Wed Jun 15 16:17:37 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.907268	105.132254	0.000000
0.882902	101.086974	0.005005
0.810556	84.125758	0.010010
0.484932	71.729745	0.015014
0.028417	73.649118	0.020019
0.103059	66.219403	0.025024
-0.353230	63.966298	0.030029
-0.790910	44.059455	0.035034
-0.469891	43.157488	0.040038
-1.248210	38.475175	0.045043
-1.367027	4.717475	0.050048
-1.719815	18.151505	0.055053
-2.159178	16.134135	0.060058
-2.746564	3.284656	0.065062
-2.947785	10.367967	0.070067
-2.776954	-7.039756	0.075072
-3.251586	-17.906722	0.080077
-3.973728	-12.171545	0.085082
-4.191545	2.170987	0.090086
-4.409358	-1.700543	0.095091
-4.127827	-19.129111	0.100096
-4.495236	-24.102546	0.105101
-5.348202	-5.737442	0.110106
-5.311540	-16.637511	0.115110
-5.878727	-5.451423	0.120115
-5.784344	-5.099927	0.125120
-5.952507	-11.044317	0.130125
-5.797652	-13.832844	0.135130
-5.740581	-3.907134	0.140134
-7.082595	-8.965236	0.145139
-7.182440	-17.795647	0.150144
-7.408222	0.635091	0.155149
-7.587332	8.404379	0.160154
-7.716859	-21.257292	0.165158
-7.734979	-14.320655	0.170163
-7.983006	-10.737461	0.175168
-8.743021	-21.379107	0.180173
-9.230424	-11.591786	0.185178
-8.728316	1.235438	0.190182
-9.079239	-2.189226	0.195187
-8.961996	-13.158744	0.200192
-9.773809	1.662526	0.205197
-10.339361	-20.589413	0.210202
-10.515115	-20.774692	0.215206
-10.887038	-12.819071	0.220211
-10.369440	-5.581215	0.225216
-10.848412	-6.645035	0.230221
-11.094101	-12.029127	0.235226
-11.138534	0.598695	0.240230
-11.811262	-12.905680	0.245235
-11.936638	-15.310824	0.250240
-12.317046	1.033661	0.255245
-12.276233	-3.700060	0.260250
-12.352357	-5.344006	0.265254
-13.858885	5.762057	0.270259
-13.541698	-27.383612	0.275264
-13.537186	-9.059011	0.280269
-14.105501	-22.314388	0.285274
-13.883465	-23.409912	0.290278
-14.085314	4.449376	0.295283
-14.096438	-0.810423	0.300288
-14.937354	-8.294863	0.305293
-15.538957	2.061881	0.310298
-15.360985	-11.809180	0.315302
-15.842621	-2.427353	0.320307
-15.575206	-11.272887	0.325312
-15.471962	6.946733	0.330317
-15.612172	-10.031372	0.335322
-16.310001	-16.778699	0.340326
-17.211957	-8.102570	0.345331
-17.020364	-17.061245	0.350336
-17.030157	-9.003986	0.355341
-17.267298	4.935812	0.360346
-17.793885	-7.001758	0.365350
-18.525267	5.799078	0.370355
-18.705923	4.431253	0.375360
-18.702757	-5.230806	0.380365
-19.021985	-0.428418	0.385370
-18.739484	-17.446385	0.390374
-18.947023	2.113594	0.395379
-19.190085	-14.578896	0.400384
-19.561687	-12.831003	0.405389
-20.236345	7.625038	0.410394
-20.099471	-2.116334	0.415398
-20.347174	-13.370897	0.420403
-20.505559	-9.512401	0.425408
-21.311714	1.930896	0.430413
-21.833422	-9.715191	0.435418
-21.682770	3.744233	0.440422
-21.770697	7.853093	0.445427
-21.880340	-1.450292	0.450432
-22.148846	-26.858060	0.455437
-22.189278	-16.775183	0.460442
-22.494247	-1.947123	0.465446
-23.267768	-7.354665	0.470451
-23.494532	9.081330	0.475456
-23.359678	-1.117130	0.480461
-23.411441	-10.279048	0.485466
-23.736229	-7.259654	0.490470
-24.652681	-1.793228	0.495475
-25.124171	-14.131126	0.500480
-25.135896	5.156785	0.505485
-25.350415	3.362883	0.510490
-25.153394	-8.722287	0.515494
-25.458845	10.997906	0.520499
-25.136568	-8.809245	0.525504
-25.684953	1.776045	0.530509
-26.556264	-6.199362	0.535514
-26.623919	-10.765114	0.540518
-26.875162	-1.947638	0.545523
-26.614693	-21.695728	0.550528
-27.149624	0.773554	0.555533
-27.490198	-5.496481	0.560538
-27.664684	0.727936	0.565542
-28.249263	-5.696894	0.570547
-28.416455	-11.161136	0.575552
-28.396562	-4.963913	0.580557
-28.704669	1.541335	0.585562
-29.189870	-6.932910	0.590566
-29.564519	11.602639	0.595571
-29.708122	-1.174471	0.600576
-29.586132	2.682576	0.605581
-30.020955	-9.936311	0.610586
-29.904138	-7.185315	0.615590
-30.500675	1.964253	0.620595
-31.256543	-15.123495	0.625600
-31.357649	7.362783	0.630605
-31.616141	0.024953	0.635610
-31.766937	-2.170511	0.640614
-31.817020	15.191477	0.645619
-32.050815	0.775867	0.650624
-32.023584	-9.574964	0.655629
-32.023292	2.684817	0.660634
-32.676689	5.054782	0.665638
-33.415630	7.049629	0.670643
-33.130701	-7.613381	0.675648
-33.360008	-5.191184	0.680653
-33.843900	-0.616484	0.685658
-34.265413	-4.319399	0.690662
-34.890957	-17.949542	0.695667
-34.794560	-8.538363	0.700672
-34.586023	7.584894	0.705677
-35.008696	-6.176151	0.710682
-34.817502	-5.297117	0.715686
-35.218561	12.072266	0.720691
-35.548725	-3.556244	0.725696
-36.140801	-15.828241	0.730701
-36.418096	-8.399340	0.735706
-36.119950	-9.880227	0.740710
-36.826530	-9.306691	0.745715
-37.263174	10.566084	0.750720
-37.506762	-4.009977	0.755725
-38.000670	-12.986069	0.760730
-37.709654	-11.970631	0.765734
-37.807269	-2.433672	0.770739
-37.805839	-8.187587	0.775744
-38.765690	-8.709283	0.780749
-39.089605	-9.522616	0.785754
-39.358304	-8.723833	0.790758
-39.392518	-7.418192	0.795763
-39.443450	-13.040736	0.800768
-39.623084	-1.231924	0.805773
-39.628909	7.520336	0.810778
-40.069174	-11.183503	0.815782
-40.834751	-4.871957	0.820787
-41.034072	0.998283	0.825792
-40.963447	-14.742619	0.830797
-41.157043	-5.410863	0.835802
-41.507422	10.884373	0.840806
-41.990301	10.765142	0.845811
-42.414254	-17.953048	0.850816
-42.718203	2.410053	0.855821
-42.753271	8.523834	0.860826
-42.614568	2.052663	0.865830
-43.167935	-0.485550	0.870835
-42.807910	15.081272	0.875840
-42.755951	8.778815	0.880845
-44.110122	9.495285	0.885850
-44.287577	-5.943213	0.890854
-44.510871	9.746740	0.895859
-44.196170	-2.786201	0.900864
-44.596124	4.638611	0.905869
-45.338561	-4.278556	0.910874
-45.655687	2.844028	0.915878
-46.031851	3.929580	0.920883
-46.014212	-23.508454	0.925888
-45.953076	-4.754042	0.930893
-46.038893	4.480003	0.935898
-46.020895	-2.424790	0.940902
-46.945849	10.677936	0.945907
-47.539269	12.960258	0.950912
-47.702524	-2.591369	0.955917
-48.045034	-12.251435	0.960922
-47.648415	1.825990	0.965926
-47.974497	2.405400	0.970931
-48.008436	11.280288	0.975936
-48.501462	0.056794	0.980941
-49.323343	0.719721	0.985946
-49.284001	4.589835	0.990950
-49.433404	1.585640	0.995955
-49.815984	9.211878	1.000960
-49.659260	5.128016	1.005965
-49.869557	3.370804	1.010970
-49.560795	-4.968804	1.015974
-50.711243	-7.217458	1.020979
-51.006183	3.987959	1.025984
-51.043385	-4.546612	1.030989
-51.332586	10.100203	1.035994
-51.321035	2.425556	1.040998
-52.090553	-1.181174	1.046003
-52.551638	5.323906	1.051008
-52.657038	-10.056457	1.056013
-53.170873	-4.099813	1.061018
-52.684564	-4.583317	1.066022
-52.911355	-0.502806	1.071027
-52.836211	-2.658173	1.076032
-53.182340	5.955797	1.081037
-53.950502	-7.036809	1.086042
-54.303983	-2.289824	1.091046
-54.449083	-3.822638	1.096051
-54.253448	-3.318304	1.101056
-54.637786	-4.829237	1.106061
-55.648292	-5.417037	1.111066
-55.755576	1.220647	1.116070
-56.083193	-0.641074	1.121075
-55.399765	-3.768211	1.126080
-55.773871	-5.768145	1.131085
-55.992950	2.600802	1.136090
-56.209816	-0.048068	1.141094
-56.886806	6.597063	1.146099
-57.282315	5.415775	1.151104
-57.474876	-14.895685	1.156109
-57.960541	3.007629	1.161114
-57.618136	2.111499	1.166118
-57.978694	6.735955	1.171123
-58.357925	12.828982	1.176128
-58.845782	-5.860088	1.181133
-59.653202	4.902074	1.186138
-59.410697	-2.709628	1.191142
-59.860714	-4.960202	1.196147
-59.694853	6.157912	1.201152
-59.915502	8.930057	1.206157
-59.860267	-10.007584	1.211162
-59.701531	-10.766328	1.216166
-60.730773	-7.509766	1.221171
-61.114419	-4.936090	1.226176
-61.038364	9.725625	1.231181
-61.198796	14.826021	1.236186
-60.964322	-4.249858	1.241190
-61.677549	-16.758404	1.246195
-62.226321	-7.961108	1.251200
-62.407705	-9.433373	1.256205
-62.881922	4.558622	1.261210
-62.793143	0.578323	1.266214
-62.939810	0.793377	1.271219
-63.236160	19.915757	1.276224
-63.562935	-7.469325	1.281229
-64.003334	-6.392886	1.286234
-64.306490	5.480931	1.291238
-64.187781	0.858434	1.296243
-64.438248	-2.914179	1.301248
-65.037581	1.713832	1.306253
-65.111999	12.530346	1.311258
-65.608263	-8.079444	1.316262
-65.715004	-10.876132	1.321267
-65.978100	-4.131909	1.326272
-65.732429	6.757276	1.331277
-65.966130	4.728317	1.336282
-66.439207	-14.925768	1.341286
-67.011628	-4.760293	1.346291
-67.413574	3.209964	1.351296
-67.224751	-12.491677	1.356301
-67.512823	4.317751	1.361306
-67.851599	20.675296	1.366310
-68.521792	-1.428948	1.371315
-68.927514	-19.346156	1.376320
-68.902780	4.415712	1.381325
-69.197394	1.444100	1.386330
-69.210825	-6.379215	1.391334
-69.272599	9.230475	1.396339
-69.409879	-4.449393	1.401344
-69.607101	-6.180847	1.406349
-69.972570	12.948706	1.411354
-70.500170	-14.443912	1.416358
-70.640401	5.406695	1.421363
-70.788235	17.617966	1.426368
-70.696479	-0.777841	1.431373
-71.388592	18.650246	1.436378
-72.168190	-9.778635	1.441382
-72.527533	3.270359	1.446387
-72.445380	1.977872	1.451392
-71.869140	-3.929441	1.456397
-72.790762	-6.836784	1.461402
-72.794062	5.114826	1.466406
-72.745283	13.516747	1.471411
-73.306265	-6.070241	1.476416
-73.629052	-15.835756	1.481421
-73.938577	0.604924	1.486426
-74.079807	-4.849895	1.491430
-74.198453	-8.759805	1.496435
-75.079810	4.297139	1.501440
-75.485811	-1.676991	1.506445
-74.999563	-4.717976	1.511450
-75.562481	0.991191	1.516454
-75.854931	-0.452559	1.521459
-75.771615	0.004047	1.526464
-75.720455	5.116721	1.531469
-76.190977	4.943070	1.536474
-76.615574	3.201450	1.541478
-76.943475	6.940984	1.546483
-76.976600	0.540730	1.551488
-77.110757	0.658523	1.556493
-77.472698	7.760697	1.561498
-78.452258	-5.980805	1.566502
-78.753957	5.960441	1.571507
-79.124391	15.717693	1.576512
-78.448090	-1.018924	1.581517
-79.159073	-5.956682	1.586522
-78.826218	-1.389517	1.591526
-79.124100	-6.407388	1.596531
-79.379825	5.803652	1.601536
-80.053314	0.897574	1.606541
-80.427544	3.959275	1.611546
-80.433338	3.724699	1.616550
-80.772836	2.376619	1.621555
-80.762191	7.887515	1.626560
-80.588119	17.068747	1.631565
-81.563277	17.439373	1.636570
-81.940776	-9.662883	1.641574
-82.204209	-0.135611	1.646579
-82.271578	5.758197	1.651584
-82.255526	-0.116115	1.656589
-82.524382	14.754619	1.661594
-82.478177	9.172934	1.666598
-82.970068	4.367252	1.671603
-83.353852	1.799338	1.676608
-83.438121	10.948391	1.681613
-83.965911	4.983635	1.686618
-84.138064	-6.286664	1.691622
-84.869741	14.418314	1.696627
-85.310674	-1.811080	1.701632
-85.262922	12.931170	1.706637
-85.612577	10.703960	1.711642
-85.173245	-4.313747	1.716646
-85.495285	1.427720	1.721651
-85.413500	10.901001	1.726656
-85.457133	-6.076878	1.731661
-86.458102	16.842520	1.736666
-86.668983	6.782288	1.741670
-86.635450	-9.934696	1.746675
-87.189985	1.330784	1.751680
-88.066919	-1.151185	1.756685
-87.687370	-4.460510	1.761690
-87.870260	8.844806	1.766694
-88.205312	2.380221	1.771699
-88.535694	-3.816126	1.776704
-88.484172	8.723626	1.781709
-88.833985	-7.940756	1.786714
-89.015888	-9.540286	1.791718
-89.338102	3.179210	1.796723
-89.778779	-13.419642	1.801728
-89.769790	-5.082082	1.806733
-89.984743	24.559944	1.811738
-90.034846	-7.835801	1.816742
-91.363032	13.472237	1.821747
-91.852995	4.190480	1.826752
-91.532795	-16.167245	1.831757
-91.859257	4.911892	1.836762
-91.225339	-14.732391	1.841766
-91.806652	4.881758	1.846771
-91.806766	19.348416	1.851776
-91.851169	6.415133	1.856781
-92.443150	5.798908	1.861786
-92.674103	-8.319734	1.866790
-92.946630	16.928544	1.871795
-93.683550	8.918404	1.876800
-94.120095	1.720986	1.881805
-94.797880	7.565345	1.886810
-93.889187	0.360443	1.891814
-94.197023	2.484492	1.896819
-94.568104	6.569123	1.901824
-94.556319	-3.697375	1.906829
-95.259570	-4.282976	1.911834
-95.678488	-7.850675	1.916838
-96.193882	4.495809	1.921843
-96.266586	-3.547553	1.926848
-96.511888	2.167913	1.931853
-96.841432	0.473916	1.936858
-96.679516	-6.752864	1.941862
-96.389574	6.909822	1.946867
-96.688648	-0.724431	1.951872
-97.314592	2.254184	1.956877
-98.012645	7.858139	1.961882
-98.206720	-3.697668	1.966886
-98.152628	-2.079907	1.971891
-98.444809	3.792559	1.976896
-98.372031	-16.518254	1.981901
-98.940158	8.694721	1.986906
-99.583279	6.743985	1.991910
-99.634916	2.219583	1.996915
-99.808180	-2.397145	2.006912
-99.334150	0.080794	2.016909
-98.752127	3.246315	2.026906
-98.699653	6.704805	2.036902
-98.254518	2.778004	2.046899
-97.462410	-3.875160	2.056896
-96.769871	-4.153319	2.066893
-96.067811	3.204496	2.076890
-96.090517	-6.979330	2.086886
-95.580966	-1.402264	2.096883
-94.909362	3.516274	2.106880
-94.425556	1.752017	2.116877
-94.247151	-4.973654	2.126874
-93.138490	2.685282	2.136870
-92.679293	2.730350	2.146867
-92.552626	-9.998430	2.156864
-92.236330	-2.826851	2.166861
-91.604154	3.029426	2.176858
-90.830584	-4.579453	2.186854
-89.939916	-4.825761	2.196851
-89.964011	-10.349291	2.206848
-89.639320	-4.700584	2.216845
-89.031641	-0.715742	2.226842
-88.126944	-3.021986	2.236838
-88.001854	-10.798568	2.246835
-87.474802	-0.690661	2.256832
-87.005536	-13.960142	2.266829
-86.387399	3.287856	2.276826
-86.016182	-3.044470	2.286822
-85.294122	-6.740277	2.296819
-85.031897	3.092468	2.306816
-84.073888	-2.589233	2.316813
-83.728945	-2.032804	2.326810
-83.675307	-2.569343	2.336806
-82.808174	-7.062413	2.346803
-82.188767	-2.265232	2.356800
-81.991414	6.116904	2.366797
-81.625933	-7.812612	2.376794
-80.672530	14.613129	2.386790
-80.432361	-14.697401	2.396787
-80.122831	-3.634865	2.406784
-79.056560	-0.025390	2.416781
-78.779897	10.965645	2.426778
-78.847264	2.905188	2.436774
-77.744935	-5.585835	2.446771
-77.436205	-6.090751	2.456768
-76.592220	-7.753040	2.466765
-76.323735	-7.064262	2.476762
-75.771064	-5.985091	2.486758
-75.386712	-3.087955	2.496755
-75.241349	-4.480303	2.506752
-74.243939	-9.351174	2.516749
-73.955019	-12.762638	2.526746
-72.978885	-7.446203	2.536742
-72.462237	-5.161491	2.546739
-72.508358	-3.533448	2.556736
-72.216371	-9.350322	2.566733
-71.310338	-8.109684	2.576730
-70.951968	-2.598500	2.586726
-70.525674	-10.159365	2.596723
-69.607110	-6.789495	2.606720
-69.384656	4.510862	2.616717
-68.837164	-2.194719	2.626714
-68.091012	-3.595785	2.636710
-67.832663	-7.352839	2.646707
-67.668360	-2.262451	2.656704
-66.753817	8.823373	2.666701
-66.262690	-3.592192	2.676698
-66.054525	1.546952	2.686694
-65.403937	1.718525	2.696691
-64.628347	-12.609950	2.706688
-64.436934	-4.786181	2.716685
-63.926470	-0.127249	2.726682
-63.249289	-5.066092	2.736678
-62.990437	-7.975666	2.746675
-62.028071	1.351910	2.756672
-61.905098	-2.230761	2.766669
-61.835743	-9.943908	2.776666
-60.452217	-7.552670	2.786662
-60.013108	-15.306873	2.796659
-60.024373	0.970512	2.806656
-59.652693	-16.527571	2.816653
-58.844494	-16.273594	2.826650
-58.308884	-0.447308	2.836646
-57.688021	4.517057	2.846643
-56.916475	-0.112028	2.856640
-56.788273	-9.692903	2.866637
-56.879530	0.842159	2.876634
-55.565564	-6.422123	2.886630
-55.240112	-9.501233	2.896627
-55.006763	-13.719765	2.906624
-53.992516	1.803801	2.916621
-53.525556	-12.630023	2.926618
-53.411417	-3.457886	2.936614
-53.073820	-5.425349	2.946611
-52.143632	-7.052200	2.956608
-51.985164	-14.522772	2.966605
-51.423687	-12.594330	2.976602
-50.293070	-7.077727	2.986598
-49.972970	-8.427145	2.996595
-50.140541	-7.298177	3.006592
-49.775698	-1.614418	3.016589
-49.076519	2.091883	3.026586
-48.135982	-11.344878	3.036582
-47.431501	-19.179087	3.046579
-47.018303	-1.373821	3.056576
-46.957417	-7.760049	3.066573
-46.448821	-9.463604	3.076570
-45.783383	-18.888011	3.086566
-45.413806	-13.008285	3.096563
-44.568515	-6.813866	3.106560
-44.052902	-2.191440	3.116557
-44.058418	-12.532786	3.126554
-43.376297	-8.848360	3.136550
-42.391890	-1.088577	3.146547
-42.389166	-2.809572	3.156544
-42.256461	-15.041441	3.166541
-41.138443	5.181347	3.176538
-40.533291	1.429005	3.186534
-40.562156	-3.596030	3.196531
-39.693917	-8.470638	3.206528
-39.521821	1.801234	3.216525
-38.668396	-13.557852	3.226522
-38.083183	2.359215	3.236518
-37.761787	-2.836900	3.246515
-37.555612	-5.181780	3.256512
-36.518987	-7.413716	3.266509
-36.115965	4.106401	3.276506
-35.784416	1.759369	3.286502
-35.480807	-7.819285	3.296499
-34.874514	1.439432	3.306496
-34.295318	2.189463	3.316493
-33.352481	-11.090532	3.326490
-32.889870	-6.058233	3.336486
-32.719008	-4.458740	3.346483
-32.743963	-9.654012	3.356480
-31.679954	-9.518659	3.366477
-31.282448	-1.456136	3.376474
-30.949861	0.075244	3.386470
-30.102571	-10.722029	3.396467
-29.476717	-9.643687	3.406464
-29.607705	-0.653864	3.416461
-28.555431	10.254729	3.426458
-28.039853	-5.461202	3.436454
-27.922372	-6.123065	3.446451
-27.206483	-5.851457	3.456448
-26.503162	-15.956345	3.466445
-26.406551	2.213174	3.476442
-25.912515	4.433477	3.486438
-25.129760	-10.564972	3.496435
-24.699292	-3.810206	3.506432
-24.305477	2.834266	3.516429
-23.527530	-14.782228	3.526426
-23.293381	-15.352253	3.536422
-23.004735	4.169230	3.546419
-21.705227	-5.418743	3.556416
-21.408178	-6.940363	3.566413
-21.156302	0.175596	3.576410
-21.077408	3.617376	3.586406
-20.366661	-4.267855	3.596403
-19.254458	-12.113247	3.606400
-19.367096	0.405040	3.616397
-19.007693	-11.152745	3.626394
-18.224872	-7.973583	3.636390
-17.661376	-14.691680	3.646387
-17.011776	3.567602	3.656384
-16.250800	-4.597257	3.666381
-16.359020	-9.329158	3.676378
-16.280898	1.042006	3.686374
-15.105031	-9.194020	3.696371
-14.639944	-3.039483	3.706368
-14.316905	5.972304	3.716365
-13.777795	-5.037071	3.726362
-13.555487	4.039465	3.736358
-12.279346	-5.536349	3.746355
-11.759194	0.034730	3.756352
-11.854919	-11.479744	3.766349
-11.560199	-2.410931	3.776346
-10.573070	-2.331022	3.786342
-10.077173	-5.099709	3.796339
-9.961825	-10.826943	3.806336
-8.927534	-7.347783	3.816333
-8.545318	-0.024706	3.826330
-8.284660	1.810336	3.836326
-7.997138	-0.593127	3.846323
-7.224814	-3.182593	3.856320
-6.955212	-0.502355	3.866317
-5.745341	3.087355	3.876314
-5.402119	8.412005	3.886310
-5.115155	-2.733986	3.896307
-5.224961	1.961382	3.906304
-4.346822	11.145555	3.916301
-3.842636	12.477703	3.926298
-3.464804	21.663175	3.936294
-2.845518	22.926127	3.946291
-2.443434	37.590057	3.956288
-2.342342	56.668895	3.966285
-1.809381	55.353140	3.976282
-1.375741	94.496842	3.986278
-0.575683	111.984967	3.996275
0.000000	114.218154	4.001280
0.155932	116.193759	4.006285
0.565788	138.180591	4.011290
0.686723	134.404862	4.016294
0.646009	136.281866	4.021299
0.254857	134.044323	4.026304
0.682402	151.272913	4.031309
0.415544	145.354341	4.036314
0.540838	141.681370	4.041318
0.867347	152.269656	4.046323
0.682221	147.101202	4.051328
0.857954	133.771530	4.056333
0.659932	134.723773	4.061338
0.737607	110.880114	4.066342
0.529886	130.681974	4.071347
0.656145	124.908857	4.076352
0.699591	126.093164	4.081357
0.454177	120.266548	4.086362
0.877651	135.996538	4.091366
0.705884	147.323783	4.096371
1.003834	161.252438	4.101376
0.710545	127.337721	4.106381
0.609017	115.618544	4.111386
0.824295	140.443636	4.116390
0.831726	143.166595	4.121395
0.831652	146.400676	4.126400
0.950050	149.342716	4.131405
0.475410	139.752596	4.136410
1.142001	150.020034	4.141414
0.819572	147.159226	4.146419
0.671200	127.511428	4.151424
1.100380	136.193455	4.156429
0.607543	158.006944	4.161434
0.955533	160.007537	4.166438
0.807433	151.127984	4.171443
0.757307	147.140217	4.176448
0.859356	142.589876	4.181453
0.726359	146.925513	4.186458
1.091783	156.372736	4.191462
1.268150	154.221630	4.196467
0.902623	151.812250	4.201472
1.183930	164.442309	4.206477
0.857660	162.928664	4.211482
0.914111	143.769355	4.216486
0.943666	158.333453	4.221491
0.667774	148.533140	4.226496
0.704187	149.830970	4.231501
0.603733	170.345831	4.236506
0.756941	147.379626	4.241510
1.094440	146.748477	4.246515
1.222954	147.460808	4.251520
0.924635	146.083709	4.256525
1.082108	160.100784	4.261530
1.069408	177.672722	4.266534
1.019017	199.643369	4.271539
1.405827	173.174328	4.276544
1.630198	181.029139	4.281549
1.122700	171.386153	4.286554
1.467264	152.063803	4.291558
1.172229	145.071974	4.296563
1.302639	142.592474	4.301568
1.166723	145.281390	4.306573
1.280568	154.163806	4.311578
1.254560	132.800631	4.316582
1.129324	150.933028	4.321587
1.119925	163.822134	4.326592
1.514685	164.921061	4.331597
1.214036	155.891913	4.336602
1.258709	156.495088	4.341606
1.508796	164.358563	4.346611
1.660418	164.561906	4.351616
1.228680	145.868883	4.356621
1.104414	148.475774	4.361626
1.237618	170.194970	4.366630
1.529837	170.127376	4.371635
1.307272	183.667482	4.376640
1.488191	183.564419	4.381645
1.473083	175.076304	4.386650
1.934587	175.995613	4.391654
1.358427	179.021566	4.396659
1.300319	161.251571	4.401664
1.629120	163.576826	4.406669
1.528561	184.571345	4.411674
1.520886	181.751440	4.416678
1.451945	169.852823	4.421683
1.450495	179.643510	4.426688
1.793753	169.328223	4.431693
1.720471	190.202430	4.436698
1.900315	193.007563	4.441702
1.520939	166.215422	4.446707
1.247402	146.136802	4.451712
1.627229	165.708831	4.456717
1.302854	173.780394	4.461722
1.654547	175.283098	4.466726
1.551464	190.837269	4.471731
1.428897	183.202250	4.476736
1.757655	184.315341	4.481741
1.593317	192.371416	4.486746
1.661861	177.570465	4.491750
1.480041	171.544806	4.496755
1.328326	184.434168	4.501760
1.480396	169.262813	4.506765
1.488329	176.975529	4.511770
1.400914	181.247810	4.516774
1.454381	193.125778	4.521779
2.059582	192.273118	4.526784
2.247943	203.576378	4.531789
2.195064	215.260143	4.536794
1.687666	188.211527	4.541798
1.570943	188.015208	4.546803
1.373013	200.008219	4.551808
1.927120	198.624403	4.556813
1.708683	194.089227	4.561818
2.114462	191.591636	4.566822
2.108476	234.450629	4.571827
2.009885	231.377518	4.576832
2.555605	196.064094	4.581837
1.843158	193.144028	4.586842
1.908296	183.504654	4.591846
1.543157	189.449424	4.596851
1.784427	209.394998	4.601856
2.126473	203.474029	4.606861
2.099833	216.929206	4.611866
2.332435	198.577444	4.616870
2.133984	227.331901	4.621875
1.966006	220.778046	4.626880
2.031834	190.924558	4.631885
2.183011	210.330922	4.636890
2.326504	204.002799	4.641894
2.249717	194.727697	4.646899
2.082997	193.933947	4.651904
2.009150	185.635464	4.656909
2.077854	193.272940	4.661914
2.496059	181.533520	4.666918
2.218430	177.235711	4.671923
1.959908	190.948971	4.676928
2.225029	187.216382	4.681933
2.017492	209.931165	4.686938
2.402671	199.354025	4.691942
2.140183	190.004753	4.696947
2.272848	180.277276	4.701952
2.306546	189.842574	4.706957
2.169358	186.151611	4.711962
2.115410	196.898293	4.716966
2.470905	198.074145	4.721971
2.302215	219.431254	4.726976
2.168544	213.925285	4.731981
2.569595	209.328864	4.736986
2.487213	193.196145	4.741990
2.265712	189.470483	4.746995
2.401947	203.722731	4.752000
2.307652	198.932554	4.757005
2.385538	211.826414	4.762010
2.490811	212.295282	4.767014
2.580133	205.305901	4.772019
2.307806	207.670627	4.777024
2.405309	197.870032	4.782029
2.380663	200.956860	4.787034
2.637338	210.022765	4.792038
2.357223	218.435853	4.797043
2.373083	213.819238	4.802048
2.698040	214.305267	4.807053
2.568687	223.978916	4.812058
2.358726	211.712434	4.817062
2.352744	216.230413	4.822067
2.314561	219.702529	4.827072
2.514946	220.136048	4.832077
2.381734	228.948357	4.837082
2.618487	206.862987	4.842086
2.716571	217.266322	4.847091
2.076665	210.814039	4.852096
2.054754	220.299763	4.857101
2.276564	236.508773	4.862106
2.367842	210.902446	4.867110
2.395279	237.940224	4.872115
2.770792	242.328972	4.877120
2.988778	238.457866	4.882125
2.564535	256.003303	4.887130
2.768143	247.720392	4.892134
2.577470	250.632736	4.897139
2.574396	244.036625	4.902144
3.018610	264.128665	4.907149
2.805293	263.654732	4.912154
2.738600	248.030554	4.917158
2.820193	245.724339	4.922163
2.770555	241.953689	4.927168
3.174401	240.153550	4.932173
2.667158	248.644931	4.937178
2.780562	251.490156	4.942182
2.906677	253.602993	4.947187
2.868758	259.230423	4.952192
3.005478	243.679568	4.957197
2.755262	259.181573	4.962202
2.791827	252.262939	4.967206
2.676970	237.737279	4.972211
2.502986	260.725764	4.977216
2.591120	250.746257	4.982221
2.770364	251.905567	4.987226
2.996354	241.016543	4.992230
3.296528	252.540186	4.997235
2.970482	255.791661	5.002240
3.301065	231.462795	5.007245
2.773343	263.316979	5.012250
3.391540	263.224417	5.017254
3.282886	246.967347	5.022259
3.107059	256.455643	5.027264
3.330364	235.899022	5.032269
3.073657	246.859378	5.037274
2.954380	253.724959	5.042278
2.611094	246.362547	5.047283
2.835710	249.055429	5.052288
3.093758	230.805765	5.057293
3.061396	242.709005	5.062298
3.067374	265.204212	5.067302
3.275270	252.979719	5.072307
3.411142	260.117527	5.077312
3.126160	252.583399	5.082317
3.139610	245.866672	5.087322
3.383325	249.652864	5.092326
3.177058	254.788538	5.097331
3.003762	259.165492	5.102336
3.368381	245.241057	5.107341
3.083108	241.662054	5.112346
3.044094	244.476039	5.117350
3.231426	252.549396	5.122355
3.103185	245.843260	5.127360
3.152677	252.242068	5.132365
3.020782	265.128519	5.137370
3.126667	268.504233	5.142374
3.587550	262.065531	5.147379
3.249774	274.463675	5.152384
3.446219	278.951869	5.157389
3.440590	288.685214	5.162394
3.406589	266.653380	5.167398
3.511932	270.850623	5.172403
3.374869	279.745377	5.177408
3.751395	263.116703	5.182413
3.587923	288.704927	5.187418
3.490177	277.962007	5.192422
3.223697	268.588981	5.197427
3.026945	266.017234	5.202432
3.580484	262.946140	5.207437
3.496991	277.566718	5.212442
3.750204	270.795855	5.217446
3.665072	275.441758	5.222451
3.498561	281.037276	5.227456
3.873246	281.892121	5.232461
3.516176	283.911391	5.237466
3.688971	262.896873	5.242470
3.852700	280.536941	5.247475
3.539272	255.085711	5.252480
3.518435	265.500052	5.257485
3.552394	286.488955	5.262490
3.648805	265.885395	5.267494
3.747815	276.164125	5.272499
3.746436	289.999917	5.277504
3.971163	260.902408	5.282509
3.543944	260.910205	5.287514
3.635039	261.138349	5.292518
3.588087	281.091203	5.297523
3.343915	276.573278	5.302528
3.740838	269.290460	5.307533
3.751404	271.416871	5.312538
3.831430	272.124299	5.317542
3.670446	267.747900	5.322547
3.671194	278.361008	5.327552
3.903753	280.203029	5.332557
3.633761	279.985278	5.337562
3.834306	268.039188	5.342566
3.844320	268.445572	5.347571
3.543418	289.184602	5.352576
3.946734	277.007996	5.357581
3.917987	285.669999	5.362586
3.614199	286.821143	5.367590
3.697923	275.218214	5.372595
3.894368	275.872961	5.377600
4.036803	282.970138	5.382605
3.707961	271.608223	5.387610
3.920178	285.742635	5.392614
3.682291	279.686739	5.397619
3.848920	305.711606	5.402624
4.077137	323.717210	5.407629
3.969697	309.132646	5.412634
4.091504	300.205836	5.417638
4.262906	304.622613	5.422643
4.064733	319.536621	5.427648
3.822256	316.281393	5.432653
3.870097	315.280924	5.437658
4.191984	320.421869	5.442662
3.978901	303.937448	5.447667
4.057620	292.570114	5.452672
4.240336	314.985581	5.457677
3.953285	331.349122	5.462682
3.831104	300.764533	5.467686
4.017664	319.911368	5.472691
3.868385	307.703045	5.477696
4.242764	301.675285	5.482701
4.217816	304.900291	5.487706
4.252318	294.081939	5.492710
4.084661	308.759663	5.497715
3.972345	322.009009	5.502720
4.010410	309.942555	5.507725
4.231573	296.468827	5.512730
4.119120	312.800239	5.517734
4.286267	322.705604	5.522739
4.713674	319.712658	5.527744
4.308858	315.803488	5.532749
4.364473	313.246946	5.537754
4.293335	304.675092	5.542758
4.215658	320.387077	5.547763
4.291986	308.489499	5.552768
4.653943	336.618950	5.557773
3.825360	327.240428	5.562778
4.541779	317.616353	5.567782
4.747719	338.708798	5.572787
4.641208	340.285959	5.577792
4.826896	304.850172	5.582797
4.454514	321.759615	5.587802
4.540832	315.170008	5.592806
4.535227	295.476919	5.597811
4.261608	316.405911	5.602816
4.604926	289.078322	5.607821
4.456380	292.689142	5.612826
4.381435	313.525813	5.617830
4.323971	318.098497	5.622835
4.511519	312.109796	5.627840
4.505209	323.514469	5.632845
4.407117	335.336111	5.637850
4.580451	323.091133	5.642854
4.633254	341.406992	5.647859
4.367225	330.389588	5.652864
4.724531	333.619792	5.657869
4.542059	346.466234	5.662874
5.319583	327.642396	5.667878
4.760700	338.657095	5.672883
4.404312	325.262906	5.677888
4.519157	310.271380	5.682893
4.606889	331.570387	5.687898
4.506370	350.263867	5.692902
4.502035	349.091690	5.697907
4.460430	335.067296	5.702912
4.655941	341.611290	5.707917
4.438987	339.617296	5.712922
4.500454	328.192118	5.717926
4.780059	336.703261	5.722931
4.684627	334.272496	5.727936
5.018814	346.336310	5.732941
4.503184	346.763766	5.737946
4.989998	320.846650	5.742950
5.027579	343.378576	5.747955
4.559141	341.305693	5.752960
4.709197	331.744723	5.757965
5.071919	361.910385	5.762970
4.793988	350.397254	5.767974
4.935155	348.554788	5.772979
4.923789	374.328928	5.777984
5.110083	366.406513	5.782989
4.877770	355.417749	5.787994
4.743311	362.922564	5.792998
4.877007	358.343943	5.798003
5.103858	379.379028	5.803008
5.193010	370.732309	5.808013
5.035091	368.418504	5.813018
5.069142	372.019193	5.818022
4.891102	378.150043	5.823027
4.747387	364.219146	5.828032
5.052291	370.815312	5.833037
4.991049	379.516180	5.838042
4.654793	361.813128	5.843046
4.610333	389.172119	5.848051
4.807429	391.078612	5.853056
5.052214	371.842613	5.858061
4.950160	389.030332	5.863066
5.074098	384.221690	5.868070
5.447609	369.290644	5.873075
5.088382	383.197694	5.878080
5.672962	374.633644	5.883085
5.229168	383.775558	5.888090
5.085136	385.978436	5.893094
5.348787	367.869144	5.898099
5.308131	360.392148	5.903104
5.236095	381.931103	5.908109
5.335182	386.345846	5.913114
5.416178	385.264329	5.918118
5.475011	372.401360	5.923123
5.087792	375.051053	5.928128
5.663290	360.441375	5.933133
5.309285	386.561100	5.938138
5.339713	368.816481	5.943142
5.710583	374.180779	5.948147
5.193600	375.376731	5.953152
5.277207	370.339778	5.958157
5.419722	366.137126	5.963162
5.355229	381.358390	5.968166
5.071821	385.491075	5.973171
5.249148	362.085818	5.978176
5.288173	378.914313	5.983181
5.271583	364.683824	5.988186
5.403316	380.010963	5.993190
5.355234	399.759168	5.998195
5.776335	393.227351	6.003200
5.705363	392.709667	6.008205
5.313091	403.972403	6.013210
5.217484	378.805873	6.018214
5.382835	398.781998	6.023219
5.802205	392.636281	6.028224
5.776072	399.893855	6.033229
5.507550	389.456675	6.038234
5.415993	375.403505	6.043238
5.442213	384.480470	6.048243
5.222674	400.457078	6.053248
5.669362	383.907238	6.058253
5.408387	388.551357	6.063258
5.477385	399.260107	6.068262
5.565918	385.162961	6.073267
5.188595	406.042133	6.078272
5.560382	412.572021	6.083277
5.880517	404.719704	6.088282
5.478121	402.250972	6.093286
5.523741	391.517524	6.098291
5.361323	390.588791	6.103296
5.478181	392.036314	6.108301
5.206753	376.738627	6.113306
5.031081	399.406302	6.118310
5.787855	414.900578	6.123315
5.682160	420.352921	6.128320
5.741469	401.657057	6.133325
5.759876	410.751705	6.138330
5.788190	390.139798	6.143334
5.592054	370.337624	6.148339
4.989367	385.744904	6.153344
5.522687	387.760279	6.158349
5.594841	373.881397	6.163354
5.612458	390.561327	6.168358
5.612591	379.745141	6.173363
5.513091	383.477797	6.178368
5.585864	384.633405	6.183373
5.518911	371.956657	6.188378
5.464959	366.735178	6.193382
5.585323	382.357875	6.198387
5.129597	378.910786	6.203392
5.417309	385.682040	6.208397
5.287590	373.225093	6.213402
5.166573	386.239078	6.218406
5.753940	385.592374	6.223411
5.379950	409.727875	6.228416
5.615707	400.657878	6.233421
5.680817	418.535869	6.238426
5.384152	403.779467	6.243430
5.612662	388.759413	6.248435
5.360330	401.071723	6.253440
5.609315	388.890938	6.258445
5.614682	386.756123	6.263450
5.368962	388.092114	6.268454
5.587437	382.206196	6.273459
5.402487	386.346680	6.278464
5.396151	387.887463	6.283469
5.345874	393.069911	6.288474
5.544128	399.613871	6.293478
5.803037	404.662363	6.298483
5.596146	398.600014	6.303488
5.709809	360.163379	6.308493
5.502640	375.287372	6.313498
4.983275	375.301221	6.318502
5.121463	371.903562	6.323507
5.302073	402.943534	6.328512
6.023925	396.277768	6.333517
5.861953	401.382002	6.338522
5.252206	383.399174	6.343526
5.309422	389.597098	6.348531
5.405857	396.750761	6.353536
5.647631	389.426642	6.358541
5.731994	418.385189	6.363546
5.911249	397.809193	6.368550
5.904748	396.724675	6.373555
5.487927	378.095785	6.378560
5.458065	360.653533	6.383565
5.539740	374.837025	6.388570
5.508974	373.140855	6.393574
5.624540	373.351541	6.398579
5.532816	380.635235	6.403584
5.580766	381.705471	6.408589
5.420119	370.426763	6.413594
5.179947	372.942459	6.418598
5.108662	369.385278	6.423603
5.234058	367.798744	6.428608
5.484671	383.180918	6.433613
5.437936	368.302849	6.438618
5.408611	391.895520	6.443622
5.628796	402.906701	6.448627
5.319088	381.716259	6.453632
5.414124	371.182609	6.458637
5.552977	407.349828	6.463642
5.639639	390.975686	6.468646
5.550468	384.807572	6.473651
5.082335	389.937835	6.478656
5.302194	390.261304	6.483661
5.758694	411.875035	6.488666
5.665812	413.247623	6.493670
5.717198	419.014837	6.498675
5.598970	400.328881	6.503680
5.523603	385.705403	6.508685
5.274194	387.839970	6.513690
5.319519	377.873177	6.518694
5.447940	402.690163	6.523699
5.457699	417.221872	6.528704
5.530068	402.696385	6.533709
5.291843	394.913461	6.538714
5.189459	412.599534	6.543718
5.421463	384.617683	6.548723
5.673802	409.205067	6.553728
5.783772	415.976704	6.558733
5.508109	401.984911	6.563738
5.472722	412.719404	6.568742
5.584342	409.325634	6.573747
5.330475	406.393567	6.578752
5.844932	402.809027	6.583757
5.592269	417.220446	6.588762
5.531794	404.312552	6.593766
5.802156	387.535362	6.598771
5.236759	405.861522	6.603776
5.488383	377.542220	6.608781
5.244676	384.774482	6.613786
5.685784	403.513370	6.618790
5.568921	406.399242	6.623795
5.431641	391.022747	6.628800
5.661133	375.153873	6.633805
5.390295	367.586571	6.638810
5.279085	386.187850	6.643814
5.548400	378.024621	6.648819
5.495131	408.826350	6.653824
5.631121	398.215873	6.658829
5.368219	391.723700	6.663834
5.270712	407.451185	6.668838
5.789889	409.811901	6.673843
5.492665	394.944325	6.678848
5.779481	398.920531	6.683853
5.276797	382.923658	6.688858
5.298845	375.958240	6.693862
5.642982	408.409886	6.698867
5.493681	406.774437	6.703872
5.480933	376.179701	6.708877
5.321704	387.671052	6.713882
5.632040	394.346236	6.718886
5.845481	389.058957	6.723891
5.310120	392.224700	6.728896
5.534774	383.685205	6.733901
5.217564	378.334298	6.738906
5.503881	406.066591	6.743910
5.669991	400.296058	6.748915
5.502437	383.828097	6.753920
5.683831	382.054741	6.758925
5.584182	397.832585	6.763930
5.462730	380.517806	6.768934
5.493364	390.893145	6.773939
4.995871	388.756003	6.778944
5.482364	381.536656	6.783949
5.810679	405.694689	6.788954
5.590721	411.123987	6.793958
5.349641	384.666011	6.798963
5.399962	410.255903	6.803968
5.675498	405.445877	6.808973
5.447815	374.342125	6.813978
5.419175	369.105711	6.818982
5.612862	378.095906	6.823987
5.474681	401.461342	6.828992
5.496537	381.370983	6.833997
5.532630	373.571147	6.839002
5.615325	387.487738	6.844006
5.628060	383.772050	6.849011
5.541963	393.392588	6.854016
5.333388	372.311814	6.859021
5.353861	380.192630	6.864026
5.636029	380.348261	6.869030
5.501439	368.244002	6.874035
5.395534	364.750450	6.879040
5.611303	370.631054	6.884045
5.229574	377.421291	6.889050
5.336554	386.168842	6.894054
5.702772	396.662544	6.899059
5.661196	395.371531	6.904064
5.507387	394.497802	6.909069
5.510307	382.653534	6.914074
5.344222	383.766441	6.919078
5.664896	386.597068	6.924083
5.293831	374.674826	6.929088
5.356862	380.368482	6.934093
5.565943	397.340937	6.939098
5.711833	395.372106	6.944102
5.739001	378.414143	6.949107
5.117348	385.819548	6.954112
5.480687	381.187384	6.959117
5.704775	367.116782	6.964122
5.620247	383.305054	6.969126
5.372497	392.828996	6.974131
5.206213	398.716913	6.979136
5.659619	383.488543	6.984141
5.465976	398.244535	6.989146
5.240746	388.343360	6.994150
5.640340	377.977881	6.999155
5.216656	400.097613	7.004160
5.264383	395.755147	7.009165
5.406246	406.595689	7.014170
5.576655	427.215486	7.019174
5.964871	404.062381	7.024179
5.415141	399.288316	7.029184
5.635105	400.728961	7.034189
5.784489	402.730842	7.039194
5.353807	387.854056	7.044198
5.491589	382.515654	7.049203
5.506825	380.122921	7.054208
5.263898	392.880645	7.059213
5.370154	387.071868	7.064218
5.635727	406.620669	7.069222
5.686983	387.668088	7.074227
5.601749	393.425317	7.079232
5.741564	380.534752	7.084237
5.792163	369.603890	7.089242
5.550397	378.366750	7.094246
5.401676	376.493467	7.099251
5.681629	399.491388	7.104256
5.695308	370.707032	7.109261
5.570939	384.325789	7.114266
5.394576	378.970842	7.119270
5.624799	373.812392	7.124275
5.325900	387.040246	7.129280
5.568827	386.592912	7.134285
5.716423	378.524967	7.139290
5.706409	391.069394	7.144294
5.553057	380.237437	7.149299
5.303353	370.679470	7.154304
5.453007	372.271813	7.159309
5.564849	388.347437	7.164314
5.363008	384.216781	7.169318
5.573054	360.115089	7.174323
5.422433	370.382852	7.179328
5.606347	374.373591	7.184333
5.597319	362.423292	7.189338
5.488438	381.646454	7.194342
5.664210	380.404459	7.199347
5.425059	383.926496	7.204352
5.357307	384.601234	7.209357
5.394472	371.663322	7.214362
5.517722	365.661748	7.219366
5.439431	367.927943	7.224371
5.606715	377.947358	7.229376
5.594803	370.046845	7.234381
5.487320	380.763241	7.239386
5.270684	375.410709	7.244390
5.803061	373.744686	7.249395
5.275482	365.758042	7.254400
5.588955	380.136930	7.259405
5.479728	383.274371	7.264410
5.462389	379.443106	7.269414
5.554519	379.701169	7.274419
5.496710	372.977025	7.279424
5.269544	381.023457	7.284429
5.462175	394.487932	7.289434
5.506976	375.411348	7.294438
5.578822	361.040470	7.299443
5.444524	381.078325	7.304448
5.345085	368.107748	7.309453
5.613589	372.034887	7.314458
5.356503	392.190709	7.319462
5.596206	368.835901	7.324467
5.236615	379.780109	7.329472
5.318261	386.978432	7.334477
5.610224	373.891081	7.339482
5.408486	380.147581	7.344486
5.490434	374.750045	7.349491
5.442874	385.081284	7.354496
5.649869	367.837919	7.359501
5.424319	387.490251	7.364506
5.579050	385.542550	7.369510
5.818960	374.972921	7.374515
5.119879	367.117410	7.379520
5.427529	379.458498	7.384525
5.522015	385.412618	7.389530
5.605795	381.391612	7.394534
5.603194	368.647016	7.399539
5.432907	379.322197	7.404544
5.356957	365.582230	7.409549
5.423380	386.262266	7.414554
5.342893	378.438288	7.419558
5.464778	370.990852	7.424563
5.409577	389.385780	7.429568
5.574190	373.104329	7.434573
5.344927	386.883364	7.439578
5.313797	384.779933	7.444582
5.428361	369.575908	7.449587
5.504368	398.735955	7.454592
5.583685	392.213172	7.459597
5.476922	380.436059	7.464602
5.400990	402.128788	7.469606
5.590198	395.541675	7.474611
5.373034	399.615177	7.479616
5.626748	409.979114	7.484621
5.678747	391.176943	7.489626
5.268029	391.415118	7.494630
5.552900	385.878490	7.499635
5.498080	410.405263	7.504640
5.510151	376.068438	7.509645
5.932659	394.239807	7.514650
5.381891	399.663397	7.519654
5.563508	373.271623	7.524659
5.525258	382.595208	7.529664
5.372661	387.872101	7.534669
5.620236	366.964742	7.539674
5.468567	370.516316	7.544678
5.609985	383.947024	7.549683
5.343534	381.554181	7.554688
5.527346	385.699620	7.559693
5.582840	382.048485	7.564698
5.560962	386.692451	7.569702
5.555961	376.944392	7.574707
5.539553	379.688572	7.579712
5.445031	383.866789	7.584717
5.527748	377.303004	7.589722
5.399628	379.035461	7.594726
5.666473	400.172479	7.599731
5.508908	382.626318	7.604736
5.379798	390.333280	7.609741
5.516268	380.593111	7.614746
5.432937	366.215812	7.619750
5.317207	369.622156	7.624755
5.276982	388.326631	7.629760
5.504848	389.616321	7.634765
5.383932	373.086802	7.639770
5.446471	374.733099	7.644774
5.650867	384.109413	7.649779
5.666278	395.506999	7.654784
5.611716	376.196464	7.659789
5.709860	380.759629	7.664794
5.842460	396.052016	7.669798
6.030921	380.694799	7.674803
5.597158	369.528209	7.679808
5.632237	378.280042	7.684813
5.726128	373.953531	7.689818
5.434279	384.485345	7.694822
5.714237	386.712561	7.699827
5.335171	397.773742	7.704832
5.866170	392.445524	7.709837
5.847394	381.206695	7.714842
5.468315	372.161870	7.719846
5.633051	362.402737	7.724851
5.453419	354.332259	7.729856
5.261212	353.815079	7.734861
5.345029	386.795639	7.739866
5.463130	379.331561	7.744870
5.784592	375.537332	7.749875
5.535726	381.639541	7.754880
5.546679	369.123739	7.759885
5.660683	347.741984	7.764890
5.160690	364.087579	7.769894
5.646847	374.947358	7.774899
5.389572	365.998714	7.779904
5.419761	365.868178	7.784909
5.486058	372.362611	7.789914
5.015058	391.740923	7.794918
5.661742	389.069425	7.799923
5.468290	385.965693	7.804928
5.309169	387.710673	7.809933
5.323205	370.842094	7.814938
5.270092	372.016532	7.819942
5.352827	382.038381	7.824947
5.113756	390.872519	7.829952
5.655740	368.897664	7.834957
5.668914	389.434980	7.839962
5.679303	382.566090	7.844966
5.689468	381.786897	7.849971
5.604023	384.987687	7.854976
5.850904	370.245072	7.859981
5.857462	373.653008	7.864986
5.712044	395.525603	7.869990
5.491216	360.424403	7.874995
5.316078	359.283116	7.880000
5.539877	349.801691	7.885005
5.632448	367.283056	7.890010
5.518823	349.928151	7.895014
5.222758	357.584953	7.900019
5.349589	371.714320	7.905024
5.361875	373.789262	7.910029
5.706737	355.306005	7.915034
5.228261	376.746194	7.920038
5.528877	373.867808	7.925043
5.554815	394.233544	7.930048
5.607696	379.845462	7.935053
5.600430	386.308949	7.940058
5.680225	382.575273	7.945062
5.829876	353.185172	7.950067
5.373796	355.705768	7.955072
5.403148	346.939716	7.960077
5.691702	341.252056	7.965082
5.449300	367.911260	7.970086
5.383962	348.954320	7.975091
5.331525	348.785255	7.980096
5.495137	361.812948	7.985101
5.647340	365.612023	7.990106
5.045043	346.247426	7.995110
5.713969	376.324042	8.000115
5.582062	376.541507	8.005133
5.567526	368.228644	8.010150
5.480777	372.460290	8.015168
5.413675	362.537297	8.020186
5.485457	369.058309	8.025203
5.472800	376.059875	8.030221
5.505536	364.948281	8.035238
5.713647	381.909178	8.040256
5.255515	379.424740	8.045274
5.576530	378.583959	8.050291
5.382846	390.615474	8.055309
5.304592	381.020004	8.060326
5.609610	386.256286	8.065344
5.576566	394.832035	8.070362
5.684722	365.996771	8.075379
5.103850	389.522805	8.080397
5.132204	390.149171	8.085414
5.308116	374.640864	8.090432
5.750819	398.457170	8.095450
5.568010	382.857098	8.100467
5.786886	364.706245	8.105485
6.041667	382.649497	8.110502
5.844315	381.118327	8.115520
5.701507	373.100693	8.120538
5.540292	379.908273	8.125555
5.641894	376.298858	8.130573
5.694182	359.461684	8.135590
5.539482	362.452954	8.140608
5.485868	386.581905	8.145626
5.358509	384.153892	8.150643
5.752363	381.291716	8.155661
5.478904	386.416274	8.160678
5.749775	393.681730	8.165696
5.305977	396.245428	8.170714
5.604464	397.674544	8.175731
5.581240	388.822219	8.180749
5.437127	376.410896	8.185766
5.524380	381.476826	8.190784
5.278571	400.790937	8.195802
5.611129	397.437752	8.200819
5.599601	418.023714	8.205837
6.005721	410.597925	8.210854
6.011362	404.215205	8.215872
5.387471	403.061324	8.220890
5.800497	389.633480	8.225907
5.788929	392.116498	8.230925
5.478982	391.984145	8.235942
5.953691	385.469699	8.240960
5.623725	407.701608	8.245978
5.457648	402.120962	8.250995
6.051316	397.311846	8.256013
5.957234	409.785936	8.261030
5.898420	410.884942	8.266048
5.660236	395.381778	8.271066
5.900897	381.824696	8.276083
5.844335	390.663506	8.281101
5.784850	374.616217	8.286118
6.005335	385.892474	8.291136
5.700012	398.510095	8.296154
5.560533	382.899714	8.301171
5.844277	396.470171	8.306189
5.558924	393.168626	8.311206
5.845603	396.558281	8.316224
5.956997	403.922024	8.321242
5.853989	416.538696	8.326259
5.730958	400.860833	8.331277
5.555417	397.829048	8.336294
6.066728	405.959335	8.341312
5.508894	401.267701	8.346330
5.748529	416.031245	8.351347
5.692260	426.019204	8.356365
5.595652	413.005093	8.361382
5.723981	411.917493	8.366400
5.598980	425.673307	8.371418
5.622022	402.802398	8.376435
5.818523	406.763982	8.381453
5.631112	423.627246	8.386470
5.907066	402.160977	8.391488
5.672259	427.109176	8.396506
5.747549	416.844793	8.401523
5.692408	410.784821	8.406541
6.025469	429.295240	8.411558
5.921205	421.827647	8.416576
5.858932	418.288992	8.421594
5.931061	426.515288	8.426611
5.893850	444.273075	8.431629
5.790098	441.126888	8.436646
5.940009	449.083329	8.441664
5.797529	437.699936	8.446682
5.998594	443.987275	8.451699
6.006161	458.265247	8.456717
5.682537	450.176007	8.461734
5.814284	438.174231	8.466752
6.068676	457.663845	8.471770
5.929851	451.895068	8.476787
5.742867	460.784400	8.481805
5.868310	439.214348	8.486822
6.428362	442.643654	8.491840
5.907194	448.993477	8.496858
5.747013	435.433122	8.501875
6.008489	446.420349	8.506893
5.906727	456.191500	8.511910
6.015400	437.726486	8.516928
5.937231	440.110412	8.521946
5.888720	453.958108	8.526963
6.200164	443.085257	8.531981
6.145902	434.420364	8.536998
6.497781	445.450213	8.542016
6.089922	442.310889	8.547034
6.063802	449.953802	8.552051
5.987066	459.726822	8.557069
6.042813	458.678766	8.562087
6.379246	448.183169	8.567104
6.130915	453.790269	8.572122
6.094295	434.963947	8.577139
6.372279	440.056135	8.582157
6.074827	444.888504	8.587175
6.289362	454.027725	8.592192
6.017065	452.293050	8.597210
6.056432	455.989359	8.602227
6.368505	461.691002	8.607245
6.109479	452.274040	8.612263
6.216405	454.300406	8.617280
6.214179	441.037374	8.622298
6.201949	438.468904	8.627315
6.369525	455.348517	8.632333
5.945223	446.851531	8.637351
6.200824	444.753022	8.642368
6.087527	463.079348	8.647386
6.208163	444.332212	8.652403
6.285298	441.150818	8.657421
6.264719	438.487103	8.662439
6.217808	425.693639	8.667456
6.242227	443.753848	8.672474
6.299972	448.920713	8.677491
6.461417	431.115397	8.682509
6.534473	456.738051	8.687527
6.092595	419.425952	8.692544
5.999739	431.636941	8.697562
5.868886	429.403439	8.702579
6.185846	424.513603	8.707597
6.106629	444.097987	8.712615
6.469792	454.282025	8.717632
6.237910	441.658152	8.722650
6.200282	428.819366	8.727667
6.254188	436.616716	8.732685
6.434801	447.444325	8.737703
6.261924	433.046055	8.742720
6.394385	455.651386	8.747738
6.472711	455.126122	8.752755
6.357381	441.162203	8.757773
6.280410	452.883617	8.762791
6.258377	446.369666	8.767808
6.088254	442.775031	8.772826
6.332125	427.220902	8.777843
6.596887	444.063188	8.782861
6.691313	443.999008	8.787879
6.545945	434.124030	8.792896
6.277641	442.907140	8.797914
6.373408	452.919583	8.802931
6.396159	428.577844	8.807949
6.256475	453.108709	8.812967
6.406485	441.477427	8.817984
6.249250	440.978694	8.823002
6.390704	453.462503	8.828019
6.502672	436.697444	8.833037
6.571834	453.244403	8.838055
6.517354	439.809252	8.843072
6.295021	427.375588	8.848090
6.223540	449.258826	8.853107
6.564639	436.154354	8.858125
6.402172	440.715863	8.863143
6.069724	444.402572	8.868160
6.149052	450.962912	8.873178
6.134514	450.937207	8.878195
6.520534	456.122243	8.883213
6.135234	455.128084	8.888231
6.127003	449.051390	8.893248
6.280492	444.894267	8.898266
6.095021	429.183693	8.903283
6.267829	448.332254	8.908301
6.096103	468.516140	8.913319
6.498949	476.567272	8.918336
6.536422	492.057016	8.923354
6.720187	485.682414	8.928371
6.736466	465.728730	8.933389
6.651107	467.854375	8.938407
6.452767	466.543868	8.943424
6.907216	466.512783	8.948442
6.649683	449.417153	8.953459
6.329543	442.102514	8.958477
6.225881	453.477554	8.963495
6.262825	449.691853	8.968512
6.497019	465.689653	8.973530
6.373077	483.574976	8.978547
6.677463	470.015353	8.983565
6.679501	473.870844	8.988583
6.566076	465.943555	8.993600
6.514116	458.568550	8.998618
6.356558	485.644708	9.003635
6.893425	457.605992	9.008653
6.460812	477.313368	9.013671
6.647187	486.103033	9.018688
6.990514	483.325445	9.023706
6.782159	470.104620	9.028723
6.763987	480.364290	9.033741
6.534824	481.464000	9.038759
6.658682	474.723720	9.043776
6.733193	474.562762	9.048794
6.676467	472.179050	9.053811
6.884334	484.411821	9.058829
6.747028	479.208468	9.063847
6.621060	455.872087	9.068864
6.781316	442.418568	9.073882
6.793583	454.355190	9.078899
6.527585	438.933131	9.083917
6.813027	455.031180	9.088935
6.439371	456.149945	9.093952
6.744108	464.363699	9.098970
6.865684	473.508455	9.103987
6.688411	471.824984	9.109005
7.156413	475.796820	9.114023
6.713638	454.818047	9.119040
6.809805	440.962935	9.124058
6.676118	458.955420	9.129075
6.750107	450.344302	9.134093
6.726876	446.599344	9.139111
6.765041	433.636740	9.144128
6.841957	436.203441	9.149146
6.521778	457.306373	9.154163
6.613111	472.763285	9.159181
6.942756	480.837538	9.164199
6.906109	455.678641	9.169216
6.888822	474.793708	9.174234
6.748295	472.559732	9.179251
7.040404	466.131712	9.184269
6.704528	476.921602	9.189287
6.729755	469.859629	9.194304
6.902403	457.386742	9.199322
6.622590	471.498795	9.204339
6.945856	471.394829	9.209357
6.891046	477.261115	9.214375
6.692392	485.029677	9.219392
6.594406	480.475939	9.224410
6.579753	497.511957	9.229427
6.987045	485.127301	9.234445
7.041148	483.703834	9.239463
6.658855	481.019497	9.244480
6.988735	483.002429	9.249498
6.777020	478.377355	9.254515
6.652087	462.712731	9.259533
6.895676	481.045435	9.264551
6.848403	479.314995	9.269568
6.848437	487.482097	9.274586
6.779126	479.629869	9.279603
6.771828	487.115896	9.284621
6.892508	477.544757	9.289639
6.906560	485.501037	9.294656
6.714083	462.243040	9.299674
6.689162	474.762037	9.304691
6.933586	499.158750	9.309709
6.920556	520.427877	9.314727
6.853037	504.762381	9.319744
7.012431	519.063435	9.324762
7.079745	506.545532	9.329779
7.272787	494.718273	9.334797
7.053753	515.203165	9.339815
6.963512	505.605859	9.344832
7.124656	513.430789	9.349850
7.340565	516.347362	9.354867
7.034365	489.502635	9.359885
7.169498	494.040168	9.364903
6.457981	486.718554	9.369920
7.294865	490.364154	9.374938
6.928444	511.108566	9.379955
7.263348	499.745518	9.384973
7.066650	505.505968	9.389991
7.206441	517.325332	9.395008
7.144432	522.945649	9.400026
7.107528	510.921800	9.405043
7.129074	497.009992	9.410061
7.249380	513.496314	9.415079
6.783427	508.517590	9.420096
7.173921	496.411706	9.425114
7.108134	515.084769	9.430131
6.982175	516.588960	9.435149
7.581018	506.494912	9.440167
7.174296	518.517749	9.445184
7.172257	500.190214	9.450202
7.020685	514.053815	9.455219
6.986703	528.511011	9.460237
7.253918	521.563313	9.465255
6.956399	516.298851	9.470272
7.321696	520.065687	9.475290
7.157601	505.105918	9.480307
7.090469	507.017198	9.485325
7.439055	519.852845	9.490343
7.230249	526.113884	9.495360
7.385448	516.181998	9.500378
7.259758	528.747505	9.505395
7.209700	526.457343	9.510413
7.485680	513.559082	9.515431
7.449702	511.922611	9.520448
7.595262	523.603367	9.525466
7.488617	512.732060	9.530483
7.282158	488.351158	9.535501
7.360365	467.295126	9.540519
7.276374	473.401992	9.545536
7.005350	489.172964	9.550554
7.273864	490.771367	9.555571
7.378359	492.658317	9.560589
7.273748	490.176542	9.565607
7.025037	495.082443	9.570624
7.505939	496.397589	9.575642
7.623805	509.572058	9.580659
7.090618	505.449089	9.585677
7.208285	516.056703	9.590695
7.146055	529.022138	9.595712
7.440969	501.457164	9.600730
7.351295	525.732116	9.605747
7.211704	519.530786	9.610765
7.589607	508.340594	9.615783
7.498693	524.616825	9.620800
7.732256	516.400539	9.625818
7.591600	515.953969	9.630835
7.194396	500.807888	9.635853
7.385346	528.159010	9.640871
7.105011	519.481445	9.645888
7.242657	505.871121	9.650906
7.609499	510.484901	9.655923
7.221832	508.293435	9.660941
7.420493	505.478942	9.665959
7.374120	524.372859	9.670976
7.623227	518.733199	9.675994
7.574896	510.320952	9.681011
7.263580	518.948169	9.686029
7.354498	515.595927	9.691047
7.418365	510.213592	9.696064
7.532102	508.931701	9.701082
7.627138	509.217912	9.706099
7.474889	508.811633	9.711117
7.749393	508.665346	9.716135
7.592688	507.042627	9.721152
7.574154	514.664935	9.726170
7.559583	522.972423	9.731187
7.506964	507.673649	9.736205
7.513861	522.012010	9.741223
7.347508	524.492586	9.746240
7.512915	508.652705	9.751258
7.601095	510.724488	9.756275
7.389602	530.297089	9.761293
7.541424	523.886916	9.766311
7.366719	513.532324	9.771328
7.731838	523.306064	9.776346
7.535175	501.608398	9.781363
7.517254	508.300844	9.786381
7.445135	519.680167	9.791399
7.694767	513.563096	9.796416
7.816142	523.333231	9.801434
7.623469	530.641802	9.806451
7.767805	511.039825	9.811469
7.881910	513.342986	9.816487
7.443472	531.994112	9.821504
7.694864	522.254733	9.826522
7.663518	511.050895	9.831539
7.424363	519.957936	9.836557
7.438648	531.387536	9.841575
7.710261	528.928595	9.846592
7.619704	537.972757	9.851610
7.834480	542.607742	9.856627
7.768703	546.608377	9.861645
7.974226	542.000528	9.866663
7.813283	552.535640	9.871680
7.732708	558.564241	9.876698
7.687448	544.224183	9.881715
7.854073	553.943171	9.886733
7.865758	561.982144	9.891751
7.370387	559.830116	9.896768
7.576815	553.850251	9.901786
7.503266	552.420027	9.906803
7.546022	545.884306	9.911821
7.450287	549.709627	9.916839
7.657753	564.781303	9.921856
7.806907	556.997233	9.926874
7.942092	538.832453	9.931891
8.012539	540.050717	9.936909
7.675142	544.858035	9.941927
7.714911	545.077909	9.946944
8.038666	540.412834	9.951962
7.643147	530.359903	9.956979
7.741846	542.940984	9.961997
8.042694	546.534573	9.967015
7.991583	542.015480	9.972032
8.203903	550.053661	9.977050
8.361790	563.771804	9.982067
7.964847	552.051546	9.987085
8.201137	534.925181	9.992103
8.124026	541.439583	9.997120
7.834737	544.096537	10.002138
8.138442	544.955280	10.007155
7.904812	550.590096	10.012173
8.116674	542.432091	10.017191
8.045652	544.502440	10.022208
7.816713	548.763831	10.027226
8.064784	544.057539	10.032243
7.846959	548.370032	10.037261
7.846844	525.852965	10.042279
7.715673	537.483723	10.047296
7.804764	540.086214	10.052314
8.234392	545.484486	10.057331
8.093430	555.697982	10.062349
8.171786	538.876080	10.067367
8.050715	536.159486	10.072384
7.769760	534.154752	10.077402
8.193694	539.895600	10.082419
7.966332	548.460252	10.087437
8.068683	529.697732	10.092455
7.935368	530.874000	10.097472
7.961068	536.160331	10.102490
8.197018	530.062341	10.107507
7.915869	545.877947	10.112525
8.118800	544.880344	10.117543
8.091215	533.393761	10.122560
7.762916	547.677533	10.127578
8.198852	558.176197	10.132595
8.314903	556.256991	10.137613
8.220165	565.261418	10.142631
8.337648	571.050558	10.147648
8.097964	556.860795	10.152666
8.231830	541.331323	10.157683
8.173276	539.168412	10.162701
8.076005	537.034433	10.167719
8.128856	569.055282	10.172736
8.280260	572.838882	10.177754
8.369661	560.315219	10.182771
8.045743	567.004435	10.187789
8.122241	548.218810	10.192807
8.055565	563.778186	10.197824
7.864991	589.256001	10.202842
8.343223	571.995345	10.207859
8.257396	579.289924	10.212877
8.699231	580.852315	10.217895
8.689108	566.807525	10.222912
8.425549	576.044722	10.227930
8.403811	554.424146	10.232947
8.030524	556.253093	10.237965
8.354217	562.834596	10.242983
8.696365	577.781004	10.248000
8.106873	551.579277	10.253018
8.237136	559.992046	10.258035
7.937945	561.718123	10.263053
8.636529	559.832237	10.268071
8.490656	578.442452	10.273088
8.215352	597.509197	10.278106
8.708434	578.143708	10.283123
8.292512	564.907413	10.288141
8.474928	579.061451	10.293159
8.568448	563.163532	10.298176
8.076545	576.467265	10.303194
8.211400	555.616455	10.308211
8.081525	573.885138	10.313229
8.254159	578.323808	10.318247
8.706164	562.565805	10.323264
8.156691	576.422502	10.328282
8.321512	582.182572	10.333299
8.182792	575.616214	10.338317
8.103998	562.694479	10.343335
8.409186	572.458769	10.348352
8.249433	572.906641	10.353370
8.439260	577.423352	10.358387
8.510802	575.069594	10.363405
8.425496	574.563791	10.368423
8.599893	570.596235	10.373440
8.427335	567.183222	10.378458
8.764820	563.702944	10.383475
8.731149	580.556914	10.388493
8.511798	576.662986	10.393511
8.419342	567.871493	10.398528
8.435922	581.239683	10.403546
8.953963	576.637147	10.408563
8.443985	571.438378	10.413581
8.747415	573.671393	10.418599
8.659853	574.671155	10.423616
8.668913	565.975158	10.428634
8.625234	563.897950	10.433651
8.606935	579.447576	10.438669
8.571437	571.984189	10.443687
8.888372	564.590285	10.448704
8.305004	572.763613	10.453722
8.660591	559.699838	10.458739
8.414055	581.383126	10.463757
8.418629	584.583387	10.468775
8.898262	577.629780	10.473792
8.559016	608.179027	10.478810
8.770192	605.843122	10.483827
9.102742	594.864834	10.488845
8.792136	595.721487	10.493863
8.740440	589.220347	10.498880
8.531137	582.531043	10.503898
8.692184	559.277350	10.508915
8.645660	582.859528	10.513933
8.547856	605.751196	10.518951
9.116284	597.456502	10.523968
8.885813	603.401557	10.528986
8.796124	587.229839	10.534003
8.655714	582.585274	10.539021
8.786256	600.135451	10.544039
8.805843	600.343607	10.549056
8.576068	608.102516	10.554074
8.940454	615.166946	10.559091
9.053070	625.144246	10.564109
8.638785	613.569583	10.569127
8.977913	604.731934	10.574144
8.589385	617.542668	10.579162
9.007236	609.559584	10.584179
8.742638	611.448211	10.589197
8.873171	623.914088	10.594215
8.997673	620.343930	10.599232
8.875481	614.862912	10.604250
8.923774	613.320937	10.609267
9.130468	605.667355	10.614285
8.821174	618.875513	10.619303
9.137983	596.058397	10.624320
9.121438	612.136753	10.629338
9.126979	618.969229	10.634355
8.939802	607.433789	10.639373
8.870688	619.039004	10.644391
9.364138	590.514935	10.649408
8.842151	569.415272	10.654426
8.694006	576.171776	10.659443
8.962927	592.453951	10.664461
8.877333	598.756944	10.669479
9.197471	605.309730	10.674496
8.803705	620.639634	10.679514
8.610891	607.128996	10.684531
8.762673	608.429467	10.689549
8.751126	615.342401	10.694567
8.955624	599.544280	10.699584
8.832841	622.043950	10.704602
8.993380	597.011540	10.709619
8.868426	612.285599	10.714637
8.715086	604.926589	10.719655
9.008508	620.730858	10.724672
8.982163	633.813451	10.729690
9.140181	624.071824	10.734707
9.314066	633.945526	10.739725
9.112592	637.061870	10.744743
9.164254	626.590580	10.749760
9.265292	644.551183	10.754778
9.335055	642.663527	10.759795
9.366572	628.620361	10.764813
9.049600	607.575817	10.769831
9.380966	599.666266	10.774848
8.982583	614.024065	10.779866
8.896646	618.616668	10.784883
9.119837	621.975046	10.789901
8.888475	638.191855	10.794919
9.024017	643.386468	10.799936
8.572923	640.421427	10.804954
8.948689	654.142707	10.809971
8.966986	651.845165	10.814989
8.938130	641.647239	10.820007
9.363213	645.651108	10.825024
9.412066	644.215898	10.830042
9.316401	638.054688	10.835059
8.970856	647.557278	10.840077
9.000374	675.418479	10.845095
9.711289	660.271938	10.850112
9.477550	681.364533	10.855130
9.290026	671.627139	10.860147
9.586133	676.035396	10.865165
9.347180	670.294793	10.870183
9.325613	636.306174	10.875200
9.383115	651.083612	10.880218
9.444793	648.061675	10.885235
9.490367	636.301088	10.890253
9.255713	651.451325	10.895271
9.576102	652.208132	10.900288
9.542520	652.357278	10.905306
9.509327	642.357160	10.910323
9.390453	649.374929	10.915341
9.168146	647.728892	10.920359
9.590551	634.758903	10.925376
9.555679	649.609070	10.930394
9.661863	666.465015	10.935411
9.574474	652.225887	10.940429
9.303224	645.710528	10.945447
9.284189	638.157700	10.950464
9.586511	668.838771	10.955482
9.493693	669.515676	10.960499
9.802402	653.875230	10.965517
9.522985	671.523840	10.970535
9.428524	648.243064	10.975552
9.290762	649.782380	10.980570
9.454416	665.598596	10.985587
9.670820	662.989156	10.990605
9.768099	675.174821	10.995623
9.721560	667.551938	11.000640
9.831892	680.353590	11.005658
9.571427	666.099855	11.010675
9.459702	668.020492	11.015693
9.232959	666.085600	11.020711
9.740044	679.679128	11.025728
9.773863	692.100627	11.030746
9.746647	667.628712	11.035763
9.750543	668.987379	11.040781
9.513225	675.426864	11.045799
9.883547	665.851645	11.050816
9.711491	664.543074	11.055834
9.620040	669.841825	11.060851
9.909991	668.920163	11.065869
9.799227	680.538802	11.070887
9.862489	672.567840	11.075904
9.849860	659.133255	11.080922
9.323702	666.018492	11.085939
9.613198	677.893926	11.090957
9.446595	684.575498	11.095975
9.817268	677.973623	11.100992
9.936364	680.684043	11.106010
9.729196	667.888621	11.111027
9.823692	676.324584	11.116045
9.677914	677.900159	11.121063
9.831847	653.636848	11.126080
9.565016	669.422761	11.131098
9.469291	683.109811	11.136115
9.622454	666.066803	11.141133
9.586770	685.651680	11.146151
9.834103	672.826210	11.151168
9.948879	662.643106	11.156186
9.586619	678.668950	11.161203
9.882760	665.819774	11.166221
9.668051	676.877596	11.171239
9.757572	681.379919	11.176256
9.907879	689.378043	11.181274
9.862326	703.839877	11.186291
10.027527	717.950346	11.191309
9.916583	725.379032	11.196327
10.103753	707.477829	11.201344
10.325581	718.002147	11.206362
10.162911	691.000115	11.211379
9.972298	679.250976	11.216397
9.882307	680.107090	11.221415
10.185706	694.181022	11.226432
10.226346	673.324958	11.231450
9.776607	681.686341	11.236467
9.883362	689.712129	11.241485
9.910218	692.927918	11.246503
9.893634	684.529024	11.251520
10.038380	704.777327	11.256538
9.680424	707.270507	11.261555
9.749337	699.659721	11.266573
9.791318	712.142764	11.271591
10.000734	719.486032	11.276608
9.976762	702.206580	11.281626
9.919856	709.971215	11.286643
10.023338	698.100053	11.291661
9.910195	693.885182	11.296679
10.262893	716.749798	11.301696
10.029210	713.856165	11.306714
10.376924	726.429011	11.311731
10.390222	716.091821	11.316749
10.273914	705.837556	11.321767
10.123786	719.102545	11.326784
10.194935	709.378368	11.331802
9.888047	717.664701	11.336819
10.429425	712.759532	11.341837
10.398258	722.952535	11.346855
10.215752	716.763923	11.351872
10.398054	728.862963	11.356890
9.892488	713.148515	11.361907
10.277015	724.116001	11.366925
10.157047	728.646857	11.371943
10.568984	744.607114	11.376960
10.572659	745.982453	11.381978
10.452535	730.355431	11.386995
10.422565	697.627373	11.392013
10.525953	717.445932	11.397031
10.298952	700.285543	11.402048
10.321976	704.209356	11.407066
9.946040	710.045062	11.412083
10.221111	709.683876	11.417101
10.045635	726.620677	11.422119
10.574508	731.743038	11.427136
10.484619	735.630021	11.432154
10.442483	729.619630	11.437171
10.473037	733.923895	11.442189
10.805876	751.510875	11.447207
10.743439	736.746817	11.452224
10.347200	727.457057	11.457242
10.207714	729.696084	11.462259
10.278787	737.932365	11.467277
10.470834	746.418863	11.472295
10.410544	738.281032	11.477312
10.719038	751.009159	11.482330
10.507673	741.385671	11.487347
10.600348	736.010795	11.492365
10.422874	743.547801	11.497383
10.314936	754.707687	11.502400
10.610001	740.941055	11.507418
10.424187	758.245742	11.512435
10.486771	749.073105	11.517453
10.511231	749.227518	11.522471
10.430415	735.224762	11.527488
10.497014	729.528006	11.532506
10.335160	745.263783	11.537523
10.359135	736.275144	11.542541
10.697120	749.250494	11.547559
10.527578	746.043088	11.552576
10.587302	745.027417	11.557594
10.389992	751.390754	11.562611
10.824674	742.130061	11.567629
10.506020	758.363882	11.572647
10.346413	747.432477	11.577664
10.867083	766.259355	11.582682
10.795875	776.893246	11.587699
11.076218	768.863235	11.592717
11.011904	778.294141	11.597735
10.804090	757.871437	11.602752
10.796615	740.451555	11.607770
10.469767	736.597000	11.612787
10.987496	755.417757	11.617805
10.822803	744.864358	11.622823
10.765030	755.855269	11.627840
10.993081	738.470561	11.632858
10.627560	741.906773	11.637875
10.762533	765.172502	11.642893
11.321754	755.543575	11.647911
10.897461	752.431404	11.652928
11.036754	744.935604	11.657946
10.897360	742.890523	11.662963
10.641864	747.872900	11.667981
10.775368	744.685474	11.672999
10.571932	758.418928	11.678016
10.968096	772.787165	11.683034
10.894160	774.489521	11.688051
10.698682	779.988327	11.693069
11.060427	766.525137	11.698087
10.888060	773.333652	11.703104
10.997871	770.993515	11.708122
10.550857	793.386922	11.713139
10.727431	775.607242	11.718157
10.630379	779.832536	11.723175
10.617330	768.308346	11.728192
11.126974	771.976312	11.733210
10.783120	792.612974	11.738227
10.699580	774.452082	11.743245
10.733823	802.484243	11.748263
10.769983	802.436776	11.753280
10.935910	788.680914	11.758298
11.162803	804.279102	11.763315
11.136169	796.449276	11.768333
11.398630	791.616645	11.773351
11.226767	818.373989	11.778368
11.125244	800.055943	11.783386
11.261339	799.953782	11.788403
11.449317	789.114079	11.793421
11.472433	807.238891	11.798439
11.148057	801.867380	11.803456
11.196212	787.470329	11.808474
10.902052	823.310564	11.813491
11.286546	801.189451	11.818509
11.369861	795.658465	11.823527
11.395380	802.493330	11.828544
11.329510	781.139993	11.833562
11.123302	784.096463	11.838579
11.243053	804.295794	11.843597
11.389970	796.400979	11.848615
11.246667	786.259163	11.853632
11.647808	777.474734	11.858650
11.387228	788.883531	11.863667
10.978444	794.456461	11.868685
11.523729	786.505558	11.873703
11.330147	792.317457	11.878720
11.373263	788.742112	11.883738
10.955365	786.137798	11.888755
11.184503	786.543646	11.893773
11.497818	812.046109	11.898791
11.238649	807.295248	11.903808
11.188062	804.848971	11.908826
11.279872	809.070319	11.913843
10.909156	796.797356	11.918861
11.079853	806.725226	11.923879
11.024157	810.425227	11.928896
11.317263	810.782523	11.933914
10.894219	801.635300	11.938931
11.342273	819.914942	11.943949
11.381575	829.765256	11.948967
11.493183	825.021307	11.953984
11.477369	832.982015	11.959002
11.789433	836.162903	11.964019
11.736904	836.658301	11.969037
11.806882	849.422778	11.974055
11.398958	836.483567	11.979072
11.501299	814.234601	11.984090
11.463833	836.200641	11.989107
11.466618	826.178124	11.994125
11.689871	832.314258	11.999143
11.358486	824.816204	12.004160
11.848475	832.138350	12.009178
11.674347	832.692022	12.014195
11.248979	834.075198	12.019213
11.830995	843.763214	12.024231
11.500031	836.900844	12.029248
11.571840	829.045583	12.034266
11.704728	836.989984	12.039283
11.688103	827.379130	12.044301
11.880484	822.615142	12.049319
11.590578	853.283163	12.054336
11.655294	831.638856	12.059354
11.531244	831.201242	12.064371
11.755618	843.924947	12.069389
11.929175	833.587664	12.074407
11.950218	834.457614	12.079424
11.824476	839.769470	12.084442
11.807630	831.768762	12.089459
11.518093	827.462367	12.094477
11.876486	833.418533	12.099495
11.825167	825.708391	12.104512
11.608549	820.854457	12.109530
11.629546	827.213728	12.114547
11.425315	848.203473	12.119565
11.779757	846.125083	12.124583
11.745855	871.613981	12.129600
11.969203	864.225165	12.134618
11.653466	848.312321	12.139635
11.855925	860.781560	12.144653
12.221577	867.531118	12.149671
11.870210	887.439415	12.154688
12.234710	849.410971	12.159706
12.170303	861.848249	12.164723
12.077763	871.662224	12.169741
12.275277	864.222082	12.174759
11.899877	860.316184	12.179776
12.178223	871.566510	12.184794
12.258648	865.953125	12.189811
11.968948	871.453267	12.194829
12.278923	843.385317	12.199847
12.001590	851.496410	12.204864
11.719993	854.915727	12.209882
12.146480	852.660216	12.214899
11.675499	859.741288	12.219917
11.808068	869.124165	12.224935
11.653109	854.335629	12.229952
11.946005	855.967631	12.234970
12.155046	866.431778	12.239987
11.883085	856.208252	12.245005
12.259807	853.194924	12.250023
12.130695	873.172056	12.255040
12.101976	852.249770	12.260058
12.184615	853.161104	12.265075
11.704593	857.687836	12.270093
12.265141	870.269416	12.275111
12.297207	893.633821	12.280128
12.311890	889.802687	12.285146
12.365816	899.802953	12.290163
12.396568	896.160057	12.295181
12.593435	883.963163	12.300199
12.205683	872.961525	12.305216
12.008947	877.178424	12.310234
12.363985	885.352113	12.315251
12.438556	893.069037	12.320269
12.429366	906.926290	12.325287
12.455704	898.182280	12.330304
12.555440	875.737740	12.335322
12.407211	876.561670	12.340339
12.194671	870.627797	12.345357
12.627636	880.546616	12.350375
12.445785	892.481809	12.355392
12.421413	869.433441	12.360410
12.667700	860.749044	12.365427
12.021918	874.883374	12.370445
12.320519	863.091622	12.375463
12.667739	890.761083	12.380480
12.754935	900.380848	12.385498
12.835982	888.088946	12.390515
12.434972	886.339969	12.395533
12.304078	870.460613	12.400551
12.369614	870.198503	12.405568
12.582736	884.995221	12.410586
12.918241	889.625711	12.415603
12.581573	884.073572	12.420621
12.864893	892.887793	12.425639
12.738058	880.417512	12.430656
12.473615	847.327986	12.435674
12.486283	863.438383	12.440691
12.261077	873.189462	12.445709
12.883710	880.930739	12.450727
12.418056	898.100085	12.455744
12.468249	903.559517	12.460762
12.775317	882.445316	12.465779
12.782997	882.531951	12.470797
12.833546	892.869593	12.475815
12.553059	911.813106	12.480832
12.578730	893.244066	12.485850
12.569838	910.155213	12.490867
12.531886	903.540968	12.495885
12.737776	878.948423	12.500903
12.518919	883.859550	12.505920
12.412332	899.024094	12.510938
12.501495	902.796119	12.515955
12.691608	891.273784	12.520973
12.647418	882.638559	12.525991
12.789081	904.375245	12.531008
12.726922	904.802865	12.536026
13.313502	923.515921	12.541043
12.888274	918.627255	12.546061
12.952492	889.453080	12.551079
12.903170	904.844621	12.556096
12.994770	908.111354	12.561114
12.746213	903.850218	12.566131
12.979104	917.373947	12.571149
13.077350	922.998432	12.576167
13.070437	936.273397	12.581184
12.883091	915.745845	12.586202
13.244717	898.963328	12.591219
12.984988	904.937343	12.596237
12.918673	915.804714	12.601255
13.232331	920.715426	12.606272
13.090833	931.097918	12.611290
13.004251	911.489506	12.616307
12.803874	909.431161	12.621325
13.014938	925.117302	12.626343
13.382424	915.070372	12.631360
13.057559	921.269473	12.636378
13.624262	924.532479	12.641395
13.052092	915.396843	12.646413
13.090149	895.907778	12.651431
13.217149	897.479427	12.656448
13.052871	900.632087	12.661466
13.327029	892.419420	12.666483
13.233752	917.051697	12.671501
13.342363	906.016223	12.676519
13.186450	900.000164	12.681536
13.384500	920.746113	12.686554
13.263496	887.331889	12.691571
12.839157	877.589711	12.696589
13.174085	909.225767	12.701607
13.131306	902.914801	12.706624
13.307732	905.119555	12.711642
13.462459	920.446002	12.716659
13.421398	921.091930	12.721677
13.490690	917.689153	12.726695
13.516075	927.277527	12.731712
13.413486	916.307550	12.736730
13.571486	914.247445	12.741747
13.242960	934.915417	12.746765
13.415924	920.379142	12.751783
13.475490	932.349943	12.756800
13.299058	926.513302	12.761818
13.403834	918.102785	12.766835
13.065585	925.459514	12.771853
13.386593	902.346147	12.776871
13.557790	916.617284	12.781888
13.294450	918.820718	12.786906
13.513479	919.252841	12.791923
13.438530	920.576147	12.796941
13.567580	923.503610	12.801959
13.460820	935.742685	12.806976
13.379095	924.390513	12.811994
13.632938	902.664174	12.817011
13.268135	922.850160	12.822029
13.250298	928.777813	12.827047
13.337022	919.037744	12.832064
13.357710	937.655113	12.837082
13.693584	953.518639	12.842099
13.824567	941.409142	12.847117
13.814828	943.351828	12.852135
13.919380	929.543302	12.857152
13.647607	928.270768	12.862170
13.564594	913.133363	12.867187
13.392115	937.634605	12.872205
13.573914	934.567767	12.877223
13.668318	942.828052	12.882240
13.554094	950.761493	12.887258
13.896558	943.258392	12.892275
13.875179	954.551915	12.897293
13.931387	939.426507	12.902311
14.074011	959.388661	12.907328
13.823218	968.073113	12.912346
13.983092	944.373204	12.917363
14.007992	960.750118	12.922381
13.694871	942.460768	12.927399
13.865410	949.764226	12.932416
13.819910	952.992027	12.937434
13.991701	934.497681	12.942451
13.612964	960.498815	12.947469
13.615419	963.403713	12.952487
13.873582	946.287249	12.957504
13.836055	944.127694	12.962522
13.897814	952.137538	12.967539
14.145208	953.569248	12.972557
14.170603	932.869346	12.977575
14.381473	950.764040	12.982592
14.023216	950.194796	12.987610
14.293594	948.029424	12.992627
14.140686	954.986339	12.997645
14.181031	945.095297	13.002663
14.091724	931.845444	13.007680
13.892784	948.638767	13.012698
14.129513	936.593471	13.017715
14.185020	951.528575	13.022733
14.206894	949.228724	13.027751
14.411338	946.268842	13.032768
14.082317	953.981252	13.037786
14.383478	946.602170	13.042803
14.324034	952.792648	13.047821
14.210315	930.644162	13.052839
14.135769	949.521414	13.057856
13.990080	945.220634	13.062874
14.342315	937.891566	13.067891
14.011532	960.382711	13.072909
13.629703	951.555079	13.077927
14.374901	941.851810	13.082944
14.525055	959.009591	13.087962
14.177850	949.024856	13.092979
14.190030	940.699297	13.097997
14.147477	954.758218	13.103015
14.389901	933.448185	13.108032
14.128059	947.718688	13.113050
14.312628	956.388579	13.118067
14.176624	951.435082	13.123085
14.516407	957.555552	13.128103
14.521951	972.031310	13.133120
14.211547	971.611794	13.138138
14.497100	977.047314	13.143155
14.664957	987.777046	13.148173
14.667169	977.666652	13.153191
14.435176	978.895473	13.158208
14.508722	973.826946	13.163226
14.492888	956.644877	13.168243
14.563279	980.893778	13.173261
14.517079	990.599310	13.178279
14.581791	973.742581	13.183296
14.810418	973.974154	13.188314
14.340908	973.715346	13.193331
14.442971	969.734058	13.198349
14.641403	955.489258	13.203367
14.820764	976.512293	13.208384
14.896615	981.654895	13.213402
14.865758	966.201513	13.218419
14.662404	980.122604	13.223437
14.575607	980.596512	13.228455
14.635428	979.434586	13.233472
14.493589	983.321165	13.238490
14.329447	959.818344	13.243507
14.815121	975.602304	13.248525
14.654520	978.280475	13.253543
14.991431	966.128367	13.258560
14.639420	988.597576	13.263578
14.773059	972.783229	13.268595
14.788327	979.216818	13.273613
14.842317	971.276065	13.278631
14.755707	964.456626	13.283648
14.790357	980.719650	13.288666
14.581874	975.326563	13.293683
14.782393	972.576623	13.298701
14.328731	989.096023	13.303719
14.875436	988.249697	13.308736
15.001327	991.821629	13.313754
15.204371	1011.696720	13.318771
15.038404	992.551112	13.323789
14.745698	998.137700	13.328807
14.690445	986.506667	13.333824
14.945719	1002.130182	13.338842
15.054895	1017.963539	13.343859
15.151370	1013.525894	13.348877
15.089138	994.625970	13.353895
15.270872	989.747282	13.358912
15.206721	1015.816964	13.363930
15.435330	998.550442	13.368947
15.229123	997.035727	13.373965
14.956428	1016.596235	13.378983
15.233129	996.887039	13.384000
14.890944	994.588009	13.389018
15.020089	996.735941	13.394035
15.354981	1014.092430	13.399053
15.178238	1015.734754	13.404071
15.103798	1003.541371	13.409088
15.164013	996.046413	13.414106
15.221219	1009.364375	13.419123
15.481149	991.166833	13.424141
15.254282	1009.482766	13.429159
15.445970	1002.270333	13.434176
15.363023	1010.293789	13.439194
15.218023	1012.277533	13.444211
15.468777	1001.927674	13.449229
15.422391	1011.277827	13.454247
15.455171	1005.201515	13.459264
15.373945	1003.288090	13.464282
15.489890	1012.370532	13.469299
15.605574	1001.773081	13.474317
15.158769	993.241525	13.479335
15.758323	992.627350	13.484352
15.350331	1011.963423	13.489370
15.618952	1027.759911	13.494387
15.652326	1014.090993	13.499405
15.282861	1001.501201	13.504423
15.775507	1002.583605	13.509440
15.256321	996.966532	13.514458
15.423476	1012.584940	13.519475
15.487207	998.808878	13.524493
15.562884	1020.147483	13.529511
15.461555	1025.112443	13.534528
15.372722	1006.045486	13.539546
15.319648	1015.331507	13.544563
15.683225	1002.611028	13.549581
15.342560	986.855369	13.554599
15.671545	1002.010813	13.559616
15.449222	1011.848884	13.564634
15.042553	1015.797341	13.569651
15.422711	1033.081722	13.574669
15.215860	1031.267085	13.579687
15.314112	1022.227136	13.584704
15.362126	1036.724497	13.589722
15.748212	1018.260664	13.594739
16.081730	1031.966438	13.599757
16.027347	1031.125374	13.604775
16.059116	1029.448622	13.609792
15.729617	1047.759519	13.614810
15.634433	1028.118136	13.619827
15.929914	1036.359214	13.624845
15.770323	1034.956546	13.629863
15.878876	1014.132780	13.634880
16.018028	1030.755093	13.639898
15.982721	1032.878547	13.644915
15.998599	1025.642710	13.649933
15.636307	1050.619681	13.654951
15.910049	1042.405921	13.659968
16.230942	1021.068531	13.664986
16.120557	1013.305080	13.670003
16.116227	1027.127297	13.675021
15.803255	1032.187948	13.680039
15.911464	1024.630531	13.685056
16.049338	1053.068262	13.690074
16.007243	1062.290406	13.695091
16.375888	1042.530828	13.700109
16.047978	1046.323793	13.705127
16.257303	1046.167610	13.710144
16.275491	1036.387723	13.715162
15.972735	1051.462130	13.720179
16.198478	1050.967589	13.725197
16.270841	1052.473104	13.730215
16.451743	1055.550056	13.735232
16.097876	1035.258178	13.740250
16.627972	1042.696406	13.745267
16.343602	1044.252509	13.750285
16.289350	1028.873583	13.755303
16.081278	1042.930320	13.760320
16.235174	1037.213217	13.765338
16.094173	1057.354423	13.770355
16.613308	1055.269945	13.775373
16.403876	1059.913986	13.780391
16.380456	1052.949526	13.785408
16.773095	1042.087139	13.790426
16.134217	1044.145026	13.795443
16.399042	1042.115072	13.800461
16.511270	1048.226641	13.805479
16.557064	1056.847197	13.810496
16.737450	1062.617372	13.815514
16.334099	1039.546949	13.820531
16.745679	1029.620973	13.825549
16.332626	1035.908100	13.830567
16.234814	1025.027096	13.835584
16.369087	1040.438224	13.840602
16.720692	1070.716583	13.845619
16.577963	1048.225365	13.850637
16.490381	1067.413305	13.855655
16.536781	1059.502690	13.860672
16.446371	1049.515108	13.865690
16.478328	1058.069661	13.870707
16.858980	1062.182928	13.875725
16.546739	1065.814784	13.880743
16.455088	1052.291856	13.885760
16.788248	1053.156192	13.890778
16.378522	1050.578131	13.895795
16.504377	1056.437512	13.900813
16.581454	1059.724783	13.905831
16.346890	1054.328402	13.910848
16.966328	1069.164129	13.915866
16.361588	1071.438568	13.920883
16.682255	1077.849281	13.925901
16.931099	1096.208916	13.930919
17.032382	1086.400701	13.935936
17.520256	1105.236763	13.940954
17.052681	1076.223818	13.945971
17.043318	1077.277995	13.950989
16.755294	1067.479319	13.956007
16.780474	1041.051579	13.961024
16.687218	1067.561583	13.966042
16.759000	1097.035559	13.971059
17.178227	1088.589219	13.976077
17.081140	1091.586952	13.981095
16.973468	1100.107629	13.986112
17.245276	1086.860253	13.991130
17.420219	1081.122042	13.996147
17.385291	1062.595184	14.001165
17.146103	1060.061165	14.006183
16.766655	1068.009272	14.011200
17.107394	1058.349252	14.016218
16.602099	1077.885104	14.021235
17.412510	1090.168551	14.026253
17.334751	1087.462118	14.031271
17.212950	1097.313446	14.036288
17.165816	1063.182570	14.041306
16.898918	1087.657145	14.046323
16.876989	1097.871700	14.051341
17.242219	1104.639932	14.056359
17.311060	1084.714247	14.061376
17.306940	1078.143438	14.066394
17.022509	1099.227764	14.071411
17.123322	1089.813131	14.076429
17.191332	1088.036903	14.081447
17.162893	1094.092916	14.086464
17.331068	1073.435749	14.091482
16.942314	1087.834612	14.096499
17.203538	1108.469219	14.101517
17.269672	1124.193489	14.106535
17.255339	1117.164029	14.111552
17.607767	1129.945926	14.116570
17.592072	1122.429897	14.121587
17.729686	1120.033550	14.126605
17.644455	1113.989096	14.131623
17.589898	1110.226323	14.136640
18.081548	1115.057991	14.141658
17.677866	1105.867533	14.146675
17.429416	1092.828933	14.151693
17.440286	1072.467676	14.156711
17.653685	1082.394081	14.161728
17.587178	1091.318972	14.166746
17.274318	1103.854284	14.171763
17.956029	1102.096095	14.176781
17.512253	1116.688580	14.181799
17.790899	1126.860074	14.186816
18.074665	1103.782375	14.191834
17.717972	1114.854332	14.196851
17.745236	1122.233211	14.201869
17.831853	1109.790936	14.206887
17.614321	1130.211947	14.211904
18.189202	1121.744294	14.216922
17.630740	1102.650915	14.221939
17.564077	1114.041880	14.226957
17.686797	1109.676131	14.231975
17.781743	1119.349071	14.236992
18.222383	1103.957166	14.242010
18.033866	1129.806707	14.247027
18.233594	1119.658757	14.252045
17.998466	1115.433817	14.257063
17.920663	1101.002576	14.262080
18.056630	1106.838657	14.267098
18.228152	1108.834165	14.272115
18.118835	1106.461702	14.277133
18.122836	1116.265783	14.282151
17.795053	1099.147185	14.287168
17.832478	1096.231014	14.292186
18.117594	1119.226466	14.297203
17.926238	1103.490292	14.302221
18.251185	1100.870714	14.307239
18.127889	1127.644975	14.312256
18.223618	1107.770118	14.317274
18.182762	1117.981811	14.322291
18.208881	1110.206380	14.327309
18.149081	1115.980449	14.332327
18.097809	1119.029558	14.337344
18.363985	1113.680983	14.342362
18.230584	1124.536857	14.347379
18.084464	1105.269452	14.352397
18.533236	1124.720415	14.357415
18.160978	1118.584253	14.362432
18.339851	1109.759908	14.367450
18.207063	1109.170617	14.372467
18.310352	1096.324317	14.377485
18.516083	1114.364702	14.382503
18.197906	1133.358605	14.387520
18.364785	1110.842404	14.392538
18.366998	1117.299660	14.397555
18.054117	1103.733934	14.402573
17.978191	1109.084983	14.407591
18.008001	1133.320585	14.412608
18.554761	1130.177750	14.417626
18.551407	1129.456071	14.422643
18.503812	1137.450922	14.427661
18.741635	1139.372107	14.432679
18.774025	1136.116979	14.437696
18.700917	1147.713316	14.442714
18.633350	1145.816607	14.447731
18.757133	1139.520824	14.452749
18.716238	1155.209873	14.457767
18.818016	1145.926904	14.462784
18.591707	1145.864951	14.467802
18.828131	1141.620822	14.472819
18.424624	1150.962869	14.477837
18.865735	1145.694993	14.482855
18.415977	1140.668118	14.487872
18.865717	1145.906429	14.492890
18.588219	1136.725997	14.497907
18.735192	1143.732137	14.502925
18.836527	1125.880548	14.507943
18.808229	1151.162244	14.512960
18.788601	1131.759460	14.517978
18.792957	1141.343178	14.522995
18.652041	1142.233613	14.528013
18.641868	1130.174059	14.533031
18.599034	1140.833821	14.538048
18.702992	1156.928457	14.543066
18.602934	1162.833380	14.548083
18.718061	1167.422932	14.553101
19.067392	1178.528124	14.558119
19.248571	1168.124903	14.563136
18.970809	1171.771062	14.568154
18.908812	1177.049278	14.573171
19.033635	1167.903497	14.578189
19.353480	1186.083338	14.583207
19.282472	1178.245103	14.588224
19.262578	1166.256304	14.593242
19.282461	1169.524023	14.598259
19.056856	1169.030954	14.603277
19.106130	1159.315618	14.608295
19.207491	1175.203172	14.613312
19.256391	1170.196021	14.618330
19.130939	1183.664666	14.623347
19.190232	1164.185920	14.628365
19.662790	1163.854869	14.633383
19.551311	1181.963696	14.638400
19.333041	1169.082406	14.643418
19.482810	1174.083852	14.648435
19.240120	1184.819083	14.653453
19.568045	1168.768932	14.658471
19.517108	1176.727751	14.663488
19.415243	1166.248795	14.668506
19.506070	1161.130708	14.673523
19.701999	1174.905203	14.678541
19.576900	1180.190896	14.683559
19.459790	1171.141578	14.688576
19.259916	1165.122741	14.693594
19.366104	1168.598289	14.698611
19.342894	1161.632564	14.703629
19.397473	1161.406110	14.708647
19.250188	1178.955828	14.713664
19.574873	1173.868758	14.718682
19.860342	1159.687886	14.723699
19.499365	1166.090347	14.728717
19.765521	1186.588254	14.733735
19.798983	1182.346560	14.738752
19.296304	1151.700194	14.743770
19.754976	1181.330816	14.748787
19.569489	1198.446324	14.753805
20.105895	1194.427541	14.758823
20.180004	1207.949723	14.763840
20.560659	1200.279496	14.768858
20.391899	1171.973009	14.773875
19.790888	1183.876541	14.778893
19.837971	1170.150604	14.783911
19.821663	1161.969461	14.788928
19.942890	1160.823254	14.793946
19.865544	1156.534442	14.798963
19.506193	1159.516586	14.803981
19.776924	1173.720247	14.808999
19.838052	1183.327278	14.814016
20.226071	1213.255593	14.819034
20.126783	1193.135556	14.824051
19.921070	1187.677680	14.829069
20.199551	1213.401971	14.834087
20.191128	1196.142221	14.839104
20.130107	1199.302675	14.844122
20.346627	1223.944568	14.849139
19.989549	1189.384429	14.854157
20.391526	1181.593983	14.859175
20.061529	1177.383916	14.864192
20.317906	1198.996576	14.869210
20.320866	1189.983985	14.874227
19.909994	1183.393067	14.879245
20.080622	1189.613418	14.884263
20.327623	1194.839690	14.889280
19.814217	1209.443869	14.894298
20.081334	1185.783503	14.899315
20.099235	1193.329869	14.904333
20.488382	1179.484713	14.909351
20.109992	1199.522359	14.914368
20.021470	1203.561364	14.919386
20.286345	1194.133823	14.924403
20.150377	1201.228569	14.929421
20.476127	1226.716483	14.934439
20.645567	1223.266485	14.939456
20.690367	1213.636676	14.944474
20.704499	1223.706018	14.949491
20.548852	1214.090834	14.954509
20.470384	1210.225026	14.959527
20.621804	1215.276201	14.964544
20.836964	1224.451796	14.969562
20.950389	1223.337280	14.974579
20.640787	1198.741341	14.979597
20.806490	1199.678132	14.984615
21.021734	1186.419845	14.989632
20.725034	1190.394651	14.994650
20.924433	1186.165878	14.999667
20.851529	1188.529271	15.004685
20.864939	1202.561459	15.009703
20.810720	1200.195227	15.014720
20.830764	1175.495156	15.019738
21.121562	1181.921576	15.024755
20.697118	1185.376970	15.029773
21.058464	1193.579500	15.034791
20.467804	1183.103572	15.039808
20.881104	1202.454912	15.044826
20.989714	1189.196729	15.049843
20.708759	1172.819442	15.054861
20.615612	1182.910717	15.059879
20.568656	1217.660582	15.064896
20.637400	1229.432508	15.069914
20.997787	1218.055764	15.074931
20.589839	1213.087983	15.079949
21.055841	1217.596441	15.084967
21.056524	1234.658592	15.089984
20.698217	1221.397148	15.095002
21.049593	1217.301088	15.100019
21.154853	1245.766413	15.105037
21.496613	1231.065858	15.110055
21.623461	1233.196098	15.115072
21.111595	1232.713531	15.120090
21.199118	1211.888937	15.125107
20.907653	1221.634557	15.130125
21.605116	1244.788084	15.135143
21.588131	1242.730973	15.140160
21.348108	1237.948867	15.145178
21.458095	1213.362778	15.150195
21.355327	1218.909692	15.155213
21.386602	1212.246383	15.160231
21.330478	1202.251263	15.165248
21.184864	1221.729038	15.170266
21.825465	1245.952738	15.175283
21.507908	1232.450452	15.180301
21.466903	1231.095278	15.185319
21.780678	1210.996895	15.190336
21.420009	1203.224327	15.195354
21.276664	1221.813650	15.200371
21.370833	1223.743136	15.205389
21.610164	1237.087583	15.210407
21.823387	1254.618353	15.215424
21.855288	1247.962895	15.220442
21.853472	1241.086785	15.225459
21.578527	1236.953410	15.230477
21.750810	1221.548662	15.235495
21.410791	1241.442061	15.240512
21.740989	1232.470128	15.245530
21.742830	1237.262828	15.250547
21.636102	1235.424832	15.255565
21.841934	1235.153307	15.260583
21.931677	1241.878368	15.265600
21.588657	1255.483991	15.270618
22.098554	1235.873418	15.275635
22.011095	1250.728036	15.280653
22.319351	1241.542747	15.285671
22.320247	1223.227441	15.290688
21.969619	1237.525186	15.295706
22.143331	1241.306151	15.300723
22.127777	1236.444343	15.305741
21.958439	1250.118972	15.310759
21.819330	1235.202674	15.315776
21.882114	1249.950690	15.320794
22.050507	1252.549546	15.325811
22.116602	1232.963019	15.330829
22.058982	1245.630142	15.335847
22.374005	1233.839526	15.340864
22.056885	1230.508507	15.345882
22.326398	1241.144963	15.350899
22.087631	1248.798323	15.355917
22.145641	1253.253083	15.360935
22.294368	1244.222176	15.365952
22.217450	1229.403455	15.370970
22.261165	1238.627466	15.375987
22.413025	1230.585680	15.381005
22.241934	1220.785589	15.386023
22.514236	1240.581241	15.391040
22.197459	1257.444266	15.396058
22.199163	1233.762938	15.401075
21.831883	1237.279944	15.406093
22.158306	1262.709651	15.411111
22.581087	1265.788986	15.416128
22.524415	1278.292927	15.421146
22.759516	1271.918274	15.426163
22.636848	1261.088836	15.431181
22.913241	1249.511826	15.436199
22.921260	1285.414595	15.441216
22.688816	1263.090904	15.446234
22.700055	1240.578486	15.451251
22.436005	1251.802219	15.456269
22.524857	1258.603205	15.461287
22.629528	1257.368114	15.466304
22.504201	1262.040040	15.471322
22.749252	1257.797799	15.476339
22.755644	1270.353305	15.481357
22.650779	1261.549096	15.486375
23.028314	1259.252417	15.491392
22.564789	1269.968309	15.496410
23.131333	1267.783569	15.501427
22.903030	1261.175140	15.506445
22.648950	1270.038635	15.511463
22.947195	1265.506564	15.516480
23.212498	1259.898596	15.521498
22.871750	1259.223122	15.526515
23.143853	1271.993419	15.531533
22.904506	1261.722114	15.536551
23.353051	1256.679494	15.541568
23.120125	1277.787240	15.546586
23.306320	1277.635566	15.551603
22.932914	1270.035501	15.556621
23.246618	1263.752267	15.561639
23.204724	1264.061712	15.566656
23.069960	1259.449858	15.571674
23.046026	1257.404816	15.576691
23.023235	1277.847077	15.581709
22.651724	1266.102386	15.586727
23.140339	1266.632554	15.591744
23.303189	1283.368521	15.596762
23.166091	1279.742154	15.601779
23.106182	1294.282785	15.606797
23.072546	1316.498824	15.611815
23.543703	1294.723718	15.616832
23.543429	1290.291354	15.621850
23.295017	1279.412523	15.626867
23.531695	1297.738395	15.631885
23.553770	1305.332344	15.636903
23.565295	1294.177922	15.641920
23.549364	1305.500619	15.646938
23.534956	1290.296694	15.651955
23.421225	1273.573726	15.656973
23.375212	1288.411789	15.661991
23.647066	1290.087858	15.667008
23.165950	1286.663287	15.672026
23.554894	1279.828661	15.677043
23.733420	1293.846143	15.682061
23.484854	1294.673490	15.687079
23.738070	1291.128746	15.692096
23.703251	1286.455003	15.697114
23.920747	1301.340161	15.702131
24.130614	1319.816324	15.707149
23.794212	1302.355595	15.712167
24.065540	1290.489596	15.717184
23.820206	1284.505579	15.722202
23.849422	1269.489991	15.727219
24.017500	1293.922337	15.732237
23.906479	1299.542871	15.737255
23.975840	1296.040907	15.742272
23.958246	1316.257609	15.747290
24.261294	1305.726699	15.752307
24.160738	1312.380113	15.757325
24.076742	1313.065134	15.762343
24.486174	1289.212624	15.767360
24.240933	1284.044054	15.772378
23.906759	1288.064833	15.777395
24.483155	1289.442501	15.782413
24.101333	1294.590090	15.787431
24.155985	1293.298808	15.792448
24.232968	1286.216689	15.797466
24.265803	1283.244757	15.802483
24.439173	1310.811948	15.807501
24.044455	1303.631926	15.812519
24.155787	1308.559374	15.817536
24.286689	1328.449751	15.822554
24.092863	1321.226584	15.827571
24.072026	1302.061131	15.832589
24.360677	1325.771992	15.837607
24.524118	1309.745826	15.842624
24.333845	1317.533103	15.847642
24.345130	1329.049406	15.852659
24.477803	1324.587780	15.857677
24.565180	1327.250420	15.862695
24.463033	1323.249354	15.867712
24.460568	1306.201930	15.872730
24.379649	1306.048347	15.877747
24.670778	1315.489135	15.882765
24.557365	1335.568386	15.887783
24.837422	1336.929199	15.892800
24.606881	1344.222964	15.897818
24.612924	1347.745804	15.902835
25.080762	1338.973257	15.907853
24.929690	1346.320213	15.912871
25.030578	1311.623498	15.917888
25.019145	1321.548837	15.922906
24.780522	1308.264291	15.927923
25.000324	1314.238432	15.932941
24.681773	1328.046032	15.937959
24.942133	1308.261398	15.942976
24.651879	1321.899197	15.947994
24.902676	1342.735798	15.953011
25.525963	1334.577872	15.958029
25.130361	1348.171404	15.963047
24.905167	1355.329970	15.968064
25.102648	1346.049467	15.973082
24.903229	1356.220116	15.978099
25.386802	1344.959210	15.983117
24.992117	1332.626502	15.988135
25.342265	1340.283154	15.993152
25.091737	1359.056952	15.998170
25.413861	1361.054863	16.003187
25.188852	1333.833605	16.008205
25.126060	1334.895645	16.013223
25.251181	1351.437673	16.018240
25.044208	1332.262991	16.023258
25.333358	1348.847087	16.028275
25.387699	1355.356150	16.033293
25.484948	1342.107191	16.038311
25.384036	1334.002422	16.043328
25.308030	1340.425761	16.048346
24.980103	1335.615543	16.053363
25.166306	1344.058467	16.058381
25.266736	1361.999643	16.063399
25.715536	1363.273039	16.068416
25.587882	1382.301695	16.073434
25.626324	1382.626305	16.078451
25.894010	1360.668047	16.083469
25.839829	1367.164642	16.088487
25.722346	1358.673810	16.093504
25.964340	1370.542775	16.098522
25.904626	1361.522137	16.103539
25.686887	1346.868274	16.108557
25.498741	1331.672747	16.113575
25.608412	1346.130102	16.118592
25.608498	1368.558802	16.123610
25.469974	1364.859143	16.128627
25.927951	1367.207158	16.133645
25.624163	1385.412361	16.138663
25.801056	1368.766430	16.143680
25.763251	1381.362788	16.148698
25.482103	1368.135305	16.153715
25.748647	1367.345396	16.158733
25.941068	1388.675948	16.163751
26.208651	1403.203597	16.168768
26.254913	1399.966392	16.173786
26.274301	1387.412884	16.178803
26.470570	1390.486872	16.183821
26.561493	1384.591605	16.188839
26.568516	1374.839030	16.193856
26.433098	1365.477929	16.198874
26.370926	1361.775394	16.203891
26.630680	1355.659860	16.208909
26.126549	1359.369155	16.213927
26.393372	1361.981088	16.218944
26.326549	1358.951612	16.223962
25.713278	1358.170023	16.228979
26.361575	1355.462230	16.233997
26.340981	1366.203297	16.239015
26.239066	1342.090602	16.244032
26.526689	1367.045213	16.249050
26.388421	1397.694184	16.254067
26.799093	1381.212809	16.259085
26.852377	1397.610986	16.264103
26.454770	1394.161765	16.269120
26.436846	1373.130708	16.274138
26.384981	1390.778949	16.279155
26.622229	1387.213696	16.284173
26.636603	1379.708217	16.289191
26.783112	1392.208195	16.294208
26.754631	1404.064122	16.299226
26.599337	1385.937585	16.304243
27.253152	1359.896834	16.309261
27.087755	1379.704285	16.314279
27.272795	1376.528679	16.319296
27.355035	1363.713384	16.324314
26.878376	1367.224287	16.329331
26.886699	1345.940953	16.334349
26.725583	1350.977203	16.339367
27.140340	1359.539122	16.344384
27.186574	1363.673295	16.349402
26.732879	1354.380739	16.354419
27.037481	1362.852226	16.359437
26.843627	1387.216216	16.364455
26.614224	1375.573518	16.369472
27.318575	1360.601746	16.374490
27.077360	1373.228465	16.379507
27.048788	1354.307970	16.384525
27.027875	1380.508891	16.389543
27.250715	1382.204878	16.394560
27.309395	1367.801114	16.399578
26.724496	1384.892896	16.404595
27.180385	1376.068378	16.409613
27.253687	1369.146733	16.414631
27.386268	1397.652599	16.419648
27.539016	1400.062377	16.424666
27.470140	1397.913055	16.429683
27.810750	1406.962443	16.434701
27.741294	1391.988133	16.439719
27.875968	1371.431846	16.444736
27.622017	1368.298676	16.449754
27.337861	1374.919973	16.454771
27.779145	1360.818654	16.459789
27.416151	1374.715610	16.464807
27.828901	1379.946536	16.469824
27.500290	1368.197431	16.474842
27.757227	1389.298278	16.479859
27.906400	1391.390016	16.484877
27.685625	1393.122905	16.489895
27.857959	1401.232894	16.494912
28.071393	1396.783879	16.499930
27.792171	1401.027640	16.504947
27.693798	1402.141126	16.509965
27.796738	1405.765165	16.514983
27.770109	1411.307930	16.520000
27.956872	1392.775527	16.525018
27.788396	1400.038002	16.530035
27.951482	1416.104837	16.535053
27.985100	1414.179466	16.540071
27.878984	1408.539635	16.545088
28.230559	1388.867551	16.550106
27.782460	1397.541382	16.555123
28.172119	1408.441599	16.560141
28.256129	1401.549561	16.565159
28.141227	1391.695301	16.570176
28.058093	1403.498461	16.575194
27.831526	1409.544930	16.580211
27.853832	1394.482831	16.585229
28.277849	1417.062953	16.590247
28.300591	1438.946401	16.595264
28.910840	1428.572566	16.600282
28.416684	1428.949570	16.605299
28.608832	1438.269519	16.610317
28.398492	1409.213136	16.615335
28.248475	1423.880174	16.620352
28.618207	1430.875218	16.625370
28.541343	1436.047048	16.630387
28.578684	1430.073531	16.635405
28.660253	1437.078117	16.640423
28.768929	1427.232152	16.645440
28.842318	1399.784731	16.650458
28.519291	1425.462555	16.655475
28.595746	1435.116020	16.660493
28.832413	1430.524113	16.665511
28.290349	1432.740616	16.670528
28.679058	1419.587290	16.675546
28.466725	1433.384910	16.680563
28.888323	1437.006679	16.685581
29.017812	1422.714757	16.690599
29.180615	1431.563082	16.695616
29.154109	1424.491605	16.700634
28.765241	1417.672490	16.705651
28.905770	1419.158117	16.710669
29.046290	1428.308089	16.715687
28.804251	1441.222731	16.720704
28.839529	1417.661232	16.725722
29.138056	1437.894047	16.730739
29.075523	1430.274312	16.735757
29.029340	1424.333986	16.740775
28.522176	1453.660578	16.745792
29.384250	1455.632939	16.750810
29.377486	1468.683292	16.755827
29.261850	1476.510174	16.760845
29.533725	1452.992772	16.765863
29.629865	1459.591604	16.770880
29.585154	1459.707270	16.775898
29.492086	1456.285939	16.780915
29.363433	1459.615265	16.785933
29.422893	1457.733640	16.790951
29.514645	1461.102216	16.795968
29.439986	1444.766218	16.800986
29.316011	1455.988011	16.806003
29.661766	1456.609497	16.811021
29.484876	1433.277285	16.816039
29.443507	1439.800724	16.821056
29.674237	1445.479968	16.826074
29.431830	1452.896682	16.831091
29.393416	1453.031776	16.836109
29.343395	1452.268198	16.841127
29.453420	1465.874023	16.846144
29.949416	1477.238304	16.851162
29.862068	1477.580063	16.856179
29.891084	1484.219815	16.861197
29.984099	1468.148342	16.866215
29.854404	1485.803847	16.871232
30.086977	1480.723534	16.876250
29.792167	1474.799970	16.881267
29.707108	1487.606936	16.886285
30.176722	1476.164423	16.891303
29.758428	1488.111992	16.896320
29.793963	1479.139507	16.901338
29.960627	1466.842243	16.906355
29.978482	1473.822442	16.911373
30.196313	1456.023839	16.916391
30.176800	1483.609735	16.921408
29.964491	1476.972689	16.926426
29.981826	1480.596919	16.931443
30.267445	1508.599263	16.936461
30.512232	1506.365913	16.941479
30.203506	1494.755815	16.946496
30.391738	1497.903087	16.951514
30.764083	1514.331223	16.956531
30.446306	1502.729602	16.961549
30.870274	1509.141632	16.966567
30.476861	1518.444741	16.971584
31.047979	1488.973201	16.976602
31.175105	1458.504656	16.981619
30.612144	1482.174743	16.986637
30.926519	1459.916171	16.991655
30.557481	1463.837760	16.996672
30.890246	1480.321110	17.001690
31.112962	1470.101231	17.006707
30.395629	1459.331055	17.011725
30.754328	1461.060395	17.016743
30.711319	1445.848642	17.021760
30.827440	1457.867877	17.026778
31.244487	1466.480648	17.031795
30.679414	1460.843824	17.036813
31.129278	1474.866622	17.041831
31.034492	1472.134692	17.046848
30.632802	1452.231279	17.051866
31.014132	1472.892092	17.056883
30.772525	1481.962460	17.061901
31.327186	1482.526694	17.066919
31.055578	1501.676017	17.071936
31.233588	1506.609730	17.076954
31.072474	1494.745466	17.081971
31.204616	1487.589880	17.086989
30.928402	1496.829228	17.092007
31.102521	1498.414113	17.097024
31.244611	1500.725394	17.102042
31.255778	1515.608744	17.107059
31.346615	1508.253228	17.112077
31.296905	1485.985214	17.117095
31.383580	1495.772629	17.122112
31.361846	1504.733365	17.127130
31.289584	1503.249798	17.132147
31.201489	1499.621971	17.137165
31.639501	1492.725218	17.142183
31.689800	1515.241976	17.147200
31.826906	1540.083388	17.152218
32.109594	1534.288432	17.157235
31.987289	1512.381612	17.162253
31.824455	1482.406510	17.167271
31.528067	1487.792057	17.172288
31.820399	1490.010511	17.177306
31.606416	1497.698376	17.182323
31.790508	1500.109976	17.187341
32.251804	1515.619182	17.192359
32.101930	1501.701332	17.197376
32.093066	1493.073996	17.202394
31.866206	1507.206098	17.207411
31.877715	1502.130034	17.212429
32.013533	1499.603835	17.217447
32.078132	1519.257538	17.222464
32.281133	1518.195211	17.227482
32.218649	1515.917679	17.232499
31.830565	1515.868385	17.237517
32.057194	1499.402045	17.242535
32.155912	1522.812487	17.247552
32.283607	1528.770347	17.252570
32.329326	1512.654095	17.257587
31.897938	1515.751043	17.262605
31.984316	1514.198060	17.267623
31.867899	1509.183185	17.272640
31.952513	1517.632858	17.277658
32.220800	1520.591450	17.282675
32.210531	1542.456983	17.287693
32.184591	1568.625599	17.292711
32.307681	1557.659197	17.297728
32.180630	1545.810027	17.302746
32.546728	1541.753075	17.307763
32.393116	1556.124735	17.312781
32.571547	1543.849377	17.317799
32.772071	1543.037207	17.322816
32.843434	1542.243528	17.327834
32.941245	1534.841975	17.332851
32.610049	1550.895969	17.337869
32.755408	1548.573850	17.342887
33.119435	1569.327004	17.347904
33.203544	1574.081416	17.352922
33.163347	1546.320488	17.357939
33.044967	1550.016266	17.362957
33.234666	1522.580697	17.367975
32.800010	1543.374385	17.372992
32.969558	1538.186089	17.378010
33.317244	1537.806687	17.383027
33.121569	1550.576683	17.388045
32.996539	1550.324798	17.393063
33.286462	1541.538732	17.398080
33.131650	1561.233865	17.403098
33.164299	1556.953922	17.408115
33.540627	1556.838726	17.413133
33.461275	1573.425707	17.418151
33.545599	1582.315232	17.423168
33.455431	1550.275963	17.428186
33.435979	1564.065738	17.433203
33.194656	1554.534562	17.438221
33.690998	1541.169883	17.443239
33.623886	1557.058516	17.448256
33.574167	1575.277163	17.453274
34.037088	1554.231144	17.458291
33.531797	1565.082560	17.463309
33.663920	1558.278445	17.468327
33.679097	1567.084133	17.473344
33.629735	1559.266235	17.478362
33.740946	1537.616789	17.483379
33.618777	1567.766893	17.488397
33.784500	1561.363043	17.493415
33.817971	1559.661843	17.498432
33.486006	1571.460299	17.503450
33.851995	1570.121579	17.508467
33.801510	1566.871790	17.513485
33.791754	1567.882571	17.518503
33.813186	1558.288586	17.523520
33.972890	1575.983359	17.528538
34.130283	1588.256156	17.533555
34.352133	1599.114178	17.538573
34.330574	1580.720577	17.543591
34.087453	1567.857129	17.548608
34.316961	1577.947793	17.553626
34.474329	1588.983849	17.558643
34.099163	1559.791459	17.563661
34.389634	1580.771896	17.568679
34.142768	1582.824504	17.573696
34.132248	1589.773822	17.578714
34.408220	1601.490041	17.583731
34.130433	1598.125675	17.588749
34.259349	1606.058636	17.593767
34.038526	1601.160471	17.598784
34.487198	1588.320154	17.603802
34.750751	1593.039506	17.608819
34.514117	1577.675111	17.613837
34.348926	1580.588937	17.618855
34.636917	1592.259570	17.623872
34.896566	1591.421489	17.628890
34.815642	1616.763132	17.633907
34.702981	1604.780857	17.638925
34.735791	1598.024723	17.643943
35.149429	1610.224687	17.648960
34.713749	1600.055171	17.653978
35.043328	1588.233930	17.658995
34.841001	1586.541780	17.664013
35.072739	1600.903924	17.669031
34.799312	1594.436932	17.674048
34.779253	1590.024972	17.679066
35.275848	1613.890657	17.684083
34.905721	1600.325978	17.689101
35.169771	1600.469541	17.694119
35.055219	1604.098473	17.699136
34.946678	1590.653631	17.704154
35.128615	1596.017638	17.709171
35.019773	1622.546922	17.714189
35.264717	1631.878142	17.719207
35.471821	1616.001002	17.724224
35.106262	1621.330323	17.729242
35.213151	1626.625952	17.734259
34.968917	1626.281781	17.739277
35.311676	1620.627031	17.744295
35.908090	1627.108723	17.749312
35.601158	1633.799333	17.754330
35.622540	1627.786555	17.759347
35.867112	1621.430070	17.764365
35.777459	1606.773979	17.769383
35.728682	1619.421056	17.774400
35.651704	1629.221627	17.779418
35.941805	1611.248140	17.784435
35.937241	1627.338375	17.789453
35.970061	1625.029824	17.794471
36.398378	1611.806416	17.799488
36.236796	1615.303191	17.804506
36.304988	1616.768123	17.809523
36.113279	1637.547670	17.814541
36.271965	1623.006397	17.819559
36.249681	1607.941814	17.824576
36.139454	1621.270265	17.829594
36.226954	1607.821253	17.834611
36.328978	1622.083717	17.839629
36.197006	1620.874616	17.844647
36.728561	1623.647331	17.849664
36.284589	1621.892867	17.854682
36.238339	1636.446819	17.859699
36.523166	1625.190704	17.864717
36.205252	1611.230066	17.869735
36.240769	1626.826476	17.874752
36.203086	1642.741332	17.879770
36.450824	1617.566594	17.884787
36.386863	1635.372792	17.889805
36.462364	1656.675806	17.894823
36.694162	1633.980721	17.899840
36.603384	1656.404883	17.904858
36.533005	1662.263271	17.909875
36.659228	1656.432820	17.914893
36.738908	1669.493561	17.919911
36.731835	1658.790083	17.924928
36.738453	1656.344154	17.929946
37.056444	1648.383138	17.934963
36.976325	1655.931465	17.939981
36.621283	1660.935900	17.944999
37.117044	1653.566143	17.950016
37.071986	1664.401995	17.955034
37.159087	1668.131547	17.960051
36.934899	1641.872693	17.965069
36.906217	1660.403155	17.970087
36.827480	1644.824449	17.975104
36.896841	1665.232908	17.980122
37.153326	1689.590560	17.985139
37.373306	1678.429456	17.990157
37.111138	1688.999788	17.995175
37.443903	1678.732850	18.000192
37.330673	1697.248102	18.005210
37.281893	1682.809350	18.010227
37.329965	1692.131418	18.015245
37.208105	1687.071920	18.020263
37.692509	1688.307973	18.025280
37.438172	1698.804395	18.030298
37.620829	1678.540001	18.035315
37.876641	1670.455714	18.040333
37.437961	1693.185107	18.045351
37.905054	1694.835354	18.050368
37.887914	1698.746870	18.055386
38.075240	1702.004842	18.060403
37.347093	1688.133577	18.065421
37.826764	1690.804862	18.070439
38.117595	1705.513664	18.075456
38.025078	1693.920134	18.080474
38.078218	1697.793565	18.085491
38.315637	1710.886137	18.090509
38.119973	1717.895237	18.095527
38.426452	1697.103176	18.100544
38.461293	1697.470112	18.105562
38.169939	1700.628091	18.110579
38.427746	1701.314211	18.115597
38.228872	1698.526621	18.120615
38.865809	1714.060241	18.125632
38.418665	1692.242960	18.130650
38.193106	1670.926678	18.135667
38.289522	1679.347133	18.140685
38.490647	1689.425537	18.145703
38.917086	1706.784219	18.150720
38.702819	1689.073382	18.155738
38.346950	1698.194250	18.160755
38.323698	1692.244322	18.165773
38.346191	1694.747213	18.170791
38.540469	1700.858768	18.175808
38.427649	1698.993184	18.180826
38.881105	1703.462631	18.185843
38.613374	1694.729959	18.190861
38.246598	1706.354780	18.195879
38.183666	1701.883744	18.200896
38.304933	1718.863233	18.205914
38.806688	1735.245719	18.210931
38.949173	1735.694257	18.215949
39.017516	1735.337888	18.220967
39.163168	1737.679615	18.225984
38.587807	1729.424545	18.231002
39.085680	1739.579607	18.236019
39.302556	1746.510508	18.241037
39.500127	1748.270642	18.246055
39.461714	1755.092978	18.251072
39.376310	1748.976072	18.256090
38.963487	1726.467283	18.261107
39.409776	1747.853214	18.266125
39.465085	1746.209987	18.271143
39.884314	1739.758167	18.276160
39.653674	1760.557894	18.281178
39.780650	1745.621924	18.286195
39.755601	1721.678372	18.291213
39.478421	1711.963494	18.296231
39.367502	1734.306470	18.301248
39.948719	1726.227717	18.306266
40.167557	1728.595038	18.311283
40.316507	1727.853180	18.316301
39.894865	1728.902910	18.321319
40.119301	1709.719835	18.326336
40.002078	1705.280994	18.331354
39.923642	1711.870899	18.336371
39.836579	1697.748337	18.341389
39.718419	1721.182425	18.346407
39.574531	1702.964866	18.351424
40.061887	1723.003010	18.356442
40.054756	1739.478354	18.361459
40.139843	1752.315876	18.366477
40.077228	1729.515791	18.371495
40.493534	1728.769508	18.376512
40.402575	1741.585435	18.381530
40.269058	1750.997771	18.386547
40.429853	1749.520441	18.391565
40.143509	1757.511673	18.396583
40.360602	1734.158176	18.401600
39.950707	1742.903627	18.406618
40.105736	1748.250583	18.411635
40.487565	1750.341120	18.416653
40.217752	1775.355945	18.421671
40.149410	1777.807338	18.426688
40.615189	1775.403893	18.431706
40.536771	1783.241215	18.436723
40.712630	1768.501238	18.441741
40.531430	1759.009005	18.446759
40.579854	1776.404156	18.451776
40.654585	1777.207130	18.456794
40.805288	1792.296188	18.461811
40.867331	1792.561308	18.466829
41.146908	1795.327280	18.471847
41.555248	1786.575432	18.476864
41.662132	1792.204124	18.481882
41.266502	1802.917530	18.486899
41.396976	1783.640464	18.491917
41.333352	1787.228451	18.496935
41.519001	1795.581774	18.501952
41.465155	1792.641092	18.506970
41.554266	1778.987079	18.511987
41.590048	1749.245508	18.517005
41.371476	1756.855929	18.522023
41.168055	1764.775698	18.527040
41.352847	1766.461288	18.532058
41.071956	1791.685999	18.537075
41.414248	1790.580660	18.542093
41.434932	1792.637989	18.547111
41.446352	1799.490389	18.552128
41.651523	1784.640259	18.557146
41.414607	1777.018761	18.562163
42.043769	1786.184044	18.567181
41.626264	1816.016880	18.572199
41.865757	1822.148566	18.577216
41.865194	1806.998422	18.582234
41.812174	1810.136916	18.587251
41.654924	1819.172680	18.592269
42.182756	1831.757414	18.597287
41.832676	1812.016229	18.602304
42.491269	1813.244763	18.607322
41.922994	1809.213927	18.612339
42.465758	1803.317832	18.617357
42.273903	1814.429869	18.622375
42.279564	1804.828002	18.627392
42.681259	1823.997636	18.632410
42.168258	1838.206062	18.637427
42.316627	1824.004919	18.642445
42.310183	1810.435553	18.647463
41.936638	1819.873425	18.652480
41.966342	1815.277031	18.657498
42.316983	1829.889471	18.662515
43.059829	1849.753205	18.667533
42.609083	1839.751045	18.672551
42.928092	1846.517800	18.677568
43.312453	1859.761970	18.682586
43.132674	1843.969588	18.687603
42.952438	1828.232404	18.692621
42.817494	1824.505865	18.697639
42.531947	1815.986558	18.702656
42.670554	1834.744161	18.707674
42.853050	1852.978001	18.712691
43.054907	1834.547077	18.717709
43.036363	1842.815000	18.722727
43.006832	1850.840499	18.727744
43.043375	1826.001049	18.732762
42.947072	1837.350412	18.737779
43.146356	1849.269910	18.742797
43.181020	1857.875536	18.747815
43.465742	1864.961882	18.752832
43.834271	1872.555442	18.757850
43.787732	1854.717700	18.762867
43.860787	1828.739065	18.767885
43.718318	1830.675358	18.772903
43.602714	1825.373883	18.777920
43.904840	1812.785013	18.782938
43.847538	1830.695434	18.787955
43.795407	1817.186653	18.792973
43.956843	1820.799943	18.797991
43.987209	1828.905181	18.803008
44.284906	1808.366241	18.808026
44.070685	1828.821092	18.813043
43.935153	1823.115609	18.818061
44.066440	1816.633403	18.823079
44.016319	1830.675977	18.828096
44.035283	1826.097197	18.833114
44.027649	1808.912792	18.838131
43.942864	1824.481851	18.843149
44.250486	1825.238273	18.848167
44.110912	1814.502951	18.853184
44.012083	1829.677859	18.858202
43.796237	1839.209247	18.863219
44.236732	1855.051011	18.868237
44.522890	1858.690738	18.873255
44.200698	1847.682283	18.878272
44.425542	1851.474731	18.883290
43.879878	1873.413171	18.888307
44.210797	1878.073752	18.893325
44.310042	1869.464553	18.898343
44.539604	1871.207409	18.903360
44.698456	1898.177681	18.908378
44.565732	1892.679838	18.913395
44.457044	1892.831960	18.918413
44.650658	1909.203362	18.923431
44.436059	1899.633997	18.928448
45.047671	1886.006022	18.933466
45.045346	1917.508497	18.938483
45.221503	1894.674318	18.943501
44.962394	1898.360174	18.948519
44.930687	1912.550439	18.953536
45.347378	1900.082401	18.958554
45.659752	1923.285445	18.963571
45.587405	1885.267384	18.968589
45.430535	1870.775268	18.973607
45.384882	1885.059822	18.978624
45.715516	1857.966337	18.983642
45.387913	1874.276619	18.988659
45.543100	1870.785927	18.993677
45.514828	1868.616840	18.998695
45.615741	1871.821918	19.003712
45.724323	1859.583731	19.008730
45.388766	1886.990638	19.013747
45.769738	1865.537738	19.018765
45.906234	1871.562374	19.023783
45.745323	1884.229086	19.028800
45.649391	1876.208722	19.033818
46.170172	1887.064293	19.038835
46.199891	1911.768376	19.043853
46.137484	1902.035992	19.048871
46.009609	1911.498960	19.053888
46.166901	1898.763416	19.058906
45.947098	1889.745403	19.063923
45.723052	1897.354928	19.068941
46.026651	1887.639122	19.073959
46.013193	1896.806454	19.078976
46.041862	1901.428425	19.083994
46.078022	1889.918778	19.089011
46.099031	1901.685135	19.094029
46.398268	1911.965640	19.099047
46.484509	1930.709775	19.104064
46.355027	1913.603251	19.109082
46.432289	1928.422448	19.114099
46.580180	1945.230301	19.119117
46.626223	1920.978583	19.124135
46.483977	1941.697130	19.129152
47.011823	1923.365940	19.134170
46.527376	1915.646230	19.139187
46.626190	1937.013485	19.144205
46.622961	1918.570789	19.149223
46.714732	1934.992506	19.154240
47.022224	1943.603971	19.159258
47.231153	1948.887081	19.164275
47.572027	1959.191440	19.169293
47.809413	1937.293555	19.174311
47.450136	1933.701287	19.179328
47.506012	1921.643087	19.184346
47.407201	1910.015893	19.189363
47.495277	1908.768929	19.194381
47.365728	1922.042085	19.199399
46.964222	1929.208010	19.204416
46.933134	1906.123863	19.209434
47.268626	1932.231503	19.214451
47.542108	1940.742898	19.219469
47.840786	1942.311872	19.224487
47.459264	1949.476374	19.229504
47.784622	1955.880583	19.234522
47.514031	1947.634761	19.239539
47.708604	1944.392123	19.244557
47.660966	1947.658274	19.249575
47.568115	1955.367188	19.254592
47.636839	1946.470425	19.259610
47.992955	1959.180179	19.264627
47.755580	1950.009158	19.269645
48.089269	1971.202436	19.274663
47.735842	1956.514810	19.279680
48.016044	1962.492806	19.284698
48.066018	1973.400950	19.289715
48.100232	1957.828747	19.294733
48.195988	1961.837794	19.299751
48.082448	1966.152737	19.304768
48.522694	1945.417452	19.309786
48.189691	1964.802161	19.314803
48.179190	1978.414779	19.319821
48.387718	1983.351280	19.324839
48.479087	2008.988365	19.329856
48.660837	1993.302195	19.334874
48.619511	2010.273056	19.339891
48.391766	2005.314597	19.344909
48.790950	1992.612315	19.349927
48.845209	1998.302722	19.354944
48.837299	1979.940731	19.359962
48.853079	1992.298759	19.364979
48.735291	1994.125010	19.369997
49.017533	1994.784767	19.375015
49.025716	2005.903936	19.380032
49.253168	2015.634961	19.385050
49.192262	2009.363733	19.390067
49.175936	2033.395431	19.395085
49.620820	2013.924608	19.400103
49.277573	2004.204815	19.405120
49.356787	2016.388631	19.410138
49.244451	2020.151522	19.415155
49.296941	2025.972621	19.420173
49.650492	2013.888775	19.425191
49.552452	2020.533420	19.430208
49.779816	2024.025058	19.435226
49.533914	2014.702384	19.440243
49.792534	2010.994210	19.445261
49.784837	2009.840019	19.450279
49.720645	2016.515087	19.455296
49.713886	2010.432905	19.460314
49.934520	2009.459642	19.465331
49.653418	2025.104056	19.470349
49.814696	2046.813144	19.475367
49.930692	2050.436852	19.480384
50.070945	2036.112959	19.485402
50.175045	2049.474658	19.490419
50.148386	2064.938901	19.495437
50.370164	2042.153646	19.500455
50.309844	2059.535107	19.505472
50.540046	2052.671856	19.510490
50.586263	2029.431567	19.515507
50.180855	2051.104508	19.520525
50.339302	2032.162308	19.525543
50.210972	2051.553354	19.530560
50.373585	2048.928561	19.535578
50.527826	2071.101853	19.540595
50.534607	2083.389603	19.545613
51.066600	2064.531474	19.550631
51.235999	2078.400325	19.555648
50.900294	2082.110495	19.560666
51.143588	2056.048727	19.565683
50.817528	2068.093195	19.570701
51.165716	2075.615134	19.575719
51.005158	2079.769503	19.580736
51.030681	2064.935897	19.585754
51.153185	2073.681629	19.590771
51.045572	2058.174880	19.595789
51.443989	2049.195038	19.600807
51.068534	2077.433530	19.605824
51.312580	2077.963408	19.610842
51.401859	2067.247265	19.615859
51.262008	2083.057239	19.620877
51.594620	2098.562324	19.625895
51.619469	2091.761234	19.630912
51.432770	2092.494554	19.635930
51.763784	2105.959724	19.640947
51.337984	2098.602604	19.645965
52.009474	2092.776647	19.650983
51.755405	2106.021729	19.656000
51.941287	2087.267806	19.661018
52.124713	2071.916751	19.666035
52.095165	2093.669938	19.671053
52.002894	2099.858726	19.676071
51.628402	2091.895697	19.681088
51.999368	2085.623135	19.686106
52.285445	2083.986611	19.691123
51.943352	2096.097421	19.696141
52.006536	2092.091466	19.701159
52.083641	2120.539846	19.706176
52.199080	2134.890416	19.711194
52.138214	2113.895453	19.716211
52.090196	2112.635732	19.721229
52.507183	2120.464772	19.726247
52.383375	2123.439271	19.731264
52.520911	2153.394780	19.736282
53.017081	2140.377288	19.741299
52.770563	2140.266510	19.746317
53.389853	2149.792932	19.751335
53.386423	2126.555386	19.756352
53.300629	2128.347532	19.761370
53.381427	2126.021136	19.766387
53.172228	2107.615301	19.771405
53.267634	2101.642162	19.776423
53.254958	2111.856453	19.781440
53.391825	2100.435795	19.786458
53.592355	2097.100325	19.791475
53.197467	2105.372324	19.796493
53.300407	2116.670860	19.801511
53.185784	2101.264520	19.806528
53.319058	2109.631985	19.811546
53.549280	2116.768785	19.816563
53.452060	2122.167398	19.821581
53.591773	2131.933366	19.826599
53.719635	2134.475697	19.831616
53.808417	2136.627510	19.836634
53.540129	2143.045367	19.841651
53.525352	2141.461998	19.846669
53.959869	2130.703815	19.851687
53.912924	2138.656175	19.856704
53.643222	2134.148427	19.861722
54.072900	2135.183954	19.866739
53.853352	2144.248999	19.871757
54.044918	2166.609042	19.876775
54.126020	2162.229503	19.881792
54.106361	2164.855361	19.886810
54.351652	2179.442443	19.891827
54.346164	2173.346997	19.896845
54.277559	2160.568953	19.901863
54.232405	2170.587997	19.906880
53.916926	2154.799218	19.911898
54.671295	2179.594181	19.916915
54.700703	2192.021857	19.921933
54.489301	2184.281688	19.926951
54.790204	2186.643293	19.931968
54.874146	2196.447550	19.936986
55.027643	2177.680269	19.942003
54.600527	2193.661134	19.947021
54.880949	2188.806402	19.952039
54.883384	2184.411121	19.957056
54.821716	2204.151911	19.962074
55.039756	2200.425896	19.967091
54.847068	2195.247543	19.972109
54.922358	2189.156751	19.977127
55.150693	2214.774400	19.982144
55.050609	2226.424131	19.987162
55.435001	2213.526704	19.992179
55.330597	2222.478591	19.997197
55.543649	2218.978948	20.002215
55.596095	2211.164263	20.007232
55.498390	2215.384942	20.012250
55.896442	2212.709897	20.017267
55.711358	2224.377216	20.022285
55.999515	2215.135034	20.027303
56.057326	2198.554627	20.032320
55.732419	2211.388153	20.037338
56.067551	2197.270547	20.042355
55.629524	2220.534769	20.047373
56.050656	2243.451966	20.052391
56.173218	2240.639599	20.057408
56.071281	2239.477838	20.062426
56.450855	2252.691551	20.067443
56.618209	2238.429418	20.072461
56.606553	2237.217114	20.077479
56.451755	2243.793492	20.082496
56.410137	2235.067724	20.087514
56.649890	2254.225197	20.092531
56.716466	2248.906755	20.097549
56.691562	2232.068373	20.102567
56.796453	2232.764436	20.107584
56.672199	2245.971653	20.112602
56.944930	2227.912832	20.117619
56.898849	2239.654026	20.122637
56.879459	2237.728751	20.127655
56.940832	2237.745311	20.132672
56.982653	2235.510168	20.137690
57.570747	2244.834557	20.142707
57.233155	2233.533733	20.147725
56.993924	2233.848548	20.152743
57.575912	2236.487673	20.157760
57.137016	2233.651573	20.162778
57.109844	2244.154618	20.167795
57.282675	2230.521009	20.172813
57.473371	2251.654953	20.177831
57.422436	2270.113167	20.182848
57.617716	2264.222362	20.187866
57.568834	2270.326010	20.192883
57.730230	2281.668444	20.197901
57.927711	2262.561760	20.202919
57.658643	2259.314584	20.207936
57.766154	2278.671470	20.212954
57.845798	2261.522521	20.217971
57.598779	2261.843544	20.222989
57.852681	2283.152489	20.228007
58.202803	2282.664913	20.233024
58.256668	2276.526454	20.238042
58.612298	2277.257646	20.243059
58.466250	2301.491485	20.248077
58.438923	2292.467309	20.253095
58.775153	2290.399416	20.258112
58.642623	2283.951852	20.263130
58.737072	2284.851578	20.268147
58.912659	2283.301096	20.273165
58.329007	2276.986341	20.278183
58.950140	2272.913822	20.283200
58.535649	2289.192944	20.288218
58.872191	2273.584534	20.293235
58.937001	2279.550126	20.298253
58.803551	2289.158515	20.303271
58.875438	2274.837333	20.308288
58.576424	2290.824191	20.313306
58.790804	2297.112654	20.318323
58.548637	2277.648360	20.323341
58.604192	2307.197807	20.328359
58.990201	2310.031706	20.333376
59.163931	2302.050500	20.338394
59.278491	2309.773733	20.343411
58.942546	2318.284883	20.348429
59.344335	2312.510893	20.353447
59.373543	2320.462768	20.358464
59.593355	2342.110642	20.363482
59.926961	2351.353155	20.368499
59.680381	2340.165144	20.373517
59.951538	2340.435967	20.378535
60.072835	2345.282588	20.383552
60.038927	2335.072462	20.388570
59.904350	2327.582277	20.393587
59.994100	2332.734255	20.398605
60.228583	2330.241116	20.403623
60.459621	2337.431026	20.408640
60.198606	2340.782218	20.413658
60.311742	2331.220521	20.418675
60.349218	2341.307897	20.423693
60.243142	2330.794200	20.428711
60.300524	2327.614106	20.433728
60.105101	2339.002360	20.438746
60.081943	2330.354971	20.443763
60.602530	2343.166978	20.448781
60.242186	2353.261648	20.453799
60.395644	2352.091329	20.458816
60.385183	2353.849402	20.463834
60.754059	2368.942240	20.468851
61.097729	2385.252451	20.473869
61.140340	2383.735349	20.478887
61.207249	2390.664854	20.483904
61.134974	2402.249305	20.488922
61.158533	2381.786198	20.493939
61.498562	2382.577445	20.498957
61.522269	2388.665208	20.503975
61.300725	2363.765388	20.508992
61.377329	2382.143222	20.514010
61.768437	2366.742005	20.519027
61.713041	2388.132714	20.524045
61.578860	2377.489005	20.529063
61.708802	2381.670929	20.534080
61.655219	2383.421763	20.539098
61.852266	2377.408792	20.544115
62.179552	2376.790953	20.549133
61.586834	2385.470142	20.554151
62.021500	2391.729721	20.559168
61.859750	2383.649605	20.564186
61.943741	2409.960421	20.569203
62.285599	2422.007273	20.574221
62.137226	2411.510154	20.579239
62.580540	2416.143767	20.584256
62.348786	2414.360829	20.589274
62.719627	2393.971398	20.594291
62.840037	2395.702535	20.599309
62.530553	2401.404095	20.604327
62.823032	2403.163088	20.609344
62.635213	2400.156746	20.614362
62.714041	2410.066102	20.619379
62.808973	2406.411947	20.624397
62.857789	2406.650430	20.629415
63.009273	2397.956231	20.634432
62.795890	2384.594936	20.639450
62.702104	2386.695667	20.644467
62.958960	2412.466782	20.649485
62.985952	2439.715465	20.654503
63.253906	2425.403075	20.659520
63.285245	2434.589503	20.664538
62.870403	2442.141666	20.669555
63.229647	2422.112130	20.674573
63.291193	2437.488266	20.679591
63.286286	2441.029601	20.684608
63.088128	2452.731138	20.689626
63.279486	2448.010612	20.694643
63.775044	2445.209590	20.699661
63.564581	2460.254969	20.704679
64.041137	2468.395948	20.709696
63.929047	2480.696968	20.714714
64.061068	2461.649666	20.719731
63.865046	2468.201067	20.724749
63.826244	2484.530106	20.729767
64.125484	2486.887113	20.734784
64.159842	2498.831124	20.739802
64.148376	2487.448271	20.744819
64.591842	2496.321984	20.749837
64.250245	2503.181861	20.754855
64.500607	2502.139395	20.759872
64.257508	2486.622816	20.764890
64.409177	2475.418888	20.769907
64.718740	2505.804953	20.774925
64.646952	2518.561872	20.779943
64.940825	2511.201553	20.784960
64.850578	2536.626556	20.789978
64.854448	2524.639657	20.794995
65.079085	2508.386413	20.800013
64.990412	2524.094893	20.805031
65.247077	2508.722837	20.810048
65.057943	2509.298432	20.815066
65.178761	2523.801801	20.820083
65.286597	2522.912197	20.825101
65.399279	2517.866906	20.830119
65.588309	2512.215192	20.835136
65.897313	2528.470663	20.840154
65.793661	2540.098390	20.845171
65.862658	2539.404151	20.850189
66.110249	2536.508283	20.855207
66.209866	2523.208906	20.860224
66.142632	2490.813246	20.865242
65.572102	2503.148119	20.870259
66.127667	2525.784310	20.875277
65.801838	2530.742274	20.880295
65.725118	2514.314841	20.885312
66.138718	2526.050752	20.890330
66.186684	2538.097844	20.895347
66.269717	2516.773872	20.900365
66.622331	2533.576980	20.905383
66.717366	2527.220035	20.910400
66.774961	2525.633917	20.915418
66.366207	2544.987095	20.920435
66.827757	2527.743642	20.925453
66.612930	2542.064144	20.930471
66.908064	2518.134440	20.935488
66.720702	2537.378988	20.940506
66.789089	2558.648903	20.945523
66.987999	2536.435805	20.950541
66.638697	2551.136161	20.955559
67.091616	2555.897147	20.960576
67.198348	2536.281970	20.965594
67.093454	2535.765263	20.970611
67.187160	2547.360973	20.975629
67.383853	2545.400935	20.980647
67.407873	2570.779361	20.985664
67.501533	2588.501176	20.990682
67.563889	2587.989698	20.995699
67.945294	2565.953850	21.000717
67.535429	2569.454867	21.005735
67.475766	2590.933952	21.010752
67.992158	2575.072322	21.015770
67.705667	2586.724393	21.020787
67.480418	2584.956500	21.025805
67.214277	2581.714872	21.030823
67.918736	2595.520376	21.035840
68.379699	2606.268547	21.040858
67.846500	2597.410649	21.045875
68.240432	2596.560562	21.050893
68.408959	2603.490297	21.055911
68.710016	2605.018600	21.060928
68.805198	2593.978032	21.065946
68.545085	2598.811591	21.070963
69.133809	2590.349514	21.075981
68.404984	2595.786828	21.080999
68.841840	2605.448393	21.086016
69.178507	2619.326112	21.091034
68.988397	2636.674660	21.096051
69.359713	2632.798427	21.101069
69.154314	2637.290721	21.106087
69.355697	2622.172534	21.111104
69.266844	2638.469856	21.116122
69.256158	2623.992137	21.121139
69.548026	2604.699377	21.126157
69.509235	2622.604907	21.131175
69.371708	2614.789131	21.136192
69.610903	2622.070727	21.141210
69.628193	2625.771013	21.146227
69.886138	2617.713335	21.151245
69.743150	2642.078681	21.156263
69.551870	2633.147727	21.161280
69.794245	2614.573662	21.166298
70.268707	2643.447139	21.171315
70.168416	2651.571351	21.176333
70.109485	2672.896711	21.181351
70.093915	2659.443441	21.186368
70.257345	2638.715180	21.191386
70.185524	2644.187818	21.196403
70.517808	2652.596993	21.201421
70.246398	2664.025008	21.206439
70.202608	2639.138275	21.211456
70.518306	2657.696779	21.216474
70.239317	2683.476594	21.221491
70.729882	2669.783005	21.226509
70.725790	2673.046542	21.231527
70.635999	2684.706925	21.236544
70.988881	2695.060676	21.241562
70.908335	2693.351326	21.246579
71.214316	2679.456177	21.251597
71.480035	2695.325923	21.256615
71.387949	2711.418962	21.261632
71.509412	2705.826565	21.266650
71.397277	2700.977005	21.271667
71.724100	2710.332062	21.276685
71.565481	2700.681596	21.281703
71.584819	2689.802882	21.286720
71.893568	2712.837567	21.291738
71.579286	2709.207859	21.296755
71.799706	2689.157616	21.301773
71.923140	2712.456356	21.306791
71.834397	2710.733006	21.311808
72.092895	2688.773388	21.316826
72.109225	2703.490426	21.321843
71.802248	2712.382778	21.326861
72.129448	2722.442801	21.331879
72.061634	2727.580797	21.336896
72.234884	2728.953091	21.341914
72.120247	2746.701046	21.346931
72.583429	2754.104135	21.351949
72.381984	2736.023483	21.356967
72.580154	2734.066524	21.361984
72.792142	2737.951562	21.367002
72.895582	2739.903426	21.372019
72.969737	2748.294098	21.377037
72.712968	2747.414344	21.382055
72.823907	2757.131241	21.387072
73.403177	2742.294540	21.392090
73.085266	2747.346722	21.397107
73.083497	2756.653759	21.402125
73.482067	2750.388277	21.407143
73.295981	2745.694801	21.412160
73.208499	2736.322085	21.417178
73.311287	2766.678081	21.422195
73.391564	2777.905170	21.427213
73.445268	2785.723728	21.432231
73.349314	2798.750781	21.437248
73.723364	2781.185723	21.442266
73.570930	2781.606267	21.447283
73.921171	2792.783048	21.452301
74.301124	2811.222079	21.457319
74.107355	2820.398304	21.462336
74.387841	2803.381486	21.467354
74.102035	2810.790867	21.472371
74.475078	2808.779217	21.477389
74.789859	2793.992274	21.482407
74.382285	2819.179866	21.487424
74.722327	2789.707418	21.492442
74.484097	2803.449233	21.497459
74.648814	2811.061295	21.502477
74.801807	2807.109103	21.507495
74.801025	2812.689534	21.512512
74.872524	2817.773638	21.517530
75.125298	2831.589831	21.522547
75.542260	2819.140987	21.527565
75.374828	2824.114595	21.532583
75.288049	2837.902270	21.537600
75.277526	2811.699695	21.542618
75.324618	2806.586026	21.547635
75.524593	2830.588934	21.552653
75.790935	2816.197718	21.557671
75.695237	2820.228885	21.562688
75.891350	2825.857286	21.567706
75.686799	2817.258492	21.572723
75.755587	2829.319692	21.577741
76.085684	2842.972350	21.582759
76.038195	2833.889188	21.587776
76.259540	2843.685521	21.592794
76.477337	2855.988225	21.597811
76.221531	2849.178756	21.602829
76.517612	2838.821848	21.607847
76.458801	2829.677772	21.612864
76.535833	2853.157795	21.617882
76.456137	2856.531490	21.622899
76.816787	2851.945640	21.627917
76.630767	2840.770678	21.632935
76.382285	2847.408261	21.637952
76.869346	2867.741224	21.642970
76.953490	2870.562915	21.647987
76.880823	2875.401210	21.653005
76.925674	2896.316866	21.658023
76.905594	2883.637276	21.663040
76.703928	2872.258801	21.668058
76.830676	2881.935767	21.673075
77.201512	2885.827463	21.678093
77.317389	2898.586949	21.683111
77.209954	2927.411663	21.688128
77.492786	2901.109481	21.693146
77.412161	2906.528359	21.698163
77.538023	2912.448090	21.703181
77.933451	2922.434772	21.708199
77.725064	2934.307634	21.713216
78.212156	2926.228660	21.718234
78.215692	2946.305450	21.723251
78.364884	2931.541212	21.728269
78.604045	2913.710730	21.733287
78.420968	2926.762917	21.738304
78.764132	2936.246105	21.743322
78.494648	2922.738709	21.748339
78.260658	2930.368887	21.753357
78.421982	2928.781530	21.758375
78.479763	2935.526198	21.763392
78.523918	2927.531244	21.768410
78.404054	2937.571005	21.773427
78.567367	2947.953497	21.778445
79.165182	2957.010018	21.783463
78.913953	2969.717641	21.788480
78.789851	2943.142911	21.793498
79.237315	2960.044184	21.798515
79.202468	2992.373918	21.803533
79.759928	2981.287585	21.808551
79.676870	2985.927459	21.813568
79.748901	2995.628498	21.818586
79.584693	2980.726851	21.823603
79.753777	2992.886551	21.828621
79.923603	2973.957749	21.833639
79.880179	2987.721073	21.838656
79.925485	2971.608576	21.843674
80.087613	2991.758223	21.848691
80.079907	2976.269171	21.853709
80.330386	2975.403012	21.858727
80.348878	3002.148448	21.863744
80.783680	3015.289725	21.868762
80.685874	3013.902051	21.873779
80.550419	2994.006666	21.878797
81.060061	3004.372709	21.883815
80.562710	2991.188700	21.888832
80.849514	2992.667830	21.893850
81.081362	2993.254378	21.898867
80.753327	2988.122331	21.903885
81.019780	2989.514086	21.908903
80.918831	3001.178127	21.913920
81.226491	2994.009766	21.918938
81.492297	2981.720005	21.923955
80.919351	2993.491954	21.928973
80.811874	3034.492389	21.933991
81.187401	3022.682831	21.939008
81.626020	3045.026161	21.944026
81.693192	3026.384894	21.949043
81.649297	3022.054996	21.954061
81.917076	3039.291918	21.959079
81.786608	3050.412513	21.964096
82.151902	3044.546657	21.969114
82.018602	3056.769367	21.974131
81.824116	3060.005794	21.979149
82.037981	3044.167892	21.984167
82.108407	3057.258210	21.989184
82.445565	3061.189175	21.994202
82.530118	3068.815202	21.999219
82.387709	3083.043144	22.004237
82.770225	3084.877291	22.009255
82.768269	3086.179369	22.014272
82.827362	3060.653962	22.019290
82.964427	3082.121299	22.024307
83.009020	3071.869959	22.029325
82.976152	3061.032085	22.034343
83.028379	3085.439880	22.039360
83.098575	3072.738525	22.044378
83.527107	3059.367209	22.049395
83.456669	3078.674203	22.054413
83.848319	3075.598937	22.059431
83.742276	3065.011117	22.064448
83.570012	3081.118185	22.069466
83.608207	3070.998991	22.074483
83.858922	3104.849900	22.079501
83.928635	3094.793780	22.084519
83.798392	3102.702928	22.089536
83.950565	3095.861361	22.094554
84.282665	3107.778492	22.099571
83.936894	3102.093101	22.104589
84.390740	3081.930161	22.109607
84.217163	3119.473047	22.114624
84.505585	3117.872542	22.119642
84.461792	3131.875202	22.124659
84.708386	3113.633858	22.129677
85.180819	3128.434182	22.134695
85.130818	3125.701936	22.139712
84.892531	3126.757079	22.144730
85.386798	3128.240321	22.149747
84.748539	3127.374378	22.154765
84.853648	3132.228647	22.159783
85.005281	3132.264739	22.164800
85.221865	3126.977302	22.169818
85.097692	3144.177941	22.174835
85.287170	3142.342630	22.179853
85.205933	3140.074154	22.184871
85.509580	3146.969013	22.189888
85.418299	3168.209076	22.194906
85.852211	3187.499982	22.199923
85.552174	3172.767822	22.204941
85.882364	3165.906059	22.209959
85.815726	3173.399265	22.214976
85.911759	3208.264043	22.219994
86.264863	3197.290057	22.225011
85.853340	3209.293341	22.230029
86.488554	3199.979050	22.235047
86.849367	3197.092301	22.240064
86.681037	3205.640011	22.245082
87.091053	3194.832391	22.250099
86.857053	3193.851024	22.255117
87.084278	3204.642965	22.260135
86.925107	3211.426951	22.265152
87.014134	3215.785335	22.270170
87.280281	3210.324342	22.275187
87.168221	3228.295630	22.280205
87.294859	3209.777963	22.285223
87.577750	3217.204574	22.290240
87.590973	3240.458552	22.295258
87.845199	3228.831464	22.300275
87.737456	3221.135249	22.305293
87.445124	3221.182506	22.310311
87.447129	3223.816479	22.315328
87.860899	3242.391763	22.320346
88.170262	3237.126355	22.325363
88.213981	3251.474074	22.330381
88.316881	3250.433685	22.335399
88.426301	3241.108825	22.340416
88.284242	3246.830266	22.345434
88.729817	3248.461710	22.350451
88.765248	3236.472978	22.355469
88.738311	3228.442573	22.360487
88.735656	3249.931855	22.365504
88.681127	3258.521609	22.370522
88.822076	3245.101800	22.375539
88.648002	3248.323280	22.380557
88.619383	3262.605805	22.385575
89.256787	3271.668176	22.390592
89.205038	3270.945437	22.395610
89.375327	3284.483770	22.400627
89.227149	3284.490672	22.405645
89.366209	3278.077920	22.410663
89.648552	3290.803137	22.415680
89.339408	3287.945001	22.420698
89.783275	3303.965250	22.425715
89.997894	3299.751398	22.430733
90.021954	3286.819915	22.435751
90.147319	3302.753438	22.440768
89.995027	3312.181343	22.445786
90.187286	3289.563380	22.450803
90.337494	3286.663389	22.455821
90.387039	3312.589354	22.460839
90.340612	3333.131945	22.465856
90.624536	3346.332490	22.470874
90.912584	3315.665780	22.475891
90.778184	3311.373785	22.480909
90.827322	3321.338629	22.485927
90.808227	3330.755754	22.490944
90.722982	3337.106950	22.495962
91.104296	3339.196814	22.500979
90.977437	3338.461880	22.505997
90.842835	3359.024981	22.511015
91.008736	3364.229479	22.516032
91.409837	3358.017858	22.521050
91.149530	3393.699938	22.526067
91.648545	3395.030272	22.531085
91.579390	3383.697624	22.536103
91.839732	3385.767331	22.541120
91.462077	3371.938274	22.546138
92.053924	3386.600032	22.551155
92.056824	3416.887996	22.556173
92.031691	3415.369390	22.561191
92.404655	3419.913765	22.566208
92.307141	3413.609728	22.571226
92.547974	3395.825852	22.576243
92.494580	3424.372313	22.581261
92.687546	3432.886625	22.586279
92.716964	3434.793335	22.591296
92.928551	3443.467159	22.596314
93.182449	3432.669228	22.601331
93.286467	3425.157189	22.606349
93.379866	3425.445796	22.611367
93.409554	3449.259324	22.616384
93.187348	3434.220772	22.621402
93.324539	3443.397396	22.626419
93.380858	3440.568398	22.631437
93.522744	3466.861021	22.636455
93.827899	3445.988977	22.641472
93.947502	3447.063930	22.646490
93.950295	3465.082453	22.651507
94.384081	3455.904633	22.656525
93.884463	3451.832580	22.661543
94.390809	3463.747569	22.666560
94.034333	3455.759888	22.671578
94.214432	3458.585711	22.676595
94.224406	3483.575672	22.681613
94.348205	3505.392414	22.686631
94.604447	3492.002350	22.691648
94.314677	3492.613899	22.696666
94.540492	3496.631479	22.701683
94.489763	3494.360665	22.706701
94.661052	3501.610401	22.711719
95.073048	3520.987820	22.716736
95.046340	3515.159008	22.721754
95.111326	3512.589566	22.726771
95.088702	3548.076834	22.731789
95.040108	3544.482739	22.736807
95.593341	3529.997395	22.741824
95.862430	3543.053132	22.746842
96.170651	3547.509826	22.751859
96.101241	3542.936380	22.756877
95.669441	3524.732842	22.761895
96.421925	3535.776379	22.766912
96.108130	3535.802382	22.771930
96.391045	3536.839136	22.776947
96.409862	3552.893862	22.781965
96.313424	3570.462014	22.786983
96.796891	3552.333755	22.792000
96.697676	3569.326823	22.797018
96.964157	3554.775464	22.802035
96.820972	3556.452661	22.807053
97.021677	3555.481123	22.812071
97.228510	3551.919812	22.817088
96.817169	3558.186611	22.822106
97.116257	3561.818116	22.827123
97.191480	3585.505442	22.832141
97.097514	3575.416023	22.837159
97.632199	3583.623381	22.842176
97.736235	3589.796368	22.847194
97.585133	3578.920980	22.852211
97.879332	3589.006906	22.857229
97.542521	3619.755701	22.862247
98.129499	3603.251880	22.867264
98.026844	3608.240229	22.872282
98.218860	3608.000774	22.877299
98.329646	3602.035832	22.882317
98.021432	3613.367487	22.887335
98.518379	3634.441309	22.892352
98.439393	3651.389788	22.897370
98.263767	3634.629697	22.902387
98.433564	3648.608356	22.907405
98.466678	3646.509478	22.912423
98.906044	3661.415379	22.917440
98.759348	3670.005042	22.922458
99.425756	3656.860420	22.927475
99.419370	3670.294635	22.932493
99.277602	3663.764756	22.937511
99.983697	3682.312738	22.942528
100.077292	3674.339540	22.947546
100.239035	3686.177404	22.952563
100.264542	3669.780071	22.957581
100.226268	3654.693589	22.962599
100.245965	3634.665053	22.967616
100.312693	3643.168651	22.972634
100.489604	3653.706054	22.977651
100.556699	3656.551768	22.982669
100.518351	3672.821560	22.987687
100.718659	3680.109495	22.992704
100.939490	3672.881357	22.997722
100.563536	3683.224529	23.002739
100.893597	3678.197660	23.007757
100.838742	3669.421696	23.012775
101.097010	3671.467574	23.017792
100.743453	3682.307597	23.022810
100.595308	3673.004568	23.027827
101.258316	3701.369384	23.032845
100.819540	3709.972494	23.037863
101.120826	3697.852472	23.042880
101.334035	3705.680570	23.047898
101.340095	3735.007683	23.052915
101.807106	3725.256735	23.057933
101.727629	3753.786266	23.062951
101.928342	3742.608550	23.067968
102.061636	3753.874830	23.072986
102.233057	3736.067193	23.078003
102.422533	3728.207052	23.083021
102.059757	3760.344765	23.088039
102.343945	3747.351213	23.093056
102.113938	3767.069462	23.098074
102.210763	3783.853612	23.103091
102.640692	3791.393596	23.108109
102.845017	3792.918323	23.113127
103.025944	3781.114561	23.118144
102.903704	3805.568464	23.123162
103.261255	3795.562154	23.128179
103.528530	3798.952139	23.133197
103.479678	3795.108242	23.138215
103.715923	3816.817872	23.143232
103.781736	3830.855609	23.148250
103.597814	3827.931406	23.153267
103.900889	3834.469016	23.158285
103.722211	3815.946552	23.163303
104.131107	3816.144059	23.168320
104.152766	3834.273272	23.173338
104.117042	3832.218222	23.178355
104.201770	3851.074780	23.183373
104.508871	3873.512497	23.188391
104.768257	3863.032238	23.193408
104.670956	3851.931443	23.198426
104.633808	3859.686429	23.203443
104.813186	3862.348087	23.208461
104.750971	3866.314941	23.213479
104.936493	3888.681438	23.218496
105.465834	3873.777701	23.223514
105.343014	3892.413504	23.228531
105.579082	3873.267944	23.233549
105.171733	3874.091639	23.238567
105.426438	3901.951496	23.243584
105.410542	3899.505191	23.248602
105.177717	3909.457759	23.253619
105.653713	3927.556884	23.258637
105.664059	3944.335026	23.263655
106.070776	3929.667628	23.268672
106.387031	3935.372641	23.273690
106.273436	3941.623461	23.278707
106.665814	3934.018253	23.283725
107.077248	3954.932245	23.288743
106.899648	3947.205480	23.293760
107.109624	3938.262774	23.298778
107.099606	3964.214633	23.303795
107.474328	3954.348289	23.308813
107.279270	3960.000408	23.313831
107.694467	3965.650502	23.318848
107.609008	3944.575026	23.323866
107.718352	3964.396889	23.328883
107.594440	3948.657380	23.333901
107.647547	3963.136878	23.338919
107.688761	3965.028516	23.343936
107.815727	3947.948020	23.348954
107.812885	3960.796305	23.353971
107.764351	3953.280087	23.358989
108.005112	3981.229393	23.364007
107.807984	3986.829899	23.369024
108.063106	3975.165296	23.374042
108.116455	4000.438672	23.379059
108.300040	4001.832012	23.384077
108.197540	4011.996561	23.389095
108.314373	4005.168307	23.394112
108.642103	4033.029325	23.399130
108.524252	4034.886629	23.404147
108.831191	4023.148471	23.409165
108.934199	4042.369545	23.414183
109.243846	4074.036576	23.419200
109.374591	4069.087398	23.424218
109.415209	4073.157384	23.429235
109.672898	4079.608312	23.434253
109.440988	4057.237657	23.439271
109.583774	4082.828262	23.444288
110.189126	4094.025053	23.449306
109.924519	4090.904497	23.454323
110.403215	4095.367826	23.459341
110.260493	4116.414549	23.464359
110.429001	4093.148582	23.469376
110.481560	4103.996983	23.474394
110.970935	4123.210609	23.479411
111.172842	4118.849234	23.484429
110.974195	4127.700282	23.489447
111.194414	4139.593395	23.494464
111.330934	4127.491604	23.499482
111.277017	4107.405136	23.504499
111.601266	4113.766343	23.509517
111.247197	4104.943123	23.514535
111.250479	4130.192702	23.519552
111.631607	4128.170497	23.524570
111.716525	4151.528756	23.529587
112.209129	4137.159161	23.534605
112.241378	4147.852689	23.539623
112.070182	4157.198408	23.544640
112.131750	4154.398333	23.549658
112.231770	4181.657117	23.554675
112.218566	4172.579903	23.559693
112.526377	4187.908429	23.564711
112.348121	4169.369528	23.569728
112.717437	4191.944665	23.574746
112.578448	4219.767791	23.579763
113.413541	4212.258184	23.584781
113.301602	4204.197225	23.589799
113.166173	4215.146450	23.594816
113.465952	4204.066005	23.599834
113.560838	4212.640653	23.604851
113.762010	4232.354776	23.609869
113.659936	4248.882938	23.614887
113.711678	4239.289067	23.619904
114.265002	4221.248876	23.624922
114.117109	4236.416148	23.629939
114.332239	4239.127473	23.634957
114.358026	4229.959139	23.639975
114.419306	4253.742702	23.644992
114.413550	4262.077325	23.650010
114.457498	4267.800294	23.655027
114.453031	4275.137504	23.660045
114.652351	4260.991449	23.665063
114.657633	4279.066017	23.670080
114.894853	4290.715501	23.675098
114.747909	4290.095843	23.680115
115.080829	4308.517866	23.685133
115.491812	4326.640407	23.690151
115.726514	4315.323400	23.695168
116.005619	4302.731786	23.700186
115.828086	4318.803610	23.705203
116.107240	4313.790462	23.710221
115.939536	4310.505034	23.715239
116.236673	4321.929294	23.720256
116.649528	4313.305199	23.725274
116.438712	4313.801961	23.730291
116.487953	4306.722548	23.735309
116.777297	4316.882389	23.740327
116.914902	4318.446736	23.745344
117.044971	4324.415328	23.750362
117.262562	4335.520470	23.755379
117.142705	4319.044112	23.760397
117.087392	4337.738190	23.765415
117.138036	4325.983100	23.770432
117.610564	4321.649389	23.775450
117.622146	4343.889386	23.780467
117.665611	4320.374064	23.785485
117.553075	4339.676398	23.790503
117.425490	4354.360130	23.795520
117.744500	4356.880694	23.800538
117.414603	4368.168844	23.805555
117.843693	4391.389100	23.810573
117.978340	4385.638018	23.815591
117.917956	4395.114777	23.820608
118.424923	4410.027555	23.825626
118.573458	4399.497932	23.830643
118.646313	4421.051163	23.835661
118.926488	4418.324757	23.840679
119.136417	4427.331290	23.845696
118.964895	4451.189449	23.850714
119.057271	4454.326204	23.855731
119.582113	4436.103075	23.860749
119.652688	4454.095800	23.865767
119.400103	4445.173727	23.870784
119.482490	4455.153689	23.875802
119.453113	4481.102131	23.880819
119.720817	4467.619376	23.885837
119.994475	4501.873875	23.890855
120.344234	4513.612803	23.895872
120.508149	4504.014799	23.900890
120.804966	4505.095781	23.905907
120.697764	4504.835286	23.910925
120.918803	4490.634647	23.915943
120.537972	4507.980389	23.920960
121.130291	4531.651431	23.925978
121.053333	4526.063214	23.930995
121.108267	4522.477178	23.936013
121.915439	4523.856105	23.941031
121.555251	4529.692012	23.946048
121.669217	4533.597641	23.951066
121.846377	4524.661596	23.956083
121.966578	4561.210828	23.961101
122.219934	4555.124720	23.966119
121.850421	4566.797506	23.971136
122.385294	4573.883535	23.976154
122.266839	4568.989155	23.981171
122.427664	4569.817027	23.986189
122.759437	4579.479487	23.991207
122.533485	4583.127522	23.996224
122.863938	4590.325683	24.001242
122.804531	4604.377922	24.006259
122.866560	4590.681412	24.011277
123.079119	4598.899041	24.016295
123.158778	4624.177354	24.021312
123.086609	4623.765795	24.026330
123.466028	4617.998591	24.031347
123.057078	4636.806187	24.036365
123.468667	4645.750785	24.041383
123.510202	4645.247997	24.046400
123.828887	4655.612264	24.051418
124.163157	4666.279077	24.056435
124.258981	4663.556321	24.061453
124.644222	4684.047286	24.066471
124.331001	4686.311750	24.071488
124.808002	4666.620682	24.076506
124.422652	4685.061449	24.081523
124.706301	4680.912392	24.086541
124.732337	4694.648236	24.091559
124.998815	4695.790149	24.096576
125.137790	4697.202735	24.101594
125.195860	4701.621181	24.106611
125.141692	4723.359599	24.111629
125.553433	4733.993973	24.116647
125.317217	4736.288239	24.121664
125.805088	4720.222446	24.126682
126.151911	4750.139063	24.131699
126.176962	4772.701069	24.136717
126.629015	4751.597882	24.141735
126.525981	4775.627504	24.146752
126.805140	4763.299681	24.151770
126.623781	4738.596867	24.156787
126.586123	4767.206192	24.161805
126.945627	4759.419010	24.166823
126.974661	4784.235873	24.171840
127.297717	4801.380591	24.176858
127.399883	4792.560327	24.181875
127.452841	4778.578931	24.186893
127.475798	4788.050426	24.191911
127.517219	4814.189300	24.196928
127.851583	4812.608201	24.201946
127.989380	4808.155653	24.206963
127.832863	4824.253660	24.211981
128.024938	4808.033899	24.216999
128.460306	4828.161655	24.222016
128.498604	4853.292452	24.227034
128.515466	4834.372482	24.232051
128.530877	4849.219665	24.237069
128.728125	4850.992716	24.242087
128.529413	4860.868993	24.247104
128.673177	4877.032791	24.252122
128.784707	4864.228649	24.257139
128.710791	4886.550086	24.262157
129.323071	4901.388063	24.267175
129.185289	4915.884245	24.272192
129.687139	4923.295973	24.277210
130.019648	4941.432595	24.282227
130.214275	4934.104463	24.287245
130.414279	4910.020253	24.292263
130.316648	4917.251508	24.297280
130.538576	4924.683112	24.302298
130.849490	4952.899746	24.307315
130.630487	4948.554936	24.312333
131.513588	4942.104381	24.317351
131.102051	4959.381681	24.322368
131.468083	4938.847971	24.327386
131.279956	4947.030419	24.332403
131.273302	4969.800313	24.337421
131.382130	4958.861121	24.342439
131.463596	4957.172977	24.347456
131.728682	4975.747162	24.352474
131.691041	4965.744774	24.357491
132.004875	4982.206959	24.362509
132.349633	4969.674038	24.367527
132.117611	4983.775222	24.372544
132.096310	4995.572680	24.377562
132.235289	5002.728656	24.382579
132.404157	5022.952671	24.387597
132.319190	5007.806051	24.392615
132.537943	5009.846829	24.397632
132.658484	5016.239708	24.402650
133.042134	5034.706576	24.407667
132.714549	5063.174981	24.412685
133.411850	5051.579029	24.417703
133.167324	5055.604658	24.422720
133.183205	5058.260862	24.427738
133.597420	5090.050094	24.432755
133.638958	5099.432880	24.437773
133.813118	5095.060070	24.442791
134.187271	5106.235960	24.447808
133.927445	5093.262280	24.452826
134.539468	5107.243398	24.457843
134.394059	5134.565276	24.462861
135.015076	5125.036244	24.467879
134.809995	5130.839264	24.472896
135.029987	5131.006985	24.477914
135.330917	5144.390317	24.482931
135.577344	5158.080704	24.487949
135.824974	5146.031810	24.492967
135.608119	5137.145560	24.497984
135.555866	5141.308734	24.503002
135.724657	5160.699854	24.508019
135.645640	5178.628765	24.513037
136.064276	5165.462600	24.518055
136.048789	5180.250244	24.523072
136.312871	5185.686777	24.528090
136.508580	5187.254998	24.533107
136.476656	5222.482074	24.538125
136.871710	5206.463405	24.543143
136.641125	5219.653519	24.548160
137.039279	5236.248895	24.553178
137.388321	5241.794641	24.558195
137.160616	5245.837618	24.563213
137.432287	5235.633155	24.568231
137.632963	5249.449296	24.573248
138.053677	5262.798369	24.578266
138.390593	5261.208537	24.583283
137.982501	5270.690920	24.588301
138.136644	5276.562986	24.593319
138.470401	5267.642767	24.598336
138.651155	5269.868997	24.603354
138.601892	5285.126113	24.608371
138.507538	5286.428486	24.613389
139.058318	5278.424789	24.618407
139.238994	5289.699318	24.623424
139.122263	5303.221882	24.628442
139.372936	5293.266528	24.633459
139.236692	5309.885717	24.638477
139.471948	5310.852910	24.643495
139.587007	5318.861828	24.648512
139.746593	5323.506204	24.653530
139.987266	5341.459251	24.658547
139.796022	5346.379328	24.663565
139.874504	5361.973296	24.668583
140.042693	5361.873587	24.673600
140.313100	5364.434634	24.678618
140.626501	5376.794813	24.683635
140.740214	5392.905055	24.688653
140.851418	5392.087965	24.693671
141.085089	5390.995118	24.698688
140.892017	5395.811571	24.703706
141.212438	5412.845192	24.708723
141.554472	5410.208005	24.713741
141.788245	5426.182691	24.718759
142.301780	5443.374601	24.723776
141.920538	5427.467836	24.728794
141.864550	5419.430466	24.733811
141.900082	5432.814199	24.738829
142.314307	5418.700483	24.743847
142.282222	5455.446672	24.748864
142.534751	5455.762570	24.753882
142.800885	5446.944766	24.758899
142.598361	5480.748985	24.763917
142.753682	5484.843304	24.768935
142.812601	5484.160050	24.773952
143.288530	5501.251541	24.778970
143.155508	5502.459529	24.783987
143.402899	5516.938689	24.789005
143.274612	5530.107437	24.794023
143.665174	5538.139452	24.799040
143.553398	5555.948613	24.804058
143.834771	5559.124445	24.809075
144.069512	5556.099432	24.814093
144.505985	5578.763529	24.819111
144.343300	5588.239806	24.824128
144.283483	5594.611541	24.829146
144.799062	5611.270596	24.834163
144.857953	5630.720227	24.839181
145.432362	5604.806063	24.844199
145.485332	5627.807235	24.849216
145.153748	5624.349383	24.854234
145.527537	5622.722319	24.859251
145.569725	5655.681323	24.864269
145.868275	5650.694860	24.869287
146.120475	5673.202919	24.874304
146.208072	5676.269055	24.879322
146.433110	5674.236621	24.884339
146.519485	5682.661118	24.889357
146.966729	5693.481241	24.894375
146.748118	5714.977727	24.899392
146.711842	5700.669285	24.904410
147.494836	5697.412701	24.909427
147.571601	5707.641260	24.914445
147.549136	5708.443967	24.919463
147.628997	5730.886486	24.924480
147.453209	5729.914427	24.929498
147.746849	5741.301728	24.934515
147.877745	5746.055308	24.939533
147.958495	5768.424895	24.944551
148.419097	5756.779343	24.949568
148.591830	5750.445449	24.954586
148.951027	5762.009345	24.959603
149.069446	5763.344320	24.964621
149.007278	5771.043759	24.969639
149.353699	5786.658450	24.974656
149.169875	5778.724700	24.979674
149.503906	5776.756531	24.984691
149.368834	5788.715917	24.989709
149.549099	5811.793970	24.994727
149.843899	5792.407201	24.999744
149.744175	5794.182578	25.004762
150.039209	5814.947045	25.009779
150.175252	5846.665278	25.014797
149.955492	5841.194284	25.019815
150.701961	5825.690180	25.024832
150.781280	5857.247717	25.029850
150.875981	5866.454847	25.034867
151.014881	5861.955358	25.039885
151.257931	5883.030887	25.044903
151.303872	5887.026056	25.049920
151.086817	5886.383661	25.054938
151.547236	5896.715497	25.059955
151.598352	5901.160632	25.064973
151.381345	5898.532662	25.069991
151.783188	5916.292013	25.075008
151.598996	5937.932735	25.080026
152.177238	5939.413020	25.085043
152.273394	5953.752998	25.090061
152.171268	5959.802322	25.095079
153.044715	5947.741931	25.100096
152.895462	5965.556570	25.105114
153.311254	5977.495554	25.110131
153.562243	5972.834195	25.115149
153.398516	5979.410279	25.120167
153.923633	5981.023371	25.125184
153.745873	5981.752926	25.130202
153.889607	5992.256454	25.135219
153.853419	6003.325978	25.140237
154.147479	6017.923099	25.145255
154.449856	6004.291153	25.150272
154.324465	6003.809210	25.155290
154.505248	6040.780677	25.160307
154.751867	6057.732704	25.165325
154.930934	6041.812655	25.170343
155.105295	6042.908471	25.175360
155.094284	6067.496575	25.180378
155.570660	6074.079143	25.185395
155.447247	6089.417019	25.190413
155.464931	6080.095774	25.195431
155.939190	6089.886827	25.200448
155.769487	6108.066847	25.205466
155.839378	6100.971396	25.210483
156.057929	6126.009100	25.215501
156.295222	6144.019541	25.220519
156.884803	6120.369529	25.225536
156.837467	6135.890958	25.230554
156.760580	6162.698546	25.235571
157.016731	6160.111257	25.240589
157.076347	6175.281954	25.245607
157.822591	6198.916328	25.250624
157.759003	6195.208142	25.255642
157.815054	6203.183167	25.260659
158.022619	6200.379470	25.265677
157.878295	6194.455691	25.270695
158.180835	6206.420652	25.275712
158.069147	6244.973346	25.280730
158.182714	6235.649158	25.285747
158.424202	6247.467926	25.290765
158.773712	6260.187440	25.295783
158.975131	6262.869496	25.300800
158.910218	6274.564094	25.305818
159.293139	6283.386019	25.310835
159.614398	6280.228845	25.315853
159.670592	6311.589134	25.320871
160.087264	6324.612988	25.325888
160.133981	6313.721304	25.330906
160.206706	6294.360766	25.335923
160.641674	6319.532328	25.340941
160.472414	6341.338478	25.345959
160.957940	6337.430065	25.350976
160.688577	6345.697538	25.355994
161.168799	6352.855236	25.361011
161.265609	6351.701073	25.366029
161.667650	6355.961175	25.371047
161.442180	6371.557158	25.376064
161.638300	6359.150847	25.381082
161.635490	6376.736619	25.386099
161.840139	6406.585021	25.391117
161.945569	6397.632592	25.396135
162.087303	6384.546597	25.401152
162.025555	6414.566604	25.406170
162.361524	6430.910906	25.411187
162.521065	6430.393288	25.416205
162.573346	6449.345767	25.421223
162.821271	6448.708809	25.426240
162.927468	6480.058811	25.431258
163.021998	6463.862114	25.436275
163.272592	6484.858067	25.441293
163.098719	6491.804190	25.446311
163.493077	6492.721154	25.451328
163.424490	6520.983255	25.456346
163.737637	6537.464130	25.461363
164.239747	6540.177662	25.466381
164.248832	6566.212204	25.471399
164.700096	6556.344178	25.476416
164.838866	6564.654970	25.481434
165.062516	6591.236447	25.486451
165.606703	6579.002398	25.491469
165.499279	6612.205092	25.496487
165.673024	6591.925424	25.501504
165.700999	6598.268493	25.506522
165.515770	6618.907851	25.511539
166.151943	6601.261518	25.516557
165.753257	6629.241706	25.521575
166.388181	6652.240757	25.526592
166.275838	6661.957818	25.531610
166.367389	6662.716928	25.536627
166.906703	6671.108461	25.541645
166.476985	6673.542471	25.546663
167.005993	6684.472231	25.551680
166.996888	6709.203957	25.556698
167.161284	6723.663695	25.561715
167.653980	6726.941875	25.566733
167.546079	6746.672453	25.571751
167.898139	6750.932261	25.576768
167.950381	6751.129691	25.581786
168.336087	6770.436177	25.586803
168.698790	6781.856927	25.591821
168.156791	6784.085463	25.596839
168.619891	6793.617354	25.601856
168.861938	6810.832404	25.606874
168.982564	6840.580542	25.611891
169.499451	6835.122142	25.616909
169.345995	6841.105081	25.621927
169.479252	6857.456155	25.626944
169.455824	6855.727652	25.631962
170.237148	6869.674512	25.636979
170.322603	6898.013427	25.641997
170.362323	6896.611143	25.647015
170.551146	6894.319543	25.652032
170.584714	6896.496304	25.657050
170.491678	6907.895587	25.662067
170.887649	6922.343626	25.667085
171.198810	6938.187373	25.672103
171.460366	6949.292631	25.677120
171.396202	6968.297661	25.682138
171.660705	6976.372907	25.687156
171.919102	6972.012433	25.692173
171.993969	6995.821163	25.697191
171.994501	6999.571329	25.702208
172.738358	7012.095571	25.707226
172.141543	7036.437846	25.712244
173.041039	7020.791522	25.717261
173.032116	7047.957554	25.722279
173.423977	7049.345110	25.727296
173.623441	7035.560749	25.732314
173.757918	7047.358428	25.737332
173.807787	7049.399427	25.742349
173.903844	7062.315433	25.747367
174.080014	7092.437603	25.752384
173.967398	7090.600171	25.757402
173.905061	7086.102870	25.762420
174.498237	7098.404800	25.767437
174.684769	7102.303810	25.772455
174.843639	7092.612916	25.777472
175.159918	7107.412926	25.782490
174.886868	7109.271035	25.787508
175.218462	7129.095640	25.792525
175.257893	7158.115169	25.797543
175.611661	7151.679528	25.802560
176.026453	7166.815731	25.807578
175.906421	7177.008860	25.812596
176.336322	7161.598675	25.817613
176.177761	7188.703049	25.822631
176.748646	7218.684246	25.827648
176.657424	7203.886189	25.832666
177.057826	7207.656173	25.837684
177.281727	7205.496154	25.842701
177.517507	7204.953314	25.847719
177.733347	7227.447964	25.852736
178.050610	7223.858915	25.857754
177.920966	7223.256752	25.862772
178.215892	7243.145837	25.867789
178.131451	7253.636331	25.872807
178.268006	7249.852692	25.877824
178.365945	7259.761790	25.882842
178.344913	7281.034043	25.887860
178.577632	7305.864962	25.892877
178.612021	7307.757348	25.897895
178.823794	7331.950724	25.902912
179.158829	7333.176015	25.907930
179.292665	7345.155156	25.912948
179.567870	7376.110067	25.917965
179.936869	7383.133051	25.922983
180.400166	7382.528987	25.928000
180.573864	7396.950796	25.933018
180.589892	7418.529761	25.938036
180.714843	7415.585145	25.943053
180.977826	7431.408213	25.948071
181.194342	7455.756140	25.953088
181.054135	7463.339755	25.958106
181.037473	7459.808191	25.963124
181.332278	7481.325429	25.968141
181.009015	7487.478426	25.973159
181.586022	7488.593659	25.978176
182.167227	7520.512638	25.983194
182.131952	7531.147975	25.988212
182.559809	7550.595729	25.993229
183.444642	7563.630679	25.998247
183.289795	7555.752665	26.003264
183.280670	7561.215092	26.008282
183.389632	7581.382621	26.013300
183.426624	7585.234007	26.018317
183.778624	7578.791397	26.023335
183.734736	7607.261251	26.028352
184.138888	7596.284811	26.033370
184.017855	7618.353708	26.038388
184.312775	7623.756469	26.043405
184.261977	7645.469644	26.048423
184.368297	7656.402987	26.053440
185.001297	7666.001057	26.058458
185.067451	7668.412742	26.063476
185.328808	7686.391843	26.068493
185.387252	7716.275952	26.073511
185.823365	7701.696650	26.078528
186.035231	7703.913367	26.083546
185.960501	7730.785885	26.088564
186.148176	7717.342308	26.093581
186.564445	7719.594557	26.098599
186.441440	7758.205600	26.103616
186.802668	7747.840197	26.108634
186.684532	7749.087635	26.113652
186.749880	7761.015405	26.118669
186.670720	7786.465651	26.123687
186.597777	7810.630415	26.128704
187.561095	7817.863328	26.133722
186.949370	7853.073592	26.138740
187.406526	7846.652090	26.143757
187.957030	7874.558771	26.148775
187.867006	7884.730073	26.153792
188.885284	7886.215818	26.158810
188.857491	7892.531216	26.163828
189.226613	7902.750311	26.168845
189.624388	7930.803611	26.173863
189.446138	7933.492773	26.178880
189.900894	7916.361660	26.183898
189.942171	7940.200604	26.188916
190.429476	7947.762673	26.193933
190.674612	7951.096985	26.198951
190.505032	7962.499046	26.203968
190.692559	7960.132296	26.208986
190.529112	7969.421118	26.214004
190.688081	7977.945508	26.219021
191.244755	7985.197649	26.224039
191.259791	7993.926968	26.229056
191.399866	8007.475189	26.234074
191.578352	8021.677839	26.239092
191.560670	8047.763361	26.244109
191.906253	8041.818577	26.249127
191.858232	8069.530738	26.254144
192.538817	8075.658283	26.259162
192.666464	8073.106881	26.264180
192.528769	8093.935634	26.269197
192.583195	8122.576039	26.274215
192.670592	8138.900584	26.279232
193.134361	8145.609765	26.284250
193.293856	8164.985275	26.289268
193.431282	8184.462901	26.294285
193.771361	8219.401729	26.299303
193.764493	8232.292386	26.304320
194.375632	8222.431956	26.309338
194.361963	8223.296736	26.314356
194.785555	8247.343112	26.319373
194.878348	8263.788181	26.324391
195.014600	8278.985658	26.329408
195.348179	8285.339163	26.334426
195.333455	8290.353851	26.339444
195.614240	8290.726578	26.344461
195.753069	8325.786315	26.349479
196.012173	8328.545044	26.354496
196.326497	8343.817121	26.359514
196.628122	8376.099065	26.364532
196.636949	8367.123281	26.369549
196.665449	8398.839239	26.374567
197.293121	8402.545973	26.379584
197.532217	8392.238133	26.384602
197.571109	8421.288825	26.389620
197.817759	8419.155601	26.394637
198.040287	8432.994571	26.399655
197.825770	8442.450413	26.404672
198.420356	8459.607446	26.409690
198.601850	8483.940698	26.414708
198.602870	8482.326902	26.419725
199.093851	8507.327330	26.424743
199.227686	8499.075872	26.429760
199.247076	8506.953376	26.434778
199.446616	8518.301149	26.439796
199.417001	8535.030568	26.444813
199.934851	8532.084622	26.449831
199.773650	8550.875648	26.454848
200.002544	8571.982335	26.459866
200.070631	8592.050010	26.464884
200.351700	8591.207448	26.469901
200.642157	8592.569373	26.474919
200.899327	8624.429935	26.479936
201.375929	8618.748396	26.484954
201.324959	8636.091833	26.489972
201.383670	8641.336289	26.494989
201.714438	8659.943771	26.500007
201.813594	8670.264679	26.505024
202.541325	8684.139323	26.510042
202.750601	8704.828065	26.515060
202.664344	8697.157098	26.520077
203.267639	8701.464929	26.525095
203.039461	8714.701284	26.530112
203.376568	8735.672170	26.535130
203.893452	8741.386761	26.540148
203.960961	8734.259802	26.545165
203.807088	8738.592724	26.550183
203.982590	8760.210971	26.555200
204.023192	8767.213229	26.560218
204.385153	8788.014683	26.565236
204.418863	8807.693725	26.570253
204.818766	8820.937444	26.575271
204.665114	8845.830694	26.580288
205.089013	8847.759720	26.585306
205.405467	8878.814733	26.590324
205.330081	8898.216563	26.595341
205.850215	8895.666339	26.600359
205.376008	8923.083390	26.605376
205.971836	8933.297991	26.610394
206.323867	8967.715106	26.615412
206.278594	8969.725606	26.620429
206.606210	8980.043624	26.625447
206.958716	9013.904709	26.630464
207.406995	9028.193645	26.635482
207.712607	9043.140980	26.640500
207.764072	9047.406192	26.645517
208.492529	9060.699003	26.650535
208.598827	9063.075915	26.655552
208.679105	9079.356140	26.660570
209.097390	9083.585168	26.665588
208.939053	9094.835753	26.670605
209.260032	9109.634116	26.675623
209.629818	9099.456234	26.680640
209.678891	9120.105831	26.685658
209.668006	9126.800134	26.690676
210.110621	9126.392397	26.695693
210.658432	9142.865591	26.700711
210.677863	9165.997201	26.705728
210.732731	9160.161470	26.710746
211.485841	9163.400296	26.715764
211.122313	9188.358690	26.720781
211.764821	9182.271483	26.725799
211.673393	9180.672890	26.730816
211.557088	9198.581435	26.735834
211.960494	9212.286449	26.740852
211.998901	9236.816204	26.745869
212.531443	9222.995381	26.750887
212.487272	9251.567485	26.755904
212.506429	9243.050256	26.760922
212.932254	9258.044094	26.765940
212.674325	9278.691852	26.770957
212.936796	9277.345887	26.775975
213.208044	9315.503355	26.780992
213.399414	9316.286272	26.786010
213.675755	9327.106831	26.791028
213.781009	9357.552615	26.796045
214.111863	9359.158400	26.801063
214.311217	9387.246288	26.806080
214.240453	9382.572508	26.811098
214.802102	9399.316991	26.816116
214.649262	9439.079130	26.821133
215.212415	9435.998727	26.826151
215.464558	9460.198151	26.831168
215.460294	9471.375499	26.836186
215.782743	9488.275380	26.841204
215.831672	9517.123216	26.846221
216.347593	9517.657186	26.851239
216.313553	9548.425653	26.856256
216.401763	9557.637593	26.861274
216.617989	9587.286509	26.866292
216.761020	9611.225367	26.871309
217.374850	9607.626169	26.876327
217.526480	9641.349294	26.881344
217.848318	9645.461300	26.886362
218.588126	9658.693670	26.891380
218.524092	9693.272475	26.896397
218.456559	9698.056102	26.901415
218.884287	9712.901980	26.906432
219.317491	9698.715151	26.911450
219.302263	9741.659449	26.916468
219.507362	9770.625294	26.921485
219.732426	9751.794179	26.926503
220.120792	9773.641714	26.931520
220.267494	9779.579317	26.936538
220.440712	9780.758294	26.941556
220.648530	9797.789293	26.946573
220.848731	9827.319220	26.951591
221.180509	9832.493749	26.956608
221.609970	9841.693579	26.961626
221.745239	9859.851946	26.966644
221.707532	9869.694515	26.971661
222.222067	9874.429282	26.976679
222.386322	9883.766687	26.981696
222.421838	9906.620253	26.986714
222.985090	9894.974792	26.991732
222.837499	9928.050891	26.996749
223.211173	9942.178910	27.001767
223.469184	9952.082942	27.006784
223.410528	9963.674480	27.011802
223.862551	9983.366995	27.016820
223.914418	9991.974757	27.021837
224.371680	10000.861325	27.026855
224.478485	10012.536619	27.031872
224.189217	10039.641479	27.036890
225.163811	10041.290630	27.041908
225.162351	10068.481101	27.046925
225.691512	10078.671231	27.051943
225.930453	10082.217327	27.056960
226.177739	10094.498814	27.061978
226.214195	10101.412554	27.066996
226.337504	10113.608205	27.072013
226.691202	10129.936490	27.077031
226.723193	10139.785827	27.082048
227.281994	10158.837874	27.087066
227.571581	10174.671903	27.092084
227.180783	10183.625441	27.097101
227.337474	10182.096025	27.102119
227.728197	10217.469631	27.107136
227.852403	10227.990635	27.112154
227.985645	10232.477380	27.117172
227.925014	10278.805800	27.122189
228.434338	10273.916973	27.127207
228.600453	10303.897666	27.132224
228.865918	10317.517732	27.137242
229.818034	10304.130764	27.142260
229.791225	10323.143498	27.147277
229.737531	10343.646255	27.152295
230.208172	10355.737444	27.157312
230.242703	10357.112668	27.162330
230.364017	10377.601518	27.167348
230.411343	10404.419808	27.172365
230.901036	10419.076520	27.177383
230.963860	10420.499850	27.182400
231.189614	10454.409375	27.187418
231.245243	10462.106997	27.192436
231.275804	10479.230241	27.197453
231.651920	10517.445738	27.202471
232.167991	10534.898420	27.207488
232.597196	10544.849368	27.212506
232.715843	10561.405191	27.217524
232.764976	10597.930968	27.222541
233.253599	10621.399924	27.227559
233.485309	10617.732883	27.232576
233.570471	10640.352445	27.237594
233.889287	10659.780302	27.242612
234.018585	10654.137313	27.247629
234.228021	10687.411212	27.252647
234.504568	10696.858148	27.257664
234.698528	10730.448196	27.262682
235.155807	10729.302296	27.267700
235.237790	10763.761627	27.272717
235.725162	10769.032849	27.277735
236.059125	10782.269415	27.282752
236.126229	10819.649747	27.287770
236.609538	10812.733578	27.292788
236.692351	10824.877388	27.297805
236.608625	10836.157046	27.302823
236.932672	10860.431008	27.307840
237.182883	10886.495052	27.312858
237.624516	10882.581375	27.317876
237.657688	10904.526175	27.322893
237.817410	10935.114857	27.327911
238.155122	10935.657060	27.332928
238.189580	10960.758062	27.337946
238.661853	10987.804087	27.342964
239.167671	10995.297614	27.347981
239.243111	11030.579394	27.352999
239.307987	11027.941793	27.358016
239.659516	11060.044511	27.363034
239.920553	11057.746295	27.368052
240.176009	11070.924391	27.373069
240.733644	11102.662303	27.378087
241.111241	11119.524090	27.383104
240.840846	11128.362159	27.388122
240.896369	11155.053535	27.393140
241.603701	11154.628802	27.398157
241.763299	11170.574313	27.403175
242.170747	11186.726232	27.408192
241.876003	11215.860004	27.413210
242.213153	11239.444699	27.418228
242.501183	11239.651675	27.423245
242.371503	11250.831301	27.428263
242.839727	11278.128196	27.433280
243.356040	11311.381839	27.438298
243.454408	11324.692442	27.443316
243.751372	11343.753726	27.448333
243.991087	11361.805173	27.453351
244.336042	11350.116743	27.458368
244.526445	11381.935578	27.463386
244.621631	11402.619905	27.468404
244.913601	11416.966758	27.473421
245.310020	11422.079139	27.478439
245.713306	11439.124501	27.483456
245.536917	11462.357970	27.488474
245.894494	11471.117681	27.493492
245.974647	11487.457896	27.498509
246.258151	11499.636806	27.503527
247.067958	11518.534794	27.508544
247.112079	11534.903067	27.513562
246.818529	11554.398531	27.518580
246.982219	11562.395501	27.523597
246.989868	11606.580938	27.528615
247.884586	11607.402950	27.533632
247.759202	11652.912627	27.538650
248.160521	11665.928473	27.543668
248.268644	11678.184548	27.548685
248.651201	11702.876294	27.553703
249.502628	11722.553027	27.558720
249.289801	11742.432406	27.563738
249.894617	11747.408842	27.568756
249.840428	11784.609807	27.573773
250.243183	11795.297728	27.578791
250.965597	11795.219465	27.583808
250.994449	11814.778564	27.588826
251.201007	11835.057477	27.593844
251.338655	11855.714892	27.598861
251.844103	11855.692171	27.603879
251.826617	11872.542831	27.608896
251.838402	11899.773620	27.613914
252.396788	11904.107881	27.618932
252.894616	11908.296173	27.623949
252.859354	11949.207864	27.628967
253.001126	11947.503502	27.633984
252.895728	11959.377560	27.639002
253.294148	11982.230070	27.644020
253.687355	12009.791118	27.649037
253.749245	12017.907543	27.654055
253.956508	12046.697558	27.659072
254.203076	12082.311027	27.664090
254.825355	12088.140983	27.669108
255.456906	12104.498650	27.674125
255.434216	12139.766003	27.679143
256.144844	12150.718402	27.684160
256.107509	12137.966845	27.689178
256.235443	12163.935012	27.694196
256.482625	12189.689728	27.699213
256.594581	12204.762629	27.704231
257.057605	12229.471041	27.709248
257.557801	12225.623781	27.714266
257.818686	12235.246741	27.719284
257.965136	12237.790018	27.724301
258.108252	12257.511966	27.729319
258.392592	12278.030675	27.734336
258.996246	12305.401484	27.739354
259.274260	12303.754928	27.744372
259.063791	12327.702701	27.749389
259.468338	12332.200358	27.754407
259.531747	12329.881047	27.759424
259.598505	12359.507033	27.764442
259.630846	12391.176740	27.769460
260.079662	12396.417065	27.774477
260.228080	12421.191932	27.779495
260.809389	12440.144523	27.784512
260.904056	12444.239649	27.789530
260.963567	12471.125565	27.794548
261.523387	12502.854082	27.799565
261.658229	12522.351629	27.804583
261.876061	12523.176818	27.809600
262.380846	12527.079737	27.814618
262.508764	12544.144990	27.819636
263.038560	12570.790301	27.824653
263.186110	12598.481182	27.829671
263.169327	12601.979500	27.834688
263.444777	12602.792023	27.839706
263.392128	12638.293879	27.844724
264.055725	12649.230759	27.849741
264.074873	12682.221980	27.854759
264.477076	12693.161112	27.859776
264.630481	12727.941380	27.864794
264.805812	12742.583634	27.869812
265.449868	12750.902821	27.874829
264.932997	12782.554535	27.879847
265.398389	12801.317152	27.884864
265.914264	12826.729923	27.889882
266.294780	12863.036740	27.894900
266.600380	12866.206121	27.899917
267.206909	12881.768314	27.904935
267.413316	12907.734961	27.909952
267.750779	12921.034173	27.914970
268.046585	12933.301953	27.919988
268.224262	12963.384985	27.925005
268.342827	12968.139628	27.930023
268.570009	12992.152372	27.935040
268.680075	13026.539452	27.940058
268.878097	13024.042602	27.945076
269.307044	13034.372513	27.950093
269.049814	13068.354770	27.955111
269.786492	13117.641587	27.960128
269.887584	13132.913320	27.965146
270.051020	13160.961000	27.970164
270.831975	13182.422977	27.975181
271.120709	13199.192922	27.980199
271.316152	13243.214755	27.985216
271.542527	13236.062694	27.990234
271.635157	13267.030883	27.995252
272.254355	13293.267139	28.000269
272.230805	13316.593057	28.005287
272.947787	13316.432976	28.010304
272.851377	13338.926418	28.015322
273.100147	13370.453575	28.020340
273.657856	13399.382708	28.025357
273.541951	13414.391974	28.030375
273.917894	13429.888016	28.035392
274.286114	13461.715474	28.040410
273.995154	13477.055459	28.045428
274.656317	13490.630188	28.050445
274.681847	13543.956052	28.055463
275.288259	13554.636714	28.060480
275.673802	13588.147526	28.065498
275.449450	13622.249207	28.070516
276.207514	13628.008453	28.075533
276.302610	13669.607307	28.080551
276.928688	13680.340741	28.085568
277.408460	13689.817325	28.090586
277.875470	13722.621657	28.095604
277.899553	13716.224470	28.100621
277.907567	13752.365574	28.105639
278.455291	13762.618030	28.110656
278.688843	13766.947385	28.115674
278.817214	13788.773253	28.120692
279.706688	13825.410984	28.125709
279.107960	13844.895821	28.130727
279.467799	13858.800332	28.135744
279.774628	13889.189135	28.140762
279.965706	13900.745408	28.145780
280.260322	13909.585403	28.150797
280.160360	13945.433577	28.155815
280.557197	13955.468427	28.160832
280.781574	13992.534715	28.165850
280.891490	14013.758863	28.170868
281.501884	14048.443630	28.175885
281.501534	14075.076603	28.180903
281.639832	14094.791356	28.185920
282.355949	14132.870274	28.190938
282.256109	14138.529572	28.195956
283.170944	14150.336743	28.200973
283.562836	14202.665119	28.205991
283.573635	14227.088900	28.211008
284.315154	14214.245626	28.216026
284.486766	14247.323584	28.221044
284.838922	14244.799507	28.226061
285.226760	14264.017852	28.231079
285.468716	14282.759236	28.236096
286.178294	14307.471079	28.241114
285.731031	14331.389248	28.246132
286.110852	14352.384886	28.251149
286.337898	14361.162233	28.256167
286.551207	14393.626937	28.261184
286.992342	14418.597604	28.266202
286.757476	14420.410837	28.271220
287.534501	14446.355019	28.276237
287.530212	14493.480466	28.281255
287.948671	14517.065211	28.286272
288.040301	14529.297032	28.291290
287.969884	14561.069915	28.296308
288.482912	14589.312865	28.301325
289.041665	14617.540432	28.306343
289.680406	14635.337389	28.311360
290.459757	14644.532617	28.316378
290.487918	14661.324286	28.321396
290.588172	14684.909847	28.326413
290.940969	14710.639327	28.331431
291.048055	14720.522402	28.336448
291.557253	14749.475367	28.341466
291.551669	14775.423314	28.346484
291.646633	14795.533724	28.351501
292.112812	14811.307708	28.356519
292.263042	14836.738364	28.361536
292.755791	14863.648871	28.366554
293.005914	14896.526088	28.371572
293.625614	14916.702807	28.376589
293.643893	14927.721075	28.381607
293.631799	14964.329128	28.386624
294.257619	14984.493890	28.391642
294.280151	15008.377983	28.396660
294.779106	15035.629702	28.401677
294.978031	15070.275912	28.406695
295.274011	15081.240525	28.411712
295.410208	15096.338126	28.416730
295.449720	15139.663642	28.421748
296.236919	15178.027959	28.426765
296.578985	15196.415058	28.431783
296.570178	15226.128911	28.436800
296.794552	15240.414708	28.441818
297.570485	15262.501169	28.446836
297.745403	15273.835749	28.451853
298.138676	15319.501721	28.456871
298.487576	15359.620301	28.461888
298.859582	15346.537780	28.466906
299.199359	15370.477150	28.471924
299.201393	15400.044552	28.476941
299.541618	15402.238785	28.481959
299.520465	15440.923224	28.486976
300.269261	15459.616902	28.491994
300.309920	15492.748976	28.497012
300.471009	15511.952686	28.502029
300.754103	15525.538806	28.507047
300.840750	15561.772595	28.512064
301.028575	15566.324307	28.517082
301.190005	15621.724149	28.522100
301.804648	15633.170709	28.527117
302.269242	15669.107490	28.532135
302.252810	15696.489592	28.537152
303.051291	15715.257303	28.542170
303.329972	15759.797781	28.547188
303.947099	15766.056219	28.552205
303.968488	15791.517535	28.557223
304.187562	15812.732306	28.562240
304.834065	15825.721260	28.567258
304.686892	15865.250141	28.572276
305.285061	15880.929295	28.577293
305.283712	15913.229213	28.582311
305.472724	15929.080020	28.587328
306.239470	15963.394786	28.592346
306.040023	15992.583664	28.597364
306.735421	16014.180167	28.602381
306.830659	16042.828767	28.607399
306.987517	16088.245988	28.612416
307.490535	16108.446622	28.617434
307.693826	16129.320863	28.622452
308.127022	16157.950076	28.627469
308.318837	16195.895109	28.632487
308.687382	16224.002457	28.637504
309.116233	16258.102609	28.642522
309.374753	16291.067934	28.647540
309.614388	16300.614885	28.652557
310.049417	16338.445999	28.657575
310.340624	16365.304040	28.662592
310.603011	16386.827591	28.667610
310.945180	16420.269476	28.672628
311.374387	16432.290939	28.677645
311.728961	16470.884228	28.682663
311.690377	16494.318843	28.687680
312.505076	16522.423914	28.692698
312.877413	16545.280104	28.697716
313.255905	16567.270107	28.702733
313.638410	16584.619843	28.707751
313.775012	16622.111655	28.712768
314.247429	16632.523371	28.717786
314.342998	16668.819607	28.722804
314.492357	16687.782366	28.727821
315.057194	16702.941447	28.732839
314.942060	16744.194427	28.737856
315.703725	16757.226566	28.742874
315.741162	16795.409679	28.747892
316.318678	16826.481060	28.752909
316.440787	16856.885448	28.757927
316.727112	16875.196976	28.762944
317.354472	16913.435773	28.767962
317.633656	16928.681657	28.772980
318.204176	16941.791228	28.777997
318.317529	16955.137090	28.783015
318.551161	16977.310754	28.788032
318.682048	17020.437049	28.793050
319.210264	17036.034316	28.798068
319.214627	17085.222516	28.803085
320.059473	17095.643921	28.808103
320.071670	17113.009693	28.813120
320.694421	17122.496983	28.818138
320.882822	17144.887956	28.823156
320.826439	17159.373118	28.828173
321.520074	17200.818292	28.833191
321.427086	17217.610544	28.838208
322.157308	17229.165221	28.843226
322.333664	17250.335334	28.848244
322.594729	17264.473426	28.853261
322.643608	17301.765373	28.858279
322.863189	17323.688087	28.863296
323.341366	17367.712997	28.868314
323.415640	17388.874937	28.873332
323.799852	17406.228417	28.878349
324.247126	17437.539972	28.883367
324.449941	17482.475931	28.888384
324.783155	17505.428187	28.893402
324.959820	17540.341792	28.898420
325.209122	17577.736795	28.903437
325.548556	17587.917348	28.908455
325.677080	17639.104051	28.913472
326.280183	17661.152982	28.918490
326.774057	17678.539068	28.923508
326.459738	17730.730674	28.928525
327.026374	17786.009439	28.933543
327.489340	17813.672076	28.938560
327.734784	17836.965545	28.943578
328.115655	17879.830572	28.948596
328.557007	17902.733998	28.953613
329.322468	17952.254545	28.958631
329.332178	17970.677618	28.963648
329.848480	18014.117962	28.968666
329.877555	18060.187474	28.973684
330.258362	18079.212900	28.978701
331.002759	18108.142436	28.983719
331.139055	18145.486476	28.988736
331.325263	18161.640949	28.993754
331.970268	18192.550892	28.998772
332.143408	18241.758802	29.003789
332.760389	18255.110782	29.008807
332.732974	18304.560061	29.013824
333.246020	18327.728058	29.018842
333.721667	18338.600561	29.023860
334.005282	18380.222057	29.028877
334.690361	18412.210174	29.033895
334.833655	18432.252454	29.038912
335.006345	18468.416989	29.043930
335.279458	18503.925099	29.048948
335.752788	18526.617637	29.053965
336.041328	18550.406212	29.058983
336.268301	18575.686578	29.064000
336.942177	18620.513150	29.069018
336.907384	18636.922110	29.074036
337.356808	18669.662084	29.079053
337.803483	18690.765752	29.084071
338.010914	18728.416171	29.089088
338.590440	18750.820373	29.094106
339.170134	18756.369002	29.099124
339.411618	18796.706050	29.104141
339.843442	18810.944936	29.109159
339.896769	18842.625303	29.114176
340.569253	18869.788557	29.119194
341.076590	18887.596118	29.124212
341.054411	18903.410615	29.129229
341.177468	18927.463502	29.134247
341.397375	18967.133076	29.139264
341.540039	18992.768468	29.144282
342.049870	19045.595685	29.149300
342.292446	19065.447374	29.154317
342.627003	19109.891576	29.159335
342.807872	19139.585914	29.164352
343.272375	19145.194688	29.169370
343.969529	19178.425929	29.174388
344.150382	19217.565069	29.179405
344.368551	19247.742067	29.184423
344.670967	19279.267056	29.189440
345.081776	19285.934511	29.194458
345.382529	19321.419323	29.199476
345.301294	19356.466078	29.204493
345.782703	19382.610401	29.209511
345.649806	19446.280790	29.214528
346.126134	19458.572537	29.219546
346.689383	19509.354337	29.224564
346.654526	19543.897310	29.229581
347.203435	19579.530829	29.234599
347.536159	19617.988530	29.239616
348.052450	19679.897502	29.244634
348.650485	19705.764564	29.249652
348.428574	19741.935603	29.254669
349.346675	19782.730733	29.259687
349.799182	19818.997015	29.264704
350.140439	19864.810343	29.269722
350.437757	19877.415706	29.274740
350.991273	19911.994651	29.279757
351.360130	19948.404291	29.284775
351.844220	19981.212073	29.289792
352.209901	20001.840576	29.294810
352.671826	20032.949730	29.299828
352.964360	20071.490786	29.304845
353.456201	20086.015627	29.309863
353.937666	20121.371417	29.314880
353.877569	20155.360246	29.319898
354.204740	20182.934227	29.324916
354.329120	20230.385921	29.329933
354.779040	20256.063935	29.334951
355.072172	20279.335636	29.339968
355.321412	20333.348115	29.344986
355.892644	20367.775335	29.350004
355.843536	20407.784423	29.355021
356.443774	20438.340266	29.360039
356.661038	20488.275836	29.365056
356.966553	20517.219057	29.370074
357.544506	20564.462784	29.375092
357.653617	20596.255513	29.380109
358.207614	20625.994913	29.385127
358.627218	20666.809946	29.390144
358.634157	20717.217599	29.395162
359.201380	20743.367236	29.400180
359.831004	20777.637482	29.405197
360.020681	20816.690662	29.410215
360.419072	20880.233061	29.415232
361.121488	20912.313013	29.420250
361.441995	20930.049603	29.425268
361.720586	20969.305992	29.430285
361.869300	21005.762202	29.435303
362.671607	21042.815161	29.440320
362.909170	21081.169016	29.445338
363.749081	21110.272479	29.450356
363.956853	21132.933649	29.455373
364.325019	21162.454063	29.460391
364.496905	21184.083960	29.465408
364.639009	21206.451833	29.470426
365.323388	21256.627821	29.475444
365.299275	21297.084192	29.480461
366.075888	21303.956872	29.485479
366.398934	21350.273874	29.490496
366.831421	21376.553963	29.495514
367.120948	21389.833319	29.500532
367.325423	21443.044938	29.505549
367.594457	21472.527103	29.510567
368.029613	21497.001931	29.515584
368.150079	21529.805058	29.520602
368.685704	21555.661672	29.525620
368.704431	21591.885254	29.530637
369.123590	21611.702939	29.535655
369.549893	21666.842871	29.540672
370.036912	21693.700891	29.545690
370.927896	21712.379798	29.550708
371.279510	21752.474100	29.555725
371.378962	21771.294871	29.560743
372.118520	21808.646819	29.565760
372.145371	21839.427656	29.570778
372.463942	21857.737811	29.575796
372.914999	21896.143400	29.580813
373.259998	21944.351763	29.585831
373.624834	21950.048904	29.590848
373.824020	21984.622911	29.595866
374.464239	22020.172489	29.600884
374.535216	22050.044678	29.605901
374.890204	22087.435558	29.610919
375.102946	22131.810225	29.615936
375.662494	22184.208831	29.620954
376.033084	22210.897737	29.625972
376.335343	22259.522382	29.630989
376.733518	22282.423241	29.636007
377.070589	22319.182267	29.641024
377.416158	22372.769240	29.646042
377.888513	22383.399020	29.651060
377.697656	22440.648786	29.656077
378.666931	22465.801411	29.661095
378.921703	22511.973683	29.666112
379.201289	22567.336312	29.671130
380.073285	22589.473525	29.676148
380.303537	22644.056290	29.681165
380.429990	22655.988853	29.686183
381.097498	22689.834262	29.691200
381.719681	22737.269178	29.696218
382.180497	22748.952655	29.701236
382.565988	22798.758562	29.706253
383.045850	22854.405941	29.711271
383.408762	22872.314166	29.716288
383.801769	22900.356311	29.721306
384.248524	22937.986180	29.726324
384.652693	22957.264024	29.731341
384.896434	22995.093098	29.736359
385.391691	23012.894476	29.741376
385.473218	23039.884709	29.746394
385.984311	23088.469376	29.751412
386.068732	23116.983809	29.756429
386.267479	23168.376173	29.761447
386.776720	23188.790988	29.766464
387.051461	23238.102526	29.771482
387.477066	23282.241690	29.776500
387.921483	23304.904548	29.781517
388.120981	23352.928158	29.786535
388.435917	23397.234107	29.791552
388.910433	23447.916440	29.796570
389.301090	23499.501992	29.801588
389.831030	23529.769250	29.806605
390.102381	23566.980168	29.811623
390.158649	23608.452064	29.816640
390.759017	23651.306754	29.821658
390.977552	23685.981974	29.826676
391.556065	23738.798535	29.831693
392.037831	23783.461065	29.836711
392.336152	23828.680619	29.841728
392.602907	23869.828283	29.846746
393.212485	23879.099345	29.851764
393.899931	23909.807957	29.856781
394.339646	23950.003323	29.861799
394.571148	24000.653363	29.866816
394.955986	24028.659324	29.871834
395.338399	24072.158108	29.876852
395.447221	24111.301697	29.881869
395.886055	24133.356421	29.886887
396.539504	24174.390494	29.891904
396.758346	24240.073858	29.896922
396.735092	24261.982773	29.901940
397.047282	24306.803992	29.906957
397.385117	24365.472395	29.911975
398.048015	24391.242988	29.916992
398.405712	24443.775011	29.922010
398.995062	24494.908228	29.927028
399.436240	24539.297233	29.932045
399.596862	24596.581399	29.937063
400.041405	24636.194215	29.942080
400.557718	24673.750251	29.947098
400.770868	24726.507276	29.952116
401.444117	24769.515172	29.957133
401.741751	24808.458896	29.962151
402.616036	24869.317242	29.967168
402.657978	24901.203330	29.972186
403.161038	24943.039875	29.977204
403.775470	24989.257280	29.982221
404.008183	25026.436801	29.987239
404.669358	25068.753679	29.992256
404.573666	25111.457436	29.997274
405.196483	25162.546146	30.002292
405.812904	25202.248576	30.007309
405.588770	25236.891307	30.012327
406.331257	25285.702670	30.017344
406.830241	25334.532323	30.022362
407.453017	25376.594566	30.027380
407.818763	25421.118182	30.032397
408.357147	25459.929024	30.037415
408.688914	25519.685691	30.042432
409.019559	25552.715800	30.047450
409.134714	25583.238171	30.052468
409.806075	25637.466036	30.057485
410.183956	25680.542385	30.062503
410.465420	25721.014086	30.067520
410.770682	25773.342868	30.072538
411.456908	25827.258247	30.077556
412.142256	25868.934511	30.082573
412.444533	25907.742806	30.087591
413.022630	25941.508601	30.092608
413.302982	25987.027027	30.097626
413.907433	26025.109205	30.102644
414.429282	26073.672296	30.107661
415.021138	26103.531839	30.112679
415.631656	26133.071402	30.117696
415.656791	26168.866960	30.122714
416.080067	26206.274613	30.127732
416.605934	26238.538984	30.132749
417.122458	26260.045934	30.137767
417.273777	26311.971316	30.142784
417.347802	26359.622074	30.147802
418.139155	26392.298599	30.152820
418.519767	26422.643012	30.157837
418.607842	26475.520743	30.162855
418.900892	26515.073089	30.167872
419.296766	26558.394684	30.172890
419.782062	26603.750020	30.177908
420.580229	26644.968016	30.182925
421.107485	26662.053620	30.187943
422.136077	26670.725588	30.192960
422.186805	26730.679584	30.197978
422.535898	26743.308367	30.202996
422.927896	26776.543602	30.208013
423.081566	26821.722493	30.213031
423.717433	26837.180289	30.218048
423.919447	26881.786812	30.223066
423.932801	26921.381573	30.228084
424.792607	26962.997006	30.233101
424.753654	26992.397769	30.238119
425.354424	27044.590177	30.243136
425.351143	27092.457598	30.248154
425.453015	27128.272453	30.253172
426.044866	27172.417943	30.258189
426.253278	27231.936061	30.263207
426.872799	27280.164754	30.268224
426.968264	27350.286565	30.273242
427.430929	27391.634329	30.278260
427.986329	27440.706711	30.283277
428.314468	27501.555887	30.288295
429.077675	27543.097226	30.293312
429.172898	27608.157982	30.298330
429.951033	27658.395869	30.303348
430.556894	27700.190671	30.308365
431.108502	27758.698258	30.313383
431.477516	27809.221799	30.318400
431.986610	27843.018529	30.323418
432.630496	27902.605817	30.328436
433.273536	27931.371958	30.333453
433.273016	28008.284081	30.338471
434.076564	28037.938568	30.343488
434.206389	28075.816705	30.348506
434.755666	28125.257934	30.353524
435.413563	28168.426776	30.358541
435.975093	28218.478146	30.363559
436.841898	28243.041265	30.368576
437.188411	28290.617688	30.373594
437.710524	28334.749308	30.378612
437.926611	28349.598105	30.383629
438.226011	28419.520272	30.388647
438.784594	28449.452499	30.393664
438.999186	28480.466704	30.398682
439.324063	28527.605774	30.403700
440.256295	28572.073990	30.408717
440.483679	28610.864519	30.413735
440.865545	28653.771069	30.418752
441.245364	28698.021753	30.423770
441.985094	28729.703514	30.428788
442.251845	28759.331218	30.433805
442.066959	28820.859651	30.438823
442.668902	28849.173604	30.443840
443.354147	28898.241323	30.448858
443.585118	28963.234314	30.453876
443.766884	29016.678472	30.458893
443.870393	29063.612698	30.463911
445.061711	29106.150092	30.468928
445.409154	29163.049655	30.473946
445.922654	29204.935925	30.478964
446.109572	29233.486246	30.483981
446.720544	29308.208706	30.488999
446.990917	29344.662748	30.494016
447.818815	29400.628908	30.499034
448.158444	29441.900992	30.504052
448.558895	29491.982673	30.509069
449.164060	29540.532365	30.514087
449.292265	29588.236754	30.519104
449.977299	29634.953451	30.524122
450.175875	29671.726017	30.529140
450.903038	29723.949848	30.534157
450.900089	29774.196770	30.539175
451.786529	29824.088730	30.544192
452.517126	29858.978954	30.549210
452.290990	29885.863658	30.554228
452.882682	29931.366353	30.559245
453.384656	29963.755244	30.564263
453.521335	30018.594741	30.569280
454.071308	30071.880396	30.574298
454.333745	30134.276477	30.579316
454.775070	30156.480529	30.584333
455.126289	30220.155585	30.589351
455.384530	30284.918759	30.594368
456.064670	30328.707619	30.599386
456.289944	30407.798119	30.604404
457.311357	30454.688590	30.609421
457.334076	30498.797830	30.614439
457.685055	30551.023207	30.619456
458.211918	30624.967146	30.624474
458.743882	30684.636160	30.629492
459.208779	30732.332242	30.634509
459.576428	30805.798520	30.639527
460.051052	30868.477646	30.644544
460.879115	30928.455056	30.649562
461.113078	30972.984867	30.654580
461.806786	31034.117341	30.659597
462.182375	31096.681155	30.664615
463.188333	31135.414978	30.669632
463.701974	31178.457444	30.674650
464.386215	31226.951479	30.679668
465.022836	31275.226379	30.684685
465.577978	31321.700933	30.689703
466.211753	31352.887642	30.694720
466.395861	31392.123740	30.699738
466.451109	31451.337834	30.704756
466.990794	31499.670380	30.709773
467.555040	31540.670596	30.714791
467.985390	31585.311494	30.719808
468.520553	31633.474803	30.724826
468.705685	31693.053140	30.729844
469.215973	31734.971292	30.734861
469.503612	31791.021792	30.739879
470.013011	31837.647242	30.744896
470.877293	31889.482677	30.749914
470.900726	31962.073719	30.754932
471.090426	32017.292483	30.759949
471.781349	32056.190816	30.764967
472.249361	32104.820811	30.769984
472.754886	32180.976941	30.775002
473.353576	32230.535305	30.780020
473.867759	32291.181294	30.785037
474.441136	32338.996358	30.790055
474.828474	32392.754509	30.795072
475.327085	32448.403148	30.800090
475.595199	32488.997049	30.805108
476.481177	32526.860956	30.810125
476.872997	32602.277373	30.815143
477.134680	32639.039472	30.820160
477.874205	32704.202211	30.825178
478.414716	32768.442121	30.830196
478.873523	32814.911323	30.835213
479.139239	32844.609264	30.840231
479.334547	32907.486977	30.845248
479.864362	32978.673497	30.850266
480.401703	33037.500979	30.855284
481.118260	33079.486086	30.860301
481.382267	33136.226273	30.865319
481.759824	33190.291365	30.870336
482.529004	33232.447982	30.875354
482.596488	33283.680891	30.880372
482.876894	33324.527098	30.885389
483.448058	33390.764515	30.890407
483.893206	33442.134270	30.895424
484.474556	33496.460061	30.900442
484.479730	33552.944616	30.905460
485.035854	33627.600005	30.910477
485.535635	33682.006100	30.915495
485.980180	33741.649507	30.920512
486.951392	33800.341616	30.925530
487.093451	33875.047520	30.930548
487.552618	33919.733776	30.935565
487.893148	33994.132903	30.940583
488.592579	34053.012730	30.945600
489.506704	34111.778411	30.950618
489.569187	34193.446511	30.955636
490.115900	34255.863972	30.960653
490.879280	34296.484358	30.965671
491.052526	34356.221986	30.970688
491.777201	34427.688234	30.975706
492.339079	34498.140430	30.980724
493.105571	34535.501484	30.985741
493.772583	34600.389787	30.990759
493.935193	34647.805694	30.995776
494.506862	34716.218836	31.000794
494.582303	34792.321636	31.005812
495.302724	34838.459520	31.010829
495.733302	34898.856952	31.015847
496.216893	34973.372247	31.020864
497.020118	35024.936734	31.025882
497.610426	35099.324494	31.030900
498.064591	35144.607882	31.035917
498.487491	35216.490032	31.040935
499.051008	35259.568976	31.045952
499.674733	35327.281696	31.050970
499.913234	35382.130608	31.055988
500.351892	35445.646108	31.061005
500.785570	35510.156616	31.066023
501.442996	35585.147481	31.071040
502.307839	35632.563621	31.076058
502.089907	35708.444284	31.081076
502.861251	35743.478357	31.086093
503.606809	35813.274348	31.091111
503.886539	35898.991299	31.096128
504.704206	35940.401680	31.101146
504.993832	36023.911900	31.106164
505.422106	36084.007658	31.111181
506.071880	36130.990481	31.116199
506.243245	36204.795720	31.121216
507.242079	36256.669121	31.126234
507.418353	36317.605650	31.131252
507.916495	36400.177542	31.136269
508.159301	36460.510318	31.141287
508.439731	36526.643400	31.146304
509.376178	36608.979769	31.151322
509.929718	36663.720635	31.156340
510.386744	36736.048229	31.161357
511.276244	36795.723081	31.166375
511.265184	36856.357891	31.171392
511.941769	36914.856535	31.176410
512.450158	37001.263661	31.181428
512.695895	37070.273008	31.186445
513.423873	37116.917319	31.191463
513.609938	37206.660617	31.196480
514.623777	37262.400234	31.201498
515.194870	37303.999679	31.206516
515.484198	37382.243050	31.211533
516.147988	37444.813314	31.216551
516.483076	37507.586413	31.221568
517.271707	37555.692444	31.226586
517.848893	37637.458579	31.231604
518.116896	37674.984316	31.236621
518.773633	37734.833295	31.241639
518.916643	37810.073114	31.246656
519.617934	37866.989718	31.251674
519.857129	37922.436461	31.256692
520.393613	38002.598342	31.261709
521.057234	38074.247107	31.266727
521.512436	38144.917542	31.271744
521.867599	38196.151795	31.276762
522.509966	38271.244788	31.281780
522.989586	38341.684738	31.286797
523.722732	38417.331413	31.291815
524.082834	38478.191272	31.296832
524.557860	38542.333490	31.301850
525.071344	38628.760233	31.306868
525.544966	38686.723796	31.311885
526.019695	38761.392062	31.316903
526.883310	38830.697457	31.321920
527.271519	38892.456692	31.326938
527.670055	38974.053271	31.331956
528.507644	39064.585071	31.336973
529.249771	39116.755338	31.341991
529.474819	39169.847524	31.347008
530.384499	39247.863986	31.352026
530.787115	39311.143507	31.357044
531.285243	39382.512357	31.362061
532.071542	39468.471986	31.367079
532.346979	39528.497218	31.372096
533.089934	39593.346920	31.377114
533.565897	39670.019735	31.382132
533.659841	39726.603828	31.387149
534.713959	39789.925752	31.392167
534.989831	39871.357271	31.397184
535.937692	39932.333256	31.402202
536.535753	40014.709561	31.407220
536.999996	40083.741704	31.412237
537.626974	40118.315812	31.417255
537.919747	40182.301424	31.422272
538.550555	40265.102708	31.427290
539.139711	40340.528720	31.432308
539.731686	40396.502387	31.437325
540.238921	40457.953769	31.442343
540.297686	40536.359368	31.447360
541.106804	40578.065936	31.452378
541.750375	40667.605683	31.457396
542.410280	40745.508881	31.462413
542.463211	40800.307132	31.467431
542.799618	40883.873199	31.472448
543.229200	40959.416514	31.477466
543.904768	41030.541593	31.482484
544.380909	41107.798068	31.487501
545.411515	41176.642964	31.492519
546.021655	41254.364017	31.497536
546.470064	41338.481826	31.502554
547.306050	41396.754038	31.507572
547.527731	41483.444599	31.512589
548.048709	41549.531099	31.517607
548.646389	41627.445188	31.522624
549.308182	41674.399453	31.527642
549.981173	41759.381710	31.532660
550.318677	41847.386919	31.537677
551.009506	41897.515593	31.542695
551.500606	41972.762540	31.547712
552.012517	42042.217209	31.552730
552.594370	42094.100536	31.557748
553.020783	42175.290211	31.562765
553.665033	42231.109361	31.567783
553.938888	42294.556260	31.572800
554.339473	42380.195619	31.577818
554.890601	42447.473588	31.582836
555.261433	42512.496169	31.587853
556.406377	42575.105696	31.592871
556.558861	42672.508085	31.597888
557.088536	42730.740444	31.602906
557.490112	42792.510707	31.607924
558.083365	42882.786189	31.612941
558.414692	42941.654910	31.617959
559.146857	43017.611313	31.622976
559.857007	43113.342402	31.627994
560.788206	43190.684028	31.633012
561.333890	43272.802729	31.638029
562.051343	43340.697324	31.643047
562.469511	43403.088785	31.648064
563.203712	43471.195759	31.653082
563.949758	43525.357331	31.658100
564.561250	43603.542705	31.663117
564.919501	43687.825079	31.668135
565.557877	43766.849585	31.673152
566.017738	43814.205722	31.678170
566.510900	43884.327081	31.683188
566.923515	43976.093082	31.688205
567.666345	44024.763646	31.693223
568.113063	44127.053059	31.698240
568.399496	44193.386698	31.703258
569.168244	44277.458741	31.708276
569.497510	44373.382402	31.713293
570.417720	44429.734055	31.718311
570.406616	44529.301069	31.723328
570.961164	44616.428119	31.728346
571.913284	44675.603932	31.733364
572.074474	44781.909340	31.738381
572.965546	44849.499830	31.743399
573.429045	44949.732618	31.748416
573.895604	45051.884947	31.753434
574.664763	45122.107476	31.758452
575.167011	45202.009852	31.763469
575.714356	45302.476949	31.768487
576.352057	45397.464649	31.773504
577.161744	45468.812052	31.778522
577.842712	45539.663214	31.783540
578.265105	45633.772104	31.788557
578.717857	45723.775255	31.793575
579.586181	45796.471826	31.798592
580.025305	45898.336557	31.803610
580.717651	45989.539051	31.808628
581.294743	46051.682701	31.813645
581.792227	46136.758299	31.818663
582.365676	46217.698329	31.823680
582.782705	46309.244644	31.828698
583.927162	46385.692976	31.833716
584.358508	46465.306220	31.838733
584.816001	46546.077386	31.843751
585.457879	46629.840030	31.848768
585.868565	46704.469091	31.853786
586.923093	46793.774950	31.858804
587.031891	46884.999263	31.863821
587.774933	46944.690438	31.868839
588.178235	47028.118538	31.873856
588.985604	47108.032356	31.878874
589.605430	47196.455232	31.883892
589.964599	47280.564280	31.888909
590.568460	47376.233856	31.893927
591.247437	47442.997319	31.898944
591.912365	47498.914177	31.903962
592.643417	47576.967044	31.908980
592.978851	47655.477111	31.913997
593.432918	47723.892215	31.919015
593.935237	47823.451978	31.924032
594.472160	47901.124615	31.929050
595.087181	47988.866823	31.934068
595.590117	48085.582891	31.939085
596.021368	48158.038748	31.944103
596.878070	48246.256928	31.949120
597.486936	48331.349344	31.954138
598.344546	48423.960479	31.959156
598.714010	48491.707134	31.964173
599.128135	48602.757374	31.969191
599.858857	48667.773595	31.974208
600.232458	48741.409561	31.979226
600.974450	48837.966851	31.984244
601.554284	48935.252435	31.989261
601.986810	49013.158461	31.994279
603.057986	49126.342100	31.999296
603.184840	49216.141086	32.004314
603.981825	49289.683996	32.009332
604.716168	49385.547470	32.014349
605.314982	49478.563347	32.019367
606.345984	49552.709667	32.024384
606.821329	49647.155161	32.029402
607.739159	49735.278615	32.034420
608.446510	49817.377261	32.039437
608.838191	49882.043126	32.044455
610.043023	49987.245621	32.049472
609.870374	50066.462248	32.054490
610.747008	50139.313186	32.059508
611.339615	50246.888792	32.064525
611.787682	50312.007867	32.069543
612.473223	50403.993928	32.074560
613.050205	50496.715228	32.079578
613.873505	50577.162161	32.084596
614.242848	50665.620525	32.089613
614.725591	50753.855297	32.094631
616.063558	50832.519280	32.099648
616.303195	50930.727099	32.104666
617.017174	51011.481304	32.109684
617.583608	51074.154867	32.114701
617.965003	51167.237012	32.119719
618.911121	51247.944402	32.124736
619.282432	51358.231435	32.129754
619.904848	51431.410371	32.134772
620.491449	51523.673977	32.139789
621.058960	51626.795854	32.144807
621.719899	51685.757580	32.149824
622.391414	51770.599231	32.154842
622.965907	51881.064155	32.159860
623.521047	51958.965133	32.164877
623.842636	52055.848198	32.169895
624.623491	52161.192704	32.174912
624.647209	52252.646357	32.179930
625.802535	52338.692877	32.184948
626.286568	52439.745270	32.189965
626.943013	52553.529390	32.194983
627.634430	52628.084845	32.200000
628.265378	52743.725092	32.205018
628.858690	52837.228818	32.210036
629.418559	52927.510640	32.215053
629.969741	53017.683775	32.220071
631.410067	53102.833871	32.225088
631.879479	53195.361735	32.230106
632.500299	53277.596898	32.235124
633.334088	53348.549939	32.240141
633.884854	53441.454036	32.245159
634.871951	53513.323589	32.250176
635.725357	53584.962810	32.255194
635.959043	53668.732281	32.260212
636.694823	53746.986515	32.265229
636.737581	53824.635376	32.270247
637.883054	53876.006454	32.275264
638.037919	53981.325312	32.280282
638.965192	54056.548531	32.285300
639.606326	54142.596423	32.290317
640.279903	54230.035445	32.295335
641.094308	54312.669446	32.300352
641.494554	54388.644306	32.305370
642.261678	54470.471861	32.310388
642.727877	54570.480186	32.315405
643.092709	54645.899658	32.320423
643.990671	54721.275595	32.325440
644.690223	54821.050830	32.330458
645.174378	54906.022482	32.335476
645.882582	54989.978296	32.340493
646.056761	55085.242538	32.345511
647.120076	55177.226906	32.350528
647.196079	55288.327445	32.355546
647.776730	55406.250404	32.360564
648.501923	55496.794851	32.365581
649.218844	55575.887173	32.370599
649.743807	55681.425756	32.375616
650.427963	55790.495496	32.380634
650.584121	55900.120559	32.385652
651.566568	56002.072642	32.390669
652.176597	56119.818153	32.395687
653.008439	56208.282350	32.400704
653.666867	56315.729256	32.405722
654.696938	56416.576318	32.410740
654.976871	56507.426422	32.415757
655.229891	56639.695818	32.420775
656.442174	56752.247036	32.425792
656.681674	56847.578557	32.430810
657.443174	56951.164215	32.435828
658.319198	57066.628548	32.440845
658.799495	57187.908451	32.445863
659.752945	57276.932331	32.450880
660.589882	57396.612976	32.455898
661.216466	57499.573023	32.460916
661.661375	57604.421192	32.465933
662.495021	57710.709482	32.470951
662.984379	57794.928270	32.475968
663.814289	57908.168444	32.480986
664.821991	58019.339049	32.486004
665.600509	58122.157197	32.491021
666.004160	58230.351653	32.496039
666.845854	58304.486955	32.501056
667.527744	58414.235051	32.506074
668.427312	58511.715000	32.511092
668.927783	58615.598923	32.516109
669.838920	58699.082125	32.521127
670.755924	58800.080103	32.526144
671.061089	58899.625237	32.531162
671.757615	58986.266537	32.536180
672.302939	59102.997937	32.541197
672.733404	59188.673055	32.546215
673.585293	59284.692390	32.551232
674.200973	59401.060063	32.556250
674.793395	59482.760400	32.561268
675.620112	59599.498788	32.566285
675.787295	59713.749683	32.571303
676.687778	59796.961219	32.576320
677.201963	59872.913145	32.581338
677.494869	59979.056440	32.586356
678.494869	60093.879703	32.591373
678.812263	60197.479837	32.596391
679.429523	60302.528625	32.601408
680.057341	60415.102385	32.606426
680.966670	60512.628430	32.611444
682.126730	60594.391229	32.616461
682.676169	60708.628908	32.621479
683.616347	60818.151684	32.626496
684.406674	60934.587909	32.631514
684.709181	61014.370741	32.636532
685.617186	61116.822748	32.641549
685.995713	61216.297786	32.646567
687.125270	61314.258999	32.651584
687.284983	61417.935710	32.656602
687.739642	61524.458596	32.661620
688.459296	61659.054116	32.666637
689.142739	61763.404461	32.671655
690.330718	61855.759477	32.676672
690.679485	61971.225561	32.681690
691.183623	62088.556243	32.686708
692.248968	62186.108879	32.691725
692.312490	62321.303795	32.696743
693.383240	62448.439794	32.701760
694.074482	62551.889188	32.706778
694.574219	62656.546239	32.711796
695.225857	62783.690361	32.716813
695.461656	62899.142475	32.721831
696.758954	63027.217970	32.726848
697.247192	63144.032830	32.731866
697.972921	63263.577340	32.736884
699.080852	63398.442629	32.741901
699.688374	63508.938717	32.746919
700.384495	63619.281729	32.751936
701.092125	63743.553239	32.756954
702.194155	63839.072655	32.761972
702.555445	63971.935120	32.766989
703.802246	64103.173248	32.772007
704.482911	64189.441379	32.777024
705.735529	64291.087773	32.782042
705.836230	64425.013807	32.787060
706.925885	64509.894775	32.792077
707.559428	64636.699509	32.797095
708.103509	64748.167183	32.802112
709.139743	64843.607359	32.807130
709.808023	64962.280110	32.812148
710.722829	65063.303506	32.817165
711.049740	65177.565181	32.822183
712.011454	65275.535308	32.827200
712.495909	65370.000859	32.832218
712.979220	65503.485183	32.837236
713.710926	65599.213037	32.842253
714.579922	65725.517876	32.847271
715.213184	65839.840093	32.852288
716.042457	65939.775771	32.857306
716.594648	66071.488867	32.862324
717.196694	66170.552971	32.867341
717.683008	66275.350863	32.872359
718.376640	66408.319596	32.877376
719.246275	66515.457406	32.882394
720.036655	66636.749221	32.887412
720.583250	66746.242467	32.892429
720.846838	66880.473633	32.897447
721.779300	67012.300597	32.902464
722.303949	67124.169931	32.907482
723.283612	67228.341225	32.912500
724.205813	67346.612806	32.917517
724.646221	67486.115979	32.922535
725.315733	67585.270532	32.927552
726.221486	67689.595419	32.932570
726.966694	67795.692071	32.937588
727.979754	67916.202338	32.942605
728.956709	68025.972626	32.947623
729.339236	68124.532345	32.952640
730.081933	68241.978928	32.957658
730.443124	68360.709255	32.962676
731.426764	68458.134530	32.967693
732.112631	68584.246810	32.972711
732.852664	68689.109807	32.977728
733.736915	68810.398803	32.982746
734.115319	68954.435795	32.987764
734.985216	69061.156796	32.992781
735.664382	69178.404190	32.997799
736.082697	69308.389766	33.002816
736.874376	69423.533710	33.007834
737.465653	69546.727689	33.012852
738.629230	69687.036501	33.017869
738.661272	69813.820493	33.022887
739.434073	69961.270089	33.027904
740.171392	70080.384266	33.032922
740.858048	70228.893119	33.037940
742.267928	70333.754871	33.042957
743.014460	70465.179120	33.047975
744.065626	70598.381033	33.052992
744.867125	70718.398631	33.058010
745.157462	70873.963682	33.063028
746.042984	70975.836206	33.068045
746.560186	71107.612121	33.073063
747.645054	71242.766174	33.078080
748.239907	71355.809841	33.083098
748.505925	71501.659433	33.088116
749.214465	71623.954680	33.093133
750.283102	71766.607072	33.098151
751.223268	71909.616741	33.103168
752.438587	72047.081133	33.108186
752.948625	72169.741085	33.113204
753.614792	72305.053238	33.118221
754.448756	72439.345849	33.123239
755.124008	72570.187913	33.128256
756.266283	72683.122940	33.133274
756.975341	72831.583081	33.138292
757.618479	72950.918619	33.143309
758.152877	73078.954343	33.148327
759.002539	73208.070606	33.153344
760.105126	73345.169946	33.158362
760.637903	73483.679481	33.163380
761.307239	73603.842667	33.168397
762.462262	73742.194207	33.173415
762.960777	73871.644352	33.178432
763.932998	73999.025200	33.183450
764.443782	74140.628390	33.188468
765.335782	74244.229089	33.193485
765.953018	74389.901259	33.198503
766.776508	74541.452817	33.203520
767.383299	74662.783120	33.208538
768.141441	74794.586230	33.213556
768.955805	74934.373898	33.218573
769.921119	75048.109421	33.223591
770.318598	75184.540136	33.228608
771.253329	75323.817197	33.233626
772.149076	75474.787907	33.238644
772.884005	75598.581213	33.243661
773.357747	75731.689105	33.248679
774.251316	75854.603956	33.253696
775.285350	75975.207051	33.258714
776.057354	76122.250253	33.263732
776.466622	76242.926383	33.268749
777.391606	76365.016813	33.273767
777.715053	76504.155748	33.278784
778.838260	76618.391998	33.283802
779.284425	76735.845798	33.288820
780.270996	76879.430996	33.293837
780.976712	77028.818552	33.298855
781.842469	77142.398070	33.303872
782.934733	77295.239896	33.308890
783.210544	77414.686003	33.313908
784.105936	77546.938472	33.318925
785.010832	77678.886599	33.323943
785.669985	77836.426859	33.328960
786.400389	77954.213396	33.333978
787.318534	78105.173300	33.338996
788.121931	78236.129610	33.344013
789.017268	78379.398168	33.349031
789.578096	78530.173331	33.354048
791.038370	78649.025770	33.359066
791.608770	78788.511563	33.364084
792.489803	78939.717326	33.369101
793.380038	79070.746474	33.374119
793.980444	79197.283023	33.379136
794.262513	79333.221031	33.384154
795.228470	79485.460104	33.389172
795.779494	79622.310533	33.394189
797.021448	79774.733715	33.399207
797.462193	79910.256904	33.404224
798.454603	80067.119205	33.409242
799.082333	80233.783536	33.414260
800.158755	80366.478401	33.419277
801.092992	80485.345332	33.424295
801.612019	80638.210069	33.429312
802.466528	80804.082185	33.434330
803.479392	80949.378356	33.439348
804.112484	81090.342046	33.444365
805.377798	81231.815790	33.449383
805.939156	81366.360117	33.454400
806.956855	81514.455010	33.459418
807.571417	81653.097519	33.464436
808.854516	81794.888159	33.469453
809.866565	81953.335525	33.474471
810.251680	82091.873141	33.479488
811.160545	82214.055435	33.484506
811.822610	82370.577264	33.489524
812.450522	82498.310885	33.494541
813.645752	82660.579050	33.499559
814.545242	82797.157294	33.504576
815.122809	82936.022563	33.509594
815.934580	83109.130273	33.514612
816.364236	83243.296372	33.519629
817.259307	83392.682730	33.524647
817.885462	83551.938858	33.529664
818.931503	83678.996473	33.534682
819.674234	83847.699276	33.539700
820.398958	83987.166646	33.544717
821.518659	84135.711049	33.549735
822.410710	84294.365437	33.554752
823.324766	84430.255219	33.559770
824.015823	84599.946382	33.564788
824.633472	84733.546162	33.569805
825.303275	84897.017869	33.574823
825.867196	85035.170669	33.579840
826.997998	85183.454348	33.584858
827.575556	85349.955945	33.589876
828.355251	85482.900686	33.594893
829.894248	85651.194305	33.599911
830.374371	85793.838454	33.604928
831.577359	85947.619374	33.609946
832.121338	86084.959312	33.614964
832.714030	86230.327069	33.619981
833.441652	86352.055355	33.624999
834.080162	86509.039712	33.630016
835.064728	86665.202437	33.635034
835.687966	86816.832503	33.640052
836.574002	86965.199721	33.645069
837.384707	87134.029360	33.650087
838.076491	87289.757464	33.655104
838.718073	87441.799854	33.660122
839.520461	87602.592486	33.665140
840.572860	87787.514965	33.670157
841.091549	87946.414361	33.675175
841.716794	88104.816370	33.680192
842.709268	88266.373118	33.685210
843.542675	88450.508138	33.690228
844.482883	88612.961754	33.695245
845.283618	88791.524041	33.700263
846.374879	88952.063148	33.705280
847.103000	89127.754629	33.710298
848.161962	89306.664188	33.715316
849.440537	89465.941997	33.720333
850.453962	89616.336244	33.725351
851.217823	89799.411310	33.730368
852.221599	89943.304289	33.735386
853.501598	90103.199979	33.740404
854.343131	90270.636080	33.745421
855.327450	90418.255980	33.750439
855.946156	90590.508739	33.755456
857.119989	90725.202829	33.760474
857.677919	90891.532129	33.765492
858.007290	91073.910469	33.770509
859.272149	91221.425777	33.775527
859.714286	91390.555758	33.780544
860.623742	91551.237510	33.785562
861.760470	91716.420202	33.790580
862.480035	91886.621681	33.795597
863.899208	92033.755837	33.800615
864.487882	92205.443058	33.805632
865.293595	92379.203056	33.810650
866.360528	92530.543582	33.815668
867.288577	92701.399924	33.820685
868.485920	92856.030809	33.825703
869.051373	93017.601952	33.830720
869.780982	93168.318717	33.835738
870.867745	93344.925188	33.840756
871.673598	93510.200224	33.845773
872.186624	93672.740072	33.850791
873.228945	93836.782160	33.855808
874.381779	94008.148633	33.860826
875.126683	94178.501431	33.865844
875.739843	94336.231881	33.870861
876.549402	94499.297940	33.875879
877.443818	94674.762384	33.880896
878.174092	94842.160268	33.885914
879.239022	95000.364751	33.890932
880.351880	95161.252259	33.895949
881.940978	95305.403655	33.900967
882.534903	95485.436319	33.905984
883.377150	95659.587345	33.911002
884.309307	95804.204610	33.916020
884.972100	95950.873630	33.921037
885.651419	96121.206578	33.926055
886.804528	96300.317437	33.931072
887.643081	96459.119438	33.936090
888.618401	96610.950017	33.941108
889.297738	96762.058196	33.946125
890.520448	96885.739853	33.951143
890.789659	97049.355265	33.956160
891.339732	97212.267099	33.961178
892.504181	97371.863047	33.966196
893.027636	97546.440917	33.971213
893.942091	97701.155683	33.976231
894.848342	97893.301441	33.981248
895.751884	98049.830545	33.986266
896.446365	98224.346987	33.991284
896.895522	98397.297338	33.996301
898.024844	98545.461980	34.001319
898.922562	98730.070202	34.006336
899.890992	98925.942137	34.011354
901.432342	99091.171430	34.016372
902.091093	99261.231935	34.021389
902.838453	99435.463291	34.026407
903.775444	99614.766805	34.031424
904.581176	99783.078415	34.036442
905.665226	99963.240070	34.041460
906.477465	100154.393289	34.046477
907.695236	100320.380499	34.051495
908.329208	100490.782642	34.056512
909.339180	100683.091055	34.061530
910.397752	100850.000669	34.066548
911.062462	101044.584579	34.071565
912.153616	101239.371802	34.076583
913.163214	101424.278963	34.081600
913.719469	101596.872880	34.086618
914.859576	101782.571460	34.091636
915.506132	101964.320092	34.096653
916.437540	102137.311577	34.101671
917.154474	102351.674878	34.106688
918.156668	102548.816679	34.111706
919.191404	102740.243961	34.116724
919.932385	102941.268589	34.121741
920.878174	103114.948113	34.126759
921.835871	103325.873663	34.131776
922.483546	103532.097321	34.136794
923.954882	103697.216394	34.141812
924.755344	103893.882714	34.146829
925.859871	104089.082091	34.151847
927.021846	104270.477125	34.156864
927.615246	104471.487473	34.161882
928.789500	104683.813025	34.166900
929.681401	104863.920862	34.171917
930.712364	105034.756399	34.176935
931.666589	105232.458610	34.181952
932.612728	105447.069532	34.186970
933.637589	105621.734350	34.191988
934.354123	105818.099933	34.197005
935.469488	106004.042121	34.202023
936.302651	106184.916002	34.207040
937.106508	106395.619765	34.212058
938.290370	106563.704686	34.217076
939.164001	106767.099065	34.222093
940.402541	106968.864402	34.227111
941.339607	107145.554890	34.232128
942.269348	107343.929384	34.237146
943.362265	107540.100127	34.242164
943.914230	107716.668074	34.247181
944.857626	107906.559230	34.252199
945.494922	108112.016748	34.257216
946.548242	108304.121635	34.262234
947.523449	108517.315465	34.267252
948.083406	108708.884162	34.272269
948.828811	108888.227002	34.277287
950.040589	109088.683143	34.282304
950.637690	109276.716181	34.287322
951.762088	109460.547198	34.292340
952.660213	109663.022610	34.297357
953.781531	109872.378183	34.302375
954.636434	110070.646147	34.307392
955.274744	110258.615976	34.312410
956.432893	110438.965043	34.317428
957.558677	110651.378478	34.322445
958.231741	110850.657525	34.327463
959.565137	111058.809407	34.332480
960.174303	111245.296340	34.337498
961.379328	111424.719643	34.342516
962.269307	111643.158400	34.347533
963.188028	111857.325520	34.352551
964.283015	112049.488451	34.357568
965.134160	112275.348761	34.362586
966.323093	112473.769273	34.367604
967.202139	112671.799052	34.372621
968.182474	112874.082367	34.377639
969.021665	113080.266652	34.382656
969.723429	113290.807404	34.387674
971.101726	113498.729935	34.392692
971.909765	113711.751860	34.397709
973.101627	113918.162924	34.402727
974.153950	114139.584462	34.407744
974.945917	114348.053610	34.412762
976.261488	114538.892868	34.417780
977.192977	114755.816883	34.422797
978.031308	114983.905897	34.427815
979.154845	115187.968831	34.432832
979.941007	115395.420727	34.437850
981.588601	115600.844366	34.442868
982.391056	115814.567550	34.447885
982.994722	116020.850747	34.452903
984.193956	116252.222436	34.457920
985.438537	116474.771098	34.462938
986.074932	116668.194886	34.467956
987.456319	116880.893168	34.472973
988.159925	117084.063827	34.477991
989.209095	117283.428842	34.483008
989.994126	117517.691929	34.488026
991.065274	117748.058249	34.493044
991.958372	117947.403060	34.498061
992.853162	118152.450285	34.503079
994.353840	118378.392523	34.508096
995.151218	118600.968507	34.513114
996.641457	118808.620831	34.518132
997.936803	119036.097253	34.523149
998.479785	119229.997485	34.528167
999.349319	119442.115396	34.533184
1000.143244	119660.911890	34.538202
1001.563675	119853.936627	34.543220
1002.303650	120092.054840	34.548237
1002.838729	120307.655397	34.553255
1003.979081	120537.285338	34.558272
1005.066708	120764.974534	34.563290
1006.028301	120962.479213	34.568308
1008.241970	121168.610120	34.573325
1009.324193	121396.039107	34.578343
1011.058656	121594.839665	34.583360
1011.803335	121767.474399	34.588378
1013.029264	121969.516596	34.593396
1013.547979	122174.147861	34.598413
1014.581603	122364.731691	34.603431
1015.682682	122571.841897	34.608448
1016.166080	122780.221335	34.613466
1017.137249	122966.460392	34.618484
1018.121014	123157.032286	34.623501
1018.506231	123366.762641	34.628519
1019.625261	123556.503805	34.633536
1020.579540	123765.484120	34.638554
1021.611527	123957.345793	34.643572
1022.341871	124169.343882	34.648589
1023.229872	124377.363724	34.653607
1024.278044	124578.642249	34.658624
1024.734924	124815.147736	34.663642
1025.759063	125023.035588	34.668660
1026.706831	125262.390950	34.673677
1027.641993	125480.371432	34.678695
1028.274383	125715.131612	34.683712
1028.816672	125950.605524	34.688730
1030.138424	126170.516872	34.693748
1031.499868	126413.044786	34.698765
1032.352397	126680.675621	34.703783
1033.399377	126917.138354	34.708800
1033.970195	127168.991058	34.713818
1035.065071	127415.563195	34.718836
1036.198437	127668.531178	34.723853
1037.158236	127903.000914	34.728871
1038.455582	128179.975516	34.733888
1039.500823	128430.771827	34.738906
1040.771406	128668.554760	34.743924
1041.838087	128935.561811	34.748941
1042.755553	129179.553993	34.753959
1044.309187	129424.685181	34.758976
1045.430733	129696.480720	34.763994
1046.871335	129940.532007	34.769012
1047.900484	130166.579060	34.774029
1049.522052	130382.149330	34.779047
1050.860068	130638.492252	34.784064
1051.598194	130870.460962	34.789082
1052.756924	131102.767571	34.794100
1054.417498	131356.743642	34.799117
1055.296093	131580.379553	34.804135
1056.462565	131803.487878	34.809152
1057.754582	132018.730977	34.814170
1058.712000	132238.999600	34.819188
1059.428845	132480.186222	34.824205
1060.178031	132701.886786	34.829223
1061.387421	132939.015442	34.834240
1062.721025	133194.518110	34.839258
1063.829517	133412.070032	34.844276
1065.102872	133645.187817	34.849293
1065.764535	133888.726710	34.854311
1066.907644	134101.498729	34.859328
1068.180386	134334.545617	34.864346
1069.236336	134585.262951	34.869364
1070.402826	134822.476148	34.874381
1071.088818	135036.813024	34.879399
1072.155130	135250.213853	34.884416
1073.109398	135502.996110	34.889434
1074.083027	135757.970263	34.894452
1075.270246	135985.972508	34.899469
1075.841576	136240.877443	34.904487
1077.166787	136478.355538	34.909504
1078.382374	136724.043006	34.914522
1079.340814	136962.954345	34.919540
1080.265367	137213.041898	34.924557
1081.050117	137473.347231	34.929575
1082.351518	137705.513621	34.934592
1083.071120	137962.055646	34.939610
1084.361007	138207.285607	34.944628
1085.473055	138459.494285	34.949645
1086.465143	138726.900350	34.954663
1087.479691	138972.878757	34.959680
1088.437215	139208.307414	34.964698
1089.517846	139443.527243	34.969716
1090.646333	139685.650588	34.974733
1091.677502	139944.590823	34.979751
1092.775917	140195.331565	34.984768
1093.861135	140421.327494	34.989786
1094.655319	140676.369436	34.994804
1096.228012	140929.826723	34.999821
1096.729864	141195.190782	35.004839
1098.196443	141434.773193	35.009856
1099.241778	141692.710244	35.014874
1099.893592	141957.142627	35.019892
1101.199298	142191.558441	35.024909
1102.105604	142455.331401	35.029927
1103.253707	142733.343698	35.034944
1104.370430	143009.829197	35.039962
1105.383049	143258.857016	35.044980
1107.184994	143530.985877	35.049997
1107.805555	143804.655995	35.055015
1108.849327	144062.027918	35.060032
1109.707406	144342.244050	35.065050
1111.025041	144612.229680	35.070068
1112.214606	144886.093388	35.075085
1113.302692	145149.692138	35.080103
1114.598486	145424.024399	35.085120
1115.787229	145683.781034	35.090138
1116.736922	145980.315244	35.095156
1117.954948	146252.764717	35.100173
1119.202692	146524.323725	35.105191
1120.268081	146802.344229	35.110208
1121.832135	147070.532781	35.115226
1122.456484	147341.706409	35.120244
1123.939461	147617.419787	35.125261
1125.357456	147915.084959	35.130279
1126.802821	148173.790323	35.135296
1127.857651	148435.973390	35.140314
1128.892701	148708.002673	35.145332
1130.217127	148979.770652	35.150349
1131.281577	149244.748032	35.155367
1132.641862	149512.760252	35.160384
1133.663875	149801.070973	35.165402
1134.506726	150065.621697	35.170420
1135.663723	150326.089509	35.175437
1137.166733	150615.227720	35.180455
1137.879634	150888.176251	35.185472
1138.933225	151153.334186	35.190490
1140.205889	151438.052633	35.195508
1141.510792	151704.910585	35.200525
1142.431450	151993.496260	35.205543
1143.406657	152260.818498	35.210560
1145.360041	152537.785203	35.215578
1146.403886	152801.992648	35.220596
1147.946014	153041.907386	35.225613
1149.210985	153339.692746	35.230631
1150.048007	153604.726367	35.235648
1151.482328	153866.593844	35.240666
1152.252493	154152.874583	35.245684
1153.669723	154414.837471	35.250701
1154.728021	154665.027441	35.255719
1155.678533	154955.622330	35.260736
1156.796398	155238.505316	35.265754
1157.857245	155497.147865	35.270772
1159.101381	155768.953426	35.275789
1160.126428	156027.465937	35.280807
1160.868275	156314.287626	35.285824
1161.823245	156609.270409	35.290842
1163.212661	156883.837744	35.295860
1164.395006	157138.209252	35.300877
1165.437185	157406.533353	35.305895
1166.893936	157690.266303	35.310912
1167.941938	157952.846990	35.315930
1168.428053	158223.031681	35.320948
1170.002786	158497.288022	35.325965
1171.074489	158775.992994	35.330983
1171.949525	159065.096227	35.336000
1173.577719	159330.710890	35.341018
1174.786016	159590.434505	35.346036
1176.015572	159856.562473	35.351053
1176.724053	160151.955041	35.356071
1177.748115	160440.815317	35.361088
1178.848841	160723.309452	35.366106
1179.738386	161024.856512	35.371124
1181.019196	161300.626836	35.376141
1182.019956	161617.142047	35.381159
1183.320033	161904.279983	35.386176
1184.386685	162215.118269	35.391194
1185.413310	162511.503126	35.396212
1186.756399	162798.526067	35.401229
1188.134703	163129.237495	35.406247
1189.049916	163450.259329	35.411264
1190.424415	163745.441159	35.416282
1191.578178	164036.741309	35.421300
1192.964984	164347.263701	35.426317
1194.030408	164665.783494	35.431335
1194.923991	164997.972672	35.436352
1196.120501	165295.833745	35.441370
1197.100477	165604.212333	35.446388
1198.847134	165926.346575	35.451405
1200.215036	166260.408545	35.456423
1201.223014	166583.151813	35.461440
1202.531370	166894.467122	35.466458
1203.803351	167207.541600	35.471476
1204.990280	167524.134234	35.476493
1206.028209	167863.515910	35.481511
1207.373502	168175.925533	35.486528
1208.864180	168496.586048	35.491546
1210.449186	168804.938485	35.496564
1211.863930	169097.346648	35.501581
1213.311600	169422.563450	35.506599
1214.177253	169753.296696	35.511616
1215.613060	170063.776178	35.516634
1216.524475	170383.873564	35.521652
1217.576770	170687.746475	35.526669
1218.675736	171010.177499	35.531687
1219.774711	171352.836980	35.536704
1221.155728	171659.974025	35.541722
1222.115129	171977.663946	35.546740
1223.158475	172311.863562	35.551757
1225.136669	172633.996087	35.556775
1225.926576	172944.043713	35.561792
1227.515741	173286.294251	35.566810
1228.538444	173621.090548	35.571828
1229.923761	173932.366268	35.576845
1231.230528	174270.038989	35.581863
1232.279757	174586.285492	35.586880
1233.349052	174905.297222	35.591898
1234.965212	175230.781584	35.596916
1236.676509	175548.943009	35.601933
1237.585014	175883.076413	35.606951
1238.809699	176192.058660	35.611968
1240.286840	176503.171290	35.616986
1241.395631	176845.209848	35.622004
1242.534058	177165.240606	35.627021
1243.912399	177484.091739	35.632039
1244.858702	177784.399069	35.637056
1246.359745	178093.677891	35.642074
1247.805678	178423.057366	35.647092
1248.799052	178727.956830	35.652109
1250.278238	179024.655767	35.657127
1251.453400	179344.060238	35.662144
1253.023062	179627.117655	35.667162
1253.855815	179935.465014	35.672180
1255.164723	180238.379961	35.677197
1256.498967	180551.661421	35.682215
1257.479353	180866.627752	35.687232
1258.813191	181161.129719	35.692250
1259.400049	181490.595177	35.697268
1260.593000	181807.740628	35.702285
1262.229430	182131.909558	35.707303
1263.012907	182464.750257	35.712320
1264.211274	182774.945671	35.717338
1264.930833	183129.897886	35.722356
1266.425046	183462.792709	35.727373
1268.351412	183803.284416	35.732391
1269.071836	184130.548967	35.737408
1270.591139	184471.987977	35.742426
1271.618276	184799.954917	35.747444
1272.961725	185146.758135	35.752461
1274.577049	185501.286609	35.757479
1275.939203	185852.635283	35.762496
1277.591939	186186.828455	35.767514
1278.832826	186534.139915	35.772532
1279.948334	186866.750509	35.777549
1280.793025	187201.692575	35.782567
1282.654645	187559.646404	35.787584
1284.201656	187889.209128	35.792602
1285.544901	188225.674493	35.797620
1287.028569	188562.524910	35.802637
1288.100168	188908.610002	35.807655
1289.417493	189249.071555	35.812672
1290.788376	189567.591897	35.817690
1291.524244	189934.061071	35.822708
1292.896657	190291.415025	35.827725
1294.477247	190617.421321	35.832743
1295.591419	190985.751576	35.837760
1297.141956	191327.545323	35.842778
1297.927186	191672.691680	35.847796
1299.444315	192039.045339	35.852813
1300.690268	192390.162285	35.857831
1301.973045	192752.001880	35.862848
1303.030148	193122.893902	35.867866
1304.303783	193461.597612	35.872884
1305.539120	193832.324999	35.877901
1307.119142	194192.829460	35.882919
1308.196240	194583.530723	35.887936
1309.670334	194939.931368	35.892954
1311.160486	195298.692674	35.897972
1312.496085	195663.143489	35.902989
1313.877716	196006.223311	35.908007
1315.554990	196372.132612	35.913024
1316.843428	196754.294450	35.918042
1317.709255	197120.011982	35.923060
1319.058438	197467.599263	35.928077
1320.365277	197823.942489	35.933095
1321.621687	198189.563642	35.938112
1323.773116	198541.645485	35.943130
1325.097377	198893.510299	35.948148
1326.532609	199248.431034	35.953165
1327.953824	199620.596689	35.958183
1329.077853	199982.314154	35.963200
1330.076098	200314.612862	35.968218
1331.667066	200662.266243	35.973236
1332.629017	201041.473011	35.978253
1334.090581	201407.230597	35.983271
1335.065079	201752.756879	35.988288
1336.645309	202080.702409	35.993306
1337.609757	202441.646917	35.998324
1338.597377	202786.211351	36.003341
1340.312022	203133.082507	36.008359
1341.259274	203500.764421	36.013376
1342.865745	203859.515450	36.018394
1343.935493	204194.665235	36.023412
1345.372262	204553.917571	36.028429
1346.663810	204936.963760	36.033447
1347.958954	205318.919486	36.038464
1349.620175	205673.328342	36.043482
1350.831211	206020.322107	36.048500
1352.018246	206385.541493	36.053517
1353.410215	206770.066308	36.058535
1354.846701	207131.109010	36.063552
1356.107895	207504.092236	36.068570
1357.691575	207876.033715	36.073588
1359.204821	208235.773952	36.078605
1360.700720	208601.054753	36.083623
1362.044485	208983.592653	36.088640
1363.297206	209356.103851	36.093658
1365.051793	209722.071013	36.098676
1366.528313	210090.942714	36.103693
1367.715475	210468.523625	36.108711
1369.046450	210837.206964	36.113728
1370.303891	211196.482467	36.118746
1371.999454	211602.884724	36.123764
1372.974550	211977.282500	36.128781
1374.739665	212340.466385	36.133799
1375.652923	212735.994344	36.138816
1377.240470	213108.696242	36.143834
1378.775409	213466.881947	36.148852
1379.835795	213878.707974	36.153869
1381.364565	214254.522963	36.158887
1382.646735	214650.519628	36.163904
1383.824555	215053.976504	36.168922
1385.320038	215499.261859	36.173940
1386.582125	215878.861188	36.178957
1387.813269	216288.206963	36.183975
1389.063905	216687.925937	36.188992
1390.429874	217086.814938	36.194010
1392.133127	217484.532544	36.199028
1393.273314	217893.113251	36.204045
1394.710331	218296.846656	36.209063
1396.468555	218689.912625	36.214080
1397.890880	219114.071567	36.219098
1398.964003	219527.546774	36.224116
1400.509156	219932.361379	36.229133
1402.346290	220329.865666	36.234151
1403.162332	220731.730751	36.239168
1404.872069	221133.094400	36.244186
1406.653939	221523.043933	36.249204
1408.165587	221945.930438	36.254221
1409.631324	222344.494538	36.259239
1410.389514	222735.277990	36.264256
1411.883689	223129.090878	36.269274
1413.359514	223548.764190	36.274292
1414.914184	223952.196278	36.279309
1416.637388	224344.756717	36.284327
1418.373016	224769.522495	36.289344
1419.492544	225168.459073	36.294362
1420.979755	225564.339293	36.299380
1421.640470	225972.396573	36.304397
1423.301519	226375.311950	36.309415
1424.491041	226791.082495	36.314432
1426.098880	227209.808040	36.319450
1427.523803	227604.892767	36.324468
1428.682946	228025.879612	36.329485
1430.196790	228421.638147	36.334503
1431.417948	228808.505494	36.339520
1432.717524	229204.301910	36.344538
1434.326840	229611.097497	36.349556
1435.489732	230028.712330	36.354573
1437.058222	230414.663687	36.359591
1438.284920	230833.388203	36.364608
1439.869432	231241.336034	36.369626
1441.318724	231640.163255	36.374644
1442.566920	232063.637972	36.379661
1443.920523	232459.181312	36.384679
1445.786983	232896.603102	36.389696
1447.004996	233311.856773	36.394714
1449.076696	233708.885365	36.399732
1450.774209	234125.891114	36.404749
1452.480889	234527.351124	36.409767
1453.960512	234951.380422	36.414784
1455.535921	235356.039436	36.419802
1457.224083	235746.938859	36.424820
1458.670425	236170.062559	36.429837
1459.853963	236563.816018	36.434855
1461.499367	236960.008956	36.439872
1462.687312	237388.207962	36.444890
1464.615549	237797.183963	36.449908
1465.661305	238206.865411	36.454925
1467.187278	238610.422997	36.459943
1468.403707	239048.248669	36.464960
1469.998264	239461.627328	36.469978
1471.635649	239879.368968	36.474996
1473.094917	240300.722603	36.480013
1474.395568	240714.304958	36.485031
1475.854117	241154.686630	36.490048
1476.737901	241592.674732	36.495066
1478.360570	242019.415741	36.500084
1479.705423	242470.919761	36.505101
1481.141842	242887.253001	36.510119
1482.891264	243320.072255	36.515136
1484.082931	243765.177497	36.520154
1485.896357	244220.850000	36.525172
1487.116531	244658.992036	36.530189
1488.238008	245107.947201	36.535207
1490.274018	245544.889320	36.540224
1491.752651	245990.459426	36.545242
1493.585410	246434.168284	36.550260
1494.670670	246893.014179	36.555277
1496.257827	247329.753921	36.560295
1497.914200	247779.057253	36.565312
1499.446868	248251.091738	36.570330
1500.966330	248682.205277	36.575348
1502.320071	249131.992421	36.580365
1503.900992	249579.608868	36.585383
1505.502353	250013.657410	36.590400
1506.821571	250478.871614	36.595418
1508.286430	250938.727771	36.600436
1509.408419	251408.878468	36.605453
1511.204432	251856.284434	36.610471
1512.510776	252320.309061	36.615488
1513.825574	252798.609312	36.620506
1515.664083	253245.095204	36.625524
1516.773574	253731.152832	36.630541
1518.359866	254196.200075	36.635559
1519.974528	254658.626517	36.640576
1520.995077	255139.238426	36.645594
1522.919315	255610.531045	36.650612
1524.326720	256083.890737	36.655629
1526.225562	256537.634575	36.660647
1528.006410	257011.466708	36.665664
1529.316944	257483.369856	36.670682
1530.878376	257908.540648	36.675700
1532.309552	258362.870660	36.680717
1533.770827	258809.143041	36.685735
1535.317685	259251.209905	36.690752
1536.598511	259699.671616	36.695770
1538.382494	260168.728693	36.700788
1539.807896	260617.496982	36.705805
1541.442940	261081.345708	36.710823
1543.061717	261545.781434	36.715840
1544.488137	261998.919041	36.720858
1546.335122	262471.725615	36.725876
1547.750406	262933.527547	36.730893
1549.029718	263381.964319	36.735911
1550.612470	263864.264346	36.740928
1552.068725	264326.186290	36.745946
1553.840950	264790.977346	36.750964
1555.437505	265279.142840	36.755981
1556.751167	265748.861238	36.760999
1558.511146	266228.260629	36.766016
1560.034784	266693.854008	36.771034
1561.705314	267184.978532	36.776052
1563.264966	267641.598083	36.781069
1564.595235	268136.461579	36.786087
1566.580957	268621.360118	36.791104
1567.812926	269112.479394	36.796122
1569.404990	269585.553414	36.801140
1571.029372	270085.599769	36.806157
1572.590512	270562.564662	36.811175
1574.062648	271060.247238	36.816192
1575.496968	271560.120154	36.821210
1576.976986	272053.939026	36.826228
1578.611449	272557.969195	36.831245
1579.726739	273064.904087	36.836263
1581.494479	273570.638294	36.841280
1582.922256	274100.814591	36.846298
1584.412011	274612.080134	36.851316
1585.932773	275121.231316	36.856333
1587.509042	275655.800617	36.861351
1589.372882	276165.376081	36.866368
1590.634306	276700.655878	36.871386
1592.307660	277222.073069	36.876404
1594.075496	277742.533755	36.881421
1595.656383	278277.224213	36.886439
1597.794273	278780.271818	36.891456
1599.668625	279310.516982	36.896474
1601.575383	279843.245024	36.901492
1602.941239	280367.652921	36.906509
1604.655102	280873.687178	36.911527
1606.184785	281385.872544	36.916544
1607.340810	281916.890428	36.921562
1609.148427	282427.249206	36.926580
1610.622961	282960.066128	36.931597
1611.818509	283495.086772	36.936615
1613.731161	284017.413699	36.941632
1615.103059	284571.809116	36.946650
1616.758186	285098.442918	36.951668
1618.063250	285645.327133	36.956685
1619.470524	286183.683250	36.961703
1621.504168	286733.237910	36.966720
1622.438127	287263.413171	36.971738
1624.263113	287803.701762	36.976756
1626.493142	288362.489891	36.981773
1627.849100	288919.007111	36.986791
1629.599030	289440.251575	36.991808
1630.915531	289991.894331	36.996826
1632.707381	290558.951018	37.001844
1634.403506	291079.944464	37.006861
1636.086890	291623.214356	37.011879
1637.791725	292155.708766	37.016896
1639.180574	292667.297915	37.021914
1641.605006	293197.891421	37.026932
1643.733637	293697.213183	37.031949
1645.044131	294221.991838	37.036967
1646.979072	294725.507129	37.041984
1648.952713	295240.037526	37.047002
1650.412922	295757.977835	37.052020
1652.065417	296254.853301	37.057037
1653.966225	296763.090103	37.062055
1655.510281	297286.191413	37.067072
1657.331261	297792.963713	37.072090
1658.686755	298324.549351	37.077108
1660.493596	298835.535563	37.082125
1662.221153	299352.272652	37.087143
1663.766339	299883.616297	37.092160
1665.147676	300394.843187	37.097178
1666.629507	300929.544703	37.102196
1668.381626	301428.183908	37.107213
1669.837309	301966.465579	37.112231
1671.697320	302507.649283	37.117248
1672.795657	303036.028136	37.122266
1674.380862	303598.560212	37.127284
1675.996613	304156.969580	37.132301
1677.401118	304699.435480	37.137319
1679.023774	305260.758007	37.142336
1680.938273	305815.120970	37.147354
1682.735458	306387.455762	37.152372
1683.910625	306948.384770	37.157389
1685.383895	307518.099219	37.162407
1687.408260	308108.112635	37.167424
1688.682689	308696.620460	37.172442
1690.586212	309264.093957	37.177460
1692.325455	309857.723456	37.182477
1693.635275	310435.217031	37.187495
1695.332762	311028.261094	37.192512
1697.203315	311629.576733	37.197530
1698.804417	312219.529875	37.202548
1700.959002	312805.705100	37.207565
1702.295189	313397.699549	37.212583
1704.527276	313992.766915	37.217600
1706.171198	314584.879435	37.222618
1708.204328	315182.636971	37.227636
1709.727156	315777.528293	37.232653
1711.624101	316381.672844	37.237671
1713.404751	316942.027285	37.242688
1715.008430	317552.356040	37.247706
1716.642735	318161.303416	37.252724
1718.576522	318750.135608	37.257741
1720.063260	319366.004121	37.262759
1722.040016	319959.415384	37.267776
1723.715363	320556.324753	37.272794
1725.501584	321153.439239	37.277812
1727.150690	321760.854989	37.282829
1728.636203	322365.524594	37.287847
1730.430048	322976.739753	37.292864
1731.959359	323587.408957	37.297882
1733.399311	324189.251116	37.302900
1735.427729	324810.922591	37.307917
1737.150032	325426.443264	37.312935
1738.990515	326034.600684	37.317952
1740.482412	326666.524295	37.322970
1742.566514	327267.723526	37.327988
1744.190028	327895.855310	37.333005
1745.416141	328511.351525	37.338023
1747.812981	329136.905667	37.343040
1749.441799	329767.632464	37.348058
1750.842257	330354.696342	37.353076
1752.946179	330926.227580	37.358093
1754.827160	331542.828770	37.363111
1756.668921	332129.522935	37.368128
1758.047672	332725.198635	37.373146
1759.700708	333321.787648	37.378164
1761.298439	333923.685468	37.383181
1763.081358	334525.850982	37.388199
1764.934457	335141.148726	37.393216
1766.500948	335739.731971	37.398234
1768.257396	336345.867824	37.403252
1770.327248	336975.376332	37.408269
1771.318741	337614.118051	37.413287
1773.364251	338215.311345	37.418304
1775.120707	338847.083575	37.423322
1776.747019	339475.112826	37.428340
1778.523755	340114.481910	37.433357
1780.138568	340748.564618	37.438375
1782.211217	341392.768246	37.443392
1784.191782	342032.206909	37.448410
1785.816529	342664.284395	37.453428
1787.621585	343305.258927	37.458445
1789.262001	343962.776327	37.463463
1791.166878	344605.291390	37.468480
1793.064625	345241.631504	37.473498
1794.240271	345918.235752	37.478516
1796.411440	346577.458032	37.483533
1797.814705	347241.797946	37.488551
1799.882405	347886.679231	37.493568
1801.725795	348568.821117	37.498586
1803.413741	349237.096129	37.503604
1805.478769	349884.615313	37.508621
1807.608513	350570.715996	37.513639
1809.231286	351246.180357	37.518656
1811.141359	351906.436603	37.523674
1813.039848	352605.665297	37.528692
1815.021827	353262.590727	37.533709
1816.810736	353930.323534	37.538727
1818.713497	354609.091671	37.543744
1820.692684	355277.457865	37.548762
1822.410709	355957.885022	37.553780
1824.049245	356641.791029	37.558797
1825.805328	357311.837413	37.563815
1827.871276	358005.090647	37.568832
1829.718230	358676.521524	37.573850
1831.549277	359356.622138	37.578868
1833.790908	360035.857385	37.583885
1835.544041	360717.115812	37.588903
1837.578793	361386.797412	37.593920
1839.448251	362080.370449	37.598938
1841.004175	362754.802414	37.603956
1842.869497	363439.853364	37.608973
1844.854404	364124.568439	37.613991
1847.236397	364798.525328	37.619008
1848.845776	365463.617233	37.624026
1850.707573	366173.940774	37.629044
1852.886355	366834.019189	37.634061
1854.776613	367526.986295	37.639079
1856.171154	368202.975333	37.644096
1857.986922	368867.619707	37.649114
1859.866588	369559.105842	37.654132
1862.011721	370226.640044	37.659149
1863.951771	370920.399628	37.664167
1865.962569	371578.597094	37.669184
1868.597792	372240.459334	37.674202
1870.242763	372931.389078	37.679220
1872.537057	373594.399242	37.684237
1874.018276	374239.954196	37.689255
1876.033241	374875.796813	37.694272
1877.447994	375520.908665	37.699290
1878.979144	376177.250723	37.704308
1880.684531	376807.378159	37.709325
1882.310026	377458.177386	37.714343
1883.718420	378125.459860	37.719360
1885.630896	378778.241548	37.724378
1887.209286	379450.771058	37.729396
1888.848646	380139.558434	37.734413
1890.595602	380824.713260	37.739431
1891.981865	381502.788047	37.744448
1894.055323	382190.346751	37.749466
1895.684979	382889.832106	37.754484
1897.478291	383598.962369	37.759501
1899.431837	384326.155812	37.764519
1900.983615	385032.683678	37.769536
1903.164885	385726.211973	37.774554
1905.001053	386487.379008	37.779572
1907.278081	387186.514740	37.784589
1909.071453	387915.252463	37.789607
1910.712864	388653.734462	37.794624
1912.949980	389367.052726	37.799642
1914.244225	390118.842998	37.804660
1916.488101	390846.653728	37.809677
1918.357678	391612.840017	37.814695
1920.068870	392349.703391	37.819712
1922.238589	393104.877610	37.824730
1923.961910	393861.957538	37.829748
1925.728643	394610.722754	37.834765
1927.823274	395395.384163	37.839783
1929.723731	396172.681354	37.844800
1931.720417	396931.287671	37.849818
1933.748104	397689.185417	37.854836
1935.789878	398453.575376	37.859853
1938.115747	399236.197636	37.864871
1939.812023	399999.008067	37.869888
1941.552357	400786.323730	37.874906
1943.622351	401563.730918	37.879924
1945.548547	402344.764940	37.884941
1947.673347	403138.770494	37.889959
1949.713219	403896.885982	37.894976
1951.755902	404682.778717	37.899994
1954.107084	405467.762667	37.905012
1956.008087	406232.376316	37.910029
1958.424815	407021.056326	37.915047
1960.134223	407801.570905	37.920064
1962.690857	408566.266022	37.925082
1964.240561	409343.343194	37.930100
1966.088796	410124.833481	37.935117
1968.668892	410889.054866	37.940135
1970.175637	411665.439909	37.945152
1972.464530	412439.013779	37.950170
1974.464566	413234.449274	37.955188
1976.365492	413991.450031	37.960205
1978.385826	414785.113552	37.965223
1980.431706	415557.750764	37.970240
1982.321934	416325.983795	37.975258
1984.078091	417091.835623	37.980276
1986.116124	417885.225544	37.985293
1988.060828	418680.582146	37.990311
1989.861205	419470.898243	37.995328
1991.762140	420249.726510	38.000346
1993.712918	421041.590284	38.005364
1995.638756	421834.218607	38.010381
1997.532961	422625.485265	38.015399
1999.705314	423431.266732	38.020416
2001.630025	424225.187531	38.025434
2003.346270	425000.886776	38.030452
2005.174542	425798.242274	38.035469
2007.333815	426553.209723	38.040487
2009.267846	427334.572589	38.045504
2011.469736	428111.258629	38.050522
2013.368337	428871.159838	38.055540
2015.547764	429660.407721	38.060557
2017.321280	430429.900589	38.065575
2019.462815	431221.230061	38.070592
2021.529737	431997.560290	38.075610
2023.584400	432765.564797	38.080628
2025.403253	433538.696250	38.085645
2027.732339	434340.876125	38.090663
2029.318387	435153.072591	38.095680
2031.518681	435922.924269	38.100698
2033.624378	436724.148114	38.105716
2035.698995	437515.783257	38.110733
2038.015562	438321.573478	38.115751
2039.719298	439125.563882	38.120768
2042.049370	439925.778851	38.125786
2044.094881	440744.383037	38.130804
2045.913797	441552.772699	38.135821
2048.143148	442342.898966	38.140839
2050.115711	443172.509189	38.145856
2051.951838	443992.901910	38.150874
2054.332386	444817.728394	38.155892
2056.263021	445639.107193	38.160909
2058.515087	446448.057345	38.165927
2060.176905	447299.319640	38.170944
2062.270471	448107.020370	38.175962
2064.856976	448951.539411	38.180980
2066.819428	449801.338800	38.185997
2069.305959	450607.211994	38.191015
2071.599522	451444.953786	38.196032
2073.838955	452277.512389	38.201050
2076.084170	453083.534172	38.206068
2077.661044	453942.639872	38.211085
2079.998961	454764.362079	38.216103
2081.762696	455594.086680	38.221120
2083.944903	456431.699450	38.226138
2085.757381	457271.867863	38.231156
2087.854329	458134.305647	38.236173
2089.772384	458960.330443	38.241191
2091.675783	459823.791105	38.246208
2094.011824	460681.228361	38.251226
2095.786650	461545.749567	38.256244
2097.581116	462415.842308	38.261261
2099.717110	463264.659151	38.266279
2101.388558	464163.309941	38.271296
2103.464855	465042.290988	38.276314
2105.548817	465919.968235	38.281332
2107.398545	466820.744130	38.286349
2109.710287	467719.027168	38.291367
2111.597448	468606.068649	38.296384
2113.813798	469485.333811	38.301402
2115.801143	470405.278036	38.306420
2117.471247	471315.629586	38.311437
2119.767554	472208.856566	38.316455
2121.820308	473127.245221	38.321472
2123.794669	474042.773204	38.326490
2126.312290	474953.923559	38.331508
2128.185312	475885.344745	38.336525
2130.605508	476786.369115	38.341543
2132.238884	477717.991665	38.346560
2134.971852	478626.251257	38.351578
2137.021092	479566.047620	38.356596
2139.335447	480471.356321	38.361613
2141.700434	481411.309837	38.366631
2143.895625	482315.183818	38.371648
2146.121598	483183.707853	38.376666
2148.641556	484072.644412	38.381684
2150.637683	484965.511975	38.386701
2152.648618	485837.125646	38.391719
2154.637303	486728.695254	38.396736
2156.470005	487633.726672	38.401754
2158.502523	488511.568231	38.406772
2160.715262	489400.241158	38.411789
2162.944602	490321.982243	38.416807
2164.915584	491244.929208	38.421824
2166.976672	492140.454984	38.426842
2169.371309	493048.851467	38.431860
2171.027151	493979.075126	38.436877
2173.199877	494872.675502	38.441895
2175.609747	495804.796331	38.446912
2177.316701	496755.552668	38.451930
2179.460147	497683.275666	38.456948
2181.602912	498623.158853	38.461965
2183.979095	499564.818349	38.466983
2186.164739	500503.682044	38.472000
2188.045570	501448.799281	38.477018
2190.539144	502414.444870	38.482036
2192.580952	503379.957831	38.487053
2194.786284	504340.142109	38.492071
2196.747463	505306.262546	38.497088
2199.241273	506272.238616	38.502106
2201.284698	507233.441278	38.507124
2203.203237	508239.942560	38.512141
2205.316308	509203.438372	38.517159
2207.513291	510219.150288	38.522176
2209.566329	511202.302333	38.527194
2211.436980	512216.782706	38.532212
2213.343084	513214.204218	38.537229
2216.138493	514203.250561	38.542247
2218.017086	515243.447532	38.547264
2220.249579	516274.747839	38.552282
2222.597430	517293.109934	38.557300
2224.408456	518322.480797	38.562317
2226.797730	519346.901293	38.567335
2229.135400	520372.573041	38.572352
2231.765941	521391.931224	38.577370
2234.691722	522451.680911	38.582388
2236.973560	523476.601552	38.587405
2239.559951	524487.147109	38.592423
2242.093519	525524.231001	38.597440
2244.369704	526551.716487	38.602458
2246.752905	527558.968412	38.607476
2248.772775	528589.832744	38.612493
2251.257753	529602.319818	38.617511
2253.278787	530649.408815	38.622528
2255.649932	531674.564262	38.627546
2258.060616	532668.577536	38.632564
2260.317843	533705.392642	38.637581
2262.902060	534744.346159	38.642599
2265.193891	535763.390921	38.647616
2267.320466	536765.580235	38.652634
2269.580737	537799.034459	38.657652
2271.537823	538830.602887	38.662669
2274.208312	539836.063417	38.667687
2276.092646	540871.121054	38.672704
2278.423790	541911.766295	38.677722
2280.729182	542929.095500	38.682740
2282.935423	543981.685121	38.687757
2285.302721	544993.070613	38.692775
2287.846375	546021.004359	38.697792
2289.846538	547049.002832	38.702810
2292.609499	548083.388607	38.707828
2294.866116	549111.343976	38.712845
2297.501856	550085.203010	38.717863
2299.587470	551081.661481	38.722880
2301.939149	552071.869999	38.727898
2304.509596	553056.440754	38.732916
2306.308029	554059.367202	38.737933
2308.605816	555039.667503	38.742951
2310.839327	556032.122181	38.747968
2312.704060	557044.317724	38.752986
2314.904289	558037.434972	38.758004
2317.122375	559059.271472	38.763021
2319.258747	560080.943077	38.768039
2321.463532	561118.051335	38.773056
2323.747387	562132.054820	38.778074
2325.870499	563140.129397	38.783092
2327.608707	564206.713748	38.788109
2329.940804	565260.706920	38.793127
2331.985121	566300.850626	38.798144
2334.823327	567349.619826	38.803162
2336.971507	568440.450981	38.808180
2339.243314	569516.859101	38.813197
2341.118453	570598.715874	38.818215
2343.417240	571683.223463	38.823232
2345.549009	572806.623070	38.828250
2347.934806	573888.519951	38.833268
2350.389044	574996.765126	38.838285
2352.676736	576089.884543	38.843303
2354.841148	577226.137968	38.848320
2356.983372	578352.156379	38.853338
2359.448233	579461.111702	38.858356
2361.634715	580599.966153	38.863373
2364.242120	581743.362639	38.868391
2366.282359	582899.136995	38.873408
2368.410237	584047.967607	38.878426
2371.161982	585211.132110	38.883444
2373.799805	586352.942894	38.888461
2376.273534	587512.524603	38.893479
2378.707531	588672.202966	38.898496
2381.195325	589818.727154	38.903514
2383.493040	590982.167166	38.908532
2386.224151	592172.289059	38.913549
2388.769493	593328.143170	38.918567
2390.820192	594496.695693	38.923584
2393.741619	595660.530346	38.928602
2396.251367	596816.853280	38.933620
2398.554999	597997.695211	38.938637
2400.996234	599161.063798	38.943655
2403.563193	600317.684618	38.948672
2406.244416	601510.983210	38.953690
2409.086565	602651.500945	38.958708
2411.266722	603804.283594	38.963725
2413.863820	604981.616174	38.968743
2416.248333	606137.086039	38.973760
2418.618672	607305.857411	38.978778
2421.226612	608446.790910	38.983796
2423.352781	609642.742100	38.988813
2426.252471	610812.918136	38.993831
2428.507976	611973.121859	38.998848
2430.904907	613126.278388	39.003866
2433.784967	614292.494017	39.008884
2436.029824	615456.441828	39.013901
2439.111088	616608.526410	39.018919
2442.027001	617762.319188	39.023936
2443.984154	618899.347690	39.028954
2446.316825	620060.697657	39.033972
2448.746948	621216.909338	39.038989
2451.437638	622375.955499	39.044007
2453.695941	623512.306634	39.049024
2456.065413	624654.468418	39.054042
2458.728300	625768.325767	39.059060
2461.009544	626891.675462	39.064077
2463.317466	628012.555319	39.069095
2466.213668	629123.479159	39.074112
2468.059204	630245.101102	39.079130
2470.381184	631342.800920	39.084148
2472.557119	632482.314196	39.089165
2474.766341	633615.656972	39.094183
2477.280149	634751.574263	39.099200
2479.536607	635891.205917	39.104218
2481.896074	637024.756132	39.109236
2484.084179	638190.058475	39.114253
2486.283751	639369.303528	39.119271
2488.730129	640547.875017	39.124288
2490.591075	641712.985934	39.129306
2493.133615	642921.360298	39.134324
2495.697180	644130.836423	39.139341
2497.838499	645322.281962	39.144359
2500.247884	646544.018613	39.149376
2502.675670	647769.046640	39.154394
2505.429222	648975.672703	39.159412
2507.191561	650235.915402	39.164429
2509.621823	651460.994260	39.169447
2512.208449	652736.191964	39.174464
2514.454203	653990.799475	39.179482
2517.031794	655247.636226	39.184500
2519.613366	656522.499980	39.189517
2522.066837	657786.359922	39.194535
2525.267514	659067.220104	39.199552
2527.703851	660379.417771	39.204570
2530.335430	661641.407935	39.209588
2532.607936	662935.261846	39.214605
2535.016909	664223.096066	39.219623
2537.826481	665509.149955	39.224640
2540.128136	666833.591559	39.229658
2542.849531	668149.619948	39.234676
2545.479115	669441.100371	39.239693
2547.756224	670738.683560	39.244711
2550.665829	672066.579893	39.249728
2553.103025	673406.057072	39.254746
2555.751005	674703.733327	39.259764
2558.376806	676024.257562	39.264781
2561.041358	677353.389909	39.269799
2563.620898	678674.542742	39.274816
2565.919157	679990.733399	39.279834
2568.803399	681336.558919	39.284852
2571.465135	682671.641470	39.289869
2573.681064	683994.084185	39.294887
2576.438060	685334.875976	39.299904
2578.754709	686687.464580	39.304922
2581.270621	688024.822299	39.309940
2584.173993	689375.326116	39.314957
2586.539791	690722.242111	39.319975
2589.082083	692057.660160	39.324992
2591.672166	693434.016857	39.330010
2594.122711	694800.558377	39.335028
2596.626832	696159.737443	39.340045
2599.640052	697509.695657	39.345063
2602.290062	698876.174471	39.350080
2605.350997	700262.311066	39.355098
2607.759916	701601.329918	39.360116
2610.445365	702960.921988	39.365133
2612.997262	704334.502098	39.370151
2615.879685	705685.111823	39.375168
2618.215819	707040.458198	39.380186
2621.144630	708390.837495	39.385204
2623.785798	709748.335358	39.390221
2626.646053	711081.906883	39.395239
2629.382120	712401.325778	39.400256
2631.534171	713740.097283	39.405274
2634.824932	715051.835169	39.410292
2637.468147	716337.687102	39.415309
2640.490103	717633.922475	39.420327
2643.249157	718935.396063	39.425344
2646.009426	720246.316382	39.430362
2648.562437	721516.549486	39.435380
2651.272938	722819.110373	39.440397
2653.213797	724130.694283	39.445415
2656.231632	725431.212978	39.450432
2658.702061	726748.476544	39.455450
2661.473276	728045.015565	39.460468
2664.174928	729352.383290	39.465485
2666.334572	730707.812493	39.470503
2669.040845	732027.007506	39.475520
2672.215287	733353.667562	39.480538
2675.141545	734672.594899	39.485556
2677.841495	736003.147377	39.490573
2680.286951	737347.643830	39.495591
2682.960414	738673.612194	39.500608
2686.014596	740020.769740	39.505626
2688.410392	741371.559412	39.510644
2691.143262	742723.742209	39.515661
2693.456569	744063.331859	39.520679
2696.219214	745421.019221	39.525696
2698.879491	746813.603440	39.530714
2701.364185	748176.237368	39.535732
2703.963663	749549.412196	39.540749
2706.188313	750937.983444	39.545767
2709.154755	752317.856342	39.550784
2711.033642	753725.354764	39.555802
2713.795727	755123.978328	39.560820
2716.586973	756539.336547	39.565837
2718.777307	757984.376294	39.570855
2721.556806	759402.163372	39.575872
2724.245633	760842.297643	39.580890
2726.830061	762292.807815	39.585908
2729.902902	763729.477093	39.590925
2732.298015	765184.188858	39.595943
2735.194946	766618.713765	39.600960
2737.530576	768103.565339	39.605978
2740.757337	769581.583500	39.610996
2743.643597	771033.752336	39.616013
2745.918208	772489.375638	39.621031
2748.987357	773965.860428	39.626048
2751.579012	775458.243952	39.631066
2754.531754	776952.377751	39.636084
2757.525796	778410.496511	39.641101
2760.175802	779906.926103	39.646119
2763.194028	781387.033130	39.651136
2766.040858	782880.217059	39.656154
2768.824028	784363.387476	39.661172
2771.707783	785850.652063	39.666189
2774.523561	787340.121978	39.671207
2777.350642	788806.574659	39.676224
2780.070796	790315.744071	39.681242
2782.663204	791781.378789	39.686260
2785.798081	793282.644132	39.691277
2788.020822	794783.888273	39.696295
2790.964397	796283.028474	39.701312
2793.680645	797805.788071	39.706330
2796.277792	799294.448305	39.711348
2799.485343	800768.296994	39.716365
2802.227743	802292.815508	39.721383
2804.883281	803798.955771	39.726400
2807.983567	805293.392806	39.731418
2810.629671	806777.210576	39.736436
2814.243339	808241.964562	39.741453
2816.658705	809705.135837	39.746471
2819.628549	811147.468604	39.751488
2822.323675	812586.657378	39.756506
2824.891387	814045.351502	39.761524
2827.445692	815503.195839	39.766541
2829.645541	816968.305042	39.771559
2832.514346	818455.691227	39.776576
2835.194724	819949.857177	39.781594
2837.967177	821439.817692	39.786612
2840.520031	822922.258705	39.791629
2843.202270	824433.717330	39.796647
2845.764196	825950.167012	39.801664
2848.778352	827475.897620	39.806682
2851.019876	828987.652776	39.811700
2854.024605	830517.016745	39.816717
2856.766112	832081.882962	39.821735
2859.634417	833641.577564	39.826752
2862.503960	835189.450737	39.831770
2865.575397	836733.316594	39.836788
2868.528337	838307.016088	39.841805
2871.243725	839876.962145	39.846823
2874.523248	841442.780785	39.851840
2877.385841	843012.662198	39.856858
2880.241958	844601.562887	39.861876
2882.919873	846174.194800	39.866893
2885.775189	847772.656263	39.871911
2888.812825	849357.365849	39.876928
2891.834262	850954.407750	39.881946
2894.386826	852561.708423	39.886964
2897.710415	854174.003809	39.891981
2900.363826	855773.077292	39.896999
2903.137687	857373.077187	39.902016
2905.924661	859001.386418	39.907034
2909.126633	860624.733415	39.912052
2912.016697	862266.616328	39.917069
2914.848659	863897.110221	39.922087
2917.279108	865532.953606	39.927104
2920.315898	867177.463589	39.932122
2923.106581	868825.539776	39.937140
2926.295001	870469.709853	39.942157
2928.609772	872128.099874	39.947175
2931.335800	873814.715950	39.952192
2934.657510	875471.528883	39.957210
2937.565272	877172.456618	39.962228
2940.662682	878834.173887	39.967245
2943.281894	880509.814586	39.972263
2946.265176	882197.389603	39.977280
2949.325221	883900.026834	39.982298
2952.109285	885588.397769	39.987316
2955.021567	887282.247295	39.992333
2958.063854	888991.224614	39.997351
2961.290139	890678.044023	40.002368
2964.558055	892369.671363	40.007386
2967.728598	894081.945526	40.012404
2970.633968	895757.680740	40.017421
2973.547700	897459.534798	40.022439
2976.487218	899169.069186	40.027456
2979.476075	900871.720739	40.032474
2982.628142	902568.149338	40.037492
2986.076883	904256.314352	40.042509
2989.439149	905969.402664	40.047527
2992.099176	907660.331422	40.052544
2995.146498	909340.870176	40.057562
2998.313176	911027.229895	40.062580
3001.664807	912723.046562	40.067597
3004.657654	914428.687548	40.072615
3007.307376	916080.907085	40.077632
3010.423232	917712.378074	40.082650
3013.049209	919354.488105	40.087668
3016.324102	921000.701537	40.092685
3019.639801	922634.795961	40.097703
3022.528466	924253.019522	40.102720
3025.728226	925874.544238	40.107738
3028.470778	927513.205146	40.112756
3031.661324	929132.214688	40.117773
3034.588968	930775.408163	40.122791
3037.139289	932415.570980	40.127808
3040.353317	934075.615303	40.132826
3043.141494	935748.614751	40.137844
3045.878112	937397.450854	40.142861
3048.648748	939062.797780	40.147879
3051.580342	940754.852371	40.152896
3054.618435	942445.290605	40.157914
3057.111823	944143.874449	40.162932
3060.086828	945828.063099	40.167949
3062.983966	947556.235435	40.172967
3065.709812	949301.525448	40.177984
3068.658520	951035.685938	40.183002
3071.235854	952777.338286	40.188020
3074.698578	954519.110534	40.193037
3077.347113	956313.740736	40.198055
3080.071175	958147.518603	40.203072
3083.410127	959970.931184	40.208090
3086.307919	961820.725111	40.213108
3089.590635	963660.382072	40.218125
3092.603784	965514.834862	40.223143
3095.625891	967376.013796	40.228160
3098.897694	969239.478296	40.233178
3101.496625	971102.449214	40.238196
3104.691277	972970.571857	40.243213
3108.166653	974847.013621	40.248231
3110.886986	976750.170519	40.253248
3114.765292	978653.868750	40.258266
3117.531984	980533.242515	40.263284
3120.384932	982413.445319	40.268301
3123.933623	984330.503379	40.273319
3126.976667	986256.345923	40.278336
3130.332070	988139.057103	40.283354
3133.674958	990042.842043	40.288372
3136.896310	991945.523805	40.293389
3140.107648	993876.541235	40.298407
3143.234653	995771.541001	40.303424
3146.736510	997670.606731	40.308442
3149.981423	999596.757754	40.313460
3153.325989	1001490.490233	40.318477
3156.456251	1003405.558622	40.323495
3159.143975	1005328.589251	40.328512
3162.975782	1007253.298646	40.333530
3165.961665	1009157.227545	40.338548
3169.014338	1011070.388821	40.343565
3172.369748	1012997.093405	40.348583
3175.392168	1014918.641256	40.353600
3178.685227	1016815.185557	40.358618
3181.790373	1018742.480835	40.363636
3184.687105	1020678.534333	40.368653
3187.959722	1022582.422657	40.373671
3191.131646	1024524.163688	40.378688
3194.587475	1026430.291479	40.383706
3197.527264	1028362.523107	40.388724
3201.183214	1030290.201839	40.393741
3204.303391	1032214.310128	40.398759
3207.406551	1034149.051013	40.403776
3210.539857	1036059.089330	40.408794
3213.476760	1037989.243328	40.413812
3216.464955	1039908.209197	40.418829
3220.014569	1041825.167160	40.423847
3222.585338	1043699.901810	40.428864
3225.605999	1045578.552719	40.433882
3228.643230	1047483.333747	40.438900
3231.631027	1049359.648963	40.443917
3235.098212	1051274.028565	40.448935
3237.725553	1053192.885778	40.453952
3241.127150	1055095.948116	40.458970
3244.145560	1057035.810632	40.463988
3247.203127	1058959.129091	40.469005
3250.386169	1060890.400815	40.474023
3253.389635	1062860.490779	40.479040
3256.325595	1064819.711184	40.484058
3259.335100	1066772.463512	40.489076
3262.442669	1068745.416013	40.494093
3265.558980	1070746.615170	40.499111
3268.515758	1072761.774973	40.504128
3271.584203	1074767.742716	40.509146
3275.088974	1076776.638240	40.514164
3278.197193	1078805.349938	40.519181
3281.490919	1080837.392563	40.524199
3284.509934	1082878.481918	40.529216
3287.801083	1084943.723199	40.534234
3290.635818	1087016.190822	40.539252
3293.691976	1089082.193677	40.544269
3296.986123	1091166.477153	40.549287
3300.448156	1093270.749438	40.554304
3303.812891	1095359.139066	40.559322
3306.973022	1097468.512113	40.564340
3310.341214	1099580.652822	40.569357
3313.562754	1101691.420104	40.574375
3316.662254	1103830.926781	40.579392
3320.291711	1105950.920318	40.584410
3323.648954	1108107.359157	40.589428
3326.883777	1110250.769648	40.594445
3330.460374	1112368.339112	40.599463
3333.472270	1114513.701429	40.604480
3337.025856	1116671.047255	40.609498
3340.660893	1118827.321189	40.614516
3343.538920	1120976.961302	40.619533
3346.976125	1123132.007891	40.624551
3350.781388	1125314.317065	40.629568
3354.135595	1127463.547142	40.634586
3357.708651	1129625.058555	40.639604
3361.003657	1131810.578308	40.644621
3364.686022	1133961.588067	40.649639
3367.745728	1136117.892576	40.654656
3371.295280	1138295.209363	40.659674
3374.608799	1140456.621168	40.664692
3378.045737	1142639.081541	40.669709
3381.944653	1144812.526835	40.674727
3385.271114	1146969.195988	40.679744
3388.651256	1149126.487530	40.684762
3391.972942	1151315.495144	40.689780
3395.273909	1153495.004628	40.694797
3399.133332	1155646.809756	40.699815
3401.743595	1157817.657716	40.704832
3405.137383	1159994.552370	40.709850
3408.290518	1162186.231444	40.714868
3411.802780	1164381.457781	40.719885
3415.220957	1166551.573533	40.724903
3418.471441	1168740.304808	40.729920
3421.949806	1170934.951450	40.734938
3425.508070	1173133.553530	40.739956
3428.820336	1175324.686958	40.744973
3432.658122	1177502.687444	40.749991
3435.323101	1179709.093177	40.755008
3438.626960	1181887.481839	40.760013
3441.871121	1184016.915997	40.765018
3444.846118	1186078.164122	40.770023
3448.501636	1188096.445849	40.775028
3452.024993	1190051.075889	40.780032
3455.352202	1191906.616525	40.785037
3458.173849	1193699.107678	40.790042
3461.141062	1195379.677326	40.795047
3464.395767	1197002.952014	40.800052
3466.779347	1198548.905358	40.805056
3469.559669	1200001.448497	40.810061
3472.255904	1201399.757705	40.815066
3474.623043	1202715.598744	40.820071
3477.226004	1203935.067003	40.825076
3479.784836	1205083.208345	40.830080
3482.494133	1206174.094433	40.835085
3484.517472	1207184.758383	40.840090
3486.369097	1208128.089502	40.845095
3488.320278	1208986.004738	40.850100
3490.126648	1209819.828192	40.855104
3491.690759	1210583.991877	40.860109
3493.678423	1211274.298308	40.865114
3494.835672	1211928.237389	40.870119
3496.483904	1212524.173251	40.875124
3497.776258	1213096.048148	40.880128
3499.093488	1213583.828637	40.885133
3500.689108	1214048.687420	40.890138
3501.566288	1214471.896833	40.895143
3502.884147	1214819.505426	40.900148
3503.750306	1215153.507534	40.905152
3504.644048	1215451.284538	40.910157
3505.571964	1215713.964075	40.915162
3506.829489	1215947.395171	40.920167
3507.617396	1216144.979712	40.925172
3508.612533	1216325.127591	40.930176
3509.571527	1216449.538212	40.935181
3510.490894	1216554.220317	40.940186
3511.038002	1216643.251054	40.945191
3511.798652	1216675.856109	40.950196
3512.463385	1216718.108679	40.955200
3513.265745	1216720.221000	40.960205
3514.083700	1216690.536002	40.965210
3514.194556	1216654.234212	40.970215
3514.835619	1216606.155383	40.975220
3515.093747	1216537.004352	40.980224
3515.702973	1216435.156556	40.985229
3516.374902	1216304.678958	40.990234
3516.580588	1216196.626934	40.995239
3517.293762	1216042.567921	41.000244
3517.727280	1215875.736837	41.005248
3517.978377	1215703.786070	41.010253
3518.258057	1215533.976121	41.015258
3518.601410	1215325.892624	41.020263
3519.277411	1215115.033116	41.025268
3519.260737	1214893.333974	41.030272
3519.317799	1214660.293348	41.035277
3519.890086	1214433.612577	41.040282
3520.012242	1214174.530544	41.045287
3520.568785	1213892.253201	41.050292
3520.513998	1213649.828337	41.055296
3520.754032	1213378.896717	41.060301
3520.907170	1213072.217406	41.065306
3521.058880	1212784.049953	41.070311
3521.507566	1212499.748171	41.075316
3521.460844	1212180.039082	41.080320
3521.717981	1211858.668710	41.085325
3521.939673	1211539.998633	41.090330
3521.972512	1211215.161250	41.095335
3521.896221	1210890.227590	41.100340
3522.085051	1210553.339059	41.105344
3522.331747	1210208.553660	41.110349
3522.753831	1209881.507580	41.115354
3522.604840	1209533.651803	41.120359
3523.059442	1209173.029993	41.125364
3523.161537	1208810.286702	41.130368
3523.086589	1208445.392578	41.135373
3523.432423	1208074.970188	41.140378
3523.247384	1207708.168242	41.145383
3523.528160	1207342.481230	41.150388
3523.464871	1206978.886019	41.155392
3523.658339	1206580.366715	41.160397
3523.956918	1206203.726418	41.165402
3523.669092	1205803.351868	41.170407
3523.856780	1205411.302611	41.175412
3524.132052	1205031.393572	41.180416
3523.997441	1204624.809504	41.185421
3523.895134	1204216.688021	41.190426
3523.719751	1203821.202344	41.195431
3524.290883	1203420.031595	41.200436
3524.122325	1203011.262656	41.205440
3524.172897	1202630.462823	41.210445
3524.414230	1202204.214415	41.215450
3524.072488	1201775.682003	41.220455
3523.923675	1201372.312826	41.225460
3524.377992	1200969.938286	41.230464
3524.253171	1200546.239132	41.235469
3524.181034	1200143.417578	41.240474
3524.244960	1199724.404287	41.245479
3524.310363	1199282.555381	41.250484
3524.557016	1198881.271486	41.255488
3524.489245	1198470.529522	41.260493
3524.502259	1198054.110189	41.265498
3524.477480	1197623.677872	41.270503
3524.333496	1197186.188913	41.275508
3524.319330	1196777.931480	41.280512
3524.154511	1196343.566247	41.285517
3524.581924	1195913.292090	41.290522
3524.231613	1195480.105253	41.295527
3524.532502	1195053.536255	41.300532
3524.176572	1194636.713624	41.305536
3524.308742	1194201.273707	41.310541
3524.197997	1193773.915276	41.315546
3523.993227	1193359.876484	41.320551
3524.475590	1192928.404861	41.325556
3524.569569	1192491.981472	41.330560
3524.379727	1192070.038395	41.335565
3524.712132	1191617.621933	41.340570
3524.414552	1191181.058277	41.345575
3524.253935	1190746.878854	41.350580
3524.433956	1190311.196912	41.355584
3524.128623	1189896.520982	41.360589
3524.506402	1189453.495926	41.365594
3524.029544	1189018.189246	41.370599
3524.037557	1188578.628863	41.375604
3524.056738	1188128.685394	41.380608
3524.020866	1187703.633389	41.385613
3524.104016	1187272.507608	41.390618
3523.854402	1186837.826487	41.395623
3523.963681	1186420.075838	41.400628
3524.034998	1185983.012508	41.405632
3524.074391	1185508.660779	41.410637
3523.880796	1185094.710534	41.415642
3523.380518	1184665.157409	41.420647
3524.002679	1184237.642370	41.425652
3524.091838	1183801.991953	41.430656
3523.729571	1183370.614773	41.435661
3523.918750	1182948.523856	41.440666
3523.750466	1182494.921400	41.445671
3523.572421	1182050.224761	41.450676
3523.912156	1181620.375198	41.455680
3523.642894	1181195.863388	41.460685
3523.849007	1180736.019221	41.465690
3523.548285	1180294.770857	41.470695
3523.728764	1179870.170786	41.475700
3523.460091	1179457.195732	41.480704
3523.658585	1179010.858074	41.485709
3523.642201	1178569.698981	41.490714
3523.194108	1178130.740542	41.495719
3523.598671	1177700.744421	41.500724
3523.695326	1177263.224866	41.505728
3523.451670	1176834.583171	41.510733
3523.560554	1176396.517525	41.515738
3523.582674	1175969.928552	41.520743
3523.512544	1175533.704902	41.525748
3523.409203	1175082.743743	41.530752
3523.281923	1174633.727363	41.535757
3523.668998	1174215.514062	41.540762
3523.311528	1173793.900892	41.545767
3523.281050	1173346.643557	41.550772
3523.219331	1172905.200307	41.555776
3523.138328	1172470.419536	41.560781
3523.206169	1172033.408475	41.565786
3522.964025	1171616.222205	41.570791
3523.117487	1171170.445941	41.575796
3523.198450	1170727.285367	41.580800
3523.110389	1170305.817509	41.585805
3523.258851	1169885.597796	41.590810
3523.205802	1169440.179615	41.595815
3523.117422	1168985.196652	41.600820
3523.180916	1168558.371762	41.605824
3522.982809	1168134.953410	41.610829
3523.215020	1167683.957838	41.615834
3522.962938	1167244.899274	41.620839
3523.028030	1166797.348057	41.625844
3523.071528	1166381.207183	41.630848
3523.241602	1165959.629450	41.635853
3523.164418	1165502.074946	41.640858
3522.941722	1165057.727876	41.645863
3522.744648	1164620.328988	41.650868
3522.780456	1164205.055385	41.655872
3522.821912	1163762.916617	41.660877
3523.000125	1163322.796665	41.665882
3522.563757	1162892.284694	41.670887
3522.532225	1162454.488652	41.675892
3522.745486	1162020.112523	41.680896
3522.564045	1161600.226323	41.685901
3522.615523	1161164.482732	41.690906
3522.543627	1160716.906821	41.695911
3522.303313	1160285.864865	41.700916
3522.149361	1159875.006307	41.705920
3522.110755	1159440.741655	41.710925
3522.313922	1159009.238125	41.715930
3522.041288	1158584.019117	41.720935
3522.400473	1158168.497678	41.725940
3522.269699	1157737.890452	41.730944
3522.037794	1157294.116138	41.735949
3522.215680	1156873.130290	41.740954
3522.363697	1156458.170575	41.745959
3522.165925	1156014.661025	41.750964
3522.284931	1155601.814670	41.755968
3522.073018	1155155.869416	41.760973
3522.417005	1154728.722704	41.765978
3522.105213	1154320.673348	41.770983
3522.066884	1153879.134313	41.775988
3521.806281	1153432.104408	41.780992
3521.931937	1153014.415439	41.785997
3522.263177	1152605.275147	41.791002
3521.708030	1152184.129373	41.796007
3521.887636	1151749.098446	41.801012
3521.778090	1151334.723952	41.806016
3521.811554	1150907.981285	41.811021
3522.103902	1150468.848371	41.816026
3521.715685	1150052.714091	41.821031
3522.188553	1149617.932587	41.826036
3522.111044	1149201.111547	41.831040
3522.052042	1148762.462848	41.836045
3521.807746	1148349.581352	41.841050
3521.880004	1147902.311665	41.846055
3521.729410	1147462.527613	41.851060
3521.809395	1147053.566435	41.856064
3521.441156	1146633.652379	41.861069
3521.883291	1146192.148352	41.866074
3521.706144	1145763.507504	41.871079
3521.623322	1145346.572540	41.876084
3521.598438	1144914.424658	41.881088
3521.475923	1144494.869025	41.886093
3521.374731	1144078.311168	41.891098
3521.435663	1143662.262825	41.896103
3521.415940	1143216.413450	41.901108
3521.237872	1142806.502162	41.906112
3521.158325	1142407.167290	41.911117
3521.762968	1141978.659990	41.916122
3521.246838	1141539.961114	41.921127
3521.112749	1141124.219723	41.926132
3521.758291	1140720.368443	41.931136
3521.312518	1140280.984331	41.936141
3521.350465	1139844.521113	41.941146
3521.099122	1139440.055627	41.946151
3521.222383	1139026.005467	41.951156
3521.183173	1138602.172079	41.956160
3521.122242	1138176.599537	41.961165
3521.209353	1137745.081933	41.966170
3520.840731	1137349.970710	41.971175
3520.963446	1136939.365878	41.976180
3520.954168	1136511.372238	41.981184
3520.735951	1136086.797556	41.986189
3521.053086	1135680.717063	41.991194
3521.045486	1135260.315753	41.996199
3520.841233	1134841.718481	42.001204
3520.747187	1134434.945497	42.006208
3520.810995	1134015.858994	42.011213
3520.881723	1133586.286282	42.016218
3520.683408	1133173.732823	42.021223
3520.951318	1132777.511286	42.026228
3520.783806	1132354.245472	42.031232
3520.478031	1131926.691578	42.036237
3520.585372	1131515.194735	42.041242
3520.464160	1131126.708871	42.046247
3520.349583	1130694.176255	42.051252
3520.324389	1130285.077955	42.056256
3520.240509	1129880.236698	42.061261
3520.544257	1129464.365242	42.066266
3520.223434	1129066.157570	42.071271
3520.079914	1128661.138373	42.076276
3520.262010	1128252.420438	42.081280
3519.758742	1127846.923033	42.086285
3520.038513	1127439.268115	42.091290
3519.861150	1127041.075731	42.096295
3520.020147	1126627.480256	42.101300
3520.070798	1126233.566593	42.106304
3519.793043	1125850.525795	42.111309
3519.723189	1125428.691600	42.116314
3519.680132	1125040.129616	42.121319
3519.683321	1124627.261294	42.126324
3519.363229	1124249.537716	42.131328
3519.592238	1123853.420110	42.136333
3519.938831	1123432.121105	42.141338
3519.433246	1123034.730980	42.146343
3519.363266	1122646.760924	42.151348
3519.676267	1122263.936757	42.156352
3519.554833	1121855.540515	42.161357
3519.473229	1121448.249333	42.166362
3519.432335	1121086.160321	42.171367
3519.336661	1120671.097701	42.176372
3519.132881	1120275.357664	42.181376
3519.235619	1119881.633656	42.186381
3519.097311	1119495.541970	42.191386
3519.212213	1119098.423900	42.196391
3519.124888	1118710.266362	42.201396
3519.055275	1118328.938691	42.206400
3518.999925	1117930.904456	42.211405
3519.394576	1117545.632652	42.216410
3519.249902	1117169.190611	42.221415
3519.180423	1116764.781523	42.226420
3519.251259	1116376.905433	42.231424
3519.231911	1115976.622934	42.236429
3519.324261	1115584.586686	42.241434
3519.051309	1115205.739722	42.246439
3518.867296	1114795.098754	42.251444
3519.296491	1114396.054710	42.256448
3519.229402	1114023.002656	42.261453
3519.204775	1113636.279211	42.266458
3518.855933	1113244.621491	42.271463
3518.811848	1112827.893307	42.276468
3519.151305	1112452.375819	42.281472
3518.512218	1112056.291036	42.286477
3518.849841	1111679.956639	42.291482
3518.605760	1111308.367046	42.296487
3518.330267	1110912.138008	42.301492
3518.474277	1110517.337533	42.306496
3518.461808	1110160.899133	42.311501
3518.462387	1109785.346512	42.316506
3518.504774	1109388.284700	42.321511
3518.475049	1109002.755674	42.326516
3518.751598	1108622.208120	42.331520
3518.095322	1108247.610943	42.336525
3518.020548	1107875.756194	42.341530
3517.855303	1107497.493300	42.346535
3517.809082	1107122.908317	42.351540
3517.753398	1106768.544002	42.356544
3518.028003	1106386.692776	42.361549
3517.657647	1106009.027613	42.366554
3517.654914	1105655.822993	42.371559
3517.852249	1105283.839948	42.376564
3517.973064	1104920.919065	42.381568
3517.663078	1104544.287631	42.386573
3517.680891	1104175.314788	42.391578
3517.617177	1103814.165089	42.396583
3517.735059	1103437.385864	42.401588
3517.830617	1103078.740676	42.406592
3517.502791	1102699.403161	42.411597
3518.033185	1102326.779002	42.416602
3517.641770	1101952.273741	42.421607
3517.520804	1101606.947754	42.426612
3517.539314	1101235.288441	42.431616
3517.390861	1100867.550665	42.436621
3517.315597	1100499.393365	42.441626
3517.284316	1100154.150912	42.446631
3517.533277	1099771.931116	42.451636
3517.511551	1099428.553127	42.456640
3517.299352	1099072.752519	42.461645
3517.713530	1098690.237761	42.466650
3517.696299	1098322.400777	42.471655
3517.303409	1097961.583229	42.476660
3517.617378	1097604.738488	42.481664
3517.548941	1097237.027433	42.486669
3517.422048	1096854.280620	42.491674
3517.048753	1096488.290971	42.496679
3517.045991	1096137.429333	42.501684
3517.225902	1095767.663846	42.506688
3516.799653	1095414.911314	42.511693
3517.214658	1095079.510883	42.516698
3516.772822	1094714.752441	42.521703
3516.640507	1094341.208317	42.526708
3516.993128	1093995.413726	42.531712
3516.756338	1093661.851600	42.536717
3516.795298	1093282.749810	42.541722
3517.067425	1092948.772779	42.546727
3516.750826	1092588.733330	42.551732
3516.616938	1092221.171126	42.556736
3516.538267	1091877.802082	42.561741
3517.095254	1091543.308550	42.566746
3516.661465	1091199.380460	42.571751
3516.689437	1090820.587207	42.576756
3516.661805	1090473.098177	42.581760
3516.598648	1090133.351757	42.586765
3516.739411	1089761.458693	42.591770
3516.499225	1089429.456908	42.596775
3516.299819	1089064.757341	42.601780
3516.547869	1088731.961841	42.606784
3516.139522	1088399.828991	42.611789
3516.509002	1088035.349902	42.616794
3516.206952	1087704.594450	42.621799
3516.334595	1087360.426486	42.626804
3516.101661	1087011.887245	42.631808
3515.913555	1086672.232438	42.636813
3516.349931	1086339.738700	42.641818
3515.993903	1085992.400521	42.646823
3516.051648	1085641.712453	42.651828
3516.138565	1085296.174252	42.656832
3515.844872	1084968.127201	42.661837
3516.276837	1084636.105376	42.666842
3516.109541	1084296.298782	42.671847
3515.699331	1083941.838413	42.676852
3515.916575	1083600.486566	42.681856
3515.716923	1083284.214779	42.686861
3515.780699	1082951.191754	42.691866
3515.706045	1082618.746707	42.696871
3515.648068	1082269.203342	42.701876
3515.934481	1081941.358007	42.706880
3515.415562	1081625.138412	42.711885
3515.430614	1081271.489545	42.716890
3515.488465	1080955.615844	42.721895
3515.217982	1080614.637027	42.726900
3515.643379	1080292.235192	42.731904
3515.322512	1079954.390187	42.736909
3515.406500	1079622.120121	42.741914
3515.266006	1079311.654470	42.746919
3515.341259	1078986.737668	42.751924
3515.394015	1078650.478141	42.756928
3514.847768	1078329.272270	42.761933
3515.080090	1078003.311084	42.766938
3514.938225	1077674.991834	42.771943
3515.023300	1077365.914511	42.776948
3515.141809	1077055.853990	42.781952
3514.925599	1076730.370813	42.786957
3514.908682	1076392.159201	42.791962
3514.841720	1076078.136427	42.796967
3514.719414	1075776.398230	42.801972
3515.164319	1075448.616881	42.806977
3514.659317	1075125.390837	42.811981
3514.879780	1074814.129744	42.816986
3514.983351	1074510.363277	42.821991
3514.577041	1074168.331665	42.826996
3514.802154	1073839.241143	42.832001
3514.656481	1073532.386959	42.837005
3514.661591	1073221.262871	42.842010
3514.358191	1072919.396851	42.847015
3514.563242	1072594.558976	42.852020
3514.849199	1072279.491155	42.857025
3514.547903	1071979.014494	42.862029
3514.835394	1071672.080786	42.867034
3514.670655	1071357.514729	42.872039
3514.771475	1071033.082008	42.877044
3514.811715	1070728.539315	42.882049
3514.544309	1070405.475920	42.887053
3515.096974	1070083.700554	42.892058
3514.802857	1069764.834077	42.897063
3514.544165	1069460.270142	42.902068
3514.506848	1069145.459951	42.907073
3514.672298	1068837.810646	42.912077
3514.475814	1068508.276875	42.917082
3514.301544	1068194.107822	42.922087
3514.211492	1067902.990409	42.927092
3514.535772	1067583.125755	42.932097
3514.270045	1067278.441804	42.937101
3514.416622	1066968.670763	42.942106
3514.485756	1066659.568419	42.947111
3514.264075	1066346.648238	42.952116
3514.057733	1066036.305467	42.957121
3513.849322	1065726.811468	42.962125
3514.097919	1065423.575579	42.967130
3514.041130	1065124.222445	42.972135
3514.007235	1064817.631598	42.977140
3514.391299	1064508.163833	42.982145
3513.794399	1064217.030669	42.987149
3513.879064	1063883.419331	42.992154
3513.560397	1063598.175143	42.997159
3513.655330	1063324.495658	43.002164
3513.631035	1063015.781232	43.007169
3513.297429	1062741.084359	43.012173
3513.589271	1062430.167023	43.017178
3513.424298	1062138.852642	43.022183
3513.630485	1061853.142642	43.027188
3513.852137	1061535.831391	43.032193
3513.596898	1061258.736564	43.037197
3513.208949	1060969.322936	43.042202
3513.469605	1060658.599560	43.047207
3513.811393	1060374.620339	43.052212
3513.729050	1060080.005040	43.057217
3513.300487	1059792.655236	43.062221
3513.485376	1059488.235630	43.067226
3513.416958	1059202.914965	43.072231
3513.102661	1058916.945651	43.077236
3513.550659	1058599.813288	43.082241
3513.549584	1058322.914225	43.087245
3513.504382	1058041.961667	43.092250
3513.408499	1057745.971178	43.097255
3513.275611	1057451.801808	43.102260
3513.335690	1057148.911734	43.107265
3513.214714	1056889.306855	43.112269
3513.178746	1056581.293613	43.117274
3512.905561	1056290.555054	43.122279
3513.263542	1056008.179473	43.127284
3513.505194	1055724.941061	43.132289
3513.197461	1055441.778599	43.137293
3513.171945	1055143.419669	43.142298
3513.253620	1054850.618708	43.147303
3513.188057	1054570.456759	43.152308
3513.318979	1054297.479669	43.157313
3513.127988	1054009.982088	43.162317
3513.279088	1053702.838051	43.167322
3513.196757	1053426.188704	43.172327
3512.986701	1053149.932295	43.177332
3513.118691	1052851.809365	43.182337
3512.981777	1052559.501611	43.187341
3513.019291	1052275.444749	43.192346
3512.783006	1052001.353687	43.197351
3512.790884	1051713.510923	43.202356
3513.027288	1051440.182366	43.207361
3513.022579	1051165.529382	43.212365
3512.772759	1050854.434128	43.217370
3512.973371	1050591.875203	43.222375
3512.444730	1050318.617227	43.227380
3512.446022	1050038.793414	43.232385
3512.438505	1049759.246396	43.237389
3512.264454	1049475.177037	43.242394
3512.596058	1049218.707589	43.247399
3512.543239	1048960.745384	43.252404
3512.445274	1048683.282191	43.257409
3512.526151	1048407.706076	43.262413
3512.385930	1048138.716469	43.267418
3512.619048	1047857.296302	43.272423
3512.144266	1047591.327684	43.277428
3512.225778	1047319.365684	43.282433
3512.052695	1047037.101889	43.287437
3512.139755	1046757.387733	43.292442
3512.186875	1046509.432690	43.297447
3512.024328	1046255.321296	43.302452
3512.237817	1045965.407617	43.307457
3512.136765	1045705.370456	43.312461
3512.107480	1045442.798369	43.317466
3512.204414	1045159.235588	43.322471
3512.043184	1044903.130432	43.327476
3512.070007	1044647.368826	43.332481
3511.641507	1044358.346161	43.337485
3512.058052	1044083.948634	43.342490
3511.630978	1043837.207963	43.347495
3511.378309	1043600.377972	43.352500
3512.275607	1043329.534986	43.357505
3511.584312	1043062.901654	43.362509
3511.719785	1042797.085533	43.367514
3511.599518	1042542.313950	43.372519
3511.500265	1042303.084365	43.377524
3511.530062	1042022.561084	43.382529
3511.335556	1041778.976125	43.387533
3511.705289	1041529.102494	43.392538
3511.461225	1041296.231735	43.397543
3511.167244	1041025.279330	43.402548
3511.773545	1040752.232331	43.407553
3511.470392	1040522.625153	43.412557
3511.481810	1040263.087706	43.417562
3511.803937	1040021.950547	43.422567
3511.192733	1039773.512907	43.427572
3511.462124	1039498.236366	43.432577
3511.512043	1039251.600053	43.437581
3511.116608	1039018.368732	43.442586
3511.290991	1038759.604437	43.447591
3511.291013	1038504.917981	43.452596
3511.626974	1038249.681045	43.457601
3511.143699	1038021.450712	43.462605
3511.295909	1037747.267266	43.467610
3511.391444	1037487.393020	43.472615
3511.344731	1037252.869698	43.477620
3511.297895	1036991.738457	43.482625
3511.552457	1036758.208605	43.487629
3511.087205	1036499.734762	43.492634
3510.885743	1036260.165202	43.497639
3510.922569	1036026.834009	43.502644
3511.364639	1035769.627899	43.507649
3511.143176	1035524.418967	43.512653
3511.180638	1035275.093086	43.517658
3511.390713	1035027.275694	43.522663
3511.066559	1034784.082938	43.527668
3511.226960	1034534.413397	43.532673
3510.991926	1034276.766100	43.537677
3511.073438	1034041.409059	43.542682
3511.126364	1033799.369261	43.547687
3510.775316	1033544.320168	43.552692
3510.768471	1033297.429410	43.557697
3510.841857	1033072.098386	43.562701
3510.748170	1032830.331044	43.567706
3510.704480	1032580.123654	43.572711
3510.739811	1032346.445038	43.577716
3510.993860	1032108.461185	43.582721
3510.659659	1031883.439701	43.587725
3510.583086	1031628.160964	43.592730
3510.308165	1031402.529440	43.597735
3510.382128	1031191.354519	43.602740
3510.438181	1030931.181006	43.607745
3510.515522	1030693.650072	43.612749
3510.541463	1030468.318556	43.617754
3510.730729	1030246.146689	43.622759
3510.616495	1029989.443501	43.627764
3510.166847	1029757.673230	43.632769
3510.297642	1029535.870128	43.637773
3510.434125	1029304.468766	43.642778
3510.375343	1029071.249684	43.647783
3510.515559	1028846.608798	43.652788
3510.325108	1028606.708551	43.657793
3510.356012	1028377.126637	43.662797
3510.230017	1028153.276693	43.667802
3510.463297	1027941.855816	43.672807
3510.252162	1027695.719719	43.677812
3510.305076	1027464.159059	43.682817
3510.344399	1027250.903180	43.687821
3510.259263	1027024.288404	43.692826
3510.203983	1026786.419437	43.697831
3510.197169	1026545.043914	43.702836
3509.882705	1026333.264846	43.707841
3509.948559	1026099.416740	43.712845
3510.283203	1025863.479410	43.717850
3510.566107	1025652.351493	43.722855
3510.301848	1025416.784732	43.727860
3510.518956	1025173.665523	43.732865
3509.926877	1024954.804451	43.737869
3509.906526	1024745.049276	43.742874
3510.122246	1024504.033744	43.747879
3509.984272	1024279.061364	43.752884
3510.071298	1024059.859571	43.757889
3509.711331	1023836.650985	43.762893
3509.859687	1023614.707113	43.767898
3509.805195	1023382.510494	43.772903
3509.548763	1023184.758348	43.777908
3509.924062	1022952.570087	43.782913
3509.727599	1022730.938899	43.787917
3509.624526	1022520.726188	43.792922
3509.926281	1022310.438917	43.797927
3509.527650	1022090.270316	43.802932
3509.589834	1021851.202523	43.807937
3509.597706	1021659.462942	43.812941
3509.833922	1021443.916718	43.817946
3509.744529	1021223.760146	43.822951
3509.100014	1021003.007378	43.827956
3509.853370	1020799.863905	43.832961
3509.609295	1020577.185404	43.837965
3509.326449	1020363.914289	43.842970
3509.569535	1020154.622957	43.847975
3509.600926	1019942.933293	43.852980
3509.857911	1019724.019041	43.857985
3509.550520	1019513.630240	43.862989
3509.842819	1019313.419624	43.867994
3509.749086	1019090.366278	43.872999
3509.646120	1018891.758220	43.878004
3509.926293	1018659.602007	43.883009
3509.830568	1018439.240189	43.888013
3509.641595	1018216.070757	43.893018
3509.894582	1018012.035445	43.898023
3509.323276	1017801.917108	43.903028
3509.516622	1017572.253634	43.908033
3509.253326	1017361.388687	43.913037
3509.095279	1017153.119221	43.918042
3509.309580	1016936.141678	43.923047
3509.287038	1016742.783111	43.928052
3509.269622	1016530.875789	43.933057
3509.021319	1016326.376465	43.938061
3509.109521	1016096.572933	43.943066
3509.232055	1015895.783077	43.948071
3508.905163	1015719.526512	43.953076
3509.100706	1015514.633291	43.958081
3508.978941	1015296.482717	43.963085
3509.447334	1015090.849451	43.968090
3509.075502	1014895.445788	43.973095
3509.246210	1014692.565882	43.978100
3509.193987	1014465.437816	43.983105
3509.264176	1014272.076125	43.988109
3508.851707	1014068.978447	43.993114
3509.495537	1013867.738996	43.998119
3508.865130	1013665.828109	44.003124
3508.744360	1013464.797312	44.008129
3508.854471	1013271.394667	44.013133
3508.953768	1013064.971136	44.018138
3508.883741	1012853.711015	44.023143
3508.504091	1012650.556737	44.028148
3508.721570	1012459.148489	44.033153
3508.824283	1012272.707207	44.038157
3508.536784	1012066.505080	44.043162
3508.661616	1011869.748713	44.048167
3508.860622	1011684.437966	44.053172
3508.580599	1011481.613740	44.058177
3508.394616	1011286.928613	44.063181
3508.235261	1011105.155788	44.068186
3508.269003	1010917.029140	44.073191
3508.343914	1010720.435209	44.078196
3508.653082	1010511.648519	44.083201
3508.336059	1010342.996185	44.088205
3508.063240	1010157.032659	44.093210
3508.253634	1009952.423768	44.098215
3508.051542	1009758.951957	44.103220
3508.290804	1009579.299677	44.108225
3508.107398	1009409.139473	44.113229
3507.762777	1009214.020078	44.118234
3507.992120	1009017.049717	44.123239
3507.614664	1008869.067741	44.128244
3508.007884	1008696.944144	44.133249
3507.690846	1008510.350328	44.138253
3507.556796	1008310.498759	44.143258
3507.955365	1008140.398859	44.148263
3507.522144	1007994.250285	44.153268
3507.835306	1007810.446186	44.158273
3508.046298	1007611.874201	44.163277
3507.755337	1007429.226708	44.168282
3507.949508	1007269.538029	44.173287
3507.791255	1007115.834351	44.178292
3507.810469	1006916.394359	44.183297
3507.845442	1006735.226578	44.188301
3507.775984	1006556.112368	44.193306
3507.991700	1006397.756947	44.198311
3507.461470	1006215.304083	44.203316
3507.797405	1006019.864877	44.208321
3507.574215	1005852.813419	44.213325
3507.782621	1005696.384722	44.218330
3507.716292	1005517.431582	44.223335
3507.508546	1005344.623932	44.228340
3507.476417	1005163.514061	44.233345
3507.595696	1005009.804621	44.238349
3507.647487	1004849.876445	44.243354
3507.735169	1004660.073122	44.248359
3507.512888	1004479.556330	44.253364
3507.402351	1004313.024484	44.258369
3507.643499	1004164.817263	44.263373
3507.737094	1003985.983867	44.268378
3507.815196	1003795.666649	44.273383
3507.184196	1003624.432818	44.278388
3507.187202	1003467.197886	44.283393
3507.333338	1003304.486056	44.288397
3507.259812	1003138.400031	44.293402
3507.350876	1002984.640184	44.298407
3507.223649	1002825.754631	44.303412
3507.128653	1002646.131442	44.308417
3507.256717	1002484.664095	44.313421
3507.250016	1002304.236976	44.318426
3507.493524	1002146.244479	44.323431
3507.651776	1001981.838135	44.328436
3507.553687	1001810.169607	44.333441
3507.534022	1001658.533192	44.338445
3507.286191	1001483.083492	44.343450
3507.501708	1001298.889028	44.348455
3507.065687	1001139.033598	44.353460
3507.146627	1000989.504171	44.358465
3507.178265	1000819.925780	44.363469
3507.171484	1000666.411104	44.368474
3507.450346	1000517.907457	44.373479
3507.034272	1000344.494541	44.378484
3507.250637	1000166.201669	44.383489
3506.818672	1000025.688084	44.388493
3506.776204	999855.022057	44.393498
3507.000482	999688.591013	44.398503
3506.862716	999541.104033	44.403508
3507.370259	999373.156560	44.408513
3507.073080	999229.679914	44.413517
3507.003219	999064.252710	44.418522
3506.852461	998916.848996	44.423527
3506.843187	998752.084348	44.428532
3507.233502	998591.533985	44.433537
3506.757356	998430.732242	44.438541
3506.868657	998284.534945	44.443546
3506.867773	998122.087942	44.448551
3506.624741	997972.045272	44.453556
3506.813610	997822.998862	44.458561
3506.651173	997667.480624	44.463565
3506.599008	997528.498330	44.468570
3506.747773	997353.634591	44.473575
3506.304635	997215.683075	44.478580
3506.577661	997076.343918	44.483585
3506.583395	996912.692262	44.488589
3506.345399	996759.596885	44.493594
3506.736815	996617.304500	44.498599
3506.703200	996496.608363	44.503604
3506.723257	996331.184020	44.508609
3506.721204	996168.876109	44.513613
3506.283005	996020.177892	44.518618
3506.468124	995879.752129	44.523623
3506.746751	995739.112627	44.528628
3506.417976	995577.523646	44.533633
3506.490980	995425.315396	44.538637
3506.564805	995283.626523	44.543642
3506.455524	995142.646375	44.548647
3506.049969	994998.398378	44.553652
3506.146675	994860.592997	44.558657
3506.098087	994719.787247	44.563661
3506.087603	994578.094655	44.568666
3506.291796	994417.261932	44.573671
3506.347831	994294.360178	44.578676
3506.220245	994149.752460	44.583681
3506.368695	994005.095595	44.588685
3506.484111	993866.385852	44.593690
3506.390444	993713.184515	44.598695
3506.398963	993585.499341	44.603700
3506.384270	993419.800948	44.608705
3506.369156	993285.777211	44.613709
3506.140011	993145.741978	44.618714
3506.393453	992993.926235	44.623719
3506.301343	992849.474535	44.628724
3506.093842	992735.453352	44.633729
3506.493408	992593.546242	44.638733
3506.109774	992432.754170	44.643738
3506.279546	992296.629376	44.648743
3505.919413	992175.700177	44.653748
3505.901038	992034.530411	44.658753
3506.236304	991878.966560	44.663757
3506.065380	991743.177129	44.668762
3506.084986	991619.931030	44.673767
3505.708741	991494.992358	44.678772
3505.713513	991352.729292	44.683777
3505.858524	991197.275643	44.688781
3505.619146	991075.035498	44.693786
3505.726083	990953.418288	44.698791
3505.292757	990825.451341	44.703796
3505.554096	990688.785398	44.708801
3505.692185	990569.300273	44.713805
3505.998460	990429.890113	44.718810
3506.013167	990299.692020	44.723815
3505.836305	990186.297341	44.728820
3505.566443	990055.360302	44.733825
3506.035444	989912.789708	44.738829
3505.942057	989783.670472	44.743834
3505.952193	989663.992349	44.748839
3505.912183	989527.835853	44.753844
3506.113601	989387.539585	44.758849
3506.047771	989261.427756	44.763853
3506.031115	989123.209315	44.768858
3505.885154	988976.717179	44.773863
3505.633295	988859.016258	44.778868
3505.751955	988717.351400	44.783873
3505.724673	988598.827685	44.788877
3505.762994	988480.876042	44.793882
3505.694666	988344.500795	44.798887
3505.386929	988215.088605	44.803892
3505.494567	988076.726727	44.808897
3505.542689	987952.420854	44.813901
3505.591782	987835.137029	44.818906
3505.567364	987696.592534	44.823911
3505.246210	987584.243055	44.828916
3505.730421	987467.953305	44.833921
3505.492999	987338.509613	44.838925
3505.083292	987221.483876	44.843930
3505.507425	987074.361011	44.848935
3505.390038	986959.721282	44.853940
3505.505252	986846.797470	44.858945
3505.654152	986710.932849	44.863949
3505.089030	986613.437690	44.868954
3505.153147	986479.923666	44.873959
3505.338143	986348.826450	44.878964
3505.301782	986225.765545	44.883969
3505.371989	986116.348126	44.888973
3505.349875	985989.668662	44.893978
3505.582017	985865.872566	44.898983
3505.443673	985770.244722	44.903988
3505.439059	985629.792251	44.908993
3505.233800	985501.277586	44.913997
3505.385793	985377.386481	44.919002
3505.563383	985268.618385	44.924007
3505.219844	985159.153135	44.929012
3505.256356	985015.847961	44.934017
3505.356848	984903.669025	44.939021
3505.108944	984782.271323	44.944026
3505.700542	984659.756539	44.949031
3505.368263	984556.428087	44.954036
3505.454579	984422.276488	44.959041
3505.658853	984304.113442	44.964045
3505.383342	984177.825984	44.969050
3505.700691	984071.940985	44.974055
3505.177883	983945.298580	44.979060
3505.400416	983813.844020	44.984065
3505.189209	983709.699189	44.989069
3505.243294	983573.091966	44.994074
3505.249123	983455.041669	44.999079
3504.928437	983341.339100	45.004084
3504.877494	983233.839250	45.009089
3504.928052	983115.969868	45.014093
3504.809326	982995.196402	45.019098
3505.042560	982869.089137	45.024103
3504.673017	982764.074247	45.029108
3505.100800	982644.082238	45.034113
3504.821240	982544.517284	45.039117
3505.080457	982442.420340	45.044122
3505.225723	982309.771955	45.049127
3505.148036	982194.443909	45.054132
3504.669957	982093.145814	45.059137
3504.801561	981990.671149	45.064141
3504.873627	981878.437441	45.069146
3504.758242	981758.809316	45.074151
3505.004688	981650.253950	45.079156
3505.040822	981542.805597	45.084161
3505.080901	981434.280118	45.089165
3504.816751	981324.435172	45.094170
3505.050161	981208.840627	45.099175
3504.816647	981094.395171	45.104180
3504.691752	980979.050362	45.109185
3504.808007	980882.517172	45.114189
3504.622324	980776.947010	45.119194
3504.932589	980668.069412	45.124199
3504.764091	980550.183164	45.129204
3504.625282	980449.386181	45.134209
3504.617191	980346.221176	45.139213
3504.502552	980242.778765	45.144218
3504.745121	980128.333243	45.149223
3504.267249	980039.797384	45.154228
3504.628016	979947.507004	45.159233
3504.898005	979837.252379	45.164237
3504.487650	979715.675959	45.169242
3504.978796	979623.163461	45.174247
3504.735644	979530.184149	45.179252
3504.676514	979401.117199	45.184257
3504.510716	979297.763827	45.189261
3504.542506	979192.324004	45.194266
3504.926694	979108.322097	45.199271
3504.781033	979001.246782	45.204276
3504.691021	978889.567397	45.209281
3504.811361	978797.298068	45.214285
3504.648527	978683.574475	45.219290
3504.507413	978560.463267	45.224295
3504.724999	978462.308902	45.229300
3504.665471	978365.859910	45.234305
3504.680701	978266.562755	45.239309
3504.469087	978147.363545	45.244314
3504.459461	978038.684060	45.249319
3504.312902	977951.918263	45.254324
3504.665648	977836.822333	45.259329
3504.907217	977748.718918	45.264333
3504.270106	977662.322748	45.269338
3504.549961	977554.759302	45.274343
3504.570392	977451.830622	45.279348
3504.638557	977344.200342	45.284353
3504.582784	977242.062423	45.289357
3504.331156	977143.962736	45.294362
3504.543514	977031.513023	45.299367
3504.464000	976939.539921	45.304372
3504.640597	976846.643353	45.309377
3504.261690	976726.757811	45.314381
3504.549369	976649.481043	45.319386
3504.592873	976553.082291	45.324391
3504.518248	976441.939166	45.329396
3504.284645	976323.389925	45.334401
3504.386394	976252.102091	45.339405
3504.416309	976150.810487	45.344410
3504.533939	976031.610748	45.349415
3504.503725	975923.090031	45.354420
3504.291504	975834.543054	45.359425
3504.363056	975756.409880	45.364429
3504.188962	975668.245151	45.369434
3504.503732	975547.634004	45.374439
3504.218208	975465.937881	45.379444
3503.938601	975373.972590	45.384449
3504.387882	975277.583320	45.389453
3504.375683	975182.930777	45.394458
3504.245571	975085.949223	45.399463
3504.400729	974976.206603	45.404468
3504.404976	974888.978387	45.409473
3504.341712	974804.400322	45.414477
3504.332551	974719.518719	45.419482
3504.154935	974603.369464	45.424487
3504.270721	974507.217764	45.429492
3504.048628	974425.789745	45.434497
3504.528444	974323.315961	45.439501
3503.985130	974233.331775	45.444506
3504.150671	974140.197548	45.449511
3504.189969	974038.084631	45.454516
3504.365160	973935.556291	45.459521
3504.063384	973861.175390	45.464525
3504.192939	973783.690419	45.469530
3504.277465	973669.239609	45.474535
3504.151255	973590.522619	45.479540
3503.958869	973479.439227	45.484545
3504.340402	973388.996009	45.489549
3504.325704	973313.484749	45.494554
3504.428544	973217.020099	45.499559
3504.146967	973115.628334	45.504564
3504.197735	973019.658041	45.509569
3504.374417	972927.284857	45.514573
3504.030585	972840.180622	45.519578
3503.938990	972740.707425	45.524583
3503.479736	972656.652023	45.529588
3503.829288	972575.788360	45.534593
3504.046029	972474.987993	45.539597
3504.147011	972404.532911	45.544602
3504.213847	972323.418764	45.549607
3503.783400	972214.991588	45.554612
3503.912256	972135.625604	45.559617
3504.364235	972032.528482	45.564621
3503.879003	971946.999379	45.569626
3504.207731	971866.324835	45.574631
3504.048851	971789.741012	45.579636
3503.902331	971676.462608	45.584641
3504.015211	971575.565710	45.589645
3503.842759	971507.786500	45.594650
3503.939944	971427.731015	45.599655
3503.713972	971339.116836	45.604660
3503.593313	971246.765578	45.609665
3503.884122	971171.273654	45.614669
3503.710387	971090.083847	45.619674
3503.853235	970998.663740	45.624679
3503.877412	970919.787469	45.629684
3504.141061	970828.931909	45.634689
3503.803271	970743.458430	45.639693
3503.715411	970644.535439	45.644698
3503.920736	970580.303944	45.649703
3503.586643	970500.991614	45.654708
3503.766778	970407.305071	45.659713
3503.972952	970325.454680	45.664717
3503.650906	970236.056353	45.669722
3503.839323	970140.602456	45.674727
3503.484350	970072.347003	45.679732
3503.513463	969981.418796	45.684737
3503.907107	969919.987227	45.689741
3503.554763	969847.422195	45.694746
3504.007668	969740.956024	45.699751
3503.590531	969645.691522	45.704756
3503.679828	969576.280326	45.709761
3503.770316	969487.096030	45.714765
3503.446947	969428.126463	45.719770
3503.736042	969349.674408	45.724775
3503.856050	969256.272653	45.729780
3503.629132	969168.114541	45.734785
3503.930571	969098.075306	45.739789
3503.225081	969034.955439	45.744794
3503.474420	968932.129725	45.749799
3503.645752	968866.807875	45.754804
3503.685323	968787.801899	45.759809
3503.996282	968700.722746	45.764813
3503.545770	968594.286245	45.769818
3503.688471	968440.366896	45.774823
3503.766959	968255.027331	45.779828
3503.661206	967988.841355	45.784833
3503.766400	967665.035919	45.789837
3503.174138	967281.400858	45.794842
3503.259776	966826.827759	45.799847
3503.217028	966317.200306	45.804852
3503.329237	965745.601033	45.809857
3503.212674	965084.842821	45.814861
3502.987645	964361.718718	45.819866
3502.994124	963572.034002	45.824871
3502.913517	962723.849581	45.829876
3502.818920	961792.330494	45.834881
3502.891678	960789.856333	45.839885
3502.567185	959698.050172	45.844890
3502.629939	958517.026381	45.849895
3502.623124	957298.989214	45.854900
3502.398940	955996.748550	45.859905
3502.179478	954619.414994	45.864909
3501.577499	953168.020003	45.869914
3501.488155	951641.579580	45.874919
3501.454904	950026.892742	45.879924
3501.373362	948345.249694	45.884929
3501.681278	946563.178757	45.889933
3500.863471	944681.690395	45.894938
3500.706127	942728.185259	45.899943
3500.356915	940708.383915	45.904948
3500.254842	938583.956531	45.909953
3499.977639	936351.874006	45.914957
3499.797139	934067.363993	45.919962
3499.625874	931691.471624	45.924967
3499.182875	929209.613390	45.929972
3498.800640	926627.554343	45.934977
3498.317375	923984.337926	45.939981
3497.693059	921256.017729	45.944986
3497.687320	918421.739542	45.949991
3496.992765	915535.038033	45.954996
3496.600821	912538.701452	45.960001
3496.357451	909451.203236	45.965005
3495.884454	906292.635916	45.970010
3495.330989	903052.243657	45.975015
3495.097160	899710.699941	45.980020
3494.600282	896281.471241	45.985025
3494.386888	892767.323103	45.990029
3493.559115	889188.688984	45.995034
3493.114425	885499.969016	46.000039
3492.736274	881728.454834	46.005044
3492.142325	877866.293527	46.010049
3491.689816	873933.262627	46.015053
3490.618277	869913.829924	46.020058
3490.449174	865811.481843	46.025063
3489.864031	861617.247519	46.030068
3489.158795	857313.786494	46.035073
3488.701436	852939.500980	46.040077
3487.872079	848502.657162	46.045082
3487.425862	843964.407335	46.050087
3486.568869	839331.284770	46.055092
3486.070207	834608.216149	46.060097
3485.452167	829799.370982	46.065101
3484.368040	824919.767232	46.070106
3483.654720	819937.188651	46.075111
3483.170939	814900.450725	46.080116
3482.246486	809762.332100	46.085121
3481.546495	804518.663327	46.090125
3480.857553	799196.680441	46.095130
3480.121050	793802.601407	46.100135
3479.092925	788293.919701	46.105140
3478.591117	782720.480923	46.110145
3477.712699	777068.847297	46.115149
3476.863756	771306.449463	46.120154
3476.006034	765438.373991	46.125159
3475.158503	759522.384278	46.130164
3474.074945	753498.405438	46.135169
3473.294409	747407.494860	46.140173
3472.430440	741213.067666	46.145178
3471.287227	734910.580780	46.150183
3470.608387	728562.669638	46.155188
3469.248946	722107.803009	46.160193
3468.493507	715537.908955	46.165197
3466.958848	708908.415439	46.170202
3466.202605	702186.456744	46.175207
3465.286033	695383.258370	46.180212
3464.325813	688482.926543	46.185217
3462.967615	681482.305465	46.190221
3461.537255	674408.237978	46.195226
3460.462680	667268.824347	46.200231
3459.202023	660029.208973	46.205236
3457.925460	652715.435547	46.210241
3457.067813	645279.773032	46.215245
3455.596567	637810.320742	46.220250
3454.242440	630243.651725	46.225255
3453.256760	622576.731831	46.230260
3451.491108	614821.249057	46.235265
3450.487189	606995.964434	46.240269
3448.730961	599107.494538	46.245274
3447.648658	591107.367075	46.250279
3446.029579	583039.196435	46.255284
3444.533935	574878.628202	46.260289
3443.056453	566646.543805	46.265293
3441.385737	558339.062277	46.270298
3440.171112	549926.646867	46.275303
3438.425711	541445.444361	46.280308
3436.909839	532900.263986	46.285313
3435.214379	524249.307272	46.290317
3433.503710	515551.052531	46.295322
3432.053613	506763.936765	46.300327
3429.951687	497880.706109	46.305332
3428.217742	488921.973250	46.310337
3426.662388	479910.879755	46.315341
3424.290821	470827.941701	46.320346
3422.844391	461648.479380	46.325351
3421.104169	452416.468564	46.330356
3418.757462	443102.109095	46.335361
3416.816283	433709.748963	46.340365
3414.568507	424266.452070	46.345370
3412.697606	414724.312583	46.350375
3410.441305	405138.564200	46.355380
3408.091635	395483.006370	46.360385
3405.656466	385755.353257	46.365389
3403.797051	375974.881593	46.370394
3401.510988	366127.725828	46.375399
3398.888242	356238.477449	46.380404
3396.273812	346262.325143	46.385409
3393.826437	336255.753353	46.390413
3391.092193	326181.901006	46.395418
3388.627734	316056.372012	46.400423
3385.929753	305884.599070	46.405428
3382.807004	295649.869615	46.410433
3380.070145	285377.149314	46.415437
3376.962720	275079.298898	46.420442
3373.854464	264712.944700	46.425447
3370.772878	254326.968749	46.430452
3367.304210	243910.915154	46.435457
3364.560019	233428.056230	46.440461
3360.801936	222917.880230	46.445466
3357.750498	212346.048192	46.450471
3353.829757	201788.534153	46.455476
3349.613019	191231.259771	46.460481
3346.016301	180652.986578	46.465485
3341.580100	170056.204682	46.470490
3337.347935	159474.050710	46.475495
3333.001394	148887.291151	46.480500
3328.145127	138302.402308	46.485505
3323.171634	127716.384634	46.490509
3317.612465	117193.335757	46.495514
3311.751773	106683.800142	46.500519
3305.845278	96206.203906	46.505524
3299.239880	85775.385120	46.510529
3292.071025	75427.595818	46.515533
3284.083443	65165.705314	46.520538
3274.281700	55017.199696	46.525543
3250.427685	45405.325958	46.530548
3202.129961	36742.578491	46.535553
3148.860586	28745.680129	46.540557
3095.883866	21581.958438	46.545562
3047.811060	15327.040623	46.550567
3005.133813	10014.403370	46.555572
2966.641588	5646.127251	46.560577
2933.174856	2210.874429	46.565581
2874.677117	411.873372	46.570586
2794.434616	393.324900	46.575591
2764.653629	363.175374	46.580596
2776.641850	349.656751	46.585601
2811.924071	344.719046	46.590605
2849.002858	342.031304	46.595610
2876.570484	350.578912	46.600615
2892.195676	340.429915	46.605620
2895.436461	329.680178	46.610625
2892.304394	345.777101	46.615629
2886.194147	347.041810	46.620634
2879.915081	333.024787	46.625639
2875.303602	332.068024	46.630644
2871.579175	319.173865	46.635649
2869.358655	326.386933	46.640653
2867.488620	335.876013	46.645658
2865.567729	327.833028	46.650663
2863.866178	325.361900	46.655668
2860.983156	335.222975	46.660673
2858.534898	318.657071	46.665677
2855.421323	306.510924	46.670682
2852.223015	312.965957	46.675687
2849.501709	321.638851	46.680692
2845.847767	325.710526	46.685697
2842.840957	311.783493	46.690701
2839.715320	306.130671	46.695706
2836.878665	298.862847	46.700711
2833.981849	308.820794	46.705716
2830.400245	312.450133	46.710721
2827.446418	308.826256	46.715725
2824.220173	305.099909	46.720730
2820.999201	299.793986	46.725735
2817.812369	302.224551	46.730740
2814.515240	301.985757	46.735745
2811.431187	290.975380	46.740749
2808.138005	308.122840	46.745754
2804.295236	293.358205	46.750759
2801.597656	311.239398	46.755764
2797.801210	302.411723	46.760769
2794.849921	275.914792	46.765773
2791.187570	301.934686	46.770778
2788.160227	284.086766	46.775783
2784.849887	276.575174	46.780788
2781.016808	289.693365	46.785793
2778.436798	289.550134	46.790797
2774.814964	287.257417	46.795802
2770.924131	272.533106	46.800807
2767.900159	281.696867	46.805812
2764.274571	299.993759	46.810817
2760.732485	298.195161	46.815821
2757.756696	286.987125	46.820826
2754.362311	272.350556	46.825831
2751.501576	284.351137	46.830836
2747.342698	291.288436	46.835841
2744.332020	283.307106	46.840845
2740.550069	289.600225	46.845850
2737.576575	287.232793	46.850855
2734.069279	269.315190	46.855860
2730.106690	286.084297	46.860865
2727.000707	276.723673	46.865869
2723.661947	275.613399	46.870874
2720.442837	285.303785	46.875879
2717.148758	272.371364	46.880884
2712.943789	266.039595	46.885889
2709.610489	273.569222	46.890893
2706.208837	270.922289	46.895898
2702.878966	262.086328	46.900903
2699.386690	276.458621	46.905908
2695.832116	279.197080	46.910913
2692.668207	264.410882	46.915917
2689.484696	270.084472	46.920922
2686.064726	274.011971	46.925927
2682.282212	262.320536	46.930932
2678.960036	263.780055	46.935937
2675.415524	272.441018	46.940941
2671.547393	279.741485	46.945946
2668.399109	268.727583	46.950951
2665.717542	275.219692	46.955956
2661.289830	260.047032	46.960961
2657.932467	254.180964	46.965965
2654.532348	261.798964	46.970970
2650.699050	280.267828	46.975975
2647.666669	268.505207	46.980980
2643.865453	273.263183	46.985985
2640.949368	271.464715	46.990989
2638.032188	252.509360	46.995994
2634.350045	262.006101	47.000999
2630.807761	249.344036	47.006004
2626.950923	258.577972	47.011009
2623.510777	265.606145	47.016013
2619.885931	263.920311	47.021018
2616.695888	273.070948	47.026023
2613.569338	244.527390	47.031028
2609.313999	253.326585	47.036033
2605.895204	258.065712	47.041037
2602.386319	241.957538	47.046042
2599.328236	256.132272	47.051047
2595.544965	251.859328	47.056052
2592.013442	255.918801	47.061057
2589.104718	261.516531	47.066061
2585.160375	259.747062	47.071066
2581.814959	244.142978	47.076071
2578.312049	263.653566	47.081076
2574.677670	246.611064	47.086081
2571.811465	244.495825	47.091085
2567.747329	251.080974	47.096090
2564.354944	253.154771	47.101095
2560.895537	250.014219	47.106100
2556.871639	241.433760	47.111105
2554.119766	250.389827	47.116109
2550.602344	251.996126	47.121114
2547.051645	245.878181	47.126119
2543.917226	252.721110	47.131124
2540.092850	250.035943	47.136129
2536.272741	242.946826	47.141133
2533.092372	249.697797	47.146138
2529.480479	233.683808	47.151143
2526.110970	244.906503	47.156148
2522.496907	259.760104	47.161153
2519.158810	251.600864	47.166157
2515.456757	241.470639	47.171162
2512.164849	227.013675	47.176167
2509.081166	240.876071	47.181172
2505.186144	265.473911	47.186177
2501.466552	257.065851	47.191181
2498.166430	246.841435	47.196186
2494.648956	243.465642	47.201191
2491.481502	245.880799	47.206196
2488.214168	252.891075	47.211201
2484.368054	235.213037	47.216205
2481.079534	233.616039	47.221210
2477.079120	259.895285	47.226215
2473.537584	254.948025	47.231220
2470.149809	244.910125	47.236225
2466.801578	228.977495	47.241229
2463.131477	244.221920	47.246234
2459.437111	234.478456	47.251239
2456.604593	238.954335	47.256244
2452.782373	255.605157	47.261249
2450.086908	248.429372	47.266253
2445.859087	233.009669	47.271258
2442.390737	223.074563	47.276263
2439.040163	243.825717	47.281268
2435.171439	249.627186	47.286273
2431.875976	227.469938	47.291277
2428.359285	252.068028	47.296282
2424.654715	230.892732	47.301287
2421.499325	222.157008	47.306292
2417.824720	237.467588	47.311297
2414.249700	248.923289	47.316301
2410.999332	237.436288	47.321306
2407.651426	241.797610	47.326311
2404.362792	223.869075	47.331316
2400.658450	237.389138	47.336321
2397.174806	234.732993	47.341325
2393.259758	242.094472	47.346330
2389.717295	233.500328	47.351335
2386.597187	243.342961	47.356340
2383.349128	227.385182	47.361345
2379.765474	230.334942	47.366349
2375.762901	237.886952	47.371354
2372.164496	232.408925	47.376359
2369.208302	237.777491	47.381364
2365.441022	246.223439	47.386369
2362.011987	230.928552	47.391373
2358.734703	234.085667	47.396378
2354.654160	229.759587	47.401383
2351.512453	228.379437	47.406388
2347.912119	228.553786	47.411393
2344.771393	237.753574	47.416397
2341.403262	224.136661	47.421402
2337.639538	227.473743	47.426407
2334.393409	231.001781	47.431412
2330.535278	244.491501	47.436417
2327.266606	228.878778	47.441421
2323.665826	233.025347	47.446426
2319.847423	240.701889	47.451431
2316.735932	210.686734	47.456436
2313.257452	233.639649	47.461441
2309.705461	240.887720	47.466445
2306.271780	222.535695	47.471450
2302.603856	239.509729	47.476455
2299.336907	226.478211	47.481460
2295.694184	225.942294	47.486465
2291.879653	235.491664	47.491469
2288.168291	221.754613	47.496474
2284.779050	222.094337	47.501479
2281.590153	219.249162	47.506484
2277.769798	242.468015	47.511489
2274.577567	235.512059	47.516493
2271.398371	221.224877	47.521498
2267.558724	227.277120	47.526503
2264.505383	203.745453	47.531508
2260.961644	213.564460	47.536513
2257.595826	220.736655	47.541517
2253.542801	234.276986	47.546522
2249.467132	223.540993	47.551527
2246.464846	217.407840	47.556532
2243.052691	228.582011	47.561537
2239.892560	223.225124	47.566541
2236.349464	214.255820	47.571546
2232.904771	216.985721	47.576551
2229.498748	230.769254	47.581556
2225.519202	216.911934	47.586561
2222.212293	203.927221	47.591565
2218.664390	217.632145	47.596570
2214.924999	224.842299	47.601575
2211.613209	209.632658	47.606580
2208.066377	224.446434	47.611585
2204.831740	222.867902	47.616589
2201.368315	210.713893	47.621594
2197.310793	229.320246	47.626599
2194.191116	221.536735	47.631604
2190.773898	229.499630	47.636609
2187.243282	208.902242	47.641613
2183.892058	221.971993	47.646618
2180.250441	210.890706	47.651623
2176.890861	202.450911	47.656628
2173.066805	212.164067	47.661633
2169.820852	192.921868	47.666637
2166.580298	203.501100	47.671642
2162.608496	215.849292	47.676647
2159.017893	201.913474	47.681652
2155.176494	197.800028	47.686657
2152.332593	208.106578	47.691661
2149.085718	203.826506	47.696666
2145.233398	207.478577	47.701671
2141.841900	195.820798	47.706676
2137.821732	212.898040	47.711681
2134.514392	202.855475	47.716685
2130.794842	206.733163	47.721690
2127.921257	206.326554	47.726695
2124.460655	204.802796	47.731700
2121.041442	201.203732	47.736705
2117.314320	208.112989	47.741709
2113.628170	217.956134	47.746714
2110.154719	206.645022	47.751719
2106.869087	194.363304	47.756724
2102.907645	207.372828	47.761729
2099.578978	207.477526	47.766733
2096.062051	194.718227	47.771738
2092.703195	216.102638	47.776743
2089.527534	216.740950	47.781748
2085.906130	216.591582	47.786753
2082.133984	218.146194	47.791757
2078.684509	209.746927	47.796762
2074.983589	186.993251	47.801767
2071.809289	194.857404	47.806772
2068.089064	218.109183	47.811777
2064.774503	209.707002	47.816781
2061.437187	209.228449	47.821786
2057.469142	211.838087	47.826791
2054.260692	208.900752	47.831796
2050.772863	199.817977	47.836801
2047.350643	214.614098	47.841805
2044.115077	209.300633	47.846810
2040.159215	206.192329	47.851815
2036.899159	219.715666	47.856820
2033.188357	203.352954	47.861825
2029.741665	186.125539	47.866829
2026.197141	200.214191	47.871834
2022.047049	207.025461	47.876839
2019.323313	190.561598	47.881844
2015.458084	204.089366	47.886849
2012.173217	207.985469	47.891853
2009.034419	195.576990	47.896858
2005.378362	201.475941	47.901863
2002.059092	202.180006	47.906868
1998.126240	197.317008	47.911873
1994.809425	188.461463	47.916877
1991.108800	200.287219	47.921882
1987.226132	199.375530	47.926887
1984.173185	174.014978	47.931892
1980.779621	198.663889	47.936897
1977.072662	214.687243	47.941901
1973.885857	204.937995	47.946906
1970.149442	202.729416	47.951911
1966.599522	205.092157	47.956916
1962.985575	198.267408	47.961921
1959.693884	188.483691	47.966925
1956.177666	194.291328	47.971930
1952.621578	199.040726	47.976935
1949.408702	190.424841	47.981940
1945.864819	208.157424	47.986945
1942.458476	193.450103	47.991949
1938.846066	188.196798	47.996954
1935.381483	203.826217	48.001959
1931.924307	188.258294	48.006964
1928.021060	202.545751	48.011969
1924.709246	199.555885	48.016973
1921.648181	187.934189	48.021978
1917.569935	216.121095	48.026983
1914.398350	203.308185	48.031988
1910.417260	188.234330	48.036993
1907.143348	193.299037	48.041997
1903.666536	182.830986	48.047002
1900.069474	190.181339	48.052007
1896.838945	184.559834	48.057012
1893.124759	195.150901	48.062017
1889.620689	187.090642	48.067021
1886.252696	194.024890	48.072026
1882.412061	206.821317	48.077031
1879.408686	193.696276	48.082036
1875.618043	206.925714	48.087041
1871.996424	207.085951	48.092045
1868.932949	194.235310	48.097050
1865.224347	198.178001	48.102055
1861.762361	207.634939	48.107060
1857.936476	213.939806	48.112065
1854.469031	186.509095	48.117069
1851.263468	189.048476	48.122074
1847.130200	195.007783	48.127079
1844.269988	190.680149	48.132084
1840.764115	204.324785	48.137089
1837.584514	211.420342	48.142093
1834.009105	186.451197	48.147098
1829.957809	207.251368	48.152103
1826.852914	189.154326	48.157108
1823.144611	188.013899	48.162113
1819.513842	199.079941	48.167117
1816.242192	181.011909	48.172122
1812.255774	198.188451	48.177127
1809.114260	195.390926	48.182132
1805.923877	195.812097	48.187137
1802.339404	201.978900	48.192141
1798.812734	193.405300	48.197146
1794.471426	187.539773	48.202151
1791.768648	187.576165	48.207156
1788.108454	206.089750	48.212161
1784.808151	197.881591	48.217165
1781.337115	187.371026	48.222170
1777.356583	180.220569	48.227175
1774.278885	185.379222	48.232180
1770.209511	195.134691	48.237185
1767.139810	200.923189	48.242189
1763.860145	182.006750	48.247194
1760.017442	196.798633	48.252199
1756.881336	180.953526	48.257204
1753.020383	201.699816	48.262209
1749.495022	209.506795	48.267213
1746.187626	200.361673	48.272218
1742.656024	204.112743	48.277223
1739.085392	191.933315	48.282228
1735.430410	208.400179	48.287233
1732.263972	194.736768	48.292237
1728.730032	183.606152	48.297242
1724.905405	202.394395	48.302247
1721.373905	169.739383	48.307252
1717.926565	177.658967	48.312257
1714.612580	178.661885	48.317261
1711.089422	178.027026	48.322266
1707.583683	192.873711	48.327271
1704.005073	190.338654	48.332276
1700.820171	180.040967	48.337281
1697.119519	189.332348	48.342285
1693.520295	192.660935	48.347290
1689.989375	184.205794	48.352295
1686.582086	192.089391	48.357300
1682.956225	190.778977	48.362305
1679.217615	191.896273	48.367309
1676.011495	176.592321	48.372314
1672.420847	186.870000	48.377319
1669.061859	194.226149	48.382324
1665.471881	179.227035	48.387329
1662.011424	195.765195	48.392333
1659.039142	185.782053	48.397338
1655.178739	188.531480	48.402343
1651.520128	189.382753	48.407348
1648.210925	175.542119	48.412353
1644.315334	186.733109	48.417357
1641.048122	194.171886	48.422362
1637.590905	199.692227	48.427367
1634.198015	178.096122	48.432372
1630.342222	175.832063	48.437377
1626.472934	189.140656	48.442381
1623.459998	169.618209	48.447386
1619.782229	188.898169	48.452391
1616.457502	193.293760	48.457396
1613.118339	183.866602	48.462401
1609.704407	197.187072	48.467405
1606.063482	183.954618	48.472410
1602.714649	175.970620	48.477415
1598.931049	186.669536	48.482420
1595.230606	174.246467	48.487425
1591.914349	175.434289	48.492429
1588.442965	178.856950	48.497434
1584.939077	176.305387	48.502439
1581.511987	184.658306	48.507444
1577.648958	194.896139	48.512449
1574.658633	181.634077	48.517453
1571.271296	162.080237	48.522458
1567.388986	180.590071	48.527463
1564.102279	192.490028	48.532468
1560.251025	184.038010	48.537473
1556.966379	186.928241	48.542477
1553.357488	186.193571	48.547482
1549.609670	185.893096	48.552487
1546.700129	184.318539	48.557492
1543.403809	185.248580	48.562497
1539.659315	182.318970	48.567501
1535.808586	190.740542	48.572506
1532.299695	189.339777	48.577511
1528.762792	172.359423	48.582516
1525.378255	182.983038	48.587521
1521.971631	167.755685	48.592525
1518.697693	167.719628	48.597530
1514.784449	188.244262	48.602535
1511.584592	176.733307	48.607540
1507.694931	179.398854	48.612545
1504.458300	196.170026	48.617549
1500.871068	184.183493	48.622554
1497.106096	174.997047	48.627559
1494.077403	168.332284	48.632564
1490.660462	183.367495	48.637569
1486.874658	186.898917	48.642573
1483.434610	164.904881	48.647578
1479.742567	177.857942	48.652583
1476.693626	165.749947	48.657588
1472.855735	176.485786	48.662593
1469.143077	175.982058	48.667597
1466.006926	162.757558	48.672602
1462.337437	183.471332	48.677607
1458.846283	170.852327	48.682612
1455.331067	181.666223	48.687617
1451.683025	175.366892	48.692621
1448.490225	168.877703	48.697626
1444.890268	172.872501	48.702631
1441.526867	175.916057	48.707636
1437.909989	173.953507	48.712641
1434.410763	171.868454	48.717645
1430.894833	187.225343	48.722650
1427.383437	183.173965	48.727655
1423.957227	169.077756	48.732660
1420.163800	183.949126	48.737665
1416.629682	182.680927	48.742669
1413.327537	161.743994	48.747674
1409.755386	174.990894	48.752679
1406.172581	185.892223	48.757684
1402.891970	178.507513	48.762689
1399.395331	163.394244	48.767693
1395.559215	167.815632	48.772698
1392.006346	188.205263	48.777703
1388.899151	188.939022	48.782708
1385.612211	176.812050	48.787713
1381.880478	155.135656	48.792717
1378.857949	167.430250	48.797722
1375.057067	189.806268	48.802727
1371.516040	161.876042	48.807732
1367.735765	183.768235	48.812737
1364.245934	172.419170	48.817741
1360.642813	162.275062	48.822746
1356.922696	176.505662	48.827751
1353.842398	163.967283	48.832756
1350.357903	169.088670	48.837761
1346.646975	163.924970	48.842765
1343.516379	163.320303	48.847770
1339.439581	185.194666	48.852775
1336.307078	174.793639	48.857780
1332.787027	168.476511	48.862785
1329.133795	173.736839	48.867789
1325.835336	161.737101	48.872794
1322.055645	163.761628	48.877799
1318.387862	173.939417	48.882804
1314.852147	176.602674	48.887809
1311.583155	166.541648	48.892813
1308.635503	185.138791	48.897818
1304.847440	169.419051	48.902823
1301.551747	151.656635	48.907828
1297.975791	160.197589	48.912833
1293.912356	175.139315	48.917837
1290.489346	155.484929	48.922842
1287.129098	167.066729	48.927847
1283.632154	178.616648	48.932852
1280.209474	159.646434	48.937857
1276.520938	170.950676	48.942861
1273.566033	162.554013	48.947866
1269.966596	156.598160	48.952871
1266.555346	176.456594	48.957876
1262.859640	172.827171	48.962881
1259.100539	172.215903	48.967885
1255.607032	179.146356	48.972890
1252.188425	168.898360	48.977895
1248.780046	154.033234	48.982900
1245.182069	167.054108	48.987905
1241.382771	169.277929	48.992909
1238.359008	168.288801	48.997914
1234.395421	166.866381	49.002919
1231.186015	155.541655	49.007924
1227.617872	167.488167	49.012929
1224.069332	164.397461	49.017933
1220.711809	154.762966	49.022938
1217.009738	178.865226	49.027943
1213.798465	170.525313	49.032948
1210.531691	159.511437	49.037953
1206.501330	155.979516	49.042957
1203.008776	170.746244	49.047962
1199.719024	180.938529	49.052967
1196.231609	160.940589	49.057972
1192.527718	157.048876	49.062977
1188.789291	168.129565	49.067981
1185.934538	151.470322	49.072986
1182.060572	155.530995	49.077991
1178.708579	162.761975	49.082996
1175.158118	154.491602	49.088001
1171.256156	174.873999	49.093005
1168.453816	160.433087	49.098010
1164.423433	165.213583	49.103015
1161.291679	160.193800	49.108020
1158.116077	171.367246	49.113025
1154.294784	164.629797	49.118029
1151.044782	163.549619	49.123034
1146.654758	179.486826	49.128039
1143.446279	166.670330	49.133044
1140.011821	147.778726	49.138049
1136.491394	166.317146	49.143053
1133.209335	169.849630	49.148058
1129.353349	168.342723	49.153063
1126.024812	168.788390	49.158068
1122.705460	180.167887	49.163073
1118.744177	164.128558	49.168077
1115.555456	147.060161	49.173082
1111.724229	162.311451	49.178087
1108.614249	168.388870	49.183092
1105.741890	161.158400	49.188097
1101.764646	173.093883	49.193101
1098.051267	159.882532	49.198106
1094.471034	158.666116	49.203111
1090.884581	161.519862	49.208116
1087.497871	148.334896	49.213121
1083.723138	164.974122	49.218125
1080.801314	163.630664	49.223130
1077.196160	160.764044	49.228135
1073.658334	147.843553	49.233140
1069.985355	157.885373	49.238145
1066.314130	167.875613	49.243149
1062.839620	152.560941	49.248154
1059.256397	163.381967	49.253159
1056.189955	176.800316	49.258164
1053.039261	164.569383	49.263169
1049.322977	150.402457	49.268173
1046.037482	158.694814	49.273178
1041.760743	162.382782	49.278183
1038.489568	160.920540	49.283188
1034.801340	171.873350	49.288193
1031.239311	179.720607	49.293197
1027.850736	149.647047	49.298202
1024.561988	144.834575	49.303207
1020.766935	166.736889	49.308212
1017.687183	158.111594	49.313217
1014.155297	167.401632	49.318221
1010.539818	138.942953	49.323226
1007.074064	158.457771	49.328231
1003.512129	156.726598	49.333236
1000.172259	156.162958	49.338241
996.845424	153.131857	49.343245
993.020802	150.536109	49.348250
989.053955	176.736884	49.353255
985.836779	171.881039	49.358260
982.635720	162.131769	49.363265
978.814317	150.145401	49.368269
975.470480	145.858571	49.373274
971.981798	164.290685	49.378279
968.280492	151.866523	49.383284
964.897885	157.960499	49.388289
961.266586	164.004293	49.393293
958.293042	148.613688	49.398298
954.268116	167.470151	49.403303
950.880090	159.858004	49.408308
947.546878	141.563713	49.413313
943.918098	152.843319	49.418317
940.733220	148.480345	49.423322
936.932288	167.882345	49.428327
933.105196	157.189921	49.433332
929.892794	151.468479	49.438337
926.366647	145.090556	49.443341
922.807049	159.956634	49.448346
919.467664	152.144312	49.453351
916.032629	156.883161	49.458356
912.432637	176.267587	49.463361
908.892998	165.975570	49.468365
905.416585	154.083906	49.473370
901.805761	143.485919	49.478375
898.013567	166.012733	49.483380
894.719608	161.051834	49.488385
891.305993	155.742346	49.493389
888.246662	158.946556	49.498394
884.503844	168.910225	49.503399
880.641709	146.584371	49.508404
877.206071	156.597440	49.513409
873.618661	162.615384	49.518413
870.173971	148.666733	49.523418
866.896911	153.406350	49.528423
863.570691	156.476582	49.533428
860.134100	173.414605	49.538433
856.485062	162.419770	49.543437
852.894994	159.623885	49.548442
849.336041	157.144751	49.553447
845.474034	161.484380	49.558452
842.232599	156.923930	49.563457
838.759044	152.818403	49.568461
835.684244	155.010499	49.573466
831.830977	162.611466	49.578471
828.310873	149.745328	49.583476
825.118216	133.548650	49.588481
821.281112	155.208576	49.593485
817.958325	168.028410	49.598490
814.255881	155.838629	49.603495
810.566889	154.839992	49.608500
807.390878	156.276797	49.613505
803.799253	147.897839	49.618509
800.463353	147.391748	49.623514
796.621292	159.246836	49.628519
792.705410	148.133648	49.633524
789.729403	166.973018	49.638529
786.456669	161.019137	49.643533
783.129551	151.719728	49.648538
779.518769	164.459286	49.653543
775.681644	143.217872	49.658548
772.692750	153.622230	49.663553
768.359730	150.940013	49.668557
765.111890	146.539882	49.673562
761.294164	157.030320	49.678567
758.033431	148.140401	49.683572
754.708303	158.946747	49.688577
751.219159	148.532961	49.693581
748.034412	154.413831	49.698586
744.365512	157.334735	49.703591
740.694151	137.150614	49.708596
737.450222	141.722341	49.713601
733.549619	160.161887	49.718605
729.960312	139.027660	49.723610
726.572697	156.301111	49.728615
723.361665	161.147773	49.733620
720.207285	145.526159	49.738625
716.333765	156.071998	49.743629
712.659745	140.014567	49.748634
708.972883	139.361693	49.753639
705.392429	154.338620	49.758644
702.101462	163.176260	49.763649
698.835199	149.590873	49.768653
694.942015	155.530663	49.773658
691.270101	157.974540	49.778663
687.983560	126.673263	49.783668
684.747653	149.601783	49.788673
681.349005	149.159286	49.793677
677.905301	145.729394	49.798682
674.144213	160.363185	49.803687
670.537689	145.370383	49.808692
667.123679	130.464673	49.813697
663.506533	142.371149	49.818701
659.991462	148.841378	49.823706
656.658939	142.418618	49.828711
653.395916	154.401175	49.833716
649.620932	147.923548	49.838721
645.887543	143.318881	49.843725
642.725003	150.373089	49.848730
639.330552	140.167967	49.853735
636.061049	123.345178	49.858740
631.998675	142.648682	49.863745
628.376511	171.118540	49.868749
625.446954	150.263589	49.873754
621.659832	135.206550	49.878759
617.967619	145.747047	49.883764
614.821292	130.449034	49.888769
611.123029	139.476687	49.893773
607.788334	150.430070	49.898778
603.832428	144.375861	49.903783
600.258141	151.358212	49.908788
597.229598	141.924869	49.913793
593.508138	145.797502	49.918797
590.439942	118.892389	49.923802
586.620709	142.272795	49.928807
582.787345	159.464354	49.933812
579.454008	144.823748	49.938817
575.736636	160.228687	49.943821
572.563230	145.138570	49.948826
568.978080	138.628362	49.953831
565.518064	150.153011	49.958836
562.640376	129.244088	49.963841
558.666460	152.524095	49.968845
555.128580	154.947680	49.973850
551.409105	146.607462	49.978855
548.175328	140.827321	49.983860
544.886171	151.590611	49.988865
540.907619	141.011581	49.993869
537.345720	136.638002	49.998874
533.728573	143.026600	50.003879
530.275959	134.310572	50.008884
527.148457	136.328221	50.013889
523.424648	144.600159	50.018893
520.135329	129.889597	50.023898
516.334527	135.055027	50.028903
512.811587	138.743387	50.033908
509.890594	139.448366	50.038913
506.570812	142.450916	50.043917
502.747170	135.578946	50.048922
498.828934	155.544408	50.053927
495.104459	141.401238	50.058932
491.911141	127.655887	50.063937
488.640902	151.101218	50.068941
485.017582	141.957563	50.073946
481.490261	146.684434	50.078951
477.820988	152.138506	50.083956
474.519803	142.311881	50.088961
470.690693	156.334032	50.093965
467.556657	139.938399	50.098970
463.912520	122.170623	50.103975
460.460301	129.389645	50.108980
457.238539	147.705902	50.113985
453.132236	146.387934	50.118989
449.858745	135.673663	50.123994
446.581274	146.939737	50.128999
442.806288	144.908278	50.134004
439.283958	138.418156	50.139009
435.995688	157.221292	50.144013
432.603015	153.687615	50.149018
429.189773	135.784835	50.154023
425.572999	147.763071	50.159028
421.741574	143.400937	50.164033
418.325686	139.442387	50.169037
414.950718	141.151264	50.174042
411.393748	139.339602	50.179047
407.889571	142.984471	50.184052
404.452239	128.547129	50.189057
400.965832	142.943477	50.194061
397.801875	158.126553	50.199066
393.742566	141.224364	50.204071
390.223193	126.976968	50.209076
386.785015	129.886971	50.214081
383.195681	154.304933	50.219085
379.784010	152.960842	50.224090
375.998712	137.403740	50.229095
372.795196	132.545195	50.234100
369.617906	137.660966	50.239105
366.051028	150.682763	50.244109
362.691224	134.813891	50.249114
359.054817	144.244778	50.254119
354.903713	142.979949	50.259124
351.567401	119.376740	50.264129
348.405002	132.453930	50.269133
344.978813	150.476489	50.274138
341.476830	157.491116	50.279143
337.677797	143.704359	50.284148
334.685092	143.464978	50.289153
330.891900	140.421418	50.294157
327.091428	136.853374	50.299162
323.759452	134.870136	50.304167
320.132230	121.550630	50.309172
316.956474	134.621063	50.314177
313.446993	130.181843	50.319181
309.797987	115.639965	50.324186
306.476031	131.785406	50.329191
302.763790	123.039128	50.334196
299.430704	130.335117	50.339201
295.823626	138.317683	50.344205
292.410345	120.932726	50.349210
289.113336	148.907167	50.354215
285.390254	134.438884	50.359220
282.027944	135.811324	50.364225
278.273013	151.597145	50.369229
274.725087	129.821261	50.374234
271.271134	137.266561	50.379239
267.536726	149.029720	50.384244
264.395426	111.527755	50.389249
260.550828	121.231797	50.394253
257.157894	140.791620	50.399258
253.659855	143.430932	50.404263
249.783148	134.010081	50.409268
246.321575	134.410004	50.414273
243.019469	140.257600	50.419277
240.060361	124.413475	50.424282
236.767777	136.011008	50.429287
232.962920	158.093157	50.434292
229.394247	136.560046	50.439297
225.601092	155.073877	50.444301
222.116666	145.743197	50.449306
218.481010	124.013528	50.454311
215.105417	138.873032	50.459316
211.820141	123.813298	50.464321
208.028156	129.952361	50.469325
204.464151	136.680759	50.474330
201.141975	128.591106	50.479335
197.304667	142.517652	50.484340
194.221194	128.108699	50.489345
190.888409	149.828945	50.494349
187.609229	146.869426	50.499354
183.978651	128.957859	50.504359
180.214476	142.824388	50.509364
176.826631	113.119748	50.514369
172.837356	143.407130	50.519373
169.485617	131.005985	50.524378
166.100879	140.084835	50.529383
162.662838	144.337220	50.534388
159.635165	128.189294	50.539393
155.665103	114.467436	50.544397
152.308374	121.171197	50.549402
148.464551	143.438148	50.554407
144.811773	138.533613	50.559412
141.709204	140.597533	50.564417
138.202951	140.890072	50.569421
134.490176	146.663725	50.574426
131.406441	138.059330	50.579431
127.803319	123.688842	50.584436
124.460688	122.653102	50.589441
120.849306	134.766999	50.594445
116.999823	123.209698	50.599450
113.309216	142.447352	50.604455
109.864815	150.921126	50.609460
106.539415	127.189138	50.614465
103.046231	138.827075	50.619469
99.444166	131.121994	50.624474
96.232903	125.576799	50.629479
92.199195	140.866419	50.634484
89.240805	128.562801	50.639489
85.642378	134.327148	50.644493
81.879429	124.543027	50.649498
78.981985	138.099090	50.654503
75.356793	146.397174	50.659508
72.060981	118.810914	50.664513
68.168207	123.717740	50.669517
64.604009	133.262428	50.674522
60.905842	134.999148	50.679527
57.432455	127.649835	50.684532
53.984313	135.523610	50.689537
50.196734	144.312870	50.694541
46.944066	141.890719	50.699546
43.553746	122.227229	50.704551
40.252965	133.787227	50.709556
36.681796	145.198004	50.714561
33.269795	140.167138	50.719565
29.652509	113.367291	50.724570
25.942414	125.708047	50.729575
22.493619	140.653633	50.734580
19.018169	127.084515	50.739585
15.086248	139.482760	50.744589
11.999761	138.668236	50.749594
8.651801	127.445701	50.754599
4.879353	128.583612	50.759604
1.925776	132.710240	50.764609