Wed Jun 15 16:14:29 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.887004	109.298992	0.000000
0.863013	98.062744	0.005005
0.394760	80.792028	0.010010
0.481657	98.326765	0.015014
0.247344	87.904492	0.020019
-0.013553	76.232132	0.025024
-0.332678	87.616370	0.030029
-0.266860	68.087184	0.035034
-0.900854	52.773019	0.040038
-0.968814	51.932911	0.045043
-1.107219	30.048015	0.050048
-1.684488	31.654257	0.055053
-1.912460	25.365043	0.060058
-1.887426	15.559310	0.065062
-2.206648	22.624102	0.070067
-2.340722	18.775661	0.075072
-3.015284	9.356035	0.080077
-3.162681	-3.054249	0.085082
-3.473951	-12.826285	0.090086
-3.512972	-13.108693	0.095091
-4.057421	-24.480497	0.100096
-4.888496	-6.302722	0.105101
-5.104617	-13.290911	0.110106
-5.215232	-18.179199	0.115110
-5.376252	-7.710945	0.120115
-5.243197	-15.075168	0.125120
-5.571115	-12.075926	0.130125
-5.728533	-11.535100	0.135130
-6.313925	-10.694491	0.140134
-6.562301	-20.238981	0.145139
-6.573096	-11.856169	0.150144
-6.958024	4.375884	0.155149
-7.135535	-12.235383	0.160154
-7.706303	-18.212041	0.165158
-8.152408	-11.823327	0.170163
-8.265800	-39.653202	0.175168
-8.591746	-6.090661	0.180173
-8.376718	7.362135	0.185178
-8.252426	-3.978544	0.190182
-8.445758	-11.308855	0.195187
-9.374803	-18.113623	0.200192
-9.918544	-6.890119	0.205197
-10.175995	-19.606746	0.210202
-10.202492	4.900661	0.215206
-10.230741	2.035005	0.220211
-9.937533	-21.832310	0.225216
-10.283910	-19.280336	0.230221
-11.263420	-1.992572	0.235226
-11.651377	-3.836686	0.240230
-11.435923	-9.560829	0.245235
-11.588661	7.534479	0.250240
-11.389159	-4.046600	0.255245
-12.261910	-5.722210	0.260250
-12.733046	-6.429296	0.265254
-12.906204	-1.194860	0.270259
-12.921531	-26.832675	0.275264
-13.223700	-3.410698	0.280269
-13.412312	-11.814168	0.285274
-13.520771	-0.476353	0.290278
-14.033353	3.163832	0.295283
-14.300277	-12.756438	0.300288
-14.346785	5.975899	0.305293
-14.637553	1.267221	0.310298
-14.386557	-21.900326	0.315302
-15.459126	-9.236601	0.320307
-15.851070	-14.925172	0.325312
-16.076314	-11.582840	0.330317
-16.239924	3.145377	0.335322
-16.189597	-12.085900	0.340326
-16.260960	12.683734	0.345331
-16.309109	-10.496836	0.350336
-17.255382	-3.589346	0.355341
-17.780886	-3.670516	0.360346
-17.848075	-6.306202	0.365350
-18.042193	3.542211	0.370355
-17.863627	-11.466308	0.375360
-18.073142	-6.716431	0.380365
-18.206982	5.709898	0.385370
-18.380130	-6.631511	0.390374
-19.090106	-9.247974	0.395379
-19.550249	-0.709415	0.400384
-19.504178	-15.562467	0.405389
-19.534681	-3.830919	0.410394
-20.039313	-24.984416	0.415398
-20.849896	-0.365788	0.420403
-21.049478	4.669411	0.425408
-20.708759	-1.137485	0.430413
-20.916247	-5.203335	0.435418
-21.031662	-16.537337	0.440422
-21.178276	-1.043088	0.445427
-21.605322	-0.160678	0.450432
-22.338715	-6.565122	0.455437
-22.286602	-3.422512	0.460442
-22.340531	8.349415	0.465446
-23.058845	-6.842831	0.470451
-22.610009	-4.627260	0.475456
-23.651008	7.874316	0.480461
-24.291916	-8.965973	0.485466
-23.580976	2.403434	0.490470
-23.937931	6.013461	0.495475
-23.986498	-14.292685	0.500480
-24.103982	-17.058754	0.505485
-24.278927	-9.419928	0.510490
-25.157865	-19.184950	0.515494
-26.043334	1.392108	0.520499
-25.713815	-15.247901	0.525504
-25.897826	7.727327	0.530509
-26.003395	3.518661	0.535514
-25.899117	-14.885597	0.540518
-26.326630	-11.362658	0.545523
-26.546713	-10.707108	0.550528
-27.136156	-10.965334	0.555533
-27.447624	2.948236	0.560538
-27.449457	-10.871182	0.565542
-27.725993	0.261803	0.570547
-28.415797	2.912954	0.575552
-28.876918	-2.039633	0.580557
-29.105281	-9.596365	0.585562
-28.701945	5.000966	0.590566
-29.051557	6.765200	0.595571
-29.335934	-9.823768	0.600576
-29.389584	16.859336	0.605581
-29.392461	-1.126134	0.610586
-29.773429	3.752699	0.615590
-30.491333	-3.707448	0.620595
-30.458920	0.213281	0.625600
-30.901545	-2.412641	0.630605
-30.988106	-16.890717	0.635610
-30.856941	-12.158870	0.640614
-31.857544	-12.559064	0.645619
-32.123496	-14.577029	0.650624
-32.447976	-2.333262	0.655629
-32.587559	0.925863	0.660634
-32.340405	-19.014440	0.665638
-32.566851	-8.068880	0.670643
-32.504127	-18.135027	0.675648
-33.327793	-12.249551	0.680653
-33.776031	0.985148	0.685658
-33.546546	-10.070460	0.690662
-33.919284	-5.190918	0.695667
-34.122302	-10.576302	0.700672
-34.809833	-10.689091	0.705677
-35.639991	-14.114905	0.710682
-34.781244	-13.738958	0.715686
-35.487269	-11.377217	0.720691
-35.509302	-5.768047	0.725696
-35.436675	4.610994	0.730701
-35.855423	-12.454813	0.735706
-36.357483	-1.657144	0.740710
-37.003469	-4.341296	0.745715
-36.982771	-18.763012	0.750720
-37.314691	-11.521140	0.755725
-37.229764	-21.057182	0.760730
-37.414382	-8.642302	0.765734
-37.204472	2.288266	0.770739
-37.547890	-19.998781	0.775744
-38.333852	3.850389	0.780749
-38.712817	-7.689635	0.785754
-38.718339	-31.886457	0.790758
-39.311657	-2.574370	0.795763
-39.242667	-4.890556	0.800768
-39.773318	-10.163789	0.805773
-40.175286	20.181402	0.810778
-40.251884	-4.274895	0.815782
-40.513977	-11.481184	0.820787
-40.518471	-12.962518	0.825792
-40.367737	1.390284	0.830797
-40.612258	-9.445529	0.835802
-41.370744	-11.875718	0.840806
-42.166785	-15.205959	0.845811
-42.099559	8.142946	0.850816
-42.090262	-4.334165	0.855821
-42.194208	-5.554422	0.860826
-42.211534	2.504633	0.865830
-42.893898	-5.068217	0.870835
-43.196669	-3.010955	0.875840
-43.667731	-12.002133	0.880845
-43.895265	-7.688648	0.885850
-43.580913	3.389299	0.890854
-43.865219	3.659894	0.895859
-44.272803	-1.544603	0.900864
-44.659589	7.090347	0.905869
-45.315108	-5.692486	0.910874
-45.379485	-25.346022	0.915878
-45.870263	-1.260855	0.920883
-45.527065	-3.235371	0.925888
-45.685373	-0.012412	0.930893
-45.832514	17.589510	0.935898
-45.688001	-11.014784	0.940902
-46.458435	-10.956432	0.945907
-46.951294	2.234050	0.950912
-46.966176	-18.318250	0.955917
-47.177567	-3.966570	0.960922
-47.331869	10.115461	0.965926
-48.339327	18.974624	0.970931
-48.689654	-9.415114	0.975936
-48.617467	-11.151592	0.980941
-48.773870	-11.448534	0.985946
-48.686538	6.660431	0.990950
-49.087297	14.765006	0.995955
-48.525716	2.855768	1.000960
-49.395301	-0.449300	1.005965
-49.968044	-8.962011	1.010970
-50.092781	-12.206891	1.015974
-50.470721	10.190065	1.020979
-50.303498	-2.689579	1.025984
-51.073650	-3.026054	1.030989
-51.815430	8.584228	1.035994
-51.422476	-15.143910	1.040998
-51.853594	-14.044496	1.046003
-52.052500	-3.271086	1.051008
-52.101562	-25.366467	1.056013
-52.364238	-5.792984	1.061018
-52.048551	-18.157164	1.066022
-52.558708	-6.836226	1.071027
-53.104412	-1.372524	1.076032
-53.586519	-9.233762	1.081037
-53.903481	-18.540520	1.086042
-53.586513	-11.773147	1.091046
-53.760204	12.534364	1.096051
-54.339896	-12.252788	1.101056
-55.104832	4.445131	1.106061
-55.444063	-7.521590	1.111066
-55.232624	-7.565237	1.116070
-55.349991	3.256652	1.121075
-55.349499	-20.787389	1.126080
-55.458212	-14.774148	1.131085
-55.859817	5.495469	1.136090
-56.428400	14.344344	1.141094
-56.867459	-10.506793	1.146099
-57.044421	-6.786636	1.151104
-57.026649	-11.027519	1.156109
-57.064165	-1.116310	1.161114
-57.160066	-9.082807	1.166118
-58.019336	-2.401288	1.171123
-58.480810	-12.123534	1.176128
-58.617248	9.076785	1.181133
-58.673464	-8.883085	1.186138
-58.646884	-0.282720	1.191142
-58.988620	-2.055651	1.196147
-59.241254	-12.691840	1.201152
-59.748861	-5.200555	1.206157
-60.106330	-17.302161	1.211162
-60.137345	-14.365600	1.216166
-60.194345	6.227541	1.221171
-60.434778	-12.033329	1.226176
-60.925461	-1.759181	1.231181
-61.581048	3.541274	1.236186
-61.609681	-15.652570	1.241190
-61.998393	-1.165539	1.246195
-61.883402	-13.797324	1.251200
-61.912255	-8.069541	1.256205
-62.217565	10.660384	1.261210
-62.086302	4.348017	1.266214
-63.046861	4.869468	1.271219
-63.412218	-14.748047	1.276224
-63.435350	-13.534750	1.281229
-63.574105	-6.381916	1.286234
-63.422486	-8.732177	1.291238
-63.960881	-1.196739	1.296243
-64.289875	-19.703980	1.301248
-64.732298	-12.600891	1.306253
-64.995137	-20.852794	1.311258
-64.663302	-16.525714	1.316262
-65.346807	7.786536	1.321267
-66.001320	2.226195	1.326272
-66.251874	-27.510429	1.331277
-66.521586	-0.757132	1.336282
-66.319141	-23.278700	1.341286
-66.216701	-16.580539	1.346291
-66.452258	1.212253	1.351296
-66.990577	-7.319463	1.356301
-67.954950	17.546359	1.361306
-67.841022	-8.809273	1.366310
-68.223763	-2.071266	1.371315
-68.051904	2.587962	1.376320
-68.352035	-12.379414	1.381325
-68.640705	0.313980	1.386330
-68.438571	-17.270811	1.391334
-69.366114	3.214258	1.396339
-69.603092	-9.723856	1.401344
-69.859512	-9.488054	1.406349
-69.981923	10.907463	1.411354
-69.732685	-16.419690	1.416358
-70.180384	8.917287	1.421363
-70.394556	-11.750148	1.426368
-71.146528	-18.737364	1.431373
-71.761266	-2.783109	1.436378
-71.299963	-16.460755	1.441382
-71.377725	-12.942843	1.446387
-71.478768	-20.131450	1.451392
-72.098779	-1.295373	1.456397
-73.000616	-0.890361	1.461402
-72.995897	-16.648452	1.466406
-73.204356	-1.261673	1.471411
-73.384900	-10.609426	1.476416
-73.262063	-22.368793	1.481421
-73.125598	-5.920580	1.486426
-73.369123	-5.418494	1.491430
-74.399620	5.694682	1.496435
-74.781009	-15.456392	1.501440
-74.688494	0.525295	1.506445
-75.196449	-9.907015	1.511450
-74.848076	-10.870872	1.516454
-75.148194	-8.276724	1.521459
-75.767886	-12.255601	1.526464
-76.191215	-6.258229	1.531469
-76.656911	-6.313667	1.536474
-76.384429	4.886907	1.541478
-76.507781	-5.533802	1.546483
-76.650917	4.440834	1.551488
-76.818749	-1.171331	1.556493
-77.654888	-25.233638	1.561498
-77.695818	-17.486164	1.566502
-78.385911	-0.356914	1.571507
-78.335995	-6.045608	1.576512
-78.243062	-13.691143	1.581517
-78.335400	-4.367192	1.586522
-78.388861	-22.336573	1.591526
-79.170959	-22.577651	1.596531
-79.506652	-13.965857	1.601536
-79.475035	-23.221511	1.606541
-79.955551	-18.369932	1.611546
-80.172602	5.257562	1.616550
-80.907975	-7.974810	1.621555
-80.917528	-13.601982	1.626560
-80.911442	-6.527442	1.631565
-81.488100	-19.160227	1.636570
-81.257115	-11.510959	1.641574
-81.491758	-6.886354	1.646579
-81.489424	-18.073392	1.651584
-82.373626	3.582837	1.656589
-83.148873	-6.372045	1.661594
-83.200094	-24.858992	1.666598
-83.481443	-16.834344	1.671603
-83.031890	-11.479793	1.676608
-83.115041	-13.198094	1.681613
-83.414094	-7.725342	1.686618
-83.324685	-13.226919	1.691622
-83.848726	-18.723484	1.696627
-84.333754	-5.420763	1.701632
-84.715555	-9.628159	1.706637
-84.895226	-12.934095	1.711642
-85.271272	-16.281855	1.716646
-85.998244	-3.573438	1.721651
-86.152695	-21.142494	1.726656
-86.133657	-12.938336	1.731661
-86.864147	9.896666	1.736666
-85.986529	-10.415760	1.741670
-86.298166	-0.555034	1.746675
-86.435822	-13.557498	1.751680
-87.014902	-5.570544	1.756685
-87.827837	-14.263824	1.761690
-88.300526	-18.043167	1.766694
-88.634628	-10.535775	1.771699
-88.171106	-20.301589	1.776704
-88.382644	-12.676352	1.781709
-88.464190	-15.864247	1.786714
-88.223576	-3.023558	1.791718
-88.833174	6.192937	1.796723
-89.594258	-3.783029	1.801728
-89.678425	-8.106893	1.806733
-89.694157	-18.101472	1.811738
-89.635762	-21.956651	1.816742
-90.601447	-4.169267	1.821747
-91.259752	-1.279859	1.826752
-91.078685	-12.843179	1.831757
-91.526863	-0.107938	1.836762
-91.332572	-6.166049	1.841766
-91.495719	-11.511062	1.846771
-91.554036	-7.108846	1.851776
-92.100894	-19.500333	1.856781
-92.600096	-15.654613	1.861786
-92.502545	-0.935541	1.866790
-92.783363	14.289395	1.871795
-92.945900	-8.578977	1.876800
-93.687348	-13.476935	1.881805
-94.425701	5.356511	1.886810
-94.455772	-18.030620	1.891814
-94.698985	-3.267364	1.896819
-94.790030	-2.913095	1.901824
-94.582813	7.834530	1.906829
-94.725789	-2.205713	1.911834
-94.387530	-13.449258	1.916838
-95.233910	-0.786013	1.921843
-95.882755	-23.058565	1.926848
-96.242704	-10.528498	1.931853
-96.197261	-2.744393	1.936858
-96.237523	-14.840810	1.941862
-96.674398	0.266671	1.946867
-96.742587	-8.147915	1.951872
-97.298390	-24.201623	1.956877
-97.629673	-2.422233	1.961882
-97.493785	-12.588560	1.966886
-97.491278	-2.645796	1.971891
-98.182357	12.269131	1.976896
-98.724756	-6.844834	1.981901
-99.461667	-2.295740	1.986906
-99.406433	-15.095107	1.991910
-99.551920	-9.829737	1.996915
-99.423751	-9.095386	2.006912
-98.763604	-11.282306	2.016909
-98.367867	0.029804	2.026906
-98.379163	-3.294920	2.036902
-98.333609	-8.045037	2.046899
-97.091450	-11.673820	2.056896
-97.002763	-5.373133	2.066893
-95.770896	-1.705993	2.076890
-95.356952	-6.140773	2.086886
-95.267055	-0.392716	2.096883
-95.173349	-11.922904	2.106880
-94.050037	-14.149037	2.116877
-93.624263	-2.296077	2.126874
-93.279241	1.479116	2.136870
-92.554946	-1.959973	2.146867
-92.383518	-15.204157	2.156864
-91.815329	-3.656730	2.166861
-91.112302	7.874446	2.176858
-90.885120	-1.288807	2.186854
-89.891301	-13.151674	2.196851
-89.322227	4.421898	2.206848
-89.286366	1.254723	2.216845
-89.048693	2.733328	2.226842
-88.157057	-8.382333	2.236838
-87.539238	1.200814	2.246835
-87.129339	-8.263664	2.256832
-86.582754	-5.196892	2.266829
-86.438796	-11.018257	2.276826
-85.871898	11.467719	2.286822
-84.696100	-5.609093	2.296819
-84.561884	-6.899850	2.306816
-84.391585	5.236344	2.316813
-83.679660	4.291520	2.326810
-83.348894	1.884252	2.336806
-82.510747	-0.713841	2.346803
-81.533305	1.761886	2.356800
-81.336422	-0.800352	2.366797
-81.409635	-7.506284	2.376794
-81.107357	-2.550515	2.386790
-79.960669	-8.721914	2.396787
-79.899650	-8.441653	2.406784
-79.146619	3.812370	2.416781
-78.740963	-4.948842	2.426778
-78.315058	-3.145273	2.436774
-77.136540	2.909815	2.446771
-76.804460	-3.707833	2.456768
-76.785290	-6.198524	2.466765
-76.551576	1.944203	2.476762
-75.553612	5.349740	2.486758
-75.111774	4.125284	2.496755
-74.529346	-4.534271	2.506752
-73.805911	-1.433906	2.516749
-73.828837	2.627993	2.526746
-73.439932	5.837775	2.536742
-72.471854	2.437710	2.546739
-71.969342	4.573335	2.556736
-71.948248	7.159908	2.566733
-70.849492	-7.503410	2.576730
-70.628569	-0.110522	2.586726
-70.249497	8.736432	2.596723
-69.328673	-0.093826	2.606720
-68.827155	-4.431763	2.616717
-68.736901	4.954216	2.626714
-68.695552	6.587154	2.636710
-67.752399	-7.285753	2.646707
-67.191757	-7.836659	2.656704
-66.008112	-7.832410	2.666701
-65.871867	0.934961	2.676698
-65.984440	3.337093	2.686694
-65.223698	-6.869764	2.696691
-64.537169	-3.424312	2.706688
-64.470740	0.817103	2.716685
-63.458945	-1.917151	2.726682
-62.739865	-7.175252	2.736678
-62.483275	-6.166274	2.746675
-62.430016	-2.112127	2.756672
-61.371144	-5.494106	2.766669
-61.218152	-8.665822	2.776666
-60.749540	-4.996787	2.786662
-59.758316	-2.108886	2.796659
-59.409688	-3.691591	2.806656
-59.629519	-10.169525	2.816653
-58.522724	-4.599307	2.826650
-58.168272	-2.852475	2.836646
-57.648312	-0.869965	2.846643
-56.536392	-8.480554	2.856640
-56.073491	-10.208473	2.866637
-56.309226	-9.861784	2.876634
-56.051153	1.705498	2.886630
-55.054957	-9.613232	2.896627
-54.637546	0.993629	2.906624
-53.896404	-3.421148	2.916621
-53.227078	-7.097091	2.926618
-53.106807	2.867078	2.936614
-53.060372	3.833846	2.946611
-51.722866	-9.458855	2.956608
-51.522701	5.122057	2.966605
-51.392199	7.580023	2.976602
-50.152702	-2.048037	2.986598
-49.807229	-1.699322	2.996595
-49.410004	4.018098	3.006592
-49.516766	3.034247	3.016589
-48.751723	-10.060134	3.026586
-48.374099	3.295614	3.036582
-47.102848	-2.609238	3.046579
-46.647083	-7.235337	3.056576
-46.537603	-2.659185	3.066573
-46.547600	0.034163	3.076570
-45.762560	-10.401611	3.086566
-44.991213	-13.195685	3.096563
-44.567726	2.952279	3.106560
-43.599636	0.102575	3.116557
-43.172605	-17.254159	3.126554
-42.857299	-2.834514	3.136550
-42.784509	-1.182375	3.146547
-42.355698	-3.005605	3.156544
-41.614305	-7.720096	3.166541
-41.067577	-4.645539	3.176538
-40.256814	3.222851	3.186534
-39.944401	-6.106400	3.196531
-39.901041	3.682914	3.206528
-39.068384	-8.501196	3.216525
-38.647136	-4.607131	3.226522
-37.962228	-7.817863	3.236518
-37.013941	-7.786367	3.246515
-37.037486	-10.151472	3.256512
-37.081986	-4.109775	3.266509
-35.991568	-3.241956	3.276506
-35.410929	-17.623081	3.286502
-35.270846	-10.156385	3.296499
-34.175229	-1.477928	3.306496
-33.513078	-11.754715	3.316493
-33.569966	-9.010950	3.326490
-33.355947	-10.271337	3.336486
-32.711674	-5.286941	3.346483
-32.137046	-6.386070	3.356480
-31.368462	-14.814342	3.366477
-30.397738	-10.346745	3.376474
-30.442251	-10.044993	3.386470
-30.276502	-10.758205	3.396467
-29.954920	-15.724520	3.406464
-28.894068	-4.209310	3.416461
-28.639804	-5.675177	3.426458
-27.752209	-9.230142	3.436454
-26.976603	-10.678753	3.446451
-26.910068	4.298397	3.456448
-26.880166	2.183141	3.466445
-26.079391	4.181670	3.476442
-25.495926	-8.993427	3.486438
-25.289962	-5.069511	3.496435
-24.199177	3.031340	3.506432
-23.712738	-10.560838	3.516429
-23.841353	0.433175	3.526426
-23.007233	1.822893	3.536422
-22.108564	-5.034476	3.546419
-21.858863	-12.683023	3.556416
-21.894997	-0.134311	3.566413
-21.045318	9.995960	3.576410
-20.615948	-1.226037	3.586406
-19.768846	-14.046944	3.596403
-19.099862	-3.248949	3.606400
-18.773987	6.739721	3.616397
-18.674160	-1.855192	3.626394
-18.325666	-4.387172	3.636390
-17.499275	-0.521735	3.646387
-17.215266	-11.848007	3.656384
-16.371029	-7.189417	3.666381
-16.143203	-7.268400	3.676378
-15.612871	1.583095	3.686374
-14.741518	-11.163397	3.696371
-14.427252	-11.717141	3.706368
-14.190713	-13.479258	3.716365
-13.108752	-3.733677	3.726362
-13.083573	-10.202622	3.736358
-12.699711	-7.137495	3.746355
-11.713728	-7.396886	3.756352
-11.248067	-3.845785	3.766349
-11.178007	-0.275927	3.776346
-10.393948	-5.781719	3.786342
-9.568768	-2.581509	3.796339
-9.223354	-11.614463	3.806336
-9.448548	-0.792057	3.816333
-8.900888	5.824720	3.826330
-7.847356	-11.670527	3.836326
-7.288252	6.081618	3.846323
-6.470981	-14.215766	3.856320
-6.296524	-6.977576	3.866317
-6.130941	-10.282642	3.876314
-5.888706	-6.584190	3.886310
-4.703056	-3.532348	3.896307
-4.584596	7.630336	3.906304
-4.132945	-0.187601	3.916301
-3.646435	6.028884	3.926298
-3.285067	17.621687	3.936294
-2.493480	24.754645	3.946291
-2.383992	24.564149	3.956288
-2.081091	55.019149	3.966285
-1.314627	71.438244	3.976282
-0.619020	75.274350	3.986278
-0.329559	101.149004	3.996275
0.000000	98.390317	4.001280
0.300553	125.390951	4.006285
0.181786	121.988081	4.011290
0.716349	105.892911	4.016294
0.411681	111.984656	4.021299
0.111019	118.716255	4.026304
0.584566	119.679388	4.031309
0.804803	146.022829	4.036314
0.950880	153.114563	4.041318
0.695912	148.751500	4.046323
0.821413	148.044944	4.051328
0.976069	149.486836	4.056333
1.077688	133.852642	4.061338
0.945850	154.406870	4.066342
0.856460	153.771636	4.071347
1.035277	152.785680	4.076352
0.862178	162.701947	4.081357
1.020712	144.850815	4.086362
1.162857	129.149853	4.091366
0.931081	136.606572	4.096371
0.555453	117.000605	4.101376
0.909745	139.248266	4.106381
0.587599	155.529687	4.111386
1.088722	147.935774	4.116390
0.807640	170.042036	4.121395
1.212447	143.545522	4.126400
1.075294	151.066712	4.131405
1.190275	151.926830	4.136410
1.427617	154.589327	4.141414
1.115582	160.340990	4.146419
1.122173	144.936258	4.151424
0.964545	159.841500	4.156429
1.113118	152.610764	4.161434
1.134569	150.149903	4.166438
1.327312	161.926464	4.171443
1.392850	150.807865	4.176448
0.821016	160.782133	4.181453
1.021807	144.392872	4.186458
1.495199	144.955230	4.191462
1.454380	160.813038	4.196467
1.499325	149.590021	4.201472
1.251811	162.043454	4.206477
1.445174	163.935981	4.211482
1.012920	144.513572	4.216486
1.037205	171.301365	4.221491
1.154073	149.175239	4.226496
1.188896	155.843421	4.231501
0.919266	151.652355	4.236506
1.294999	157.069091	4.241510
1.154491	158.812298	4.246515
1.409573	139.068853	4.251520
1.498434	168.323386	4.256525
1.253923	171.115926	4.261530
1.522059	159.066940	4.266534
1.053755	175.416730	4.271539
1.249136	157.321459	4.276544
1.211899	172.863609	4.281549
1.118758	148.201744	4.286554
1.240790	154.350540	4.291558
1.329714	164.660314	4.296563
1.517867	177.961349	4.301568
1.636684	189.619934	4.306573
1.764822	184.921086	4.311578
1.493523	170.160152	4.316582
1.315651	158.875305	4.321587
1.472893	176.524676	4.326592
1.846168	176.082091	4.331597
1.725286	167.895399	4.336602
1.695809	157.944004	4.341606
1.358082	164.926589	4.346611
1.467225	158.338739	4.351616
1.403694	158.134462	4.356621
1.489309	170.903367	4.361626
1.899848	197.378585	4.366630
1.809939	190.819966	4.371635
1.772884	168.391150	4.376640
1.477808	176.876880	4.381645
1.726407	177.179954	4.386650
1.827706	170.337998	4.391654
1.801711	183.221736	4.396659
1.900702	164.224079	4.401664
1.298853	153.226720	4.406669
1.565530	177.569552	4.411674
1.787618	186.095399	4.416678
1.800786	192.350589	4.421683
1.920683	196.943201	4.426688
2.068288	181.915142	4.431693
1.976725	180.099558	4.436698
1.663172	169.301852	4.441702
1.388439	175.397455	4.446707
1.879309	187.813916	4.451712
1.908892	194.116112	4.456717
2.190947	190.688543	4.461722
2.112605	191.202990	4.466726
1.670560	192.041819	4.471731
1.923009	193.220639	4.476736
2.229893	188.591785	4.481741
1.684224	196.932693	4.486746
1.857386	174.167859	4.491750
1.953287	185.089586	4.496755
2.193832	200.150725	4.501760
2.021570	186.115631	4.506765
1.868356	188.262732	4.511770
2.120446	186.790863	4.516774
2.005045	193.939736	4.521779
2.016344	193.443427	4.526784
2.043967	202.076886	4.531789
1.802749	197.641792	4.536794
2.163994	175.496057	4.541798
1.714140	196.794018	4.546803
1.967930	208.079721	4.551808
2.038535	191.839572	4.556813
1.930348	195.724104	4.561818
2.266416	186.489423	4.566822
1.908174	189.094687	4.571827
2.061609	186.636768	4.576832
2.205973	195.047520	4.581837
1.966171	192.940564	4.586842
2.377755	187.804920	4.591846
1.949569	190.645574	4.596851
1.985289	181.898426	4.601856
2.153281	197.956643	4.606861
1.813235	198.867201	4.611866
2.026405	207.169026	4.616870
1.933075	226.238558	4.621875
2.331563	210.278916	4.626880
2.204720	234.763620	4.631885
2.085867	216.155057	4.636890
2.279415	223.199223	4.641894
2.463204	209.571475	4.646899
2.592320	212.015706	4.651904
2.649894	208.811378	4.656909
2.416477	211.403811	4.661914
2.527836	224.141476	4.666918
2.123256	212.619420	4.671923
2.244487	222.857012	4.676928
1.996765	211.345238	4.681933
1.998669	219.014536	4.686938
2.249821	214.491459	4.691942
2.193282	213.597073	4.696947
2.224715	216.776094	4.701952
2.312181	230.894634	4.706957
2.525601	255.749001	4.711962
2.843210	239.663699	4.716966
2.552615	245.191965	4.721971
2.718395	232.335439	4.726976
2.758929	204.155624	4.731981
2.473359	207.820684	4.736986
2.460319	214.492955	4.741990
2.458220	214.490715	4.746995
2.674326	223.457045	4.752000
2.729166	232.060966	4.757005
2.454576	230.910124	4.762010
2.467849	227.742904	4.767014
2.561436	245.045080	4.772019
2.505124	247.320101	4.777024
2.653000	240.187199	4.782029
2.605706	243.813384	4.787034
2.724554	248.718207	4.792038
2.537839	248.913093	4.797043
2.695050	252.873932	4.802048
2.726188	254.903766	4.807053
2.711762	240.995146	4.812058
2.888430	230.808888	4.817062
2.620675	242.621365	4.822067
2.849856	237.207871	4.827072
3.008833	249.674694	4.832077
2.782247	252.138256	4.837082
2.872423	229.247369	4.842086
2.615100	254.963086	4.847091
3.010976	248.392032	4.852096
2.941661	227.562308	4.857101
2.502066	249.603829	4.862106
2.706854	240.258623	4.867110
2.443867	253.472102	4.872115
2.854931	252.960234	4.877120
3.077211	238.834242	4.882125
2.732298	251.909243	4.887130
2.879873	251.942147	4.892134
2.633052	238.745994	4.897139
2.891576	255.639060	4.902144
3.295973	267.465365	4.907149
2.661372	269.986789	4.912154
3.071374	281.307300	4.917158
3.298918	273.262437	4.922163
3.518167	279.384958	4.927168
3.120118	253.489905	4.932173
2.751280	244.355010	4.937178
3.198062	250.102444	4.942182
2.944762	240.012786	4.947187
2.871412	246.059944	4.952192
3.158978	261.119094	4.957197
3.039558	271.799859	4.962202
3.092030	269.618056	4.967206
3.150902	293.197749	4.972211
3.652128	267.888491	4.977216
3.624174	258.503509	4.982221
3.151362	254.202459	4.987226
3.435870	265.590160	4.992230
2.903042	255.746546	4.997235
3.112457	232.683440	5.002240
3.351902	241.747038	5.007245
3.328678	263.530169	5.012250
2.991338	246.602034	5.017254
3.051674	253.268509	5.022259
3.203454	269.931034	5.027264
3.456368	259.227771	5.032269
3.367982	267.611229	5.037274
3.286535	254.938481	5.042278
3.426358	266.398332	5.047283
3.589055	275.784683	5.052288
3.454801	249.523267	5.057293
3.265598	253.806815	5.062298
3.591522	255.471964	5.067302
3.296621	248.355213	5.072307
3.077421	252.406077	5.077312
3.120140	258.931341	5.082317
3.517756	265.061372	5.087322
3.614128	274.310514	5.092326
3.435703	290.057036	5.097331
3.571107	282.016347	5.102336
3.603050	284.743097	5.107341
3.551778	273.310579	5.112346
3.436546	284.355657	5.117350
3.416168	271.796606	5.122355
3.611115	261.390282	5.127360
3.770919	279.952827	5.132365
3.575569	278.853895	5.137370
3.951839	282.186358	5.142374
3.785920	265.886177	5.147379
3.459933	257.629949	5.152384
3.202839	263.511961	5.157389
2.968028	267.895285	5.162394
3.325641	273.299472	5.167398
3.257360	277.416157	5.172403
3.172535	270.181223	5.177408
3.416447	279.824942	5.182413
3.389318	276.218699	5.187418
3.863296	291.236222	5.192422
3.830793	297.049365	5.197427
3.852002	275.469295	5.202432
4.015555	288.990629	5.207437
3.574333	273.880348	5.212442
3.439248	273.156677	5.217446
3.482385	290.228514	5.222451
4.084226	295.205451	5.227456
3.978453	313.000645	5.232461
3.841251	313.565762	5.237466
3.641183	286.073378	5.242470
3.550214	307.953296	5.247475
3.854332	307.199755	5.252480
3.848933	305.488788	5.257485
3.968721	318.235497	5.262490
3.880678	294.472322	5.267494
3.722502	319.468699	5.272499
4.090108	327.943647	5.277504
4.215645	306.422448	5.282509
4.111315	304.141270	5.287514
3.992504	309.106597	5.292518
4.170699	323.764334	5.297523
3.928198	309.129610	5.302528
4.039119	317.420376	5.307533
3.970958	328.063905	5.312538
3.944718	318.317650	5.317542
3.676408	322.982346	5.322547
3.869520	298.744766	5.327552
4.260906	298.343280	5.332557
4.085818	321.490144	5.337562
4.208672	304.353607	5.342566
4.232751	318.676349	5.347571
4.088731	319.988372	5.352576
4.189079	331.840115	5.357581
3.807482	313.281365	5.362586
4.303976	310.159456	5.367590
4.234040	329.243206	5.372595
3.738386	315.144342	5.377600
4.036711	324.764399	5.382605
3.982904	320.688748	5.387610
4.130503	324.200471	5.392614
4.205304	317.257176	5.397619
4.197544	328.387613	5.402624
4.250847	323.349803	5.407629
3.948130	312.740101	5.412634
4.110106	313.955586	5.417638
4.070505	322.854832	5.422643
4.047389	322.751794	5.427648
4.064227	318.335280	5.432653
4.095573	350.399495	5.437658
4.553686	342.178483	5.442662
4.356838	351.334273	5.447667
4.269272	351.128046	5.452672
4.371662	341.356672	5.457677
4.356719	356.982530	5.462682
4.567358	341.011179	5.467686
4.243451	343.337934	5.472691
4.420652	348.320548	5.477696
4.676622	335.544621	5.482701
4.522249	348.070806	5.487706
4.600299	352.817070	5.492710
4.467961	330.997722	5.497715
4.285419	324.546788	5.502720
4.503032	337.302205	5.507725
4.461584	351.557480	5.512730
4.513771	344.376715	5.517734
4.450325	356.501278	5.522739
4.387998	352.874790	5.527744
4.662698	353.887177	5.532749
4.464079	361.573999	5.537754
4.454829	336.628065	5.542758
4.582683	345.138401	5.547763
4.711700	351.888665	5.552768
4.798660	356.552073	5.557773
4.458437	351.654951	5.562778
4.538808	361.508841	5.567782
4.684313	350.624981	5.572787
4.577654	337.177406	5.577792
4.884387	349.395863	5.582797
4.611593	354.782527	5.587802
4.658903	353.393809	5.592806
4.400616	347.981126	5.597811
4.496658	347.829986	5.602816
4.574996	340.958799	5.607821
4.426339	352.809191	5.612826
4.680558	328.630618	5.617830
4.454137	344.578773	5.622835
4.470772	349.095471	5.627840
4.619048	367.236037	5.632845
4.859339	369.590796	5.637850
4.976731	380.855860	5.642854
5.088620	378.097685	5.647859
4.823613	388.616441	5.652864
4.957775	384.376237	5.657869
4.880642	383.057110	5.662874
5.088908	390.488583	5.667878
4.845793	366.240911	5.672883
4.638802	359.138484	5.677888
4.671713	373.176302	5.682893
4.580708	371.790217	5.687898
4.766617	377.954886	5.692902
4.788219	379.419182	5.697907
4.786862	389.792958	5.702912
5.153258	396.589936	5.707917
4.819734	397.195491	5.712922
5.318946	387.723311	5.717926
5.055085	372.225726	5.722931
5.147656	385.639018	5.727936
5.221423	373.235481	5.732941
4.863093	386.187431	5.737946
4.991142	371.083401	5.742950
4.973350	381.122609	5.747955
4.847772	383.562200	5.752960
5.027409	387.089852	5.757965
5.336640	410.858500	5.762970
5.184143	386.997418	5.767974
5.429406	378.305496	5.772979
5.339923	389.628826	5.777984
5.310058	373.873569	5.782989
5.319012	383.320513	5.787994
5.316086	369.237339	5.792998
5.340674	373.205429	5.798003
5.392122	374.810693	5.803008
5.549977	385.786053	5.808013
5.447909	393.814042	5.813018
5.627458	393.005716	5.818022
5.616053	378.351083	5.823027
4.919582	376.208098	5.828032
4.918211	372.866688	5.833037
5.162745	402.336645	5.838042
4.963125	386.621069	5.843046
5.025508	397.216930	5.848051
5.033298	376.800422	5.853056
5.359821	386.827815	5.858061
5.063505	387.600546	5.863066
5.133921	390.816172	5.868070
4.866490	393.826212	5.873075
5.144339	396.459764	5.878080
5.130473	423.550742	5.883085
5.298840	439.682743	5.888090
5.404876	422.790937	5.893094
5.374998	421.112709	5.898099
5.375018	430.677761	5.903104
5.178112	410.211580	5.908109
5.263661	413.179272	5.913114
5.581556	418.709735	5.918118
5.248515	415.067400	5.923123
5.156460	429.009812	5.928128
5.562385	430.542789	5.933133
5.334830	460.346868	5.938138
5.553068	449.474890	5.943142
5.487659	471.601090	5.948147
5.194704	455.141864	5.953152
5.859133	449.953694	5.958157
5.647126	466.422827	5.963162
5.824228	455.583785	5.968166
5.759997	451.007501	5.973171
5.852262	449.870101	5.978176
6.173424	467.704026	5.983181
5.697074	448.306866	5.988186
5.734791	439.091546	5.993190
5.719650	440.001694	5.998195
5.604827	435.409212	6.003200
6.102826	451.418092	6.008205
5.610614	433.693006	6.013210
5.774962	426.845646	6.018214
5.816884	429.467783	6.023219
5.474916	421.140615	6.028224
5.773842	435.925198	6.033229
5.722520	459.070264	6.038234
6.094075	434.732347	6.043238
5.839697	424.992158	6.048243
5.879576	428.154143	6.053248
5.706750	419.759761	6.058253
5.669307	427.306336	6.063258
5.543187	421.940642	6.068262
5.473099	422.404803	6.073267
5.640423	423.826082	6.078272
5.998328	429.434775	6.083277
5.900755	430.970463	6.088282
6.042344	408.770921	6.093286
5.836567	414.840326	6.098291
5.493426	417.555297	6.103296
6.047565	406.326961	6.108301
5.770447	424.971061	6.113306
5.801850	412.863337	6.118310
5.635068	413.200436	6.123315
5.599339	413.358534	6.128320
5.512165	414.472851	6.133325
5.536311	426.139075	6.138330
5.749568	416.106359	6.143334
5.872229	419.070484	6.148339
5.666285	418.365717	6.153344
5.441030	404.752320	6.158349
5.812437	420.251950	6.163354
5.995313	436.444587	6.168358
5.784569	427.359810	6.173363
5.869602	425.040315	6.178368
5.957978	414.141190	6.183373
5.480941	429.011188	6.188378
5.394981	411.993679	6.193382
5.548857	425.164557	6.198387
5.582222	447.141519	6.203392
5.924157	444.362084	6.208397
5.826791	450.696315	6.213402
5.767726	421.680134	6.218406
5.573050	426.265809	6.223411
5.669865	429.415622	6.228416
5.687809	428.435421	6.233421
5.603578	456.079667	6.238426
5.782942	449.800794	6.243430
5.841320	471.255257	6.248435
5.771710	455.341445	6.253440
6.143213	448.973111	6.258445
5.698007	445.323360	6.263450
5.579609	418.993332	6.268454
5.498152	421.030155	6.273459
5.962094	428.580486	6.278464
5.931631	424.274550	6.283469
5.530751	418.634544	6.288474
5.839358	422.264202	6.293478
5.638612	432.852472	6.298483
5.500745	427.396678	6.303488
5.821765	415.094399	6.308493
5.725396	448.670211	6.313498
5.978016	455.347219	6.318502
6.150993	434.786929	6.323507
6.073928	437.516430	6.328512
5.942037	422.365537	6.333517
5.588881	436.740471	6.338522
5.832683	426.749658	6.343526
5.869264	413.823574	6.348531
5.685907	423.620959	6.353536
5.815173	434.468099	6.358541
5.466733	431.155622	6.363546
5.672273	419.717251	6.368550
5.671354	428.469493	6.373555
5.420539	438.249032	6.378560
5.766919	412.120594	6.383565
5.548076	422.336193	6.388570
5.773799	406.193592	6.393574
5.589066	416.798836	6.398579
5.871135	437.638105	6.403584
5.860768	417.896736	6.408589
5.725945	419.967632	6.413594
5.634486	427.254415	6.418598
5.542272	427.060990	6.423603
5.569633	421.077843	6.428608
5.760730	405.646895	6.433613
5.356488	426.505556	6.438618
5.939081	435.097249	6.443622
6.112956	440.009317	6.448627
5.932578	423.570190	6.453632
5.954431	420.501444	6.458637
5.510128	422.191699	6.463642
5.644383	430.909865	6.468646
5.669447	420.099130	6.473651
5.725896	402.947413	6.478656
6.048783	410.818472	6.483661
5.712189	428.212860	6.488666
5.677469	419.814497	6.493670
5.789143	423.770773	6.498675
5.722898	436.301603	6.503680
5.860000	422.496711	6.508685
5.620501	417.366585	6.513690
5.564327	429.335027	6.518694
5.632503	413.901103	6.523699
5.198233	428.825196	6.528704
5.943816	432.292872	6.533709
5.730142	443.620093	6.538714
5.958879	446.870729	6.543718
5.780306	430.572463	6.548723
5.418332	425.085244	6.553728
5.589847	434.850131	6.558733
5.664515	442.165698	6.563738
6.049487	453.405241	6.568742
5.724484	443.653036	6.573747
5.709239	456.539962	6.578752
6.015718	465.951105	6.583757
5.570674	438.097432	6.588762
5.653492	426.674700	6.593766
5.774674	441.782636	6.598771
5.952987	426.553445	6.603776
5.671324	422.374945	6.608781
5.749164	418.495131	6.613786
5.615459	423.663706	6.618790
5.737489	424.068891	6.623795
5.698461	428.586130	6.628800
5.744074	438.075387	6.633805
5.615219	431.742199	6.638810
5.674241	445.194234	6.643814
5.719579	447.750997	6.648819
5.787672	448.097719	6.653824
6.003921	441.837516	6.658829
5.666207	443.039406	6.663834
5.682527	438.130883	6.668838
5.757408	417.650061	6.673843
5.692872	436.536544	6.678848
6.083197	422.733505	6.683853
5.631068	415.835615	6.688858
5.625297	413.730004	6.693862
6.022303	432.932041	6.698867
5.710138	417.463996	6.703872
5.838770	401.477625	6.708877
5.889212	416.429327	6.713882
5.603187	430.998351	6.718886
5.716556	428.553920	6.723891
5.705458	415.351706	6.728896
5.850819	428.007667	6.733901
5.772840	428.607689	6.738906
5.896917	416.647515	6.743910
5.788840	412.056786	6.748915
5.741275	411.299210	6.753920
5.868773	416.198514	6.758925
5.743126	428.325817	6.763930
5.953328	416.212908	6.768934
5.637127	415.167379	6.773939
5.867573	423.176243	6.778944
6.109158	404.724221	6.783949
5.967414	415.045354	6.788954
5.988155	429.314988	6.793958
6.002689	434.458970	6.798963
5.913466	422.386562	6.803968
6.279187	400.817744	6.808973
5.817360	403.822821	6.813978
5.727480	395.619736	6.818982
5.742826	380.686635	6.823987
5.635456	403.456644	6.828992
5.584958	395.962845	6.833997
5.651908	380.470758	6.839002
5.730128	377.612493	6.844006
5.763691	401.525825	6.849011
5.185086	413.751450	6.854016
6.051417	403.263376	6.859021
5.581367	427.032984	6.864026
5.905506	423.423603	6.869030
5.954630	413.215882	6.874035
5.948366	407.704806	6.879040
5.821846	381.221307	6.884045
5.812258	395.760990	6.889050
5.682416	417.119620	6.894054
5.683749	395.306106	6.899059
5.478813	385.407037	6.904064
5.724730	394.574223	6.909069
5.466170	392.448834	6.914074
5.762475	394.910746	6.919078
5.782416	409.114793	6.924083
5.463558	423.596111	6.929088
5.814012	410.463184	6.934093
5.940872	410.260289	6.939098
5.968478	412.530641	6.944102
5.640566	383.545150	6.949107
5.402533	395.363191	6.954112
5.603383	412.434750	6.959117
5.759361	418.586724	6.964122
5.975605	423.514770	6.969126
5.777120	431.317221	6.974131
5.507130	413.924873	6.979136
5.526856	417.272785	6.984141
5.463495	407.544741	6.989146
5.854908	424.356844	6.994150
5.772336	411.471072	6.999155
5.649346	417.656421	7.004160
5.811240	419.636159	7.009165
5.926744	423.222362	7.014170
6.056940	421.158007	7.019174
6.197723	419.984575	7.024179
5.548262	401.240134	7.029184
5.883134	399.896718	7.034189
5.720511	398.086538	7.039194
5.545954	373.146850	7.044198
5.533931	391.056463	7.049203
5.609215	402.550067	7.054208
5.880533	397.828182	7.059213
5.654591	422.952233	7.064218
5.678315	419.283986	7.069222
5.727225	430.487010	7.074227
5.623893	419.344332	7.079232
5.860055	430.512958	7.084237
5.660305	422.660956	7.089242
5.579453	409.724491	7.094246
5.952172	428.027703	7.099251
5.472068	410.806810	7.104256
6.196103	412.423055	7.109261
5.676706	429.497747	7.114266
5.854109	433.536583	7.119270
5.779569	411.356281	7.124275
5.494842	402.556705	7.129280
5.976117	396.943262	7.134285
5.671187	407.252687	7.139290
5.661301	384.866710	7.144294
5.750079	411.373969	7.149299
5.740303	403.197990	7.154304
5.991935	404.982467	7.159309
5.493686	399.282007	7.164314
5.670157	385.245921	7.169318
5.930482	408.360814	7.174323
5.271779	395.954502	7.179328
5.576914	402.288291	7.184333
5.953154	420.047654	7.189338
5.537954	412.145931	7.194342
5.713200	430.635475	7.199347
5.630646	426.985775	7.204352
5.678398	418.219339	7.209357
5.663677	423.605304	7.214362
5.639783	408.706381	7.219366
5.921665	421.202554	7.224371
5.986222	428.503015	7.229376
5.642477	419.994529	7.234381
5.922644	432.214187	7.239386
5.872194	435.508591	7.244390
5.897976	422.015082	7.249395
5.859581	431.323091	7.254400
5.884408	403.621286	7.259405
5.466236	397.667681	7.264410
5.717152	409.802089	7.269414
5.881664	403.023470	7.274419
5.595764	421.877660	7.279424
6.002622	397.398621	7.284429
5.590970	400.732586	7.289434
5.805810	412.261041	7.294438
5.718247	394.158287	7.299443
5.810386	390.337082	7.304448
5.815771	396.885049	7.309453
5.507971	401.320722	7.314458
5.561128	401.615754	7.319462
5.600097	409.031610	7.324467
5.566408	430.057805	7.329472
5.883735	434.852547	7.334477
5.865329	425.056295	7.339482
5.587012	417.404909	7.344486
5.770634	429.911015	7.349491
5.760140	415.794818	7.354496
5.764851	427.836259	7.359501
5.716333	431.398569	7.364506
5.720442	433.171474	7.369510
5.620060	424.588734	7.374515
5.892898	428.105828	7.379520
6.065368	423.647188	7.384525
5.404002	417.191295	7.389530
5.705629	435.868799	7.394534
5.945429	429.386398	7.399539
5.630843	441.227977	7.404544
6.025687	419.618906	7.409549
5.843405	418.523131	7.414554
5.504528	403.597150	7.419558
5.646004	403.610445	7.424563
5.558957	422.421909	7.429568
5.926589	421.278463	7.434573
5.978408	419.766768	7.439578
5.990194	419.172512	7.444582
6.020755	410.576426	7.449587
5.798917	395.298469	7.454592
5.841001	404.385112	7.459597
5.813735	389.163592	7.464602
5.413710	387.021531	7.469606
5.734558	398.300534	7.474611
5.620192	414.739666	7.479616
5.976130	402.561448	7.484621
5.695326	384.942944	7.489626
5.693429	406.995913	7.494630
6.053182	391.594915	7.499635
5.384157	402.493460	7.504640
5.691538	390.090663	7.509645
5.393468	405.341341	7.514650
5.358811	401.000789	7.519654
5.954580	408.794591	7.524659
5.810480	417.254517	7.529664
5.652378	394.857703	7.534669
5.825482	394.228305	7.539674
5.659949	403.216773	7.544678
5.628324	391.726564	7.549683
5.499040	414.155532	7.554688
6.053271	412.369629	7.559693
5.777092	418.410520	7.564698
5.786531	398.690368	7.569702
5.820831	402.318791	7.574707
5.449498	413.887789	7.579712
5.790097	397.795859	7.584717
5.635257	400.485725	7.589722
5.680959	428.048371	7.594726
6.064258	426.167896	7.599731
5.775295	414.201602	7.604736
5.556835	415.849897	7.609741
5.781449	405.540970	7.614746
5.701116	401.083274	7.619750
5.707747	405.743202	7.624755
5.681223	404.093424	7.629760
5.563398	411.398368	7.634765
5.679497	430.372679	7.639770
5.833333	421.561384	7.644774
5.997789	427.647740	7.649779
6.024996	427.646773	7.654784
5.954983	410.427360	7.659789
5.716200	399.102287	7.664794
5.810226	393.380108	7.669798
5.629116	384.438530	7.674803
5.680535	405.896518	7.679808
5.865543	392.662013	7.684813
5.392065	397.668026	7.689818
5.343928	400.014029	7.694822
5.723408	423.724821	7.699827
5.486299	423.920835	7.704832
5.956325	425.447461	7.709837
5.752386	440.553487	7.714842
5.801363	424.499758	7.719846
6.048874	424.541895	7.724851
5.809415	395.391818	7.729856
6.140994	401.594079	7.734861
5.460049	401.482756	7.739866
5.316460	396.071719	7.744870
5.768102	415.547529	7.749875
5.406540	415.507328	7.754880
5.993744	409.444490	7.759885
5.545124	426.940551	7.764890
5.976041	405.623063	7.769894
5.823146	397.697235	7.774899
5.578084	408.025079	7.779904
5.682542	405.345763	7.784909
5.804258	417.088783	7.789914
5.950854	419.246643	7.794918
6.117211	397.853127	7.799923
5.642559	396.332157	7.804928
5.546913	410.283037	7.809933
5.456789	407.242269	7.814938
5.515409	410.121878	7.819942
5.983362	419.261363	7.824947
5.624151	417.894245	7.829952
5.611439	395.956682	7.834957
5.758910	426.179531	7.839962
5.793053	416.628128	7.844966
5.956885	426.214049	7.849971
5.502647	423.472772	7.854976
5.900050	408.846537	7.859981
6.084411	404.580669	7.864986
5.929250	412.228471	7.869990
5.804778	385.198903	7.874995
5.601774	393.458626	7.880000
5.991545	395.508032	7.885005
5.557451	392.273445	7.890010
5.680661	406.864389	7.895014
5.686681	405.742133	7.900019
5.682504	384.928065	7.905024
5.663061	386.606307	7.910029
5.544113	402.001297	7.915034
5.394698	392.000023	7.920038
5.495330	405.658129	7.925043
5.547710	440.992513	7.930048
5.672380	423.660908	7.935053
5.934124	434.723109	7.940058
5.717537	432.255669	7.945062
6.226677	418.924959	7.950067
5.658175	432.772687	7.955072
5.870894	420.041423	7.960077
5.575580	408.752715	7.965082
5.644577	423.382919	7.970086
5.835926	429.932723	7.975091
5.877497	417.432369	7.980096
5.804246	422.369388	7.985101
5.372285	397.695540	7.990106
5.309125	415.136765	7.995110
5.738586	424.774970	8.000115
5.608215	419.654092	8.005133
5.634185	438.956761	8.010150
5.533078	436.670071	8.015168
5.633539	422.769326	8.020186
6.131177	429.081988	8.025203
5.998931	432.551361	8.030221
5.981165	414.560706	8.035238
5.818926	438.937815	8.040256
5.977182	442.622591	8.045274
5.999077	427.631104	8.050291
5.853663	416.320663	8.055309
5.772948	408.946731	8.060326
5.335045	402.983115	8.065344
5.662381	414.640990	8.070362
5.788884	412.903331	8.075379
5.470688	436.827510	8.080397
5.786177	446.042099	8.085414
5.483595	436.429778	8.090432
5.576319	425.010114	8.095450
5.612484	433.645840	8.100467
5.526674	436.223835	8.105485
5.929384	413.977880	8.110502
5.617748	431.785793	8.115520
5.527905	442.385394	8.120538
5.909334	431.352930	8.125555
5.645276	434.109847	8.130573
5.783116	445.465888	8.135590
6.155250	445.013240	8.140608
5.945957	451.782898	8.145626
5.735875	432.025795	8.150643
5.992697	456.523684	8.155661
6.054070	463.928345	8.160678
6.031262	446.248044	8.165696
5.678480	429.849208	8.170714
5.919163	429.091507	8.175731
5.425976	443.480521	8.180749
6.069312	458.461427	8.185766
6.288832	458.861028	8.190784
5.812254	447.764104	8.195802
6.070474	454.850485	8.200819
5.745089	441.230472	8.205837
6.019030	450.943326	8.210854
6.094275	465.370569	8.215872
5.692618	434.758843	8.220890
6.082207	446.733034	8.225907
5.968299	463.523942	8.230925
6.106727	458.376121	8.235942
6.042132	456.212392	8.240960
5.777800	451.418552	8.245978
5.841194	448.431146	8.250995
5.956775	468.659228	8.256013
6.273361	459.961604	8.261030
6.257443	460.521536	8.266048
5.797872	445.323557	8.271066
6.224747	440.636394	8.276083
5.654146	450.913007	8.281101
5.898758	466.508870	8.286118
6.012616	459.711542	8.291136
5.663693	460.407586	8.296154
6.063278	469.025878	8.301171
5.985077	472.502564	8.306189
5.872000	464.772835	8.311206
5.981907	479.895050	8.316224
5.695355	468.298927	8.321242
6.304442	476.544312	8.326259
6.160487	463.977552	8.331277
6.190870	482.011205	8.336294
6.247790	468.760050	8.341312
5.979382	473.007724	8.346330
6.119764	459.482326	8.351347
5.977615	462.343771	8.356365
6.119169	462.974207	8.361382
6.106477	449.403467	8.366400
6.337422	472.323627	8.371418
6.331089	480.982933	8.376435
5.953482	477.023125	8.381453
6.060200	465.749796	8.386470
6.367311	474.596503	8.391488
6.258748	458.115852	8.396506
6.275572	464.827976	8.401523
6.202142	464.898243	8.406541
6.454419	460.595043	8.411558
6.518235	458.881514	8.416576
5.867941	459.579246	8.421594
5.946823	435.036853	8.426611
6.092807	449.349369	8.431629
5.938502	458.519788	8.436646
6.231238	481.497743	8.441664
6.039805	467.898471	8.446682
6.686333	471.356245	8.451699
6.266235	471.549827	8.456717
6.093035	459.321864	8.461734
6.084346	469.320838	8.466752
5.866403	476.131885	8.471770
6.087414	457.702620	8.476787
6.130640	473.483500	8.481805
6.176542	484.253851	8.486822
6.413691	463.041595	8.491840
6.337505	470.792621	8.496858
6.392022	472.334530	8.501875
6.048563	459.969888	8.506893
6.420409	474.294398	8.511910
6.258023	467.029872	8.516928
6.233632	479.151418	8.521946
6.529426	475.192498	8.526963
6.298905	458.043121	8.531981
6.208911	474.606727	8.536998
6.231012	462.490048	8.542016
6.214785	469.253194	8.547034
6.330646	462.607755	8.552051
6.298938	468.609896	8.557069
6.443240	482.602536	8.562087
6.288723	468.514621	8.567104
6.188543	472.470986	8.572122
6.171594	473.316342	8.577139
6.383958	462.253445	8.582157
5.839662	466.450182	8.587175
6.392709	471.977154	8.592192
5.880039	461.077667	8.597210
6.336829	465.870659	8.602227
6.143177	487.497223	8.607245
6.599047	473.610709	8.612263
6.434496	470.263935	8.617280
6.457707	487.374336	8.622298
6.182125	473.814252	8.627315
6.631596	465.162657	8.632333
6.292217	469.239531	8.637351
6.313521	469.482573	8.642368
6.396305	474.717878	8.647386
6.541136	490.458172	8.652403
6.538235	471.613757	8.657421
6.453463	463.377131	8.662439
6.692099	472.413448	8.667456
6.099770	471.956453	8.672474
5.955981	471.566138	8.677491
6.400338	483.725839	8.682509
6.415959	501.820698	8.687527
6.696218	497.183133	8.692544
6.566835	491.533945	8.697562
6.619667	498.496853	8.702579
6.738332	491.428320	8.707597
6.215829	475.669023	8.712615
6.744584	482.634254	8.717632
6.191899	491.892373	8.722650
6.499055	484.420260	8.727667
6.670754	497.688609	8.732685
6.505124	488.648140	8.737703
6.510204	499.771214	8.742720
6.212199	511.900708	8.747738
6.596036	509.011868	8.752755
6.766671	485.018936	8.757773
6.534479	492.706410	8.762791
7.022806	502.614512	8.767808
6.394822	499.140241	8.772826
6.665895	472.413877	8.777843
6.459475	488.531418	8.782861
6.372725	491.576276	8.787879
6.639818	500.513840	8.792896
6.254362	511.631401	8.797914
6.761390	490.653761	8.802931
6.515018	492.104196	8.807949
6.404228	506.081156	8.812967
6.952111	493.625173	8.817984
6.353832	505.048495	8.823002
6.454715	503.572370	8.828019
6.518013	493.084127	8.833037
6.354607	498.199344	8.838055
6.682091	493.703639	8.843072
6.430858	494.871689	8.848090
6.291674	503.755465	8.853107
6.622971	500.173241	8.858125
6.303149	504.890904	8.863143
6.616987	488.250381	8.868160
6.424899	519.615425	8.873178
6.502796	506.445099	8.878195
7.082631	517.908906	8.883213
6.644711	523.119090	8.888231
6.862297	494.585008	8.893248
6.809152	512.355214	8.898266
6.601806	491.319399	8.903283
6.856985	504.606725	8.908301
6.474795	505.676964	8.913319
6.858734	500.722151	8.918336
6.508114	511.635292	8.923354
6.929966	510.098349	8.928371
7.020191	507.883151	8.933389
6.606883	502.569579	8.938407
6.689322	495.899342	8.943424
6.516524	512.377192	8.948442
6.778584	527.028963	8.953459
6.954226	527.632809	8.958477
6.712017	532.015205	8.963495
6.820529	524.716018	8.968512
6.812036	536.011196	8.973530
6.637510	533.120753	8.978547
7.160825	521.562848	8.983565
6.617703	533.218249	8.988583
6.522413	523.711932	8.993600
6.444799	537.449645	8.998618
6.543934	537.666345	9.003635
6.830995	536.743047	9.008653
6.485245	537.409246	9.013671
6.819131	538.509435	9.018688
6.803260	544.732155	9.023706
6.742511	521.764333	9.028723
6.818201	530.738367	9.033741
6.423834	530.183908	9.038759
6.842350	512.033858	9.043776
6.799706	532.373681	9.048794
6.461101	536.233674	9.053811
6.922841	560.296500	9.058829
6.726615	581.680385	9.063847
7.198118	557.491987	9.068864
7.308668	560.170489	9.073882
6.969107	542.853360	9.078899
7.079295	528.235954	9.083917
6.920954	536.828410	9.088935
7.068986	527.008727	9.093952
6.913879	536.755838	9.098970
6.999871	550.194061	9.103987
6.695936	545.497459	9.109005
6.854710	523.542967	9.114023
7.263835	537.466998	9.119040
7.041872	536.983626	9.124058
7.049780	525.979071	9.129075
7.056286	537.171504	9.134093
6.649848	554.588252	9.139111
7.219829	542.744745	9.144128
6.882416	547.984967	9.149146
6.952217	539.114952	9.154163
7.200037	549.852079	9.159181
6.854632	533.423279	9.164199
7.158080	558.336932	9.169216
7.377737	556.300575	9.174234
7.380015	540.441300	9.179251
6.940759	528.874401	9.184269
6.784996	538.659997	9.189287
6.806723	527.428417	9.194304
7.062793	552.112259	9.199322
6.869774	546.013361	9.204339
6.989286	542.760041	9.209357
6.908067	567.695855	9.214375
7.405283	564.137167	9.219392
7.371460	569.518806	9.224410
7.389680	565.832246	9.229427
6.764251	550.199200	9.234445
6.583864	567.023249	9.239463
7.199128	556.671536	9.244480
7.313761	554.437930	9.249498
7.426420	560.931461	9.254515
7.465843	561.125560	9.259533
6.999133	579.047140	9.264551
7.257248	577.052443	9.269568
7.463441	561.958439	9.274586
7.386800	548.411560	9.279603
7.378454	538.771114	9.284621
6.957842	543.885557	9.289639
7.149562	527.458622	9.294656
6.933096	548.918422	9.299674
7.447266	570.018599	9.304691
7.312292	549.897354	9.309709
7.098094	558.998423	9.314727
7.336024	542.658987	9.319744
7.297249	549.488671	9.324762
7.005981	544.399436	9.329779
7.554611	539.097208	9.334797
7.024622	553.795963	9.339815
7.317313	550.716328	9.344832
7.600918	569.052433	9.349850
7.017581	571.216057	9.354867
7.486353	550.211986	9.359885
7.488232	549.296948	9.364903
7.213538	555.419670	9.369920
6.930113	552.467419	9.374938
6.992015	572.772504	9.379955
7.414001	564.024145	9.384973
7.485509	573.280608	9.389991
7.480440	579.705733	9.395008
7.678765	556.458495	9.400026
7.158550	566.224833	9.405043
7.122394	551.562413	9.410061
7.320188	568.949679	9.415079
7.396511	559.120079	9.420096
7.168674	565.943626	9.425114
7.499032	566.655826	9.430131
7.643712	564.782211	9.435149
7.577587	567.484203	9.440167
7.243130	557.729869	9.445184
7.343226	563.820473	9.450202
7.207546	559.427069	9.455219
7.730121	563.650223	9.460237
7.447619	576.823474	9.465255
7.096127	576.947171	9.470272
7.162175	563.884728	9.475290
7.403502	572.988161	9.480307
7.818895	563.716233	9.485325
7.695291	571.933878	9.490343
7.545254	584.513158	9.495360
7.460892	571.512267	9.500378
7.350892	585.566313	9.505395
7.658742	564.300315	9.510413
7.547188	577.841466	9.515431
7.571185	555.840517	9.520448
7.951428	563.819327	9.525466
7.717982	553.966336	9.530483
7.297030	548.442061	9.535501
7.225648	539.036479	9.540519
7.222051	567.129447	9.545536
7.524961	564.818675	9.550554
7.340118	575.646116	9.555571
7.708793	578.207475	9.560589
7.862616	571.722795	9.565607
7.454050	566.549027	9.570624
7.675519	576.106505	9.575642
7.449260	564.606024	9.580659
7.603346	571.743419	9.585677
7.587148	573.044732	9.590695
7.387474	566.512203	9.595712
7.717733	578.208587	9.600730
7.527667	586.115658	9.605747
7.730775	563.586319	9.610765
7.516972	569.539284	9.615783
7.399798	576.937690	9.620800
7.673902	570.793073	9.625818
7.426373	585.147033	9.630835
7.583377	572.885468	9.635853
7.662166	586.724115	9.640871
7.614253	578.403207	9.645888
7.486193	577.440861	9.650906
7.348476	578.045624	9.655923
7.479515	572.941887	9.660941
7.665184	566.320388	9.665959
7.429804	564.178472	9.670976
7.641794	583.956151	9.675994
7.729174	585.414709	9.681011
7.939680	589.277448	9.686029
7.771413	600.481984	9.691047
7.456703	586.298026	9.696064
7.959385	599.632894	9.701082
7.645024	594.797880	9.706099
7.784108	576.229790	9.711117
8.025419	599.697391	9.716135
7.743070	588.740364	9.721152
7.947003	578.981863	9.726170
7.673032	574.449741	9.731187
7.842729	560.162630	9.736205
7.598781	585.023326	9.741223
7.417785	589.385783	9.746240
8.114148	603.695063	9.751258
8.281162	606.221662	9.756275
7.791548	582.048399	9.761293
7.763174	586.503021	9.766311
7.453300	579.968330	9.771328
7.882294	593.105978	9.776346
7.767103	598.773539	9.781363
7.836619	604.993193	9.786381
8.048663	602.384919	9.791399
7.855847	623.380018	9.796416
7.994060	605.812550	9.801434
7.762483	625.630917	9.806451
8.146676	605.956040	9.811469
8.135466	602.250031	9.816487
7.793029	600.441660	9.821504
8.061506	580.518591	9.826522
7.732707	573.977976	9.831539
8.225036	591.529132	9.836557
7.755126	602.825239	9.841575
7.779323	607.606422	9.846592
7.907269	595.718142	9.851610
7.654303	613.530247	9.856627
7.678102	610.312803	9.861645
7.647202	604.254886	9.866663
7.522669	614.837413	9.871680
8.083354	614.533374	9.876698
7.549114	611.773406	9.881715
7.926281	618.356775	9.886733
7.882972	612.300413	9.891751
7.835426	617.762466	9.896768
8.243644	617.769766	9.901786
7.843305	629.445726	9.906803
8.189197	627.972394	9.911821
8.088186	613.111145	9.916839
7.979803	618.022283	9.921856
8.108661	620.684977	9.926874
8.170068	639.509829	9.931891
8.216969	628.375168	9.936909
8.137208	627.840250	9.941927
7.834032	613.068005	9.946944
8.363076	622.149996	9.951962
8.120570	607.223872	9.956979
7.944664	595.588113	9.961997
8.212765	628.492832	9.967015
8.121786	626.791976	9.972032
8.307687	623.962588	9.977050
8.137141	632.245389	9.982067
8.202515	620.205171	9.987085
8.344748	608.976543	9.992103
7.636702	623.559752	9.997120
8.111229	625.063950	10.002138
8.350115	633.407007	10.007155
8.066698	651.470971	10.012173
8.432006	629.819997	10.017191
8.044043	632.622615	10.022208
8.285998	644.281197	10.027226
8.275657	632.246791	10.032243
8.528738	633.422036	10.037261
8.509240	647.690057	10.042279
8.332208	627.242584	10.047296
8.436996	620.170283	10.052314
8.208783	618.002477	10.057331
8.087916	611.877558	10.062349
8.064560	609.365255	10.067367
8.188350	612.377411	10.072384
8.179040	633.833697	10.077402
8.119384	637.568603	10.082419
8.446663	641.354889	10.087437
8.816891	625.952491	10.092455
8.560715	632.056242	10.097472
8.338477	604.584429	10.102490
8.405424	615.015168	10.107507
8.196361	614.742005	10.112525
8.158873	605.601178	10.117543
8.090885	629.609372	10.122560
8.342601	629.983978	10.127578
8.592915	637.262348	10.132595
8.641590	635.228850	10.137613
8.653028	624.929748	10.142631
8.338794	617.350475	10.147648
8.691289	610.335248	10.152666
8.244282	611.144724	10.157683
8.106287	619.498495	10.162701
8.743145	607.346625	10.167719
8.530929	623.639725	10.172736
8.748525	598.279876	10.177754
8.378150	598.968942	10.182771
8.278564	619.549230	10.187789
8.341362	604.720252	10.192807
7.944295	609.208456	10.197824
8.218274	633.844700	10.202842
8.260080	640.307663	10.207859
8.080488	624.377597	10.212877
8.292177	635.689497	10.217895
8.315660	645.696160	10.222912
8.430022	631.764983	10.227930
8.471424	635.653515	10.232947
8.296487	650.589670	10.237965
8.324055	626.684611	10.242983
8.249524	654.869066	10.248000
8.609434	661.474100	10.253018
8.657378	657.679681	10.258035
8.623629	667.729567	10.263053
9.213011	680.352630	10.268071
8.692158	667.818764	10.273088
8.292206	642.580675	10.278106
8.432953	640.930278	10.283123
8.543614	668.933604	10.288141
8.879449	672.185458	10.293159
8.513241	666.240394	10.298176
9.090059	671.133366	10.303194
8.981405	662.116441	10.308211
8.317992	631.374396	10.313229
8.820971	635.978855	10.318247
8.740497	639.709526	10.323264
8.429974	625.551703	10.328282
8.290439	654.402036	10.333299
8.401643	672.660484	10.338317
8.892417	676.001270	10.343335
8.951160	679.744466	10.348352
9.059654	675.979495	10.353370
9.049664	652.579482	10.358387
8.587447	647.754323	10.363405
8.668197	637.591355	10.368423
8.847904	630.763882	10.373440
8.690595	658.502700	10.378458
8.751488	642.100313	10.383475
8.569555	634.496216	10.388493
9.200724	665.060926	10.393511
9.150926	655.452644	10.398528
8.951233	648.627642	10.403546
8.980164	645.919146	10.408563
8.867228	631.600155	10.413581
8.849386	629.337756	10.418599
8.698417	659.579373	10.423616
8.741771	644.577929	10.428634
8.946017	634.028414	10.433651
8.974981	645.291111	10.438669
8.888146	641.134429	10.443687
8.606854	637.813110	10.448704
8.383797	639.622402	10.453722
8.555558	636.868754	10.458739
8.970891	666.247224	10.463757
8.812366	677.664813	10.468775
8.547354	675.169705	10.473792
8.991515	680.307181	10.478810
8.572668	669.359174	10.483827
8.569158	667.049826	10.488845
8.680032	671.149956	10.493863
8.537639	672.784745	10.498880
8.712073	671.077708	10.503898
8.729848	678.899903	10.508915
8.658420	697.284107	10.513933
8.795087	704.685986	10.518951
8.922557	717.099960	10.523968
9.063614	706.058807	10.528986
9.408339	719.739877	10.534003
8.832559	712.040241	10.539021
9.403561	719.054588	10.544039
9.088837	711.260249	10.549056
8.805904	710.425528	10.554074
9.336054	693.300632	10.559091
8.864398	713.609552	10.564109
8.793583	729.791724	10.569127
8.846950	720.649196	10.574144
8.814870	700.446693	10.579162
8.986679	702.718155	10.584179
8.665717	718.716222	10.589197
9.040716	703.733712	10.594215
9.039512	730.432862	10.599232
9.119455	718.306127	10.604250
9.222466	699.588575	10.609267
9.078730	718.871230	10.614285
9.101312	695.510147	10.619303
9.078636	706.307535	10.624320
8.844286	719.171750	10.629338
9.228360	732.821139	10.634355
9.240576	748.108839	10.639373
9.527094	742.598351	10.644391
9.134999	731.900534	10.649408
8.990130	741.109611	10.654426
9.432668	738.830153	10.659443
9.507271	737.662894	10.664461
9.231456	729.865855	10.669479
8.954588	712.831008	10.674496
9.053537	745.196071	10.679514
9.468739	740.042367	10.684531
9.428940	746.830096	10.689549
9.358196	740.917650	10.694567
9.447717	732.760412	10.699584
9.131706	718.313428	10.704602
9.375575	738.545954	10.709619
9.221652	742.990571	10.714637
9.195381	739.159493	10.719655
9.484576	743.931562	10.724672
9.578480	738.375270	10.729690
9.663087	744.992380	10.734707
9.110574	728.804726	10.739725
9.433990	720.601757	10.744743
9.627963	738.046129	10.749760
9.375212	713.786283	10.754778
9.656789	710.980329	10.759795
9.150730	726.376288	10.764813
9.108097	710.055586	10.769831
9.249602	732.112903	10.774848
9.274620	741.705902	10.779866
9.617283	733.657872	10.784883
9.259902	743.334042	10.789901
9.584330	744.432266	10.794919
9.933099	740.198552	10.799936
9.605110	753.457599	10.804954
9.541160	740.755080	10.809971
9.461678	717.491124	10.814989
9.772951	733.423592	10.820007
9.468982	714.430752	10.825024
9.560532	713.078066	10.830042
9.271956	719.198423	10.835059
9.528744	714.758912	10.840077
9.596125	727.720575	10.845095
9.529912	749.674387	10.850112
9.607844	749.836244	10.855130
9.947465	745.760691	10.860147
9.774964	726.413029	10.865165
9.468155	717.778429	10.870183
9.300800	720.905533	10.875200
9.056773	720.710962	10.880218
9.827313	745.003878	10.885235
9.649692	740.423508	10.890253
9.839231	747.380074	10.895271
9.913108	737.115251	10.900288
9.691727	750.403910	10.905306
9.760379	733.079718	10.910323
9.488526	734.256212	10.915341
9.744856	753.453214	10.920359
9.764530	732.904705	10.925376
9.957931	727.955823	10.930394
9.598039	729.327723	10.935411
9.636451	723.724519	10.940429
9.709234	739.973596	10.945447
9.724270	752.263303	10.950464
9.525936	741.147440	10.955482
9.735457	756.065623	10.960499
9.469085	740.970917	10.965517
9.416063	753.136672	10.970535
9.874849	742.810597	10.975552
9.769287	751.412360	10.980570
9.860220	736.018124	10.985587
9.703851	743.849844	10.990605
9.483717	737.404656	10.995623
9.857791	743.264570	11.000640
9.723054	757.196123	11.005658
9.935742	745.647369	11.010675
9.673908	761.596842	11.015693
9.756818	745.612445	11.020711
9.934960	744.026409	11.025728
9.662439	754.499371	11.030746
9.545500	738.277607	11.035763
9.721851	759.798638	11.040781
10.059467	763.221235	11.045799
9.985492	759.335650	11.050816
10.024275	777.070900	11.055834
9.765811	772.299014	11.060851
9.591818	753.299700	11.065869
9.841836	773.776665	11.070887
10.162329	764.587211	11.075904
9.796787	792.045215	11.080922
10.235377	763.247200	11.085939
10.273674	759.732132	11.090957
10.343392	772.338520	11.095975
10.449471	756.938710	11.100992
10.031844	749.553773	11.106010
10.005312	750.260018	11.111027
9.988635	757.067054	11.116045
10.053871	745.555657	11.121063
10.190863	736.532630	11.126080
9.957776	742.066028	11.131098
9.948274	747.560707	11.136115
9.772835	745.729641	11.141133
10.195644	763.785365	11.146151
10.301099	748.056128	11.151168
10.140410	737.258664	11.156186
10.234160	750.737110	11.161203
10.117058	731.894520	11.166221
9.907099	744.764566	11.171239
10.158513	758.028430	11.176256
9.927915	764.568343	11.181274
10.309273	753.657773	11.186291
10.155363	764.454651	11.191309
9.919984	770.911029	11.196327
9.916743	760.864589	11.201344
9.717032	774.460333	11.206362
10.033857	786.759529	11.211379
10.303159	770.372059	11.216397
10.100321	776.276257	11.221415
10.625472	777.884969	11.226432
10.144779	772.686445	11.231450
10.250049	761.063034	11.236467
10.165061	780.872432	11.241485
9.854690	772.217530	11.246503
10.032290	770.814111	11.251520
9.964358	786.133200	11.256538
10.189122	779.548936	11.261555
10.331054	798.413615	11.266573
10.163228	813.406710	11.271591
10.298832	807.442227	11.276608
10.144630	822.188360	11.281626
10.118996	816.436398	11.286643
10.453312	804.785630	11.291661
10.241064	813.794918	11.296679
10.593812	795.885067	11.301696
10.348916	806.563482	11.306714
10.308887	817.841743	11.311731
10.286749	812.210334	11.316749
10.213497	819.656012	11.321767
10.431914	820.140824	11.326784
10.357568	811.718575	11.331802
10.347253	807.292674	11.336819
10.323761	808.811002	11.341837
10.076308	799.145653	11.346855
10.588044	801.641589	11.351872
10.480623	801.588276	11.356890
10.274204	809.413737	11.361907
10.369383	829.966746	11.366925
10.427403	835.443311	11.371943
10.731276	843.471197	11.376960
10.391331	841.384701	11.381978
10.917560	821.603124	11.386995
10.982922	832.844496	11.392013
10.693741	817.891342	11.397031
10.551528	820.206450	11.402048
10.512966	826.713572	11.407066
10.380472	800.601710	11.412083
10.672146	822.014424	11.417101
10.572353	827.610546	11.422119
10.704547	836.692911	11.427136
10.366185	825.835105	11.432154
10.341001	821.631679	11.437171
10.855550	832.294028	11.442189
10.509609	835.785916	11.447207
10.974706	842.031018	11.452224
10.809402	843.961759	11.457242
10.900632	826.842535	11.462259
10.947663	845.145840	11.467277
11.189460	825.185633	11.472295
11.093388	805.705980	11.477312
10.864978	814.665885	11.482330
10.629211	821.070786	11.487347
10.523056	798.705863	11.492365
10.696126	811.815540	11.497383
10.588642	804.210371	11.502400
10.607791	800.071161	11.507418
10.713424	814.346210	11.512435
10.915204	831.117133	11.517453
10.671266	837.793597	11.522471
11.236177	841.935442	11.527488
10.700130	832.658030	11.532506
10.827444	826.827651	11.537523
10.879100	821.234621	11.542541
10.609053	836.879506	11.547559
10.637478	845.134558	11.552576
10.493845	832.711499	11.557594
10.422219	854.583603	11.562611
10.872168	836.936801	11.567629
10.877708	825.694885	11.572647
11.164493	834.440955	11.577664
10.888163	823.278291	11.582682
10.748092	834.774914	11.587699
11.067352	823.632494	11.592717
10.672414	834.763369	11.597735
10.662930	848.516473	11.602752
10.650842	835.306024	11.607770
10.722291	851.662893	11.612787
11.376640	867.193913	11.617805
10.828685	876.913763	11.622823
11.235389	872.532776	11.627840
10.993893	862.124467	11.632858
11.188362	881.688553	11.637875
11.410237	865.145475	11.642893
11.125149	884.139375	11.647911
11.382818	868.809554	11.652928
10.980144	863.300939	11.657946
10.770098	864.192496	11.662963
11.180267	858.704729	11.667981
10.883847	874.793367	11.672999
11.277810	851.797531	11.678016
11.185800	868.544329	11.683034
11.134445	860.976792	11.688051
11.440382	862.055253	11.693069
11.264958	879.954629	11.698087
11.210232	868.890020	11.703104
11.520493	866.603769	11.708122
11.267347	874.483627	11.713139
11.150961	854.873641	11.718157
10.929396	856.966890	11.723175
11.559373	860.035761	11.728192
11.241573	880.475833	11.733210
11.069090	877.670005	11.738227
11.234987	869.145144	11.743245
11.225943	883.824740	11.748263
11.192937	879.364095	11.753280
11.341998	874.681876	11.758298
11.134687	884.174712	11.763315
11.400261	862.921093	11.768333
11.407798	874.466267	11.773351
11.450636	865.662610	11.778368
11.300719	874.551030	11.783386
11.143182	891.798123	11.788403
11.323536	886.545028	11.793421
11.345722	873.024728	11.798439
11.282009	859.006858	11.803456
10.951055	871.018688	11.808474
11.038110	869.148656	11.813491
11.283094	873.674299	11.818509
11.072840	886.672235	11.823527
11.674011	895.784585	11.828544
11.626844	911.823608	11.833562
11.325261	896.859634	11.838579
11.592612	902.867234	11.843597
11.653599	913.408976	11.848615
11.684991	890.720575	11.853632
11.726406	886.305192	11.858650
11.200771	875.906142	11.863667
11.411826	884.997741	11.868685
11.649960	901.816756	11.873703
11.726971	898.913801	11.878720
11.685905	909.213907	11.883738
11.416845	907.429191	11.888755
11.446274	911.294778	11.893773
11.620661	901.379677	11.898791
11.974440	902.306570	11.903808
11.698465	905.262438	11.908826
11.600413	900.890370	11.913843
11.922498	909.050285	11.918861
11.552271	900.582223	11.923879
11.426089	899.638635	11.928896
11.892785	898.366715	11.933914
11.821612	912.539809	11.938931
11.768604	915.123583	11.943949
11.900135	911.189828	11.948967
11.983068	895.172406	11.953984
11.884023	888.163089	11.959002
11.642519	865.975021	11.964019
11.776598	860.094115	11.969037
11.587611	864.765568	11.974055
11.881135	876.687388	11.979072
11.775349	888.814148	11.984090
11.666427	893.583964	11.989107
11.908445	905.472498	11.994125
11.740501	902.799050	11.999143
11.525911	901.970637	12.004160
11.919418	888.908315	12.009178
11.811200	917.783980	12.014195
11.890507	899.294651	12.019213
11.926480	906.629432	12.024231
12.049039	907.686048	12.029248
12.155204	910.002239	12.034266
11.922458	917.244657	12.039283
12.164158	901.894220	12.044301
11.924841	887.226580	12.049319
11.732198	906.996860	12.054336
11.951556	893.312692	12.059354
11.687324	903.332040	12.064371
11.999867	910.972406	12.069389
11.776035	914.586517	12.074407
11.886495	895.418101	12.079424
12.232351	900.384938	12.084442
11.802906	906.118321	12.089459
11.743403	893.050072	12.094477
11.782083	912.852979	12.099495
12.032571	894.384272	12.104512
11.956652	910.648953	12.109530
11.779375	910.962212	12.114547
12.180509	906.421055	12.119565
12.232241	934.171188	12.124583
11.944831	913.982358	12.129600
12.349544	923.138605	12.134618
12.175252	910.324095	12.139635
11.927030	919.665192	12.144653
12.127153	943.409743	12.149671
12.041463	934.329330	12.154688
11.945218	941.560321	12.159706
11.979879	942.916236	12.164723
12.148421	931.023251	12.169741
11.916442	950.805376	12.174759
12.104768	928.693712	12.179776
12.101058	944.213512	12.184794
12.151318	937.548598	12.189811
12.211652	942.706986	12.194829
11.892121	932.629062	12.199847
11.610837	941.080095	12.204864
12.181857	962.419953	12.209882
12.161271	965.269962	12.214899
12.640222	968.057395	12.219917
12.588283	969.657094	12.224935
12.407672	958.451059	12.229952
12.495909	972.318112	12.234970
12.568739	969.376474	12.239987
12.524655	971.503975	12.245005
12.813947	983.785150	12.250023
12.463644	956.596992	12.255040
12.374411	940.138235	12.260058
12.465321	952.503215	12.265075
12.842991	924.244779	12.270093
12.634841	934.370204	12.275111
12.205580	954.800529	12.280128
12.379056	930.014825	12.285146
12.340456	926.063229	12.290163
12.033531	940.222270	12.295181
12.483848	959.944297	12.300199
12.173389	982.326602	12.305216
12.461855	963.992248	12.310234
12.377978	977.018774	12.315251
12.725523	976.877776	12.320269
12.636302	963.268649	12.325287
12.401126	966.862999	12.330304
12.451686	979.818602	12.335322
12.488577	967.599892	12.340339
12.559653	975.920586	12.345357
12.962783	967.719367	12.350375
12.852003	988.367929	12.355392
12.784451	973.791968	12.360410
12.456731	979.944186	12.365427
12.463181	970.510519	12.370445
12.648389	963.320859	12.375463
12.639993	978.929931	12.380480
12.856923	952.355639	12.385498
12.578754	978.708669	12.390515
12.789502	978.071412	12.395533
12.685037	970.669744	12.400551
12.399948	980.103957	12.405568
12.785302	973.342027	12.410586
12.923484	993.429503	12.415603
12.792737	1000.675079	12.420621
13.111082	988.375105	12.425639
12.800395	1002.177926	12.430656
12.698216	977.611057	12.435674
12.738781	986.273624	12.440691
12.771977	1013.749080	12.445709
12.912963	1007.282181	12.450727
12.907469	1001.924556	12.455744
12.918015	1011.776646	12.460762
12.687467	1008.994755	12.465779
13.105873	1003.779918	12.470797
12.899234	1000.143009	12.475815
12.876897	1007.239406	12.480832
13.513481	1001.900543	12.485850
13.234571	998.465098	12.490867
12.890672	970.815242	12.495885
13.015767	983.007144	12.500903
13.051683	995.209167	12.505920
13.063856	983.158170	12.510938
13.395101	995.289150	12.515955
12.964946	987.435616	12.520973
12.987116	976.172047	12.525991
12.922694	977.884117	12.531008
13.278075	984.036118	12.536026
13.228712	989.381112	12.541043
13.299123	998.391619	12.546061
13.163503	968.726147	12.551079
12.869919	977.008999	12.556096
13.075235	977.909755	12.561114
13.375084	1009.887148	12.566131
13.154555	976.947630	12.571149
13.211281	993.945112	12.576167
13.140649	1008.255179	12.581184
13.077135	982.780856	12.586202
13.205383	1005.811185	12.591219
13.146570	999.344737	12.596237
13.029830	1009.903419	12.601255
13.080569	1018.128800	12.606272
13.050215	999.132406	12.611290
12.970444	1015.816530	12.616307
12.785784	1019.985470	12.621325
13.219050	1000.222373	12.626343
13.108430	1017.759221	12.631360
13.128952	1026.199785	12.636378
13.164089	1034.482760	12.641395
13.124342	1048.521389	12.646413
13.476971	1041.952684	12.651431
13.420977	1049.379288	12.656448
13.344551	1042.831107	12.661466
13.399099	1026.802593	12.666483
13.299462	1038.852686	12.671501
13.973013	1024.667463	12.676519
13.311436	1037.321022	12.681536
13.691386	1050.222939	12.686554
13.587346	1044.406308	12.691571
13.398733	1043.411331	12.696589
13.772383	1046.739477	12.701607
13.422478	1046.988769	12.706624
13.859468	1039.748018	12.711642
13.727489	1033.881691	12.716659
13.689867	1039.919276	12.721677
13.908931	1028.914594	12.726695
13.394143	1031.068526	12.731712
13.610939	1010.117278	12.736730
13.765405	1005.213118	12.741747
13.711230	1019.442444	12.746765
13.825585	1000.748333	12.751783
13.433484	1002.154705	12.756800
13.327318	1018.042212	12.761818
13.564558	1015.825079	12.766835
13.544155	1033.692817	12.771853
14.032589	1030.403224	12.776871
13.695447	1022.147585	12.781888
13.773478	1040.963294	12.786906
14.087994	1029.048963	12.791923
13.863746	1034.564572	12.796941
14.012856	1017.383909	12.801959
13.561325	1018.017030	12.806976
13.588124	1018.539616	12.811994
14.120145	1028.873706	12.817011
13.870289	1027.938642	12.822029
13.624470	1008.461436	12.827047
13.650408	1016.342478	12.832064
13.865754	1023.081375	12.837082
13.917217	1027.022268	12.842099
14.076687	1035.250059	12.847117
14.382153	1043.742338	12.852135
13.920583	1026.125020	12.857152
13.491959	1012.765099	12.862170
13.687222	1017.746135	12.867187
13.527999	1033.401737	12.872205
13.954227	1026.853054	12.877223
13.646960	1033.559945	12.882240
13.890421	1027.016177	12.887258
13.970576	1036.239904	12.892275
13.812590	1039.186532	12.897293
13.960704	1025.107625	12.902311
13.579216	1056.638106	12.907328
13.768281	1036.914334	12.912346
13.852915	1068.668227	12.917363
13.845363	1065.472991	12.922381
14.268858	1068.165203	12.927399
14.350970	1070.281802	12.932416
14.157027	1059.833223	12.937434
14.448784	1083.360437	12.942451
14.291822	1095.590086	12.947469
14.314029	1063.238659	12.952487
13.835525	1065.543942	12.957504
14.019951	1077.704761	12.962522
14.159508	1067.030633	12.967539
13.643470	1081.911793	12.972557
14.093648	1059.789508	12.977575
14.335264	1084.401518	12.982592
14.157979	1066.878576	12.987610
14.054853	1075.291482	12.992627
14.424141	1088.098366	12.997645
14.435206	1068.805545	13.002663
13.896180	1061.157615	13.007680
14.112651	1064.279021	13.012698
14.308767	1079.122490	13.017715
14.147878	1074.676229	13.022733
14.494755	1080.014224	13.027751
14.565909	1085.031733	13.032768
14.348864	1071.347693	13.037786
14.274173	1078.422074	13.042803
14.374814	1090.383808	13.047821
14.414323	1086.946202	13.052839
14.534887	1109.191435	13.057856
14.620169	1124.669256	13.062874
14.742720	1092.919245	13.067891
14.565802	1097.783411	13.072909
14.304481	1070.562928	13.077927
14.372436	1093.810193	13.082944
14.634241	1088.790949	13.087962
14.633583	1106.697231	13.092979
14.939086	1094.420549	13.097997
14.460850	1077.516777	13.103015
14.261779	1091.089867	13.108032
14.278471	1106.607837	13.113050
14.637418	1085.691150	13.118067
14.642551	1114.262104	13.123085
14.595384	1093.335768	13.128103
14.576198	1091.833771	13.133120
14.758743	1104.934064	13.138138
14.831167	1108.026246	13.143155
14.568923	1089.533993	13.148173
14.807881	1094.274818	13.153191
14.605227	1095.431441	13.158208
14.652616	1084.515508	13.163226
15.021973	1088.296625	13.168243
14.728619	1106.742792	13.173261
14.957037	1099.092986	13.178279
14.650484	1110.769752	13.183296
14.776477	1093.562615	13.188314
14.895739	1111.408544	13.193331
14.821608	1094.371945	13.198349
15.064549	1077.145204	13.203367
14.845386	1092.481030	13.208384
14.833241	1102.618553	13.213402
15.128208	1098.977546	13.218419
14.818905	1093.150340	13.223437
14.811573	1101.411832	13.228455
14.648627	1090.523176	13.233472
14.854120	1085.105465	13.238490
15.181487	1097.062012	13.243507
15.015804	1119.317467	13.248525
14.964394	1098.765750	13.253543
15.109960	1081.217875	13.258560
14.774859	1086.438020	13.263578
15.001550	1099.569981	13.268595
14.826783	1086.833236	13.273613
14.969507	1096.218370	13.278631
15.018061	1093.733564	13.283648
14.747827	1100.409862	13.288666
15.103110	1112.451944	13.293683
14.755447	1145.946031	13.298701
14.901871	1126.142303	13.303719
15.282791	1133.437408	13.308736
14.852722	1139.469038	13.313754
15.367011	1138.117598	13.318771
15.227378	1129.506405	13.323789
15.147175	1128.361354	13.328807
15.268268	1145.663941	13.333824
15.119638	1129.335413	13.338842
15.459519	1118.827112	13.343859
15.364967	1135.599812	13.348877
15.471961	1118.180386	13.353895
15.141703	1135.499003	13.358912
15.016264	1142.985640	13.363930
15.382240	1136.276239	13.368947
15.138809	1141.537637	13.373965
15.325554	1124.375039	13.378983
15.333954	1117.722672	13.384000
15.262283	1132.330592	13.389018
15.230462	1123.842693	13.394035
15.401068	1140.373693	13.399053
15.389541	1133.003821	13.404071
15.488276	1138.295758	13.409088
15.532795	1139.694244	13.414106
15.553157	1134.355818	13.419123
15.543990	1135.199925	13.424141
15.568632	1134.529259	13.429159
15.647649	1128.908668	13.434176
15.403734	1135.540780	13.439194
15.628157	1143.504609	13.444211
15.580898	1134.826388	13.449229
15.655706	1158.845662	13.454247
15.570102	1132.104572	13.459264
15.675197	1146.562259	13.464282
15.908427	1133.216744	13.469299
15.465737	1120.765923	13.474317
15.618386	1124.354570	13.479335
15.836728	1149.181405	13.484352
15.523130	1137.751802	13.489370
15.904212	1143.846779	13.494387
15.435680	1150.792919	13.499405
15.927623	1142.193755	13.504423
16.098899	1151.339516	13.509440
15.697532	1144.152538	13.514458
15.824826	1129.116280	13.519475
15.902752	1149.684870	13.524493
15.782628	1140.832905	13.529511
15.953634	1117.244239	13.534528
15.671713	1132.386194	13.539546
15.898755	1116.945664	13.544563
15.673603	1144.859820	13.549581
15.689837	1164.257804	13.554599
16.066701	1154.438084	13.559616
15.678914	1160.453485	13.564634
16.022189	1167.748333	13.569651
15.878610	1157.468586	13.574669
15.815176	1145.892051	13.579687
15.824562	1156.547482	13.584704
15.790693	1164.226132	13.589722
16.117661	1144.923814	13.594739
16.286602	1158.563085	13.599757
15.868721	1148.991705	13.604775
16.142640	1160.355212	13.609792
16.039412	1150.757614	13.614810
16.097687	1148.202311	13.619827
15.911179	1151.342113	13.624845
16.149995	1156.620748	13.629863
16.088501	1150.071824	13.634880
15.722415	1175.149478	13.639898
16.026918	1146.545895	13.644915
16.012948	1156.261022	13.649933
16.036722	1156.906327	13.654951
15.951585	1157.181435	13.659968
16.049714	1171.996709	13.664986
16.378682	1170.059405	13.670003
16.461946	1189.232614	13.675021
16.725489	1200.385711	13.680039
16.662835	1164.682450	13.685056
16.061306	1170.785921	13.690074
16.256169	1149.290699	13.695091
16.010422	1165.707013	13.700109
16.407404	1171.295360	13.705127
16.685541	1168.620275	13.710144
16.523130	1188.466315	13.715162
16.689201	1179.048059	13.720179
16.559298	1157.288265	13.725197
16.504960	1157.741704	13.730215
16.693837	1149.778996	13.735232
16.157483	1151.455126	13.740250
16.543400	1144.491306	13.745267
16.525815	1150.124145	13.750285
15.993657	1153.410910	13.755303
16.775892	1165.766932	13.760320
16.514816	1187.562281	13.765338
16.415119	1173.569947	13.770355
16.628031	1184.320571	13.775373
16.421865	1177.092069	13.780391
16.888595	1164.316752	13.785408
16.385727	1181.856420	13.790426
16.244083	1188.083556	13.795443
16.452218	1183.445011	13.800461
16.615118	1168.316336	13.805479
16.458306	1176.173245	13.810496
16.480616	1170.432021	13.815514
16.463798	1186.692738	13.820531
16.830798	1191.183551	13.825549
16.295515	1186.138754	13.830567
16.435033	1186.679323	13.835584
16.770833	1203.709050	13.840602
16.990640	1212.934898	13.845619
17.142857	1206.664339	13.850637
16.726456	1214.285590	13.855655
16.940909	1190.515559	13.860672
16.679775	1190.410302	13.865690
17.056943	1211.044849	13.870707
17.143502	1208.655294	13.875725
16.849382	1203.081678	13.880743
16.860017	1173.922813	13.885760
16.482177	1210.115581	13.890778
17.124406	1215.363387	13.895795
17.024521	1205.798167	13.900813
17.126303	1222.088917	13.905831
17.269107	1208.091606	13.910848
17.103095	1223.832657	13.915866
16.789784	1211.009380	13.920883
16.975158	1209.947668	13.925901
17.197537	1213.364713	13.930919
17.069382	1221.139958	13.935936
17.001447	1219.887680	13.940954
16.957785	1215.637605	13.945971
17.150685	1199.030862	13.950989
17.010650	1215.883984	13.956007
17.093436	1217.936825	13.961024
17.230093	1208.473818	13.966042
16.998289	1220.014721	13.971059
17.260542	1216.551690	13.976077
17.126160	1227.070041	13.981095
17.369627	1213.194641	13.986112
16.962252	1217.018344	13.991130
17.141220	1218.014688	13.996147
17.303266	1218.521227	14.001165
17.249570	1211.628648	14.006183
17.426728	1211.543360	14.011200
17.407551	1214.489223	14.016218
17.193366	1212.399407	14.021235
17.225842	1222.486339	14.026253
16.812613	1238.047347	14.031271
17.322019	1235.180917	14.036288
17.300401	1242.780337	14.041306
17.555137	1259.630458	14.046323
17.520538	1231.450781	14.051341
17.511463	1255.100989	14.056359
17.626246	1245.956953	14.061376
17.743911	1246.787289	14.066394
17.831898	1254.026949	14.071411
17.619850	1248.060805	14.076429
17.692932	1247.609537	14.081447
17.778442	1246.172389	14.086464
17.843408	1237.306017	14.091482
17.684784	1225.600009	14.096499
18.110512	1224.284747	14.101517
17.727286	1219.877450	14.106535
17.855273	1209.529371	14.111552
17.908340	1208.813168	14.116570
17.890125	1205.201849	14.121587
18.094010	1211.785576	14.126605
17.426694	1199.333828	14.131623
17.687261	1195.240323	14.136640
17.497528	1217.284591	14.141658
17.236195	1206.327387	14.146675
17.631250	1233.959530	14.151693
17.907108	1235.696183	14.156711
18.188067	1257.429608	14.161728
17.987023	1228.737214	14.166746
17.706600	1235.867019	14.171763
17.776434	1227.271635	14.176781
17.861781	1226.401313	14.181799
18.061568	1254.489974	14.186816
18.030255	1235.671750	14.191834
17.946994	1244.574855	14.196851
17.946423	1256.294844	14.201869
17.941435	1241.248259	14.206887
17.983467	1242.273237	14.211904
18.085108	1244.756329	14.216922
17.884324	1237.976312	14.221939
18.113725	1242.545674	14.226957
17.834214	1249.569848	14.231975
18.133348	1243.447199	14.236992
18.005780	1249.375055	14.242010
18.016570	1253.442484	14.247027
18.121147	1236.182243	14.252045
18.037598	1232.775764	14.257063
18.113786	1250.243728	14.262080
17.982887	1237.000218	14.267098
17.847851	1248.189500	14.272115
17.895117	1243.514151	14.277133
17.716029	1260.264844	14.282151
18.131137	1282.370532	14.287168
18.152542	1258.563909	14.292186
18.246683	1269.224206	14.297203
18.297285	1265.868270	14.302221
18.488517	1283.658323	14.307239
18.422845	1280.889087	14.312256
18.286446	1263.869970	14.317274
18.637515	1258.088258	14.322291
18.831981	1268.109187	14.327309
18.505812	1279.223311	14.332327
18.406095	1258.249048	14.337344
18.820108	1273.412224	14.342362
18.640601	1264.984865	14.347379
18.871991	1272.597299	14.352397
18.473905	1279.550157	14.357415
18.714257	1254.144234	14.362432
18.586268	1267.083829	14.367450
18.430445	1275.351160	14.372467
18.328539	1254.507057	14.377485
18.562086	1277.333921	14.382503
18.590217	1268.191498	14.387520
18.883731	1246.685840	14.392538
18.566055	1268.513978	14.397555
18.800094	1256.178915	14.402573
18.654035	1255.388358	14.407591
18.687039	1272.005021	14.412608
18.615505	1261.864740	14.417626
18.704630	1275.028342	14.422643
18.965281	1263.799446	14.427661
18.734233	1256.346626	14.432679
18.524190	1267.735183	14.437696
18.573166	1248.997650	14.442714
18.406857	1261.043585	14.447731
18.744684	1272.139783	14.452749
18.773675	1267.112017	14.457767
19.169414	1288.295539	14.462784
19.097740	1286.652133	14.467802
18.942548	1265.283676	14.472819
18.822849	1252.915460	14.477837
18.828473	1272.775760	14.482855
18.843725	1276.772985	14.487872
19.278891	1304.502047	14.492890
18.793150	1304.685621	14.497907
19.283352	1297.146457	14.502925
19.079048	1294.739715	14.507943
19.263394	1302.887474	14.512960
19.484414	1288.292455	14.517978
19.070017	1281.715102	14.522995
19.240546	1271.282803	14.528013
19.239129	1254.330444	14.533031
18.955419	1255.922422	14.538048
19.451986	1257.540340	14.543066
19.487618	1277.823442	14.548083
19.534939	1271.471789	14.553101
19.367929	1265.139912	14.558119
19.189382	1253.663795	14.563136
19.354289	1258.123474	14.568154
19.269073	1261.384225	14.573171
19.294765	1254.343498	14.578189
19.238970	1266.245514	14.583207
19.104683	1266.418930	14.588224
19.048932	1280.484524	14.593242
19.073738	1300.280680	14.598259
19.218111	1286.458687	14.603277
19.529577	1287.784141	14.608295
19.496947	1302.509661	14.613312
19.375723	1296.912456	14.618330
19.226731	1295.147211	14.623347
19.654647	1316.016863	14.628365
19.216335	1293.731791	14.633383
19.229673	1279.597382	14.638400
19.571701	1304.405800	14.643418
19.409445	1311.903426	14.648435
19.366413	1295.225456	14.653453
19.338543	1310.067984	14.658471
19.454677	1321.505608	14.663488
19.914963	1321.372349	14.668506
19.743912	1315.746667	14.673523
19.635774	1322.826294	14.678541
19.650333	1319.907012	14.683559
19.593472	1335.017681	14.688576
19.829519	1332.070945	14.693594
19.735886	1327.370834	14.698611
19.674614	1332.911278	14.703629
19.631866	1337.472702	14.708647
19.718789	1326.247672	14.713664
19.859542	1319.505152	14.718682
19.831352	1334.831209	14.723699
19.743028	1321.132070	14.728717
19.980987	1335.682816	14.733735
20.122332	1332.823466	14.738752
20.179914	1310.924915	14.743770
19.620386	1326.984983	14.748787
20.177825	1316.361478	14.753805
20.071317	1324.158291	14.758823
20.004156	1319.819080	14.763840
19.845869	1317.478532	14.768858
20.046072	1332.512964	14.773875
20.338622	1318.206717	14.778893
20.019830	1324.831800	14.783911
20.003296	1329.827472	14.788928
20.097506	1334.649957	14.793946
20.378516	1343.245930	14.798963
20.527946	1331.323517	14.803981
19.978398	1332.898130	14.808999
20.304536	1330.478017	14.814016
20.431474	1325.866428	14.819034
20.203467	1324.955484	14.824051
20.569351	1306.292350	14.829069
20.597230	1334.499015	14.834087
20.400463	1332.462000	14.839104
20.592995	1309.407057	14.844122
20.230965	1319.401901	14.849139
20.400998	1317.689421	14.854157
20.330873	1311.788164	14.859175
19.959423	1315.343022	14.864192
20.260053	1317.156281	14.869210
20.081997	1350.184992	14.874227
20.551012	1361.367326	14.879245
20.786557	1364.601266	14.884263
20.330028	1366.407403	14.889280
20.723835	1352.601302	14.894298
20.408235	1340.048608	14.899315
20.647159	1348.995654	14.904333
20.636268	1367.429994	14.909351
20.450020	1351.049093	14.914368
20.539311	1363.642696	14.919386
20.327269	1360.212453	14.924403
20.244479	1351.830172	14.929421
20.593381	1358.579422	14.934439
20.560892	1343.772759	14.939456
20.594470	1352.508620	14.944474
20.496677	1349.330304	14.949491
20.580410	1362.379152	14.954509
21.138925	1385.503281	14.959527
21.331368	1370.232941	14.964544
21.235125	1363.430868	14.969562
21.009339	1358.197201	14.974579
20.832421	1346.480543	14.979597
21.173565	1350.964853	14.984615
20.775194	1342.406630	14.989632
20.996371	1358.169149	14.994650
20.934299	1339.427420	14.999667
20.848653	1347.162149	15.004685
21.227491	1344.884177	15.009703
20.784924	1330.315237	15.014720
20.887024	1339.434953	15.019738
21.057640	1359.785501	15.024755
20.951019	1366.159348	15.029773
21.258875	1384.431707	15.034791
21.309787	1374.871080	15.039808
21.644939	1371.546525	15.044826
21.358040	1351.513395	15.049843
21.445075	1348.407760	15.054861
21.381213	1336.839416	15.059879
21.217777	1337.836952	15.064896
21.105643	1341.409775	15.069914
21.166240	1336.294597	15.074931
21.253681	1346.274616	15.079949
21.180315	1343.371040	15.084967
21.040161	1356.893692	15.089984
21.150623	1359.400439	15.095002
21.372756	1380.087699	15.100019
21.392926	1367.712414	15.105037
21.577905	1377.453746	15.110055
21.365973	1371.942748	15.115072
21.858112	1375.499755	15.120090
21.633301	1374.204507	15.125107
21.529319	1364.470710	15.130125
21.924171	1370.117638	15.135143
21.605593	1362.073363	15.140160
21.608416	1363.870798	15.145178
21.445119	1364.975179	15.150195
21.446184	1362.106828	15.155213
21.576677	1366.450501	15.160231
21.102535	1371.995718	15.165248
21.485918	1354.864919	15.170266
21.431959	1373.224610	15.175283
21.471063	1365.621703	15.180301
21.738414	1370.697020	15.185319
21.675125	1365.909225	15.190336
21.693062	1376.674985	15.195354
21.940799	1381.513542	15.200371
21.949578	1371.418465	15.205389
21.892419	1372.001876	15.210407
21.569767	1372.042186	15.215424
21.992121	1363.425666	15.220442
21.497914	1378.656968	15.225459
21.910326	1377.137347	15.230477
22.065439	1396.439560	15.235495
21.893752	1401.015030	15.240512
22.017450	1402.586732	15.245530
22.201074	1400.042949	15.250547
21.809191	1402.046235	15.255565
22.551273	1399.753590	15.260583
22.027698	1371.524964	15.265600
22.078506	1370.089504	15.270618
21.765965	1363.414200	15.275635
22.303643	1379.555738	15.280653
22.495101	1392.866372	15.285671
22.170665	1383.817373	15.290688
22.315712	1393.834841	15.295706
22.358346	1391.718304	15.300723
22.217212	1376.450635	15.305741
22.584225	1360.544308	15.310759
21.975048	1364.820495	15.315776
21.975685	1367.061696	15.320794
22.130052	1396.736018	15.325811
22.434739	1405.473848	15.330829
22.598925	1388.085502	15.335847
22.662013	1410.109128	15.340864
22.692600	1384.817852	15.345882
22.730398	1387.160666	15.350899
22.412453	1394.090197	15.355917
22.415893	1382.204860	15.360935
22.428075	1392.766904	15.365952
22.671260	1392.395863	15.370970
22.471736	1396.125727	15.375987
22.613807	1401.728634	15.381005
22.697427	1389.138462	15.386023
22.515669	1403.872683	15.391040
22.557222	1390.008940	15.396058
22.583360	1403.964484	15.401075
22.547159	1403.703772	15.406093
22.578881	1408.242185	15.411111
22.547892	1411.555508	15.416128
22.840090	1378.031195	15.421146
22.758875	1374.271720	15.426163
22.384521	1394.329193	15.431181
22.707924	1378.214650	15.436199
22.496461	1396.848276	15.441216
22.772972	1392.190202	15.446234
23.002481	1389.596229	15.451251
22.747631	1414.374063	15.456269
23.057776	1405.282177	15.461287
22.713455	1420.305818	15.466304
22.997422	1413.913228	15.471322
22.984221	1419.275520	15.476339
23.047391	1433.845503	15.481357
23.367338	1418.507991	15.486375
23.225327	1425.281324	15.491392
23.165436	1426.179292	15.496410
23.667198	1409.427502	15.501427
22.926694	1397.251899	15.506445
22.907132	1393.132407	15.511463
22.711268	1385.262188	15.516480
22.898368	1407.407705	15.521498
23.200843	1419.180078	15.526515
23.146053	1417.765903	15.531533
23.545452	1429.593806	15.536551
23.462468	1414.810573	15.541568
23.633136	1412.141497	15.546586
23.675801	1403.286094	15.551603
23.093815	1415.114391	15.556621
23.024383	1424.732676	15.561639
23.242387	1426.822537	15.566656
23.131016	1413.304545	15.571674
23.279136	1430.776080	15.576691
23.057831	1425.122057	15.581709
23.353440	1403.320721	15.586727
23.537618	1421.608446	15.591744
23.287895	1408.023874	15.596762
23.621472	1421.431591	15.601779
23.616902	1428.375280	15.606797
23.662868	1422.805014	15.611815
23.650003	1435.943099	15.616832
23.441936	1423.934745	15.621850
23.575797	1418.078657	15.626867
23.301108	1447.418755	15.631885
23.877778	1436.675973	15.636903
23.762936	1452.634639	15.641920
23.396274	1454.023759	15.646938
24.156990	1442.628253	15.651955
23.726012	1464.981287	15.656973
23.880202	1456.366619	15.661991
23.915564	1442.962019	15.667008
24.006869	1445.497432	15.672026
23.981303	1447.285989	15.677043
23.952472	1457.209918	15.682061
23.983900	1428.732317	15.687079
23.816670	1451.726929	15.692096
23.972797	1451.968765	15.697114
24.060965	1440.136984	15.702131
23.881748	1461.216592	15.707149
23.951528	1442.508546	15.712167
23.877419	1433.398665	15.717184
24.080160	1444.276027	15.722202
24.177233	1456.874818	15.727219
23.896353	1447.474170	15.732237
23.763572	1455.877424	15.737255
24.342169	1451.140087	15.742272
24.306037	1479.136090	15.747290
24.227032	1481.587276	15.752307
24.678012	1469.123199	15.757325
24.371898	1471.186615	15.762343
24.451922	1459.583182	15.767360
24.201844	1461.831585	15.772378
24.396515	1462.310010	15.777395
24.500057	1480.722033	15.782413
24.562940	1458.761188	15.787431
24.701564	1458.435766	15.792448
24.403468	1464.284527	15.797466
24.508345	1445.301248	15.802483
24.490809	1463.604941	15.807501
24.605348	1482.882480	15.812519
24.481835	1473.417039	15.817536
24.366923	1483.427143	15.822554
24.832461	1478.861893	15.827571
24.620205	1467.463021	15.832589
24.778217	1474.090556	15.837607
24.305524	1489.855795	15.842624
24.845915	1471.305620	15.847642
25.074124	1477.058259	15.852659
24.969478	1467.050845	15.857677
24.982601	1448.462760	15.862695
24.730337	1455.297034	15.867712
24.611768	1471.484632	15.872730
24.708181	1460.544093	15.877747
24.588763	1485.984946	15.882765
24.395069	1476.734993	15.887783
24.733553	1456.259868	15.892800
24.559582	1474.807981	15.897818
24.800610	1476.753327	15.902835
24.670100	1472.473448	15.907853
25.301673	1499.967303	15.912871
25.138697	1498.349589	15.917888
24.942057	1494.837457	15.922906
25.395729	1490.726133	15.927923
24.991019	1481.879375	15.932941
25.256908	1481.531642	15.937959
25.384823	1483.410168	15.942976
25.093029	1491.499735	15.947994
25.364589	1496.580598	15.953011
25.161867	1480.931256	15.958029
25.184890	1493.870983	15.963047
25.090540	1499.813521	15.968064
25.437878	1491.418829	15.973082
25.586468	1507.862939	15.978099
25.381491	1506.784433	15.983117
25.641742	1505.737487	15.988135
25.573981	1497.524849	15.993152
25.212849	1513.472912	15.998170
25.401832	1496.122857	16.003187
25.349839	1485.688611	16.008205
25.694547	1492.753408	16.013223
25.503237	1485.307391	16.018240
25.672612	1493.522968	16.023258
25.719070	1497.723316	16.028275
25.806799	1501.534743	16.033293
25.442083	1499.649843	16.038311
25.909010	1498.084300	16.043328
25.534565	1485.444479	16.048346
25.628954	1495.737848	16.053363
25.727879	1500.112853	16.058381
25.652544	1517.715981	16.063399
25.602048	1493.860847	16.068416
25.551630	1486.459247	16.073434
25.433229	1495.060990	16.078451
25.718369	1486.259641	16.083469
25.914519	1492.786906	16.088487
25.876163	1506.625374	16.093504
25.744606	1495.325523	16.098522
26.347979	1494.805606	16.103539
25.696797	1500.243049	16.108557
26.010129	1505.770162	16.113575
25.675455	1510.630221	16.118592
25.629488	1537.594221	16.123610
26.212173	1530.176638	16.128627
26.200143	1528.347305	16.133645
25.982108	1523.788434	16.138663
26.291822	1526.832729	16.143680
26.146247	1524.980888	16.148698
26.166702	1514.721814	16.153715
25.963697	1518.302807	16.158733
26.383315	1511.298024	16.163751
26.452237	1523.847891	16.168768
26.437842	1543.447733	16.173786
26.625658	1523.723640	16.178803
26.533204	1526.472859	16.183821
25.925155	1536.986154	16.188839
26.168671	1510.625353	16.193856
26.440829	1521.494054	16.198874
26.578899	1522.966565	16.203891
26.531931	1516.392058	16.208909
26.845139	1524.341611	16.213927
26.829934	1522.860169	16.218944
26.620328	1522.738128	16.223962
26.603504	1527.853866	16.228979
26.746120	1517.021277	16.233997
26.568153	1520.268774	16.239015
26.655319	1511.549330	16.244032
26.642135	1522.303705	16.249050
26.768963	1514.359427	16.254067
26.660629	1519.498650	16.259085
26.577083	1530.421022	16.264103
26.882330	1543.103271	16.269120
26.746269	1536.395675	16.274138
26.932929	1534.995219	16.279155
26.814774	1549.596752	16.284173
26.782287	1572.708422	16.289191
27.016367	1556.503752	16.294208
26.995306	1546.049101	16.299226
26.953407	1546.452376	16.304243
27.165295	1561.642550	16.309261
26.993928	1561.263061	16.314279
27.455816	1538.656464	16.319296
27.017318	1562.194684	16.324314
27.571966	1555.516606	16.329331
27.629344	1544.447645	16.334349
27.132201	1534.783139	16.339367
27.176628	1520.710285	16.344384
27.053480	1534.592312	16.349402
27.018923	1540.762335	16.354419
27.131411	1558.049787	16.359437
26.710774	1545.922462	16.364455
27.380024	1542.792310	16.369472
27.055848	1567.115904	16.374490
27.225829	1544.139614	16.379507
27.049641	1552.021172	16.384525
26.997363	1560.502401	16.389543
27.258339	1559.954340	16.394560
27.349295	1591.702959	16.399578
27.399039	1583.595436	16.404595
27.565473	1580.972001	16.409613
27.243590	1587.161382	16.414631
28.024067	1560.511211	16.419648
27.966888	1570.681186	16.424666
28.203164	1557.844435	16.429683
27.898537	1568.161380	16.434701
27.781003	1581.184927	16.439719
28.055403	1577.189212	16.444736
28.074492	1569.956362	16.449754
28.204501	1551.457671	16.454771
28.097887	1559.088711	16.459789
28.111256	1543.314638	16.464807
28.023008	1523.118266	16.469824
28.119125	1539.399170	16.474842
28.041701	1545.188468	16.479859
28.122914	1531.786743	16.484877
27.913566	1547.843096	16.489895
28.017318	1539.488730	16.494912
28.037686	1537.011560	16.499930
27.902738	1548.693560	16.504947
27.857139	1529.208384	16.509965
28.190762	1544.471416	16.514983
28.154384	1556.267615	16.520000
28.312809	1561.320356	16.525018
28.360049	1542.028341	16.530035
28.325982	1540.762961	16.535053
28.183859	1544.832907	16.540071
28.118305	1538.372757	16.545088
28.261893	1574.509736	16.550106
27.843620	1559.433125	16.555123
28.338531	1559.455035	16.560141
28.341452	1554.731420	16.565159
28.560134	1553.573649	16.570176
28.363737	1571.039791	16.575194
28.434350	1560.951494	16.580211
28.655827	1570.855682	16.585229
28.430677	1570.698913	16.590247
28.373145	1554.315515	16.595264
28.545212	1561.006992	16.600282
28.231243	1562.850897	16.605299
28.390232	1544.739665	16.610317
28.120161	1568.347777	16.615335
28.812026	1564.742330	16.620352
28.576308	1602.268450	16.625370
28.733336	1612.942015	16.630387
29.239355	1602.511616	16.635405
29.042085	1597.398226	16.640423
29.188482	1600.915987	16.645440
29.023147	1580.559676	16.650458
28.856180	1579.248357	16.655475
29.003066	1583.618215	16.660493
28.937458	1594.130963	16.665511
29.111882	1598.845316	16.670528
28.925367	1603.249317	16.675546
28.733023	1584.298057	16.680563
28.923764	1596.794593	16.685581
29.262040	1589.395034	16.690599
29.282008	1589.435503	16.695616
29.212002	1596.094967	16.700634
29.218931	1599.320684	16.705651
29.325073	1587.027254	16.710669
28.588620	1601.183885	16.715687
29.070324	1589.032579	16.720704
29.088053	1585.454888	16.725722
29.220338	1582.948786	16.730739
29.249397	1570.808137	16.735757
29.043479	1582.302719	16.740775
29.262022	1606.852271	16.745792
29.387516	1620.690039	16.750810
29.564954	1609.364527	16.755827
29.593595	1625.265712	16.760845
29.348430	1627.388647	16.765863
29.428517	1630.034879	16.770880
29.614720	1617.220327	16.775898
29.669842	1603.515631	16.780915
29.686567	1600.821382	16.785933
29.601292	1618.823233	16.790951
29.835608	1622.662128	16.795968
29.780319	1607.979720	16.800986
29.497358	1604.904376	16.806003
29.880126	1614.228314	16.811021
30.075758	1606.250084	16.816039
30.040024	1613.884887	16.821056
29.888314	1616.861979	16.826074
29.979239	1612.010047	16.831091
29.830260	1607.024472	16.836109
29.856396	1611.105106	16.841127
29.867385	1614.552057	16.846144
30.093346	1603.324808	16.851162
29.780689	1614.331647	16.856179
30.112646	1636.587094	16.861197
29.905793	1643.759249	16.866215
29.894515	1634.735105	16.871232
30.154200	1633.600171	16.876250
30.212676	1654.967075	16.881267
30.363545	1635.777478	16.886285
30.271696	1650.036739	16.891303
30.469394	1631.280262	16.896320
30.595142	1628.162859	16.901338
30.455174	1636.611879	16.906355
30.490414	1628.811489	16.911373
30.588202	1633.956738	16.916391
30.354480	1630.213251	16.921408
30.651087	1629.544265	16.926426
30.732309	1649.274473	16.931443
31.067463	1615.697079	16.936461
30.611025	1597.565465	16.941479
30.468712	1597.775833	16.946496
30.864528	1613.466162	16.951514
30.647610	1627.921232	16.956531
31.020027	1597.161347	16.961549
30.504004	1603.022656	16.966567
30.461241	1628.318132	16.971584
30.641895	1617.858536	16.976602
30.755035	1638.943017	16.981619
30.584695	1622.343000	16.986637
30.417697	1632.548188	16.991655
31.021036	1634.016838	16.996672
30.846607	1628.072767	17.001690
30.858900	1632.730870	17.006707
30.864082	1640.835106	17.011725
30.800818	1634.727908	17.016743
30.779951	1634.495263	17.021760
30.852438	1626.986196	17.026778
30.879852	1629.130805	17.031795
31.255130	1644.389808	17.036813
31.138494	1639.159360	17.041831
31.016889	1646.555470	17.046848
31.379209	1647.667773	17.051866
31.012013	1661.313727	17.056883
31.442326	1651.826618	17.061901
31.361362	1653.097297	17.066919
31.276464	1641.525507	17.071936
31.516237	1653.354280	17.076954
31.535204	1648.538042	17.081971
31.336671	1642.146467	17.086989
31.291951	1658.614912	17.092007
31.359644	1653.270648	17.097024
31.379581	1638.381331	17.102042
31.199587	1638.000806	17.107059
31.536554	1651.712827	17.112077
31.624574	1685.682043	17.117095
31.556206	1687.626981	17.122112
31.819393	1663.342559	17.127130
31.662725	1672.554537	17.132147
31.646588	1682.683755	17.137165
31.617739	1670.643130	17.142183
31.829433	1677.848869	17.147200
32.353730	1681.168891	17.152218
31.874484	1682.609995	17.157235
32.085189	1684.942584	17.162253
32.220715	1674.341324	17.167271
32.006676	1669.453174	17.172288
32.024869	1671.226653	17.177306
31.712783	1682.319256	17.182323
31.940868	1667.876812	17.187341
32.266105	1678.968500	17.192359
32.071697	1675.886872	17.197376
32.206467	1661.649777	17.202394
31.862824	1662.553319	17.207411
32.145971	1671.127967	17.212429
32.138501	1668.762442	17.217447
31.736209	1680.129838	17.222464
32.559886	1688.762089	17.227482
32.480268	1695.323106	17.232499
32.596878	1682.469322	17.237517
32.263453	1689.878709	17.242535
32.236298	1694.712017	17.247552
32.770974	1686.132453	17.252570
32.269886	1720.348084	17.257587
32.811686	1703.524214	17.262605
32.882888	1689.995192	17.267623
32.530386	1704.637372	17.272640
32.651592	1682.590402	17.277658
32.928296	1686.906167	17.282675
32.664386	1697.345478	17.287693
33.157935	1701.046986	17.292711
32.987066	1665.165993	17.297728
33.382056	1665.863731	17.302746
33.093657	1669.425511	17.307763
33.169307	1656.169940	17.312781
32.947724	1656.973603	17.317799
32.645176	1676.557173	17.322816
32.870737	1657.656324	17.327834
33.005403	1676.723245	17.332851
32.954742	1659.486410	17.337869
32.941563	1651.111748	17.342887
33.014254	1675.482012	17.347904
32.981020	1656.063220	17.352922
32.907022	1683.746924	17.357939
32.966274	1701.072070	17.362957
33.020277	1698.625529	17.367975
32.894182	1690.195013	17.372992
33.096819	1684.038146	17.378010
33.178383	1707.713239	17.383027
32.937906	1694.438632	17.388045
33.146722	1707.282002	17.393063
33.318817	1735.290805	17.398080
33.412882	1720.584690	17.403098
33.242487	1708.843059	17.408115
33.430324	1731.165561	17.413133
33.573617	1737.799383	17.418151
33.522694	1734.665396	17.423168
33.643658	1729.874984	17.428186
33.495728	1727.439176	17.433203
33.587982	1737.785707	17.438221
33.629270	1722.735134	17.443239
33.779675	1727.516771	17.448256
34.225676	1714.666980	17.453274
34.195334	1715.722155	17.458291
33.850625	1731.620200	17.463309
34.246999	1711.419561	17.468327
34.156752	1730.579217	17.473344
34.083600	1718.737766	17.478362
34.267778	1732.581879	17.483379
33.939500	1714.660200	17.488397
33.984647	1721.170006	17.493415
33.897118	1729.516828	17.498432
33.900758	1704.582162	17.503450
33.822690	1723.453044	17.508467
33.687806	1732.801391	17.513485
33.710049	1726.208369	17.518503
33.481657	1744.976586	17.523520
34.068174	1749.003127	17.528538
34.021073	1748.043072	17.533555
34.056281	1744.434901	17.538573
34.119180	1757.510063	17.543591
34.382832	1760.572351	17.548608
34.732565	1777.260326	17.553626
34.972693	1774.853867	17.558643
35.071456	1762.591924	17.563661
35.026157	1750.297804	17.568679
35.020305	1728.907760	17.573696
35.128895	1734.901185	17.578714
34.914004	1730.979597	17.583731
34.965900	1721.527427	17.588749
35.019536	1731.428754	17.593767
34.981254	1724.436663	17.598784
35.087854	1743.325173	17.603802
35.048639	1720.217967	17.608819
34.752086	1695.338633	17.613837
34.767814	1687.780955	17.618855
35.060282	1710.924353	17.623872
35.132712	1720.394700	17.628890
34.866384	1714.095975	17.633907
34.839101	1738.244719	17.638925
35.200932	1735.010049	17.643943
34.826825	1719.596322	17.648960
34.934602	1723.635055	17.653978
34.939675	1724.892407	17.658995
35.053185	1726.937091	17.664013
35.205654	1724.768014	17.669031
34.781438	1748.309374	17.674048
35.358217	1736.182391	17.679066
35.358104	1739.241618	17.684083
35.222104	1739.124730	17.689101
35.697688	1736.273936	17.694119
35.304594	1759.506688	17.699136
35.290658	1754.507801	17.704154
35.200274	1775.786111	17.709171
35.311371	1777.980580	17.714189
35.746783	1774.488613	17.719207
35.399032	1776.823365	17.724224
35.551969	1773.947650	17.729242
35.666358	1768.924305	17.734259
35.498273	1767.702211	17.739277
35.427111	1766.548925	17.744295
35.668176	1759.855370	17.749312
35.594199	1785.594858	17.754330
35.838120	1796.883399	17.759347
35.673515	1803.137408	17.764365
35.968404	1815.602347	17.769383
36.036777	1814.330250	17.774400
36.359014	1787.909222	17.779418
35.999631	1778.546829	17.784435
36.000371	1798.161815	17.789453
36.040182	1783.754508	17.794471
36.037253	1792.037098	17.799488
36.202850	1791.650924	17.804506
36.325118	1794.769254	17.809523
36.194931	1793.810526	17.814541
36.615986	1792.313548	17.819559
36.214088	1799.881026	17.824576
36.268980	1809.155547	17.829594
36.358646	1797.292442	17.834611
36.093936	1785.032290	17.839629
36.460371	1783.113026	17.844647
36.157200	1819.247656	17.849664
36.520472	1818.296536	17.854682
36.685259	1822.644808	17.859699
36.668134	1831.402409	17.864717
36.799829	1825.336132	17.869735
37.025641	1829.645882	17.874752
36.991467	1805.912639	17.879770
36.793119	1822.177656	17.884787
36.711605	1837.663589	17.889805
36.868441	1811.351629	17.894823
36.819400	1835.322366	17.899840
37.239404	1824.265704	17.904858
37.122953	1822.254024	17.909875
37.078911	1838.649139	17.914893
36.933603	1824.586892	17.919911
36.831323	1817.357352	17.924928
37.141852	1819.513851	17.929946
37.011639	1840.902454	17.934963
36.615501	1826.036840	17.939981
37.015256	1802.317704	17.944999
36.878516	1824.671544	17.950016
36.931082	1818.666959	17.955034
37.108748	1816.886640	17.960051
37.143936	1852.190386	17.965069
37.198353	1843.381794	17.970087
37.158188	1840.517313	17.975104
37.537999	1848.610724	17.980122
37.671483	1847.484429	17.985139
37.363670	1855.592086	17.990157
37.561690	1855.799748	17.995175
37.508049	1846.264273	18.000192
37.640768	1860.638657	18.005210
37.586373	1860.211685	18.010227
37.459825	1840.032836	18.015245
37.526309	1837.481278	18.020263
37.933643	1838.932055	18.025280
37.978832	1835.180214	18.030298
37.838764	1846.959330	18.035315
37.641145	1857.657822	18.040333
37.847346	1860.449362	18.045351
38.067819	1872.213495	18.050368
37.794622	1861.336310	18.055386
38.405060	1869.296559	18.060403
38.132096	1859.021583	18.065421
38.121594	1857.424688	18.070439
38.370248	1878.120737	18.075456
38.397623	1858.336426	18.080474
38.268373	1861.691572	18.085491
38.146695	1875.883939	18.090509
38.118238	1858.466671	18.095527
38.113167	1867.444895	18.100544
38.272779	1855.414311	18.105562
38.519181	1857.850456	18.110579
38.377561	1864.014193	18.115597
38.804700	1858.726578	18.120615
38.357914	1854.940405	18.125632
38.630285	1864.561328	18.130650
38.753458	1864.078837	18.135667
38.393947	1853.309603	18.140685
38.500621	1861.571756	18.145703
38.492113	1854.403755	18.150720
38.620326	1881.980694	18.155738
39.152364	1882.846408	18.160755
38.672608	1895.549149	18.165773
38.804395	1884.565166	18.170791
38.732451	1904.353981	18.175808
38.778754	1898.596317	18.180826
39.178615	1874.086455	18.185843
38.802140	1881.369216	18.190861
38.845808	1886.615799	18.195879
39.083364	1882.378503	18.200896
38.966539	1886.029772	18.205914
38.827280	1881.284186	18.210931
38.999064	1909.773878	18.215949
39.534314	1916.289963	18.220967
39.397843	1918.155848	18.225984
39.538115	1929.056869	18.231002
39.497340	1915.642394	18.236019
39.586708	1916.024676	18.241037
39.502196	1918.203763	18.246055
39.522231	1910.814426	18.251072
39.678339	1924.492123	18.256090
40.147264	1912.946007	18.261107
39.775767	1911.090319	18.266125
39.835886	1894.279318	18.271143
39.716890	1868.712118	18.276160
39.572588	1871.924604	18.281178
39.834205	1866.290296	18.286195
39.539591	1865.868285	18.291213
39.773327	1893.234831	18.296231
39.875717	1907.670855	18.301248
39.693479	1912.271246	18.306266
40.229141	1916.573411	18.311283
40.007599	1904.233602	18.316301
39.840950	1910.710096	18.321319
39.885752	1912.325987	18.326336
40.031386	1915.421093	18.331354
40.252887	1904.916371	18.336371
39.821992	1916.248222	18.341389
40.264658	1923.135547	18.346407
40.215481	1896.634889	18.351424
39.711598	1896.809754	18.356442
40.559837	1927.245273	18.361459
40.460763	1940.652123	18.366477
40.569721	1937.169687	18.371495
40.538137	1941.699727	18.376512
40.496097	1941.356325	18.381530
40.878577	1922.788698	18.386547
40.710409	1944.951291	18.391565
40.884423	1955.722270	18.396583
41.034125	1934.489270	18.401600
40.566578	1911.474800	18.406618
40.890463	1915.078832	18.411635
40.864942	1925.400768	18.416653
40.932577	1912.820583	18.421671
41.066368	1936.729775	18.426688
40.981263	1953.828616	18.431706
41.038948	1928.595635	18.436723
41.057976	1929.106743	18.441741
41.215807	1940.176589	18.446759
41.383508	1925.774487	18.451776
40.976135	1935.882813	18.456794
41.288120	1919.591770	18.461811
41.039207	1944.258967	18.466829
40.868411	1932.476293	18.471847
41.212245	1933.263782	18.476864
40.957531	1946.004657	18.481882
41.053313	1929.020629	18.486899
40.999433	1936.418775	18.491917
41.154239	1930.716776	18.496935
41.216832	1946.172510	18.501952
41.312621	1961.368884	18.506970
41.551956	1960.816317	18.511987
41.510394	1962.934091	18.517005
41.836612	1961.412324	18.522023
42.141844	1968.741103	18.527040
41.985837	1959.726415	18.532058
42.251497	1948.928296	18.537075
41.542477	1969.242277	18.542093
42.038147	1957.975907	18.547111
42.069641	1960.633768	18.552128
41.897893	1947.742687	18.557146
42.119457	1955.949691	18.562163
42.000129	1960.202559	18.567181
41.945527	1953.714444	18.572199
41.994588	1968.957319	18.577216
41.819630	1956.147750	18.582234
42.056752	1960.541676	18.587251
41.891929	1966.798936	18.592269
42.369005	1965.857934	18.597287
42.548490	1972.804617	18.602304
42.302754	1970.983148	18.607322
42.526626	1960.077381	18.612339
42.409397	1973.898208	18.617357
42.560657	1974.528089	18.622375
42.788582	1989.353999	18.627392
42.258697	1984.611527	18.632410
42.464203	1974.760265	18.637427
42.815294	1992.604042	18.642445
43.097446	1971.480181	18.647463
43.124993	1971.832432	18.652480
42.723621	1973.162186	18.657498
42.963546	1969.486576	18.662515
43.075232	1984.182898	18.667533
43.193598	1962.942441	18.672551
42.815078	1958.012003	18.677568
42.949027	1954.912171	18.682586
43.236056	1951.897850	18.687603
42.905399	1970.061703	18.692621
43.025320	1966.225447	18.697639
43.206456	1964.615766	18.702656
43.357503	1986.604233	18.707674
43.084495	1977.657286	18.712691
43.483802	1970.892714	18.717709
43.409784	1955.257635	18.722727
43.400278	1970.318395	18.727744
43.219305	1987.017642	18.732762
43.153410	1966.087107	18.737779
43.148063	1972.296563	18.742797
43.061136	1968.888411	18.747815
43.106369	1986.426886	18.752832
43.155592	2001.425422	18.757850
43.615698	2003.254333	18.762867
43.844722	2001.754725	18.767885
43.500785	2002.750345	18.772903
43.665872	2019.719939	18.777920
43.559820	2011.188511	18.782938
43.742556	2002.055430	18.787955
43.777609	2025.456468	18.792973
43.708421	2029.911463	18.797991
44.216504	2007.496016	18.803008
44.861007	2022.522064	18.808026
44.699908	2015.164774	18.813043
44.370115	1997.912477	18.818061
44.614995	1997.568796	18.823079
44.775501	1982.599233	18.828096
44.429062	1995.350189	18.833114
44.630276	1990.411913	18.838131
44.803351	1971.378236	18.843149
44.551275	1982.664643	18.848167
44.916009	1981.755293	18.853184
44.723986	1981.412369	18.858202
44.443829	2001.460872	18.863219
44.716061	1984.535502	18.868237
44.564087	1980.243085	18.873255
44.930119	1990.435313	18.878272
44.619838	1987.282924	18.883290
44.519769	1966.179525	18.888307
44.661467	1983.848584	18.893325
44.541666	1979.893109	18.898343
44.516006	1991.063283	18.903360
44.597219	1997.432232	18.908378
44.732353	1999.231790	18.913395
45.172749	2006.072293	18.918413
44.852320	1999.810140	18.923431
45.448219	2016.134037	18.928448
45.037661	1994.083174	18.933466
44.792650	2009.005462	18.938483
45.143892	2017.065502	18.943501
45.159624	2009.185776	18.948519
45.007027	2015.399409	18.953536
45.347422	2005.791929	18.958554
45.311384	2021.531804	18.963571
45.396461	2034.476494	18.968589
45.591778	2025.088413	18.973607
45.941802	2040.415065	18.978624
45.320207	2044.895911	18.983642
45.329819	2032.264302	18.988659
45.677247	2046.105143	18.993677
45.272938	2043.906891	18.998695
45.522213	2054.436017	19.003712
45.253407	2041.029987	19.008730
45.327055	2056.949177	19.013747
45.737058	2061.078287	19.018765
45.650905	2055.221903	19.023783
46.106207	2072.944831	19.028800
45.862637	2071.022026	19.033818
45.745249	2076.474883	19.038835
46.105084	2077.893678	19.043853
45.612791	2067.811372	19.048871
46.073770	2096.694094	19.053888
46.504476	2100.372726	19.058906
46.474256	2090.087003	19.063923
46.762261	2104.724387	19.068941
46.686261	2087.307237	19.073959
47.122301	2093.743453	19.078976
46.635786	2084.144643	19.083994
46.726073	2064.337172	19.089011
46.741398	2060.897637	19.094029
46.542370	2050.766387	19.099047
46.719597	2076.757712	19.104064
46.989088	2085.664024	19.109082
47.116491	2084.837089	19.114099
47.128621	2075.083749	19.119117
46.976481	2058.291604	19.124135
47.052937	2057.208472	19.129152
46.828219	2070.065533	19.134170
46.721936	2077.816341	19.139187
46.976098	2095.285381	19.144205
46.995669	2082.226767	19.149223
47.170909	2093.062589	19.154240
47.183580	2076.433510	19.159258
47.046375	2081.951542	19.164275
47.180662	2094.918755	19.169293
47.124306	2101.601669	19.174311
47.236304	2081.407881	19.179328
47.441795	2080.513524	19.184346
47.283486	2102.708763	19.189363
47.499361	2120.820857	19.194381
47.576990	2124.334752	19.199399
47.732018	2122.450285	19.204416
47.855988	2117.264444	19.209434
47.619859	2119.999132	19.214451
47.832837	2116.365139	19.219469
47.481127	2122.432322	19.224487
47.913356	2106.278171	19.229504
48.129100	2132.239509	19.234522
47.806849	2126.179341	19.239539
48.220701	2113.967097	19.244557
47.975931	2121.188744	19.249575
48.019016	2106.924072	19.254592
47.930580	2108.985746	19.259610
47.839223	2126.629319	19.264627
48.387360	2127.688123	19.269645
48.101694	2147.150328	19.274663
48.361707	2161.177933	19.279680
48.177689	2146.468947	19.284698
48.367327	2128.479204	19.289715
48.586704	2143.836505	19.294733
48.704880	2139.463973	19.299751
48.576847	2124.070973	19.304768
48.681160	2153.768712	19.309786
48.618447	2139.167421	19.314803
48.901104	2119.524020	19.319821
48.795490	2118.927288	19.324839
49.140516	2139.925131	19.329856
48.938809	2135.442399	19.334874
48.695410	2143.452767	19.339891
48.740826	2140.635986	19.344909
48.722857	2132.504330	19.349927
48.857849	2137.392759	19.354944
49.062556	2151.392590	19.359962
48.961269	2151.889736	19.364979
49.250122	2167.799655	19.369997
49.185591	2177.943987	19.375015
49.244410	2162.788430	19.380032
49.413344	2162.466252	19.385050
49.427528	2166.173483	19.390067
49.409604	2148.729444	19.395085
49.243068	2154.065668	19.400103
49.453890	2166.131275	19.405120
49.461094	2162.568179	19.410138
49.460667	2170.245546	19.415155
49.976809	2186.004262	19.420173
49.979353	2197.468988	19.425191
50.043218	2182.635751	19.430208
50.014673	2187.977132	19.435226
49.758179	2194.471938	19.440243
49.837425	2185.657176	19.445261
49.892377	2193.891350	19.450279
49.994150	2176.761694	19.455296
49.955571	2187.426260	19.460314
49.808263	2192.630602	19.465331
50.197409	2169.731510	19.470349
50.088024	2177.079112	19.475367
50.139388	2174.812231	19.480384
50.176478	2190.986280	19.485402
50.037856	2194.185199	19.490419
50.190169	2205.661592	19.495437
50.292997	2207.970168	19.500455
50.385431	2217.739040	19.505472
50.514399	2208.808981	19.510490
50.547927	2209.343682	19.515507
50.714769	2209.323372	19.520525
50.750945	2204.571526	19.525543
50.593774	2205.277677	19.530560
51.163812	2232.448531	19.535578
51.329443	2227.252325	19.540595
51.194961	2223.540708	19.545613
51.299034	2199.103221	19.550631
50.968758	2187.981931	19.555648
51.605935	2188.011435	19.560666
51.015483	2202.644696	19.565683
51.406980	2189.892183	19.570701
51.419693	2190.730666	19.575719
51.395147	2191.925640	19.580736
51.115131	2195.489205	19.585754
50.915424	2214.426453	19.590771
51.619717	2219.858713	19.595789
51.611793	2234.434711	19.600807
51.508375	2218.398188	19.605824
51.629216	2222.100009	19.610842
51.482934	2233.717484	19.615859
51.957865	2220.450061	19.620877
52.019098	2238.610090	19.625895
52.260538	2228.834603	19.630912
52.080809	2236.304960	19.635930
52.057894	2240.766049	19.640947
52.057259	2211.787358	19.645965
52.017755	2220.026920	19.650983
52.046477	2244.419033	19.656000
51.985942	2220.140779	19.661018
51.999104	2238.145786	19.666035
52.222681	2242.047922	19.671053
52.088478	2226.438257	19.676071
52.123621	2241.737927	19.681088
52.377434	2231.702562	19.686106
52.328730	2226.151487	19.691123
52.360293	2239.226924	19.696141
52.346744	2238.419633	19.701159
52.442515	2252.379793	19.706176
52.406664	2256.358656	19.711194
52.167310	2270.026435	19.716211
52.368231	2245.466195	19.721229
52.421076	2269.005093	19.726247
52.480239	2289.665110	19.731264
52.964278	2288.101290	19.736282
52.448837	2292.979556	19.741299
52.836422	2304.327395	19.746317
53.075007	2292.822898	19.751335
53.235961	2281.648902	19.756352
53.227041	2296.458549	19.761370
53.052421	2299.692764	19.766387
53.008003	2280.636880	19.771405
53.440136	2301.941265	19.776423
53.587211	2292.034703	19.781440
53.519149	2283.940570	19.786458
53.283790	2292.827396	19.791475
53.522043	2302.225039	19.796493
53.771014	2319.608986	19.801511
53.715998	2314.695826	19.806528
54.101501	2317.410781	19.811546
53.919658	2321.706849	19.816563
54.331845	2315.863865	19.821581
54.042720	2293.380464	19.826599
53.973156	2276.088885	19.831616
54.132781	2278.721495	19.836634
53.764924	2273.853354	19.841651
54.222909	2287.227399	19.846669
54.137903	2310.543315	19.851687
54.228992	2311.836690	19.856704
54.416945	2294.816263	19.861722
54.333109	2310.302564	19.866739
54.507966	2299.419320	19.871757
54.582556	2290.651521	19.876775
54.441066	2309.983333	19.881792
54.357134	2295.655040	19.886810
54.169724	2319.859797	19.891827
54.640207	2299.638859	19.896845
54.369349	2300.155764	19.901863
54.573705	2297.487563	19.906880
54.506432	2306.046472	19.911898
54.814392	2323.300616	19.916915
54.685749	2307.230576	19.921933
54.943530	2329.754956	19.926951
55.179824	2348.181217	19.931968
55.305182	2331.657629	19.936986
55.311639	2349.304878	19.942003
55.495312	2334.945907	19.947021
55.329183	2343.799278	19.952039
55.119236	2330.116677	19.957056
55.519501	2331.822863	19.962074
55.511937	2330.553628	19.967091
55.356715	2326.706657	19.972109
55.411585	2329.967118	19.977127
55.357915	2323.652582	19.982144
55.604002	2333.616180	19.987162
55.082305	2335.213150	19.992179
55.135616	2341.473190	19.997197
55.045161	2342.446230	20.002215
55.150098	2353.675290	20.007232
55.849895	2356.384174	20.012250
55.582832	2365.174328	20.017267
55.922360	2357.868177	20.022285
55.680229	2336.531093	20.027303
55.931195	2368.426800	20.032320
56.351183	2383.601608	20.037338
56.303827	2378.238414	20.042355
56.386304	2401.187868	20.047373
56.856236	2395.834643	20.052391
56.578975	2358.237598	20.057408
56.553749	2357.273397	20.062426
56.733124	2350.703444	20.067443
56.619446	2344.787532	20.072461
56.586598	2348.997972	20.077479
56.876009	2351.650677	20.082496
57.251403	2345.786010	20.087514
57.134956	2352.352606	20.092531
56.747993	2322.875629	20.097549
56.965407	2335.805494	20.102567
56.835801	2331.073132	20.107584
57.018819	2330.141044	20.112602
56.909911	2352.377685	20.117619
57.082060	2354.206989	20.122637
57.197153	2369.492984	20.127655
57.062522	2381.299756	20.132672
57.137843	2363.137814	20.137690
57.147025	2369.006599	20.142707
57.175927	2372.728965	20.147725
57.343368	2375.316213	20.152743
57.341245	2372.179050	20.157760
57.373418	2347.356617	20.162778
57.408307	2375.155049	20.167795
57.677370	2391.748285	20.172813
57.876834	2371.954654	20.177831
57.642512	2395.835446	20.182848
57.803954	2389.346578	20.187866
57.737371	2393.989506	20.192883
57.665032	2397.791590	20.197901
58.076309	2382.503962	20.202919
57.724045	2373.441356	20.207936
58.105270	2381.374903	20.212954
58.072297	2395.655043	20.217971
58.225053	2410.614237	20.222989
58.455389	2418.630602	20.228007
58.083837	2418.071998	20.233024
58.384841	2425.476586	20.238042
58.316500	2414.296298	20.243059
57.964843	2416.742598	20.248077
58.416048	2413.950723	20.253095
58.237928	2413.875626	20.258112
58.580100	2433.808270	20.263130
58.555557	2441.052522	20.268147
58.689398	2467.141132	20.273165
58.958403	2443.662661	20.278183
58.914102	2447.693553	20.283200
59.146008	2427.516202	20.288218
59.128214	2434.096053	20.293235
59.065449	2448.573459	20.298253
59.059827	2442.766799	20.303271
59.105155	2462.400753	20.308288
59.100496	2437.285883	20.313306
59.224630	2432.501324	20.318323
59.000460	2460.760568	20.323341
59.508031	2457.036875	20.328359
59.446239	2473.546115	20.333376
59.614107	2465.608932	20.338394
59.774098	2477.896145	20.343411
59.600518	2493.569482	20.348429
59.833386	2471.616592	20.353447
59.729433	2486.661975	20.358464
59.861708	2463.487128	20.363482
59.518146	2459.400816	20.368499
59.740189	2468.193262	20.373517
59.655034	2473.242764	20.378535
59.782230	2487.088710	20.383552
60.233604	2507.316742	20.388570
60.416338	2502.995832	20.393587
60.285499	2505.545791	20.398605
60.615242	2499.373698	20.403623
60.376375	2486.149802	20.408640
60.530349	2496.716435	20.413658
60.416458	2480.600475	20.418675
60.472460	2485.017692	20.423693
60.831135	2468.158793	20.428711
60.590521	2498.379777	20.433728
60.662205	2501.986262	20.438746
60.667019	2490.249817	20.443763
61.078736	2485.782427	20.448781
61.148265	2498.072401	20.453799
60.769042	2525.703155	20.458816
60.729301	2527.924529	20.463834
61.424317	2513.368705	20.468851
61.189084	2514.716218	20.473869
61.134144	2521.798431	20.478887
61.484857	2505.850120	20.483904
61.086015	2518.899296	20.488922
61.371671	2520.877555	20.493939
61.481908	2529.183863	20.498957
61.467987	2524.795262	20.503975
61.539686	2526.149134	20.508992
61.684727	2531.765447	20.514010
61.768087	2545.731074	20.519027
61.662933	2543.470224	20.524045
62.094208	2542.521111	20.529063
61.786113	2551.309098	20.534080
61.883988	2551.570028	20.539098
62.112959	2533.932216	20.544115
61.654232	2536.032502	20.549133
62.044964	2548.382216	20.554151
62.134808	2556.987929	20.559168
62.215397	2552.839176	20.564186
62.350307	2566.793941	20.569203
62.318704	2575.810228	20.574221
63.053537	2570.423009	20.579239
62.934048	2557.367486	20.584256
62.610459	2559.347820	20.589274
63.023818	2560.366930	20.594291
62.853521	2567.874466	20.599309
63.003331	2564.991643	20.604327
62.906283	2569.571361	20.609344
63.009536	2559.135333	20.614362
63.104477	2557.786945	20.619379
62.869627	2555.044450	20.624397
63.174973	2571.182934	20.629415
63.043453	2569.344289	20.634432
62.930330	2565.448574	20.639450
63.030175	2573.882393	20.644467
62.949179	2568.486311	20.649485
63.405368	2557.525494	20.654503
63.287881	2562.792345	20.659520
63.220995	2588.291194	20.664538
63.647013	2598.821996	20.669555
63.631184	2606.249505	20.674573
63.618059	2598.105189	20.679591
63.580985	2585.128333	20.684608
63.971700	2583.166778	20.689626
63.991170	2595.123617	20.694643
63.734567	2586.133647	20.699661
63.730407	2573.330076	20.704679
63.723814	2600.233735	20.709696
63.887468	2610.801996	20.714714
64.304146	2620.184717	20.719731
64.135656	2635.152340	20.724749
64.318597	2610.440573	20.729767
64.427195	2618.683234	20.734784
64.116035	2625.733435	20.739802
64.311250	2611.432921	20.744819
64.605779	2626.113815	20.749837
64.520728	2653.953630	20.754855
64.822067	2647.798375	20.759872
64.692209	2635.789036	20.764890
64.891317	2641.727707	20.769907
64.626991	2635.511427	20.774925
65.094461	2635.516231	20.779943
65.173087	2639.763637	20.784960
65.215062	2632.605136	20.789978
65.505371	2644.119281	20.794995
65.244404	2643.649859	20.800013
65.496391	2630.352008	20.805031
65.596795	2632.204421	20.810048
65.645842	2616.561912	20.815066
65.902408	2627.246898	20.820083
65.578171	2627.968866	20.825101
65.947505	2626.533796	20.830119
65.926300	2642.106130	20.835136
65.480638	2631.407858	20.840154
65.985793	2632.331107	20.845171
65.922306	2647.897838	20.850189
65.679827	2652.246925	20.855207
65.752911	2655.010420	20.860224
65.846427	2650.723894	20.865242
66.031459	2662.053313	20.870259
65.930783	2672.448398	20.875277
66.075146	2652.958550	20.880295
66.354903	2680.145299	20.885312
66.364869	2680.684107	20.890330
66.457732	2679.937543	20.895347
66.287985	2694.256702	20.900365
66.683743	2686.894064	20.905383
66.743168	2679.752733	20.910400
66.822993	2691.111172	20.915418
67.208289	2672.188685	20.920435
66.958623	2674.992725	20.925453
66.865949	2681.867890	20.930471
66.652607	2683.505854	20.935488
67.030832	2703.666324	20.940506
67.457323	2700.106542	20.945523
67.063426	2724.129157	20.950541
67.342216	2718.995177	20.955559
67.466317	2711.720129	20.960576
67.418045	2695.945611	20.965594
67.377136	2703.759739	20.970611
67.471615	2697.058019	20.975629
67.746638	2705.283065	20.980647
67.823332	2715.647491	20.985664
67.706587	2709.903772	20.990682
67.890928	2691.045961	20.995699
67.774713	2697.250117	21.000717
68.001141	2714.714605	21.005735
67.920721	2703.340459	21.010752
67.829920	2717.577509	21.015770
68.217594	2728.525704	21.020787
67.923532	2744.404416	21.025805
68.340508	2731.676967	21.030823
68.566005	2750.234611	21.035840
68.137015	2742.952731	21.040858
68.285875	2717.290255	21.045875
68.225405	2735.935290	21.050893
68.405736	2741.323437	21.055911
68.732063	2750.551901	21.060928
68.707364	2772.375483	21.065946
69.300604	2778.193376	21.070963
69.197787	2765.689374	21.075981
68.882405	2774.024618	21.080999
69.115045	2754.984362	21.086016
68.935392	2764.227362	21.091034
69.329985	2777.446389	21.096051
69.293872	2772.573456	21.101069
69.378685	2761.712246	21.106087
69.370720	2771.249670	21.111104
69.062914	2752.167050	21.116122
69.406286	2744.815403	21.121139
69.512778	2771.554435	21.126157
69.403431	2785.520436	21.131175
69.811158	2766.090651	21.136192
69.756342	2780.311577	21.141210
70.189822	2776.373114	21.146227
69.870019	2783.434066	21.151245
69.563800	2783.619669	21.156263
69.712304	2775.074191	21.161280
69.840211	2798.054521	21.166298
70.087809	2804.487145	21.171315
70.450168	2815.228589	21.176333
70.108128	2806.891895	21.181351
70.366404	2793.958170	21.186368
70.183059	2807.517183	21.191386
70.312447	2797.334121	21.196403
70.876645	2811.462626	21.201421
70.686079	2829.266982	21.206439
71.110804	2842.423220	21.211456
70.870770	2831.580015	21.216474
71.035155	2834.356602	21.221491
70.837022	2835.257124	21.226509
70.990396	2820.289401	21.231527
71.025452	2823.933901	21.236544
71.320600	2816.977541	21.241562
71.502081	2824.134588	21.246579
71.428645	2842.021559	21.251597
71.506644	2830.648500	21.256615
71.586608	2816.616021	21.261632
71.324385	2837.478683	21.266650
71.572112	2826.187604	21.271667
71.721571	2861.780554	21.276685
71.518055	2867.965941	21.281703
71.932445	2855.662977	21.286720
71.832267	2865.296002	21.291738
71.911442	2866.167234	21.296755
72.127313	2852.140411	21.301773
72.017465	2861.761647	21.306791
72.455833	2850.425074	21.311808
71.895142	2854.922458	21.316826
72.194425	2874.216191	21.321843
72.203324	2879.559891	21.326861
72.309799	2879.550542	21.331879
72.818102	2879.559623	21.336896
72.865266	2883.986092	21.341914
72.808424	2876.412169	21.346931
72.853163	2887.700182	21.351949
72.776237	2896.211414	21.356967
72.893215	2880.607603	21.361984
72.791692	2878.571468	21.367002
72.530313	2890.503892	21.372019
72.921556	2878.210639	21.377037
72.619073	2910.023358	21.382055
73.267814	2915.608342	21.387072
73.245551	2912.699959	21.392090
73.238763	2917.267423	21.397107
73.484369	2905.048603	21.402125
73.225802	2919.093511	21.407143
73.913269	2907.127025	21.412160
73.660715	2930.549314	21.417178
73.922503	2943.859516	21.422195
74.384868	2929.961357	21.427213
74.328553	2941.670981	21.432231
74.197470	2941.386753	21.437248
74.223988	2932.148638	21.442266
74.061968	2937.299172	21.447283
74.312963	2915.961280	21.452301
74.042389	2924.925736	21.457319
74.396530	2919.124202	21.462336
74.514784	2930.278460	21.467354
74.641322	2922.505137	21.472371
74.550246	2925.996509	21.477389
74.420644	2931.119049	21.482407
74.358492	2925.532940	21.487424
74.655561	2959.982768	21.492442
74.802085	2949.343089	21.497459
75.109213	2958.353422	21.502477
75.007411	2970.445538	21.507495
75.205525	2952.088222	21.512512
75.122403	2944.165305	21.517530
75.059900	2952.179559	21.522547
75.244652	2955.661968	21.527565
75.321853	2980.883947	21.532583
75.513372	2980.489133	21.537600
75.573720	2982.154923	21.542618
75.635615	2986.896076	21.547635
75.848353	2988.779373	21.552653
75.572494	2976.102245	21.557671
75.887189	2988.311354	21.562688
75.872841	2980.424882	21.567706
75.858578	2997.910964	21.572723
76.260768	3012.078038	21.577741
76.106925	3018.862096	21.582759
76.273234	3012.674095	21.587776
76.426869	3021.864338	21.592794
76.370299	3023.120370	21.597811
76.789658	3014.782137	21.602829
76.700458	3009.052847	21.607847
76.844901	3009.538936	21.612864
76.696152	3002.228731	21.617882
76.536259	3007.978079	21.622899
76.696139	3008.981438	21.627917
76.752319	3031.945430	21.632935
76.880892	3028.743037	21.637952
76.871245	3046.567348	21.642970
76.920937	3036.007974	21.647987
77.085262	3029.640197	21.653005
77.313128	3043.032066	21.658023
77.211036	3026.552799	21.663040
77.416654	3032.853102	21.668058
77.298437	3063.119722	21.673075
77.309437	3083.131948	21.678093
77.313092	3076.975524	21.683111
77.312715	3053.657950	21.688128
77.849045	3072.750182	21.693146
77.988919	3092.273461	21.698163
78.534658	3082.129863	21.703181
78.314635	3093.230899	21.708199
78.236733	3056.357583	21.713216
78.552116	3079.326838	21.718234
78.137241	3074.528604	21.723251
78.483756	3072.006444	21.728269
78.389075	3081.276335	21.733287
78.843165	3087.584612	21.738304
78.865567	3085.540371	21.743322
78.941135	3080.404229	21.748339
78.970102	3089.451943	21.753357
78.984477	3090.005783	21.758375
78.839862	3078.342593	21.763392
79.091127	3097.090077	21.768410
79.002105	3083.120316	21.773427
79.073998	3081.640667	21.778445
78.702866	3084.519964	21.783463
79.087739	3087.956934	21.788480
79.087524	3117.310953	21.793498
79.208377	3111.462081	21.798515
79.350774	3121.745458	21.803533
79.554647	3137.387387	21.808551
79.473153	3140.702047	21.813568
79.643865	3146.974901	21.818586
79.847128	3136.126330	21.823603
79.839863	3143.327510	21.828621
79.572776	3135.519137	21.833639
79.905168	3151.211684	21.838656
80.179414	3156.500806	21.843674
80.401416	3165.397782	21.848691
80.949616	3160.782069	21.853709
80.736320	3165.829550	21.858727
80.822544	3159.851948	21.863744
80.891845	3165.806564	21.868762
81.189345	3183.364356	21.873779
81.103659	3157.324794	21.878797
80.969497	3169.667860	21.883815
80.688296	3155.827024	21.888832
81.034312	3167.775814	21.893850
80.921098	3159.218063	21.898867
80.917409	3152.394784	21.903885
80.917380	3177.322990	21.908903
81.141533	3178.179337	21.913920
81.220944	3181.567996	21.918938
81.049829	3186.144193	21.923955
81.395310	3178.183987	21.928973
81.022558	3178.091445	21.933991
81.573814	3206.783110	21.939008
81.534149	3230.560396	21.944026
81.347589	3226.338297	21.949043
81.818754	3215.714861	21.954061
81.860196	3242.840814	21.959079
81.770089	3232.106987	21.964096
82.488806	3244.572535	21.969114
82.098412	3248.889937	21.974131
82.792891	3244.844652	21.979149
82.435579	3248.449376	21.984167
82.609696	3245.424433	21.989184
82.718219	3239.452169	21.994202
82.709094	3238.315781	21.999219
82.992752	3240.189358	22.004237
83.109662	3231.393167	22.009255
82.990605	3220.210832	22.014272
83.080887	3236.457594	22.019290
83.173954	3247.210577	22.024307
83.391555	3256.404365	22.029325
83.694070	3280.079125	22.034343
83.508627	3255.352603	22.039360
83.775140	3254.197434	22.044378
83.719279	3270.633523	22.049395
83.830737	3243.000963	22.054413
83.967108	3266.245329	22.059431
83.842433	3261.979336	22.064448
84.015226	3262.237741	22.069466
84.088516	3268.846396	22.074483
84.346068	3245.882327	22.079501
84.398331	3253.426638	22.084519
84.242374	3258.302486	22.089536
84.182483	3241.952418	22.094554
84.324691	3260.816341	22.099571
84.313055	3261.570529	22.104589
84.321338	3248.721037	22.109607
84.462458	3260.307735	22.114624
84.875717	3264.430535	22.119642
84.906216	3286.778938	22.124659
84.840664	3285.062166	22.129677
84.740832	3267.382584	22.134695
85.111897	3278.371512	22.139712
85.033863	3286.322371	22.144730
84.931697	3286.842726	22.149747
85.250898	3278.863586	22.154765
85.466106	3308.902379	22.159783
85.722487	3291.861475	22.164800
85.707507	3291.624190	22.169818
85.293586	3318.189563	22.174835
85.821883	3306.455157	22.179853
85.745793	3312.735401	22.184871
85.820505	3312.725986	22.189888
85.977610	3306.791333	22.194906
85.696906	3323.106577	22.199923
85.967769	3331.622777	22.204941
85.968841	3335.438351	22.209959
85.900387	3334.610747	22.214976
86.053658	3337.991566	22.219994
86.338550	3360.319688	22.225011
86.832040	3350.958099	22.230029
86.692410	3370.305103	22.235047
86.938992	3363.011675	22.240064
87.108312	3362.161509	22.245082
86.739121	3363.985123	22.250099
87.089285	3375.407849	22.255117
86.977451	3369.853408	22.260135
87.231031	3371.723705	22.265152
87.583369	3385.910385	22.270170
87.347978	3388.079575	22.275187
87.804271	3384.074402	22.280205
87.768917	3387.290160	22.285223
87.978579	3382.700013	22.290240
88.118225	3379.310106	22.295258
87.858762	3409.663337	22.300275
88.017103	3380.816398	22.305293
87.925785	3380.201015	22.310311
87.853584	3384.730022	22.315328
87.927377	3365.712310	22.320346
88.001934	3384.749950	22.325363
88.059936	3406.872742	22.330381
88.319941	3403.473766	22.335399
88.161925	3399.668911	22.340416
88.289004	3414.681548	22.345434
88.390053	3420.040716	22.350451
88.525298	3417.261512	22.355469
89.121911	3433.698213	22.360487
88.574481	3448.622558	22.365504
88.844896	3454.955827	22.370522
88.861927	3450.849420	22.375539
89.355580	3439.657599	22.380557
88.411247	3450.229622	22.385575
88.528513	3460.346527	22.390592
88.490573	3465.567866	22.395610
89.086733	3498.630814	22.400627
89.198978	3507.428615	22.405645
89.752463	3519.397524	22.410663
89.782278	3501.978510	22.415680
90.394561	3492.766285	22.420698
90.093250	3504.905763	22.425715
90.389815	3490.112927	22.430733
90.164075	3507.301882	22.435751
90.439949	3490.066808	22.440768
90.573429	3490.282899	22.445786
90.349147	3498.887704	22.450803
90.460714	3522.742015	22.455821
90.861879	3537.877773	22.460839
90.771490	3529.794942	22.465856
91.042106	3529.452787	22.470874
91.056202	3536.806907	22.475891
91.196147	3511.289849	22.480909
90.815103	3530.103767	22.485927
90.822344	3519.151308	22.490944
91.424322	3522.690481	22.495962
91.324550	3567.079247	22.500979
91.453494	3551.853261	22.505997
91.627708	3558.896901	22.511015
91.651127	3556.589853	22.516032
91.952003	3546.425989	22.521050
91.807012	3554.122718	22.526067
91.953543	3532.973468	22.531085
92.172803	3541.904380	22.536103
91.775996	3565.468779	22.541120
92.095507	3572.342758	22.546138
92.303911	3575.404898	22.551155
92.206588	3582.927636	22.556173
92.531444	3572.777114	22.561191
92.391289	3568.364197	22.566208
92.445512	3581.868884	22.571226
92.311367	3595.448800	22.576243
92.791582	3610.052710	22.581261
92.839772	3626.323176	22.586279
92.704959	3604.888258	22.591296
93.272767	3602.823503	22.596314
93.412139	3606.232857	22.601331
93.416566	3607.514286	22.606349
93.560943	3627.568953	22.611367
93.865976	3642.993907	22.616384
94.185550	3625.229258	22.621402
94.247693	3633.111072	22.626419
94.260915	3606.721756	22.631437
94.218212	3586.638463	22.636455
94.087755	3590.803172	22.641472
94.329868	3574.994334	22.646490
94.340533	3588.504060	22.651507
94.354590	3588.903849	22.656525
94.277388	3596.544913	22.661543
94.548199	3630.984834	22.666560
94.545981	3604.397104	22.671578
94.549035	3623.381505	22.676595
94.251789	3623.930760	22.681613
94.568458	3616.945882	22.686631
94.468161	3622.915316	22.691648
94.744388	3614.399840	22.696666
94.865666	3642.036096	22.701683
95.000076	3660.297708	22.706701
94.966235	3638.583086	22.711719
94.648911	3673.379322	22.716736
95.243503	3668.999873	22.721754
95.392651	3671.625401	22.726771
95.256475	3675.527514	22.731789
95.602685	3668.419236	22.736807
95.481969	3689.384456	22.741824
95.895503	3695.680790	22.746842
95.790379	3704.500057	22.751859
95.808131	3724.487000	22.756877
95.976374	3706.791159	22.761895
96.093692	3709.503837	22.766912
96.626372	3728.798655	22.771930
96.618000	3715.999162	22.776947
96.648618	3738.809188	22.781965
96.787816	3735.791298	22.786983
96.681388	3730.642892	22.792000
96.935516	3730.110755	22.797018
96.745549	3738.039007	22.802035
96.316022	3728.911008	22.807053
96.910476	3722.200040	22.812071
96.875490	3754.504900	22.817088
97.104961	3763.276981	22.822106
97.534205	3780.208607	22.827123
97.762339	3768.372480	22.832141
98.496177	3768.233481	22.837159
98.616017	3769.040569	22.842176
98.429734	3739.183644	22.847194
98.449067	3750.081830	22.852211
98.164979	3743.438079	22.857229
98.460090	3729.913276	22.862247
98.399146	3742.247849	22.867264
98.306572	3722.485197	22.872282
98.771621	3739.051439	22.877299
98.621225	3757.798387	22.882317
98.910327	3758.479087	22.887335
98.859541	3785.074814	22.892352
98.739602	3781.585597	22.897370
98.821133	3769.660317	22.902387
98.764066	3761.136061	22.907405
98.882208	3756.546165	22.912423
98.856679	3777.073559	22.917440
99.377746	3786.878498	22.922458
99.150322	3782.372270	22.927475
99.093621	3799.436182	22.932493
99.286587	3814.425920	22.937511
99.639706	3815.353900	22.942528
99.863726	3828.882907	22.947546
100.127636	3827.245876	22.952563
99.793525	3830.076279	22.957581
100.058983	3825.136844	22.962599
100.106440	3829.132462	22.967616
99.977745	3865.052018	22.972634
100.214658	3856.815921	22.977651
100.405033	3862.023680	22.982669
100.556642	3858.058105	22.987687
100.266490	3857.088968	22.992704
100.523963	3884.655911	22.997722
101.077590	3874.466011	23.002739
100.793098	3883.093773	23.007757
101.477299	3877.839472	23.012775
101.181957	3878.992714	23.017792
101.276447	3887.924760	23.022810
101.269370	3899.623823	23.027827
101.242692	3906.587440	23.032845
101.816283	3915.890701	23.037863
101.692014	3914.176868	23.042880
101.863080	3897.949350	23.047898
102.105251	3914.269949	23.052915
101.994113	3926.138187	23.057933
102.012584	3900.084098	23.062951
102.195112	3921.327652	23.067968
102.648123	3925.225179	23.072986
102.716396	3913.623417	23.078003
102.675112	3941.123300	23.083021
103.292627	3922.779186	23.088039
102.873463	3939.688987	23.093056
102.884447	3947.616422	23.098074
103.510323	3935.733930	23.103091
103.027359	3929.750485	23.108109
103.232753	3939.944476	23.113127
103.064484	3921.681787	23.118144
103.116917	3928.659505	23.123162
103.341026	3936.961141	23.128179
103.006107	3940.047982	23.133197
103.402371	3960.424429	23.138215
103.542049	3955.729740	23.143232
103.453601	3958.086132	23.148250
103.517649	3976.478242	23.153267
103.926938	3986.048052	23.158285
103.952120	3987.129835	23.163303
104.148353	3994.307823	23.168320
104.234340	4003.053556	23.173338
104.263992	4023.186746	23.178355
104.464541	4022.232571	23.183373
104.653288	4008.870763	23.188391
104.467938	4014.891407	23.193408
104.400013	4033.338462	23.198426
104.817876	4032.471598	23.203443
104.664886	4044.939332	23.208461
105.255651	4036.847807	23.213479
105.032791	4071.961791	23.218496
105.255865	4071.632601	23.223514
105.538338	4067.390637	23.228531
105.400527	4084.276936	23.233549
105.767085	4081.759967	23.238567
105.927504	4089.960404	23.243584
105.702263	4119.116907	23.248602
106.438083	4107.419652	23.253619
106.187236	4116.069934	23.258637
106.518634	4123.148486	23.263655
106.716386	4101.566590	23.268672
106.714353	4098.288516	23.273690
106.713055	4093.578894	23.278707
106.896476	4086.696726	23.283725
106.937192	4096.445221	23.288743
107.083632	4099.682461	23.293760
106.868329	4120.474336	23.298778
107.208003	4128.406995	23.303795
106.934859	4136.404310	23.308813
107.368058	4119.644290	23.313831
107.449339	4125.957123	23.318848
107.252858	4144.694438	23.323866
107.656654	4143.471248	23.328883
107.500631	4148.096609	23.333901
107.780747	4162.095948	23.338919
108.116886	4152.112665	23.343936
108.234586	4152.028434	23.348954
108.311552	4179.227321	23.353971
108.346108	4181.410278	23.358989
108.355982	4178.585319	23.364007
108.072508	4195.854850	23.369024
108.463270	4188.875779	23.374042
108.757219	4199.137588	23.379059
108.484256	4208.131720	23.384077
108.680237	4204.222109	23.389095
108.963705	4223.349483	23.394112
108.702018	4217.810050	23.399130
108.644052	4219.251244	23.404147
108.983982	4237.642169	23.409165
109.184605	4238.814659	23.414183
109.184710	4247.602673	23.419200
109.264483	4282.666732	23.424218
110.026128	4266.616820	23.429235
110.036911	4276.443993	23.434253
109.967228	4271.405865	23.439271
110.504905	4258.010200	23.444288
110.266865	4271.796846	23.449306
110.461079	4268.654412	23.454323
110.518579	4261.581172	23.459341
110.787779	4281.607399	23.464359
110.927355	4293.017968	23.469376
111.132560	4282.788924	23.474394
111.495709	4293.746423	23.479411
110.840673	4288.904617	23.484429
111.036254	4297.721380	23.489447
111.439609	4307.064426	23.494464
111.597293	4298.054994	23.499482
111.757443	4310.497574	23.504499
111.617959	4299.621956	23.509517
111.371405	4289.959272	23.514535
111.534546	4320.825537	23.519552
111.846731	4321.639846	23.524570
111.787546	4321.738382	23.529587
111.896396	4346.863465	23.534605
111.941763	4354.668107	23.539623
112.242497	4351.469080	23.544640
112.288331	4365.580543	23.549658
112.468163	4341.506862	23.554675
112.391302	4365.518605	23.559693
112.397916	4389.631943	23.564711
112.528213	4403.626336	23.569728
112.334345	4397.989807	23.574746
112.847149	4412.407603	23.579763
113.169874	4415.428384	23.584781
113.356083	4409.115677	23.589799
113.421428	4436.390950	23.594816
113.833640	4439.657178	23.599834
114.131932	4442.076899	23.604851
114.217454	4451.854826	23.609869
113.827966	4435.239071	23.614887
114.349656	4440.663532	23.619904
114.135894	4441.252953	23.624922
114.306033	4428.042676	23.629939
114.673226	4435.115063	23.634957
114.580611	4460.993288	23.639975
114.747576	4463.433926	23.644992
114.748951	4454.992345	23.650010
115.159991	4463.227550	23.655027
114.892002	4464.989685	23.660045
114.919134	4458.334355	23.665063
115.353484	4476.210762	23.670080
114.999303	4491.228970	23.675098
115.050041	4492.490026	23.680115
115.230208	4498.842576	23.685133
115.415179	4500.147985	23.690151
115.619676	4506.304789	23.695168
115.562152	4523.653093	23.700186
115.887693	4523.053817	23.705203
115.854803	4511.367145	23.710221
115.948524	4531.362064	23.715239
116.496574	4555.845238	23.720256
116.257698	4563.870966	23.725274
116.854092	4563.893064	23.730291
116.848754	4558.608387	23.735309
116.672451	4549.944938	23.740327
117.144430	4545.888062	23.745344
117.124859	4537.298720	23.750362
117.422350	4540.941400	23.755379
117.423134	4565.918951	23.760397
117.469971	4564.164174	23.765415
117.953492	4564.304920	23.770432
117.588091	4561.559619	23.775450
118.187900	4563.109472	23.780467
117.908127	4551.789544	23.785485
118.158412	4576.260143	23.790503
118.361202	4558.861358	23.795520
118.061957	4559.188142	23.800538
118.509768	4560.826102	23.805555
118.339120	4563.042233	23.810573
118.522480	4597.084392	23.815591
118.707548	4591.552890	23.820608
118.473842	4589.827538	23.825626
118.555753	4588.180347	23.830643
118.721259	4611.012281	23.835661
118.521836	4616.650842	23.840679
119.099240	4625.049586	23.845696
119.010338	4637.646179	23.850714
119.366955	4635.250843	23.855731
119.232586	4649.456907	23.860749
119.416423	4678.952370	23.865767
119.645650	4686.866166	23.870784
119.693025	4680.152673	23.875802
119.893743	4685.984586	23.880819
120.124434	4704.118135	23.885837
119.782184	4715.710207	23.890855
120.722370	4706.944069	23.895872
120.365382	4722.052726	23.900890
120.759832	4748.113149	23.905907
121.034115	4747.070764	23.910925
120.822784	4762.138856	23.915943
121.434010	4750.871945	23.920960
121.375477	4742.005464	23.925978
121.642182	4744.476516	23.930995
121.758371	4732.027253	23.936013
121.571071	4751.498423	23.941031
121.859724	4750.687913	23.946048
122.034432	4780.945704	23.951066
121.915290	4782.282492	23.956083
122.088296	4779.406452	23.961101
121.938861	4782.319107	23.966119
122.435360	4773.019557	23.971136
122.198950	4771.238332	23.976154
122.208541	4800.410457	23.981171
122.399371	4793.488565	23.986189
122.634701	4812.568716	23.991207
122.955902	4817.928015	23.996224
123.123683	4834.450854	24.001242
123.122971	4843.200757	24.006259
123.012382	4833.808967	24.011277
123.153069	4823.783930	24.016295
123.600517	4852.139707	24.021312
123.288778	4863.091018	24.026330
123.639295	4868.675413	24.031347
124.131953	4876.044988	24.036365
124.128698	4873.343726	24.041383
124.356385	4861.280661	24.046400
124.160336	4889.857012	24.051418
124.107481	4878.444231	24.056435
124.258431	4902.293962	24.061453
124.273871	4898.051017	24.066471
124.540480	4892.703180	24.071488
124.589827	4919.353989	24.076506
124.689605	4919.656577	24.081523
125.413616	4914.178820	24.086541
125.092217	4922.542386	24.091559
125.235122	4918.725620	24.096576
125.481127	4945.872328	24.101594
125.616839	4959.650579	24.106611
125.553653	4950.496950	24.111629
125.864258	4959.165949	24.116647
126.112206	4937.134046	24.121664
126.025380	4963.479477	24.126682
125.791544	4978.516851	24.131699
126.426209	4969.390813	24.136717
126.510738	4966.334475	24.141735
126.339586	4983.650886	24.146752
126.628710	5008.924025	24.151770
126.643694	5025.142390	24.156787
126.860807	4998.812686	24.161805
126.547973	5018.749032	24.166823
127.113272	5033.414643	24.171840
126.830246	5043.260928	24.176858
127.091852	5057.297994	24.181875
127.391005	5056.855425	24.186893
127.389437	5075.512440	24.191911
127.700239	5082.611765	24.196928
127.952663	5100.357928	24.201946
128.006858	5094.793936	24.206963
128.248043	5100.232305	24.211981
128.036509	5118.783512	24.216999
128.861100	5124.516439	24.222016
129.119579	5133.091785	24.227034
129.293664	5128.274127	24.232051
129.438907	5113.585464	24.237069
129.525295	5135.773750	24.242087
129.559889	5114.309539	24.247104
129.794332	5116.574561	24.252122
129.642866	5112.349295	24.257139
129.909517	5114.284185	24.262157
129.915687	5105.592636	24.267175
129.757048	5118.931863	24.272192
129.752651	5118.598901	24.277210
129.614862	5141.164008	24.282227
130.376752	5139.869762	24.287245
130.041238	5150.153536	24.292263
130.359542	5166.621934	24.297280
130.546075	5171.963057	24.302298
130.310308	5168.552510	24.307315
130.776200	5177.921972	24.312333
130.590006	5200.803438	24.317351
131.067609	5223.680373	24.322368
130.846898	5208.936734	24.327386
131.023720	5217.830745	24.332403
131.280485	5233.471960	24.337421
131.514134	5258.627503	24.342439
131.807187	5246.712794	24.347456
131.717861	5260.898979	24.352474
132.082737	5271.859249	24.357491
132.377719	5276.793107	24.362509
132.204697	5278.758149	24.367527
132.551034	5284.965451	24.372544
132.319453	5302.631974	24.377562
132.781037	5291.112623	24.382579
133.269425	5289.686784	24.387597
133.364588	5311.340390	24.392615
133.556177	5275.861402	24.397632
133.300039	5295.019025	24.402650
133.423567	5303.031707	24.407667
133.335944	5292.952753	24.412685
133.394760	5315.784847	24.417703
133.825960	5304.387440	24.422720
133.882258	5326.252614	24.427738
133.783460	5336.612753	24.432755
134.206613	5342.511706	24.437773
134.183726	5336.389874	24.442791
134.257305	5359.814494	24.447808
134.354072	5360.224286	24.452826
134.352531	5348.546372	24.457843
134.637693	5349.232524	24.462861
134.634656	5377.450698	24.467879
134.770939	5372.198252	24.472896
134.736187	5388.200796	24.477914
134.695445	5410.725846	24.482931
135.126908	5411.052774	24.487949
135.184774	5422.890683	24.492967
135.189791	5446.559055	24.497984
135.305207	5455.385393	24.503002
135.942046	5457.050488	24.508019
136.284997	5470.313826	24.513037
136.326061	5478.907571	24.518055
136.628833	5466.947779	24.523072
136.737072	5470.067993	24.528090
136.907342	5507.077026	24.533107
137.016021	5493.586226	24.538125
137.009623	5515.097835	24.543143
137.097384	5502.686515	24.548160
137.216473	5504.674973	24.553178
137.277161	5518.295243	24.558195
137.662602	5536.064020	24.563213
137.547566	5538.178181	24.568231
137.596664	5518.017770	24.573248
137.830045	5552.841191	24.578266
137.701102	5552.747314	24.583283
138.084922	5561.175407	24.588301
138.061419	5575.119101	24.593319
138.606148	5604.110601	24.598336
138.564847	5593.998600	24.603354
138.549262	5600.730028	24.608371
138.990971	5612.335749	24.613389
139.060410	5647.139224	24.618407
139.405472	5625.324174	24.623424
139.692845	5632.239426	24.628442
139.388611	5625.716308	24.633459
139.621041	5621.166038	24.638477
139.460009	5645.453124	24.643495
139.722573	5659.024804	24.648512
139.885352	5666.570927	24.653530
139.843555	5680.170081	24.658547
140.336234	5685.667498	24.663565
140.421546	5690.363285	24.668583
140.338604	5692.957229	24.673600
140.912138	5722.644229	24.678618
140.491598	5730.975392	24.683635
140.785685	5707.948501	24.688653
140.922257	5734.156345	24.693671
141.343849	5738.620585	24.698688
141.500004	5736.433810	24.703706
141.666741	5758.075816	24.708723
141.609615	5756.314460	24.713741
141.862589	5775.811013	24.718759
142.070545	5793.998018	24.723776
142.419877	5788.683062	24.728794
142.402331	5789.774393	24.733811
142.458981	5774.117798	24.738829
142.201234	5801.114971	24.743847
142.541447	5804.513476	24.748864
142.734974	5795.452768	24.753882
142.953692	5796.378280	24.758899
143.483600	5800.652977	24.763917
143.519597	5791.415532	24.768935
143.506570	5825.203046	24.773952
143.887237	5826.310868	24.778970
143.792251	5835.031627	24.783987
144.218339	5837.160358	24.789005
144.168384	5833.779594	24.794023
144.204104	5837.400479	24.799040
144.115231	5832.074839	24.804058
144.225617	5836.413355	24.809075
144.523387	5857.247576	24.814093
144.526204	5877.235621	24.819111
144.551429	5858.807177	24.824128
144.776212	5857.562257	24.829146
144.752100	5893.477874	24.834163
145.088619	5901.523785	24.839181
145.212337	5912.452304	24.844199
145.187718	5916.287917	24.849216
145.731522	5922.479776	24.854234
145.609357	5922.949382	24.859251
145.975007	5950.643467	24.864269
145.772381	5950.562155	24.869287
145.584628	5953.777048	24.874304
145.997460	5967.387951	24.879322
145.868756	6001.362294	24.884339
146.371966	6029.520045	24.889357
146.494959	6015.079114	24.894375
147.129446	6045.566955	24.899392
147.152467	6049.613643	24.904410
147.271239	6047.307795	24.909427
147.459446	6038.662424	24.914445
147.635223	6073.086257	24.919463
147.813066	6080.143832	24.924480
148.255993	6074.633378	24.929498
148.174090	6077.879629	24.934515
148.306141	6067.575278	24.939533
148.505354	6074.465527	24.944551
148.492351	6103.435145	24.949568
148.638654	6110.443611	24.954586
148.745609	6111.375798	24.959603
148.984240	6134.763284	24.964621
149.079560	6126.534428	24.969639
149.190935	6141.179235	24.974656
149.760984	6140.156400	24.979674
149.471633	6140.075243	24.984691
149.985572	6170.810433	24.989709
149.809881	6171.687744	24.994727
150.196754	6166.603092	24.999744
150.358381	6170.807632	25.004762
150.373863	6182.130635	25.009779
150.765002	6184.297870	25.014797
150.535208	6202.089139	25.019815
150.531793	6204.093598	25.024832
150.719961	6196.150178	25.029850
150.799509	6229.997291	25.034867
151.279404	6220.470871	25.039885
151.505888	6221.766026	25.044903
151.624427	6232.256610	25.049920
151.906034	6236.460636	25.054938
152.193757	6248.938023	25.059955
152.206550	6261.466362	25.064973
152.490937	6251.572979	25.069991
152.164784	6266.741815	25.075008
152.503843	6256.294463	25.080026
152.170114	6274.331355	25.085043
152.438906	6263.510141	25.090061
152.821491	6287.255207	25.095079
152.585685	6286.406075	25.100096
152.982062	6293.400469	25.105114
153.058365	6322.600641	25.110131
153.144814	6317.611256	25.115149
153.611966	6334.418928	25.120167
153.379469	6349.922008	25.125184
153.407158	6356.144594	25.130202
153.598201	6366.492959	25.135219
153.628656	6372.353247	25.140237
153.849301	6386.645550	25.145255
153.849920	6413.154584	25.150272
154.535980	6419.125086	25.155290
154.378263	6443.472317	25.160307
154.435427	6436.610374	25.165325
155.066531	6450.584887	25.170343
154.930497	6465.040933	25.175360
155.402267	6470.394827	25.180378
155.466889	6468.817231	25.185395
155.666109	6499.949597	25.190413
156.018348	6497.607862	25.195431
156.002748	6502.445384	25.200448
156.388828	6513.574306	25.205466
156.284582	6532.487453	25.210483
156.505316	6529.428780	25.215501
156.944747	6524.147907	25.220519
157.078985	6545.621553	25.225536
157.062366	6547.857791	25.230554
157.449898	6561.573799	25.235571
157.497244	6575.648426	25.240589
157.569865	6556.850659	25.245607
157.424721	6572.349762	25.250624
158.050424	6585.275566	25.255642
158.180077	6585.153914	25.260659
158.038802	6582.032592	25.265677
158.220264	6584.421560	25.270695
158.683844	6604.908873	25.275712
158.658285	6610.325305	25.280730
158.876913	6615.086753	25.285747
158.902863	6639.892579	25.290765
159.421642	6635.592375	25.295783
159.401983	6640.201449	25.300800
159.523931	6645.217886	25.305818
159.793035	6643.189114	25.310835
159.685136	6663.170470	25.315853
160.029662	6689.909401	25.320871
159.775657	6673.403525	25.325888
160.282789	6684.202688	25.330906
160.252171	6707.010249	25.335923
160.173632	6696.858800	25.340941
160.689714	6712.597251	25.345959
160.652741	6727.970748	25.350976
161.103355	6739.888084	25.355994
161.223802	6755.473420	25.361011
161.093735	6772.203846	25.366029
161.606556	6760.514700	25.371047
161.383817	6758.984952	25.376064
161.692653	6782.236201	25.381082
161.903025	6810.357517	25.386099
162.047462	6802.511185	25.391117
162.224693	6815.623109	25.396135
162.245204	6820.286237	25.401152
162.380871	6811.694010	25.406170
162.594283	6831.542557	25.411187
162.597719	6834.328742	25.416205
163.044437	6852.955543	25.421223
162.958105	6855.884929	25.426240
163.159959	6860.873268	25.431258
163.592755	6881.459745	25.436275
163.449301	6891.838922	25.441293
163.550403	6892.084632	25.446311
163.686982	6911.455359	25.451328
164.053649	6903.384831	25.456346
164.474470	6933.029675	25.461363
164.282387	6958.402023	25.466381
164.864476	6954.205461	25.471399
165.056101	6952.688339	25.476416
165.267472	6947.089450	25.481434
165.353335	6949.056022	25.486451
165.122100	6978.730337	25.491469
165.449527	6964.256721	25.496487
165.517852	6984.664153	25.501504
165.732937	7001.505532	25.506522
166.195397	7003.151187	25.511539
166.106471	7018.139796	25.516557
166.211596	7031.430768	25.521575
166.160442	7028.579151	25.526592
166.643544	7049.025628	25.531610
166.929496	7047.164518	25.536627
166.693152	7070.542109	25.541645
167.255110	7061.137471	25.546663
167.595148	7092.468250	25.551680
167.664876	7114.738094	25.556698
167.975054	7094.831376	25.561715
167.880828	7107.006760	25.566733
168.406707	7097.411970	25.571751
168.252845	7115.421287	25.576768
168.772703	7122.926439	25.581786
168.659881	7117.506666	25.586803
168.393433	7139.766729	25.591821
168.930590	7136.690306	25.596839
168.851969	7164.451682	25.601856
169.211737	7172.752716	25.606874
169.555562	7172.038502	25.611891
169.592679	7200.342318	25.616909
170.035683	7201.661632	25.621927
169.960826	7193.896622	25.626944
169.818949	7225.161210	25.631962
170.358153	7227.761680	25.636979
170.012191	7228.079690	25.641997
170.347803	7252.731365	25.647015
170.346291	7257.274227	25.652032
170.761176	7264.199850	25.657050
170.933879	7279.243131	25.662067
170.899707	7303.926849	25.667085
171.448486	7297.765312	25.672103
171.451595	7324.810205	25.677120
171.530114	7334.401302	25.682138
171.921069	7353.348593	25.687156
172.005100	7352.356774	25.692173
172.555151	7349.696359	25.697191
172.461219	7383.270247	25.702208
172.526328	7389.257494	25.707226
172.881691	7392.444365	25.712244
172.483915	7415.920414	25.717261
172.914962	7417.663840	25.722279
173.171543	7431.931865	25.727296
173.546483	7459.203000	25.732314
173.734562	7448.082840	25.737332
173.950456	7464.513097	25.742349
174.440076	7468.900053	25.747367
174.400997	7492.404363	25.752384
174.622253	7495.129868	25.757402
174.720200	7483.420536	25.762420
174.912657	7474.122778	25.767437
175.265963	7474.053550	25.772455
175.199249	7485.045347	25.777472
175.209511	7510.981317	25.782490
175.373852	7506.325988	25.787508
175.297390	7508.804574	25.792525
175.313163	7524.794651	25.797543
175.551163	7557.811617	25.802560
175.579106	7561.584212	25.807578
176.099569	7564.698161	25.812596
176.211394	7587.942206	25.817613
176.094873	7598.643835	25.822631
176.453692	7603.144584	25.827648
176.462959	7627.876760	25.832666
177.027726	7656.050897	25.837684
177.371577	7650.377497	25.842701
177.781677	7656.607109	25.847719
177.607366	7684.854589	25.852736
177.696882	7681.775637	25.857754
177.945065	7699.369521	25.862772
177.892872	7716.109740	25.867789
178.217619	7712.591840	25.872807
178.395985	7741.076477	25.877824
178.159336	7744.000543	25.882842
178.211813	7772.480049	25.887860
178.700638	7774.422670	25.892877
178.672981	7772.964936	25.897895
179.081252	7814.665394	25.902912
179.349377	7829.160263	25.907930
179.806180	7830.503343	25.912948
179.699930	7860.409502	25.917965
179.882330	7867.313165	25.922983
180.543071	7863.646784	25.928000
180.479756	7869.805069	25.933018
180.726354	7898.737862	25.938036
180.936269	7905.900827	25.943053
181.085180	7895.924842	25.948071
181.424856	7921.153386	25.953088
181.246416	7948.314404	25.958106
181.651462	7941.322656	25.963124
181.430594	7955.895288	25.968141
182.004349	7961.546691	25.973159
181.765403	7983.892395	25.978176
182.010237	8008.005025	25.983194
182.624613	8011.921825	25.988212
182.429602	8035.640937	25.993229
182.613418	8043.115427	25.998247
182.764064	8044.389403	26.003264
182.768558	8062.000330	26.008282
183.143943	8092.778726	26.013300
183.503374	8098.129301	26.018317
183.634913	8107.301787	26.023335
184.141088	8127.478480	26.028352
184.167706	8120.979193	26.033370
184.609363	8132.531672	26.038388
184.795738	8173.134859	26.043405
184.805342	8168.171761	26.048423
185.076816	8161.179935	26.053440
185.426450	8198.924904	26.058458
185.909559	8187.230166	26.063476
185.847276	8186.877563	26.068493
185.597964	8201.954442	26.073511
185.910482	8208.535904	26.078528
185.899752	8217.793393	26.083546
186.160713	8234.229608	26.088564
186.275333	8246.071692	26.093581
186.377079	8238.185628	26.098599
186.504310	8250.060284	26.103616
186.862679	8280.159032	26.108634
187.080735	8276.911449	26.113652
187.236794	8297.902282	26.118669
187.223718	8309.597759	26.123687
187.731291	8314.117453	26.128704
187.460479	8331.619805	26.133722
187.822705	8332.112222	26.138740
187.842174	8352.076643	26.143757
188.242748	8368.152847	26.148775
188.692035	8378.848148	26.153792
188.316466	8390.951691	26.158810
189.048081	8407.546595	26.163828
189.258115	8411.356251	26.168845
189.255131	8425.625538	26.173863
189.471457	8434.254950	26.178880
189.498227	8446.666158	26.183898
189.842167	8460.675745	26.188916
189.977313	8490.707030	26.193933
190.162787	8475.268249	26.198951
190.578801	8501.454626	26.203968
190.662896	8509.470347	26.208986
191.125887	8513.607610	26.214004
191.233317	8522.153464	26.219021
191.586046	8549.489229	26.224039
191.859687	8537.794978	26.229056
191.701596	8557.077018	26.234074
192.283022	8556.102964	26.239092
192.323463	8574.757592	26.244109
192.204829	8577.000735	26.249127
192.673878	8582.812219	26.254144
192.767661	8587.794158	26.259162
193.156761	8584.430040	26.264180
193.027422	8604.966744	26.269197
193.469155	8608.465658	26.274215
193.721142	8624.958108	26.279232
193.679162	8635.309457	26.284250
194.134464	8616.496802	26.289268
194.609700	8642.290072	26.294285
194.697515	8663.335198	26.299303
194.500378	8657.396410	26.304320
194.474428	8663.238519	26.309338
194.758471	8667.849594	26.314356
194.858230	8678.293328	26.319373
195.000465	8696.795027	26.324391
195.430854	8705.367166	26.329408
195.430405	8719.941887	26.334426
195.884463	8737.793539	26.339444
196.164609	8752.778734	26.344461
196.087890	8766.957337	26.349479
196.727668	8769.309900	26.354496
196.457327	8797.722516	26.359514
196.598338	8785.699515	26.364532
196.875112	8802.926037	26.369549
197.004395	8814.893717	26.374567
196.985092	8824.221499	26.379584
196.949942	8841.131004	26.384602
197.414347	8853.678936	26.389620
197.726307	8886.022515	26.394637
197.818832	8897.700979	26.399655
198.250325	8900.145472	26.404672
198.167295	8912.238880	26.409690
198.398092	8935.170688	26.414708
198.736892	8949.021675	26.419725
198.957393	8968.252687	26.424743
199.488800	8961.118323	26.429760
199.023725	8985.660851	26.434778
199.406432	9013.698953	26.439796
199.745704	9010.727335	26.444813
199.949567	9013.538679	26.449831
200.292837	9031.468827	26.454848
200.311008	9042.236601	26.459866
200.437486	9060.374302	26.464884
200.941565	9085.880778	26.469901
200.912145	9074.805652	26.474919
201.296543	9098.693686	26.479936
201.428611	9114.583458	26.484954
201.828492	9101.295852	26.489972
202.216953	9118.711409	26.494989
202.147757	9148.761954	26.500007
202.609785	9141.486963	26.505024
202.493023	9153.484526	26.510042
202.584867	9166.038344	26.515060
202.790012	9168.667564	26.520077
203.175165	9193.172322	26.525095
203.443850	9193.002084	26.530112
203.440851	9196.287920	26.535130
203.522052	9230.712632	26.540148
203.475110	9251.928092	26.545165
203.592918	9262.787458	26.550183
203.702889	9262.074779	26.555200
204.163793	9294.471771	26.560218
204.231578	9312.057881	26.565236
204.708082	9345.545625	26.570253
204.756224	9347.432880	26.575271
205.216454	9366.979199	26.580288
205.154969	9363.651563	26.585306
205.677526	9381.601319	26.590324
205.819798	9409.152137	26.595341
206.013780	9433.646322	26.600359
206.637710	9429.761986	26.605376
206.733811	9450.067202	26.610394
206.957107	9455.031166	26.615412
207.175472	9464.915507	26.620429
207.085690	9478.301393	26.625447
207.593218	9471.655143	26.630464
207.793185	9498.727942	26.635482
208.201317	9511.246315	26.640500
208.244398	9522.237927	26.645517
208.311142	9551.292467	26.650535
208.956407	9529.772527	26.655552
209.155317	9538.031294	26.660570
209.286022	9551.210683	26.665588
209.169032	9543.449114	26.670605
209.332963	9570.091638	26.675623
209.851023	9568.235604	26.680640
209.944262	9581.714210	26.685658
209.914810	9589.190015	26.690676
210.173973	9625.955402	26.695693
210.388250	9636.615565	26.700711
210.407894	9634.307066	26.705728
210.530524	9645.846421	26.710746
210.685777	9677.982794	26.715764
211.165830	9670.391102	26.720781
211.005811	9699.268354	26.725799
211.503189	9715.995499	26.730816
211.787873	9736.907917	26.735834
212.079182	9758.791227	26.740852
212.275151	9744.872789	26.745869
212.297200	9759.499884	26.750887
212.836657	9789.523541	26.755904
212.960468	9810.122372	26.760922
213.014628	9815.657087	26.765940
213.443898	9828.867715	26.770957
213.085218	9832.366831	26.775975
213.540154	9838.433950	26.780992
214.022883	9866.043520	26.786010
214.144363	9867.841529	26.791028
214.512037	9873.407955	26.796045
214.352344	9883.762239	26.801063
214.533231	9889.349293	26.806080
214.663677	9906.597257	26.811098
214.952455	9947.316466	26.816116
215.131257	9948.088935	26.821133
215.143636	9990.767144	26.826151
215.716334	9996.602987	26.831168
215.938721	9996.104063	26.836186
215.805143	10006.607706	26.841204
216.363730	10023.457390	26.846221
216.183559	10049.680250	26.851239
216.948553	10053.220600	26.856256
216.998838	10090.311435	26.861274
217.058415	10096.095042	26.866292
217.379702	10098.732797	26.871309
217.788433	10118.035714	26.876327
218.262053	10128.358771	26.881344
218.233456	10132.781695	26.886362
218.575341	10161.164120	26.891380
218.784920	10166.996223	26.896397
219.060395	10166.626364	26.901415
219.428243	10172.425230	26.906432
219.336700	10217.822923	26.911450
219.606614	10209.448883	26.916468
219.902725	10236.202226	26.921485
219.957591	10253.911240	26.926503
220.226129	10255.121810	26.931520
220.316131	10281.490242	26.936538
220.595436	10271.652694	26.941556
220.928656	10290.519324	26.946573
220.771977	10327.085657	26.951591
220.917623	10317.801846	26.956608
221.307383	10352.782157	26.961626
221.223753	10381.083259	26.966644
221.904472	10392.702661	26.971661
221.843741	10419.809864	26.976679
222.239094	10419.836089	26.981696
222.650236	10437.101265	26.986714
222.484917	10456.924790	26.991732
222.986351	10463.093170	26.996749
223.471788	10489.832200	27.001767
223.982460	10523.007226	27.006784
224.027345	10532.709797	27.011802
224.128554	10513.386275	27.016820
224.845862	10526.857093	27.021837
224.659973	10546.735328	27.026855
224.797816	10541.621119	27.031872
225.254209	10560.845808	27.036890
225.619143	10572.196929	27.041908
226.004588	10564.755143	27.046925
225.690132	10591.183037	27.051943
226.055374	10596.326344	27.056960
226.174525	10609.005186	27.061978
226.496322	10622.543797	27.066996
226.847114	10641.606439	27.072013
226.746580	10643.988665	27.077031
226.778362	10661.100937	27.082048
226.919725	10681.126919	27.087066
226.971567	10701.506425	27.092084
227.400214	10701.520850	27.097101
227.601972	10737.405835	27.102119
227.560097	10746.310754	27.107136
228.174005	10774.007356	27.112154
228.057067	10778.588416	27.117172
228.374339	10802.817005	27.122189
228.584162	10833.983340	27.127207
228.593872	10847.685561	27.132224
229.097326	10846.036603	27.137242
229.427522	10885.146032	27.142260
229.539878	10880.685782	27.147277
229.805664	10900.448081	27.152295
229.701072	10932.107671	27.157312
230.133613	10951.279272	27.162330
230.336399	10968.543217	27.167348
230.955451	10967.721146	27.172365
231.095089	10998.025042	27.177383
231.415554	10992.697767	27.182400
231.339686	11023.271267	27.187418
231.796843	11047.110830	27.192436
232.335383	11054.216990	27.197453
232.447066	11081.409473	27.202471
232.564370	11088.439519	27.207488
233.023683	11101.040494	27.212506
232.949076	11122.524539	27.217524
233.560901	11117.512220	27.222541
233.475443	11135.493529	27.227559
234.004955	11152.457923	27.232576
234.257451	11163.171876	27.237594
234.133251	11195.022704	27.242612
234.871401	11195.488559	27.247629
234.841821	11206.342885	27.252647
235.017693	11218.765496	27.257664
235.475611	11237.797761	27.262682
235.310386	11238.315199	27.267700
235.687710	11256.614830	27.272717
236.176727	11296.334719	27.277735
236.105494	11308.397276	27.282752
236.446250	11295.952606	27.287770
236.255448	11323.734283	27.292788
236.799773	11333.105900	27.297805
236.800792	11363.966684	27.302823
236.994027	11379.122330	27.307840
237.125491	11408.258579	27.312858
237.280349	11438.962539	27.317876
237.895135	11454.536212	27.322893
238.338893	11484.027471	27.327911
238.259299	11478.922105	27.332928
238.755474	11501.427783	27.337946
238.676399	11528.561955	27.342964
239.303098	11535.985404	27.347981
239.312713	11564.034511	27.352999
239.783533	11588.266495	27.358016
240.113331	11596.264448	27.363034
240.356989	11599.963764	27.368052
240.610539	11602.395550	27.373069
240.524835	11646.751010	27.378087
241.006043	11646.792992	27.383104
241.680598	11649.688527	27.388122
241.449425	11685.979600	27.393140
241.865295	11673.977544	27.398157
242.719736	11690.873073	27.403175
242.432794	11727.738267	27.408192
242.606835	11726.674590	27.413210
242.471546	11739.739039	27.418228
242.698911	11765.416067	27.423245
243.126015	11769.424633	27.428263
243.241804	11784.027068	27.433280
243.380492	11808.768793	27.438298
243.419783	11814.669813	27.443316
243.754987	11843.525838	27.448333
244.079393	11878.055520	27.453351
243.963104	11892.166240	27.458368
244.616026	11891.479541	27.463386
244.597877	11910.221809	27.468404
245.108057	11950.626751	27.473421
245.117279	11965.711735	27.478439
245.269480	11987.211458	27.483456
245.930979	12004.650454	27.488474
245.956015	12013.802620	27.493492
246.277439	12030.199695	27.498509
246.403802	12048.729186	27.503527
246.509928	12053.565226	27.508544
246.985804	12087.081692	27.513562
247.085725	12127.487116	27.518580
247.196154	12122.931520	27.523597
247.471315	12164.753633	27.528615
247.541782	12181.178933	27.533632
248.066713	12195.739354	27.538650
248.266963	12215.764619	27.543668
248.625002	12235.726027	27.548685
249.055603	12267.169061	27.553703
249.415909	12285.294647	27.558720
249.693951	12306.165058	27.563738
249.527915	12342.990418	27.568756
250.449249	12327.521654	27.573773
251.072320	12345.298237	27.578791
251.036424	12354.549685	27.583808
251.590416	12367.696917	27.588826
251.927640	12373.256652	27.593844
252.004691	12376.198262	27.598861
252.609762	12386.632631	27.603879
252.518790	12386.788062	27.608896
252.773057	12404.755629	27.613914
252.859825	12427.120706	27.618932
253.253126	12420.796990	27.623949
253.245829	12440.327440	27.628967
253.326924	12465.384565	27.633984
253.518828	12475.566629	27.639002
253.928654	12482.023508	27.644020
254.115898	12502.298644	27.649037
254.452267	12534.371455	27.654055
254.825670	12537.776981	27.659072
254.860170	12563.706946	27.664090
254.811093	12571.388274	27.669108
255.063362	12599.888317	27.674125
255.310209	12609.958189	27.679143
255.412638	12627.583982	27.684160
255.814208	12649.746889	27.689178
256.031718	12672.835169	27.694196
256.062804	12708.247010	27.699213
256.530995	12715.794888	27.704231
256.882648	12752.641219	27.709248
257.091840	12762.484219	27.714266
257.369262	12810.003409	27.719284
257.419755	12819.680442	27.724301
257.961128	12838.418795	27.729319
257.907106	12873.058048	27.734336
258.460219	12888.689794	27.739354
258.911828	12913.234991	27.744372
258.661777	12919.057384	27.749389
259.296938	12952.230282	27.754407
259.752285	12953.243974	27.759424
259.667586	12973.408649	27.764442
259.961886	13020.414386	27.769460
260.743157	13020.186217	27.774477
260.802611	13051.072891	27.779495
260.976703	13068.630606	27.784512
261.536552	13085.402182	27.789530
261.806059	13085.725738	27.794548
261.739253	13112.447745	27.799565
262.394247	13107.771962	27.804583
262.187904	13114.857947	27.809600
262.890688	13129.687629	27.814618
262.674294	13141.788937	27.819636
262.843483	13170.927669	27.824653
263.353388	13181.523241	27.829671
263.278338	13200.629357	27.834688
263.697270	13214.388101	27.839706
263.949722	13255.239123	27.844724
263.813831	13254.191102	27.849741
264.207687	13277.542608	27.854759
264.306151	13307.729258	27.859776
264.735130	13326.853877	27.864794
265.037150	13350.687842	27.869812
265.450368	13380.930558	27.874829
265.977549	13396.958635	27.879847
266.099545	13416.224680	27.884864
266.624541	13441.469968	27.889882
266.976824	13450.269510	27.894900
266.922060	13455.712399	27.899917
267.356878	13471.106637	27.904935
267.543603	13488.364135	27.909952
267.816315	13523.420351	27.914970
268.527281	13537.697576	27.919988
268.206766	13568.400638	27.925005
268.317943	13584.116321	27.930023
268.534097	13602.264061	27.935040
268.933722	13615.137658	27.940058
269.081837	13644.620286	27.945076
269.248487	13673.627990	27.950093
269.783269	13688.051057	27.955111
269.733375	13727.761225	27.960128
270.192316	13745.234011	27.965146
270.176130	13747.116658	27.970164
270.508764	13788.571878	27.975181
271.306759	13814.144511	27.980199
271.214524	13842.848637	27.985216
271.591082	13871.372941	27.990234
272.072703	13898.534287	27.995252
272.076520	13934.897961	28.000269
272.460264	13938.335958	28.005287
272.888118	13954.570875	28.010304
273.420229	13977.367176	28.015322
273.258335	14004.376603	28.020340
273.357977	14033.585109	28.025357
273.975570	14035.060541	28.030375
274.258698	14073.663170	28.035392
274.580297	14098.977760	28.040410
274.983470	14119.903122	28.045428
274.997130	14127.948272	28.050445
275.632342	14173.112595	28.055463
275.530800	14169.316281	28.060480
275.861891	14191.265264	28.065498
276.308598	14226.982855	28.070516
276.241899	14237.737420	28.075533
276.851144	14261.132765	28.080551
276.611554	14272.289367	28.085568
276.993153	14308.036804	28.090586
277.423910	14334.892139	28.095604
277.546391	14369.237563	28.100621
278.177393	14369.092518	28.105639
278.442184	14387.296135	28.110656
278.868606	14410.033298	28.115674
278.965316	14454.702773	28.120692
278.636276	14468.929683	28.125709
279.578150	14490.248706	28.130727
279.868613	14524.933859	28.135744
280.126937	14521.183582	28.140762
280.617747	14552.016041	28.145780
280.614594	14560.960795	28.150797
280.973681	14570.668257	28.155815
281.149434	14605.692416	28.160832
281.442861	14612.911578	28.165850
281.759421	14628.328825	28.170868
282.108866	14667.651500	28.175885
282.435216	14665.046572	28.180903
282.537730	14683.849342	28.185920
282.574893	14706.235227	28.190938
282.871552	14720.850627	28.195956
283.285169	14754.390815	28.200973
283.872034	14776.945984	28.205991
284.403077	14793.437309	28.211008
284.291790	14796.098472	28.216026
284.671323	14819.047235	28.221044
284.862299	14850.163017	28.226061
285.504011	14850.748947	28.231079
285.744971	14890.715677	28.236096
285.942262	14904.444726	28.241114
286.446004	14919.700535	28.246132
286.501288	14939.050328	28.251149
286.730240	14938.324051	28.256167
287.168215	14970.242311	28.261184
287.339958	14978.477651	28.266202
287.645934	15003.405438	28.271220
287.529819	15043.861736	28.276237
287.981065	15050.410511	28.281255
288.104527	15082.644115	28.286272
288.205880	15117.415358	28.291290
288.603678	15106.479795	28.296308
288.611441	15152.667645	28.301325
289.255644	15177.749404	28.306343
289.278378	15219.607748	28.311360
289.518420	15231.609202	28.316378
290.175223	15268.887550	28.321396
290.202638	15313.867096	28.326413
290.650423	15322.638490	28.331431
290.674115	15351.872950	28.336448
291.130117	15388.574897	28.341466
291.895770	15400.425028	28.346484
291.890420	15450.681583	28.351501
292.370201	15449.764138	28.356519
292.481664	15492.363358	28.361536
293.028186	15508.586536	28.366554
293.516152	15531.341897	28.371572
293.308937	15557.247258	28.376589
293.893966	15573.542932	28.381607
294.084375	15604.578308	28.386624
294.357350	15620.478038	28.391642
294.838554	15640.555689	28.396660
294.915086	15676.394366	28.401677
295.445071	15688.639793	28.406695
295.527980	15733.808316	28.411712
295.782394	15754.213538	28.416730
296.348113	15772.170433	28.421748
296.494576	15804.039213	28.426765
296.685321	15809.832361	28.431783
297.270990	15829.008912	28.436800
297.482549	15859.445593	28.441818
297.878610	15874.795736	28.446836
298.293652	15894.745954	28.451853
298.651522	15908.272822	28.456871
299.006195	15931.592875	28.461888
299.354149	15955.517642	28.466906
299.567984	15960.646726	28.471924
300.062962	15978.711667	28.476941
300.102042	16000.755470	28.481959
300.257642	16008.891567	28.486976
300.505171	16034.471987	28.491994
300.721614	16063.742068	28.497012
300.954067	16066.200088	28.502029
301.113579	16085.007669	28.507047
301.402977	16118.178794	28.512064
301.743584	16141.272963	28.517082
302.068259	16144.615610	28.522100
302.226423	16174.726030	28.527117
302.694749	16208.925224	28.532135
302.803489	16220.870307	28.537152
302.985134	16260.572839	28.542170
303.667377	16276.786971	28.547188
303.862128	16310.519399	28.552205
303.992528	16327.793954	28.557223
304.588093	16359.627446	28.562240
304.740022	16385.303008	28.567258
305.233440	16410.066453	28.572276
305.391840	16420.829397	28.577293
305.965974	16442.687692	28.582311
306.230833	16468.519658	28.587328
306.128477	16482.526483	28.592346
306.685405	16521.200013	28.597364
306.930235	16533.967554	28.602381
307.215950	16563.157746	28.607399
307.624197	16583.224976	28.612416
307.514912	16634.544061	28.617434
307.912578	16655.002392	28.622452
307.985065	16685.967902	28.627469
308.183652	16719.962152	28.632487
308.857526	16738.196955	28.637504
308.864443	16782.640224	28.642522
309.572729	16808.913240	28.647540
309.673146	16849.916629	28.652557
310.354419	16877.699288	28.657575
311.240668	16883.500842	28.662592
311.737377	16915.438432	28.667610
312.163651	16916.031677	28.672628
312.248450	16934.092950	28.677645
312.413714	16956.813788	28.682663
313.028444	16984.558768	28.687680
312.889117	16992.485616	28.692698
313.330526	17011.810326	28.697716
313.594889	17039.211402	28.702733
314.106120	17058.095957	28.707751
314.632173	17053.887959	28.712768
314.307121	17101.072458	28.717786
314.653819	17103.009013	28.722804
314.748684	17146.683830	28.727821
315.065065	17176.201014	28.732839
315.634707	17190.232961	28.737856
315.688562	17210.329567	28.742874
316.029768	17236.233663	28.747892
316.179498	17260.150540	28.752909
316.429643	17298.247759	28.757927
316.839209	17328.005139	28.762944
316.964779	17362.510814	28.767962
317.618275	17390.127148	28.772980
317.781909	17427.777179	28.777997
318.080187	17462.226163	28.783015
318.588292	17473.737387	28.788032
318.566080	17510.601919	28.793050
319.247963	17537.358014	28.798068
319.577421	17565.590830	28.803085
319.897280	17579.158464	28.808103
320.442984	17617.992474	28.813120
320.401273	17646.250500	28.818138
320.681547	17654.191876	28.823156
321.215197	17700.279558	28.828173
321.276886	17712.022309	28.833191
321.887308	17721.285086	28.838208
322.338732	17747.502757	28.843226
322.493818	17762.355473	28.848244
322.843396	17794.115772	28.853261
323.125730	17812.670213	28.858279
323.543545	17814.790541	28.863296
323.596090	17850.444086	28.868314
323.991576	17896.135905	28.873332
324.179005	17925.997265	28.878349
324.185622	17933.867357	28.883367
324.751211	17961.431407	28.888384
324.718824	18014.192111	28.893402
325.358129	18030.634164	28.898420
325.444677	18065.053196	28.903437
325.771859	18106.014380	28.908455
326.388150	18132.590001	28.913472
326.099962	18170.499208	28.918490
326.937604	18207.776465	28.923508
327.489342	18227.927608	28.928525
327.501836	18255.946036	28.933543
328.143229	18299.092312	28.938560
328.682274	18318.686138	28.943578
328.913037	18354.894501	28.948596
329.305194	18380.907046	28.953613
330.090702	18391.682741	28.958631
330.689258	18409.875116	28.963648
331.152675	18417.640026	28.968666
331.335364	18420.696103	28.973684
331.631186	18459.704207	28.978701
331.887927	18470.286758	28.983719
332.199036	18503.055635	28.988736
332.382790	18532.754785	28.993754
332.572214	18524.808239	28.998772
332.868995	18550.075527	29.003789
332.825601	18592.535020	29.008807
333.461748	18616.204864	29.013824
333.458292	18650.192360	29.018842
333.848794	18689.585712	29.023860
334.277636	18702.338731	29.028877
334.288032	18715.657383	29.033895
334.983952	18754.292733	29.038912
335.181876	18780.566543	29.043930
335.320643	18812.661534	29.048948
335.188887	18861.132097	29.053965
335.969340	18887.590400	29.058983
336.544674	18937.011446	29.064000
336.632631	18970.743343	29.069018
336.857714	18983.487685	29.074036
337.313847	19030.892263	29.079053
337.182009	19060.166912	29.084071
337.909791	19095.565011	29.089088
338.138677	19137.512789	29.094106
338.630189	19183.840139	29.099124
339.142179	19203.133706	29.104141
339.471234	19233.319230	29.109159
340.226745	19273.813772	29.114176
340.808988	19303.210466	29.119194
340.736691	19333.106252	29.124212
341.331043	19338.093147	29.129229
341.437880	19373.876572	29.134247
342.008231	19393.520101	29.139264
342.304835	19423.233735	29.144282
342.447758	19454.311038	29.149300
342.868867	19481.209536	29.154317
343.145969	19513.174273	29.159335
343.325729	19543.038254	29.164352
343.701004	19553.017131	29.169370
343.991538	19570.859736	29.174388
344.504431	19607.169252	29.179405
344.698034	19642.563776	29.184423
345.041949	19658.074254	29.189440
345.174745	19697.635534	29.194458
345.649987	19720.594282	29.199476
345.821346	19760.158799	29.204493
346.198064	19780.252489	29.209511
346.859187	19809.266630	29.214528
347.037769	19819.848774	29.219546
347.052587	19868.299646	29.224564
347.708225	19897.488239	29.229581
347.847261	19942.126274	29.234599
348.603751	19968.107930	29.239616
348.814860	19995.984579	29.244634
349.240301	20015.227190	29.249652
349.523791	20043.438746	29.254669
349.636556	20082.701605	29.259687
350.279948	20097.412703	29.264704
350.895084	20136.419303	29.269722
351.270896	20181.214327	29.274740
351.443827	20190.946435	29.279757
351.434919	20223.779476	29.284775
351.723630	20261.008622	29.289792
352.228202	20282.026012	29.294810
352.307268	20323.817118	29.299828
352.859546	20360.684528	29.304845
353.176325	20403.927767	29.309863
353.617329	20447.984477	29.314880
354.169897	20477.714465	29.319898
354.381758	20518.194678	29.324916
354.990892	20535.824903	29.329933
355.115354	20554.020730	29.334951
355.589239	20599.196341	29.339968
356.152072	20642.762113	29.344986
356.303216	20669.068719	29.350004
356.647512	20685.317831	29.355021
356.856457	20733.893640	29.360039
357.541069	20744.150017	29.365056
357.918512	20785.700674	29.370074
358.116800	20821.048070	29.375092
358.418977	20845.876592	29.380109
358.394325	20894.102095	29.385127
358.881758	20931.221095	29.390144
359.241423	20945.746517	29.395162
359.872970	20993.152954	29.400180
360.339276	21033.868255	29.405197
360.502120	21083.007587	29.410215
360.956088	21104.899821	29.415232
361.493128	21132.012001	29.420250
362.118314	21172.622574	29.425268
362.687852	21179.240981	29.430285
362.621905	21196.311887	29.435303
363.049437	21241.342414	29.440320
363.339323	21272.833930	29.445338
363.949692	21282.737180	29.450356
364.520789	21324.684400	29.455373
364.188137	21351.153980	29.460391
365.137063	21370.690025	29.465408
364.995298	21403.162692	29.470426
365.474867	21440.091803	29.475444
366.202532	21468.519309	29.480461
366.362940	21503.956386	29.485479
366.600759	21529.562707	29.490496
366.519773	21556.484461	29.495514
367.013783	21592.777796	29.500532
367.743559	21608.756040	29.505549
367.635416	21653.991256	29.510567
368.285705	21703.228450	29.515584
368.724610	21701.352658	29.520602
368.960144	21744.318004	29.525620
369.317679	21770.887050	29.530637
369.666972	21785.515814	29.535655
369.752152	21824.926067	29.540672
369.832802	21840.543561	29.545690
370.421371	21900.599780	29.550708
371.132793	21949.840215	29.555725
371.101783	21987.900090	29.560743
371.685361	22003.951737	29.565760
371.998268	22052.960356	29.570778
372.277401	22081.448819	29.575796
372.647289	22118.214677	29.580813
373.011956	22160.976888	29.585831
373.287679	22204.695072	29.590848
373.833531	22240.233991	29.595866
373.998250	22263.884462	29.600884
374.745106	22317.423985	29.605901
375.136063	22355.968341	29.610919
375.518083	22365.900505	29.615936
375.692424	22414.893662	29.620954
376.083411	22463.296236	29.625972
376.786855	22497.996182	29.630989
377.025604	22540.261487	29.636007
377.718770	22564.674833	29.641024
378.222130	22589.250424	29.646042
378.335142	22634.404456	29.651060
379.175034	22659.588278	29.656077
379.002080	22692.672412	29.661095
379.584971	22706.134586	29.666112
380.491219	22737.298441	29.671130
380.498241	22787.036080	29.676148
380.954083	22798.510789	29.681165
381.475747	22845.349432	29.686183
381.642501	22878.223308	29.691200
382.328050	22888.816671	29.696218
381.865509	22941.014524	29.701236
382.699478	22961.466923	29.706253
382.878661	23005.852693	29.711271
383.384825	23053.350332	29.716288
383.539336	23074.118493	29.721306
383.740654	23121.375018	29.726324
384.583171	23150.770207	29.731341
384.801171	23184.410321	29.736359
385.389315	23235.137980	29.741376
385.620275	23256.010405	29.746394
385.660029	23301.347027	29.751412
386.411350	23325.051866	29.756429
386.377308	23378.723784	29.761447
386.940172	23428.160228	29.766464
387.658909	23446.629958	29.771482
387.962164	23484.125604	29.776500
388.417873	23528.091834	29.781517
388.805961	23558.899787	29.786535
389.320784	23592.988321	29.791552
389.923159	23638.308585	29.796570
389.863484	23662.628750	29.801588
390.379501	23690.603092	29.806605
390.791787	23712.860375	29.811623
391.458813	23768.345950	29.816640
391.648545	23784.147467	29.821658
391.925569	23799.757993	29.826676
392.234278	23852.318442	29.831693
392.409681	23893.504993	29.836711
393.007876	23926.013232	29.841728
393.456347	23968.353118	29.846746
393.616956	23998.581403	29.851764
394.231777	24045.669728	29.856781
394.385189	24057.900034	29.861799
394.587119	24087.643919	29.866816
395.026073	24141.057231	29.871834
395.364617	24169.503158	29.876852
395.811610	24214.092255	29.881869
395.828436	24265.109754	29.886887
396.309956	24302.423256	29.891904
396.740011	24327.484934	29.896922
396.917263	24382.328158	29.901940
397.456970	24436.726966	29.906957
397.795572	24474.674644	29.911975
397.903859	24537.075906	29.916992
398.943257	24576.502105	29.922010
399.154528	24617.495289	29.927028
399.689395	24653.367510	29.932045
399.760249	24686.886718	29.937063
400.151281	24743.780237	29.942080
400.783191	24786.255851	29.947098
401.088229	24831.311514	29.952116
401.539706	24877.437371	29.957133
402.158595	24921.124841	29.962151
402.472138	24953.937520	29.967168
403.318076	24991.873502	29.972186
403.808407	25051.007993	29.977204
404.160287	25081.794750	29.982221
404.906703	25110.509158	29.987239
404.682838	25170.388026	29.992256
405.273619	25191.840423	29.997274
405.620673	25226.751516	30.002292
406.342132	25277.638318	30.007309
406.992211	25320.094926	30.012327
407.075087	25345.786266	30.017344
407.728605	25393.576781	30.022362
407.627127	25439.063878	30.027380
408.380926	25451.186550	30.032397
408.798448	25490.976212	30.037415
409.577877	25518.894304	30.042432
409.616842	25562.408019	30.047450
409.831669	25612.411355	30.052468
410.527022	25628.775989	30.057485
410.925984	25678.488927	30.062503
411.587680	25705.606827	30.067520
411.697183	25749.893052	30.072538
412.298377	25785.955397	30.077556
412.557516	25797.094095	30.082573
412.957748	25848.724752	30.087591
413.193638	25889.980277	30.092608
414.374524	25907.960081	30.097626
415.199698	25945.508998	30.102644
415.426965	25966.615602	30.107661
416.046790	25979.101387	30.112679
416.332356	25991.894694	30.117696
416.705386	26033.325020	30.122714
416.810923	26063.342172	30.127732
417.132600	26084.035958	30.132749
417.579906	26125.211400	30.137767
418.077648	26153.700592	30.142784
417.953382	26187.868396	30.147802
418.278320	26224.548136	30.152820
418.458438	26247.619779	30.157837
419.003402	26304.549869	30.162855
418.819090	26352.710136	30.167872
419.419217	26391.706952	30.172890
419.415150	26445.962346	30.177908
420.000115	26505.220303	30.182925
420.119117	26547.263102	30.187943
420.495383	26580.450172	30.192960
421.236826	26639.496671	30.197978
421.541871	26686.361241	30.202996
421.925712	26732.514346	30.208013
422.568123	26782.693330	30.213031
422.448121	26828.127270	30.218048
423.085161	26881.335136	30.223066
423.521940	26953.343419	30.228084
424.249501	26989.042090	30.233101
424.354227	27032.116609	30.238119
424.630997	27097.394707	30.243136
425.554021	27127.488422	30.248154
425.907935	27192.486057	30.253172
426.389154	27249.883996	30.258189
426.945922	27282.902263	30.263207
426.901803	27333.792371	30.268224
427.472668	27381.234685	30.273242
428.129190	27420.292347	30.278260
428.374524	27483.855045	30.283277
428.897155	27553.591844	30.288295
429.175023	27597.733619	30.293312
429.604712	27639.141135	30.298330
430.322062	27709.521361	30.303348
430.642555	27757.447640	30.308365
431.183680	27793.267103	30.313383
431.781594	27853.738745	30.318400
432.537642	27893.295155	30.323418
433.012004	27937.313878	30.328436
433.301797	27989.595332	30.333453
433.700046	28027.381795	30.338471
433.864017	28066.799856	30.343488
434.803561	28115.713035	30.348506
434.875698	28173.834543	30.353524
435.324997	28221.176254	30.358541
435.732079	28266.673600	30.363559
436.427584	28314.126295	30.368576
436.646587	28361.380270	30.373594
437.335011	28385.064738	30.378612
437.786444	28434.775450	30.383629
438.447609	28499.768286	30.388647
438.797084	28550.773613	30.393664
439.206404	28573.245930	30.398682
439.674471	28620.443704	30.403700
439.637045	28673.651847	30.408717
440.482489	28705.451808	30.413735
440.676521	28756.202697	30.418752
441.001187	28803.273257	30.423770
441.688235	28853.353152	30.428788
441.988204	28915.161519	30.433805
442.708037	28955.830347	30.438823
443.002520	28994.964017	30.443840
443.763564	29040.291384	30.448858
444.123522	29088.211699	30.453876
444.471859	29126.743768	30.458893
444.920785	29180.125475	30.463911
445.424453	29230.918087	30.468928
445.699053	29250.344409	30.473946
446.188588	29314.248893	30.478964
446.751177	29340.311740	30.483981
447.373009	29384.767183	30.488999
447.525756	29445.049838	30.494016
448.168579	29484.063989	30.499034
448.677748	29535.484303	30.504052
449.137461	29570.144342	30.509069
449.724126	29600.001458	30.514087
450.170615	29640.165040	30.519104
450.452927	29678.431663	30.524122
450.714499	29725.439456	30.529140
451.298191	29762.845802	30.534157
451.803728	29802.372283	30.539175
451.665350	29862.363806	30.544192
452.141127	29890.589982	30.549210
452.598473	29923.099806	30.554228
452.691555	29964.682078	30.559245
453.601755	30021.002671	30.564263
453.463928	30071.850096	30.569280
453.939430	30128.138747	30.574298
454.727101	30174.420497	30.579316
455.298658	30229.756733	30.584333
455.815191	30279.641810	30.589351
456.159501	30330.706873	30.594368
456.839282	30385.669271	30.599386
457.164895	30432.315097	30.604404
457.282067	30500.667098	30.609421
458.066455	30538.209159	30.614439
458.150164	30580.419054	30.619456
458.557006	30631.645017	30.624474
459.393580	30700.841109	30.629492
459.623188	30750.292287	30.634509
460.316971	30791.729993	30.639527
460.483005	30864.337196	30.644544
460.826585	30921.158101	30.649562
461.762534	30981.834077	30.654580
461.949237	31038.144993	30.659597
462.586391	31097.022116	30.664615
463.007706	31141.354304	30.669632
463.353533	31187.430981	30.674650
463.822923	31239.127910	30.679668
464.152652	31315.189548	30.684685
464.586821	31358.586381	30.689703
465.165416	31427.282218	30.694720
465.694685	31479.329604	30.699738
466.533376	31550.011438	30.704756
466.604455	31594.749654	30.709773
467.341876	31643.292944	30.714791
467.835428	31702.495534	30.719808
468.276619	31763.069831	30.724826
468.856416	31810.472363	30.729844
469.291212	31882.657683	30.734861
470.012550	31919.957608	30.739879
470.497276	31972.256741	30.744896
470.840134	32038.356513	30.749914
471.595078	32072.521643	30.754932
471.944554	32127.159216	30.759949
472.260145	32181.212603	30.764967
472.841295	32255.028419	30.769984
473.038489	32293.229673	30.775002
473.765697	32336.681489	30.780020
474.090035	32410.881108	30.785037
474.476895	32436.207847	30.790055
474.977359	32495.039704	30.795072
475.277880	32565.546380	30.800090
475.636884	32619.502457	30.805108
475.876859	32683.962176	30.810125
476.726851	32737.925851	30.815143
477.105570	32781.029349	30.820160
477.433576	32851.759791	30.825178
478.176724	32905.284162	30.830196
478.641323	32958.719045	30.835213
479.263953	33029.802220	30.840231
479.964606	33075.825262	30.845248
480.483960	33120.285096	30.850266
481.336112	33178.843460	30.855284
481.725736	33222.378477	30.860301
482.146425	33250.963099	30.865319
482.623642	33315.657281	30.870336
482.942341	33355.768507	30.875354
483.435931	33394.380681	30.880372
483.734963	33460.458347	30.885389
484.470243	33493.673517	30.890407
484.694967	33550.746605	30.895424
484.872671	33576.958258	30.900442
485.416552	33645.958801	30.905460
485.580533	33699.035429	30.910477
486.534540	33734.496067	30.915495
486.536921	33787.788963	30.920512
487.118846	33848.211546	30.925530
487.976187	33904.395654	30.930548
488.743691	33942.345378	30.935565
489.346403	33999.568878	30.940583
489.819237	34042.334941	30.945600
490.171726	34089.916856	30.950618
490.856157	34150.206801	30.955636
490.647312	34196.285199	30.960653
491.364614	34243.526455	30.965671
491.786147	34319.289363	30.970688
492.072863	34355.158068	30.975706
492.426625	34420.952633	30.980724
492.676480	34491.421753	30.985741
493.555417	34547.689537	30.990759
493.601601	34618.987933	30.995776
494.292169	34680.389330	31.000794
495.017231	34736.351828	31.005812
495.051372	34818.866932	31.010829
495.835198	34881.039293	31.015847
496.168031	34940.206766	31.020864
497.124290	35015.818068	31.025882
497.785361	35064.408674	31.030900
497.997196	35127.938524	31.035917
498.590434	35196.854934	31.040935
499.354663	35244.482381	31.045952
499.330267	35313.261454	31.050970
500.028393	35385.143119	31.055988
500.258013	35460.084336	31.061005
501.073529	35498.411280	31.066023
501.733008	35583.477205	31.071040
502.298040	35640.819524	31.076058
503.388627	35682.354704	31.081076
503.231464	35754.937659	31.086093
503.973809	35811.626457	31.091111
504.867691	35858.451578	31.096128
504.841832	35933.604232	31.101146
505.883889	35972.308152	31.106164
506.150554	36033.803190	31.111181
506.554049	36090.618271	31.116199
507.596571	36153.885200	31.121216
507.301231	36214.807873	31.126234
508.044988	36255.483418	31.131252
508.118075	36330.618245	31.136269
508.687388	36390.780205	31.141287
509.305296	36453.704954	31.146304
509.773539	36520.302532	31.151322
510.101911	36579.886428	31.156340
510.339604	36659.081976	31.161357
511.162562	36709.385939	31.166375
511.662957	36776.181121	31.171392
512.220526	36853.036843	31.176410
512.976877	36905.031176	31.181428
513.289167	36988.352955	31.186445
513.884654	37039.730490	31.191463
514.543109	37078.970382	31.196480
515.256726	37150.342234	31.201498
516.016235	37191.500139	31.206516
516.631959	37244.194013	31.211533
517.182608	37294.326860	31.216551
518.284886	37323.417687	31.221568
518.640797	37375.346991	31.226586
519.246299	37409.982638	31.231604
519.590406	37455.028243	31.236621
520.155330	37509.277619	31.241639
520.684651	37531.811036	31.246656
520.810059	37575.154228	31.251674
521.208842	37619.190827	31.256692
521.518246	37691.890771	31.261709
521.845293	37738.817617	31.266727
522.483774	37777.525853	31.271744
522.628766	37833.391930	31.276762
522.847642	37914.442305	31.281780
523.137361	37979.894513	31.286797
523.628819	38039.513134	31.291815
524.285831	38128.309212	31.296832
524.409969	38190.841935	31.301850
525.185461	38270.823646	31.306868
525.361534	38339.057360	31.311885
526.116080	38421.053526	31.316903
526.637502	38483.556359	31.321920
526.717706	38555.281434	31.326938
527.607350	38648.204373	31.331956
528.185226	38729.546277	31.336973
528.807433	38807.176069	31.341991
529.319412	38884.799153	31.347008
529.795230	38960.474957	31.352026
530.498940	39034.819455	31.357044
531.290895	39097.576401	31.362061
531.773952	39178.595137	31.367079
532.393128	39256.684994	31.372096
532.899426	39327.430646	31.377114
533.672590	39382.875845	31.382132
533.900306	39471.339153	31.387149
534.610859	39561.077125	31.392167
535.445482	39620.754759	31.397184
535.719685	39683.062713	31.402202
536.530109	39750.644653	31.407220
537.212533	39797.508691	31.412237
537.472134	39877.630081	31.417255
538.056577	39953.077475	31.422272
538.690228	40027.497596	31.427290
539.205252	40087.131714	31.432308
539.826189	40166.437200	31.437325
540.214192	40228.961795	31.442343
541.051757	40274.318001	31.447360
541.498407	40376.823363	31.452378
542.224924	40423.886898	31.457396
542.885688	40495.615299	31.462413
543.062998	40569.364973	31.467431
543.869277	40617.870899	31.472448
544.224386	40680.380387	31.477466
544.641383	40750.783365	31.482484
545.040384	40834.547315	31.487501
545.694491	40898.797825	31.492519
546.603836	40960.282443	31.497536
546.742418	41041.407431	31.502554
547.387564	41093.031356	31.507572
547.992517	41172.788925	31.512589
548.272396	41241.720304	31.517607
549.353326	41290.059559	31.522624
550.216120	41373.992429	31.527642
550.666395	41432.524269	31.532660
551.137591	41490.532023	31.537677
551.822786	41549.599915	31.542695
552.485835	41598.747630	31.547712
552.935851	41654.644551	31.552730
553.275636	41711.633066	31.557748
553.773727	41784.690740	31.562765
554.017866	41826.585117	31.567783
555.044410	41878.577559	31.572800
555.034006	41943.111961	31.577818
555.641442	42000.290752	31.582836
555.765324	42079.566716	31.587853
556.137823	42135.114903	31.592871
556.746716	42212.313211	31.597888
557.273028	42296.343774	31.602906
557.695987	42369.280457	31.607924
558.440636	42450.693543	31.612941
558.400870	42519.751979	31.617959
559.296211	42592.816710	31.622976
560.095799	42676.207266	31.627994
561.216444	42738.032303	31.633012
561.572890	42813.289279	31.638029
562.077303	42896.155069	31.643047
563.120414	42960.215992	31.648064
563.392263	43046.315482	31.653082
564.201712	43101.529257	31.658100
564.792684	43164.046156	31.663117
565.256823	43251.036619	31.668135
565.784225	43309.002964	31.673152
565.874510	43387.721898	31.678170
566.656433	43460.521545	31.683188
567.281765	43553.004925	31.688205
567.582701	43625.581612	31.693223
568.334027	43695.833356	31.698240
568.302690	43777.380485	31.703258
568.786089	43851.354828	31.708276
569.937714	43936.040938	31.713293
570.520205	44017.358308	31.718311
570.942377	44091.065916	31.723328
571.450479	44172.708792	31.728346
572.224196	44254.949019	31.733364
572.973292	44343.002495	31.738381
573.310918	44437.545655	31.743399
574.254094	44485.429918	31.748416
574.692083	44575.319585	31.753434
574.999100	44649.897673	31.758452
576.030011	44736.094344	31.763469
576.550723	44802.015892	31.768487
577.295686	44887.891125	31.773504
577.984412	44958.416885	31.778522
578.361108	45023.838934	31.783540
578.956059	45107.912011	31.788557
579.477583	45179.492284	31.793575
580.014966	45259.184017	31.798592
580.470178	45341.551129	31.803610
581.008428	45411.140536	31.808628
581.810137	45506.682762	31.813645
582.193980	45592.308337	31.818663
582.895988	45659.052263	31.823680
583.332094	45738.083979	31.828698
583.868082	45826.466998	31.833716
584.547506	45901.698972	31.838733
584.915456	45980.079952	31.843751
585.514944	46075.225953	31.848768
585.986363	46142.016009	31.853786
586.654721	46217.560498	31.858804
587.408637	46324.484197	31.863821
587.736842	46399.621481	31.868839
588.405506	46491.821875	31.873856
589.306678	46589.898033	31.878874
589.623301	46653.008758	31.883892
590.436230	46720.429623	31.888909
590.971746	46810.525513	31.893927
591.661970	46855.691797	31.898944
592.278933	46944.230914	31.903962
592.895268	47021.732208	31.908980
593.199258	47090.564582	31.913997
593.741612	47189.344104	31.919015
594.128842	47243.026487	31.924032
594.672004	47333.871947	31.929050
594.930678	47410.290915	31.934068
595.678154	47480.188164	31.939085
596.100333	47581.019866	31.944103
596.884650	47672.496526	31.949120
597.135518	47752.274626	31.954138
597.901615	47863.530927	31.959156
598.666963	47943.467997	31.964173
599.300241	48025.880666	31.969191
600.118577	48125.162627	31.974208
600.786824	48207.207190	31.979226
601.298713	48290.468361	31.984244
602.243298	48384.767041	31.989261
602.687526	48467.733878	31.994279
603.643605	48551.986973	31.999296
604.280870	48631.427100	32.004314
604.730508	48724.116700	32.009332
605.198101	48786.723363	32.014349
605.625589	48878.277443	32.019367
606.428099	48986.878703	32.024384
607.187601	49066.145738	32.029402
607.256798	49137.215854	32.034420
608.112168	49229.383040	32.039437
608.742534	49320.267875	32.044455
609.523810	49402.700002	32.049472
610.266950	49499.904815	32.054490
611.159326	49583.203572	32.059508
611.627504	49672.301119	32.064525
612.000145	49749.759138	32.069543
612.517035	49841.653628	32.074560
613.195761	49920.539683	32.079578
613.832109	50005.272055	32.084596
614.814330	50105.993144	32.089613
614.904523	50187.317539	32.094631
615.707992	50270.555045	32.099648
616.493029	50340.308247	32.104666
616.922712	50445.060383	32.109684
617.726510	50535.811858	32.114701
618.157043	50625.368522	32.119719
618.845143	50719.358004	32.124736
619.714861	50809.717773	32.129754
620.212459	50891.704236	32.134772
620.922961	50971.274695	32.139789
621.428138	51075.847287	32.144807
622.154863	51154.515774	32.149824
622.857026	51224.825936	32.154842
623.170343	51321.365720	32.159860
623.867594	51408.241800	32.164877
624.284231	51499.371296	32.169895
625.285044	51594.096657	32.174912
625.870174	51681.665188	32.179930
626.293648	51767.880680	32.184948
626.743901	51860.064339	32.189965
627.522640	51943.445865	32.194983
628.431120	52008.737972	32.200000
629.109038	52114.547845	32.205018
629.726832	52206.544425	32.210036
630.782655	52278.110729	32.215053
631.197514	52381.881046	32.220071
631.583130	52454.152459	32.225088
632.488568	52520.890165	32.230106
632.675276	52612.258733	32.235124
633.454207	52681.001330	32.240141
633.649484	52760.348472	32.245159
634.955240	52861.106430	32.250176
635.250209	52922.476023	32.255194
636.180261	52999.615093	32.260212
636.954617	53081.713647	32.265229
637.125891	53159.212397	32.270247
637.766608	53240.038736	32.275264
638.669809	53311.981523	32.280282
639.184989	53416.688377	32.285300
640.014564	53478.483117	32.290317
640.377824	53584.662560	32.295335
640.888159	53650.976705	32.300352
641.623543	53735.061704	32.305370
641.724556	53825.619468	32.310388
642.825825	53912.424330	32.315405
643.354330	53999.204152	32.320423
643.918907	54090.191962	32.325440
644.523362	54181.382081	32.330458
645.041254	54282.972468	32.335476
645.616819	54364.679724	32.340493
646.434808	54453.359485	32.345511
647.266551	54567.590980	32.350528
648.262368	54648.844667	32.355546
648.482414	54754.997307	32.360564
649.198392	54826.954530	32.365581
649.908222	54929.666366	32.370599
650.295774	55030.751518	32.375616
651.144856	55125.942538	32.380634
651.899116	55200.699796	32.385652
652.223517	55308.221755	32.390669
653.035229	55412.384984	32.395687
653.512863	55506.558897	32.400704
654.298342	55624.247339	32.405722
654.770280	55717.620864	32.410740
655.658021	55805.303378	32.415757
656.427650	55916.312034	32.420775
656.591063	56000.962483	32.425792
657.591386	56112.913412	32.430810
658.110412	56207.898864	32.435828
658.664827	56309.253688	32.440845
659.293164	56426.416929	32.445863
659.788158	56529.671767	32.450880
660.291205	56623.126601	32.455898
661.056405	56735.126230	32.460916
661.754033	56838.658810	32.465933
662.493951	56943.385389	32.470951
663.172684	57064.518196	32.475968
663.925086	57176.895225	32.480986
664.694253	57284.032329	32.486004
665.681344	57382.522260	32.491021
666.536903	57475.872378	32.496039
667.205166	57576.905334	32.501056
667.798679	57672.024555	32.506074
667.973516	57787.381608	32.511092
669.230053	57861.421579	32.516109
670.057629	57975.123920	32.521127
670.312115	58083.386586	32.526144
671.152087	58174.638532	32.531162
671.903133	58281.613441	32.536180
672.624534	58370.800759	32.541197
673.008603	58468.782795	32.546215
673.796488	58569.068107	32.551232
674.664208	58657.821842	32.556250
675.048520	58764.082727	32.561268
675.846138	58869.315477	32.566285
676.502507	58963.318423	32.571303
676.950903	59047.840088	32.576320
677.851313	59150.283410	32.581338
678.296758	59245.042866	32.586356
678.943552	59330.373370	32.591373
679.827261	59419.582825	32.596391
680.690009	59506.483418	32.601408
681.180005	59615.985640	32.606426
681.609714	59729.163432	32.611444
682.036796	59805.527700	32.616461
682.906362	59909.155354	32.621479
683.439246	60024.080791	32.626496
684.063345	60114.555812	32.631514
685.136913	60237.879751	32.636532
685.263875	60338.782337	32.641549
685.999816	60435.957631	32.646567
686.765599	60554.797159	32.651584
687.868812	60646.193900	32.656602
687.965810	60773.303362	32.661620
688.795038	60872.506505	32.666637
689.834788	60984.724896	32.671655
690.153612	61078.281669	32.676672
690.684596	61173.889256	32.681690
691.771734	61309.685812	32.686708
692.595231	61432.003038	32.691725
693.412626	61529.334481	32.696743
693.778988	61622.235017	32.701760
694.692678	61730.952064	32.706778
695.358631	61861.601897	32.711796
696.229891	61962.143241	32.716813
697.086459	62072.950744	32.721831
697.729824	62191.282981	32.726848
698.293707	62276.285805	32.731866
698.885420	62397.686558	32.736884
699.485552	62500.575775	32.741901
700.374693	62600.460078	32.746919
700.556276	62717.993192	32.751936
701.473609	62832.934375	32.756954
702.214192	62961.600839	32.761972
702.676371	63078.324980	32.766989
703.906843	63178.528644	32.772007
704.531198	63305.389982	32.777024
705.412646	63409.937462	32.782042
705.628854	63529.902810	32.787060
706.403791	63628.471155	32.792077
707.284876	63761.107529	32.797095
707.774305	63885.852202	32.802112
708.750093	63982.859583	32.807130
709.693930	64110.684427	32.812148
710.551638	64212.364185	32.817165
711.479053	64293.403093	32.822183
712.315923	64417.550082	32.827200
713.331611	64528.553278	32.832218
714.301216	64633.541230	32.837236
714.822990	64721.316976	32.842253
715.721563	64824.332987	32.847271
716.079185	64917.603983	32.852288
717.159978	65012.411983	32.857306
717.805209	65113.012557	32.862324
718.218142	65210.978331	32.867341
719.053305	65309.608047	32.872359
719.407042	65418.860771	32.877376
719.938942	65510.525490	32.882394
720.630966	65637.219461	32.887412
721.488468	65740.588180	32.892429
722.368710	65845.034535	32.897447
722.723636	65959.220227	32.902464
723.632809	66050.407865	32.907482
724.358995	66158.174467	32.912500
725.052658	66255.213912	32.917517
725.590860	66344.403462	32.922535
726.180936	66454.855252	32.927552
727.003166	66554.744642	32.932570
727.620697	66667.455992	32.937588
728.314300	66772.291847	32.942605
729.282463	66861.848787	32.947623
729.491395	66970.021104	32.952640
730.077164	67088.144646	32.957658
730.798732	67193.995743	32.962676
731.295322	67305.617987	32.967693
732.029760	67444.149581	32.972711
732.962575	67557.053913	32.977728
733.758452	67654.841608	32.982746
734.525337	67787.118222	32.987764
735.341403	67908.742110	32.992781
735.949733	68015.924650	32.997799
736.471548	68151.449078	33.002816
737.090891	68253.636961	33.007834
738.208675	68393.932199	33.012852
738.789344	68515.996768	33.017869
739.519510	68612.086625	33.022887
739.942477	68748.244459	33.027904
740.798295	68874.020816	33.032922
741.549130	68999.145149	33.037940
742.409798	69143.034434	33.042957
743.267387	69252.546543	33.047975
743.981116	69402.543571	33.052992
744.755366	69515.743883	33.058010
745.312013	69633.115356	33.063028
745.910502	69773.360187	33.068045
747.029981	69908.468538	33.073063
747.881247	70026.640719	33.078080
749.075749	70163.337824	33.083098
749.903638	70276.615563	33.088116
750.512921	70409.977938	33.093133
751.502165	70518.229410	33.098151
752.336566	70655.912233	33.103168
753.128297	70763.502122	33.108186
754.055884	70873.327225	33.113204
754.737165	70989.180932	33.118221
755.635931	71077.066645	33.123239
756.614735	71210.632271	33.128256
757.643391	71332.057528	33.133274
758.119456	71424.503499	33.138292
758.826330	71528.501098	33.143309
759.698846	71655.075304	33.148327
760.321317	71761.958466	33.153344
761.008224	71871.253124	33.158362
761.791956	71979.027540	33.163380
762.353650	72100.060097	33.168397
763.295590	72217.356994	33.173415
764.238472	72335.318281	33.178432
764.851982	72435.478795	33.183450
765.763065	72556.336112	33.188468
766.375286	72667.423927	33.193485
766.991034	72789.659154	33.198503
767.864280	72896.633055	33.203520
768.684757	73007.694572	33.208538
769.210412	73131.350347	33.213556
769.840527	73246.402789	33.218573
770.653068	73366.623355	33.223591
771.188592	73491.183787	33.228608
772.186096	73607.619186	33.233626
773.099663	73734.066153	33.238644
773.491089	73845.980626	33.243661
774.677909	73975.260988	33.248679
775.101332	74077.281691	33.253696
775.793099	74192.126672	33.258714
776.716172	74318.132866	33.263732
777.115405	74423.997530	33.268749
777.955323	74556.588931	33.273767
778.700476	74666.925292	33.278784
779.731900	74765.819878	33.283802
780.735897	74879.548278	33.288820
781.153725	75010.245527	33.293837
782.034188	75127.062593	33.298855
782.562860	75230.854642	33.303872
783.138450	75374.181764	33.308890
784.284597	75489.483480	33.313908
784.752969	75599.326458	33.318925
785.087150	75732.071814	33.323943
785.857722	75868.786881	33.328960
786.851941	76009.879978	33.333978
787.546076	76152.282013	33.338996
788.236043	76276.029847	33.344013
788.932200	76418.578742	33.349031
789.350219	76555.590330	33.354048
790.281764	76720.280903	33.359066
791.031316	76853.666480	33.364084
791.491027	76994.278713	33.369101
792.775851	77147.068919	33.374119
793.269433	77292.243586	33.379136
794.083589	77450.723287	33.384154
795.251925	77601.537408	33.389172
795.762968	77738.041410	33.394189
796.873753	77898.265173	33.399207
797.353788	78044.136417	33.404224
798.574999	78196.527022	33.409242
799.443649	78349.337403	33.414260
799.769438	78485.092379	33.419277
800.488008	78657.491801	33.424295
801.555622	78808.254931	33.429312
802.330226	78958.529869	33.434330
803.163138	79113.489216	33.439348
804.273607	79255.867936	33.444365
804.920754	79417.399994	33.449383
805.983870	79569.743958	33.454400
807.367140	79693.010722	33.459418
808.388589	79830.056895	33.464436
808.943177	79996.244693	33.469453
809.886500	80109.662384	33.474471
810.571383	80255.368899	33.479488
811.679769	80393.302358	33.484506
812.862999	80517.599785	33.489524
813.312147	80675.131859	33.494541
814.415237	80812.474211	33.499559
815.292952	80935.843995	33.504576
815.960596	81068.800465	33.509594
817.182366	81188.876241	33.514612
817.548928	81312.402087	33.519629
818.161677	81465.301462	33.524647
819.418941	81579.503420	33.529664
819.937555	81727.252174	33.534682
820.770924	81877.511795	33.539700
821.389466	82006.123590	33.544717
822.062231	82131.526374	33.549735
822.852045	82280.866007	33.554752
823.845484	82425.289521	33.559770
824.621607	82553.113002	33.564788
825.369918	82710.913599	33.569805
826.235815	82848.446744	33.574823
826.797845	82992.584550	33.579840
827.687007	83149.004875	33.584858
828.117644	83280.697748	33.589876
829.106178	83432.928468	33.594893
829.632391	83569.060766	33.599911
830.504671	83708.812208	33.604928
830.831191	83860.237823	33.609946
832.104836	84012.716355	33.614964
832.580688	84153.750624	33.619981
833.390190	84309.540495	33.624999
834.369609	84445.691772	33.630016
835.026019	84604.937807	33.635034
835.928625	84754.679994	33.640052
836.863124	84920.164430	33.645069
837.503593	85062.265280	33.650087
838.364250	85214.895961	33.655104
838.872845	85360.803705	33.660122
839.949420	85537.973309	33.665140
840.873464	85695.158216	33.670157
841.650671	85849.666940	33.675175
842.354367	86017.234604	33.680192
842.970260	86190.043923	33.685210
844.012554	86358.988020	33.690228
844.723521	86521.003175	33.695245
845.778342	86667.461698	33.700263
846.806951	86843.238361	33.705280
847.525365	87001.358234	33.710298
848.930375	87165.781461	33.715316
849.737394	87331.563694	33.720333
850.301215	87500.683719	33.725351
851.342592	87655.243150	33.730368
851.951656	87822.928102	33.735386
853.205402	87985.977470	33.740404
853.988695	88156.995852	33.745421
854.775319	88332.583311	33.750439
856.289401	88472.953726	33.755456
856.682144	88665.888931	33.760474
857.978986	88806.626252	33.765492
858.780903	88972.851280	33.770509
859.148145	89123.393532	33.775527
860.376585	89289.164392	33.780544
861.589049	89439.594421	33.785562
862.897163	89577.252931	33.790580
863.974510	89736.711525	33.795597
864.976366	89881.787909	33.800615
865.783605	90022.069178	33.805632
866.381703	90187.728985	33.810650
867.621967	90321.581011	33.815668
867.951364	90485.616706	33.820685
868.798320	90627.413728	33.825703
869.620150	90783.903138	33.830720
870.291016	90949.214553	33.835738
871.421361	91081.956308	33.840756
871.751726	91262.481993	33.845773
872.456927	91423.519527	33.850791
873.554038	91567.078079	33.855808
874.352153	91744.644509	33.860826
875.069879	91908.189263	33.865844
875.951577	92050.432034	33.870861
876.813493	92235.471735	33.875879
877.769169	92390.905432	33.880896
878.674253	92574.307884	33.885914
879.848422	92738.941081	33.890932
880.440000	92919.701976	33.895949
881.131037	93085.448892	33.900967
882.304993	93235.858724	33.905984
882.862423	93386.839623	33.911002
884.161779	93566.248087	33.916020
884.772985	93742.929870	33.921037
885.811813	93892.600333	33.926055
886.650699	94063.607851	33.931072
887.334267	94243.762256	33.936090
888.327489	94383.424552	33.941108
889.252645	94535.718990	33.946125
889.900948	94706.370122	33.951143
891.077368	94854.916238	33.956160
892.054133	95013.464657	33.961178
892.745903	95173.864992	33.966196
893.496696	95334.712345	33.971213
894.097596	95502.243921	33.976231
895.222901	95653.316086	33.981248
895.982031	95835.514200	33.986266
896.894615	95991.073132	33.991284
897.490712	96169.749857	33.996301
898.177893	96340.349057	34.001319
899.059505	96524.753740	34.006336
900.078949	96688.091141	34.011354
901.180200	96861.581521	34.016372
902.408031	97041.312286	34.021389
903.419607	97226.378058	34.026407
904.166463	97392.157788	34.031424
904.893343	97588.211142	34.036442
906.012378	97746.987987	34.041460
906.740944	97910.381530	34.046477
907.734025	98096.121523	34.051495
908.775552	98266.947756	34.056512
909.326924	98458.359119	34.061530
910.262583	98653.266022	34.066548
911.106199	98840.644117	34.071565
911.638042	99007.185470	34.076583
912.635340	99208.859853	34.081600
913.664501	99398.958839	34.086618
914.377540	99592.029754	34.091636
915.581890	99783.318166	34.096653
916.171051	99978.241998	34.101671
917.269819	100156.484683	34.106688
918.028199	100355.871822	34.111706
919.135151	100564.357012	34.116724
920.275799	100770.989824	34.121741
920.840697	100949.193339	34.126759
922.076392	101156.041521	34.131776
922.906452	101340.598061	34.136794
924.206850	101533.719866	34.141812
925.012049	101741.061755	34.146829
925.399396	101925.372783	34.151847
926.962509	102130.351571	34.156864
927.565677	102332.173055	34.161882
928.704181	102522.290233	34.166900
929.836756	102714.676351	34.171917
930.431878	102889.450722	34.176935
931.716983	103099.117632	34.181952
932.549575	103311.653067	34.186970
934.141102	103478.986001	34.191988
935.226926	103679.136629	34.197005
935.993584	103871.262642	34.202023
937.177539	104047.581206	34.207040
937.949226	104235.789948	34.212058
938.992493	104414.894793	34.217076
939.877155	104599.402585	34.222093
940.609643	104794.947529	34.227111
941.522339	104970.646047	34.232128
942.601028	105167.592937	34.237146
944.170060	105343.533869	34.242164
945.197733	105503.387609	34.247181
945.947748	105682.676295	34.252199
947.323225	105851.459653	34.257216
948.594518	106019.305187	34.262234
949.592430	106191.926925	34.267252
950.662362	106348.068349	34.272269
951.161340	106529.873805	34.277287
952.148086	106684.986191	34.282304
952.932993	106842.716332	34.287322
953.993567	106984.546163	34.292340
954.764320	107166.621448	34.297357
955.300044	107315.213874	34.302375
956.152650	107457.739156	34.307392
956.616695	107631.446373	34.312410
957.832006	107829.587616	34.317428
958.570476	108003.555934	34.322445
959.080786	108179.298162	34.327463
960.336706	108365.785019	34.332480
960.761324	108538.833478	34.337498
962.004526	108729.707120	34.342516
962.681502	108941.750626	34.347533
963.529556	109120.571661	34.352551
964.322502	109321.352218	34.357568
965.171060	109538.691648	34.362586
966.373642	109738.280482	34.367604
966.968213	109928.243906	34.372621
967.930201	110140.110575	34.377639
968.798977	110355.540776	34.382656
970.132944	110563.346944	34.387674
970.807397	110779.597931	34.392692
972.003671	110989.140060	34.397709
972.725057	111210.427927	34.402727
973.830467	111413.414529	34.407744
974.469743	111631.704798	34.412762
975.310455	111853.978898	34.417780
976.730432	112082.707898	34.422797
977.022350	112301.428253	34.427815
978.097948	112517.500258	34.432832
979.254532	112751.611171	34.437850
980.527592	112956.000363	34.442868
981.665188	113201.037368	34.447885
983.053931	113398.887135	34.452903
984.003372	113630.658329	34.457920
985.166411	113859.470009	34.462938
986.409188	114057.247294	34.467956
987.962305	114268.275918	34.472973
988.591361	114472.263380	34.477991
990.020382	114657.675743	34.483008
991.264550	114883.543589	34.488026
992.132096	115079.185926	34.493044
993.490788	115268.376441	34.498061
994.008748	115493.495058	34.503079
995.482780	115682.846718	34.508096
996.685392	115880.377660	34.513114
997.408892	116080.155437	34.518132
998.058537	116281.391069	34.523149
999.105012	116500.476295	34.528167
1000.044623	116688.478786	34.533184
1000.801450	116904.637816	34.538202
1002.130233	117087.650509	34.543220
1003.156715	117287.779636	34.548237
1003.982032	117524.354798	34.553255
1005.364912	117704.081244	34.558272
1006.431472	117913.900248	34.563290
1007.256464	118107.873125	34.568308
1008.208359	118317.346644	34.573325
1009.004249	118530.661049	34.578343
1010.026721	118717.865226	34.583360
1011.083946	118933.306048	34.588378
1011.917310	119160.327812	34.593396
1012.863250	119350.336188	34.598413
1013.990591	119582.140075	34.603431
1014.832863	119784.471194	34.608448
1016.087009	119977.359691	34.613466
1017.191198	120191.535232	34.618484
1018.199142	120385.531442	34.623501
1019.248147	120575.442249	34.628519
1020.239600	120759.256540	34.633536
1021.052438	120975.779424	34.638554
1021.828499	121165.143656	34.643572
1022.687994	121379.533162	34.648589
1023.552725	121590.084064	34.653607
1024.497970	121774.292578	34.658624
1025.602198	121980.333867	34.663642
1026.064747	122209.607709	34.668660
1026.901434	122413.301356	34.673677
1027.798585	122659.030510	34.678695
1028.997389	122882.714000	34.683712
1029.883534	123104.334645	34.688730
1030.476219	123350.031170	34.693748
1031.854662	123567.734484	34.698765
1032.864259	123813.746218	34.703783
1033.785381	124057.050108	34.708800
1035.097409	124278.343184	34.713818
1035.907748	124531.984464	34.718836
1037.136957	124770.478575	34.723853
1037.837274	125009.809600	34.728871
1038.988585	125266.378916	34.733888
1040.309352	125503.368428	34.738906
1041.182668	125743.741307	34.743924
1042.288892	125984.723989	34.748941
1043.110810	126230.191116	34.753959
1044.103246	126486.860516	34.758976
1045.313173	126745.701352	34.763994
1046.221019	126993.137559	34.769012
1047.533531	127251.078669	34.774029
1048.718625	127501.007968	34.779047
1049.741023	127721.322454	34.784064
1050.904406	127991.347164	34.789082
1051.834233	128240.576951	34.794100
1053.301602	128493.205385	34.799117
1054.107118	128741.179718	34.804135
1055.088153	129006.908998	34.809152
1056.419786	129243.545855	34.814170
1057.396283	129498.215480	34.819188
1058.477533	129753.985280	34.824205
1059.562395	130015.041927	34.829223
1060.916950	130267.209301	34.834240
1061.906614	130507.271138	34.839258
1062.718655	130776.795348	34.844276
1063.969576	131003.205019	34.849293
1064.807256	131271.588539	34.854311
1065.939407	131533.321955	34.859328
1067.683662	131758.375479	34.864346
1068.405997	132024.743791	34.869364
1069.480467	132284.667759	34.874381
1070.649534	132542.169889	34.879399
1071.483614	132795.305592	34.884416
1072.779812	133047.860005	34.889434
1073.895655	133281.559043	34.894452
1074.939805	133528.467408	34.899469
1075.671390	133804.140781	34.904487
1076.774868	134046.746167	34.909504
1078.105329	134305.364198	34.914522
1079.231777	134557.223424	34.919540
1080.576607	134803.166663	34.924557
1081.549129	135044.964607	34.929575
1082.717837	135306.457009	34.934592
1083.982587	135573.057135	34.939610
1084.619282	135812.140059	34.944628
1085.908123	136061.994002	34.949645
1087.161226	136312.603729	34.954663
1088.188570	136565.965595	34.959680
1089.357231	136784.709649	34.964698
1090.308905	137025.549711	34.969716
1091.097343	137268.713131	34.974733
1092.771504	137494.008844	34.979751
1093.882350	137724.698381	34.984768
1094.889134	137943.121948	34.989786
1096.368054	138180.219598	34.994804
1097.415333	138419.203163	34.999821
1098.511705	138640.038062	35.004839
1099.400032	138860.338267	35.009856
1100.503857	139120.756309	35.014874
1101.412762	139362.672856	35.019892
1102.647241	139584.366061	35.024909
1103.291553	139851.914891	35.029927
1104.003371	140087.048199	35.034944
1105.143443	140333.269715	35.039962
1106.054176	140612.330945	35.044980
1106.774245	140849.585605	35.049997
1108.618226	141123.615649	35.055015
1109.136498	141361.604575	35.060032
1110.977354	141631.835542	35.065050
1112.026339	141914.206676	35.070068
1113.002119	142146.762257	35.075085
1114.232439	142418.228744	35.080103
1115.153019	142684.473822	35.085120
1116.531505	142924.791537	35.090138
1117.441384	143207.754261	35.095156
1118.687977	143472.835835	35.100173
1119.750403	143746.407395	35.105191
1120.528941	144011.342143	35.110208
1121.669278	144265.796105	35.115226
1122.344969	144567.055404	35.120244
1123.713041	144828.957268	35.125261
1124.870116	145089.298198	35.130279
1126.142586	145379.129687	35.135296
1127.500084	145638.579352	35.140314
1128.590482	145944.321769	35.145332
1129.920030	146214.470200	35.150349
1130.645764	146515.864843	35.155367
1132.046840	146782.277613	35.160384
1132.773070	147061.763946	35.165402
1134.057514	147366.459478	35.170420
1135.550310	147630.656940	35.175437
1137.108820	147902.010545	35.180455
1138.303968	148173.832005	35.185472
1139.626586	148437.695766	35.190490
1140.655359	148717.665077	35.195508
1141.801278	148980.686953	35.200525
1142.956510	149272.535279	35.205543
1144.097074	149548.675318	35.210560
1145.257811	149804.776345	35.215578
1146.067392	150084.209042	35.220596
1147.180908	150359.091481	35.225613
1148.467166	150634.530867	35.230631
1149.456795	150928.905573	35.235648
1151.029001	151184.479101	35.240666
1152.031370	151485.895020	35.245684
1153.474881	151753.732572	35.250701
1154.563927	152013.069617	35.255719
1155.646469	152303.457524	35.260736
1156.925664	152561.397249	35.265754
1158.023783	152827.409785	35.270772
1159.411946	153121.190759	35.275789
1160.356530	153377.948396	35.280807
1161.067975	153663.639191	35.285824
1162.540024	153937.486993	35.290842
1163.545330	154232.823830	35.295860
1164.908129	154501.011475	35.300877
1166.428292	154740.775949	35.305895
1167.354260	155000.300076	35.310912
1168.635973	155275.533458	35.315930
1169.933501	155534.365683	35.320948
1170.892370	155782.994067	35.325965
1172.117967	156058.965339	35.330983
1173.172209	156308.114115	35.336000
1174.316612	156551.947528	35.341018
1175.299662	156830.108021	35.346036
1175.938424	157108.416132	35.351053
1177.258160	157381.210146	35.356071
1178.346081	157673.680382	35.361088
1179.491435	157935.078061	35.366106
1180.214681	158238.927623	35.371124
1181.369849	158506.023036	35.376141
1182.395165	158809.383161	35.381159
1183.729860	159091.066199	35.386176
1185.162051	159377.200383	35.391194
1185.863189	159694.054560	35.396212
1186.970848	159987.705739	35.401229
1188.434672	160292.894943	35.406247
1189.580592	160595.297343	35.411264
1190.856306	160893.824104	35.416282
1191.822843	161205.863860	35.421300
1192.929872	161497.737449	35.426317
1194.317346	161812.528685	35.431335
1195.503613	162121.050526	35.436352
1197.365533	162410.357615	35.441370
1198.478564	162727.636973	35.446388
1199.925772	163031.783856	35.451405
1201.390977	163329.954637	35.456423
1202.454999	163619.211633	35.461440
1203.833097	163914.165901	35.466458
1204.995868	164239.555482	35.471476
1206.047249	164532.119491	35.476493
1207.340138	164838.411106	35.481511
1208.442307	165147.235799	35.486528
1209.252352	165430.596990	35.491546
1211.119082	165748.929477	35.496564
1212.535337	166037.333025	35.501581
1213.809608	166341.025001	35.506599
1214.846947	166663.320168	35.511616
1216.543520	166926.701630	35.516634
1217.451400	167250.773477	35.521652
1218.548257	167533.822162	35.526669
1220.253477	167820.210709	35.531687
1221.584039	168124.692644	35.536704
1222.850390	168412.020321	35.541722
1223.985580	168702.315198	35.546740
1225.501871	169007.356294	35.551757
1226.577013	169287.527039	35.556775
1227.983260	169592.298527	35.561792
1229.312909	169896.031614	35.566810
1230.446670	170170.754912	35.571828
1231.509781	170448.181567	35.576845
1232.937911	170751.422074	35.581863
1233.882036	171029.265330	35.586880
1235.088467	171339.081160	35.591898
1236.222404	171650.941329	35.596916
1237.565592	171939.662263	35.601933
1239.126295	172233.513629	35.606951
1239.977121	172524.984280	35.611968
1241.200796	172801.853271	35.616986
1242.406646	173123.888517	35.622004
1243.189195	173409.259763	35.627021
1244.457879	173722.342727	35.632039
1245.522734	174040.892634	35.637056
1246.480131	174325.339703	35.642074
1247.751612	174646.917885	35.647092
1248.871528	174933.384900	35.652109
1249.902919	175222.330135	35.657127
1251.160005	175530.122725	35.662144
1252.458406	175825.271102	35.667162
1253.698865	176148.095606	35.672180
1254.762583	176455.558105	35.677197
1256.353233	176754.433037	35.682215
1257.174245	177071.102025	35.687232
1258.087933	177394.610710	35.692250
1259.656121	177719.790226	35.697268
1260.659269	178037.768009	35.702285
1261.951298	178369.368209	35.707303
1263.312890	178688.725138	35.712320
1264.689830	179013.272231	35.717338
1265.925139	179319.747366	35.722356
1266.953438	179652.364277	35.727373
1268.339984	179998.706980	35.732391
1269.415248	180333.262455	35.737408
1270.649394	180667.502039	35.742426
1271.939103	181014.971914	35.747444
1272.953396	181339.175191	35.752461
1275.448784	181636.293217	35.757479
1277.252995	181980.118439	35.762496
1278.611017	182306.644508	35.767514
1279.841930	182643.664461	35.772532
1280.790150	182981.748637	35.777549
1281.997188	183285.676016	35.782567
1283.062820	183628.733016	35.787584
1284.169079	183959.715254	35.792602
1285.472987	184296.391193	35.797620
1286.579681	184642.646519	35.802637
1288.124101	184971.493943	35.807655
1288.971230	185336.365739	35.812672
1290.269108	185668.037833	35.817690
1291.699188	186025.481772	35.822708
1292.568274	186391.575631	35.827725
1294.145212	186733.095932	35.832743
1295.006861	187078.925119	35.837760
1296.605738	187443.382459	35.842778
1297.636888	187820.806769	35.847796
1298.897113	188186.771950	35.852813
1300.241938	188541.987045	35.857831
1301.522925	188911.228447	35.862848
1302.541121	189281.759620	35.867866
1303.756594	189655.129418	35.872884
1305.038625	190020.836430	35.877901
1307.009310	190381.837009	35.882919
1308.006396	190765.468595	35.887936
1309.963578	191107.879559	35.892954
1311.374686	191476.405304	35.897972
1312.690593	191828.243744	35.902989
1314.624936	192176.605603	35.908007
1315.912755	192554.184029	35.913024
1317.469216	192908.591566	35.918042
1318.675328	193256.039075	35.923060
1320.085615	193612.696454	35.928077
1321.879739	193964.913008	35.933095
1323.063660	194309.577511	35.938112
1324.306890	194656.366891	35.943130
1326.168536	195012.869201	35.948148
1327.123591	195347.561235	35.953165
1328.832804	195694.266908	35.958183
1329.826948	196032.498081	35.963200
1331.121841	196394.928911	35.968218
1332.684696	196729.794705	35.973236
1333.679170	197064.197509	35.978253
1335.075485	197411.662610	35.983271
1336.188315	197741.161809	35.988288
1336.924900	198074.101770	35.993306
1338.315175	198406.834012	35.998324
1339.238093	198764.655189	36.003341
1340.777385	199088.695345	36.008359
1341.825291	199443.135318	36.013376
1343.196306	199790.909439	36.018394
1344.637609	200133.024193	36.023412
1345.696804	200500.214523	36.028429
1347.033781	200838.325560	36.033447
1348.311448	201185.424125	36.038464
1349.771350	201553.188896	36.043482
1351.054055	201913.341871	36.048500
1352.071419	202290.731123	36.053517
1353.837089	202658.260954	36.058535
1355.199097	203010.712702	36.063552
1356.942479	203380.179883	36.068570
1358.341520	203731.359533	36.073588
1359.156694	204106.278138	36.078605
1360.529433	204455.650142	36.083623
1361.900327	204830.214231	36.088640
1362.880796	205221.058366	36.093658
1364.239737	205604.211415	36.098676
1365.555433	205998.153215	36.103693
1366.930334	206361.627558	36.108711
1368.606970	206758.015155	36.113728
1370.162257	207139.721763	36.118746
1371.391512	207525.686862	36.123764
1372.844856	207911.007497	36.128781
1374.713067	208299.550200	36.133799
1376.220255	208664.651828	36.138816
1377.510120	209049.827437	36.143834
1378.908012	209434.860162	36.148852
1379.924095	209813.253547	36.153869
1381.747583	210208.758730	36.158887
1382.525355	210599.130882	36.163904
1384.413704	210992.077051	36.168922
1385.948998	211379.648793	36.173940
1387.167535	211773.928295	36.178957
1388.754133	212151.514813	36.183975
1389.661365	212535.970455	36.188992
1391.104022	212933.494585	36.194010
1392.442469	213337.501087	36.199028
1394.103334	213727.818601	36.204045
1395.500353	214123.768625	36.209063
1396.463286	214521.265108	36.214080
1398.071295	214928.460002	36.219098
1399.606009	215315.224641	36.224116
1400.980474	215716.950691	36.229133
1402.216032	216130.866564	36.234151
1403.573697	216591.519977	36.239168
1404.811478	217011.230045	36.244186
1406.498390	217407.324738	36.249204
1407.735887	217819.470200	36.254221
1409.342945	218226.350037	36.259239
1410.827098	218628.883552	36.264256
1412.230693	219029.654243	36.269274
1413.508052	219435.577791	36.274292
1414.603132	219856.340067	36.279309
1416.444779	220242.211177	36.284327
1417.553770	220683.166077	36.289344
1418.809100	221068.781605	36.294362
1420.427323	221498.734870	36.299380
1421.596365	221898.590838	36.304397
1423.294986	222333.131464	36.309415
1424.770158	222743.810741	36.314432
1426.079986	223156.957190	36.319450
1427.933665	223551.322018	36.324468
1429.283886	223969.265328	36.329485
1430.471469	224343.042925	36.334503
1431.826836	224753.673515	36.339520
1433.317417	225157.831941	36.344538
1434.907037	225539.039994	36.349556
1435.817063	225947.970536	36.354573
1437.564697	226348.560313	36.359591
1438.917296	226747.260915	36.364608
1440.326789	227165.765162	36.369626
1441.641961	227568.767265	36.374644
1442.990180	227972.120874	36.379661
1444.462281	228385.183524	36.384679
1446.103060	228793.825549	36.389696
1447.282455	229209.149065	36.394714
1448.369780	229635.690591	36.399732
1449.816844	230054.223931	36.404749
1451.285742	230481.543519	36.409767
1452.865910	230913.418207	36.414784
1454.421524	231334.731784	36.419802
1455.851150	231753.019417	36.424820
1457.251710	232190.007961	36.429837
1459.222523	232620.756827	36.434855
1461.170130	233035.457585	36.439872
1462.482701	233468.171920	36.444890
1463.858545	233896.127149	36.449908
1465.051889	234311.514870	36.454925
1466.548323	234749.917873	36.459943
1467.842435	235170.930380	36.464960
1469.576212	235612.370237	36.469978
1471.691798	236043.613242	36.474996
1472.770867	236468.601935	36.480013
1474.142161	236918.335272	36.485031
1475.874294	237338.392209	36.490048
1476.945681	237793.410114	36.495066
1478.294721	238240.991559	36.500084
1479.694378	238681.935978	36.505101
1481.375624	239126.340467	36.510119
1482.719006	239571.792476	36.515136
1484.003357	240035.951056	36.520154
1485.445292	240474.987710	36.525172
1487.086906	240946.989556	36.530189
1488.562531	241377.309829	36.535207
1489.917450	241833.383239	36.540224
1491.335421	242291.403225	36.545242
1493.025336	242740.031339	36.550260
1494.676822	243211.376329	36.555277
1496.366128	243668.592420	36.560295
1497.562813	244128.888205	36.565312
1499.213416	244588.271727	36.570330
1500.841571	245050.174684	36.575348
1502.364740	245502.747729	36.580365
1503.743518	245960.654547	36.585383
1505.602954	246433.216356	36.590400
1506.877060	246881.616096	36.595418
1508.381836	247334.220751	36.600436
1509.416379	247825.846063	36.605453
1511.228915	248268.545162	36.610471
1512.902977	248738.651953	36.615488
1514.783506	249188.580952	36.620506
1516.430352	249646.068381	36.625524
1517.758488	250096.496219	36.630541
1519.386068	250560.110145	36.635559
1521.109404	251026.172949	36.640576
1522.583713	251465.959937	36.645594
1523.702620	251933.825573	36.650612
1525.022751	252393.885208	36.655629
1526.669110	252858.946708	36.660647
1528.299858	253322.639493	36.665664
1529.618532	253772.514125	36.670682
1531.182359	254214.397523	36.675700
1532.700100	254662.233227	36.680717
1534.631516	255106.393773	36.685735
1536.023968	255545.207296	36.690752
1537.196423	255999.375547	36.695770
1538.621860	256438.971708	36.700788
1540.213504	256890.835862	36.705805
1541.093909	257347.695047	36.710823
1542.709030	257814.873966	36.715840
1544.263908	258274.823108	36.720858
1545.661847	258738.989871	36.725876
1547.713714	259212.778354	36.730893
1549.244161	259662.494485	36.735911
1550.918169	260138.784290	36.740928
1551.786162	260616.909208	36.745946
1553.854838	261079.873526	36.750964
1555.301750	261579.063982	36.755981
1556.621503	262057.063673	36.760999
1558.474695	262528.548295	36.766016
1559.748360	263013.236608	36.771034
1561.635975	263489.389653	36.776052
1563.142043	263988.747964	36.781069
1564.688817	264474.305442	36.786087
1566.100508	264935.421699	36.791104
1567.506931	265441.934305	36.796122
1568.971338	265946.760501	36.801140
1570.847930	266437.927695	36.806157
1572.415055	266951.043261	36.811175
1574.161404	267428.691446	36.816192
1575.607106	267959.202163	36.821210
1577.241066	268432.270228	36.826228
1578.831010	268940.020496	36.831245
1580.385723	269440.917284	36.836263
1582.412151	269934.597498	36.841280
1583.752737	270444.775380	36.846298
1585.540382	270926.325919	36.851316
1587.374269	271450.215149	36.856333
1589.004004	271965.678223	36.861351
1590.929590	272453.072362	36.866368
1592.784651	272953.001161	36.871386
1594.355630	273439.792054	36.876404
1596.133895	273932.416130	36.881421
1597.892911	274429.335740	36.886439
1599.518330	274908.672508	36.891456
1601.080398	275395.995452	36.896474
1602.773521	275891.221625	36.901492
1604.227942	276370.304850	36.906509
1605.421213	276885.349632	36.911527
1607.294143	277374.954947	36.916544
1608.541891	277878.583077	36.921562
1610.165187	278385.145736	36.926580
1611.762551	278878.781811	36.931597
1613.361088	279388.979008	36.936615
1614.989445	279891.447870	36.941632
1616.498894	280384.688819	36.946650
1618.553011	280873.698242	36.951668
1620.052508	281378.801395	36.956685
1621.283498	281912.550345	36.961703
1622.828743	282414.747578	36.966720
1624.713164	282914.321984	36.971738
1625.954592	283416.795397	36.976756
1627.929556	283943.786183	36.981773
1628.956915	284439.205069	36.986791
1630.847272	284977.434393	36.991808
1632.243279	285484.372704	36.996826
1633.693594	286005.957228	37.001844
1635.264434	286527.418651	37.006861
1636.227234	287030.893003	37.011879
1638.234982	287554.311176	37.016896
1640.005084	288058.639754	37.021914
1641.539229	288559.576483	37.026932
1643.453040	289060.982350	37.031949
1644.644338	289591.030976	37.036967
1646.364898	290097.469209	37.041984
1647.355637	290642.609792	37.047002
1649.321898	291159.341825	37.052020
1650.966826	291685.446955	37.057037
1652.076140	292235.184639	37.062055
1653.598082	292750.815548	37.067072
1654.767577	293305.745954	37.072090
1656.555476	293861.968964	37.077108
1658.420599	294395.951800	37.082125
1659.891483	294973.253434	37.087143
1661.483456	295526.859794	37.092160
1663.378115	296098.091851	37.097178
1665.038924	296659.860325	37.102196
1666.669692	297236.870714	37.107213
1668.165247	297821.215519	37.112231
1669.984471	298363.646107	37.117248
1671.580458	298970.903815	37.122266
1673.204907	299530.784555	37.127284
1674.899424	300124.405785	37.132301
1676.752519	300701.488453	37.137319
1678.477908	301267.439092	37.142336
1680.252399	301880.721022	37.147354
1681.940143	302452.538357	37.152372
1683.754075	303039.722829	37.157389
1685.455757	303644.599263	37.162407
1687.753441	304215.493063	37.167424
1689.127110	304829.610202	37.172442
1690.974765	305392.977351	37.177460
1692.830018	305991.286480	37.182477
1694.414602	306573.560040	37.187495
1696.482616	307143.051667	37.192512
1698.187854	307747.393107	37.197530
1699.628784	308346.694730	37.202548
1701.833552	308918.717480	37.207565
1703.540701	309524.976500	37.212583
1705.380575	310091.464493	37.217600
1707.275736	310676.300803	37.222618
1708.859332	311264.739825	37.227636
1710.495128	311849.051967	37.232653
1712.185085	312434.011271	37.237671
1714.370282	313020.433735	37.242688
1715.703199	313612.503206	37.247706
1717.396960	314199.302769	37.252724
1719.204877	314786.307635	37.257741
1720.796788	315376.137052	37.262759
1722.611568	315968.362982	37.267776
1724.103726	316561.983369	37.272794
1725.806430	317163.537949	37.277812
1727.358391	317764.198325	37.282829
1728.903204	318374.504419	37.287847
1730.790918	318971.061873	37.292864
1732.147227	319555.411829	37.297882
1733.438176	320181.843498	37.302900
1735.546690	320778.400061	37.307917
1737.324363	321398.900205	37.312935
1739.500220	321998.304422	37.317952
1741.215447	322609.815061	37.322970
1742.918646	323225.511730	37.327988
1744.530603	323818.238569	37.333005
1745.859499	324447.163739	37.338023
1747.825496	325072.524578	37.343040
1749.650559	325676.447523	37.348058
1751.094630	326291.320096	37.353076
1753.018126	326859.389723	37.358093
1754.163488	327458.913749	37.363111
1756.014435	328077.078562	37.368128
1757.510195	328674.501837	37.373146
1759.212038	329295.878032	37.378164
1761.280465	329900.126026	37.383181
1762.563149	330525.468574	37.388199
1764.669874	331131.576541	37.393216
1766.182073	331752.501455	37.398234
1767.905401	332379.503402	37.403252
1770.097840	332990.350836	37.408269
1771.185001	333640.140489	37.413287
1773.327114	334251.922054	37.418304
1775.138299	334888.757490	37.423322
1776.813966	335523.957904	37.428340
1778.540204	336156.527917	37.433357
1779.897929	336809.155474	37.438375
1781.912812	337456.005824	37.443392
1783.855680	338117.837578	37.448410
1785.495474	338769.709486	37.453428
1787.948813	339399.379958	37.458445
1789.386998	340072.998253	37.463463
1790.927107	340723.745475	37.468480
1792.451599	341382.838302	37.473498
1794.068123	342067.874593	37.478516
1795.970279	342718.384476	37.483533
1797.659581	343412.376143	37.488551
1799.812603	344070.924174	37.493568
1801.377456	344752.175794	37.498586
1803.446330	345437.878138	37.503604
1805.422651	346130.185227	37.508621
1807.087005	346801.163192	37.513639
1808.864753	347460.945648	37.518656
1811.075280	348143.337430	37.523674
1812.670181	348842.368523	37.528692
1814.766676	349534.174838	37.533709
1816.116020	350209.851539	37.538727
1818.200784	350914.024142	37.543744
1820.155721	351604.706099	37.548762
1821.888600	352280.263597	37.553780
1823.977371	352960.218702	37.558797
1825.690362	353685.295172	37.563815
1827.611797	354377.640263	37.568832
1829.285868	355070.497427	37.573850
1831.102422	355748.627476	37.578868
1833.034505	356463.395435	37.583885
1835.087830	357156.182118	37.588903
1837.334320	357850.803435	37.593920
1839.656154	358515.510110	37.598938
1841.826507	359211.948579	37.603956
1844.063720	359888.141827	37.608973
1845.388197	360560.820924	37.613991
1846.915840	361257.026671	37.619008
1848.856626	361948.128762	37.624026
1850.480019	362619.912857	37.629044
1852.446308	363323.343338	37.634061
1854.018646	364008.457994	37.639079
1856.213365	364695.589330	37.644096
1858.009491	365401.700483	37.649114
1859.544157	366079.884900	37.654132
1861.582686	366782.303367	37.659149
1863.783245	367472.074203	37.664167
1865.452986	368169.251655	37.669184
1867.270951	368830.192273	37.674202
1869.110984	369534.724077	37.679220
1871.342781	370208.484343	37.684237
1872.854996	370907.692175	37.689255
1874.998492	371573.781826	37.694272
1876.905737	372220.392494	37.699290
1878.386481	372926.238598	37.704308
1880.228589	373567.382870	37.709325
1881.871632	374237.565140	37.714343
1883.643383	374900.535900	37.719360
1885.814009	375573.168083	37.724378
1887.439845	376267.080612	37.729396
1889.059203	376933.513531	37.734413
1891.143073	377625.751484	37.739431
1892.914999	378308.136430	37.744448
1895.237076	378994.069235	37.749466
1896.629937	379692.416062	37.754484
1898.682410	380371.341319	37.759501
1900.405032	381061.313407	37.764519
1902.226417	381784.956794	37.769536
1904.422547	382474.391038	37.774554
1906.001880	383194.646225	37.779572
1907.993483	383912.738672	37.784589
1909.409835	384616.051683	37.789607
1911.330965	385356.945317	37.794624
1913.241384	386072.063088	37.799642
1914.777260	386784.767616	37.804660
1917.000241	387535.425173	37.809677
1918.513069	388282.886492	37.814695
1920.228385	389032.959113	37.819712
1922.677292	389796.203140	37.824730
1924.152735	390540.829101	37.829748
1926.730580	391285.281039	37.834765
1928.447805	392037.361056	37.839783
1930.328711	392791.525367	37.844800
1932.432489	393553.340801	37.849818
1934.000618	394316.366480	37.854836
1936.046724	395067.634244	37.859853
1938.491931	395858.815940	37.864871
1940.285441	396614.218811	37.869888
1942.298443	397366.727797	37.874906
1944.081321	398145.184313	37.879924
1946.493316	398895.105179	37.884941
1948.509326	399656.401255	37.889959
1950.716876	400440.125806	37.894976
1953.083041	401197.852161	37.899994
1954.842276	401953.580872	37.905012
1956.951377	402732.419698	37.910029
1958.825046	403488.798988	37.915047
1960.534878	404261.555120	37.920064
1962.674924	405020.966809	37.925082
1965.054358	405763.214978	37.930100
1967.519682	406528.335160	37.935117
1969.999874	407278.381582	37.940135
1971.750037	408041.906090	37.945152
1974.264731	408786.914854	37.950170
1976.192161	409532.633781	37.955188
1978.025571	410282.502888	37.960205
1979.979890	411020.044498	37.965223
1981.828062	411748.362292	37.970240
1983.701112	412510.146177	37.975258
1985.468431	413264.529046	37.980276
1987.447244	414015.892057	37.985293
1989.412617	414767.134804	37.990311
1990.940051	415515.642246	37.995328
1993.076307	416281.809070	38.000346
1995.062646	417036.403243	38.005364
1997.168605	417791.259847	38.010381
1998.893997	418563.328926	38.015399
2000.595047	419309.951604	38.020416
2002.738221	420078.968655	38.025434
2004.458489	420859.453782	38.030452
2006.512857	421600.987868	38.035469
2008.614505	422332.261970	38.040487
2010.489020	423083.075922	38.045504
2012.536390	423832.826096	38.050522
2014.087037	424568.506712	38.055540
2016.119859	425336.521130	38.060557
2017.920493	426095.080649	38.065575
2019.945820	426862.365333	38.070592
2022.176779	427624.984320	38.075610
2023.788956	428385.858764	38.080628
2025.854264	429169.621743	38.085645
2027.874616	429944.810214	38.090663
2029.353342	430734.340465	38.095680
2031.689461	431508.211392	38.100698
2033.434174	432326.806587	38.105716
2034.903245	433105.983066	38.110733
2036.997001	433922.238190	38.115751
2038.852100	434740.124237	38.120768
2041.160471	435530.167962	38.125786
2042.485005	436377.898619	38.130804
2044.782500	437198.409438	38.135821
2046.742341	438045.923653	38.140839
2048.361256	438878.481896	38.145856
2050.940952	439736.409187	38.150874
2052.461353	440601.614511	38.155892
2054.881624	441442.297089	38.160909
2057.231313	442304.112322	38.165927
2059.393323	443152.111119	38.170944
2061.500350	444019.871323	38.175962
2063.353707	444875.951375	38.180980
2065.627072	445745.336940	38.185997
2067.942053	446608.559441	38.191015
2069.942910	447478.073124	38.196032
2072.462531	448340.131046	38.201050
2074.455394	449215.900305	38.206068
2076.267394	450072.238934	38.211085
2078.890380	450947.328038	38.216103
2081.100870	451801.103889	38.221120
2083.241278	452662.393442	38.226138
2085.119734	453551.862918	38.231156
2087.368903	454419.385168	38.236173
2089.776655	455282.192674	38.241191
2091.749969	456166.883002	38.246208
2093.803172	457020.119113	38.251226
2096.047573	457896.245990	38.256244
2098.095250	458778.233607	38.261261
2100.423524	459655.535847	38.266279
2102.487814	460523.692495	38.271296
2104.624802	461390.030560	38.276314
2106.444624	462273.522418	38.281332
2108.883331	463152.424750	38.286349
2110.919508	464023.115036	38.291367
2112.732078	464902.650428	38.296384
2115.375287	465785.194435	38.301402
2117.344373	466685.602121	38.306420
2119.708346	467548.956836	38.311437
2122.050716	468432.998753	38.316455
2123.844103	469309.005099	38.321472
2125.908317	470191.395953	38.326490
2127.752754	471070.902451	38.331508
2129.966616	471937.270850	38.336525
2132.113587	472830.593712	38.341543
2133.983283	473743.777537	38.346560
2136.003930	474627.285502	38.351578
2138.215813	475508.598848	38.356596
2140.434073	476406.642478	38.361613
2142.622086	477300.101662	38.366631
2144.622131	478209.966458	38.371648
2146.650818	479070.027593	38.376666
2148.644406	479918.386872	38.381684
2150.818646	480791.274642	38.386701
2153.305692	481679.726047	38.391719
2155.657906	482524.825282	38.396736
2158.071026	483379.722954	38.401754
2160.326111	484252.583810	38.406772
2162.529774	485099.708830	38.411789
2164.741940	485957.194296	38.416807
2166.498603	486833.092626	38.421824
2168.847426	487689.210504	38.426842
2170.818731	488580.790626	38.431860
2172.552915	489461.006359	38.436877
2175.596614	490341.820538	38.441895
2177.124629	491211.483001	38.446912
2179.177139	492110.948025	38.451930
2181.507282	493021.677441	38.456948
2183.057747	493919.415940	38.461965
2185.298070	494795.494897	38.466983
2187.117489	495716.563410	38.472000
2189.243215	496644.647327	38.477018
2191.557399	497580.269325	38.482036
2193.611238	498497.667977	38.487053
2195.934634	499431.824394	38.492071
2197.842200	500353.637215	38.497088
2200.292272	501286.661145	38.502106
2202.813340	502233.544585	38.507124
2204.752660	503179.814579	38.512141
2207.227431	504112.878528	38.517159
2209.065420	505051.038730	38.522176
2211.477104	506030.054221	38.527194
2213.666859	506972.182732	38.532212
2216.032752	507915.438328	38.537229
2218.593583	508883.870479	38.542247
2220.542152	509852.093789	38.547264
2222.592047	510799.772179	38.552282
2225.078469	511757.204558	38.557300
2226.886935	512733.596732	38.562317
2229.363381	513709.920009	38.567335
2231.253238	514698.377944	38.572352
2233.901522	515649.400573	38.577370
2236.470434	516633.492636	38.582388
2238.598647	517605.500348	38.587405
2241.046688	518587.978005	38.592423
2243.378286	519573.688530	38.597440
2245.136873	520543.357174	38.602458
2247.146982	521554.743466	38.607476
2249.205549	522537.539332	38.612493
2251.799147	523533.635291	38.617511
2253.618252	524533.622700	38.622528
2255.663229	525548.669326	38.627546
2258.175468	526530.126249	38.632564
2260.251152	527550.826212	38.637581
2263.036767	528569.325532	38.642599
2265.048997	529574.437532	38.647616
2267.113904	530583.048528	38.652634
2269.383305	531610.540147	38.657652
2271.494525	532619.911670	38.662669
2273.725426	533647.671092	38.667687
2275.939683	534666.602130	38.672704
2278.257852	535698.885435	38.677722
2280.354173	536740.142194	38.682740
2282.435792	537774.230257	38.687757
2284.757377	538796.529112	38.692775
2287.128282	539850.803459	38.697792
2289.521750	540879.937583	38.702810
2291.808006	541921.544157	38.707828
2293.511066	542968.956785	38.712845
2295.937293	543975.020456	38.717863
2298.346137	544989.064348	38.722880
2300.812966	546013.639419	38.727898
2303.428612	547014.777024	38.732916
2305.934840	548008.115751	38.737933
2308.085966	549039.411800	38.742951
2310.927201	550040.194500	38.747968
2313.579017	551039.176178	38.752986
2316.099942	552031.269055	38.758004
2318.472593	553023.716996	38.763021
2321.094773	554008.259659	38.768039
2323.234075	555027.094267	38.773056
2325.483380	556023.416219	38.778074
2327.981806	557035.104353	38.783092
2330.116344	558051.651670	38.788109
2331.849100	559037.131595	38.793127
2334.308192	560053.071907	38.798144
2336.025621	561098.350756	38.803162
2338.207767	562141.260267	38.808180
2340.303291	563175.008942	38.813197
2342.625078	564233.153771	38.818215
2344.726344	565272.564287	38.823232
2347.123951	566328.870287	38.828250
2349.475041	567408.502081	38.833268
2351.915871	568488.029575	38.838285
2354.514061	569534.400661	38.843303
2356.695347	570627.852427	38.848320
2358.773436	571718.718118	38.853338
2361.520121	572786.940971	38.858356
2363.393089	573878.710743	38.863373
2365.881608	574995.632657	38.868391
2368.345543	576091.080217	38.873408
2370.797652	577173.387041	38.878426
2373.499175	578278.190662	38.883444
2375.520623	579380.701100	38.888461
2377.908085	580483.455361	38.893479
2380.481338	581619.943429	38.898496
2382.792435	582713.984263	38.903514
2385.241952	583805.949369	38.908532
2387.611344	584944.322298	38.913549
2390.018490	586074.108473	38.918567
2392.456156	587205.139125	38.923584
2395.027662	588317.591757	38.928602
2397.478236	589442.495884	38.933620
2399.476266	590585.216018	38.938637
2401.626315	591717.076134	38.943655
2403.956066	592848.248638	38.948672
2406.157308	593997.827808	38.953690
2408.784005	595145.422026	38.958708
2410.824887	596294.905939	38.963725
2413.295811	597466.051045	38.968743
2415.742603	598649.407227	38.973760
2417.875028	599798.434300	38.978778
2420.628275	600967.831298	38.983796
2422.569135	602136.994541	38.988813
2425.326286	603297.092323	38.993831
2427.987300	604492.088718	38.998848
2430.370302	605669.985042	39.003866
2432.903724	606836.272116	39.008884
2434.964225	608001.567302	39.013901
2437.558119	609190.979628	39.018919
2440.224577	610381.406535	39.023936
2442.150751	611566.576237	39.028954
2444.826373	612768.859622	39.033972
2447.138299	613948.661654	39.038989
2449.601167	615130.815697	39.044007
2452.097266	616340.398850	39.049024
2454.546814	617532.703880	39.054042
2457.088257	618682.009408	39.059060
2459.003762	619857.599482	39.064077
2461.717387	620987.535498	39.069095
2464.111873	622167.599053	39.074112
2466.288532	623322.778047	39.079130
2468.902857	624502.252861	39.084148
2471.027201	625673.384363	39.089165
2473.416757	626866.731744	39.094183
2475.664668	628042.782649	39.099200
2478.200571	629232.296000	39.104218
2480.754060	630414.031391	39.109236
2482.984752	631630.002963	39.114253
2485.301973	632845.271768	39.119271
2488.057375	634051.290446	39.124288
2490.335493	635267.685364	39.129306
2492.993069	636489.668239	39.134324
2495.298288	637717.457054	39.139341
2497.782323	638933.292599	39.144359
2500.577075	640175.684888	39.149376
2502.974268	641408.313044	39.154394
2505.732918	642637.591152	39.159412
2508.255642	643893.451869	39.164429
2511.114974	645122.266416	39.169447
2513.414863	646367.784023	39.174464
2515.542203	647626.243857	39.179482
2518.257043	648884.151625	39.184500
2520.609528	650139.120737	39.189517
2523.257304	651400.365641	39.194535
2525.716181	652691.390601	39.199552
2528.308275	653969.817097	39.204570
2531.194960	655232.134456	39.209588
2533.428057	656529.626388	39.214605
2535.934058	657804.185470	39.219623
2538.600742	659081.392751	39.224640
2541.199883	660374.383408	39.229658
2543.842639	661670.383410	39.234676
2546.416174	662959.600184	39.239693
2548.666882	664252.931179	39.244711
2551.478345	665544.653093	39.249728
2554.216474	666847.164522	39.254746
2557.187621	668127.812628	39.259764
2559.964527	669427.180874	39.264781
2562.479192	670718.853142	39.269799
2565.262557	671998.267212	39.274816
2567.746482	673294.420039	39.279834
2570.873923	674601.876992	39.284852
2573.349235	675902.198918	39.289869
2575.883771	677179.460133	39.294887
2578.704259	678472.954814	39.299904
2580.801787	679773.894854	39.304922
2583.572837	681062.614149	39.309940
2586.033066	682360.149939	39.314957
2588.743434	683654.977922	39.319975
2591.229069	684951.300112	39.324992
2594.021586	686258.763081	39.330010
2596.801793	687544.635996	39.335028
2599.053109	688845.311551	39.340045
2601.281203	690156.131680	39.345063
2604.280290	691465.989475	39.350080
2606.692755	692782.652926	39.355098
2609.456729	694083.234281	39.360116
2611.767998	695396.056889	39.365133
2613.983608	696723.288451	39.370151
2616.604744	698036.712803	39.375168
2618.722669	699378.742950	39.380186
2621.103201	700721.121085	39.385204
2623.287858	702055.046487	39.390221
2625.912875	703375.906043	39.395239
2628.422254	704709.522475	39.400256
2630.750763	706041.923920	39.405274
2633.275572	707352.334912	39.410292
2635.926688	708679.074974	39.415309
2638.343983	710017.885447	39.420327
2640.821254	711362.668910	39.425344
2642.689076	712710.016077	39.430362
2645.196720	714048.974501	39.435380
2647.561439	715430.173034	39.440397
2650.166280	716827.243648	39.445415
2652.567433	718189.721401	39.450432
2655.321410	719609.666339	39.455450
2658.026148	720993.609913	39.460468
2661.295400	722357.791653	39.465485
2664.404943	723767.623642	39.470503
2667.168934	725156.307144	39.475520
2669.759920	726567.627994	39.480538
2672.590732	727976.048207	39.485556
2674.900233	729382.188071	39.490573
2677.057853	730826.260336	39.495591
2680.065154	732244.147351	39.500608
2682.669406	733661.952741	39.505626
2685.489329	735106.194410	39.510644
2687.999440	736545.241883	39.515661
2690.614208	738003.023163	39.520679
2693.455642	739457.145914	39.525696
2696.256170	740915.798534	39.530714
2699.052155	742387.606807	39.535732
2701.916785	743840.482629	39.540749
2704.605447	745300.815863	39.545767
2707.728711	746767.908981	39.550784
2710.000714	748227.521974	39.555802
2712.596405	749690.063628	39.560820
2715.270748	751184.504363	39.565837
2717.761530	752688.790835	39.570855
2720.598671	754157.155664	39.575872
2723.196154	755651.438572	39.580890
2725.875302	757166.743931	39.585908
2728.773963	758674.721851	39.590925
2731.223396	760171.448767	39.595943
2734.113765	761656.045223	39.600960
2736.191019	763196.587495	39.605978
2739.131398	764703.905606	39.610996
2742.047724	766240.491117	39.616013
2744.713738	767768.000305	39.621031
2747.655777	769305.921317	39.626048
2749.996043	770862.502889	39.631066
2753.434046	772373.751717	39.636084
2756.101276	773914.943339	39.641101
2758.791037	775467.846963	39.646119
2762.017159	776995.086590	39.651136
2764.842196	778535.481649	39.656154
2767.569476	780082.491477	39.661172
2770.519179	781613.967490	39.666189
2774.008446	783131.878293	39.671207
2777.734573	784659.490868	39.676224
2780.569719	786178.537626	39.681242
2783.269165	787681.688307	39.686260
2786.186589	789174.287727	39.691277
2788.897519	790709.900861	39.696295
2791.558923	792223.476147	39.701312
2794.461315	793722.966786	39.706330
2797.019237	795241.353754	39.711348
2800.100497	796730.964385	39.716365
2802.687079	798240.861313	39.721383
2805.308073	799764.920471	39.726400
2807.746531	801289.313157	39.731418
2810.068367	802781.822304	39.736436
2812.785924	804257.552232	39.741453
2814.980103	805764.510366	39.746471
2817.669712	807258.926935	39.751488
2820.461651	808768.796286	39.756506
2822.940182	810272.468284	39.761524
2825.730930	811766.665632	39.766541
2827.871540	813292.748333	39.771559
2830.233093	814831.935528	39.776576
2832.995340	816374.808907	39.781594
2835.958527	817898.982241	39.786612
2838.553689	819469.643153	39.791629
2841.097044	821039.699505	39.796647
2843.831510	822610.818396	39.801664
2846.151707	824217.786486	39.806682
2849.371787	825818.314055	39.811700
2852.904662	827392.555983	39.816717
2856.307928	828966.442165	39.821735
2859.131222	830580.988888	39.826752
2861.905675	832195.144378	39.831770
2864.984767	833785.805791	39.836788
2867.766729	835380.217238	39.841805
2870.133712	837006.587542	39.846823
2873.371142	838643.259655	39.851840
2875.803411	840268.647985	39.856858
2878.595595	841886.168290	39.861876
2881.490171	843523.351280	39.866893
2884.049853	845180.689966	39.871911
2886.871816	846830.550606	39.876928
2889.634965	848512.652524	39.881946
2892.288067	850171.970062	39.886964
2895.272876	851849.351026	39.891981
2897.653567	853541.048064	39.896999
2901.043865	855223.573549	39.902016
2903.467884	856926.965176	39.907034
2906.194338	858640.028065	39.912052
2909.272036	860353.138724	39.917069
2912.024021	862066.891800	39.922087
2915.015698	863798.064819	39.927104
2917.865274	865543.795670	39.932122
2920.676276	867261.700771	39.937140
2923.940565	868988.150947	39.942157
2926.619249	870749.750913	39.947175
2929.533619	872493.462724	39.952192
2932.498088	874242.273016	39.957210
2935.250498	876026.508987	39.962228
2938.223396	877771.571626	39.967245
2940.910390	879537.251614	39.972263
2944.034935	881305.038603	39.977280
2947.149830	883100.906787	39.982298
2950.202223	884865.410282	39.987316
2953.168160	886613.069432	39.992333
2955.964934	888410.062135	39.997351
2959.152470	890194.366004	40.002368
2961.902559	891973.654904	40.007386
2964.522517	893762.931813	40.012404
2967.746555	895550.490224	40.017421
2970.450538	897369.297606	40.022439
2973.882039	899170.632662	40.027456
2977.051060	900954.094631	40.032474
2979.810318	902757.772346	40.037492
2982.626769	904550.944775	40.042509
2985.552208	906351.324311	40.047527
2988.562420	908167.663180	40.052544
2991.742849	909989.443215	40.057562
2994.708588	911774.981250	40.062580
2997.928169	913572.496230	40.067597
3000.567945	915386.340388	40.072615
3003.517465	917172.633169	40.077632
3006.520277	918969.956493	40.082650
3009.410501	920733.581247	40.087668
3012.601419	922493.321316	40.092685
3015.254617	924278.006553	40.097703
3018.177114	926027.238372	40.102720
3021.292030	927796.582735	40.107738
3023.484544	929592.527923	40.112756
3026.984756	931362.260655	40.117773
3029.800355	933154.030284	40.122791
3032.614202	934959.464362	40.127808
3035.280163	936758.467563	40.132826
3038.497849	938559.637272	40.137844
3041.710780	940365.069456	40.142861
3044.745073	942202.710036	40.147879
3047.970577	944017.015876	40.152896
3050.898110	945854.151005	40.157914
3053.238287	947692.546931	40.162932
3056.737732	949537.259829	40.167949
3059.585116	951389.915041	40.172967
3062.667003	953262.569902	40.177984
3065.805258	955118.885361	40.183002
3068.403931	957013.239720	40.188020
3071.515824	958963.416623	40.193037
3074.368360	960906.132914	40.198055
3077.750827	962827.385423	40.203072
3080.801434	964785.671494	40.208090
3083.470205	966749.703530	40.213108
3086.537295	968690.443093	40.218125
3089.672956	970677.663036	40.223143
3092.434830	972659.377826	40.228160
3095.506806	974640.942228	40.233178
3098.099095	976647.350967	40.238196
3101.622078	978648.614393	40.243213
3104.520766	980662.922501	40.248231
3107.633821	982655.347776	40.253248
3111.187396	984689.460431	40.258266
3113.904950	986723.666861	40.263284
3117.306463	988733.194995	40.268301
3120.052648	990786.087961	40.273319
3123.419614	992813.148529	40.278336
3126.692931	994845.333544	40.283354
3129.417330	996885.140716	40.288372
3132.638990	998950.357687	40.293389
3135.965375	1001004.415693	40.298407
3138.899546	1003060.219601	40.303424
3142.042318	1005124.750373	40.308442
3145.036858	1007202.905620	40.313460
3148.186280	1009275.228871	40.318477
3151.143480	1011347.791552	40.323495
3154.059089	1013434.712271	40.328512
3157.877465	1015521.001164	40.333530
3161.200320	1017609.017890	40.338548
3164.669270	1019673.008900	40.343565
3167.703167	1021771.331652	40.348583
3170.834980	1023835.974559	40.353600
3174.331029	1025910.816468	40.358618
3177.570256	1027998.169750	40.363636
3180.588474	1030066.523879	40.368653
3183.914792	1032150.765947	40.373671
3186.882209	1034224.153818	40.378688
3190.302760	1036327.667956	40.383706
3193.338814	1038403.445025	40.388724
3196.561807	1040495.192858	40.393741
3199.834107	1042584.314220	40.398759
3203.124237	1044665.132053	40.403776
3207.366841	1046717.372847	40.408794
3210.065261	1048781.526726	40.413812
3213.581790	1050821.199021	40.418829
3217.071136	1052862.528577	40.423847
3220.214414	1054884.505342	40.428864
3223.339967	1056878.155595	40.433882
3226.234569	1058898.990402	40.438900
3229.681880	1060875.766692	40.443917
3232.226634	1062890.199358	40.448935
3235.000737	1064905.872219	40.453952
3238.231985	1066950.379853	40.458970
3241.187485	1068977.289952	40.463988
3244.544332	1071025.821099	40.469005
3247.474661	1073074.231557	40.474023
3250.155237	1075139.832931	40.479040
3253.301990	1077197.873096	40.484058
3256.278391	1079294.418082	40.489076
3259.354497	1081382.963689	40.494093
3262.588594	1083477.762212	40.499111
3265.837905	1085570.509321	40.504128
3269.497154	1087696.413709	40.509146
3272.255152	1089841.031907	40.514164
3275.349310	1091965.835967	40.519181
3278.590222	1094097.994456	40.524199
3281.643896	1096252.536340	40.529216
3285.042163	1098421.427916	40.534234
3288.023518	1100583.605742	40.539252
3291.685741	1102761.582908	40.544269
3294.824410	1104934.193470	40.549287
3297.777438	1107118.912453	40.554304
3300.914172	1109331.562669	40.559322
3304.051029	1111528.551615	40.564340
3307.252596	1113747.177230	40.569357
3310.194670	1115994.691516	40.574375
3313.471233	1118217.256145	40.579392
3317.081575	1120465.161250	40.584410
3319.958263	1122725.253510	40.589428
3323.675512	1124947.039063	40.594445
3326.371166	1127230.600691	40.599463
3329.745556	1129498.940196	40.604480
3333.125828	1131761.477486	40.609498
3336.425504	1134049.885349	40.614516
3339.770460	1136344.783867	40.619533
3343.017012	1138637.475628	40.624551
3346.596682	1140928.931994	40.629568
3349.870148	1143225.502139	40.634586
3352.958823	1145533.777327	40.639604
3356.429390	1147851.000762	40.644621
3359.951510	1150157.089180	40.649639
3363.064548	1152484.996096	40.654656
3365.867712	1154810.131661	40.659674
3368.966443	1157141.456330	40.664692
3371.903038	1159492.145010	40.669709
3375.487597	1161830.927458	40.674727
3378.773954	1164190.953536	40.679744
3382.250912	1166556.289260	40.684762
3385.320235	1168916.386051	40.689780
3388.683591	1171291.271260	40.694797
3391.844435	1173675.643420	40.699815
3395.366995	1176060.275500	40.704832
3399.080637	1178431.943454	40.709850
3401.985866	1180841.736824	40.714868
3405.298713	1183225.935135	40.719885
3408.910569	1185622.032356	40.724903
3412.531535	1188014.956431	40.729920
3415.724442	1190425.314092	40.734938
3419.435993	1192836.524012	40.739956
3422.576306	1195237.616184	40.744973
3425.763889	1197652.655848	40.749991
3429.243129	1200040.593677	40.755008
3433.013635	1202410.710547	40.760013
3436.205045	1204755.346865	40.765018
3439.631588	1207026.919061	40.770023
3443.000855	1209263.218181	40.775028
3445.845215	1211403.706348	40.780032
3449.231113	1213458.900660	40.785037
3452.042098	1215437.785486	40.790042
3454.818104	1217337.741560	40.795047
3457.681178	1219175.847296	40.800052
3460.424487	1220953.324009	40.805056
3463.360565	1222622.546492	40.810061
3466.054800	1224242.519059	40.815066
3468.388936	1225740.030096	40.820071
3471.007945	1227199.257588	40.825076
3473.394024	1228562.009667	40.830080
3475.496829	1229858.778867	40.835085
3477.473609	1231107.586777	40.840090
3479.458449	1232273.299809	40.845095
3481.719872	1233374.386013	40.850100
3483.185629	1234424.389858	40.855104
3485.371628	1235378.651325	40.860109
3486.959576	1236308.983790	40.865114
3488.690338	1237176.626585	40.870119
3490.743408	1237992.757039	40.875124
3492.282643	1238725.974005	40.880128
3494.009480	1239419.860242	40.885133
3495.025726	1240082.398878	40.890138
3496.762059	1240672.042543	40.895143
3498.233113	1241217.363221	40.900148
3499.676021	1241742.250909	40.905152
3501.026600	1242170.333156	40.910157
3501.867140	1242598.276900	40.915162
3503.023315	1242974.686850	40.920167
3504.030376	1243304.023222	40.925172
3504.720224	1243610.135715	40.930176
3506.004455	1243889.995035	40.935181
3506.532516	1244117.878516	40.940186
3507.471470	1244328.757095	40.945191
3508.592788	1244511.510343	40.950196
3509.064600	1244665.069335	40.955200
3509.896740	1244791.595366	40.960205
3510.421565	1244874.647340	40.965210
3511.412694	1244942.091210	40.970215
3511.929252	1245011.844147	40.975220
3512.255485	1245043.314945	40.980224
3512.962231	1245044.314632	40.985229
3513.744285	1245018.520192	40.990234
3514.105266	1244988.517295	40.995239
3514.458861	1244952.377865	41.000244
3515.024019	1244880.493423	41.005248
3515.333559	1244785.214951	41.010253
3516.104131	1244681.674882	41.015258
3516.425612	1244567.325579	41.020263
3517.022601	1244434.792729	41.025268
3517.496403	1244298.928477	41.030272
3517.727805	1244126.176109	41.035277
3517.834444	1243948.880765	41.040282
3518.615535	1243755.841494	41.045287
3518.852805	1243560.465884	41.050292
3519.052788	1243349.647008	41.055296
3519.257526	1243117.236190	41.060301
3519.577526	1242905.727767	41.065306
3519.778033	1242665.668224	41.070311
3520.404303	1242402.453082	41.075316
3520.051355	1242163.205056	41.080320
3520.456800	1241897.115475	41.085325
3520.490209	1241618.882900	41.090330
3520.820573	1241333.141222	41.095335
3521.022650	1241049.172717	41.100340
3521.388129	1240765.161301	41.105344
3521.441598	1240452.610801	41.110349
3521.709479	1240156.574261	41.115354
3521.548173	1239852.585477	41.120359
3521.781049	1239517.047778	41.125364
3521.888061	1239202.176678	41.130368
3522.297739	1238894.032780	41.135373
3522.252118	1238565.832995	41.140378
3522.580408	1238209.987396	41.145383
3522.854761	1237857.384953	41.150388
3522.442302	1237534.020939	41.155392
3522.937057	1237166.619294	41.160397
3522.968423	1236813.331977	41.165402
3523.123330	1236461.862604	41.170407
3523.209654	1236081.221894	41.175412
3522.971788	1235722.219982	41.180416
3523.505221	1235364.556261	41.185421
3523.361908	1234995.704233	41.190426
3523.284809	1234623.646113	41.195431
3523.518630	1234236.319228	41.200436
3523.738751	1233849.151328	41.205440
3523.808771	1233468.036873	41.210445
3523.749544	1233099.964728	41.215450
3523.845819	1232703.594723	41.220455
3523.553880	1232301.291074	41.225460
3523.604057	1231918.198589	41.230464
3524.142702	1231522.222612	41.235469
3523.961334	1231119.806842	41.240474
3523.748645	1230729.860561	41.245479
3523.927795	1230328.255076	41.250484
3523.856655	1229921.995435	41.255488
3524.131685	1229527.492542	41.260493
3523.949028	1229115.589925	41.265498
3524.109422	1228712.646775	41.270503
3524.276073	1228317.227910	41.275508
3524.124594	1227907.461207	41.280512
3524.211040	1227487.730763	41.285517
3524.287085	1227065.447575	41.290522
3524.060832	1226637.859149	41.295527
3524.083840	1226233.155017	41.300532
3523.937934	1225823.125705	41.305536
3524.044380	1225398.925275	41.310541
3524.151911	1225005.778634	41.315546
3524.069086	1224575.378747	41.320551
3524.252591	1224150.501157	41.325556
3524.120365	1223740.674974	41.330560
3524.422502	1223328.969759	41.335565
3524.586713	1222903.897758	41.340570
3524.186522	1222468.795134	41.345575
3524.363053	1222053.177592	41.350580
3524.377827	1221627.276181	41.355584
3524.393150	1221182.559333	41.360589
3523.936203	1220770.678616	41.365594
3524.276365	1220335.365023	41.370599
3524.411391	1219907.430947	41.375604
3524.291973	1219501.092667	41.380608
3524.462601	1219056.164494	41.385613
3524.082031	1218617.177396	41.390618
3524.079298	1218197.535427	41.395623
3524.475740	1217781.252444	41.400628
3524.239297	1217337.082671	41.405632
3524.327105	1216902.545852	41.410637
3523.987433	1216492.169995	41.415642
3524.053678	1216055.320130	41.420647
3524.381505	1215607.633417	41.425652
3524.421239	1215187.736771	41.430656
3524.333918	1214755.010263	41.435661
3524.317560	1214296.507067	41.440666
3524.438547	1213876.769902	41.445671
3524.409389	1213443.548424	41.450676
3524.265383	1213003.852009	41.455680
3524.462352	1212554.983413	41.460685
3523.913791	1212117.804308	41.465690
3523.755234	1211689.696924	41.470695
3524.119006	1211249.017083	41.475700
3524.065633	1210821.100510	41.480704
3523.842185	1210373.607603	41.485709
3523.898421	1209956.180773	41.490714
3523.899372	1209516.254186	41.495719
3523.983170	1209090.417783	41.500724
3524.038677	1208670.825899	41.505728
3524.026981	1208206.905357	41.510733
3523.897216	1207767.224713	41.515738
3523.810585	1207340.334101	41.520743
3524.193086	1206891.219103	41.525748
3523.980690	1206460.340793	41.530752
3524.063973	1206007.168486	41.535757
3523.969493	1205577.133633	41.540762
3523.752614	1205143.896225	41.545767
3523.824473	1204705.419352	41.550772
3523.460840	1204280.381711	41.555776
3523.594062	1203832.633543	41.560781
3523.824104	1203403.300543	41.565786
3523.478922	1202977.776976	41.570791
3523.629729	1202542.946747	41.575796
3523.475680	1202106.723213	41.580800
3523.674283	1201663.557990	41.585805
3523.529216	1201219.285596	41.590810
3523.395105	1200791.764057	41.595815
3523.652762	1200348.381932	41.600820
3523.191080	1199926.752619	41.605824
3523.611807	1199497.530986	41.610829
3523.562802	1199045.361027	41.615834
3523.483035	1198599.913219	41.620839
3523.689643	1198185.163304	41.625844
3523.488094	1197737.220747	41.630848
3523.448869	1197296.064884	41.635853
3523.206693	1196871.426882	41.640858
3523.127364	1196425.321490	41.645863
3522.937638	1195985.298658	41.650868
3522.953516	1195562.012516	41.655872
3523.106924	1195119.323951	41.660877
3522.968065	1194709.797792	41.665882
3522.757318	1194270.571213	41.670887
3523.392823	1193827.504533	41.675892
3523.121358	1193405.403744	41.680896
3523.191773	1192962.261915	41.685901
3523.049893	1192534.431710	41.690906
3522.807107	1192113.347990	41.695911
3523.048468	1191681.907409	41.700916
3522.861626	1191244.392716	41.705920
3523.314431	1190813.314675	41.710925
3522.928083	1190382.526874	41.715930
3522.822273	1189937.650628	41.720935
3523.272736	1189501.293435	41.725940
3522.874656	1189084.688940	41.730944
3522.358477	1188622.091700	41.735949
3522.494255	1188205.140378	41.740954
3522.367800	1187786.317820	41.745959
3523.164385	1187354.518666	41.750964
3522.678265	1186921.577961	41.755968
3522.520247	1186496.636590	41.760973
3522.738323	1186060.591905	41.765978
3522.591526	1185626.169980	41.770983
3522.788189	1185191.184617	41.775988
3522.447314	1184775.541011	41.780992
3522.408303	1184322.643275	41.785997
3522.555437	1183905.814409	41.791002
3522.459270	1183475.438889	41.796007
3522.652095	1183048.556903	41.801012
3522.506173	1182608.893181	41.806016
3522.602091	1182175.836549	41.811021
3522.550574	1181767.718055	41.816026
3522.503109	1181320.114418	41.821031
3522.590982	1180900.229069	41.826036
3522.652326	1180476.076309	41.831040
3522.298410	1180017.109924	41.836045
3522.134501	1179606.014558	41.841050
3521.894181	1179185.479508	41.846055
3522.294607	1178755.290177	41.851060
3522.069225	1178323.566700	41.856064
3521.980664	1177895.082571	41.861069
3522.134655	1177465.580905	41.866074
3521.834225	1177043.280584	41.871079
3521.788584	1176625.616214	41.876084
3521.602187	1176216.235623	41.881088
3521.642746	1175773.889065	41.886093
3521.787042	1175350.906868	41.891098
3521.602041	1174941.048702	41.896103
3521.609603	1174527.449576	41.901108
3521.481129	1174106.485444	41.906112
3521.517004	1173668.298136	41.911117
3521.158950	1173261.070917	41.916122
3521.774404	1172840.825084	41.921127
3521.563775	1172434.169181	41.926132
3521.373017	1171999.368745	41.931136
3521.415455	1171579.681641	41.936141
3521.399111	1171181.386219	41.941146
3521.435149	1170771.069360	41.946151
3521.240118	1170329.997760	41.951156
3521.475958	1169924.582420	41.956160
3521.357620	1169495.789526	41.961165
3521.304159	1169090.640212	41.966170
3521.163768	1168679.244212	41.971175
3521.200894	1168242.111072	41.976180
3521.163014	1167831.008987	41.981184
3521.130754	1167430.353179	41.986189
3521.204854	1167018.602304	41.991194
3520.829151	1166611.331060	41.996199
3520.904886	1166201.026342	42.001204
3520.922341	1165791.737879	42.006208
3520.857878	1165370.247200	42.011213
3520.800369	1164966.006652	42.016218
3520.437324	1164575.198778	42.021223
3520.418727	1164150.579549	42.026228
3520.843884	1163740.118814	42.031232
3520.554555	1163335.696088	42.036237
3520.573558	1162949.239167	42.041242
3520.479635	1162526.295995	42.046247
3520.766368	1162120.267096	42.051252
3520.907223	1161726.044923	42.056256
3520.780939	1161298.849465	42.061261
3520.765221	1160895.043997	42.066266
3520.657168	1160499.069072	42.071271
3520.328480	1160080.410388	42.076276
3520.279385	1159664.414202	42.081280
3520.290978	1159267.286552	42.086285
3520.120486	1158876.021842	42.091290
3520.458579	1158465.729883	42.096295
3520.597141	1158057.330319	42.101300
3520.209587	1157671.970121	42.106304
3520.499782	1157242.389487	42.111309
3520.421202	1156857.013216	42.116314
3519.945284	1156466.281480	42.121319
3520.096198	1156042.112928	42.126324
3519.824017	1155662.074000	42.131328
3519.898872	1155258.671634	42.136333
3519.648890	1154854.156184	42.141338
3519.682857	1154449.941436	42.146343
3520.069755	1154071.287962	42.151348
3519.899607	1153677.553741	42.156352
3519.846948	1153277.428152	42.161357
3519.856011	1152892.314868	42.166362
3519.513725	1152492.650696	42.171367
3519.728006	1152082.638377	42.176372
3519.382743	1151716.908219	42.181376
3519.900929	1151321.085245	42.186381
3519.677201	1150922.892345	42.191386
3519.530459	1150521.815239	42.196391
3519.539992	1150136.974018	42.201396
3519.289546	1149764.556947	42.206400
3519.581068	1149360.098527	42.211405
3519.315037	1148954.090298	42.216410
3519.244696	1148578.149047	42.221415
3519.392632	1148190.205750	42.226420
3518.995222	1147804.124260	42.231424
3519.043612	1147421.542380	42.236429
3519.131069	1147039.589785	42.241434
3518.938830	1146643.058863	42.246439
3519.099113	1146266.156694	42.251444
3518.968311	1145879.511389	42.256448
3518.520643	1145506.826286	42.261453
3518.650956	1145136.105552	42.266458
3518.944405	1144747.032044	42.271463
3518.473794	1144371.520923	42.276468
3518.578136	1143986.215580	42.281472
3518.838423	1143605.219073	42.286477
3518.424948	1143227.151463	42.291482
3518.395582	1142877.069795	42.296487
3518.303181	1142486.186187	42.301492
3518.585528	1142110.011048	42.306496
3518.574773	1141753.306252	42.311501
3518.573071	1141363.273510	42.316506
3518.000459	1140992.283229	42.321511
3518.552847	1140620.132747	42.326516
3518.232864	1140261.575443	42.331520
3518.177246	1139873.150027	42.336525
3518.466709	1139502.862504	42.341530
3518.287240	1139144.206447	42.346535
3518.357742	1138779.124964	42.351540
3517.790849	1138398.174751	42.356544
3517.974118	1138034.827161	42.361549
3517.934125	1137665.225075	42.366554
3517.794968	1137294.853954	42.371559
3518.148275	1136945.836445	42.376564
3517.983037	1136593.082816	42.381568
3518.055404	1136211.775319	42.386573
3517.855875	1135841.027768	42.391578
3517.496239	1135498.111075	42.396583
3517.659390	1135106.735942	42.401588
3517.494036	1134771.814581	42.406592
3517.540724	1134420.591649	42.411597
3517.459590	1134045.994157	42.416602
3517.700996	1133685.759651	42.421607
3517.875753	1133335.964214	42.426612
3517.856869	1132972.303421	42.431616
3517.911262	1132600.907796	42.436621
3517.629183	1132253.587327	42.441626
3517.560825	1131886.438915	42.446631
3517.487209	1131519.741305	42.451636
3517.412110	1131168.038386	42.456640
3517.061601	1130805.424790	42.461645
3517.324892	1130446.678516	42.466650
3517.271402	1130101.461682	42.471655
3517.260772	1129735.106143	42.476660
3516.985221	1129375.615762	42.481664
3517.425577	1129033.291342	42.486669
3517.378820	1128699.774869	42.491674
3517.221649	1128339.719558	42.496679
3517.399252	1127969.597353	42.501684
3517.181239	1127630.144794	42.506688
3517.155342	1127263.716952	42.511693
3516.989854	1126926.398945	42.516698
3516.983975	1126574.095826	42.521703
3517.026054	1126215.481657	42.526708
3516.570295	1125876.051728	42.531712
3516.781497	1125519.741837	42.536717
3516.818667	1125173.144004	42.541722
3516.566775	1124831.425171	42.546727
3516.580182	1124487.166072	42.551732
3516.870328	1124137.413554	42.556736
3516.891984	1123786.540037	42.561741
3516.932709	1123459.725706	42.566746
3516.662193	1123117.138634	42.571751
3516.843282	1122758.078880	42.576756
3516.417100	1122419.281151	42.581760
3516.563944	1122084.652617	42.586765
3516.575256	1121725.265773	42.591770
3516.515881	1121404.341696	42.596775
3516.381276	1121055.219272	42.601780
3516.233901	1120717.601147	42.606784
3516.741914	1120359.374176	42.611789
3516.250613	1120028.055942	42.616794
3516.257108	1119683.488488	42.621799
3516.368161	1119348.504122	42.626804
3515.900352	1119022.454982	42.631808
3516.100109	1118670.739935	42.636813
3516.482828	1118354.610158	42.641818
3516.128898	1118006.373101	42.646823
3516.343835	1117689.183432	42.651828
3516.237090	1117333.809612	42.656832
3516.168820	1116990.415467	42.661837
3515.961904	1116669.803623	42.666842
3515.759883	1116343.738236	42.671847
3516.299296	1115999.703908	42.676852
3515.586695	1115673.586515	42.681856
3515.745478	1115351.596208	42.686861
3515.646128	1115006.268548	42.691866
3515.622936	1114698.189975	42.696871
3515.666279	1114377.876620	42.701876
3516.133498	1114036.016896	42.706880
3515.887344	1113697.400191	42.711885
3516.021914	1113380.064183	42.716890
3515.820360	1113036.629532	42.721895
3515.984349	1112702.174789	42.726900
3515.510816	1112399.857251	42.731904
3515.693847	1112058.777002	42.736909
3515.456696	1111721.560610	42.741914
3515.327093	1111408.349530	42.746919
3515.449628	1111089.639790	42.751924
3515.176859	1110765.537053	42.756928
3515.321061	1110426.745220	42.761933
3515.420090	1110109.985311	42.766938
3515.227620	1109805.089538	42.771943
3515.462241	1109497.624509	42.776948
3515.072806	1109161.704274	42.781952
3515.133780	1108854.231069	42.786957
3514.863464	1108524.456221	42.791962
3515.074424	1108213.294039	42.796967
3515.243645	1107897.060541	42.801972
3515.059409	1107580.675717	42.806977
3515.166168	1107284.563020	42.811981
3515.154125	1106967.445393	42.816986
3514.926125	1106640.890380	42.821991
3515.277020	1106312.501156	42.826996
3514.807793	1106010.874071	42.832001
3514.991406	1105698.329436	42.837005
3514.885742	1105368.143072	42.842010
3514.616474	1105050.190769	42.847015
3514.840846	1104749.429610	42.852020
3514.479490	1104464.129530	42.857025
3514.591940	1104153.513301	42.862029
3514.693353	1103825.300242	42.867034
3514.773970	1103526.309948	42.872039
3514.800455	1103228.936488	42.877044
3514.480405	1102916.026824	42.882049
3514.557210	1102600.262133	42.887053
3514.271302	1102301.646609	42.892058
3514.278375	1101986.622096	42.897063
3514.331096	1101682.181705	42.902068
3514.671356	1101402.912780	42.907073
3514.258961	1101087.426929	42.912077
3514.390307	1100800.800361	42.917082
3514.226477	1100482.274575	42.922087
3514.229207	1100185.597808	42.927092
3514.144188	1099894.082541	42.932097
3514.522450	1099588.609963	42.937101
3514.122729	1099291.185387	42.942106
3513.877242	1098985.590201	42.947111
3514.235712	1098694.415348	42.952116
3513.891322	1098394.541349	42.957121
3513.934192	1098097.839004	42.962125
3514.007718	1097816.133050	42.967130
3513.753154	1097522.987357	42.972135
3513.939181	1097216.264502	42.977140
3514.131743	1096917.942152	42.982145
3513.916764	1096623.975864	42.987149
3513.842097	1096346.523177	42.992154
3513.777912	1096032.598433	42.997159
3513.886513	1095743.506679	43.002164
3513.671791	1095457.323616	43.007169
3513.605698	1095151.195130	43.012173
3513.652099	1094862.545095	43.017178
3513.608459	1094585.475578	43.022183
3513.596651	1094280.437470	43.027188
3513.340747	1093996.194023	43.032193
3513.386225	1093721.362954	43.037197
3513.820501	1093458.803244	43.042202
3513.426353	1093158.838715	43.047207
3513.696440	1092853.195163	43.052212
3513.334671	1092566.596363	43.057217
3513.571431	1092285.628947	43.062221
3513.519121	1091997.512823	43.067226
3513.502575	1091722.207598	43.072231
3513.426482	1091440.386072	43.077236
3513.247273	1091144.201111	43.082241
3513.321110	1090848.628744	43.087245
3513.439023	1090583.012834	43.092250
3513.063410	1090298.116287	43.097255
3513.223664	1090022.599921	43.102260
3513.176970	1089746.241490	43.107265
3513.139941	1089452.623098	43.112269
3513.269342	1089179.080855	43.117274
3512.836295	1088911.270346	43.122279
3512.991751	1088625.048794	43.127284
3512.618193	1088359.596692	43.132289
3513.122842	1088076.355004	43.137293
3512.978187	1087786.976475	43.142298
3512.775524	1087522.413636	43.147303
3513.269480	1087266.157147	43.152308
3512.730291	1086973.541712	43.157313
3512.871434	1086684.824199	43.162317
3512.900857	1086411.446653	43.167322
3512.719414	1086164.739185	43.172327
3512.590714	1085895.963038	43.177332
3512.644378	1085608.736644	43.182337
3512.798079	1085334.325800	43.187341
3512.535881	1085068.790503	43.192346
3512.415498	1084818.464391	43.197351
3512.572272	1084537.109227	43.202356
3512.514299	1084262.487427	43.207361
3512.207206	1084005.825728	43.212365
3512.577127	1083741.080522	43.217370
3512.237050	1083470.013602	43.222375
3512.592342	1083195.078089	43.227380
3512.313533	1082940.663411	43.232385
3512.166061	1082662.426739	43.237389
3512.474830	1082393.597419	43.242394
3512.323352	1082161.955794	43.247399
3512.490918	1081873.074587	43.252404
3512.044845	1081629.275030	43.257409
3512.067238	1081360.345974	43.262413
3512.181353	1081098.200932	43.267418
3512.022139	1080849.521796	43.272423
3512.093001	1080587.551236	43.277428
3511.977169	1080333.275844	43.282433
3512.085967	1080063.500901	43.287437
3512.011354	1079809.194290	43.292442
3511.761259	1079556.056440	43.297447
3511.965020	1079283.252015	43.302452
3511.858584	1079045.135790	43.307457
3512.020941	1078796.502058	43.312461
3511.997334	1078535.504406	43.317466
3511.976043	1078286.685715	43.322471
3511.758767	1078025.983596	43.327476
3511.670757	1077773.024350	43.332481
3511.737510	1077518.587718	43.337485
3511.930209	1077281.497440	43.342490
3511.757296	1077013.058358	43.347495
3511.906256	1076752.043062	43.352500
3511.526795	1076524.328620	43.357505
3511.718374	1076275.863403	43.362509
3511.819607	1076012.323757	43.367514
3511.585153	1075761.312278	43.372519
3511.425042	1075513.350537	43.377524
3511.382616	1075265.838423	43.382529
3511.387633	1075026.183869	43.387533
3511.328515	1074788.930874	43.392538
3511.192502	1074534.196554	43.397543
3511.674005	1074280.117216	43.402548
3511.501779	1074058.030007	43.407553
3511.400846	1073793.936370	43.412557
3511.425929	1073554.598342	43.417562
3511.067349	1073330.878916	43.422567
3511.293457	1073061.795714	43.427572
3510.881711	1072829.416409	43.432577
3511.056881	1072594.047616	43.437581
3510.877420	1072377.370988	43.442586
3510.765899	1072133.572611	43.447591
3511.075234	1071879.890748	43.452596
3510.996097	1071650.097704	43.457601
3511.022867	1071435.656605	43.462605
3510.971786	1071184.597112	43.467610
3511.023655	1070947.159262	43.472615
3511.081927	1070707.210648	43.477620
3510.681695	1070487.130980	43.482625
3510.699913	1070224.864371	43.487629
3510.816151	1070008.526020	43.492634
3510.792107	1069796.240435	43.497639
3510.652257	1069540.793602	43.502644
3510.624712	1069323.682690	43.507649
3510.751435	1069088.844367	43.512653
3510.959195	1068851.482375	43.517658
3510.646605	1068633.910279	43.522663
3510.720612	1068399.531965	43.527668
3510.755277	1068171.497740	43.532673
3510.703353	1067930.868698	43.537677
3510.929963	1067721.154547	43.542682
3510.756815	1067476.293440	43.547687
3510.724211	1067235.149766	43.552692
3510.885888	1067020.225133	43.557697
3510.922495	1066768.660365	43.562701
3510.749874	1066539.341850	43.567706
3510.595174	1066333.197046	43.572711
3510.715050	1066102.850043	43.577716
3510.720474	1065865.199783	43.582721
3510.505000	1065625.651209	43.587725
3510.343695	1065392.915224	43.592730
3510.115825	1065170.188128	43.597735
3510.419864	1064945.439744	43.602740
3510.415673	1064729.875398	43.607745
3510.349929	1064507.575921	43.612749
3510.347762	1064283.717073	43.617754
3510.209957	1064064.395106	43.622759
3510.430496	1063828.257520	43.627764
3510.382954	1063624.784728	43.632769
3510.010646	1063406.533946	43.637773
3510.127071	1063169.326355	43.642778
3510.019647	1062950.051189	43.647783
3510.469513	1062733.756176	43.652788
3510.202541	1062517.667002	43.657793
3510.340319	1062303.331972	43.662797
3510.377757	1062072.733339	43.667802
3510.152592	1061851.796974	43.672807
3510.057021	1061628.615707	43.677812
3510.100940	1061426.105703	43.682817
3510.094169	1061187.003339	43.687821
3509.998256	1060967.936165	43.692826
3509.707386	1060774.991254	43.697831
3510.126228	1060551.777905	43.702836
3509.962014	1060335.875040	43.707841
3509.836837	1060137.294317	43.712845
3509.967734	1059915.740002	43.717850
3509.921329	1059695.843493	43.722855
3509.896953	1059477.861143	43.727860
3509.689133	1059287.836611	43.732865
3509.705788	1059054.417673	43.737869
3509.664276	1058835.931067	43.742874
3509.152927	1058657.784534	43.747879
3509.558220	1058427.647028	43.752884
3509.215059	1058236.163311	43.757889
3509.398516	1058049.018455	43.762893
3509.484661	1057838.083166	43.767898
3509.531388	1057620.208332	43.772903
3509.500082	1057421.225159	43.777908
3509.345983	1057223.989647	43.782913
3509.269244	1057021.626668	43.787917
3509.440351	1056802.542589	43.792922
3509.202853	1056606.840740	43.797927
3509.569340	1056423.080189	43.802932
3509.106037	1056215.932231	43.807937
3508.969990	1056002.457311	43.812941
3509.279929	1055810.588997	43.817946
3509.253472	1055607.201925	43.822951
3509.316684	1055392.128243	43.827956
3509.152144	1055199.931253	43.832961
3509.211352	1055005.955404	43.837965
3509.224521	1054799.061395	43.842970
3508.750586	1054613.257991	43.847975
3509.110662	1054427.118135	43.852980
3508.970292	1054216.274498	43.857985
3508.889424	1054027.686880	43.862989
3508.874818	1053832.814165	43.867994
3508.801883	1053641.029949	43.872999
3509.087420	1053451.494440	43.878004
3509.008108	1053267.412983	43.883009
3508.792716	1053069.267552	43.888013
3508.880889	1052864.410398	43.893018
3508.977562	1052673.143313	43.898023
3508.729107	1052491.764391	43.903028
3508.877555	1052284.464558	43.908033
3508.698724	1052104.122439	43.913037
3508.654885	1051928.382289	43.918042
3508.409248	1051732.605410	43.923047
3508.730805	1051529.010817	43.928052
3508.735322	1051341.764463	43.933057
3508.397379	1051167.881516	43.938061
3508.606518	1050981.361045	43.943066
3508.203449	1050795.706957	43.948071
3508.550504	1050612.624614	43.953076
3508.459786	1050428.836428	43.958081
3508.366524	1050248.902132	43.963085
3508.331564	1050060.364537	43.968090
3508.002395	1049885.281902	43.973095
3508.540946	1049694.707478	43.978100
3508.506441	1049525.740873	43.983105
3508.481429	1049338.142057	43.988109
3508.606130	1049148.196018	43.993114
3508.083823	1048982.767487	43.998119
3508.268322	1048790.772595	44.003124
3508.452413	1048619.329449	44.008129
3508.177765	1048427.976708	44.013133
3508.475867	1048236.716069	44.018138
3508.139916	1048069.299051	44.023143
3508.267164	1047912.419006	44.028148
3508.363922	1047726.579602	44.033153
3508.423237	1047534.079101	44.038157
3508.166718	1047356.104924	44.043162
3508.169835	1047172.289687	44.048167
3507.937953	1046998.161673	44.053172
3507.957112	1046849.186098	44.058177
3508.288867	1046663.465432	44.063181
3508.336790	1046470.253988	44.068186
3508.159055	1046306.233607	44.073191
3508.312657	1046126.414337	44.078196
3508.294622	1045964.192196	44.083201
3508.127375	1045756.506683	44.088205
3508.185042	1045577.940807	44.093210
3508.178974	1045433.856461	44.098215
3508.198510	1045259.149532	44.103220
3507.879932	1045070.971655	44.108225
3507.835736	1044871.924903	44.113229
3507.990925	1044720.744901	44.118234
3507.790199	1044579.471404	44.123239
3507.911679	1044390.811618	44.128244
3507.865476	1044231.730954	44.133249
3508.000164	1044045.278913	44.138253
3508.162706	1043881.323949	44.143258
3507.819350	1043698.996222	44.148263
3508.096806	1043520.714340	44.153268
3508.166136	1043369.898107	44.158273
3507.766113	1043192.393528	44.163277
3507.756218	1043011.630704	44.168282
3507.461311	1042854.580451	44.173287
3507.550397	1042677.751799	44.178292
3507.623907	1042522.563901	44.183297
3507.599838	1042371.446057	44.188301
3507.885983	1042194.376308	44.193306
3507.558712	1042034.409292	44.198311
3507.808287	1041853.276129	44.203316
3507.721233	1041700.217684	44.208321
3507.435505	1041541.679205	44.213325
3507.806941	1041377.519264	44.218330
3507.218032	1041212.062945	44.223335
3507.567416	1041039.488375	44.228340
3507.395896	1040882.072058	44.233345
3507.261645	1040710.340145	44.238349
3507.424425	1040567.261504	44.243354
3507.343566	1040395.994374	44.248359
3507.053016	1040244.765907	44.253364
3507.299001	1040100.114923	44.258369
3507.571444	1039915.048180	44.263373
3507.682285	1039735.318886	44.268378
3507.112004	1039597.846363	44.273383
3507.356713	1039454.145537	44.278388
3507.412285	1039290.846106	44.283393
3507.262834	1039127.769015	44.288397
3507.521790	1038960.849127	44.293402
3507.340823	1038815.461567	44.298407
3507.281330	1038662.798370	44.303412
3507.129709	1038496.802402	44.308417
3507.058410	1038328.370829	44.313421
3507.263792	1038195.570717	44.318426
3506.941363	1038044.287642	44.323431
3507.383709	1037876.918229	44.328436
3507.139878	1037708.496310	44.333441
3507.020548	1037574.284240	44.338445
3507.136931	1037422.428435	44.343450
3507.049658	1037271.665899	44.348455
3506.932359	1037093.532990	44.353460
3507.308682	1036960.191664	44.358465
3506.940472	1036819.135204	44.363469
3507.159433	1036660.858003	44.368474
3506.863777	1036506.917122	44.373479
3506.856894	1036362.113882	44.378484
3506.978221	1036198.519412	44.383489
3507.177051	1036047.870084	44.388493
3507.234669	1035896.175811	44.393498
3506.884283	1035753.928554	44.398503
3506.935721	1035612.578923	44.403508
3506.943582	1035465.041100	44.408513
3506.855304	1035306.002035	44.413517
3506.999072	1035156.111662	44.418522
3506.690448	1035017.902311	44.423527
3506.995292	1034843.207807	44.428532
3506.626482	1034703.065409	44.433537
3506.666666	1034562.755360	44.438541
3506.747640	1034422.725356	44.443546
3506.485040	1034282.748422	44.448551
3506.983593	1034129.869005	44.453556
3506.853624	1033987.927427	44.458561
3506.938919	1033840.043516	44.463565
3506.895790	1033685.789522	44.468570
3506.861513	1033555.047347	44.473575
3506.641724	1033395.297960	44.478580
3506.588110	1033254.970449	44.483585
3506.948257	1033114.764836	44.488589
3506.576759	1032948.639664	44.493594
3506.500891	1032812.950632	44.498599
3506.419098	1032680.356716	44.503604
3506.568985	1032542.107244	44.508609
3506.115041	1032393.402613	44.513613
3506.314473	1032252.621009	44.518618
3506.610046	1032144.249552	44.523623
3506.754221	1031989.821001	44.528628
3506.372275	1031845.736644	44.533633
3506.396172	1031714.748134	44.538637
3506.244734	1031574.297646	44.543642
3506.360841	1031435.929524	44.548647
3506.537739	1031298.903426	44.553652
3506.498028	1031163.652426	44.558657
3506.320160	1031023.386072	44.563661
3506.225624	1030884.942165	44.568666
3506.176279	1030749.585894	44.573671
3506.270682	1030592.803012	44.578676
3505.949221	1030473.074656	44.583681
3506.243047	1030332.713261	44.588685
3506.437766	1030202.338983	44.593690
3505.931228	1030094.447210	44.598695
3506.267251	1029960.073570	44.603700
3506.267120	1029817.132900	44.608705
3506.245813	1029685.038928	44.613709
3506.337029	1029545.175356	44.618714
3506.080680	1029415.341253	44.623719
3505.829488	1029279.982609	44.628724
3506.037519	1029164.400557	44.633729
3506.042398	1029034.127145	44.638733
3505.994526	1028909.283569	44.643738
3505.620374	1028783.134867	44.648743
3506.237370	1028639.965579	44.653748
3505.737394	1028518.868614	44.658753
3506.164277	1028389.285606	44.663757
3506.075277	1028285.261746	44.668762
3506.135043	1028144.690209	44.673767
3506.439136	1027991.384119	44.678772
3506.107361	1027876.833120	44.683777
3506.148711	1027760.571353	44.688781
3506.182984	1027596.545158	44.693786
3505.621712	1027486.965003	44.698791
3505.891171	1027352.152105	44.703796
3506.089416	1027211.534304	44.708801
3505.838910	1027101.604740	44.713805
3506.030635	1026984.914516	44.718810
3505.657570	1026841.765385	44.723815
3505.837013	1026697.940197	44.728820
3505.766091	1026586.129847	44.733825
3505.616485	1026484.408079	44.738829
3506.221383	1026353.682681	44.743834
3505.848378	1026233.968861	44.748839
3505.589063	1026095.239594	44.753844
3505.766801	1025975.235709	44.758849
3505.965607	1025863.172666	44.763853
3505.883795	1025727.021690	44.768858
3505.405526	1025589.382014	44.773863
3505.654723	1025489.514832	44.778868
3505.811372	1025360.293868	44.783873
3505.402280	1025249.190954	44.788877
3505.664664	1025144.372331	44.793882
3505.323965	1025015.903812	44.798887
3505.637166	1024876.565399	44.803892
3505.777085	1024773.020091	44.808897
3504.879969	1024674.684227	44.813901
3505.560972	1024537.118533	44.818906
3505.420662	1024411.511221	44.823911
3505.615192	1024307.560561	44.828916
3505.745910	1024201.291877	44.833921
3505.540885	1024087.805689	44.838925
3505.819565	1023944.572027	44.843930
3505.543266	1023834.194722	44.848935
3505.655736	1023729.762117	44.853940
3505.485241	1023591.731768	44.858945
3505.552121	1023478.285398	44.863949
3505.800636	1023364.418991	44.868954
3505.258168	1023239.433368	44.873959
3505.857090	1023129.188894	44.878964
3505.538111	1023023.359779	44.883969
3505.530800	1022902.738764	44.888973
3505.383070	1022770.405326	44.893978
3505.111889	1022640.513319	44.898983
3505.706733	1022532.197162	44.903988
3505.605199	1022432.139310	44.908993
3505.388214	1022307.370196	44.913997
3505.489712	1022167.611397	44.919002
3505.366358	1022061.731897	44.924007
3505.195284	1021965.750285	44.929012
3505.292929	1021859.927555	44.934017
3505.143754	1021728.151641	44.939021
3505.388104	1021629.089318	44.944026
3505.081268	1021520.223231	44.949031
3505.164016	1021392.862700	44.954036
3505.147671	1021297.038136	44.959041
3505.126340	1021172.502515	44.964045
3505.407238	1021074.588314	44.969050
3505.131590	1020974.339128	44.974055
3505.248837	1020853.847512	44.979060
3505.022226	1020743.013123	44.984065
3505.261034	1020633.069925	44.989069
3505.179277	1020532.780911	44.994074
3505.123062	1020417.643790	44.999079
3504.962673	1020320.177139	45.004084
3505.244186	1020200.420510	45.009089
3505.294579	1020085.161999	45.014093
3505.239733	1019983.306521	45.019098
3504.921061	1019884.209113	45.024103
3504.886253	1019769.637270	45.029108
3504.954171	1019674.547264	45.034113
3505.034759	1019552.093333	45.039117
3504.987094	1019433.150733	45.044122
3505.146133	1019337.554890	45.049127
3505.274826	1019248.075159	45.054132
3505.096550	1019124.781296	45.059137
3505.090908	1019009.801023	45.064141
3505.122049	1018922.078734	45.069146
3505.294823	1018822.008325	45.074151
3505.304443	1018695.666007	45.079156
3505.193321	1018586.613703	45.084161
3504.841003	1018484.585946	45.089165
3505.186896	1018374.774971	45.094170
3504.849614	1018272.837932	45.099175
3504.915734	1018164.136408	45.104180
3504.811212	1018053.908116	45.109185
3504.672171	1017951.544398	45.114189
3504.928674	1017870.659114	45.119194
3504.895322	1017766.624747	45.124199
3504.822537	1017657.645142	45.129204
3504.769345	1017573.215547	45.134209
3504.780272	1017455.677257	45.139213
3504.583193	1017348.459179	45.144218
3504.752830	1017257.388027	45.149223
3504.504789	1017152.892345	45.154228
3504.925962	1017062.650183	45.159233
3504.622826	1016962.236772	45.164237
3504.618390	1016868.955454	45.169242
3504.378268	1016774.352423	45.174247
3504.547759	1016656.383018	45.179252
3504.348991	1016566.429145	45.184257
3504.394021	1016484.782160	45.189261
3504.386641	1016392.367096	45.194266
3504.295224	1016287.441213	45.199271
3504.196617	1016184.262004	45.204276
3504.593317	1016106.920233	45.209281
3504.448283	1016028.016210	45.214285
3504.663628	1015912.450726	45.219290
3504.003570	1015819.939580	45.224295
3504.365859	1015736.579001	45.229300
3504.833932	1015667.083571	45.234305
3504.298196	1015565.906800	45.239309
3504.369928	1015455.889783	45.244314
3504.446534	1015362.667218	45.249319
3504.395481	1015274.998619	45.254324
3504.398010	1015199.262835	45.259329
3504.555270	1015101.459072	45.264333
3504.792338	1014981.404321	45.269338
3504.406989	1014897.086334	45.274343
3504.666386	1014812.466681	45.279348
3504.510982	1014725.098011	45.284353
3504.239578	1014617.451650	45.289357
3504.512475	1014529.038317	45.294362
3504.472806	1014425.428693	45.299367
3504.443785	1014338.033195	45.304372
3504.428784	1014265.006867	45.309377
3504.275815	1014165.781234	45.314381
3504.566224	1014055.409470	45.319386
3504.558168	1013985.583240	45.324391
3504.284489	1013874.523888	45.329396
3504.410463	1013775.439670	45.334401
3504.392349	1013711.050524	45.339405
3504.451417	1013614.014071	45.344410
3504.361977	1013512.629710	45.349415
3504.720177	1013423.699339	45.354420
3504.586547	1013343.201717	45.359425
3504.495070	1013239.675925	45.364429
3504.374673	1013121.485875	45.369434
3504.878098	1013042.530295	45.374439
3504.421136	1012970.337039	45.379444
3504.387001	1012861.938056	45.384449
3504.104600	1012782.719712	45.389453
3504.092924	1012693.547317	45.394458
3504.317544	1012603.460310	45.399463
3504.514723	1012519.010724	45.404468
3504.216688	1012421.332526	45.409473
3504.184423	1012339.832406	45.414477
3504.360231	1012247.901964	45.419482
3504.277742	1012170.293598	45.424487
3504.515831	1012081.361824	45.429492
3504.239503	1011977.260357	45.434497
3504.083507	1011886.544505	45.439501
3504.290077	1011798.973631	45.444506
3504.197303	1011732.048089	45.449511
3504.296176	1011626.323821	45.454516
3504.455461	1011536.230514	45.459521
3504.238908	1011459.508882	45.464525
3504.427166	1011385.634431	45.469530
3504.228123	1011282.381860	45.474535
3504.044199	1011186.606749	45.479540
3504.401525	1011114.352731	45.484545
3503.829470	1011013.002850	45.489549
3504.226597	1010927.816298	45.494554
3503.768381	1010862.106665	45.499559
3504.110626	1010758.463823	45.504564
3504.193563	1010677.212199	45.509569
3503.877844	1010601.758498	45.514573
3504.256181	1010526.092294	45.519578
3503.989529	1010432.164369	45.524583
3504.020662	1010353.929188	45.529588
3504.113494	1010271.406731	45.534593
3503.801615	1010180.008796	45.539597
3503.712071	1010113.743787	45.544602
3503.708671	1010026.082770	45.549607
3503.869563	1009938.782084	45.554612
3503.934903	1009875.695978	45.559617
3503.917870	1009794.642479	45.564621
3504.046978	1009699.956832	45.569626
3503.883854	1009614.162374	45.574631
3503.675687	1009544.994402	45.579636
3504.070034	1009477.087091	45.584641
3504.007797	1009398.854038	45.589645
3503.881773	1009305.856155	45.594650
3503.897595	1009225.663860	45.599655
3503.949097	1009139.438026	45.604660
3503.892044	1009062.171469	45.609665
3503.677348	1008993.095005	45.614669
3504.099361	1008924.107237	45.619674
3503.618868	1008839.228110	45.624679
3503.836920	1008763.661882	45.629684
3504.166281	1008689.340037	45.634689
3503.892092	1008605.201086	45.639693
3503.861120	1008508.674798	45.644698
3503.784482	1008433.638753	45.649703
3503.419311	1008373.328749	45.654708
3503.531541	1008301.273506	45.659713
3503.361697	1008222.069689	45.664717
3503.805218	1008161.332570	45.669722
3503.381205	1008070.599432	45.674727
3503.788854	1007976.325084	45.679732
3503.659305	1007918.401957	45.684737
3503.502738	1007865.149437	45.689741
3503.610206	1007781.032554	45.694746
3503.896354	1007710.107827	45.699751
3503.581496	1007620.613418	45.704756
3503.737596	1007544.166018	45.709761
3503.436027	1007483.544332	45.714765
3503.438702	1007417.718607	45.719770
3503.347879	1007345.879077	45.724775
3503.519080	1007273.995477	45.729780
3503.555211	1007209.425858	45.734785
3503.714680	1007129.180108	45.739789
3504.078733	1007055.219992	45.744794
3503.387837	1006981.043705	45.749799
3503.458198	1006912.964445	45.754804
3503.637900	1006833.100119	45.759809
3503.192447	1006759.172212	45.764813
3503.269031	1006680.684116	45.769818
3503.504008	1006547.127497	45.774823
3503.631324	1006345.705270	45.779828
3503.483387	1006103.280029	45.784833
3503.317499	1005786.444111	45.789837
3503.451609	1005420.519129	45.794842
3503.289961	1004976.703471	45.799847
3503.363195	1004448.178874	45.804852
3503.537629	1003876.098555	45.809857
3503.237180	1003253.149153	45.814861
3503.280542	1002536.944170	45.819866
3503.023505	1001771.449826	45.824871
3502.555597	1000917.402099	45.829876
3502.970818	999988.989992	45.834881
3502.607098	998993.754090	45.839885
3502.514768	997932.654960	45.844890
3502.335031	996778.244007	45.849895
3502.385169	995565.001838	45.854900
3502.289548	994252.118056	45.859905
3502.250892	992861.423832	45.864909
3501.724193	991371.890532	45.869914
3501.431630	989835.697653	45.874919
3501.326194	988211.352062	45.879924
3501.180220	986483.787276	45.884929
3500.846338	984685.832893	45.889933
3500.736166	982774.680238	45.894938
3500.578068	980816.591688	45.899943
3500.721956	978762.600783	45.904948
3500.550441	976592.274984	45.909953
3499.950944	974330.831453	45.914957
3500.061884	971992.945267	45.919962
3499.051829	969584.307372	45.924967
3499.045860	967062.960904	45.929972
3498.668865	964469.740274	45.934977
3498.196356	961780.197659	45.939981
3498.296571	959004.288354	45.944986
3497.779917	956124.622720	45.949991
3497.480774	953227.715149	45.954996
3497.054645	950270.095556	45.960001
3496.195744	947236.232262	45.965005
3495.936505	944078.104297	45.970010
3495.435021	940866.025502	45.975015
3495.002585	937569.631519	45.980020
3494.582106	934181.681782	45.985025
3493.736800	930697.667746	45.990029
3493.306440	927127.854975	45.995034
3492.648744	923507.024192	46.000039
3491.972097	919774.209993	46.005044
3491.511260	915965.966607	46.010049
3490.737929	912101.527394	46.015053
3490.477337	908105.309111	46.020058
3489.504407	904050.632954	46.025063
3488.820443	899898.196975	46.030068
3488.434290	895677.689612	46.035073
3487.789367	891376.790258	46.040077
3486.929153	886969.484530	46.045082
3486.213759	882513.650457	46.050087
3485.369857	877941.750901	46.055092
3485.450448	873295.309542	46.060097
3484.121017	868567.482038	46.065101
3483.331576	863735.432630	46.070106
3482.650107	858834.926823	46.075111
3482.089602	853861.945550	46.080116
3481.413283	848777.220698	46.085121
3479.981436	843612.964017	46.090125
3479.699452	838386.822252	46.095130
3478.436556	833058.306746	46.100135
3477.697957	827636.208168	46.105140
3476.685248	822144.748767	46.110145
3475.389672	816582.540721	46.115149
3475.072366	810904.855480	46.120154
3474.195102	805155.766291	46.125159
3473.254375	799334.879104	46.130164
3472.241818	793409.505047	46.135169
3470.879165	787387.362846	46.140173
3470.382986	781289.734038	46.145178
3469.044490	775140.969404	46.150183
3468.076640	768878.994075	46.155188
3467.073106	762515.263250	46.160193
3465.711629	756077.852593	46.165197
3464.643955	749579.997064	46.170202
3463.531670	742986.764923	46.175207
3462.333886	736289.300393	46.180212
3461.273579	729509.745364	46.185217
3460.110861	722669.552840	46.190221
3459.146895	715708.270916	46.195226
3457.463081	708690.873598	46.200231
3456.586682	701572.285881	46.205236
3455.034540	694394.455023	46.210241
3453.405476	687126.925998	46.215245
3452.372385	679741.430510	46.220250
3450.957678	672319.705227	46.225255
3449.818037	664807.124164	46.230260
3448.574651	657183.180780	46.235265
3446.919400	649516.077917	46.240269
3445.897362	641762.901984	46.245274
3443.955826	633894.409150	46.250279
3442.526727	625959.390319	46.255284
3441.295712	617960.096812	46.260289
3439.594445	609891.423816	46.265293
3438.511610	601706.443974	46.270298
3436.818939	593455.206938	46.275303
3435.100605	585141.805607	46.280308
3433.279534	576715.717801	46.285313
3431.556940	568246.826656	46.290317
3430.015459	559691.771848	46.295322
3427.983987	551048.598453	46.300327
3426.473036	542324.509717	46.305332
3424.889153	533541.434373	46.310337
3422.470292	524696.136504	46.315341
3421.072363	515748.917263	46.320346
3419.299122	506746.383077	46.325351
3417.081974	497669.622264	46.330356
3415.254402	488512.345720	46.335361
3413.086286	479293.837207	46.340365
3411.231309	469999.100928	46.345370
3409.094934	460649.415729	46.350375
3407.239835	451213.733878	46.355380
3405.011497	441733.557885	46.360385
3402.870193	432160.194917	46.365389
3400.484860	422525.920806	46.370394
3398.037988	412825.449317	46.375399
3395.826275	403049.054678	46.380404
3393.573914	393245.528109	46.385409
3390.843798	383382.584361	46.390413
3388.690807	373453.316806	46.395418
3386.010815	363459.975975	46.400423
3383.642824	353405.749623	46.405428
3380.886356	343293.530812	46.410433
3378.347463	333161.997365	46.415437
3375.660624	322956.213699	46.420442
3372.839370	312703.771317	46.425447
3369.998457	302400.872695	46.430452
3367.269946	292062.414507	46.435457
3364.163965	281665.843445	46.440461
3361.179439	271227.360270	46.445466
3357.841050	260764.966073	46.450471
3354.809946	250244.703995	46.455476
3351.801368	239701.823168	46.460481
3348.631870	229159.790853	46.465485
3345.178334	218446.201324	46.470490
3341.658612	207795.162957	46.475495
3337.940767	197138.800304	46.480500
3334.391716	186452.537692	46.485505
3330.500960	175766.291951	46.490509
3326.451693	165064.624399	46.495514
3322.099029	154345.926541	46.500519
3318.013097	143627.533416	46.505524
3313.235439	132910.987875	46.510529
3308.316526	122232.506056	46.515533
3302.946486	111545.504564	46.520538
3297.344991	100901.088438	46.525543
3290.858327	90295.270225	46.530548
3284.276483	79746.084250	46.535553
3275.521496	69279.920034	46.540557
3262.737695	59037.803973	46.545562
3235.557463	49342.200747	46.550567
3202.835803	40095.693023	46.555572
3164.965106	31438.053303	46.560577
3119.269221	23655.904775	46.565581
3070.617720	16747.990628	46.570586
3023.207853	10767.800191	46.575591
2980.471413	5728.044854	46.580596
2939.758097	1678.308834	46.585601
2837.275775	383.155505	46.590605
2743.315885	391.297710	46.595610
2715.897854	373.997899	46.600615
2739.623501	352.447899	46.605620
2787.434196	343.705919	46.610625
2834.751684	343.281133	46.615629
2867.821643	332.287923	46.620634
2884.209869	355.589797	46.625639
2886.335195	359.482894	46.630644
2880.953490	333.374347	46.635649
2872.970360	336.377121	46.640653
2866.202839	323.416135	46.645658
2860.611245	338.198113	46.650663
2857.085672	349.942186	46.655668
2854.758070	332.176631	46.660673
2853.443354	349.933336	46.665677
2852.097222	331.245379	46.670682
2849.652500	310.421147	46.675687
2847.530226	320.019632	46.680692
2844.594511	326.321042	46.685697
2841.624601	329.981875	46.690701
2838.773600	321.485668	46.695706
2835.213452	317.426305	46.700711
2831.728377	320.277206	46.705716
2829.359658	314.982237	46.710721
2826.033161	308.930183	46.715725
2823.155993	315.449532	46.720730
2820.360701	296.947466	46.725735
2817.229002	311.872499	46.730740
2813.681042	298.716315	46.735745
2810.351498	301.750623	46.740749
2807.125390	320.606488	46.745754
2803.731028	305.866197	46.750759
2800.145492	319.686889	46.755764
2797.116056	307.676780	46.760769
2794.044746	295.592791	46.765773
2790.945071	294.767474	46.770778
2787.583057	276.061749	46.775783
2784.409219	296.273312	46.780788
2781.070341	305.626771	46.785793
2777.415867	304.993650	46.790797
2774.411039	293.554148	46.795802
2770.770658	299.823969	46.800807
2767.512114	286.599095	46.805812
2764.158651	292.545488	46.810817
2760.784254	303.457178	46.815821
2757.565934	302.613355	46.820826
2754.033958	295.306446	46.825831
2750.306135	289.820172	46.830836
2747.438399	286.936463	46.835841
2743.686692	278.181398	46.840845
2740.114894	279.298835	46.845850
2736.950793	283.518111	46.850855
2733.637475	276.158401	46.855860
2730.515268	288.418202	46.860865
2726.924245	301.524488	46.865869
2723.722566	282.901369	46.870874
2719.886418	299.500057	46.875879
2716.474032	288.482730	46.880884
2713.353552	270.903386	46.885889
2709.850849	287.537649	46.890893
2706.695583	270.050166	46.895898
2702.583916	276.881196	46.900903
2698.965433	289.827362	46.905908
2696.320687	275.910419	46.910913
2692.616510	265.658028	46.915917
2689.079641	276.592268	46.920922
2685.388566	275.399071	46.925927
2682.376508	289.521203	46.930932
2679.435438	281.680481	46.935937
2675.524122	273.932755	46.940941
2671.976286	270.755268	46.945946
2668.764100	269.379045	46.950951
2665.047743	277.180348	46.955956
2661.739898	263.347611	46.960961
2658.038387	274.151856	46.965965
2654.514834	262.236450	46.970970
2650.994665	281.439698	46.975975
2647.484081	270.092253	46.980980
2644.208698	277.807144	46.985985
2640.485116	270.944161	46.990989
2637.493538	274.967910	46.995994
2633.774308	266.573751	47.000999
2630.905082	259.859151	47.006004
2627.427724	251.896178	47.011009
2623.341125	252.273143	47.016013
2620.262635	267.161293	47.021018
2616.500146	279.443431	47.026023
2613.055659	261.781937	47.031028
2609.782242	258.182095	47.036033
2605.859390	268.471396	47.041037
2602.703447	252.774219	47.046042
2599.490933	257.886415	47.051047
2595.872709	258.665604	47.056052
2592.399197	251.198919	47.061057
2588.707628	263.246509	47.066061
2585.757324	259.043621	47.071066
2581.454507	251.987244	47.076071
2578.038489	260.703851	47.081076
2574.990937	248.705574	47.086081
2571.450707	253.546370	47.091085
2568.312620	252.093850	47.096090
2564.887802	251.171999	47.101095
2561.009212	249.029893	47.106100
2557.768053	259.406567	47.111105
2553.686568	262.253225	47.116109
2550.554173	247.358373	47.121114
2546.961610	255.552546	47.126119
2543.248348	250.533969	47.131124
2540.009818	241.835590	47.136129
2536.423885	251.791454	47.141133
2533.073178	239.328538	47.146138
2530.086038	242.924923	47.151143
2526.399205	260.734603	47.156148
2522.884249	248.746938	47.161153
2519.051492	246.990024	47.166157
2515.926880	241.910107	47.171162
2512.162332	237.854745	47.176167
2508.854661	249.929116	47.181172
2505.357658	244.116576	47.186177
2501.967843	253.682604	47.191181
2498.753706	242.466123	47.196186
2494.970256	242.303367	47.201191
2491.262714	252.846145	47.206196
2487.805416	234.015405	47.211201
2484.462203	222.117547	47.216205
2480.809868	231.680791	47.221210
2477.467386	225.424811	47.226215
2473.545276	238.826631	47.231220
2470.815289	226.298099	47.236225
2466.781923	241.516660	47.241229
2463.612509	251.059672	47.246234
2460.071130	229.389562	47.251239
2456.247229	244.651620	47.256244
2453.527338	230.404719	47.261249
2449.544662	228.159882	47.266253
2445.632438	242.442016	47.271258
2442.338722	222.912931	47.276263
2438.753707	239.954603	47.281268
2435.843394	248.825802	47.286273
2432.222091	236.761231	47.291277
2428.868405	222.721663	47.296282
2425.131763	231.724885	47.301287
2421.339854	233.586874	47.306292
2417.824446	226.557614	47.311297
2414.235510	234.867736	47.316301
2411.143448	227.306192	47.321306
2408.160486	242.964166	47.326311
2404.598988	236.286601	47.331316
2401.165505	243.775187	47.336321
2397.328542	237.658895	47.341325
2393.707147	221.356469	47.346330
2389.983802	235.632919	47.351335
2386.531249	224.667830	47.356340
2383.167599	233.521660	47.361345
2379.476952	232.806804	47.366349
2376.278806	235.504220	47.371354
2373.026479	234.995174	47.376359
2369.062573	234.252882	47.381364
2365.979097	228.084953	47.386369
2362.215162	245.052184	47.391373
2358.808949	229.065577	47.396378
2355.127962	229.737244	47.401383
2351.527181	231.994011	47.406388
2347.980942	225.759666	47.411393
2344.544830	230.626980	47.416397
2341.351762	232.603724	47.421402
2337.754052	224.539926	47.426407
2334.095573	242.064307	47.431412
2330.998914	237.568611	47.436417
2327.472908	228.534706	47.441421
2323.943987	224.422042	47.446426
2319.962113	227.074619	47.451431
2316.532366	219.112958	47.456436
2313.283006	212.364343	47.461441
2309.441244	232.147744	47.466445
2305.958887	237.001690	47.471450
2303.157874	226.983068	47.476455
2299.552787	218.956321	47.481460
2296.145870	221.668864	47.486465
2292.427166	222.947263	47.491469
2289.035466	214.287218	47.496474
2285.414263	229.716838	47.501479
2281.696743	216.421705	47.506484
2278.367029	205.949807	47.511489
2274.633828	234.744726	47.516493
2271.289211	219.705126	47.521498
2268.055301	225.684544	47.526503
2264.505939	232.165145	47.531508
2260.898758	222.943128	47.536513
2257.503687	218.643186	47.541517
2254.251515	232.514548	47.546522
2250.298581	219.003350	47.551527
2246.869428	218.797377	47.556532
2243.268190	229.557585	47.561537
2239.384071	241.168357	47.566541
2236.240743	215.913634	47.571546
2233.024977	221.888294	47.576551
2229.379036	216.074827	47.581556
2225.841228	205.112859	47.586561
2222.475741	222.539700	47.591565
2218.967146	211.463016	47.596570
2215.172917	216.460573	47.601575
2211.731552	233.391306	47.606580
2208.773670	215.124163	47.611585
2204.992882	228.046411	47.616589
2201.419123	201.185686	47.621594
2198.055664	200.560688	47.626599
2194.137622	218.790528	47.631604
2190.935923	207.503235	47.636609
2187.175508	213.835973	47.641613
2183.991118	212.888160	47.646618
2180.715207	218.018058	47.651623
2176.697337	200.693975	47.656628
2173.589291	209.492191	47.661633
2169.513515	233.856065	47.666637
2166.424090	222.423489	47.671642
2163.159422	210.583601	47.676647
2158.990045	206.058067	47.681652
2156.036682	209.463647	47.686657
2152.458772	216.355236	47.691661
2148.851426	206.073429	47.696666
2145.300332	216.396564	47.701671
2141.831487	219.366011	47.706676
2138.674328	191.592489	47.711681
2134.916895	215.297040	47.716685
2131.665267	196.868294	47.721690
2127.984378	201.720426	47.726695
2124.316637	221.233079	47.731700
2121.087577	199.765954	47.736705
2117.575471	232.559491	47.741709
2113.864125	214.032844	47.746714
2110.529044	216.295021	47.751719
2106.623525	216.845020	47.756724
2103.498550	206.642398	47.761729
2100.215282	206.888117	47.766733
2096.131814	208.611317	47.771738
2092.780147	218.223756	47.776743
2089.125600	202.615297	47.781748
2085.970456	211.702560	47.786753
2082.500090	220.437662	47.791757
2078.825156	218.148680	47.796762
2075.353019	199.993693	47.801767
2071.847707	217.781902	47.806772
2068.736155	212.007336	47.811777
2065.202773	201.673923	47.816781
2061.744098	210.475165	47.821786
2058.000606	202.362489	47.826791
2054.126264	220.576289	47.831796
2050.836937	204.932369	47.836801
2047.269888	203.028101	47.841805
2043.823421	200.362789	47.846810
2040.617659	209.152012	47.851815
2036.713411	206.903645	47.856820
2033.620125	217.065671	47.861825
2029.627654	206.898964	47.866829
2026.715124	195.707899	47.871834
2022.959858	194.719677	47.876839
2019.409258	195.992180	47.881844
2016.012737	187.179400	47.886849
2012.479098	208.897250	47.891853
2008.947742	196.582955	47.896858
2005.190499	208.547537	47.901863
2001.705182	197.383400	47.906868
1998.364495	202.401034	47.911873
1994.964934	211.382944	47.916877
1991.504972	189.596408	47.921882
1987.871705	189.210556	47.926887
1983.953028	200.966395	47.931892
1981.050087	188.758971	47.936897
1977.637726	190.029404	47.941901
1974.158424	206.530404	47.946906
1970.739904	192.826787	47.951911
1966.910120	185.066976	47.956916
1963.293001	192.525034	47.961921
1959.828812	180.411306	47.966925
1956.369318	193.713386	47.971930
1953.007804	188.714273	47.976935
1949.156792	188.123560	47.981940
1945.908143	199.141563	47.986945
1942.378318	203.232045	47.991949
1939.035384	188.374611	47.996954
1935.716856	193.996586	48.001959
1932.195498	192.286579	48.006964
1928.276115	184.843539	48.011969
1924.499771	200.525537	48.016973
1921.211209	187.385803	48.021978
1917.818218	203.565777	48.026983
1914.299433	195.767015	48.031988
1911.034691	206.866412	48.036993
1907.618568	200.702596	48.041997
1904.210047	171.538268	48.047002
1900.360383	196.963414	48.052007
1896.642838	199.411301	48.057012
1893.356995	190.118158	48.062017
1890.118053	196.714601	48.067021
1886.223529	184.096786	48.072026
1883.076984	198.923284	48.077031
1879.803872	184.596151	48.082036
1876.259467	174.704663	48.087041
1872.121269	189.957763	48.092045
1868.832348	193.764669	48.097050
1865.342381	179.498484	48.102055
1861.646247	189.346274	48.107060
1858.465082	193.411230	48.112065
1854.892658	181.979428	48.117069
1851.435736	165.398733	48.122074
1847.947402	181.331833	48.127079
1844.088944	179.435404	48.132084
1840.651475	186.680679	48.137089
1837.146445	189.767602	48.142093
1833.897374	188.163652	48.147098
1830.524210	186.506881	48.152103
1826.775457	188.502910	48.157108
1823.415633	191.019266	48.162113
1819.913838	185.853269	48.167117
1816.359742	178.374891	48.172122
1812.870202	188.491664	48.177127
1809.395917	190.969597	48.182132
1805.756033	201.048643	48.187137
1802.194963	194.126711	48.192141
1798.816152	174.340177	48.197146
1795.493314	185.070767	48.202151
1791.933564	181.878354	48.207156
1788.194718	177.685894	48.212161
1784.879899	182.911436	48.217165
1781.227730	183.139643	48.222170
1777.939397	184.889360	48.227175
1774.370411	185.581898	48.232180
1771.095259	188.845284	48.237185
1767.096956	191.902550	48.242189
1764.092386	184.239119	48.247194
1760.267904	190.676032	48.252199
1756.673375	182.337331	48.257204
1753.451217	171.081505	48.262209
1749.454674	193.393589	48.267213
1746.323014	175.798046	48.272218
1742.555304	198.951147	48.277223
1739.157599	190.154994	48.282228
1736.269542	164.693548	48.287233
1732.089888	179.590508	48.292237
1728.827366	168.356551	48.297242
1725.352788	182.064762	48.302247
1721.614103	179.718232	48.307252
1718.556246	171.430298	48.312257
1714.720148	198.849516	48.317261
1711.415447	178.146591	48.322266
1708.075503	187.668725	48.327271
1704.301814	184.325213	48.332276
1700.988166	168.273112	48.337281
1697.130483	174.002196	48.342285
1693.643347	177.092246	48.347290
1690.410347	177.507424	48.352295
1686.727808	201.826429	48.357300
1683.127954	184.347337	48.362305
1679.818424	188.322071	48.367309
1676.159146	182.598139	48.372314
1672.686251	165.969887	48.377319
1669.075236	177.514767	48.382324
1666.060781	172.529071	48.387329
1662.292113	174.388978	48.392333
1658.862904	186.699865	48.397338
1655.308602	178.756583	48.402343
1651.776964	169.269264	48.407348
1648.474557	171.540351	48.412353
1644.741480	185.805407	48.417357
1641.194528	182.200287	48.422362
1638.017871	185.235973	48.427367
1634.086431	182.178177	48.432372
1630.617643	172.520292	48.437377
1627.205472	190.348572	48.442381
1623.669736	197.694402	48.447386
1620.115487	178.384803	48.452391
1616.677488	191.355640	48.457396
1613.081145	177.277934	48.462401
1609.536175	180.493479	48.467405
1606.419797	181.813494	48.472410
1602.603997	178.503921	48.477415
1598.925371	183.260621	48.482420
1595.695084	182.122168	48.487425
1591.936106	186.060523	48.492429
1588.987679	180.730236	48.497434
1585.332766	180.117719	48.502439
1581.676771	176.984313	48.507444
1578.452288	172.876174	48.512449
1574.687041	183.673043	48.517453
1571.194077	176.755797	48.522458
1568.240714	177.847583	48.527463
1564.373434	190.465190	48.532468
1560.519584	169.644166	48.537473
1556.977175	167.800508	48.542477
1553.385989	172.125216	48.547482
1550.114169	185.475869	48.552487
1546.469467	186.172038	48.557492
1543.032274	177.960506	48.562497
1539.393598	183.438077	48.567501
1536.311584	178.952692	48.572506
1532.818615	175.666829	48.577511
1529.345402	180.815627	48.582516
1525.760215	172.813892	48.587521
1522.174790	179.217082	48.592525
1518.578897	177.100528	48.597530
1515.477625	178.689964	48.602535
1511.393912	184.837426	48.607540
1508.290503	162.504023	48.612545
1504.911509	175.637093	48.617549
1501.158055	155.579285	48.622554
1497.633037	170.470497	48.627559
1493.795104	168.255894	48.632564
1490.583019	168.724039	48.637569
1486.898114	182.541228	48.642573
1483.909260	167.774424	48.647578
1480.321589	169.457664	48.652583
1476.415782	168.196565	48.657588
1473.330348	143.384661	48.662593
1469.491093	162.239050	48.667597
1466.323627	179.433015	48.672602
1462.724361	167.727612	48.677607
1458.780881	154.869797	48.682612
1455.749617	160.457765	48.687617
1451.852022	174.136244	48.692621
1448.512717	153.978262	48.697626
1444.884425	172.298593	48.702631
1441.458129	175.358199	48.707636
1438.314317	169.213732	48.712641
1434.425952	165.854680	48.717645
1431.024373	159.382734	48.722650
1427.811485	179.835959	48.727655
1424.168730	178.349564	48.732660
1420.710826	158.561963	48.737665
1416.720215	169.322887	48.742669
1413.223091	172.145996	48.747674
1410.118615	151.752481	48.752679
1406.766575	170.585577	48.757684
1403.375547	161.721551	48.762689
1399.766999	160.922531	48.767693
1396.074606	175.454312	48.772698
1392.393447	156.737025	48.777703
1388.547573	163.517181	48.782708
1385.570770	158.493647	48.787713
1382.253849	145.898267	48.792717
1378.675070	156.259766	48.797722
1374.824486	159.835519	48.802727
1371.044753	165.572905	48.807732
1368.092762	174.747707	48.812737
1364.451332	161.259156	48.817741
1361.198404	161.356771	48.822746
1357.613458	159.885930	48.827751
1354.096293	157.956729	48.832756
1350.636545	158.631842	48.837761
1347.081272	167.972219	48.842765
1343.612183	177.533457	48.847770
1339.603563	163.451392	48.852775
1336.480162	169.165594	48.857780
1333.053127	144.046753	48.862785
1329.284346	158.988212	48.867789
1325.692095	167.621572	48.872794
1322.246294	155.802253	48.877799
1318.694551	183.259443	48.882804
1315.839185	174.391683	48.887809
1312.532397	162.003597	48.892813
1308.684553	154.247193	48.897818
1305.172189	160.099793	48.902823
1301.418443	169.561340	48.907828
1298.226262	150.478521	48.912833
1294.250047	171.872305	48.917837
1290.619852	163.837799	48.922842
1287.676603	137.800043	48.927847
1283.807421	159.405405	48.932852
1280.499765	161.702085	48.937857
1277.224166	164.272157	48.942861
1273.395187	161.185238	48.947866
1269.622410	160.189169	48.952871
1265.701089	149.247633	48.957876
1262.887599	159.062416	48.962881
1259.508023	163.126326	48.967885
1256.139697	151.609740	48.972890
1252.677327	158.728152	48.977895
1249.092784	162.921294	48.982900
1246.056900	152.483701	48.987905
1241.835757	154.710711	48.992909
1237.868535	153.356900	48.997914
1234.968837	149.200262	49.002919
1231.328664	162.296328	49.007924
1228.310567	144.831464	49.012929
1224.063438	164.790557	49.017933
1220.659989	163.356613	49.022938
1217.624230	149.041349	49.027943
1213.685738	165.853721	49.032948
1210.553097	134.860224	49.037953
1206.808034	159.750130	49.042957
1203.048256	161.861149	49.047962
1200.023663	150.144124	49.052967
1196.345682	160.090885	49.057972
1193.258638	163.401001	49.062977
1189.416313	155.932309	49.067981
1185.885246	158.379851	49.072986
1182.473687	141.876587	49.077991
1178.633588	141.599583	49.082996
1175.588418	147.297375	49.088001
1171.813971	165.639745	49.093005
1168.311868	154.479220	49.098010
1165.246417	154.834820	49.103015
1161.299082	156.486640	49.108020
1157.840030	137.894173	49.113025
1154.433459	154.527494	49.118029
1150.557993	148.541953	49.123034
1147.392914	160.596516	49.128039
1143.415797	167.943096	49.133044
1140.297031	147.075460	49.138049
1136.744112	150.912146	49.143053
1133.307065	161.441530	49.148058
1129.723052	135.355586	49.153063
1126.128261	158.505511	49.158068
1122.750610	155.548769	49.163073
1119.561209	153.602378	49.168077
1116.039067	147.685784	49.173082
1112.186769	152.718396	49.178087
1108.409868	156.560803	49.183092
1105.286784	154.828784	49.188097
1101.650929	148.359404	49.193101
1098.428287	141.660126	49.198106
1095.144562	158.806678	49.203111
1091.683866	165.722953	49.208116
1088.045350	143.217092	49.213121
1083.877409	153.291646	49.218125
1080.309944	152.673248	49.223130
1077.466076	132.352870	49.228135
1073.569732	151.233186	49.233140
1070.465082	140.822342	49.238145
1067.046761	153.046091	49.243149
1062.909161	153.412427	49.248154
1059.772425	144.815103	49.253159
1056.234358	151.332602	49.258164
1052.888390	158.394297	49.263169
1049.337424	162.971750	49.268173
1045.553903	141.034601	49.273178
1042.034650	149.926022	49.278183
1038.631160	153.202130	49.283188
1035.225429	150.012329	49.288193
1031.651312	133.084603	49.293197
1028.235211	148.220280	49.298202
1024.875647	153.468021	49.303207
1020.966870	149.075604	49.308212
1017.801241	139.116704	49.313217
1014.364871	159.181926	49.318221
1010.306001	133.701364	49.323226
1007.555692	153.109559	49.328231
1003.748228	141.179702	49.333236
1000.129158	148.350628	49.338241
996.653536	162.545191	49.343245
992.784038	145.207535	49.348250
989.851445	143.556973	49.353255
986.445038	150.046945	49.358260
983.249576	139.488377	49.363265
979.523206	155.671750	49.368269
975.646690	161.986714	49.373274
972.300674	151.114541	49.378279
968.199105	153.256962	49.383284
964.680605	150.170361	49.388289
961.408975	141.423522	49.393293
957.946519	145.656225	49.398298
954.782129	142.445068	49.403303
951.197402	145.678437	49.408308
948.088481	144.847376	49.413313
944.330751	156.351942	49.418317
940.541102	137.009942	49.423322
936.929068	145.923334	49.428327
933.028381	149.092677	49.433332
930.377459	138.242196	49.438337
926.738384	150.868332	49.443341
923.255568	146.197299	49.448346
920.261167	152.600329	49.453351
916.077441	145.701062	49.458356
912.479566	146.125651	49.463361
908.754912	141.261751	49.468365
905.371761	148.286929	49.473370
902.201970	129.967990	49.478375
898.531626	146.862459	49.483380
895.267204	152.502554	49.488385
891.716629	142.111288	49.493389
887.612908	137.036347	49.498394
884.787975	132.892788	49.503399
881.055365	153.817547	49.508404
877.700722	150.241969	49.513409
874.086668	146.834809	49.518413
870.610495	153.265523	49.523418
867.187058	134.636412	49.528423
863.716521	132.575187	49.533428
859.952327	144.405104	49.538433
856.387876	146.492732	49.543437
852.884078	143.145507	49.548442
849.441066	149.887512	49.553447
846.218402	136.817408	49.558452
842.679348	145.305950	49.563457
839.134396	136.999601	49.568461
835.752708	126.827309	49.573466
832.047486	140.249930	49.578471
828.133860	156.123652	49.583476
825.013646	142.967387	49.588481
821.526260	134.000272	49.593485
818.067846	145.594256	49.598490
814.735684	135.943629	49.603495
810.718497	136.964098	49.608500
807.488784	153.469775	49.613505
804.216261	148.757275	49.618509
800.504248	145.238092	49.623514
797.073174	145.720429	49.628519
793.395197	127.925949	49.633524
789.812882	137.472449	49.638529
786.732270	139.961612	49.643533
782.791743	141.007022	49.648538
779.326866	138.522893	49.653543
776.040604	137.940002	49.658548
772.592653	157.823918	49.663553
769.451289	146.292355	49.668557
765.715879	151.587876	49.673562
762.287792	129.008280	49.678567
758.023721	138.554826	49.683572
754.840770	138.297783	49.688577
751.334324	135.309737	49.693581
747.747165	125.267911	49.698586
744.607572	125.369597	49.703591
740.941819	150.406924	49.708596
737.488517	137.898401	49.713601
734.096018	150.783783	49.718605
730.247213	155.966948	49.723610
726.976394	132.103347	49.728615
723.400267	141.073741	49.733620
720.181673	130.338729	49.738625
716.475513	128.200292	49.743629
713.014913	141.440708	49.748634
709.553522	138.020862	49.753639
705.667438	136.679031	49.758644
702.348310	140.686844	49.763649
699.049753	129.500323	49.768653
695.246806	142.227005	49.773658
691.959652	117.815894	49.778663
688.122684	121.869576	49.783668
684.878954	127.601334	49.788673
681.457834	116.769294	49.793677
677.834582	134.415836	49.798682
674.560640	135.224456	49.803687
670.605887	136.491378	49.808692
667.434801	139.598568	49.813697
664.169885	134.562809	49.818701
660.460063	141.222297	49.823706
657.324953	125.372672	49.828711
653.331004	136.121169	49.833716
649.804532	133.228132	49.838721
645.995215	141.684549	49.843725
642.605253	128.893072	49.848730
639.507661	138.288653	49.853735
635.792192	130.575848	49.858740
632.360805	136.608427	49.863745
628.860065	131.122050	49.868749
625.351673	134.771499	49.873754
621.893484	134.276665	49.878759
618.097010	121.635906	49.883764
615.049811	119.295964	49.888769
611.481400	124.706716	49.893773
607.723330	121.704677	49.898778
604.467614	138.413669	49.903783
600.729147	148.894692	49.908788
597.534589	134.523875	49.913793
593.947045	134.209244	49.918797
589.904786	128.526355	49.923802
586.811581	130.294599	49.928807
583.004265	144.222001	49.933812
580.049687	140.786682	49.938817
576.303496	131.235467	49.943821
572.859817	136.200666	49.948826
569.579296	134.914561	49.953831
565.443775	145.287758	49.958836
562.393957	118.515481	49.963841
559.111900	128.189948	49.968845
555.051575	125.956906	49.973850
552.042323	121.001406	49.978855
548.440141	141.090187	49.983860
544.508274	138.637354	49.988865
541.317146	127.695689	49.993869
537.834567	143.786964	49.998874
534.058742	124.609532	50.003879
530.315479	125.271816	50.008884
527.411500	132.248879	50.013889
523.916138	128.401197	50.018893
520.106054	124.265861	50.023898
516.614820	126.403224	50.028903
513.087729	130.110961	50.033908
509.965020	128.361319	50.038913
506.255457	121.846489	50.043917
502.618031	116.202050	50.048922
499.165415	134.688172	50.053927
495.658633	134.755337	50.058932
492.599431	119.273474	50.063937
488.544366	139.791818	50.068941
484.867296	122.383928	50.073946
481.924871	124.220633	50.078951
477.898915	122.796002	50.083956
474.668673	102.037963	50.088961
471.232874	120.233941	50.093965
467.606400	122.819331	50.098970
464.287597	119.307121	50.103975
460.702573	118.405493	50.108980
457.285358	128.401624	50.113985
453.613821	131.648499	50.118989
450.244580	132.264530	50.123994
447.025448	131.491475	50.128999
443.091773	120.550314	50.134004
439.745254	104.344739	50.139009
435.912159	135.973656	50.144013
432.518628	119.796452	50.149018
429.520206	122.808539	50.154023
425.418839	144.794148	50.159028
422.104079	126.942611	50.164033
418.733532	120.865268	50.169037
415.224526	134.468525	50.174042
411.696961	108.735929	50.179047
407.858788	123.545262	50.184052
404.691511	130.258975	50.189057
401.095641	131.343953	50.194061
397.544383	123.381634	50.199066
394.096280	119.960862	50.204071
390.599537	122.788250	50.209076
387.404634	124.617481	50.214081
383.973529	114.801277	50.219085
379.935274	122.360364	50.224090
376.755840	125.542752	50.229095
373.049064	127.163472	50.234100
369.455492	135.854478	50.239105
365.961750	136.654875	50.244109
362.578156	118.085169	50.249114
359.244953	124.421561	50.254119
355.656801	113.494709	50.259124
351.895214	115.469267	50.264129
348.420011	136.256269	50.269133
344.374248	120.607610	50.274138
341.721837	131.576072	50.279143
338.045853	123.856450	50.284148
334.923739	115.782437	50.289153
331.324618	126.568747	50.294157
327.198588	117.773855	50.299162
324.417715	116.236449	50.304167
320.519534	143.150081	50.309172
316.999074	136.339258	50.314177
313.713537	125.560414	50.319181
309.883612	134.066665	50.324186
306.366913	126.691462	50.329191
302.703085	114.826684	50.334196
299.395966	126.123206	50.339201
295.877669	143.096061	50.344205
292.503949	138.070001	50.349210
289.242866	124.390557	50.354215
285.557062	131.820049	50.359220
282.240112	123.479548	50.364225
278.854802	125.864401	50.369229
274.689270	116.611348	50.374234
271.584358	129.339975	50.379239
268.283738	139.699384	50.384244
264.379322	130.000116	50.389249
260.832912	143.786792	50.394253
257.409507	124.074592	50.399258
253.764586	117.628659	50.404263
250.394672	129.210605	50.409268
247.098066	108.515576	50.414273
243.726008	123.866583	50.419277
240.051913	143.832997	50.424282
236.959385	128.514235	50.429287
232.937371	124.712013	50.434292
229.392416	115.851865	50.439297
226.012246	137.784280	50.444301
222.239847	121.918412	50.449306
219.058876	111.237878	50.454311
215.118187	139.818197	50.459316
211.569459	119.006508	50.464321
208.226091	110.498582	50.469325
204.768569	125.056597	50.474330
201.510660	121.748041	50.479335
198.270860	124.836611	50.484340
194.746793	122.999655	50.489345
191.007227	116.641413	50.494349
187.396808	118.433448	50.499354
184.367796	128.089340	50.504359
180.194342	127.147289	50.509364
176.824964	112.936953	50.514369
173.278786	120.653965	50.519373
169.894055	112.328389	50.524378
166.488574	106.127253	50.529383
162.482048	129.663294	50.534388
159.314208	119.966794	50.539393
156.075470	106.517458	50.544397
152.327089	114.645903	50.549402
149.199381	130.433828	50.554407
145.494795	117.833278	50.559412
141.560358	122.086554	50.564417
138.057315	132.695693	50.569421
134.640522	126.540335	50.574426
131.550413	119.098604	50.579431
127.581872	131.719625	50.584436
124.660224	115.053805	50.589441
121.235786	128.563099	50.594445
117.303136	111.461025	50.599450
114.220832	123.679514	50.604455
110.390792	144.737328	50.609460
106.918103	130.783905	50.614465
103.277400	115.803826	50.619469
99.760707	111.852299	50.624474
96.167752	119.048034	50.629479
92.813568	141.400381	50.634484
89.185979	120.114700	50.639489
85.958079	126.473473	50.644493
82.304277	119.240928	50.649498
78.998477	99.378927	50.654503
75.207426	111.139233	50.659508
71.996370	120.183769	50.664513
68.497977	111.220027	50.669517
64.838714	110.597931	50.674522
61.582040	126.744984	50.679527
57.521290	121.782586	50.684532
54.114788	110.804493	50.689537
50.466396	117.826940	50.694541
47.372114	122.872065	50.699546
43.655902	133.184329	50.704551
40.599714	136.932471	50.709556
36.835512	129.123750	50.714561
33.076848	134.774675	50.719565
29.328621	118.990071	50.724570
26.125109	121.434506	50.729575
22.602884	127.656886	50.734580
19.141216	116.673822	50.739585
15.805166	127.910453	50.744589
12.510958	133.670779	50.749594
9.089673	118.358246	50.754599
5.478818	120.767490	50.759604
1.687420	126.601920	50.764609