Wed Jun 15 16:08:25 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.318372	115.122659	0.000000
1.705853	117.804665	0.005005
1.360335	103.813658	0.010010
1.400039	114.525680	0.015014
1.403157	96.636938	0.020019
1.104875	96.709418	0.025024
1.397737	89.062853	0.030029
0.489888	61.508235	0.035034
0.466957	41.868445	0.040038
0.261988	47.220059	0.045043
-0.251428	21.467043	0.050048
-0.502929	26.070412	0.055053
-1.099394	8.570780	0.060058
-1.587093	11.914994	0.065062
-1.536173	13.938993	0.070067
-1.977696	-2.833461	0.075072
-1.788770	1.929528	0.080077
-2.243407	-6.793884	0.085082
-2.182968	-8.648551	0.090086
-2.376971	-25.977704	0.095091
-3.205855	-35.115417	0.100096
-3.195724	-18.897016	0.105101
-4.308353	-40.315532	0.110106
-4.744041	-30.451730	0.115110
-4.392517	-35.296515	0.120115
-4.730523	-13.999496	0.125120
-4.730592	-22.907122	0.130125
-5.273001	-17.806457	0.135130
-5.183721	-28.216922	0.140134
-5.149302	-28.030541	0.145139
-5.903145	-20.486493	0.150144
-6.255078	-15.785649	0.155149
-6.751967	-18.941883	0.160154
-6.787391	-12.940413	0.165158
-6.722247	-31.832325	0.170163
-7.105545	-13.473685	0.175168
-7.045586	-28.022836	0.180173
-7.604552	-21.788459	0.185178
-8.264817	-30.446604	0.190182
-8.400732	-35.452913	0.195187
-8.443506	-3.297775	0.200192
-8.247343	-29.639298	0.205197
-8.259326	-11.867408	0.210202
-8.795556	-13.876595	0.215206
-9.334131	-34.696107	0.220211
-10.013844	-37.200259	0.225216
-9.649943	-25.989102	0.230221
-9.969668	-37.487705	0.235226
-10.246961	-23.815805	0.240230
-10.940500	-30.926613	0.245235
-11.594142	-19.566725	0.250240
-11.679463	-36.048306	0.255245
-11.369854	-21.497786	0.260250
-11.480215	-28.154624	0.265254
-11.613953	-36.135765	0.270259
-11.951760	-22.467181	0.275264
-11.931271	-19.709952	0.280269
-12.864201	-27.361436	0.285274
-13.101930	-13.882506	0.290278
-13.373058	-35.104991	0.295283
-13.372399	-32.972764	0.300288
-13.600414	-30.057081	0.305293
-13.473799	-29.947590	0.310298
-13.550876	-41.664444	0.315302
-14.038500	-18.250624	0.320307
-14.829668	-32.367711	0.325312
-14.857366	-14.108285	0.330317
-14.998776	-10.780168	0.335322
-15.509074	-30.321957	0.340326
-16.094015	-17.916924	0.345331
-16.508385	-25.610799	0.350336
-16.504583	-39.422550	0.355341
-16.750588	-24.579371	0.360346
-17.001410	-34.704174	0.365350
-16.947201	-34.475786	0.370355
-17.016096	-25.361146	0.375360
-17.073561	-44.108089	0.380365
-16.893380	-22.606898	0.385370
-17.464993	-8.023587	0.390374
-17.731753	-21.794093	0.395379
-18.540418	-22.474278	0.400384
-18.292270	-23.445514	0.405389
-19.420656	-9.654160	0.410394
-19.849879	-28.696290	0.415398
-19.638838	-22.008238	0.420403
-19.573506	-25.535465	0.425408
-19.766287	-24.876213	0.430413
-19.865251	-36.014446	0.435418
-20.096378	-36.996441	0.440422
-20.140367	-28.237296	0.445427
-21.265017	-36.380406	0.450432
-21.560293	-22.271689	0.455437
-21.451754	-19.381832	0.460442
-21.771509	-18.979580	0.465446
-21.338655	-31.452492	0.470451
-22.066999	-3.329559	0.475456
-22.747389	-23.261112	0.480461
-23.317157	-12.083075	0.485466
-23.539146	-22.111538	0.490470
-23.106403	-18.768416	0.495475
-23.543959	-13.350272	0.500480
-23.450434	-19.022582	0.505485
-23.673517	-19.726049	0.510490
-23.518736	-16.936956	0.515494
-24.191986	-37.134830	0.520499
-24.832000	-26.858459	0.525504
-24.672908	-40.506569	0.530509
-24.826750	-37.496805	0.535514
-25.168130	-19.334404	0.540518
-25.737661	-35.019298	0.545523
-26.311166	-24.552876	0.550528
-26.206614	-26.489308	0.555533
-26.579104	-35.303121	0.560538
-26.701968	-30.029618	0.565542
-26.626523	-24.604911	0.570547
-26.821522	-28.238760	0.575552
-27.446206	-20.727894	0.580557
-27.640029	-25.184449	0.585562
-27.963188	-26.954510	0.590566
-27.515597	-34.306180	0.595571
-28.400160	-29.173832	0.600576
-28.965745	-25.263645	0.605581
-29.485444	-31.134196	0.610586
-29.320479	-31.645115	0.615590
-29.201230	-31.573077	0.620595
-29.541247	-36.228310	0.625600
-29.129221	-30.271793	0.630605
-30.149954	-27.097948	0.635610
-30.803835	-30.599338	0.640614
-30.884195	-11.452470	0.645619
-30.830961	-27.962971	0.650624
-30.947242	-15.727326	0.655629
-30.983174	-26.838397	0.660634
-31.906431	-16.400977	0.665638
-32.047806	-32.271355	0.670643
-32.479950	-28.947970	0.675648
-32.508636	-21.647859	0.680653
-32.796726	-31.174825	0.685658
-32.998452	-19.813172	0.690662
-32.568537	-18.292562	0.695667
-33.560151	-13.205749	0.700672
-33.818545	-5.750082	0.705677
-33.967576	-20.560044	0.710682
-34.161871	-7.357987	0.715686
-33.869445	-22.102404	0.720691
-34.587539	-28.597841	0.725696
-35.691270	-18.774262	0.730701
-35.582312	-30.589538	0.735706
-35.516566	-26.448488	0.740710
-35.582097	-21.780081	0.745715
-35.697292	-10.546560	0.750720
-36.109761	-39.575607	0.755725
-36.220812	-23.119379	0.760730
-36.882278	-16.050087	0.765734
-37.033947	-18.552428	0.770739
-37.549202	3.061455	0.775744
-37.655521	-25.026031	0.780749
-37.653445	-25.999315	0.785754
-37.778258	-25.108428	0.790758
-37.600136	-41.093350	0.795763
-38.499166	-22.266057	0.800768
-38.536280	-30.305880	0.805773
-39.010613	-19.257655	0.810778
-39.118313	-22.251219	0.815782
-38.844398	-19.184398	0.820787
-39.897899	-12.911692	0.825792
-40.338040	-30.662212	0.830797
-40.608445	-25.437323	0.835802
-40.647813	-29.101824	0.840806
-40.603097	-25.362339	0.845811
-41.133894	-33.850400	0.850816
-40.836964	-29.561807	0.855821
-41.024523	-26.874467	0.860826
-41.671285	-25.124626	0.865830
-41.973312	-41.621381	0.870835
-43.064204	-16.039555	0.875840
-42.649435	-13.971522	0.880845
-42.898525	-25.701980	0.885850
-42.946333	-20.411777	0.890854
-42.157254	-25.503087	0.895859
-43.058087	-19.879649	0.900864
-43.366430	-14.983488	0.905869
-43.944717	-25.611230	0.910874
-44.286284	-28.831105	0.915878
-44.556723	-8.530725	0.920883
-45.322857	-18.192657	0.925888
-45.566309	-16.738031	0.930893
-45.791195	-14.665496	0.935898
-45.071424	-11.871426	0.940902
-45.486565	-9.342481	0.945907
-45.707564	-22.422721	0.950912
-45.527212	-17.521109	0.955917
-46.357104	-33.430992	0.960922
-47.089971	-22.251459	0.965926
-47.083329	-27.268404	0.970931
-47.281477	-15.234970	0.975936
-47.365142	-21.096496	0.980941
-47.464959	-12.388786	0.985946
-48.147157	-17.603122	0.990950
-48.728080	-37.946458	0.995955
-48.911322	-18.788223	1.000960
-49.005141	-29.068396	1.005965
-48.819696	-12.084179	1.010970
-49.161540	-29.881523	1.015974
-49.180183	-37.473977	1.020979
-49.340045	-24.032097	1.025984
-50.078144	-35.252423	1.030989
-50.296285	-22.947078	1.035994
-50.947205	-32.091998	1.040998
-50.606131	-22.205833	1.046003
-50.785606	-11.626565	1.051008
-50.745530	-18.749016	1.056013
-51.130221	-27.838798	1.061018
-51.929071	-10.244352	1.066022
-51.996491	-25.383559	1.071027
-52.700145	-8.920038	1.076032
-52.738092	-35.177866	1.081037
-52.518085	-19.140649	1.086042
-52.697431	-19.294486	1.091046
-52.867359	-11.996184	1.096051
-53.498949	-21.667622	1.101056
-53.574799	-25.310705	1.106061
-53.772655	-19.137978	1.111066
-54.304432	-35.977836	1.116070
-54.864154	-36.346596	1.121075
-55.395982	-3.594634	1.126080
-54.930395	-29.379720	1.131085
-55.190247	-14.234757	1.136090
-55.429939	-21.331391	1.141094
-55.569877	-20.181722	1.146099
-55.520765	-15.762008	1.151104
-56.007284	-36.964862	1.156109
-56.477231	-19.071433	1.161114
-56.910815	-9.637965	1.166118
-56.970770	-27.460886	1.171123
-57.542910	-14.431368	1.176128
-57.215608	-22.028621	1.181133
-57.324610	-22.073340	1.186138
-58.201467	-14.965195	1.191142
-58.320983	-23.993152	1.196147
-58.519190	-28.778260	1.201152
-58.654649	-16.843674	1.206157
-58.713437	-27.810195	1.211162
-59.194108	-12.502569	1.216166
-59.904614	-37.354609	1.221171
-60.221285	-20.753128	1.226176
-60.395228	-29.719804	1.231181
-60.757146	-16.745352	1.236186
-60.536673	-17.720204	1.241190
-60.364586	-28.746483	1.246195
-60.428739	-8.266926	1.251200
-60.653382	-27.612456	1.256205
-61.740816	-14.755441	1.261210
-62.214771	-24.302393	1.266214
-61.961384	-19.894344	1.271219
-62.152953	-23.551842	1.276224
-62.108362	-12.285939	1.281229
-62.518039	-32.664879	1.286234
-63.297619	-23.746089	1.291238
-63.368608	-31.873235	1.296243
-63.485852	-22.937245	1.301248
-63.372439	-29.071640	1.306253
-63.854590	-13.098008	1.311258
-64.919721	-21.226488	1.316262
-64.959350	-19.058501	1.321267
-64.943495	-23.661473	1.326272
-65.570151	-23.489836	1.331277
-65.100939	-36.921374	1.336282
-65.540414	-13.738453	1.341286
-65.437981	-32.302401	1.346291
-65.735429	-20.856275	1.351296
-65.710211	-29.106353	1.356301
-66.463247	-26.526795	1.361306
-66.600267	-25.951334	1.366310
-66.785895	-30.617086	1.371315
-67.209869	-14.623872	1.376320
-67.081249	-29.110276	1.381325
-68.007146	-19.166243	1.386330
-68.619096	-32.636518	1.391334
-68.429895	-27.446255	1.396339
-68.472119	-34.757617	1.401344
-68.415531	-11.968497	1.406349
-68.797580	-20.208190	1.411354
-69.747492	-27.839394	1.416358
-70.103340	-25.309694	1.421363
-70.313362	-22.072635	1.426368
-70.526337	-25.539759	1.431373
-70.089743	-14.163153	1.436378
-70.254301	-27.432150	1.441382
-69.944770	-25.388061	1.446387
-70.788236	-30.126207	1.451392
-71.601502	-24.404981	1.456397
-71.886044	-27.386776	1.461402
-72.136900	-26.153472	1.466406
-72.111883	-29.309636	1.471411
-72.329000	-30.011028	1.476416
-72.371364	-22.736774	1.481421
-72.123178	-17.817274	1.486426
-73.016988	-25.785649	1.491430
-73.100338	-20.926971	1.496435
-73.707659	-29.244942	1.501440
-73.633916	-23.829428	1.506445
-73.527642	-26.501549	1.511450
-74.362424	-18.501496	1.516454
-74.558470	-33.239055	1.521459
-75.456589	-20.286768	1.526464
-75.510272	-26.841696	1.531469
-75.163518	-19.890005	1.536474
-75.540471	-43.810596	1.541478
-75.315562	-38.761680	1.546483
-75.722169	-27.013320	1.551488
-76.340614	-45.290511	1.556493
-76.819123	-26.476300	1.561498
-76.908147	-24.196079	1.566502
-76.626426	-25.384067	1.571507
-76.885190	-15.033185	1.576512
-77.663551	-31.494129	1.581517
-77.692612	-19.144076	1.586522
-78.144810	-33.162982	1.591526
-78.345984	-30.861860	1.596531
-78.377226	-19.039498	1.601536
-78.564951	-27.854644	1.606541
-79.132433	-6.761780	1.611546
-79.474010	-26.143618	1.616550
-79.577392	-21.587530	1.621555
-79.434577	-19.589478	1.626560
-80.034267	-12.608126	1.631565
-79.904490	-34.289758	1.636570
-80.945310	-34.386349	1.641574
-81.177224	-45.545209	1.646579
-81.601539	-26.428431	1.651584
-81.756763	-35.297478	1.656589
-81.517171	-17.378576	1.661594
-81.864640	-22.076868	1.666598
-81.542655	-27.755758	1.671603
-81.998378	-16.937988	1.676608
-82.314129	-17.955614	1.681613
-82.626357	-5.147792	1.686618
-83.221669	-10.531951	1.691622
-83.326782	-32.730634	1.696627
-83.744384	-15.472455	1.701632
-83.665746	-37.599697	1.706637
-84.051746	-20.955984	1.711642
-84.787719	-36.760236	1.716646
-84.826244	-26.995515	1.721651
-85.222716	-18.113699	1.726656
-84.897468	-17.888675	1.731661
-85.278502	-16.431137	1.736666
-85.271707	-22.638765	1.741670
-84.796584	-25.946164	1.746675
-86.173911	-7.307631	1.751680
-86.248457	-22.165897	1.756685
-86.364161	-17.136738	1.761690
-86.763587	-17.505649	1.766694
-87.463458	-13.262627	1.771699
-87.936556	-11.861688	1.776704
-88.092109	-10.005006	1.781709
-87.760832	-21.798232	1.786714
-88.191099	-24.613892	1.791718
-88.210102	-19.518148	1.796723
-88.644413	-32.173368	1.801728
-88.228652	-16.768078	1.806733
-88.565653	-24.850472	1.811738
-89.495460	-20.619661	1.816742
-89.426962	-36.007410	1.821747
-89.778942	-7.340423	1.826752
-90.064751	-23.683512	1.831757
-89.852220	-12.682908	1.836762
-91.062765	-22.182202	1.841766
-91.140735	-18.754385	1.846771
-91.790870	-17.989357	1.851776
-91.775116	-31.064221	1.856781
-91.950670	-24.445456	1.861786
-91.930897	-34.668831	1.866790
-91.716805	-24.760208	1.871795
-91.700915	-31.335509	1.876800
-92.036646	-24.725883	1.881805
-92.218445	-40.259195	1.886810
-93.156798	-26.881316	1.891814
-93.303130	-30.685279	1.896819
-93.297092	-18.501130	1.901824
-94.032201	-10.643516	1.906829
-94.278998	-26.367732	1.911834
-94.935240	-10.901766	1.916838
-94.959141	-28.080757	1.921843
-95.013519	-17.924450	1.926848
-94.895856	-30.847965	1.931853
-94.707192	-30.957170	1.936858
-95.354262	-17.250300	1.941862
-95.774715	-41.613426	1.946867
-95.983783	-15.823504	1.951872
-96.433840	-22.791454	1.956877
-96.297229	-13.969329	1.961882
-96.793945	-10.276589	1.966886
-97.282506	-17.978614	1.971891
-97.801052	-24.634472	1.976896
-98.240668	-7.498914	1.981901
-98.054466	-20.169196	1.986906
-98.104084	-34.787518	1.991910
-97.936309	-26.563019	1.996915
-98.224182	-30.757524	2.006912
-98.340147	-29.448187	2.016909
-98.167866	-10.523042	2.026906
-97.170639	-33.208221	2.036902
-96.969034	-21.620683	2.046899
-96.319349	-18.757177	2.056896
-95.414242	-22.713738	2.066893
-95.620217	-23.160313	2.076890
-95.130392	-17.247461	2.086886
-93.942570	-16.929163	2.096883
-93.831670	-23.943327	2.106880
-93.548117	-28.757127	2.116877
-92.330991	-15.907101	2.126874
-92.333660	-19.673432	2.136870
-91.886089	-20.711807	2.146867
-90.870766	-26.632099	2.156864
-90.654698	-24.797647	2.166861
-90.936894	-18.482022	2.176858
-89.779704	-17.113748	2.186854
-89.296767	-20.244434	2.196851
-88.911883	-16.461843	2.206848
-87.813182	-25.579050	2.216845
-87.365051	-22.969759	2.226842
-87.288973	-24.540555	2.236838
-87.248343	-29.321517	2.246835
-86.009980	-25.235310	2.256832
-85.865325	-26.467984	2.266829
-85.734805	-12.676932	2.276826
-84.657259	-15.930683	2.286822
-84.545090	-20.702136	2.296819
-83.464424	-22.275888	2.306816
-82.872918	-18.799760	2.316813
-82.810517	-23.309340	2.326810
-82.567612	-21.829174	2.336806
-81.778141	-18.989559	2.346803
-81.380245	-7.714271	2.356800
-80.534240	-19.534898	2.366797
-79.986611	-19.275545	2.376794
-80.031126	-25.513946	2.386790
-79.570331	-32.468987	2.396787
-78.526554	-18.394375	2.406784
-78.405483	-23.215104	2.416781
-77.888988	-18.942919	2.426778
-77.020484	-26.452688	2.436774
-77.095693	-31.595370	2.446771
-75.917500	-21.933499	2.456768
-75.235861	-15.877814	2.466765
-75.100334	-12.858608	2.476762
-75.152860	-33.503400	2.486758
-74.646826	-23.919789	2.496755
-73.857764	-18.806071	2.506752
-72.954893	-20.472125	2.516749
-72.255315	-12.796969	2.526746
-72.085367	-20.995297	2.536742
-72.117249	-29.109693	2.546739
-71.500542	-23.464839	2.556736
-70.729467	-25.932773	2.566733
-70.276160	-26.940191	2.576730
-69.246374	-31.235596	2.586726
-68.732300	-24.211513	2.596723
-68.975399	-25.382573	2.606720
-68.838311	-21.844480	2.616717
-67.621554	-16.479249	2.626714
-67.270646	-19.345924	2.636710
-66.577585	-23.187333	2.646707
-65.792766	-25.338701	2.656704
-65.466988	-27.542015	2.666701
-65.461974	-12.890160	2.676698
-64.999620	-14.472250	2.686694
-64.119614	-20.441887	2.696691
-64.065657	-22.060192	2.706688
-62.949261	-24.485238	2.716685
-62.345833	-12.102308	2.726682
-62.349946	-6.326595	2.736678
-61.966022	-21.784104	2.746675
-60.977842	-25.326607	2.756672
-60.741110	-34.275967	2.766669
-60.684333	-23.535661	2.776666
-59.319104	-10.533490	2.786662
-58.972422	-13.688180	2.796659
-58.839091	-11.799356	2.806656
-58.394651	-27.469936	2.816653
-57.624478	-28.800258	2.826650
-57.070343	-19.418381	2.836646
-56.443378	-13.880804	2.846643
-56.095419	-16.722200	2.856640
-55.825693	-19.682824	2.866637
-55.496381	-25.291898	2.876634
-54.644946	-14.442601	2.886630
-54.250061	-23.135321	2.896627
-53.804362	-14.788334	2.906624
-52.960641	-15.265170	2.916621
-52.676594	-17.207941	2.926618
-52.197103	-21.356695	2.936614
-51.514414	-24.742332	2.946611
-51.322121	-25.827213	2.956608
-50.748341	-21.230741	2.966605
-49.794098	-18.990836	2.976602
-49.501952	-14.968109	2.986598
-49.622083	-31.066110	2.996595
-48.642505	-20.507247	3.006592
-47.965846	-16.654345	3.016589
-48.071658	-26.303696	3.026586
-47.045079	-21.378176	3.036582
-46.520197	-20.712761	3.046579
-46.579139	-20.460920	3.056576
-45.320603	-11.307852	3.066573
-44.826447	-30.606753	3.076570
-44.935206	-22.041608	3.086566
-44.440899	-17.581147	3.096563
-43.716966	-15.283819	3.106560
-43.306502	-27.712805	3.116557
-42.121043	-28.382027	3.126554
-41.643279	-18.034372	3.136550
-41.586887	-21.414191	3.146547
-41.593275	-20.828296	3.156544
-40.881911	-23.138299	3.166541
-40.043844	-14.630953	3.176538
-39.805690	-24.411330	3.186534
-38.991664	-17.853531	3.196531
-38.629975	-14.897678	3.206528
-38.382186	-16.883942	3.216525
-37.672379	-35.045654	3.226522
-37.004099	-24.827668	3.236518
-36.751919	-17.470695	3.246515
-35.956300	-24.902239	3.256512
-35.660063	-23.201930	3.266509
-35.306706	-29.042548	3.276506
-34.261340	-23.676346	3.286502
-33.797020	-24.271134	3.296499
-33.898763	-26.667516	3.306496
-33.448978	-22.190609	3.316493
-32.054080	-24.699605	3.326490
-32.056558	-26.840769	3.336486
-32.130602	-20.667303	3.346483
-31.319134	-23.932878	3.356480
-30.611376	-22.312134	3.366477
-30.245709	-28.874639	3.376474
-29.626557	-22.865416	3.386470
-29.443523	-31.634931	3.396467
-28.274429	-32.313496	3.406464
-27.806433	-28.857745	3.416461
-27.738690	-20.960726	3.426458
-27.415465	-16.946096	3.436454
-26.403307	-27.408005	3.446451
-26.496470	-27.775836	3.456448
-25.311534	-25.235758	3.466445
-24.632609	-17.318745	3.476442
-24.354123	-14.603775	3.486438
-24.407853	-28.018642	3.496435
-24.072615	-29.080723	3.506432
-23.084911	-32.848638	3.516429
-22.665502	-15.253103	3.526426
-21.823433	-20.030804	3.536422
-21.115115	-23.358547	3.546419
-20.950886	-18.018389	3.556416
-20.898101	-21.680990	3.566413
-20.603410	-23.036539	3.576410
-19.429674	-29.697818	3.586406
-19.155341	-23.875576	3.596403
-18.026100	-29.321517	3.606400
-18.007346	-26.846213	3.616397
-17.697616	-31.148451	3.626394
-17.335422	-31.447131	3.636390
-16.600151	-24.720452	3.646387
-16.024921	-21.824482	3.656384
-15.962893	-18.696134	3.666381
-14.747290	-21.243946	3.676378
-14.501344	-31.902114	3.686374
-14.351531	-27.103417	3.696371
-13.427867	-26.206992	3.706368
-12.871952	-27.298923	3.716365
-12.439701	-23.683572	3.726362
-12.072300	-20.658039	3.736358
-11.258742	-24.705741	3.746355
-10.962352	-19.333099	3.756352
-10.977635	-20.949444	3.766349
-9.950765	-26.041356	3.776346
-9.368615	-39.993527	3.786342
-9.310294	-28.046180	3.796339
-8.706064	-28.422786	3.806336
-7.837489	-19.831384	3.816333
-7.531766	-24.432046	3.826330
-7.234690	-28.087704	3.836326
-6.220977	-19.609381	3.846323
-6.131641	-27.780263	3.856320
-5.994486	-27.784153	3.866317
-5.152100	-23.959721	3.876314
-4.708564	-13.098809	3.886310
-4.225455	2.747041	3.896307
-3.775383	4.349434	3.906304
-3.398469	21.141906	3.916301
-2.989545	22.388013	3.926298
-2.188323	32.617757	3.936294
-1.978352	55.059408	3.946291
-1.541604	76.217396	3.956288
-0.986432	83.988386	3.966285
-0.753789	87.757452	3.976282
-0.227234	105.938535	3.986278
0.000000	131.763317	3.991283
0.232325	146.178998	3.996288
0.542275	159.924380	4.001293
0.877103	168.568655	4.006298
1.187097	174.581084	4.011302
1.259837	171.662227	4.016307
1.293145	176.088952	4.021312
0.884014	172.535817	4.026317
1.227732	176.657622	4.031322
1.110549	175.530611	4.036326
0.808047	167.303900	4.041331
1.047779	171.137180	4.046336
1.095814	191.911881	4.051341
0.875273	183.475308	4.056346
0.972866	210.639031	4.061350
1.095938	205.587968	4.066355
1.717419	210.944621	4.071360
1.620646	210.526470	4.076365
1.413515	204.456592	4.081370
1.749500	197.609587	4.086374
1.113966	183.061825	4.091379
1.389180	187.133496	4.096384
1.320170	186.188026	4.101389
1.368126	199.093746	4.106394
1.403685	205.222665	4.111398
1.315974	195.547021	4.116403
1.853954	199.931882	4.121408
1.195260	201.941777	4.126413
1.548402	203.608077	4.131418
1.699256	199.920074	4.136422
1.684814	195.216389	4.141427
1.567055	188.252405	4.146432
1.049122	188.192694	4.151437
1.456132	203.137905	4.156442
1.813890	201.325328	4.161446
1.262024	206.986961	4.166451
1.515605	196.227304	4.171456
1.566080	215.542046	4.176461
1.862482	207.642793	4.181466
1.920457	201.534136	4.186470
1.279168	204.652025	4.191475
1.531426	190.145071	4.196480
1.394128	211.827501	4.201485
1.482439	204.488035	4.206490
1.916375	212.827019	4.211494
1.782446	212.150041	4.216499
2.113527	214.972192	4.221504
1.787265	207.915005	4.226509
1.774505	185.325170	4.231514
1.518735	208.218439	4.236518
1.475362	213.160851	4.241523
1.779409	203.581848	4.246528
1.843057	213.482355	4.251533
2.141013	211.535733	4.256538
1.625212	186.195772	4.261542
1.674968	205.002289	4.266547
1.890110	199.445143	4.271552
2.112282	213.589805	4.276557
1.313772	196.747785	4.281562
1.547322	208.031758	4.286566
1.735723	216.789634	4.291571
2.095259	212.603991	4.296576
1.617898	205.386812	4.301581
1.455700	220.701726	4.306586
1.784266	212.316150	4.311590
1.669599	216.005091	4.316595
2.294735	210.074773	4.321600
1.931432	201.625776	4.326605
1.900654	194.833957	4.331610
1.954145	217.566338	4.336614
1.673136	218.629148	4.341619
1.697647	210.502756	4.346624
1.694112	222.185095	4.351629
2.318909	211.337249	4.356634
1.775185	217.440270	4.361638
1.857851	234.949497	4.366643
1.937572	249.253472	4.371648
1.975184	241.726650	4.376653
2.063495	253.239648	4.381658
2.214077	238.461498	4.386662
2.320575	233.282456	4.391667
2.107565	252.414391	4.396672
2.113729	256.430120	4.401677
1.814470	244.884318	4.406682
2.188300	227.347691	4.411686
2.040257	243.262731	4.416691
2.210384	233.698936	4.421696
2.016845	237.388288	4.426701
2.009027	248.849793	4.431706
1.987093	242.076911	4.436710
1.916817	236.339635	4.441715
2.053836	243.068744	4.446720
1.763200	256.481091	4.451725
2.345607	240.524057	4.456730
2.610533	254.116465	4.461734
2.024101	256.549560	4.466739
2.178339	268.503383	4.471744
2.444296	267.433499	4.476749
2.256200	260.637560	4.481754
2.508894	272.313502	4.486758
2.242566	266.788152	4.491763
2.733862	265.225472	4.496768
2.336195	243.659004	4.501773
1.912525	256.379422	4.506778
2.282369	252.233103	4.511782
2.087625	280.433218	4.516787
2.805346	274.495961	4.521792
2.748416	267.708333	4.526797
2.546135	286.559462	4.531802
2.870730	267.898052	4.536806
2.594034	275.203384	4.541811
2.520264	253.350666	4.546816
2.274651	246.474272	4.551821
2.658077	257.855344	4.556826
2.652996	235.135036	4.561830
2.090539	264.827466	4.566835
2.794062	263.147639	4.571840
2.742709	285.932172	4.576845
2.749286	262.483157	4.581850
2.723273	251.666579	4.586854
2.528638	256.376531	4.591859
2.700684	225.691833	4.596864
2.642513	251.778390	4.601869
2.252302	236.808169	4.606874
2.328966	260.536185	4.611878
2.569074	268.275786	4.616883
2.720987	274.167886	4.621888
2.975082	271.260078	4.626893
2.644674	280.707551	4.631898
2.771869	274.843517	4.636902
2.650811	271.918688	4.641907
3.114211	265.653237	4.646912
2.747108	286.924212	4.651917
2.845491	284.455469	4.656922
3.255274	273.477778	4.661926
2.932334	284.069322	4.666931
2.963118	249.503728	4.671936
2.655314	255.376006	4.676941
2.692732	243.350084	4.681946
2.579466	234.050936	4.686950
2.843890	260.225756	4.691955
2.981011	272.234003	4.696960
3.075711	267.997015	4.701965
2.983899	278.593272	4.706970
2.840561	256.064174	4.711974
2.702227	272.924067	4.716979
2.962551	264.732633	4.721984
2.788449	273.479027	4.726989
3.036528	286.717833	4.731994
3.091850	263.540033	4.736998
2.990626	277.533800	4.742003
3.135248	274.981655	4.747008
3.173788	266.687679	4.752013
2.999531	284.934889	4.757018
2.868004	279.020387	4.762022
2.716625	283.053279	4.767027
2.981071	276.603973	4.772032
3.166427	288.061500	4.777037
3.205181	279.763142	4.782042
2.891245	281.825374	4.787046
2.997921	277.974880	4.792051
2.945198	254.267257	4.797056
3.136844	285.271319	4.802061
2.775119	266.759730	4.807066
3.148991	274.724934	4.812070
3.064756	274.159795	4.817075
3.091418	281.307571	4.822080
2.727579	280.377079	4.827085
2.886668	286.899839	4.832090
3.259374	293.116906	4.837094
3.202789	299.545492	4.842099
3.528988	306.254414	4.847104
3.267154	304.780184	4.852109
2.913836	284.713476	4.857114
3.667588	291.928531	4.862118
3.371857	306.345903	4.867123
3.134283	285.049259	4.872128
3.442515	300.128674	4.877133
3.303434	294.794281	4.882138
3.626972	318.635579	4.887142
3.208451	291.917329	4.892147
3.467472	294.646836	4.897152
3.174249	291.526721	4.902157
3.163904	304.898413	4.907162
3.520891	302.981385	4.912166
3.316340	302.904708	4.917171
3.507779	316.968030	4.922176
3.307011	307.004992	4.927181
3.207780	320.533341	4.932186
3.397647	304.387092	4.937190
3.326024	314.429285	4.942195
3.577982	321.151568	4.947200
3.104414	308.181434	4.952205
3.297400	329.805306	4.957210
3.641052	304.637706	4.962214
3.513899	318.934206	4.967219
3.210727	315.550268	4.972224
3.323093	308.829938	4.977229
3.473525	323.037459	4.982234
3.465184	297.267788	4.987238
3.506283	322.481400	4.992243
3.570681	336.677405	4.997248
3.887692	335.580138	5.002253
3.428465	351.046074	5.007258
4.111929	332.158268	5.012262
3.896847	329.822705	5.017267
3.851663	318.337453	5.022272
3.684986	316.152421	5.027277
3.355238	315.650247	5.032282
3.686477	307.692409	5.037286
3.529117	321.426972	5.042291
4.160936	331.582383	5.047296
3.679561	316.699951	5.052301
3.767532	317.225616	5.057306
3.839141	305.478201	5.062310
3.532132	315.895684	5.067315
3.815731	316.535709	5.072320
3.988176	343.721530	5.077325
3.866451	328.385354	5.082330
3.769790	328.754198	5.087334
3.641252	352.816553	5.092339
4.075001	348.985779	5.097344
3.733273	331.804929	5.102349
3.634872	339.283056	5.107354
4.122779	336.790083	5.112358
4.078793	346.495975	5.117363
3.934330	329.185261	5.122368
3.789100	344.349720	5.127373
3.852034	342.871732	5.132378
3.924569	344.099958	5.137382
3.804544	361.335832	5.142387
3.967854	341.334309	5.147392
3.762592	344.568882	5.152397
3.681625	339.692167	5.157402
3.879357	346.776189	5.162406
3.929165	338.345657	5.167411
4.091327	350.117807	5.172416
3.816246	351.779823	5.177421
3.800892	345.262196	5.182426
4.229910	333.901684	5.187430
3.919287	346.597477	5.192435
4.151336	353.450716	5.197440
4.274104	351.420766	5.202445
3.995092	378.528645	5.207450
4.626420	367.384158	5.212454
4.053714	360.833248	5.217459
4.320050	344.813413	5.222464
4.166892	348.665104	5.227469
4.065428	344.806867	5.232474
4.385852	363.462605	5.237478
4.168661	357.931667	5.242483
4.149090	368.347951	5.247488
4.190686	363.093373	5.252493
4.321496	370.287114	5.257498
4.654855	361.996156	5.262502
4.264287	353.631091	5.267507
4.317727	353.755834	5.272512
4.154302	334.500532	5.277517
4.067554	368.736718	5.282522
4.660276	376.463874	5.287526
4.370201	365.375080	5.292531
4.600337	382.157727	5.297536
4.423675	369.537706	5.302541
4.187589	369.310079	5.307546
4.360249	379.237070	5.312550
4.391262	376.915679	5.317555
4.511860	381.050540	5.322560
4.584469	373.858897	5.327565
4.351781	383.500999	5.332570
4.819108	361.387451	5.337574
4.566086	380.748315	5.342579
4.509248	364.872426	5.347584
4.214003	363.215687	5.352589
4.165940	369.832102	5.357594
4.841579	377.182629	5.362598
4.601748	371.764039	5.367603
4.356646	392.226204	5.372608
4.532993	379.631491	5.377613
4.366115	387.655141	5.382618
4.544224	378.780379	5.387622
4.527450	376.971572	5.392627
4.531236	393.536926	5.397632
4.447132	369.448002	5.402637
4.453686	384.694451	5.407642
4.609841	382.244754	5.412646
4.314558	387.353937	5.417651
3.971119	398.008334	5.422656
4.226358	402.636587	5.427661
4.476726	410.492154	5.432666
4.728420	411.865781	5.437670
4.704367	417.250860	5.442675
4.982931	406.669822	5.447680
4.889468	421.363140	5.452685
4.676833	407.330559	5.457690
4.929816	408.029314	5.462694
4.756563	401.427171	5.467699
4.964133	408.306577	5.472704
5.092549	405.388735	5.477709
4.785749	410.372375	5.482714
4.848792	402.977012	5.487718
4.902140	416.343406	5.492723
4.647744	413.821862	5.497728
4.914792	411.742511	5.502733
4.553088	432.175364	5.507738
5.144897	411.253767	5.512742
4.876681	429.669780	5.517747
4.655501	412.289475	5.522752
4.814856	419.048709	5.527757
4.524589	407.611586	5.532762
4.584214	410.188705	5.537766
4.490049	413.804461	5.542771
4.598704	438.908650	5.547776
4.904328	436.215045	5.552781
4.945919	455.571412	5.557786
5.137100	437.436828	5.562790
5.353457	459.120946	5.567795
5.373842	442.230334	5.572800
5.318803	446.952886	5.577805
4.956211	445.085406	5.582810
5.180685	442.649663	5.587814
5.449864	443.413811	5.592819
5.316393	433.092127	5.597824
5.351841	412.228930	5.602829
4.798009	417.657956	5.607834
5.004101	410.479948	5.612838
5.215839	442.038572	5.617843
5.411444	435.734047	5.622848
5.156921	421.900347	5.627853
5.075003	429.007439	5.632858
5.317857	431.632904	5.637862
5.333610	451.475831	5.642867
5.330884	429.660149	5.647872
5.403466	439.444301	5.652877
5.228426	420.532432	5.657882
5.282699	408.851825	5.662886
5.263173	414.407311	5.667891
5.222472	433.193938	5.672896
5.262585	441.370053	5.677901
5.314746	434.166669	5.682906
5.474428	443.626968	5.687910
5.157577	450.100995	5.692915
5.126118	450.410630	5.697920
5.247825	447.113596	5.702925
5.415653	446.469408	5.707930
5.338938	439.301425	5.712934
5.479977	446.654409	5.717939
5.205874	441.078194	5.722944
5.479833	443.866323	5.727949
5.112060	445.056439	5.732954
5.630965	428.193650	5.737958
5.395552	447.394343	5.742963
5.321131	438.029461	5.747968
5.424429	440.896203	5.752973
5.257661	440.124907	5.757978
5.709969	440.772374	5.762982
5.513023	457.285836	5.767987
5.378479	447.950515	5.772992
5.327123	450.290184	5.777997
5.275740	447.236908	5.783002
5.856136	465.019381	5.788006
5.825919	466.643903	5.793011
5.594062	447.223382	5.798016
5.715554	457.034484	5.803021
5.462801	473.429927	5.808026
5.873691	460.144614	5.813030
5.857609	468.790426	5.818035
5.360064	462.423462	5.823040
5.460858	444.161160	5.828045
5.532834	469.562969	5.833050
6.035664	459.486418	5.838054
5.944853	472.397149	5.843059
5.884895	451.342602	5.848064
6.027404	471.486696	5.853069
5.747417	463.323384	5.858074
5.843123	451.811592	5.863078
5.775936	446.184706	5.868083
5.781553	460.934787	5.873088
5.870170	462.081939	5.878093
5.572165	466.838434	5.883098
5.838763	453.620772	5.888102
5.702857	479.898624	5.893107
5.721100	461.139534	5.898112
6.070432	468.272942	5.903117
5.888369	462.236305	5.908122
5.843403	471.829385	5.913126
6.249781	474.009364	5.918131
6.221231	472.148235	5.923136
6.252108	468.116671	5.928141
5.897421	465.771604	5.933146
5.867092	453.185830	5.938150
5.791066	467.342026	5.943155
5.743264	460.461356	5.948160
5.882076	470.868799	5.953165
5.724715	465.111005	5.958170
6.093348	458.656637	5.963174
5.814494	470.183814	5.968179
6.035278	477.812477	5.973184
6.458059	466.324163	5.978189
6.057605	462.387358	5.983194
6.261912	461.112495	5.988198
5.856249	470.819736	5.993203
5.535202	476.939428	5.998208
6.228270	454.375793	6.003213
5.759949	474.025092	6.008218
5.852658	455.872036	6.013222
5.773261	483.123200	6.018227
5.845438	497.036917	6.023232
6.318777	501.607356	6.028237
6.125479	505.883402	6.033242
6.281003	508.225194	6.038246
6.158482	498.566357	6.043251
5.986818	498.821032	6.048256
6.263698	486.321684	6.053261
6.085545	496.728748	6.058266
6.293642	483.639796	6.063270
5.893633	493.727398	6.068275
6.090571	502.339308	6.073280
6.195887	495.439336	6.078285
6.063513	510.933790	6.083290
6.145870	494.406662	6.088294
6.271193	511.513572	6.093299
5.988626	486.488326	6.098304
5.771455	497.538619	6.103309
5.998846	499.630887	6.108314
6.202392	486.407832	6.113318
5.994195	508.145606	6.118323
6.420606	505.536301	6.123328
6.608510	506.427527	6.128333
6.072412	490.412200	6.133338
5.930814	477.386074	6.138342
6.009372	477.796697	6.143347
6.119745	484.643862	6.148352
6.087500	502.760138	6.153357
6.219859	501.856738	6.158362
6.585624	497.832268	6.163366
6.162155	480.518066	6.168371
5.939231	480.155874	6.173376
5.891280	473.180519	6.178381
5.968497	490.961239	6.183386
6.215840	488.067232	6.188390
6.185906	511.308759	6.193395
6.252719	487.338540	6.198400
5.920729	485.432950	6.203405
5.938983	490.621952	6.208410
6.600846	490.417876	6.213414
6.291824	484.066508	6.218419
6.394911	489.810599	6.223424
6.518071	464.182772	6.228429
5.959967	485.024794	6.233434
5.933493	460.208332	6.238438
6.069697	468.497418	6.243443
6.097717	464.001491	6.248448
6.042937	462.581516	6.253453
5.918739	466.007416	6.258458
6.095785	460.982666	6.263462
5.920896	467.083332	6.268467
6.078677	468.241842	6.273472
6.262594	479.966597	6.278477
5.975528	485.084025	6.283482
6.239010	482.020929	6.288486
6.132799	488.229818	6.293491
6.276122	473.909189	6.298496
6.260899	477.418691	6.303501
6.163044	466.813205	6.308506
6.458118	481.385449	6.313510
6.149341	475.623671	6.318515
5.941147	462.847493	6.323520
6.308966	478.076851	6.328525
6.077725	474.339071	6.333530
5.934076	457.390615	6.338534
6.178236	473.377016	6.343539
5.957907	468.444175	6.348544
6.183772	466.777169	6.353549
5.577237	482.077679	6.358554
5.955714	478.601576	6.363558
6.162719	512.860370	6.368563
5.887679	502.951207	6.373568
6.210207	518.105027	6.378573
6.182534	505.329464	6.383578
6.390583	519.792717	6.388582
6.249214	499.708951	6.393587
6.044988	493.382285	6.398592
6.505479	476.839742	6.403597
6.165500	469.784603	6.408602
6.082029	477.645160	6.413606
5.998730	490.679162	6.418611
5.892468	475.556029	6.423616
6.015277	477.940019	6.428621
6.238792	499.644123	6.433626
6.339635	502.078309	6.438630
5.811535	478.739814	6.443635
6.165016	493.324615	6.448640
6.348656	475.114779	6.453645
6.184483	466.575315	6.458650
6.176226	471.033161	6.463654
6.146202	470.128090	6.468659
5.908490	483.863646	6.473664
5.927072	486.638842	6.478669
5.813983	492.725556	6.483674
6.245541	506.600016	6.488678
6.292244	511.500607	6.493683
6.212114	496.726005	6.498688
6.031030	501.348954	6.503693
5.992086	498.620832	6.508698
6.242652	506.179284	6.513702
6.241412	507.673540	6.518707
6.417411	499.443731	6.523712
6.266973	474.246819	6.528717
5.964810	485.623277	6.533722
6.069668	470.790410	6.538726
6.253097	469.514457	6.543731
6.084484	477.609960	6.548736
6.201219	466.189288	6.553741
6.170307	486.439994	6.558746
5.795251	476.614655	6.563750
6.129990	467.514687	6.568755
6.153432	480.819983	6.573760
5.988199	470.372715	6.578765
6.178525	469.191412	6.583770
6.478062	493.936728	6.588774
6.574016	481.730578	6.593779
5.969079	480.549986	6.598784
6.138037	474.678776	6.603789
5.543180	485.067885	6.608794
6.168843	467.176354	6.613798
6.177772	474.032878	6.618803
5.990365	470.021899	6.623808
6.167303	470.274110	6.628813
6.188578	460.661476	6.633818
6.212232	469.170701	6.638822
5.966484	467.603039	6.643827
5.764437	483.218380	6.648832
6.248305	480.782677	6.653837
6.284421	503.322240	6.658842
6.090020	468.050635	6.663846
6.152843	478.883783	6.668851
6.237849	472.721227	6.673856
6.201510	481.064778	6.678861
5.948234	481.316662	6.683866
6.207086	474.083541	6.688870
6.213298	477.068731	6.693875
5.825011	476.426278	6.698880
6.557546	465.958797	6.703885
6.304605	478.483676	6.708890
6.345452	465.416857	6.713894
6.218504	472.371795	6.718899
6.065813	469.441700	6.723904
6.191789	472.458493	6.728909
6.001155	479.408275	6.733914
5.989023	469.926441	6.738918
6.335788	459.860489	6.743923
6.033073	475.587260	6.748928
6.352555	452.539440	6.753933
5.820031	472.650174	6.758938
6.059810	474.184601	6.763942
5.945337	469.267610	6.768947
5.932137	481.533477	6.773952
6.140154	473.358073	6.778957
5.753685	486.577421	6.783962
6.080660	476.779601	6.788966
6.347814	492.754628	6.793971
6.237190	485.839542	6.798976
6.141731	478.633402	6.803981
5.869136	480.997404	6.808986
6.181932	481.499732	6.813990
6.080045	489.783488	6.818995
6.015239	485.981109	6.824000
6.754373	489.479792	6.829005
6.514706	477.738800	6.834010
6.037062	483.716079	6.839014
6.140489	472.647805	6.844019
5.943754	488.842235	6.849024
5.929971	470.998762	6.854029
5.861436	482.750440	6.859034
5.581556	475.703714	6.864038
6.111611	494.351408	6.869043
6.278174	498.180191	6.874048
6.422058	493.554324	6.879053
5.954409	493.653413	6.884058
6.076314	484.944039	6.889062
6.655485	499.473398	6.894067
6.315147	490.405564	6.899072
6.471592	467.705965	6.904077
6.073717	481.590706	6.909082
6.166171	470.533916	6.914086
6.368037	470.719760	6.919091
6.400527	474.150150	6.924096
6.409173	483.672033	6.929101
6.141696	468.374997	6.934106
6.290639	459.279989	6.939110
6.287847	462.167719	6.944115
5.928444	480.388441	6.949120
6.476051	482.350843	6.954125
6.205641	470.219848	6.959130
6.177809	453.211315	6.964134
6.081351	466.051258	6.969139
5.843869	478.799884	6.974144
6.130289	464.306954	6.979149
5.885287	479.822356	6.984154
6.368213	481.050051	6.989158
6.191815	491.992685	6.994163
6.317053	476.636561	6.999168
6.337867	473.472206	7.004173
6.347108	463.241057	7.009178
6.124511	463.021754	7.014182
6.047301	451.491186	7.019187
5.877866	465.624443	7.024192
6.319050	459.801968	7.029197
5.952379	462.834374	7.034202
6.491182	481.009456	7.039206
6.378450	473.773619	7.044211
5.954711	453.354509	7.049216
6.281586	433.802903	7.054221
6.294349	450.826738	7.059226
6.451682	442.119820	7.064230
6.035376	435.681239	7.069235
5.856625	453.064733	7.074240
6.145685	437.128253	7.079245
5.822820	448.556935	7.084250
6.114583	441.944812	7.089254
6.305113	449.080876	7.094259
5.961391	456.005931	7.099264
6.116207	444.721331	7.104269
5.962804	460.445511	7.109274
5.909600	464.306559	7.114278
6.074232	450.610530	7.119283
5.817673	467.659753	7.124288
6.111676	470.114495	7.129293
6.308109	484.284278	7.134298
5.852458	476.110329	7.139302
6.157042	471.161571	7.144307
6.121020	490.208226	7.149312
6.134334	468.052951	7.154317
5.948296	482.417930	7.159322
6.318013	466.972880	7.164326
6.015510	493.562496	7.169331
5.906034	481.393353	7.174336
6.424390	474.951327	7.179341
6.110889	482.417029	7.184346
6.043287	491.796836	7.189350
6.105096	479.562789	7.194355
6.047094	467.366508	7.199360
6.154841	481.707402	7.204365
6.306079	468.815492	7.209370
6.193132	480.116677	7.214374
6.296427	473.723514	7.219379
5.911439	477.030137	7.224384
5.982473	473.184991	7.229389
6.209737	476.427526	7.234394
6.248093	480.555190	7.239398
5.967631	457.773619	7.244403
6.242715	476.113121	7.249408
6.017287	470.917827	7.254413
6.051129	475.174477	7.259418
5.830105	493.023426	7.264422
5.953949	479.778429	7.269427
5.969389	486.355102	7.274432
6.132852	478.264399	7.279437
5.899652	477.176465	7.284442
6.012680	478.403239	7.289446
6.365879	467.853725	7.294451
5.847514	480.251411	7.299456
6.235969	463.574295	7.304461
6.225942	473.589345	7.309466
6.028982	481.816596	7.314470
6.222078	474.201421	7.319475
5.798115	498.217630	7.324480
5.959208	483.174901	7.329485
6.257119	474.915883	7.334490
6.045135	478.747141	7.339494
6.266380	486.316545	7.344499
5.616222	473.772121	7.349504
6.148631	465.527726	7.354509
5.972015	477.440007	7.359514
5.936762	478.706476	7.364518
6.046137	476.201556	7.369523
5.928927	483.738007	7.374528
6.492459	486.492892	7.379533
6.091856	470.320736	7.384538
6.127022	476.087685	7.389542
5.979076	482.904833	7.394547
6.233888	468.052219	7.399552
6.421934	480.870707	7.404557
6.273322	473.358959	7.409562
6.088943	475.305103	7.414566
6.230538	474.467655	7.419571
5.823368	480.069270	7.424576
6.304725	474.726887	7.429581
6.132637	477.861500	7.434586
6.431846	473.387836	7.439590
6.681387	471.954859	7.444595
6.142697	478.400845	7.449600
6.175560	461.775194	7.454605
6.229998	493.619562	7.459610
6.293719	474.014025	7.464614
6.482177	471.508763	7.469619
5.931768	491.239226	7.474624
6.629071	487.500606	7.479629
6.318925	483.172918	7.484634
6.508491	476.114708	7.489638
6.352854	452.085616	7.494643
5.868087	467.258759	7.499648
6.300714	444.364099	7.504653
6.024346	456.918286	7.509658
5.776983	449.810757	7.514662
6.037473	434.981799	7.519667
6.084273	463.701477	7.524672
6.511213	457.412872	7.529677
6.317699	470.644218	7.534682
6.327501	460.520997	7.539686
6.369265	451.497371	7.544691
5.996016	465.774697	7.549696
6.186220	452.316033	7.554701
5.919872	458.955144	7.559706
5.872409	447.406641	7.564710
6.222035	457.608475	7.569715
5.946486	447.832510	7.574720
6.379281	456.955682	7.579725
6.307114	440.980935	7.584730
6.033512	449.023733	7.589734
6.124066	450.751409	7.594739
6.040564	446.836612	7.599744
6.120203	463.504335	7.604749
6.038938	462.910484	7.609754
5.910751	449.055290	7.614758
6.009055	455.336217	7.619763
5.799229	436.087863	7.624768
5.919103	455.698041	7.629773
6.090268	476.199645	7.634778
6.301310	462.801750	7.639782
6.365326	480.134204	7.644787
6.314780	482.203938	7.649792
6.088072	450.509805	7.654797
5.856918	463.257079	7.659802
5.936590	463.577647	7.664806
6.348974	460.491134	7.669811
5.884902	468.592449	7.674816
6.308653	460.104196	7.679821
6.153761	485.433330	7.684826
6.078941	462.933248	7.689830
6.218893	478.962821	7.694835
6.062478	476.883598	7.699840
6.033986	456.721848	7.704845
6.156511	484.457652	7.709850
6.122996	467.432978	7.714854
6.462834	473.613623	7.719859
6.115947	462.008150	7.724864
5.864973	458.133850	7.729869
5.912921	447.089363	7.734874
6.004801	467.896357	7.739878
6.235750	466.834020	7.744883
5.996463	466.660585	7.749888
6.579294	459.665636	7.754893
6.343561	452.828554	7.759898
5.990517	443.841865	7.764902
5.887984	445.437298	7.769907
5.676170	449.969620	7.774912
6.159846	476.900926	7.779917
6.333816	476.535984	7.784922
5.974408	473.997061	7.789926
6.230082	484.358665	7.794931
6.068467	478.656220	7.799936
6.458432	481.738890	7.804941
6.350368	467.109312	7.809946
6.055816	458.008380	7.814950
6.167809	461.440526	7.819955
5.632165	446.979684	7.824960
5.910604	469.818800	7.829965
5.734695	483.856071	7.834970
5.674092	477.200259	7.839974
6.095860	471.716100	7.844979
5.948518	468.991101	7.849984
6.096518	483.051296	7.854989
6.045167	466.210396	7.859994
5.847658	478.466667	7.864998
6.100432	476.607977	7.870003
5.878989	489.339659	7.875008
5.870189	474.489168	7.880013
5.984650	479.614028	7.885018
6.014634	475.338353	7.890022
6.005827	482.546440	7.895027
6.253713	523.880836	7.900032
5.906665	507.088458	7.905037
6.416794	507.998448	7.910042
6.186634	508.055923	7.915046
6.341337	477.769959	7.920051
5.883697	485.393054	7.925056
5.862692	487.756419	7.930061
5.942539	507.942880	7.935066
6.341366	513.574477	7.940070
6.425286	503.305112	7.945075
6.257268	491.965314	7.950080
6.080843	503.270003	7.955085
6.134938	478.438026	7.960090
5.873353	476.262933	7.965094
6.224073	488.320891	7.970099
5.859358	476.888324	7.975104
6.206891	494.094629	7.980109
6.371278	509.208973	7.985114
6.088505	497.916644	7.990118
6.455019	487.303055	7.995136
5.941583	482.102675	8.000154
6.207125	495.312968	8.005171
6.138208	483.665219	8.010189
6.128388	467.893711	8.015206
6.252904	479.966892	8.020224
6.252451	491.114938	8.025242
6.273598	483.559525	8.030259
5.743775	480.560943	8.035277
5.728115	483.836046	8.040294
6.321543	507.002556	8.045312
6.104853	516.870087	8.050330
6.160548	516.569434	8.055347
6.274763	523.853659	8.060365
6.216078	515.825631	8.065382
6.536482	501.686645	8.070400
5.866979	500.292395	8.075418
5.850665	507.106685	8.080435
5.856688	521.191742	8.085453
6.017450	510.536439	8.090470
6.431455	509.792134	8.095488
5.851798	510.588130	8.100506
6.197333	503.628133	8.105523
6.411201	519.598483	8.110541
5.790077	511.193949	8.115558
6.178190	521.312816	8.120576
6.044236	520.241660	8.125594
6.206135	517.107505	8.130611
6.033175	520.954325	8.135629
6.368504	504.599903	8.140646
6.533940	507.261978	8.145664
6.275488	522.080314	8.150682
6.276108	507.062146	8.155699
6.391994	510.539370	8.160717
6.409988	497.881954	8.165734
6.483130	510.029281	8.170752
6.343341	522.579913	8.175770
6.560750	521.391062	8.180787
6.595751	515.474818	8.185805
6.182252	534.465376	8.190822
6.375173	520.023415	8.195840
6.328754	505.840055	8.200858
6.634630	517.857320	8.205875
6.395646	504.136079	8.210893
6.168413	515.318863	8.215910
6.371322	516.020565	8.220928
6.446224	509.246982	8.225946
6.506328	523.619087	8.230963
6.594657	524.229421	8.235981
6.495566	517.824156	8.240998
6.382154	519.093541	8.246016
6.443070	513.430620	8.251034
6.550041	516.074021	8.256051
6.620000	498.621944	8.261069
6.513110	518.693681	8.266086
6.506164	481.993154	8.271104
6.098291	488.955290	8.276122
6.247412	482.552120	8.281139
6.534252	510.025688	8.286157
6.231335	515.086959	8.291174
6.529680	520.348097	8.296192
6.402430	518.361421	8.301210
6.388673	520.983741	8.306227
6.413967	519.575133	8.311245
6.491318	519.289991	8.316262
6.383961	518.397361	8.321280
6.155576	509.014302	8.326298
6.182273	513.767037	8.331315
6.407652	521.855593	8.336333
6.398808	520.221097	8.341350
6.498178	515.895739	8.346368
6.560369	508.620263	8.351386
6.476928	514.835188	8.356403
6.948830	505.410989	8.361421
6.885364	529.805464	8.366438
6.820835	526.489397	8.371456
6.876634	514.875525	8.376474
6.592351	508.913256	8.381491
6.542221	491.110762	8.386509
6.383940	479.092852	8.391526
6.243215	492.423022	8.396544
6.370485	524.227888	8.401562
6.446436	499.291560	8.406579
6.838598	522.719441	8.411597
6.797118	523.044521	8.416614
6.841919	520.126708	8.421632
6.475701	501.900192	8.426650
6.557985	489.996512	8.431667
6.608298	496.255744	8.436685
6.280453	496.062360	8.441702
6.379914	490.960242	8.446720
6.558232	506.611940	8.451738
6.629553	526.298825	8.456755
6.503561	509.976646	8.461773
6.437934	518.204506	8.466790
6.712161	519.212150	8.471808
6.706153	520.292376	8.476826
6.683245	532.956049	8.481843
6.769067	509.636425	8.486861
6.677473	509.718871	8.491878
6.642038	517.139306	8.496896
6.570089	512.317210	8.501914
6.749479	524.114703	8.506931
6.777860	513.566584	8.511949
6.581056	517.526664	8.516966
6.878798	519.876899	8.521984
6.665024	524.689649	8.527002
6.491583	525.441542	8.532019
6.956553	521.100239	8.537037
6.784190	527.229500	8.542054
6.752129	515.834224	8.547072
6.780656	518.132125	8.552090
6.607746	500.549068	8.557107
6.623031	512.393939	8.562125
6.590128	515.341380	8.567143
6.995901	521.651595	8.572160
6.602002	509.351527	8.577178
6.825111	519.606882	8.582195
6.678085	513.162705	8.587213
6.619879	525.762244	8.592231
6.728284	510.934762	8.597248
7.053921	509.266050	8.602266
6.414071	520.945942	8.607283
6.602674	521.651682	8.612301
6.542261	520.704063	8.617319
6.416430	534.735059	8.622336
6.793590	521.611785	8.627354
6.484052	525.231051	8.632371
6.728179	515.114570	8.637389
6.388667	507.738103	8.642407
6.602727	524.690931	8.647424
6.606689	509.708909	8.652442
6.994677	535.955023	8.657459
7.066376	527.341918	8.662477
6.868187	530.212768	8.667495
6.757931	512.357702	8.672512
6.882079	529.769268	8.677530
6.669430	532.558968	8.682547
6.947966	526.082932	8.687565
7.040053	543.945750	8.692583
7.030393	520.282047	8.697600
6.995554	522.018334	8.702618
6.780542	515.321193	8.707635
7.220251	513.877163	8.712653
6.733686	524.691805	8.717671
6.865953	517.373943	8.722688
6.630122	506.842435	8.727706
6.751418	519.651704	8.732723
6.729504	521.566219	8.737741
6.974475	538.854510	8.742759
6.536608	545.046447	8.747776
6.979083	545.786493	8.752794
6.886695	539.741037	8.757811
7.118966	540.577023	8.762829
6.857981	539.155012	8.767847
7.345290	548.457135	8.772864
7.469208	544.546101	8.777882
6.550744	538.222314	8.782899
7.049363	551.740401	8.787917
6.718228	544.736740	8.792935
7.014718	555.996248	8.797952
7.255002	545.647081	8.802970
6.838809	551.826682	8.807987
6.837934	548.315791	8.813005
7.037754	565.811518	8.818023
7.138282	541.245467	8.823040
7.175988	547.803474	8.828058
6.732542	555.753334	8.833075
6.936813	535.908706	8.838093
7.115164	551.193026	8.843111
7.258195	546.687952	8.848128
7.178127	549.385784	8.853146
7.059448	543.655216	8.858163
7.038374	550.989164	8.863181
7.129705	566.812440	8.868199
6.917513	547.553802	8.873216
7.166303	552.683316	8.878234
6.907257	551.510127	8.883251
7.167539	532.851588	8.888269
7.112473	547.069467	8.893287
7.350655	543.730234	8.898304
7.304601	544.611035	8.903322
6.988415	543.960239	8.908339
7.162456	552.070579	8.913357
6.935748	556.400569	8.918375
6.969383	554.783353	8.923392
7.339987	549.682754	8.928410
6.896283	559.617348	8.933427
7.047544	552.203542	8.938445
6.809896	559.724621	8.943463
7.118006	562.620833	8.948480
7.294297	542.142414	8.953498
7.097076	552.470895	8.958515
7.471037	543.877003	8.963533
6.887470	537.844234	8.968551
6.909327	564.590741	8.973568
7.191450	549.493145	8.978586
7.072840	574.255267	8.983603
6.934993	551.990571	8.988621
6.718981	562.744094	8.993639
7.041151	567.284579	8.998656
7.661924	573.248150	9.003674
7.369956	567.773903	9.008691
7.430480	557.925467	9.013709
7.380932	551.670030	9.018727
7.484665	559.219217	9.023744
7.547919	531.210585	9.028762
7.189719	551.190173	9.033779
7.212310	543.678869	9.038797
7.284421	543.364876	9.043815
7.077669	532.118701	9.048832
7.587003	541.834485	9.053850
7.373957	548.729323	9.058867
7.218305	543.243775	9.063885
7.258753	554.570785	9.068903
6.861816	554.840662	9.073920
7.317937	553.709872	9.078938
7.109105	553.900547	9.083955
7.306110	571.837176	9.088973
7.535798	567.663448	9.093991
7.390546	565.862171	9.099008
7.609803	556.457553	9.104026
7.238791	557.602332	9.109043
7.514550	541.630839	9.114061
7.372228	548.775728	9.119079
7.186080	549.019331	9.124096
7.344720	549.867584	9.129114
7.232696	549.988633	9.134131
7.501534	580.517809	9.139149
7.571898	569.784418	9.144167
7.488490	569.255541	9.149184
7.189126	546.940694	9.154202
7.347841	576.040821	9.159219
7.422028	576.087999	9.164237
7.725833	593.476342	9.169255
7.185728	595.532292	9.174272
7.299385	567.647906	9.179290
7.451097	585.686596	9.184307
7.575039	568.033643	9.189325
7.694223	573.527009	9.194343
7.408018	580.674435	9.199360
7.527247	574.944784	9.204378
7.410108	599.070558	9.209395
7.221997	591.451963	9.214413
7.478228	581.482218	9.219431
7.488524	581.763024	9.224448
7.501954	574.426597	9.229466
7.288279	591.517882	9.234483
7.456308	577.821020	9.239501
7.535264	584.029406	9.244519
7.604173	579.960964	9.249536
7.847155	581.142627	9.254554
7.363502	599.973153	9.259571
7.744621	575.435263	9.264589
7.553981	587.902055	9.269607
7.679451	592.795241	9.274624
7.954962	578.475368	9.279642
7.734636	583.969642	9.284659
7.528640	577.314082	9.289677
7.533561	577.771122	9.294695
7.503355	580.773823	9.299712
7.647931	574.248173	9.304730
7.874575	573.412124	9.309747
7.426159	589.528304	9.314765
7.503374	578.931335	9.319783
7.442514	595.871619	9.324800
7.527066	581.170519	9.329818
7.445891	594.788788	9.334835
7.282771	589.144168	9.339853
7.630812	566.917526	9.344871
7.621880	588.682049	9.349888
7.539953	569.336421	9.354906
7.402466	571.067045	9.359923
7.498663	578.242000	9.364941
7.660026	562.216280	9.369959
7.429669	595.022456	9.374976
7.669332	596.132247	9.379994
7.547617	613.806229	9.385011
7.796649	609.008400	9.390029
8.300519	611.068945	9.395047
7.827202	599.894717	9.400064
7.942480	569.872746	9.405082
7.867699	580.178158	9.410099
7.937280	576.685137	9.415117
7.831822	582.475499	9.420135
7.665731	582.925376	9.425152
8.082196	574.314014	9.430170
7.754932	592.677666	9.435187
7.850338	579.379509	9.440205
7.845843	587.090355	9.445223
7.889503	590.044936	9.450240
8.155185	591.254532	9.455258
8.134271	583.048228	9.460275
8.145421	593.508201	9.465293
8.085316	574.564657	9.470311
8.067773	583.559590	9.475328
7.847275	574.016470	9.480346
7.868964	580.302410	9.485363
8.025651	583.153787	9.490381
8.002409	576.880414	9.495399
7.701716	553.709810	9.500416
7.914469	561.810610	9.505434
7.951317	584.329163	9.510451
7.713586	572.212824	9.515469
7.699780	574.590347	9.520487
7.555606	585.177037	9.525504
8.005950	569.535621	9.530522
8.045896	577.480489	9.535539
7.975804	589.923327	9.540557
8.473495	587.961677	9.545575
7.587656	591.797717	9.550592
8.070691	575.388010	9.555610
7.920018	598.371902	9.560627
7.588964	592.200164	9.565645
8.313276	576.105506	9.570663
7.667174	598.206968	9.575680
8.352623	576.615410	9.580698
8.156871	578.979509	9.585715
8.047754	576.607945	9.590733
8.127577	576.084564	9.595751
8.139896	586.685639	9.600768
7.930184	571.954950	9.605786
8.064625	587.478093	9.610803
8.271248	581.919281	9.615821
8.320847	565.676069	9.620839
7.798885	557.451229	9.625856
7.761801	553.028070	9.630874
8.121163	570.700728	9.635891
7.947778	571.365039	9.640909
8.161836	582.906227	9.645927
7.768219	581.329603	9.650944
7.752613	587.708300	9.655962
7.959785	575.262010	9.660979
8.070953	584.614113	9.665997
7.964933	574.362991	9.671015
8.043747	588.754106	9.676032
8.121215	573.630480	9.681050
7.977324	579.326925	9.686067
7.921687	586.122557	9.691085
7.977660	589.544562	9.696103
7.916940	585.236981	9.701120
7.965179	587.627770	9.706138
8.088601	590.843504	9.711155
7.775949	596.947957	9.716173
8.359355	604.710731	9.721191
8.185380	605.950182	9.726208
8.052835	626.009080	9.731226
8.455207	610.387358	9.736243
8.067590	619.159983	9.741261
8.259306	616.746078	9.746279
8.336844	619.682864	9.751296
8.266819	608.439129	9.756314
8.292293	592.733982	9.761331
7.872138	606.826080	9.766349
8.126374	621.234581	9.771367
8.240318	612.994560	9.776384
8.216589	629.769536	9.781402
8.273248	629.282749	9.786419
8.255350	609.493928	9.791437
8.197108	615.774200	9.796455
8.230530	617.986782	9.801472
8.553647	613.447894	9.806490
8.585454	607.269910	9.811507
8.661005	618.317914	9.816525
8.376235	596.517963	9.821543
8.570857	616.154280	9.826560
7.906665	597.459020	9.831578
7.929812	604.720939	9.836595
7.847820	613.522463	9.841613
8.307934	600.607499	9.846631
8.165956	613.923124	9.851648
8.130235	623.370273	9.856666
8.051811	616.564515	9.861683
7.865729	621.489025	9.866701
8.253107	599.580355	9.871719
8.243817	641.966283	9.876736
8.564851	637.077531	9.881754
8.561891	659.036390	9.886771
8.505021	647.621010	9.891789
8.631699	645.265965	9.896807
8.433264	627.789905	9.901824
8.388357	600.797962	9.906842
8.215644	611.280657	9.911859
8.181779	624.609715	9.916877
8.289846	639.297634	9.921895
8.444503	649.687584	9.926912
8.662372	652.586426	9.931930
8.698601	656.920913	9.936947
8.467037	646.932944	9.941965
8.730697	642.601754	9.946983
8.826306	641.107322	9.952000
8.508845	634.416629	9.957018
8.501338	615.137954	9.962035
8.237956	626.269624	9.967053
8.733768	648.509625	9.972071
8.864840	637.585396	9.977088
8.350432	629.704845	9.982106
8.922393	623.896029	9.987123
8.715424	621.900571	9.992141
8.792843	623.744662	9.997159
8.509620	608.523269	10.002176
8.490223	621.284044	10.007194
8.626827	618.551284	10.012211
8.177327	639.175234	10.017229
8.703600	631.517577	10.022247
8.577877	614.785315	10.027264
8.638828	645.086644	10.032282
8.686890	625.116969	10.037299
8.697257	637.401608	10.042317
9.292826	629.290493	10.047335
8.645517	613.695325	10.052352
8.528743	614.001362	10.057370
8.853427	612.506075	10.062387
8.500285	613.982165	10.067405
8.313624	610.858165	10.072423
8.496065	617.397401	10.077440
8.718047	640.519227	10.082458
8.888398	647.846580	10.087475
8.587696	634.887088	10.092493
8.882725	649.001845	10.097511
8.796828	645.550443	10.102528
8.395826	635.401065	10.107546
8.739263	659.037251	10.112563
8.665081	662.377756	10.117581
9.040162	670.895861	10.122599
9.108146	655.800684	10.127616
9.002834	639.058921	10.132634
8.579812	614.782269	10.137651
8.539824	615.396592	10.142669
8.530797	649.417445	10.147687
9.086056	638.000296	10.152704
8.730121	655.818811	10.157722
8.971565	639.572549	10.162739
8.987548	660.239552	10.167757
9.061817	637.533389	10.172775
8.822250	636.802228	10.177792
8.442579	648.833800	10.182810
8.828118	640.549570	10.187827
9.113775	661.854011	10.192845
8.860795	646.385817	10.197863
9.185389	645.664939	10.202880
8.993291	653.008602	10.207898
9.182565	618.280590	10.212915
8.449206	627.889377	10.217933
8.551303	619.113661	10.222951
8.974871	644.682118	10.227968
9.104474	660.206430	10.232986
9.513292	656.174389	10.238003
9.373055	649.002751	10.243021
8.854412	638.931851	10.248039
8.987476	626.263676	10.253056
8.905244	627.459628	10.258074
9.118606	621.570250	10.263091
8.990457	622.538027	10.268109
8.996010	623.312693	10.273127
9.096320	615.013622	10.278144
8.893084	621.066055	10.283162
8.961434	608.603516	10.288179
8.839728	609.369987	10.293197
8.861011	615.633181	10.298215
9.168275	640.213742	10.303232
8.842339	644.769449	10.308250
9.262627	635.150999	10.313267
8.896219	654.813365	10.318285
9.002221	654.783061	10.323303
9.227245	650.667154	10.328320
9.095622	674.108813	10.333338
9.390875	649.320105	10.338355
9.252312	669.572523	10.343373
8.979288	635.709044	10.348391
9.178825	644.075484	10.353408
9.330817	650.536815	10.358426
9.128704	643.095363	10.363443
8.829672	628.560139	10.368461
8.858426	648.362945	10.373479
9.157480	633.751411	10.378496
9.354516	660.885856	10.383514
9.255670	640.721009	10.388531
9.310506	642.996967	10.393549
9.089922	650.475419	10.398567
9.277303	643.155672	10.403584
9.234194	651.685508	10.408602
9.207864	648.179195	10.413619
9.504467	662.778909	10.418637
9.536072	652.445755	10.423655
9.345360	637.609725	10.428672
8.848660	634.131456	10.433690
8.976532	639.848053	10.438707
9.237292	651.068175	10.443725
8.910096	638.728050	10.448743
9.416428	647.261941	10.453760
9.321856	647.712892	10.458778
9.400802	657.122811	10.463795
9.553129	665.626655	10.468813
9.024877	656.090260	10.473831
9.380036	649.536862	10.478848
9.209563	661.405068	10.483866
9.439766	645.618015	10.488883
9.528364	648.690738	10.493901
9.376587	634.144851	10.498919
9.426380	648.523794	10.503936
9.215899	647.705663	10.508954
9.204666	657.019786	10.513971
9.448028	646.792057	10.518989
8.976699	657.780406	10.524007
9.725001	656.020969	10.529024
9.172646	650.176645	10.534042
9.038077	648.759513	10.539059
9.438335	654.191010	10.544077
9.132917	658.255469	10.549095
9.578616	634.677713	10.554112
9.554724	647.556544	10.559130
9.589969	644.456184	10.564147
9.441335	642.676711	10.569165
9.205177	656.221068	10.574183
9.498263	647.784638	10.579200
9.139203	652.169392	10.584218
9.511179	656.469845	10.589235
9.887756	672.604854	10.594253
9.592306	671.126534	10.599271
9.761868	644.592542	10.604288
9.447399	656.632533	10.609306
9.099613	631.825252	10.614323
9.533128	658.260751	10.619341
9.482760	675.876078	10.624359
9.976518	656.932610	10.629376
9.822220	675.845182	10.634394
9.572891	674.285342	10.639411
9.448929	657.434763	10.644429
9.786556	668.202548	10.649447
9.925977	670.764452	10.654464
9.744761	651.101359	10.659482
9.559790	657.207466	10.664499
9.417662	643.658034	10.669517
9.361941	667.471485	10.674535
9.773469	675.908787	10.679552
9.578900	673.289588	10.684570
9.672763	672.211276	10.689587
9.771437	688.383764	10.694605
9.516041	676.892635	10.699623
9.646112	672.585678	10.704640
9.572588	667.279178	10.709658
9.787268	682.024303	10.714675
9.968492	674.792150	10.719693
9.892969	685.263360	10.724711
10.036180	675.070662	10.729728
10.099113	688.027870	10.734746
9.687498	683.754831	10.739763
9.779233	660.083406	10.744781
9.728054	667.771898	10.749799
9.513590	655.140171	10.754816
9.628234	675.480836	10.759834
10.069153	671.896514	10.764851
9.928850	667.054276	10.769869
9.777017	682.232802	10.774887
9.635322	676.951932	10.779904
9.539754	694.208803	10.784922
9.279786	680.722895	10.789939
9.949190	684.406049	10.794957
9.422584	678.430918	10.799975
9.661931	672.373195	10.804992
9.661463	685.775900	10.810010
9.420876	697.744379	10.815027
9.888009	690.774632	10.820045
9.997335	719.492156	10.825063
10.154314	705.012174	10.830080
9.757098	714.619683	10.835098
10.103131	704.047280	10.840115
10.327476	703.511328	10.845133
9.727920	693.644854	10.850151
10.135341	682.489343	10.855168
9.747904	680.148112	10.860186
9.596213	695.110248	10.865203
10.425456	702.029412	10.870221
10.178112	722.322016	10.875239
10.311127	702.081281	10.880256
9.939309	687.547697	10.885274
9.924737	696.822348	10.890291
9.814851	676.491605	10.895309
9.923768	716.346868	10.900327
10.075980	687.735413	10.905344
9.992861	716.090743	10.910362
9.896187	719.087826	10.915379
10.401913	715.157539	10.920397
9.976276	720.018743	10.925415
10.245801	723.696354	10.930432
10.320775	709.803882	10.935450
10.264802	719.338471	10.940467
10.296833	701.665916	10.945485
10.221026	708.425183	10.950503
10.243289	687.067343	10.955520
10.187790	699.389484	10.960538
9.953203	684.736891	10.965555
10.262061	694.475080	10.970573
10.084132	709.033702	10.975591
10.348712	719.567007	10.980608
10.268198	727.719212	10.985626
9.935673	726.956571	10.990643
10.304527	724.516721	10.995661
10.609480	709.893612	11.000679
10.283553	699.770750	11.005696
10.283563	684.402994	11.010714
9.935149	703.889661	11.015731
10.298699	696.099063	11.020749
10.190857	716.973957	11.025767
10.594555	698.073069	11.030784
10.714239	718.109790	11.035802
9.872829	695.729915	11.040819
10.142612	709.533531	11.045837
9.925938	715.547878	11.050855
10.405287	714.612202	11.055872
10.328168	710.608398	11.060890
10.381069	711.992698	11.065907
10.387108	698.962485	11.070925
9.995007	723.130154	11.075943
10.069147	706.038177	11.080960
10.452301	713.483701	11.085978
10.380399	714.962425	11.090995
10.687091	725.753272	11.096013
10.437707	719.176652	11.101031
10.386674	706.245703	11.106048
10.253040	706.917128	11.111066
10.254200	710.203768	11.116083
10.346138	720.646147	11.121101
10.249393	720.245027	11.126119
10.236256	710.134329	11.131136
10.687783	721.076191	11.136154
10.290103	722.459777	11.141171
10.465497	700.158056	11.146189
10.278526	716.943377	11.151207
10.561325	718.039161	11.156224
10.786226	733.235282	11.161242
10.641943	722.312709	11.166259
11.019081	710.191081	11.171277
10.473999	717.861638	11.176295
10.508396	715.092026	11.181312
10.233621	718.301662	11.186330
10.282364	718.654048	11.191347
10.728191	721.340771	11.196365
10.630847	740.969311	11.201383
10.720392	749.619763	11.206400
10.698895	722.853696	11.211418
10.549238	737.283591	11.216435
11.053693	719.347069	11.221453
10.648637	703.857995	11.226471
10.474999	718.289474	11.231488
10.702936	717.093064	11.236506
10.612441	705.309280	11.241523
10.917741	719.483806	11.246541
10.688476	711.745214	11.251559
10.756581	728.339614	11.256576
10.515299	706.298818	11.261594
10.501736	725.519602	11.266611
10.993382	728.900734	11.271629
11.031829	733.062874	11.276647
10.762467	724.564273	11.281664
10.746488	714.615219	11.286682
10.551169	714.406917	11.291699
10.722319	715.429247	11.296717
10.711520	740.340804	11.301735
11.151763	729.816577	11.306752
11.053385	738.262017	11.311770
10.732089	725.265016	11.316787
10.782727	714.460098	11.321805
10.957043	732.677561	11.326823
10.902795	727.486426	11.331840
11.143400	720.801083	11.336858
10.707056	717.021951	11.341875
10.765462	720.264890	11.346893
10.690871	721.355481	11.351911
10.978759	742.789159	11.356928
11.157693	727.235042	11.361946
10.783244	741.865630	11.366963
10.878481	729.462116	11.371981
11.263808	745.410863	11.376999
11.080442	721.036283	11.382016
11.324351	714.444564	11.387034
11.011767	711.194246	11.392051
11.011422	692.858134	11.397069
10.544214	728.831350	11.402087
10.495450	711.506201	11.407104
10.678459	743.323859	11.412122
10.526395	731.759033	11.417139
10.375320	733.996119	11.422157
10.720355	739.598344	11.427175
10.835019	746.205218	11.432192
11.367543	761.596923	11.437210
10.642321	749.620635	11.442227
11.316399	766.946608	11.447245
11.400057	750.413394	11.452263
11.093562	759.610865	11.457280
11.266328	739.379846	11.462298
10.989523	745.663818	11.467315
11.492828	748.275119	11.472333
11.285928	735.333988	11.477351
11.191986	741.839739	11.482368
11.483824	734.342592	11.487386
11.124221	730.939157	11.492403
11.159600	749.628891	11.497421
11.262350	738.273361	11.502439
11.215896	762.387514	11.507456
11.287781	728.952628	11.512474
11.171229	743.581631	11.517491
11.753611	736.338456	11.522509
11.557383	725.394059	11.527527
11.468979	746.138353	11.532544
11.455742	725.024355	11.537562
11.113989	740.790773	11.542579
11.379237	731.509810	11.547597
11.231743	731.824566	11.552615
11.130595	740.005673	11.557632
11.152283	740.873814	11.562650
10.895613	743.423254	11.567667
11.239959	731.266685	11.572685
11.694121	727.701023	11.577703
11.242849	736.339095	11.582720
11.481703	739.638612	11.587738
11.375435	738.685962	11.592755
11.478113	724.251442	11.597773
11.374953	731.975419	11.602791
11.339257	727.678718	11.607808
11.596405	731.944935	11.612826
11.465147	729.652085	11.617843
11.580501	743.501129	11.622861
11.668224	735.152806	11.627879
11.430137	742.373536	11.632896
11.609055	739.911740	11.637914
11.192320	724.907125	11.642931
11.673985	724.928589	11.647949
11.542757	731.513510	11.652967
11.402003	736.597156	11.657984
11.494945	742.014133	11.663002
11.702405	730.730553	11.668019
11.556668	741.450547	11.673037
11.564418	726.146807	11.678055
11.280624	741.426706	11.683072
11.423812	751.349650	11.688090
11.342785	739.561913	11.693107
11.123690	744.779047	11.698125
11.450309	752.151770	11.703143
11.422100	776.670796	11.708160
11.704958	766.205517	11.713178
12.022903	788.315315	11.718195
11.479387	762.693339	11.723213
12.184682	772.247690	11.728231
11.768325	750.611353	11.733248
11.816693	736.871246	11.738266
11.673446	736.489224	11.743283
11.220278	737.482479	11.748301
11.749849	757.029283	11.753319
11.693684	759.842265	11.758336
11.666295	771.645289	11.763354
12.078525	759.582963	11.768371
11.693910	753.597720	11.773389
11.850850	766.269746	11.778407
12.064186	764.250665	11.783424
11.931733	743.370165	11.788442
11.577971	752.469565	11.793459
11.810026	753.323016	11.798477
12.116883	741.557081	11.803495
11.583044	749.717104	11.808512
11.843044	745.202089	11.813530
11.593994	771.581631	11.818547
11.833114	761.411107	11.823565
11.692250	750.725386	11.828583
11.860024	772.798577	11.833600
11.902432	747.054019	11.838618
11.849378	767.464044	11.843635
11.705658	765.567436	11.848653
11.781674	762.845548	11.853671
11.672918	762.472979	11.858688
11.661796	770.345601	11.863706
11.736076	788.420549	11.868723
11.797139	765.646613	11.873741
12.034694	787.488863	11.878759
12.009880	773.716635	11.883776
11.918462	759.185845	11.888794
11.866886	765.245645	11.893811
11.936880	778.341392	11.898829
12.235927	769.484532	11.903847
12.148250	774.146436	11.908864
12.342406	776.964203	11.913882
12.200037	778.119922	11.918899
11.962748	776.161040	11.923917
12.096934	786.656900	11.928935
11.949430	786.987501	11.933952
12.007707	770.345792	11.938970
12.096218	778.015387	11.943987
11.813893	788.835820	11.949005
12.309553	792.197706	11.954023
12.165362	807.904878	11.959040
12.545553	793.074916	11.964058
12.288501	777.713336	11.969075
11.998302	771.778804	11.974093
12.409140	772.663817	11.979111
12.037172	782.894592	11.984128
12.126554	785.100509	11.989146
12.287504	802.533559	11.994163
12.034125	811.248587	11.999181
12.503684	798.382180	12.004199
12.510924	799.149786	12.009216
12.109815	799.348818	12.014234
12.338729	786.157421	12.019251
12.079105	803.061015	12.024269
12.479177	802.091499	12.029287
12.463060	782.152495	12.034304
12.606393	795.044749	12.039322
12.458610	782.729470	12.044339
12.219446	771.181370	12.049357
12.540319	782.162678	12.054375
12.403498	771.405033	12.059392
12.246271	790.928406	12.064410
12.322379	795.716557	12.069427
12.597267	781.394531	12.074445
12.602977	793.404250	12.079463
12.234442	783.452210	12.084480
12.287410	789.516489	12.089498
12.733263	795.675843	12.094515
12.448978	785.560114	12.099533
12.222362	796.753924	12.104551
12.829159	798.738644	12.109568
12.707916	798.481691	12.114586
12.245298	780.641148	12.119603
12.426690	806.623521	12.124621
12.759522	807.773724	12.129639
12.182255	813.206724	12.134656
12.276924	811.225844	12.139674
12.590571	790.447596	12.144691
12.326305	802.909707	12.149709
12.651390	791.573187	12.154727
12.528454	796.432017	12.159744
12.496436	798.991868	12.164762
12.626782	802.876901	12.169779
12.459069	792.071899	12.174797
12.447641	796.901478	12.179815
12.248220	793.025414	12.184832
12.489668	802.914933	12.189850
12.582193	806.414683	12.194867
12.636646	820.428053	12.199885
12.768131	826.729505	12.204903
12.856076	816.452957	12.209920
12.768133	819.923199	12.214938
13.178352	812.506227	12.219955
12.665467	795.289170	12.224973
12.808799	799.896080	12.229991
12.707603	790.618271	12.235008
12.726929	801.121118	12.240026
13.145180	779.941248	12.245043
12.942529	799.443406	12.250061
12.715836	764.537214	12.255079
12.901716	777.346949	12.260096
12.640816	790.443958	12.265114
12.971207	791.149600	12.270131
12.773073	796.796837	12.275149
12.731393	805.709592	12.280167
13.044391	811.095346	12.285184
13.050754	821.796164	12.290202
13.185615	795.255543	12.295219
12.493936	802.883457	12.300237
12.930721	807.483891	12.305255
13.351648	822.408103	12.310272
12.957336	800.832012	12.315290
13.087611	796.538467	12.320307
12.980076	792.084372	12.325325
13.080439	790.402575	12.330343
13.064795	790.463911	12.335360
12.770621	803.618482	12.340378
12.895655	816.825411	12.345395
13.033087	822.086382	12.350413
13.018852	815.869773	12.355431
12.928916	831.603624	12.360448
13.261433	827.494702	12.365466
13.066012	819.468940	12.370483
13.280938	830.660459	12.375501
13.195416	836.199359	12.380519
13.406531	822.567285	12.385536
13.223816	830.668046	12.390554
13.612043	815.139375	12.395571
13.281443	800.296292	12.400589
13.203059	799.800820	12.405607
12.868002	785.019398	12.410624
12.806360	819.714998	12.415642
12.918783	823.982919	12.420659
12.979383	816.252854	12.425677
13.364560	833.393045	12.430695
13.284889	826.879647	12.435712
12.991528	820.634084	12.440730
13.119872	821.177695	12.445747
13.117272	807.532146	12.450765
13.077238	830.844273	12.455783
13.470610	816.124878	12.460800
13.295371	822.459697	12.465818
13.367743	816.973268	12.470835
13.085392	819.224976	12.475853
13.450958	836.117294	12.480871
13.346431	818.501021	12.485888
13.038471	842.661664	12.490906
13.385296	826.754686	12.495923
13.025467	843.448761	12.500941
13.230634	840.741532	12.505959
13.719120	843.186346	12.510976
13.222000	851.800178	12.515994
13.666208	830.177282	12.521011
13.830053	849.920731	12.526029
13.771988	831.707447	12.531047
13.560778	846.009365	12.536064
13.694985	854.242954	12.541082
13.587681	817.567063	12.546099
13.239311	820.085421	12.551117
13.652639	830.270388	12.556135
13.708121	839.537976	12.561152
13.416231	855.604460	12.566170
13.433586	839.452681	12.571187
13.414620	849.647895	12.576205
13.519994	847.704602	12.581223
13.626050	828.153905	12.586240
13.650250	845.615113	12.591258
13.807311	834.840051	12.596275
13.592032	843.513869	12.601293
13.936375	829.776526	12.606311
13.759842	840.620053	12.611328
13.622364	827.670618	12.616346
13.939460	839.597723	12.621363
13.811528	840.868845	12.626381
13.790471	835.744906	12.631399
14.033867	841.730604	12.636416
13.868689	839.194194	12.641434
13.993946	838.998939	12.646451
13.931633	835.189652	12.651469
13.687251	843.974945	12.656487
13.729388	819.916492	12.661504
13.665002	837.734270	12.666522
13.994085	826.399820	12.671539
13.886729	834.104567	12.676557
14.047664	842.640150	12.681575
14.276561	836.807064	12.686592
13.996237	837.898205	12.691610
14.061843	810.791197	12.696627
13.857825	824.395433	12.701645
13.723320	814.270874	12.706663
14.107088	812.829764	12.711680
13.936711	832.195857	12.716698
14.146118	820.514845	12.721715
13.879291	834.622846	12.726733
14.011323	826.711231	12.731751
14.284700	835.079153	12.736768
14.085704	828.006095	12.741786
13.801865	815.937132	12.746803
13.868776	824.779900	12.751821
14.273670	827.347160	12.756839
14.385481	837.006024	12.761856
14.213958	819.222422	12.766874
14.131208	812.593525	12.771891
14.022342	826.410523	12.776909
14.033877	820.990136	12.781927
13.857157	832.754712	12.786944
14.139836	841.372905	12.791962
14.079016	840.399651	12.796979
13.986203	848.698994	12.801997
13.879944	849.005659	12.807015
13.933831	834.873018	12.812032
14.015023	849.807645	12.817050
14.120606	835.435516	12.822067
13.799525	843.141146	12.827085
14.021617	834.551330	12.832103
14.393515	849.821577	12.837120
13.756334	832.558794	12.842138
13.870558	835.692264	12.847155
14.558818	862.147223	12.852173
14.497407	860.794635	12.857191
14.622771	882.111211	12.862208
14.413734	873.358230	12.867226
14.698911	874.685562	12.872243
14.258550	857.217632	12.877261
14.571788	872.761210	12.882279
14.738752	848.895021	12.887296
14.568346	856.192785	12.892314
14.439299	831.104508	12.897331
14.639187	819.504380	12.902349
14.413788	837.455727	12.907367
14.507001	826.209160	12.912384
14.488716	836.965132	12.917402
14.255469	806.568219	12.922419
14.652737	839.814466	12.927437
14.353915	833.234748	12.932455
14.777146	831.605371	12.937472
14.235770	842.250204	12.942490
14.734528	840.927455	12.947507
14.914909	844.541600	12.952525
14.724503	839.751079	12.957543
14.316881	841.206280	12.962560
14.477982	842.158644	12.967578
14.854729	858.371557	12.972595
14.947082	839.185125	12.977613
14.533233	843.380022	12.982631
14.783418	830.792691	12.987648
14.523964	840.421203	12.992666
14.572038	830.314873	12.997683
14.970821	849.474656	13.002701
14.630575	852.111037	13.007719
14.768677	860.501721	13.012736
14.849246	868.731685	13.017754
15.077613	858.285188	13.022771
14.815327	863.917664	13.027789
14.545080	842.726222	13.032807
14.862554	849.622181	13.037824
14.759008	860.476884	13.042842
14.766026	850.107808	13.047859
15.008885	864.875906	13.052877
14.860565	861.976562	13.057895
15.045314	868.853135	13.062912
15.103622	869.696536	13.067930
14.970530	861.572383	13.072947
14.890443	849.314350	13.077965
14.717420	861.214128	13.082983
14.976588	862.109254	13.088000
14.950520	859.478315	13.093018
14.967141	867.386844	13.098035
15.282059	866.364091	13.103053
15.039148	860.167936	13.108071
15.157175	877.939281	13.113088
14.731664	881.317131	13.118106
14.917282	876.041535	13.123123
15.200370	869.379119	13.128141
14.967232	880.568656	13.133159
14.961999	869.637463	13.138176
14.724207	870.029333	13.143194
14.854684	858.100477	13.148211
15.045683	866.025551	13.153229
15.015349	862.208710	13.158247
15.210357	862.785192	13.163264
15.053047	869.044252	13.168282
15.087774	859.719044	13.173299
15.395982	868.863214	13.178317
15.017214	864.524867	13.183335
14.729597	875.708053	13.188352
14.987114	865.398824	13.193370
15.034261	884.427046	13.198387
15.577256	898.314194	13.203405
15.489875	902.206991	13.208423
15.325835	901.451134	13.213440
15.769609	892.924330	13.218458
15.880114	885.121038	13.223475
15.422678	874.078004	13.228493
15.280085	881.623482	13.233511
15.238340	868.005307	13.238528
15.163021	871.470719	13.243546
14.807842	868.365363	13.248563
15.263109	878.757452	13.253581
15.444988	888.708925	13.258599
15.557490	892.540742	13.263616
15.376782	896.640940	13.268634
15.757268	898.903563	13.273651
16.266337	886.426614	13.278669
15.406860	879.268930	13.283687
15.674826	876.077913	13.288704
15.465923	859.471108	13.293722
15.254455	857.268443	13.298739
15.779857	865.301795	13.303757
15.430199	880.285315	13.308775
15.619267	882.212733	13.313792
15.938697	874.671696	13.318810
15.748466	868.659400	13.323827
15.519053	869.422035	13.328845
15.381377	867.924215	13.333863
15.679781	876.942877	13.338880
15.916366	884.644832	13.343898
15.696481	869.696400	13.348915
15.567198	886.080543	13.353933
15.642654	897.277151	13.358951
15.571328	894.691766	13.363968
15.496188	889.918786	13.368986
15.456496	893.269091	13.374003
15.782257	894.303472	13.379021
15.326475	889.360482	13.384039
15.641285	891.369950	13.389056
15.884998	879.986493	13.394074
15.634167	891.527299	13.399091
15.951432	896.510018	13.404109
16.078592	881.001791	13.409127
15.653636	896.285591	13.414144
15.810772	885.080471	13.419162
15.772519	900.911042	13.424179
16.260058	892.689723	13.429197
15.649979	907.342580	13.434215
16.018580	887.452433	13.439232
16.267608	900.846174	13.444250
15.847569	901.347571	13.449267
15.924120	895.585985	13.454285
16.019154	891.780891	13.459303
16.327543	908.620230	13.464320
16.295787	886.878445	13.469338
15.801634	894.812258	13.474355
16.149800	893.454662	13.479373
16.207957	890.383431	13.484391
16.083663	891.876635	13.489408
15.983266	888.079631	13.494426
15.986947	923.882672	13.499443
16.330855	899.016271	13.504461
16.206598	917.028117	13.509479
16.185929	921.516435	13.514496
16.457216	921.900045	13.519514
16.368176	895.158442	13.524531
16.317115	884.817046	13.529549
16.143707	876.580484	13.534567
16.294133	879.368105	13.539584
16.494210	875.772271	13.544602
16.278605	889.398652	13.549619
16.444613	875.906628	13.554637
16.350642	884.684702	13.559655
16.474955	882.096115	13.564672
16.698742	886.242035	13.569690
16.403997	880.809364	13.574707
16.607253	888.015480	13.579725
16.289535	888.067990	13.584743
16.267294	883.783388	13.589760
16.550401	886.975749	13.594778
16.274776	885.084589	13.599795
16.531263	888.133060	13.604813
16.797461	872.961222	13.609831
16.599440	871.417876	13.614848
16.172006	872.924373	13.619866
16.520417	870.559515	13.624883
16.487057	875.152941	13.629901
16.582281	889.865561	13.634919
16.498231	894.765720	13.639936
16.611829	887.058151	13.644954
16.540943	876.793443	13.649971
16.810972	884.184438	13.654989
16.711871	868.861903	13.660007
16.791065	883.638469	13.665024
16.688304	862.704190	13.670042
16.599563	886.187698	13.675059
16.725168	862.516758	13.680077
16.666578	880.476309	13.685095
16.446670	869.386842	13.690112
16.615561	880.531590	13.695130
16.561926	897.995093	13.700147
16.566217	907.693910	13.705165
16.747919	905.484812	13.710183
16.534837	917.200726	13.715200
16.509686	906.167928	13.720218
16.541177	905.570753	13.725235
17.251571	911.891185	13.730253
17.387733	908.562533	13.735271
17.152083	923.234710	13.740288
17.269782	907.081751	13.745306
16.973599	911.796235	13.750323
17.372941	908.122986	13.755341
17.057263	916.557990	13.760359
17.093271	901.786302	13.765376
17.175071	880.423667	13.770394
16.807334	886.139800	13.775411
16.850960	875.124760	13.780429
16.999160	900.410300	13.785447
17.169948	892.427006	13.790464
17.075430	899.162389	13.795482
17.039137	905.330715	13.800499
17.150775	912.386548	13.805517
17.199155	910.741962	13.810535
16.954914	919.944887	13.815552
17.180890	909.302344	13.820570
17.127925	922.880721	13.825587
17.187535	902.947766	13.830605
17.164388	923.301863	13.835623
17.065803	916.120265	13.840640
16.959391	917.293372	13.845658
17.096193	910.762861	13.850675
17.160009	904.535409	13.855693
17.242579	921.209965	13.860711
17.162624	897.912841	13.865728
17.277457	901.402236	13.870746
16.958851	916.185507	13.875763
16.832431	916.755577	13.880781
17.136867	908.032875	13.885799
17.122147	922.312602	13.890816
17.726550	936.236771	13.895834
17.333300	929.929147	13.900851
17.607891	944.433777	13.905869
17.493775	924.129776	13.910887
17.247556	917.204504	13.915904
17.765368	925.274174	13.920922
17.518353	916.047643	13.925939
17.473780	918.824790	13.930957
17.322392	922.802660	13.935975
17.316649	933.041402	13.940992
17.626545	948.876481	13.946010
17.454885	942.132628	13.951027
17.608689	923.867198	13.956045
17.793199	933.659939	13.961063
17.551361	938.584120	13.966080
18.037284	935.685042	13.971098
17.751767	940.173836	13.976115
17.818979	918.602686	13.981133
18.029079	921.178340	13.986151
17.771901	921.614054	13.991168
17.536868	904.114426	13.996186
17.586572	918.314131	14.001203
17.973171	918.651428	14.006221
17.674288	926.498474	14.011239
17.624915	922.524371	14.016256
17.737167	926.736753	14.021274
17.848232	941.034800	14.026291
17.800337	926.214937	14.031309
18.040003	933.078036	14.036327
17.773641	928.623384	14.041344
18.274991	925.938140	14.046362
17.778894	922.786098	14.051379
17.776365	922.418011	14.056397
17.617241	933.653806	14.061415
17.631906	926.359416	14.066432
18.146334	929.357102	14.071450
17.868163	939.288791	14.076467
18.070888	933.595786	14.081485
17.949708	938.655895	14.086503
17.950233	929.517649	14.091520
17.959847	927.965077	14.096538
17.723577	927.639062	14.101555
17.732501	920.118417	14.106573
17.935287	931.543946	14.111591
17.993219	913.833803	14.116608
17.871188	934.527034	14.121626
18.012896	955.943644	14.126643
18.261586	967.940801	14.131661
18.257121	956.801203	14.136679
18.103855	973.822415	14.141696
18.258337	951.978986	14.146714
18.627581	957.259851	14.151731
18.490129	952.232746	14.156749
18.688466	940.120903	14.161767
18.438805	926.934179	14.166784
18.528960	908.211785	14.171802
18.338097	918.450507	14.176819
18.379361	921.851991	14.181837
18.344125	909.525980	14.186855
18.212401	913.988171	14.191872
18.290005	898.344673	14.196890
18.304284	908.528897	14.201907
18.221919	912.469183	14.206925
18.376047	922.398695	14.211943
18.443972	941.182178	14.216960
18.436695	940.678591	14.221978
18.572934	959.864188	14.226995
18.852973	945.082217	14.232013
18.474091	931.981689	14.237031
18.406602	930.593199	14.242048
18.256058	943.808189	14.247066
18.610136	939.239391	14.252083
18.872028	957.050425	14.257101
18.728584	950.264020	14.262119
18.454507	954.309700	14.267136
18.656421	962.915430	14.272154
18.661063	961.244611	14.277171
18.610380	953.836038	14.282189
19.055923	948.696060	14.287207
18.921051	963.027195	14.292224
18.865209	948.772754	14.297242
19.020371	956.180897	14.302259
18.896374	935.228970	14.307277
18.644725	922.821616	14.312295
18.615905	952.728847	14.317312
18.970321	946.052937	14.322330
19.041255	969.521895	14.327347
18.759147	962.786936	14.332365
18.832387	956.625384	14.337383
18.732405	955.702874	14.342400
18.912286	934.263636	14.347418
18.743580	955.553831	14.352435
18.578867	953.900570	14.357453
18.646342	946.911440	14.362471
18.474080	947.772579	14.367488
18.766932	953.736372	14.372506
18.790505	970.236550	14.377523
18.793984	965.229448	14.382541
19.400776	983.192715	14.387559
19.302478	975.893157	14.392576
19.313862	976.756913	14.397594
18.906145	947.740677	14.402611
19.113602	950.180094	14.407629
19.149532	972.818731	14.412647
19.067789	994.303219	14.417664
19.586936	976.769577	14.422682
19.319883	959.333504	14.427699
19.116556	951.802557	14.432717
19.093469	966.646191	14.437735
19.297320	966.581021	14.442752
19.611151	952.552817	14.447770
19.381770	962.503913	14.452787
19.194500	967.616675	14.457805
19.162385	948.010725	14.462823
19.093797	986.535539	14.467840
19.488482	969.846383	14.472858
19.552566	989.351247	14.477875
19.495196	986.655299	14.482893
19.603771	983.692420	14.487911
19.524238	995.770801	14.492928
19.335528	971.191539	14.497946
19.558761	990.845159	14.502963
19.444644	969.584444	14.507981
19.532053	980.203592	14.512999
19.039065	973.289455	14.518016
19.751943	971.080342	14.523034
19.686560	956.938172	14.528051
19.326588	981.481651	14.533069
19.864382	975.539409	14.538087
19.433499	987.676633	14.543104
19.606158	982.599353	14.548122
19.422364	976.388559	14.553139
19.645578	975.990055	14.558157
19.712109	985.095119	14.563175
19.635381	996.748339	14.568192
19.635571	968.994149	14.573210
20.022788	971.271415	14.578227
19.545450	976.342177	14.583245
19.405018	984.115343	14.588263
19.674857	965.665374	14.593280
19.700509	971.365631	14.598298
19.887946	976.090374	14.603315
19.746887	999.475247	14.608333
20.019092	995.926998	14.613351
19.987941	1009.602413	14.618368
20.419893	984.581569	14.623386
20.366939	970.731846	14.628403
20.022242	975.952200	14.633421
20.186095	961.587839	14.638439
20.124157	974.419308	14.643456
20.032603	956.901395	14.648474
20.146855	961.591389	14.653491
20.259183	976.848275	14.658509
20.286063	954.870160	14.663527
19.865809	970.664448	14.668544
19.952003	974.519625	14.673562
20.284992	964.613896	14.678579
19.870868	977.814712	14.683597
20.112817	951.580649	14.688615
20.093283	970.284844	14.693632
19.897462	958.390743	14.698650
20.106705	969.600032	14.703667
19.750104	995.089296	14.708685
20.354890	980.716306	14.713703
20.258408	1003.813376	14.718720
20.522839	1002.163976	14.723738
20.675169	988.047496	14.728755
20.641072	1004.592863	14.733773
20.943279	980.770441	14.738791
20.669334	969.949510	14.743808
20.357600	966.980128	14.748826
20.488064	966.231982	14.753843
20.246578	964.878835	14.758861
20.451457	961.025657	14.763879
20.467837	969.302298	14.768896
20.304137	953.362163	14.773914
20.493460	969.891825	14.778931
20.682159	983.541808	14.783949
20.859231	982.617498	14.788967
20.607840	968.222759	14.793984
20.445176	962.505993	14.799002
20.347466	963.558208	14.804019
20.416937	984.783008	14.809037
20.379132	973.797886	14.814055
20.470278	978.437878	14.819072
20.497455	1006.689813	14.824090
20.533677	1003.388481	14.829107
20.391754	991.425619	14.834125
20.702964	990.934836	14.839143
21.039366	990.842743	14.844160
20.786405	1003.049667	14.849178
20.924777	984.582237	14.854195
20.739010	987.415104	14.859213
20.994975	988.076967	14.864231
20.944845	999.591083	14.869248
20.351705	1001.622983	14.874266
20.603728	997.098880	14.879283
21.060563	1022.668969	14.884301
21.090013	1011.459667	14.889319
21.183726	1008.703028	14.894336
21.024804	999.547892	14.899354
21.085238	991.434788	14.904371
20.452503	998.955541	14.909389
21.097980	1016.005297	14.914407
21.230254	1010.920610	14.919424
21.190582	1004.358902	14.924442
21.522976	1015.758156	14.929459
21.048321	994.766088	14.934477
21.249311	1013.381348	14.939495
21.195902	1008.508110	14.944512
20.738257	1010.828566	14.949530
21.391179	1010.862174	14.954547
21.543530	1023.488630	14.959565
21.282877	1021.213576	14.964583
21.289539	1008.832738	14.969600
21.599279	1024.914910	14.974618
21.438458	1003.655370	14.979635
21.481694	1012.039085	14.984653
21.402321	1000.286888	14.989671
21.079232	987.428310	14.994688
20.993808	997.595048	14.999706
21.569956	1020.245146	15.004723
21.240933	1016.376764	15.009741
21.288771	1025.117216	15.014759
21.930352	1003.133194	15.019776
21.282583	1013.983672	15.024794
21.558693	999.740650	15.029811
21.472902	1008.232081	15.034829
21.422312	1008.969205	15.039847
21.395979	1011.837426	15.044864
21.378288	1027.431520	15.049882
21.653313	1008.776755	15.054899
21.367955	1020.028258	15.059917
21.560325	1012.817425	15.064935
21.778474	1004.479482	15.069952
21.435222	1013.882835	15.074970
21.553659	1011.277780	15.079987
21.752651	1024.633848	15.085005
22.021374	1052.184105	15.090023
22.474973	1034.850848	15.095040
21.621258	1017.642531	15.100058
21.609652	1008.079673	15.105075
22.010725	997.974234	15.110093
21.820494	1013.625855	15.115111
22.028158	1001.730774	15.120128
21.725873	1008.347231	15.125146
22.079024	1018.260448	15.130163
21.981061	1019.057456	15.135181
22.200026	1006.614476	15.140199
22.397304	1012.050814	15.145216
21.856860	1011.050043	15.150234
22.030749	1009.530832	15.155251
21.997124	1013.567001	15.160269
22.012816	993.241948	15.165287
22.001570	1000.026394	15.170304
22.174766	1030.794072	15.175322
22.392199	1035.017048	15.180339
22.100469	1012.889680	15.185357
22.086844	1026.466962	15.190375
22.267818	1017.718819	15.195392
22.266581	1032.606238	15.200410
22.292978	1034.947274	15.205427
22.223667	1025.163290	15.210445
22.495311	1042.869196	15.215463
22.370974	1030.078204	15.220480
22.425936	1017.825664	15.225498
22.568259	1030.029279	15.230515
22.402848	999.148741	15.235533
22.387996	1014.584124	15.240551
22.280772	1002.320021	15.245568
21.916698	1015.538577	15.250586
21.995883	1023.321817	15.255603
22.416822	1040.172543	15.260621
22.754866	1031.222297	15.265639
22.548022	1022.319199	15.270656
22.286142	1040.387415	15.275674
22.510461	1015.052887	15.280691
22.649016	1037.427576	15.285709
22.216044	1035.827689	15.290727
22.353546	1039.398782	15.295744
22.386269	1036.936301	15.300762
22.845488	1041.051131	15.305779
22.778368	1035.914269	15.310797
22.334083	1048.268074	15.315815
22.980260	1056.298987	15.320832
22.596382	1067.328281	15.325850
22.974744	1064.546143	15.330867
23.173599	1065.681508	15.335885
23.238393	1053.194201	15.340903
23.153866	1031.083144	15.345920
22.787548	1035.906402	15.350938
22.797019	1013.851374	15.355955
22.769441	1036.775238	15.360973
22.739581	1018.532272	15.365991
23.138673	1041.395376	15.371008
22.632411	1041.828861	15.376026
23.133499	1056.454791	15.381043
23.058466	1067.769383	15.386061
23.253118	1065.392414	15.391079
23.537939	1058.356099	15.396096
23.367790	1062.382762	15.401114
23.303706	1031.608317	15.406131
23.150871	1030.439088	15.411149
23.142683	1037.689565	15.416167
23.253634	1017.423326	15.421184
22.945395	1030.826911	15.426202
22.924481	1028.672534	15.431219
23.354830	1025.852488	15.436237
23.422816	1058.890995	15.441255
23.407800	1069.793898	15.446272
23.383271	1051.761378	15.451290
23.113142	1064.794905	15.456307
23.424803	1042.908545	15.461325
23.483471	1046.398497	15.466343
23.718697	1054.900766	15.471360
23.458958	1037.847947	15.476378
23.301934	1035.376577	15.481395
23.483862	1042.715394	15.486413
23.429811	1065.588177	15.491431
23.809757	1048.932959	15.496448
23.769489	1061.441608	15.501466
23.650537	1038.894898	15.506483
23.344854	1038.225221	15.511501
23.639096	1051.338855	15.516519
23.620287	1046.631991	15.521536
23.390954	1064.471387	15.526554
23.496048	1053.397451	15.531571
23.557484	1063.530419	15.536589
23.485130	1056.123508	15.541607
23.795072	1053.736739	15.546624
23.405163	1058.282966	15.551642
23.462892	1072.758415	15.556659
23.638673	1051.162051	15.561677
23.474539	1064.881927	15.566695
23.833325	1052.236615	15.571712
23.670405	1069.535643	15.576730
24.106717	1088.599981	15.581747
23.984383	1089.665818	15.586765
24.026081	1100.060671	15.591783
24.182393	1077.684702	15.596800
23.811586	1078.468449	15.601818
23.958595	1076.880168	15.606835
24.274782	1083.200207	15.611853
23.747051	1097.671567	15.616871
24.177703	1086.425726	15.621888
24.027964	1087.576288	15.626906
24.205122	1090.670284	15.631923
24.596950	1084.383510	15.636941
24.215803	1080.113194	15.641959
24.134887	1075.479856	15.646976
24.470642	1083.389880	15.651994
24.215493	1077.867839	15.657011
24.411617	1083.462721	15.662029
24.017592	1085.955800	15.667047
24.290813	1079.921939	15.672064
24.247918	1098.641468	15.677082
24.079063	1076.482681	15.682099
24.394569	1082.559978	15.687117
24.316410	1066.735085	15.692135
24.461599	1072.367802	15.697152
24.209699	1068.616946	15.702170
24.053292	1068.716206	15.707187
24.399524	1070.631649	15.712205
23.957853	1076.150376	15.717223
24.291697	1094.603657	15.722240
24.569780	1098.098395	15.727258
24.397701	1111.741396	15.732275
24.892692	1100.549562	15.737293
24.753770	1113.042674	15.742311
24.929284	1103.009669	15.747328
24.751823	1096.119201	15.752346
25.008923	1107.499773	15.757363
25.142594	1093.291322	15.762381
24.545322	1089.132587	15.767399
24.577745	1075.331539	15.772416
24.950291	1098.898258	15.777434
24.604824	1086.466323	15.782451
25.050249	1099.695926	15.787469
24.538435	1103.433968	15.792487
25.057060	1108.071450	15.797504
24.871719	1104.195538	15.802522
24.741719	1108.588718	15.807539
25.206706	1103.653595	15.812557
25.044623	1098.963602	15.817575
25.248849	1075.070533	15.822592
25.098711	1101.687780	15.827610
24.938547	1085.483797	15.832627
25.323654	1101.811998	15.837645
24.959205	1092.959898	15.842663
25.089587	1110.828563	15.847680
25.179663	1098.605088	15.852698
25.066413	1095.148165	15.857715
25.425728	1097.326445	15.862733
25.087506	1107.385166	15.867751
25.087225	1088.630559	15.872768
25.015255	1087.653817	15.877786
24.881040	1075.481988	15.882803
25.281899	1081.650174	15.887821
24.879236	1102.647427	15.892839
25.256504	1116.191680	15.897856
25.339938	1131.563214	15.902874
25.165422	1118.297977	15.907891
25.691813	1131.891107	15.912909
25.646900	1130.716926	15.917927
25.949853	1135.738105	15.922944
25.871703	1114.480690	15.927962
25.775876	1126.382087	15.932979
25.868777	1091.709468	15.937997
25.585091	1091.172931	15.943015
25.495407	1083.247540	15.948032
25.668851	1098.027139	15.953050
25.619017	1101.122436	15.958067
25.962209	1111.474657	15.963085
26.051380	1105.085761	15.968103
25.552030	1102.365020	15.973120
26.019790	1089.088824	15.978138
25.598202	1089.033332	15.983155
25.782354	1098.425645	15.988173
25.890879	1118.811996	15.993191
25.804907	1114.825588	15.998208
25.995628	1118.408470	16.003226
25.868433	1129.386928	16.008243
25.872392	1107.076832	16.013261
26.233807	1109.581952	16.018279
26.120788	1124.580726	16.023296
26.431573	1117.098367	16.028314
25.996022	1127.679068	16.033331
26.008963	1113.117312	16.038349
26.249418	1143.026469	16.043367
26.055542	1129.450126	16.048384
26.148983	1124.560160	16.053402
25.995397	1133.769191	16.058419
26.249056	1115.940860	16.063437
26.150792	1126.434235	16.068455
26.151972	1136.703557	16.073472
26.374442	1129.158246	16.078490
26.390237	1113.777216	16.083507
26.162933	1119.930256	16.088525
26.070874	1114.646935	16.093543
25.743383	1122.787912	16.098560
26.059933	1111.351214	16.103578
25.775156	1135.098350	16.108595
26.495072	1149.678073	16.113613
26.452804	1146.089653	16.118631
26.561177	1166.388810	16.123648
26.528136	1139.577671	16.128666
26.370173	1159.241661	16.133683
26.749078	1140.348264	16.138701
27.072281	1142.102600	16.143719
26.806653	1147.989411	16.148736
27.220061	1134.832171	16.153754
27.015237	1158.242683	16.158771
27.161867	1139.062945	16.163789
26.784908	1123.340901	16.168807
27.051605	1124.647596	16.173824
26.843609	1107.919631	16.178842
26.793949	1119.356809	16.183859
26.956918	1097.416025	16.188877
26.727824	1108.193052	16.193895
26.581197	1103.669262	16.198912
26.953364	1099.128030	16.203930
26.861104	1106.579987	16.208947
26.910041	1111.426947	16.213965
27.120116	1104.813789	16.218983
26.754178	1139.011713	16.224000
27.088362	1119.665604	16.229018
27.173136	1140.019597	16.234035
27.248405	1131.746230	16.239053
27.408878	1142.592730	16.244071
27.190351	1137.039325	16.249088
27.308638	1113.311741	16.254106
26.884817	1123.966074	16.259123
27.235709	1130.943429	16.264141
27.223627	1131.981898	16.269159
26.967690	1125.734748	16.274176
26.830344	1134.561954	16.279194
27.029456	1130.850893	16.284211
27.227837	1134.306756	16.289229
27.087585	1133.191627	16.294247
27.253024	1139.063780	16.299264
27.368195	1126.751411	16.304282
27.443150	1163.895695	16.309299
27.569541	1168.051982	16.314317
27.345013	1174.140131	16.319335
27.656632	1160.298772	16.324352
27.685787	1179.818705	16.329370
27.548066	1164.030713	16.334387
28.017393	1160.181509	16.339405
28.061975	1163.660433	16.344423
27.930852	1142.655573	16.349440
27.911065	1126.362419	16.354458
27.579222	1133.760794	16.359475
27.547808	1128.071576	16.364493
27.744997	1119.307707	16.369511
27.809456	1150.680660	16.374528
27.968113	1147.387208	16.379546
27.691656	1160.755149	16.384563
28.049110	1147.591893	16.389581
27.911995	1164.672149	16.394599
27.678944	1158.812351	16.399616
28.004675	1157.057749	16.404634
27.867422	1163.509729	16.409651
28.149476	1169.921252	16.414669
28.181572	1166.497957	16.419687
28.066472	1163.611171	16.424704
28.227954	1164.961136	16.429722
28.045536	1165.257957	16.434739
28.092166	1157.026898	16.439757
28.237124	1163.013344	16.444775
27.769070	1173.110488	16.449792
27.970011	1160.893636	16.454810
28.159555	1167.857524	16.459827
28.362260	1161.575403	16.464845
28.115735	1164.652638	16.469863
28.179410	1173.627510	16.474880
28.135022	1168.787761	16.479898
28.479246	1202.446620	16.484915
28.568002	1192.545090	16.489933
28.673562	1190.013179	16.494951
28.375859	1190.308485	16.499968
28.654145	1188.084272	16.504986
28.563611	1185.269586	16.510003
28.575052	1179.354813	16.515021
28.576197	1190.314566	16.520039
28.463660	1183.861945	16.525056
28.580916	1180.184867	16.530074
28.662431	1210.580157	16.535091
28.704448	1179.694299	16.540109
29.030759	1170.368835	16.545127
28.666676	1189.957012	16.550144
28.703723	1169.469374	16.555162
28.971464	1185.774059	16.560179
28.828457	1168.750906	16.565197
28.931519	1179.248047	16.570215
28.693561	1187.513896	16.575232
28.880333	1177.960561	16.580250
28.985174	1201.700586	16.585267
28.945439	1185.986318	16.590285
29.132689	1185.270993	16.595303
28.692664	1177.120640	16.600320
29.136423	1198.628785	16.605338
28.760596	1182.778078	16.610355
28.870631	1186.853529	16.615373
28.945615	1183.474214	16.620391
29.064518	1191.965869	16.625408
29.564192	1216.730376	16.630426
29.362754	1206.955317	16.635443
29.531140	1209.641728	16.640461
29.568885	1196.385233	16.645479
28.986089	1198.637640	16.650496
29.259176	1190.905432	16.655514
29.501117	1213.471513	16.660531
29.369515	1215.822844	16.665549
29.648060	1221.178324	16.670567
29.603205	1213.540565	16.675584
29.384816	1192.473698	16.680602
29.358065	1205.536794	16.685619
29.739419	1196.330437	16.690637
29.814642	1209.482664	16.695655
29.663491	1195.554302	16.700672
29.799906	1200.781230	16.705690
29.964470	1192.363969	16.710707
29.749232	1210.510386	16.715725
29.847062	1198.335833	16.720743
29.896003	1207.959467	16.725760
29.982177	1185.077237	16.730778
29.746735	1184.109496	16.735795
29.703425	1208.237609	16.740813
30.178792	1188.233191	16.745831
30.034542	1210.066717	16.750848
30.185471	1193.620505	16.755866
29.879370	1194.204239	16.760883
29.841797	1190.832895	16.765901
30.073897	1197.072215	16.770919
29.882359	1204.172601	16.775936
30.371314	1198.962291	16.780954
29.911992	1208.887976	16.785971
30.047196	1190.450244	16.790989
30.279530	1194.741554	16.796007
29.806550	1190.298827	16.801024
30.065570	1199.738660	16.806042
30.372979	1187.819473	16.811059
30.407710	1195.704909	16.816077
30.569938	1185.092094	16.821095
30.331066	1196.651522	16.826112
30.336115	1195.320689	16.831130
30.211812	1199.681071	16.836147
30.238265	1198.433688	16.841165
30.733368	1195.385934	16.846183
30.314792	1203.500677	16.851200
30.314743	1188.536956	16.856218
30.555284	1192.188967	16.861235
30.447869	1192.954679	16.866253
30.696929	1175.730145	16.871271
30.233051	1197.658491	16.876288
30.466804	1208.726043	16.881306
30.513982	1219.107968	16.886323
30.475762	1220.542798	16.891341
30.724476	1219.779527	16.896359
30.404975	1215.482257	16.901376
30.862436	1228.986594	16.906394
30.972773	1210.932386	16.911411
30.870196	1223.173871	16.916429
31.151772	1209.916826	16.921447
31.072174	1216.349067	16.926464
31.049198	1210.941821	16.931482
30.749670	1218.139962	16.936499
30.918202	1204.350352	16.941517
31.027340	1217.437252	16.946535
30.907882	1197.244079	16.951552
30.810689	1200.372019	16.956570
31.131238	1209.985014	16.961587
31.053402	1209.921817	16.966605
31.054485	1199.619709	16.971623
31.506460	1237.376122	16.976640
31.349919	1218.541788	16.981658
31.265773	1218.158350	16.986675
31.198305	1226.613121	16.991693
31.569834	1229.429314	16.996711
31.590063	1239.205808	17.001728
31.864650	1218.687903	17.006746
31.499568	1221.611257	17.011763
31.411139	1207.954047	17.016781
31.831344	1204.278463	17.021799
31.380028	1211.948825	17.026816
31.614353	1201.432523	17.031834
31.469007	1220.781097	17.036851
31.579690	1216.229118	17.041869
31.990955	1214.302931	17.046887
31.825551	1205.710323	17.051904
31.444837	1202.036022	17.056922
31.827525	1215.039338	17.061939
31.722301	1223.961559	17.066957
31.972460	1242.686466	17.071975
32.117710	1246.961677	17.076992
32.262044	1229.037232	17.082010
32.391705	1211.986585	17.087027
32.186137	1207.826653	17.092045
32.151220	1206.805404	17.097063
31.926999	1185.005921	17.102080
32.008462	1197.631836	17.107098
31.978001	1186.034171	17.112115
32.053959	1185.007098	17.117133
32.399958	1184.430264	17.122151
32.316585	1184.788751	17.127168
32.110462	1202.189043	17.132186
32.070453	1197.726720	17.137203
32.015746	1206.927722	17.142221
32.177974	1201.416171	17.147239
32.143196	1222.497150	17.152256
32.569393	1225.363251	17.157274
32.638720	1236.295632	17.162291
32.223302	1218.580404	17.167309
32.546624	1241.526787	17.172327
32.267983	1231.097793	17.177344
32.299396	1246.561387	17.182362
32.540710	1222.269726	17.187379
32.569430	1246.913238	17.192397
32.656014	1231.380660	17.197415
32.438247	1228.170748	17.202432
32.471545	1236.316323	17.207450
32.669011	1227.777885	17.212467
32.426296	1249.937806	17.217485
32.208449	1227.405290	17.222503
32.164651	1236.335277	17.227520
32.466806	1234.931136	17.232538
32.866093	1248.608451	17.237555
32.676230	1253.483504	17.242573
32.844941	1254.726106	17.247591
33.135766	1244.672279	17.252608
32.956110	1246.833177	17.257626
33.205973	1232.858191	17.262643
32.886194	1228.338081	17.267661
32.955413	1239.434126	17.272679
32.924078	1243.185986	17.277696
32.708337	1244.238438	17.282714
32.720058	1246.186550	17.287731
32.690610	1260.787286	17.292749
32.972050	1283.440426	17.297767
33.469167	1275.438924	17.302784
33.239202	1268.396756	17.307802
33.308273	1279.079661	17.312819
33.303060	1271.941899	17.317837
33.663399	1267.811240	17.322855
33.432605	1289.119541	17.327872
33.488350	1277.599272	17.332890
34.025693	1270.811122	17.337907
33.601927	1279.126127	17.342925
33.889789	1272.606711	17.347943
34.028133	1281.292107	17.352960
33.826033	1261.035948	17.357978
33.631683	1250.714933	17.362995
33.737226	1242.794884	17.368013
33.696150	1267.361893	17.373031
34.007261	1276.618500	17.378048
33.554619	1264.297121	17.383066
33.663443	1264.793199	17.388083
33.637115	1271.795661	17.393101
33.632086	1269.797840	17.398119
34.097503	1260.102858	17.403136
33.579699	1269.371372	17.408154
34.050798	1265.730759	17.413171
33.862512	1269.170451	17.418189
33.774069	1250.114537	17.423207
33.857833	1258.617941	17.428224
33.475079	1268.865088	17.433242
34.096995	1280.247989	17.438259
34.137367	1295.526040	17.443277
34.221859	1295.914256	17.448295
34.344031	1305.194133	17.453312
34.373818	1306.865609	17.458330
34.734573	1287.446606	17.463347
34.671247	1283.566130	17.468365
34.606359	1305.960170	17.473383
34.596790	1292.033808	17.478400
33.984280	1303.899789	17.483418
34.629267	1293.398713	17.488435
34.785982	1295.924113	17.493453
34.514475	1302.414574	17.498471
34.349413	1298.079064	17.503488
34.238712	1290.433649	17.508506
34.137841	1313.476413	17.513523
34.282034	1292.260927	17.518541
34.242453	1291.930641	17.523559
34.600993	1303.918373	17.528576
34.713089	1308.383290	17.533594
35.023882	1320.993453	17.538611
34.758847	1319.270528	17.543629
34.800641	1319.961796	17.548647
35.066167	1334.537278	17.553664
34.952746	1317.942830	17.558682
35.202212	1335.813335	17.563699
35.228104	1318.840826	17.568717
34.989052	1335.445906	17.573735
35.318165	1306.592297	17.578752
35.056899	1322.747298	17.583770
35.583393	1313.915025	17.588787
35.516243	1309.771848	17.593805
35.407533	1307.715483	17.598823
35.263220	1280.867477	17.603840
34.923035	1288.452303	17.608858
35.043138	1292.580929	17.613875
35.223233	1309.410941	17.618893
35.393216	1309.048089	17.623911
35.201801	1320.095649	17.628928
35.207811	1334.204682	17.633946
35.483797	1319.226214	17.638963
35.137719	1315.657160	17.643981
35.294835	1308.331667	17.648999
35.486815	1309.705438	17.654016
35.458903	1311.456807	17.659034
35.640755	1323.076106	17.664051
35.738982	1331.662377	17.669069
35.734588	1336.032700	17.674087
35.897521	1339.977037	17.679104
35.717817	1340.613198	17.684122
36.177321	1338.610831	17.689139
36.146770	1329.698494	17.694157
35.965755	1352.400704	17.699175
36.304508	1325.839934	17.704192
36.144802	1323.588694	17.709210
36.120794	1296.155159	17.714227
36.105893	1298.913893	17.719245
36.144639	1293.067283	17.724263
36.317785	1295.245558	17.729280
36.185941	1278.193081	17.734298
35.861136	1287.973290	17.739315
36.016066	1306.593272	17.744333
36.135364	1316.087263	17.749351
35.813720	1331.598069	17.754368
36.269899	1335.589888	17.759386
36.597793	1327.076091	17.764403
36.633775	1336.893833	17.769421
36.201853	1326.636626	17.774439
36.269514	1336.589849	17.779456
36.372744	1330.901725	17.784474
36.246159	1320.861917	17.789491
36.296525	1344.269215	17.794509
36.478287	1364.631294	17.799527
36.952402	1355.795648	17.804544
36.638080	1375.191921	17.809562
36.492339	1358.475338	17.814579
36.522565	1371.594205	17.819597
36.698783	1368.480834	17.824615
37.171390	1358.743568	17.829632
36.514850	1366.223264	17.834650
36.929744	1359.774138	17.839667
36.985581	1364.053432	17.844685
36.736232	1360.234576	17.849703
36.812696	1362.906191	17.854720
36.768386	1359.220443	17.859738
36.969530	1366.474960	17.864755
36.939009	1372.497375	17.869773
36.954927	1374.143892	17.874791
37.505946	1380.759329	17.879808
37.264986	1379.530045	17.884826
37.462035	1397.134542	17.889843
37.634788	1380.783518	17.894861
37.440403	1385.807948	17.899879
37.622644	1372.296569	17.904896
37.262273	1369.657217	17.909914
37.279376	1362.175644	17.914931
37.558425	1371.250051	17.919949
37.467649	1383.777052	17.924967
37.590070	1381.526415	17.929984
37.550373	1369.576573	17.935002
37.589379	1382.782366	17.940019
38.230200	1371.599989	17.945037
37.738634	1367.551631	17.950055
38.043700	1371.315732	17.955072
38.101339	1356.608002	17.960090
38.003663	1353.767994	17.965107
38.150405	1363.122962	17.970125
37.860546	1351.188693	17.975143
37.869565	1333.641721	17.980160
37.876572	1350.384561	17.985178
37.679049	1338.168174	17.990195
38.115540	1345.860454	17.995213
37.767476	1372.388171	18.000231
38.212730	1359.151084	18.005248
37.928445	1368.416985	18.010266
38.058682	1378.552568	18.015283
38.107518	1371.444698	18.020301
38.113901	1391.044336	18.025319
38.162998	1363.778186	18.030336
38.216950	1364.857223	18.035354
38.306399	1372.400416	18.040371
38.403488	1372.511515	18.045389
38.283880	1375.807234	18.050407
38.441223	1366.548640	18.055424
38.204581	1376.625585	18.060442
38.252667	1400.938461	18.065459
38.834508	1405.167744	18.070477
38.736410	1401.373282	18.075495
38.999912	1420.300980	18.080512
38.805453	1402.484669	18.085530
38.749570	1403.582155	18.090547
38.939055	1408.422613	18.095565
38.936894	1398.890227	18.100583
38.645365	1414.985478	18.105600
38.673276	1402.923968	18.110618
38.844131	1402.839650	18.115635
39.061329	1392.149217	18.120653
38.832607	1405.206893	18.125671
38.872009	1387.210941	18.130688
38.834194	1395.360086	18.135706
38.743329	1406.426222	18.140723
38.865057	1402.358575	18.145741
38.670795	1438.435366	18.150759
39.252853	1428.312628	18.155776
39.304945	1434.442452	18.160794
39.284203	1433.300170	18.165811
39.404613	1418.160250	18.170829
39.323097	1433.868334	18.175847
39.807647	1410.509493	18.180864
39.879627	1418.063664	18.185882
39.734493	1420.823965	18.190899
39.780826	1425.477993	18.195917
39.494281	1410.750530	18.200935
39.499014	1428.069492	18.205952
39.831030	1420.012933	18.210970
39.991542	1422.850257	18.215987
39.951629	1416.007568	18.221005
40.029128	1426.357956	18.226023
40.068670	1420.262303	18.231040
40.012038	1418.669065	18.236058
39.996408	1430.820873	18.241075
39.861919	1427.971091	18.246093
39.963585	1430.075389	18.251111
39.998207	1422.189404	18.256128
39.987880	1421.205112	18.261146
40.105634	1416.466218	18.266163
39.967687	1415.986472	18.271181
40.076712	1424.792320	18.276199
40.169938	1418.963525	18.281216
40.179751	1419.342239	18.286234
40.272281	1422.856498	18.291251
40.371063	1405.740281	18.296269
40.119601	1429.981078	18.301287
40.327227	1416.580498	18.306304
40.521461	1427.617347	18.311322
40.198964	1417.949638	18.316339
40.435447	1429.364266	18.321357
40.173057	1427.765273	18.326375
40.511374	1435.028349	18.331392
40.720927	1446.761347	18.336410
40.519362	1452.778602	18.341427
40.665390	1447.916548	18.346445
40.764896	1452.018116	18.351463
40.706914	1455.020559	18.356480
40.771840	1449.993402	18.361498
40.156130	1449.780361	18.366515
40.650672	1440.611834	18.371533
40.675406	1472.254258	18.376551
40.763416	1464.447993	18.381568
41.026790	1480.066461	18.386586
41.018758	1483.573243	18.391603
41.120341	1472.416039	18.396621
41.318294	1486.425004	18.401639
41.284403	1477.153171	18.406656
41.523357	1472.074221	18.411674
41.464880	1476.782684	18.416691
41.435630	1463.346814	18.421709
41.619278	1473.528741	18.426727
41.498226	1463.707563	18.431744
41.638665	1473.689785	18.436762
41.155641	1472.623499	18.441779
41.925721	1475.369351	18.446797
41.725680	1475.886955	18.451815
41.697449	1468.558164	18.456832
41.917844	1482.993738	18.461850
41.782493	1468.378311	18.466867
41.897889	1472.314105	18.471885
41.789082	1458.921202	18.476903
41.742301	1467.266707	18.481920
41.865588	1457.971175	18.486938
41.567784	1462.208466	18.491955
41.731179	1481.400859	18.496973
41.631625	1468.334498	18.501991
41.413462	1474.951226	18.507008
41.842339	1471.241477	18.512026
41.566431	1506.697313	18.517043
41.808410	1493.210692	18.522061
42.125133	1514.071226	18.527079
41.882445	1506.524170	18.532096
42.235848	1501.773665	18.537114
42.244229	1514.839682	18.542131
42.483915	1496.222244	18.547149
42.191497	1496.124147	18.552167
42.096093	1513.109139	18.557184
42.430465	1532.092572	18.562202
42.411295	1523.466764	18.567219
42.927577	1521.535781	18.572237
42.561460	1530.135328	18.577255
42.863034	1519.439425	18.582272
43.051596	1520.265569	18.587290
42.699442	1542.137566	18.592307
42.967293	1525.475655	18.597325
42.970002	1495.174963	18.602343
42.439858	1497.597510	18.607360
43.167191	1511.884786	18.612378
42.937100	1507.882040	18.617395
43.151407	1509.229014	18.622413
43.083221	1522.590702	18.627431
43.085794	1508.435807	18.632448
43.131843	1517.028148	18.637466
43.004869	1508.526833	18.642483
43.278383	1525.683896	18.647501
43.459832	1518.799070	18.652519
43.506756	1514.590244	18.657536
43.652460	1522.016954	18.662554
43.511645	1503.563840	18.667571
43.112483	1494.968171	18.672589
43.527130	1486.366639	18.677607
43.523265	1504.599905	18.682624
43.852826	1498.043392	18.687642
43.498910	1493.573027	18.692659
43.561584	1512.043186	18.697677
43.457812	1504.727452	18.702695
43.586566	1507.551342	18.707712
43.810961	1498.078285	18.712730
43.375225	1499.630001	18.717747
43.805020	1498.681512	18.722765
43.704703	1511.632940	18.727783
43.669300	1502.099291	18.732800
44.059876	1517.538445	18.737818
43.567980	1508.226850	18.742835
43.571718	1520.040658	18.747853
43.763655	1541.895661	18.752871
44.078128	1532.697892	18.757888
44.186735	1536.721912	18.762906
44.136798	1530.081574	18.767923
44.327420	1532.890424	18.772941
44.436661	1535.315956	18.777959
44.315347	1528.119325	18.782976
44.724798	1527.394524	18.787994
44.612359	1523.646191	18.793011
44.473406	1538.075170	18.798029
44.588026	1528.525373	18.803047
44.320203	1538.016658	18.808064
44.926046	1508.781379	18.813082
44.446768	1531.671499	18.818099
44.854097	1547.550931	18.823117
44.929800	1530.660881	18.828135
44.914139	1549.234071	18.833152
44.822346	1529.823811	18.838170
44.643139	1541.804256	18.843187
44.494491	1530.437036	18.848205
44.988851	1521.563901	18.853223
44.936189	1543.599061	18.858240
44.902580	1541.548754	18.863258
45.026200	1554.384783	18.868275
45.142742	1568.701801	18.873293
45.643000	1560.457361	18.878311
45.307560	1585.050792	18.883328
45.806203	1555.345839	18.888346
45.149654	1557.688123	18.893363
45.536057	1542.475981	18.898381
45.599110	1563.242507	18.903399
45.545941	1562.455205	18.908416
45.394444	1529.581750	18.913434
45.479192	1538.515764	18.918451
45.264433	1543.476010	18.923469
45.511842	1551.417213	18.928487
45.318204	1552.109118	18.933504
45.502511	1558.431174	18.938522
45.678569	1550.154603	18.943539
45.549382	1566.999402	18.948557
45.779804	1550.310881	18.953575
45.717541	1561.709241	18.958592
45.890646	1559.819318	18.963610
45.641164	1559.052157	18.968627
45.866926	1575.564449	18.973645
46.150855	1573.760225	18.978663
46.283843	1583.561997	18.983680
46.319941	1579.498023	18.988698
46.263490	1580.178576	18.993715
46.270462	1576.890318	18.998733
46.367955	1578.947994	19.003751
46.180211	1590.154656	19.008768
46.680455	1575.878489	19.013786
46.703296	1576.601538	19.018803
46.411216	1561.315118	19.023821
46.664404	1572.935218	19.028839
46.435893	1572.270081	19.033856
46.505642	1566.312951	19.038874
46.456048	1578.281551	19.043891
46.397186	1581.338189	19.048909
46.245317	1581.223951	19.053927
46.325997	1585.165215	19.058944
46.506660	1567.680636	19.063962
47.012051	1593.427284	19.068979
46.721208	1604.638102	19.073997
47.310296	1584.860879	19.079015
46.845878	1602.121669	19.084032
47.377196	1586.992501	19.089050
47.446757	1588.653401	19.094067
46.996613	1583.330489	19.099085
47.284545	1569.405587	19.104103
47.391052	1586.177903	19.109120
47.599222	1581.212545	19.114138
47.336291	1589.022399	19.119155
47.285630	1580.610577	19.124173
47.439075	1583.327569	19.129191
47.481194	1577.792532	19.134208
47.423603	1600.601262	19.139226
47.491084	1583.736719	19.144243
47.330428	1596.616514	19.149261
47.698239	1587.584763	19.154279
47.106646	1586.816863	19.159296
47.307086	1598.343752	19.164314
47.411674	1618.979007	19.169331
47.439581	1616.170057	19.174349
48.094805	1604.259986	19.179367
48.055158	1618.690147	19.184384
47.990337	1601.445858	19.189402
47.882354	1620.908717	19.194419
47.443851	1606.554235	19.199437
47.902829	1623.567102	19.204455
48.147541	1647.076579	19.209472
48.337770	1637.415420	19.214490
48.475208	1647.490851	19.219507
48.328792	1640.388258	19.224525
48.592781	1654.137893	19.229543
48.440381	1639.523152	19.234560
48.425581	1637.982906	19.239578
48.454116	1635.497798	19.244595
48.755886	1627.070124	19.249613
48.746724	1635.156996	19.254631
48.820342	1634.816557	19.259648
48.826332	1637.799313	19.264666
49.103573	1633.702857	19.269683
48.957395	1643.771030	19.274701
49.039140	1641.000216	19.279719
48.928407	1649.007935	19.284736
48.889085	1634.571520	19.289754
49.019848	1639.140416	19.294771
48.874390	1631.540918	19.299789
48.851157	1643.733513	19.304807
48.938254	1639.229295	19.309824
48.991018	1632.550586	19.314842
49.248098	1629.671485	19.319859
49.353188	1629.784315	19.324877
49.123870	1623.641297	19.329895
49.176476	1620.388788	19.334912
49.242757	1634.353519	19.339930
49.500617	1635.394747	19.344947
49.374366	1659.581758	19.349965
49.414280	1657.070656	19.354983
49.268040	1663.088002	19.360000
49.594930	1668.564956	19.365018
49.768135	1667.167817	19.370035
49.206346	1682.757531	19.375053
49.558671	1668.504738	19.380071
49.669277	1677.792854	19.385088
49.607995	1671.126678	19.390106
50.252037	1671.070343	19.395123
50.255791	1669.470643	19.400141
50.771075	1686.620703	19.405159
50.336339	1644.229887	19.410176
50.472831	1646.497324	19.415194
50.046388	1651.157514	19.420211
50.364109	1651.719163	19.425229
50.420886	1653.305427	19.430247
50.478887	1647.299332	19.435264
50.270262	1654.114323	19.440282
50.563348	1651.198074	19.445299
50.545077	1662.885538	19.450317
50.390878	1646.850213	19.455335
50.490926	1678.512994	19.460352
50.572098	1674.697597	19.465370
50.650051	1681.497422	19.470387
50.530272	1676.113390	19.475405
50.830997	1681.707937	19.480423
50.599992	1672.698532	19.485440
50.833154	1662.706510	19.490458
50.619499	1670.127531	19.495475
50.773429	1676.896791	19.500493
50.908214	1693.545481	19.505511
51.243101	1709.544217	19.510528
51.030533	1714.999036	19.515546
51.133177	1724.876372	19.520563
50.921652	1712.174202	19.525581
51.344075	1711.901883	19.530599
51.225002	1701.940391	19.535616
51.331731	1693.514799	19.540634
51.546824	1703.250826	19.545651
51.350577	1698.959127	19.550669
51.031028	1708.065640	19.555687
51.257498	1695.463610	19.560704
51.150103	1735.073080	19.565722
51.521361	1722.424469	19.570739
51.500983	1733.480570	19.575757
51.716800	1741.800740	19.580775
51.832716	1729.975659	19.585792
51.865156	1738.151263	19.590810
52.136080	1723.548951	19.595827
52.163143	1736.366352	19.600845
52.279603	1727.222740	19.605863
52.383296	1732.005839	19.610880
52.364026	1723.847066	19.615898
52.272777	1726.878875	19.620915
52.046213	1718.150936	19.625933
52.220540	1729.085114	19.630951
52.098823	1716.750995	19.635968
52.437619	1742.770947	19.640986
52.618310	1746.931409	19.646003
52.341451	1764.994489	19.651021
52.217006	1750.737550	19.656039
52.619491	1744.657565	19.661056
52.735119	1757.815692	19.666074
53.110685	1750.124034	19.671091
52.681812	1753.354426	19.676109
52.548244	1752.282920	19.681127
52.676980	1751.000975	19.686144
52.666021	1772.330891	19.691162
52.770639	1749.570631	19.696179
52.885198	1769.769882	19.701197
53.082171	1772.215003	19.706215
52.972581	1789.326931	19.711232
52.998640	1772.741316	19.716250
52.955903	1777.503754	19.721267
52.974210	1773.620784	19.726285
53.277992	1778.733263	19.731303
53.734113	1768.220072	19.736320
53.384360	1781.640324	19.741338
53.574177	1761.454439	19.746355
53.686334	1782.742965	19.751373
53.653032	1785.325531	19.756391
53.955419	1775.976692	19.761408
53.650511	1788.395342	19.766426
53.727819	1770.033987	19.771443
53.655027	1787.180474	19.776461
53.649683	1794.902697	19.781479
53.909934	1808.272356	19.786496
53.782674	1807.841805	19.791514
54.215552	1804.810909	19.796531
54.235597	1794.150612	19.801549
54.037659	1786.359060	19.806567
53.866075	1800.166831	19.811584
54.180302	1803.483058	19.816602
54.243853	1806.284223	19.821619
54.105090	1789.172489	19.826637
54.422004	1807.865901	19.831655
54.589191	1816.550378	19.836672
54.488282	1822.418984	19.841690
54.932265	1822.331747	19.846707
54.851640	1829.985833	19.851725
55.061487	1818.666715	19.856743
55.097348	1819.747003	19.861760
54.672418	1802.651348	19.866778
54.929450	1791.888320	19.871795
55.118916	1787.221206	19.876813
54.696300	1805.193383	19.881831
54.921925	1799.935068	19.886848
54.971576	1825.072412	19.891866
55.000702	1814.997889	19.896883
54.747913	1808.700635	19.901901
55.106060	1825.812756	19.906919
55.217127	1819.423782	19.911936
55.310274	1815.959847	19.916954
55.425303	1822.696336	19.921971
55.583739	1807.023471	19.926989
55.327147	1827.526505	19.932007
55.425062	1813.330283	19.937024
55.636154	1842.845444	19.942042
55.663711	1840.887037	19.947059
55.756346	1852.862658	19.952077
55.636776	1839.186609	19.957095
56.034896	1854.713719	19.962112
55.740150	1851.730921	19.967130
55.990531	1845.947044	19.972147
56.131266	1851.356321	19.977165
56.066863	1856.745966	19.982183
56.040503	1845.940378	19.987200
55.988589	1836.234381	19.992218
55.851692	1849.765453	19.997235
55.910235	1839.752378	20.002253
55.860306	1845.848351	20.007271
56.245838	1845.063132	20.012288
56.430193	1867.907066	20.017306
56.445049	1871.484157	20.022323
56.405060	1876.865051	20.027341
56.430830	1880.483048	20.032359
56.561200	1868.442225	20.037376
56.613821	1878.559969	20.042394
56.880094	1870.695993	20.047411
56.883565	1877.815537	20.052429
56.792505	1869.078897	20.057447
57.251622	1863.923878	20.062464
56.812148	1887.345052	20.067482
57.369927	1858.310716	20.072499
57.169257	1871.869273	20.077517
56.774852	1864.304992	20.082535
56.881272	1865.596514	20.087552
56.874887	1877.447106	20.092570
57.036416	1893.752190	20.097587
57.213092	1883.600198	20.102605
57.145365	1887.649218	20.107623
56.856537	1898.969542	20.112640
56.983704	1916.967020	20.117658
57.558815	1913.000466	20.122675
57.930640	1913.861101	20.127693
57.947809	1928.280294	20.132711
58.238291	1905.418236	20.137728
58.086318	1920.749657	20.142746
58.551471	1902.308110	20.147763
58.433524	1902.427883	20.152781
58.221207	1898.880770	20.157799
58.449364	1878.953897	20.162816
58.552759	1899.497029	20.167834
58.573254	1876.995613	20.172851
58.178471	1877.969936	20.177869
57.916695	1885.918699	20.182887
58.368423	1895.469711	20.187904
58.281015	1878.967777	20.192922
58.257340	1883.539044	20.197939
58.617181	1905.428422	20.202957
58.403977	1904.819095	20.207975
58.547912	1921.642571	20.212992
58.715461	1907.467918	20.218010
58.503444	1912.711633	20.223027
58.627699	1903.560723	20.228045
58.831108	1912.203941	20.233063
58.847735	1913.097882	20.238080
58.509749	1905.804521	20.243098
58.898134	1924.615867	20.248115
59.057813	1940.538601	20.253133
59.242342	1954.515968	20.258151
59.272376	1945.936013	20.263168
59.086919	1947.918275	20.268186
59.273960	1950.120623	20.273203
59.522372	1937.124782	20.278221
59.569657	1950.867392	20.283239
59.413716	1934.907237	20.288256
59.264738	1940.916680	20.293274
59.673011	1925.134312	20.298291
59.575900	1932.577139	20.303309
59.398919	1943.076405	20.308327
59.842656	1931.903068	20.313344
59.668446	1932.465326	20.318362
59.782756	1956.874519	20.323379
59.843261	1949.948376	20.328397
60.070617	1946.540566	20.333415
60.403586	1958.140887	20.338432
60.035598	1947.840515	20.343450
59.875293	1950.607058	20.348467
60.247217	1946.543683	20.353485
60.324807	1946.249029	20.358503
60.232745	1940.622375	20.363520
60.095901	1945.142491	20.368538
60.119514	1950.436242	20.373555
60.074819	1968.683597	20.378573
60.336415	1975.885608	20.383591
60.513050	1987.160471	20.388608
60.684909	1985.269620	20.393626
60.844178	1975.672706	20.398643
61.324442	1973.562125	20.403661
60.941760	1965.117768	20.408679
61.185005	1967.925975	20.413696
61.195083	1964.078365	20.418714
60.947476	1968.405610	20.423731
61.035851	1982.058205	20.428749
61.057700	1980.459714	20.433767
61.658342	1986.929054	20.438784
61.438612	2006.403389	20.443802
61.332788	1996.758946	20.448819
61.668238	1998.547674	20.453837
61.420125	1998.221423	20.458855
61.797003	1987.293008	20.463872
61.755239	1995.680680	20.468890
61.564692	1997.080528	20.473907
62.083742	1986.259798	20.478925
61.807972	1999.462046	20.483943
61.844564	1992.742948	20.488960
61.714731	1981.856447	20.493978
61.953620	1978.194309	20.498995
62.154825	1986.358001	20.504013
61.916152	1982.885290	20.509031
62.176074	1998.047757	20.514048
62.055211	1996.842464	20.519066
62.136353	2022.411660	20.524083
62.534526	2034.695137	20.529101
62.251315	2032.709924	20.534119
62.472792	2018.128592	20.539136
62.711842	2022.514089	20.544154
63.008236	2023.862897	20.549171
62.957720	2036.264311	20.554189
62.464003	2037.280677	20.559207
62.600463	2033.551609	20.564224
62.568974	2036.891263	20.569242
62.856856	2022.444007	20.574259
62.892581	2033.297781	20.579277
62.918166	2038.474426	20.584295
63.144761	2056.948563	20.589312
63.173445	2054.240173	20.594330
62.983539	2049.248239	20.599347
63.256987	2051.251021	20.604365
63.200013	2060.047075	20.609383
63.589988	2049.686430	20.614400
63.211840	2048.393161	20.619418
62.996556	2038.492714	20.624435
63.424758	2070.000717	20.629453
63.476242	2092.684593	20.634471
63.550629	2077.161145	20.639488
63.902211	2096.277354	20.644506
63.767322	2082.208512	20.649523
63.775094	2072.290766	20.654541
63.682691	2069.408618	20.659559
63.880223	2071.663375	20.664576
63.841594	2076.894633	20.669594
63.879469	2091.186564	20.674611
64.467177	2093.355395	20.679629
64.526797	2102.756507	20.684647
64.498011	2083.508725	20.689664
64.841045	2092.306205	20.694682
64.497115	2083.160127	20.699699
64.901509	2073.273870	20.704717
64.967184	2082.427949	20.709735
65.107194	2080.975837	20.714752
65.089754	2061.433641	20.719770
64.698529	2061.776790	20.724787
65.285539	2060.225130	20.729805
64.735032	2069.165233	20.734823
64.885081	2071.312305	20.739840
64.776837	2072.983647	20.744858
64.911310	2068.761875	20.749875
65.348841	2074.027322	20.754893
65.177650	2073.193662	20.759911
65.163023	2073.940147	20.764928
65.143100	2070.594624	20.769946
65.234571	2077.646087	20.774963
65.369203	2091.357956	20.779981
65.284870	2114.824215	20.784999
65.373920	2109.923148	20.790016
65.613334	2115.994638	20.795034
65.809876	2116.882971	20.800051
66.152363	2115.037617	20.805069
65.892326	2109.174038	20.810087
65.988379	2115.023296	20.815104
66.110503	2118.036848	20.820122
65.991580	2097.309419	20.825139
65.943525	2121.285155	20.830157
65.779819	2130.152617	20.835175
66.438660	2131.039938	20.840192
66.918609	2133.574554	20.845210
66.540560	2129.569129	20.850227
66.801740	2134.228512	20.855245
66.913516	2133.472182	20.860263
66.937279	2128.656885	20.865280
67.148530	2129.260159	20.870298
67.018663	2125.114233	20.875315
66.873612	2125.482145	20.880333
67.005572	2126.026782	20.885351
66.855473	2123.521123	20.890368
66.929426	2113.439192	20.895386
66.755026	2125.436322	20.900403
67.122818	2137.220954	20.905421
66.798210	2128.441769	20.910439
66.733885	2146.141985	20.915456
66.914218	2143.536057	20.920474
67.258341	2165.994845	20.925491
67.274248	2158.097305	20.930509
67.310649	2156.131984	20.935527
67.197918	2164.599771	20.940544
67.891005	2182.474325	20.945562
67.775179	2186.703194	20.950579
68.016355	2168.111955	20.955597
68.306264	2183.126466	20.960615
68.247731	2174.833807	20.965632
68.225393	2192.044247	20.970650
68.069798	2191.169919	20.975667
68.518853	2186.958030	20.980685
68.302848	2175.589160	20.985703
68.325675	2191.321321	20.990720
68.393230	2182.644695	20.995738
68.286228	2182.748785	21.000755
68.585565	2177.422265	21.005773
68.598726	2162.207715	21.010791
68.473574	2173.870914	21.015808
68.656485	2165.448023	21.020826
68.563680	2168.911008	21.025843
68.452535	2178.161871	21.030861
68.338214	2186.805494	21.035879
68.850810	2196.315637	21.040896
69.289257	2190.644329	21.045914
69.145119	2212.261976	21.050931
69.304489	2211.771354	21.055949
69.262169	2194.216529	21.060967
69.178148	2206.686403	21.065984
69.512042	2200.654084	21.071002
68.908399	2204.636261	21.076019
69.053536	2196.058599	21.081037
69.423088	2211.877753	21.086055
69.283977	2231.618335	21.091072
69.952284	2230.301215	21.096090
69.454901	2231.738896	21.101107
69.713603	2232.187016	21.106125
69.783090	2231.105637	21.111143
69.818827	2238.755558	21.116160
70.153290	2217.833873	21.121178
70.052137	2235.218382	21.126195
70.227390	2257.212180	21.131213
70.075397	2259.485162	21.136231
70.202250	2258.526170	21.141248
70.833002	2258.319601	21.146266
70.764294	2266.717580	21.151283
70.624901	2269.029223	21.156301
70.609925	2242.564391	21.161319
70.515718	2245.597971	21.166336
70.635526	2259.139928	21.171354
70.840841	2264.280946	21.176371
70.705622	2240.818570	21.181389
70.557490	2272.632134	21.186407
70.976911	2275.069904	21.191424
71.008155	2273.268189	21.196442
71.049246	2284.602475	21.201459
71.060183	2276.903104	21.206477
71.270826	2276.522689	21.211495
71.200704	2275.266378	21.216512
71.232635	2283.900255	21.221530
71.466021	2294.335393	21.226547
71.554365	2318.566707	21.231565
71.789180	2312.808157	21.236583
72.010466	2319.897227	21.241600
72.311718	2321.881182	21.246618
72.051460	2309.004609	21.251635
72.134372	2316.278329	21.256653
72.665598	2296.622239	21.261671
72.629706	2284.311664	21.266688
72.669475	2299.883486	21.271706
72.340750	2277.238927	21.276723
72.340912	2285.865852	21.281741
72.532894	2278.371171	21.286759
72.505324	2299.044041	21.291776
72.828585	2282.350210	21.296794
72.397753	2308.559710	21.301811
72.666289	2298.898581	21.306829
72.876206	2300.259146	21.311847
72.936825	2290.615847	21.316864
72.952892	2280.882295	21.321882
72.931525	2290.881652	21.326899
73.012604	2281.165698	21.331917
73.079738	2296.404505	21.336935
73.028088	2285.332554	21.341952
73.057195	2276.246350	21.346970
73.099207	2285.230670	21.351987
73.453400	2284.480526	21.357005
73.611378	2323.408200	21.362023
73.348580	2300.348841	21.367040
73.591087	2318.330093	21.372058
73.752506	2308.682722	21.377075
73.626356	2309.099573	21.382093
73.650644	2318.156318	21.387111
73.572128	2299.644517	21.392128
73.809755	2311.630685	21.397146
73.722763	2307.237308	21.402163
74.022549	2334.403703	21.407181
74.306875	2331.748281	21.412199
74.176495	2345.269462	21.417216
74.087571	2331.050397	21.422234
74.273200	2337.329158	21.427251
74.117934	2336.585061	21.432269
74.250720	2338.437827	21.437287
74.276495	2369.153535	21.442304
74.680290	2353.195414	21.447322
74.885322	2368.655758	21.452339
74.558815	2358.906532	21.457357
74.979670	2365.563693	21.462375
74.915771	2355.194787	21.467392
75.107323	2351.544812	21.472410
74.716802	2353.017002	21.477427
75.055919	2381.491930	21.482445
75.636319	2374.066659	21.487463
75.661503	2390.375514	21.492480
75.431883	2382.083853	21.497498
75.570009	2396.253711	21.502515
75.507317	2394.257498	21.507533
75.545660	2383.295192	21.512551
75.470163	2391.135787	21.517568
75.648947	2385.151073	21.522586
75.774459	2400.577549	21.527603
76.131736	2394.207879	21.532621
76.187664	2407.614876	21.537639
76.164994	2394.400592	21.542656
76.544419	2418.880178	21.547674
76.562377	2408.194410	21.552691
76.286778	2408.029950	21.557709
76.935535	2397.158272	21.562727
76.658901	2417.372929	21.567744
76.630519	2401.015381	21.572762
76.676178	2413.722024	21.577779
76.650390	2420.216436	21.582797
76.920760	2400.452753	21.587815
76.867444	2407.206984	21.592832
76.943981	2405.331638	21.597850
77.007892	2385.920151	21.602867
76.601707	2406.654745	21.607885
77.162029	2415.949692	21.612903
76.987051	2434.547425	21.617920
77.147584	2440.274752	21.622938
77.402760	2434.924344	21.627955
76.914233	2453.201922	21.632973
77.398203	2434.065987	21.637991
77.327106	2453.731452	21.643008
77.474345	2463.022454	21.648026
77.706913	2453.986370	21.653043
77.612875	2466.961380	21.658061
77.715570	2450.641559	21.663079
77.460799	2462.917448	21.668096
78.020420	2479.337266	21.673114
78.163636	2488.986179	21.678131
78.135268	2497.476423	21.683149
78.548772	2477.661039	21.688167
78.653887	2491.154653	21.693184
78.567052	2484.288339	21.698202
78.592850	2482.449120	21.703219
78.454803	2484.305325	21.708237
78.882012	2465.408225	21.713255
78.656112	2476.981231	21.718272
78.942924	2467.382912	21.723290
79.139211	2475.058971	21.728307
79.019619	2488.170288	21.733325
79.161199	2504.444875	21.738343
78.982662	2511.532199	21.743360
79.043736	2508.216301	21.748378
79.349949	2501.428316	21.753395
79.162095	2502.863881	21.758413
79.330864	2510.782659	21.763431
79.204057	2509.318602	21.768448
79.296279	2530.869100	21.773466
79.804107	2537.770194	21.778483
79.799005	2548.313802	21.783501
79.956074	2542.076550	21.788519
80.061764	2528.873809	21.793536
80.153134	2531.309342	21.798554
80.259906	2530.177497	21.803571
80.097020	2551.811118	21.808589
80.181003	2533.235968	21.813607
80.452517	2557.979832	21.818624
80.642401	2551.127596	21.823642
80.915643	2568.153412	21.828659
80.857443	2559.667211	21.833677
81.009321	2560.340051	21.838695
81.248971	2566.088401	21.843712
81.276070	2549.525493	21.848730
81.190428	2528.412805	21.853747
80.964606	2531.254835	21.858765
81.092743	2514.014341	21.863783
81.178700	2548.884614	21.868800
81.537426	2552.771424	21.873818
81.341523	2564.166139	21.878835
81.196609	2552.829132	21.883853
81.655376	2553.723070	21.888871
81.404836	2556.072410	21.893888
81.285592	2546.335462	21.898906
81.273953	2563.595527	21.903923
81.321697	2571.868933	21.908941
81.780084	2587.687771	21.913959
81.506503	2593.062148	21.918976
81.715688	2596.823702	21.923994
82.114962	2604.640275	21.929011
81.721014	2610.323877	21.934029
82.364962	2624.943357	21.939047
82.819867	2605.228632	21.944064
82.567095	2612.233007	21.949082
83.018310	2601.618011	21.954099
82.743964	2595.712422	21.959117
82.849569	2600.814921	21.964135
82.558437	2604.720166	21.969152
83.031315	2595.080394	21.974170
83.393138	2591.730526	21.979187
82.781163	2616.870441	21.984205
82.892503	2595.747745	21.989223
83.008528	2616.310318	21.994240
82.874421	2625.264499	21.999258
83.264845	2617.796893	22.004275
83.294731	2627.302832	22.009293
83.602827	2633.295768	22.014311
83.539918	2632.262417	22.019328
83.654018	2641.711738	22.024346
83.515790	2627.575338	22.029363
83.570355	2660.589501	22.034381
83.807214	2655.903960	22.039399
84.196451	2659.805242	22.044416
84.295878	2677.776705	22.049434
84.378819	2648.985072	22.054451
84.340810	2654.863381	22.059469
84.461933	2650.166656	22.064487
84.462947	2652.081190	22.069504
84.225766	2656.822496	22.074522
84.539691	2642.188590	22.079539
84.366990	2665.615280	22.084557
84.635593	2672.779558	22.089575
84.811478	2688.738870	22.094592
84.820320	2681.662590	22.099610
85.102253	2687.444545	22.104627
84.649177	2688.961546	22.109645
84.921591	2713.946818	22.114663
85.393313	2695.546542	22.119680
85.366173	2716.843439	22.124698
85.606723	2695.090479	22.129715
85.369800	2691.465761	22.134733
85.571976	2694.375070	22.139751
85.672313	2681.315780	22.144768
85.276944	2699.025377	22.149786
85.867458	2716.186700	22.154803
86.168033	2733.582346	22.159821
85.959558	2738.191390	22.164839
86.248058	2730.518162	22.169856
86.101654	2737.055077	22.174874
86.290326	2726.627257	22.179891
86.126963	2731.438660	22.184909
86.036265	2725.317857	22.189927
86.602473	2750.613648	22.194944
86.466807	2747.576633	22.199962
86.967217	2759.691752	22.204979
87.036439	2758.064980	22.209997
87.079781	2749.096799	22.215015
87.255255	2741.448343	22.220032
87.041127	2747.286705	22.225050
87.229832	2736.491206	22.230067
87.105716	2747.839946	22.235085
87.293425	2742.061662	22.240103
87.436608	2753.366630	22.245120
87.446553	2780.651778	22.250138
87.445687	2779.356229	22.255155
87.666885	2780.551610	22.260173
87.565745	2790.250341	22.265191
87.741541	2787.217553	22.270208
87.687797	2784.412040	22.275226
87.951371	2796.016002	22.280243
87.996960	2800.542536	22.285261
88.096192	2805.102722	22.290279
88.512906	2798.635675	22.295296
88.377749	2820.971300	22.300314
88.448645	2790.662689	22.305331
88.519101	2795.457715	22.310349
88.854584	2806.524870	22.315367
88.854566	2792.465467	22.320384
88.731556	2812.978443	22.325402
89.367216	2818.195959	22.330419
89.042019	2831.926507	22.335437
89.367325	2826.207925	22.340455
89.379229	2837.451784	22.345472
88.995453	2826.103659	22.350490
89.234784	2835.541066	22.355507
89.345542	2833.478934	22.360525
89.175472	2825.490342	22.365543
89.406888	2817.265157	22.370560
89.288133	2824.316568	22.375578
89.734645	2823.085064	22.380595
89.990559	2835.777782	22.385613
89.887300	2861.757341	22.390631
89.744915	2844.344672	22.395648
89.982369	2857.265233	22.400666
90.062669	2843.638519	22.405683
90.090485	2853.731874	22.410701
89.989237	2854.024560	22.415719
90.498302	2878.233094	22.420736
90.434051	2885.925447	22.425754
90.582157	2863.628145	22.430771
90.743133	2875.720519	22.435789
90.795807	2850.063047	22.440807
91.163819	2877.218538	22.445824
91.267348	2893.446680	22.450842
91.773155	2879.230591	22.455859
91.418472	2882.146334	22.460877
91.433807	2860.130394	22.465895
91.772104	2882.885843	22.470912
91.312486	2889.186622	22.475930
91.805867	2879.766683	22.480947
91.890771	2878.935634	22.485965
91.636433	2892.118373	22.490983
92.004477	2888.617039	22.496000
91.835921	2887.896368	22.501018
91.898244	2889.072150	22.506035
92.012975	2892.153800	22.511053
92.020844	2912.381534	22.516071
92.288330	2905.313981	22.521088
92.298617	2918.689010	22.526106
92.393287	2920.917982	22.531123
92.292253	2925.986436	22.536141
92.506521	2938.647740	22.541159
92.287306	2925.078910	22.546176
92.609139	2945.997237	22.551194
92.797722	2949.108030	22.556211
92.735478	2945.467378	22.561229
92.706683	2943.760338	22.566247
93.341776	2973.455612	22.571264
93.071941	2979.503833	22.576282
93.316364	2972.624488	22.581299
93.349987	2982.847858	22.586317
93.748232	2978.874048	22.591335
93.931316	2976.924537	22.596352
93.935143	2975.534703	22.601370
94.365816	2975.361587	22.606387
94.044782	2984.683045	22.611405
94.370062	2995.601450	22.616423
94.395779	3006.324116	22.621440
94.389314	2992.785417	22.626458
94.863304	3003.832387	22.631475
94.912317	3005.724861	22.636493
94.843624	2982.198595	22.641511
95.082855	2981.277086	22.646528
94.974894	2958.255712	22.651546
94.882871	2969.441063	22.656563
95.080228	2970.740386	22.661581
95.118969	2994.892981	22.666599
95.413392	2989.430397	22.671616
95.404201	2981.934370	22.676634
95.085166	2993.646170	22.681651
95.325784	2979.781451	22.686669
95.142913	2971.408132	22.691687
95.351545	2982.092093	22.696704
95.246562	2979.110781	22.701722
95.720961	2986.034137	22.706739
95.719119	3023.525595	22.711757
95.447170	3020.016811	22.716775
95.916136	3016.676508	22.721792
95.741141	3034.952760	22.726810
95.947535	3019.373384	22.731827
96.088651	3039.242099	22.736845
96.151314	3039.906674	22.741863
96.118269	3054.203641	22.746880
96.543166	3042.064322	22.751898
96.621665	3050.622044	22.756915
96.745199	3067.156281	22.761933
96.469760	3072.439605	22.766951
97.126589	3087.400670	22.771968
97.178871	3069.354267	22.776986
97.305880	3063.724264	22.782003
97.540481	3078.751744	22.787021
97.454437	3077.047457	22.792039
97.568952	3068.026586	22.797056
97.632205	3075.770201	22.802074
97.627885	3071.097422	22.807091
97.859259	3076.347586	22.812109
97.636666	3093.395295	22.817127
97.911387	3076.654106	22.822144
97.917612	3089.807144	22.827162
98.249463	3080.895219	22.832179
98.431012	3083.830843	22.837197
98.513401	3090.960740	22.842215
98.903363	3082.971588	22.847232
98.845778	3100.648660	22.852250
98.414003	3101.724431	22.857267
98.675657	3120.408697	22.862285
98.847183	3123.861677	22.867303
98.967866	3124.948905	22.872320
99.042710	3130.436544	22.877338
98.686024	3123.608630	22.882355
99.266223	3130.323645	22.887373
99.040190	3149.711104	22.892391
99.447458	3139.419505	22.897408
99.243942	3158.493445	22.902426
99.406565	3137.808336	22.907443
99.345256	3156.344263	22.912461
99.405660	3165.216226	22.917479
99.602406	3177.973329	22.922496
99.529908	3179.021624	22.927514
99.814260	3185.960138	22.932531
100.542418	3203.838164	22.937549
100.444441	3185.453500	22.942567
100.612898	3198.663279	22.947584
101.028938	3194.538065	22.952602
100.845194	3185.244397	22.957619
101.059471	3198.866641	22.962637
101.041193	3203.863249	22.967655
101.498384	3199.573376	22.972672
101.324850	3214.990051	22.977690
100.963644	3192.044029	22.982707
101.453184	3193.269700	22.987725
101.141611	3201.311117	22.992743
101.401679	3194.661741	22.997760
101.459648	3210.413151	23.002778
101.303094	3214.452397	23.007795
102.045306	3220.613175	23.012813
101.449851	3232.422794	23.017831
101.854917	3226.113778	23.022848
101.692506	3229.140909	23.027866
101.730838	3243.712448	23.032883
102.196694	3233.312297	23.037901
102.007409	3250.909147	23.042919
102.005702	3247.698731	23.047936
102.225095	3235.714269	23.052954
102.681429	3265.891965	23.057971
102.741955	3280.320515	23.062989
102.547741	3298.368584	23.068007
102.989756	3287.102341	23.073024
103.112637	3284.864147	23.078042
102.889244	3287.488610	23.083059
103.045446	3277.494878	23.088077
103.308885	3302.095422	23.093095
103.400500	3301.948215	23.098112
103.437275	3306.442106	23.103130
103.706141	3306.558692	23.108147
103.694293	3303.725494	23.113165
103.837823	3310.381852	23.118183
103.987897	3281.292540	23.123200
104.314973	3302.911797	23.128218
104.196460	3317.553217	23.133235
104.757064	3324.647701	23.138253
104.472151	3317.477951	23.143271
104.582567	3323.603814	23.148288
104.835152	3319.051289	23.153306
104.621946	3338.446510	23.158323
104.953611	3324.734729	23.163341
104.735261	3329.600871	23.168359
104.737348	3325.745187	23.173376
105.144694	3340.866808	23.178394
104.666869	3347.592197	23.183411
105.257929	3350.956615	23.188429
104.924794	3355.621870	23.193447
104.984922	3364.915412	23.198464
105.309746	3370.497250	23.203482
105.365479	3382.304487	23.208499
105.739095	3380.609637	23.213517
105.909643	3391.615303	23.218535
106.258578	3404.995223	23.223552
106.429424	3409.173118	23.228570
106.355810	3400.109328	23.233587
106.835351	3395.142344	23.238605
106.713492	3395.398489	23.243623
106.802426	3404.416256	23.248640
107.101759	3386.122576	23.253658
107.007000	3398.892404	23.258675
107.060694	3388.595882	23.263693
106.862857	3411.488535	23.268711
107.118955	3388.863210	23.273728
107.496026	3395.334373	23.278746
107.254481	3412.378479	23.283763
107.612281	3415.201586	23.288781
107.756405	3426.702742	23.293799
108.061185	3412.275902	23.298816
107.933088	3421.981255	23.303834
107.675736	3424.068488	23.308851
108.145987	3417.557499	23.313869
108.016853	3423.731252	23.318887
108.172733	3419.654086	23.323904
108.153032	3423.298167	23.328922
108.248297	3446.642396	23.333939
108.470596	3431.860301	23.338957
108.523078	3443.492547	23.343975
108.313798	3446.407790	23.348992
108.793193	3447.730624	23.354010
108.970086	3451.041859	23.359027
109.451812	3476.579559	23.364045
109.504842	3467.928033	23.369063
109.540012	3460.506130	23.374080
109.374671	3446.913962	23.379098
109.181384	3472.157324	23.384115
109.307723	3461.496220	23.389133
109.407787	3484.586979	23.394151
109.546508	3488.331856	23.399168
109.348819	3477.510325	23.404186
109.534626	3507.497587	23.409203
109.648567	3485.325890	23.414221
109.475560	3510.136471	23.419239
109.527001	3535.146600	23.424256
110.041472	3522.234095	23.429274
109.729178	3564.192568	23.434291
110.215833	3554.520007	23.439309
110.167400	3579.055016	23.444327
110.597631	3594.284907	23.449344
111.302047	3593.036712	23.454362
110.656962	3600.586046	23.459379
111.414430	3579.231233	23.464397
111.594822	3579.795085	23.469415
111.336927	3596.728915	23.474432
111.833754	3590.787041	23.479450
111.947693	3607.527167	23.484467
112.228002	3607.546597	23.489485
112.209730	3616.997329	23.494503
112.130728	3607.164091	23.499520
112.552583	3618.827159	23.504538
112.360718	3617.354061	23.509555
112.644466	3601.321587	23.514573
112.641289	3614.690390	23.519591
112.644648	3598.700707	23.524608
112.910060	3603.115569	23.529626
112.910607	3606.377440	23.534643
112.427296	3596.824582	23.539661
112.709850	3611.622235	23.544679
112.833649	3631.603229	23.549696
113.119820	3631.671490	23.554714
113.084281	3646.875255	23.559731
113.020158	3642.241908	23.564749
113.397345	3661.313812	23.569767
113.408491	3669.244077	23.574784
114.037063	3650.261674	23.579802
113.802581	3664.883218	23.584819
113.789782	3670.824081	23.589837
113.946591	3687.989267	23.594855
114.126284	3689.298855	23.599872
114.719792	3708.139613	23.604890
114.474876	3689.135367	23.609907
114.555446	3708.601593	23.614925
114.972182	3694.863028	23.619943
114.615548	3716.288776	23.624960
115.424229	3709.210559	23.629978
115.252137	3705.201488	23.634995
115.273219	3722.314538	23.640013
115.513362	3704.110180	23.645031
115.306639	3706.008190	23.650048
115.424151	3688.955727	23.655066
115.454410	3715.765780	23.660083
115.529607	3731.572941	23.665101
115.840992	3746.067751	23.670119
116.027102	3739.888404	23.675136
116.101697	3742.258206	23.680154
116.429676	3746.600373	23.685171
116.285537	3724.472554	23.690189
116.569346	3726.217469	23.695207
116.305970	3756.227668	23.700224
116.818430	3755.962692	23.705242
116.765759	3772.884258	23.710259
116.626356	3775.790771	23.715277
116.968866	3761.306982	23.720295
116.731697	3772.978087	23.725312
116.976608	3773.702337	23.730330
117.214567	3778.901657	23.735347
117.314994	3796.029235	23.740365
117.718123	3792.392975	23.745383
117.716473	3800.258300	23.750400
117.773338	3785.162282	23.755418
118.058765	3782.226138	23.760435
117.682471	3809.191124	23.765453
118.170599	3824.750238	23.770471
118.054535	3828.969358	23.775488
118.111398	3817.384115	23.780506
118.310457	3833.367357	23.785523
118.424454	3842.054881	23.790541
118.443246	3848.924788	23.795559
118.220129	3851.739249	23.800576
119.152110	3878.244884	23.805594
119.096257	3879.257800	23.810611
118.953377	3873.077253	23.815629
119.288754	3873.556259	23.820647
119.404178	3868.599886	23.825664
119.532608	3871.048012	23.830682
119.677778	3875.877877	23.835699
119.701282	3914.199542	23.840717
120.092311	3903.710527	23.845735
119.944778	3904.898427	23.850752
120.314098	3909.123973	23.855770
120.380970	3914.586832	23.860787
120.338929	3899.454292	23.865805
120.524136	3924.311064	23.870823
120.576850	3921.245641	23.875840
121.140365	3916.358904	23.880858
121.067978	3926.793712	23.885875
120.938499	3925.503178	23.890893
121.048104	3919.797398	23.895911
121.266048	3943.850412	23.900928
121.650782	3947.369917	23.905946
121.342350	3967.499534	23.910963
121.272811	3966.921101	23.915981
121.766992	3947.811140	23.920999
121.656268	3979.654320	23.926016
121.671247	3983.055413	23.931034
122.124212	3986.846709	23.936051
122.038876	3976.078898	23.941069
122.256283	3989.783800	23.946087
122.111911	4001.488756	23.951104
122.772645	4006.859423	23.956122
123.076574	4007.156631	23.961139
122.837676	4013.141285	23.966157
123.183079	4008.327960	23.971175
123.336943	4014.659506	23.976192
123.596972	3997.595555	23.981210
123.415538	4017.295611	23.986227
123.212277	4021.268968	23.991245
123.729697	4041.905887	23.996263
123.698634	4042.669454	24.001280
124.318294	4041.711400	24.006298
124.151266	4033.203002	24.011315
123.906530	4045.798549	24.016333
124.509993	4023.457206	24.021351
124.333525	4042.806491	24.026368
124.299549	4049.578912	24.031386
124.631653	4062.207102	24.036403
124.591683	4062.911121	24.041421
124.655774	4062.543270	24.046439
124.495995	4055.331239	24.051456
124.743786	4062.552359	24.056474
124.732970	4089.409411	24.061491
124.869054	4071.813916	24.066509
125.137249	4083.204316	24.071527
124.904729	4111.095632	24.076544
125.359630	4115.475985	24.081562
125.446401	4126.351537	24.086579
125.664695	4133.936211	24.091597
126.037769	4137.756493	24.096615
125.854634	4144.560295	24.101632
125.802732	4153.138011	24.106650
126.215717	4150.067734	24.111667
125.739835	4187.566330	24.116685
126.510786	4173.470794	24.121703
126.496330	4195.954791	24.126720
126.829676	4196.343202	24.131738
127.049376	4209.773521	24.136755
127.420824	4210.958362	24.141773
127.836108	4191.973733	24.146791
127.448778	4200.544698	24.151808
127.960747	4214.470014	24.156826
128.133657	4195.619521	24.161843
127.645725	4204.961807	24.166861
128.278905	4208.578898	24.171879
128.369362	4242.099152	24.176896
128.063560	4233.028556	24.181914
128.478452	4237.604131	24.186931
128.119404	4233.300826	24.191949
128.461426	4237.133745	24.196967
128.726799	4244.197720	24.201984
128.794692	4263.267933	24.207002
128.998866	4250.950175	24.212019
128.978571	4263.145438	24.217037
129.018179	4258.731372	24.222055
129.242426	4261.609775	24.227072
129.316405	4285.492233	24.232090
129.668967	4306.689408	24.237107
129.891327	4294.247748	24.242125
129.937841	4272.991352	24.247143
129.858507	4295.223230	24.252160
130.169023	4311.075561	24.257178
130.548939	4309.647282	24.262195
130.236887	4331.091312	24.267213
130.447725	4317.609442	24.272231
130.474808	4323.403419	24.277248
130.824768	4333.874222	24.282266
131.013711	4342.883492	24.287283
130.750580	4357.022836	24.292301
131.406109	4347.047283	24.297319
131.305294	4336.440829	24.302336
131.239075	4340.076278	24.307354
131.574239	4346.494928	24.312371
131.560499	4370.127057	24.317389
132.160555	4355.539137	24.322407
131.945518	4355.652823	24.327424
131.910415	4375.771661	24.332442
132.284757	4385.026297	24.337459
132.313303	4399.926912	24.342477
132.615861	4387.337284	24.347495
132.434554	4393.274774	24.352512
132.384071	4391.884928	24.357530
133.058837	4410.343247	24.362547
132.794520	4415.269683	24.367565
132.782252	4419.608816	24.372583
132.806259	4420.334562	24.377600
132.904286	4442.708994	24.382618
133.510592	4442.740899	24.387635
133.140023	4458.748047	24.392653
133.403824	4432.322963	24.397671
133.501220	4457.408481	24.402688
133.923287	4475.691315	24.407706
134.378129	4465.844909	24.412723
134.022448	4497.886711	24.417741
134.313466	4482.533611	24.422759
134.836222	4502.951372	24.427776
134.788044	4511.464499	24.432794
135.116514	4497.895320	24.437811
135.110522	4508.830956	24.442829
135.234116	4503.633666	24.447847
135.400220	4511.692102	24.452864
135.113565	4510.111747	24.457882
135.446286	4523.114221	24.462899
135.373419	4535.543578	24.467917
135.408371	4542.014671	24.472935
135.645739	4538.740665	24.477952
136.029203	4565.604650	24.482970
136.422790	4566.447285	24.487987
136.290119	4577.309414	24.493005
136.434328	4559.536042	24.498023
136.313902	4572.898077	24.503040
136.496289	4582.599898	24.508058
136.591554	4594.330269	24.513075
136.840813	4598.399864	24.518093
137.043974	4608.362439	24.523111
137.312518	4627.387740	24.528128
137.078918	4628.824165	24.533146
137.472374	4643.264722	24.538163
137.603396	4646.431434	24.543181
138.103631	4640.545491	24.548199
138.138181	4647.307243	24.553216
137.872747	4637.647855	24.558234
138.076295	4653.406795	24.563251
138.126178	4656.393217	24.568269
138.398197	4669.357814	24.573287
138.834623	4685.042481	24.578304
138.697666	4670.021329	24.583322
139.207497	4655.661816	24.588339
139.122378	4694.467133	24.593357
139.688452	4680.533340	24.598375
139.666812	4688.704385	24.603392
139.963189	4695.388644	24.608410
140.288403	4686.130838	24.613427
139.672039	4689.386408	24.618445
139.994908	4695.163539	24.623463
140.442648	4690.521678	24.628480
140.282693	4692.801446	24.633498
140.499922	4689.270107	24.638515
140.628286	4718.953658	24.643533
140.619242	4705.169992	24.648551
140.781885	4716.725938	24.653568
140.902602	4706.483411	24.658586
140.913275	4715.294403	24.663603
141.154004	4739.153943	24.668621
141.291793	4739.567597	24.673639
141.625500	4747.426808	24.678656
141.253612	4759.187644	24.683674
141.635949	4748.706586	24.688691
141.818087	4782.717582	24.693709
142.084912	4776.289842	24.698727
142.466643	4778.052951	24.703744
142.227132	4792.261228	24.708762
142.580543	4769.312892	24.713779
142.443721	4790.445530	24.718797
142.772420	4791.702444	24.723815
143.037203	4805.117563	24.728832
142.734479	4802.346917	24.733850
143.036892	4819.510165	24.738867
142.904253	4826.170880	24.743885
143.007565	4808.490202	24.748903
143.495761	4829.163318	24.753920
143.482680	4815.914081	24.758938
143.614328	4845.569378	24.763955
143.893583	4840.088380	24.768973
143.733215	4870.261268	24.773991
144.375996	4857.828431	24.779008
144.264669	4874.140808	24.784026
144.413656	4905.277220	24.789043
144.750810	4894.209038	24.794061
144.698363	4898.339982	24.799079
145.105771	4884.651518	24.804096
144.842420	4902.440628	24.809114
145.410318	4912.088405	24.814131
145.454683	4924.873902	24.819149
145.046877	4913.531552	24.824167
145.208622	4943.202141	24.829184
145.360357	4947.049357	24.834202
145.892294	4959.352345	24.839219
145.799082	4975.966957	24.844237
146.054950	4972.275625	24.849255
146.449610	4973.442127	24.854272
146.437100	4979.103519	24.859290
146.638573	4995.150949	24.864307
146.888897	5011.504107	24.869325
146.940617	5007.565000	24.874343
147.068816	5034.636546	24.879360
147.355654	5042.554834	24.884378
147.509967	5016.822845	24.889395
147.350210	5021.185335	24.894413
147.851962	5051.322005	24.899431
148.386016	5055.485610	24.904448
148.173453	5069.041643	24.909466
148.298964	5078.815773	24.914483
148.306533	5066.494029	24.919501
148.505221	5082.618783	24.924519
148.759331	5081.597058	24.929536
148.899574	5091.538450	24.934554
149.007691	5085.084444	24.939571
149.012689	5092.926491	24.944589
149.295796	5092.628335	24.949607
149.434039	5111.821040	24.954624
149.504346	5117.838491	24.959642
150.045105	5124.449877	24.964659
150.044289	5107.448285	24.969677
150.028554	5119.429288	24.974695
150.393057	5124.993791	24.979712
150.440216	5138.493190	24.984730
150.720400	5155.227402	24.989747
150.627521	5146.772677	24.994765
150.436969	5159.830258	24.999783
150.730520	5153.758586	25.004800
150.879772	5159.782301	25.009818
151.056485	5173.800888	25.014835
151.292347	5160.719283	25.019853
151.464875	5189.850753	25.024871
151.777056	5178.841615	25.029888
151.709506	5203.461093	25.034906
152.324881	5200.540248	25.039923
152.253374	5211.376964	25.044941
151.921366	5235.884674	25.049959
152.348342	5225.269933	25.054976
152.574829	5248.246757	25.059994
152.540505	5229.061922	25.065011
152.668502	5236.670719	25.070029
152.515490	5251.220249	25.075047
153.159196	5237.914492	25.080064
152.855682	5254.494857	25.085082
152.962857	5264.783566	25.090099
153.446783	5287.187185	25.095117
153.323526	5293.335903	25.100135
153.673088	5306.079158	25.105152
153.726141	5319.899798	25.110170
154.029819	5328.797767	25.115187
154.523201	5331.455124	25.120205
154.563921	5335.573545	25.125223
154.802471	5342.031804	25.130240
154.754134	5334.349172	25.135258
154.955994	5328.773702	25.140275
154.928423	5351.192242	25.145293
154.992160	5353.769408	25.150311
155.499990	5370.906411	25.155328
155.636053	5371.878263	25.160346
155.698508	5368.105801	25.165363
155.770115	5394.965663	25.170381
155.964611	5411.873371	25.175399
156.040286	5404.497785	25.180416
156.175537	5414.357922	25.185434
156.348964	5422.038441	25.190451
157.010247	5426.304358	25.195469
156.782239	5442.033041	25.200487
157.073719	5423.805985	25.205504
157.114317	5459.211195	25.210522
157.360794	5442.819979	25.215539
157.352308	5455.141395	25.220557
157.430691	5468.546153	25.225575
157.975706	5473.693538	25.230592
157.950096	5494.416217	25.235610
157.779418	5487.557303	25.240627
158.145076	5490.122402	25.245645
158.093283	5516.542606	25.250663
158.416756	5520.980121	25.255680
158.523291	5521.238718	25.260698
158.847060	5548.197343	25.265715
159.149541	5538.985705	25.270733
158.923677	5553.535743	25.275751
159.328052	5570.172711	25.280768
159.378776	5584.335720	25.285786
159.483807	5591.021273	25.290803
159.659730	5586.791799	25.295821
159.778036	5616.907092	25.300839
160.486121	5591.272822	25.305856
160.544759	5603.812017	25.310874
160.404261	5612.629990	25.315891
160.832805	5627.745231	25.320909
160.593555	5640.082875	25.325927
160.886471	5629.738057	25.330944
160.971368	5664.537168	25.335962
161.531949	5655.369042	25.340979
161.637949	5669.520239	25.345997
161.563167	5672.393983	25.351015
161.720478	5687.913567	25.356032
161.876095	5694.037625	25.361050
162.194963	5702.911644	25.366067
162.578159	5698.219126	25.371085
162.496851	5704.918587	25.376103
162.394409	5713.175572	25.381120
162.639129	5712.694761	25.386138
162.514242	5730.555641	25.391155
162.741527	5715.499674	25.396173
163.009171	5756.848714	25.401191
163.344892	5755.024832	25.406208
163.101444	5762.394455	25.411226
163.612698	5787.938965	25.416243
163.778175	5785.028177	25.421261
164.169242	5784.046775	25.426279
164.435737	5788.061471	25.431296
164.403931	5788.822489	25.436314
164.463439	5808.979517	25.441331
164.947880	5800.826315	25.446349
164.732813	5810.171321	25.451367
164.689445	5806.119369	25.456384
165.100007	5798.572114	25.461402
165.483568	5834.487685	25.466419
165.413312	5823.163702	25.471437
165.403980	5849.049466	25.476455
165.763814	5861.740295	25.481472
166.003133	5866.739097	25.486490
165.481320	5888.330955	25.491507
166.431564	5878.321488	25.496525
166.390809	5902.052539	25.501543
166.544960	5895.251199	25.506560
166.663235	5897.348150	25.511578
167.051410	5923.727845	25.516595
167.119238	5936.543762	25.521613
166.869696	5935.910737	25.526631
167.477524	5953.123205	25.531648
167.495050	5972.769233	25.536666
167.487130	5965.411527	25.541683
167.735614	5978.380712	25.546701
167.989299	6017.605423	25.551719
168.389027	5993.625904	25.556736
168.704081	6017.069974	25.561754
168.617688	6020.783955	25.566771
168.651763	6022.532603	25.571789
168.335643	6038.712698	25.576807
168.452493	6058.442430	25.581824
168.794260	6067.732199	25.586842
168.677833	6086.166543	25.591859
169.812984	6102.599863	25.596877
169.976728	6105.833127	25.601895
170.221134	6117.650249	25.606912
170.449847	6109.697423	25.611930
170.324858	6119.728576	25.616947
170.400496	6115.291101	25.621965
170.721773	6144.306855	25.626983
170.945255	6134.072400	25.632000
171.144185	6141.739217	25.637018
171.066235	6176.203351	25.642035
171.416954	6169.704483	25.647053
171.700960	6180.384301	25.652071
171.814606	6171.955136	25.657088
172.118805	6199.415803	25.662106
172.127570	6205.218625	25.667123
172.377477	6188.767395	25.672141
172.561619	6203.049878	25.677159
172.757047	6196.085668	25.682176
172.715107	6210.285424	25.687194
172.885985	6216.591040	25.692212
173.019711	6224.634453	25.697229
173.597768	6233.233251	25.702247
173.434016	6254.297508	25.707264
173.932790	6254.774800	25.712282
173.627030	6258.432949	25.717300
174.048296	6268.676329	25.722317
174.049335	6279.964835	25.727335
174.377748	6300.254460	25.732352
174.711251	6272.634711	25.737370
174.452628	6280.001178	25.742388
174.740066	6300.004632	25.747405
175.242296	6297.485002	25.752423
175.134718	6316.063443	25.757440
175.346125	6303.875564	25.762458
175.203950	6320.639472	25.767476
175.804373	6339.387995	25.772493
175.763198	6343.175298	25.777511
175.859463	6343.537191	25.782528
176.076354	6368.662347	25.787546
176.004903	6377.965062	25.792564
176.157925	6373.207216	25.797581
176.179649	6403.721913	25.802599
176.303600	6416.531707	25.807616
176.757732	6411.442966	25.812634
176.828111	6436.989725	25.817652
176.835071	6446.964636	25.822669
177.123763	6459.810637	25.827687
177.365237	6473.853949	25.832704
177.795320	6493.243072	25.837722
177.829904	6496.617063	25.842740
178.180876	6510.813594	25.847757
178.451133	6534.207175	25.852775
178.511683	6551.358747	25.857792
178.777788	6529.040832	25.862810
179.112504	6550.641698	25.867828
179.207186	6557.553417	25.872845
179.325566	6554.399847	25.877863
179.645428	6579.207112	25.882880
179.796539	6577.190387	25.887898
180.301928	6588.091415	25.892916
180.438455	6586.637399	25.897933
180.672000	6609.031530	25.902951
180.791859	6608.106311	25.907968
180.893948	6626.448485	25.912986
180.800718	6620.731136	25.918004
180.994939	6624.701685	25.923021
181.185484	6641.102264	25.928039
181.214370	6635.404500	25.933056
181.410292	6651.156880	25.938074
181.689578	6650.669545	25.943092
181.964641	6666.311608	25.948109
181.779215	6664.850143	25.953127
182.118530	6710.439982	25.958144
182.694689	6685.431314	25.963162
182.768771	6709.680506	25.968180
182.981369	6712.292363	25.973197
183.524542	6722.589925	25.978215
183.501922	6743.406296	25.983232
184.011568	6721.075430	25.988250
183.942115	6734.045408	25.993268
184.309674	6727.755759	25.998285
184.454469	6721.754919	26.003303
184.552817	6716.894573	26.008320
184.790250	6720.645383	26.013338
184.957325	6744.856033	26.018356
184.821516	6756.271049	26.023373
184.945414	6742.210437	26.028391
184.626835	6768.290960	26.033408
185.274153	6751.612827	26.038426
185.144915	6778.753165	26.043444
185.539889	6779.106664	26.048461
185.930115	6794.310483	26.053479
186.060098	6818.251355	26.058496
185.848477	6806.222758	26.063514
186.004403	6843.339828	26.068532
186.412812	6844.396713	26.073549
186.747381	6856.194772	26.078567
186.372772	6864.589077	26.083584
186.916139	6872.856911	26.088602
186.849117	6898.413344	26.093620
187.058640	6904.735298	26.098637
187.448651	6894.109004	26.103655
187.398219	6908.886070	26.108672
187.884493	6922.942494	26.113690
187.937865	6946.029566	26.118708
187.870554	6939.799873	26.123725
188.547324	6965.298884	26.128743
188.399570	6956.839250	26.133760
188.812726	6978.790003	26.138778
189.004904	6999.749200	26.143796
188.927487	7009.628159	26.148813
189.539518	7013.736890	26.153831
189.507027	7025.100773	26.158848
189.720121	7033.833952	26.163866
190.043738	7056.811958	26.168884
190.376298	7048.372535	26.173901
190.285389	7056.040440	26.178919
189.895843	7086.894932	26.183936
190.686084	7077.836484	26.188954
190.836930	7101.920033	26.193972
190.790039	7122.338888	26.198989
191.248247	7126.289967	26.204007
191.572540	7132.135107	26.209024
192.170139	7138.981706	26.214042
192.149818	7159.344243	26.219060
192.159078	7158.178172	26.224077
192.651049	7169.367302	26.229095
192.519239	7183.966310	26.234112
192.767059	7182.205618	26.239130
193.116830	7191.888892	26.244148
192.610997	7216.582769	26.249165
193.353515	7213.644890	26.254183
193.157419	7215.089523	26.259200
193.465438	7242.088719	26.264218
193.539358	7239.790523	26.269236
193.702948	7255.097601	26.274253
194.032781	7290.526103	26.279271
193.845449	7307.725365	26.284288
194.242909	7312.159834	26.289306
194.724948	7333.779966	26.294324
194.896707	7342.295701	26.299341
195.463871	7346.776168	26.304359
195.091987	7366.327626	26.309376
195.814564	7374.476732	26.314394
195.614662	7390.457488	26.319412
195.967820	7399.644973	26.324429
196.638887	7400.971545	26.329447
196.711851	7427.244415	26.334464
196.828370	7447.828063	26.339482
197.109096	7432.435189	26.344500
197.070082	7441.715060	26.349517
197.572564	7447.689959	26.354535
197.444428	7465.969563	26.359552
197.623502	7460.214790	26.364570
197.963113	7456.910294	26.369588
197.822244	7493.683385	26.374605
197.949428	7485.347753	26.379623
198.027248	7503.465790	26.384640
198.425030	7522.583920	26.389658
198.579507	7538.943358	26.394676
199.020349	7568.281426	26.399693
198.920735	7548.609566	26.404711
198.891546	7586.237015	26.409728
199.434323	7583.495882	26.414746
199.845884	7582.698819	26.419764
199.676431	7621.298515	26.424781
199.967957	7637.092006	26.429799
200.008292	7635.428549	26.434816
200.696272	7637.798208	26.439834
200.966279	7653.492102	26.444852
200.744866	7650.685849	26.449869
200.931723	7663.775690	26.454887
201.329913	7674.149817	26.459904
201.304945	7683.365293	26.464922
201.695318	7686.918200	26.469940
202.167349	7712.727111	26.474957
202.100431	7706.052872	26.479975
202.168058	7719.196324	26.484992
202.454878	7738.616570	26.490010
202.837200	7740.651636	26.495028
202.806551	7754.006668	26.500045
203.386932	7764.347601	26.505063
203.390765	7777.148820	26.510080
203.632920	7786.070566	26.515098
203.496410	7799.003673	26.520116
203.812510	7806.130981	26.525133
203.944012	7813.276980	26.530151
204.091378	7838.983807	26.535168
204.119560	7841.375882	26.540186
204.554835	7871.354931	26.545204
204.642266	7885.765579	26.550221
205.190574	7885.999661	26.555239
205.559482	7904.699323	26.560256
205.547177	7917.701786	26.565274
206.109932	7921.417642	26.570292
205.643833	7934.032013	26.575309
206.255223	7940.482121	26.580327
206.411100	7949.148083	26.585344
206.643489	7956.761040	26.590362
207.039954	7981.256626	26.595380
207.083706	8003.934551	26.600397
207.334661	7985.012263	26.605415
207.512023	8025.265443	26.610432
207.860492	8011.121702	26.615450
208.201002	8024.195908	26.620468
208.172964	8044.762481	26.625485
208.457981	8050.337233	26.630503
208.254112	8047.258661	26.635520
208.780747	8068.222697	26.640538
208.868563	8081.416671	26.645556
208.719516	8084.459457	26.650573
209.427468	8114.379740	26.655591
209.461930	8134.381655	26.660608
209.640879	8134.420022	26.665626
210.003186	8150.214148	26.670644
209.575159	8154.905747	26.675661
210.087888	8158.655129	26.680679
210.319032	8186.508199	26.685696
210.548718	8206.839446	26.690714
211.013280	8207.628434	26.695732
211.014622	8240.000861	26.700749
211.532767	8226.136836	26.705767
211.732319	8247.932490	26.710784
211.915001	8265.295332	26.715802
212.194762	8261.932041	26.720820
212.333553	8274.795635	26.725837
213.000873	8292.908539	26.730855
213.229591	8302.427421	26.735872
213.126746	8300.400064	26.740890
213.419409	8308.444277	26.745908
213.677882	8321.543311	26.750925
213.632815	8336.478738	26.755943
213.880518	8325.370948	26.760960
214.113915	8338.970315	26.765978
214.610617	8355.057473	26.770996
214.067022	8353.901538	26.776013
214.554762	8357.400708	26.781031
215.171495	8369.526995	26.786048
215.209859	8380.747048	26.791066
215.189990	8380.799364	26.796084
215.159211	8403.762682	26.801101
215.408122	8402.793198	26.806119
215.836648	8433.312353	26.811136
216.111989	8450.696318	26.816154
216.596665	8435.711394	26.821172
216.373050	8446.420319	26.826189
216.786848	8466.868760	26.831207
217.004461	8474.552930	26.836224
217.041848	8486.137872	26.841242
217.364280	8501.102521	26.846260
217.072475	8511.258056	26.851277
217.439827	8550.226556	26.856295
217.912416	8547.977290	26.861312
218.154574	8570.649239	26.866330
218.287786	8575.540428	26.871348
218.417602	8597.063766	26.876365
218.729198	8613.612586	26.881383
219.010845	8615.706146	26.886400
219.004450	8640.336265	26.891418
219.718031	8637.383226	26.896436
219.946527	8668.473813	26.901453
220.311448	8662.788710	26.906471
220.227994	8669.348413	26.911488
220.445611	8685.330802	26.916506
221.004611	8697.207763	26.921524
220.642498	8706.976515	26.926541
221.100911	8703.720656	26.931559
221.196202	8715.331641	26.936576
221.029401	8752.917662	26.941594
221.623627	8757.377530	26.946612
221.626443	8774.274461	26.951629
221.884059	8797.148959	26.956647
222.388690	8820.725387	26.961664
222.592728	8825.852259	26.966682
222.764557	8862.390210	26.971700
222.620956	8868.492095	26.976717
222.940200	8894.047800	26.981735
223.437864	8902.975222	26.986752
223.456998	8930.889051	26.991770
223.810767	8928.551462	26.996788
223.775143	8945.450990	27.001805
224.146072	8968.333004	27.006823
224.497034	8969.292026	27.011840
224.755098	9015.588766	27.016858
225.291530	9013.334400	27.021876
225.300578	9026.054645	27.026893
225.611569	9041.466700	27.031911
225.989030	9048.554506	27.036928
225.971084	9065.156673	27.041946
226.336989	9087.200091	27.046964
226.641812	9087.707563	27.051981
226.684769	9115.428753	27.056999
227.245069	9122.656510	27.062016
227.148268	9140.178333	27.067034
227.672187	9137.427455	27.072052
227.712184	9163.731504	27.077069
228.242828	9143.133610	27.082087
228.272827	9171.343788	27.087104
228.413953	9182.446616	27.092122
229.195340	9191.864483	27.097140
228.978211	9175.328996	27.102157
229.087351	9199.313949	27.107175
229.315689	9201.942528	27.112192
229.030891	9224.586700	27.117210
229.605524	9223.193169	27.122228
229.580762	9243.740282	27.127245
229.749399	9250.978463	27.132263
229.943172	9280.290444	27.137280
230.116461	9295.161557	27.142298
230.666528	9308.813406	27.147316
230.567332	9326.293298	27.152333
230.865485	9350.161399	27.157351
231.093182	9356.796786	27.162368
231.245296	9395.295698	27.167386
231.448630	9401.826435	27.172404
231.524571	9427.765035	27.177421
231.870127	9461.193652	27.182439
232.062003	9455.406112	27.187456
232.208618	9481.653691	27.192474
232.745877	9501.638849	27.197492
232.867760	9522.277088	27.202509
233.458156	9539.625952	27.207527
233.696090	9549.586718	27.212544
233.787400	9578.092307	27.217562
234.457673	9580.375409	27.222580
234.617563	9600.076478	27.227597
234.771077	9606.461153	27.232615
235.184011	9631.800935	27.237632
235.479715	9635.936248	27.242650
235.733563	9653.544054	27.247668
236.142963	9646.263361	27.252685
236.042826	9661.971578	27.257703
236.711861	9656.888835	27.262720
236.476700	9656.328493	27.267738
236.809165	9674.821250	27.272756
236.838822	9687.276334	27.277773
236.953784	9712.500858	27.282791
237.212000	9719.503912	27.287808
237.227568	9744.209308	27.292826
237.621343	9762.205269	27.297844
237.876866	9767.227061	27.302861
238.135621	9786.181086	27.307879
238.290242	9792.329359	27.312896
238.626404	9822.141816	27.317914
239.259239	9829.316170	27.322932
239.481873	9834.066163	27.327949
239.766438	9847.431531	27.332967
240.124692	9866.913484	27.337984
240.272576	9881.675922	27.343002
240.359350	9887.539282	27.348020
240.818179	9913.735992	27.353037
240.840476	9915.800114	27.358055
241.065938	9940.045800	27.363072
240.862122	9945.921748	27.368090
241.344215	9956.979024	27.373108
241.814123	9977.246078	27.378125
241.564936	10007.820383	27.383143
242.264725	10005.644440	27.388160
242.635407	10028.327175	27.393178
242.749121	10038.854624	27.398196
242.933802	10049.571997	27.403213
243.284828	10051.132067	27.408231
243.493611	10071.770054	27.413248
243.601444	10080.676699	27.418266
243.945293	10089.922434	27.423284
244.139997	10110.190230	27.428301
244.022464	10112.833574	27.433319
244.523314	10146.712155	27.438336
244.888805	10150.776998	27.443354
245.270175	10179.616188	27.448372
245.555670	10177.065214	27.453389
245.682882	10185.814332	27.458407
245.881936	10187.686237	27.463424
245.670358	10218.238978	27.468442
246.093430	10203.046751	27.473460
246.357399	10219.548409	27.478477
246.556980	10243.762602	27.483495
246.756367	10241.938690	27.488512
246.922010	10262.199668	27.493530
247.376093	10302.797305	27.498548
247.691022	10304.646929	27.503565
247.514057	10317.062603	27.508583
247.867065	10344.520464	27.513600
248.129649	10358.657095	27.518618
248.204389	10382.439209	27.523636
248.498677	10396.574573	27.528653
248.551964	10427.488823	27.533671
249.070966	10429.417384	27.538688
249.270884	10483.128302	27.543706
249.956976	10490.105116	27.548724
249.981062	10486.428356	27.553741
250.377001	10509.010720	27.558759
250.942029	10513.984765	27.563776
250.915356	10538.381722	27.568794
251.343782	10553.237855	27.573812
251.836504	10564.037801	27.578829
252.196787	10581.125718	27.583847
252.174223	10579.827595	27.588864
252.385308	10613.433669	27.593882
252.451456	10603.319211	27.598900
252.902678	10633.433985	27.603917
252.762595	10642.466188	27.608935
253.549010	10658.166758	27.613952
253.450725	10677.917333	27.618970
253.532708	10684.188230	27.623988
253.826753	10703.174542	27.629005
254.015679	10721.363765	27.634023
254.174267	10729.662949	27.639040
254.543929	10755.848212	27.644058
254.685511	10793.427492	27.649076
255.346962	10813.355190	27.654093
255.582951	10816.416013	27.659111
255.836836	10836.250386	27.664128
256.093819	10856.338700	27.669146
256.436498	10856.065667	27.674164
257.100351	10871.726834	27.679181
256.788277	10889.188473	27.684199
257.043739	10906.795039	27.689216
257.254855	10915.787489	27.694234
257.353850	10935.544386	27.699252
258.071139	10955.950630	27.704269
258.026380	10969.127163	27.709287
258.593629	10993.756741	27.714304
258.353518	11006.234584	27.719322
258.777152	11029.658327	27.724340
259.049252	11030.361114	27.729357
259.114917	11064.072510	27.734375
259.650654	11061.124795	27.739392
259.793579	11087.737196	27.744410
259.924662	11112.663519	27.749428
260.659843	11122.575417	27.754445
260.490208	11146.209205	27.759463
261.012321	11147.949078	27.764480
261.198246	11176.923195	27.769498
261.269020	11197.788676	27.774516
261.910095	11201.868916	27.779533
261.872340	11229.807994	27.784551
262.164635	11230.562595	27.789568
262.507465	11248.593079	27.794586
262.402222	11257.014112	27.799604
262.922902	11273.862800	27.804621
262.779771	11302.981312	27.809639
263.318869	11312.194714	27.814656
263.366043	11343.443382	27.819674
263.605154	11356.953019	27.824692
264.154095	11377.750763	27.829709
264.112467	11392.405697	27.834727
264.630191	11405.922123	27.839744
264.647807	11425.137720	27.844762
265.019959	11460.834031	27.849780
265.520508	11459.996885	27.854797
265.688139	11494.832196	27.859815
266.057546	11498.461911	27.864832
266.201791	11528.671633	27.869850
266.409348	11547.063531	27.874868
266.871386	11558.937399	27.879885
267.097652	11583.298889	27.884903
267.405012	11594.438169	27.889920
267.669867	11615.875540	27.894938
268.323417	11635.246278	27.899956
268.540869	11644.396429	27.904973
268.520568	11663.925010	27.909991
268.831148	11681.682450	27.915008
269.227268	11711.245127	27.920026
268.931688	11721.397021	27.925044
269.804387	11738.956884	27.930061
270.113664	11754.860262	27.935079
270.142822	11774.944834	27.940096
270.550638	11779.289060	27.945114
270.808140	11801.181639	27.950132
271.386334	11801.155637	27.955149
271.484500	11832.398410	27.960167
271.500382	11837.006706	27.965184
271.830950	11853.535292	27.970202
272.144401	11875.411639	27.975220
272.324754	11891.302580	27.980237
272.654768	11918.568438	27.985255
272.711233	11924.732964	27.990272
273.143276	11969.471063	27.995290
273.319091	11975.479609	28.000308
273.652382	11999.221414	28.005325
273.994368	12006.438514	28.010343
274.303657	12018.665671	28.015360
274.682966	12042.276258	28.020378
274.663287	12067.405436	28.025396
275.253760	12076.250000	28.030413
275.137519	12115.208668	28.035431
275.489757	12123.017316	28.040448
275.869534	12139.378938	28.045466
276.099024	12160.950501	28.050484
276.345651	12182.255359	28.055501
276.481327	12202.000671	28.060519
277.188730	12225.541567	28.065536
277.923858	12240.280069	28.070554
277.892150	12233.836015	28.075572
278.315653	12249.077403	28.080589
278.355971	12272.048732	28.085607
278.384489	12273.633164	28.090624
278.365332	12302.280825	28.095642
278.518734	12317.516485	28.100660
279.149722	12334.107798	28.105677
279.165488	12372.251988	28.110695
279.379210	12388.352973	28.115712
280.215146	12406.630225	28.120730
280.156853	12418.438659	28.125748
280.804750	12427.776536	28.130765
280.804156	12466.287608	28.135783
280.937132	12464.750933	28.140800
281.172739	12490.791815	28.145818
281.245821	12510.250853	28.150836
281.890541	12535.741304	28.155853
281.873988	12554.698416	28.160871
282.017202	12575.478883	28.165888
282.545814	12598.760750	28.170906
282.681408	12620.234214	28.175924
283.064271	12658.124637	28.180941
283.339328	12675.636168	28.185959
283.992454	12676.271355	28.190976
284.266192	12709.352326	28.195994
284.207347	12728.379653	28.201012
284.899081	12743.789115	28.206029
285.247163	12761.439144	28.211047
285.386846	12790.129183	28.216064
285.849515	12794.901855	28.221082
285.749595	12830.353061	28.226100
286.269001	12819.874774	28.231117
286.467277	12857.637028	28.236135
286.840082	12871.992441	28.241152
286.838331	12891.028648	28.246170
287.076303	12912.861371	28.251188
287.356602	12948.301228	28.256205
287.445088	12962.303489	28.261223
288.159605	12992.378423	28.266240
288.476247	13011.223514	28.271258
288.857268	13045.380932	28.276276
288.884277	13049.414211	28.281293
288.981165	13078.142558	28.286311
289.141741	13108.384856	28.291328
289.974495	13117.672904	28.296346
289.903118	13162.708634	28.301364
290.651239	13164.552420	28.306381
290.730118	13200.296330	28.311399
290.757326	13223.662730	28.316416
291.617867	13247.689552	28.321434
291.528095	13275.422556	28.326452
291.876454	13288.204371	28.331469
292.377676	13313.128111	28.336487
292.592706	13331.105637	28.341504
292.938363	13362.512180	28.346522
292.994947	13381.915909	28.351540
293.267213	13401.287969	28.356557
293.678520	13412.880889	28.361575
293.894132	13437.161868	28.366592
294.566538	13446.322185	28.371610
294.714786	13474.819009	28.376628
295.172633	13505.455703	28.381645
295.348966	13505.926260	28.386663
295.846032	13534.131574	28.391680
295.802387	13537.945812	28.396698
296.128538	13569.065269	28.401716
296.601241	13571.772383	28.406733
297.218310	13614.507810	28.411751
296.935960	13617.790320	28.416768
297.846227	13631.014517	28.421786
297.812265	13656.233622	28.426804
297.945171	13659.772914	28.431821
298.462826	13684.729180	28.436839
298.469150	13695.841662	28.441856
299.234637	13731.135329	28.446874
299.422350	13733.526358	28.451892
299.672494	13766.160387	28.456909
299.826773	13782.653119	28.461927
299.458567	13808.259365	28.466944
300.057570	13820.277736	28.471962
300.246344	13843.571859	28.476980
300.666111	13873.023524	28.481997
301.269736	13887.943632	28.487015
301.236279	13915.590434	28.492032
301.895846	13920.303341	28.497050
301.785237	13952.620752	28.502068
302.079217	13953.324002	28.507085
302.729731	13977.506370	28.512103
302.731438	14007.586727	28.517120
303.239243	14037.435411	28.522138
303.229980	14031.296559	28.527156
303.453901	14071.903960	28.532173
303.686823	14083.866405	28.537191
304.216385	14129.922741	28.542208
304.676803	14134.036746	28.547226
304.667093	14178.223679	28.552244
305.265393	14197.722466	28.557261
305.271020	14229.846320	28.562279
305.323050	14252.326905	28.567296
306.144520	14288.096296	28.572314
306.758803	14296.954706	28.577332
306.663057	14339.635698	28.582349
307.383306	14352.854069	28.587367
307.627578	14372.693616	28.592384
308.134823	14393.356407	28.597402
308.415184	14397.150409	28.602420
308.430691	14440.646863	28.607437
308.859919	14440.951184	28.612455
308.815364	14462.901229	28.617472
309.176823	14511.127885	28.622490
309.606570	14524.058752	28.627508
309.667953	14547.535663	28.632525
309.789946	14578.000605	28.637543
310.365103	14597.150725	28.642560
310.801621	14627.445615	28.647578
311.159592	14662.287063	28.652596
311.143939	14693.288667	28.657613
311.891901	14697.115794	28.662631
312.036357	14735.535040	28.667648
312.184781	14745.272739	28.672666
312.222293	14789.275472	28.677684
312.860519	14805.476563	28.682701
313.011455	14851.799209	28.687719
313.622651	14882.298936	28.692736
314.071647	14889.071828	28.697754
314.593624	14926.557737	28.702772
315.209117	14930.599054	28.707789
315.723992	14956.341712	28.712807
316.061282	14963.464011	28.717824
316.299364	14983.762315	28.722842
316.689408	14997.166561	28.727860
316.590896	15009.546885	28.732877
317.100762	15031.710237	28.737895
317.086714	15051.818635	28.742912
317.742423	15065.506819	28.747930
317.650327	15098.181165	28.752948
317.787613	15103.886810	28.757965
318.442011	15129.624027	28.762983
318.288420	15160.797440	28.768000
318.840693	15191.517070	28.773018
318.815074	15206.167308	28.778036
318.960023	15228.364427	28.783053
319.295740	15265.021484	28.788071
319.483194	15294.183191	28.793088
319.934092	15337.532901	28.798106
320.241783	15368.121505	28.803124
320.674497	15388.095051	28.808141
321.413239	15423.521328	28.813159
321.543439	15448.749980	28.818176
321.860605	15449.181573	28.823194
322.257995	15485.004764	28.828212
322.292706	15497.015183	28.833229
322.336987	15523.741033	28.838247
322.894316	15573.645151	28.843264
323.199904	15583.800209	28.848282
323.905309	15611.157640	28.853300
324.087559	15626.500393	28.858317
324.672134	15645.349207	28.863335
324.635236	15671.978401	28.868352
325.313035	15684.016666	28.873370
325.504938	15715.069450	28.878388
326.043811	15738.190266	28.883405
326.614680	15765.203002	28.888423
326.719031	15786.975797	28.893440
327.445592	15793.479439	28.898458
327.350182	15807.697347	28.903476
327.505414	15815.921707	28.908493
328.039384	15847.599019	28.913511
328.102957	15869.846703	28.918528
327.996141	15902.143726	28.923546
328.790256	15911.520157	28.928564
328.880040	15962.391519	28.933581
329.391442	15974.462219	28.938599
329.678366	16024.250074	28.943616
330.549673	16027.009166	28.948634
330.327398	16061.166246	28.953652
330.294927	16106.154867	28.958669
330.864999	16123.860939	28.963687
330.759861	16163.513039	28.968704
331.481897	16189.992483	28.973722
331.715136	16214.949998	28.978740
331.770395	16240.376641	28.983757
332.151117	16279.937725	28.988775
332.556054	16313.148586	28.993792
332.875487	16333.488718	28.998810
333.547687	16382.162861	29.003828
333.277545	16414.275125	29.008845
334.494694	16442.480802	29.013863
334.561753	16485.157858	29.018880
334.917556	16510.114489	29.023898
335.068862	16542.182594	29.028916
335.545074	16564.331535	29.033933
336.434680	16605.197765	29.038951
336.732814	16632.751853	29.043968
336.818591	16630.624506	29.048986
337.375193	16655.521395	29.054004
337.570016	16684.410153	29.059021
338.488577	16700.103493	29.064039
338.586935	16736.875570	29.069056
338.845329	16753.754421	29.074074
339.322170	16765.227817	29.079092
339.452520	16796.321196	29.084109
340.053859	16804.065752	29.089127
340.039591	16830.415721	29.094144
340.498679	16863.681796	29.099162
340.717769	16888.221888	29.104180
340.862732	16900.689502	29.109197
341.312735	16930.959666	29.114215
341.575020	16947.218705	29.119232
342.012136	16986.159119	29.124250
342.332749	17015.918126	29.129268
342.588345	17044.230117	29.134285
342.656849	17053.906753	29.139303
342.980274	17097.450837	29.144320
343.524855	17099.717219	29.149338
343.540391	17133.922355	29.154356
343.835219	17178.163251	29.159373
344.100989	17180.526138	29.164391
344.627761	17234.690930	29.169408
344.786096	17253.889408	29.174426
345.445620	17288.313139	29.179444
345.457059	17310.045000	29.184461
346.045585	17349.531791	29.189479
346.161749	17368.277165	29.194496
346.280565	17392.903925	29.199514
346.943102	17432.673411	29.204532
346.859869	17465.949925	29.209549
347.502434	17508.518812	29.214567
347.695123	17530.760034	29.219584
348.223514	17567.641027	29.224602
348.800562	17591.320822	29.229620
349.122608	17634.898083	29.234637
349.511760	17655.204702	29.239655
349.881688	17691.866287	29.244672
349.938813	17722.302112	29.249690
350.524538	17755.839078	29.254708
350.656755	17782.842515	29.259725
351.340402	17825.946036	29.264743
351.527884	17849.536105	29.269760
352.187682	17894.289184	29.274778
352.609832	17903.732952	29.279796
353.207122	17917.207815	29.284813
353.482782	17940.217628	29.289831
354.079836	17984.235824	29.294848
353.916335	18000.358204	29.299866
354.437983	18039.023946	29.304884
354.831893	18059.965452	29.309901
355.358639	18095.702074	29.314919
355.855492	18110.462460	29.319936
356.077590	18150.279655	29.324954
356.630036	18157.782333	29.329972
356.809478	18192.927181	29.334989
357.397199	18218.368224	29.340007
357.545576	18235.427542	29.345024
357.895558	18270.719332	29.350042
358.504992	18270.134984	29.355060
358.618214	18321.298228	29.360077
358.985176	18327.991547	29.365095
359.549853	18349.395390	29.370112
359.197046	18383.413370	29.375130
359.969326	18405.503287	29.380148
360.137091	18454.832762	29.385165
360.182625	18463.554150	29.390183
360.460552	18487.938757	29.395200
360.598831	18534.196695	29.400218
361.602587	18546.044535	29.405236
361.891992	18582.746629	29.410253
361.915064	18630.612639	29.415271
362.450412	18663.092718	29.420288
362.673723	18697.574134	29.425306
363.094710	18723.833166	29.430324
363.416835	18775.800258	29.435341
363.926002	18812.345193	29.440359
364.432399	18826.578203	29.445376
365.140664	18854.988763	29.450394
365.937109	18872.926796	29.455412
366.175669	18890.540899	29.460429
366.251072	18920.283971	29.465447
366.875617	18932.782659	29.470464
366.838267	18977.496237	29.475482
367.128311	18985.777154	29.480500
367.302192	19012.756811	29.485517
367.874174	19050.445676	29.490535
368.047876	19060.930470	29.495552
368.191989	19090.853220	29.500570
368.639873	19117.584452	29.505588
368.823136	19146.802574	29.510605
369.049714	19183.215327	29.515623
369.595222	19207.525270	29.520640
370.064366	19242.296642	29.525658
370.606523	19278.874991	29.530676
370.535825	19306.240725	29.535693
371.113350	19331.875900	29.540711
371.369054	19379.901103	29.545728
371.665555	19416.898636	29.550746
372.272510	19447.138053	29.555764
372.611688	19472.339949	29.560781
372.611800	19515.072180	29.565799
373.253760	19529.012289	29.570816
373.476909	19579.893311	29.575834
374.309671	19608.987614	29.580852
374.530790	19631.963090	29.585869
375.219167	19671.410590	29.590887
375.581458	19687.315347	29.595904
375.596910	19737.149845	29.600922
376.240602	19744.010825	29.605940
376.522892	19798.404137	29.610957
376.843490	19820.307335	29.615975
377.385800	19854.773146	29.620992
377.435825	19886.404227	29.626010
377.993854	19910.471966	29.631028
378.281639	19955.426086	29.636045
378.747777	19998.304833	29.641063
379.346491	20008.330673	29.646080
379.657344	20056.507934	29.651098
380.158125	20071.817987	29.656116
380.281683	20119.648059	29.661133
380.435832	20152.432065	29.666151
381.387379	20188.148759	29.671168
381.426850	20225.231543	29.676186
381.791459	20250.583326	29.681204
381.976225	20277.706691	29.686221
382.242699	20323.177632	29.691239
382.850456	20339.805409	29.696256
382.996962	20403.659033	29.701274
383.720258	20419.003584	29.706292
384.102265	20455.696113	29.711309
384.459469	20518.629470	29.716327
385.410467	20532.853563	29.721344
385.495586	20563.704575	29.726362
386.338755	20580.479714	29.731380
386.500421	20631.591655	29.736397
386.679228	20652.898293	29.741415
387.460143	20677.437916	29.746432
387.138825	20705.667064	29.751450
387.953162	20752.243557	29.756468
388.246112	20764.164718	29.761485
388.337098	20808.649220	29.766503
388.928935	20829.786967	29.771520
389.117172	20871.630911	29.776538
390.075283	20888.696346	29.781556
390.052983	20928.653607	29.786573
390.397903	20960.387773	29.791591
390.952679	20987.057076	29.796608
391.242967	21026.658690	29.801626
391.842089	21062.170656	29.806644
392.001164	21091.024169	29.811661
392.562595	21135.731346	29.816679
393.196805	21155.462663	29.821696
393.227098	21189.687938	29.826714
393.582398	21233.816207	29.831732
393.662744	21246.989826	29.836749
393.818182	21260.750087	29.841767
394.680436	21305.855728	29.846784
395.100741	21341.903861	29.851802
395.402196	21371.945032	29.856820
395.800301	21405.693814	29.861837
396.256057	21425.089200	29.866855
396.768037	21471.429170	29.871872
396.736362	21495.721166	29.876890
397.297734	21522.814301	29.881908
397.555234	21555.409013	29.886925
397.806165	21601.150855	29.891943
398.419246	21626.413244	29.896960
398.450062	21658.730315	29.901978
399.030343	21701.906739	29.906996
399.619050	21731.201159	29.912013
399.796779	21781.319225	29.917031
400.196470	21811.564088	29.922048
400.534036	21872.683408	29.927066
401.112773	21893.291825	29.932084
401.570126	21934.731390	29.937101
401.521697	21987.922155	29.942119
402.395901	22018.818919	29.947136
403.136542	22054.817251	29.952154
403.386978	22095.414868	29.957172
403.719012	22122.917339	29.962189
403.956991	22158.589043	29.967207
404.598103	22206.109435	29.972224
404.544331	22244.394488	29.977242
405.416977	22284.546101	29.982260
405.941189	22324.058549	29.987277
405.949581	22356.650256	29.992295
406.789618	22394.305586	29.997312
406.939401	22435.344738	30.002330
407.277355	22483.440981	30.007348
407.610275	22511.051148	30.012365
407.774540	22554.749386	30.017383
408.249660	22598.210355	30.022400
408.588345	22646.321133	30.027418
409.047843	22667.771585	30.032436
409.638294	22730.901773	30.037453
409.702355	22762.531257	30.042471
410.597658	22815.362219	30.047488
410.795468	22864.310399	30.052506
411.324319	22899.856802	30.057524
412.068380	22932.974494	30.062541
412.391046	22986.359373	30.067559
412.679161	23019.093770	30.072576
413.126838	23057.991537	30.077594
413.682320	23096.332393	30.082612
414.145119	23130.695144	30.087629
414.498354	23172.276368	30.092647
415.336017	23205.770132	30.097664
415.396617	23241.210148	30.102682
415.667051	23278.217405	30.107700
416.188188	23305.029981	30.112717
416.566953	23355.862124	30.117735
417.421904	23379.791236	30.122752
417.412963	23419.477899	30.127770
418.193495	23451.375019	30.132788
418.317463	23499.914713	30.137805
418.672863	23529.924043	30.142823
419.224428	23577.264460	30.147840
419.372666	23605.968009	30.152858
419.749343	23639.207697	30.157876
420.152363	23683.495354	30.162893
420.505016	23714.957554	30.167911
421.103112	23764.015660	30.172928
421.338858	23794.645930	30.177946
421.904086	23842.866185	30.182964
422.526605	23873.459511	30.187981
422.624737	23902.521861	30.192999
423.254194	23944.973830	30.198016
423.439208	23970.521746	30.203034
423.775291	24019.111458	30.208052
424.300530	24043.423932	30.213069
424.283118	24091.153044	30.218087
424.695692	24119.706588	30.223104
425.205402	24173.143166	30.228122
425.511858	24223.974105	30.233140
426.091217	24257.517367	30.238157
426.318594	24330.716093	30.243175
426.802847	24355.474111	30.248192
427.169735	24403.093320	30.253210
427.515037	24447.635331	30.258228
428.328610	24500.958106	30.263245
428.686430	24549.061700	30.268263
429.252728	24575.413168	30.273280
429.911058	24641.257581	30.278298
430.189931	24682.293497	30.283316
430.620819	24723.540912	30.288333
430.899658	24764.469815	30.293351
431.490646	24803.748432	30.298368
432.531429	24848.830964	30.303386
432.892466	24872.744459	30.308404
433.281494	24929.817283	30.313421
433.973306	24947.675103	30.318439
434.280172	24987.686972	30.323456
434.912776	25013.618213	30.328474
435.138527	25059.745736	30.333492
435.728668	25080.681004	30.338509
435.836947	25114.672750	30.343527
436.560730	25154.244024	30.348544
436.578260	25199.838684	30.353562
437.088384	25229.702488	30.358580
437.372673	25280.604911	30.363597
437.906240	25320.166998	30.368615
438.889768	25357.478868	30.373632
439.285589	25393.098233	30.378650
439.558320	25418.542392	30.383668
440.116062	25453.121251	30.388685
440.346660	25505.977422	30.393703
441.130636	25532.825812	30.398720
441.364448	25565.794871	30.403738
441.511474	25616.340963	30.408756
441.904901	25635.467685	30.413773
442.153732	25693.294729	30.418791
442.588304	25714.311668	30.423808
442.934962	25775.066774	30.428826
443.241186	25813.363522	30.433844
443.757462	25867.331027	30.438861
444.279060	25932.729990	30.443879
444.549888	25971.296274	30.448896
445.217645	26013.210976	30.453914
444.946613	26068.461856	30.458932
445.734924	26125.365515	30.463949
446.272673	26156.558842	30.468967
446.466080	26225.195269	30.473984
447.506119	26264.043564	30.479002
447.740654	26317.183866	30.484020
448.128546	26348.235149	30.489037
448.714746	26401.098435	30.494055
449.358903	26435.337025	30.499072
449.816561	26484.041447	30.504090
449.969654	26522.850771	30.509108
450.896151	26579.736277	30.514125
451.185237	26609.031909	30.519143
451.668116	26650.527724	30.524160
452.308400	26677.870007	30.529178
452.492622	26722.408325	30.534196
453.271640	26765.968581	30.539213
453.404919	26787.030309	30.544231
454.047837	26811.190126	30.549248
454.479571	26870.272997	30.554266
454.609079	26903.121527	30.559284
455.241566	26947.408190	30.564301
455.469619	26987.538706	30.569319
455.867405	27021.844404	30.574336
456.207113	27068.570403	30.579354
456.452111	27113.867679	30.584372
457.163196	27153.486708	30.589389
457.463705	27208.315698	30.594407
457.742509	27262.956058	30.599424
458.531758	27330.840905	30.604442
458.640940	27371.483975	30.609460
459.126990	27429.941629	30.614477
459.224612	27476.434334	30.619495
459.942581	27535.683537	30.624512
460.819393	27588.043586	30.629530
461.084922	27622.539498	30.634548
461.820931	27672.683715	30.639565
462.238080	27735.682971	30.644583
462.931914	27774.155065	30.649600
463.426436	27836.416481	30.654618
463.868358	27886.654060	30.659636
464.071613	27929.383518	30.664653
464.680833	27976.382881	30.669671
465.105729	28004.485152	30.674688
465.595580	28072.397161	30.679706
465.884426	28118.557225	30.684724
466.660444	28176.351321	30.689741
467.169096	28216.422593	30.694759
467.186299	28277.067533	30.699776
467.877750	28313.591978	30.704794
468.255426	28370.585138	30.709812
468.700846	28426.252012	30.714829
469.239961	28482.181156	30.719847
469.875065	28544.645863	30.724864
470.181355	28588.198951	30.729882
470.449347	28645.356232	30.734900
471.326340	28701.205043	30.739917
471.574058	28748.972777	30.744935
472.623996	28800.238649	30.749952
473.011425	28833.205980	30.754970
473.458284	28879.521776	30.759988
473.790878	28924.780970	30.765005
474.385272	28960.423861	30.770023
475.008395	29009.751597	30.775040
475.857144	29045.630224	30.780058
476.180579	29095.345216	30.785076
476.449266	29149.548491	30.790093
477.034210	29184.023162	30.795111
477.523404	29246.757399	30.800128
477.788162	29274.156398	30.805146
478.562865	29335.790255	30.810164
478.849708	29363.289840	30.815181
479.350006	29416.878453	30.820199
479.795759	29470.971476	30.825216
480.421541	29495.847643	30.830234
480.732503	29532.834976	30.835252
481.605627	29567.464692	30.840269
482.149239	29622.721760	30.845287
482.679225	29663.628787	30.850304
482.852736	29682.583442	30.855322
483.216276	29729.410521	30.860340
483.834862	29751.146465	30.865357
483.942309	29791.092099	30.870375
484.401799	29849.322624	30.875392
484.894122	29879.703775	30.880410
484.742336	29918.642100	30.885428
485.239402	29976.677579	30.890445
485.799889	30021.249034	30.895463
486.068207	30074.919012	30.900480
486.657866	30132.829315	30.905498
486.915098	30176.769895	30.910516
487.621045	30225.661568	30.915533
488.120331	30289.937312	30.920551
488.639224	30334.576378	30.925568
489.296202	30396.624623	30.930586
489.506101	30446.122506	30.935604
490.268902	30515.330251	30.940621
490.919954	30564.951185	30.945639
491.098502	30625.675500	30.950656
491.785803	30668.325470	30.955674
492.062547	30731.781567	30.960692
492.467574	30771.241816	30.965709
493.124211	30826.159129	30.970727
494.477553	30885.428460	30.975744
494.843218	30924.283565	30.980762
495.396156	30967.877614	30.985780
495.602360	31027.463099	30.990797
496.263150	31061.405315	30.995815
496.936986	31121.453322	31.000832
497.736562	31163.767345	31.005850
497.911610	31211.427688	31.010868
498.510894	31242.676867	31.015885
498.864976	31296.538352	31.020903
499.260747	31345.415012	31.025920
499.679122	31390.410947	31.030938
500.190958	31430.138972	31.035956
500.532856	31497.192927	31.040973
501.440586	31525.587121	31.045991
501.606540	31593.105859	31.051008
501.930308	31640.004598	31.056026
502.598408	31682.411005	31.061044
502.979706	31735.647863	31.066061
503.446061	31784.365820	31.071079
503.664862	31862.603097	31.076096
504.697902	31915.180763	31.081114
504.918979	31968.555214	31.086132
505.063861	32027.409709	31.091149
506.051424	32073.143104	31.096167
506.075538	32135.485062	31.101184
506.533103	32202.648812	31.106202
507.056901	32254.175869	31.111220
507.398243	32334.086016	31.116237
508.071859	32381.755535	31.121255
508.317437	32468.824763	31.126272
509.115871	32513.915405	31.131290
509.747311	32581.544053	31.136308
510.122437	32650.874791	31.141325
510.906437	32708.739472	31.146343
511.585331	32747.316586	31.151360
512.295356	32794.195633	31.156378
512.798197	32852.889660	31.161396
513.285194	32905.541570	31.166413
514.027519	32956.242699	31.171431
514.013002	33013.981575	31.176448
514.453984	33069.705076	31.181466
515.484028	33124.690988	31.186484
516.029810	33180.839233	31.191501
516.593960	33231.539038	31.196519
516.702333	33280.033178	31.201536
517.211740	33317.292340	31.206554
517.387332	33383.507037	31.211572
518.083353	33423.830714	31.216589
518.537238	33482.560171	31.221607
518.532810	33560.021568	31.226624
519.479873	33596.114215	31.231642
519.965251	33676.827005	31.236660
520.362136	33717.866495	31.241677
520.997298	33769.695120	31.246695
521.622928	33835.171447	31.251712
522.176321	33884.458253	31.256730
522.612699	33954.705319	31.261748
523.067841	33990.290013	31.266765
523.883814	34062.632944	31.271783
524.068148	34112.098087	31.276800
524.625199	34167.843756	31.281818
525.370253	34218.008535	31.286836
525.751404	34286.104724	31.291853
526.491348	34333.468839	31.296871
527.110936	34404.138630	31.301888
527.670136	34443.376598	31.306906
528.316418	34512.133486	31.311924
528.525728	34566.767250	31.316941
529.267547	34633.211792	31.321959
529.268928	34685.409680	31.326976
530.017286	34751.544368	31.331994
530.437865	34810.116515	31.337012
530.794899	34884.718940	31.342029
531.939701	34927.455175	31.347047
532.018271	35005.458224	31.352064
533.015411	35085.856271	31.357082
533.130375	35132.218225	31.362100
534.034927	35202.320344	31.367117
534.602936	35258.622988	31.372135
534.730573	35318.239149	31.377152
535.537952	35379.077975	31.382170
536.108771	35415.624612	31.387188
536.332984	35497.095661	31.392205
537.104945	35568.126737	31.397223
537.806634	35623.496534	31.402240
538.535122	35671.519305	31.407258
539.489020	35732.287811	31.412276
539.576177	35805.922620	31.417293
540.387885	35826.826421	31.422311
540.774236	35893.978124	31.427328
541.217573	35949.609341	31.432346
542.019085	36015.070993	31.437364
542.237202	36087.088637	31.442381
542.840075	36128.184892	31.447399
543.241121	36185.710850	31.452416
543.896813	36255.018851	31.457434
544.410664	36319.733933	31.462452
544.641484	36386.259976	31.467469
545.202589	36440.932909	31.472487
545.975066	36508.531203	31.477504
546.201892	36576.636422	31.482522
546.674018	36639.513515	31.487540
547.141517	36684.940861	31.492557
547.952157	36764.758801	31.497575
548.350486	36829.141377	31.502592
548.920537	36895.701645	31.507610
549.679691	36966.727793	31.512628
549.934287	37030.497384	31.517645
550.954597	37094.831832	31.522663
551.243677	37179.263071	31.527680
551.961431	37226.856318	31.532698
552.527033	37286.589752	31.537716
552.786931	37339.775179	31.542733
553.460689	37376.498185	31.547751
553.729063	37452.498765	31.552768
554.210256	37515.102885	31.557786
554.967406	37563.144954	31.562804
555.800191	37626.739119	31.567821
556.546478	37675.102020	31.572839
557.117103	37734.444796	31.577856
557.614906	37795.882652	31.582874
558.086434	37850.606250	31.587892
558.473741	37917.020614	31.592909
558.941872	37965.862596	31.597927
559.738018	38018.649034	31.602944
560.060753	38084.254153	31.607962
560.563839	38152.572204	31.612980
560.958144	38227.261342	31.617997
561.610033	38280.861357	31.623015
561.840584	38361.110438	31.628032
562.633186	38428.403376	31.633050
563.143058	38505.959124	31.638068
564.153921	38567.469519	31.643085
564.752437	38623.771420	31.648103
565.041584	38694.553818	31.653120
565.640767	38765.200074	31.658138
566.120460	38823.418987	31.663156
566.297617	38902.233838	31.668173
567.367980	38968.921145	31.673191
567.788913	39049.343831	31.678208
568.233143	39108.219670	31.683226
569.165098	39187.962072	31.688244
569.446333	39271.066243	31.693261
569.919698	39316.186825	31.698279
570.380148	39384.715422	31.703296
570.818697	39476.196145	31.708314
571.857117	39536.165101	31.713332
572.520211	39612.674549	31.718349
572.991664	39696.525671	31.723367
573.182451	39779.808081	31.728384
574.010975	39842.972068	31.733402
574.471101	39919.847738	31.738420
575.433932	40001.476043	31.743437
575.976394	40045.072042	31.748455
576.915792	40121.124536	31.753472
577.535891	40195.809768	31.758490
577.951461	40242.027958	31.763508
578.239254	40329.614645	31.768525
579.195064	40394.893182	31.773543
579.286382	40470.588519	31.778560
580.171542	40562.487028	31.783578
580.774755	40617.844307	31.788596
581.164374	40698.917064	31.793613
581.801598	40750.721396	31.798631
582.276325	40819.262524	31.803648
582.603453	40905.794417	31.808666
583.628195	40953.504620	31.813684
584.340840	41050.964091	31.818701
585.071320	41096.299149	31.823719
585.828741	41169.425369	31.828736
586.712020	41252.716937	31.833754
587.414458	41288.903421	31.838772
587.868951	41361.903685	31.843789
588.187824	41418.904378	31.848807
588.903265	41467.222554	31.853824
589.444316	41548.210948	31.858842
589.878207	41599.022259	31.863860
590.088797	41677.445908	31.868877
590.786891	41734.949970	31.873895
591.395266	41798.381226	31.878912
592.001209	41875.095868	31.883930
592.779126	41933.531181	31.888948
592.928360	42007.692395	31.893965
593.213228	42054.501796	31.898983
593.842674	42137.037550	31.904000
594.306451	42194.881636	31.909018
595.299984	42252.729950	31.914036
595.463517	42333.856776	31.919053
596.012513	42406.681456	31.924071
596.711487	42484.005142	31.929088
597.176317	42562.816738	31.934106
597.762351	42631.829251	31.939124
598.320643	42708.975094	31.944141
599.125849	42788.163906	31.949159
599.836277	42846.714294	31.954176
600.381555	42941.989151	31.959194
600.907431	43016.126955	31.964212
601.350460	43086.408554	31.969229
602.249386	43184.353698	31.974247
602.871865	43250.155229	31.979264
603.152879	43345.216964	31.984282
603.908709	43405.854594	31.989300
604.522381	43476.374670	31.994317
605.215370	43562.984956	31.999335
605.802225	43620.405969	32.004352
606.383449	43729.225014	32.009370
607.172911	43790.590751	32.014388
607.378956	43884.098673	32.019405
608.219883	43955.940515	32.024423
608.809596	44047.434928	32.029440
609.778832	44114.568164	32.034458
610.892432	44190.892931	32.039476
611.210496	44267.589334	32.044493
611.915380	44334.943822	32.049511
612.768986	44421.679986	32.054528
613.021940	44475.796614	32.059546
613.644782	44546.713888	32.064564
614.025478	44620.490646	32.069581
614.622711	44709.742450	32.074599
615.646673	44769.986689	32.079616
616.131029	44858.332836	32.084634
616.782333	44909.016353	32.089652
617.044779	44995.947553	32.094669
617.750627	45096.911856	32.099687
618.260340	45171.960753	32.104704
618.759828	45259.144489	32.109722
619.316664	45330.138802	32.114740
619.672533	45428.917982	32.119757
620.434212	45509.609515	32.124775
620.848259	45600.701756	32.129792
621.559596	45681.860142	32.134810
622.535630	45778.164534	32.139828
623.337258	45849.372975	32.144845
623.891750	45936.421352	32.149863
624.592347	46029.236419	32.154880
625.094504	46106.651962	32.159898
626.171483	46186.965998	32.164916
626.421941	46266.176068	32.169933
626.959522	46349.591954	32.174951
627.729586	46422.272790	32.179968
628.086359	46520.836590	32.184986
628.582542	46593.885376	32.190004
629.236412	46687.150301	32.195021
630.140193	46762.156302	32.200039
631.102559	46839.423096	32.205056
631.165404	46922.177953	32.210074
631.974518	47008.507269	32.215092
632.720977	47070.604520	32.220109
633.208935	47176.614284	32.225127
634.112571	47236.198052	32.230144
634.803437	47317.436387	32.235162
635.265780	47390.443347	32.240180
635.690599	47483.996352	32.245197
636.418671	47536.546731	32.250215
636.919741	47613.270872	32.255232
637.378005	47692.948380	32.260250
638.129108	47780.361234	32.265268
639.144977	47852.943872	32.270285
639.272809	47951.300389	32.275303
640.038188	48018.058244	32.280320
640.704409	48109.323123	32.285338
641.375916	48187.625522	32.290356
642.067789	48279.385893	32.295373
642.357699	48358.535119	32.300391
643.645255	48440.882825	32.305408
644.083947	48527.690791	32.310426
644.575015	48594.972804	32.315444
645.346649	48695.326735	32.320461
646.088451	48763.297369	32.325479
647.179762	48845.796090	32.330496
647.798167	48931.328925	32.335514
648.740131	48986.882624	32.340532
648.931980	49060.891212	32.345549
649.636345	49141.617309	32.350567
650.675774	49223.731525	32.355584
650.841435	49306.066191	32.360602
652.081283	49382.413414	32.365620
652.586329	49469.192636	32.370637
652.669779	49542.668386	32.375655
653.384140	49624.913816	32.380672
653.975662	49712.661965	32.385690
654.638953	49786.383945	32.390708
654.934267	49881.542836	32.395725
655.164889	49974.249709	32.400743
656.567009	50075.959469	32.405760
656.967395	50163.592843	32.410778
657.681672	50262.155034	32.415796
658.220990	50347.113613	32.420813
659.129662	50451.925911	32.425831
659.457859	50527.515639	32.430848
660.145090	50625.957859	32.435866
660.700682	50708.831063	32.440884
661.710829	50811.108459	32.445901
661.941464	50888.294758	32.450919
663.167280	50999.958080	32.455936
663.819570	51089.610022	32.460954
664.262739	51175.649293	32.465972
664.754237	51281.100344	32.470989
665.176450	51367.216573	32.476007
666.155763	51472.098599	32.481024
667.201416	51559.833935	32.486042
667.546350	51664.812311	32.491060
668.482014	51738.253670	32.496077
669.139311	51833.315128	32.501095
669.957342	51923.243632	32.506112
670.510477	52005.895466	32.511130
671.179650	52095.776722	32.516148
671.943914	52180.466265	32.521165
672.335898	52285.535012	32.526183
673.489604	52374.260569	32.531200
673.973300	52460.542099	32.536218
674.573597	52547.761737	32.541236
675.861244	52628.617862	32.546253
676.194005	52725.193331	32.551271
676.856390	52807.956904	32.556288
677.495395	52896.068709	32.561306
678.135555	52972.033458	32.566324
678.997946	53051.947742	32.571341
679.411667	53129.551831	32.576359
680.272281	53212.009616	32.581376
680.518105	53289.272535	32.586394
680.984598	53362.772315	32.591412
681.621202	53457.908380	32.596429
681.996546	53538.628407	32.601447
682.461711	53641.828933	32.606464
683.216275	53736.662619	32.611482
683.871497	53850.009683	32.616500
684.746002	53942.341942	32.621517
685.123090	54038.673439	32.626535
686.075020	54136.597173	32.631552
686.404220	54242.925102	32.636570
687.052212	54361.488074	32.641588
687.830274	54455.159013	32.646605
688.590253	54576.073792	32.651623
689.339656	54665.012462	32.656640
690.006475	54776.512025	32.661658
690.674261	54878.870714	32.666676
691.479908	54992.862934	32.671693
692.179918	55100.814761	32.676711
693.228246	55178.846595	32.681728
694.091523	55281.712106	32.686746
694.679482	55382.791521	32.691764
695.517536	55473.797737	32.696781
696.036563	55590.993290	32.701799
697.204937	55686.090343	32.706816
697.796342	55776.525884	32.711834
698.357937	55888.447194	32.716852
699.148429	55970.574469	32.721869
699.546295	56088.134169	32.726887
700.053953	56171.528338	32.731904
700.936433	56300.248767	32.736922
701.508904	56393.470163	32.741940
702.285285	56511.885992	32.746957
702.668066	56623.190272	32.751975
703.853938	56710.417168	32.756992
704.360546	56824.071402	32.762010
705.068937	56926.301413	32.767028
706.056693	57023.267035	32.772045
706.651320	57122.477827	32.777063
707.700870	57236.897734	32.782080
708.444063	57323.069495	32.787098
709.048852	57443.067233	32.792116
710.092009	57526.069117	32.797133
710.688117	57644.186658	32.802151
711.677208	57724.462464	32.807168
712.335544	57833.447143	32.812186
712.603590	57934.105997	32.817204
713.395096	58025.213859	32.822221
713.841588	58142.461863	32.827239
714.345634	58244.208011	32.832256
715.364341	58355.347537	32.837274
716.615899	58447.070090	32.842292
717.843475	58540.572562	32.847309
718.653755	58637.847123	32.852327
719.421263	58719.749544	32.857344
720.333510	58816.028743	32.862362
720.742191	58901.131571	32.867380
721.736070	58990.415928	32.872397
721.950047	59059.230214	32.877415
722.591612	59150.481747	32.882432
723.181050	59240.851349	32.887450
723.468608	59350.714407	32.892468
723.966511	59425.808274	32.897485
724.680605	59543.386848	32.902503
725.258384	59617.823715	32.907520
726.105119	59746.193337	32.912538
726.648027	59816.813705	32.917556
727.191828	59935.541181	32.922573
727.733479	60030.320323	32.927591
728.690612	60138.857556	32.932608
729.256690	60241.450432	32.937626
729.451111	60358.961646	32.942644
730.527407	60456.308579	32.947661
730.818391	60587.094532	32.952679
731.661525	60690.079982	32.957696
732.258257	60810.269981	32.962714
732.451545	60929.825873	32.967732
733.672750	61047.102039	32.972749
734.664112	61187.868357	32.977767
735.382419	61286.340105	32.982784
736.127099	61404.562822	32.987802
737.001294	61523.757017	32.992820
737.755834	61644.020731	32.997837
738.484994	61769.768485	33.002855
739.429743	61873.804918	33.007872
740.647547	62003.202043	33.012890
740.802005	62113.102201	33.017908
742.000852	62225.939822	33.022925
742.089400	62352.789203	33.027943
743.036602	62451.222520	33.032960
743.979661	62582.514124	33.037978
744.362131	62706.795544	33.042996
745.474214	62824.517184	33.048013
746.380566	62939.574837	33.053031
747.054419	63053.622411	33.058048
747.735488	63183.956287	33.063066
748.443531	63303.359050	33.068084
750.012375	63412.122581	33.073101
750.718527	63537.929353	33.078119
751.462292	63624.519996	33.083136
752.485796	63748.145746	33.088154
753.124570	63842.389529	33.093172
754.163719	63952.893022	33.098189
754.726899	64055.707995	33.103207
755.840058	64172.874755	33.108224
756.893153	64253.791842	33.113242
757.198380	64379.101174	33.118260
757.805152	64473.037132	33.123277
758.448324	64594.910520	33.128295
759.195089	64697.824817	33.133312
759.488970	64805.915132	33.138330
760.310956	64933.664436	33.143348
760.984004	65028.540091	33.148365
761.685291	65160.678315	33.153383
762.568588	65271.916269	33.158400
763.275899	65383.733794	33.163418
763.832826	65500.879912	33.168436
764.892067	65617.716198	33.173453
765.187777	65746.107375	33.178471
766.072827	65860.805746	33.183488
766.665459	65999.755962	33.188506
767.332321	66108.050688	33.193524
768.243275	66247.879195	33.198541
768.783290	66369.546260	33.203559
769.653559	66491.943321	33.208576
770.513171	66629.374548	33.213594
771.004541	66747.752232	33.218612
772.274168	66845.932217	33.223629
773.117815	66983.400038	33.228647
774.376888	67113.606536	33.233664
774.827804	67225.893584	33.238682
775.540898	67362.342457	33.243700
776.592325	67454.480202	33.248717
777.393271	67563.822398	33.253735
777.726590	67667.458251	33.258752
778.601456	67793.857406	33.263770
778.903991	67898.188534	33.268788
779.691689	68007.769147	33.273805
780.540079	68139.238345	33.278823
781.049436	68256.515374	33.283840
781.494735	68385.353346	33.288858
782.320108	68508.161647	33.293876
783.296867	68651.061504	33.298893
784.161806	68781.185477	33.303911
784.826985	68903.681178	33.308928
785.294417	69040.472402	33.313946
786.450849	69171.840331	33.318964
787.091469	69304.343706	33.323981
787.978823	69435.125522	33.328999
788.863599	69565.497647	33.334016
789.700807	69701.182658	33.339034
790.462668	69829.503076	33.344052
791.360778	69970.439768	33.349069
792.104681	70093.959926	33.354087
793.035458	70245.141341	33.359104
793.663024	70355.196907	33.364122
794.630031	70498.256357	33.369140
795.321642	70628.015759	33.374157
796.190023	70771.447398	33.379175
796.896163	70893.935278	33.384192
797.810533	71033.194614	33.389210
798.460915	71180.129738	33.394228
799.271087	71305.941112	33.399245
800.393457	71454.014126	33.404263
801.511991	71596.543848	33.409280
802.382206	71707.628581	33.414298
803.074906	71848.605385	33.419316
803.937368	71960.723325	33.424333
805.064656	72083.464666	33.429351
805.901366	72203.390459	33.434368
807.193888	72342.267150	33.439386
807.862415	72447.363361	33.444404
809.046495	72563.048061	33.449421
809.705633	72687.665900	33.454439
810.347202	72803.517363	33.459456
811.396553	72930.557123	33.464474
812.048767	73047.426158	33.469492
812.897855	73169.637965	33.474509
813.586868	73281.367837	33.479527
814.493527	73407.966081	33.484544
815.886590	73504.158628	33.489562
816.008749	73639.455729	33.494580
816.891486	73748.993497	33.499597
817.707673	73881.060139	33.504615
818.247897	74014.874144	33.509632
819.126374	74112.469649	33.514650
819.541949	74259.148556	33.519668
820.266761	74377.543112	33.524685
821.287322	74530.213461	33.529703
821.716394	74651.649375	33.534720
822.554089	74761.098553	33.539738
823.400295	74917.879141	33.544756
824.085931	75033.039742	33.549773
824.948510	75165.504978	33.554791
825.667670	75304.836986	33.559808
826.442469	75458.047719	33.564826
827.237572	75589.470617	33.569844
828.102580	75728.534635	33.574861
828.979404	75883.818400	33.579879
829.539354	76011.836155	33.584896
830.764848	76150.558771	33.589914
831.564914	76270.974923	33.594932
832.295291	76409.218106	33.599949
833.169789	76524.020252	33.604967
833.628296	76657.453000	33.609984
834.787835	76791.251443	33.615002
835.538858	76920.659598	33.620020
836.429665	77068.600768	33.625037
837.333650	77191.458646	33.630055
837.730681	77331.407019	33.635072
838.563154	77455.315374	33.640090
839.501402	77605.883273	33.645108
839.940137	77738.073639	33.650125
841.040450	77893.771170	33.655143
841.488084	78032.027015	33.660160
842.595801	78193.341624	33.665178
843.498172	78341.928248	33.670196
844.282554	78476.444029	33.675213
844.844559	78634.278547	33.680231
845.697860	78786.917753	33.685248
847.080602	78943.872642	33.690266
847.860736	79079.088522	33.695284
848.544886	79243.611535	33.700301
849.465216	79382.664292	33.705319
850.270409	79546.726824	33.710336
851.019458	79695.430086	33.715354
851.626263	79851.583431	33.720372
852.799864	80006.739795	33.725389
853.965230	80168.299636	33.730407
854.701282	80323.909969	33.735424
855.387470	80463.450912	33.740442
856.533403	80629.818150	33.745460
857.124853	80772.431772	33.750477
858.226158	80935.152628	33.755495
859.081733	81094.240188	33.760512
859.910213	81250.657692	33.765530
860.769344	81390.915945	33.770548
861.642897	81552.103848	33.775565
863.022721	81691.120432	33.780583
864.939121	81826.146382	33.785600
865.874209	81946.039786	33.790618
867.356865	82077.969728	33.795636
868.425747	82199.740096	33.800653
869.124958	82323.495188	33.805671
869.834490	82461.735288	33.810688
870.330054	82595.121708	33.815706
871.220115	82715.842676	33.820724
872.029762	82848.995285	33.825741
872.906962	82989.058088	33.830759
873.328481	83109.852200	33.835776
874.183409	83255.158225	33.840794
875.306135	83379.690530	33.845812
875.903278	83532.062798	33.850829
876.897497	83649.621161	33.855847
877.657889	83796.730229	33.860864
878.566429	83926.690787	33.865882
878.837997	84082.138093	33.870900
879.641029	84219.930644	33.875917
880.335923	84372.899726	33.880935
880.846975	84525.976106	33.885952
881.843861	84692.575052	33.890970
882.863540	84836.345637	33.895988
883.123667	85016.834938	33.901005
884.120704	85170.252935	33.906023
885.129347	85348.312071	33.911040
885.682180	85504.602001	33.916058
886.580475	85666.023822	33.921076
887.366982	85831.805363	33.926093
888.696999	85979.675876	33.931111
889.540562	86142.501966	33.936128
890.837623	86279.130796	33.941146
891.578830	86444.848308	33.946164
892.186535	86577.322081	33.951181
893.287861	86726.956073	33.956199
894.105971	86872.790981	33.961216
895.032551	87031.813436	33.966234
895.870975	87170.117681	33.971252
896.469747	87348.038491	33.976269
897.225080	87512.268111	33.981287
898.119297	87671.167424	33.986304
898.990307	87851.938682	33.991322
899.924960	88011.276550	33.996340
900.455662	88179.078607	34.001357
901.365949	88359.486660	34.006375
902.251482	88510.433257	34.011392
903.308134	88704.638956	34.016410
904.227780	88854.550761	34.021428
905.087907	89040.331777	34.026445
906.295231	89226.284734	34.031463
906.994178	89399.756316	34.036480
908.248398	89582.300056	34.041498
909.261878	89735.264622	34.046516
910.095064	89918.968872	34.051533
911.066414	90080.504188	34.056551
912.001403	90258.682703	34.061568
913.207951	90415.612725	34.066586
914.261908	90590.629107	34.071604
915.327788	90741.984238	34.076621
916.403859	90911.721755	34.081639
916.828296	91071.411422	34.086656
918.009173	91252.233623	34.091674
918.837973	91415.098867	34.096692
919.718276	91593.524271	34.101709
920.588656	91760.390812	34.106727
921.349320	91931.807746	34.111744
922.106476	92124.730432	34.116762
923.334913	92285.320698	34.121780
924.010872	92467.153118	34.126797
925.294499	92633.729709	34.131815
926.133767	92822.948601	34.136832
927.275566	92983.608490	34.141850
928.479506	93159.264509	34.146868
929.221415	93334.643689	34.151885
930.367452	93479.623602	34.156903
930.877690	93674.131091	34.161920
932.129080	93830.987586	34.166938
932.974735	94013.797329	34.171956
933.825910	94183.443312	34.176973
934.576909	94358.556296	34.181991
935.296824	94528.365608	34.187008
936.159485	94729.671435	34.192026
937.055645	94890.327625	34.197044
937.664084	95084.817585	34.202061
938.998735	95259.372348	34.207079
940.135540	95460.930118	34.212096
941.170465	95630.948301	34.217114
942.068859	95803.332081	34.222132
942.957089	95973.497131	34.227149
944.393447	96168.403374	34.232167
945.427792	96332.293279	34.237184
945.965350	96521.242750	34.242202
946.642645	96682.630476	34.247220
947.481497	96876.204184	34.252237
948.714573	97064.872104	34.257255
949.270595	97232.758754	34.262272
950.150293	97411.271465	34.267290
950.837483	97587.671438	34.272308
951.497654	97763.342867	34.277325
952.879927	97966.836638	34.282343
953.370398	98148.235761	34.287360
953.827054	98334.712148	34.292378
955.493514	98513.742256	34.297396
955.892524	98705.984989	34.302413
956.934581	98889.735561	34.307431
958.226291	99081.055194	34.312448
959.256672	99280.439894	34.317466
960.206476	99450.124987	34.322484
960.817361	99657.583477	34.327501
961.697649	99839.240753	34.332519
963.107558	100040.043841	34.337536
964.104903	100225.818387	34.342554
965.659210	100415.376654	34.347572
965.983767	100610.754634	34.352589
967.408441	100796.222285	34.357607
969.086339	100961.359614	34.362624
969.991414	101146.415507	34.367642
971.121437	101338.829978	34.372660
971.672168	101535.235022	34.377677
972.795255	101696.018183	34.382695
973.749092	101890.428512	34.387712
974.465505	102081.327854	34.392730
975.815335	102268.585013	34.397748
976.611893	102455.574028	34.402765
977.783819	102650.226403	34.407783
978.608043	102830.502622	34.412800
979.239143	103029.508055	34.417818
980.358891	103213.315321	34.422836
981.034967	103415.285690	34.427853
981.917115	103603.136370	34.432871
983.405303	103804.507209	34.437888
984.136112	103991.948856	34.442906
985.346307	104187.948882	34.447924
985.793157	104385.773283	34.452941
986.707684	104596.273819	34.457959
988.385035	104796.481508	34.462976
988.820331	104998.200141	34.467994
989.648149	105194.296272	34.473012
990.713369	105407.298567	34.478029
991.940664	105608.979844	34.483047
993.377563	105803.245098	34.488064
994.659429	105996.429311	34.493082
996.013025	106208.168501	34.498100
996.502659	106393.894405	34.503117
997.983135	106588.019016	34.508135
999.056212	106765.001614	34.513152
999.738898	106972.494936	34.518170
1000.786178	107150.586198	34.523188
1001.696796	107363.794639	34.528205
1002.571912	107550.554255	34.533223
1003.315539	107739.895177	34.538240
1004.317997	107950.826231	34.543258
1005.490859	108122.760909	34.548276
1006.632245	108341.600381	34.553293
1007.579231	108537.043314	34.558311
1009.218803	108735.767620	34.563328
1009.980481	108919.060053	34.568346
1011.665932	109104.670989	34.573364
1012.490590	109291.894529	34.578381
1013.334191	109471.187626	34.583399
1014.002474	109682.415616	34.588416
1014.893730	109855.902569	34.593434
1015.863890	110054.721920	34.598452
1016.743168	110253.671747	34.603469
1017.522588	110437.326337	34.608487
1018.690177	110634.572148	34.613504
1019.350754	110832.903742	34.618522
1020.050686	111022.363906	34.623540
1021.036010	111221.835385	34.628557
1022.091888	111393.873808	34.633575
1022.963912	111602.993317	34.638592
1023.907207	111804.680024	34.643610
1024.914149	112000.543693	34.648628
1025.833975	112212.231367	34.653645
1026.761288	112433.191654	34.658663
1028.147789	112638.434138	34.663680
1028.440719	112844.960751	34.668698
1029.627557	113058.802349	34.673716
1030.599721	113278.799384	34.678733
1031.487713	113503.980399	34.683751
1032.996342	113727.033998	34.688768
1033.453653	113952.733168	34.693786
1034.443804	114163.157600	34.698804
1035.522209	114394.952389	34.703821
1036.920109	114613.445709	34.708839
1037.950827	114848.963899	34.713856
1038.665312	115078.746954	34.718874
1039.976547	115295.967830	34.723892
1041.267676	115522.580984	34.728909
1042.253770	115740.923166	34.733927
1043.704096	115965.081306	34.738944
1044.850843	116193.434024	34.743962
1046.004900	116427.805072	34.748980
1047.068072	116643.924573	34.753997
1048.293669	116872.573881	34.759015
1049.145976	117077.101421	34.764032
1049.973715	117314.371637	34.769050
1051.433627	117527.974637	34.774068
1052.554327	117762.527053	34.779085
1053.358015	117971.554085	34.784103
1054.826873	118193.788567	34.789120
1055.696020	118411.436025	34.794138
1056.980864	118629.105217	34.799156
1058.125400	118847.420067	34.804173
1059.294505	119060.119748	34.809191
1060.607326	119296.236899	34.814208
1061.526957	119506.662481	34.819226
1062.320455	119723.749648	34.824244
1063.265914	119957.854998	34.829261
1064.296125	120169.901683	34.834279
1065.562694	120385.141904	34.839296
1066.460488	120628.383391	34.844314
1067.692621	120826.615926	34.849332
1069.059817	121058.101134	34.854349
1069.974230	121275.154725	34.859367
1071.209691	121489.483358	34.864384
1071.640622	121713.589119	34.869402
1073.114751	121949.777472	34.874420
1074.264517	122157.802251	34.879437
1075.458419	122388.959237	34.884455
1076.511371	122584.572388	34.889472
1077.401839	122820.737448	34.894490
1078.355716	123038.798752	34.899508
1079.606766	123275.098031	34.904525
1080.619733	123481.532833	34.909543
1081.516540	123720.086412	34.914560
1082.477560	123962.901822	34.919578
1083.624158	124172.474766	34.924596
1084.625832	124407.455711	34.929613
1085.524873	124641.061504	34.934631
1086.987756	124869.963272	34.939648
1087.616563	125098.586303	34.944666
1088.944489	125331.632501	34.949684
1089.946510	125550.426754	34.954701
1090.762368	125778.491870	34.959719
1091.969704	125984.696597	34.964736
1092.453999	126215.658525	34.969754
1094.015483	126433.162942	34.974772
1094.713299	126682.976223	34.979789
1095.699592	126913.391737	34.984807
1097.391195	127136.747529	34.989824
1098.825724	127370.691804	34.994842
1099.622575	127598.761199	34.999860
1101.081156	127816.191199	35.004877
1101.894776	128049.115255	35.009895
1103.048486	128276.953405	35.014912
1103.949409	128494.898562	35.019930
1105.289607	128724.344222	35.024948
1106.390069	128975.466059	35.029965
1107.543373	129204.857460	35.034983
1108.877259	129425.627523	35.040000
1109.776219	129667.624705	35.045018
1111.085268	129905.360802	35.050036
1111.949669	130130.269297	35.055053
1112.703369	130365.755801	35.060071
1113.820321	130614.125192	35.065088
1115.172149	130865.322348	35.070106
1115.903225	131094.201777	35.075124
1117.269179	131350.901515	35.080141
1118.491001	131607.145501	35.085159
1119.874527	131836.138155	35.090176
1120.733385	132100.659755	35.095194
1122.094054	132319.950297	35.100212
1123.197563	132571.873986	35.105229
1124.123174	132816.882730	35.110247
1124.947027	133090.037966	35.115264
1126.317120	133329.450629	35.120282
1127.097812	133568.455356	35.125300
1128.228706	133838.802983	35.130317
1129.367754	134119.596836	35.135335
1130.522943	134362.551427	35.140352
1131.711610	134634.709000	35.145370
1132.854214	134889.699686	35.150388
1134.263011	135146.169665	35.155405
1135.129914	135403.301602	35.160423
1136.250095	135678.990820	35.165440
1137.485950	135931.641826	35.170458
1138.997113	136204.228506	35.175476
1140.388781	136451.761653	35.180493
1141.128080	136697.604199	35.185511
1142.266159	136972.249258	35.190528
1143.498894	137244.713149	35.195546
1144.189336	137490.709197	35.200564
1145.471155	137765.780920	35.205581
1146.624223	138035.906493	35.210599
1147.964505	138305.965348	35.215616
1148.968462	138575.042337	35.220634
1150.251589	138835.682504	35.225652
1151.054655	139104.480012	35.230669
1152.052940	139375.364757	35.235687
1153.654071	139650.221982	35.240704
1154.755624	139908.149321	35.245722
1155.928184	140168.602662	35.250740
1157.264550	140447.782869	35.255757
1158.220078	140700.225162	35.260775
1159.594921	140986.782595	35.265792
1160.939013	141245.643791	35.270810
1161.997491	141517.245956	35.275828
1163.345722	141787.686698	35.280845
1165.016667	142036.166398	35.285863
1166.278943	142291.308689	35.290880
1167.540547	142523.490359	35.295898
1168.326824	142756.817159	35.300916
1169.618580	142996.630203	35.305933
1170.811625	143241.165426	35.310951
1172.733529	143469.719541	35.315968
1173.920137	143694.110723	35.320986
1174.200101	143946.168743	35.326004
1175.596334	144164.923800	35.331021
1176.301424	144436.582124	35.336039
1177.423599	144673.733945	35.341056
1178.583214	144920.226670	35.346074
1179.751462	145176.686595	35.351092
1181.152896	145411.641661	35.356109
1181.559684	145679.605465	35.361127
1182.785062	145948.425296	35.366144
1184.014246	146221.126907	35.371162
1184.819126	146471.442652	35.376180
1186.439113	146751.121798	35.381197
1187.428271	147011.517771	35.386215
1188.340909	147275.897522	35.391232
1189.782835	147551.567053	35.396250
1190.608889	147823.713480	35.401268
1192.127536	148091.613470	35.406285
1192.780163	148383.106793	35.411303
1194.014199	148670.346894	35.416320
1195.416523	148963.407848	35.421338
1196.359307	149242.317876	35.426356
1197.890675	149531.253184	35.431373
1199.332533	149801.879851	35.436391
1201.170702	150094.548285	35.441408
1202.040334	150363.789761	35.446426
1203.082290	150652.890855	35.451444
1204.569842	150934.476022	35.456461
1205.770824	151225.965068	35.461479
1206.732769	151507.260902	35.466496
1207.967581	151797.772314	35.471514
1209.135471	152085.341926	35.476532
1210.428201	152372.740965	35.481549
1211.616319	152661.161459	35.486567
1213.192565	152931.725541	35.491584
1214.339006	153224.165164	35.496602
1215.601054	153506.669545	35.501620
1217.055609	153794.141581	35.506637
1217.964639	154073.372718	35.511655
1219.403881	154369.070645	35.516672
1220.527085	154657.301544	35.521690
1221.423713	154957.127069	35.526708
1222.970807	155241.842404	35.531725
1223.691099	155542.576830	35.536743
1224.852635	155821.195641	35.541760
1226.262407	156126.894518	35.546778
1226.870389	156434.288345	35.551796
1228.468848	156720.832715	35.556813
1229.827343	157048.161725	35.561831
1230.994216	157334.832604	35.566848
1232.516883	157634.321923	35.571866
1233.512110	157932.048603	35.576884
1235.031593	158226.367544	35.581901
1236.164516	158532.752579	35.586919
1237.566005	158827.171598	35.591936
1238.534956	159132.332515	35.596954
1239.380364	159455.922646	35.601972
1240.784489	159735.962761	35.606989
1241.752455	160071.639596	35.612007
1243.316967	160361.463569	35.617024
1244.638914	160672.375342	35.622042
1245.644596	160977.607710	35.627060
1247.314137	161286.855743	35.632077
1248.557720	161570.423771	35.637095
1249.458605	161854.545100	35.642112
1250.846732	162155.930053	35.647130
1252.000860	162443.159863	35.652148
1253.027035	162722.407686	35.657165
1254.683129	163038.674107	35.662183
1255.834857	163317.385095	35.667200
1257.419800	163611.504194	35.672218
1258.511348	163902.497065	35.677236
1259.806655	164183.093185	35.682253
1260.956425	164493.745190	35.687271
1261.620880	164779.207038	35.692288
1263.372901	165093.062706	35.697306
1264.753077	165403.416980	35.702324
1266.184384	165702.168896	35.707341
1267.491571	165994.345960	35.712359
1268.424957	166303.867078	35.717376
1269.881104	166606.960370	35.722394
1270.928520	166917.114173	35.727412
1272.452413	167198.631442	35.732429
1273.755651	167525.634805	35.737447
1274.655899	167843.191201	35.742464
1275.930571	168146.452156	35.747482
1277.247172	168459.605034	35.752500
1278.563408	168786.983701	35.757517
1279.690991	169103.712398	35.762535
1281.138709	169427.711743	35.767552
1282.456265	169725.279459	35.772570
1283.058770	170069.927605	35.777588
1284.750625	170394.160187	35.782605
1285.965593	170722.331223	35.787623
1287.320422	171051.763156	35.792640
1288.713554	171377.955501	35.797658
1290.343961	171709.618089	35.802676
1291.570848	172032.657652	35.807693
1292.665380	172357.307511	35.812711
1293.840658	172688.620935	35.817728
1295.332871	173018.361720	35.822746
1296.623332	173349.724359	35.827764
1297.429311	173676.791436	35.832781
1299.102742	174026.635217	35.837799
1300.341158	174352.252510	35.842816
1302.342199	174682.162280	35.847834
1303.683467	175008.617395	35.852852
1304.877335	175329.020578	35.857869
1306.140422	175654.769747	35.862887
1307.286185	176003.915898	35.867904
1309.033944	176314.018706	35.872922
1310.325822	176670.988241	35.877940
1311.646128	176989.643168	35.882957
1312.807781	177323.301261	35.887975
1314.150258	177659.571473	35.892992
1315.773513	177973.690405	35.898010
1316.568262	178320.373164	35.903028
1317.826111	178645.711975	35.908045
1319.326368	178990.658603	35.913063
1320.276739	179317.677058	35.918080
1321.619293	179670.573705	35.923098
1323.079536	180009.454972	35.928116
1324.065386	180350.802812	35.933133
1325.418185	180691.851278	35.938151
1326.613363	181029.209456	35.943168
1328.083809	181372.959101	35.948186
1328.902448	181718.595489	35.953204
1330.355651	182081.199937	35.958221
1331.593472	182427.444605	35.963239
1332.629911	182789.856318	35.968256
1334.085520	183139.560117	35.973274
1335.237383	183492.616360	35.978292
1336.440273	183825.257495	35.983309
1338.236337	184181.880128	35.988327
1339.298124	184537.623670	35.993344
1340.835693	184878.707442	35.998362
1341.896982	185222.664373	36.003380
1343.476072	185552.906187	36.008397
1345.145536	185906.248541	36.013415
1346.295728	186258.371562	36.018432
1348.066036	186585.960759	36.023450
1348.923079	186951.108779	36.028468
1350.137423	187303.062983	36.033485
1351.662670	187657.900248	36.038503
1352.826934	188023.944007	36.043520
1354.314887	188375.314105	36.048538
1355.697038	188723.784414	36.053556
1356.990215	189101.263405	36.058573
1358.633743	189440.200341	36.063591
1359.549389	189813.976445	36.068608
1361.201740	190173.099156	36.073626
1362.547452	190534.623086	36.078644
1363.620156	190908.888202	36.083661
1365.191936	191256.213033	36.088679
1366.419867	191629.759040	36.093696
1367.793550	192017.246892	36.098714
1369.016831	192400.446113	36.103732
1370.551378	192787.366656	36.108749
1372.130003	193164.863257	36.113767
1373.239895	193546.070215	36.118784
1375.214756	193901.811331	36.123802
1376.511931	194301.615013	36.128820
1378.082357	194648.769582	36.133837
1379.775372	195034.218592	36.138855
1381.001703	195387.857694	36.143872
1382.634064	195761.553207	36.148890
1384.155308	196134.228332	36.153908
1385.396391	196497.443347	36.158925
1386.575470	196887.152702	36.163943
1387.795160	197251.353139	36.168960
1389.362610	197617.681866	36.173978
1390.407673	198009.743487	36.178996
1391.741992	198396.338831	36.184013
1393.520871	198752.939873	36.189031
1394.437971	199151.313828	36.194048
1395.952242	199528.453433	36.199066
1397.576906	199903.520285	36.204084
1398.839480	200305.538689	36.209101
1400.202089	200690.352827	36.214119
1401.985608	201067.901128	36.219136
1403.606487	201455.203527	36.224154
1404.606453	201846.533699	36.229172
1406.270954	202226.545755	36.234189
1408.103458	202581.355605	36.239207
1409.559871	202949.738186	36.244224
1411.650478	203329.228936	36.249242
1413.222704	203684.722203	36.254260
1414.302731	204068.522765	36.259277
1415.736088	204427.851641	36.264295
1416.899822	204801.853321	36.269312
1418.298904	205180.160378	36.274330
1419.653919	205546.643328	36.279348
1420.508328	205923.025373	36.284365
1422.191970	206298.891604	36.289383
1423.236408	206691.637897	36.294400
1424.122961	207057.900981	36.299418
1425.524483	207462.133990	36.304436
1426.669335	207848.965664	36.309453
1428.153748	208250.319666	36.314471
1429.612660	208623.212716	36.319488
1431.320873	208977.299791	36.324506
1433.019369	209364.911184	36.329524
1434.451876	209734.842765	36.334541
1435.860365	210100.831130	36.339559
1437.230962	210474.369798	36.344576
1438.605740	210857.394655	36.349594
1440.145934	211227.455104	36.354612
1441.417376	211625.077611	36.359629
1442.646960	211992.158047	36.364647
1444.175774	212384.637261	36.369664
1445.998534	212758.759427	36.374682
1447.324568	213152.304270	36.379700
1448.746900	213529.403802	36.384717
1450.175007	213928.852711	36.389735
1451.436340	214317.943920	36.394752
1452.614008	214719.850495	36.399770
1453.616331	215120.518039	36.404788
1455.132151	215538.347013	36.409805
1456.699016	215994.239329	36.414823
1457.505100	216435.402322	36.419840
1459.091040	216847.282979	36.424858
1460.086955	217252.354845	36.429876
1461.322228	217716.463047	36.434893
1462.930430	218133.120490	36.439911
1464.057808	218589.784017	36.444928
1465.255876	219033.053531	36.449946
1467.146490	219477.683887	36.454964
1468.361288	219924.154870	36.459981
1470.264535	220382.197359	36.464999
1471.533781	220831.254079	36.470016
1473.384157	221285.804530	36.475034
1475.144900	221729.247354	36.480052
1476.553310	222194.973882	36.485069
1478.198242	222622.083085	36.490087
1479.811072	223088.414855	36.495104
1481.068953	223525.446285	36.500122
1482.868264	223972.651300	36.505140
1484.236768	224426.355198	36.510157
1486.320872	224852.054708	36.515175
1487.764985	225315.985627	36.520192
1489.659190	225756.705450	36.525210
1491.414408	226199.278677	36.530228
1492.461887	226636.001523	36.535245
1494.345049	227079.039600	36.540263
1495.392784	227523.817381	36.545280
1497.010918	227978.941998	36.550298
1498.459418	228414.335235	36.555316
1499.470359	228869.436380	36.560333
1501.624363	229309.821752	36.565351
1502.988524	229768.525490	36.570368
1504.037039	230219.637497	36.575386
1505.952494	230671.344629	36.580404
1507.537942	231129.584870	36.585421
1509.558473	231540.916421	36.590439
1511.182545	231986.910194	36.595456
1512.646061	232436.310195	36.600474
1514.289811	232865.818548	36.605492
1515.691579	233312.310464	36.610509
1517.504503	233746.924520	36.615527
1519.135637	234180.960248	36.620544
1520.488702	234633.154059	36.625562
1522.054742	235052.699083	36.630580
1523.513077	235502.617419	36.635597
1524.988807	235932.721223	36.640615
1526.304573	236376.569298	36.645632
1527.254647	236821.876016	36.650650
1529.144215	237251.051412	36.655668
1530.411591	237697.578206	36.660685
1531.728308	238116.765942	36.665703
1533.276461	238566.474671	36.670720
1534.690795	238979.043948	36.675738
1536.081120	239420.169709	36.680756
1537.504612	239857.785611	36.685773
1539.371121	240291.087326	36.690791
1540.708874	240741.674387	36.695808
1541.997209	241177.461287	36.700826
1543.516015	241632.262651	36.705844
1544.855641	242081.709354	36.710861
1546.446477	242530.785352	36.715879
1547.774566	242994.562731	36.720896
1549.870789	243440.077136	36.725914
1551.085366	243905.196082	36.730932
1552.705423	244356.836619	36.735949
1554.298394	244827.966147	36.740967
1555.616015	245286.008957	36.745984
1557.218612	245756.427419	36.751002
1559.145636	246224.456181	36.756020
1560.393268	246701.082350	36.761037
1561.854606	247167.919479	36.766055
1563.714877	247639.899113	36.771072
1564.878479	248127.769565	36.776090
1566.436378	248605.541659	36.781108
1567.871147	249101.015160	36.786125
1569.483316	249591.100151	36.791143
1571.279218	250071.299223	36.796160
1572.438278	250567.049011	36.801178
1574.683582	251052.967118	36.806196
1575.716062	251547.418143	36.811213
1577.418772	252042.394267	36.816231
1579.274255	252536.126420	36.821248
1580.267718	253042.220237	36.826266
1582.327912	253529.137073	36.831284
1583.573167	254054.166521	36.836301
1585.311183	254565.778533	36.841319
1586.967405	255069.885165	36.846336
1588.521378	255574.923600	36.851354
1590.687044	256088.244552	36.856372
1591.642246	256590.334146	36.861389
1593.260727	257107.912209	36.866407
1594.883671	257622.822500	36.871424
1596.398385	258143.111009	36.876442
1598.356949	258642.394223	36.881460
1599.933443	259166.559681	36.886477
1601.663579	259680.792679	36.891495
1603.232135	260197.008528	36.896512
1604.844546	260717.586613	36.901530
1606.740573	261216.906210	36.906548
1608.036809	261744.979738	36.911565
1610.023262	262259.094582	36.916583
1611.615055	262772.918867	36.921600
1613.274298	263285.868246	36.926618
1615.042136	263786.733046	36.931636
1616.575264	264304.224796	36.936653
1618.418943	264835.027266	36.941671
1619.899657	265351.587373	36.946688
1621.289433	265855.663849	36.951706
1623.321146	266369.947872	36.956724
1624.750459	266886.922120	36.961741
1626.536135	267393.218695	36.966759
1627.829292	267918.877203	36.971776
1629.052763	268423.665386	36.976794
1631.688638	268953.724882	36.981812
1633.005551	269450.494781	36.986829
1634.675531	269952.794646	36.991847
1636.471520	270458.909080	36.996864
1637.923704	270945.951201	37.001882
1639.750022	271440.374146	37.006900
1641.425792	271911.272781	37.011917
1642.958401	272411.103054	37.016935
1644.468350	272917.591981	37.021952
1645.690004	273419.453643	37.026970
1647.715097	273895.728372	37.031988
1649.050732	274409.204291	37.037005
1650.561456	274887.493070	37.042023
1652.053736	275411.153438	37.047040
1652.956193	275928.788159	37.052058
1655.282802	276443.164070	37.057076
1657.073529	276951.378407	37.062093
1658.681110	277475.879631	37.067111
1660.499636	277980.581856	37.072128
1661.767258	278516.034708	37.077146
1663.469871	279025.199359	37.082164
1665.029334	279566.825305	37.087181
1666.256876	280095.092341	37.092199
1667.999525	280627.032667	37.097216
1669.640433	281178.649731	37.102234
1671.378467	281729.055428	37.107252
1672.697497	282285.218824	37.112269
1674.229425	282829.432038	37.117287
1676.027945	283387.062728	37.122304
1677.439886	283946.330463	37.127322
1679.310019	284521.803399	37.132340
1680.874407	285070.805643	37.137357
1682.329719	285655.538729	37.142375
1684.144073	286219.330589	37.147392
1685.423279	286806.247876	37.152410
1687.566858	287374.782333	37.157428
1689.487813	287957.042731	37.162445
1690.868253	288535.960986	37.167463
1692.730673	289107.405841	37.172480
1694.520540	289693.821606	37.177498
1696.235063	290269.325114	37.182516
1698.080040	290868.757632	37.187533
1699.989687	291443.690772	37.192551
1701.778467	292022.705527	37.197568
1703.585387	292617.691631	37.202586
1705.654132	293196.147112	37.207604
1707.025582	293795.085960	37.212621
1708.795293	294368.556286	37.217639
1710.900177	294947.683668	37.222656
1712.633798	295530.120748	37.227674
1714.660361	296114.538668	37.232692
1715.949375	296710.200387	37.237709
1718.056977	297270.647464	37.242727
1719.645287	297862.443981	37.247744
1721.206155	298436.259348	37.252762
1722.983900	299024.157824	37.257780
1724.909781	299591.023851	37.262797
1726.265366	300185.970387	37.267815
1728.365158	300771.545735	37.272832
1729.998220	301360.572801	37.277850
1731.980756	301929.728180	37.282868
1733.521069	302525.875373	37.287885
1734.947953	303114.367538	37.292903
1737.016946	303676.615880	37.297920
1738.491958	304285.157387	37.302938
1740.776388	304859.478014	37.307956
1742.528991	305447.953050	37.312973
1744.201236	306041.999632	37.317991
1746.246212	306617.288665	37.323008
1747.761514	307201.448772	37.328026
1749.186722	307786.305661	37.333044
1750.760707	308368.010375	37.338061
1752.326277	308946.766636	37.343079
1754.159808	309495.913614	37.348096
1755.812716	310094.888542	37.353114
1757.305192	310643.931996	37.358132
1758.867426	311212.565829	37.363149
1760.674260	311800.151257	37.368167
1762.433241	312387.410212	37.373184
1764.289395	312955.170769	37.378202
1766.267284	313521.535875	37.383220
1768.334544	314119.854226	37.388237
1769.912096	314702.732673	37.393255
1771.898743	315278.174850	37.398272
1773.062249	315878.787179	37.403290
1774.430994	316468.619206	37.408308
1776.175218	317062.015946	37.413325
1777.610918	317677.398888	37.418343
1779.610005	318285.929066	37.423360
1781.028108	318915.651684	37.428378
1782.962256	319517.122850	37.433396
1784.786994	320144.812242	37.438413
1786.205996	320768.957201	37.443431
1788.203279	321414.635341	37.448448
1789.779456	322029.728691	37.453466
1791.766100	322656.682887	37.458484
1793.359065	323294.436791	37.463501
1795.260751	323943.128073	37.468519
1797.823435	324579.922458	37.473536
1799.598666	325219.836620	37.478554
1801.515049	325828.592316	37.483572
1803.248849	326490.565005	37.488589
1805.302115	327117.312852	37.493607
1807.286343	327753.536188	37.498624
1808.940098	328426.063719	37.503642
1810.403944	329059.490388	37.508660
1812.349612	329691.180678	37.513677
1814.127201	330346.884378	37.518695
1815.763236	331001.334787	37.523712
1817.763776	331660.389218	37.528730
1819.633529	332328.394307	37.533748
1821.645264	332956.738290	37.538765
1823.277386	333616.669005	37.543783
1825.033267	334264.563599	37.548800
1826.900714	334932.183172	37.553818
1828.337099	335603.267636	37.558836
1830.583295	336255.653155	37.563853
1832.154000	336921.495244	37.568871
1833.929408	337600.978157	37.573888
1835.966388	338270.356834	37.578906
1837.721415	338945.942129	37.583924
1839.551713	339618.637930	37.588941
1841.539428	340284.572331	37.593959
1843.121033	340975.898240	37.598976
1844.821229	341646.253944	37.603994
1846.820246	342333.685179	37.609012
1848.861245	342993.712118	37.614029
1850.542098	343693.538725	37.619047
1852.817062	344373.053347	37.624064
1854.345934	345049.585116	37.629082
1856.221409	345729.832199	37.634100
1858.431043	346411.867452	37.639117
1859.845397	347095.267891	37.644135
1861.785415	347787.048878	37.649152
1863.519046	348462.737551	37.654170
1865.897479	349151.152227	37.659188
1868.435711	349817.932682	37.664205
1870.134475	350504.789779	37.669223
1872.535595	351148.047441	37.674240
1874.355805	351834.889934	37.679258
1876.363062	352462.992473	37.684276
1878.407202	353110.163944	37.689293
1880.233419	353735.385485	37.694311
1882.424044	354367.237539	37.699328
1883.802050	354996.093282	37.704346
1885.335606	355626.995153	37.709364
1887.106913	356266.349457	37.714381
1888.745859	356906.198247	37.719399
1890.842134	357562.455662	37.724416
1892.222548	358217.450821	37.729434
1894.204865	358870.230505	37.734452
1896.058140	359527.588574	37.739469
1897.384097	360200.399417	37.744487
1899.425597	360870.924617	37.749504
1901.133157	361574.681008	37.754522
1902.621267	362243.778061	37.759540
1904.731721	362936.407664	37.764557
1906.486428	363618.199853	37.769575
1908.411176	364322.024818	37.774592
1910.510303	365004.345391	37.779610
1912.597590	365686.351685	37.784628
1914.902035	366395.962819	37.789645
1916.257145	367088.771240	37.794663
1917.961122	367790.946745	37.799680
1920.085247	368499.229887	37.804698
1921.827806	369220.576309	37.809716
1923.969231	369930.250530	37.814733
1925.546665	370662.859577	37.819751
1927.576629	371385.004966	37.824768
1929.432587	372103.233377	37.829786
1931.594916	372841.283408	37.834804
1933.556126	373560.480612	37.839821
1935.210512	374305.103531	37.844839
1937.384910	375027.483098	37.849856
1939.801107	375744.634235	37.854874
1941.419526	376500.732385	37.859892
1943.663208	377208.320882	37.864909
1945.297820	377956.827412	37.869927
1947.785834	378711.238425	37.874944
1949.666472	379437.558040	37.879962
1951.441617	380183.279989	37.884980
1953.240740	380920.866881	37.889997
1954.906062	381690.690700	37.895015
1956.610057	382425.674118	37.900032
1958.531435	383198.058654	37.905050
1960.411078	383946.115031	37.910068
1962.535269	384710.798729	37.915085
1963.973475	385487.850073	37.920103
1965.985656	386259.945571	37.925120
1968.367761	387014.872875	37.930138
1970.500696	387788.585637	37.935156
1972.924802	388560.279631	37.940173
1974.897807	389325.234945	37.945191
1976.685357	390098.289819	37.950208
1978.638577	390859.915709	37.955226
1980.464716	391644.664132	37.960244
1982.574833	392400.345407	37.965261
1984.730021	393171.464170	37.970279
1987.082445	393945.725162	37.975296
1989.086009	394710.442541	37.980314
1991.210369	395482.370322	37.985332
1993.427404	396230.817197	37.990349
1995.286910	397002.192343	37.995367
1997.085917	397765.624454	38.000384
1999.576852	398531.786951	38.005402
2001.279255	399301.684013	38.010420
2003.212434	400052.565792	38.015437
2005.328498	400807.098332	38.020455
2007.028861	401560.767631	38.025472
2008.998819	402296.456237	38.030490
2010.538919	403041.776009	38.035508
2012.953436	403774.515381	38.040525
2014.380373	404523.920494	38.045543
2016.725854	405258.558986	38.050560
2018.869277	406010.492656	38.055578
2020.649865	406758.842777	38.060596
2022.707293	407514.145667	38.065613
2024.810432	408290.069816	38.070631
2026.588255	409037.016400	38.075648
2028.428589	409809.546263	38.080666
2029.935562	410583.426747	38.085684
2032.574478	411356.642600	38.090701
2034.261967	412137.973225	38.095719
2035.721430	412942.472491	38.100736
2037.723458	413729.404826	38.105754
2039.681478	414538.029647	38.110772
2041.909563	415322.851195	38.115789
2043.726881	416125.700902	38.120807
2045.308788	416955.463662	38.125824
2047.238202	417783.572488	38.130842
2048.879632	418618.236756	38.135860
2051.241650	419476.055105	38.140877
2052.862821	420304.615290	38.145895
2054.621034	421151.840684	38.150912
2057.099180	421990.891641	38.155930
2058.874484	422878.194183	38.160948
2060.974512	423728.265070	38.165965
2062.785779	424587.571503	38.170983
2064.798108	425478.920776	38.176000
2067.058768	426372.526380	38.181018
2069.147515	427259.292058	38.186036
2071.614484	428123.886725	38.191053
2073.766240	429017.110067	38.196071
2076.299126	429874.897474	38.201088
2079.204900	430738.263308	38.206106
2081.136017	431638.362115	38.211124
2083.167807	432514.515353	38.216141
2085.167780	433386.287913	38.221159
2087.453408	434277.774126	38.226176
2089.889470	435129.364222	38.231194
2091.751810	436011.945251	38.236212
2094.051366	436877.110140	38.241229
2096.270136	437769.384966	38.246247
2098.363897	438637.959520	38.251264
2100.241933	439511.344653	38.256282
2102.366240	440389.868322	38.261300
2104.299164	441272.488601	38.266317
2106.479182	442179.121075	38.271335
2108.057092	443048.775650	38.276352
2110.141293	443950.494430	38.281370
2111.900925	444847.322166	38.286388
2113.952401	445763.038819	38.291405
2115.910025	446664.263061	38.296423
2118.090132	447587.977349	38.301440
2120.029135	448510.983978	38.306458
2122.033958	449407.888020	38.311476
2124.320071	450344.721206	38.316493
2126.301852	451255.007664	38.321511
2128.268038	452187.361671	38.326528
2130.655355	453106.808960	38.331546
2132.158949	454055.443354	38.336564
2134.854802	454977.034153	38.341581
2137.270781	455909.149456	38.346599
2138.956032	456864.656075	38.351616
2141.463886	457791.210299	38.356634
2143.522736	458701.818430	38.361652
2146.676859	459595.418734	38.366669
2149.034846	460486.684330	38.371687
2151.137062	461375.324017	38.376704
2153.512263	462230.866539	38.381722
2155.657799	463126.044931	38.386740
2157.793756	464014.714358	38.391757
2159.796645	464900.687078	38.396775
2161.808884	465772.465578	38.401792
2164.076652	466670.093117	38.406810
2166.161064	467550.980407	38.411828
2168.034939	468437.877182	38.416845
2170.156158	469337.024201	38.421863
2172.583862	470230.570730	38.426880
2174.880190	471139.611433	38.431898
2176.799268	472036.038747	38.436916
2178.759473	472940.249356	38.441933
2181.102154	473874.012974	38.446951
2182.817041	474780.399937	38.451968
2184.908572	475696.179429	38.456986
2187.026598	476628.833878	38.462004
2189.175426	477563.356541	38.467021
2191.344483	478507.931888	38.472039
2193.160226	479467.064747	38.477056
2195.415680	480393.648993	38.482074
2197.648119	481359.938663	38.487092
2199.915403	482307.839055	38.492109
2201.838659	483280.037821	38.497127
2203.936769	484246.500057	38.502144
2206.645277	485205.084319	38.507162
2208.648134	486176.609577	38.512180
2211.045968	487149.582328	38.517197
2213.454054	488149.359494	38.522215
2215.452829	489112.546984	38.527232
2217.936442	490099.126503	38.532250
2219.520125	491107.404035	38.537268
2222.138264	492087.641041	38.542285
2224.447890	493066.511183	38.547303
2226.815297	494067.170235	38.552320
2229.142221	495035.731602	38.557338
2231.135376	496045.926594	38.562356
2233.726421	497044.407987	38.567373
2235.685270	498040.109662	38.572391
2237.833241	499049.899867	38.577408
2240.449855	500043.407928	38.582426
2242.700092	501049.126651	38.587444
2244.976585	502041.967511	38.592461
2247.297194	503037.869677	38.597479
2249.613569	504055.049241	38.602496
2252.066613	505053.885667	38.607514
2254.364890	506068.725258	38.612532
2256.541153	507075.554271	38.617549
2258.832618	508073.124533	38.622567
2261.061186	509094.848040	38.627584
2263.303565	510080.352712	38.632602
2265.534812	511091.764722	38.637620
2268.199136	512089.177594	38.642637
2270.678969	513086.659684	38.647655
2272.709075	514109.912657	38.652672
2275.293486	515107.301465	38.657690
2277.323385	516124.123915	38.662708
2279.282478	517137.767752	38.667725
2281.771285	518131.150808	38.672743
2284.243262	519142.917382	38.677760
2286.620488	520151.257787	38.682778
2288.426651	521159.727617	38.687796
2290.939136	522185.447734	38.692813
2293.208887	523201.113984	38.697831
2295.580436	524205.563002	38.702848
2297.772098	525182.421539	38.707866
2299.504404	526188.507603	38.712884
2301.650222	527147.617833	38.717901
2304.515651	528126.190191	38.722919
2306.610343	529113.739665	38.727936
2309.161954	530120.636733	38.732954
2311.364672	531099.980140	38.737972
2312.953648	532096.579911	38.742989
2315.785133	533078.307258	38.748007
2317.462884	534102.397406	38.753024
2319.901647	535103.939934	38.758042
2322.206415	536105.033339	38.763060
2323.939847	537134.439199	38.768077
2326.376873	538169.393629	38.773095
2328.290355	539207.379877	38.778112
2331.022437	540248.075079	38.783130
2333.104318	541285.631991	38.788148
2335.178293	542346.309904	38.793165
2337.560065	543402.179202	38.798183
2339.919911	544483.177294	38.803200
2342.222928	545547.149949	38.808218
2344.545866	546615.062839	38.813236
2346.887782	547677.912020	38.818253
2349.408948	548759.459804	38.823271
2351.975599	549848.610001	38.828288
2354.142157	550931.404812	38.833306
2357.034685	552013.994990	38.838324
2359.555718	553103.599754	38.843341
2361.874430	554172.791129	38.848359
2363.815037	555281.370949	38.853376
2366.566238	556374.597353	38.858394
2368.581705	557467.605448	38.863412
2370.800957	558579.538151	38.868429
2373.502894	559678.736398	38.873447
2375.649633	560796.326290	38.878464
2377.667329	561918.415825	38.883482
2380.374896	563036.026484	38.888500
2382.823457	564163.330816	38.893517
2385.050154	565277.364724	38.898535
2386.882098	566416.281065	38.903552
2389.165961	567561.954177	38.908570
2391.618493	568695.998968	38.913588
2393.657298	569860.843190	38.918605
2396.438381	570998.397914	38.923623
2398.170582	572177.091325	38.928640
2400.842662	573359.085458	38.933658
2402.814268	574509.664069	38.938676
2405.223480	575703.982208	38.943693
2408.456242	576856.247981	38.948711
2410.866941	578034.738027	38.953728
2413.389312	579214.202942	38.958746
2415.896033	580384.127142	38.963764
2418.399373	581574.309444	38.968781
2420.625912	582748.923465	38.973799
2422.643694	583950.193650	38.978816
2425.185275	585137.217925	38.983834
2427.889183	586308.053657	38.988852
2430.337585	587510.508929	38.993869
2432.446893	588688.635111	38.998887
2435.181979	589889.704623	39.003904
2437.642429	591089.045786	39.008922
2439.910770	592278.625544	39.013940
2441.798846	593491.805109	39.018957
2444.571006	594680.110780	39.023975
2446.876290	595899.090137	39.028992
2449.435374	597082.129688	39.034010
2451.977804	598310.240509	39.039028
2454.389414	599504.182527	39.044045
2457.104158	600671.156689	39.049063
2459.297826	601861.337775	39.054080
2461.912831	603013.019272	39.059098
2464.191500	604190.478476	39.064116
2466.646019	605379.554098	39.069133
2469.565650	606519.220171	39.074151
2471.927811	607696.056376	39.079168
2474.690006	608870.453044	39.084186
2477.602308	610019.580803	39.089204
2479.862571	611213.435753	39.094221
2482.305318	612379.414939	39.099239
2484.738222	613565.086817	39.104256
2487.340099	614741.751096	39.109274
2490.371575	615885.507877	39.114292
2492.689248	617057.873024	39.119309
2495.613193	618242.016498	39.124327
2498.142146	619413.597327	39.129344
2500.319504	620585.211507	39.134362
2502.877854	621771.685714	39.139380
2505.031454	622975.393594	39.144397
2507.504493	624145.378005	39.149415
2509.965613	625350.671715	39.154432
2512.218072	626559.313580	39.159450
2514.772065	627771.267849	39.164468
2516.769407	628984.226333	39.169485
2519.287950	630216.043889	39.174503
2521.543945	631435.824898	39.179520
2524.232443	632688.556345	39.184538
2526.608893	633928.607099	39.189556
2529.120786	635154.808857	39.194573
2531.567167	636417.672893	39.199591
2533.647099	637667.965486	39.204608
2536.204563	638935.998161	39.209626
2538.618698	640218.971612	39.214644
2541.003221	641501.541621	39.219661
2543.379179	642780.810419	39.224679
2545.992360	644092.258152	39.229696
2548.303061	645376.452532	39.234714
2551.357617	646667.145825	39.239732
2553.600351	647986.134575	39.244749
2556.232078	649291.724012	39.249767
2558.898733	650603.620159	39.254784
2561.907619	651924.411248	39.259802
2564.650462	653225.085313	39.264820
2566.843431	654541.977053	39.269837
2569.422072	655865.457626	39.274855
2572.202272	657181.753160	39.279872
2574.412778	658517.196235	39.284890
2577.108278	659840.174947	39.289908
2579.490405	661176.124935	39.294925
2582.021561	662515.950984	39.299943
2584.402803	663837.046137	39.304960
2586.937663	665213.243858	39.309978
2589.359794	666560.544156	39.314996
2592.016201	667905.726173	39.320013
2594.628932	669271.974697	39.325031
2597.642705	670630.250034	39.330048
2599.730854	671973.013017	39.335066
2602.638983	673345.394121	39.340084
2605.015827	674716.967352	39.345101
2607.827544	676075.688796	39.350119
2610.235262	677458.194437	39.355136
2613.005635	678818.662771	39.360154
2615.712993	680166.616460	39.365172
2618.345917	681546.738846	39.370189
2621.434141	682919.276108	39.375207
2624.123934	684275.031482	39.380224
2626.806614	685626.266304	39.385242
2629.837279	686947.295320	39.390260
2632.048617	688255.306912	39.395277
2634.754261	689587.279208	39.400295
2637.812735	690910.259994	39.405312
2640.160806	692218.024465	39.410330
2642.840352	693534.725905	39.415348
2644.679076	694859.014585	39.420365
2647.162608	696175.260714	39.425383
2649.946681	697514.926059	39.430400
2652.267726	698877.182733	39.435418
2654.965101	700217.743338	39.440436
2657.118201	701593.246839	39.445453
2659.742936	702937.867731	39.450471
2662.308783	704315.553433	39.455488
2664.689714	705691.416518	39.460506
2667.268823	707059.893387	39.465524
2669.913307	708468.028302	39.470541
2672.726232	709856.139992	39.475559
2675.507511	711259.882667	39.480576
2678.040757	712665.813462	39.485594
2681.204510	714068.933294	39.490612
2683.948129	715481.742783	39.495629
2686.755526	716895.147960	39.500647
2689.528356	718301.690981	39.505664
2692.357722	719735.699217	39.510682
2695.430635	721144.092458	39.515700
2697.838724	722576.100977	39.520717
2700.697470	723993.002049	39.525735
2703.169272	725408.934102	39.530752
2705.497648	726856.585058	39.535770
2708.330930	728301.674481	39.540788
2710.990890	729740.113719	39.545805
2713.675389	731203.101450	39.550823
2716.550674	732642.773508	39.555840
2718.952927	734104.644645	39.560858
2722.048622	735561.545041	39.565876
2724.703018	737020.773660	39.570893
2727.255419	738483.802794	39.575911
2730.136345	739953.914848	39.580928
2733.298410	741421.834945	39.585946
2736.205107	742871.467915	39.590964
2739.150921	744355.213965	39.595981
2741.635661	745837.426041	39.600999
2744.327590	747299.895962	39.606016
2746.990251	748777.777154	39.611034
2749.938317	750252.719754	39.616052
2752.260280	751745.278689	39.621069
2755.015678	753231.714459	39.626087
2757.785697	754725.794540	39.631104
2760.282417	756215.197471	39.636122
2763.359833	757713.721130	39.641140
2766.047364	759205.270653	39.646157
2768.988717	760695.551897	39.651175
2771.757114	762211.458747	39.656192
2774.801215	763716.978876	39.661210
2777.521786	765203.360365	39.666228
2779.945784	766716.699003	39.671245
2782.840919	768219.819341	39.676263
2785.399794	769718.022186	39.681280
2788.116116	771250.850231	39.686298
2790.672189	772759.502304	39.691316
2793.477836	774289.771063	39.696333
2796.193431	775808.929184	39.701351
2799.115822	777354.017853	39.706368
2801.628011	778869.531033	39.711386
2804.774505	780397.096203	39.716404
2807.195982	781926.276603	39.721421
2809.939010	783448.063761	39.726439
2813.318098	784963.734120	39.731456
2815.753140	786446.863896	39.736474
2818.409791	787951.035248	39.741492
2820.964267	789439.706207	39.746509
2823.401989	790931.713778	39.751527
2826.059021	792449.889671	39.756544
2828.614956	793949.625206	39.761562
2831.691324	795484.967640	39.766580
2834.625690	796994.723010	39.771597
2837.188619	798534.333339	39.776615
2840.849854	800055.699376	39.781632
2843.569597	801578.699682	39.786650
2846.390246	803116.276501	39.791668
2849.204358	804650.723956	39.796685
2851.867840	806216.114337	39.801703
2854.365520	807753.934066	39.806720
2856.921521	809321.177424	39.811738
2859.981067	810896.533250	39.816756
2863.196246	812452.291316	39.821773
2865.872431	814037.294721	39.826791
2868.982431	815599.090349	39.831808
2871.750629	817179.334992	39.836826
2874.427813	818774.847997	39.841844
2877.827184	820384.360302	39.846861
2880.190247	821975.450739	39.851879
2883.002786	823585.896443	39.856896
2885.832787	825184.289074	39.861914
2888.741924	826800.911714	39.866932
2891.699730	828420.883497	39.871949
2894.672048	830046.594623	39.876967
2897.795676	831673.923196	39.881984
2900.555567	833307.531134	39.887002
2903.820096	834921.697060	39.892020
2906.579495	836584.385937	39.897037
2909.509584	838203.581290	39.902055
2912.562189	839830.525178	39.907072
2914.906382	841483.934897	39.912090
2917.889355	843134.281313	39.917108
2920.918568	844794.113035	39.922125
2923.450499	846467.740585	39.927143
2926.364805	848125.209771	39.932160
2929.481239	849789.206794	39.937178
2932.532844	851461.906413	39.942196
2935.467062	853150.496890	39.947213
2938.415137	854832.023621	39.952231
2941.301583	856488.153847	39.957248
2944.452289	858190.385673	39.962266
2947.338353	859836.300048	39.967284
2950.677247	861534.858512	39.972301
2953.250436	863212.415130	39.977319
2956.512185	864899.964873	39.982336
2959.485220	866603.377252	39.987354
2962.089421	868287.573134	39.992372
2964.956850	870000.801634	39.997389
2968.070439	871686.579175	40.002407
2971.448268	873373.097822	40.007424
2974.556268	875073.800064	40.012442
2977.453994	876766.987651	40.017460
2980.304770	878465.794143	40.022477
2983.203888	880155.981428	40.027495
2986.428404	881850.464363	40.032512
2989.405662	883562.089568	40.037530
2992.324079	885250.228012	40.042548
2995.618070	886948.731260	40.047565
2998.588794	888643.025534	40.052583
3002.081629	890342.627204	40.057600
3004.937418	892040.868538	40.062618
3007.811645	893711.784162	40.067636
3011.284054	895372.083461	40.072653
3014.304943	897002.083206	40.077671
3017.161263	898635.017806	40.082688
3019.718991	900264.448402	40.087706
3022.763085	901901.422779	40.092724
3025.349489	903553.119116	40.097741
3028.122742	905197.463521	40.102759
3031.214508	906873.423214	40.107776
3033.980393	908524.780787	40.112794
3036.680030	910175.852233	40.117812
3039.806344	911860.310870	40.122829
3042.613116	913557.673158	40.127847
3045.497081	915240.276001	40.132864
3048.868818	916959.659504	40.137882
3051.411108	918648.479956	40.142900
3054.422534	920366.563858	40.147917
3057.235085	922099.016976	40.152935
3060.692408	923808.931697	40.157952
3063.488853	925557.266294	40.162970
3066.360209	927292.362808	40.167988
3069.996879	929034.346338	40.173005
3072.600032	930797.592253	40.178023
3076.000186	932539.909430	40.183040
3078.925545	934308.167266	40.188058
3081.571077	936060.562653	40.193076
3084.790453	937837.549296	40.198093
3088.029349	939626.083698	40.203111
3091.362549	941397.733295	40.208128
3094.437565	943207.547492	40.213146
3097.398501	944985.784592	40.218164
3100.911707	946762.557327	40.223181
3103.456411	948574.601004	40.228199
3106.455258	950371.897875	40.233216
3109.803675	952186.738553	40.238234
3112.428703	954010.787157	40.243252
3115.772067	955832.921046	40.248269
3118.411412	957703.499638	40.253287
3121.674368	959600.591213	40.258304
3124.802199	961484.958146	40.263322
3127.749157	963376.460134	40.268340
3130.918053	965291.925778	40.273357
3133.951002	967185.484067	40.278375
3136.835664	969099.240339	40.283392
3139.586861	971022.434596	40.288410
3142.754827	972937.597916	40.293428
3145.520435	974893.545149	40.298445
3148.277699	976852.823944	40.303463
3151.593730	978790.675830	40.308480
3154.567273	980765.442142	40.313498
3157.373066	982734.878224	40.318516
3160.721784	984708.901089	40.323533
3163.404846	986690.818980	40.328551
3166.607252	988696.482984	40.333568
3169.607681	990687.175023	40.338586
3172.543806	992712.964015	40.343604
3175.998339	994705.091437	40.348621
3178.845038	996740.734045	40.353639
3181.894607	998751.912521	40.358656
3185.190205	1000765.346844	40.363674
3188.433449	1002804.572107	40.368692
3191.969732	1004812.935214	40.373709
3194.924230	1006858.120031	40.378727
3198.197293	1008894.948850	40.383744
3201.319993	1010918.273070	40.388762
3204.595868	1012962.548710	40.393780
3208.085437	1014990.453492	40.398797
3210.896598	1017039.716689	40.403815
3214.363297	1019052.798760	40.408832
3217.449387	1021066.285914	40.413850
3220.600839	1023053.797076	40.418868
3224.164273	1025024.969907	40.423885
3226.466331	1027031.222247	40.428903
3229.933319	1029015.695114	40.433920
3233.517981	1031003.693222	40.438938
3236.663882	1033018.280656	40.443956
3240.000622	1035007.885588	40.448973
3243.046382	1037005.221231	40.453991
3245.852622	1039023.771290	40.459008
3249.255119	1041025.873244	40.464026
3252.234606	1043048.524577	40.469044
3255.447988	1045088.414754	40.474061
3258.253383	1047121.169907	40.479079
3261.680007	1049179.164049	40.484096
3264.755235	1051224.037728	40.489114
3267.708480	1053296.936331	40.494132
3270.887362	1055379.116206	40.499149
3273.700238	1057465.376740	40.504167
3276.815758	1059570.590791	40.509184
3279.932697	1061679.994331	40.514202
3282.925167	1063806.851139	40.519220
3285.851501	1065923.011110	40.524237
3289.227683	1068069.939389	40.529255
3292.863560	1070224.135771	40.534272
3296.031158	1072380.342364	40.539290
3299.237052	1074548.054150	40.544308
3302.049095	1076708.841673	40.549325
3305.377676	1078909.188877	40.554343
3308.329968	1081109.859449	40.559360
3311.732995	1083291.869457	40.564378
3315.140956	1085509.247098	40.569396
3318.839794	1087722.231968	40.574413
3321.600415	1089943.260744	40.579431
3325.013907	1092186.004696	40.584448
3328.379141	1094405.298250	40.589466
3331.598626	1096625.710729	40.594484
3335.269910	1098861.163586	40.599501
3338.394996	1101129.822549	40.604519
3341.931068	1103370.487572	40.609536
3345.188831	1105615.031296	40.614554
3348.448057	1107877.400598	40.619572
3351.890526	1110135.647484	40.624589
3355.254104	1112384.585473	40.629607
3358.841963	1114663.361177	40.634624
3362.117654	1116932.758976	40.639642
3365.588277	1119187.194014	40.644660
3369.260854	1121460.689537	40.649677
3372.835242	1123717.947448	40.654695
3376.185475	1125987.860598	40.659712
3379.862943	1128234.649292	40.664730
3383.095197	1130498.581925	40.669748
3386.627223	1132761.786835	40.674765
3390.407327	1135015.933937	40.679783
3394.156926	1137276.422108	40.684800
3397.469634	1139539.427281	40.689818
3400.838773	1141779.029887	40.694836
3404.004063	1144035.312245	40.699853
3407.680998	1146283.456623	40.704871
3410.905459	1148542.343274	40.709888
3414.370040	1150796.444730	40.714906
3417.778711	1153051.668850	40.719924
3420.797303	1155325.057360	40.724941
3424.125380	1157585.713384	40.729959
3427.413809	1159850.872859	40.734976
3431.057671	1162114.241928	40.739994
3434.128920	1164388.034807	40.745012
3437.946601	1166610.318521	40.750016
3441.208598	1168829.513579	40.755021
3444.233832	1170949.685954	40.760026
3447.489736	1173028.406522	40.765031
3450.494000	1175048.268473	40.770036
3453.888507	1176957.497412	40.775040
3456.931231	1178813.141406	40.780045
3459.715007	1180576.819776	40.785050
3462.686625	1182253.447219	40.790055
3465.278004	1183883.575058	40.795060
3468.332842	1185418.654666	40.800064
3470.840976	1186868.153939	40.805069
3473.064792	1188258.806406	40.810074
3475.765074	1189558.571026	40.815079
3477.391368	1190799.726669	40.820084
3479.857972	1191957.099475	40.825088
3482.116773	1193063.235208	40.830093
3483.969772	1194104.580004	40.835098
3485.818063	1195077.256679	40.840103
3487.627709	1195989.196448	40.845108
3489.746174	1196830.517220	40.850112
3491.311545	1197641.192857	40.855117
3492.420041	1198372.514988	40.860122
3494.239638	1199063.548462	40.865127
3495.405869	1199694.362000	40.870132
3496.759305	1200293.640029	40.875136
3498.112705	1200837.410810	40.880141
3499.520958	1201341.252719	40.885146
3500.709075	1201800.345916	40.890151
3501.741429	1202224.726033	40.895156
3502.746689	1202608.097833	40.900160
3503.796360	1202933.674822	40.905165
3504.578169	1203261.619242	40.910170
3505.771250	1203523.284972	40.915175
3506.714832	1203776.822236	40.920180
3507.534676	1203983.400943	40.925184
3508.322760	1204167.478435	40.930189
3508.751128	1204331.548370	40.935194
3509.550419	1204445.027811	40.940199
3510.275330	1204565.265919	40.945204
3510.780707	1204642.420039	40.950208
3511.340752	1204706.722654	40.955213
3511.949522	1204754.425962	40.960218
3512.639540	1204760.780006	40.965223
3513.144705	1204782.348951	40.970228
3513.564855	1204748.630372	40.975232
3514.045726	1204712.183332	40.980237
3514.566382	1204643.578937	40.985242
3515.039027	1204562.046099	40.990247
3515.329500	1204481.198125	40.995252
3515.723939	1204362.836380	41.000256
3516.186890	1204274.738862	41.005261
3516.590534	1204150.933774	41.010266
3517.120881	1203999.637504	41.015271
3517.192963	1203847.474767	41.020276
3517.823289	1203680.402912	41.025280
3518.028080	1203506.364129	41.030285
3518.242309	1203292.845796	41.035290
3518.601352	1203103.204048	41.040295
3518.423410	1202885.795384	41.045300
3518.670688	1202668.963876	41.050304
3519.445975	1202447.066256	41.055309
3519.293258	1202223.811448	41.060314
3519.593763	1201999.909606	41.065319
3519.663104	1201751.182732	41.070324
3519.819076	1201487.610557	41.075328
3519.890613	1201218.879988	41.080333
3520.330688	1200954.858530	41.085338
3520.577878	1200675.377309	41.090343
3520.791457	1200388.287725	41.095348
3520.900328	1200124.465815	41.100352
3521.172259	1199818.290105	41.105357
3520.747281	1199539.608444	41.110362
3521.325859	1199222.369029	41.115367
3521.371815	1198911.954140	41.120372
3521.367058	1198591.393731	41.125376
3521.476280	1198292.380025	41.130381
3521.715726	1197963.481538	41.135386
3522.022560	1197644.969567	41.140391
3522.056361	1197306.864599	41.145396
3521.927786	1196982.939082	41.150400
3522.342730	1196646.793239	41.155405
3522.023210	1196297.602426	41.160410
3522.233291	1195959.567782	41.165415
3521.917916	1195634.837137	41.170420
3522.111620	1195279.107727	41.175424
3522.342287	1194939.312519	41.180429
3522.192068	1194589.978131	41.185434
3522.494558	1194229.650405	41.190439
3522.436538	1193888.424662	41.195444
3522.385074	1193511.761293	41.200448
3522.515493	1193168.860012	41.205453
3522.418374	1192807.089624	41.210458
3522.606164	1192442.334323	41.215463
3522.689008	1192094.671725	41.220468
3522.492224	1191715.834067	41.225472
3522.439556	1191342.959355	41.230477
3522.620199	1190970.395237	41.235482
3522.887122	1190608.692835	41.240487
3522.823011	1190226.998455	41.245492
3522.575203	1189861.380679	41.250496
3522.858406	1189489.726979	41.255501
3522.473927	1189121.259076	41.260506
3522.789772	1188753.119694	41.265511
3522.458475	1188380.265171	41.270516
3522.609336	1187974.673521	41.275520
3523.061530	1187619.031986	41.280525
3522.965083	1187219.628787	41.285530
3523.204092	1186842.995635	41.290535
3522.897834	1186462.944496	41.295540
3522.692474	1186085.012489	41.300544
3523.073448	1185698.959662	41.305549
3522.673372	1185322.415261	41.310554
3522.832359	1184927.403383	41.315559
3522.958461	1184546.575871	41.320564
3522.873903	1184144.204649	41.325568
3522.801604	1183761.846458	41.330573
3522.401641	1183369.443105	41.335578
3522.714356	1182971.056743	41.340583
3522.770727	1182600.075335	41.345588
3522.793319	1182211.280171	41.350592
3522.687375	1181812.214799	41.355597
3522.530223	1181440.055841	41.360602
3522.349362	1181035.482045	41.365607
3522.337852	1180673.507939	41.370612
3522.520782	1180261.186148	41.375616
3522.793872	1179881.310432	41.380621
3522.325701	1179498.420718	41.385626
3522.690875	1179093.794137	41.390631
3522.681661	1178717.553590	41.395636
3522.752827	1178328.082866	41.400640
3522.723465	1177916.646362	41.405645
3522.830195	1177531.821137	41.410650
3522.431189	1177136.025375	41.415655
3522.500587	1176751.525514	41.420660
3522.781519	1176345.379604	41.425664
3522.550199	1175952.199371	41.430669
3522.575269	1175539.057790	41.435674
3522.890166	1175145.538157	41.440679
3522.460357	1174755.222585	41.445684
3522.191892	1174343.448650	41.450688
3522.440479	1173962.767548	41.455693
3522.162548	1173578.090526	41.460698
3522.681546	1173172.223739	41.465703
3522.647354	1172782.826908	41.470708
3522.454236	1172384.089503	41.475712
3522.889680	1171992.009640	41.480717
3522.380422	1171601.753910	41.485722
3522.635527	1171182.097261	41.490727
3522.285238	1170798.830904	41.495732
3522.080720	1170395.792046	41.500736
3522.435025	1169988.666779	41.505741
3522.610426	1169591.353771	41.510746
3522.778363	1169197.503739	41.515751
3522.624898	1168798.202633	41.520756
3522.363314	1168395.962658	41.525760
3522.296340	1167992.810069	41.530765
3521.866355	1167587.420406	41.535770
3522.147097	1167195.949903	41.540775
3522.105598	1166804.880849	41.545780
3521.993678	1166386.126727	41.550784
3522.322044	1166004.568599	41.555789
3522.128065	1165606.824613	41.560794
3521.937258	1165208.199821	41.565799
3521.973053	1164835.388430	41.570804
3522.021356	1164424.007376	41.575808
3521.899634	1164039.073851	41.580813
3521.934618	1163624.987039	41.585818
3522.143337	1163226.240007	41.590823
3521.716670	1162827.283793	41.595828
3521.677048	1162449.401342	41.600832
3521.936524	1162053.202668	41.605837
3521.905417	1161643.128392	41.610842
3522.078550	1161242.062436	41.615847
3522.035701	1160860.568705	41.620852
3521.767047	1160445.524437	41.625856
3522.163871	1160054.729745	41.630861
3521.738546	1159655.059143	41.635866
3521.789832	1159263.033259	41.640871
3521.720255	1158870.052365	41.645876
3521.547348	1158462.305989	41.650880
3521.839070	1158071.853845	41.655885
3521.354252	1157676.014623	41.660890
3521.858998	1157277.334001	41.665895
3521.479027	1156876.309251	41.670900
3521.446496	1156473.304531	41.675904
3521.695737	1156082.806184	41.680909
3521.422573	1155684.416699	41.685914
3521.656513	1155295.849476	41.690919
3521.492741	1154912.523981	41.695924
3521.691801	1154493.430654	41.700928
3521.592637	1154101.801532	41.705933
3521.360279	1153716.791163	41.710938
3521.224418	1153305.893536	41.715943
3521.351292	1152929.475493	41.720948
3520.724698	1152537.911533	41.725952
3521.190923	1152141.025487	41.730957
3520.989912	1151750.374413	41.735962
3521.098534	1151371.859525	41.740967
3521.110466	1150995.985127	41.745972
3521.047296	1150584.484374	41.750976
3521.046412	1150201.546680	41.755981
3520.766281	1149819.290250	41.760986
3521.135405	1149421.741799	41.765991
3520.917699	1149047.566248	41.770996
3520.770383	1148648.149746	41.776000
3521.010433	1148249.018229	41.781005
3520.528526	1147873.002543	41.786010
3520.806703	1147488.684800	41.791015
3520.403712	1147101.323682	41.796020
3520.806710	1146721.763113	41.801024
3520.612898	1146328.718715	41.806029
3520.472330	1145953.742369	41.811034
3520.552364	1145562.965798	41.816039
3520.386746	1145164.805602	41.821044
3520.488095	1144786.198586	41.826048
3520.426460	1144420.771784	41.831053
3520.384422	1144026.962234	41.836058
3520.363162	1143656.924128	41.841063
3520.637477	1143274.861119	41.846068
3520.302116	1142875.608041	41.851072
3520.464865	1142502.708214	41.856077
3519.840979	1142140.441626	41.861082
3520.299518	1141739.169635	41.866087
3520.399931	1141386.503925	41.871092
3520.066195	1141000.486884	41.876096
3520.066067	1140591.897373	41.881101
3520.047345	1140236.327933	41.886106
3520.331577	1139867.682755	41.891111
3519.885770	1139486.698723	41.896116
3520.002684	1139125.052927	41.901120
3520.192037	1138719.040434	41.906125
3520.000828	1138350.842702	41.911130
3520.278875	1137974.567252	41.916135
3519.930384	1137594.570470	41.921140
3519.885914	1137214.591345	41.926144
3519.936865	1136844.350102	41.931149
3520.106229	1136458.489110	41.936154
3519.825286	1136085.020711	41.941159
3520.002759	1135705.181889	41.946164
3519.739307	1135328.428081	41.951168
3520.142833	1134952.962591	41.956173
3519.554030	1134581.053990	41.961178
3519.800319	1134209.741860	41.966183
3519.783378	1133827.615654	41.971188
3519.755681	1133463.422493	41.976192
3519.832714	1133086.358583	41.981197
3519.787706	1132710.143332	41.986202
3519.890320	1132320.476515	41.991207
3519.573824	1131970.484653	41.996212
3519.626508	1131585.524538	42.001216
3519.836233	1131210.111771	42.006221
3519.510996	1130825.634225	42.011226
3519.657351	1130452.079766	42.016231
3519.488037	1130095.190086	42.021236
3519.166263	1129714.625070	42.026240
3519.311863	1129352.023601	42.031245
3519.024705	1128990.609919	42.036250
3519.083506	1128600.963281	42.041255
3519.073188	1128247.062080	42.046260
3519.323692	1127877.209502	42.051264
3519.358093	1127506.225346	42.056269
3519.186078	1127164.550152	42.061274
3519.160252	1126774.974235	42.066279
3519.053437	1126394.992940	42.071284
3518.791866	1126042.223652	42.076288
3518.880148	1125671.007801	42.081293
3518.866797	1125310.917206	42.086298
3518.958278	1124960.682892	42.091303
3518.865594	1124594.275698	42.096308
3518.871341	1124239.249275	42.101312
3518.899434	1123863.443969	42.106317
3518.299436	1123507.897537	42.111322
3518.707505	1123139.594506	42.116327
3518.476207	1122790.984714	42.121332
3518.393472	1122435.662561	42.126336
3518.659845	1122069.879994	42.131341
3518.208340	1121735.521040	42.136346
3518.617966	1121369.762214	42.141351
3518.772784	1121009.544374	42.146356
3518.682591	1120650.485607	42.151360
3518.440468	1120298.667105	42.156365
3518.363538	1119931.937557	42.161370
3518.633181	1119598.469339	42.166375
3518.262384	1119219.640457	42.171380
3518.101946	1118863.712652	42.176384
3518.590595	1118515.848905	42.181389
3518.076841	1118165.650054	42.186394
3518.193321	1117805.985219	42.191399
3517.957813	1117464.748091	42.196404
3518.126759	1117102.740084	42.201408
3518.169832	1116754.263468	42.206413
3518.148274	1116399.102170	42.211418
3518.133922	1116031.713872	42.216423
3518.125597	1115703.578088	42.221428
3518.019075	1115340.829105	42.226432
3518.091643	1114989.181929	42.231437
3517.776805	1114655.692962	42.236442
3517.753102	1114288.091393	42.241447
3518.182064	1113936.507249	42.246452
3517.827693	1113598.190674	42.251456
3518.066308	1113259.755107	42.256461
3517.946923	1112898.846097	42.261466
3517.891425	1112571.575755	42.266471
3517.913320	1112210.406423	42.271476
3518.126893	1111838.972920	42.276480
3517.697352	1111497.197146	42.281485
3517.421429	1111171.118117	42.286490
3517.451380	1110809.185336	42.291495
3517.530302	1110495.316439	42.296500
3516.865913	1110150.439948	42.301504
3517.580299	1109788.421158	42.306509
3517.302468	1109464.911282	42.311514
3517.316489	1109107.829835	42.316519
3517.809019	1108768.783198	42.321524
3517.330587	1108449.445494	42.326528
3517.459069	1108092.850624	42.331533
3517.416057	1107768.245320	42.336538
3517.235986	1107415.284509	42.341543
3517.283684	1107088.904600	42.346548
3517.335794	1106733.282630	42.351552
3517.372644	1106387.380870	42.356557
3517.353511	1106076.612869	42.361562
3517.482079	1105735.907066	42.366567
3517.007071	1105389.165891	42.371572
3517.141736	1105048.702191	42.376576
3517.425945	1104710.485112	42.381581
3517.071674	1104362.893765	42.386586
3517.089334	1104035.282886	42.391591
3516.809092	1103709.229953	42.396596
3516.902290	1103363.602566	42.401600
3516.983863	1103033.626991	42.406605
3516.587218	1102700.556286	42.411610
3516.522917	1102367.027987	42.416615
3516.445476	1102039.024806	42.421620
3516.440196	1101711.850067	42.426624
3516.321473	1101398.343578	42.431629
3516.176748	1101082.720062	42.436634
3516.775938	1100755.961427	42.441639
3516.442091	1100442.817298	42.446644
3516.107900	1100108.620276	42.451648
3516.450261	1099772.187536	42.456653
3516.409181	1099455.782550	42.461658
3516.416455	1099120.703188	42.466663
3516.513793	1098802.802724	42.471668
3516.309745	1098490.767340	42.476672
3516.661663	1098164.370956	42.481677
3516.216483	1097821.825115	42.486682
3515.942576	1097509.075009	42.491687
3516.072284	1097188.874180	42.496692
3516.273725	1096867.207536	42.501696
3516.261478	1096545.365617	42.506701
3515.925822	1096224.514637	42.511706
3516.194351	1095913.975025	42.516711
3515.795017	1095592.522945	42.521716
3515.893549	1095287.525579	42.526720
3516.135325	1094961.624038	42.531725
3515.585271	1094643.968615	42.536730
3516.202986	1094338.162320	42.541735
3515.924749	1094007.790440	42.546740
3515.816186	1093709.630227	42.551744
3515.943403	1093388.630686	42.556749
3515.584495	1093080.138039	42.561754
3515.494430	1092766.700680	42.566759
3515.545877	1092455.902843	42.571764
3515.544362	1092146.244959	42.576768
3515.758162	1091825.138591	42.581773
3515.584818	1091529.358867	42.586778
3515.497374	1091204.434793	42.591783
3515.501587	1090907.346900	42.596788
3515.588070	1090616.359156	42.601792
3515.865351	1090305.305131	42.606797
3515.610374	1089976.312099	42.611802
3515.410701	1089670.089825	42.616807
3515.333840	1089376.859205	42.621812
3515.391844	1089062.991854	42.626816
3515.140751	1088761.133955	42.631821
3515.088019	1088459.130790	42.636826
3515.131261	1088145.404491	42.641831
3515.158318	1087854.566003	42.646836
3514.775423	1087555.633534	42.651840
3515.363176	1087246.174040	42.656845
3514.843482	1086958.061149	42.661850
3514.768561	1086639.666828	42.666855
3515.129839	1086356.936328	42.671860
3514.840900	1086048.032326	42.676864
3514.839619	1085758.620155	42.681869
3514.624895	1085446.122690	42.686874
3514.938981	1085160.365755	42.691879
3514.767008	1084867.099200	42.696884
3514.762507	1084570.145544	42.701888
3514.865502	1084279.966344	42.706893
3514.709352	1083995.088715	42.711898
3514.635593	1083678.534738	42.716903
3514.535536	1083393.328676	42.721908
3514.722385	1083100.962861	42.726912
3514.441177	1082808.466607	42.731917
3514.111977	1082530.830654	42.736922
3514.713976	1082231.155552	42.741927
3514.252985	1081964.927934	42.746932
3514.562041	1081663.255265	42.751936
3514.153069	1081379.337775	42.756941
3514.290836	1081088.119312	42.761946
3514.230101	1080792.696027	42.766951
3514.190988	1080526.616525	42.771956
3514.054158	1080226.856990	42.776960
3514.112817	1079952.864368	42.781965
3514.146043	1079670.992357	42.786970
3513.984306	1079383.475165	42.791975
3514.168412	1079098.861352	42.796980
3513.729241	1078828.349657	42.801985
3514.140162	1078544.917453	42.806989
3513.722924	1078283.014499	42.811994
3513.878500	1077984.427574	42.816999
3514.185064	1077702.216861	42.822004
3513.707503	1077406.198806	42.827009
3513.913614	1077128.775672	42.832013
3513.845726	1076865.114854	42.837018
3514.091063	1076577.286790	42.842023
3513.990767	1076315.333281	42.847028
3513.786570	1076023.516723	42.852033
3514.054253	1075745.629080	42.857037
3513.862205	1075468.091173	42.862042
3513.830558	1075189.071972	42.867047
3513.838052	1074919.061449	42.872052
3513.581701	1074641.876416	42.877057
3513.645885	1074380.763723	42.882061
3513.717948	1074098.885890	42.887066
3513.838169	1073808.434803	42.892071
3513.665319	1073544.631100	42.897076
3513.521815	1073266.108705	42.902081
3513.476629	1072996.492386	42.907085
3513.283776	1072720.833087	42.912090
3513.485034	1072457.299735	42.917095
3513.631117	1072186.170502	42.922100
3513.441212	1071914.218194	42.927105
3513.334252	1071640.797000	42.932109
3513.126954	1071365.456293	42.937114
3513.152737	1071106.308319	42.942119
3513.523204	1070820.752059	42.947124
3512.966499	1070574.075461	42.952129
3513.213931	1070302.355623	42.957133
3512.948262	1070029.168538	42.962138
3512.775651	1069778.739441	42.967143
3513.356285	1069503.559981	42.972148
3513.237956	1069256.848032	42.977153
3513.139893	1068986.946872	42.982157
3512.992204	1068725.887848	42.987162
3513.263845	1068462.920099	42.992167
3513.158536	1068194.519859	42.997172
3513.078613	1067943.222261	43.002177
3513.197077	1067671.778031	43.007181
3512.684800	1067400.616634	43.012186
3512.610677	1067148.704557	43.017191
3513.124748	1066888.411034	43.022196
3512.799414	1066632.091519	43.027201
3512.870387	1066373.770625	43.032205
3512.648846	1066112.503200	43.037210
3512.835141	1065860.200473	43.042215
3512.974146	1065583.453936	43.047220
3512.622908	1065318.994834	43.052225
3513.024021	1065080.477352	43.057229
3512.507415	1064831.899884	43.062234
3512.642576	1064548.557940	43.067239
3512.906068	1064292.705917	43.072244
3512.323184	1064052.381012	43.077249
3512.711130	1063787.726456	43.082253
3512.532802	1063535.184517	43.087258
3512.365137	1063289.367486	43.092263
3512.310271	1063019.069471	43.097268
3512.295900	1062785.141577	43.102273
3512.303865	1062519.333329	43.107277
3512.290311	1062269.786913	43.112282
3512.466960	1062032.425793	43.117287
3512.369137	1061799.432556	43.122292
3512.137247	1061542.089844	43.127297
3512.330115	1061277.539230	43.132301
3512.096776	1061036.447128	43.137306
3512.105340	1060805.031373	43.142311
3512.298965	1060542.275087	43.147316
3512.070459	1060310.203416	43.152321
3512.466603	1060066.461020	43.157325
3512.294224	1059808.834835	43.162330
3511.964031	1059572.318008	43.167335
3512.308875	1059319.689030	43.172340
3511.732397	1059085.696456	43.177345
3512.087434	1058823.505934	43.182349
3511.834634	1058594.256123	43.187354
3511.889068	1058362.633844	43.192359
3512.076942	1058101.399978	43.197364
3511.923649	1057859.962912	43.202369
3512.169835	1057625.098320	43.207373
3511.782685	1057367.682431	43.212378
3511.853333	1057128.489196	43.217383
3511.943839	1056910.195182	43.222388
3511.949743	1056654.705094	43.227393
3511.866816	1056403.073058	43.232397
3511.567659	1056162.356732	43.237402
3511.641924	1055942.195762	43.242407
3511.568482	1055706.916580	43.247412
3511.247573	1055478.897939	43.252417
3511.443952	1055223.406597	43.257421
3511.409028	1055004.286617	43.262426
3511.340465	1054766.845629	43.267431
3511.455213	1054532.738729	43.272436
3511.289694	1054322.579695	43.277441
3511.564149	1054075.603550	43.282445
3511.281052	1053854.357524	43.287450
3511.597099	1053629.339625	43.292455
3511.329944	1053375.767737	43.297460
3511.286327	1053150.210956	43.302465
3511.352924	1052927.616518	43.307469
3510.989426	1052707.591543	43.312474
3511.244160	1052481.668998	43.317479
3511.300321	1052252.008229	43.322484
3511.126949	1052028.259646	43.327489
3511.337581	1051790.065962	43.332493
3510.896509	1051583.320719	43.337498
3510.804211	1051336.089609	43.342503
3510.717502	1051122.226459	43.347508
3510.616646	1050904.305323	43.352513
3511.004931	1050677.032844	43.357517
3510.961887	1050475.776540	43.362522
3510.945714	1050242.956728	43.367527
3510.994944	1050018.897194	43.372532
3510.765375	1049811.664899	43.377537
3511.117691	1049572.869923	43.382541
3510.857057	1049350.281861	43.387546
3510.616627	1049144.473934	43.392551
3510.700974	1048939.763002	43.397556
3510.714886	1048710.058626	43.402561
3510.609143	1048493.008478	43.407565
3510.009833	1048256.726450	43.412570
3510.647583	1048043.011056	43.417575
3510.778335	1047848.387483	43.422580
3510.611952	1047633.340771	43.427585
3510.528929	1047424.353875	43.432589
3510.258537	1047209.693997	43.437594
3510.210689	1046987.941323	43.442599
3510.533229	1046799.814426	43.447604
3510.506767	1046575.724564	43.452609
3510.845872	1046354.655247	43.457613
3510.529627	1046146.720698	43.462618
3510.614724	1045940.546960	43.467623
3510.629353	1045711.394069	43.472628
3510.319832	1045509.614849	43.477633
3510.193534	1045286.455026	43.482637
3510.427691	1045068.828439	43.487642
3510.254730	1044874.536773	43.492647
3510.274672	1044660.213238	43.497652
3509.965525	1044465.060381	43.502657
3510.339644	1044232.116759	43.507661
3509.726207	1044037.192151	43.512666
3509.678038	1043830.961937	43.517671
3509.901659	1043641.391788	43.522676
3510.067970	1043434.725113	43.527681
3510.541488	1043228.966259	43.532685
3510.231795	1043014.053769	43.537690
3510.094891	1042806.640737	43.542695
3510.339194	1042605.340974	43.547700
3509.975768	1042393.408581	43.552705
3509.866772	1042185.871136	43.557709
3509.852249	1041998.603224	43.562714
3510.108785	1041795.436079	43.567719
3510.001295	1041579.081834	43.572724
3509.543714	1041392.156366	43.577729
3510.055772	1041184.865806	43.582733
3510.157319	1041000.831129	43.587738
3509.719727	1040788.849716	43.592743
3509.971619	1040586.509019	43.597748
3509.959858	1040399.960025	43.602753
3509.892016	1040174.845143	43.607757
3509.668683	1039983.677143	43.612762
3509.671595	1039796.138794	43.617767
3509.731543	1039587.219731	43.622772
3509.302218	1039403.896337	43.627777
3509.858833	1039204.258804	43.632781
3509.469033	1039027.394111	43.637786
3509.628682	1038813.498673	43.642791
3509.802427	1038627.923238	43.647796
3509.421985	1038439.822144	43.652801
3509.776947	1038224.131385	43.657805
3509.638926	1038050.771993	43.662810
3509.409954	1037857.694510	43.667815
3509.586142	1037646.846044	43.672820
3509.544178	1037474.033113	43.677825
3509.540838	1037259.040949	43.682829
3509.587495	1037066.664346	43.687834
3509.616041	1036879.507038	43.692839
3509.224289	1036681.095864	43.697844
3509.143895	1036502.455606	43.702849
3509.270979	1036311.103659	43.707853
3509.616564	1036116.807114	43.712858
3509.207401	1035935.300771	43.717863
3509.446109	1035738.880416	43.722868
3509.322664	1035534.289484	43.727873
3509.409557	1035354.810907	43.732877
3509.287158	1035160.074339	43.737882
3509.217537	1034983.415364	43.742887
3509.471975	1034789.958358	43.747892
3509.416276	1034588.611306	43.752897
3509.663851	1034393.787027	43.757901
3509.653877	1034227.738372	43.762906
3509.337019	1034023.704439	43.767911
3509.677022	1033826.425839	43.772916
3509.022755	1033628.045907	43.777921
3509.256283	1033455.159682	43.782925
3509.290064	1033270.203000	43.787930
3509.437236	1033083.382551	43.792935
3509.388799	1032876.262008	43.797940
3508.883144	1032703.377436	43.802945
3509.464112	1032521.403211	43.807949
3509.667268	1032340.937286	43.812954
3509.427292	1032128.593318	43.817959
3509.349655	1031929.767575	43.822964
3508.894843	1031756.651667	43.827969
3509.113354	1031565.993060	43.832973
3509.261164	1031388.990761	43.837978
3509.178833	1031220.153612	43.842983
3509.311341	1031023.197356	43.847988
3508.821874	1030825.465154	43.852993
3509.004254	1030658.503951	43.857997
3509.067434	1030478.678682	43.863002
3508.636489	1030286.727704	43.868007
3508.955018	1030127.862420	43.873012
3508.929665	1029927.601012	43.878017
3508.817438	1029736.740740	43.883021
3508.875027	1029580.420848	43.888026
3508.702584	1029392.561025	43.893031
3509.170327	1029213.500060	43.898036
3508.828338	1029046.577047	43.903041
3508.748874	1028847.254398	43.908045
3508.767150	1028679.583059	43.913050
3508.631718	1028496.433330	43.918055
3508.719647	1028322.249717	43.923060
3508.752217	1028160.372640	43.928065
3508.867724	1027959.436258	43.933069
3508.506425	1027799.551128	43.938074
3508.616748	1027618.560375	43.943079
3508.667197	1027454.431629	43.948084
3508.344815	1027279.701808	43.953089
3508.788394	1027114.045006	43.958093
3508.922948	1026915.296463	43.963098
3508.698049	1026753.324168	43.968103
3508.625442	1026565.837376	43.973108
3508.560922	1026399.758614	43.978113
3508.774537	1026235.470328	43.983117
3508.572453	1026045.467867	43.988122
3508.378154	1025871.448229	43.993127
3508.446359	1025703.291776	43.998132
3508.080606	1025535.783254	44.003137
3508.370531	1025376.787692	44.008141
3508.318565	1025207.376164	44.013146
3508.163094	1025048.056929	44.018151
3508.253662	1024868.240509	44.023156
3507.893711	1024712.531801	44.028161
3508.155739	1024539.267976	44.033165
3508.010535	1024386.616767	44.038170
3507.921568	1024216.405843	44.043175
3508.131955	1024033.149940	44.048180
3507.724680	1023892.937274	44.053185
3508.228526	1023738.901207	44.058189
3507.888160	1023577.049889	44.063194
3507.653263	1023407.032308	44.068199
3508.141080	1023245.907615	44.073204
3507.930254	1023083.535914	44.078209
3508.101072	1022934.089728	44.083213
3507.799913	1022768.717922	44.088218
3507.800594	1022614.636870	44.093223
3507.896372	1022470.717903	44.098228
3507.736370	1022303.563639	44.103233
3507.815170	1022149.747865	44.108237
3507.993496	1021986.310512	44.113242
3507.696407	1021829.153566	44.118247
3508.075931	1021656.945065	44.123252
3507.769430	1021506.860555	44.128257
3507.632738	1021366.152124	44.133261
3507.889356	1021196.180498	44.138266
3507.663579	1021051.890105	44.143271
3507.912608	1020893.744033	44.148276
3507.703736	1020726.453801	44.153281
3507.919434	1020566.848986	44.158285
3507.934550	1020401.355247	44.163290
3507.888923	1020253.716413	44.168295
3507.991562	1020098.094278	44.173300
3507.741945	1019937.966143	44.178305
3508.139939	1019782.868714	44.183309
3508.033109	1019623.387211	44.188314
3507.680095	1019454.239396	44.193319
3507.877463	1019313.909586	44.198324
3507.668628	1019150.162300	44.203329
3507.548682	1018998.136387	44.208333
3507.739551	1018843.144149	44.213338
3507.578140	1018673.553113	44.218343
3507.773547	1018528.352153	44.223348
3507.391742	1018385.183345	44.228353
3507.545247	1018231.247836	44.233357
3507.528399	1018091.310937	44.238362
3507.487967	1017927.306155	44.243367
3507.550308	1017774.246587	44.248372
3507.199496	1017638.041389	44.253377
3507.377694	1017478.063781	44.258381
3507.442470	1017346.150642	44.263386
3507.436242	1017179.012470	44.268391
3507.619940	1017037.172094	44.273396
3507.079318	1016883.993453	44.278401
3507.130568	1016743.817640	44.283405
3507.300181	1016610.899275	44.288410
3507.162424	1016455.798230	44.293415
3507.466097	1016308.968887	44.298420
3507.502971	1016162.470895	44.303425
3507.293890	1016020.669564	44.308429
3507.381817	1015866.097574	44.313434
3507.296168	1015721.258716	44.318439
3507.379163	1015593.767492	44.323444
3507.168950	1015438.650318	44.328449
3507.222436	1015290.185009	44.333453
3506.816278	1015150.918675	44.338458
3507.180159	1015005.016354	44.343463
3507.018314	1014862.886742	44.348468
3506.987959	1014726.752393	44.353473
3507.061198	1014582.343559	44.358477
3507.092913	1014454.446529	44.363482
3506.774465	1014323.788019	44.368487
3507.092001	1014156.603782	44.373492
3506.846525	1014035.638035	44.378497
3506.685885	1013883.189069	44.383501
3506.791150	1013742.541070	44.388506
3506.539191	1013615.060172	44.393511
3506.898629	1013489.612467	44.398516
3506.653128	1013366.398430	44.403521
3506.723772	1013217.098567	44.408525
3506.614364	1013083.754290	44.413530
3506.604096	1012936.791520	44.418535
3506.923726	1012807.935433	44.423540
3506.499293	1012692.118596	44.428545
3506.798725	1012554.323139	44.433549
3506.698148	1012420.670277	44.438554
3506.634907	1012300.705815	44.443559
3506.766683	1012152.241974	44.448564
3506.616280	1012014.021644	44.453569
3506.571997	1011878.403605	44.458573
3506.604004	1011745.490117	44.463578
3506.658154	1011617.913573	44.468583
3506.578700	1011511.731486	44.473588
3506.820997	1011371.293177	44.478593
3506.735222	1011242.662392	44.483597
3506.739579	1011093.802988	44.488602
3506.465562	1010971.318571	44.493607
3506.825195	1010832.499399	44.498612
3506.600291	1010709.126644	44.503617
3506.418059	1010575.346273	44.508621
3506.477885	1010456.488390	44.513626
3506.494982	1010307.606123	44.518631
3506.741391	1010166.165304	44.523636
3506.581600	1010054.915446	44.528641
3506.521036	1009929.263284	44.533645
3506.791262	1009795.195501	44.538650
3506.560202	1009667.427403	44.543655
3506.813257	1009520.818115	44.548660
3506.237519	1009404.861390	44.553665
3506.609454	1009282.039475	44.558669
3506.685602	1009151.195915	44.563674
3506.695905	1009025.025927	44.568679
3506.930826	1008885.304544	44.573684
3506.681784	1008756.352295	44.578689
3506.768162	1008621.120398	44.583693
3506.661711	1008494.082873	44.588698
3506.392850	1008364.444441	44.593703
3506.561702	1008226.467491	44.598708
3506.073932	1008107.941952	44.603713
3506.363258	1007966.827800	44.608717
3505.975088	1007853.919365	44.613722
3505.933206	1007730.354053	44.618727
3506.556124	1007615.135350	44.623732
3506.204728	1007488.990586	44.628737
3506.188274	1007384.081593	44.633741
3506.544456	1007250.814288	44.638746
3506.311110	1007123.572341	44.643751
3506.412594	1007008.913337	44.648756
3506.295560	1006870.464141	44.653761
3506.383141	1006760.858890	44.658765
3506.565019	1006638.108000	44.663770
3506.288209	1006516.596948	44.668775
3506.392832	1006374.306463	44.673780
3506.174892	1006245.291700	44.678785
3506.234382	1006112.240904	44.683789
3506.504624	1006011.149322	44.688794
3506.579079	1005889.080636	44.693799
3506.580211	1005744.457158	44.698804
3506.206519	1005617.787947	44.703809
3506.271231	1005504.271601	44.708813
3506.432541	1005383.928447	44.713818
3506.411091	1005254.566893	44.718823
3506.456481	1005123.926852	44.723828
3506.323592	1005020.938547	44.728833
3506.193390	1004886.431044	44.733837
3506.333830	1004749.346564	44.738842
3506.140960	1004633.325947	44.743847
3506.346040	1004511.692389	44.748852
3506.249896	1004396.818358	44.753857
3506.310537	1004259.735150	44.758861
3506.333931	1004139.874654	44.763866
3506.165914	1004018.875670	44.768871
3506.682456	1003887.059261	44.773876
3506.107717	1003776.143113	44.778881
3506.094919	1003642.170425	44.783885
3506.405725	1003538.109062	44.788890
3506.263732	1003413.298216	44.793895
3506.223083	1003281.656774	44.798900
3505.951382	1003179.533497	44.803905
3506.322534	1003042.856169	44.808909
3506.603394	1002918.159364	44.813914
3506.216344	1002798.338037	44.818919
3506.483219	1002644.833529	44.823924
3506.330818	1002550.172346	44.828929
3506.456685	1002429.285573	44.833933
3506.490539	1002299.458024	44.838938
3506.214608	1002185.444551	44.843943
3506.459370	1002046.817568	44.848948
3506.434076	1001919.034825	44.853953
3506.048006	1001802.306652	44.858957
3506.244896	1001673.800485	44.863962
3506.198782	1001561.877850	44.868967
3506.169525	1001443.039529	44.873972
3506.046082	1001325.090249	44.878977
3506.209208	1001188.597086	44.883981
3506.212553	1001075.585970	44.888986
3506.259126	1000962.760164	44.893991
3506.409238	1000823.437423	44.898996
3506.388862	1000705.847644	44.904001
3506.123639	1000584.109763	44.909005
3506.544447	1000463.035078	44.914010
3506.014202	1000349.415899	44.919015
3505.865017	1000225.704146	44.924020
3506.291254	1000097.708569	44.929025
3506.367894	999986.708149	44.934029
3506.107930	999871.379757	44.939034
3506.023891	999747.646833	44.944039
3505.969382	999633.740207	44.949044
3505.743040	999516.159650	44.954049
3506.035427	999387.391143	44.959053
3505.830171	999286.549816	44.964058
3505.519000	999168.099667	44.969063
3505.615980	999064.186041	44.974068
3505.544704	998946.275991	44.979073
3505.895254	998843.095563	44.984077
3505.861404	998730.238534	44.989082
3505.638218	998616.047090	44.994087
3505.659119	998504.539903	44.999092
3505.568364	998404.053546	45.004097
3505.659143	998290.582921	45.009101
3505.850307	998172.710942	45.014106
3505.815786	998072.306834	45.019111
3506.190571	997949.725174	45.024116
3506.165518	997833.342663	45.029121
3506.001696	997727.889166	45.034125
3505.724386	997603.556871	45.039130
3506.055937	997492.563017	45.044135
3505.663669	997388.504456	45.049140
3505.887924	997268.854982	45.054145
3505.816419	997146.719099	45.059149
3506.008624	997041.973468	45.064154
3505.776089	996940.315607	45.069159
3505.854689	996808.698831	45.074164
3505.627604	996683.753613	45.079169
3505.629524	996576.497924	45.084173
3505.755428	996480.715249	45.089178
3505.486284	996370.480318	45.094183
3505.785116	996266.579602	45.099188
3505.837082	996159.307785	45.104193
3505.606770	996028.795468	45.109197
3505.474974	995927.102853	45.114202
3505.280328	995825.223908	45.119207
3505.423390	995714.226320	45.124212
3505.532058	995615.801217	45.129217
3505.601507	995488.247546	45.134221
3505.163093	995390.395822	45.139226
3505.204342	995292.171088	45.144231
3505.197055	995180.895518	45.149236
3505.550799	995095.088390	45.154241
3505.495564	994977.385498	45.159245
3505.622457	994887.617359	45.164250
3505.341995	994767.413601	45.169255
3505.154849	994665.610051	45.174260
3505.309323	994573.591050	45.179265
3505.350033	994445.141613	45.184269
3505.425799	994368.140146	45.189274
3505.114832	994277.167555	45.194279
3505.354567	994161.835597	45.199284
3505.150589	994056.125535	45.204289
3505.224582	993959.919039	45.209293
3505.370634	993840.794962	45.214298
3505.179287	993743.069066	45.219303
3505.324806	993664.292181	45.224308
3505.322157	993547.623135	45.229313
3505.029141	993438.602282	45.234317
3505.271450	993339.628365	45.239322
3505.196102	993270.044845	45.244327
3505.365136	993151.389903	45.249332
3505.255824	993065.628401	45.254337
3505.120315	992947.019351	45.259341
3504.985547	992859.309332	45.264346
3505.077901	992761.422340	45.269351
3504.922360	992648.659332	45.274356
3505.092473	992563.331651	45.279361
3505.090719	992457.071091	45.284365
3505.113564	992371.374832	45.289370
3504.890601	992275.481197	45.294375
3505.064156	992198.336730	45.299380
3505.006121	992088.471324	45.304385
3504.967076	991992.640120	45.309389
3505.087821	991888.006181	45.314394
3504.838817	991788.111198	45.319399
3505.045760	991703.837050	45.324404
3504.891657	991609.480854	45.329409
3504.726282	991529.263049	45.334413
3504.742493	991431.073182	45.339418
3504.624953	991337.193972	45.344423
3505.134070	991246.330285	45.349428
3504.846799	991148.868093	45.354433
3504.781302	991065.994517	45.359437
3504.982055	990967.571230	45.364442
3504.904833	990886.452215	45.369447
3505.005845	990797.013783	45.374452
3504.723136	990688.718602	45.379457
3504.822934	990584.454209	45.384461
3504.926731	990501.251960	45.389466
3504.818196	990400.919382	45.394471
3504.931188	990319.468382	45.399476
3504.855106	990241.850876	45.404481
3504.697263	990139.766343	45.409485
3504.771382	990036.178829	45.414490
3504.449004	989954.989378	45.419495
3504.965905	989885.657008	45.424500
3504.843045	989782.194848	45.429505
3504.714074	989675.903275	45.434509
3504.826403	989594.149398	45.439514
3504.676484	989498.684583	45.444519
3504.731049	989401.526299	45.449524
3504.847745	989335.374444	45.454529
3504.742215	989239.312718	45.459533
3504.884174	989154.816441	45.464538
3504.435861	989064.465811	45.469543
3504.718068	988989.991246	45.474548
3504.649445	988900.746051	45.479553
3504.696215	988812.455957	45.484557
3504.753633	988714.895285	45.489562
3504.733336	988642.612151	45.494567
3504.907504	988544.931785	45.499572
3504.769003	988468.763706	45.504577
3504.911356	988363.085826	45.509581
3505.146258	988264.219945	45.514586
3505.048521	988187.065784	45.519591
3504.878287	988066.506989	45.524596
3504.546924	987995.340071	45.529601
3504.898487	987915.766683	45.534605
3505.075502	987815.731763	45.539610
3504.904769	987741.022773	45.544615
3504.645634	987632.958252	45.549620
3504.611215	987531.099314	45.554625
3504.454313	987450.139584	45.559629
3504.608012	987369.420272	45.564634
3504.681593	987283.639023	45.569639
3504.973213	987200.455183	45.574644
3504.823402	987109.731621	45.579649
3504.709274	987022.123337	45.584653
3504.773214	986935.265039	45.589658
3504.659980	986857.412340	45.594663
3504.583147	986755.448938	45.599668
3504.586433	986666.059296	45.604673
3504.610078	986597.451291	45.609677
3504.470644	986483.489934	45.614682
3504.386213	986422.119308	45.619687
3504.774043	986312.752086	45.624692
3504.221402	986238.671853	45.629697
3504.579624	986174.493004	45.634701
3504.830902	986076.952826	45.639706
3504.535601	985991.993676	45.644711
3504.303762	985917.075630	45.649716
3504.499848	985833.887592	45.654721
3504.258456	985766.582060	45.659725
3504.684021	985673.886419	45.664730
3504.277051	985598.016981	45.669735
3504.564210	985510.807400	45.674740
3504.075758	985427.042924	45.679745
3504.102929	985343.289900	45.684749
3504.303681	985268.389689	45.689754
3504.314167	985187.370239	45.694759
3504.615219	985115.379879	45.699764
3504.683917	985034.055823	45.704769
3504.177591	984958.096614	45.709773
3504.273129	984863.880309	45.714778
3504.386975	984791.916703	45.719783
3504.751151	984717.079959	45.724788
3504.485084	984622.138255	45.729793
3504.215281	984548.868059	45.734797
3504.712664	984474.787190	45.739802
3504.589590	984370.348125	45.744807
3504.287433	984279.116464	45.749812
3504.137986	984215.292086	45.754817
3504.409284	984103.753873	45.759821
3504.278883	983983.297391	45.764826
3504.113935	983789.714738	45.769831
3504.374546	983505.835468	45.774836
3504.025632	983183.862656	45.779841
3504.392026	982803.748024	45.784845
3504.376597	982359.117407	45.789850
3504.459981	981837.960848	45.794855
3504.217186	981260.449494	45.799860
3503.944485	980610.300790	45.804865
3503.729079	979862.561217	45.809869
3503.863541	979073.527431	45.814874
3503.695240	978224.036795	45.819879
3503.507082	977285.375812	45.824884
3503.519911	976300.969697	45.829889
3503.359273	975216.391753	45.834893
3503.292401	974061.957914	45.839898
3503.097292	972820.837016	45.844903
3502.969646	971500.377058	45.849908
3503.070075	970111.752130	45.854913
3502.730693	968627.906137	45.859917
3502.950669	967093.449228	45.864922
3502.583161	965439.867945	45.869927
3501.893066	963693.176870	45.874932
3501.841362	961903.216712	45.879937
3501.578970	959981.948225	45.884941
3501.447808	958004.311288	45.889946
3501.091050	955933.319780	45.894951
3500.789883	953824.842063	45.899956
3500.661592	951647.535593	45.904961
3499.818984	949363.342709	45.909965
3500.178800	947021.521726	45.914970
3499.388754	944578.689345	45.919975
3498.977348	942054.206912	45.924980
3499.092615	939440.359929	45.929985
3498.519505	936767.932972	45.934989
3498.543042	933977.867105	45.939994
3497.389164	931125.712056	45.944999
3497.266113	928182.463436	45.950004
3496.454306	925144.032368	45.955009
3496.055737	922036.840588	45.960013
3496.408873	918826.926878	45.965018
3495.227639	915553.617644	45.970023
3495.138427	912159.787329	45.975028
3494.619116	908733.653339	45.980033
3493.701426	905184.717246	45.985037
3493.502681	901574.494265	45.990042
3492.605906	897873.154701	45.995047
3492.308268	894084.290845	46.000052
3491.653082	890226.102291	46.005057
3490.992031	886269.745232	46.010061
3490.558677	882226.827295	46.015066
3490.050703	878112.179015	46.020071
3489.256665	873911.734842	46.025076
3488.741434	869609.998440	46.030081
3487.974555	865252.646650	46.035085
3487.226457	860786.924516	46.040090
3486.738316	856245.194319	46.045095
3486.199936	851612.469064	46.050100
3485.308491	846891.360106	46.055105
3484.364998	842108.483552	46.060109
3483.877321	837200.048286	46.065114
3482.691594	832235.173229	46.070119
3482.203509	827196.967063	46.075124
3481.527298	822054.674696	46.080129
3480.544686	816843.522379	46.085133
3479.723413	811514.756127	46.090138
3478.572310	806130.467121	46.095143
3477.871202	800654.863449	46.100148
3476.708492	795095.842308	46.105153
3475.771378	789461.604592	46.110157
3475.440593	783720.824030	46.115162
3474.229825	777915.159737	46.120167
3473.517090	772004.771504	46.125172
3472.335116	766018.731838	46.130177
3471.350521	759942.109507	46.135181
3470.776169	753768.696968	46.140186
3469.246255	747538.703986	46.145191
3468.494448	741192.858971	46.150196
3467.222108	734781.634866	46.155201
3466.092870	728295.481963	46.160205
3465.225621	721686.774714	46.165210
3463.782917	714985.674471	46.170215
3462.751152	708232.722129	46.175220
3461.768882	701390.316091	46.180225
3460.619908	694455.094518	46.185229
3459.335124	687440.328293	46.190234
3458.175204	680329.647867	46.195239
3456.978008	673136.029294	46.200244
3455.591201	665881.773803	46.205249
3454.164867	658514.090952	46.210253
3453.520068	651076.587114	46.215258
3451.670958	643562.999837	46.220263
3450.567730	635924.608528	46.225268
3448.730734	628249.116757	46.230273
3447.417059	620486.790654	46.235277
3446.031742	612638.877917	46.240282
3444.655777	604711.543689	46.245287
3443.151158	596698.906624	46.250292
3441.843622	588602.337500	46.255297
3440.168402	580425.778297	46.260301
3438.990100	572174.864637	46.265306
3436.969623	563836.176109	46.270311
3435.252919	555423.521536	46.275316
3433.606247	546934.186934	46.280321
3432.188975	538356.967025	46.285325
3430.668428	529707.324192	46.290330
3428.732256	520984.999975	46.295335
3426.984283	512170.384429	46.300340
3425.052634	503305.132966	46.305345
3423.158312	494347.262147	46.310349
3421.592114	485332.251331	46.315354
3419.449730	476242.472803	46.320359
3417.482054	467057.059024	46.325364
3415.347016	457820.537846	46.330369
3413.176639	448501.471757	46.335373
3411.143125	439134.330645	46.340378
3408.919943	429671.703024	46.345383
3407.250299	420175.135178	46.350388
3405.031012	410571.404874	46.355393
3402.542844	400936.235267	46.360397
3400.520509	391210.909976	46.365402
3397.987318	381446.630206	46.370407
3395.410934	371599.139151	46.375412
3392.972259	361708.205365	46.380417
3390.265711	351771.913801	46.385421
3388.104319	341745.933987	46.390426
3385.567109	331717.760617	46.395431
3382.665428	321585.886904	46.400436
3380.081867	311406.877004	46.405441
3377.493157	301220.364388	46.410445
3374.841710	290948.104576	46.415450
3371.819971	280635.697220	46.420455
3368.852313	270288.834304	46.425460
3366.259169	259892.219961	46.430465
3362.763179	249451.711639	46.435469
3359.546956	238955.705680	46.440474
3356.119895	228473.786507	46.445479
3352.706951	217821.975417	46.450484
3349.170770	207260.349951	46.455489
3345.075732	196654.552740	46.460493
3341.892382	186056.980933	46.465498
3338.192912	175419.557191	46.470503
3333.498384	164787.594622	46.475508
3329.719710	154126.495529	46.480513
3325.084130	143487.495572	46.485517
3320.790791	132867.473578	46.490522
3315.613620	122243.205211	46.495527
3310.299315	111623.937962	46.500532
3304.516214	101059.501366	46.505537
3297.783962	90523.767467	46.510541
3290.538809	80078.490545	46.515546
3280.181160	69745.776568	46.520551
3262.068671	59739.375752	46.525556
3230.001890	50336.707933	46.530561
3188.248313	41579.181850	46.535565
3142.055054	33558.567372	46.540570
3095.196499	26362.487393	46.545575
3050.689789	20020.606016	46.550580
3011.637245	14534.784195	46.555585
2977.179072	9948.244302	46.560589
2947.465587	6148.843438	46.565594
2922.074957	3138.365668	46.570599
2897.489216	895.283105	46.575604
2838.763829	342.448821	46.580609
2794.307764	345.375569	46.585613
2787.367514	332.943075	46.590618
2804.824597	324.562078	46.595623
2831.743040	308.940693	46.600628
2856.794542	312.383734	46.605633
2872.911496	308.917743	46.610637
2879.829386	304.220241	46.615642
2880.072738	307.620689	46.620647
2875.800661	285.177939	46.625652
2871.112128	306.609901	46.630657
2865.922685	300.276298	46.635661
2862.411370	310.502559	46.640666
2859.547455	295.743245	46.645671
2857.498106	305.698797	46.650676
2855.710324	301.275830	46.655681
2853.254870	304.823263	46.660685
2850.850460	291.292670	46.665690
2848.104627	284.527240	46.670695
2845.618739	290.514497	46.675700
2842.601940	282.193226	46.680705
2839.339102	295.370214	46.685709
2836.042957	272.760112	46.690714
2833.087808	284.857142	46.695719
2829.951545	269.917449	46.700724
2826.839656	282.226276	46.705729
2823.657700	276.792927	46.710733
2820.953755	277.417755	46.715738
2817.489073	271.459142	46.720743
2814.326941	280.849280	46.725748
2810.951363	265.985359	46.730753
2807.332550	288.733750	46.735757
2804.853043	272.224673	46.740762
2801.372830	284.884857	46.745767
2797.886626	270.211718	46.750772
2794.449294	273.583650	46.755777
2791.328790	268.827095	46.760781
2788.328368	262.625437	46.765786
2784.753319	263.839794	46.770791
2781.486816	267.837030	46.775796
2778.608985	266.756258	46.780801
2774.745945	268.182057	46.785805
2771.624436	259.758431	46.790810
2768.171778	269.546291	46.795815
2764.652266	260.024699	46.800820
2761.326363	264.830708	46.805825
2757.637879	260.239532	46.810829
2754.623331	260.669753	46.815834
2751.329620	258.655266	46.820839
2747.703375	263.059864	46.825844
2744.409030	260.564659	46.830849
2741.012965	251.528812	46.835853
2737.559948	251.343143	46.840858
2734.462649	262.959019	46.845863
2730.925377	253.392039	46.850868
2727.971466	250.740388	46.855873
2723.966233	260.340673	46.860877
2720.130641	254.777892	46.865882
2716.624082	249.032917	46.870887
2713.440951	262.842242	46.875892
2710.613568	255.482838	46.880897
2706.886892	235.399477	46.885901
2703.392830	244.174122	46.890906
2700.163241	257.108676	46.895911
2696.648407	245.891836	46.900916
2693.236164	257.876512	46.905921
2689.314495	249.562861	46.910925
2685.827144	243.386001	46.915930
2682.676053	241.453785	46.920935
2679.987166	252.854453	46.925940
2676.273512	225.383300	46.930945
2671.963184	235.797746	46.935949
2669.082575	244.430713	46.940954
2665.665732	240.783579	46.945959
2662.166589	230.513005	46.950964
2658.421673	242.102586	46.955969
2654.294272	245.107328	46.960973
2651.879849	236.210470	46.965978
2648.559388	248.397050	46.970983
2644.655077	232.609665	46.975988
2641.234052	224.131137	46.980993
2637.718578	240.421865	46.985997
2634.159902	224.107140	46.991002
2630.996649	223.743820	46.996007
2627.595952	214.991059	47.001012
2624.323759	236.146867	47.006017
2620.205374	240.148088	47.011021
2617.006204	222.584571	47.016026
2613.542889	241.167037	47.021031
2610.180396	225.983462	47.026036
2607.364174	219.522763	47.031041
2603.390577	239.655215	47.036045
2600.207287	215.805751	47.041050
2596.022698	235.248699	47.046055
2592.323677	244.510379	47.051060
2589.483604	229.614360	47.056065
2585.610014	228.284511	47.061069
2582.315433	221.893129	47.066074
2579.012666	226.209824	47.071079
2575.321757	231.867553	47.076084
2572.030319	217.988684	47.081089
2568.168326	233.742392	47.086093
2564.731543	223.196719	47.091098
2561.362362	223.431664	47.096103
2557.954702	217.157592	47.101108
2554.838642	226.539984	47.106113
2551.175934	226.318343	47.111117
2547.687776	235.827800	47.116122
2544.097934	235.679183	47.121127
2540.652027	219.287133	47.126132
2537.080252	222.105212	47.131137
2533.498594	213.832286	47.136141
2529.982368	204.631327	47.141146
2526.942561	223.284930	47.146151
2523.570970	217.741254	47.151156
2519.545890	225.131953	47.156161
2516.089116	216.324473	47.161165
2512.502483	219.838820	47.166170
2509.227223	229.686671	47.171175
2505.596447	212.230116	47.176180
2502.213847	207.826300	47.181185
2498.671871	220.137428	47.186189
2495.384994	225.674305	47.191194
2491.720395	223.097235	47.196199
2488.553604	203.676812	47.201204
2485.084881	208.652365	47.206209
2481.193343	204.226141	47.211213
2477.949650	217.038455	47.216218
2474.347753	219.913517	47.221223
2470.834780	220.332618	47.226228
2467.348924	214.182570	47.231233
2463.953386	218.841040	47.236237
2460.598451	211.957053	47.241242
2456.897617	208.863132	47.246247
2453.544028	216.974843	47.251252
2450.202617	193.282795	47.256257
2446.429218	195.094190	47.261261
2443.070026	222.504573	47.266266
2439.204545	214.407637	47.271271
2435.790609	217.263754	47.276276
2432.444726	213.540324	47.281281
2428.992076	210.868060	47.286285
2425.779591	214.755494	47.291290
2421.978576	206.683159	47.296295
2418.096274	210.319601	47.301300
2415.044749	195.448419	47.306305
2411.576885	200.039024	47.311309
2408.306139	210.879952	47.316314
2404.691591	211.381635	47.321319
2401.030007	214.928021	47.326324
2397.272360	210.313437	47.331329
2393.971736	226.000167	47.336333
2390.206127	213.667325	47.341338
2387.215903	207.469717	47.346343
2384.026994	199.545949	47.351348
2380.328898	212.477125	47.356353
2376.308497	214.250567	47.361357
2373.036612	203.625143	47.366362
2369.744936	205.506388	47.371367
2366.382220	199.202716	47.376372
2363.053604	195.957691	47.381377
2358.880706	203.203152	47.386381
2355.665626	194.870867	47.391386
2352.028517	195.155615	47.396391
2348.455742	202.962373	47.401396
2345.382765	212.359517	47.406401
2341.403338	199.155485	47.411405
2338.093615	216.273160	47.416410
2334.694302	200.807496	47.421415
2331.057208	202.981794	47.426420
2327.994495	198.309661	47.431425
2324.509705	208.967998	47.436429
2321.029387	195.227878	47.441434
2317.488394	192.675797	47.446439
2313.673284	189.704189	47.451444
2310.193795	203.335059	47.456449
2306.205937	197.243726	47.461453
2302.890691	204.736150	47.466458
2300.047757	204.611059	47.471463
2296.580630	203.292458	47.476468
2293.186381	201.041533	47.481473
2289.223932	214.367536	47.486477
2285.899440	201.937551	47.491482
2281.940347	217.449779	47.496487
2278.617470	203.011707	47.501492
2275.539280	203.917252	47.506497
2271.847478	216.050438	47.511501
2268.176754	190.329841	47.516506
2264.778184	192.819179	47.521511
2260.919269	202.233706	47.526516
2257.999869	210.693429	47.531521
2254.021466	210.814526	47.536525
2250.861294	200.486228	47.541530
2247.256076	195.700589	47.546535
2243.561917	211.845176	47.551540
2240.359291	192.341556	47.556545
2236.745290	203.677253	47.561549
2233.694225	188.554449	47.566554
2229.686940	201.553435	47.571559
2225.895984	215.214209	47.576564
2222.744109	195.383685	47.581569
2219.232035	211.001643	47.586573
2216.015039	200.197379	47.591578
2212.219358	203.603785	47.596583
2208.867376	192.043941	47.601588
2205.241424	196.168146	47.606593
2201.870342	196.067662	47.611597
2198.369103	204.476281	47.616602
2194.971647	195.559276	47.621607
2191.303562	199.600370	47.626612
2187.747944	188.366034	47.631617
2184.289808	190.010727	47.636621
2180.997201	187.420311	47.641626
2177.536922	183.890097	47.646631
2173.664375	192.147275	47.651636
2170.286370	190.750407	47.656641
2166.591917	179.365466	47.661645
2163.388722	198.999413	47.666650
2159.946028	186.301348	47.671655
2156.103867	204.659405	47.676660
2152.936556	184.345933	47.681665
2149.384812	187.112141	47.686669
2145.984635	193.095671	47.691674
2142.345988	176.794705	47.696679
2138.644362	192.481916	47.701684
2135.437888	173.185694	47.706689
2131.590463	196.122946	47.711693
2128.176597	195.732616	47.716698
2124.756188	196.378006	47.721703
2120.835374	200.171480	47.726708
2117.842577	178.224517	47.731713
2114.410388	189.044605	47.736717
2111.135610	168.996122	47.741722
2107.501148	187.243363	47.746727
2103.813210	184.453716	47.751732
2100.374506	191.715805	47.756737
2096.767923	169.858274	47.761741
2093.450304	184.805019	47.766746
2089.860487	180.545988	47.771751
2086.181674	183.980819	47.776756
2083.080410	184.701235	47.781761
2079.119166	182.554206	47.786765
2075.628322	184.610778	47.791770
2072.460784	186.369863	47.796775
2068.528586	183.469493	47.801780
2065.555767	191.288766	47.806785
2061.772126	183.086041	47.811789
2058.396862	184.662764	47.816794
2054.869121	184.084780	47.821799
2051.340546	176.934014	47.826804
2047.900932	187.252237	47.831809
2044.411980	182.668113	47.836813
2041.151837	178.022078	47.841818
2037.313485	191.438473	47.846823
2033.641263	179.902957	47.851828
2030.272804	191.398180	47.856833
2026.771866	172.596007	47.861837
2023.817287	185.102175	47.866842
2019.878344	178.495205	47.871847
2016.016926	169.580964	47.876852
2012.678704	173.072596	47.881857
2008.889130	187.196553	47.886861
2005.645149	172.443793	47.891866
2002.727980	174.866059	47.896871
1998.584180	183.342469	47.901876
1995.398919	173.481430	47.906881
1991.866452	193.702039	47.911885
1988.750128	174.723981	47.916890
1985.190937	174.498072	47.921895
1981.339217	177.315124	47.926900
1977.932384	181.351785	47.931905
1974.243843	172.547848	47.936909
1970.713272	169.384377	47.941914
1967.234058	170.996340	47.946919
1963.785979	176.437672	47.951924
1960.417644	171.277117	47.956929
1956.668925	175.418722	47.961933
1953.287517	173.767215	47.966938
1949.746659	162.489175	47.971943
1946.351268	179.814991	47.976948
1943.278488	172.572816	47.981953
1939.132113	178.542602	47.986957
1935.554793	165.486016	47.991962
1932.143372	173.265418	47.996967
1928.872072	181.677923	48.001972
1925.794435	174.435375	48.006977
1921.689774	161.513348	48.011981
1918.288785	166.421027	48.016986
1914.906903	178.598975	48.021991
1911.274383	192.271982	48.026996
1908.001229	172.193670	48.032001
1904.267501	185.736876	48.037005
1900.874218	166.810790	48.042010
1897.291533	156.816211	48.047015
1893.174185	176.256820	48.052020
1890.458358	163.922992	48.057025
1886.921592	179.960804	48.062029
1883.453310	171.667989	48.067034
1879.825231	172.417201	48.072039
1876.151919	175.790454	48.077044
1872.957343	159.005354	48.082049
1869.451083	180.490876	48.087053
1865.692678	163.755984	48.092058
1862.616386	165.069890	48.097063
1858.632101	175.232891	48.102068
1855.405138	162.325128	48.107073
1851.370896	169.086264	48.112077
1848.346187	170.218635	48.117082
1844.733303	165.890152	48.122087
1841.238162	174.388940	48.127092
1837.876689	171.459947	48.132097
1834.393646	162.361369	48.137101
1830.859825	180.502998	48.142106
1827.308574	176.387692	48.147111
1823.657037	177.733192	48.152116
1820.612230	159.013762	48.157121
1816.404529	175.317759	48.162125
1813.368089	159.932283	48.167130
1809.776534	157.861833	48.172135
1806.243502	161.442711	48.177140
1802.799304	147.501969	48.182145
1799.148526	159.987700	48.187149
1795.911399	160.425432	48.192154
1792.127974	165.165326	48.197159
1788.683503	159.081937	48.202164
1785.276444	171.109197	48.207169
1781.663540	168.191433	48.212173
1778.243822	182.411396	48.217178
1774.752797	165.833200	48.222183
1771.332033	158.112180	48.227188
1767.791637	162.519984	48.232193
1764.100784	161.527011	48.237197
1760.712621	174.721538	48.242202
1757.380962	162.039453	48.247207
1753.599486	173.243326	48.252212
1750.407096	163.410831	48.257217
1746.619600	166.004221	48.262221
1743.124314	167.968947	48.267226
1739.771837	169.894031	48.272231
1735.959173	163.885232	48.277236
1732.833261	148.397678	48.282241
1729.250059	176.362568	48.287245
1725.895710	155.535535	48.292250
1722.203228	160.957607	48.297255
1718.278076	162.141242	48.302260
1715.107733	148.980960	48.307265
1711.591483	152.612381	48.312269
1708.165039	152.592091	48.317274
1704.654776	172.236430	48.322279
1701.713231	177.785767	48.327284
1698.480578	160.634261	48.332289
1694.019624	164.291260	48.337293
1690.379177	170.360090	48.342298
1686.863413	156.215476	48.347303
1683.505177	169.560754	48.352308
1680.096072	158.666984	48.357313
1676.852140	161.344929	48.362317
1673.050304	158.264951	48.367322
1669.585681	138.728650	48.372327
1666.051889	162.650340	48.377332
1662.795696	141.870999	48.382337
1658.888187	169.768857	48.387341
1655.648136	162.060203	48.392346
1652.155114	155.901543	48.397351
1648.591162	159.672562	48.402356
1645.359371	158.433928	48.407361
1642.039902	171.645567	48.412365
1638.196043	166.582789	48.417370
1634.682362	172.402057	48.422375
1631.177996	155.582900	48.427380
1627.928746	161.111416	48.432385
1623.967493	144.515842	48.437389
1620.530485	151.796073	48.442394
1616.953465	154.218166	48.447399
1613.307611	159.347893	48.452404
1610.129573	164.898502	48.457409
1606.274469	153.796835	48.462413
1602.823913	164.417791	48.467418
1599.796502	143.561968	48.472423
1596.320789	163.550039	48.477428
1593.144784	155.770776	48.482433
1589.304794	160.037805	48.487437
1585.868891	159.626710	48.492442
1582.148522	139.165619	48.497447
1578.835612	156.962860	48.502452
1574.983585	144.263390	48.507457
1571.302895	158.642281	48.512461
1568.100898	139.652335	48.517466
1564.417250	153.203950	48.522471
1560.854307	173.448128	48.527476
1557.480962	150.874814	48.532481
1554.211799	153.235281	48.537485
1550.495866	152.547045	48.542490
1547.122945	145.660133	48.547495
1543.566975	153.518578	48.552500
1540.129529	153.656050	48.557505
1536.660119	142.332949	48.562509
1532.867465	151.671519	48.567514
1529.499516	138.435059	48.572519
1525.895667	144.103318	48.577524
1522.917529	150.380562	48.582529
1519.158869	142.206725	48.587533
1515.706689	160.417522	48.592538
1512.321109	150.089773	48.597543
1508.284696	160.214667	48.602548
1505.104011	143.542054	48.607553
1501.407490	134.589997	48.612557
1497.522010	150.267874	48.617562
1494.263998	140.275803	48.622567
1490.971492	148.601294	48.627572
1487.770115	156.534123	48.632577
1483.965449	141.681093	48.637581
1480.271059	149.932537	48.642586
1477.167638	150.823735	48.647591
1473.449000	166.101604	48.652596
1470.065042	139.858511	48.657601
1466.263920	149.401525	48.662605
1463.039405	151.776661	48.667610
1459.981120	161.367157	48.672615
1455.992854	148.960054	48.677620
1452.478835	153.317082	48.682625
1448.762311	144.133077	48.687629
1445.829137	149.162124	48.692634
1442.473956	144.940789	48.697639
1438.438909	140.864714	48.702644
1434.924085	144.140099	48.707649
1431.405229	130.353887	48.712653
1427.570251	140.808489	48.717658
1424.483073	147.777534	48.722663
1420.886384	144.725599	48.727668
1417.692748	152.920369	48.732673
1413.746238	152.027785	48.737677
1410.570358	145.829746	48.742682
1407.127125	156.523647	48.747687
1403.103193	148.884933	48.752692
1400.021304	148.958660	48.757697
1396.703751	136.122668	48.762701
1392.825250	138.680747	48.767706
1389.442465	147.026799	48.772711
1385.763033	153.503102	48.777716
1382.472812	132.503480	48.782721
1378.657497	154.999365	48.787725
1375.406168	139.996782	48.792730
1371.974738	153.631138	48.797735
1368.264760	149.531241	48.802740
1364.862530	148.915822	48.807745
1361.869765	137.870873	48.812749
1358.108481	156.119906	48.817754
1354.644253	152.811654	48.822759
1350.536101	152.691767	48.827764
1347.487565	150.365416	48.832769
1343.915012	141.011518	48.837773
1340.532895	148.130292	48.842778
1337.395426	146.872882	48.847783
1333.196232	140.173970	48.852788
1329.551189	151.424439	48.857793
1326.037488	142.380853	48.862797
1322.863386	149.525969	48.867802
1319.420953	148.030457	48.872807
1315.894994	153.435686	48.877812
1312.577433	145.389228	48.882817
1309.030140	156.683356	48.887821
1305.559663	147.543368	48.892826
1301.794558	145.682462	48.897831
1297.992635	153.133448	48.902836
1294.879447	150.737789	48.907841
1291.601109	142.676386	48.912845
1288.098801	150.894927	48.917850
1284.786166	126.753378	48.922855
1280.534235	140.435887	48.927860
1277.384631	140.731658	48.932865
1273.533774	137.338215	48.937869
1269.956314	148.281507	48.942874
1266.876340	145.782717	48.947879
1263.248915	149.279297	48.952884
1260.099175	157.884955	48.957889
1256.613570	146.235014	48.962893
1253.277023	152.372939	48.967898
1249.642405	151.659507	48.972903
1245.472504	136.604437	48.977908
1242.141246	145.903271	48.982913
1238.528358	143.579966	48.987917
1235.098086	147.357717	48.992922
1231.760784	134.975517	48.997927
1228.378576	153.887379	49.002932
1225.153858	139.153755	49.007937
1221.543666	139.460968	49.012941
1217.726399	140.890261	49.017946
1214.306884	141.844505	49.022951
1210.528625	130.736553	49.027956
1207.242859	135.959727	49.032961
1203.567813	130.680842	49.037965
1200.329117	147.218816	49.042970
1196.981547	135.862105	49.047975
1193.026658	132.917965	49.052980
1190.056744	144.778649	49.057985
1186.160748	137.762054	49.062989
1182.439379	156.364626	49.067994
1179.323248	131.807459	49.072999
1175.512191	154.792886	49.078004
1172.535303	131.744945	49.083009
1168.720730	133.499260	49.088013
1165.143903	134.520042	49.093018
1161.747870	137.529324	49.098023
1157.944996	135.739252	49.103028
1155.000458	145.336713	49.108033
1150.927946	150.275275	49.113037
1147.877077	135.581663	49.118042
1144.604965	139.876106	49.123047
1140.882214	133.182427	49.128052
1137.489651	135.977278	49.133057
1133.805456	135.892000	49.138061
1130.395129	132.040598	49.143066
1126.608766	135.272369	49.148071
1122.657690	128.361589	49.153076
1119.484795	141.403870	49.158081
1116.096725	135.517829	49.163085
1112.824938	151.140020	49.168090
1109.726380	129.308816	49.173095
1105.927155	139.834406	49.178100
1102.017512	134.347492	49.183105
1098.141238	127.144021	49.188109
1094.957770	149.714225	49.193114
1092.113251	125.493565	49.198119
1088.190741	133.533751	49.203124
1084.728345	134.752117	49.208129
1081.384705	126.051137	49.213133
1077.474713	132.603718	49.218138
1074.465877	127.914041	49.223143
1070.643385	125.087509	49.228148
1067.335343	124.094258	49.233153
1063.343305	141.869590	49.238157
1059.810406	140.545408	49.243162
1056.672009	123.349108	49.248167
1052.625695	142.237672	49.253172
1049.916389	130.757528	49.258177
1046.387814	146.914582	49.263181
1042.396281	138.923819	49.268186
1039.364720	126.981648	49.273191
1035.681879	134.603876	49.278196
1032.006597	134.424058	49.283201
1028.487049	131.416626	49.288205
1025.004593	131.613971	49.293210
1021.916044	121.140624	49.298215
1018.007494	140.512223	49.303220
1014.375022	130.659899	49.308225
1010.747073	143.394496	49.313229
1007.529978	143.683284	49.318234
1004.471052	130.808392	49.323239
1000.547316	143.082311	49.328244
997.451466	128.333583	49.333249
993.739101	143.048872	49.338253
989.854753	138.098147	49.343258
986.493982	131.888448	49.348263
982.844609	124.286932	49.353268
979.676868	130.254250	49.358273
976.476668	131.347205	49.363277
972.466388	136.405998	49.368282
969.269614	139.574045	49.373287
965.587845	135.654006	49.378292
961.820918	139.594500	49.383297
958.523400	148.393649	49.388301
954.785611	120.622656	49.393306
951.702650	129.651931	49.398311
948.071376	146.639724	49.403316
944.836653	137.140429	49.408321
941.064328	134.913656	49.413325
937.266358	147.813382	49.418330
933.838053	127.716531	49.423335
930.271949	137.104668	49.428340
927.322962	122.708871	49.433345
923.856146	128.172573	49.438349
920.151801	130.027200	49.443354
916.855669	120.721261	49.448359
912.844232	150.946185	49.453364
909.513884	129.934390	49.458369
906.069163	135.692964	49.463373
902.549842	150.364483	49.468378
898.970694	120.737224	49.473383
895.010592	121.167791	49.478388
891.519360	130.867242	49.483393
888.630893	133.991715	49.488397
885.105899	123.422614	49.493402
881.837493	133.799093	49.498407
878.107510	135.377322	49.503412
874.804708	145.724176	49.508417
870.644889	135.530196	49.513421
867.387912	148.103864	49.518426
863.940425	130.884734	49.523431
860.563331	136.516250	49.528436
857.192692	128.450220	49.533441
853.680148	135.135963	49.538445
849.791321	138.928845	49.543450
846.494749	126.192927	49.548455
842.488837	130.563986	49.553460
839.205568	115.217437	49.558465
835.992003	135.294097	49.563469
832.461573	137.938436	49.568474
829.088140	140.062428	49.573479
825.351170	144.293596	49.578484
821.788415	130.590406	49.583489
818.361159	142.667497	49.588493
815.089809	134.024477	49.593498
811.717809	127.904135	49.598503
807.982395	134.993672	49.603508
804.326886	142.472306	49.608513
801.033041	131.718490	49.613517
797.131161	142.775030	49.618522
794.181445	118.600763	49.623527
790.298413	146.908497	49.628532
786.795793	132.721099	49.633537
783.209335	135.261466	49.638541
779.810905	121.333091	49.643546
776.805413	129.478872	49.648551
772.677705	129.043145	49.653556
769.712719	138.743839	49.658561
765.994242	128.749129	49.663565
762.534030	131.597747	49.668570
759.026668	123.034384	49.673575
755.369810	135.387745	49.678580
751.858290	117.939372	49.683585
747.831755	125.549435	49.688589
744.446872	137.706857	49.693594
740.917047	120.892365	49.698599
737.851319	127.782752	49.703604
734.530278	139.762230	49.708609
731.068469	137.953174	49.713613
727.520441	136.938071	49.718618
724.134919	133.333953	49.723623
720.129834	140.692494	49.728628
716.907486	120.108611	49.733633
713.237113	126.521478	49.738637
709.788954	126.968722	49.743642
706.725986	117.511747	49.748647
702.845747	117.090931	49.753652
699.320186	120.599177	49.758657
695.791288	123.176347	49.763661
692.210970	133.839982	49.768666
689.073079	122.408622	49.773671
685.321229	141.048051	49.778676
681.478615	128.927322	49.783681
678.360388	133.865386	49.788685
674.710190	124.571405	49.793690
671.400514	129.007011	49.798695
667.346575	128.507672	49.803700
663.974557	124.015897	49.808705
660.923364	115.261646	49.813709
657.456896	124.171471	49.818714
654.005461	130.935205	49.823719
650.307504	114.439761	49.828724
646.732343	127.041972	49.833729
643.433118	112.761514	49.838733
639.693578	130.911497	49.843738
636.116975	113.961281	49.848743
632.581373	129.118548	49.853748
628.997347	113.214441	49.858753
625.694309	115.964659	49.863757
622.272965	121.219748	49.868762
619.013963	117.565004	49.873767
615.225558	128.941930	49.878772
611.675275	113.278881	49.883777
608.165896	120.716889	49.888781
604.720964	129.689770	49.893786
601.452283	117.473919	49.898791
597.497624	116.184238	49.903796
594.309831	120.119629	49.908801
590.826705	117.808111	49.913805
587.197777	123.478973	49.918810
583.734284	120.809873	49.923815
579.995371	119.274054	49.928820
576.274567	109.338170	49.933825
573.044401	124.050613	49.938829
569.807706	113.644519	49.943834
566.661324	121.480709	49.948839
562.878948	127.216191	49.953844
559.132724	119.809692	49.958849
555.639176	118.333684	49.963853
552.062075	129.131302	49.968858
548.820680	125.639610	49.973863
545.209984	113.832955	49.978868
542.059937	117.162751	49.983873
538.472888	117.655714	49.988877
534.231870	116.867742	49.993882
531.133857	111.366113	49.998887
527.508640	129.332412	50.003892
524.143199	132.295216	50.008897
520.578012	115.610335	50.013901
516.874212	128.474844	50.018906
513.808769	113.673765	50.023911
509.705338	122.601268	50.028916
506.656981	112.707652	50.033921
503.048209	126.879825	50.038925
499.882697	108.341159	50.043930
496.521684	113.261196	50.048935
492.862318	110.689118	50.053940
489.054070	105.197307	50.058945
485.762910	112.897236	50.063949
481.815392	126.418564	50.068954
478.425544	118.209942	50.073959
474.679366	114.471404	50.078964
471.836026	113.504190	50.083969
468.161066	120.454378	50.088973
464.762490	131.323757	50.093978
461.293238	118.190164	50.098983
457.708532	119.596950	50.103988
453.979472	124.881049	50.108993
450.624165	121.707525	50.113997
446.579861	119.721695	50.119002
443.361183	104.672038	50.124007
439.831670	113.989719	50.129012
436.647506	120.670431	50.134017
433.272173	107.191771	50.139021
429.690054	118.853724	50.144026
426.313790	127.172156	50.149031
422.405083	120.940548	50.154036
418.853706	130.083109	50.159041
415.262673	116.470905	50.164045
411.807533	127.347773	50.169050
408.308850	118.473940	50.174055
404.970655	127.871116	50.179060
401.752005	122.609366	50.184065
398.363630	122.885016	50.189069
394.502463	115.877704	50.194074
391.292306	118.699402	50.199079
387.615103	101.868200	50.204084
383.803738	122.879661	50.209089
380.697949	109.884071	50.214093
376.926307	128.898968	50.219098
373.401498	109.453788	50.224103
369.846886	125.510404	50.229108
366.491804	112.636501	50.234113
363.126368	120.832425	50.239117
359.352466	132.487431	50.244122
355.942027	118.475011	50.249127
352.468134	122.430844	50.254132
348.932515	123.329339	50.259137
345.497375	116.004567	50.264141
341.744101	118.439646	50.269146
338.643834	109.437599	50.274151
335.361443	107.239654	50.279156
331.494001	110.768854	50.284161
328.216677	117.747330	50.289165
324.033006	105.772993	50.294170
321.079089	128.393025	50.299175
317.398464	114.870764	50.304180
313.675506	116.797256	50.309185
310.297455	109.505692	50.314189
306.792173	105.447008	50.319194
303.718260	101.323769	50.324199
299.795890	109.943477	50.329204
296.676751	114.845646	50.334209
292.908319	114.502193	50.339213
289.365728	113.424784	50.344218
285.996988	115.156834	50.349223
282.403359	117.539626	50.354228
278.992084	109.520720	50.359233
275.602785	124.311839	50.364237
271.759745	117.871500	50.369242
268.526351	124.179343	50.374247
264.944587	126.740414	50.379252
261.228305	108.118798	50.384257
257.666659	113.709357	50.389261
254.258596	104.452015	50.394266
250.968318	127.855355	50.399271
247.249201	116.871482	50.404276
243.777476	114.000229	50.409281
240.376097	106.395611	50.414285
236.612701	120.938304	50.419290
233.678502	109.400183	50.424295
229.923155	112.450238	50.429300
226.578979	122.888117	50.434305
223.073180	109.097627	50.439309
219.185853	97.173458	50.444314
215.947857	108.280963	50.449319
212.238530	96.417159	50.454324
208.835942	111.591362	50.459329
205.418773	100.336376	50.464333
201.775802	115.593905	50.469338
198.327269	106.014395	50.474343
194.832173	119.591115	50.479348
191.115786	119.601849	50.484353
187.973460	108.903302	50.489357
184.173615	126.365686	50.494362
180.879749	101.271848	50.499367
177.484143	106.972720	50.504372
173.929504	104.910108	50.509377
170.522614	110.008341	50.514381
166.588024	114.587681	50.519386
163.660779	102.497810	50.524391
159.991928	102.989405	50.529396
156.212468	115.773835	50.534401
152.874494	111.645671	50.539405
148.945856	106.865095	50.544410
145.783971	112.912780	50.549415
141.817007	115.128475	50.554420
138.888032	106.947101	50.559425
135.445292	110.828248	50.564429
131.924398	107.250686	50.569434
128.424636	109.813765	50.574439
124.604602	94.809640	50.579444
121.251094	110.681979	50.584449
117.939217	104.183278	50.589453
114.502898	119.759264	50.594458
110.628827	105.259967	50.599463
107.001972	115.947222	50.604468
103.515202	129.654700	50.609473
100.086803	103.621343	50.614477
96.517550	109.211067	50.619482
93.454416	104.732507	50.624487
89.364629	107.729689	50.629492
85.921065	121.092556	50.634497
82.766868	95.051896	50.639501
79.023147	115.576508	50.644506
76.052756	112.337814	50.649511
72.250646	115.116712	50.654516
68.897006	113.893872	50.659521
65.495161	103.987414	50.664525
61.530011	117.321555	50.669530
58.275012	110.787643	50.674535
55.001226	106.605525	50.679540
51.219917	125.883259	50.684545
47.614138	113.268415	50.689549
44.263285	125.180766	50.694554
40.488673	110.704936	50.699559
36.984346	93.961648	50.704564
33.528396	118.112135	50.709569
30.255926	97.323591	50.714573
26.759880	121.400315	50.719578
23.668899	107.981184	50.724583
19.825814	115.510420	50.729588
15.940437	107.688010	50.734593
12.424782	113.673866	50.739597
9.110690	120.464916	50.744602
5.837927	102.437857	50.749607
1.966207	105.402310	50.754612
