Wed Jun 15 16:05:22 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.985159	129.419464	0.000000
1.628259	132.331702	0.005005
1.332752	104.752205	0.010010
0.975327	106.137895	0.015014
0.904866	104.330509	0.020019
0.660690	100.250104	0.025024
0.507393	80.511352	0.030029
0.434832	78.692281	0.035034
-0.328979	54.969818	0.040038
-0.133816	47.796955	0.045043
-0.621678	49.710845	0.050048
-0.959628	47.151989	0.055053
-1.051261	28.226738	0.060058
-0.987732	40.959697	0.065062
-1.130019	12.209366	0.070067
-1.806677	10.429175	0.075072
-2.611042	-0.389283	0.080077
-2.848398	-9.364621	0.085082
-3.051145	3.018910	0.090086
-3.031257	-23.228273	0.095091
-2.907064	-10.086729	0.100096
-3.040612	-9.268764	0.105101
-3.612675	-28.953334	0.110106
-4.308098	-24.009468	0.115110
-4.192463	-35.280025	0.120115
-4.840188	-23.057457	0.125120
-5.601417	-15.195121	0.130125
-5.748530	-32.793609	0.135130
-6.055728	-27.303088	0.140134
-5.752688	-30.222468	0.145139
-5.646142	-29.959313	0.150144
-5.914806	-25.033199	0.155149
-5.893488	-41.627281	0.160154
-6.549012	-23.647631	0.165158
-7.006930	-32.895957	0.170163
-7.172799	-22.393406	0.175168
-7.373594	-33.403526	0.180173
-7.839355	-23.097535	0.185178
-8.996822	-27.876707	0.190182
-8.108121	-19.876187	0.195187
-8.714942	-16.259644	0.200192
-9.005039	-27.727130	0.205197
-8.938333	-25.562893	0.210202
-9.351066	-17.329929	0.215206
-8.970642	-31.450335	0.220211
-9.255967	-25.230390	0.225216
-10.052301	-24.524054	0.230221
-10.351169	-25.253751	0.235226
-10.855426	-19.858801	0.240230
-10.858835	-25.182048	0.245235
-10.877507	-17.921753	0.250240
-11.201237	-29.216276	0.255245
-12.129093	-18.969159	0.260250
-12.428467	-13.815618	0.265254
-11.927897	-23.431286	0.270259
-12.300829	-19.908837	0.275264
-12.578806	-11.398454	0.280269
-12.377725	-24.044456	0.285274
-12.560426	-12.308704	0.290278
-13.008515	-21.089499	0.295283
-13.561999	-27.663128	0.300288
-13.824226	-11.388354	0.305293
-13.903078	-25.708972	0.310298
-14.382785	-20.437639	0.315302
-14.780172	-22.021210	0.320307
-15.126236	-25.339766	0.325312
-15.549995	-32.002403	0.330317
-15.529307	-25.921122	0.335322
-15.572472	-27.868247	0.340326
-15.620514	-20.189181	0.345331
-15.459753	-30.845234	0.350336
-15.963163	-27.668087	0.355341
-16.521501	-27.830598	0.360346
-17.051523	-20.424043	0.365350
-17.150064	-16.408333	0.370355
-17.409490	-17.785648	0.375360
-17.308373	-21.445637	0.380365
-17.621687	-24.546073	0.385370
-18.296138	-22.542068	0.390374
-18.223170	-28.273408	0.395379
-18.786227	-22.232573	0.400384
-18.933403	-18.953307	0.405389
-18.576724	-13.099095	0.410394
-18.687167	-16.284850	0.415398
-19.624054	-32.219656	0.420403
-20.157041	-21.583238	0.425408
-20.228731	-22.471419	0.430413
-20.228096	-30.090332	0.435418
-20.407576	-21.943467	0.440422
-20.180511	-22.545132	0.445427
-21.081415	-28.782864	0.450432
-21.418600	-12.314195	0.455437
-21.333047	-19.867441	0.460442
-21.666052	-13.244435	0.465446
-21.900708	-15.725650	0.470451
-22.526499	-25.774268	0.475456
-23.153269	-17.726011	0.480461
-22.852467	-20.494490	0.485466
-23.566051	-19.536273	0.490470
-23.353122	-10.865042	0.495475
-23.296459	-21.920677	0.500480
-23.264441	-24.064104	0.505485
-24.336058	-22.363691	0.510490
-24.354561	-28.454275	0.515494
-24.895967	-17.816069	0.520499
-24.827042	-25.092032	0.525504
-25.016916	-11.730791	0.530509
-24.715103	-22.743584	0.535514
-25.365652	-18.262778	0.540518
-26.105017	-15.916888	0.545523
-26.344475	-32.196306	0.550528
-26.344478	-22.874735	0.555533
-26.086982	-40.529721	0.560538
-26.625151	-17.218609	0.565542
-27.349784	-33.354314	0.570547
-27.718525	-15.368191	0.575552
-28.259269	-21.368030	0.580557
-27.843567	-28.633335	0.585562
-28.248629	-23.969076	0.590566
-27.929801	-31.384292	0.595571
-28.065187	-27.749977	0.600576
-28.717144	-18.880375	0.605581
-28.948326	-17.348254	0.610586
-29.565765	-21.484225	0.615590
-29.543202	-22.719137	0.620595
-29.445438	-37.281316	0.625600
-29.817588	-12.526332	0.630605
-30.446225	-13.427230	0.635610
-31.050802	-18.517557	0.640614
-31.005510	-17.777978	0.645619
-30.973741	-13.157697	0.650624
-31.155502	-12.718259	0.655629
-31.130053	-15.131779	0.660634
-32.151255	-20.113004	0.665638
-32.723172	-17.186930	0.670643
-32.995924	-12.069849	0.675648
-32.877742	-18.604048	0.680653
-32.810035	-28.191874	0.685658
-33.067917	-18.455589	0.690662
-33.195752	-31.367429	0.695667
-33.140751	-21.702881	0.700672
-33.487461	-21.428936	0.705677
-33.969768	-27.466247	0.710682
-34.419195	-18.800971	0.715686
-34.778313	-20.164867	0.720691
-34.841085	-31.363126	0.725696
-34.783395	-27.051851	0.730701
-35.652401	-31.994301	0.735706
-36.089680	-16.496148	0.740710
-36.158663	-32.335662	0.745715
-36.335579	-14.316038	0.750720
-36.490146	-23.450549	0.755725
-36.404962	-37.801123	0.760730
-36.613145	-19.677198	0.765734
-36.667130	-28.536830	0.770739
-37.187086	-28.620255	0.775744
-38.003393	-16.932596	0.780749
-37.869461	-32.004937	0.785754
-38.282982	-23.430038	0.790758
-38.235576	-27.173875	0.795763
-38.094318	-31.306597	0.800768
-38.605957	-16.516566	0.805773
-39.112800	-39.333840	0.810778
-39.752078	-10.963626	0.815782
-39.744977	-25.820579	0.820787
-39.867121	-24.988913	0.825792
-39.878979	-15.913475	0.830797
-40.148696	-36.776700	0.835802
-40.691065	-10.549111	0.840806
-41.133208	-22.474635	0.845811
-41.198767	-19.864263	0.850816
-41.264225	-21.878728	0.855821
-41.024539	-18.969005	0.860826
-42.053754	-15.868806	0.865830
-42.431663	-11.731854	0.870835
-42.565892	-23.567597	0.875840
-42.832616	-6.161792	0.880845
-42.794762	-21.623501	0.885850
-42.787453	-16.675324	0.890854
-43.073620	-20.272687	0.895859
-43.549438	-26.199007	0.900864
-44.242539	-14.623056	0.905869
-44.350825	-22.008823	0.910874
-44.272408	-14.932469	0.915878
-44.179799	-24.570282	0.920883
-44.482342	-19.958872	0.925888
-45.395720	-15.402368	0.930893
-45.516819	-27.964142	0.935898
-45.965694	8.335863	0.940902
-46.051015	-21.068655	0.945907
-45.828395	-19.778246	0.950912
-46.087208	-12.434365	0.955917
-46.268375	-16.702414	0.960922
-47.099170	-20.684055	0.965926
-47.374684	-19.331345	0.970931
-47.555617	-8.622792	0.975936
-47.519354	-11.136055	0.980941
-47.375675	-10.325336	0.985946
-47.957573	-12.957994	0.990950
-48.637560	-20.586053	0.995955
-48.694140	-17.523492	1.000960
-49.011307	-18.527258	1.005965
-48.867900	-39.025009	1.010970
-49.230331	-21.268700	1.015974
-49.590307	-22.241913	1.020979
-50.130611	-21.136052	1.025984
-50.664652	-13.866342	1.030989
-50.591998	-25.210194	1.035994
-50.612252	-19.699128	1.040998
-50.893228	-24.434932	1.046003
-50.792384	-25.474836	1.051008
-51.015981	-31.556281	1.056013
-51.543735	-22.951357	1.061018
-52.232880	-37.758924	1.066022
-52.248671	-22.402746	1.071027
-52.138487	-19.392802	1.076032
-52.595401	-25.498033	1.081037
-52.432193	-29.692486	1.086042
-53.668264	-22.212645	1.091046
-54.033309	-27.307338	1.096051
-53.942611	-22.240562	1.101056
-54.143949	-18.607479	1.106061
-54.250136	-26.607957	1.111066
-54.245649	-28.563844	1.116070
-54.312659	-35.563222	1.121075
-53.876197	-17.532423	1.126080
-55.077455	-25.737130	1.131085
-55.648141	-23.919646	1.136090
-55.783337	-21.496734	1.141094
-55.776413	-24.271194	1.146099
-55.485976	-28.028858	1.151104
-56.345500	-22.583281	1.156109
-56.830742	-15.450567	1.161114
-57.393151	-17.222108	1.166118
-57.181309	-14.315083	1.171123
-57.473353	-21.106124	1.176128
-57.324706	-6.757945	1.181133
-58.183561	-29.457566	1.186138
-58.799289	-4.726241	1.191142
-59.004516	-19.144150	1.196147
-58.615019	-12.365924	1.201152
-58.850546	-16.004702	1.206157
-58.617642	-21.379334	1.211162
-58.947813	-2.971255	1.216166
-59.389821	-21.734058	1.221171
-60.131497	-24.602704	1.226176
-60.690926	-5.644568	1.231181
-60.204437	-15.853636	1.236186
-60.741755	-16.345050	1.241190
-60.691050	-12.642349	1.246195
-60.906816	-27.693689	1.251200
-61.955495	-3.859906	1.256205
-62.220896	-29.929205	1.261210
-62.586933	-5.709789	1.266214
-61.825112	-29.122848	1.271219
-62.060102	-4.188104	1.276224
-62.530414	-23.802868	1.281229
-62.450015	-16.550762	1.286234
-63.195680	-19.102786	1.291238
-63.770450	-24.147033	1.296243
-63.901355	-8.099347	1.301248
-64.055724	-10.147949	1.306253
-63.716633	-20.265179	1.311258
-64.197510	-17.796972	1.316262
-64.494522	-26.621960	1.321267
-64.809024	-24.912218	1.326272
-65.403452	-16.451441	1.331277
-65.187246	-32.624552	1.336282
-65.706089	-8.712422	1.341286
-65.894832	-27.016248	1.346291
-66.149532	-28.413972	1.351296
-67.037938	-22.235515	1.356301
-66.795508	-35.354931	1.361306
-67.501196	-20.849094	1.366310
-66.910270	-24.229186	1.371315
-67.384002	-40.556675	1.376320
-67.370895	-24.597422	1.381325
-67.276944	-34.688924	1.386330
-68.276004	-26.579831	1.391334
-68.850174	-32.826569	1.396339
-68.842318	-39.886752	1.401344
-68.954326	-26.278466	1.406349
-69.010002	-29.364658	1.411354
-69.263704	-22.687092	1.416358
-69.564496	-32.157189	1.421363
-69.634170	-15.311129	1.426368
-69.960808	-21.704531	1.431373
-69.693438	-23.121559	1.436378
-71.080506	-16.902115	1.441382
-71.365343	-21.802315	1.446387
-71.843786	-18.199687	1.451392
-71.936323	-12.695020	1.456397
-71.683212	-23.168059	1.461402
-71.983108	-5.887876	1.466406
-71.862496	-24.764670	1.471411
-71.757980	-18.933404	1.476416
-72.638847	-15.512556	1.481421
-72.804143	-21.111099	1.486426
-73.215404	-22.217491	1.491430
-73.327783	-8.682324	1.496435
-73.321686	-30.640531	1.501440
-74.124989	-18.913789	1.506445
-74.570058	-29.143981	1.511450
-75.024194	-26.591117	1.516454
-75.046514	-25.930231	1.521459
-75.251716	-33.967212	1.526464
-75.487090	-25.666895	1.531469
-74.982667	-28.946670	1.536474
-75.317148	-27.910140	1.541478
-75.692873	-19.944214	1.546483
-75.849379	-27.360675	1.551488
-76.571425	-20.903515	1.556493
-76.643735	-27.202718	1.561498
-76.875533	-23.359714	1.566502
-76.885899	-44.961039	1.571507
-77.599358	-37.457490	1.576512
-78.422968	-17.283104	1.581517
-78.255900	-27.682336	1.586522
-78.667343	-18.914138	1.591526
-78.732130	-22.880720	1.596531
-78.689388	-26.917750	1.601536
-78.767953	-21.821817	1.606541
-78.435847	-38.961372	1.611546
-79.004928	-17.740695	1.616550
-79.538994	-22.748954	1.621555
-79.796174	-27.062636	1.626560
-80.026497	-21.295786	1.631565
-80.153152	-41.684082	1.636570
-80.988196	-20.452400	1.641574
-81.225436	-34.857106	1.646579
-81.405741	-30.793066	1.651584
-81.796626	-20.593067	1.656589
-81.537572	-25.402931	1.661594
-82.013224	-32.371663	1.666598
-81.816207	-23.334109	1.671603
-82.213471	-19.431697	1.676608
-82.665144	-28.244338	1.681613
-82.976964	-35.017798	1.686618
-83.494574	-32.688630	1.691622
-83.337879	-30.253295	1.696627
-83.334090	-37.537719	1.701632
-84.598042	-35.045345	1.706637
-84.754794	-31.858115	1.711642
-84.732161	-33.208157	1.716646
-84.776000	-18.140619	1.721651
-84.674123	-25.247914	1.726656
-85.021087	-25.064975	1.731661
-85.069258	-19.078360	1.736666
-86.118580	-26.932820	1.741670
-86.498731	-29.147509	1.746675
-86.414776	-36.880902	1.751680
-86.928067	-33.735758	1.756685
-86.409256	-25.339814	1.761690
-86.608050	-27.099731	1.766694
-86.639361	-28.140383	1.771699
-87.163114	-30.855542	1.776704
-88.090035	-17.240212	1.781709
-87.965513	-46.846257	1.786714
-88.376997	-25.528333	1.791718
-88.391398	-32.710514	1.796723
-88.409308	-33.938243	1.801728
-89.065922	-25.640809	1.806733
-89.622659	-34.245299	1.811738
-89.912299	-21.602793	1.816742
-90.008160	-38.506875	1.821747
-90.101009	-15.910966	1.826752
-90.531978	-37.222211	1.831757
-90.095875	-29.649215	1.836762
-90.125103	-32.886167	1.841766
-91.244535	-30.890585	1.846771
-91.225169	-41.661853	1.851776
-91.636504	-27.579922	1.856781
-91.679882	-37.474710	1.861786
-91.371842	-38.941469	1.866790
-91.930900	-27.415106	1.871795
-92.439351	-24.554564	1.876800
-93.087549	-33.135553	1.881805
-92.883346	-34.366650	1.886810
-93.320850	-32.994170	1.891814
-92.995895	-36.146524	1.896819
-93.487987	-46.254105	1.901824
-94.768484	-22.727991	1.906829
-94.551325	-48.062781	1.911834
-94.665827	-33.845054	1.916838
-95.010684	-37.143873	1.921843
-94.615579	-34.521058	1.926848
-94.885644	-23.425991	1.931853
-95.294705	-43.748467	1.936858
-95.856966	-27.030042	1.941862
-95.909484	-29.139568	1.946867
-95.834732	-35.387706	1.951872
-96.091483	-44.143180	1.956877
-96.887378	-32.940003	1.961882
-97.533940	-35.671755	1.966886
-97.912621	-28.900441	1.971891
-97.619991	-30.661282	1.976896
-97.766718	-31.470966	1.981901
-97.719386	-30.975480	1.986906
-98.011716	-25.409979	1.991910
-98.039350	-26.589737	1.996915
-99.268730	-27.543094	2.006912
-98.431379	-34.039719	2.016909
-98.212986	-34.924135	2.026906
-97.191102	-24.656825	2.036902
-96.908635	-29.272186	2.046899
-96.393511	-32.817874	2.056896
-96.237605	-28.854396	2.066893
-95.410087	-28.422798	2.076890
-95.376290	-38.932673	2.086886
-94.375044	-28.699091	2.096883
-94.237025	-27.043531	2.106880
-93.182476	-27.868305	2.116877
-92.515913	-30.349961	2.126874
-92.398749	-31.620735	2.136870
-92.488348	-35.155765	2.146867
-91.490856	-30.717415	2.156864
-91.027539	-30.875148	2.166861
-90.649885	-32.314614	2.176858
-89.775934	-32.817765	2.186854
-89.579268	-30.179633	2.196851
-89.133041	-32.248549	2.206848
-88.027313	-30.322086	2.216845
-87.965631	-33.845475	2.226842
-87.391815	-34.523332	2.236838
-86.616041	-26.920417	2.246835
-86.478865	-31.971253	2.256832
-86.401695	-23.152254	2.266829
-85.362067	-20.159877	2.276826
-84.758629	-27.020045	2.286822
-84.718995	-24.949974	2.296819
-83.612517	-24.757480	2.306816
-83.196454	-30.974191	2.316813
-83.103026	-22.489259	2.326810
-82.715862	-18.808560	2.336806
-81.844418	-22.166210	2.346803
-81.738581	-20.651710	2.356800
-80.879376	-16.967837	2.366797
-80.311642	-23.740420	2.376794
-80.127141	-21.836425	2.386790
-79.279744	-23.589298	2.396787
-78.905607	-13.905138	2.406784
-78.716430	-15.246783	2.416781
-77.661162	-23.090532	2.426778
-77.063348	-22.347071	2.436774
-76.954751	-17.336883	2.446771
-76.838443	-22.729285	2.456768
-75.951450	-16.989120	2.466765
-75.470302	-18.518486	2.476762
-74.455168	-15.081336	2.486758
-74.008294	-18.709876	2.496755
-73.853300	-3.420608	2.506752
-73.735694	-19.091280	2.516749
-73.230675	-18.411994	2.526746
-72.267398	-15.997060	2.536742
-72.100075	-21.304752	2.546739
-71.001789	-15.928319	2.556736
-70.885029	-22.959725	2.566733
-70.692219	-22.119102	2.576730
-70.020487	-25.584493	2.586726
-69.604140	-16.514760	2.596723
-68.846772	-20.228692	2.606720
-67.817000	-24.201191	2.616717
-67.609272	-29.971392	2.626714
-67.385399	-23.111882	2.636710
-67.468561	-23.632659	2.646707
-66.676947	-24.223144	2.656704
-65.974186	-28.954294	2.666701
-64.994836	-28.765874	2.676698
-64.431522	-26.524360	2.686694
-64.766707	-30.812933	2.696691
-64.148494	-18.701289	2.706688
-63.130267	-17.289480	2.716685
-63.103634	-23.651129	2.726682
-62.225366	-16.412625	2.736678
-61.427373	-25.033760	2.746675
-61.364349	-21.303734	2.756672
-61.238984	-22.497736	2.766669
-59.993091	-19.068201	2.776666
-59.662366	-30.199151	2.786662
-59.780106	-19.583367	2.796659
-58.983243	-15.922275	2.806656
-58.281174	-15.398525	2.816653
-57.984215	-17.891988	2.826650
-57.233702	-16.258933	2.836646
-56.343541	-23.795866	2.846643
-56.592180	-25.256572	2.856640
-56.164465	-22.489993	2.866637
-55.234219	-21.363417	2.876634
-55.018293	-24.182571	2.886630
-54.395662	-19.030260	2.896627
-53.324832	-9.613841	2.906624
-52.957344	-10.232607	2.916621
-53.370812	-13.941491	2.926618
-52.461071	-17.858594	2.936614
-51.775867	-14.126400	2.946611
-51.774878	-12.010529	2.956608
-50.560594	-13.346669	2.966605
-49.991687	-18.546300	2.976602
-49.943640	-21.218097	2.986598
-49.620306	-18.242845	2.996595
-48.619418	-14.091087	3.006592
-48.483967	-14.244708	3.016589
-47.991784	-20.544724	3.026586
-46.867511	-21.688394	3.036582
-46.711992	-17.709734	3.046579
-46.613593	-11.926741	3.056576
-46.088782	-22.247344	3.066573
-45.306743	-23.849056	3.076570
-44.926601	-19.312318	3.086566
-44.186671	-12.428749	3.096563
-43.941475	-17.362915	3.106560
-43.415538	-23.300779	3.116557
-42.525168	-14.415661	3.126554
-42.335518	-14.494480	3.136550
-42.147208	-18.299561	3.146547
-41.040749	-21.174530	3.156544
-40.702645	-18.167247	3.166541
-40.497109	-17.368432	3.176538
-40.040885	-17.121109	3.186534
-39.297557	-7.997842	3.196531
-38.802014	-15.193887	3.206528
-37.894635	-15.413746	3.216525
-37.436863	-24.535926	3.226522
-37.651957	-4.590204	3.236518
-37.386747	-21.287815	3.246515
-36.108069	-11.620686	3.256512
-35.950130	-13.532122	3.266509
-35.231314	-17.451251	3.276506
-34.237405	-10.271852	3.286502
-34.404791	-13.366449	3.296499
-34.271495	-25.588211	3.306496
-33.155300	-15.634460	3.316493
-33.015959	-21.343384	3.326490
-32.437751	-17.201971	3.336486
-31.430325	-19.284024	3.346483
-31.055797	-12.589858	3.356480
-31.019306	-17.572995	3.366477
-30.054871	-19.106176	3.376474
-29.658187	-14.954911	3.386470
-29.514650	-15.184441	3.396467
-28.642706	-16.328780	3.406464
-27.841366	-17.631338	3.416461
-27.686062	-19.695731	3.426458
-27.669306	-20.681646	3.436454
-27.127789	-30.640832	3.446451
-26.660197	-18.779268	3.456448
-25.348278	-22.895189	3.466445
-24.643211	-20.308479	3.476442
-24.839961	-16.985130	3.486438
-24.884660	-16.647216	3.496435
-23.969747	-17.296299	3.506432
-23.175919	-21.254690	3.516429
-22.831782	-21.898041	3.526426
-21.575306	-17.763826	3.536422
-21.803286	-24.378926	3.546419
-21.315135	-24.136582	3.556416
-21.252484	-15.341445	3.566413
-20.252336	-19.088979	3.576410
-19.788022	-24.301250	3.586406
-19.369495	-22.823807	3.596403
-18.450514	-18.716389	3.606400
-18.256798	-19.159362	3.616397
-17.902766	-25.823040	3.626394
-16.785164	-29.670679	3.636390
-16.572081	-25.551695	3.646387
-16.490824	-27.992320	3.656384
-15.939587	-30.557535	3.666381
-15.110334	-25.124185	3.676378
-14.764125	-21.524519	3.686374
-14.517090	-26.943860	3.696371
-13.602571	-36.826109	3.706368
-13.367575	-29.759630	3.716365
-12.494068	-34.426542	3.726362
-11.873049	-36.511895	3.736358
-11.695973	-31.240611	3.746355
-11.371161	-28.476283	3.756352
-11.195237	-34.254068	3.766349
-10.108679	-29.060787	3.776346
-9.767172	-33.036082	3.786342
-8.826704	-29.100129	3.796339
-8.419978	-26.335707	3.806336
-8.787773	-25.844835	3.816333
-7.924277	-32.900383	3.826330
-6.877499	-30.416172	3.836326
-6.914162	-24.669037	3.846323
-6.480273	-18.591340	3.856320
-5.440258	-9.044572	3.866317
-5.332156	-23.046105	3.876314
-5.126258	-15.374174	3.886310
-4.343498	-4.030887	3.896307
-3.899128	11.125246	3.906304
-3.307829	19.253342	3.916301
-3.152528	22.664306	3.926298
-2.396246	34.157096	3.936294
-2.250470	43.043921	3.946291
-1.647069	58.754406	3.956288
-1.101762	72.284909	3.966285
-0.843084	89.878117	3.976282
-0.234239	117.818197	3.986278
0.000000	123.996720	3.991283
0.405313	130.976603	3.996288
0.550018	126.459236	4.001293
0.594979	144.005575	4.006298
1.054174	151.449577	4.011302
0.878617	148.827958	4.016307
0.783238	157.621562	4.021312
1.058459	162.046788	4.026317
0.961450	157.016045	4.031322
1.226064	165.694326	4.036326
0.927166	157.633161	4.041331
0.862951	161.058169	4.046336
1.046963	167.266919	4.051341
0.873978	156.913987	4.056346
0.899676	158.922457	4.061350
0.956675	165.896194	4.066355
0.941999	160.710285	4.071360
1.054552	164.976346	4.076365
0.978411	165.704929	4.081370
1.001415	168.919019	4.086374
1.211346	162.692254	4.091379
1.305282	163.539121	4.096384
1.077339	169.367108	4.101389
1.028693	175.399161	4.106394
1.724418	192.811671	4.111398
1.044247	172.383246	4.116403
1.368292	168.003929	4.121408
1.100969	176.313980	4.126413
1.271213	184.855358	4.131418
1.566632	187.431265	4.136422
1.151762	189.282996	4.141427
1.288550	197.080585	4.146432
1.499826	192.331620	4.151437
1.204511	202.162325	4.156442
1.588665	184.978296	4.161446
1.434001	210.759545	4.166451
1.144146	191.872178	4.171456
1.593453	203.759046	4.176461
1.378459	195.397424	4.181466
1.552749	192.697462	4.186470
1.197046	196.268409	4.191475
1.558465	194.045458	4.196480
1.533079	191.029875	4.201485
1.410051	196.990774	4.206490
1.842630	194.609176	4.211494
1.656359	183.939889	4.216499
1.462974	176.380853	4.221504
1.478090	168.546072	4.226509
1.420860	172.568026	4.231514
1.324765	172.862406	4.236518
1.544696	182.793306	4.241523
1.572147	191.089472	4.246528
1.529225	189.407148	4.251533
1.401697	196.753997	4.256538
1.575428	195.858389	4.261542
1.519157	194.914081	4.266547
1.644933	192.883272	4.271552
1.446133	194.807413	4.276557
1.543985	204.415110	4.281562
1.789258	190.005110	4.286566
1.662779	200.235449	4.291571
1.574317	194.395063	4.296576
1.627358	189.794967	4.301581
1.393907	195.342926	4.306586
1.364116	189.419354	4.311590
1.449837	188.974707	4.316595
1.878286	188.698041	4.321600
1.809707	200.971270	4.326605
2.020702	196.329679	4.331610
2.086882	189.392822	4.336614
1.863689	193.453356	4.341619
1.926462	187.207298	4.346624
1.861943	196.204365	4.351629
1.630770	193.188067	4.356634
1.980586	196.725677	4.361638
1.924957	196.726108	4.366643
2.348877	192.132490	4.371648
2.042463	205.039674	4.376653
2.097053	192.982755	4.381658
2.007623	195.316753	4.386662
2.191542	192.723712	4.391667
1.891706	196.624676	4.396672
1.945032	194.469114	4.401677
1.831977	195.220964	4.406682
1.927627	187.720694	4.411686
1.923138	202.880806	4.416691
2.091056	201.848742	4.421696
2.139494	194.640574	4.426701
1.788022	204.577236	4.431706
2.193324	192.731369	4.436710
1.772589	205.702627	4.441715
1.829257	196.886229	4.446720
1.695610	197.530799	4.451725
1.816514	217.576533	4.456730
2.215855	220.192684	4.461734
2.146227	228.624672	4.466739
2.269908	225.934055	4.471744
2.278161	243.830264	4.476749
2.204704	226.755256	4.481754
2.391808	231.477395	4.486758
1.954032	233.847758	4.491763
2.231176	228.653551	4.496768
2.412561	233.414417	4.501773
1.976122	231.204447	4.506778
2.100828	232.391303	4.511782
1.916974	236.907512	4.516787
2.033209	243.261457	4.521792
2.182683	238.867466	4.526797
1.917700	237.241366	4.531802
2.233069	232.912591	4.536806
2.189551	235.648001	4.541811
2.073659	242.294721	4.546816
2.536112	224.682894	4.551821
2.248413	240.223374	4.556826
2.408175	231.423951	4.561830
2.165014	230.916758	4.566835
2.595293	234.578988	4.571840
2.311150	231.632993	4.576845
2.299693	240.419187	4.581850
2.293365	225.779946	4.586854
1.807113	245.692460	4.591859
2.472869	249.415708	4.596864
2.493555	254.865756	4.601869
2.385964	261.713537	4.606874
2.710829	262.485648	4.611878
2.765325	262.072400	4.616883
2.780509	267.870405	4.621888
2.729668	260.934111	4.626893
2.199791	242.797993	4.631898
2.729789	242.965919	4.636902
2.417768	246.159532	4.641907
2.440489	254.275496	4.646912
2.842925	249.968728	4.651917
2.808857	256.593151	4.656922
2.863999	264.145810	4.661926
2.494611	240.527648	4.666931
2.436172	253.090451	4.671936
2.945987	235.600605	4.676941
2.514900	247.960613	4.681946
2.722073	235.053058	4.686950
2.797369	246.891976	4.691955
2.616461	252.054338	4.696960
2.518684	240.838675	4.701965
2.624488	263.957871	4.706970
2.956191	255.966454	4.711974
2.763789	258.737226	4.716979
2.951852	272.229509	4.721984
2.504282	264.838608	4.726989
2.797714	258.289236	4.731994
3.101417	267.165710	4.736998
2.988115	266.054835	4.742003
3.095885	260.955689	4.747008
2.618171	239.177162	4.752013
2.819007	239.386563	4.757018
2.991640	246.865737	4.762022
2.866986	247.621183	4.767027
2.854197	240.214669	4.772032
2.976624	234.633090	4.777037
2.657329	255.236180	4.782042
3.147042	256.383037	4.787046
3.139928	250.921507	4.792051
3.175787	242.965574	4.797056
2.946499	244.757638	4.802061
2.979501	241.769981	4.807066
2.971621	230.759848	4.812070
2.719585	241.461390	4.817075
2.971393	247.183585	4.822080
3.089513	271.448622	4.827085
2.942546	274.063620	4.832090
3.180109	253.767722	4.837094
2.934092	268.447447	4.842099
2.998715	260.357817	4.847104
3.205267	254.461748	4.852109
2.814561	251.642267	4.857114
3.007408	262.358590	4.862118
2.794841	265.332656	4.867123
3.105604	267.026002	4.872128
3.073027	256.378123	4.877133
2.918283	262.790177	4.882138
3.088646	256.777369	4.887142
2.724403	263.380206	4.892147
2.899793	260.931010	4.897152
3.286318	269.872816	4.902157
3.104370	271.817856	4.907162
3.444991	271.082686	4.912166
3.007484	283.903188	4.917171
3.395955	280.950888	4.922176
3.451063	276.415631	4.927181
3.109687	287.025331	4.932186
3.600753	273.665679	4.937190
3.621329	290.143222	4.942195
3.388004	266.743333	4.947200
3.290644	279.175962	4.952205
3.058266	270.634180	4.957210
3.750124	273.472787	4.962214
3.313589	279.069728	4.967219
2.889692	274.146239	4.972224
3.400855	296.145524	4.977229
3.325601	294.891139	4.982234
3.687158	304.604771	4.987238
3.588303	300.451860	4.992243
3.727026	281.681477	4.997248
3.677439	269.010663	5.002253
3.640436	282.957728	5.007258
3.235895	267.873555	5.012262
3.077241	269.667661	5.017267
3.622627	280.387588	5.022272
3.981993	298.533617	5.027277
3.250331	276.559953	5.032282
3.564526	264.748619	5.037286
3.099224	278.472294	5.042291
3.502325	284.341542	5.047296
3.806146	284.735561	5.052301
3.666391	298.146106	5.057306
4.097154	287.982545	5.062310
3.631586	281.980910	5.067315
3.491077	267.461761	5.072320
3.636380	278.016772	5.077325
3.220883	296.783898	5.082330
3.639561	290.233544	5.087334
3.418200	291.834900	5.092339
3.753785	290.424033	5.097344
3.771255	294.676250	5.102349
3.649896	296.187291	5.107354
3.696506	289.512968	5.112358
3.809747	302.002456	5.117363
3.802340	292.832086	5.122368
3.851924	293.791351	5.127373
3.995247	303.191932	5.132378
3.627267	295.965133	5.137382
3.400102	300.291616	5.142387
3.505819	295.748286	5.147392
3.696817	303.197719	5.152397
3.332329	307.293965	5.157402
3.945491	298.067499	5.162406
3.634935	305.107765	5.167411
3.766915	316.041248	5.172416
4.001018	330.060943	5.177421
3.871101	338.787852	5.182426
4.439532	329.931095	5.187430
3.780099	332.374506	5.192435
3.588060	319.259797	5.197440
3.800670	332.618551	5.202445
3.987684	337.159224	5.207450
4.177003	327.027154	5.212454
3.968494	339.504738	5.217459
4.050802	348.067350	5.222464
4.270073	327.056020	5.227469
4.053794	349.069356	5.232474
4.085221	333.451986	5.237478
3.999698	349.672491	5.242483
4.119005	331.566891	5.247488
4.043456	339.703678	5.252493
4.103338	340.714810	5.257498
4.239477	338.957597	5.262502
4.079247	340.580620	5.267507
3.779455	348.244557	5.272512
3.804437	342.391680	5.277517
3.756854	329.241547	5.282522
4.154056	335.104982	5.287526
4.134324	344.927524	5.292531
3.866171	341.072286	5.297536
4.200052	339.049386	5.302541
4.078246	342.197674	5.307546
4.095623	341.158419	5.312550
3.963237	346.918694	5.317555
4.281938	359.909639	5.322560
4.644786	370.545266	5.327565
4.099757	357.467946	5.332570
4.455289	364.172649	5.337574
4.587406	377.454581	5.342579
4.419650	345.436644	5.347584
4.392328	353.340353	5.352589
4.106972	340.087747	5.357594
4.268396	348.899492	5.362598
4.646961	356.167811	5.367603
4.323968	349.463885	5.372608
4.567311	356.833174	5.377613
4.358622	342.427323	5.382618
4.549973	358.287884	5.387622
4.153805	347.765729	5.392627
4.367371	369.262265	5.397632
4.916156	368.768806	5.402637
4.317245	362.253219	5.407642
4.241498	379.634614	5.412646
4.453262	371.275862	5.417651
4.451724	383.562031	5.422656
4.758628	376.410698	5.427661
4.517590	369.488228	5.432666
4.793688	359.495587	5.437670
4.611481	369.817720	5.442675
4.582468	371.339945	5.447680
4.674743	368.634763	5.452685
4.798435	367.846064	5.457690
4.732014	358.318238	5.462694
4.456282	358.597522	5.467699
4.384010	357.295386	5.472704
4.727798	363.904368	5.477709
4.543483	366.559785	5.482714
4.570438	371.135798	5.487718
4.712674	374.837281	5.492723
4.903504	383.820570	5.497728
5.096914	366.852334	5.502733
4.548234	385.180297	5.507738
4.809439	373.153408	5.512742
4.856065	377.316682	5.517747
4.711228	371.911707	5.522752
5.291204	363.774242	5.527757
4.334218	362.762935	5.532762
4.622115	374.506246	5.537766
4.663980	373.105342	5.542771
4.981754	373.445661	5.547776
4.818282	371.994544	5.552781
4.653075	386.270575	5.557786
4.873324	371.764017	5.562790
4.726217	379.701148	5.567795
4.637670	373.348524	5.572800
4.778670	370.296432	5.577805
4.676376	380.299751	5.582810
4.769094	367.977637	5.587814
4.358485	378.056867	5.592819
4.580459	378.508215	5.597824
4.753413	398.602702	5.602829
4.810264	400.691386	5.607834
5.503955	394.693449	5.612838
5.089109	398.730073	5.617843
4.761936	394.843537	5.622848
4.775902	404.085918	5.627853
4.796004	407.225466	5.632858
4.956073	397.643908	5.637862
4.796418	416.286034	5.642867
4.596031	403.677911	5.647872
4.823331	381.363410	5.652877
4.761363	406.300921	5.657882
4.865271	409.292951	5.662886
5.094530	424.583933	5.667891
5.100142	431.147815	5.672896
5.264652	426.339524	5.677901
5.160584	437.113425	5.682906
5.383015	420.579913	5.687910
5.325282	435.906202	5.692915
5.553655	426.024692	5.697920
5.347157	412.131683	5.702925
5.267618	418.005969	5.707930
5.112561	403.486234	5.712934
5.217251	397.305671	5.717939
5.319777	406.543974	5.722944
5.274681	410.709492	5.727949
5.301995	426.562411	5.732954
5.363878	418.151555	5.737958
5.234717	427.329906	5.742963
5.470628	432.862729	5.747968
5.572974	420.331029	5.752973
4.918575	410.029174	5.757978
5.284174	414.582578	5.762982
5.220460	437.373238	5.767987
5.266177	419.273086	5.772992
5.504610	426.415835	5.777997
4.743629	439.270589	5.783002
5.154998	429.105207	5.788006
5.310390	434.596883	5.793011
5.356625	437.436467	5.798016
5.430520	432.550321	5.803021
5.315890	434.726539	5.808026
5.181869	431.781245	5.813030
5.311037	447.615380	5.818035
5.271136	451.576538	5.823040
5.532211	474.571444	5.828045
5.316347	470.397281	5.833050
5.761599	460.649484	5.838054
5.517120	467.243072	5.843059
5.585599	467.687433	5.848064
5.818971	479.304980	5.853069
5.616765	458.907867	5.858074
5.948206	477.200974	5.863078
5.898796	461.065806	5.868083
5.534945	463.552527	5.873088
5.383572	461.019587	5.878093
5.404321	475.638454	5.883098
5.916258	467.724474	5.888102
5.603656	473.385741	5.893107
5.465249	477.404617	5.898112
5.841198	469.472861	5.903117
5.722097	481.618725	5.908122
5.497750	476.239677	5.913126
5.562856	479.238724	5.918131
5.376570	484.558412	5.923136
5.855864	463.486957	5.928141
5.544821	478.287325	5.933146
5.520406	485.622304	5.938150
5.579534	470.203533	5.943155
5.669441	483.547677	5.948160
6.217619	478.868527	5.953165
5.735990	485.052066	5.958170
5.989130	479.176622	5.963174
5.701197	476.533269	5.968179
6.035802	473.739683	5.973184
6.088124	466.397471	5.978189
5.647556	491.514983	5.983194
6.018125	472.245952	5.988198
5.605177	496.407040	5.993203
5.871456	495.863491	5.998208
6.036200	504.439104	6.003213
5.872134	505.483509	6.008218
5.903143	509.988063	6.013222
5.921734	502.957615	6.018227
5.989398	504.637400	6.023232
6.321886	508.245621	6.028237
6.104638	497.540590	6.033242
6.101253	487.066676	6.038246
5.863256	480.006431	6.043251
5.798332	467.570603	6.048256
5.998804	485.907661	6.053261
6.104259	483.360388	6.058266
6.115754	472.066618	6.063270
5.696860	470.413546	6.068275
5.786172	484.339720	6.073280
6.158182	490.043129	6.078285
5.785347	485.374230	6.083290
6.141150	487.520160	6.088294
5.956590	483.836235	6.093299
5.796353	470.453340	6.098304
6.150937	472.848853	6.103309
5.873196	487.350148	6.108314
5.795523	489.757616	6.113318
5.906201	487.603880	6.118323
6.029284	501.157120	6.123328
6.220101	488.439588	6.128333
6.293052	489.775494	6.133338
5.986597	481.011641	6.138342
5.664629	481.377291	6.143347
5.643494	464.892271	6.148352
5.976664	490.468677	6.153357
5.878962	495.748870	6.158362
6.162147	500.897952	6.163366
6.125364	501.093948	6.168371
6.183330	486.158637	6.173376
6.254827	479.156942	6.178381
5.962176	482.384002	6.183386
5.831268	469.288756	6.188390
6.054754	462.020754	6.193395
6.040453	472.879677	6.198400
5.911326	460.601354	6.203405
5.586816	469.291047	6.208410
6.001535	473.538824	6.213414
5.621277	479.798535	6.218419
5.836709	460.452661	6.223424
6.086707	478.826212	6.228429
5.659555	465.407428	6.233434
6.292266	479.286213	6.238438
6.096834	482.807852	6.243443
6.052052	471.162327	6.248448
6.062170	466.426990	6.253453
5.870813	476.235854	6.258458
6.166258	467.920734	6.263462
6.227547	461.689114	6.268467
5.896461	472.994591	6.273472
5.956569	457.049675	6.278477
5.826873	468.955887	6.283482
5.960983	458.453251	6.288486
6.068665	466.589123	6.293491
5.913642	466.071894	6.298496
5.937353	465.341540	6.303501
5.970239	478.182915	6.308506
5.761866	471.282821	6.313510
5.801657	473.663277	6.318515
5.300940	471.073342	6.323520
6.050736	467.923381	6.328525
6.171291	487.543954	6.333530
6.172243	486.792698	6.338534
6.153403	481.206752	6.343539
5.783374	468.134057	6.348544
5.995981	469.361945	6.353549
5.839382	479.539638	6.358554
6.261579	463.192957	6.363558
6.043932	465.233495	6.368563
5.633596	466.587909	6.373568
5.834328	467.279923	6.378573
5.828789	468.696176	6.383578
5.890790	477.997152	6.388582
6.056005	468.926789	6.393587
6.239686	487.786209	6.398592
6.078671	466.636587	6.403597
6.143522	475.134481	6.408602
6.061713	472.946758	6.413606
6.063982	450.074000	6.418611
5.565026	471.010219	6.423616
6.226253	462.768320	6.428621
6.068825	471.006605	6.433626
5.788820	468.810304	6.438630
5.820791	457.162067	6.443635
5.864297	469.247213	6.448640
6.192566	457.523275	6.453645
5.997301	460.473209	6.458650
6.079885	475.328677	6.463654
5.938090	465.631432	6.468659
5.965473	469.878705	6.473664
6.144343	465.037744	6.478669
5.821500	470.562299	6.483674
5.644272	471.104483	6.488678
5.971724	468.603786	6.493683
5.506670	485.456954	6.498688
5.965378	460.113345	6.503693
5.669510	474.604501	6.508698
5.927393	487.421724	6.513702
6.301027	493.859605	6.518707
5.706154	477.385240	6.523712
6.204693	489.133092	6.528717
5.720413	472.497117	6.533722
6.159476	487.783283	6.538726
6.003048	462.558395	6.543731
5.675489	471.395877	6.548736
6.179902	467.533578	6.553741
6.183333	496.890764	6.558746
6.102487	482.383155	6.563750
6.061021	487.437912	6.568755
6.233433	493.659957	6.573760
6.379602	474.790642	6.578765
6.106422	473.753919	6.583770
6.256477	472.958194	6.588774
6.232840	470.805746	6.593779
5.939696	468.072301	6.598784
6.479169	459.010922	6.603789
6.004715	473.173001	6.608794
6.109960	463.914957	6.613798
6.058269	460.821987	6.618803
5.814040	443.076622	6.623808
6.000172	441.609253	6.628813
5.780717	448.625157	6.633818
5.921328	463.095369	6.638822
6.099192	472.238495	6.643827
5.970015	467.384024	6.648832
6.304236	458.780658	6.653837
5.521638	462.854299	6.658842
5.621912	449.628132	6.663846
6.225692	465.488714	6.668851
6.170081	473.446582	6.673856
5.931861	460.013744	6.678861
5.629244	453.743322	6.683866
6.269768	463.130197	6.688870
5.958476	462.974496	6.693875
5.944668	453.916660	6.698880
5.791950	453.102412	6.703885
5.687089	471.148093	6.708890
6.527617	469.818901	6.713894
6.391613	455.501257	6.718899
6.095573	454.917858	6.723904
6.143639	456.898896	6.728909
5.857552	453.695605	6.733914
6.250267	447.835876	6.738918
6.287185	451.693285	6.743923
5.854082	454.317425	6.748928
6.248679	443.369460	6.753933
6.056343	456.578612	6.758938
5.976156	452.253490	6.763942
6.178339	457.455404	6.768947
6.056601	441.008935	6.773952
5.889814	442.024387	6.778957
5.725966	450.087436	6.783962
5.808541	450.258774	6.788966
6.035343	449.148205	6.793971
5.797151	459.953758	6.798976
5.904960	442.338931	6.803981
5.852228	448.489456	6.808986
6.040006	447.402994	6.813990
5.852258	455.258492	6.818995
5.444742	444.035171	6.824000
6.110473	448.136300	6.829005
5.943548	441.053280	6.834010
5.899023	450.742174	6.839014
6.048890	434.896385	6.844019
5.784469	449.022055	6.849024
5.913451	446.929422	6.854029
5.654369	432.840486	6.859034
5.612018	441.472288	6.864038
5.938357	440.978004	6.869043
5.748287	441.807898	6.874048
6.000963	444.303905	6.879053
6.094121	445.372976	6.884058
5.999679	440.283217	6.889062
5.886083	438.337116	6.894067
5.969427	448.526829	6.899072
6.103941	447.955042	6.904077
5.915457	443.825684	6.909082
5.900753	442.196279	6.914086
5.997351	444.443145	6.919091
5.876085	450.286162	6.924096
5.981133	447.715781	6.929101
6.202223	437.050713	6.934106
6.046107	440.425369	6.939110
5.963109	440.679116	6.944115
5.950632	440.786849	6.949120
6.331514	442.632385	6.954125
6.280304	432.419742	6.959130
6.140138	444.215008	6.964134
6.048970	446.624897	6.969139
5.716373	444.245912	6.974144
6.288293	447.041337	6.979149
5.962974	443.538029	6.984154
5.927058	443.059714	6.989158
6.530992	443.992977	6.994163
6.217567	434.927155	6.999168
6.215552	443.784314	7.004173
6.090050	436.555059	7.009178
5.736266	419.955188	7.014182
5.848036	429.243965	7.019187
5.703935	438.376946	7.024192
5.658840	444.138220	7.029197
5.586615	450.431456	7.034202
5.946451	439.757860	7.039206
6.059559	446.699862	7.044211
5.779524	446.467278	7.049216
5.803109	450.079972	7.054221
5.600890	449.511748	7.059226
5.810809	452.255328	7.064230
5.684389	448.016176	7.069235
5.627282	443.224479	7.074240
5.932520	447.865506	7.079245
5.824299	443.846491	7.084250
5.530102	443.667052	7.089254
6.133107	469.006858	7.094259
5.732086	482.127010	7.099264
6.319307	465.572328	7.104269
6.101150	472.858227	7.109274
5.708314	453.448833	7.114278
6.188518	467.737347	7.119283
5.837195	469.450364	7.124288
6.228056	456.495495	7.129293
5.883733	467.091996	7.134298
6.075758	444.234546	7.139302
6.210758	446.441623	7.144307
5.688704	444.232452	7.149312
5.915384	434.359995	7.154317
5.947505	440.055039	7.159322
6.171790	451.063628	7.164326
6.131416	445.198429	7.169331
6.036491	441.160151	7.174336
6.036627	440.688012	7.179341
5.812491	443.294582	7.184346
5.940297	441.705353	7.189350
6.258029	428.054688	7.194355
6.066797	442.786096	7.199360
6.069793	425.200843	7.204365
6.277482	436.435505	7.209370
5.909156	440.908964	7.214374
6.045331	448.363681	7.219379
6.298845	436.171495	7.224384
5.990159	436.859010	7.229389
6.020987	449.306107	7.234394
5.853920	439.882267	7.239398
6.213382	439.359228	7.244403
5.977686	439.993347	7.249408
6.164349	448.902291	7.254413
5.881302	436.301784	7.259418
5.913974	444.356423	7.264422
5.946304	430.566180	7.269427
5.614838	438.932944	7.274432
5.770326	448.114773	7.279437
5.619655	449.949113	7.284442
5.799493	449.071915	7.289446
5.743767	442.827580	7.294451
5.729265	442.808094	7.299456
5.859571	447.334102	7.304461
5.646333	452.279322	7.309466
5.681574	444.301288	7.314470
5.809200	454.485561	7.319475
6.063234	475.050622	7.324480
6.220693	466.868301	7.329485
5.912497	459.785436	7.334490
5.649207	459.739984	7.339494
6.230144	463.567469	7.344499
6.197594	452.877423	7.349504
6.063218	455.580931	7.354509
5.759602	454.018015	7.359514
5.885626	454.808594	7.364518
6.131902	446.873418	7.369523
5.602103	454.162869	7.374528
5.936214	444.767377	7.379533
5.896151	463.031403	7.384538
5.796219	451.884108	7.389542
6.110184	472.374351	7.394547
5.886183	469.346849	7.399552
6.114729	456.327555	7.404557
5.888955	457.583399	7.409562
5.764607	456.593996	7.414566
6.186057	471.728374	7.419571
5.873348	458.385483	7.424576
5.790265	453.336952	7.429581
5.851358	473.279261	7.434586
5.956647	469.385853	7.439590
6.161730	477.541442	7.444595
5.887860	482.024951	7.449600
5.990344	475.673071	7.454605
6.089691	483.019064	7.459610
5.904635	464.111673	7.464614
6.147239	453.755165	7.469619
5.949814	460.617783	7.474624
5.907173	454.672654	7.479629
6.045098	447.336723	7.484634
5.822921	456.879484	7.489638
6.427379	439.447259	7.494643
6.075551	457.580005	7.499648
5.894504	446.335829	7.504653
5.999776	452.691476	7.509658
6.004051	450.420477	7.514662
6.295364	453.796462	7.519667
5.873919	455.370922	7.524672
5.926071	447.328436	7.529677
5.825288	451.208208	7.534682
5.861918	447.195440	7.539686
5.975991	450.439424	7.544691
5.644889	458.575694	7.549696
5.615445	444.137362	7.554701
5.628874	459.624748	7.559706
5.777306	474.064969	7.564710
6.202021	488.725111	7.569715
5.901543	488.157833	7.574720
6.203233	491.465721	7.579725
6.074888	471.932883	7.584730
6.134237	480.140771	7.589734
6.111941	465.733991	7.594739
6.007050	462.739583	7.599744
5.972011	462.847690	7.604749
5.952972	458.842443	7.609754
5.827516	451.225778	7.614758
5.556290	458.412224	7.619763
5.852683	465.592073	7.624768
6.298097	482.115820	7.629773
5.909468	471.346895	7.634778
5.565930	466.059563	7.639782
6.143859	476.680532	7.644787
6.005413	479.798946	7.649792
6.093198	482.620130	7.654797
5.901628	473.583077	7.659802
5.868006	472.184380	7.664806
6.112360	473.551344	7.669811
5.878246	452.620493	7.674816
6.106554	466.479980	7.679821
5.978663	444.981219	7.684826
5.886974	459.680507	7.689830
6.136290	452.890537	7.694835
5.834227	449.932959	7.699840
5.991083	452.249181	7.704845
5.652710	452.872450	7.709850
5.795458	466.979678	7.714854
6.393936	465.316509	7.719859
6.068007	467.210494	7.724864
6.058134	456.024735	7.729869
5.998005	455.493204	7.734874
5.961170	454.809456	7.739878
5.954337	449.240085	7.744883
5.592271	459.885779	7.749888
5.626573	448.538536	7.754893
5.651995	473.647470	7.759898
5.903136	477.509436	7.764902
6.125760	486.561420	7.769907
5.985610	482.998399	7.774912
6.016691	489.628928	7.779917
6.164528	492.513091	7.784922
6.215743	467.998879	7.789926
6.207885	467.497676	7.794931
5.836169	457.620615	7.799936
5.991757	459.621370	7.804941
5.918592	450.088288	7.809946
5.623695	462.152703	7.814950
5.886038	461.820520	7.819955
6.125838	470.086875	7.824960
6.203093	460.109273	7.829965
6.003909	465.803882	7.834970
5.829189	451.044478	7.839974
5.916913	463.541965	7.844979
5.696001	455.194989	7.849984
6.027779	458.279882	7.854989
6.049487	468.569467	7.859994
5.467535	473.414632	7.864998
6.245929	486.036628	7.870003
5.949812	491.320312	7.875008
5.872808	486.646718	7.880013
5.859934	498.856328	7.885018
6.012524	497.093616	7.890022
5.863660	485.329735	7.895027
5.995278	505.437902	7.900032
6.183444	496.734650	7.905037
6.258212	484.456644	7.910042
5.812569	470.940091	7.915046
5.948452	466.377026	7.920051
5.685895	485.348464	7.925056
5.946509	486.996854	7.930061
6.010903	488.519142	7.935066
5.823694	494.599277	7.940070
6.153888	492.416464	7.945075
6.094754	486.223676	7.950080
5.754770	475.870011	7.955085
5.923310	479.970648	7.960090
5.776237	494.565281	7.965094
6.489965	490.476315	7.970099
6.172642	481.567369	7.975104
6.082960	462.556816	7.980109
5.814918	457.571602	7.985114
5.601026	458.396062	7.990118
5.874928	461.966329	7.995136
5.670682	482.149957	8.000154
6.314310	485.300669	8.005171
5.937004	472.936110	8.010189
5.981932	462.921674	8.015206
6.012556	477.129569	8.020224
5.961802	467.734709	8.025242
6.117052	474.431789	8.030259
6.031777	459.665015	8.035277
5.897092	473.237715	8.040294
6.045900	455.280684	8.045312
5.695042	483.783749	8.050330
6.097692	474.441772	8.055347
6.228267	477.098397	8.060365
6.104396	484.801775	8.065382
6.272985	470.013307	8.070400
5.672842	468.339776	8.075418
5.961595	473.512655	8.080435
5.993461	493.804679	8.085453
6.087067	495.437194	8.090470
6.064849	499.208534	8.095488
6.055166	500.559087	8.100506
6.391237	500.639060	8.105523
6.088644	472.583461	8.110541
5.859160	471.735927	8.115558
6.239221	480.686748	8.120576
5.943022	484.369838	8.125594
6.247560	483.790837	8.130611
6.243650	467.152665	8.135629
6.167318	464.647010	8.140646
5.799940	469.425708	8.145664
6.185101	472.561372	8.150682
6.032062	479.528141	8.155699
6.294713	478.363709	8.160717
6.095823	486.927772	8.165734
6.295109	465.461004	8.170752
5.968169	463.778829	8.175770
6.023292	482.930404	8.180787
6.264230	488.852914	8.185805
6.175925	471.347237	8.190822
6.181511	464.220874	8.195840
5.910564	472.025399	8.200858
6.126766	482.923334	8.205875
6.174749	496.003399	8.210893
6.220068	489.220262	8.215910
6.525809	482.676687	8.220928
6.089678	489.655708	8.225946
5.971779	490.541603	8.230963
6.348626	495.758085	8.235981
6.104163	489.882735	8.240998
6.333551	497.372663	8.246016
6.344644	489.231390	8.251034
6.072929	490.231459	8.256051
6.166202	477.391010	8.261069
6.009129	508.952177	8.266086
6.405704	488.420711	8.271104
6.114734	503.618131	8.276122
5.886366	500.124198	8.281139
6.016624	508.998637	8.286157
5.882076	498.145279	8.291174
6.150665	509.652318	8.296192
6.013391	490.502121	8.301210
5.807038	503.682672	8.306227
6.126121	493.173327	8.311245
5.918516	521.315382	8.316262
6.269104	521.068439	8.321280
6.173042	530.293692	8.326298
6.330611	535.707602	8.331315
6.789660	532.050563	8.336333
6.171192	519.899098	8.341350
6.413831	524.839823	8.346368
6.415935	514.384815	8.351386
6.323582	524.043581	8.356403
6.227464	502.762254	8.361421
6.297641	523.958658	8.366438
6.433957	516.324580	8.371456
6.581655	523.948854	8.376474
6.496423	498.920021	8.381491
6.248048	495.784315	8.386509
6.319283	495.940133	8.391526
6.216639	486.459473	8.396544
6.074948	501.723534	8.401562
6.110935	510.673380	8.406579
6.530296	510.745787	8.411597
6.508509	523.106899	8.416614
6.681086	519.801845	8.421632
6.753740	526.093917	8.426650
6.396503	501.165724	8.431667
6.454391	493.821017	8.436685
6.227955	482.300861	8.441702
6.388772	484.387786	8.446720
6.374110	503.159102	8.451738
6.298676	519.367968	8.456755
6.830856	512.613680	8.461773
6.719305	510.572274	8.466790
6.503016	493.555702	8.471808
6.376243	499.920276	8.476826
6.140158	496.964477	8.481843
6.353339	498.739783	8.486861
6.226722	518.250677	8.491878
6.206756	517.973266	8.496896
6.432892	524.017985	8.501914
6.610094	517.530373	8.506931
6.791448	509.849988	8.511949
6.542596	521.458194	8.516966
7.006254	510.819167	8.521984
6.943143	496.246769	8.527002
6.501013	496.699276	8.532019
6.677056	478.904007	8.537037
6.574803	494.320850	8.542054
6.351211	481.360371	8.547072
6.330173	484.299363	8.552090
6.110915	494.089584	8.557107
6.379826	503.514961	8.562125
6.198596	514.000387	8.567143
6.636571	521.241447	8.572160
6.582182	519.903879	8.577178
6.481622	522.878849	8.582195
6.658951	522.890101	8.587213
6.482673	519.498154	8.592231
6.480559	516.071521	8.597248
6.617888	524.111274	8.602266
6.480281	531.594860	8.607283
6.798726	521.098983	8.612301
6.712261	540.000682	8.617319
6.768180	539.782462	8.622336
6.548496	521.536050	8.627354
6.739319	548.581987	8.632371
6.911426	528.464724	8.637389
6.573998	535.025203	8.642407
6.864656	532.215056	8.647424
6.768471	529.517647	8.652442
6.750893	539.641984	8.657459
6.827245	525.035785	8.662477
6.767318	510.419551	8.667495
6.356636	503.056338	8.672512
6.623530	514.266008	8.677530
6.788716	521.522433	8.682547
6.867184	529.202137	8.687565
6.675729	528.729309	8.692583
6.846021	508.812217	8.697600
6.733309	515.540906	8.702618
6.200097	508.052412	8.707635
6.755744	531.384221	8.712653
6.895714	524.587295	8.717671
6.634189	520.981052	8.722688
6.775882	535.154707	8.727706
6.515140	532.594600	8.732723
6.747812	527.462006	8.737741
6.419049	520.256557	8.742759
6.692915	524.406807	8.747776
6.631460	526.764067	8.752794
6.494512	531.018814	8.757811
6.843528	529.969302	8.762829
6.882180	521.496577	8.767847
6.757921	520.865835	8.772864
6.794393	532.903636	8.777882
6.726755	539.532197	8.782899
6.591271	532.645098	8.787917
6.702375	530.389875	8.792935
6.616705	534.065538	8.797952
7.018613	509.280697	8.802970
6.633853	529.240946	8.807987
6.784837	523.281927	8.813005
7.006315	531.286719	8.818023
6.839190	518.806209	8.823040
7.099743	527.832997	8.828058
6.702393	535.959148	8.833075
6.845760	517.642509	8.838093
6.805372	527.912302	8.843111
6.536272	516.983949	8.848128
7.017446	526.966422	8.853146
6.837029	519.967397	8.858163
6.929801	523.818039	8.863181
6.774848	538.464423	8.868199
6.726790	525.622692	8.873216
7.134320	538.205305	8.878234
6.577000	550.988907	8.883251
6.948053	544.911152	8.888269
6.884626	558.223009	8.893287
6.843903	542.553073	8.898304
7.155486	561.893108	8.903322
7.258351	545.035193	8.908339
6.845615	550.343118	8.913357
7.077373	552.331541	8.918375
7.006292	539.002007	8.923392
6.935814	539.734536	8.928410
6.700370	539.631181	8.933427
7.105770	549.387378	8.938445
7.130932	560.717324	8.943463
6.502702	560.488284	8.948480
6.967899	550.065550	8.953498
6.893144	566.202327	8.958515
6.726700	547.273355	8.963533
7.062838	545.660279	8.968551
7.147928	557.326877	8.973568
7.359596	552.153762	8.978586
7.303215	547.141942	8.983603
7.330236	548.964354	8.988621
7.378481	561.965614	8.993639
7.101911	541.959677	8.998656
6.929682	528.290568	9.003674
6.748941	546.319321	9.008691
7.032531	547.207943	9.013709
7.030129	563.974709	9.018727
7.039559	571.418075	9.023744
7.201914	564.801535	9.028762
7.137165	567.370607	9.033779
7.307615	561.554381	9.038797
7.326975	554.589728	9.043815
7.039703	553.985532	9.048832
7.282686	564.459826	9.053850
7.209764	553.281666	9.058867
6.808489	549.190877	9.063885
7.265387	542.738209	9.068903
7.108249	564.200126	9.073920
6.887410	544.517660	9.078938
6.967444	561.295005	9.083955
6.960153	561.889176	9.088973
7.108374	553.743606	9.093991
6.788082	568.755733	9.099008
7.213436	548.915598	9.104026
7.199267	560.566917	9.109043
7.154394	548.635118	9.114061
7.503950	555.372839	9.119079
7.194747	562.503211	9.124096
7.547284	552.933608	9.129114
7.024226	557.779192	9.134131
7.205642	557.972593	9.139149
7.312707	558.332176	9.144167
7.301866	560.481231	9.149184
7.581872	554.374437	9.154202
7.497864	575.287620	9.159219
7.386018	557.123318	9.164237
7.264973	564.686445	9.169255
7.195656	556.649147	9.174272
7.199550	548.263430	9.179290
7.252965	564.265766	9.184307
7.502282	562.594420	9.189325
7.389149	559.125904	9.194343
6.803213	575.435236	9.199360
7.294898	571.085974	9.204378
7.175905	566.935837	9.209395
6.950865	570.825533	9.214413
6.976522	559.099924	9.219431
7.047996	568.772085	9.224448
7.255666	565.832576	9.229466
7.065173	563.902607	9.234483
7.035481	596.843798	9.239501
7.614351	581.805970	9.244519
7.463167	602.212126	9.249536
7.362133	588.378385	9.254554
7.432179	618.696371	9.259571
7.563658	594.493046	9.264589
7.517390	592.641081	9.269607
7.092950	593.374153	9.274624
7.027662	585.926170	9.279642
7.100762	614.484774	9.284659
7.221146	597.212699	9.289677
7.801603	597.616948	9.294695
7.173601	611.697561	9.299712
7.295560	595.225699	9.304730
7.397900	609.754748	9.309747
7.112597	612.858764	9.314765
7.482765	597.606856	9.319783
7.212415	604.185110	9.324800
7.410010	598.029140	9.329818
7.202668	594.222936	9.334835
7.456025	608.416874	9.339853
7.672974	601.297533	9.344871
7.378912	606.518757	9.349888
7.793695	601.422461	9.354906
7.533319	592.569509	9.359923
7.710046	602.417847	9.364941
7.827404	590.048785	9.369959
7.663676	620.219633	9.374976
7.529451	599.635620	9.379994
7.364588	596.472907	9.385011
7.604968	601.013841	9.390029
7.675272	578.044138	9.395047
7.490104	597.362207	9.400064
7.811875	585.970804	9.405082
7.945800	595.983452	9.410099
7.823329	594.552924	9.415117
7.855717	585.056677	9.420135
7.801160	595.125860	9.425152
7.925651	581.510394	9.430170
7.839658	604.476632	9.435187
7.471400	587.322222	9.440205
7.564208	606.415771	9.445223
7.633676	596.502083	9.450240
7.700089	602.052898	9.455258
7.588360	598.687657	9.460275
7.590783	603.045439	9.465293
7.752705	595.173492	9.470311
7.669057	598.972228	9.475328
7.829899	592.418508	9.480346
7.598524	596.982007	9.485363
7.802360	604.951672	9.490381
7.683269	599.993396	9.495399
7.379432	594.851242	9.500416
7.852101	595.098058	9.505434
7.911186	595.818723	9.510451
7.792471	604.312727	9.515469
7.760436	595.871619	9.520487
7.746196	602.851618	9.525504
7.693918	599.271292	9.530522
7.915108	595.605332	9.535539
7.771412	614.544131	9.540557
8.173823	588.361723	9.545575
7.706065	584.620403	9.550592
7.391705	582.676167	9.555610
7.949830	587.919006	9.560627
7.745822	600.091851	9.565645
7.941879	590.211759	9.570663
7.666639	610.252903	9.575680
7.723961	594.844096	9.580698
7.590279	604.983235	9.585715
7.807607	610.992545	9.590733
7.926826	603.452268	9.595751
7.446231	622.031118	9.600768
7.681789	602.010920	9.605786
7.669182	601.417810	9.610803
7.354101	603.433735	9.615821
7.649950	605.188996	9.620839
7.748619	604.249141	9.625856
8.007671	591.970508	9.630874
8.198822	601.633735	9.635891
7.838745	601.400034	9.640909
8.031531	593.608594	9.645927
7.954218	603.422755	9.650944
7.586993	589.163939	9.655962
7.829460	596.596652	9.660979
7.671701	611.988445	9.665997
7.710401	600.894530	9.671015
7.957280	622.038351	9.676032
7.670423	623.033945	9.681050
7.933444	625.455183	9.686067
7.913692	638.556010	9.691085
8.034841	630.959804	9.696103
7.986505	627.142467	9.701120
7.990930	634.520666	9.706138
8.014558	635.747943	9.711155
7.735933	640.841072	9.716173
8.044980	641.719982	9.721191
7.890487	633.362165	9.726208
7.955765	636.489328	9.731226
8.212313	630.236913	9.736243
8.076001	634.482432	9.741261
8.218268	626.117395	9.746279
7.945132	637.234856	9.751296
8.010452	633.925364	9.756314
8.382240	635.341592	9.761331
7.967741	632.482556	9.766349
8.020598	638.176925	9.771367
7.977120	629.549453	9.776384
8.164811	628.521479	9.781402
8.312790	636.995632	9.786419
7.704059	627.292600	9.791437
7.909886	637.025354	9.796455
7.950177	623.521280	9.801472
7.893108	631.979232	9.806490
8.142253	642.042043	9.811507
7.847039	634.348745	9.816525
8.079445	635.995334	9.821543
8.150290	635.786748	9.826560
7.814065	635.422170	9.831578
8.249845	639.621459	9.836595
8.268077	653.485105	9.841613
8.284397	657.499654	9.846631
8.238293	648.706410	9.851648
8.018674	641.194264	9.856666
8.036791	646.309496	9.861683
8.077953	654.110946	9.866701
8.321018	660.958415	9.871719
8.425667	663.066356	9.876736
8.363120	679.188147	9.881754
8.402233	648.030605	9.886771
7.799534	645.438531	9.891789
8.070998	644.627850	9.896807
8.410331	661.439597	9.901824
8.319869	660.267187	9.906842
8.490628	664.181432	9.911859
8.259487	657.874108	9.916877
8.527719	655.587684	9.921895
8.795808	659.573319	9.926912
8.232162	646.563415	9.931930
8.448538	644.138062	9.936947
8.194740	633.600693	9.941965
8.178099	629.878385	9.946983
7.902678	640.952735	9.952000
8.399285	653.686327	9.957018
8.381095	654.222476	9.962035
8.483733	666.708083	9.967053
8.346032	674.970385	9.972071
8.704809	664.233655	9.977088
8.527303	666.206091	9.982106
8.899184	633.703280	9.987123
8.296243	634.982250	9.992141
8.063375	627.150045	9.997159
8.343909	636.496931	10.002176
8.285786	649.101193	10.007194
8.294060	645.230413	10.012211
8.074602	664.878950	10.017229
8.527632	646.765441	10.022247
8.666370	659.365123	10.027264
8.234849	667.317512	10.032282
8.621240	656.486976	10.037299
8.557095	666.425936	10.042317
8.446187	662.133529	10.047335
8.398108	663.980567	10.052352
8.006086	647.459474	10.057370
8.280682	665.804153	10.062387
8.143063	659.601222	10.067405
8.314032	657.143126	10.072423
8.562270	656.470499	10.077440
8.437853	664.042891	10.082458
8.906538	661.088469	10.087475
8.641159	663.637677	10.092493
8.550664	658.370800	10.097511
8.704613	659.712234	10.102528
8.324506	670.069260	10.107546
8.565635	659.773516	10.112563
8.672368	666.373019	10.117581
8.582141	658.789002	10.122599
8.543961	654.560346	10.127616
8.461401	667.545135	10.132634
8.541778	655.761897	10.137651
8.609986	662.098054	10.142669
8.463787	666.664717	10.147687
8.727532	658.431416	10.152704
8.773967	656.649532	10.157722
8.505273	658.485600	10.162739
8.472096	665.797213	10.167757
8.794953	662.004130	10.172775
8.840429	662.313477	10.177792
8.785590	664.205715	10.182810
8.544009	637.389791	10.187827
8.755603	665.471393	10.192845
8.528558	665.704846	10.197863
8.853026	664.888258	10.202880
8.592062	678.274585	10.207898
8.788552	682.716625	10.212915
8.916093	667.667498	10.217933
8.464893	679.307296	10.222951
8.824916	673.693100	10.227968
8.607130	688.577016	10.232986
8.901497	675.373631	10.238003
8.787691	685.987758	10.243021
8.307994	680.258071	10.248039
8.562055	687.653390	10.253056
8.615529	684.766501	10.258074
9.079164	699.980118	10.263091
8.720899	692.536812	10.268109
8.723988	698.753958	10.273127
8.999329	692.071065	10.278144
8.594353	698.362044	10.283162
9.006229	686.201742	10.288179
8.609572	685.305168	10.293197
8.713946	696.116254	10.298215
9.139927	682.023725	10.303232
8.764143	692.520761	10.308250
8.586839	686.857602	10.313267
8.993618	687.836671	10.318285
8.847512	675.692431	10.323303
8.892603	690.606016	10.328320
9.122022	692.636959	10.333338
9.331628	691.547205	10.338355
8.982739	690.291255	10.343373
8.930052	694.659745	10.348391
9.255258	688.265779	10.353408
8.947589	690.518812	10.358426
9.022830	697.671615	10.363443
8.749698	691.890665	10.368461
8.914971	690.096420	10.373479
9.322549	681.263997	10.378496
8.854442	698.124208	10.383514
9.000193	683.526462	10.388531
9.050397	698.340516	10.393549
8.957146	685.777995	10.398567
9.008841	687.498734	10.403584
8.873116	705.512755	10.408602
9.027858	686.213883	10.413619
8.991992	687.721102	10.418637
8.939252	684.839859	10.423655
9.273317	689.241748	10.428672
8.942231	693.515635	10.433690
9.126136	690.259053	10.438707
9.177888	674.367652	10.443725
8.900825	695.255045	10.448743
9.025239	674.746463	10.453760
8.828942	693.079847	10.458778
9.194312	702.310517	10.463795
9.528125	724.622082	10.468813
8.916351	716.655750	10.473831
9.208227	701.170386	10.478848
9.006117	718.432309	10.483866
9.133637	720.942867	10.488883
9.438335	725.545533	10.493901
9.392718	711.871670	10.498919
9.301499	699.416550	10.503936
8.886888	692.582397	10.508954
9.112513	721.074370	10.513971
9.382889	709.805512	10.518989
9.289143	720.298563	10.524007
9.345407	717.965391	10.529024
9.132811	731.994780	10.534042
9.368186	719.585151	10.539059
9.472950	734.267617	10.544077
9.438400	705.737191	10.549095
9.488823	703.012570	10.554112
9.332391	692.809369	10.559130
9.137835	686.834479	10.564147
9.257106	698.975428	10.569165
9.093884	690.775771	10.574183
9.392329	714.093588	10.579200
9.425770	720.847119	10.584218
9.550134	707.745009	10.589235
9.578430	690.107834	10.594253
9.076453	688.816472	10.599271
9.425146	682.209233	10.604288
9.299127	708.141786	10.609306
9.229003	713.435655	10.614323
9.788783	706.619257	10.619341
9.501090	706.966347	10.624359
9.283557	692.466808	10.629376
9.316097	689.432039	10.634394
9.081601	715.611506	10.639411
9.393350	707.619983	10.644429
9.240050	721.988192	10.649447
9.211810	711.940813	10.654464
8.926922	716.642979	10.659482
9.185274	717.537062	10.664499
9.139161	724.691040	10.669517
9.016776	734.281889	10.674535
9.751058	734.251775	10.679552
9.453976	740.219213	10.684570
9.663930	726.813354	10.689587
9.841914	715.638676	10.694605
9.446734	709.953558	10.699623
9.719275	712.294321	10.704640
9.457832	721.623573	10.709658
9.163011	713.013877	10.714675
9.406098	718.236699	10.719693
9.619959	733.643458	10.724711
9.783532	740.481369	10.729728
9.871714	733.125244	10.734746
9.678124	721.862501	10.739763
9.573263	717.648684	10.744781
9.579041	703.538495	10.749799
9.728216	719.126456	10.754816
9.173425	721.375464	10.759834
9.557532	736.952169	10.764851
9.797192	739.720109	10.769869
9.785480	756.570886	10.774887
9.802443	742.722032	10.779904
9.406575	740.947602	10.784922
9.741497	730.986120	10.789939
9.716911	748.223560	10.794957
9.953944	742.862871	10.799975
9.872972	740.374666	10.804992
9.913048	729.109512	10.810010
9.767972	728.467934	10.815027
9.935695	710.216117	10.820045
9.500052	722.498875	10.825063
9.692189	723.021719	10.830080
9.548017	720.692052	10.835098
9.432565	737.623518	10.840115
9.789400	751.184411	10.845133
9.764364	747.434533	10.850151
9.858041	751.828444	10.855168
9.486010	747.396341	10.860186
9.606373	751.508159	10.865203
9.913611	743.341818	10.870221
9.730859	755.809817	10.875239
9.771240	740.895462	10.880256
9.852866	744.429188	10.885274
9.766244	743.490918	10.890291
9.780641	736.397805	10.895309
9.701860	759.907330	10.900327
9.741167	747.256137	10.905344
9.688751	761.729530	10.910362
9.609734	749.268908	10.915379
9.691224	748.866388	10.920397
9.790057	770.940647	10.925415
10.271395	777.501316	10.930432
10.256981	779.644792	10.935450
9.943278	763.951257	10.940467
10.371443	758.345252	10.945485
9.818941	756.167684	10.950503
9.910867	766.083770	10.955520
9.983856	760.077723	10.960538
9.948829	756.170678	10.965555
10.181729	749.105703	10.970573
10.073172	754.953038	10.975591
10.031437	758.979078	10.980608
9.923212	754.444041	10.985626
9.614402	771.172030	10.990643
9.819429	765.867495	10.995661
10.233647	788.083800	11.000679
10.424619	785.911771	11.005696
10.417418	781.270094	11.010714
9.958763	773.926684	11.015731
9.856426	761.427594	11.020749
10.185095	791.215022	11.025767
10.318839	777.921687	11.030784
10.116065	778.980047	11.035802
10.124634	771.794598	11.040819
10.390588	773.282942	11.045837
9.963587	756.856169	11.050855
10.236325	769.095990	11.055872
10.128401	756.138401	11.060890
10.258360	787.139650	11.065907
10.420669	765.300915	11.070925
10.016724	773.530224	11.075943
9.962666	750.019741	11.080960
10.359202	769.710963	11.085978
10.272407	772.221131	11.090995
10.521629	767.831196	11.096013
10.361644	770.659679	11.101031
10.402154	756.504735	11.106048
10.366186	739.045206	11.111066
10.280016	755.267511	11.116083
10.558556	730.356677	11.121101
10.472963	740.923868	11.126119
10.324258	756.933241	11.131136
10.333080	759.243992	11.136154
10.256990	748.721552	11.141171
10.399298	754.956253	11.146189
9.916495	758.069419	11.151207
10.039228	761.459974	11.156224
10.297619	762.297572	11.161242
10.441014	787.599078	11.166259
10.656179	790.197105	11.171277
10.633093	769.471596	11.176295
10.185573	774.254874	11.181312
9.913731	755.044618	11.186330
10.186245	779.415069	11.191347
10.512712	771.433282	11.196365
10.188281	787.290082	11.201383
10.440728	786.299119	11.206400
10.396082	799.834204	11.211418
10.489021	794.830000	11.216435
10.586002	791.033477	11.221453
10.623620	796.555764	11.226471
10.583020	787.389285	11.231488
10.601727	787.788666	11.236506
10.449025	788.821926	11.241523
10.655556	784.107830	11.246541
10.429053	796.581025	11.251559
10.487974	795.639855	11.256576
10.599757	782.161218	11.261594
10.418064	786.012513	11.266611
10.159652	797.758595	11.271629
10.201036	793.753403	11.276647
10.166296	801.201228	11.281664
10.399513	783.777259	11.286682
10.525588	805.367270	11.291699
10.817045	794.025691	11.296717
10.684458	798.997714	11.301735
10.409160	805.418841	11.306752
10.758585	799.616145	11.311770
10.716571	812.987167	11.316787
10.707431	807.460008	11.321805
10.834284	801.420444	11.326823
10.634394	793.329521	11.331840
10.640597	787.178538	11.336858
10.716012	791.839288	11.341875
10.647483	801.726416	11.346893
10.773332	809.956355	11.351911
10.934375	819.989760	11.356928
11.096958	805.385082	11.361946
10.625878	803.799013	11.366963
10.253447	782.762220	11.371981
10.677071	809.848766	11.376999
10.972420	803.446993	11.382016
10.831657	815.070620	11.387034
10.881329	832.922494	11.392051
10.437021	831.243831	11.397069
10.759388	821.507339	11.402087
10.760836	819.694692	11.407104
10.859543	825.073071	11.412122
10.611887	826.257129	11.417139
10.927034	821.086306	11.422157
10.993911	824.024020	11.427175
10.987673	825.571915	11.432192
11.138585	819.089799	11.437210
10.784738	832.670404	11.442227
10.760657	814.726664	11.447245
10.800011	825.905287	11.452263
11.046254	819.975872	11.457280
11.003449	806.820716	11.462298
10.882936	822.179209	11.467315
10.887941	810.833986	11.472333
11.146943	820.307740	11.477351
11.197545	807.114908	11.482368
11.502179	823.930306	11.487386
11.258291	819.084980	11.492403
11.062134	811.071659	11.497421
11.216268	813.092035	11.502439
10.870251	810.667398	11.507456
11.306219	811.086186	11.512474
10.847856	815.724358	11.517491
11.033163	812.576546	11.522509
11.004993	825.366799	11.527527
10.807623	823.334613	11.532544
11.034143	816.058512	11.537562
10.968302	829.203133	11.542579
10.576078	815.848005	11.547597
11.020497	820.987013	11.552615
10.661747	800.890014	11.557632
10.853109	811.192839	11.562650
10.983666	822.805483	11.567667
11.115297	824.824561	11.572685
11.083054	838.366486	11.577703
11.123333	849.419414	11.582720
11.437582	853.896655	11.587738
11.103142	859.104761	11.592755
11.688535	846.312071	11.597773
11.187844	837.326885	11.602791
11.317402	824.959751	11.607808
11.347597	831.851922	11.612826
10.978970	825.444249	11.617843
11.183075	855.635459	11.622861
11.194019	844.853062	11.627879
11.228422	859.071512	11.632896
11.494086	851.759700	11.637914
11.413401	858.713799	11.642931
11.150643	858.242609	11.647949
11.395094	854.072674	11.652967
11.078355	857.634475	11.657984
11.250460	856.008330	11.663002
11.363178	842.389265	11.668019
11.170463	844.774367	11.673037
11.374518	850.824243	11.678055
11.043818	858.651336	11.683072
11.423688	853.884464	11.688090
11.558199	858.869142	11.693107
11.189118	837.853171	11.698125
11.473311	843.892753	11.703143
11.023277	856.943843	11.708160
11.087279	854.358352	11.713178
11.267964	862.037762	11.718195
11.387260	880.514931	11.723213
11.734321	877.342932	11.728231
11.567140	881.830372	11.733248
11.689691	877.530319	11.738266
11.549338	864.313694	11.743283
11.300838	857.533884	11.748301
11.599021	866.597161	11.753319
11.506055	870.170298	11.758336
11.548965	875.643130	11.763354
11.853487	881.157157	11.768371
11.543909	872.593204	11.773389
11.750489	873.224268	11.778407
11.777318	869.283748	11.783424
11.729786	858.829625	11.788442
11.921841	857.248890	11.793459
11.639167	857.315304	11.798477
11.696341	842.768847	11.803495
11.533293	861.389381	11.808512
11.542836	843.486890	11.813530
11.196306	847.255430	11.818547
11.496873	875.968613	11.823565
11.812285	879.003418	11.828583
11.542475	882.522734	11.833600
11.738056	881.654914	11.838618
11.457854	889.448192	11.843635
11.740664	880.059059	11.848653
11.921764	870.858154	11.853671
11.580117	885.072945	11.858688
11.933304	879.629644	11.863706
11.569506	890.121390	11.868723
11.585907	881.585232	11.873741
11.852528	869.637719	11.878759
11.558240	886.663653	11.883776
11.663439	880.613270	11.888794
11.797356	879.167699	11.893811
11.936493	888.616139	11.898829
12.075786	869.148571	11.903847
11.552465	875.967022	11.908864
12.205235	893.656616	11.913882
12.085923	876.919481	11.918899
11.818521	897.504644	11.923917
12.082467	883.236103	11.928935
11.813821	889.135727	11.933952
11.842897	884.976383	11.938970
11.864457	884.876111	11.943987
11.815916	897.938719	11.949005
11.898937	889.798826	11.954023
11.836371	880.453684	11.959040
11.681765	884.370096	11.964058
12.023159	910.179398	11.969075
11.717570	910.548908	11.974093
12.026636	912.365785	11.979111
11.847986	924.988322	11.984128
12.068149	917.467912	11.989146
12.054575	917.063780	11.994163
12.068826	912.423339	11.999181
12.262812	912.698013	12.004199
12.359203	908.521462	12.009216
12.251636	912.229543	12.014234
12.253361	917.963069	12.019251
12.542557	910.052634	12.024269
12.474887	903.023584	12.029287
12.001870	896.080616	12.034304
12.110118	881.267873	12.039322
12.284006	890.962377	12.044339
12.270351	902.790894	12.049357
12.299094	869.819916	12.054375
12.099097	883.556491	12.059392
12.206451	897.502652	12.064410
12.301050	899.865963	12.069427
12.392228	900.081662	12.074445
12.194673	896.096644	12.079463
12.285070	885.705119	12.084480
12.279979	898.898702	12.089498
12.426035	894.676235	12.094515
11.873081	898.910978	12.099533
12.348056	890.900256	12.104551
12.331753	908.653306	12.109568
12.264689	907.717009	12.114586
12.406307	914.999829	12.119603
12.214259	914.780369	12.124621
12.518184	912.596544	12.129639
12.340493	913.567620	12.134656
12.128067	915.224875	12.139674
12.374668	912.261845	12.144691
12.238302	905.431329	12.149709
11.979617	902.291732	12.154727
12.240442	908.685703	12.159744
12.045101	918.874379	12.164762
12.174174	904.055737	12.169779
12.241303	932.105295	12.174797
12.534900	931.230327	12.179815
12.149825	938.585957	12.184832
12.271830	951.685469	12.189850
12.450561	950.536249	12.194867
12.318598	958.704373	12.199885
12.590920	952.779159	12.204903
12.164777	944.922349	12.209920
12.391677	952.051191	12.214938
12.859909	944.699758	12.219955
12.881503	940.404958	12.224973
12.659417	946.819416	12.229991
12.757561	947.952632	12.235008
12.479372	941.221381	12.240026
12.646631	944.707939	12.245043
12.478579	949.239822	12.250061
12.455413	937.556924	12.255079
12.374994	959.085828	12.260096
12.627167	956.284229	12.265114
12.636660	951.204909	12.270131
12.534144	960.643834	12.275149
12.741351	945.667860	12.280167
12.985582	958.085533	12.285184
12.644271	954.580246	12.290202
13.059178	964.291251	12.295219
12.485300	965.489870	12.300237
12.671150	959.292008	12.305255
12.508835	978.393250	12.310272
12.892701	984.785516	12.315290
12.929567	989.856633	12.320307
13.064330	990.000088	12.325325
13.385964	985.841667	12.330343
13.171318	969.510739	12.335360
13.000360	959.005407	12.340378
13.109826	954.775786	12.345395
12.864773	952.648830	12.350413
13.046088	943.442533	12.355431
13.031446	951.031660	12.360448
12.816184	946.468499	12.365466
12.872197	946.747083	12.370483
12.714434	949.709547	12.375501
12.959520	951.273878	12.380519
12.734970	951.541657	12.385536
12.729557	943.553324	12.390554
13.121786	951.933856	12.395571
12.630348	944.220284	12.400589
13.037806	986.250085	12.405607
13.461530	977.822598	12.410624
13.048216	970.282374	12.415642
12.969540	961.126806	12.420659
12.891948	969.448312	12.425677
13.180129	967.856797	12.430695
13.205590	980.966287	12.435712
13.190695	987.663765	12.440730
13.217954	984.664251	12.445747
12.965170	970.669462	12.450765
13.163714	972.644439	12.455783
13.506828	980.874874	12.460800
13.120891	981.566077	12.465818
13.416548	955.582925	12.470835
12.834686	966.328029	12.475853
13.276372	967.332148	12.480871
13.157230	983.160045	12.485888
13.162825	977.613268	12.490906
13.517772	993.727205	12.495923
12.956763	986.579401	12.500941
13.475776	979.407112	12.505959
13.236643	987.111979	12.510976
13.393817	1007.154110	12.515994
13.178731	994.038187	12.521011
12.984094	996.466828	12.526029
13.299256	993.510557	12.531047
13.256541	990.096628	12.536064
13.263730	998.386623	12.541082
13.178665	989.032636	12.546099
12.972968	987.821975	12.551117
12.982894	987.184782	12.556135
13.217567	980.944500	12.561152
13.345662	989.598075	12.566170
13.020306	990.596511	12.571187
13.380524	1006.372273	12.576205
13.293642	1014.746901	12.581223
13.361192	1018.897728	12.586240
13.448623	1014.912715	12.591258
13.476490	1010.673439	12.596275
13.635258	1008.225964	12.601293
13.680279	1021.653633	12.606311
13.987433	1014.262268	12.611328
13.598688	1021.438568	12.616346
13.548529	1009.863791	12.621363
13.648727	1012.667228	12.626381
13.589204	1008.269602	12.631399
13.554212	1003.988563	12.636416
13.658635	1017.598295	12.641434
13.942394	1009.962630	12.646451
13.847658	1011.117494	12.651469
13.874722	987.382663	12.656487
13.679757	983.932297	12.661504
13.288122	991.026503	12.666522
13.587266	970.913348	12.671539
13.732510	995.329284	12.676557
13.614526	994.424816	12.681575
13.837908	992.227722	12.686592
13.586005	1011.632323	12.691610
13.930428	1009.911952	12.696627
13.728373	1014.337198	12.701645
13.809120	1009.964115	12.706663
14.036246	1005.917741	12.711680
13.496091	1005.092094	12.716698
13.600191	1004.214392	12.721715
14.001820	1017.475474	12.726733
13.630328	1017.629481	12.731751
13.756003	1020.709053	12.736768
13.462125	1018.626271	12.741786
13.299739	1023.813083	12.746803
13.647317	1021.455731	12.751821
13.505530	1026.660296	12.756839
13.789579	1022.091053	12.761856
13.747011	1028.969359	12.766874
14.203226	1028.358877	12.771891
13.715384	1045.465190	12.776909
13.564100	1039.565963	12.781927
14.382754	1053.536216	12.786944
14.023921	1054.585158	12.791962
14.246161	1057.305851	12.796979
13.920816	1056.692279	12.801997
13.827639	1068.869614	12.807015
13.777854	1051.312529	12.812032
13.527786	1073.353961	12.817050
13.873317	1044.142328	12.822067
13.850471	1064.798099	12.827085
13.906676	1050.127817	12.832103
14.152550	1060.060766	12.837120
13.884063	1052.647712	12.842138
14.011458	1052.483109	12.847155
13.968132	1062.742429	12.852173
13.862470	1056.551571	12.857191
14.116067	1055.738410	12.862208
14.133616	1071.275861	12.867226
14.087450	1086.473647	12.872243
14.500070	1084.360003	12.877261
14.138561	1093.287515	12.882279
14.346078	1091.227938	12.887296
14.180577	1083.606852	12.892314
14.512956	1085.160609	12.897331
14.572576	1078.699572	12.902349
14.339870	1077.620207	12.907367
14.081209	1062.966621	12.912384
14.183011	1083.097413	12.917402
14.628671	1079.360096	12.922419
14.549967	1078.212082	12.927437
14.643058	1077.444536	12.932455
14.124668	1062.120955	12.937472
14.248489	1069.603814	12.942490
14.408225	1080.986099	12.947507
14.425620	1083.690662	12.952525
14.478366	1076.492357	12.957543
14.470483	1071.609031	12.962560
14.379485	1084.308234	12.967578
14.797321	1079.071941	12.972595
14.532165	1080.632245	12.977613
14.361940	1082.397871	12.982631
14.871063	1075.557800	12.987648
14.419670	1077.588343	12.992666
14.690002	1070.221339	12.997683
14.640937	1070.374215	13.002701
14.537916	1066.555375	13.007719
14.496021	1061.898386	13.012736
14.360081	1057.924398	13.017754
14.338519	1066.756354	13.022771
14.505692	1085.035550	13.027789
14.358661	1084.162543	13.032807
15.011683	1064.519790	13.037824
14.626516	1077.743078	13.042842
14.737786	1075.561450	13.047859
14.827149	1076.618489	13.052877
14.732908	1066.506509	13.057895
14.873923	1076.936702	13.062912
14.567520	1073.115359	13.067930
14.333885	1077.585399	13.072947
14.804621	1077.920516	13.077965
14.643180	1080.397608	13.082983
14.563168	1071.352798	13.088000
14.278132	1081.684843	13.093018
14.664276	1078.894440	13.098035
14.790301	1081.125156	13.103053
14.856500	1086.366907	13.108071
15.246356	1083.054952	13.113088
14.844367	1082.885929	13.118106
15.080155	1075.598236	13.123123
15.315898	1071.882328	13.128141
14.590039	1076.131818	13.133159
15.092315	1075.523464	13.138176
15.109309	1081.387075	13.143194
14.824272	1088.530720	13.148211
14.845878	1066.372766	13.153229
14.908889	1091.741491	13.158247
14.681485	1072.430502	13.163264
14.639292	1093.082030	13.168282
15.111508	1100.098076	13.173299
15.293524	1096.524867	13.178317
15.194555	1106.643349	13.183335
15.378803	1088.215854	13.188352
14.809012	1088.629941	13.193370
14.750897	1089.747565	13.198387
15.090386	1105.385648	13.203405
14.902830	1119.070586	13.208423
15.096534	1110.535209	13.213440
15.042136	1119.086371	13.218458
15.109862	1115.641273	13.223475
15.262640	1118.447356	13.228493
14.989069	1110.768051	13.233511
15.261880	1110.162390	13.238528
14.995646	1113.674279	13.243546
15.171421	1109.678086	13.248563
15.186167	1120.859022	13.253581
15.069979	1103.529138	13.258599
15.184315	1104.988254	13.263616
14.996160	1110.018861	13.268634
14.983931	1105.028295	13.273651
15.374871	1115.687816	13.278669
15.259552	1133.368928	13.283687
15.467576	1129.587919	13.288704
15.263724	1142.149756	13.293722
15.572596	1133.752776	13.298739
15.737098	1141.103386	13.303757
15.472466	1122.108552	13.308775
15.721320	1114.145219	13.313792
15.201391	1102.423749	13.318810
15.417909	1111.586278	13.323827
15.409513	1098.556747	13.328845
15.357963	1106.615916	13.333863
15.488147	1120.073682	13.338880
15.664741	1127.904160	13.343898
15.630544	1136.440481	13.348915
15.245546	1119.131288	13.353933
15.549448	1135.791479	13.358951
15.721431	1134.036615	13.363968
15.775609	1132.955297	13.368986
15.749626	1136.056413	13.374003
15.699073	1126.034493	13.379021
15.412653	1133.361611	13.384039
16.017521	1130.596750	13.389056
15.994631	1122.638765	13.394074
15.500422	1117.517760	13.399091
16.012625	1115.895014	13.404109
15.744138	1103.378527	13.409127
15.880345	1102.931039	13.414144
15.905609	1108.691153	13.419162
15.628654	1101.676033	13.424179
15.595033	1113.164491	13.429197
15.278904	1103.680943	13.434215
15.565057	1110.268305	13.439232
15.377325	1140.789041	13.444250
15.695629	1126.068286	13.449267
16.007896	1137.703391	13.454285
16.020352	1138.968275	13.459303
16.044279	1135.282732	13.464320
15.914500	1142.368566	13.469338
15.917642	1141.493962	13.474355
16.270289	1128.276817	13.479373
15.862725	1149.618280	13.484391
15.957773	1138.556289	13.489408
15.702135	1140.670110	13.494426
15.944701	1143.508100	13.499443
16.086051	1133.674389	13.504461
16.028803	1136.982987	13.509479
15.911013	1137.057576	13.514496
15.945240	1132.423116	13.519514
16.091024	1140.409346	13.524531
16.414876	1124.933425	13.529549
16.114849	1138.853452	13.534567
16.112272	1131.028588	13.539584
16.363091	1139.846372	13.544602
15.859904	1136.217338	13.549619
15.908823	1124.619704	13.554637
15.642694	1144.541661	13.559655
15.882599	1119.543297	13.564672
16.144090	1134.818111	13.569690
15.934534	1132.438177	13.574707
16.127003	1134.062293	13.579725
15.760648	1143.636053	13.584743
16.231810	1151.933981	13.589760
16.152331	1178.728724	13.594778
16.198819	1166.672119	13.599795
16.563488	1169.339872	13.604813
16.722111	1167.114193	13.609831
16.740021	1164.897797	13.614848
16.543076	1150.420596	13.619866
16.349081	1141.990504	13.624883
16.639104	1138.892627	13.629901
16.007362	1120.991289	13.634919
16.432946	1136.524449	13.639936
16.395288	1129.909724	13.644954
15.999870	1131.572840	13.649971
16.425586	1151.367679	13.654989
16.275098	1164.335971	13.660007
16.433224	1169.875772	13.665024
16.372498	1166.661782	13.670042
16.400498	1184.210729	13.675059
16.459300	1158.277202	13.680077
16.510198	1174.912235	13.685095
16.561401	1174.831859	13.690112
16.859586	1161.279378	13.695130
16.598914	1178.030358	13.700147
16.738292	1161.942616	13.705165
16.757894	1172.139554	13.710183
16.571719	1170.982627	13.715200
16.965993	1185.518885	13.720218
16.608060	1175.955706	13.725235
16.931872	1180.297734	13.730253
16.805632	1171.503559	13.735271
16.825043	1179.441123	13.740288
17.164373	1162.184382	13.745306
16.913445	1179.466994	13.750323
16.669867	1156.931966	13.755341
16.857397	1160.305506	13.760359
16.679061	1176.587571	13.765376
16.458268	1158.728091	13.770394
16.093767	1169.953042	13.775411
16.710477	1165.503149	13.780429
16.746846	1174.833840	13.785447
16.847531	1168.933956	13.790464
16.947074	1162.533594	13.795482
16.855018	1169.186535	13.800499
16.815794	1156.657603	13.805517
16.904179	1175.130888	13.810535
16.692891	1165.177129	13.815552
16.653188	1170.583226	13.820570
16.898623	1167.164147	13.825587
17.207083	1170.548897	13.830605
16.795445	1181.488408	13.835623
16.663125	1181.906953	13.840640
17.253459	1188.104887	13.845658
17.135974	1188.990359	13.850675
17.218444	1191.887879	13.855693
17.157702	1193.160239	13.860711
17.122258	1185.738718	13.865728
17.260394	1185.238165	13.870746
17.080894	1195.954327	13.875763
17.187291	1187.136850	13.880781
16.798578	1186.923712	13.885799
17.053574	1193.237584	13.890816
17.448054	1185.156666	13.895834
17.078180	1193.365512	13.900851
17.170583	1184.718617	13.905869
17.063957	1193.051831	13.910887
16.956709	1177.470371	13.915904
16.838890	1190.014388	13.920922
16.673523	1181.230117	13.925939
17.233709	1191.998206	13.930957
17.339189	1213.568874	13.935975
17.294195	1218.706535	13.940992
17.519631	1217.227703	13.946010
17.437811	1232.590938	13.951027
17.391385	1222.369893	13.956045
17.624053	1221.086965	13.961063
17.613780	1221.098817	13.966080
17.629255	1207.912233	13.971098
17.487014	1212.526817	13.976115
17.440856	1210.184124	13.981133
17.398203	1215.598793	13.986151
17.667487	1219.386491	13.991168
17.815653	1200.502629	13.996186
17.544669	1216.303707	14.001203
17.899892	1197.595423	14.006221
17.644223	1201.346377	14.011239
17.323576	1196.791700	14.016256
17.712560	1190.345165	14.021274
17.304039	1205.802414	14.026291
17.574142	1210.898725	14.031309
17.766855	1217.573803	14.036327
17.487793	1213.747315	14.041344
17.837451	1209.205453	14.046362
18.090883	1214.387473	14.051379
17.831799	1212.794861	14.056397
17.810653	1226.412738	14.061415
17.624249	1221.138097	14.066432
17.615956	1212.732972	14.071450
17.713811	1220.045827	14.076467
17.561183	1204.067110	14.081485
17.604976	1215.853311	14.086503
17.709043	1228.093036	14.091520
18.160560	1210.395455	14.096538
17.963311	1215.816584	14.101555
18.148685	1221.819804	14.106573
18.045693	1220.503589	14.111591
18.006516	1225.431383	14.116608
18.228523	1223.095048	14.121626
17.838528	1219.083789	14.126643
17.923424	1219.580879	14.131661
17.681734	1206.931563	14.136679
17.870356	1217.254697	14.141696
18.277583	1206.752636	14.146714
17.843187	1215.841639	14.151731
17.867746	1199.724714	14.156749
17.783163	1209.395123	14.161767
17.837487	1215.104127	14.166784
18.213383	1210.961968	14.171802
17.959017	1240.144916	14.176819
18.197422	1231.126900	14.181837
18.195841	1245.056742	14.186855
18.213066	1243.558983	14.191872
18.365671	1245.356590	14.196890
18.134320	1243.171633	14.201907
18.251858	1244.243708	14.206925
18.098083	1243.706376	14.211943
18.033195	1247.117516	14.216960
18.678985	1235.902347	14.221978
18.402322	1232.582034	14.226995
18.287694	1245.389976	14.232013
18.273578	1229.871891	14.237031
18.107068	1258.190945	14.242048
18.312916	1239.547543	14.247066
18.237162	1245.718701	14.252083
18.185912	1236.113558	14.257101
18.409809	1239.519285	14.262119
18.064077	1246.200209	14.267136
18.503030	1252.639279	14.272154
18.537843	1247.757107	14.277171
18.088536	1258.403556	14.282189
18.264633	1259.025111	14.287207
18.605707	1266.535928	14.292224
19.264825	1270.185511	14.297242
18.777432	1258.546417	14.302259
18.734563	1241.661340	14.307277
18.605077	1240.332183	14.312295
18.398104	1256.343834	14.317312
18.677398	1242.098500	14.322330
18.633458	1254.879122	14.327347
18.740543	1282.306546	14.332365
18.919911	1260.125389	14.337383
18.864875	1256.894104	14.342400
19.095347	1241.414998	14.347418
18.583726	1242.586128	14.352435
18.556023	1239.369223	14.357453
18.905971	1250.964829	14.362471
18.695717	1261.428303	14.367488
18.960790	1264.589589	14.372506
18.863000	1279.609526	14.377523
18.569004	1269.088988	14.382541
19.099196	1280.376940	14.387559
18.779769	1275.882260	14.392576
18.911678	1267.926957	14.397594
18.743374	1273.150551	14.402611
18.938477	1253.260375	14.407629
19.217176	1278.160693	14.412647
19.038745	1272.912959	14.417664
18.802896	1270.532625	14.422682
18.869898	1269.141866	14.427699
18.861459	1276.253762	14.432717
18.933631	1267.667827	14.437735
18.910020	1282.152891	14.442752
19.151651	1270.480691	14.447770
19.324626	1274.557977	14.452787
19.339250	1277.637749	14.457805
19.464493	1273.092512	14.462823
18.936101	1276.726583	14.467840
18.981599	1268.082669	14.472858
19.209814	1270.363636	14.477875
19.199016	1260.655063	14.482893
19.330699	1263.560700	14.487911
19.123176	1271.479726	14.492928
19.453452	1262.848384	14.497946
19.382604	1274.015238	14.502963
19.325267	1268.213953	14.507981
19.345199	1279.824168	14.512999
19.312484	1271.453552	14.518016
19.273031	1266.283124	14.523034
19.351748	1264.670402	14.528051
19.229810	1271.980834	14.533069
19.551835	1278.082332	14.538087
19.660357	1264.454140	14.543104
19.340357	1272.935626	14.548122
19.162695	1283.413509	14.553139
19.603016	1301.806546	14.558157
20.331551	1290.152267	14.563175
19.625290	1287.940596	14.568192
19.807569	1270.591801	14.573210
19.372752	1269.796553	14.578227
19.332065	1266.813329	14.583245
19.755826	1261.220270	14.588263
19.495890	1263.146279	14.593280
19.649247	1267.948392	14.598298
19.715397	1264.662539	14.603315
19.627294	1293.048307	14.608333
20.082288	1277.738607	14.613351
19.498917	1290.100647	14.618368
19.982787	1278.205084	14.623386
19.816798	1280.555134	14.628403
19.332899	1296.445406	14.633421
19.950984	1288.017021	14.638439
20.185149	1297.856118	14.643456
19.876879	1293.344337	14.648474
19.907982	1286.115463	14.653491
20.158375	1300.366526	14.658509
20.117494	1286.842317	14.663527
19.829430	1271.473082	14.668544
19.675078	1267.983074	14.673562
19.989374	1276.874286	14.678579
19.858655	1294.939932	14.683597
19.862685	1283.478011	14.688615
19.637807	1291.561002	14.693632
19.952771	1295.614434	14.698650
19.902682	1291.260729	14.703667
19.828186	1294.250040	14.708685
20.014413	1282.074308	14.713703
19.873732	1305.036659	14.718720
19.537151	1294.979632	14.723738
20.143340	1301.071571	14.728755
19.989505	1316.238177	14.733773
20.362514	1321.895440	14.738791
20.499128	1325.934664	14.743808
20.756113	1316.497380	14.748826
20.651697	1298.533484	14.753843
20.389892	1290.542274	14.758861
20.586202	1282.846829	14.763879
20.441323	1281.893552	14.768896
20.333721	1279.912301	14.773914
20.700736	1285.092303	14.778931
20.566770	1291.504937	14.783949
20.746598	1282.970774	14.788967
20.442391	1291.740736	14.793984
20.592114	1289.621114	14.799002
20.858504	1291.428656	14.804019
20.334430	1298.711091	14.809037
20.361178	1289.158168	14.814055
20.430502	1287.437178	14.819072
20.507397	1283.168272	14.824090
20.472451	1285.190339	14.829107
20.285345	1301.052429	14.834125
20.644582	1281.687819	14.839143
20.718960	1283.143814	14.844160
20.533363	1291.302183	14.849178
20.848599	1274.231245	14.854195
20.514324	1278.207659	14.859213
20.541141	1280.341144	14.864231
20.523210	1286.538680	14.869248
20.483428	1289.831632	14.874266
20.957548	1278.371341	14.879283
20.374933	1290.856949	14.884301
20.624364	1279.480432	14.889319
20.400674	1302.968783	14.894336
20.561875	1317.558052	14.899354
20.842795	1316.152208	14.904371
20.593783	1317.458644	14.909389
20.868011	1317.268987	14.914407
20.764382	1315.957887	14.919424
20.827500	1336.387956	14.924442
21.044948	1319.612396	14.929459
20.596686	1333.129535	14.934477
20.777826	1328.661048	14.939495
21.003130	1316.235677	14.944512
20.639392	1310.356892	14.949530
21.070136	1327.650808	14.954547
20.782148	1326.185177	14.959565
21.374957	1349.049994	14.964583
21.328434	1350.447843	14.969600
21.264016	1332.111533	14.974618
21.101179	1334.783242	14.979635
21.065678	1352.304007	14.984653
21.418257	1344.305309	14.989671
21.653685	1346.178689	14.994688
21.209378	1330.436584	14.999706
21.712899	1313.629794	15.004723
21.070917	1329.380317	15.009741
21.251109	1321.251591	15.014759
21.163638	1316.491550	15.019776
21.020131	1316.646653	15.024794
21.620137	1329.244361	15.029811
21.496936	1350.577485	15.034829
21.344544	1330.094388	15.039847
21.592079	1334.019537	15.044864
21.651814	1328.025201	15.049882
21.656255	1307.336728	15.054899
20.980499	1317.534531	15.059917
21.219201	1325.600855	15.064935
21.914857	1336.685264	15.069952
21.318830	1343.994864	15.074970
21.670873	1340.312909	15.079987
21.316444	1347.414806	15.085005
21.344716	1333.640500	15.090023
21.579693	1339.384347	15.095040
21.400686	1341.062299	15.100058
21.710994	1344.208450	15.105075
21.783159	1346.469066	15.110093
21.846228	1355.820351	15.115111
21.932736	1331.249659	15.120128
21.791056	1352.218304	15.125146
22.196855	1347.398975	15.130163
21.720837	1346.557787	15.135181
21.828178	1340.137759	15.140199
21.877264	1346.134916	15.145216
21.762942	1347.959821	15.150234
22.023225	1335.121560	15.155251
21.681292	1349.102627	15.160269
21.882611	1344.018241	15.165287
22.072722	1348.907002	15.170304
21.814787	1348.113416	15.175322
22.026999	1339.592763	15.180339
21.836565	1356.033479	15.185357
22.193188	1343.500576	15.190375
22.355651	1343.432909	15.195392
22.061439	1346.297356	15.200410
22.240118	1339.824702	15.205427
21.895543	1356.532570	15.210445
22.038144	1337.800606	15.215463
22.143458	1354.847121	15.220480
22.258848	1339.101566	15.225498
22.005033	1349.593555	15.230515
21.946567	1350.919673	15.235533
22.012573	1335.743772	15.240551
21.901597	1344.927302	15.245568
22.131325	1351.614428	15.250586
22.364067	1380.504592	15.255603
22.170573	1378.635532	15.260621
22.557047	1376.327789	15.265639
22.806789	1373.725882	15.270656
22.044237	1372.016796	15.275674
22.573605	1357.481264	15.280691
22.397184	1377.547128	15.285709
22.591182	1366.029249	15.290727
22.490231	1374.681927	15.295744
22.680469	1366.948870	15.300762
22.476698	1365.034769	15.305779
22.643403	1372.562941	15.310797
22.408830	1367.284107	15.315815
22.854777	1370.473876	15.320832
22.440085	1373.911365	15.325850
22.593165	1375.312836	15.330867
22.602785	1388.524581	15.335885
22.817414	1383.352666	15.340903
22.565648	1385.004172	15.345920
22.340969	1377.801486	15.350938
23.047548	1373.616739	15.355955
22.665350	1380.403234	15.360973
22.766341	1380.099815	15.365991
22.778381	1375.304712	15.371008
22.488120	1377.279536	15.376026
22.296570	1381.389048	15.381043
22.332386	1383.272296	15.386061
22.425828	1389.626429	15.391079
23.020579	1381.512903	15.396096
22.652651	1410.020607	15.401114
22.819274	1393.451354	15.406131
22.972944	1409.257435	15.411149
22.955008	1415.780838	15.416167
22.978011	1397.879313	15.421184
23.129923	1412.205600	15.426202
22.995855	1400.923860	15.431219
23.167211	1413.196107	15.436237
23.207686	1399.098536	15.441255
23.556541	1409.176076	15.446272
23.006320	1406.667595	15.451290
23.327854	1405.876450	15.456307
23.059590	1400.016490	15.461325
22.967308	1409.874183	15.466343
23.463491	1397.182278	15.471360
23.220899	1404.371897	15.476378
23.373887	1387.747534	15.481395
23.381926	1395.388927	15.486413
23.454085	1388.098804	15.491431
23.616587	1394.666083	15.496448
23.213280	1390.092535	15.501466
23.466284	1396.571253	15.506483
23.556469	1395.751722	15.511501
23.356822	1401.928658	15.516519
23.691370	1395.122808	15.521536
23.208264	1391.948953	15.526554
23.266945	1387.870290	15.531571
23.399915	1398.709030	15.536589
23.569374	1397.923533	15.541607
23.358560	1396.798508	15.546624
23.257103	1399.843564	15.551642
23.233883	1396.845620	15.556659
23.428420	1410.645193	15.561677
23.856698	1409.377846	15.566695
23.900866	1411.674489	15.571712
24.151774	1396.790242	15.576730
23.854635	1388.149944	15.581747
23.706726	1395.926042	15.586765
23.945266	1381.298129	15.591783
23.863765	1382.151391	15.596800
23.738868	1395.216217	15.601818
23.904014	1378.019115	15.606835
23.865032	1380.417762	15.611853
23.831173	1393.538491	15.616871
24.000511	1375.407637	15.621888
23.893098	1383.653014	15.626906
23.832482	1383.456009	15.631923
24.189302	1392.940326	15.636941
24.120472	1397.220365	15.641959
24.233163	1375.048880	15.646976
23.652003	1381.489993	15.651994
24.134261	1402.009706	15.657011
24.421625	1410.288358	15.662029
24.253885	1407.319806	15.667047
24.286025	1392.784443	15.672064
24.019505	1377.586403	15.677082
24.106305	1386.676854	15.682099
24.256364	1403.493244	15.687117
23.930189	1402.197168	15.692135
24.254913	1405.178486	15.697152
24.021270	1421.114320	15.702170
24.250299	1405.599763	15.707187
24.540746	1422.274299	15.712205
24.181302	1398.724430	15.717223
24.516900	1399.252816	15.722240
24.390641	1403.544808	15.727258
24.091551	1398.815187	15.732275
24.483014	1405.526778	15.737293
24.506385	1398.861309	15.742311
25.098583	1392.395081	15.747328
24.808520	1391.833327	15.752346
25.113170	1396.232018	15.757363
24.487845	1407.122769	15.762381
24.313250	1406.889789	15.767399
24.789770	1392.445322	15.772416
24.388336	1401.602789	15.777434
24.614902	1400.337880	15.782451
24.604277	1400.883038	15.787469
24.829092	1403.227270	15.792487
24.818288	1402.131579	15.797504
24.528378	1400.700798	15.802522
24.601778	1398.542899	15.807539
24.719770	1386.504711	15.812557
24.189843	1411.243669	15.817575
24.981380	1409.010092	15.822592
24.651206	1421.419448	15.827610
24.936658	1421.443045	15.832627
25.074115	1448.750026	15.837645
24.873153	1441.619752	15.842663
25.132317	1434.944624	15.847680
25.293534	1445.372124	15.852698
25.152386	1430.792642	15.857715
25.236197	1416.048860	15.862733
24.880840	1406.699924	15.867751
24.673606	1422.456729	15.872768
24.820990	1431.855235	15.877786
24.757916	1434.107315	15.882803
24.903019	1442.498846	15.887821
24.771529	1449.936406	15.892839
24.938757	1442.652391	15.897856
24.967220	1441.973935	15.902874
25.189113	1461.495151	15.907891
25.221416	1463.285408	15.912909
25.168355	1481.278019	15.917927
25.475678	1467.605575	15.922944
25.788042	1478.163695	15.927962
25.375441	1468.542746	15.932979
25.767332	1475.567616	15.937997
25.461152	1459.587045	15.943015
25.555815	1440.191960	15.948032
25.357742	1437.924917	15.953050
25.283822	1447.368469	15.958067
25.599335	1448.693114	15.963085
25.484945	1463.683698	15.968103
25.603055	1467.082948	15.973120
25.676778	1468.260881	15.978138
25.880400	1471.167560	15.983155
26.048310	1462.214491	15.988173
25.531157	1472.692516	15.993191
25.866218	1447.268631	15.998208
25.568971	1461.733352	16.003226
25.467686	1460.690692	16.008243
25.753862	1460.257280	16.013261
25.465243	1464.516980	16.018279
25.631782	1457.321241	16.023296
25.710579	1464.833875	16.028314
25.941271	1453.178105	16.033331
25.905648	1455.266729	16.038349
25.906220	1457.967545	16.043367
25.965896	1469.273860	16.048384
25.530614	1456.413173	16.053402
25.879934	1461.011936	16.058419
26.215564	1464.365989	16.063437
25.732197	1478.785418	16.068455
26.254096	1480.363790	16.073472
26.440668	1491.576923	16.078490
26.460909	1477.543339	16.083507
26.845077	1467.588889	16.088525
26.339161	1466.454963	16.093543
26.515774	1453.877719	16.098560
26.405176	1448.460481	16.103578
26.304286	1455.425568	16.108595
26.632599	1445.007927	16.113613
26.469479	1454.475769	16.118631
26.409656	1446.383198	16.123648
26.370927	1449.991690	16.128666
26.543866	1462.419488	16.133683
26.361850	1465.779970	16.138701
26.054747	1462.033037	16.143719
26.492833	1447.826709	16.148736
26.526127	1458.314031	16.153754
26.257695	1461.304920	16.158771
26.466729	1453.463224	16.163789
26.462026	1467.343894	16.168807
26.364951	1457.691275	16.173824
26.615571	1463.008659	16.178842
26.458781	1463.841403	16.183859
26.595709	1475.698811	16.188877
26.883645	1493.953323	16.193895
26.921627	1485.864347	16.198912
26.971230	1496.498968	16.203930
26.783856	1471.008657	16.208947
26.796575	1456.898793	16.213965
26.867531	1470.873534	16.218983
26.865102	1467.605171	16.224000
26.990983	1469.749372	16.229018
26.682550	1483.949386	16.234035
27.119983	1470.097893	16.239053
26.974137	1480.799343	16.244071
26.969736	1489.122122	16.249088
27.172551	1484.650402	16.254106
26.705133	1499.440166	16.259123
27.093058	1480.607950	16.264141
26.935769	1492.076292	16.269159
26.938883	1480.726753	16.274176
27.231399	1481.844322	16.279194
26.789287	1485.381621	16.284211
26.862431	1485.843072	16.289229
26.757837	1494.275601	16.294247
26.734226	1490.911935	16.299264
26.556102	1503.992144	16.304282
26.979457	1519.436123	16.309299
27.122753	1511.767136	16.314317
26.948234	1528.943636	16.319335
27.238665	1520.153318	16.324352
27.314575	1521.842399	16.329370
27.167175	1525.018963	16.334387
27.896398	1525.117814	16.339405
27.752428	1529.471318	16.344423
27.520978	1515.944451	16.349440
27.948426	1517.224527	16.354458
27.652318	1507.967093	16.359475
27.704576	1514.580984	16.364493
27.638395	1513.570700	16.369511
27.555049	1511.162370	16.374528
27.790448	1515.323085	16.379546
27.272774	1517.659062	16.384563
27.624354	1515.971305	16.389581
27.970825	1529.355900	16.394599
28.080497	1544.586543	16.399616
28.253515	1523.117323	16.404634
27.735882	1504.673951	16.409651
28.088999	1505.120723	16.414669
28.039583	1502.930656	16.419687
27.869500	1505.418002	16.424704
27.914478	1503.302671	16.429722
27.537268	1507.932951	16.434739
28.090152	1523.442615	16.439757
27.916801	1535.662993	16.444775
28.128928	1537.478253	16.449792
28.115182	1534.784656	16.454810
28.339445	1540.203548	16.459827
28.806857	1530.333411	16.464845
28.629243	1515.227704	16.469863
28.287950	1515.790808	16.474880
28.300884	1514.422247	16.479898
28.395188	1496.848121	16.484915
28.193552	1513.678077	16.489933
28.209461	1509.394586	16.494951
27.940742	1488.278573	16.499968
28.235609	1497.946385	16.504986
28.236578	1500.045303	16.510003
28.357646	1523.505652	16.515021
28.344250	1535.260024	16.520039
28.378372	1529.834289	16.525056
28.583432	1525.785718	16.530074
28.673220	1529.713863	16.535091
28.921032	1518.894307	16.540109
28.902054	1534.007155	16.545127
28.330815	1509.459166	16.550144
28.708782	1527.710058	16.555162
28.269146	1523.027636	16.560179
28.625415	1527.305162	16.565197
28.576216	1532.753695	16.570215
28.409178	1519.789877	16.575232
28.566724	1531.323910	16.580250
28.355783	1524.646923	16.585267
28.557579	1525.545482	16.590285
28.578717	1540.747651	16.595303
28.255757	1525.962347	16.600320
28.714139	1546.026848	16.605338
28.710614	1568.640323	16.610355
29.010251	1552.279282	16.615373
29.119538	1559.808376	16.620391
29.205746	1568.205281	16.625408
29.300567	1561.639524	16.630426
29.167595	1571.317371	16.635443
29.285531	1574.984827	16.640461
29.111717	1569.100140	16.645479
29.102002	1574.002708	16.650496
29.072913	1562.684606	16.655514
29.175893	1565.747966	16.660531
29.406473	1573.708108	16.665549
29.502329	1556.968817	16.670567
29.453253	1567.011655	16.675584
29.531189	1554.160146	16.680602
29.153047	1570.714477	16.685619
29.530384	1558.372424	16.690637
29.456297	1553.086783	16.695655
29.469229	1581.359951	16.700672
29.276527	1560.750360	16.705690
29.378913	1563.756151	16.710707
29.270257	1561.131176	16.715725
29.288009	1573.814682	16.720743
29.347186	1569.627447	16.725760
29.559184	1559.530266	16.730778
29.539733	1590.019263	16.735795
29.620069	1577.037838	16.740813
29.781356	1586.410033	16.745831
29.684183	1592.838361	16.750848
29.893474	1585.251129	16.755866
30.085309	1584.671823	16.760883
29.838464	1582.992717	16.765901
29.790327	1596.074353	16.770919
29.650227	1582.132217	16.775936
30.038468	1581.314295	16.780954
29.936517	1592.750934	16.785971
29.921354	1582.004708	16.790989
29.791154	1586.208247	16.796007
29.793289	1592.913803	16.801024
30.092135	1577.436640	16.806042
30.263433	1585.664504	16.811059
30.179979	1588.197771	16.816077
30.125340	1566.831354	16.821095
29.878656	1592.954600	16.826112
30.401053	1574.036675	16.831130
30.030866	1583.953001	16.836147
30.382797	1578.873956	16.841165
30.385597	1585.529902	16.846183
30.122033	1577.950655	16.851200
29.993395	1577.873626	16.856218
30.060381	1587.985861	16.861235
30.403788	1602.197036	16.866253
30.414016	1614.488692	16.871271
30.382915	1605.262881	16.876288
30.760076	1614.543426	16.881306
30.407421	1619.567138	16.886323
30.572837	1618.862106	16.891341
30.865140	1605.650785	16.896359
30.725918	1608.223580	16.901376
30.717676	1602.925957	16.906394
30.955979	1603.650018	16.911411
31.109985	1602.384587	16.916429
31.215205	1584.207893	16.921447
30.717092	1588.441728	16.926464
30.794351	1577.891999	16.931482
30.505216	1573.360637	16.936499
30.861605	1579.056858	16.941517
31.018132	1573.335051	16.946535
30.653521	1585.636672	16.951552
30.660031	1587.308692	16.956570
30.942888	1601.158592	16.961587
31.084716	1606.871879	16.966605
31.002087	1603.373287	16.971623
30.651107	1608.726966	16.976640
31.014637	1596.910973	16.981658
30.759231	1609.476791	16.986675
30.997160	1605.986135	16.991693
31.429931	1603.995248	16.996711
30.899825	1613.039781	17.001728
31.339040	1603.833964	17.006746
31.315912	1607.385988	17.011763
31.288002	1604.161070	17.016781
31.573222	1602.639849	17.021799
31.152658	1607.294150	17.026816
31.252318	1595.949236	17.031834
31.271988	1608.594371	17.036851
31.455725	1625.067320	17.041869
31.889432	1621.340904	17.046887
31.481318	1634.857970	17.051904
31.504208	1633.382263	17.056922
31.782724	1626.084099	17.061939
31.670382	1631.273670	17.066957
31.732287	1622.951778	17.071975
31.471239	1646.932457	17.076992
31.622407	1629.252345	17.082010
31.677265	1630.015482	17.087027
31.719202	1624.540204	17.092045
31.829215	1633.202939	17.097063
31.702257	1627.074018	17.102080
31.938871	1627.171422	17.107098
31.798663	1633.468423	17.112115
31.927919	1636.877973	17.117133
32.047085	1635.497356	17.122151
32.004616	1634.572104	17.127168
32.303424	1632.543226	17.132186
31.927984	1638.301859	17.137203
31.862748	1639.045383	17.142221
32.285700	1631.217939	17.147239
32.091736	1637.374348	17.152256
32.161999	1627.545869	17.157274
31.884425	1623.341451	17.162291
31.917047	1630.067079	17.167309
32.433152	1637.583694	17.172327
32.062421	1671.265205	17.177344
32.508181	1656.608591	17.182362
32.737545	1649.844909	17.187379
32.332639	1641.607532	17.192397
32.368436	1642.886412	17.197415
32.549178	1655.612229	17.202432
32.560067	1651.924092	17.207450
32.541037	1648.311850	17.212467
32.483393	1649.980604	17.217485
32.635681	1635.705315	17.222503
32.594731	1651.919028	17.227520
32.803184	1654.210699	17.232538
32.908587	1650.099841	17.237555
32.608301	1645.248023	17.242573
32.790558	1650.261481	17.247591
32.578934	1645.248977	17.252608
32.635304	1651.370025	17.257626
32.996268	1650.459580	17.262643
32.538901	1639.799578	17.267661
33.044697	1651.465088	17.272679
32.824570	1646.268300	17.277696
32.705473	1657.865957	17.282714
32.768849	1653.053330	17.287731
32.567563	1652.137691	17.292749
32.966176	1646.449950	17.297767
33.056606	1651.958898	17.302784
32.973383	1649.359620	17.307802
33.335369	1669.211126	17.312819
32.865411	1675.715167	17.317837
33.313446	1677.055130	17.322855
33.005196	1678.851406	17.327872
33.196042	1666.070496	17.332890
33.102189	1686.907212	17.337907
33.534894	1678.967427	17.342925
33.532253	1678.888272	17.347943
33.518936	1678.092621	17.352960
33.333926	1682.791169	17.357978
33.829136	1680.221860	17.362995
33.471765	1687.601607	17.368013
33.386357	1666.320927	17.373031
33.480178	1680.077065	17.378048
33.426020	1673.596302	17.383066
33.740751	1662.425498	17.388083
33.507817	1664.520877	17.393101
33.671319	1671.499444	17.398119
33.577302	1671.548162	17.403136
33.559655	1680.182227	17.408154
33.737529	1681.957801	17.413171
33.862633	1697.397618	17.418189
33.970044	1701.081604	17.423207
33.886883	1709.222184	17.428224
34.024800	1710.029854	17.433242
33.844547	1708.475234	17.438259
34.005231	1708.888374	17.443277
34.082594	1712.205552	17.448295
34.236176	1703.619796	17.453312
34.291267	1704.986320	17.458330
34.493882	1702.742077	17.463347
34.045300	1706.811196	17.468365
34.234539	1701.567107	17.473383
34.114623	1704.524740	17.478400
34.361575	1704.899415	17.483418
34.566071	1692.793257	17.488435
34.271025	1708.044105	17.493453
34.507623	1696.378416	17.498471
34.310476	1704.485971	17.503488
34.288580	1684.499627	17.508506
34.462871	1695.529839	17.513523
34.556656	1684.481932	17.518541
34.632468	1695.568174	17.523559
34.572203	1682.085000	17.528576
34.321382	1703.311975	17.533594
34.700720	1688.273572	17.538611
34.656164	1706.443647	17.543629
34.407605	1701.297297	17.548647
34.520249	1703.107467	17.553664
34.524670	1693.602855	17.558682
34.939349	1723.816183	17.563699
34.748117	1728.060156	17.568717
34.936558	1733.268741	17.573735
34.708559	1719.916187	17.578752
35.068849	1730.870911	17.583770
34.868442	1725.750348	17.588787
34.791933	1740.384618	17.593805
34.747566	1722.573162	17.598823
35.129273	1725.936879	17.603840
34.980765	1739.068387	17.608858
35.149171	1724.278052	17.613875
35.049871	1725.319670	17.618893
35.209155	1721.161511	17.623911
35.024662	1721.887057	17.628928
35.304181	1737.299821	17.633946
35.395013	1720.209480	17.638963
35.378341	1728.640991	17.643981
35.340134	1719.344843	17.648999
35.232267	1737.827819	17.654016
35.532989	1741.830587	17.659034
36.186768	1739.006073	17.664051
35.876066	1733.672874	17.669069
35.742786	1717.675662	17.674087
35.869560	1710.507731	17.679104
35.944819	1712.552284	17.684122
36.302599	1693.530045	17.689139
35.789411	1698.592023	17.694157
35.535860	1704.831224	17.699175
35.994034	1700.061781	17.704192
35.852391	1699.284777	17.709210
35.922820	1696.218356	17.714227
35.851573	1705.109865	17.719245
35.899911	1699.499770	17.724263
35.998836	1702.975358	17.729280
35.959860	1688.150740	17.734298
36.222396	1702.207494	17.739315
36.028202	1693.088193	17.744333
35.947223	1702.066035	17.749351
36.032802	1695.803558	17.754368
35.957155	1704.351178	17.759386
36.046881	1697.542651	17.764403
36.106162	1723.478083	17.769421
36.009671	1723.767714	17.774439
36.281897	1728.560661	17.779456
35.981154	1737.778738	17.784474
36.345459	1719.067238	17.789491
36.412787	1727.392660	17.794509
36.230826	1736.709391	17.799527
36.373339	1725.774539	17.804544
36.171232	1730.876439	17.809562
36.613342	1734.194553	17.814579
36.531004	1728.338772	17.819597
36.674084	1728.655924	17.824615
36.658993	1750.308581	17.829632
36.760099	1754.942156	17.834650
36.989227	1764.481068	17.839667
36.788658	1763.426454	17.844685
37.015801	1743.783053	17.849703
36.970544	1734.967986	17.854720
36.676177	1723.368767	17.859738
37.111002	1737.089760	17.864755
37.102176	1749.886838	17.869773
36.923736	1736.976777	17.874791
37.064816	1751.479154	17.879808
36.725259	1748.750403	17.884826
37.228808	1752.683146	17.889843
37.213922	1758.727743	17.894861
37.100951	1755.302522	17.899879
37.312850	1752.381772	17.904896
37.086563	1762.565024	17.909914
37.283111	1755.493788	17.914931
37.014386	1755.079349	17.919949
37.428415	1759.834899	17.924967
37.183910	1743.121638	17.929984
36.942614	1762.660742	17.935002
37.398667	1758.561283	17.940019
37.215180	1760.626657	17.945037
37.226152	1746.933957	17.950055
37.457049	1771.002889	17.955072
37.384170	1775.993209	17.960090
37.596597	1790.121600	17.965107
37.606919	1786.335216	17.970125
37.314996	1791.110411	17.975143
37.497958	1783.589527	17.980160
37.298821	1795.344189	17.985178
37.753749	1781.477027	17.990195
37.531120	1796.635795	17.995213
37.767887	1800.337790	18.000231
38.342795	1805.157301	18.005248
37.909208	1812.626952	18.010266
38.578864	1816.355229	18.015283
38.341956	1806.294972	18.020301
38.207829	1798.271176	18.025319
38.478210	1775.268288	18.030336
38.311700	1779.019111	18.035354
38.661907	1770.203126	18.040371
37.973645	1782.358429	18.045389
38.473399	1784.079936	18.050407
38.803357	1780.766122	18.055424
38.325392	1779.936447	18.060442
38.140784	1775.095091	18.065459
38.089770	1775.639950	18.070477
38.248441	1780.702025	18.075495
38.539801	1786.468016	18.080512
38.592072	1807.409069	18.085530
38.751705	1798.584214	18.090547
38.882081	1800.623410	18.095565
38.601311	1808.257039	18.100583
38.914556	1796.482367	18.105600
38.965031	1813.770203	18.110618
38.985498	1784.414955	18.115635
38.595819	1776.667412	18.120653
38.724862	1785.189024	18.125671
38.983105	1798.424197	18.130688
38.601161	1808.598368	18.135706
39.162755	1798.217710	18.140723
38.799978	1801.023407	18.145741
38.683163	1815.850988	18.150759
38.974961	1790.994599	18.155776
38.883085	1812.974145	18.160794
38.649859	1794.466201	18.165811
38.883942	1809.569285	18.170829
38.927966	1835.674030	18.175847
39.228983	1829.360249	18.180864
39.199967	1842.788376	18.185882
39.415130	1837.476977	18.190899
39.390806	1842.201568	18.195917
39.071552	1834.838935	18.200935
39.431399	1827.991320	18.205952
39.336106	1833.476116	18.210970
39.495148	1829.691321	18.215987
39.853841	1833.199783	18.221005
39.462907	1822.890022	18.226023
39.775791	1840.667491	18.231040
39.547749	1835.656064	18.236058
39.633196	1820.672593	18.241075
39.792809	1836.103305	18.246093
39.711318	1837.886333	18.251111
40.016560	1827.402673	18.256128
39.565430	1834.674091	18.261146
39.856041	1841.896641	18.266163
40.134037	1862.497473	18.271181
40.048054	1862.798949	18.276199
40.150506	1857.109690	18.281216
39.973920	1870.070491	18.286234
40.431591	1848.232871	18.291251
40.395115	1850.972255	18.296269
40.363613	1859.881198	18.301287
40.324618	1836.477757	18.306304
40.047966	1844.880853	18.311322
40.399145	1846.389663	18.316339
40.618395	1837.436158	18.321357
40.039153	1848.219523	18.326375
40.391556	1843.730949	18.331392
40.373020	1838.731346	18.336410
40.494988	1852.554726	18.341427
40.800083	1842.934793	18.346445
40.827715	1850.531452	18.351463
40.998692	1832.171288	18.356480
40.606661	1846.466243	18.361498
40.770928	1843.691609	18.366515
40.905316	1845.709678	18.371533
40.719691	1839.854884	18.376551
40.579268	1841.048652	18.381568
40.584220	1849.862310	18.386586
40.802345	1852.175736	18.391603
40.840777	1849.145964	18.396621
40.570950	1856.130491	18.401639
40.784221	1850.818416	18.406656
40.794704	1871.968786	18.411674
41.033615	1882.627990	18.416691
41.064745	1878.869833	18.421709
41.111639	1883.735690	18.426727
41.228976	1872.705405	18.431744
41.215037	1880.181413	18.436762
40.916976	1887.554603	18.441779
41.299136	1879.096593	18.446797
41.175134	1880.587495	18.451815
41.075831	1880.035922	18.456832
41.003600	1897.746023	18.461850
41.106735	1909.827421	18.466867
41.289829	1928.248668	18.471885
41.601257	1914.452632	18.476903
41.782582	1916.750007	18.481920
41.684067	1910.539810	18.486938
41.748269	1913.723111	18.491955
41.735354	1915.824282	18.496973
41.573847	1911.989112	18.501991
41.731857	1911.046064	18.507008
41.545043	1912.728221	18.512026
42.142126	1930.501538	18.517043
42.257977	1922.999057	18.522061
42.300737	1946.560184	18.527079
42.377708	1915.417329	18.532096
42.798162	1923.843232	18.537114
42.475523	1902.474975	18.542131
42.307632	1900.344876	18.547149
42.217382	1903.922035	18.552167
42.678283	1895.048815	18.557184
42.379576	1905.945771	18.562202
42.277719	1894.600578	18.567219
42.314688	1897.293784	18.572237
42.200230	1905.039911	18.577255
42.316895	1894.073293	18.582272
42.474001	1906.294069	18.587290
42.347622	1906.286139	18.592307
42.500063	1894.339578	18.597325
42.188564	1915.694666	18.602343
42.601391	1912.409149	18.607360
42.483122	1929.117732	18.612378
42.641316	1926.303051	18.617395
42.445665	1923.842460	18.622413
42.618459	1921.218441	18.627431
42.896511	1924.848204	18.632448
42.973517	1929.988280	18.637466
42.686564	1925.943665	18.642483
42.927774	1928.024983	18.647501
42.820410	1941.595746	18.652519
42.861192	1939.150499	18.657536
43.310885	1946.942172	18.662554
43.066132	1943.977188	18.667571
43.481699	1944.829916	18.672589
43.146612	1931.164915	18.677607
43.526760	1942.017906	18.682624
43.443030	1931.892102	18.687642
43.549191	1943.216081	18.692659
43.407484	1925.633920	18.697677
43.286833	1947.225475	18.702695
43.628343	1944.590399	18.707712
43.592981	1946.915321	18.712730
43.517395	1941.023507	18.717747
43.565864	1938.085644	18.722765
43.427350	1940.207673	18.727783
43.605452	1936.873457	18.732800
43.630512	1928.606298	18.737818
43.591752	1940.861044	18.742835
43.769861	1953.771665	18.747853
43.992908	1963.932065	18.752871
43.904595	1964.255676	18.757888
44.204218	1976.321976	18.762906
44.144159	1986.105927	18.767923
44.411968	1972.431889	18.772941
44.317380	1981.305175	18.777959
44.295205	1973.531733	18.782976
44.092463	1975.756687	18.787994
44.169388	1977.513158	18.793011
44.463778	1964.678675	18.798029
44.202576	1976.754010	18.803047
44.599904	1967.317147	18.808064
44.498886	1989.759593	18.813082
44.261957	1967.287122	18.818099
44.260204	1977.336677	18.823117
44.293150	1973.377051	18.828135
44.448894	1978.739325	18.833152
44.427966	1973.218613	18.838170
44.427695	1977.516416	18.843187
44.838066	1980.829202	18.848205
44.496034	1995.849561	18.853223
44.710630	1998.418664	18.858240
45.223251	1997.885329	18.863258
44.783041	1992.733943	18.868275
44.751941	1989.556903	18.873293
44.658339	2000.442664	18.878311
44.599154	1990.735917	18.883328
44.631001	1993.222543	18.888346
44.817195	2001.852527	18.893363
45.311499	2012.180495	18.898381
45.269663	2034.832577	18.903399
45.223552	2025.395449	18.908416
45.590816	2034.423503	18.913434
45.432576	2022.445916	18.918451
45.577557	2019.256106	18.923469
45.525128	2011.743898	18.928487
45.375761	2024.570630	18.933504
45.567572	2019.272278	18.938522
45.767092	2029.704377	18.943539
45.751979	2016.010532	18.948557
45.415392	2042.540568	18.953575
45.931776	2027.703653	18.958592
45.916339	2020.237090	18.963610
45.639133	2036.797088	18.968627
45.885419	2016.532175	18.973645
45.808850	2021.051912	18.978663
45.298832	2012.980495	18.983680
45.592132	2013.913757	18.988698
45.421804	2019.933169	18.993715
45.794093	2023.259442	18.998733
45.876021	2032.735757	19.003751
45.771432	2041.780877	19.008768
46.184855	2043.662326	19.013786
46.297245	2059.893740	19.018803
46.118506	2056.025758	19.023821
46.167459	2051.718155	19.028839
46.477702	2043.874982	19.033856
46.481918	2054.122679	19.038874
46.141509	2045.962007	19.043891
46.472565	2061.405058	19.048909
46.318480	2070.543498	19.053927
46.348513	2095.858124	19.058944
46.828868	2079.837263	19.063962
46.583255	2086.773314	19.068979
47.258283	2083.370329	19.073997
47.237977	2076.269834	19.079015
46.934506	2075.248341	19.084032
46.780017	2072.247750	19.089050
46.857838	2073.923784	19.094067
47.523355	2075.691050	19.099085
47.013973	2063.142239	19.104103
47.130654	2077.016686	19.109120
47.206953	2065.380850	19.114138
47.177141	2070.451928	19.119155
47.335405	2076.780579	19.124173
46.957797	2067.289172	19.129191
47.019535	2076.121228	19.134208
47.438447	2073.515359	19.139226
47.372397	2073.251439	19.144243
47.525263	2068.636060	19.149261
47.462951	2066.534643	19.154279
47.411079	2071.881662	19.159296
47.601141	2061.905177	19.164314
47.461996	2071.353494	19.169331
47.911871	2076.657355	19.174349
47.848992	2079.238572	19.179367
47.799262	2090.265545	19.184384
47.786622	2082.385570	19.189402
47.732850	2086.467776	19.194419
47.811957	2097.988333	19.199437
47.749436	2092.378800	19.204455
47.879425	2082.584345	19.209472
47.735372	2094.049275	19.214490
47.711874	2098.796738	19.219507
48.027630	2090.255016	19.224525
47.913940	2104.801109	19.229543
47.901020	2106.270822	19.234560
48.166482	2119.108889	19.239578
48.267123	2111.389084	19.244595
48.056459	2117.003952	19.249613
48.508999	2116.679819	19.254631
48.481798	2104.406741	19.259648
49.049713	2114.457897	19.264666
48.658563	2110.179314	19.269683
48.417906	2117.571075	19.274701
48.558969	2118.728482	19.279719
48.866585	2121.884394	19.284736
48.815423	2109.580829	19.289754
48.886512	2116.995370	19.294771
48.964853	2113.741469	19.299789
49.175417	2105.852543	19.304807
49.057408	2111.641729	19.309824
49.102135	2100.352363	19.314842
48.882867	2111.033320	19.319859
49.395991	2117.407558	19.324877
49.326698	2095.600383	19.329895
48.968850	2110.029082	19.334912
49.423423	2102.164784	19.339930
49.208090	2103.059391	19.344947
49.552549	2110.634819	19.349965
49.382574	2108.463211	19.354983
49.349881	2106.106740	19.360000
49.433449	2101.626108	19.365018
49.282107	2100.228944	19.370035
49.508358	2126.901899	19.375053
49.511514	2136.524245	19.380071
49.642416	2142.879095	19.385088
49.770834	2141.842121	19.390106
49.523037	2147.618129	19.395123
49.568373	2143.693217	19.400141
49.578052	2127.495998	19.405159
49.314715	2148.531988	19.410176
49.911493	2145.134935	19.415194
49.821286	2156.928948	19.420211
50.075885	2166.468527	19.425229
50.230261	2158.294422	19.430247
49.801808	2177.063641	19.435264
49.971816	2172.296407	19.440282
50.032462	2169.397918	19.445299
50.587764	2166.375368	19.450317
50.499841	2171.520935	19.455335
50.074557	2176.563225	19.460352
50.356064	2185.496110	19.465370
50.504618	2203.673240	19.470387
50.586091	2206.192244	19.475405
50.485109	2204.351191	19.480423
50.581475	2218.729335	19.485440
50.715182	2199.160135	19.490458
50.761601	2216.543075	19.495475
50.688592	2195.904484	19.500493
50.650221	2204.699723	19.505511
51.017771	2197.374866	19.510528
51.155991	2200.930576	19.515546
50.928520	2202.999931	19.520563
50.851980	2192.490941	19.525581
50.875023	2213.418483	19.530599
51.065685	2226.126800	19.535616
51.485819	2229.014772	19.540634
51.174542	2234.709192	19.545651
51.286239	2220.441938	19.550669
51.784927	2220.330810	19.555687
51.599779	2217.239505	19.560704
51.757220	2231.835089	19.565722
51.602156	2220.455936	19.570739
51.473257	2226.168828	19.575757
51.968184	2231.438531	19.580775
51.513944	2232.855322	19.585792
51.957070	2227.044481	19.590810
51.487656	2231.054491	19.595827
51.542421	2227.823750	19.600845
51.944180	2222.536787	19.605863
51.837103	2241.721204	19.610880
52.125731	2224.568880	19.615898
51.708768	2234.846936	19.620915
51.887691	2226.774626	19.625933
51.985617	2211.379136	19.630951
52.148115	2244.130320	19.635968
52.511404	2241.672471	19.640986
52.431245	2243.658442	19.646003
52.395962	2259.249718	19.651021
52.516579	2247.085148	19.656039
52.692199	2239.555611	19.661056
52.690076	2245.066290	19.666074
52.935274	2232.520573	19.671091
52.609643	2219.479337	19.676109
52.859700	2211.683027	19.681127
52.444762	2213.790646	19.686144
52.677356	2221.298606	19.691162
53.005502	2232.245718	19.696179
52.662610	2241.851018	19.701197
52.630683	2236.420401	19.706215
52.822986	2245.369833	19.711232
53.160372	2243.273488	19.716250
52.718601	2249.060924	19.721267
52.793988	2241.679621	19.726285
52.781115	2244.671037	19.731303
52.735116	2255.141895	19.736320
53.010650	2263.249570	19.741338
53.050116	2266.945610	19.746355
52.822532	2283.844663	19.751373
53.000142	2275.850288	19.756391
53.291448	2300.861488	19.761408
53.535518	2294.170279	19.766426
54.004842	2284.373448	19.771443
54.051461	2301.455713	19.776461
54.037943	2290.124758	19.781479
53.954808	2300.762191	19.786496
53.992777	2279.950251	19.791514
54.058437	2298.145129	19.796531
54.107820	2288.726305	19.801549
54.303850	2277.368997	19.806567
53.987614	2269.852628	19.811584
54.257964	2276.573401	19.816602
54.639641	2264.748684	19.821619
54.274219	2263.224704	19.826637
54.328446	2257.942413	19.831655
54.172743	2264.739494	19.836672
54.408445	2268.816423	19.841690
54.790190	2282.706397	19.846707
54.577845	2286.074824	19.851725
54.439303	2265.595370	19.856743
54.447336	2263.685712	19.861760
54.669039	2274.311327	19.866778
54.830755	2285.301923	19.871795
54.857577	2292.536689	19.876813
54.776641	2289.005578	19.881831
54.435343	2286.947577	19.886848
54.586229	2284.066629	19.891866
54.742450	2284.894629	19.896883
54.366434	2288.584544	19.901901
54.697656	2297.745855	19.906919
54.637273	2308.971760	19.911936
54.792225	2317.461341	19.916954
55.043367	2313.764340	19.921971
55.077302	2317.233391	19.926989
55.204383	2312.809374	19.932007
55.192405	2321.138975	19.937024
55.438703	2334.663055	19.942042
55.502628	2331.261318	19.947059
55.481072	2347.089550	19.952077
55.796762	2339.624795	19.957095
55.678974	2334.872596	19.962112
55.386348	2338.434390	19.967130
55.874462	2331.412921	19.972147
55.989227	2330.351030	19.977165
55.891433	2331.005100	19.982183
55.949510	2330.408213	19.987200
56.097358	2331.494645	19.992218
56.142055	2327.582585	19.997235
55.790650	2336.053311	20.002253
56.147823	2332.035683	20.007271
56.053797	2322.199663	20.012288
56.284219	2317.705230	20.017306
56.359176	2314.164293	20.022323
56.149341	2319.782542	20.027341
56.319939	2319.867539	20.032359
56.302733	2336.436852	20.037376
56.834221	2357.732858	20.042394
56.665684	2339.028260	20.047411
56.474595	2359.274572	20.052429
56.797927	2346.609568	20.057447
56.510486	2356.337250	20.062464
56.485880	2351.924119	20.067482
56.460788	2347.609676	20.072499
56.659985	2348.351653	20.077517
57.141389	2345.446580	20.082535
56.940230	2354.813208	20.087552
56.947060	2376.719286	20.092570
56.983107	2378.901981	20.097587
56.749258	2390.942120	20.102605
57.079645	2372.369368	20.107623
57.180995	2374.420621	20.112640
57.345731	2382.113863	20.117658
57.490167	2379.127877	20.122675
57.238105	2387.206485	20.127693
57.790294	2376.823157	20.132711
57.523112	2385.815932	20.137728
57.769828	2397.755798	20.142746
57.851122	2398.957941	20.147763
57.900444	2405.572013	20.152781
58.136753	2402.042772	20.157799
58.225008	2422.979308	20.162816
58.033541	2387.695166	20.167834
57.989861	2387.957481	20.172851
57.698367	2397.448888	20.177869
58.134053	2387.954356	20.182887
58.181886	2400.966495	20.187904
58.102838	2396.166347	20.192922
58.451252	2392.996279	20.197939
58.302884	2396.961149	20.202957
58.569358	2399.365965	20.207975
58.522935	2394.220911	20.212992
58.609054	2399.270086	20.218010
58.409287	2406.205986	20.223027
58.442704	2391.016614	20.228045
58.341300	2401.281407	20.233063
58.883834	2413.819347	20.238080
59.042499	2422.428038	20.243098
58.914155	2413.265245	20.248115
58.996895	2438.096602	20.253133
58.928783	2425.012831	20.258151
58.808128	2433.845023	20.263168
58.655948	2423.823893	20.268186
58.808099	2424.769288	20.273203
58.826956	2431.323061	20.278221
58.874677	2421.236225	20.283239
59.223891	2445.863544	20.288256
59.170854	2461.894901	20.293274
59.565402	2457.360118	20.298291
59.343068	2475.854729	20.303309
59.453895	2465.781842	20.308327
59.640717	2465.515393	20.313344
59.650709	2474.982612	20.318362
59.459769	2456.110339	20.323379
59.988087	2458.636041	20.328397
59.744112	2450.630155	20.333415
59.464995	2466.226705	20.338432
59.735172	2477.687040	20.343450
60.077564	2476.632988	20.348467
59.992519	2492.073496	20.353485
60.052748	2481.525567	20.358503
60.097364	2489.850236	20.363520
60.114409	2480.980061	20.368538
60.583540	2480.428412	20.373555
60.619245	2481.218474	20.378573
60.520121	2490.576983	20.383591
60.535839	2484.355647	20.388608
60.281416	2483.253983	20.393626
60.139924	2482.535762	20.398643
60.472845	2505.395661	20.403661
60.812057	2512.668658	20.408679
61.019641	2509.317736	20.413696
60.927867	2526.347148	20.418714
60.909878	2505.531751	20.423731
61.012879	2514.648634	20.428749
61.061836	2495.995685	20.433767
61.069864	2511.626707	20.438784
60.984822	2500.285963	20.443802
61.254547	2511.159871	20.448819
61.082302	2499.978596	20.453837
61.402128	2502.200031	20.458855
61.416131	2502.401642	20.463872
61.342638	2513.088999	20.468890
61.633644	2535.071157	20.473907
61.482654	2523.879660	20.478925
61.800598	2527.041429	20.483943
62.099232	2519.616605	20.488960
61.773138	2532.750680	20.493978
62.218032	2526.533393	20.498995
62.023981	2517.151508	20.504013
61.973746	2526.386425	20.509031
61.678638	2519.030197	20.514048
62.001083	2521.429128	20.519066
61.658579	2511.613776	20.524083
61.400135	2533.496405	20.529101
61.770391	2539.956135	20.534119
62.166757	2560.088114	20.539136
62.086724	2555.820088	20.544154
62.463336	2545.958308	20.549171
62.616650	2550.566373	20.554189
62.668662	2549.279832	20.559207
62.831657	2562.807842	20.564224
62.449218	2557.394883	20.569242
62.578269	2575.176128	20.574259
62.785406	2581.112517	20.579277
63.103551	2598.317146	20.584295
63.191313	2582.710396	20.589312
62.834070	2586.935981	20.594330
63.338130	2581.923681	20.599347
63.220260	2587.807498	20.604365
63.286196	2588.376065	20.609383
63.342048	2579.997774	20.614400
63.419738	2577.102690	20.619418
63.798086	2571.308134	20.624435
63.477602	2578.805518	20.629453
63.513961	2573.823470	20.634471
63.476751	2575.117838	20.639488
63.469277	2573.753343	20.644506
63.775120	2571.030369	20.649523
63.681908	2568.878781	20.654541
63.533565	2585.549745	20.659559
63.784005	2562.853363	20.664576
63.762613	2588.313303	20.669594
63.839441	2595.011677	20.674611
63.854033	2605.796730	20.679629
63.899002	2608.808969	20.684647
63.924879	2603.133270	20.689664
63.586484	2619.917754	20.694682
64.342441	2628.835082	20.699699
64.420801	2634.805960	20.704717
64.520246	2631.143795	20.709735
64.865122	2640.047972	20.714752
64.792923	2633.789536	20.719770
64.879602	2635.763733	20.724787
64.871342	2637.821326	20.729805
64.887902	2644.349194	20.734823
65.325550	2624.260394	20.739840
65.017978	2629.403440	20.744858
64.951483	2618.328011	20.749875
64.834232	2619.766103	20.754893
65.131267	2621.146756	20.759911
65.111269	2634.614335	20.764928
65.147356	2622.074712	20.769946
65.714967	2628.209585	20.774963
65.410971	2626.020980	20.779981
65.281733	2622.987666	20.784999
65.457307	2618.097346	20.790016
65.401189	2630.826310	20.795034
65.613085	2625.413522	20.800051
65.415684	2627.157733	20.805069
65.435737	2635.724696	20.810087
65.849739	2663.258179	20.815104
65.725880	2663.549888	20.820122
65.754150	2666.043907	20.825139
65.950973	2663.067711	20.830157
65.783941	2662.469040	20.835175
65.903615	2651.427380	20.840192
65.975768	2659.154365	20.845210
66.125060	2677.510454	20.850227
66.379566	2680.854369	20.855245
66.435547	2691.408657	20.860263
66.817314	2679.168704	20.865280
66.459160	2699.425553	20.870298
66.922031	2681.289530	20.875315
66.671525	2672.962799	20.880333
66.499394	2683.914966	20.885351
66.924638	2677.842578	20.890368
66.678340	2685.136638	20.895386
66.923329	2684.092962	20.900403
66.862705	2676.872885	20.905421
66.898048	2691.600486	20.910439
67.173712	2698.272148	20.915456
67.202300	2706.659811	20.920474
67.253476	2725.131173	20.925491
67.359853	2717.662052	20.930509
67.285499	2732.519222	20.935527
67.558620	2714.037402	20.940544
67.331885	2723.245509	20.945562
67.450597	2704.738632	20.950579
67.620710	2712.589792	20.955597
67.438300	2719.031297	20.960615
67.441959	2713.229325	20.965632
67.841898	2738.489787	20.970650
67.806791	2731.814016	20.975667
67.815027	2733.741944	20.980685
67.558492	2731.041414	20.985703
68.011313	2732.281781	20.990720
67.794274	2733.174835	20.995738
67.987034	2751.339601	21.000755
68.285472	2754.429455	21.005773
68.519817	2753.578649	21.010791
68.540990	2754.074316	21.015808
68.683129	2756.176943	21.020826
68.821037	2758.952819	21.025843
69.039917	2755.077409	21.030861
68.445125	2764.411315	21.035879
68.690501	2758.322957	21.040896
68.950853	2749.945814	21.045914
68.720951	2752.794477	21.050931
68.960387	2746.143007	21.055949
69.119747	2755.944133	21.060967
69.101453	2735.589437	21.065984
69.081121	2748.924709	21.071002
69.266602	2752.619371	21.076019
69.366311	2779.800331	21.081037
69.236335	2774.693166	21.086055
69.619050	2783.022744	21.091072
69.638106	2773.018161	21.096090
69.769770	2775.055011	21.101107
69.682768	2777.515545	21.106125
69.513312	2778.990228	21.111143
69.719862	2776.264732	21.116160
69.871153	2774.382905	21.121178
69.593650	2770.615107	21.126195
70.009027	2784.604887	21.131213
70.095310	2809.178023	21.136231
70.410727	2798.023803	21.141248
70.481040	2809.497732	21.146266
70.115175	2799.028463	21.151283
70.344207	2808.463627	21.156301
70.253304	2804.719899	21.161319
70.646570	2801.211081	21.166336
70.564843	2816.079785	21.171354
70.438030	2812.553379	21.176371
70.719522	2807.215039	21.181389
70.357387	2829.665743	21.186407
70.771805	2826.623246	21.191424
70.592866	2842.465202	21.196442
70.736362	2835.819706	21.201459
70.838793	2835.927585	21.206477
70.805523	2849.419589	21.211495
71.005398	2855.853089	21.216512
71.127250	2861.282092	21.221530
71.454030	2861.922904	21.226547
71.852261	2851.850690	21.231565
71.479107	2862.941308	21.236583
71.715976	2855.722372	21.241600
71.894249	2852.171915	21.246618
71.837319	2861.665390	21.251635
72.254348	2846.703479	21.256653
71.943245	2862.278553	21.261671
72.146653	2844.235209	21.266688
72.327254	2860.110079	21.271706
72.229259	2848.302577	21.276723
72.260102	2854.868524	21.281741
72.663048	2856.144897	21.286759
72.235414	2853.187813	21.291776
72.197226	2857.874658	21.296794
72.268864	2856.822220	21.301811
72.393358	2849.642131	21.306829
72.412349	2862.052220	21.311847
72.279926	2863.198391	21.316864
72.484524	2884.156481	21.321882
72.504021	2886.873218	21.326899
72.597950	2882.331501	21.331917
72.544286	2880.500655	21.336935
72.807777	2881.084021	21.341952
72.842405	2900.722751	21.346970
72.977486	2905.873634	21.351987
73.011590	2902.398362	21.357005
73.150045	2920.927574	21.362023
73.436743	2903.563817	21.367040
73.364523	2911.039820	21.372058
73.208843	2912.675803	21.377075
73.724907	2897.493171	21.382093
73.218447	2913.230090	21.387111
73.570457	2933.347648	21.392128
74.163280	2937.347634	21.397146
73.769165	2939.386167	21.402163
74.213367	2931.714480	21.407181
74.137365	2936.950249	21.412199
74.059064	2942.481640	21.417216
74.162323	2930.178865	21.422234
74.121928	2939.802710	21.427251
74.290272	2934.404885	21.432269
74.181939	2927.102034	21.437287
74.285862	2938.659471	21.442304
74.347166	2945.614863	21.447322
74.293790	2968.212359	21.452339
74.635178	2959.159585	21.457357
74.434483	2974.168166	21.462375
74.765580	2950.424148	21.467392
74.952503	2971.390002	21.472410
74.727061	2977.988118	21.477427
75.147173	2983.867818	21.482445
75.075149	2987.219506	21.487463
74.958276	2990.623876	21.492480
75.359021	2984.724297	21.497498
75.621354	2988.662389	21.502515
75.538295	2989.925200	21.507533
75.173425	2991.959496	21.512551
75.566253	2974.784397	21.517568
75.868279	2985.527531	21.522586
75.706657	2985.006094	21.527603
76.263578	3001.014962	21.532621
75.942301	2989.596571	21.537639
75.892227	3001.451715	21.542656
76.128852	2993.973731	21.547674
76.253332	3007.541171	21.552691
76.555761	2996.315735	21.557709
76.277233	3007.791560	21.562727
76.711154	2998.174323	21.567744
76.562400	3005.249878	21.572762
76.644786	3003.537070	21.577779
76.863366	3011.925388	21.582797
76.408694	3008.795597	21.587815
76.678760	3001.019400	21.592832
76.910297	3003.485001	21.597850
76.852217	3012.804763	21.602867
76.856395	3006.536900	21.607885
76.611652	3011.133727	21.612903
76.879591	3023.157964	21.617920
76.878368	3031.128731	21.622938
76.733564	3045.291823	21.627955
76.924097	3034.649156	21.632973
76.926991	3046.584549	21.637991
77.186600	3063.580500	21.643008
77.399316	3068.103716	21.648026
77.139408	3073.997805	21.653043
77.564022	3065.415021	21.658061
77.436635	3072.632729	21.663079
77.756622	3059.993479	21.668096
78.178969	3089.276348	21.673114
78.031227	3090.035937	21.678131
78.241816	3090.450318	21.683149
78.308045	3091.222574	21.688167
78.437672	3082.965662	21.693184
78.813303	3088.032765	21.698202
78.259436	3092.371481	21.703219
78.796305	3081.713081	21.708237
78.663144	3090.982706	21.713255
78.693439	3086.904545	21.718272
78.809723	3083.563076	21.723290
78.585751	3094.939999	21.728307
78.819256	3073.386288	21.733325
78.927586	3080.183790	21.738343
78.668864	3074.395714	21.743360
78.879294	3079.517276	21.748378
78.553914	3089.926810	21.753395
78.794919	3096.221936	21.758413
78.899696	3104.896011	21.763431
79.237677	3115.047926	21.768448
79.923026	3109.911219	21.773466
79.736045	3115.606875	21.778483
79.953879	3125.451915	21.783501
79.803735	3105.300980	21.788519
79.756021	3126.968346	21.793536
79.970725	3109.038760	21.798554
79.736019	3125.517908	21.803571
80.065312	3111.854944	21.808589
79.907309	3127.839780	21.813607
80.381492	3120.354758	21.818624
80.361661	3124.002935	21.823642
80.520617	3124.550050	21.828659
80.568241	3123.226789	21.833677
80.496747	3117.483142	21.838695
80.565392	3121.289711	21.843712
80.860762	3143.406846	21.848730
80.423671	3163.673608	21.853747
80.852392	3152.704916	21.858765
80.885603	3146.758935	21.863783
81.026310	3151.684389	21.868800
81.173488	3149.037530	21.873818
81.154175	3157.958102	21.878835
81.103094	3139.456521	21.883853
81.207667	3170.439322	21.888871
81.367443	3173.889148	21.893888
81.715452	3180.969298	21.898906
81.523480	3178.284985	21.903923
81.808618	3182.432919	21.908941
81.962679	3191.993295	21.913959
81.655031	3175.208699	21.918976
82.159258	3173.854070	21.923994
81.819672	3179.958196	21.929011
81.830775	3175.947349	21.934029
82.201788	3181.966132	21.939047
82.040167	3188.766761	21.944064
82.171818	3207.095494	21.949082
82.009976	3205.622017	21.954099
82.347460	3206.972224	21.959117
82.547166	3220.697482	21.964135
82.538679	3212.895170	21.969152
82.572805	3221.823482	21.974170
82.546789	3227.828569	21.979187
82.790280	3231.640914	21.984205
82.892297	3233.342011	21.989223
83.059014	3230.423433	21.994240
83.161201	3231.866850	21.999258
83.108635	3240.481579	22.004275
83.450803	3235.056106	22.009293
83.652381	3228.094182	22.014311
83.497189	3226.425726	22.019328
83.738222	3217.386237	22.024346
83.642309	3230.467906	22.029363
83.487367	3230.334293	22.034381
83.395071	3241.124266	22.039399
83.530985	3250.445182	22.044416
83.969305	3263.520084	22.049434
83.672095	3277.141306	22.054451
84.009455	3256.049265	22.059469
84.200297	3269.180618	22.064487
83.898945	3265.804002	22.069504
84.151086	3272.134364	22.074522
84.380093	3294.708112	22.079539
84.341684	3293.348862	22.084557
84.594543	3292.216059	22.089575
84.524995	3298.823192	22.094592
84.808810	3282.031282	22.099610
84.584214	3295.296854	22.104627
84.664252	3304.798672	22.109645
85.217496	3309.528261	22.114663
85.143661	3318.168396	22.119680
85.407752	3317.552780	22.124698
85.442461	3310.295197	22.129715
85.234948	3321.587291	22.134733
85.169870	3316.002731	22.139751
85.390434	3306.100120	22.144768
85.602989	3331.924558	22.149786
85.335326	3332.016047	22.154803
85.449183	3342.879888	22.159821
85.639540	3343.677506	22.164839
85.405396	3354.511863	22.169856
85.775982	3355.769614	22.174874
85.971576	3375.094383	22.179891
86.302606	3371.251857	22.184909
86.550999	3373.701348	22.189927
86.465912	3379.942022	22.194944
86.821013	3374.379337	22.199962
86.718356	3380.142841	22.204979
86.949193	3376.994171	22.209997
86.970111	3367.996086	22.215015
86.798551	3375.501917	22.220032
86.963691	3363.818829	22.225050
86.992936	3352.087937	22.230067
86.961190	3376.976731	22.235085
86.829627	3383.815781	22.240103
87.077025	3395.426813	22.245120
87.196514	3387.875288	22.250138
87.340694	3390.735274	22.255155
87.289663	3389.688703	22.260173
87.850006	3413.325486	22.265191
87.381923	3418.992713	22.270208
87.866466	3421.027827	22.275226
87.871459	3416.392589	22.280243
87.709058	3435.842138	22.285261
88.211578	3429.131548	22.290279
87.892316	3432.796015	22.295296
88.040871	3410.537825	22.300314
88.499903	3441.345284	22.305331
88.516816	3453.081250	22.310349
88.922693	3435.309835	22.315367
88.552474	3453.374188	22.320384
89.084852	3446.379744	22.325402
88.908287	3450.944766	22.330419
88.776110	3445.640711	22.335437
88.819106	3445.595046	22.340455
88.946826	3443.745771	22.345472
89.004772	3442.090098	22.350490
89.188371	3446.118872	22.355507
89.059716	3460.664483	22.360525
89.267229	3436.431329	22.365543
88.763131	3457.128407	22.370560
89.120099	3471.697511	22.375578
89.074061	3472.969597	22.380595
89.216492	3488.364062	22.385613
89.522400	3479.554034	22.390631
89.520066	3503.556356	22.395648
89.925313	3502.682979	22.400666
90.031970	3508.200935	22.405683
90.017987	3511.596487	22.410701
90.201254	3496.682618	22.415719
89.904320	3518.158861	22.420736
90.350763	3530.427400	22.425754
90.453983	3531.908665	22.430771
90.360265	3534.963096	22.435789
90.621065	3530.420187	22.440807
90.673904	3547.661848	22.445824
90.901573	3544.858522	22.450842
91.042189	3550.252584	22.455859
90.804807	3561.518491	22.460877
91.098673	3564.583087	22.465895
91.114083	3555.960773	22.470912
91.416818	3554.514616	22.475930
91.294198	3561.189682	22.480947
91.363088	3549.965630	22.485965
91.827170	3566.759857	22.490983
91.903675	3568.229202	22.496000
92.161680	3585.459441	22.501018
92.083754	3578.933281	22.506035
91.963002	3575.443490	22.511053
92.452529	3579.512092	22.516071
92.217971	3581.076539	22.521088
92.199973	3562.816603	22.526106
92.350531	3569.091045	22.531123
92.040756	3577.497501	22.536141
92.290180	3564.371509	22.541159
92.272856	3590.680788	22.546176
92.211184	3585.669932	22.551194
92.438970	3603.414987	22.556211
92.251677	3602.868244	22.561229
92.590457	3630.980020	22.566247
92.832509	3637.631468	22.571264
92.924106	3638.871374	22.576282
93.355066	3635.716549	22.581299
93.131777	3634.870658	22.586317
93.344489	3664.298112	22.591335
93.290321	3654.293052	22.596352
93.644700	3662.280179	22.601370
93.936055	3658.315606	22.606387
93.751118	3663.442269	22.611405
94.156616	3657.742621	22.616423
94.024222	3654.992083	22.621440
93.910157	3656.035482	22.626458
94.123084	3675.256195	22.631475
94.284368	3683.134701	22.636493
94.743534	3677.738949	22.641511
94.493110	3687.397770	22.646528
94.930070	3685.040705	22.651546
94.458948	3673.284979	22.656563
94.549248	3686.374054	22.661581
94.860564	3675.122843	22.666599
94.964494	3677.126210	22.671616
94.848899	3687.180634	22.676634
95.080391	3685.288397	22.681651
95.200641	3707.200652	22.686669
95.470613	3695.785993	22.691687
95.061216	3711.337810	22.696704
95.095454	3697.463462	22.701722
95.568179	3704.685045	22.706739
95.496358	3713.774052	22.711757
95.614736	3705.045473	22.716775
95.471595	3735.793196	22.721792
95.748836	3728.031198	22.726810
95.918404	3739.303012	22.731827
95.734583	3748.473732	22.736845
96.092384	3746.182098	22.741863
96.086673	3768.286896	22.746880
96.225188	3768.264812	22.751898
96.346481	3771.698692	22.756915
96.076657	3774.082121	22.761933
96.453012	3780.982679	22.766951
96.510194	3798.341807	22.771968
96.884848	3804.631279	22.776986
96.717251	3797.509648	22.782003
96.630965	3813.529793	22.787021
96.996208	3819.733037	22.792039
97.409361	3825.081962	22.797056
97.417118	3829.331812	22.802074
97.630636	3822.476304	22.807091
97.435662	3832.283325	22.812109
97.741813	3825.678633	22.817127
97.868850	3837.946856	22.822144
98.126457	3845.911097	22.827162
98.594538	3845.515478	22.832179
98.389500	3857.496880	22.837197
98.483713	3842.981229	22.842215
98.781438	3852.653305	22.847232
98.896152	3837.044575	22.852250
99.344422	3825.540322	22.857267
99.049068	3804.106450	22.862285
99.278654	3807.342927	22.867303
99.144825	3801.979775	22.872320
99.071126	3795.419363	22.877338
99.260895	3804.783679	22.882355
99.029750	3804.031590	22.887373
99.113784	3787.722119	22.892391
99.073465	3799.453436	22.897408
99.098093	3829.154003	22.902426
99.197199	3825.079039	22.907443
99.171477	3841.156917	22.912461
99.553815	3831.669731	22.917479
99.636290	3850.879939	22.922496
100.005624	3860.777574	22.927514
100.266005	3854.979992	22.932531
99.752618	3856.542906	22.937549
99.986522	3859.296427	22.942567
99.680334	3864.478820	22.947584
99.765837	3884.204679	22.952602
100.116482	3889.260825	22.957619
100.158333	3913.270850	22.962637
100.263572	3903.730991	22.967655
100.247121	3928.717942	22.972672
100.461594	3925.840749	22.977690
100.728193	3938.680051	22.982707
100.810834	3961.784642	22.987725
101.109430	3957.708173	22.992743
101.032150	3974.427352	22.997760
101.039567	3961.975430	23.002778
101.598667	3965.885403	23.007795
101.411252	3969.334123	23.012813
101.786747	3978.193863	23.017831
101.640901	3981.150309	23.022848
101.770839	3994.766531	23.027866
102.059723	3979.582002	23.032883
101.816129	3984.295848	23.037901
101.959061	3982.369788	23.042919
101.928097	3993.636738	23.047936
102.022357	4005.834137	23.052954
102.780498	3998.313780	23.057971
102.674886	4019.380380	23.062989
102.902300	4005.190187	23.068007
102.911805	4013.168348	23.073024
102.783712	4015.369542	23.078042
103.142362	4000.017173	23.083059
102.990189	4010.007776	23.088077
103.262650	4001.854325	23.093095
103.213036	4006.625488	23.098112
103.347612	4036.172856	23.103130
103.602895	4018.019972	23.108147
103.510372	4025.630374	23.113165
103.628803	4029.900964	23.118183
103.774934	4020.899524	23.123200
103.765144	4023.039439	23.128218
103.708781	4036.761284	23.133235
103.679515	4055.020178	23.138253
103.818697	4059.414901	23.143271
104.099767	4060.539087	23.148288
103.936615	4079.192163	23.153306
104.265044	4077.429918	23.158323
104.352595	4098.200544	23.163341
104.304941	4093.304918	23.168359
104.611594	4106.044831	23.173376
104.911003	4124.023520	23.178394
105.202847	4115.201875	23.183411
104.967359	4133.134718	23.188429
105.454791	4119.710080	23.193447
105.773255	4123.803947	23.198464
105.516443	4109.637379	23.203482
105.931847	4124.043120	23.208499
105.985085	4120.600041	23.213517
105.584886	4122.496624	23.218535
105.854131	4131.020875	23.223552
106.019805	4150.121647	23.228570
106.323812	4133.077460	23.233587
106.244063	4146.838304	23.238605
106.540496	4138.083602	23.243623
106.479550	4134.194841	23.248640
106.134015	4144.774545	23.253658
106.646316	4151.065429	23.258675
106.820757	4162.305252	23.263693
106.744657	4179.782694	23.268711
107.056808	4163.156797	23.273728
106.749949	4175.076139	23.278746
107.235002	4162.711657	23.283763
106.994561	4169.333227	23.288781
107.201991	4194.357623	23.293799
107.390603	4208.676909	23.298816
107.221524	4201.870285	23.303834
107.763519	4210.046765	23.308851
107.792630	4216.378153	23.313869
107.944073	4223.246394	23.318887
107.928355	4225.440465	23.323904
107.917079	4242.268312	23.328922
108.294748	4222.985950	23.333939
107.972999	4241.839439	23.338957
108.384433	4234.847505	23.343975
108.445013	4256.950312	23.348992
108.528792	4252.511641	23.354010
108.756093	4265.925012	23.359027
109.083602	4260.470111	23.364045
108.878950	4248.252603	23.369063
109.165226	4250.109776	23.374080
109.012707	4254.559056	23.379098
109.424894	4247.387471	23.384115
109.433606	4259.437007	23.389133
109.266169	4260.662487	23.394151
109.630344	4279.046781	23.399168
109.604077	4288.616376	23.404186
109.769534	4271.063848	23.409203
109.819855	4281.290445	23.414221
110.059909	4274.426810	23.419239
110.130540	4291.504553	23.424256
110.066008	4308.034590	23.429274
110.485960	4294.523318	23.434291
110.302696	4306.334150	23.439309
110.294501	4288.202443	23.444327
110.750965	4308.328551	23.449344
110.598939	4314.579678	23.454362
110.805729	4331.972357	23.459379
110.807632	4333.294660	23.464397
111.120118	4336.896279	23.469415
111.244106	4338.814925	23.474432
111.228649	4356.556553	23.479450
111.477726	4363.128022	23.484467
111.646654	4371.568199	23.489485
111.472480	4368.329176	23.494503
111.726103	4356.853941	23.499520
111.422107	4374.945624	23.504538
112.171346	4381.614367	23.509555
112.210778	4398.773760	23.514573
112.261556	4385.351760	23.519591
112.610587	4389.704420	23.524608
112.477205	4395.762346	23.529626
112.634081	4385.477063	23.534643
112.792812	4401.398274	23.539661
112.705170	4405.112091	23.544679
113.110582	4406.944872	23.549696
113.037742	4409.275963	23.554714
113.044820	4411.367871	23.559731
113.209358	4401.590747	23.564749
112.922171	4423.225682	23.569767
113.442575	4431.301913	23.574784
113.155314	4444.438272	23.579802
113.474341	4441.644493	23.584819
113.277381	4468.143604	23.589837
113.727081	4462.500729	23.594855
114.118618	4462.401206	23.599872
113.920820	4473.589777	23.604890
114.134498	4506.061129	23.609907
114.331943	4495.212387	23.614925
114.149294	4503.215467	23.619943
114.342929	4499.734144	23.624960
114.662719	4517.150090	23.629978
114.725639	4533.797098	23.634995
115.438644	4527.791404	23.640013
115.431672	4546.068845	23.645031
115.782379	4517.600960	23.650048
115.728984	4533.196342	23.655066
115.789430	4522.663521	23.660083
115.748745	4520.914979	23.665101
115.895820	4530.904103	23.670119
116.067766	4513.733293	23.675136
115.868829	4519.946979	23.680154
115.885897	4520.932152	23.685171
116.068466	4540.277459	23.690189
116.257017	4550.242025	23.695207
116.282801	4541.846776	23.700224
116.536606	4554.340284	23.705242
116.574240	4551.586686	23.710259
116.540002	4545.809580	23.715277
116.350264	4561.360985	23.720295
117.248698	4560.433616	23.725312
116.877386	4587.714486	23.730330
116.865821	4575.324657	23.735347
116.729720	4580.396898	23.740365
117.023336	4609.416723	23.745383
117.405611	4600.405060	23.750400
117.461661	4615.984408	23.755418
117.591529	4617.928101	23.760435
117.990386	4616.636831	23.765453
117.537171	4621.013070	23.770471
117.554944	4632.727937	23.775488
117.829433	4633.017437	23.780506
118.037774	4652.219256	23.785523
118.232238	4663.113224	23.790541
118.260333	4672.580372	23.795559
118.442122	4663.776998	23.800576
118.344626	4679.866818	23.805594
119.138065	4688.490189	23.810611
119.402874	4695.477307	23.815629
118.994298	4705.233955	23.820647
119.192567	4688.999935	23.825664
119.444950	4708.118168	23.830682
119.675162	4695.780416	23.835699
119.543911	4716.777790	23.840717
119.627047	4732.134669	23.845735
120.036895	4735.880136	23.850752
120.257404	4722.938457	23.855770
119.867730	4731.476255	23.860787
120.351616	4731.460289	23.865805
120.286060	4742.839798	23.870823
120.611741	4747.841298	23.875840
120.734130	4750.597659	23.880858
120.601510	4759.956773	23.885875
120.755954	4744.756706	23.890893
120.840673	4749.425585	23.895911
121.305888	4775.471704	23.900928
121.380116	4767.655729	23.905946
121.360530	4779.535935	23.910963
121.521883	4779.061063	23.915981
121.723511	4784.206696	23.920999
121.974240	4777.777297	23.926016
121.933879	4772.027496	23.931034
121.881870	4791.261092	23.936051
121.689296	4784.953762	23.941069
121.648495	4811.757574	23.946087
121.854539	4811.169804	23.951104
122.300935	4831.295500	23.956122
122.421662	4836.891922	23.961139
122.335222	4841.328480	23.966157
122.743240	4857.423927	23.971175
123.032106	4847.740940	23.976192
123.113729	4864.117495	23.981210
123.209897	4861.005743	23.986227
123.505079	4865.032789	23.991245
123.282750	4863.308318	23.996263
123.579854	4871.438610	24.001280
123.704810	4858.510639	24.006298
123.715497	4890.529723	24.011315
123.806859	4891.831778	24.016333
123.776323	4903.402076	24.021351
124.027152	4894.592281	24.026368
124.179827	4892.282214	24.031386
124.202753	4901.930278	24.036403
124.371592	4918.179092	24.041421
124.418456	4922.170414	24.046439
124.462044	4917.413782	24.051456
124.538254	4927.642433	24.056474
124.525909	4940.030624	24.061491
125.054085	4952.330296	24.066509
124.723449	4942.190559	24.071527
125.181042	4960.349200	24.076544
125.218924	4971.892101	24.081562
125.290504	4975.744706	24.086579
125.689056	4980.044074	24.091597
125.526917	4972.897770	24.096615
125.943205	5000.390558	24.101632
126.235801	4993.036030	24.106650
126.461804	5000.163165	24.111667
126.927421	4977.472774	24.116685
126.696452	5001.268931	24.121703
126.883398	4996.144488	24.126720
126.876211	4994.020667	24.131738
126.867417	5000.070445	24.136755
127.042650	4997.706634	24.141773
127.065238	5000.215354	24.146791
127.032842	5023.850385	24.151808
127.503213	5013.410521	24.156826
127.420343	5022.958031	24.161843
127.772182	5011.625538	24.166861
127.727222	5025.914883	24.171879
127.929048	5031.730654	24.176896
127.961474	5047.395048	24.181914
127.968959	5055.566996	24.186931
127.941024	5043.742500	24.191949
128.379463	5066.063553	24.196967
128.229211	5068.965024	24.201984
128.748415	5085.627779	24.207002
128.359737	5078.913749	24.212019
128.723293	5096.389652	24.217037
129.021572	5117.103591	24.222055
129.131998	5113.759901	24.227072
129.207150	5114.753230	24.232090
129.234025	5113.637564	24.237107
129.571691	5137.495875	24.242125
129.384284	5159.699214	24.247143
129.584325	5147.814133	24.252160
129.618231	5157.728264	24.257178
129.961838	5157.599652	24.262195
130.531694	5157.795473	24.267213
130.269304	5167.966450	24.272231
130.820902	5162.024985	24.277248
130.835498	5160.379837	24.282266
130.905493	5171.421505	24.287283
131.160790	5178.818692	24.292301
130.759944	5180.009581	24.297319
131.363077	5191.336010	24.302336
131.472637	5198.554921	24.307354
131.865123	5205.053050	24.312371
131.829969	5185.669600	24.317389
131.740720	5204.879544	24.322407
131.820598	5189.466163	24.327424
131.976574	5200.024340	24.332442
131.881826	5217.678869	24.337459
132.252259	5217.411962	24.342477
131.976543	5241.071387	24.347495
132.180404	5226.909565	24.352512
132.206695	5240.072342	24.357530
132.218065	5259.897241	24.362547
132.655039	5252.884886	24.367565
132.768993	5279.916696	24.372583
132.736127	5282.258241	24.377600
133.268734	5287.565892	24.382618
133.434089	5291.885378	24.387635
133.618180	5287.271564	24.392653
133.765275	5282.905604	24.397671
133.549252	5270.967523	24.402688
134.103823	5287.007309	24.407706
134.043392	5299.543501	24.412723
134.155131	5297.086591	24.417741
134.112625	5313.396332	24.422759
134.207146	5295.890200	24.427776
134.352825	5312.803904	24.432794
134.196934	5325.834647	24.437811
134.691362	5320.751417	24.442829
134.609180	5328.613117	24.447847
135.003518	5347.304336	24.452864
135.332508	5363.598413	24.457882
134.958420	5356.122376	24.462899
135.288405	5365.488090	24.467917
135.477813	5363.981757	24.472935
135.669681	5377.883853	24.477952
135.945431	5390.657097	24.482970
135.813930	5389.372299	24.487987
135.683365	5380.930777	24.493005
136.303624	5400.778868	24.498023
136.671035	5404.785459	24.503040
136.833369	5422.298128	24.508058
136.907560	5410.403721	24.513075
136.906213	5410.591174	24.518093
137.068887	5408.775068	24.523111
137.124752	5434.532836	24.528128
137.384573	5429.986390	24.533146
137.147883	5447.442578	24.538163
137.370291	5454.618156	24.543181
137.554099	5459.049212	24.548199
137.380501	5479.132129	24.553216
137.878135	5475.902733	24.558234
137.818877	5475.498155	24.563251
138.275730	5510.461455	24.568269
138.210984	5510.398350	24.573287
138.264179	5524.575472	24.578304
138.539688	5513.484767	24.583322
138.387087	5537.788501	24.588339
138.742210	5536.184293	24.593357
139.129220	5533.785014	24.598375
139.066828	5545.462631	24.603392
139.211717	5545.721989	24.608410
139.264115	5551.857938	24.613427
139.543919	5565.833865	24.618445
139.703580	5553.916563	24.623463
139.681657	5579.859480	24.628480
140.132601	5587.746213	24.633498
140.112926	5578.072025	24.638515
140.407091	5582.728200	24.643533
140.591163	5582.300735	24.648551
141.181357	5610.416292	24.653568
141.300261	5595.834294	24.658586
141.172480	5614.420762	24.663603
141.069290	5611.373695	24.668621
141.194494	5611.802851	24.673639
141.275786	5624.231235	24.678656
141.499233	5609.111055	24.683674
141.355467	5620.026151	24.688691
141.910482	5630.330483	24.693709
142.181721	5634.965658	24.698727
141.969500	5650.097824	24.703744
142.356278	5635.942810	24.708762
142.329001	5643.527865	24.713779
142.400134	5635.311945	24.718797
142.472096	5629.985810	24.723815
142.576857	5658.519089	24.728832
142.788294	5657.453600	24.733850
142.638012	5672.499171	24.738867
143.047789	5678.352088	24.743885
142.992711	5669.698317	24.748903
142.972719	5686.654371	24.753920
143.387652	5707.658895	24.758938
143.591401	5712.182796	24.763955
143.485175	5715.009785	24.768973
143.886691	5733.063631	24.773991
143.993318	5734.853422	24.779008
144.036356	5747.520129	24.784026
144.075942	5740.223596	24.789043
144.338851	5768.328950	24.794061
144.575890	5746.335886	24.799079
144.533482	5759.304535	24.804096
144.910807	5782.760802	24.809114
144.970527	5793.434506	24.814131
145.149722	5784.457691	24.819149
145.213267	5778.172599	24.824167
145.386739	5812.310121	24.829184
145.701120	5808.992820	24.834202
145.909882	5814.855775	24.839219
146.042008	5810.224802	24.844237
146.427332	5813.274934	24.849255
146.237500	5827.963781	24.854272
146.721928	5832.343694	24.859290
146.704077	5836.807786	24.864307
146.556662	5843.358782	24.869325
146.926853	5847.652844	24.874343
146.865179	5837.189712	24.879360
147.091513	5861.080917	24.884378
146.784522	5871.815271	24.889395
147.171850	5882.037237	24.894413
147.275438	5888.116430	24.899431
147.293276	5903.246656	24.904448
147.528549	5916.464847	24.909466
147.772829	5938.361329	24.914483
147.597011	5936.598734	24.919501
147.996413	5950.215848	24.924519
148.045568	5972.752540	24.929536
148.526507	5975.411681	24.934554
148.835431	5981.329019	24.939571
148.728293	5997.013885	24.944589
148.890341	5989.146957	24.949607
149.274402	6000.498761	24.954624
149.332728	6000.210577	24.959642
149.752976	6021.797369	24.964659
149.444596	6028.249833	24.969677
150.040083	6012.995341	24.974695
149.782130	6049.564697	24.979712
150.142280	6040.379867	24.984730
150.310111	6051.818623	24.989747
150.345893	6061.448744	24.994765
150.606335	6044.194301	24.999783
150.643166	6079.663751	25.004800
150.943459	6087.182294	25.009818
151.261166	6086.177570	25.014835
151.353119	6089.157721	25.019853
151.419882	6082.784567	25.024871
151.249953	6107.813370	25.029888
151.523561	6095.487425	25.034906
151.763270	6115.707606	25.039923
151.472257	6121.674914	25.044941
151.865048	6137.032410	25.049959
152.016639	6140.866964	25.054976
152.110827	6149.711043	25.059994
152.318858	6160.840849	25.065011
152.577641	6176.242182	25.070029
152.961125	6166.634881	25.075047
152.904774	6188.129382	25.080064
153.129802	6175.580278	25.085082
153.020778	6210.704015	25.090099
153.307011	6199.506320	25.095117
153.872654	6208.598544	25.100135
153.535298	6213.177749	25.105152
153.621474	6216.461662	25.110170
154.287505	6216.495536	25.115187
154.004951	6217.454335	25.120205
154.601279	6225.346901	25.125223
154.386610	6228.059212	25.130240
154.647259	6226.285490	25.135258
154.569843	6248.600559	25.140275
154.699111	6252.136044	25.145293
154.799279	6267.231362	25.150311
155.017482	6265.664669	25.155328
155.153622	6283.664569	25.160346
155.306719	6278.844936	25.165363
155.278325	6312.197930	25.170381
155.690339	6302.590164	25.175399
155.836806	6323.761939	25.180416
156.014966	6337.898676	25.185434
156.168306	6335.739878	25.190451
156.474218	6354.215794	25.195469
156.202013	6369.788137	25.200487
156.699602	6373.089150	25.205504
156.859223	6374.014661	25.210522
157.152279	6395.863169	25.215539
157.143993	6392.532129	25.220557
157.655361	6388.516342	25.225575
157.959636	6386.831467	25.230592
157.781343	6392.469590	25.235610
158.204130	6404.340935	25.240627
158.528560	6414.699248	25.245645
158.978506	6414.608972	25.250663
158.971994	6409.384919	25.255680
159.151708	6409.691300	25.260698
159.247937	6409.866973	25.265715
159.317816	6416.637840	25.270733
159.865836	6413.871633	25.275751
159.550590	6400.878497	25.280768
159.698972	6412.775504	25.285786
159.931513	6397.309325	25.290803
159.626602	6423.993782	25.295821
159.860644	6422.518955	25.300839
160.097392	6436.718155	25.305856
159.986609	6431.922785	25.310874
160.482922	6430.955070	25.315891
160.354197	6459.563436	25.320909
160.677784	6454.459645	25.325927
160.683190	6473.918134	25.330944
160.762041	6479.695314	25.335962
160.940780	6493.281643	25.340979
161.032598	6508.276200	25.345997
161.203318	6497.173766	25.351015
161.102850	6527.301768	25.356032
161.057822	6541.683465	25.361050
161.725356	6551.287066	25.366067
161.521366	6566.510893	25.371085
161.744720	6586.496565	25.376103
162.022718	6598.961339	25.381120
162.424985	6612.277344	25.386138
162.359807	6618.278004	25.391155
162.398108	6640.363067	25.396173
162.599459	6636.118097	25.401191
163.191360	6652.680355	25.406208
163.360917	6668.061873	25.411226
163.547752	6677.041354	25.416243
163.169764	6683.189407	25.421261
163.684978	6678.796489	25.426279
163.778806	6693.778686	25.431296
163.855672	6704.478923	25.436314
164.083907	6702.082869	25.441331
164.012292	6732.028128	25.446349
164.217508	6734.848332	25.451367
164.541144	6754.560528	25.456384
165.036965	6767.755289	25.461402
165.164461	6751.820625	25.466419
165.067415	6785.372214	25.471437
165.233949	6795.290276	25.476455
165.451733	6795.495481	25.481472
165.385950	6809.588297	25.486490
165.568460	6808.855902	25.491507
165.638442	6821.854109	25.496525
165.975886	6844.093206	25.501543
166.400557	6852.824406	25.506560
166.298543	6858.178402	25.511578
166.665626	6871.396492	25.516595
166.722762	6878.022401	25.521613
167.394601	6883.689540	25.526631
167.703468	6885.919338	25.531648
168.041766	6899.375310	25.536666
167.951683	6900.046798	25.541683
167.967971	6905.410794	25.546701
168.160241	6907.119632	25.551719
168.663255	6897.631131	25.556736
168.580453	6903.219008	25.561754
168.681694	6901.551484	25.566771
168.345869	6925.932142	25.571789
169.289908	6932.562333	25.576807
169.136589	6931.602708	25.581824
169.041023	6931.171409	25.586842
169.144742	6957.486454	25.591859
168.997537	6954.758250	25.596877
169.709432	6972.790202	25.601895
170.079622	6980.514587	25.606912
169.930946	6993.727833	25.611930
170.042095	6994.593271	25.616947
170.364031	7010.679578	25.621965
170.420844	7025.611901	25.626983
170.501535	7029.565491	25.632000
170.457263	7038.013600	25.637018
170.758351	7062.404992	25.642035
170.928682	7062.911392	25.647053
171.299460	7077.083514	25.652071
171.314850	7101.830488	25.657088
171.742225	7090.219017	25.662106
172.017656	7119.836371	25.667123
171.764276	7118.968870	25.672141
171.722075	7130.499823	25.677159
172.172299	7144.553745	25.682176
172.965184	7145.156128	25.687194
173.391112	7143.557388	25.692212
173.071847	7152.403019	25.697229
173.351240	7157.838998	25.702247
173.668860	7172.181039	25.707264
173.506055	7172.349910	25.712282
173.495327	7173.034678	25.717300
173.825074	7181.124168	25.722317
173.734964	7212.134584	25.727335
174.370621	7205.521674	25.732352
174.047284	7217.025905	25.737370
174.360283	7213.491973	25.742388
174.373811	7233.405644	25.747405
174.453077	7229.632333	25.752423
174.437831	7242.265385	25.757440
174.681747	7280.087960	25.762458
175.160190	7262.403182	25.767476
175.550018	7280.103213	25.772493
175.517625	7291.444444	25.777511
175.586352	7285.618203	25.782528
175.591839	7303.043131	25.787546
175.942494	7329.220342	25.792564
176.002842	7334.335039	25.797581
176.506311	7350.189304	25.802599
176.855241	7349.318345	25.807616
176.518233	7365.420181	25.812634
176.848411	7365.529646	25.817652
177.213002	7376.178467	25.822669
177.215627	7378.162829	25.827687
177.356374	7400.696284	25.832704
177.820853	7410.081172	25.837722
178.471930	7416.652089	25.842740
178.438155	7408.236791	25.847757
178.414180	7416.392725	25.852775
178.611080	7420.675303	25.857792
178.752030	7430.781490	25.862810
179.211102	7445.973784	25.867828
178.895183	7441.757762	25.872845
178.744764	7454.570827	25.877863
179.607813	7473.953814	25.882880
179.266228	7478.800268	25.887898
179.788017	7498.491686	25.892916
179.901105	7505.997351	25.897933
180.115683	7510.930689	25.902951
180.475112	7519.841577	25.907968
180.530854	7530.024124	25.912986
181.101140	7545.461964	25.918004
181.110954	7530.810745	25.923021
181.078967	7546.481197	25.928039
181.417660	7542.315277	25.933056
181.425859	7569.826079	25.938074
181.817443	7568.141618	25.943092
181.602830	7582.040388	25.948109
181.969275	7599.305196	25.953127
182.016039	7591.990077	25.958144
182.047781	7613.336909	25.963162
182.291402	7610.474315	25.968180
182.611990	7643.633079	25.973197
182.679071	7631.850780	25.978215
183.423770	7636.316967	25.983232
183.817798	7655.020060	25.988250
184.028642	7641.215210	25.993268
183.759604	7654.314228	25.998285
183.524790	7650.809288	26.003303
184.032539	7673.291944	26.008320
183.965114	7684.597507	26.013338
184.120512	7679.519932	26.018356
184.468886	7705.194118	26.023373
184.569723	7717.072014	26.028391
184.923725	7708.064036	26.033408
184.844805	7737.743470	26.038426
185.053032	7734.125141	26.043444
185.016288	7754.291131	26.048461
185.293817	7779.328991	26.053479
185.797539	7769.324401	26.058496
185.458407	7794.837477	26.063514
186.097383	7806.390255	26.068532
186.036869	7809.616837	26.073549
186.096304	7837.333854	26.078567
186.241437	7832.977751	26.083584
186.518031	7856.884172	26.088602
186.781364	7871.854842	26.093620
187.254607	7879.805213	26.098637
187.377788	7879.682692	26.103655
187.422913	7903.402977	26.108672
187.601648	7900.453395	26.113690
188.037676	7914.073261	26.118708
188.278662	7926.540090	26.123725
188.198578	7929.272192	26.128743
188.841010	7931.616352	26.133760
188.989319	7942.231204	26.138778
189.025924	7955.253979	26.143796
189.415063	7962.406313	26.148813
189.151238	7964.562360	26.153831
189.653328	7972.359950	26.158848
189.419993	7984.624039	26.163866
189.819573	7986.324732	26.168884
189.878812	8002.378282	26.173901
190.197353	8029.410961	26.178919
190.368844	8023.086266	26.183936
190.440974	8029.816898	26.188954
190.634940	8049.092212	26.193972
190.805575	8063.842900	26.198989
190.720259	8072.905560	26.204007
191.062997	8088.638281	26.209024
190.937499	8112.804485	26.214042
191.383191	8115.622221	26.219060
191.584260	8130.997210	26.224077
191.890966	8157.783980	26.229095
192.327698	8161.261613	26.234112
192.487231	8183.266201	26.239130
192.486733	8182.007171	26.244148
192.988102	8194.739917	26.249165
192.841947	8199.798446	26.254183
193.253311	8210.453496	26.259200
193.386132	8225.240511	26.264218
193.620710	8247.589559	26.269236
194.081668	8248.661894	26.274253
194.073965	8270.123243	26.279271
194.486675	8271.885592	26.284288
194.253540	8274.265006	26.289306
194.807485	8296.351859	26.294324
195.078256	8302.944251	26.299341
195.198772	8305.751170	26.304359
195.333585	8320.872666	26.309376
195.342402	8317.143027	26.314394
195.500571	8345.366788	26.319412
195.998825	8344.011946	26.324429
196.021241	8372.475558	26.329447
196.467042	8358.560377	26.334464
196.670712	8374.789700	26.339482
196.783350	8391.449137	26.344500
197.091756	8403.551580	26.349517
197.093424	8401.722752	26.354535
197.065310	8412.478121	26.359552
197.699104	8420.625913	26.364570
197.852359	8424.236292	26.369588
198.137800	8431.260273	26.374605
198.326046	8443.905558	26.379623
198.576463	8458.057469	26.384640
198.529566	8462.339661	26.389658
198.542206	8449.309549	26.394676
199.096456	8479.886779	26.399693
199.105015	8486.439878	26.404711
199.547025	8491.519454	26.409728
199.673762	8496.550313	26.414746
199.628100	8505.659437	26.419764
199.937789	8515.347798	26.424781
199.699194	8523.438168	26.429799
199.965824	8527.385040	26.434816
200.050264	8544.342281	26.439834
200.055566	8557.265188	26.444852
200.554917	8576.599375	26.449869
200.329423	8584.936491	26.454887
200.740211	8614.039686	26.459904
201.161118	8623.823937	26.464922
200.960456	8627.874038	26.469940
201.312953	8647.676780	26.474957
201.634248	8667.541410	26.479975
201.905538	8679.107545	26.484992
202.026349	8688.014420	26.490010
202.135831	8708.664680	26.495028
202.349869	8714.140354	26.500045
202.654174	8745.872276	26.505063
203.029855	8760.702363	26.510080
203.496716	8772.012572	26.515098
203.297722	8780.390305	26.520116
204.094677	8772.338718	26.525133
203.641437	8784.055361	26.530151
203.944076	8810.339847	26.535168
204.361793	8817.472886	26.540186
204.467256	8838.631985	26.545204
205.008691	8837.134501	26.550221
204.915532	8858.865954	26.555239
205.600925	8857.950351	26.560256
205.804127	8857.519250	26.565274
205.720767	8878.441816	26.570292
206.153674	8872.934442	26.575309
206.202003	8896.436735	26.580327
206.575309	8890.312268	26.585344
206.789709	8897.640398	26.590362
206.864821	8929.375117	26.595380
207.429975	8923.694653	26.600397
207.056549	8926.131211	26.605415
207.409880	8947.562180	26.610432
207.613807	8955.446545	26.615450
207.580143	8955.945367	26.620468
207.853488	8964.572010	26.625485
208.023496	8994.180382	26.630503
208.593258	8986.948326	26.635520
209.035244	9012.202769	26.640538
208.913430	9013.062707	26.645556
209.188347	9014.206794	26.650573
209.074400	9033.135655	26.655591
209.648157	9038.837909	26.660608
209.987897	9051.997379	26.665626
209.682280	9057.287308	26.670644
210.044085	9053.603924	26.675661
210.431472	9080.871978	26.680679
210.492880	9068.926510	26.685696
210.785241	9101.551914	26.690714
210.972683	9109.533594	26.695732
211.224913	9122.086151	26.700749
211.238485	9130.934596	26.705767
211.187086	9136.289664	26.710784
211.577141	9161.912868	26.715802
211.538579	9175.255453	26.720820
211.943015	9179.249819	26.725837
211.709835	9202.558856	26.730855
212.034228	9216.324317	26.735872
212.615251	9234.963737	26.740890
212.703987	9246.858173	26.745908
212.900316	9274.720495	26.750925
212.903316	9280.444683	26.755943
212.967865	9307.449845	26.760960
213.483289	9305.046120	26.765978
213.863935	9345.731414	26.770996
214.072532	9338.097325	26.776013
214.491086	9371.280554	26.781031
214.342849	9371.648670	26.786048
214.613949	9384.013223	26.791066
214.510996	9414.994642	26.796084
215.026828	9403.682707	26.801101
215.167383	9432.304348	26.806119
215.343824	9436.703489	26.811136
215.952143	9452.448038	26.816154
215.925582	9467.227895	26.821172
216.458043	9475.235454	26.826189
216.370799	9488.475289	26.831207
216.865477	9502.205775	26.836224
217.002029	9502.276369	26.841242
217.048499	9527.644244	26.846260
217.335818	9521.822019	26.851277
217.397580	9551.938443	26.856295
217.906069	9555.913350	26.861312
218.320200	9565.343295	26.866330
218.327119	9580.286280	26.871348
218.824023	9582.356229	26.876365
218.796274	9583.939463	26.881383
219.167039	9615.206891	26.886400
219.481150	9621.921850	26.891418
219.258322	9624.584886	26.896436
219.665389	9632.280072	26.901453
219.764364	9648.130241	26.906471
219.946580	9657.825402	26.911488
220.421489	9679.827223	26.916506
220.381236	9682.328565	26.921524
220.653330	9703.732238	26.926541
220.559817	9715.300335	26.931559
220.852127	9736.384864	26.936576
221.003460	9746.291546	26.941594
221.553843	9773.114832	26.946612
221.917818	9782.456313	26.951629
221.960966	9807.435297	26.956647
222.233046	9814.028107	26.961664
222.381176	9824.640317	26.966682
222.747850	9843.295393	26.971700
222.981628	9849.533801	26.976717
223.176488	9880.439353	26.981735
223.718218	9871.566906	26.986752
223.455654	9880.186503	26.991770
223.446797	9902.759276	26.996788
224.153136	9918.722030	27.001805
224.362091	9935.453033	27.006823
224.390473	9953.452091	27.011840
225.031164	9972.846553	27.016858
224.816700	9981.172337	27.021876
225.046916	9984.835735	27.026893
225.169681	10003.572259	27.031911
225.158829	10018.639105	27.036928
225.619702	10021.568894	27.041946
225.205893	10058.804991	27.046964
225.971809	10057.739759	27.051981
226.417837	10090.344959	27.056999
226.483596	10094.467985	27.062016
227.147648	10140.222025	27.067034
227.481105	10146.683532	27.072052
227.628126	10148.932669	27.077069
228.053658	10150.697845	27.082087
228.047668	10171.002036	27.087104
228.200707	10166.687311	27.092122
228.105816	10194.056660	27.097140
228.761323	10190.387504	27.102157
228.865991	10207.352635	27.107175
228.953386	10227.516228	27.112192
229.196139	10243.303065	27.117210
229.426376	10243.114005	27.122228
229.473064	10262.094980	27.127245
229.845232	10273.566847	27.132263
229.700840	10296.965214	27.137280
230.258442	10307.472282	27.142298
230.411517	10320.654986	27.147316
230.640484	10329.094363	27.152333
231.050636	10331.998721	27.157351
230.810600	10357.998930	27.162368
231.651310	10372.078654	27.167386
231.467751	10398.979370	27.172404
231.800807	10399.998953	27.177421
232.092378	10421.915520	27.182439
232.454399	10430.583451	27.187456
232.492843	10442.434318	27.192474
232.833211	10472.582858	27.197492
232.982248	10468.594028	27.202509
233.454572	10489.306384	27.207527
233.291436	10500.097292	27.212544
233.768290	10516.979990	27.217562
233.940839	10532.252538	27.222580
234.313391	10542.201147	27.227597
234.780140	10562.431666	27.232615
235.062599	10570.721337	27.237632
235.361737	10566.503670	27.242650
235.347726	10587.632066	27.247668
235.586023	10599.654041	27.252685
235.849360	10614.741527	27.257703
235.827635	10632.880389	27.262720
236.157064	10638.451094	27.267738
236.204952	10672.051963	27.272756
236.591014	10685.948723	27.277773
236.730552	10697.953219	27.282791
236.603620	10720.575805	27.287808
237.230117	10741.447338	27.292826
237.498358	10760.117393	27.297844
237.870814	10756.182950	27.302861
238.435561	10777.445980	27.307879
238.755845	10781.244344	27.312896
239.296090	10798.471334	27.317914
239.019054	10798.986793	27.322932
239.339258	10806.577174	27.327949
239.531582	10825.721443	27.332967
239.503286	10834.988149	27.337984
240.182702	10847.493546	27.343002
240.169261	10859.622692	27.348020
240.230123	10880.269633	27.353037
240.430006	10886.366749	27.358055
240.809510	10916.118961	27.363072
240.889435	10911.871256	27.368090
241.258690	10934.497234	27.373108
241.418885	10953.342122	27.378125
241.381124	10960.037806	27.383143
241.466786	10991.295184	27.388160
242.132660	11004.227519	27.393178
242.117206	11014.618635	27.398196
242.270383	11033.089038	27.403213
242.925543	11057.314273	27.408231
242.968631	11091.809299	27.413248
243.049779	11104.218395	27.418266
243.708268	11122.447080	27.423284
243.833254	11145.660394	27.428301
244.118377	11149.776594	27.433319
244.208324	11185.553577	27.438336
244.485853	11192.880217	27.443354
244.586646	11193.556186	27.448372
244.567337	11220.317714	27.453389
244.919449	11225.851795	27.458407
244.958530	11245.040005	27.463424
245.507240	11275.959908	27.468442
245.733387	11282.160755	27.473460
245.610288	11310.295259	27.478477
246.368548	11318.737511	27.483495
246.324680	11341.546546	27.488512
247.081748	11364.723487	27.493530
247.234382	11375.728277	27.498548
247.537904	11385.164979	27.503565
247.999464	11388.425761	27.508583
247.805273	11411.943483	27.513600
248.309113	11420.552288	27.518618
248.548448	11443.476950	27.523636
248.790378	11461.512535	27.528653
249.353005	11455.250256	27.533671
249.537553	11485.876255	27.538688
249.904065	11493.700361	27.543706
249.942472	11502.423923	27.548724
249.512452	11515.469211	27.553741
249.939773	11518.758521	27.558759
250.189533	11557.324516	27.563776
250.709283	11571.038475	27.568794
250.967884	11587.754347	27.573812
251.123354	11600.051506	27.578829
251.335166	11628.942607	27.583847
251.241384	11643.607185	27.588864
252.158226	11669.027660	27.593882
252.183839	11674.318864	27.598900
252.561597	11704.366663	27.603917
252.852899	11721.961125	27.608935
252.640767	11745.370441	27.613952
253.071181	11746.377969	27.618970
253.437193	11770.611101	27.623988
253.739189	11786.844999	27.629005
254.105039	11803.506352	27.634023
254.036835	11806.699564	27.639040
254.458660	11831.896440	27.644058
254.926050	11846.617371	27.649076
254.932770	11875.109538	27.654093
255.400420	11886.566795	27.659111
255.485176	11906.124798	27.664128
255.627973	11924.546743	27.669146
256.137203	11938.907143	27.674164
256.062869	11983.619445	27.679181
256.777885	11987.287498	27.684199
256.814783	12010.745860	27.689216
257.260536	12021.400164	27.694234
257.687128	12047.525364	27.699252
257.641369	12055.005075	27.704269
257.697612	12068.300542	27.709287
258.048185	12075.412278	27.714304
258.627351	12105.890761	27.719322
258.860931	12116.017719	27.724340
258.964230	12143.386806	27.729357
259.291428	12154.641373	27.734375
259.491411	12160.303326	27.739392
259.302086	12183.291994	27.744410
260.032435	12204.279845	27.749428
259.968027	12233.791173	27.754445
260.268752	12241.917205	27.759463
260.435543	12274.414667	27.764480
260.801226	12288.321708	27.769498
261.102150	12301.413871	27.774516
260.976570	12320.685720	27.779533
261.635309	12330.188762	27.784551
261.613352	12349.951640	27.789568
261.810417	12381.740833	27.794586
262.536414	12384.607570	27.799604
262.590111	12419.795373	27.804621
263.003201	12429.380026	27.809639
263.535731	12447.089834	27.814656
263.396072	12459.766496	27.819674
264.150311	12465.010839	27.824692
264.131929	12487.815718	27.829709
264.404848	12500.105192	27.834727
264.680888	12515.007246	27.839744
264.747254	12528.926924	27.844762
265.303214	12540.825402	27.849780
265.313947	12570.900018	27.854797
265.462850	12571.786315	27.859815
265.710884	12601.676829	27.864832
265.605241	12611.799489	27.869850
266.273001	12655.216454	27.874868
266.442360	12664.843881	27.879885
266.338782	12683.008042	27.884903
267.023130	12718.051336	27.889920
267.177409	12727.390596	27.894938
267.915630	12757.729809	27.899956
267.862888	12771.637077	27.904973
268.132207	12798.166842	27.909991
268.444740	12802.467227	27.915008
268.818093	12828.557593	27.920026
269.300544	12843.022494	27.925044
269.407313	12873.602546	27.930061
269.659615	12874.217317	27.935079
270.091902	12896.871110	27.940096
269.817170	12920.145946	27.945114
270.490328	12933.388258	27.950132
270.785199	12955.999451	27.955149
271.293693	12961.015920	27.960167
271.731254	12986.216740	27.965184
271.693865	13007.180446	27.970202
272.092954	13009.607355	27.975220
271.792723	13039.914634	27.980237
272.372235	13061.487880	27.985255
272.572389	13090.533225	27.990272
272.810650	13094.715184	27.995290
273.228452	13111.560755	28.000308
273.214171	13140.120872	28.005325
273.567747	13149.753606	28.010343
273.675215	13184.385877	28.015360
273.996379	13206.265921	28.020378
274.272231	13225.147945	28.025396
274.137186	13259.385568	28.030413
274.645101	13276.785233	28.035431
275.213036	13309.691205	28.040448
275.691790	13322.605135	28.045466
276.090160	13353.745334	28.050484
276.407420	13368.780816	28.055501
276.640068	13385.943248	28.060519
276.771881	13393.268978	28.065536
276.846633	13415.396430	28.070554
277.332843	13435.533623	28.075572
277.452174	13454.751395	28.080589
278.221171	13478.907134	28.085607
278.303851	13486.311141	28.090624
278.399790	13525.013634	28.095642
279.068766	13530.282663	28.100660
279.094285	13564.927716	28.105677
279.893892	13565.539539	28.110695
280.101570	13571.868807	28.115712
280.190947	13607.429109	28.120730
280.483972	13607.967064	28.125748
280.546445	13622.848707	28.130765
280.881191	13627.841309	28.135783
281.398215	13632.109710	28.140800
281.364065	13661.249944	28.145818
281.536858	13659.315820	28.150836
281.631688	13687.093096	28.155853
281.893734	13703.452924	28.160871
282.434652	13730.572780	28.165888
282.230999	13738.845933	28.170906
282.818410	13764.465984	28.175924
282.714868	13794.531826	28.180941
283.048894	13808.122398	28.185959
283.653405	13837.522993	28.190976
283.570415	13852.885835	28.195994
283.984451	13887.450056	28.201012
283.944903	13905.936700	28.206029
284.109038	13921.911121	28.211047
284.486826	13945.646880	28.216064
284.427562	13992.090034	28.221082
285.234790	14014.708667	28.226100
285.625377	14040.919481	28.231117
286.133635	14069.186125	28.236135
286.342616	14087.118228	28.241152
286.656152	14106.711227	28.246170
287.273793	14138.421794	28.251188
287.378188	14151.872538	28.256205
287.201391	14182.646101	28.261223
287.863775	14191.255423	28.266240
288.468363	14232.536203	28.271258
288.746613	14241.599802	28.276276
289.057252	14259.044154	28.281293
289.277143	14295.086280	28.286311
289.785829	14295.749355	28.291328
290.241748	14334.388796	28.296346
290.401544	14330.454751	28.301364
290.529512	14363.573445	28.306381
290.843222	14378.604942	28.311399
291.234651	14381.376844	28.316416
291.393349	14421.562566	28.321434
291.628291	14414.535478	28.326452
291.697011	14451.241111	28.331469
291.807738	14466.912894	28.336487
292.261290	14484.729394	28.341504
292.422331	14514.663040	28.346522
293.054293	14536.520329	28.351540
293.058108	14566.071923	28.356557
293.342129	14589.384479	28.361575
293.803786	14622.220083	28.366592
293.818447	14649.064425	28.371610
294.084263	14671.075361	28.376628
294.474616	14691.608150	28.381645
294.978303	14724.290469	28.386663
295.534625	14736.118033	28.391680
295.659377	14781.458360	28.396698
296.017133	14773.180132	28.401716
296.527326	14797.128484	28.406733
296.576928	14820.669199	28.411751
296.922638	14836.072450	28.416768
296.877584	14871.357550	28.421786
297.213665	14887.785137	28.426804
297.262025	14909.217760	28.431821
297.718745	14936.303127	28.436839
298.315022	14956.238091	28.441856
298.547608	15004.827881	28.446874
298.991427	15002.466687	28.451892
299.415785	15029.752958	28.456909
299.735394	15031.403827	28.461927
299.995357	15057.351072	28.466944
300.114627	15069.663955	28.471962
300.635015	15097.977669	28.476980
300.653734	15117.396834	28.481997
300.830003	15133.688764	28.487015
300.985733	15153.328013	28.492032
301.203716	15167.228855	28.497050
301.540388	15201.608535	28.502068
301.923696	15223.427468	28.507085
302.068049	15253.762346	28.512103
302.306789	15282.981749	28.517120
302.465201	15307.179652	28.522138
302.942061	15315.583854	28.527156
303.231337	15363.363245	28.532173
303.252713	15377.641861	28.537191
303.785680	15408.937126	28.542208
303.906789	15444.485975	28.547226
304.139452	15478.128589	28.552244
304.420633	15503.381238	28.557261
305.165486	15541.969519	28.562279
306.123756	15567.015849	28.567296
306.153112	15570.320540	28.572314
306.697277	15595.838755	28.577332
307.118332	15618.104258	28.582349
307.153399	15628.718500	28.587367
308.187268	15648.736457	28.592384
308.189679	15647.535456	28.597402
308.328376	15676.713788	28.602420
308.575708	15691.811051	28.607437
308.757227	15713.410264	28.612455
308.963178	15727.201686	28.617472
308.668180	15759.540554	28.622490
309.038830	15783.166723	28.627508
309.605035	15812.974363	28.632525
309.872326	15851.465780	28.637543
310.374220	15869.540570	28.642560
310.433278	15911.164748	28.647578
310.797388	15931.296861	28.652596
311.217037	15959.222139	28.657613
311.617732	15987.136412	28.662631
312.001362	16010.100460	28.667648
312.627055	16021.301325	28.672666
312.937028	16062.971111	28.677684
313.145953	16055.823120	28.682701
313.501570	16094.740200	28.687719
313.888835	16113.798664	28.692736
314.181456	16140.900545	28.697754
314.246655	16169.392192	28.702772
314.603348	16174.598651	28.707789
314.611528	16212.065250	28.712807
315.032413	16231.907839	28.717824
315.342935	16254.077432	28.722842
315.648626	16286.280277	28.727860
315.716008	16305.081354	28.732877
315.927956	16352.739316	28.737895
316.366988	16374.621506	28.742912
316.619134	16410.060983	28.747930
316.681901	16437.609504	28.752948
317.351888	16471.435646	28.757965
317.144512	16505.717275	28.762983
317.982580	16528.307542	28.768000
318.622364	16566.241101	28.773018
319.027249	16591.506520	28.778036
319.470117	16607.111308	28.783053
319.386148	16633.671054	28.788071
320.271588	16665.435303	28.793088
320.248033	16688.891518	28.798106
320.733048	16703.058447	28.803124
321.158751	16725.521695	28.808141
321.336342	16731.864264	28.813159
321.563785	16753.343797	28.818176
321.760106	16777.280735	28.823194
322.015183	16793.127909	28.828212
322.251964	16820.733430	28.833229
322.323417	16837.520331	28.838247
322.563450	16870.416004	28.843264
323.076932	16890.466313	28.848282
323.114087	16932.404031	28.853300
323.519446	16952.019966	28.858317
323.881812	16988.249400	28.863335
324.044634	17015.856437	28.868352
324.425091	17044.951568	28.873370
324.607349	17078.867429	28.878388
325.180414	17112.094691	28.883405
325.678226	17134.510340	28.888423
325.938662	17163.638119	28.893440
326.259883	17193.255508	28.898458
326.723195	17212.077320	28.903476
327.235943	17253.056286	28.908493
327.296112	17288.540415	28.913511
327.996017	17291.950589	28.918528
328.048051	17342.953836	28.923546
328.483450	17371.509345	28.928564
329.249800	17376.260805	28.933581
329.362806	17412.786119	28.938599
329.578956	17436.708137	28.943616
330.026097	17452.587262	28.948634
330.114048	17481.419436	28.953652
330.767211	17513.045618	28.958669
330.841224	17532.185860	28.963687
331.222236	17557.113135	28.968704
331.445042	17593.461529	28.973722
331.893674	17603.578463	28.978740
332.241284	17642.401259	28.983757
332.322653	17664.126770	28.988775
332.698970	17702.238884	28.993792
333.219669	17728.007031	28.998810
333.519855	17753.280510	29.003828
333.828889	17782.229567	29.008845
334.019956	17812.715935	29.013863
334.676862	17850.986930	29.018880
334.749422	17877.759241	29.023898
334.742494	17903.641627	29.028916
335.485012	17932.892868	29.033933
335.544059	17959.546186	29.038951
336.054056	17994.839318	29.043968
336.724089	18006.529125	29.048986
337.362888	18037.131072	29.054004
338.026407	18052.631441	29.059021
337.756440	18085.126791	29.064039
338.177647	18109.362656	29.069056
338.562478	18124.858700	29.074074
339.003741	18149.044027	29.079092
339.503619	18169.991812	29.084109
339.517898	18186.890411	29.089127
340.043181	18198.563292	29.094144
340.337890	18235.027316	29.099162
340.454265	18244.909533	29.104180
340.950146	18271.919894	29.109197
341.238652	18299.107989	29.114215
341.638598	18340.724577	29.119232
341.963225	18352.618278	29.124250
341.926605	18392.037482	29.129268
342.266952	18405.339270	29.134285
342.731862	18444.160343	29.139303
343.394682	18459.635995	29.144320
343.609769	18475.619072	29.149338
343.875925	18507.620036	29.154356
343.995264	18529.619396	29.159373
344.284240	18564.086534	29.164391
344.750647	18572.869279	29.169408
345.093233	18605.138361	29.174426
345.231476	18628.830681	29.179444
345.732440	18653.430876	29.184461
346.055828	18682.700686	29.189479
346.001908	18710.174576	29.194496
346.388529	18736.555946	29.199514
346.478765	18783.016387	29.204532
346.807478	18803.263488	29.209549
346.845444	18858.513681	29.214567
347.309361	18886.567464	29.219584
347.576597	18929.714300	29.224602
347.841636	18973.318709	29.229620
348.735263	19013.512516	29.234637
348.847812	19038.142779	29.239655
349.067389	19087.407264	29.244672
349.341040	19100.882984	29.249690
349.961714	19158.704858	29.254708
350.176565	19187.351975	29.259725
350.579340	19230.625369	29.264743
351.155519	19262.630171	29.269760
351.817287	19303.860741	29.274778
352.325652	19332.926184	29.279796
352.963844	19358.634919	29.284813
353.029176	19408.349850	29.289831
353.349422	19431.705887	29.294848
354.007968	19461.388274	29.299866
353.876505	19481.013956	29.304884
354.079042	19518.268405	29.309901
354.846781	19555.265632	29.314919
355.158905	19579.119739	29.319936
355.761702	19611.213818	29.324954
355.723275	19643.948247	29.329972
356.525847	19673.845238	29.334989
356.983377	19699.644250	29.340007
357.014222	19734.875253	29.345024
357.449254	19754.688245	29.350042
357.559025	19778.907087	29.355060
358.003062	19812.063397	29.360077
358.417546	19836.829391	29.365095
358.866886	19888.616605	29.370112
359.524376	19913.865895	29.375130
359.854106	19932.931999	29.380148
360.127120	19952.191921	29.385165
360.414560	19990.628234	29.390183
360.556837	20004.399094	29.395200
360.963558	20047.324037	29.400218
360.876776	20078.598201	29.405236
361.475405	20103.628942	29.410253
362.005097	20148.966069	29.415271
362.298280	20177.748556	29.420288
362.711462	20220.311904	29.425306
362.568748	20252.344385	29.430324
363.353740	20292.322806	29.435341
363.376026	20313.382169	29.440359
363.724941	20357.040995	29.445376
364.098469	20388.638508	29.450394
364.500884	20425.009178	29.455412
365.025404	20469.577209	29.460429
365.549960	20517.446216	29.465447
366.064126	20535.713288	29.470464
366.654753	20583.276793	29.475482
366.955822	20592.778376	29.480500
367.125866	20624.684240	29.485517
367.469617	20645.843822	29.490535
368.058941	20674.152631	29.495552
368.731536	20679.286274	29.500570
368.696986	20717.801111	29.505588
369.203086	20743.994122	29.510605
369.597589	20772.891741	29.515623
369.645520	20800.604486	29.520640
370.066641	20815.838540	29.525658
369.919061	20853.639351	29.530676
370.321190	20879.766204	29.535693
370.677304	20922.284029	29.540711
370.925986	20951.292750	29.545728
371.594961	20986.999518	29.550746
371.738180	21028.739370	29.555764
372.045935	21066.449676	29.560781
372.535775	21117.294498	29.565799
372.799814	21149.228402	29.570816
373.186222	21184.655961	29.575834
373.556839	21223.891658	29.580852
373.820269	21265.213410	29.585869
374.354282	21297.202311	29.590887
374.634725	21343.567559	29.595904
375.618814	21368.126660	29.600922
375.893329	21406.232603	29.605940
376.442662	21441.526596	29.610957
376.979682	21466.738251	29.615975
377.073351	21486.633355	29.620992
377.526810	21527.314283	29.626010
377.840928	21554.602808	29.631028
378.320773	21597.146054	29.636045
378.916276	21615.035143	29.641063
379.281013	21671.505019	29.646080
379.871197	21674.623697	29.651098
379.996747	21725.901025	29.656116
380.741842	21736.078726	29.661133
380.960573	21768.494238	29.666151
381.105444	21791.776946	29.671168
381.499523	21818.168296	29.676186
381.985314	21854.274505	29.681204
382.113636	21880.596352	29.686221
382.617107	21926.007290	29.691239
382.451161	21946.267432	29.696256
383.164304	21991.938713	29.701274
383.575022	22021.073868	29.706292
383.847167	22066.783524	29.711309
384.321611	22091.828320	29.716327
384.494853	22136.165616	29.721344
385.227104	22155.613921	29.726362
385.479823	22207.765592	29.731380
385.843383	22230.271826	29.736397
386.222499	22271.048826	29.741415
386.452924	22306.520301	29.746432
386.979622	22338.956985	29.751450
387.772981	22374.906305	29.756468
387.904537	22396.175687	29.761485
388.428263	22423.063673	29.766503
388.388046	22472.716901	29.771520
388.992511	22501.838228	29.776538
389.376656	22555.129595	29.781556
389.657658	22583.602943	29.786573
390.275250	22619.830921	29.791591
390.130038	22656.095130	29.796608
390.740036	22687.542848	29.801626
391.208642	22744.459536	29.806644
391.437813	22767.628775	29.811661
392.117309	22799.345849	29.816679
392.286373	22851.943743	29.821696
392.420509	22882.883959	29.826714
392.650047	22925.144009	29.831732
392.949921	22965.915295	29.836749
393.543647	23013.888819	29.841767
393.925086	23047.183306	29.846784
394.601134	23088.770903	29.851802
395.103833	23123.596870	29.856820
395.269652	23155.724255	29.861837
396.054634	23193.570206	29.866855
396.089619	23231.171217	29.871872
396.593166	23257.371750	29.876890
396.763304	23294.458677	29.881908
397.440841	23339.398511	29.886925
398.055799	23365.768425	29.891943
398.520380	23399.114515	29.896960
398.671007	23444.524794	29.901978
398.942966	23471.713045	29.906996
399.265959	23520.117436	29.912013
399.783454	23543.566476	29.917031
400.296699	23583.838907	29.922048
400.761130	23616.942653	29.927066
401.154677	23637.188082	29.932084
401.389968	23691.034239	29.937101
401.916438	23727.088887	29.942119
402.287567	23759.904036	29.947136
402.626712	23809.080724	29.952154
402.888122	23837.091167	29.957172
403.421252	23881.906526	29.962189
403.532171	23904.120914	29.967207
404.042766	23971.425025	29.972224
404.606614	24002.446094	29.977242
404.925761	24038.967668	29.982260
405.133902	24097.864968	29.987277
405.408605	24122.669876	29.992295
406.114240	24165.820895	29.997312
406.638082	24222.810718	30.002330
407.114643	24258.327637	30.007348
407.316327	24311.520690	30.012365
407.893383	24343.150387	30.017383
408.132000	24392.611845	30.022400
408.693503	24429.923577	30.027418
409.311202	24470.575049	30.032436
409.606659	24516.812559	30.037453
410.170837	24541.294336	30.042471
410.319355	24600.300993	30.047488
411.129072	24616.434544	30.052506
411.518205	24669.760161	30.057524
411.956377	24715.071170	30.062541
412.559415	24743.296302	30.067559
412.830584	24773.635533	30.072576
413.514204	24816.173769	30.077594
413.749551	24853.833592	30.082612
414.069524	24888.813228	30.087629
414.454864	24914.357864	30.092647
415.035133	24962.241401	30.097664
415.279118	24976.275482	30.102682
415.610312	25030.196784	30.107700
415.649553	25065.674117	30.112717
416.359934	25095.793152	30.117735
416.555678	25147.465074	30.122752
416.982988	25185.615836	30.127770
417.615891	25218.453646	30.132788
417.717262	25271.921726	30.137805
418.349865	25315.761037	30.142823
418.388669	25353.657845	30.147840
418.921863	25397.978946	30.152858
419.203260	25439.194456	30.157876
419.732907	25502.471198	30.162893
420.311901	25525.323107	30.167911
420.757057	25583.090533	30.172928
421.070669	25616.869609	30.177946
421.718060	25651.101351	30.182964
421.916833	25676.632229	30.187981
422.662892	25717.905685	30.192999
422.911130	25759.058068	30.198016
423.127042	25789.610080	30.203034
423.626972	25830.686367	30.208052
423.649948	25870.047096	30.213069
424.492481	25905.883880	30.218087
424.619568	25953.461906	30.223104
424.963490	26002.664675	30.228122
426.312694	26019.334885	30.233140
426.542116	26069.039280	30.238157
426.892657	26100.872100	30.243175
427.361302	26145.442345	30.248192
427.606606	26189.614384	30.253210
428.501546	26201.985570	30.258228
428.611120	26253.421211	30.263245
428.837017	26272.371335	30.268263
429.392169	26313.507473	30.273280
429.885002	26358.657729	30.278298
430.544801	26390.758535	30.283316
430.696465	26425.065845	30.288333
431.315809	26462.877104	30.293351
431.516629	26516.793122	30.298368
431.794187	26543.096006	30.303386
432.279118	26600.710509	30.308404
432.572391	26647.930291	30.313421
432.977636	26697.216397	30.318439
433.268002	26734.466028	30.323456
433.698397	26790.216793	30.328474
434.310331	26842.307648	30.333492
434.489691	26895.361091	30.338509
435.026963	26954.354271	30.343527
435.375032	26991.399389	30.348544
435.800438	27046.891619	30.353562
436.578698	27074.460905	30.358580
436.601175	27146.051361	30.363597
437.118963	27193.363296	30.368615
437.489079	27248.130446	30.373632
438.003900	27284.287626	30.378650
438.568005	27335.550511	30.383668
439.125547	27382.064756	30.388685
439.624567	27444.566852	30.393703
440.257950	27481.928609	30.398720
440.575574	27528.060250	30.403738
441.474041	27578.328737	30.408756
441.613047	27612.984308	30.413773
442.040943	27645.400184	30.418791
442.481118	27702.983215	30.423808
442.619437	27758.969897	30.428826
443.352114	27781.690637	30.433844
443.659241	27843.737012	30.438861
443.979069	27881.747554	30.443879
444.570965	27929.437230	30.448896
444.752605	27985.925301	30.453914
445.754922	28020.741873	30.458932
445.677482	28088.608868	30.463949
446.423239	28118.052435	30.468967
446.734258	28165.265584	30.473984
446.974119	28212.462230	30.479002
447.596777	28258.769389	30.484020
447.923687	28293.890491	30.489037
448.850271	28346.673590	30.494055
449.445336	28387.033781	30.499072
450.186458	28427.199615	30.504090
450.858637	28450.416979	30.509108
451.353535	28499.732888	30.514125
451.662064	28509.996288	30.519143
452.023521	28538.797526	30.524160
452.034820	28576.371674	30.529178
452.572352	28605.989261	30.534196
452.687344	28652.441273	30.539213
452.951439	28686.419116	30.544231
453.165574	28737.781854	30.549248
453.921076	28779.034341	30.554266
454.544616	28814.142202	30.559284
454.758181	28869.088633	30.564301
455.270261	28913.318252	30.569319
455.573769	28955.005410	30.574336
455.831299	29012.358041	30.579354
456.420398	29057.963186	30.584372
456.901837	29097.025327	30.589389
457.165314	29155.115552	30.594407
457.690667	29207.207388	30.599424
458.130147	29256.966759	30.604442
458.760759	29313.337701	30.609460
458.970361	29366.150893	30.614477
459.479546	29426.292764	30.619495
460.090210	29461.132797	30.624512
460.377665	29519.169816	30.629530
461.161061	29568.696629	30.634548
461.413353	29622.336304	30.639565
461.946557	29662.555139	30.644583
462.721945	29717.676430	30.649600
462.783508	29772.401645	30.654618
463.524122	29825.096976	30.659636
463.860403	29888.890288	30.664653
464.145993	29926.917307	30.669671
464.706520	29993.494025	30.674688
465.432213	30030.625261	30.679706
465.591409	30093.041691	30.684724
466.121382	30133.542902	30.689741
466.660364	30191.234641	30.694759
467.205826	30237.033067	30.699776
467.832892	30297.395079	30.704794
468.884411	30329.463787	30.709812
469.522619	30371.676346	30.714829
469.431828	30428.289962	30.719847
470.359027	30446.780270	30.724864
470.645738	30521.953025	30.729882
470.959584	30550.260756	30.734900
471.452944	30592.418916	30.739917
471.792505	30643.280790	30.744935
472.294442	30699.131762	30.749952
472.491720	30756.108954	30.754970
472.727540	30790.638190	30.759988
473.368501	30840.368828	30.765005
473.661589	30892.466246	30.770023
474.301931	30948.093261	30.775040
474.630711	30997.244992	30.780058
474.999883	31061.734354	30.785076
475.688379	31121.423454	30.790093
476.256646	31160.838693	30.795111
477.187976	31213.714948	30.800128
477.869027	31257.695509	30.805146
477.963064	31307.811214	30.810164
478.694614	31345.748744	30.815181
478.597888	31392.814072	30.820199
479.303801	31443.236048	30.825216
479.832902	31500.309132	30.830234
480.162238	31540.168503	30.835252
480.816351	31597.022506	30.840269
481.217840	31636.217146	30.845287
481.914939	31682.593735	30.850304
482.538747	31742.232555	30.855322
483.053246	31767.758169	30.860340
483.433654	31815.894155	30.865357
483.938249	31836.935414	30.870375
484.609448	31880.228278	30.875392
484.630457	31921.158447	30.880410
484.726087	31956.085416	30.885428
485.304921	32009.899352	30.890445
485.957906	32073.768242	30.895463
486.715969	32100.351988	30.900480
486.527099	32161.748065	30.905498
487.159089	32208.218833	30.910516
487.720292	32267.828776	30.915533
487.965955	32317.203021	30.920551
488.517088	32375.136604	30.925568
488.808687	32434.491936	30.930586
489.254525	32482.265602	30.935604
489.487222	32535.150848	30.940621
490.093293	32613.879608	30.945639
490.761623	32652.931494	30.950656
491.231285	32728.376938	30.955674
491.820948	32770.934601	30.960692
492.486605	32825.553835	30.965709
492.773944	32896.168328	30.970727
493.344534	32934.555513	30.975744
493.670016	33008.104594	30.980762
494.141771	33059.778276	30.985780
494.915414	33121.463572	30.990797
495.147334	33183.210173	30.995815
495.848485	33240.960930	31.000832
496.205050	33307.053942	31.005850
496.861258	33376.337950	31.010868
497.434891	33431.072076	31.015885
497.936542	33498.990713	31.020903
499.197293	33532.034081	31.025920
499.662399	33603.874620	31.030938
499.916378	33637.803853	31.035956
500.686437	33700.968364	31.040973
501.077750	33743.356066	31.045991
501.557063	33794.159844	31.051008
501.964179	33849.203584	31.056026
502.563166	33911.895443	31.061044
503.193642	33933.271808	31.066061
503.241078	34007.839628	31.071079
503.605767	34050.784623	31.076096
504.256523	34103.286855	31.081114
504.639201	34157.013569	31.086132
505.328609	34217.760599	31.091149
505.884595	34277.706365	31.096167
506.418374	34321.280372	31.101184
506.924684	34389.217446	31.106202
507.335994	34438.567127	31.111220
508.200922	34498.042962	31.116237
508.540251	34573.836523	31.121255
508.699265	34593.619275	31.126272
509.271136	34672.504879	31.131290
509.821683	34721.056149	31.136308
510.747903	34776.225282	31.141325
511.126502	34831.043300	31.146343
511.653850	34871.123635	31.151360
512.231361	34937.167325	31.156378
512.660191	34975.654949	31.161396
513.407086	35035.656945	31.166413
513.710392	35065.043374	31.171431
514.565390	35131.467926	31.176448
515.110742	35173.215163	31.181466
515.255173	35230.925560	31.186484
515.784240	35271.779589	31.191501
516.256475	35327.145335	31.196519
516.839744	35362.433952	31.201536
516.964086	35431.406831	31.206554
517.522036	35469.422974	31.211572
517.865175	35521.257636	31.216589
518.293279	35584.523230	31.221607
518.927220	35622.640746	31.226624
519.352821	35683.789796	31.231642
519.658221	35748.540380	31.236660
520.290261	35798.018317	31.241677
520.453073	35871.360054	31.246695
520.946904	35914.483877	31.251712
521.554964	35984.480272	31.256730
521.952883	36048.105919	31.261748
522.825225	36106.541449	31.266765
522.680354	36166.271726	31.271783
523.456832	36248.333424	31.276800
523.895060	36319.460481	31.281818
524.497965	36393.129274	31.286836
524.911292	36455.478971	31.291853
525.282338	36540.976015	31.296871
525.779497	36598.421154	31.301888
526.492102	36674.512290	31.306906
526.697451	36744.631835	31.311924
527.890818	36812.669808	31.316941
528.337739	36881.673904	31.321959
529.177784	36958.890714	31.326976
529.820602	37017.670090	31.331994
530.400665	37093.538760	31.337012
530.952155	37144.772542	31.342029
531.384151	37208.592352	31.347047
532.117040	37263.741185	31.352064
532.709880	37340.082152	31.357082
532.852778	37403.502291	31.362100
534.012919	37463.611468	31.367117
534.128567	37521.488661	31.372135
534.735546	37610.306453	31.377152
535.162041	37658.343427	31.382170
535.596098	37745.912347	31.387188
536.842507	37789.790557	31.392205
536.712116	37868.806311	31.397223
537.279770	37911.727100	31.402240
538.208039	37978.105977	31.407258
538.396529	38036.714428	31.412276
539.179989	38107.040464	31.417293
539.519776	38174.419856	31.422311
540.015712	38229.314144	31.427328
540.688217	38290.658553	31.432346
540.952251	38373.237533	31.437364
541.763451	38439.277674	31.442381
541.753379	38505.905016	31.447399
542.583839	38566.425815	31.452416
543.494323	38649.410551	31.457434
543.597401	38712.280117	31.462452
544.492127	38782.543075	31.467469
545.135571	38853.261253	31.472487
545.369742	38906.610206	31.477504
546.142599	38987.621462	31.482522
546.761810	39049.829394	31.487540
547.021422	39123.780717	31.492557
547.417588	39186.332100	31.497575
547.941989	39255.045309	31.502592
548.238031	39331.989758	31.507610
548.881591	39398.878537	31.512628
549.647839	39475.704902	31.517645
549.758923	39551.708746	31.522663
550.131406	39613.867844	31.527680
551.064660	39695.992000	31.532698
551.401664	39778.821002	31.537716
552.299643	39830.797405	31.542733
553.064519	39910.207610	31.547751
553.960168	39951.980721	31.552768
554.689195	40022.575714	31.557786
555.311377	40060.032336	31.562804
556.008828	40124.285750	31.567821
556.455261	40175.296166	31.572839
557.271592	40234.644452	31.577856
557.623960	40288.303049	31.582874
558.199080	40357.438162	31.587892
558.681854	40391.762208	31.592909
559.035244	40457.626531	31.597927
559.296696	40513.317689	31.602944
560.036192	40588.073178	31.607962
560.215656	40647.613228	31.612980
560.910775	40720.710046	31.617997
561.214473	40769.949744	31.623015
561.402122	40858.657075	31.628032
562.258016	40930.361468	31.633050
562.482057	41007.735244	31.638068
563.306906	41083.962180	31.643085
563.585601	41152.868356	31.648103
564.512433	41225.341831	31.653120
565.365137	41301.268371	31.658138
565.615702	41373.633185	31.663156
566.563678	41442.385717	31.668173
567.169792	41502.022224	31.673191
567.882581	41575.892893	31.678208
569.007431	41642.865110	31.683226
569.195743	41713.799029	31.688244
569.826670	41778.381768	31.693261
570.045731	41848.771365	31.698279
570.607531	41914.499203	31.703296
571.337900	41964.315587	31.708314
571.735942	42052.902427	31.713332
572.537850	42115.841948	31.718349
572.987964	42197.801515	31.723367
573.473591	42259.849946	31.728384
573.994104	42326.599357	31.733402
574.607329	42417.393623	31.738420
575.316641	42464.929439	31.743437
576.109172	42544.343399	31.748455
576.202029	42613.311024	31.753472
577.335384	42685.554151	31.758490
577.435922	42749.280913	31.763508
578.059352	42824.475097	31.768525
578.398799	42887.714624	31.773543
578.914316	42971.813417	31.778560
579.711169	43052.381071	31.783578
580.343206	43132.297596	31.788596
580.963307	43217.671357	31.793613
580.954440	43295.595190	31.798631
581.793972	43385.223568	31.803648
582.677821	43433.932653	31.808666
582.981350	43522.349621	31.813684
583.283732	43604.671329	31.818701
584.131068	43686.811845	31.823719
584.541522	43775.354423	31.828736
585.205090	43836.147601	31.833754
585.804780	43937.129406	31.838772
586.758647	44003.061980	31.843789
587.249414	44091.447590	31.848807
587.462274	44166.800303	31.853824
588.508482	44249.052535	31.858842
589.243158	44323.972435	31.863860
589.646519	44405.056124	31.868877
590.174716	44477.358883	31.873895
590.696863	44550.995180	31.878912
591.549120	44614.550550	31.883930
592.164662	44677.002390	31.888948
592.920012	44728.299626	31.893965
593.697786	44796.474043	31.898983
593.761050	44856.735161	31.904000
594.593508	44926.807890	31.909018
594.708539	45008.573257	31.914036
595.144695	45069.253351	31.919053
595.922070	45157.397810	31.924071
596.505956	45226.426680	31.929088
597.167490	45309.249140	31.934106
597.501304	45384.290049	31.939124
598.231152	45464.352038	31.944141
598.645149	45529.359453	31.949159
599.007083	45631.359007	31.954176
599.916951	45695.161138	31.959194
600.328249	45793.049060	31.964212
600.955413	45880.801846	31.969229
601.522640	45963.908003	31.974247
601.976994	46053.811817	31.979264
603.133118	46135.820620	31.984282
603.824216	46220.268246	31.989300
604.211622	46288.010598	31.994317
604.898332	46378.155439	31.999335
605.030009	46466.216985	32.004352
606.224607	46562.407213	32.009370
607.100767	46626.495946	32.014388
607.641848	46721.427796	32.019405
608.345197	46771.833089	32.024423
608.870961	46854.959530	32.029440
609.956152	46925.064339	32.034458
610.676271	47006.047042	32.039476
611.411776	47070.119481	32.044493
612.091570	47153.360733	32.049511
612.324396	47219.152265	32.054528
613.014414	47289.307921	32.059546
613.454745	47371.569828	32.064564
613.918143	47443.670612	32.069581
614.283730	47510.451636	32.074599
614.945694	47603.776602	32.079616
615.659183	47671.173289	32.084634
616.218037	47767.850457	32.089652
616.861839	47841.691201	32.094669
617.419102	47931.192328	32.099687
617.797981	48031.579156	32.104704
618.426598	48092.935103	32.109722
619.412389	48185.808454	32.114740
619.906619	48268.636910	32.119757
620.551205	48344.831936	32.124775
620.939237	48445.598374	32.129792
621.847805	48520.683219	32.134810
622.306729	48607.121903	32.139828
622.557930	48695.474126	32.144845
623.291496	48774.567597	32.149863
623.991359	48872.104981	32.154880
624.606764	48957.995240	32.159898
625.727029	49025.184328	32.164916
625.931617	49116.523986	32.169933
626.699210	49194.783098	32.174951
627.268851	49297.892424	32.179968
627.620279	49385.217655	32.184986
628.551647	49467.720222	32.190004
629.160227	49564.941521	32.195021
629.889399	49637.625727	32.200039
629.988361	49734.357332	32.205056
630.809828	49832.100624	32.210074
631.622111	49916.096390	32.215092
632.039330	50016.509516	32.220109
633.076306	50083.946645	32.225127
633.035151	50180.103649	32.230144
634.023724	50253.233691	32.235162
634.600389	50328.472101	32.240180
635.179508	50427.025867	32.245197
636.236451	50491.110510	32.250215
636.301743	50591.363731	32.255232
637.149400	50668.671443	32.260250
637.662483	50749.098035	32.265268
638.253704	50842.927511	32.270285
639.266911	50918.929880	32.275303
639.992211	51013.230709	32.280320
640.602694	51081.569232	32.285338
641.382014	51174.642908	32.290356
641.609430	51251.745926	32.295373
642.349523	51347.801882	32.300391
642.823996	51430.773712	32.305408
643.592106	51533.811827	32.310426
644.309638	51607.443447	32.315444
644.621959	51721.778904	32.320461
645.524138	51793.163678	32.325479
645.792924	51895.888272	32.330496
646.242140	51993.792544	32.335514
647.329946	52080.970588	32.340532
647.557399	52185.064768	32.345549
648.532191	52288.334937	32.350567
648.943972	52370.193668	32.355584
649.557482	52481.028700	32.360602
650.444127	52576.314917	32.365620
651.090756	52679.047613	32.370637
651.801043	52780.506991	32.375655
652.616325	52869.249643	32.380672
653.223252	52970.727092	32.385690
653.857044	53068.615820	32.390708
654.739681	53167.133535	32.395725
655.438227	53253.777919	32.400743
656.137851	53354.149247	32.405760
656.729035	53451.510011	32.410778
657.441859	53546.286467	32.415796
657.707716	53647.410035	32.420813
658.528797	53742.131668	32.425831
658.869858	53842.245734	32.430848
659.470743	53934.522050	32.435866
660.465774	54041.958099	32.440884
660.991599	54148.474116	32.445901
662.096226	54250.637302	32.450919
662.617985	54345.247068	32.455936
663.364242	54445.720583	32.460954
663.968232	54540.039755	32.465972
664.239867	54641.066466	32.470989
665.330756	54747.283968	32.476007
665.679112	54838.292263	32.481024
666.621137	54932.039477	32.486042
667.698625	55028.512881	32.491060
668.028741	55138.048497	32.496077
669.011363	55217.980262	32.501095
669.774696	55308.467352	32.506112
670.912134	55398.608784	32.511130
671.960979	55466.217600	32.516148
672.640258	55562.658332	32.521165
673.169034	55628.616244	32.526183
674.001579	55725.613695	32.531200
674.736718	55783.508226	32.536218
675.559942	55857.366000	32.541236
675.524678	55955.645112	32.546253
676.363206	56009.201863	32.551271
676.996005	56103.466975	32.556288
677.407456	56187.230885	32.561306
677.980917	56269.180432	32.566324
678.386849	56358.910082	32.571341
678.710756	56439.176760	32.576359
679.367877	56529.882897	32.581376
679.983682	56623.199296	32.586394
680.744098	56702.832657	32.591412
681.107798	56811.607602	32.596429
682.212936	56883.141858	32.601447
682.730383	56978.794931	32.606464
683.255402	57064.098081	32.611482
683.814299	57168.148373	32.616500
684.694048	57264.431679	32.621517
685.421998	57367.374688	32.626535
686.140069	57454.732668	32.631552
686.302958	57575.164308	32.636570
687.223095	57653.953756	32.641588
687.753776	57764.140641	32.646605
688.578506	57870.703357	32.651623
689.622058	57973.553174	32.656640
690.069557	58071.712563	32.661658
691.287627	58171.109973	32.666676
691.538333	58279.614697	32.671693
692.329362	58379.033130	32.676711
693.115095	58483.122385	32.681728
693.540708	58589.179891	32.686746
694.411138	58685.749680	32.691764
694.999675	58803.357228	32.696781
695.577386	58899.932171	32.701799
696.375995	59006.619046	32.706816
697.254430	59096.845466	32.711834
698.184509	59208.832144	32.716852
698.740510	59312.079046	32.721869
699.528130	59408.880866	32.726887
700.216267	59502.976128	32.731904
700.794174	59618.966286	32.736922
701.832173	59714.837268	32.741940
702.551134	59823.848109	32.746957
703.235338	59926.325054	32.751975
703.902787	60022.189199	32.756992
704.247579	60137.146620	32.762010
705.382663	60230.925053	32.767028
705.671022	60349.627637	32.772045
706.410738	60443.061612	32.777063
707.421211	60540.855830	32.782080
707.848309	60653.849972	32.787098
708.948674	60749.709299	32.792116
709.317314	60854.315847	32.797133
710.044077	60967.243306	32.802151
710.974811	61052.597673	32.807168
711.523743	61178.472582	32.812186
712.094610	61277.196116	32.817204
712.458642	61388.637573	32.822221
713.422045	61497.484435	32.827239
714.328289	61604.774066	32.832256
714.818071	61701.876299	32.837274
715.390698	61822.916813	32.842292
715.962805	61941.708326	32.847309
716.837858	62044.594302	32.852327
717.766336	62168.794862	32.857344
718.494719	62276.932692	32.862362
719.098153	62390.204483	32.867380
719.474287	62511.502764	32.872397
720.678410	62619.589138	32.877415
721.771213	62716.647218	32.882432
722.367750	62830.308125	32.887450
723.035766	62919.847044	32.892468
723.612860	63038.650492	32.897485
724.498017	63145.338738	32.902503
725.556628	63243.194995	32.907520
726.034248	63341.659604	32.912538
726.826412	63430.036326	32.917556
727.589125	63547.200451	32.922573
728.319401	63616.855153	32.927591
728.995531	63723.587275	32.932608
729.219524	63817.949988	32.937626
729.829097	63917.507959	32.942644
730.753424	64033.238760	32.947661
731.175013	64139.168167	32.952679
732.056193	64255.792209	32.957696
732.519299	64358.998121	32.962714
733.502570	64460.184583	32.967732
734.170540	64573.875026	32.972749
734.774585	64684.081395	32.977767
735.776565	64807.034463	32.982784
736.278115	64917.947960	32.987802
737.386605	65018.775192	32.992820
738.116332	65145.991130	32.997837
738.690288	65246.756062	33.002855
739.804653	65370.717908	33.007872
740.216630	65485.492286	33.012890
741.041557	65603.726131	33.017908
741.836805	65711.239048	33.022925
742.867172	65814.301713	33.027943
743.801757	65927.898737	33.032960
744.039930	66051.712302	33.037978
744.804523	66159.441212	33.042996
745.536218	66266.607226	33.048013
745.997969	66394.981318	33.053031
746.699730	66515.819733	33.058048
747.278944	66625.478022	33.063066
748.303549	66754.134339	33.068084
748.654254	66880.475397	33.073101
749.259580	67015.403698	33.078119
750.326599	67132.316780	33.083136
750.658534	67274.782656	33.088154
751.853589	67385.942567	33.093172
752.465760	67531.809077	33.098189
753.411984	67654.914757	33.103207
754.760503	67783.599826	33.108224
755.303157	67891.880117	33.113242
756.461330	68017.361444	33.118260
757.098615	68138.011340	33.123277
757.690730	68239.710803	33.128295
758.483149	68374.857249	33.133312
759.120766	68493.416671	33.138330
759.921872	68620.534700	33.143348
760.673373	68720.857331	33.148365
761.363674	68853.406519	33.153383
762.151782	68959.900670	33.158400
763.142117	69104.463997	33.163418
763.623993	69219.083099	33.168436
764.725922	69335.920593	33.173453
765.869185	69457.853767	33.178471
766.840520	69556.487733	33.183488
767.397553	69673.625719	33.188506
768.473656	69787.536554	33.193524
769.124246	69898.673315	33.198541
769.689188	70007.523537	33.203559
770.597480	70126.319344	33.208576
771.480051	70234.150988	33.213594
772.123082	70339.632925	33.218612
772.654876	70454.863777	33.223629
773.323895	70562.599598	33.228647
774.226443	70682.929494	33.233664
774.907812	70783.488514	33.238682
776.000831	70901.625941	33.243700
776.607156	71002.723158	33.248717
776.981244	71108.480954	33.253735
778.187674	71215.050205	33.258752
778.746280	71327.309795	33.263770
779.358490	71432.315434	33.268788
780.041029	71544.106801	33.273805
780.909874	71661.134765	33.278823
781.549384	71757.127713	33.283840
782.389913	71889.215939	33.288858
782.719939	71999.645301	33.293876
783.648764	72118.189662	33.298893
784.353050	72240.925865	33.303911
785.210267	72365.363662	33.308928
785.698266	72490.033877	33.313946
787.154701	72604.055133	33.318964
787.852564	72714.136596	33.323981
788.568600	72840.712354	33.328999
789.592928	72935.003076	33.334016
790.183567	73067.158833	33.339034
790.710869	73180.653710	33.344052
791.777592	73320.237943	33.349069
792.445276	73439.895054	33.354087
793.410700	73555.912075	33.359104
794.172502	73688.435436	33.364122
794.973471	73816.375078	33.369140
795.642892	73924.779138	33.374157
796.368950	74076.255496	33.379175
797.201188	74190.457836	33.384192
797.654438	74326.374839	33.389210
798.483862	74472.550513	33.394228
799.397550	74606.976788	33.399245
800.076548	74746.210627	33.404263
801.048977	74871.864384	33.409280
801.639283	75005.397999	33.414298
802.856671	75126.244755	33.419316
803.310238	75267.315101	33.424333
804.045752	75409.648824	33.429351
805.042921	75538.685581	33.434368
805.617268	75675.451099	33.439386
806.632816	75821.649417	33.444404
807.702400	75942.664258	33.449421
808.065742	76092.374366	33.454439
808.989391	76225.088915	33.459456
809.541754	76375.655116	33.464474
810.136948	76504.080985	33.469492
811.176809	76659.602614	33.474509
811.883864	76804.448190	33.479527
812.875354	76959.783895	33.484544
813.885198	77095.487182	33.489562
814.550294	77244.042287	33.494580
815.342834	77385.728096	33.499597
816.253434	77524.353300	33.504615
817.098061	77671.838136	33.509632
817.969031	77804.716435	33.514650
818.581315	77967.989530	33.519668
819.733109	78092.196572	33.524685
820.565885	78260.229427	33.529703
821.535040	78380.641882	33.534720
822.252189	78535.414226	33.539738
823.118477	78664.864196	33.544756
824.176870	78810.063439	33.549773
824.940576	78939.791275	33.554791
825.668483	79072.365629	33.559808
826.617856	79216.877167	33.564826
827.514719	79356.888663	33.569844
828.280420	79472.090996	33.574861
828.909666	79630.073281	33.579879
829.809277	79748.487001	33.584896
830.487061	79895.229936	33.589914
831.345288	80028.161662	33.594932
832.529346	80140.464738	33.599949
833.044057	80276.484407	33.604967
834.140735	80405.261330	33.609984
835.090377	80534.075927	33.615002
835.750786	80642.324975	33.620020
836.601660	80787.565094	33.625037
837.391346	80902.853103	33.630055
838.684031	81030.323549	33.635072
839.564765	81144.440225	33.640090
839.944871	81289.868876	33.645108
840.801492	81401.296202	33.650125
841.340218	81558.149524	33.655143
842.347982	81690.895665	33.660160
843.027009	81840.972095	33.665178
843.754328	81973.456260	33.670196
844.705923	82113.178703	33.675213
844.959496	82259.608679	33.680231
846.201198	82401.486359	33.685248
847.019561	82540.347846	33.690266
847.709711	82704.034992	33.695284
849.094695	82822.802333	33.700301
849.769664	82965.782960	33.705319
850.832910	83112.730012	33.710336
851.885244	83254.441892	33.715354
852.476189	83391.821596	33.720372
853.427870	83526.536221	33.725389
853.975272	83682.491918	33.730407
854.760075	83829.666727	33.735424
855.640471	83976.795074	33.740442
856.267952	84132.196578	33.745460
857.535049	84299.646328	33.750477
858.031968	84445.790862	33.755495
859.197338	84593.135513	33.760512
860.237542	84746.910441	33.765530
860.557423	84890.467918	33.770548
861.787792	85048.275058	33.775565
862.414321	85202.437682	33.780583
863.058559	85354.921874	33.785600
863.727540	85509.161796	33.790618
864.192051	85685.864566	33.795636
865.648415	85847.594062	33.800653
865.826086	86021.803437	33.805671
866.424970	86187.289495	33.810688
867.879825	86358.867355	33.815706
868.594013	86537.870045	33.820724
869.820469	86682.649299	33.825741
870.847698	86862.608800	33.830759
871.575047	87001.031581	33.835776
873.406228	87167.447393	33.840794
874.333537	87331.451167	33.845812
875.458876	87475.094214	33.850829
876.322081	87621.071882	33.855847
877.263265	87778.015361	33.860864
878.364531	87917.640992	33.865882
878.916905	88076.631127	33.870900
880.133058	88201.749916	33.875917
880.719020	88366.886680	33.880935
881.522778	88500.465310	33.885952
882.342345	88656.390759	33.890970
882.982172	88797.597466	33.895988
884.165827	88956.786749	33.901005
884.769445	89092.958147	33.906023
885.667239	89260.302355	33.911040
886.643871	89396.470872	33.916058
887.556426	89568.060713	33.921076
888.224591	89731.086386	33.926093
889.026908	89874.601365	33.931111
889.532643	90031.435698	33.936128
890.575897	90157.852729	33.941146
891.087918	90319.269330	33.946164
891.992628	90464.663046	33.951181
892.836897	90625.387753	33.956199
893.953409	90784.543538	33.961216
895.066417	90940.530594	33.966234
895.567996	91080.147495	33.971252
896.626861	91234.082452	33.976269
897.442455	91400.487198	33.981287
898.239058	91557.384866	33.986304
899.379422	91705.297571	33.991322
900.255589	91869.664214	33.996340
901.417083	92032.206601	34.001357
902.177671	92170.008854	34.006375
903.056966	92331.587329	34.011392
904.206323	92491.723703	34.016410
905.093740	92647.582001	34.021428
906.261634	92821.792227	34.026445
906.846670	92975.690095	34.031463
907.654602	93138.254079	34.036480
908.676656	93266.387222	34.041498
909.276856	93466.618294	34.046516
910.368025	93612.133325	34.051533
911.238805	93788.291934	34.056551
911.796692	93955.959482	34.061568
913.046727	94116.349552	34.066586
913.932861	94299.711690	34.071604
914.857582	94457.461592	34.076621
915.825748	94625.021735	34.081639
916.496469	94810.341017	34.086656
917.638382	94968.298890	34.091674
918.156360	95142.481293	34.096692
919.315978	95322.983188	34.101709
920.584469	95491.398477	34.106727
921.189344	95669.007107	34.111744
922.341868	95848.919115	34.116762
922.999211	96014.502091	34.121780
924.011736	96201.459152	34.126797
925.112297	96367.363764	34.131815
926.084959	96554.494671	34.136832
927.066190	96717.598370	34.141850
927.747612	96913.869433	34.146868
928.616650	97074.405193	34.151885
929.875197	97243.429177	34.156903
930.852142	97431.331956	34.161920
931.798122	97583.958751	34.166938
932.602556	97767.265464	34.171956
933.745274	97923.716775	34.176973
934.732322	98108.211210	34.181991
935.512895	98280.903983	34.187008
936.607878	98454.432255	34.192026
937.496605	98638.098642	34.197044
938.661487	98798.685379	34.202061
939.182944	98979.901865	34.207079
940.212979	99147.235782	34.212096
941.213995	99324.096354	34.217114
941.973659	99505.771094	34.222132
942.810939	99670.810791	34.227149
944.080321	99855.493134	34.232167
944.624421	100024.711004	34.237184
945.831469	100208.994767	34.242202
946.927088	100380.396627	34.247220
948.029706	100555.628509	34.252237
949.142830	100725.694081	34.257255
949.982274	100890.083059	34.262272
950.926538	101076.271460	34.267290
951.713784	101231.782955	34.272308
952.390127	101388.985050	34.277325
953.702798	101557.086060	34.282343
954.175684	101727.529992	34.287360
955.462330	101890.053672	34.292378
955.992360	102063.352005	34.297396
956.821538	102219.318474	34.302413
957.852815	102397.784734	34.307431
959.195920	102572.737653	34.312448
959.960984	102723.462993	34.317466
960.639872	102916.457713	34.322484
961.820772	103090.238043	34.327501
962.857698	103264.207940	34.332519
963.419531	103436.965876	34.337536
964.429879	103624.618242	34.342554
965.662811	103800.547468	34.347572
966.652450	103994.758962	34.352589
967.565340	104182.336527	34.357607
968.359287	104361.653447	34.362624
969.295035	104551.958824	34.367642
970.412589	104731.269208	34.372660
971.473518	104919.454528	34.377677
972.564883	105087.020122	34.382695
973.440259	105275.878175	34.387712
974.677443	105448.367140	34.392730
975.645044	105650.180229	34.397748
976.535274	105817.441835	34.402765
977.864721	106012.948423	34.407783
978.417321	106196.667942	34.412800
979.832592	106362.022751	34.417818
980.903643	106553.732521	34.422836
981.415265	106752.514057	34.427853
982.287777	106934.014028	34.432871
982.701657	107123.252951	34.437888
984.110038	107311.695816	34.442906
985.423511	107507.387192	34.447924
986.436062	107699.393625	34.452941
987.336911	107891.546548	34.457959
988.496843	108076.831727	34.462976
989.432415	108271.134713	34.467994
990.603757	108454.305609	34.473012
991.338804	108650.290947	34.478029
992.397291	108844.818491	34.483047
993.111798	109033.869503	34.488064
994.214102	109234.003409	34.493082
994.938664	109437.810864	34.498100
995.950320	109632.402568	34.503117
996.732984	109850.224428	34.508135
997.639283	110043.759941	34.513152
999.133899	110252.132829	34.518170
999.948041	110440.886050	34.523188
1000.888870	110656.598471	34.528205
1002.125718	110851.757174	34.533223
1003.029240	111055.724732	34.538240
1004.046169	111264.298345	34.543258
1005.040175	111457.677576	34.548276
1006.148891	111672.445767	34.553293
1007.391329	111874.754909	34.558311
1008.133982	112082.442789	34.563328
1009.459329	112267.451038	34.568346
1010.373102	112482.093167	34.573364
1011.076446	112678.265166	34.578381
1012.618224	112873.185445	34.583399
1013.443642	113065.337262	34.588416
1014.593612	113272.612301	34.593434
1015.824680	113470.134278	34.598452
1016.485987	113676.973697	34.603469
1017.445583	113850.474974	34.608487
1018.484883	114074.052215	34.613504
1019.741112	114236.790092	34.618522
1020.709996	114422.948559	34.623540
1021.223260	114622.535521	34.628557
1022.530153	114784.140822	34.633575
1023.788091	114982.581335	34.638592
1024.168604	115167.917195	34.643610
1025.587254	115357.846175	34.648628
1026.308285	115554.998592	34.653645
1027.556496	115773.437081	34.658663
1028.154415	115953.510215	34.663680
1029.117285	116173.481177	34.668698
1030.169599	116373.865885	34.673716
1031.183247	116591.399359	34.678733
1032.110958	116787.069455	34.683751
1033.106707	117004.647105	34.688768
1033.942978	117212.852278	34.693786
1035.078991	117425.735128	34.698804
1035.976993	117648.819681	34.703821
1037.632778	117855.323317	34.708839
1037.788170	118075.556536	34.713856
1039.151212	118292.779438	34.718874
1040.178679	118506.233159	34.723892
1041.161420	118739.840865	34.728909
1042.586658	118943.615823	34.733927
1043.389541	119179.486743	34.738944
1044.333577	119386.385119	34.743962
1045.428505	119619.233990	34.748980
1046.530917	119839.552594	34.753997
1048.076297	120068.314272	34.759015
1048.533279	120291.771140	34.764032
1049.681179	120523.947087	34.769050
1051.229769	120742.285707	34.774068
1052.241942	120977.604717	34.779085
1053.326756	121201.737918	34.784103
1054.422880	121428.151771	34.789120
1055.602519	121647.191701	34.794138
1056.728152	121869.574727	34.799156
1057.922783	122078.998011	34.804173
1059.056263	122311.570840	34.809191
1060.216817	122518.050479	34.814208
1061.652216	122738.868434	34.819226
1062.918211	122933.004168	34.824244
1063.875495	123159.162971	34.829261
1065.031945	123366.067448	34.834279
1065.839199	123568.418451	34.839296
1066.943575	123789.134241	34.844314
1068.072369	123992.512201	34.849332
1068.995107	124224.159256	34.854349
1069.878006	124416.099711	34.859367
1071.109140	124640.551944	34.864384
1071.926016	124854.923610	34.869402
1073.061871	125088.721914	34.874420
1074.015721	125292.847358	34.879437
1075.343189	125527.048346	34.884455
1076.428528	125736.946582	34.889472
1077.445766	125949.316087	34.894490
1078.767996	126166.161024	34.899508
1079.623168	126391.867118	34.904525
1080.779966	126615.041161	34.909543
1082.207378	126825.258076	34.914560
1082.953706	127041.165196	34.919578
1084.206929	127261.033026	34.924596
1085.138257	127483.439622	34.929613
1085.886877	127700.149511	34.934631
1086.828039	127928.767860	34.939648
1087.913313	128150.608965	34.944666
1089.031487	128365.361513	34.949684
1089.560428	128586.131633	34.954701
1090.959258	128811.398478	34.959719
1091.615954	129023.798410	34.964736
1092.482208	129261.792707	34.969754
1093.766099	129482.723500	34.974772
1094.806147	129704.279165	34.979789
1095.587640	129931.417913	34.984807
1097.009181	130163.269057	34.989824
1097.687331	130404.725417	34.994842
1098.636154	130636.138482	34.999860
1099.765812	130878.056341	35.004877
1100.803564	131124.414865	35.009895
1102.137135	131369.243507	35.014912
1103.108061	131602.586750	35.019930
1104.657011	131868.576848	35.024948
1105.575174	132105.050701	35.029965
1106.308999	132360.316645	35.034983
1107.846212	132600.431337	35.040000
1109.016125	132839.302892	35.045018
1110.057608	133080.757988	35.050036
1111.045985	133332.022233	35.055053
1112.570861	133575.505521	35.060071
1114.194923	133823.702523	35.065088
1115.146643	134049.055719	35.070106
1116.436545	134292.076243	35.075124
1118.064299	134521.187472	35.080141
1118.989926	134755.715054	35.085159
1120.130131	134992.896380	35.090176
1121.434265	135237.683797	35.095194
1122.444655	135481.951115	35.100212
1123.466255	135706.036760	35.105229
1124.396706	135967.485520	35.110247
1125.488042	136201.768105	35.115264
1126.309117	136449.991230	35.120282
1127.609180	136690.847726	35.125300
1128.686481	136931.514588	35.130317
1129.804706	137196.504606	35.135335
1130.993410	137451.469828	35.140352
1132.016890	137711.953761	35.145370
1133.098205	137954.934843	35.150388
1134.293175	138207.267928	35.155405
1135.767296	138465.857832	35.160423
1137.123748	138696.501314	35.165440
1137.874479	138960.120928	35.170458
1139.488267	139185.172292	35.175476
1140.643652	139434.427788	35.180493
1141.760447	139688.255772	35.185511
1143.296654	139921.248973	35.190528
1144.158279	140181.449435	35.195546
1145.559003	140411.805907	35.200564
1146.724873	140662.742442	35.205581
1147.867169	140914.191901	35.210599
1149.130245	141136.778530	35.215616
1149.832150	141392.006527	35.220634
1150.966977	141632.507827	35.225652
1152.395016	141877.501620	35.230669
1153.267267	142121.612618	35.235687
1154.314413	142390.142533	35.240704
1155.327729	142631.152785	35.245722
1156.546436	142893.546789	35.250740
1157.610728	143151.302143	35.255757
1158.609287	143381.250681	35.260775
1159.818838	143648.254759	35.265792
1160.814379	143897.404694	35.270810
1162.510393	144155.126689	35.275828
1163.709389	144385.619447	35.280845
1164.679871	144650.071290	35.285863
1166.192889	144885.917351	35.290880
1167.403787	145141.913463	35.295898
1168.170069	145365.230905	35.300916
1169.424231	145596.064952	35.305933
1170.289959	145851.755503	35.310951
1171.281114	146082.230383	35.315968
1172.146801	146330.379328	35.320986
1173.701005	146582.499651	35.326004
1174.837138	146827.500601	35.331021
1175.869400	147086.178038	35.336039
1177.013050	147331.612393	35.341056
1177.841736	147589.819852	35.346074
1179.018192	147842.708965	35.351092
1180.022550	148106.559780	35.356109
1181.271243	148380.669709	35.361127
1182.529140	148636.759448	35.366144
1183.255218	148917.034295	35.371162
1184.809021	149183.833285	35.376180
1185.930298	149450.198361	35.381197
1186.789881	149725.397308	35.386215
1187.940971	149992.281410	35.391232
1189.079516	150286.373113	35.396250
1190.552706	150577.583763	35.401268
1191.538368	150845.820386	35.406285
1192.604183	151147.591255	35.411303
1193.800552	151414.884102	35.416320
1194.828722	151726.292105	35.421338
1195.960511	151992.750046	35.426356
1197.151553	152302.347717	35.431373
1198.262050	152591.465343	35.436391
1200.322316	152889.065702	35.441408
1201.579929	153178.835804	35.446426
1203.004734	153456.239591	35.451444
1204.443676	153745.552902	35.456461
1205.446299	154036.563958	35.461479
1206.990823	154310.009671	35.466496
1208.063336	154608.484286	35.471514
1209.202886	154887.188681	35.476532
1210.494236	155162.166335	35.481549
1211.773910	155457.340941	35.486567
1213.201330	155728.774038	35.491584
1214.431551	156030.531619	35.496602
1215.714081	156298.720118	35.501620
1216.549760	156594.065531	35.506637
1217.768748	156870.107474	35.511655
1218.689940	157155.346155	35.516672
1220.463596	157468.733164	35.521690
1221.653444	157746.359039	35.526708
1222.835915	158035.176198	35.531725
1224.113350	158320.034768	35.536743
1225.388069	158603.246786	35.541760
1226.591383	158904.282637	35.546778
1227.888833	159182.788847	35.551796
1229.344395	159479.182669	35.556813
1230.376499	159760.413342	35.561831
1231.327319	160044.082356	35.566848
1232.378209	160341.183653	35.571866
1233.824050	160632.069369	35.576884
1235.057964	160919.046873	35.581901
1236.069900	161217.657996	35.586919
1237.751616	161511.175158	35.591936
1238.945238	161797.201399	35.596954
1240.105837	162094.665367	35.601972
1241.655914	162385.647947	35.606989
1242.558021	162678.223857	35.612007
1244.168452	162959.127555	35.617024
1245.458390	163257.136806	35.622042
1246.661237	163536.995297	35.627060
1247.528158	163822.163433	35.632077
1248.907152	164093.991274	35.637095
1250.096387	164374.771101	35.642112
1251.299079	164669.138359	35.647130
1252.441828	164938.333729	35.652148
1253.531210	165228.511502	35.657165
1254.597372	165503.305474	35.662183
1256.002553	165779.719999	35.667200
1257.023254	166079.747625	35.672218
1258.323154	166380.111906	35.677236
1259.647266	166662.597486	35.682253
1260.564688	166954.883505	35.687271
1261.816531	167240.518676	35.692288
1263.182619	167552.832114	35.697306
1264.392737	167851.381761	35.702324
1265.660513	168166.963968	35.707341
1266.437817	168464.866052	35.712359
1268.362115	168773.822597	35.717376
1269.108822	169079.727489	35.722394
1270.157943	169387.196018	35.727412
1271.633705	169707.462383	35.732429
1272.757159	170033.778221	35.737447
1274.238574	170352.830212	35.742464
1275.418339	170676.324585	35.747482
1276.515118	170983.364880	35.752500
1278.057343	171313.364156	35.757517
1279.023915	171627.739167	35.762535
1280.711146	171970.459093	35.767552
1281.963924	172294.549423	35.772570
1283.026717	172629.078642	35.777588
1284.807151	172948.619893	35.782605
1285.736636	173275.016557	35.787623
1287.498523	173603.359232	35.792640
1288.968729	173921.410313	35.797658
1290.092451	174253.327206	35.802676
1291.391415	174571.575967	35.807693
1292.805057	174907.053571	35.812711
1294.106256	175227.336808	35.817728
1295.521219	175555.154055	35.822746
1296.703707	175888.062640	35.827764
1297.865985	176217.398238	35.832781
1299.090717	176550.659817	35.837799
1300.347497	176879.552913	35.842816
1301.461088	177212.355200	35.847834
1302.859903	177549.097564	35.852852
1304.271284	177876.220637	35.857869
1305.397643	178225.868363	35.862887
1306.742240	178561.459138	35.867904
1307.806475	178898.532567	35.872922
1308.941557	179254.366698	35.877940
1310.673106	179601.741471	35.882957
1311.743734	179942.590241	35.887975
1312.884534	180291.983719	35.892992
1314.247817	180645.962593	35.898010
1315.455934	181007.686011	35.903028
1316.911660	181343.721426	35.908045
1318.082866	181712.093678	35.913063
1319.288602	182064.547404	35.918080
1320.944334	182433.263719	35.923098
1322.377723	182772.231357	35.928116
1323.731944	183123.944401	35.933133
1324.974489	183474.282130	35.938151
1326.317736	183833.426682	35.943168
1327.418793	184186.927522	35.948186
1328.870648	184541.718234	35.953204
1330.317094	184900.472273	35.958221
1331.425539	185256.086001	35.963239
1332.827341	185612.961025	35.968256
1334.489300	185958.600511	35.973274
1335.664760	186302.215509	35.978292
1337.308240	186641.604875	35.983309
1338.425390	186961.307606	35.988327
1340.037454	187307.458964	35.993344
1341.434984	187632.386957	35.998362
1342.999586	187970.414049	36.003380
1344.499015	188284.387540	36.008397
1345.625923	188626.349627	36.013415
1346.906216	188944.310640	36.018432
1348.008876	189293.401814	36.023450
1349.207591	189623.578582	36.028468
1350.831257	189967.688225	36.033485
1352.027782	190308.290824	36.038503
1353.458682	190661.334770	36.043520
1354.738543	190992.115384	36.048538
1356.048050	191353.434630	36.053556
1357.202024	191693.988990	36.058573
1358.819083	192054.360564	36.063591
1360.057354	192409.833451	36.068608
1361.617217	192754.604934	36.073626
1362.943672	193116.097294	36.078644
1364.454682	193459.497260	36.083661
1365.372385	193842.845087	36.088679
1366.827913	194193.100744	36.093696
1368.574311	194548.337500	36.098714
1369.612805	194919.891615	36.103732
1371.189010	195270.882564	36.108749
1372.666988	195644.425100	36.113767
1373.799412	195996.242426	36.118784
1375.337094	196375.504938	36.123802
1376.446226	196728.701311	36.128820
1377.710642	197095.838711	36.133837
1379.148659	197471.303057	36.138855
1380.263464	197838.012427	36.143872
1381.612361	198229.910982	36.148890
1382.824707	198596.189650	36.153908
1384.489830	198980.067839	36.158925
1385.708141	199354.424165	36.163943
1386.920619	199750.251980	36.168960
1388.514552	200129.857532	36.173978
1390.065249	200526.383233	36.178996
1391.142345	200914.495900	36.184013
1392.557053	201297.578274	36.189031
1393.955564	201697.068785	36.194048
1395.001783	202086.653333	36.199066
1396.570474	202494.487173	36.204084
1398.238325	202869.030156	36.209101
1399.942063	203275.094236	36.214119
1401.341201	203673.072552	36.219136
1402.946723	204068.530552	36.224154
1404.450771	204454.789817	36.229172
1405.671397	204837.339754	36.234189
1407.009717	205236.225639	36.239207
1408.027651	205633.312876	36.244224
1409.760492	206034.410766	36.249242
1411.019624	206435.487456	36.254260
1412.369393	206836.602158	36.259277
1413.800954	207229.541335	36.264295
1415.094368	207643.836501	36.269312
1416.531387	208033.896743	36.274330
1417.730209	208451.589388	36.279348
1419.034240	208826.832568	36.284365
1420.506982	209256.508724	36.289383
1422.088671	209638.401530	36.294400
1424.021403	210053.023196	36.299418
1425.209637	210455.681828	36.304436
1426.906492	210858.918836	36.309453
1428.479111	211249.887013	36.314471
1430.162536	211641.422893	36.319488
1431.962320	212000.244601	36.324506
1433.266018	212373.193583	36.329524
1435.175526	212739.085813	36.334541
1436.348877	213094.561823	36.339559
1437.513454	213462.383269	36.344576
1439.306338	213835.181860	36.349594
1440.786666	214204.554375	36.354612
1441.963264	214578.981692	36.359629
1443.045629	214951.191290	36.364647
1444.089446	215403.966898	36.369664
1445.745900	215786.828077	36.374682
1446.992684	216171.180739	36.379700
1447.878038	216574.032887	36.384717
1449.089788	216969.137654	36.389735
1450.266565	217388.148654	36.394752
1452.197332	217773.563498	36.399770
1453.069001	218207.257404	36.404788
1454.852812	218604.128768	36.409805
1456.368891	219030.100865	36.414823
1457.754048	219444.362712	36.419840
1459.225557	219870.345894	36.424858
1460.899833	220285.782721	36.429876
1462.330989	220697.553306	36.434893
1464.148796	221123.052996	36.439911
1465.286640	221531.929236	36.444928
1467.104076	221942.015690	36.449946
1468.377965	222372.004298	36.454964
1469.693593	222792.158550	36.459981
1471.174265	223222.675314	36.464999
1472.566043	223643.912540	36.470016
1474.496227	224072.580645	36.475034
1475.794668	224514.206590	36.480052
1477.528513	224943.062916	36.485069
1478.898416	225370.533207	36.490087
1480.146654	225797.720412	36.495104
1481.909977	226219.871345	36.500122
1483.625562	226660.192333	36.505140
1485.036013	227093.504262	36.510157
1486.871126	227526.061915	36.515175
1488.059272	227959.769293	36.520192
1489.622271	228369.997713	36.525210
1491.308805	228813.963630	36.530228
1492.709234	229250.205945	36.535245
1494.202066	229667.282847	36.540263
1495.623059	230106.953740	36.545280
1497.468166	230535.888029	36.550298
1499.164782	230961.876388	36.555316
1500.657883	231388.991920	36.560333
1502.461095	231821.036136	36.565351
1503.638767	232246.936401	36.570368
1505.070034	232673.329544	36.575386
1506.753343	233107.886834	36.580404
1508.560201	233531.959920	36.585421
1510.282031	233958.842382	36.590439
1511.335749	234385.607726	36.595456
1512.930067	234809.440165	36.600474
1514.816505	235230.558469	36.605492
1516.265977	235663.815598	36.610509
1517.750403	236087.847502	36.615527
1518.591111	236515.720755	36.620544
1520.182201	236944.055548	36.625562
1521.381732	237382.692857	36.630580
1523.062994	237810.938804	36.635597
1524.761873	238246.142954	36.640615
1525.887033	238696.353639	36.645632
1527.912609	239120.634146	36.650650
1528.788087	239557.145875	36.655668
1530.400391	239978.422963	36.660685
1532.520938	240395.883054	36.665703
1533.301976	240812.142587	36.670720
1534.823826	241244.639651	36.675738
1536.272303	241657.107544	36.680756
1537.922358	242101.879890	36.685773
1539.147979	242507.883328	36.690791
1540.819036	242968.225567	36.695808
1542.467617	243385.998303	36.700826
1543.814468	243831.840359	36.705844
1545.212141	244265.735794	36.710861
1546.716355	244701.316417	36.715879
1547.913840	245152.977392	36.720896
1549.699106	245593.161889	36.725914
1551.108981	246063.206277	36.730932
1552.302180	246518.248938	36.735949
1553.978328	246973.288889	36.740967
1555.192688	247449.947255	36.745984
1556.905876	247903.001194	36.751002
1558.876533	248381.720930	36.756020
1560.677074	248850.511595	36.761037
1562.463467	249289.533179	36.766055
1564.040579	249766.008298	36.771072
1565.936505	250220.889822	36.776090
1567.662890	250692.794466	36.781108
1568.529668	251152.800555	36.786125
1570.567708	251623.892853	36.791143
1572.319577	252080.731025	36.796160
1573.883533	252557.389672	36.801178
1575.640799	253000.103835	36.806196
1577.142884	253476.214788	36.811213
1579.084531	253948.214576	36.816231
1580.485138	254409.507732	36.821248
1581.876657	254874.537036	36.826266
1583.813956	255333.557708	36.831284
1585.286411	255808.989671	36.836301
1587.047835	256252.772685	36.841319
1588.958479	256731.333767	36.846336
1590.638286	257198.095310	36.851354
1592.045782	257656.264923	36.856372
1593.220337	258131.569583	36.861389
1595.062810	258589.058152	36.866407
1596.266667	259078.025316	36.871424
1597.947790	259547.505772	36.876442
1599.933768	260015.361042	36.881460
1601.197830	260500.990821	36.886477
1603.083426	260963.299498	36.891495
1604.550259	261450.547153	36.896512
1606.335097	261929.435474	36.901530
1607.509511	262393.436557	36.906548
1608.899010	262893.042955	36.911565
1610.704129	263372.639116	36.916583
1611.735726	263864.124545	36.921600
1613.628425	264347.668960	36.926618
1615.465072	264842.526936	36.931636
1616.328842	265337.621463	36.936653
1618.428036	265832.892981	36.941671
1620.067540	266339.214307	36.946688
1621.519469	266825.827987	36.951706
1623.018150	267330.901797	36.956724
1624.549690	267830.279524	36.961741
1626.550323	268328.893596	36.966759
1628.221225	268836.325763	36.971776
1629.668027	269344.251718	36.976794
1631.550823	269838.184356	36.981812
1632.960589	270334.176002	36.986829
1635.140505	270829.074745	36.991847
1636.468481	271325.485276	36.996864
1638.157321	271790.488393	37.001882
1639.786595	272272.673215	37.006900
1641.206259	272762.360488	37.011917
1643.009936	273235.929122	37.016935
1644.358675	273710.689917	37.021952
1645.956919	274193.004334	37.026970
1647.586780	274666.421850	37.031988
1648.901171	275180.662127	37.037005
1650.538878	275652.654293	37.042023
1651.919177	276164.138516	37.047040
1653.393230	276669.128682	37.052058
1654.905659	277163.493312	37.057076
1656.435373	277691.080670	37.062093
1658.299518	278188.586046	37.067111
1659.899164	278715.651680	37.072128
1661.510009	279239.183386	37.077146
1663.090516	279762.617318	37.082164
1664.364121	280289.809409	37.087181
1666.163087	280823.594334	37.092199
1668.027608	281349.111427	37.097216
1669.573267	281899.497613	37.102234
1671.374838	282427.968977	37.107252
1672.971136	282978.496257	37.112269
1674.523856	283522.475481	37.117287
1676.139803	284062.505425	37.122304
1678.200800	284610.487283	37.127322
1679.978330	285160.393953	37.132340
1681.534775	285714.552022	37.137357
1683.196124	286245.042238	37.142375
1684.607684	286810.092436	37.147392
1686.451384	287364.502451	37.152410
1688.283543	287937.175896	37.157428
1690.053132	288490.781347	37.162445
1691.572497	289062.105172	37.167463
1693.662150	289625.991868	37.172480
1695.111443	290191.404493	37.177498
1696.885247	290749.217347	37.182516
1698.312755	291321.538070	37.187533
1700.033748	291878.364505	37.192551
1702.089333	292461.956260	37.197568
1703.601907	293028.997868	37.202586
1705.764911	293598.291921	37.207604
1706.874173	294162.042290	37.212621
1708.850127	294731.768534	37.217639
1710.884033	295309.508941	37.222656
1712.978865	295884.086995	37.227674
1714.934464	296453.046558	37.232692
1716.596870	297014.812903	37.237709
1718.439073	297578.223219	37.242727
1720.192812	298149.011115	37.247744
1721.630648	298717.206727	37.252762
1723.880824	299270.788003	37.257780
1724.863309	299845.758219	37.262797
1726.438093	300409.909398	37.267815
1728.249414	300975.085281	37.272832
1730.222600	301566.696521	37.277850
1731.774604	302132.366035	37.282868
1733.792946	302696.253779	37.287885
1735.593031	303279.146621	37.292903
1737.412916	303848.902079	37.297920
1739.236724	304417.332867	37.302938
1741.338518	304966.412314	37.307956
1742.936967	305541.045166	37.312973
1744.498439	306103.718500	37.317991
1746.399579	306671.792726	37.323008
1748.347084	307245.341482	37.328026
1750.170439	307801.307129	37.333044
1751.367452	308370.756615	37.338061
1753.024592	308915.695155	37.343079
1754.703467	309468.118573	37.348096
1756.017657	310021.208098	37.353114
1758.075326	310562.235276	37.358132
1759.578316	311134.587231	37.363149
1761.251544	311680.749708	37.368167
1763.032967	312235.829872	37.373184
1764.407986	312795.341254	37.378202
1766.190727	313368.037673	37.383220
1767.825797	313934.964283	37.388237
1769.690386	314508.654696	37.393255
1771.452986	315099.524350	37.398272
1772.915410	315677.284731	37.403290
1774.738907	316263.564339	37.408308
1776.348386	316841.443899	37.413325
1778.021504	317443.813362	37.418343
1779.814531	318031.582244	37.423360
1781.559916	318662.471984	37.428378
1783.216655	319224.047800	37.433396
1785.028026	319851.488090	37.438413
1786.974880	320457.138967	37.443431
1789.007005	321070.540576	37.448448
1790.761491	321674.968306	37.453466
1792.434870	322295.248622	37.458484
1794.298594	322909.397828	37.463501
1796.377792	323531.580323	37.468519
1798.179141	324134.937121	37.473536
1799.732205	324765.726191	37.478554
1801.587603	325375.131029	37.483572
1803.373922	326000.410536	37.488589
1805.222238	326632.351298	37.493607
1807.238748	327261.718971	37.498624
1808.917802	327891.009010	37.503642
1810.829433	328524.341971	37.508660
1812.775090	329148.852708	37.513677
1814.465364	329794.598898	37.518695
1816.286945	330414.902428	37.523712
1818.000719	331071.573452	37.528730
1819.953530	331689.303138	37.533748
1821.886435	332332.544353	37.538765
1823.627107	332985.127359	37.543783
1825.436146	333614.183050	37.548800
1827.317332	334270.561653	37.553818
1829.364306	334902.686358	37.558836
1830.988028	335546.729171	37.563853
1832.634976	336190.633725	37.568871
1834.582446	336840.979908	37.573888
1836.190199	337492.364385	37.578906
1838.501829	338151.240431	37.583924
1840.532366	338795.913809	37.588941
1842.099657	339456.216494	37.593959
1843.823171	340085.490949	37.598976
1845.577154	340762.753790	37.603994
1847.985963	341396.493783	37.609012
1850.057515	342041.196384	37.614029
1851.943138	342702.445783	37.619047
1853.922199	343334.887197	37.624064
1856.025930	343989.839536	37.629082
1857.996842	344621.707546	37.634100
1859.597693	345277.334946	37.639117
1861.458328	345910.448243	37.644135
1863.444439	346553.837249	37.649152
1864.869908	347220.304977	37.654170
1866.866108	347862.354959	37.659188
1868.592145	348500.912995	37.664205
1870.448988	349166.419274	37.669223
1872.748475	349806.869898	37.674240
1873.959134	350441.831790	37.679258
1876.055020	351070.751077	37.684276
1877.859252	351707.475532	37.689293
1879.247337	352327.510334	37.694311
1881.277130	352961.819769	37.699328
1882.861816	353603.882890	37.704346
1884.598570	354234.086086	37.709364
1886.430335	354890.072366	37.714381
1888.205713	355534.994193	37.719399
1889.652436	356182.828112	37.724416
1891.557533	356845.167452	37.729434
1893.775812	357506.328409	37.734452
1895.355524	358165.452982	37.739469
1897.286475	358844.021969	37.744487
1899.302042	359504.525396	37.749504
1900.986418	360176.592431	37.754522
1902.785088	360848.832692	37.759540
1904.916911	361531.511177	37.764557
1906.345107	362205.312650	37.769575
1908.623311	362895.327359	37.774592
1910.624069	363585.401390	37.779610
1912.277045	364281.178543	37.784628
1914.414880	364977.573909	37.789645
1916.205127	365686.344021	37.794663
1918.298942	366375.110991	37.799680
1919.979432	367096.735859	37.804698
1921.801957	367793.538957	37.809716
1923.767432	368511.031411	37.814733
1925.464197	369225.535980	37.819751
1927.364167	369931.368810	37.824768
1929.209023	370660.636105	37.829786
1931.462197	371377.595446	37.834804
1933.556955	372105.448868	37.839821
1935.242219	372841.827379	37.844839
1937.459472	373573.055831	37.849856
1939.244369	374294.854809	37.854874
1941.234172	375030.961295	37.859892
1943.099724	375758.957077	37.864909
1945.146234	376485.817595	37.869927
1947.289362	377214.980585	37.874944
1949.248970	377973.730084	37.879962
1951.122813	378699.837975	37.884980
1952.698058	379464.451474	37.889997
1955.003760	380206.357477	37.895015
1957.196420	380965.307449	37.900032
1958.677005	381705.060136	37.905050
1960.819334	382468.422656	37.910068
1962.976709	383218.402046	37.915085
1964.664864	383979.320144	37.920103
1966.506121	384726.173581	37.925120
1968.605458	385492.009738	37.930138
1970.771106	386256.929700	37.935156
1972.428485	387007.945254	37.940173
1974.793986	387778.830908	37.945191
1976.557674	388520.717152	37.950208
1978.593344	389301.001496	37.955226
1980.424691	390069.815953	37.960244
1982.929620	390837.892236	37.965261
1984.503465	391608.486355	37.970279
1986.899127	392359.076723	37.975296
1988.802308	393133.964489	37.980314
1990.958248	393876.344442	37.985332
1993.426753	394643.977992	37.990349
1995.190165	395389.529292	37.995367
1997.372311	396158.084509	38.000384
1999.349927	396912.865450	38.005402
2001.148447	397677.567226	38.010420
2003.389440	398419.974075	38.015437
2005.230949	399177.001420	38.020455
2006.904303	399911.785160	38.025472
2009.072487	400650.498526	38.030490
2010.951075	401373.629928	38.035508
2013.238837	402115.885149	38.040525
2014.881444	402844.619430	38.045543
2016.900841	403582.649211	38.050560
2019.143622	404320.724502	38.055578
2020.257241	405074.753379	38.060596
2022.738474	405825.318628	38.065613
2024.450823	406572.291359	38.070631
2026.495345	407335.962771	38.075648
2028.271462	408089.852259	38.080666
2030.246410	408867.529654	38.085684
2032.362621	409630.948766	38.090701
2033.770696	410410.246891	38.095719
2036.547237	411191.931815	38.100736
2038.533893	411969.468569	38.105754
2040.560484	412756.273360	38.110772
2042.742411	413539.635078	38.115789
2044.147212	414319.657030	38.120807
2046.426592	415114.127377	38.125824
2048.802490	415904.707901	38.130842
2050.616371	416707.540445	38.135860
2052.846765	417498.451605	38.140877
2055.028010	418308.443470	38.145895
2056.856774	419104.209483	38.150912
2058.935428	419915.029048	38.155930
2060.895901	420711.255476	38.160948
2063.305511	421537.062580	38.165965
2065.037940	422333.782367	38.170983
2067.297020	423157.586276	38.176000
2069.563348	423979.513532	38.181018
2071.625031	424800.966437	38.186036
2074.034519	425619.448413	38.191053
2076.205470	426460.957536	38.196071
2078.166838	427267.482960	38.201088
2080.411558	428075.555412	38.206106
2082.300469	428908.824223	38.211124
2084.466063	429727.842120	38.216141
2086.447342	430554.862050	38.221159
2088.658151	431384.600167	38.226176
2091.267401	432196.069129	38.231194
2093.471306	433026.308135	38.236212
2095.597764	433843.166525	38.241229
2097.537548	434668.835336	38.246247
2099.594937	435496.480417	38.251264
2101.928651	436329.365334	38.256282
2103.655920	437153.918284	38.261300
2105.713175	437991.698669	38.266317
2107.751786	438820.240331	38.271335
2109.486124	439655.938119	38.276352
2111.947711	440495.685743	38.281370
2113.618887	441338.771373	38.286388
2115.804149	442199.097838	38.291405
2117.825370	443049.652212	38.296423
2119.978230	443894.434693	38.301440
2122.401482	444748.501125	38.306458
2124.185968	445591.002826	38.311476
2126.548656	446451.692037	38.316493
2128.637071	447297.215029	38.321511
2130.999621	448163.250257	38.326528
2133.489734	448998.067579	38.331546
2135.328126	449855.976873	38.336564
2137.498413	450710.205751	38.341581
2139.637200	451563.444687	38.346599
2141.631070	452417.381494	38.351616
2143.788912	453272.470772	38.356634
2145.770733	454126.441789	38.361652
2147.822229	454976.168994	38.366669
2149.741313	455798.827526	38.371687
2151.630321	456647.400957	38.376704
2153.780977	457463.988175	38.381722
2155.662367	458317.905173	38.386740
2158.234733	459156.149691	38.391757
2160.156375	460007.259321	38.396775
2161.937274	460852.137807	38.401792
2164.355033	461702.639667	38.406810
2166.264193	462566.839550	38.411828
2168.112595	463434.702725	38.416845
2169.874635	464302.694207	38.421863
2172.217011	465190.114575	38.426880
2174.405793	466068.725536	38.431898
2176.300993	466956.999805	38.436916
2178.548199	467847.450331	38.441933
2181.000232	468750.815286	38.446951
2183.091136	469646.061469	38.451968
2185.021992	470558.727312	38.456986
2186.907325	471463.676655	38.462004
2189.468592	472381.458228	38.467021
2191.466367	473301.309872	38.472039
2193.573894	474221.503275	38.477056
2195.973401	475161.863560	38.482074
2198.161679	476081.902792	38.487092
2200.216760	477017.276414	38.492109
2202.665106	477944.759165	38.497127
2204.965650	478888.384236	38.502144
2207.141562	479828.143158	38.507162
2209.030013	480774.417197	38.512180
2211.737997	481712.275166	38.517197
2213.645328	482675.468319	38.522215
2215.840453	483620.383322	38.527232
2218.292709	484579.194446	38.532250
2220.658676	485540.190722	38.537268
2222.927063	486504.635724	38.542285
2225.596847	487450.988617	38.547303
2227.589665	488429.007310	38.552320
2229.949482	489386.516387	38.557338
2231.864647	490357.626267	38.562356
2234.332550	491332.831619	38.567373
2236.256574	492297.018402	38.572391
2238.377508	493280.248468	38.577408
2241.011412	494235.428785	38.582426
2242.964612	495229.124183	38.587444
2245.073062	496191.701561	38.592461
2247.909371	497176.459095	38.597479
2250.336463	498150.732116	38.602496
2252.602567	499134.713727	38.607514
2254.617629	500112.978515	38.612532
2257.043955	501090.160248	38.617549
2259.207583	502072.978444	38.622567
2261.521535	503073.066589	38.627584
2263.674615	504034.332715	38.632602
2265.901029	505040.621976	38.637620
2268.255874	506014.197864	38.642637
2270.399171	507022.649399	38.647655
2272.517677	508010.367455	38.652672
2274.690253	509000.689330	38.657690
2276.849882	510008.751913	38.662708
2279.509498	510997.963890	38.667725
2281.767340	511980.224013	38.672743
2284.038777	512984.552895	38.677760
2286.942416	513972.079316	38.682778
2288.691225	514976.620972	38.687796
2291.325420	515959.884501	38.692813
2293.844062	516960.191414	38.697831
2296.026078	517955.904089	38.702848
2298.535251	518909.269697	38.707866
2300.692369	519877.601070	38.712884
2303.067152	520835.859509	38.717901
2305.472380	521777.326014	38.722919
2307.401434	522754.029999	38.727936
2309.816776	523688.878731	38.732954
2311.578456	524672.541027	38.737972
2313.842588	525631.022329	38.742989
2315.917861	526598.641332	38.748007
2318.163612	527592.460953	38.753024
2320.616973	528562.863279	38.758042
2322.649695	529572.098665	38.763060
2325.226346	530555.394441	38.768077
2327.639458	531550.535299	38.773095
2329.337691	532559.371703	38.778112
2332.095773	533553.515521	38.783130
2333.810450	534563.017738	38.788148
2336.390513	535575.881809	38.793165
2338.951185	536594.517669	38.798183
2341.089833	537625.633901	38.803200
2343.532644	538639.515346	38.808218
2345.804035	539672.778886	38.813236
2348.311751	540695.865215	38.818253
2350.992539	541718.095224	38.823271
2353.133439	542775.258249	38.828288
2355.786400	543803.179545	38.833306
2358.067806	544851.561879	38.838324
2360.213896	545894.355447	38.843341
2362.507386	546944.541775	38.848359
2365.036173	548012.917656	38.853376
2367.195642	549075.841241	38.858394
2369.214897	550134.432287	38.863412
2371.923051	551186.694313	38.868429
2373.896508	552251.315477	38.873447
2376.213714	553332.237346	38.878464
2378.592039	554417.286500	38.883482
2380.779539	555502.934204	38.888500
2382.824325	556615.358947	38.893517
2385.701394	557695.288926	38.898535
2388.008845	558804.223139	38.903552
2390.407230	559904.960400	38.908570
2392.780173	561007.922536	38.913588
2395.427361	562114.315276	38.918605
2397.950461	563225.659960	38.923623
2399.934918	564336.949727	38.928640
2402.642503	565437.026201	38.933658
2404.991099	566563.839553	38.938676
2407.334918	567680.813633	38.943693
2409.891951	568803.280900	38.948711
2411.789253	569919.131706	38.953728
2414.296054	571062.199004	38.958746
2416.962041	572176.622992	38.963764
2419.279871	573337.240564	38.968781
2422.196956	574448.915121	38.973799
2424.145690	575596.889211	38.978816
2426.699699	576715.451581	38.983834
2429.559310	577868.689908	38.988852
2432.058770	578990.621956	38.993869
2434.470858	580135.296016	38.998887
2436.841222	581241.794999	39.003904
2439.644934	582371.349355	39.008922
2442.315230	583493.399226	39.013940
2444.794519	584606.501315	39.018957
2447.358653	585735.987616	39.023975
2449.832966	586865.534951	39.028992
2452.270788	587997.691246	39.034010
2454.766217	589124.217719	39.039028
2456.906687	590245.283818	39.044045
2459.399312	591340.122290	39.049063
2461.434648	592415.539492	39.054080
2463.810842	593513.256296	39.059098
2466.430911	594618.048103	39.064116
2468.406820	595714.425440	39.069133
2470.929295	596800.841223	39.074151
2473.179444	597945.766707	39.079168
2475.501992	599043.230786	39.084186
2477.894473	600160.916625	39.089204
2479.852097	601297.298586	39.094221
2482.529500	602414.370988	39.099239
2484.634345	603571.789858	39.104256
2486.899740	604699.876250	39.109274
2489.616859	605859.017675	39.114292
2492.045715	607008.177931	39.119309
2494.587052	608177.225750	39.124327
2496.459495	609340.007866	39.129344
2498.687691	610531.787670	39.134362
2501.644963	611717.367249	39.139380
2503.923590	612925.348751	39.144397
2506.460220	614110.845594	39.149415
2509.076380	615322.465401	39.154432
2511.550218	616508.068386	39.159450
2514.000496	617722.005226	39.164468
2515.889707	618937.801686	39.169485
2518.648118	620173.070975	39.174503
2521.019927	621396.516428	39.179520
2523.915347	622646.882881	39.184538
2526.966156	623872.438679	39.189556
2529.309889	625117.963872	39.194573
2532.053818	626343.441042	39.199591
2534.704948	627599.823278	39.204608
2537.402146	628832.819577	39.209626
2540.187757	630081.594852	39.214644
2543.056516	631312.028983	39.219661
2545.589985	632547.869722	39.224679
2547.780927	633801.350419	39.229696
2550.481382	635037.172366	39.234714
2553.305716	636301.136270	39.239732
2555.578779	637536.035589	39.244749
2558.179423	638801.731009	39.249767
2560.907323	640061.462274	39.254784
2563.536574	641280.437223	39.259802
2566.248628	642545.906722	39.264820
2568.837500	643819.771972	39.269837
2571.245986	645079.192408	39.274855
2573.633304	646333.672994	39.279872
2576.181650	647592.909699	39.284890
2579.227883	648850.811068	39.289908
2581.472901	650141.345001	39.294925
2584.359933	651386.492105	39.299943
2586.832188	652677.959253	39.304960
2589.435710	653944.617624	39.309978
2592.307631	655209.077510	39.314996
2594.530668	656508.710542	39.320013
2597.340890	657766.725826	39.325031
2599.745638	659048.806984	39.330048
2602.449834	660318.120242	39.335066
2605.047638	661592.216788	39.340084
2607.654895	662889.349385	39.345101
2609.918544	664163.911628	39.350119
2612.421739	665456.536282	39.355136
2615.174270	666742.526016	39.360154
2618.034890	668033.203299	39.365172
2620.275639	669321.569844	39.370189
2623.116709	670606.579051	39.375207
2625.709824	671921.900956	39.380224
2628.059656	673186.544650	39.385242
2631.000782	674458.481332	39.390260
2633.248505	675719.520210	39.395277
2635.710181	676981.547871	39.400295
2638.064093	678232.237653	39.405312
2640.661853	679498.277917	39.410330
2643.291062	680769.756792	39.415348
2645.813050	682048.036008	39.420365
2648.543621	683324.464350	39.425383
2651.033192	684611.039121	39.430400
2653.384777	685910.818152	39.435418
2655.966629	687192.594351	39.440436
2658.379167	688516.725703	39.445453
2661.250162	689808.265710	39.450471
2663.752294	691124.553876	39.455488
2665.942798	692465.072938	39.460506
2668.689020	693795.374775	39.465524
2670.940540	695129.679274	39.470541
2673.396701	696481.115697	39.475559
2676.069770	697859.644389	39.480576
2678.622440	699235.895506	39.485594
2681.443183	700590.266406	39.490612
2683.944746	701981.570039	39.495629
2686.646362	703353.880605	39.500647
2689.688956	704742.376123	39.505664
2692.496269	706119.141756	39.510682
2695.367923	707519.958961	39.515700
2697.862967	708926.011767	39.520717
2700.543564	710320.312476	39.525735
2703.254675	711730.577486	39.530752
2705.913884	713150.027500	39.535770
2708.804394	714554.102380	39.540788
2711.469006	715987.139894	39.545805
2713.936547	717412.741349	39.550823
2716.704054	718830.332849	39.555840
2719.167741	720282.716369	39.560858
2722.232146	721707.293937	39.565876
2724.669541	723157.550422	39.570893
2727.649386	724622.102677	39.575911
2730.627121	726047.484851	39.580928
2733.007516	727507.373472	39.585946
2735.790150	728955.816270	39.590964
2738.360422	730420.593245	39.595981
2740.846560	731898.610245	39.600999
2743.999909	733353.624414	39.606016
2746.636137	734839.924813	39.611034
2749.520727	736299.689873	39.616052
2752.161499	737796.506983	39.621069
2754.688785	739267.987578	39.626087
2757.675688	740746.771926	39.631104
2760.607708	742252.874989	39.636122
2763.238325	743732.249336	39.641140
2766.151100	745219.242504	39.646157
2768.804074	746720.103063	39.651175
2772.181946	748189.592752	39.656192
2774.833643	749686.287202	39.661210
2777.651767	751177.492209	39.666228
2780.628096	752672.919228	39.671245
2783.480108	754151.129681	39.676263
2786.224825	755647.153759	39.681280
2788.930588	757150.232148	39.686298
2792.146129	758621.614930	39.691316
2795.008347	760108.182509	39.696333
2798.068835	761587.782638	39.701351
2800.747395	763073.309188	39.706368
2803.738697	764556.573924	39.711386
2806.581181	766024.666168	39.716404
2809.134781	767500.929898	39.721421
2811.858899	768987.299702	39.726439
2814.421142	770419.024941	39.731456
2816.829658	771885.645938	39.736474
2819.939949	773306.451471	39.741492
2823.086633	774763.436790	39.746509
2825.407548	776190.106998	39.751527
2827.959896	777644.949682	39.756544
2830.440460	779094.408237	39.761562
2833.447831	780564.947557	39.766580
2836.129986	782026.260478	39.771597
2838.799037	783511.426990	39.776615
2841.966772	784981.633476	39.781632
2844.433832	786465.685681	39.786650
2847.242609	787946.873613	39.791668
2850.346321	789447.419066	39.796685
2852.799129	790937.460783	39.801703
2855.625710	792434.039948	39.806720
2858.083513	793954.523449	39.811738
2861.023735	795472.444480	39.816756
2863.787289	796996.190376	39.821773
2866.577019	798533.950256	39.826791
2869.514771	800072.033114	39.831808
2872.087821	801627.801866	39.836826
2875.014704	803177.388934	39.841844
2877.550161	804757.372402	39.846861
2880.182368	806318.780593	39.851879
2883.115345	807894.701320	39.856896
2885.745614	809500.820364	39.861914
2888.619739	811074.746834	39.866932
2891.233748	812698.251202	39.871949
2893.987550	814301.457532	39.876967
2896.903208	815924.822443	39.881984
2899.766895	817560.648857	39.887002
2902.765468	819186.240422	39.892020
2905.468327	820828.131007	39.897037
2908.583378	822468.426758	39.902055
2911.801953	824116.643284	39.907072
2914.505506	825761.900205	39.912090
2917.595650	827408.828650	39.917108
2920.678849	829068.849994	39.922125
2923.629038	830754.840874	39.927143
2926.786001	832394.460679	39.932160
2929.828573	834074.217057	39.937178
2933.137324	835722.032236	39.942196
2936.284639	837359.471981	39.947213
2939.203162	839036.448600	39.952231
2942.303274	840687.699617	39.957248
2945.102657	842339.838487	39.962266
2948.162859	844013.004597	39.967284
2951.091426	845659.346834	39.972301
2953.805642	847329.797471	39.977319
2956.957373	849000.608145	39.982336
2960.103696	850668.545832	39.987354
2962.693013	852338.559610	39.992372
2965.919883	854014.820001	39.997389
2968.513977	855685.295116	40.002407
2971.638747	857358.144549	40.007424
2974.491183	859031.653072	40.012442
2977.354501	860724.205502	40.017460
2980.562383	862397.417392	40.022477
2983.407797	864099.805383	40.027495
2986.468968	865784.717637	40.032512
2989.054707	867469.628037	40.037530
2991.964358	869156.437779	40.042548
2994.847594	870857.889523	40.047565
2997.831451	872572.883000	40.052583
3000.858893	874273.632013	40.057600
3003.623395	875977.616826	40.062618
3006.457681	877663.880775	40.067636
3009.367882	879353.037403	40.072653
3012.362557	881024.002259	40.077671
3015.554844	882679.380372	40.082688
3018.215525	884355.059118	40.087706
3021.396725	886002.638046	40.092724
3023.933971	887682.115469	40.097741
3027.092956	889376.936026	40.102759
3029.740272	891058.699664	40.107776
3032.639461	892769.266481	40.112794
3035.527856	894465.434594	40.117812
3038.412238	896166.019546	40.122829
3040.843241	897903.772700	40.127847
3044.439739	899609.286556	40.132864
3047.202866	901353.061734	40.137882
3050.233806	903117.638073	40.142900
3053.314402	904833.603819	40.147917
3056.617052	906608.209382	40.152935
3059.726123	908358.514643	40.157952
3062.683469	910119.743122	40.162970
3065.654563	911886.277244	40.167988
3068.691069	913670.214839	40.173005
3071.287745	915448.073669	40.178023
3074.618817	917246.949857	40.183040
3077.341429	919060.510573	40.188058
3080.338908	920847.211915	40.193076
3083.360396	922672.770706	40.198093
3086.404989	924486.868618	40.203111
3089.695598	926297.055513	40.208128
3092.829597	928143.095240	40.213146
3096.322475	929983.647859	40.218164
3099.296219	931801.613955	40.223181
3102.416807	933639.145870	40.228199
3105.418264	935465.145398	40.233216
3108.741983	937320.038277	40.238234
3111.976312	939175.249707	40.243252
3115.139253	941017.478398	40.248269
3117.911570	942884.556822	40.253287
3121.306870	944743.790859	40.258304
3124.013439	946621.964679	40.263322
3127.309292	948478.347028	40.268340
3130.694347	950342.830575	40.273357
3133.460863	952235.945455	40.278375
3136.557550	954099.874383	40.283392
3140.093224	955991.923242	40.288410
3143.049931	957908.214255	40.293428
3146.261802	959853.068313	40.298445
3149.366935	961801.390428	40.303463
3152.644944	963729.284211	40.308480
3155.705579	965701.411263	40.313498
3158.696605	967635.371282	40.318516
3161.973684	969586.597657	40.323533
3165.186392	971539.221364	40.328551
3168.032790	973477.386980	40.333568
3171.311727	975449.352171	40.338586
3174.291216	977409.963218	40.343604
3177.739094	979381.326238	40.348621
3180.963611	981350.000396	40.353639
3184.170261	983309.136046	40.358656
3187.163182	985289.346434	40.363674
3190.295698	987262.519878	40.368692
3193.583517	989230.898005	40.373709
3196.544821	991194.369758	40.378727
3199.589446	993200.610844	40.383744
3202.724014	995179.400567	40.388762
3205.998577	997164.570152	40.393780
3209.182312	999162.560310	40.398797
3212.193650	1001146.281594	40.403815
3215.566760	1003125.462952	40.408832
3218.682805	1005069.938710	40.413850
3221.464398	1007030.870810	40.418868
3225.168476	1008967.603269	40.423885
3228.346308	1010912.965128	40.428903
3231.380648	1012846.439807	40.433920
3234.576492	1014803.535034	40.438938
3237.404935	1016748.197466	40.443956
3241.289608	1018713.209968	40.448973
3243.942753	1020675.415467	40.453991
3247.091455	1022638.787490	40.459008
3250.445997	1024603.564959	40.464026
3253.419905	1026597.388357	40.469044
3256.759929	1028563.967248	40.474061
3259.632275	1030574.263703	40.479079
3262.634113	1032592.601166	40.484096
3265.708041	1034591.376163	40.489114
3268.745213	1036631.988123	40.494132
3271.942516	1038665.171230	40.499149
3275.057039	1040693.382856	40.504167
3278.355831	1042758.024217	40.509184
3281.447297	1044819.523525	40.514202
3284.548150	1046897.878341	40.519220
3287.633340	1048959.091105	40.524237
3290.728741	1051051.867883	40.529255
3294.038861	1053153.532866	40.534272
3297.373900	1055256.028945	40.539290
3300.167343	1057389.340438	40.544308
3303.754326	1059506.707161	40.549325
3306.948971	1061634.849981	40.554343
3310.162832	1063773.111498	40.559360
3313.631611	1065930.077206	40.564378
3316.921652	1068088.719389	40.569396
3320.083801	1070233.203945	40.574413
3323.285054	1072416.623473	40.579431
3327.005595	1074573.215764	40.584448
3330.523246	1076755.043345	40.589466
3333.350277	1078909.305518	40.594484
3336.795366	1081088.073039	40.599501
3340.170027	1083284.158001	40.604519
3343.451488	1085472.774550	40.609536
3346.600663	1087682.517877	40.614554
3349.781035	1089880.656112	40.619572
3353.411749	1092087.190314	40.624589
3356.838226	1094295.533625	40.629607
3359.959959	1096508.752964	40.634624
3363.668964	1098730.128330	40.639642
3366.950966	1100939.314044	40.644660
3370.481003	1103153.369459	40.649677
3373.921953	1105377.487644	40.654695
3377.393417	1107603.444736	40.659712
3380.891685	1109820.575558	40.664730
3383.862607	1112048.107774	40.669748
3387.502026	1114262.526109	40.674765
3391.008927	1116491.550348	40.679783
3394.126568	1118722.087724	40.684800
3397.400447	1120950.340178	40.689818
3400.804499	1123203.757020	40.694836
3404.339325	1125432.566693	40.699853
3407.290312	1127673.825016	40.704871
3410.706775	1129907.330761	40.709888
3414.303000	1132158.356315	40.714906
3417.624591	1134402.030767	40.719924
3421.057874	1136640.571710	40.724941
3424.641584	1138904.275649	40.729959
3427.982189	1141170.838692	40.734976
3431.178074	1143414.035422	40.739994
3434.481535	1145673.662247	40.745012
3437.838511	1147903.870742	40.750016
3440.749613	1150108.310010	40.755021
3443.977926	1152232.904695	40.760026
3447.503754	1154311.447389	40.765031
3450.880203	1156295.908522	40.770036
3454.047918	1158209.858228	40.775040
3457.428930	1160057.652112	40.780045
3460.119164	1161831.569166	40.785050
3463.104936	1163494.768414	40.790055
3465.759616	1165112.629731	40.795060
3468.586921	1166622.980907	40.800064
3470.880776	1168072.946869	40.805069
3473.465943	1169452.910008	40.810074
3475.916781	1170727.614360	40.815079
3477.958163	1171974.625510	40.820084
3480.182301	1173121.627104	40.825088
3482.585278	1174202.346189	40.830093
3484.501036	1175229.659781	40.835098
3486.579012	1176187.752490	40.840103
3487.904126	1177076.813106	40.845108
3489.872042	1177911.157019	40.850112
3491.839140	1178687.619226	40.855117
3493.289725	1179403.013776	40.860122
3495.156096	1180073.599814	40.865127
3496.361409	1180681.773917	40.870132
3497.850343	1181255.462002	40.875136
3499.061950	1181773.395845	40.880141
3500.535326	1182259.226971	40.885146
3501.744960	1182686.693633	40.890151
3502.929608	1183069.325165	40.895156
3504.339810	1183403.137166	40.900160
3505.186449	1183709.162554	40.905165
3506.113459	1183986.265002	40.910170
3507.345482	1184220.672753	40.915175
3508.156132	1184438.389230	40.920180
3509.120593	1184598.294948	40.925184
3509.798980	1184727.097039	40.930189
3510.428684	1184858.068104	40.935194
3511.342163	1184924.912349	40.940199
3511.917847	1185008.277354	40.945204
3512.816341	1185045.201408	40.950208
3513.120516	1185053.807852	40.955213
3513.610073	1185053.539259	40.960218
3514.380162	1185022.174534	40.965223
3514.847801	1184964.231455	40.970228
3515.326932	1184908.167700	40.975232
3515.948609	1184833.919677	40.980237
3516.089077	1184729.639122	40.985242
3516.920890	1184622.419664	40.990247
3517.318219	1184481.393377	40.995252
3517.752071	1184329.817656	41.000256
3518.213408	1184163.081848	41.005261
3518.060621	1184000.300315	41.010266
3519.042448	1183789.705678	41.015271
3518.863542	1183604.705236	41.020276
3519.419257	1183383.246739	41.025280
3519.755187	1183170.474459	41.030285
3519.826053	1182952.277658	41.035290
3520.120916	1182693.840062	41.040295
3520.151036	1182457.932109	41.045300
3520.633871	1182188.989148	41.050304
3520.674484	1181918.222143	41.055309
3520.775082	1181662.495465	41.060314
3521.320142	1181378.718417	41.065319
3521.427273	1181103.284261	41.070324
3521.239920	1180790.499539	41.075328
3521.896657	1180503.925448	41.080333
3521.943259	1180184.850309	41.085338
3522.236747	1179878.147253	41.090343
3522.209931	1179549.344191	41.095348
3522.072603	1179221.574684	41.100352
3522.360685	1178884.482627	41.105357
3522.292350	1178562.029695	41.110362
3523.243877	1178217.531114	41.115367
3522.800638	1177876.914040	41.120372
3523.073788	1177524.849448	41.125376
3523.149704	1177168.553018	41.130381
3523.091658	1176822.337902	41.135386
3523.620877	1176456.305602	41.140391
3523.281218	1176093.124001	41.145396
3523.596193	1175719.534954	41.150400
3523.408153	1175356.465506	41.155405
3523.368286	1174979.111133	41.160410
3523.804869	1174610.890367	41.165415
3523.496907	1174240.880478	41.170420
3523.704005	1173842.754365	41.175424
3523.512467	1173471.256242	41.180429
3523.597113	1173079.504413	41.185434
3523.990604	1172694.840178	41.190439
3523.815071	1172306.940042	41.195444
3523.962025	1171913.958535	41.200448
3523.867831	1171520.515462	41.205453
3524.092019	1171122.650517	41.210458
3524.170909	1170733.081961	41.215463
3524.015402	1170324.651531	41.220468
3524.529671	1169914.569002	41.225472
3524.338242	1169527.219733	41.230477
3524.265726	1169127.741672	41.235482
3524.368377	1168726.694033	41.240487
3524.183228	1168313.486260	41.245492
3524.283930	1167883.678533	41.250496
3524.495075	1167485.633025	41.255501
3524.427605	1167067.398112	41.260506
3524.485528	1166663.178185	41.265511
3524.478146	1166241.845803	41.270516
3524.434940	1165815.291263	41.275520
3524.438547	1165402.483380	41.280525
3524.412665	1164982.374865	41.285530
3524.666571	1164557.463486	41.290535
3524.450940	1164148.276785	41.295540
3524.608190	1163706.024434	41.300544
3524.496714	1163292.029838	41.305549
3524.219569	1162876.990398	41.310554
3524.542293	1162449.156384	41.315559
3524.370211	1162015.509502	41.320564
3524.581979	1161586.772815	41.325568
3524.706723	1161176.447285	41.330573
3524.330777	1160756.151956	41.335578
3524.438180	1160318.159341	41.340583
3524.566059	1159901.777699	41.345588
3524.206176	1159455.186382	41.350592
3524.523494	1159032.274929	41.355597
3524.078265	1158609.076727	41.360602
3524.473682	1158174.735109	41.365607
3524.240490	1157763.728765	41.370612
3524.322632	1157328.706704	41.375616
3524.403983	1156902.730293	41.380621
3524.338696	1156460.281874	41.385626
3524.387386	1156041.620412	41.390631
3523.955487	1155610.987716	41.395636
3524.186346	1155174.248881	41.400640
3524.630740	1154740.561680	41.405645
3524.240679	1154310.288775	41.410650
3524.464875	1153875.146826	41.415655
3524.091581	1153443.664446	41.420660
3524.228152	1153012.157387	41.425664
3524.308706	1152573.334058	41.430669
3524.325062	1152146.130984	41.435674
3524.347844	1151699.385514	41.440679
3523.965874	1151272.555971	41.445684
3524.033849	1150837.756956	41.450688
3523.924427	1150404.656183	41.455693
3523.974884	1149965.999506	41.460698
3524.001723	1149536.972872	41.465703
3523.864463	1149105.190923	41.470708
3523.814837	1148669.758800	41.475712
3523.861697	1148246.687755	41.480717
3523.549526	1147803.362719	41.485722
3523.967607	1147383.383278	41.490727
3523.707682	1146939.029348	41.495732
3523.882516	1146523.760524	41.500736
3523.729064	1146081.212599	41.505741
3523.541846	1145651.905378	41.510746
3523.903679	1145220.387047	41.515751
3523.640404	1144796.806244	41.520756
3523.723098	1144364.884789	41.525760
3523.673433	1143922.328630	41.530765
3523.479784	1143491.329664	41.535770
3523.751122	1143033.471818	41.540775
3523.509030	1142630.106325	41.545780
3523.511710	1142190.621762	41.550784
3523.706834	1141756.381810	41.555789
3523.434757	1141337.648457	41.560794
3523.562841	1140901.356976	41.565799
3523.444657	1140458.996874	41.570804
3523.726763	1140013.591929	41.575808
3523.585116	1139585.208290	41.580813
3523.258163	1139154.827266	41.585818
3523.139950	1138730.167371	41.590823
3523.197860	1138308.672179	41.595828
3523.105910	1137871.028250	41.600832
3523.394940	1137445.533831	41.605837
3523.180418	1137019.043711	41.610842
3523.279417	1136577.463384	41.615847
3523.040595	1136167.527508	41.620852
3523.241175	1135720.445794	41.625856
3523.093885	1135299.315214	41.630861
3523.027396	1134873.768186	41.635866
3523.172457	1134436.276952	41.640871
3522.993122	1134022.840631	41.645876
3523.258692	1133576.992964	41.650880
3523.180227	1133149.979610	41.655885
3522.799272	1132704.355293	41.660890
3523.252951	1132284.692432	41.665895
3523.165964	1131854.250006	41.670900
3522.895792	1131409.449426	41.675904
3522.960706	1131009.711836	41.680909
3522.796161	1130567.009903	41.685914
3522.993817	1130143.322409	41.690919
3522.658708	1129708.658898	41.695924
3522.643175	1129263.446862	41.700928
3523.009701	1128844.097652	41.705933
3522.595200	1128437.874087	41.710938
3522.972278	1127990.113254	41.715943
3522.772208	1127580.650152	41.720948
3522.399118	1127135.224058	41.725952
3522.820384	1126694.386948	41.730957
3522.369317	1126275.255728	41.735962
3522.583160	1125846.656810	41.740967
3522.521155	1125413.025242	41.745972
3522.434276	1125006.295899	41.750976
3522.253143	1124563.573716	41.755981
3522.071095	1124166.694633	41.760986
3522.340326	1123742.105773	41.765991
3522.332837	1123328.191217	41.770996
3522.216242	1122898.172393	41.776000
3522.370972	1122475.786755	41.781005
3522.125571	1122049.053367	41.786010
3522.158793	1121618.240316	41.791015
3521.931633	1121214.864112	41.796020
3521.988524	1120780.551097	41.801024
3521.946358	1120373.747374	41.806029
3521.817909	1119950.256327	41.811034
3521.936565	1119547.554772	41.816039
3521.857597	1119128.849234	41.821044
3521.890079	1118698.182227	41.826048
3522.297955	1118280.568850	41.831053
3521.790557	1117861.834788	41.836058
3521.622384	1117452.447330	41.841063
3521.882455	1117019.511140	41.846068
3521.896505	1116604.024134	41.851072
3521.757920	1116188.053419	41.856077
3521.666796	1115778.620722	41.861082
3521.812002	1115353.672374	41.866087
3521.469395	1114936.303348	41.871092
3521.765376	1114528.713818	41.876096
3521.939021	1114100.228635	41.881101
3521.432208	1113688.797570	41.886106
3521.850006	1113262.684986	41.891111
3521.603385	1112850.574534	41.896116
3521.719814	1112431.313471	41.901120
3521.336224	1112037.478868	41.906125
3521.385985	1111612.345369	41.911130
3521.519498	1111205.770625	41.916135
3521.333125	1110782.136992	41.921140
3521.211193	1110373.632894	41.926144
3521.302649	1109946.452125	41.931149
3520.978307	1109545.553521	41.936154
3520.951149	1109143.812456	41.941159
3520.747909	1108736.915550	41.946164
3520.764523	1108339.784771	41.951168
3521.127153	1107927.960141	41.956173
3520.849762	1107516.400383	41.961178
3520.917004	1107109.240372	41.966183
3520.946222	1106694.320648	41.971188
3520.647969	1106288.877738	41.976192
3521.017886	1105891.508164	41.981197
3520.783045	1105483.797474	41.986202
3520.938057	1105081.914264	41.991207
3520.758248	1104686.265808	41.996212
3520.591260	1104264.981729	42.001216
3520.789353	1103871.695274	42.006221
3520.583896	1103457.711518	42.011226
3520.820661	1103055.186009	42.016231
3520.511455	1102640.200991	42.021236
3520.343337	1102239.592683	42.026240
3520.608656	1101854.271971	42.031245
3520.606627	1101450.423531	42.036250
3520.616224	1101055.433417	42.041255
3520.403391	1100645.441336	42.046260
3520.362258	1100244.950905	42.051264
3520.487786	1099846.889391	42.056269
3520.265147	1099449.142771	42.061274
3520.212955	1099048.087326	42.066279
3520.048283	1098659.262393	42.071284
3520.055640	1098258.521117	42.076288
3520.120689	1097871.036350	42.081293
3519.696326	1097483.795748	42.086298
3520.032806	1097077.268839	42.091303
3519.758554	1096707.072188	42.096308
3519.565005	1096303.827353	42.101312
3519.917206	1095910.414058	42.106317
3519.579848	1095523.401556	42.111322
3520.004819	1095122.359195	42.116327
3519.909870	1094737.068889	42.121332
3519.937367	1094343.403825	42.126336
3520.050094	1093951.993442	42.131341
3519.685910	1093544.838086	42.136346
3519.767146	1093164.863498	42.141351
3519.547025	1092789.794769	42.146356
3519.715648	1092386.581566	42.151360
3519.738043	1091987.575755	42.156365
3519.370219	1091611.109228	42.161370
3519.733656	1091211.128268	42.166375
3519.681026	1090840.494097	42.171380
3519.495300	1090436.523873	42.176384
3519.603005	1090057.955578	42.181389
3519.273820	1089667.074996	42.186394
3519.455667	1089274.549232	42.191399
3519.393035	1088897.173520	42.196404
3519.104839	1088502.369906	42.201408
3519.590835	1088137.307367	42.206413
3519.302010	1087727.115604	42.211418
3519.289351	1087356.716195	42.216423
3519.202611	1086966.847249	42.221428
3519.087682	1086591.907858	42.226432
3519.316977	1086201.356867	42.231437
3519.401916	1085819.046028	42.236442
3519.335480	1085444.498877	42.241447
3519.073764	1085050.111235	42.246452
3519.035760	1084680.204847	42.251456
3519.011044	1084277.092467	42.256461
3519.015075	1083912.784655	42.261466
3519.152267	1083539.223628	42.266471
3519.033167	1083152.635149	42.271476
3518.798486	1082762.393342	42.276480
3518.883378	1082384.733151	42.281485
3518.665240	1082028.585501	42.286490
3518.464250	1081632.405352	42.291495
3518.473881	1081266.480541	42.296500
3518.778465	1080907.295167	42.301504
3518.784895	1080532.494063	42.306509
3518.564577	1080149.259630	42.311514
3518.559333	1079765.674929	42.316519
3518.454069	1079402.907036	42.321524
3518.333338	1079025.335929	42.326528
3518.552892	1078662.945273	42.331533
3518.492332	1078284.737078	42.336538
3518.575212	1077923.855842	42.341543
3518.416442	1077545.420603	42.346548
3518.083535	1077184.078904	42.351552
3518.292906	1076806.395980	42.356557
3517.999767	1076447.879744	42.361562
3517.991291	1076075.079686	42.366567
3517.706815	1075694.616192	42.371572
3517.863153	1075350.552506	42.376576
3517.855016	1074997.176873	42.381581
3517.813109	1074629.278611	42.386586
3518.211911	1074274.732594	42.391591
3517.875851	1073905.104842	42.396596
3517.749377	1073528.403652	42.401600
3517.854042	1073177.005638	42.406605
3517.637206	1072825.445827	42.411610
3517.627565	1072452.783385	42.416615
3517.636306	1072104.888055	42.421620
3517.587538	1071741.505959	42.426624
3517.797210	1071393.436230	42.431629
3517.547142	1071044.843356	42.436634
3517.489388	1070671.875396	42.441639
3517.489207	1070330.309630	42.446644
3517.156861	1069959.645718	42.451648
3517.385413	1069614.344186	42.456653
3516.866788	1069269.047814	42.461658
3517.178677	1068913.495861	42.466663
3516.921809	1068587.634390	42.471668
3517.325129	1068228.849455	42.476672
3517.335203	1067886.456521	42.481677
3517.089589	1067539.948317	42.486682
3517.280001	1067183.149996	42.491687
3517.245168	1066827.423772	42.496692
3517.109123	1066477.655883	42.501696
3516.858286	1066122.400575	42.506701
3516.403131	1065783.897754	42.511706
3516.797176	1065449.949130	42.516711
3516.728148	1065106.818495	42.521716
3516.600464	1064774.454410	42.526720
3516.759609	1064424.507138	42.531725
3516.639940	1064071.503596	42.536730
3516.751129	1063743.561440	42.541735
3516.584425	1063404.960767	42.546740
3516.578880	1063072.184847	42.551744
3516.450392	1062726.990125	42.556749
3516.306124	1062402.764637	42.561754
3516.394051	1062057.781103	42.566759
3516.693670	1061735.850267	42.571764
3516.683635	1061384.389348	42.576768
3516.602704	1061046.881201	42.581773
3516.640150	1060700.280086	42.586778
3516.452644	1060364.770103	42.591783
3516.500350	1060024.192397	42.596788
3516.340139	1059690.466874	42.601792
3516.485567	1059366.207424	42.606797
3516.167403	1059025.724569	42.611802
3516.369383	1058694.865477	42.616807
3516.602456	1058345.001000	42.621812
3516.355723	1058012.633302	42.626816
3516.516003	1057677.962267	42.631821
3516.306900	1057349.691839	42.636826
3516.363551	1057001.120246	42.641831
3516.269742	1056679.536891	42.646836
3516.113953	1056348.595922	42.651840
3516.319884	1056010.442799	42.656845
3516.198991	1055686.107126	42.661850
3516.111818	1055345.648091	42.666855
3516.360597	1054990.941059	42.671860
3516.034147	1054679.691297	42.676864
3515.930095	1054367.423186	42.681869
3515.863951	1054027.457891	42.686874
3515.949067	1053700.464623	42.691879
3515.629795	1053368.214717	42.696884
3515.483531	1053031.672962	42.701888
3515.970851	1052722.396972	42.706893
3515.794060	1052390.932840	42.711898
3515.490332	1052070.755210	42.716903
3515.581931	1051739.497177	42.721908
3515.305183	1051428.441852	42.726912
3515.593357	1051100.971918	42.731917
3515.308402	1050798.758115	42.736922
3515.395672	1050473.406661	42.741927
3515.438981	1050161.069520	42.746932
3515.289724	1049830.701733	42.751936
3515.229072	1049514.774880	42.756941
3515.224279	1049196.890651	42.761946
3515.372011	1048879.928173	42.766951
3515.471244	1048573.379489	42.771956
3515.252501	1048263.005274	42.776960
3515.377232	1047943.966022	42.781965
3515.367623	1047636.321580	42.786970
3515.405979	1047314.171187	42.791975
3515.463301	1047001.846574	42.796980
3515.264992	1046667.050083	42.801985
3515.450793	1046355.150621	42.806989
3515.253594	1046035.668287	42.811994
3515.066701	1045727.367687	42.816999
3515.199501	1045402.966161	42.822004
3515.464713	1045087.409099	42.827009
3515.117338	1044770.969141	42.832013
3514.953410	1044465.781896	42.837018
3514.918183	1044147.612941	42.842023
3515.099146	1043849.579621	42.847028
3514.670579	1043536.560224	42.852033
3514.975360	1043216.929433	42.857037
3514.911228	1042909.224859	42.862042
3514.995381	1042612.783566	42.867047
3515.007592	1042283.195166	42.872052
3514.765329	1041975.468186	42.877057
3514.977667	1041681.855077	42.882061
3514.327278	1041366.720460	42.887066
3514.446817	1041061.106031	42.892071
3514.772960	1040764.332935	42.897076
3514.617380	1040465.786817	42.902081
3514.989774	1040146.644834	42.907085
3514.712514	1039854.369118	42.912090
3514.602461	1039530.631090	42.917095
3514.707486	1039222.501088	42.922100
3514.507856	1038940.702745	42.927105
3514.873812	1038621.184231	42.932109
3514.802751	1038340.978082	42.937114
3514.550320	1038017.949025	42.942119
3514.476786	1037705.219416	42.947124
3514.317377	1037414.440077	42.952129
3514.626670	1037105.288770	42.957133
3514.580126	1036806.238079	42.962138
3514.376708	1036491.623950	42.967143
3514.262428	1036208.609172	42.972148
3514.149830	1035917.163521	42.977153
3514.182953	1035619.293564	42.982157
3514.226039	1035320.051561	42.987162
3514.034845	1035020.251554	42.992167
3513.906844	1034738.422137	42.997172
3513.652232	1034430.473114	43.002177
3513.872751	1034141.782645	43.007181
3513.726794	1033870.169786	43.012186
3513.640414	1033562.532200	43.017191
3513.860360	1033291.701909	43.022196
3513.646716	1033001.088223	43.027201
3513.763549	1032690.755784	43.032205
3513.599945	1032410.266451	43.037210
3513.702772	1032109.390280	43.042215
3513.706412	1031839.202737	43.047220
3513.427155	1031560.432292	43.052225
3513.543466	1031261.347646	43.057229
3513.649650	1030975.319888	43.062234
3513.738301	1030691.023288	43.067239
3513.575629	1030402.589755	43.072244
3513.638271	1030129.598406	43.077249
3513.831136	1029843.595250	43.082253
3513.584262	1029562.492304	43.087258
3513.434731	1029272.448670	43.092263
3513.290582	1028998.758147	43.097268
3513.419754	1028713.191914	43.102273
3513.293040	1028432.690375	43.107277
3513.284742	1028151.186528	43.112282
3513.123205	1027863.977956	43.117287
3513.001029	1027597.190381	43.122292
3512.919437	1027325.442150	43.127297
3513.148959	1027039.773918	43.132301
3512.577460	1026782.613798	43.137306
3512.990879	1026506.190095	43.142311
3513.095710	1026241.819916	43.147316
3513.143842	1025962.716171	43.152321
3512.997409	1025685.956528	43.157325
3512.727304	1025419.477114	43.162330
3512.815059	1025122.491606	43.167335
3513.013926	1024866.279616	43.172340
3512.827282	1024603.721742	43.177345
3513.368167	1024328.914360	43.182349
3513.192171	1024048.588835	43.187354
3513.333542	1023788.653154	43.192359
3513.133093	1023521.199384	43.197364
3512.735850	1023233.985861	43.202369
3513.234754	1022963.966356	43.207373
3512.991590	1022694.250005	43.212378
3512.802717	1022429.845187	43.217383
3513.076407	1022147.508009	43.222388
3512.494790	1021867.140143	43.227393
3513.005356	1021599.380562	43.232397
3512.928192	1021343.149921	43.237402
3512.712159	1021056.182906	43.242407
3512.971855	1020789.492945	43.247412
3512.883929	1020511.012958	43.252417
3512.927059	1020226.094906	43.257421
3512.731080	1019970.500204	43.262426
3512.743972	1019723.882203	43.267431
3512.826729	1019442.313488	43.272436
3512.884447	1019181.692876	43.277441
3512.741351	1018898.581641	43.282445
3512.790734	1018624.448940	43.287450
3512.499488	1018351.135301	43.292455
3512.684331	1018079.573839	43.297460
3512.543863	1017835.615474	43.302465
3512.419535	1017578.638397	43.307469
3512.537497	1017296.665134	43.312474
3512.471878	1017014.125567	43.317479
3512.620630	1016767.840695	43.322484
3512.156720	1016512.715125	43.327489
3512.286046	1016238.355750	43.332493
3512.207378	1015987.026021	43.337498
3512.159415	1015723.155687	43.342503
3512.515630	1015468.041799	43.347508
3512.296774	1015223.594581	43.352513
3512.207778	1014950.664788	43.357517
3512.026053	1014688.515763	43.362522
3512.025914	1014429.626358	43.367527
3512.226104	1014171.080505	43.372532
3512.099472	1013916.946961	43.377537
3511.963098	1013673.001488	43.382541
3511.787401	1013409.237896	43.387546
3511.756128	1013170.401097	43.392551
3512.104968	1012906.527558	43.397556
3511.701765	1012665.302182	43.402561
3511.624453	1012402.446620	43.407565
3511.772580	1012169.852263	43.412570
3511.976388	1011913.339414	43.417575
3512.016198	1011666.460528	43.422580
3511.839416	1011408.918664	43.427585
3512.093704	1011146.824358	43.432589
3511.538293	1010910.115702	43.437594
3511.649504	1010656.670365	43.442599
3511.678801	1010428.007863	43.447604
3511.482387	1010162.637936	43.452609
3511.544207	1009931.423158	43.457613
3511.383445	1009690.127616	43.462618
3511.456615	1009427.011267	43.467623
3512.070366	1009193.051012	43.472628
3511.680043	1008944.082522	43.477633
3511.740083	1008700.861399	43.482637
3511.830249	1008444.014979	43.487642
3511.378700	1008214.953086	43.492647
3511.832927	1007948.885738	43.497652
3511.563778	1007714.329051	43.502657
3511.729070	1007453.438913	43.507661
3511.302788	1007217.137296	43.512666
3511.615142	1006964.756982	43.517671
3511.915711	1006729.579346	43.522676
3511.264084	1006474.321358	43.527681
3511.253111	1006231.200001	43.532685
3511.294282	1006014.610315	43.537690
3511.169246	1005748.923741	43.542695
3511.015181	1005523.302211	43.547700
3510.847297	1005289.211665	43.552705
3511.176013	1005045.691537	43.557709
3511.076770	1004807.581588	43.562714
3510.827744	1004563.454911	43.567719
3510.952209	1004330.443860	43.572724
3510.928496	1004101.728291	43.577729
3511.058681	1003862.665157	43.582733
3511.122131	1003651.526886	43.587738
3510.860370	1003411.341679	43.592743
3510.870405	1003163.511776	43.597748
3510.533747	1002947.937140	43.602753
3510.825347	1002699.553997	43.607757
3510.899366	1002482.531613	43.612762
3510.683608	1002244.527543	43.617767
3510.745594	1002020.579697	43.622772
3510.440353	1001792.693036	43.627777
3510.832195	1001565.266372	43.632781
3510.579937	1001347.280876	43.637786
3510.085485	1001136.529972	43.642791
3510.632307	1000896.786195	43.647796
3510.388254	1000672.251354	43.652801
3510.418747	1000456.813368	43.657805
3510.650175	1000221.181678	43.662810
3510.226040	1000011.058776	43.667815
3510.680296	999768.459103	43.672820
3510.270078	999566.982698	43.677825
3510.407959	999332.595219	43.682829
3510.394288	999134.738190	43.687834
3510.279787	998899.498007	43.692839
3510.328149	998691.293249	43.697844
3509.900096	998468.162051	43.702849
3510.480281	998232.098055	43.707853
3510.543884	998023.671492	43.712858
3510.156334	997801.578700	43.717863
3510.406683	997576.157930	43.722868
3510.387963	997362.753217	43.727873
3510.236885	997146.342639	43.732877
3510.351420	996929.685231	43.737882
3510.420840	996717.020999	43.742887
3510.520181	996484.178166	43.747892
3510.139486	996283.067238	43.752897
3510.073828	996042.439651	43.757901
3510.207738	995842.494892	43.762906
3510.202273	995615.869213	43.767911
3510.224806	995394.199202	43.772916
3510.114698	995190.861362	43.777921
3510.228000	994971.498485	43.782925
3510.413074	994750.556134	43.787930
3510.093592	994534.463467	43.792935
3510.118100	994320.255039	43.797940
3509.580651	994112.271057	43.802945
3509.985983	993898.373834	43.807949
3509.660718	993698.234270	43.812954
3509.264824	993478.995079	43.817959
3509.989917	993279.837421	43.822964
3509.870376	993077.400198	43.827969
3509.988859	992874.039229	43.832973
3509.979293	992648.075636	43.837978
3509.788195	992434.806480	43.842983
3510.006222	992238.425546	43.847988
3509.594020	992018.742728	43.852993
3509.552692	991805.620288	43.857997
3509.841013	991614.471188	43.863002
3509.873019	991389.230734	43.868007
3509.835173	991199.584011	43.873012
3509.548609	990989.494178	43.878017
3509.529745	990785.788601	43.883021
3509.517768	990589.291090	43.888026
3509.535807	990370.839017	43.893031
3509.646809	990174.892084	43.898036
3509.297011	989975.015546	43.903041
3509.592070	989768.100847	43.908045
3509.510004	989557.241695	43.913050
3509.345424	989356.727706	43.918055
3509.553636	989157.901055	43.923060
3509.234025	988962.275937	43.928065
3509.156156	988762.702221	43.933069
3509.185594	988560.957628	43.938074
3509.302904	988368.849685	43.943079
3509.272886	988164.076522	43.948084
3509.240413	987993.736815	43.953089
3509.232904	987776.750432	43.958093
3509.157750	987588.745749	43.963098
3509.232293	987381.390368	43.968103
3509.180839	987182.635111	43.973108
3508.966896	986991.901394	43.978113
3509.222264	986794.155451	43.983117
3509.233954	986613.423166	43.988122
3508.837274	986420.553482	43.993127
3509.251493	986226.177379	43.998132
3508.888418	986040.218520	44.003137
3509.281791	985822.213303	44.008141
3509.011657	985646.376866	44.013146
3509.076005	985439.440544	44.018151
3509.450297	985241.523562	44.023156
3509.057636	985055.635072	44.028161
3509.051690	984854.253145	44.033165
3508.885428	984667.729009	44.038170
3508.840406	984471.318697	44.043175
3508.973376	984287.173455	44.048180
3509.022608	984092.687147	44.053185
3508.947810	983918.522625	44.058189
3508.831172	983715.947139	44.063194
3508.732596	983533.377919	44.068199
3508.828157	983360.828215	44.073204
3508.732619	983165.162418	44.078209
3508.815850	982992.017715	44.083213
3508.573259	982801.246174	44.088218
3508.407010	982600.006403	44.093223
3508.629274	982414.516504	44.098228
3508.335548	982252.544705	44.103233
3508.540080	982052.103521	44.108237
3508.402593	981868.706144	44.113242
3508.604973	981704.195345	44.118247
3508.826425	981513.402020	44.123252
3508.558143	981333.134608	44.128257
3508.664515	981144.203804	44.133261
3508.465004	980989.116060	44.138266
3508.303364	980794.942889	44.143271
3508.554185	980613.883467	44.148276
3508.477920	980435.412229	44.153281
3508.625597	980241.071602	44.158285
3508.813945	980065.476148	44.163290
3508.487502	979899.828113	44.168295
3508.578159	979708.898397	44.173300
3508.439156	979518.000133	44.178305
3508.505203	979341.816345	44.183309
3508.492451	979163.490365	44.188314
3508.237980	978982.560233	44.193319
3508.486350	978819.913230	44.198324
3507.883782	978634.534229	44.203329
3508.636537	978462.021500	44.208333
3508.069880	978287.570822	44.213338
3508.214485	978096.578401	44.218343
3508.169088	977940.600692	44.223348
3508.188302	977761.541589	44.228353
3508.135639	977591.090071	44.233357
3508.136440	977397.458959	44.238362
3508.124316	977233.539083	44.243367
3508.430678	977054.899324	44.248372
3508.043599	976892.595471	44.253377
3508.357649	976704.265811	44.258381
3508.253449	976547.868805	44.263386
3508.396038	976366.790550	44.268391
3508.558592	976194.013431	44.273396
3508.335658	976018.557053	44.278401
3508.312523	975843.551251	44.283405
3508.332537	975651.520062	44.288410
3508.238937	975476.123540	44.293415
3508.311075	975294.631885	44.298420
3507.828750	975125.057757	44.303425
3507.981499	974969.748749	44.308429
3508.251044	974785.470410	44.313434
3508.167353	974620.216247	44.318439
3508.588981	974423.090287	44.323444
3507.938829	974262.124350	44.328449
3507.848715	974076.219863	44.333453
3508.265219	973908.417729	44.338458
3508.178160	973743.041026	44.343463
3508.164354	973574.810967	44.348468
3507.930140	973404.362555	44.353473
3507.867202	973240.336775	44.358477
3507.972531	973058.866679	44.363482
3507.659110	972895.067920	44.368487
3508.063464	972720.189796	44.373492
3507.787143	972576.625701	44.378497
3507.984381	972384.945021	44.383501
3507.429091	972223.025699	44.388506
3507.469848	972052.491815	44.393511
3507.777231	971903.335851	44.398516
3507.521974	971743.212517	44.403521
3507.599259	971581.366575	44.408525
3507.660672	971415.800467	44.413530
3507.419152	971246.952555	44.418535
3507.184059	971095.810094	44.423540
3507.220557	970934.344041	44.428545
3507.578456	970780.844928	44.433549
3507.255348	970630.096136	44.438554
3507.064230	970473.743404	44.443559
3507.496188	970320.415517	44.448564
3507.361444	970164.240805	44.453569
3507.364144	969998.447757	44.458573
3507.865814	969855.470409	44.463578
3507.387627	969696.305432	44.468583
3507.931778	969522.285651	44.473588
3507.613953	969370.719883	44.478593
3507.638900	969204.215071	44.483597
3507.698808	969042.887758	44.488602
3507.406457	968887.683179	44.493607
3507.537320	968730.251040	44.498612
3507.454430	968580.779392	44.503617
3507.337679	968421.519552	44.508621
3507.187160	968258.540599	44.513626
3507.252008	968103.451806	44.518631
3507.547805	967945.383580	44.523636
3507.209808	967797.598001	44.528641
3507.277086	967652.875053	44.533645
3507.350248	967501.195564	44.538650
3506.700702	967345.224838	44.543655
3507.042662	967193.982558	44.548660
3506.842647	967049.484289	44.553665
3506.743008	966897.621497	44.558669
3507.177375	966744.883320	44.563674
3507.258189	966595.333086	44.568679
3507.495346	966454.567133	44.573684
3507.099341	966290.789373	44.578689
3506.938952	966144.401069	44.583693
3507.110816	965991.490261	44.588698
3506.702990	965842.686528	44.593703
3507.084782	965694.140667	44.598708
3507.342698	965554.916417	44.603713
3507.126361	965398.233828	44.608717
3507.415541	965239.406695	44.613722
3507.257372	965097.497231	44.618727
3507.094866	964941.576987	44.623732
3507.008272	964800.334114	44.628737
3506.963168	964655.358348	44.633741
3507.165891	964496.524966	44.638746
3506.965363	964357.053366	44.643751
3507.150885	964198.802416	44.648756
3506.992214	964047.853841	44.653761
3506.896469	963897.282849	44.658765
3507.219424	963743.797580	44.663770
3506.795812	963600.621217	44.668775
3507.182407	963456.230026	44.673780
3507.087018	963315.246125	44.678785
3507.318296	963169.011592	44.683789
3507.126392	963009.614283	44.688794
3507.047075	962864.207101	44.693799
3506.978176	962706.937014	44.698804
3507.199005	962574.898550	44.703809
3507.051836	962405.873322	44.708813
3507.272454	962274.808033	44.713818
3506.993624	962141.273881	44.718823
3507.045730	961978.377651	44.723828
3506.844943	961839.629201	44.728833
3506.817937	961692.713681	44.733837
3507.212412	961540.628169	44.738842
3507.026316	961407.061731	44.743847
3507.130791	961245.508428	44.748852
3507.178016	961105.035091	44.753857
3506.912234	960940.299451	44.758861
3507.194912	960805.367523	44.763866
3506.892477	960649.452166	44.768871
3507.302191	960502.042258	44.773876
3506.707578	960353.029359	44.778881
3507.034727	960226.507674	44.783885
3506.788366	960073.508657	44.788890
3506.629275	959922.550121	44.793895
3506.747378	959782.817260	44.798900
3506.518361	959636.863101	44.803905
3506.951805	959504.131028	44.808909
3506.865975	959352.263051	44.813914
3506.620483	959230.618460	44.818919
3506.676375	959062.638440	44.823924
3506.470861	958953.925082	44.828929
3506.701023	958810.031698	44.833933
3506.866156	958657.515731	44.838938
3506.545336	958527.827402	44.843943
3506.696933	958373.933234	44.848948
3506.462603	958255.306409	44.853953
3506.636365	958115.524024	44.858957
3506.595921	957976.558151	44.863962
3506.350840	957851.353667	44.868967
3506.488738	957691.755015	44.873972
3506.261196	957559.577535	44.878977
3506.273029	957422.747564	44.883981
3506.396188	957295.606745	44.888986
3505.928808	957165.519598	44.893991
3506.322826	957031.756306	44.898996
3506.215083	956923.871448	44.904001
3506.396166	956764.828646	44.909005
3506.335781	956654.772827	44.914010
3506.228548	956501.361901	44.919015
3506.466633	956367.020305	44.924020
3506.440620	956232.326664	44.929025
3506.563128	956104.865439	44.934029
3506.504213	955970.367329	44.939034
3506.378829	955827.144988	44.944039
3506.529591	955701.301503	44.949044
3506.413994	955564.484257	44.954049
3506.264997	955438.092149	44.959053
3506.183068	955305.469964	44.964058
3506.180122	955200.181888	44.969063
3506.248507	955060.643123	44.974068
3506.301451	954931.431795	44.979073
3506.101350	954809.623036	44.984077
3505.906527	954687.332291	44.989082
3505.602421	954556.831303	44.994087
3505.868802	954430.250122	44.999092
3505.793267	954317.017166	45.004097
3505.808380	954202.332017	45.009101
3506.078888	954066.558742	45.014106
3505.938758	953957.441496	45.019111
3506.208713	953835.245073	45.024116
3505.914542	953718.112911	45.029121
3506.076725	953595.545869	45.034125
3506.306679	953459.476153	45.039130
3505.851410	953340.448586	45.044135
3505.783034	953223.554887	45.049140
3506.040950	953105.552396	45.054145
3506.209625	952974.454721	45.059149
3505.891718	952868.787720	45.064154
3505.594316	952756.226424	45.069159
3506.226215	952621.694718	45.074164
3506.063106	952506.235418	45.079169
3505.729183	952376.162013	45.084173
3505.919481	952253.462493	45.089178
3505.562202	952152.571495	45.094183
3505.876111	952035.970448	45.099188
3505.621061	951928.168477	45.104193
3505.669080	951796.294966	45.109197
3505.994942	951689.349238	45.114202
3505.536738	951570.855152	45.119207
3505.569577	951452.181743	45.124212
3505.616366	951331.972035	45.129217
3505.664570	951228.890581	45.134221
3505.486616	951112.732380	45.139226
3505.507562	951007.832530	45.144231
3505.599863	950881.383645	45.149236
3505.730830	950780.959497	45.154241
3505.953607	950657.067871	45.159245
3505.632753	950530.391248	45.164250
3505.396682	950419.970049	45.169255
3505.827272	950304.937707	45.174260
3505.680304	950193.444014	45.179265
3505.444610	950079.186439	45.184269
3505.416838	949974.273509	45.189274
3505.522951	949861.199265	45.194279
3505.968669	949751.991652	45.199284
3505.665832	949631.991219	45.204289
3505.454987	949509.483660	45.209293
3505.628570	949396.100873	45.214298
3505.569319	949287.923988	45.219303
3505.590847	949177.242192	45.224308
3505.263075	949069.870904	45.229313
3505.435311	948963.755486	45.234317
3505.992670	948849.052730	45.239322
3505.382047	948737.412360	45.244327
3505.590186	948621.325783	45.249332
3505.619441	948502.201860	45.254337
3505.433049	948405.039332	45.259341
3505.219860	948280.204732	45.264346
3505.284622	948184.050036	45.269351
3505.316315	948068.746186	45.274356
3505.462522	947967.115471	45.279361
3505.288495	947865.918574	45.284365
3505.512406	947741.286247	45.289370
3505.304875	947641.527025	45.294375
3505.385126	947536.929773	45.299380
3505.269573	947428.148507	45.304385
3505.367444	947329.194935	45.309389
3505.640570	947220.153718	45.314394
3505.310300	947111.018024	45.319399
3505.424221	947006.691844	45.324404
3505.002245	946887.221856	45.329409
3505.050212	946768.821162	45.334413
3505.227285	946688.042028	45.339418
3504.754991	946597.118911	45.344423
3505.141999	946481.146371	45.349428
3505.131621	946372.421370	45.354433
3505.128442	946273.368454	45.359437
3505.346793	946152.913865	45.364442
3504.900033	946066.096598	45.369447
3505.101514	945950.621751	45.374452
3505.144719	945875.696007	45.379457
3504.887571	945762.591828	45.384461
3504.954441	945658.342042	45.389466
3504.844653	945565.329107	45.394471
3504.935897	945471.514893	45.399476
3504.929852	945373.211746	45.404481
3504.776756	945274.930957	45.409485
3505.101312	945157.214410	45.414490
3504.633249	945072.300361	45.419495
3504.781506	944982.588164	45.424500
3504.750035	944890.795914	45.429505
3504.786486	944791.803995	45.434509
3504.931150	944698.062830	45.439514
3504.466620	944606.816023	45.444519
3504.872768	944520.311526	45.449524
3504.704147	944422.687970	45.454529
3504.533017	944333.112997	45.459533
3504.917350	944222.169584	45.464538
3504.490301	944128.033131	45.469543
3504.816502	944044.409001	45.474548
3504.864174	943952.587145	45.479553
3504.652977	943859.368676	45.484557
3504.679701	943760.742095	45.489562
3504.573692	943676.704029	45.494567
3504.507316	943582.594139	45.499572
3504.974380	943488.394684	45.504577
3504.573582	943401.525263	45.509581
3504.819404	943294.323061	45.514586
3503.976169	943203.593259	45.519591
3503.962759	943105.344289	45.524596
3504.027716	943020.979912	45.529601
3504.572009	942965.580420	45.534605
3504.701411	942863.277309	45.539610
3504.241589	942800.180894	45.544615
3504.714654	942701.460741	45.549620
3504.468918	942630.849667	45.554625
3504.323460	942534.720716	45.559629
3504.598248	942436.219937	45.564634
3504.188483	942348.567486	45.569639
3504.389179	942259.758425	45.574644
3504.492947	942177.674931	45.579649
3504.463134	942095.132777	45.584653
3504.552697	942002.886171	45.589658
3504.332180	941912.031299	45.594663
3504.578328	941834.712854	45.599668
3504.415519	941750.173688	45.604673
3503.853095	941663.206033	45.609677
3503.975811	941556.659586	45.614682
3504.041499	941494.707311	45.619687
3504.051148	941400.066086	45.624692
3503.988761	941338.133051	45.629697
3504.045202	941264.385287	45.634701
3504.147284	941164.930093	45.639706
3503.701222	941106.797282	45.644711
3504.302756	941014.640692	45.649716
3504.075175	940933.838867	45.654721
3503.747396	940851.326145	45.659725
3504.192837	940756.889195	45.664730
3503.873861	940706.115215	45.669735
3504.007834	940648.169466	45.674740
3504.016679	940550.827781	45.679745
3504.183384	940467.460337	45.684749
3504.211644	940399.171567	45.689754
3504.000966	940331.304891	45.694759
3504.408248	940224.780365	45.699764
3504.328303	940161.685394	45.704769
3504.161401	940074.530249	45.709773
3504.303372	939996.626344	45.714778
3504.128319	939922.801901	45.719783
3504.411997	939830.101358	45.724788
3504.131693	939749.481770	45.729793
3504.137465	939674.760792	45.734797
3504.327705	939590.032656	45.739802
3504.281855	939511.864726	45.744807
3504.171718	939425.264969	45.749812
3504.105015	939343.740649	45.754817
3504.103134	939247.623556	45.759821
3503.989684	939103.654590	45.764826
3503.650465	938895.731894	45.769831
3503.793946	938660.379378	45.774836
3503.904932	938346.540810	45.779841
3503.731882	937976.024241	45.784845
3503.589020	937538.210596	45.789850
3503.765036	937032.747668	45.794855
3503.633230	936471.044610	45.799860
3503.672565	935835.246718	45.804865
3503.904528	935142.124072	45.809869
3503.558304	934374.498508	45.814874
3503.196435	933534.549834	45.819879
3503.389671	932618.211976	45.824884
3503.118590	931639.735199	45.829889
3503.008645	930588.605506	45.834893
3502.829981	929443.002632	45.839898
3502.457835	928259.024548	45.844903
3502.543531	926955.582408	45.849908
3502.464180	925605.303810	45.854913
3501.993314	924163.940533	45.859917
3502.328876	922630.549805	45.864922
3501.763132	921024.298356	45.869927
3501.927853	919315.680052	45.874932
3501.818167	917536.165197	45.879937
3501.394365	915666.230778	45.884941
3501.152319	913698.283580	45.889946
3500.644064	911655.532222	45.894951
3500.606538	909545.299123	45.899956
3500.297274	907344.474840	45.904961
3499.964676	905026.175371	45.909965
3499.855017	902635.319443	45.914970
3499.235720	900160.636223	45.919975
3499.231755	897610.341995	45.924980
3499.038673	894949.466503	45.929985
3498.398334	892218.056620	45.934989
3498.113606	889383.556115	45.939994
3497.758061	886481.338122	45.944999
3497.287773	883485.542761	45.950004
3496.677557	880415.720446	45.955009
3496.156394	877232.249125	45.960013
3495.741593	873975.522479	45.965018
3495.318867	870637.780207	45.970023
3495.071526	867219.841801	45.975028
3494.508333	863698.917193	45.980033
3493.984375	860111.749253	45.985037
3493.749838	856417.900687	45.990042
3492.797535	852650.769546	45.995047
3492.567786	848805.131393	46.000052
3491.874464	844847.561278	46.005057
3491.435277	840815.221278	46.010061
3491.120155	836706.646813	46.015066
3490.355465	832519.172258	46.020071
3489.895834	828209.479761	46.025076
3489.245179	823837.651990	46.030081
3488.580511	819371.895394	46.035085
3488.293186	814808.900998	46.040090
3487.448761	810175.909423	46.045095
3486.674036	805439.060091	46.050100
3485.993036	800635.079940	46.055105
3485.340723	795737.795962	46.060109
3484.762652	790745.765978	46.065114
3484.150485	785684.720768	46.070119
3483.167833	780510.361696	46.075124
3482.467889	775260.360691	46.080129
3481.457429	769948.551218	46.085133
3480.850679	764507.349115	46.090138
3479.880124	759014.597210	46.095143
3479.020855	753419.326165	46.100148
3478.250340	747735.757646	46.105153
3477.312837	741974.385782	46.110157
3476.922668	736109.783251	46.115162
3475.308512	730176.462177	46.120167
3474.882329	724133.382408	46.125172
3474.122011	718015.452998	46.130177
3472.960005	711793.544067	46.135181
3472.301562	705499.103000	46.140186
3470.915409	699110.072201	46.145191
3469.996656	692617.467879	46.150196
3468.842765	686078.977410	46.155201
3467.952682	679422.941710	46.160205
3467.189099	672693.899405	46.165210
3465.933513	665862.141804	46.170215
3465.002204	658960.218278	46.175220
3463.606215	651956.670832	46.180225
3462.434355	644882.326738	46.185229
3461.562804	637700.043398	46.190234
3460.299602	630454.336689	46.195239
3458.997368	623111.449365	46.200244
3458.123334	615703.362317	46.205249
3456.476493	608181.781431	46.210253
3455.745166	600587.043632	46.215258
3453.715474	592911.552152	46.220263
3452.763218	585122.704156	46.225268
3451.606327	577302.025344	46.230273
3449.958670	569346.533220	46.235277
3448.709936	561339.484160	46.240282
3447.358022	553253.938964	46.245287
3445.532801	545061.717248	46.250292
3444.193568	536806.016459	46.255297
3442.895378	528450.647474	46.260301
3441.491882	520019.413990	46.265306
3439.829481	511520.713619	46.270311
3438.260651	502907.053252	46.275316
3436.603345	494249.487871	46.280321
3434.698217	485506.128282	46.285325
3433.319424	476684.337539	46.290330
3431.554331	467785.748901	46.295335
3429.796668	458802.665914	46.300340
3427.944456	449749.428086	46.305345
3426.318130	440597.922145	46.310349
3424.260142	431390.913352	46.315354
3422.326128	422131.843383	46.320359
3420.224880	412768.431327	46.325364
3418.467886	403329.826719	46.330369
3416.182528	393830.513389	46.335373
3414.503464	384257.240872	46.340378
3411.804602	374629.118883	46.345383
3409.894255	364922.726624	46.350388
3407.693653	355169.140545	46.355393
3405.600979	345351.492722	46.360397
3403.259792	335447.433486	46.365402
3400.704485	325509.177765	46.370407
3398.349025	315475.320961	46.375412
3395.934696	305430.443140	46.380417
3392.814952	295315.256857	46.385421
3390.386474	285134.145292	46.390426
3387.579179	274906.273047	46.395431
3384.771358	264643.089827	46.400436
3382.268411	254316.053802	46.405441
3378.708969	243956.551271	46.410445
3375.951181	233537.964490	46.415450
3372.863318	223094.735246	46.420455
3369.652695	212532.972826	46.425460
3366.493207	202004.918752	46.430465
3362.596987	191463.364870	46.435469
3359.543388	180902.670354	46.440474
3355.488243	170313.071944	46.445479
3351.746101	159715.395267	46.450484
3347.926486	149092.585617	46.455489
3343.279478	138482.415069	46.460493
3339.036571	127830.493454	46.465498
3334.059732	117240.399694	46.470503
3329.579639	106617.239317	46.475508
3323.651058	96038.391368	46.480513
3317.138770	85479.275380	46.485517
3310.273496	74997.082014	46.490522
3300.851396	64628.636427	46.495527
3283.575916	54577.464666	46.500532
3250.373497	45141.492177	46.505537
3206.945659	36365.063829	46.510541
3158.364195	28370.518173	46.515546
3108.159017	21239.228018	46.520551
3061.107758	15020.690300	46.525556
3018.858575	9718.595977	46.530561
2981.674579	5319.874109	46.535565
2947.671510	1887.745228	46.540570
2878.934318	359.216819	46.545575
2798.539110	355.452553	46.550580
2772.186570	322.539353	46.555585
2787.222401	325.696057	46.560589
2824.250889	335.485305	46.565594
2862.549047	329.334370	46.570599
2890.479154	327.492414	46.575604
2905.592339	308.032615	46.580609
2907.900496	326.588542	46.585613
2903.913820	314.537118	46.590618
2897.290310	315.727114	46.595623
2890.816058	326.625551	46.600628
2886.395230	318.829611	46.605633
2882.982669	304.928259	46.610637
2880.690132	311.083827	46.615642
2878.543888	290.869189	46.620647
2876.746705	313.584467	46.625652
2874.813967	291.613660	46.630657
2871.983676	294.252178	46.635661
2869.963790	288.358036	46.640666
2866.877095	292.861011	46.645671
2863.583372	294.660254	46.650676
2860.403304	298.795564	46.655681
2857.106810	293.440493	46.660685
2854.399147	289.828291	46.665690
2851.412675	281.278994	46.670695
2848.213166	289.699461	46.675700
2844.833906	275.706447	46.680705
2841.503526	285.102543	46.685709
2838.465470	281.835347	46.690714
2835.366263	289.675590	46.695719
2832.249880	269.422359	46.700724
2829.240395	280.689542	46.705729
2825.522094	288.948721	46.710733
2822.142880	287.662852	46.715738
2818.815841	296.002351	46.720743
2815.666083	290.870723	46.725748
2812.384502	278.040996	46.730753
2809.175500	284.959991	46.735757
2806.285422	269.331912	46.740762
2802.818290	288.369135	46.745767
2799.173418	268.077178	46.750772
2795.853021	279.773955	46.755777
2791.939701	283.085987	46.760781
2789.165878	269.832023	46.765786
2785.934920	269.240303	46.770791
2782.127249	270.784360	46.775796
2778.765431	250.631238	46.780801
2775.551626	268.763088	46.785805
2772.140641	253.693267	46.790810
2768.694545	273.099713	46.795815
2765.190421	263.573936	46.800820
2761.714293	275.146248	46.805825
2758.268635	274.871685	46.810829
2755.310185	261.989418	46.815834
2751.712059	275.972060	46.820839
2748.519513	263.311488	46.825844
2745.543508	264.850140	46.830849
2741.512335	243.454021	46.835853
2738.445181	257.980372	46.840858
2735.216317	251.463957	46.845863
2731.167778	258.090382	46.850868
2727.283715	264.086443	46.855873
2723.669134	251.096239	46.860877
2720.927261	263.673691	46.865882
2717.323501	268.524671	46.870887
2713.512070	267.544215	46.875892
2710.873496	262.635068	46.880897
2707.775637	255.108584	46.885901
2704.170733	264.017459	46.890906
2700.009258	250.938292	46.895911
2696.611890	261.070746	46.900916
2693.824448	243.158147	46.905921
2689.577721	261.338089	46.910925
2686.644477	247.880921	46.915930
2682.923265	255.921812	46.920935
2679.217628	258.390319	46.925940
2675.794627	242.018682	46.930945
2672.500632	256.844861	46.935949
2668.838493	234.162326	46.940954
2665.250744	246.566131	46.945959
2662.045365	245.340068	46.950964
2658.567208	247.029123	46.955969
2655.166857	251.049093	46.960973
2652.338074	258.524273	46.965978
2649.056206	245.784189	46.970983
2645.174550	249.779151	46.975988
2641.770272	246.173391	46.980993
2638.114294	251.043960	46.985997
2634.349536	248.050282	46.991002
2631.028740	243.220221	46.996007
2627.380702	259.552392	47.001012
2624.170799	235.030852	47.006017
2620.459894	251.836843	47.011021
2616.864261	235.834257	47.016026
2613.893568	242.577276	47.021031
2610.371083	244.697661	47.026036
2606.848132	236.603060	47.031041
2603.414638	258.131001	47.036045
2599.595217	234.961268	47.041050
2596.167493	246.729050	47.046055
2592.956867	233.425606	47.051060
2589.462047	237.082951	47.056065
2586.051342	239.950936	47.061069
2582.351299	241.267015	47.066074
2578.703396	222.917806	47.071079
2575.025590	240.586069	47.076084
2572.148920	234.682884	47.081089
2568.555207	249.815590	47.086093
2564.893979	227.026447	47.091098
2561.778087	232.375519	47.096103
2558.250607	238.105680	47.101108
2554.906209	226.586516	47.106113
2550.948391	235.001383	47.111117
2547.456792	222.559357	47.116122
2543.879739	246.937793	47.121127
2540.248419	241.449982	47.126132
2537.036163	223.230208	47.131137
2533.565427	251.336284	47.136141
2530.188102	232.129991	47.141146
2526.642557	251.058333	47.146151
2522.899738	235.681551	47.151156
2519.739274	225.942311	47.156161
2516.172259	237.200764	47.161165
2512.523650	231.177783	47.166170
2509.787901	241.763588	47.171175
2506.283498	235.217953	47.176180
2502.606229	228.609479	47.181185
2498.293489	235.045472	47.186189
2495.016098	229.459864	47.191194
2491.530727	226.808777	47.196199
2488.340791	216.281864	47.201204
2484.841114	228.771322	47.206209
2481.066529	220.028138	47.211213
2477.758755	219.554283	47.216218
2474.583357	214.966193	47.221223
2470.930180	232.391584	47.226228
2467.605250	206.114745	47.231233
2464.020558	231.073015	47.236237
2460.530061	211.228842	47.241242
2456.742285	222.321774	47.246247
2453.192612	219.875455	47.251252
2449.831614	223.706016	47.256257
2446.282637	227.529006	47.261261
2443.211631	214.225723	47.266266
2439.623253	226.444822	47.271271
2435.767445	222.807681	47.276276
2432.515600	229.958573	47.281281
2428.848389	219.607569	47.286285
2425.476031	216.130822	47.291290
2421.936939	216.278261	47.296295
2418.528003	228.259328	47.301300
2415.273017	214.311240	47.306305
2411.370271	217.872071	47.311309
2408.174761	203.687786	47.316314
2404.587922	212.563086	47.321319
2400.916043	209.140780	47.326324
2397.360634	215.041928	47.331329
2394.125098	220.020231	47.336333
2390.317244	208.356730	47.341338
2386.948855	210.115498	47.346343
2383.632736	224.875925	47.351348
2380.247106	218.134588	47.356353
2376.389321	214.891520	47.361357
2373.108654	202.278790	47.366362
2369.510764	222.195169	47.371367
2366.018576	214.300733	47.376372
2362.589833	214.773697	47.381377
2359.179274	224.288401	47.386381
2355.645288	223.935563	47.391386
2352.085654	211.075262	47.396391
2348.602840	209.377872	47.401396
2345.180387	205.092409	47.406401
2341.129830	204.117454	47.411405
2338.071296	207.224392	47.416410
2334.649823	201.826988	47.421415
2331.049542	216.205752	47.426420
2327.856830	196.868961	47.431425
2324.322998	204.542176	47.436429
2320.679979	216.494791	47.441434
2317.423286	209.172682	47.446439
2313.399954	216.482616	47.451444
2310.469475	204.247013	47.456449
2306.438840	213.343126	47.461453
2302.918320	215.090719	47.466458
2299.623850	207.549830	47.471463
2296.128910	216.159051	47.476468
2292.672089	214.355790	47.481473
2289.040254	216.039574	47.486477
2285.976635	206.340234	47.491482
2282.371410	198.279331	47.496487
2278.695998	213.591891	47.501492
2275.162255	193.294108	47.506497
2271.593317	199.528207	47.511501
2267.992294	202.144288	47.516506
2264.436545	201.827935	47.521511
2260.970138	210.221940	47.526516
2258.054671	192.667257	47.531521
2254.211937	209.142583	47.536525
2250.601381	204.105603	47.541530
2247.086698	206.044330	47.546535
2243.253320	209.090092	47.551540
2239.968210	208.618228	47.556545
2236.811731	213.059224	47.561549
2233.571093	211.450782	47.566554
2229.850119	227.862449	47.571559
2226.351737	216.127087	47.576564
2222.780332	211.056928	47.581569
2218.860732	212.594756	47.586573
2215.498595	207.659664	47.591578
2212.125554	209.270708	47.596583
2208.484974	201.636321	47.601588
2205.340537	204.324996	47.606593
2201.882092	210.809526	47.611597
2198.216921	193.233226	47.616602
2194.912767	199.535452	47.621607
2191.054055	188.217668	47.626612
2187.806142	192.413324	47.631617
2183.833756	189.424848	47.636621
2180.566738	207.315462	47.641626
2177.526979	196.309973	47.646631
2173.844917	201.216894	47.651636
2170.795976	198.631303	47.656641
2166.691603	199.885633	47.661645
2162.957032	201.571327	47.666650
2159.668597	200.808143	47.671655
2156.163530	192.316564	47.676660
2152.794969	193.661626	47.681665
2149.104953	191.314871	47.686669
2145.836456	187.835637	47.691674
2142.463794	193.011059	47.696679
2138.404893	197.003819	47.701684
2135.240845	198.468258	47.706689
2131.617996	200.120050	47.711693
2128.225142	204.394392	47.716698
2124.733803	189.138324	47.721703
2121.188139	206.301799	47.726708
2117.747701	193.088265	47.731713
2114.274449	209.805939	47.736717
2110.496452	200.653860	47.741722
2107.063002	190.003385	47.746727
2103.748486	199.832009	47.751732
2100.542691	188.508286	47.756737
2096.773502	208.055321	47.761741
2093.134744	185.292082	47.766746
2089.761157	183.058597	47.771751
2086.169222	185.543240	47.776756
2082.754599	188.222077	47.781761
2079.054363	189.090755	47.786765
2075.400670	185.610187	47.791770
2072.104138	184.440660	47.796775
2068.505877	191.938349	47.801780
2065.300130	179.551891	47.806785
2061.827060	193.198377	47.811789
2058.209616	188.293059	47.816794
2054.738008	195.099339	47.821799
2051.440394	191.743925	47.826804
2047.900501	187.702615	47.831809
2044.059248	191.538772	47.836813
2040.521783	205.502796	47.841818
2037.312273	186.547690	47.846823
2033.635470	198.166319	47.851828
2030.069064	186.968713	47.856833
2026.521228	199.742368	47.861837
2023.121606	203.012136	47.866842
2019.888817	179.195294	47.871847
2016.309549	203.197893	47.876852
2013.044218	186.299682	47.881857
2008.608505	195.451500	47.886861
2005.788304	194.975059	47.891866
2002.447948	188.485323	47.896871
1998.715179	182.989707	47.901876
1995.622645	177.126657	47.906881
1991.832749	185.705519	47.911885
1987.916785	186.065483	47.916890
1984.551774	177.969968	47.921895
1981.062850	192.191754	47.926900
1977.493098	174.463455	47.931905
1974.237173	182.540693	47.936909
1971.021817	182.071946	47.941914
1967.251695	184.885245	47.946919
1963.306958	183.167774	47.951924
1960.288513	181.751473	47.956929
1956.525209	185.237330	47.961933
1953.093281	200.690542	47.966938
1949.949606	174.536845	47.971943
1946.597319	188.379184	47.976948
1942.455141	170.890760	47.981953
1939.168394	180.843388	47.986957
1935.584269	191.083127	47.991962
1932.364495	187.451436	47.996967
1928.736169	194.136142	48.001972
1925.262557	171.729253	48.006977
1921.446237	185.853739	48.011981
1918.028863	172.953403	48.016986
1914.789718	188.159161	48.021991
1911.193893	190.385672	48.026996
1907.824958	186.828421	48.032001
1904.154216	171.754722	48.037005
1900.857221	184.526778	48.042010
1897.063482	192.755916	48.047015
1893.521073	200.511609	48.052020
1890.350256	177.643213	48.057025
1886.588338	183.756301	48.062029
1882.965813	172.502258	48.067034
1879.796976	180.642305	48.072039
1876.168365	173.269050	48.077044
1872.665927	170.091945	48.082049
1869.257171	182.446419	48.087053
1865.624273	181.298551	48.092058
1861.890407	168.612748	48.097063
1858.305696	185.061695	48.102068
1855.542901	176.571928	48.107073
1851.506043	177.478995	48.112077
1848.237819	189.399421	48.117082
1844.545281	175.754936	48.122087
1840.610444	186.224816	48.127092
1837.657023	179.183607	48.132097
1833.793772	193.563585	48.137101
1830.420589	188.073941	48.142106
1827.189238	177.265501	48.147111
1823.772374	191.119818	48.152116
1820.455079	172.443782	48.157121
1816.850613	181.981869	48.162125
1813.500082	183.191621	48.167130
1810.054994	183.534360	48.172135
1805.948156	178.985954	48.177140
1802.691876	181.290950	48.182145
1798.976270	177.834759	48.187149
1795.410355	174.685232	48.192154
1792.070030	172.745709	48.197159
1788.370998	196.702903	48.202164
1785.431128	172.468464	48.207169
1781.611798	188.022039	48.212173
1777.766354	187.072946	48.217178
1774.548126	173.243906	48.222183
1771.257634	165.332236	48.227188
1767.535863	182.129267	48.232193
1764.009514	174.794249	48.237197
1760.365754	176.484986	48.242202
1757.194069	162.639406	48.247207
1753.619599	175.948560	48.252212
1750.060897	170.089455	48.257217
1746.410639	170.794877	48.262221
1743.088604	164.623370	48.267226
1740.046448	169.324662	48.272231
1735.798268	184.153607	48.277236
1732.617754	176.028381	48.282241
1728.851679	188.497111	48.287245
1725.336518	176.133499	48.292250
1722.074960	176.961044	48.297255
1718.577396	177.228042	48.302260
1715.172957	171.479342	48.307265
1711.780738	176.827247	48.312269
1708.288351	174.004198	48.317274
1704.807123	180.948831	48.322279
1700.947437	176.657727	48.327284
1697.661085	165.658387	48.332289
1693.516675	176.714650	48.337293
1690.338715	167.474196	48.342298
1687.342085	169.095964	48.347303
1683.894665	179.203833	48.352308
1680.434339	159.175254	48.357313
1676.484099	157.658030	48.362317
1672.880257	155.823510	48.367322
1669.252467	152.083989	48.372327
1665.734601	171.650406	48.377332
1662.643445	169.529846	48.382337
1658.903844	167.174178	48.387341
1655.375667	180.656851	48.392346
1652.397381	167.049220	48.397351
1648.449724	168.226184	48.402356
1645.044007	168.340348	48.407361
1641.466875	164.869090	48.412365
1638.044498	165.213491	48.417370
1634.582021	160.292414	48.422375
1630.667616	170.680478	48.427380
1627.549673	165.758283	48.432385
1623.859015	185.296324	48.437389
1620.600743	162.161323	48.442394
1616.941729	163.548538	48.447399
1613.100545	170.689137	48.452404
1610.117095	182.443768	48.457409
1606.404638	167.320437	48.462413
1602.883777	178.515236	48.467418
1599.602924	161.638130	48.472423
1596.079873	179.051137	48.477428
1592.760410	149.539045	48.482433
1589.272980	160.608658	48.487437
1585.517490	156.658628	48.492442
1582.058059	163.149869	48.497447
1578.173361	156.111456	48.502452
1574.943509	154.063645	48.507457
1571.213638	168.113806	48.512461
1567.474981	167.147011	48.517466
1564.400967	165.083646	48.522471
1560.900042	166.163650	48.527476
1557.556479	155.456273	48.532481
1553.813305	170.142161	48.537485
1550.322195	166.651034	48.542490
1547.007901	172.524967	48.547495
1543.440759	160.678498	48.552500
1540.409306	170.563085	48.557505
1536.419721	164.522081	48.562509
1532.968056	176.097812	48.567514
1529.209233	158.225450	48.572519
1525.802144	172.355932	48.577524
1522.404026	157.363982	48.582529
1518.667726	157.015648	48.587533
1515.338173	155.550861	48.592538
1512.324292	162.683604	48.597543
1508.542586	155.647178	48.602548
1505.151387	157.811402	48.607553
1501.176363	159.729080	48.612557
1497.576541	155.721644	48.617562
1494.505265	147.849620	48.622567
1490.814733	174.438687	48.627572
1487.363746	152.879358	48.632577
1484.100505	157.892857	48.637581
1480.711362	160.054879	48.642586
1477.267155	162.947903	48.647591
1473.210127	158.930114	48.652596
1469.929076	181.249079	48.657601
1466.472340	167.117381	48.662605
1462.666091	173.359316	48.667610
1459.299062	165.012683	48.672615
1455.856493	166.448601	48.677620
1452.598979	149.878398	48.682625
1448.332459	162.863773	48.687629
1445.033434	161.644154	48.692634
1442.111332	161.141256	48.697639
1438.510329	152.460664	48.702644
1434.976555	157.171294	48.707649
1431.392436	163.706854	48.712653
1427.544125	168.616985	48.717658
1424.379673	147.412608	48.722663
1420.638751	156.263193	48.727668
1417.137865	154.589088	48.732673
1413.859513	155.764420	48.737677
1410.170573	168.224575	48.742682
1407.010000	140.159446	48.747687
1403.328081	166.749862	48.752692
1399.867621	148.934506	48.757697
1396.548096	166.843219	48.762701
1392.996783	149.224377	48.767706
1389.398076	155.302756	48.772711
1385.934845	169.544749	48.777716
1382.065845	149.641559	48.782721
1378.594996	167.832433	48.787725
1375.375429	155.864188	48.792730
1372.114458	166.793520	48.797735
1368.174892	159.041003	48.802740
1364.778871	167.932154	48.807745
1361.284039	152.699889	48.812749
1357.916954	159.880530	48.817754
1354.464902	133.395086	48.822759
1350.391082	156.286153	48.827764
1347.192989	142.814243	48.832769
1343.306401	167.409848	48.837773
1339.897697	153.496815	48.842778
1336.993512	152.100998	48.847783
1333.522990	156.709392	48.852788
1329.998107	160.252577	48.857793
1326.270197	153.493763	48.862797
1322.554513	167.918219	48.867802
1319.506094	151.965455	48.872807
1315.721518	165.089454	48.877812
1312.206794	159.405154	48.882817
1308.393774	173.052848	48.887821
1304.755120	164.985925	48.892826
1302.040635	165.723751	48.897831
1298.232402	155.389176	48.902836
1294.430418	172.238469	48.907841
1291.148584	155.780892	48.912845
1287.842604	158.459512	48.917850
1284.333096	149.162748	48.922855
1280.656628	148.288933	48.927860
1277.352305	152.210748	48.932865
1273.441934	160.186047	48.937869
1269.948629	160.717832	48.942874
1266.738112	148.947138	48.947879
1263.546699	163.263071	48.952884
1260.053529	153.989171	48.957889
1256.105752	155.585627	48.962893
1252.657166	159.660597	48.967898
1249.051472	146.653877	48.972903
1245.486164	159.114102	48.977908
1242.154919	152.692345	48.982913
1238.539858	164.897498	48.987917
1234.868899	150.992610	48.992922
1231.825088	156.793803	48.997927
1228.357278	169.475888	49.002932
1224.590771	153.076271	49.007937
1220.833462	161.788092	49.012941
1217.223385	151.493074	49.017946
1214.368193	148.534523	49.022951
1210.985214	146.350188	49.027956
1207.493453	142.938082	49.032961
1203.626424	152.216899	49.037965
1199.994736	153.162902	49.042970
1196.902555	149.766023	49.047975
1193.252521	158.773848	49.052980
1189.349915	134.053551	49.057985
1185.896364	160.395202	49.062989
1182.647726	141.384043	49.067994
1179.181997	145.286279	49.072999
1175.481327	158.398156	49.078004
1171.941976	161.656738	49.083009
1168.695193	140.303763	49.088013
1164.935213	154.687046	49.093018
1161.568702	150.603600	49.098023
1157.876073	156.990479	49.103028
1154.959363	146.102394	49.108033
1151.068474	160.702228	49.113037
1147.365742	149.686141	49.118042
1144.185185	153.117917	49.123047
1140.745249	156.616389	49.128052
1137.053165	150.534327	49.133057
1133.498909	147.311131	49.138061
1130.083499	153.350489	49.143066
1126.818956	155.570530	49.148071
1122.977459	157.999469	49.153076
1119.461647	151.371891	49.158081
1116.101859	152.072792	49.163085
1111.855839	158.842956	49.168090
1109.209490	140.451560	49.173095
1105.763991	169.320170	49.178100
1102.420886	146.021020	49.183105
1098.920456	146.605167	49.188109
1095.000827	150.832653	49.193114
1091.420088	141.116482	49.198119
1087.759882	160.137849	49.203124
1084.300678	126.904094	49.208129
1080.946035	149.026317	49.213133
1077.429107	135.873963	49.218138
1073.886083	152.000087	49.223143
1070.782715	144.537553	49.228148
1067.361645	139.849676	49.233153
1063.407691	137.602148	49.238157
1059.617073	146.580755	49.243162
1056.423466	129.585466	49.248167
1052.867131	152.454820	49.253172
1049.486302	148.865758	49.258177
1046.348042	156.676003	49.263181
1042.507155	155.601784	49.268186
1039.043933	143.864570	49.273191
1035.475580	145.782541	49.278196
1032.205367	154.816704	49.283201
1028.561465	147.531728	49.288205
1024.604159	149.590969	49.293210
1021.442260	154.521045	49.298215
1018.203979	136.936031	49.303220
1014.386863	148.489116	49.308225
1011.072803	142.454217	49.313229
1007.388336	143.954659	49.318234
1004.085090	139.726102	49.323239
1000.107343	137.280708	49.328244
996.602678	144.619455	49.333249
993.624909	131.567246	49.338253
990.250156	133.424468	49.343258
986.774605	130.680420	49.348263
983.030191	143.785083	49.353268
979.557519	130.790036	49.358273
975.850019	150.198244	49.363277
972.248694	145.864635	49.368282
968.996041	141.871207	49.373287
965.184652	148.446077	49.378292
961.835086	153.923785	49.383297
958.437652	143.367134	49.388301
954.668751	138.591643	49.393306
951.525475	132.141487	49.398311
947.882281	138.037709	49.403316
944.456895	142.137792	49.408321
941.031795	124.065100	49.413325
937.647182	144.155123	49.418330
934.475763	131.667427	49.423335
930.221648	147.917328	49.428340
926.709405	133.192246	49.433345
923.122774	141.519892	49.438349
919.671708	132.590648	49.443354
916.578410	142.088876	49.448359
912.880973	147.129425	49.453364
909.176050	143.558937	49.458369
905.466390	138.292488	49.463373
902.132516	144.354584	49.468378
898.890509	134.146287	49.473383
894.996644	139.381258	49.478388
891.669592	148.733133	49.483393
888.381837	124.167077	49.488397
884.889185	141.877018	49.493402
881.853797	131.664306	49.498407
877.984605	132.679489	49.503412
874.307962	141.155688	49.508417
870.886521	126.842310	49.513421
866.903806	131.192099	49.518426
863.771469	132.060357	49.523431
860.228042	136.586894	49.528436
856.621004	133.907640	49.533441
853.339472	147.462802	49.538445
849.732296	137.341468	49.543450
846.497450	140.384588	49.548455
842.882758	152.298818	49.553460
839.112154	135.727742	49.558465
835.936864	138.872109	49.563469
832.162891	132.447152	49.568474
828.733420	138.933369	49.573479
825.233968	123.483066	49.578484
821.638834	139.807769	49.583489
818.460068	133.935112	49.588493
814.720158	132.799370	49.593498
811.459945	130.967075	49.598503
807.642495	140.667891	49.603508
804.353995	131.667283	49.608513
800.823161	142.040605	49.613517
797.219764	131.207533	49.618522
793.916069	127.394772	49.623527
790.235270	131.521420	49.628532
786.610205	134.434968	49.633537
783.277914	131.252756	49.638541
779.373888	135.879328	49.643546
776.230688	131.352790	49.648551
772.548111	128.950535	49.653556
769.646844	126.091051	49.658561
765.774700	126.350255	49.663565
762.397312	126.163744	49.668570
758.940851	121.710754	49.673575
754.981728	125.777830	49.678580
751.522940	131.009583	49.683585
748.369953	127.955516	49.688589
744.710127	124.217973	49.693594
741.419891	121.089213	49.698599
737.238972	135.702670	49.703604
734.082219	128.000947	49.708609
730.862714	125.959348	49.713613
727.456313	121.511722	49.718618
723.865639	122.893047	49.723623
720.205989	120.951965	49.728628
716.289125	133.373371	49.733633
713.575980	129.018317	49.738637
709.673136	136.301021	49.743642
706.338529	131.960417	49.748647
702.528953	130.645067	49.753652
699.093511	143.135640	49.758657
695.619825	123.223967	49.763661
691.810115	131.286989	49.768666
688.483549	117.046166	49.773671
685.076160	137.324091	49.778676
681.661099	131.641960	49.783681
678.202188	126.115244	49.788685
674.491827	137.841725	49.793690
671.578094	127.161775	49.798695
667.762939	140.743080	49.803700
664.004328	130.030139	49.808705
660.667962	134.170894	49.813709
657.009880	129.462815	49.818714
653.830043	125.916639	49.823719
650.122022	127.029432	49.828724
646.996087	140.283142	49.833729
643.278835	120.651947	49.838733
639.358512	133.240280	49.843738
635.879796	116.995142	49.848743
632.208633	129.853259	49.853748
628.928015	109.607410	49.858753
625.606667	123.435359	49.863757
622.202800	122.603994	49.868762
618.957312	115.941948	49.873767
615.372832	123.515503	49.878772
611.479349	114.502686	49.883777
608.136390	126.956797	49.888781
604.344423	124.984366	49.893786
600.985371	124.042820	49.898791
597.237106	126.455461	49.903796
594.059753	121.767456	49.908801
590.976557	134.138820	49.913805
587.061805	115.712232	49.918810
583.775589	114.223009	49.923815
580.224047	120.428520	49.928820
576.568463	124.765670	49.933825
572.793269	125.510992	49.938829
568.978311	143.039595	49.943834
566.073919	126.989063	49.948839
562.237295	128.373811	49.953844
559.100658	117.772970	49.958849
555.912966	129.172464	49.963853
551.982182	123.902911	49.968858
548.657235	122.660112	49.973863
544.853178	130.725034	49.978868
541.605458	121.634793	49.983873
538.124292	113.046763	49.988877
534.560798	128.687443	49.993882
531.003528	106.007170	49.998887
527.077909	125.335525	50.003892
523.722519	119.835996	50.008897
520.748635	108.660117	50.013901
517.172653	114.765620	50.018906
513.642303	111.439796	50.023911
510.158746	128.637254	50.028916
506.646675	128.749632	50.033921
503.249425	120.638431	50.038925
499.298701	138.588809	50.043930
495.834058	115.711836	50.048935
492.313545	139.949477	50.053940
489.082406	116.685413	50.058945
485.378011	137.351216	50.063949
481.567475	126.429858	50.068954
478.732721	130.592698	50.073959
475.132190	115.308601	50.078964
471.265696	111.037650	50.083969
467.735356	115.847106	50.088973
464.208970	109.009695	50.093978
460.835892	111.187404	50.098983
457.494677	107.465966	50.103988
453.999793	124.480544	50.108993
450.357081	119.125986	50.113997
446.616685	124.654275	50.119002
443.293697	130.084710	50.124007
439.565533	129.641725	50.129012
436.579111	127.017831	50.134017
433.260380	121.329407	50.139021
429.273874	119.700749	50.144026
425.901057	125.721343	50.149031
422.424479	115.329253	50.154036
418.844380	134.762660	50.159041
415.328951	117.967075	50.164045
411.804199	123.412406	50.169050
408.577148	107.141945	50.174055
404.881289	118.611034	50.179060
401.215948	119.822172	50.184065
398.074260	118.760776	50.189069
394.404287	111.200763	50.194074
390.949319	126.665829	50.199079
387.229364	117.585928	50.204084
383.727933	121.385237	50.209089
380.138444	108.082204	50.214093
376.544010	122.232852	50.219098
373.596039	106.070397	50.224103
369.988289	133.241743	50.229108
366.403159	126.254478	50.234113
363.139281	128.185828	50.239117
359.325107	128.327874	50.244122
355.698289	108.017099	50.249127
351.899727	131.171388	50.254132
348.484594	114.460400	50.259137
345.720822	121.946927	50.264141
341.904842	114.050711	50.269146
338.477254	114.113413	50.274151
334.974197	117.723218	50.279156
331.195719	122.503107	50.284161
327.825745	105.689093	50.289165
324.201560	121.928403	50.294170
320.704773	111.519597	50.299175
317.162961	131.514424	50.304180
313.614527	121.168208	50.309185
310.291652	124.246734	50.314189
306.692223	134.418913	50.319194
303.418676	119.762269	50.324199
299.851956	127.956196	50.329204
296.609661	129.026768	50.334209
293.028027	115.392615	50.339213
289.069169	121.769933	50.344218
285.870154	128.609750	50.349223
282.238296	136.059602	50.354228
278.866026	143.548841	50.359233
275.488196	121.966839	50.364237
271.655665	128.727060	50.369242
268.184823	116.312939	50.374247
264.704345	126.604077	50.379252
261.193517	116.760015	50.384257
257.841523	117.831270	50.389261
254.115892	127.659621	50.394266
250.341667	118.943515	50.399271
247.226730	121.213827	50.404276
243.957099	124.909307	50.409281
240.570257	117.553767	50.414285
236.546462	125.796708	50.419290
233.371532	123.062602	50.424295
229.670005	117.490125	50.429300
225.962417	130.018838	50.434305
222.860227	128.044040	50.439309
218.863906	137.033360	50.444314
215.900960	121.784471	50.449319
212.182599	123.901178	50.454324
208.542795	127.372750	50.459329
205.702384	115.916737	50.464333
201.505164	128.316639	50.469338
198.056630	116.571949	50.474343
194.653258	126.531945	50.479348
190.986608	119.278699	50.484353
187.946136	126.132905	50.489357
184.338185	130.576032	50.494362
180.736217	115.515526	50.499367
177.079334	126.856553	50.504372
173.602761	118.855043	50.509377
169.946443	125.895754	50.514381
166.490210	124.388775	50.519386
163.415746	133.047540	50.524391
159.773264	117.217290	50.529396
156.180380	125.953431	50.534401
152.404905	126.101340	50.539405
148.833225	135.079321	50.544410
145.993533	124.687028	50.549415
142.013762	122.362177	50.554420
138.534645	124.098271	50.559425
135.441433	115.413540	50.564429
131.734357	131.229330	50.569434
128.109991	108.802643	50.574439
124.391478	128.443289	50.579444
120.679013	116.346197	50.584449
117.889120	120.083107	50.589453
114.182554	122.919919	50.594458
110.694843	128.633814	50.599463
106.526406	123.824069	50.604468
103.185016	116.160526	50.609473
100.235192	111.104333	50.614477
96.673225	113.738510	50.619482
93.229509	123.973633	50.624487
89.718831	105.689721	50.629492
86.249694	125.571497	50.634497
82.633079	113.973434	50.639501
79.068237	124.400324	50.644506
75.759874	110.022357	50.649511
72.011438	111.221073	50.654516
68.436026	125.217876	50.659521
65.172958	118.903135	50.664525
61.369110	129.957963	50.669530
58.347886	122.984051	50.674535
54.669475	109.419041	50.679540
50.819900	126.206997	50.684545
47.405159	128.460559	50.689549
43.755942	110.643285	50.694554
40.666747	115.432730	50.699559
36.778552	115.174365	50.704564
33.469032	121.697052	50.709569
30.258533	114.712021	50.714573
26.619458	114.040988	50.719578
22.737644	105.244082	50.724583
19.371263	105.048746	50.729588
15.505288	113.078390	50.734593
12.754305	107.126914	50.739597
9.232683	124.895395	50.744602
5.636502	104.005024	50.749607
2.224500	125.851803	50.754612