Wed Jun 15 16:11:27 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.544778	124.469208	0.000000
0.443905	105.657842	0.005005
-0.127435	114.416514	0.010010
-0.155131	95.266521	0.015014
0.105915	103.453605	0.020019
-0.106967	89.187845	0.025024
-0.129705	88.402233	0.030029
-0.134916	62.977324	0.035034
-0.556344	66.948344	0.040038
-1.126046	60.451722	0.045043
-1.423315	46.900954	0.050048
-1.603504	24.954002	0.055053
-1.782841	20.564781	0.060058
-2.191945	26.952954	0.065062
-2.010302	9.447656	0.070067
-2.754395	4.589587	0.075072
-3.486917	3.928679	0.080077
-3.244460	0.341000	0.085082
-3.808235	-5.858464	0.090086
-3.868460	-3.193351	0.095091
-4.439991	-4.026467	0.100096
-5.281890	-27.114722	0.105101
-5.406107	-18.536456	0.110106
-5.517096	-8.916894	0.115110
-5.297568	-22.813333	0.120115
-5.449585	-11.087805	0.125120
-5.464351	-19.479055	0.130125
-5.868630	-12.081362	0.135130
-6.723011	-9.855773	0.140134
-6.613847	-1.568798	0.145139
-6.653054	-0.719584	0.150144
-6.918801	-8.986400	0.155149
-7.727481	-16.578712	0.160154
-8.252410	-3.026674	0.165158
-8.107015	-17.052030	0.170163
-8.298129	-16.685245	0.175168
-8.794543	-14.069482	0.180173
-8.391506	-28.412825	0.185178
-8.529439	-3.842066	0.190182
-8.668163	-20.879083	0.195187
-9.367765	-14.197980	0.200192
-9.731376	-12.820766	0.205197
-9.504859	-14.631855	0.210202
-10.118565	-0.409739	0.215206
-10.191974	-28.239263	0.220211
-11.065586	-17.926558	0.225216
-11.167747	-4.747529	0.230221
-11.276782	-12.138616	0.235226
-11.697237	1.899650	0.240230
-11.439557	-8.160445	0.245235
-11.700259	-12.238792	0.250240
-12.261517	-11.985242	0.255245
-12.729440	-16.743242	0.260250
-12.882012	-8.001071	0.265254
-12.795700	-18.442120	0.270259
-13.165095	-11.164918	0.275264
-13.592091	0.333108	0.280269
-13.490731	-17.573894	0.285274
-14.375184	-6.782436	0.290278
-14.811907	-4.500490	0.295283
-14.863582	-13.825345	0.300288
-15.038786	-11.358549	0.305293
-14.837031	-9.843345	0.310298
-15.016949	-15.247329	0.315302
-14.902808	-6.204171	0.320307
-15.107723	-14.621213	0.325312
-15.677821	-1.275869	0.330317
-15.992234	-13.087971	0.335322
-16.534375	-4.084518	0.340326
-16.459962	-13.429619	0.345331
-16.990739	-16.209934	0.350336
-17.394718	-16.253455	0.355341
-17.770216	-16.324471	0.360346
-18.228667	-15.923666	0.365350
-17.802426	-4.766214	0.370355
-17.988634	-9.577876	0.375360
-18.123378	-12.828484	0.380365
-18.841228	-14.535786	0.385370
-19.074285	-12.249323	0.390374
-19.535690	-9.924135	0.395379
-19.669117	-21.236707	0.400384
-19.777759	-10.687895	0.405389
-19.560885	-20.908245	0.410394
-20.026932	-14.743088	0.415398
-20.646283	-3.408595	0.420403
-20.807948	-9.308433	0.425408
-21.212513	-5.254199	0.430413
-21.013860	-21.409438	0.435418
-21.583921	-9.688511	0.440422
-21.443694	-16.217488	0.445427
-21.464852	-12.685126	0.450432
-22.374735	-15.365795	0.455437
-22.561986	-11.243702	0.460442
-22.787108	-3.723896	0.465446
-22.844173	-23.724611	0.470451
-23.167305	-16.874796	0.475456
-23.607548	-11.140250	0.480461
-23.989266	-30.833189	0.485466
-24.263380	-27.339028	0.490470
-24.281261	-35.158001	0.495475
-24.382400	-15.210957	0.500480
-24.350573	-29.669822	0.505485
-24.496333	-25.484452	0.510490
-25.552013	-14.858344	0.515494
-25.648448	-19.286111	0.520499
-25.723615	-26.231482	0.525504
-26.122160	-14.991099	0.530509
-26.010332	-5.010619	0.535514
-26.144283	-11.687139	0.540518
-26.697600	-8.378846	0.545523
-27.257150	-18.623091	0.550528
-27.595341	-25.996226	0.555533
-27.209294	-12.745481	0.560538
-27.456567	-13.818130	0.565542
-27.813692	-21.569207	0.570547
-28.747637	-26.388289	0.575552
-29.028315	-11.658744	0.580557
-28.967528	-8.990351	0.585562
-29.148734	-8.267513	0.590566
-29.210251	-13.213716	0.595571
-29.221105	-10.278188	0.600576
-29.302117	-20.823077	0.605581
-29.857616	-18.983954	0.610586
-30.271405	-3.477859	0.615590
-30.627786	-26.080906	0.620595
-30.941709	-6.013062	0.625600
-31.125556	-20.129008	0.630605
-30.946552	-7.808603	0.635610
-31.357244	-7.849041	0.640614
-31.815182	-26.376808	0.645619
-32.233980	-22.758115	0.650624
-32.361380	-6.773670	0.655629
-32.245807	-26.747668	0.660634
-32.474172	-2.796557	0.665638
-32.694956	-20.674086	0.670643
-33.776455	1.041349	0.675648
-34.103721	2.687880	0.680653
-34.117014	-19.107343	0.685658
-34.187140	-9.410490	0.690662
-34.176972	-26.188792	0.695667
-34.134595	-12.557200	0.700672
-34.203879	-20.107161	0.705677
-34.722629	-10.044272	0.710682
-35.207182	-19.212943	0.715686
-35.516395	-8.185301	0.720691
-35.564733	-19.681408	0.725696
-36.016094	-15.578307	0.730701
-36.408004	-4.452949	0.735706
-37.006072	-5.153534	0.740710
-37.379009	-16.703226	0.745715
-37.255420	-11.139102	0.750720
-37.250250	-27.052733	0.755725
-37.176460	-16.941387	0.760730
-37.327951	-12.678714	0.765734
-37.452361	-9.203371	0.770739
-38.143375	6.684242	0.775744
-38.664223	0.141896	0.780749
-38.308218	-20.658745	0.785754
-38.881684	-7.203650	0.790758
-39.504367	-32.238394	0.795763
-40.052623	-6.828916	0.800768
-40.518882	-14.308537	0.805773
-40.322266	-14.634600	0.810778
-40.685195	6.890666	0.815782
-40.705202	-7.285217	0.820787
-40.850875	-8.958740	0.825792
-40.517033	-13.432366	0.830797
-40.282722	-9.230592	0.835802
-41.243300	-23.416543	0.840806
-41.685875	-1.940766	0.845811
-41.837828	3.986541	0.850816
-42.331160	3.038900	0.855821
-42.395596	-25.583639	0.860826
-43.448456	-3.409505	0.865830
-43.599773	-19.524759	0.870835
-43.314571	-7.160746	0.875840
-43.991964	2.817787	0.880845
-43.604234	-12.731157	0.885850
-43.571823	-7.957211	0.890854
-43.660079	-18.693262	0.895859
-44.037609	-3.138609	0.900864
-44.830425	-15.972430	0.905869
-44.845937	-4.380635	0.910874
-45.295603	-7.597840	0.915878
-45.375390	-5.613014	0.920883
-46.062932	-23.362890	0.925888
-46.666100	-9.896970	0.930893
-46.690989	-2.301944	0.935898
-46.956142	-8.816209	0.940902
-47.015809	-11.126205	0.945907
-47.135551	-2.896006	0.950912
-47.209347	-9.988296	0.955917
-47.144498	-6.777233	0.960922
-47.330177	-15.215107	0.965926
-47.815571	-10.918361	0.970931
-47.910904	-19.230692	0.975936
-48.303152	-5.955784	0.980941
-48.746578	-20.528962	0.985946
-49.734735	-0.838474	0.990950
-49.886139	-5.314769	0.995955
-49.379870	-4.072043	1.000960
-49.627670	12.311809	1.005965
-50.095389	-8.564799	1.010970
-50.222453	-19.259712	1.015974
-50.338679	-20.505932	1.020979
-50.354422	-4.412588	1.025984
-51.631589	-19.161374	1.030989
-51.441546	-5.076440	1.035994
-51.666123	-0.880208	1.040998
-51.531543	-11.664829	1.046003
-51.698526	-12.654764	1.051008
-52.175597	-12.645266	1.056013
-52.612881	-26.290306	1.061018
-53.132828	-20.076389	1.066022
-53.403731	-16.903553	1.071027
-53.222401	-14.212370	1.076032
-53.246956	-2.013394	1.081037
-53.243101	-19.127139	1.086042
-54.473920	-15.283684	1.091046
-54.593245	-8.955550	1.096051
-55.101639	-21.514883	1.101056
-55.167765	-12.755733	1.106061
-54.621333	4.893972	1.111066
-55.032491	-6.168705	1.116070
-55.230600	-12.687044	1.121075
-55.614469	-7.929037	1.126080
-56.342979	-30.926115	1.131085
-56.202878	-13.675479	1.136090
-56.545747	-22.173191	1.141094
-56.712122	-10.343492	1.146099
-56.644458	-24.496460	1.151104
-57.342151	-16.575100	1.156109
-57.640249	-13.703472	1.161114
-57.927573	-6.717027	1.166118
-57.958792	-18.592789	1.171123
-58.199854	-12.398129	1.176128
-58.660003	-15.964582	1.181133
-59.252063	-12.555185	1.186138
-59.700373	-10.104018	1.191142
-59.280247	-19.222543	1.196147
-59.424243	-18.301656	1.201152
-59.970133	-22.887746	1.206157
-59.460807	-19.936290	1.211162
-59.860310	-6.487357	1.216166
-60.701382	-13.472170	1.221171
-60.924876	-15.049475	1.226176
-61.277925	-15.773091	1.231181
-61.483698	-9.708853	1.236186
-61.099916	-7.518119	1.241190
-61.671579	-11.048781	1.246195
-62.385538	-17.730153	1.251200
-62.748258	-15.932063	1.256205
-62.321658	-15.709785	1.261210
-63.028599	-16.732702	1.266214
-63.174430	-2.169856	1.271219
-63.040596	-2.576791	1.276224
-63.312546	-0.986949	1.281229
-63.939440	-11.197669	1.286234
-63.902578	-17.965349	1.291238
-64.519932	2.082413	1.296243
-64.118019	-20.974250	1.301248
-64.941344	7.455179	1.306253
-65.135663	-17.559326	1.311258
-65.798245	-14.243627	1.316262
-65.934946	-1.374857	1.321267
-66.028135	-11.323491	1.326272
-66.167212	-13.696319	1.331277
-65.791110	1.072953	1.336282
-66.481820	-16.217697	1.341286
-66.446022	-7.322884	1.346291
-67.050921	-21.141560	1.351296
-67.837029	-6.928643	1.356301
-67.653589	-13.525132	1.361306
-67.880143	-13.324922	1.366310
-67.939461	-12.000758	1.371315
-67.880468	-9.828753	1.376320
-68.969658	-6.457639	1.381325
-69.140966	-9.168626	1.386330
-69.306569	-14.137576	1.391334
-69.383997	-9.961424	1.396339
-69.224350	-22.343805	1.401344
-69.543174	-11.668521	1.406349
-69.674370	-6.178988	1.411354
-70.710412	3.860300	1.416358
-71.061197	-18.464700	1.421363
-71.186405	-9.271804	1.426368
-70.992683	-12.611617	1.431373
-70.619988	-23.992340	1.436378
-70.984474	-7.356817	1.441382
-72.476419	-12.899968	1.446387
-72.355389	-12.759078	1.451392
-72.925064	3.429470	1.456397
-72.729743	-14.790077	1.461402
-72.874057	-2.514392	1.466406
-73.006427	-13.443995	1.471411
-72.942914	-28.660167	1.476416
-73.617518	-0.375682	1.481421
-73.970059	-23.862138	1.486426
-74.266145	-1.641730	1.491430
-74.264407	0.738806	1.496435
-74.485591	-25.066330	1.501440
-74.718812	-13.154267	1.506445
-75.031592	-3.318960	1.511450
-75.673232	-30.077655	1.516454
-75.863711	-10.118119	1.521459
-76.082301	-14.943362	1.526464
-76.172458	-13.828656	1.531469
-76.077332	-14.039005	1.536474
-76.185041	-10.919379	1.541478
-76.793382	-12.763640	1.546483
-77.157416	-6.052662	1.551488
-77.764260	3.890931	1.556493
-77.458581	-15.819640	1.561498
-77.749522	-6.813710	1.566502
-77.896700	-2.006827	1.571507
-78.367839	-7.998155	1.576512
-79.154600	-15.707617	1.581517
-78.897116	-18.278071	1.586522
-78.967325	-26.629962	1.591526
-79.424044	-18.063432	1.596531
-79.528271	-13.828893	1.601536
-79.507815	-12.347947	1.606541
-80.159526	-4.661461	1.611546
-80.739699	-16.592686	1.616550
-80.922952	3.282908	1.621555
-80.787802	-10.314698	1.626560
-80.997644	-25.830855	1.631565
-81.119826	-15.145656	1.636570
-81.406716	1.780092	1.641574
-81.979332	-0.518915	1.646579
-81.907109	-26.383489	1.651584
-82.342060	-10.553901	1.656589
-82.293547	-16.459072	1.661594
-82.872151	-21.177067	1.666598
-83.681566	-2.191750	1.671603
-83.514194	-25.339852	1.676608
-83.965429	-10.694481	1.681613
-83.674305	-21.140173	1.686618
-83.726831	-3.913824	1.691622
-84.107319	-7.054763	1.696627
-84.761829	-20.005733	1.701632
-85.100301	-14.640568	1.706637
-85.479443	-5.128705	1.711642
-85.542234	-18.329782	1.716646
-85.689216	-3.272238	1.721651
-85.780303	-18.621193	1.726656
-85.904432	-2.747282	1.731661
-85.797861	-10.089360	1.736666
-86.713256	-11.231413	1.741670
-87.132275	-4.834808	1.746675
-87.255033	-14.026178	1.751680
-87.581753	-6.024074	1.756685
-87.151852	-23.990682	1.761690
-87.690657	-14.587680	1.766694
-88.666722	-22.772001	1.771699
-88.829808	-19.072360	1.776704
-88.962656	-21.594480	1.781709
-89.082548	-8.623833	1.786714
-89.283030	-16.910693	1.791718
-89.307906	-19.864774	1.796723
-89.200293	-15.379274	1.801728
-89.593078	-18.706492	1.806733
-90.285152	-12.067469	1.811738
-90.579107	-15.385078	1.816742
-90.842086	-13.909569	1.821747
-90.567581	-7.814127	1.826752
-90.932155	-17.481940	1.831757
-91.594070	-21.087742	1.836762
-92.130809	-12.239470	1.841766
-92.274172	-25.326999	1.846771
-92.360702	-15.326180	1.851776
-92.818812	-22.158637	1.856781
-92.553181	-14.116237	1.861786
-92.190733	-3.017109	1.866790
-92.601489	-18.698837	1.871795
-93.565341	-10.861624	1.876800
-94.067609	-7.297394	1.881805
-94.065500	-26.232530	1.886810
-94.012460	-19.523905	1.891814
-94.066375	-31.481328	1.896819
-93.899259	-19.452646	1.901824
-95.174864	-7.006564	1.906829
-95.526996	-24.974624	1.911834
-95.771632	-3.705585	1.916838
-95.828132	-14.298615	1.921843
-95.678997	-20.048375	1.926848
-95.856402	-8.372815	1.931853
-95.820129	-27.027622	1.936858
-96.764404	-15.938137	1.941862
-97.302451	-13.703561	1.946867
-97.182814	-18.183904	1.951872
-97.238621	-18.970259	1.956877
-97.481931	-12.479192	1.961882
-98.247544	-1.646604	1.966886
-98.470405	-18.154078	1.971891
-98.762350	-10.127440	1.976896
-98.900872	-14.576165	1.981901
-98.867691	-25.354076	1.986906
-98.604003	-15.978749	1.991910
-99.163444	-35.278186	1.996915
-99.787412	-12.828136	2.006912
-99.391691	-14.150711	2.016909
-99.101192	-12.051611	2.026906
-98.466583	-13.436189	2.036902
-97.543212	-13.718980	2.046899
-97.611070	-17.239661	2.056896
-96.838765	-13.692285	2.066893
-96.282422	-7.091523	2.076890
-96.425771	-7.486624	2.086886
-95.363327	-8.111238	2.096883
-94.849174	-23.257597	2.106880
-94.250488	-25.176717	2.116877
-93.600997	-6.562969	2.126874
-93.438201	-4.695915	2.136870
-93.189878	-1.979330	2.146867
-92.427681	-8.022257	2.156864
-91.746759	-16.238960	2.166861
-91.401491	-11.103961	2.176858
-90.654409	-3.185591	2.186854
-90.015584	-24.976026	2.196851
-90.017091	-19.374404	2.206848
-89.708653	-16.296868	2.216845
-88.909641	-15.435077	2.226842
-88.373118	-5.620742	2.236838
-87.900919	-21.110613	2.246835
-87.037046	-20.998260	2.256832
-87.032521	-16.222579	2.266829
-86.556204	-13.970078	2.276826
-85.921271	-10.657494	2.286822
-85.499197	-5.502591	2.296819
-84.530141	-16.710133	2.306816
-84.022393	-28.818972	2.316813
-83.978897	-14.670817	2.326810
-83.495941	-6.478161	2.336806
-82.836750	-15.924346	2.346803
-82.694669	-6.636071	2.356800
-81.717854	-17.107263	2.366797
-81.317580	-23.025472	2.376794
-80.991355	-16.502342	2.386790
-80.285978	-9.587323	2.396787
-79.540492	-14.523013	2.406784
-79.611172	-28.486313	2.416781
-78.762161	-16.341245	2.426778
-78.330655	-11.062560	2.436774
-78.244519	-16.437066	2.446771
-77.252756	-23.620028	2.456768
-76.419789	-24.876683	2.466765
-76.298071	-8.387017	2.476762
-75.905043	-6.185642	2.486758
-74.985572	-6.129392	2.496755
-74.905116	-19.521787	2.506752
-74.872939	-6.445506	2.516749
-73.845063	-7.566364	2.526746
-73.395297	-21.939365	2.536742
-72.569377	-20.483558	2.546739
-71.745060	-13.395492	2.556736
-71.460838	-23.777794	2.566733
-71.428295	-14.450972	2.576730
-71.441432	-4.978117	2.586726
-70.590753	-21.835719	2.596723
-69.970933	-13.760505	2.606720
-68.629579	-8.907964	2.616717
-68.507881	-6.765751	2.626714
-68.648223	-7.595454	2.636710
-68.143055	-8.368670	2.646707
-67.161074	-10.554806	2.656704
-67.005187	-3.936945	2.666701
-65.798982	-20.020262	2.676698
-65.539487	-16.583203	2.686694
-65.662993	-3.915490	2.696691
-65.130302	-18.559896	2.706688
-64.256874	-16.440585	2.716685
-63.698885	-16.008520	2.726682
-63.412980	-5.577807	2.736678
-62.280846	-7.239980	2.746675
-62.095200	-11.491201	2.756672
-61.991784	-23.531641	2.766669
-61.628335	-10.997354	2.776666
-60.496779	-18.159763	2.786662
-60.460230	-15.219820	2.796659
-59.962223	-25.572462	2.806656
-59.178702	-13.815701	2.816653
-58.901368	-4.136610	2.826650
-57.881608	-5.285361	2.836646
-57.659416	-19.814644	2.846643
-57.710694	-8.831184	2.856640
-56.783387	-12.185353	2.866637
-56.296517	-19.395693	2.876634
-56.000744	-13.345485	2.886630
-55.028338	-22.660406	2.896627
-54.465263	-1.749237	2.906624
-54.242742	-10.376143	2.916621
-53.928945	-10.203197	2.926618
-53.325309	-13.008825	2.936614
-52.796989	-0.506716	2.946611
-52.458271	-15.066522	2.956608
-51.694050	-12.388381	2.966605
-51.125745	-23.047478	2.976602
-50.812096	-8.891414	2.986598
-49.740222	-7.701946	2.996595
-49.523396	-10.888419	3.006592
-49.252883	-12.275737	3.016589
-49.196030	-16.432678	3.026586
-48.258165	-21.321732	3.036582
-47.661521	-12.224737	3.046579
-47.474456	-9.329028	3.056576
-46.445714	-15.667771	3.066573
-46.339823	-20.251511	3.076570
-46.117399	-15.923523	3.086566
-44.991967	-10.774235	3.096563
-44.598413	-23.011378	3.106560
-44.750633	-14.189759	3.116557
-43.516932	-8.056417	3.126554
-43.026824	-5.406951	3.136550
-43.108705	-11.379811	3.146547
-42.043405	-18.384690	3.156544
-41.485905	-14.223097	3.166541
-41.213723	-18.760144	3.176538
-41.060700	-14.482911	3.186534
-40.053963	-21.640392	3.196531
-39.863821	-21.475357	3.206528
-39.068976	-11.703708	3.216525
-38.377199	-16.538759	3.226522
-38.273530	-11.672785	3.236518
-38.112474	-9.328864	3.246515
-36.985567	-25.841174	3.256512
-36.306704	-15.893016	3.266509
-36.641127	-11.167297	3.276506
-36.045629	-12.741863	3.286502
-35.125719	-24.857981	3.296499
-34.816146	-24.628826	3.306496
-33.848515	-25.248032	3.316493
-33.372081	-18.787255	3.326490
-32.997996	-12.998498	3.336486
-33.178489	-22.438558	3.346483
-32.473318	-19.386582	3.356480
-31.583938	-21.354827	3.366477
-31.345218	-7.468172	3.376474
-30.539992	-6.969795	3.386470
-30.216573	-19.711042	3.396467
-29.876333	-20.839246	3.406464
-29.033310	-16.511097	3.416461
-28.674571	-18.481034	3.426458
-28.326960	-11.902166	3.436454
-27.474545	-3.244991	3.446451
-27.087878	-21.937550	3.456448
-27.080408	-16.504529	3.466445
-25.997508	-5.888862	3.476442
-25.361372	-4.376298	3.486438
-25.383746	-12.572186	3.496435
-24.937977	-19.742348	3.506432
-24.306445	-11.247105	3.516429
-23.659415	-12.158141	3.526426
-22.721515	-18.167574	3.536422
-22.535730	-16.169690	3.546419
-22.268925	-19.550113	3.556416
-22.031626	-4.449899	3.566413
-20.856483	-9.451161	3.576410
-20.556388	-11.453089	3.586406
-20.405179	-4.079434	3.596403
-19.757746	-31.485020	3.606400
-18.886505	-8.107666	3.616397
-19.096392	-9.495695	3.626394
-17.927294	-11.385121	3.636390
-17.312031	-30.335219	3.646387
-17.087484	-11.893810	3.656384
-17.060861	-15.330349	3.666381
-16.119492	-7.031207	3.676378
-15.614863	-11.868911	3.686374
-15.489786	-22.147677	3.696371
-14.495893	-8.016809	3.706368
-14.030473	-9.094881	3.716365
-13.838819	-15.974241	3.726362
-12.722630	-11.528258	3.736358
-12.531042	-14.466492	3.746355
-12.370405	-11.450553	3.756352
-11.878782	-23.115223	3.766349
-11.023489	-15.172649	3.776346
-10.555846	-10.329291	3.786342
-10.488576	-15.857138	3.796339
-9.370021	-16.881557	3.806336
-8.783017	-22.076895	3.816333
-8.925918	-20.383828	3.826330
-8.335427	-18.385069	3.836326
-7.760342	-28.225178	3.846323
-7.450755	-24.104199	3.856320
-6.361756	-15.182300	3.866317
-6.277284	-22.461555	3.876314
-5.624485	-19.215820	3.886310
-4.900008	-8.777376	3.896307
-4.794358	-3.363439	3.906304
-4.644628	-9.400853	3.916301
-4.137451	8.500211	3.926298
-3.375652	23.173998	3.936294
-2.873260	32.656607	3.946291
-2.687138	48.571418	3.956288
-2.210105	73.130182	3.966285
-1.771565	91.399948	3.976282
-1.481102	99.243914	3.986278
-0.769901	121.507291	3.996275
0.000000	148.353887	4.001280
-0.014355	159.146578	4.006285
0.258142	145.189246	4.011290
0.002455	172.140768	4.016294
-0.011453	170.756187	4.021299
0.426726	176.672747	4.026304
0.641763	191.634760	4.031309
0.733527	175.498850	4.036314
0.757274	195.967996	4.041318
0.928327	195.149958	4.046323
0.925965	179.784349	4.051328
0.468566	196.407145	4.056333
0.979904	187.639109	4.061338
0.874882	186.294837	4.066342
0.569051	172.296725	4.071347
0.382902	179.822314	4.076352
0.918738	191.439846	4.081357
1.008490	182.505619	4.086362
0.707384	178.597947	4.091366
0.398875	165.142055	4.096371
0.645459	177.350431	4.101376
0.790333	186.807483	4.106381
0.912112	174.390551	4.111386
1.079936	198.911601	4.116390
0.916145	199.077171	4.121395
1.017162	194.158393	4.126400
0.818118	184.803415	4.131405
0.709423	171.773896	4.136410
0.861596	194.131034	4.141414
0.996643	176.626833	4.146419
0.984126	191.024013	4.151424
0.903023	174.205424	4.156429
0.924443	179.991494	4.161434
0.652271	196.457706	4.166438
0.949603	196.306963	4.171443
1.075941	181.455937	4.176448
0.810306	203.991143	4.181453
1.238025	185.187715	4.186458
0.923609	192.182675	4.191462
0.850038	188.231184	4.196467
0.903782	203.504067	4.201472
0.650994	211.046011	4.206477
0.920796	188.714408	4.211482
0.996929	200.414922	4.216486
1.073926	202.817679	4.221491
1.319060	190.390312	4.226496
1.254461	193.289779	4.231501
1.237333	209.561840	4.236506
1.056292	198.805452	4.241510
1.325105	186.918116	4.246515
1.632431	201.019479	4.251520
0.988395	205.872829	4.256525
1.250936	199.973829	4.261530
1.047972	205.183206	4.266534
1.261631	207.538817	4.271539
1.235204	198.924457	4.276544
1.253417	200.944608	4.281549
1.226935	186.983575	4.286554
1.184135	197.107727	4.291558
1.313832	207.517372	4.296563
1.168947	212.261106	4.301568
0.779814	212.024246	4.306573
0.986423	216.116528	4.311578
1.045670	210.591948	4.316582
1.139905	218.185453	4.321587
1.078379	197.580077	4.326592
0.964743	215.038545	4.331597
1.150380	208.737340	4.336602
1.586766	224.403154	4.341606
1.455925	228.635057	4.346611
1.541049	227.990139	4.351616
1.106828	236.645724	4.356621
1.650179	237.837659	4.361626
1.328408	249.266100	4.366630
1.305001	240.869526	4.371635
1.433726	219.207730	4.376640
1.195194	221.441270	4.381645
1.522862	236.666846	4.386650
1.451023	232.007457	4.391654
1.399155	249.800728	4.396659
1.545022	242.739095	4.401664
1.405877	240.064768	4.406669
1.458674	246.548740	4.411674
1.585825	235.258710	4.416678
1.260274	239.635845	4.421683
2.002105	230.500111	4.426688
1.471767	230.802315	4.431693
1.252620	238.807289	4.436698
0.972364	241.644152	4.441702
1.391879	251.564582	4.446707
1.885613	250.624457	4.451712
1.937439	270.401290	4.456717
1.760822	243.036877	4.461722
1.500540	244.681143	4.466726
1.434800	244.198277	4.471731
1.727442	251.156074	4.476736
1.720635	267.763670	4.481741
2.062798	261.668694	4.486746
2.225976	240.198865	4.491750
1.707244	248.472944	4.496755
1.643934	217.471552	4.501760
1.560986	244.340201	4.506765
1.717812	251.980496	4.511770
2.165676	257.606845	4.516774
2.036871	246.292716	4.521779
1.829500	248.913630	4.526784
1.859179	247.617823	4.531789
1.968213	225.121062	4.536794
1.865887	242.373591	4.541798
1.718171	236.073110	4.546803
1.595784	231.967005	4.551808
1.847807	263.411048	4.556813
2.010726	254.793776	4.561818
2.315882	267.072745	4.566822
1.845650	249.461428	4.571827
1.975838	246.348590	4.576832
1.976606	239.339151	4.581837
2.176533	252.279866	4.586842
1.765979	242.964344	4.591846
1.425997	268.567247	4.596851
2.013053	253.379089	4.601856
1.692359	274.356477	4.606861
1.399697	272.987767	4.611866
1.812208	253.907201	4.616870
1.764916	269.559279	4.621875
1.782986	262.850608	4.626880
2.041087	271.667815	4.631885
2.425458	294.907310	4.636890
2.534057	274.349575	4.641894
2.110497	273.877208	4.646899
2.432985	261.811763	4.651904
2.151156	280.447151	4.656909
2.112153	273.317605	4.661914
1.758137	257.566513	4.666918
1.973265	284.214226	4.671923
2.363535	273.275770	4.676928
2.449102	288.893482	4.681933
2.368517	267.772568	4.686938
2.336838	284.368114	4.691942
2.272330	276.906688	4.696947
2.188437	265.271028	4.701952
2.019477	283.171978	4.706957
2.258656	274.655340	4.711962
2.629106	293.111132	4.716966
2.325914	274.469621	4.721971
2.434193	264.938621	4.726976
1.855082	282.272553	4.731981
2.332070	284.024732	4.736986
2.652305	307.000898	4.741990
2.353228	299.057069	4.746995
2.428192	302.305691	4.752000
2.191211	298.355429	4.757005
2.467791	309.844348	4.762010
2.415996	301.010488	4.767014
2.256995	301.903192	4.772019
2.607256	301.109986	4.777024
2.377868	310.892060	4.782029
2.248957	308.365778	4.787034
2.476253	306.353083	4.792038
2.203567	308.900457	4.797043
2.370786	291.849423	4.802048
2.346123	299.092490	4.807053
2.398556	293.031375	4.812058
2.636350	283.100546	4.817062
2.207080	305.015811	4.822067
2.573441	303.789938	4.827072
2.472363	304.455254	4.832077
2.391293	297.168894	4.837082
2.787313	314.898086	4.842086
2.609969	317.387780	4.847091
2.624717	336.158597	4.852096
2.354600	317.879722	4.857101
3.030037	310.311582	4.862106
2.807527	336.826721	4.867110
2.795497	313.746209	4.872115
2.958903	310.141139	4.877120
2.346052	317.894163	4.882125
2.831492	319.301752	4.887130
3.182985	325.909029	4.892134
2.882982	320.005387	4.897139
2.768253	297.905368	4.902144
2.432557	309.664555	4.907149
2.494531	287.549455	4.912154
2.937852	322.105324	4.917158
2.793658	342.733327	4.922163
3.067427	323.340494	4.927168
3.003214	347.378675	4.932173
2.552566	328.526289	4.937178
3.108237	335.657387	4.942182
2.612415	339.245980	4.947187
2.858320	323.735223	4.952192
2.954353	339.147844	4.957197
2.686554	339.080728	4.962202
2.986071	327.959244	4.967206
2.700638	353.970952	4.972211
2.759651	331.869793	4.977216
3.056651	347.243193	4.982221
2.944092	338.468283	4.987226
2.914996	343.162735	4.992230
2.834320	330.807052	4.997235
3.278989	347.028197	5.002240
3.055287	340.207332	5.007245
2.986271	322.962197	5.012250
3.059521	343.823477	5.017254
2.906099	337.860584	5.022259
3.220218	326.018232	5.027264
3.294480	351.416287	5.032269
3.265773	326.769114	5.037274
3.351008	342.890043	5.042278
3.193764	343.356199	5.047283
3.148419	323.471466	5.052288
3.099837	351.300883	5.057293
2.919757	335.890600	5.062298
3.304609	338.276832	5.067302
3.050649	339.603500	5.072307
3.075752	338.531288	5.077312
3.042183	347.127430	5.082317
2.860443	329.121102	5.087322
3.178836	332.847208	5.092326
2.988132	338.007450	5.097331
3.459521	344.414000	5.102336
2.865220	344.183716	5.107341
3.201066	350.538091	5.112346
3.789432	372.030863	5.117350
3.602082	360.605283	5.122355
3.430220	352.231109	5.127360
3.246840	340.223653	5.132365
2.831279	353.186164	5.137370
3.398721	351.749588	5.142374
3.299429	375.266531	5.147379
3.485007	373.849358	5.152384
3.363718	366.481123	5.157389
3.397533	360.515590	5.162394
3.364252	378.899408	5.167398
3.271490	386.771015	5.172403
3.680787	369.691726	5.177408
3.255502	384.607041	5.182413
3.194397	366.558832	5.187418
3.407835	372.447503	5.192422
3.414047	378.593170	5.197427
3.568419	367.911546	5.202432
3.661290	381.407893	5.207437
3.669293	374.937791	5.212442
3.556554	372.503824	5.217446
3.300352	382.977856	5.222451
3.617467	367.875628	5.227456
3.542571	375.194213	5.232461
3.133528	368.057412	5.237466
3.745010	381.360428	5.242470
3.678842	376.093567	5.247475
3.733295	364.415930	5.252480
3.799952	383.128211	5.257485
3.462627	373.391116	5.262490
3.598775	376.264445	5.267494
3.831209	375.096508	5.272499
3.968859	375.694853	5.277504
3.587256	378.415412	5.282509
3.347569	353.324321	5.287514
3.773719	379.716947	5.292518
3.550162	388.328134	5.297523
3.936244	390.131356	5.302528
3.668451	401.233735	5.307533
3.617163	399.938866	5.312538
3.719047	411.279756	5.317542
3.769554	401.746972	5.322547
3.754595	390.772214	5.327552
3.616390	406.477733	5.332557
3.532382	386.390863	5.337562
3.591863	402.875684	5.342566
3.500577	397.968595	5.347571
3.729954	396.002207	5.352576
3.404028	398.705084	5.357581
3.809904	414.923341	5.362586
3.772148	428.904178	5.367590
3.755827	434.049839	5.372595
4.287529	437.570055	5.377600
4.095276	422.391944	5.382605
4.113970	436.461910	5.387610
4.426681	442.730672	5.392614
4.033228	435.291469	5.397619
3.930256	406.878088	5.402624
3.968934	421.019908	5.407629
4.243497	436.847635	5.412634
4.352455	425.330620	5.417638
4.006549	413.897663	5.422643
4.191300	412.776669	5.427648
3.893710	403.213712	5.432653
4.059331	425.646209	5.437658
4.082809	425.439311	5.442662
3.843856	436.613797	5.447667
4.259162	416.821603	5.452672
4.044220	432.824925	5.457677
4.033300	426.912532	5.462682
3.904764	429.565334	5.467686
4.066579	449.458581	5.472691
4.163107	431.536560	5.477696
4.336750	449.162775	5.482701
4.354967	448.939384	5.487706
4.154034	429.342632	5.492710
4.272051	438.602442	5.497715
4.755764	426.662143	5.502720
4.398282	441.072668	5.507725
4.286656	435.995010	5.512730
4.538261	424.630016	5.517734
4.474204	444.916708	5.522739
4.216680	433.111331	5.527744
4.367888	446.394385	5.532749
4.581715	436.679315	5.537754
4.597589	419.880536	5.542758
4.115810	437.007671	5.547763
4.424052	422.573131	5.552768
4.355665	432.169357	5.557773
4.459214	436.515488	5.562778
4.275933	427.230361	5.567782
4.511439	443.453720	5.572787
4.448913	429.153348	5.577792
4.767075	432.915129	5.582797
4.406607	441.947613	5.587802
4.607923	436.174455	5.592806
4.365642	441.845575	5.597811
4.648001	430.208551	5.602816
4.109877	431.432932	5.607821
4.271627	447.592031	5.612826
4.537008	431.327820	5.617830
4.476508	429.613042	5.622835
4.444543	432.903532	5.627840
4.179344	428.253843	5.632845
4.722548	439.906552	5.637850
4.629293	445.011167	5.642854
4.493886	432.515683	5.647859
4.506894	421.336715	5.652864
4.500906	441.496118	5.657869
4.718403	464.239030	5.662874
4.796081	451.237563	5.667878
4.622787	474.422208	5.672883
4.876768	472.876527	5.677888
4.735869	464.228948	5.682893
4.737756	474.053501	5.687898
5.023269	467.861363	5.692902
4.488139	467.103292	5.697907
4.719489	463.427078	5.702912
5.000828	472.184824	5.707917
4.717201	474.370511	5.712922
4.977500	461.972971	5.717926
4.690788	467.874983	5.722931
4.702733	474.600489	5.727936
4.491004	459.219975	5.732941
4.373990	457.512659	5.737946
4.709977	475.477570	5.742950
4.427939	477.812251	5.747955
4.976418	474.445076	5.752960
4.918325	478.666900	5.757965
4.930882	477.756563	5.762970
4.936340	482.169623	5.767974
4.806547	469.154385	5.772979
4.994196	451.823086	5.777984
4.965828	478.096361	5.782989
4.939100	463.229418	5.787994
4.985373	465.863991	5.792998
4.886464	482.408614	5.798003
4.975078	480.631701	5.803008
5.248595	493.254545	5.808013
4.869508	495.992960	5.813018
5.208149	496.201377	5.818022
4.668119	502.866984	5.823027
5.334270	495.644181	5.828032
5.343812	491.634483	5.833037
5.102149	497.964796	5.838042
5.284445	495.773856	5.843046
4.936945	490.587581	5.848051
5.270074	499.466015	5.853056
5.368044	501.404168	5.858061
4.790892	518.630811	5.863066
5.283590	504.578163	5.868070
4.807528	510.485341	5.873075
5.307157	499.669326	5.878080
5.202607	510.065902	5.883085
4.995302	504.913473	5.888090
5.261201	500.644478	5.893094
5.180086	518.023338	5.898099
5.361662	498.393865	5.903104
5.456173	495.030384	5.908109
5.299813	495.112555	5.913114
5.179413	496.297996	5.918118
5.128628	506.699791	5.923123
5.206472	497.599052	5.928128
5.213707	508.265603	5.933133
5.120712	499.876441	5.938138
5.531128	505.388422	5.943142
4.782869	522.773662	5.948147
5.013434	500.797999	5.953152
5.477666	526.683249	5.958157
5.384017	523.436782	5.963162
5.548281	526.843034	5.968166
5.530523	544.069696	5.973171
5.578030	525.985098	5.978176
5.441104	537.195280	5.983181
5.416196	542.251836	5.988186
5.613097	525.279685	5.993190
5.702124	537.253559	5.998195
5.486920	531.290342	6.003200
5.481571	538.020412	6.008205
5.604697	525.803822	6.013210
5.567425	534.260303	6.018214
5.883445	553.090015	6.023219
5.563401	515.885625	6.028224
5.414223	520.101797	6.033229
5.263792	516.312574	6.038234
5.896156	528.976374	6.043238
5.576759	509.961004	6.048243
5.713944	518.294534	6.053248
5.376416	505.026033	6.058253
5.105291	501.047032	6.063258
5.317330	520.240441	6.068262
5.314232	538.256433	6.073267
5.877602	524.792073	6.078272
6.003401	549.419084	6.083277
5.269639	528.861909	6.088282
5.455633	530.012008	6.093286
5.289160	527.207292	6.098291
5.653062	509.907075	6.103296
5.761653	530.896538	6.108301
5.659566	539.157557	6.113306
5.650192	523.234010	6.118310
5.513294	523.220135	6.123315
5.608777	517.426062	6.128320
5.593547	505.582461	6.133325
5.067543	513.359704	6.138330
5.821906	528.069356	6.143334
5.704310	518.935697	6.148339
5.580182	522.575068	6.153344
5.618993	500.415941	6.158349
5.149212	513.736866	6.163354
5.530285	512.910837	6.168358
5.297771	533.492727	6.173363
5.450360	524.236874	6.178368
6.020641	525.859625	6.183373
5.529934	515.296935	6.188378
5.559643	512.676830	6.193382
5.424919	518.315012	6.198387
5.533849	518.342884	6.203392
5.551949	528.841034	6.208397
5.627323	539.138152	6.213402
5.603774	521.369539	6.218406
5.406274	523.723401	6.223411
5.668244	531.159914	6.228416
5.392962	511.116328	6.233421
5.237196	528.827457	6.238426
5.759576	529.228162	6.243430
5.717867	530.668434	6.248435
5.506490	534.879600	6.253440
5.407057	512.923137	6.258445
5.629418	525.104523	6.263450
5.740179	520.121783	6.268454
5.613708	499.837084	6.273459
5.282363	509.467048	6.278464
5.615303	514.800654	6.283469
5.321298	533.666735	6.288474
5.596584	525.080165	6.293478
5.360231	547.326532	6.298483
5.585222	536.673369	6.303488
5.682622	554.490270	6.308493
5.586162	548.156428	6.313498
5.693455	528.940201	6.318502
5.780193	521.700285	6.323507
5.065460	488.605818	6.328512
5.622842	520.951006	6.333517
5.719180	529.835738	6.338522
5.852102	528.334325	6.343526
5.807521	534.765558	6.348531
5.707178	514.826922	6.353536
5.932407	502.216342	6.358541
5.794046	517.517439	6.363546
5.712791	493.895954	6.368550
5.482902	506.348673	6.373555
5.764773	504.718079	6.378560
5.683391	502.053790	6.383565
5.627800	515.903294	6.388570
5.561208	508.082522	6.393574
5.649373	511.139502	6.398579
5.536932	511.767837	6.403584
5.550764	514.993954	6.408589
5.481728	514.071943	6.413594
5.565945	489.885775	6.418598
5.364109	506.796555	6.423603
5.356985	495.450590	6.428608
5.493938	509.567078	6.433613
5.408488	497.094163	6.438618
5.611497	507.287101	6.443622
5.445503	520.369112	6.448627
5.326839	505.187339	6.453632
5.583007	505.121527	6.458637
5.412796	501.909124	6.463642
5.743166	508.261412	6.468646
5.674888	503.954221	6.473651
5.746833	499.957391	6.478656
5.699047	501.981091	6.483661
5.411404	501.304542	6.488666
5.626577	502.971080	6.493670
5.804756	496.474381	6.498675
5.457668	505.038671	6.503680
5.882895	523.253073	6.508685
5.609514	501.287198	6.513690
5.865235	488.799735	6.518694
5.378576	492.869341	6.523699
4.929756	479.225054	6.528704
5.483709	496.957163	6.533709
5.380686	523.251435	6.538714
5.219873	513.148686	6.543718
5.357577	510.152340	6.548723
5.440498	515.084329	6.553728
5.294277	505.554792	6.558733
5.165438	524.000349	6.563738
5.521521	495.544973	6.568742
5.416115	514.586731	6.573747
5.337818	517.472443	6.578752
5.595631	502.135430	6.583757
5.566287	517.747802	6.588762
5.605902	512.578635	6.593766
5.492101	511.753694	6.598771
5.140535	513.046295	6.603776
5.504314	507.115650	6.608781
5.417134	533.043994	6.613786
5.739784	517.548080	6.618790
5.780445	521.017572	6.623795
5.823491	529.181401	6.628800
5.604937	522.542500	6.633805
4.909289	518.996977	6.638810
5.320092	519.447985	6.643814
5.573076	540.498340	6.648819
5.531500	538.863682	6.653824
5.354165	532.069298	6.658829
5.589297	535.123206	6.663834
5.374031	543.310791	6.668838
5.678473	537.830806	6.673843
5.690955	543.741802	6.678848
5.835781	538.580690	6.683853
5.663152	544.782812	6.688858
5.266749	521.362821	6.693862
5.434293	531.299228	6.698867
5.680990	543.347377	6.703872
5.634859	527.846892	6.708877
5.598674	546.796655	6.713882
5.679622	516.699602	6.718886
5.606536	512.648705	6.723891
5.474735	531.748906	6.728896
5.488622	519.558070	6.733901
5.306247	526.150572	6.738906
5.395954	533.579843	6.743910
5.473760	536.038653	6.748915
5.588431	535.355200	6.753920
5.671475	531.154986	6.758925
5.433631	556.938989	6.763930
5.562732	540.461214	6.768934
5.811723	549.992239	6.773939
5.792124	537.420216	6.778944
5.796261	505.179498	6.783949
5.486136	512.049989	6.788954
5.609537	501.972588	6.793958
5.668309	513.144588	6.798963
5.767917	523.781975	6.803968
5.608552	515.957986	6.808973
5.650130	516.121582	6.813978
5.350452	520.581924	6.818982
5.118518	508.020155	6.823987
5.218143	518.632183	6.828992
5.611742	516.717362	6.833997
5.281907	519.588117	6.839002
5.657104	510.092957	6.844006
5.537220	521.998155	6.849011
5.307590	529.266720	6.854016
5.868087	518.236330	6.859021
5.605369	536.662004	6.864026
5.760434	502.249636	6.869030
5.413508	516.320021	6.874035
5.237527	520.893394	6.879040
5.446752	520.709364	6.884045
5.399251	548.177312	6.889050
5.741421	539.525719	6.894054
5.514789	552.154815	6.899059
5.549523	540.643765	6.904064
5.744681	519.604290	6.909069
5.392909	529.194729	6.914074
5.485070	507.028157	6.919078
5.595460	532.318833	6.924083
5.719840	521.716835	6.929088
5.542375	522.148753	6.934093
5.458817	513.838028	6.939098
5.675514	515.111593	6.944102
5.958024	521.777805	6.949107
5.852594	520.088199	6.954112
5.548435	513.127942	6.959117
5.550517	523.296584	6.964122
5.660482	508.337953	6.969126
5.478048	519.812524	6.974131
5.466026	507.261963	6.979136
5.722466	516.687957	6.984141
5.618682	510.268825	6.989146
5.811086	514.166829	6.994150
5.928828	506.274359	6.999155
5.512378	510.034447	7.004160
5.644537	517.036349	7.009165
5.311024	514.297911	7.014170
5.484679	517.850979	7.019174
5.429108	522.404945	7.024179
5.156699	513.982388	7.029184
5.387677	517.578859	7.034189
5.101657	504.540775	7.039194
5.483705	518.529264	7.044198
5.628640	506.174824	7.049203
5.125755	505.120998	7.054208
5.448863	517.042558	7.059213
5.336644	533.309271	7.064218
5.398360	530.434388	7.069222
5.538975	529.738066	7.074227
5.607696	552.031686	7.079232
5.771433	534.190575	7.084237
5.753243	547.279258	7.089242
5.916555	511.554847	7.094246
5.601795	531.198654	7.099251
5.392079	533.533032	7.104256
5.728373	510.141624	7.109261
5.728956	522.900850	7.114266
5.429369	514.762751	7.119270
5.446891	501.857403	7.124275
5.505344	528.207567	7.129280
5.638797	506.413873	7.134285
5.021756	514.433252	7.139290
5.442580	515.353951	7.144294
5.729654	513.506750	7.149299
5.577855	530.000877	7.154304
5.417170	503.411020	7.159309
5.322170	516.589217	7.164314
5.598826	515.830756	7.169318
5.640899	515.563074	7.174323
5.671196	527.068095	7.179328
5.667654	511.254678	7.184333
5.621099	518.440798	7.189338
5.902580	505.259800	7.194342
5.908342	515.283998	7.199347
5.277559	521.439599	7.204352
5.261921	513.409060	7.209357
5.033315	531.906727	7.214362
5.350235	517.742640	7.219366
5.729045	512.677130	7.224371
5.712944	527.712099	7.229376
5.763215	506.717304	7.234381
5.516341	525.098517	7.239386
5.647107	520.154101	7.244390
5.558973	521.652947	7.249395
5.406019	522.005643	7.254400
5.777970	506.567490	7.259405
5.372587	520.714029	7.264410
5.425805	512.825906	7.269414
5.641841	512.225338	7.274419
5.089905	516.484394	7.279424
5.246472	510.465962	7.284429
5.666885	532.456878	7.289434
5.681937	529.363899	7.294438
5.761868	529.241091	7.299443
5.384936	526.158536	7.304448
5.790333	508.604839	7.309453
5.546664	527.240337	7.314458
5.781343	511.811250	7.319462
5.772843	525.233423	7.324467
5.701663	525.962370	7.329472
5.783788	517.085439	7.334477
5.539263	527.752571	7.339482
5.576525	506.660783	7.344486
5.657051	517.777894	7.349491
5.606214	516.757087	7.354496
5.812105	515.554560	7.359501
5.423078	524.087416	7.364506
5.636685	515.348077	7.369510
5.611880	504.913983	7.374515
5.631658	515.425659	7.379520
5.728880	501.244427	7.384525
5.447650	518.007936	7.389530
5.879581	527.021089	7.394534
5.678395	509.722021	7.399539
5.771764	524.062160	7.404544
6.096418	499.460290	7.409549
5.645851	498.044457	7.414554
5.519871	462.638565	7.419558
5.382897	463.699978	7.424563
5.148652	477.321694	7.429568
5.873235	464.310379	7.434573
5.500943	474.642960	7.439578
5.523630	481.066307	7.444582
5.514592	472.300650	7.449587
5.261503	473.262479	7.454592
5.306667	483.966051	7.459597
5.673185	498.803597	7.464602
5.481864	500.421005	7.469606
5.527652	499.957285	7.474611
5.621682	502.752464	7.479616
5.458390	509.185743	7.484621
5.179067	508.682329	7.489626
5.388925	512.012581	7.494630
5.845759	503.420584	7.499635
5.570471	502.234442	7.504640
5.600304	512.206815	7.509645
5.621238	505.631530	7.514650
5.371026	503.512460	7.519654
5.682511	505.570603	7.524659
5.253909	516.560841	7.529664
5.668281	508.410015	7.534669
5.380733	512.062877	7.539674
5.397914	517.883908	7.544678
5.598126	506.437083	7.549683
5.324781	499.432280	7.554688
5.367768	509.600763	7.559693
5.383667	510.335738	7.564698
5.377704	521.830274	7.569702
5.625738	524.504021	7.574707
5.528793	512.834619	7.579712
5.649374	518.211904	7.584717
5.390867	510.769599	7.589722
5.450054	503.420994	7.594726
5.868492	507.640232	7.599731
5.582904	502.572558	7.604736
5.754763	502.776378	7.609741
5.434701	503.299337	7.614746
5.630851	518.772146	7.619750
5.489872	513.121030	7.624755
5.571695	520.355878	7.629760
5.406814	507.472382	7.634765
5.578750	518.739823	7.639770
5.574582	518.570342	7.644774
5.629202	521.976167	7.649779
5.899854	510.507242	7.654784
5.543808	508.364820	7.659789
5.473165	522.336478	7.664794
5.482219	509.160842	7.669798
5.661643	520.905497	7.674803
5.468721	510.893091	7.679808
5.839213	517.791978	7.684813
5.541851	511.714201	7.689818
5.928559	496.600839	7.694822
5.693363	502.397674	7.699827
5.140234	480.670920	7.704832
5.454678	494.218349	7.709837
5.527337	507.350482	7.714842
5.711661	514.544908	7.719846
5.575905	513.120157	7.724851
5.321351	484.354940	7.729856
5.550092	498.368155	7.734861
5.428003	509.782040	7.739866
5.726275	512.371226	7.744870
5.645714	507.826740	7.749875
5.240827	498.859344	7.754880
5.673642	509.087405	7.759885
5.530612	504.946954	7.764890
5.533995	522.728747	7.769894
5.367061	524.455277	7.774899
5.134357	511.783640	7.779904
5.333235	504.273248	7.784909
5.382857	520.682979	7.789914
5.472732	503.895947	7.794918
5.666393	517.389964	7.799923
5.430549	520.975193	7.804928
5.639434	507.889352	7.809933
5.474025	530.947099	7.814938
5.359251	513.067006	7.819942
5.662848	509.185587	7.824947
5.155507	519.037108	7.829952
5.490009	514.972912	7.834957
5.525335	514.704964	7.839962
6.020896	508.456888	7.844966
5.590772	514.403630	7.849971
5.288140	519.507161	7.854976
5.352253	528.017220	7.859981
5.421577	525.755667	7.864986
5.325140	509.483889	7.869990
5.482779	513.342061	7.874995
5.416950	530.562839	7.880000
5.544621	524.558154	7.885005
5.160213	514.913489	7.890010
5.119055	515.200852	7.895014
5.394130	513.002074	7.900019
5.564203	547.859311	7.905024
5.869980	552.815744	7.910029
5.793521	544.609877	7.915034
5.850294	532.613187	7.920038
5.934446	524.179938	7.925043
5.433242	521.216374	7.930048
5.661947	525.700672	7.935053
5.442403	512.576918	7.940058
5.656062	517.813437	7.945062
5.663777	514.975104	7.950067
5.475433	514.638170	7.955072
5.702689	519.082063	7.960077
5.665021	515.677878	7.965082
5.235603	531.420700	7.970086
5.484103	534.024823	7.975091
5.357644	516.278947	7.980096
5.458090	509.033811	7.985101
5.432998	515.328241	7.990106
5.230084	509.913072	7.995110
5.334331	524.064374	8.000115
5.359381	531.913629	8.005133
5.746259	530.388290	8.010150
5.521345	536.808241	8.015168
5.480566	522.030207	8.020186
5.551670	531.158932	8.025203
5.727711	536.160928	8.030221
5.787143	516.131669	8.035238
5.665829	528.095937	8.040256
5.347658	518.077699	8.045274
5.539526	524.273099	8.050291
5.015163	520.435161	8.055309
6.090957	547.708428	8.060326
5.596225	548.363359	8.065344
5.838577	530.010761	8.070362
5.374383	526.780029	8.075379
5.361237	533.865474	8.080397
5.874834	542.055671	8.085414
6.138292	550.356973	8.090432
5.712070	533.248996	8.095450
5.772620	507.382602	8.100467
5.377988	526.537684	8.105485
5.390626	512.083713	8.110502
5.934181	524.911651	8.115520
5.371773	513.390604	8.120538
5.478195	529.553264	8.125555
5.299725	538.893566	8.130573
5.386266	530.369124	8.135590
5.567976	545.582711	8.140608
5.505746	541.636316	8.145626
6.049287	540.784400	8.150643
5.892147	559.870068	8.155661
5.901754	558.611546	8.160678
6.158115	548.032031	8.165696
5.831508	553.659863	8.170714
5.834291	525.139349	8.175731
5.787636	525.956777	8.180749
5.683015	526.013527	8.185766
5.825291	513.343634	8.190784
5.905688	520.501090	8.195802
5.878399	508.864750	8.200819
5.884903	522.505547	8.205837
5.813047	507.971083	8.210854
6.041471	521.555033	8.215872
5.935096	522.038726	8.220890
5.996870	535.744497	8.225907
5.801620	534.818567	8.230925
5.763861	507.499239	8.235942
5.605750	526.780246	8.240960
5.312598	519.005477	8.245978
5.616673	519.618035	8.250995
5.521213	524.914136	8.256013
5.692717	515.122764	8.261030
5.629310	520.607411	8.266048
5.432832	523.137613	8.271066
5.959062	532.579304	8.276083
6.007870	541.713295	8.281101
5.940674	525.853703	8.286118
5.804738	529.381693	8.291136
5.670437	519.916468	8.296154
5.918901	536.597736	8.301171
5.550757	543.023056	8.306189
5.905823	541.901091	8.311206
5.749233	561.427395	8.316224
5.714164	552.974993	8.321242
5.919259	568.765679	8.326259
5.611526	555.677243	8.331277
5.953084	557.813993	8.336294
5.832989	556.778031	8.341312
5.890133	561.567071	8.346330
6.236271	541.149449	8.351347
5.986438	559.193739	8.356365
6.112305	542.707409	8.361382
6.473077	545.049881	8.366400
5.862615	544.833829	8.371418
5.972293	522.604147	8.376435
5.863895	538.899536	8.381453
5.644945	535.325896	8.386470
5.945715	530.749493	8.391488
6.017726	543.602930	8.396506
5.943844	522.577963	8.401523
5.758610	543.441876	8.406541
5.904895	551.466660	8.411558
6.001251	542.091908	8.416576
5.975519	556.775670	8.421594
6.097575	545.426347	8.426611
6.224118	568.704032	8.431629
6.063445	552.990534	8.436646
6.088121	530.812868	8.441664
5.677303	533.065098	8.446682
5.495872	530.641237	8.451699
5.752925	556.294801	8.456717
5.947794	540.417470	8.461734
6.006970	559.653164	8.466752
6.071093	547.492674	8.471770
6.335606	560.251237	8.476787
6.235323	550.548643	8.481805
5.930544	562.937245	8.486822
6.269327	542.829708	8.491840
6.066020	557.936508	8.496858
6.448798	554.659965	8.501875
6.401870	550.472129	8.506893
5.878375	544.679167	8.511910
5.942749	531.501901	8.516928
5.904927	546.658291	8.521946
6.103844	540.581029	8.526963
6.056806	554.086846	8.531981
6.072560	559.766241	8.536998
5.980665	556.793376	8.542016
5.826662	570.169090	8.547034
5.999592	556.942376	8.552051
6.137779	563.851785	8.557069
6.444455	563.395214	8.562087
6.352332	546.108423	8.567104
5.832131	569.101660	8.572122
6.287834	548.699476	8.577139
6.220367	552.688466	8.582157
6.291121	559.480411	8.587175
6.339566	545.264125	8.592192
6.230507	562.879066	8.597210
5.914684	563.321902	8.602227
6.068356	569.075922	8.607245
6.131905	560.015748	8.612263
6.126685	566.883521	8.617280
5.827983	568.153024	8.622298
6.026481	537.855348	8.627315
6.047280	550.230084	8.632333
5.843584	551.905028	8.637351
6.273437	553.780503	8.642368
5.773429	556.695230	8.647386
5.828201	562.527189	8.652403
5.754615	577.062131	8.657421
5.699306	585.892379	8.662439
6.013923	579.775612	8.667456
5.575254	597.778734	8.672474
6.005834	605.243809	8.677491
5.956237	583.751093	8.682509
5.855287	598.957915	8.687527
6.383374	607.181666	8.692544
6.392383	620.213051	8.697562
6.439363	625.106321	8.702579
6.405941	615.432685	8.707597
6.024706	612.055878	8.712615
6.321481	605.887340	8.717632
6.181191	626.208551	8.722650
6.248649	644.368570	8.727667
6.364890	624.621337	8.732685
5.992028	626.405031	8.737703
6.096871	623.608835	8.742720
6.241297	620.110814	8.747738
6.132357	632.128321	8.752755
6.420747	630.060050	8.757773
6.298450	643.832940	8.762791
6.583686	634.753601	8.767808
6.509265	624.104028	8.772826
6.311676	621.623094	8.777843
6.384927	630.368065	8.782861
6.257306	626.395457	8.787879
6.240209	627.677761	8.792896
6.258610	644.960497	8.797914
6.504717	628.567756	8.802931
6.382668	639.096501	8.807949
6.482312	626.333094	8.812967
6.538143	636.935562	8.817984
6.345760	623.380194	8.823002
6.428194	623.945648	8.828019
6.635847	620.247368	8.833037
6.340908	608.485151	8.838055
6.519891	624.963784	8.843072
6.658497	619.450442	8.848090
6.598615	621.825052	8.853107
6.486746	637.005377	8.858125
6.374986	630.352231	8.863143
6.503566	631.743101	8.868160
6.468665	617.937855	8.873178
6.532016	605.991660	8.878195
6.609299	631.888976	8.883213
6.549690	616.005505	8.888231
6.653868	615.492461	8.893248
6.462640	628.866113	8.898266
6.307283	629.954887	8.903283
6.651442	619.229551	8.908301
5.986184	641.491365	8.913319
6.327991	627.318820	8.918336
6.468341	630.314691	8.923354
6.196235	626.657516	8.928371
6.478496	605.834533	8.933389
6.179557	623.394923	8.938407
6.753539	623.903251	8.943424
6.467211	637.651880	8.948442
6.741734	648.947349	8.953459
6.742446	625.794638	8.958477
6.684420	630.136421	8.963495
6.888915	623.894962	8.968512
6.708211	619.729313	8.973530
6.590228	628.241095	8.978547
6.532772	615.468335	8.983565
6.756123	628.455843	8.988583
6.797942	618.223659	8.993600
6.470651	627.437763	8.998618
6.474326	623.694275	9.003635
6.884021	624.567261	9.008653
6.803589	645.014198	9.013671
6.894543	614.826637	9.018688
6.858051	641.352449	9.023706
6.480669	630.862555	9.028723
6.673847	611.811683	9.033741
6.419956	631.542884	9.038759
6.647962	632.058402	9.043776
6.368448	626.241915	9.048794
6.824022	637.584599	9.053811
6.614699	639.498410	9.058829
6.317774	633.613852	9.063847
6.427536	623.684032	9.068864
6.803878	643.863702	9.073882
6.982280	656.761050	9.078899
7.044194	653.684816	9.083917
6.687198	628.558004	9.088935
6.837579	622.411686	9.093952
6.940310	634.926156	9.098970
6.817354	614.644015	9.103987
6.733998	619.125869	9.109005
6.735025	613.659570	9.114023
6.769459	628.320863	9.119040
6.740832	638.786740	9.124058
6.398093	624.881221	9.129075
6.936869	625.834618	9.134093
6.721636	640.845269	9.139111
7.018772	661.853974	9.144128
6.846458	641.789936	9.149146
6.637597	649.378223	9.154163
7.208889	634.206982	9.159181
6.768050	647.208331	9.164199
6.757628	629.452949	9.169216
6.895219	621.014878	9.174234
6.829295	635.731138	9.179251
6.934853	623.886685	9.184269
6.890936	633.301336	9.189287
6.544367	610.858914	9.194304
7.091681	646.995163	9.199322
6.695802	648.598264	9.204339
7.265494	649.871959	9.209357
6.877115	637.561436	9.214375
6.890871	647.543180	9.219392
7.135559	652.100915	9.224410
6.769018	631.877012	9.229427
6.830941	629.424825	9.234445
6.519087	636.279443	9.239463
6.914242	655.677687	9.244480
7.188749	648.515443	9.249498
6.795006	655.485544	9.254515
7.414585	647.455961	9.259533
7.093209	663.956219	9.264551
7.056381	661.037307	9.269568
6.932679	634.237431	9.274586
6.946099	640.266556	9.279603
6.902907	653.044462	9.284621
6.724208	655.082314	9.289639
7.048692	673.850405	9.294656
7.326181	657.709464	9.299674
6.757186	663.492028	9.304691
7.282150	648.090796	9.309709
7.267819	658.565247	9.314727
7.052412	661.729533	9.319744
7.012316	641.454818	9.324762
6.972776	658.896515	9.329779
7.204007	656.438877	9.334797
7.098045	662.987114	9.339815
7.036293	662.778679	9.344832
6.862926	643.035594	9.349850
6.889123	661.253028	9.354867
7.194993	662.974644	9.359885
7.090687	654.267952	9.364903
7.192662	676.213410	9.369920
7.414130	662.737703	9.374938
7.063827	659.016888	9.379955
7.204585	647.693525	9.384973
6.995545	653.320463	9.389991
6.949490	650.358896	9.395008
7.347115	666.334243	9.400026
6.855509	666.073750	9.405043
7.308554	663.086082	9.410061
7.305804	663.981377	9.415079
7.125446	652.280878	9.420096
7.242697	664.144821	9.425114
7.298828	664.413622	9.430131
7.466614	651.653496	9.435149
6.952968	640.172904	9.440167
7.274872	642.456380	9.445184
7.292577	639.126206	9.450202
6.779940	655.434403	9.455219
7.273509	659.559875	9.460237
7.385593	671.286919	9.465255
7.356893	679.951646	9.470272
7.233459	655.295308	9.475290
7.213015	665.790355	9.480307
7.391947	652.711542	9.485325
7.390523	652.233956	9.490343
7.299187	655.105173	9.495360
7.196680	635.385810	9.500378
6.656093	663.453037	9.505395
7.048584	656.614408	9.510413
7.283469	670.290804	9.515431
7.149522	664.748688	9.520448
7.431910	672.095314	9.525466
7.262888	683.051719	9.530483
7.093199	665.065106	9.535501
7.271771	666.553694	9.540519
7.303024	658.946146	9.545536
7.398873	664.362017	9.550554
6.884214	681.185201	9.555571
6.940025	660.269090	9.560589
6.822446	680.596755	9.565607
7.112468	691.352239	9.570624
7.364592	696.116379	9.575642
6.920205	706.525946	9.580659
7.403024	689.655850	9.585677
7.290322	691.757779	9.590695
7.542465	704.141934	9.595712
7.477569	693.081694	9.600730
7.057522	703.258459	9.605747
7.590511	694.820439	9.610765
7.379566	703.651089	9.615783
7.139065	704.047336	9.620800
7.357802	688.974058	9.625818
7.448963	689.065659	9.630835
7.429689	684.403558	9.635853
7.475080	689.473443	9.640871
7.767523	708.353437	9.645888
7.667379	682.824047	9.650906
7.273451	703.456299	9.655923
7.295224	690.775867	9.660941
7.665559	693.290358	9.665959
6.924284	706.127881	9.670976
7.137286	694.963167	9.675994
7.274857	716.829788	9.681011
7.431868	731.228565	9.686029
7.609196	722.173699	9.691047
7.577493	743.993156	9.696064
7.681489	718.582685	9.701082
7.725613	725.571967	9.706099
7.884483	738.429710	9.711117
7.655177	708.479685	9.716135
7.667656	713.704583	9.721152
7.561706	693.467152	9.726170
7.559941	706.570943	9.731187
7.375060	694.712343	9.736205
7.775531	715.618536	9.741223
7.521370	713.448923	9.746240
7.775057	725.087369	9.751258
7.643522	721.626960	9.756275
7.562102	710.747442	9.761293
7.956412	721.550066	9.766311
7.785866	697.849816	9.771328
7.631749	690.047160	9.776346
7.541270	703.726975	9.781363
7.527202	684.485618	9.786381
7.921940	696.552481	9.791399
7.613808	699.996595	9.796416
7.718945	706.955023	9.801434
7.592476	707.289523	9.806451
7.606238	689.539423	9.811469
7.890006	702.444194	9.816487
7.535960	709.491201	9.821504
7.543034	710.796774	9.826522
7.875125	732.061933	9.831539
7.790757	738.076950	9.836557
8.112002	728.613850	9.841575
7.566783	717.806744	9.846592
8.074074	705.287042	9.851610
7.613565	708.254997	9.856627
7.542801	697.482557	9.861645
7.948006	701.337188	9.866663
7.855808	724.633055	9.871680
7.552594	701.824474	9.876698
7.888488	724.658262	9.881715
7.832352	731.554400	9.886733
8.001318	736.762300	9.891751
7.469918	748.994460	9.896768
7.735714	733.044299	9.901786
7.869489	729.432394	9.906803
7.866184	739.452934	9.911821
7.710536	723.771492	9.916839
7.557163	740.334005	9.921856
7.698896	730.720499	9.926874
7.875528	737.060593	9.931891
7.556841	748.531511	9.936909
7.922539	743.413946	9.941927
7.875399	740.504102	9.946944
7.968414	744.478232	9.951962
7.661949	741.253367	9.956979
7.835455	732.254623	9.961997
8.004357	731.823866	9.967015
7.955364	727.260340	9.972032
8.223389	721.317414	9.977050
7.976901	739.707334	9.982067
7.870080	752.016929	9.987085
8.088648	730.827728	9.992103
7.768569	743.131329	9.997120
7.866538	730.996195	10.002138
7.788543	741.057122	10.007155
7.585924	734.085962	10.012173
7.818362	747.965043	10.017191
7.846117	764.141934	10.022208
7.979032	759.604030	10.027226
7.777635	765.440321	10.032243
7.787742	764.698296	10.037261
8.172734	763.808611	10.042279
7.881288	779.254027	10.047296
8.383956	773.102466	10.052314
7.892155	762.935937	10.057331
7.701870	782.527129	10.062349
8.032800	763.169324	10.067367
7.774155	767.156016	10.072384
8.161419	772.384236	10.077402
7.976407	748.933083	10.082419
7.763345	769.256473	10.087437
7.990354	755.352224	10.092455
8.049017	778.871798	10.097472
8.004123	778.294235	10.102490
8.082056	796.515482	10.107507
8.308078	806.414920	10.112525
8.481749	799.716399	10.117543
8.100149	792.744877	10.122560
7.644894	769.269769	10.127578
7.992034	791.633220	10.132595
7.911107	798.171080	10.137613
8.208997	792.546532	10.142631
8.403268	797.974426	10.147648
8.778063	797.559038	10.152666
8.624543	815.617527	10.157683
8.451088	805.246725	10.162701
8.527044	771.016914	10.167719
8.093231	782.290798	10.172736
8.462008	768.686153	10.177754
8.565701	769.865753	10.182771
8.438785	767.053417	10.187789
8.587310	764.676833	10.192807
8.291367	765.584671	10.197824
8.485854	756.343828	10.202842
8.196038	760.078355	10.207859
8.268090	768.090133	10.212877
8.397287	762.175546	10.217895
8.279556	771.896892	10.222912
8.652977	769.420657	10.227930
8.530832	766.708884	10.232947
8.041819	752.317614	10.237965
8.305689	770.834395	10.242983
8.147431	761.018150	10.248000
8.336609	777.029734	10.253018
8.577733	751.620754	10.258035
8.333770	765.546108	10.263053
8.577685	771.597217	10.268071
8.160995	762.981153	10.273088
8.354014	783.051871	10.278106
8.716466	765.328288	10.283123
8.556652	775.079025	10.288141
8.836268	765.914536	10.293159
8.602492	755.481905	10.298176
8.417643	770.660844	10.303194
8.418931	755.558198	10.308211
8.456949	766.380866	10.313229
8.302344	775.249576	10.318247
8.532098	768.023136	10.323264
8.395379	760.625533	10.328282
8.537349	768.816357	10.333299
8.353078	756.670183	10.338317
8.548111	763.810875	10.343335
8.475737	756.750973	10.348352
8.491675	759.603891	10.353370
8.465958	772.670468	10.358387
8.031140	779.094801	10.363405
8.549538	772.052684	10.368423
8.584884	770.992495	10.373440
8.350028	765.701997	10.378458
8.279947	769.189147	10.383475
8.308225	779.793906	10.388493
8.850633	779.714011	10.393511
8.787302	799.103485	10.398528
8.641358	783.377476	10.403546
8.760838	780.713640	10.408563
8.406537	783.046404	10.413581
8.522132	763.961917	10.418599
8.558187	794.011494	10.423616
8.725093	805.211310	10.428634
8.945367	783.350177	10.433651
8.426328	800.429758	10.438669
8.852561	799.832982	10.443687
8.708891	787.989836	10.448704
8.492613	801.712373	10.453722
8.965596	803.575143	10.458739
8.566377	798.122967	10.463757
8.839488	785.749943	10.468775
8.692615	791.506681	10.473792
8.513032	788.189595	10.478810
8.648779	786.052656	10.483827
8.658509	811.057541	10.488845
8.954101	790.116190	10.493863
8.779987	807.192404	10.498880
8.497749	823.025218	10.503898
8.827058	796.247019	10.508915
8.407053	812.092847	10.513933
8.821465	806.779956	10.518951
8.897020	803.749554	10.523968
8.922291	794.691533	10.528986
9.210104	804.338893	10.534003
8.674443	798.482998	10.539021
8.808114	800.130850	10.544039
8.615721	804.112113	10.549056
8.527150	808.528071	10.554074
8.803643	800.591909	10.559091
9.080324	804.479615	10.564109
8.991215	805.886993	10.569127
8.820953	813.301505	10.574144
8.676834	825.401434	10.579162
8.947932	795.685783	10.584179
8.506271	805.783728	10.589197
8.874573	806.283743	10.594215
8.997464	799.725961	10.599232
8.802110	809.470490	10.604250
8.765337	796.587102	10.609267
8.546412	798.068971	10.614285
8.537166	815.178267	10.619303
9.253999	834.751569	10.624320
9.286490	829.093624	10.629338
9.402863	833.369055	10.634355
8.743019	820.964700	10.639373
8.699280	825.009371	10.644391
9.270648	820.248045	10.649408
9.211157	837.963055	10.654426
9.265327	816.348659	10.659443
8.976620	825.091467	10.664461
8.953948	809.326758	10.669479
8.878812	809.638017	10.674496
8.563107	804.159639	10.679514
9.105629	828.763986	10.684531
8.788291	828.946222	10.689549
8.985082	821.632413	10.694567
8.938055	837.352079	10.699584
8.871402	856.039204	10.704602
9.418065	833.582468	10.709619
9.328680	836.044643	10.714637
8.936729	835.511837	10.719655
9.361598	823.279802	10.724672
9.219774	842.736717	10.729690
9.443635	817.673011	10.734707
8.809760	838.258603	10.739725
9.174413	852.573488	10.744743
9.245582	835.475963	10.749760
9.291273	867.495828	10.754778
9.107278	835.490952	10.759795
9.105634	828.336772	10.764813
9.103845	838.608241	10.769831
9.391168	826.054930	10.774848
9.056138	836.152591	10.779866
9.601501	824.269544	10.784883
9.284666	837.709104	10.789901
9.201714	832.972759	10.794919
9.467382	824.230708	10.799936
9.227356	850.354212	10.804954
9.309700	828.114043	10.809971
9.454742	838.663532	10.814989
9.146547	836.464061	10.820007
9.319017	830.629184	10.825024
9.303230	832.475709	10.830042
9.564455	825.365664	10.835059
9.506370	835.533473	10.840077
9.289005	821.584620	10.845095
9.704542	829.548226	10.850112
9.301631	836.379114	10.855130
9.438267	840.863250	10.860147
9.538570	844.631825	10.865165
9.681420	837.469111	10.870183
9.462092	846.253208	10.875200
9.436983	836.728905	10.880218
9.553674	834.785709	10.885235
9.329240	831.867658	10.890253
9.691383	843.932250	10.895271
9.540579	829.513453	10.900288
9.250269	833.674348	10.905306
9.247154	825.560718	10.910323
9.194622	832.731924	10.915341
8.932497	853.461069	10.920359
9.461027	848.918176	10.925376
9.456115	832.374133	10.930394
9.491777	816.495373	10.935411
9.357444	830.974470	10.940429
9.420816	837.163091	10.945447
9.528127	834.136489	10.950464
9.396874	828.015475	10.955482
9.278056	839.382681	10.960499
9.327845	826.636793	10.965517
9.290704	855.738304	10.970535
9.766780	858.016310	10.975552
9.690306	871.507591	10.980570
9.832185	845.741624	10.985587
9.541335	861.872675	10.990605
9.759932	871.870996	10.995623
9.706807	849.986168	11.000640
9.594104	863.241365	11.005658
9.513956	841.828710	11.010675
9.760706	864.936625	11.015693
9.976686	847.671884	11.020711
9.842274	839.964197	11.025728
9.297262	840.308336	11.030746
9.763460	859.146322	11.035763
10.058697	860.096294	11.040781
9.830376	860.197299	11.045799
9.774476	829.450565	11.050816
9.406631	843.378850	11.055834
9.276533	834.552629	11.060851
10.015123	855.899170	11.065869
9.567795	879.677573	11.070887
9.792167	860.212386	11.075904
9.589734	875.582770	11.080922
9.573925	871.725543	11.085939
9.529838	853.991307	11.090957
9.442892	875.383184	11.095975
9.699165	885.657007	11.100992
9.722274	882.424288	11.106010
9.955602	858.630279	11.111027
9.733868	883.485983	11.116045
9.583982	876.598835	11.121063
9.818314	869.449033	11.126080
9.637638	869.379509	11.131098
9.725053	865.268671	11.136115
9.884239	867.771445	11.141133
9.742892	886.504703	11.146151
9.960817	894.016773	11.151168
9.888172	899.794445	11.156186
9.711795	903.728414	11.161203
10.154570	903.564419	11.166221
10.003254	910.315778	11.171239
10.378193	889.611214	11.176256
10.024936	887.171018	11.181274
10.150572	877.730313	11.186291
10.027262	865.630066	11.191309
9.872903	870.617893	11.196327
10.318651	864.038020	11.201344
9.952490	884.017961	11.206362
9.954279	862.739336	11.211379
10.037216	868.282283	11.216397
9.779741	877.183500	11.221415
10.071961	873.462820	11.226432
9.887898	884.899193	11.231450
10.149805	893.010632	11.236467
10.124662	887.043570	11.241485
10.273634	899.924733	11.246503
10.160475	900.166805	11.251520
10.051358	875.802060	11.256538
10.040166	891.398960	11.261555
10.247912	890.433764	11.266573
10.043585	898.474360	11.271591
10.142091	879.472258	11.276608
10.143962	908.099529	11.281626
9.973756	895.352942	11.286643
10.343402	903.380555	11.291661
9.929261	901.732012	11.296679
10.280925	913.424765	11.301696
10.512905	900.597933	11.306714
10.280659	912.698816	11.311731
10.702872	894.617461	11.316749
10.176118	885.458635	11.321767
9.978837	875.494081	11.326784
10.419886	895.155842	11.331802
10.002943	881.817722	11.336819
10.177236	885.331819	11.341837
10.400123	908.270952	11.346855
10.380810	889.327767	11.351872
10.430290	904.455026	11.356890
10.210673	908.575722	11.361907
10.263244	904.998844	11.366925
9.868102	919.494656	11.371943
9.961686	901.257420	11.376960
9.873889	913.742302	11.381978
9.772494	900.940058	11.386995
10.201522	897.705788	11.392013
10.113267	927.453983	11.397031
10.343470	927.516606	11.402048
10.264421	943.635471	11.407066
10.636602	941.132059	11.412083
10.626393	936.755712	11.417101
10.277663	949.444531	11.422119
10.689472	938.841027	11.427136
10.531740	942.246367	11.432154
10.546559	919.070931	11.437171
10.699285	914.154310	11.442189
10.242813	909.722620	11.447207
10.264035	911.260458	11.452224
10.807856	933.267162	11.457242
10.598819	930.915794	11.462259
10.643844	927.937252	11.467277
10.590258	911.848913	11.472295
10.781742	895.372025	11.477312
10.603729	906.562201	11.482330
10.621918	903.453979	11.487347
10.451556	893.174020	11.492365
10.189663	907.494689	11.497383
10.694787	915.475812	11.502400
10.609537	901.793857	11.507418
10.493976	920.334655	11.512435
11.026542	922.110522	11.517453
10.545378	920.990934	11.522471
10.685904	914.483645	11.527488
10.565975	890.567795	11.532506
10.633940	908.917366	11.537523
10.730966	897.892801	11.542541
10.522781	906.998533	11.547559
10.518629	922.125595	11.552576
11.122429	921.770662	11.557594
10.870934	932.126462	11.562611
11.052998	909.208665	11.567629
10.426808	905.394540	11.572647
10.530761	909.368676	11.577664
10.502996	915.341346	11.582682
10.525581	931.385715	11.587699
10.808752	934.048673	11.592717
10.427834	923.168315	11.597735
10.661181	941.730003	11.602752
10.577392	933.163623	11.607770
10.854013	942.244755	11.612787
10.740955	929.905323	11.617805
10.810289	939.808110	11.622823
10.725204	933.840997	11.627840
10.724894	937.411906	11.632858
10.801706	949.049249	11.637875
11.169743	927.649786	11.642893
10.999085	942.674719	11.647911
11.052880	921.628105	11.652928
11.092259	929.115776	11.657946
11.085359	942.988830	11.662963
10.960149	931.535928	11.667981
10.647379	956.339489	11.672999
11.013303	950.251489	11.678016
11.262157	931.298179	11.683034
11.074848	935.541365	11.688051
10.897741	934.205133	11.693069
10.973734	932.105305	11.698087
10.865089	941.122480	11.703104
11.007346	934.223336	11.708122
10.770873	953.047967	11.713139
10.948163	944.373688	11.718157
10.664451	936.304305	11.723175
10.905000	948.416430	11.728192
10.942465	941.278169	11.733210
10.925856	940.543798	11.738227
11.107444	965.192465	11.743245
11.053317	978.603296	11.748263
10.883515	961.738024	11.753280
11.250516	961.666945	11.758298
11.373233	962.386936	11.763315
11.157478	967.664693	11.768333
10.992956	976.577371	11.773351
11.071754	954.932535	11.778368
11.179810	968.624156	11.783386
10.897496	960.666312	11.788403
11.005232	971.017383	11.793421
11.007675	969.779790	11.798439
10.999946	962.920967	11.803456
11.467133	968.795232	11.808474
11.313960	960.195237	11.813491
11.374053	961.472487	11.818509
11.328250	964.183617	11.823527
11.098144	948.185199	11.828544
11.278402	952.860731	11.833562
11.025811	978.578266	11.838579
11.156324	960.156751	11.843597
11.098938	971.813336	11.848615
11.120564	971.145363	11.853632
11.230062	964.169553	11.858650
11.144028	967.289496	11.863667
11.366692	990.247878	11.868685
11.501115	992.670730	11.873703
11.250325	1000.044618	11.878720
11.633515	987.236316	11.883738
11.426387	989.003977	11.888755
11.566111	963.317579	11.893773
11.212116	969.958892	11.898791
11.208714	995.421744	11.903808
11.418966	996.398168	11.908826
11.443501	1003.751256	11.913843
11.446035	1011.616520	11.918861
11.416982	995.003769	11.923879
11.240071	986.677004	11.928896
11.790843	996.244915	11.933914
11.492753	1001.671789	11.938931
11.492721	989.525783	11.943949
11.745024	1011.554233	11.948967
11.832243	1002.962407	11.953984
11.838622	990.343902	11.959002
11.454345	994.427675	11.964019
11.688359	1004.652711	11.969037
11.757043	994.506463	11.974055
11.404718	998.617429	11.979072
11.508470	998.435267	11.984090
11.516561	990.870645	11.989107
11.427968	1005.514647	11.994125
11.659811	986.206098	11.999143
11.350788	984.616631	12.004160
11.608338	1002.519436	12.009178
11.625109	996.780288	12.014195
11.497383	1004.434947	12.019213
11.721985	1006.931066	12.024231
11.419514	1001.469323	12.029248
11.739682	1010.219264	12.034266
11.589665	1005.120419	12.039283
11.454693	986.787617	12.044301
11.787704	995.835255	12.049319
11.442307	991.361470	12.054336
11.497276	1013.468979	12.059354
11.833657	1028.881740	12.064371
12.017704	1021.444580	12.069389
12.018315	1037.003564	12.074407
11.874454	1016.204197	12.079424
11.743415	1010.713825	12.084442
11.910510	1005.059548	12.089459
11.381156	999.197121	12.094477
11.968169	1026.830300	12.099495
11.821200	1028.586351	12.104512
12.142058	1028.323537	12.109530
11.991788	1043.046944	12.114547
12.039443	1028.435654	12.119565
11.933893	1038.181034	12.124583
11.912169	1033.725087	12.129600
12.231746	1018.196936	12.134618
11.875968	1012.240579	12.139635
11.592527	997.703322	12.144653
11.928483	1022.366128	12.149671
11.639304	1044.884308	12.154688
12.136905	1035.271432	12.159706
12.092633	1021.639770	12.164723
11.884625	1037.804547	12.169741
12.015341	1030.547513	12.174759
11.803934	1023.819444	12.179776
12.034557	1030.897602	12.184794
11.845554	1035.156151	12.189811
11.870521	1027.195314	12.194829
12.149064	1028.588302	12.199847
11.885799	1038.291652	12.204864
12.143046	1041.995963	12.209882
12.222152	1036.455798	12.214899
12.369698	1018.675630	12.219917
12.174792	1029.009548	12.224935
11.944284	1032.420342	12.229952
12.493172	1032.098786	12.234970
12.289504	1045.193232	12.239987
12.083844	1020.833289	12.245005
12.178224	1033.577067	12.250023
12.200206	1024.723636	12.255040
12.016041	1021.651882	12.260058
11.801207	1031.906635	12.265075
12.265695	1010.643738	12.270093
12.147225	1046.018042	12.275111
12.398881	1045.765188	12.280128
12.454783	1052.437986	12.285146
12.207620	1047.622045	12.290163
12.322102	1049.030142	12.295181
12.597448	1055.267068	12.300199
12.067875	1047.502071	12.305216
12.548331	1066.736776	12.310234
12.511380	1059.220696	12.315251
12.731395	1054.011679	12.320269
12.465249	1018.046457	12.325287
12.103861	1018.041336	12.330304
12.036440	1046.813453	12.335322
12.465027	1053.815806	12.340339
12.406245	1057.390502	12.345357
12.644223	1066.709042	12.350375
12.352493	1074.607617	12.355392
12.539906	1049.323626	12.360410
12.505431	1057.814662	12.365427
12.821926	1053.330467	12.370445
12.960617	1047.375234	12.375463
12.278411	1043.338399	12.380480
12.545020	1033.496834	12.385498
12.366382	1040.213896	12.390515
12.464575	1047.499236	12.395533
12.610803	1054.025742	12.400551
12.535448	1057.852919	12.405568
12.696335	1059.057924	12.410586
12.449033	1076.122325	12.415603
12.505861	1064.183346	12.420621
12.426218	1070.364404	12.425639
12.637715	1077.104291	12.430656
12.430933	1083.444718	12.435674
13.010216	1056.829626	12.440691
12.751394	1063.304107	12.445709
12.742464	1055.716582	12.450727
12.458178	1056.159631	12.455744
12.509009	1068.284507	12.460762
12.699457	1062.303495	12.465779
12.662684	1067.265262	12.470797
12.836518	1076.259155	12.475815
12.698444	1060.394193	12.480832
12.995829	1067.655874	12.485850
12.941949	1061.890099	12.490867
12.784820	1062.466820	12.495885
13.006286	1056.333378	12.500903
12.852221	1048.763249	12.505920
13.060364	1060.904533	12.510938
12.788237	1051.210045	12.515955
12.609394	1052.183271	12.520973
13.267472	1055.321761	12.525991
12.945947	1049.089224	12.531008
13.243934	1054.484620	12.536026
12.857719	1066.598867	12.541043
12.639092	1059.337264	12.546061
12.940596	1068.005697	12.551079
12.705968	1074.471559	12.556096
12.997551	1057.383610	12.561114
13.214568	1061.495855	12.566131
12.644020	1056.539306	12.571149
12.926773	1049.322869	12.576167
12.746312	1070.274088	12.581184
12.788903	1066.841603	12.586202
12.890580	1062.476448	12.591219
12.702926	1077.755539	12.596237
12.919450	1055.208682	12.601255
13.353944	1089.592908	12.606272
12.909984	1061.731501	12.611290
13.150484	1064.361386	12.616307
13.153502	1087.745883	12.621325
13.170568	1082.197060	12.626343
12.887441	1095.543107	12.631360
13.196139	1091.081640	12.636378
13.335561	1082.108792	12.641395
13.050932	1090.080298	12.646413
13.174716	1086.636162	12.651431
13.086873	1087.395482	12.656448
13.252109	1106.868014	12.661466
13.417388	1073.375244	12.666483
13.233860	1089.095192	12.671501
13.538869	1088.312976	12.676519
13.273625	1098.780386	12.681536
13.024265	1086.776270	12.686554
13.188566	1093.324504	12.691571
12.819465	1096.398951	12.696589
13.061029	1082.121422	12.701607
13.077479	1082.922744	12.706624
13.137841	1093.355627	12.711642
12.989196	1082.671556	12.716659
13.313762	1095.596190	12.721677
13.405704	1090.364832	12.726695
13.414068	1081.111649	12.731712
13.014409	1102.761477	12.736730
13.584517	1094.511547	12.741747
13.543441	1122.246236	12.746765
13.461716	1131.899669	12.751783
13.549212	1113.966755	12.756800
13.614143	1122.256798	12.761818
13.761204	1102.027396	12.766835
13.473475	1082.190662	12.771853
13.543689	1087.892643	12.776871
13.327113	1087.400316	12.781888
13.307428	1095.788461	12.786906
13.559223	1102.338378	12.791923
13.677763	1117.356524	12.796941
13.682374	1130.360533	12.801959
13.619897	1120.730740	12.806976
13.415026	1132.138854	12.811994
13.886029	1114.714767	12.817011
13.709192	1138.140675	12.822029
13.523588	1132.146701	12.827047
13.725789	1113.777608	12.832064
13.498631	1136.327493	12.837082
13.914070	1108.764030	12.842099
13.869328	1113.371013	12.847117
13.832394	1122.399961	12.852135
13.626571	1098.603862	12.857152
13.240266	1113.085801	12.862170
13.736807	1123.248834	12.867187
13.638729	1124.220230	12.872205
13.893569	1120.422519	12.877223
13.910566	1107.329441	12.882240
13.685070	1128.318095	12.887258
13.727701	1118.451694	12.892275
13.674634	1115.595699	12.897293
13.976678	1131.098568	12.902311
13.942367	1115.758200	12.907328
13.695385	1132.972379	12.912346
13.739154	1121.700808	12.917363
13.484951	1126.275301	12.922381
13.869198	1120.157638	12.927399
13.803236	1104.336310	12.932416
13.595653	1118.897747	12.937434
13.842295	1133.894051	12.942451
13.622212	1134.571217	12.947469
13.911046	1152.561525	12.952487
14.404937	1150.172580	12.957504
13.858769	1158.939921	12.962522
14.265616	1142.482971	12.967539
13.999543	1139.864880	12.972557
13.987937	1131.550866	12.977575
14.101529	1118.693232	12.982592
14.165904	1145.352128	12.987610
14.336442	1138.946427	12.992627
14.230937	1128.862235	12.997645
14.031496	1132.999337	13.002663
14.291442	1131.662988	13.007680
13.878771	1123.948300	13.012698
14.021815	1120.003750	13.017715
14.146882	1150.945202	13.022733
14.005331	1154.367300	13.027751
14.370563	1147.426291	13.032768
14.361126	1157.496629	13.037786
14.540600	1137.870341	13.042803
14.605417	1128.169125	13.047821
14.445736	1110.621568	13.052839
14.297922	1110.468186	13.057856
13.892684	1114.435798	13.062874
14.205615	1110.575254	13.067891
14.314987	1126.099725	13.072909
13.914323	1114.215648	13.077927
14.403150	1142.124451	13.082944
14.410280	1149.081958	13.087962
14.651710	1141.064822	13.092979
14.712491	1141.301473	13.097997
14.582645	1138.143178	13.103015
14.097251	1127.802945	13.108032
14.157378	1129.986582	13.113050
14.620486	1121.658969	13.118067
14.396676	1151.882870	13.123085
14.222909	1148.349737	13.128103
14.536477	1151.490764	13.133120
14.496643	1167.463161	13.138138
14.604151	1145.978134	13.143155
14.569060	1157.951769	13.148173
14.636964	1155.681832	13.153191
14.865082	1142.978635	13.158208
14.691517	1145.511352	13.163226
14.500624	1112.158441	13.168243
14.304919	1136.446116	13.173261
14.646004	1139.005763	13.178279
14.780066	1146.439123	13.183296
14.627829	1155.217524	13.188314
14.682233	1137.711802	13.193331
14.294925	1148.609359	13.198349
14.467811	1154.261728	13.203367
14.504487	1145.450670	13.208384
14.565005	1151.823606	13.213402
14.666433	1134.450733	13.218419
14.603988	1149.310381	13.223437
14.440218	1148.475841	13.228455
14.873090	1142.301721	13.233472
14.620814	1163.073837	13.238490
14.687914	1164.572631	13.243507
14.945454	1152.859801	13.248525
14.665703	1134.636062	13.253543
14.932604	1148.257016	13.258560
14.643697	1157.290725	13.263578
14.800573	1142.585901	13.268595
14.737466	1146.338849	13.273613
14.667630	1151.999840	13.278631
15.021160	1150.362560	13.283648
14.744512	1150.382894	13.288666
14.965109	1162.777258	13.293683
15.000709	1177.266976	13.298701
14.865885	1161.892988	13.303719
14.967176	1157.793948	13.308736
15.207740	1179.771247	13.313754
15.221872	1165.603353	13.318771
15.230514	1155.609998	13.323789
14.841395	1170.524144	13.328807
15.289023	1150.917486	13.333824
14.760188	1157.637565	13.338842
14.617212	1149.834899	13.343859
15.068321	1174.665982	13.348877
15.008114	1176.254402	13.353895
15.011808	1180.132015	13.358912
15.279829	1184.090130	13.363930
14.731459	1168.782608	13.368947
14.999911	1180.691042	13.373965
14.771702	1181.887049	13.378983
15.129626	1185.702680	13.384000
15.024540	1180.720338	13.389018
15.166333	1180.901879	13.394035
15.348743	1196.982229	13.399053
15.452837	1190.230780	13.404071
15.399287	1185.239230	13.409088
15.348756	1191.923773	13.414106
15.320363	1178.133380	13.419123
15.285625	1188.615501	13.424141
15.120136	1186.241053	13.429159
15.448316	1165.972287	13.434176
15.060508	1180.173993	13.439194
15.268702	1174.714389	13.444211
15.276010	1178.852859	13.449229
15.207024	1175.577929	13.454247
15.679327	1201.123199	13.459264
15.452107	1205.920172	13.464282
15.441539	1204.637280	13.469299
15.415287	1204.492738	13.474317
15.344009	1193.536907	13.479335
15.509240	1204.096498	13.484352
15.378968	1207.955420	13.489370
15.361402	1214.408200	13.494387
15.517936	1196.399524	13.499405
15.438014	1210.969472	13.504423
15.658063	1220.371070	13.509440
15.633890	1218.032108	13.514458
15.712250	1226.370862	13.519475
15.698081	1221.303123	13.524493
15.820914	1208.147991	13.529511
15.834044	1200.915819	13.534528
15.776424	1200.814740	13.539546
15.736040	1186.709268	13.544563
16.001896	1185.025169	13.549581
15.642382	1180.257864	13.554599
15.919305	1165.312070	13.559616
15.927907	1166.533590	13.564634
15.621342	1187.658627	13.569651
15.903682	1175.659267	13.574669
15.752458	1166.966237	13.579687
15.850303	1180.518724	13.584704
15.926263	1176.879369	13.589722
15.592788	1176.635634	13.594739
15.890265	1171.019184	13.599757
15.645836	1176.394348	13.604775
15.694314	1162.769077	13.609792
15.493591	1184.141122	13.614810
15.786805	1213.982823	13.619827
15.988378	1202.305183	13.624845
15.881295	1214.048788	13.629863
16.031932	1210.393739	13.634880
16.084833	1204.405783	13.639898
16.138021	1208.182235	13.644915
16.195414	1190.608946	13.649933
15.986018	1211.100779	13.654951
16.268699	1189.980055	13.659968
16.173590	1205.252639	13.664986
16.216577	1208.869003	13.670003
16.249456	1178.405745	13.675021
15.899627	1193.060920	13.680039
15.992991	1174.524548	13.685056
15.873651	1180.621189	13.690074
16.259050	1201.129451	13.695091
16.088636	1198.885607	13.700109
16.111473	1200.527612	13.705127
16.107116	1199.075918	13.710144
16.408397	1215.422600	13.715162
16.264912	1198.190204	13.720179
16.297092	1197.785277	13.725197
16.245186	1204.641863	13.730215
16.179930	1190.617745	13.735232
16.334789	1211.157033	13.740250
15.889561	1210.700028	13.745267
16.433225	1193.773273	13.750285
16.013103	1215.824087	13.755303
15.984407	1201.855123	13.760320
16.129074	1201.507966	13.765338
15.683533	1218.413993	13.770355
15.997003	1204.499477	13.775373
16.164274	1232.684467	13.780391
16.264916	1242.317180	13.785408
16.263938	1242.757498	13.790426
16.237506	1259.456938	13.795443
16.833871	1238.846187	13.800461
16.305374	1249.826583	13.805479
16.565990	1250.029818	13.810496
16.432534	1238.316101	13.815514
16.154120	1248.017462	13.820531
16.633466	1220.512316	13.825549
16.441999	1246.023393	13.830567
16.644984	1229.019760	13.835584
16.935512	1247.000060	13.840602
16.692939	1250.517301	13.845619
16.906940	1228.933377	13.850637
16.780345	1250.164848	13.855655
16.726102	1229.649623	13.860672
16.557131	1240.834218	13.865690
16.340518	1241.667176	13.870707
16.668058	1218.546941	13.875725
16.599380	1237.749609	13.880743
16.641450	1234.788618	13.885760
16.404921	1235.203606	13.890778
16.580844	1232.114614	13.895795
16.971959	1232.810632	13.900813
16.834143	1233.757113	13.905831
16.811384	1241.704314	13.910848
16.769048	1239.797976	13.915866
16.565282	1242.197051	13.920883
16.642118	1247.428125	13.925901
16.657811	1260.531964	13.930919
16.713326	1257.275803	13.935936
16.569337	1267.576176	13.940954
16.535065	1264.924382	13.945971
17.074555	1261.016716	13.950989
16.864475	1278.081488	13.956007
17.230923	1274.405912	13.961024
17.398357	1268.883834	13.966042
17.337092	1264.107560	13.971059
17.334114	1277.775099	13.976077
17.278033	1266.738081	13.981095
16.956175	1268.328617	13.986112
17.250331	1261.372932	13.991130
17.375496	1277.511045	13.996147
17.453070	1257.086474	14.001165
17.323846	1257.761716	14.006183
17.177422	1231.596491	14.011200
17.347583	1234.689599	14.016218
16.810269	1241.181738	14.021235
17.141958	1222.291232	14.026253
17.154827	1254.332975	14.031271
17.249077	1269.509679	14.036288
17.427702	1254.042174	14.041306
17.250144	1287.798140	14.046323
17.357375	1269.283765	14.051341
17.376359	1278.994646	14.056359
17.333486	1254.955184	14.061376
17.299377	1266.395597	14.066394
17.305527	1266.233891	14.071411
17.422092	1265.126101	14.076429
17.190375	1270.677108	14.081447
16.793540	1256.805242	14.086464
17.254247	1267.421534	14.091482
17.121509	1284.256061	14.096499
17.348284	1260.846186	14.101517
17.166308	1251.580664	14.106535
17.342787	1247.969355	14.111552
17.324439	1264.529012	14.116570
17.414987	1268.424079	14.121587
17.678851	1281.872761	14.126605
17.738971	1282.794800	14.131623
17.386463	1272.187387	14.136640
17.684912	1285.497119	14.141658
17.653654	1281.464824	14.146675
17.472634	1259.277590	14.151693
17.466415	1271.164769	14.156711
17.512388	1284.597702	14.161728
17.745115	1292.642145	14.166746
17.452554	1298.918803	14.171763
17.505140	1308.706414	14.176781
17.574311	1292.089508	14.181799
17.586291	1306.994279	14.186816
17.822474	1286.857067	14.191834
17.485894	1311.390296	14.196851
17.619219	1292.219663	14.201869
17.842244	1277.677950	14.206887
17.875951	1287.388470	14.211904
17.919219	1288.668331	14.216922
17.877994	1299.099446	14.221939
17.940922	1305.644647	14.226957
18.103851	1292.289947	14.231975
18.235650	1303.475658	14.236992
17.816850	1288.144537	14.242010
17.701797	1295.710062	14.247027
18.110323	1278.953150	14.252045
18.083451	1290.582794	14.257063
17.723489	1286.806052	14.262080
18.270217	1287.552618	14.267098
17.781101	1301.320985	14.272115
18.166675	1300.855784	14.277133
18.058978	1297.594704	14.282151
18.131833	1296.430172	14.287168
18.254217	1299.572911	14.292186
18.242632	1285.172400	14.297203
18.110678	1287.114244	14.302221
18.046509	1281.320467	14.307239
18.090965	1283.030348	14.312256
18.254652	1294.978227	14.317274
17.791161	1296.052040	14.322291
18.173429	1294.222735	14.327309
18.451585	1292.710568	14.332327
18.324852	1295.029417	14.337344
18.691335	1306.283212	14.342362
18.407345	1295.745937	14.347379
18.442789	1295.496634	14.352397
18.377032	1294.656220	14.357415
18.269579	1280.510380	14.362432
18.344630	1290.358820	14.367450
18.029519	1279.811741	14.372467
18.392533	1287.715780	14.377485
18.825183	1312.487653	14.382503
18.509398	1300.092370	14.387520
18.424320	1298.571152	14.392538
18.703106	1289.093568	14.397555
18.538024	1271.438968	14.402573
18.584442	1276.550108	14.407591
18.433348	1282.634816	14.412608
18.319190	1270.681030	14.417626
18.423791	1297.262102	14.422643
18.695947	1299.424500	14.427661
18.902725	1313.006336	14.432679
18.706301	1321.805419	14.437696
18.553067	1292.891442	14.442714
18.636894	1275.741150	14.447731
18.936919	1312.480635	14.452749
18.925186	1288.104849	14.457767
18.420810	1289.936526	14.462784
18.651917	1300.117171	14.467802
18.885809	1304.804908	14.472819
18.804152	1306.385569	14.477837
19.275113	1318.046716	14.482855
18.490387	1279.372232	14.487872
18.651361	1290.969357	14.492890
18.997166	1312.202552	14.497907
18.642983	1305.084662	14.502925
18.947985	1309.744117	14.507943
19.021968	1319.936867	14.512960
19.189399	1319.839334	14.517978
18.803038	1305.386887	14.522995
19.158662	1316.204887	14.528013
19.071801	1300.495545	14.533031
18.695598	1292.322289	14.538048
18.807301	1294.122807	14.543066
19.042061	1307.692634	14.548083
19.096964	1305.684410	14.553101
18.992506	1304.527040	14.558119
18.920807	1309.183802	14.563136
19.349028	1304.657158	14.568154
18.764813	1318.783600	14.573171
18.706304	1329.588276	14.578189
19.032441	1307.325229	14.583207
18.707631	1315.614150	14.588224
19.196406	1307.293414	14.593242
19.205776	1307.670227	14.598259
19.227956	1317.319201	14.603277
19.219342	1300.964885	14.608295
19.254648	1323.870301	14.613312
19.250971	1314.057480	14.618330
19.444910	1324.785894	14.623347
18.838803	1316.312899	14.628365
18.944079	1339.004753	14.633383
19.331986	1337.239951	14.638400
19.505428	1354.166148	14.643418
19.516012	1339.955973	14.648435
19.257069	1355.205595	14.653453
19.723566	1344.948699	14.658471
19.448121	1331.342073	14.663488
19.845814	1348.851243	14.668506
19.494063	1337.726846	14.673523
19.590219	1352.885310	14.678541
19.837859	1337.063086	14.683559
19.364333	1344.093029	14.688576
19.666562	1335.428584	14.693594
19.838946	1329.102402	14.698611
20.108509	1324.999028	14.703629
19.882575	1309.034869	14.708647
19.949686	1306.058607	14.713664
19.810856	1293.878124	14.718682
19.891783	1299.924005	14.723699
19.680939	1292.965560	14.728717
19.907226	1300.254354	14.733735
19.712400	1299.301442	14.738752
19.789875	1301.017481	14.743770
19.694434	1280.778619	14.748787
19.894852	1284.559983	14.753805
20.078082	1283.789914	14.758823
19.652697	1291.813420	14.763840
19.855010	1300.051827	14.768858
19.897033	1286.966170	14.773875
20.041954	1293.249939	14.778893
20.153444	1287.405974	14.783911
19.927073	1293.456779	14.788928
20.017173	1279.549294	14.793946
20.069045	1288.188257	14.798963
19.888727	1293.616337	14.803981
20.124766	1270.833314	14.808999
20.294494	1287.971914	14.814016
20.151835	1278.724381	14.819034
20.032614	1289.417338	14.824051
20.128861	1295.515790	14.829069
20.241661	1295.016945	14.834087
20.284517	1285.448757	14.839104
19.850861	1301.859323	14.844122
19.800128	1287.498932	14.849139
19.792332	1299.861779	14.854157
20.176116	1297.334351	14.859175
20.106671	1306.544823	14.864192
20.431206	1309.019950	14.869210
20.485185	1315.423458	14.874227
20.104587	1310.399812	14.879245
20.318208	1301.505990	14.884263
20.438622	1328.032152	14.889280
20.561621	1316.861492	14.894298
20.381319	1313.022186	14.899315
20.284829	1335.482674	14.904333
20.448406	1319.556080	14.909351
20.344166	1319.979024	14.914368
20.532779	1333.043230	14.919386
20.258985	1313.427268	14.924403
20.065093	1330.179650	14.929421
20.466816	1305.572160	14.934439
20.190525	1319.697409	14.939456
20.420253	1324.322862	14.944474
20.599768	1311.336581	14.949491
20.327299	1333.691731	14.954509
20.256406	1315.138642	14.959527
20.619904	1306.701534	14.964544
20.330378	1320.801222	14.969562
20.181824	1321.123837	14.974579
20.703885	1350.970497	14.979597
20.977220	1354.220359	14.984615
20.944105	1354.592680	14.989632
20.635045	1366.102419	14.994650
20.711615	1342.100351	14.999667
20.841456	1356.892999	15.004685
20.878378	1355.679886	15.009703
20.851030	1355.599781	15.014720
20.932131	1353.097174	15.019738
20.906115	1357.693165	15.024755
20.653934	1347.714644	15.029773
20.910621	1345.275914	15.034791
20.788163	1353.541845	15.039808
20.929026	1341.436927	15.044826
21.039592	1351.653370	15.049843
20.566312	1363.723591	15.054861
20.821570	1350.702028	15.059879
20.992637	1352.746524	15.064896
21.051024	1342.592400	15.069914
21.164459	1344.000402	15.074931
20.746489	1351.939367	15.079949
21.135581	1347.110389	15.084967
21.110580	1381.398508	15.089984
21.376002	1377.516228	15.095002
21.584365	1367.032745	15.100019
21.093899	1372.633634	15.105037
21.278515	1341.083304	15.110055
21.266640	1356.121466	15.115072
21.416359	1351.313446	15.120090
21.220720	1344.259572	15.125107
21.228004	1354.170717	15.130125
21.708988	1349.698318	15.135143
21.299293	1367.085876	15.140160
21.349596	1366.631012	15.145178
21.604991	1340.654946	15.150195
21.350764	1352.578648	15.155213
21.446621	1342.377493	15.160231
21.755604	1344.200620	15.165248
21.280810	1340.396591	15.170266
21.576354	1343.460341	15.175283
21.596183	1358.901344	15.180301
21.479260	1355.594936	15.185319
21.380706	1339.114628	15.190336
21.552566	1355.256325	15.195354
21.829923	1365.797792	15.200371
21.647125	1365.738752	15.205389
21.636204	1364.671900	15.210407
21.987104	1366.084845	15.215424
21.790741	1357.576389	15.220442
21.550971	1359.385994	15.225459
21.700070	1348.506797	15.230477
21.726458	1349.868078	15.235495
21.810850	1377.436267	15.240512
21.826483	1367.366241	15.245530
21.814510	1363.750230	15.250547
21.882690	1365.848238	15.255565
21.999817	1379.828230	15.260583
21.810851	1360.431307	15.265600
22.019944	1378.798267	15.270618
22.117145	1363.693439	15.275635
21.931428	1370.605866	15.280653
22.125732	1356.565762	15.285671
21.912522	1357.968114	15.290688
21.687025	1363.009678	15.295706
22.091816	1350.331628	15.300723
22.127358	1369.054054	15.305741
22.203856	1370.977204	15.310759
22.285106	1361.876041	15.315776
22.013909	1377.202005	15.320794
22.315239	1381.379224	15.325811
21.967281	1375.972785	15.330829
22.291961	1380.145653	15.335847
22.488976	1365.185809	15.340864
22.237930	1379.298478	15.345882
22.287124	1365.864401	15.350899
22.248878	1367.956086	15.355917
21.997206	1383.973950	15.360935
22.319607	1363.555518	15.365952
22.050766	1377.860849	15.370970
21.871574	1386.677687	15.375987
21.809587	1375.025759	15.381005
22.198233	1381.710428	15.386023
22.260485	1376.217503	15.391040
22.271133	1390.911009	15.396058
22.591835	1405.892488	15.401075
22.413064	1406.421923	15.406093
22.318627	1387.529112	15.411111
22.326171	1387.803987	15.416128
22.255866	1399.907619	15.421146
22.383003	1395.854332	15.426163
22.451145	1402.152310	15.431181
22.484087	1405.055676	15.436199
22.614943	1402.060595	15.441216
22.658955	1399.664973	15.446234
22.945667	1413.881184	15.451251
22.977656	1400.701439	15.456269
22.638333	1404.837523	15.461287
22.660005	1391.993079	15.466304
22.697313	1392.105984	15.471322
22.806937	1404.070362	15.476339
22.838250	1395.419755	15.481357
22.386463	1403.599913	15.486375
22.770186	1427.307656	15.491392
23.042840	1424.264340	15.496410
23.304540	1427.937308	15.501427
23.163229	1406.128450	15.506445
22.916477	1387.600498	15.511463
23.080321	1387.206872	15.516480
22.750188	1380.605624	15.521498
23.077412	1395.904448	15.526515
22.864511	1396.836680	15.531533
23.039581	1410.027867	15.536551
23.235090	1422.846280	15.541568
23.235711	1425.642811	15.546586
23.446300	1419.119474	15.551603
23.082998	1399.990530	15.556621
22.742884	1412.335468	15.561639
23.343943	1405.359997	15.566656
23.185737	1404.367078	15.571674
23.140595	1416.270840	15.576691
23.724945	1431.108500	15.581709
23.420670	1411.776128	15.586727
23.439072	1390.182185	15.591744
23.265294	1403.861728	15.596762
23.152056	1419.508305	15.601779
23.153409	1425.020950	15.606797
23.275306	1428.588408	15.611815
23.715604	1431.272820	15.616832
23.377090	1429.399659	15.621850
23.485121	1410.635036	15.626867
23.572426	1424.866400	15.631885
23.139189	1421.190296	15.636903
23.678825	1421.236227	15.641920
23.366649	1421.206439	15.646938
23.663828	1419.884185	15.651955
23.689672	1424.301191	15.656973
23.588414	1428.808282	15.661991
23.868418	1413.991432	15.667008
23.544977	1434.853318	15.672026
23.597504	1421.468827	15.677043
23.538048	1415.540982	15.682061
23.600051	1427.954293	15.687079
23.720966	1408.471559	15.692096
23.917400	1431.999776	15.697114
23.740908	1412.821444	15.702131
23.696466	1425.893935	15.707149
23.752505	1438.738657	15.712167
23.966786	1431.719538	15.717184
23.769007	1447.344000	15.722202
23.851686	1445.957508	15.727219
23.807862	1454.588172	15.732237
24.026333	1456.519262	15.737255
24.092950	1448.874382	15.742272
23.657545	1449.756596	15.747290
24.173818	1443.453638	15.752307
24.226390	1446.254675	15.757325
24.298695	1454.531280	15.762343
24.064896	1434.860433	15.767360
24.076168	1451.476014	15.772378
24.449793	1465.631267	15.777395
24.220931	1444.533818	15.782413
24.070936	1457.233903	15.787431
23.979125	1452.843047	15.792448
24.025041	1450.750383	15.797466
23.636049	1452.058985	15.802483
24.116714	1447.442647	15.807501
24.185150	1468.593087	15.812519
24.599024	1470.524556	15.817536
24.408774	1476.651828	15.822554
24.482106	1482.099263	15.827571
24.298281	1479.449021	15.832589
24.218509	1481.037851	15.837607
24.416627	1472.377447	15.842624
24.524039	1475.265075	15.847642
24.541069	1486.345111	15.852659
24.736105	1468.650353	15.857677
24.526680	1487.259207	15.862695
24.652447	1472.535000	15.867712
24.264688	1484.721272	15.872730
24.187575	1474.952662	15.877747
24.458268	1474.246360	15.882765
24.422298	1473.845111	15.887783
24.658803	1478.727999	15.892800
24.649331	1474.827751	15.897818
24.662671	1503.926577	15.902835
25.175767	1487.144483	15.907853
25.036065	1504.324620	15.912871
24.728812	1478.028696	15.917888
24.886589	1482.368415	15.922906
25.057130	1513.898726	15.927923
25.437929	1482.449612	15.932941
25.122567	1491.065932	15.937959
25.186318	1464.818734	15.942976
24.988112	1488.099527	15.947994
24.863901	1470.335012	15.953011
25.163995	1466.194968	15.958029
25.155156	1470.577078	15.963047
25.419926	1467.693487	15.968064
25.312309	1461.117819	15.973082
25.476482	1469.152725	15.978099
25.360047	1455.540375	15.983117
24.995862	1476.941809	15.988135
25.219620	1463.853029	15.993152
25.201614	1464.915030	15.998170
25.354336	1463.847992	16.003187
25.650861	1458.742607	16.008205
25.156607	1468.792405	16.013223
25.150229	1465.940634	16.018240
25.144005	1458.713014	16.023258
25.323935	1471.873635	16.028275
25.506505	1464.464452	16.033293
25.066323	1489.788444	16.038311
25.280165	1478.019708	16.043328
25.464331	1511.213938	16.048346
25.220021	1500.454753	16.053363
25.823547	1501.227765	16.058381
25.603908	1500.571791	16.063399
25.704607	1504.391044	16.068416
25.652676	1506.182416	16.073434
25.632823	1492.833639	16.078451
25.916357	1498.807344	16.083469
25.951603	1497.585247	16.088487
25.816575	1503.857997	16.093504
25.531025	1515.107224	16.098522
25.682291	1500.312846	16.103539
25.765326	1495.838370	16.108557
25.672252	1503.878019	16.113575
25.907929	1491.533542	16.118592
25.588071	1505.367800	16.123610
25.526906	1493.742313	16.128627
25.950730	1504.186853	16.133645
25.551312	1498.339955	16.138663
26.218558	1495.628968	16.143680
25.969959	1507.300043	16.148698
25.905022	1506.808817	16.153715
25.915019	1497.630786	16.158733
25.831539	1519.496312	16.163751
25.918598	1526.453870	16.168768
26.106528	1531.638243	16.173786
26.080209	1539.560012	16.178803
26.388785	1529.900820	16.183821
26.115311	1546.117493	16.188839
26.429606	1541.816651	16.193856
26.270881	1521.529575	16.198874
25.794979	1518.110347	16.203891
26.452898	1527.938978	16.208909
25.887041	1517.402273	16.213927
26.093544	1532.369980	16.218944
26.152536	1531.499983	16.223962
25.955667	1539.367670	16.228979
26.312372	1530.404312	16.233997
26.285410	1563.839604	16.239015
26.541815	1559.928854	16.244032
26.612337	1544.775512	16.249050
26.195359	1548.004189	16.254067
26.351517	1542.688952	16.259085
26.526519	1554.076226	16.264103
26.609548	1561.085439	16.269120
26.597535	1546.693707	16.274138
26.767907	1548.524611	16.279155
26.981513	1538.392432	16.284173
26.616202	1543.009813	16.289191
26.914931	1551.140512	16.294208
26.758607	1546.018124	16.299226
26.968492	1547.258861	16.304243
26.947216	1543.077338	16.309261
26.924449	1541.792497	16.314279
26.882029	1547.019666	16.319296
26.971147	1560.419044	16.324314
26.734221	1542.292739	16.329331
27.089923	1548.555458	16.334349
27.274940	1539.671835	16.339367
26.724140	1554.440471	16.344384
26.888108	1539.522918	16.349402
26.953574	1558.164366	16.354419
26.743459	1522.998468	16.359437
26.864926	1552.717769	16.364455
26.981702	1562.454688	16.369472
27.436988	1557.742532	16.374490
27.424135	1578.405679	16.379507
27.798731	1559.549391	16.384525
27.723077	1556.807849	16.389543
27.801382	1551.854023	16.394560
28.117910	1523.777533	16.399578
27.999867	1522.160481	16.404595
27.932120	1521.142567	16.409613
27.599209	1515.868406	16.414631
27.819572	1493.904693	16.419648
27.656268	1496.169490	16.424666
27.483230	1519.556089	16.429683
27.397200	1500.986088	16.434701
27.362375	1501.079917	16.439719
27.541783	1486.672746	16.444736
27.744963	1513.690366	16.449754
27.512474	1497.125745	16.454771
27.612665	1505.859088	16.459789
27.843446	1492.650841	16.464807
27.826268	1483.215356	16.469824
27.658315	1482.326186	16.474842
27.632234	1488.930555	16.479859
28.122637	1512.599645	16.484877
27.835091	1502.647630	16.489895
27.579826	1496.051967	16.494912
27.946682	1512.188666	16.499930
27.912983	1515.993919	16.504947
28.146413	1528.411357	16.509965
28.056089	1506.466890	16.514983
27.735665	1491.195963	16.520000
27.942253	1514.643906	16.525018
27.674988	1516.349533	16.530035
28.019198	1533.015966	16.535053
28.344743	1529.202239	16.540071
28.437544	1523.637298	16.545088
28.186661	1530.479678	16.550106
27.971166	1525.135136	16.555123
27.955123	1540.113255	16.560141
28.340330	1522.710955	16.565159
28.081587	1516.602368	16.570176
28.347941	1521.522946	16.575194
28.366626	1544.117923	16.580211
28.282872	1530.703409	16.585229
28.392972	1518.050600	16.590247
27.863781	1508.360121	16.595264
28.125370	1519.224902	16.600282
28.196576	1524.706456	16.605299
28.144935	1526.695182	16.610317
28.748911	1523.614511	16.615335
28.631519	1540.451507	16.620352
28.508286	1535.861729	16.625370
28.336521	1529.591157	16.630387
28.415927	1536.355045	16.635405
28.737544	1551.242834	16.640423
28.811845	1554.267811	16.645440
28.751701	1563.721140	16.650458
28.562059	1555.854636	16.655475
28.889156	1550.964791	16.660493
28.803705	1572.310454	16.665511
28.711184	1561.661744	16.670528
28.818392	1555.622757	16.675546
28.721364	1568.056066	16.680563
28.628149	1550.172383	16.685581
28.763220	1557.688437	16.690599
28.412462	1563.517140	16.695616
28.697158	1541.922372	16.700634
28.660558	1567.332422	16.705651
28.629360	1573.403730	16.710669
29.090983	1585.548021	16.715687
28.577598	1597.479708	16.720704
28.914637	1573.383851	16.725722
28.958138	1577.819337	16.730739
29.237508	1589.474174	16.735757
29.281513	1578.804070	16.740775
29.069936	1591.742447	16.745792
29.251307	1578.824910	16.750810
29.445116	1584.986177	16.755827
29.329158	1578.616224	16.760845
29.500275	1576.772875	16.765863
29.271720	1592.487297	16.770880
29.447384	1572.601393	16.775898
29.239273	1575.505855	16.780915
29.335376	1585.336344	16.785933
29.547293	1590.513920	16.790951
29.447451	1619.641216	16.795968
29.755706	1623.225354	16.800986
29.734662	1610.724330	16.806003
29.781449	1615.281798	16.811021
29.417430	1613.471478	16.816039
29.695821	1603.981958	16.821056
29.873207	1618.137309	16.826074
29.694132	1609.554512	16.831091
29.879551	1616.319711	16.836109
29.950766	1608.405150	16.841127
29.995511	1615.736594	16.846144
30.138772	1611.163272	16.851162
29.638730	1614.028897	16.856179
29.829130	1615.477345	16.861197
29.887111	1600.842547	16.866215
29.939029	1605.592333	16.871232
30.109666	1600.333922	16.876250
29.891457	1604.834020	16.881267
29.940165	1609.668473	16.886285
30.394565	1593.243135	16.891303
30.095674	1605.572658	16.896320
30.255237	1596.059481	16.901338
30.082873	1613.959459	16.906355
29.962520	1619.984212	16.911373
30.338497	1603.824035	16.916391
29.991537	1615.365021	16.921408
30.277003	1596.112872	16.926426
30.307387	1591.103383	16.931443
30.040475	1603.105540	16.936461
30.359812	1602.966961	16.941479
30.307502	1610.748603	16.946496
30.300945	1604.024803	16.951514
30.040303	1618.956727	16.956531
30.260067	1622.764697	16.961549
30.257102	1635.456180	16.966567
30.440926	1632.209241	16.971584
30.496476	1650.898297	16.976602
30.624865	1636.668969	16.981619
30.668275	1646.342687	16.986637
30.941146	1632.153548	16.991655
30.720518	1628.842865	16.996672
30.661682	1622.610668	17.001690
30.664156	1620.369089	17.006707
30.876173	1633.366410	17.011725
31.065745	1642.445518	17.016743
30.736352	1642.028004	17.021760
31.193223	1627.598859	17.026778
30.949874	1635.768311	17.031795
30.537096	1616.045427	17.036813
31.014221	1635.941994	17.041831
31.018078	1615.988580	17.046848
30.790994	1625.329504	17.051866
31.136900	1612.346469	17.056883
30.785029	1630.369713	17.061901
31.152769	1632.110837	17.066919
30.861323	1657.380217	17.071936
31.275540	1659.773273	17.076954
31.384804	1658.905588	17.081971
31.560817	1670.682369	17.086989
31.342511	1659.072589	17.092007
31.117440	1649.109170	17.097024
31.435190	1661.257716	17.102042
31.322605	1642.444443	17.107059
31.740452	1662.603544	17.112077
31.739378	1663.825031	17.117095
31.491046	1657.233368	17.122112
31.916376	1644.702931	17.127130
31.807752	1634.228647	17.132147
31.719240	1623.877496	17.137165
31.804587	1601.881818	17.142183
31.436280	1631.103000	17.147200
31.726680	1615.214872	17.152218
31.474427	1616.795219	17.157235
31.766790	1636.495399	17.162253
31.835953	1640.296182	17.167271
31.560113	1647.017763	17.172288
31.697284	1661.234611	17.177306
31.908604	1646.606509	17.182323
31.866501	1659.000802	17.187341
32.194952	1651.751537	17.192359
31.917116	1644.605125	17.197376
32.169304	1652.193880	17.202394
32.251866	1638.242836	17.207411
31.898908	1646.437491	17.212429
32.253942	1653.091525	17.217447
32.081121	1668.494022	17.222464
32.037188	1637.130920	17.227482
32.185584	1649.320432	17.232499
31.475700	1651.411852	17.237517
32.144557	1637.369135	17.242535
32.111815	1647.691528	17.247552
32.300184	1642.979175	17.252570
32.309496	1648.861375	17.257587
32.123443	1633.001385	17.262605
32.153989	1646.232110	17.267623
32.475143	1648.126672	17.272640
32.274095	1665.821848	17.277658
32.406326	1661.710082	17.282675
32.377942	1672.439268	17.287693
32.539790	1676.677998	17.292711
32.495137	1677.956185	17.297728
32.334730	1658.613797	17.302746
32.654484	1680.160900	17.307763
32.378386	1691.414698	17.312781
32.900707	1666.425356	17.317799
32.946215	1684.396181	17.322816
32.704498	1668.416147	17.327834
33.119444	1670.347171	17.332851
32.729375	1676.125928	17.337869
32.797529	1674.762579	17.342887
32.938380	1666.513810	17.347904
32.863308	1673.724166	17.352922
33.012637	1667.610472	17.357939
32.894668	1667.787319	17.362957
33.058956	1670.241951	17.367975
33.196486	1668.619058	17.372992
32.962708	1677.898437	17.378010
33.107403	1667.650618	17.383027
32.947533	1669.484547	17.388045
33.228335	1680.254160	17.393063
33.476262	1674.223952	17.398080
33.389412	1689.399019	17.403098
33.335263	1670.007272	17.408115
33.246630	1688.840453	17.413133
33.395533	1682.734105	17.418151
33.230224	1695.677519	17.423168
33.451403	1685.554915	17.428186
34.084329	1699.831281	17.433203
33.492427	1689.516334	17.438221
33.761639	1678.327644	17.443239
33.685493	1682.384392	17.448256
33.325218	1659.271964	17.453274
33.895393	1651.976160	17.458291
33.850740	1687.993452	17.463309
33.929412	1666.871148	17.468327
33.859008	1672.425163	17.473344
33.770083	1658.236450	17.478362
33.815683	1652.802170	17.483379
33.112716	1679.142438	17.488397
33.851700	1677.735933	17.493415
33.842921	1685.213334	17.498432
33.701840	1688.219611	17.503450
34.258553	1695.585952	17.508467
33.877979	1689.842438	17.513485
34.026510	1690.037733	17.518503
33.930470	1681.847095	17.523520
33.739636	1692.032390	17.528538
33.860828	1680.743677	17.533555
33.800860	1693.434295	17.538573
33.944081	1686.695548	17.543591
34.120349	1707.651270	17.548608
33.947330	1712.834048	17.553626
34.468171	1713.679386	17.558643
33.950655	1735.987741	17.563661
34.282370	1707.544993	17.568679
34.046113	1716.116777	17.573696
34.004843	1725.655652	17.578714
34.484304	1709.520282	17.583731
34.468221	1716.909454	17.588749
34.670477	1719.525404	17.593767
34.410567	1711.347268	17.598784
34.482253	1742.878248	17.603802
34.800473	1742.532512	17.608819
34.390555	1769.137829	17.613837
34.660403	1741.688415	17.618855
34.840208	1753.461681	17.623872
34.449497	1751.281911	17.628890
35.047123	1725.029195	17.633907
35.013559	1741.693929	17.638925
35.067625	1749.885044	17.643943
35.319142	1746.069525	17.648960
34.912770	1732.877701	17.653978
35.195179	1744.403145	17.658995
34.800718	1739.300364	17.664013
35.365087	1750.688584	17.669031
35.214761	1733.917155	17.674048
35.205234	1746.353271	17.679066
35.448087	1733.034773	17.684083
35.199370	1735.942630	17.689101
35.171707	1747.810598	17.694119
35.442553	1727.775915	17.699136
35.208545	1743.135657	17.704154
35.580344	1747.982595	17.709171
35.498355	1742.087278	17.714189
35.424691	1747.481359	17.719207
35.506672	1738.237263	17.724224
35.362021	1753.343220	17.729242
35.533894	1737.933321	17.734259
35.556595	1732.774002	17.739277
35.201062	1747.090754	17.744295
35.450675	1734.047363	17.749312
35.371351	1736.863460	17.754330
35.596636	1731.041459	17.759347
35.474947	1730.159979	17.764365
35.473583	1752.536868	17.769383
35.890195	1735.700973	17.774400
35.544838	1741.928377	17.779418
35.736968	1747.777255	17.784435
35.839362	1749.037740	17.789453
35.910578	1759.290776	17.794471
36.092062	1737.288071	17.799488
35.996892	1759.650557	17.804506
36.526263	1761.285081	17.809523
36.329594	1753.534278	17.814541
36.119368	1763.775570	17.819559
36.124480	1760.086478	17.824576
36.317700	1763.009479	17.829594
36.211143	1758.641538	17.834611
35.980145	1765.297406	17.839629
36.256841	1743.730542	17.844647
36.241284	1759.884153	17.849664
36.391284	1750.208025	17.854682
36.146533	1770.052049	17.859699
36.243971	1754.279507	17.864717
35.914389	1749.034826	17.869735
36.224752	1758.685264	17.874752
36.251875	1770.729789	17.879770
36.650646	1786.026726	17.884787
36.277229	1809.270832	17.889805
36.582842	1776.400060	17.894823
36.649198	1794.973454	17.899840
36.358161	1790.926190	17.904858
36.717362	1772.476339	17.909875
36.815505	1787.827092	17.914893
36.422784	1766.058579	17.919911
36.972930	1777.013725	17.924928
36.575111	1779.223439	17.929946
36.726823	1784.163834	17.934963
37.043791	1796.876385	17.939981
37.178421	1805.706747	17.944999
37.334628	1805.111951	17.950016
37.170432	1794.054139	17.955034
37.142110	1788.434526	17.960051
36.984187	1786.994870	17.965069
36.983659	1805.556499	17.970087
37.433724	1789.671820	17.975104
37.329152	1811.298481	17.980122
37.538198	1784.826074	17.985139
37.869035	1807.762396	17.990157
37.865888	1783.121560	17.995175
37.560509	1777.217486	18.000192
37.237613	1772.992948	18.005210
37.555772	1770.516932	18.010227
37.702203	1770.392657	18.015245
37.759207	1782.419657	18.020263
37.782295	1776.354926	18.025280
37.238424	1762.090443	18.030298
37.622323	1769.327339	18.035315
37.741443	1777.118327	18.040333
37.505885	1792.273591	18.045351
37.807772	1777.481214	18.050368
37.690130	1801.698589	18.055386
37.563518	1785.645780	18.060403
37.609361	1802.472522	18.065421
37.378881	1792.723149	18.070439
37.756260	1796.453453	18.075456
37.735291	1801.047660	18.080474
38.143398	1822.920948	18.085491
38.060534	1825.042505	18.090509
38.079440	1832.644708	18.095527
38.211137	1831.259626	18.100544
38.516522	1833.479198	18.105562
38.409455	1843.587671	18.110579
38.587698	1828.093082	18.115597
38.437760	1834.949913	18.120615
38.596137	1808.758620	18.125632
38.278249	1791.526330	18.130650
38.337566	1823.315967	18.135667
38.541147	1810.863371	18.140685
38.373360	1836.160533	18.145703
38.470161	1828.366115	18.150720
38.444644	1834.752274	18.155738
38.355046	1830.183615	18.160755
38.777020	1832.324088	18.165773
38.452221	1837.037007	18.170791
38.810861	1839.203594	18.175808
38.681966	1840.949369	18.180826
38.711334	1828.557727	18.185843
38.764206	1839.196648	18.190861
38.709186	1826.858119	18.195879
38.919966	1837.601824	18.200896
38.520177	1830.678294	18.205914
39.028367	1830.951825	18.210931
38.961001	1863.134651	18.215949
38.748203	1872.169092	18.220967
39.094658	1851.683451	18.225984
39.095342	1863.309959	18.231002
39.165277	1858.614947	18.236019
39.224339	1847.764840	18.241037
39.388181	1846.440377	18.246055
39.727749	1856.153557	18.251072
39.582475	1847.975198	18.256090
39.505655	1853.048541	18.261107
39.421059	1838.351859	18.266125
39.518270	1859.897811	18.271143
39.609622	1837.731544	18.276160
39.550641	1856.254282	18.281178
39.256697	1846.086606	18.286195
39.223110	1833.146318	18.291213
39.176565	1843.662427	18.296231
39.313230	1844.950617	18.301248
39.616441	1866.403393	18.306266
39.440765	1880.703536	18.311283
39.991929	1864.634683	18.316301
39.446610	1879.005160	18.321319
39.881004	1885.917291	18.326336
39.841087	1874.598968	18.331354
39.916317	1893.115612	18.336371
40.259587	1879.691531	18.341389
39.735938	1887.681889	18.346407
40.077510	1875.874323	18.351424
40.171026	1868.278717	18.356442
39.867369	1873.781604	18.361459
40.213343	1868.052380	18.366477
40.008639	1901.472319	18.371495
40.448822	1898.021474	18.376512
40.570205	1913.224642	18.381530
40.834182	1895.639728	18.386547
40.694325	1889.769663	18.391565
40.510443	1890.366875	18.396583
40.548497	1863.219574	18.401600
40.545272	1868.020672	18.406618
40.495309	1850.569171	18.411635
40.867020	1865.766054	18.416653
40.508602	1888.900539	18.421671
40.654741	1892.728321	18.426688
40.889838	1899.140324	18.431706
40.518375	1906.661728	18.436723
40.914700	1895.083834	18.441741
40.883504	1889.036885	18.446759
40.989379	1900.006198	18.451776
41.006262	1893.144761	18.456794
40.879421	1900.382476	18.461811
41.757213	1887.594526	18.466829
41.193890	1903.101350	18.471847
41.147060	1885.682750	18.476864
40.962963	1899.035761	18.481882
40.812607	1899.192968	18.486899
40.861448	1888.530116	18.491917
41.263405	1895.511379	18.496935
41.172145	1891.547390	18.501952
41.045474	1888.327402	18.506970
41.143706	1913.108771	18.511987
41.138189	1912.776086	18.517005
41.386372	1929.641957	18.522023
41.662249	1946.300257	18.527040
41.659914	1929.353201	18.532058
41.508091	1922.171270	18.537075
41.643884	1930.839141	18.542093
41.178743	1926.350030	18.547111
41.421100	1918.576976	18.552128
41.146803	1919.751427	18.557146
41.472641	1948.677531	18.562163
41.733424	1934.023662	18.567181
42.042800	1963.671082	18.572199
42.273167	1958.131174	18.577216
42.491152	1947.446627	18.582234
42.131617	1956.969159	18.587251
42.337568	1915.434174	18.592269
42.095514	1912.374561	18.597287
42.225178	1911.842896	18.602304
42.319724	1905.876225	18.607322
42.412315	1925.182213	18.612339
42.339539	1920.302143	18.617357
42.091482	1919.008151	18.622375
42.174871	1921.658246	18.627392
42.514171	1913.618433	18.632410
42.281808	1932.847447	18.637427
42.603821	1935.063400	18.642445
42.637036	1938.196110	18.647463
42.394097	1941.896013	18.652480
42.554356	1938.674652	18.657498
42.552441	1959.020421	18.662515
42.684199	1934.918756	18.667533
42.499994	1956.718102	18.672551
42.408367	1950.758266	18.677568
42.736535	1925.801278	18.682586
42.441989	1931.834667	18.687603
42.894666	1946.435781	18.692621
42.563282	1936.253173	18.697639
42.643089	1952.616776	18.702656
42.852335	1962.187417	18.707674
42.959735	1976.267181	18.712691
43.225232	1972.002133	18.717709
43.011569	1958.753470	18.722727
43.107349	1951.873950	18.727744
43.246927	1961.502748	18.732762
43.175765	1983.180812	18.737779
43.437348	1955.524940	18.742797
43.435557	1967.076162	18.747815
43.379414	1958.985850	18.752832
43.550871	1970.353946	18.757850
43.232548	1963.008897	18.762867
43.804549	1959.688786	18.767885
43.585925	1967.978812	18.772903
43.552452	1949.126798	18.777920
43.835394	1958.272932	18.782938
43.684916	1952.555751	18.787955
44.067134	1973.517560	18.792973
43.731460	1973.656680	18.797991
43.755133	1955.869032	18.803008
44.026210	1983.312302	18.808026
43.902046	1984.895924	18.813043
44.250235	1993.353172	18.818061
44.350285	1982.235811	18.823079
44.100581	1957.297018	18.828096
44.392636	1947.856495	18.833114
43.837919	1967.840564	18.838131
44.132460	1960.688277	18.843149
44.215788	1991.481071	18.848167
44.367046	1981.502382	18.853184
44.423769	1993.321562	18.858202
44.198541	1992.173665	18.863219
44.122682	1985.908706	18.868237
44.424821	1994.656782	18.873255
44.211816	1996.662689	18.878272
44.289782	1990.319266	18.883290
44.268290	1984.230132	18.888307
44.280796	1979.857213	18.893325
44.735482	2007.676705	18.898343
44.706732	2031.390569	18.903360
44.965877	2020.499009	18.908378
44.766509	2021.922160	18.913395
44.860480	2028.302332	18.918413
44.709728	2015.030037	18.923431
44.574239	2020.705839	18.928448
45.177425	2012.534292	18.933466
44.955906	2009.589649	18.938483
45.128847	2019.349265	18.943501
45.299323	2009.894550	18.948519
45.002158	2025.308505	18.953536
45.316437	2014.071974	18.958554
44.955106	2012.600764	18.963571
45.183659	2028.300022	18.968589
45.135120	2007.413981	18.973607
45.168995	1998.710948	18.978624
45.254982	2012.727662	18.983642
45.298583	2040.285875	18.988659
45.552860	2020.516101	18.993677
45.411424	2050.818399	18.998695
45.290096	2044.598423	19.003712
45.822594	2027.834578	19.008730
45.433728	2038.440159	19.013747
45.761310	2041.470416	19.018765
45.747951	2027.838260	19.023783
45.685265	2032.529572	19.028800
45.999053	2033.831512	19.033818
45.813572	2045.766039	19.038835
45.922464	2042.289511	19.043853
45.819896	2035.374437	19.048871
45.640146	2048.188373	19.053888
46.021408	2054.031502	19.058906
46.082072	2072.310950	19.063923
46.226204	2061.338681	19.068941
46.349521	2055.767126	19.073959
46.201844	2082.138638	19.078976
46.473553	2078.669737	19.083994
46.238976	2076.065073	19.089011
46.269789	2073.914693	19.094029
46.314002	2064.530014	19.099047
46.287923	2077.502405	19.104064
46.629862	2055.275126	19.109082
46.628544	2063.242533	19.114099
46.947388	2066.448125	19.119117
46.527319	2060.579229	19.124135
46.436675	2083.726536	19.129152
46.988735	2081.312194	19.134170
46.767200	2085.720772	19.139187
46.747432	2098.692925	19.144205
46.989167	2088.685635	19.149223
46.904987	2078.450960	19.154240
47.304804	2087.739738	19.159258
46.866942	2093.211544	19.164275
47.043981	2094.216164	19.169293
46.893947	2082.402786	19.174311
47.224235	2101.417496	19.179328
47.594784	2091.305663	19.184346
47.447987	2086.380893	19.189363
48.064160	2086.595156	19.194381
47.584050	2078.624342	19.199399
47.561697	2068.101750	19.204416
47.745214	2082.239985	19.209434
47.663482	2077.539857	19.214451
47.784770	2072.493932	19.219469
47.818801	2062.280671	19.224487
47.647429	2085.346456	19.229504
47.867421	2068.763517	19.234522
47.971298	2083.404493	19.239539
47.924182	2068.966014	19.244557
47.674546	2077.062932	19.249575
47.642394	2076.925458	19.254592
47.862463	2079.349092	19.259610
47.977103	2068.758297	19.264627
47.736815	2068.748312	19.269645
47.784457	2091.142396	19.274663
47.738505	2095.657764	19.279680
48.182153	2101.330099	19.284698
48.042315	2104.346584	19.289715
47.962282	2105.357866	19.294733
48.451149	2112.640855	19.299751
48.446199	2109.535524	19.304768
48.689786	2098.957646	19.309786
48.346960	2090.793401	19.314803
48.450555	2102.676856	19.319821
48.680151	2076.642206	19.324839
48.411573	2101.324878	19.329856
48.561317	2096.833398	19.334874
48.726973	2118.910335	19.339891
48.963561	2118.301064	19.344909
48.852797	2113.920432	19.349927
48.709692	2132.723107	19.354944
48.854837	2106.512926	19.359962
48.971818	2118.831408	19.364979
48.520602	2131.462656	19.369997
49.304668	2115.397468	19.375015
48.768671	2128.987540	19.380032
48.809431	2123.241349	19.385050
48.638566	2126.414613	19.390067
48.880746	2145.380465	19.395085
49.430101	2141.339971	19.400103
49.158368	2144.664431	19.405120
49.683984	2158.745219	19.410138
49.333129	2149.355511	19.415155
49.362486	2156.744177	19.420173
49.570536	2157.300051	19.425191
49.573473	2151.807892	19.430208
49.423047	2151.422587	19.435226
49.693750	2163.510127	19.440243
49.532826	2156.718204	19.445261
49.810066	2180.575597	19.450279
49.790487	2182.424387	19.455296
49.883879	2186.498617	19.460314
49.956923	2187.936697	19.465331
49.854129	2191.878022	19.470349
49.633195	2178.475671	19.475367
50.059962	2186.783058	19.480384
50.203487	2175.778923	19.485402
50.364042	2185.189373	19.490419
50.109859	2175.946146	19.495437
50.212723	2176.507201	19.500455
50.293190	2197.296287	19.505472
50.166441	2204.384154	19.510490
50.477205	2212.510758	19.515507
50.386545	2212.729054	19.520525
50.709334	2219.848923	19.525543
50.923788	2211.342661	19.530560
50.949488	2221.403856	19.535578
50.998724	2201.541180	19.540595
51.027075	2216.827630	19.545613
51.242450	2204.377983	19.550631
51.090629	2208.333909	19.555648
51.164373	2208.711620	19.560666
51.263734	2179.519030	19.565683
50.879178	2185.169035	19.570701
51.150778	2175.183914	19.575719
51.086990	2208.952529	19.580736
50.899382	2199.877980	19.585754
51.544847	2194.617855	19.590771
51.228508	2213.886191	19.595789
51.639462	2190.379317	19.600807
51.594121	2209.904782	19.605824
51.561878	2214.046820	19.610842
51.454970	2202.546346	19.615859
51.289863	2214.839682	19.620877
51.822027	2197.334396	19.625895
51.467428	2210.822233	19.630912
51.525559	2191.188179	19.635930
51.105050	2200.633255	19.640947
51.197315	2220.759904	19.645965
51.605215	2187.854719	19.650983
51.212594	2217.516785	19.656000
51.601543	2225.757226	19.661018
51.978298	2234.306722	19.666035
51.684209	2243.449089	19.671053
52.191837	2230.927310	19.676071
52.005149	2246.274321	19.681088
51.786735	2237.337496	19.686106
51.965749	2233.762442	19.691123
51.849475	2268.646173	19.696141
52.615705	2247.435430	19.701159
52.667579	2264.694287	19.706176
52.376673	2274.431522	19.711194
52.826363	2256.623314	19.716211
52.591605	2269.580065	19.721229
53.070962	2257.822851	19.726247
52.788042	2255.458390	19.731264
52.789694	2245.219457	19.736282
53.001081	2232.120555	19.741299
52.909868	2260.586629	19.746317
53.007890	2239.480809	19.751335
52.860605	2246.762412	19.756352
53.014325	2257.607067	19.761370
53.052007	2248.876495	19.766387
52.865112	2263.898021	19.771405
53.304321	2239.342086	19.776423
53.403420	2243.698215	19.781440
53.274088	2243.540092	19.786458
53.407123	2227.077339	19.791475
53.282944	2248.754699	19.796493
53.427459	2231.790717	19.801511
53.544417	2246.699819	19.806528
53.471700	2238.216593	19.811546
53.419723	2242.615991	19.816563
53.154293	2247.218747	19.821581
53.298263	2253.074892	19.826599
53.854520	2273.660673	19.831616
53.412278	2270.761803	19.836634
53.956411	2279.117944	19.841651
53.710592	2277.594258	19.846669
53.893094	2265.869364	19.851687
53.745844	2271.820484	19.856704
53.631180	2271.751260	19.861722
53.856521	2298.391564	19.866739
54.133520	2311.469850	19.871757
54.370193	2308.511331	19.876775
54.401091	2301.134191	19.881792
54.657339	2293.060080	19.886810
54.999433	2297.079660	19.891827
54.855469	2301.559030	19.896845
54.516185	2269.840751	19.901863
54.422452	2268.655259	19.906880
54.350754	2272.652283	19.911898
54.792626	2287.735450	19.916915
54.702849	2286.293243	19.921933
55.015438	2288.798849	19.926951
54.832651	2287.075013	19.931968
54.877834	2285.467612	19.936986
54.953723	2295.666405	19.942003
55.092152	2287.925888	19.947021
55.028306	2295.644440	19.952039
55.089366	2293.567759	19.957056
55.088335	2310.981648	19.962074
55.417812	2286.943296	19.967091
55.108272	2281.238106	19.972109
54.862514	2279.618755	19.977127
55.247754	2289.028551	19.982144
54.981709	2284.359506	19.987162
54.787612	2294.991630	19.992179
54.877683	2327.690172	19.997197
54.984093	2306.944823	20.002215
55.458746	2313.161434	20.007232
55.266358	2329.172158	20.012250
55.506022	2329.014660	20.017267
55.458271	2350.278022	20.022285
55.709618	2362.701443	20.027303
56.022732	2349.752730	20.032320
55.897445	2339.955904	20.037338
56.125019	2351.743583	20.042355
56.176766	2333.814660	20.047373
56.389714	2339.713171	20.052391
56.773530	2324.192967	20.057408
56.209508	2338.135141	20.062426
56.029427	2330.714321	20.067443
56.196159	2344.162769	20.072461
56.298580	2343.486699	20.077479
56.550374	2336.747537	20.082496
56.447743	2351.911498	20.087514
56.610146	2340.360905	20.092531
56.318124	2349.866322	20.097549
56.486444	2354.851886	20.102567
56.812128	2357.284486	20.107584
56.455095	2369.664968	20.112602
57.127534	2363.409738	20.117619
57.145005	2359.164020	20.122637
57.003257	2352.632186	20.127655
57.180877	2367.753393	20.132672
56.865587	2362.147729	20.137690
57.158735	2365.747138	20.142707
57.163559	2370.463709	20.147725
57.037743	2366.886448	20.152743
57.149432	2376.077174	20.157760
57.220136	2360.345332	20.162778
57.625023	2375.376833	20.167795
57.516652	2356.204661	20.172813
57.732805	2367.769473	20.177831
57.809978	2364.548567	20.182848
57.388812	2361.895763	20.187866
57.561133	2381.220345	20.192883
57.723906	2410.869337	20.197901
57.828569	2393.411053	20.202919
57.757265	2403.501979	20.207936
57.809311	2403.610291	20.212954
57.888835	2399.696971	20.217971
57.781041	2392.399981	20.222989
57.576266	2385.417991	20.228007
58.020209	2392.913132	20.233024
57.795701	2416.786299	20.238042
58.190950	2424.109216	20.243059
58.215724	2416.768854	20.248077
58.044830	2415.189275	20.253095
58.247066	2418.833439	20.258112
58.179674	2438.936569	20.263130
58.472261	2431.913305	20.268147
58.783810	2459.911283	20.273165
58.850387	2442.783992	20.278183
59.052681	2454.629463	20.283200
59.206576	2445.137168	20.288218
59.409425	2416.616882	20.293235
59.068691	2413.856501	20.298253
58.902064	2397.203359	20.303271
59.313774	2398.396546	20.308288
59.105428	2394.590829	20.313306
59.344102	2390.205217	20.318323
59.143308	2396.950347	20.323341
59.206239	2387.259177	20.328359
59.333999	2405.571037	20.333376
59.170374	2424.214886	20.338394
59.291057	2432.210249	20.343411
59.530576	2425.587627	20.348429
59.407313	2443.641061	20.353447
59.789923	2421.031492	20.358464
59.536599	2421.302456	20.363482
59.810051	2428.294572	20.368499
59.675703	2428.716124	20.373517
59.696027	2435.129499	20.378535
59.650697	2431.048643	20.383552
59.539257	2435.968869	20.388570
60.004412	2457.233630	20.393587
60.137323	2471.248914	20.398605
59.879895	2472.637316	20.403623
59.956735	2470.879215	20.408640
59.950480	2475.806870	20.413658
60.360816	2471.756003	20.418675
60.324744	2454.602557	20.423693
60.078789	2466.020415	20.428711
60.445277	2485.053238	20.433728
60.493162	2490.828516	20.438746
60.583878	2501.517441	20.443763
60.916739	2484.162268	20.448781
60.847193	2490.632835	20.453799
61.172449	2474.600975	20.458816
61.136267	2491.083813	20.463834
61.183643	2491.573550	20.468851
61.169873	2473.143754	20.473869
61.196096	2494.846598	20.478887
61.399710	2490.989115	20.483904
61.198571	2497.935890	20.488922
61.237359	2490.081836	20.493939
61.460926	2485.319027	20.498957
61.177930	2476.355338	20.503975
61.626121	2486.354369	20.508992
61.457950	2471.717832	20.514010
61.408686	2459.889577	20.519027
61.619369	2491.860966	20.524045
61.692909	2483.311316	20.529063
61.829447	2478.444010	20.534080
61.653962	2490.827654	20.539098
61.886958	2486.761410	20.544115
61.873976	2506.663541	20.549133
61.984922	2499.771232	20.554151
62.075342	2480.627069	20.559168
62.093973	2501.719852	20.564186
62.158566	2484.412160	20.569203
62.061081	2485.080142	20.574221
62.086109	2511.461837	20.579239
62.231420	2484.059234	20.584256
62.195189	2494.560896	20.589274
62.066101	2493.066315	20.594291
62.498634	2513.723842	20.599309
62.486073	2526.293748	20.604327
62.812920	2508.492560	20.609344
62.662894	2525.652812	20.614362
62.611117	2516.674115	20.619379
62.788778	2531.104831	20.624397
62.614873	2512.085990	20.629415
63.200448	2523.043102	20.634432
62.686133	2518.379190	20.639450
63.104600	2518.274613	20.644467
63.098033	2520.168334	20.649485
62.927305	2550.524973	20.654503
63.451760	2550.172598	20.659520
63.620796	2536.232332	20.664538
63.425576	2546.638470	20.669555
63.391180	2556.590148	20.674573
63.129645	2553.356287	20.679591
63.276212	2550.827906	20.684608
63.315074	2563.580656	20.689626
63.273441	2543.058834	20.694643
63.839278	2560.336422	20.699661
63.263571	2571.546487	20.704679
63.875399	2582.256622	20.709696
64.036359	2571.947845	20.714714
63.890954	2565.210452	20.719731
64.083590	2577.991141	20.724749
64.222643	2572.185730	20.729767
64.510119	2580.891100	20.734784
64.130359	2579.548548	20.739802
64.392037	2566.456994	20.744819
64.433971	2579.975084	20.749837
64.265312	2570.218541	20.754855
64.712146	2591.849063	20.759872
64.977803	2583.887796	20.764890
64.669624	2595.218803	20.769907
65.317364	2588.182835	20.774925
64.836261	2592.160404	20.779943
64.762051	2599.001025	20.784960
64.966325	2608.175803	20.789978
64.973330	2595.564436	20.794995
65.638584	2585.263246	20.800013
65.400180	2594.154921	20.805031
65.494070	2587.287436	20.810048
65.587259	2584.989689	20.815066
65.676088	2581.327701	20.820083
65.576442	2574.747482	20.825101
65.410283	2577.776085	20.830119
65.994753	2563.645900	20.835136
65.595100	2577.138155	20.840154
65.621576	2566.263895	20.845171
65.717866	2589.549158	20.850189
65.596050	2586.277243	20.855207
65.786946	2576.834651	20.860224
66.002121	2578.738973	20.865242
65.406065	2599.413464	20.870259
65.657027	2587.578208	20.875277
65.494383	2598.669844	20.880295
65.979756	2618.335456	20.885312
66.054327	2604.081848	20.890330
65.773374	2617.830272	20.895347
66.185780	2590.899410	20.900365
66.218989	2617.001430	20.905383
66.590090	2639.904593	20.910400
66.991266	2641.147960	20.915418
66.937619	2627.988990	20.920435
67.003329	2628.436140	20.925453
66.835732	2621.528398	20.930471
67.008726	2633.155062	20.935488
66.838716	2632.771996	20.940506
67.026649	2635.471858	20.945523
67.173958	2630.867255	20.950541
67.057319	2642.062721	20.955559
67.139078	2622.019546	20.960576
67.216808	2628.800431	20.965594
67.329032	2626.988440	20.970611
66.940882	2629.423708	20.975629
67.213144	2614.965398	20.980647
67.330297	2632.781715	20.985664
67.204995	2645.627596	20.990682
67.460998	2660.905210	20.995699
67.572524	2667.803346	21.000717
67.391835	2655.229638	21.005735
67.334328	2682.982361	21.010752
67.746283	2667.259356	21.015770
67.576812	2687.098418	21.020787
67.834598	2696.168946	21.025805
68.017139	2683.769018	21.030823
68.002399	2686.889336	21.035840
68.216222	2697.541324	21.040858
68.101661	2705.269052	21.045875
68.428313	2687.143129	21.050893
68.200917	2711.227239	21.055911
68.627216	2706.607017	21.060928
68.935000	2703.681154	21.065946
68.571054	2728.410016	21.070963
68.849419	2710.766390	21.075981
69.058833	2718.218767	21.080999
68.875482	2716.370188	21.086016
69.072123	2719.266631	21.091034
68.844568	2717.770389	21.096051
69.177514	2716.566314	21.101069
69.225228	2711.766953	21.106087
68.795513	2729.354701	21.111104
68.773748	2718.892581	21.116122
68.845142	2708.179279	21.121139
69.302212	2721.969004	21.126157
69.176054	2741.211294	21.131175
69.283418	2734.651908	21.136192
69.769905	2733.200639	21.141210
69.717610	2740.624827	21.146227
69.432179	2735.328420	21.151245
69.652138	2756.451069	21.156263
70.088072	2756.365255	21.161280
70.418945	2764.682900	21.166298
70.459738	2766.224973	21.171315
70.398097	2753.381151	21.176333
70.297263	2751.146737	21.181351
70.393615	2755.215905	21.186368
70.253926	2767.225007	21.191386
70.432213	2768.604810	21.196403
70.857049	2749.634942	21.201421
70.714374	2768.397776	21.206439
70.790682	2759.803032	21.211456
71.087882	2753.473454	21.216474
71.064808	2762.207611	21.221491
71.052083	2755.260438	21.226509
70.777950	2754.200769	21.231527
71.120775	2759.394606	21.236544
71.302776	2760.887756	21.241562
70.965339	2755.007691	21.246579
71.081584	2756.989400	21.251597
70.885134	2757.452518	21.256615
70.909408	2762.027628	21.261632
71.316151	2767.285501	21.266650
70.945465	2781.179787	21.271667
71.543106	2767.842411	21.276685
71.564119	2784.690472	21.281703
71.421416	2784.049576	21.286720
71.703769	2772.165690	21.291738
71.513492	2786.863130	21.296755
71.552270	2767.868464	21.301773
71.717892	2798.961442	21.306791
71.974079	2806.000673	21.311808
72.071856	2808.870169	21.316826
71.890770	2827.174127	21.321843
72.280800	2809.622158	21.326861
72.435486	2824.450793	21.331879
72.095485	2806.512640	21.336896
72.581803	2800.549378	21.341914
72.371194	2810.984808	21.346931
72.399182	2792.401488	21.351949
72.544724	2818.852562	21.356967
72.830819	2832.222666	21.361984
72.553918	2840.771872	21.367002
72.732000	2844.378993	21.372019
72.732519	2839.361436	21.377037
73.285082	2835.678064	21.382055
72.994915	2854.761795	21.387072
73.286391	2840.533731	21.392090
73.138010	2863.477409	21.397107
73.239616	2828.347939	21.402125
73.183049	2831.085878	21.407143
73.464221	2869.129881	21.412160
73.677821	2864.828979	21.417178
73.308579	2885.135112	21.422195
73.805889	2891.212604	21.427213
73.904910	2875.940459	21.432231
73.540376	2869.985113	21.437248
74.028128	2871.736766	21.442266
73.943658	2851.718990	21.447283
73.731297	2877.239866	21.452301
74.019757	2869.176862	21.457319
73.818969	2883.858417	21.462336
74.157843	2884.526346	21.467354
74.021721	2889.531099	21.472371
74.140528	2886.361071	21.477389
74.493054	2879.734737	21.482407
74.233459	2891.386631	21.487424
74.875587	2924.787636	21.492442
74.745232	2924.241335	21.497459
74.727463	2929.081088	21.502477
75.308972	2918.848432	21.507495
74.927253	2916.610219	21.512512
75.336490	2910.772237	21.517530
75.003417	2914.526041	21.522547
75.006982	2911.268568	21.527565
75.508806	2919.440345	21.532583
75.111160	2913.918354	21.537600
75.133537	2931.571370	21.542618
75.158883	2918.266044	21.547635
75.281435	2922.492522	21.552653
75.335273	2938.381505	21.557671
75.338180	2934.208499	21.562688
75.816676	2935.009048	21.567706
75.399741	2944.049309	21.572723
75.713086	2945.466843	21.577741
75.973199	2965.694668	21.582759
76.091669	2968.137793	21.587776
76.482713	2970.739591	21.592794
76.524130	2974.846436	21.597811
76.464265	2953.569492	21.602829
76.643216	2954.591962	21.607847
76.653037	2951.738321	21.612864
76.802541	2947.645404	21.617882
76.995901	2965.411132	21.622899
76.788694	2960.802424	21.627917
76.993308	2966.934613	21.632935
76.758642	2967.588675	21.637952
76.879521	2951.078542	21.642970
77.140353	2966.076168	21.647987
76.951917	2944.184338	21.653005
77.035089	2958.984767	21.658023
77.303614	2960.095770	21.663040
77.306174	2940.189860	21.668058
76.786669	2962.132739	21.673075
77.198049	2977.919772	21.678093
77.476165	2979.481303	21.683111
77.230098	2998.365427	21.688128
77.399930	2984.194730	21.693146
77.320146	2968.231063	21.698163
77.472747	2992.283523	21.703181
77.978083	3014.272844	21.708199
77.670617	3021.937146	21.713216
78.093308	3022.184191	21.718234
77.868859	3020.425034	21.723251
78.186545	3032.806347	21.728269
78.643457	3015.314935	21.733287
78.130577	3017.651005	21.738304
78.200225	3015.006337	21.743322
78.469044	3027.152049	21.748339
78.462584	3045.459689	21.753357
78.626232	3033.011033	21.758375
78.677913	3049.938165	21.763392
78.641657	3031.143151	21.768410
79.069336	3050.295290	21.773427
78.986369	3052.861272	21.778445
79.356092	3039.959511	21.783463
79.174667	3045.695931	21.788480
79.293955	3027.136409	21.793498
79.514049	3049.669317	21.798515
79.462861	3060.829864	21.803533
79.806702	3060.684868	21.808551
79.880015	3063.010681	21.813568
79.741380	3053.963553	21.818586
79.762059	3070.045532	21.823603
79.903891	3058.453122	21.828621
80.122016	3069.624874	21.833639
79.770822	3078.504366	21.838656
80.120208	3071.553505	21.843674
80.256718	3072.488913	21.848691
79.944255	3051.376593	21.853709
80.473319	3064.204837	21.858727
80.359970	3041.391310	21.863744
80.448403	3058.106496	21.868762
80.286865	3069.414798	21.873779
80.469303	3075.679814	21.878797
80.869372	3090.128234	21.883815
80.642335	3096.111356	21.888832
80.916912	3079.452079	21.893850
80.726062	3080.657701	21.898867
80.390015	3096.234349	21.903885
80.773369	3079.580322	21.908903
80.462148	3106.317583	21.913920
80.903842	3131.976440	21.918938
80.841742	3126.196386	21.923955
81.074066	3132.115424	21.928973
81.585167	3139.647863	21.933991
81.104855	3135.980002	21.939008
81.234590	3133.793051	21.944026
81.589403	3142.533080	21.949043
81.857958	3149.029145	21.954061
81.989255	3150.850758	21.959079
82.474811	3178.283553	21.964096
82.392054	3168.414611	21.969114
82.444870	3128.153104	21.974131
82.343898	3138.232092	21.979149
82.885055	3139.762376	21.984167
82.281710	3135.366305	21.989184
82.703543	3149.681473	21.994202
82.701719	3123.985922	21.999219
82.479773	3139.465617	22.004237
82.721929	3158.226153	22.009255
82.564535	3170.903580	22.014272
82.949040	3152.831718	22.019290
83.196843	3158.893074	22.024307
83.095298	3151.984806	22.029325
83.065292	3160.699470	22.034343
82.647804	3159.391836	22.039360
83.028678	3152.560132	22.044378
83.150111	3172.836932	22.049395
82.947608	3177.666546	22.054413
83.071431	3194.959435	22.059431
83.325987	3197.483051	22.064448
83.523267	3195.931516	22.069466
83.823890	3203.895971	22.074483
83.920772	3220.564469	22.079501
84.099751	3214.223140	22.084519
83.876358	3225.199687	22.089536
84.211440	3235.788117	22.094554
84.259340	3214.133987	22.099571
84.308890	3228.875671	22.104589
84.727927	3212.047316	22.109607
84.610671	3217.466140	22.114624
84.639840	3226.104730	22.119642
84.808066	3200.670882	22.124659
84.558969	3217.115869	22.129677
84.935316	3207.585953	22.134695
84.982632	3213.915870	22.139712
84.970057	3217.259734	22.144730
84.924054	3200.478714	22.149747
85.125090	3236.595139	22.154765
85.416988	3217.614779	22.159783
85.401963	3232.641520	22.164800
85.261748	3233.312855	22.169818
85.661875	3223.461315	22.174835
85.624823	3246.677490	22.179853
85.708363	3224.583838	22.184871
85.391496	3237.863795	22.189888
85.511108	3229.341154	22.194906
86.247299	3247.812307	22.199923
86.051953	3274.949961	22.204941
86.150095	3264.206265	22.209959
85.993850	3265.893339	22.214976
86.121772	3277.297252	22.219994
86.251442	3262.779625	22.225011
86.148591	3272.513966	22.230029
86.288588	3256.058807	22.235047
86.328544	3281.830163	22.240064
86.452785	3274.263725	22.245082
86.528988	3287.835822	22.250099
86.477087	3290.510479	22.255117
86.638837	3289.874757	22.260135
86.622222	3306.672722	22.265152
86.742599	3320.902248	22.270170
87.041524	3320.289325	22.275187
87.029516	3324.369071	22.280205
87.270632	3309.645600	22.285223
87.362364	3332.527267	22.290240
87.740950	3345.118629	22.295258
87.724477	3326.313885	22.300275
87.837665	3350.480886	22.305293
87.955132	3342.978127	22.310311
87.916520	3340.182806	22.315328
87.984748	3350.854189	22.320346
88.669578	3319.000531	22.325363
88.098141	3326.802296	22.330381
88.201936	3330.768035	22.335399
88.453466	3318.760096	22.340416
88.169290	3330.961212	22.345434
88.426962	3334.833026	22.350451
88.675827	3348.543164	22.355469
89.112685	3355.422097	22.360487
88.877669	3341.277032	22.365504
88.799787	3347.289142	22.370522
89.013694	3358.174624	22.375539
88.959875	3342.710956	22.380557
89.243562	3356.585607	22.385575
89.335086	3363.205299	22.390592
89.367879	3350.414463	22.395610
89.185852	3359.596445	22.400627
89.443682	3353.986645	22.405645
89.124910	3366.954458	22.410663
89.327909	3360.572490	22.415680
89.429779	3370.965519	22.420698
89.867998	3378.971889	22.425715
89.749521	3363.280324	22.430733
90.045819	3369.527039	22.435751
90.089005	3388.810847	22.440768
90.109190	3368.661139	22.445786
90.238719	3401.228681	22.450803
90.206645	3420.726128	22.455821
90.354139	3393.873271	22.460839
90.574032	3396.329623	22.465856
90.219113	3419.748177	22.470874
90.679514	3404.350839	22.475891
90.694126	3421.977158	22.480909
90.777448	3432.097727	22.485927
90.861866	3441.835084	22.490944
90.769789	3450.861323	22.495962
91.074761	3437.272354	22.500979
91.107242	3444.722042	22.505997
91.651035	3458.560298	22.511015
91.644739	3449.520987	22.516032
91.336332	3473.559441	22.521050
91.973770	3474.316633	22.526067
91.738176	3464.867014	22.531085
92.090464	3472.046957	22.536103
92.192604	3467.366900	22.541120
91.912990	3458.298739	22.546138
91.957654	3467.694484	22.551155
92.082329	3468.722219	22.556173
91.989151	3468.258329	22.561191
92.457084	3478.438984	22.566208
92.328606	3489.056361	22.571226
92.681352	3488.211525	22.576243
92.797877	3484.691783	22.581261
92.550589	3500.610242	22.586279
93.123915	3483.737594	22.591296
92.675420	3494.620633	22.596314
92.978925	3484.216046	22.601331
92.833273	3505.549733	22.606349
92.901928	3509.521325	22.611367
93.514399	3529.942433	22.616384
93.088136	3521.167147	22.621402
93.184551	3528.031554	22.626419
93.255732	3532.001160	22.631437
93.387407	3555.581223	22.636455
93.726604	3540.836798	22.641472
93.804534	3546.057158	22.646490
94.195712	3540.550049	22.651507
94.158862	3544.008615	22.656525
94.112829	3542.890529	22.661543
94.162471	3543.467910	22.666560
94.143681	3557.185459	22.671578
94.251520	3565.232545	22.676595
94.392158	3564.395396	22.681613
94.305999	3575.930175	22.686631
94.473736	3555.394453	22.691648
94.641106	3575.268159	22.696666
95.182318	3586.021770	22.701683
94.852424	3601.478035	22.706701
95.086996	3588.715662	22.711719
95.327439	3594.797303	22.716736
94.978522	3615.164218	22.721754
95.506841	3582.326119	22.726771
95.720979	3599.251415	22.731789
95.388786	3589.495463	22.736807
95.722990	3580.408470	22.741824
95.981843	3575.494626	22.746842
96.128958	3579.509959	22.751859
95.991297	3579.487240	22.756877
95.753262	3604.016393	22.761895
96.256017	3603.219987	22.766912
96.262175	3630.148404	22.771930
96.234874	3611.168934	22.776947
96.589041	3626.675166	22.781965
96.498970	3623.412349	22.786983
96.753320	3604.917604	22.792000
96.516937	3619.608887	22.797018
96.813852	3619.836379	22.802035
97.042969	3625.228028	22.807053
97.058340	3633.095759	22.812071
97.125745	3647.572118	22.817088
97.032223	3638.697689	22.822106
97.062242	3647.328698	22.827123
97.014713	3644.967637	22.832141
96.875271	3665.816500	22.837159
97.408225	3682.397100	22.842176
97.493315	3681.236471	22.847194
97.414755	3686.995693	22.852211
97.656571	3676.335049	22.857229
97.787333	3700.667792	22.862247
97.912456	3694.327491	22.867264
97.829327	3691.385536	22.872282
98.002717	3705.970214	22.877299
97.930604	3711.205779	22.882317
98.389879	3734.849493	22.887335
98.226856	3739.455056	22.892352
98.698283	3737.675108	22.897370
98.675148	3730.873301	22.902387
99.001534	3722.481760	22.907405
99.226962	3726.770982	22.912423
99.498834	3742.632441	22.917440
99.440143	3743.473187	22.922458
99.610136	3741.206866	22.927475
100.008802	3725.647573	22.932493
99.926855	3722.508383	22.937511
99.873652	3708.975215	22.942528
99.910219	3715.337820	22.947546
100.080705	3703.398878	22.952563
100.195915	3698.370553	22.957581
99.917435	3715.621457	22.962599
99.890690	3707.913431	22.967616
100.198983	3730.446538	22.972634
100.133438	3723.816100	22.977651
100.500646	3737.431445	22.982669
100.297390	3738.907258	22.987687
100.640710	3737.383896	22.992704
100.385675	3745.892785	22.997722
100.363049	3760.639424	23.002739
100.512729	3771.934013	23.007757
100.673537	3767.643750	23.012775
100.720317	3768.736343	23.017792
100.945251	3779.835247	23.022810
101.023461	3789.739389	23.027827
101.071519	3782.835446	23.032845
101.220994	3773.399167	23.037863
101.507339	3807.191765	23.042880
101.434189	3805.069150	23.047898
101.257924	3827.182501	23.052915
101.639837	3817.245807	23.057933
101.289181	3842.779121	23.062951
101.728569	3832.483335	23.067968
101.763221	3846.211205	23.072986
102.234777	3866.888512	23.078003
102.180433	3851.575003	23.083021
102.259158	3854.004169	23.088039
102.652027	3853.615453	23.093056
102.552851	3864.144391	23.098074
102.682197	3881.062356	23.103091
103.081859	3865.281315	23.108109
102.922654	3885.776281	23.113127
103.355108	3883.124070	23.118144
103.042276	3882.588990	23.123162
102.917875	3902.958943	23.128179
103.546225	3883.117887	23.133197
103.260078	3870.527544	23.138215
103.529062	3898.108428	23.143232
103.481526	3912.334161	23.148250
103.472319	3918.863854	23.153267
103.627914	3917.694706	23.158285
103.404279	3933.143191	23.163303
104.165502	3930.070917	23.168320
103.923237	3947.600724	23.173338
104.174784	3942.295869	23.178355
104.827372	3941.534724	23.183373
104.335700	3931.065185	23.188391
104.778891	3956.787962	23.193408
104.752407	3948.363866	23.198426
104.911466	3950.236890	23.203443
105.138222	3958.584198	23.208461
105.125420	3965.777854	23.213479
104.956395	3952.046892	23.218496
105.185594	3966.577321	23.223514
105.498500	3976.078056	23.228531
105.504867	3977.185412	23.233549
105.449265	3993.429374	23.238567
105.879969	3993.119044	23.243584
105.950779	3987.774358	23.248602
105.708797	3995.307064	23.253619
106.074417	3979.461064	23.258637
105.769739	3992.072364	23.263655
106.086464	3998.020700	23.268672
106.124305	4003.092335	23.273690
106.177414	4010.219612	23.278707
106.430319	4005.096785	23.283725
106.226002	4023.472725	23.288743
106.615362	4027.139893	23.293760
106.473617	4051.146977	23.298778
106.815559	4061.934637	23.303795
107.313892	4040.466914	23.308813
106.958252	4046.113401	23.313831
107.119187	4062.684629	23.318848
107.379892	4061.687070	23.323866
107.719312	4069.602455	23.328883
107.775003	4075.051068	23.333901
107.694535	4067.749949	23.338919
107.872869	4065.932182	23.343936
108.060669	4060.292167	23.348954
107.910208	4071.996595	23.353971
108.293793	4081.868375	23.358989
108.669279	4093.171356	23.364007
108.662333	4088.941796	23.369024
108.701731	4092.293204	23.374042
108.764478	4088.008035	23.379059
109.429751	4075.068584	23.384077
108.956092	4078.735861	23.389095
109.156523	4082.338991	23.394112
109.003492	4091.240051	23.399130
108.994956	4098.665730	23.404147
109.205382	4081.703984	23.409165
108.971980	4093.447723	23.414183
109.278793	4080.623404	23.419200
109.485392	4088.593030	23.424218
109.138963	4108.016128	23.429235
109.426992	4101.972939	23.434253
109.390570	4118.170558	23.439271
109.639967	4123.471043	23.444288
109.894675	4119.448226	23.449306
109.646661	4141.851035	23.454323
109.671937	4160.541545	23.459341
109.860005	4158.644603	23.464359
110.041296	4185.190533	23.469376
110.340800	4159.850145	23.474394
110.193232	4181.196298	23.479411
110.980864	4191.724976	23.484429
110.823642	4196.769462	23.489447
110.982732	4203.706880	23.494464
111.386496	4186.840232	23.499482
111.459234	4201.536495	23.504499
111.770694	4196.347239	23.509517
111.663605	4207.695796	23.514535
111.641814	4202.363188	23.519552
112.258484	4214.933834	23.524570
112.679331	4215.236130	23.529587
112.725792	4190.987859	23.534605
112.489084	4176.484447	23.539623
112.433907	4184.748944	23.544640
112.385678	4174.831922	23.549658
112.579950	4199.252589	23.554675
112.941197	4189.735986	23.559693
112.817632	4198.945218	23.564711
113.150719	4210.414341	23.569728
113.112522	4191.674730	23.574746
112.931922	4191.324079	23.579763
113.091224	4191.566054	23.584781
113.197320	4182.504199	23.589799
113.540700	4205.482578	23.594816
113.982775	4184.466061	23.599834
113.425452	4209.654616	23.604851
113.636598	4221.902530	23.609869
113.506750	4219.904183	23.614887
113.613888	4228.395809	23.619904
113.747335	4219.982931	23.624922
113.673919	4242.489313	23.629939
113.883403	4241.949403	23.634957
113.915770	4242.563916	23.639975
114.101612	4265.411728	23.644992
114.468892	4270.673100	23.650010
114.293674	4286.718639	23.655027
114.645878	4305.577342	23.660045
114.899119	4300.918914	23.665063
114.639509	4323.024304	23.670080
114.995612	4321.309412	23.675098
114.923926	4324.612693	23.680115
114.752211	4328.971055	23.685133
114.986931	4346.954367	23.690151
115.234709	4359.184919	23.695168
115.587906	4346.887741	23.700186
115.439083	4378.739972	23.705203
115.811941	4374.917245	23.710221
116.061484	4381.923259	23.715239
116.097588	4390.906620	23.720256
116.210937	4371.496099	23.725274
116.247119	4392.159441	23.730291
116.486075	4402.134064	23.735309
116.599861	4423.195637	23.740327
117.096974	4421.796008	23.745344
117.044804	4424.225241	23.750362
117.131142	4408.753292	23.755379
117.302191	4406.508354	23.760397
117.635016	4396.704990	23.765415
117.347283	4397.959397	23.770432
117.596029	4403.626611	23.775450
117.492452	4387.647497	23.780467
117.554898	4413.158366	23.785485
118.081952	4432.082816	23.790503
117.982035	4437.024605	23.795520
118.086986	4445.645449	23.800538
117.908306	4433.449871	23.805555
118.238792	4439.946485	23.810573
118.196438	4434.199489	23.815591
118.505541	4439.615410	23.820608
118.754161	4464.606635	23.825626
118.520996	4458.433690	23.830643
118.744343	4469.423906	23.835661
118.859533	4462.531992	23.840679
118.868380	4480.608688	23.845696
119.125651	4489.305565	23.850714
119.028512	4489.079694	23.855731
119.117554	4497.891381	23.860749
119.560725	4507.124861	23.865767
119.655948	4515.499717	23.870784
119.763241	4510.050793	23.875802
119.645012	4516.269625	23.880819
119.840073	4533.130988	23.885837
119.939978	4553.225363	23.890855
120.380522	4541.569099	23.895872
120.824671	4558.253898	23.900890
120.718001	4551.103729	23.905907
120.821491	4535.475279	23.910925
121.014417	4540.265957	23.915943
120.929388	4554.216590	23.920960
121.009221	4556.892530	23.925978
120.991263	4568.071900	23.930995
121.010853	4581.350949	23.936013
121.213231	4565.762426	23.941031
121.136786	4585.520242	23.946048
121.484073	4604.516733	23.951066
121.639741	4603.262092	23.956083
121.836539	4607.928530	23.961101
122.125039	4607.899954	23.966119
122.147949	4638.150737	23.971136
122.727972	4637.429508	23.976154
122.854748	4621.598307	23.981171
123.068334	4634.950069	23.986189
123.217038	4614.593254	23.991207
122.733327	4619.401672	23.996224
122.832129	4620.124906	24.001242
122.959062	4605.648798	24.006259
122.956714	4624.106246	24.011277
123.173214	4616.461705	24.016295
123.094581	4654.520152	24.021312
123.527815	4653.633022	24.026330
123.521055	4640.828563	24.031347
123.956616	4626.851430	24.036365
124.043047	4634.521120	24.041383
123.635257	4649.613742	24.046400
123.767846	4674.401253	24.051418
124.068615	4695.649226	24.056435
124.215431	4691.864561	24.061453
124.436746	4674.058251	24.066471
124.273549	4692.919522	24.071488
124.437024	4696.739531	24.076506
124.325789	4706.069466	24.081523
124.681098	4716.429394	24.086541
124.630465	4735.022117	24.091559
124.828972	4733.278105	24.096576
125.037986	4739.212244	24.101594
125.356507	4743.450737	24.106611
125.180232	4762.038270	24.111629
125.667947	4768.536601	24.116647
125.507821	4763.292013	24.121664
125.677312	4763.739401	24.126682
125.997452	4776.369742	24.131699
126.421763	4773.707312	24.136717
126.384938	4784.772633	24.141735
126.392606	4785.183769	24.146752
126.697663	4795.478039	24.151770
126.388086	4790.263255	24.156787
126.669274	4805.790212	24.161805
127.241250	4814.734482	24.166823
127.234350	4821.592914	24.171840
127.594389	4804.706839	24.176858
127.791256	4805.771752	24.181875
127.645490	4809.060999	24.186893
127.859049	4808.750712	24.191911
127.909024	4823.189908	24.196928
128.139478	4803.659890	24.201946
128.110221	4823.346430	24.206963
127.838545	4815.870648	24.211981
128.613165	4827.744042	24.216999
128.384588	4839.152505	24.222016
128.716212	4818.445512	24.227034
128.973588	4840.719359	24.232051
128.722588	4829.019673	24.237069
128.982561	4828.544236	24.242087
128.855190	4856.896260	24.247104
129.005912	4855.491234	24.252122
129.255019	4869.247171	24.257139
129.036313	4860.596075	24.262157
129.363655	4862.642979	24.267175
129.344355	4894.668566	24.272192
129.641476	4886.380253	24.277210
129.977805	4900.642281	24.282227
130.474069	4913.024732	24.287245
130.612457	4918.192258	24.292263
130.394393	4921.321426	24.297280
130.690038	4926.753130	24.302298
130.976257	4917.766596	24.307315
130.830902	4921.385329	24.312333
130.830301	4928.585289	24.317351
131.195225	4910.367967	24.322368
131.327788	4897.576101	24.327386
131.222141	4915.332850	24.332403
131.291445	4910.690463	24.337421
131.630819	4938.521412	24.342439
131.703191	4963.353193	24.347456
131.962435	4945.811961	24.352474
131.762154	4928.371878	24.357491
131.642892	4943.159231	24.362509
131.948768	4946.486083	24.367527
132.022652	4949.893396	24.372544
131.980466	4948.988353	24.377562
132.044128	4972.667246	24.382579
132.017788	4991.760204	24.387597
132.256552	4996.958415	24.392615
132.552445	4996.598693	24.397632
132.807958	5027.125582	24.402650
132.930170	5005.782068	24.407667
133.321196	5023.919474	24.412685
133.194110	5052.154876	24.417703
133.159524	5044.518151	24.422720
133.422308	5055.099504	24.427738
133.632508	5055.745689	24.432755
133.804516	5063.552239	24.437773
133.783562	5078.949471	24.442791
134.110465	5087.098162	24.447808
134.104627	5085.332365	24.452826
134.477142	5091.340017	24.457843
134.499737	5111.230562	24.462861
134.797809	5112.039399	24.467879
134.770387	5103.751448	24.472896
135.140725	5141.761702	24.477914
135.550785	5135.853860	24.482931
134.866981	5143.374297	24.487949
135.593540	5128.937993	24.492967
135.741037	5128.283886	24.497984
135.784430	5125.592213	24.503002
136.049136	5143.474249	24.508019
136.111627	5151.071376	24.513037
136.338392	5146.713536	24.518055
136.946180	5148.964537	24.523072
137.113625	5156.356131	24.528090
137.013715	5155.210215	24.533107
137.008707	5141.663305	24.538125
137.002642	5155.549065	24.543143
137.242535	5142.144761	24.548160
136.983162	5141.836631	24.553178
137.346511	5140.056674	24.558195
137.420371	5154.346952	24.563213
137.320190	5170.833375	24.568231
137.672722	5170.454842	24.573248
137.712957	5165.853010	24.578266
137.967604	5194.196855	24.583283
138.004153	5189.756652	24.588301
138.262024	5189.617388	24.593319
138.195562	5208.590074	24.598336
138.368708	5207.026189	24.603354
138.696866	5222.215478	24.608371
138.726671	5244.576723	24.613389
138.865407	5230.412265	24.618407
139.089195	5235.992570	24.623424
139.204989	5247.341277	24.628442
139.513495	5270.941189	24.633459
139.329569	5268.569346	24.638477
139.514825	5251.211262	24.643495
139.609956	5271.223888	24.648512
139.640135	5264.318107	24.653530
140.068931	5289.035999	24.658547
139.807509	5293.101175	24.663565
140.078702	5298.294129	24.668583
140.006556	5314.078411	24.673600
140.376202	5326.685666	24.678618
140.333686	5340.946524	24.683635
140.564980	5353.655405	24.688653
141.015297	5344.812384	24.693671
141.588603	5365.529216	24.698688
141.293396	5346.791309	24.703706
141.489527	5354.737332	24.708723
141.372782	5362.510641	24.713741
141.686660	5388.822146	24.718759
142.020639	5383.720908	24.723776
141.877801	5385.104996	24.728794
142.212235	5381.547441	24.733811
142.108871	5392.008418	24.738829
142.254902	5406.340940	24.743847
142.497580	5399.252737	24.748864
142.305346	5421.583600	24.753882
142.838148	5400.028388	24.758899
143.024028	5423.508632	24.763917
143.112841	5425.033193	24.768935
143.369578	5442.888149	24.773952
143.028654	5438.880343	24.778970
143.542073	5455.307803	24.783987
143.890902	5444.934187	24.789005
143.778263	5447.759807	24.794023
144.248727	5467.404354	24.799040
144.115657	5470.570376	24.804058
144.338156	5471.736223	24.809075
144.259649	5471.003694	24.814093
144.470512	5467.477169	24.819111
145.131807	5480.549765	24.824128
145.022298	5494.897428	24.829146
145.044547	5487.888524	24.834163
145.104331	5486.836279	24.839181
145.033149	5482.021652	24.844199
145.189080	5500.492963	24.849216
145.381644	5523.736023	24.854234
145.350253	5530.069261	24.859251
145.174664	5539.931612	24.864269
145.590091	5559.414102	24.869287
145.891750	5558.964436	24.874304
145.840754	5586.391736	24.879322
146.087790	5574.940311	24.884339
146.126100	5590.479444	24.889357
146.584461	5619.541227	24.894375
146.744889	5618.444389	24.899392
146.634287	5633.490821	24.904410
147.167949	5661.043310	24.909427
147.051040	5655.347553	24.914445
147.466541	5667.389604	24.919463
147.534799	5668.487641	24.924480
147.443727	5681.689058	24.929498
147.812292	5682.245713	24.934515
148.027313	5703.999027	24.939533
148.320918	5699.173664	24.944551
148.455269	5712.713471	24.949568
148.373083	5706.070959	24.954586
148.279838	5719.694052	24.959603
148.938875	5744.185241	24.964621
148.904539	5739.671157	24.969639
148.879696	5738.953371	24.974656
148.850779	5757.483485	24.979674
149.230099	5766.307772	24.984691
149.296865	5755.316738	24.989709
149.544985	5793.578321	24.994727
149.952067	5800.846367	24.999744
149.802882	5807.372028	25.004762
150.185524	5814.036206	25.009779
150.377776	5824.366335	25.014797
150.297463	5823.815202	25.019815
150.389643	5840.018560	25.024832
150.633951	5828.565038	25.029850
150.972946	5842.521173	25.034867
151.168076	5858.697303	25.039885
151.184555	5859.954313	25.044903
151.345966	5859.447100	25.049920
151.289378	5868.394658	25.054938
151.848983	5869.740677	25.059955
151.709148	5897.021773	25.064973
151.598704	5890.295263	25.069991
151.720922	5883.630711	25.075008
151.654408	5914.794087	25.080026
152.369941	5902.981918	25.085043
152.350088	5914.635829	25.090061
152.495001	5927.487414	25.095079
153.022090	5925.959864	25.100096
152.704851	5953.647565	25.105114
153.141673	5932.292142	25.110131
153.350824	5962.948613	25.115149
153.302648	5966.168429	25.120167
153.374101	5967.691582	25.125184
153.796980	5986.759171	25.130202
153.735460	5968.893781	25.135219
154.329157	5989.242301	25.140237
154.054484	6006.174218	25.145255
154.337629	5992.018282	25.150272
154.067300	6003.325429	25.155290
154.454391	6016.658764	25.160307
154.890739	6003.362612	25.165325
155.076882	6018.971452	25.170343
155.395508	6017.237769	25.175360
155.421715	6046.493815	25.180378
155.553733	6042.207687	25.185395
155.968499	6055.078573	25.190413
155.873503	6066.085117	25.195431
156.137232	6042.758771	25.200448
156.162054	6075.548057	25.205466
156.589516	6074.764967	25.210483
156.833534	6074.768944	25.215501
156.661787	6097.768701	25.220519
156.799524	6074.773387	25.225536
156.922566	6091.744018	25.230554
157.127186	6109.340611	25.235571
157.136200	6113.615663	25.240589
157.185850	6129.359382	25.245607
157.436458	6126.235626	25.250624
157.804657	6140.139954	25.255642
157.767688	6156.037000	25.260659
157.943195	6145.984106	25.265677
158.407133	6143.523976	25.270695
158.677110	6134.339413	25.275712
159.008694	6156.519805	25.280730
159.064507	6143.950249	25.285747
159.185801	6154.800241	25.290765
159.214736	6159.192891	25.295783
159.332037	6156.319523	25.300800
159.277585	6160.911400	25.305818
159.410526	6166.714550	25.310835
159.629317	6186.924866	25.315853
159.665496	6188.792875	25.320871
160.005722	6191.503244	25.325888
159.965655	6185.144145	25.330906
160.262670	6215.212133	25.335923
160.737546	6218.516456	25.340941
160.606249	6217.381552	25.345959
160.201554	6231.479426	25.350976
160.490914	6243.485675	25.355994
160.628287	6246.880026	25.361011
160.785191	6258.638070	25.366029
160.844145	6286.918985	25.371047
161.030356	6289.356760	25.376064
161.305907	6316.227398	25.381082
161.584539	6328.222886	25.386099
161.682924	6310.476367	25.391117
161.876008	6340.616500	25.396135
161.938869	6342.725418	25.401152
162.008960	6351.899983	25.406170
162.002924	6385.357288	25.411187
162.652056	6380.446592	25.416205
162.541985	6411.896924	25.421223
162.849834	6420.932233	25.426240
162.960943	6408.466332	25.431258
162.811487	6434.205307	25.436275
163.247024	6433.493315	25.441293
163.233691	6447.865728	25.446311
163.345504	6473.725000	25.451328
163.427757	6476.114620	25.456346
163.775815	6489.935178	25.461363
164.370541	6501.444270	25.466381
164.301676	6518.941222	25.471399
164.831009	6525.233399	25.476416
164.853042	6546.782741	25.481434
165.181924	6526.349565	25.486451
165.436820	6531.099907	25.491469
165.451332	6542.036717	25.496487
165.641006	6532.537989	25.501504
165.617037	6562.546679	25.506522
166.115574	6557.296205	25.511539
166.292267	6568.582656	25.516557
165.833449	6594.014702	25.521575
166.338782	6581.496912	25.526592
166.846785	6604.329181	25.531610
167.066438	6588.483004	25.536627
167.264041	6586.270776	25.541645
167.336986	6613.771534	25.546663
167.369403	6615.600841	25.551680
167.380050	6612.776907	25.556698
167.651299	6623.535509	25.561715
167.855925	6625.355656	25.566733
167.911362	6634.091024	25.571751
168.365547	6648.365108	25.576768
168.453671	6647.126192	25.581786
168.081936	6639.484939	25.586803
168.642386	6657.179672	25.591821
168.412793	6676.106280	25.596839
168.346869	6668.570800	25.601856
168.632743	6712.833051	25.606874
168.870271	6705.471062	25.611891
169.404969	6734.277792	25.616909
169.064782	6761.445448	25.621927
169.670193	6758.548018	25.626944
169.976289	6760.690827	25.631962
170.132633	6761.987799	25.636979
170.486779	6768.519679	25.641997
170.454989	6778.162566	25.647015
170.862554	6804.551935	25.652032
171.027490	6803.996467	25.657050
170.756944	6815.592852	25.662067
171.308068	6810.110349	25.667085
171.195071	6826.529758	25.672103
171.576286	6835.910712	25.677120
171.733577	6825.407184	25.682138
171.664739	6849.238392	25.687156
171.980086	6830.194641	25.692173
171.970829	6851.149101	25.697191
171.945200	6881.121268	25.702208
172.392598	6886.238390	25.707226
172.673566	6882.125087	25.712244
172.576973	6900.162156	25.717261
173.337800	6908.531877	25.722279
173.423063	6912.749267	25.727296
173.487371	6905.495345	25.732314
173.627597	6924.838375	25.737332
174.098508	6910.285184	25.742349
173.779585	6934.087756	25.747367
173.957764	6950.791905	25.752384
174.117110	6945.792258	25.757402
174.101870	6946.625798	25.762420
174.414773	6967.175557	25.767437
174.302854	6971.591315	25.772455
174.665699	6960.969862	25.777472
175.083912	6987.349906	25.782490
175.155659	7018.267797	25.787508
175.706946	7001.237901	25.792525
175.347376	7014.054823	25.797543
175.588385	7033.649877	25.802560
175.961453	7025.564850	25.807578
175.893851	7029.339353	25.812596
176.438207	7053.435744	25.817613
176.517504	7059.517419	25.822631
176.751578	7055.652406	25.827648
176.933473	7069.760419	25.832666
176.491783	7090.570478	25.837684
176.870980	7097.604335	25.842701
177.041522	7107.702253	25.847719
177.470522	7121.895092	25.852736
177.676951	7124.031583	25.857754
177.977451	7148.232990	25.862772
178.459267	7148.436297	25.867789
178.562648	7169.065830	25.872807
178.555964	7150.875417	25.877824
178.567896	7161.894987	25.882842
178.711744	7178.151046	25.887860
178.985551	7179.798386	25.892877
179.144952	7183.654727	25.897895
179.572123	7193.450415	25.902912
179.726179	7206.042840	25.907930
179.433423	7227.663244	25.912948
179.738062	7215.295454	25.917965
179.901646	7238.970721	25.922983
180.216782	7244.510272	25.928000
180.482707	7242.952910	25.933018
180.570525	7258.616642	25.938036
180.704507	7282.804032	25.943053
180.979742	7292.980849	25.948071
180.881596	7294.863704	25.953088
181.516760	7313.300499	25.958106
181.557293	7304.750901	25.963124
181.653815	7327.642767	25.968141
181.749747	7320.644888	25.973159
181.995806	7322.236976	25.978176
182.012330	7348.629267	25.983194
182.181972	7354.039330	25.988212
182.489121	7375.036317	25.993229
182.742274	7377.206074	25.998247
182.879771	7399.899905	26.003264
183.113614	7402.776123	26.008282
183.387547	7420.673420	26.013300
183.297651	7433.659151	26.018317
183.727771	7421.778426	26.023335
184.003082	7450.189103	26.028352
184.252621	7448.426519	26.033370
184.053307	7453.503024	26.038388
184.745549	7485.164334	26.043405
184.544256	7491.005876	26.048423
184.533535	7501.260791	26.053440
184.866156	7502.173126	26.058458
185.241274	7524.986958	26.063476
185.457413	7512.425649	26.068493
185.578368	7541.844843	26.073511
185.702992	7545.926744	26.078528
185.919442	7558.734378	26.083546
186.022432	7556.678619	26.088564
186.099917	7564.874548	26.093581
186.311280	7569.918672	26.098599
186.351083	7580.182617	26.103616
187.048593	7586.171011	26.108634
187.041505	7607.349388	26.113652
187.019822	7612.680109	26.118669
186.923400	7623.430454	26.123687
187.588898	7641.559420	26.128704
187.744445	7642.493934	26.133722
187.501421	7646.164869	26.138740
187.989798	7671.398438	26.143757
188.241219	7677.799220	26.148775
187.897190	7678.832034	26.153792
188.041375	7684.701618	26.158810
188.563028	7719.173201	26.163828
188.945449	7731.414083	26.168845
189.077810	7739.567171	26.173863
189.168882	7773.276791	26.178880
189.443579	7766.264928	26.183898
189.705219	7791.160492	26.188916
189.664051	7785.978315	26.193933
190.193245	7802.333584	26.198951
189.998453	7799.273251	26.203968
190.282463	7834.297837	26.208986
190.426838	7827.601238	26.214004
190.914969	7844.608343	26.219021
191.247517	7858.730369	26.224039
190.792899	7861.109285	26.229056
191.425094	7882.669112	26.234074
191.439877	7890.169132	26.239092
191.571612	7919.690421	26.244109
192.342084	7934.155987	26.249127
192.500770	7926.992321	26.254144
192.866059	7932.504929	26.259162
192.953434	7955.709519	26.264180
193.207997	7938.220061	26.269197
193.590344	7954.416252	26.274215
193.408725	7951.009549	26.279232
193.938888	7966.873393	26.284250
194.080494	7973.467280	26.289268
194.254947	7974.796409	26.294285
194.102885	7993.278236	26.299303
194.353266	8001.908124	26.304320
194.382704	8010.491828	26.309338
194.695890	8015.041222	26.314356
194.531973	8011.130691	26.319373
194.840729	8041.055330	26.324391
194.882730	8050.862431	26.329408
195.227877	8067.760306	26.334426
195.504512	8081.434195	26.339444
195.404603	8105.276377	26.344461
195.799860	8118.349474	26.349479
195.833595	8141.319841	26.354496
196.203079	8150.697224	26.359514
196.189965	8150.858679	26.364532
196.541247	8177.766460	26.369549
197.013740	8188.985513	26.374567
196.684398	8210.647173	26.379584
197.079677	8210.292234	26.384602
197.223284	8233.638368	26.389620
197.619510	8254.343011	26.394637
198.388817	8266.469980	26.399655
198.385870	8294.135069	26.404672
198.641750	8280.405696	26.409690
198.528001	8280.709792	26.414708
198.996030	8294.237257	26.419725
199.482349	8289.623022	26.424743
199.293049	8303.108678	26.429760
199.590995	8294.872783	26.434778
199.572748	8309.191790	26.439796
199.623473	8314.076828	26.444813
200.211263	8328.635952	26.449831
200.118951	8324.532367	26.454848
200.388485	8352.807015	26.459866
200.533694	8369.424005	26.464884
200.802107	8357.605527	26.469901
200.818451	8385.233723	26.474919
200.963494	8384.237293	26.479936
201.172537	8392.507213	26.484954
201.722147	8412.919732	26.489972
201.454157	8431.416500	26.494989
201.869459	8425.944468	26.500007
201.925964	8444.087566	26.505024
202.037503	8459.560341	26.510042
202.409913	8465.003440	26.515060
202.372138	8494.871999	26.520077
202.566259	8506.133337	26.525095
202.512006	8529.704773	26.530112
203.063033	8542.554801	26.535130
203.111773	8554.119001	26.540148
203.234252	8571.838647	26.545165
203.890949	8596.545770	26.550183
204.244618	8587.640514	26.555200
204.640582	8601.429818	26.560218
205.199757	8610.558757	26.565236
205.760312	8594.788524	26.570253
205.517535	8591.024768	26.575271
205.499841	8610.088410	26.580288
205.701819	8616.310299	26.585306
206.071465	8633.771013	26.590324
205.761225	8626.621504	26.595341
206.386196	8640.072930	26.600359
206.620060	8641.373398	26.605376
206.913214	8652.222317	26.610394
206.986148	8658.236354	26.615412
206.736564	8664.784116	26.620429
207.459097	8665.213886	26.625447
207.294366	8680.382046	26.630464
207.590540	8697.505277	26.635482
207.910285	8705.713753	26.640500
207.870330	8731.228493	26.645517
208.071840	8731.782946	26.650535
208.422683	8747.272383	26.655552
208.401197	8762.509889	26.660570
208.473182	8782.405591	26.665588
208.440402	8785.244209	26.670605
208.522512	8791.394611	26.675623
208.711121	8817.240322	26.680640
209.386423	8815.546647	26.685658
209.381119	8834.979474	26.690676
209.595036	8873.529089	26.695693
210.173969	8869.975255	26.700711
210.362074	8894.672847	26.705728
210.555918	8891.214141	26.710746
211.324041	8907.778394	26.715764
211.637210	8931.385809	26.720781
211.941087	8932.862185	26.725799
211.654706	8942.188523	26.730816
212.265948	8927.500424	26.735834
212.209700	8928.407791	26.740852
212.493859	8937.106647	26.745869
213.017511	8946.498413	26.750887
212.952645	8959.186697	26.755904
213.244008	8950.750709	26.760922
213.169672	8943.807812	26.765940
212.980665	8992.879810	26.770957
213.996656	8983.904279	26.775975
213.539131	8986.924165	26.780992
213.594032	8989.797952	26.786010
213.865426	8998.698216	26.791028
213.611052	9007.223817	26.796045
213.768181	9038.980612	26.801063
214.046393	9050.951474	26.806080
214.187960	9085.707808	26.811098
214.574023	9107.995999	26.816116
214.278868	9125.504880	26.821133
214.854846	9148.468242	26.826151
215.028257	9163.214750	26.831168
215.270632	9194.071698	26.836186
215.874939	9194.698236	26.841204
215.965389	9226.185242	26.846221
216.218337	9244.536238	26.851239
216.619270	9257.540822	26.856256
216.981757	9273.762131	26.861274
217.250168	9284.479315	26.866292
217.029567	9288.249312	26.871309
217.902587	9308.008597	26.876327
218.124439	9306.954525	26.881344
218.403626	9302.783004	26.886362
218.538904	9323.624321	26.891380
218.723631	9327.291913	26.896397
218.957614	9341.839548	26.901415
219.178557	9335.464404	26.906432
219.601699	9367.157426	26.911450
219.596397	9374.624451	26.916468
219.341070	9379.793526	26.921485
219.974634	9405.988063	26.926503
220.217605	9419.682067	26.931520
220.182004	9413.710803	26.936538
220.689451	9443.862830	26.941556
220.570422	9451.985090	26.946573
220.777067	9460.895527	26.951591
220.702645	9472.105046	26.956608
220.983711	9499.074728	26.961626
221.355449	9505.440624	26.966644
221.436602	9521.985133	26.971661
221.981008	9551.186092	26.976679
222.226840	9574.588992	26.981696
222.606008	9576.562593	26.986714
222.771453	9592.541900	26.991732
222.768111	9600.708133	26.996749
223.223004	9617.332765	27.001767
223.127643	9633.942787	27.006784
223.538381	9659.238840	27.011802
223.865710	9647.070195	27.016820
224.010084	9661.635293	27.021837
224.645019	9678.439755	27.026855
224.855187	9690.954795	27.031872
224.877386	9703.337859	27.036890
225.630883	9711.055376	27.041908
225.801408	9729.074776	27.046925
225.785374	9737.964662	27.051943
226.001163	9738.136359	27.056960
226.153470	9768.284671	27.061978
226.184252	9766.068062	27.066996
226.322700	9764.885965	27.072013
226.377101	9779.210838	27.077031
226.720367	9802.890196	27.082048
226.627142	9822.163900	27.087066
226.854485	9806.426258	27.092084
227.256589	9844.659651	27.097101
227.341268	9869.746838	27.102119
227.586462	9879.293080	27.107136
227.794679	9907.212804	27.112154
228.320072	9945.630072	27.117172
228.422138	9937.513912	27.122189
228.447496	9961.224765	27.127207
228.931344	9960.007639	27.132224
228.803467	9992.854721	27.137242
229.474499	9979.725587	27.142260
229.429275	9999.498041	27.147277
229.526688	10026.352459	27.152295
229.826482	10033.585859	27.157312
230.242668	10056.077564	27.162330
230.645130	10053.735704	27.167348
230.811904	10095.635779	27.172365
230.874237	10093.319392	27.177383
230.970872	10116.567367	27.182400
231.395418	10128.152541	27.187418
231.643567	10151.099061	27.192436
231.809517	10167.286020	27.197453
232.632385	10162.161160	27.202471
233.163013	10193.627768	27.207488
233.021049	10175.859513	27.212506
233.220349	10176.937399	27.217524
233.435619	10198.969422	27.222541
233.772252	10204.323730	27.227559
234.189443	10221.319131	27.232576
233.953294	10224.680752	27.237594
234.214368	10237.942403	27.242612
233.994159	10267.249749	27.247629
234.040039	10260.506960	27.252647
234.691046	10286.206202	27.257664
234.970547	10307.287277	27.262682
235.471565	10312.631003	27.267700
235.551055	10349.097805	27.272717
235.514354	10355.954514	27.277735
236.060377	10372.246661	27.282752
236.079535	10390.517885	27.287770
236.442454	10395.779695	27.292788
236.544969	10408.847136	27.297805
236.501969	10432.588103	27.302823
236.946517	10427.450050	27.307840
236.965747	10482.626716	27.312858
237.431679	10483.063503	27.317876
237.817152	10502.820559	27.322893
237.732385	10543.733868	27.327911
238.337295	10536.070737	27.332928
238.290908	10574.992811	27.337946
238.803483	10575.287199	27.342964
239.188823	10593.335102	27.347981
239.701235	10612.067802	27.352999
239.928398	10609.552389	27.358016
239.954514	10647.596200	27.363034
240.045021	10644.239261	27.368052
240.376765	10667.711498	27.373069
240.481656	10687.395412	27.378087
240.932252	10682.045177	27.383104
240.879922	10707.635241	27.388122
241.278206	10721.076276	27.393140
241.525874	10725.150486	27.398157
241.822304	10759.532007	27.403175
242.091317	10762.858325	27.408192
242.151426	10787.212943	27.413210
242.168710	10793.964821	27.418228
242.573864	10818.860343	27.423245
243.117488	10843.131220	27.428263
243.106040	10839.008896	27.433280
243.104805	10848.290021	27.438298
243.732299	10879.833358	27.443316
243.835798	10913.916252	27.448333
243.938102	10911.037810	27.453351
244.309472	10920.434648	27.458368
244.498314	10942.323978	27.463386
244.623824	10936.675265	27.468404
244.861788	10961.523802	27.473421
244.996069	10990.612424	27.478439
245.599588	11014.616086	27.483456
245.403909	11017.583630	27.488474
245.969109	11041.888269	27.493492
246.235478	11052.422662	27.498509
246.637673	11073.201692	27.503527
246.994715	11066.500890	27.508544
246.899241	11099.219650	27.513562
247.181694	11103.735633	27.518580
247.857695	11109.197235	27.523597
247.689207	11123.139504	27.528615
248.340023	11135.011782	27.533632
248.529490	11159.632325	27.538650
248.663318	11172.977222	27.543668
248.842847	11184.572931	27.548685
249.150487	11213.320592	27.553703
249.553632	11212.565714	27.558720
249.704070	11230.105684	27.563738
250.105342	11241.446598	27.568756
250.036891	11257.472525	27.573773
250.232690	11269.150680	27.578791
250.659360	11286.689186	27.583808
250.917776	11307.849117	27.588826
251.224000	11317.684690	27.593844
251.428004	11328.103534	27.598861
251.273307	11363.109938	27.603879
251.696999	11364.101993	27.608896
251.841221	11402.073734	27.613914
251.789311	11405.641479	27.618932
252.303870	11428.203160	27.623949
252.589517	11460.763587	27.628967
252.752268	11459.810521	27.633984
252.685233	11482.625130	27.639002
253.258727	11515.623355	27.644020
253.346440	11536.617222	27.649037
254.081693	11565.313771	27.654055
254.141666	11589.722414	27.659072
254.481413	11607.814449	27.664090
255.173708	11629.642809	27.669108
255.549726	11642.567605	27.674125
255.729334	11655.810813	27.679143
255.833041	11648.424539	27.684160
255.898079	11658.138684	27.689178
256.181068	11693.460278	27.694196
256.727198	11702.037021	27.699213
257.163364	11718.297497	27.704231
257.735326	11723.483462	27.709248
257.248233	11739.046522	27.714266
257.923674	11746.536890	27.719284
258.057158	11743.022161	27.724301
258.001645	11763.694956	27.729319
258.877159	11767.562507	27.734336
259.137915	11778.654460	27.739354
258.997915	11775.904912	27.744372
259.230325	11802.659666	27.749389
259.470271	11834.112161	27.754407
259.950920	11836.762509	27.759424
259.785408	11848.570895	27.764442
260.220647	11858.590303	27.769460
260.561645	11890.444510	27.774477
260.370552	11910.852365	27.779495
260.956162	11897.928784	27.784512
261.514649	11925.626380	27.789530
261.519090	11942.265640	27.794548
261.937687	11938.091674	27.799565
261.717586	11970.534245	27.804583
262.275542	11972.870132	27.809600
262.399682	11998.518182	27.814618
262.554356	12013.168807	27.819636
262.697387	12033.653171	27.824653
262.481570	12049.071664	27.829671
262.795902	12049.049864	27.834688
263.022961	12087.590127	27.839706
263.053087	12106.802880	27.844724
263.458935	12143.334082	27.849741
263.474112	12167.324823	27.854759
264.118885	12191.639338	27.859776
264.442373	12225.302673	27.864794
264.511182	12250.373378	27.869812
265.247448	12260.538670	27.874829
265.676784	12278.246409	27.879847
265.730989	12323.690703	27.884864
265.957307	12326.498171	27.889882
266.203395	12365.896210	27.894900
266.607943	12388.612135	27.899917
266.857581	12400.612303	27.904935
267.041175	12437.675622	27.909952
267.642616	12436.227769	27.914970
267.696317	12465.681373	27.919988
268.052865	12480.543285	27.925005
267.918597	12505.641639	27.930023
268.277862	12516.386170	27.935040
268.971716	12535.304645	27.940058
269.222820	12567.108876	27.945076
269.917462	12579.891980	27.950093
269.715418	12606.025814	27.955111
270.327135	12611.683692	27.960128
270.277446	12626.241020	27.965146
270.938433	12637.359615	27.970164
271.501321	12657.484712	27.975181
271.591938	12660.688072	27.980199
271.794343	12688.411158	27.985216
271.801079	12700.775465	27.990234
272.026741	12735.231223	27.995252
272.316754	12731.390267	28.000269
272.643658	12752.083871	28.005287
272.945377	12785.404560	28.010304
273.134664	12799.332500	28.015322
273.087585	12826.690538	28.020340
273.939713	12828.610050	28.025357
273.702487	12842.772358	28.030375
273.890361	12884.855087	28.035392
274.147807	12896.213064	28.040410
274.446417	12925.630986	28.045428
275.025669	12940.928426	28.050445
275.187748	12967.997687	28.055463
275.320540	12975.925717	28.060480
275.914544	12999.675536	28.065498
276.101863	13032.230979	28.070516
276.592663	13028.032202	28.075533
276.570724	13075.865663	28.080551
276.554482	13087.777921	28.085568
277.021765	13117.297528	28.090586
277.668719	13125.782753	28.095604
278.227042	13118.707512	28.100621
278.242777	13152.548112	28.105639
278.804348	13151.885150	28.110656
279.294554	13173.334619	28.115674
279.364884	13196.910483	28.120692
279.553421	13203.209660	28.125709
279.848900	13206.906334	28.130727
280.149019	13234.214004	28.135744
280.257766	13230.543112	28.140762
280.158580	13256.575133	28.145780
280.433432	13281.311668	28.150797
281.123843	13283.182326	28.155815
281.598913	13302.998160	28.160832
281.847042	13302.157723	28.165850
281.773105	13321.690069	28.170868
282.451086	13328.357491	28.175885
282.444978	13349.492130	28.180903
282.777979	13359.863411	28.185920
282.612133	13366.719897	28.190938
282.470567	13400.624035	28.195956
283.110035	13411.227546	28.200973
283.221272	13451.666038	28.205991
283.950861	13492.183670	28.211008
284.015977	13488.233157	28.216026
283.817492	13504.960344	28.221044
284.088513	13532.319809	28.226061
284.506123	13556.060991	28.231079
284.883418	13587.741609	28.236096
285.488613	13603.527796	28.241114
286.047356	13623.464921	28.246132
286.524262	13628.392263	28.251149
286.759334	13663.625264	28.256167
286.945652	13672.022227	28.261184
287.555610	13688.901236	28.266202
287.420460	13704.940621	28.271220
287.873671	13723.909714	28.276237
287.915330	13744.809293	28.281255
288.461986	13739.662782	28.286272
288.562870	13769.140126	28.291290
288.542181	13786.033615	28.296308
289.020249	13817.301748	28.301325
289.102857	13820.047347	28.306343
289.581593	13857.167594	28.311360
289.906270	13885.439004	28.316378
289.933852	13898.301860	28.321396
290.457642	13910.734514	28.326413
291.020782	13943.028803	28.331431
291.267239	13961.022305	28.336448
291.336229	13991.105669	28.341466
291.548039	14011.002112	28.346484
291.704481	14024.135287	28.351501
292.127414	14042.873401	28.356519
292.516476	14077.501998	28.361536
293.006851	14090.140429	28.366554
293.007207	14124.784501	28.371572
293.132987	14144.635444	28.376589
293.545093	14175.795414	28.381607
293.653297	14212.861092	28.386624
294.232522	14214.257817	28.391642
294.003626	14238.100514	28.396660
294.580540	14276.677245	28.401677
294.790859	14314.161189	28.406695
294.646780	14340.049524	28.411712
295.488308	14372.724131	28.416730
295.502948	14397.217005	28.421748
296.300035	14432.113010	28.426765
297.113607	14453.530458	28.431783
297.293608	14467.366041	28.436800
297.463613	14482.941355	28.441818
297.785903	14519.644606	28.446836
298.213695	14527.055871	28.451853
298.395124	14551.338633	28.456871
298.585806	14559.050665	28.461888
298.761254	14571.487805	28.466906
298.960742	14591.394877	28.471924
299.299637	14613.956186	28.476941
299.650015	14646.093211	28.481959
299.442132	14656.442810	28.486976
299.998815	14682.608285	28.491994
300.386903	14707.569392	28.497012
300.924575	14741.954250	28.502029
300.804075	14749.826514	28.507047
301.060108	14760.835427	28.512064
301.673793	14790.025056	28.517082
301.693921	14826.476371	28.522100
302.012554	14842.396211	28.527117
302.313294	14876.809470	28.532135
302.497042	14900.301320	28.537152
303.378376	14904.807684	28.542170
303.637823	14934.112826	28.547188
303.852241	14959.500119	28.552205
304.345899	14977.910896	28.557223
304.512426	15004.194928	28.562240
304.993423	15015.934270	28.567258
305.136454	15042.384554	28.572276
305.380221	15072.467839	28.577293
306.219294	15074.469377	28.582311
306.356424	15103.637452	28.587328
306.594576	15105.519235	28.592346
306.848660	15130.827754	28.597364
307.146998	15137.609872	28.602381
307.815425	15135.129595	28.607399
307.421496	15171.327048	28.612416
307.966756	15187.706173	28.617434
308.282216	15209.091885	28.622452
308.204758	15238.093947	28.627469
308.770106	15259.157941	28.632487
308.954702	15296.219777	28.637504
309.218641	15309.317325	28.642522
309.725798	15323.421061	28.647540
309.831424	15357.708415	28.652557
310.287826	15381.995844	28.657575
310.547832	15403.769178	28.662592
310.874889	15438.875807	28.667610
311.029467	15459.331884	28.672628
311.063241	15500.809445	28.677645
311.833407	15517.871917	28.682663
311.587278	15555.021262	28.687680
312.307152	15560.176958	28.692698
312.385620	15608.798701	28.697716
312.879953	15655.118865	28.702733
313.402651	15656.068059	28.707751
313.716190	15691.076611	28.712768
313.900537	15709.690607	28.717786
314.469664	15732.721294	28.722804
314.784870	15752.435749	28.727821
315.470673	15785.449389	28.732839
315.469036	15816.094638	28.737856
315.876913	15829.646321	28.742874
316.114744	15855.341597	28.747892
316.526159	15862.259776	28.752909
317.142883	15876.558639	28.757927
316.596156	15913.414917	28.762944
317.271816	15915.517632	28.767962
317.565315	15967.493110	28.772980
317.507502	15989.072318	28.777997
317.986622	16021.592654	28.783015
318.198308	16067.272014	28.788032
318.462542	16078.508976	28.793050
319.087954	16105.993893	28.798068
318.945767	16147.664491	28.803085
319.696076	16152.088850	28.808103
319.709166	16186.599683	28.813120
320.214477	16233.720251	28.818138
320.525102	16257.520894	28.823156
320.580953	16278.484426	28.828173
321.181446	16294.253538	28.833191
321.529586	16312.297464	28.838208
321.873419	16329.684953	28.843226
321.948754	16354.809004	28.848244
322.372779	16381.911610	28.853261
322.683284	16422.182747	28.858279
322.798172	16436.546101	28.863296
323.057837	16470.679543	28.868314
323.455723	16497.324905	28.873332
323.884175	16535.126219	28.878349
324.285016	16562.245562	28.883367
324.198075	16592.357925	28.888384
324.740178	16606.264737	28.893402
325.199537	16660.936720	28.898420
325.473836	16679.448708	28.903437
326.305219	16699.963156	28.908455
326.725235	16738.106746	28.913472
327.405954	16746.496906	28.918490
327.779207	16754.767662	28.923508
328.225702	16768.602153	28.928525
328.485918	16796.487408	28.933543
328.632199	16831.776624	28.938560
329.199972	16814.314038	28.943578
329.625947	16840.408452	28.948596
329.568224	16858.015717	28.953613
329.963219	16864.480000	28.958631
330.115045	16891.689888	28.963648
330.450465	16924.087622	28.968666
330.860115	16929.104318	28.973684
330.432215	16971.353752	28.978701
330.944334	16999.273385	28.983719
331.374848	17018.656698	28.988736
331.583807	17055.247280	28.993754
331.894665	17088.785703	28.998772
331.970806	17106.631162	29.003789
332.648971	17152.449252	29.008807
332.864724	17188.646580	29.013824
333.285744	17194.165808	29.018842
333.786653	17259.518384	29.023860
333.781063	17273.804665	29.028877
334.350046	17302.268608	29.033895
334.586682	17336.363533	29.038912
335.056850	17352.992079	29.043930
335.280996	17400.264906	29.048948
335.535315	17436.464290	29.053965
336.096080	17450.570476	29.058983
336.135710	17495.960737	29.064000
336.127651	17504.250740	29.069018
336.822586	17552.623541	29.074036
337.383183	17571.461191	29.079053
337.922248	17618.294908	29.084071
338.125802	17628.605204	29.089088
338.731787	17647.328271	29.094106
339.214772	17678.719652	29.099124
339.793563	17706.243339	29.104141
340.264087	17710.061861	29.109159
340.384007	17755.936041	29.114176
340.474684	17751.125250	29.119194
340.862604	17795.011958	29.124212
341.289810	17807.473021	29.129229
341.928385	17834.788461	29.134247
341.826703	17876.368501	29.139264
342.011770	17880.691289	29.144282
342.531168	17908.494640	29.149300
342.391435	17925.186703	29.154317
343.213618	17951.789555	29.159335
343.226492	17985.358553	29.164352
343.911264	17999.845057	29.169370
344.526288	17996.602477	29.174388
344.422836	18021.544270	29.179405
345.119195	18045.783417	29.184423
344.945334	18062.933600	29.189440
345.323197	18106.587962	29.194458
345.942513	18121.756812	29.199476
346.002951	18147.920004	29.204493
346.327065	18165.568036	29.209511
346.369146	18200.067285	29.214528
346.753352	18226.293745	29.219546
347.265575	18268.345487	29.224564
347.373588	18284.691216	29.229581
347.849257	18320.982072	29.234599
348.150142	18336.312481	29.239616
348.404416	18379.318127	29.244634
348.956926	18402.326959	29.249652
349.205448	18432.018457	29.254669
350.260945	18446.039042	29.259687
350.235258	18492.372770	29.264704
350.356968	18507.129274	29.269722
351.116898	18533.596774	29.274740
351.231184	18559.761181	29.279757
351.844385	18589.339127	29.284775
352.181480	18629.488353	29.289792
352.590884	18647.734365	29.294810
352.783481	18677.867414	29.299828
352.905973	18692.080177	29.304845
353.432490	18716.814920	29.309863
353.556393	18756.511063	29.314880
353.462275	18783.908149	29.319898
354.295013	18827.334809	29.324916
354.318538	18856.265118	29.329933
354.868969	18904.008504	29.334951
355.016676	18934.623872	29.339968
355.156198	18971.414605	29.344986
356.080977	19001.854436	29.350004
356.494300	19052.336692	29.355021
356.681201	19078.015487	29.360039
357.014638	19103.766263	29.365056
357.271623	19133.906846	29.370074
358.224147	19168.629696	29.375092
358.279395	19201.546344	29.380109
358.908580	19241.116043	29.385127
359.106350	19251.927976	29.390144
359.387776	19279.690997	29.395162
359.929697	19317.363335	29.400180
359.760288	19344.190581	29.405197
360.121039	19384.290449	29.410215
360.437708	19422.205149	29.415232
360.831822	19466.363247	29.420250
361.225563	19499.752609	29.425268
361.537554	19554.179569	29.430285
362.048610	19569.012987	29.435303
362.353611	19627.965189	29.440320
362.641941	19654.217643	29.445338
363.421482	19698.802905	29.450356
363.620224	19731.622817	29.455373
364.028553	19746.911569	29.460391
364.502936	19791.774478	29.465408
364.657805	19796.862524	29.470426
365.444298	19841.150683	29.475444
365.793865	19858.296644	29.480461
366.173886	19902.273810	29.485479
366.218887	19934.594619	29.490496
366.592256	19955.280243	29.495514
367.262266	19999.788259	29.500532
367.549811	20023.571377	29.505549
367.714543	20059.707778	29.510567
368.379026	20075.553511	29.515584
368.501990	20114.936231	29.520602
369.014460	20131.653606	29.525620
368.857180	20154.939777	29.530637
369.451477	20179.093316	29.535655
369.672911	20234.867878	29.540672
369.833862	20264.759988	29.545690
370.460939	20285.878584	29.550708
370.980928	20322.987783	29.555725
371.537475	20356.285772	29.560743
371.673379	20373.831696	29.565760
372.159006	20402.492900	29.570778
372.859633	20418.213190	29.575796
373.312818	20439.026527	29.580813
373.709908	20465.314318	29.585831
374.306068	20500.403078	29.590848
374.386580	20514.375279	29.595866
374.919280	20538.473314	29.600884
375.362354	20573.816088	29.605901
375.274256	20583.293661	29.610919
375.973941	20632.239049	29.615936
376.004202	20649.214737	29.620954
376.246470	20682.060866	29.625972
376.495554	20732.365721	29.630989
376.857253	20752.245594	29.636007
377.711874	20786.656986	29.641024
377.444523	20822.130263	29.646042
377.770602	20862.130664	29.651060
377.919855	20886.765463	29.656077
378.028775	20938.818654	29.661095
378.690388	20970.733794	29.666112
379.188619	21031.429340	29.671130
379.986264	21050.146688	29.676148
380.193233	21111.574797	29.681165
380.506121	21159.912515	29.686183
381.057764	21188.077061	29.691200
381.147673	21241.950359	29.696218
381.935940	21257.485141	29.701236
382.199709	21310.626859	29.706253
382.995775	21340.222081	29.711271
383.312101	21364.516278	29.716288
383.582758	21408.502886	29.721306
384.246410	21423.629622	29.726324
384.460525	21469.449659	29.731341
384.836278	21511.339862	29.736359
385.512467	21526.324318	29.741376
385.602648	21579.951161	29.746394
386.147467	21597.720889	29.751412
386.402006	21633.877402	29.756429
386.662363	21663.774520	29.761447
386.959830	21684.396015	29.766464
387.121529	21742.249071	29.771482
387.792858	21750.238211	29.776500
387.883936	21807.619187	29.781517
388.338662	21842.133509	29.786535
388.640836	21873.832304	29.791552
389.247829	21912.557595	29.796570
389.775071	21962.886421	29.801588
390.273027	21982.213981	29.806605
391.103819	22012.755282	29.811623
391.100662	22045.554781	29.816640
391.655551	22074.765501	29.821658
392.207802	22102.706056	29.826676
392.244299	22130.999863	29.831693
392.537516	22159.513007	29.836711
393.273410	22185.014473	29.841728
393.317341	22216.898466	29.846746
393.733348	22248.296972	29.851764
393.966836	22281.393635	29.856781
394.282125	22314.798459	29.861799
395.202306	22348.235850	29.866816
395.067977	22376.001781	29.871834
395.313207	22410.794671	29.876852
395.782856	22445.567901	29.881869
396.210466	22474.407792	29.886887
396.498181	22516.699731	29.891904
396.816819	22559.732369	29.896922
397.623108	22591.196321	29.901940
397.933918	22613.033846	29.906957
398.302693	22641.910547	29.911975
399.220514	22685.985943	29.916992
399.443509	22717.426674	29.922010
399.856674	22747.885387	29.927028
400.028517	22771.705731	29.932045
400.075224	22816.316363	29.937063
400.608633	22835.317436	29.942080
400.578665	22890.056149	29.947098
401.288024	22932.820245	29.952116
401.714997	22959.135411	29.957133
401.996814	23024.914250	29.962151
402.632070	23043.731617	29.967168
402.899490	23104.654126	29.972186
403.226222	23133.526006	29.977204
403.644552	23180.770604	29.982221
403.587793	23212.856006	29.987239
404.281320	23249.284031	29.992256
404.475450	23308.340077	29.997274
404.674967	23353.005718	30.002292
405.144856	23410.457301	30.007309
405.907178	23450.787557	30.012327
406.657734	23510.387770	30.017344
407.032208	23547.271187	30.022362
407.445633	23573.534372	30.027380
408.199189	23638.182914	30.032397
408.332516	23662.239495	30.037415
409.096979	23696.473128	30.042432
409.524757	23741.885684	30.047450
409.958869	23772.431086	30.052468
410.501177	23809.463937	30.057485
410.530964	23850.967794	30.062503
410.769338	23891.237456	30.067520
411.626715	23923.665116	30.072538
412.742692	23950.806130	30.077556
413.086656	23979.794866	30.082573
413.002434	23999.342333	30.087591
413.726296	24038.266080	30.092608
413.854275	24058.612621	30.097626
414.261919	24090.466884	30.102644
414.605990	24132.874983	30.107661
415.019392	24164.633834	30.112679
415.247171	24207.230036	30.117696
415.305446	24253.649448	30.122714
415.837379	24279.756985	30.127732
416.150712	24335.520563	30.132749
416.005187	24370.482966	30.137767
416.598282	24412.696112	30.142784
417.035293	24457.568259	30.147802
417.381027	24512.319548	30.152820
418.196876	24552.779201	30.157837
418.058634	24591.078776	30.162855
419.237027	24643.991654	30.167872
419.427434	24706.965077	30.172890
419.738423	24730.192850	30.177908
420.507384	24781.016816	30.182925
420.550590	24818.965276	30.187943
421.392159	24844.439141	30.192960
421.684319	24891.250541	30.197978
421.988612	24909.616960	30.202996
422.596519	24963.284163	30.208013
422.729647	24983.509556	30.213031
423.264287	25027.596051	30.218048
423.199726	25085.233075	30.223066
423.806177	25115.238412	30.228084
424.398416	25172.371462	30.233101
424.487306	25216.497395	30.238119
425.165290	25240.355873	30.243136
425.728844	25288.566296	30.248154
426.321985	25311.918551	30.253172
426.923624	25362.650492	30.258189
427.075981	25401.665484	30.263207
427.560828	25430.810037	30.268224
427.786613	25494.825962	30.273242
428.331151	25527.615866	30.278260
428.626361	25588.676768	30.283277
428.969547	25621.134292	30.288295
429.717744	25661.316062	30.293312
430.072333	25707.009315	30.298330
430.319254	25736.931654	30.303348
431.400114	25794.634162	30.308365
431.488118	25823.020259	30.313383
432.226676	25854.022143	30.318400
432.504512	25905.159255	30.323418
432.795104	25942.558460	30.328436
433.289769	25978.897505	30.333453
433.430052	26022.480909	30.338471
434.243357	26080.816756	30.343488
434.789228	26112.738718	30.348506
434.976884	26168.891763	30.353524
435.554227	26198.500147	30.358541
435.718197	26248.528057	30.363559
436.473243	26274.548203	30.368576
436.809061	26341.677671	30.373594
437.009298	26378.931918	30.378612
437.604811	26418.721250	30.383629
437.911322	26473.231462	30.388647
438.470780	26492.733811	30.393664
438.854237	26550.790627	30.398682
439.231032	26585.715454	30.403700
439.890207	26641.681781	30.408717
440.254334	26709.382016	30.413735
440.550343	26737.798352	30.418752
441.170857	26772.635993	30.423770
441.607969	26826.567527	30.428788
442.318417	26861.414147	30.433805
442.357829	26907.202107	30.438823
442.765150	26966.018055	30.443840
443.613840	27004.522723	30.448858
443.484646	27045.380978	30.453876
444.264764	27092.258175	30.458893
444.673158	27142.587374	30.463911
445.390351	27177.140210	30.468928
445.503279	27220.333796	30.473946
445.756580	27271.140006	30.478964
446.464105	27312.201306	30.483981
447.130534	27352.111990	30.488999
447.475935	27387.026294	30.494016
448.055782	27437.832674	30.499034
448.044414	27476.691796	30.504052
448.781349	27527.365257	30.509069
449.056096	27574.443957	30.514087
449.625611	27618.547172	30.519104
450.243764	27681.459352	30.524122
450.568316	27705.799163	30.529140
451.217939	27738.768360	30.534157
451.633288	27775.233148	30.539175
451.693036	27796.286165	30.544192
452.515886	27842.861883	30.549210
452.744448	27886.757170	30.554228
453.007707	27916.103436	30.559245
453.222265	27979.301009	30.564263
453.383849	28013.168260	30.569280
453.904025	28055.047658	30.574298
454.075308	28139.562018	30.579316
454.902084	28188.834788	30.584333
455.082228	28240.435020	30.589351
455.826843	28284.794895	30.594368
456.796697	28332.338056	30.599386
456.793655	28391.655647	30.604404
457.220101	28415.803001	30.609421
457.962822	28465.604578	30.614439
458.329612	28532.374786	30.619456
459.501778	28552.680373	30.624474
459.794188	28614.725607	30.629492
460.143243	28641.112924	30.634509
460.720261	28704.105038	30.639527
460.899134	28744.701958	30.644544
461.466911	28796.936907	30.649562
461.656562	28845.168667	30.654580
462.608126	28883.733117	30.659597
462.976459	28935.720706	30.664615
463.172076	28969.164700	30.669632
463.597089	29023.310165	30.674650
463.924674	29073.292477	30.679668
464.748223	29119.865234	30.684685
465.394126	29153.127958	30.689703
465.454125	29228.452359	30.694720
465.980884	29248.754986	30.699738
466.594606	29329.666118	30.704756
467.029542	29358.245219	30.709773
467.229905	29410.230440	30.714791
467.740198	29464.757496	30.719808
468.625141	29518.998877	30.724826
468.719874	29584.518502	30.729844
469.121533	29608.882967	30.734861
469.521911	29665.069086	30.739879
470.421173	29701.943796	30.744896
471.041326	29751.728332	30.749914
471.350412	29798.927308	30.754932
471.449894	29843.993952	30.759949
472.335013	29888.732208	30.764967
472.881782	29957.203668	30.769984
473.685041	29986.495804	30.775002
473.764602	30052.000777	30.780020
474.390575	30079.085847	30.785037
474.642399	30128.692572	30.790055
474.867188	30184.429902	30.795072
475.292460	30233.759071	30.800090
475.675653	30276.221684	30.805108
476.573043	30331.324736	30.810125
476.643131	30375.873969	30.815143
477.456378	30444.069900	30.820160
478.220645	30476.870834	30.825178
478.038447	30545.436641	30.830196
478.814782	30587.759365	30.835213
479.359444	30646.356993	30.840231
479.544090	30709.399145	30.845248
480.065570	30748.158681	30.850266
480.367568	30810.919986	30.855284
480.976689	30849.996505	30.860301
481.578493	30901.282655	30.865319
481.796133	30956.203443	30.870336
482.537786	30993.419249	30.875354
482.965798	31047.419125	30.880372
483.326425	31099.654234	30.885389
484.152392	31144.156287	30.890407
484.231158	31218.867914	30.895424
484.844807	31256.859394	30.900442
484.772603	31309.601975	30.905460
485.505139	31359.855228	30.910477
485.841023	31407.883835	30.915495
486.347883	31477.295360	30.920512
486.930291	31534.990652	30.925530
487.216198	31581.885982	30.930548
487.561524	31647.573891	30.935565
488.123172	31716.276964	30.940583
488.845792	31771.350357	30.945600
489.328226	31823.775729	30.950618
489.837968	31896.349531	30.955636
490.625234	31932.427242	30.960653
491.107490	32004.466564	30.965671
491.952908	32049.601835	30.970688
492.424861	32103.061403	30.975706
492.504858	32178.474146	30.980724
493.149114	32207.054911	30.985741
493.869358	32266.723715	30.990759
494.202115	32313.127421	30.995776
494.812680	32359.207733	31.000794
495.284947	32423.230744	31.005812
496.148313	32456.706810	31.010829
496.737155	32523.727009	31.015847
496.810997	32566.123260	31.020864
498.075527	32627.968616	31.025882
498.339117	32672.914508	31.030900
498.321514	32741.203036	31.035917
498.926293	32786.326326	31.040935
499.033112	32849.073559	31.045952
499.585451	32906.696316	31.050970
500.125039	32945.927835	31.055988
500.320203	33004.584799	31.061005
501.249731	33060.429442	31.066023
501.661851	33131.876070	31.071040
502.560115	33163.028790	31.076058
502.814387	33220.828014	31.081076
503.553519	33287.744276	31.086093
504.469738	33338.373568	31.091111
504.791459	33389.867885	31.096128
505.299421	33443.644253	31.101146
505.472092	33481.416835	31.106164
505.947166	33532.927256	31.111181
506.564052	33593.952250	31.116199
506.936833	33641.283610	31.121216
507.274760	33699.395563	31.126234
507.451803	33763.948649	31.131252
507.960512	33821.401770	31.136269
508.331201	33889.968214	31.141287
508.667367	33972.167768	31.146304
509.368583	34030.731940	31.151322
509.935701	34085.197789	31.156340
510.706505	34142.375179	31.161357
511.746432	34210.838637	31.166375
511.775297	34275.528503	31.171392
512.398043	34313.326334	31.176410
512.721755	34385.963238	31.181428
513.612179	34438.679258	31.186445
514.132940	34506.989823	31.191463
514.224165	34565.896329	31.196480
515.211854	34594.316978	31.201498
515.970271	34672.061057	31.206516
516.537787	34705.823775	31.211533
516.857262	34752.769354	31.216551
517.411968	34821.927459	31.221568
518.065816	34844.121427	31.226586
518.406385	34902.902675	31.231604
518.485697	34934.635557	31.236621
519.187440	34976.965442	31.241639
519.248486	35037.651804	31.246656
519.830334	35105.815755	31.251674
520.183371	35161.856946	31.256692
520.556397	35217.339665	31.261709
520.922074	35292.589169	31.266727
521.182387	35344.481129	31.271744
522.090423	35431.162027	31.276762
522.786396	35493.127145	31.281780
523.032143	35564.696289	31.286797
523.615171	35619.107434	31.291815
524.156443	35696.831922	31.296832
524.995278	35768.676268	31.301850
525.630812	35829.693277	31.306868
525.910409	35884.666546	31.311885
526.435269	35958.179136	31.316903
526.611733	36030.042437	31.321920
527.317936	36096.040732	31.326938
528.124156	36165.859903	31.331956
528.595864	36229.931519	31.336973
529.410069	36285.426744	31.341991
529.862533	36352.928934	31.347008
530.400735	36420.474018	31.352026
531.142409	36470.954936	31.357044
531.523364	36547.393730	31.362061
532.283730	36610.639597	31.367079
532.775094	36670.843904	31.372096
533.796307	36734.479447	31.377114
534.668373	36779.868570	31.382132
534.734787	36849.859954	31.387149
535.407879	36896.071157	31.392167
535.762008	36943.001014	31.397184
536.420556	37012.055813	31.402202
536.851558	37074.704498	31.407220
536.945715	37123.921483	31.412237
537.703813	37187.128743	31.417255
538.169752	37248.639358	31.422272
538.434696	37325.050147	31.427290
539.078487	37375.401470	31.432308
539.305130	37454.381618	31.437325
540.437266	37519.614241	31.442343
540.843157	37560.067797	31.447360
541.467940	37636.676098	31.452378
542.128336	37694.814121	31.457396
542.840592	37747.752425	31.462413
543.559864	37813.243663	31.467431
543.366737	37890.770795	31.472448
544.172301	37936.296918	31.477466
544.675588	38016.540373	31.482484
545.056883	38079.409067	31.487501
545.927878	38149.856467	31.492519
546.207328	38211.505331	31.497536
546.414276	38269.511824	31.502554
547.427198	38341.050571	31.507572
547.678619	38433.983326	31.512589
547.938247	38502.172436	31.517607
548.315587	38553.145461	31.522624
548.991830	38635.755336	31.527642
549.757634	38700.964396	31.532660
550.245135	38758.317015	31.537677
551.220999	38840.963555	31.542695
551.353612	38897.791371	31.547712
552.321249	38977.088188	31.552730
552.794160	39027.305097	31.557748
552.937840	39086.710177	31.562765
553.704635	39149.648330	31.567783
554.750704	39214.999167	31.572800
554.660445	39277.646944	31.577818
555.708533	39332.595375	31.582836
556.130835	39413.628518	31.587853
556.517088	39445.852079	31.592871
556.898545	39524.029854	31.597888
557.541658	39583.199422	31.602906
558.222028	39650.505929	31.607924
558.611062	39731.119906	31.612941
559.035273	39787.372116	31.617959
559.301896	39866.097418	31.622976
559.887462	39928.225511	31.627994
560.543972	40026.585041	31.633012
560.721951	40098.142415	31.638029
561.742126	40172.423687	31.643047
561.511519	40244.045967	31.648064
562.464189	40315.103800	31.653082
562.969666	40412.906458	31.658100
563.691516	40497.338485	31.663117
564.405933	40564.421820	31.668135
564.582182	40668.343527	31.673152
565.562521	40735.875962	31.678170
566.399674	40818.608101	31.683188
566.889708	40889.151197	31.688205
567.854154	40964.799003	31.693223
568.481356	41048.305460	31.698240
568.936532	41111.241924	31.703258
569.506869	41189.307288	31.708276
569.619427	41259.125057	31.713293
570.652584	41335.410124	31.718311
571.153365	41421.666350	31.723328
571.499281	41496.998717	31.728346
572.484064	41562.500710	31.733364
573.053661	41627.478090	31.738381
573.592808	41703.262338	31.743399
574.475828	41765.328635	31.748416
575.186520	41816.388343	31.753434
576.042577	41888.623571	31.758452
576.460395	41957.516067	31.763469
577.048642	42024.155287	31.768487
577.925081	42090.627199	31.773504
578.581492	42150.566816	31.778522
579.485792	42220.405844	31.783540
579.971645	42266.491253	31.788557
580.364507	42303.182242	31.793575
581.032697	42379.506700	31.798592
581.467946	42446.472608	31.803610
581.506234	42494.851638	31.808628
582.359584	42577.797413	31.813645
582.782605	42654.182448	31.818663
583.313736	42695.318092	31.823680
583.559360	42782.588821	31.828698
584.064654	42842.249460	31.833716
584.477494	42899.371772	31.838733
585.187803	42977.942506	31.843751
585.703192	43069.804135	31.848768
585.721438	43133.842507	31.853786
586.718121	43217.108426	31.858804
587.004857	43304.775752	31.863821
587.774119	43394.295765	31.868839
588.099091	43474.081341	31.873856
588.572063	43569.627011	31.878874
589.589679	43639.111780	31.883892
589.985624	43712.102591	31.888909
590.742066	43780.456677	31.893927
591.320527	43879.597995	31.898944
591.842435	43936.351935	31.903962
592.772012	44016.939715	31.908980
593.192652	44097.618221	31.913997
593.695564	44138.392390	31.919015
594.740106	44216.060826	31.924032
594.867638	44287.213542	31.929050
595.643582	44365.709897	31.934068
596.204276	44431.838331	31.939085
596.582640	44511.666923	31.944103
597.279374	44599.380011	31.949120
598.163363	44670.257720	31.954138
598.770040	44747.640808	31.959156
599.197191	44825.356948	31.964173
599.985490	44877.653060	31.969191
600.470252	44962.750945	31.974208
601.402815	45037.454729	31.979226
601.818031	45099.685312	31.984244
602.270703	45182.241723	31.989261
602.874150	45248.713292	31.994279
603.898516	45336.097923	31.999296
603.951230	45413.805754	32.004314
604.973307	45485.800349	32.009332
605.253851	45569.157256	32.014349
605.636353	45638.274541	32.019367
606.409851	45719.283837	32.024384
607.048418	45793.174143	32.029402
607.525854	45874.375088	32.034420
608.042586	45979.034561	32.039437
608.421450	46053.837037	32.044455
609.146468	46142.916674	32.049472
609.610662	46238.114447	32.054490
610.513575	46318.969211	32.059508
610.938293	46425.212405	32.064525
611.462551	46493.700081	32.069543
611.947192	46588.315310	32.074560
612.366729	46686.263322	32.079578
613.314565	46774.718742	32.084596
613.681447	46866.257431	32.089613
614.514505	46962.793538	32.094631
615.154283	47043.379153	32.099648
615.951800	47156.356553	32.104666
616.536213	47231.761279	32.109684
616.951160	47326.609610	32.114701
617.754287	47438.618438	32.119719
618.472867	47518.331081	32.124736
618.948026	47627.029296	32.129754
619.697104	47711.079320	32.134772
620.281938	47797.701837	32.139789
620.998255	47891.578080	32.144807
621.891674	47969.808121	32.149824
622.354123	48061.156865	32.154842
623.149060	48155.394035	32.159860
623.542087	48234.705629	32.164877
624.455369	48332.602778	32.169895
625.456475	48411.950465	32.174912
626.126458	48491.302652	32.179930
626.776789	48575.325478	32.184948
627.287525	48652.712146	32.189965
627.566893	48735.363357	32.194983
628.362650	48799.930610	32.200000
629.028155	48895.045437	32.205018
629.828049	48969.988922	32.210036
630.257757	49066.523493	32.215053
630.801618	49134.202842	32.220071
632.038117	49216.338087	32.225088
632.672669	49285.922939	32.230106
633.243612	49357.684814	32.235124
634.002571	49417.274062	32.240141
634.496293	49500.164781	32.245159
635.019635	49542.658907	32.250176
635.903704	49626.382537	32.255194
636.389453	49693.053492	32.260212
637.037249	49774.587341	32.265229
637.601650	49838.214245	32.270247
637.965728	49903.229190	32.275264
638.420102	49982.421131	32.280282
639.163307	50069.757379	32.285300
639.844348	50136.606059	32.290317
640.043824	50234.940414	32.295335
640.825625	50288.282177	32.300352
641.150808	50376.254149	32.305370
641.805772	50482.627420	32.310388
642.431113	50571.349693	32.315405
643.152505	50648.261268	32.320423
643.549099	50730.889168	32.325440
644.240046	50835.063621	32.330458
645.046873	50915.780261	32.335476
645.878515	51019.367187	32.340493
646.228630	51090.215166	32.345511
647.399366	51176.045777	32.350528
648.167033	51283.491289	32.355546
649.008958	51346.249961	32.360564
649.421063	51439.312878	32.365581
650.081935	51519.835103	32.370599
650.656257	51599.696109	32.375616
651.033424	51681.879706	32.380634
652.176951	51782.917961	32.385652
652.610771	51884.522432	32.390669
652.966049	51974.445413	32.395687
653.616464	52063.479972	32.400704
654.213377	52154.560870	32.405722
654.622250	52243.105564	32.410740
655.037201	52356.995095	32.415757
655.695070	52454.263953	32.420775
656.939949	52559.676475	32.425792
657.449268	52641.450713	32.430810
657.842870	52736.670652	32.435828
658.576589	52843.647268	32.440845
659.151511	52947.763919	32.445863
660.033507	53034.844413	32.450880
660.546380	53160.838233	32.455898
661.258561	53247.199179	32.460916
662.249625	53340.368337	32.465933
662.908112	53440.269915	32.470951
663.730896	53533.594137	32.475968
664.045600	53642.485788	32.480986
664.532659	53740.907457	32.486004
665.332351	53844.596998	32.491021
665.974676	53944.213259	32.496039
666.889552	54050.803400	32.501056
667.488853	54156.106998	32.506074
668.109577	54237.433698	32.511092
668.801705	54331.516141	32.516109
668.916339	54442.169935	32.521127
669.858589	54552.106479	32.526144
670.241972	54657.745369	32.531162
671.012724	54755.259846	32.536180
672.116073	54861.412677	32.541197
673.062474	54955.171857	32.546215
674.108852	55051.359851	32.551232
674.348946	55155.748971	32.556250
675.208200	55257.585176	32.561268
676.268287	55329.664455	32.566285
676.776017	55434.585766	32.571303
677.632535	55526.669416	32.576320
678.015574	55598.785695	32.581338
678.688157	55684.317446	32.586356
679.348638	55757.152931	32.591373
680.085091	55852.631615	32.596391
680.489061	55929.521883	32.601408
681.041301	56034.540145	32.606426
681.227746	56124.563945	32.611444
682.141075	56213.002365	32.616461
682.610124	56321.687636	32.621479
683.199198	56414.748367	32.626496
684.118657	56508.797441	32.631514
685.038982	56623.140254	32.636532
685.509272	56710.921198	32.641549
685.880398	56817.439344	32.646567
686.988953	56915.711199	32.651584
687.240106	57030.899797	32.656602
687.783899	57126.359631	32.661620
688.416359	57228.913260	32.666637
688.723027	57361.589731	32.671655
689.717982	57477.138282	32.676672
690.408777	57586.356242	32.681690
690.797955	57717.542991	32.686708
691.557846	57820.476705	32.691725
692.065280	57954.570912	32.696743
693.324827	58064.936000	32.701760
694.115726	58175.467561	32.706778
694.848992	58298.128220	32.711796
696.436583	58383.337351	32.716813
696.986042	58489.304300	32.721831
698.015152	58570.948001	32.726848
699.097020	58674.907152	32.731866
699.611584	58792.160299	32.736884
700.518552	58864.966566	32.741901
700.537598	58977.140241	32.746919
701.326820	59057.309059	32.751936
702.379344	59180.965048	32.756954
702.702411	59285.646679	32.761972
703.872807	59354.411399	32.766989
703.937204	59472.918212	32.772007
704.546683	59588.157276	32.777024
705.438389	59691.173707	32.782042
705.788387	59815.865910	32.787060
706.711785	59911.838854	32.792077
706.961129	60026.470103	32.797095
708.192344	60126.184696	32.802112
708.752335	60248.266714	32.807130
709.178540	60346.156410	32.812148
710.136578	60467.763282	32.817165
710.917909	60581.248220	32.822183
711.981945	60670.123999	32.827200
712.993287	60775.641339	32.832218
713.596358	60863.684121	32.837236
714.800877	60960.083298	32.842253
715.217775	61073.062459	32.847271
716.341447	61157.077234	32.852288
716.727183	61280.312852	32.857306
717.272488	61383.091858	32.862324
718.207420	61460.415104	32.867341
718.749572	61565.420041	32.872359
719.458608	61645.928455	32.877376
720.072633	61747.339257	32.882394
720.430491	61874.425449	32.887412
721.287536	61983.374593	32.892429
721.875944	62089.524805	32.897447
722.327731	62196.083644	32.902464
722.979143	62296.555703	32.907482
723.881904	62396.910914	32.912500
724.656802	62500.890064	32.917517
725.026291	62618.695128	32.922535
726.134907	62713.469038	32.927552
726.804927	62826.422529	32.932570
727.397404	62916.839690	32.937588
727.674237	63017.731106	32.942605
728.121882	63137.314843	32.947623
728.999442	63230.612512	32.952640
729.858569	63355.046611	32.957658
730.288226	63486.213858	32.962676
731.459613	63588.843790	32.967693
731.761849	63718.794818	32.972711
732.565518	63823.736668	32.977728
733.278858	63949.197078	32.982746
733.819002	64077.177083	32.987764
735.123633	64186.658253	32.992781
735.530062	64324.237283	32.997799
736.219175	64445.299400	33.002816
736.750279	64549.063821	33.007834
737.211701	64671.827172	33.012852
738.294944	64804.702628	33.017869
738.914250	64934.564777	33.022887
739.908606	65059.214473	33.027904
740.920269	65185.341112	33.032922
741.474528	65304.464838	33.037940
742.486138	65443.171339	33.042957
743.336930	65573.953742	33.047975
744.109588	65677.962097	33.052992
745.727397	65797.222764	33.058010
745.550242	65896.370292	33.063028
746.727223	66017.594989	33.068045
747.486505	66141.417776	33.073063
748.173165	66263.401238	33.078080
748.908824	66364.448284	33.083098
749.284662	66507.148073	33.088116
750.080748	66626.606129	33.093133
751.189753	66752.922248	33.098151
751.877440	66862.974694	33.103168
752.976113	66970.873843	33.108186
753.261985	67089.843597	33.113204
754.199164	67224.124177	33.118221
755.075735	67330.197084	33.123239
755.426186	67465.612821	33.128256
756.076187	67573.892629	33.133274
756.876283	67717.902436	33.138292
757.662623	67852.351059	33.143309
758.388566	67964.350051	33.148327
759.115334	68090.471929	33.153344
760.136920	68217.449875	33.158362
761.268932	68329.990651	33.163380
761.965405	68455.936414	33.168397
762.652179	68570.650818	33.173415
763.372143	68700.709625	33.178432
764.259621	68809.708925	33.183450
764.932869	68945.093604	33.188468
765.696557	69043.658237	33.193485
766.456564	69178.701361	33.198503
767.127445	69304.081160	33.203520
767.676103	69433.129681	33.208538
768.723970	69542.308611	33.213556
769.625725	69675.826884	33.218573
770.406357	69789.255402	33.223591
771.093319	69936.561370	33.228608
771.574730	70037.699820	33.233626
772.143854	70191.153214	33.238644
773.145391	70306.065369	33.243661
773.638535	70420.493100	33.248679
774.148802	70565.967569	33.253696
775.121494	70668.096387	33.258714
775.511907	70795.554538	33.263732
776.394387	70938.011218	33.268749
777.157716	71049.217546	33.273767
777.815472	71190.239896	33.278784
778.903595	71316.656556	33.283802
779.698545	71454.092086	33.288820
780.615195	71557.302969	33.293837
781.515991	71690.144967	33.298855
782.452352	71808.812743	33.303872
783.486598	71934.464288	33.308890
784.109313	72045.857129	33.313908
785.046446	72171.064547	33.318925
785.609113	72283.157730	33.323943
786.257002	72408.932783	33.328960
787.182507	72534.327619	33.333978
787.797380	72665.952015	33.338996
788.862032	72793.620629	33.344013
789.385512	72916.921636	33.349031
789.818234	73057.026088	33.354048
790.908555	73168.878709	33.359066
791.481462	73315.442885	33.364084
792.231536	73438.368025	33.369101
793.029101	73588.924839	33.374119
793.648509	73728.446405	33.379136
794.444380	73845.239065	33.384154
795.253759	73993.925069	33.389172
796.023108	74144.351319	33.394189
796.885781	74293.795724	33.399207
797.515727	74440.592117	33.404224
798.738707	74588.809225	33.409242
799.554625	74708.891490	33.414260
800.509050	74844.874361	33.419277
801.119022	74992.980468	33.424295
802.762266	75110.013147	33.429312
803.885798	75236.213128	33.434330
804.600475	75380.845531	33.439348
804.985215	75489.013496	33.444365
806.204546	75635.006082	33.449383
806.827966	75760.532841	33.454400
807.568929	75895.141009	33.459418
808.108198	76021.208054	33.464436
808.705716	76160.053292	33.469453
809.736090	76293.294420	33.474471
810.336611	76445.535257	33.479488
811.213972	76560.526755	33.484506
811.763790	76717.065595	33.489524
812.387162	76855.512570	33.494541
813.360541	77009.820694	33.499559
813.811202	77140.797464	33.504576
815.037199	77285.130400	33.509594
816.164536	77433.249891	33.514612
816.417937	77593.632230	33.519629
817.621874	77731.229944	33.524647
818.509155	77869.848455	33.529664
819.543224	78010.726751	33.534682
819.996085	78151.373047	33.539700
821.107766	78301.815767	33.544717
822.338536	78416.429767	33.549735
822.896277	78557.029710	33.554752
823.775193	78707.089881	33.559770
824.470714	78852.557959	33.564788
825.216838	78981.890413	33.569805
825.948156	79118.449024	33.574823
826.621568	79264.283975	33.579840
827.773241	79399.687031	33.584858
828.538484	79526.179622	33.589876
829.180459	79657.531903	33.594893
830.118969	79819.044320	33.599911
830.798878	79955.066294	33.604928
831.712960	80066.812632	33.609946
832.667587	80210.336651	33.614964
833.475199	80335.928685	33.619981
834.701981	80465.867211	33.624999
834.899333	80588.727745	33.630016
835.716775	80724.586227	33.635034
836.452046	80856.518427	33.640052
837.074130	81007.654926	33.645069
837.933573	81128.581067	33.650087
838.771900	81287.432367	33.655104
839.517710	81426.963052	33.660122
840.129279	81573.873358	33.665140
840.921464	81729.629576	33.670157
841.841104	81880.615291	33.675175
842.486332	82043.647106	33.680192
843.438426	82191.757702	33.685210
844.334352	82362.682860	33.690228
845.214471	82508.719928	33.695245
846.401668	82648.495271	33.700263
846.928214	82819.054724	33.705280
847.948110	82951.926412	33.710298
849.104925	83120.631789	33.715316
849.723740	83258.391887	33.720333
850.676096	83427.639393	33.725351
850.839476	83594.007220	33.730368
852.414839	83733.510083	33.735386
853.254838	83904.854671	33.740404
854.094423	84048.485435	33.745421
854.853219	84220.516387	33.750439
855.496367	84363.890569	33.755456
857.018404	84521.158694	33.760474
857.660702	84673.202061	33.765492
858.402467	84817.733193	33.770509
859.516733	84993.855092	33.775527
860.184173	85163.080293	33.780544
861.304515	85306.792819	33.785562
862.152758	85461.243144	33.790580
862.897553	85609.226773	33.795597
864.120787	85789.600956	33.800615
864.324065	85937.517948	33.805632
865.218382	86079.849118	33.810650
866.043599	86249.682622	33.815668
866.694237	86426.315959	33.820685
868.118731	86564.007226	33.825703
869.078965	86740.408366	33.830720
869.949320	86894.744442	33.835738
870.975438	87045.822707	33.840756
871.668316	87200.139508	33.845773
872.803360	87374.890557	33.850791
873.784084	87525.099972	33.855808
874.516157	87669.707540	33.860826
875.741400	87827.002976	33.865844
876.265055	87971.526617	33.870861
877.054111	88133.135435	33.875879
877.919528	88300.313518	33.880896
878.936066	88457.824843	33.885914
879.423451	88624.643732	33.890932
880.320677	88789.782620	33.895949
881.278577	88960.075947	33.900967
882.086757	89111.013774	33.905984
882.474036	89292.723826	33.911002
883.680118	89445.515383	33.916020
884.189755	89598.030611	33.921037
885.472706	89770.699672	33.926055
886.288013	89925.773600	33.931072
886.981396	90113.083866	33.936090
888.013140	90256.784686	33.941108
888.775887	90432.885635	33.946125
889.808098	90576.379502	33.951143
890.643508	90752.616378	33.956160
891.409101	90889.986328	33.961178
892.672683	91055.732414	33.966196
893.468115	91206.540215	33.971213
895.127665	91342.847599	33.976231
895.743601	91499.540488	33.981248
896.537808	91633.486439	33.986266
897.669782	91799.088582	33.991284
898.391247	91960.279176	33.996301
899.253022	92119.397287	34.001319
899.899544	92276.716750	34.006336
900.447372	92436.186247	34.011354
901.569946	92601.339860	34.016372
902.100747	92765.149408	34.021389
903.285566	92920.283133	34.026407
904.044473	93103.612775	34.031424
905.019322	93272.662224	34.036442
905.975436	93433.096188	34.041460
906.509872	93618.662901	34.046477
907.646738	93788.429693	34.051495
908.494735	93960.498464	34.056512
909.378346	94140.619322	34.061530
910.364617	94308.440009	34.066548
911.332261	94493.758379	34.071565
912.092935	94662.302306	34.076583
912.684811	94833.938571	34.081600
913.799870	95026.325290	34.086618
915.378435	95190.345396	34.091636
916.387128	95376.170067	34.096653
918.039986	95546.072852	34.101671
919.174833	95690.915854	34.106688
919.836668	95837.996137	34.111706
920.827273	96004.486000	34.116724
921.903183	96151.012433	34.121741
922.775398	96328.499345	34.126759
923.187661	96493.543628	34.131776
924.477107	96643.594963	34.136794
925.761090	96820.365501	34.141812
926.218409	96999.679084	34.146829
927.256199	97166.048785	34.151847
927.820252	97321.616961	34.156864
928.453389	97492.853646	34.161882
929.387718	97661.376921	34.166900
930.160831	97846.797144	34.171917
930.765772	98017.187584	34.176935
931.811664	98215.719161	34.181952
932.718718	98386.024276	34.186970
934.091501	98550.949058	34.191988
934.765766	98751.894747	34.197005
936.202031	98919.856292	34.202023
937.159719	99077.263228	34.207040
938.252942	99249.822404	34.212058
939.568636	99408.539660	34.217076
940.321528	99593.115340	34.222093
941.172583	99753.481431	34.227111
942.088534	99928.505437	34.232128
942.822459	100113.315983	34.237146
943.836566	100270.721126	34.242164
944.496153	100463.693903	34.247181
944.975967	100629.381262	34.252199
945.913024	100825.989089	34.257216
947.091198	100993.336123	34.262234
948.204791	101178.256410	34.267252
948.865712	101358.985840	34.272269
949.908009	101532.240187	34.277287
950.924767	101701.410193	34.282304
951.625052	101887.904331	34.287322
952.969556	102039.853031	34.292340
953.425801	102223.509343	34.297357
954.493132	102392.859211	34.302375
955.402466	102573.714563	34.307392
956.032087	102755.123873	34.312410
957.117840	102910.374705	34.317428
958.096782	103110.317206	34.322445
959.002459	103283.606051	34.327463
960.028062	103457.585378	34.332480
960.914004	103667.044554	34.337498
962.049169	103845.731625	34.342516
962.691951	104023.114648	34.347533
963.496093	104193.703886	34.352551
964.802743	104405.416951	34.357568
965.186600	104594.319422	34.362586
966.674241	104772.080973	34.367604
967.263072	104985.563541	34.372621
968.229307	105178.742996	34.377639
969.057720	105376.397891	34.382656
970.027311	105577.494495	34.387674
970.983992	105783.255053	34.392692
972.048438	105993.881367	34.397709
973.086474	106167.199390	34.402727
974.517910	106380.396010	34.407744
975.180050	106591.612805	34.412762
976.348709	106781.674360	34.417780
977.186572	106989.370023	34.422797
978.198951	107201.458411	34.427815
979.465490	107384.631386	34.432832
981.120943	107580.368066	34.437850
982.204785	107770.298817	34.442868
982.985769	107952.504745	34.447885
983.599450	108152.014482	34.452903
984.826107	108369.877440	34.457920
985.440733	108563.880851	34.462938
986.581677	108752.783370	34.467956
987.762980	108957.651501	34.472973
988.799946	109143.344320	34.477991
989.795545	109358.302519	34.483008
990.569296	109556.504519	34.488026
991.907071	109754.298231	34.493044
992.560648	109948.647292	34.498061
993.850806	110161.790129	34.503079
994.675329	110344.093938	34.508096
995.662268	110565.345597	34.513114
996.585473	110763.265882	34.518132
997.382037	110985.793719	34.523149
998.415927	111177.378318	34.528167
999.575368	111389.070522	34.533184
1000.527956	111604.231173	34.538202
1001.585975	111780.932891	34.543220
1002.543682	112005.431195	34.548237
1003.255119	112192.832879	34.553255
1004.653166	112424.292039	34.558272
1005.576051	112634.893019	34.563290
1006.562204	112825.711813	34.568308
1007.478678	113052.378986	34.573325
1008.449746	113250.284219	34.578343
1009.435213	113445.781702	34.583360
1010.582939	113665.664061	34.588378
1011.819395	113871.282484	34.593396
1012.404895	114072.576229	34.598413
1013.592043	114288.238730	34.603431
1014.505006	114498.171632	34.608448
1015.479675	114712.099029	34.613466
1016.305939	114925.153152	34.618484
1017.275011	115127.379384	34.623501
1018.795268	115326.197010	34.628519
1020.240668	115518.048159	34.633536
1021.397897	115696.088941	34.638554
1022.423567	115898.552157	34.643572
1023.286315	116086.132784	34.648589
1023.575462	116296.004939	34.653607
1024.929183	116471.231125	34.658624
1025.624882	116680.253583	34.663642
1026.383246	116880.196272	34.668660
1027.367770	117100.804304	34.673677
1027.985983	117319.422142	34.678695
1029.304698	117535.886279	34.683712
1029.990509	117773.956491	34.688730
1031.128544	117986.412390	34.693748
1032.163847	118208.465042	34.698765
1032.706740	118431.804350	34.703783
1034.120837	118647.247690	34.708800
1035.341089	118880.538502	34.713818
1036.214428	119088.915997	34.718836
1037.570575	119326.229749	34.723853
1038.605160	119560.747778	34.728871
1039.848500	119767.536060	34.733888
1040.715504	120016.504260	34.738906
1042.179008	120239.870474	34.743924
1043.257591	120463.821469	34.748941
1044.148886	120682.673509	34.753959
1044.896291	120905.314185	34.758976
1046.003018	121129.151675	34.763994
1046.998795	121368.607176	34.769012
1048.175115	121587.089576	34.774029
1049.148077	121828.503993	34.779047
1050.196529	122062.191150	34.784064
1051.209670	122309.862543	34.789082
1052.124293	122534.502881	34.794100
1053.497367	122784.412424	34.799117
1054.435269	123009.648141	34.804135
1055.851607	123243.752884	34.809152
1056.998000	123461.506648	34.814170
1058.048554	123680.874518	34.819188
1059.105255	123928.628454	34.824205
1060.305351	124164.005421	34.829223
1061.514403	124399.218048	34.834240
1062.502690	124622.050062	34.839258
1063.524398	124863.696861	34.844276
1064.805682	125083.252490	34.849293
1065.746371	125324.029331	34.854311
1066.582843	125540.290836	34.859328
1067.582391	125797.118185	34.864346
1068.869245	126006.845551	34.869364
1070.404856	126242.728537	34.874381
1071.249924	126460.604761	34.879399
1072.549491	126674.377441	34.884416
1073.690777	126928.225544	34.889434
1074.522050	127146.185053	34.894452
1075.675392	127369.681996	34.899469
1076.247708	127618.902610	34.904487
1077.540236	127838.679336	34.909504
1078.498254	128104.582277	34.914522
1079.534875	128329.030756	34.919540
1080.814949	128538.130469	34.924557
1081.570169	128790.790505	34.929575
1083.047551	128999.062335	34.934592
1083.646535	129260.700045	34.939610
1084.737066	129499.204051	34.944628
1086.184942	129734.026004	34.949645
1086.865773	129973.209700	34.954663
1088.025869	130198.741511	34.959680
1089.141486	130447.008246	34.964698
1090.488192	130654.653771	34.969716
1091.668734	130881.974351	34.974733
1092.349019	131109.518606	34.979751
1093.476628	131339.348263	34.984768
1094.628187	131562.660572	34.989786
1095.637332	131799.890187	34.994804
1096.618842	132038.659895	34.999821
1097.486649	132286.018872	35.004839
1098.330352	132529.162782	35.009856
1099.831177	132762.414408	35.014874
1100.872451	133006.365989	35.019892
1102.175724	133232.745371	35.024909
1103.237731	133459.026767	35.029927
1104.330695	133703.786463	35.034944
1105.514204	133947.404914	35.039962
1106.782930	134180.794049	35.044980
1107.760193	134432.537756	35.049997
1108.574464	134670.645069	35.055015
1109.946418	134914.911660	35.060032
1110.756295	135166.435243	35.065050
1112.016404	135406.857649	35.070068
1113.061603	135662.491582	35.075085
1114.012887	135917.813445	35.080103
1115.104629	136171.935167	35.085120
1116.300779	136425.902200	35.090138
1117.385578	136680.624888	35.095156
1118.596359	136948.310439	35.100173
1119.733673	137209.646208	35.105191
1121.362423	137464.158454	35.110208
1122.641359	137704.277846	35.115226
1123.656130	137957.766972	35.120244
1125.224217	138203.826212	35.125261
1125.905905	138461.202929	35.130279
1127.075185	138695.617214	35.135296
1128.246813	138968.764619	35.140314
1129.523046	139226.391460	35.145332
1130.810429	139466.902647	35.150349
1131.964182	139724.984640	35.155367
1133.536403	139963.956340	35.160384
1134.035330	140221.376879	35.165402
1135.026751	140465.050395	35.170420
1136.637372	140714.164125	35.175437
1137.229780	140970.763539	35.180455
1138.982403	141201.396895	35.185472
1139.982512	141475.924409	35.190490
1140.359685	141735.506728	35.195508
1142.037742	141987.877298	35.200525
1143.374088	142240.623141	35.205543
1144.638141	142507.850128	35.210560
1145.379201	142765.288118	35.215578
1146.432991	143014.637486	35.220596
1147.651869	143270.123801	35.225613
1148.925775	143548.477482	35.230631
1150.103960	143797.456965	35.235648
1151.211979	144065.469970	35.240666
1152.056012	144322.839228	35.245684
1153.175752	144589.484897	35.250701
1154.063856	144853.355806	35.255719
1155.420906	145130.110760	35.260736
1156.923433	145381.038911	35.265754
1158.134250	145642.301043	35.270772
1159.326409	145894.298564	35.275789
1160.661108	146156.774114	35.280807
1161.696071	146432.983851	35.285824
1162.897998	146693.418321	35.290842
1164.056048	146960.329337	35.295860
1165.332650	147206.907451	35.300877
1165.922613	147455.629634	35.305895
1167.642121	147713.779609	35.310912
1168.406312	147958.519941	35.315930
1169.455546	148200.602488	35.320948
1170.837527	148449.441803	35.325965
1171.789050	148705.671278	35.330983
1172.730866	148968.676292	35.336000
1174.074285	149227.926482	35.341018
1175.012687	149492.838168	35.346036
1176.592587	149736.948661	35.351053
1177.559324	150014.085049	35.356071
1178.740940	150267.066311	35.361088
1179.826164	150539.241032	35.366106
1180.233490	150814.256415	35.371124
1181.719782	151071.809380	35.376141
1182.947725	151363.472487	35.381159
1183.920190	151626.225274	35.386176
1185.313846	151909.596172	35.391194
1186.406651	152182.644228	35.396212
1187.728335	152466.842975	35.401229
1188.945908	152747.015147	35.406247
1190.022824	153020.668080	35.411264
1191.457209	153320.429765	35.416282
1192.099345	153599.599854	35.421300
1193.261046	153894.426533	35.426317
1194.483594	154184.311532	35.431335
1195.909204	154489.575987	35.436352
1197.048990	154784.349799	35.441370
1198.338354	155070.323915	35.446388
1199.771366	155385.703444	35.451405
1200.956645	155667.056847	35.456423
1202.175335	155956.714973	35.461440
1203.680802	156253.951227	35.466458
1204.561900	156560.260729	35.471476
1205.828602	156837.499483	35.476493
1206.638386	157134.781231	35.481511
1207.798402	157458.518512	35.486528
1209.141752	157742.955992	35.491546
1210.422537	158050.530469	35.496564
1211.505770	158346.101885	35.501581
1212.835018	158650.273472	35.506599
1214.263144	158950.333758	35.511616
1215.805443	159256.821609	35.516634
1216.766950	159556.050160	35.521652
1218.141891	159872.782133	35.526669
1219.285039	160179.368339	35.531687
1220.430397	160487.998923	35.536704
1221.817175	160777.702882	35.541722
1222.695521	161100.095571	35.546740
1224.246634	161392.732630	35.551757
1225.886723	161696.355941	35.556775
1227.327577	161979.906829	35.561792
1229.107557	162284.031564	35.566810
1230.115423	162572.009418	35.571828
1231.756775	162850.382588	35.576845
1232.979969	163152.423596	35.581863
1234.453668	163429.749998	35.586880
1235.628543	163706.379067	35.591898
1236.538045	163997.123424	35.596916
1237.983927	164289.278326	35.601933
1239.298333	164562.946699	35.606951
1240.128047	164831.964597	35.611968
1241.049050	165145.551710	35.616986
1242.357067	165426.699485	35.622004
1243.671431	165721.930988	35.627021
1244.573508	166005.065391	35.632039
1245.824084	166322.717536	35.637056
1247.169130	166599.451719	35.642074
1247.800149	166900.412086	35.647092
1249.330907	167173.655593	35.652109
1250.833849	167469.159862	35.657127
1251.891881	167742.802199	35.662144
1253.002913	168018.366090	35.667162
1253.999959	168320.608174	35.672180
1255.457740	168586.665818	35.677197
1256.764066	168884.876681	35.682215
1257.947856	169172.540428	35.687232
1259.151230	169453.592166	35.692250
1260.385310	169766.818624	35.697268
1261.427077	170059.117512	35.702285
1262.603077	170367.079350	35.707303
1263.662454	170679.452871	35.712320
1264.842472	170980.553664	35.717338
1266.147641	171297.357394	35.722356
1267.339982	171594.755101	35.727373
1268.633490	171916.095077	35.732391
1269.732741	172252.277678	35.737408
1271.368573	172548.314142	35.742426
1272.647363	172886.070631	35.747444
1273.888603	173190.487916	35.752461
1275.357801	173508.460085	35.757479
1276.685246	173829.566800	35.762496
1278.227775	174128.179450	35.767514
1279.236444	174468.111280	35.772532
1280.649539	174770.239107	35.777549
1282.113032	175080.824771	35.782567
1283.242777	175415.464466	35.787584
1284.659590	175724.145879	35.792602
1285.926652	176061.077085	35.797620
1286.959186	176378.836248	35.802637
1288.537161	176710.885724	35.807655
1289.619898	177037.816141	35.812672
1291.238469	177348.073761	35.817690
1292.107468	177693.559449	35.822708
1293.685676	178025.909835	35.827725
1294.777232	178338.418207	35.832743
1295.609421	178688.155767	35.837760
1297.023136	179004.701696	35.842778
1298.528871	179345.918634	35.847796
1299.974130	179691.894409	35.852813
1301.236480	180049.198011	35.857831
1302.295556	180378.730963	35.862848
1304.089310	180693.397379	35.867866
1305.374780	181034.446475	35.872884
1306.972833	181368.364369	35.877901
1308.111334	181707.335453	35.882919
1309.348642	182039.413546	35.887936
1310.846717	182366.983226	35.892954
1312.190116	182720.916287	35.897972
1313.300108	183053.516938	35.902989
1314.491093	183405.817191	35.908007
1315.880741	183729.491545	35.913024
1317.484200	184079.824448	35.918042
1318.391003	184402.529197	35.923060
1319.693052	184759.072161	35.928077
1321.442085	185073.886929	35.933095
1322.967374	185408.299763	35.938112
1324.520361	185735.551458	35.943130
1325.757246	186081.756818	35.948148
1327.150790	186417.454273	35.953165
1328.383870	186742.315170	35.958183
1329.613076	187075.149839	35.963200
1330.995332	187406.082705	35.968218
1332.087107	187747.892753	35.973236
1333.581552	188081.908297	35.978253
1335.315175	188390.372883	35.983271
1336.371836	188728.247173	35.988288
1337.740721	189037.613304	35.993306
1338.579795	189347.322455	35.998324
1339.999973	189682.794204	36.003341
1341.400696	189985.026499	36.008359
1342.596593	190325.375345	36.013376
1343.948741	190638.586498	36.018394
1345.388218	190987.480083	36.023412
1346.154991	191304.548862	36.028429
1347.772432	191628.054474	36.033447
1348.693050	191985.671633	36.038464
1350.228591	192297.706338	36.043482
1350.962105	192651.397866	36.048500
1352.022982	193018.188783	36.053517
1354.097827	193371.891741	36.058535
1354.934248	193727.565718	36.063552
1356.114856	194107.418863	36.068570
1357.680810	194455.931280	36.073588
1359.110589	194808.136941	36.078605
1360.508887	195165.643547	36.083623
1362.065321	195539.984878	36.088640
1363.672483	195879.713797	36.093658
1364.970311	196246.066217	36.098676
1366.243865	196603.017766	36.103693
1367.537695	196958.635017	36.108711
1368.661348	197347.988112	36.113728
1370.067669	197731.215912	36.118746
1371.490636	198082.133603	36.123764
1372.522570	198472.714769	36.128781
1373.943783	198839.709297	36.133799
1375.352240	199234.892175	36.138816
1376.717360	199601.912958	36.143834
1377.965207	199989.192121	36.148852
1379.633054	200372.214629	36.153869
1381.396720	200754.360213	36.158887
1382.501087	201157.819010	36.163904
1384.247493	201524.228864	36.168922
1385.040819	201926.994525	36.173940
1386.645156	202329.920730	36.178957
1388.097008	202695.242837	36.183975
1389.308057	203089.147894	36.188992
1390.698214	203483.584264	36.194010
1392.123130	203877.090280	36.199028
1393.458201	204262.703393	36.204045
1395.159879	204655.393579	36.209063
1396.249016	205067.689073	36.214080
1397.679327	205456.809886	36.219098
1398.861701	205851.991987	36.224116
1400.513134	206256.545283	36.229133
1402.172993	206645.710735	36.234151
1403.302230	207056.131699	36.239168
1405.243402	207444.048694	36.244186
1406.603345	207852.620272	36.249204
1408.266206	208231.445314	36.254221
1409.964571	208647.240811	36.259239
1411.047990	209033.479077	36.264256
1412.200527	209414.184499	36.269274
1414.046328	209829.898534	36.274292
1415.129766	210207.241693	36.279309
1416.217142	210613.231748	36.284327
1417.931340	210999.489860	36.289344
1419.386073	211397.499936	36.294362
1420.877601	211802.476971	36.299380
1422.047232	212209.782050	36.304397
1423.637191	212609.578809	36.309415
1424.766202	213005.085467	36.314432
1426.259221	213412.317682	36.319450
1428.346479	213805.816060	36.324468
1429.463816	214166.588160	36.329485
1431.097482	214552.342787	36.334503
1432.696572	214930.511293	36.339520
1433.743329	215315.528087	36.344538
1435.291938	215676.387672	36.349556
1436.029166	216067.223878	36.354573
1438.000511	216526.328260	36.359591
1439.113215	216918.325261	36.364608
1440.270159	217318.545330	36.369626
1441.769000	217703.802523	36.374644
1443.215862	218100.600306	36.379661
1444.738705	218489.894977	36.384679
1446.019083	218896.222256	36.389696
1447.299197	219301.281427	36.394714
1448.904232	219689.551534	36.399732
1450.243897	220102.782333	36.404749
1451.938513	220496.018859	36.409767
1453.078853	220923.305699	36.414784
1454.873717	221317.290876	36.419802
1456.142967	221741.639130	36.424820
1457.815404	222151.470909	36.429837
1459.221232	222577.628773	36.434855
1460.368554	222985.798011	36.439872
1461.913554	223410.844159	36.444890
1463.621669	223829.921761	36.449908
1464.871292	224263.681042	36.454925
1466.575121	224675.803321	36.459943
1467.795739	225112.390046	36.464960
1469.247819	225539.390177	36.469978
1470.973731	225963.806806	36.474996
1472.111102	226392.081251	36.480013
1474.299434	226814.367367	36.485031
1475.750846	227240.357963	36.490048
1477.607001	227667.807284	36.495066
1479.030929	228088.903315	36.500084
1480.340277	228508.063927	36.505101
1482.468191	228925.643094	36.510119
1483.699801	229347.740380	36.515136
1485.167627	229780.722154	36.520154
1486.504293	230191.755861	36.525172
1487.786623	230625.837903	36.530189
1489.139226	231052.772282	36.535207
1490.787674	231491.826031	36.540224
1491.908521	231923.703720	36.545242
1493.356484	232352.810927	36.550260
1494.980071	232788.443858	36.555277
1496.700677	233234.197038	36.560295
1498.268189	233669.816528	36.565312
1499.996969	234100.635339	36.570330
1502.019480	234517.309385	36.575348
1503.403493	234944.809204	36.580365
1505.373199	235368.708218	36.585383
1506.783621	235809.084467	36.590400
1508.125939	236225.849997	36.595418
1509.624357	236661.337048	36.600436
1510.971102	237081.050616	36.605453
1512.574996	237524.574803	36.610471
1514.310394	237933.786376	36.615488
1515.520876	238359.139359	36.620506
1517.381682	238782.633352	36.625524
1518.840163	239202.308281	36.630541
1521.002458	239626.211750	36.635559
1522.362189	240028.682468	36.640576
1523.809566	240458.268808	36.645594
1525.080470	240863.067528	36.650612
1526.336618	241297.843885	36.655629
1527.827443	241728.746754	36.660647
1529.314853	242139.837453	36.665664
1530.393215	242551.885538	36.670682
1532.114016	242964.946111	36.675700
1533.263863	243382.293056	36.680717
1534.678098	243781.205892	36.685735
1536.466011	244204.469424	36.690752
1537.591211	244635.895642	36.695770
1539.251957	245047.750599	36.700788
1540.674184	245472.499266	36.705805
1541.897852	245902.311117	36.710823
1543.709472	246336.980170	36.715840
1545.418060	246757.466882	36.720858
1546.921437	247191.324496	36.725876
1548.572100	247609.383411	36.730893
1550.293140	248058.295628	36.735911
1551.823409	248484.936379	36.740928
1552.894067	248922.271930	36.745946
1554.790721	249361.300791	36.750964
1556.028431	249792.208443	36.755981
1557.309942	250253.364260	36.760999
1558.685229	250704.750480	36.766016
1560.061613	251158.880591	36.771034
1561.867142	251633.262816	36.776052
1563.086699	252094.659738	36.781069
1564.777673	252582.982814	36.786087
1566.066867	253045.690218	36.791104
1566.998410	253505.002274	36.796122
1569.280282	253991.095462	36.801140
1570.660813	254474.721304	36.806157
1572.338076	254963.455444	36.811175
1573.914193	255434.551462	36.816192
1575.031792	255944.514171	36.821210
1576.902055	256414.724038	36.826228
1578.063241	256917.160885	36.831245
1579.616299	257419.482565	36.836263
1581.521640	257919.536305	36.841280
1582.883634	258440.205781	36.846298
1584.660027	258937.334468	36.851316
1585.943163	259463.809309	36.856333
1587.296588	259963.827877	36.861351
1589.554227	260476.144977	36.866368
1591.018653	261000.888245	36.871386
1592.900025	261499.092523	36.876404
1594.326055	262012.690145	36.881421
1596.200322	262509.320595	36.886439
1598.512271	263034.508308	36.891456
1599.980610	263513.169273	36.896474
1601.942118	264013.366971	36.901492
1603.314232	264532.688845	36.906509
1605.032298	265020.021538	36.911527
1606.926623	265529.705238	36.916544
1608.256081	266041.056905	36.921562
1610.089252	266527.226788	36.926580
1611.609126	267029.807768	36.931597
1612.953367	267544.610942	36.936615
1614.518713	268030.798675	36.941632
1615.842729	268557.061259	36.946650
1618.025773	269068.981289	36.951668
1619.202043	269578.831494	36.956685
1620.797194	270103.295077	36.961703
1622.509030	270607.467202	36.966720
1623.594180	271127.644482	36.971738
1625.601634	271635.323105	36.976756
1626.948425	272165.312315	36.981773
1628.589982	272685.954701	36.986791
1629.904247	273208.072929	36.991808
1631.524916	273730.139840	36.996826
1633.317401	274256.165850	37.001844
1634.724661	274765.234711	37.006861
1636.212086	275279.090641	37.011879
1637.956336	275801.514840	37.016896
1639.535097	276309.968546	37.021914
1641.610994	276821.921078	37.026932
1642.993121	277330.075119	37.031949
1644.295617	277846.801962	37.036967
1646.409560	278339.337748	37.041984
1647.713026	278880.347048	37.047002
1649.658051	279378.243102	37.052020
1651.597141	279871.287230	37.057037
1653.296970	280396.655999	37.062055
1655.187228	280904.947236	37.067072
1656.760349	281418.751042	37.072090
1658.596395	281934.694777	37.077108
1660.628796	282419.665186	37.082125
1662.301318	282944.879623	37.087143
1664.545392	283454.299989	37.092160
1666.213290	283948.268152	37.097178
1668.113185	284450.045844	37.102196
1670.190919	284947.957150	37.107213
1672.104630	285451.228444	37.112231
1673.827760	285939.466627	37.117248
1674.873685	286427.027689	37.122266
1676.230460	286935.923964	37.127284
1678.182680	287456.531991	37.132301
1679.772204	287944.786251	37.137319
1681.193115	288466.215239	37.142336
1682.299496	288984.290610	37.147354
1683.985010	289521.522545	37.152372
1685.569802	290028.516752	37.157389
1687.053272	290557.929351	37.162407
1688.931759	291089.764068	37.167424
1690.001787	291644.641429	37.172442
1691.542271	292168.831395	37.177460
1692.917748	292718.624683	37.182477
1694.200390	293284.229941	37.187495
1696.018404	293839.127158	37.192512
1698.177273	294418.756126	37.197530
1700.176052	294967.116166	37.202548
1701.965254	295514.111352	37.207565
1703.691922	296091.771770	37.212583
1705.652546	296636.752390	37.217600
1706.913033	297221.443671	37.222618
1708.457517	297767.503623	37.227636
1710.252965	298338.436121	37.232653
1711.658384	298927.183970	37.237671
1713.822656	299491.242746	37.242688
1714.822278	300066.310603	37.247706
1716.350261	300665.137492	37.252724
1718.353439	301231.702708	37.257741
1719.636938	301828.861556	37.262759
1721.531933	302417.763209	37.267776
1723.162143	303011.632315	37.272794
1724.650965	303616.823243	37.277812
1726.205482	304211.738906	37.282829
1727.883557	304805.766992	37.287847
1730.021257	305427.373298	37.292864
1731.728456	306034.493890	37.297882
1733.669411	306637.889352	37.302900
1735.349218	307231.469906	37.307917
1737.081801	307846.955204	37.312935
1738.896587	308466.816270	37.317952
1740.653984	309064.917732	37.322970
1742.182340	309686.214160	37.327988
1743.820887	310271.298583	37.333005
1746.004640	310873.888304	37.338023
1747.996956	311500.986634	37.343040
1749.400990	312094.401294	37.348058
1751.061927	312699.222496	37.353076
1753.217494	313271.324874	37.358093
1754.720335	313850.793747	37.363111
1756.793087	314432.754578	37.368128
1758.680327	315008.240654	37.373146
1760.494725	315596.939474	37.378164
1762.489055	316175.852703	37.383181
1763.928263	316757.747956	37.388199
1765.264302	317338.944647	37.393216
1767.096522	317936.382918	37.398234
1768.843814	318523.317464	37.403252
1770.811942	319118.768266	37.408269
1772.116616	319715.161506	37.413287
1774.490796	320325.263049	37.418304
1775.934725	320912.430990	37.423322
1777.890024	321528.939166	37.428340
1779.317529	322132.756679	37.433357
1781.181404	322736.344467	37.438375
1783.030815	323344.347328	37.443392
1784.705730	323975.200178	37.448410
1786.179323	324601.382835	37.453428
1788.124932	325200.288037	37.458445
1789.528518	325850.185168	37.463463
1791.517227	326461.436666	37.468480
1793.483401	327099.726373	37.473498
1795.271200	327739.562377	37.478516
1797.498222	328371.423165	37.483533
1798.896308	329009.863061	37.488551
1800.571011	329630.960703	37.493568
1802.403696	330293.028677	37.498586
1803.978925	330930.657304	37.503604
1806.054108	331563.144321	37.508621
1807.592052	332228.895105	37.513639
1809.520602	332871.902677	37.518656
1811.598692	333536.990730	37.523674
1813.300709	334197.309513	37.528692
1815.127751	334846.302846	37.533709
1816.695223	335517.899986	37.538727
1818.856771	336176.570993	37.543744
1820.606616	336826.188501	37.548762
1822.457865	337496.673789	37.553780
1824.251410	338151.116820	37.558797
1826.158557	338815.687044	37.563815
1828.155961	339493.484775	37.568832
1830.278966	340136.730496	37.573850
1832.364775	340800.763828	37.578868
1834.702147	341469.290783	37.583885
1836.379438	342126.063920	37.588903
1838.426802	342792.286110	37.593920
1839.794826	343426.071076	37.598938
1841.773229	344073.732945	37.603956
1843.844278	344746.499176	37.608973
1845.121939	345400.427043	37.613991
1847.311974	346055.667753	37.619008
1849.235933	346722.872502	37.624026
1850.580014	347392.143320	37.629044
1852.862275	348039.879866	37.634061
1854.216642	348721.921849	37.639079
1856.066645	349375.244135	37.644096
1858.002990	350053.719077	37.649114
1860.194518	350717.396924	37.654132
1862.089555	351396.569491	37.659149
1863.805941	352062.767869	37.664167
1865.842271	352737.532029	37.669184
1867.653420	353400.091360	37.674202
1869.587604	354081.069492	37.679220
1871.445157	354733.704279	37.684237
1872.730054	355415.174902	37.689255
1874.818548	356059.174694	37.694272
1876.984885	356717.895103	37.699290
1878.972142	357364.150492	37.704308
1880.822116	357978.218449	37.709325
1882.169227	358638.186194	37.714343
1883.960024	359294.061354	37.719360
1885.433028	359942.518878	37.724378
1887.405542	360622.447832	37.729396
1889.260937	361289.850868	37.734413
1890.818408	361957.165312	37.739431
1892.927785	362633.232497	37.744448
1895.097924	363289.691726	37.749466
1896.571750	363978.881993	37.754484
1898.711091	364639.611826	37.759501
1900.547086	365330.621698	37.764519
1902.650173	366032.433538	37.769536
1904.093394	366707.830939	37.774554
1905.668306	367414.854923	37.779572
1908.081971	368117.567221	37.784589
1909.347875	368814.469176	37.789607
1911.492854	369522.628624	37.794624
1913.686245	370232.643962	37.799642
1915.124613	370953.627176	37.804660
1917.433410	371649.594433	37.809677
1919.486282	372372.249760	37.814695
1921.623695	373068.954145	37.819712
1923.548087	373795.584922	37.824730
1925.241461	374501.821429	37.829748
1927.352530	375217.182115	37.834765
1928.649293	375970.605581	37.839783
1930.856499	376685.033369	37.844800
1933.100174	377434.465289	37.849818
1934.930246	378165.613341	37.854836
1936.999906	378897.999990	37.859853
1938.757684	379638.690052	37.864871
1940.790866	380368.135235	37.869888
1942.483789	381109.590508	37.874906
1944.660005	381847.272974	37.879924
1946.879119	382584.095501	37.884941
1948.432618	383340.739732	37.889959
1950.600340	384074.596588	37.894976
1952.637868	384837.643753	37.899994
1954.258689	385594.479207	37.905012
1956.720270	386339.013490	37.910029
1958.628485	387100.812409	37.915047
1960.476484	387844.399305	37.920064
1962.415776	388604.737895	37.925082
1964.388680	389361.427488	37.930100
1966.681522	390115.460445	37.935117
1968.094674	390882.777977	37.940135
1969.653105	391637.960509	37.945152
1971.691754	392413.883530	37.950170
1973.630178	393199.335196	37.955188
1975.770654	393969.549582	37.960205
1978.083321	394752.719974	37.965223
1979.729772	395511.367606	37.970240
1982.003226	396292.553151	37.975258
1983.879605	397067.675526	37.980276
1985.707445	397831.963295	37.985293
1988.104392	398626.526389	37.990311
1990.218134	399390.600301	37.995328
1992.253127	400169.366808	38.000346
1993.757620	400949.619380	38.005364
1995.796213	401714.633620	38.010381
1997.867395	402509.069404	38.015399
1999.971448	403279.936119	38.020416
2001.930870	404061.550301	38.025434
2003.953710	404839.711786	38.030452
2006.511631	405580.490097	38.035469
2008.169428	406352.943621	38.040487
2009.896805	407089.967819	38.045504
2012.138571	407843.204739	38.050522
2014.459413	408605.351911	38.055540
2016.361451	409346.620002	38.060557
2018.151557	410108.407831	38.065575
2020.164484	410850.199744	38.070592
2022.137182	411614.423543	38.075610
2024.108847	412361.298371	38.080628
2026.138315	413140.314665	38.085645
2027.873685	413901.903588	38.090663
2029.758390	414680.493627	38.095680
2031.822217	415463.565334	38.100698
2033.470359	416249.873849	38.105716
2035.483510	417043.570491	38.110733
2037.501256	417838.103417	38.115751
2039.913650	418603.699815	38.120768
2041.747951	419406.091606	38.125786
2043.422313	420219.475905	38.130804
2045.644064	421029.882447	38.135821
2047.552137	421833.629527	38.140839
2049.710700	422651.110723	38.145856
2052.181461	423457.853398	38.150874
2053.790085	424286.488485	38.155892
2055.769714	425108.578218	38.160909
2058.080878	425917.116122	38.165927
2060.222662	426762.164925	38.170944
2062.753878	427563.270148	38.175962
2064.631889	428411.293122	38.180980
2066.688743	429235.308119	38.185997
2068.393280	430067.707182	38.191015
2070.101633	430888.229783	38.196032
2072.316272	431743.421411	38.201050
2074.056242	432601.293157	38.206068
2076.505076	433451.372903	38.211085
2078.476393	434308.840878	38.216103
2080.470431	435154.378247	38.221120
2082.872010	436014.496923	38.226138
2084.856358	436882.902955	38.231156
2086.859940	437724.802212	38.236173
2089.004654	438594.382763	38.241191
2091.128115	439467.324689	38.246208
2093.096128	440320.572292	38.251226
2095.654364	441197.222330	38.256244
2098.066360	442068.093565	38.261261
2100.480410	442921.472932	38.266279
2102.467274	443799.684307	38.271296
2104.788083	444653.822361	38.276314
2106.332917	445512.609104	38.281332
2108.463645	446388.821998	38.286349
2111.189612	447260.753148	38.291367
2113.177452	448124.120244	38.296384
2115.342264	449000.475613	38.301402
2117.344287	449863.214609	38.306420
2119.437819	450723.577048	38.311437
2121.844767	451589.417274	38.316455
2123.863678	452463.075654	38.321472
2126.089669	453314.864784	38.326490
2128.314541	454193.121551	38.331508
2130.492030	455048.591208	38.336525
2132.580536	455936.305352	38.341543
2134.841942	456789.515249	38.346560
2137.075517	457636.019708	38.351578
2139.191787	458517.702359	38.356596
2141.112171	459359.232232	38.361613
2143.509200	460224.362107	38.366631
2145.485867	461086.440454	38.371648
2147.595348	461933.495405	38.376666
2149.471899	462774.537208	38.381684
2151.628533	463606.954231	38.386701
2153.920935	464436.685619	38.391719
2156.016723	465293.812177	38.396736
2157.811509	466134.726002	38.401754
2160.111608	466966.624952	38.406772
2162.299421	467822.363087	38.411789
2164.317325	468667.680685	38.416807
2166.195990	469508.840551	38.421824
2168.875837	470352.914559	38.426842
2170.842029	471217.788042	38.431860
2172.897685	472077.049570	38.436877
2175.368451	472949.190033	38.441895
2177.090285	473816.361567	38.446912
2179.441060	474683.996170	38.451930
2181.161603	475567.356692	38.456948
2183.007260	476451.514071	38.461965
2185.431550	477326.289846	38.466983
2187.206332	478234.572432	38.472000
2189.219466	479133.982360	38.477018
2191.045926	480043.632915	38.482036
2193.346946	480979.323060	38.487053
2195.486892	481898.426722	38.492071
2197.622693	482838.897739	38.497088
2200.270545	483745.906295	38.502106
2202.538659	484691.006704	38.507124
2204.787191	485617.125662	38.512141
2207.019126	486553.752434	38.517159
2208.916182	487485.185139	38.522176
2211.213884	488443.563762	38.527194
2213.020209	489392.834234	38.532212
2215.150817	490359.769519	38.537229
2217.364709	491301.500002	38.542247
2219.378713	492292.678564	38.547264
2221.448766	493261.533376	38.552282
2223.972333	494242.018819	38.557300
2226.373769	495227.515534	38.562317
2228.814677	496177.927579	38.567335
2230.925632	497161.191482	38.572352
2233.846149	498137.806714	38.577370
2235.636125	499111.525016	38.582388
2237.917698	500092.320989	38.587405
2240.345337	501071.522401	38.592423
2242.649874	502057.749537	38.597440
2245.429220	503037.837504	38.602458
2247.681765	504013.364614	38.607476
2249.642632	504985.503167	38.612493
2252.030119	505969.013242	38.617511
2254.207976	506945.236987	38.622528
2256.767801	507945.393928	38.627546
2258.864919	508942.489932	38.632564
2260.622292	509922.991900	38.637581
2263.090124	510923.484971	38.642599
2265.115704	511918.745606	38.647616
2267.463960	512891.457617	38.652634
2269.643823	513913.590160	38.657652
2271.998832	514898.277010	38.662669
2274.441834	515911.214884	38.667687
2276.275769	516924.994610	38.672704
2279.053276	517913.909349	38.677722
2281.885598	518918.324250	38.682740
2284.168769	519916.516605	38.687757
2286.267261	520897.190920	38.692775
2288.606610	521897.060456	38.697792
2290.731575	522901.938550	38.702810
2293.270647	523894.894283	38.707828
2295.335341	524897.283714	38.712845
2297.803764	525853.854235	38.717863
2299.567911	526838.636127	38.722880
2302.158613	527796.423706	38.727898
2304.526205	528780.022453	38.732916
2306.361379	529738.364818	38.737933
2308.433959	530692.225731	38.742951
2310.545833	531700.851752	38.747968
2312.991235	532684.381619	38.752986
2315.030567	533670.933644	38.758004
2317.013811	534663.771795	38.763021
2319.413496	535642.631167	38.768039
2321.567152	536665.810113	38.773056
2323.944739	537692.604678	38.778074
2326.112226	538702.803500	38.783092
2328.412179	539723.326821	38.788109
2330.902004	540743.947721	38.793127
2333.131462	541772.287597	38.798144
2335.470808	542817.440392	38.803162
2338.170146	543836.145333	38.808180
2340.291311	544880.226320	38.813197
2342.916153	545920.022274	38.818215
2345.082894	546983.658091	38.823232
2347.365003	548023.304369	38.828250
2349.861297	549053.986727	38.833268
2352.438037	550116.360567	38.838285
2355.013828	551177.345677	38.843303
2357.468758	552234.146209	38.848320
2359.664665	553296.237301	38.853338
2362.371213	554349.012431	38.858356
2364.148245	555412.767502	38.863373
2366.549022	556464.725608	38.868391
2368.922328	557549.727365	38.873408
2371.493529	558620.085385	38.878426
2374.036974	559680.814907	38.883444
2375.936135	560772.317863	38.888461
2378.661621	561862.087899	38.893479
2380.784529	562937.700419	38.898496
2383.037489	564026.566504	38.903514
2385.885081	565106.956494	38.908532
2387.716586	566217.159178	38.913549
2390.148511	567329.378397	38.918567
2392.485475	568424.896159	38.923584
2395.047354	569526.761918	38.928602
2397.526641	570638.488828	38.933620
2399.844849	571740.004898	38.938637
2402.013940	572869.964980	38.943655
2404.393580	574001.195947	38.948672
2406.627979	575112.926131	38.953690
2408.958769	576251.493590	38.958708
2411.396303	577385.524772	38.963725
2413.790018	578490.558300	38.968743
2416.494069	579637.137768	38.973760
2419.464596	580749.503154	38.978778
2421.750356	581880.643629	38.983796
2424.135587	583036.242975	38.988813
2426.549414	584158.626924	38.993831
2429.215265	585287.637335	38.998848
2431.602616	586414.533699	39.003866
2434.417587	587555.846820	39.008884
2436.669611	588679.497525	39.013901
2438.926467	589801.238557	39.018919
2441.335132	590931.923519	39.023936
2444.140231	592065.895403	39.028954
2446.615627	593175.757702	39.033972
2448.924511	594334.054206	39.038989
2451.447358	595472.209470	39.044007
2453.848861	596596.346700	39.049024
2456.359801	597710.138786	39.054042
2458.770089	598825.495262	39.059060
2460.925210	599919.149116	39.064077
2463.680212	601027.276714	39.069095
2466.510424	602129.677584	39.074112
2468.226466	603217.685704	39.079130
2470.336228	604311.384959	39.084148
2472.696032	605436.831297	39.089165
2475.044774	606541.393991	39.094183
2477.374100	607670.430959	39.099200
2479.376913	608804.865682	39.104218
2481.876067	609950.165664	39.109236
2484.179180	611075.265776	39.114253
2486.749374	612232.733229	39.119271
2488.876020	613373.444509	39.124288
2491.141081	614561.441325	39.129306
2493.804253	615725.286554	39.134324
2496.333456	616902.936454	39.139341
2498.630170	618073.648400	39.144359
2501.645253	619265.269878	39.149376
2503.752035	620463.562090	39.154394
2506.055066	621648.092980	39.159412
2509.235291	622862.793752	39.164429
2511.859024	624054.808868	39.169447
2514.338491	625249.165848	39.174464
2516.700980	626441.911202	39.179482
2519.602880	627657.719861	39.184500
2521.590791	628880.386199	39.189517
2524.961448	630061.922153	39.194535
2528.159590	631257.691090	39.199552
2531.143704	632467.095269	39.204570
2534.146359	633661.476949	39.209588
2536.348945	634862.296659	39.214605
2539.338462	636054.112548	39.219623
2541.801204	637251.720542	39.224640
2543.793317	638452.613197	39.229658
2546.323359	639648.986559	39.234676
2548.601983	640854.345891	39.239693
2550.888585	642072.636610	39.244711
2553.240535	643296.460221	39.249728
2555.662449	644505.709572	39.254746
2558.063986	645739.110853	39.259764
2560.532051	646980.481446	39.264781
2562.740333	648225.333739	39.269799
2565.454728	649487.750112	39.274816
2567.582900	650743.823513	39.279834
2570.252039	652013.110068	39.284852
2572.546025	653266.597372	39.289869
2575.431992	654520.677016	39.294887
2577.967402	655817.908678	39.299904
2580.161228	657089.916081	39.304922
2583.379730	658358.053883	39.309940
2586.189402	659629.482868	39.314957
2588.743627	660914.784140	39.319975
2591.378348	662171.369305	39.324992
2593.683240	663459.563669	39.330010
2596.852265	664755.758705	39.335028
2599.273497	666019.995901	39.340045
2601.906333	667294.882612	39.345063
2604.731564	668574.544946	39.350080
2607.915124	669838.154225	39.355098
2610.836193	671104.077282	39.360116
2613.418837	672402.918055	39.365133
2616.622027	673649.452821	39.370151
2618.911306	674895.675349	39.375168
2621.454032	676164.862912	39.380186
2624.571118	677431.994314	39.385204
2626.635854	678688.588706	39.390221
2629.135999	679926.948900	39.395239
2631.915115	681161.470110	39.400256
2634.035583	682395.587477	39.405274
2636.862093	683617.151355	39.410292
2639.266122	684837.480091	39.415309
2641.593895	686072.461172	39.420327
2644.284872	687297.232945	39.425344
2645.901137	688539.596239	39.430362
2648.419708	689776.477208	39.435380
2650.671781	691060.494620	39.440397
2652.802913	692330.252330	39.445415
2655.793308	693601.972192	39.450432
2658.231956	694918.312993	39.455450
2661.021418	696218.326595	39.460468
2663.484320	697503.123267	39.465485
2665.813260	698814.292761	39.470503
2668.458397	700148.475325	39.475520
2670.700174	701482.621667	39.480538
2673.812849	702804.027253	39.485556
2676.440760	704137.854863	39.490573
2678.906517	705484.837975	39.495591
2681.513704	706830.152096	39.500608
2684.077139	708200.187352	39.505626
2686.980847	709574.506973	39.510644
2689.252128	710947.720816	39.515661
2692.191452	712314.166655	39.520679
2694.717484	713700.565878	39.525696
2697.369063	715097.066080	39.530714
2700.009146	716485.468045	39.535732
2702.463610	717902.922501	39.540749
2705.434300	719310.255948	39.545767
2708.040147	720712.565296	39.550784
2710.441958	722146.035446	39.555802
2713.267246	723566.775611	39.560820
2716.202275	725021.770895	39.565837
2718.838081	726443.137935	39.570855
2721.861332	727875.121112	39.575872
2724.404442	729313.903038	39.580890
2727.821558	730763.308117	39.585908
2730.396521	732188.583410	39.590925
2733.164751	733631.360661	39.595943
2736.682577	735062.200897	39.600960
2739.497328	736501.545411	39.605978
2742.554234	737939.654959	39.610996
2745.440088	739369.291694	39.616013
2748.257948	740786.099123	39.621031
2751.145691	742227.858743	39.626048
2753.878411	743664.892929	39.631066
2756.488794	745087.727141	39.636084
2759.100736	746545.764495	39.641101
2761.736184	747968.124078	39.646119
2764.913327	749394.327007	39.651136
2767.531643	750853.238928	39.656154
2770.447179	752254.957512	39.661172
2773.287673	753697.332007	39.666189
2775.866181	755151.008569	39.671207
2778.719672	756585.747755	39.676224
2781.298844	758029.374757	39.681242
2784.172011	759462.095630	39.686260
2786.988978	760920.056344	39.691277
2789.811474	762380.296166	39.696295
2792.557003	763827.473617	39.701312
2794.942870	765269.218334	39.706330
2797.576168	766745.816371	39.711348
2800.225123	768189.220781	39.716365
2802.878990	769657.570031	39.721383
2805.868563	771121.494710	39.726400
2808.315441	772590.037308	39.731418
2810.849274	774066.137038	39.736436
2813.786315	775502.570902	39.741453
2816.133589	776937.495414	39.746471
2819.052643	778382.898767	39.751488
2821.586385	779817.179400	39.756506
2824.790565	781268.445982	39.761524
2827.795475	782720.584441	39.766541
2830.254565	784158.585174	39.771559
2833.271274	785620.984208	39.776576
2835.677474	787080.243523	39.781594
2838.251843	788527.898515	39.786612
2841.326656	790025.289115	39.791629
2843.846450	791524.515464	39.796647
2846.679423	792999.701144	39.801664
2849.227710	794478.840488	39.806682
2852.139198	795989.307200	39.811700
2855.395003	797494.984536	39.816717
2858.024851	799016.258872	39.821735
2860.589196	800520.664558	39.826752
2863.123283	802050.399312	39.831770
2865.695371	803602.840286	39.836788
2868.557297	805139.081797	39.841805
2871.493168	806686.121567	39.846823
2874.403540	808242.695927	39.851840
2877.451281	809819.331239	39.856858
2880.208408	811377.172760	39.861876
2883.094060	812960.684429	39.866893
2885.792434	814533.254545	39.871911
2889.400576	816088.114162	39.876928
2892.474090	817665.949015	39.881946
2895.512569	819251.377091	39.886964
2898.778348	820821.796568	39.891981
2901.543463	822424.381777	39.896999
2904.911264	824015.356871	39.902016
2907.516181	825595.441558	39.907034
2909.978278	827179.316535	39.912052
2913.143676	828781.513508	39.917069
2915.709951	830399.843781	39.922087
2918.404568	832000.647401	39.927104
2921.520296	833626.029335	39.932122
2924.645178	835220.463457	39.937140
2927.523593	836839.330414	39.942157
2930.146340	838474.628041	39.947175
2933.429202	840080.977289	39.952192
2936.522433	841709.920850	39.957210
2939.097982	843334.739306	39.962228
2941.900751	844978.849750	39.967245
2944.676974	846609.215984	39.972263
2947.755715	848268.081176	39.977280
2950.478623	849908.976417	39.982298
2953.449368	851550.470162	39.987316
2956.452321	853211.343412	39.992333
2959.367726	854885.286557	39.997351
2962.400294	856526.720710	40.002368
2965.441690	858193.729686	40.007386
2968.451575	859864.756484	40.012404
2971.298219	861525.945926	40.017421
2973.892392	863201.370179	40.022439
2977.384716	864865.327544	40.027456
2980.294780	866519.329616	40.032474
2983.149945	868191.978644	40.037492
2986.262831	869874.874860	40.042509
2989.072596	871550.764865	40.047527
2992.284532	873233.962685	40.052544
2995.357698	874920.581033	40.057562
2998.456524	876596.073526	40.062580
3000.957905	878256.681006	40.067597
3003.389203	879966.059287	40.072615
3006.782643	881636.497653	40.077632
3009.770258	883276.275141	40.082650
3012.755473	884923.227567	40.087668
3016.006661	886562.812932	40.092685
3018.908873	888222.370722	40.097703
3022.301238	889847.871601	40.102720
3025.073468	891477.457417	40.107738
3027.919717	893139.956069	40.112756
3030.617186	894812.030124	40.117773
3033.652152	896455.015558	40.122791
3036.849556	898114.468717	40.127808
3039.963052	899767.283223	40.132826
3043.057378	901426.363469	40.137844
3045.983451	903095.098046	40.142861
3049.185295	904794.202763	40.147879
3052.096891	906461.073831	40.152896
3055.417750	908124.782443	40.157914
3058.075813	909813.598538	40.162932
3061.784449	911505.575451	40.167949
3064.249905	913210.797075	40.172967
3067.806720	914902.624701	40.177984
3071.212918	916593.956904	40.183002
3073.779548	918300.659369	40.188020
3077.266395	920003.700503	40.193037
3079.826659	921700.121998	40.198055
3082.800088	923435.196379	40.203072
3085.528131	925167.644316	40.208090
3088.410587	926898.071803	40.213108
3091.468631	928651.306832	40.218125
3094.570808	930399.264533	40.223143
3097.431793	932147.647870	40.228160
3100.655846	933927.770662	40.233178
3103.731083	935686.064429	40.238196
3106.850875	937463.483412	40.243213
3109.811519	939253.246099	40.248231
3112.893373	941036.065683	40.253248
3115.884339	942816.571561	40.258266
3119.166228	944623.089712	40.263284
3122.477356	946424.483995	40.268301
3125.185047	948228.407558	40.273319
3128.410514	950037.917236	40.278336
3131.772180	951850.013071	40.283354
3134.422304	953682.672526	40.288372
3137.640416	955480.338336	40.293389
3140.558900	957367.519550	40.298407
3143.714729	959254.961153	40.303424
3146.624614	961135.275164	40.308442
3149.901866	963028.012967	40.313460
3153.710503	964923.461254	40.318477
3156.677078	966798.986216	40.323495
3160.245566	968708.952885	40.328512
3163.537876	970586.020215	40.333530
3166.514395	972467.404960	40.338548
3169.353427	974368.875797	40.343565
3172.493806	976299.603775	40.348583
3175.538587	978196.064681	40.353600
3178.798671	980096.344293	40.358618
3181.596686	982006.492164	40.363636
3185.259326	983928.324249	40.368653
3188.243240	985838.522551	40.373671
3191.303035	987773.469093	40.378688
3194.646577	989677.552430	40.383706
3197.301233	991600.271490	40.388724
3200.688048	993513.275396	40.393741
3203.993369	995469.869664	40.398759
3207.292016	997396.060936	40.403776
3210.300035	999313.681742	40.408794
3213.662135	1001253.702633	40.413812
3217.061001	1003155.103367	40.418829
3219.872316	1005047.714549	40.423847
3223.317794	1006934.446822	40.428864
3226.479823	1008815.359411	40.433882
3229.543381	1010710.878655	40.438900
3232.823679	1012576.268609	40.443917
3236.022267	1014468.950571	40.448935
3239.092156	1016374.185881	40.453952
3242.110009	1018251.971158	40.458970
3245.044709	1020147.817934	40.463988
3247.901471	1022076.602967	40.469005
3250.640120	1024015.864187	40.474023
3253.810243	1025948.293077	40.479040
3257.190401	1027910.941993	40.484058
3259.876186	1029858.430154	40.489076
3263.048092	1031807.476822	40.494093
3266.040534	1033813.403737	40.499111
3269.292678	1035800.039351	40.504128
3272.347741	1037773.555560	40.509146
3275.315259	1039800.095293	40.514164
3278.711741	1041813.969779	40.519181
3281.595695	1043846.951268	40.524199
3284.715995	1045882.712902	40.529216
3287.954773	1047942.933838	40.534234
3290.682594	1049994.099039	40.539252
3294.273543	1052071.301103	40.544269
3297.432361	1054153.179587	40.549287
3300.471003	1056235.927407	40.554304
3303.801614	1058345.998958	40.559322
3306.690898	1060441.405835	40.564340
3310.500331	1062559.006752	40.569357
3313.985055	1064679.013582	40.574375
3317.346613	1066804.747680	40.579392
3320.769409	1068928.401583	40.584410
3323.852274	1071056.946009	40.589428
3327.156970	1073209.737719	40.594445
3330.656853	1075350.632870	40.599463
3333.470056	1077485.343989	40.604480
3336.998811	1079653.182788	40.609498
3340.213782	1081816.862682	40.614516
3343.753484	1083985.082412	40.619533
3347.265115	1086139.343953	40.624551
3350.628853	1088314.281547	40.629568
3354.191222	1090482.583454	40.634586
3357.788080	1092673.411164	40.639604
3361.196917	1094841.141866	40.644621
3364.580115	1097025.090133	40.649639
3367.808789	1099194.446800	40.654656
3371.892595	1101368.512778	40.659674
3375.174650	1103527.062415	40.664692
3379.024897	1105689.227631	40.669709
3382.391616	1107876.888947	40.674727
3385.680129	1110053.869031	40.679744
3389.309488	1112199.081177	40.684762
3392.267731	1114364.282654	40.689780
3395.788164	1116534.127494	40.694797
3399.454871	1118696.607046	40.699815
3402.536955	1120873.414776	40.704832
3406.610470	1123027.616630	40.709850
3409.775722	1125191.825988	40.714868
3413.303745	1127346.842929	40.719885
3417.321108	1129525.473893	40.724903
3420.295193	1131664.703173	40.729920
3423.783363	1133811.232834	40.734938
3426.859951	1135990.025162	40.739956
3430.418412	1138134.038254	40.744973
3433.848160	1140307.684991	40.749991
3436.846748	1142488.458757	40.755008
3440.268362	1144620.144398	40.760013
3442.840376	1146732.749769	40.765018
3446.141020	1148773.805003	40.770023
3449.292176	1150769.297625	40.775028
3452.231470	1152687.572419	40.780032
3455.509711	1154535.247065	40.785037
3458.473291	1156295.094340	40.790042
3461.303857	1158004.625545	40.795047
3463.863350	1159616.447619	40.800052
3466.308574	1161156.050946	40.805056
3469.242242	1162631.904050	40.810061
3471.344078	1164035.680862	40.815066
3473.997526	1165359.749887	40.820071
3476.691379	1166607.654707	40.825076
3478.985349	1167766.305570	40.830080
3481.380740	1168873.338321	40.835085
3483.321956	1169906.984436	40.840090
3485.681153	1170860.445055	40.845095
3487.694218	1171784.357182	40.850100
3489.141167	1172621.711842	40.855104
3491.011529	1173395.491745	40.860109
3492.369466	1174127.188523	40.865114
3493.982322	1174797.272573	40.870119
3495.705597	1175423.324777	40.875124
3497.059489	1175990.264970	40.880128
3498.482710	1176524.428955	40.885133
3499.465124	1176988.687386	40.890138
3500.940696	1177415.131630	40.895143
3502.586256	1177813.529050	40.900148
3503.173122	1178174.949551	40.905152
3504.574619	1178477.329910	40.910157
3505.253793	1178771.804240	40.915162
3506.492565	1178997.121233	40.920167
3507.729677	1179224.312643	40.925172
3508.246098	1179390.104910	40.930176
3509.343694	1179519.438573	40.935181
3509.880979	1179643.492531	40.940186
3510.610384	1179750.746660	40.945191
3511.516820	1179821.237194	40.950196
3511.816306	1179844.640210	40.955200
3512.632951	1179852.417455	40.960205
3513.350329	1179860.870330	40.965210
3513.785851	1179829.529356	40.970215
3514.683364	1179786.715599	40.975220
3514.712939	1179728.032634	40.980224
3515.209039	1179629.430387	40.985229
3516.015696	1179521.261850	40.990234
3516.476625	1179417.104105	40.995239
3517.286648	1179269.839622	41.000244
3517.233542	1179128.176613	41.005248
3517.868149	1178965.860706	41.010253
3518.138806	1178791.353149	41.015258
3518.419940	1178590.836726	41.020263
3518.764253	1178394.635892	41.025268
3519.172604	1178176.276564	41.030272
3518.891289	1177964.522779	41.035277
3518.991671	1177730.555060	41.040282
3519.677591	1177474.148392	41.045287
3519.949437	1177232.780264	41.050292
3520.356246	1176961.505575	41.055296
3520.575418	1176699.577624	41.060301
3520.842485	1176425.565003	41.065306
3520.822961	1176138.861128	41.070311
3521.241667	1175863.945706	41.075316
3521.555535	1175542.561595	41.080320
3521.508077	1175215.466759	41.085325
3521.559019	1174916.806094	41.090330
3521.701211	1174600.200100	41.095335
3521.776581	1174283.491585	41.100340
3521.798074	1173961.775241	41.105344
3522.221981	1173630.920202	41.110349
3522.491637	1173280.077178	41.115354
3522.489700	1172945.476618	41.120359
3522.484046	1172596.236190	41.125364
3522.452990	1172244.618490	41.130368
3522.931543	1171902.892022	41.135373
3522.656060	1171544.664372	41.140378
3522.656136	1171167.781371	41.145383
3523.004269	1170807.230519	41.150388
3522.749656	1170452.037919	41.155392
3523.401875	1170064.588796	41.160397
3522.911166	1169711.743761	41.165402
3523.122378	1169335.354266	41.170407
3523.176636	1168948.958995	41.175412
3523.151288	1168575.290783	41.180416
3523.179694	1168192.430601	41.185421
3523.258809	1167799.432909	41.190426
3523.440532	1167420.644676	41.195431
3523.537023	1167038.916122	41.200436
3523.425472	1166631.416256	41.205440
3523.420687	1166234.443363	41.210445
3523.592952	1165856.582147	41.215450
3523.504845	1165455.408589	41.220455
3523.509907	1165056.266885	41.225460
3523.242103	1164669.419429	41.230464
3523.358606	1164250.833727	41.235469
3523.602974	1163852.977875	41.240474
3523.799474	1163473.051122	41.245479
3524.031503	1163060.870486	41.250484
3523.834309	1162636.349138	41.255488
3523.884575	1162242.277280	41.260493
3523.836795	1161836.567155	41.265498
3523.890561	1161409.731375	41.270503
3524.071729	1161010.535902	41.275508
3523.798777	1160590.304014	41.280512
3523.770601	1160176.143276	41.285517
3523.480140	1159761.520301	41.290522
3523.731381	1159330.039006	41.295527
3524.403194	1158928.902346	41.300532
3524.234825	1158516.619559	41.305536
3524.248528	1158079.873278	41.310541
3524.449347	1157661.693295	41.315546
3524.338292	1157230.572092	41.320551
3524.446205	1156805.717733	41.325556
3524.110308	1156360.561183	41.330560
3524.006888	1155917.220981	41.335565
3523.943168	1155517.364250	41.340570
3523.971208	1155099.765867	41.345575
3523.861324	1154663.607689	41.350580
3524.234314	1154226.481994	41.355584
3524.091115	1153801.899516	41.360589
3523.969944	1153377.941794	41.365594
3524.099687	1152940.938730	41.370599
3524.078232	1152523.144016	41.375604
3524.019633	1152086.763838	41.380608
3524.211384	1151635.249924	41.385613
3523.934996	1151217.961839	41.390618
3524.002195	1150790.071389	41.395623
3523.515799	1150359.490582	41.400628
3523.366599	1149936.491770	41.405632
3523.567261	1149504.496558	41.410637
3523.737961	1149074.744667	41.415642
3523.778423	1148634.083202	41.420647
3524.083122	1148209.544672	41.425652
3523.911443	1147799.359701	41.430656
3523.849861	1147344.298108	41.435661
3524.007158	1146903.472918	41.440666
3523.776104	1146462.295745	41.445671
3524.005766	1146040.628369	41.450676
3523.768674	1145604.025446	41.455680
3523.599496	1145159.980050	41.460685
3523.359241	1144727.192429	41.465690
3523.314851	1144297.087067	41.470695
3523.555689	1143875.814098	41.475700
3523.608501	1143427.888151	41.480704
3523.510472	1142995.694120	41.485709
3523.521759	1142571.130192	41.490714
3523.543889	1142134.387752	41.495719
3523.507332	1141705.493357	41.500724
3523.245619	1141288.556172	41.505728
3523.462896	1140835.639743	41.510733
3523.173733	1140394.914682	41.515738
3523.170202	1139973.845849	41.520743
3523.003428	1139539.577808	41.525748
3522.705095	1139113.079194	41.530752
3522.592061	1138687.939639	41.535757
3522.628862	1138262.646382	41.540762
3522.655207	1137848.618787	41.545767
3522.824713	1137424.280814	41.550772
3522.562829	1137001.404304	41.555776
3522.797007	1136578.127499	41.560781
3522.480267	1136166.779132	41.565786
3522.376929	1135729.244481	41.570791
3522.701429	1135308.700978	41.575796
3522.376481	1134906.850013	41.580800
3522.748677	1134483.668506	41.585805
3522.458209	1134048.211230	41.590810
3522.249978	1133617.930665	41.595815
3522.654095	1133207.184512	41.600820
3522.502545	1132786.804899	41.605824
3522.482115	1132352.779794	41.610829
3522.621169	1131947.777450	41.615834
3522.652909	1131516.431878	41.620839
3522.683864	1131090.850269	41.625844
3522.320565	1130673.570632	41.630848
3522.774169	1130237.203347	41.635853
3522.256589	1129821.593727	41.640858
3522.318773	1129392.828508	41.645863
3522.478312	1128954.502710	41.650868
3522.287127	1128544.826116	41.655872
3522.117358	1128116.757261	41.660877
3522.069476	1127687.397348	41.665882
3522.290270	1127261.193045	41.670887
3521.787995	1126847.251444	41.675892
3522.081180	1126448.655369	41.680896
3521.998315	1126011.174050	41.685901
3521.949143	1125588.020556	41.690906
3521.927667	1125172.918219	41.695911
3522.242356	1124749.257629	41.700916
3521.810517	1124340.725262	41.705920
3521.866119	1123902.001231	41.710925
3521.820612	1123507.620054	41.715930
3522.173810	1123080.203211	41.720935
3522.387378	1122654.489011	41.725940
3521.753596	1122236.498077	41.730944
3522.139218	1121799.832357	41.735949
3521.931033	1121383.894894	41.740954
3521.614355	1120959.752055	41.745959
3521.457334	1120557.171094	41.750964
3521.631521	1120126.404317	41.755968
3521.572641	1119705.548844	41.760973
3521.438914	1119303.631846	41.765978
3521.498882	1118884.121295	41.770983
3521.449907	1118474.410405	41.775988
3521.262673	1118077.079201	41.780992
3521.223120	1117643.288971	41.785997
3521.250705	1117231.659664	41.791002
3520.927067	1116837.690122	41.796007
3521.277650	1116435.478083	41.801012
3521.055987	1116011.213376	41.806016
3521.220439	1115604.679772	41.811021
3521.058477	1115195.213402	41.816026
3521.190193	1114782.711463	41.821031
3521.185399	1114378.305898	41.826036
3520.770392	1113963.923847	41.831040
3520.956254	1113549.792328	41.836045
3520.939180	1113144.055903	41.841050
3521.182824	1112735.861146	41.846055
3521.174811	1112321.953022	41.851060
3520.835673	1111923.045926	41.856064
3520.988346	1111500.366292	41.861069
3520.785482	1111099.276535	41.866074
3520.685318	1110701.766087	41.871079
3520.885562	1110284.803958	41.876084
3520.578274	1109881.445562	41.881088
3520.657990	1109487.919647	41.886093
3520.908605	1109078.968703	41.891098
3520.827134	1108659.349686	41.896103
3520.369786	1108263.054231	41.901108
3520.666225	1107858.871906	41.906112
3520.458662	1107452.164204	41.911117
3520.441163	1107051.983288	41.916122
3519.962953	1106663.117162	41.921127
3519.966650	1106245.205831	41.926132
3520.090085	1105877.290298	41.931136
3520.139911	1105481.661645	41.936141
3520.259903	1105071.568109	41.941146
3520.302044	1104664.704297	41.946151
3520.578334	1104279.936356	41.951156
3520.071133	1103880.746987	41.956160
3520.141059	1103478.853066	41.961165
3519.846067	1103088.265431	41.966170
3519.763220	1102686.433194	41.971175
3519.707444	1102289.345298	41.976180
3519.802866	1101896.217704	41.981184
3519.837132	1101518.939202	41.986189
3519.720328	1101137.835425	41.991194
3519.717360	1100740.816113	41.996199
3519.854402	1100335.617795	42.001204
3519.580534	1099956.177464	42.006208
3519.547600	1099559.458726	42.011213
3519.523315	1099162.709440	42.016218
3519.373243	1098787.565625	42.021223
3519.590842	1098400.858040	42.026228
3519.473949	1098001.265113	42.031232
3519.585071	1097606.579288	42.036237
3519.446159	1097233.812927	42.041242
3519.099563	1096839.720520	42.046247
3519.148205	1096462.564940	42.051252
3518.942279	1096082.171741	42.056256
3519.504032	1095692.726101	42.061261
3519.183012	1095303.684946	42.066266
3518.796851	1094916.923480	42.071271
3519.051843	1094538.929972	42.076276
3519.206479	1094177.677287	42.081280
3519.155186	1093784.270972	42.086285
3518.847873	1093407.152647	42.091290
3518.898369	1093022.290086	42.096295
3518.689480	1092653.911061	42.101300
3518.680632	1092268.430292	42.106304
3519.020396	1091887.173835	42.111309
3519.038539	1091511.785226	42.116314
3518.716310	1091150.409341	42.121319
3518.873590	1090749.852941	42.126324
3518.620457	1090366.480156	42.131328
3518.659262	1089999.987360	42.136333
3518.660494	1089638.457515	42.141338
3518.924095	1089250.035079	42.146343
3518.646818	1088877.099623	42.151348
3518.510060	1088500.761779	42.156352
3518.795198	1088117.620642	42.161357
3518.711019	1087743.329825	42.166362
3518.363971	1087366.948085	42.171367
3518.527771	1086992.468882	42.176372
3518.317552	1086631.348806	42.181376
3518.558487	1086240.989697	42.186381
3518.440706	1085868.588353	42.191386
3518.115096	1085507.125034	42.196391
3518.330589	1085131.454599	42.201396
3517.975951	1084777.042487	42.206400
3517.862891	1084401.088098	42.211405
3517.856555	1084038.611625	42.216410
3517.753483	1083682.168849	42.221415
3518.204279	1083302.305502	42.226420
3517.981784	1082952.931983	42.231424
3518.076385	1082579.695110	42.236429
3517.913060	1082221.727845	42.241434
3517.854584	1081845.108360	42.246439
3518.272795	1081482.583739	42.251444
3517.879062	1081131.202770	42.256448
3517.722021	1080742.146014	42.261453
3517.790925	1080391.504767	42.266458
3517.474253	1080024.686014	42.271463
3517.610624	1079663.334453	42.276468
3517.405847	1079307.390035	42.281472
3517.380434	1078965.982752	42.286477
3517.544327	1078607.052353	42.291482
3517.506507	1078235.747739	42.296487
3517.642862	1077882.918197	42.301492
3517.269070	1077541.863246	42.306496
3517.389616	1077168.539759	42.311501
3517.421162	1076799.334457	42.316506
3517.546127	1076455.920996	42.321511
3517.529231	1076110.108415	42.326516
3517.189258	1075767.496558	42.331520
3517.143745	1075409.158830	42.336525
3517.381405	1075045.660067	42.341530
3517.284409	1074699.963579	42.346535
3517.347866	1074325.878948	42.351540
3517.140220	1073977.561197	42.356544
3516.811025	1073635.294310	42.361549
3517.086916	1073303.091427	42.366554
3516.362982	1072935.671314	42.371559
3516.679836	1072593.040644	42.376564
3516.915835	1072263.760297	42.381568
3517.064273	1071901.124452	42.386573
3516.596788	1071567.400917	42.391578
3516.887176	1071220.747995	42.396583
3517.067815	1070865.535805	42.401588
3516.790147	1070523.642625	42.406592
3517.034415	1070170.393718	42.411597
3517.202487	1069807.423771	42.416602
3516.325142	1069479.313185	42.421607
3516.778375	1069123.847068	42.426612
3516.484046	1068777.135892	42.431616
3516.954665	1068429.315096	42.436621
3516.616952	1068090.165145	42.441626
3516.686637	1067747.175988	42.446631
3516.791407	1067410.508087	42.451636
3516.493200	1067075.232631	42.456640
3516.444592	1066720.944019	42.461645
3516.359465	1066392.903059	42.466650
3516.296581	1066046.847071	42.471655
3516.520172	1065703.031345	42.476660
3516.182959	1065378.820074	42.481664
3516.193648	1065038.943052	42.486669
3516.214639	1064686.725034	42.491674
3516.144916	1064336.327994	42.496679
3516.517447	1064022.410234	42.501684
3515.898332	1063688.713314	42.506688
3515.997381	1063350.257367	42.511693
3516.219989	1063022.638281	42.516698
3515.937536	1062675.924806	42.521703
3516.052921	1062336.248506	42.526708
3515.931180	1062012.380796	42.531712
3515.742710	1061665.106708	42.536717
3515.674617	1061355.057144	42.541722
3515.596544	1061028.428069	42.546727
3515.638880	1060691.262375	42.551732
3515.549529	1060373.552804	42.556736
3515.364162	1060045.438397	42.561741
3515.546971	1059723.215858	42.566746
3515.471489	1059405.737138	42.571751
3515.828241	1059073.237050	42.576756
3515.407584	1058745.083932	42.581760
3515.290018	1058424.376353	42.586765
3515.312528	1058109.408145	42.591770
3515.083533	1057792.825290	42.596775
3515.137684	1057458.350479	42.601780
3514.859892	1057154.266177	42.606784
3515.193404	1056839.656052	42.611789
3515.462257	1056515.497070	42.616794
3515.136560	1056212.428904	42.621799
3515.363379	1055879.082889	42.626804
3515.371410	1055562.525740	42.631808
3515.399988	1055243.922614	42.636813
3515.416828	1054931.665911	42.641818
3515.157450	1054610.470656	42.646823
3515.443566	1054294.469879	42.651828
3515.238205	1053973.132233	42.656832
3515.108103	1053632.863268	42.661837
3515.013622	1053315.422717	42.666842
3514.747483	1053028.660341	42.671847
3515.013045	1052709.486191	42.676852
3514.718262	1052385.081063	42.681856
3514.490239	1052069.327046	42.686861
3514.727527	1051783.188780	42.691866
3514.795940	1051470.245589	42.696871
3514.929853	1051141.066400	42.701876
3514.558656	1050838.000110	42.706880
3514.604371	1050543.435607	42.711885
3514.462270	1050233.448104	42.716890
3514.639398	1049918.855406	42.721895
3514.288931	1049615.429230	42.726900
3514.318642	1049310.476219	42.731904
3514.291758	1048996.829768	42.736909
3514.352964	1048689.907170	42.741914
3514.264445	1048391.872188	42.746919
3514.106593	1048094.315215	42.751924
3514.096231	1047801.061887	42.756928
3514.094551	1047510.011947	42.761933
3514.143292	1047210.539274	42.766938
3514.112729	1046910.966932	42.771943
3514.277554	1046606.518595	42.776948
3513.943383	1046297.694067	42.781952
3513.968612	1046004.436346	42.786957
3514.012842	1045712.125664	42.791962
3513.856251	1045412.010223	42.796967
3514.238453	1045120.675008	42.801972
3514.036587	1044816.285341	42.806977
3514.105680	1044523.231817	42.811981
3513.835699	1044223.360498	42.816986
3514.009998	1043926.780762	42.821991
3514.100212	1043644.206625	42.826996
3513.981064	1043340.301976	42.832001
3513.965897	1043054.333842	42.837005
3513.921662	1042752.606808	42.842010
3513.740267	1042461.321432	42.847015
3513.918500	1042156.819896	42.852020
3513.601713	1041863.496233	42.857025
3513.423241	1041583.470610	42.862029
3513.567084	1041292.843500	42.867034
3513.458636	1040997.893494	42.872039
3513.650304	1040708.001124	42.877044
3513.653241	1040419.767942	42.882049
3513.488147	1040121.107650	42.887053
3513.512837	1039843.377505	42.892058
3513.489042	1039578.982599	42.897063
3513.398002	1039270.403583	42.902068
3513.305193	1038979.211086	42.907073
3513.317954	1038701.909325	42.912077
3513.396347	1038418.297770	42.917082
3513.350576	1038139.817297	42.922087
3513.410193	1037869.622115	42.927092
3513.099371	1037574.136985	42.932097
3513.398335	1037286.369614	42.937101
3513.286933	1037004.071253	42.942106
3513.121823	1036718.188620	42.947111
3513.188695	1036441.248924	42.952116
3512.968837	1036159.892916	42.957121
3513.097829	1035890.460858	42.962125
3513.074325	1035605.368423	42.967130
3512.565686	1035329.242175	42.972135
3513.004777	1035046.463665	42.977140
3513.075920	1034763.054106	42.982145
3512.773534	1034501.850406	42.987149
3512.944210	1034237.556757	42.992154
3512.822758	1033950.557211	42.997159
3512.838163	1033667.294670	43.002164
3512.945905	1033395.422831	43.007169
3512.813883	1033112.349948	43.012173
3513.216486	1032847.274704	43.017178
3512.680374	1032568.015623	43.022183
3512.807276	1032297.829471	43.027188
3512.732778	1032017.789206	43.032193
3512.596426	1031734.743938	43.037197
3512.620615	1031479.347128	43.042202
3512.605748	1031215.812200	43.047207
3512.613105	1030936.575584	43.052212
3512.493207	1030664.220859	43.057217
3512.353864	1030405.315989	43.062221
3512.547310	1030121.553605	43.067226
3512.036809	1029852.516145	43.072231
3511.889630	1029608.102121	43.077236
3512.111864	1029341.824811	43.082241
3512.020604	1029094.376679	43.087245
3512.154862	1028829.057997	43.092250
3511.814007	1028566.032889	43.097255
3512.164076	1028314.215428	43.102260
3511.972380	1028055.888386	43.107265
3511.977292	1027786.569667	43.112269
3512.300593	1027528.908491	43.117274
3511.994705	1027266.494663	43.122279
3512.253728	1027000.681116	43.127284
3511.740934	1026753.101878	43.132289
3511.965859	1026493.858877	43.137293
3512.056964	1026243.928899	43.142298
3511.940225	1025997.510765	43.147303
3511.867765	1025727.136529	43.152308
3511.958019	1025470.000415	43.157313
3511.834757	1025207.653764	43.162317
3512.083506	1024952.503182	43.167322
3511.977376	1024703.409261	43.172327
3512.143010	1024453.290127	43.177332
3511.992757	1024188.379799	43.182337
3511.799689	1023913.187682	43.187341
3511.938516	1023677.871122	43.192346
3511.604600	1023402.386256	43.197351
3511.825175	1023144.831050	43.202356
3511.619805	1022920.301884	43.207361
3511.590793	1022670.038233	43.212365
3511.546156	1022405.220124	43.217370
3511.550779	1022172.286762	43.222375
3512.134633	1021900.843888	43.227380
3511.561570	1021644.611227	43.232385
3511.455915	1021390.229668	43.237389
3511.307904	1021144.476047	43.242394
3511.078586	1020926.175574	43.247399
3511.797123	1020657.172291	43.252404
3511.309856	1020425.508427	43.257409
3511.136761	1020159.926393	43.262413
3511.134040	1019922.438275	43.267418
3510.540094	1019705.702608	43.272423
3511.176875	1019448.491199	43.277428
3511.412652	1019217.240497	43.282433
3511.182852	1018970.920002	43.287437
3511.322607	1018724.721903	43.292442
3511.161631	1018473.128280	43.297447
3511.308013	1018238.455581	43.302452
3511.274671	1017996.718128	43.307457
3511.037808	1017749.665882	43.312461
3511.037129	1017507.125557	43.317466
3511.190140	1017269.596638	43.322471
3511.301854	1017035.170575	43.327476
3510.969669	1016791.392109	43.332481
3511.053756	1016548.505241	43.337485
3510.908544	1016306.033958	43.342490
3510.922037	1016077.311718	43.347495
3511.134257	1015834.372897	43.352500
3511.023019	1015602.836405	43.357505
3510.991543	1015360.888169	43.362509
3510.991007	1015109.311678	43.367514
3510.762474	1014883.299497	43.372519
3510.705995	1014640.353360	43.377524
3510.647748	1014410.215643	43.382529
3510.406765	1014176.602482	43.387533
3511.077069	1013954.192405	43.392538
3510.636095	1013708.938537	43.397543
3510.374487	1013488.606011	43.402548
3510.361214	1013243.261402	43.407553
3510.094553	1013019.803170	43.412557
3510.277039	1012817.341103	43.417562
3510.279804	1012592.461601	43.422567
3510.233296	1012342.906128	43.427572
3510.354950	1012121.194056	43.432577
3510.326919	1011904.744224	43.437581
3510.269404	1011698.006682	43.442586
3510.128574	1011457.074504	43.447591
3510.422390	1011222.181871	43.452596
3509.877386	1011027.062699	43.457601
3510.270196	1010819.927264	43.462605
3510.516723	1010575.978438	43.467610
3510.006720	1010339.918135	43.472615
3510.453607	1010123.710394	43.477620
3510.047238	1009893.348205	43.482625
3510.128770	1009674.267752	43.487629
3510.121181	1009472.591542	43.492634
3510.079629	1009251.473827	43.497639
3510.167491	1009015.940006	43.502644
3510.001676	1008809.600373	43.507649
3509.929631	1008589.919856	43.512653
3509.908701	1008381.013197	43.517658
3509.615834	1008167.865990	43.522663
3509.791533	1007945.300240	43.527668
3509.684384	1007738.620108	43.532673
3509.837956	1007534.222966	43.537677
3509.805756	1007306.124192	43.542682
3509.712636	1007082.110190	43.547687
3509.657981	1006883.460764	43.552692
3509.793742	1006663.573795	43.557697
3509.858594	1006451.469777	43.562701
3510.065068	1006249.254111	43.567706
3509.709168	1006026.408526	43.572711
3509.826086	1005795.209249	43.577716
3509.620398	1005598.970996	43.582721
3509.807478	1005374.843122	43.587725
3509.575365	1005179.761855	43.592730
3509.673059	1004967.888537	43.597735
3509.877833	1004750.931233	43.602740
3509.747842	1004553.379595	43.607745
3509.266874	1004329.223007	43.612749
3509.736639	1004117.548390	43.617754
3509.626859	1003926.295224	43.622759
3509.432967	1003703.039433	43.627764
3509.246444	1003494.757635	43.632769
3509.252716	1003296.263934	43.637773
3509.376462	1003092.294805	43.642778
3509.024334	1002899.684552	43.647783
3509.273105	1002681.083644	43.652788
3508.972949	1002494.679048	43.657793
3508.953167	1002290.899299	43.662797
3508.765777	1002082.954929	43.667802
3508.851631	1001900.457418	43.672807
3508.952995	1001694.787054	43.677812
3508.960947	1001496.035257	43.682817
3509.125474	1001287.127688	43.687821
3509.201789	1001090.005102	43.692826
3509.028111	1000921.730420	43.697831
3509.084155	1000704.350374	43.702836
3508.724249	1000505.234996	43.707841
3508.927139	1000309.427292	43.712845
3509.073422	1000103.983808	43.717850
3508.950841	999917.757153	43.722855
3508.940960	999729.363818	43.727860
3508.945191	999532.004151	43.732865
3508.917365	999326.366413	43.737869
3508.952846	999126.747964	43.742874
3508.884593	998950.996945	43.747879
3508.886885	998749.715278	43.752884
3508.712245	998551.864034	43.757889
3508.756943	998365.071874	43.762893
3508.882403	998161.119574	43.767898
3508.842908	997977.737184	43.772903
3508.917847	997784.005955	43.777908
3508.597803	997589.846163	43.782913
3508.616166	997402.442227	43.787917
3508.585792	997209.487945	43.792922
3508.596693	997030.449922	43.797927
3508.548706	996826.283366	43.802932
3508.493216	996637.405119	43.807937
3508.663471	996450.529218	43.812941
3508.529970	996263.210079	43.817946
3508.315984	996090.999055	43.822951
3508.607311	995895.803735	43.827956
3508.657115	995703.564465	43.832961
3508.494054	995513.984513	43.837965
3508.739370	995345.377776	43.842970
3508.297983	995143.943766	43.847975
3508.640681	994954.554157	43.852980
3508.393069	994779.385506	43.857985
3508.359301	994585.368064	43.862989
3508.870407	994414.935794	43.867994
3508.395468	994219.906529	43.872999
3508.589127	994031.875118	43.878004
3508.515662	993834.622346	43.883009
3508.426835	993663.584101	43.888013
3508.531054	993476.133837	43.893018
3508.432138	993298.165820	43.898023
3508.476811	993114.027529	43.903028
3508.175830	992911.906340	43.908033
3508.476638	992730.442888	43.913037
3508.616608	992566.255261	43.918042
3508.103561	992376.043272	43.923047
3508.696543	992185.447758	43.928052
3508.272528	992001.155624	43.933057
3508.185994	991814.559445	43.938061
3508.061423	991622.210754	43.943066
3508.021394	991454.998102	43.948071
3508.107597	991288.637318	43.953076
3507.967755	991091.982840	43.958081
3507.845800	990915.601715	43.963085
3508.253750	990755.413284	43.968090
3508.064006	990587.322126	43.973095
3508.205770	990379.576827	43.978100
3508.107156	990220.432012	43.983105
3507.976645	990033.492061	43.988109
3507.938065	989857.552051	43.993114
3507.455678	989691.140671	43.998119
3507.603969	989514.671603	44.003124
3507.900267	989357.681007	44.008129
3508.009377	989180.135069	44.013133
3507.933252	989005.540530	44.018138
3507.704396	988842.476734	44.023143
3507.758616	988659.558338	44.028148
3507.670399	988490.217868	44.033153
3507.406397	988325.193918	44.038157
3508.001115	988160.706681	44.043162
3507.576172	987987.309115	44.048167
3507.713361	987800.544435	44.053172
3507.861403	987650.263394	44.058177
3507.799802	987490.255587	44.063181
3507.802516	987316.767168	44.068186
3507.651156	987145.738327	44.073191
3507.844769	986955.814130	44.078196
3507.605472	986799.426744	44.083201
3507.215583	986641.205698	44.088205
3507.542461	986466.954901	44.093210
3507.650177	986301.323136	44.098215
3507.823634	986130.503109	44.103220
3507.342334	985969.643362	44.108225
3507.274858	985801.878754	44.113229
3507.565836	985631.707646	44.118234
3507.428022	985472.827012	44.123239
3507.299496	985317.844847	44.128244
3507.052130	985156.045111	44.133249
3507.282858	984998.749995	44.138253
3507.432208	984835.704437	44.143258
3507.178276	984674.380212	44.148263
3507.637890	984502.878578	44.153268
3507.451601	984345.243636	44.158273
3507.501540	984203.771977	44.163277
3507.316312	984020.353593	44.168282
3507.084611	983876.967563	44.173287
3507.491063	983698.127859	44.178292
3507.609573	983524.309691	44.183297
3507.085445	983367.582153	44.188301
3507.292374	983226.743927	44.193306
3507.359761	983052.626878	44.198311
3507.235011	982897.480687	44.203316
3507.168756	982727.867737	44.208321
3506.846562	982563.467765	44.213325
3507.101983	982414.495924	44.218330
3506.922030	982264.908269	44.223335
3506.983886	982096.232085	44.228340
3506.926317	981945.150911	44.233345
3507.056359	981810.052841	44.238349
3507.162365	981640.476894	44.243354
3506.940688	981486.480413	44.248359
3507.127746	981347.650326	44.253364
3506.696920	981194.950254	44.258369
3506.884703	981021.044483	44.263373
3506.887835	980869.143383	44.268378
3506.466599	980748.959383	44.273383
3506.765042	980585.767895	44.278388
3506.652372	980430.943475	44.283393
3506.732860	980285.657327	44.288397
3506.838278	980119.260328	44.293402
3506.404314	979991.246518	44.298407
3506.406896	979835.605376	44.303412
3506.590113	979703.575294	44.308417
3506.576560	979564.539531	44.313421
3506.748951	979398.599075	44.318426
3506.654901	979258.689729	44.323431
3506.576224	979116.722379	44.328436
3506.609052	978992.029387	44.333441
3506.414951	978831.214209	44.338445
3506.696180	978669.925320	44.343450
3506.676669	978529.790419	44.348455
3506.714045	978376.644737	44.353460
3506.733471	978252.328748	44.358465
3506.276276	978116.067324	44.363469
3506.617467	977953.771041	44.368474
3506.144727	977816.234460	44.373479
3506.420447	977662.639457	44.378484
3506.280637	977518.883176	44.383489
3506.384610	977383.098328	44.388493
3506.884644	977249.004500	44.393498
3506.384749	977125.824810	44.398503
3506.743151	976967.505512	44.403508
3506.499906	976810.258494	44.408513
3506.328965	976662.380075	44.413517
3506.714655	976530.341188	44.418522
3506.060514	976402.381048	44.423527
3506.548380	976257.316547	44.428532
3506.415147	976125.158261	44.433537
3506.448143	975970.482407	44.438541
3506.529724	975828.113759	44.443546
3506.301654	975679.241633	44.448551
3506.381559	975537.452690	44.453556
3506.202150	975421.027956	44.458561
3506.354069	975269.442539	44.463565
3506.796266	975115.165108	44.468570
3506.257363	974999.475514	44.473575
3506.416563	974851.887116	44.478580
3506.411860	974707.940216	44.483585
3506.456788	974555.766795	44.488589
3506.423488	974406.144943	44.493594
3505.947761	974292.093201	44.498599
3506.095242	974144.292918	44.503604
3506.330803	974018.871399	44.508609
3506.168898	973882.460538	44.513613
3506.326389	973732.887495	44.518618
3506.028227	973614.098200	44.523623
3506.227390	973469.010695	44.528628
3505.943430	973340.138632	44.533633
3506.062288	973224.598296	44.538637
3506.063967	973075.229400	44.543642
3505.733986	972939.312880	44.548647
3506.173829	972803.951112	44.553652
3505.847597	972678.690644	44.558657
3505.802160	972558.566107	44.563661
3506.175480	972420.760545	44.568666
3505.741653	972299.422750	44.573671
3505.973633	972150.676678	44.578676
3505.903294	972028.099248	44.583681
3505.656610	971889.796031	44.588685
3505.729398	971769.244136	44.593690
3505.439415	971647.868863	44.598695
3505.666151	971505.760336	44.603700
3505.656859	971393.922411	44.608705
3505.350468	971249.057735	44.613709
3505.643983	971137.752049	44.618714
3505.369939	971010.195933	44.623719
3505.529047	970897.048476	44.628724
3505.496864	970765.337091	44.633729
3505.430643	970642.729392	44.638733
3505.659993	970533.575514	44.643738
3505.592892	970411.648068	44.648743
3505.678846	970258.081619	44.653748
3505.328584	970150.288205	44.658753
3505.292921	970044.104762	44.663757
3505.366984	969920.969190	44.668762
3505.254564	969798.448948	44.673767
3505.292999	969691.072267	44.678772
3505.401877	969550.794449	44.683777
3505.185733	969444.629652	44.688781
3505.458834	969341.710345	44.693786
3504.965391	969222.177069	44.698791
3505.543388	969094.731713	44.703796
3505.701826	969004.159073	44.708801
3505.133482	968865.150730	44.713805
3505.436242	968737.547009	44.718810
3505.080989	968644.508074	44.723815
3505.532412	968516.091790	44.728820
3505.653564	968384.006851	44.733825
3505.079993	968278.075165	44.738829
3505.320772	968159.769465	44.743834
3505.342601	968052.071184	44.748839
3505.753746	967914.444992	44.753844
3505.432156	967809.931785	44.758849
3505.154130	967678.288018	44.763853
3505.635737	967553.468004	44.768858
3505.272489	967448.367600	44.773863
3505.143471	967345.772545	44.778868
3505.390673	967201.399993	44.783873
3505.625394	967099.132308	44.788877
3505.557870	966980.461446	44.793882
3505.461179	966873.641928	44.798887
3505.307014	966751.651150	44.803892
3505.152531	966637.002550	44.808897
3505.357424	966511.324144	44.813901
3505.704269	966376.707638	44.818906
3505.246250	966286.487530	44.823911
3505.240644	966161.227891	44.828916
3505.328306	966044.275030	44.833921
3505.189145	965932.548051	44.838925
3505.277865	965811.378800	44.843930
3505.114406	965704.450623	44.848935
3505.059626	965589.666781	44.853940
3505.047139	965487.900917	44.858945
3504.975517	965360.088038	44.863949
3505.193003	965245.056578	44.868954
3505.123009	965139.277942	44.873959
3505.089369	965024.479347	44.878964
3505.160575	964917.106062	44.883969
3504.952254	964808.895170	44.888973
3504.964097	964698.686731	44.893978
3504.736392	964583.911314	44.898983
3504.824231	964483.678602	44.903988
3504.801558	964382.972510	44.908993
3504.328727	964278.615957	44.913997
3504.856781	964155.282125	44.919002
3504.750663	964061.442167	44.924007
3504.430465	963972.142782	44.929012
3504.491531	963879.154090	44.934017
3504.692666	963749.692910	44.939021
3504.847514	963661.290246	44.944026
3504.761605	963557.738716	44.949031
3504.988775	963444.041437	44.954036
3505.033994	963328.020226	44.959041
3504.776186	963231.742090	44.964045
3504.911048	963128.538431	44.969050
3504.603537	963015.116734	44.974055
3504.925680	962919.227807	44.979060
3504.938842	962811.922829	44.984065
3504.796124	962715.715105	44.989069
3504.908566	962604.666061	44.994074
3504.503792	962514.476017	44.999079
3504.691061	962407.330828	45.004084
3504.610364	962302.089845	45.009089
3504.603221	962190.268489	45.014093
3504.713017	962103.809458	45.019098
3504.453327	962000.258558	45.024103
3504.546307	961881.456124	45.029108
3504.505097	961803.936404	45.034113
3504.480773	961714.553276	45.039117
3504.674823	961602.687385	45.044122
3504.350017	961519.721706	45.049127
3504.564189	961398.929040	45.054132
3504.706858	961281.282280	45.059137
3504.626518	961197.389511	45.064141
3504.610481	961102.310251	45.069146
3504.691567	961001.527962	45.074151
3504.640603	960889.786627	45.079156
3504.668989	960801.556992	45.084161
3504.514868	960697.475155	45.089165
3504.508520	960595.229711	45.094170
3504.230494	960520.770743	45.099175
3504.668483	960401.586900	45.104180
3504.402541	960292.810471	45.109185
3504.542091	960207.004367	45.114189
3504.538056	960106.808701	45.119194
3504.603821	960011.599949	45.124199
3504.702984	959928.835668	45.129204
3504.530160	959815.524897	45.134209
3504.609775	959709.131681	45.139213
3504.844363	959608.691969	45.144218
3504.506854	959533.543708	45.149223
3504.479460	959409.611575	45.154228
3504.799202	959314.741705	45.159233
3504.226321	959217.271744	45.164237
3504.788136	959111.376423	45.169242
3504.424697	959021.615189	45.174247
3504.307592	958940.833540	45.179252
3504.423726	958828.436395	45.184257
3504.376100	958743.325799	45.189261
3504.490141	958640.633638	45.194266
3504.276723	958547.015758	45.199271
3504.338055	958469.630470	45.204276
3504.540427	958353.973630	45.209281
3504.247550	958264.777421	45.214285
3504.325930	958165.809418	45.219290
3504.331772	958066.655516	45.224295
3504.520074	957982.769828	45.229300
3504.127028	957880.049587	45.234305
3503.464568	957793.849322	45.239309
3504.105758	957710.767807	45.244314
3503.987111	957633.302875	45.249319
3503.902588	957537.783830	45.254324
3504.401643	957445.305828	45.259329
3504.027043	957374.745581	45.264333
3504.222005	957268.680744	45.269338
3504.145287	957181.590146	45.274343
3504.140080	957081.538343	45.279348
3504.229094	956997.164240	45.284353
3504.154598	956912.913931	45.289357
3504.468942	956799.758000	45.294362
3503.883829	956731.284592	45.299367
3504.236806	956634.403278	45.304372
3504.248216	956555.234775	45.309377
3503.867463	956477.993722	45.314381
3504.386051	956371.270501	45.319386
3504.067988	956285.285288	45.324391
3503.993238	956204.360273	45.329396
3504.084532	956109.671618	45.334401
3504.036114	956026.090843	45.339405
3504.005048	955950.845449	45.344410
3503.666365	955851.023489	45.349415
3503.822531	955765.192377	45.354420
3503.891083	955688.301658	45.359425
3503.836738	955606.840086	45.364429
3504.130108	955515.661782	45.369434
3504.013117	955445.491729	45.374439
3503.536788	955354.628569	45.379444
3503.745710	955287.845283	45.384449
3503.611463	955198.739959	45.389453
3503.626898	955117.067792	45.394458
3503.552678	955050.041126	45.399463
3503.574922	954983.858407	45.404468
3503.593533	954886.593431	45.409473
3503.759304	954810.055986	45.414477
3503.645061	954732.128913	45.419482
3503.655609	954651.980337	45.424487
3503.667852	954569.917359	45.429492
3503.966408	954503.874184	45.434497
3503.586050	954418.525880	45.439501
3503.410455	954330.655581	45.444506
3503.443174	954274.409271	45.449511
3503.430573	954205.161424	45.454516
3503.575457	954123.356364	45.459521
3503.748202	954052.258535	45.464525
3503.809603	953974.769221	45.469530
3503.452880	953893.138745	45.474535
3503.630770	953806.731694	45.479540
3503.694032	953736.221442	45.484545
3503.366226	953674.479691	45.489549
3503.487165	953578.320834	45.494554
3503.319353	953520.472997	45.499559
3503.248145	953454.764146	45.504564
3503.487798	953368.530839	45.509569
3503.367482	953312.873137	45.514573
3503.586102	953234.007356	45.519578
3503.341221	953160.956878	45.524583
3503.368719	953071.787754	45.529588
3503.531495	953015.793175	45.534593
3503.389704	952972.094317	45.539597
3503.685223	952877.328616	45.544602
3503.728361	952796.475821	45.549607
3503.377048	952716.452142	45.554612
3503.764958	952644.055474	45.559617
3503.624056	952581.695653	45.564621
3503.597508	952490.133283	45.569626
3503.635320	952435.970903	45.574631
3503.501160	952356.862661	45.579636
3503.268226	952284.658857	45.584641
3503.438313	952228.367404	45.589645
3503.483086	952140.136069	45.594650
3503.297246	952075.959403	45.599655
3503.522810	952014.010755	45.604660
3503.655496	951939.253893	45.609665
3503.281713	951872.043470	45.614669
3503.734391	951789.384833	45.619674
3503.319469	951719.499718	45.624679
3503.338963	951648.010932	45.629684
3503.416640	951576.894362	45.634689
3503.512934	951505.008136	45.639693
3503.571096	951440.591921	45.644698
3503.088449	951366.502269	45.649703
3503.156774	951307.920598	45.654708
3503.487929	951233.312164	45.659713
3503.363429	951161.457491	45.664717
3503.510124	951091.279892	45.669722
3503.492976	951038.068875	45.674727
3503.120491	950948.641545	45.679732
3503.091929	950870.258649	45.684737
3502.823014	950817.948229	45.689741
3503.412194	950751.904494	45.694746
3503.021038	950676.066933	45.699751
3503.181105	950600.328894	45.704756
3503.276583	950543.074067	45.709761
3503.405297	950472.699541	45.714765
3503.304828	950406.573525	45.719770
3503.184374	950341.981504	45.724775
3503.113725	950290.781722	45.729780
3503.276221	950226.715986	45.734785
3503.090695	950159.452107	45.739789
3503.322414	950066.942407	45.744794
3503.068624	950014.908497	45.749799
3503.352560	949957.616110	45.754804
3503.639842	949893.621403	45.759809
3502.968736	949826.433145	45.764813
3503.350930	949724.797984	45.769818
3503.188405	949609.943279	45.774823
3503.128667	949417.425033	45.779828
3503.268175	949178.143996	45.784833
3503.090170	948883.561346	45.789837
3503.467220	948513.032098	45.794842
3503.119030	948085.616362	45.799847
3502.364500	947587.551903	45.804852
3502.664498	947037.159730	45.809857
3502.687290	946424.296761	45.814861
3502.908097	945730.275943	45.819866
3502.574770	944983.743584	45.824871
3502.353033	944177.571443	45.829876
3503.010192	943292.147539	45.834881
3502.022855	942320.081900	45.839885
3501.982398	941284.008881	45.844890
3501.994019	940183.079218	45.849895
3501.867914	938989.655576	45.854900
3501.753134	937726.488180	45.859905
3501.423811	936386.942225	45.864909
3501.479199	934957.421030	45.869914
3501.005512	933476.992339	45.874919
3500.904364	931891.384471	45.879924
3500.521394	930213.104505	45.884929
3499.900499	928472.338004	45.889933
3499.871969	926653.600711	45.894938
3499.619391	924749.062860	45.899943
3499.201208	922747.272067	45.904948
3499.074829	920685.204805	45.909953
3498.842566	918522.608625	45.914957
3498.766006	916252.484660	45.919962
3498.319169	913934.256701	45.924967
3497.984367	911522.085661	45.929972
3497.409499	908989.962784	45.934977
3497.031714	906382.342606	45.939981
3496.548357	903713.273198	45.944986
3496.064302	900978.019828	45.949991
3495.550225	898126.626673	45.954996
3495.571209	895177.207536	45.960001
3494.727547	892178.614034	45.965005
3494.815154	889074.433682	45.970010
3494.073640	885898.310194	45.975015
3493.606230	882609.349602	45.980020
3493.025433	879261.352354	45.985025
3492.251285	875849.102462	45.990029
3492.082213	872322.181698	45.995034
3491.321994	868706.730244	46.000039
3490.960683	865014.008788	46.005044
3490.460667	861258.182480	46.010049
3489.772757	857388.069725	46.015053
3489.127511	853442.292501	46.020058
3488.463509	849443.052874	46.025063
3487.835959	845308.990184	46.030068
3487.067405	841105.559253	46.035073
3486.329752	836840.382327	46.040077
3485.749532	832481.735925	46.045082
3485.316086	828033.030342	46.050087
3484.668634	823511.635213	46.055092
3484.091734	818888.014819	46.060097
3482.866342	814191.843101	46.065101
3482.534702	809397.944678	46.070106
3481.400820	804540.523196	46.075111
3480.664606	799588.701293	46.080116
3480.158533	794544.899787	46.085121
3478.966797	789435.365979	46.090125
3478.324927	784207.453020	46.095130
3477.231057	778923.492439	46.100135
3476.277471	773558.037726	46.105140
3475.543505	768104.143571	46.110145
3474.389844	762550.868954	46.115149
3473.489915	756915.911493	46.120154
3472.860244	751224.148248	46.125159
3471.824105	745444.025296	46.130164
3470.724412	739543.976763	46.135169
3469.714462	733573.744194	46.140173
3468.746153	727529.182039	46.145178
3467.726325	721421.219806	46.150183
3466.592100	715182.942028	46.155188
3465.615858	708875.530756	46.160193
3464.334850	702487.056255	46.165197
3463.259567	696002.809572	46.170202
3462.052473	689434.266404	46.175207
3460.985457	682807.733892	46.180212
3459.747584	676093.113462	46.185217
3458.712677	669280.364469	46.190221
3457.426871	662374.884461	46.195226
3456.148190	655404.704469	46.200231
3454.776141	648357.653321	46.205236
3453.430406	641221.743372	46.210241
3452.107727	633996.693132	46.215245
3450.770776	626698.612680	46.220250
3449.309322	619310.536032	46.225255
3447.992757	611851.010717	46.230260
3446.482640	604323.930616	46.235265
3444.955108	596711.017945	46.240269
3443.715191	589005.793356	46.245274
3442.501479	581232.791633	46.250279
3440.810243	573357.118800	46.255284
3439.124058	565429.144117	46.260289
3437.472550	557404.308572	46.265293
3435.754296	549301.600263	46.270298
3434.137220	541145.109430	46.275303
3432.203350	532879.383071	46.280308
3431.145950	524561.762113	46.285313
3428.784743	516165.941020	46.290317
3427.201057	507688.773985	46.295322
3425.091616	499171.934360	46.300327
3423.674031	490540.420824	46.305332
3421.751649	481829.058715	46.310337
3419.922055	473082.534137	46.315341
3418.078522	464233.684712	46.320346
3415.606441	455334.873163	46.325351
3413.374442	446375.013090	46.330356
3411.846704	437323.891035	46.335361
3409.408656	428229.009789	46.340365
3407.404596	419043.923517	46.345370
3405.241909	409812.208432	46.350375
3402.988276	400503.055110	46.355380
3400.997040	391114.294084	46.360385
3398.395677	381693.514291	46.365389
3396.086855	372213.308034	46.370394
3393.813980	362659.484111	46.375399
3391.358054	353060.658545	46.380404
3388.783042	343387.082448	46.385409
3385.958860	333666.951569	46.390413
3383.909849	323889.809521	46.395418
3380.982504	314073.290691	46.400423
3377.904514	304193.810646	46.405428
3375.639575	294289.240567	46.410433
3372.446283	284321.312663	46.415437
3369.835203	274313.641491	46.420442
3366.644598	264269.128746	46.425447
3363.480508	254152.774128	46.430452
3360.332431	244035.047032	46.435457
3357.016215	233864.255139	46.440461
3354.022461	223653.901356	46.445466
3350.438730	213361.631507	46.450471
3346.674469	203103.745841	46.455476
3343.238888	192810.401074	46.460481
3339.520069	182521.810131	46.465485
3335.715064	172221.247522	46.470490
3331.582854	161891.897590	46.475495
3327.148326	151566.943318	46.480500
3322.856663	141232.215914	46.485505
3318.421504	130927.895632	46.490509
3313.919570	120580.889906	46.495514
3308.680391	110290.969720	46.500519
3303.099831	100027.535523	46.505524
3297.494834	89772.694429	46.510529
3291.340643	79599.844842	46.515533
3284.572754	69431.827389	46.520538
3276.169306	59388.729274	46.525543
3266.646740	49462.838025	46.530548
3245.136556	39966.036910	46.535553
3196.394749	31473.001731	46.540557
3142.975383	23650.246394	46.545562
3091.572719	16636.268704	46.550567
3045.001630	10465.675807	46.555572
3002.546587	5219.874479	46.560577
2955.851574	1176.361732	46.565581
2831.778115	350.768000	46.570586
2741.363238	346.809686	46.575591
2721.987761	318.619913	46.580596
2753.131722	295.478418	46.585601
2804.858676	320.743986	46.590605
2853.839859	304.135119	46.595610
2886.864451	310.042274	46.600615
2901.789603	326.779733	46.605620
2902.925451	292.342065	46.610625
2896.412139	275.213999	46.615629
2887.353057	286.137284	46.620634
2879.450412	305.516021	46.625639
2873.932579	297.626088	46.630644
2871.416808	288.194565	46.635649
2869.549814	305.602240	46.640653
2868.155858	282.903560	46.645658
2866.924692	272.909469	46.650663
2864.156835	285.774093	46.655668
2861.554799	275.953617	46.660673
2858.673531	291.021668	46.665677
2855.802034	261.816512	46.670682
2852.794482	264.208306	46.675687
2849.366299	284.749008	46.680692
2846.810591	264.106395	46.685697
2843.574293	268.473802	46.690701
2840.486051	267.169532	46.695706
2837.686556	268.509843	46.700711
2834.295616	257.368987	46.705716
2830.807744	275.384689	46.710721
2827.375648	270.482787	46.715725
2823.979062	249.188642	46.720730
2821.278682	251.290873	46.725735
2818.029831	269.002978	46.730740
2815.135270	259.448877	46.735745
2811.718206	273.894377	46.740749
2808.026077	270.716070	46.745754
2804.998955	265.934160	46.750759
2801.550451	262.584191	46.755764
2798.463868	264.014562	46.760769
2794.933422	263.975213	46.765773
2791.508870	250.566125	46.770778
2788.209804	256.713790	46.775783
2784.788381	260.485009	46.780788
2781.859043	246.962915	46.785793
2778.238237	257.931318	46.790797
2774.644904	267.284332	46.795802
2771.520675	259.094280	46.800807
2767.764221	265.668463	46.805812
2765.083530	249.360028	46.810817
2761.076981	253.886317	46.815821
2758.007370	256.056646	46.820826
2754.519722	235.692664	46.825831
2750.864075	249.794731	46.830836
2747.904966	247.788126	46.835841
2744.435319	249.573383	46.840845
2741.362211	258.340868	46.845850
2737.706897	240.855738	46.850855
2733.881004	233.233028	46.855860
2730.357537	249.810548	46.860865
2727.145461	249.005890	46.865869
2723.385074	235.699183	46.870874
2720.357018	247.342797	46.875879
2716.367677	240.922069	46.880884
2713.318827	242.483571	46.885889
2710.266543	234.890868	46.890893
2706.860402	221.760665	46.895898
2703.153951	229.010263	46.900903
2699.233347	243.439646	46.905908
2696.241084	224.050984	46.910913
2692.755226	251.986457	46.915917
2689.382630	233.014454	46.920922
2685.678011	233.788934	46.925927
2682.023791	236.619862	46.930932
2679.623374	238.001066	46.935937
2676.174821	235.894957	46.940941
2672.252800	233.450810	46.945946
2668.724733	226.054565	46.950951
2665.367112	240.972479	46.955956
2661.882668	215.500133	46.960961
2658.275774	238.508130	46.965965
2654.533449	221.949744	46.970970
2650.601644	226.009863	46.975975
2647.312744	231.148179	46.980980
2644.496504	218.955986	46.985985
2641.183498	236.544805	46.990989
2637.661525	225.816640	46.995994
2634.510452	234.480789	47.000999
2630.594191	232.719066	47.006004
2627.189137	222.543409	47.011009
2623.769578	235.815597	47.016013
2620.329066	226.224372	47.021018
2617.015500	223.986040	47.026023
2612.971816	217.863488	47.031028
2609.386002	223.704826	47.036033
2605.769233	219.422740	47.041037
2602.629176	209.443624	47.046042
2599.791520	216.934245	47.051047
2595.793738	227.388438	47.056052
2592.655820	217.255172	47.061057
2588.658006	218.829660	47.066061
2585.678697	218.766415	47.071066
2581.892735	216.704251	47.076071
2578.186375	222.079625	47.081076
2575.112786	210.852092	47.086081
2571.374519	210.166528	47.091085
2568.205042	226.266138	47.096090
2564.582900	220.543086	47.101095
2560.760017	226.290062	47.106100
2558.003718	227.715878	47.111105
2554.056320	210.394983	47.116109
2550.652878	203.512849	47.121114
2547.125285	219.491275	47.126119
2543.260453	217.234873	47.131124
2540.324111	206.213302	47.136129
2536.480900	234.187372	47.141133
2532.941045	210.579484	47.146138
2530.201615	209.985229	47.151143
2526.226142	217.213160	47.156148
2523.065855	202.875803	47.161153
2519.259678	219.411382	47.166157
2515.445652	226.895726	47.171162
2512.188545	213.820876	47.176167
2508.622861	209.306681	47.181172
2505.487925	215.482513	47.186177
2501.556391	210.295779	47.191181
2498.153697	207.117664	47.196186
2495.008367	189.863745	47.201191
2491.025778	213.693992	47.206196
2488.263634	195.958998	47.211201
2484.113354	208.217724	47.216205
2480.689461	200.222971	47.221210
2477.393314	198.787215	47.226215
2473.726499	224.766984	47.231220
2470.504349	206.140482	47.236225
2466.652214	211.561643	47.241229
2463.845622	197.748033	47.246234
2460.327836	193.386178	47.251239
2456.010751	210.652277	47.256244
2453.185963	186.675695	47.261249
2449.423394	195.624313	47.266253
2446.202802	216.238408	47.271258
2442.451426	207.710314	47.276263
2438.949694	194.283533	47.281268
2435.377460	190.704579	47.286273
2431.874297	189.848814	47.291277
2428.706848	202.449084	47.296282
2425.214854	194.411437	47.301287
2421.273918	216.213599	47.306292
2418.147828	199.447326	47.311297
2414.626667	207.728738	47.316301
2411.407962	203.474731	47.321306
2407.782181	203.787484	47.326311
2404.324850	220.395294	47.331316
2400.461275	196.392348	47.336321
2396.808278	195.927202	47.341325
2393.611170	213.403421	47.346330
2390.224965	192.491587	47.351335
2386.302408	205.766179	47.356340
2383.074258	185.803941	47.361345
2379.457868	204.363619	47.366349
2375.944536	213.292184	47.371354
2372.699234	204.614872	47.376359
2369.355107	194.656816	47.381364
2365.871280	189.030834	47.386369
2362.169981	185.160189	47.391373
2358.599055	198.325792	47.396378
2355.192036	184.744254	47.401383
2351.360688	197.534237	47.406388
2348.193766	203.217212	47.411393
2344.704562	193.791638	47.416397
2341.273672	201.874501	47.421402
2337.854548	181.947049	47.426407
2334.433550	181.704107	47.431412
2331.044011	194.982053	47.436417
2327.120390	180.914358	47.441421
2323.791814	183.342214	47.446426
2320.292850	187.049645	47.451431
2316.120417	182.659799	47.456436
2313.034653	192.253390	47.461441
2309.801253	195.516707	47.466445
2306.272216	178.518468	47.471450
2302.812526	191.903089	47.476455
2299.347001	184.817955	47.481460
2296.091922	169.792232	47.486465
2291.886339	181.661988	47.491469
2288.419456	175.446391	47.496474
2285.182368	190.765915	47.501479
2281.445748	199.837679	47.506484
2278.275975	172.683402	47.511489
2274.915074	196.891175	47.516493
2271.370645	173.761556	47.521498
2267.999668	181.151109	47.526503
2264.319332	188.413530	47.531508
2261.214433	181.339473	47.536513
2257.276096	188.480395	47.541517
2253.424816	174.691150	47.546522
2250.347051	194.073635	47.551527
2246.818530	181.035643	47.556532
2243.518120	170.817229	47.561537
2239.656658	175.474498	47.566541
2235.969290	188.780679	47.571546
2232.633370	173.660795	47.576551
2228.955543	196.617491	47.581556
2226.074487	184.831123	47.586561
2222.283087	187.515692	47.591565
2218.701818	179.675098	47.596570
2215.500238	173.267806	47.601575
2211.689516	188.248695	47.606580
2208.729411	163.255644	47.611585
2204.495958	177.557503	47.616589
2201.148664	198.641380	47.621594
2197.706134	181.857215	47.626599
2193.962417	182.705954	47.631604
2190.720301	183.017184	47.636609
2187.245034	193.125002	47.641613
2183.325981	170.827500	47.646618
2180.185858	179.110457	47.651623
2176.820551	183.033254	47.656628
2173.528288	174.119257	47.661633
2170.292052	181.744592	47.666637
2166.237931	182.617812	47.671642
2162.689281	175.054106	47.676647
2159.062064	190.070350	47.681652
2155.783470	175.151080	47.686657
2152.379724	191.703235	47.691661
2148.940733	178.732020	47.696666
2145.065769	166.442586	47.701671
2141.563228	184.448849	47.706676
2138.440548	161.350400	47.711681
2135.047346	169.763009	47.716685
2131.686013	175.853976	47.721690
2127.904293	174.143241	47.726695
2124.495822	197.697348	47.731700
2120.746727	172.921990	47.736705
2117.063211	184.239785	47.741709
2113.739211	185.944170	47.746714
2110.484272	172.690576	47.751719
2106.417316	184.442745	47.756724
2103.268660	166.933150	47.761729
2099.587693	177.822783	47.766733
2096.331775	165.499531	47.771738
2092.773511	170.452916	47.776743
2088.995953	185.700548	47.781748
2086.054855	179.214442	47.786753
2082.558934	170.026308	47.791757
2078.787429	179.972605	47.796762
2075.055358	173.881759	47.801767
2071.655713	173.531934	47.806772
2068.276486	177.608596	47.811777
2064.959204	164.118301	47.816781
2061.305077	165.147751	47.821786
2057.762616	174.283451	47.826791
2054.027767	188.839820	47.831796
2050.943887	160.020168	47.836801
2047.305018	176.343289	47.841805
2043.852191	175.705512	47.846810
2040.445941	158.641540	47.851815
2036.837871	175.024790	47.856820
2033.273547	157.627916	47.861825
2029.893695	175.873507	47.866829
2026.121964	161.856839	47.871834
2022.929064	163.579192	47.876839
2019.328933	172.449484	47.881844
2015.811168	161.237061	47.886849
2012.358247	187.746249	47.891853
2008.719956	168.053875	47.896858
2005.608577	150.651755	47.901863
2001.379424	164.805692	47.906868
1998.272652	167.610927	47.911873
1994.913101	164.566230	47.916877
1991.302525	179.003660	47.921882
1987.808107	162.971141	47.926887
1984.130345	186.838801	47.931892
1980.787514	179.385271	47.936897
1977.493064	159.553635	47.941901
1974.027709	182.806785	47.946906
1970.516268	151.169487	47.951911
1966.090478	151.695131	47.956916
1962.958789	166.049903	47.961921
1959.586630	160.161077	47.966925
1956.238431	165.384393	47.971930
1952.907955	162.974069	47.976935
1949.411421	162.953499	47.981940
1946.309253	164.197065	47.986945
1942.366418	159.653961	47.991949
1938.386915	163.470228	47.996954
1935.491993	165.241122	48.001959
1931.412068	174.405066	48.006964
1927.797336	168.066676	48.011969
1924.869853	176.169029	48.016973
1921.275023	159.086035	48.021978
1917.984138	160.270387	48.026983
1914.222042	157.550211	48.031988
1911.004459	159.601930	48.036993
1907.471654	154.610708	48.041997
1903.667881	162.038057	48.047002
1900.472231	164.442384	48.052007
1896.832775	155.792700	48.057012
1893.647474	156.087880	48.062017
1889.677774	164.619663	48.067021
1886.146917	149.930722	48.072026
1882.479010	153.872880	48.077031
1879.141168	158.454777	48.082036
1875.562091	155.945328	48.087041
1872.309198	157.905325	48.092045
1868.644883	166.933842	48.097050
1865.385332	154.265566	48.102055
1861.500503	158.508595	48.107060
1858.205796	166.209578	48.112065
1854.932632	155.515058	48.117069
1851.296769	146.767249	48.122074
1848.083867	143.059880	48.127079
1844.325477	168.411015	48.132084
1840.838667	170.642630	48.137089
1837.285423	163.858020	48.142093
1833.662849	168.492343	48.147098
1830.256941	159.551423	48.152103
1826.718843	153.028212	48.157108
1823.099420	153.650354	48.162113
1819.455460	138.359331	48.167117
1815.773495	162.185664	48.172122
1812.886093	142.633555	48.177127
1808.898359	156.971373	48.182132
1805.472769	162.293739	48.187137
1802.322993	152.637989	48.192141
1798.712202	156.141343	48.197146
1795.542218	146.555622	48.202151
1791.446875	136.081056	48.207156
1788.359096	143.443481	48.212161
1785.045379	159.936264	48.217165
1781.391020	155.907068	48.222170
1777.811121	164.155880	48.227175
1774.163818	157.824435	48.232180
1770.691785	131.988606	48.237185
1766.909278	149.908054	48.242189
1763.494773	140.715963	48.247194
1760.403539	152.736780	48.252199
1756.665978	149.643499	48.257204
1753.272928	152.983886	48.262209
1749.426578	158.337622	48.267213
1745.850310	154.875420	48.272218
1742.610909	155.998577	48.277223
1739.129423	159.353465	48.282228
1735.781605	139.961723	48.287233
1732.420856	146.387556	48.292237
1728.632461	136.661342	48.297242
1725.195317	150.014775	48.302247
1721.458292	163.777476	48.307252
1718.073825	148.492228	48.312257
1714.366732	150.147441	48.317261
1711.047805	168.500251	48.322266
1707.898091	141.725498	48.327271
1704.306867	159.457647	48.332276
1700.649094	144.389063	48.337281
1697.213165	139.282538	48.342285
1693.366153	159.932711	48.347290
1690.177181	137.870505	48.352295
1686.718935	158.330946	48.357300
1682.837859	147.876432	48.362305
1679.394812	152.936166	48.367309
1676.275719	152.119101	48.372314
1673.070147	147.441085	48.377319
1669.436563	158.233185	48.382324
1665.704960	130.924038	48.387329
1661.826132	149.348712	48.392333
1658.146045	142.903189	48.397338
1655.092323	141.908829	48.402343
1651.560675	154.268510	48.407348
1648.283159	149.055764	48.412353
1644.859790	154.273557	48.417357
1641.197873	132.265566	48.422362
1637.536200	147.506925	48.427367
1633.947714	142.474637	48.432372
1630.490398	145.206956	48.437377
1626.805668	130.879199	48.442381
1623.473196	139.364138	48.447386
1619.735780	136.648343	48.452391
1616.509344	150.305802	48.457396
1613.119350	129.842095	48.462401
1610.051045	136.495831	48.467405
1606.131962	133.847215	48.472410
1602.692135	140.988329	48.477415
1598.756075	155.035863	48.482420
1595.430332	133.028461	48.487425
1591.959764	155.219183	48.492429
1588.655027	139.251636	48.497434
1585.353830	115.512975	48.502439
1581.646376	142.452159	48.507444
1578.084649	129.216205	48.512449
1574.706311	135.662559	48.517453
1570.846895	149.856671	48.522458
1567.761738	135.300674	48.527463
1563.886240	152.611587	48.532468
1560.461448	129.725717	48.537473
1556.759465	145.839003	48.542477
1553.373722	143.963502	48.547482
1550.138208	137.751178	48.552487
1546.456263	141.389602	48.557492
1543.082418	132.090608	48.562497
1539.848810	136.080910	48.567501
1535.929366	160.254880	48.572506
1532.519915	143.611145	48.577511
1528.849596	145.001430	48.582516
1525.511408	149.163780	48.587521
1522.266064	137.938680	48.592525
1518.292066	139.209116	48.597530
1514.670196	143.595362	48.602535
1511.268601	138.939916	48.607540
1507.977912	152.785977	48.612545
1504.832519	143.810644	48.617549
1501.020144	132.162718	48.622554
1497.508629	117.476101	48.627559
1494.145730	125.926940	48.632564
1490.575139	145.014125	48.637569
1486.784899	140.274960	48.642573
1483.389672	142.113109	48.647578
1480.265181	139.853303	48.652583
1476.451138	132.769942	48.657588
1473.006416	136.444025	48.662593
1469.441643	124.555695	48.667597
1465.726164	135.189136	48.672602
1462.380870	141.378828	48.677607
1458.583166	138.137707	48.682612
1455.480397	142.274055	48.687617
1452.170020	160.270084	48.692621
1448.422125	137.693604	48.697626
1445.141892	130.586973	48.702631
1441.539162	144.516314	48.707636
1438.195044	121.501714	48.712641
1434.377031	139.258631	48.717645
1430.671429	143.026793	48.722650
1427.420293	134.757134	48.727655
1424.016064	147.583089	48.732660
1420.335538	134.533656	48.737665
1417.213095	146.933504	48.742669
1413.012385	145.071740	48.747674
1409.829831	116.945662	48.752679
1406.046239	139.332100	48.757684
1402.702861	159.515398	48.762689
1399.534606	146.069292	48.767693
1395.871100	148.727634	48.772698
1392.343174	133.083040	48.777703
1388.795389	137.088762	48.782708
1385.701705	134.997932	48.787713
1382.136927	129.771881	48.792717
1378.475198	139.453707	48.797722
1375.177019	130.485324	48.802727
1371.303748	128.463397	48.807732
1367.647400	129.763462	48.812737
1364.471454	121.668177	48.817741
1360.685843	131.574458	48.822746
1357.410467	129.278849	48.827751
1353.658426	133.217088	48.832756
1350.370018	121.808226	48.837761
1346.699726	138.283715	48.842765
1343.461672	132.059591	48.847770
1340.225192	137.058737	48.852775
1336.389903	138.268004	48.857780
1332.873873	131.003650	48.862785
1329.391118	123.322545	48.867789
1325.775922	148.305369	48.872794
1322.432952	135.446213	48.877799
1318.633277	141.209733	48.882804
1315.185245	134.929724	48.887809
1311.776649	128.543279	48.892813
1308.315696	141.477972	48.897818
1305.129508	126.519858	48.902823
1300.928046	156.250251	48.907828
1297.830789	132.827620	48.912833
1294.363996	137.398590	48.917837
1290.791714	124.414940	48.922842
1287.182269	129.952931	48.927847
1283.769780	134.781193	48.932852
1280.239157	133.740736	48.937857
1277.042055	118.058398	48.942861
1273.133251	132.225548	48.947866
1269.920573	143.714817	48.952871
1266.002938	137.309236	48.957876
1262.861956	139.791816	48.962881
1259.231032	136.979036	48.967885
1255.781886	128.012264	48.972890
1252.440101	135.777960	48.977895
1248.510241	140.514668	48.982900
1245.112326	123.655572	48.987905
1241.729807	145.423234	48.992909
1237.947308	143.366175	48.997914
1234.935538	137.503194	49.002919
1231.341626	150.091122	49.007924
1227.923643	126.736490	49.012929
1224.445003	140.858010	49.017933
1220.824917	140.745046	49.022938
1217.369660	122.622970	49.027943
1213.620011	141.944984	49.032948
1210.446609	132.379102	49.037953
1206.742961	136.186018	49.042957
1202.889597	144.998997	49.047962
1199.761737	134.670645	49.052967
1195.737455	144.470014	49.057972
1192.560245	117.275249	49.062977
1189.391019	126.156995	49.067981
1185.549774	138.887568	49.072986
1182.293924	116.298169	49.077991
1178.795277	138.280923	49.082996
1175.198097	138.157099	49.088001
1171.875364	123.444460	49.093005
1168.084130	135.826150	49.098010
1164.815023	136.545574	49.103015
1161.000697	129.070235	49.108020
1157.754195	128.940515	49.113025
1154.273074	124.132175	49.118029
1150.724742	142.558396	49.123034
1147.221775	131.827468	49.128039
1143.434315	128.756393	49.133044
1139.855158	134.564781	49.138049
1136.726487	125.140519	49.143053
1133.181942	129.515953	49.148058
1129.804366	124.577777	49.153063
1126.161587	135.000584	49.158068
1122.699725	127.271659	49.163073
1119.222862	131.122956	49.168077
1115.385018	136.572368	49.173082
1112.402497	119.764250	49.178087
1108.502256	142.418438	49.183092
1104.954048	147.732245	49.188097
1101.914268	125.599472	49.193101
1097.889315	125.705532	49.198106
1094.809929	130.011981	49.203111
1090.899060	132.867177	49.208116
1087.592827	121.512320	49.213121
1084.097729	136.514077	49.218125
1080.319113	122.569275	49.223130
1077.351039	128.243950	49.228135
1073.841228	137.879516	49.233140
1070.300068	115.485474	49.238145
1066.718350	117.766956	49.243149
1062.893946	124.584590	49.248154
1059.474738	129.477195	49.253159
1056.095249	125.711807	49.258164
1052.324910	119.659480	49.263169
1049.427584	124.991323	49.268173
1045.514524	127.863478	49.273178
1042.186881	100.905295	49.278183
1038.568878	122.952855	49.283188
1035.052636	123.009980	49.288193
1031.846653	112.144776	49.293197
1027.615635	132.527372	49.298202
1024.503524	117.654579	49.303207
1021.069221	125.734444	49.308212
1017.489897	134.816749	49.313217
1014.326507	122.077304	49.318221
1010.555772	142.798542	49.323226
1007.269862	117.471517	49.328231
1003.271695	117.527931	49.333236
1000.167650	120.968315	49.338241
996.495120	121.546774	49.343245
992.955273	123.618659	49.348250
989.684413	111.972936	49.353255
985.989129	118.122649	49.358260
982.431835	119.480052	49.363265
978.736708	126.585546	49.368269
975.362374	124.662491	49.373274
971.974162	126.999375	49.378279
968.348984	132.134868	49.383284
965.370018	117.890119	49.388289
961.782859	122.726844	49.393293
957.995463	112.407814	49.398298
954.699841	124.329240	49.403303
951.219553	111.631810	49.408308
947.693680	117.356610	49.413313
943.845984	136.066413	49.418317
940.385538	135.708142	49.423322
937.098657	115.290356	49.428327
933.463366	128.406177	49.433332
929.814101	118.163692	49.438337
926.343561	114.246501	49.443341
922.925750	137.489127	49.448346
919.367009	116.955347	49.453351
915.490343	123.170954	49.458356
912.409409	120.591321	49.463361
909.407084	128.727358	49.468365
905.647829	121.156087	49.473370
902.160975	112.014352	49.478375
898.587859	126.264824	49.483380
894.829569	107.948584	49.488385
891.505749	106.586136	49.493389
887.987878	110.188515	49.498394
884.131835	135.813647	49.503399
880.692952	116.927551	49.508404
877.289961	110.063968	49.513409
873.767924	111.901347	49.518413
870.358701	121.748057	49.523418
867.073339	101.504894	49.528423
863.436147	111.824874	49.533428
860.053198	122.618807	49.538433
856.642665	100.502283	49.543437
852.810514	126.120898	49.548442
849.128004	110.848977	49.553447
845.615445	131.926948	49.558452
842.032546	110.094186	49.563457
838.694447	120.005122	49.568461
835.044227	129.929628	49.573466
832.204671	103.379214	49.578471
828.570152	117.164264	49.583476
824.837251	127.340365	49.588481
821.620068	120.805302	49.593485
818.026720	114.108335	49.598490
814.349679	131.621714	49.603495
810.454413	118.340936	49.608500
807.356548	120.140560	49.613505
803.920007	120.056403	49.618509
800.384968	114.622274	49.623514
797.100073	121.505230	49.628519
793.445330	114.723516	49.633524
789.828860	123.880214	49.638529
786.334370	125.473573	49.643533
782.599496	131.979437	49.648538
779.348425	120.689942	49.653543
775.848441	117.447515	49.658548
772.299161	123.061537	49.663553
769.079660	116.532610	49.668557
765.056987	121.184573	49.673562
761.721097	109.436879	49.678567
758.386144	106.952938	49.683572
754.548697	112.560397	49.688577
751.332610	106.328739	49.693581
748.193944	112.663052	49.698586
744.449977	119.422575	49.703591
740.598972	122.615416	49.708596
737.345458	114.611028	49.713601
733.798330	124.565999	49.718605
730.055090	121.228525	49.723610
726.686147	97.859315	49.728615
723.256514	103.509527	49.733620
719.918297	115.748313	49.738625
716.422173	107.182654	49.743629
712.296284	129.563483	49.748634
709.292370	116.750541	49.753639
705.614284	101.777989	49.758644
702.227361	121.127355	49.763649
698.702005	108.316399	49.768653
695.260012	111.396630	49.773658
692.135179	117.543029	49.778663
688.394347	126.989522	49.783668
684.873963	113.164638	49.788673
681.409457	114.848588	49.793677
677.301657	120.054459	49.798682
674.327166	96.131346	49.803687
670.822838	109.243877	49.808692
667.128081	107.777771	49.813697
663.705535	106.870234	49.818701
660.286624	127.494892	49.823706
656.840033	101.335088	49.828711
653.283566	106.917400	49.833716
649.543666	112.047033	49.838721
646.180310	98.778472	49.843725
642.503201	114.815648	49.848730
639.311302	92.070023	49.853735
636.005266	112.973350	49.858740
631.949929	97.548027	49.863745
628.655550	111.741504	49.868749
624.836278	126.040038	49.873754
621.747748	114.206590	49.878759
618.168876	96.794641	49.883764
614.647276	118.394424	49.888769
611.091655	118.071678	49.893773
607.641858	120.696406	49.898778
604.348294	96.365359	49.903783
600.659060	126.503158	49.908788
597.155804	108.661442	49.913793
593.899273	126.933192	49.918797
589.810596	110.787053	49.923802
586.760797	90.741063	49.928807
583.238400	117.555485	49.933812
579.839996	101.169180	49.938817
576.320975	110.258968	49.943821
572.651033	125.046220	49.948826
569.406239	109.563208	49.953831
565.387895	123.464150	49.958836
561.950909	111.422639	49.963841
558.521101	96.620689	49.968845
554.923557	117.658512	49.973850
551.591665	117.833710	49.978855
547.992141	112.926409	49.983860
544.234093	105.409537	49.988865
540.988308	119.477043	49.993869
537.526794	114.091299	49.998874
534.587638	104.212105	50.003879
530.516142	110.146983	50.008884
527.067012	127.971635	50.013889
523.912507	106.919692	50.018893
519.912978	135.726142	50.023898
516.614219	112.515545	50.028903
512.761724	103.510910	50.033908
509.430710	113.680936	50.038913
506.440867	109.397715	50.043917
502.458164	112.839329	50.048922
499.037484	98.817691	50.053927
495.504048	113.654920	50.058932
491.898332	116.217960	50.063937
488.622368	105.577233	50.068941
484.740927	113.988852	50.073946
481.693400	111.901295	50.078951
478.194339	122.442983	50.083956
474.798868	96.583361	50.088961
471.416447	105.189452	50.093965
467.189819	111.711296	50.098970
464.041460	111.842312	50.103975
460.816783	107.098159	50.108980
456.935097	88.480877	50.113985
453.650910	110.846244	50.118989
449.750163	117.351753	50.123994
446.365369	103.392383	50.128999
442.972775	112.562559	50.134004
439.688669	95.973993	50.139009
436.270777	94.192881	50.144013
432.385574	99.041215	50.149018
429.149728	94.024789	50.154023
425.613525	105.934548	50.159028
421.719414	102.225726	50.164033
418.543672	118.527604	50.169037
414.587996	114.678123	50.174042
411.200491	108.278861	50.179047
407.879727	111.171112	50.184052
404.634225	99.391163	50.189057
401.041512	107.067453	50.194061
397.419434	101.876121	50.199066
394.111878	105.491056	50.204071
390.167355	108.488433	50.209076
386.842071	115.483687	50.214081
383.665788	111.006708	50.219085
380.009192	104.083418	50.224090
376.366983	98.212294	50.229095
372.945854	112.209186	50.234100
369.476529	109.212985	50.239105
366.149666	112.804490	50.244109
362.365653	99.745098	50.249114
359.214523	115.307018	50.254119
355.516086	109.988639	50.259124
351.485175	97.171090	50.264129
348.180096	98.855506	50.269133
344.417269	108.874980	50.274138
341.255758	104.333635	50.279143
337.844208	106.955828	50.284148
334.206111	119.897155	50.289153
331.094008	99.673404	50.294157
327.501094	93.181077	50.299162
324.413055	83.091044	50.304167
320.297777	100.480471	50.309172
316.980542	120.211749	50.314177
313.692006	105.998922	50.319181
309.757237	89.978634	50.324186
306.231724	85.410841	50.329191
302.663616	101.329409	50.334196
299.182959	105.500553	50.339201
295.829158	108.933576	50.344205
292.557863	102.015935	50.349210
288.965696	114.019248	50.354215
285.284571	93.891128	50.359220
281.731304	110.222566	50.364225
278.585563	104.981609	50.369229
274.300305	99.216005	50.374234
271.476366	106.053699	50.379239
267.883686	99.347305	50.384244
264.699289	105.871672	50.389249
261.209527	93.975326	50.394253
257.176768	106.367212	50.399258
253.659668	98.375102	50.404263
250.099122	113.452474	50.409268
246.751212	99.981470	50.414273
243.410865	96.425126	50.419277
239.657932	106.616238	50.424282
236.325071	106.322396	50.429287
233.144290	86.667041	50.434292
229.422965	102.729233	50.439297
225.676025	92.630829	50.444301
221.571913	98.452990	50.449306
218.670241	107.640989	50.454311
215.589313	97.599357	50.459316
212.095708	114.001562	50.464321
208.944588	96.468042	50.469325
204.644838	88.607851	50.474330
200.943176	101.083850	50.479335
197.509602	93.185305	50.484340
194.037391	105.556614	50.489345
190.781361	89.184164	50.494349
187.488842	103.567576	50.499354
184.137325	110.861912	50.504359
180.504613	95.970838	50.509364
176.591602	98.496236	50.514369
173.163800	103.862892	50.519373
169.318045	99.870231	50.524378
166.031750	96.817864	50.529383
162.682218	111.656992	50.534388
159.254414	96.507653	50.539393
155.985967	97.723064	50.544397
152.437479	109.284676	50.549402
148.712773	96.686092	50.554407
145.126676	90.006511	50.559412
141.757325	108.961310	50.564417
138.310422	88.863269	50.569421
134.671163	101.683523	50.574426
131.457688	103.444456	50.579431
127.833486	96.231877	50.584436
123.917564	92.216908	50.589441
120.205544	102.583811	50.594445
116.895035	94.826169	50.599450
114.028484	98.891685	50.604455
110.512276	112.097457	50.609460
106.538641	104.073452	50.614465
103.558867	93.604310	50.619469
99.562824	107.954859	50.624474
95.991579	88.977805	50.629479
92.865291	89.194336	50.634484
89.085601	104.679481	50.639489
85.618449	94.516197	50.644493
82.222294	110.803500	50.649498
78.918488	97.529522	50.654503
74.807596	111.958254	50.659508
71.039688	98.375265	50.664513
68.257719	101.053166	50.669517
64.578120	108.241963	50.674522
61.393869	97.773981	50.679527
57.607297	109.729022	50.684532
53.991860	109.844304	50.689537
50.764563	90.767729	50.694541
47.426404	97.565299	50.699546
43.605610	111.358466	50.704551
40.104111	97.456744	50.709556
36.600479	110.222279	50.714561
33.243398	91.475509	50.719565
29.440869	97.570148	50.724570
26.236312	100.661785	50.729575
22.679929	111.360812	50.734580
18.999281	100.233458	50.739585
15.338232	93.076935	50.744589
11.547072	112.264971	50.749594
8.481454	94.478811	50.754599
5.416771	99.318766	50.759604
1.455697	91.980212	50.764609