215413	34.884455
1075.815448	120608.640052	34.889472
1077.081498	120810.478317	34.894490
1078.025602	121052.563052	34.899508
1078.544841	121278.754557	34.904525
1080.126810	121504.823072	34.909543
1081.202596	121726.275923	34.914560
1082.148296	121971.763951	34.919578
1083.362198	122187.064632	34.924596
1083.934508	122428.766071	34.929613
1085.358171	122649.243507	34.934631
1086.576460	122888.029026	34.939648
1087.585621	123114.293314	34.944666
1089.122483	123341.853466	34.949684
1089.784528	123555.722044	34.954701
1090.864191	123773.261484	34.959719
1092.122194	123984.284964	34.964736
1092.591760	124221.392816	34.969754
1093.644358	124429.095247	34.974772
1094.721152	124653.434010	34.979789
1095.845949	124874.066177	34.984807
1096.931694	125114.881211	34.989824
1097.880330	125333.860419	34.994842
1099.616537	125562.329872	34.999860
1100.326365	125784.291901	35.004877
1101.536926	126021.101694	35.009895
1102.678701	126246.506265	35.014912
1103.340284	126481.724806	35.019930
1104.758238	126721.737560	35.024948
1105.660682	126963.598931	35.029965
1106.650544	127199.415231	35.034983
1107.515715	127436.457948	35.040000
1108.472372	127696.363429	35.045018
1109.523751	127925.115984	35.050036
1110.326017	128195.861975	35.055053
1111.677947	128435.379595	35.060071
1113.068403	128701.774520	35.065088
1114.201414	128963.638875	35.070106
1115.117244	129202.410680	35.075124
1116.329402	129469.500788	35.080141
1117.263278	129710.326823	35.085159
1118.311755	129991.175002	35.090176
1119.460630	130239.904013	35.095194
1120.941661	130507.871319	35.100212
1122.288548	130775.330741	35.105229
1123.389784	131029.752347	35.110247
1124.740220	131288.900763	35.115264
1125.535800	131557.801495	35.120282
1127.263764	131806.168599	35.125300
1128.467591	132049.604710	35.130317
1129.725495	132321.566533	35.135335
1130.868815	132566.575742	35.140352
1131.639763	132799.010570	35.145370
1133.074114	133071.761001	35.150388
1134.382506	133326.205084	35.155405
1135.438984	133584.216754	35.160423
1136.573078	133831.316177	35.165440
1137.931184	134083.210212	35.170458
1139.105841	134336.708398	35.175476
1139.958109	134591.935115	35.180493
1141.253603	134839.129797	35.185511
1142.482838	135085.995055	35.190528
1143.371621	135348.460165	35.195546
1144.630866	135602.461476	35.200564
1145.452224	135870.139498	35.205581
1146.350758	136118.664567	35.210599
1147.671432	136381.421744	35.215616
1148.848683	136652.470330	35.220634
1150.094707	136900.411581	35.225652
1151.152393	137181.182528	35.230669
1152.373354	137437.106156	35.235687
1153.566320	137696.687590	35.240704
1154.585835	137965.896821	35.245722
1156.058784	138213.759859	35.250740
1157.014882	138491.820372	35.255757
1157.887581	138757.852774	35.260775
1159.348323	139025.869476	35.265792
1160.312355	139285.843531	35.270810
1161.362670	139553.501183	35.275828
1162.589655	139820.827540	35.280845
1163.698015	140099.954072	35.285863
1164.927054	140341.559317	35.290880
1166.227567	140612.734203	35.295898
1167.598607	140836.797439	35.300916
1168.572471	141119.618867	35.305933
1169.622386	141350.648598	35.310951
1170.704624	141612.840047	35.315968
1171.423393	141869.375159	35.320986
1172.855981	142133.858476	35.326004
1173.874606	142388.902562	35.331021
1174.916314	142662.697865	35.336039
1176.183027	142918.186780	35.341056
1177.100732	143196.913869	35.346074
1178.256838	143458.879089	35.351092
1179.471032	143735.215825	35.356109
1180.613873	144017.792481	35.361127
1181.989734	144278.282123	35.366144
1183.439146	144569.067482	35.371162
1184.650274	144838.477416	35.376180
1185.610986	145116.769077	35.381197
1187.027386	145397.891596	35.386215
1188.302705	145651.509871	35.391232
1189.018662	145941.844436	35.396250
1190.672933	146224.100950	35.401268
1191.830311	146501.978038	35.406285
1192.617290	146785.105023	35.411303
1194.277013	147054.990532	35.416320
1195.404104	147341.705326	35.421338
1197.231003	147633.848687	35.426356
1198.478126	147905.837788	35.431373
1199.957854	148165.565507	35.436391
1202.207593	148405.016821	35.441408
1203.621183	148659.090327	35.446426
1205.283089	148900.962743	35.451444
1206.327365	149158.385333	35.456461
1207.360365	149405.361626	35.461479
1208.713910	149651.715997	35.466496
1209.509158	149904.238969	35.471514
1210.478340	150159.689957	35.476532
1211.640709	150425.840138	35.481549
1212.792428	150686.540552	35.486567
1213.739690	150935.646661	35.491584
1214.813912	151211.722179	35.496602
1215.768922	151473.525991	35.501620
1216.779097	151744.352731	35.506637
1217.855173	152015.969600	35.511655
1219.023078	152295.030919	35.516672
1220.374132	152590.146298	35.521690
1221.682382	152854.565005	35.526708
1223.080239	153140.646564	35.531725
1224.015707	153424.840703	35.536743
1225.182690	153701.122321	35.541760
1226.090788	153987.456053	35.546778
1227.572870	154275.219256	35.551796
1228.574185	154567.718953	35.556813
1229.453812	154854.419083	35.561831
1230.965990	155162.896836	35.566848
1231.795882	155460.644803	35.571866
1233.146149	155742.606171	35.576884
1234.229737	156049.627024	35.581901
1235.444378	156346.684137	35.586919
1237.062027	156644.691772	35.591936
1238.005153	156947.316061	35.596954
1239.195647	157233.703551	35.601972
1240.809438	157543.807213	35.606989
1241.781451	157829.372573	35.612007
1243.290459	158141.413682	35.617024
1244.466104	158441.613706	35.622042
1245.450761	158748.545304	35.627060
1246.957902	159039.219343	35.632077
1247.784054	159337.010229	35.637095
1249.518273	159622.640349	35.642112
1250.404453	159918.827312	35.647130
1251.133283	160204.500686	35.652148
1252.478171	160509.762639	35.657165
1253.886030	160781.728952	35.662183
1255.408299	161108.100717	35.667200
1256.644000	161387.355862	35.672218
1257.742329	161693.301755	35.677236
1259.269102	161990.260842	35.682253
1260.413207	162294.681351	35.687271
1261.944453	162587.559058	35.692288
1262.763099	162894.942919	35.697306
1263.593842	163192.279324	35.702324
1265.161650	163507.257515	35.707341
1266.085186	163806.536759	35.712359
1267.626167	164125.571139	35.717376
1268.539452	164453.744661	35.722394
1270.128775	164773.968584	35.727412
1271.514172	165084.738635	35.732429
1272.484680	165411.895227	35.737447
1275.053363	165684.767974	35.742464
1275.914384	166011.147967	35.747482
1277.523900	166305.802365	35.752500
1279.118399	166622.233169	35.757517
1280.149995	166924.244518	35.762535
1281.414595	167253.130288	35.767552
1282.489307	167556.927936	35.772570
1283.395383	167869.713244	35.777588
1284.394730	168169.860809	35.782605
1285.368356	168520.120133	35.787623
1286.929263	168829.619529	35.792640
1288.074638	169190.488607	35.797658
1289.228024	169503.561994	35.802676
1290.958489	169848.365160	35.807693
1291.924802	170177.360226	35.812711
1293.665217	170508.184018	35.817728
1295.252844	170838.565993	35.822746
1296.824829	171163.509449	35.827764
1298.115852	171481.167390	35.832781
1299.024989	171814.916904	35.837799
1300.762918	172114.969228	35.842816
1301.903141	172445.982449	35.847834
1303.089428	172771.660940	35.852852
1304.795853	173096.862527	35.857869
1305.952954	173448.119860	35.862887
1307.300092	173764.578925	35.867904
1308.542611	174107.464709	35.872922
1309.985482	174434.445006	35.877940
1311.381322	174736.880421	35.882957
1312.436553	175077.075914	35.887975
1314.076523	175406.911093	35.892992
1315.357162	175726.008564	35.898010
1316.742702	176046.423345	35.903028
1318.285685	176382.651824	35.908045
1319.630079	176711.973792	35.913063
1320.780008	177036.647323	35.918080
1322.399995	177342.704521	35.923098
1323.869291	177670.210371	35.928116
1325.182318	177971.677428	35.933133
1326.374230	178306.911254	35.938151
1327.962358	178621.636920	35.943168
1329.097285	178956.973439	35.948186
1330.225394	179270.510086	35.953204
1331.444341	179602.182092	35.958221
1332.445316	179928.993467	35.963239
1333.913052	180254.689260	35.968256
1335.008061	180576.527043	35.973274
1336.079675	180888.496768	35.978292
1337.531720	181192.054582	35.983309
1338.854134	181535.601615	35.988327
1340.054169	181828.455002	35.993344
1341.425547	182153.912418	35.998362
1342.491988	182469.941390	36.003380
1343.666603	182812.252206	36.008397
1345.242043	183145.259321	36.013415
1346.398287	183478.388530	36.018432
1347.456806	183819.544784	36.023450
1348.863287	184141.201236	36.028468
1350.344606	184486.696277	36.033485
1351.538903	184828.509368	36.038503
1353.056081	185167.060160	36.043520
1354.389928	185501.315180	36.048538
1355.847412	185857.332557	36.053556
1357.405086	186189.498710	36.058573
1358.477397	186537.828867	36.063591
1359.924454	186871.972168	36.068608
1361.311659	187244.815732	36.073626
1362.473412	187580.825560	36.078644
1364.055582	187936.480572	36.083661
1364.903415	188284.097298	36.088679
1366.116185	188658.654723	36.093696
1367.463740	189012.654439	36.098714
1368.457370	189406.128171	36.103732
1369.960682	189762.480590	36.108749
1371.199722	190150.486140	36.113767
1372.545411	190528.575587	36.118784
1373.623652	190922.578991	36.123802
1374.967583	191292.397361	36.128820
1376.563250	191697.529406	36.133837
1377.866125	192078.873046	36.138855
1379.425282	192471.804755	36.143872
1381.045385	192856.515830	36.148890
1382.425538	193256.946542	36.153908
1384.202014	193645.407147	36.158925
1385.688081	194028.840388	36.163943
1387.300463	194409.767081	36.168960
1388.759421	194804.660257	36.173978
1390.321649	195175.444277	36.178996
1392.270626	195561.019682	36.184013
1392.959553	195934.872223	36.189031
1394.568076	196298.178048	36.194048
1396.093076	196688.045175	36.199066
1397.628682	197064.760796	36.204084
1399.306102	197443.042167	36.209101
1400.465742	197820.839956	36.214119
1402.167424	198178.694957	36.219136
1403.861313	198563.505675	36.224154
1405.198270	198938.970209	36.229172
1406.798955	199297.063901	36.234189
1407.957702	199676.599296	36.239207
1409.519760	200047.818090	36.244224
1410.667677	200402.348849	36.249242
1411.937292	200802.236482	36.254260
1413.247813	201160.388151	36.259277
1414.402412	201548.872857	36.264295
1416.055202	201923.375348	36.269312
1417.281117	202289.723230	36.274330
1418.232669	202687.414557	36.279348
1420.260322	203054.624504	36.284365
1421.953479	203450.217196	36.289383
1423.041983	203823.769315	36.294400
1424.957647	204194.863446	36.299418
1426.135864	204581.901154	36.304436
1427.375850	204969.616385	36.309453
1428.704079	205332.052689	36.314471
1429.886777	205715.007419	36.319488
1431.475455	206067.031146	36.324506
1433.109669	206446.029962	36.329524
1434.510299	206798.659586	36.334541
1435.635712	207151.234727	36.339559
1436.780378	207541.645668	36.344576
1438.255797	207905.593973	36.349594
1439.445448	208262.747389	36.354612
1441.025954	208662.348441	36.359629
1442.089687	209058.240348	36.364647
1443.326538	209439.237047	36.369664
1445.016181	209832.515518	36.374682
1445.928266	210220.362756	36.379700
1447.667111	210614.665505	36.384717
1449.505286	211002.871634	36.389735
1450.635825	211404.021108	36.394752
1452.489712	211798.564630	36.399770
1453.660566	212202.936623	36.404788
1455.297514	212617.214235	36.409805
1456.481024	213008.242579	36.414823
1458.087496	213425.716425	36.419840
1459.919870	213817.657295	36.424858
1461.072434	214235.971919	36.429876
1462.665995	214634.482791	36.434893
1464.153159	215064.123805	36.439911
1465.563303	215526.871495	36.444928
1467.241020	215944.193379	36.449946
1468.292953	216355.068083	36.454964
1469.769399	216766.357153	36.459981
1471.350081	217193.631083	36.464999
1472.750655	217605.241222	36.470016
1474.581808	218025.417244	36.475034
1475.355222	218466.646439	36.480052
1477.314450	218865.420405	36.485069
1478.838259	219311.228255	36.490087
1480.050500	219722.269167	36.495104
1481.410696	220157.974191	36.500122
1482.914491	220598.102110	36.505140
1484.570287	221026.447551	36.510157
1486.348328	221449.872785	36.515175
1487.809027	221887.905422	36.520192
1489.470161	222301.498920	36.525210
1491.119616	222737.726131	36.530228
1492.828199	223173.437429	36.535245
1494.807648	223588.735996	36.540263
1496.308650	224026.288355	36.545280
1498.263851	224436.946202	36.550298
1499.279924	224858.605970	36.555316
1500.888283	225273.972207	36.560333
1502.643167	225674.939821	36.565351
1504.082582	226097.626566	36.570368
1505.902210	226507.831797	36.575386
1507.226865	226932.064507	36.580404
1508.404777	227334.580882	36.585421
1509.934121	227750.832676	36.590439
1511.616596	228160.990090	36.595456
1513.450119	228589.945283	36.600474
1514.018683	229001.356121	36.605492
1516.085925	229430.809057	36.610509
1517.035268	229843.302823	36.615527
1518.510887	230278.647481	36.620544
1520.431457	230689.154871	36.625562
1521.657126	231124.086387	36.630580
1522.854806	231563.926231	36.635597
1523.939978	231988.571136	36.640615
1525.428659	232423.920640	36.645632
1527.608195	232857.252451	36.650650
1529.306070	233289.039421	36.655668
1531.012328	233689.227631	36.660685
1532.643530	234113.560213	36.665703
1533.696820	234520.691291	36.670720
1535.205633	234927.799109	36.675738
1536.419699	235342.627797	36.680756
1537.949138	235759.513858	36.685773
1539.405696	236188.631066	36.690791
1541.163045	236606.345390	36.695808
1542.496733	237026.924853	36.700826
1543.538567	237462.870635	36.705844
1544.991735	237884.524810	36.710861
1546.535470	238335.173710	36.715879
1547.837652	238774.940915	36.720896
1549.506799	239211.676652	36.725914
1551.154078	239659.949464	36.730932
1552.484901	240127.022150	36.735949
1554.178559	240566.551246	36.740967
1555.764744	241034.600093	36.745984
1557.347244	241469.145377	36.751002
1558.757480	241940.248226	36.756020
1560.162288	242377.746009	36.761037
1562.196759	242848.443080	36.766055
1563.680146	243322.000956	36.771072
1564.982567	243780.856366	36.776090
1566.861281	244242.665893	36.781108
1568.286109	244735.186532	36.786125
1569.748009	245194.120013	36.791143
1571.265202	245683.883866	36.796160
1573.395761	246132.547733	36.801178
1574.651289	246619.562259	36.806196
1576.549689	247079.443175	36.811213
1578.042498	247553.972916	36.816231
1579.694370	248034.370624	36.821248
1581.722315	248510.032946	36.826266
1583.373624	248977.146598	36.831284
1585.025856	249444.311585	36.836301
1586.954994	249899.924038	36.841319
1589.601577	250357.298529	36.846336
1591.407543	250800.485052	36.851354
1592.873306	251251.857184	36.856372
1594.499664	251700.840864	36.861389
1596.104166	252146.119804	36.866407
1597.197830	252608.579752	36.871424
1598.723795	253049.274622	36.876442
1599.927049	253514.943592	36.881460
1601.650167	253987.563886	36.886477
1603.213838	254457.365762	36.891495
1604.659352	254918.652064	36.896512
1606.456704	255389.762507	36.901530
1608.111115	255856.171886	36.906548
1609.332109	256326.768414	36.911565
1610.826739	256803.696297	36.916583
1612.386347	257280.766154	36.921600
1613.886545	257753.171863	36.926618
1615.664899	258237.496835	36.931636
1616.857549	258703.298045	36.936653
1618.648558	259199.484635	36.941671
1620.233478	259679.447273	36.946688
1621.945246	260163.352015	36.951706
1623.322433	260650.639885	36.956724
1624.757682	261153.261836	36.961741
1626.331726	261630.559229	36.966759
1627.470136	262135.389483	36.971776
1629.276975	262630.176731	36.976794
1630.963191	263142.004043	36.981812
1632.762549	263640.806109	36.986829
1634.669572	264128.006395	36.991847
1636.013169	264626.451548	36.996864
1637.774394	265095.512241	37.001882
1639.258407	265586.897155	37.006900
1640.987724	266062.618369	37.011917
1642.615851	266528.906036	37.016935
1643.900281	267021.593299	37.021952
1645.848331	267501.799395	37.026970
1647.755294	267983.942588	37.031988
1649.110170	268471.638197	37.037005
1651.221040	268950.774838	37.042023
1652.429071	269429.348748	37.047040
1653.995392	269935.095238	37.052058
1655.551696	270409.800310	37.057076
1656.987467	270910.080259	37.062093
1658.803964	271404.047688	37.067111
1659.978750	271920.221016	37.072128
1661.421157	272426.391569	37.077146
1663.230882	272934.329859	37.082164
1664.310383	273460.779609	37.087181
1666.295646	273976.740167	37.092199
1667.854045	274511.365208	37.097216
1669.525135	275046.707444	37.102234
1671.200635	275574.020763	37.107252
1672.801065	276123.801484	37.112269
1674.898424	276655.869739	37.117287
1676.164622	277200.267325	37.122304
1677.602114	277723.475235	37.127322
1679.407142	278285.131566	37.132340
1681.067334	278826.183767	37.137357
1683.433667	279386.373217	37.142375
1685.069439	279924.226230	37.147392
1686.936011	280476.087304	37.152410
1688.521415	281029.847729	37.157428
1690.141272	281572.805136	37.162445
1692.143593	282124.588718	37.167463
1694.212450	282660.534391	37.172480
1696.058848	283205.913992	37.177498
1698.042185	283735.139291	37.182516
1699.934035	284287.823976	37.187533
1702.129836	284802.887782	37.192551
1703.658852	285340.261081	37.197568
1705.613795	285864.785488	37.202586
1706.930405	286396.475181	37.207604
1708.850812	286947.800390	37.212621
1710.634150	287467.648789	37.217639
1712.178007	288021.064537	37.222656
1713.820841	288524.548870	37.227674
1716.304280	289075.799129	37.232692
1717.549964	289582.266573	37.237709
1719.642511	290120.546772	37.242727
1721.238209	290663.225050	37.247744
1722.720948	291187.555237	37.252762
1724.511209	291723.491545	37.257780
1725.845714	292257.646707	37.262797
1727.824449	292798.678540	37.267815
1728.917787	293347.042478	37.272832
1730.476301	293883.008300	37.277850
1732.581035	294431.302342	37.282868
1734.313797	294994.336476	37.287885
1735.937016	295544.432225	37.292903
1737.141998	296093.095892	37.297920
1738.718545	296659.754790	37.302938
1740.766500	297192.907561	37.307956
1742.366846	297769.589882	37.312973
1744.441304	298309.794070	37.317991
1746.046807	298891.829011	37.323008
1747.529552	299437.535314	37.328026
1749.202472	299996.541846	37.333044
1751.006352	300555.523847	37.338061
1752.839321	301113.685328	37.343079
1754.422094	301646.715311	37.348096
1756.047444	302198.352394	37.353114
1757.934728	302735.136167	37.358132
1759.620822	303278.299728	37.363149
1761.715278	303824.262872	37.368167
1763.278737	304372.418552	37.373184
1765.261039	304906.939723	37.378202
1766.911931	305460.789156	37.383220
1768.328823	306034.458342	37.388237
1770.202765	306578.994323	37.393255
1771.521109	307147.771167	37.398272
1773.482135	307702.368595	37.403290
1775.359482	308281.052327	37.408308
1776.619844	308848.380247	37.413325
1779.037059	309410.281981	37.418343
1780.412315	309997.519436	37.423360
1782.604104	310569.329782	37.428378
1784.550312	311145.443214	37.433396
1786.045432	311706.694464	37.438413
1788.149882	312293.896993	37.443431
1789.778689	312872.437777	37.448448
1791.237255	313456.563961	37.453466
1793.217756	314050.122775	37.458484
1794.973009	314636.933874	37.463501
1796.977988	315234.644310	37.468519
1798.604017	315827.486104	37.473536
1800.268564	316431.769590	37.478554
1801.998116	317015.189143	37.483572
1803.703043	317638.171393	37.488589
1805.367482	318247.442582	37.493607
1807.329543	318846.984737	37.498624
1809.037524	319468.274760	37.503642
1810.817953	320067.988943	37.508660
1812.517548	320698.994901	37.513677
1814.797829	321320.478783	37.518695
1816.659845	321928.035007	37.523712
1818.462393	322554.182413	37.528730
1820.289585	323165.846713	37.533748
1821.895087	323792.192763	37.538765
1823.818821	324421.451114	37.543783
1825.583616	325043.239302	37.548800
1827.256640	325672.526864	37.553818
1829.380310	326314.479844	37.558836
1831.093652	326939.279509	37.563853
1833.305586	327574.146628	37.568871
1834.978193	328189.470066	37.573888
1836.529408	328845.633401	37.578906
1839.125759	329455.739236	37.583924
1840.349001	330114.456443	37.588941
1842.727690	330742.687291	37.593959
1844.203308	331381.418840	37.598976
1846.030658	332013.052941	37.603994
1848.125933	332655.806558	37.609012
1849.769795	333295.555586	37.614029
1851.939308	333927.569206	37.619047
1854.002041	334559.415668	37.624064
1855.983124	335204.824887	37.629082
1857.971847	335824.026740	37.634100
1859.731909	336467.071383	37.639117
1861.867909	337093.825005	37.644135
1863.762669	337728.353703	37.649152
1865.532782	338354.036077	37.654170
1867.878103	338969.081537	37.659188
1869.630807	339598.483665	37.664205
1871.514481	340202.726302	37.669223
1873.426807	340812.110118	37.674240
1875.080715	341451.913498	37.679258
1877.036153	342044.370137	37.684276
1878.987192	342659.589111	37.689293
1881.219193	343237.594021	37.694311
1883.227498	343798.039167	37.699328
1885.194380	344396.532573	37.704346
1887.478499	344969.609999	37.709364
1888.591970	345550.107547	37.714381
1890.532000	346156.096809	37.719399
1892.185071	346752.506466	37.724416
1893.696467	347353.119866	37.729434
1895.674131	347951.009242	37.734452
1897.011687	348555.823838	37.739469
1898.874860	349158.107509	37.744487
1900.759874	349798.245595	37.749504
1902.464822	350416.654852	37.754522
1904.706817	351048.087902	37.759540
1906.031202	351682.252152	37.764557
1907.828347	352316.735597	37.769575
1909.855575	352978.376765	37.774592
1911.259105	353615.216117	37.779610
1913.163099	354266.453878	37.784628
1914.373378	354945.101355	37.789645
1916.283914	355591.826773	37.794663
1918.219762	356265.512590	37.799680
1919.783956	356967.466330	37.804698
1921.890381	357634.302019	37.809716
1923.567862	358344.638822	37.814733
1925.498492	359021.606008	37.819751
1927.600176	359720.862698	37.824768
1929.515726	360440.259150	37.829786
1931.543588	361140.569732	37.834804
1933.249975	361850.080728	37.839821
1934.961366	362576.374603	37.844839
1937.188313	363290.341450	37.849856
1938.855599	364005.402740	37.854874
1941.013924	364731.583894	37.859892
1942.738941	365452.774588	37.864909
1944.724698	366196.437060	37.869927
1946.684020	366911.575060	37.874944
1948.502889	367666.602210	37.879962
1950.735452	368377.634402	37.884980
1952.876289	369141.280608	37.889997
1954.907651	369865.280960	37.895015
1957.083434	370607.076203	37.900032
1958.953807	371337.771460	37.905050
1961.617130	372077.884339	37.910068
1963.560740	372807.270255	37.915085
1965.623454	373536.368374	37.920103
1967.257074	374273.106493	37.925120
1969.276468	375018.465638	37.930138
1971.042590	375748.455832	37.935156
1972.970376	376501.484196	37.940173
1975.012411	377232.539758	37.945191
1976.764723	377977.449857	37.950208
1978.541961	378721.680625	37.955226
1980.619303	379487.681118	37.960244
1982.868204	380227.211599	37.965261
1984.814668	380982.092939	37.970279
1986.534638	381736.842795	37.975296
1988.638287	382503.709756	37.980314
1990.761307	383247.658357	37.985332
1992.628776	384014.910146	37.990349
1994.558074	384757.056738	37.995367
1996.507117	385531.486538	38.000384
1998.463803	386290.430251	38.005402
2000.609654	387065.349158	38.010420
2002.221655	387823.325182	38.015437
2004.268203	388573.960699	38.020455
2006.710385	389333.133309	38.025472
2008.737046	390062.187400	38.030490
2010.904800	390795.637968	38.035508
2012.481343	391519.966597	38.040525
2014.828806	392253.607013	38.045543
2016.932742	392987.118224	38.050560
2018.926590	393723.114445	38.055578
2021.003629	394459.459594	38.060596
2022.809152	395202.371590	38.065613
2024.830703	395929.641263	38.070631
2026.949922	396670.691313	38.075648
2028.720055	397422.552784	38.080666
2030.927941	398180.177981	38.085684
2032.970195	398942.246564	38.090701
2034.937442	399685.198467	38.095719
2037.151802	400441.903072	38.100736
2038.957794	401199.897288	38.105754
2041.252309	401965.824679	38.110772
2043.225849	402718.581863	38.115789
2045.190048	403482.876341	38.120807
2047.551489	404248.022514	38.125824
2049.639280	405019.680184	38.130842
2051.587041	405794.988732	38.135860
2053.313119	406565.548980	38.140877
2055.395772	407351.282338	38.145895
2057.821994	408111.676285	38.150912
2059.983358	408896.567592	38.155930
2062.205185	409680.995913	38.160948
2064.310016	410437.958530	38.165965
2066.119848	411237.357570	38.170983
2068.763409	411988.640153	38.176000
2071.038379	412790.424638	38.181018
2073.311940	413562.344862	38.186036
2075.444263	414358.457044	38.191053
2077.225723	415128.335984	38.196071
2079.384673	415911.022912	38.201088
2081.210719	416696.704923	38.206106
2083.619239	417482.976491	38.211124
2085.427956	418271.754653	38.216141
2087.776354	419054.746735	38.221159
2089.936806	419838.024627	38.226176
2091.846997	420636.919926	38.231194
2094.175962	421405.762949	38.236212
2096.506575	422220.797217	38.241229
2098.155691	423003.074525	38.246247
2100.485831	423796.002187	38.251264
2102.286919	424598.993679	38.256282
2104.546764	425367.043387	38.261300
2106.450197	426188.652757	38.266317
2108.412028	426994.527794	38.271335
2110.761383	427792.160239	38.276352
2112.710097	428586.997240	38.281370
2114.612381	429412.245494	38.286388
2116.869982	430222.977486	38.291405
2118.551064	431034.739176	38.296423
2120.856665	431849.762332	38.301440
2122.663290	432660.840551	38.306458
2124.865452	433481.393542	38.311476
2127.366317	434303.134274	38.316493
2129.227471	435135.075626	38.321511
2131.563165	435974.046187	38.326528
2133.568414	436795.882240	38.331546
2135.874859	437630.900298	38.336564
2137.880536	438459.712396	38.341581
2140.126550	439283.242039	38.346599
2142.128182	440095.749611	38.351616
2144.074567	440947.254936	38.356634
2146.197896	441757.354948	38.361652
2148.647516	442581.439593	38.366669
2150.956807	443366.200005	38.371687
2153.035222	444145.708533	38.376704
2155.203563	444956.848916	38.381722
2157.334735	445750.105384	38.386740
2159.279675	446566.282965	38.391757
2161.418070	447360.340144	38.396775
2163.706914	448169.166495	38.401792
2165.509894	448979.661655	38.406810
2167.928828	449799.585656	38.411828
2170.096940	450623.920610	38.416845
2171.581302	451441.659721	38.421863
2173.822720	452261.619923	38.426880
2175.723821	453098.649525	38.431898
2177.945537	453931.445845	38.436916
2179.904306	454763.797401	38.441933
2181.624252	455625.082690	38.446951
2184.105404	456470.428961	38.451968
2186.285433	457338.495603	38.456986
2188.364072	458197.794579	38.462004
2190.916360	459077.407403	38.467021
2193.138841	459931.048084	38.472039
2195.517555	460786.548538	38.477056
2197.492556	461669.835597	38.482074
2199.805069	462534.676832	38.487092
2201.976240	463412.395254	38.492109
2204.304838	464299.148420	38.497127
2206.566600	465188.703904	38.502144
2208.716555	466070.302195	38.507162
2210.753034	466974.675258	38.512180
2213.593721	467848.953429	38.517197
2215.419616	468758.636482	38.522215
2217.817226	469641.701391	38.527232
2220.027754	470555.835898	38.532250
2222.026378	471446.969883	38.537268
2224.245641	472353.892674	38.542285
2226.432945	473260.474650	38.547303
2228.685759	474165.840667	38.552320
2231.000813	475073.578366	38.557338
2232.889546	475995.033822	38.562356
2235.329968	476907.462069	38.567373
2237.122669	477830.459924	38.572391
2239.367976	478763.440094	38.577408
2241.539143	479695.627995	38.582426
2243.890425	480607.637113	38.587444
2246.225889	481550.310919	38.592461
2248.471561	482503.051612	38.597479
2250.869545	483433.850967	38.602496
2252.868508	484379.211730	38.607514
2255.634386	485317.680859	38.612532
2257.943342	486247.744263	38.617549
2260.150861	487202.112155	38.622567
2262.588590	488155.280406	38.627584
2264.736323	489117.885932	38.632602
2266.761218	490050.927805	38.637620
2269.369439	491006.287166	38.642637
2271.367459	491962.300884	38.647655
2273.749736	492900.533372	38.652672
2275.965915	493863.018985	38.657690
2278.184212	494824.542412	38.662708
2280.383286	495769.160219	38.667725
2282.516272	496739.977286	38.672743
2284.667769	497685.153464	38.677760
2286.917487	498659.979848	38.682778
2289.281101	499630.039317	38.687796
2291.586022	500604.744704	38.692813
2293.677075	501572.366264	38.697831
2295.855945	502541.329953	38.702848
2298.212200	503482.616504	38.707866
2300.333625	504415.969570	38.712884
2302.676048	505359.421702	38.717901
2304.653059	506304.241824	38.722919
2306.673952	507260.599354	38.727936
2308.840995	508220.356387	38.732954
2310.870986	509171.860333	38.737972
2313.397268	510157.866156	38.742989
2315.242957	511128.596912	38.748007
2317.427195	512114.237063	38.753024
2319.556438	513088.785456	38.758042
2321.902130	514071.959460	38.763060
2324.193990	515087.744552	38.768077
2326.562285	516084.702151	38.773095
2328.662374	517108.050243	38.778112
2331.069997	518112.382452	38.783130
2333.085865	519138.232527	38.788148
2335.747494	520157.660306	38.793165
2338.026218	521189.076152	38.798183
2339.912116	522230.010275	38.803200
2342.362133	523263.828647	38.808218
2344.706524	524339.154799	38.813236
2347.130276	525368.099938	38.818253
2349.431709	526424.194820	38.823271
2351.725805	527499.406430	38.828288
2354.176504	528562.831605	38.833306
2356.395411	529625.565004	38.838324
2358.928974	530698.392957	38.843341
2360.966090	531775.354223	38.848359
2363.760911	532851.407475	38.853376
2366.630212	533929.937532	38.858394
2368.620518	535009.741545	38.863412
2371.301886	536103.244768	38.868429
2373.523405	537188.587960	38.873447
2375.734100	538282.307021	38.878464
2378.219906	539375.696712	38.883482
2380.273823	540456.393726	38.888500
2383.172954	541554.430649	38.893517
2385.543509	542657.753193	38.898535
2387.786455	543774.997185	38.903552
2390.612342	544866.451562	38.908570
2392.727819	545997.475520	38.913588
2395.454679	547072.427281	38.918605
2397.322740	548212.316649	38.923623
2399.794195	549304.691070	38.928640
2402.153638	550438.332577	38.933658
2404.376063	551551.891801	38.938676
2407.378728	552666.036773	38.943693
2409.540022	553804.059349	38.948711
2411.941628	554916.059039	38.953728
2414.705037	556050.929428	38.958746
2417.275734	557160.254440	38.963764
2419.727925	558287.650354	38.968781
2421.871837	559409.474797	38.973799
2424.500846	560537.707749	38.978816
2426.913712	561658.545298	38.983834
2429.358004	562782.196971	38.988852
2432.401512	563906.006069	38.993869
2435.127983	565023.743880	38.998887
2437.544340	566145.455765	39.003904
2439.934413	567251.858405	39.008922
2442.313795	568380.365196	39.013940
2444.792098	569480.185968	39.018957
2447.106184	570624.877597	39.023975
2449.128014	571739.141722	39.028992
2451.843401	572866.497861	39.034010
2454.023771	573986.012151	39.039028
2456.668198	575109.969120	39.044045
2458.814044	576212.629283	39.049063
2461.091504	577310.103051	39.054080
2463.478487	578408.667369	39.059098
2465.640758	579498.141165	39.064116
2468.564554	580595.020242	39.069133
2470.781404	581710.129213	39.074151
2473.452590	582805.299709	39.079168
2475.972570	583911.181696	39.084186
2478.013702	585021.958189	39.089204
2480.474118	586122.686008	39.094221
2482.848525	587235.413301	39.099239
2485.216400	588361.677589	39.104256
2487.921302	589494.700212	39.109274
2490.541977	590626.828494	39.114292
2493.281338	591753.016444	39.119309
2496.119406	592857.380797	39.124327
2498.621829	593994.824297	39.129344
2501.358373	595108.067920	39.134362
2503.535475	596275.312676	39.139380
2506.198286	597407.141860	39.144397
2508.583366	598554.888564	39.149415
2510.746686	599703.060585	39.154432
2513.326370	600865.676284	39.159450
2515.596099	602022.217514	39.164468
2518.150505	603187.660348	39.169485
2520.470872	604362.888283	39.174503
2522.977005	605544.774718	39.179520
2525.800518	606700.305870	39.184538
2527.983491	607887.911237	39.189556
2530.420188	609076.752552	39.194573
2533.082309	610253.021338	39.199591
2535.488385	611460.234482	39.204608
2538.164033	612656.366664	39.209626
2540.517994	613880.490570	39.214644
2543.094376	615073.279715	39.219661
2545.634886	616290.856072	39.224679
2548.153058	617515.304472	39.229696
2551.049445	618718.852463	39.234714
2553.527300	619944.938704	39.239732
2556.159024	621146.365070	39.244749
2559.077705	622379.955950	39.249767
2561.389108	623592.264185	39.254784
2564.120683	624830.007161	39.259802
2566.510347	626046.576515	39.264820
2569.531811	627275.546429	39.269837
2572.356086	628499.212442	39.274855
2574.812926	629714.906300	39.279872
2577.527485	630946.503325	39.284890
2579.781728	632185.874998	39.289908
2582.513821	633415.884320	39.294925
2585.146476	634641.872103	39.299943
2587.714867	635878.611822	39.304960
2590.253904	637109.669367	39.309978
2592.652967	638354.830857	39.314996
2595.279210	639586.031147	39.320013
2598.175420	640830.365082	39.325031
2600.321370	642071.729054	39.330048
2603.097503	643321.670404	39.335066
2605.620919	644584.221978	39.340084
2608.281965	645811.131175	39.345101
2611.479359	647061.942875	39.350119
2613.921974	648288.988404	39.355136
2616.954924	649535.482968	39.360154
2619.085272	650778.681932	39.365172
2622.054554	652027.171968	39.370189
2625.104785	653266.770727	39.375207
2627.354685	654505.948840	39.380224
2630.361027	655722.275067	39.385242
2633.021506	656944.587633	39.390260
2635.215540	658137.981514	39.395277
2637.928113	659311.370123	39.400295
2640.310105	660530.295072	39.405312
2643.195474	661736.336207	39.410330
2645.602227	662927.966646	39.415348
2648.046157	664128.854725	39.420365
2650.590254	665341.823637	39.425383
2652.734620	666549.877987	39.430400
2655.836285	667772.105620	39.435418
2657.873218	668996.343557	39.440436
2660.494053	670230.080696	39.445453
2663.163853	671466.585309	39.450471
2665.487566	672723.877965	39.455488
2668.132356	673971.699892	39.460506
2670.902880	675234.901425	39.465524
2673.101149	676506.878274	39.470541
2675.632950	677765.452877	39.475559
2678.240234	679066.247391	39.480576
2680.994725	680358.983004	39.485594
2683.408267	681651.694116	39.490612
2686.009352	682943.994882	39.495629
2689.009711	684256.666337	39.500647
2691.534234	685559.740873	39.505664
2694.349174	686878.972145	39.510682
2696.784710	688211.632258	39.515700
2699.495082	689540.923634	39.520717
2702.402212	690881.356250	39.525735
2704.849000	692215.411376	39.530752
2707.555309	693556.670475	39.535770
2710.050899	694911.856533	39.540788
2712.558152	696286.929268	39.545805
2715.642133	697638.775944	39.550823
2718.447875	699009.360064	39.555840
2721.340493	700365.385263	39.560858
2724.092659	701738.678681	39.565876
2726.914963	703102.821941	39.570893
2729.681769	704472.313414	39.575911
2732.718443	705838.125607	39.580928
2735.283218	707215.743272	39.585946
2738.037916	708601.136864	39.590964
2740.443658	709996.817973	39.595981
2743.619507	711381.942621	39.600999
2746.191947	712766.348580	39.606016
2748.986817	714160.247614	39.611034
2751.981128	715559.875623	39.616052
2754.752985	716956.735481	39.621069
2757.849150	718329.160476	39.626087
2760.415658	719724.358761	39.631104
2763.365057	721134.400652	39.636122
2766.162145	722517.964525	39.641140
2769.022644	723910.388253	39.646157
2772.152308	725320.434311	39.651175
2774.843302	726708.312114	39.656192
2777.587965	728085.567178	39.661210
2780.049033	729487.053143	39.666228
2782.905642	730883.638819	39.671245
2786.028207	732282.461605	39.676263
2788.458140	733693.112306	39.681280
2791.364381	735088.672137	39.686298
2794.208113	736488.001226	39.691316
2797.052611	737893.258679	39.696333
2799.670549	739299.097451	39.701351
2802.368270	740701.665638	39.706368
2805.370156	742097.966384	39.711386
2808.033209	743502.465062	39.716404
2810.826259	744920.307970	39.721421
2813.444376	746301.379797	39.726439
2816.027730	747696.909676	39.731456
2818.729409	749068.605692	39.736474
2821.510213	750466.617148	39.741492
2824.082764	751837.897360	39.746509
2827.317033	753207.988921	39.751527
2829.919868	754599.176246	39.756544
2832.612101	755950.790345	39.761562
2835.793619	757365.125591	39.766580
2838.260764	758732.638205	39.771597
2841.035366	760130.231440	39.776615
2843.587300	761556.498587	39.781632
2845.997375	762968.052865	39.786650
2848.731407	764395.429538	39.791668
2851.234521	765827.592231	39.796685
2854.134116	767259.564595	39.801703
2856.671750	768697.420975	39.806720
2859.472804	770169.471860	39.811738
2862.161406	771612.936526	39.816756
2865.196603	773091.743905	39.821773
2867.999167	774553.882515	39.826791
2870.435521	776059.465404	39.831808
2873.705701	777555.761608	39.836826
2876.744437	779045.111872	39.841844
2879.171025	780542.900258	39.846861
2882.072003	782045.996291	39.851879
2884.781247	783549.008758	39.856896
2888.299209	785076.206572	39.861914
2890.885130	786618.833820	39.866932
2893.641819	788140.110333	39.871949
2896.433041	789677.876549	39.876967
2899.289951	791234.468617	39.881984
2902.658313	792766.815176	39.887002
2905.160589	794322.690033	39.892020
2907.890348	795877.694564	39.897037
2911.311160	797419.163651	39.902055
2914.454279	798978.360427	39.907072
2917.469598	800539.482386	39.912090
2920.599391	802097.200688	39.917108
2923.224209	803676.478301	39.922125
2926.191777	805231.854504	39.927143
2929.221260	806818.468243	39.932160
2932.068974	808391.443751	39.937178
2935.074254	809973.712408	39.942196
2937.960586	811529.189237	39.947213
2941.544214	813104.622681	39.952231
2944.318926	814700.147920	39.957248
2947.285564	816258.287807	39.962266
2950.295517	817849.218793	39.967284
2953.159846	819430.519925	39.972301
2956.162905	821000.783096	39.977319
2959.574411	822601.938598	39.982336
2962.129745	824171.624323	39.987354
2965.113412	825767.255433	39.992372
2967.840822	827346.986600	39.997389
2971.186844	828935.450514	40.002407
2974.060525	830526.336526	40.007424
2977.696504	832136.785789	40.012442
2980.492717	833729.436453	40.017460
2983.167474	835317.381151	40.022477
2986.229649	836912.273258	40.027495
2989.472771	838509.904898	40.032512
2992.337446	840102.821017	40.037530
2995.428240	841671.315253	40.042548
2998.596259	843264.171402	40.047565
3001.872306	844858.944920	40.052583
3004.784099	846431.351726	40.057600
3007.675554	848028.841231	40.062618
3010.955527	849585.234655	40.067636
3013.305792	851134.301734	40.072653
3016.867594	852664.133613	40.077671
3019.494441	854218.607005	40.082688
3022.534093	855743.979919	40.087706
3025.589559	857265.674046	40.092724
3028.974981	858809.065925	40.097741
3031.900102	860324.979656	40.102759
3034.728984	861867.500890	40.107776
3037.834703	863434.510264	40.112794
3040.923140	864955.649684	40.117812
3043.358837	866532.054878	40.122829
3046.475541	868075.960323	40.127847
3049.156840	869662.846500	40.132864
3051.632581	871218.549751	40.137882
3054.978598	872818.923787	40.142900
3057.508153	874396.062701	40.147917
3060.831764	876006.911473	40.152935
3063.446225	877617.246950	40.157952
3066.512271	879243.319349	40.162970
3069.359013	880866.175942	40.167988
3072.116003	882508.706552	40.173005
3074.814404	884148.080998	40.178023
3078.070911	885818.785905	40.183040
3080.893472	887491.111555	40.188058
3084.185651	889144.146333	40.193076
3087.204798	890840.867662	40.198093
3090.485976	892514.755275	40.203111
3093.034299	894213.744924	40.208128
3096.250255	895935.652993	40.213146
3099.361991	897615.890286	40.218164
3102.672921	899326.249376	40.223181
3106.088110	901023.549271	40.228199
3109.175625	902731.471231	40.233216
3111.823641	904471.400277	40.238234
3115.052680	906193.847688	40.243252
3118.100714	907934.657457	40.248269
3121.184819	909663.565423	40.253287
3124.264875	911424.444407	40.258304
3127.629673	913160.391523	40.263322
3130.760033	914902.271218	40.268340
3133.806556	916649.954960	40.273357
3137.434327	918406.975689	40.278375
3140.430435	920164.303690	40.283392
3143.378144	921948.238716	40.288410
3146.689247	923692.566992	40.293428
3149.758588	925471.771014	40.298445
3153.069066	927236.538572	40.303463
3156.358478	928993.347996	40.308480
3159.284909	930774.078858	40.313498
3162.509104	932533.664291	40.318516
3165.725431	934313.451267	40.323533
3168.784284	936103.197750	40.328551
3172.159394	937873.431230	40.333568
3175.328636	939655.349558	40.338586
3178.848142	941426.466669	40.343604
3181.557188	943214.326938	40.348621
3184.627365	944992.816638	40.353639
3187.999370	946782.494844	40.358656
3191.125148	948584.106460	40.363674
3194.437189	950368.922184	40.368692
3197.154950	952180.990143	40.373709
3200.564883	953965.874234	40.378727
3203.960850	955775.983543	40.383744
3206.905320	957616.360851	40.388762
3210.353292	959450.844490	40.393780
3213.315016	961310.929707	40.398797
3216.726857	963145.124094	40.403815
3219.563593	964974.139224	40.408832
3222.664272	966811.613671	40.413850
3225.974412	968617.708107	40.418868
3228.775473	970417.168954	40.423885
3231.673977	972224.734869	40.428903
3234.838378	974034.906760	40.433920
3237.959867	975852.608489	40.438938
3241.286914	977692.415080	40.443956
3244.126110	979522.646692	40.448973
3247.100441	981360.551702	40.453991
3250.400810	983220.700187	40.459008
3253.398404	985061.403360	40.464026
3256.659852	986929.695955	40.469044
3259.815623	988782.408827	40.474061
3263.187514	990667.652440	40.479079
3266.411423	992556.476841	40.484096
3269.719189	994445.728960	40.489114
3273.311246	996351.213796	40.494132
3276.516750	998252.430964	40.499149
3279.666763	1000140.492682	40.504167
3282.990384	1002051.291562	40.509184
3286.187855	1003973.596260	40.514202
3289.737264	1005882.966182	40.519220
3293.175924	1007807.225127	40.524237
3296.864218	1009725.067145	40.529255
3300.387573	1011665.639320	40.534272
3303.197404	1013578.341217	40.539290
3306.869428	1015502.453482	40.544308
3310.210501	1017441.838798	40.549325
3313.454971	1019370.408924	40.554343
3317.013389	1021320.902784	40.559360
3319.839515	1023256.525731	40.564378
3323.652458	1025222.737384	40.569396
3326.970729	1027164.565746	40.574413
3330.077295	1029138.988236	40.579431
3333.589222	1031081.259469	40.584448
3336.676391	1033047.253269	40.589466
3339.780656	1035013.226808	40.594484
3342.732977	1036984.416600	40.599501
3346.058982	1038983.874882	40.604519
3349.477048	1040967.174602	40.609536
3352.580616	1042968.031996	40.614554
3356.140232	1044977.341220	40.619572
3359.448091	1046998.097621	40.624589
3362.650010	1048981.072748	40.629607
3366.034128	1051003.916484	40.634624
3369.223777	1053037.403249	40.639642
3372.797391	1055046.230977	40.644660
3376.273829	1057080.585392	40.649677
3379.702470	1059100.840902	40.654695
3383.441300	1061125.491325	40.659712
3386.260049	1063152.044921	40.664730
3389.981109	1065207.553446	40.669748
3393.170471	1067223.042436	40.674765
3396.713965	1069265.355277	40.679783
3400.348963	1071292.415097	40.684800
3403.462619	1073339.320251	40.689818
3407.120109	1075396.866596	40.694836
3410.314976	1077438.391882	40.699853
3413.680038	1079487.550388	40.704871
3417.003139	1081527.429252	40.709888
3420.134815	1083580.733896	40.714906
3424.036166	1085623.383909	40.719924
3427.462257	1087680.830365	40.724941
3430.880199	1089736.448173	40.729959
3434.526667	1091776.254104	40.734976
3437.334852	1093832.426301	40.739994
3441.244096	1095882.960246	40.745012
3444.524593	1097910.292611	40.750016
3447.486025	1099891.723573	40.755021
3451.219496	1101829.384517	40.760026
3454.709040	1103693.199853	40.765031
3458.560236	1105466.907603	40.770036
3461.432475	1107184.905777	40.775040
3464.287568	1108788.095585	40.780045
3467.367108	1110336.088746	40.785050
3470.089991	1111798.498516	40.790055
3472.867769	1113183.720132	40.795060
3475.473710	1114514.545342	40.800064
3477.773770	1115740.985644	40.805069
3480.223420	1116893.538225	40.810074
3482.457249	1117998.135747	40.815079
3484.641104	1118994.756020	40.820084
3486.712715	1119949.294771	40.825088
3488.971386	1120844.771647	40.830093
3490.956174	1121646.818930	40.835098
3492.281513	1122418.385287	40.840103
3494.112769	1123127.779635	40.845108
3496.033149	1123767.575117	40.850112
3497.312315	1124365.900470	40.855117
3499.309160	1124918.358280	40.860122
3500.698858	1125406.814485	40.865127
3502.031121	1125825.677115	40.870132
3503.545118	1126243.239978	40.875136
3504.415772	1126581.623285	40.880141
3505.989871	1126884.288244	40.885146
3507.099251	1127151.052779	40.890151
3508.244557	1127364.050904	40.895156
3508.792931	1127577.614439	40.900160
3509.688632	1127722.434749	40.905165
3510.756202	1127858.662080	40.910170
3511.376960	1127951.776270	40.915175
3512.154477	1128028.122573	40.920180
3513.129812	1128081.417338	40.925184
3513.215385	1128093.292960	40.930189
3514.536374	1128091.839216	40.935194
3514.495625	1128051.802613	40.940199
3515.524712	1128007.975084	40.945204
3515.969034	1127931.523012	40.950208
3516.483910	1127844.975565	40.955213
3516.980614	1127746.063952	40.960218
3517.360309	1127605.981330	40.965223
3517.808001	1127474.064688	40.970228
3518.465314	1127322.799140	40.975232
3518.584990	1127138.131441	40.980237
3518.950048	1126958.744518	40.985242
3519.173753	1126747.598477	40.990247
3519.577881	1126545.643215	40.995252
3520.029709	1126303.139973	41.000256
3520.157546	1126090.080763	41.005261
3520.738359	1125852.293336	41.010266
3520.751008	1125589.086136	41.015271
3520.709086	1125330.728328	41.020276
3521.195008	1125061.421804	41.025280
3521.180640	1124769.818166	41.030285
3521.711840	1124486.199005	41.035290
3521.959165	1124191.189389	41.040295
3522.057438	1123885.241174	41.045300
3522.101498	1123587.851960	41.050304
3521.942133	1123264.775431	41.055309
3522.307256	1122938.451151	41.060314
3522.516514	1122616.417194	41.065319
3522.877856	1122263.773568	41.070324
3523.000067	1121935.618916	41.075328
3522.782655	1121596.167589	41.080333
3523.090686	1121243.846400	41.085338
3523.426190	1120897.974034	41.090343
3523.592085	1120528.485311	41.095348
3523.520658	1120167.011698	41.100352
3523.463224	1119792.841391	41.105357
3523.854398	1119431.622967	41.110362
3523.586000	1119050.385554	41.115367
3523.552975	1118676.514291	41.120372
3523.921941	1118305.123533	41.125376
3524.032527	1117914.785622	41.130381
3523.896733	1117529.510922	41.135386
3524.018906	1117137.970863	41.140391
3524.001745	1116741.373328	41.145396
3523.957908	1116343.988242	41.150400
3524.230471	1115952.527464	41.155405
3524.368030	1115564.492521	41.160410
3524.062379	1115164.488997	41.165415
3524.479334	1114743.931157	41.170420
3524.642771	1114341.214458	41.175424
3524.427683	1113937.099370	41.180429
3524.648561	1113515.047012	41.185434
3524.386133	1113125.757054	41.190439
3524.504680	1112705.374767	41.195444
3524.607670	1112289.922751	41.200448
3524.414014	1111877.540378	41.205453
3524.600445	1111445.218206	41.210458
3524.503734	1111043.251073	41.215463
3524.214640	1110608.363590	41.220468
3524.518359	1110206.649646	41.225472
3524.328255	1109797.065452	41.230477
3524.575669	1109366.856651	41.235482
3523.952872	1108954.893364	41.240487
3524.480437	1108541.372573	41.245492
3524.258640	1108106.558042	41.250496
3523.768955	1107691.421007	41.255501
3524.358224	1107258.313929	41.260506
3524.435667	1106850.180042	41.265511
3524.541363	1106443.061073	41.270516
3524.035785	1106004.589983	41.275520
3524.038703	1105598.188149	41.280525
3524.656852	1105147.809395	41.285530
3524.421759	1104730.205090	41.290535
3524.458139	1104304.498524	41.295540
3524.520943	1103874.072257	41.300544
3524.039961	1103446.090028	41.305549
3524.152501	1103010.617886	41.310554
3523.986430	1102589.491771	41.315559
3523.894343	1102171.379030	41.320564
3524.246545	1101727.926681	41.325568
3524.266087	1101312.692140	41.330573
3524.491427	1100895.001812	41.335578
3524.356307	1100444.641250	41.340583
3524.423278	1100023.276552	41.345588
3524.326414	1099572.837010	41.350592
3524.228446	1099145.980617	41.355597
3524.159520	1098696.706632	41.360602
3524.119480	1098271.684406	41.365607
3524.009653	1097832.388040	41.370612
3524.103366	1097405.171327	41.375616
3524.165808	1096993.615516	41.380621
3524.226077	1096546.437635	41.385626
3524.002065	1096113.048002	41.390631
3523.776529	1095676.083357	41.395636
3524.103959	1095241.384830	41.400640
3523.765508	1094812.981980	41.405645
3524.069687	1094379.175148	41.410650
3524.065402	1093953.616420	41.415655
3524.076867	1093514.332451	41.420660
3523.960947	1093072.831913	41.425664
3523.846813	1092638.763190	41.430669
3524.217455	1092193.855628	41.435674
3523.573406	1091780.487925	41.440679
3523.690945	1091327.315643	41.445684
3523.617089	1090896.644246	41.450688
3523.920282	1090458.118159	41.455693
3523.760223	1090027.583564	41.460698
3523.697819	1089579.563455	41.465703
3523.818214	1089162.613236	41.470708
3523.796258	1088729.174573	41.475712
3523.778930	1088283.818739	41.480717
3523.584940	1087855.321395	41.485722
3523.622962	1087412.759919	41.490727
3523.352815	1086990.436302	41.495732
3523.472470	1086540.602071	41.500736
3523.297804	1086114.552316	41.505741
3523.578424	1085676.219075	41.510746
3523.418369	1085251.249703	41.515751
3523.585782	1084794.456100	41.520756
3523.580740	1084371.693698	41.525760
3523.387413	1083947.107417	41.530765
3523.548066	1083489.438242	41.535770
3523.147853	1083083.040718	41.540775
3523.397982	1082628.449588	41.545780
3523.263230	1082189.999956	41.550784
3523.637398	1081754.788997	41.555789
3523.437862	1081306.589390	41.560794
3523.386187	1080898.244492	41.565799
3523.123790	1080450.464610	41.570804
3523.337329	1080028.096766	41.575808
3523.175125	1079594.625101	41.580813
3523.242396	1079144.380319	41.585818
3523.346916	1078732.200208	41.590823
3523.168555	1078278.084839	41.595828
3523.144637	1077837.827026	41.600832
3522.724222	1077418.241760	41.605837
3522.815273	1076974.150892	41.610842
3522.892682	1076561.523325	41.615847
3522.843292	1076140.242336	41.620852
3522.758177	1075695.596395	41.625856
3522.550853	1075258.234254	41.630861
3523.100163	1074828.397157	41.635866
3522.849817	1074404.229792	41.640871
3522.777196	1073971.065462	41.645876
3522.856224	1073530.155393	41.650880
3522.538215	1073108.781143	41.655885
3522.771435	1072672.292711	41.660890
3522.453500	1072257.675728	41.665895
3522.306733	1071818.490919	41.670900
3522.283341	1071403.280170	41.675904
3522.041658	1070975.481444	41.680909
3522.332050	1070554.387129	41.685914
3522.175498	1070114.009801	41.690919
3522.214557	1069707.505201	41.695924
3522.359326	1069269.991024	41.700928
3522.403186	1068841.497901	41.705933
3522.456324	1068417.585962	41.710938
3522.344133	1067990.109905	41.715943
3522.342238	1067582.877488	41.720948
3521.950935	1067151.919424	41.725952
3522.110552	1066730.168199	41.730957
3521.990376	1066299.098518	41.735962
3521.945759	1065884.339116	41.740967
3521.977892	1065442.882126	41.745972
3522.292726	1065018.760778	41.750976
3521.735503	1064612.939192	41.755981
3521.961307	1064187.036044	41.760986
3521.951302	1063775.095280	41.765991
3521.767783	1063339.953729	41.770996
3522.109037	1062922.885768	41.776000
3521.702080	1062507.160979	41.781005
3522.030170	1062076.360065	41.786010
3522.078991	1061661.940559	41.791015
3521.658468	1061213.478205	41.796020
3521.906310	1060812.058265	41.801024
3521.543871	1060398.863335	41.806029
3521.621103	1059969.190855	41.811034
3521.555243	1059573.222423	41.816039
3521.950094	1059133.799920	41.821044
3521.610593	1058720.186257	41.826048
3521.592489	1058304.176265	41.831053
3521.533687	1057883.131121	41.836058
3521.395211	1057466.403242	41.841063
3521.386872	1057049.333322	41.846068
3521.228946	1056635.918816	41.851072
3521.346657	1056223.391765	41.856077
3521.256651	1055804.506261	41.861082
3521.231915	1055389.723346	41.866087
3521.297941	1054985.209718	41.871092
3520.979922	1054570.124301	41.876096
3521.193850	1054150.773993	41.881101
3521.235876	1053740.773619	41.886106
3520.985349	1053324.137013	41.891111
3521.034169	1052921.500173	41.896116
3520.861015	1052495.529933	41.901120
3520.780253	1052082.919077	41.906125
3521.083603	1051670.310622	41.911130
3520.673946	1051278.337026	41.916135
3520.848358	1050863.277836	41.921140
3520.982026	1050454.369237	41.926144
3520.440386	1050057.699593	41.931149
3520.758612	1049656.227950	41.936154
3520.540547	1049242.076767	41.941159
3520.655535	1048826.488556	41.946164
3520.627155	1048430.968950	41.951168
3520.772842	1048040.797924	41.956173
3520.881082	1047626.279077	41.961178
3520.497910	1047211.520527	41.966183
3520.606092	1046805.918636	41.971188
3520.674983	1046388.899992	41.976192
3520.245827	1045984.967965	41.981197
3520.250500	1045585.473814	41.986202
3520.187251	1045185.575762	41.991207
3519.857654	1044769.756451	41.996212
3520.278648	1044383.242504	42.001216
3519.844572	1043986.120173	42.006221
3520.253021	1043586.898562	42.011226
3520.109424	1043202.810503	42.016231
3520.355362	1042792.834730	42.021236
3519.976325	1042410.083255	42.026240
3519.930897	1042011.306234	42.031245
3520.132474	1041609.367462	42.036250
3519.871509	1041216.753775	42.041255
3519.741117	1040800.894217	42.046260
3519.785090	1040419.675654	42.051264
3519.648315	1040022.317466	42.056269
3519.571570	1039631.108070	42.061274
3519.695628	1039248.539263	42.066279
3519.589434	1038838.523055	42.071284
3519.725067	1038466.534108	42.076288
3519.824898	1038065.419466	42.081293
3519.724052	1037660.053842	42.086298
3519.732019	1037287.620288	42.091303
3519.682481	1036886.251840	42.096308
3519.776283	1036494.600347	42.101312
3519.540933	1036107.328570	42.106317
3519.785483	1035705.342901	42.111322
3519.372314	1035326.269110	42.116327
3519.412208	1034926.389401	42.121332
3519.293933	1034530.764567	42.126336
3519.407442	1034158.297888	42.131341
3519.101777	1033755.294493	42.136346
3519.384201	1033386.813015	42.141351
3519.457645	1032999.855084	42.146356
3519.525745	1032614.129525	42.151360
3519.072857	1032221.686986	42.156365
3518.992709	1031825.186291	42.161370
3519.063347	1031454.579095	42.166375
3518.906921	1031054.647696	42.171380
3519.146753	1030673.213511	42.176384
3518.989566	1030308.764810	42.181389
3519.270000	1029911.584640	42.186394
3519.035237	1029533.249713	42.191399
3518.945429	1029155.640126	42.196404
3518.855973	1028766.381571	42.201408
3518.862087	1028379.114400	42.206413
3519.055355	1028007.095823	42.211418
3518.784683	1027625.634534	42.216423
3518.532436	1027238.815336	42.221428
3518.671468	1026875.741022	42.226432
3518.609184	1026481.280375	42.231437
3518.521881	1026105.111641	42.236442
3518.435432	1025739.093472	42.241447
3518.554680	1025362.840828	42.246452
3518.717271	1024991.208261	42.251456
3518.267401	1024619.070303	42.256461
3518.610987	1024252.399437	42.261466
3518.603546	1023868.021203	42.266471
3518.441222	1023497.312485	42.271476
3518.829730	1023109.326682	42.276480
3518.239928	1022726.905268	42.281485
3518.289362	1022372.086642	42.286490
3518.291697	1021975.843326	42.291495
3517.956326	1021628.023488	42.296500
3518.258533	1021245.257079	42.301504
3517.761418	1020892.083675	42.306509
3518.451759	1020523.753797	42.311514
3518.148954	1020143.922027	42.316519
3518.250351	1019782.625298	42.321524
3518.376681	1019393.358392	42.326528
3518.027868	1019036.162770	42.331533
3517.949637	1018655.417029	42.336538
3518.042912	1018302.177436	42.341543
3517.657979	1017922.888186	42.346548
3517.656006	1017565.541882	42.351552
3517.572673	1017207.895065	42.356557
3517.504240	1016830.615293	42.361562
3517.683519	1016480.450244	42.366567
3517.555373	1016116.819845	42.371572
3517.538126	1015764.312629	42.376576
3517.544799	1015411.196820	42.381581
3517.382103	1015046.629067	42.386586
3517.217892	1014695.147129	42.391591
3517.101718	1014331.690638	42.396596
3517.304360	1013984.376773	42.401600
3517.256018	1013617.852368	42.406605
3517.485815	1013257.183211	42.411610
3517.205950	1012925.327102	42.416615
3517.127666	1012559.710092	42.421620
3517.076725	1012222.626339	42.426624
3516.977566	1011860.853305	42.431629
3517.017381	1011518.660471	42.436634
3516.957802	1011170.147448	42.441639
3516.971917	1010805.761697	42.446644
3517.035061	1010460.585607	42.451648
3516.958281	1010111.329697	42.456653
3516.886916	1009755.831088	42.461658
3517.070201	1009430.982090	42.466663
3516.642235	1009060.044192	42.471668
3516.677734	1008705.433791	42.476672
3516.535749	1008366.384623	42.481677
3516.707901	1008010.347032	42.486682
3516.787147	1007683.275692	42.491687
3516.783815	1007331.599358	42.496692
3516.958798	1006995.138103	42.501696
3516.676761	1006649.591169	42.506701
3516.490597	1006309.161527	42.511706
3516.639143	1005960.778536	42.516711
3516.518146	1005615.433566	42.521716
3516.599783	1005274.605680	42.526720
3516.648597	1004942.322688	42.531725
3516.611951	1004581.628739	42.536730
3516.394871	1004246.527534	42.541735
3516.185648	1003913.253694	42.546740
3516.540963	1003555.932216	42.551744
3516.504527	1003219.767433	42.556749
3516.238921	1002886.928905	42.561754
3516.352832	1002552.451254	42.566759
3516.032382	1002219.679812	42.571764
3516.016343	1001869.611983	42.576768
3515.635865	1001544.110140	42.581773
3516.092274	1001202.293738	42.586778
3516.092888	1000882.239302	42.591783
3515.842823	1000552.667906	42.596788
3515.998953	1000219.603022	42.601792
3515.815217	999888.911174	42.606797
3515.707631	999551.371872	42.611802
3516.051116	999236.815199	42.616807
3515.851315	998895.162402	42.621812
3515.932428	998577.691050	42.626816
3515.427457	998234.880116	42.631821
3516.052625	997893.323221	42.636826
3515.657281	997580.549431	42.641831
3515.623201	997248.997077	42.646836
3515.830646	996926.444785	42.651840
3515.753590	996600.511437	42.656845
3515.492537	996269.621139	42.661850
3515.430152	995957.092662	42.666855
3515.304499	995620.783705	42.671860
3515.330883	995302.553428	42.676864
3515.338394	994962.578306	42.681869
3515.372725	994655.516577	42.686874
3515.246490	994353.434904	42.691879
3515.308530	994010.275224	42.696884
3515.484202	993697.290751	42.701888
3515.102860	993380.969269	42.706893
3515.218422	993057.724919	42.711898
3515.168682	992736.829000	42.716903
3514.754514	992430.695706	42.721908
3514.931224	992103.389999	42.726912
3514.908957	991813.440336	42.731917
3515.106836	991480.537867	42.736922
3514.911616	991186.879577	42.741927
3515.005205	990856.395491	42.746932
3515.117868	990557.485697	42.751936
3514.863325	990229.167959	42.756941
3514.896675	989919.022209	42.761946
3514.552941	989615.359067	42.766951
3514.912793	989287.763648	42.771956
3515.040325	988992.475801	42.776960
3514.800234	988681.819944	42.781965
3514.775694	988361.648531	42.786970
3514.510399	988062.377282	42.791975
3514.299114	987747.958337	42.796980
3514.545083	987431.104954	42.801985
3514.658584	987133.869156	42.806989
3514.398499	986837.167306	42.811994
3514.388299	986519.134406	42.816999
3514.540657	986238.533273	42.822004
3514.300403	985925.189646	42.827009
3514.573774	985621.407075	42.832013
3514.283222	985320.531895	42.837018
3514.404802	985009.420983	42.842023
3514.335958	984711.600847	42.847028
3514.347165	984404.282306	42.852033
3514.179775	984104.103673	42.857037
3514.255475	983797.132333	42.862042
3514.371898	983511.814082	42.867047
3514.104384	983219.514313	42.872052
3514.088388	982894.249720	42.877057
3513.805616	982624.088797	42.882061
3513.892528	982302.093827	42.887066
3513.845282	982008.816836	42.892071
3513.679748	981725.116072	42.897076
3513.845140	981426.402228	42.902081
3513.582177	981137.999881	42.907085
3513.738120	980857.524254	42.912090
3513.976127	980559.925395	42.917095
3513.858353	980261.392681	42.922100
3514.027625	979966.607454	42.927105
3513.459212	979693.521624	42.932109
3513.801056	979384.705985	42.937114
3513.484173	979092.691697	42.942119
3513.414609	978812.641475	42.947124
3513.981636	978527.097763	42.952129
3513.784912	978232.478890	42.957133
3513.468018	977946.367671	42.962138
3513.605013	977655.378082	42.967143
3513.483204	977368.521653	42.972148
3513.780792	977080.995266	42.977153
3513.322515	976797.293652	42.982157
3513.538614	976522.754133	42.987162
3513.284332	976227.748253	42.992167
3513.292415	975941.189974	42.997172
3513.314733	975669.672357	43.002177
3513.277539	975367.057722	43.007181
3513.123961	975090.750419	43.012186
3512.996465	974807.286862	43.017191
3512.960589	974524.576547	43.022196
3512.997590	974258.270524	43.027201
3512.842475	973982.007812	43.032205
3513.213009	973717.969045	43.037210
3513.059771	973431.018381	43.042215
3512.647388	973162.779229	43.047220
3512.902195	972871.429379	43.052225
3512.615479	972599.425919	43.057229
3512.909026	972332.401238	43.062234
3512.862679	972061.310991	43.067239
3512.888398	971788.239246	43.072244
3512.966225	971496.359523	43.077249
3512.382589	971251.933586	43.082253
3512.748436	970971.134627	43.087258
3512.619592	970705.082361	43.092263
3512.318078	970429.357659	43.097268
3512.853403	970183.331815	43.102273
3512.492546	969902.404558	43.107277
3512.651081	969625.195248	43.112282
3512.310629	969377.419460	43.117287
3512.504079	969110.065630	43.122292
3512.915020	968828.273514	43.127297
3512.588748	968564.895583	43.132301
3512.534015	968288.537981	43.137306
3512.714137	968035.821460	43.142311
3512.673399	967756.890466	43.147316
3512.634151	967492.045360	43.152321
3512.334845	967200.890688	43.157325
3512.583516	966944.002288	43.162330
3512.568325	966675.394514	43.167335
3512.582779	966425.278565	43.172340
3512.561897	966142.740443	43.177345
3512.297187	965889.709075	43.182349
3512.534615	965634.820847	43.187354
3512.667070	965353.002261	43.192359
3512.100130	965079.709236	43.197364
3512.131235	964816.786430	43.202369
3512.138708	964561.888571	43.207373
3512.286507	964301.274144	43.212378
3511.974728	964036.216863	43.217383
3511.886133	963785.023414	43.222388
3512.105151	963523.382286	43.227393
3511.994821	963266.878805	43.232397
3512.102227	963004.056646	43.237402
3511.977637	962762.623596	43.242407
3511.860461	962481.195558	43.247412
3512.041749	962243.708366	43.252417
3512.087423	961996.628979	43.257421
3512.100651	961732.686273	43.262426
3511.875751	961477.200135	43.267431
3511.877432	961212.451382	43.272436
3511.983929	960947.085058	43.277441
3511.701150	960709.022939	43.282445
3512.041015	960472.809109	43.287450
3512.173660	960200.835895	43.292455
3511.810192	959946.775350	43.297460
3511.952822	959693.012443	43.302465
3511.316391	959457.702238	43.307469
3511.537868	959183.509324	43.312474
3511.369355	958941.629333	43.317479
3511.586941	958693.595657	43.322484
3511.834544	958447.801950	43.327489
3511.781560	958203.126086	43.332493
3511.461844	957937.691567	43.337498
3511.218486	957680.765326	43.342503
3511.182156	957448.118685	43.347508
3511.345479	957211.702410	43.352513
3511.277367	956958.246369	43.357517
3511.472056	956705.030217	43.362522
3511.609467	956467.999200	43.367527
3511.220051	956222.215720	43.372532
3511.435081	955975.439236	43.377537
3511.288902	955726.199485	43.382541
3511.395957	955502.807309	43.387546
3511.288440	955252.186306	43.392551
3511.126518	955028.435096	43.397556
3511.182697	954787.997092	43.402561
3510.789933	954559.385744	43.407565
3510.857566	954324.471256	43.412570
3510.772712	954103.249199	43.417575
3510.618329	953860.889136	43.422580
3511.065435	953639.655025	43.427585
3510.822744	953414.411398	43.432589
3511.019424	953179.422965	43.437594
3510.973626	952950.012693	43.442599
3510.907834	952732.268009	43.447604
3510.776103	952500.364124	43.452609
3510.500319	952276.893773	43.457613
3510.846407	952040.393137	43.462618
3510.567684	951818.434299	43.467623
3510.658075	951603.295304	43.472628
3510.699369	951365.473959	43.477633
3510.456343	951157.740264	43.482637
3510.361288	950926.811886	43.487642
3510.626972	950707.873758	43.492647
3510.758879	950488.661178	43.497652
3510.902029	950253.068772	43.502657
3510.612665	950036.777997	43.507661
3510.435612	949818.640730	43.512666
3510.341753	949592.438741	43.517671
3510.217960	949378.582133	43.522676
3510.187891	949164.892690	43.527681
3510.005876	948946.432041	43.532685
3510.282059	948727.599404	43.537690
3510.104970	948525.206308	43.542695
3510.026984	948297.508511	43.547700
3510.082358	948086.728842	43.552705
3509.856769	947882.977848	43.557709
3509.771316	947660.711909	43.562714
3509.931932	947475.460817	43.567719
3509.916776	947255.847574	43.572724
3510.273030	947032.045163	43.577729
3509.805605	946837.487922	43.582733
3509.864823	946620.230098	43.587738
3510.017991	946413.580868	43.592743
3510.029191	946197.175351	43.597748
3509.948313	946000.990219	43.602753
3509.745042	945792.842102	43.607757
3509.898813	945579.069853	43.612762
3509.574998	945376.098583	43.617767
3509.572146	945155.819364	43.622772
3509.789996	944955.425313	43.627777
3510.014216	944770.546110	43.632781
3509.687406	944550.869533	43.637786
3509.652749	944348.385424	43.642791
3509.618968	944143.593213	43.647796
3509.973816	943934.991163	43.652801
3509.732281	943747.564612	43.657805
3509.541912	943523.796732	43.662810
3509.475322	943317.731399	43.667815
3509.571720	943128.789134	43.672820
3509.481793	942916.577056	43.677825
3509.223754	942731.608981	43.682829
3509.466647	942535.431406	43.687834
3509.505473	942329.788981	43.692839
3509.388570	942142.763514	43.697844
3509.524792	941938.911235	43.702849
3509.290506	941737.892563	43.707853
3509.295687	941547.278079	43.712858
3509.360360	941354.441431	43.717863
3509.149791	941151.478541	43.722868
3509.110582	940958.836197	43.727873
3508.985666	940747.021174	43.732877
3509.222990	940570.717646	43.737882
3508.815888	940365.838610	43.742887
3508.482928	940197.001161	43.747892
3509.038382	939984.467779	43.752897
3509.056915	939818.725366	43.757901
3509.126276	939617.479300	43.762906
3509.122169	939435.709955	43.767911
3509.090857	939252.020274	43.772916
3508.933454	939041.388705	43.777921
3509.120843	938855.442740	43.782925
3509.333131	938676.873214	43.787930
3509.246679	938466.590657	43.792935
3508.848023	938292.713844	43.797940
3509.165771	938100.771211	43.802945
3509.125103	937909.360365	43.807949
3509.205188	937710.822066	43.812954
3508.772597	937519.077763	43.817959
3508.770092	937319.194893	43.822964
3509.262292	937147.916396	43.827969
3508.786900	936955.007035	43.832973
3508.713755	936756.266066	43.837978
3508.589200	936572.018305	43.842983
3508.543829	936385.447588	43.847988
3508.600437	936224.768471	43.852993
3508.426865	936043.869686	43.857997
3508.335656	935867.270586	43.863002
3508.326557	935679.997056	43.868007
3508.244438	935498.776568	43.873012
3508.353494	935320.398310	43.878017
3508.379897	935159.403781	43.883021
3508.166089	934965.610625	43.888026
3508.253692	934794.898505	43.893031
3508.018745	934623.657948	43.898036
3508.348976	934449.726399	43.903041
3508.143155	934290.567953	43.908045
3507.997091	934112.767125	43.913050
3508.302842	933938.342733	43.918055
3507.775244	933767.026668	43.923060
3507.946948	933607.785540	43.928065
3507.959885	933428.303087	43.933069
3508.070146	933255.617029	43.938074
3508.170606	933091.570400	43.943079
3507.818418	932914.627712	43.948084
3507.940257	932754.792974	43.953089
3507.968634	932606.494450	43.958093
3508.017415	932424.667064	43.963098
3508.050109	932268.194134	43.968103
3507.835980	932100.710839	43.973108
3507.510705	931922.866202	43.978113
3507.409156	931767.169124	43.983117
3507.838183	931594.856941	43.988122
3507.774259	931424.637813	43.993127
3507.473385	931274.531113	43.998132
3507.636353	931103.687938	44.003137
3507.481325	930956.142243	44.008141
3507.791775	930787.666568	44.013146
3507.871898	930639.400825	44.018151
3507.619001	930468.894067	44.023156
3507.827517	930310.412985	44.028161
3507.772784	930146.205097	44.033165
3507.531242	929978.755731	44.038170
3507.712273	929830.547006	44.043175
3507.697431	929662.762109	44.048180
3507.663091	929501.317941	44.053185
3507.630366	929344.289490	44.058189
3507.479266	929181.317207	44.063194
3507.739123	929030.670627	44.068199
3507.737318	928880.062908	44.073204
3507.815230	928711.944577	44.078209
3507.426867	928536.881013	44.083213
3507.350993	928382.811191	44.088218
3507.554677	928226.095502	44.093223
3507.417088	928071.738528	44.098228
3507.576049	927912.521706	44.103233
3507.300648	927769.906741	44.108237
3507.351188	927595.220802	44.113242
3507.328878	927453.132553	44.118247
3507.239335	927289.708051	44.123252
3507.767855	927140.502408	44.128257
3507.433837	926971.339784	44.133261
3507.419494	926832.214390	44.138266
3507.548265	926678.542693	44.143271
3507.294794	926516.756294	44.148276
3507.052842	926376.406566	44.153281
3507.024812	926215.535561	44.158285
3506.915989	926070.540168	44.163290
3506.885309	925922.835329	44.168295
3506.969343	925766.356117	44.173300
3507.165469	925628.607484	44.178305
3506.984328	925483.704377	44.183309
3507.126982	925327.298937	44.188314
3507.086986	925185.538422	44.193319
3506.891947	925041.106607	44.198324
3507.093820	924876.021893	44.203329
3506.930959	924745.908494	44.208333
3507.146625	924592.932502	44.213338
3506.955504	924450.408042	44.218343
3506.850454	924309.500968	44.223348
3506.970314	924155.277821	44.228353
3506.950655	924011.462960	44.233357
3507.013314	923843.579799	44.238362
3507.063252	923713.598892	44.243367
3506.530569	923557.542050	44.248372
3506.716433	923412.138055	44.253377
3506.665852	923287.070244	44.258381
3506.480755	923148.166578	44.263386
3506.512523	923014.996747	44.268391
3506.175964	922876.495932	44.273396
3506.555134	922741.145285	44.278401
3506.403963	922604.435225	44.283405
3506.326766	922473.290771	44.288410
3506.489351	922345.183027	44.293415
3506.573760	922202.842666	44.298420
3506.337437	922073.254476	44.303425
3506.563763	921930.594892	44.308429
3506.374784	921789.732293	44.313434
3506.181908	921668.500183	44.318439
3506.322703	921528.635159	44.323444
3506.405814	921391.855953	44.328449
3506.610680	921266.025719	44.333453
3506.341244	921134.976841	44.338458
3506.582164	920993.734033	44.343463
3506.389569	920869.788929	44.348468
3506.827077	920720.228564	44.353473
3506.244045	920590.469583	44.358477
3506.550699	920452.571055	44.363482
3506.419695	920312.430728	44.368487
3506.495515	920202.384832	44.373492
3506.492957	920057.499632	44.378497
3506.160070	919929.127741	44.383501
3506.480868	919804.111073	44.388506
3506.571251	919657.948359	44.393511
3506.313305	919522.237400	44.398516
3506.257697	919386.489735	44.403521
3506.134800	919253.349475	44.408525
3506.404489	919146.620316	44.413530
3505.957520	919008.424239	44.418535
3506.143515	918870.987031	44.423540
3506.279313	918736.732346	44.428545
3506.276348	918613.378733	44.433549
3506.198842	918477.804668	44.438554
3506.056536	918372.765329	44.443559
3505.856438	918236.338758	44.448564
3505.904149	918111.039394	44.453569
3506.020955	917993.141456	44.458573
3506.208023	917853.752344	44.463578
3506.139994	917728.655906	44.468583
3505.777425	917604.086693	44.473588
3506.297247	917473.590312	44.478593
3505.924364	917359.419407	44.483597
3505.905099	917238.541751	44.488602
3505.821828	917113.337440	44.493607
3505.788465	916987.351447	44.498612
3506.136867	916869.198511	44.503617
3506.148197	916742.814228	44.508621
3506.096497	916621.735650	44.513626
3506.265402	916484.048648	44.518631
3505.689018	916364.495820	44.523636
3506.102149	916232.253424	44.528641
3506.086968	916123.489133	44.533645
3505.910817	916000.779564	44.538650
3506.102131	915869.335705	44.543655
3506.069536	915750.354338	44.548660
3505.905169	915618.288630	44.553665
3505.699918	915496.536077	44.558669
3505.768564	915381.673154	44.563674
3505.964984	915252.622536	44.568679
3506.019406	915140.358515	44.573684
3505.942116	915016.550746	44.578689
3505.946268	914889.932282	44.583693
3506.066712	914763.580841	44.588698
3505.649834	914653.986355	44.593703
3505.624324	914528.520852	44.598708
3506.005081	914414.935496	44.603713
3505.794741	914282.267056	44.608717
3505.431336	914160.607355	44.613722
3505.736232	914054.447909	44.618727
3505.449950	913933.252367	44.623732
3505.684827	913817.172877	44.628737
3505.561258	913700.089775	44.633741
3505.451695	913598.712575	44.638746
3505.527453	913480.917297	44.643751
3505.409405	913372.790280	44.648756
3505.536319	913238.595344	44.653761
3505.576642	913141.811818	44.658765
3505.432716	913012.764803	44.663770
3505.538961	912914.134928	44.668775
3505.375126	912800.220448	44.673780
3505.383520	912689.070861	44.678785
3505.789205	912557.319870	44.683789
3505.774989	912453.303061	44.688794
3505.542619	912332.449099	44.693799
3505.349071	912234.145690	44.698804
3505.384192	912105.047986	44.703809
3505.540375	912007.550641	44.708813
3505.499303	911904.684884	44.713818
3505.645478	911787.709644	44.718823
3505.324309	911662.516944	44.723828
3505.265915	911551.259078	44.728833
3505.277250	911449.051164	44.733837
3504.949720	911341.015328	44.738842
3505.143464	911245.426856	44.743847
3505.138417	911139.937469	44.748852
3505.656267	911000.320338	44.753857
3505.374298	910913.772468	44.758861
3505.314813	910818.218342	44.763866
3505.452772	910688.202784	44.768871
3505.324309	910572.982976	44.773876
3505.487963	910472.660720	44.778881
3505.444733	910356.072224	44.783885
3504.998370	910252.278144	44.788890
3505.191903	910159.950061	44.793895
3504.874108	910046.968739	44.798900
3505.135345	909955.976364	44.803905
3504.762776	909843.964412	44.808909
3504.775226	909719.155128	44.813914
3505.281606	909609.983699	44.818919
3504.741628	909533.005721	44.823924
3504.983188	909421.173458	44.828929
3504.696920	909336.241467	44.833933
3505.160101	909227.166103	44.838938
3505.094290	909127.146737	44.843943
3504.593152	909030.862909	44.848948
3504.807930	908931.179660	44.853953
3505.079685	908818.365656	44.858957
3504.555169	908716.002762	44.863962
3504.788028	908622.581522	44.868967
3504.586626	908517.557039	44.873972
3504.601903	908427.351969	44.878977
3504.827497	908338.075556	44.883981
3504.573824	908238.071163	44.888986
3504.868240	908143.859940	44.893991
3504.805853	908050.091821	44.898996
3504.784306	907942.807820	44.904001
3504.782057	907861.183440	44.909005
3504.656385	907757.096996	44.914010
3504.948800	907668.860216	44.919015
3504.628025	907574.451247	44.924020
3504.915996	907463.536949	44.929025
3504.788808	907368.610156	44.934029
3504.734400	907273.862751	44.939034
3504.541708	907168.714935	44.944039
3504.726235	907082.513083	44.949044
3504.691213	906984.862650	44.954049
3504.789068	906889.794153	44.959053
3504.624826	906794.477702	44.964058
3504.741627	906704.035052	44.969063
3504.177471	906613.703101	44.974068
3504.496966	906508.941035	44.979073
3504.577513	906435.195797	44.984077
3504.562125	906329.037890	44.989082
3504.657317	906240.618031	44.994087
3504.464431	906169.423645	44.999092
3504.595881	906060.051506	45.004097
3504.421567	905967.907631	45.009101
3504.396952	905878.343582	45.014106
3504.483980	905780.072904	45.019111
3504.203952	905710.527876	45.024116
3504.545323	905617.714171	45.029121
3504.180967	905532.157985	45.034125
3504.135307	905438.536343	45.039130
3504.407775	905344.571154	45.044135
3504.378790	905255.094390	45.049140
3504.488297	905164.917671	45.054145
3504.319915	905073.916484	45.059149
3504.321010	905004.219852	45.064154
3504.171210	904920.356587	45.069159
3504.158166	904822.085601	45.074164
3504.270904	904747.926709	45.079169
3504.166398	904657.197854	45.084173
3504.209732	904570.884068	45.089178
3504.240072	904485.633062	45.094183
3503.717874	904397.092734	45.099188
3504.116246	904331.956426	45.104193
3504.120313	904237.823833	45.109197
3503.960883	904164.957180	45.114202
3504.007252	904079.600824	45.119207
3503.885228	903989.926118	45.124212
3503.974679	903911.511778	45.129217
3503.921036	903837.175165	45.134221
3504.011611	903760.979273	45.139226
3504.132310	903675.411429	45.144231
3504.009062	903622.229241	45.149236
3504.033216	903525.764042	45.154241
3503.642853	903451.188112	45.159245
3503.806889	903384.920719	45.164250
3504.077784	903297.584287	45.169255
3504.123785	903211.152623	45.174260
3504.274374	903120.163811	45.179265
3504.026602	903053.380951	45.184269
3503.990451	902962.999761	45.189274
3504.339915	902887.328813	45.194279
3504.087217	902802.195481	45.199284
3503.847012	902710.878142	45.204289
3503.781352	902652.462366	45.209293
3504.162002	902573.981433	45.214298
3503.890097	902485.273190	45.219303
3503.871393	902420.086895	45.224308
3504.076071	902327.531131	45.229313
3503.685299	902253.905200	45.234317
3504.006316	902180.161066	45.239322
3504.169223	902077.370381	45.244327
3504.110151	902019.429881	45.249332
3503.977375	901930.689996	45.254337
3503.804072	901866.102281	45.259341
3503.755024	901781.209746	45.264346
3503.766007	901703.067361	45.269351
3503.793770	901642.307572	45.274356
3504.175181	901554.829362	45.279361
3503.725086	901481.879272	45.284365
3503.906176	901384.868619	45.289370
3504.019463	901326.216446	45.294375
3503.913294	901262.190344	45.299380
3503.983240	901169.541197	45.304385
3503.735229	901107.372090	45.309389
3503.951859	901022.520994	45.314394
3504.063640	900948.505448	45.319399
3503.697886	900864.424128	45.324404
3503.913048	900790.292879	45.329409
3503.665960	900722.806070	45.334413
3503.872090	900644.713518	45.339418
3503.759318	900584.158720	45.344423
3503.727252	900505.233994	45.349428
3503.765291	900417.794761	45.354433
3503.781266	900352.675509	45.359437
3504.145789	900257.450962	45.364442
3503.654172	900194.152560	45.369447
3503.561924	900132.236923	45.374452
3503.718132	900043.516427	45.379457
3503.486859	899987.032734	45.384461
3503.718490	899911.148115	45.389466
3503.520000	899840.937403	45.394471
3503.717765	899773.559246	45.399476
3503.682578	899696.749475	45.404481
3503.654407	899620.420636	45.409485
3503.842337	899575.458865	45.414490
3503.743897	899485.998576	45.419495
3503.770570	899404.343254	45.424500
3503.715534	899326.565444	45.429505
3503.573202	899275.181431	45.434509
3503.656668	899193.417086	45.439514
3503.955132	899131.619430	45.444519
3503.827984	899052.980042	45.449524
3503.684702	898962.842442	45.454529
3503.947685	898896.312861	45.459533
3503.795294	898816.707977	45.464538
3503.751237	898742.882574	45.469543
3503.662305	898686.072552	45.474548
3503.638977	898616.784249	45.479553
3503.501426	898539.202528	45.484557
3503.287666	898481.347933	45.489562
3503.837945	898395.822702	45.494567
3503.556085	898339.524225	45.499572
3503.833511	898269.408969	45.504577
3503.802910	898201.663182	45.509581
3503.614282	898134.812477	45.514586
3503.719443	898049.258704	45.519591
3503.362705	897995.965379	45.524596
3503.635331	897903.712749	45.529601
3503.200220	897844.341649	45.534605
3503.249009	897773.291381	45.539610
3503.414165	897700.094574	45.544615
3503.392769	897645.196192	45.549620
3503.500544	897571.040585	45.554625
3503.822893	897513.571140	45.559629
3503.560209	897454.360891	45.564634
3503.536399	897374.037987	45.569639
3503.601473	897295.632614	45.574644
3503.624178	897241.883063	45.579649
3503.384860	897164.589352	45.584653
3503.315752	897109.113655	45.589658
3503.662203	897050.088873	45.594663
3503.566260	896968.612102	45.599668
3503.378415	896898.943294	45.604673
3503.534718	896833.277220	45.609677
3503.529279	896751.589092	45.614682
3503.590864	896694.154341	45.619687
3503.369336	896627.484701	45.624692
3503.564890	896563.452557	45.629697
3503.219243	896509.370060	45.634701
3503.404877	896454.812823	45.639706
3503.587048	896377.729054	45.644711
3503.517236	896315.478091	45.649716
3503.357743	896241.735944	45.654721
3503.373195	896172.508190	45.659725
3503.226299	896112.684819	45.664730
3503.502128	896043.025867	45.669735
3503.239164	895996.659800	45.674740
3503.147147	895916.424285	45.679745
3503.393125	895856.050070	45.684749
3503.138033	895811.808376	45.689754
3503.437633	895728.024857	45.694759
3503.449640	895670.878053	45.699764
3503.452092	895601.742216	45.704769
3503.521753	895544.487958	45.709773
3503.309694	895488.633271	45.714778
3503.521523	895417.913590	45.719783
3503.334483	895368.919099	45.724788
3503.419568	895278.492170	45.729793
3503.632675	895234.265584	45.734797
3503.403732	895150.077156	45.739802
3503.426141	895088.281138	45.744807
3503.377569	895021.951071	45.749812
3503.712181	894947.530610	45.754817
3503.399380	894875.053239	45.759821
3503.562202	894758.011009	45.764826
3503.518741	894557.152031	45.769831
3503.078734	894335.944427	45.774836
3503.046634	894027.032952	45.779841
3503.147993	893655.114043	45.784845
3503.105524	893248.854372	45.789850
3503.198750	892767.375749	45.794855
3503.143035	892197.548023	45.799860
3502.886427	891585.412275	45.804865
3502.873599	890906.495087	45.809869
3502.727059	890148.833757	45.814874
3502.829621	889322.207945	45.819879
3502.526067	888448.576266	45.824884
3502.582578	887471.823729	45.829889
3502.395971	886435.385930	45.834893
3502.254302	885329.884756	45.839898
3502.280667	884130.555249	45.844903
3501.774268	882887.265876	45.849908
3501.377379	881536.880068	45.854913
3501.634763	880121.506389	45.859917
3500.818066	878628.582854	45.864922
3501.161106	877041.290333	45.869927
3500.672023	875367.645049	45.874932
3500.573844	873611.450626	45.879937
3500.199324	871792.357876	45.884941
3499.725560	869869.783839	45.889946
3499.642386	867860.552554	45.894951
3499.420742	865795.183606	45.899956
3499.089726	863607.703349	45.904961
3498.693007	861342.714338	45.909965
3498.663422	859004.052225	45.914970
3498.392166	856552.610614	45.919975
3497.908811	854047.164955	45.924980
3497.271044	851444.103072	45.929985
3496.952456	848739.722531	45.934989
3496.509800	845972.775854	45.939994
3496.393099	843100.440146	45.944999
3495.732944	840160.001485	45.950004
3495.077388	837123.459233	45.955009
3494.740452	834006.361300	45.960013
3494.286108	830789.519011	45.965018
3494.126280	827498.247598	45.970023
3493.454941	824138.889742	45.975028
3493.039955	820667.868364	45.980033
3492.403092	817119.523676	45.985037
3491.944403	813470.166296	45.990042
3491.534902	809763.982191	45.995047
3490.429609	805972.081948	46.000052
3489.938379	802082.495500	46.005057
3489.753498	798124.048619	46.010061
3488.703106	794064.019894	46.015066
3488.401449	789935.760560	46.020071
3487.743701	785713.780170	46.025076
3486.760345	781407.775712	46.030081
3486.368324	777006.441125	46.035085
3485.820398	772535.378148	46.040090
3484.940143	767959.807049	46.045095
3484.304879	763311.983366	46.050100
3483.648327	758587.110313	46.055105
3482.730461	753768.075562	46.060109
3482.094477	748859.096802	46.065114
3481.456962	743873.194922	46.070119
3480.670247	738786.580783	46.075124
3479.639404	733637.300673	46.080129
3479.158037	728379.258607	46.085133
3477.724344	723043.876117	46.090138
3477.269302	717639.762676	46.095143
3476.186590	712122.958998	46.100148
3475.597318	706551.887339	46.105153
3474.040455	700849.378564	46.110157
3473.193011	695080.771548	46.115162
3472.370705	689243.220641	46.120167
3471.222394	683323.857343	46.125172
3470.459240	677306.915451	46.130177
3469.522960	671214.556953	46.135181
3468.214039	665033.409252	46.140186
3467.344696	658765.583003	46.145191
3466.270983	652400.844377	46.150196
3465.299157	645965.183685	46.155201
3464.142079	639463.743210	46.160205
3462.758864	632856.328892	46.165210
3462.077448	626153.641369	46.170215
3460.154912	619391.499882	46.175220
3458.891157	612529.087166	46.180225
3458.054909	605603.739889	46.185229
3456.535069	598577.600326	46.190234
3455.248577	591492.240733	46.195239
3454.220465	584308.077135	46.200244
3452.929662	577042.781433	46.205249
3451.543236	569709.226248	46.210253
3449.714048	562271.142052	46.215258
3448.613158	554758.456863	46.220263
3447.149592	547165.792773	46.225268
3445.598280	539504.744104	46.230273
3444.216262	531758.165178	46.235277
3442.832763	523935.515950	46.240282
3441.478085	516006.227934	46.245287
3439.582062	508029.665464	46.250292
3438.158058	499952.613936	46.255297
3436.344936	491800.305989	46.260301
3434.720546	483579.362810	46.265306
3433.066842	475295.238051	46.270311
3431.423307	466932.480915	46.275316
3429.270140	458484.431692	46.280321
3427.408457	449954.301284	46.285325
3425.688990	441359.472891	46.290330
3423.924911	432691.434473	46.295335
3422.214700	423958.832528	46.300340
3419.832714	415162.113495	46.305345
3418.194396	406253.315570	46.310349
3416.254062	397315.365076	46.315354
3414.171946	388276.733232	46.320359
3411.733185	379198.241095	46.325364
3409.450174	370034.613108	46.330369
3407.210502	360838.776523	46.335373
3404.995302	351554.547941	46.340378
3402.824529	342230.593801	46.345383
3400.692921	332829.243713	46.350388
3398.038993	323375.522990	46.355393
3395.457152	313851.644229	46.360397
3392.808997	304289.005782	46.365402
3390.657370	294665.001573	46.370407
3387.947438	284993.453512	46.375412
3385.011055	275252.718288	46.380417
3382.366620	265494.780545	46.385421
3379.075294	255664.372989	46.390426
3376.642123	245812.491693	46.395431
3373.567034	235904.959599	46.400436
3370.282482	225966.371871	46.405441
3367.482655	215912.327854	46.410445
3364.290702	205876.429482	46.415450
3360.947663	195812.002812	46.420455
3357.438797	185736.046792	46.425460
3353.929798	175622.480967	46.430465
3350.297834	165503.185949	46.435469
3345.992801	155344.304035	46.440474
3342.412317	145184.846753	46.445479
3338.283988	135015.688332	46.450484
3333.605860	124853.768097	46.455489
3329.216075	114700.624605	46.460493
3324.223377	104525.761603	46.465498
3319.284184	94406.499515	46.470503
3313.924176	84276.981807	46.475508
3307.563453	74198.966951	46.480513
3300.714046	64174.980749	46.485517
3289.822414	54313.217800	46.490522
3268.464472	44859.295635	46.495527
3241.974319	35750.757804	46.500532
3207.202894	27242.239312	46.505537
3162.966700	19520.858723	46.510541
3114.129349	12675.986698	46.515546
3066.781137	6631.492385	46.520551
3017.070930	1685.922270	46.525556
2875.423467	373.750344	46.530561
2753.531100	363.731363	46.535565
2715.991580	366.978179	46.540570
2744.132203	324.042703	46.545575
2803.227347	328.994789	46.550580
2862.292297	325.905299	46.555585
2903.800506	322.455789	46.560589
2924.842412	334.346285	46.565594
2928.359141	307.565307	46.570599
2921.657741	308.501947	46.575604
2911.296600	316.615450	46.580609
2902.666199	304.919929	46.585613
2896.065953	317.478913	46.590618
2892.094008	311.787273	46.595623
2890.470671	313.354636	46.600628
2889.422564	299.347084	46.605633
2887.757098	290.080595	46.610637
2885.343119	299.823711	46.615642
2883.009678	304.829436	46.620647
2880.308169	300.999456	46.625652
2877.292216	303.885612	46.630657
2874.128565	289.820784	46.635661
2871.453318	301.272605	46.640666
2868.341503	290.650059	46.645671
2865.014620	303.143339	46.650676
2861.898038	301.689448	46.655681
2858.967496	294.779854	46.660685
2855.691329	291.237585	46.665690
2852.237955	294.711906	46.670695
2849.084776	287.000882	46.675700
2846.026963	301.937300	46.680705
2842.635501	294.668351	46.685709
2838.856079	293.937061	46.690714
2836.327615	288.611531	46.695719
2832.794102	287.570386	46.700724
2829.495094	298.695224	46.705729
2826.545505	278.373699	46.710733
2823.083779	304.387867	46.715738
2820.336018	280.193559	46.720743
2816.891538	289.985826	46.725748
2812.881121	287.116090	46.730753
2809.770591	281.343261	46.735757
2805.865360	284.406927	46.740762
2802.806768	284.843820	46.745767
2799.651413	273.545242	46.750772
2796.362095	280.750551	46.755777
2793.168346	260.427595	46.760781
2789.430026	281.834851	46.765786
2786.163223	266.390694	46.770791
2782.605520	269.803909	46.775796
2779.265823	267.439593	46.780801
2775.667725	265.710576	46.785805
2772.286147	281.220459	46.790810
2769.448124	261.169842	46.795815
2765.743476	281.917004	46.800820
2761.937793	268.092770	46.805825
2759.068681	263.572991	46.810829
2755.579703	256.768553	46.815834
2751.860060	266.076142	46.820839
2748.861731	265.275408	46.825844
2745.447803	258.628083	46.830849
2742.243517	268.381450	46.835853
2738.385962	274.635059	46.840858
2734.553816	269.118469	46.845863
2730.852069	273.670706	46.850868
2728.201873	264.300084	46.855873
2725.045638	265.288287	46.860877
2721.442761	257.417090	46.865882
2717.906146	255.200594	46.870887
2713.495826	258.976278	46.875892
2710.344924	243.329490	46.880897
2707.007586	258.447138	46.885901
2703.904267	254.741200	46.890906
2700.686149	254.058802	46.895911
2697.033961	270.821094	46.900916
2693.456318	245.959941	46.905921
2689.449872	254.780246	46.910925
2686.185038	247.220516	46.915930
2683.394629	263.711285	46.920935
2679.373491	250.503501	46.925940
2675.893489	259.880809	46.930945
2672.651742	248.349639	46.935949
2669.114213	247.102168	46.940954
2666.214663	232.421297	46.945959
2662.178072	250.962989	46.950964
2658.690436	246.431104	46.955969
2655.361822	232.745045	46.960973
2652.012868	260.834140	46.965978
2648.636888	235.322429	46.970983
2644.849976	251.825185	46.975988
2641.295740	234.993070	46.980993
2638.549244	249.840175	46.985997
2634.315084	250.749064	46.991002
2631.257138	250.473264	46.996007
2627.496565	235.616726	47.001012
2623.933850	254.584799	47.006017
2621.065532	246.898557	47.011021
2617.466131	234.634334	47.016026
2613.815625	250.201889	47.021031
2609.477915	236.631044	47.026036
2606.416103	238.196516	47.031041
2603.558221	223.774581	47.036045
2599.568058	242.240559	47.041050
2596.404499	230.148350	47.046055
2592.948726	232.753259	47.051060
2589.465156	215.471440	47.056065
2585.852085	231.637344	47.061069
2582.313063	221.315098	47.066074
2579.060066	232.006110	47.071079
2575.643868	223.764773	47.076084
2571.825932	228.023503	47.081089
2568.581932	237.108980	47.086093
2564.609189	240.421238	47.091098
2561.474650	244.496259	47.096103
2558.171085	239.212838	47.101108
2554.626744	234.410585	47.106113
2551.106576	241.228450	47.111117
2547.348604	240.158755	47.116122
2543.838531	233.829467	47.121127
2540.841345	235.689138	47.126132
2537.432751	240.392383	47.131137
2533.605243	241.678888	47.136141
2529.955832	222.525620	47.141146
2526.915480	231.690283	47.146151
2522.838959	232.050587	47.151156
2519.577550	239.686718	47.156161
2516.215946	234.793977	47.161165
2512.553533	225.397235	47.166170
2509.423672	230.332225	47.171175
2505.667878	214.412436	47.176180
2501.837333	227.187402	47.181185
2498.617310	220.877495	47.186189
2495.153780	237.771278	47.191194
2492.348565	220.481728	47.196199
2488.306084	234.404530	47.201204
2484.643854	221.336103	47.206209
2481.278963	221.472732	47.211213
2477.683602	216.107260	47.216218
2474.003120	219.340682	47.221223
2470.506897	224.146593	47.226228
2467.186916	211.629827	47.231233
2464.082461	229.517685	47.236237
2460.619871	217.829521	47.241242
2457.183494	219.423573	47.246247
2453.549834	214.372219	47.251252
2449.757932	223.335786	47.256257
2446.373853	217.762257	47.261261
2442.626290	220.840431	47.266266
2439.447947	222.816234	47.271271
2435.606236	217.762797	47.276276
2432.308423	217.140419	47.281281
2429.267237	199.080417	47.286285
2425.348623	208.479115	47.291290
2421.874107	227.765410	47.296295
2418.281041	212.294636	47.301300
2414.976625	220.110425	47.306305
2411.441040	228.059836	47.311309
2407.562767	218.928416	47.316314
2404.342603	216.890930	47.321319
2401.018014	211.422247	47.326324
2397.437426	219.843330	47.331329
2394.388367	211.976203	47.336333
2390.499325	208.682136	47.341338
2387.038874	213.538804	47.346343
2383.503947	217.072624	47.351348
2380.108893	220.537901	47.356353
2376.783300	209.060508	47.361357
2373.086068	218.950501	47.366362
2369.491004	218.771183	47.371367
2365.459256	222.029242	47.376372
2362.170418	210.721490	47.381377
2359.038914	222.406061	47.386381
2355.734531	211.258815	47.391386
2352.196240	236.567601	47.396391
2348.537803	209.703278	47.401396
2344.756190	226.027657	47.406401
2341.467471	206.507362	47.411405
2337.775223	221.796760	47.416410
2334.550531	213.046902	47.421415
2331.361164	216.758343	47.426420
2327.334514	207.214726	47.431425
2324.027833	200.234673	47.436429
2320.699221	197.753826	47.441434
2317.266573	204.686564	47.446439
2313.125174	211.289216	47.451444
2309.626231	204.578624	47.456449
2306.810104	206.323580	47.461453
2302.905944	208.525982	47.466458
2299.837621	189.839776	47.471463
2296.099348	217.904267	47.476468
2292.513908	216.707400	47.481473
2289.276211	218.886406	47.486477
2285.445411	217.165336	47.491482
2281.892750	213.312634	47.496487
2278.764270	225.756337	47.501492
2275.170447	220.847271	47.506497
2271.625220	224.640317	47.511501
2267.684292	214.465143	47.516506
2264.523977	216.666416	47.521511
2261.080853	206.958727	47.526516
2257.724663	225.537559	47.531521
2254.317070	205.397477	47.536525
2250.705880	213.434683	47.541530
2247.074667	205.140903	47.546535
2243.832339	188.416679	47.551540
2239.886983	212.947356	47.556545
2236.815953	214.092563	47.561549
2232.846786	210.110199	47.566554
2229.454571	206.440594	47.571559
2226.094925	203.037106	47.576564
2222.570421	211.226348	47.581569
2219.558702	206.598246	47.586573
2215.492796	211.554650	47.591578
2211.843627	192.668054	47.596583
2208.227785	196.494866	47.601588
2204.796423	208.400187	47.606593
2201.387095	196.968282	47.611597
2198.366054	212.807863	47.616602
2195.005825	192.284959	47.621607
2191.686563	197.678451	47.626612
2187.743839	199.576227	47.631617
2184.444705	200.595221	47.636621
2180.155347	209.526312	47.641626
2177.043468	188.833426	47.646631
2173.621463	204.294527	47.651636
2169.808243	201.610560	47.656641
2166.583731	204.419687	47.661645
2162.812429	212.248550	47.666650
2159.474175	205.184312	47.671655
2156.384591	212.343062	47.676660
2152.682677	206.059352	47.681665
2149.028022	210.860352	47.686669
2145.657521	210.528680	47.691674
2141.995079	205.055585	47.696679
2138.919671	198.250366	47.701684
2134.794321	212.632459	47.706689
2131.792510	198.175254	47.711693
2128.132834	213.994123	47.716698
2124.426995	212.446571	47.721703
2121.034629	209.730596	47.726708
2117.442047	220.239621	47.731713
2114.350465	197.638286	47.736717
2110.237320	229.647927	47.741722
2107.016553	194.705874	47.746727
2103.443485	208.078246	47.751732
2099.916058	200.915325	47.756737
2096.629799	205.078179	47.761741
2093.116676	202.311999	47.766746
2089.776648	189.644192	47.771751
2086.368412	196.934443	47.776756
2082.510483	205.882111	47.781761
2079.161823	215.193845	47.786765
2075.665957	210.995485	47.791770
2072.296877	197.629692	47.796775
2068.567372	208.160920	47.801780
2065.120440	195.078672	47.806785
2061.592856	196.736972	47.811789
2057.924306	196.763084	47.816794
2054.503112	190.174371	47.821799
2051.163823	209.453525	47.826804
2047.714008	195.088031	47.831809
2044.416777	210.281377	47.836813
2040.419562	197.941797	47.841818
2037.018787	197.358877	47.846823
2033.426277	196.030328	47.851828
2029.527117	202.673947	47.856833
2026.413136	204.155617	47.861837
2022.836950	199.823155	47.866842
2019.994923	203.439731	47.871847
2016.697287	196.067695	47.876852
2012.530301	200.455484	47.881857
2009.363688	186.629086	47.886861
2005.518338	194.981032	47.891866
2002.058495	203.485431	47.896871
1998.471963	197.965762	47.901876
1994.779853	195.458817	47.906881
1991.775117	190.045210	47.911885
1987.738397	197.065002	47.916890
1984.693417	191.810550	47.921895
1981.134334	191.473763	47.926900
1977.722965	204.633149	47.931905
1973.934386	195.555975	47.936909
1970.328197	211.898876	47.941914
1967.083028	196.206076	47.946919
1963.815890	203.725445	47.951924
1960.137102	199.171606	47.956929
1956.656886	204.802560	47.961933
1953.186106	193.207812	47.966938
1949.914890	199.743629	47.971943
1946.133846	191.405104	47.976948
1942.232182	191.538887	47.981953
1939.043075	196.010925	47.986957
1935.472719	206.351400	47.991962
1932.372406	195.944647	47.996967
1928.384643	201.151201	48.001972
1924.785837	199.492972	48.006977
1921.625450	201.922078	48.011981
1917.833159	200.033563	48.016986
1914.350237	200.351609	48.021991
1911.407558	192.759184	48.026996
1907.349876	197.362992	48.032001
1904.237743	183.815627	48.037005
1900.330486	193.685101	48.042010
1897.144579	193.538048	48.047015
1893.840107	182.384095	48.052020
1890.263281	196.763378	48.057025
1886.534320	185.588901	48.062029
1883.062702	208.886620	48.067034
1879.283585	203.523383	48.072039
1875.743631	199.067531	48.077044
1872.226079	203.615094	48.082049
1869.512865	200.362211	48.087053
1865.269055	203.066867	48.092058
1862.011291	192.670544	48.097063
1858.938889	188.739523	48.102068
1855.039520	199.982104	48.107073
1851.351003	199.318404	48.112077
1847.891785	179.887761	48.117082
1844.400129	196.632728	48.122087
1841.171529	197.214760	48.127092
1837.509171	189.242143	48.132097
1834.274292	169.374979	48.137101
1830.455750	189.499841	48.142106
1827.110525	171.589744	48.147111
1823.333206	179.527654	48.152116
1819.876174	187.136405	48.157121
1816.419041	184.565337	48.162125
1812.785756	180.238173	48.167130
1809.515042	193.283838	48.172135
1806.119237	186.325872	48.177140
1802.632648	194.458999	48.182145
1799.183915	176.974302	48.187149
1795.401201	187.811537	48.192154
1791.887435	181.276915	48.197159
1788.599345	192.628682	48.202164
1784.893158	192.301763	48.207169
1781.673376	174.974334	48.212173
1778.024140	186.736684	48.217178
1774.400308	184.870469	48.222183
1771.084615	196.955030	48.227188
1767.389191	187.733191	48.232193
1763.781828	196.187932	48.237197
1760.151266	186.964668	48.242202
1756.882904	181.134673	48.247207
1753.492782	185.279879	48.252212
1749.886816	187.885171	48.257217
1746.547890	176.021689	48.262221
1742.961875	183.055318	48.267226
1739.611756	176.520164	48.272231
1735.822378	185.434069	48.277236
1731.880883	188.201572	48.282241
1729.164379	169.557428	48.287245
1725.423427	189.246809	48.292250
1722.171178	183.868945	48.297255
1718.528690	170.840607	48.302260
1714.778046	185.209456	48.307265
1711.783095	164.462594	48.312269
1707.549776	184.883810	48.317274
1704.529456	170.742845	48.322279
1701.202216	169.602226	48.327284
1697.308473	192.259342	48.332289
1693.962050	171.469460	48.337293
1690.172027	197.756634	48.342298
1687.289624	182.449761	48.347303
1683.615642	192.077320	48.352308
1679.816632	191.889084	48.357313
1676.309503	185.426431	48.362317
1672.879155	188.115636	48.367322
1669.607691	187.536907	48.372327
1666.093541	189.085944	48.377332
1662.476605	190.891168	48.382337
1658.839745	195.686292	48.387341
1655.396078	176.966061	48.392346
1651.511375	199.520890	48.397351
1648.265794	187.670858	48.402356
1644.779910	174.501206	48.407361
1641.300779	181.224941	48.412365
1637.468987	172.235326	48.417370
1634.377918	182.994100	48.422375
1631.239966	163.607292	48.427380
1627.098115	189.798139	48.432385
1623.854127	189.241434	48.437389
1620.267483	192.205348	48.442394
1616.985856	181.582469	48.447399
1613.538238	187.228504	48.452404
1609.584141	180.673132	48.457409
1606.457503	183.804900	48.462413
1602.717287	186.582956	48.467418
1599.396578	186.747522	48.472423
1595.932774	178.636836	48.477428
1592.263708	199.650118	48.482433
1588.952889	169.517279	48.487437
1585.089667	191.458621	48.492442
1581.482889	187.727590	48.497447
1578.277460	179.545273	48.502452
1574.739168	186.702895	48.507457
1571.649021	197.373552	48.512461
1567.786160	186.468891	48.517466
1564.542605	190.426627	48.522471
1561.176642	177.174790	48.527476
1557.397905	182.852804	48.532481
1553.925431	169.222577	48.537485
1550.051232	193.603957	48.542490
1546.648495	176.743690	48.547495
1542.942636	178.583870	48.552500
1539.563421	184.067024	48.557505
1536.540213	163.504184	48.562509
1532.661751	167.013782	48.567514
1529.099718	175.901895	48.572519
1525.771254	188.929654	48.577524
1521.976191	172.501425	48.582529
1518.753529	180.338561	48.587533
1515.365206	177.553963	48.592538
1511.512212	185.194547	48.597543
1508.690178	183.209169	48.602548
1504.900250	181.183372	48.607553
1501.621181	173.719383	48.612557
1497.587552	186.632493	48.617562
1494.363757	182.054832	48.622567
1490.698764	171.427631	48.627572
1487.319078	170.737422	48.632577
1483.674720	178.462061	48.637581
1480.173060	175.015804	48.642586
1476.736576	176.914155	48.647591
1473.009334	165.174123	48.652596
1469.305927	186.211243	48.657601
1466.127137	169.524789	48.662605
1462.755767	180.379205	48.667610
1459.234167	174.885336	48.672615
1456.038077	190.199857	48.677620
1452.296837	184.080204	48.682625
1449.154455	176.861909	48.687629
1445.238835	186.331259	48.692634
1441.520363	170.103433	48.697639
1438.331741	169.058738	48.702644
1434.322629	185.631850	48.707649
1431.062808	161.823317	48.712653
1427.804216	180.872447	48.717658
1424.374696	181.864174	48.722663
1420.692278	175.142843	48.727668
1416.703326	164.059542	48.732673
1413.834413	173.600000	48.737677
1410.123156	165.789916	48.742682
1406.582646	169.199211	48.747687
1403.151980	171.330434	48.752692
1399.373182	167.316072	48.757697
1396.338010	166.958512	48.762701
1392.746794	175.837291	48.767706
1389.487869	173.642433	48.772711
1386.054141	163.670340	48.777716
1382.331977	178.450313	48.782721
1378.757629	172.421443	48.787725
1374.807614	157.430185	48.792730
1371.326249	169.242215	48.797735
1367.754523	160.298342	48.802740
1364.187115	167.227449	48.807745
1361.241870	142.570287	48.812749
1357.344338	168.954556	48.817754
1354.108874	165.684221	48.822759
1350.935723	156.427753	48.827764
1347.411689	162.483865	48.832769
1344.058242	162.622684	48.837773
1340.252064	163.886252	48.842778
1336.398339	165.245368	48.847783
1333.134414	167.020304	48.852788
1329.676743	172.815103	48.857793
1326.092513	156.777212	48.862797
1322.370360	167.617953	48.867802
1319.046384	163.827077	48.872807
1315.478420	166.057160	48.877812
1312.168074	176.185661	48.882817
1308.666290	161.836157	48.887821
1305.053280	163.877764	48.892826
1301.641019	184.850894	48.897831
1297.995555	168.976614	48.902836
1294.355357	173.654963	48.907841
1291.200115	160.760556	48.912845
1287.739631	161.978630	48.917850
1284.338498	169.165126	48.922855
1280.388673	165.811898	48.927860
1276.789598	167.644255	48.932865
1273.843714	152.497386	48.937869
1270.170389	167.702594	48.942874
1266.144430	161.052771	48.947879
1263.365802	171.082071	48.952884
1259.657332	150.039276	48.957889
1256.167088	162.984212	48.962893
1252.210490	154.737862	48.967898
1248.940935	160.119376	48.972903
1245.610643	158.949002	48.977908
1241.803836	165.857802	48.982913
1238.733358	162.911875	48.987917
1234.979805	171.761879	48.992922
1231.347989	158.837075	48.997927
1228.029594	160.416157	49.002932
1224.623103	165.687013	49.007937
1221.105544	158.848332	49.012941
1217.406467	164.172818	49.017946
1214.017996	160.391460	49.022951
1210.730995	160.271668	49.027956
1206.817346	158.800454	49.032961
1203.650370	160.316571	49.037965
1200.027275	150.030689	49.042970
1196.224991	167.968769	49.047975
1192.718276	149.972237	49.052980
1189.111879	163.237744	49.057985
1186.186064	144.336111	49.062989
1182.747664	156.522190	49.067994
1178.911280	144.784111	49.072999
1175.694901	155.051522	49.078004
1171.850450	160.914480	49.083009
1168.528982	143.482834	49.088013
1164.784660	162.296919	49.093018
1161.359334	156.342131	49.098023
1158.287963	159.582154	49.103028
1154.366476	163.201943	49.108033
1150.767457	150.533205	49.113037
1147.442419	166.133460	49.118042
1143.507768	152.819236	49.123047
1140.529421	157.059791	49.128052
1136.586020	154.420106	49.133057
1133.508349	152.730821	49.138061
1130.191257	154.929740	49.143066
1126.753015	165.129629	49.148071
1123.145527	146.596467	49.153076
1119.331905	151.697231	49.158081
1116.229168	136.807698	49.163085
1112.362929	157.761878	49.168090
1108.576323	143.590356	49.173095
1105.167740	157.494239	49.178100
1101.750263	151.437768	49.183105
1098.513396	155.128833	49.188109
1095.271115	170.569447	49.193114
1091.297305	150.310354	49.198119
1087.920246	156.431987	49.203124
1084.055029	160.845128	49.208129
1080.708460	147.511301	49.213133
1077.207797	166.577587	49.218138
1074.094427	153.638523	49.223143
1070.759768	140.071116	49.228148
1066.874130	162.404074	49.233153
1063.638141	145.143844	49.238157
1059.985956	157.850813	49.243162
1056.094218	142.268158	49.248167
1052.669717	151.421606	49.253172
1049.347285	153.384095	49.258177
1045.879542	153.649556	49.263181
1042.338786	151.860783	49.268186
1038.991465	154.686812	49.273191
1035.642650	145.484292	49.278196
1031.903459	160.989104	49.283201
1028.091965	148.949196	49.288205
1024.403862	154.405827	49.293210
1021.086427	150.483717	49.298215
1018.023512	150.607675	49.303220
1014.292179	164.894273	49.308225
1010.764165	150.622408	49.313229
1007.244336	153.631714	49.318234
1003.995142	146.139309	49.323239
1000.616275	154.218462	49.328244
996.753601	161.918687	49.333249
993.785943	170.405047	49.338253
989.397929	157.954085	49.343258
985.936128	160.960825	49.348263
982.955854	165.933833	49.353268
978.765021	168.213362	49.358273
975.772743	151.538079	49.363277
972.296345	153.841406	49.368282
968.607363	161.344968	49.373287
965.895795	155.932891	49.378292
962.171397	150.125066	49.383297
958.528656	144.211428	49.388301
954.562734	157.959094	49.393306
951.081956	141.739065	49.398311
947.712915	153.652951	49.403316
943.807363	140.574089	49.408321
941.083864	140.641841	49.413325
937.505445	142.936085	49.418330
933.609331	154.460634	49.423335
930.179588	148.950432	49.428340
926.466593	150.946888	49.433345
923.070838	161.791413	49.438349
919.451369	144.092679	49.443354
916.172089	155.553462	49.448359
913.263288	147.357472	49.453364
909.256851	161.373170	49.458369
906.059794	152.482450	49.463373
902.204918	136.955681	49.468378
898.696752	153.358955	49.473383
895.258284	142.660131	49.478388
891.467481	147.357915	49.483393
888.363807	137.863850	49.488397
884.419602	156.270962	49.493402
880.960821	150.267605	49.498407
877.489028	155.409217	49.503412
873.750409	166.909472	49.508417
870.708923	150.159420	49.513421
867.309808	171.091809	49.518426
863.714956	160.076408	49.523431
860.489101	165.397108	49.528436
856.962118	150.535656	49.533441
853.298726	150.539552	49.538445
849.875532	149.521446	49.543450
845.786048	151.181380	49.548455
842.665539	151.716328	49.553460
838.949004	151.270294	49.558465
835.773480	148.627795	49.563469
832.580979	161.356907	49.568474
828.766604	144.558037	49.573479
825.331514	147.032969	49.578484
821.177413	157.380193	49.583489
817.795814	138.604381	49.588493
814.390437	139.578708	49.593498
810.947372	147.658871	49.598503
807.797677	147.270869	49.603508
804.226817	142.214053	49.608513
800.955943	145.788441	49.613517
796.926012	145.480896	49.618522
793.358293	153.338289	49.623527
789.986693	144.150236	49.628532
786.636169	147.759191	49.633537
783.385872	144.413474	49.638541
779.637918	156.549810	49.643546
775.823666	141.471881	49.648551
772.601543	154.497504	49.653556
768.802155	146.508052	49.658561
765.663290	161.518347	49.663565
762.009446	149.459397	49.668570
758.661716	161.200363	49.673575
755.452627	150.459401	49.678580
751.703943	158.184030	49.683585
747.886285	148.388302	49.688589
744.322789	152.641700	49.693594
740.642593	147.802147	49.698599
737.633438	148.087227	49.703604
734.085161	159.128365	49.708609
730.754038	143.465995	49.713613
727.128775	152.281225	49.718618
723.496813	145.841635	49.723623
719.993969	139.512520	49.728628
716.671321	147.365083	49.733633
712.885429	149.174424	49.738637
709.418293	143.945754	49.743642
705.844263	136.622393	49.748647
702.563263	141.794030	49.753652
699.150764	144.915976	49.758657
695.399309	143.902448	49.763661
692.182067	139.093797	49.768666
688.436428	147.143981	49.773671
685.283864	141.765514	49.778676
681.381140	149.462739	49.783681
678.012985	136.884050	49.788685
674.693023	147.651038	49.793690
670.916366	154.171097	49.798695
667.800861	148.473111	49.803700
663.713899	143.122316	49.808705
660.144652	147.618097	49.813709
656.876547	144.656564	49.818714
653.241881	133.943053	49.823719
650.011645	148.717404	49.828724
646.503640	136.723734	49.833729
643.122390	142.281983	49.838733
639.740477	135.150469	49.843738
635.738309	127.758085	49.848743
632.623415	143.581447	49.853748
628.931709	136.171228	49.858753
625.711356	139.538772	49.863757
621.980206	139.024051	49.868762
618.473347	148.444115	49.873767
614.746824	138.426568	49.878772
611.399797	145.511380	49.883777
607.624471	149.364795	49.888781
604.168560	134.633553	49.893786
600.700252	150.496069	49.898791
597.602608	133.591927	49.903796
594.155747	147.146782	49.908801
590.775921	139.578828	49.913805
587.204397	145.616788	49.918810
583.509392	144.666310	49.923815
579.879467	145.931074	49.928820
576.360327	152.953676	49.933825
573.007331	147.590912	49.938829
569.199551	134.213555	49.943834
565.603936	161.711824	49.948839
562.548620	131.972831	49.953844
558.776295	145.390572	49.958849
555.299287	147.264891	49.963853
551.715569	135.686472	49.968858
548.237024	150.524859	49.973863
545.134060	129.156240	49.978868
541.179206	154.059229	49.983873
538.226874	134.705272	49.988877
534.559904	144.957474	49.993882
530.733885	160.817457	49.998887
527.357948	146.022637	50.003892
523.885766	154.040953	50.008897
520.383040	143.361762	50.013901
516.606691	154.965863	50.018906
513.403507	149.416900	50.023911
510.149648	157.745020	50.028916
506.032042	145.614983	50.033921
502.734606	141.799353	50.038925
499.210050	140.001498	50.043930
495.736221	149.285550	50.048935
492.631558	142.338666	50.053940
488.958857	135.007177	50.058945
485.237650	158.817349	50.063949
481.827798	138.259143	50.068954
478.423309	144.776514	50.073959
474.879908	127.730253	50.078964
471.342337	142.826708	50.083969
467.974975	142.760018	50.088973
464.134186	146.362513	50.093978
460.502252	145.802592	50.098983
457.175783	126.079018	50.103988
453.802672	152.606647	50.108993
450.244077	130.827322	50.113997
446.601494	147.165454	50.119002
443.001359	156.506109	50.124007
439.756160	138.492188	50.129012
436.129007	165.432823	50.134017
432.871617	139.169717	50.139021
429.431760	148.984435	50.144026
425.812598	146.519015	50.149031
422.458351	151.956800	50.154036
418.690067	152.009242	50.159041
415.289928	146.607500	50.164045
411.965613	146.411602	50.169050
407.967006	151.206710	50.174055
404.583149	134.752065	50.179060
401.059957	149.619387	50.184065
397.855570	138.087706	50.189069
394.627656	139.866701	50.194074
390.495634	131.652402	50.199079
387.266803	145.441314	50.204084
383.445157	135.252112	50.209089
380.136833	151.479712	50.214093
376.585257	131.947960	50.219098
372.953047	147.570396	50.224103
369.576965	149.369443	50.229108
365.981347	154.777584	50.234113
362.837062	137.251433	50.239117
358.980554	147.234845	50.244122
355.589048	154.562396	50.249127
352.024173	148.742511	50.254132
348.321600	152.134116	50.259137
345.498793	150.682182	50.264141
341.753453	156.152655	50.269146
338.445108	144.478372	50.274151
334.663476	134.554172	50.279156
331.077937	150.774416	50.284161
327.712200	135.260495	50.289165
324.376586	149.781382	50.294170
320.904179	140.618759	50.299175
317.363829	144.842108	50.304180
313.267809	149.737214	50.309185
309.860193	132.403372	50.314189
306.558064	144.904050	50.319194
302.721343	153.232369	50.324199
299.715530	148.591720	50.329204
296.258039	145.439713	50.334209
292.959869	146.895062	50.339213
289.334637	144.527696	50.344218
285.643615	152.472974	50.349223
282.304986	146.705325	50.354228
278.578907	154.531413	50.359233
274.980919	158.087586	50.364237
271.727087	147.084612	50.369242
267.739298	155.789293	50.374247
264.614965	138.138871	50.379252
261.041382	137.653077	50.384257
257.726578	139.567732	50.389261
253.966906	142.602739	50.394266
250.106472	144.304504	50.399271
247.001167	136.083142	50.404276
243.556533	132.828424	50.409281
240.232638	141.827579	50.414285
236.270229	122.947819	50.419290
232.838778	148.375645	50.424295
229.905079	125.145333	50.429300
226.083781	151.426660	50.434305
222.760142	138.949032	50.439309
219.468103	136.936044	50.444314
215.636827	133.562629	50.449319
212.404181	133.777255	50.454324
208.144137	146.173747	50.459329
204.959295	140.895380	50.464333
201.724397	132.186438	50.469338
198.132660	133.836733	50.474343
194.840083	127.598977	50.479348
190.883489	142.784703	50.484353
187.382219	129.141245	50.489357
183.731679	139.869823	50.494362
180.031735	143.020482	50.499367
177.184258	142.351821	50.504372
173.712412	133.826467	50.509377
170.037872	136.247381	50.514381
166.544328	135.862945	50.519386
162.965499	138.112383	50.524391
159.465044	139.298474	50.529396
155.843468	142.557435	50.534401
152.407292	144.307333	50.539405
149.065171	139.135582	50.544410
145.471038	136.655244	50.549415
142.147104	131.484342	50.554420
138.384452	136.486145	50.559425
135.134248	128.572998	50.564429
131.249789	135.395345	50.569434
127.770315	136.807144	50.574439
124.264554	130.975076	50.579444
120.871568	141.976995	50.584449
117.381183	129.216358	50.589453
114.028878	122.604783	50.594458
110.508145	130.452254	50.599463
107.246104	135.364345	50.604468
103.539380	136.748405	50.609473
100.044649	136.547982	50.614477
96.424202	133.771741	50.619482
92.666280	139.051367	50.624487
89.798015	143.789295	50.629492
86.066656	144.220754	50.634497
82.470623	130.326877	50.639501
79.136473	135.624574	50.644506
75.435341	136.498114	50.649511
71.897442	143.583337	50.654516
68.118949	133.527605	50.659521
64.678386	140.768589	50.664525
61.503939	135.154469	50.669530
57.958241	141.066689	50.674535
54.631431	124.141011	50.679540
50.868620	136.468136	50.684545
47.281018	128.676005	50.689549
43.992417	134.742643	50.694554
40.385698	139.830992	50.699559
37.032643	121.952787	50.704564
33.334745	138.818113	50.709569
29.480112	133.699662	50.714573
26.349171	135.092785	50.719578
22.815780	127.145221	50.724583
19.563055	130.718748	50.729588
15.949301	134.145867	50.734593
12.070472	127.929243	50.739597
8.621649	135.499520	50.744602
5.097342	147.591839	50.749607
2.171506	132.643600	50.754612