Wed Jun 15 15:59:09 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.360091	87.179639	0.000000
1.340897	104.895570	0.005005
1.388088	89.131769	0.010010
1.491931	103.520225	0.015014
1.034816	86.895226	0.020019
1.140076	90.189603	0.025024
0.716293	85.691199	0.030029
0.919829	56.711221	0.035034
0.142413	61.436539	0.040038
-0.035548	48.747793	0.045043
-0.098543	46.557394	0.050048
-0.502057	43.306591	0.055053
-0.666426	30.474574	0.060058
-1.005267	41.071159	0.065062
-1.071518	30.393647	0.070067
-1.623862	31.213827	0.075072
-1.750525	12.697004	0.080077
-1.878203	2.109666	0.085082
-2.299134	-1.904041	0.090086
-2.771994	0.869913	0.095091
-2.563039	-3.735402	0.100096
-3.450290	-10.224218	0.105101
-3.469465	-0.524214	0.110106
-3.842054	-9.399703	0.115110
-3.874416	-9.115089	0.120115
-4.439151	-13.790323	0.125120
-5.400475	-13.154891	0.130125
-5.525533	-8.215720	0.135130
-5.683108	-20.150838	0.140134
-5.637697	-11.174925	0.145139
-5.409999	-21.816933	0.150144
-5.868104	2.070120	0.155149
-5.648280	-22.204499	0.160154
-6.089861	-2.904964	0.165158
-6.682325	-7.411173	0.170163
-7.185766	-7.488175	0.175168
-7.268924	-9.159313	0.180173
-7.305165	-14.499166	0.185178
-7.648048	-0.953306	0.190182
-7.649751	-11.335653	0.195187
-8.240904	-10.150973	0.200192
-8.651157	-11.789262	0.205197
-8.626156	-22.692033	0.210202
-8.871492	-9.325759	0.215206
-9.109527	-27.791079	0.220211
-9.206632	-16.316483	0.225216
-10.134344	-12.888405	0.230221
-10.012983	-14.190076	0.235226
-10.454950	-23.363939	0.240230
-10.272246	-12.810181	0.245235
-10.066104	-17.640236	0.250240
-11.178113	-0.797366	0.255245
-11.454027	-11.068104	0.260250
-11.745760	-4.719155	0.265254
-11.741238	-6.319750	0.270259
-11.884766	-14.607279	0.275264
-11.929612	-13.617156	0.280269
-12.092215	0.607980	0.285274
-12.596334	-7.684177	0.290278
-13.142851	-3.492439	0.295283
-13.256183	-12.797959	0.300288
-13.892325	3.224253	0.305293
-13.622839	-10.045112	0.310298
-13.658658	-2.282535	0.315302
-13.411347	-11.985521	0.320307
-14.253435	-10.454651	0.325312
-15.128803	-10.571495	0.330317
-14.988868	-21.489512	0.335322
-15.423210	-15.358879	0.340326
-15.517271	-13.922336	0.345331
-15.526971	-5.157786	0.350336
-16.421211	0.005280	0.355341
-16.547345	-5.874802	0.360346
-16.561808	-3.312344	0.365350
-16.832271	-0.102185	0.370355
-16.702772	-10.546560	0.375360
-17.268469	-3.474534	0.380365
-17.029268	-12.398748	0.385370
-17.720745	-12.515895	0.390374
-18.341737	-6.003921	0.395379
-18.536002	-9.613938	0.400384
-18.579267	2.722129	0.405389
-18.554090	-11.644546	0.410394
-18.785257	-6.306768	0.415398
-18.942325	-2.694820	0.420403
-19.563260	10.765605	0.425408
-20.316163	-7.768336	0.430413
-20.082716	-9.258697	0.435418
-20.162643	-3.355712	0.440422
-20.202135	0.708532	0.445427
-20.190705	-3.372682	0.450432
-20.591993	-11.838678	0.455437
-21.272701	-9.720505	0.460442
-21.491284	-7.470463	0.465446
-21.659127	-4.780755	0.470451
-21.817773	-18.583267	0.475456
-23.059131	6.502562	0.480461
-22.384208	-17.895511	0.485466
-22.799269	-7.083153	0.490470
-23.090405	-5.441704	0.495475
-22.999782	-15.775085	0.500480
-23.491833	-0.449065	0.505485
-23.299084	-17.916459	0.510490
-24.223945	-4.633000	0.515494
-24.731938	-29.042615	0.520499
-24.603000	-17.241080	0.525504
-25.157408	-20.842573	0.530509
-25.036225	-19.336151	0.535514
-24.905409	-6.544904	0.540518
-25.054194	-21.545229	0.545523
-25.073075	-25.066246	0.550528
-26.251453	-12.624864	0.555533
-26.701284	-14.929871	0.560538
-26.758664	-24.653320	0.565542
-26.786404	-15.710305	0.570547
-26.683339	-13.269766	0.575552
-26.976272	-27.745729	0.580557
-27.030657	-12.616348	0.585562
-27.626553	-12.448420	0.590566
-28.039151	-9.501240	0.595571
-28.021624	-25.057298	0.600576
-28.921843	-11.691602	0.605581
-28.941906	-18.533451	0.610586
-29.155657	-19.436154	0.615590
-29.687536	-14.660188	0.620595
-29.692667	-18.886531	0.625600
-30.056211	-19.015358	0.630605
-29.717665	-20.349668	0.635610
-29.704808	-17.328288	0.640614
-30.098025	-17.223647	0.645619
-30.444445	-12.944633	0.650624
-31.531987	-11.885958	0.655629
-30.999146	-15.296627	0.660634
-31.530942	-24.374453	0.665638
-31.641472	-4.999523	0.670643
-31.997443	-25.860900	0.675648
-32.822545	-11.269314	0.680653
-32.975852	-30.268296	0.685658
-33.063944	-19.012019	0.690662
-33.025264	-15.503747	0.695667
-33.052692	-8.629785	0.700672
-33.178617	-12.890225	0.705677
-33.314549	-26.586491	0.710682
-34.029940	-17.523812	0.715686
-34.578391	-30.103189	0.720691
-34.539253	-25.691890	0.725696
-34.664486	-14.706372	0.730701
-34.523245	-11.972849	0.735706
-34.672586	0.079972	0.740710
-35.612154	-21.122752	0.745715
-35.755667	2.226372	0.750720
-35.991944	-20.438122	0.755725
-35.938997	-11.073213	0.760730
-36.724315	-10.729461	0.765734
-37.396791	-8.206026	0.770739
-37.548156	-14.167854	0.775744
-37.419310	-5.117046	0.780749
-37.493485	-26.124627	0.785754
-37.454182	-4.074909	0.790758
-37.745846	-18.525934	0.795763
-37.456767	-13.617824	0.800768
-38.495148	-0.723404	0.805773
-38.757692	-8.819816	0.810778
-38.982129	-11.400698	0.815782
-38.898564	-9.454311	0.820787
-39.569235	-21.474098	0.825792
-40.666861	-2.489926	0.830797
-40.102533	-14.997535	0.835802
-39.972540	-12.799579	0.840806
-40.454701	-11.744479	0.845811
-40.219651	-20.496553	0.850816
-40.660834	-2.304886	0.855821
-41.266480	-23.708591	0.860826
-41.740210	-3.158044	0.865830
-42.305218	-17.445419	0.870835
-41.796438	-20.549463	0.875840
-42.226702	-19.214697	0.880845
-42.227234	-1.339018	0.885850
-42.910998	-6.597010	0.890854
-43.675598	-9.802620	0.895859
-43.783847	-1.220753	0.900864
-44.021903	-6.795767	0.905869
-44.164499	-14.534480	0.910874
-43.782527	-6.956964	0.915878
-43.878320	-24.596246	0.920883
-43.505471	-15.653641	0.925888
-44.334337	-25.941980	0.930893
-44.834399	-19.147055	0.935898
-45.322319	-3.595723	0.940902
-45.480905	-16.493558	0.945907
-45.963469	-14.165165	0.950912
-46.249042	-1.087486	0.955917
-46.520458	-21.277051	0.960922
-46.689889	-6.240714	0.965926
-46.821701	-18.176239	0.970931
-46.683284	1.917129	0.975936
-47.008775	-13.644788	0.980941
-47.369385	-6.660716	0.985946
-47.731941	-12.380187	0.990950
-48.107175	-4.958766	0.995955
-48.266792	-21.400491	1.000960
-48.407822	-13.297467	1.005965
-48.510328	-25.231812	1.010970
-49.158012	-19.632446	1.015974
-49.852051	-10.238091	1.020979
-49.921262	-8.730486	1.025984
-50.328018	-7.524391	1.030989
-50.195097	-18.399126	1.035994
-50.119294	-4.700714	1.040998
-49.982754	-13.073295	1.046003
-50.041848	-15.075322	1.051008
-51.315062	-6.256037	1.056013
-51.459139	-18.448381	1.061018
-51.564043	-9.816861	1.066022
-51.666383	-20.721271	1.071027
-51.606016	-8.551596	1.076032
-52.772845	-14.606119	1.081037
-52.962695	-9.828971	1.086042
-53.382892	-15.718745	1.091046
-53.441561	-14.849941	1.096051
-53.515979	-7.687467	1.101056
-53.885459	-9.603177	1.106061
-53.453834	-12.128933	1.111066
-53.690040	-16.013649	1.116070
-53.923272	1.788724	1.121075
-54.039620	-24.303515	1.126080
-54.786154	5.886360	1.131085
-55.150630	-9.996621	1.136090
-55.570133	0.640096	1.141094
-55.516399	-0.141583	1.146099
-55.384298	-10.097987	1.151104
-56.644112	3.713255	1.156109
-56.818502	-22.594505	1.161114
-56.937645	-4.201658	1.166118
-57.310583	-13.643308	1.171123
-56.749853	-25.893635	1.176128
-57.189587	-6.957238	1.181133
-57.174277	-18.516178	1.186138
-57.435180	-8.930023	1.191142
-57.899588	-17.768227	1.196147
-58.190755	-19.501558	1.201152
-58.333194	-11.486589	1.206157
-58.590498	-18.530317	1.211162
-59.379841	-9.052243	1.216166
-59.876286	-16.934991	1.221171
-59.533301	-16.780380	1.226176
-59.846578	-31.643511	1.231181
-59.942970	-20.569348	1.236186
-60.136584	-33.715193	1.241190
-60.432855	-16.848440	1.246195
-60.421233	-28.889241	1.251200
-61.095869	-12.728304	1.256205
-60.983262	-14.875012	1.261210
-61.265713	-12.557102	1.266214
-62.283559	-11.070867	1.271219
-62.544640	-19.089384	1.276224
-63.076922	-27.277333	1.281229
-62.379426	-17.120884	1.286234
-62.845542	-27.502415	1.291238
-63.127903	-10.625032	1.296243
-62.765141	-33.737318	1.301248
-63.334954	-14.445022	1.306253
-63.730242	-24.816164	1.311258
-64.396563	-14.846551	1.316262
-64.769222	-17.018706	1.321267
-64.849295	-18.208662	1.326272
-64.691711	-17.918449	1.331277
-64.427512	-10.837196	1.336282
-64.823896	-22.099328	1.341286
-65.484210	-3.336786	1.346291
-65.959425	-8.224002	1.351296
-66.445307	-1.736031	1.356301
-66.105826	-5.556582	1.361306
-66.593033	-7.920417	1.366310
-67.103993	-7.831629	1.371315
-67.148115	-23.246491	1.376320
-67.737722	-12.269257	1.381325
-68.207438	-6.952130	1.386330
-67.852888	-12.848122	1.391334
-67.952627	-0.209060	1.396339
-67.936108	-7.212522	1.401344
-68.215279	-23.261994	1.406349
-68.622732	-13.586021	1.411354
-69.179282	-9.250179	1.416358
-69.609502	-11.067954	1.421363
-69.711883	-17.102586	1.426368
-69.728481	-23.434705	1.431373
-69.849119	-10.430660	1.436378
-70.349175	-26.208547	1.441382
-70.871600	-7.452030	1.446387
-71.154403	-33.321714	1.451392
-71.602205	-5.299267	1.456397
-71.373427	-17.708009	1.461402
-71.344323	-16.312243	1.466406
-71.500507	-14.285591	1.471411
-71.874014	-33.994030	1.476416
-72.756726	-15.819965	1.481421
-72.829373	-26.020108	1.486426
-72.894789	-19.069047	1.491430
-73.092469	-28.904938	1.496435
-73.044918	-21.603712	1.501440
-73.261073	-21.332520	1.506445
-74.139105	-9.599927	1.511450
-74.604070	-19.119287	1.516454
-74.658540	-1.604820	1.521459
-74.592922	-25.191818	1.526464
-74.796925	0.107563	1.531469
-74.718734	-18.256623	1.536474
-74.839110	-29.278785	1.541478
-75.655925	-16.387062	1.546483
-76.136838	-28.246528	1.551488
-76.463591	-20.088153	1.556493
-76.647663	-26.900421	1.561498
-76.896022	-20.304930	1.566502
-76.847559	-19.178017	1.571507
-76.411123	-37.387031	1.576512
-77.166410	-25.726625	1.581517
-77.903882	-27.639020	1.586522
-78.044412	-25.365973	1.591526
-78.257790	-18.434158	1.596531
-77.891085	-31.279900	1.601536
-78.149894	-21.944464	1.606541
-78.897200	-30.347925	1.611546
-79.419113	-20.313697	1.616550
-79.670080	-29.561529	1.621555
-79.561404	-18.744694	1.626560
-79.628714	-14.031206	1.631565
-79.547863	-18.862253	1.636570
-80.653189	-21.674270	1.641574
-80.884939	-12.450726	1.646579
-81.233952	-31.870333	1.651584
-81.290096	-24.910944	1.656589
-81.205390	-24.406856	1.661594
-81.291984	-33.589422	1.666598
-81.749015	-17.733662	1.671603
-82.265683	-17.228531	1.676608
-82.798185	-9.017598	1.681613
-83.278050	-21.474741	1.686618
-83.330619	-11.308259	1.691622
-83.555513	-4.801772	1.696627
-83.184823	-16.677209	1.701632
-83.359423	-1.101607	1.706637
-83.289513	-13.311562	1.711642
-83.515743	-11.806515	1.716646
-84.658465	-18.278438	1.721651
-84.267173	-25.603272	1.726656
-84.745194	-5.397780	1.731661
-85.293699	-26.582249	1.736666
-86.027276	-19.650477	1.741670
-85.838284	-13.324757	1.746675
-85.563607	-36.860465	1.751680
-85.990322	-19.335004	1.756685
-86.230768	-22.793159	1.761690
-86.295485	-15.616511	1.766694
-87.087963	-4.066740	1.771699
-87.025674	-18.783018	1.776704
-87.661329	-6.912130	1.781709
-87.547539	-2.894827	1.786714
-87.799839	-17.768833	1.791718
-87.933111	-9.874644	1.796723
-88.273705	-9.772778	1.801728
-89.079938	-11.220234	1.806733
-89.182802	-17.460067	1.811738
-89.318127	-23.379851	1.816742
-89.725746	-20.721443	1.821747
-89.503731	-22.280743	1.826752
-89.495043	-19.017881	1.831757
-89.418345	-12.773333	1.836762
-90.312279	-14.822043	1.841766
-90.759638	-13.583686	1.846771
-90.975617	-19.611278	1.851776
-91.369763	-12.132284	1.856781
-91.264310	-14.647634	1.861786
-91.331788	-20.849515	1.866790
-92.265547	-15.235811	1.871795
-92.391811	-25.299639	1.876800
-92.481939	-13.469006	1.881805
-92.584476	-23.396680	1.886810
-92.275708	-13.654518	1.891814
-93.090339	-19.911065	1.896819
-93.700100	-20.414790	1.901824
-94.082096	-15.366867	1.906829
-94.041613	-26.107643	1.911834
-94.051146	-16.633573	1.916838
-94.342675	-11.016813	1.921843
-94.099498	-22.933021	1.926848
-94.950761	-5.288743	1.931853
-95.342814	-18.530530	1.936858
-95.557094	-16.584142	1.941862
-96.073526	-15.414667	1.946867
-95.806985	-8.764789	1.951872
-96.284805	-11.488158	1.956877
-96.191044	-14.176476	1.961882
-96.227786	-16.168484	1.966886
-97.048502	-9.344921	1.971891
-97.119533	-20.060068	1.976896
-97.644154	-6.794229	1.981901
-97.602256	-5.309822	1.986906
-97.438069	-22.095173	1.991910
-98.113873	-15.118100	1.996915
-98.770162	-15.058610	2.006912
-97.838030	-17.652261	2.016909
-97.730421	-24.711441	2.026906
-97.555825	-17.834826	2.036902
-96.479440	-20.271762	2.046899
-96.316259	-23.276925	2.056896
-95.794019	-21.291890	2.066893
-94.972501	-17.740204	2.076890
-94.515585	-20.054703	2.086886
-94.283517	-28.626904	2.096883
-93.445673	-22.301721	2.106880
-93.370829	-19.683095	2.116877
-92.434603	-11.487712	2.126874
-91.899840	-8.314140	2.136870
-91.725920	-14.154074	2.146867
-91.638146	-16.736474	2.156864
-90.468282	-14.936803	2.166861
-90.154895	-25.520911	2.176858
-89.079188	-13.428797	2.186854
-89.068928	-19.755592	2.196851
-88.797135	-19.755874	2.206848
-88.495647	-22.218029	2.216845
-87.475978	-11.863147	2.226842
-87.250962	-16.450397	2.236838
-86.592828	-23.662005	2.246835
-86.048118	-20.821560	2.256832
-85.741915	-24.985257	2.266829
-85.129253	-19.251836	2.276826
-84.330524	-15.629512	2.286822
-84.411487	-20.605530	2.296819
-83.503946	-23.873680	2.306816
-82.940773	-18.613792	2.316813
-82.953867	-11.940736	2.326810
-81.972557	-13.766556	2.336806
-81.123510	-19.846081	2.346803
-81.158113	-22.155792	2.356800
-80.837479	-13.633067	2.366797
-80.043235	-11.500082	2.376794
-80.172311	-17.130715	2.386790
-78.943719	-19.770497	2.396787
-78.373356	-15.466827	2.406784
-78.162724	-24.787246	2.416781
-77.124813	-10.635697	2.426778
-76.629450	-9.731133	2.436774
-76.374642	-15.306292	2.446771
-76.373401	-9.247006	2.456768
-76.115568	-17.486560	2.466765
-75.314317	-8.668227	2.476762
-74.240230	2.503414	2.486758
-73.796038	-9.228827	2.496755
-73.490218	-8.621849	2.506752
-73.230261	-6.322329	2.516749
-72.593638	-0.367262	2.526746
-71.720097	-0.317062	2.536742
-71.972253	7.515497	2.546739
-71.026981	13.057951	2.556736
-70.146044	-1.921528	2.566733
-70.132533	3.136355	2.576730
-70.131898	2.438317	2.586726
-68.824417	-0.332637	2.596723
-68.507303	-3.711913	2.606720
-68.218226	-7.145225	2.616717
-67.282523	-6.260891	2.626714
-67.206955	-13.357453	2.636710
-66.735432	-1.553543	2.646707
-65.733150	-3.991070	2.656704
-65.480701	-11.085655	2.666701
-65.453622	-14.431611	2.676698
-64.294093	-13.971162	2.686694
-64.111727	-7.302455	2.696691
-63.696308	-14.099506	2.706688
-62.791154	-4.309430	2.716685
-62.386880	-11.486099	2.726682
-62.351764	-11.658439	2.736678
-61.499790	-6.035184	2.746675
-60.669152	-10.614375	2.756672
-60.773253	-9.653897	2.766669
-60.100903	-6.907930	2.776666
-59.446470	-6.436203	2.786662
-59.348821	0.030395	2.796659
-58.449477	-12.686369	2.806656
-57.661752	-8.513144	2.816653
-57.614361	-9.691240	2.826650
-57.115072	-11.770156	2.836646
-56.359313	-6.809269	2.846643
-56.051205	-15.379331	2.856640
-55.929437	-14.429910	2.866637
-54.924483	-7.386796	2.876634
-54.822266	-7.199237	2.886630
-53.483450	-7.055351	2.896627
-53.359702	-19.337730	2.906624
-53.169887	-11.144515	2.916621
-52.469408	-1.079701	2.926618
-51.806021	-5.173340	2.936614
-51.315538	2.275916	2.946611
-51.467277	-5.832739	2.956608
-50.261506	-5.566215	2.966605
-49.906431	1.715383	2.976602
-49.958041	-0.743927	2.986598
-49.028884	-10.579484	2.996595
-48.151603	-6.096788	3.006592
-47.980877	-2.554972	3.016589
-47.644412	2.865468	3.026586
-47.114839	-2.834620	3.036582
-46.724938	-2.251413	3.046579
-45.731047	-5.231985	3.056576
-44.912051	0.266642	3.066573
-44.907595	-0.463832	3.076570
-44.829431	-11.480420	3.086566
-44.365087	-7.894582	3.096563
-43.305189	-2.754015	3.106560
-43.044397	-11.564474	3.116557
-42.249249	-12.453481	3.126554
-41.783263	-3.669217	3.136550
-41.738863	2.250193	3.146547
-41.328059	-0.352509	3.156544
-40.325719	1.825603	3.166541
-40.047351	1.256293	3.176538
-39.005120	10.174383	3.186534
-38.824714	7.060779	3.196531
-38.499920	2.682925	3.206528
-38.047220	2.826092	3.216525
-37.789326	1.296343	3.226522
-36.850601	-2.464206	3.236518
-36.744853	2.624858	3.246515
-35.359392	-1.797221	3.256512
-34.911781	6.069724	3.266509
-35.386874	-1.854127	3.276506
-34.789447	-9.546904	3.286502
-33.756032	-8.013283	3.296499
-33.395347	-20.055197	3.306496
-33.218610	-5.125700	3.316493
-32.609954	-0.074416	3.326490
-32.121316	-1.578888	3.336486
-31.272856	-4.796578	3.346483
-30.420011	3.580818	3.356480
-30.129341	-5.048003	3.366477
-30.324508	-6.243892	3.376474
-29.952043	-5.735537	3.386470
-29.024324	-6.511134	3.396467
-28.430898	-10.348351	3.406464
-27.537920	0.581313	3.416461
-27.013411	-9.508576	3.426458
-27.229440	-8.532070	3.436454
-27.022222	3.086973	3.446451
-25.665625	-12.823022	3.456448
-25.466964	-1.350529	3.466445
-25.003997	-13.832890	3.476442
-24.141551	-12.915897	3.486438
-23.848377	-15.406112	3.496435
-23.872292	-15.056560	3.506432
-22.717938	-15.923443	3.516429
-22.126416	-5.966949	3.526426
-22.397397	-17.705937	3.536422
-21.407139	-13.369820	3.546419
-20.930102	-21.240733	3.556416
-20.416383	-20.710979	3.566413
-19.508291	-10.224739	3.576410
-18.932326	-10.908717	3.586406
-18.810601	-9.216024	3.596403
-18.886715	-1.754709	3.606400
-18.143097	-5.652504	3.616397
-17.109285	-13.205236	3.626394
-17.050307	-10.170916	3.636390
-16.685492	-6.024883	3.646387
-15.619571	-8.148255	3.656384
-15.770591	-5.880966	3.666381
-14.355533	-13.622146	3.676378
-14.042176	-13.398166	3.686374
-13.992977	-15.059558	3.696371
-13.997968	-6.274595	3.706368
-12.847474	-2.792076	3.716365
-12.130485	1.386331	3.726362
-12.194757	1.137472	3.736358
-11.380260	-8.376990	3.746355
-11.043623	-14.623500	3.756352
-10.485256	-8.435625	3.766349
-9.713529	-9.759901	3.776346
-9.172386	-9.139955	3.786342
-9.215229	-5.068583	3.796339
-8.360291	-8.651120	3.806336
-7.751848	-12.419701	3.816333
-7.593048	-17.621437	3.826330
-6.571467	-16.142354	3.836326
-6.169041	-5.923872	3.846323
-6.188607	-20.485652	3.856320
-5.699541	-6.849538	3.866317
-4.966531	-6.104844	3.876314
-4.733075	8.672670	3.886310
-4.118858	17.931060	3.896307
-3.455244	21.773480	3.906304
-2.851108	30.315664	3.916301
-3.034382	27.687179	3.926298
-2.358551	58.136035	3.936294
-1.755124	57.840535	3.946291
-1.244870	76.505761	3.956288
-0.719303	91.168062	3.966285
-0.380085	102.797570	3.976282
0.000000	129.509919	3.981286
0.337238	108.196511	3.986291
0.278698	132.486801	3.991296
0.289517	136.043711	3.996301
0.797556	160.771625	4.001306
0.565099	149.493903	4.006310
0.864603	157.875696	4.011315
1.085733	154.959138	4.016320
0.986813	163.104622	4.021325
1.219244	156.485833	4.026330
0.987499	177.678289	4.031334
1.133816	151.995214	4.036339
0.985241	167.316035	4.041344
1.101110	157.411424	4.046349
1.604177	162.516249	4.051354
0.581768	145.747165	4.056358
1.018119	151.922780	4.061363
0.795273	161.550600	4.066368
0.814266	146.011779	4.071373
1.024457	162.543683	4.076378
0.991424	156.814767	4.081382
1.289643	153.084649	4.086387
0.985742	153.236873	4.091392
1.217656	165.295281	4.096397
1.486523	145.648622	4.101402
1.013300	158.547631	4.106406
1.257403	144.787609	4.111411
1.012402	145.804706	4.116416
0.955022	169.615832	4.121421
1.328413	147.209102	4.126426
1.033679	159.993284	4.131430
1.214258	147.582207	4.136435
1.154354	153.169133	4.141440
0.997463	166.711827	4.146445
1.186165	155.092428	4.151450
0.854192	156.559525	4.156454
1.033705	163.656441	4.161459
1.016768	159.740864	4.166464
1.052021	170.690723	4.171469
1.087646	164.779697	4.176474
0.947492	173.412908	4.181478
1.159795	165.337557	4.186483
1.235076	172.515232	4.191488
1.069887	171.789553	4.196493
1.288809	173.496374	4.201498
1.199538	176.607671	4.206502
1.439103	183.464625	4.211507
1.770616	191.598375	4.216512
1.460510	179.423636	4.221517
1.077938	162.655330	4.226522
0.934076	186.172106	4.231526
1.680162	178.384182	4.236531
1.458987	188.033346	4.241536
1.793086	191.610926	4.246541
1.489449	182.096728	4.251546
1.274066	186.805651	4.256550
1.840518	163.295383	4.261555
1.483667	169.222597	4.266560
1.271521	169.987055	4.271565
1.351592	165.752498	4.276570
1.582090	186.027209	4.281574
1.729823	176.093053	4.286579
1.851017	181.126341	4.291584
1.374213	181.876237	4.296589
1.757370	182.378656	4.301594
1.295194	182.054625	4.306598
1.467944	177.990501	4.311603
1.604190	185.140547	4.316608
1.624055	192.885341	4.321613
1.981376	198.982787	4.326618
1.781622	198.863979	4.331622
2.021303	178.703708	4.336627
1.532545	172.643080	4.341632
1.358863	150.274969	4.346637
1.417036	166.438496	4.351642
1.851365	162.580823	4.356646
2.056623	181.796478	4.361651
1.864816	186.250842	4.366656
1.870528	183.486185	4.371661
1.526587	161.546310	4.376666
1.530164	188.216650	4.381670
1.825960	176.657072	4.386675
1.879170	178.293224	4.391680
1.858350	190.805077	4.396685
2.062343	174.872235	4.401690
1.469555	187.436193	4.406694
1.592935	181.487969	4.411699
1.499654	187.480045	4.416704
1.399430	193.767536	4.421709
1.963755	173.158931	4.426714
1.790383	196.335038	4.431718
1.636025	183.670616	4.436723
1.654035	187.834412	4.441728
1.879008	176.539867	4.446733
2.053012	188.790954	4.451738
1.841252	183.536761	4.456742
1.789368	199.977462	4.461747
2.206542	199.745254	4.466752
2.029184	219.373599	4.471757
2.049453	195.510717	4.476762
1.765531	201.178384	4.481766
2.283843	207.472073	4.486771
2.310897	213.909988	4.491776
2.044374	204.716264	4.496781
2.257898	195.432459	4.501786
1.794385	199.687280	4.506790
2.212724	195.773744	4.511795
2.113803	202.641861	4.516800
2.451078	204.924464	4.521805
2.225110	192.118670	4.526810
1.898314	200.118645	4.531814
1.934116	190.424837	4.536819
1.914178	204.156530	4.541824
2.340328	205.343365	4.546829
2.604693	226.709397	4.551834
2.214616	208.525895	4.556838
2.018192	212.947489	4.561843
2.121297	209.281763	4.566848
2.220471	224.991603	4.571853
2.517310	206.421622	4.576858
2.285979	225.067780	4.581862
2.651621	194.594549	4.586867
2.321373	205.906699	4.591872
1.982393	185.394882	4.596877
2.543570	209.501197	4.601882
2.521341	191.554739	4.606886
2.347510	189.862262	4.611891
1.969916	187.276567	4.616896
2.362217	215.465315	4.621901
2.856891	204.214171	4.626906
2.360699	210.372082	4.631910
2.130094	197.882130	4.636915
2.249007	216.916185	4.641920
2.875130	212.279349	4.646925
2.937102	208.309286	4.651930
2.253124	193.518827	4.656934
2.349006	181.625315	4.661939
2.210165	212.231794	4.666944
2.286141	213.244975	4.671949
2.956015	213.573446	4.676954
2.507627	214.401512	4.681958
2.550734	222.718385	4.686963
2.948669	213.933337	4.691968
2.448108	206.259881	4.696973
2.373301	202.474109	4.701978
2.287240	231.715991	4.706982
2.441526	211.853994	4.711987
2.541428	217.194647	4.716992
2.488060	214.156827	4.721997
2.709235	216.925716	4.727002
2.827808	208.996344	4.732006
2.487335	219.502762	4.737011
2.469683	193.983737	4.742016
2.828627	209.766246	4.747021
2.826205	212.614802	4.752026
2.521111	226.713458	4.757030
3.000417	222.453745	4.762035
2.715400	215.718120	4.767040
2.823832	224.110909	4.772045
2.952574	203.331182	4.777050
2.785618	226.688378	4.782054
3.072323	212.609922	4.787059
2.713955	229.460187	4.792064
2.943545	208.616237	4.797069
3.026324	220.409706	4.802074
2.832493	216.427858	4.807078
2.829460	213.810935	4.812083
2.782827	236.995555	4.817088
2.596219	213.760399	4.822093
3.073168	217.864634	4.827098
2.543415	225.023750	4.832102
2.944067	210.524771	4.837107
2.875682	226.085330	4.842112
2.855762	219.020504	4.847117
3.036094	214.653847	4.852122
2.818880	225.650697	4.857126
2.944866	223.104194	4.862131
2.924622	218.766343	4.867136
2.957983	221.080333	4.872141
3.075394	213.633440	4.877146
2.857906	225.683894	4.882150
2.894288	221.182300	4.887155
3.017529	221.838457	4.892160
2.604056	214.498832	4.897165
3.091105	221.831621	4.902170
3.150302	225.260699	4.907174
3.036094	214.391419	4.912179
3.011325	229.371136	4.917184
3.363517	241.965016	4.922189
3.432779	231.422706	4.927194
3.351580	229.652372	4.932198
3.321502	206.663231	4.937203
3.103257	213.789406	4.942208
3.086948	234.803200	4.947213
3.358313	216.487685	4.952218
3.247977	230.106099	4.957222
3.005419	215.595432	4.962227
3.120744	231.759251	4.967232
3.020172	215.245848	4.972237
3.355687	236.173385	4.977242
3.574164	243.991033	4.982246
3.750656	233.301376	4.987251
3.654509	216.794343	4.992256
3.088824	228.866239	4.997261
3.354709	207.668756	5.002266
3.089610	225.075069	5.007270
3.310407	208.286703	5.012275
3.064207	223.578138	5.017280
3.198163	213.430789	5.022285
3.768977	235.402590	5.027290
2.998816	220.819106	5.032294
3.705704	237.604210	5.037299
3.282299	245.311210	5.042304
3.477134	248.369156	5.047309
3.757276	250.625301	5.052314
3.313545	231.293497	5.057318
3.616783	244.250306	5.062323
3.563865	231.263074	5.067328
3.220035	236.628828	5.072333
3.458162	255.254458	5.077338
3.573835	249.801214	5.082342
3.928155	245.753824	5.087347
3.960821	236.978227	5.092352
3.093560	250.009316	5.097357
3.527146	228.429549	5.102362
3.310948	249.708318	5.107366
3.672117	238.477437	5.112371
3.560613	247.473517	5.117376
3.866425	251.418712	5.122381
3.519386	238.320173	5.127386
3.504942	254.591582	5.132390
3.807894	243.377224	5.137395
3.809259	251.671811	5.142400
3.699831	246.340016	5.147405
3.992232	250.792110	5.152410
3.864205	257.663681	5.157414
3.554605	234.172704	5.162419
3.868361	243.653988	5.167424
3.784482	241.469873	5.172429
3.645616	237.285092	5.177434
3.777352	240.086720	5.182438
4.036298	248.896888	5.187443
3.597449	230.795503	5.192448
3.445413	242.091940	5.197453
3.917122	242.634181	5.202458
3.731551	244.668387	5.207462
3.682525	230.895866	5.212467
4.024175	247.323372	5.217472
3.659566	245.188907	5.222477
3.894641	238.401944	5.227482
3.757787	238.516893	5.232486
3.927426	242.684747	5.237491
3.781339	248.482458	5.242496
3.894479	241.115471	5.247501
3.845788	238.020545	5.252506
3.633172	245.243268	5.257510
3.954634	239.535146	5.262515
3.526396	242.742231	5.267520
3.926241	247.362322	5.272525
4.221253	256.167519	5.277530
3.922197	265.268493	5.282534
4.328211	244.247267	5.287539
4.005026	259.871673	5.292544
3.986613	245.089744	5.297549
4.191315	254.607208	5.302554
4.146096	248.487158	5.307558
4.339510	246.669860	5.312563
3.816407	244.707094	5.317568
3.750565	266.639343	5.322573
4.469753	260.957028	5.327578
4.482143	280.666256	5.332582
4.331661	256.694278	5.337587
3.839577	247.675913	5.342592
3.863876	267.553521	5.347597
4.561784	262.161789	5.352602
4.144474	272.454841	5.357606
4.397617	264.495308	5.362611
4.482078	257.765683	5.367616
4.084992	269.687424	5.372621
4.287034	251.282901	5.377626
4.263814	269.346730	5.382630
4.517752	263.698392	5.387635
4.489435	262.964985	5.392640
4.266717	248.426445	5.397645
4.517691	237.044298	5.402650
4.303190	244.246025	5.407654
4.132664	238.182990	5.412659
4.227445	252.562233	5.417664
4.595874	262.607835	5.422669
4.606440	268.144191	5.427674
4.057420	254.004445	5.432678
4.474575	264.671568	5.437683
4.643131	269.522944	5.442688
4.281481	273.128419	5.447693
4.510483	275.864459	5.452698
4.543469	282.581189	5.457702
4.581006	260.353898	5.462707
4.712574	260.216833	5.467712
4.318639	245.637637	5.472717
4.655049	252.110956	5.477722
4.714890	259.677826	5.482726
4.612876	245.668119	5.487731
4.507416	234.642896	5.492736
4.422315	229.516515	5.497741
4.389223	243.048288	5.502746
4.532174	266.563758	5.507750
4.985939	255.953742	5.512755
4.690760	257.580793	5.517760
4.619041	230.901859	5.522765
4.711921	236.019650	5.527770
4.300875	229.789997	5.532774
4.756391	249.438776	5.537779
4.825137	256.295386	5.542784
4.779005	264.019852	5.547789
4.725820	255.592158	5.552794
4.403317	258.358078	5.557798
4.526480	256.256544	5.562803
4.862507	261.393842	5.567808
4.509810	259.421655	5.572813
4.644151	267.864641	5.577818
4.390442	259.701908	5.582822
4.857735	260.548222	5.587827
5.032884	263.080376	5.592832
4.704715	261.967503	5.597837
5.066591	257.018303	5.602842
4.768895	263.418659	5.607846
4.880315	256.102358	5.612851
4.625655	259.606594	5.617856
4.595986	266.032400	5.622861
4.877497	259.507951	5.627866
4.483136	273.052794	5.632870
4.680475	263.370322	5.637875
4.726291	271.099325	5.642880
5.037291	277.730253	5.647885
5.187103	289.892394	5.652890
4.841269	282.953117	5.657894
4.770309	278.448728	5.662899
5.353731	281.325465	5.667904
5.108018	288.526254	5.672909
5.045604	280.659408	5.677914
5.117115	281.728969	5.682918
5.056989	272.313071	5.687923
5.085615	282.439604	5.692928
4.743671	272.803338	5.697933
5.243435	271.743140	5.702938
5.121146	279.504762	5.707942
4.971625	287.307685	5.712947
5.173800	286.916276	5.717952
5.031416	283.905188	5.722957
5.390571	276.369284	5.727962
5.250253	289.720536	5.732966
5.173649	286.418317	5.737971
5.111844	285.936668	5.742976
5.375456	292.792757	5.747981
5.367815	288.211707	5.752986
4.705275	288.216928	5.757990
5.211142	290.371456	5.762995
5.086209	296.707958	5.768000
4.925242	303.639842	5.773005
5.074059	285.037702	5.778010
5.044308	290.949181	5.783014
5.108865	288.815402	5.788019
5.237736	299.154934	5.793024
5.079310	299.360555	5.798029
5.430588	303.440994	5.803034
5.094572	290.252989	5.808038
5.213111	296.436006	5.813043
5.223597	309.444704	5.818048
5.380737	303.155252	5.823053
5.650878	314.498180	5.828058
5.359158	303.533579	5.833062
5.561744	295.807994	5.838067
5.342201	291.476622	5.843072
5.330832	297.975376	5.848077
5.508073	305.325767	5.853082
5.496958	312.399902	5.858086
5.451222	300.032021	5.863091
5.299285	305.104767	5.868096
5.722729	321.267084	5.873101
6.104429	309.290625	5.878106
5.618807	293.988842	5.883110
5.032659	299.032527	5.888115
5.233521	296.474426	5.893120
5.458358	318.623285	5.898125
5.465848	313.803858	5.903130
5.500152	327.150748	5.908134
5.842704	312.499195	5.913139
5.934467	322.507498	5.918144
5.697184	323.643978	5.923149
5.769924	322.213093	5.928154
5.773344	323.239358	5.933158
5.806410	322.486136	5.938163
5.446874	308.187176	5.943168
5.428700	324.358063	5.948173
5.987519	313.707365	5.953178
5.673154	322.672893	5.958182
5.882377	317.035378	5.963187
6.017874	326.285050	5.968192
5.880827	311.671030	5.973197
5.803482	308.213360	5.978202
5.368638	291.706188	5.983206
5.597249	313.888647	5.988211
5.896659	318.270451	5.993216
5.409983	320.223029	5.998221
5.892191	322.760873	6.003226
5.639075	315.613993	6.008230
5.678703	322.172002	6.013235
5.839522	312.546240	6.018240
5.451524	328.270506	6.023245
5.978923	319.851197	6.028250
5.802130	326.156921	6.033254
5.762264	320.234241	6.038259
5.661877	320.694057	6.043264
5.535534	320.219424	6.048269
5.740280	325.837155	6.053274
5.707250	311.474762	6.058278
5.706455	317.928668	6.063283
5.866214	308.950513	6.068288
5.923791	327.616526	6.073293
5.975888	315.603679	6.078298
5.746479	322.384901	6.083302
5.970330	324.300355	6.088307
6.048004	323.061809	6.093312
5.979331	319.245793	6.098317
6.108351	311.466560	6.103322
6.023262	326.452494	6.108326
6.099943	314.257525	6.113331
5.982214	307.120828	6.118336
5.557656	313.692412	6.123341
5.533103	300.225244	6.128346
5.756418	309.662228	6.133350
5.895603	319.713397	6.138355
6.053446	327.058816	6.143360
5.706666	308.129951	6.148365
5.844172	309.540683	6.153370
5.624080	307.956952	6.158374
5.976474	312.264594	6.163379
5.721672	322.372195	6.168384
5.660643	314.004265	6.173389
5.755695	335.003837	6.178394
6.055062	325.072639	6.183398
5.934217	318.823302	6.188403
5.740611	305.549402	6.193408
5.494136	297.926835	6.198413
5.648946	318.812830	6.203418
5.850655	327.116965	6.208422
6.036536	325.531346	6.213427
5.788048	315.525361	6.218432
5.673192	315.540888	6.223437
5.760814	328.946148	6.228442
5.842892	332.857904	6.233446
5.827723	324.344182	6.238451
5.866073	307.276400	6.243456
5.668741	308.914808	6.248461
5.804327	310.678625	6.253466
5.965479	316.204810	6.258470
5.786199	301.354907	6.263475
6.010299	297.460622	6.268480
5.370526	286.293715	6.273485
5.869941	308.451536	6.278490
6.109244	314.755867	6.283494
5.997577	293.960701	6.288499
5.725189	295.244047	6.293504
5.705283	296.465839	6.298509
6.191151	288.344917	6.303514
5.735953	297.242356	6.308518
5.673225	294.965166	6.313523
5.785218	283.905647	6.318528
5.419653	278.423017	6.323533
5.725529	298.250974	6.328538
5.811903	293.415952	6.333542
5.957633	299.302675	6.338547
5.730921	286.020552	6.343552
6.031093	293.402411	6.348557
5.530750	280.913465	6.353562
5.348676	301.611252	6.358566
5.858811	309.445250	6.363571
5.924647	310.165845	6.368576
6.040282	320.110815	6.373581
6.028271	296.268302	6.378586
5.769575	291.185880	6.383590
5.758382	281.121465	6.388595
5.811126	292.412803	6.393600
5.401944	297.735616	6.398605
5.862181	283.712859	6.403610
5.819448	303.862320	6.408614
6.196538	300.468841	6.413619
5.746576	298.559088	6.418624
5.831556	295.516243	6.423629
5.745403	303.807270	6.428634
5.534837	292.583829	6.433638
5.703315	288.926516	6.438643
5.813980	287.868769	6.443648
5.498000	291.293573	6.448653
5.522013	304.895572	6.453658
5.922633	316.017273	6.458662
6.214086	328.941377	6.463667
6.110754	306.701491	6.468672
5.665144	307.464783	6.473677
5.965345	304.576463	6.478682
5.670623	298.799688	6.483686
5.755920	308.058830	6.488691
5.632039	288.835777	6.493696
5.490404	298.110122	6.498701
5.905677	309.078366	6.503706
6.287085	326.622794	6.508710
6.108968	302.660440	6.513715
6.087766	314.470969	6.518720
5.760594	298.427104	6.523725
5.676171	289.396683	6.528730
5.690196	299.919050	6.533734
5.603822	301.834178	6.538739
5.617404	295.771768	6.543744
5.326921	303.064899	6.548749
6.120382	308.836687	6.553754
5.663692	294.752868	6.558758
5.548704	296.884127	6.563763
5.814892	295.683580	6.568768
5.746130	316.287491	6.573773
6.156228	298.030534	6.578778
5.828618	299.585510	6.583782
5.854923	299.169698	6.588787
6.065855	287.108033	6.593792
5.786323	298.896924	6.598797
6.117734	295.053563	6.603802
6.004788	304.636675	6.608806
5.889377	295.586908	6.613811
6.086131	308.201401	6.618816
6.255157	293.489662	6.623821
6.284138	304.996932	6.628826
5.848349	292.796212	6.633830
5.801521	304.132129	6.638835
5.826139	276.555870	6.643840
5.653304	296.355905	6.648845
6.127149	290.474016	6.653850
5.983283	297.377127	6.658854
5.649479	279.238693	6.663859
5.405539	284.711661	6.668864
5.521334	306.557324	6.673869
5.884380	297.599638	6.678874
5.629622	301.249702	6.683878
5.935794	296.983464	6.688883
5.851643	303.838137	6.693888
5.656213	300.356381	6.698893
5.790050	288.154749	6.703898
5.716068	304.846033	6.708902
5.754312	296.884611	6.713907
5.839457	308.291944	6.718912
5.575746	297.707053	6.723917
5.448677	297.373804	6.728922
5.627402	298.961013	6.733926
5.827814	306.992687	6.738931
5.915423	286.546763	6.743936
5.986473	309.085035	6.748941
6.064843	291.133574	6.753946
5.802972	305.560958	6.758950
5.994278	298.950087	6.763955
6.074065	287.480283	6.768960
5.903201	304.613837	6.773965
5.924281	290.067224	6.778970
5.739044	298.621145	6.783974
5.755886	284.745059	6.788979
5.758697	284.137709	6.793984
5.750359	300.105406	6.798989
6.151800	292.726952	6.803994
5.589564	287.741159	6.808998
5.606008	289.484809	6.814003
5.409278	286.696375	6.819008
5.501424	288.134529	6.824013
5.903948	286.783406	6.829018
5.949083	279.247311	6.834022
5.790881	280.071715	6.839027
5.779617	287.690302	6.844032
5.650864	304.287352	6.849037
5.642430	287.167544	6.854042
5.430384	289.691086	6.859046
5.490419	304.313763	6.864051
5.500549	287.824899	6.869056
5.633471	286.913813	6.874061
5.666042	293.939879	6.879066
5.456393	294.748519	6.884070
5.549960	298.826859	6.889075
5.946913	288.981461	6.894080
5.705824	304.513624	6.899085
5.918140	290.354266	6.904090
5.702843	305.792102	6.909094
5.855383	309.667644	6.914099
5.778419	305.951354	6.919104
5.674728	310.459456	6.924109
6.145226	305.813784	6.929114
5.698183	299.481242	6.934118
5.906042	288.880473	6.939123
6.008823	288.264197	6.944128
5.738768	278.983215	6.949133
5.854835	292.427541	6.954138
5.818684	288.545391	6.959142
5.993480	286.180511	6.964147
5.988921	292.586592	6.969152
5.640475	281.934035	6.974157
5.449291	291.192889	6.979162
5.734483	281.328184	6.984166
5.909965	294.858678	6.989171
5.997242	284.502167	6.994176
5.782846	284.514020	6.999181
6.129342	277.306437	7.004186
5.636901	287.674951	7.009190
5.615536	292.384989	7.014195
5.951783	281.852777	7.019200
5.624782	297.503204	7.024205
5.803056	299.773528	7.029210
5.733874	280.434215	7.034214
5.600977	293.723279	7.039219
5.827437	290.407769	7.044224
5.367440	291.241506	7.049229
5.726677	277.510675	7.054234
5.687604	299.783322	7.059238
5.931291	312.864365	7.064243
6.004568	296.877927	7.069248
5.707323	299.397499	7.074253
6.193224	296.656946	7.079258
5.668553	299.621027	7.084262
5.766139	296.970100	7.089267
5.842125	294.135410	7.094272
5.232501	310.465090	7.099277
5.921683	304.238346	7.104282
5.842654	325.381501	7.109286
5.751138	315.595702	7.114291
5.997470	299.424995	7.119296
5.696668	305.096575	7.124301
5.748705	302.759773	7.129306
5.892800	296.743565	7.134310
5.948756	303.807006	7.139315
5.725555	307.893308	7.144320
5.350946	297.580862	7.149325
5.948079	313.872797	7.154330
5.815030	323.559766	7.159334
5.659688	321.648474	7.164339
6.054515	305.758536	7.169344
5.512604	316.629869	7.174349
5.984927	300.271966	7.179354
5.808658	323.039057	7.184358
5.798376	312.552847	7.189363
5.797520	315.905355	7.194368
5.659089	320.644810	7.199373
5.984008	302.672616	7.204378
5.282433	309.417137	7.209382
5.898669	305.074400	7.214387
6.186976	320.847193	7.219392
5.680464	302.686963	7.224397
6.089159	307.963594	7.229402
5.873497	306.060399	7.234406
5.872325	293.594402	7.239411
6.080003	292.533149	7.244416
5.980026	298.443215	7.249421
6.025508	296.771203	7.254426
5.871764	286.048289	7.259430
6.095687	285.298054	7.264435
6.027016	302.249580	7.269440
5.780135	289.170944	7.274445
6.229861	303.537250	7.279450
5.984096	287.808934	7.284454
5.894686	287.293770	7.289459
6.089051	295.540899	7.294464
5.502263	288.771854	7.299469
5.571823	296.311487	7.304474
5.732260	293.654514	7.309478
5.990131	302.498726	7.314483
6.028174	279.825236	7.319488
5.774123	300.296978	7.324493
5.696551	281.526574	7.329498
6.022194	301.121418	7.334502
5.737673	280.208444	7.339507
5.873368	286.919151	7.344512
5.747459	281.633966	7.349517
5.736863	272.582673	7.354522
5.857476	283.930856	7.359526
5.520842	289.574811	7.364531
5.789506	279.508637	7.369536
5.674054	302.473893	7.374541
5.844455	291.110645	7.379546
5.595047	298.159145	7.384550
5.938912	302.285891	7.389555
6.126500	303.545109	7.394560
5.666360	306.513916	7.399565
5.914885	287.978652	7.404570
5.889627	296.669002	7.409574
5.740004	303.667967	7.414579
5.660862	280.245569	7.419584
5.448768	290.830356	7.424589
5.866890	294.603209	7.429594
5.718119	285.932048	7.434598
5.557517	309.567002	7.439603
5.887643	306.071192	7.444608
5.538970	299.599575	7.449613
5.856666	311.742670	7.454618
5.795377	312.077350	7.459622
5.527583	307.359453	7.464627
5.688721	294.053966	7.469632
5.526171	319.042119	7.474637
5.908000	310.383383	7.479642
6.089455	311.348854	7.484646
6.102120	298.368187	7.489651
6.004431	301.450221	7.494656
5.781551	290.032210	7.499661
5.617534	300.627210	7.504666
5.825117	291.720079	7.509670
5.687673	309.343626	7.514675
6.015912	293.051271	7.519680
5.392286	295.127495	7.524685
5.827304	312.922788	7.529690
5.691158	302.378665	7.534694
5.762459	315.587932	7.539699
5.790106	298.760164	7.544704
5.496170	317.037577	7.549709
5.771572	293.887038	7.554714
5.450530	313.290754	7.559718
5.901979	296.924664	7.564723
5.807529	304.045417	7.569728
6.109537	312.160827	7.574733
5.919736	302.067910	7.579738
5.898075	305.307647	7.584742
5.716228	304.573765	7.589747
6.102570	289.396008	7.594752
5.958275	313.246088	7.599757
6.130578	302.835461	7.604762
6.174746	321.367350	7.609766
5.732483	303.639433	7.614771
5.631461	292.920625	7.619776
5.660763	291.477982	7.624781
5.932088	303.264327	7.629786
6.015690	307.741080	7.634790
5.788428	290.501173	7.639795
5.619714	289.679100	7.644800
5.620144	295.236772	7.649805
5.897899	303.349970	7.654810
5.915862	300.236322	7.659814
5.666587	304.527089	7.664819
5.909363	301.412786	7.669824
5.602290	297.414216	7.674829
5.608326	302.785407	7.679834
5.544893	308.605980	7.684838
5.590498	298.439635	7.689843
5.677507	306.382426	7.694848
5.775446	297.445765	7.699853
5.770899	299.680109	7.704858
5.989528	301.518294	7.709862
5.815002	304.708518	7.714867
6.118542	300.914746	7.719872
5.873893	302.348879	7.724877
5.650245	299.764456	7.729882
5.668709	299.086352	7.734886
5.746187	297.824461	7.739891
5.875707	299.512727	7.744896
5.659505	307.054509	7.749901
5.738831	301.395259	7.754906
5.721383	303.046752	7.759910
5.589929	306.161199	7.764915
5.966936	300.974504	7.769920
5.715964	300.486336	7.774925
5.826865	291.401734	7.779930
5.934684	303.282477	7.784934
5.751494	295.317008	7.789939
5.892361	298.025396	7.794944
6.009913	294.520525	7.799949
6.260104	302.859349	7.804954
5.965292	300.733761	7.809958
5.883405	294.891726	7.814963
5.709999	282.325664	7.819968
5.580475	290.505572	7.824973
5.811125	277.005719	7.829978
5.444620	284.451881	7.834982
5.489439	299.121657	7.839987
5.717701	285.404474	7.844992
5.474860	301.355586	7.849997
5.637501	302.069159	7.855002
5.889723	309.565392	7.860006
5.745968	295.212336	7.865011
5.987913	303.262202	7.870016
5.780663	303.950588	7.875021
5.810243	303.366730	7.880026
5.668076	306.736671	7.885030
5.647325	312.752718	7.890035
6.073746	303.633129	7.895040
5.790170	301.099155	7.900045
5.727096	315.001931	7.905050
5.888706	306.094300	7.910054
5.736330	290.104322	7.915059
6.020875	300.390901	7.920064
5.582418	306.934889	7.925069
6.006816	295.447093	7.930074
5.732483	298.720299	7.935078
5.658426	299.227849	7.940083
5.743275	299.899924	7.945088
5.928613	294.981860	7.950093
5.585997	289.876019	7.955098
5.849556	295.853852	7.960102
5.513874	297.497465	7.965107
5.772784	286.872082	7.970112
5.665808	305.623466	7.975117
5.778112	293.454588	7.980122
5.717567	305.980604	7.985139
6.005323	295.311225	7.990157
6.036457	294.503851	7.995174
6.217249	300.883825	8.000192
6.025954	295.102952	8.005210
5.903592	301.848486	8.010227
5.599604	295.662246	8.015245
6.215066	302.564996	8.020262
5.935761	298.181828	8.025280
5.888351	312.796456	8.030298
5.943632	297.395026	8.035315
5.774874	310.057050	8.040333
6.003360	300.903917	8.045350
5.896156	307.631993	8.050368
5.624480	308.582731	8.055386
5.929028	312.628950	8.060403
5.567052	304.425316	8.065421
5.686760	299.771147	8.070438
5.691842	323.456567	8.075456
5.827878	290.239954	8.080474
5.922606	315.785199	8.085491
5.572137	305.125943	8.090509
5.800276	306.060300	8.095526
5.833959	302.346949	8.100544
5.945330	297.895576	8.105562
5.743159	295.208517	8.110579
6.078316	294.630148	8.115597
6.038128	303.083159	8.120614
6.034366	305.109669	8.125632
5.863063	305.371966	8.130650
6.086492	310.257534	8.135667
5.890376	311.781540	8.140685
6.046238	306.212011	8.145702
5.941485	303.489171	8.150720
6.000047	290.128150	8.155738
6.148800	289.275755	8.160755
6.134596	285.450475	8.165773
6.155667	297.339698	8.170790
5.932069	301.620401	8.175808
6.019442	296.875639	8.180826
5.935359	310.642243	8.185843
5.933781	299.479004	8.190861
6.041304	290.340948	8.195878
6.007061	292.972616	8.200896
6.091306	288.507328	8.205914
6.115726	301.697395	8.210931
5.777910	295.132408	8.215949
5.662198	282.241208	8.220966
5.503292	303.880484	8.225984
5.684230	283.584418	8.231002
5.871930	299.894615	8.236019
5.889638	300.625826	8.241037
6.119438	312.430383	8.246054
6.004838	321.757657	8.251072
6.235838	310.391159	8.256090
6.194682	310.748547	8.261107
5.947914	293.082944	8.266125
6.387997	304.361351	8.271142
6.115884	306.611293	8.276160
6.167324	293.841333	8.281178
6.370290	294.672106	8.286195
6.253754	292.271890	8.291213
6.068342	291.601455	8.296230
6.140864	310.315242	8.301248
6.145316	307.545818	8.306266
6.132280	300.356847	8.311283
6.203556	310.440371	8.316301
6.207534	294.046531	8.321318
6.077355	297.974982	8.326336
6.293862	296.137558	8.331354
6.068736	297.312523	8.336371
5.641262	312.811574	8.341389
6.260537	290.351143	8.346406
6.030877	304.133633	8.351424
5.816781	301.666492	8.356442
6.076111	316.216950	8.361459
6.439900	326.758788	8.366477
6.396492	313.318859	8.371494
6.238165	312.405925	8.376512
5.963319	303.817133	8.381530
6.160571	305.336446	8.386547
6.025033	327.583823	8.391565
6.170120	324.637262	8.396582
6.200254	333.312360	8.401600
6.252216	319.115440	8.406618
6.529214	318.373209	8.411635
6.157379	327.016534	8.416653
6.676247	326.333318	8.421670
5.934546	321.682369	8.426688
6.226338	318.921247	8.431706
6.344367	320.956069	8.436723
6.238193	338.552312	8.441741
6.168366	319.245598	8.446758
6.114793	341.285016	8.451776
6.181317	319.685651	8.456794
6.201045	321.499583	8.461811
5.946277	329.659720	8.466829
6.387236	321.442637	8.471846
6.221226	338.227451	8.476864
6.119668	338.949248	8.481882
6.372088	333.055769	8.486899
6.058544	330.191792	8.491917
6.268089	329.659962	8.496934
6.717609	318.353576	8.501952
5.991010	336.398609	8.506970
6.138698	322.816098	8.511987
6.044352	334.603200	8.517005
6.205788	315.170993	8.522022
6.167132	319.390731	8.527040
6.230631	329.146711	8.532058
6.388917	315.762102	8.537075
6.007962	342.050576	8.542093
6.430981	333.606400	8.547110
6.709758	355.984600	8.552128
6.521747	333.115649	8.557146
6.542443	321.988071	8.562163
6.507044	331.153880	8.567181
6.476045	329.826610	8.572199
6.459907	333.075192	8.577216
6.305483	336.766587	8.582234
6.479168	327.462108	8.587251
6.070369	332.511402	8.592269
6.419171	328.470553	8.597287
6.594742	347.859872	8.602304
6.537593	341.216207	8.607322
6.603661	329.230681	8.612339
6.587032	327.486589	8.617357
6.655110	329.666438	8.622375
6.494825	319.290612	8.627392
6.241032	326.293342	8.632410
6.241045	321.005592	8.637427
6.430934	322.207319	8.642445
6.618922	334.258104	8.647463
6.583297	337.709457	8.652480
6.312793	331.146416	8.657498
6.596809	331.563813	8.662515
6.697586	341.252142	8.667533
6.777438	337.385033	8.672551
6.714510	328.023228	8.677568
6.632795	335.969980	8.682586
6.671993	336.650115	8.687603
6.461437	323.717878	8.692621
6.673812	323.678253	8.697639
6.647292	328.952967	8.702656
6.399913	338.983593	8.707674
6.726062	326.877353	8.712691
6.173509	340.654102	8.717709
6.514030	338.324266	8.722727
6.517504	342.773889	8.727744
6.263259	338.986199	8.732762
6.786595	329.301290	8.737779
6.604229	342.501755	8.742797
6.642757	335.272758	8.747815
6.546303	326.667755	8.752832
6.368763	345.622657	8.757850
7.064559	350.967615	8.762867
6.811395	338.209880	8.767885
6.611226	334.399872	8.772903
6.700537	330.863783	8.777920
6.450289	331.218632	8.782938
6.939645	336.367847	8.787955
6.349271	334.780565	8.792973
6.451032	331.822270	8.797991
6.877318	344.563688	8.803008
6.567232	354.307824	8.808026
6.847018	347.428897	8.813043
6.829321	356.864453	8.818061
6.611101	345.344970	8.823079
6.853932	359.399324	8.828096
6.530418	341.043302	8.833114
6.748620	345.561937	8.838131
6.726904	336.864186	8.843149
6.620535	356.667919	8.848167
6.946660	357.345406	8.853184
6.633520	359.925075	8.858202
6.862479	337.626690	8.863219
6.788666	341.250252	8.868237
6.817689	322.925138	8.873255
6.977043	326.728406	8.878272
6.727664	331.822691	8.883290
6.815201	338.304682	8.888307
6.990313	336.716839	8.893325
6.498304	338.759693	8.898343
6.883587	333.308395	8.903360
6.414147	333.028008	8.908378
6.606549	340.302278	8.913395
6.774856	356.357055	8.918413
6.824527	350.412161	8.923431
7.003825	350.130632	8.928448
6.634252	351.523119	8.933466
7.350436	359.763586	8.938483
6.980042	344.867568	8.943501
6.475199	353.287586	8.948519
7.098631	344.929637	8.953536
6.742353	359.324567	8.958554
7.307463	346.267466	8.963571
6.792990	338.361478	8.968589
6.857810	333.367454	8.973607
7.061528	321.585301	8.978624
6.643603	329.623823	8.983642
6.917474	330.431957	8.988659
6.942695	339.859032	8.993677
7.060992	333.200741	8.998695
7.038472	338.150776	9.003712
6.602157	324.970792	9.008730
6.920576	333.180946	9.013747
6.649847	344.807496	9.018765
6.987864	349.777947	9.023783
7.558152	346.406390	9.028800
6.705958	345.660670	9.033818
7.018725	335.982415	9.038835
6.926371	341.243316	9.043853
7.014796	336.181235	9.048871
7.050976	354.820200	9.053888
6.865863	330.748067	9.058906
7.061059	341.758498	9.063923
7.004383	336.309197	9.068941
6.824752	353.332431	9.073959
7.327901	350.014082	9.078976
6.834349	343.236986	9.083994
7.215160	347.112980	9.089011
6.905410	328.300892	9.094029
6.839591	350.409848	9.099047
7.078193	356.529182	9.104064
7.123210	361.460388	9.109082
6.976162	362.261927	9.114099
6.946009	346.266669	9.119117
6.688764	365.192162	9.124135
6.659890	344.710182	9.129152
6.553345	363.506466	9.134170
6.507347	363.551163	9.139187
6.692047	350.941659	9.144205
6.730767	371.150739	9.149223
7.522163	373.162054	9.154240
7.276708	380.277669	9.159258
7.183473	361.695037	9.164275
7.229864	357.213256	9.169293
7.233313	361.700378	9.174311
7.284236	346.528883	9.179328
7.166831	354.049777	9.184346
7.051692	351.125160	9.189363
7.114343	336.350048	9.194381
7.079657	368.977044	9.199399
7.275010	349.470900	9.204416
7.181654	364.855650	9.209434
7.221231	351.256640	9.214451
6.929123	349.378498	9.219469
6.861700	367.862602	9.224487
6.970909	371.786145	9.229504
7.459354	384.053479	9.234522
7.216662	392.401069	9.239539
7.294140	395.319420	9.244557
7.161062	391.846932	9.249575
7.156427	395.833771	9.254592
7.177669	403.321443	9.259610
7.307084	394.798823	9.264627
7.364749	380.884288	9.269645
7.404315	393.437761	9.274663
7.531711	385.743099	9.279680
7.517907	382.586534	9.284698
7.268508	383.246964	9.289715
7.376243	364.544427	9.294733
7.300218	367.694283	9.299751
7.478881	358.497298	9.304768
6.906175	359.142280	9.309786
7.171918	376.089376	9.314803
7.451459	378.189023	9.319821
7.271550	396.907045	9.324839
7.695393	392.317316	9.329856
7.419269	378.013487	9.334874
7.089413	370.221615	9.339891
7.292454	365.202474	9.344909
7.222709	393.578069	9.349927
7.606227	377.098587	9.354944
7.312642	388.613725	9.359962
7.263225	386.826240	9.364979
7.578788	381.517611	9.369997
7.296335	391.463936	9.375015
7.619683	385.514535	9.380032
7.442193	370.607964	9.385050
7.184145	371.625135	9.390067
7.505626	384.122071	9.395085
7.588463	371.909690	9.400103
7.483832	372.506344	9.405120
7.133386	380.611966	9.410138
7.399335	372.070140	9.415155
7.465142	385.978036	9.420173
7.361747	406.375661	9.425191
7.322088	388.210596	9.430208
7.386516	394.009519	9.435226
7.450759	393.077214	9.440243
7.579697	391.651677	9.445261
7.479580	392.101564	9.450279
7.809435	379.481627	9.455296
7.563518	393.032895	9.460314
7.460643	384.275519	9.465331
7.542164	387.125306	9.470349
7.423691	386.701507	9.475367
7.527738	388.885949	9.480384
7.471384	399.203852	9.485402
7.464962	394.742104	9.490419
7.424902	392.483619	9.495437
7.590039	398.680447	9.500455
7.991984	395.397707	9.505472
7.786003	410.591923	9.510490
7.510467	391.890703	9.515507
7.758156	388.385496	9.520525
7.508548	388.725875	9.525543
7.637685	381.579984	9.530560
7.590875	399.109514	9.535578
7.606885	387.752807	9.540595
7.569060	399.318473	9.545613
7.745304	391.236414	9.550631
7.841296	392.876870	9.555648
7.755709	365.574187	9.560666
7.179028	377.021961	9.565683
7.530938	365.723702	9.570701
7.527387	388.147427	9.575719
7.686389	372.085852	9.580736
7.741859	385.721716	9.585754
7.713341	388.285346	9.590771
7.785565	392.470839	9.595789
7.486153	390.503374	9.600807
7.662522	395.618041	9.605824
7.646232	397.185152	9.610842
7.961042	395.567623	9.615859
8.174423	386.037811	9.620877
7.767968	398.049524	9.625895
7.620657	393.192478	9.630912
7.815081	397.405599	9.635930
7.713507	389.546372	9.640947
8.169335	390.358779	9.645965
7.470496	386.734882	9.650983
7.757718	375.283081	9.656000
7.904767	385.938908	9.661018
7.615912	397.615626	9.666035
7.660832	387.395943	9.671053
7.563482	406.283254	9.676071
7.605176	400.950213	9.681088
7.670022	390.179852	9.686106
7.966622	394.798800	9.691123
7.954474	403.794714	9.696141
7.815066	408.318152	9.701159
7.707306	392.619450	9.706176
7.616383	397.944386	9.711194
7.835383	399.342432	9.716211
8.146133	397.503197	9.721229
7.982344	389.883813	9.726247
7.758678	407.332572	9.731264
8.237450	390.911427	9.736282
7.812158	404.691407	9.741299
7.965661	389.312124	9.746317
7.614010	393.506860	9.751335
7.714259	399.532672	9.756352
7.888033	399.655878	9.761370
7.826500	397.103093	9.766387
8.209194	393.030256	9.771405
7.880366	404.714077	9.776423
7.589725	388.819387	9.781440
7.857566	402.590100	9.786458
7.724994	396.757369	9.791475
7.782066	385.335135	9.796493
7.673163	398.141135	9.801511
7.915053	396.731271	9.806528
8.070308	401.645551	9.811546
8.067499	411.151887	9.816563
8.232468	398.799864	9.821581
7.875223	386.608247	9.826599
8.087417	404.694711	9.831616
8.061700	384.846129	9.836634
7.749678	399.116492	9.841651
7.976020	403.095073	9.846669
7.845005	404.464080	9.851687
8.259859	417.957925	9.856704
8.337008	410.538408	9.861722
7.962164	416.407377	9.866739
8.243485	400.511233	9.871757
7.937294	406.264748	9.876775
7.944839	400.401577	9.881792
8.290524	413.837480	9.886810
8.216523	406.908857	9.891827
8.271513	393.861042	9.896845
7.963018	386.530952	9.901863
7.930519	387.477196	9.906880
8.518718	408.923584	9.911898
7.953569	408.949974	9.916915
8.114247	381.743630	9.921933
8.350039	406.465843	9.926951
8.201771	396.685152	9.931968
8.162187	391.472800	9.936986
8.191908	390.894822	9.942003
8.145003	389.127683	9.947021
8.200253	407.875833	9.952039
8.341570	404.905772	9.957056
8.410818	401.172055	9.962074
8.046998	400.535134	9.967091
7.956039	389.021940	9.972109
8.467826	400.667791	9.977127
8.347684	408.828451	9.982144
8.368501	393.056250	9.987162
8.214658	412.120672	9.992179
8.131158	390.261632	9.997197
8.272268	403.860531	10.002215
8.289213	409.572451	10.007232
8.449537	407.125183	10.012250
8.234637	399.817108	10.017267
8.055543	405.188007	10.022285
8.563080	407.337454	10.027303
8.143884	412.835806	10.032320
8.221915	404.080107	10.037338
8.026777	413.361905	10.042355
8.525639	407.299557	10.047373
8.547477	411.972479	10.052391
8.292234	421.805893	10.057408
8.816142	410.625099	10.062426
8.353018	410.647616	10.067443
8.298051	400.059503	10.072461
8.230143	403.659964	10.077479
8.276533	423.402327	10.082496
8.952777	416.309564	10.087514
8.281531	412.307879	10.092531
8.537789	398.371331	10.097549
8.090367	401.058903	10.102567
8.033436	411.613358	10.107584
8.260457	413.608532	10.112602
8.346878	410.944703	10.117619
8.586610	414.079875	10.122637
8.518338	415.044825	10.127655
8.363943	433.989025	10.132672
8.620970	419.205128	10.137690
8.737630	427.460090	10.142707
8.875989	409.848388	10.147725
8.672100	414.858531	10.152743
8.196208	410.643510	10.157760
8.656817	409.950927	10.162778
8.292925	420.260533	10.167795
8.729074	412.325908	10.172813
8.669507	422.093628	10.177831
8.557534	422.339233	10.182848
8.526353	413.957875	10.187866
8.479833	418.298788	10.192883
8.544089	417.346800	10.197901
8.418587	422.475351	10.202919
8.349018	419.348953	10.207936
8.636085	409.090025	10.212954
8.292728	413.465824	10.217971
8.712330	420.084649	10.222989
8.739502	410.301030	10.228007
8.664292	409.666398	10.233024
8.690696	415.069659	10.238042
8.486622	418.768000	10.243059
8.623453	423.232112	10.248077
8.501741	426.122874	10.253095
8.462917	421.352880	10.258112
8.858905	413.074696	10.263130
8.679020	431.117751	10.268147
8.852889	413.886582	10.273165
9.080137	426.376594	10.278183
8.491298	409.386112	10.283200
8.863771	416.019809	10.288218
8.668711	413.072276	10.293235
8.481938	416.372987	10.298253
8.652943	426.747894	10.303271
8.584840	416.618405	10.308288
8.469155	414.521290	10.313306
8.156639	431.768582	10.318323
8.554220	424.263533	10.323341
8.856532	422.460621	10.328359
8.694911	437.692500	10.333376
8.774660	427.609121	10.338394
8.442956	443.331580	10.343411
8.668944	444.342659	10.348429
8.701986	448.931480	10.353447
8.946275	458.867450	10.358464
9.090004	453.517921	10.363482
8.845330	451.797727	10.368499
8.735187	448.953149	10.373517
8.667154	449.554875	10.378535
8.720025	450.236593	10.383552
8.934327	453.654638	10.388570
8.927702	453.006505	10.393587
8.900590	458.220650	10.398605
8.843288	442.245031	10.403623
8.755544	455.820593	10.408640
9.029713	442.476549	10.413658
8.908281	451.315698	10.418675
9.083067	447.038986	10.423693
9.291853	458.815250	10.428711
9.126799	451.199487	10.433728
8.922592	443.942365	10.438746
8.974587	458.062492	10.443763
9.154535	458.713271	10.448781
8.907372	448.971914	10.453799
8.616165	467.078573	10.458816
9.031780	439.263029	10.463834
8.826491	461.692748	10.468851
8.914726	453.731764	10.473869
9.123046	460.159506	10.478887
8.770646	457.517613	10.483904
9.063516	443.567593	10.488922
9.052105	458.776638	10.493939
9.017862	459.177068	10.498957
9.038533	449.681720	10.503975
8.590797	452.206996	10.508992
8.955611	464.388755	10.514010
9.331757	468.008536	10.519027
9.260020	467.211266	10.524045
9.413147	453.997813	10.529063
8.899200	458.353111	10.534080
9.014134	453.605713	10.539098
9.148067	458.636300	10.544115
9.257419	469.038545	10.549133
9.251064	459.695452	10.554151
9.010281	456.541846	10.559168
9.049802	454.502516	10.564186
9.291234	460.161416	10.569203
9.052009	451.142362	10.574221
9.279364	454.863972	10.579239
8.975265	452.025273	10.584256
9.402949	454.051741	10.589274
9.044954	457.336085	10.594291
9.101781	447.242409	10.599309
9.258797	452.677823	10.604327
8.965864	445.033508	10.609344
9.165683	453.185494	10.614362
9.424472	450.396348	10.619379
9.516866	458.126746	10.624397
9.528211	450.012770	10.629415
9.250275	455.979290	10.634432
9.287114	438.880454	10.639450
9.219387	458.460768	10.644467
9.438149	442.054003	10.649485
9.489688	442.523107	10.654503
9.256762	447.863262	10.659520
9.253554	443.631415	10.664538
9.520845	440.072186	10.669555
9.058378	439.734951	10.674573
9.210184	437.447309	10.679591
9.322881	452.979636	10.684608
9.427797	432.813227	10.689626
9.009933	448.720750	10.694643
9.345509	451.658940	10.699661
9.510001	451.185719	10.704679
9.599013	460.534924	10.709696
9.709076	461.572640	10.714714
9.398174	446.411840	10.719731
9.541849	452.938917	10.724749
9.317707	445.606863	10.729767
9.289529	452.435689	10.734784
9.323195	445.881468	10.739802
9.467586	468.532464	10.744819
9.140656	462.040486	10.749837
9.813421	481.577171	10.754855
9.735856	479.091866	10.759872
9.813402	452.904760	10.764890
9.470044	454.090814	10.769907
9.318186	458.034303	10.774925
9.480264	448.470028	10.779943
9.254141	456.889107	10.784960
9.655806	464.234040	10.789978
9.726006	487.743152	10.794995
9.170141	475.292540	10.800013
9.644867	480.943297	10.805031
9.587570	474.202479	10.810048
9.688417	490.798614	10.815066
9.811765	487.007425	10.820083
9.678304	493.355677	10.825101
9.554344	461.404059	10.830119
9.574277	482.988055	10.835136
9.506863	463.847051	10.840154
9.710145	485.875814	10.845171
9.732326	470.906235	10.850189
9.639103	483.857508	10.855207
9.896652	480.716495	10.860224
9.715240	474.299549	10.865242
9.449341	469.039655	10.870259
9.974371	472.418947	10.875277
9.727556	479.359489	10.880295
9.789669	487.710776	10.885312
9.678978	470.715201	10.890330
9.846740	479.311451	10.895347
9.475480	482.613538	10.900365
9.582110	468.136360	10.905383
9.837931	485.143272	10.910400
9.850134	480.510751	10.915418
9.959866	474.401102	10.920435
9.953552	484.438919	10.925453
9.970757	475.413291	10.930471
9.808801	458.959910	10.935488
9.488629	463.581034	10.940506
9.710633	470.311845	10.945523
9.708478	479.465262	10.950541
9.771624	474.140655	10.955559
9.793882	480.088863	10.960576
9.939240	477.054261	10.965594
9.702885	484.082026	10.970611
9.371507	482.734129	10.975629
9.753083	484.184426	10.980647
9.822854	490.813079	10.985664
9.617640	480.300317	10.990682
9.711693	480.417512	10.995699
9.331268	485.813544	11.000717
9.364480	496.201629	11.005735
10.109064	514.652475	11.010752
10.084218	502.408882	11.015770
10.201609	514.018748	11.020787
10.009952	516.429981	11.025805
10.276928	512.392473	11.030823
9.972034	494.502154	11.035840
10.045319	500.270331	11.040858
10.148198	480.639380	11.045875
9.942266	486.831740	11.050893
9.741259	479.824691	11.055911
9.939923	487.178683	11.060928
9.803688	511.434153	11.065946
10.157206	502.807723	11.070963
10.158080	510.558880	11.075981
10.602732	489.429609	11.080999
10.076188	502.667807	11.086016
9.972103	479.806512	11.091034
10.024086	491.712818	11.096051
10.201429	510.017117	11.101069
10.182958	512.019026	11.106087
10.244665	497.718587	11.111104
10.033296	493.981727	11.116122
9.813604	498.391626	11.121139
9.698576	517.290064	11.126157
10.041315	500.452231	11.131175
9.926981	516.067406	11.136192
10.183762	501.021930	11.141210
10.400834	511.082574	11.146227
10.310133	510.970138	11.151245
10.291812	517.206386	11.156263
10.323118	504.346986	11.161280
10.141466	508.173988	11.166298
10.391999	504.507601	11.171315
10.027694	523.725020	11.176333
9.809652	512.250055	11.181351
9.969019	524.642340	11.186368
9.896479	513.586709	11.191386
10.223369	509.288975	11.196403
9.943627	527.871435	11.201421
10.272291	525.984945	11.206439
10.648656	533.101381	11.211456
10.155651	529.308233	11.216474
10.288857	542.454453	11.221491
10.229821	546.316008	11.226509
10.498120	555.892067	11.231527
10.450553	539.509435	11.236544
10.518357	538.920237	11.241562
10.614732	528.506968	11.246579
10.488278	536.986271	11.251597
10.413198	508.106241	11.256615
10.494867	507.863870	11.261632
10.500288	518.605973	11.266650
9.973651	520.831394	11.271667
10.404176	523.654918	11.276685
10.753751	541.721595	11.281703
10.636072	521.606910	11.286720
10.290663	526.853804	11.291738
10.439064	516.657868	11.296755
10.468187	544.717092	11.301773
10.672059	523.780773	11.306791
10.505448	522.347785	11.311808
10.603147	515.984962	11.316826
10.485139	510.711338	11.321843
10.106394	526.310396	11.326861
10.644699	540.494284	11.331879
10.858046	537.075602	11.336896
10.571100	558.284356	11.341914
10.651508	533.499407	11.346931
10.413418	552.717061	11.351949
10.388205	541.029350	11.356967
10.656813	548.863607	11.361984
10.192672	546.277655	11.367002
10.780563	541.746279	11.372019
10.527055	542.570932	11.377037
10.692580	533.522134	11.382055
10.995716	546.730900	11.387072
10.670299	535.710845	11.392090
10.745933	550.987069	11.397107
10.412952	536.767564	11.402125
10.775826	536.276413	11.407143
10.628800	521.741722	11.412160
10.877711	536.153894	11.417178
10.882040	539.307923	11.422195
10.737669	540.192766	11.427213
10.804516	554.758337	11.432231
10.748277	542.270264	11.437248
10.721935	549.504724	11.442266
10.790743	538.151282	11.447283
10.926808	535.492117	11.452301
10.616079	554.489263	11.457319
10.667826	542.211628	11.462336
10.871001	553.249724	11.467354
10.816512	543.210888	11.472371
10.895683	552.809050	11.477389
10.783158	549.427789	11.482407
11.086187	548.136709	11.487424
11.010310	549.149368	11.492442
10.940179	549.741508	11.497459
11.019566	543.395082	11.502477
10.476147	555.108480	11.507495
10.785404	538.325535	11.512512
10.510935	561.029261	11.517530
10.724691	547.747850	11.522547
10.467853	533.220767	11.527565
10.305764	555.533279	11.532583
11.023818	552.991552	11.537600
11.157610	582.780019	11.542618
11.175722	575.568649	11.547635
10.761725	564.576103	11.552653
10.983068	582.190133	11.557671
11.223021	568.739164	11.562688
11.414486	580.628786	11.567706
11.108644	553.654116	11.572723
10.971732	550.248545	11.577741
10.832622	555.275284	11.582759
10.905874	555.035878	11.587776
11.054945	580.798409	11.592794
11.332385	566.646848	11.597811
11.014779	568.970174	11.602829
11.015323	583.914839	11.607847
11.483576	572.289214	11.612864
10.712482	573.262185	11.617882
11.295354	584.944447	11.622899
11.093008	578.687863	11.627917
11.287150	574.408901	11.632935
11.353250	558.871302	11.637952
10.998686	561.096433	11.642970
11.045972	562.272153	11.647987
11.543865	571.713848	11.653005
11.155881	569.751846	11.658023
11.046300	567.328395	11.663040
11.347105	573.233656	11.668058
11.227706	574.847048	11.673075
11.089377	583.789828	11.678093
11.159833	583.007330	11.683111
11.219455	583.340985	11.688128
11.304574	579.146851	11.693146
11.479241	577.283345	11.698163
11.446898	573.848287	11.703181
11.411947	592.851367	11.708199
11.486407	579.308971	11.713216
10.884251	580.574113	11.718234
11.433659	574.750129	11.723251
11.233730	577.900924	11.728269
11.144258	585.167973	11.733287
11.398159	566.201926	11.738304
11.264105	588.109961	11.743322
11.483598	570.599201	11.748339
11.601731	585.548248	11.753357
11.404790	584.808366	11.758375
11.363556	575.722079	11.763392
11.260182	584.290579	11.768410
11.363325	577.330143	11.773427
11.187087	585.701295	11.778445
11.231912	582.637826	11.783463
11.462922	586.561860	11.788480
11.006515	583.411292	11.793498
11.138146	579.183593	11.798515
11.704062	586.277584	11.803533
11.522381	597.477418	11.808551
11.644050	575.833450	11.813568
11.486044	557.217300	11.818586
11.590604	586.037544	11.823603
11.559627	573.201959	11.828621
11.376299	574.785770	11.833639
11.515657	581.160606	11.838656
11.662093	607.410788	11.843674
11.647248	604.237720	11.848691
11.547553	602.451336	11.853709
11.728305	597.105381	11.858727
11.998438	601.037320	11.863744
11.429819	591.327350	11.868762
11.859896	596.428495	11.873779
11.754544	583.133666	11.878797
11.751082	585.343579	11.883815
11.617096	585.473173	11.888832
11.453658	589.429432	11.893850
11.418446	604.684865	11.898867
11.972067	609.692586	11.903885
11.730180	597.050946	11.908903
11.708511	610.273004	11.913920
11.855222	604.552657	11.918938
11.567265	612.310665	11.923955
11.643907	603.431001	11.928973
11.310522	618.824382	11.933991
11.722302	601.926616	11.939008
11.580575	609.004629	11.944026
11.502485	611.774664	11.949043
11.939234	613.141762	11.954061
11.628446	613.102105	11.959079
11.706801	606.089173	11.964096
11.401889	613.083458	11.969114
11.958473	637.824271	11.974131
12.447538	634.827888	11.979149
12.169882	633.033323	11.984167
12.366046	594.138147	11.989184
12.093819	609.298834	11.994202
11.658696	607.362821	11.999219
11.793984	605.880915	12.004237
11.864345	595.043571	12.009255
12.132180	611.064160	12.014272
11.830366	615.912548	12.019290
11.915904	607.259402	12.024307
12.227874	596.249978	12.029325
11.987822	605.688291	12.034343
12.233181	605.402925	12.039360
12.103353	602.102050	12.044378
12.248263	605.484070	12.049395
12.415666	596.461099	12.054413
11.964742	610.497301	12.059431
12.063915	613.376292	12.064448
12.020035	606.067308	12.069466
11.790313	606.866877	12.074483
12.083466	603.968510	12.079501
11.740866	611.649744	12.084519
11.988238	620.107164	12.089536
12.296800	621.591091	12.094554
12.216001	629.422520	12.099571
12.455079	629.093421	12.104589
12.011432	629.553939	12.109607
11.799982	628.486325	12.114624
11.872709	647.530224	12.119642
12.190026	636.067549	12.124659
12.303514	648.493691	12.129677
12.194050	638.241989	12.134695
12.403247	635.057571	12.139712
12.498864	654.480959	12.144730
12.225925	644.583839	12.149747
12.407999	654.766375	12.154765
12.186057	651.107288	12.159783
12.250196	654.797176	12.164800
12.402137	644.339812	12.169818
12.046908	662.230866	12.174835
11.941608	643.439114	12.179853
12.158106	648.317178	12.184871
12.534255	641.741303	12.189888
12.662871	643.358388	12.194906
12.055392	645.350992	12.199923
12.346301	642.028003	12.204941
12.186729	661.162855	12.209959
12.494547	639.233083	12.214976
12.356427	654.551033	12.219994
12.337462	640.726070	12.225011
12.530511	637.786578	12.230029
12.094622	656.452169	12.235047
12.482530	657.241180	12.240064
12.686128	679.114207	12.245082
12.484014	673.781415	12.250099
12.327928	656.716678	12.255117
12.190072	681.196246	12.260135
12.645431	670.304275	12.265152
12.712668	671.213489	12.270170
12.919046	692.701041	12.275187
12.792660	677.489543	12.280205
12.579223	669.230168	12.285223
12.665576	673.366467	12.290240
12.781656	667.842151	12.295258
12.629659	664.343404	12.300275
12.459884	658.775708	12.305293
12.391177	660.716666	12.310311
12.866317	677.862992	12.315328
12.683986	672.834821	12.320346
12.332714	680.585714	12.325363
12.690099	663.555666	12.330381
12.763455	673.997358	12.335399
13.137909	660.112674	12.340416
13.038980	674.376907	12.345434
12.659632	670.481004	12.350451
12.889313	661.123773	12.355469
12.794586	684.319492	12.360487
12.949352	667.351757	12.365504
12.749062	679.013953	12.370522
12.799799	668.268557	12.375539
13.076601	670.067694	12.380557
12.624059	654.042734	12.385575
12.517740	674.722227	12.390592
13.028433	655.213370	12.395610
12.698698	678.779523	12.400627
12.868073	651.149525	12.405645
12.941037	680.672325	12.410663
13.054637	661.694218	12.415680
13.130562	670.793025	12.420698
12.732465	685.107497	12.425715
13.145047	676.878778	12.430733
13.006118	683.221715	12.435751
12.815891	673.580816	12.440768
12.960707	685.394590	12.445786
12.567671	685.346188	12.450803
12.958649	673.197278	12.455821
12.754792	693.771688	12.460839
12.682214	685.001457	12.465856
12.813778	676.097029	12.470874
13.000666	680.579217	12.475891
13.172719	674.391984	12.480909
12.868406	682.705831	12.485927
12.671353	687.552378	12.490944
12.931274	693.891691	12.495962
13.010068	712.667515	12.500979
13.234367	706.684274	12.505997
13.160318	716.080657	12.511015
13.327177	712.663814	12.516032
13.241063	713.247383	12.521050
13.300343	721.431693	12.526067
13.427486	701.375006	12.531085
13.157755	699.364908	12.536103
13.053296	679.616631	12.541120
13.168396	706.492470	12.546138
13.023468	699.613319	12.551155
13.083199	712.531833	12.556173
13.101049	722.929792	12.561191
13.123447	720.699509	12.566208
13.273041	714.117551	12.571226
13.284322	714.068848	12.576243
13.333016	709.924585	12.581261
13.082623	709.212621	12.586279
13.160532	729.330089	12.591296
13.111034	711.089712	12.596314
13.368680	722.151990	12.601331
13.435635	717.432220	12.606349
13.406017	718.474046	12.611367
13.374669	713.531019	12.616384
13.668998	718.416808	12.621402
13.370529	731.261007	12.626419
13.618820	713.788522	12.631437
13.644269	714.584303	12.636455
13.307210	710.040428	12.641472
13.293114	715.612060	12.646490
13.402566	713.118244	12.651507
13.404760	708.669543	12.656525
13.180199	715.352741	12.661543
13.458973	720.539153	12.666560
13.754977	734.041801	12.671578
13.410656	733.808130	12.676595
13.996906	732.415815	12.681613
13.773962	720.711740	12.686631
13.593898	723.401626	12.691648
13.843827	703.446857	12.696666
13.479588	716.179602	12.701683
13.807340	710.584374	12.706701
13.716026	714.584735	12.711719
13.580381	708.301231	12.716736
13.918063	700.091569	12.721754
13.370050	713.336446	12.726771
13.609769	709.168978	12.731789
13.631811	712.896046	12.736807
13.628973	716.709882	12.741824
13.931034	731.236356	12.746842
13.520975	734.029197	12.751859
13.972180	724.974205	12.756877
14.101197	731.084052	12.761895
13.985289	712.426907	12.766912
14.029981	714.983315	12.771930
13.962608	718.726440	12.776947
13.907600	699.590373	12.781965
13.943912	695.720922	12.786983
13.882418	705.537356	12.792000
14.147539	696.988205	12.797018
13.788005	720.439496	12.802035
13.875185	709.299371	12.807053
13.958577	725.572649	12.812071
13.754214	708.663629	12.817088
13.737856	710.013123	12.822106
13.691244	717.043388	12.827123
13.760302	712.323764	12.832141
13.888109	711.342362	12.837159
13.615643	732.917765	12.842176
14.039184	729.442066	12.847194
13.632286	752.306802	12.852211
13.855085	744.452826	12.857229
13.834715	749.331397	12.862247
13.793201	757.879242	12.867264
14.138156	745.026255	12.872282
13.832481	755.082432	12.877299
14.121689	748.604322	12.882317
14.192982	753.885255	12.887335
14.053339	745.371876	12.892352
14.126721	747.489016	12.897370
14.193503	757.374122	12.902387
13.960726	740.806289	12.907405
14.049495	750.208256	12.912423
14.039667	752.181020	12.917440
14.092734	747.149837	12.922458
13.768759	752.104660	12.927475
14.293250	765.241117	12.932493
14.200724	776.814731	12.937511
14.301561	767.932449	12.942528
14.558703	771.791107	12.947546
14.071514	779.251009	12.952563
14.424434	764.210641	12.957581
14.299395	766.399640	12.962599
14.215553	771.190800	12.967616
14.346001	771.308280	12.972634
13.994037	778.508297	12.977651
14.280696	765.056522	12.982669
14.496461	772.323792	12.987687
14.233074	767.709669	12.992704
14.136551	778.646512	12.997722
14.282998	781.615629	13.002739
14.347374	788.771544	13.007757
14.381585	789.678450	13.012775
14.162884	792.899204	13.017792
14.472540	776.795679	13.022810
14.034066	776.742781	13.027827
14.061893	791.146467	13.032845
14.523423	806.929989	13.037863
14.433921	810.414558	13.042880
14.644492	797.822060	13.047898
14.354195	808.801182	13.052915
14.650074	806.879240	13.057933
14.584270	793.901330	13.062951
14.373627	812.642750	13.067968
14.734071	796.402005	13.072986
14.669674	808.384371	13.078003
14.780228	811.871303	13.083021
15.038691	797.793415	13.088039
14.646014	805.163813	13.093056
14.938126	795.243765	13.098074
14.820322	798.262658	13.103091
14.562022	804.746503	13.108109
15.079382	797.456162	13.113127
14.346316	812.504380	13.118144
14.484785	794.732417	13.123162
14.431605	807.887233	13.128179
14.661043	802.087508	13.133197
14.569440	793.777132	13.138215
14.453738	802.535341	13.143232
14.588105	812.334038	13.148250
14.700325	815.527365	13.153267
14.590026	804.306843	13.158285
14.824403	828.635094	13.163303
14.909513	829.875432	13.168320
15.282494	838.308573	13.173338
14.849137	829.861399	13.178355
14.725429	827.801370	13.183373
14.990607	827.135165	13.188391
14.914635	831.475847	13.193408
15.249732	840.574433	13.198426
15.067297	831.236596	13.203443
14.686901	819.998019	13.208461
15.335383	829.504237	13.213479
14.904702	827.519638	13.218496
15.159015	841.404372	13.223514
14.931677	828.068581	13.228531
15.231988	827.399029	13.233549
15.213788	820.384835	13.238567
14.715204	821.201493	13.243584
15.083656	835.220665	13.248602
15.128567	824.379198	13.253619
15.198282	838.426391	13.258637
15.260156	836.625184	13.263655
15.138390	846.602713	13.268672
15.298733	832.981448	13.273690
14.906132	831.947791	13.278707
14.815742	831.360127	13.283725
15.127673	836.033846	13.288743
15.032161	841.932285	13.293760
15.092360	818.764075	13.298778
15.152444	843.578320	13.303795
15.148641	845.667393	13.308813
15.449335	836.769066	13.313831
15.454814	852.523896	13.318848
15.434387	843.783726	13.323866
15.254605	854.330843	13.328883
15.444023	850.204220	13.333901
15.574588	848.869590	13.338919
15.250428	844.539531	13.343936
15.523252	840.577330	13.348954
15.448733	852.276830	13.353971
15.408107	845.454669	13.358989
15.644461	843.840811	13.364007
15.144027	842.041217	13.369024
15.493421	855.932785	13.374042
15.490039	849.413738	13.379059
14.988087	839.078771	13.384077
15.358442	844.795916	13.389095
15.209245	855.219309	13.394112
14.803457	862.692367	13.399130
15.349128	866.692196	13.404147
15.394927	873.629623	13.409165
15.502175	867.463846	13.414183
15.507005	877.827358	13.419200
15.524023	872.911120	13.424218
15.742026	879.021375	13.429235
15.730571	866.567850	13.434253
15.569457	883.252255	13.439271
15.651496	878.309746	13.444288
15.610434	867.685850	13.449306
15.689421	882.347020	13.454323
15.500087	873.261834	13.459341
15.628001	876.583256	13.464359
15.623053	864.469516	13.469376
15.975815	885.690566	13.474394
15.916810	876.752793	13.479411
15.723739	873.967301	13.484429
15.983242	877.759273	13.489447
16.168872	862.796934	13.494464
15.867302	868.541690	13.499482
15.974847	856.189736	13.504499
15.368824	865.522097	13.509517
15.843317	857.843834	13.514535
15.806446	895.374392	13.519552
15.963286	898.853202	13.524570
16.038618	903.753300	13.529587
16.284128	904.204826	13.534605
16.145804	869.785589	13.539623
15.612742	876.303261	13.544640
15.442756	891.450848	13.549658
16.112140	903.076254	13.554675
16.112156	912.447232	13.559693
16.140063	894.857064	13.564711
16.136161	903.788441	13.569728
16.185070	894.857497	13.574746
16.407962	902.167243	13.579763
16.016299	896.841196	13.584781
15.976587	902.658014	13.589799
16.191642	912.915960	13.594816
16.134219	904.132472	13.599834
16.486554	911.020044	13.604851
16.062783	905.893543	13.609869
16.115369	903.822671	13.614887
16.222917	898.477492	13.619904
16.036074	898.686475	13.624922
16.191319	902.351428	13.629939
15.879004	912.582581	13.634957
15.903433	907.593963	13.639975
16.049472	906.721024	13.644992
16.281316	913.852470	13.650010
16.427245	898.804063	13.655027
16.244762	901.012119	13.660045
16.572476	903.131922	13.665063
16.453048	892.034763	13.670080
16.346169	901.767507	13.675098
16.439094	911.567212	13.680115
16.263056	897.315924	13.685133
16.465429	896.192103	13.690151
16.539248	902.429418	13.695168
16.412787	901.670886	13.700186
16.492580	889.931410	13.705203
16.198283	882.742202	13.710221
16.409520	891.136470	13.715239
16.483343	902.786008	13.720256
16.495021	911.061730	13.725274
16.423940	888.866152	13.730291
16.191678	923.148619	13.735309
16.545249	921.470118	13.740327
16.754872	923.067941	13.745344
16.717254	927.623320	13.750362
16.747958	921.414279	13.755379
16.769863	928.856343	13.760397
16.944066	930.890228	13.765415
16.678920	921.286646	13.770432
16.744462	919.985388	13.775450
16.538524	917.888654	13.780467
16.590766	915.062121	13.785485
16.900935	914.443187	13.790503
16.975159	926.122197	13.795520
16.753609	925.049343	13.800538
16.591457	924.819904	13.805555
16.439016	939.199991	13.810573
16.519990	917.066230	13.815591
16.729551	931.824367	13.820608
16.643135	924.258153	13.825626
16.938231	925.439884	13.830643
16.533860	926.297164	13.835661
16.651925	935.937060	13.840679
16.868239	927.713977	13.845696
16.807360	938.828560	13.850714
16.823203	931.548419	13.855731
16.856372	960.172949	13.860749
17.187072	952.670235	13.865767
16.848593	951.862311	13.870784
17.068663	974.604575	13.875802
17.286728	950.343213	13.880819
17.140467	964.283238	13.885837
17.042858	927.139974	13.890855
16.864562	944.677491	13.895872
16.804982	949.998423	13.900890
17.338513	962.202192	13.905907
17.121448	964.531692	13.910925
17.068830	968.547864	13.915943
17.095030	981.911802	13.920960
17.128677	966.143385	13.925978
17.260782	981.284555	13.930995
17.188675	968.293468	13.936013
17.407612	972.034800	13.941031
17.319085	972.128544	13.946048
17.223413	968.386618	13.951066
17.610515	957.343561	13.956083
17.036404	978.558434	13.961101
17.240974	972.830552	13.966119
17.534273	961.437238	13.971136
17.297572	968.018738	13.976154
17.467755	967.859149	13.981171
17.456195	974.368315	13.986189
17.710032	966.667817	13.991207
17.676606	969.016169	13.996224
17.502918	969.690580	14.001242
17.729095	965.331037	14.006259
17.052299	956.623212	14.011277
17.353509	960.654019	14.016295
17.558273	965.789081	14.021312
17.400621	984.557377	14.026330
17.629042	967.873718	14.031347
17.668290	975.813308	14.036365
17.917155	974.689965	14.041383
17.601973	971.729309	14.046400
17.395083	979.043009	14.051418
17.749230	971.395205	14.056435
17.419803	976.631935	14.061453
17.443035	974.094466	14.066471
17.643531	970.398059	14.071488
17.609121	974.874200	14.076506
17.721961	973.306031	14.081523
17.420431	972.292246	14.086541
17.576139	970.158567	14.091559
17.567794	963.191288	14.096576
17.251555	974.584655	14.101594
17.606647	972.198984	14.106611
17.582016	983.532456	14.111629
17.753199	990.143778	14.116647
17.649794	1017.241857	14.121664
17.389781	1008.784730	14.126682
17.690463	998.316714	14.131699
17.522277	1014.241420	14.136717
17.546830	1008.745392	14.141735
17.332551	1014.822443	14.146752
17.389269	1010.953477	14.151770
17.779869	1041.146940	14.156787
17.980105	1025.413809	14.161805
17.607288	1037.106364	14.166823
17.815890	1036.746771	14.171840
17.447393	1054.006374	14.176858
17.866184	1032.242991	14.181875
17.870260	1050.762056	14.186893
18.120388	1038.800466	14.191911
18.014927	1052.120786	14.196928
17.872116	1060.514913	14.201946
18.121333	1076.708810	14.206963
18.215814	1055.146790	14.211981
18.075671	1072.565970	14.216999
18.459325	1057.506559	14.222016
18.056867	1079.365875	14.227034
18.411454	1062.130190	14.232051
18.212885	1070.538555	14.237069
18.090375	1069.529914	14.242087
18.075184	1059.229090	14.247104
18.135624	1061.833827	14.252122
18.369914	1058.570389	14.257139
18.483285	1062.572931	14.262157
18.278447	1065.181262	14.267175
18.508416	1067.190403	14.272192
18.163173	1069.295589	14.277210
18.406368	1067.840875	14.282227
18.303223	1078.288690	14.287245
18.290960	1075.026536	14.292263
18.289126	1074.131580	14.297280
17.971984	1078.284979	14.302298
18.142525	1075.031877	14.307315
18.349975	1086.298533	14.312333
18.414028	1092.672055	14.317351
18.827015	1109.349036	14.322368
18.507895	1105.340828	14.327386
18.772632	1104.713652	14.332403
18.669590	1121.380476	14.337421
18.545479	1085.821936	14.342439
18.812284	1094.812697	14.347456
18.798139	1094.082630	14.352474
18.551797	1077.341125	14.357491
18.970338	1083.053152	14.362509
18.674955	1073.677548	14.367527
18.840251	1069.130053	14.372544
18.708629	1066.626918	14.377562
19.001754	1069.205896	14.382579
19.018173	1070.616426	14.387597
18.794915	1071.809246	14.392615
18.907474	1062.698729	14.397632
18.736358	1075.092252	14.402650
19.016420	1072.601966	14.407667
19.066856	1058.488846	14.412685
18.891637	1073.274104	14.417703
18.891710	1059.290242	14.422720
19.018596	1064.490065	14.427738
18.763346	1057.101257	14.432755
18.652529	1073.754358	14.437773
18.528340	1067.638065	14.442791
18.743042	1087.043109	14.447808
19.049696	1096.216511	14.452826
19.197842	1092.473130	14.457843
19.047514	1093.769127	14.462861
19.076831	1102.092320	14.467879
19.243954	1092.865117	14.472896
19.037643	1105.671273	14.477914
19.263023	1101.567374	14.482931
18.985034	1111.417090	14.487949
19.007878	1098.312684	14.492967
19.137621	1097.589637	14.497984
19.099974	1103.145523	14.503002
19.133015	1097.221194	14.508019
19.322638	1104.901605	14.513037
19.289840	1097.372497	14.518055
19.469686	1099.785796	14.523072
19.561759	1102.591168	14.528090
19.321965	1099.513034	14.533107
19.273507	1104.874789	14.538125
19.225810	1101.432408	14.543143
19.459778	1098.979552	14.548160
19.209750	1111.087101	14.553178
19.233738	1103.261862	14.558195
19.335748	1091.010315	14.563213
19.209447	1104.031540	14.568231
19.767110	1092.112368	14.573248
19.433331	1114.775939	14.578266
19.510023	1094.987054	14.583283
19.665150	1082.580314	14.588301
19.420907	1100.266669	14.593319
19.491316	1087.447650	14.598336
19.433715	1103.473828	14.603354
19.593325	1100.849052	14.608371
19.425964	1097.670976	14.613389
19.168580	1112.956940	14.618407
19.265719	1094.698564	14.623424
19.370459	1118.792167	14.628442
19.533245	1126.973660	14.633459
19.664823	1130.484250	14.638477
19.586467	1118.035378	14.643495
19.929768	1129.696151	14.648512
19.820273	1126.177875	14.653530
19.656049	1130.995617	14.658547
19.920661	1118.448834	14.663565
20.025524	1132.794649	14.668583
19.717392	1114.364798	14.673600
19.711656	1115.557786	14.678618
19.654061	1122.969884	14.683635
19.995386	1117.862405	14.688653
19.761484	1123.386476	14.693671
19.967039	1116.171919	14.698688
20.044355	1121.257049	14.703706
20.086990	1117.051094	14.708723
19.919849	1117.045062	14.713741
19.594247	1126.681450	14.718759
19.612771	1121.714107	14.723776
19.941811	1119.921950	14.728794
19.955631	1125.908605	14.733811
19.970790	1105.640621	14.738829
19.972487	1137.008517	14.743847
20.179749	1146.650730	14.748864
20.166829	1155.539955	14.753882
20.104674	1154.878926	14.758899
20.227720	1154.744346	14.763917
20.233063	1161.142162	14.768935
20.417694	1141.644755	14.773952
20.345905	1162.275114	14.778970
20.168871	1150.482826	14.783987
20.650692	1144.789161	14.789005
20.250150	1155.132473	14.794023
20.417346	1148.027268	14.799040
20.136566	1138.516564	14.804058
20.273020	1154.721307	14.809075
20.684181	1150.266491	14.814093
20.361137	1164.311092	14.819111
20.290778	1148.986741	14.824128
20.348835	1158.390492	14.829146
20.462719	1156.836203	14.834163
20.457428	1148.429598	14.839181
20.207754	1164.144061	14.844199
20.201279	1157.530141	14.849216
20.394294	1147.322674	14.854234
20.271027	1158.296089	14.859251
20.694330	1155.204005	14.864269
20.263611	1156.446073	14.869287
20.323652	1163.161644	14.874304
20.276126	1153.724562	14.879322
20.546559	1160.088999	14.884339
20.633085	1168.430916	14.889357
20.609575	1179.342202	14.894375
20.625851	1186.388661	14.899392
20.695290	1188.107689	14.904410
20.532393	1192.507414	14.909427
20.976626	1182.568177	14.914445
20.542946	1196.263854	14.919463
20.771351	1187.897032	14.924480
20.941121	1193.148460	14.929498
20.508891	1200.185208	14.934515
20.968993	1204.769117	14.939533
20.620997	1197.971223	14.944551
20.825397	1181.669167	14.949568
20.956633	1188.887235	14.954586
20.700139	1176.685617	14.959603
21.119214	1174.901502	14.964621
21.016816	1176.884994	14.969639
20.872215	1173.325867	14.974656
20.650823	1170.411567	14.979674
20.489410	1184.675677	14.984691
20.894809	1181.618724	14.989709
20.695085	1213.768316	14.994727
21.277063	1223.028153	14.999744
21.524147	1215.685258	15.004762
21.424427	1216.798729	15.009779
21.842273	1209.867967	15.014797
21.285268	1196.855959	15.019815
21.299047	1185.374354	15.024832
21.259895	1171.852375	15.029850
21.079501	1198.300561	15.034867
21.378251	1167.500360	15.039885
21.041667	1189.627130	15.044903
21.451619	1195.612111	15.049920
21.723429	1189.694142	15.054938
21.332257	1197.311270	15.059955
21.501737	1162.522249	15.064973
21.070313	1181.723439	15.069991
21.034113	1173.930251	15.075008
21.576796	1185.035698	15.080026
21.568005	1199.143626	15.085043
21.844701	1190.285273	15.090061
21.452764	1209.899069	15.095079
21.680410	1189.297009	15.100096
21.697623	1207.992398	15.105114
21.657662	1201.115552	15.110131
21.629983	1190.612125	15.115149
21.760990	1199.452004	15.120167
21.773046	1183.248746	15.125184
21.093237	1180.995894	15.130202
21.353521	1190.946228	15.135219
21.815200	1191.549890	15.140237
21.715126	1192.561178	15.145255
21.789797	1195.279700	15.150272
21.965557	1198.149786	15.155290
21.908628	1199.132885	15.160307
22.172299	1201.085305	15.165325
22.067814	1201.448752	15.170343
21.831535	1188.256807	15.175360
21.842752	1168.863499	15.180378
21.823534	1191.120260	15.185395
21.861078	1200.685757	15.190413
21.606881	1202.850011	15.195431
21.575498	1203.694668	15.200448
21.812861	1217.138061	15.205466
21.836882	1210.218656	15.210483
22.023413	1206.651440	15.215501
21.945061	1202.161884	15.220519
22.093845	1200.643546	15.225536
21.886077	1215.971696	15.230554
21.916306	1193.909391	15.235571
22.099872	1208.220818	15.240589
22.102801	1197.877053	15.245607
21.960086	1211.220987	15.250624
22.168443	1207.733019	15.255642
21.941086	1198.874320	15.260659
22.003886	1225.634938	15.265677
22.302441	1229.875952	15.270695
22.612691	1236.161318	15.275712
22.563977	1223.102186	15.280730
22.119153	1212.878264	15.285747
22.467179	1217.707221	15.290765
22.271271	1199.765396	15.295783
22.065972	1224.102582	15.300800
22.766977	1228.017795	15.305818
22.542653	1217.431519	15.310835
22.675496	1215.522499	15.315853
22.416855	1207.525264	15.320871
22.205637	1193.655510	15.325888
22.581137	1214.550425	15.330906
22.614706	1218.344494	15.335923
22.826074	1228.146476	15.340941
22.516056	1227.549434	15.345959
22.777514	1229.668720	15.350976
23.040541	1196.579910	15.355994
22.695605	1210.319581	15.361011
22.520675	1199.160324	15.366029
22.413892	1199.180333	15.371047
22.748125	1205.145752	15.376064
22.771497	1210.046860	15.381082
23.025477	1222.859113	15.386099
22.694805	1206.380952	15.391117
22.727401	1208.144645	15.396135
22.512558	1213.153708	15.401152
22.826086	1225.309421	15.406170
22.825697	1223.818685	15.411187
22.678551	1219.013206	15.416205
22.219143	1228.017196	15.421223
22.609137	1229.819442	15.426240
22.959371	1224.929402	15.431258
22.727245	1229.032677	15.436275
22.701872	1236.071183	15.441293
22.758207	1231.828098	15.446311
22.898056	1253.091954	15.451328
23.068756	1262.036604	15.456346
23.088101	1267.302584	15.461363
23.205421	1261.182316	15.466381
23.357719	1263.584253	15.471399
23.523962	1259.201764	15.476416
23.582706	1248.121938	15.481434
22.963657	1236.990982	15.486451
23.373477	1235.531052	15.491469
23.283817	1222.674805	15.496487
23.379486	1230.554328	15.501504
23.437758	1224.651561	15.506522
23.146812	1214.599602	15.511539
23.253478	1217.609230	15.516557
23.180666	1224.807012	15.521575
23.151986	1230.163181	15.526592
23.434169	1240.406711	15.531610
23.415603	1247.650055	15.536627
23.172220	1260.520623	15.541645
23.294906	1251.690147	15.546663
23.236414	1261.414925	15.551680
23.581642	1254.229571	15.556698
23.246950	1244.797380	15.561715
23.474966	1265.712310	15.566733
23.387174	1257.994914	15.571751
23.017259	1258.899555	15.576768
23.531723	1249.657956	15.581786
23.368774	1267.838139	15.586803
23.427697	1259.993565	15.591821
23.729888	1273.391262	15.596839
23.918781	1268.797201	15.601856
23.823461	1271.211032	15.606874
23.803528	1283.393460	15.611891
24.113600	1263.497005	15.616909
23.968336	1275.600262	15.621927
23.494855	1275.958269	15.626944
23.938996	1257.244609	15.631962
23.953140	1275.170881	15.636979
24.312201	1267.110598	15.641997
23.778204	1265.446291	15.647015
23.806699	1273.104510	15.652032
24.255013	1272.930443	15.657050
24.034404	1272.648665	15.662067
24.231884	1255.682570	15.667085
24.296345	1259.208612	15.672103
23.965317	1242.947645	15.677120
24.370473	1242.184292	15.682138
24.046153	1243.489867	15.687155
23.729178	1240.999524	15.692173
24.163292	1252.777833	15.697191
24.137509	1265.855401	15.702208
24.302209	1275.287161	15.707226
24.377068	1275.810494	15.712243
24.347833	1281.687915	15.717261
24.607085	1268.028171	15.722279
24.386064	1272.832711	15.727296
24.442882	1242.359186	15.732314
23.970493	1256.361146	15.737331
24.086712	1261.473056	15.742349
24.302700	1266.188250	15.747367
24.267640	1277.704921	15.752384
24.285061	1262.297166	15.757402
24.425599	1272.001458	15.762419
24.205297	1272.210759	15.767437
24.329583	1281.675278	15.772455
24.230919	1269.709944	15.777472
24.256688	1267.791256	15.782490
24.395374	1267.232532	15.787507
24.221364	1297.390509	15.792525
24.926517	1303.001427	15.797543
24.557464	1308.014849	15.802560
25.023459	1305.598204	15.807578
24.656663	1302.089740	15.812595
24.366086	1310.600922	15.817613
24.832313	1305.920770	15.822631
24.594672	1310.406191	15.827648
24.589655	1295.208758	15.832666
24.640238	1306.374857	15.837683
24.694823	1295.222767	15.842701
24.717542	1303.663768	15.847719
24.854505	1303.483786	15.852736
24.984210	1309.519850	15.857754
24.691558	1303.004233	15.862771
24.873874	1309.971352	15.867789
25.238383	1308.320819	15.872807
24.777870	1316.757060	15.877824
24.818621	1306.482840	15.882842
24.800778	1304.344832	15.887859
24.974165	1333.126668	15.892877
25.191270	1330.733636	15.897895
25.307750	1330.351967	15.902912
25.578681	1327.685925	15.907930
24.900286	1324.224129	15.912947
25.059777	1336.130054	15.917965
25.382605	1331.015526	15.922983
25.212937	1328.135452	15.928000
25.313662	1329.630575	15.933018
25.300643	1334.208283	15.938035
25.348443	1325.047106	15.943053
25.357200	1326.593247	15.948071
25.320257	1313.548920	15.953088
25.706110	1313.349356	15.958106
25.663769	1323.465117	15.963123
25.635594	1322.954238	15.968141
25.854021	1302.622388	15.973159
25.375919	1309.018683	15.978176
25.271130	1296.769167	15.983194
25.695499	1304.512929	15.988211
25.767551	1315.664662	15.993229
25.833462	1312.532715	15.998247
25.173059	1306.033000	16.003264
25.176133	1319.376748	16.008282
25.457670	1319.767131	16.013299
25.317664	1336.970790	16.018317
25.660718	1311.411616	16.023335
25.361373	1323.960359	16.028352
25.332238	1329.685945	16.033370
25.699053	1336.975362	16.038387
25.802373	1353.983055	16.043405
25.901821	1345.937590	16.048423
26.031369	1359.863193	16.053440
26.064170	1362.911035	16.058458
25.959109	1358.723026	16.063475
25.939439	1360.627136	16.068493
26.201883	1340.222622	16.073511
26.021785	1371.633834	16.078528
26.223119	1338.630094	16.083546
26.267865	1351.948189	16.088563
25.998237	1337.319426	16.093581
26.124920	1335.185475	16.098599
26.173273	1339.850264	16.103616
26.319295	1338.060284	16.108634
26.338922	1344.811249	16.113651
25.743553	1327.429865	16.118669
26.295715	1335.351593	16.123687
26.279403	1346.192925	16.128704
26.176440	1352.852072	16.133722
26.142899	1331.466102	16.138739
26.313402	1353.145803	16.143757
26.548551	1337.758769	16.148775
26.254905	1351.553068	16.153792
26.423035	1345.270467	16.158810
26.363031	1347.405305	16.163827
26.494205	1356.635812	16.168845
26.381561	1342.581067	16.173863
26.292645	1350.269847	16.178880
26.472576	1350.970559	16.183898
26.634411	1338.290419	16.188915
26.647851	1358.558904	16.193933
26.801304	1338.816355	16.198951
26.300841	1356.137959	16.203968
26.325267	1337.767716	16.208986
26.906431	1354.344846	16.214003
26.386917	1346.980283	16.219021
26.723022	1346.296924	16.224039
26.653354	1349.365436	16.229056
26.742099	1369.650520	16.234074
27.238035	1364.272876	16.239091
26.886171	1376.703992	16.244109
27.041063	1359.880321	16.249127
26.804470	1363.092342	16.254144
26.968115	1350.219513	16.259162
27.073942	1357.691804	16.264179
26.938526	1374.315249	16.269197
27.018583	1367.601229	16.274215
26.869133	1370.424424	16.279232
26.953375	1365.338489	16.284250
27.174475	1367.096140	16.289267
27.213879	1381.176885	16.294285
27.249594	1367.058435	16.299303
27.074313	1380.968996	16.304320
27.198511	1368.894623	16.309338
27.260846	1367.037877	16.314355
27.481051	1377.483235	16.319373
27.719030	1354.943056	16.324391
27.416625	1375.629526	16.329408
27.486457	1357.951405	16.334426
27.594837	1350.718652	16.339443
27.277517	1338.540733	16.344461
27.548102	1339.911252	16.349479
27.390509	1346.783414	16.354496
27.427470	1341.615163	16.359514
27.675248	1347.897123	16.364531
27.604163	1361.719793	16.369549
27.605631	1335.420847	16.374567
27.341350	1344.245840	16.379584
27.613050	1347.750643	16.384602
27.406246	1364.796513	16.389619
27.106858	1368.801122	16.394637
27.579748	1374.435887	16.399655
27.516886	1368.786202	16.404672
27.529428	1368.421708	16.409690
27.701808	1369.728851	16.414707
27.743179	1384.016019	16.419725
27.790653	1365.469039	16.424743
27.778834	1375.877068	16.429760
27.498071	1372.698191	16.434778
27.483031	1370.456387	16.439795
27.610171	1388.349454	16.444813
27.740439	1398.635515	16.449831
27.770523	1401.656064	16.454848
27.954805	1408.517612	16.459866
28.365341	1398.023002	16.464883
28.104807	1400.849899	16.469901
28.269606	1396.429036	16.474919
28.480717	1404.717233	16.479936
28.572818	1411.313663	16.484954
28.302346	1396.683311	16.489971
28.161421	1409.539630	16.494989
28.413437	1400.477603	16.500007
28.231917	1403.757876	16.505024
28.197847	1392.414999	16.510042
28.217807	1402.486960	16.515059
28.496504	1404.636782	16.520077
28.677605	1398.468820	16.525095
28.837972	1397.896570	16.530112
28.265671	1394.320986	16.535130
28.502778	1382.666331	16.540147
28.477413	1393.198238	16.545165
28.470414	1398.853867	16.550183
28.290312	1392.973012	16.555200
28.158840	1397.562737	16.560218
28.357424	1386.898876	16.565235
28.204375	1392.622725	16.570253
28.565583	1389.928764	16.575271
28.677719	1395.175420	16.580288
28.447196	1393.968807	16.585306
28.209511	1388.632491	16.590323
28.289294	1406.560664	16.595341
28.565904	1410.597035	16.600359
28.748094	1421.267456	16.605376
28.708945	1413.476504	16.610394
29.082156	1413.317406	16.615411
28.894308	1419.490620	16.620429
29.042038	1415.432336	16.625447
28.995637	1419.267028	16.630464
29.214821	1420.106894	16.635482
29.248051	1417.405137	16.640499
29.258431	1404.696734	16.645517
29.110072	1417.021333	16.650535
29.389219	1398.409359	16.655552
29.310946	1415.153593	16.660570
29.333561	1398.251762	16.665587
29.272637	1409.746926	16.670605
29.117472	1401.144821	16.675623
29.440885	1405.991289	16.680640
29.453153	1404.768267	16.685658
29.635651	1403.815473	16.690675
29.026766	1399.246741	16.695693
29.549503	1392.159028	16.700711
29.588439	1387.186553	16.705728
29.456053	1377.222136	16.710746
29.463269	1374.726314	16.715763
29.410720	1389.789570	16.720781
29.362810	1391.127905	16.725799
29.654433	1402.704633	16.730816
29.736222	1407.073232	16.735834
29.719955	1398.719965	16.740851
29.304654	1387.725662	16.745869
29.671323	1415.012252	16.750887
29.870711	1412.056904	16.755904
29.566072	1415.404760	16.760922
29.695965	1405.860659	16.765939
29.634124	1414.282238	16.770957
29.776702	1402.730671	16.775975
29.372809	1403.777618	16.780992
29.227022	1404.873229	16.786010
29.818358	1393.301432	16.791027
29.433359	1401.102935	16.796045
29.651579	1399.259096	16.801063
29.803243	1419.525287	16.806080
29.699861	1416.934374	16.811098
30.244332	1436.209396	16.816115
30.207635	1433.947642	16.821133
29.931483	1434.932938	16.826151
30.502085	1432.466218	16.831168
30.126989	1435.779867	16.836186
30.497386	1436.701414	16.841203
30.178848	1434.328890	16.846221
30.467601	1435.910838	16.851239
30.365245	1443.559179	16.856256
30.399163	1428.020606	16.861274
30.486994	1422.918510	16.866291
29.932969	1410.132056	16.871309
29.919838	1428.266415	16.876327
30.532448	1425.266195	16.881344
30.217396	1425.581786	16.886362
30.519019	1422.646048	16.891379
30.146065	1430.682728	16.896397
30.263171	1429.356472	16.901415
30.480705	1430.784969	16.906432
30.277190	1432.006337	16.911450
30.436754	1432.015294	16.916467
30.684028	1435.560662	16.921485
30.457017	1433.810276	16.926503
30.560188	1430.966277	16.931520
30.523052	1471.445314	16.936538
30.792381	1456.874384	16.941555
30.705810	1462.920273	16.946573
30.931053	1458.088012	16.951591
30.967669	1459.819580	16.956608
30.985006	1456.971163	16.961626
31.062011	1457.752459	16.966643
31.103315	1459.075269	16.971661
31.005686	1466.892095	16.976679
31.276173	1463.637549	16.981696
31.066081	1456.970849	16.986714
31.305255	1465.777656	16.991731
31.217685	1453.892413	16.996749
31.256715	1457.383933	17.001767
30.949699	1432.771374	17.006784
31.076266	1455.363602	17.011802
31.594186	1459.089889	17.016819
31.503183	1458.142437	17.021837
30.902398	1447.028874	17.026855
31.046805	1445.777910	17.031872
31.091072	1454.403483	17.036890
31.232866	1465.081596	17.041907
31.302224	1454.817211	17.046925
31.155971	1459.486054	17.051943
31.292134	1462.437323	17.056960
31.296053	1461.112844	17.061978
31.231914	1453.889758	17.066995
31.614434	1458.122471	17.072013
31.238687	1462.736938	17.077031
31.997461	1464.606981	17.082048
31.899871	1470.451587	17.087066
31.913598	1457.455444	17.092083
31.708005	1453.214451	17.097101
31.602473	1454.198416	17.102119
31.518738	1460.408759	17.107136
31.557897	1463.068744	17.112154
31.857024	1479.217623	17.117171
31.606333	1480.511443	17.122189
31.765353	1483.896051	17.127207
31.911120	1476.761270	17.132224
32.106709	1481.160679	17.137242
32.144039	1484.678957	17.142259
32.256269	1464.284833	17.147277
31.806398	1482.708807	17.152295
32.277420	1464.415559	17.157312
31.936016	1489.672613	17.162330
32.243744	1477.489495	17.167347
31.967639	1480.630823	17.172365
31.830478	1482.360311	17.177383
31.999096	1462.277866	17.182400
31.696504	1485.149874	17.187418
32.193720	1488.692031	17.192435
32.495584	1508.027804	17.197453
32.668009	1520.748690	17.202471
32.740952	1503.459568	17.207488
32.655011	1496.435003	17.212506
32.232172	1477.406282	17.217523
32.522500	1480.431958	17.222541
32.370420	1475.120038	17.227559
32.591569	1493.070413	17.232576
32.572855	1514.562369	17.237594
32.842564	1505.159534	17.242611
32.640619	1497.940111	17.247629
32.708371	1497.760543	17.252647
33.005854	1491.221417	17.257664
32.466358	1498.804852	17.262682
32.380757	1507.523949	17.267699
33.046160	1499.457398	17.272717
32.824651	1516.460895	17.277735
33.081980	1502.864239	17.282752
32.890259	1506.293630	17.287770
33.163029	1501.177773	17.292787
33.051179	1518.109322	17.297805
33.139197	1505.711756	17.302823
33.447919	1507.645750	17.307840
33.214467	1491.105358	17.312858
33.134106	1479.131914	17.317875
33.196948	1467.584324	17.322893
33.103409	1475.898700	17.327911
33.052798	1462.840267	17.332928
33.063611	1487.090395	17.337946
33.413706	1481.167151	17.342963
33.778883	1489.688737	17.347981
33.128677	1490.645911	17.352999
33.002248	1482.170086	17.358016
33.182432	1495.567870	17.363034
33.138474	1491.555612	17.368051
33.579810	1490.194957	17.373069
33.247005	1501.462443	17.378087
33.029872	1496.534711	17.383104
32.955918	1492.706014	17.388122
32.688353	1501.712999	17.393139
33.424226	1527.133841	17.398157
33.467758	1523.486269	17.403175
33.634896	1517.443672	17.408192
33.523093	1509.439429	17.413210
33.624542	1528.013338	17.418227
33.575909	1507.814603	17.423245
33.680210	1535.138371	17.428263
34.345864	1528.930822	17.433280
34.115006	1529.495438	17.438298
33.810125	1523.316913	17.443315
34.339450	1508.499565	17.448333
34.004834	1522.827842	17.453351
34.127836	1510.022016	17.458368
34.227365	1505.368062	17.463386
34.048950	1511.584922	17.468403
34.060610	1503.312496	17.473421
33.944128	1517.380259	17.478439
33.980446	1506.174255	17.483456
34.166477	1540.042098	17.488474
33.810971	1547.769622	17.493491
34.286833	1546.058938	17.498509
34.333539	1543.659494	17.503527
34.235812	1551.304958	17.508544
34.307872	1554.161842	17.513562
34.274544	1556.676276	17.518579
34.896222	1531.671254	17.523597
34.466423	1543.580456	17.528615
34.589331	1547.494755	17.533632
34.424785	1535.884516	17.538650
34.066526	1548.102501	17.543667
34.775241	1533.393250	17.548685
34.917156	1546.442950	17.553703
34.750265	1547.629638	17.558720
34.833936	1538.633335	17.563738
34.745507	1542.708517	17.568755
34.953856	1531.285817	17.573773
34.738771	1551.942252	17.578791
34.911751	1524.934955	17.583808
35.046458	1547.311549	17.588826
34.818956	1541.196591	17.593843
34.913153	1534.738768	17.598861
34.529591	1535.564791	17.603879
35.083119	1549.427683	17.608896
35.042315	1570.918547	17.613914
34.901131	1575.552146	17.618931
35.232282	1567.416119	17.623949
35.093661	1576.772824	17.628967
35.300085	1550.735836	17.633984
34.973500	1569.469491	17.639002
35.347119	1576.999187	17.644019
35.669098	1574.471980	17.649037
35.261608	1580.310865	17.654055
35.430724	1566.810309	17.659072
35.654106	1567.356834	17.664090
35.488558	1567.465081	17.669107
35.870032	1565.326877	17.674125
35.689334	1553.324494	17.679143
35.579230	1562.506926	17.684160
35.560495	1551.516244	17.689178
35.546703	1560.451410	17.694195
35.859234	1552.157182	17.699213
35.554842	1560.853326	17.704231
35.330396	1552.975429	17.709248
35.616669	1562.789849	17.714266
35.625214	1551.268685	17.719283
35.940413	1566.985858	17.724301
35.682157	1555.824170	17.729319
35.394312	1570.050194	17.734336
35.788182	1564.750361	17.739354
35.690756	1584.050663	17.744371
36.157876	1586.030522	17.749389
36.001535	1600.877526	17.754407
36.188245	1595.466966	17.759424
36.444847	1595.409897	17.764442
36.119992	1602.275374	17.769459
36.225696	1592.409729	17.774477
36.349280	1598.169613	17.779495
36.195919	1592.244309	17.784512
36.459762	1585.359889	17.789530
36.373829	1593.941324	17.794547
36.580423	1580.080009	17.799565
36.440200	1598.557849	17.804583
36.470048	1585.999394	17.809600
36.347857	1584.486733	17.814618
36.410353	1582.071782	17.819635
36.687061	1581.516610	17.824653
36.475002	1597.585265	17.829671
36.346869	1584.036494	17.834688
36.354614	1585.203772	17.839706
36.249651	1588.827757	17.844723
36.910684	1579.116753	17.849741
36.414369	1582.462273	17.854759
36.637657	1575.502293	17.859776
36.769614	1582.602933	17.864794
36.683505	1604.838974	17.869811
37.319172	1614.756284	17.874829
36.926681	1607.743557	17.879847
37.208702	1609.022958	17.884864
37.266274	1606.100555	17.889882
36.795878	1596.630052	17.894899
37.103436	1589.500167	17.899917
36.964875	1607.051851	17.904935
36.871279	1608.753685	17.909952
37.408488	1618.664636	17.914970
36.897436	1620.109444	17.919987
37.106999	1617.051412	17.925005
37.214485	1622.338374	17.930023
37.210075	1620.883296	17.935040
37.256614	1604.711485	17.940058
37.324238	1618.754426	17.945075
37.605641	1611.407540	17.950093
37.187997	1614.453314	17.955111
37.219572	1612.985893	17.960128
37.537146	1621.920554	17.965146
37.473387	1631.650079	17.970163
37.657708	1626.672985	17.975181
37.793048	1638.211362	17.980199
37.990045	1635.706275	17.985216
38.128688	1621.519803	17.990234
37.893461	1619.133383	17.995251
37.966364	1607.009044	18.000269
38.355978	1598.283635	18.005287
37.810219	1605.768276	18.010304
38.365205	1582.373078	18.015322
37.816063	1606.777732	18.020339
38.093808	1580.110038	18.025357
38.365532	1589.342847	18.030375
37.966321	1586.452341	18.035392
38.147684	1587.234013	18.040410
37.951172	1587.711573	18.045427
37.973107	1596.068138	18.050445
38.092607	1601.005345	18.055463
38.194952	1623.326387	18.060480
38.441088	1631.800712	18.065498
38.625025	1628.044594	18.070515
38.539654	1634.497355	18.075533
38.390051	1620.006230	18.080551
38.437310	1634.302893	18.085568
38.609596	1618.872237	18.090586
38.277916	1634.478219	18.095603
38.406288	1626.929103	18.100621
38.457008	1626.738277	18.105639
38.410659	1634.315364	18.110656
38.354651	1620.187335	18.115674
38.512323	1633.274753	18.120691
38.643172	1618.146851	18.125709
38.660068	1630.631576	18.130727
38.279711	1654.004186	18.135744
38.897864	1660.182261	18.140762
38.425474	1664.247026	18.145779
38.715251	1664.615786	18.150797
38.794140	1660.634943	18.155815
38.572227	1669.314762	18.160832
38.843683	1657.278412	18.165850
38.891788	1683.682293	18.170867
39.221106	1682.160249	18.175885
39.641483	1674.006272	18.180903
39.262820	1681.420331	18.185920
40.011488	1674.746144	18.190938
39.910430	1654.279852	18.195955
39.972185	1647.570309	18.200973
39.968381	1641.053553	18.205991
39.748487	1645.714548	18.211008
40.003168	1642.521127	18.216026
39.714931	1627.683688	18.221043
39.764162	1613.810167	18.226061
39.334346	1596.718864	18.231079
39.224350	1614.022775	18.236096
39.759338	1630.178398	18.241114
39.574434	1638.250138	18.246131
39.650479	1643.360156	18.251149
39.687386	1644.014847	18.256167
39.423263	1639.504102	18.261184
39.410228	1637.726695	18.266202
39.226487	1627.459936	18.271219
39.367566	1639.550601	18.276237
39.450421	1656.975611	18.281255
39.767653	1675.361117	18.286272
39.908916	1660.394706	18.291290
39.737674	1680.599767	18.296307
39.815469	1673.814545	18.301325
39.897469	1674.046613	18.306343
40.010518	1685.891110	18.311360
40.523198	1698.234226	18.316378
40.548761	1717.989375	18.321395
40.767071	1693.398025	18.326413
40.800032	1674.847755	18.331431
40.455973	1674.774718	18.336448
40.773409	1659.381734	18.341466
40.626210	1661.008395	18.346483
40.499910	1658.066378	18.351501
40.345326	1652.076305	18.356519
40.256912	1663.775572	18.361536
40.616590	1665.348185	18.366554
40.526269	1668.462587	18.371571
40.462749	1682.609526	18.376589
40.765227	1690.517499	18.381607
40.489911	1697.224959	18.386624
40.687302	1683.924999	18.391642
40.888887	1690.730282	18.396659
40.885930	1693.449521	18.401677
40.980931	1702.354981	18.406695
41.000973	1693.178589	18.411712
41.283751	1699.695414	18.416730
40.998035	1703.032136	18.421747
40.801038	1698.501718	18.426765
41.149954	1688.011683	18.431783
41.122689	1691.857943	18.436800
41.487122	1699.936944	18.441818
41.370467	1706.608053	18.446835
41.096740	1697.516124	18.451853
41.531636	1691.280518	18.456871
41.347812	1702.813040	18.461888
41.278849	1698.748670	18.466906
41.677799	1715.098385	18.471923
41.370422	1729.576555	18.476941
41.849539	1727.428196	18.481959
41.653339	1736.991326	18.486976
41.986032	1723.987610	18.491994
41.774393	1712.630935	18.497011
41.651232	1712.583290	18.502029
41.924627	1725.349163	18.507047
41.691699	1725.209541	18.512064
41.656726	1726.706169	18.517082
41.685391	1715.622906	18.522099
41.611952	1729.497074	18.527117
42.000292	1719.525694	18.532135
41.981782	1727.639163	18.537152
42.145964	1704.727474	18.542170
41.850027	1726.736413	18.547187
41.768759	1712.942723	18.552205
41.906764	1735.750065	18.557223
42.355825	1741.528151	18.562240
42.230667	1755.024842	18.567258
42.191765	1750.361021	18.572275
42.193982	1762.773491	18.577293
42.487571	1750.044077	18.582311
42.481679	1770.917169	18.587328
42.455514	1757.156255	18.592346
42.208768	1760.099714	18.597363
42.300204	1772.177726	18.602381
42.811472	1759.891962	18.607399
42.416025	1754.789422	18.612416
42.511157	1752.660923	18.617434
42.594168	1759.013877	18.622451
42.404808	1743.546521	18.627469
42.679907	1763.934278	18.632487
42.627223	1770.269609	18.637504
42.848813	1789.485861	18.642522
42.777253	1779.472456	18.647539
42.705074	1783.148932	18.652557
43.291025	1789.368497	18.657575
43.190564	1786.484280	18.662592
43.093592	1783.732433	18.667610
43.056790	1773.018935	18.672627
43.152847	1776.819742	18.677645
43.554518	1781.403053	18.682663
43.349312	1776.554247	18.687680
43.206854	1781.515122	18.692698
43.400186	1766.719200	18.697715
43.512583	1784.974351	18.702733
43.703276	1763.658278	18.707751
43.469049	1767.076251	18.712768
43.329726	1765.055479	18.717786
43.508439	1769.221783	18.722803
43.618047	1769.068754	18.727821
43.637082	1759.505654	18.732839
43.510527	1782.449288	18.737856
43.661120	1762.596157	18.742874
43.773396	1785.178834	18.747891
43.880302	1782.425474	18.752909
43.916642	1793.822880	18.757927
44.065580	1794.649480	18.762944
44.201283	1784.604870	18.767962
44.379977	1793.902478	18.772979
44.283880	1771.972695	18.777997
43.951022	1759.700175	18.783015
43.850491	1765.210012	18.788032
44.259017	1784.911899	18.793050
44.379657	1789.084263	18.798067
44.223260	1789.979035	18.803085
44.448785	1797.815348	18.808103
44.420964	1785.606450	18.813120
45.018013	1768.325969	18.818138
44.631983	1773.812925	18.823155
44.530407	1751.577049	18.828173
44.470123	1769.108798	18.833191
44.578006	1771.887572	18.838208
44.550011	1779.070041	18.843226
44.568584	1783.595623	18.848243
44.763448	1791.984827	18.853261
44.796909	1773.635300	18.858279
44.711592	1781.914040	18.863296
44.705381	1786.692884	18.868314
44.758786	1778.930044	18.873331
44.413575	1799.079775	18.878349
44.683659	1772.239523	18.883367
44.680327	1786.364507	18.888384
44.560430	1791.887985	18.893402
45.330076	1809.888613	18.898419
45.190076	1812.715838	18.903437
45.170094	1806.163012	18.908455
45.064156	1815.082556	18.913472
45.378429	1801.305393	18.918490
45.533532	1816.701710	18.923507
45.071392	1815.409839	18.928525
45.513333	1823.060527	18.933543
45.279846	1818.660096	18.938560
45.638557	1819.482931	18.943578
45.576284	1804.961059	18.948595
45.504457	1814.159655	18.953613
45.669917	1803.343431	18.958631
45.517134	1820.118921	18.963648
45.586622	1815.084379	18.968666
45.541769	1821.986342	18.973683
45.655108	1814.907836	18.978701
45.948926	1819.053754	18.983719
45.955033	1837.049617	18.988736
45.947049	1837.819884	18.993754
46.024969	1829.574416	18.998771
45.779532	1830.208170	19.003789
46.192673	1836.231061	19.008807
46.349928	1836.891261	19.013824
46.180777	1832.559609	19.018842
46.346289	1836.329271	19.023859
46.087921	1832.646396	19.028877
46.512146	1840.047608	19.033895
46.573987	1838.948617	19.038912
46.120882	1834.164181	19.043930
46.407047	1823.447953	19.048947
46.432988	1837.213195	19.053965
46.640696	1826.463384	19.058983
46.585243	1840.818151	19.064000
46.301566	1838.183157	19.069018
46.584115	1840.916546	19.074035
46.213418	1838.149897	19.079053
46.791621	1842.417691	19.084071
46.618031	1864.258604	19.089088
46.784410	1853.008023	19.094106
47.161122	1869.917380	19.099123
47.044009	1864.206115	19.104141
46.994412	1870.006433	19.109159
47.182792	1856.026150	19.114176
46.693145	1871.538716	19.119194
47.099054	1854.728719	19.124211
47.118564	1868.675135	19.129229
47.197044	1856.075161	19.134247
47.455626	1861.012592	19.139264
47.083533	1860.039534	19.144282
47.476659	1842.835378	19.149299
47.600200	1862.061233	19.154317
47.200411	1847.900257	19.159335
47.489817	1869.256374	19.164352
47.461397	1879.951589	19.169370
48.034925	1888.440837	19.174387
47.717065	1892.006590	19.179405
47.928474	1890.633613	19.184423
48.143900	1895.927631	19.189440
47.908848	1880.184966	19.194458
48.314073	1868.879550	19.199475
47.906482	1861.436113	19.204493
47.984745	1839.602001	19.209511
48.005492	1853.586874	19.214528
47.911534	1848.814229	19.219546
48.261239	1867.753944	19.224563
48.284532	1874.693281	19.229581
48.265242	1884.624732	19.234599
48.479074	1865.874096	19.239616
47.827433	1872.428804	19.244634
48.011973	1871.280504	19.249651
48.001774	1874.770217	19.254669
47.989980	1873.981664	19.259687
47.925283	1868.869496	19.264704
48.290978	1874.420018	19.269722
48.470368	1893.189522	19.274739
48.406188	1898.131987	19.279757
48.449309	1893.519614	19.284775
48.784724	1905.420528	19.289792
48.597663	1909.413995	19.294810
48.916906	1900.231038	19.299827
48.831211	1901.109310	19.304845
48.974751	1903.106474	19.309863
48.992147	1899.216130	19.314880
48.932362	1898.136349	19.319898
49.013546	1880.802338	19.324915
49.027627	1901.381122	19.329933
49.050563	1896.746793	19.334951
49.334361	1887.392666	19.339968
49.064073	1905.269946	19.344986
49.394848	1899.337238	19.350003
49.328883	1895.188183	19.355021
49.254797	1900.475135	19.360039
49.494354	1904.276862	19.365056
49.786179	1917.191594	19.370074
49.626927	1908.377122	19.375091
49.350783	1901.014778	19.380109
49.957612	1925.685708	19.385127
50.159435	1918.120178	19.390144
49.747101	1910.843906	19.395162
49.853648	1902.581760	19.400179
49.799693	1885.655930	19.405197
49.910704	1911.755080	19.410215
49.957889	1919.156250	19.415232
50.406351	1918.541390	19.420250
50.384158	1893.020648	19.425267
49.826093	1899.647485	19.430285
50.073782	1903.243181	19.435303
50.180106	1899.464299	19.440320
50.155625	1918.218224	19.445338
49.995439	1915.918254	19.450355
49.906930	1922.017389	19.455373
50.194879	1915.940106	19.460391
50.351723	1916.272092	19.465408
49.972355	1926.311886	19.470426
50.165143	1910.119618	19.475443
50.514631	1937.365107	19.480461
50.459455	1933.446598	19.485479
50.609931	1935.137951	19.490496
50.730979	1933.278913	19.495514
51.142163	1950.572749	19.500531
51.180181	1939.028020	19.505549
50.904286	1954.238564	19.510567
50.837743	1943.313660	19.515584
50.908965	1943.943209	19.520602
50.731842	1944.671466	19.525619
50.591450	1953.505560	19.530637
50.877430	1949.138318	19.535655
50.955461	1952.202617	19.540672
51.237517	1970.359492	19.545690
51.608877	1969.889239	19.550707
51.445352	1979.979700	19.555725
51.203183	1975.331590	19.560743
51.653746	1966.436186	19.565760
51.549605	1981.554112	19.570778
51.913168	1962.293269	19.575795
51.730593	1973.192240	19.580813
51.821909	1964.098969	19.585831
51.877933	1973.730780	19.590848
52.134778	1964.094795	19.595866
51.469321	1953.945015	19.600883
51.605156	1951.679767	19.605901
51.851266	1965.003300	19.610919
51.886793	1964.883670	19.615936
52.139269	1972.389693	19.620954
52.130097	1954.238004	19.625971
51.974428	1961.032677	19.630989
52.068419	1974.028468	19.636007
52.273344	1955.391380	19.641024
51.978177	1968.237147	19.646042
52.300252	1961.785868	19.651059
52.319132	1971.587861	19.656077
51.991097	1963.140854	19.661095
52.070421	1968.073010	19.666112
51.999122	1982.206258	19.671130
52.532219	1974.190455	19.676147
52.508556	1978.313798	19.681165
52.388882	1998.154815	19.686183
52.895250	1976.442837	19.691200
52.516160	2000.398729	19.696218
52.633993	1995.124882	19.701235
52.698552	1990.229853	19.706253
53.164013	1982.996738	19.711271
52.758193	1993.255966	19.716288
52.584967	1992.220708	19.721306
52.929286	2019.655354	19.726323
53.161363	2005.786984	19.731341
53.193528	2017.774609	19.736359
53.316729	2007.875103	19.741376
53.109673	2019.201108	19.746394
53.403660	2000.477311	19.751411
53.558327	2009.211701	19.756429
53.172218	2000.126454	19.761447
53.389158	1993.251965	19.766464
53.331757	1998.122686	19.771482
53.390851	2005.971849	19.776499
53.569986	2001.863643	19.781517
53.878681	2016.009210	19.786535
53.965300	2022.960783	19.791552
53.928821	2027.693729	19.796570
53.923351	2041.232692	19.801587
54.099543	2028.831351	19.806605
54.030467	2032.582065	19.811623
54.420682	2030.650586	19.816640
54.121700	2033.012183	19.821658
53.877085	2026.007201	19.826675
54.186205	2034.089519	19.831693
54.159882	2038.417022	19.836711
54.200428	2019.854650	19.841728
54.222684	2032.830265	19.846746
54.480407	2023.144599	19.851763
54.378405	2020.035730	19.856781
54.534965	2037.062349	19.861799
54.599967	2020.975811	19.866816
54.234769	2033.762745	19.871834
54.794019	2040.647046	19.876851
55.001619	2042.826816	19.881869
54.855014	2045.767163	19.886887
54.892976	2027.293874	19.891904
54.762249	2048.577375	19.896922
55.016047	2064.288379	19.901939
54.982108	2056.882883	19.906957
54.631940	2062.834895	19.911975
54.933107	2066.391286	19.916992
54.896425	2057.401480	19.922010
55.166137	2055.058098	19.927027
55.461655	2054.422651	19.932045
55.264062	2053.958442	19.937063
55.597201	2058.489494	19.942080
55.299688	2058.940754	19.947098
55.221002	2047.601910	19.952115
55.497068	2047.109319	19.957133
55.115144	2057.498378	19.962151
55.597831	2068.807661	19.967168
55.716054	2079.204420	19.972186
55.541892	2082.771366	19.977203
55.669855	2068.845453	19.982221
55.553521	2085.536778	19.987239
55.799974	2080.497408	19.992256
55.562309	2069.016150	19.997274
55.674791	2085.879172	20.002291
56.065717	2105.830501	20.007309
55.840344	2098.040944	20.012327
56.418942	2103.992315	20.017344
56.305453	2113.821883	20.022362
56.146686	2110.001142	20.027379
56.621840	2090.327179	20.032397
56.315880	2103.894010	20.037415
56.735172	2095.215179	20.042432
56.506414	2104.667402	20.047450
56.761837	2108.037400	20.052467
56.813223	2083.890950	20.057485
56.623119	2099.175829	20.062503
56.723247	2093.632185	20.067520
56.495416	2089.246092	20.072538
56.471609	2106.021737	20.077555
57.173858	2119.100074	20.082573
56.821827	2132.650728	20.087591
57.087777	2131.548198	20.092608
57.202130	2130.593534	20.097626
57.063828	2127.327088	20.102643
57.341810	2111.820606	20.107661
57.221116	2132.565747	20.112679
57.619052	2129.467923	20.117696
57.464678	2130.467579	20.122714
57.413893	2123.717577	20.127731
57.518685	2120.671150	20.132749
57.549128	2130.169319	20.137767
57.677879	2117.604023	20.142784
57.501775	2126.021749	20.147802
57.552900	2122.355953	20.152819
57.623682	2129.394921	20.157837
57.425332	2152.390828	20.162855
57.641190	2139.832375	20.167872
58.188295	2160.989647	20.172890
58.061911	2154.648712	20.177907
58.497229	2145.923610	20.182925
58.000055	2157.490541	20.187943
58.395302	2159.106928	20.192960
58.027923	2150.636698	20.197978
58.212253	2153.330086	20.202995
58.374306	2145.461620	20.208013
58.167874	2153.920981	20.213031
58.397348	2151.976393	20.218048
58.339191	2164.685928	20.223066
58.727101	2164.986624	20.228083
58.566909	2177.667763	20.233101
58.832992	2176.049743	20.238119
58.804579	2177.485399	20.243136
59.052672	2169.649545	20.248154
59.142832	2181.761058	20.253171
59.209267	2163.506780	20.258189
59.078442	2170.268310	20.263207
59.298779	2163.041866	20.268224
59.616468	2166.444788	20.273242
58.897366	2155.594507	20.278259
59.345318	2146.221559	20.283277
59.345863	2158.299250	20.288295
59.444162	2162.223581	20.293312
59.632452	2160.514499	20.298330
59.462239	2152.989079	20.303347
59.452580	2146.732580	20.308365
59.695366	2156.822339	20.313383
59.580252	2151.257364	20.318400
59.526003	2157.724194	20.323418
59.484025	2155.165521	20.328435
59.820198	2154.472769	20.333453
59.617880	2146.494271	20.338471
59.770886	2161.582279	20.343488
59.801124	2150.349550	20.348506
59.734699	2177.497397	20.353523
59.906353	2170.067416	20.358541
60.002299	2189.992812	20.363559
60.179877	2188.572063	20.368576
60.315219	2191.528433	20.373594
60.164784	2186.555208	20.378611
60.391057	2191.058888	20.383629
60.026148	2187.129403	20.388647
60.347830	2199.148938	20.393664
60.515882	2192.396201	20.398682
60.605525	2222.828219	20.403699
61.036774	2206.570154	20.408717
60.869744	2227.696149	20.413735
61.041161	2205.642613	20.418752
61.280388	2217.303016	20.423770
61.124431	2206.985910	20.428787
61.035199	2207.794717	20.433805
61.264032	2203.639963	20.438823
61.114464	2210.741954	20.443840
61.328781	2204.031951	20.448858
61.214872	2211.624817	20.453875
61.495278	2213.496763	20.458893
61.523923	2213.285862	20.463911
61.574469	2207.949157	20.468928
61.858421	2209.868540	20.473946
61.371013	2200.885922	20.478963
61.591526	2213.800782	20.483981
61.643137	2198.559636	20.488999
61.652129	2204.215184	20.494016
61.892287	2208.726809	20.499034
61.211676	2216.376917	20.504051
61.546947	2223.433037	20.509069
61.688741	2235.744293	20.514087
61.976451	2241.854894	20.519104
62.063651	2236.456028	20.524122
61.678423	2255.973704	20.529139
61.873038	2241.175737	20.534157
62.239909	2249.772655	20.539175
62.211394	2262.203401	20.544192
62.131543	2260.275080	20.549210
62.345314	2256.307221	20.554227
62.457489	2260.571157	20.559245
62.548289	2260.558415	20.564263
62.519926	2262.872865	20.569280
62.714478	2254.230594	20.574298
62.448525	2266.465187	20.579315
62.749063	2272.907681	20.584333
63.291891	2277.617104	20.589351
62.905291	2284.225117	20.594368
63.105955	2283.857462	20.599386
62.941425	2285.888955	20.604403
63.498586	2276.853140	20.609421
63.544406	2270.068608	20.614439
63.299121	2280.317046	20.619456
63.718655	2272.573064	20.624474
63.472253	2276.543366	20.629491
63.767966	2261.604873	20.634509
63.947498	2273.809350	20.639527
63.734261	2278.222328	20.644544
63.988987	2276.925415	20.649562
63.549973	2266.661934	20.654579
64.016581	2275.589178	20.659597
63.719472	2274.131137	20.664615
63.881247	2269.562123	20.669632
64.263361	2285.357940	20.674650
63.553552	2289.729578	20.679667
63.940709	2289.275404	20.684685
64.012598	2272.961319	20.689703
63.737318	2288.484736	20.694720
64.370421	2263.224614	20.699738
64.065941	2278.035640	20.704755
64.629953	2284.766042	20.709773
64.262956	2309.173886	20.714791
64.453760	2286.764724	20.719808
64.506035	2301.445371	20.724826
64.515038	2295.605936	20.729843
64.807927	2303.759867	20.734861
64.622547	2282.224560	20.739879
64.767241	2305.448802	20.744896
64.668399	2289.570133	20.749914
64.866479	2315.119446	20.754931
64.955159	2332.348230	20.759949
65.073135	2335.796790	20.764967
65.087999	2343.715237	20.769984
65.617842	2333.037901	20.775002
65.405376	2344.569141	20.780019
65.377678	2334.079596	20.785037
65.387213	2343.694916	20.790055
65.188106	2332.434611	20.795072
65.590798	2323.433350	20.800090
65.366799	2336.498925	20.805107
65.733850	2334.313699	20.810125
65.558995	2340.189413	20.815143
65.649589	2346.228316	20.820160
66.021535	2341.090970	20.825178
65.720383	2338.102729	20.830195
66.083316	2336.737150	20.835213
66.299934	2341.215506	20.840231
66.016197	2348.823514	20.845248
66.313638	2345.940452	20.850266
66.185922	2352.448635	20.855283
66.055877	2358.021130	20.860301
66.229481	2376.659132	20.865319
66.078658	2375.774256	20.870336
66.239851	2377.508664	20.875354
66.503476	2369.428841	20.880371
66.850903	2378.807073	20.885389
66.293719	2371.265783	20.890407
66.562619	2391.860389	20.895424
67.022244	2404.046237	20.900442
66.929827	2407.444752	20.905459
67.230581	2417.718382	20.910477
67.458065	2404.778520	20.915495
67.570100	2412.130043	20.920512
67.521919	2397.284071	20.925530
67.611617	2405.002809	20.930547
67.341132	2408.151070	20.935565
67.841160	2402.804574	20.940583
67.414390	2406.813180	20.945600
67.500598	2398.776044	20.950618
67.634521	2406.759874	20.955635
67.542541	2396.742650	20.960653
67.746463	2394.316699	20.965671
67.620601	2401.201112	20.970688
67.882410	2395.239362	20.975706
67.633848	2399.285238	20.980723
67.816400	2400.224311	20.985741
67.952111	2416.976788	20.990759
68.054140	2430.562691	20.995776
68.395637	2435.220210	21.000794
68.330662	2428.284850	21.005811
68.334919	2420.391541	21.010829
68.430459	2427.228553	21.015847
68.575926	2419.317223	21.020864
68.556418	2420.011385	21.025882
68.653620	2420.505184	21.030899
68.565607	2420.736526	21.035917
68.544537	2423.797320	21.040935
68.482690	2425.831545	21.045952
68.946610	2440.764329	21.050970
68.961137	2436.439841	21.055987
68.807258	2462.818707	21.061005
69.096586	2453.422583	21.066023
69.057643	2453.594052	21.071040
69.178003	2449.289468	21.076058
69.122840	2451.718201	21.081075
69.050071	2442.880076	21.086093
69.429469	2464.404211	21.091111
69.335487	2471.128292	21.096128
69.640398	2482.441282	21.101146
69.436459	2478.814205	21.106163
69.399163	2477.127803	21.111181
69.749815	2474.294971	21.116199
69.753994	2470.983648	21.121216
69.899320	2474.764284	21.126234
69.935866	2500.845447	21.131251
70.135508	2507.140172	21.136269
70.290323	2493.037219	21.141287
70.234948	2512.683753	21.146304
70.500701	2489.274653	21.151322
70.470996	2511.156575	21.156339
70.463249	2495.624988	21.161357
70.761131	2498.142215	21.166375
70.519058	2501.597958	21.171392
70.801497	2497.862355	21.176410
70.784070	2484.562367	21.181427
70.518325	2501.883567	21.186445
70.544121	2499.296316	21.191463
70.590661	2503.539675	21.196480
71.076960	2517.733314	21.201498
71.116483	2528.143481	21.206515
71.317676	2532.727774	21.211533
71.773287	2520.407895	21.216551
71.478246	2519.941667	21.221568
71.459165	2523.495387	21.226586
71.674647	2522.053583	21.231603
71.586628	2529.944843	21.236621
71.871652	2514.961224	21.241639
71.514525	2527.260886	21.246656
71.864514	2531.816063	21.251674
71.897923	2511.956235	21.256691
71.439428	2529.583492	21.261709
71.694344	2510.479269	21.266727
71.597531	2524.359887	21.271744
71.870578	2505.206421	21.276762
72.159578	2531.388023	21.281779
72.222302	2534.066934	21.286797
72.465207	2531.569568	21.291815
72.303420	2546.010666	21.296832
72.349833	2538.969262	21.301850
72.478837	2543.571786	21.306867
71.992986	2546.848565	21.311885
72.200308	2528.118668	21.316903
72.152002	2559.054591	21.321920
72.233036	2564.281103	21.326938
72.462019	2574.268315	21.331955
72.565607	2573.379371	21.336973
72.846269	2577.443727	21.341991
72.919677	2594.224210	21.347008
72.997069	2598.591417	21.352026
73.639897	2607.110851	21.357043
73.651364	2606.784492	21.362061
73.905242	2594.041460	21.367079
73.856414	2600.579027	21.372096
73.324594	2574.977908	21.377114
73.520609	2577.528122	21.382131
73.734256	2593.856554	21.387149
73.599934	2591.871060	21.392167
73.855391	2588.213112	21.397184
74.018791	2605.108639	21.402202
73.915244	2593.160988	21.407219
73.468885	2584.103062	21.412237
73.910044	2587.312275	21.417255
74.184480	2589.971168	21.422272
74.215726	2597.300899	21.427290
74.137150	2599.171990	21.432307
74.116551	2620.329632	21.437325
74.211976	2603.115172	21.442343
74.300201	2610.837801	21.447360
74.162096	2621.281321	21.452378
74.592613	2630.412939	21.457395
74.353207	2647.354608	21.462413
74.608721	2642.336981	21.467431
74.621480	2647.387231	21.472448
74.806805	2652.427073	21.477466
74.952233	2638.523150	21.482483
75.130911	2643.112968	21.487501
75.661859	2658.546039	21.492519
75.452422	2658.774815	21.497536
75.475062	2658.738499	21.502554
75.647830	2653.789456	21.507571
75.316782	2664.186948	21.512589
75.342102	2667.423367	21.517607
75.614970	2668.635682	21.522624
75.619257	2668.668138	21.527642
75.601015	2669.993709	21.532659
75.679605	2682.751143	21.537677
76.367417	2665.852640	21.542695
76.360375	2666.149727	21.547712
76.143030	2665.604916	21.552730
76.210546	2667.082630	21.557747
75.917539	2676.276368	21.562765
76.782643	2694.298386	21.567783
76.732589	2690.257101	21.572800
76.769170	2702.897102	21.577818
76.879234	2684.228948	21.582835
76.568640	2687.544895	21.587853
77.127338	2707.492902	21.592871
76.618956	2685.900971	21.597888
76.783950	2705.167089	21.602906
76.631304	2678.652267	21.607923
76.579789	2695.954422	21.612941
76.744655	2688.950453	21.617959
77.002433	2696.450840	21.622976
77.244527	2710.815509	21.627994
77.359797	2725.073016	21.633011
77.297461	2712.537632	21.638029
77.514989	2717.254303	21.643047
77.852042	2722.935345	21.648064
77.320646	2712.295937	21.653082
77.569929	2727.884861	21.658099
77.484214	2721.758398	21.663117
77.857812	2716.069745	21.668135
77.756192	2715.228088	21.673152
77.923147	2721.002585	21.678170
77.976857	2717.573589	21.683187
77.789379	2744.470036	21.688205
78.457106	2718.159492	21.693223
78.460387	2740.440566	21.698240
78.278599	2730.017744	21.703258
78.394939	2730.857756	21.708275
78.346050	2730.471890	21.713293
78.483263	2724.874062	21.718311
78.663971	2730.218590	21.723328
78.837678	2760.839133	21.728346
79.081864	2769.487913	21.733363
78.971367	2761.051064	21.738381
79.449226	2750.764660	21.743399
79.243203	2753.464796	21.748416
79.303309	2755.650542	21.753434
79.483032	2755.154465	21.758451
79.394680	2758.123701	21.763469
79.387863	2753.615668	21.768487
79.548648	2765.553984	21.773504
79.536945	2764.304406	21.778522
79.722303	2747.938394	21.783539
79.803012	2769.923879	21.788557
80.027935	2760.889544	21.793575
79.858543	2751.770790	21.798592
79.475726	2760.242113	21.803610
79.772422	2751.189035	21.808627
79.911138	2770.738676	21.813645
79.835951	2781.499817	21.818663
79.671560	2769.266452	21.823680
79.927710	2786.892228	21.828698
80.372933	2797.679375	21.833715
80.476275	2807.055299	21.838733
80.517526	2805.286008	21.843751
80.642520	2808.002702	21.848768
80.839262	2809.464390	21.853786
81.065924	2799.709758	21.858803
81.029901	2813.626844	21.863821
81.012338	2789.689770	21.868839
81.389435	2806.131163	21.873856
81.281878	2814.602102	21.878874
81.234416	2800.891108	21.883891
81.594750	2824.558785	21.888909
81.576962	2820.093289	21.893927
81.704074	2830.761593	21.898944
81.597647	2812.966356	21.903962
81.812313	2824.577941	21.908979
81.704069	2819.421182	21.913997
81.538104	2825.514284	21.919015
82.081519	2831.656085	21.924032
81.706864	2832.536891	21.929050
81.852822	2833.144483	21.934067
81.920444	2841.480595	21.939085
82.099345	2843.509337	21.944103
82.150079	2857.983119	21.949120
81.922299	2850.280081	21.954138
82.253850	2844.222393	21.959155
82.223749	2860.963586	21.964173
82.368820	2868.654709	21.969191
82.720228	2869.500365	21.974208
82.833426	2877.656348	21.979226
83.248144	2866.119433	21.984243
83.003154	2872.691106	21.989261
83.180186	2870.539768	21.994279
83.371232	2875.215790	21.999296
83.310759	2880.899599	22.004314
83.360892	2872.369223	22.009331
83.420081	2885.193213	22.014349
83.456333	2871.549021	22.019367
83.135526	2873.102934	22.024384
83.153056	2878.259544	22.029402
83.815608	2882.780102	22.034419
83.767813	2913.895372	22.039437
83.900095	2906.208977	22.044455
83.960672	2917.887823	22.049472
83.966682	2906.380430	22.054490
84.243615	2900.180189	22.059507
84.113067	2897.884029	22.064525
83.912836	2905.830830	22.069543
83.838345	2894.489290	22.074560
83.980597	2933.558649	22.079578
84.308459	2930.863934	22.084595
84.554952	2929.333514	22.089613
84.551813	2926.905875	22.094631
84.676708	2929.775148	22.099648
84.845560	2947.355306	22.104666
85.292176	2944.253412	22.109683
85.046293	2947.390826	22.114701
85.123688	2952.718453	22.119719
85.049961	2953.611536	22.124736
85.049710	2957.968056	22.129754
85.063480	2951.603630	22.134771
85.418472	2957.868341	22.139789
85.573137	2967.927534	22.144807
85.982070	2968.673936	22.149824
85.769790	2983.393835	22.154842
86.169455	2979.688345	22.159859
86.006442	2985.129129	22.164877
86.000458	2989.244113	22.169895
86.473546	2962.300041	22.174912
86.158515	2979.965119	22.179930
86.559411	2972.801756	22.184947
86.029653	2983.553128	22.189965
86.356824	2979.681095	22.194983
86.468785	2956.871635	22.200000
86.352083	2970.264659	22.205018
86.532817	2992.482525	22.210035
86.775051	2991.988117	22.215053
86.954665	2999.642498	22.220071
86.889622	2997.899017	22.225088
86.741008	2995.232052	22.230106
86.730007	2998.657789	22.235123
87.199507	3003.938943	22.240141
87.184660	3006.176476	22.245159
87.732276	3016.821675	22.250176
87.362067	3030.717813	22.255194
87.665230	3025.596727	22.260211
87.772260	3019.825848	22.265229
88.097726	3034.483701	22.270247
88.176858	3014.544024	22.275264
87.837804	3023.961104	22.280282
88.246213	3028.697896	22.285299
87.948079	3017.250523	22.290317
87.788290	3034.382979	22.295335
88.102245	3009.406047	22.300352
88.135399	3019.270023	22.305370
88.233285	3024.165204	22.310387
88.565443	3050.368310	22.315405
88.380536	3043.379073	22.320423
88.601377	3045.966007	22.325440
88.516579	3042.905262	22.330458
88.594282	3045.856561	22.335475
88.721317	3058.243742	22.340493
88.487045	3059.405659	22.345511
89.086218	3075.485087	22.350528
89.104783	3082.900798	22.355546
89.225539	3082.162318	22.360563
89.307962	3072.541574	22.365581
89.226084	3074.939981	22.370599
89.316243	3069.541319	22.375616
89.568981	3105.115677	22.380634
89.752223	3089.418873	22.385651
90.295452	3103.217272	22.390669
90.106758	3107.382558	22.395687
90.100727	3090.204988	22.400704
90.127328	3107.128594	22.405722
90.137455	3095.760719	22.410739
90.436837	3086.810533	22.415757
90.302540	3103.582003	22.420775
90.621960	3086.592755	22.425792
90.479372	3089.458825	22.430810
90.709231	3084.126826	22.435827
90.787685	3081.475860	22.440845
90.752434	3101.236933	22.445863
91.218252	3100.313490	22.450880
91.251933	3108.423885	22.455898
91.301985	3114.687680	22.460915
91.343695	3113.184391	22.465933
91.127238	3108.713456	22.470951
91.681575	3106.643421	22.475968
91.387604	3111.837217	22.480986
91.414989	3110.672480	22.486003
91.720135	3104.472613	22.491021
91.380729	3094.005323	22.496039
91.815333	3098.924206	22.501056
91.737344	3113.604716	22.506074
92.059381	3128.368922	22.511091
91.858817	3134.255484	22.516109
92.226496	3141.407253	22.521127
92.090876	3132.757642	22.526144
91.894975	3155.811917	22.531162
92.325196	3155.576961	22.536179
91.911328	3166.411069	22.541197
92.059041	3161.822071	22.546215
92.378619	3167.557934	22.551232
92.803234	3189.529111	22.556250
92.859875	3191.869216	22.561267
93.145223	3204.828916	22.566285
93.003690	3193.336833	22.571303
93.554973	3187.613726	22.576320
93.244229	3183.458320	22.581338
93.225036	3189.730045	22.586355
93.074751	3172.366794	22.591373
93.312880	3213.182845	22.596391
93.383749	3211.184816	22.601408
93.746864	3205.168617	22.606426
93.565950	3213.805031	22.611443
93.899981	3221.881402	22.616461
94.154527	3229.534144	22.621479
94.420043	3237.786789	22.626496
94.255844	3238.952097	22.631514
94.575739	3241.982494	22.636531
94.748527	3252.019194	22.641549
94.423252	3234.798952	22.646567
94.826272	3255.059984	22.651584
94.837242	3246.880131	22.656602
95.109616	3247.931371	22.661619
95.153247	3235.227279	22.666637
95.348918	3245.352507	22.671655
95.262760	3233.504427	22.676672
95.118068	3236.681864	22.681690
95.240755	3240.039111	22.686707
95.573869	3230.058763	22.691725
95.368012	3250.335573	22.696743
95.252290	3243.102355	22.701760
95.233454	3237.033525	22.706778
95.340814	3250.858420	22.711795
95.669929	3267.344847	22.716813
95.569668	3266.022470	22.721831
95.856845	3269.201965	22.726848
95.680768	3271.461062	22.731866
95.856753	3291.962004	22.736883
96.348866	3304.155405	22.741901
95.985058	3299.076344	22.746919
96.038013	3311.148246	22.751936
96.229294	3301.458588	22.756954
96.205759	3319.092417	22.761971
96.234157	3326.278885	22.766989
96.107205	3337.016096	22.772007
96.842507	3337.894396	22.777024
96.901907	3351.363167	22.782042
96.879443	3360.675974	22.787059
97.303818	3348.271042	22.792077
97.232863	3351.971505	22.797095
97.188032	3357.544646	22.802112
97.547823	3374.116268	22.807130
97.639848	3389.494667	22.812147
97.717404	3375.136181	22.817165
97.585115	3384.709451	22.822183
98.213495	3372.211345	22.827200
98.266975	3380.620158	22.832218
98.020714	3360.065559	22.837235
98.313834	3389.643106	22.842253
98.396551	3399.353675	22.847271
98.662118	3410.090831	22.852288
98.838699	3406.413446	22.857306
98.824947	3397.743154	22.862323
99.067128	3407.561617	22.867341
98.884436	3406.444958	22.872359
98.778759	3405.991300	22.877376
99.033265	3402.875004	22.882394
99.233750	3409.538826	22.887411
99.558105	3405.825014	22.892429
99.233277	3390.465385	22.897447
99.098481	3409.895695	22.902464
99.233756	3420.334732	22.907482
99.413078	3415.376295	22.912499
99.348085	3435.552910	22.917517
99.135516	3441.118961	22.922535
99.488934	3468.948064	22.927552
100.111426	3449.754973	22.932570
100.119641	3472.535459	22.937587
100.295139	3465.081586	22.942605
100.276693	3466.393283	22.947623
100.264097	3465.856138	22.952640
100.444492	3486.381016	22.957658
100.521106	3485.887587	22.962675
100.658192	3499.005489	22.967693
100.701645	3492.630226	22.972711
100.861216	3484.435533	22.977728
101.500924	3484.130329	22.982746
100.902611	3487.707357	22.987763
101.680098	3492.624821	22.992781
101.554986	3473.461352	22.997799
101.602827	3475.109312	23.002816
101.609454	3470.320131	23.007834
101.866304	3492.039762	23.012851
101.767238	3489.857002	23.017869
101.783843	3511.725210	23.022887
102.009586	3524.452136	23.027904
102.311626	3507.678865	23.032922
102.201007	3516.624080	23.037939
102.220710	3516.896687	23.042957
102.296633	3505.332810	23.047975
102.130620	3506.365969	23.052992
102.501869	3500.490624	23.058010
102.422132	3512.710191	23.063027
102.510511	3508.425360	23.068045
102.558041	3530.951818	23.073063
102.797150	3523.747030	23.078080
103.008926	3540.099215	23.083098
103.106591	3531.310050	23.088115
103.256670	3543.559770	23.093133
103.174509	3535.534316	23.098151
103.401273	3538.105592	23.103168
103.493478	3555.449129	23.108186
103.275425	3563.258475	23.113203
103.930279	3551.497722	23.118221
103.739690	3559.149390	23.123239
103.626725	3546.135512	23.128256
104.214672	3569.419703	23.133274
104.174435	3571.858153	23.138291
104.625659	3572.692868	23.143309
104.696709	3572.341684	23.148327
104.443592	3574.598203	23.153344
104.450050	3574.849773	23.158362
104.371405	3589.240314	23.163379
104.696443	3572.069305	23.168397
104.773173	3588.304498	23.173415
104.860906	3604.132999	23.178432
105.240668	3606.735103	23.183450
105.129069	3620.031003	23.188467
104.860331	3600.033301	23.193485
105.053808	3611.267120	23.198503
105.421124	3625.391298	23.203520
105.519020	3638.578388	23.208538
105.488050	3641.005672	23.213555
105.702737	3627.120121	23.218573
106.021313	3650.040316	23.223591
106.235039	3657.065023	23.228608
106.287960	3667.599524	23.233626
106.083976	3657.913351	23.238643
106.341675	3657.308503	23.243661
106.621674	3661.505532	23.248679
106.239090	3662.837069	23.253696
106.268884	3672.057968	23.258714
106.460205	3689.750409	23.263731
106.795698	3687.678278	23.268749
107.113649	3671.684430	23.273767
106.997872	3687.801352	23.278784
107.227262	3682.893410	23.283802
106.842226	3711.856130	23.288819
107.145966	3711.335792	23.293837
107.422182	3708.509332	23.298855
107.387087	3706.024847	23.303872
107.948903	3718.216508	23.308890
107.833152	3734.930680	23.313907
108.225803	3727.580551	23.318925
108.094564	3728.855992	23.323943
108.087101	3728.513448	23.328960
108.548890	3725.475033	23.333978
108.746280	3727.280381	23.338995
108.786474	3719.787725	23.344013
108.730636	3730.553022	23.349031
108.699976	3726.451177	23.354048
109.222962	3721.582693	23.359066
108.998606	3727.449592	23.364083
109.447546	3721.240285	23.369101
109.145463	3714.761214	23.374119
109.317832	3726.093678	23.379136
109.431618	3734.661211	23.384154
109.488684	3748.485612	23.389171
109.368596	3746.256883	23.394189
109.637943	3766.918803	23.399207
109.656800	3765.923132	23.404224
109.921811	3754.887038	23.409242
109.959812	3766.662575	23.414259
110.021065	3767.446003	23.419277
109.985486	3784.190874	23.424295
110.087833	3782.983780	23.429312
110.201670	3782.545605	23.434330
110.171389	3788.712326	23.439347
110.134219	3801.170347	23.444365
110.891479	3805.863711	23.449383
110.851657	3817.875360	23.454400
111.437744	3815.952538	23.459418
111.153292	3819.109491	23.464435
111.244787	3823.822725	23.469453
111.354726	3811.751651	23.474471
111.188602	3829.203928	23.479488
111.653554	3836.055714	23.484506
111.574164	3826.376797	23.489523
111.560500	3846.591526	23.494541
112.117600	3842.668886	23.499559
111.705116	3849.420412	23.504576
111.940226	3858.818703	23.509594
112.204835	3856.687598	23.514611
112.151758	3871.242670	23.519629
112.422731	3858.513095	23.524647
112.125500	3887.726973	23.529664
112.680386	3878.232171	23.534682
112.690578	3905.673726	23.539699
112.930164	3885.967814	23.544717
113.044719	3900.071220	23.549735
113.067369	3899.389463	23.554752
113.263053	3914.309744	23.559770
113.331526	3921.695564	23.564787
113.867943	3923.606321	23.569805
114.065058	3917.225176	23.574823
113.982491	3920.968832	23.579840
114.258802	3906.534886	23.584858
114.284874	3915.019775	23.589875
114.354178	3916.682148	23.594893
114.825290	3907.197629	23.599911
114.514866	3902.817182	23.604928
114.847912	3904.794612	23.609946
114.450524	3899.187661	23.614963
114.730435	3899.391687	23.619981
114.988228	3898.984836	23.624999
114.352580	3901.972293	23.630016
114.967868	3906.213585	23.635034
115.009343	3915.916728	23.640051
114.683343	3923.652759	23.645069
115.372468	3918.714636	23.650087
115.067227	3926.890127	23.655104
115.391581	3940.125088	23.660122
115.321735	3948.513254	23.665139
115.624239	3959.135444	23.670157
115.554577	3953.531007	23.675175
115.450181	3965.471556	23.680192
116.026838	3973.076559	23.685210
116.163891	3977.016603	23.690227
116.158927	3982.453663	23.695245
116.361816	3985.189189	23.700263
116.601364	3992.336941	23.705280
116.540055	3985.874856	23.710298
116.544088	4008.617061	23.715315
116.804413	4013.626061	23.720333
117.084483	4012.319899	23.725351
116.687970	4020.048733	23.730368
116.826678	4015.421603	23.735386
117.323452	4038.504848	23.740403
117.240460	4034.917058	23.745421
117.534409	4037.777303	23.750439
117.260262	4039.657459	23.755456
117.506867	4058.120875	23.760474
117.765779	4076.116944	23.765491
118.057949	4074.976094	23.770509
118.339503	4064.726775	23.775527
118.251689	4087.898822	23.780544
118.533866	4056.613329	23.785562
118.650882	4074.330891	23.790579
118.736643	4101.131592	23.795597
119.007018	4093.789490	23.800615
118.830751	4108.420257	23.805632
119.154819	4089.888265	23.810650
119.420294	4090.927714	23.815667
119.168122	4081.513793	23.820685
119.577599	4083.152254	23.825703
119.444347	4109.469499	23.830720
119.730001	4105.131433	23.835738
119.966911	4127.764468	23.840755
120.053734	4114.049408	23.845773
120.092833	4121.294514	23.850791
120.399738	4107.402941	23.855808
120.134128	4104.313402	23.860826
120.395685	4106.827059	23.865843
120.133485	4112.922395	23.870861
120.686422	4132.252956	23.875879
120.619485	4125.067363	23.880896
120.794525	4139.388148	23.885914
120.835512	4140.583590	23.890931
120.908818	4139.376150	23.895949
121.265300	4160.082069	23.900967
121.358917	4157.761472	23.905984
121.320152	4169.124426	23.911002
121.143068	4167.766635	23.916019
121.234059	4181.544283	23.921037
121.594152	4189.763898	23.926055
121.492669	4190.587626	23.931072
121.899786	4209.206974	23.936090
121.949111	4211.644306	23.941107
122.273401	4223.880344	23.946125
122.278248	4223.703072	23.951143
122.565383	4241.365942	23.956160
122.435227	4213.872554	23.961178
122.715417	4233.288469	23.966195
122.843790	4239.225222	23.971213
123.132270	4245.442989	23.976231
123.064476	4234.132035	23.981248
123.413759	4247.733206	23.986266
123.574794	4236.395066	23.991283
123.377228	4240.712115	23.996301
123.860230	4264.918409	24.001319
123.705199	4259.165769	24.006336
124.153400	4260.993119	24.011354
124.226679	4257.754638	24.016371
124.174185	4265.361392	24.021389
124.770638	4260.878621	24.026407
124.345749	4263.575814	24.031424
124.624036	4265.467855	24.036442
124.848239	4258.886431	24.041459
124.329733	4262.297496	24.046477
125.248002	4269.992648	24.051495
125.227874	4274.965009	24.056512
125.295019	4276.236452	24.061530
125.350616	4286.873685	24.066547
125.418192	4295.466488	24.071565
125.903502	4278.231602	24.076583
125.592233	4299.178756	24.081600
125.345448	4294.982950	24.086618
125.707307	4288.898436	24.091635
125.657362	4302.210519	24.096653
125.836551	4301.322567	24.101671
125.822125	4330.983839	24.106688
125.920735	4322.536186	24.111706
126.090063	4324.947801	24.116723
125.751189	4345.620453	24.121741
126.407991	4344.594128	24.126759
126.478832	4372.480807	24.131776
126.406353	4376.877614	24.136794
126.946306	4377.000883	24.141811
127.013768	4395.495485	24.146829
127.230036	4392.012880	24.151847
127.288733	4402.418583	24.156864
127.305886	4407.355693	24.161882
127.727948	4418.342686	24.166899
127.832071	4430.408581	24.171917
128.014860	4429.332237	24.176935
128.355076	4430.214481	24.181952
128.235307	4418.711984	24.186970
128.477944	4421.523302	24.191987
128.614008	4422.192436	24.197005
128.925869	4438.769186	24.202023
129.030228	4449.839803	24.207040
128.899618	4451.093938	24.212058
129.312995	4444.308738	24.217075
128.985312	4452.320893	24.222093
129.197403	4438.265956	24.227111
129.478229	4442.701248	24.232128
129.460830	4459.485182	24.237146
129.776110	4469.449326	24.242163
129.563773	4480.187659	24.247181
130.221650	4467.986555	24.252199
129.785911	4484.390047	24.257216
130.063060	4498.066743	24.262234
130.058699	4503.229482	24.267251
130.286420	4525.296515	24.272269
130.317262	4503.912529	24.277287
130.414462	4526.470022	24.282304
130.580860	4540.983156	24.287322
130.693854	4562.415666	24.292339
130.619248	4550.098533	24.297357
130.728276	4568.130966	24.302375
130.948344	4586.964354	24.307392
130.869509	4588.707971	24.312410
131.459444	4607.692860	24.317427
131.651886	4605.711375	24.322445
131.749416	4610.547473	24.327463
132.004527	4614.083529	24.332480
132.203734	4632.153497	24.337498
132.362484	4633.378336	24.342515
132.507540	4632.069238	24.347533
132.682328	4626.856837	24.352551
132.571961	4630.924152	24.357568
132.657390	4648.036571	24.362586
132.662114	4655.539967	24.367603
133.015193	4668.842459	24.372621
133.273598	4668.028405	24.377639
133.132434	4668.203600	24.382656
133.375405	4676.900307	24.387674
133.625546	4673.139604	24.392691
133.752167	4686.207486	24.397709
134.031308	4681.247506	24.402727
133.732554	4693.258133	24.407744
134.101998	4687.510398	24.412762
134.453212	4690.406185	24.417779
134.324335	4703.380475	24.422797
134.526595	4727.993333	24.427815
134.437523	4720.048131	24.432832
134.775757	4728.100387	24.437850
135.393474	4704.054981	24.442867
135.127941	4705.437731	24.447885
135.107141	4720.355980	24.452903
135.176097	4725.748015	24.457920
135.114314	4736.100229	24.462938
135.761719	4738.842358	24.467955
135.555042	4755.984660	24.472973
135.750906	4762.700618	24.477991
136.075730	4764.441725	24.483008
136.019235	4783.047429	24.488026
136.329939	4765.037709	24.493043
136.174109	4775.149584	24.498061
136.276243	4779.871982	24.503079
136.600566	4806.454954	24.508096
136.536780	4809.155560	24.513114
136.696420	4801.224336	24.518131
136.818882	4822.032804	24.523149
137.034449	4818.354157	24.528167
137.477844	4819.861898	24.533184
137.233892	4837.023047	24.538202
137.712504	4836.685985	24.543219
137.357293	4860.227780	24.548237
137.751919	4858.280963	24.553255
137.699160	4868.036495	24.558272
137.699367	4879.993532	24.563290
138.232672	4880.676573	24.568307
138.411300	4895.649044	24.573325
138.817639	4898.286941	24.578343
139.179931	4908.017220	24.583360
139.348284	4906.982600	24.588378
139.442888	4895.046684	24.593395
139.536494	4911.895048	24.598413
139.547349	4891.131948	24.603431
139.468570	4902.353624	24.608448
139.216917	4912.360161	24.613466
139.512844	4927.592810	24.618483
139.617501	4931.045926	24.623501
139.643257	4949.424850	24.628519
139.919689	4948.584968	24.633536
139.536515	4970.311450	24.638554
140.273813	4981.369196	24.643571
140.491909	4998.425431	24.648589
140.861147	5010.556238	24.653607
141.192746	5009.382823	24.658624
141.160398	5011.814879	24.663642
141.445544	4992.511855	24.668659
141.318709	4992.018534	24.673677
141.292122	5016.981481	24.678695
141.722920	5021.643737	24.683712
141.555059	5033.231808	24.688730
141.824449	5013.719547	24.693747
141.726690	5042.375063	24.698765
141.918896	5047.307466	24.703783
142.573540	5060.013209	24.708800
142.451318	5074.059957	24.713818
142.917599	5055.585602	24.718835
142.801369	5065.974985	24.723853
142.366499	5055.655603	24.728871
142.838719	5068.852136	24.733888
142.681419	5081.023547	24.738906
142.845939	5093.139034	24.743923
142.803819	5098.733809	24.748941
143.274422	5110.714477	24.753959
143.071348	5126.372306	24.758976
143.260717	5128.746876	24.763994
144.053970	5139.258863	24.769011
144.232894	5139.759132	24.774029
143.973602	5158.936604	24.779047
144.316359	5142.301503	24.784064
144.317359	5155.130295	24.789082
144.601661	5160.558946	24.794099
144.617682	5162.430657	24.799117
144.913598	5174.185903	24.804135
145.488165	5162.623634	24.809152
145.486756	5196.327816	24.814170
145.837830	5181.289768	24.819187
145.875466	5192.836126	24.824205
145.834770	5183.513758	24.829223
145.900799	5183.300380	24.834240
146.149986	5185.796575	24.839258
146.375594	5181.276004	24.844275
146.382288	5186.912746	24.849293
146.623603	5191.767393	24.854311
146.932323	5208.690377	24.859328
146.971679	5220.341199	24.864346
147.096800	5210.978421	24.869363
146.954132	5211.660577	24.874381
147.164718	5215.387600	24.879399
147.160758	5213.722752	24.884416
147.233532	5222.746718	24.889434
147.456421	5232.236843	24.894451
147.530283	5243.281174	24.899469
148.111345	5247.730869	24.904487
148.167446	5259.848259	24.909504
148.219585	5273.345098	24.914522
148.458238	5272.826807	24.919539
148.495540	5255.533375	24.924557
148.587983	5277.502174	24.929575
148.631359	5289.602004	24.934592
148.704393	5291.056422	24.939610
148.678912	5301.583727	24.944627
149.042055	5316.915105	24.949645
149.105486	5334.037031	24.954663
149.329163	5329.737218	24.959680
149.443107	5346.561037	24.964698
149.631978	5344.279644	24.969715
149.759253	5358.289751	24.974733
149.988889	5357.721765	24.979751
150.281382	5380.897858	24.984768
150.367353	5373.597833	24.989786
150.990219	5372.140427	24.994803
150.914207	5370.071311	24.999821
150.947751	5376.814358	25.004839
151.239175	5383.270297	25.009856
151.390576	5415.116558	25.014874
151.191796	5403.520084	25.019891
151.526149	5409.848070	25.024909
151.104420	5422.486295	25.029927
151.435321	5424.794215	25.034944
151.845594	5442.093209	25.039962
151.793643	5457.317719	25.044979
151.869987	5455.992348	25.049997
151.611772	5481.335273	25.055015
152.254427	5473.187667	25.060032
152.674686	5500.241035	25.065050
152.711222	5506.437555	25.070067
152.983764	5500.040151	25.075085
153.090414	5509.258300	25.080103
153.324847	5498.878027	25.085120
153.502451	5533.451432	25.090138
153.589725	5533.908588	25.095155
153.756954	5533.960781	25.100173
153.514986	5526.708180	25.105191
153.943663	5543.883769	25.110208
153.904558	5564.046271	25.115226
154.218470	5564.031704	25.120243
154.266066	5546.773258	25.125261
154.491594	5580.668342	25.130279
155.079359	5581.538099	25.135296
155.074032	5589.757424	25.140314
154.949565	5585.501288	25.145331
155.363734	5604.566842	25.150349
155.419923	5611.770841	25.155367
155.872809	5615.081524	25.160384
155.985656	5620.973731	25.165402
155.869765	5608.506667	25.170419
156.004490	5623.837508	25.175437
156.078143	5631.378019	25.180455
156.359993	5633.054671	25.185472
156.557077	5659.013240	25.190490
156.494597	5636.278081	25.195507
156.978912	5667.576512	25.200525
156.744326	5676.246781	25.205543
157.102858	5669.881952	25.210560
157.134594	5688.776537	25.215578
157.376816	5689.888844	25.220595
157.564251	5706.863123	25.225613
157.420759	5696.178610	25.230631
157.711194	5722.812846	25.235648
158.051987	5738.384568	25.240666
157.956102	5736.434048	25.245683
158.482598	5744.820316	25.250701
158.369411	5749.785689	25.255719
158.819298	5766.903685	25.260736
158.893276	5754.174013	25.265754
158.984319	5786.408589	25.270771
159.340207	5783.578241	25.275789
159.031234	5813.396920	25.280807
159.538271	5807.409098	25.285824
159.693732	5811.743052	25.290842
159.963758	5818.425165	25.295859
159.944938	5826.034597	25.300877
160.113086	5825.022394	25.305895
160.324263	5847.499184	25.310912
160.696592	5851.664233	25.315930
160.492014	5858.883087	25.320947
160.728009	5856.517451	25.325965
160.635441	5881.281251	25.330983
161.225224	5877.211365	25.336000
161.260112	5889.098874	25.341018
161.245504	5885.381629	25.346035
161.434523	5904.906833	25.351053
161.604844	5910.334896	25.356071
161.967457	5930.660248	25.361088
161.944438	5916.717640	25.366106
162.215533	5947.306929	25.371123
162.290661	5936.187278	25.376141
162.314713	5953.964865	25.381159
162.620873	5970.026044	25.386176
162.764895	5988.028353	25.391194
162.767117	5980.185148	25.396211
163.196467	5975.162930	25.401229
163.253698	6008.226449	25.406247
163.160097	5999.781696	25.411264
163.514465	6014.580524	25.416282
163.590497	6026.814517	25.421299
164.023944	6028.349224	25.426317
163.993362	6052.503005	25.431335
164.250968	6037.498874	25.436352
164.284249	6063.945457	25.441370
164.347332	6072.193105	25.446387
164.608882	6066.047702	25.451405
164.535579	6089.533739	25.456423
164.457333	6103.440275	25.461440
165.318928	6104.667609	25.466458
165.505484	6125.379818	25.471475
166.130112	6109.693264	25.476493
166.362295	6121.409360	25.481511
166.650369	6105.707156	25.486528
166.679361	6122.541912	25.491546
166.585740	6110.934622	25.496563
166.780596	6110.619623	25.501581
166.995828	6114.842989	25.506599
166.655272	6123.269181	25.511616
167.126512	6140.926628	25.516634
167.193393	6149.802485	25.521651
167.395763	6144.163725	25.526669
167.198095	6152.545848	25.531687
167.365451	6150.033622	25.536704
167.696497	6174.181383	25.541722
167.718894	6192.078030	25.546739
167.982242	6205.548257	25.551757
167.895197	6196.576280	25.556775
167.855755	6231.442630	25.561792
168.567787	6225.462514	25.566810
168.429839	6244.487000	25.571827
168.805493	6265.811911	25.576845
168.825396	6270.258558	25.581863
169.126513	6282.335862	25.586880
169.345848	6300.604855	25.591898
169.420147	6308.929916	25.596915
169.828590	6306.260100	25.601933
169.843354	6323.758513	25.606951
170.046822	6324.117745	25.611968
170.383635	6325.341253	25.616986
170.328501	6345.060910	25.622003
170.684477	6343.410883	25.627021
170.945670	6364.300859	25.632039
171.117715	6386.273028	25.637056
171.778699	6370.564851	25.642074
171.241432	6382.879989	25.647091
171.831311	6376.167561	25.652109
171.963460	6396.539084	25.657127
172.073951	6403.148193	25.662144
172.472283	6391.721243	25.667162
172.413387	6391.778519	25.672180
172.656058	6402.292574	25.677197
173.141943	6409.591705	25.682215
172.838039	6412.711437	25.687232
173.081173	6421.249630	25.692250
173.125539	6432.978490	25.697268
173.383276	6419.072909	25.702285
173.599080	6452.431672	25.707303
173.765698	6462.053513	25.712320
174.157431	6452.973927	25.717338
174.045523	6465.238531	25.722356
174.404802	6434.986040	25.727373
174.337964	6465.419563	25.732391
174.679675	6483.001152	25.737408
174.837472	6480.946803	25.742426
174.845831	6485.178860	25.747444
175.022104	6476.346303	25.752461
175.366675	6488.639052	25.757479
175.218549	6500.106430	25.762496
175.549914	6503.219252	25.767514
175.442397	6516.803790	25.772532
175.525632	6527.545479	25.777549
175.654183	6531.997872	25.782567
175.901377	6535.667584	25.787584
176.184556	6540.964607	25.792602
176.356036	6567.630572	25.797620
176.447247	6560.704763	25.802637
176.536152	6591.090744	25.807655
176.790204	6595.217265	25.812672
177.104511	6594.829364	25.817690
177.384506	6616.597776	25.822708
177.771170	6609.468776	25.827725
177.483629	6631.811753	25.832743
177.533533	6637.224136	25.837760
178.028483	6653.940733	25.842778
178.003666	6667.283756	25.847796
178.194316	6684.049091	25.852813
178.389973	6694.984550	25.857831
178.680180	6714.205820	25.862848
179.050970	6711.511447	25.867866
179.136715	6730.736204	25.872884
179.696482	6736.349842	25.877901
179.718088	6737.740837	25.882919
180.035355	6752.177552	25.887936
180.182324	6744.201764	25.892954
180.283375	6763.048394	25.897972
180.482607	6767.134012	25.902989
180.692128	6786.896725	25.908007
180.609283	6779.846016	25.913024
181.052436	6799.124019	25.918042
181.028700	6802.852737	25.923060
181.452984	6805.257263	25.928077
181.437024	6808.529914	25.933095
181.380111	6825.359539	25.938112
181.884748	6847.354968	25.943130
181.717017	6843.054448	25.948148
181.882551	6877.142990	25.953165
182.234345	6876.760309	25.958183
182.267299	6884.407375	25.963200
182.797719	6883.774282	25.968218
182.446602	6896.029529	25.973236
183.106600	6887.465285	25.978253
183.248127	6907.361449	25.983271
183.469481	6926.110827	25.988288
184.039685	6907.318657	25.993306
184.269954	6931.546455	25.998324
184.550649	6941.266686	26.003341
184.502702	6949.455179	26.008359
184.672043	6950.022851	26.013376
184.959395	6945.509293	26.018394
185.137743	6952.531891	26.023412
185.345037	6950.473634	26.028429
185.282584	6950.967780	26.033447
185.436472	6965.697868	26.038464
185.636116	6969.167243	26.043482
185.628666	6979.966359	26.048500
185.767312	6978.866426	26.053517
185.939536	6990.382029	26.058535
185.982848	7001.000700	26.063552
186.280571	6997.688735	26.068570
186.113674	7021.630279	26.073588
186.165880	7045.413591	26.078605
186.726620	7053.098745	26.083623
187.060806	7081.006208	26.088640
186.960186	7079.504793	26.093658
186.895053	7087.568226	26.098676
186.950825	7097.813588	26.103693
187.090559	7114.051498	26.108711
187.352796	7133.400364	26.113728
187.596339	7129.066853	26.118746
187.768527	7166.165616	26.123764
188.156172	7171.305020	26.128781
188.206302	7192.334142	26.133799
188.492357	7195.378989	26.138816
188.996265	7205.911060	26.143834
189.289677	7219.029501	26.148852
189.402444	7231.459578	26.153869
190.029484	7233.310115	26.158887
190.402502	7238.444871	26.163904
190.671614	7235.578992	26.168922
191.002060	7233.430654	26.173940
190.887877	7237.638666	26.178957
191.222555	7239.447735	26.183975
191.005607	7243.497111	26.188992
191.233879	7247.314629	26.194010
191.445069	7262.018596	26.199028
191.456752	7269.192124	26.204045
191.693332	7276.375745	26.209063
191.553580	7300.021842	26.214080
191.696273	7303.963769	26.219098
191.789762	7327.897406	26.224116
192.004470	7338.388361	26.229133
192.585696	7359.096055	26.234151
192.597521	7367.013034	26.239168
192.694413	7374.145754	26.244186
193.105636	7398.459352	26.249204
193.165105	7405.499041	26.254221
193.251619	7417.189383	26.259239
193.122372	7438.157120	26.264256
193.871640	7447.234397	26.269274
194.093142	7471.684987	26.274292
194.266949	7449.705535	26.279309
194.556442	7488.559210	26.284327
194.542778	7492.020632	26.289344
194.724495	7508.312653	26.294362
194.796566	7527.210666	26.299380
195.006141	7521.872246	26.304397
195.596343	7547.981234	26.309415
195.761384	7559.070412	26.314432
196.025207	7552.903974	26.319450
196.378067	7560.842667	26.324468
196.747187	7577.489690	26.329485
196.945559	7574.132987	26.334503
197.042082	7570.502510	26.339520
197.042782	7570.388496	26.344538
196.857842	7590.861611	26.349556
197.322899	7597.917060	26.354573
197.582987	7610.337271	26.359591
197.611758	7620.018828	26.364608
198.016265	7617.833000	26.369626
198.391615	7621.217572	26.374644
198.517382	7638.689265	26.379661
198.976047	7641.078005	26.384679
198.865155	7666.137466	26.389696
199.211601	7654.289358	26.394714
199.386003	7666.834028	26.399732
199.427191	7679.720465	26.404749
199.851778	7680.620075	26.409767
199.778018	7703.502190	26.414784
200.205439	7698.991656	26.419802
199.669740	7699.860141	26.424820
199.970801	7723.912079	26.429837
200.105789	7714.652104	26.434855
200.309925	7737.029208	26.439872
200.233377	7750.735309	26.444890
200.419793	7765.500544	26.449908
200.665564	7786.059468	26.454925
200.957732	7796.307965	26.459943
201.084451	7814.892511	26.464960
201.292568	7823.582954	26.469978
201.866521	7835.736480	26.474996
201.832894	7854.447586	26.480013
202.407624	7872.286387	26.485031
202.579424	7874.101967	26.490048
203.038860	7894.325668	26.495066
203.057290	7873.251002	26.500084
202.830975	7913.327402	26.505101
203.266705	7904.217663	26.510119
203.557152	7938.778519	26.515136
203.712933	7934.872760	26.520154
204.268127	7951.689474	26.525172
204.077003	7975.616782	26.530189
204.737271	7974.749555	26.535207
204.672804	7978.921985	26.540224
204.802979	8002.646607	26.545242
205.327324	7998.561798	26.550260
205.250454	8026.153742	26.555277
205.183858	8035.945033	26.560295
205.270157	8051.001940	26.565312
205.479619	8054.471510	26.570330
206.013545	8074.961934	26.575348
206.014185	8086.904021	26.580365
206.634848	8094.682175	26.585383
206.651536	8106.720072	26.590400
206.800660	8127.104818	26.595418
207.369699	8135.085265	26.600436
207.182353	8133.978475	26.605453
207.798283	8155.954203	26.610471
208.199482	8156.265453	26.615488
208.250501	8163.512433	26.620506
208.644878	8170.651491	26.625524
208.582097	8190.773631	26.630541
208.867336	8182.982583	26.635559
208.999584	8201.179185	26.640576
209.073031	8204.281413	26.645594
209.220067	8212.196952	26.650612
209.273071	8228.881935	26.655629
209.531595	8219.609128	26.660647
209.619090	8257.428551	26.665664
210.397005	8267.728621	26.670682
210.194602	8290.865966	26.675700
210.564877	8291.610773	26.680717
210.406353	8306.501243	26.685735
210.485493	8322.996138	26.690752
210.895231	8333.194844	26.695770
211.347301	8345.149170	26.700788
211.268375	8349.526495	26.705805
211.945239	8378.123905	26.710823
211.794779	8376.008410	26.715840
212.036802	8399.878179	26.720858
212.564908	8394.917643	26.725876
212.526948	8417.638148	26.730893
213.034573	8406.214920	26.735911
213.205868	8443.116007	26.740928
213.148453	8439.151627	26.745946
213.285248	8451.420394	26.750964
213.534004	8463.977042	26.755981
214.003392	8463.424864	26.760999
213.923722	8481.053512	26.766016
214.114640	8484.395502	26.771034
214.341189	8497.412647	26.776052
214.368857	8525.365445	26.781069
214.978130	8537.364826	26.786087
214.931741	8530.094658	26.791104
215.313960	8558.709577	26.796122
215.559735	8557.120068	26.801140
215.585180	8565.942705	26.806157
215.790305	8595.149294	26.811175
215.954691	8597.689196	26.816192
216.323815	8619.183389	26.821210
216.826474	8610.355962	26.826228
216.700806	8632.736851	26.831245
216.897256	8634.083766	26.836263
216.810247	8661.234290	26.841280
217.287530	8663.893411	26.846298
217.533481	8692.355454	26.851316
217.313245	8699.421460	26.856333
217.975752	8710.558420	26.861351
218.034835	8743.566742	26.866368
218.011804	8749.091928	26.871386
218.538901	8768.823562	26.876404
218.747461	8793.470519	26.881421
219.119253	8800.401730	26.886439
219.474688	8817.437466	26.891456
219.547906	8839.721989	26.896474
219.908931	8850.045647	26.901492
220.051995	8849.474916	26.906509
220.323494	8874.179333	26.911527
220.803345	8883.811549	26.916544
221.005523	8890.049377	26.921562
221.503161	8893.955897	26.926580
221.578959	8898.770135	26.931597
221.776248	8916.247178	26.936615
221.873668	8919.414896	26.941632
222.336683	8933.501498	26.946650
222.863124	8935.101083	26.951668
223.158994	8939.799422	26.956685
222.770304	8944.234395	26.961703
222.670559	8948.553104	26.966720
222.825234	8965.497730	26.971738
223.085177	8983.782825	26.976756
223.137095	8996.696918	26.981773
223.408551	9022.432561	26.986791
223.781387	9043.435248	26.991808
223.984749	9048.363136	26.996826
224.802145	9047.612456	27.001844
224.446464	9057.396224	27.006861
224.528229	9067.372358	27.011879
225.094031	9081.787085	27.016896
225.038839	9099.817214	27.021914
225.609343	9111.098830	27.026932
225.356162	9127.535269	27.031949
225.663285	9146.307383	27.036967
226.208754	9162.175555	27.041984
226.371436	9166.672284	27.047002
226.602028	9177.261083	27.052020
227.167772	9201.667718	27.057037
227.592818	9201.658429	27.062055
227.864961	9213.120951	27.067072
227.611437	9211.402794	27.072090
228.069408	9234.271728	27.077108
228.207715	9235.334519	27.082125
228.498576	9245.244711	27.087143
228.856958	9262.155208	27.092160
228.496716	9267.984395	27.097178
228.881840	9270.865995	27.102196
229.140274	9273.900850	27.107213
229.348857	9300.926442	27.112231
229.588058	9297.839090	27.117248
229.516387	9309.560910	27.122266
229.754207	9329.150437	27.127284
229.869684	9337.998010	27.132301
230.067141	9354.438201	27.137319
230.423530	9369.426534	27.142336
230.372077	9402.215840	27.147354
230.823083	9403.577472	27.152372
230.900066	9429.899618	27.157389
230.903063	9443.059236	27.162407
231.415130	9476.371517	27.167424
231.618835	9491.645901	27.172442
231.865664	9508.760190	27.177460
231.932660	9535.534690	27.182477
232.131760	9553.955732	27.187495
232.708492	9567.966614	27.192512
232.942186	9601.474018	27.197530
233.209382	9607.201233	27.202548
233.509390	9619.541607	27.207565
233.580606	9654.125111	27.212583
234.194775	9656.579840	27.217600
234.436242	9679.590736	27.222618
234.818629	9683.766971	27.227636
235.181869	9691.901940	27.232653
235.066388	9699.786775	27.237671
235.676613	9704.714594	27.242688
235.802508	9738.953710	27.247706
235.814190	9718.689771	27.252724
236.372401	9746.739010	27.257741
236.624203	9769.574258	27.262759
236.744123	9767.707694	27.267776
236.890439	9791.433121	27.272794
237.106289	9787.039665	27.277812
237.490214	9806.129111	27.282829
237.551360	9810.494722	27.287847
237.657378	9831.607129	27.292864
237.974733	9846.560618	27.297882
238.355472	9856.119227	27.302900
238.394396	9877.717738	27.307917
238.560615	9901.131279	27.312935
238.748072	9891.087884	27.317952
238.604287	9926.535335	27.322970
238.980447	9933.617556	27.327988
239.231180	9963.346077	27.333005
239.155158	10000.325525	27.338023
239.975043	10002.458824	27.343040
240.017060	10032.459047	27.348058
240.308889	10041.252669	27.353076
240.863936	10069.651152	27.358093
240.764808	10091.531906	27.363111
241.525388	10074.061298	27.368128
241.378478	10114.878426	27.373146
242.148788	10107.244169	27.378164
242.517715	10114.766398	27.383181
242.827244	10156.911845	27.388199
243.055226	10143.722725	27.393216
243.094782	10150.642475	27.398234
243.475515	10152.727842	27.403252
243.644150	10184.457637	27.408269
243.630385	10189.502101	27.413287
243.923350	10187.170525	27.418304
244.005728	10206.287435	27.423322
244.303677	10216.033229	27.428340
244.379599	10241.739358	27.433357
244.208785	10266.747456	27.438375
244.820422	10269.108969	27.443392
244.710937	10279.548325	27.448410
245.027981	10302.175852	27.453428
245.148436	10317.061495	27.458445
245.467555	10337.024010	27.463463
245.894668	10354.701759	27.468480
245.921066	10374.377921	27.473498
246.519022	10401.466294	27.478516
246.834389	10408.607610	27.483533
247.085430	10415.225508	27.488551
247.413254	10440.677662	27.493568
247.660515	10460.524600	27.498586
247.896182	10468.736187	27.503604
247.985531	10481.762669	27.508621
247.824507	10511.082122	27.513639
248.275029	10519.312586	27.518656
248.268313	10539.530052	27.523674
248.705939	10550.227346	27.528692
249.041756	10577.776021	27.533709
249.303671	10595.055192	27.538727
249.731973	10607.594904	27.543744
249.737022	10617.167998	27.548762
250.237201	10643.210339	27.553780
250.427183	10658.565309	27.558797
250.763402	10684.233870	27.563815
250.969948	10695.400314	27.568832
251.170117	10711.761117	27.573850
251.702983	10734.883722	27.578868
251.917721	10746.087445	27.583885
252.145632	10772.284474	27.588903
252.378707	10782.357204	27.593920
252.740497	10791.312190	27.598938
253.070581	10819.900424	27.603956
253.173025	10824.740777	27.608973
253.226439	10848.969145	27.613991
253.457859	10859.317894	27.619008
253.669858	10886.007692	27.624026
254.277704	10895.441970	27.629044
254.605826	10902.749183	27.634061
254.809253	10930.937119	27.639079
255.263213	10937.818674	27.644096
255.368117	10955.373095	27.649114
256.089542	10958.386919	27.654132
256.299274	10988.196599	27.659149
256.324590	10992.119459	27.664167
256.516002	10971.964441	27.669184
256.760821	11019.313885	27.674202
256.847851	11015.114675	27.679220
257.497919	11033.848115	27.684237
256.900054	11048.190658	27.689255
257.733284	11049.707484	27.694272
257.727383	11076.670707	27.699290
258.352611	11089.317690	27.704308
258.357503	11099.928523	27.709325
258.331196	11117.590663	27.714343
258.576159	11120.997542	27.719360
258.708148	11145.555248	27.724378
258.909292	11172.901916	27.729396
259.490471	11192.445674	27.734413
259.714062	11209.084335	27.739431
260.226828	11229.030153	27.744448
260.239303	11244.110954	27.749466
260.776821	11259.911650	27.754484
261.387463	11255.413966	27.759501
261.406354	11265.720897	27.764519
262.070519	11271.742331	27.769536
262.064068	11281.984140	27.774554
262.092406	11276.701194	27.779572
262.487619	11312.293471	27.784589
262.297776	11308.810288	27.789607
262.561438	11333.210250	27.794624
262.774909	11347.312663	27.799642
263.337644	11347.583124	27.804660
263.118736	11376.485203	27.809677
263.087324	11402.200696	27.814695
263.642462	11409.194928	27.819712
263.815209	11432.493845	27.824730
263.592076	11459.017813	27.829748
264.617270	11480.160139	27.834765
264.740106	11507.740884	27.839783
265.110783	11519.072996	27.844800
265.306973	11539.574086	27.849818
265.501719	11558.592914	27.854836
266.009250	11563.513081	27.859853
265.862264	11596.916643	27.864871
266.740527	11613.904450	27.869888
266.705499	11623.872338	27.874906
267.452932	11649.162565	27.879924
267.900439	11645.284112	27.884941
267.717059	11664.558539	27.889959
268.231063	11675.164411	27.894976
268.299419	11688.254428	27.899994
268.625310	11702.337005	27.905012
268.992017	11712.674985	27.910029
268.906026	11731.545041	27.915047
269.817457	11747.781513	27.920064
269.720819	11767.941342	27.925082
269.957584	11770.386297	27.930100
270.484189	11796.385983	27.935117
270.560623	11808.410510	27.940135
270.750076	11830.031696	27.945152
270.814369	11842.416682	27.950170
271.395741	11859.499496	27.955188
271.724884	11862.438092	27.960205
271.892348	11894.874160	27.965223
272.253846	11893.961586	27.970240
272.246533	11920.989485	27.975258
272.244690	11938.134869	27.980276
272.735344	11953.975509	27.985293
272.600056	11986.724109	27.990311
273.438690	11995.656133	27.995328
273.560314	12024.765441	28.000346
273.872654	12025.557825	28.005364
274.064473	12060.997099	28.010381
274.533619	12068.253190	28.015399
275.020202	12096.018270	28.020416
275.304628	12111.973492	28.025434
275.371303	12131.447434	28.030452
275.806920	12146.254352	28.035469
275.798713	12157.399794	28.040487
276.154389	12179.209049	28.045504
276.613148	12194.870072	28.050522
276.667749	12216.676341	28.055540
276.937225	12227.834248	28.060557
276.853081	12258.904085	28.065575
277.450161	12276.321918	28.070592
277.572749	12295.834874	28.075610
277.662037	12319.835026	28.080628
277.982464	12334.402759	28.085645
278.178018	12360.680214	28.090663
278.479024	12382.647668	28.095680
278.845481	12404.891092	28.100698
279.391364	12425.987825	28.105716
279.772552	12445.226629	28.110733
279.948624	12470.538508	28.115751
280.513392	12488.566142	28.120768
280.852429	12492.504498	28.125786
280.890000	12514.577894	28.130804
281.097624	12540.131247	28.135821
281.261594	12543.079141	28.140839
282.120920	12554.245385	28.145856
282.259664	12578.975911	28.150874
281.811628	12596.819650	28.155892
282.433783	12607.398822	28.160909
282.481211	12624.752654	28.165927
282.863709	12657.182308	28.170944
282.981793	12681.451606	28.175962
282.924217	12700.996398	28.180980
283.295692	12709.107135	28.185997
283.407703	12749.921289	28.191015
283.673567	12765.451666	28.196032
284.271800	12789.459816	28.201050
284.724733	12835.692291	28.206068
285.018432	12848.319033	28.211085
285.364891	12873.907489	28.216103
285.695248	12890.373485	28.221120
285.921570	12908.038398	28.226138
286.285972	12934.696191	28.231156
286.800277	12967.601801	28.236173
287.032464	12982.608545	28.241191
287.369880	13024.140088	28.246208
287.645248	13026.238524	28.251226
287.713262	13056.780561	28.256244
288.113237	13063.069282	28.261261
288.186472	13087.137044	28.266279
288.823363	13110.223057	28.271296
289.276449	13132.459479	28.276314
289.240982	13149.948897	28.281332
289.626811	13161.075626	28.286349
289.968580	13194.103957	28.291367
290.055941	13210.659275	28.296384
290.613227	13220.282915	28.301402
290.985189	13246.517704	28.306420
291.677209	13257.126731	28.311437
291.720528	13294.918919	28.316455
292.001802	13284.727124	28.321472
292.362124	13297.156498	28.326490
292.480070	13319.253170	28.331508
292.936514	13322.208821	28.336525
293.230264	13339.888279	28.341543
293.351851	13361.257242	28.346560
293.794115	13375.326791	28.351578
293.810681	13411.670914	28.356596
294.018059	13412.562648	28.361613
294.329760	13434.494322	28.366631
294.395760	13463.144301	28.371648
295.114320	13473.949986	28.376666
295.179064	13503.228147	28.381684
295.518398	13517.616569	28.386701
295.785526	13541.957080	28.391719
295.982290	13573.299751	28.396736
296.458499	13588.945861	28.401754
296.291554	13606.899475	28.406772
297.086938	13648.341206	28.411789
297.160763	13654.282247	28.416807
297.190131	13674.424431	28.421824
297.458809	13703.445514	28.426842
297.726692	13735.109220	28.431860
298.032513	13762.290164	28.436877
298.700448	13782.618485	28.441895
298.883851	13810.903817	28.446912
299.190045	13823.634046	28.451930
299.686622	13845.150475	28.456948
299.957195	13869.710723	28.461965
300.127710	13895.975125	28.466983
300.435628	13910.088612	28.472000
301.096855	13929.261654	28.477018
301.398744	13934.950821	28.482036
301.544848	13959.731886	28.487053
301.817508	13974.270394	28.492071
302.310384	13982.568927	28.497088
302.772107	13985.070812	28.502106
302.574021	14023.857112	28.507124
303.131805	14036.782302	28.512141
303.113422	14052.489306	28.517159
303.361496	14066.129069	28.522176
303.813651	14087.443590	28.527194
304.011102	14117.121657	28.532212
304.025443	14142.953726	28.537229
304.481668	14152.356689	28.542247
304.557075	14194.857917	28.547264
305.053775	14208.551267	28.552282
305.120723	14248.704605	28.557300
305.335722	14276.222871	28.562317
306.033024	14290.256600	28.567335
305.876349	14331.907809	28.572352
306.353343	14345.769986	28.577370
306.510239	14388.370137	28.582388
307.285683	14395.924138	28.587405
307.964397	14439.090573	28.592423
308.296074	14472.146037	28.597440
308.819736	14468.471794	28.602458
308.809880	14496.643710	28.607476
309.161545	14513.624699	28.612493
309.426094	14539.195453	28.617511
309.655662	14573.705100	28.622528
309.957504	14581.406770	28.627546
310.229203	14614.185642	28.632564
310.691284	14638.849360	28.637581
311.025553	14652.659744	28.642599
311.355390	14681.647266	28.647616
312.250659	14690.640789	28.652634
312.137561	14717.826370	28.657652
312.396268	14743.474049	28.662669
312.664561	14766.892011	28.667687
312.785277	14784.017020	28.672704
313.361905	14799.256130	28.677722
313.636039	14824.682354	28.682740
313.856214	14838.790664	28.687757
314.436588	14862.568489	28.692775
314.367265	14905.325559	28.697792
314.809065	14899.269517	28.702810
315.381075	14931.255634	28.707828
315.600044	14935.698206	28.712845
315.614025	14951.221092	28.717863
315.694362	14985.307163	28.722880
316.261743	15004.991798	28.727898
316.665683	15032.998579	28.732916
316.863386	15053.061088	28.737933
317.422206	15070.238508	28.742951
317.564035	15108.224299	28.747968
318.202804	15123.212347	28.752986
318.270236	15147.157279	28.758004
318.632016	15170.398068	28.763021
319.191969	15174.212343	28.768039
319.042683	15204.972407	28.773056
319.514058	15221.817750	28.778074
319.430837	15268.549187	28.783092
319.822413	15279.696918	28.788109
320.621470	15315.272300	28.793127
320.641334	15328.429226	28.798144
320.986603	15351.628879	28.803162
321.197851	15375.923864	28.808180
321.497515	15405.158771	28.813197
321.628577	15427.215182	28.818215
322.021032	15454.123061	28.823232
322.207984	15471.006200	28.828250
322.813800	15496.994841	28.833268
322.867508	15521.141150	28.838285
323.357096	15532.920545	28.843303
323.310575	15561.084605	28.848320
323.755333	15585.547763	28.853338
324.499214	15609.595936	28.858356
324.908128	15647.660203	28.863373
325.151868	15660.892297	28.868391
325.408829	15686.026442	28.873408
325.999828	15704.625394	28.878426
326.457930	15720.537373	28.883444
326.562623	15759.879781	28.888461
326.770122	15766.875846	28.893479
326.870272	15801.128974	28.898496
327.538920	15822.312308	28.903514
327.942340	15854.343857	28.908532
328.055896	15881.856392	28.913549
328.846362	15875.584798	28.918567
328.509786	15914.045485	28.923584
329.114439	15948.537058	28.928602
329.567224	15966.930639	28.933620
329.959941	16002.253175	28.938637
330.504319	15994.756734	28.943655
330.304711	16029.578342	28.948672
330.974724	16056.699814	28.953690
330.993667	16085.465421	28.958708
331.063074	16109.939376	28.963725
331.751399	16137.102083	28.968743
331.966288	16176.819697	28.973760
332.445540	16189.931364	28.978778
332.713763	16221.012045	28.983796
332.726479	16243.884962	28.988813
333.580946	16271.445947	28.993831
333.616583	16307.491610	28.998848
334.340182	16309.008187	29.003866
334.883500	16339.544070	29.008884
335.135601	16356.099023	29.013901
335.293684	16381.780096	29.018919
335.961382	16403.816936	29.023936
336.096740	16416.348916	29.028954
336.478875	16453.358874	29.033972
336.428620	16463.864932	29.038989
337.063240	16501.537739	29.044007
337.338083	16522.440337	29.049024
337.856087	16548.555486	29.054042
337.976405	16560.724438	29.059060
338.026904	16593.893712	29.064077
338.500097	16615.094612	29.069095
338.758186	16641.427784	29.074112
338.858688	16662.704503	29.079130
339.612115	16692.352156	29.084148
339.744632	16716.857570	29.089165
340.184491	16749.612964	29.094183
340.462213	16785.003473	29.099200
340.809753	16803.869274	29.104218
341.163626	16842.840590	29.109236
341.238496	16870.063318	29.114253
341.852419	16883.397576	29.119271
342.031422	16913.958476	29.124288
342.572527	16940.384061	29.129306
343.033550	16977.490918	29.134324
343.127350	16989.604682	29.139341
343.729549	17014.965944	29.144359
343.550704	17054.074630	29.149376
343.951099	17058.974802	29.154394
344.262103	17090.095773	29.159412
344.562455	17124.583372	29.164429
345.221103	17143.625114	29.169447
345.409206	17173.179491	29.174464
345.722740	17210.052774	29.179482
346.140276	17220.286604	29.184500
346.475586	17260.735572	29.189517
346.956467	17263.939303	29.194535
347.113085	17305.112934	29.199552
347.613991	17327.481180	29.204570
348.143176	17354.109561	29.209588
348.009856	17387.469990	29.214605
348.807781	17423.217231	29.219623
348.939670	17442.139885	29.224640
349.241503	17486.692680	29.229658
349.896753	17516.340713	29.234676
349.689723	17536.028695	29.239693
349.995897	17570.492630	29.244711
350.354920	17599.937583	29.249728
350.821970	17640.881099	29.254746
351.611160	17668.806698	29.259764
351.710409	17696.625679	29.264781
352.242910	17712.982802	29.269799
352.577264	17741.007309	29.274816
353.253999	17757.446244	29.279834
353.526396	17791.359866	29.284852
353.413626	17808.428906	29.289869
354.214038	17835.817067	29.294887
354.542881	17877.149659	29.299904
354.835478	17899.143316	29.304922
355.300374	17923.888776	29.309940
355.386502	17956.104531	29.314957
355.654480	17979.631182	29.319975
356.176878	18024.569818	29.324992
356.870608	18045.461897	29.330010
357.387871	18073.593876	29.335028
357.421391	18087.947035	29.340045
358.069769	18127.419663	29.345063
358.599218	18137.892488	29.350080
359.287807	18164.833142	29.355098
359.702890	18164.145445	29.360116
359.500134	18202.250519	29.365133
360.154282	18209.199060	29.370151
360.108229	18241.434059	29.375168
360.253117	18258.241915	29.380186
360.953287	18266.369706	29.385204
361.130925	18302.706792	29.390221
361.455962	18323.636495	29.395239
361.777893	18354.384516	29.400256
361.731659	18379.227716	29.405274
362.283353	18400.410082	29.410292
362.425762	18444.293580	29.415309
363.070146	18461.581809	29.420327
363.081441	18512.165302	29.425344
363.328691	18543.963125	29.430362
363.596744	18577.619020	29.435380
364.118340	18611.835191	29.440397
364.366296	18647.196807	29.445415
364.765840	18691.312735	29.450432
365.017950	18710.001051	29.455450
365.943483	18738.422935	29.460468
366.199215	18786.282655	29.465485
366.611786	18814.660169	29.470503
366.914338	18839.012987	29.475520
367.245231	18864.344702	29.480538
367.921232	18891.729962	29.485556
367.863654	18915.073731	29.490573
368.299801	18949.738175	29.495591
368.810626	18971.870596	29.500608
369.171855	18998.037619	29.505626
369.656286	19033.014230	29.510644
369.327168	19067.882583	29.515661
369.904383	19094.513735	29.520679
370.471941	19116.455714	29.525696
370.855587	19157.533424	29.530714
371.058450	19188.728251	29.535732
371.033477	19226.552543	29.540749
371.600141	19253.847710	29.545767
372.112362	19287.616032	29.550784
372.507117	19330.553865	29.555802
372.357140	19341.692965	29.560820
373.323255	19406.752071	29.565837
373.741941	19428.288746	29.570855
373.912077	19477.453976	29.575872
374.574242	19497.096849	29.580890
374.981082	19538.184284	29.585908
375.249225	19569.019115	29.590925
375.895076	19600.453633	29.595943
376.106138	19636.324712	29.600960
376.415050	19659.214918	29.605978
377.135028	19695.410302	29.610996
377.414991	19725.272491	29.616013
378.060146	19746.912455	29.621031
378.499233	19770.777515	29.626048
379.034214	19805.870362	29.631066
379.325089	19826.709889	29.636084
379.674885	19857.779245	29.641101
379.961419	19873.698390	29.646119
380.446092	19906.123228	29.651136
380.667559	19946.841925	29.656154
381.335928	19968.467311	29.661172
381.645230	19983.594654	29.666189
381.533202	20026.983718	29.671207
382.092299	20061.169902	29.676224
382.404219	20077.922067	29.681242
382.963630	20117.067371	29.686260
382.898886	20153.179019	29.691277
383.367735	20191.385790	29.696295
383.874095	20216.521924	29.701312
383.519039	20256.789644	29.706330
384.168234	20299.658005	29.711348
384.529096	20333.622136	29.716365
385.182488	20382.596718	29.721383
385.662435	20420.449085	29.726400
385.647658	20469.178055	29.731418
386.223674	20506.820858	29.736436
386.514381	20535.282935	29.741453
386.772528	20578.738392	29.746471
387.430694	20605.639197	29.751488
387.734299	20651.458171	29.756506
388.426805	20681.119937	29.761524
388.940599	20715.781558	29.766541
389.305523	20755.267889	29.771559
390.163627	20780.168638	29.776576
390.156970	20819.949812	29.781594
390.956501	20837.290573	29.786612
391.018140	20881.249044	29.791629
391.273567	20912.225618	29.796647
391.562723	20941.454770	29.801664
391.966815	20978.148108	29.806682
392.446568	21016.167385	29.811700
392.488112	21061.821123	29.816717
392.779150	21077.980293	29.821735
393.383830	21108.330454	29.826752
393.570657	21155.402854	29.831770
394.928052	21169.773284	29.836788
394.622838	21211.157476	29.841805
395.198434	21222.650890	29.846823
395.929671	21255.813228	29.851840
395.833697	21300.583898	29.856858
396.300225	21317.608140	29.861876
396.958119	21343.063031	29.866893
397.061260	21377.973586	29.871911
397.659139	21394.533231	29.876928
397.818078	21441.379312	29.881946
398.401712	21462.274995	29.886964
398.569772	21503.290084	29.891981
398.965748	21526.750189	29.896999
399.574355	21564.284381	29.902016
399.607805	21606.873184	29.907034
399.920542	21636.176905	29.912052
400.144522	21687.508973	29.917069
400.302734	21710.223540	29.922087
401.138514	21766.961354	29.927104
401.310968	21812.505659	29.932122
402.116879	21839.112902	29.937140
402.308523	21886.730452	29.942157
402.920095	21922.027940	29.947175
403.655327	21954.142650	29.952192
404.333798	21996.389414	29.957210
404.924744	22006.881345	29.962228
405.347187	22032.116066	29.967245
405.582227	22071.496124	29.972263
406.394390	22103.997267	29.977280
406.503551	22127.720003	29.982298
406.975656	22145.445713	29.987316
407.226301	22183.388840	29.992333
407.430835	22207.974047	29.997351
407.901931	22243.207138	30.002368
408.180164	22276.892497	30.007386
408.325616	22314.000405	30.012404
408.904924	22354.128277	30.017421
409.063865	22384.218601	30.022439
409.852616	22415.637995	30.027456
409.902374	22473.458706	30.032474
410.270640	22487.189662	30.037492
410.534482	22537.574986	30.042509
410.720444	22572.573674	30.047527
410.989292	22623.362022	30.052544
411.396224	22675.158777	30.057562
412.267198	22707.575705	30.062580
412.528344	22761.572454	30.067597
412.724235	22803.256166	30.072615
413.422446	22840.573470	30.077632
413.794021	22888.280807	30.082650
414.891426	22918.865025	30.087668
415.246242	22945.483915	30.092685
415.302328	22989.727896	30.097703
416.226655	23009.393109	30.102720
416.413300	23064.295484	30.107738
416.756367	23097.378985	30.112756
417.277586	23117.255963	30.117773
417.633115	23169.641345	30.122791
418.103339	23194.102123	30.127808
418.017470	23243.516241	30.132826
418.866880	23272.716827	30.137844
418.895545	23304.194084	30.142861
419.371001	23353.482687	30.147879
419.811859	23385.380752	30.152896
420.182437	23444.048897	30.157914
420.408350	23465.182765	30.162932
420.865258	23517.180398	30.167949
421.393045	23557.319661	30.172967
421.947834	23586.744470	30.177984
422.357711	23638.277256	30.183002
423.037890	23654.732530	30.188020
423.217273	23689.499710	30.193037
423.222236	23729.252759	30.198055
423.591022	23769.081391	30.203072
424.159285	23822.835306	30.208090
424.491507	23840.425101	30.213108
424.829705	23907.912160	30.218125
425.326320	23942.422489	30.223143
425.730916	24003.409395	30.228160
426.303274	24044.739152	30.233178
426.450611	24076.783194	30.238196
427.105510	24144.508991	30.243213
427.160049	24174.490475	30.248231
427.940264	24236.552965	30.253248
428.076216	24284.252727	30.258266
428.441316	24316.902969	30.263284
429.317684	24360.620862	30.268301
429.723964	24402.775170	30.273319
430.464481	24447.201600	30.278336
430.749910	24481.230756	30.283354
431.263066	24516.909454	30.288372
431.825943	24548.510485	30.293389
432.198846	24606.258326	30.298407
432.843211	24640.133904	30.303424
433.145817	24684.090902	30.308442
433.747093	24737.407097	30.313460
434.236383	24765.804137	30.318477
434.730133	24809.174870	30.323495
435.278715	24828.902715	30.328512
435.532252	24861.097836	30.333530
436.032238	24899.819500	30.338548
436.349916	24940.441409	30.343565
436.406886	24983.042752	30.348583
437.175224	25027.062459	30.353600
437.248841	25072.242448	30.358618
437.926504	25120.566203	30.363636
437.842579	25158.397855	30.368653
438.373564	25213.911006	30.373671
438.775453	25263.393936	30.378688
439.140362	25311.870817	30.383706
439.933228	25359.170226	30.388724
440.424362	25400.141438	30.393741
440.992446	25461.289499	30.398759
441.708526	25470.443145	30.403776
442.326875	25521.269203	30.408794
442.579425	25564.883548	30.413812
443.365760	25595.582371	30.418829
443.499297	25640.093283	30.423847
444.363494	25667.067524	30.428864
444.388922	25709.691668	30.433882
444.798605	25758.894079	30.438900
445.216548	25778.646191	30.443917
445.487376	25830.207047	30.448935
445.921309	25872.070303	30.453952
446.367192	25920.276941	30.458970
446.929765	25966.480754	30.463988
447.298483	26013.848902	30.469005
447.382478	26057.374089	30.474023
447.535179	26099.060447	30.479040
448.027393	26138.590426	30.484058
448.687169	26187.082591	30.489076
449.318814	26234.581376	30.494093
449.609101	26294.218787	30.499111
449.681145	26335.401828	30.504128
450.444868	26390.347385	30.509146
450.687820	26432.388642	30.514164
451.693868	26456.689939	30.519181
451.813349	26515.161048	30.524199
452.500107	26551.717340	30.529216
452.441183	26595.442547	30.534234
452.816505	26632.506187	30.539252
453.430309	26692.042662	30.544269
453.506614	26732.685072	30.549287
454.556926	26782.144151	30.554304
454.983129	26837.995297	30.559322
455.231869	26870.001050	30.564340
456.187819	26923.273400	30.569357
456.353739	26972.267271	30.574375
457.202223	27019.798656	30.579392
457.595859	27071.477017	30.584410
458.125382	27103.581905	30.589428
459.015741	27147.763570	30.594445
459.099514	27194.513433	30.599463
459.418778	27243.192587	30.604480
460.172824	27270.208073	30.609498
460.686456	27324.327460	30.614516
460.970629	27352.035718	30.619533
461.269116	27399.444545	30.624551
461.784824	27430.129885	30.629568
462.314385	27480.575899	30.634586
462.706383	27525.487435	30.639604
463.163052	27551.511670	30.644621
463.493241	27619.126749	30.649639
463.864831	27656.453434	30.654656
464.418621	27688.896047	30.659674
464.431341	27754.299508	30.664692
465.502916	27795.302023	30.669709
465.883233	27848.177160	30.674727
466.056494	27898.371010	30.679744
466.563798	27941.813717	30.684762
466.813401	28004.179471	30.689780
467.412174	28032.562300	30.694797
468.094267	28092.749997	30.699815
468.874479	28155.609004	30.704832
469.112919	28197.021363	30.709850
469.753779	28259.768143	30.714868
470.362072	28286.847163	30.719885
470.660913	28350.366763	30.724903
471.313040	28377.675247	30.729920
472.000542	28425.697637	30.734938
472.206848	28465.466321	30.739956
472.927932	28511.354336	30.744973
473.778402	28544.664273	30.749991
474.014366	28588.882058	30.755008
474.778157	28625.048401	30.760026
475.306245	28666.606449	30.765044
475.595609	28699.116734	30.770061
475.534112	28736.984133	30.775079
476.128816	28776.695685	30.780096
476.632425	28813.640340	30.785114
476.707662	28855.923425	30.790132
477.670288	28903.113140	30.795149
477.988687	28959.875347	30.800167
478.365451	28996.447065	30.805184
478.561873	29053.762802	30.810202
478.830245	29096.512949	30.815220
479.950626	29150.490548	30.820237
480.024274	29202.855887	30.825255
480.526251	29257.475362	30.830272
481.159804	29298.443427	30.835290
481.310768	29351.925695	30.840308
481.906685	29403.255913	30.845325
482.467790	29442.132339	30.850343
482.952052	29482.371613	30.855360
483.437282	29521.626658	30.860378
483.567713	29581.453304	30.865396
484.046076	29614.814165	30.870413
484.331524	29670.382330	30.875431
485.203866	29718.431415	30.880448
485.568581	29766.094481	30.885466
485.891597	29826.754471	30.890484
486.473646	29852.297779	30.895501
486.868492	29913.605483	30.900519
487.245101	29967.544471	30.905536
488.096610	30010.903993	30.910554
488.127532	30070.956962	30.915572
488.565511	30126.211182	30.920589
489.013938	30184.337590	30.925607
489.423561	30251.713283	30.930624
490.271486	30303.717461	30.935642
490.458852	30369.666634	30.940660
490.907890	30424.957833	30.945677
491.554611	30480.399517	30.950695
491.832821	30545.198715	30.955712
492.408924	30596.087797	30.960730
492.866078	30664.182788	30.965748
493.448457	30730.339371	30.970765
493.763657	30806.067230	30.975783
494.535406	30860.047821	30.980800
495.474783	30907.947176	30.985818
496.138269	30957.037368	30.990836
496.942624	31013.577762	30.995853
497.833712	31057.305613	31.000871
498.045930	31105.593776	31.005888
498.584120	31165.052520	31.010906
498.591151	31200.894992	31.015924
499.335270	31263.370622	31.020941
499.809359	31303.760919	31.025959
500.087867	31370.850292	31.030976
500.642323	31408.391479	31.035994
500.844977	31479.809444	31.041012
501.381260	31528.266076	31.046029
501.904235	31581.226856	31.051047
502.430510	31643.575788	31.056064
503.788845	31674.047462	31.061082
504.612503	31718.822876	31.066100
505.480535	31765.420843	31.071117
505.720867	31794.787105	31.076135
506.108781	31840.940889	31.081152
506.929532	31880.388765	31.086170
506.817100	31926.208991	31.091188
507.544517	31962.741659	31.096205
507.896115	32003.027617	31.101223
508.568630	32054.501297	31.106240
508.970215	32108.723576	31.111258
509.069888	32143.423247	31.116276
509.942523	32186.440835	31.121293
509.975243	32241.705615	31.126311
510.506502	32295.585257	31.131328
510.626761	32354.400934	31.136346
510.980040	32412.771337	31.141364
511.278134	32476.432353	31.146381
511.615825	32522.457416	31.151399
511.997854	32590.338870	31.156416
512.471283	32660.240422	31.161434
513.038348	32733.411086	31.166452
513.747308	32796.835029	31.171469
514.256544	32864.440980	31.176487
514.286162	32930.482670	31.181504
515.423641	32982.276647	31.186522
515.862903	33053.769216	31.191540
516.540824	33091.350414	31.196557
517.072541	33150.485704	31.201575
518.014784	33195.365203	31.206592
518.345648	33246.482357	31.211610
518.535228	33310.255818	31.216628
519.053647	33365.891922	31.221645
519.474233	33425.096973	31.226663
519.849475	33483.950034	31.231680
520.949946	33539.124553	31.236698
521.044121	33604.388266	31.241716
521.984858	33661.015659	31.246733
522.028698	33712.067993	31.251751
522.446856	33769.050240	31.256768
522.936174	33835.549453	31.261786
523.323871	33894.408138	31.266804
523.812434	33962.536014	31.271821
524.638707	34031.643269	31.276839
525.023087	34102.089020	31.281856
525.638742	34161.977398	31.286874
526.192537	34230.710800	31.291892
526.897607	34289.411101	31.296909
527.797941	34361.908750	31.301927
528.386435	34416.287122	31.306944
528.867586	34462.258853	31.311962
529.407353	34507.343859	31.316980
530.313886	34569.353239	31.321997
531.226941	34617.491124	31.327015
531.211870	34675.958272	31.332032
532.469511	34725.560385	31.337050
532.820311	34778.653907	31.342068
533.637539	34820.932983	31.347085
534.303035	34876.975528	31.352103
534.383272	34904.862026	31.357120
535.195890	34957.176160	31.362138
535.603978	35015.243219	31.367156
535.680180	35068.588066	31.372173
536.360806	35111.792837	31.377191
536.737185	35162.273790	31.382208
536.867182	35208.772462	31.387226
537.080821	35277.537719	31.392244
537.820518	35349.712548	31.397261
538.418219	35408.904457	31.402279
538.791759	35472.008466	31.407296
539.270861	35543.835854	31.412314
540.208916	35595.421178	31.417332
540.776475	35664.804742	31.422349
541.298376	35719.116071	31.427367
541.743437	35788.495108	31.432384
542.435956	35813.880567	31.437402
542.432129	35907.912400	31.442420
543.015215	35963.855238	31.447437
543.639426	36026.875633	31.452455
543.894297	36109.606854	31.457472
544.976852	36179.712025	31.462490
545.217528	36243.664318	31.467508
545.912796	36300.719380	31.472525
546.869341	36354.566407	31.477543
546.967559	36418.053740	31.482560
547.723814	36475.926058	31.487578
547.968388	36550.446962	31.492596
548.446686	36622.578619	31.497613
549.352638	36680.679326	31.502631
549.887822	36752.483391	31.507648
550.408240	36800.455381	31.512666
550.663225	36883.512048	31.517684
551.292012	36940.447598	31.522701
552.248998	37014.461457	31.527719
552.679295	37069.647229	31.532736
553.276518	37113.823668	31.537754
553.708786	37174.500404	31.542772
554.340534	37234.162959	31.547789
555.101124	37270.972533	31.552807
555.481709	37341.693675	31.557824
555.866619	37393.552298	31.562842
556.337049	37459.096214	31.567860
556.819703	37528.346415	31.572877
557.356232	37578.485865	31.577895
557.831208	37651.218665	31.582912
558.391762	37715.647251	31.587930
558.631243	37767.856029	31.592948
559.322130	37835.318371	31.597965
560.361333	37905.235503	31.602983
560.550580	37983.994059	31.608000
561.449304	38025.490942	31.613018
562.119214	38095.176315	31.618036
562.737450	38155.216563	31.623053
563.303816	38207.988029	31.628071
563.716804	38287.689293	31.633088
564.555476	38321.385848	31.638106
565.236772	38399.743044	31.643124
565.835762	38457.783452	31.648141
566.361921	38515.687747	31.653159
566.907322	38579.777933	31.658176
567.507732	38636.796145	31.663194
568.345342	38696.117114	31.668212
568.883737	38745.249591	31.673229
569.524948	38809.217465	31.678247
569.925942	38874.497125	31.683264
570.261999	38934.551866	31.688282
570.584178	39007.801420	31.693300
571.148441	39071.798715	31.698317
571.756472	39131.206377	31.703335
572.490645	39185.142832	31.708352
573.471923	39237.899281	31.713370
574.050986	39294.998847	31.718388
574.239574	39376.705088	31.723405
574.762864	39429.727113	31.728423
575.500918	39489.796204	31.733440
575.953014	39561.306445	31.738458
576.822313	39628.490387	31.743476
577.021034	39695.008921	31.748493
577.723075	39759.449851	31.753511
577.979158	39830.687381	31.758528
578.673758	39875.545729	31.763546
579.288056	39961.483050	31.768564
579.306401	40034.414510	31.773581
580.018864	40112.183770	31.778599
580.878443	40190.292035	31.783616
581.032408	40266.424572	31.788634
581.442711	40341.154726	31.793652
581.887854	40429.943929	31.798669
582.789412	40502.513599	31.803687
583.277821	40590.838775	31.808704
583.917575	40663.502832	31.813722
584.811389	40739.827626	31.818740
585.235028	40823.474279	31.823757
586.141267	40906.091530	31.828775
587.012777	40967.614350	31.833792
588.198414	41025.597661	31.838810
588.936630	41082.480869	31.843828
589.387449	41137.117002	31.848845
590.344182	41197.638562	31.853863
590.330901	41252.926169	31.858880
590.825743	41316.990198	31.863898
591.672843	41374.916906	31.868916
591.929312	41431.855525	31.873933
592.130960	41487.256696	31.878951
592.458094	41560.749308	31.883968
593.305758	41633.348172	31.888986
593.551807	41683.689025	31.894004
594.075096	41757.443586	31.899021
594.574745	41816.161400	31.904039
595.006714	41890.749127	31.909056
595.778934	41973.405976	31.914074
596.251020	42045.427726	31.919092
596.453387	42130.616292	31.924109
597.489313	42198.997499	31.929127
597.547252	42290.473381	31.934144
598.269435	42372.038631	31.939162
599.299187	42451.713113	31.944180
599.656055	42531.196040	31.949197
600.148474	42616.411557	31.954215
600.666560	42679.371676	31.959232
601.490218	42774.978723	31.964250
602.459486	42835.494166	31.969268
602.923391	42929.860870	31.974285
603.945862	43004.939591	31.979303
604.345343	43075.853574	31.984320
605.156472	43150.011296	31.989338
605.907549	43215.681165	31.994356
606.331176	43306.956492	31.999373
607.101102	43359.589329	32.004391
607.423665	43443.899161	32.009408
608.307242	43523.466692	32.014426
609.257780	43586.194333	32.019444
609.711570	43664.731721	32.024461
610.220421	43737.735815	32.029479
610.993152	43794.306056	32.034496
611.549383	43883.017882	32.039514
612.394279	43950.054438	32.044532
612.892079	44033.738208	32.049549
613.573277	44086.504583	32.054567
613.447603	44181.095033	32.059584
614.321695	44233.820499	32.064602
614.789600	44316.266642	32.069620
615.346107	44410.499345	32.074637
616.132677	44484.047717	32.079655
616.732376	44569.308207	32.084672
617.501136	44634.503495	32.089690
618.223641	44721.004055	32.094708
618.708659	44808.409277	32.099725
619.792172	44859.138246	32.104743
620.322764	44932.525469	32.109760
621.183460	45018.401590	32.114778
622.173862	45072.834010	32.119796
622.760262	45151.728342	32.124813
623.451609	45195.100625	32.129831
623.733479	45278.102696	32.134848
624.462661	45339.174305	32.139866
624.933743	45412.696383	32.144884
625.578479	45483.358085	32.149901
626.303625	45542.400967	32.154919
626.450424	45616.040552	32.159936
627.245016	45690.637414	32.164954
628.210280	45752.182855	32.169972
628.612674	45831.580887	32.174989
629.074755	45894.927443	32.180007
629.533925	45966.685620	32.185024
630.052795	46052.285146	32.190042
630.519244	46119.578330	32.195060
631.143427	46212.779718	32.200077
632.187256	46288.253423	32.205095
632.715207	46361.548838	32.210112
633.195644	46415.497943	32.215130
634.224237	46478.244580	32.220148
634.548793	46554.990591	32.225165
635.265381	46622.266374	32.230183
636.234854	46680.868365	32.235200
636.505205	46747.608927	32.240218
637.520312	46812.265976	32.245236
637.800227	46876.037463	32.250253
638.289105	46936.898246	32.255271
639.040731	47012.539963	32.260288
639.329239	47086.171405	32.265306
640.050466	47171.565815	32.270324
640.516293	47225.131299	32.275341
641.193809	47315.973902	32.280359
641.987576	47382.497661	32.285376
642.414041	47468.516770	32.290394
643.176684	47546.852176	32.295412
643.788212	47643.791807	32.300429
644.313699	47726.960275	32.305447
644.858225	47807.202062	32.310464
645.419282	47891.836809	32.315482
646.129053	47968.237635	32.320500
646.861315	48059.838927	32.325517
647.326499	48151.525825	32.330535
648.122108	48237.863238	32.335552
648.821854	48319.234106	32.340570
649.263389	48397.168228	32.345588
650.086682	48494.850890	32.350605
651.222868	48577.606480	32.355623
652.145581	48652.973923	32.360640
653.062678	48715.901188	32.365658
653.976018	48773.009594	32.370676
654.223331	48864.789621	32.375693
655.117514	48920.376448	32.380711
656.081800	49001.264480	32.385728
656.341467	49074.971611	32.390746
656.839760	49143.896619	32.395764
657.825040	49230.428289	32.400781
658.399745	49292.217217	32.405799
658.838966	49372.580940	32.410816
659.337966	49433.568113	32.415834
660.109317	49523.477445	32.420852
660.729343	49610.206963	32.425869
661.340149	49684.190043	32.430887
662.109236	49769.067257	32.435904
662.751176	49840.683702	32.440922
663.465514	49930.607537	32.445940
664.299563	50001.229694	32.450957
665.175873	50057.264921	32.455975
665.830262	50141.079567	32.460992
666.255938	50203.281345	32.466010
667.121722	50290.800766	32.471028
667.573660	50368.577059	32.476045
668.139610	50433.447030	32.481063
668.523744	50532.201175	32.486080
669.101954	50607.459595	32.491098
669.966226	50686.896529	32.496116
670.122439	50782.032596	32.501133
670.795033	50873.016250	32.506151
671.747745	50948.068891	32.511168
672.124008	51048.203930	32.516186
673.007678	51126.275188	32.521204
673.607085	51217.926303	32.526221
674.160293	51306.297856	32.531239
675.003875	51389.764609	32.536256
675.844530	51469.515040	32.541274
676.669544	51559.848313	32.546292
677.393063	51644.921419	32.551309
677.904261	51706.081233	32.556327
678.780501	51791.780359	32.561344
679.290832	51864.822072	32.566362
679.835004	51930.913484	32.571380
680.535946	52011.655671	32.576397
680.823411	52078.996445	32.581415
681.559877	52179.046318	32.586432
681.711187	52257.151549	32.591450
683.089986	52344.374560	32.596468
683.212979	52442.025733	32.601485
683.724723	52521.749584	32.606503
684.596912	52617.319738	32.611520
685.004237	52713.488273	32.616538
685.561264	52806.859494	32.621556
686.188085	52910.977180	32.626573
687.049825	53010.559031	32.631591
687.446964	53112.410086	32.636608
688.512884	53214.675529	32.641626
689.665738	53301.728577	32.646644
690.356171	53396.861999	32.651661
690.969195	53492.791981	32.656679
691.615653	53595.356129	32.661696
691.949993	53679.242246	32.666714
692.524779	53800.953732	32.671732
693.473534	53904.770916	32.676749
693.842524	54002.733627	32.681767
694.520170	54106.710377	32.686784
695.120925	54209.733843	32.691802
696.163876	54321.598504	32.696820
697.265457	54410.572826	32.701837
697.888420	54525.894104	32.706855
698.926840	54616.648657	32.711872
699.320416	54719.949105	32.716890
700.236314	54832.646320	32.721908
701.202710	54909.168301	32.726925
701.528482	55019.032750	32.731943
702.312103	55100.923963	32.736960
703.204753	55217.506208	32.741978
704.012078	55298.061328	32.746996
704.596606	55404.606381	32.752013
705.339968	55498.389377	32.757031
706.668257	55599.246800	32.762048
706.924952	55678.403452	32.767066
707.352583	55779.751709	32.772084
708.190507	55870.153511	32.777101
708.845069	55956.233043	32.782119
709.470857	56051.826050	32.787136
710.112229	56167.981623	32.792154
710.911049	56262.119239	32.797172
711.822041	56357.710861	32.802189
712.433144	56456.688363	32.807207
713.553849	56545.511313	32.812224
714.008439	56643.814309	32.817242
714.659915	56738.130175	32.822260
715.344280	56829.351516	32.827277
716.315630	56921.877962	32.832295
716.922828	57017.036470	32.837312
717.672895	57123.159158	32.842330
718.798778	57205.154281	32.847348
719.193407	57292.862152	32.852365
719.807765	57393.195930	32.857383
720.427899	57488.304031	32.862400
721.269522	57591.134921	32.867418
721.874433	57688.350504	32.872436
722.649136	57777.830085	32.877453
723.414606	57873.143499	32.882471
724.072649	57975.817157	32.887488
724.671114	58071.614037	32.892506
725.303903	58165.023632	32.897524
725.965927	58249.835620	32.902541
726.660876	58349.427990	32.907559
728.067460	58448.618999	32.912576
728.277928	58531.933435	32.917594
728.862861	58608.564425	32.922612
729.694703	58718.283806	32.927629
730.045646	58787.396976	32.932647
731.061703	58888.676670	32.937664
731.397323	58995.737197	32.942682
732.042127	59102.999992	32.947700
732.691697	59189.119725	32.952717
733.312935	59316.089715	32.957735
733.981014	59422.674267	32.962752
734.634375	59525.792718	32.967770
735.369031	59630.111520	32.972788
736.330803	59732.541889	32.977805
736.660653	59862.451267	32.982823
737.685963	59946.578589	32.987840
738.098800	60074.327151	32.992858
739.058990	60178.061805	32.997876
740.431619	60298.620077	33.002893
740.761548	60395.609943	33.007911
741.751107	60511.057315	33.012928
742.307384	60635.828357	33.017946
743.295317	60739.826751	33.022964
744.199501	60836.426904	33.027981
744.637324	60956.922340	33.032999
745.592646	61066.014927	33.038016
746.449364	61192.294391	33.043034
746.851361	61292.967261	33.048052
747.966496	61408.380097	33.053069
748.399442	61517.074795	33.058087
749.304599	61644.903714	33.063104
750.100184	61743.459961	33.068122
750.486377	61865.214328	33.073140
751.454766	61978.417496	33.078157
752.317792	62098.072210	33.083175
753.099341	62203.192928	33.088192
753.883035	62314.513586	33.093210
754.731068	62433.054150	33.098228
755.640474	62550.182256	33.103245
756.383302	62650.603372	33.108263
757.185553	62761.209269	33.113280
758.148758	62865.203754	33.118298
759.224758	62977.604743	33.123316
760.016771	63067.086150	33.128333
760.928570	63190.720903	33.133351
761.256700	63266.179664	33.138368
762.573288	63385.021303	33.143386
763.309977	63469.501735	33.148404
764.359670	63570.426581	33.153421
764.872519	63661.713729	33.158439
765.483209	63763.735911	33.163456
766.147818	63866.034114	33.168474
766.680588	63962.369243	33.173492
767.334105	64073.158529	33.178509
767.990154	64187.639114	33.183527
768.777475	64301.270685	33.188544
769.416397	64408.891341	33.193562
770.277346	64514.560784	33.198580
771.287557	64622.867071	33.203597
771.606419	64727.293499	33.208615
772.451812	64844.704522	33.213632
773.034449	64961.742446	33.218650
773.971712	65073.975645	33.223668
774.709291	65187.772046	33.228685
775.137740	65302.606165	33.233703
776.705036	65388.720854	33.238720
776.986289	65504.680225	33.243738
777.987435	65589.966415	33.248756
779.395393	65684.584904	33.253773
780.233751	65773.014924	33.258791
780.915246	65865.200572	33.263808
781.865040	65959.162760	33.268826
782.605229	66055.934900	33.273844
783.386356	66134.717470	33.278861
783.611606	66244.767474	33.283879
784.634103	66335.394505	33.288896
784.788461	66441.740478	33.293914
785.596250	66548.352038	33.298932
786.655409	66655.023775	33.303949
786.849785	66772.313097	33.308967
787.436742	66886.415562	33.313984
788.275231	67013.783392	33.319002
788.660069	67131.833454	33.324020
789.650569	67231.603989	33.329037
790.181274	67368.026410	33.334055
791.216636	67497.033540	33.339072
792.054380	67624.443170	33.344090
792.673775	67755.240031	33.349108
793.750854	67869.583035	33.354125
794.357655	68015.631155	33.359143
795.255521	68127.071956	33.364160
796.022972	68257.740056	33.369178
796.656270	68383.032404	33.374196
797.839981	68515.036789	33.379213
798.543596	68659.821727	33.384231
799.430175	68768.227043	33.389248
800.247948	68900.825326	33.394266
800.875874	69031.243140	33.399284
801.762081	69145.036715	33.404301
802.914827	69287.349495	33.409319
803.844288	69394.556122	33.414336
805.137215	69519.702090	33.419354
805.684373	69649.062338	33.424372
806.572840	69753.710808	33.429389
807.062104	69889.928934	33.434407
807.853212	70014.794035	33.439424
808.924494	70121.911409	33.444442
809.287226	70262.654255	33.449460
810.524234	70383.079227	33.454477
811.209160	70509.033257	33.459495
812.173994	70628.379201	33.464512
812.893780	70767.346766	33.469530
813.550822	70876.312971	33.474548
814.340222	71011.666855	33.479565
814.919330	71141.517806	33.484583
815.808877	71258.066215	33.489600
816.492704	71396.613913	33.494618
817.316985	71516.936466	33.499636
818.340724	71667.524992	33.504653
818.868281	71788.068792	33.509671
819.478542	71911.583954	33.514688
820.547118	72056.559557	33.519706
820.942071	72193.857658	33.524724
822.012182	72324.191160	33.529741
822.744380	72465.248008	33.534759
823.814437	72599.528699	33.539776
824.927420	72726.594939	33.544794
825.540115	72865.682425	33.549812
826.793062	72994.352164	33.554829
827.330320	73133.877494	33.559847
827.887810	73270.460129	33.564864
829.071938	73407.654674	33.569882
829.511387	73541.956889	33.574900
830.202111	73660.707482	33.579917
831.240721	73802.354865	33.584935
831.750336	73912.360011	33.589952
832.682340	74052.983299	33.594970
833.419092	74186.582814	33.599988
834.209538	74307.223857	33.605005
834.891292	74440.720208	33.610023
836.306493	74576.733181	33.615040
836.935071	74708.007760	33.620058
837.458842	74834.873917	33.625076
838.471160	74975.913642	33.630093
838.789256	75107.855312	33.635111
839.973790	75259.625041	33.640128
841.100697	75398.454263	33.645146
841.582052	75533.071812	33.650164
842.666960	75667.641120	33.655181
843.822870	75798.917441	33.660199
844.886469	75945.456790	33.665216
845.942570	76057.716135	33.670234
846.655267	76213.611462	33.675252
847.704425	76323.116056	33.680269
848.500018	76465.548268	33.685287
849.046251	76584.718209	33.690304
850.277205	76725.543468	33.695322
851.118275	76865.409497	33.700340
851.854917	76995.314021	33.705357
852.789478	77130.176486	33.710375
853.539040	77259.580827	33.715392
854.480291	77399.060590	33.720410
855.169793	77528.653520	33.725428
855.962720	77681.276355	33.730445
856.749004	77813.694656	33.735463
857.667513	77956.426170	33.740480
858.586140	78085.371071	33.745498
859.332273	78228.828517	33.750516
860.401877	78372.846972	33.755533
861.349501	78508.183763	33.760551
862.473049	78649.785421	33.765568
863.528505	78780.191777	33.770586
863.961319	78916.868384	33.775604
864.910983	79061.164127	33.780621
865.725695	79188.551429	33.785639
866.431469	79334.742414	33.790656
867.584659	79476.667043	33.795674
868.089278	79622.956393	33.800692
869.439761	79746.640540	33.805709
870.107768	79892.411333	33.810727
870.719245	80035.086790	33.815744
871.754713	80185.454104	33.820762
872.046025	80331.511355	33.825780
873.147495	80480.895686	33.830797
873.930876	80626.026031	33.835815
874.878170	80778.176653	33.840832
875.552020	80926.989398	33.845850
876.225892	81074.651906	33.850868
876.852133	81224.157631	33.855885
878.023819	81388.647918	33.860903
878.992568	81540.053770	33.865920
880.070867	81704.599749	33.870938
881.005196	81853.065677	33.875956
882.135061	81980.037343	33.880973
882.886718	82141.907779	33.885991
883.554101	82285.998980	33.891008
884.618361	82430.050871	33.896026
885.558990	82589.122623	33.901044
886.505791	82715.540362	33.906061
887.423638	82866.451146	33.911079
888.540710	83007.752562	33.916096
889.467211	83151.338378	33.921114
889.977576	83285.201139	33.926132
891.114234	83430.341853	33.931149
892.133546	83558.144060	33.936167
892.771988	83687.509171	33.941184
893.780429	83818.338530	33.946202
894.270468	83952.739981	33.951220
895.269568	84099.021095	33.956237
896.356218	84237.317574	33.961255
897.152121	84385.139735	33.966272
897.907222	84528.294406	33.971290
898.785259	84664.805932	33.976308
899.485697	84823.180155	33.981325
900.161102	84966.932767	33.986343
901.056209	85138.328571	33.991360
901.773055	85283.556737	33.996378
902.231989	85435.648499	34.001396
903.533136	85590.006332	34.006413
904.435300	85758.273908	34.011431
905.567421	85917.349939	34.016448
906.855981	86080.406098	34.021466
907.622852	86227.118763	34.026484
908.900750	86368.060123	34.031501
909.879186	86544.520478	34.036519
911.013676	86686.449155	34.041536
912.192431	86824.619486	34.046554
912.939031	86976.768825	34.051572
913.581312	87125.298319	34.056589
914.122312	87281.786023	34.061607
914.810478	87438.680730	34.066624
915.597383	87602.216415	34.071642
916.545932	87768.744660	34.076660
917.556893	87927.734308	34.081677
918.793035	88103.227533	34.086695
919.162271	88277.378284	34.091712
919.980820	88436.592996	34.096730
921.101116	88603.832832	34.101748
922.020843	88764.089758	34.106765
923.227099	88936.044438	34.111783
924.188595	89087.520345	34.116800
925.637224	89247.237660	34.121818
926.343373	89425.049325	34.126836
927.523115	89573.929618	34.131853
928.816271	89732.397703	34.136871
929.691208	89895.365390	34.141888
930.702372	90045.371217	34.146906
931.501940	90196.425402	34.151924
932.367131	90359.119476	34.156941
933.399327	90529.374364	34.161959
934.186986	90688.077882	34.166976
935.097334	90831.258409	34.171994
935.825100	90998.187742	34.177012
936.814331	91155.367672	34.182029
937.719333	91327.187040	34.187047
938.400726	91471.763475	34.192064
939.717975	91631.214861	34.197082
940.615009	91792.698484	34.202100
941.359220	91958.954717	34.207117
942.632540	92124.903252	34.212135
943.156497	92286.875825	34.217152
944.533958	92454.372587	34.222170
945.258126	92609.036500	34.227188
945.980272	92765.328194	34.232205
947.256903	92937.218041	34.237223
948.044165	93098.886829	34.242240
948.989557	93253.214595	34.247258
950.041230	93428.758805	34.252276
950.784236	93588.583866	34.257293
951.723715	93738.675421	34.262311
952.310304	93910.470982	34.267328
953.469492	94060.275107	34.272346
954.449171	94204.141582	34.277364
955.217653	94376.853443	34.282381
956.450190	94522.148392	34.287399
957.091986	94699.528998	34.292416
958.296310	94848.805240	34.297434
959.106905	95011.919704	34.302452
960.076486	95163.610084	34.307469
961.163135	95343.187803	34.312487
961.751852	95507.734665	34.317504
962.571232	95675.681392	34.322522
963.206329	95846.666165	34.327540
964.062809	96014.438203	34.332557
965.321521	96177.252290	34.337575
965.996144	96372.203976	34.342592
967.375284	96539.083136	34.347610
968.526718	96725.983645	34.352628
969.678043	96899.276804	34.357645
970.786723	97063.058339	34.362663
971.491041	97260.588369	34.367680
972.365203	97423.607145	34.372698
973.035679	97605.738791	34.377716
973.877626	97796.262234	34.382733
975.050787	97981.421633	34.387751
975.671592	98174.231631	34.392768
976.951897	98369.725790	34.397786
977.690412	98546.833402	34.402804
978.641729	98746.505738	34.407821
980.124502	98920.302740	34.412839
980.862173	99128.533849	34.417856
982.002899	99308.656974	34.422874
982.780798	99496.671926	34.427892
984.051998	99685.777965	34.432909
985.419965	99863.911490	34.437927
986.126764	100054.993643	34.442944
986.820259	100232.013035	34.447962
987.985641	100434.170407	34.452980
988.922401	100626.105220	34.457997
990.095909	100813.570944	34.463015
990.913838	101006.655137	34.468032
992.324316	101204.245439	34.473050
993.486402	101373.547933	34.478068
994.063137	101582.357760	34.483085
995.828086	101750.031173	34.488103
996.805337	101943.463412	34.493120
998.343190	102112.164345	34.498138
999.476084	102291.056583	34.503156
1000.428807	102463.490474	34.508173
1001.441242	102616.409503	34.513191
1001.995219	102816.224059	34.518208
1002.974708	102984.123941	34.523226
1003.693245	103169.586580	34.528244
1004.695934	103358.872071	34.533261
1005.942157	103544.345274	34.538279
1006.484547	103722.142084	34.543296
1007.543407	103933.936976	34.548314
1008.657671	104110.863293	34.553332
1009.390344	104291.709730	34.558349
1010.055511	104489.461224	34.563367
1011.232203	104686.635912	34.568384
1012.351485	104880.294844	34.573402
1013.229704	105078.838794	34.578420
1014.084671	105267.725827	34.583437
1015.572727	105461.961405	34.588455
1016.173830	105649.234195	34.593472
1017.050844	105852.286220	34.598490
1018.441730	106029.357287	34.603508
1019.024195	106215.864736	34.608525
1020.265551	106393.988754	34.613543
1021.156787	106571.924843	34.618560
1022.119361	106764.933498	34.623578
1023.324890	106936.526041	34.628596
1024.111819	107141.762240	34.633613
1025.478555	107332.834015	34.638631
1026.289404	107517.400687	34.643648
1027.231317	107714.105144	34.648666
1028.210937	107901.635521	34.653684
1028.973337	108099.980928	34.658701
1030.196287	108285.434810	34.663719
1030.889476	108495.091787	34.668736
1031.991299	108700.604766	34.673754
1033.099334	108896.720670	34.678772
1033.963952	109116.473824	34.683789
1035.326228	109298.568134	34.688807
1036.566645	109497.972310	34.693824
1037.299795	109712.001919	34.698842
1039.128280	109901.496131	34.703860
1039.951478	110114.944144	34.708877
1041.369803	110303.052347	34.713895
1042.074667	110512.507959	34.718912
1043.224033	110710.910269	34.723930
1044.487559	110914.374360	34.728948
1044.928283	111094.897776	34.733965
1046.169838	111305.132268	34.738983
1047.193755	111511.389044	34.744000
1048.208063	111718.662311	34.749018
1049.655023	111904.484329	34.754036
1050.489578	112124.077086	34.759053
1051.780284	112321.099887	34.764071
1052.304475	112542.317964	34.769088
1053.576204	112741.817015	34.774106
1055.057710	112950.517278	34.779124
1055.532494	113168.505796	34.784141
1056.760486	113366.230549	34.789159
1057.781484	113580.876659	34.794176
1059.105504	113787.189825	34.799194
1060.253416	113993.698299	34.804212
1061.367166	114205.787785	34.809229
1062.351118	114400.266665	34.814247
1063.440826	114618.253857	34.819264
1064.134804	114832.672370	34.824282
1065.428857	115045.181931	34.829300
1066.167414	115268.261484	34.834317
1067.037747	115472.457891	34.839335
1067.994280	115705.094917	34.844352
1069.190770	115928.256194	34.849370
1070.185795	116135.718047	34.854388
1071.286028	116378.915310	34.859405
1072.367870	116584.225143	34.864423
1073.265415	116813.979992	34.869440
1074.485456	117037.298275	34.874458
1075.831573	117262.979325	34.879476
1077.056505	117492.153575	34.884493
1078.275575	117686.033811	34.889511
1079.635492	117901.126124	34.894528
1080.844221	118115.117448	34.899546
1081.794511	118325.998317	34.904564
1082.806366	118542.103195	34.909581
1084.215821	118757.358551	34.914599
1084.978411	118972.658982	34.919616
1085.641951	119182.275882	34.924634
1086.963281	119409.980025	34.929652
1087.995472	119626.292508	34.934669
1089.184116	119836.575071	34.939687
1090.233265	120038.367695	34.944704
1091.237084	120255.994675	34.949722
1092.335777	120454.373684	34.954740
1093.106914	120665.858938	34.959757
1093.927670	120872.598684	34.964775
1094.829935	121098.788908	34.969792
1096.065774	121309.441913	34.974810
1097.186851	121534.446367	34.979828
1098.126107	121746.494650	34.984845
1099.216464	121969.860305	34.989863
1100.379294	122187.310866	34.994880
1101.499385	122416.668594	34.999898
1102.826941	122638.213548	35.004916
1104.001128	122858.074833	35.009933
1105.001141	123090.524215	35.014951
1106.420734	123304.227891	35.019968
1107.623795	123543.198680	35.024986
1108.555354	123755.706345	35.030004
1109.683199	123986.329617	35.035021
1110.935553	124207.696089	35.040039
1111.624839	124440.435538	35.045056
1112.609126	124668.958891	35.050074
1114.057548	124888.194467	35.055092
1115.116903	125116.442754	35.060109
1116.553364	125358.811298	35.065127
1118.397891	125572.499249	35.070144
1118.953093	125799.467338	35.075162
1120.537438	126020.399657	35.080180
1121.457938	126250.517129	35.085197
1122.498592	126473.811032	35.090215
1123.769227	126704.152992	35.095232
1124.205255	126930.325548	35.100250
1125.677572	127158.381828	35.105268
1126.573108	127396.610536	35.110285
1127.864550	127625.409922	35.115303
1129.218823	127860.119312	35.120320
1129.564736	128093.526814	35.125338
1131.235179	128345.373521	35.130356
1131.891323	128585.247998	35.135373
1133.344136	128817.540435	35.140391
1134.720779	129055.664698	35.145408
1135.852625	129291.220307	35.150426
1137.867140	129505.516376	35.155444
1138.833137	129754.094228	35.160461
1140.170076	129971.496596	35.165479
1141.336161	130197.927762	35.170496
1142.537591	130413.745926	35.175514
1143.584428	130641.632282	35.180532
1144.605355	130879.740647	35.185549
1145.493594	131113.411105	35.190567
1146.780966	131332.909933	35.195584
1147.647438	131570.935010	35.200602
1149.230464	131806.942303	35.205620
1150.419574	132032.381679	35.210637
1151.646440	132243.962049	35.215655
1152.962021	132483.795913	35.220672
1154.163192	132708.502967	35.225690
1155.016461	132925.359332	35.230708
1155.953115	133164.817280	35.235725
1157.106325	133397.953983	35.240743
1157.939309	133635.543880	35.245760
1158.762126	133881.883824	35.250778
1159.924564	134102.842337	35.255796
1161.031183	134369.066366	35.260813
1162.107302	134601.349948	35.265831
1163.595847	134849.704449	35.270848
1164.210036	135095.619166	35.275866
1165.515705	135342.866773	35.280884
1166.631816	135576.000160	35.285901
1167.754133	135810.579385	35.290919
1168.861015	136024.980966	35.295936
1169.925139	136269.993684	35.300954
1171.358172	136500.660089	35.305972
1172.169151	136750.459518	35.310989
1173.145294	136989.014062	35.316007
1174.546277	137237.071761	35.321024
1175.603903	137476.186905	35.326042
1176.826688	137724.860894	35.331060
1177.891897	137979.318515	35.336077
1178.884137	138222.519479	35.341095
1180.289807	138484.189253	35.346112
1181.356484	138736.624002	35.351130
1182.431344	138998.504599	35.356148
1183.530574	139235.191434	35.361165
1184.863623	139504.792534	35.366183
1186.421793	139753.641972	35.371200
1187.146951	140032.564968	35.376218
1188.309890	140264.519481	35.381236
1189.772517	140530.329225	35.386253
1191.175402	140790.445434	35.391271
1192.527546	141065.419140	35.396288
1193.447294	141320.534919	35.401306
1194.782791	141584.243886	35.406324
1195.709387	141848.352068	35.411341
1196.701391	142132.561033	35.416359
1197.944010	142400.830905	35.421376
1199.081077	142673.646930	35.426394
1200.591454	142964.966602	35.431412
1201.789496	143219.999972	35.436429
1202.835118	143505.555567	35.441447
1204.432932	143769.288842	35.446464
1205.334371	144036.537354	35.451482
1206.821078	144322.001540	35.456500
1208.147010	144577.442288	35.461517
1209.736988	144859.077078	35.466535
1211.497303	145102.441639	35.471552
1212.736981	145374.082789	35.476570
1213.994770	145643.186921	35.481588
1215.666118	145897.401018	35.486605
1216.751842	146135.203131	35.491623
1218.207517	146411.191559	35.496640
1219.340102	146654.366171	35.501658
1220.442547	146912.156110	35.506676
1221.630775	147148.680014	35.511693
1222.688911	147415.028072	35.516711
1224.207560	147652.933781	35.521728
1225.552768	147919.555260	35.526746
1226.785875	148163.611311	35.531764
1227.609773	148419.403718	35.536781
1228.486469	148692.347673	35.541799
1229.974199	148941.870876	35.546816
1231.016384	149219.800846	35.551834
1232.088552	149474.874936	35.556852
1233.216067	149735.699378	35.561869
1234.108489	150011.047613	35.566887
1235.466931	150286.346370	35.571904
1236.449132	150554.708606	35.576922
1237.537321	150834.469585	35.581940
1238.936529	151107.865414	35.586957
1239.589199	151389.414661	35.591975
1241.096017	151669.607515	35.596992
1242.100275	151969.328352	35.602010
1243.312983	152244.196547	35.607028
1244.500724	152541.012670	35.612045
1245.295889	152829.512355	35.617063
1246.692105	153119.525834	35.622080
1247.737394	153420.735513	35.627098
1249.074300	153679.891712	35.632116
1250.572543	153953.482350	35.637133
1251.796188	154236.062292	35.642151
1253.400966	154518.023346	35.647168
1254.909032	154787.800577	35.652186
1256.309730	155073.097241	35.657204
1257.554793	155339.763487	35.662221
1258.736623	155629.425693	35.667239
1260.022006	155910.435027	35.672256
1260.935364	156197.380666	35.677274
1261.992327	156466.939759	35.682292
1263.418493	156749.010141	35.687309
1264.856922	157036.611038	35.692327
1266.416936	157313.386632	35.697344
1267.349583	157595.265551	35.702362
1268.486535	157889.937195	35.707380
1270.308739	158165.330947	35.712397
1271.085575	158452.696288	35.717415
1272.444874	158743.468684	35.722432
1273.852876	159037.964645	35.727450
1274.923516	159331.605134	35.732468
1276.164390	159630.331924	35.737485
1277.779180	159939.946854	35.742503
1279.312753	160203.516062	35.747520
1280.508396	160508.916835	35.752538
1282.164725	160774.461187	35.757556
1283.537286	161070.842786	35.762573
1284.397554	161375.595067	35.767591
1285.979646	161657.877614	35.772608
1287.047141	161964.300039	35.777626
1288.365430	162245.488444	35.782644
1289.704931	162537.522110	35.787661
1290.666161	162857.543160	35.792679
1291.983344	163140.298309	35.797696
1292.943394	163448.639838	35.802714
1294.167550	163764.514046	35.807732
1295.869826	164068.551051	35.812749
1297.000911	164375.209248	35.817767
1298.278685	164681.946977	35.822784
1299.651828	164989.660801	35.827802
1301.580077	165291.969318	35.832820
1302.770870	165589.999234	35.837837
1303.894861	165914.000640	35.842855
1305.339232	166202.794658	35.847872
1306.469969	166507.933216	35.852890
1307.658780	166807.507177	35.857908
1309.329988	167119.424898	35.862925
1310.463239	167420.966217	35.867943
1311.923969	167738.734182	35.872960
1313.347168	168041.741833	35.877978
1314.649090	168351.724688	35.882996
1316.348171	168653.105045	35.888013
1317.871128	168948.819517	35.893031
1319.494744	169245.712072	35.898048
1320.699620	169541.280015	35.903066
1321.858405	169841.552296	35.908084
1323.119872	170130.694441	35.913101
1323.902025	170439.255145	35.918119
1325.393933	170737.232590	35.923136
1326.870489	171059.298023	35.928154
1327.733551	171354.236520	35.933172
1329.227402	171665.479761	35.938189
1330.154837	171975.537029	35.943207
1331.579835	172291.770074	35.948224
1332.470537	172606.735744	35.953242
1333.547455	172926.850120	35.958260
1335.035647	173240.820588	35.963277
1336.058255	173564.602938	35.968295
1337.330209	173867.383094	35.973312
1338.272805	174185.409201	35.978330
1339.604229	174501.431761	35.983348
1341.267529	174809.445110	35.988365
1342.200096	175129.535063	35.993383
1343.605514	175463.254437	35.998400
1344.966096	175778.722414	36.003418
1346.026313	176092.401978	36.008436
1347.433223	176430.912141	36.013453
1348.819933	176766.547309	36.018471
1350.030863	177095.525935	36.023488
1351.631283	177428.820782	36.028506
1352.786712	177759.615161	36.033524
1353.983956	178120.152084	36.038541
1355.340804	178455.499325	36.043559
1356.894731	178806.502365	36.048576
1358.689658	179149.333170	36.053594
1360.132520	179498.493889	36.058612
1361.731800	179826.221150	36.063629
1363.238367	180168.941618	36.068647
1364.320035	180497.710571	36.073664
1365.785556	180830.669969	36.078682
1367.388825	181185.920605	36.083700
1368.829237	181520.411684	36.088717
1370.190153	181863.561158	36.093735
1371.453500	182190.115449	36.098752
1372.583025	182543.829193	36.103770
1374.203604	182895.192456	36.108788
1375.793568	183226.636601	36.113805
1377.603420	183567.794146	36.118823
1379.075804	183907.486552	36.123840
1380.796965	184229.117010	36.128858
1381.928852	184575.838020	36.133876
1383.280164	184910.314922	36.138893
1384.640820	185255.365294	36.143911
1386.012027	185592.165940	36.148928
1387.471943	185933.929610	36.153946
1388.542952	186270.314426	36.158964
1390.262290	186605.655061	36.163981
1391.735042	186951.789403	36.168999
1393.123072	187296.721392	36.174016
1394.655049	187638.598141	36.179034
1395.987224	187972.970231	36.184052
1397.354936	188319.460555	36.189069
1398.475448	188664.749889	36.194087
1399.406881	189004.030491	36.199104
1401.105769	189366.542544	36.204122
1402.291507	189714.442440	36.209140
1403.983265	190074.992711	36.214157
1405.105454	190429.482798	36.219175
1406.462243	190777.234022	36.224192
1407.963917	191142.709520	36.229210
1409.125589	191486.739831	36.234228
1410.813089	191846.273705	36.239245
1411.760878	192211.669626	36.244263
1413.449834	192576.564675	36.249280
1414.746834	192949.727187	36.254298
1415.975088	193321.735510	36.259316
1417.341523	193698.686882	36.264333
1418.530260	194067.710475	36.269351
1419.744563	194432.898333	36.274368
1421.243255	194803.360533	36.279386
1422.750222	195200.939650	36.284404
1424.569703	195563.127301	36.289421
1425.749488	195963.177365	36.294439
1427.245377	196328.825147	36.299456
1428.695999	196690.978702	36.304474
1429.729569	197068.856301	36.309492
1431.456668	197410.262576	36.314509
1432.762604	197774.299732	36.319527
1434.208045	198132.095214	36.324544
1435.618311	198494.011818	36.329562
1436.631572	198859.779234	36.334580
1438.309697	199217.720073	36.339597
1439.984692	199582.684087	36.344615
1441.320309	199965.708674	36.349632
1442.573911	200311.753473	36.354650
1444.139088	200697.918356	36.359668
1446.074507	201054.823721	36.364685
1447.572916	201423.750037	36.369703
1448.906403	201795.447934	36.374720
1450.782886	202147.887081	36.379738
1452.017476	202536.097613	36.384756
1453.607902	202895.507238	36.389773
1454.853004	203277.600596	36.394791
1456.008075	203651.483628	36.399808
1457.860789	204014.918584	36.404826
1459.319659	204399.610937	36.409844
1460.890806	204760.582267	36.414861
1462.265362	205159.182718	36.419879
1463.262798	205549.010671	36.424896
1464.947711	205915.695241	36.429914
1466.094245	206317.526580	36.434932
1467.533485	206699.415688	36.439949
1468.812800	207097.496452	36.444967
1470.161381	207503.198854	36.449984
1471.915471	207895.542607	36.455002
1473.006212	208310.522723	36.460020
1474.534293	208695.340356	36.465037
1475.875507	209109.420046	36.470055
1477.196643	209523.429076	36.475072
1478.838733	209936.727062	36.480090
1480.240627	210361.824789	36.485108
1482.039513	210765.743136	36.490125
1483.405473	211187.600604	36.495143
1484.728585	211593.747534	36.500160
1486.472691	212009.629726	36.505178
1488.023174	212452.173428	36.510196
1489.907910	212860.710030	36.515213
1491.647534	213272.828020	36.520231
1493.110568	213692.231569	36.525248
1494.831937	214089.449022	36.530266
1496.079714	214492.181294	36.535284
1497.764042	214969.585302	36.540301
1499.215434	215392.859325	36.545319
1500.357841	215821.164135	36.550336
1502.213158	216223.346963	36.555354
1503.272393	216637.853519	36.560372
1504.829700	217064.571978	36.565389
1506.254410	217478.691892	36.570407
1508.120743	217900.258399	36.575424
1509.886707	218300.052368	36.580442
1511.350206	218715.161881	36.585460
1513.113946	219141.271650	36.590477
1514.868550	219527.129345	36.595495
1516.330352	219949.559046	36.600512
1518.058220	220350.612357	36.605530
1519.510881	220762.735485	36.610548
1521.162617	221171.500302	36.615565
1522.729208	221581.576144	36.620583
1524.025385	221987.075754	36.625600
1525.875768	222376.713046	36.630618
1527.129935	222783.695831	36.635636
1528.647112	223195.106965	36.640653
1530.317970	223576.599964	36.645671
1531.532650	223982.222338	36.650688
1533.486127	224346.323999	36.655706
1534.750657	224742.644965	36.660724
1536.177125	225129.034964	36.665741
1537.606466	225516.746589	36.670759
1538.787336	225916.870017	36.675776
1540.585756	226298.783166	36.680794
1541.731541	226710.116292	36.685812
1543.253642	227104.447248	36.690829
1545.104358	227489.048026	36.695847
1546.688168	227901.176615	36.700864
1548.149811	228287.139542	36.705882
1549.456576	228697.055966	36.710900
1550.739090	229101.161151	36.715917
1553.134436	229508.436819	36.720935
1554.904717	229917.442552	36.725952
1556.666147	230294.497549	36.730970
1557.915934	230714.564599	36.735988
1559.193549	231107.653177	36.741005
1561.180761	231519.625373	36.746023
1562.849329	231931.422801	36.751040
1564.209517	232318.709952	36.756058
1565.812100	232738.217065	36.761076
1567.084519	233146.095556	36.766093
1568.919853	233556.015994	36.771111
1570.066652	233980.885342	36.776128
1571.410900	234399.779504	36.781146
1572.933943	234828.881964	36.786164
1573.930895	235254.694098	36.791181
1575.492112	235700.328839	36.796199
1577.034058	236137.433198	36.801216
1578.915302	236588.478907	36.806234
1580.328003	237027.410505	36.811252
1582.116226	237463.182324	36.816269
1583.807074	237917.743082	36.821287
1584.968779	238373.586234	36.826304
1586.783995	238821.905449	36.831322
1588.088573	239270.614873	36.836340
1589.738094	239726.914429	36.841357
1591.500605	240183.933117	36.846375
1592.451891	240646.116348	36.851392
1594.049676	241107.660562	36.856410
1595.826918	241575.602958	36.861428
1597.250531	242041.318597	36.866445
1599.002435	242515.186010	36.871463
1600.800425	242979.597251	36.876480
1602.508271	243450.095500	36.881498
1604.299014	243916.745311	36.886516
1605.868368	244390.926303	36.891533
1607.449174	244859.975071	36.896551
1608.529196	245345.923818	36.901568
1610.045382	245826.619428	36.906586
1611.442681	246319.452581	36.911604
1612.962437	246784.044139	36.916621
1614.683714	247285.945143	36.921639
1615.982748	247786.214730	36.926656
1617.631687	248270.093469	36.931674
1619.297541	248780.490699	36.936692
1620.650148	249279.102725	36.941709
1622.500346	249768.412166	36.946727
1624.278336	250274.322317	36.951744
1625.756318	250769.486441	36.956762
1627.907525	251279.324668	36.961780
1629.471056	251772.469145	36.966797
1631.507610	252258.829767	36.971815
1632.894167	252733.130124	36.976832
1634.747341	253236.542128	36.981850
1636.392145	253727.211277	36.986868
1637.876338	254208.711465	36.991885
1639.797839	254669.258533	36.996903
1641.265094	255135.952277	37.001920
1643.041956	255609.428747	37.006938
1644.384517	256072.257059	37.011956
1646.124264	256551.862471	37.016973
1647.788454	257010.472163	37.021991
1649.488584	257499.204427	37.027008
1651.565950	257952.157705	37.032026
1653.019948	258428.102380	37.037044
1654.558737	258898.520735	37.042061
1656.516524	259369.911646	37.047079
1658.123511	259859.269892	37.052096
1659.658295	260336.954643	37.057114
1661.449014	260802.251237	37.062132
1663.326079	261282.292957	37.067149
1665.087327	261771.422793	37.072167
1666.800609	262251.618578	37.077184
1668.774290	262705.961612	37.082202
1670.807473	263189.991240	37.087220
1672.320684	263660.617427	37.092237
1674.111144	264117.937248	37.097255
1675.733215	264607.851740	37.102272
1677.525284	265065.933117	37.107290
1679.152338	265553.179093	37.112308
1680.469286	266034.023587	37.117325
1682.336996	266490.974133	37.122343
1683.723597	266991.062280	37.127360
1685.636101	267470.740771	37.132378
1687.317395	267971.059073	37.137396
1688.765918	268437.629185	37.142413
1690.816939	268927.318011	37.147431
1692.453509	269405.160731	37.152448
1694.382652	269909.043737	37.157466
1695.923772	270387.688792	37.162484
1697.320358	270897.577557	37.167501
1699.247071	271380.222446	37.172519
1700.555014	271886.542851	37.177536
1702.232904	272378.423508	37.182554
1703.925890	272872.231668	37.187572
1705.546713	273396.382118	37.192589
1707.209294	273889.304793	37.197607
1708.619898	274426.799446	37.202624
1710.148386	274936.000474	37.207642
1711.709523	275443.848934	37.212660
1713.267943	275965.770062	37.217677
1715.283108	276497.090068	37.222695
1716.638875	277032.353635	37.227712
1718.162465	277561.669654	37.232730
1720.002356	278102.007882	37.237748
1721.420554	278629.078243	37.242765
1723.230842	279159.232661	37.247783
1724.808947	279719.170288	37.252800
1726.473486	280264.308171	37.257818
1728.449843	280808.910620	37.262836
1729.861257	281339.582925	37.267853
1731.665633	281916.268360	37.272871
1733.444690	282461.102257	37.277888
1735.004962	283008.256916	37.282906
1736.905239	283575.370563	37.287924
1738.642650	284131.815224	37.292941
1740.724097	284687.490183	37.297959
1742.712858	285233.221274	37.302976
1744.981603	285785.483453	37.307994
1746.509751	286328.746909	37.313012
1748.539375	286879.444653	37.318029
1750.275059	287418.123428	37.323047
1751.684810	287951.138888	37.328064
1753.585298	288486.738678	37.333082
1755.677661	288996.548322	37.338100
1756.947896	289518.023882	37.343117
1759.239682	290037.576400	37.348135
1761.037425	290546.972063	37.353152
1762.644065	291071.993415	37.358170
1764.399720	291581.849482	37.363188
1765.983790	292103.085957	37.368205
1768.227221	292616.540729	37.373223
1769.931647	293131.098441	37.378240
1771.489482	293659.521383	37.383258
1773.007945	294167.323807	37.388276
1774.485829	294702.054810	37.393293
1776.772068	295241.222114	37.398311
1778.359536	295780.324518	37.403328
1780.135434	296310.046363	37.408346
1781.552654	296856.131472	37.413364
1783.325783	297397.126229	37.418381
1785.033349	297936.884685	37.423399
1786.603362	298499.954239	37.428416
1788.375661	299046.605225	37.433434
1790.180637	299608.766791	37.438452
1791.526817	300178.646131	37.443469
1793.342884	300746.209822	37.448487
1795.405816	301314.999633	37.453504
1797.074950	301887.229249	37.458522
1798.892284	302452.649891	37.463540
1800.444996	303053.363439	37.468557
1802.668550	303620.742274	37.473575
1804.610544	304203.250496	37.478592
1806.469960	304774.898661	37.483610
1808.694457	305337.314693	37.488628
1810.825430	305926.130515	37.493645
1812.600023	306484.804247	37.498663
1814.144561	307062.382430	37.503680
1816.436962	307630.538321	37.508698
1818.724324	308196.354928	37.513716
1820.231148	308766.436277	37.518733
1822.653142	309339.512047	37.523751
1824.389248	309909.116289	37.528768
1825.951453	310475.520110	37.533786
1828.125820	311021.781862	37.538804
1830.009024	311611.031982	37.543821
1831.886356	312159.493814	37.548839
1833.929598	312731.694499	37.553856
1836.059708	313284.297183	37.558874
1838.104424	313847.652129	37.563892
1839.659435	314417.457877	37.568909
1841.549698	314962.012786	37.573927
1843.174678	315529.564059	37.578944
1845.028457	316087.220423	37.583962
1847.096428	316649.992283	37.588980
1848.671231	317212.993601	37.593997
1850.390229	317774.214672	37.599015
1852.057376	318344.632367	37.604032
1853.547639	318923.454471	37.609050
1855.511953	319483.199760	37.614068
1857.276442	320067.452182	37.619085
1859.179715	320639.843917	37.624103
1861.253934	321214.894311	37.629120
1863.352319	321790.418350	37.634138
1865.283787	322356.823973	37.639156
1867.157884	322936.920406	37.644173
1868.743954	323511.168493	37.649191
1870.856077	324081.820822	37.654208
1872.256105	324673.837915	37.659226
1873.747460	325245.775832	37.664244
1875.333786	325817.870728	37.669261
1877.041074	326402.102494	37.674279
1878.788917	326969.666270	37.679296
1880.341810	327566.556941	37.684314
1882.045265	328132.111651	37.689332
1883.670883	328718.848732	37.694349
1885.630908	329315.782205	37.699367
1887.068611	329890.529902	37.704384
1888.867039	330521.549919	37.709402
1890.719573	331107.236108	37.714420
1892.441612	331730.918577	37.719437
1894.196351	332335.852775	37.724455
1895.426518	332975.495785	37.729472
1897.478791	333590.852760	37.734490
1899.694227	334237.021334	37.739508
1901.532331	334864.204719	37.744525
1903.579972	335493.098153	37.749543
1905.831297	336131.572174	37.754560
1907.465008	336778.289485	37.759578
1909.572428	337396.946133	37.764596
1911.373780	338057.455619	37.769613
1913.013545	338694.832576	37.774631
1914.959838	339358.982817	37.779648
1916.839930	340025.547091	37.784666
1918.919472	340683.896313	37.789684
1920.679398	341361.657561	37.794701
1922.240212	342007.561298	37.799719
1924.736429	342679.599267	37.804736
1926.677318	343342.176016	37.809754
1928.848335	344008.386451	37.814772
1930.490836	344682.340455	37.819789
1932.699989	345361.598030	37.824807
1934.852943	346040.855414	37.829824
1936.326181	346713.794024	37.834842
1938.200574	347398.560485	37.839860
1940.073782	348098.393091	37.844877
1942.103839	348790.524770	37.849895
1943.760052	349475.880837	37.854912
1945.819618	350171.667172	37.859930
1948.011721	350869.908251	37.864948
1949.848437	351576.343703	37.869965
1951.925922	352271.790603	37.874983
1953.958942	352974.974216	37.880000
1955.370463	353676.980428	37.885018
1957.708049	354385.420701	37.890036
1959.980587	355091.449557	37.895053
1962.716637	355778.079551	37.900071
1964.588338	356476.691554	37.905088
1966.800359	357174.652456	37.910106
1969.247870	357851.527581	37.915124
1971.109781	358542.495038	37.920141
1973.168696	359229.181246	37.925159
1975.933025	359906.047203	37.930176
1977.948923	360575.337572	37.935194
1980.507969	361240.366394	37.940212
1982.364138	361910.600146	37.945229
1984.293511	362575.888673	37.950247
1986.461211	363235.545257	37.955264
1988.059989	363902.794616	37.960282
1989.646597	364560.723872	37.965300
1991.749564	365232.637391	37.970317
1993.729148	365915.620925	37.975335
1995.960694	366597.510839	37.980352
1997.374503	367254.104244	37.985370
1999.127460	367930.874411	37.990388
2001.270910	368608.861989	37.995405
2002.755976	369283.217102	38.000423
2005.243075	369977.231840	38.005440
2006.642955	370653.123917	38.010458
2008.965629	371314.291513	38.015476
2010.437937	371982.385562	38.020493
2012.112582	372644.270451	38.025511
2013.944979	373323.492139	38.030528
2015.389781	373996.119717	38.035546
2017.752529	374685.577063	38.040564
2019.214972	375375.930611	38.045581
2021.199879	376083.558106	38.050599
2023.195526	376769.231508	38.055616
2024.854544	377487.587598	38.060634
2026.626634	378183.871549	38.065652
2028.557891	378908.772883	38.070669
2030.482741	379632.696469	38.075687
2032.711680	380360.206498	38.080704
2034.648032	381109.735612	38.085722
2036.858832	381827.555650	38.090740
2038.414322	382576.075559	38.095757
2040.451638	383324.499368	38.100775
2042.931602	384055.058342	38.105792
2044.112023	384843.348814	38.110810
2046.426306	385592.284468	38.115828
2048.331997	386372.304963	38.120845
2050.432338	387138.405869	38.125863
2052.788315	387923.461865	38.130880
2054.716230	388704.994551	38.135898
2057.150283	389473.013201	38.140916
2059.905549	390240.656127	38.145933
2062.085501	391006.296512	38.150951
2064.328373	391766.584241	38.155968
2066.443973	392546.140548	38.160986
2068.622022	393324.526287	38.166004
2070.699509	394090.259953	38.171021
2072.406707	394879.229184	38.176039
2074.510544	395642.030028	38.181056
2076.384316	396428.548988	38.186074
2078.497583	397216.883577	38.191092
2080.658565	398002.325544	38.196109
2082.689653	398792.659817	38.201127
2084.927822	399572.268974	38.206144
2087.178305	400371.547406	38.211162
2089.492556	401153.712468	38.216180
2091.684318	401948.598504	38.221197
2093.729778	402753.446057	38.226215
2095.958609	403510.448245	38.231232
2098.033933	404316.742202	38.236250
2100.415572	405095.368283	38.241268
2103.030324	405889.923218	38.246285
2105.094674	406666.277871	38.251303
2107.629958	407450.337226	38.256320
2109.238412	408221.149698	38.261338
2112.225640	409008.840373	38.266356
2114.598071	409772.592265	38.271373
2116.785948	410536.733349	38.276391
2119.053644	411300.713207	38.281408
2120.573604	412076.726716	38.286426
2122.726568	412836.274244	38.291444
2125.063519	413599.012397	38.296461
2126.887357	414395.123404	38.301479
2128.958397	415157.835493	38.306496
2130.942867	415929.987709	38.311514
2133.108370	416712.320163	38.316532
2134.946123	417491.416017	38.321549
2137.115926	418278.082586	38.326567
2139.140288	419050.566562	38.331584
2140.853910	419846.428770	38.336602
2143.459193	420626.797803	38.341620
2145.468564	421402.531008	38.346637
2147.506870	422165.650142	38.351655
2149.656337	422936.704480	38.356672
2151.877571	423696.480550	38.361690
2153.941396	424443.953581	38.366708
2156.240650	425219.546666	38.371725
2158.436070	425974.269509	38.376743
2161.064294	426723.732923	38.381760
2162.821053	427480.811262	38.386778
2164.839550	428247.240935	38.391796
2167.306670	429012.407959	38.396813
2169.282848	429783.859373	38.401831
2171.454564	430513.940461	38.406848
2173.483906	431296.624944	38.411866
2175.516831	432069.006152	38.416884
2177.595167	432861.250141	38.421901
2179.498666	433628.691401	38.426919
2181.859433	434426.911037	38.431936
2183.472876	435212.976922	38.436954
2185.329401	436022.007216	38.441972
2187.208764	436847.050756	38.446989
2189.391211	437665.485715	38.452007
2191.383446	438496.778408	38.457024
2193.300476	439324.763691	38.462042
2195.251491	440164.403840	38.467060
2197.365311	441024.026226	38.472077
2199.426599	441876.286917	38.477095
2201.577864	442724.452259	38.482112
2203.582061	443615.012996	38.487130
2206.016871	444466.658006	38.492148
2208.167732	445335.975328	38.497165
2210.576325	446218.674040	38.502183
2212.733251	447090.400158	38.507200
2214.990501	447989.798535	38.512218
2217.314959	448872.353253	38.517236
2220.067939	449744.684013	38.522253
2221.771522	450638.296698	38.527271
2224.750139	451521.697161	38.532288
2227.013804	452399.513934	38.537306
2229.165490	453285.607645	38.542324
2231.292020	454183.857101	38.547341
2233.495025	455073.609753	38.552359
2236.142652	455955.311508	38.557376
2238.315832	456851.517000	38.562394
2240.810998	457751.676011	38.567412
2243.290444	458641.786463	38.572429
2245.375911	459550.024755	38.577447
2247.500175	460432.430420	38.582464
2249.547285	461345.802774	38.587482
2251.694144	462248.804053	38.592500
2254.249774	463145.782678	38.597517
2256.341313	464054.576214	38.602535
2258.557535	464946.424407	38.607552
2261.192712	465861.869997	38.612570
2263.513468	466761.403548	38.617588
2266.032471	467659.448146	38.622605
2268.371024	468572.491728	38.627623
2270.731143	469463.757900	38.632640
2272.502976	470377.265175	38.637658
2274.757528	471280.037836	38.642676
2277.059252	472177.202059	38.647693
2279.386169	473102.464301	38.652711
2281.730596	474006.357005	38.657728
2284.152647	474911.861196	38.662746
2286.930025	475808.877016	38.667764
2289.796213	476684.516697	38.672781
2292.130586	477588.340666	38.677799
2294.964635	478466.529137	38.682816
2297.582317	479360.016744	38.687834
2299.608059	480225.677990	38.692852
2302.002319	481077.045532	38.697869
2304.038356	481920.352030	38.702887
2306.259729	482753.741254	38.707904
2308.539996	483615.917936	38.712922
2310.819830	484441.544304	38.717940
2312.767070	485286.779860	38.722957
2314.470842	486159.837272	38.727975
2317.072113	487025.938590	38.732992
2319.095475	487909.864844	38.738010
2320.736969	488790.831583	38.743028
2322.831468	489659.412640	38.748045
2324.683122	490555.098791	38.753063
2326.793819	491444.689839	38.758080
2329.008221	492381.463004	38.763098
2331.155355	493290.033606	38.768116
2333.379970	494207.981724	38.773133
2334.851154	495166.429181	38.778151
2336.845148	496092.743106	38.783168
2339.756009	497053.169421	38.788186
2341.768665	498004.708314	38.793204
2344.179390	498974.645521	38.798221
2346.386406	499936.942505	38.803239
2348.713331	500928.375164	38.808256
2351.203676	501899.039324	38.813274
2353.100127	502899.658188	38.818292
2355.555236	503890.692502	38.823309
2357.460841	504893.409321	38.828327
2360.025952	505918.248588	38.833344
2362.283450	506925.675967	38.838362
2364.326561	507951.382182	38.843380
2366.984635	508970.669835	38.848397
2369.647544	510000.027517	38.853415
2372.226467	511018.090201	38.858432
2374.406943	512054.656676	38.863450
2376.645845	513092.709309	38.868468
2379.330081	514142.416701	38.873485
2381.942081	515174.424802	38.878503
2384.166508	516215.703541	38.883520
2386.832155	517268.432497	38.888538
2389.247583	518290.239709	38.893556
2392.347195	519345.075759	38.898573
2394.579691	520372.571836	38.903591
2397.501022	521423.164295	38.908608
2400.918602	522433.398626	38.913626
2403.198554	523485.669170	38.918644
2405.442456	524494.903322	38.923661
2407.600417	525536.524343	38.928679
2409.938567	526559.559037	38.933696
2412.452073	527604.354032	38.938714
2414.946508	528632.007184	38.943732
2417.734874	529664.728373	38.948749
2420.070304	530681.188351	38.953767
2422.419877	531719.982835	38.958784
2424.996804	532740.290199	38.963802
2426.992649	533778.243304	38.968820
2429.816156	534793.585188	38.973837
2432.476545	535820.058427	38.978855
2434.713877	536865.353936	38.983872
2437.284680	537888.223194	38.988890
2439.448589	538931.620410	38.993908
2442.236760	539959.994065	38.998925
2443.958504	541000.848412	39.003943
2446.134471	542042.357245	39.008960
2449.051836	543061.027508	39.013978
2451.054976	544107.193325	39.018996
2453.331422	545166.617676	39.024013
2456.052901	546214.470813	39.029031
2458.476965	547265.010790	39.034048
2460.877012	548280.471875	39.039066
2462.594244	549312.919043	39.044084
2464.899243	550326.033705	39.049101
2466.978707	551363.347225	39.054119
2469.377295	552409.781209	39.059136
2471.959906	553442.782399	39.064154
2473.964490	554509.733371	39.069172
2476.296404	555536.484441	39.074189
2478.787056	556609.976463	39.079207
2480.695008	557686.896900	39.084224
2483.020395	558757.581626	39.089242
2484.999147	559863.011396	39.094260
2487.604376	560952.770618	39.099277
2490.070970	562064.871495	39.104295
2492.475445	563171.765096	39.109312
2495.177650	564303.784398	39.114330
2497.110371	565415.992598	39.119348
2499.826870	566564.892610	39.124365
2502.231863	567694.307526	39.129383
2504.529891	568820.880111	39.134400
2507.274189	569967.918219	39.139418
2509.671024	571143.128119	39.144436
2512.506653	572284.422046	39.149453
2514.880928	573463.539701	39.154471
2517.245298	574618.557480	39.159488
2519.881281	575796.411986	39.164506
2523.018187	576967.399756	39.169524
2526.385178	578113.602586	39.174541
2529.127522	579282.834048	39.179559
2531.656349	580442.559364	39.184576
2534.262487	581600.859658	39.189594
2537.041189	582779.739834	39.194612
2539.868434	583909.948397	39.199629
2542.448966	585074.447730	39.204647
2544.752404	586233.416204	39.209664
2547.516790	587391.446659	39.214682
2549.787121	588579.681119	39.219700
2552.693487	589726.686120	39.224717
2555.362822	590902.845653	39.229735
2557.798104	592070.909227	39.234752
2560.351331	593239.491116	39.239770
2562.678676	594406.693002	39.244788
2565.177980	595578.261793	39.249805
2567.837769	596761.713066	39.254823
2570.884915	597938.419104	39.259840
2573.456499	599101.660981	39.264858
2576.020215	600305.259723	39.269876
2578.409127	601470.550199	39.274893
2580.981459	602662.885939	39.279911
2583.566571	603836.269708	39.284928
2586.561007	605033.348961	39.289946
2588.633355	606207.026602	39.294964
2591.643459	607385.585430	39.299981
2594.208213	608569.601794	39.304999
2596.699740	609765.668413	39.310016
2599.132597	610947.506916	39.315034
2601.561718	612162.146174	39.320052
2604.094315	613337.063081	39.325069
2606.577117	614557.538350	39.330087
2609.185173	615749.698501	39.335104
2612.087071	616960.137967	39.340122
2614.031787	618184.705705	39.345140
2616.717175	619392.664588	39.350157
2619.270578	620601.712703	39.355175
2621.370636	621822.350602	39.360192
2624.349373	623052.304895	39.365210
2626.569568	624257.004837	39.370228
2629.519839	625480.541471	39.375245
2632.590344	626678.235267	39.380263
2635.292791	627873.808078	39.385280
2637.978991	629041.423283	39.390298
2640.264743	630230.507119	39.395316
2642.947230	631413.648985	39.400333
2645.489865	632607.170108	39.405351
2648.308887	633781.834825	39.410368
2650.574324	634981.924985	39.415386
2653.023837	636176.605728	39.420404
2656.085413	637392.315238	39.425421
2658.343906	638584.206687	39.430439
2661.140659	639816.747740	39.435456
2664.200229	641018.958099	39.440474
2666.400010	642244.621659	39.445492
2669.208416	643469.689858	39.450509
2671.887012	644695.730712	39.455527
2674.357470	645927.943617	39.460544
2677.515973	647146.279012	39.465562
2680.184149	648377.215173	39.470580
2682.433379	649626.519029	39.475597
2684.969215	650867.993285	39.480615
2687.495346	652139.822724	39.485632
2690.588577	653380.096764	39.490650
2692.945434	654665.090155	39.495668
2695.074345	655935.305494	39.500685
2698.083104	657213.732695	39.505703
2700.800523	658492.391157	39.510720
2703.370205	659773.199099	39.515738
2706.247456	661067.833506	39.520756
2708.898821	662354.615232	39.525773
2712.509426	663644.106010	39.530791
2715.368347	664932.802567	39.535808
2718.169797	666231.341917	39.540826
2720.760066	667516.253523	39.545844
2723.553923	668817.580495	39.550861
2726.801806	670106.465406	39.555879
2729.637245	671409.223674	39.560896
2732.192737	672711.551034	39.565914
2734.784752	673998.523876	39.570932
2737.622147	675305.918299	39.575949
2740.561199	676590.590126	39.580967
2742.686574	677906.192540	39.585984
2745.528354	679198.973789	39.591002
2748.333150	680531.193442	39.596020
2751.279476	681824.884299	39.601037
2754.508860	683137.278239	39.606055
2757.149478	684450.973264	39.611072
2759.938237	685750.994526	39.616090
2762.673959	687076.169371	39.621108
2765.042858	688383.384643	39.626125
2768.246375	689713.163611	39.631143
2770.521558	691035.552962	39.636160
2773.199880	692371.530770	39.641178
2775.567714	693709.098318	39.646196
2778.247091	695049.342608	39.651213
2780.904425	696397.129270	39.656231
2783.075887	697776.837911	39.661248
2785.899539	699101.863833	39.666266
2788.569969	700485.085772	39.671284
2791.255180	701840.172400	39.676301
2794.158604	703210.927826	39.681319
2796.688679	704589.560049	39.686336
2799.160686	705971.254815	39.691354
2802.185334	707352.688307	39.696372
2805.010723	708757.418292	39.701389
2808.058175	710137.956824	39.706407
2810.831994	711529.215016	39.711424
2813.743869	712908.537685	39.716442
2816.606090	714255.957626	39.721460
2819.461377	715618.858351	39.726477
2822.142898	716951.623066	39.731495
2824.516210	718319.365639	39.736512
2827.362216	719650.390242	39.741530
2830.196736	721024.890488	39.746548
2833.042735	722373.342374	39.751565
2835.914475	723730.770990	39.756583
2838.693527	725113.854921	39.761600
2841.645526	726487.186880	39.766618
2844.136041	727858.784634	39.771636
2846.699281	729253.519342	39.776653
2849.873253	730628.248855	39.781671
2852.502016	732046.117650	39.786688
2855.180350	733447.726422	39.791706
2857.974852	734847.246669	39.796724
2860.556686	736269.324707	39.801741
2863.440251	737681.968338	39.806759
2866.202810	739124.199362	39.811776
2869.423256	740546.846833	39.816794
2872.962554	741969.730995	39.821812
2875.719410	743405.859968	39.826829
2878.752546	744845.037604	39.831847
2881.063912	746313.564903	39.836864
2883.752489	747738.856503	39.841882
2886.630316	749197.136277	39.846900
2889.150502	750683.299327	39.851917
2892.137700	752155.303034	39.856935
2894.190603	753652.261591	39.861952
2897.009578	755145.750115	39.866970
2900.107299	756665.894480	39.871988
2902.210097	758186.542303	39.877005
2905.331966	759702.633902	39.882023
2907.935075	761222.792309	39.887040
2910.939405	762768.172154	39.892058
2914.055285	764305.887065	39.897076
2916.801256	765870.996827	39.902093
2919.564264	767419.006603	39.907111
2922.115269	768982.762305	39.912128
2925.086378	770555.855808	39.917146
2928.201949	772124.365958	39.922164
2931.481423	773703.181310	39.927181
2935.113153	775261.555569	39.932199
2938.052002	776849.629162	39.937216
2940.975416	778428.570851	39.942234
2943.683280	780005.537748	39.947252
2946.710992	781593.793969	39.952269
2949.500833	783184.981165	39.957287
2952.458862	784773.828011	39.962304
2954.931326	786376.925575	39.967322
2957.927929	787966.189523	39.972340
2960.532655	789592.088550	39.977357
2963.999586	791185.070192	39.982375
2967.334311	792791.734225	39.987392
2970.277617	794400.058317	39.992410
2973.154139	796017.433045	39.997428
2975.950749	797630.285731	40.002445
2978.653927	799256.493581	40.007463
2981.337318	800876.891808	40.012480
2984.022688	802527.698650	40.017498
2986.921172	804151.849131	40.022516
2990.193587	805813.372537	40.027533
2993.104373	807454.550366	40.032551
2996.039508	809095.673761	40.037568
2998.660486	810739.192470	40.042586
3001.877431	812393.995093	40.047604
3004.322784	814058.684671	40.052621
3007.530342	815706.522816	40.057639
3010.615991	817331.414589	40.062656
3013.161815	818962.642494	40.067674
3016.485024	820574.404439	40.072692
3019.281327	822207.678532	40.077709
3022.608324	823820.800909	40.082727
3025.274880	825466.321093	40.087744
3028.253627	827090.653570	40.092762
3031.547764	828739.836570	40.097780
3034.606944	830376.457576	40.102797
3037.344829	832023.734364	40.107815
3040.382351	833675.221718	40.112832
3043.427358	835324.436443	40.117850
3046.813210	836962.266878	40.122868
3049.730602	838643.570365	40.127885
3053.137429	840321.092008	40.132903
3055.793659	841989.782659	40.137920
3058.710124	843663.441426	40.142938
3061.536280	845324.857086	40.147956
3064.626684	847026.144636	40.152973
3067.766225	848714.717133	40.157991
3070.914766	850423.922483	40.163008
3073.910821	852132.200662	40.168026
3077.132337	853845.218873	40.173044
3080.058251	855562.183336	40.178061
3083.687979	857261.665377	40.183079
3086.909406	858998.012525	40.188096
3089.630118	860697.279111	40.193114
3092.945768	862428.662929	40.198132
3095.754258	864161.966753	40.203149
3099.132153	865899.142347	40.208167
3102.145329	867641.210495	40.213184
3105.615601	869369.428675	40.218202
3108.853428	871104.356371	40.223220
3112.110431	872849.720596	40.228237
3115.766755	874574.860078	40.233255
3119.258267	876298.849969	40.238272
3122.273111	878043.797518	40.243290
3125.625702	879768.832708	40.248308
3128.655593	881513.043209	40.253325
3131.923899	883234.369670	40.258343
3135.193697	884983.501418	40.263360
3138.741316	886693.327816	40.268378
3141.970000	888427.329157	40.273396
3144.891884	890147.250251	40.278413
3148.046430	891881.001105	40.283431
3150.925894	893627.396656	40.288448
3153.890225	895364.373053	40.293466
3157.300698	897135.556815	40.298484
3160.202273	898873.885885	40.303501
3163.185483	900637.301894	40.308519
3166.338033	902380.103181	40.313536
3169.399903	904134.226033	40.318554
3172.543843	905890.675986	40.323572
3175.190552	907660.900833	40.328589
3178.800140	909432.329784	40.333607
3182.046506	911195.367393	40.338624
3185.084816	912969.608765	40.343642
3189.184245	914723.208550	40.348660
3192.199607	916499.009026	40.353677
3195.288459	918256.643877	40.358695
3198.973239	920023.794233	40.363712
3201.919328	921781.661335	40.368730
3205.139364	923546.591277	40.373748
3208.159834	925310.786453	40.378765
3211.634995	927069.822086	40.383783
3215.023913	928824.652965	40.388800
3218.270602	930583.628315	40.393818
3221.347039	932320.207849	40.398836
3224.333785	934062.652221	40.403853
3227.586293	935771.256563	40.408871
3230.451752	937492.389290	40.413888
3233.207361	939197.189957	40.418906
3236.583191	940942.273711	40.423924
3239.409543	942681.702429	40.428941
3241.851286	944411.342295	40.433959
3245.141988	946163.773413	40.438976
3247.671094	947913.253496	40.443994
3250.973476	949680.156582	40.449012
3253.814608	951462.565701	40.454029
3256.913610	953260.916559	40.459047
3260.533441	955050.154450	40.464064
3263.491909	956896.373774	40.469082
3266.682478	958744.232316	40.474100
3270.240920	960627.618016	40.479117
3273.488273	962488.055198	40.484135
3277.009130	964370.126445	40.489152
3279.796740	966255.219937	40.494170
3282.869407	968158.105379	40.499188
3285.680164	970063.723125	40.504205
3288.900846	971995.575533	40.509223
3292.059459	973927.860830	40.514240
3295.493940	975867.836323	40.519258
3298.671169	977812.266530	40.524276
3301.601296	979773.423949	40.529293
3304.932363	981745.533333	40.534311
3308.137160	983716.690463	40.539328
3310.987725	985704.067532	40.544346
3314.428385	987690.654718	40.549364
3317.469595	989714.751259	40.554381
3320.529901	991708.754693	40.559399
3323.909163	993749.448587	40.564416
3326.722705	995786.781453	40.569434
3329.873212	997810.309701	40.574452
3333.556715	999857.500442	40.579469
3337.656413	1001906.406732	40.584487
3340.930684	1003960.141460	40.589504
3343.899266	1006023.851293	40.594522
3347.261173	1008084.512027	40.599540
3350.010657	1010184.749459	40.604557
3353.657177	1012252.564410	40.609575
3357.420595	1014335.292842	40.614592
3360.449960	1016432.089045	40.619610
3364.144191	1018510.571075	40.624628
3366.968756	1020620.259710	40.629645
3370.253366	1022708.961636	40.634663
3373.626725	1024822.975040	40.639680
3376.826048	1026940.568030	40.644698
3379.978644	1029067.221267	40.649716
3383.381875	1031190.223275	40.654733
3386.473507	1033321.929773	40.659751
3389.810579	1035465.036440	40.664768
3393.120490	1037615.908295	40.669786
3396.074552	1039771.793021	40.674804
3399.439838	1041941.714087	40.679821
3402.596777	1044108.509368	40.684839
3405.858743	1046291.295713	40.689856
3409.080102	1048465.719874	40.694874
3412.251364	1050661.143874	40.699892
3415.343643	1052868.215169	40.704909
3418.797133	1055056.363829	40.709927
3422.933013	1057266.889951	40.714944
3426.215523	1059469.752519	40.719962
3429.527469	1061674.130412	40.724980
3433.123477	1063895.723346	40.729997
3435.854931	1066094.200757	40.735015
3439.337609	1068294.952062	40.740020
3442.603965	1070459.128534	40.745024
3445.978613	1072534.214694	40.750029
3449.148624	1074566.952891	40.755034
3452.700116	1076509.374663	40.760039
3456.332593	1078385.143803	40.765044
3459.355712	1080168.723467	40.770048
3462.394042	1081876.121616	40.775053
3465.412983	1083498.975192	40.780058
3468.437939	1085040.614902	40.785063
3470.845976	1086499.103119	40.790068
3473.409783	1087906.960777	40.795072
3475.816724	1089207.466211	40.800077
3478.121737	1090460.839251	40.805082
3480.664333	1091619.366856	40.810087
3482.423537	1092717.745353	40.815092
3484.431377	1093741.769658	40.820096
3486.712068	1094698.560170	40.825101
3488.928619	1095587.538037	40.830106
3490.569113	1096426.042883	40.835111
3492.477177	1097193.869780	40.840116
3493.624137	1097905.565903	40.845120
3495.415679	1098565.321321	40.850125
3496.701664	1099181.472863	40.855130
3498.373049	1099727.211011	40.860135
3499.867012	1100234.870493	40.865140
3501.000604	1100707.073419	40.870144
3502.260508	1101116.695737	40.875149
3503.485299	1101502.395853	40.880154
3504.470492	1101837.640890	40.885159
3505.237420	1102121.480972	40.890164
3506.324580	1102401.621646	40.895168
3507.407561	1102628.613013	40.900173
3508.280170	1102829.827186	40.905178
3508.933426	1102989.118675	40.910183
3509.665804	1103124.311607	40.915188
3510.046982	1103244.747691	40.920192
3510.867743	1103326.122208	40.925197
3511.864104	1103403.931072	40.930202
3512.359442	1103439.013561	40.935207
3512.926862	1103427.645083	40.940212
3513.260301	1103444.885638	40.945216
3514.066372	1103400.129583	40.950221
3514.412390	1103373.795441	40.955226
3514.738945	1103292.615501	40.960231
3515.549141	1103227.886099	40.965236
3515.385072	1103123.181747	40.970240
3515.912311	1103010.238823	40.975245
3516.193649	1102891.982507	40.980250
3516.441655	1102772.582308	40.985255
3517.048707	1102626.648117	40.990260
3517.177227	1102468.938056	40.995264
3517.482602	1102296.284791	41.000269
3517.635308	1102109.123471	41.005274
3518.411712	1101919.081111	41.010279
3518.700176	1101699.481406	41.015284
3518.974227	1101499.757435	41.020288
3519.140281	1101250.527352	41.025293
3519.419301	1101032.813941	41.030298
3519.939715	1100780.827136	41.035303
3520.020285	1100529.379050	41.040308
3519.932337	1100270.107040	41.045312
3520.158720	1099996.811138	41.050317
3520.490160	1099727.786974	41.055322
3520.401854	1099457.288573	41.060327
3521.256038	1099170.651389	41.065332
3520.808027	1098871.781052	41.070336
3520.676282	1098573.607211	41.075341
3520.745497	1098267.445301	41.080346
3520.997199	1097969.844528	41.085351
3521.367157	1097642.458974	41.090356
3521.085745	1097336.015121	41.095360
3521.339809	1097005.740285	41.100365
3521.409041	1096694.323302	41.105370
3521.515793	1096363.650855	41.110375
3521.615906	1096036.499624	41.115380
3521.311070	1095712.266023	41.120384
3521.769197	1095370.279274	41.125389
3521.784368	1095033.224701	41.130394
3521.853764	1094704.562525	41.135399
3522.406074	1094341.152392	41.140404
3522.063958	1094010.314446	41.145408
3522.079999	1093647.424716	41.150413
3522.116379	1093293.601966	41.155418
3522.222322	1092923.947689	41.160423
3522.465738	1092570.905330	41.165428
3522.301425	1092200.480279	41.170432
3522.268096	1091841.786656	41.175437
3522.535400	1091461.376908	41.180442
3522.440447	1091123.810029	41.185447
3522.389742	1090741.103653	41.190452
3522.454724	1090374.347249	41.195456
3522.623600	1090003.813110	41.200461
3522.477471	1089634.934124	41.205466
3522.268320	1089262.495707	41.210471
3522.571297	1088877.396199	41.215476
3522.478575	1088490.034946	41.220480
3522.617913	1088125.030726	41.225485
3522.385486	1087738.501318	41.230490
3522.286030	1087369.844131	41.235495
3522.478247	1086994.021451	41.240500
3522.444523	1086613.705027	41.245504
3522.334058	1086235.579363	41.250509
3522.668041	1085842.399398	41.255514
3522.564771	1085471.025761	41.260519
3522.759226	1085084.620846	41.265524
3522.353494	1084691.000125	41.270528
3522.453342	1084298.226575	41.275533
3522.735491	1083911.340361	41.280538
3522.589837	1083529.004662	41.285543
3522.634390	1083128.483434	41.290548
3522.728430	1082756.604355	41.295552
3522.354035	1082361.275322	41.300557
3522.616260	1081974.830400	41.305562
3522.535326	1081573.544003	41.310567
3522.150357	1081179.857908	41.315572
3522.337123	1080805.431747	41.320576
3522.473255	1080403.447754	41.325581
3522.721591	1080010.916393	41.330586
3522.275586	1079616.551673	41.335591
3522.502742	1079215.904790	41.340596
3522.467151	1078823.718710	41.345600
3522.565798	1078420.346938	41.350605
3522.208594	1078042.460921	41.355610
3522.129687	1077645.301229	41.360615
3522.505735	1077240.356471	41.365620
3522.347967	1076849.584955	41.370624
3522.514401	1076451.049729	41.375629
3522.259007	1076059.469543	41.380634
3522.494668	1075668.164591	41.385639
3522.115465	1075256.282074	41.390644
3522.021262	1074860.075032	41.395648
3522.127186	1074478.696292	41.400653
3521.749636	1074075.754595	41.405658
3521.898964	1073692.680694	41.410663
3521.905332	1073297.400747	41.415668
3521.957199	1072919.477359	41.420672
3522.193857	1072520.451894	41.425677
3522.147874	1072109.046267	41.430682
3521.536668	1071725.094965	41.435687
3522.196396	1071325.720539	41.440692
3521.988391	1070941.455650	41.445696
3521.915480	1070520.514745	41.450701
3522.176545	1070129.290144	41.455706
3521.586046	1069752.215381	41.460711
3521.943441	1069341.208469	41.465716
3521.540943	1068960.394401	41.470720
3521.872115	1068563.950017	41.475725
3521.710698	1068158.132964	41.480730
3521.824391	1067752.240577	41.485735
3521.728695	1067378.575986	41.490740
3521.730397	1066975.337867	41.495744
3521.800170	1066575.522217	41.500749
3521.575550	1066191.600542	41.505754
3521.488539	1065802.818537	41.510759
3521.554281	1065405.516203	41.515764
3521.306696	1065021.420275	41.520768
3521.453621	1064608.650110	41.525773
3521.552487	1064220.976623	41.530778
3521.278408	1063837.476004	41.535783
3521.350099	1063451.100208	41.540788
3521.048316	1063064.469980	41.545792
3521.267675	1062670.410122	41.550797
3521.155908	1062268.481763	41.555802
3520.944300	1061885.123511	41.560807
3521.023647	1061497.935247	41.565812
3520.838195	1061113.844909	41.570816
3520.958522	1060726.017805	41.575821
3520.917418	1060341.560891	41.580826
3520.718500	1059961.533784	41.585831
3521.141665	1059573.768290	41.590836
3520.739079	1059183.317878	41.595840
3520.942793	1058791.391180	41.600845
3520.978879	1058415.168583	41.605850
3520.491312	1058021.759476	41.610855
3520.747766	1057642.749991	41.615860
3520.694468	1057252.587033	41.620864
3520.470163	1056863.966599	41.625869
3520.308686	1056496.511891	41.630874
3520.266327	1056109.061227	41.635879
3520.461542	1055725.110755	41.640884
3520.371692	1055358.628783	41.645888
3520.350104	1054967.817002	41.650893
3520.426593	1054592.483825	41.655898
3520.426013	1054205.471118	41.660903
3520.351316	1053821.914830	41.665908
3520.130536	1053459.667527	41.670912
3520.295682	1053063.097115	41.675917
3520.331602	1052696.610616	41.680922
3520.228368	1052297.136076	41.685927
3520.155423	1051931.195469	41.690932
3519.927325	1051564.677401	41.695936
3520.244202	1051179.426208	41.700941
3520.110361	1050793.643548	41.705946
3519.738304	1050420.705765	41.710951
3519.758367	1050042.950153	41.715956
3519.725585	1049682.836638	41.720960
3519.550934	1049309.212425	41.725965
3519.235188	1048937.902495	41.730970
3519.217033	1048569.028097	41.735975
3519.550261	1048213.584588	41.740980
3519.413878	1047839.179195	41.745984
3519.534839	1047482.758452	41.750989
3519.152772	1047105.061662	41.755994
3519.513078	1046750.099059	41.760999
3519.412902	1046367.574658	41.766004
3519.469259	1046010.007717	41.771008
3519.517045	1045637.644152	41.776013
3519.155668	1045283.189334	41.781018
3519.308060	1044917.713577	41.786023
3519.239581	1044535.540459	41.791028
3519.310293	1044185.966910	41.796032
3519.364700	1043800.631928	41.801037
3519.407136	1043457.296172	41.806042
3518.896765	1043076.930895	41.811047
3519.122181	1042716.515239	41.816052
3519.183579	1042344.121606	41.821056
3519.098177	1041983.999484	41.826061
3518.728120	1041631.921881	41.831066
3518.919662	1041282.628792	41.836071
3519.048207	1040913.414093	41.841076
3518.419491	1040565.950769	41.846080
3518.502098	1040187.899657	41.851085
3518.727108	1039846.727200	41.856090
3518.639635	1039465.561567	41.861095
3518.840604	1039120.288113	41.866100
3518.663418	1038759.682102	41.871104
3518.714112	1038411.682146	41.876109
3518.537038	1038052.867491	41.881114
3518.297717	1037705.354628	41.886119
3518.960409	1037334.750561	41.891124
3519.008131	1037002.040298	41.896128
3518.596500	1036622.764373	41.901133
3518.679197	1036275.302647	41.906138
3518.200223	1035909.821822	41.911143
3518.334152	1035553.696975	41.916148
3518.345314	1035211.017838	41.921152
3518.305410	1034854.199667	41.926157
3518.093070	1034502.418688	41.931162
3517.852857	1034143.846308	41.936167
3518.168320	1033806.159398	41.941172
3517.879353	1033451.518264	41.946176
3518.019663	1033110.237188	41.951181
3518.119753	1032748.518649	41.956186
3517.815343	1032409.106986	41.961191
3518.135553	1032050.501291	41.966196
3517.693492	1031710.488971	41.971200
3517.730210	1031347.721956	41.976205
3517.670686	1031020.965342	41.981210
3517.461652	1030675.623170	41.986215
3517.705952	1030345.097476	41.991220
3517.654042	1030010.727409	41.996224
3517.764643	1029670.015572	42.001229
3517.612306	1029320.803290	42.006234
3517.543781	1028970.102503	42.011239
3517.518958	1028627.702828	42.016244
3517.446689	1028290.520970	42.021248
3517.330138	1027955.069831	42.026253
3517.752334	1027590.639052	42.031258
3517.474547	1027272.999821	42.036263
3517.556700	1026921.467482	42.041268
3517.123760	1026596.742155	42.046272
3517.293785	1026250.967164	42.051277
3517.226501	1025918.002166	42.056282
3517.042657	1025576.992456	42.061287
3517.466694	1025253.889465	42.066292
3517.178689	1024905.005244	42.071296
3517.340509	1024566.106380	42.076301
3517.242097	1024238.474935	42.081306
3517.144118	1023903.650260	42.086311
3517.027863	1023551.745059	42.091316
3516.631555	1023229.048181	42.096320
3516.770366	1022893.639353	42.101325
3516.631584	1022576.195443	42.106330
3516.511415	1022241.662976	42.111335
3516.557532	1021927.739951	42.116340
3516.822348	1021594.560167	42.121344
3516.700250	1021277.330919	42.126349
3516.635566	1020947.949657	42.131354
3516.587203	1020597.108723	42.136359
3516.783927	1020285.397044	42.141364
3516.628826	1019961.308211	42.146368
3516.639160	1019632.322427	42.151373
3516.625147	1019308.851818	42.156378
3516.418890	1018990.051719	42.161383
3516.523011	1018660.799492	42.166388
3516.543058	1018340.954900	42.171392
3516.102331	1018012.045503	42.176397
3516.053369	1017701.007173	42.181402
3516.023863	1017381.407262	42.186407
3516.245865	1017067.668659	42.191412
3516.075075	1016742.523028	42.196416
3515.917800	1016426.966806	42.201421
3516.001329	1016106.693336	42.206426
3516.092083	1015800.963344	42.211431
3516.290250	1015468.110523	42.216436
3516.003814	1015159.689228	42.221440
3516.082874	1014841.286369	42.226445
3516.389406	1014524.964400	42.231450
3515.926427	1014203.313042	42.236455
3515.822192	1013864.588339	42.241460
3515.895529	1013571.851164	42.246464
3515.862978	1013243.469579	42.251469
3515.906190	1012952.259230	42.256474
3515.681123	1012634.850111	42.261479
3516.073291	1012311.978400	42.266484
3515.563646	1012016.924893	42.271488
3515.481753	1011687.489181	42.276493
3515.560355	1011382.201206	42.281498
3515.421014	1011069.547858	42.286503
3515.382625	1010762.107872	42.291508
3515.479769	1010467.942187	42.296512
3515.438752	1010146.183865	42.301517
3515.479663	1009856.174412	42.306522
3515.471295	1009554.883705	42.311527
3515.343152	1009245.529117	42.316532
3515.117145	1008942.297548	42.321536
3515.212464	1008615.277592	42.326541
3515.298999	1008327.709489	42.331546
3515.083383	1008020.829729	42.336551
3515.367243	1007713.364883	42.341556
3515.219085	1007415.385821	42.346560
3515.152270	1007107.556819	42.351565
3515.132156	1006813.608807	42.356570
3514.913273	1006506.452764	42.361575
3515.066823	1006220.613957	42.366580
3514.713489	1005916.851778	42.371584
3514.804312	1005614.945335	42.376589
3515.154076	1005316.773513	42.381594
3514.512590	1005032.950896	42.386599
3514.687832	1004723.395729	42.391604
3514.889716	1004441.447307	42.396608
3514.904097	1004134.123851	42.401613
3514.636322	1003838.310644	42.406618
3514.802681	1003559.534737	42.411623
3514.632771	1003255.307370	42.416628
3514.616719	1002974.489326	42.421632
3514.443853	1002674.415399	42.426637
3514.481402	1002393.754323	42.431642
3514.277102	1002096.866399	42.436647
3514.503536	1001802.227802	42.441652
3514.398168	1001516.875074	42.446656
3514.415778	1001230.806346	42.451661
3514.788566	1000934.346414	42.456666
3514.335559	1000653.193117	42.461671
3514.469324	1000356.158206	42.466676
3514.207858	1000060.925245	42.471680
3514.284554	999784.022611	42.476685
3514.589896	999482.240248	42.481690
3514.042109	999208.430717	42.486695
3514.554967	998914.763177	42.491700
3514.412728	998639.203936	42.496704
3514.091238	998350.611049	42.501709
3514.173641	998053.950839	42.506714
3513.742927	997781.513942	42.511719
3513.958953	997489.574610	42.516724
3513.951944	997214.995278	42.521728
3514.094663	996936.091921	42.526733
3513.872764	996654.117611	42.531738
3514.070198	996374.008624	42.536743
3514.069758	996088.170313	42.541748
3513.622424	995807.262722	42.546752
3513.733379	995524.203131	42.551757
3513.657051	995234.729240	42.556762
3513.735049	994979.710571	42.561767
3513.979993	994678.267173	42.566772
3513.589240	994424.372716	42.571776
3513.646995	994137.939347	42.576781
3514.014047	993868.789103	42.581786
3513.395687	993600.958034	42.586791
3513.496155	993308.627733	42.591796
3513.244963	993056.013734	42.596800
3513.290662	992769.220912	42.601805
3513.081500	992509.459482	42.606810
3513.042187	992233.182172	42.611815
3513.444058	991961.596079	42.616820
3513.265200	991701.012747	42.621824
3513.078837	991438.078586	42.626829
3513.285740	991164.536446	42.631834
3513.279400	990898.427371	42.636839
3513.001529	990643.760272	42.641844
3513.076462	990385.220258	42.646848
3513.338555	990100.597751	42.651853
3513.187865	989847.336974	42.656858
3512.691989	989574.321796	42.661863
3512.777893	989310.269064	42.666868
3513.031213	989055.931111	42.671872
3512.798200	988788.199949	42.676877
3512.819438	988522.462976	42.681882
3512.876586	988273.878152	42.686887
3512.843875	988001.979540	42.691892
3513.046263	987746.713437	42.696896
3512.670287	987484.505921	42.701901
3512.806169	987221.518983	42.706906
3512.493235	986987.965892	42.711911
3512.595342	986720.277481	42.716916
3512.499039	986465.003160	42.721920
3512.502952	986209.505710	42.726925
3512.752068	985954.346818	42.731930
3512.408783	985706.984748	42.736935
3512.397353	985425.394557	42.741940
3512.628026	985191.971155	42.746944
3512.540588	984927.841454	42.751949
3512.507501	984683.312381	42.756954
3512.542451	984423.922606	42.761959
3512.322882	984166.222664	42.766964
3512.117377	983922.177515	42.771968
3512.069063	983674.581067	42.776973
3511.997466	983420.435677	42.781978
3512.388916	983184.560260	42.786983
3512.257903	982926.985064	42.791988
3512.105105	982690.983600	42.796993
3511.846040	982444.442713	42.801997
3512.260381	982201.003151	42.807002
3511.642367	981954.597899	42.812007
3512.221352	981701.538519	42.817012
3512.123490	981469.872772	42.822017
3511.744049	981206.400337	42.827021
3511.874870	980965.787574	42.832026
3511.736900	980729.214181	42.837031
3511.884939	980485.061562	42.842036
3511.873106	980244.930414	42.847041
3511.845767	980011.630784	42.852045
3511.819333	979765.522161	42.857050
3511.956226	979520.939389	42.862055
3512.168913	979285.030144	42.867060
3511.769345	979037.681386	42.872065
3511.515985	978806.030988	42.877069
3511.632341	978556.622019	42.882074
3511.444617	978330.414175	42.887079
3511.613146	978085.276159	42.892084
3511.371065	977860.720168	42.897089
3511.477767	977613.519644	42.902093
3511.543052	977392.804330	42.907098
3511.079245	977143.136078	42.912103
3511.351351	976930.579843	42.917108
3511.424229	976689.210172	42.922113
3511.354038	976463.006910	42.927117
3511.416252	976221.130461	42.932122
3511.212762	976008.031732	42.937127
3511.262867	975765.551424	42.942132
3511.140314	975540.591405	42.947137
3510.976288	975300.375547	42.952141
3511.269495	975078.066758	42.957146
3510.979116	974851.542766	42.962151
3510.952406	974621.543644	42.967156
3511.197898	974397.358253	42.972161
3510.893413	974172.276679	42.977165
3510.902367	973952.611671	42.982170
3511.004915	973722.163957	42.987175
3511.071397	973499.635687	42.992180
3511.060789	973268.112435	42.997185
3510.685794	973047.595654	43.002189
3511.083094	972820.486845	43.007194
3510.821295	972597.390699	43.012199
3510.729210	972384.432338	43.017204
3510.692991	972154.140140	43.022209
3510.742612	971937.228448	43.027213
3511.067492	971708.424304	43.032218
3510.816131	971495.654877	43.037223
3510.830926	971269.428305	43.042228
3510.542722	971059.877834	43.047233
3510.664622	970842.912881	43.052237
3511.148602	970623.335711	43.057242
3510.636449	970407.730943	43.062247
3510.354247	970182.880577	43.067252
3510.543071	969965.479978	43.072257
3510.290816	969739.041347	43.077261
3510.360753	969525.656598	43.082266
3510.142598	969311.919843	43.087271
3510.088777	969104.706482	43.092276
3510.336193	968898.512825	43.097281
3510.077815	968690.828782	43.102285
3510.207438	968482.094349	43.107290
3510.098527	968268.496579	43.112295
3510.204969	968078.548272	43.117300
3510.004462	967851.145567	43.122305
3509.927460	967659.451282	43.127309
3510.171735	967447.233494	43.132314
3509.873863	967241.559798	43.137319
3510.121802	967042.741299	43.142324
3510.165514	966826.616773	43.147329
3509.861406	966626.797645	43.152333
3510.055140	966392.809014	43.157338
3509.840104	966212.253568	43.162343
3509.961069	965994.420141	43.167348
3509.752766	965804.644453	43.172353
3509.559941	965588.806215	43.177357
3509.729739	965395.330724	43.182362
3509.318546	965201.258755	43.187367
3509.887316	964995.655861	43.192372
3509.885958	964823.641830	43.197377
3509.432872	964624.757296	43.202381
3509.904410	964421.403070	43.207386
3509.458775	964222.993260	43.212391
3509.714972	964007.413643	43.217396
3509.694327	963820.186897	43.222401
3509.556170	963640.125948	43.227405
3509.857176	963424.615124	43.232410
3509.139697	963243.069446	43.237415
3509.261189	963026.397455	43.242420
3509.652020	962847.302487	43.247425
3509.328860	962656.755984	43.252429
3509.387308	962457.516340	43.257434
3509.499116	962255.516929	43.262439
3509.590420	962064.000529	43.267444
3509.099058	961875.416024	43.272449
3509.452773	961683.941787	43.277453
3509.603894	961495.239020	43.282458
3509.341864	961295.717961	43.287463
3509.215624	961086.169273	43.292468
3509.421709	960921.356284	43.297473
3509.445302	960716.768820	43.302477
3509.632179	960534.008510	43.307482
3509.491077	960328.356040	43.312487
3509.199226	960137.426983	43.317492
3509.180910	959946.348508	43.322497
3509.248259	959765.642441	43.327501
3509.221585	959569.258391	43.332506
3508.975733	959375.943379	43.337511
3508.916800	959194.455809	43.342516
3509.100366	959013.118708	43.347521
3508.894510	958824.877684	43.352525
3509.160579	958629.295988	43.357530
3508.894861	958449.093889	43.362535
3509.071735	958265.478847	43.367540
3508.612421	958091.083652	43.372545
3508.533590	957906.420495	43.377549
3509.052046	957720.181848	43.382554
3509.026385	957533.045989	43.387559
3509.022311	957357.965167	43.392564
3508.932563	957168.277796	43.397569
3508.745242	957002.927272	43.402573
3508.631473	956823.826534	43.407578
3508.468900	956649.731309	43.412583
3508.699380	956471.151529	43.417588
3508.637125	956287.513009	43.422593
3508.920725	956115.682720	43.427597
3508.855946	955911.037589	43.432602
3508.714731	955754.571848	43.437607
3508.891723	955564.897171	43.442612
3508.750499	955395.377046	43.447617
3508.491301	955214.777604	43.452621
3508.751601	955046.231650	43.457626
3508.399161	954874.911948	43.462631
3508.822213	954717.230875	43.467636
3508.478020	954527.535290	43.472641
3508.198753	954364.602970	43.477645
3508.629457	954179.644763	43.482650
3508.298124	954013.266403	43.487655
3508.343247	953841.081249	43.492660
3508.443653	953679.881989	43.497665
3508.425947	953528.071974	43.502669
3508.594922	953339.108632	43.507674
3508.645456	953185.842227	43.512679
3508.493763	953009.643396	43.517684
3508.240859	952839.769704	43.522689
3508.524886	952681.665985	43.527693
3508.277447	952503.838975	43.532698
3508.522139	952339.990314	43.537703
3508.734577	952168.486741	43.542708
3508.522207	951992.741321	43.547713
3508.221884	951818.918236	43.552717
3508.668074	951653.291936	43.557722
3508.468345	951489.106481	43.562727
3508.340393	951323.659804	43.567732
3508.249567	951154.564837	43.572737
3508.209649	950988.710032	43.577741
3508.007803	950819.239464	43.582746
3507.926002	950662.282268	43.587751
3507.923802	950498.415435	43.592756
3508.182443	950331.724486	43.597761
3507.965835	950187.888847	43.602765
3508.283961	950008.829183	43.607770
3507.909815	949870.084161	43.612775
3508.201907	949682.114496	43.617780
3507.873055	949537.800491	43.622785
3507.900778	949378.584125	43.627789
3507.749446	949219.488071	43.632794
3507.715854	949055.484696	43.637799
3507.994738	948884.913736	43.642804
3507.694301	948739.040682	43.647809
3507.617759	948566.602706	43.652813
3507.703280	948421.423128	43.657818
3507.250682	948261.389542	43.662823
3507.261871	948110.563608	43.667828
3507.316435	947982.231016	43.672833
3507.294349	947817.132941	43.677837
3507.488856	947684.556091	43.682842
3506.981524	947524.795987	43.687847
3507.134863	947376.511091	43.692852
3507.271152	947232.822153	43.697857
3507.211758	947096.153524	43.702861
3507.312874	946928.324870	43.707866
3507.000086	946801.172871	43.712871
3507.442903	946649.466899	43.717876
3507.482617	946511.617024	43.722881
3507.183362	946367.880012	43.727885
3507.332549	946225.885302	43.732890
3506.717492	946074.815731	43.737895
3506.953627	945943.528619	43.742900
3507.015778	945804.027564	43.747905
3507.093421	945664.903436	43.752909
3507.109934	945511.893066	43.757914
3507.265721	945370.352891	43.762919
3507.074206	945222.158920	43.767924
3506.977268	945076.053156	43.772929
3506.934917	944955.710280	43.777933
3506.881738	944796.557731	43.782938
3506.806422	944669.314298	43.787943
3506.381230	944534.746545	43.792948
3506.719916	944398.037020	43.797953
3506.748631	944266.070828	43.802957
3506.916071	944130.724160	43.807962
3506.580844	944005.232335	43.812967
3506.684398	943858.867641	43.817972
3506.296168	943743.441576	43.822977
3506.636210	943605.656729	43.827981
3507.012357	943475.242636	43.832986
3506.548369	943340.650365	43.837991
3506.617567	943191.780448	43.842996
3506.426140	943078.416001	43.848001
3506.446659	942947.759715	43.853005
3506.708224	942822.045204	43.858010
3506.658697	942698.200299	43.863015
3506.499497	942551.362831	43.868020
3506.526564	942423.855903	43.873025
3506.489640	942291.371143	43.878029
3506.884470	942154.210008	43.883034
3506.354706	942026.497469	43.888039
3506.512578	941897.805642	43.893044
3506.645063	941774.579980	43.898049
3506.216269	941646.457991	43.903053
3506.639695	941513.014719	43.908058
3506.378299	941383.803984	43.913063
3506.575686	941266.788312	43.918068
3506.346451	941118.579637	43.923073
3506.058211	941000.966763	43.928077
3506.494060	940872.875179	43.933082
3506.186857	940763.411272	43.938087
3505.985058	940634.076296	43.943092
3506.289212	940514.724604	43.948097
3506.077748	940393.824735	43.953101
3506.379597	940263.918133	43.958106
3506.462407	940141.141719	43.963111
3506.367655	940021.460859	43.968116
3505.928633	939895.119977	43.973121
3506.058950	939767.339437	43.978125
3505.934223	939653.218266	43.983130
3505.981531	939536.860097	43.988135
3505.987009	939411.681319	43.993140
3505.895978	939296.491683	43.998145
3505.831896	939173.141250	44.003149
3506.458767	939062.720538	44.008154
3506.143057	938932.498972	44.013159
3506.253084	938808.343839	44.018164
3506.287572	938684.294152	44.023169
3505.991554	938576.509584	44.028173
3506.149293	938449.651844	44.033178
3505.808993	938327.286453	44.038183
3505.619164	938214.775769	44.043188
3505.958609	938099.776823	44.048193
3505.879860	937993.095869	44.053197
3505.941834	937852.230922	44.058202
3505.990958	937749.457980	44.063207
3505.965575	937623.665976	44.068212
3505.965746	937516.002796	44.073217
3506.008122	937394.704172	44.078221
3505.800317	937264.999291	44.083226
3505.757559	937163.573522	44.088231
3505.826088	937046.101130	44.093236
3505.774696	936946.975805	44.098241
3505.494740	936840.016729	44.103245
3505.925448	936711.536636	44.108250
3505.492490	936607.381239	44.113255
3505.549246	936494.025379	44.118260
3505.502916	936369.262627	44.123265
3505.496197	936253.416611	44.128269
3505.633590	936164.899342	44.133274
3505.468831	936049.362827	44.138279
3505.552500	935935.414636	44.143284
3505.615320	935846.520369	44.148289
3505.351718	935720.338250	44.153293
3505.890607	935608.611801	44.158298
3505.688070	935495.757189	44.163303
3505.526681	935376.749610	44.168308
3505.237040	935283.488084	44.173313
3505.330254	935183.825847	44.178317
3505.227342	935076.513879	44.183322
3505.170367	934974.088369	44.188327
3505.189690	934865.503937	44.193332
3505.383687	934756.888507	44.198337
3505.201128	934665.710622	44.203341
3505.537879	934548.906600	44.208346
3505.326213	934435.838857	44.213351
3505.275824	934347.610148	44.218356
3505.280926	934243.912092	44.223361
3505.252420	934153.564171	44.228365
3505.700539	934036.922563	44.233370
3505.554155	933947.454734	44.238375
3505.701540	933824.520501	44.243380
3505.635027	933715.638572	44.248385
3505.226956	933594.038836	44.253389
3505.636884	933498.998159	44.258394
3505.525928	933389.828772	44.263399
3505.262947	933287.212527	44.268404
3505.237158	933173.799150	44.273409
3505.344403	933076.399855	44.278413
3505.397470	932970.268049	44.283418
3504.996242	932865.745624	44.288423
3505.195355	932771.591041	44.293428
3505.549029	932655.606961	44.298433
3505.103425	932567.029561	44.303437
3505.238252	932459.529425	44.308442
3505.171646	932361.569371	44.313447
3505.207459	932260.997214	44.318452
3505.247689	932166.473878	44.323457
3505.121503	932050.651706	44.328461
3505.223650	931956.402611	44.333466
3505.140259	931868.522379	44.338471
3505.169771	931752.668077	44.343476
3505.048365	931664.886807	44.348481
3504.870675	931555.882876	44.353485
3504.991854	931455.665707	44.358490
3504.834376	931367.981552	44.363495
3504.978112	931278.997421	44.368500
3504.977077	931179.371612	44.373505
3504.774712	931096.974378	44.378509
3504.963201	930992.125855	44.383514
3504.874062	930907.401219	44.388519
3505.035586	930788.525814	44.393524
3505.060320	930694.939721	44.398529
3505.153121	930602.109439	44.403533
3505.042536	930491.727534	44.408538
3504.978835	930414.197240	44.413543
3504.996875	930314.744316	44.418548
3504.918729	930220.878594	44.423553
3505.084169	930121.878249	44.428557
3504.726161	930032.571615	44.433562
3504.844213	929932.518543	44.438567
3504.862411	929846.221865	44.443572
3505.113553	929750.660002	44.448577
3504.694284	929647.999358	44.453581
3504.748688	929549.967712	44.458586
3505.048669	929453.911994	44.463591
3504.812927	929352.176474	44.468596
3505.025244	929273.623114	44.473601
3504.509297	929183.175016	44.478605
3504.449784	929099.954565	44.483610
3504.501517	929013.158373	44.488615
3504.884793	928906.218501	44.493620
3504.705603	928821.379505	44.498625
3504.415717	928727.522444	44.503629
3504.905773	928634.880925	44.508634
3504.676916	928539.376503	44.513639
3504.842460	928455.243884	44.518644
3504.579529	928380.985059	44.523649
3504.455220	928290.745736	44.528653
3504.653232	928189.108917	44.533658
3504.316147	928121.683671	44.538663
3504.413433	928018.137653	44.543668
3504.430282	927930.945162	44.548673
3504.487785	927847.493722	44.553677
3504.785145	927755.733956	44.558682
3504.409800	927672.447224	44.563687
3504.206612	927588.361745	44.568692
3504.296749	927488.459891	44.573697
3503.852880	927420.466582	44.578701
3504.126229	927337.644644	44.583706
3504.200711	927281.389587	44.588711
3504.029584	927193.158506	44.593716
3504.214751	927111.309046	44.598721
3503.812490	927047.246122	44.603725
3504.270533	926955.734667	44.608730
3504.505724	926886.949711	44.613735
3504.405828	926790.431415	44.618740
3504.483026	926715.035841	44.623745
3504.194325	926613.833990	44.628749
3504.390367	926533.800884	44.633754
3504.146158	926448.165819	44.638759
3504.166717	926383.448390	44.643764
3504.502796	926310.119989	44.648769
3504.092194	926223.739479	44.653773
3504.411503	926154.258174	44.658778
3504.552237	926065.572570	44.663783
3504.280918	925972.337415	44.668788
3504.568709	925901.607887	44.673793
3504.074329	925818.023510	44.678797
3504.413193	925739.493773	44.683802
3504.184191	925651.727787	44.688807
3504.353366	925569.280483	44.693812
3504.361373	925485.031147	44.698817
3504.188171	925399.944757	44.703821
3504.208575	925311.939804	44.708826
3503.951873	925246.869677	44.713831
3503.899987	925163.202250	44.718836
3504.120480	925092.184650	44.723841
3503.736966	925020.303775	44.728845
3504.065665	924938.878571	44.733850
3503.706062	924868.338312	44.738855
3503.904133	924794.050171	44.743860
3504.109504	924711.968551	44.748865
3503.831493	924653.050822	44.753869
3503.647153	924566.221702	44.758874
3503.770728	924513.007754	44.763879
3503.867662	924415.548756	44.768884
3503.927080	924361.862919	44.773889
3504.028826	924294.028805	44.778893
3503.980260	924211.211837	44.783898
3503.753307	924153.338414	44.788903
3503.995002	924068.162682	44.793908
3504.019540	924001.011008	44.798913
3503.758762	923924.477665	44.803917
3504.047785	923838.809515	44.808922
3504.122008	923757.793250	44.813927
3503.712862	923697.636025	44.818932
3503.747090	923618.740806	44.823937
3503.419682	923561.166209	44.828941
3504.007049	923471.017485	44.833946
3504.096353	923423.667300	44.838951
3503.762605	923350.216609	44.843956
3503.967678	923262.051628	44.848961
3503.869053	923198.566419	44.853965
3504.039975	923117.717075	44.858970
3503.534255	923059.492991	44.863975
3503.837112	922974.097533	44.868980
3503.745269	922904.257276	44.873985
3503.818811	922828.519344	44.878989
3504.105837	922760.250598	44.883994
3503.814258	922687.265079	44.888999
3503.737320	922619.343181	44.894004
3503.736678	922551.792773	44.899009
3503.627027	922497.827612	44.904013
3503.965078	922410.396696	44.909018
3503.729671	922360.107591	44.914023
3503.514975	922289.221111	44.919028
3503.756691	922213.158187	44.924033
3503.499152	922151.322839	44.929037
3503.753675	922092.770665	44.934042
3503.829720	922007.686057	44.939047
3503.809773	921944.558142	44.944052
3503.945088	921876.495742	44.949057
3503.732011	921801.849310	44.954061
3504.014854	921725.869027	44.959066
3504.135207	921654.341614	44.964071
3503.726643	921578.280666	44.969076
3504.095956	921491.503515	44.974081
3503.809189	921437.364488	44.979085
3503.874424	921372.579700	44.984090
3503.791634	921285.103741	44.989095
3503.796415	921221.097099	44.994100
3504.033607	921149.928803	44.999105
3503.418948	921090.161470	45.004109
3503.735832	921011.278010	45.009114
3503.785872	920948.608263	45.014119
3503.497298	920881.854544	45.019124
3503.535907	920811.677097	45.024129
3503.580162	920750.257366	45.029133
3503.687759	920682.377097	45.034138
3503.257012	920623.921978	45.039143
3503.582824	920550.132193	45.044148
3503.528295	920490.073469	45.049153
3503.310021	920423.302541	45.054157
3504.063413	920355.023025	45.059162
3503.374178	920295.548028	45.064167
3503.632831	920220.609641	45.069172
3503.711843	920171.211153	45.074177
3503.488518	920109.154381	45.079181
3503.687344	920022.285617	45.084186
3503.529867	919966.955387	45.089191
3503.353883	919903.733204	45.094196
3503.790694	919834.247759	45.099201
3503.608396	919769.484659	45.104205
3503.782989	919689.931568	45.109210
3503.649688	919636.519549	45.114215
3503.487117	919571.269452	45.119220
3503.478583	919505.222955	45.124225
3503.240123	919459.240133	45.129229
3503.735323	919389.161713	45.134234
3503.262472	919334.069569	45.139239
3503.465229	919261.823157	45.144244
3503.475497	919213.679022	45.149249
3503.327683	919137.829848	45.154253
3503.785070	919079.308137	45.159258
3503.563321	919012.905647	45.164263
3503.674170	918941.729323	45.169268
3503.681414	918889.346033	45.174273
3503.295018	918810.739153	45.179277
3503.368386	918740.818192	45.184282
3503.612398	918694.267978	45.189287
3503.621749	918624.644960	45.194292
3503.754786	918562.319288	45.199297
3503.198511	918503.284294	45.204301
3503.736493	918430.779078	45.209306
3503.449014	918376.417121	45.214311
3503.322368	918315.864824	45.219316
3503.388441	918232.167392	45.224321
3503.140115	918190.027623	45.229325
3503.446639	918117.363770	45.234330
3503.383447	918069.125342	45.239335
3503.660154	917994.923878	45.244340
3503.855006	917931.714071	45.249345
3503.458793	917875.824106	45.254349
3503.116247	917812.123577	45.259354
3503.403037	917755.638329	45.264359
3503.613365	917700.995033	45.269364
3503.916734	917612.529719	45.274369
3503.769095	917556.017656	45.279373
3503.493328	917471.498057	45.284378
3503.437746	917433.943906	45.289383
3503.286728	917349.883467	45.294388
3503.311610	917307.691895	45.299393
3503.011783	917255.054569	45.304397
3503.249534	917186.627790	45.309402
3503.362265	917129.586829	45.314407
3503.335147	917069.485954	45.319412
3503.325678	917006.491770	45.324417
3503.241450	916943.412850	45.329421
3503.480903	916882.206428	45.334426
3503.376863	916819.418325	45.339431
3503.330304	916765.578639	45.344436
3503.455376	916710.746854	45.349441
3503.494285	916648.607559	45.354445
3503.493071	916588.786139	45.359450
3503.410525	916515.972472	45.364455
3503.340835	916468.106342	45.369460
3503.365965	916402.016818	45.374465
3503.149579	916357.545623	45.379469
3503.659542	916279.140053	45.384474
3503.230555	916237.304015	45.389479
3503.259336	916173.523256	45.394484
3503.465381	916107.400384	45.399489
3503.089316	916056.594570	45.404493
3503.444517	915981.389510	45.409498
3503.438905	915936.398469	45.414503
3503.194317	915861.483249	45.419508
3503.437653	915811.054860	45.424513
3503.037118	915748.977762	45.429517
3503.190544	915687.772194	45.434522
3503.312989	915623.198832	45.439527
3503.386884	915584.165448	45.444532
3503.125428	915510.308062	45.449537
3502.790030	915468.450741	45.454541
3502.786459	915405.340852	45.459546
3503.090898	915360.004962	45.464551
3502.829513	915303.681125	45.469556
3503.034944	915243.714658	45.474561
3503.027549	915204.691970	45.479565
3503.011556	915145.049969	45.484570
3502.961880	915102.468293	45.489575
3502.653093	915041.524382	45.494580
3503.104651	914991.825059	45.499585
3502.936766	914947.045368	45.504589
3503.041546	914883.429839	45.509594
3503.115885	914852.871043	45.514599
3502.745688	914789.910844	45.519604
3502.829458	914742.775310	45.524609
3502.852176	914685.241966	45.529613
3503.033401	914629.609242	45.534618
3502.892968	914577.209062	45.539623
3502.712567	914525.585913	45.544628
3502.955729	914476.398111	45.549633
3502.798293	914434.407230	45.554637
3503.176597	914382.016119	45.559642
3502.749938	914336.984973	45.564647
3502.808240	914277.803195	45.569652
3502.991577	914239.224108	45.574657
3502.762293	914175.751802	45.579661
3502.837658	914134.491283	45.584666
3502.942194	914081.371409	45.589671
3502.764391	914026.466366	45.594676
3503.384148	913967.574285	45.599681
3502.673915	913923.935760	45.604685
3503.052089	913855.733526	45.609690
3503.072230	913820.069787	45.614695
3502.809002	913765.561738	45.619700
3502.672839	913718.453668	45.624705
3502.893783	913656.539723	45.629709
3503.024634	913619.410699	45.634714
3502.875276	913568.448155	45.639719
3502.795791	913512.557948	45.644724
3502.918094	913451.139876	45.649729
3502.976591	913416.816632	45.654733
3502.764165	913362.103449	45.659738
3502.850947	913327.389435	45.664743
3502.543940	913271.919822	45.669748
3502.894805	913212.100077	45.674753
3502.514055	913168.401289	45.679757
3502.763169	913132.406214	45.684762
3502.688092	913086.824971	45.689767
3502.404120	913049.374867	45.694772
3502.831617	912985.491494	45.699777
3502.520583	912957.684737	45.704781
3502.993663	912907.384728	45.709786
3502.734934	912857.493994	45.714791
3502.583061	912810.669954	45.719796
3502.667980	912747.418647	45.724801
3502.717748	912721.093657	45.729805
3503.104591	912654.128358	45.734810
3502.792999	912626.512826	45.739815
3502.649862	912570.045152	45.744820
3502.598579	912503.439401	45.749825
3502.759266	912404.116621	45.754829
3502.792484	912230.386296	45.759834
3502.656346	912014.353648	45.764839
3502.565823	911733.127522	45.769844
3502.459935	911387.961536	45.774849
3502.530278	910979.294342	45.779853
3502.805629	910511.543350	45.784858
3502.493731	909970.549923	45.789863
3502.451092	909386.150064	45.794868
3502.431675	908713.319637	45.799873
3501.986245	907998.991057	45.804877
3501.913426	907198.339611	45.809882
3501.830104	906347.293448	45.814887
3501.559759	905402.325511	45.819892
3501.755672	904427.096523	45.824897
3501.421915	903347.596041	45.829901
3501.318564	902183.921467	45.834906
3501.201611	900964.752551	45.839911
3500.939101	899678.674070	45.844916
3500.886946	898286.536770	45.849921
3500.400385	896841.153533	45.854925
3500.317079	895303.183952	45.859930
3500.093369	893702.919489	45.864935
3499.662144	891998.329114	45.869940
3499.311590	890216.277288	45.874945
3499.108389	888361.233661	45.879949
3498.981290	886419.970863	45.884954
3498.494797	884407.881071	45.889959
3498.004303	882313.690052	45.894964
3498.086227	880123.063167	45.899969
3497.443441	877866.080014	45.904973
3497.043215	875517.282180	45.909978
3496.961962	873070.631742	45.914983
3496.079329	870569.314267	45.919988
3496.264868	867974.876328	45.924993
3495.500669	865304.642476	45.929997
3494.708820	862539.503367	45.935002
3494.240373	859707.685807	45.940007
3493.670207	856773.650979	45.945012
3493.671589	853773.179831	45.950017
3492.907884	850695.494465	45.955021
3492.512791	847529.971972	45.960026
3491.883371	844282.246418	45.965031
3491.323753	840956.251077	45.970036
3490.755948	837540.173984	45.975041
3490.043531	834066.336608	45.980045
3489.202982	830469.617337	45.985050
3488.378425	826842.212985	45.990055
3487.586583	823100.334697	45.995060
3487.437427	819302.688719	46.000065
3486.478312	815408.836064	46.005069
3485.984352	811448.018605	46.010074
3485.261392	807390.490340	46.015079
3484.481708	803245.934885	46.020084
3483.944744	799031.499954	46.025089
3483.046492	794742.221562	46.030093
3482.379215	790372.779029	46.035098
3481.750680	785907.836083	46.040103
3480.796803	781378.604553	46.045108
3480.049127	776748.956171	46.050113
3478.844641	772052.153801	46.055117
3478.141831	767261.711949	46.060122
3477.040076	762396.137406	46.065127
3475.968739	757449.029812	46.070132
3475.435353	752431.301962	46.075137
3474.885025	747311.060186	46.080141
3473.522969	742121.916365	46.085146
3472.458080	736855.477274	46.090151
3471.534512	731507.599825	46.095156
3470.456541	726086.001454	46.100161
3469.368801	720554.352429	46.105165
3468.175330	714967.645296	46.110170
3467.229854	709282.803466	46.115175
3466.024174	703542.612847	46.120180
3465.229438	697683.898185	46.125185
3463.897757	691769.445093	46.130189
3462.744408	685749.486882	46.135194
3461.595045	679665.268244	46.140199
3460.149294	673509.148891	46.145204
3459.281811	667260.303998	46.150209
3457.805135	660939.689304	46.155213
3456.891708	654542.548037	46.160218
3455.330662	648047.409061	46.165223
3453.669491	641493.442091	46.170228
3452.718635	634833.576123	46.175233
3451.040429	628143.115489	46.180237
3450.046328	621315.295782	46.185242
3448.769774	614454.325287	46.190247
3447.263262	607479.729356	46.195252
3445.969986	600459.962726	46.200257
3444.194130	593350.837986	46.205261
3442.594910	586156.105684	46.210266
3441.078842	578900.933150	46.215271
3439.674361	571567.999197	46.220276
3437.803618	564130.578774	46.225281
3436.365839	556646.152768	46.230285
3434.631659	549071.314048	46.235290
3432.725874	541438.495583	46.240295
3431.013460	533712.330986	46.245300
3429.430372	525927.547351	46.250305
3427.387412	518076.746754	46.255309
3425.913131	510134.662868	46.260314
3423.675637	502142.070481	46.265319
3421.788423	494064.944704	46.270324
3420.315903	485911.289823	46.275329
3418.091913	477717.846900	46.280333
3416.276038	469416.113523	46.285338
3414.252744	461072.040050	46.290343
3412.024243	452655.904798	46.295348
3410.179401	444166.863177	46.300353
3407.952475	435636.117760	46.305357
3405.879486	427001.045645	46.310362
3403.657959	418324.514062	46.315367
3401.427250	409584.142611	46.320372
3399.150167	400780.880529	46.325377
3396.521630	391897.531379	46.330381
3394.266732	382967.484655	46.335386
3392.058514	373996.221937	46.340391
3389.345057	364948.855883	46.345396
3386.832899	355844.250133	46.350401
3384.485193	346706.427388	46.355405
3381.664683	337504.433317	46.360410
3379.028349	328245.723715	46.365415
3375.970878	318961.650110	46.370420
3373.386877	309613.931861	46.375425
3370.437469	300233.848165	46.380429
3367.473250	290779.922896	46.385434
3364.411006	281317.987736	46.390439
3361.615705	271790.223291	46.395444
3358.776730	262250.597848	46.400449
3355.422361	252660.944092	46.405453
3352.381000	243018.566521	46.410458
3348.895969	233356.028282	46.415463
3345.178251	223669.826266	46.420468
3342.551868	213859.500093	46.425473
3338.388507	204112.104803	46.430477
3334.943145	194355.016670	46.435482
3331.103533	184554.421070	46.440487
3327.218027	174780.386097	46.445492
3323.513176	164955.982104	46.450497
3319.198151	155147.770599	46.455501
3315.335819	145317.022727	46.460506
3310.536002	135496.731596	46.465511
3305.687251	125692.973830	46.470516
3301.055034	115877.512223	46.475521
3295.555156	106106.060311	46.480525
3289.674277	96348.828820	46.485530
3283.247579	86665.282403	46.490535
3271.090539	77155.955391	46.495540
3250.355300	68010.342184	46.500545
3227.123542	59137.377906	46.505549
3203.478183	50593.857534	46.510554
3175.988927	42593.225066	46.515559
3142.445172	35229.412841	46.520564
3104.870432	28598.193718	46.525569
3066.749768	22684.848090	46.530573
3031.157653	17495.260254	46.535578
2999.556371	13023.766597	46.540583
2971.630371	9273.074431	46.545588
2947.886393	6143.735905	46.550593
2927.496470	3646.328221	46.555597
2909.693746	1703.195765	46.560602
2887.471898	441.870561	46.565607
2843.153016	319.958672	46.570612
2820.645170	313.983643	46.575617
2821.767637	304.603879	46.580621
2836.669951	320.745842	46.585626
2854.633281	319.371834	46.590631
2869.064478	313.364967	46.595636
2878.218308	292.950012	46.600641
2880.569183	303.059344	46.605645
2879.151404	297.908486	46.610650
2875.138633	298.827015	46.615655
2870.862514	304.941327	46.620660
2866.937157	287.135630	46.625665
2863.977876	298.472578	46.630669
2861.446780	287.948833	46.635674
2859.397695	286.304348	46.640679
2856.813133	289.364332	46.645684
2854.734849	289.025083	46.650689
2852.013874	292.742380	46.655693
2849.007025	281.393828	46.660698
2845.928290	263.803740	46.665703
2842.785442	283.544062	46.670708
2840.027244	274.295455	46.675713
2836.612972	275.205302	46.680717
2833.552353	276.882752	46.685722
2830.371062	270.141478	46.690727
2827.017685	284.041147	46.695732
2824.484912	263.980608	46.700737
2821.547572	276.981040	46.705741
2818.330148	273.847975	46.710746
2814.601047	255.974678	46.715751
2811.050193	273.200858	46.720756
2808.127675	267.299071	46.725761
2804.767368	274.276844	46.730765
2801.289853	284.505067	46.735770
2798.403492	269.640487	46.740775
2794.802285	273.400423	46.745780
2791.997866	266.277207	46.750785
2788.351518	264.306153	46.755789
2784.923228	256.863083	46.760794
2781.668608	251.803402	46.765799
2777.926995	269.549952	46.770804
2775.026159	256.062980	46.775809
2771.501591	265.233529	46.780813
2768.410592	256.767091	46.785818
2764.886430	247.176132	46.790823
2761.380305	259.185477	46.795828
2758.243589	246.749178	46.800833
2754.276973	255.223823	46.805837
2751.173909	250.373958	46.810842
2748.153199	245.889634	46.815847
2744.699319	257.712797	46.820852
2740.945639	240.821548	46.825857
2737.242242	253.127214	46.830861
2734.091945	255.382882	46.835866
2730.997670	233.497337	46.840871
2727.409748	256.440233	46.845876
2723.763088	237.511574	46.850881
2720.719210	257.191865	46.855885
2717.467018	250.682237	46.860890
2714.238954	252.542714	46.865895
2710.068194	255.378217	46.870900
2706.542149	242.815351	46.875905
2703.331843	253.162600	46.880909
2700.254227	260.069920	46.885914
2696.899224	236.018490	46.890919
2692.994134	257.962764	46.895924
2689.687452	246.028347	46.900929
2686.101049	264.843759	46.905933
2682.878090	241.369862	46.910938
2679.043863	246.213567	46.915943
2675.695551	237.809441	46.920948
2672.543905	238.867437	46.925953
2668.880382	232.006497	46.930957
2664.837246	241.114993	46.935962
2662.003599	234.564208	46.940967
2658.561404	228.045798	46.945972
2654.774035	232.675997	46.950977
2650.837631	238.114752	46.955981
2647.752435	230.717200	46.960986
2644.731570	233.980977	46.965991
2640.978541	235.149196	46.970996
2638.157137	221.692931	46.976001
2634.678661	222.734593	46.981005
2630.844931	223.515403	46.986010
2627.490817	229.729927	46.991015
2623.931742	235.334159	46.996020
2620.587579	227.062070	47.001025
2616.855517	227.496926	47.006029
2613.808376	233.387083	47.011034
2609.977864	229.363086	47.016039
2606.194965	227.797606	47.021044
2603.285571	235.549379	47.026049
2599.465877	229.882748	47.031053
2595.763156	235.846189	47.036058
2592.741558	224.294064	47.041063
2588.808162	227.041356	47.046068
2585.572177	217.066698	47.051073
2582.416583	225.077383	47.056077
2578.892242	222.446177	47.061082
2575.287378	221.586500	47.066087
2571.402426	236.646582	47.071092
2568.429735	213.894205	47.076097
2565.129250	237.839845	47.081101
2561.803163	221.660626	47.086106
2558.168888	209.461197	47.091111
2554.147997	221.493514	47.096116
2550.632381	215.352675	47.101121
2547.330374	234.861661	47.106125
2544.084590	222.257428	47.111130
2540.656489	212.783364	47.116135
2536.554576	225.236773	47.121140
2533.335452	208.732946	47.126145
2529.633865	227.494052	47.131149
2526.416881	218.216414	47.136154
2522.858500	223.701498	47.141159
2519.354600	215.922625	47.146164
2516.229342	221.764035	47.151169
2513.028495	221.351436	47.156173
2509.000977	230.782471	47.161178
2505.553376	217.879685	47.166183
2501.953026	228.822928	47.171188
2498.723091	221.738170	47.176193
2494.901532	212.866068	47.181197
2491.084739	215.842677	47.186202
2488.571180	216.415419	47.191207
2485.012301	209.965379	47.196212
2481.406180	212.507520	47.201217
2477.718286	208.172221	47.206221
2474.040632	217.586704	47.211226
2470.378703	216.486015	47.216231
2466.989386	206.321261	47.221236
2464.147410	214.859141	47.226241
2460.151941	204.438818	47.231245
2456.495621	214.117624	47.236250
2453.430646	210.206501	47.241255
2449.566839	207.625425	47.246260
2446.505220	217.749626	47.251265
2443.036172	215.757601	47.256269
2439.241774	206.555807	47.261274
2435.728862	197.947050	47.266279
2431.975317	199.216667	47.271284
2429.263344	191.171215	47.276289
2425.024063	201.746712	47.281293
2421.699973	199.817014	47.286298
2418.096557	184.148302	47.291303
2414.916523	198.043004	47.296308
2411.439129	212.009153	47.301313
2408.115636	202.576317	47.306317
2404.224309	206.348344	47.311322
2401.173988	192.211610	47.316327
2396.994818	206.496222	47.321332
2393.762261	193.245732	47.326337
2390.471230	206.587273	47.331341
2387.016360	190.345680	47.336346
2383.747191	202.716843	47.341351
2380.323971	198.854974	47.346356
2376.645981	195.469581	47.351361
2372.763466	183.396265	47.356365
2369.332639	197.596920	47.361370
2366.035472	194.575289	47.366375
2362.163598	223.936666	47.371380
2358.761298	195.774292	47.376385
2355.529435	211.044663	47.381389
2351.638261	196.242534	47.386394
2348.530105	203.616469	47.391399
2344.790495	205.916796	47.396404
2341.589458	199.529456	47.401409
2338.344335	200.213728	47.406413
2334.441070	196.099986	47.411418
2330.799650	202.279426	47.416423
2327.134767	202.276681	47.421428
2323.940679	203.054349	47.426433
2320.824451	187.827500	47.431437
2317.042193	195.702586	47.436442
2313.833066	201.240140	47.441447
2310.079881	190.930504	47.446452
2306.537986	194.705217	47.451457
2302.979949	187.597842	47.456461
2299.250316	204.317610	47.461466
2295.990428	189.809359	47.466471
2292.361673	202.123845	47.471476
2289.369296	187.915866	47.476481
2285.735882	198.584355	47.481485
2281.691940	201.594383	47.486490
2278.298015	191.125578	47.491495
2274.917327	197.788136	47.496500
2271.876709	189.180596	47.501505
2268.038904	199.023759	47.506509
2264.540091	198.432434	47.511514
2260.879612	200.074676	47.516519
2257.449310	201.533052	47.521524
2254.228607	176.245297	47.526529
2250.775605	196.832691	47.531533
2247.145431	201.865476	47.536538
2243.683758	190.286609	47.541543
2240.161271	202.840076	47.546548
2236.548580	188.653055	47.551553
2233.219802	193.193883	47.556557
2229.304337	194.070156	47.561562
2226.091068	181.433055	47.566567
2222.439885	185.177787	47.571572
2219.185569	179.347503	47.576577
2215.443566	194.006164	47.581581
2211.854988	187.483544	47.586586
2208.556949	185.787396	47.591591
2204.773659	209.988884	47.596596
2201.958100	189.203297	47.601601
2198.195463	194.162754	47.606605
2193.902764	204.632832	47.611610
2190.604620	188.697571	47.616615
2187.081985	187.748365	47.621620
2184.441865	189.067455	47.626625
2181.468213	187.772589	47.631629
2177.382034	183.892133	47.636634
2174.006001	184.087358	47.641639
2170.339619	177.556883	47.646644
2166.594761	180.641932	47.651649
2163.081341	193.263273	47.656653
2159.459557	184.735971	47.661658
2156.264782	173.721714	47.666663
2152.543008	199.946915	47.671668
2148.761603	193.702365	47.676673
2145.458844	206.916781	47.681677
2141.963579	185.559810	47.686682
2138.860551	177.389596	47.691687
2135.251128	201.256593	47.696692
2131.296991	179.127534	47.701697
2127.911193	193.244970	47.706701
2124.706970	177.282431	47.711706
2121.171019	202.484474	47.716711
2117.572220	187.047121	47.721716
2114.032928	189.264497	47.726721
2110.595067	199.565286	47.731725
2106.971309	189.762893	47.736730
2103.460398	199.076115	47.741735
2099.666777	183.437312	47.746740
2096.849097	202.845158	47.751745
2093.255369	182.906974	47.756749
2089.353571	192.473298	47.761754
2086.014902	180.105365	47.766759
2082.404337	187.129188	47.771764
2079.009896	191.851278	47.776769
2075.698074	192.266106	47.781773
2072.027500	193.618987	47.786778
2068.676175	175.203062	47.791783
2064.964947	189.796321	47.796788
2061.808283	169.128576	47.801793
2058.059069	195.221391	47.806797
2054.600529	190.687099	47.811802
2051.411213	182.690480	47.816807
2047.566903	181.698916	47.821812
2043.709333	178.595971	47.826817
2040.544881	188.784297	47.831821
2037.082328	184.666488	47.836826
2033.250702	179.875317	47.841831
2029.717431	171.128602	47.846836
2026.833773	179.622662	47.851841
2023.012635	187.762252	47.856845
2019.679318	180.394228	47.861850
2016.142338	182.711594	47.866855
2012.610721	187.224514	47.871860
2009.088282	182.802400	47.876865
2005.777088	177.558905	47.881869
2002.365309	179.053108	47.886874
1999.071144	178.949908	47.891879
1995.147367	179.769175	47.896884
1991.355529	194.853129	47.901889
1987.767671	184.527470	47.906893
1984.111598	182.790760	47.911898
1981.166263	187.083560	47.916903
1977.249374	183.151028	47.921908
1974.237833	176.819234	47.926913
1970.560406	195.870753	47.931917
1967.045853	190.349090	47.936922
1963.431425	178.251252	47.941927
1959.960639	181.028775	47.946932
1956.578923	168.541757	47.951937
1952.906213	178.030187	47.956941
1949.701954	168.368027	47.961946
1946.371117	179.402620	47.966951
1942.776791	182.781678	47.971956
1939.223158	180.514028	47.976961
1935.629413	180.890395	47.981965
1932.163485	183.015943	47.986970
1928.470636	173.234142	47.991975
1924.687885	175.947236	47.996980
1921.256575	184.699193	48.001985
1918.319535	177.026520	48.006989
1914.763229	192.172954	48.011994
1911.447949	184.317246	48.016999
1907.310103	198.359857	48.022004
1904.268190	184.484432	48.027009
1900.262747	183.631892	48.032013
1896.755930	180.636497	48.037018
1893.743294	189.297095	48.042023
1890.010075	190.716829	48.047028
1886.808231	187.854016	48.052033
1883.308681	165.886829	48.057037
1879.572720	175.799654	48.062042
1876.057266	175.793296	48.067047
1872.169762	185.404111	48.072052
1868.615199	183.371831	48.077057
1865.743817	173.734404	48.082061
1861.988300	190.478892	48.087066
1858.736309	180.911166	48.092071
1855.199307	182.350038	48.097076
1851.489990	175.061410	48.102081
1847.939458	169.632174	48.107085
1844.092303	190.303337	48.112090
1840.957888	176.906083	48.117095
1837.394767	187.843203	48.122100
1834.149359	180.005113	48.127105
1830.398801	185.321630	48.132109
1826.913543	179.368951	48.137114
1823.999559	187.530600	48.142119
1820.030649	181.172863	48.147124
1816.375457	182.984616	48.152129
1813.128700	168.457247	48.157133
1809.178008	181.912621	48.162138
1806.192277	182.275245	48.167143
1802.456069	177.851620	48.172148
1798.759586	178.072469	48.177153
1795.286784	176.533499	48.182157
1791.729879	172.508337	48.187162
1788.578699	176.302659	48.192167
1784.963584	164.772786	48.197172
1781.555384	175.121660	48.202177
1778.299567	173.687175	48.207181
1774.231445	168.510596	48.212186
1771.459845	166.922329	48.217191
1767.677917	173.002859	48.222196
1763.804736	168.245441	48.227201
1760.495865	176.193874	48.232205
1756.845232	171.441466	48.237210
1753.804096	165.944210	48.242215
1749.666619	176.359472	48.247220
1746.179045	175.767040	48.252225
1742.794043	177.413301	48.257229
1739.094825	182.154549	48.262234
1735.963553	163.754535	48.267239
1732.394788	168.743274	48.272244
1728.899016	159.190806	48.277249
1725.523128	158.424089	48.282253
1722.208175	165.083104	48.287258
1718.747328	164.616394	48.292263
1715.049646	161.015320	48.297268
1711.474063	157.796983	48.302273
1707.893214	162.382276	48.307277
1704.273951	158.797665	48.312282
1701.185260	156.980799	48.317287
1697.306796	159.325560	48.322292
1693.982967	164.704894	48.327297
1690.316340	150.175580	48.332301
1686.629083	160.607029	48.337306
1683.273952	159.978568	48.342311
1679.720149	163.214033	48.347316
1676.641469	167.766194	48.352321
1672.982108	153.040167	48.357325
1669.278979	159.505390	48.362330
1666.190658	157.563490	48.367335
1662.346819	167.095759	48.372340
1658.832066	158.067727	48.377345
1655.339642	153.772161	48.382349
1651.919504	165.354287	48.387354
1648.258280	155.537366	48.392359
1644.861216	165.740321	48.397364
1641.376752	135.439154	48.402369
1637.674769	153.597957	48.407373
1634.128686	144.068161	48.412378
1631.238054	146.922231	48.417383
1627.441076	145.141690	48.422388
1623.985083	139.932562	48.427393
1620.309629	153.339215	48.432397
1616.540875	150.819973	48.437402
1613.249116	154.524607	48.442407
1610.130415	145.866985	48.447412
1606.560574	151.224900	48.452417
1603.159583	146.309458	48.457421
1599.097457	155.127250	48.462426
1595.812595	140.195654	48.467431
1592.087883	157.603465	48.472436
1588.753047	153.335693	48.477441
1585.357001	157.071361	48.482445
1581.834895	145.446672	48.487450
1578.392663	153.025339	48.492455
1574.709639	156.489539	48.497460
1571.357315	148.256702	48.502465
1567.816118	159.926703	48.507469
1563.970480	142.377684	48.512474
1561.156619	151.288786	48.517479
1557.710605	146.617163	48.522484
1553.937790	147.470449	48.527489
1550.183006	149.852683	48.532493
1546.385719	145.916757	48.537498
1543.597715	156.356408	48.542503
1539.582744	153.324324	48.547508
1536.044034	152.418052	48.552513
1532.674790	152.454914	48.557517
1529.282146	158.834234	48.562522
1525.903102	149.295379	48.567527
1522.332944	168.404469	48.572532
1518.613196	158.617115	48.577537
1515.380427	160.962144	48.582541
1511.456226	152.958476	48.587546
1508.435114	153.405096	48.592551
1504.791935	153.923013	48.597556
1501.396847	150.053810	48.602561
1497.858679	168.593159	48.607565
1494.303661	155.690821	48.612570
1491.293776	146.570495	48.617575
1487.327941	164.700993	48.622580
1483.722091	155.182723	48.627585
1480.193047	161.065189	48.632589
1476.602229	149.808224	48.637594
1473.350263	146.293240	48.642599
1469.708493	157.428823	48.647604
1465.839637	155.758685	48.652609
1462.807790	151.035229	48.657613
1459.127907	155.523139	48.662618
1455.845032	143.862893	48.667623
1452.178198	139.708788	48.672628
1448.705859	138.975588	48.677633
1445.376517	145.577695	48.682637
1441.641639	146.668541	48.687642
1438.246725	136.527746	48.692647
1434.458731	165.008346	48.697652
1431.132723	148.920072	48.702657
1427.876872	170.212502	48.707661
1424.121736	153.746401	48.712666
1420.669509	157.584145	48.717671
1417.209211	155.068853	48.722676
1413.839895	157.251496	48.727681
1410.188461	156.909128	48.732685
1406.376472	145.415557	48.737690
1403.233617	152.225436	48.742695
1399.456745	153.774357	48.747700
1395.990684	150.385605	48.752705
1393.166601	153.304743	48.757709
1389.292219	157.508917	48.762714
1385.816295	151.969970	48.767719
1382.408813	145.887421	48.772724
1378.328287	157.574106	48.777729
1374.831481	147.608985	48.782733
1371.388958	147.274080	48.787738
1368.541888	146.806363	48.792743
1364.538369	147.509707	48.797748
1361.175973	148.109695	48.802753
1357.682703	151.567341	48.807757
1353.854423	148.258328	48.812762
1350.838963	149.783793	48.817767
1347.372627	144.854515	48.822772
1343.831209	146.971783	48.827777
1339.964886	142.269925	48.832781
1336.415914	159.757923	48.837786
1333.119635	148.630591	48.842791
1329.345206	167.226056	48.847796
1326.071460	152.901545	48.852801
1322.690651	159.072822	48.857805
1319.140454	154.466664	48.862810
1315.795873	146.426936	48.867815
1311.828125	165.859388	48.872820
1308.479648	153.065233	48.877825
1305.032882	160.367561	48.882829
1301.533234	151.083530	48.887834
1298.469195	155.284992	48.892839
1294.447599	162.894901	48.897844
1291.195946	153.726986	48.902849
1287.686163	145.806090	48.907853
1283.776101	152.564599	48.912858
1280.821832	153.608058	48.917863
1277.090041	156.737846	48.922868
1273.474789	141.921464	48.927873
1270.012683	155.625480	48.932877
1266.704305	150.286229	48.937882
1263.332471	156.626415	48.942887
1259.458668	148.353571	48.947892
1255.985235	156.621356	48.952897
1252.589681	152.061031	48.957901
1248.784401	147.239452	48.962906
1245.770580	148.240768	48.967911
1242.013570	149.984481	48.972916
1238.347742	161.391963	48.977921
1235.058199	144.171531	48.982925
1231.564640	161.127777	48.987930
1228.118855	133.633343	48.992935
1224.242577	144.268714	48.997940
1220.656056	138.785116	49.002945
1217.392064	146.087785	49.007949
1213.880170	153.782671	49.012954
1210.828153	146.952377	49.017959
1207.357197	149.519460	49.022964
1203.413140	154.310057	49.027969
1199.974252	147.354921	49.032973
1196.191558	154.973182	49.037978
1193.184098	132.725257	49.042983
1189.437592	139.614940	49.047988
1186.221401	150.311430	49.052993
1182.244571	132.524031	49.057997
1178.677295	159.880941	49.063002
1175.618765	147.911258	49.068007
1171.920729	146.252748	49.073012
1168.516917	146.583746	49.078017
1165.345982	141.147779	49.083021
1161.234183	151.021631	49.088026
1157.889725	139.164869	49.093031
1154.418289	142.656984	49.098036
1151.094551	136.427569	49.103041
1147.708397	143.733663	49.108045
1144.096866	138.844256	49.113050
1140.476866	134.194092	49.118055
1136.494254	135.647495	49.123060
1133.077345	133.936973	49.128065
1130.113896	138.603986	49.133069
1126.421245	146.542717	49.138074
1122.964705	131.933254	49.143079
1119.696642	135.897184	49.148084
1115.800323	145.982792	49.153089
1112.075886	134.765298	49.158093
1108.860551	129.399732	49.163098
1105.727754	136.766309	49.168103
1101.966421	138.204901	49.173108
1098.401015	134.933831	49.178113
1095.027292	129.105816	49.183117
1091.250153	133.697853	49.188122
1088.080530	139.942967	49.193127
1084.357638	133.859002	49.198132
1080.793624	144.287413	49.203137
1077.568750	133.178349	49.208141
1073.734417	135.938664	49.213146
1070.409056	136.471023	49.218151
1067.348520	129.409705	49.223156
1063.474476	141.882202	49.228161
1060.032249	133.489905	49.233165
1056.022380	139.761303	49.238170
1052.618860	143.258628	49.243175
1049.003265	142.801234	49.248180
1046.021878	137.239728	49.253185
1042.755514	125.268251	49.258189
1039.177608	147.646669	49.263194
1035.240206	123.340315	49.268199
1031.767097	143.045913	49.273204
1028.252789	141.874362	49.278209
1025.203417	125.272817	49.283213
1020.879420	141.792686	49.288218
1017.976503	126.603480	49.293223
1014.330689	134.843786	49.298228
1010.809923	134.021245	49.303233
1007.354518	135.823304	49.308237
1003.410581	126.111499	49.313242
1000.591050	134.846828	49.318247
996.986580	130.956342	49.323252
993.411571	140.542765	49.328257
989.836517	121.868435	49.333261
986.010333	144.484366	49.338266
982.626528	112.761040	49.343271
978.977003	127.890672	49.348276
975.643078	137.914553	49.353281
972.432900	122.312072	49.358285
968.672981	119.636281	49.363290
965.496389	133.661102	49.368295
961.825462	141.271570	49.373300
958.170374	130.139013	49.378305
954.979056	129.012918	49.383309
951.096312	138.234270	49.388314
947.992088	134.487213	49.393319
944.438728	153.732788	49.398324
940.690448	139.548054	49.403329
937.129592	148.047728	49.408333
933.800026	133.871107	49.413338
929.974127	134.442681	49.418343
926.772669	134.678929	49.423348
923.147962	130.495094	49.428353
920.040796	129.542157	49.433357
915.917229	137.523529	49.438362
912.889482	119.055026	49.443367
909.365071	126.664204	49.448372
905.295336	134.075185	49.453377
902.405754	120.605461	49.458381
898.613781	124.282419	49.463386
895.362395	127.646279	49.468391
891.728125	122.555100	49.473396
888.119058	119.374523	49.478401
884.358905	133.112191	49.483405
880.836769	121.600730	49.488410
877.900987	128.967709	49.493415
873.928839	137.339309	49.498420
870.826246	120.822318	49.503425
867.526876	124.937428	49.508429
863.968951	128.830958	49.513434
860.320948	120.005177	49.518439
856.555709	139.619478	49.523444
853.200825	122.134397	49.528449
849.908089	129.864366	49.533453
846.355244	132.541327	49.538458
842.977699	123.039939	49.543463
838.768641	139.042638	49.548468
835.551419	125.390003	49.553473
832.315161	130.556950	49.558477
828.812034	135.171642	49.563482
824.948238	136.595443	49.568487
821.479736	129.900827	49.573492
818.024587	143.206691	49.578497
815.171135	121.959351	49.583501
811.012401	130.776214	49.588506
807.860821	115.382774	49.593511
804.206651	121.203629	49.598516
800.373868	136.324833	49.603521
797.023838	121.788273	49.608525
793.281697	134.778509	49.613530
790.072790	116.055902	49.618535
786.550753	125.888465	49.623540
782.920358	117.223288	49.628545
779.857647	116.066275	49.633549
775.905975	119.723405	49.638554
772.859809	116.311135	49.643559
769.261625	122.495553	49.648564
765.583462	119.036432	49.653569
761.989236	127.955710	49.658573
758.244792	131.128102	49.663578
755.105369	122.186434	49.668583
751.460578	121.242562	49.673588
747.935713	131.402827	49.678593
745.181597	117.818490	49.683597
741.151453	111.766946	49.688602
737.741984	118.904125	49.693607
734.031537	124.937327	49.698612
730.171267	121.784222	49.703617
726.911701	126.395630	49.708621
723.433263	111.397553	49.713626
720.125711	121.368831	49.718631
716.531074	113.238188	49.723636
713.399822	122.249708	49.728641
709.907503	104.473253	49.733645
705.754833	123.451570	49.738650
702.348690	111.038475	49.743655
699.029955	115.139593	49.748660
695.607599	104.554072	49.753665
692.298880	125.433441	49.758669
688.452455	127.884433	49.763674
685.037571	118.642443	49.768679
681.361583	108.005597	49.773684
678.012847	135.875957	49.778689
674.416034	123.699845	49.783693
670.771892	123.205351	49.788698
667.378721	110.940081	49.793703
663.789300	131.197094	49.798708
660.597260	119.245941	49.803713
657.216459	112.433663	49.808717
653.270955	121.215879	49.813722
650.175661	110.340200	49.818727
646.595995	112.024066	49.823732
642.896742	117.986113	49.828737
639.646332	112.320497	49.833741
636.023569	123.671080	49.838746
632.633759	112.955132	49.843751
629.215266	116.457198	49.848756
624.990235	98.233525	49.853761
622.050931	115.034753	49.858765
618.282361	120.357878	49.863770
614.889829	128.400173	49.868775
611.397657	120.621117	49.873780
607.866619	115.243260	49.878785
604.300739	116.757564	49.883789
600.933280	110.629508	49.888794
597.431770	114.058392	49.893799
593.940054	113.174163	49.898804
590.513305	110.141509	49.903809
587.123610	111.822339	49.908813
583.475554	107.049697	49.913818
579.884728	112.177358	49.918823
576.559236	106.816375	49.923828
572.599752	112.306993	49.928833
569.522231	108.902966	49.933837
566.049804	115.708113	49.938842
562.651357	102.684597	49.943847
558.775428	122.614592	49.948852
554.991063	117.250200	49.953857
552.189246	132.668107	49.958861
548.045578	126.874070	49.963866
545.022294	117.917189	49.968871
541.326262	124.843532	49.973876
537.896095	121.356013	49.978881
534.821557	116.612366	49.983885
530.774619	129.780413	49.988890
527.439318	121.964349	49.993895
523.577593	134.863476	49.998900
520.308622	126.263255	50.003905
517.050414	125.162534	50.008909
513.186772	139.234217	50.013914
509.905345	118.400781	50.018919
506.429548	134.686368	50.023924
502.791619	118.271370	50.028929
499.888747	124.178291	50.033933
495.863526	113.849329	50.038938
491.994722	119.796747	50.043943
488.624574	118.654061	50.048948
485.196327	118.490188	50.053953
481.964178	116.719606	50.058957
478.163722	110.410808	50.063962
474.838043	107.980044	50.068967
471.331376	116.999611	50.073972
467.781026	118.306630	50.078977
464.551669	129.939445	50.083981
460.862480	130.382660	50.088986
457.339318	114.529874	50.093991
453.852244	122.431103	50.098996
449.938353	132.128885	50.104001
446.861065	117.589334	50.109005
443.183946	131.071587	50.114010
440.094334	116.810389	50.119015
436.248321	124.232801	50.124020
432.581061	117.993867	50.129025
429.307326	123.393280	50.134029
425.586706	121.996997	50.139034
422.417663	125.593498	50.144039
419.069617	121.208696	50.149044
415.275747	125.602409	50.154049
411.803380	102.101317	50.159053
407.899572	124.548627	50.164058
404.557500	106.417497	50.169063
401.342363	108.064058	50.174068
398.066369	110.901585	50.179073
394.434954	121.878052	50.184077
390.551089	116.464505	50.189082
387.343563	118.024092	50.194087
383.419691	115.992484	50.199092
380.212242	124.201203	50.204097
376.770717	114.764740	50.209101
373.200062	122.895063	50.214106
369.436112	109.102922	50.219111
366.050062	127.685825	50.224116
362.446895	125.701669	50.229121
359.425242	124.977550	50.234125
355.679716	125.190517	50.239130
352.410640	127.186941	50.244135
348.984822	122.491857	50.249140
344.934937	130.556262	50.254145
341.403443	125.813731	50.259149
337.725884	116.318824	50.264154
334.706705	119.870875	50.269159
331.277457	109.543799	50.274164
327.631747	126.549921	50.279169
324.493014	118.008605	50.284173
320.779571	117.980426	50.289178
317.311782	129.502843	50.294183
313.933833	125.360484	50.299188
310.092972	127.011036	50.304193
306.836808	118.122755	50.309197
302.993475	128.400343	50.314202
299.598599	122.328680	50.319207
296.236121	125.841189	50.324212
292.805281	117.015219	50.329217
288.921465	119.178250	50.334221
285.139814	113.894773	50.339226
281.995536	125.337806	50.344231
278.528308	121.517013	50.349236
275.185541	118.670815	50.354241
271.832954	116.245000	50.359245
268.124411	106.683648	50.364250
264.589877	107.189317	50.369255
261.339971	112.213655	50.374260
257.223647	124.086711	50.379265
254.243435	106.423466	50.384269
250.514758	122.349126	50.389274
247.082683	109.427947	50.394279
243.443526	123.053654	50.399284
239.866175	113.060070	50.404289
236.440914	114.935668	50.409293
232.991322	112.509034	50.414298
229.855067	114.847284	50.419303
226.440833	119.673876	50.424308
222.527756	116.791530	50.429313
219.124502	118.000689	50.434317
215.427948	114.085344	50.439322
212.260423	114.867576	50.444327
208.484200	105.691815	50.449332
204.910226	123.042245	50.454337
201.516436	112.524626	50.459341
197.834419	129.544495	50.464346
194.681544	105.425925	50.469351
191.307704	112.169381	50.474356
187.235437	104.303069	50.479361
183.971899	103.424966	50.484365
180.390709	114.575624	50.489370
177.379004	98.857345	50.494375
173.526899	119.476446	50.499380
169.960664	113.095905	50.504385
166.600745	104.763970	50.509389
162.960867	117.441727	50.514394
159.852746	108.686223	50.519399
156.321045	108.618344	50.524404
152.226844	98.639603	50.529409
149.022877	114.366726	50.534413
145.217452	118.788636	50.539418
142.042153	118.938971	50.544423
138.297594	106.199425	50.549428
134.944149	100.040331	50.554433
131.521530	99.987881	50.559437
127.875196	107.276633	50.564442
124.331007	110.991390	50.569447
120.714780	104.068891	50.574452
117.291027	113.523168	50.579457
114.355284	101.424960	50.584461
110.827005	116.946940	50.589466
107.390548	111.743755	50.594471
103.505707	116.902487	50.599476
99.534150	123.152880	50.604481
96.567405	115.335957	50.609485
92.864559	125.150860	50.614490
89.607358	108.146884	50.619495
86.073852	119.260804	50.624500
82.389466	108.803816	50.629505
78.901437	114.850214	50.634509
75.119549	120.030620	50.639514
71.857883	124.693576	50.644519
68.688973	107.813328	50.649524
64.861812	127.919341	50.654529
61.593740	118.297861	50.659533
57.763485	119.681743	50.664538
54.406296	128.959329	50.669543
51.060936	121.053870	50.674548
47.041645	125.426738	50.679553
43.799357	113.052799	50.684557
40.466009	123.698137	50.689562
36.463076	124.118178	50.694567
33.417537	113.373837	50.699572
29.683136	122.278144	50.704577
26.655358	107.816514	50.709581
22.825419	126.536121	50.714586
19.295601	107.646526	50.719591
15.946540	108.638888	50.724596
12.202881	111.066081	50.729601
8.985467	99.722084	50.734605
5.480957	94.366953	50.739610
2.211106	110.588973	50.744615