Wed Jun 15 16:02:18 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
0.370110	93.369870	0.000000
-0.299790	84.702890	0.005005
-0.501870	86.275977	0.010010
-0.652498	79.559653	0.015014
-0.600483	85.069077	0.020019
-0.454727	83.730435	0.025024
-0.728953	78.927471	0.030029
-0.513607	61.950379	0.035034
-0.687419	52.971490	0.040038
-1.348014	56.418280	0.045043
-1.591348	38.685840	0.050048
-1.718643	43.917499	0.055053
-2.323872	21.005273	0.060058
-2.713148	21.788649	0.065062
-3.271306	19.280482	0.070067
-3.000367	4.672853	0.075072
-3.424654	9.610389	0.080077
-3.710997	8.793973	0.085082
-3.812464	-0.498795	0.090086
-4.471459	9.489450	0.095091
-4.543418	-10.318065	0.100096
-5.124256	5.567453	0.105101
-5.075297	-4.107469	0.110106
-5.309769	-18.639346	0.115110
-5.741194	4.154137	0.120115
-6.219137	-18.892802	0.125120
-6.867409	1.066697	0.130125
-6.883651	2.298625	0.135130
-6.735960	4.092282	0.140134
-7.078525	-9.319861	0.145139
-6.941604	-12.300382	0.150144
-7.331701	3.166426	0.155149
-7.362090	4.102583	0.160154
-7.909604	4.026166	0.165158
-8.675028	9.439520	0.170163
-8.859970	-10.783465	0.175168
-9.161927	-1.989352	0.180173
-9.085474	-2.194729	0.185178
-8.888328	-10.465244	0.190182
-8.610596	2.968784	0.195187
-9.556141	-2.792835	0.200192
-10.201598	-2.097634	0.205197
-10.328282	-13.123091	0.210202
-10.249955	-8.817094	0.215206
-10.641549	-2.256316	0.220211
-10.723697	-3.425793	0.225216
-11.663941	-8.572831	0.230221
-11.866991	-12.220247	0.235226
-11.818177	-11.770978	0.240230
-11.982138	-9.135368	0.245235
-11.895644	-7.617870	0.250240
-12.036824	-8.819615	0.255245
-12.695393	0.891161	0.260250
-12.839942	-3.833672	0.265254
-13.490005	-7.325537	0.270259
-13.714876	-21.685774	0.275264
-13.919952	-8.837930	0.280269
-13.752123	-19.353320	0.285274
-13.861087	-9.928105	0.290278
-15.005836	-17.076317	0.295283
-15.002026	-11.072834	0.300288
-15.269050	-5.661353	0.305293
-15.140256	-12.634914	0.310298
-15.247503	-3.573293	0.315302
-15.122683	-18.266939	0.320307
-15.604529	-12.031481	0.325312
-16.446070	-14.261386	0.330317
-16.820614	-17.214696	0.335322
-17.109015	-10.404433	0.340326
-17.010809	-0.754009	0.345331
-16.686881	-15.793270	0.350336
-17.096703	-0.445824	0.355341
-17.749105	-7.078594	0.360346
-17.867626	-1.063966	0.365350
-18.540857	-4.892530	0.370355
-18.162173	-3.840494	0.375360
-18.633723	1.827236	0.380365
-19.240268	-13.243320	0.385370
-19.292928	-9.235784	0.390374
-19.883081	17.643831	0.395379
-19.455388	-3.159135	0.400384
-20.041082	-0.608309	0.405389
-19.850244	-6.051173	0.410394
-20.271015	-11.808163	0.415398
-20.754802	4.420880	0.420403
-21.140793	-9.611771	0.425408
-21.382056	9.506695	0.430413
-21.612704	-4.072901	0.435418
-21.366392	-7.932386	0.440422
-22.388271	6.850352	0.445427
-22.962327	-15.246621	0.450432
-22.768941	-4.104122	0.455437
-22.569819	-16.350008	0.460442
-22.721582	-6.296247	0.465446
-23.011892	-3.289168	0.470451
-23.227456	-18.949917	0.475456
-23.707387	-4.077609	0.480461
-24.246820	-2.577513	0.485466
-24.515804	-14.623720	0.490470
-24.786866	1.403551	0.495475
-24.675680	-10.216693	0.500480
-24.816425	-4.393221	0.505485
-24.843611	-19.167789	0.510490
-25.683448	0.055108	0.515494
-26.145121	-13.363881	0.520499
-26.220175	-8.655314	0.525504
-26.235970	-2.025243	0.530509
-26.141306	-1.715540	0.535514
-26.008909	-8.089435	0.540518
-26.876516	-1.101474	0.545523
-27.169892	-3.983068	0.550528
-27.341917	-13.390137	0.555533
-27.703063	-2.416718	0.560538
-28.044422	-2.250302	0.565542
-29.117895	-18.191973	0.570547
-28.435239	-3.562300	0.575552
-28.809394	-4.507731	0.580557
-29.394756	-4.967446	0.585562
-29.663927	-13.840468	0.590566
-29.599114	-6.967241	0.595571
-29.666436	-11.094607	0.600576
-29.592819	2.570934	0.605581
-29.985713	-12.156520	0.610586
-30.749079	-8.430163	0.615590
-30.929413	3.066685	0.620595
-30.917977	-5.681958	0.625600
-31.000709	1.079130	0.630605
-31.409340	0.296933	0.635610
-31.554745	4.882478	0.640614
-32.869270	4.012153	0.645619
-32.530887	5.688177	0.650624
-32.906100	-9.616224	0.655629
-32.906930	9.165975	0.660634
-32.639674	-14.628839	0.665638
-32.818430	0.869624	0.670643
-32.790751	-13.318291	0.675648
-33.606216	6.420451	0.680653
-33.960794	3.948488	0.685658
-33.973552	-6.164676	0.690662
-34.643039	5.838965	0.695667
-35.102874	5.649316	0.700672
-35.605904	-2.581152	0.705677
-36.031970	0.384638	0.710682
-35.292723	-3.993905	0.715686
-35.978884	10.277018	0.720691
-35.707827	9.472560	0.725696
-36.056047	0.568203	0.730701
-36.064203	0.417352	0.735706
-36.889713	-5.179234	0.740710
-37.643995	5.919037	0.745715
-37.451891	-9.138394	0.750720
-37.741708	11.372299	0.755725
-37.890971	-5.027428	0.760730
-37.793404	3.016746	0.765734
-38.196513	-15.372934	0.770739
-37.570218	-16.688785	0.775744
-38.614401	-4.388550	0.780749
-39.114519	-2.635610	0.785754
-39.398589	-6.804495	0.790758
-39.369554	-3.556718	0.795763
-40.207500	-2.427127	0.800768
-40.748390	1.681121	0.805773
-40.315331	-3.048608	0.810778
-40.451538	-1.844206	0.815782
-40.885689	7.319485	0.820787
-41.148791	-3.372694	0.825792
-41.177688	11.607683	0.830797
-41.520135	-5.387310	0.835802
-41.524652	-5.299841	0.840806
-42.242830	-7.978452	0.845811
-42.542444	-9.354067	0.850816
-42.753165	-8.987976	0.855821
-42.897397	0.864488	0.860826
-42.765538	4.551020	0.865830
-42.904267	3.189163	0.870835
-43.331132	-8.899809	0.875840
-43.872716	-11.393442	0.880845
-44.219971	-8.315595	0.885850
-44.274025	-14.324855	0.890854
-44.460666	-11.142746	0.895859
-44.272250	-18.067462	0.900864
-44.720962	-11.428886	0.905869
-45.088406	-14.498981	0.910874
-45.204168	-2.731669	0.915878
-46.206189	-4.400584	0.920883
-46.482252	-19.403323	0.925888
-47.018325	5.550535	0.930893
-46.851403	-18.651867	0.935898
-47.112061	-15.461670	0.940902
-47.324856	-6.513711	0.945907
-47.192651	-8.467237	0.950912
-47.581373	-6.766936	0.955917
-47.603340	-18.260109	0.960922
-47.356507	-2.838101	0.965926
-47.872945	-6.030656	0.970931
-48.358892	-8.456145	0.975936
-48.477269	-16.684967	0.980941
-49.169376	-9.616909	0.985946
-49.441355	-12.589831	0.990950
-50.341314	-11.672537	0.995955
-50.110432	-15.858356	1.000960
-50.201808	-9.084994	1.005965
-50.445935	-5.054695	1.010970
-50.300226	-17.568550	1.015974
-50.506784	4.937596	1.020979
-50.351560	-16.561940	1.025984
-51.047547	-2.965329	1.030989
-51.666397	-9.755059	1.035994
-51.729435	-19.720220	1.040998
-51.770005	-18.679888	1.046003
-52.388449	-10.745561	1.051008
-53.134870	-16.565229	1.056013
-53.564619	-5.076691	1.061018
-53.390244	-4.480868	1.066022
-53.725401	-18.743167	1.071027
-53.360903	-7.499531	1.076032
-53.734893	-16.917212	1.081037
-53.828102	-0.654869	1.086042
-53.616213	-15.686165	1.091046
-54.450348	-13.832450	1.096051
-55.019741	-11.195437	1.101056
-55.089285	-16.092663	1.106061
-55.323171	-16.067117	1.111066
-55.102367	-11.062580	1.116070
-56.267371	-8.817899	1.121075
-56.637336	-1.002759	1.126080
-56.696992	-6.184736	1.131085
-56.969873	-2.339775	1.136090
-56.808353	-4.954044	1.141094
-57.622722	-2.037623	1.146099
-57.288584	-10.297334	1.151104
-57.405500	-3.159197	1.156109
-57.160538	2.296012	1.161114
-57.311435	-6.487159	1.166118
-58.186184	13.801574	1.171123
-58.699506	-4.603735	1.176128
-58.522450	-0.411025	1.181133
-59.378801	0.638156	1.186138
-59.716019	-15.914961	1.191142
-60.221080	-12.009140	1.196147
-60.583725	-13.353719	1.201152
-59.625299	-11.029670	1.206157
-60.046074	0.304685	1.211162
-60.045859	-9.014148	1.216166
-60.590743	-3.549743	1.221171
-61.401986	-0.230178	1.226176
-61.479511	-10.601147	1.231181
-61.914858	-6.251791	1.236186
-61.883339	-9.970029	1.241190
-62.201754	-0.375052	1.246195
-61.645039	-8.214520	1.251200
-62.219344	-4.487640	1.256205
-63.037412	3.435689	1.261210
-63.282916	-7.030533	1.266214
-63.814461	-3.553094	1.271219
-63.414605	-4.384658	1.276224
-63.448273	-11.562495	1.281229
-64.012802	0.362733	1.286234
-64.506151	4.113426	1.291238
-64.936889	-4.578909	1.296243
-64.967018	-3.380890	1.301248
-65.101399	-1.399062	1.306253
-65.215645	-1.171631	1.311258
-65.241825	-4.360765	1.316262
-65.627180	-3.226262	1.321267
-66.390940	-20.061147	1.326272
-66.762210	-15.345949	1.331277
-67.060355	-6.421174	1.336282
-66.569387	-17.850651	1.341286
-67.053295	-7.309934	1.346291
-66.875960	-7.386184	1.351296
-67.520216	-20.315488	1.356301
-68.420363	-1.716332	1.361306
-68.134494	-18.013841	1.366310
-68.568830	-11.976917	1.371315
-68.454323	-13.974078	1.376320
-68.398553	-17.700070	1.381325
-68.939608	-7.455119	1.386330
-69.705918	-15.930208	1.391334
-69.925785	-9.961873	1.396339
-70.170815	-8.992020	1.401344
-70.073579	-11.017401	1.406349
-70.279940	-9.219589	1.411354
-69.981250	-9.488724	1.416358
-71.088171	0.741536	1.421363
-71.136264	-7.257516	1.426368
-71.349073	6.868686	1.431373
-71.547300	-0.461200	1.436378
-71.683175	1.557275	1.441382
-71.616781	-6.129346	1.446387
-72.376092	2.282732	1.451392
-72.936942	-7.294458	1.456397
-73.286996	-3.716306	1.461402
-73.342139	-7.741513	1.466406
-73.403931	2.142308	1.471411
-73.657902	-12.401925	1.476416
-73.286288	-2.104198	1.481421
-74.196356	5.380071	1.486426
-74.740450	-8.171878	1.491430
-74.844379	16.361761	1.496435
-74.832545	-7.365491	1.501440
-75.070751	-5.224355	1.506445
-75.061332	-4.209252	1.511450
-75.404672	-3.132101	1.516454
-75.989282	-9.594653	1.521459
-76.782426	-1.320713	1.526464
-76.754581	-11.613210	1.531469
-76.666987	8.950614	1.536474
-76.474337	-8.596044	1.541478
-76.641945	-4.171080	1.546483
-77.272414	-5.349371	1.551488
-77.820787	-5.695338	1.556493
-78.292997	-14.108055	1.561498
-78.122791	-3.400610	1.566502
-78.308065	3.836720	1.571507
-78.113937	-11.479491	1.576512
-78.922559	-6.890685	1.581517
-79.573099	-19.810168	1.586522
-79.510362	-6.945726	1.591526
-79.868829	-10.086355	1.596531
-79.877033	-1.216400	1.601536
-79.843551	-0.247691	1.606541
-80.139176	10.323674	1.611546
-80.661222	-3.703648	1.616550
-81.413970	-3.577455	1.621555
-81.430029	-1.332955	1.626560
-81.537310	-2.060090	1.631565
-81.608305	-8.893204	1.636570
-81.380569	-4.862662	1.641574
-81.576327	-2.498498	1.646579
-82.414995	-16.564432	1.651584
-82.615965	-2.149191	1.656589
-83.057735	-12.260989	1.661594
-83.005653	-2.102125	1.666598
-83.056368	-1.330209	1.671603
-83.795414	3.923421	1.676608
-84.195203	-6.227083	1.681613
-84.449681	-11.990931	1.686618
-84.381601	5.870841	1.691622
-84.759863	-0.162179	1.696627
-84.819870	2.550854	1.701632
-84.540563	-7.358926	1.706637
-85.578601	3.737706	1.711642
-85.914167	-3.736586	1.716646
-86.040610	12.436953	1.721651
-86.034163	-1.851034	1.726656
-86.324791	-6.499633	1.731661
-86.504443	-2.338036	1.736666
-87.127058	-4.180329	1.741670
-87.706926	-7.225278	1.746675
-87.932570	-5.562581	1.751680
-88.109679	10.718468	1.756685
-88.434728	-10.127179	1.761690
-87.743817	-0.387785	1.766694
-88.243018	-0.442487	1.771699
-88.569411	-9.029344	1.776704
-88.422825	-10.143400	1.781709
-88.996324	-3.026677	1.786714
-89.270430	-6.190126	1.791718
-89.844532	-6.142484	1.796723
-90.003658	0.464415	1.801728
-89.684058	-4.071467	1.806733
-90.605411	12.979210	1.811738
-91.126832	-1.944711	1.816742
-91.125760	9.799055	1.821747
-91.269663	-5.699525	1.826752
-91.208160	-2.151806	1.831757
-91.424022	8.650722	1.836762
-91.296785	-3.394872	1.841766
-92.422064	11.866130	1.846771
-92.694420	-3.842350	1.851776
-92.980114	-0.618615	1.856781
-93.255337	9.417772	1.861786
-92.919015	-2.895380	1.866790
-92.912994	-10.148729	1.871795
-93.438602	-4.025199	1.876800
-94.175982	-1.545282	1.881805
-94.744249	3.742271	1.886810
-94.916735	-6.452110	1.891814
-94.706212	-2.559590	1.896819
-94.726745	-10.143158	1.901824
-94.461998	-8.557858	1.906829
-95.069786	-0.241651	1.911834
-95.856881	-10.259088	1.916838
-96.066011	-12.840608	1.921843
-96.317767	-5.135268	1.926848
-96.022164	-9.421159	1.931853
-96.571033	-8.602821	1.936858
-97.009682	-1.348380	1.941862
-97.666214	-2.846809	1.946867
-97.849250	-2.162029	1.951872
-97.582917	2.762282	1.956877
-97.921652	5.556894	1.961882
-97.672798	-12.221591	1.966886
-97.847570	-3.937690	1.971891
-98.707923	-1.311576	1.976896
-99.012226	-5.009135	1.981901
-99.491931	-1.973712	1.986906
-99.281554	-2.020208	1.991910
-99.575445	-0.413310	1.996915
-99.849328	-8.720716	2.006912
-99.674171	-3.987920	2.016909
-99.749519	-3.782047	2.026906
-98.793452	4.218378	2.036902
-98.059262	-4.339887	2.046899
-97.675887	-3.277119	2.056896
-97.184206	-8.648115	2.066893
-96.879027	-11.589400	2.076890
-95.930447	-10.770277	2.086886
-95.312346	-9.078403	2.096883
-95.341979	-8.741705	2.106880
-95.008145	-12.559788	2.116877
-93.895543	-17.185636	2.126874
-93.722795	-13.270081	2.136870
-92.967805	-5.340041	2.146867
-92.199373	-5.616459	2.156864
-92.151764	-8.460950	2.166861
-91.944400	-5.181678	2.176858
-91.326811	-2.371515	2.186854
-90.568111	-3.884239	2.196851
-90.300570	-4.468717	2.206848
-89.720292	-3.005275	2.216845
-89.364167	-3.802234	2.226842
-88.385546	-4.939720	2.236838
-87.729529	-4.047254	2.246835
-87.443972	-9.854241	2.256832
-87.826994	-12.343986	2.266829
-86.725212	-6.262595	2.276826
-85.929382	-10.269829	2.286822
-85.833657	-7.657489	2.296819
-84.867207	-16.230229	2.306816
-84.205139	-12.011911	2.316813
-84.478965	-2.776547	2.326810
-83.731512	-6.389685	2.336806
-82.818376	-7.727819	2.346803
-82.827411	-0.544555	2.356800
-82.400382	-1.604608	2.366797
-81.584612	-13.725937	2.376794
-80.943756	-9.651382	2.386790
-80.133356	-7.548391	2.396787
-79.656523	-11.136953	2.406784
-79.521086	-17.513738	2.416781
-79.561935	-13.301629	2.426778
-78.806154	-8.073440	2.436774
-78.423524	-16.689555	2.446771
-77.383559	-9.289114	2.456768
-76.841695	-7.448234	2.466765
-76.831663	-7.724554	2.476762
-76.198617	-11.301103	2.486758
-75.181426	-14.151353	2.496755
-75.133879	-14.656111	2.506752
-74.984500	-10.487490	2.516749
-73.797056	-9.650848	2.526746
-73.370627	-8.168497	2.536742
-73.461403	-7.954840	2.546739
-72.568636	-12.890355	2.556736
-72.109107	-15.177494	2.566733
-71.708415	-10.518320	2.576730
-70.584263	-11.623652	2.586726
-70.325351	-13.161635	2.596723
-70.533868	-8.555270	2.606720
-69.857263	-6.127033	2.616717
-68.969657	-2.575461	2.626714
-68.803234	-7.590360	2.636710
-67.623374	-6.711669	2.646707
-67.345423	-16.297321	2.656704
-67.105988	-5.269217	2.666701
-66.977457	-4.687725	2.676698
-66.046079	-10.179291	2.686694
-65.715535	-0.929526	2.696691
-64.710495	-6.706175	2.706688
-64.219372	-8.531738	2.716685
-64.017535	-8.661374	2.726682
-64.207084	-5.937586	2.736678
-62.855456	-5.211735	2.746675
-62.340793	-8.148131	2.756672
-62.251257	-16.930046	2.766669
-61.448316	-11.707773	2.776666
-60.709771	-13.828761	2.786662
-60.662814	-3.197221	2.796659
-60.371303	-5.803483	2.806656
-59.574668	-5.408064	2.816653
-59.140996	8.504110	2.826650
-58.370614	3.583878	2.836646
-57.686022	1.021105	2.846643
-57.354181	-2.226238	2.856640
-57.454427	-11.347684	2.866637
-56.566060	-5.012728	2.876634
-55.812438	-2.115503	2.886630
-55.526381	-1.883624	2.896627
-55.154919	-1.820141	2.906624
-54.226207	-8.932122	2.916621
-54.206728	0.470591	2.926618
-53.717847	-1.751173	2.936614
-52.727904	-2.140545	2.946611
-52.350531	-13.582071	2.956608
-52.230027	-8.498586	2.966605
-51.890684	-9.022233	2.976602
-50.864646	-11.303333	2.986598
-50.762768	-13.185069	2.996595
-49.785613	-10.808081	3.006592
-49.362000	-11.686517	3.016589
-49.256541	-9.396893	3.026586
-48.386459	-1.203966	3.036582
-47.726368	-3.691473	3.046579
-47.694491	1.323594	3.056576
-47.364641	-5.275858	3.066573
-46.742502	6.238680	3.076570
-46.192808	2.759862	3.086566
-45.080470	-2.585005	3.096563
-44.959925	-3.954333	3.106560
-44.653782	-1.177540	3.116557
-43.624248	-11.569725	3.126554
-43.303928	-5.636827	3.136550
-43.245027	-12.135199	3.146547
-42.684011	-9.717982	3.156544
-41.732783	-5.416569	3.166541
-41.420859	-3.073849	3.176538
-41.435834	-11.845312	3.186534
-40.415232	-2.275973	3.196531
-40.053115	-1.760345	3.206528
-39.808498	-3.642855	3.216525
-38.642039	-8.068893	3.226522
-38.316831	-14.007083	3.236518
-38.319245	-8.220964	3.246515
-37.210039	-8.103387	3.256512
-36.644712	-2.270932	3.266509
-36.694044	-4.416195	3.276506
-36.335254	-6.524995	3.286502
-35.138785	-14.154541	3.296499
-34.658104	2.208312	3.306496
-34.739075	1.611302	3.316493
-34.301135	2.114993	3.326490
-33.642593	3.975711	3.336486
-32.676333	3.813877	3.346483
-31.903039	-6.940042	3.356480
-32.005723	-4.714101	3.366477
-31.603907	-4.492855	3.376474
-31.315362	7.066248	3.386470
-30.083234	4.647971	3.396467
-30.000440	0.984468	3.406464
-29.738560	-6.877227	3.416461
-28.674644	-0.441488	3.426458
-28.230788	5.200265	3.436454
-27.985650	-2.567103	3.446451
-27.796108	-4.800241	3.456448
-26.659553	-3.465366	3.466445
-26.800173	-1.673581	3.476442
-25.755411	10.774356	3.486438
-24.879988	3.379008	3.496435
-24.827716	3.732790	3.506432
-24.972782	1.380417	3.516429
-24.042904	6.185352	3.526426
-23.443526	1.125075	3.536422
-23.037197	2.216354	3.546419
-22.417254	-3.283106	3.556416
-21.851762	0.775568	3.566413
-21.616716	-3.524300	3.576410
-20.848442	-0.836914	3.586406
-20.339254	-8.407305	3.596403
-20.212382	-3.979139	3.606400
-19.181487	-7.893550	3.616397
-18.622989	-5.700523	3.626394
-18.495706	-1.892912	3.636390
-18.471702	-5.737824	3.646387
-17.249253	0.888229	3.656384
-17.069814	-9.376608	3.666381
-16.470556	-1.100297	3.676378
-15.331520	-12.049282	3.686374
-15.204864	-3.448631	3.696371
-15.022988	-2.686113	3.706368
-14.987119	-2.750590	3.716365
-13.904068	0.749039	3.726362
-13.742001	-1.426814	3.736358
-12.779140	4.050943	3.746355
-12.651739	-1.273287	3.756352
-11.811154	-3.459138	3.766349
-10.979868	-5.308021	3.776346
-10.736013	-2.453668	3.786342
-10.661628	0.558282	3.796339
-10.188428	-1.074278	3.806336
-9.151380	-5.260442	3.816333
-9.136430	3.655090	3.826330
-8.399024	-4.079447	3.836326
-7.507377	-0.406843	3.846323
-7.379165	5.845732	3.856320
-7.367984	5.431236	3.866317
-6.018994	6.676882	3.876314
-5.749023	1.649015	3.886310
-5.472058	4.902570	3.896307
-5.396922	-5.058495	3.906304
-4.533955	5.935331	3.916301
-3.925732	19.253308	3.926298
-2.962388	19.924713	3.936294
-3.086213	25.996314	3.946291
-2.867755	35.668219	3.956288
-2.401360	35.739722	3.966285
-2.234515	51.299521	3.976282
-1.300088	68.918534	3.986278
-0.610406	85.228376	3.996275
-0.412460	95.584651	4.006272
0.156481	105.407340	4.016269
0.000000	118.605048	4.021274
0.579019	130.004029	4.026278
0.756396	135.082284	4.031283
0.949007	149.676987	4.036288
1.115544	157.757298	4.041293
0.976774	152.889113	4.046298
1.393777	163.374785	4.051302
1.090975	160.003057	4.056307
1.278217	156.526968	4.061312
1.196930	158.838995	4.066317
1.373528	150.078059	4.071322
1.024240	163.131588	4.076326
1.534279	186.053273	4.081331
1.640798	182.165347	4.086336
1.486373	181.522050	4.091341
1.081866	174.056092	4.096346
1.553199	197.139559	4.101350
1.464848	184.268537	4.106355
1.627491	208.156305	4.111360
1.901712	194.017024	4.116365
1.523022	191.854128	4.121370
1.438799	168.254621	4.126374
1.551432	169.484304	4.131379
1.224555	174.786574	4.136384
1.858360	171.573665	4.141389
1.428443	187.586446	4.146394
1.783691	172.437356	4.151398
1.484127	175.024281	4.156403
1.313098	180.045005	4.161408
1.529393	194.548041	4.166413
1.700845	188.791258	4.171418
1.508429	184.029195	4.176422
1.761144	186.174558	4.181427
1.569608	202.451697	4.186432
1.695045	198.343222	4.191437
1.569424	186.333632	4.196442
1.868688	194.331460	4.201446
1.838882	194.062651	4.206451
1.905078	188.313398	4.211456
1.760799	187.954895	4.216461
1.787846	190.069978	4.221466
1.885119	203.069179	4.226470
1.852599	188.056265	4.231475
1.721909	189.161517	4.236480
1.865735	199.694726	4.241485
1.736789	205.188128	4.246490
1.795654	204.153957	4.251494
1.977604	186.965837	4.256499
1.648741	198.791214	4.261504
1.985072	199.521966	4.266509
1.891938	196.134324	4.271514
1.894131	199.154168	4.276518
1.873123	202.174394	4.281523
1.610709	194.173951	4.286528
2.059307	201.212418	4.291533
2.012180	194.270596	4.296538
2.033223	205.802387	4.301542
2.056286	197.973664	4.306547
1.669951	205.797337	4.311552
1.782739	191.772334	4.316557
1.945185	193.268521	4.321562
2.053185	194.169292	4.326566
1.927649	197.689966	4.331571
1.883561	210.751993	4.336576
2.068114	187.382478	4.341581
2.005204	184.859421	4.346586
1.900047	195.214775	4.351590
2.212094	195.988210	4.356595
1.899652	197.633210	4.361600
2.122382	189.605077	4.366605
1.652083	201.925562	4.371610
1.924753	195.249819	4.376614
2.489711	198.242165	4.381619
2.082925	218.833732	4.386624
2.184851	190.586421	4.391629
2.045640	208.755463	4.396634
1.823077	219.950392	4.401638
2.116869	219.939044	4.406643
1.944602	241.534099	4.411648
2.207810	223.627572	4.416653
2.334475	236.834727	4.421658
2.447110	229.753141	4.426662
3.041543	212.058537	4.431667
2.442436	241.212178	4.436672
2.659156	200.744821	4.441677
2.326011	205.633817	4.446682
2.369660	194.417982	4.451686
2.344841	194.902214	4.456691
2.434601	186.686825	4.461696
2.459568	195.150023	4.466701
2.281139	190.286406	4.471706
2.381269	194.163687	4.476710
2.131498	197.365446	4.481715
2.411305	211.195484	4.486720
2.523154	205.304224	4.491725
2.502651	215.867559	4.496730
2.325348	217.928521	4.501734
2.320674	219.209161	4.506739
2.449049	233.340063	4.511744
2.459237	224.247113	4.516749
2.447665	232.144015	4.521754
2.514046	225.475518	4.526758
2.495978	221.484565	4.531763
2.173293	234.812932	4.536768
2.683887	225.578986	4.541773
2.535959	241.295546	4.546778
2.461862	226.321822	4.551782
2.461951	238.281877	4.556787
2.631999	244.241417	4.561792
2.582371	229.582772	4.566797
2.768041	234.244283	4.571802
2.685125	237.745198	4.576806
2.613912	231.502708	4.581811
2.266814	235.481527	4.586816
2.445193	237.126806	4.591821
2.379537	239.724214	4.596826
2.275480	232.751929	4.601830
2.467776	241.433923	4.606835
2.638343	264.503863	4.611840
3.025401	258.366847	4.616845
3.253003	256.381345	4.621850
2.606700	265.641904	4.626854
2.727991	232.982046	4.631859
2.432962	260.334672	4.636864
2.947242	253.186801	4.641869
2.986373	262.879709	4.646874
2.887607	263.230953	4.651878
3.100194	257.788742	4.656883
2.553400	258.174861	4.661888
2.919392	247.524143	4.666893
2.786386	264.280377	4.671898
3.132231	274.247652	4.676902
3.187013	258.948763	4.681907
2.816479	258.805411	4.686912
2.982602	247.702572	4.691917
2.797815	244.482378	4.696922
2.702687	260.733979	4.701926
2.923333	250.750858	4.706931
3.142788	275.489947	4.711936
2.931011	261.711176	4.716941
2.857652	270.545501	4.721946
2.744848	268.837716	4.726950
3.251389	255.839717	4.731955
3.154157	258.341134	4.736960
3.006373	254.024171	4.741965
3.044634	254.808129	4.746970
3.109572	261.830516	4.751974
3.249433	255.683844	4.756979
2.781467	270.538066	4.761984
2.592433	263.208203	4.766989
3.033923	261.845139	4.771994
2.983261	258.021938	4.776998
2.941509	253.161955	4.782003
2.817626	269.518150	4.787008
2.983576	253.883445	4.792013
3.426237	267.366411	4.797018
3.119154	266.002163	4.802022
3.243834	259.207316	4.807027
3.161326	291.810832	4.812032
3.251691	276.926679	4.817037
3.168292	292.983027	4.822042
3.599246	298.958365	4.827046
3.415281	273.079142	4.832051
3.029954	282.247359	4.837056
3.267913	271.919645	4.842061
3.199255	293.763902	4.847066
3.250785	299.690667	4.852070
3.486619	296.418512	4.857075
3.389867	301.387541	4.862080
3.404544	295.718676	4.867085
3.530894	284.476877	4.872090
3.558831	292.273664	4.877094
3.614890	280.472902	4.882099
3.376186	269.780439	4.887104
3.551610	269.831761	4.892109
3.360899	253.856076	4.897114
3.260321	251.200436	4.902118
3.563985	274.585477	4.907123
3.649392	279.358865	4.912128
3.576869	278.937008	4.917133
3.439849	273.970242	4.922138
3.769565	287.285347	4.927142
3.869503	266.206691	4.932147
3.318829	269.271646	4.937152
3.061709	263.154469	4.942157
3.105542	279.144102	4.947162
3.352642	293.635926	4.952166
3.709595	303.073913	4.957171
3.628553	296.704975	4.962176
3.575006	303.643677	4.967181
3.754786	299.332943	4.972186
3.683119	297.614213	4.977190
3.555027	302.769540	4.982195
3.361917	302.891629	4.987200
3.507984	288.940450	4.992205
3.782156	298.527163	4.997210
3.793695	290.902920	5.002214
3.984621	289.199097	5.007219
3.425367	296.315871	5.012224
3.603654	287.875283	5.017229
3.955273	299.643824	5.022234
3.583551	304.494637	5.027238
3.997705	296.615932	5.032243
3.465084	305.884956	5.037248
3.736983	291.750210	5.042253
3.635534	288.815632	5.047258
3.855118	301.216724	5.052262
4.045417	296.627938	5.057267
3.898512	282.030302	5.062272
3.807807	289.342207	5.067277
3.606983	303.709385	5.072282
3.581259	305.563994	5.077286
3.860551	300.362396	5.082291
3.917860	311.276458	5.087296
4.374633	314.884909	5.092301
4.198243	309.167807	5.097306
3.861117	295.476110	5.102310
4.091196	280.790330	5.107315
3.342905	298.524769	5.112320
3.771982	310.218566	5.117325
3.971160	324.455145	5.122330
3.840248	330.367877	5.127334
4.216487	318.576619	5.132339
3.824756	343.196636	5.137344
4.273585	335.194100	5.142349
3.924314	322.644958	5.147354
3.893261	339.925513	5.152358
4.291333	328.291240	5.157363
4.192625	333.027694	5.162368
4.071268	340.441562	5.167373
3.993547	328.400663	5.172378
4.086422	336.559041	5.177382
4.063688	325.254248	5.182387
3.858462	334.146408	5.187392
4.037437	338.725503	5.192397
3.944740	335.633111	5.197402
3.971686	332.148847	5.202406
4.071101	336.470398	5.207411
3.855484	333.940590	5.212416
4.217971	358.326198	5.217421
4.328477	366.616630	5.222426
4.263317	367.821947	5.227430
4.653743	373.844162	5.232435
4.481215	369.945382	5.237440
4.425574	359.603684	5.242445
4.624717	334.584891	5.247450
4.024224	348.574732	5.252454
4.647533	338.267934	5.257459
4.276119	326.672137	5.262464
4.269294	338.561302	5.267469
4.538524	333.907178	5.272474
4.385410	341.180097	5.277478
4.555675	321.884751	5.282483
4.197738	346.435462	5.287488
4.091192	320.542871	5.292493
4.550975	348.675130	5.297498
4.830787	350.996862	5.302502
4.768360	341.669911	5.307507
4.272594	352.619664	5.312512
4.199454	340.348936	5.317517
4.733794	348.514272	5.322522
4.178668	356.724009	5.327526
5.082440	355.155116	5.332531
4.432791	357.651853	5.337536
4.613293	344.897952	5.342541
4.429742	338.844940	5.347546
4.599553	370.732862	5.352550
4.728182	349.966209	5.357555
4.541745	354.996343	5.362560
4.552916	353.042353	5.367565
4.659614	347.609125	5.372570
4.802540	356.313647	5.377574
4.904871	356.217534	5.382579
4.737231	349.066890	5.387584
4.506117	340.295388	5.392589
4.814878	338.704276	5.397594
4.561703	348.336932	5.402598
4.819752	341.449080	5.407603
4.817141	368.047450	5.412608
4.767501	346.374973	5.417613
4.797369	341.020933	5.422618
4.497654	355.654083	5.427622
4.730246	351.542262	5.432627
4.906309	365.008998	5.437632
4.875825	358.416428	5.442637
5.196623	360.959662	5.447642
4.789747	349.082246	5.452646
4.709505	349.169012	5.457651
4.667529	343.050480	5.462656
4.795324	367.011534	5.467661
5.009232	358.291764	5.472666
4.758421	377.127471	5.477670
4.440922	363.097754	5.482675
4.383087	368.224328	5.487680
5.039131	368.403980	5.492685
4.929915	359.659280	5.497690
4.871075	382.928107	5.502694
5.070579	360.238014	5.507699
4.919155	368.146950	5.512704
4.749927	369.793555	5.517709
5.112731	372.287430	5.522714
4.871867	360.071730	5.527718
4.883984	366.591598	5.532723
4.815104	361.608314	5.537728
4.820944	372.205581	5.542733
5.254681	378.124064	5.547738
5.468170	381.226320	5.552742
5.101127	376.107337	5.557747
4.880204	369.471162	5.562752
5.030631	379.914127	5.567757
5.121368	377.252103	5.572762
5.204585	407.075094	5.577766
5.446328	387.502290	5.582771
5.206686	393.886897	5.587776
5.237245	373.104062	5.592781
5.144290	378.710450	5.597786
4.842850	373.905083	5.602790
5.039986	389.959664	5.607795
4.962814	389.229899	5.612800
5.235718	408.411378	5.617805
5.257120	397.347537	5.622810
5.316465	407.413247	5.627814
5.468016	404.969738	5.632819
5.460345	400.244750	5.637824
5.407190	400.517728	5.642829
5.614331	399.176215	5.647834
5.441225	422.037427	5.652838
5.643903	399.654733	5.657843
5.225122	398.462133	5.662848
5.175681	381.921288	5.667853
5.366236	404.112135	5.672858
5.599444	402.904521	5.677862
5.456301	404.975547	5.682867
5.735707	389.697905	5.687872
5.202751	384.766543	5.692877
5.503559	400.339564	5.697882
5.399294	404.546227	5.702886
5.240312	403.771779	5.707891
5.172390	411.078005	5.712896
5.330938	406.341922	5.717901
5.834223	395.411236	5.722906
5.550622	408.638197	5.727910
5.732877	403.455363	5.732915
5.381336	409.044713	5.737920
5.530327	395.458547	5.742925
5.648530	408.386790	5.747930
5.282232	413.323551	5.752934
5.603788	385.956429	5.757939
5.825019	407.689414	5.762944
5.560385	404.001960	5.767949
5.586291	392.187056	5.772954
5.560530	393.139637	5.777958
5.497628	398.912123	5.782963
5.348348	395.900393	5.787968
5.513231	395.308196	5.792973
5.619283	395.966131	5.797978
5.453219	394.735025	5.802982
5.665946	396.755331	5.807987
5.480712	393.889525	5.812992
5.424126	404.155214	5.817997
5.536840	426.997709	5.823002
5.619543	436.187816	5.828006
5.772869	428.178031	5.833011
5.939883	431.388698	5.838016
6.052695	437.784824	5.843021
6.062888	440.188612	5.848026
5.834382	443.761478	5.853030
5.786213	442.232004	5.858035
5.601238	433.859850	5.863040
5.666098	435.889207	5.868045
5.752267	429.602477	5.873050
5.515595	443.311012	5.878054
5.508545	422.624490	5.883059
5.367830	435.399528	5.888064
5.435674	450.804133	5.893069
6.085334	448.518119	5.898074
5.862162	463.504709	5.903078
6.305444	466.149946	5.908083
6.098328	462.880815	5.913088
6.255125	461.437425	5.918093
5.924313	442.008396	5.923098
5.897956	440.347270	5.928102
6.217167	438.905848	5.933107
5.946464	451.444512	5.938112
6.040426	455.400318	5.943117
6.561441	445.414192	5.948122
6.233098	452.284334	5.953126
6.261379	426.004677	5.958131
5.930861	433.296006	5.963136
6.180647	450.754309	5.968141
6.285224	422.647792	5.973146
6.027573	436.503026	5.978150
6.239048	426.997879	5.983155
6.325772	434.890283	5.988160
5.759657	430.021010	5.993165
6.390823	432.427438	5.998170
6.031783	436.591867	6.003174
6.368608	440.742222	6.008179
6.217528	440.457246	6.013184
6.034054	439.716536	6.018189
6.557992	432.651627	6.023194
6.092241	450.210417	6.028198
6.038049	461.961207	6.033203
6.248020	467.838277	6.038208
6.323930	482.207736	6.043213
6.429498	471.136247	6.048218
6.379215	478.244067	6.053222
6.519115	454.144121	6.058227
6.155889	448.671220	6.063232
6.114065	438.806422	6.068237
6.068277	444.535947	6.073242
6.505350	454.670865	6.078246
6.511160	444.221094	6.083251
6.033486	453.639458	6.088256
6.306920	442.298855	6.093261
6.020812	431.838045	6.098266
6.302889	446.710347	6.103270
6.404122	456.589230	6.108275
6.371062	469.878520	6.113280
6.233738	455.782346	6.118285
6.478879	449.597975	6.123290
6.137603	438.673254	6.128294
6.239519	440.484492	6.133299
6.213257	442.195474	6.138304
6.425635	446.663823	6.143309
6.342521	433.203382	6.148314
6.041605	453.169300	6.153318
6.094370	452.112050	6.158323
6.156558	466.499642	6.163328
6.228764	473.378280	6.168333
6.312122	460.803599	6.173338
6.239803	477.328768	6.178342
6.563573	474.412669	6.183347
6.533572	462.614051	6.188352
6.580367	465.169535	6.193357
6.639036	439.506818	6.198362
6.013918	451.807609	6.203366
6.245321	437.676462	6.208371
5.852683	429.149221	6.213376
6.107970	440.190272	6.218381
6.506021	433.068529	6.223386
6.078829	435.668598	6.228390
6.419241	421.278747	6.233395
6.250643	432.196390	6.238400
6.227255	417.408339	6.243405
6.660081	435.258396	6.248410
6.569552	430.795490	6.253414
6.526617	437.634836	6.258419
6.211322	441.993578	6.263424
6.150974	443.897035	6.268429
6.115188	429.996594	6.273434
6.009304	440.491132	6.278438
6.328783	435.127969	6.283443
6.073989	426.757590	6.288448
5.935614	430.234469	6.293453
6.389398	431.986769	6.298458
5.999886	436.621759	6.303462
6.480889	453.381005	6.308467
6.479792	449.243062	6.313472
5.978219	448.530948	6.318477
6.251029	443.887543	6.323482
6.106691	466.944225	6.328486
6.425294	453.960546	6.333491
6.568954	463.153813	6.338496
5.904272	457.101542	6.343501
6.600693	461.947044	6.348506
6.471289	462.375764	6.353510
6.680324	447.939434	6.358515
6.346255	439.517238	6.363520
6.221804	442.668743	6.368525
6.494315	444.231900	6.373530
6.423704	441.549571	6.378534
6.516317	434.127309	6.383539
6.141629	433.239348	6.388544
6.163986	437.985719	6.393549
6.602295	435.383344	6.398554
6.600993	438.585130	6.403558
6.571145	433.586297	6.408563
6.787219	440.123691	6.413568
6.772628	427.986555	6.418573
6.339622	409.673207	6.423578
6.221725	402.895299	6.428582
6.268842	407.519288	6.433587
6.261596	397.356210	6.438592
6.024408	412.485741	6.443597
6.147322	405.812361	6.448602
5.968969	409.778925	6.453606
6.135076	426.187987	6.458611
6.456580	437.251535	6.463616
6.217819	440.063241	6.468621
6.306373	430.162008	6.473626
6.129510	444.973619	6.478630
6.613316	413.383791	6.483635
6.183631	439.894726	6.488640
6.362531	423.817634	6.493645
6.227237	406.326163	6.498650
6.250482	411.964855	6.503654
6.268518	418.466406	6.508659
6.354108	422.643081	6.513664
6.336165	416.542941	6.518669
6.320336	406.921872	6.523674
6.114702	410.036770	6.528678
6.386189	399.408766	6.533683
6.192264	392.131834	6.538688
6.105249	408.873326	6.543693
6.443786	421.293923	6.548698
6.086941	425.009430	6.553702
6.159626	422.853887	6.558707
6.764200	434.870068	6.563712
6.011073	403.031771	6.568717
6.037284	402.898321	6.573722
5.826401	430.904903	6.578726
6.238415	436.820093	6.583731
6.258132	443.011124	6.588736
6.098158	446.615381	6.593741
6.426808	437.263500	6.598746
6.079765	429.323973	6.603750
6.258909	443.236853	6.608755
6.354101	433.506367	6.613760
6.413122	436.073538	6.618765
6.611719	438.410283	6.623770
6.369391	435.121427	6.628774
6.311499	430.426333	6.633779
6.589986	442.429425	6.638784
6.416458	425.342694	6.643789
6.296319	417.806441	6.648794
6.027131	413.348500	6.653798
6.316084	413.968122	6.658803
6.501147	416.676244	6.663808
6.333474	414.687778	6.668813
6.318990	394.397908	6.673818
6.202835	399.043056	6.678822
6.034669	410.902906	6.683827
6.364774	419.800367	6.688832
6.329795	420.337681	6.693837
6.596636	404.284944	6.698842
6.303407	403.974430	6.703846
6.578177	405.630631	6.708851
6.449414	402.850984	6.713856
6.030403	416.067873	6.718861
6.360015	406.216491	6.723866
6.305179	400.407056	6.728870
5.998071	403.868506	6.733875
6.056338	396.392847	6.738880
5.869260	403.031473	6.743885
5.893235	413.316606	6.748890
6.199058	429.282437	6.753894
6.301354	434.354850	6.758899
6.621225	428.716986	6.763904
6.306779	439.460550	6.768909
6.595785	419.546658	6.773914
6.178361	423.326038	6.778918
6.304068	400.596783	6.783923
6.435312	418.695041	6.788928
6.285021	411.781809	6.793933
6.384759	405.387884	6.798938
6.059645	407.367841	6.803942
6.153014	409.985068	6.808947
6.349338	394.033963	6.813952
6.244917	404.549542	6.818957
6.347309	407.877029	6.823962
6.055341	423.872883	6.828966
5.960263	413.201174	6.833971
6.323602	438.536660	6.838976
6.239881	444.215040	6.843981
6.190116	432.320471	6.848986
6.129419	453.607063	6.853990
5.988593	437.786700	6.858995
6.186533	435.365411	6.864000
6.068421	447.768467	6.869005
6.488854	434.218893	6.874010
6.177604	451.944914	6.879014
6.118278	443.989598	6.884019
6.275494	452.137109	6.889024
6.153381	435.128584	6.894029
6.432887	445.267831	6.899034
6.115681	446.770405	6.904038
6.367161	441.527583	6.909043
6.465000	447.919874	6.914048
6.091115	447.732287	6.919053
6.311036	444.924902	6.924058
6.338482	452.827604	6.929062
6.455351	439.334899	6.934067
6.682843	447.427388	6.939072
6.247886	446.453203	6.944077
6.610026	437.493936	6.949082
6.582658	452.385714	6.954086
6.424874	418.793964	6.959091
6.254162	424.924220	6.964096
6.106811	416.433497	6.969101
6.046594	411.426668	6.974106
6.246812	422.492196	6.979110
5.947473	429.842690	6.984115
6.353770	441.864317	6.989120
6.276996	443.406868	6.994125
6.435011	444.273049	6.999130
6.304336	451.101745	7.004134
6.237042	446.591491	7.009139
6.382935	437.699033	7.014144
6.172478	444.925544	7.019149
6.597725	438.463312	7.024154
6.437503	422.307902	7.029158
6.183611	419.283761	7.034163
6.278203	408.542041	7.039168
6.243776	415.914254	7.044173
6.493538	409.118893	7.049178
6.163320	413.079184	7.054182
6.328110	396.968741	7.059187
6.373497	421.471171	7.064192
6.259218	413.365733	7.069197
6.195679	404.443881	7.074202
6.114101	410.390220	7.079206
5.894714	408.137338	7.084211
6.502287	419.123807	7.089216
6.259007	413.761906	7.094221
6.338571	404.379292	7.099226
6.035095	401.378640	7.104230
6.402404	414.946598	7.109235
6.273450	399.355250	7.114240
6.217634	410.690465	7.119245
6.383910	411.822519	7.124250
6.046993	424.015881	7.129254
6.121026	423.651186	7.134259
6.255327	440.632456	7.139264
6.183491	441.724646	7.144269
6.195702	444.267591	7.149274
6.172559	438.696174	7.154278
6.073502	433.733143	7.159283
6.473940	439.931792	7.164288
6.182503	442.338864	7.169293
6.769473	433.409526	7.174298
6.340788	426.447393	7.179302
6.503534	433.567537	7.184307
6.442272	402.978829	7.189312
6.311451	410.030478	7.194317
6.090963	400.816915	7.199322
6.074599	413.737214	7.204326
6.289397	408.463964	7.209331
6.543232	412.117419	7.214336
6.442521	409.021305	7.219341
6.734374	397.258138	7.224346
6.284952	404.137909	7.229350
6.360716	398.275917	7.234355
6.417173	398.016821	7.239360
6.182960	405.443057	7.244365
6.738666	405.852077	7.249370
6.344958	406.296950	7.254374
6.472095	400.255904	7.259379
6.588987	399.511925	7.264384
6.455937	420.806679	7.269389
6.606568	412.405021	7.274394
6.322681	411.682486	7.279398
6.361662	382.293496	7.284403
6.435758	384.711477	7.289408
6.072329	384.982064	7.294413
5.998997	377.474398	7.299418
6.497306	410.837469	7.304422
6.109588	406.681846	7.309427
6.387357	398.358920	7.314432
6.230736	403.593672	7.319437
6.272112	402.854872	7.324442
6.025064	395.532855	7.329446
6.160364	410.360422	7.334451
6.403125	403.946413	7.339456
6.360991	404.778981	7.344461
6.480212	400.504763	7.349466
6.129685	393.051085	7.354470
6.204953	392.093998	7.359475
6.430207	396.866213	7.364480
6.295036	410.508522	7.369485
6.275731	395.287045	7.374490
6.217296	392.054817	7.379494
6.401169	394.008568	7.384499
6.020989	380.989097	7.389504
5.911467	407.862578	7.394509
6.223103	399.041205	7.399514
6.205223	406.907376	7.404518
6.269308	409.791750	7.409523
6.627432	401.162852	7.414528
6.283912	405.783229	7.419533
6.400591	406.640060	7.424538
6.702882	408.463067	7.429542
6.306971	394.988650	7.434547
6.140627	379.800562	7.439552
5.927305	379.543827	7.444557
6.130010	387.800488	7.449562
6.188500	396.923940	7.454566
6.374337	404.212594	7.459571
6.362959	406.701326	7.464576
6.214388	400.379018	7.469581
6.326659	407.594401	7.474586
5.879006	414.033022	7.479590
6.159530	403.454326	7.484595
6.201043	396.753856	7.489600
6.340174	415.684390	7.494605
6.157935	398.373618	7.499610
6.263138	405.112510	7.504614
6.244275	412.232567	7.509619
6.658445	403.377181	7.514624
6.136407	415.138070	7.519629
6.194046	409.572747	7.524634
6.443731	405.451083	7.529638
6.229270	401.167293	7.534643
6.199658	404.758579	7.539648
5.919496	410.537181	7.544653
6.336010	396.851462	7.549658
6.080204	408.232549	7.554662
6.151274	408.842206	7.559667
6.248659	401.538635	7.564672
6.260553	413.830113	7.569677
6.414236	407.517043	7.574682
6.342593	411.193505	7.579686
6.230402	407.914322	7.584691
6.273020	404.014606	7.589696
6.005587	414.796058	7.594701
6.403152	401.695889	7.599706
6.132490	406.184368	7.604710
6.212393	402.679202	7.609715
6.495626	403.015858	7.614720
6.224538	399.200637	7.619725
6.292718	397.158597	7.624730
6.501492	402.291829	7.629734
6.236996	404.787666	7.634739
6.511218	399.921490	7.639744
5.783849	396.492909	7.644749
5.914380	406.401742	7.649754
5.973860	419.777798	7.654758
6.022349	404.426631	7.659763
6.455777	401.226566	7.664768
6.086502	410.034604	7.669773
6.309446	407.760120	7.674778
6.219129	407.771605	7.679782
5.779910	408.462926	7.684787
6.380796	414.878712	7.689792
6.468501	435.027106	7.694797
6.367236	421.904490	7.699802
6.417505	404.815227	7.704806
6.061348	410.686194	7.709811
6.393012	409.229794	7.714816
6.200695	409.744770	7.719821
6.336468	410.433703	7.724826
6.321552	409.016820	7.729830
6.337624	421.368085	7.734835
6.474038	394.879923	7.739840
6.025954	421.147047	7.744845
6.364923	401.592982	7.749850
6.128746	409.439690	7.754854
6.165787	401.524997	7.759859
6.285037	401.682279	7.764864
5.872020	406.137460	7.769869
6.146510	422.597859	7.774874
6.587274	436.407126	7.779878
6.367002	421.751341	7.784883
6.674022	412.893138	7.789888
6.353828	413.172364	7.794893
6.253320	402.418300	7.799898
6.425035	407.132975	7.804902
5.954869	400.065249	7.809907
6.380205	397.300280	7.814912
6.181555	406.772437	7.819917
6.337459	409.238262	7.824922
6.478843	421.240121	7.829926
6.476089	412.580786	7.834931
6.590677	407.975970	7.839936
6.411490	421.514681	7.844941
6.429745	401.477655	7.849946
6.523931	414.362521	7.854950
6.312042	406.181474	7.859955
6.656816	405.315984	7.864960
6.374977	417.790760	7.869965
6.404780	406.142017	7.874970
6.402928	414.333058	7.879974
6.414864	414.415738	7.884979
6.164929	388.137533	7.889984
6.365383	388.938101	7.894989
6.417899	390.496372	7.899994
6.220836	378.388246	7.904998
5.812652	385.748815	7.910003
6.238703	403.312492	7.915008
6.259333	409.397903	7.920013
6.452406	400.289423	7.925018
6.287413	400.630996	7.930022
6.193704	412.813062	7.935027
6.643922	404.628450	7.940032
6.445834	397.587678	7.945037
6.077141	393.051583	7.950042
5.810702	399.131850	7.955046
5.960792	404.013558	7.960051
6.377972	400.183839	7.965056
5.962577	408.881612	7.970061
6.489424	410.188668	7.975066
6.426434	388.610772	7.980070
6.330480	402.915136	7.985075
6.761108	405.876157	7.990080
6.431909	392.313575	7.995085
6.394570	375.972671	8.000090
6.311635	370.871947	8.005094
6.057721	361.809734	8.010099
5.884812	373.827290	8.015104
6.112549	388.258578	8.020109
5.935685	389.304169	8.025126
6.073303	394.015821	8.030144
6.048631	388.647722	8.035162
6.370783	403.528733	8.040179
6.448689	401.169197	8.045197
6.181415	398.385640	8.050214
6.624005	397.502016	8.055232
6.547546	396.006630	8.060250
6.599527	395.949741	8.065267
6.347224	401.084685	8.070285
6.507899	396.364305	8.075302
6.477194	405.557037	8.080320
6.317029	394.454499	8.085338
6.245551	368.198335	8.090355
6.065542	376.005595	8.095373
6.149149	393.379350	8.100390
6.415904	391.780016	8.105408
6.440997	405.686296	8.110426
6.485455	409.377519	8.115443
6.342627	408.347794	8.120461
6.441845	418.325231	8.125478
6.776450	398.081390	8.130496
6.125648	391.132890	8.135514
6.258025	387.847490	8.140531
6.340658	401.915863	8.145549
6.310798	390.700678	8.150566
6.622692	393.391676	8.155584
6.381934	396.972003	8.160602
6.814487	398.864938	8.165619
6.286422	389.244942	8.170637
6.483402	377.653007	8.175654
6.283249	373.583530	8.180672
6.040823	400.731327	8.185690
6.592765	399.606369	8.190707
6.507610	407.461141	8.195725
6.513096	388.914639	8.200742
6.505793	398.351066	8.205760
5.902695	398.499845	8.210778
6.371190	407.457174	8.215795
6.125361	382.062731	8.220813
6.241316	407.803768	8.225830
6.262241	392.003538	8.230848
5.883765	406.610581	8.235866
6.357455	409.608805	8.240883
6.433166	395.910925	8.245901
6.215607	400.364041	8.250918
6.150323	397.875259	8.255936
6.187986	435.133786	8.260954
6.768032	422.347239	8.265971
6.622360	419.887679	8.270989
6.470806	431.439991	8.276006
6.769754	431.750343	8.281024
6.702096	428.395068	8.286042
6.418671	437.331044	8.291059
6.797141	434.143018	8.296077
6.921453	427.139224	8.301094
6.746574	419.522663	8.306112
6.365775	405.450342	8.311130
6.391927	397.031694	8.316147
6.176696	408.477714	8.321165
6.669369	428.299140	8.326182
7.016224	432.846932	8.331200
6.812077	415.383859	8.336218
6.654083	409.916953	8.341235
6.608944	405.276238	8.346253
6.244744	412.915488	8.351270
6.655457	403.269738	8.356288
6.722814	435.383581	8.361306
6.619601	405.249835	8.366323
6.702506	412.849047	8.371341
6.591059	410.811959	8.376358
6.497755	400.731342	8.381376
6.715623	421.563350	8.386394
6.975365	400.308151	8.391411
6.772584	408.189840	8.396429
6.706255	420.354063	8.401446
6.741658	402.061976	8.406464
6.869559	409.385225	8.411482
6.612570	397.711056	8.416499
6.555350	404.680654	8.421517
6.523640	406.470539	8.426534
6.767235	396.609861	8.431552
6.553334	409.545888	8.436570
6.718734	396.391295	8.441587
6.612820	396.490482	8.446605
6.519843	418.429164	8.451622
6.553986	409.377478	8.456640
7.152523	434.562963	8.461658
6.889898	415.489636	8.466675
6.983297	405.276617	8.471693
6.932777	416.440181	8.476710
7.145570	402.246646	8.481728
6.745043	392.244258	8.486746
7.034813	402.954250	8.491763
7.005872	396.085608	8.496781
6.228199	402.215381	8.501798
6.456948	409.748376	8.506816
6.627012	403.552648	8.511834
6.581229	407.539216	8.516851
6.645559	409.491428	8.521869
6.395237	396.643361	8.526886
7.036267	421.198554	8.531904
6.921210	425.268109	8.536922
6.851921	412.909257	8.541939
6.852893	410.446423	8.546957
6.718476	402.408144	8.551974
7.030486	399.503471	8.556992
6.592474	403.582013	8.562010
6.522784	409.364050	8.567027
6.806575	429.768759	8.572045
6.837050	430.102716	8.577063
7.072504	435.446257	8.582080
6.713303	432.322375	8.587098
6.870064	436.082128	8.592115
7.118343	428.370739	8.597133
6.902097	426.370352	8.602151
7.119024	424.719817	8.607168
6.918321	431.366385	8.612186
7.180028	414.783833	8.617203
7.034737	412.064737	8.622221
6.511156	413.502762	8.627239
7.003441	405.542065	8.632256
6.746774	405.494067	8.637274
6.952822	429.572394	8.642291
7.100147	422.446625	8.647309
6.781261	429.007634	8.652327
6.831285	437.973325	8.657344
7.039300	433.568937	8.662362
6.904531	453.478339	8.667379
7.007500	434.822194	8.672397
6.999154	433.090022	8.677415
7.206206	431.419569	8.682432
7.205540	426.657259	8.687450
7.072868	400.674463	8.692467
6.817674	405.088044	8.697485
6.805535	408.145890	8.702503
6.812273	420.535274	8.707520
6.937648	427.540437	8.712538
7.107685	448.164600	8.717555
7.282301	439.855117	8.722573
6.800195	425.947902	8.727591
7.206150	441.364650	8.732608
6.814937	423.944780	8.737626
7.208088	443.460519	8.742643
7.227550	439.121727	8.747661
6.724947	422.162761	8.752679
7.324122	432.355830	8.757696
6.782453	425.175856	8.762714
6.836196	438.708343	8.767731
7.431884	423.901176	8.772749
6.974218	454.570168	8.777767
6.940090	443.127171	8.782784
6.927097	458.635701	8.787802
6.934451	441.720653	8.792819
7.187341	447.743213	8.797837
7.064678	450.585341	8.802855
7.238645	442.941525	8.807872
6.857121	449.094114	8.812890
6.807097	449.622819	8.817907
7.247680	444.131864	8.822925
6.770015	438.479161	8.827943
7.043974	446.367987	8.832960
7.268752	440.154346	8.837978
7.352727	443.264210	8.842995
7.373374	436.492443	8.848013
7.204417	451.459775	8.853031
7.126343	435.516061	8.858048
7.319878	445.720579	8.863066
7.030457	445.569953	8.868083
7.175653	446.452312	8.873101
6.857645	440.843480	8.878119
6.797473	442.404182	8.883136
7.107777	444.953268	8.888154
6.710369	449.990686	8.893171
7.240614	450.820042	8.898189
7.035528	469.526170	8.903207
7.223862	466.252464	8.908224
7.295419	474.787475	8.913242
7.409551	463.445813	8.918259
7.630166	475.654369	8.923277
7.308747	459.273811	8.928295
6.961341	446.247216	8.933312
7.090631	450.827720	8.938330
7.199404	466.730881	8.943347
7.362035	477.537309	8.948365
7.142777	475.636401	8.953383
7.311551	469.484252	8.958400
7.190925	473.703026	8.963418
7.407500	481.194970	8.968435
7.788299	467.147972	8.973453
7.602775	462.907302	8.978471
7.225978	456.477705	8.983488
7.104073	447.652613	8.988506
7.297350	461.754119	8.993523
7.576403	454.593185	8.998541
7.089081	457.196251	9.003559
7.238240	463.550042	9.008576
7.431862	458.001398	9.013594
7.107665	480.577424	9.018611
7.405900	475.912317	9.023629
7.128418	481.580927	9.028647
7.170141	478.577343	9.033664
7.529611	478.995280	9.038682
7.333925	476.127065	9.043699
7.474842	477.754708	9.048717
7.387369	478.601130	9.053735
7.325739	478.544910	9.058752
7.248955	480.729743	9.063770
7.113308	476.149226	9.068787
7.709262	475.923529	9.073805
7.354225	476.688709	9.078823
7.146313	482.143812	9.083840
7.306081	468.916683	9.088858
7.080564	487.339086	9.093875
7.061584	474.940285	9.098893
7.080364	484.066634	9.103911
7.702970	503.706495	9.108928
7.878203	496.056441	9.113946
7.396634	497.592422	9.118963
7.555741	477.715867	9.123981
7.455965	476.164895	9.128999
7.149466	479.576431	9.134016
7.624122	490.040047	9.139034
7.406791	489.682384	9.144051
7.639606	508.908059	9.149069
7.281397	503.642958	9.154087
7.483094	496.698667	9.159104
7.465428	502.391850	9.164122
7.656836	506.254822	9.169139
8.054032	500.200014	9.174157
7.796710	501.460323	9.179175
7.653756	485.318086	9.184192
7.440576	487.915213	9.189210
7.218206	484.674345	9.194227
7.379139	483.706885	9.199245
7.594796	504.702613	9.204263
7.640871	511.045813	9.209280
7.676876	507.462816	9.214298
7.517636	530.659016	9.219315
7.979106	503.405153	9.224333
7.684001	528.761497	9.229351
7.567100	504.702650	9.234368
8.008090	511.029196	9.239386
7.700563	489.857087	9.244403
7.689685	495.785596	9.249421
7.481171	489.400988	9.254439
7.376239	501.717972	9.259456
8.135918	494.738643	9.264474
7.987293	501.851798	9.269491
7.436358	487.670154	9.274509
7.785369	479.709382	9.279527
7.475124	481.781755	9.284544
7.861531	495.579013	9.289562
7.847004	487.271339	9.294579
7.519772	475.555191	9.299597
7.689406	504.440871	9.304615
7.640627	501.807356	9.309632
7.941805	507.985693	9.314650
7.860627	518.102723	9.319667
7.923935	489.090385	9.324685
7.573915	487.672274	9.329703
7.381293	480.479756	9.334720
7.862063	497.939431	9.339738
7.744623	511.356612	9.344755
7.667993	506.931247	9.349773
7.713171	503.794250	9.354791
7.490550	507.307745	9.359808
7.768300	511.367613	9.364826
7.673683	519.212887	9.369843
7.958247	510.716345	9.374861
7.740984	511.531082	9.379879
7.906153	506.696766	9.384896
8.062256	505.079988	9.389914
7.902054	506.145755	9.394931
7.712811	514.233570	9.399949
7.937406	514.675372	9.404967
7.858345	508.514471	9.409984
8.172988	507.998838	9.415002
7.849966	509.665074	9.420019
7.724187	503.521539	9.425037
7.995760	513.433266	9.430055
7.825002	510.409981	9.435072
7.867824	503.510144	9.440090
8.113378	505.348684	9.445107
7.799307	515.449587	9.450125
7.992524	504.140383	9.455143
7.971048	511.781396	9.460160
8.190505	508.212756	9.465178
7.992568	516.403555	9.470195
8.215948	514.860379	9.475213
8.080151	508.594221	9.480231
7.767480	511.472879	9.485248
8.285733	498.598277	9.490266
7.682417	520.747786	9.495283
8.068630	504.236465	9.500301
7.923055	508.641309	9.505319
7.966127	502.000416	9.510336
7.906885	503.427051	9.515354
7.933161	515.859729	9.520371
7.825364	519.448911	9.525389
8.046977	512.293998	9.530407
7.896131	525.002930	9.535424
8.222339	515.890027	9.540442
8.147952	507.111264	9.545459
7.677929	512.508738	9.550477
7.981074	506.780012	9.555495
7.781413	518.860079	9.560512
7.901588	510.474735	9.565530
7.858937	506.844714	9.570547
7.919830	523.570289	9.575565
8.111884	500.316356	9.580583
7.911708	520.188441	9.585600
7.764124	504.684565	9.590618
8.137754	510.107930	9.595635
8.119447	503.064694	9.600653
7.865519	516.079552	9.605671
7.799526	512.113423	9.610688
8.233093	535.745181	9.615706
8.184994	533.994868	9.620723
8.095290	542.684286	9.625741
8.278500	531.554817	9.630759
8.226019	543.776872	9.635776
8.346938	539.364805	9.640794
8.358437	531.151697	9.645811
8.410805	520.947645	9.650829
8.160147	500.953096	9.655847
8.105420	506.375907	9.660864
8.388293	513.194793	9.665882
8.469924	506.467036	9.670899
8.220741	501.771846	9.675917
8.320742	505.782661	9.680935
8.105731	489.158764	9.685952
8.167247	506.533936	9.690970
8.280641	511.611143	9.695987
7.821460	506.637452	9.701005
8.453067	509.455707	9.706023
8.020559	536.430882	9.711040
8.306789	545.811414	9.716058
8.310891	539.562862	9.721075
8.525993	539.724717	9.726093
8.488374	531.977375	9.731111
8.063986	525.290133	9.736128
8.359018	529.623549	9.741146
8.374579	527.370628	9.746163
8.510714	527.957721	9.751181
8.471452	508.991518	9.756199
8.069269	516.159670	9.761216
8.394349	509.393156	9.766234
8.541122	520.638237	9.771251
8.236333	514.762208	9.776269
8.496244	513.973315	9.781287
8.230647	522.353497	9.786304
8.246854	520.714867	9.791322
8.541810	524.526489	9.796339
8.389309	541.337529	9.801357
8.660795	538.312004	9.806375
8.046057	537.600148	9.811392
8.383488	535.389876	9.816410
8.132795	531.389125	9.821427
8.563882	543.157750	9.826445
8.472066	542.296209	9.831463
8.146232	558.424887	9.836480
8.177840	537.914681	9.841498
8.534921	543.230585	9.846515
8.192201	549.877549	9.851533
8.373588	554.900040	9.856551
8.382911	543.608209	9.861568
8.712131	550.972646	9.866586
8.655102	549.682736	9.871603
8.315879	549.118506	9.876621
8.643876	546.221988	9.881639
8.574393	545.950196	9.886656
8.084016	560.190255	9.891674
8.409892	549.030310	9.896691
8.220229	557.118019	9.901709
8.294097	547.807688	9.906727
8.631496	567.006511	9.911744
8.639881	547.892465	9.916762
8.817560	554.069385	9.921779
8.535155	547.112183	9.926797
8.782496	552.936248	9.931815
8.451092	552.957671	9.936832
8.330056	541.221468	9.941850
8.415909	545.629405	9.946867
8.332853	566.242024	9.951885
8.663282	568.268163	9.956903
8.726776	586.470531	9.961920
8.864527	581.740796	9.966938
8.801699	568.197805	9.971955
8.717369	556.311667	9.976973
8.645328	545.252708	9.981991
8.375252	547.347282	9.987008
8.639179	580.958643	9.992026
8.826028	569.418323	9.997043
8.844877	587.366625	10.002061
8.918003	562.285906	10.007079
8.560370	567.619758	10.012096
8.275172	551.186378	10.017114
8.697000	573.478081	10.022131
8.450257	578.155597	10.027149
8.666702	576.282253	10.032167
8.679253	580.501187	10.037184
9.043661	584.917321	10.042202
9.042476	571.377720	10.047219
8.839375	574.322805	10.052237
8.870337	583.799074	10.057255
8.944468	575.686093	10.062272
8.522896	576.525347	10.067290
9.219024	586.783481	10.072307
8.763013	569.992389	10.077325
8.821639	582.819960	10.082343
8.920892	570.113728	10.087360
8.624387	563.160620	10.092378
8.912262	583.121672	10.097395
8.831788	570.493552	10.102413
8.899609	580.866828	10.107431
9.198348	571.934760	10.112448
8.726772	565.336576	10.117466
8.901203	549.021284	10.122483
8.579883	553.528391	10.127501
8.988687	566.227430	10.132519
8.989830	573.067414	10.137536
8.828193	583.956727	10.142554
9.195395	583.183163	10.147571
8.812298	581.193994	10.152589
8.937503	564.231979	10.157607
9.075692	562.982623	10.162624
8.584251	555.563247	10.167642
8.812651	569.685322	10.172659
8.696308	584.946762	10.177677
9.008107	590.334517	10.182695
9.446473	574.502211	10.187712
8.929108	594.245950	10.192730
9.362712	589.453546	10.197747
8.834094	573.968486	10.202765
9.069782	575.136014	10.207783
8.954859	573.264000	10.212800
8.851563	574.175820	10.217818
8.853045	581.777354	10.222835
8.854329	578.204902	10.227853
9.123055	585.418963	10.232871
8.659913	585.808420	10.237888
8.639976	589.203423	10.242906
8.927144	574.851219	10.247923
9.056444	580.375006	10.252941
8.931841	571.172735	10.257959
8.796612	578.071663	10.262976
8.736002	577.106369	10.267994
8.828349	569.764088	10.273011
8.552609	596.698898	10.278029
8.732242	609.479140	10.283047
9.010779	589.713968	10.288064
9.216683	611.463711	10.293082
9.399604	607.150109	10.298099
9.080947	607.619205	10.303117
9.436535	611.693491	10.308135
9.449798	600.169829	10.313152
9.246919	606.921528	10.318170
9.454909	599.052091	10.323187
9.133171	614.072479	10.328205
9.192874	614.112318	10.333223
9.387780	610.765960	10.338240
9.177160	618.726491	10.343258
9.289677	600.906431	10.348275
9.553618	609.952786	10.353293
9.137627	593.727636	10.358311
9.150618	597.281231	10.363328
9.150333	611.386622	10.368346
9.576338	609.182071	10.373363
9.073915	605.012327	10.378381
9.175656	608.937865	10.383399
9.443020	605.146286	10.388416
9.097100	601.021134	10.393434
9.463626	603.822204	10.398451
9.065469	616.682190	10.403469
9.389002	607.162206	10.408487
9.559103	607.927202	10.413504
9.306179	613.360172	10.418522
9.504908	599.759072	10.423539
9.697780	619.895671	10.428557
9.153065	585.763779	10.433575
9.357283	596.360620	10.438592
9.398692	597.660031	10.443610
9.369605	598.981325	10.448627
9.076699	591.037032	10.453645
9.313292	597.209056	10.458663
9.416140	606.472037	10.463680
9.222488	607.849653	10.468698
9.388929	612.567039	10.473715
9.474324	609.063826	10.478733
9.870774	608.924625	10.483751
9.665062	614.866583	10.488768
9.307655	620.494726	10.493786
9.061000	607.822698	10.498803
9.396864	614.365128	10.503821
9.559275	624.869810	10.508839
9.543542	625.721407	10.513856
9.367613	633.718328	10.518874
9.634446	614.794005	10.523891
9.420970	621.342891	10.528909
9.281233	622.320760	10.533927
9.356362	612.057093	10.538944
9.348403	630.776007	10.543962
9.599905	619.141031	10.548979
9.627932	608.839002	10.553997
9.668325	613.589124	10.559015
10.084428	607.901719	10.564032
9.524906	607.041993	10.569050
9.627751	612.802090	10.574067
9.428346	614.607510	10.579085
9.442895	607.831362	10.584103
9.587957	615.931387	10.589120
9.552084	619.246967	10.594138
9.569990	615.990865	10.599155
9.490976	611.989569	10.604173
9.223391	609.352245	10.609191
9.654455	610.958818	10.614208
9.750986	607.159455	10.619226
9.614494	617.245247	10.624243
9.782828	607.937966	10.629261
9.392262	612.481625	10.634279
9.688558	614.266037	10.639296
9.292037	618.270572	10.644314
9.689975	637.552269	10.649331
9.884758	645.232196	10.654349
9.608197	655.556161	10.659367
9.861184	638.483701	10.664384
9.642321	653.513989	10.669402
9.655776	653.177224	10.674419
10.212436	667.230776	10.679437
9.900102	651.744336	10.684455
9.861826	630.009567	10.689472
9.637556	629.961232	10.694490
9.434845	629.762918	10.699507
9.590723	642.196616	10.704525
9.749807	657.423929	10.709543
9.699123	642.694931	10.714560
9.832720	641.707674	10.719578
9.837868	645.987577	10.724595
9.974896	655.423436	10.729613
9.585753	653.666394	10.734631
9.709289	657.085427	10.739648
9.795788	667.211251	10.744666
9.952149	644.803228	10.749683
9.904626	651.105864	10.754701
9.875782	655.565357	10.759719
10.292279	640.353754	10.764736
10.116023	644.064584	10.769754
10.019620	646.325792	10.774771
9.987323	639.440179	10.779789
9.648280	645.295451	10.784807
9.851193	648.305703	10.789824
9.610799	636.029656	10.794842
9.625220	645.385501	10.799859
9.800501	648.822647	10.804877
9.626329	650.649485	10.809895
10.057271	648.617885	10.814912
10.004255	663.561639	10.819930
9.719476	651.272054	10.824947
10.055514	648.626581	10.829965
10.290113	675.036564	10.834983
10.097531	668.736233	10.840000
9.886158	672.734982	10.845018
10.177205	662.071721	10.850035
10.278358	663.701627	10.855053
10.028257	678.564117	10.860071
10.023943	646.174976	10.865088
9.908278	659.451380	10.870106
9.999786	674.101746	10.875123
10.115330	668.271519	10.880141
10.018511	669.251252	10.885159
10.189381	675.547623	10.890176
10.236642	672.761630	10.895194
10.209103	662.492362	10.900211
10.247986	664.111500	10.905229
10.103411	678.793505	10.910247
10.310938	672.583803	10.915264
10.226336	670.673311	10.920282
10.207239	678.852944	10.925299
10.486681	667.602285	10.930317
10.096695	667.441117	10.935335
10.220589	667.130282	10.940352
10.617047	660.925081	10.945370
10.391738	659.581497	10.950387
10.399426	654.592894	10.955405
9.875905	656.245734	10.960423
9.944072	646.968463	10.965440
10.089205	669.625630	10.970458
10.061134	674.825748	10.975475
10.585288	663.539081	10.980493
10.183612	677.901463	10.985511
10.283381	666.327638	10.990528
10.179390	672.753954	10.995546
10.066422	689.275726	11.000563
10.219779	675.884366	11.005581
10.267029	685.866630	11.010599
10.139875	678.296664	11.015616
10.018171	683.828414	11.020634
10.092741	678.555497	11.025651
10.479815	677.960486	11.030669
10.065065	691.731696	11.035687
10.321320	667.477008	11.040704
10.170353	691.205700	11.045722
10.341818	706.164058	11.050739
10.856115	697.379811	11.055757
10.632139	691.783981	11.060775
10.505626	691.213523	11.065792
10.496884	690.398565	11.070810
10.454362	681.472743	11.075827
10.512773	670.081490	11.080845
10.461168	682.248506	11.085863
10.662604	680.167155	11.090880
10.488057	686.388363	11.095898
10.280347	692.169897	11.100915
10.628269	666.419057	11.105933
10.344748	688.244770	11.110951
10.524512	686.483254	11.115968
10.915693	703.257467	11.120986
10.754553	686.612447	11.126003
10.860464	684.222164	11.131021
10.416150	686.998132	11.136039
10.523031	674.849459	11.141056
10.522312	674.948975	11.146074
10.643236	687.107164	11.151091
10.986069	683.414088	11.156109
10.752135	674.416977	11.161127
10.497222	674.254545	11.166144
10.791468	673.728797	11.171162
10.381149	670.263307	11.176179
10.537753	678.729175	11.181197
10.583381	670.129549	11.186215
10.629059	676.755778	11.191232
10.682180	665.730168	11.196250
10.961620	687.317612	11.201267
10.903801	671.284699	11.206285
10.497357	685.538063	11.211303
10.609668	674.407218	11.216320
10.419751	683.193668	11.221338
10.404434	701.267502	11.226355
11.244598	697.954811	11.231373
10.755796	700.874613	11.236391
10.931161	704.822154	11.241408
10.784575	701.193717	11.246426
10.769835	703.408869	11.251443
10.765904	696.898756	11.256461
10.737712	704.833023	11.261479
10.778339	697.116553	11.266496
10.699170	704.825447	11.271514
11.011688	700.840999	11.276531
11.078583	694.128289	11.281549
11.089593	708.971078	11.286567
10.853947	689.816003	11.291584
10.873621	676.231829	11.296602
10.599567	698.376281	11.301619
11.100411	689.892902	11.306637
10.969328	708.041470	11.311655
10.885965	712.221581	11.316672
11.171356	704.391450	11.321690
10.662494	696.263852	11.326707
10.936019	712.787117	11.331725
10.896425	715.682971	11.336743
11.040439	718.040841	11.341760
11.105039	717.355063	11.346778
10.793324	712.403479	11.351795
11.240811	711.127795	11.356813
10.858588	723.110566	11.361831
10.903167	716.100826	11.366848
10.856115	708.618762	11.371866
10.641812	722.158797	11.376883
10.676894	704.991008	11.381901
10.944798	724.612723	11.386919
11.092801	710.088558	11.391936
11.246954	710.792532	11.396954
11.118350	714.982579	11.401971
10.938357	711.920929	11.406989
11.074554	705.083702	11.412007
10.785513	709.768444	11.417024
11.204582	706.921593	11.422042
11.007560	708.621933	11.427059
11.450005	701.597520	11.432077
11.153875	701.083431	11.437095
11.095513	701.494361	11.442112
11.075172	706.139914	11.447130
11.288262	709.672374	11.452147
10.892527	714.392953	11.457165
10.932474	706.114043	11.462183
11.098582	730.144438	11.467200
11.348944	740.323034	11.472218
11.236489	745.867054	11.477235
11.469793	734.074607	11.482253
11.415609	718.908237	11.487271
11.157269	719.793043	11.492288
11.369938	710.574607	11.497306
11.072870	708.613909	11.502323
11.113744	713.912263	11.507341
11.225242	739.716882	11.512359
11.428753	735.448648	11.517376
11.584775	740.971817	11.522394
11.461089	749.823816	11.527411
11.330641	721.422828	11.532429
11.149469	725.884882	11.537447
11.533859	732.865782	11.542464
11.612640	734.923001	11.547482
11.309628	720.290041	11.552499
11.395680	727.905815	11.557517
11.412737	718.604671	11.562535
11.127086	746.205085	11.567552
11.763970	728.929553	11.572570
11.311966	742.398187	11.577587
11.521175	737.784711	11.582605
11.460692	761.811077	11.587623
11.405305	742.729368	11.592640
11.457413	738.975984	11.597658
11.166040	745.280974	11.602675
11.518923	731.144673	11.607693
11.141824	740.462842	11.612711
11.238218	751.217729	11.617728
11.808844	738.378849	11.622746
11.398129	741.569243	11.627763
11.573735	752.485798	11.632781
11.681415	738.169301	11.637799
11.419206	739.497053	11.642816
11.711376	739.566569	11.647834
11.372283	741.986468	11.652851
11.599119	740.312221	11.657869
11.766240	737.626555	11.662887
11.398700	746.487461	11.667904
11.796204	741.887245	11.672922
11.661251	740.714303	11.677939
11.473183	744.467944	11.682957
11.731071	736.549355	11.687975
11.316853	741.539560	11.692992
11.804419	738.514991	11.698010
11.669821	732.339957	11.703027
11.685363	732.347636	11.708045
11.823840	737.995817	11.713063
11.621838	738.952494	11.718080
12.092730	740.470631	11.723098
11.713295	727.825169	11.728115
11.435336	730.382563	11.733133
11.837538	733.646930	11.738151
11.599689	736.955371	11.743168
11.686085	732.574341	11.748186
11.702010	747.940824	11.753203
11.636903	755.381446	11.758221
11.915853	762.094426	11.763239
11.865238	760.328857	11.768256
12.285347	759.735863	11.773274
11.822794	755.393980	11.778291
11.818954	726.750365	11.783309
12.192676	734.914805	11.788327
11.978592	731.542333	11.793344
11.950620	732.130182	11.798362
11.934546	740.830964	11.803379
11.817226	744.180595	11.808397
11.834923	735.822591	11.813415
11.798006	735.617049	11.818432
11.922091	737.249864	11.823450
12.000447	721.461057	11.828467
11.864571	732.524518	11.833485
12.193548	728.788753	11.838503
11.823033	735.780754	11.843520
11.963360	750.421158	11.848538
12.128511	757.733302	11.853555
11.872834	758.087690	11.858573
11.939595	757.636236	11.863591
11.666934	772.566307	11.868608
11.835054	777.292421	11.873626
11.915927	770.122664	11.878643
11.925696	774.414041	11.883661
12.414944	768.523496	11.888679
11.812409	773.532729	11.893696
12.133712	778.236482	11.898714
12.095321	771.657642	11.903731
12.124289	789.575186	11.908749
12.139760	769.289031	11.913767
12.265517	774.445854	11.918784
12.213499	770.980662	11.923802
12.014653	782.455544	11.928819
12.359865	757.947983	11.933837
11.981582	764.276887	11.938855
11.666333	768.502221	11.943872
12.208693	770.440722	11.948890
12.133379	773.901104	11.953907
12.000560	777.783481	11.958925
12.450047	774.437232	11.963943
11.903966	781.254874	11.968960
12.370080	779.175526	11.973978
12.572619	798.059218	11.978995
12.380326	802.156396	11.984013
12.414069	772.991853	11.989031
12.092636	779.893107	11.994048
12.372499	770.559031	11.999066
12.438517	795.778796	12.004083
12.131101	782.397066	12.009101
12.452992	793.861277	12.014119
12.463831	788.561068	12.019136
12.480350	799.839785	12.024154
12.442766	794.269302	12.029171
12.319038	785.013818	12.034189
12.662197	779.874485	12.039207
12.273205	784.258527	12.044224
12.444812	796.453297	12.049242
12.630613	795.748962	12.054259
12.263162	807.342154	12.059277
12.537097	788.819194	12.064295
12.649807	792.704395	12.069312
12.655655	802.936723	12.074330
12.703079	777.909196	12.079347
12.637142	783.419959	12.084365
12.677834	773.055210	12.089383
12.213822	774.430877	12.094400
12.516943	771.299612	12.099418
12.727883	774.585754	12.104435
11.981864	772.251520	12.109453
12.682719	788.435323	12.114471
12.655452	793.373901	12.119488
12.554759	806.597478	12.124506
12.983208	809.945002	12.129523
12.670985	810.539877	12.134541
12.691969	799.114271	12.139559
12.624751	790.627394	12.144576
12.930200	804.052189	12.149594
12.632552	784.796639	12.154611
12.048891	783.840032	12.159629
12.961024	791.038688	12.164647
12.604683	802.373217	12.169664
12.677281	804.871610	12.174682
12.771531	796.241836	12.179699
12.723312	801.685324	12.184717
12.799782	803.099301	12.189735
12.647711	801.082945	12.194752
12.855601	799.109440	12.199770
12.835616	796.839328	12.204787
12.749408	787.796090	12.209805
12.840277	797.360203	12.214823
12.645623	794.512420	12.219840
12.628296	787.577822	12.224858
12.790666	803.250094	12.229875
12.593851	795.388608	12.234893
13.091590	807.558324	12.239911
12.926424	808.168356	12.244928
12.871400	803.201778	12.249946
12.843769	807.734816	12.254963
12.934405	813.187735	12.259981
12.886936	806.974460	12.264999
13.072919	815.877463	12.270016
12.971101	821.241943	12.275034
12.912538	802.509119	12.280051
12.717923	820.962633	12.285069
12.795145	809.442216	12.290087
13.043157	816.489972	12.295104
12.877630	817.647856	12.300122
12.957124	800.454121	12.305139
12.939300	814.674282	12.310157
12.988658	808.074628	12.315175
12.828403	823.878366	12.320192
12.897010	845.494182	12.325210
13.363168	835.381637	12.330227
13.076236	836.230044	12.335245
13.117187	838.223369	12.340263
13.435114	844.219889	12.345280
13.130389	831.541922	12.350298
13.426260	833.978035	12.355315
12.937282	831.735335	12.360333
13.070292	825.584133	12.365351
13.189223	837.897850	12.370368
13.166053	841.409359	12.375386
13.230218	829.908108	12.380403
12.843944	837.821421	12.385421
13.150551	835.467518	12.390439
13.240290	818.690073	12.395456
13.280753	844.694748	12.400474
13.655126	830.199482	12.405491
13.362058	827.910042	12.410509
13.279843	837.364137	12.415527
13.109863	809.882965	12.420544
13.290746	837.990057	12.425562
13.468703	840.565411	12.430579
13.018985	840.362549	12.435597
13.256674	831.811191	12.440615
13.277629	840.194670	12.445632
13.206841	838.390410	12.450650
13.332047	834.819263	12.455667
13.222460	843.028599	12.460685
13.252107	832.503177	12.465703
13.194595	832.261873	12.470720
13.155763	845.479099	12.475738
13.195552	842.857359	12.480755
13.286955	858.306338	12.485773
13.620800	852.299450	12.490791
13.658441	864.091226	12.495808
13.659488	856.413689	12.500826
13.626528	854.037965	12.505843
13.677291	852.322938	12.510861
13.605242	836.171368	12.515879
13.359498	842.832937	12.520896
13.359317	837.653203	12.525914
13.636227	850.329798	12.530931
13.868883	859.605430	12.535949
13.969138	847.935251	12.540967
14.058713	832.363612	12.545984
13.570341	840.676182	12.551002
13.809070	839.476904	12.556019
13.508715	839.301806	12.561037
13.465768	842.495603	12.566055
13.672245	836.288075	12.571072
13.345531	846.722891	12.576090
13.395208	828.483336	12.581107
13.519168	862.503977	12.586125
13.756835	865.782476	12.591143
13.717493	865.107471	12.596160
13.610819	875.596374	12.601178
13.861750	858.458770	12.606195
13.900245	873.737910	12.611213
14.115947	876.824224	12.616231
14.099076	857.722034	12.621248
13.593508	860.850489	12.626266
13.747080	864.350312	12.631283
13.850844	862.982833	12.636301
13.976143	876.805380	12.641319
14.215968	862.150081	12.646336
13.750512	864.432457	12.651354
14.201292	825.980473	12.656371
13.631450	835.320219	12.661389
13.755299	844.645114	12.666407
13.940262	849.356068	12.671424
13.930882	865.446648	12.676442
14.151989	870.225830	12.681459
14.112916	879.025151	12.686477
14.038437	868.149977	12.691495
13.976290	837.633099	12.696512
13.655715	856.300630	12.701530
14.331510	854.994290	12.706547
14.197448	865.220655	12.711565
13.828750	858.295873	12.716583
14.074910	867.194964	12.721600
13.713426	868.468284	12.726618
14.332949	873.683173	12.731635
14.134612	865.256594	12.736653
14.082531	868.900118	12.741671
14.321437	860.419293	12.746688
13.813927	874.458687	12.751706
14.174333	858.492552	12.756723
14.041450	872.670871	12.761741
14.370719	869.454183	12.766759
14.259579	865.032254	12.771776
14.024365	882.833565	12.776794
14.370980	869.912727	12.781811
13.988137	871.668196	12.786829
13.943309	862.089568	12.791847
14.146210	869.588883	12.796864
13.939039	863.071942	12.801882
14.065441	863.746265	12.806899
14.191502	855.693238	12.811917
14.107090	865.924682	12.816935
14.083778	868.695956	12.821952
14.014293	869.381002	12.826970
14.291763	876.746572	12.831987
14.293299	905.626717	12.837005
14.501983	894.799810	12.842023
14.487647	895.766590	12.847040
14.379634	899.995598	12.852058
14.519829	892.204249	12.857075
14.002590	886.235656	12.862093
14.267904	893.210724	12.867111
14.847592	888.652290	12.872128
14.633578	912.586748	12.877146
14.555841	884.649585	12.882163
14.559135	886.638808	12.887181
14.322685	890.692237	12.892199
14.599556	891.633157	12.897216
14.299761	901.766664	12.902234
14.551950	901.851841	12.907251
14.706002	894.742773	12.912269
14.416770	898.433834	12.917287
14.896437	896.550016	12.922304
14.659185	901.818038	12.927322
14.704949	907.040080	12.932339
14.774506	886.413543	12.937357
14.510625	886.123390	12.942375
14.525294	879.165062	12.947392
14.393647	890.832116	12.952410
14.528518	887.282190	12.957427
14.832101	899.076465	12.962445
14.492205	899.516311	12.967463
14.911222	889.108078	12.972480
14.545126	893.541602	12.977498
14.688038	908.411569	12.982515
14.738413	889.752959	12.987533
14.757446	902.322816	12.992551
14.725757	884.313933	12.997568
14.424690	889.359583	13.002586
14.473643	900.588414	13.007603
14.709799	882.886954	13.012621
14.457647	893.197205	13.017639
14.684268	889.942373	13.022656
14.967686	897.860939	13.027674
14.711668	905.739576	13.032691
14.954431	895.878618	13.037709
14.847836	923.144129	13.042727
14.871234	916.029853	13.047744
14.979852	929.943962	13.052762
15.223450	930.295257	13.057779
15.086539	899.886354	13.062797
14.494565	904.500970	13.067815
14.631711	913.125459	13.072832
14.649853	920.032161	13.077850
14.585242	915.881690	13.082867
15.198007	921.459335	13.087885
15.274761	919.575185	13.092903
15.135722	919.488360	13.097920
14.963719	938.106543	13.102938
14.781235	922.235567	13.107955
15.170297	922.468949	13.112973
15.100378	912.014439	13.117991
15.303747	910.199502	13.123008
15.247213	923.458589	13.128026
15.392833	916.056859	13.133043
15.031902	914.893694	13.138061
15.099142	922.005123	13.143079
15.514106	918.378990	13.148096
14.824326	905.094976	13.153114
15.030812	922.465459	13.158131
15.226156	898.379191	13.163149
15.158464	911.011529	13.168167
15.259494	919.844597	13.173184
15.449934	910.840882	13.178202
15.436252	928.668909	13.183219
15.193703	903.706415	13.188237
15.133405	920.118182	13.193255
15.821592	918.533974	13.198272
15.500295	913.106370	13.203290
15.123558	922.502523	13.208307
15.681276	907.242522	13.213325
15.474377	914.657158	13.218343
15.647695	915.974256	13.223360
15.489450	905.457496	13.228378
15.517520	912.305284	13.233395
15.684273	906.675310	13.238413
15.229309	922.383694	13.243431
15.382367	918.057425	13.248448
15.393244	926.408078	13.253466
15.171121	923.734650	13.258483
15.257787	921.496784	13.263501
15.373985	920.738510	13.268519
15.607507	914.360479	13.273536
15.633383	927.082361	13.278554
15.433694	906.994630	13.283571
15.611539	918.349209	13.288589
15.547094	923.192127	13.293607
15.564689	907.019174	13.298624
15.765846	909.194053	13.303642
15.623863	923.131267	13.308659
15.708020	906.842911	13.313677
15.390354	916.316087	13.318695
15.513596	931.980985	13.323712
15.895824	934.281024	13.328730
15.381402	947.629181	13.333747
15.902279	943.560350	13.338765
15.496816	939.734439	13.343783
15.737458	949.029864	13.348800
15.853946	946.556415	13.353818
15.869119	952.542591	13.358835
15.785842	948.300928	13.363853
15.540091	960.387874	13.368871
15.600748	949.102218	13.373888
15.879754	928.003301	13.378906
15.806186	951.769397	13.383923
15.998824	946.449423	13.388941
15.820878	952.074500	13.393959
15.777165	936.981066	13.398976
15.771430	940.216753	13.403994
15.993419	947.806728	13.409011
15.917625	945.299224	13.414029
15.969953	948.544900	13.419047
16.114714	949.140818	13.424064
16.028095	934.022989	13.429082
15.856829	951.204220	13.434099
15.804319	941.151339	13.439117
15.619524	953.328083	13.444135
15.906290	942.468731	13.449152
16.008487	962.923447	13.454170
16.232733	967.413531	13.459187
16.517954	979.299390	13.464205
16.377647	963.599211	13.469223
15.967437	943.055005	13.474240
15.998039	955.949709	13.479258
15.957321	955.444570	13.484275
16.240046	966.967044	13.489293
16.295318	967.985426	13.494311
16.463764	964.253993	13.499328
16.073072	956.536246	13.504346
15.851298	953.970208	13.509363
16.206807	962.645725	13.514381
16.508576	975.280137	13.519399
16.717381	963.955031	13.524416
16.332931	956.343116	13.529434
16.509816	943.014054	13.534451
16.584750	934.962449	13.539469
16.233094	935.363501	13.544487
16.528469	942.701642	13.549504
16.361275	944.467435	13.554522
16.304181	942.954625	13.559539
16.404255	942.398374	13.564557
16.695237	937.903674	13.569575
16.481630	940.815731	13.574592
16.681298	943.334181	13.579610
16.500094	943.693093	13.584627
16.509411	941.657034	13.589645
16.155823	950.723968	13.594663
15.969432	939.495675	13.599680
16.575945	947.858119	13.604698
16.427491	965.860883	13.609715
16.580725	958.399523	13.614733
16.450670	968.927483	13.619751
16.923003	974.337653	13.624768
16.901224	958.207561	13.629786
16.238144	955.149728	13.634803
16.754556	964.543649	13.639821
16.790643	978.052372	13.644839
16.573193	973.078729	13.649856
16.970308	964.940607	13.654874
16.880060	969.667066	13.659891
16.642098	943.171155	13.664909
16.725343	956.000580	13.669927
16.537749	941.174657	13.674944
16.671978	960.277659	13.679962
16.669637	966.978468	13.684979
16.945887	976.518062	13.689997
16.927170	976.789213	13.695015
16.873662	982.593392	13.700032
17.165141	974.477740	13.705050
16.561913	958.517042	13.710067
16.779602	958.917687	13.715085
17.012526	956.955376	13.720103
16.746644	969.573674	13.725120
17.141019	979.295963	13.730138
16.807384	969.923320	13.735155
16.676702	974.387828	13.740173
17.069531	958.716748	13.745191
16.957963	968.649083	13.750208
16.893341	962.282712	13.755226
17.002707	960.719366	13.760243
17.066761	959.908502	13.765261
16.920411	965.476603	13.770279
16.679926	981.376909	13.775296
17.221251	964.502637	13.780314
17.071319	970.079401	13.785331
17.235048	973.814815	13.790349
16.994602	966.383673	13.795367
16.720317	971.332722	13.800384
17.176456	954.737532	13.805402
16.643590	975.303803	13.810419
16.955231	962.142370	13.815437
16.783603	982.420665	13.820455
17.068002	993.958922	13.825472
17.187147	1003.400705	13.830490
16.889611	1008.829181	13.835507
17.310797	1006.938877	13.840525
17.556775	1003.689285	13.845543
17.209269	999.711592	13.850560
17.889165	980.417255	13.855578
17.678292	1001.498813	13.860595
17.642577	978.112842	13.865613
17.534375	976.568918	13.870631
17.178003	979.967846	13.875648
17.127742	957.261506	13.880666
17.325481	983.426699	13.885683
17.373063	970.592782	13.890701
17.701472	995.785851	13.895719
17.648708	988.348284	13.900736
17.445410	962.248580	13.905754
16.894431	984.117632	13.910771
17.249132	985.412340	13.915789
17.818573	1007.231476	13.920807
17.638601	1013.053908	13.925824
17.632715	1005.680813	13.930842
17.426337	1012.619246	13.935859
17.443673	1006.721676	13.940877
17.764811	1008.502129	13.945895
17.696848	1006.240407	13.950912
17.600211	999.925756	13.955930
17.624643	1003.041244	13.960947
17.833796	997.885509	13.965965
17.654916	1002.372455	13.970983
17.379057	989.620213	13.976000
17.836518	995.571201	13.981018
17.773805	998.107730	13.986035
17.691086	1000.032854	13.991053
17.826556	996.536334	13.996071
17.590179	1002.384024	14.001088
17.569586	1002.310787	14.006106
17.728200	998.813098	14.011123
17.754368	1002.805052	14.016141
17.485256	1004.059084	14.021159
17.517139	1005.767189	14.026176
18.018812	1005.938372	14.031194
17.659811	1009.812526	14.036211
17.851741	1008.438042	14.041229
18.083322	1008.511767	14.046247
17.886003	1015.751682	14.051264
18.112410	1011.870732	14.056282
17.929953	1002.012570	14.061299
18.073717	1029.942041	14.066317
18.250278	1017.105467	14.071335
17.754436	1007.073554	14.076352
17.929818	1008.136936	14.081370
18.003095	1015.029944	14.086387
18.030608	1026.866028	14.091405
17.901473	1020.377551	14.096423
18.096413	1027.192796	14.101440
18.143180	1030.259728	14.106458
18.383125	1014.155207	14.111475
18.095185	1033.414560	14.116493
18.106925	1021.649257	14.121511
17.964173	1022.084473	14.126528
18.342159	1028.906371	14.131546
18.431506	1026.115819	14.136563
18.533892	1029.390140	14.141581
18.566847	1026.605464	14.146599
18.430335	1037.031806	14.151616
18.498362	1027.651596	14.156634
18.402667	1026.921444	14.161651
18.305796	1016.179066	14.166669
18.781446	1012.744703	14.171687
18.163409	1013.475927	14.176704
18.251768	989.228500	14.181722
18.072848	1007.484023	14.186739
18.303529	1003.821017	14.191757
18.269595	1021.091710	14.196775
18.008926	1014.651737	14.201792
18.178658	1021.725906	14.206810
18.326894	1024.072008	14.211827
18.316504	1017.145408	14.216845
18.478274	1020.344576	14.221863
17.892855	1023.937231	14.226880
18.510405	1049.377023	14.231898
18.543561	1051.070261	14.236915
18.764387	1055.007921	14.241933
18.761586	1052.841795	14.246951
18.649330	1055.207430	14.251968
18.819664	1040.968268	14.256986
18.940147	1037.545556	14.262003
18.617841	1026.305317	14.267021
18.600862	1016.292863	14.272039
18.387770	1025.752958	14.277056
18.862409	1030.864711	14.282074
19.030156	1038.396683	14.287091
19.002586	1031.679067	14.292109
19.061014	1020.265116	14.297127
18.845814	1021.442048	14.302144
18.753582	1009.088572	14.307162
19.128903	1010.706074	14.312179
18.553278	1010.615430	14.317197
18.769157	1009.615930	14.322215
18.577204	1021.476666	14.327232
18.959748	1027.132937	14.332250
18.955962	1048.774387	14.337267
18.818648	1046.707145	14.342285
18.839160	1051.618230	14.347303
18.876598	1050.648215	14.352320
18.905368	1056.116758	14.357338
19.229285	1052.096290	14.362355
18.924100	1057.951928	14.367373
19.506318	1049.581548	14.372391
19.028497	1058.465186	14.377408
19.011210	1044.136189	14.382426
19.370078	1048.049460	14.387443
19.167668	1066.189082	14.392461
19.105597	1049.262892	14.397479
19.419516	1057.839948	14.402496
19.178589	1052.727871	14.407514
19.698573	1040.463705	14.412531
19.130308	1039.738533	14.417549
19.239285	1035.578040	14.422567
19.219235	1030.855646	14.427584
19.279897	1046.341579	14.432602
19.605059	1033.103952	14.437619
19.334832	1026.797312	14.442637
19.714012	1023.845114	14.447655
19.517144	1009.040731	14.452672
19.231057	1012.099785	14.457690
19.283222	1007.624653	14.462707
18.969373	995.685277	14.467725
19.366974	1019.015731	14.472743
19.750526	1034.943549	14.477760
19.381218	1043.271483	14.482778
19.337982	1044.669644	14.487795
19.271625	1041.567992	14.492813
19.742388	1051.919084	14.497831
19.800663	1042.330979	14.502848
20.028416	1037.370831	14.507866
19.954196	1031.836032	14.512883
19.289988	1025.050635	14.517901
19.613627	1004.874621	14.522919
19.453474	1020.834215	14.527936
19.417408	1016.149503	14.532954
19.572457	1029.852537	14.537971
19.388116	1038.147541	14.542989
19.581645	1038.497568	14.548007
19.511448	1038.981804	14.553024
19.779655	1042.542133	14.558042
19.479867	1042.132744	14.563059
19.222588	1043.305709	14.568077
19.896952	1049.936646	14.573095
19.536237	1049.390215	14.578112
19.714257	1053.153397	14.583130
19.682564	1034.191395	14.588147
19.515569	1049.997955	14.593165
19.597560	1049.426779	14.598183
19.877071	1072.522167	14.603200
19.787304	1085.443070	14.608218
20.057621	1067.955458	14.613235
19.612021	1083.168089	14.618253
19.920840	1078.114825	14.623271
20.232104	1077.328933	14.628288
19.565386	1088.372132	14.633306
20.112174	1071.202127	14.638323
20.118654	1083.346382	14.643341
20.104208	1088.941341	14.648359
20.127407	1079.899136	14.653376
20.098247	1094.398234	14.658394
20.200465	1070.512474	14.663411
20.142509	1086.561521	14.668429
20.120466	1076.889546	14.673447
20.088733	1081.259603	14.678464
19.962556	1061.680557	14.683482
20.423946	1067.425166	14.688499
20.374065	1057.850104	14.693517
19.853341	1073.395633	14.698535
20.106317	1066.242266	14.703552
20.027593	1071.358195	14.708570
20.378957	1068.153166	14.713587
20.479580	1074.420769	14.718605
20.531453	1068.476139	14.723623
20.352836	1070.328853	14.728640
20.390153	1073.368916	14.733658
20.587896	1073.073226	14.738675
20.103741	1078.796379	14.743693
20.324030	1074.306532	14.748711
20.489334	1079.485164	14.753728
20.274309	1106.535118	14.758746
20.419251	1097.297039	14.763763
20.367831	1101.211705	14.768781
20.559487	1104.081619	14.773799
20.924443	1099.094251	14.778816
20.711421	1109.081425	14.783834
20.932148	1091.495411	14.788851
20.860097	1081.399517	14.793869
20.466398	1074.716309	14.798887
20.671570	1065.396562	14.803904
21.046572	1079.299063	14.808922
20.717947	1073.802945	14.813939
20.545398	1062.635448	14.818957
20.706444	1064.065781	14.823975
20.869200	1055.252732	14.828992
20.551404	1056.939907	14.834010
21.240265	1069.985610	14.839027
20.844056	1075.075874	14.844045
20.893613	1055.424892	14.849063
20.770527	1060.489993	14.854080
20.612273	1059.543263	14.859098
20.670639	1063.208336	14.864115
21.035807	1084.040326	14.869133
21.082329	1098.318703	14.874151
21.218587	1099.051138	14.879168
20.952223	1084.655217	14.884186
21.142247	1065.452058	14.889203
20.837030	1065.931442	14.894221
20.918083	1080.171820	14.899239
21.196138	1082.841867	14.904256
21.107504	1098.827313	14.909274
21.281689	1092.783445	14.914291
21.265991	1071.584051	14.919309
20.866971	1065.629406	14.924327
20.895580	1069.430272	14.929344
20.839073	1092.527982	14.934362
21.279931	1091.131346	14.939379
21.355329	1101.187656	14.944397
21.186713	1105.739652	14.949415
21.310053	1102.134903	14.954432
21.292672	1101.656703	14.959450
21.187022	1106.443708	14.964467
21.440134	1101.318166	14.969485
21.574682	1098.585175	14.974503
21.639873	1100.515685	14.979520
21.231388	1100.931937	14.984538
21.484344	1092.218206	14.989555
21.127884	1095.101942	14.994573
21.290975	1090.882307	14.999591
21.445356	1090.934448	15.004608
21.324071	1086.256220	15.009626
21.152647	1092.831617	15.014643
21.066319	1092.889981	15.019661
21.163505	1106.277133	15.024679
21.435315	1093.543231	15.029696
21.117667	1111.902099	15.034714
21.684539	1105.114460	15.039731
21.847204	1100.905028	15.044749
21.184435	1106.910896	15.049767
21.844249	1105.950994	15.054784
21.532621	1111.040971	15.059802
21.402015	1100.720446	15.064819
21.557558	1093.592318	15.069837
21.548420	1122.068360	15.074855
22.011130	1105.098290	15.079872
21.726535	1129.482171	15.084890
22.025278	1104.634180	15.089907
21.983143	1101.175252	15.094925
21.645952	1113.754677	15.099943
21.793197	1105.173341	15.104960
21.777102	1113.266608	15.109978
21.674169	1106.286085	15.114995
21.942507	1112.839791	15.120013
21.363413	1114.164933	15.125031
21.972979	1114.102691	15.130048
21.675862	1128.768513	15.135066
22.086933	1124.686193	15.140083
22.352371	1132.446893	15.145101
22.213889	1143.622767	15.150119
22.415772	1123.666965	15.155136
21.833910	1123.446476	15.160154
22.091758	1095.844692	15.165171
22.074445	1115.665286	15.170189
22.247544	1107.761698	15.175207
22.689254	1112.092297	15.180224
22.186095	1102.608052	15.185242
22.270545	1097.356385	15.190259
22.616223	1099.584851	15.195277
22.225215	1092.645740	15.200295
22.261566	1102.886807	15.205312
22.190925	1092.567793	15.210330
22.362274	1098.790556	15.215347
22.488670	1087.050340	15.220365
22.304953	1108.423746	15.225383
22.551664	1103.115939	15.230400
22.348696	1119.226771	15.235418
22.545790	1096.963288	15.240435
22.601074	1088.721784	15.245453
22.115498	1100.416883	15.250471
22.278958	1101.058721	15.255488
22.107787	1111.711852	15.260506
22.441801	1123.643094	15.265523
22.514710	1130.459757	15.270541
22.264657	1151.282508	15.275559
22.799068	1130.561283	15.280576
22.650784	1139.692310	15.285594
22.707085	1125.764265	15.290611
22.668826	1140.023038	15.295629
22.694150	1138.599812	15.300647
22.763494	1138.701529	15.305664
22.734988	1147.427721	15.310682
23.001389	1132.692297	15.315699
22.793743	1136.762384	15.320717
22.700632	1129.563152	15.325735
22.689990	1133.856626	15.330752
22.567142	1132.502856	15.335770
22.617226	1134.370627	15.340787
22.665731	1132.892599	15.345805
22.305399	1136.539105	15.350823
22.644681	1133.155788	15.355840
22.650042	1141.577434	15.360858
23.009887	1167.292730	15.365875
23.165443	1158.871370	15.370893
23.272251	1176.173790	15.375911
23.329229	1149.742731	15.380928
23.014999	1151.122018	15.385946
23.127477	1145.804397	15.390963
23.158821	1155.982563	15.395981
23.026375	1155.778631	15.400999
23.227289	1151.320008	15.406016
23.013755	1152.515469	15.411034
23.267767	1164.201855	15.416051
23.726991	1145.825264	15.421069
22.780399	1147.332271	15.426087
22.909396	1156.517464	15.431104
23.100648	1157.452673	15.436122
23.295259	1166.370101	15.441139
23.332041	1155.238006	15.446157
23.290428	1158.638096	15.451175
23.469449	1145.906495	15.456192
23.674131	1159.650251	15.461210
23.607724	1159.810318	15.466227
23.780867	1146.422067	15.471245
23.625520	1152.862482	15.476263
23.946808	1152.837841	15.481280
23.830831	1135.650742	15.486298
23.409383	1133.065812	15.491315
23.292593	1121.255940	15.496333
23.216369	1125.770042	15.501351
23.391494	1143.489775	15.506368
23.483935	1149.084608	15.511386
23.215944	1151.176851	15.516403
23.500144	1148.686775	15.521421
23.397390	1163.111505	15.526439
23.420228	1157.484163	15.531456
23.478274	1165.142176	15.536474
23.411233	1165.943733	15.541491
23.792833	1156.788135	15.546509
23.769230	1176.894328	15.551527
23.996404	1177.599541	15.556544
23.876105	1158.035045	15.561562
23.725292	1163.982410	15.566579
24.010936	1152.609043	15.571597
23.712081	1171.815071	15.576615
23.921267	1162.157082	15.581632
24.108487	1180.680871	15.586650
23.895861	1188.468644	15.591667
23.915754	1176.784237	15.596685
24.122384	1192.357982	15.601703
24.211161	1176.726789	15.606720
24.227715	1176.158156	15.611738
24.421459	1174.275996	15.616755
24.214831	1146.195298	15.621773
24.349509	1143.905087	15.626791
24.328881	1155.997396	15.631808
24.210309	1150.394606	15.636826
23.965868	1147.727187	15.641843
23.989658	1140.657416	15.646861
24.020846	1157.766554	15.651879
23.977769	1170.398384	15.656896
24.275398	1178.485894	15.661914
24.367330	1197.923863	15.666931
24.584069	1173.316425	15.671949
24.360775	1188.340983	15.676967
24.370986	1187.499938	15.681984
24.776900	1178.806244	15.687002
24.441219	1176.977525	15.692019
24.446403	1180.565706	15.697037
24.366382	1188.280593	15.702055
24.465032	1191.164023	15.707072
24.800455	1182.158823	15.712090
24.470567	1193.230175	15.717107
24.717207	1180.702577	15.722125
24.565748	1191.451794	15.727143
24.208776	1180.756021	15.732160
24.411124	1202.181678	15.737178
24.128722	1184.024719	15.742195
24.138864	1190.303287	15.747213
24.362912	1195.745022	15.752231
24.472785	1195.332680	15.757248
24.725640	1212.601954	15.762266
24.673110	1206.080566	15.767283
24.770504	1213.737414	15.772301
25.054418	1220.291250	15.777319
25.062701	1211.213056	15.782336
25.279546	1211.311752	15.787354
25.070686	1216.579618	15.792371
24.938347	1184.970161	15.797389
24.592472	1190.933928	15.802407
24.574838	1183.825619	15.807424
24.717190	1199.874944	15.812442
24.927221	1213.485710	15.817459
25.393837	1198.900068	15.822477
24.952189	1209.699318	15.827495
25.162677	1216.880105	15.832512
24.969525	1204.085872	15.837530
25.197422	1217.088416	15.842547
25.280913	1206.278706	15.847565
25.326776	1211.036081	15.852583
25.112028	1207.690475	15.857600
25.167735	1206.141089	15.862618
25.232439	1213.912369	15.867635
25.786890	1199.823313	15.872653
25.308016	1205.814870	15.877671
25.400507	1208.785030	15.882688
25.620092	1203.776977	15.887706
25.111740	1204.380266	15.892723
25.374618	1209.651060	15.897741
25.780800	1205.018966	15.902759
25.614786	1215.823743	15.907776
25.657416	1207.944616	15.912794
25.333748	1218.834685	15.917811
25.649689	1213.526519	15.922829
25.594229	1204.750527	15.927847
25.568430	1211.606072	15.932864
25.915461	1192.985624	15.937882
25.816002	1223.458111	15.942899
25.982376	1197.374556	15.947917
26.104067	1195.316745	15.952935
25.430314	1175.859528	15.957952
25.506829	1174.981647	15.962970
25.318223	1187.818207	15.967987
25.704652	1191.116178	15.973005
25.722453	1200.773703	15.978023
25.648307	1206.918996	15.983040
26.087561	1200.318212	15.988058
25.709507	1200.200722	15.993075
26.009410	1202.934980	15.998093
26.056079	1199.457319	16.003111
25.963927	1188.252828	16.008128
26.280907	1194.442807	16.013146
25.839541	1204.491788	16.018163
25.801931	1201.825802	16.023181
26.193846	1200.003388	16.028199
25.956953	1206.935636	16.033216
26.505483	1192.894207	16.038234
25.845982	1202.531700	16.043251
26.053641	1202.842102	16.048269
26.162251	1219.009891	16.053287
26.082485	1203.065755	16.058304
26.283990	1207.918149	16.063322
25.896947	1198.146214	16.068339
25.900477	1202.327253	16.073357
26.301591	1212.389542	16.078375
25.922051	1201.451281	16.083392
26.578836	1201.600279	16.088410
25.945053	1228.379865	16.093427
26.303068	1222.128443	16.098445
26.461142	1237.951541	16.103463
26.434711	1234.287868	16.108480
26.938887	1220.502112	16.113498
26.641510	1216.421612	16.118515
26.902337	1213.645002	16.123533
26.729108	1194.572362	16.128551
26.526957	1194.774246	16.133568
26.416681	1188.393579	16.138586
26.286292	1183.157703	16.143603
26.925263	1211.255811	16.148621
26.817948	1205.807600	16.153639
26.796033	1197.214904	16.158656
26.672748	1188.866765	16.163674
26.418919	1197.548742	16.168691
26.860190	1212.761171	16.173709
26.801904	1206.990855	16.178727
26.654780	1212.765425	16.183744
26.783112	1232.844518	16.188762
26.900998	1222.844082	16.193779
26.952254	1224.531593	16.198797
26.779496	1211.122314	16.203815
26.992455	1215.836432	16.208832
27.190973	1209.276902	16.213850
27.054027	1212.381314	16.218867
26.882004	1213.797918	16.223885
27.099296	1220.555239	16.228903
26.807474	1214.432166	16.233920
27.005156	1222.210110	16.238938
26.942481	1211.613188	16.243955
26.894617	1219.062403	16.248973
26.987189	1214.579156	16.253991
26.801619	1215.161480	16.259008
27.200450	1230.598605	16.264026
27.264648	1228.299364	16.269043
27.398572	1240.226272	16.274061
27.249852	1243.315513	16.279079
27.170027	1254.878142	16.284096
27.601579	1244.331188	16.289114
27.383543	1258.396602	16.294131
27.619689	1257.630101	16.299149
27.719465	1242.232501	16.304167
27.259929	1243.144581	16.309184
27.319573	1245.512934	16.314202
27.196053	1242.620838	16.319219
27.470179	1262.098352	16.324237
27.432994	1259.106474	16.329255
27.087324	1257.738640	16.334272
27.384401	1248.816886	16.339290
27.463420	1258.811495	16.344307
27.302713	1263.486022	16.349325
27.596489	1247.132553	16.354343
27.336133	1264.745888	16.359360
27.586061	1277.847773	16.364378
27.636943	1288.072590	16.369395
27.514330	1281.256226	16.374413
27.817661	1277.842901	16.379431
27.562687	1281.881387	16.384448
27.939170	1277.622206	16.389466
27.902679	1291.113580	16.394483
28.001858	1272.476231	16.399501
27.896052	1280.682421	16.404519
27.963391	1283.825316	16.409536
28.048397	1276.779118	16.414554
27.994193	1277.257078	16.419571
27.984510	1269.577465	16.424589
28.381502	1265.487792	16.429607
27.710603	1276.763161	16.434624
28.027081	1275.747808	16.439642
28.299102	1304.792943	16.444659
28.516815	1315.060174	16.449677
28.516441	1291.361654	16.454695
28.439298	1292.163706	16.459712
28.529111	1265.720329	16.464730
28.115403	1273.069335	16.469747
28.501184	1277.677765	16.474765
28.741145	1263.162876	16.479783
28.119264	1277.636599	16.484800
28.448042	1264.363439	16.489818
28.277378	1283.485248	16.494835
28.469071	1274.514373	16.499853
28.298228	1279.879498	16.504871
28.681539	1294.607210	16.509888
28.608665	1295.637442	16.514906
28.598372	1297.808057	16.519923
28.676791	1300.104434	16.524941
28.979157	1293.375478	16.529959
28.960093	1309.153628	16.534976
28.923894	1282.669938	16.539994
28.882249	1286.436119	16.545011
28.483678	1266.705116	16.550029
28.938334	1261.963935	16.555047
28.655789	1266.966105	16.560064
28.614437	1276.982684	16.565082
28.685522	1292.941840	16.570099
28.593073	1302.589209	16.575117
29.042098	1298.728769	16.580135
28.896000	1300.395173	16.585152
28.893449	1292.748911	16.590170
29.046539	1295.085199	16.595187
29.016293	1301.983439	16.600205
28.897247	1297.410559	16.605223
28.776385	1304.518415	16.610240
28.763596	1301.863563	16.615258
28.988134	1288.080463	16.620275
28.693030	1297.448200	16.625293
29.086863	1293.683870	16.630311
28.986816	1325.680919	16.635328
29.248012	1330.641178	16.640346
29.349306	1344.187371	16.645363
29.058061	1333.358904	16.650381
29.567050	1328.233120	16.655399
29.548185	1338.927957	16.660416
29.572905	1333.638550	16.665434
29.531597	1329.879500	16.670451
29.562648	1324.882095	16.675469
29.815817	1324.150761	16.680487
29.625512	1320.426175	16.685504
29.897799	1322.927965	16.690522
29.690606	1305.896465	16.695539
29.372257	1310.628545	16.700557
29.649510	1310.388987	16.705575
29.914645	1327.553925	16.710592
29.572764	1328.726721	16.715610
29.886138	1321.580279	16.720627
29.694906	1330.099560	16.725645
29.606665	1323.166893	16.730663
29.576238	1325.237810	16.735680
29.673248	1336.986880	16.740698
30.046825	1332.036685	16.745715
29.852857	1324.615203	16.750733
29.757837	1325.084558	16.755751
29.808975	1321.214191	16.760768
29.754725	1334.195070	16.765786
29.950396	1313.461384	16.770803
29.796736	1325.946003	16.775821
30.138435	1310.633821	16.780839
30.038607	1328.271772	16.785856
29.905768	1326.105645	16.790874
29.875537	1330.112515	16.795891
29.987528	1346.261676	16.800909
30.277092	1358.612954	16.805927
30.227680	1345.772906	16.810944
30.209573	1356.912807	16.815962
30.352856	1358.170355	16.820979
30.355206	1350.112026	16.825997
30.871098	1357.805081	16.831015
30.726781	1356.132961	16.836032
30.514767	1353.416259	16.841050
30.476729	1328.123376	16.846067
30.191278	1330.513344	16.851085
30.722672	1334.164276	16.856103
30.702762	1345.806422	16.861120
30.613450	1351.654740	16.866138
30.657550	1333.260520	16.871155
30.420026	1334.446675	16.876173
30.802411	1334.006812	16.881191
30.852214	1347.781154	16.886208
30.597162	1328.976043	16.891226
30.713106	1336.586885	16.896243
30.731115	1349.436473	16.901261
31.014827	1340.370155	16.906279
30.931091	1348.290907	16.911296
30.749792	1340.802083	16.916314
30.938189	1342.567512	16.921331
30.760119	1340.708004	16.926349
31.071994	1349.862600	16.931367
31.117145	1337.848083	16.936384
30.700152	1348.252891	16.941402
30.987474	1339.454914	16.946419
31.007169	1338.272113	16.951437
30.999906	1334.258672	16.956455
31.087433	1340.609928	16.961472
31.037022	1336.296303	16.966490
31.190400	1347.444367	16.971507
30.888718	1357.527242	16.976525
31.129678	1346.285694	16.981543
31.336302	1351.998316	16.986560
30.992755	1335.925623	16.991578
31.221011	1336.280448	16.996595
30.984582	1344.414972	17.001613
31.022924	1351.323253	17.006631
31.490993	1369.629245	17.011648
31.508553	1369.131487	17.016666
31.519404	1367.639584	17.021683
31.632827	1380.346392	17.026701
31.832269	1373.669441	17.031719
31.513855	1372.437810	17.036736
31.596474	1367.734754	17.041754
31.616667	1369.305788	17.046771
31.631785	1373.463802	17.051789
31.873440	1379.662565	17.056807
31.702611	1365.233962	17.061824
31.671872	1361.400733	17.066842
31.257413	1363.819798	17.071859
31.388174	1368.110143	17.076877
31.571239	1368.074494	17.081895
31.847972	1369.264823	17.086912
31.673172	1363.722908	17.091930
31.735309	1367.418035	17.096947
32.005703	1385.227498	17.101965
32.006110	1391.908260	17.106983
32.419879	1382.817374	17.112000
32.094797	1387.861152	17.117018
32.475030	1359.442289	17.122035
32.276497	1366.267800	17.127053
32.288919	1359.844643	17.132071
32.059970	1364.932160	17.137088
32.243571	1363.447530	17.142106
32.213475	1349.075590	17.147123
32.041845	1352.439051	17.152141
32.214264	1381.604508	17.157159
32.579917	1379.103593	17.162176
32.305633	1397.405647	17.167194
32.453454	1386.688306	17.172211
32.423738	1394.375795	17.177229
32.583658	1391.150773	17.182247
32.883857	1383.888887	17.187264
32.400669	1385.867641	17.192282
32.928258	1392.743114	17.197299
32.613531	1385.922139	17.202317
32.576522	1384.893359	17.207335
32.700080	1403.925763	17.212352
32.608267	1394.751525	17.217370
32.758305	1396.297267	17.222387
32.928657	1385.555243	17.227405
32.695168	1392.738728	17.232423
32.885485	1386.179297	17.237440
32.807556	1394.546456	17.242458
32.972488	1392.654762	17.247475
32.599968	1377.753682	17.252493
32.722853	1386.964428	17.257511
32.924491	1382.380449	17.262528
32.729571	1383.410780	17.267546
32.802365	1389.770297	17.272563
32.750884	1389.308941	17.277581
32.520893	1399.161934	17.282599
32.679222	1394.520850	17.287616
32.831873	1411.874808	17.292634
33.212185	1418.089642	17.297651
33.174451	1418.159362	17.302669
33.122851	1415.646700	17.307687
33.631250	1421.314499	17.312704
33.071617	1432.948382	17.317722
33.041362	1413.397513	17.322739
33.614537	1410.825594	17.327757
33.395279	1418.761889	17.332775
33.577878	1403.812742	17.337792
33.553997	1413.817863	17.342810
33.754338	1407.693975	17.347827
33.934287	1408.238536	17.352845
33.701503	1419.132425	17.357863
33.811690	1411.556922	17.362880
33.948080	1407.958899	17.367898
33.773686	1404.988486	17.372915
33.803158	1397.919822	17.377933
33.826320	1406.788279	17.382951
33.883221	1414.910776	17.387968
33.859379	1408.915842	17.392986
33.748209	1402.608543	17.398003
33.686638	1406.274723	17.403021
33.531575	1412.272187	17.408039
33.891177	1400.770692	17.413056
33.642403	1402.735410	17.418074
33.900470	1403.837016	17.423091
33.726150	1400.753132	17.428109
33.688718	1415.669755	17.433127
34.430927	1416.507933	17.438144
34.141021	1435.840147	17.443162
34.084655	1437.040359	17.448179
34.161787	1441.927747	17.453197
33.923089	1445.840975	17.458215
34.266816	1433.207284	17.463232
34.053499	1446.167802	17.468250
34.187375	1439.684787	17.473267
34.691064	1441.652796	17.478285
34.325575	1440.961204	17.483303
34.557846	1430.139346	17.488320
34.624379	1436.101971	17.493338
34.400067	1435.115456	17.498355
34.440806	1426.278764	17.503373
34.534415	1438.084072	17.508391
34.801900	1424.918814	17.513408
34.727551	1438.380656	17.518426
34.705558	1433.091062	17.523443
34.539251	1430.937142	17.528461
34.533108	1430.646108	17.533479
34.840694	1426.543910	17.538496
34.825187	1427.687183	17.543514
34.722166	1429.753481	17.548531
34.892673	1426.113800	17.553549
34.646270	1429.903324	17.558567
35.230211	1445.460637	17.563584
35.109662	1441.884597	17.568602
34.959066	1430.590886	17.573619
35.029533	1421.985159	17.578637
35.149139	1456.252670	17.583655
35.105320	1448.643752	17.588672
35.146726	1445.492918	17.593690
35.385067	1450.980305	17.598707
35.272967	1437.471748	17.603725
35.062532	1445.109518	17.608743
35.400135	1452.277479	17.613760
35.290949	1463.047158	17.618778
35.324523	1473.357914	17.623795
35.451641	1449.376425	17.628813
35.371564	1470.879930	17.633831
35.802257	1449.548287	17.638848
35.588603	1458.553622	17.643866
35.209899	1445.361694	17.648883
35.597148	1442.349730	17.653901
35.278009	1456.872194	17.658919
35.733342	1450.493500	17.663936
35.721684	1456.326073	17.668954
35.281933	1449.228353	17.673971
35.937630	1445.657474	17.678989
35.695090	1455.707219	17.684007
35.755290	1459.469799	17.689024
35.635583	1454.617219	17.694042
35.609203	1459.481963	17.699059
35.892775	1451.276146	17.704077
35.486730	1451.771611	17.709095
35.756674	1457.200444	17.714112
35.734513	1449.295589	17.719130
35.755587	1473.124790	17.724147
36.099892	1473.329564	17.729165
36.051509	1475.823754	17.734183
36.108819	1462.285212	17.739200
36.233004	1483.558468	17.744218
36.143758	1473.681350	17.749235
36.357907	1476.928147	17.754253
36.465570	1466.803678	17.759271
36.406625	1474.142471	17.764288
36.311396	1475.880392	17.769306
36.474050	1479.676922	17.774323
36.562559	1475.299562	17.779341
36.477830	1468.778955	17.784359
36.521586	1472.588144	17.789376
36.504897	1474.247943	17.794394
36.213268	1473.866713	17.799411
36.633397	1466.312095	17.804429
36.748770	1473.838473	17.809447
36.376667	1464.031720	17.814464
36.586079	1475.731718	17.819482
36.334824	1474.754572	17.824499
36.676302	1480.200227	17.829517
36.526308	1487.759442	17.834535
36.870873	1492.036829	17.839552
37.161696	1485.282046	17.844570
37.177247	1491.335187	17.849587
37.359807	1494.304492	17.854605
37.015997	1491.684135	17.859623
37.054792	1504.285687	17.864640
37.472070	1490.533042	17.869658
37.372391	1475.418607	17.874675
37.272017	1457.212840	17.879693
37.305550	1440.485824	17.884711
37.220951	1456.723481	17.889728
37.328125	1451.803494	17.894746
36.985408	1458.048573	17.899763
37.356132	1464.776121	17.904781
37.235189	1480.923767	17.909799
37.408437	1497.044858	17.914816
37.741987	1489.637578	17.919834
37.331557	1495.177675	17.924851
37.568394	1498.484494	17.929869
37.383641	1483.146069	17.934887
37.627800	1500.546706	17.939904
37.564619	1483.377356	17.944922
37.488799	1488.226957	17.949939
37.877238	1488.200470	17.954957
37.541359	1493.328726	17.959975
37.598650	1494.485166	17.964992
37.732041	1489.059269	17.970010
37.661797	1494.705419	17.975027
37.774827	1482.507560	17.980045
37.639853	1479.104331	17.985063
37.569912	1486.205038	17.990080
37.485086	1488.120928	17.995098
37.521563	1493.714803	18.000115
37.858229	1515.699585	18.005133
37.974850	1513.046829	18.010151
38.143470	1514.502031	18.015168
38.117088	1526.383424	18.020186
37.926728	1527.509349	18.025203
37.977238	1529.376803	18.030221
38.274650	1521.568085	18.035239
38.593088	1514.104937	18.040256
38.422683	1514.008629	18.045274
38.170236	1512.920185	18.050291
38.452502	1510.525922	18.055309
38.303031	1508.362714	18.060327
38.305391	1504.433644	18.065344
38.819605	1513.428945	18.070362
38.182909	1521.922360	18.075379
38.491009	1521.513859	18.080397
38.814973	1537.880404	18.085415
38.888962	1539.880663	18.090432
38.941311	1534.817576	18.095450
38.767220	1534.885523	18.100467
39.039634	1531.159209	18.105485
39.251300	1534.986130	18.110503
38.787684	1519.716974	18.115520
39.223563	1500.424523	18.120538
38.974266	1507.314870	18.125555
39.059460	1504.773783	18.130573
38.925502	1507.162360	18.135591
38.946581	1511.535523	18.140608
39.081905	1510.833496	18.145626
38.740258	1532.349118	18.150643
39.188436	1532.681481	18.155661
39.251862	1540.165896	18.160679
39.197266	1549.839934	18.165696
39.378713	1531.543521	18.170714
39.094925	1538.085916	18.175731
39.597738	1537.259493	18.180749
39.375097	1547.759163	18.185767
39.367001	1538.310331	18.190784
39.355560	1525.640591	18.195802
39.315263	1541.707764	18.200819
39.422481	1532.259660	18.205837
39.388779	1530.043368	18.210855
39.437518	1530.449315	18.215872
39.729792	1535.531940	18.220890
39.384607	1554.115231	18.225907
39.796720	1550.110270	18.230925
39.877160	1555.090928	18.235943
39.739461	1554.858336	18.240960
40.148769	1556.059837	18.245978
39.930837	1555.597937	18.250995
39.702477	1561.053355	18.256013
39.676705	1558.300133	18.261031
39.821203	1549.757183	18.266048
40.290311	1552.813864	18.271066
39.915110	1557.254197	18.276083
40.356544	1557.924023	18.281101
40.075710	1554.249371	18.286119
40.067952	1553.216139	18.291136
40.168020	1549.182445	18.296154
40.030681	1565.939063	18.301171
40.065749	1559.320093	18.306189
40.041484	1558.429619	18.311207
40.053093	1571.094269	18.316224
40.807313	1574.499722	18.321242
40.155419	1589.748616	18.326259
40.503738	1579.101530	18.331277
40.686780	1582.301533	18.336295
40.910825	1590.012429	18.341312
40.931947	1585.395339	18.346330
40.728537	1590.028606	18.351347
40.744596	1587.342859	18.356365
40.910925	1585.577853	18.361383
40.944024	1588.319566	18.366400
41.201350	1576.213709	18.371418
41.095946	1583.161496	18.376435
40.954215	1549.818254	18.381453
40.665369	1561.789592	18.386471
40.733888	1582.282979	18.391488
40.911221	1575.641576	18.396506
40.713129	1595.174128	18.401523
40.863913	1591.136667	18.406541
40.830159	1580.709969	18.411559
40.495690	1584.648799	18.416576
40.770803	1597.561796	18.421594
41.123513	1610.233190	18.426611
41.384745	1620.584952	18.431629
41.211446	1613.711474	18.436647
41.433597	1620.148550	18.441664
41.815336	1606.056864	18.446682
41.366531	1617.117075	18.451699
41.464423	1592.787409	18.456717
41.674351	1602.439909	18.461735
41.541354	1605.601904	18.466752
41.958613	1601.778129	18.471770
41.869696	1600.643073	18.476787
41.699018	1603.507322	18.481805
41.876108	1591.815318	18.486823
41.602072	1592.822426	18.491840
41.867794	1582.343384	18.496858
41.762444	1611.845968	18.501875
41.644095	1599.190685	18.506893
41.923611	1600.333339	18.511911
41.759383	1610.960280	18.516928
42.037742	1623.419805	18.521946
42.336742	1628.838977	18.526963
42.291139	1630.306662	18.531981
42.364875	1629.506463	18.536999
42.264382	1616.895449	18.542016
42.157573	1617.681459	18.547034
42.349843	1616.467955	18.552051
42.324298	1625.486389	18.557069
42.594651	1622.978058	18.562087
42.838825	1621.237381	18.567104
42.776032	1604.113590	18.572122
42.518067	1590.332901	18.577139
42.382652	1584.085526	18.582157
42.563531	1591.523889	18.587175
42.332286	1607.083820	18.592192
42.342365	1604.212384	18.597210
42.541680	1620.063505	18.602227
42.597400	1618.819623	18.607245
42.610842	1604.795786	18.612263
42.587607	1620.198350	18.617280
42.865917	1617.749618	18.622298
42.764073	1618.026054	18.627315
42.722499	1621.041672	18.632333
43.068802	1615.050636	18.637351
42.611840	1619.654959	18.642368
42.853264	1628.139910	18.647386
43.259223	1645.904545	18.652403
43.054276	1656.690184	18.657421
43.364261	1643.235293	18.662439
43.016590	1655.692017	18.667456
43.705554	1640.020805	18.672474
43.576359	1660.694872	18.677491
43.335005	1646.613219	18.682509
43.629678	1650.619720	18.687527
43.082579	1654.693783	18.692544
43.037186	1649.466040	18.697562
43.409975	1644.794855	18.702579
43.453701	1645.783898	18.707597
43.254486	1644.375983	18.712615
43.097323	1647.484610	18.717632
43.874149	1655.238220	18.722650
43.855068	1673.592605	18.727667
43.843308	1688.506727	18.732685
43.875334	1689.049371	18.737703
43.826079	1686.804039	18.742720
44.444196	1682.510132	18.747738
44.117533	1686.408139	18.752755
43.881430	1672.660272	18.757773
43.732918	1679.876590	18.762791
43.895168	1678.238797	18.767808
44.275037	1666.031042	18.772826
44.268647	1681.418190	18.777843
44.076013	1668.443892	18.782861
44.405849	1670.508069	18.787879
43.946694	1667.269861	18.792896
44.099601	1680.107571	18.797914
44.306271	1662.499314	18.802931
43.739740	1665.403107	18.807949
44.233058	1694.924615	18.812967
44.394730	1695.436585	18.817984
44.507467	1700.268379	18.823002
44.642166	1686.492289	18.828019
44.289744	1702.636105	18.833037
44.861286	1678.999926	18.838055
44.688550	1702.513746	18.843072
44.914535	1688.163626	18.848090
44.967609	1697.626992	18.853107
44.860828	1691.671337	18.858125
44.915608	1699.825629	18.863143
45.054109	1679.330869	18.868160
44.998136	1693.002355	18.873178
45.231716	1691.057262	18.878195
45.191475	1687.907471	18.883213
45.128234	1689.635210	18.888231
45.275826	1691.077470	18.893248
45.613070	1700.414269	18.898266
45.428220	1691.904310	18.903283
45.186394	1683.316879	18.908301
45.349577	1681.860195	18.913319
45.279949	1702.192060	18.918336
45.515312	1710.301166	18.923354
45.787009	1726.169564	18.928371
45.921751	1712.965476	18.933389
45.935296	1704.843016	18.938407
45.698194	1691.009192	18.943424
45.631154	1677.130352	18.948442
45.565673	1684.483414	18.953459
45.816889	1687.383452	18.958477
45.699027	1676.537012	18.963495
45.678769	1700.181900	18.968512
45.753465	1706.854853	18.973530
45.762470	1711.669744	18.978547
45.318909	1717.000772	18.983565
45.917446	1701.571069	18.988583
45.822835	1715.435832	18.993600
45.966530	1711.624763	18.998618
46.142618	1703.689279	19.003635
45.679808	1704.387892	19.008653
46.171498	1726.499199	19.013671
46.158080	1725.433728	19.018688
46.097558	1745.359108	19.023706
46.406127	1735.652552	19.028723
46.280977	1727.238495	19.033741
46.438086	1740.406991	19.038759
46.249640	1722.040498	19.043776
46.323432	1742.518664	19.048794
46.633360	1732.984980	19.053811
46.538901	1747.895999	19.058829
46.936416	1736.381198	19.063847
46.763347	1738.714574	19.068864
46.771963	1747.306750	19.073882
47.103799	1760.697227	19.078899
47.145601	1753.761965	19.083917
47.055875	1751.617092	19.088935
46.787974	1740.445863	19.093952
46.920407	1756.248839	19.098970
47.228599	1757.637800	19.103987
47.302945	1767.393010	19.109005
47.403232	1773.874398	19.114023
47.619444	1758.074437	19.119040
47.360044	1749.964485	19.124058
47.406143	1737.156051	19.129075
47.029974	1740.170499	19.134093
47.512943	1753.183211	19.139111
47.529001	1757.195631	19.144128
47.542476	1743.439522	19.149146
47.749055	1765.830632	19.154163
47.726758	1758.448471	19.159181
47.901234	1746.899766	19.164199
47.898051	1752.325619	19.169216
47.763612	1744.592186	19.174234
47.890925	1753.487522	19.179251
47.699968	1751.677228	19.184269
47.734577	1740.654396	19.189287
47.952801	1754.329141	19.194304
47.948111	1755.342527	19.199322
47.732056	1744.050348	19.204339
47.875540	1751.401975	19.209357
47.931753	1745.269099	19.214375
47.964599	1748.395550	19.219392
47.966940	1748.640995	19.224410
48.138787	1757.017460	19.229427
47.951915	1759.539403	19.234445
48.400034	1773.705206	19.239463
48.335075	1767.512045	19.244480
48.237951	1775.299035	19.249498
48.178304	1787.841611	19.254515
48.451561	1776.163491	19.259533
48.302617	1791.045177	19.264551
48.577304	1775.606231	19.269568
48.573426	1779.534764	19.274586
48.903236	1778.144809	19.279603
48.743645	1791.620063	19.284621
48.553188	1790.325133	19.289639
48.794262	1783.409674	19.294656
48.821882	1817.730687	19.299674
49.133241	1810.818461	19.304691
48.979446	1819.339109	19.309709
48.987626	1814.562014	19.314727
48.809210	1807.777565	19.319744
48.957373	1808.358884	19.324762
49.551943	1802.784438	19.329779
49.530167	1815.336129	19.334797
49.655000	1805.990830	19.339815
49.725036	1818.134022	19.344832
49.619178	1795.151921	19.349850
49.754674	1789.101478	19.354867
49.555892	1772.040908	19.359885
49.696428	1755.802066	19.364903
49.380779	1756.069946	19.369920
49.399486	1760.851464	19.374938
49.518948	1787.064820	19.379955
49.576400	1784.157280	19.384973
49.643504	1790.858291	19.389991
49.395630	1804.817642	19.395008
49.462011	1801.453691	19.400026
49.765052	1804.595532	19.405043
49.731605	1812.831478	19.410061
49.801469	1795.262700	19.415079
49.848189	1821.687901	19.420096
49.928406	1823.826511	19.425114
50.222633	1817.685469	19.430131
49.790612	1831.661497	19.435149
49.806684	1833.739265	19.440167
49.893247	1822.435400	19.445184
49.814749	1842.811921	19.450202
50.501564	1848.292457	19.455219
50.737635	1838.758612	19.460237
50.399816	1849.976797	19.465255
50.718197	1850.921746	19.470272
51.057396	1847.428467	19.475290
51.250567	1847.735374	19.480307
50.678119	1843.946567	19.485325
50.729193	1843.050515	19.490343
50.839311	1843.567073	19.495360
50.802675	1840.372076	19.500378
51.161402	1836.944555	19.505395
51.128372	1842.316329	19.510413
50.929195	1831.910694	19.515431
51.389173	1850.759444	19.520448
51.144718	1839.764154	19.525466
51.360539	1837.956401	19.530483
51.143027	1851.185422	19.535501
51.103298	1840.879393	19.540519
51.152650	1836.854005	19.545536
50.727802	1847.291347	19.550554
51.320185	1836.748607	19.555571
51.488097	1837.383543	19.560589
51.258004	1832.049769	19.565607
51.214549	1849.390772	19.570624
51.356625	1857.603346	19.575642
51.514488	1867.723881	19.580659
51.682975	1863.023214	19.585677
51.525906	1871.398889	19.590695
52.008852	1863.740211	19.595712
51.885679	1879.107296	19.600730
51.884317	1868.381403	19.605747
51.840242	1864.023972	19.610765
51.813898	1862.772671	19.615783
51.704430	1864.708326	19.620800
52.148028	1887.972284	19.625818
52.116867	1894.974662	19.630835
52.227578	1894.912984	19.635853
52.162412	1900.828276	19.640871
52.282386	1906.499334	19.645888
51.907346	1901.410411	19.650906
52.125147	1901.386144	19.655923
52.251371	1894.718607	19.660941
52.422331	1884.677775	19.665959
52.263018	1901.554116	19.670976
52.340328	1894.068634	19.675994
52.808534	1906.515519	19.681011
53.027032	1912.451349	19.686029
52.786337	1904.684123	19.691047
52.955280	1908.859769	19.696064
53.011957	1909.679594	19.701082
52.947720	1910.042126	19.706099
53.149386	1922.668181	19.711117
52.751893	1927.045189	19.716135
53.090498	1919.036094	19.721152
53.070827	1925.849123	19.726170
53.335003	1921.883472	19.731187
53.768142	1920.506837	19.736205
53.421569	1919.790446	19.741223
53.647942	1918.897699	19.746240
53.505117	1928.964832	19.751258
53.628929	1904.908781	19.756275
53.893886	1919.210872	19.761293
53.509929	1913.279579	19.766311
53.748476	1897.129195	19.771328
53.358198	1923.095091	19.776346
53.719562	1906.113233	19.781363
53.822994	1910.386500	19.786381
53.711049	1907.144299	19.791399
53.804575	1912.077644	19.796416
54.107613	1913.003975	19.801434
54.071399	1904.385789	19.806451
53.663671	1919.802101	19.811469
53.618889	1911.412450	19.816487
54.050874	1902.219056	19.821504
53.568157	1920.292937	19.826522
53.934830	1939.590108	19.831539
54.079903	1931.468525	19.836557
54.144299	1954.072643	19.841575
54.358757	1941.261804	19.846592
54.096705	1951.503055	19.851610
54.450593	1941.068146	19.856627
54.608248	1949.914595	19.861645
54.397075	1971.707247	19.866663
54.540991	1965.976152	19.871680
54.549638	1975.160173	19.876698
54.772089	1959.804759	19.881715
55.109594	1973.876744	19.886733
54.824681	1960.083446	19.891751
54.510034	1965.515477	19.896768
54.579940	1951.394213	19.901786
54.957663	1956.501730	19.906803
55.086766	1970.346485	19.911821
55.136745	1988.649488	19.916839
55.014010	1996.334543	19.921856
55.160070	1990.544531	19.926874
55.333758	1989.766865	19.931891
55.778104	2001.070142	19.936909
55.497870	1984.331598	19.941927
56.077504	1985.477829	19.946944
55.563651	1978.976153	19.951962
55.490334	1983.848032	19.956979
55.680603	1982.179696	19.961997
55.746086	1988.152354	19.967015
55.765753	1983.508520	19.972032
55.773931	1991.171054	19.977050
55.802614	1983.707636	19.982067
55.820905	1989.758455	19.987085
55.580049	1999.130150	19.992103
55.991189	1987.408716	19.997120
56.081539	1997.793597	20.002138
55.927543	1985.563986	20.007155
56.085685	1992.717083	20.012173
55.833741	2001.350293	20.017191
55.815175	2006.487098	20.022208
56.209924	2017.051178	20.027226
56.159119	2011.408532	20.032243
56.415019	2015.844690	20.037261
56.223399	2019.806867	20.042279
56.297224	2020.473103	20.047296
56.351721	2044.686085	20.052314
56.651425	2064.700063	20.057331
56.973109	2052.686133	20.062349
56.690668	2050.129932	20.067367
57.160388	2034.791742	20.072384
56.912148	2028.881178	20.077402
57.144280	2034.576164	20.082419
57.167748	2034.057922	20.087437
56.839342	2030.995042	20.092455
56.958519	2035.966011	20.097472
56.930568	2039.062319	20.102490
57.123314	2039.065024	20.107507
57.320080	2042.543318	20.112525
57.462259	2038.171396	20.117543
57.730674	2033.214246	20.122560
57.511985	2050.765799	20.127578
57.404424	2033.863356	20.132595
57.799691	2041.097447	20.137613
57.572638	2033.057477	20.142631
57.483659	2051.135727	20.147648
57.605151	2056.745577	20.152666
58.154415	2058.958162	20.157683
58.247513	2066.774978	20.162701
58.110729	2062.261876	20.167719
58.107963	2061.954822	20.172736
58.318467	2061.837093	20.177754
58.067628	2062.413995	20.182771
58.393807	2053.798132	20.187789
57.975372	2056.086880	20.192807
58.178349	2058.445648	20.197824
58.082813	2063.500228	20.202842
58.362701	2066.989492	20.207859
58.380690	2060.106345	20.212877
58.312648	2054.750340	20.217895
58.127176	2061.512199	20.222912
58.294517	2062.701964	20.227930
58.290750	2077.302305	20.232947
58.425438	2092.573557	20.237965
58.266734	2086.518079	20.242983
58.378423	2095.183362	20.248000
58.568285	2094.137513	20.253018
58.966133	2105.436644	20.258035
59.141349	2101.391274	20.263053
59.181603	2105.095902	20.268071
59.167906	2105.087158	20.273088
59.464404	2111.472104	20.278106
59.303113	2097.856152	20.283123
59.563407	2098.510375	20.288141
59.328156	2092.046554	20.293159
59.386365	2102.665223	20.298176
59.574193	2100.876924	20.303194
59.677539	2100.821088	20.308211
59.772828	2093.839439	20.313229
59.699995	2109.135355	20.318247
59.769735	2089.209681	20.323264
59.718424	2106.970901	20.328282
59.716837	2094.035033	20.333299
60.055649	2100.082823	20.338317
60.035586	2107.488316	20.343335
59.479971	2097.282813	20.348352
59.705689	2099.944764	20.353370
59.720018	2103.708687	20.358387
60.089183	2115.423321	20.363405
60.242443	2132.849735	20.368423
60.236114	2121.996260	20.373440
60.208662	2130.393169	20.378458
60.349269	2135.741568	20.383475
60.656328	2125.172861	20.388493
60.539728	2139.499633	20.393511
60.681018	2121.493062	20.398528
60.586360	2130.636187	20.403546
60.847564	2135.017772	20.408563
60.753943	2113.891022	20.413581
60.534381	2129.251651	20.418599
60.591046	2125.628059	20.423616
61.276169	2146.172842	20.428634
61.239781	2145.787695	20.433651
61.305858	2153.095525	20.438669
61.141823	2134.067332	20.443687
61.076630	2151.179434	20.448704
61.518621	2152.999297	20.453722
61.381102	2171.280066	20.458739
61.743855	2138.508467	20.463757
61.381723	2158.152685	20.468775
61.449343	2150.367747	20.473792
61.714554	2148.680219	20.478810
61.549081	2157.658320	20.483827
61.797956	2157.125067	20.488845
61.774319	2152.406659	20.493863
61.432747	2144.089247	20.498880
61.586526	2145.425133	20.503898
61.457456	2151.861427	20.508915
61.421658	2157.915246	20.513933
61.740952	2173.134227	20.518951
61.988120	2179.332602	20.523968
62.290616	2181.420361	20.528986
62.113405	2183.311255	20.534003
62.327031	2183.255007	20.539021
62.474019	2191.373756	20.544039
62.204234	2186.846184	20.549056
62.598304	2179.328690	20.554074
62.349150	2187.227315	20.559091
62.434413	2179.496327	20.564109
62.543978	2194.573047	20.569127
62.609255	2191.933482	20.574144
62.648129	2187.207095	20.579162
62.462577	2193.443129	20.584179
62.868762	2188.935723	20.589197
63.082601	2189.514176	20.594215
62.699923	2187.033266	20.599232
63.545249	2197.955423	20.604250
63.292304	2197.884754	20.609267
63.303822	2180.079057	20.614285
63.520566	2197.622100	20.619303
63.441197	2196.033036	20.624320
63.563606	2182.084940	20.629338
63.256426	2200.094420	20.634355
63.731062	2217.193165	20.639373
63.643546	2213.280044	20.644391
63.536862	2235.858427	20.649408
63.876862	2215.245516	20.654426
63.361739	2229.446526	20.659443
63.695389	2213.989918	20.664461
63.996693	2215.017228	20.669479
64.005835	2210.697846	20.674496
64.336343	2220.411605	20.679514
64.075673	2208.765983	20.684531
64.245636	2217.471600	20.689549
64.305371	2211.749206	20.694567
64.332530	2205.321686	20.699584
64.584236	2208.478295	20.704602
64.271488	2218.977173	20.709619
64.466996	2204.922701	20.714637
64.558079	2219.625003	20.719655
64.207366	2211.755644	20.724672
64.373779	2210.852615	20.729690
64.498880	2218.017280	20.734707
64.679946	2232.222325	20.739725
64.905217	2233.020705	20.744743
64.042455	2240.146882	20.749760
64.481643	2243.992871	20.754778
64.932429	2244.619363	20.759795
64.632671	2258.714941	20.764813
65.191322	2263.637867	20.769831
65.093237	2271.273225	20.774848
65.156115	2267.167549	20.779866
65.180407	2270.503656	20.784883
65.378773	2274.123153	20.789901
65.277858	2262.449123	20.794919
65.357053	2282.727937	20.799936
66.027625	2283.575354	20.804954
65.966722	2294.503260	20.809971
66.009745	2283.810189	20.814989
66.025649	2266.374867	20.820007
65.642590	2273.071847	20.825024
65.977327	2273.512628	20.830042
65.923745	2290.885916	20.835059
66.008336	2300.438426	20.840077
66.527218	2286.223769	20.845095
66.299433	2288.204712	20.850112
65.919856	2298.552311	20.855130
66.333982	2289.040825	20.860147
66.272575	2294.354168	20.865165
66.467617	2288.980587	20.870183
66.253030	2295.518460	20.875200
66.921314	2290.590215	20.880218
66.750313	2284.976777	20.885235
66.607720	2298.185142	20.890253
66.848079	2292.709008	20.895271
66.766659	2316.228064	20.900288
67.193984	2314.781601	20.905306
67.048347	2308.366847	20.910323
67.203123	2316.808733	20.915341
67.506831	2295.389636	20.920359
66.871788	2309.510551	20.925376
67.379188	2296.114384	20.930394
67.231041	2308.170317	20.935411
67.206297	2297.155810	20.940429
67.500499	2299.388241	20.945447
67.376687	2312.200467	20.950464
68.021877	2304.642006	20.955482
68.189783	2308.498004	20.960499
67.828948	2305.430683	20.965517
68.039494	2298.252857	20.970535
67.531795	2306.607586	20.975552
68.218475	2292.309692	20.980570
68.048439	2308.510703	20.985587
67.850195	2291.239262	20.990605
67.936141	2295.550855	20.995623
67.954026	2300.623772	21.000640
68.181593	2298.588372	21.005658
68.490811	2326.223129	21.010675
68.248326	2328.150216	21.015693
68.420462	2325.279028	21.020711
68.451362	2334.230686	21.025728
68.855235	2325.274721	21.030746
68.691837	2328.546398	21.035763
68.530954	2325.140175	21.040781
68.784823	2329.173675	21.045799
68.376948	2332.962644	21.050816
68.552071	2328.435122	21.055834
69.027777	2342.021592	21.060851
68.865602	2353.646089	21.065869
68.993574	2361.886359	21.070887
68.905626	2357.347780	21.075904
69.033361	2370.730006	21.080922
69.021364	2357.303884	21.085939
69.067369	2371.110575	21.090957
69.235165	2359.509767	21.095975
69.117108	2388.792355	21.100992
69.316089	2383.515123	21.106010
69.392993	2380.800191	21.111027
69.681422	2394.974261	21.116045
70.087392	2373.278553	21.121063
69.603548	2390.441993	21.126080
70.045040	2390.182566	21.131098
69.997297	2386.272079	21.136115
70.167082	2405.461252	21.141133
70.616212	2408.299497	21.146151
70.405606	2409.752894	21.151168
70.740591	2397.078134	21.156186
70.481548	2384.226390	21.161203
70.647097	2389.425700	21.166221
70.933592	2377.832031	21.171239
70.472883	2372.376849	21.176256
70.783546	2378.057019	21.181274
70.829363	2370.466684	21.186291
70.605155	2405.284885	21.191309
71.004498	2400.329208	21.196327
70.792533	2413.090347	21.201344
70.934989	2412.142454	21.206362
71.101435	2400.358008	21.211379
70.908062	2399.615784	21.216397
71.321455	2399.523376	21.221415
70.963812	2399.262558	21.226432
70.943955	2399.657033	21.231450
71.309936	2410.175360	21.236467
71.235719	2432.344988	21.241485
71.473480	2428.901998	21.246503
71.331289	2422.041812	21.251520
71.614154	2429.025215	21.256538
71.456066	2419.465705	21.261555
71.208334	2452.614730	21.266573
71.634676	2453.631433	21.271591
71.840558	2457.034803	21.276608
71.965685	2456.515495	21.281626
71.971819	2450.374966	21.286643
71.806157	2450.377457	21.291661
72.058926	2471.709959	21.296679
72.341074	2481.057128	21.301696
72.579503	2479.473779	21.306714
72.997579	2487.598670	21.311731
72.717774	2489.299301	21.316749
73.453310	2479.774147	21.321767
73.057257	2474.881978	21.326784
72.976010	2456.359903	21.331802
72.922182	2453.375856	21.336819
72.715749	2444.675963	21.341837
72.947003	2439.295952	21.346855
72.869832	2473.275566	21.351872
73.214860	2461.653858	21.356890
73.525314	2480.732689	21.361907
73.116879	2478.337076	21.366925
73.737793	2468.369521	21.371943
73.341376	2480.290066	21.376960
73.099154	2471.285881	21.381978
73.393025	2473.077907	21.386995
73.367315	2478.194498	21.392013
73.545298	2476.675855	21.397031
73.297683	2479.030713	21.402048
73.473813	2490.524224	21.407066
73.546414	2502.942395	21.412083
73.790818	2501.875501	21.417101
74.125267	2504.053484	21.422119
73.902647	2506.802385	21.427136
73.814757	2505.679983	21.432154
74.135325	2522.510872	21.437171
74.194495	2532.638117	21.442189
74.471387	2534.009592	21.447207
74.237271	2528.344298	21.452224
74.743390	2530.635629	21.457242
74.770459	2526.577724	21.462259
74.719202	2521.930686	21.467277
74.868096	2522.393919	21.472295
74.981334	2524.902510	21.477312
75.006295	2522.764950	21.482330
75.253700	2524.488096	21.487347
74.968933	2515.843030	21.492365
74.950249	2522.751324	21.497383
74.862531	2542.095604	21.502400
75.034953	2554.745908	21.507418
75.341259	2562.575770	21.512435
75.634224	2556.817661	21.517453
75.666130	2559.463105	21.522471
75.734805	2561.885772	21.527488
75.756005	2557.154319	21.532506
75.587373	2555.911810	21.537523
75.865488	2561.173078	21.542541
75.839948	2557.740502	21.547559
76.226270	2558.182807	21.552576
75.835265	2569.867914	21.557594
76.177440	2580.117299	21.562611
76.169329	2581.527804	21.567629
76.714430	2562.393315	21.572647
76.344879	2564.532148	21.577664
76.250461	2569.471371	21.582682
76.289481	2573.775641	21.587699
76.609346	2564.891679	21.592717
76.398393	2555.699430	21.597735
76.688831	2578.645506	21.602752
76.967583	2584.220411	21.607770
77.123258	2603.434208	21.612787
77.089636	2589.923672	21.617805
77.093565	2602.431016	21.622823
77.161062	2585.273972	21.627840
77.181132	2600.750470	21.632858
77.338742	2588.331800	21.637875
77.053241	2604.710250	21.642893
77.505471	2595.224952	21.647911
77.258847	2596.706953	21.652928
77.345357	2592.837606	21.657946
77.681605	2606.330050	21.662963
77.568185	2625.071483	21.667981
77.553131	2618.187248	21.672999
77.796708	2624.760165	21.678016
77.825066	2619.388820	21.683034
78.141777	2621.347735	21.688051
77.793559	2620.497837	21.693069
78.013229	2622.474756	21.698087
77.889669	2627.878001	21.703104
78.446446	2636.025124	21.708122
78.485211	2634.019698	21.713139
78.346463	2653.506390	21.718157
78.510956	2649.154719	21.723175
78.654131	2652.548222	21.728192
78.528205	2648.143177	21.733210
78.871314	2655.389723	21.738227
78.791967	2651.524345	21.743245
78.941137	2645.198905	21.748263
79.137817	2649.801705	21.753280
79.013133	2653.399291	21.758298
79.049719	2655.333446	21.763315
79.074470	2662.441879	21.768333
79.657214	2674.303318	21.773351
79.498730	2662.462734	21.778368
79.436506	2675.066883	21.783386
79.505166	2673.687529	21.788403
79.601033	2669.673919	21.793421
79.939229	2672.887780	21.798439
79.774547	2671.074214	21.803456
80.026503	2666.232560	21.808474
80.101924	2676.614463	21.813491
79.731708	2672.414716	21.818509
79.695465	2701.142524	21.823527
80.111333	2697.331704	21.828544
79.931184	2699.818538	21.833562
80.067338	2699.502687	21.838579
80.307244	2702.394653	21.843597
80.409930	2713.561733	21.848615
80.460736	2718.506924	21.853632
80.645373	2719.992466	21.858650
80.943380	2715.218964	21.863667
81.037631	2719.713532	21.868685
81.243221	2708.906109	21.873703
81.396089	2705.909508	21.878720
81.164852	2713.089986	21.883738
81.148233	2708.895571	21.888755
81.472920	2716.636660	21.893773
81.368027	2718.309002	21.898791
81.470851	2705.031297	21.903808
81.444120	2719.028446	21.908826
81.488883	2707.936224	21.913843
81.728816	2716.849824	21.918861
81.881208	2748.697115	21.923879
82.115147	2725.872797	21.928896
81.677868	2744.825351	21.933914
82.001228	2751.709112	21.938931
82.027783	2747.794522	21.943949
82.249013	2748.692011	21.948967
82.004600	2743.306255	21.953984
82.039576	2757.246791	21.959002
82.317951	2746.822736	21.964019
82.333490	2759.280657	21.969037
82.434560	2765.563838	21.974055
82.777919	2769.254757	21.979072
82.762712	2773.764475	21.984090
82.431545	2765.879593	21.989107
82.596621	2775.640528	21.994125
82.511880	2760.810312	21.999143
83.103178	2783.966198	22.004160
82.787308	2803.929337	22.009178
82.896325	2792.112946	22.014195
83.077870	2796.054794	22.019213
82.999626	2807.736817	22.024231
83.432996	2791.771288	22.029248
83.220316	2808.461895	22.034266
83.491674	2816.645453	22.039283
83.763066	2816.485970	22.044301
83.814647	2831.420554	22.049319
84.024407	2828.652294	22.054336
83.767272	2823.721311	22.059354
83.761894	2825.456738	22.064371
84.132674	2815.669451	22.069389
84.221305	2815.605908	22.074407
84.526501	2805.370467	22.079424
84.402702	2803.794586	22.084442
84.607734	2805.001211	22.089459
84.451174	2811.604113	22.094477
84.480315	2805.365754	22.099495
84.650512	2825.868013	22.104512
84.455603	2846.884116	22.109530
84.895573	2842.290635	22.114547
84.995879	2849.414620	22.119565
84.904275	2849.445812	22.124583
85.206861	2827.859451	22.129600
85.084923	2832.710600	22.134618
85.179652	2838.398674	22.139635
85.385327	2847.880146	22.144653
85.572083	2866.255971	22.149671
85.727515	2857.465934	22.154688
85.468542	2881.466908	22.159706
85.647122	2856.101661	22.164723
85.900188	2862.028704	22.169741
85.741483	2863.587529	22.174759
86.084461	2851.601542	22.179776
85.967063	2863.925235	22.184794
86.045627	2859.663285	22.189811
86.040245	2859.172025	22.194829
86.084126	2878.756564	22.199847
86.269032	2873.466532	22.204864
86.401495	2888.636594	22.209882
86.580772	2876.885290	22.214899
86.821731	2881.704045	22.219917
86.642745	2888.159325	22.224935
86.797060	2873.409562	22.229952
86.747904	2896.506508	22.234970
86.895458	2908.584512	22.239987
87.172121	2915.755754	22.245005
87.301167	2908.038226	22.250023
87.386245	2897.734386	22.255040
87.451941	2921.262138	22.260058
87.307854	2907.368839	22.265075
87.496121	2917.079187	22.270093
87.292000	2922.389757	22.275111
87.552137	2911.228142	22.280128
87.203537	2924.001455	22.285146
87.694250	2921.629024	22.290163
88.011307	2936.166143	22.295181
87.627105	2935.271391	22.300199
88.009129	2934.930458	22.305216
88.088588	2953.551059	22.310234
88.196280	2967.028248	22.315251
88.480525	2965.903958	22.320269
88.288453	2967.945022	22.325287
88.701206	2969.204138	22.330304
88.537266	2966.890865	22.335322
88.727343	2953.770162	22.340339
88.719458	2961.853500	22.345357
88.706776	2961.579559	22.350375
88.961286	2972.979978	22.355392
89.175599	2988.516294	22.360410
89.120770	2977.474189	22.365427
89.437643	2984.320549	22.370445
89.076738	2996.917630	22.375463
89.499211	2971.015493	22.380480
89.497110	2989.152429	22.385498
89.512026	2973.532401	22.390515
89.431701	2984.536044	22.395533
89.297381	2981.992311	22.400551
89.635828	3001.119913	22.405568
89.783541	3000.523045	22.410586
90.084798	3006.156781	22.415603
90.444579	3008.272391	22.420621
90.264448	3001.784511	22.425639
90.172092	3004.227165	22.430656
89.907775	3011.121351	22.435674
90.567515	2990.574439	22.440691
90.787195	3014.886049	22.445709
90.657316	3033.676953	22.450727
91.395685	3029.861772	22.455744
90.970857	3028.319668	22.460762
90.921841	3024.413952	22.465779
91.164227	3032.502227	22.470797
91.151737	3030.022794	22.475815
91.245823	3031.267847	22.480832
91.105197	3030.303119	22.485850
91.093045	3044.214699	22.490867
91.329205	3018.043501	22.495885
91.513299	3035.040597	22.500903
91.628136	3046.306688	22.505920
91.869851	3043.930900	22.510938
91.474234	3060.318974	22.515955
91.908444	3053.317989	22.520973
91.978674	3054.350672	22.525991
91.986440	3054.349895	22.531008
91.866722	3055.191548	22.536026
91.817846	3083.923338	22.541043
92.342846	3082.880504	22.546061
92.270929	3104.743076	22.551079
92.369438	3098.331540	22.556096
92.237881	3089.045545	22.561114
92.478566	3116.617662	22.566131
93.035868	3114.155271	22.571149
92.825298	3122.847714	22.576167
93.351896	3130.231865	22.581184
93.340328	3121.891078	22.586202
92.903642	3129.696185	22.591219
93.359341	3111.829201	22.596237
93.286475	3124.284704	22.601255
93.440272	3128.189102	22.606272
93.518579	3156.533318	22.611290
93.557386	3151.916675	22.616307
93.672150	3146.391710	22.621325
93.755966	3147.253077	22.626343
93.683500	3141.562025	22.631360
94.042417	3151.694079	22.636378
93.857933	3164.553845	22.641395
94.186941	3160.683257	22.646413
94.136578	3161.369180	22.651431
94.262812	3156.006866	22.656448
94.449295	3163.010665	22.661466
94.544939	3173.059871	22.666483
95.095318	3180.301351	22.671501
94.966546	3193.583584	22.676519
94.950815	3188.519295	22.681536
95.444723	3195.849436	22.686554
95.244746	3196.141424	22.691571
95.394895	3185.003495	22.696589
95.215821	3181.372748	22.701607
95.346255	3175.388144	22.706624
95.605106	3186.923621	22.711642
95.411224	3193.290160	22.716659
95.727251	3177.516637	22.721677
95.889715	3185.674493	22.726695
95.754288	3183.045288	22.731712
95.685717	3180.541439	22.736730
95.533301	3180.849975	22.741747
95.826924	3203.965929	22.746765
95.973887	3213.124488	22.751783
95.901389	3207.161201	22.756800
95.927310	3212.981440	22.761818
96.126731	3233.234752	22.766835
96.443943	3229.383024	22.771853
96.436734	3245.213461	22.776871
96.455337	3252.234215	22.781888
96.694019	3235.965590	22.786906
96.804590	3254.657194	22.791923
96.968113	3250.845028	22.796941
97.248389	3268.354390	22.801959
97.072510	3269.926131	22.806976
97.057694	3276.710906	22.811994
97.132409	3274.301464	22.817011
97.789701	3291.472596	22.822029
97.876051	3304.604625	22.827047
97.808534	3294.441274	22.832064
98.170332	3298.308786	22.837082
98.129185	3302.092700	22.842099
98.296067	3290.959606	22.847117
98.099705	3300.281630	22.852135
97.869376	3303.660822	22.857152
98.262852	3293.498653	22.862170
98.366323	3305.407498	22.867187
98.342099	3293.277141	22.872205
98.248729	3305.700159	22.877223
98.402248	3310.669312	22.882240
98.696447	3330.528189	22.887258
98.582688	3319.306028	22.892275
98.656634	3339.112146	22.897293
99.108243	3336.075902	22.902311
99.069007	3345.415489	22.907328
99.419033	3350.219126	22.912346
98.987351	3363.336813	22.917363
99.160434	3360.033624	22.922381
99.763857	3374.636822	22.927399
99.560652	3377.100016	22.932416
99.727976	3372.796883	22.937434
99.857259	3371.431660	22.942451
100.037400	3359.669414	22.947469
100.216500	3373.722310	22.952487
100.401738	3374.809429	22.957504
100.385534	3366.633435	22.962522
100.341474	3391.574205	22.967539
100.491366	3398.055465	22.972557
100.438111	3401.365658	22.977575
100.662010	3401.763380	22.982592
100.900822	3400.614878	22.987610
100.655789	3405.217279	22.992627
100.964735	3395.881734	22.997645
100.908545	3408.900212	23.002663
101.143160	3425.595519	23.007680
101.141817	3421.534594	23.012698
101.193201	3431.832207	23.017715
101.868001	3429.677489	23.022733
101.670975	3415.279728	23.027751
101.634507	3421.541616	23.032768
102.077491	3416.275679	23.037786
102.167683	3417.051173	23.042803
102.295800	3417.935154	23.047821
102.507563	3410.888490	23.052839
102.070824	3423.683273	23.057856
102.841258	3418.245915	23.062874
102.438160	3409.888180	23.067891
102.651026	3423.658401	23.072909
102.792654	3414.116655	23.077927
102.866673	3416.752532	23.082944
102.816264	3416.068909	23.087962
102.645524	3442.057768	23.092979
102.817834	3423.984322	23.097997
103.133900	3436.717906	23.103015
102.943590	3448.024871	23.108032
103.053307	3433.091606	23.113050
103.060194	3456.908019	23.118067
103.065209	3455.174576	23.123085
103.343500	3457.049406	23.128103
103.147592	3473.010068	23.133120
103.512133	3477.363352	23.138138
103.864964	3501.055943	23.143155
103.871710	3508.180732	23.148173
104.182513	3501.462319	23.153191
103.864960	3508.609203	23.158208
103.862813	3521.714507	23.163226
103.994489	3530.602771	23.168243
104.013588	3529.855299	23.173261
104.432709	3536.197255	23.178279
104.518726	3551.910838	23.183296
105.151037	3562.163920	23.188314
105.373326	3565.649072	23.193331
105.431806	3554.353401	23.198349
105.734274	3564.892859	23.203367
105.374269	3565.069181	23.208384
105.712237	3560.892708	23.213402
105.631326	3568.147945	23.218419
105.982403	3568.669332	23.223437
105.891683	3552.831349	23.228455
105.747280	3561.238520	23.233472
105.861349	3556.299108	23.238490
105.973874	3548.277520	23.243507
105.820533	3556.352727	23.248525
106.110242	3573.467010	23.253543
106.321307	3575.460238	23.258560
106.519597	3587.401070	23.263578
106.377630	3580.474586	23.268595
106.577945	3572.123346	23.273613
106.582504	3587.665795	23.278631
106.609201	3595.183360	23.283648
106.983922	3615.221608	23.288666
106.793494	3612.827581	23.293683
106.854826	3619.697358	23.298701
107.202229	3611.116690	23.303719
107.198340	3628.934617	23.308736
107.389968	3636.776105	23.313754
107.432918	3655.551016	23.318771
107.526779	3643.275685	23.323789
107.587394	3648.999811	23.328807
107.930513	3666.209892	23.333824
108.164085	3658.824103	23.338842
108.117498	3676.108628	23.343859
108.549546	3663.993722	23.348877
108.667242	3663.450999	23.353895
108.324779	3657.452821	23.358912
108.503809	3671.467224	23.363930
108.942794	3665.907987	23.368947
108.881068	3661.157618	23.373965
108.761746	3663.296585	23.378983
108.576779	3677.661670	23.384000
109.148245	3692.572792	23.389018
109.110078	3680.353497	23.394035
109.079740	3684.501833	23.399053
109.399721	3686.537705	23.404071
109.135169	3690.074002	23.409088
109.382760	3715.034814	23.414106
109.343657	3697.855568	23.419123
109.349154	3721.068132	23.424141
109.803983	3708.729954	23.429159
109.594451	3732.723487	23.434176
109.582080	3744.893922	23.439194
109.900638	3746.375743	23.444211
110.237301	3748.336824	23.449229
110.769215	3766.407297	23.454247
110.746186	3781.489174	23.459264
110.853023	3772.999936	23.464282
111.367082	3790.057508	23.469299
111.127219	3768.782290	23.474317
111.298124	3780.917351	23.479335
111.379870	3782.058015	23.484352
111.351586	3782.772795	23.489370
111.390976	3777.758650	23.494387
111.219492	3778.708102	23.499405
111.807006	3765.648984	23.504423
111.800037	3777.607739	23.509440
111.706508	3774.472919	23.514458
112.017931	3783.103099	23.519475
111.758645	3792.370860	23.524493
112.259950	3792.715472	23.529511
112.341214	3796.180873	23.534528
112.219669	3794.189189	23.539546
112.333965	3799.916705	23.544563
112.348416	3812.113861	23.549581
112.625782	3828.012629	23.554599
112.693457	3824.317730	23.559616
113.141040	3826.959269	23.564634
112.951380	3824.187152	23.569651
113.110829	3835.184062	23.574669
113.233560	3839.933487	23.579687
113.155976	3853.465882	23.584704
113.440437	3848.250206	23.589722
113.788320	3847.096641	23.594739
113.461343	3854.619036	23.599757
113.677928	3871.706956	23.604775
113.636457	3886.660888	23.609792
114.043116	3885.125976	23.614810
114.143192	3883.694083	23.619827
113.949834	3877.751885	23.624845
114.288449	3895.106657	23.629863
114.342516	3908.682304	23.634880
114.569799	3898.558225	23.639898
114.950566	3911.857070	23.644915
114.587535	3914.355418	23.649933
114.948783	3919.271350	23.654951
115.397747	3939.605411	23.659968
115.423030	3938.263032	23.664986
115.580225	3923.810990	23.670003
115.385122	3948.100881	23.675021
115.635654	3927.313673	23.680039
115.755448	3934.283963	23.685056
115.560067	3929.010547	23.690074
115.879771	3936.428488	23.695091
115.769772	3949.153769	23.700109
116.184239	3958.923259	23.705127
116.150013	3953.170473	23.710144
116.326436	3964.928016	23.715162
116.425957	3957.002061	23.720179
116.131950	3977.559721	23.725197
116.567224	3984.512155	23.730215
116.531803	3994.125308	23.735232
116.693330	3997.990857	23.740250
117.128030	3982.051247	23.745267
116.839361	4006.959021	23.750285
116.971175	4010.551938	23.755303
117.243559	4009.129354	23.760320
117.154395	4019.312793	23.765338
117.387867	4015.605413	23.770355
117.684990	4036.509547	23.775373
117.798761	4047.503919	23.780391
117.814574	4045.518245	23.785408
117.860267	4035.898863	23.790426
118.211698	4035.602531	23.795443
117.734906	4048.258586	23.800461
117.998580	4051.263608	23.805479
118.498624	4070.291824	23.810496
118.610454	4068.120604	23.815514
118.637406	4080.676913	23.820531
118.602449	4097.881446	23.825549
119.021510	4102.931579	23.830567
118.966001	4096.889750	23.835584
118.883907	4104.811940	23.840602
119.510314	4092.991541	23.845619
119.643840	4136.097861	23.850637
119.739588	4118.899212	23.855655
119.702180	4124.984185	23.860672
119.664231	4128.060715	23.865690
120.347159	4120.718563	23.870707
120.118896	4118.687780	23.875725
120.563756	4117.670134	23.880743
120.596048	4120.541756	23.885760
120.601359	4137.658975	23.890778
121.194688	4140.558759	23.895795
120.667585	4142.986226	23.900813
120.969600	4137.986048	23.905831
120.940156	4140.457262	23.910848
121.001959	4143.272440	23.915866
121.405704	4145.700028	23.920883
121.254119	4144.715190	23.925901
121.345816	4135.410572	23.930919
121.652617	4158.089182	23.935936
121.477437	4172.437557	23.940954
121.657736	4157.598030	23.945971
121.578146	4158.055960	23.950989
121.433258	4184.402408	23.956007
122.137254	4191.402656	23.961024
121.975865	4200.166706	23.966042
122.660197	4204.428973	23.971059
122.515862	4191.498498	23.976077
122.712050	4210.162544	23.981095
122.893531	4209.801776	23.986112
122.852981	4219.051756	23.991130
122.951453	4206.340981	23.996147
123.062056	4226.127809	24.001165
123.230276	4207.741144	24.006183
123.428325	4219.599240	24.011200
123.212426	4232.003287	24.016218
123.786069	4251.029408	24.021235
123.737352	4249.685057	24.026253
123.861189	4242.085243	24.031271
123.893384	4241.595603	24.036288
124.016240	4262.276878	24.041306
124.261827	4259.048131	24.046323
124.275037	4283.655295	24.051341
124.687345	4271.368580	24.056359
124.508909	4272.303855	24.061376
124.383990	4280.991060	24.066394
124.827964	4281.492400	24.071411
124.736178	4306.329147	24.076429
125.104359	4301.568763	24.081447
125.193509	4305.057778	24.086464
125.058806	4311.823448	24.091482
125.273490	4313.631141	24.096499
125.579696	4324.782097	24.101517
125.726017	4327.457363	24.106535
125.863866	4331.007626	24.111552
125.939826	4328.803321	24.116570
126.226704	4333.035632	24.121587
125.627078	4319.640532	24.126605
126.019693	4340.862753	24.131623
126.364454	4351.816025	24.136640
126.141426	4353.324406	24.141658
126.397580	4360.407393	24.146675
126.621941	4377.221759	24.151693
126.614775	4388.681227	24.156711
126.986841	4394.310467	24.161728
126.969351	4382.017125	24.166746
127.036179	4403.060199	24.171763
127.433543	4414.382767	24.176781
127.453872	4414.965530	24.181799
127.838589	4412.115722	24.186816
127.739122	4429.926150	24.191834
128.073562	4433.234903	24.196851
127.894220	4433.943177	24.201869
127.996355	4441.525261	24.206887
128.593223	4433.839712	24.211904
128.300435	4450.286863	24.216922
128.374668	4445.596266	24.221939
128.596578	4466.130346	24.226957
128.380668	4468.174165	24.231975
128.820393	4477.840206	24.236992
128.904413	4494.049948	24.242010
129.411511	4505.471772	24.247027
129.499577	4493.379794	24.252045
129.039691	4513.707702	24.257063
129.431073	4502.360073	24.262080
129.797103	4531.180516	24.267098
129.777703	4529.276187	24.272115
129.966064	4541.629824	24.277133
129.815114	4533.130011	24.282151
130.144246	4546.880054	24.287168
130.235787	4560.626849	24.292186
130.813756	4555.271102	24.297203
130.989999	4551.695097	24.302221
130.919746	4560.807278	24.307239
131.374235	4552.898743	24.312256
131.559329	4550.266932	24.317274
131.666759	4543.450379	24.322291
131.771079	4536.400882	24.327309
131.588933	4538.799361	24.332327
131.679770	4548.829784	24.337344
131.824462	4556.693079	24.342362
132.174779	4572.005763	24.347379
131.973169	4575.822012	24.352397
131.754960	4566.668343	24.357415
132.147741	4567.724995	24.362432
132.139311	4584.128845	24.367450
132.402933	4596.977171	24.372467
132.621800	4608.094338	24.377485
132.289921	4590.131584	24.382503
132.626908	4614.158614	24.387520
132.686872	4626.465818	24.392538
132.953119	4635.177562	24.397555
133.153721	4643.026544	24.402573
133.281937	4647.144608	24.407591
133.081104	4655.843385	24.412608
133.088554	4653.929092	24.417626
133.727442	4662.036369	24.422643
133.654430	4673.095120	24.427661
134.125096	4686.784106	24.432679
133.971325	4690.846021	24.437696
134.209204	4699.000287	24.442714
134.463250	4688.719305	24.447731
134.674996	4694.358610	24.452749
134.889430	4709.326169	24.457767
135.057090	4715.570401	24.462784
135.125221	4723.160605	24.467802
135.050692	4711.154773	24.472819
135.269871	4716.381442	24.477837
135.192299	4707.710748	24.482855
135.501238	4727.508357	24.487872
135.580335	4751.661283	24.492890
135.933959	4748.735843	24.497907
135.958416	4748.329356	24.502925
135.841571	4759.924938	24.507943
135.976551	4763.686404	24.512960
136.122772	4774.501915	24.517978
136.349085	4773.546720	24.522995
136.599409	4771.622203	24.528013
136.511419	4797.555958	24.533031
136.912514	4795.124636	24.538048
136.920492	4801.503949	24.543066
136.881693	4804.266973	24.548083
137.270721	4801.297879	24.553101
137.278449	4827.674924	24.558119
137.586439	4827.064892	24.563136
137.927756	4838.167110	24.568154
137.826464	4824.919544	24.573171
138.099556	4847.837412	24.578189
138.065127	4859.930082	24.583207
138.700124	4847.004935	24.588224
138.638109	4872.022313	24.593242
138.685538	4855.792256	24.598259
138.985090	4863.824607	24.603277
138.606211	4870.637164	24.608295
138.822150	4862.914742	24.613312
139.002507	4880.711340	24.618330
138.909778	4889.260888	24.623347
139.537601	4880.032988	24.628365
139.008108	4903.220167	24.633383
139.602425	4917.323576	24.638400
139.463566	4910.269996	24.643418
139.681737	4920.541039	24.648435
139.978458	4941.000000	24.653453
139.858221	4944.650923	24.658471
140.303391	4945.793436	24.663488
140.364987	4954.516341	24.668506
140.226855	4969.169961	24.673523
140.546195	4974.340010	24.678541
140.615224	4972.597395	24.683559
140.998259	5000.894241	24.688576
141.168919	4996.061166	24.693594
141.570890	4998.858482	24.698611
141.780096	4998.950209	24.703629
141.651090	5004.401440	24.708647
141.936389	5011.225969	24.713664
141.692134	5030.669301	24.718682
141.908302	5029.782303	24.723699
142.044673	5028.573052	24.728717
141.862366	5039.972175	24.733735
142.207027	5040.279320	24.738752
142.417658	5072.668238	24.743770
142.414432	5059.653880	24.748787
142.699962	5079.688881	24.753805
142.483867	5085.334848	24.758823
142.965517	5090.873400	24.763840
143.084385	5106.614628	24.768858
143.095554	5111.828557	24.773875
143.298647	5132.350092	24.778893
143.555930	5133.454765	24.783911
143.966771	5130.000499	24.788928
144.213989	5119.080191	24.793946
143.902881	5153.194497	24.798963
144.420220	5137.685340	24.803981
144.260668	5154.162400	24.808999
144.485636	5139.309439	24.814016
144.761970	5135.638021	24.819034
144.821093	5159.116125	24.824051
145.405060	5165.325611	24.829069
145.227634	5176.022434	24.834087
145.237571	5173.691514	24.839104
145.747193	5178.014029	24.844122
145.830690	5165.999057	24.849139
145.584456	5189.070169	24.854157
145.523193	5203.535319	24.859175
145.749966	5207.484881	24.864192
146.010034	5211.234056	24.869210
146.647922	5226.674680	24.874227
146.604159	5243.017344	24.879245
146.658294	5239.599158	24.884263
146.680943	5245.922685	24.889280
146.699557	5240.971739	24.894298
146.798687	5255.358465	24.899315
147.011665	5270.481534	24.904333
147.415017	5265.466222	24.909351
147.237258	5269.964153	24.914368
147.386469	5282.805179	24.919386
147.507188	5304.998481	24.924403
147.686609	5298.388214	24.929421
147.996553	5312.551964	24.934439
147.978886	5327.320272	24.939456
148.334127	5323.579865	24.944474
148.495288	5327.886768	24.949491
148.807219	5328.515482	24.954509
148.970624	5344.737404	24.959527
149.217094	5345.807265	24.964544
149.084767	5338.893755	24.969562
149.334416	5343.603773	24.974579
149.600960	5342.495435	24.979597
149.535649	5362.772636	24.984615
149.518416	5370.979646	24.989632
149.649451	5366.219542	24.994650
149.913434	5375.054522	24.999667
150.359914	5396.904354	25.004685
150.424130	5406.768069	25.009703
150.425594	5403.875500	25.014720
150.639171	5399.434832	25.019738
150.464698	5419.526986	25.024755
150.928552	5429.732180	25.029773
150.887126	5432.483150	25.034791
150.739621	5450.637343	25.039808
151.204525	5451.435676	25.044826
151.365076	5474.377788	25.049843
151.241872	5468.315113	25.054861
151.893578	5491.881245	25.059879
151.725442	5498.224587	25.064896
151.856368	5499.693095	25.069914
151.763787	5502.265513	25.074931
152.082680	5528.405707	25.079949
152.333757	5544.358221	25.084967
152.223343	5543.002691	25.089984
152.765213	5552.575360	25.095002
153.054894	5560.764436	25.100019
153.420613	5556.159995	25.105037
153.741985	5548.239490	25.110055
153.625568	5556.137379	25.115072
153.909644	5554.478465	25.120090
153.873817	5548.745039	25.125107
154.119434	5551.437971	25.130125
153.815175	5566.376306	25.135143
153.806909	5565.783069	25.140160
154.518982	5574.790594	25.145178
154.457639	5572.303668	25.150195
154.664352	5600.444116	25.155213
154.305041	5619.190223	25.160231
154.795575	5622.008456	25.165248
154.787084	5617.289048	25.170266
154.773507	5647.714919	25.175283
154.891879	5638.058128	25.180301
155.354415	5665.433155	25.185319
155.534829	5674.399444	25.190336
155.818727	5679.714176	25.195354
155.911510	5703.885610	25.200371
156.214330	5695.685797	25.205389
156.122763	5706.927096	25.210407
156.264126	5699.129178	25.215424
156.444835	5727.110755	25.220442
156.404150	5733.203985	25.225459
157.048304	5736.499250	25.230477
157.556303	5762.000679	25.235495
157.263861	5770.669933	25.240512
157.462883	5762.930964	25.245530
157.360767	5758.408096	25.250547
157.553328	5777.367950	25.255565
157.897360	5782.825548	25.260583
157.746696	5795.548818	25.265600
158.397019	5800.191590	25.270618
158.451400	5819.218818	25.275635
158.855967	5819.262130	25.280653
158.940700	5829.471172	25.285671
158.897660	5816.637575	25.290688
159.137284	5829.540496	25.295706
159.202969	5847.392189	25.300723
159.451712	5842.171517	25.305741
159.623669	5854.704511	25.310759
159.444350	5850.540854	25.315776
160.002312	5855.548534	25.320794
159.568762	5882.271160	25.325811
160.057028	5881.688789	25.330829
160.339167	5892.712165	25.335847
160.443992	5900.397280	25.340864
160.682321	5912.233084	25.345882
160.573915	5910.856716	25.350899
161.017797	5931.902946	25.355917
161.401531	5929.541649	25.360935
161.723874	5933.891385	25.365952
161.974757	5949.203748	25.370970
161.851941	5944.772442	25.375987
161.773000	5930.339446	25.381005
161.912942	5948.471132	25.386023
162.138984	5963.611616	25.391040
162.322479	5969.356849	25.396058
162.402461	5969.377016	25.401075
162.240652	5972.020796	25.406093
162.656180	5994.236452	25.411111
162.513989	5999.220485	25.416128
162.992721	6004.321627	25.421146
162.898551	6030.509652	25.426163
163.061836	6028.429667	25.431181
163.402268	6035.688488	25.436199
163.331633	6043.446763	25.441216
163.235717	6040.373300	25.446234
163.639948	6051.951071	25.451251
163.763456	6067.864171	25.456269
163.930858	6088.741711	25.461287
164.329546	6087.344144	25.466304
164.560616	6103.805303	25.471322
165.018836	6119.574955	25.476339
164.809152	6123.280698	25.481357
165.002349	6122.785266	25.486375
165.120839	6146.303869	25.491392
165.320200	6144.605344	25.496410
165.155349	6147.066569	25.501427
165.684722	6177.712450	25.506445
165.501901	6174.217454	25.511463
165.712996	6191.911644	25.516480
166.505726	6200.672723	25.521498
166.248205	6221.658056	25.526515
166.535749	6206.000758	25.531533
166.661319	6216.560424	25.536551
166.734385	6241.263161	25.541568
167.291056	6235.181168	25.546586
167.201171	6247.057282	25.551603
167.413191	6267.341807	25.556621
167.778566	6270.004840	25.561639
167.696144	6278.388861	25.566656
167.838297	6286.000276	25.571674
167.850588	6302.119016	25.576691
168.205062	6298.167463	25.581709
168.547929	6311.006869	25.586727
168.306556	6329.377216	25.591744
168.762179	6319.742242	25.596762
169.110535	6334.477011	25.601779
169.415508	6346.184799	25.606797
169.820785	6365.134632	25.611815
169.744043	6351.669879	25.616832
170.065459	6345.484575	25.621850
170.072580	6361.938517	25.626867
169.853667	6354.891209	25.631885
170.336256	6362.316871	25.636903
169.923305	6389.857907	25.641920
170.370245	6385.887117	25.646938
170.701842	6395.707278	25.651955
171.095775	6414.140882	25.656973
171.524015	6406.440502	25.661991
171.543293	6411.336169	25.667008
171.746910	6393.310019	25.672026
171.927497	6384.331142	25.677044
172.014304	6405.607895	25.682061
172.341420	6408.022523	25.687079
172.153641	6441.703863	25.692096
172.620302	6417.115026	25.697114
172.511608	6423.343396	25.702132
172.809038	6438.192201	25.707149
172.823322	6421.139134	25.712167
172.808275	6451.558545	25.717184
173.093430	6447.674320	25.722202
173.052034	6438.086745	25.727220
172.954367	6467.172843	25.732237
173.492337	6493.286726	25.737255
173.712965	6497.830219	25.742272
173.642795	6506.632856	25.747290
173.682830	6512.624459	25.752308
173.860716	6514.601899	25.757325
174.315407	6535.598334	25.762343
174.164685	6551.737572	25.767360
174.342388	6549.685850	25.772378
174.830546	6580.602748	25.777396
174.616744	6575.372028	25.782413
174.914035	6592.034203	25.787431
174.948233	6603.519963	25.792448
175.247945	6613.004152	25.797466
175.370464	6632.504238	25.802484
175.553816	6645.027715	25.807501
175.931469	6666.926926	25.812519
175.747882	6675.424736	25.817536
176.344807	6679.075298	25.822554
176.578375	6697.842463	25.827572
176.780859	6701.482603	25.832589
177.026159	6705.027075	25.837607
176.971212	6723.627349	25.842624
177.367637	6736.075138	25.847642
177.895452	6731.489249	25.852660
178.054491	6718.793592	25.857677
178.607235	6750.148635	25.862695
178.398809	6760.220478	25.867712
178.495044	6761.153826	25.872730
178.794810	6765.779609	25.877748
178.709773	6753.547928	25.882765
178.946856	6767.951841	25.887783
178.694309	6782.329962	25.892800
179.175695	6789.703265	25.897818
179.036143	6794.655220	25.902836
179.135072	6810.334917	25.907853
179.738856	6818.290450	25.912871
179.425061	6840.108849	25.917888
179.377399	6849.585608	25.922906
179.691030	6855.063964	25.927924
180.181536	6882.926335	25.932941
180.674541	6878.763929	25.937959
180.770946	6902.577120	25.942976
180.832757	6916.582513	25.947994
181.237252	6918.252447	25.953012
181.187568	6922.496191	25.958029
181.612093	6936.258181	25.963047
181.719490	6945.970438	25.968064
181.803341	6956.578054	25.973082
182.158524	6979.836723	25.978100
182.098117	6971.448195	25.983117
182.421923	6986.885766	25.988135
182.663174	7004.553843	25.993152
182.563048	6998.110328	25.998170
182.851336	7021.891602	26.003188
183.013465	7037.387831	26.008205
183.487326	7035.600543	26.013223
183.612393	7041.517267	26.018240
183.768839	7073.601919	26.023258
184.371725	7071.774803	26.028276
184.408632	7081.075106	26.033293
184.275636	7058.856335	26.038311
184.236410	7084.107772	26.043328
184.350182	7099.481324	26.048346
184.824046	7110.139581	26.053364
184.839752	7121.884720	26.058381
185.176285	7127.940578	26.063399
185.583884	7132.582123	26.068416
185.003873	7147.694706	26.073434
185.574421	7156.737566	26.078452
185.991960	7176.955449	26.083469
186.417622	7175.612004	26.088487
186.615671	7201.467832	26.093504
186.581656	7192.337702	26.098522
186.859348	7191.499094	26.103540
187.319617	7189.261604	26.108557
187.327746	7185.842721	26.113575
187.250715	7199.286964	26.118592
187.735998	7214.196033	26.123610
187.508100	7213.864648	26.128628
187.661145	7220.155616	26.133645
188.128721	7217.219956	26.138663
187.981469	7254.889092	26.143680
187.940602	7252.472148	26.148698
188.283157	7263.931069	26.153716
188.483022	7269.806382	26.158733
188.912158	7276.932210	26.163751
188.591183	7289.819104	26.168768
188.777584	7296.151054	26.173786
189.035122	7309.580277	26.178804
189.010384	7324.368962	26.183821
189.146033	7329.416188	26.188839
189.309091	7360.267062	26.193856
189.814031	7377.952238	26.198874
190.279963	7395.865964	26.203892
190.093580	7421.020976	26.208909
190.234191	7422.381751	26.213927
190.812317	7435.447035	26.218944
191.112912	7459.752226	26.223962
191.414550	7465.245380	26.228980
191.074432	7486.867020	26.233997
191.548316	7481.409361	26.239015
191.867780	7492.285550	26.244032
191.790664	7514.791493	26.249050
192.234678	7506.566623	26.254068
192.239736	7524.395986	26.259085
192.533752	7532.027018	26.264103
193.138827	7532.355776	26.269120
193.181505	7558.285114	26.274138
193.582943	7552.026658	26.279156
193.514844	7557.200552	26.284173
193.818967	7585.421798	26.289191
194.279617	7602.101766	26.294208
194.132584	7599.542438	26.299226
194.610054	7602.704599	26.304244
194.575338	7622.557545	26.309261
194.878548	7618.339283	26.314279
195.082650	7628.657357	26.319296
194.967367	7634.316324	26.324314
195.549257	7647.607978	26.329332
195.281723	7656.892769	26.334349
195.320807	7661.621350	26.339367
195.506564	7677.557696	26.344384
195.336955	7693.246416	26.349402
195.987934	7707.648962	26.354420
196.036898	7721.981666	26.359437
196.067116	7731.527599	26.364455
196.573870	7746.495845	26.369472
196.660577	7770.338336	26.374490
197.028099	7768.889467	26.379508
197.192208	7780.927962	26.384525
197.758055	7806.890978	26.389543
197.739882	7813.007284	26.394560
197.989403	7813.234135	26.399578
198.209790	7831.435433	26.404596
198.433079	7845.400798	26.409613
198.569995	7840.720881	26.414631
198.810735	7860.636509	26.419648
199.008119	7857.526435	26.424666
199.221385	7870.242839	26.429684
199.740650	7888.130990	26.434701
199.430608	7896.230582	26.439719
199.796043	7910.078798	26.444736
199.756764	7909.717807	26.449754
200.164871	7918.430398	26.454772
200.269603	7947.678351	26.459789
200.144625	7945.840666	26.464807
200.328818	7952.028336	26.469824
200.520883	7969.904486	26.474842
200.469764	7981.258864	26.479860
200.751809	7997.954586	26.484877
201.235760	8013.187538	26.489895
201.778831	8025.491234	26.494912
201.610419	8035.048905	26.499930
202.242179	8032.813681	26.504948
202.370128	8050.661138	26.509965
202.457585	8059.171615	26.514983
202.630556	8056.196272	26.520000
202.839692	8080.923131	26.525018
203.269514	8084.672127	26.530036
203.712142	8077.953808	26.535053
203.357097	8108.910654	26.540071
203.184378	8102.812215	26.545088
203.517358	8133.933444	26.550106
203.705326	8129.141048	26.555124
203.958552	8159.352472	26.560141
203.970351	8170.798975	26.565159
204.474843	8189.708241	26.570176
204.427555	8215.522788	26.575194
204.942008	8224.131345	26.580212
205.330722	8230.491678	26.585229
205.387794	8257.596426	26.590247
206.052589	8262.456503	26.595264
205.801970	8279.598093	26.600282
205.840587	8278.815470	26.605300
206.019583	8289.694944	26.610317
206.399814	8290.880741	26.615335
206.837758	8310.741517	26.620352
206.685039	8337.204533	26.625370
207.068705	8356.327708	26.630388
207.064006	8363.728909	26.635405
207.375794	8374.154119	26.640423
207.847064	8404.959266	26.645440
208.023018	8398.749548	26.650458
208.573880	8425.772212	26.655476
208.528367	8439.162686	26.660493
208.470269	8453.108925	26.665511
208.917242	8451.637418	26.670528
208.846346	8477.157011	26.675546
209.026692	8483.124214	26.680564
209.501941	8497.535257	26.685581
209.898855	8503.936089	26.690599
210.097776	8505.058924	26.695616
209.681689	8528.909239	26.700634
210.128275	8521.964830	26.705652
210.600346	8558.272246	26.710669
210.786114	8568.473465	26.715687
210.914633	8581.639196	26.720704
210.976613	8597.481147	26.725722
211.209747	8595.438512	26.730740
211.706412	8627.837139	26.735757
211.931774	8626.083256	26.740775
212.542484	8636.172567	26.745792
212.344907	8650.967424	26.750810
212.380811	8668.498423	26.755828
212.501794	8665.318117	26.760845
212.440545	8691.059351	26.765863
212.999141	8697.131111	26.770880
212.932882	8726.313459	26.775898
213.235651	8757.921346	26.780916
213.540108	8744.363996	26.785933
213.788110	8775.970730	26.790951
214.112822	8767.790912	26.795968
214.335208	8792.572618	26.800986
214.273760	8798.506643	26.806004
214.703972	8809.687576	26.811021
214.656937	8816.126444	26.816039
214.752677	8821.193345	26.821056
214.805711	8845.964522	26.826074
215.120693	8852.050602	26.831092
215.603113	8877.486509	26.836109
215.367162	8893.288194	26.841127
216.004869	8907.334887	26.846144
216.234724	8919.368116	26.851162
216.701854	8921.537507	26.856180
216.996209	8949.466669	26.861197
216.853940	8976.681196	26.866215
217.484185	8972.839369	26.871232
217.533153	8994.835906	26.876250
217.527599	8985.818966	26.881268
217.965335	9003.964442	26.886285
217.787238	9011.576534	26.891303
218.174351	9031.899496	26.896320
218.312499	9045.166412	26.901338
218.708506	9069.090506	26.906356
218.843025	9069.184370	26.911373
218.795068	9091.380570	26.916391
219.433142	9103.774957	26.921408
219.431943	9121.351968	26.926426
219.534675	9148.544426	26.931444
220.134895	9165.474723	26.936461
220.066645	9181.872784	26.941479
220.634481	9177.494609	26.946496
220.779087	9214.332574	26.951514
220.887592	9204.372782	26.956532
221.287390	9232.617400	26.961549
221.311472	9250.032064	26.966567
221.819046	9240.735656	26.971584
221.907619	9266.723227	26.976602
222.171979	9275.800577	26.981620
222.474405	9295.346304	26.986637
222.294184	9310.796578	26.991655
222.912637	9308.415309	26.996672
223.243419	9340.377316	27.001690
223.511274	9335.704468	27.006708
223.797631	9356.141372	27.011725
223.334870	9373.099444	27.016743
223.953096	9388.303667	27.021760
223.826964	9392.335442	27.026778
224.232542	9418.537106	27.031796
224.652317	9434.879213	27.036813
224.673120	9448.964517	27.041831
225.259814	9452.105076	27.046848
225.600327	9479.065844	27.051866
225.490953	9474.942041	27.056884
226.173146	9493.620303	27.061901
226.050482	9501.653521	27.066919
226.255956	9508.355765	27.071936
226.572166	9523.147674	27.076954
227.003395	9525.336473	27.081972
227.221277	9541.170151	27.086989
227.154750	9554.315358	27.092007
227.346319	9572.832182	27.097024
227.385980	9577.975542	27.102042
227.316607	9613.784896	27.107060
227.894991	9604.315899	27.112077
227.986261	9636.275542	27.117095
228.115288	9644.382244	27.122112
228.535294	9655.602485	27.127130
228.522862	9678.549777	27.132148
228.833459	9680.307995	27.137165
229.163598	9705.443521	27.142183
229.538453	9707.993739	27.147200
229.529252	9729.077782	27.152218
229.803235	9745.458476	27.157236
230.198610	9751.391420	27.162253
230.228236	9774.772199	27.167271
230.953453	9784.472347	27.172288
231.098285	9790.341155	27.177306
231.063569	9805.078672	27.182324
231.163829	9808.099608	27.187341
231.079047	9839.964300	27.192359
231.564792	9841.443124	27.197376
231.666113	9864.401821	27.202394
231.607959	9900.128839	27.207412
232.314175	9905.111767	27.212429
232.434406	9929.583676	27.217447
232.719337	9939.279472	27.222464
232.940795	9958.643269	27.227482
233.152624	9971.052839	27.232500
233.597826	10002.528619	27.237517
234.012368	10003.215807	27.242535
234.292628	10024.780152	27.247552
234.493974	10036.955995	27.252570
234.441695	10040.956827	27.257588
234.820992	10049.881729	27.262605
235.104695	10079.159977	27.267623
235.229145	10082.719671	27.272640
235.721880	10103.949705	27.277658
235.802722	10116.766201	27.282676
236.187939	10116.086908	27.287693
236.275498	10149.369118	27.292711
236.449900	10162.153651	27.297728
236.961560	10163.334425	27.302746
236.681415	10189.393089	27.307764
237.269008	10195.704820	27.312781
237.234169	10223.714248	27.317799
237.456120	10229.255408	27.322816
237.942729	10247.966877	27.327834
237.979304	10282.049401	27.332852
238.369565	10286.664034	27.337869
238.658238	10299.323462	27.342887
238.808938	10323.445153	27.347904
239.275932	10328.949801	27.352922
239.184344	10352.766563	27.357940
239.638552	10361.205869	27.362957
239.908367	10375.309142	27.367975
239.867273	10398.750571	27.372992
240.065557	10420.683455	27.378010
240.246106	10423.681791	27.383028
240.883070	10449.056094	27.388045
240.893264	10463.100728	27.393063
241.354824	10488.658461	27.398080
241.664457	10499.893599	27.403098
241.915011	10506.474603	27.408116
242.067262	10534.636411	27.413133
242.352227	10528.503164	27.418151
242.895860	10559.475418	27.423168
243.097916	10561.015362	27.428186
243.161886	10562.690761	27.433204
243.787690	10586.635895	27.438221
243.673507	10581.798948	27.443239
243.975420	10608.887743	27.448256
244.050573	10613.890091	27.453274
243.845441	10630.979436	27.458292
244.655471	10645.378879	27.463309
244.640091	10653.480022	27.468327
244.465370	10673.331562	27.473344
244.764694	10692.532938	27.478362
245.125647	10700.559326	27.483380
245.404212	10729.669477	27.488397
245.217091	10744.843435	27.493415
245.649684	10765.469098	27.498432
246.040289	10781.241605	27.503450
246.021617	10811.090252	27.508468
246.281608	10823.175875	27.513485
246.504800	10848.879910	27.518503
246.974223	10868.615029	27.523520
247.322853	10886.379595	27.528538
247.407450	10909.156663	27.533556
248.095400	10918.135039	27.538573
248.127217	10924.956373	27.543591
248.358461	10965.439050	27.548608
248.867814	10962.031067	27.553626
249.244852	11003.479118	27.558644
249.643075	10993.675935	27.563661
249.493173	11000.654146	27.568679
249.825193	11030.985635	27.573696
250.549389	11033.743815	27.578714
250.548711	11063.623045	27.583732
250.722232	11068.347762	27.588749
250.960915	11065.962820	27.593767
250.850819	11102.171379	27.598784
251.462256	11103.238854	27.603802
251.263229	11133.569263	27.608820
251.654317	11132.508494	27.613837
251.921461	11159.149455	27.618855
251.902024	11184.091429	27.623872
252.416695	11199.457871	27.628890
252.486205	11222.753050	27.633908
252.583365	11239.747414	27.638925
253.191279	11268.029801	27.643943
253.449959	11287.864852	27.648960
254.084558	11308.442878	27.653978
254.073275	11315.124195	27.658996
254.275919	11318.507400	27.664013
254.900082	11349.314280	27.669031
255.006401	11370.152178	27.674048
255.578694	11365.586777	27.679066
255.397880	11384.437425	27.684084
255.886396	11399.862735	27.689101
256.080356	11415.768403	27.694119
255.972636	11437.358588	27.699136
256.182804	11453.608218	27.704154
256.652486	11474.268846	27.709172
256.975733	11488.863703	27.714189
257.309448	11512.819891	27.719207
257.422036	11537.729575	27.724224
257.908261	11536.523874	27.729242
257.481161	11568.424940	27.734260
257.861575	11589.465190	27.739277
258.370653	11605.193733	27.744295
258.367413	11631.613897	27.749312
258.692736	11645.303436	27.754330
258.931903	11672.051494	27.759348
259.329105	11676.919042	27.764365
259.702260	11693.161682	27.769383
259.472750	11720.660776	27.774400
259.933322	11741.093233	27.779418
260.044538	11760.582205	27.784436
260.785027	11788.684487	27.789453
261.388236	11805.465867	27.794471
261.283790	11833.744061	27.799488
261.698654	11832.930614	27.804506
262.178375	11855.167160	27.809524
262.394620	11874.990257	27.814541
262.616432	11873.769136	27.819559
262.794006	11877.959326	27.824576
263.381558	11883.676200	27.829594
263.122941	11913.128554	27.834612
263.655302	11901.267093	27.839629
263.832101	11918.126130	27.844647
263.768606	11939.108625	27.849664
263.972475	11943.366174	27.854682
263.846158	11967.907152	27.859700
264.466706	11988.604179	27.864717
264.657594	12008.860174	27.869735
264.677450	12039.875362	27.874752
265.371881	12051.114982	27.879770
265.561908	12077.945886	27.884788
265.384017	12089.000366	27.889805
265.868352	12108.410786	27.894823
266.074456	12147.758348	27.899840
266.418088	12166.454732	27.904858
266.786277	12193.759781	27.909876
267.068581	12215.666282	27.914893
267.086108	12225.467523	27.919911
267.067860	12275.106902	27.924928
267.919555	12272.525973	27.929946
268.258007	12298.599307	27.934964
268.466583	12317.124387	27.939981
268.923799	12333.899721	27.944999
268.970094	12351.674903	27.950016
269.614252	12368.556461	27.955034
269.886984	12384.382328	27.960052
269.967394	12404.423892	27.965069
270.701311	12410.944735	27.970087
270.540563	12438.320257	27.975104
270.874856	12447.395745	27.980122
271.064222	12477.473096	27.985140
271.359969	12500.734331	27.990157
271.473387	12508.759201	27.995175
271.692937	12545.783910	28.000192
271.975186	12543.683824	28.005210
272.141364	12580.162040	28.010228
272.326045	12613.828016	28.015245
272.745118	12621.844197	28.020263
272.966406	12657.197182	28.025280
273.229222	12670.494576	28.030298
273.451544	12703.962300	28.035316
273.569921	12737.520532	28.040333
274.196709	12747.542856	28.045351
274.350881	12773.801816	28.050368
274.819860	12805.985066	28.055386
275.379020	12803.540622	28.060404
275.450276	12835.861331	28.065421
275.865798	12838.095738	28.070439
276.135860	12864.367999	28.075456
275.962179	12885.947394	28.080474
276.372239	12902.685421	28.085492
276.797605	12934.388483	28.090509
276.885540	12951.017491	28.095527
277.016974	12971.182108	28.100544
277.836681	12991.761660	28.105562
278.075229	13013.745019	28.110580
278.359238	13026.394777	28.115597
278.754622	13040.474145	28.120615
278.764860	13073.135505	28.125632
279.103883	13087.681946	28.130650
279.395118	13115.248650	28.135668
279.407467	13137.048172	28.140685
279.968071	13154.151560	28.145703
280.081529	13160.369494	28.150720
280.089489	13185.945821	28.155738
280.643358	13204.637045	28.160756
280.410056	13225.707570	28.165773
281.202057	13251.894234	28.170791
281.332137	13274.275600	28.175808
281.731426	13286.121058	28.180826
281.997452	13298.727520	28.185844
281.995281	13315.069266	28.190861
282.632205	13339.797431	28.195879
282.902842	13358.191346	28.200896
282.998781	13375.950004	28.205914
283.559838	13387.915347	28.210932
283.297572	13418.700911	28.215949
284.106602	13430.441754	28.220967
284.290249	13441.749411	28.225984
284.246184	13468.723730	28.231002
284.755449	13489.562411	28.236020
284.785361	13521.472985	28.241037
285.656730	13526.098895	28.246055
285.751546	13559.450805	28.251072
285.924325	13575.254179	28.256090
286.435901	13593.557349	28.261108
286.556632	13628.674607	28.266125
287.159394	13641.488846	28.271143
287.333595	13658.334382	28.276160
287.333659	13688.851010	28.281178
287.884262	13694.168117	28.286196
287.950393	13725.483804	28.291213
288.700654	13738.813426	28.296231
288.699929	13759.031589	28.301248
288.718642	13779.333229	28.306266
288.914420	13789.032703	28.311284
289.017015	13830.557823	28.316301
289.597256	13850.049838	28.321319
289.680772	13882.005842	28.326336
289.793556	13909.690051	28.331354
290.329468	13934.405092	28.336372
290.215138	13975.080871	28.341389
290.752092	14006.681733	28.346407
291.027423	14027.565273	28.351424
291.708083	14056.167528	28.356442
291.916037	14087.339154	28.361460
292.091301	14117.428986	28.366477
292.598973	14134.971551	28.371495
293.140632	14151.791561	28.376512
293.319598	14187.771006	28.381530
293.714392	14201.363010	28.386548
294.147809	14220.777307	28.391565
294.587502	14250.803218	28.396583
294.756883	14261.711205	28.401600
294.957025	14282.213561	28.406618
295.212738	14290.203204	28.411636
294.962398	14316.622898	28.416653
295.442529	14346.850305	28.421671
295.644615	14367.760568	28.426688
296.108613	14393.376919	28.431706
296.294017	14417.531335	28.436724
296.204653	14448.314714	28.441741
296.702560	14471.891278	28.446759
296.999816	14496.931822	28.451776
297.047320	14527.897591	28.456794
298.073118	14540.206958	28.461812
298.039874	14573.133807	28.466829
298.489562	14613.736918	28.471847
298.817246	14634.989205	28.476864
299.037790	14669.769986	28.481882
299.487614	14679.037230	28.486900
299.583018	14703.848286	28.491917
300.071194	14723.184806	28.496935
300.266982	14741.033258	28.501952
300.643313	14768.256235	28.506970
300.913147	14788.552320	28.511988
300.828460	14800.752250	28.517005
300.942102	14821.561102	28.522023
301.483516	14859.871071	28.527040
301.767613	14870.533601	28.532058
302.112920	14911.558109	28.537076
302.277985	14938.438081	28.542093
302.646446	14958.272130	28.547111
303.303904	14990.650793	28.552128
303.636698	15000.503274	28.557146
304.134021	15026.118273	28.562164
304.257010	15061.508519	28.567181
304.696575	15066.702606	28.572199
304.769889	15089.861713	28.577216
305.097427	15113.431115	28.582234
305.745404	15121.389457	28.587252
305.808628	15156.165755	28.592269
306.513514	15174.983234	28.597287
306.592938	15188.087660	28.602304
306.799790	15205.310765	28.607322
307.139144	15221.681532	28.612340
307.303152	15257.995173	28.617357
307.382479	15268.852531	28.622375
307.732731	15294.738084	28.627392
308.103491	15327.714755	28.632410
308.460281	15348.966322	28.637428
308.804602	15387.833283	28.642445
309.197674	15400.578772	28.647463
309.609086	15432.321348	28.652480
310.032531	15460.045130	28.657498
310.170436	15468.213981	28.662516
310.802092	15490.714107	28.667533
310.857148	15521.901144	28.672551
311.063334	15539.504497	28.677568
311.411727	15571.253029	28.682586
311.621795	15583.773605	28.687604
311.831397	15614.245055	28.692621
312.318247	15637.243645	28.697639
312.830940	15649.829316	28.702656
312.741084	15676.877118	28.707674
313.442808	15708.513966	28.712692
313.546770	15731.709896	28.717709
313.800904	15752.195735	28.722727
314.194628	15786.646151	28.727744
313.681402	15802.406654	28.732762
314.787652	15822.794357	28.737780
315.000862	15855.949413	28.742797
315.313665	15891.976713	28.747815
315.708740	15902.509700	28.752832
315.813871	15938.306658	28.757850
316.332657	15971.857450	28.762868
316.674803	16005.584052	28.767885
317.031889	16014.919390	28.772903
317.355825	16049.413410	28.777920
317.405118	16070.335349	28.782938
317.733064	16100.351628	28.787956
318.375002	16127.277705	28.792973
318.788259	16142.529316	28.797991
319.335355	16176.313817	28.803008
319.611564	16205.683250	28.808026
319.742122	16210.624603	28.813044
319.927404	16244.747960	28.818061
320.130517	16259.998151	28.823079
320.369905	16301.246959	28.828096
320.562100	16315.156304	28.833114
320.932548	16351.844873	28.838132
321.206706	16377.779391	28.843149
321.304419	16385.380121	28.848167
321.728611	16433.577041	28.853184
321.933991	16453.699891	28.858202
322.210375	16472.911164	28.863220
322.709618	16507.999696	28.868237
323.117775	16540.575504	28.873255
323.548831	16557.621164	28.878272
323.918434	16594.163852	28.883290
324.104627	16613.979604	28.888308
324.051091	16646.031450	28.893325
324.541488	16661.795604	28.898343
325.274819	16703.748663	28.903360
325.390921	16717.825368	28.908378
325.557053	16753.508445	28.913396
325.649348	16775.710188	28.918413
325.985488	16810.265263	28.923431
326.942299	16831.083955	28.928448
327.004903	16866.975078	28.933466
327.426397	16890.060308	28.938484
327.694800	16916.426880	28.943501
327.961942	16938.317854	28.948519
328.372718	16965.830380	28.953536
328.271689	17005.324796	28.958554
328.929180	17025.837008	28.963572
329.505795	17050.081999	28.968589
329.390260	17085.205566	28.973607
330.224873	17123.685191	28.978624
330.419426	17156.396804	28.983642
330.763823	17179.094869	28.988660
331.004464	17199.627308	28.993677
331.780624	17238.534508	28.998695
332.067034	17262.701675	29.003712
332.198519	17291.485467	29.008730
332.455649	17317.219404	29.013748
333.131912	17332.948774	29.018765
332.954095	17371.410266	29.023783
333.167211	17391.811953	29.028800
333.767969	17438.267926	29.033818
334.385745	17449.999173	29.038836
334.623626	17486.379641	29.043853
334.494894	17517.539381	29.048871
334.972131	17533.968498	29.053888
334.893161	17585.868994	29.058906
335.552915	17612.414749	29.063924
335.860274	17646.213527	29.068941
336.149724	17685.908276	29.073959
336.656766	17711.642524	29.078976
336.922714	17745.427858	29.083994
337.468830	17768.336133	29.089012
337.430056	17804.526597	29.094029
337.859624	17828.677253	29.099047
338.627832	17850.458299	29.104064
338.730718	17901.182354	29.109082
339.024665	17922.732930	29.114100
339.591519	17944.734922	29.119117
339.765344	17967.348779	29.124135
340.189112	18007.961474	29.129152
340.191503	18038.315637	29.134170
340.841751	18074.027210	29.139188
341.557834	18107.253483	29.144205
341.786265	18122.034698	29.149223
342.494516	18166.654561	29.154240
342.270574	18187.151505	29.159258
342.963869	18219.300549	29.164276
343.116719	18227.386354	29.169293
343.371708	18262.939825	29.174311
343.804466	18277.967976	29.179328
344.066765	18327.680352	29.184346
344.290312	18326.710658	29.189364
344.733877	18354.116073	29.194381
344.865711	18403.629572	29.199399
345.340021	18402.180279	29.204416
345.696961	18436.907146	29.209434
345.805360	18468.108318	29.214452
346.362477	18489.565725	29.219469
346.470160	18518.339836	29.224487
346.994235	18542.431798	29.229504
346.505030	18586.484608	29.234522
347.173979	18620.733179	29.239540
347.723009	18650.299924	29.244557
347.507767	18702.163403	29.249575
348.242158	18722.069246	29.254592
348.580269	18767.287785	29.259610
348.511240	18801.564075	29.264628
349.113640	18843.225853	29.269645
349.384923	18885.889727	29.274663
350.071902	18898.587822	29.279680
350.549314	18944.686992	29.284698
351.053824	18992.536126	29.289716
351.654584	19014.975287	29.294733
351.933336	19045.690733	29.299751
352.690036	19073.031430	29.304768
352.813166	19095.336817	29.309786
352.951511	19128.769356	29.314804
353.492417	19143.364313	29.319821
353.617976	19178.600678	29.324839
354.647764	19200.417541	29.329856
354.893481	19238.548614	29.334874
355.052857	19255.451242	29.339892
355.497585	19279.702404	29.344909
355.607409	19329.359446	29.349927
356.132961	19332.891964	29.354944
356.193653	19355.572127	29.359962
356.709887	19399.579220	29.364980
356.782893	19427.239938	29.369997
356.944649	19455.232814	29.375015
357.480226	19487.025787	29.380032
357.982721	19526.940401	29.385050
358.176941	19557.495799	29.390068
358.727182	19591.994557	29.395085
358.903768	19626.269810	29.400103
359.158792	19659.575385	29.405120
359.889316	19688.135149	29.410138
359.940101	19719.280422	29.415156
360.451598	19755.149393	29.420173
360.500063	19789.490285	29.425191
360.943577	19827.902143	29.430208
361.453924	19868.235573	29.435226
361.346820	19908.765680	29.440244
362.005608	19930.551801	29.445261
362.335939	19985.209050	29.450279
362.920573	20004.993014	29.455296
363.528688	20025.621172	29.460314
364.071896	20054.512012	29.465332
365.200597	20082.773390	29.470349
365.220421	20104.767756	29.475367
365.692986	20111.961498	29.480384
366.039567	20142.328870	29.485402
365.950600	20160.167215	29.490420
366.430668	20184.587261	29.495437
366.403407	20222.656931	29.500455
366.822504	20234.837569	29.505472
367.313676	20274.383845	29.510490
367.567743	20309.639218	29.515508
367.752468	20338.307611	29.520525
368.104942	20368.538860	29.525543
368.133729	20393.085783	29.530560
368.957291	20422.261981	29.535578
369.032303	20450.567219	29.540596
369.618049	20481.002893	29.545613
369.727122	20510.891559	29.550631
369.799067	20545.282155	29.555648
370.578068	20585.921324	29.560666
370.510790	20613.224140	29.565684
371.153035	20661.249235	29.570701
371.514533	20678.138841	29.575719
372.066555	20714.800833	29.580736
372.257814	20748.273611	29.585754
372.560434	20793.356944	29.590772
372.986354	20818.226677	29.595789
373.446854	20856.034359	29.600807
373.576068	20889.754128	29.605824
374.355919	20921.626155	29.610842
374.582841	20963.366334	29.615860
375.024812	20994.272818	29.620877
375.333340	21027.539195	29.625895
375.786004	21074.034596	29.630912
376.467980	21081.224121	29.635930
376.474319	21131.321392	29.640948
377.051760	21157.129783	29.645965
377.122549	21200.627243	29.650983
377.498098	21240.814448	29.656000
378.362760	21264.977076	29.661018
378.329947	21301.554110	29.666036
378.802190	21335.172397	29.671053
378.924170	21377.463780	29.676071
379.225150	21428.886339	29.681088
379.973910	21450.241843	29.686106
380.178767	21497.632213	29.691124
380.795118	21519.618184	29.696141
381.067668	21556.935129	29.701159
381.427379	21600.846224	29.706176
381.821805	21629.220508	29.711194
381.920923	21673.248936	29.716212
382.317423	21705.351321	29.721229
382.298647	21757.081522	29.726247
382.917097	21789.798483	29.731264
383.604760	21829.470490	29.736282
383.703334	21886.146005	29.741300
384.120653	21909.235796	29.746317
384.311725	21953.238734	29.751335
385.145313	22002.016445	29.756352
385.629826	22038.799706	29.761370
386.257690	22080.274654	29.766388
386.255452	22112.539857	29.771405
386.825892	22152.205195	29.776423
387.712289	22194.952521	29.781440
388.531199	22215.833928	29.786458
388.544643	22259.643152	29.791476
388.728702	22267.795141	29.796493
389.409916	22313.601989	29.801511
390.022601	22337.522453	29.806528
390.637882	22349.684848	29.811546
390.829919	22389.842073	29.816564
391.537024	22406.499771	29.821581
391.445532	22439.486630	29.826599
391.455870	22469.152328	29.831616
391.906845	22487.447864	29.836634
392.263920	22526.126168	29.841652
392.495950	22539.559638	29.846669
392.554705	22588.363007	29.851687
393.261954	22620.469419	29.856704
393.575292	22646.981164	29.861722
393.724815	22685.902226	29.866740
394.167543	22719.099354	29.871757
394.618303	22760.417636	29.876775
394.390280	22792.746670	29.881792
395.019348	22827.817714	29.886810
395.290077	22873.523635	29.891828
396.070261	22914.319637	29.896845
396.265422	22949.435813	29.901863
396.532025	23001.237798	29.906880
397.111480	23024.743788	29.911898
397.231269	23085.238331	29.916916
397.863775	23106.969896	29.921933
398.217837	23154.866887	29.926951
398.458433	23197.352956	29.931968
399.039254	23235.095695	29.936986
399.626800	23280.547005	29.942004
400.175514	23309.589205	29.947021
400.475133	23350.678497	29.952039
400.838941	23393.724902	29.957056
401.140449	23434.669038	29.962074
401.463891	23470.181337	29.967092
402.141879	23511.055585	29.972109
402.913061	23550.363133	29.977127
402.823042	23586.383857	29.982144
403.356758	23611.966770	29.987162
403.810710	23664.785161	29.992180
403.915866	23691.701879	29.997197
404.548196	23739.940846	30.002215
404.708001	23777.680249	30.007232
405.417457	23832.725761	30.012250
405.508196	23875.736520	30.017268
405.541476	23918.734807	30.022285
406.190121	23966.708425	30.027303
406.642658	24011.299501	30.032320
407.284474	24057.484981	30.037338
407.640764	24100.923874	30.042356
407.900213	24144.743091	30.047373
408.843173	24193.354594	30.052391
408.883359	24240.109812	30.057408
409.236337	24272.594823	30.062426
409.558351	24320.202425	30.067444
410.430771	24365.466126	30.072461
410.749447	24410.465084	30.077479
411.088806	24456.561293	30.082496
411.983976	24475.036319	30.087514
412.130322	24539.571238	30.092532
412.554574	24555.945113	30.097549
413.291320	24604.367972	30.102567
413.400111	24630.101461	30.107584
413.934956	24671.602906	30.112602
414.171247	24708.666372	30.117620
414.575213	24755.944739	30.122637
415.044313	24776.915510	30.127655
415.168815	24838.123513	30.132672
416.096942	24866.774607	30.137690
416.003370	24911.524493	30.142708
416.451395	24954.207773	30.147725
417.111478	24986.359608	30.152743
417.507039	25029.608342	30.157760
417.858335	25061.634731	30.162778
418.012474	25116.927531	30.167796
418.425976	25146.099299	30.172813
419.001341	25183.273354	30.177831
419.276754	25235.052357	30.182848
419.805852	25271.870011	30.187866
420.457745	25325.398832	30.192884
420.821775	25365.145261	30.197901
421.011580	25402.834452	30.202919
421.371564	25434.812807	30.207936
422.224070	25474.076715	30.212954
422.365348	25513.552810	30.217972
422.891083	25551.967363	30.222989
423.271938	25584.604815	30.228007
423.117512	25635.749629	30.233024
424.030891	25668.920545	30.238042
424.303553	25703.471445	30.243060
424.718680	25753.532279	30.248077
424.951463	25787.309404	30.253095
425.186757	25836.455662	30.258112
425.805513	25876.473425	30.263130
426.236601	25918.337238	30.268148
426.774720	25969.324501	30.273165
427.650408	26000.354616	30.278183
427.853619	26056.413450	30.283200
428.453095	26092.103263	30.288218
428.669446	26138.799919	30.293236
428.955440	26169.301735	30.298253
429.362620	26216.883246	30.303271
429.857034	26259.645720	30.308288
430.356112	26311.643356	30.313306
430.823558	26348.612295	30.318324
431.302030	26388.372173	30.323341
431.882129	26427.714824	30.328359
432.265806	26481.676356	30.333376
432.853082	26510.947916	30.338394
432.942231	26549.047346	30.343412
433.395227	26602.808581	30.348429
433.931395	26632.662790	30.353447
433.832927	26692.171802	30.358464
434.384296	26730.315129	30.363482
434.872466	26778.567639	30.368500
435.378935	26829.140087	30.373517
435.716176	26883.641987	30.378535
436.042251	26924.383914	30.383552
436.428592	26987.748345	30.388570
437.224973	27032.594912	30.393588
437.290697	27081.583534	30.398605
438.354073	27122.352375	30.403623
438.460089	27187.476433	30.408640
439.177800	27231.525956	30.413658
439.603576	27278.459220	30.418676
440.112084	27334.594823	30.423693
440.523304	27361.398987	30.428711
441.008079	27419.778106	30.433728
441.872057	27444.858082	30.438746
442.448514	27476.514344	30.443764
442.506932	27527.467229	30.448781
443.473351	27552.035263	30.453799
443.903710	27598.754176	30.458816
444.225410	27631.288620	30.463834
444.727047	27665.256870	30.468852
444.868360	27697.843316	30.473869
445.467521	27737.463391	30.478887
445.883052	27785.882136	30.483904
446.188996	27828.553508	30.488922
446.522670	27861.010713	30.493940
446.754179	27918.502920	30.498957
447.234364	27958.458566	30.503975
447.477834	28005.660492	30.508992
447.642231	28053.613667	30.514010
448.266722	28104.891100	30.519028
448.741612	28138.653381	30.524045
449.372474	28182.363284	30.529063
449.507595	28239.519225	30.534080
450.208695	28298.427037	30.539098
450.850403	28331.783645	30.544116
450.898691	28379.075612	30.549133
451.618763	28426.187349	30.554151
451.736411	28470.187780	30.559168
452.350051	28505.650041	30.564186
452.871449	28551.268317	30.569204
452.960844	28599.724302	30.574221
453.500392	28642.456888	30.579239
453.740271	28703.265402	30.584256
454.162571	28730.915206	30.589274
454.825775	28786.862831	30.594292
455.015078	28847.434178	30.599309
455.593330	28892.905182	30.604327
456.278832	28953.912236	30.609344
456.639279	28995.861485	30.614362
457.156964	29038.018278	30.619380
457.468574	29084.284549	30.624397
458.019576	29136.056646	30.629415
458.741998	29175.662832	30.634432
459.120124	29235.582954	30.639450
459.597765	29275.614630	30.644468
459.802668	29342.446460	30.649485
460.896472	29383.688808	30.654503
461.127596	29442.599308	30.659520
461.403074	29480.494660	30.664538
461.875042	29522.742204	30.669556
462.362824	29578.907483	30.674573
462.994178	29622.273980	30.679591
463.505163	29677.811181	30.684608
463.576619	29733.799690	30.689626
464.419337	29777.371397	30.694644
464.530537	29832.278006	30.699661
465.339614	29892.148145	30.704679
465.660786	29944.569434	30.709696
465.618856	29996.710179	30.714714
466.676238	30035.821387	30.719732
466.927117	30095.181931	30.724749
468.135215	30159.113127	30.729767
468.526121	30190.915443	30.734784
468.920567	30246.763932	30.739802
469.762793	30290.166671	30.744820
470.029690	30321.907694	30.749837
470.410295	30377.796745	30.754855
471.155858	30418.547050	30.759872
471.244309	30461.740348	30.764890
471.741723	30498.083937	30.769908
471.901848	30550.634605	30.774925
472.483729	30596.295609	30.779943
472.895113	30657.823983	30.784960
472.960739	30705.393891	30.789978
473.618883	30760.500158	30.794996
473.836240	30808.654120	30.800013
474.624640	30874.512185	30.805031
474.908436	30915.346241	30.810048
475.169913	30988.080509	30.815066
476.231580	31040.294462	30.820084
476.228192	31086.624419	30.825101
477.058589	31144.331272	30.830119
477.417444	31206.188882	30.835136
477.825575	31258.760661	30.840154
478.535275	31310.907378	30.845172
479.259482	31356.262948	30.850189
480.093835	31397.452007	30.855207
480.889643	31443.502631	30.860224
480.897196	31494.992975	30.865242
481.162605	31511.596916	30.870260
481.375089	31571.467286	30.875277
482.137012	31613.242981	30.880295
482.577309	31663.611813	30.885312
483.116984	31717.497708	30.890330
483.485937	31761.199977	30.895348
483.997420	31810.652056	30.900365
484.313030	31841.353038	30.905383
485.183724	31896.412019	30.910400
485.203387	31943.462890	30.915418
485.854356	31973.073933	30.920436
486.367136	32027.126122	30.925453
486.705035	32070.578755	30.930471
487.140934	32113.564167	30.935488
487.444909	32182.043677	30.940506
488.274730	32218.335952	30.945524
488.532151	32265.764857	30.950541
488.959766	32318.592154	30.955559
489.372848	32373.939604	30.960576
489.483453	32431.059761	30.965594
490.050829	32490.966150	30.970612
490.440517	32555.388380	30.975629
491.213621	32600.433081	30.980647
491.997226	32663.459265	30.985664
492.104262	32723.593924	30.990682
492.864132	32783.904902	30.995700
492.739001	32839.339567	31.000717
493.478168	32899.373570	31.005735
494.092514	32953.995513	31.010752
494.259853	33013.720521	31.015770
495.384622	33066.753573	31.020788
495.817788	33137.095855	31.025805
496.221880	33182.275570	31.030823
496.992351	33252.931739	31.035840
497.311920	33310.446170	31.040858
498.120184	33363.333630	31.045876
498.874579	33422.234241	31.050893
499.125475	33475.100519	31.055911
499.793556	33517.397922	31.060928
500.214693	33569.539091	31.065946
500.993059	33622.668902	31.070964
501.337424	33671.879344	31.075981
501.853179	33721.023751	31.080999
502.640706	33775.152684	31.086016
502.883634	33830.829413	31.091034
503.403814	33878.231891	31.096052
503.635064	33927.625798	31.101069
504.272454	33988.958174	31.106087
504.618006	34042.457329	31.111104
505.256590	34094.472634	31.116122
505.552569	34149.068840	31.121140
505.790409	34202.870241	31.126157
506.133195	34267.599921	31.131175
506.991345	34321.387569	31.136192
507.333417	34388.162398	31.141210
507.584934	34455.936874	31.146228
508.169848	34515.910369	31.151245
508.715319	34586.889870	31.156263
509.429191	34650.035659	31.161280
509.348554	34714.458279	31.166298
510.327540	34773.032864	31.171316
510.798412	34842.107284	31.176333
511.439822	34904.268867	31.181351
512.090894	34970.818157	31.186368
512.460023	35028.910583	31.191386
513.068568	35087.960750	31.196404
513.863414	35140.038518	31.201421
514.173355	35194.610400	31.206439
514.921129	35249.592907	31.211456
515.460420	35319.102796	31.216474
515.924913	35355.020136	31.221492
516.558361	35421.122804	31.226509
516.554570	35463.116173	31.231527
517.321660	35508.992877	31.236544
517.679002	35570.096157	31.241562
517.801420	35626.464237	31.246580
518.310274	35694.301916	31.251597
518.986118	35748.783510	31.256615
519.605351	35801.911449	31.261632
519.631028	35866.244953	31.266650
520.560538	35918.343785	31.271668
520.889615	35985.511745	31.276685
521.299245	36063.171436	31.281703
522.004398	36110.836493	31.286720
522.643012	36181.302099	31.291738
523.589349	36239.590302	31.296756
524.204493	36291.745308	31.301773
524.249750	36367.345960	31.306791
524.988922	36414.330915	31.311808
524.978936	36484.737605	31.316826
525.745656	36540.033382	31.321844
526.472172	36593.414191	31.326861
526.511061	36673.387740	31.331879
527.153158	36730.131042	31.336896
527.733621	36795.843643	31.341914
528.049692	36866.914319	31.346932
528.780172	36933.972214	31.351949
528.874273	37000.324457	31.356967
529.671145	37078.237017	31.361984
529.857966	37144.486119	31.367002
530.594272	37230.551128	31.372020
531.459823	37296.354177	31.377037
531.642145	37370.065063	31.382055
532.667675	37444.993966	31.387072
533.188599	37497.338468	31.392090
533.776318	37561.686225	31.397108
534.499771	37628.400745	31.402125
535.045860	37690.114424	31.407143
535.485863	37762.588304	31.412160
536.076507	37824.276150	31.417178
536.431578	37888.250090	31.422196
537.071937	37958.883363	31.427213
537.716067	38034.518368	31.432231
538.141971	38103.423491	31.437248
538.845039	38164.598461	31.442266
539.338096	38221.942327	31.447284
539.949788	38276.707323	31.452301
540.542954	38348.031601	31.457319
541.299185	38418.855836	31.462336
541.517098	38482.153920	31.467354
542.119428	38541.042957	31.472372
542.712495	38616.048180	31.477389
543.396837	38668.691015	31.482407
543.851806	38745.070350	31.487424
544.145135	38806.359363	31.492442
544.853015	38866.841602	31.497460
545.437782	38926.135614	31.502477
546.056472	38989.362971	31.507495
546.647581	39053.926965	31.512512
547.258226	39117.676851	31.517530
547.915256	39178.790282	31.522548
548.604878	39240.097371	31.527565
549.217763	39300.786121	31.532583
549.786711	39362.965708	31.537600
550.535608	39420.665646	31.542618
550.823407	39470.046602	31.547636
551.194501	39518.271412	31.552653
551.707953	39582.354606	31.557671
552.284303	39644.047888	31.562688
552.635204	39701.287378	31.567706
553.308969	39764.104360	31.572724
554.330202	39793.468465	31.577741
554.427460	39850.112768	31.582759
554.942439	39908.061207	31.587776
555.505254	39964.853064	31.592794
555.750270	40032.536095	31.597812
556.285876	40078.907766	31.602829
556.968549	40155.438511	31.607847
557.617368	40195.154177	31.612864
557.974449	40259.199310	31.617882
558.430856	40313.159720	31.622900
559.185981	40376.037979	31.627917
559.548038	40442.945698	31.632935
559.973183	40509.417140	31.637952
560.767628	40584.536142	31.642970
561.101094	40655.268523	31.647988
562.007630	40710.405678	31.653005
562.574867	40783.887008	31.658023
563.266979	40831.765589	31.663040
563.625321	40887.205301	31.668058
564.144440	40958.918241	31.673076
564.918006	41027.003760	31.678093
565.283985	41098.543690	31.683111
565.793489	41150.130499	31.688128
566.291819	41218.969235	31.693146
566.761611	41284.672275	31.698164
567.419719	41374.024245	31.703181
567.692980	41436.367090	31.708199
568.297256	41503.977315	31.713216
568.773299	41585.806915	31.718234
569.269614	41666.670796	31.723252
570.259409	41735.187254	31.728269
570.599119	41826.080749	31.733287
571.539250	41891.013847	31.738304
572.167835	41969.635007	31.743322
572.430107	42037.126923	31.748340
573.119415	42101.316206	31.753357
573.586053	42189.583197	31.758375
574.155787	42249.591305	31.763392
574.571694	42326.765515	31.768410
575.159072	42411.544495	31.773428
576.189022	42492.368079	31.778445
576.499973	42555.687074	31.783463
577.110972	42644.352246	31.788480
578.033757	42706.838359	31.793498
578.204616	42786.021594	31.798516
579.100501	42853.130916	31.803533
579.137827	42937.595956	31.808551
579.704854	43004.457098	31.813568
580.443781	43081.322274	31.818586
581.001041	43163.309652	31.823604
582.168814	43231.616062	31.828621
582.549723	43303.954490	31.833639
583.603110	43367.895507	31.838656
583.824743	43443.253444	31.843674
584.737055	43501.356007	31.848692
585.396738	43567.171607	31.853709
585.910063	43653.376496	31.858727
586.487225	43696.442096	31.863744
587.212350	43773.476598	31.868762
587.190171	43835.507028	31.873780
587.697593	43906.993507	31.878797
588.293428	43988.795085	31.883815
588.596627	44059.419320	31.888832
589.383927	44149.429569	31.893850
589.785048	44215.804768	31.898868
590.424876	44291.583266	31.903885
590.880022	44376.872990	31.908903
591.645155	44443.065761	31.913920
591.784697	44512.626435	31.918938
592.331773	44593.633703	31.923956
593.525796	44661.963178	31.928973
593.788892	44758.178133	31.933991
594.530825	44814.118822	31.939008
595.089738	44897.840533	31.944026
595.521601	44959.408258	31.949044
595.842936	45037.607063	31.954061
596.434855	45133.229790	31.959079
597.033858	45198.928619	31.964096
598.135217	45287.266607	31.969114
598.580805	45363.883481	31.974132
599.427500	45435.000948	31.979149
600.382282	45517.990754	31.984167
600.784927	45588.980090	31.989184
601.577203	45648.034279	31.994202
602.068962	45710.535444	31.999220
602.578530	45798.203242	32.004237
603.034237	45861.746437	32.009255
603.610546	45929.077568	32.014272
604.224197	46011.974371	32.019290
604.769361	46107.625611	32.024308
605.802741	46183.874095	32.029325
606.139515	46258.233055	32.034343
606.923407	46346.186480	32.039360
607.302349	46418.085878	32.044378
607.981076	46495.025673	32.049396
608.636451	46562.882779	32.054413
608.997811	46651.990400	32.059431
609.505380	46725.606287	32.064448
610.395872	46808.040968	32.069466
610.872027	46891.510609	32.074484
611.624238	46955.996824	32.079501
612.284272	47052.012813	32.084519
612.428600	47127.313192	32.089536
613.539142	47208.305070	32.094554
614.259543	47285.654859	32.099572
614.815335	47360.300926	32.104589
615.632187	47439.337304	32.109607
615.918708	47536.601523	32.114624
616.712895	47606.315047	32.119642
617.133276	47694.814784	32.124660
617.849305	47760.736951	32.129677
618.495158	47846.765691	32.134695
619.305255	47926.629359	32.139712
620.083290	48006.763900	32.144730
620.607980	48095.131460	32.149748
621.253151	48167.653531	32.154765
621.749484	48249.559691	32.159783
622.155038	48327.429936	32.164800
622.923529	48405.250034	32.169818
623.484939	48479.912245	32.174836
624.101934	48561.228291	32.179853
624.693731	48653.209250	32.184871
624.762578	48741.468817	32.189888
625.685451	48826.651057	32.194906
626.098600	48909.189573	32.199924
627.034267	48997.398749	32.204941
627.386115	49085.790016	32.209959
627.989829	49173.334863	32.214976
628.825701	49261.258602	32.219994
629.496550	49353.163593	32.225012
630.291682	49434.990804	32.230029
630.924211	49512.812652	32.235047
631.446850	49600.347598	32.240064
632.823674	49685.423995	32.245082
633.044769	49770.521122	32.250100
633.662064	49829.364725	32.255117
634.380277	49902.816122	32.260135
634.492132	49971.681589	32.265152
635.387744	50039.539959	32.270170
635.728925	50130.047349	32.275188
636.268353	50208.010582	32.280205
636.698869	50290.520657	32.285223
637.363753	50381.117888	32.290240
637.735020	50462.207922	32.295258
638.362140	50557.391334	32.300276
638.850544	50644.999900	32.305293
639.592870	50730.274189	32.310311
639.734729	50843.764273	32.315328
640.777809	50926.952818	32.320346
641.444711	51025.239544	32.325364
642.040624	51126.611342	32.330381
642.998330	51228.937687	32.335399
643.698492	51321.646345	32.340416
644.241035	51411.573878	32.345434
644.477615	51524.600738	32.350452
645.644363	51602.545015	32.355469
646.182075	51712.125034	32.360487
646.655224	51798.086498	32.365504
647.812803	51890.908702	32.370522
648.287666	51987.722444	32.375540
649.145102	52091.784889	32.380557
649.799225	52161.490897	32.385575
650.004852	52264.149105	32.390592
651.140395	52351.674392	32.395610
651.757833	52462.256183	32.400628
652.611316	52545.937871	32.405645
653.638530	52640.335976	32.410663
653.792846	52728.261904	32.415680
654.442812	52808.456755	32.420698
655.193312	52905.144314	32.425716
655.709023	53002.989213	32.430733
656.589878	53098.197021	32.435751
657.063177	53192.465060	32.440768
658.118170	53277.143140	32.445786
658.776676	53383.311053	32.450804
659.157391	53452.571004	32.455821
659.939484	53553.432121	32.460839
660.451630	53643.744647	32.465856
660.912744	53748.652168	32.470874
661.757273	53847.419867	32.475892
662.444783	53933.030113	32.480909
662.978134	54026.430005	32.485927
663.556011	54120.859015	32.490944
664.559735	54218.477851	32.495962
665.018422	54307.879982	32.500980
665.985554	54407.508386	32.505997
666.478292	54501.814329	32.511015
667.452598	54593.305781	32.516032
667.842625	54672.815311	32.521050
668.660298	54785.768439	32.526068
669.411444	54859.824016	32.531085
669.857340	54961.430256	32.536103
670.491029	55054.711119	32.541120
671.155417	55148.050535	32.546138
671.801570	55242.619017	32.551156
672.532301	55326.345624	32.556173
673.409393	55427.245001	32.561191
673.873511	55517.744737	32.566208
674.608944	55612.925717	32.571226
675.475403	55711.869837	32.576244
676.059886	55800.045033	32.581261
676.427765	55887.542489	32.586279
677.097176	56003.079528	32.591296
677.592333	56081.775069	32.596314
677.953242	56174.398727	32.601332
678.425508	56268.419641	32.606349
679.547351	56355.737810	32.611367
679.944348	56464.107480	32.616384
680.601926	56543.504616	32.621402
681.077859	56655.027615	32.626420
681.542671	56745.153821	32.631437
682.391484	56852.010496	32.636455
683.062871	56958.353695	32.641472
684.140212	57062.419072	32.646490
684.577873	57164.891047	32.651508
685.261030	57271.341401	32.656525
686.342755	57365.747096	32.661543
686.878542	57485.838787	32.666560
687.680130	57574.990701	32.671578
688.719139	57670.125197	32.676596
689.253333	57779.679931	32.681613
689.766784	57871.054292	32.686631
690.076498	57985.436596	32.691648
691.090356	58081.733504	32.696666
691.598478	58188.552587	32.701684
692.523900	58298.500517	32.706701
693.609907	58401.061386	32.711719
693.994597	58506.051219	32.716736
694.980824	58614.802962	32.721754
695.446073	58717.139411	32.726772
695.762170	58831.955214	32.731789
696.795531	58917.005640	32.736807
697.319334	59051.155378	32.741824
698.206698	59141.513385	32.746842
698.570651	59254.895672	32.751860
699.511716	59371.298510	32.756877
700.419690	59462.141124	32.761895
700.890052	59582.047783	32.766912
701.510477	59682.986037	32.771930
702.238437	59798.661966	32.776948
702.950615	59909.285921	32.781965
703.462519	60016.202657	32.786983
704.083717	60129.111408	32.792000
704.961272	60256.480955	32.797018
706.005114	60360.480697	32.802036
706.462247	60479.491275	32.807053
707.358996	60575.080237	32.812071
707.986664	60695.498410	32.817088
709.004774	60801.381526	32.822106
709.528892	60908.073508	32.827124
710.116139	61039.009543	32.832141
710.743537	61127.201343	32.837159
711.037548	61249.927663	32.842176
712.151583	61367.368900	32.847194
713.138187	61480.054282	32.852212
713.830473	61581.040781	32.857229
714.988346	61701.724999	32.862247
715.305765	61803.084178	32.867264
715.838422	61923.765539	32.872282
716.454811	62033.797686	32.877300
717.608119	62142.060708	32.882317
718.240785	62250.972751	32.887335
718.815573	62364.824408	32.892352
719.575008	62466.240315	32.897370
720.520719	62575.165606	32.902388
720.961328	62691.594498	32.907405
721.851529	62802.678957	32.912423
722.592006	62915.874353	32.917440
723.253896	63013.997428	32.922458
724.251826	63113.955183	32.927476
724.560545	63221.326961	32.932493
725.463086	63324.954526	32.937511
726.145278	63432.038216	32.942528
726.846645	63521.119387	32.947546
727.395315	63640.177711	32.952564
728.109060	63727.481756	32.957581
728.577949	63835.196896	32.962599
729.804004	63931.031769	32.967616
730.425690	64041.453144	32.972634
731.121581	64151.989270	32.977652
732.042490	64260.504222	32.982669
732.839926	64349.750122	32.987687
733.294193	64468.436999	32.992704
734.225838	64559.425067	32.997722
734.985722	64669.725887	33.002740
735.593505	64776.430726	33.007757
736.686649	64897.947340	33.012775
737.095811	64986.855618	33.017792
737.324158	65107.504981	33.022810
738.239207	65209.907515	33.027828
738.716982	65333.829073	33.032845
739.387076	65456.455459	33.037863
740.228490	65581.911300	33.042880
740.370848	65695.973051	33.047898
741.410385	65821.277537	33.052916
742.027790	65958.434732	33.057933
743.333285	66061.990654	33.062951
743.692852	66201.897424	33.067968
744.330293	66319.439599	33.072986
745.610108	66461.294750	33.078004
746.341673	66565.921428	33.083021
747.361872	66682.163518	33.088039
748.000281	66803.387204	33.093056
748.682647	66914.850670	33.098074
749.524448	67053.571028	33.103092
750.088562	67166.977047	33.108109
751.235604	67289.447058	33.113127
752.020604	67410.340339	33.118144
752.516130	67524.891167	33.123162
753.446843	67642.449312	33.128180
753.565534	67775.585628	33.133197
754.246955	67890.442810	33.138215
755.278626	68020.288124	33.143232
755.585065	68154.603277	33.148250
756.496448	68273.780189	33.153268
757.412227	68405.518248	33.158285
758.477021	68545.735258	33.163303
759.155401	68669.877537	33.168320
759.794602	68815.761404	33.173338
760.800637	68925.905182	33.178356
761.233521	69071.047310	33.183373
762.051345	69198.653059	33.188391
762.781846	69326.153888	33.193408
763.276099	69462.867734	33.198426
764.678481	69574.902974	33.203444
765.578832	69711.039290	33.208461
766.681604	69818.143503	33.213479
767.662521	69934.549298	33.218496
768.324239	70067.351300	33.223514
769.178689	70173.790245	33.228532
769.569021	70302.744056	33.233549
770.639223	70411.841859	33.238567
771.725942	70524.427422	33.243584
772.054331	70657.092188	33.248602
773.037787	70758.815265	33.253620
773.546308	70897.666710	33.258637
773.947672	71004.159370	33.263655
774.764408	71129.519874	33.268672
775.178660	71271.575879	33.273690
776.290988	71378.079467	33.278708
776.528176	71489.931614	33.283725
777.369855	71611.149534	33.288743
778.136687	71740.890843	33.293760
778.486037	71879.933067	33.298778
779.854716	72003.532066	33.303796
780.516325	72125.376993	33.308813
781.161905	72237.563969	33.313831
782.043687	72365.159306	33.318848
782.676400	72505.979810	33.323866
783.615243	72631.366942	33.328884
784.021912	72758.372852	33.333901
784.922459	72886.707998	33.338919
785.744585	73021.771960	33.343936
786.433090	73170.327063	33.348954
787.328297	73288.200751	33.353972
788.039707	73431.050402	33.358989
788.633702	73568.918717	33.364007
789.470220	73704.149006	33.369024
790.183659	73864.921359	33.374042
791.120697	73982.867834	33.379060
792.077641	74127.515342	33.384077
792.720114	74267.390969	33.389095
793.570203	74414.125809	33.394112
794.352479	74558.394025	33.399130
795.281239	74693.729121	33.404148
795.992166	74836.411117	33.409165
796.728161	74992.685749	33.414183
797.771923	75130.129333	33.419200
798.289160	75278.499603	33.424218
799.337704	75416.722035	33.429236
799.734793	75556.235474	33.434253
801.084025	75693.417179	33.439271
802.270972	75833.541864	33.444288
802.955402	75976.703708	33.449306
803.880828	76103.719542	33.454324
804.791449	76242.924927	33.459341
805.335888	76386.637475	33.464359
806.320421	76521.019829	33.469376
807.452702	76650.496386	33.474394
808.488691	76782.854459	33.479412
808.854692	76928.990578	33.484429
809.551091	77073.928425	33.489447
811.009152	77214.048838	33.494464
811.163645	77343.665662	33.499482
812.072646	77483.473706	33.504500
812.616019	77621.477314	33.509517
813.288680	77761.085825	33.514535
814.149943	77906.773536	33.519552
814.956698	78059.934163	33.524570
815.706064	78195.782319	33.529588
816.279831	78338.693278	33.534605
817.134849	78478.813822	33.539623
818.061563	78627.240393	33.544640
818.808739	78779.726467	33.549658
819.828583	78922.093190	33.554676
820.639307	79076.657997	33.559693
821.276741	79229.494185	33.564711
822.457000	79347.321977	33.569728
823.021356	79508.540004	33.574746
823.822381	79654.280815	33.579764
824.895517	79806.460810	33.584781
826.002275	79947.915294	33.589799
827.014097	80076.242771	33.594816
827.432664	80230.595739	33.599834
828.437893	80360.918369	33.604852
829.296074	80497.477418	33.609869
830.012458	80652.176292	33.614887
830.890867	80766.911468	33.619904
831.736297	80898.142841	33.624922
832.449659	81024.279560	33.629940
833.004314	81167.901347	33.634957
833.667823	81301.341068	33.639975
834.344521	81433.223335	33.644992
835.154556	81586.717687	33.650010
836.416374	81722.268732	33.655028
836.878206	81875.835208	33.660045
837.693137	82040.034798	33.665063
838.807788	82154.617881	33.670080
839.464265	82303.240067	33.675098
840.874207	82445.103077	33.680116
841.500572	82589.702603	33.685133
841.847177	82746.146979	33.690151
842.940787	82884.168253	33.695168
843.759708	83039.651045	33.700186
844.534182	83191.675603	33.705204
845.396082	83342.611320	33.710221
846.028981	83490.637906	33.715239
847.110730	83650.041609	33.720256
847.572854	83798.256551	33.725274
848.518417	83938.769568	33.730292
849.741482	84106.775746	33.735309
850.378255	84266.105412	33.740327
851.336834	84418.645514	33.745344
852.212280	84583.884740	33.750362
853.002872	84738.795479	33.755380
853.673109	84891.183903	33.760397
854.711190	85058.841723	33.765415
855.618080	85198.419907	33.770432
856.717528	85360.034277	33.775450
857.495784	85520.216062	33.780468
858.271880	85665.253263	33.785485
859.173432	85841.151367	33.790503
860.169846	85985.641746	33.795520
861.059640	86155.502140	33.800538
861.677261	86306.118158	33.805556
862.904514	86470.832043	33.810573
863.339766	86621.233480	33.815591
864.098052	86781.927165	33.820608
865.028607	86949.508958	33.825626
866.022899	87120.668890	33.830644
867.177001	87263.445575	33.835661
867.812741	87444.493104	33.840679
869.087334	87598.925571	33.845696
869.736529	87759.599756	33.850714
870.782216	87924.081884	33.855732
871.564145	88069.683675	33.860749
872.394225	88248.731248	33.865767
873.303445	88388.473845	33.870784
874.479250	88553.894373	33.875802
875.208959	88707.664866	33.880820
876.256843	88862.788549	33.885837
877.009826	89014.159075	33.890855
878.608176	89168.497860	33.895872
879.367489	89329.044435	33.900890
879.930758	89471.280444	33.905908
880.841849	89627.488501	33.910925
881.430734	89782.681400	33.915943
882.318095	89929.511268	33.920960
883.188800	90100.302131	33.925978
883.891856	90271.450964	33.930996
884.605799	90405.757835	33.936013
885.520496	90572.412694	33.941031
886.184258	90739.818901	33.946048
887.062038	90916.594502	33.951066
887.866989	91071.038787	33.956084
888.845997	91224.094780	33.961101
889.505486	91375.565509	33.966119
890.619969	91524.006782	33.971136
891.321463	91698.861883	33.976154
892.019559	91862.365773	33.981172
892.941260	92015.436322	33.986189
893.844638	92192.432348	33.991207
894.400066	92344.559263	33.996224
895.313326	92514.449167	34.001242
895.831961	92696.530967	34.006260
896.911226	92869.560267	34.011277
897.734328	93050.436348	34.016295
898.608634	93230.343374	34.021312
899.637923	93412.137442	34.026330
900.557711	93588.375288	34.031348
901.567997	93752.346834	34.036365
902.113594	93936.566397	34.041383
903.388529	94103.756017	34.046400
904.402766	94287.894554	34.051418
905.567026	94461.737704	34.056436
906.375474	94642.457267	34.061453
907.173621	94818.920377	34.066471
907.949717	94990.976980	34.071488
909.159204	95191.216872	34.076506
910.459450	95347.556287	34.081524
911.642737	95519.087362	34.086541
912.418327	95702.687411	34.091559
913.669520	95858.063483	34.096576
914.649027	96039.480405	34.101594
915.820347	96201.467129	34.106612
916.824342	96354.779458	34.111629
917.428519	96531.116094	34.116647
918.651007	96704.725120	34.121664
919.711595	96863.038009	34.126682
920.737752	97015.990024	34.131700
921.764209	97173.145884	34.136717
922.475489	97346.641299	34.141735
923.660567	97489.239821	34.146752
924.449203	97649.488957	34.151770
925.074366	97812.513299	34.156788
926.186662	97976.141921	34.161805
926.952486	98135.872592	34.166823
928.131386	98305.518538	34.171840
929.407313	98449.747081	34.176858
929.846121	98623.391393	34.181876
931.269748	98771.629698	34.186893
931.625545	98945.068408	34.191911
932.444491	99098.491639	34.196928
933.608263	99271.811884	34.201946
934.536791	99446.362272	34.206964
935.208793	99619.519244	34.211981
935.886935	99781.294343	34.216999
936.727414	99957.673334	34.222016
937.826030	100135.030156	34.227034
938.893389	100302.853284	34.232052
939.949152	100467.659766	34.237069
940.258230	100645.960868	34.242087
941.091582	100825.803653	34.247104
942.218195	101008.562075	34.252122
942.817568	101193.156160	34.257140
943.890092	101377.255642	34.262157
944.415319	101566.156976	34.267175
945.421729	101751.941445	34.272192
946.854315	101938.612887	34.277210
947.925903	102137.564113	34.282228
948.882564	102303.297938	34.287245
949.497887	102492.545834	34.292263
950.420387	102677.432924	34.297280
951.544697	102850.967908	34.302298
952.366453	103026.681311	34.307316
953.489823	103205.511754	34.312333
953.955255	103375.657903	34.317351
954.825037	103555.577325	34.322368
955.773237	103726.747753	34.327386
956.370254	103913.242376	34.332404
957.534158	104083.531159	34.337421
958.466001	104270.935482	34.342439
959.182431	104478.922665	34.347456
959.966668	104668.025780	34.352474
960.988922	104854.501334	34.357492
961.876126	105065.086353	34.362509
962.819460	105259.574812	34.367527
963.857140	105463.673503	34.372544
964.718934	105661.243034	34.377562
965.493957	105880.147928	34.382580
967.135678	106063.370282	34.387597
968.151866	106267.453506	34.392615
968.744455	106457.456126	34.397632
970.323783	106664.723154	34.402650
971.239284	106874.532971	34.407668
972.332698	107047.271736	34.412685
973.302264	107262.648066	34.417703
974.507132	107455.013750	34.422720
975.293848	107653.161649	34.427738
976.081751	107859.137675	34.432756
977.329918	108051.513236	34.437773
978.385920	108258.397984	34.442791
979.179855	108456.386081	34.447808
980.532378	108652.472321	34.452826
980.975019	108861.388152	34.457844
982.154893	109050.995902	34.462861
983.519286	109258.964767	34.467879
984.256189	109471.332476	34.472896
985.246626	109666.118102	34.477914
985.686912	109874.700305	34.482932
986.989349	110079.582698	34.487949
988.255957	110287.778385	34.492967
988.952148	110487.469630	34.497984
990.159977	110683.088063	34.503002
991.024153	110892.773494	34.508020
992.234596	111089.990403	34.513037
993.301991	111304.800685	34.518055
994.171295	111514.363446	34.523072
995.313979	111723.363368	34.528090
995.967882	111935.548945	34.533108
996.981769	112145.282726	34.538125
998.333690	112352.960950	34.543143
999.168713	112574.343130	34.548160
1000.557441	112780.245164	34.553178
1001.292385	112988.511452	34.558196
1002.269055	113195.840045	34.563213
1003.245545	113394.391740	34.568231
1004.011531	113598.946014	34.573248
1005.145360	113814.588556	34.578266
1005.727197	114032.363421	34.583284
1006.951534	114245.764897	34.588301
1007.918922	114457.677636	34.593319
1008.806476	114664.107284	34.598336
1009.955650	114894.247923	34.603354
1010.580369	115114.519871	34.608372
1011.707228	115329.820717	34.613389
1012.878118	115550.588705	34.618407
1014.192158	115751.419974	34.623424
1015.517784	115961.498834	34.628442
1015.938079	116195.887891	34.633460
1017.463806	116414.425144	34.638477
1018.525674	116615.050897	34.643495
1019.159697	116816.559537	34.648512
1020.346144	117011.846609	34.653530
1021.384142	117225.656485	34.658548
1022.197038	117404.360716	34.663565
1023.255000	117615.611081	34.668583
1024.352120	117813.414328	34.673600
1025.553222	118026.658580	34.678618
1026.378335	118230.274276	34.683636
1027.182698	118445.208891	34.688653
1028.701661	118651.639770	34.693671
1029.666912	118843.124432	34.698688
1030.954390	119048.025348	34.703706
1032.239276	119259.516593	34.708724
1032.971988	119458.278385	34.713741
1034.038519	119653.058683	34.718759
1034.941350	119874.614369	34.723776
1035.695926	120087.428318	34.728794
1036.709790	120294.030503	34.733812
1037.598893	120532.001848	34.738829
1038.668074	120742.551358	34.743847
1039.612674	120971.204208	34.748864
1040.439431	121197.965018	34.753882
1041.101767	121419.534298	34.758900
1041.687828	121643.031202	34.763917
1042.762221	121889.282716	34.768935
1044.075737	122131.188596	34.773952
1045.307357	122356.358401	34.778970
1045.943643	122601.155027	34.783988
1047.307148	122841.474615	34.789005
1048.641348	123077.530646	34.794023
1049.522476	123306.453109	34.799040
1050.600854	123560.878725	34.804058
1051.690593	123787.514897	34.809076
1052.916765	124036.762716	34.814093
1054.098858	124272.283212	34.819111
1054.885004	124509.619733	34.824128
1056.055417	124757.248104	34.829146
1056.912700	124999.595095	34.834164
1058.393407	125235.111968	34.839181
1059.649121	125478.030717	34.844199
1060.475500	125706.435872	34.849216
1061.727439	125957.507791	34.854234
1062.651409	126206.354810	34.859252
1063.979115	126441.082708	34.864269
1065.035003	126690.051367	34.869287
1065.820915	126921.906920	34.874304
1067.014927	127159.830840	34.879322
1068.440935	127408.997809	34.884340
1069.595329	127630.215547	34.889357
1070.963949	127874.364381	34.894375
1071.847370	128105.731311	34.899392
1072.994883	128333.647112	34.904410
1074.405582	128567.997610	34.909428
1075.413498	128806.586196	34.914445
1076.561265	129041.782208	34.919463
1077.448240	129258.353779	34.924480
1078.382948	129492.942035	34.929498
1079.327181	129733.322770	34.934516
1080.236546	129976.486883	34.939533
1081.328087	130204.438516	34.944551
1082.271749	130454.381709	34.949568
1083.486568	130691.962130	34.954586
1084.417869	130945.333555	34.959604
1085.342362	131183.599418	34.964621
1086.292164	131428.935701	34.969639
1087.226738	131679.143752	34.974656
1088.875530	131900.906339	34.979674
1089.785382	132155.305169	34.984692
1090.713449	132367.353835	34.989709
1092.228378	132603.302143	34.994727
1092.778079	132827.699129	34.999744
1094.042805	133065.859767	35.004762
1094.922879	133308.788487	35.009780
1096.110348	133549.868325	35.014797
1097.278728	133773.992431	35.019815
1098.073986	134037.070494	35.024832
1099.254063	134267.407522	35.029850
1100.041711	134522.618828	35.034868
1101.292630	134763.025530	35.039885
1102.798913	135015.536123	35.044903
1103.297455	135264.323294	35.049920
1104.699267	135507.867184	35.054938
1105.739042	135767.851306	35.059956
1106.790110	136022.371846	35.064973
1107.542716	136276.106966	35.069991
1108.576836	136539.077353	35.075008
1109.844721	136804.927074	35.080026
1111.144187	137058.730164	35.085044
1111.900195	137330.056591	35.090061
1113.407161	137579.620528	35.095079
1114.374422	137845.908684	35.100096
1115.724369	138102.728852	35.105114
1116.897738	138376.036176	35.110132
1117.863021	138637.095065	35.115149
1119.046699	138909.175331	35.120167
1120.251316	139159.574529	35.125184
1121.415160	139426.591011	35.130202
1122.803407	139694.092412	35.135220
1123.829382	139955.861656	35.140237
1125.312462	140206.019905	35.145255
1126.234607	140477.484199	35.150272
1127.191830	140728.227627	35.155290
1128.632947	140996.440733	35.160308
1129.906880	141260.550197	35.165325
1131.160643	141514.952820	35.170343
1132.097340	141787.541037	35.175360
1133.317390	142061.276532	35.180378
1134.578164	142301.812681	35.185396
1135.702245	142584.722798	35.190413
1137.182317	142844.283960	35.195431
1137.756992	143105.137725	35.200448
1139.103371	143367.387670	35.205466
1140.342102	143621.580262	35.210484
1141.903213	143869.901379	35.215501
1143.037522	144135.400231	35.220519
1143.862230	144391.606900	35.225536
1145.117356	144654.490343	35.230554
1146.561883	144915.810181	35.235572
1147.382191	145196.052906	35.240589
1148.530236	145446.266807	35.245607
1149.555993	145699.596776	35.250624
1150.742288	145971.339953	35.255642
1151.386460	146225.472191	35.260660
1152.519027	146511.228113	35.265677
1153.981058	146778.810682	35.270695
1154.823279	147039.890690	35.275712
1155.960730	147323.268301	35.280730
1157.425434	147592.073970	35.285748
1158.505987	147864.977787	35.290765
1159.381454	148129.344799	35.295783
1160.571742	148405.924966	35.300800
1161.884210	148669.006383	35.305818
1163.066395	148945.617405	35.310836
1164.279276	149241.070872	35.315853
1165.799878	149483.426919	35.320871
1166.966947	149744.143265	35.325888
1167.750057	149986.231260	35.330906
1169.137521	150244.467144	35.335924
1169.845190	150514.992175	35.340941
1171.359029	150756.609554	35.345959
1172.265566	151030.542521	35.350976
1173.261663	151293.606374	35.355994
1174.649075	151556.341175	35.361012
1175.555979	151836.253653	35.366029
1177.185859	152089.097637	35.371047
1177.906040	152362.246849	35.376064
1178.594005	152627.704723	35.381082
1180.038990	152914.626375	35.386100
1181.308622	153197.457094	35.391117
1182.572495	153478.274233	35.396135
1183.713933	153750.349374	35.401152
1184.468362	154044.394947	35.406170
1185.600712	154322.157967	35.411188
1186.735496	154612.542999	35.416205
1188.180919	154914.827207	35.421223
1189.112704	155202.624684	35.426240
1190.102400	155505.686416	35.431258
1191.620863	155786.148826	35.436276
1192.384562	156106.604581	35.441293
1193.605510	156394.414003	35.446311
1195.014160	156703.555261	35.451328
1196.003351	157009.457544	35.456346
1197.491148	157308.785373	35.461364
1198.613162	157611.207541	35.466381
1199.860411	157925.167308	35.471399
1201.041074	158224.743120	35.476416
1202.218725	158530.905268	35.481434
1203.685698	158838.442777	35.486452
1204.899649	159138.616240	35.491469
1205.916991	159451.116553	35.496487
1207.256282	159759.963503	35.501504
1208.732213	160066.215118	35.506522
1210.121396	160385.739921	35.511540
1210.993623	160691.918362	35.516557
1212.631790	160991.845431	35.521575
1213.687626	161318.295703	35.526592
1215.057787	161623.523680	35.531610
1216.515177	161913.833321	35.536628
1217.451257	162231.405012	35.541645
1218.821345	162539.291281	35.546663
1220.104739	162845.100905	35.551680
1220.951558	163151.822173	35.556698
1222.322688	163455.211400	35.561716
1223.546546	163775.399003	35.566733
1225.069388	164074.276615	35.571751
1226.219167	164377.544182	35.576768
1227.655504	164694.151436	35.581786
1229.267322	164987.324424	35.586804
1230.152959	165295.146140	35.591821
1231.826880	165594.402950	35.596839
1232.886030	165899.447286	35.601856
1233.779267	166209.202867	35.606874
1235.578484	166503.218167	35.611892
1236.934697	166795.062898	35.616909
1238.643528	167085.874461	35.621927
1240.015984	167374.675398	35.626944
1241.218830	167666.234160	35.631962
1242.318539	167949.932677	35.636980
1243.728070	168250.152512	35.641997
1244.858961	168538.595056	35.647015
1246.463530	168804.503169	35.652032
1247.068782	169104.950443	35.657050
1248.531719	169381.987700	35.662068
1249.294341	169676.347850	35.667085
1250.607052	169957.372314	35.672103
1251.809172	170219.498068	35.677120
1252.374912	170509.341021	35.682138
1253.849362	170792.551898	35.687156
1255.150858	171071.681920	35.692173
1256.201594	171366.792383	35.697191
1256.877782	171662.156933	35.702208
1257.883138	171952.558394	35.707226
1259.423958	172258.582560	35.712244
1260.507655	172569.823393	35.717261
1261.682102	172877.384140	35.722279
1263.210612	173167.427823	35.727296
1264.007845	173505.865034	35.732314
1265.776538	173797.078545	35.737332
1266.897117	174118.538916	35.742349
1267.919963	174443.278918	35.747367
1269.014050	174764.507011	35.752384
1269.857679	175097.123483	35.757402
1270.929878	175438.930260	35.762420
1272.313520	175775.294790	35.767437
1273.473340	176103.653031	35.772455
1275.093030	176450.528980	35.777472
1276.117507	176805.830611	35.782490
1277.476611	177147.005850	35.787508
1278.381271	177508.690402	35.792525
1279.791344	177839.988826	35.797543
1280.921051	178191.983706	35.802560
1282.030816	178542.321911	35.807578
1283.562681	178893.900125	35.812596
1284.692294	179260.306958	35.817613
1286.011978	179613.308649	35.822631
1287.951633	179979.688640	35.827648
1288.486918	180343.739458	35.832666
1290.282706	180702.584453	35.837684
1291.776306	181064.324787	35.842701
1293.098068	181436.858568	35.847719
1294.133908	181788.424795	35.852736
1295.453443	182156.979020	35.857754
1296.654371	182522.179429	35.862772
1297.832464	182889.137692	35.867789
1298.823910	183273.403278	35.872807
1300.594101	183631.232315	35.877824
1302.008954	184002.322396	35.882842
1303.782579	184364.090480	35.887860
1304.938733	184737.957305	35.892877
1306.383879	185104.595107	35.897895
1308.190283	185466.593783	35.902912
1309.495833	185817.508007	35.907930
1311.071874	186178.673721	35.912948
1312.277405	186520.127532	35.917965
1313.448061	186890.135666	35.922983
1314.981750	187237.086639	35.928000
1316.116394	187601.317518	35.933018
1317.719633	187956.905571	35.938036
1318.758929	188321.740833	35.943053
1319.794998	188674.888447	35.948071
1321.464006	189031.970346	35.953088
1322.791162	189404.343155	35.958106
1324.569010	189746.141331	35.963124
1325.449919	190120.318837	35.968141
1326.999217	190470.384596	35.973159
1328.396133	190821.835887	35.978176
1329.444961	191170.554115	35.983194
1330.981600	191535.289914	35.988212
1332.546896	191882.264276	35.993229
1333.638747	192236.681440	35.998247
1335.339118	192586.036876	36.003264
1336.649179	192937.718383	36.008282
1337.813887	193270.270169	36.013300
1339.446241	193589.569813	36.018317
1340.459126	193932.737502	36.023335
1341.898594	194276.141417	36.028352
1342.901024	194615.493650	36.033370
1344.167895	194937.463155	36.038388
1345.670984	195286.067113	36.043405
1346.674543	195636.570856	36.048423
1348.202016	195982.064493	36.053440
1349.472218	196327.551734	36.058458
1351.025731	196665.300922	36.063476
1352.027517	197027.276443	36.068493
1353.427349	197377.280242	36.073511
1355.151839	197708.227562	36.078528
1356.571731	198060.313840	36.083546
1357.899423	198420.923200	36.088564
1359.180753	198758.893481	36.093581
1360.647167	199122.733910	36.098599
1362.088607	199485.057017	36.103616
1363.000523	199846.504646	36.108634
1364.370888	200199.016953	36.113652
1365.761693	200566.953198	36.118669
1367.262055	200925.681560	36.123687
1368.746673	201280.199377	36.128704
1369.699147	201646.538017	36.133722
1371.012632	202008.781692	36.138740
1372.495742	202384.216013	36.143757
1373.815010	202761.812392	36.148775
1375.054382	203148.641543	36.153792
1376.322335	203520.638750	36.158810
1377.647570	203885.556556	36.163828
1379.064433	204276.679435	36.168845
1379.954480	204672.500271	36.173863
1381.593604	205056.175943	36.178880
1382.932875	205457.259569	36.183898
1384.313167	205848.460538	36.188916
1385.652107	206237.308812	36.193933
1386.727014	206645.502051	36.198951
1388.217708	207033.910480	36.203968
1389.542121	207450.218437	36.208986
1390.649966	207853.613358	36.214004
1392.201773	208256.848281	36.219021
1393.581231	208681.216648	36.224039
1395.170885	209074.990164	36.229056
1396.473946	209489.395474	36.234074
1397.657859	209906.933527	36.239092
1399.533176	210314.836537	36.244109
1400.609062	210734.555372	36.249127
1402.293424	211139.751437	36.254144
1403.563982	211555.480762	36.259162
1404.915681	211981.458646	36.264180
1406.532945	212394.785935	36.269197
1407.497059	212823.727252	36.274215
1409.317249	213233.647579	36.279232
1410.898580	213643.939472	36.284250
1412.394392	214077.027887	36.289268
1413.947739	214487.607820	36.294285
1414.901289	214935.621523	36.299303
1416.522431	215367.019555	36.304320
1417.925986	215799.014337	36.309338
1419.386767	216212.868418	36.314356
1421.081876	216620.234909	36.319373
1422.357719	217037.170935	36.324391
1423.754220	217450.203182	36.329408
1425.560902	217868.706207	36.334426
1426.871947	218280.816562	36.339444
1428.538654	218685.733324	36.344461
1429.582455	219082.652761	36.349479
1431.566336	219476.701150	36.354496
1432.873059	219855.852765	36.359514
1434.044122	220259.816643	36.364532
1435.972096	220630.462016	36.369549
1437.087394	221033.930300	36.374567
1438.716621	221420.527154	36.379584
1440.394131	221815.651362	36.384602
1441.545821	222207.663666	36.389620
1443.110304	222583.963839	36.394637
1444.732114	222977.323790	36.399655
1446.056054	223352.421886	36.404672
1447.774859	223771.040516	36.409690
1448.536331	224164.877018	36.414708
1450.253877	224552.080430	36.419725
1451.420246	224958.095298	36.424743
1453.028173	225364.241980	36.429760
1454.195208	225763.655881	36.434778
1455.571651	226188.664598	36.439796
1457.130983	226588.219844	36.444813
1458.094640	227014.214100	36.449831
1459.589162	227428.616256	36.454848
1460.926094	227861.105074	36.459866
1462.604111	228284.598420	36.464884
1463.927465	228712.977747	36.469901
1465.269563	229144.022466	36.474919
1466.875454	229570.402323	36.479936
1468.542360	230001.396376	36.484954
1470.039436	230437.245948	36.489972
1471.684008	230872.945637	36.494989
1473.076860	231308.002489	36.500007
1474.655941	231737.467310	36.505024
1475.929377	232181.792467	36.510042
1477.259118	232624.915931	36.515060
1479.199779	233050.438870	36.520077
1480.674557	233480.688311	36.525095
1481.880954	233930.364207	36.530112
1483.705585	234352.506410	36.535130
1484.873868	234818.473320	36.540148
1486.385127	235248.163061	36.545165
1487.677244	235704.180399	36.550183
1489.113768	236149.709913	36.555200
1490.800847	236597.383841	36.560218
1492.009402	237059.184948	36.565236
1493.882139	237493.393345	36.570253
1495.455941	237936.390322	36.575271
1496.866555	238399.812866	36.580288
1498.378063	238836.116400	36.585306
1499.818161	239292.601767	36.590324
1501.479405	239746.689421	36.595341
1502.922386	240213.057902	36.600359
1504.401255	240664.713893	36.605376
1505.879712	241129.249813	36.610394
1507.101333	241588.012136	36.615412
1509.009168	242027.407475	36.620429
1510.480309	242493.776686	36.625447
1511.689017	242959.021726	36.630464
1513.580195	243414.222865	36.635482
1514.706652	243898.585966	36.640500
1516.378087	244341.708332	36.645517
1517.830999	244815.756931	36.650535
1519.172440	245287.767255	36.655552
1520.946425	245749.977944	36.660570
1522.140335	246215.917753	36.665588
1523.967155	246673.904550	36.670605
1525.471951	247133.113781	36.675623
1527.276429	247595.373445	36.680640
1528.634402	248046.835161	36.685658
1530.174698	248484.321362	36.690676
1531.779683	248938.715775	36.695693
1533.462219	249370.540325	36.700711
1535.260058	249806.817319	36.705728
1537.065306	250249.164942	36.710746
1538.388712	250681.888704	36.715764
1540.148951	251121.729933	36.720781
1541.392197	251578.295927	36.725799
1542.441027	252014.699126	36.730816
1544.112573	252460.907213	36.735834
1545.237175	252911.626136	36.740852
1546.914845	253367.741308	36.745869
1547.915189	253823.587623	36.750887
1549.900679	254288.823369	36.755904
1551.544860	254753.506152	36.760922
1552.699109	255214.612090	36.765940
1554.396496	255675.882781	36.770957
1555.835633	256152.235103	36.775975
1557.645292	256634.318536	36.780992
1559.063648	257097.592219	36.786010
1560.224400	257581.485288	36.791028
1562.022493	258055.696404	36.796045
1563.492172	258543.044601	36.801063
1564.979360	259038.011083	36.806080
1566.335694	259527.944064	36.811098
1567.759842	260019.974461	36.816116
1569.952195	260507.889890	36.821133
1571.268254	261018.609731	36.826151
1572.490218	261511.283394	36.831168
1574.405163	262012.683082	36.836186
1575.905961	262515.751498	36.841204
1577.514491	263028.658574	36.846221
1579.247833	263535.346571	36.851239
1580.627285	264046.690845	36.856256
1582.144571	264544.777119	36.861274
1583.557497	265063.101452	36.866292
1585.420344	265570.504139	36.871309
1587.195792	266071.951244	36.876327
1588.666663	266585.591085	36.881344
1590.337555	267103.643177	36.886362
1591.962567	267610.271048	36.891380
1594.286442	268122.981620	36.896397
1596.076270	268636.008528	36.901415
1597.625053	269128.549027	36.906432
1599.754220	269631.205383	36.911450
1601.136058	270140.690975	36.916468
1602.811764	270633.463139	36.921485
1604.290513	271143.414322	36.926503
1605.642100	271652.064934	36.931520
1607.076053	272157.754586	36.936538
1608.610473	272688.525115	36.941556
1609.970385	273189.195843	36.946573
1611.383657	273707.029404	36.951591
1612.993065	274231.561570	36.956608
1614.602260	274751.368014	36.961626
1615.732755	275269.448988	36.966644
1617.519891	275795.778222	36.971661
1619.148485	276332.954193	36.976679
1620.982438	276855.361745	36.981696
1622.543244	277382.182595	36.986714
1624.586296	277907.500280	36.991732
1626.107442	278444.867536	36.996749
1627.892656	278968.371146	37.001767
1629.314731	279494.676969	37.006784
1630.936880	280028.696274	37.011802
1632.293394	280559.024007	37.016820
1633.870888	281093.505342	37.021837
1635.955812	281608.443610	37.026855
1637.112452	282136.666592	37.031872
1638.959324	282637.314791	37.036890
1640.408799	283165.562922	37.041908
1641.859133	283666.400891	37.046925
1644.059232	284176.664871	37.051943
1645.647190	284706.079676	37.056960
1647.433335	285209.525176	37.061978
1648.631322	285733.997119	37.066996
1650.346261	286245.986252	37.072013
1651.983378	286759.180519	37.077031
1653.676246	287285.318634	37.082048
1655.157168	287806.104934	37.087066
1657.071455	288325.674957	37.092084
1658.834381	288861.194643	37.097101
1660.473470	289376.793123	37.102119
1661.707374	289917.984508	37.107136
1663.510291	290437.413156	37.112154
1665.213408	290971.664962	37.117172
1666.721003	291515.954806	37.122189
1668.594472	292059.953527	37.127207
1669.925975	292603.582262	37.132224
1671.542274	293144.951960	37.137242
1673.383793	293703.503546	37.142260
1675.319885	294244.434870	37.147277
1677.088323	294799.336085	37.152295
1678.569995	295362.664056	37.157312
1680.295245	295914.493975	37.162330
1681.920837	296478.199389	37.167348
1683.450538	297010.524208	37.172365
1685.423063	297580.135937	37.177383
1686.847291	298141.275751	37.182400
1688.761947	298689.937104	37.187418
1690.743934	299259.741948	37.192436
1692.521188	299823.634269	37.197453
1694.329348	300390.642566	37.202471
1695.957871	300950.769057	37.207488
1697.530680	301509.682608	37.212506
1698.955172	302084.059733	37.217524
1700.484087	302661.946712	37.222541
1702.259274	303219.928508	37.227559
1703.663402	303803.467776	37.232576
1705.606269	304391.638626	37.237594
1707.348739	304962.187657	37.242612
1708.814788	305555.407893	37.247629
1710.508739	306142.135873	37.252647
1711.977890	306733.646444	37.257664
1713.944991	307304.880509	37.262682
1715.859801	307907.357501	37.267700
1717.682366	308500.855243	37.272717
1719.511097	309084.062416	37.277735
1720.771521	309682.216168	37.282752
1722.572264	310259.705827	37.287770
1724.522549	310855.197891	37.292788
1726.228310	311457.912998	37.297805
1727.826419	312054.191002	37.302823
1729.645662	312654.821527	37.307840
1731.566610	313244.536293	37.312858
1733.304882	313854.516533	37.317876
1734.944641	314446.401871	37.322893
1736.817076	315031.311609	37.327911
1738.447200	315644.190582	37.332928
1740.806508	316231.880342	37.337946
1742.160123	316831.615745	37.342964
1743.861081	317422.502784	37.347981
1745.809465	318014.385379	37.352999
1747.763181	318620.330138	37.358016
1748.795871	319208.976700	37.363034
1750.929647	319796.268672	37.368052
1752.336258	320384.132769	37.373069
1754.431714	320950.345495	37.378087
1756.119439	321534.344600	37.383104
1757.700784	322099.388443	37.388122
1759.319846	322672.343582	37.393140
1761.029468	323254.673763	37.398157
1762.763223	323844.713823	37.403175
1764.236856	324429.129283	37.408192
1765.925520	325011.447368	37.413210
1767.677056	325613.452970	37.418228
1769.364291	326214.447895	37.423245
1771.236465	326818.504209	37.428263
1772.604059	327423.805883	37.433280
1774.485377	328031.327378	37.438298
1776.003959	328638.318764	37.443316
1777.729749	329266.698380	37.448333
1780.004993	329873.120991	37.453351
1781.634999	330498.304552	37.458368
1783.787751	331101.739022	37.463386
1785.776973	331716.136556	37.468404
1788.046276	332326.977895	37.473421
1789.925422	332952.043405	37.478439
1791.229283	333563.386318	37.483456
1793.501802	334169.460074	37.488474
1795.629407	334786.873704	37.493492
1797.560000	335408.654096	37.498509
1799.056237	336006.839249	37.503527
1800.754757	336625.521715	37.508544
1802.489314	337239.571035	37.513562
1804.253343	337863.229554	37.518580
1806.064244	338498.144034	37.523597
1807.846090	339120.134909	37.528615
1809.296394	339746.437722	37.533632
1810.934765	340384.048710	37.538650
1812.943775	341028.241276	37.543668
1814.471794	341671.870537	37.548685
1816.407627	342314.332938	37.553703
1818.204676	342958.942241	37.558720
1819.992915	343614.763787	37.563738
1822.073928	344239.765232	37.568756
1823.356696	344914.131212	37.573773
1825.246846	345557.701525	37.578791
1827.081017	346222.567344	37.583808
1828.713554	346881.238978	37.588826
1830.891749	347550.319052	37.593844
1832.557908	348206.860273	37.598861
1834.852197	348862.628872	37.603879
1836.905919	349515.686997	37.608896
1838.719689	350179.358575	37.613914
1840.486007	350831.887206	37.618932
1842.418016	351483.541723	37.623949
1844.370264	352139.447049	37.628967
1846.098934	352810.885402	37.633984
1848.169584	353473.527534	37.639002
1849.767385	354126.569232	37.644020
1851.731462	354796.898317	37.649037
1853.576240	355456.375892	37.654055
1855.573890	356112.494047	37.659072
1857.379217	356790.228298	37.664090
1859.141708	357447.354536	37.669108
1860.616040	358123.041522	37.674125
1862.416085	358788.412879	37.679143
1864.321107	359461.038617	37.684160
1866.116264	360139.101505	37.689178
1867.862928	360813.913577	37.694196
1869.871269	361480.273157	37.699213
1872.114766	362154.752862	37.704231
1873.906862	362819.806855	37.709248
1875.444423	363488.240858	37.714266
1877.411994	364134.748589	37.719284
1879.470484	364789.349323	37.724301
1880.822785	365443.675158	37.729319
1882.991788	366090.878786	37.734336
1884.206138	366756.621711	37.739354
1886.601350	367406.100112	37.744372
1888.127053	368085.011235	37.749389
1889.987613	368744.601000	37.754407
1891.896695	369430.883080	37.759424
1893.731355	370099.154551	37.764442
1895.513463	370757.327000	37.769460
1897.206098	371446.981716	37.774477
1899.195884	372133.226376	37.779495
1901.274087	372827.991682	37.784512
1902.826016	373511.416617	37.789530
1904.968592	374210.127262	37.794548
1906.368666	374918.153849	37.799565
1908.782304	375606.850262	37.804583
1910.520794	376320.880473	37.809600
1912.114990	377035.148402	37.814618
1914.314771	377750.798330	37.819636
1916.107655	378478.648679	37.824653
1918.003772	379184.834373	37.829671
1920.037444	379903.713672	37.834688
1922.001296	380638.286941	37.839706
1924.027330	381340.805993	37.844724
1925.885976	382083.505710	37.849741
1927.888010	382800.909164	37.854759
1929.880221	383523.725377	37.859776
1931.839097	384268.541025	37.864794
1934.104936	384978.576874	37.869812
1935.931050	385717.803495	37.874829
1938.230072	386450.038925	37.879847
1940.220484	387179.266300	37.884864
1941.981940	387904.661268	37.889882
1944.322355	388640.466030	37.894900
1946.004820	389369.136919	37.899917
1948.210657	390112.383686	37.904935
1950.209593	390833.743468	37.909952
1951.835666	391586.304493	37.914970
1954.189910	392307.850694	37.919988
1956.086337	393038.759037	37.925005
1958.333805	393783.508896	37.930023
1960.372774	394502.115496	37.935040
1962.425956	395234.618894	37.940058
1964.689000	395970.263826	37.945076
1966.903199	396709.776991	37.950093
1968.948341	397425.981526	37.955111
1970.877425	398162.185641	37.960128
1972.700812	398888.200394	37.965146
1974.329014	399611.948586	37.970164
1976.265884	400352.506921	37.975181
1977.800313	401094.785569	37.980199
1980.133660	401828.398564	37.985216
1981.819226	402575.987062	37.990234
1983.872190	403311.712055	37.995252
1985.639536	404065.684988	38.000269
1987.995925	404799.674586	38.005287
1990.201826	405545.376652	38.010304
1991.837681	406288.568550	38.015322
1993.966739	407039.108728	38.020340
1995.746506	407791.764003	38.025357
1997.662735	408528.490565	38.030375
1999.899940	409285.539739	38.035392
2001.538869	410047.125712	38.040410
2003.997964	410791.733343	38.045428
2005.485496	411531.946169	38.050445
2007.540874	412268.574544	38.055463
2009.256851	412991.635431	38.060480
2011.196343	413724.519253	38.065498
2013.359928	414465.071892	38.070516
2015.117974	415203.137787	38.075533
2017.018357	415927.861720	38.080551
2019.061613	416688.964710	38.085568
2020.669792	417433.223653	38.090586
2022.809291	418189.860018	38.095604
2024.232330	418949.302408	38.100621
2026.177704	419716.588578	38.105639
2028.439345	420473.087243	38.110656
2030.032598	421269.787190	38.115674
2031.847794	422040.798374	38.120692
2034.068051	422835.699743	38.125709
2035.815714	423621.538137	38.130727
2037.811862	424409.058062	38.135744
2039.914524	425234.161289	38.140762
2041.779053	426017.524828	38.145780
2043.539347	426845.922311	38.150797
2045.612567	427660.973825	38.155815
2048.034520	428475.940652	38.160832
2050.019374	429298.243247	38.165850
2052.156130	430122.720580	38.170868
2054.828434	430944.246176	38.175885
2056.981187	431765.120514	38.180903
2059.197025	432595.676172	38.185920
2061.381188	433412.033508	38.190938
2063.845213	434214.749930	38.195956
2065.816175	435044.854861	38.200973
2067.819945	435859.132154	38.205991
2070.492152	436691.644358	38.211008
2072.555005	437503.728360	38.216026
2074.364798	438330.756169	38.221044
2076.548827	439158.147950	38.226061
2078.237227	439990.095672	38.231079
2080.785634	440813.166726	38.236096
2082.901303	441638.202187	38.241114
2084.748678	442476.610911	38.246132
2086.191151	443316.674287	38.251149
2088.178917	444157.425694	38.256167
2090.831096	444986.550063	38.261184
2092.865322	445845.697793	38.266202
2094.724692	446687.740173	38.271220
2097.134262	447534.971551	38.276237
2098.980038	448385.197158	38.281255
2101.372823	449228.672243	38.286272
2103.546580	450075.286800	38.291290
2105.878130	450923.157156	38.296308
2108.051674	451778.860115	38.301325
2110.057101	452628.790332	38.306343
2112.948224	453468.526039	38.311360
2114.445495	454317.561785	38.316378
2116.609536	455167.869323	38.321396
2119.078438	456017.940295	38.326413
2120.694787	456864.627855	38.331431
2123.122030	457721.563978	38.336448
2125.006035	458573.143612	38.341466
2127.065017	459433.002004	38.346484
2129.079221	460283.376723	38.351501
2130.935798	461153.560993	38.356519
2133.558742	462000.982690	38.361536
2135.309308	462865.650658	38.366554
2137.480253	463721.668747	38.371572
2139.725991	464590.528176	38.376589
2141.576143	465455.118359	38.381607
2143.843803	466316.973622	38.386624
2146.104847	467185.767371	38.391642
2148.077701	468039.508929	38.396660
2149.595624	468870.596183	38.401677
2151.980834	469727.228345	38.406695
2153.811972	470565.266739	38.411712
2155.873968	471420.765552	38.416730
2158.078996	472263.368062	38.421748
2159.835666	473123.894428	38.426765
2161.870578	473983.022465	38.431783
2164.199746	474854.239327	38.436800
2165.780980	475735.340539	38.441818
2168.186225	476610.101417	38.446836
2170.474992	477497.873978	38.451853
2172.251350	478388.012525	38.456871
2174.718599	479281.580914	38.461888
2176.778562	480182.093141	38.466906
2179.103271	481072.871021	38.471924
2181.521382	481965.307479	38.476941
2183.553450	482877.964770	38.481959
2186.191014	483769.670870	38.486976
2188.276764	484684.349653	38.491994
2190.528673	485595.016221	38.497012
2192.946157	486511.617913	38.502029
2194.792643	487421.703330	38.507047
2197.281323	488337.240450	38.512064
2199.502550	489274.533009	38.517082
2201.687886	490183.512468	38.522100
2203.885114	491101.125402	38.527117
2205.951642	492032.643254	38.532135
2208.513547	492953.077132	38.537152
2210.324533	493887.919778	38.542170
2212.442649	494825.184773	38.547188
2215.038915	495755.759615	38.552205
2216.784254	496700.755675	38.557223
2219.273211	497638.310831	38.562240
2221.547820	498597.848870	38.567258
2223.998597	499527.687300	38.572276
2226.375621	500472.268920	38.577293
2228.378444	501417.666452	38.582311
2230.610338	502359.340887	38.587328
2233.050588	503329.175656	38.592346
2235.369705	504280.210399	38.597364
2237.671367	505218.231241	38.602381
2239.863329	506184.459749	38.607399
2241.946373	507130.578002	38.612416
2244.136283	508100.123331	38.617434
2246.201397	509061.967033	38.622452
2248.255648	510019.469720	38.627469
2250.492288	510999.725379	38.632487
2252.630723	511962.544175	38.637504
2254.834772	512949.542882	38.642522
2257.003602	513927.311913	38.647540
2259.708347	514916.677220	38.652557
2261.743527	515896.413751	38.657575
2264.001641	516879.379151	38.662592
2266.103480	517860.192210	38.667610
2268.377089	518856.033682	38.672628
2270.808320	519851.886384	38.677645
2272.665509	520839.153679	38.682663
2275.173998	521828.215603	38.687680
2277.461032	522843.448625	38.692698
2279.978572	523834.798332	38.697716
2282.559215	524825.468880	38.702733
2284.646647	525827.741646	38.707751
2287.263569	526804.677078	38.712768
2289.491715	527815.206518	38.717786
2291.345111	528805.786974	38.722804
2293.816198	529801.739513	38.727821
2295.858637	530789.287160	38.732839
2298.369616	531772.009387	38.737856
2300.839880	532728.995855	38.742874
2302.763717	533694.820696	38.747892
2304.945976	534663.811727	38.752909
2307.098686	535640.596289	38.757927
2309.437348	536616.177523	38.762944
2311.473380	537591.541933	38.767962
2313.341860	538584.583683	38.772980
2315.921114	539564.959603	38.777997
2318.090400	540578.900215	38.783015
2320.309272	541566.545749	38.788032
2322.814601	542572.289300	38.793050
2324.911048	543589.701108	38.798068
2327.096388	544605.868208	38.803085
2329.303200	545623.618656	38.808103
2331.446572	546638.388609	38.813120
2333.754008	547693.495557	38.818138
2335.730451	548726.247913	38.823156
2337.942840	549774.071637	38.828173
2339.992339	550830.290710	38.833191
2342.687947	551894.367277	38.838208
2344.926722	552950.794848	38.843226
2347.035601	554014.803773	38.848244
2349.849835	555092.738872	38.853261
2352.197656	556158.903538	38.858279
2354.259061	557255.087195	38.863296
2356.869845	558328.124112	38.868314
2359.004214	559434.923392	38.873332
2361.664828	560511.747323	38.878349
2364.258614	561608.040242	38.883367
2367.311119	562676.233698	38.888384
2369.715905	563765.697470	38.893402
2371.946322	564865.698842	38.898420
2374.458883	565950.443139	38.903437
2376.170482	567050.848991	38.908455
2378.542859	568155.723398	38.913472
2381.033709	569255.462809	38.918490
2383.402103	570384.652607	38.923508
2385.712414	571490.256677	38.928525
2387.828013	572632.494994	38.933543
2390.711320	573736.405155	38.938560
2393.004237	574851.760951	38.943578
2395.070645	575959.176520	38.948596
2397.663485	577110.971622	38.953613
2399.962504	578235.914134	38.958631
2402.385668	579372.074849	38.963648
2405.337263	580512.259495	38.968666
2407.948665	581645.021497	38.973684
2410.827404	582753.358058	38.978701
2413.175539	583875.024373	38.983719
2416.002288	585001.625144	38.988736
2418.500210	586106.613311	38.993754
2420.612576	587232.374467	38.998772
2423.245786	588353.984823	39.003789
2425.767832	589473.654918	39.008807
2427.861810	590599.808679	39.013824
2430.341173	591713.563364	39.018842
2432.719644	592845.575122	39.023860
2435.367175	593963.553614	39.028877
2437.687397	595098.017531	39.033895
2440.220142	596228.029006	39.038912
2442.965958	597343.869310	39.043930
2444.900501	598472.963045	39.048948
2447.444410	599580.959915	39.053965
2450.133768	600724.639573	39.058983
2452.405814	601838.978381	39.064000
2454.788026	602972.020976	39.069018
2457.349452	604090.402466	39.074036
2460.064657	605182.315130	39.079053
2461.990340	606283.365606	39.084071
2464.449646	607365.000404	39.089088
2466.968285	608452.028820	39.094106
2468.954998	609560.061210	39.099124
2471.326035	610647.254404	39.104141
2473.623516	611765.328749	39.109159
2476.118664	612868.499899	39.114176
2478.509131	613988.989752	39.119194
2480.622638	615100.859203	39.124212
2482.870676	616244.907319	39.129229
2485.069034	617385.595111	39.134247
2487.531837	618541.074180	39.139264
2490.228492	619676.742884	39.144282
2492.461940	620840.119186	39.149300
2494.907896	622008.736179	39.154317
2497.250090	623174.795997	39.159335
2499.639065	624364.314311	39.164352
2502.286209	625529.271644	39.169370
2504.356383	626733.575052	39.174388
2506.859493	627918.036503	39.179405
2509.169440	629131.075593	39.184423
2511.455614	630341.982985	39.189440
2514.365562	631551.051738	39.194458
2516.485770	632772.398775	39.199476
2519.481930	634011.886925	39.204493
2522.254408	635228.198604	39.209511
2524.434983	636476.568446	39.214528
2527.147671	637691.805629	39.219546
2529.408173	638947.205346	39.224564
2532.092760	640162.757904	39.229581
2534.666951	641437.617663	39.234599
2537.198200	642666.174837	39.239616
2540.018665	643929.509451	39.244634
2542.499527	645195.388141	39.249652
2545.350069	646429.876521	39.254669
2548.141313	647692.750627	39.259687
2550.855699	648930.249117	39.264704
2553.196030	650194.580922	39.269722
2555.788016	651459.909008	39.274740
2558.490885	652719.028072	39.279757
2561.110232	653989.265969	39.284775
2563.446098	655254.704478	39.289792
2565.841270	656524.506173	39.294810
2568.322155	657799.013166	39.299828
2571.573058	659066.155079	39.304845
2574.140989	660348.487031	39.309863
2576.598835	661618.318795	39.314880
2579.093381	662889.672291	39.319898
2581.901245	664172.059859	39.324916
2584.452159	665443.915963	39.329933
2587.293075	666729.095314	39.334951
2589.407650	668013.526036	39.339968
2592.449200	669286.784164	39.344986
2594.822292	670583.715505	39.350004
2597.490450	671853.906377	39.355021
2599.354338	673153.655477	39.360039
2602.116299	674443.479413	39.365056
2605.147512	675752.525673	39.370074
2607.926000	677028.218278	39.375092
2610.272479	678318.175373	39.380109
2612.891158	679613.973442	39.385127
2615.408269	680908.961592	39.390144
2618.188780	682187.972890	39.395162
2620.633020	683504.076868	39.400180
2623.374451	684786.410830	39.405197
2625.871521	686103.375743	39.410215
2628.048392	687392.193134	39.415232
2631.042959	688671.407555	39.420250
2633.966923	689930.940824	39.425268
2636.238866	691209.866477	39.430285
2638.725490	692463.509092	39.435303
2640.870069	693741.996906	39.440320
2643.936030	694996.877629	39.445338
2646.394879	696292.217825	39.450356
2649.157519	697553.586034	39.455373
2651.733133	698839.507102	39.460391
2654.177458	700131.015754	39.465408
2656.936617	701410.432182	39.470426
2659.578207	702705.943708	39.475444
2662.354593	704016.856532	39.480461
2665.268541	705314.018780	39.485479
2667.717838	706619.042909	39.490496
2671.112463	707904.985169	39.495514
2673.291937	709228.885634	39.500532
2675.651863	710535.166405	39.505549
2678.151470	711845.237174	39.510567
2681.078878	713187.323480	39.515584
2683.626388	714495.544016	39.520602
2685.926966	715851.226617	39.525620
2688.950915	717185.191028	39.530637
2691.821198	718544.357409	39.535655
2694.295470	719882.835497	39.540672
2697.012821	721235.357467	39.545690
2699.703611	722597.409503	39.550708
2702.380973	723954.444003	39.555725
2705.081224	725306.901694	39.560743
2707.496542	726693.644864	39.565760
2710.486302	728051.736277	39.570778
2713.164380	729441.335024	39.575796
2715.978315	730804.584922	39.580813
2718.810081	732193.641629	39.585831
2721.335654	733574.064846	39.590848
2723.898375	734974.694442	39.595866
2726.720946	736369.557461	39.600884
2729.511110	737766.751878	39.605901
2732.711110	739169.905020	39.610919
2735.274816	740565.069738	39.615936
2738.873568	741956.908607	39.620954
2741.441802	743367.816834	39.625972
2744.244777	744743.559747	39.630989
2747.481908	746120.273981	39.636007
2750.158529	747529.829566	39.641024
2753.269144	748914.014738	39.646042
2755.934073	750308.725386	39.651060
2758.726860	751697.694943	39.656077
2761.562938	753085.916492	39.661095
2763.948253	754493.276605	39.666112
2767.055215	755878.538341	39.671130
2769.514683	757283.258994	39.676148
2771.911033	758679.854457	39.681165
2775.132609	760083.591454	39.686183
2777.115296	761490.030667	39.691200
2780.310827	762901.324869	39.696218
2782.648030	764315.695888	39.701236
2785.398684	765724.420830	39.706253
2787.986239	767147.172906	39.711271
2791.018930	768576.515722	39.716288
2793.965184	770001.272882	39.721306
2796.607069	771425.758713	39.726324
2799.006021	772855.860118	39.731341
2802.012108	774275.167937	39.736359
2804.805383	775727.007072	39.741376
2807.638352	777160.526382	39.746394
2810.505742	778605.300626	39.751412
2813.071184	780020.919106	39.756429
2815.856490	781428.617299	39.761447
2818.553186	782823.296165	39.766464
2821.358713	784224.264107	39.771482
2824.271895	785606.691225	39.776500
2826.731750	787022.087187	39.781517
2829.443826	788416.269982	39.786535
2831.716815	789862.719103	39.791552
2834.448930	791275.757336	39.796570
2837.534271	792708.895092	39.801588
2840.022765	794154.582190	39.806605
2842.915175	795586.433525	39.811623
2845.395942	797066.261185	39.816640
2848.041339	798495.943918	39.821658
2851.296254	799973.070962	39.826676
2853.888055	801447.644555	39.831693
2857.014274	802910.903078	39.836711
2859.672754	804383.373411	39.841728
2862.631223	805867.074673	39.846746
2865.362602	807362.280984	39.851764
2867.984998	808841.678051	39.856781
2870.730288	810353.686290	39.861799
2873.272382	811864.512791	39.866816
2876.568763	813370.041139	39.871834
2879.856653	814894.583366	39.876852
2882.587277	816420.338399	39.881869
2885.493427	817948.843883	39.886887
2888.307310	819487.513134	39.891904
2891.360045	821011.926186	39.896922
2894.399653	822553.756029	39.901940
2896.987833	824104.425818	39.906957
2900.185614	825657.753611	39.911975
2903.074347	827187.212320	39.916992
2905.902511	828742.945464	39.922010
2909.173308	830317.587416	39.927028
2911.984293	831884.323357	39.932045
2915.123845	833436.548053	39.937063
2917.713906	835003.981119	39.942080
2920.724936	836587.619036	39.947098
2923.693770	838130.223401	39.952116
2926.687940	839709.931111	39.957133
2929.921609	841270.280696	39.962151
2933.020074	842852.065649	39.967168
2936.149053	844413.414018	39.972186
2939.339097	845989.587320	39.977204
2941.941685	847556.325195	39.982221
2945.151508	849122.767781	39.987239
2948.029437	850705.005497	39.992256
2951.303193	852266.473307	39.997274
2953.995735	853850.082414	40.002292
2956.602673	855433.690747	40.007309
2960.093620	856999.857319	40.012327
2963.112693	858581.524185	40.017344
2966.229886	860156.655862	40.022362
2969.313654	861719.845449	40.027380
2971.692354	863313.009003	40.032397
2974.779398	864884.310097	40.037415
2977.576720	866468.822639	40.042432
2980.141875	868068.366535	40.047450
2983.223539	869654.032800	40.052468
2985.524562	871261.879411	40.057485
2988.907252	872860.015525	40.062503
2991.677358	874474.958903	40.067520
2994.803550	876085.148187	40.072538
2998.134429	877695.254414	40.077556
3000.265015	879318.081139	40.082573
3003.253893	880934.035404	40.087591
3006.234128	882559.310657	40.092608
3009.225799	884167.221745	40.097626
3012.148829	885765.813524	40.102644
3014.960320	887372.291655	40.107661
3017.786592	888951.286275	40.112679
3020.668489	890541.039138	40.117696
3023.639296	892122.329448	40.122714
3026.195727	893733.741354	40.127732
3029.199250	895341.444000	40.132749
3032.610686	896951.520175	40.137767
3035.458565	898572.609377	40.142784
3038.568082	900198.589709	40.147802
3041.362230	901830.128426	40.152820
3043.967782	903469.220839	40.157837
3047.179060	905098.107312	40.162855
3050.095051	906752.174239	40.167872
3053.152418	908411.309851	40.172890
3056.097020	910071.701672	40.177908
3059.325522	911734.531723	40.182925
3062.352863	913423.623329	40.187943
3065.951026	915091.151025	40.192960
3068.409770	916772.485287	40.197978
3071.622008	918462.785313	40.202996
3074.897599	920154.472499	40.208013
3077.887661	921865.264242	40.213031
3081.006247	923555.438962	40.218048
3084.065402	925252.866186	40.223066
3086.898713	926968.689499	40.228084
3089.969518	928675.393181	40.233101
3093.494875	930398.634139	40.238119
3096.184280	932118.869670	40.243136
3099.278613	933856.680804	40.248154
3102.963255	935593.059284	40.253172
3105.580222	937321.290086	40.258189
3109.196474	939058.166663	40.263207
3112.174749	940801.939186	40.268224
3115.087755	942552.026282	40.273242
3118.213660	944294.226264	40.278260
3120.869173	946058.662731	40.283277
3124.539489	947824.337227	40.288295
3127.440253	949579.507963	40.293312
3130.616743	951363.054544	40.298330
3133.557409	953125.693910	40.303348
3136.741966	954923.648717	40.308365
3139.931307	956705.387810	40.313383
3143.392236	958532.243473	40.318400
3145.930940	960376.078947	40.323418
3149.401011	962204.997143	40.328436
3152.186359	964054.751609	40.333453
3155.058631	965892.662953	40.338471
3158.618551	967743.058257	40.343488
3161.577134	969613.166359	40.348506
3164.788620	971459.786009	40.353524
3167.550658	973325.008583	40.358541
3170.473226	975199.644098	40.363559
3173.826228	977070.475251	40.368576
3176.698266	978934.730988	40.373594
3180.602027	980829.876780	40.378612
3183.201502	982710.679724	40.383629
3186.509339	984606.618483	40.388647
3189.671389	986485.694998	40.393664
3193.018889	988373.268584	40.398682
3196.355988	990266.346678	40.403700
3199.081283	992154.714119	40.408717
3202.627965	994049.512753	40.413735
3205.457042	995948.850809	40.418752
3208.676822	997843.214318	40.423770
3211.889379	999741.510482	40.428788
3215.095554	1001660.044306	40.433805
3217.879577	1003548.105998	40.438823
3221.370766	1005411.069353	40.443840
3224.186187	1007272.656814	40.448858
3227.959993	1009138.417162	40.453876
3231.090536	1010991.938627	40.458893
3233.974915	1012847.119441	40.463911
3237.196736	1014713.353236	40.468928
3240.235809	1016573.382083	40.473946
3243.676773	1018467.962068	40.478964
3246.575472	1020344.962236	40.483981
3249.290560	1022245.353376	40.488999
3252.422549	1024134.781900	40.494016
3255.381904	1026056.370099	40.499034
3258.722905	1027969.988369	40.504052
3261.939277	1029887.318964	40.509069
3264.965288	1031830.770656	40.514087
3267.970966	1033770.653030	40.519104
3271.287983	1035719.265732	40.524122
3274.550172	1037678.491773	40.529140
3277.511753	1039645.563183	40.534157
3280.967204	1041615.134717	40.539175
3284.159350	1043597.252405	40.544192
3287.230314	1045588.892494	40.549210
3291.260195	1047560.786484	40.554228
3294.142164	1049579.525000	40.559245
3297.222570	1051579.790064	40.564263
3300.760862	1053592.241025	40.569280
3303.948565	1055604.497250	40.574298
3307.381865	1057621.650032	40.579316
3310.606596	1059640.981493	40.584333
3313.781271	1061671.490321	40.589351
3317.346064	1063706.850120	40.594368
3320.809060	1065764.698439	40.599386
3324.486983	1067792.863295	40.604404
3327.469382	1069843.984656	40.609421
3330.398385	1071884.281449	40.614439
3333.859099	1073942.992229	40.619456
3337.186974	1076003.440748	40.624474
3340.605311	1078067.406615	40.629492
3343.849950	1080141.245839	40.634509
3346.918240	1082208.106137	40.639527
3350.913966	1084290.481167	40.644544
3353.729850	1086369.959191	40.649562
3357.310509	1088444.597587	40.654580
3360.384101	1090551.296726	40.659597
3363.503362	1092646.952057	40.664615
3367.231229	1094733.678188	40.669632
3370.446169	1096844.686682	40.674650
3373.713213	1098945.991791	40.679668
3377.062525	1101063.915995	40.684685
3380.275475	1103174.836512	40.689703
3383.416526	1105290.564234	40.694720
3387.057929	1107427.569842	40.699738
3390.111765	1109549.638767	40.704756
3393.431713	1111692.999867	40.709773
3396.745035	1113825.708924	40.714791
3400.455850	1115951.799672	40.719808
3403.770914	1118110.570284	40.724826
3407.400053	1120241.815544	40.729844
3410.739330	1122388.690121	40.734861
3413.975059	1124532.251020	40.739879
3417.606465	1126665.491203	40.744896
3420.570431	1128828.343288	40.749914
3424.395358	1130980.693459	40.754932
3427.727433	1133132.159529	40.759949
3430.720107	1135288.495564	40.764967
3434.255239	1137443.961519	40.769984
3437.910661	1139612.637416	40.775002
3441.303506	1141748.524884	40.780007
3444.972915	1143838.284260	40.785012
3447.931340	1145890.838187	40.790016
3451.705585	1147841.065895	40.795021
3454.488225	1149744.130313	40.800026
3457.721254	1151561.492804	40.805031
3460.857280	1153295.508555	40.810036
3463.908243	1154959.127503	40.815040
3467.026139	1156525.711962	40.820045
3469.680457	1158037.334062	40.825050
3471.897059	1159464.252460	40.830055
3475.012937	1160821.723869	40.835060
3477.175389	1162095.458524	40.840064
3479.819015	1163288.210023	40.845069
3482.009995	1164420.780298	40.850074
3484.488002	1165470.325302	40.855079
3486.221152	1166461.332491	40.860084
3488.256382	1167389.980658	40.865088
3490.144151	1168248.164610	40.870093
3491.851357	1169057.254344	40.875098
3493.448531	1169783.289058	40.880103
3495.754034	1170463.816154	40.885108
3496.916321	1171096.139299	40.890112
3498.346869	1171672.874318	40.895117
3500.042014	1172192.719684	40.900122
3501.046017	1172672.543484	40.905127
3502.448848	1173104.632742	40.910132
3503.590503	1173494.294484	40.915136
3505.019690	1173847.576931	40.920141
3506.011506	1174167.058327	40.925146
3506.723628	1174437.162325	40.930151
3507.879035	1174682.761318	40.935156
3508.652968	1174881.463018	40.940160
3510.006979	1175048.857815	40.945165
3510.671945	1175207.970791	40.950170
3511.228982	1175321.660378	40.955175
3512.052290	1175392.601619	40.960180
3512.562228	1175467.458323	40.965184
3513.636883	1175475.105549	40.970189
3514.147235	1175500.944290	40.975194
3514.917662	1175478.382995	40.980199
3515.752369	1175442.802550	40.985204
3515.928931	1175372.357809	40.990208
3516.545238	1175303.725035	40.995213
3517.106914	1175207.008375	41.000218
3517.213079	1175099.995185	41.005223
3518.046411	1174958.921824	41.010228
3518.069778	1174821.371964	41.015232
3518.797418	1174668.429410	41.020237
3519.075841	1174499.245688	41.025242
3519.219747	1174301.038918	41.030247
3519.833186	1174105.953096	41.035252
3519.866744	1173901.620550	41.040256
3520.118810	1173672.632705	41.045261
3520.746943	1173436.971826	41.050266
3520.983265	1173207.966170	41.055271
3521.143247	1172957.932091	41.060276
3521.165644	1172697.911403	41.065280
3521.648942	1172416.485768	41.070285
3521.833763	1172143.205985	41.075290
3521.966189	1171847.281506	41.080295
3522.157734	1171557.273592	41.085300
3522.145020	1171249.075568	41.090304
3522.824340	1170947.632610	41.095309
3522.741346	1170643.561613	41.100314
3523.283792	1170310.779750	41.105319
3523.075357	1169981.591783	41.110324
3523.072622	1169656.312681	41.115328
3523.221772	1169311.830165	41.120333
3522.966809	1168983.813834	41.125338
3523.270459	1168628.595739	41.130343
3523.618578	1168293.640847	41.135348
3523.640494	1167926.433423	41.140352
3524.118601	1167557.708969	41.145357
3523.515705	1167205.186828	41.150362
3524.052570	1166843.577747	41.155367
3524.105401	1166474.658127	41.160372
3524.251584	1166102.297519	41.165376
3524.393144	1165714.706323	41.170381
3524.467952	1165337.014357	41.175386
3524.230984	1164951.979076	41.180391
3524.643190	1164559.818444	41.185396
3524.174294	1164176.936951	41.190400
3524.468777	1163792.768033	41.195405
3524.407452	1163409.763320	41.200410
3524.488846	1163002.801406	41.205415
3524.372700	1162611.621300	41.210420
3524.357872	1162220.300801	41.215424
3524.657603	1161810.847787	41.220429
3524.630429	1161422.210554	41.225434
3524.872468	1161025.938204	41.230439
3525.117767	1160601.181202	41.235444
3525.045953	1160190.906646	41.240448
3524.828659	1159794.711477	41.245453
3524.693425	1159380.791233	41.250458
3524.583412	1158969.860168	41.255463
3524.786161	1158550.712468	41.260468
3524.521258	1158149.483335	41.265472
3524.957737	1157732.312514	41.270477
3524.940901	1157313.953539	41.275482
3524.786688	1156906.557365	41.280487
3525.014146	1156469.265684	41.285492
3524.759794	1156061.536677	41.290496
3524.939240	1155629.954551	41.295501
3524.680678	1155218.470598	41.300506
3524.842456	1154803.194387	41.305511
3524.862551	1154386.110489	41.310516
3524.673626	1153959.373460	41.315520
3524.943393	1153529.591832	41.320525
3524.797155	1153110.446373	41.325530
3524.920148	1152671.530812	41.330535
3525.274536	1152259.051742	41.335540
3524.624985	1151818.677414	41.340544
3524.921718	1151406.898644	41.345549
3524.972507	1150973.724774	41.350554
3525.016329	1150549.798359	41.355559
3524.951178	1150115.057609	41.360564
3524.418868	1149680.831592	41.365568
3524.778202	1149249.738747	41.370573
3524.805004	1148825.771266	41.375578
3524.676299	1148388.245797	41.380583
3524.648774	1147952.088784	41.385588
3524.565156	1147522.443939	41.390592
3524.636482	1147095.107991	41.395597
3524.751842	1146679.862415	41.400602
3524.332022	1146239.363290	41.405607
3524.936417	1145822.168736	41.410612
3524.253497	1145369.601036	41.415616
3524.677647	1144936.438780	41.420621
3524.531933	1144513.575634	41.425626
3524.536182	1144072.446731	41.430631
3524.599176	1143639.427369	41.435636
3524.198365	1143221.149904	41.440640
3524.695664	1142770.346725	41.445645
3524.546572	1142360.781095	41.450650
3524.323512	1141906.987492	41.455655
3524.485544	1141479.562031	41.460660
3524.342044	1141057.276103	41.465664
3524.489933	1140609.098065	41.470669
3524.439489	1140176.288491	41.475674
3524.204036	1139752.395288	41.480679
3524.466254	1139311.491402	41.485684
3524.195988	1138892.280877	41.490688
3524.623304	1138448.430361	41.495693
3524.440031	1138020.687799	41.500698
3524.345101	1137580.078517	41.505703
3524.249507	1137140.477239	41.510708
3524.169851	1136714.986167	41.515712
3524.402834	1136269.655924	41.520717
3524.325610	1135831.652658	41.525722
3524.139572	1135398.950332	41.530727
3524.405672	1134954.454185	41.535732
3524.236837	1134523.482566	41.540736
3524.535720	1134093.729071	41.545741
3524.313566	1133651.009452	41.550746
3524.104522	1133215.567637	41.555751
3524.449007	1132758.901923	41.560756
3524.005128	1132328.747943	41.565760
3524.265297	1131894.546269	41.570765
3524.075693	1131449.927150	41.575770
3524.112791	1131013.979361	41.580775
3524.066280	1130565.745463	41.585780
3524.040375	1130151.033283	41.590784
3524.336565	1129691.354967	41.595789
3524.148665	1129277.837594	41.600794
3524.122083	1128815.759519	41.605799
3524.153467	1128387.491122	41.610804
3524.212068	1127943.489377	41.615808
3524.115436	1127490.439242	41.620813
3523.818344	1127059.264435	41.625818
3523.549501	1126608.831490	41.630823
3523.992437	1126177.273213	41.635828
3523.694410	1125745.231123	41.640832
3523.699134	1125304.063506	41.645837
3523.884700	1124869.111052	41.650842
3523.619484	1124427.249213	41.655847
3523.613212	1123993.589556	41.660852
3523.292544	1123559.565679	41.665856
3523.469330	1123133.992947	41.670861
3523.150068	1122699.803776	41.675866
3523.486949	1122264.138187	41.680871
3523.536667	1121839.816394	41.685876
3523.117509	1121399.062568	41.690880
3523.249854	1120966.277183	41.695885
3523.016483	1120541.899012	41.700890
3522.693648	1120125.884556	41.705895
3523.160156	1119697.513846	41.710900
3522.893037	1119279.804928	41.715904
3523.160102	1118840.061022	41.720909
3522.982970	1118419.411738	41.725914
3522.746389	1117986.827283	41.730919
3522.739357	1117559.888263	41.735924
3522.598192	1117138.370011	41.740928
3522.814112	1116713.995564	41.745933
3523.046817	1116292.635173	41.750938
3522.703605	1115869.906520	41.755943
3522.503979	1115434.631250	41.760948
3522.281340	1115015.915056	41.765952
3522.530877	1114578.207946	41.770957
3522.568558	1114179.980494	41.775962
3522.535905	1113747.401697	41.780967
3522.879110	1113325.694647	41.785972
3522.219913	1112919.095111	41.790976
3522.102066	1112476.317038	41.795981
3522.401035	1112072.261974	41.800986
3522.307404	1111665.378948	41.805991
3522.669512	1111237.589539	41.810996
3521.980650	1110817.095887	41.816000
3522.348839	1110402.979919	41.821005
3522.220466	1109979.751828	41.826010
3521.953944	1109566.725801	41.831015
3522.282675	1109152.233680	41.836020
3522.112207	1108738.841900	41.841024
3522.150616	1108320.228728	41.846029
3522.218211	1107910.361839	41.851034
3521.935376	1107490.018458	41.856039
3522.166862	1107076.719238	41.861044
3521.651638	1106660.932871	41.866048
3521.595511	1106246.280332	41.871053
3521.924883	1105835.066300	41.876058
3521.421739	1105419.946221	41.881063
3521.504873	1105013.677026	41.886068
3521.430249	1104602.531007	41.891072
3521.403540	1104196.600455	41.896077
3521.922595	1103784.721062	41.901082
3521.383111	1103386.744439	41.906087
3521.707871	1102961.265404	41.911092
3521.709347	1102560.367415	41.916096
3521.393739	1102148.500574	41.921101
3521.175090	1101740.122928	41.926106
3521.195673	1101333.491212	41.931111
3521.169618	1100925.593778	41.936116
3520.982454	1100520.847046	41.941120
3521.204178	1100127.571741	41.946125
3521.014832	1099722.861190	41.951130
3521.167861	1099324.470917	41.956135
3521.051433	1098911.941874	41.961140
3520.885023	1098517.274435	41.966144
3521.242740	1098117.709474	41.971149
3521.040175	1097711.128804	41.976154
3521.083870	1097317.869706	41.981159
3521.325547	1096908.094331	41.986164
3520.644594	1096512.312953	41.991168
3520.816497	1096095.790220	41.996173
3520.827153	1095702.897614	42.001178
3520.962878	1095297.706606	42.006183
3520.983191	1094895.088322	42.011188
3520.593110	1094505.524506	42.016192
3520.662856	1094090.778607	42.021197
3520.659879	1093694.679549	42.026202
3520.422820	1093299.834620	42.031207
3520.752912	1092908.122677	42.036212
3520.309475	1092504.924453	42.041216
3520.540399	1092126.481202	42.046221
3520.662911	1091725.621422	42.051226
3520.265583	1091343.779642	42.056231
3520.290981	1090926.596309	42.061236
3519.908203	1090545.270578	42.066240
3520.236048	1090151.731665	42.071245
3519.992866	1089770.424293	42.076250
3519.940886	1089384.172741	42.081255
3520.494970	1088981.314740	42.086260
3520.162158	1088598.502698	42.091264
3519.626610	1088195.286783	42.096269
3519.889615	1087814.333638	42.101274
3519.973595	1087429.358145	42.106279
3520.101150	1087046.360923	42.111284
3519.620249	1086659.411225	42.116288
3519.727604	1086275.308665	42.121293
3519.541037	1085902.059976	42.126298
3519.798680	1085528.904254	42.131303
3519.787217	1085141.098115	42.136308
3519.742437	1084752.119219	42.141312
3519.695808	1084376.729280	42.146317
3519.824361	1083988.626183	42.151322
3519.399367	1083611.136027	42.156327
3519.499883	1083225.956209	42.161332
3519.321862	1082853.168362	42.166336
3519.534588	1082468.300162	42.171341
3519.553730	1082092.646009	42.176346
3519.344449	1081703.476417	42.181351
3519.412977	1081317.399442	42.186356
3519.249627	1080960.310455	42.191360
3519.335611	1080577.536484	42.196365
3519.313021	1080206.269198	42.201370
3519.302964	1079824.513801	42.206375
3519.559009	1079455.740754	42.211380
3519.299961	1079079.540904	42.216384
3519.680777	1078699.562103	42.221389
3519.600507	1078329.712472	42.226394
3519.262398	1077945.479734	42.231399
3519.255999	1077547.723859	42.236404
3519.228082	1077180.284019	42.241408
3518.959102	1076805.081257	42.246413
3518.819037	1076425.798221	42.251418
3518.770168	1076063.952531	42.256423
3519.235397	1075672.128763	42.261428
3518.774872	1075317.120515	42.266432
3518.930201	1074940.759363	42.271437
3519.032885	1074568.319562	42.276442
3518.614062	1074199.494859	42.281447
3518.956757	1073825.619990	42.286452
3518.585823	1073457.794224	42.291456
3518.476599	1073086.057067	42.296461
3518.925223	1072724.292798	42.301466
3518.471633	1072361.403900	42.306471
3518.479403	1071993.513444	42.311476
3518.318386	1071635.525863	42.316480
3518.422073	1071271.704040	42.321485
3518.332269	1070900.295872	42.326490
3518.362244	1070551.722596	42.331495
3518.421185	1070176.587805	42.336500
3518.092004	1069829.854425	42.341504
3518.111718	1069450.734426	42.346509
3518.142441	1069096.780095	42.351514
3517.921744	1068742.267334	42.356519
3518.427722	1068382.514889	42.361524
3518.145431	1068033.063518	42.366528
3518.327278	1067660.333121	42.371533
3518.152897	1067304.950367	42.376538
3517.809931	1066955.247956	42.381543
3518.140663	1066583.478069	42.386548
3518.283547	1066236.439736	42.391552
3518.363693	1065884.097971	42.396557
3518.370137	1065527.704441	42.401562
3518.286371	1065156.964695	42.406567
3518.117390	1064787.849950	42.411572
3517.858928	1064438.262010	42.416576
3518.029355	1064074.336665	42.421581
3517.749193	1063727.883257	42.426586
3517.494833	1063371.104033	42.431591
3517.803272	1063012.187387	42.436596
3517.629085	1062671.233336	42.441600
3517.694866	1062317.124875	42.446605
3517.577965	1061975.348032	42.451610
3517.454544	1061619.589014	42.456615
3517.633757	1061261.638638	42.461620
3517.329091	1060917.997418	42.466624
3517.323446	1060578.619360	42.471629
3517.369686	1060221.104768	42.476634
3517.071802	1059890.400706	42.481639
3517.367164	1059542.144056	42.486644
3517.034443	1059209.959979	42.491648
3517.537665	1058857.965236	42.496653
3517.555116	1058510.074483	42.501658
3517.334054	1058151.891555	42.506663
3517.201532	1057815.158288	42.511668
3517.066634	1057464.046841	42.516672
3517.147537	1057136.391403	42.521677
3517.100798	1056789.655435	42.526682
3517.147456	1056455.700866	42.531687
3517.293169	1056105.034962	42.536692
3516.885420	1055761.667356	42.541696
3516.990782	1055421.471409	42.546701
3517.148393	1055084.812845	42.551706
3516.665394	1054743.997217	42.556711
3516.866862	1054405.940291	42.561716
3516.779486	1054071.092166	42.566720
3516.713237	1053733.327428	42.571725
3516.813771	1053405.350786	42.576730
3516.757060	1053059.346420	42.581735
3516.635500	1052722.686273	42.586740
3516.598531	1052393.514875	42.591744
3516.549016	1052056.223557	42.596749
3516.792553	1051729.281375	42.601754
3516.542766	1051381.949777	42.606759
3516.770409	1051057.189261	42.611764
3516.477785	1050728.346720	42.616768
3516.809618	1050386.935086	42.621773
3516.671124	1050044.228963	42.626778
3516.367041	1049711.178680	42.631783
3516.501944	1049375.912968	42.636788
3516.364808	1049055.341191	42.641792
3516.123961	1048721.931431	42.646797
3516.287657	1048404.167855	42.651802
3516.009176	1048071.883396	42.656807
3516.198047	1047751.278948	42.661812
3516.071817	1047429.549392	42.666816
3515.730511	1047093.741240	42.671821
3516.001068	1046786.004298	42.676826
3515.968411	1046470.575868	42.681831
3516.161921	1046133.462788	42.686836
3515.951624	1045827.972743	42.691840
3515.852421	1045499.946507	42.696845
3516.138419	1045183.523226	42.701850
3515.765156	1044857.242491	42.706855
3516.001250	1044532.097843	42.711860
3515.503515	1044211.691503	42.716864
3515.754614	1043889.307935	42.721869
3515.600390	1043570.450174	42.726874
3515.714949	1043260.128145	42.731879
3515.605001	1042934.657068	42.736884
3515.756213	1042627.965073	42.741888
3515.740271	1042310.751363	42.746893
3515.910563	1041998.030578	42.751898
3515.379901	1041697.777242	42.756903
3515.475141	1041368.025136	42.761908
3515.061395	1041060.276549	42.766912
3515.511468	1040747.922562	42.771917
3515.353060	1040440.967508	42.776922
3515.347769	1040138.996842	42.781927
3515.046233	1039805.060769	42.786932
3515.148495	1039511.738644	42.791937
3515.314300	1039201.568143	42.796941
3515.687890	1038891.346126	42.801946
3515.237038	1038580.662449	42.806951
3515.380707	1038266.769192	42.811956
3515.076683	1037965.696685	42.816961
3515.113062	1037640.471588	42.821965
3515.164783	1037344.625825	42.826970
3515.049787	1037042.505108	42.831975
3515.078322	1036735.701621	42.836980
3514.667645	1036432.145623	42.841985
3515.063832	1036135.405045	42.846989
3514.804260	1035821.246830	42.851994
3514.597913	1035541.503252	42.856999
3514.789047	1035224.334810	42.862004
3514.593688	1034925.982498	42.867009
3514.798779	1034630.160784	42.872013
3514.749523	1034333.687906	42.877018
3514.537557	1034044.483844	42.882023
3514.722566	1033733.328103	42.887028
3514.437797	1033453.105498	42.892033
3514.307505	1033146.711208	42.897037
3514.627175	1032855.422192	42.902042
3514.007047	1032569.499742	42.907047
3514.139261	1032264.465696	42.912052
3514.366130	1031991.539085	42.917057
3514.607985	1031696.233329	42.922061
3514.633947	1031393.008570	42.927066
3514.581843	1031100.527394	42.932071
3514.655165	1030805.299093	42.937076
3514.724820	1030501.244093	42.942081
3514.245916	1030214.790384	42.947085
3514.537383	1029913.281438	42.952090
3513.869977	1029629.056094	42.957095
3513.938157	1029337.043823	42.962100
3513.887293	1029052.493891	42.967105
3513.845021	1028767.346884	42.972109
3514.209931	1028486.283541	42.977114
3513.786525	1028194.195652	42.982119
3514.294709	1027915.695572	42.987124
3514.114960	1027619.856230	42.992129
3513.886809	1027340.479962	42.997133
3514.064617	1027058.213021	43.002138
3513.771758	1026770.001775	43.007143
3514.307089	1026494.817867	43.012148
3513.771591	1026205.551587	43.017153
3513.604027	1025925.900871	43.022157
3513.713138	1025628.745704	43.027162
3513.815929	1025366.661259	43.032167
3513.990321	1025066.364024	43.037172
3513.830090	1024801.097864	43.042177
3513.822580	1024514.274322	43.047181
3513.858367	1024237.026067	43.052186
3513.538697	1023947.607524	43.057191
3513.684953	1023674.578832	43.062196
3513.670061	1023396.327813	43.067201
3513.716422	1023111.556581	43.072205
3513.783755	1022843.057487	43.077210
3513.486741	1022561.805595	43.082215
3513.731308	1022288.208323	43.087220
3513.636609	1022014.847538	43.092225
3513.139724	1021737.369368	43.097229
3513.367438	1021459.564142	43.102234
3513.107245	1021185.608253	43.107239
3513.201314	1020915.169554	43.112244
3513.129163	1020647.849276	43.117249
3513.013951	1020382.366487	43.122253
3513.167985	1020115.856674	43.127258
3513.175327	1019852.947968	43.132263
3513.389527	1019574.372513	43.137268
3512.977356	1019314.321281	43.142273
3513.233684	1019029.114092	43.147277
3513.319755	1018761.969014	43.152282
3512.826334	1018494.615552	43.157287
3512.943329	1018238.794126	43.162292
3512.840419	1017962.519990	43.167297
3512.628003	1017713.910526	43.172301
3512.819996	1017446.103096	43.177306
3512.930142	1017196.738218	43.182311
3513.140702	1016915.507861	43.187316
3512.600960	1016657.878343	43.192321
3512.682984	1016390.329932	43.197325
3513.244886	1016119.971496	43.202330
3512.873460	1015867.811636	43.207335
3512.739429	1015613.853755	43.212340
3512.905214	1015342.940672	43.217345
3512.651180	1015078.298007	43.222349
3512.921486	1014820.936371	43.227354
3512.804720	1014559.451090	43.232359
3513.073922	1014302.454355	43.237364
3512.821431	1014034.169166	43.242369
3512.573509	1013787.722691	43.247373
3512.617634	1013509.942915	43.252378
3512.470398	1013271.421555	43.257383
3512.563191	1012990.499976	43.262388
3512.508158	1012749.221533	43.267393
3512.484589	1012476.938854	43.272397
3512.753433	1012218.195592	43.277402
3512.270452	1011977.537458	43.282407
3512.566312	1011713.811817	43.287412
3512.366448	1011461.231858	43.292417
3512.328694	1011215.998443	43.297421
3512.027311	1010958.068550	43.302426
3512.036317	1010719.121842	43.307431
3512.325340	1010467.388552	43.312436
3512.309402	1010199.561923	43.317441
3512.022047	1009962.867176	43.322445
3512.460927	1009712.533312	43.327450
3512.052369	1009468.937208	43.332455
3512.441661	1009202.551610	43.337460
3512.329242	1008960.634376	43.342465
3512.338235	1008698.175767	43.347469
3512.227188	1008444.376691	43.352474
3512.221984	1008193.951376	43.357479
3512.107229	1007949.366291	43.362484
3512.250957	1007690.630270	43.367489
3512.029518	1007458.000256	43.372493
3512.198992	1007194.570213	43.377498
3511.704999	1006967.021050	43.382503
3511.658664	1006717.801115	43.387508
3511.798971	1006469.803652	43.392513
3511.666003	1006230.592927	43.397517
3511.946592	1005986.732954	43.402522
3511.603986	1005762.514247	43.407527
3511.770011	1005513.789765	43.412532
3511.704730	1005271.706641	43.417537
3511.517245	1005033.718691	43.422541
3511.645278	1004797.127890	43.427546
3511.262457	1004553.120762	43.432551
3511.447652	1004325.353282	43.437556
3511.470281	1004085.053246	43.442561
3511.479902	1003860.214591	43.447565
3511.550823	1003611.130173	43.452570
3511.367728	1003382.509708	43.457575
3511.334320	1003134.297174	43.462580
3511.176448	1002912.562172	43.467585
3511.091715	1002678.058527	43.472589
3511.283036	1002444.278227	43.477594
3511.159660	1002232.047866	43.482599
3511.315906	1001991.928852	43.487604
3511.348133	1001768.463190	43.492609
3511.177639	1001542.978125	43.497613
3511.262110	1001311.601936	43.502618
3510.975269	1001073.171635	43.507623
3510.929135	1000860.585102	43.512628
3511.134724	1000618.258138	43.517633
3510.936213	1000396.333880	43.522637
3510.974404	1000156.643230	43.527642
3510.597928	999947.484275	43.532647
3510.955288	999715.413767	43.537652
3511.065437	999498.076912	43.542657
3510.837357	999266.376540	43.547661
3510.914538	999059.446980	43.552666
3510.926634	998836.745309	43.557671
3510.758485	998601.502255	43.562676
3511.011337	998387.897238	43.567681
3510.657112	998165.619076	43.572685
3511.058706	997944.960798	43.577690
3510.587817	997729.502305	43.582695
3510.845231	997498.526271	43.587700
3510.841301	997281.805039	43.592705
3510.744361	997060.902264	43.597709
3510.878716	996833.036487	43.602714
3510.626783	996615.259094	43.607719
3510.686041	996398.883388	43.612724
3510.333932	996184.515664	43.617729
3510.097725	995972.653866	43.622733
3510.631521	995740.586472	43.627738
3510.542070	995536.771046	43.632743
3510.608590	995332.922612	43.637748
3510.589793	995111.931086	43.642753
3510.358980	994898.761561	43.647757
3510.472756	994678.218548	43.652762
3510.530829	994460.697206	43.657767
3510.405297	994256.646857	43.662772
3510.231899	994040.804326	43.667777
3509.970195	993825.747850	43.672781
3510.578310	993619.312092	43.677786
3510.396035	993401.887258	43.682791
3510.368416	993201.779227	43.687796
3510.281463	992974.574821	43.692801
3510.113865	992771.842771	43.697805
3510.091875	992561.573081	43.702810
3509.960494	992361.160081	43.707815
3510.247688	992152.384167	43.712820
3510.244132	991946.865866	43.717825
3509.938670	991725.887314	43.722829
3509.942388	991518.499823	43.727834
3509.721962	991323.915159	43.732839
3509.532134	991136.242048	43.737844
3509.626239	990931.451046	43.742849
3509.394812	990745.039560	43.747853
3509.685041	990535.911260	43.752858
3509.504477	990364.594637	43.757863
3509.743687	990139.953891	43.762868
3509.630857	989947.059899	43.767873
3509.506350	989757.477453	43.772877
3509.879412	989553.566261	43.777882
3509.945925	989355.940888	43.782887
3509.686535	989150.461227	43.787892
3509.696166	988957.318433	43.792897
3509.335349	988762.376628	43.797901
3509.721676	988570.719498	43.802906
3509.700689	988371.025706	43.807911
3509.652588	988183.329409	43.812916
3509.570939	987993.193344	43.817921
3509.669457	987815.705037	43.822925
3509.770975	987590.205835	43.827930
3509.528343	987403.784318	43.832935
3509.167375	987203.520143	43.837940
3509.161721	987019.486466	43.842945
3509.425036	986819.105959	43.847949
3509.470477	986629.879307	43.852954
3509.408061	986432.173717	43.857959
3509.624541	986247.200200	43.862964
3509.349354	986049.321187	43.867969
3509.224246	985866.538729	43.872973
3509.193916	985665.970857	43.877978
3509.205777	985484.812875	43.882983
3509.104006	985304.253517	43.887988
3509.239541	985107.933558	43.892993
3509.431012	984933.073363	43.897997
3509.327684	984739.513338	43.903002
3509.181258	984559.621102	43.908007
3508.981174	984367.235858	43.913012
3509.165013	984180.736303	43.918017
3509.220985	984003.331562	43.923021
3509.147584	983812.468870	43.928026
3508.863235	983634.034705	43.933031
3509.118888	983427.287396	43.938036
3509.350039	983251.783295	43.943041
3509.117950	983050.375527	43.948045
3509.310365	982874.085006	43.953050
3509.087452	982680.670142	43.958055
3508.944262	982500.126516	43.963060
3508.965746	982318.768767	43.968065
3508.756290	982152.678952	43.973069
3509.336832	981952.368246	43.978074
3509.033094	981776.516237	43.983079
3508.911242	981581.289415	43.988084
3508.818412	981405.488919	43.993089
3509.029333	981232.856427	43.998093
3509.072364	981039.439855	44.003098
3508.945551	980855.324937	44.008103
3508.990955	980667.463513	44.013108
3508.789229	980480.515855	44.018113
3508.572588	980315.839208	44.023117
3508.893028	980135.437568	44.028122
3508.941267	979963.868234	44.033127
3509.062863	979787.689549	44.038132
3508.859704	979597.684405	44.043137
3508.887435	979433.332919	44.048141
3508.774273	979240.956038	44.053146
3508.414323	979077.733038	44.058151
3508.785052	978889.759621	44.063156
3508.729277	978705.856931	44.068161
3508.486989	978534.292560	44.073165
3508.740444	978364.205057	44.078170
3508.715641	978183.700998	44.083175
3508.584995	978013.568604	44.088180
3508.765385	977825.102893	44.093185
3508.434622	977659.488890	44.098189
3508.743667	977481.644453	44.103194
3508.427507	977312.205971	44.108199
3508.493971	977143.090451	44.113204
3508.334246	976972.247639	44.118209
3508.077681	976793.888479	44.123213
3508.531456	976626.160239	44.128218
3508.383209	976450.998596	44.133223
3508.237403	976287.171889	44.138228
3508.663843	976111.514152	44.143233
3508.466268	975956.192274	44.148237
3508.464208	975775.217440	44.153242
3508.197380	975621.560037	44.158247
3508.579452	975439.924689	44.163252
3508.384721	975275.392647	44.168257
3508.180958	975112.128566	44.173261
3508.427842	974933.041819	44.178266
3508.307240	974770.243238	44.183271
3508.444557	974580.699944	44.188276
3508.263734	974428.756667	44.193281
3508.230626	974262.799780	44.198285
3508.231376	974103.385236	44.203290
3508.181209	973935.172232	44.208295
3508.040122	973763.546002	44.213300
3508.390437	973596.039549	44.218305
3507.850146	973432.880863	44.223309
3508.373673	973263.379903	44.228314
3508.133659	973107.987799	44.233319
3508.220474	972948.233509	44.238324
3508.135952	972783.709601	44.243329
3507.983291	972632.887976	44.248333
3508.193534	972453.436341	44.253338
3507.988855	972289.602861	44.258343
3507.977210	972124.461046	44.263348
3508.052266	971981.215951	44.268353
3507.865192	971812.278361	44.273357
3508.050304	971652.276116	44.278362
3507.978962	971484.777478	44.283367
3508.010660	971331.738661	44.288372
3508.034423	971160.985890	44.293377
3507.633576	971002.236259	44.298381
3507.965284	970835.141554	44.303386
3507.805994	970684.563379	44.308391
3507.708770	970520.661693	44.313396
3507.869238	970349.960149	44.318401
3507.825678	970216.183523	44.323405
3507.600391	970042.404593	44.328410
3507.660751	969900.186574	44.333415
3507.772050	969728.495925	44.338420
3507.699606	969583.257764	44.343425
3507.578986	969426.375974	44.348429
3507.997908	969258.829531	44.353434
3507.676392	969102.755067	44.358439
3507.709659	968966.293726	44.363444
3507.294479	968794.955562	44.368449
3507.305460	968647.820058	44.373453
3507.481941	968493.702815	44.378458
3507.055247	968362.687253	44.383463
3507.199251	968209.742542	44.388468
3507.400382	968065.987405	44.393473
3507.005024	967921.152032	44.398477
3507.534864	967780.958195	44.403482
3507.344244	967627.857302	44.408487
3507.357870	967473.445798	44.413492
3507.624569	967336.221909	44.418497
3507.286824	967175.006060	44.423501
3507.436255	967041.613331	44.428506
3507.049499	966894.204688	44.433511
3506.984887	966744.291025	44.438516
3507.415158	966604.966280	44.443521
3506.867557	966445.723138	44.448525
3507.064029	966324.057887	44.453530
3506.914291	966174.045449	44.458535
3507.290737	966040.788000	44.463540
3506.937114	965902.652697	44.468545
3506.982666	965773.067385	44.473549
3507.290383	965616.500777	44.478554
3506.744672	965482.500769	44.483559
3507.014908	965330.438192	44.488564
3507.307351	965196.685286	44.493569
3506.669979	965065.629269	44.498573
3506.995099	964922.558806	44.503578
3506.746126	964776.836447	44.508583
3506.698585	964657.919069	44.513588
3506.486976	964511.791994	44.518593
3505.936784	964389.816978	44.523597
3506.717675	964244.695264	44.528602
3506.610635	964134.888063	44.533607
3506.572351	964003.905132	44.538612
3506.597552	963884.567906	44.543617
3506.544089	963758.284730	44.548621
3506.583611	963623.459188	44.553626
3506.556029	963480.508980	44.558631
3506.593577	963365.666177	44.563636
3506.711892	963212.102923	44.568641
3506.654232	963082.376063	44.573645
3506.804931	962940.852946	44.578650
3506.646029	962811.920608	44.583655
3506.640703	962684.920015	44.588660
3506.687966	962564.179859	44.593665
3506.870315	962422.736806	44.598669
3506.738556	962299.080559	44.603674
3506.639302	962161.793603	44.608679
3506.444908	962028.145322	44.613684
3506.736083	961891.081636	44.618689
3506.550884	961771.931329	44.623693
3506.455543	961642.766339	44.628698
3506.243322	961518.812562	44.633703
3506.402307	961386.953517	44.638708
3506.438695	961249.034371	44.643713
3506.233360	961127.717609	44.648717
3506.551532	961001.704902	44.653722
3506.640792	960876.805443	44.658727
3506.512141	960745.175157	44.663732
3506.308711	960627.180544	44.668737
3506.285451	960496.311469	44.673741
3506.644505	960378.611262	44.678746
3506.307438	960253.964607	44.683751
3506.390153	960120.030376	44.688756
3506.913441	959987.785232	44.693761
3506.635069	959866.355922	44.698765
3506.692102	959722.318133	44.703770
3506.690422	959609.073747	44.708775
3506.615952	959467.894674	44.713780
3506.606988	959334.643674	44.718785
3506.671812	959215.399361	44.723789
3507.000129	959072.379279	44.728794
3506.693904	958949.366334	44.733799
3506.618408	958814.643392	44.738804
3506.681062	958689.210656	44.743809
3506.383901	958574.033346	44.748813
3506.800685	958424.412212	44.753818
3506.748769	958302.324277	44.758823
3506.465467	958162.226443	44.763828
3506.548833	958049.525894	44.768833
3506.410221	957907.828854	44.773837
3506.306370	957801.038935	44.778842
3506.475440	957669.583688	44.783847
3506.025114	957545.976076	44.788852
3506.003665	957428.376488	44.793857
3505.885201	957307.455506	44.798861
3505.921086	957189.253082	44.803866
3505.976302	957060.058779	44.808871
3505.802255	956952.774278	44.813876
3506.326720	956838.996526	44.818881
3505.974111	956722.221872	44.823885
3506.028032	956609.694279	44.828890
3506.073873	956483.922122	44.833895
3506.073139	956376.107859	44.838900
3506.093096	956259.164379	44.843905
3506.280150	956137.383745	44.848909
3506.186058	956014.175210	44.853914
3506.326004	955902.993226	44.858919
3505.881170	955768.456277	44.863924
3506.407796	955659.570277	44.868929
3505.915951	955537.444911	44.873933
3506.158310	955430.878460	44.878938
3506.081248	955319.772217	44.883943
3506.161112	955198.978992	44.888948
3506.090918	955092.170040	44.893953
3506.243504	954957.587958	44.898957
3506.047079	954836.831651	44.903962
3506.162040	954726.254660	44.908967
3505.772926	954618.723189	44.913972
3505.574065	954512.114550	44.918977
3505.767036	954390.518381	44.923981
3505.533169	954290.223504	44.928986
3505.829781	954183.143789	44.933991
3506.000555	954082.108624	44.938996
3506.215684	953968.437846	44.944001
3505.850576	953853.616577	44.949005
3505.862206	953741.122128	44.954010
3505.784653	953631.414039	44.959015
3505.722335	953528.684430	44.964020
3505.790074	953420.382811	44.969025
3505.296538	953304.422367	44.974029
3505.683021	953190.897397	44.979034
3505.804046	953093.677617	44.984039
3505.929125	952989.662593	44.989044
3505.574703	952874.339181	44.994049
3505.234598	952773.266605	44.999053
3505.535208	952681.367282	45.004058
3505.352584	952576.629114	45.009063
3505.417847	952485.147751	45.014068
3505.879153	952369.678607	45.019073
3505.440979	952280.285863	45.024077
3505.688049	952164.943076	45.029082
3505.459760	952060.775999	45.034087
3505.590843	951944.394763	45.039092
3505.799350	951851.538806	45.044097
3505.474980	951732.835442	45.049101
3505.811517	951626.365499	45.054106
3505.655965	951528.970167	45.059111
3505.455604	951432.154573	45.064116
3505.592888	951329.252233	45.069121
3505.216536	951224.614028	45.074125
3505.585865	951123.679157	45.079130
3505.500578	951020.137326	45.084135
3505.476928	950921.560225	45.089140
3505.600368	950825.254111	45.094145
3505.296829	950732.175094	45.099149
3505.329792	950614.152696	45.104154
3505.151737	950537.129847	45.109159
3505.345309	950418.215032	45.114164
3505.780967	950318.402061	45.119169
3505.150618	950232.642695	45.124173
3505.300963	950121.386029	45.129178
3505.471986	950023.238256	45.134183
3505.242691	949935.301861	45.139188
3505.574453	949828.221061	45.144193
3505.145788	949728.347539	45.149197
3505.305095	949630.960078	45.154202
3505.389598	949533.200148	45.159207
3505.097455	949439.521418	45.164212
3505.422738	949346.505210	45.169217
3504.958915	949258.404389	45.174221
3505.340656	949144.216231	45.179226
3505.046042	949054.935130	45.184231
3505.137410	948939.258325	45.189236
3505.279266	948856.221243	45.194241
3505.050788	948758.881164	45.199245
3505.409620	948670.251780	45.204250
3505.335244	948568.478094	45.209255
3505.223507	948482.795634	45.214260
3505.167481	948381.972807	45.219265
3505.013799	948289.590970	45.224269
3505.360584	948190.134447	45.229274
3505.084710	948106.771057	45.234279
3504.948490	948009.497398	45.239284
3504.943963	947912.008682	45.244289
3505.146539	947807.875971	45.249293
3505.559968	947721.807072	45.254298
3504.966490	947633.125194	45.259303
3504.902950	947525.391280	45.264308
3505.053458	947452.769555	45.269313
3505.130142	947358.034494	45.274317
3505.226149	947257.547777	45.279322
3505.024235	947172.241534	45.284327
3505.092456	947069.744350	45.289332
3504.916058	946973.224055	45.294337
3504.947956	946892.759685	45.299341
3504.993770	946805.586660	45.304346
3505.220998	946718.669653	45.309351
3504.578937	946626.817459	45.314356
3504.809690	946526.390137	45.319361
3504.735831	946445.074092	45.324365
3504.662406	946352.644401	45.329370
3504.974315	946290.996289	45.334375
3504.900187	946189.175692	45.339380
3504.963093	946099.305592	45.344385
3504.720229	946009.388494	45.349389
3504.940565	945916.902645	45.354394
3504.946496	945832.977145	45.359399
3504.976763	945749.429506	45.364404
3504.933429	945658.132152	45.369409
3504.586300	945575.889387	45.374413
3504.950823	945480.593515	45.379418
3504.826354	945399.173580	45.384423
3504.984665	945310.807114	45.389428
3504.992806	945218.631211	45.394433
3504.307964	945134.424914	45.399437
3504.965167	945051.816782	45.404442
3504.953524	944961.843432	45.409447
3504.578496	944875.473829	45.414452
3504.760189	944784.028209	45.419457
3504.306494	944705.430531	45.424461
3504.367852	944633.263106	45.429466
3504.461288	944550.069065	45.434471
3504.852514	944481.295044	45.439476
3504.702787	944367.568169	45.444481
3504.247241	944314.647906	45.449485
3504.440814	944222.519616	45.454490
3504.583775	944155.123866	45.459495
3504.298284	944065.755121	45.464500
3504.127392	943988.345904	45.469505
3504.146753	943911.191721	45.474509
3504.536704	943843.367889	45.479514
3504.436228	943752.717344	45.484519
3504.756502	943669.567702	45.489524
3504.901058	943590.279547	45.494529
3504.496269	943502.933562	45.499533
3504.570372	943428.446961	45.504538
3504.441394	943345.366139	45.509543
3504.387532	943274.924171	45.514548
3504.311244	943191.736366	45.519553
3504.248000	943124.073670	45.524557
3504.511253	943026.353127	45.529562
3504.104811	942969.289220	45.534567
3504.032903	942893.189427	45.539572
3504.311785	942816.551440	45.544577
3504.208539	942746.110457	45.549581
3504.306759	942659.913689	45.554586
3504.226882	942588.699819	45.559591
3504.033955	942526.706769	45.564596
3504.320999	942434.435595	45.569601
3504.122945	942378.577178	45.574605
3504.259103	942292.080478	45.579610
3504.341429	942236.174357	45.584615
3504.115846	942147.529794	45.589620
3504.551188	942078.237436	45.594625
3504.163344	941999.204525	45.599629
3504.140447	941934.779536	45.604634
3504.208409	941842.150473	45.609639
3504.357567	941782.680969	45.614644
3504.349290	941703.293421	45.619649
3504.215982	941622.199367	45.624653
3504.091950	941549.923884	45.629658
3504.457044	941484.470596	45.634663
3504.193759	941409.818975	45.639668
3503.965002	941330.557965	45.644673
3504.135652	941268.585978	45.649677
3504.071154	941190.734134	45.654682
3504.455133	941129.013031	45.659687
3503.907066	941049.320889	45.664692
3504.214954	940981.665186	45.669697
3503.924240	940902.503785	45.674701
3504.098559	940840.526125	45.679706
3503.935414	940762.492361	45.684711
3503.606781	940700.595883	45.689716
3504.158672	940630.497959	45.694721
3504.035275	940570.004649	45.699725
3503.820356	940508.662584	45.704730
3504.100320	940427.769650	45.709735
3503.806277	940368.357069	45.714740
3504.185820	940287.541475	45.719745
3504.036742	940231.652038	45.724749
3504.036699	940140.442671	45.729754
3504.122987	940086.047476	45.734759
3503.819219	940019.151465	45.739764
3504.318071	939957.205818	45.744769
3504.249123	939880.869843	45.749773
3504.277078	939814.875736	45.754778
3504.311639	939735.930869	45.759783
3504.037196	939671.327607	45.764788
3504.370568	939591.851762	45.769793
3504.251329	939531.921303	45.774797
3504.345041	939444.713081	45.779802
3504.028535	939371.959615	45.784807
3503.782788	939282.502428	45.789812
3504.264429	939157.430655	45.794817
3503.671791	938979.291246	45.799821
3504.304277	938727.937301	45.804826
3504.154007	938434.678172	45.809831
3503.945656	938055.923144	45.814836
3503.982564	937622.501742	45.819841
3503.567380	937129.429217	45.824845
3503.808281	936568.924284	45.829850
3503.353686	935947.043343	45.834855
3503.301286	935263.391965	45.839860
3503.629844	934517.469769	45.844865
3503.358346	933679.931799	45.849869
3503.348308	932789.970996	45.854874
3503.207376	931819.960357	45.859879
3502.521376	930781.550345	45.864884
3503.017593	929666.921075	45.869889
3502.965894	928484.288529	45.874893
3502.717806	927201.918969	45.879898
3502.394310	925856.073486	45.884903
3501.912905	924427.672639	45.889908
3501.879574	922905.871640	45.894913
3501.617197	921323.044335	45.899917
3501.567440	919650.375167	45.904922
3501.238096	917898.843492	45.909927
3501.049860	916061.273227	45.914932
3500.711725	914134.255023	45.919937
3500.276621	912132.343254	45.924941
3500.249755	910014.386401	45.929946
3499.635028	907845.257358	45.934951
3499.312101	905572.825544	45.939956
3499.177065	903214.368266	45.944961
3498.580124	900778.583759	45.949965
3498.621017	898264.036330	45.954970
3498.219847	895652.240116	45.959975
3497.749643	892952.003292	45.964980
3497.408695	890173.241218	45.969985
3496.427624	887311.520692	45.974989
3496.306484	884359.214075	45.979994
3495.961225	881317.922899	45.984999
3495.584075	878220.461850	45.990004
3495.250455	874992.411550	45.995009
3494.684198	871726.532025	46.000013
3494.293588	868325.563140	46.005018
3493.858839	864869.030581	46.010023
3493.065352	861318.489867	46.015028
3492.730189	857687.671488	46.020033
3492.118346	853977.350501	46.025037
3491.583058	850172.339532	46.030042
3491.180482	846273.450620	46.035047
3490.308226	842280.824517	46.040052
3489.820934	838229.551202	46.045057
3489.186305	834088.373535	46.050061
3488.732334	829869.844250	46.055066
3488.326611	825543.345587	46.060071
3487.191891	821155.210726	46.065076
3487.029579	816648.850670	46.070081
3486.201360	812070.536263	46.075085
3485.517211	807407.614416	46.080090
3484.716596	802680.254161	46.085095
3483.571758	797849.850662	46.090100
3483.308685	792942.116732	46.095105
3482.566300	787935.519174	46.100109
3481.310775	782866.013400	46.105114
3480.740416	777688.502803	46.110119
3480.146596	772438.250183	46.115124
3479.649790	767080.313534	46.120129
3478.340497	761666.425067	46.125133
3477.517779	756129.635211	46.130138
3476.633026	750549.533244	46.135143
3475.518474	744859.049305	46.140148
3474.831213	739098.227226	46.145153
3473.868364	733228.509750	46.150157
3472.841279	727296.324823	46.155162
3471.627390	721272.259806	46.160167
3470.793932	715151.869681	46.165172
3469.847987	708938.324617	46.170177
3468.969452	702666.905081	46.175181
3467.901909	696273.038597	46.180186
3466.791473	689825.554865	46.185191
3465.651495	683277.144076	46.190196
3464.546455	676644.361150	46.195201
3463.394111	669929.419826	46.200205
3462.081191	663127.061099	46.205210
3461.042995	656243.563964	46.210215
3459.730519	649282.742040	46.215220
3458.937788	642228.192751	46.220225
3457.431263	635094.892916	46.225229
3455.864111	627874.912132	46.230234
3454.875896	620577.548835	46.235239
3453.456895	613194.697095	46.240244
3452.176452	605749.042491	46.245249
3450.788536	598199.282633	46.250253
3449.230429	590567.055075	46.255258
3447.909863	582875.741210	46.260263
3446.494490	575091.191761	46.265268
3444.886143	567211.111864	46.270273
3443.451417	559264.064770	46.275277
3441.921076	551231.256044	46.280282
3440.359785	543114.881460	46.285287
3438.628034	534935.502053	46.290292
3437.564240	526673.778878	46.295297
3435.224137	518325.800491	46.300301
3433.596057	509914.504923	46.305306
3432.169359	501408.522833	46.310311
3430.178088	492857.837320	46.315316
3428.527507	484207.869715	46.320321
3426.678963	475488.108439	46.325325
3424.666016	466706.119607	46.330330
3422.936205	457829.523525	46.335335
3420.894522	448905.791226	46.340340
3419.156408	439883.544850	46.345345
3417.105039	430826.094599	46.350349
3414.780277	421666.911145	46.355354
3412.738367	412455.609092	46.360359
3410.107030	403161.783191	46.365364
3408.091836	393814.222838	46.370369
3405.862929	384416.090545	46.375373
3403.413823	374951.834650	46.380378
3401.193481	365416.653693	46.385383
3398.824836	355836.516291	46.390388
3396.442041	346195.606149	46.395393
3393.957431	336500.304676	46.400397
3391.326701	326742.157854	46.405402
3388.736333	316934.239286	46.410407
3385.830249	307078.039718	46.415412
3383.068352	297177.570972	46.420417
3379.865996	287222.407188	46.425421
3377.325080	277220.949252	46.430426
3374.363675	267188.995798	46.435431
3371.052685	257112.389949	46.440436
3367.927966	246990.503732	46.445441
3364.515648	236850.182346	46.450445
3361.234624	226667.092023	46.455450
3357.796918	216407.021541	46.460455
3354.037716	206151.346223	46.465460
3350.848419	195884.883439	46.470465
3346.676684	185621.329855	46.475469
3342.687432	175334.918068	46.480474
3338.452431	165034.230058	46.485479
3334.303487	154744.757987	46.490484
3329.903797	144441.328694	46.495489
3324.957399	134151.940955	46.500493
3320.087243	123879.951284	46.505498
3314.884248	113613.754184	46.510503
3309.132590	103398.545780	46.515508
3303.157305	93204.862557	46.520513
3295.937762	83087.656015	46.525517
3287.272369	73064.396780	46.530522
3272.400703	63289.882832	46.535527
3245.948797	54004.750692	46.540532
3213.579730	45175.040305	46.545537
3173.289820	37060.445898	46.550541
3128.580110	29683.619511	46.555546
3085.763943	23104.287052	46.560551
3046.336343	17328.117909	46.565556
3011.338205	12371.570554	46.570561
2980.145310	8218.920663	46.575565
2952.895064	4819.972384	46.580570
2928.326504	2163.082275	46.585575
2894.692442	493.126674	46.590580
2833.880289	328.251602	46.595585
2803.466398	348.104475	46.600589
2805.896930	340.135048	46.605594
2827.992525	330.934671	46.610599
2854.499217	334.390910	46.615604
2876.276965	315.063520	46.620609
2888.905978	321.093632	46.625613
2892.744467	335.485095	46.630618
2891.157890	317.249602	46.635623
2886.068282	319.117275	46.640628
2881.297221	319.417942	46.645633
2876.943193	306.725351	46.650637
2873.774693	326.865610	46.655642
2871.408663	308.021211	46.660647
2869.124568	319.622906	46.665652
2867.061612	303.832618	46.670657
2864.765597	290.716926	46.675661
2861.811341	304.556700	46.680666
2859.279623	296.893944	46.685671
2855.922020	309.695521	46.690676
2853.407805	297.057461	46.695681
2850.072393	295.058579	46.700685
2847.348288	304.319006	46.705690
2844.517491	302.262191	46.710695
2841.071688	298.138213	46.715700
2837.783898	299.134527	46.720705
2834.480435	301.241280	46.725709
2831.078909	287.112204	46.730714
2828.436538	291.422750	46.735719
2825.060705	295.493940	46.740724
2822.317536	301.717282	46.745729
2818.802765	290.386477	46.750733
2815.719215	288.105282	46.755738
2812.243234	284.074492	46.760743
2808.911602	296.097280	46.765748
2805.718801	283.673426	46.770753
2802.649957	278.741032	46.775757
2798.902655	276.084797	46.780762
2795.600613	272.184960	46.785767
2792.015634	275.317940	46.790772
2788.797105	279.909932	46.795777
2785.600027	265.713754	46.800781
2782.537032	282.103134	46.805786
2779.270060	265.087001	46.810791
2775.386997	275.898107	46.815796
2772.189286	271.276712	46.820801
2768.884957	268.296299	46.825805
2765.714854	270.522061	46.830810
2762.548682	275.469451	46.835815
2757.989081	280.789913	46.840820
2754.481930	268.794773	46.845825
2751.624239	280.202373	46.850829
2748.122202	257.227929	46.855834
2745.296490	268.672473	46.860839
2741.489119	271.617017	46.865844
2738.490176	266.486385	46.870849
2734.725485	272.778915	46.875853
2730.992037	259.099154	46.880858
2728.092029	271.404251	46.885863
2724.227825	266.730682	46.890868
2721.120673	265.375511	46.895873
2717.493753	267.827741	46.900877
2713.993280	264.847137	46.905882
2710.441715	262.492316	46.910887
2707.245915	248.351529	46.915892
2704.341668	264.380998	46.920897
2701.125890	246.766165	46.925901
2697.186125	261.878048	46.930906
2693.712550	241.740019	46.935911
2689.861177	260.039630	46.940916
2686.865024	247.292528	46.945921
2683.368518	259.265660	46.950925
2679.628773	254.382880	46.955930
2675.969384	251.843719	46.960935
2672.871056	258.258133	46.965940
2669.002437	249.242030	46.970945
2665.712456	247.502992	46.975949
2662.460051	246.402344	46.980954
2658.551594	254.934101	46.985959
2654.862858	238.530292	46.990964
2652.326732	249.815326	46.995969
2648.886043	255.360062	47.000973
2644.856891	250.174217	47.005978
2642.000688	248.597667	47.010983
2638.545523	232.904714	47.015988
2634.905071	247.539306	47.020993
2630.905360	251.620302	47.025997
2627.603507	242.034295	47.031002
2624.790991	245.184696	47.036007
2620.522016	248.922692	47.041012
2617.219791	237.823947	47.046017
2614.008637	238.381741	47.051021
2610.463499	250.680465	47.056026
2607.221661	242.540559	47.061031
2603.615737	246.781165	47.066036
2599.789499	244.749491	47.071041
2596.619450	242.967921	47.076045
2592.870375	246.867819	47.081050
2589.780729	236.179742	47.086055
2585.955244	251.908712	47.091060
2582.451057	246.149503	47.096065
2578.806024	240.740746	47.101069
2575.696980	243.259269	47.106074
2572.831465	232.163912	47.111079
2569.141407	248.170253	47.116084
2565.701645	239.924006	47.121089
2562.034226	237.560940	47.126093
2557.969237	235.094543	47.131098
2554.651835	223.444324	47.136103
2551.031238	238.870586	47.141108
2547.535916	236.622785	47.146113
2544.635804	231.110159	47.151117
2540.836507	238.924328	47.156122
2537.590856	224.755773	47.161127
2533.757653	244.292157	47.166132
2530.460106	230.020881	47.171137
2527.173410	233.019942	47.176141
2522.951489	224.617700	47.181146
2519.692074	239.223820	47.186151
2516.448765	226.920174	47.191156
2513.195050	218.883699	47.196161
2509.529140	227.604082	47.201165
2506.156795	220.043233	47.206170
2502.596799	233.357174	47.211175
2498.888900	227.185215	47.216180
2495.226459	230.502345	47.221185
2491.996664	226.634354	47.226189
2488.545114	240.239790	47.231194
2485.285606	218.297336	47.236199
2481.677340	234.140944	47.241204
2477.989915	216.038891	47.246209
2474.640385	237.134303	47.251213
2471.269677	230.872127	47.256218
2467.785138	228.211512	47.261223
2464.476438	235.828599	47.266228
2460.807755	228.880621	47.271233
2457.039542	223.896222	47.276237
2453.369304	231.592661	47.281242
2450.532617	228.876518	47.286247
2446.348807	236.032209	47.291252
2443.060369	233.278892	47.296257
2439.617166	216.236642	47.301261
2436.297506	227.115737	47.306266
2433.026016	224.297778	47.311271
2428.951459	228.874890	47.316276
2425.638992	231.003608	47.321281
2422.317564	234.082821	47.326285
2418.693930	226.281709	47.331290
2415.401829	228.434891	47.336295
2411.560934	225.313676	47.341300
2408.396408	218.978767	47.346305
2404.834242	227.438514	47.351309
2401.006189	234.336185	47.356314
2398.056973	217.006711	47.361319
2394.253844	224.809530	47.366324
2390.660782	214.499754	47.371329
2387.374294	217.635958	47.376333
2384.085609	212.932891	47.381338
2380.876566	220.747637	47.386343
2376.715624	212.437051	47.391348
2373.045068	205.822091	47.396353
2369.855578	202.187827	47.401357
2366.341686	222.479616	47.406362
2363.046270	221.409772	47.411367
2359.139009	224.376090	47.416372
2355.901717	218.324890	47.421377
2352.407809	218.121380	47.426381
2348.734140	215.405599	47.431386
2345.553649	211.956407	47.436391
2341.699791	216.717941	47.441396
2338.601105	201.203966	47.446401
2334.798725	207.265209	47.451405
2331.298332	206.474923	47.456410
2328.211216	207.927951	47.461415
2324.356363	216.923819	47.466420
2320.762319	204.629115	47.471425
2317.501166	211.860375	47.476429
2314.188780	199.117623	47.481434
2310.455377	211.564367	47.486439
2306.904811	212.058702	47.491444
2303.252472	205.647942	47.496449
2299.982479	203.669906	47.501453
2296.559442	205.214552	47.506458
2293.072778	193.121761	47.511463
2289.474120	208.800355	47.516468
2285.943433	203.486556	47.521473
2282.687767	202.430417	47.526477
2279.038046	197.787643	47.531482
2275.213846	202.651742	47.536487
2271.756763	197.480299	47.541492
2268.614055	203.658679	47.546497
2265.301290	208.987717	47.551501
2261.535573	199.131192	47.556506
2257.787306	204.212728	47.561511
2253.930337	202.790937	47.566516
2250.981813	193.394698	47.571521
2247.610354	199.658066	47.576525
2244.163714	207.593228	47.581530
2241.202867	195.542973	47.586535
2236.796510	198.239582	47.591540
2233.595529	195.390560	47.596545
2229.843244	210.159804	47.601549
2226.139322	197.025526	47.606554
2222.960949	193.405481	47.611559
2219.232073	209.349733	47.616564
2215.829214	199.669062	47.621569
2212.726496	198.205855	47.626573
2208.701226	196.302123	47.631578
2206.003169	194.882762	47.636583
2202.185477	183.050218	47.641588
2198.298369	200.847167	47.646593
2195.178501	196.775435	47.651597
2191.373202	203.260823	47.656602
2187.872676	187.008938	47.661607
2184.372065	204.426961	47.666612
2181.071737	195.964991	47.671617
2177.518595	196.726758	47.676621
2174.091439	212.482264	47.681626
2170.612874	204.651557	47.686631
2166.742417	213.458286	47.691636
2163.429104	202.097760	47.696641
2159.940362	208.817529	47.701645
2156.374372	214.212350	47.706650
2153.257977	196.683623	47.711655
2149.614663	198.787216	47.716660
2146.218839	208.476611	47.721665
2142.667258	199.189857	47.726669
2138.809348	212.707822	47.731674
2135.590416	201.284491	47.736679
2131.829841	207.422189	47.741684
2128.324099	196.409009	47.746689
2125.256350	195.795957	47.751693
2121.599623	203.004439	47.756698
2117.967372	194.297555	47.761703
2114.301559	208.859418	47.766708
2111.188826	203.146787	47.771713
2107.562372	190.451332	47.776717
2104.022178	210.911269	47.781722
2100.533167	196.969291	47.786727
2096.821742	200.001390	47.791732
2093.247850	197.982426	47.796737
2090.005513	197.636822	47.801741
2086.504859	198.422331	47.806746
2083.071665	203.469730	47.811751
2079.645124	202.172161	47.816756
2076.021695	190.316526	47.821761
2072.690392	196.869581	47.826765
2069.189391	189.704875	47.831770
2065.776392	186.341427	47.836775
2061.558224	195.497848	47.841780
2058.492544	188.774219	47.846785
2055.003338	196.473495	47.851789
2051.850047	195.492022	47.856794
2047.961127	198.882913	47.861799
2044.557256	191.130324	47.866804
2040.851121	193.420124	47.871809
2037.589241	184.316000	47.876813
2033.651568	192.815126	47.881818
2030.876106	183.598408	47.886823
2026.893050	182.229109	47.891828
2023.540589	179.127870	47.896833
2020.137547	181.671226	47.901837
2016.620938	185.178085	47.906842
2012.978886	175.456305	47.911847
2009.459843	191.078333	47.916852
2005.782541	184.702252	47.921857
2002.906667	190.322147	47.926861
1998.990041	190.266571	47.931866
1995.939016	192.847162	47.936871
1992.169464	189.608566	47.941876
1988.303431	192.154919	47.946881
1985.008201	190.028484	47.951885
1981.094789	202.686553	47.956890
1977.950207	194.620036	47.961895
1974.724081	194.019069	47.966900
1970.943377	178.465430	47.971905
1967.684934	180.202267	47.976909
1963.549071	195.590465	47.981914
1960.695451	183.773247	47.986919
1957.038281	179.547493	47.991924
1953.652795	208.253808	47.996929
1949.901087	192.757141	48.001933
1946.080481	206.285789	48.006938
1943.002663	171.349160	48.011943
1939.506089	200.416398	48.016948
1935.982277	185.441987	48.021953
1932.717094	200.487783	48.026957
1928.785985	183.385815	48.031962
1925.712919	184.514200	48.036967
1922.127819	177.396011	48.041972
1918.265711	180.217475	48.046977
1914.913634	182.556550	48.051981
1911.222425	177.911652	48.056986
1908.037631	178.466875	48.061991
1904.224283	183.797048	48.066996
1900.897232	175.797383	48.072001
1897.706310	184.828401	48.077005
1893.851380	188.673365	48.082010
1890.605054	194.849736	48.087015
1887.233883	187.840395	48.092020
1883.634249	190.265309	48.097025
1880.165502	187.126011	48.102029
1876.379164	191.072129	48.107034
1873.388829	182.806603	48.112039
1869.260515	175.788325	48.117044
1865.664385	185.225559	48.122049
1862.342208	192.720475	48.127053
1858.735706	180.526092	48.132058
1855.460803	175.052942	48.137063
1852.072993	186.770325	48.142068
1848.529685	187.119653	48.147073
1845.167057	183.833634	48.152077
1840.913539	193.804819	48.157082
1837.942200	182.593955	48.162087
1834.428432	175.101511	48.167092
1830.908273	182.443834	48.172097
1827.721490	174.103121	48.177101
1823.843725	194.475369	48.182106
1820.922385	184.172915	48.187111
1817.231243	189.979174	48.192116
1813.397478	183.333662	48.197121
1810.059645	181.061435	48.202125
1806.245650	194.659076	48.207130
1802.684527	177.762517	48.212135
1799.354282	193.608076	48.217140
1795.855112	178.863399	48.222145
1792.454345	182.637622	48.227149
1788.667109	190.160563	48.232154
1785.475792	181.536012	48.237159
1782.077304	183.159506	48.242164
1778.438481	189.328959	48.247169
1775.200387	179.909324	48.252173
1771.479433	184.944151	48.257178
1767.901604	183.867318	48.262183
1764.286625	189.437791	48.267188
1760.847997	193.611000	48.272193
1757.342691	174.648129	48.277197
1753.740068	182.227630	48.282202
1750.489636	183.114855	48.287207
1746.874838	181.448587	48.292212
1743.460236	165.367808	48.297217
1739.918635	171.690414	48.302221
1736.246627	169.808574	48.307226
1733.078613	168.191710	48.312231
1729.595218	173.920417	48.317236
1725.735406	175.551494	48.322241
1722.056488	174.548385	48.327245
1718.559982	169.058701	48.332250
1715.626998	168.081080	48.337255
1712.140609	172.115199	48.342260
1708.231634	166.231804	48.347265
1705.000182	170.841306	48.352269
1701.271095	162.071946	48.357274
1697.794905	160.262878	48.362279
1694.176850	170.236496	48.367284
1690.937626	166.008221	48.372289
1687.491731	156.424358	48.377293
1683.858495	172.570691	48.382298
1680.494714	168.690292	48.387303
1676.641044	168.093771	48.392308
1673.003424	175.320093	48.397313
1669.852974	177.143807	48.402317
1666.236800	177.405809	48.407322
1663.072255	180.641254	48.412327
1659.432840	175.271463	48.417332
1655.769351	169.512137	48.422337
1652.357886	173.366907	48.427341
1648.847062	185.613195	48.432346
1645.678227	164.519017	48.437351
1641.476489	184.741949	48.442356
1638.094323	181.017705	48.447361
1634.730987	183.853980	48.452365
1631.306440	173.496166	48.457370
1628.128712	169.204799	48.462375
1624.311876	179.570236	48.467380
1620.521118	174.448389	48.472385
1617.382893	169.528526	48.477389
1613.666727	183.110089	48.482394
1610.526655	165.687152	48.487399
1606.926733	165.726909	48.492404
1602.764263	176.742271	48.497409
1599.567647	162.805761	48.502413
1596.407340	172.061183	48.507418
1592.886262	165.482493	48.512423
1589.509347	172.345811	48.517428
1585.641677	176.396148	48.522433
1582.330701	167.130611	48.527437
1578.443555	165.211162	48.532442
1575.521770	157.864058	48.537447
1571.976340	167.033685	48.542452
1568.007018	164.700257	48.547457
1564.652787	169.572359	48.552461
1561.065261	170.303498	48.557466
1557.915709	175.159485	48.562471
1554.567975	178.005650	48.567476
1550.714250	180.916675	48.572481
1547.570839	170.534318	48.577485
1543.478252	182.861753	48.582490
1540.352068	160.308401	48.587495
1536.719767	176.904473	48.592500
1533.157000	164.694610	48.597505
1530.001812	158.394436	48.602509
1526.077512	169.183485	48.607514
1522.857830	168.519415	48.612519
1519.477499	172.622139	48.617524
1515.333785	176.749931	48.622529
1512.003065	164.156416	48.627533
1508.500505	170.285244	48.632538
1505.114071	161.399282	48.637543
1501.963406	172.718952	48.642548
1497.747765	167.709621	48.647553
1494.774711	166.657716	48.652557
1490.758824	166.783642	48.657562
1487.886324	160.994301	48.662567
1484.561181	155.222252	48.667572
1480.545457	169.947111	48.672577
1477.197876	153.179909	48.677581
1473.564700	170.843620	48.682586
1470.413186	169.095615	48.687591
1466.632745	153.671344	48.692596
1463.087153	161.683691	48.697601
1459.919875	160.092679	48.702605
1456.140051	165.454224	48.707610
1452.723859	160.172212	48.712615
1449.213525	161.774660	48.717620
1445.501149	162.951244	48.722625
1442.354337	166.058764	48.727629
1438.470054	160.375764	48.732634
1435.246258	160.460666	48.737639
1431.761470	158.990039	48.742644
1428.179793	171.489781	48.747649
1424.721024	151.543262	48.752653
1421.271048	176.444513	48.757658
1417.746786	156.871337	48.762663
1414.443244	152.505947	48.767668
1410.539224	151.306853	48.772673
1407.141764	158.656022	48.777677
1403.432410	151.211016	48.782682
1399.789291	158.523787	48.787687
1396.428694	163.153741	48.792692
1392.841819	159.548158	48.797697
1389.899259	152.641591	48.802701
1386.193958	173.013111	48.807706
1382.416468	165.184662	48.812711
1379.076078	168.757523	48.817716
1375.392973	162.921498	48.822721
1372.334702	148.429207	48.827725
1368.913224	170.475895	48.832730
1365.097558	144.470925	48.837735
1361.459639	156.352261	48.842740
1357.894554	144.297590	48.847745
1354.662194	155.399845	48.852749
1351.127724	149.575413	48.857754
1347.631147	152.216580	48.862759
1344.362044	151.081812	48.867764
1340.573663	145.712931	48.872769
1336.778119	151.317826	48.877773
1333.257776	160.203835	48.882778
1330.059121	151.176401	48.887783
1326.397054	153.386572	48.892788
1323.142597	154.232136	48.897793
1320.220933	153.138483	48.902797
1316.309910	162.754174	48.907802
1312.716932	151.020892	48.912807
1309.007231	159.616966	48.917812
1305.334245	155.037186	48.922817
1302.039300	151.567646	48.927821
1298.390272	153.401406	48.932826
1294.933817	156.527048	48.937831
1291.682920	152.281572	48.942836
1287.965841	153.481211	48.947841
1284.412563	157.223808	48.952845
1281.103276	157.316283	48.957850
1277.555926	152.765993	48.962855
1273.788422	155.167118	48.967860
1270.470738	162.325708	48.972865
1267.147977	163.590386	48.977869
1263.831133	169.099832	48.982874
1259.728393	162.869692	48.987879
1256.165209	167.101067	48.992884
1252.887519	176.355963	48.997889
1249.524602	164.691868	49.002893
1246.024612	155.794223	49.007898
1242.573693	170.811961	49.012903
1239.205273	148.227202	49.017908
1235.293328	158.621122	49.022913
1231.954299	145.618887	49.027917
1228.240103	170.237951	49.032922
1224.841685	151.681734	49.037927
1221.619549	148.912361	49.042932
1218.079221	152.408203	49.047937
1214.798489	152.528254	49.052941
1210.926273	153.571042	49.057946
1207.487693	159.444887	49.062951
1203.943700	151.622405	49.067956
1200.332414	171.377889	49.072961
1197.182053	151.827994	49.077965
1193.364747	171.122076	49.082970
1189.778135	146.174931	49.087975
1186.447123	171.224488	49.092980
1182.683077	161.805113	49.097985
1179.573139	156.525572	49.102989
1175.897617	165.614044	49.107994
1172.493083	141.596319	49.112999
1168.886102	156.112358	49.118004
1165.380818	157.799245	49.123009
1161.731401	153.674077	49.128013
1158.451942	170.486070	49.133018
1155.134191	155.335841	49.138023
1151.373309	160.543473	49.143028
1147.732496	169.470957	49.148033
1144.490375	153.098031	49.153037
1140.919654	162.584821	49.158042
1137.378770	148.926018	49.163047
1133.935951	163.934953	49.168052
1130.122458	162.131355	49.173057
1127.044360	149.481588	49.178061
1123.117465	165.746628	49.183066
1120.164312	145.604702	49.188071
1116.272859	144.739899	49.193076
1112.486896	148.672810	49.198081
1109.175900	147.344619	49.203085
1105.876963	157.586986	49.208090
1102.649312	141.193067	49.213095
1098.987855	160.880991	49.218100
1095.345829	157.189878	49.223105
1091.985121	154.010182	49.228109
1088.210853	163.274508	49.233114
1085.141498	147.084015	49.238119
1081.508533	159.356479	49.243124
1077.756941	153.731903	49.248129
1074.291836	144.207915	49.253133
1070.797988	164.349980	49.258138
1067.420291	149.837706	49.263143
1063.793342	159.250650	49.268148
1060.047410	166.196020	49.273153
1056.903624	150.191352	49.278157
1052.994787	157.112813	49.283162
1049.983218	168.021682	49.288167
1046.607890	167.158714	49.293172
1043.020882	155.277534	49.298177
1039.368008	158.996740	49.303181
1035.616154	155.523952	49.308186
1032.235462	149.702923	49.313191
1028.693645	158.110213	49.318196
1025.104748	151.650583	49.323201
1022.092647	151.466634	49.328205
1018.173469	157.622534	49.333210
1014.820143	147.968454	49.338215
1011.120755	161.653609	49.343220
1007.591326	161.332528	49.348225
1004.222826	156.171331	49.353229
1000.784080	152.122060	49.358234
997.349921	151.348441	49.363239
993.872702	153.808522	49.368244
990.247817	155.786427	49.373249
987.100548	147.266142	49.378253
983.107279	159.516947	49.383258
979.738013	146.664876	49.388263
976.072920	152.800842	49.393268
972.688620	163.412491	49.398273
969.361993	151.812135	49.403277
965.548152	148.913696	49.408282
962.103695	146.867359	49.413287
958.946391	154.072690	49.418292
955.018626	151.419860	49.423297
951.523778	144.261906	49.428301
948.279301	152.900886	49.433306
944.605913	138.859740	49.438311
941.191188	149.252682	49.443316
938.113836	143.997385	49.448321
934.556871	136.525544	49.453325
930.586754	146.499588	49.458330
927.024830	138.259212	49.463335
923.978722	148.524806	49.468340
919.981045	146.485690	49.473345
916.520497	144.791348	49.478349
913.238792	145.840774	49.483354
909.387236	147.960911	49.488359
906.152763	150.647501	49.493364
902.258851	147.473479	49.498369
899.216773	147.944331	49.503373
895.950841	151.523559	49.508378
892.595808	143.082718	49.513383
889.018842	142.900851	49.518388
885.214648	157.732682	49.523393
881.615330	146.999251	49.528397
877.948260	149.423755	49.533402
874.872794	153.265908	49.538407
871.308327	148.019460	49.543412
867.343400	152.771039	49.548417
864.107447	150.200043	49.553421
860.356832	156.281725	49.558426
856.875611	158.302564	49.563431
853.730583	146.551750	49.568436
850.398428	138.711379	49.573441
846.949417	130.280665	49.578445
842.586646	154.395589	49.583450
839.217721	136.278807	49.588455
836.105992	142.147373	49.593460
832.792503	149.238463	49.598465
829.276005	145.975628	49.603469
825.592966	148.404374	49.608474
821.712200	145.998674	49.613479
818.710694	146.669136	49.618484
815.028369	153.970987	49.623489
811.712305	142.769898	49.628493
807.781674	144.788718	49.633498
804.482285	147.699054	49.638503
801.203606	138.265593	49.643508
797.397921	150.529202	49.648513
794.490735	140.540170	49.653517
790.698496	145.170246	49.658522
787.241334	153.119249	49.663527
783.583486	140.385597	49.668532
779.924109	150.789114	49.673537
776.875922	132.593866	49.678541
773.033262	146.307991	49.683546
769.580932	140.562771	49.688551
765.744369	143.036335	49.693556
762.549490	138.688372	49.698561
759.358434	139.227491	49.703565
755.585082	152.180065	49.708570
751.573117	137.162716	49.713575
748.207161	141.761777	49.718580
744.867767	140.714775	49.723585
741.818058	132.493114	49.728589
738.273343	144.426778	49.733594
734.558576	135.731447	49.738599
730.853465	131.940683	49.743604
727.410427	155.097712	49.748609
724.420250	131.745957	49.753613
720.233062	145.047537	49.758618
716.964984	147.619608	49.763623
713.853864	147.510255	49.768628
709.841437	148.927274	49.773633
706.628639	141.194924	49.778637
702.592728	132.883123	49.783642
699.478340	134.745697	49.788647
695.969487	130.861973	49.793652
692.367653	136.420298	49.798657
688.972342	129.154723	49.803661
685.407418	132.106106	49.808666
682.031426	132.829301	49.813671
678.447322	142.759444	49.818676
674.862124	150.929009	49.823681
671.685389	133.321298	49.828685
668.103878	142.852678	49.833690
664.343863	144.674220	49.838695
661.032916	134.233554	49.843700
657.222621	135.964855	49.848705
653.320565	143.416119	49.853709
650.217858	138.856980	49.858714
647.180701	123.752320	49.863719
643.731808	138.387742	49.868724
639.843338	124.107613	49.873729
636.528346	140.550840	49.878733
632.819277	139.500140	49.883738
629.332302	143.791732	49.888743
625.826720	139.498215	49.893748
621.989456	143.332724	49.898753
618.912070	131.882420	49.903757
615.206599	143.750252	49.908762
612.158319	136.166775	49.913767
608.978441	140.294605	49.918772
604.972215	138.382481	49.923777
601.266024	131.427747	49.928781
597.737226	136.072711	49.933786
594.417986	141.246050	49.938791
590.883960	139.593713	49.943796
586.963185	141.909934	49.948801
584.063996	126.734975	49.953805
580.341010	141.254898	49.958810
576.810376	148.845507	49.963815
573.601126	133.371363	49.968820
569.887557	140.055032	49.973825
566.393184	122.041454	49.978829
562.688461	139.119456	49.983834
559.268092	130.702931	49.988839
555.985230	131.241528	49.993844
552.480056	145.086055	49.998849
548.866178	141.977374	50.003853
545.058171	130.343861	50.008858
541.633747	135.011565	50.013863
538.802994	131.896851	50.018868
534.688431	140.321712	50.023873
531.482875	125.724761	50.028877
527.818524	121.545131	50.033882
524.123214	145.800189	50.038887
520.981345	131.001146	50.043892
517.124620	140.108882	50.048897
513.803964	132.777020	50.053901
510.474273	136.185637	50.058906
507.054147	135.696926	50.063911
503.198510	137.054825	50.068916
499.376270	136.815530	50.073921
496.180498	132.425638	50.078925
492.634829	137.672232	50.083930
489.225506	138.655345	50.088935
486.201447	133.787457	50.093940
482.164545	138.594044	50.098945
479.300247	146.442881	50.103949
475.352322	134.919731	50.108954
471.488692	151.061722	50.113959
468.189013	140.512868	50.118964
464.255785	155.650293	50.123969
461.274409	135.155783	50.128973
457.913908	142.082851	50.133978
454.749857	140.296082	50.138983
450.925016	132.486336	50.143988
447.133184	134.061209	50.148993
444.094568	121.770943	50.153997
439.920023	136.227898	50.159002
436.567814	141.152934	50.164007
433.055322	132.262115	50.169012
429.522450	136.420122	50.174017
426.424134	125.681686	50.179021
422.742904	129.632675	50.184026
418.873207	130.160953	50.189031
415.755236	133.475846	50.194036
412.094380	127.563456	50.199041
408.952687	132.573584	50.204045
405.081991	142.450965	50.209050
401.365956	136.729895	50.214055
398.237673	141.736039	50.219060
394.558656	140.523860	50.224065
391.260844	126.018693	50.229069
387.663687	137.439413	50.234074
384.109246	121.081531	50.239079
381.113347	116.855884	50.244084
377.142283	140.764706	50.249089
373.618784	118.368142	50.254093
369.747059	139.173087	50.259098
366.568126	137.250715	50.264103
363.319502	122.366036	50.269108
359.731232	121.366172	50.274113
356.114486	133.683589	50.279117
352.736018	131.874093	50.284122
349.084772	126.243077	50.289127
345.417152	139.774972	50.294132
342.223712	132.818955	50.299137
338.898006	121.600931	50.304141
335.357281	137.863536	50.309146
331.513242	115.780592	50.314151
327.953625	138.967916	50.319156
324.536769	137.892894	50.324161
321.168356	129.312367	50.329165
317.474397	125.228907	50.334170
313.929259	128.676959	50.339175
310.754987	130.063370	50.344180
307.297147	129.021271	50.349185
303.806536	116.115532	50.354189
299.896754	133.738600	50.359194
296.422840	133.375291	50.364199
293.089166	132.377103	50.369204
289.439187	135.234427	50.374209
286.527648	139.171970	50.379213
282.347952	127.525773	50.384218
278.954530	138.733245	50.389223
275.281713	134.081756	50.394228
271.865422	130.542457	50.399233
268.620943	134.506899	50.404237
265.073719	130.324156	50.409242
261.761877	136.376555	50.414247
258.253814	116.119566	50.419252
254.249740	134.970115	50.424257
251.250515	117.144078	50.429261
247.375037	131.326007	50.434266
243.936080	141.053021	50.439271
240.829505	126.313046	50.444276
236.777557	131.918540	50.449281
233.873487	133.256301	50.454285
229.981743	141.961074	50.459290
226.355871	134.649821	50.464295
223.133219	131.966777	50.469300
219.579263	127.738515	50.474305
215.972674	130.738554	50.479309
212.301220	139.511405	50.484314
208.702577	147.182178	50.489319
205.707926	128.119547	50.494324
201.948071	135.677664	50.499329
198.401392	124.290263	50.504333
194.887407	130.340971	50.509338
191.416376	140.997830	50.514343
188.235139	133.827695	50.519348
184.500505	124.868390	50.524353
181.245610	134.331319	50.529357
177.469083	132.940158	50.534362
174.051352	137.905539	50.539367
170.525348	125.021614	50.544372
167.060944	126.388854	50.549377
163.515231	126.314484	50.554381
159.827457	131.776689	50.559386
156.171445	130.814571	50.564391
153.257772	115.357389	50.569396
148.945683	118.642228	50.574401
145.884189	132.094272	50.579405
142.342109	121.747373	50.584410
138.608218	125.980369	50.589415
135.648137	123.572027	50.594420
132.111985	126.792885	50.599425
128.666631	131.178761	50.604429
125.082577	128.851331	50.609434
121.549943	131.710170	50.614439
118.361055	124.203872	50.619444
114.293597	124.300480	50.624449
111.089257	128.741536	50.629453
107.151118	124.691453	50.634458
103.767173	145.032365	50.639463
100.581935	113.957963	50.644468
96.839684	143.596486	50.649473
93.424987	126.275513	50.654477
89.928286	140.909575	50.659482
86.353843	124.777466	50.664487
82.668295	116.931743	50.669492
79.491620	131.670457	50.674497
76.021512	127.544040	50.679501
72.635104	126.818862	50.684506
68.342417	121.864892	50.689511
65.027160	130.246114	50.694516
61.644581	124.371124	50.699521
58.579206	135.691288	50.704525
55.196667	124.836388	50.709530
51.291919	132.732814	50.714535
48.049265	121.432694	50.719540
44.115018	137.515893	50.724545
40.844828	131.388842	50.729549
37.299100	120.624354	50.734554
33.441842	125.586672	50.739559
30.157825	118.669091	50.744564
26.816086	127.715936	50.749569
23.641259	115.988336	50.754573
19.949634	131.242861	50.759578
16.321221	129.778294	50.764583
13.068371	133.983853	50.769588
9.080476	136.710927	50.774593
5.865130	124.567028	50.779597
2.520005	140.428104	50.784602