Wed Jun 15 16:20:39 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.230910	112.672545	0.000000
-0.260673	113.298247	0.005005
0.320580	91.433553	0.010010
-0.055833	85.917987	0.015014
-0.439771	72.953395	0.020019
-0.243977	83.620429	0.025024
-0.605301	79.528208	0.030029
-0.423990	49.192312	0.035034
-0.895886	53.511688	0.040038
-1.120870	49.257459	0.045043
-1.683150	43.546427	0.050048
-1.652183	18.297764	0.055053
-1.979232	9.567382	0.060058
-2.348392	14.797733	0.065062
-2.483375	-9.194331	0.070067
-2.636516	1.992563	0.075072
-3.351833	2.265645	0.080077
-3.570335	-14.680729	0.085082
-3.709147	-20.089327	0.090086
-3.668686	-38.316869	0.095091
-4.299686	-17.853592	0.100096
-4.595595	-20.079366	0.105101
-4.646926	-24.476799	0.110106
-5.541180	-16.033599	0.115110
-5.870342	-21.870924	0.120115
-6.254437	-28.505203	0.125120
-6.266398	-15.232409	0.130125
-6.294417	-35.140808	0.135130
-6.680855	-7.551912	0.140134
-6.661274	-8.520792	0.145139
-6.391462	-27.579163	0.150144
-6.797091	-12.768728	0.155149
-7.562803	-21.101662	0.160154
-7.988513	-32.733460	0.165158
-8.318242	-29.715260	0.170163
-8.583677	-14.840989	0.175168
-8.604611	-12.574989	0.180173
-8.222161	-35.839182	0.185178
-8.683826	-24.302427	0.190182
-9.171315	-17.088593	0.195187
-9.304497	-3.862245	0.200192
-9.603314	-19.880103	0.205197
-9.585817	-31.112631	0.210202
-10.727730	-17.371772	0.215206
-11.168710	-25.664949	0.220211
-11.195262	-21.594580	0.225216
-11.582061	-5.583279	0.230221
-11.256339	-12.237599	0.235226
-11.155900	-21.337307	0.240230
-11.190725	-23.902360	0.245235
-11.619510	-26.388893	0.250240
-12.262113	-28.558260	0.255245
-12.487898	-13.365405	0.260250
-13.081790	-5.945273	0.265254
-13.272943	-25.012107	0.270259
-13.134049	-17.296890	0.275264
-13.368721	-25.698539	0.280269
-13.620020	-27.118842	0.285274
-14.334061	-14.970103	0.290278
-14.286558	-22.782118	0.295283
-14.599696	-11.656590	0.300288
-14.766274	-3.415708	0.305293
-14.532502	-20.605400	0.310298
-14.954228	-12.686362	0.315302
-15.548892	-12.390997	0.320307
-16.196682	-33.197244	0.325312
-16.467181	-28.843205	0.330317
-16.347880	-19.242295	0.335322
-16.726553	-10.094043	0.340326
-16.892683	-25.851496	0.345331
-16.627349	-35.593993	0.350336
-16.838554	-12.771329	0.355341
-17.403721	-18.819917	0.360346
-18.074154	-24.796358	0.365350
-18.267710	-20.723644	0.370355
-18.283366	-27.091107	0.375360
-18.238259	-33.510730	0.380365
-18.662549	-18.178440	0.385370
-19.431212	-0.872141	0.390374
-19.656003	-25.510063	0.395379
-19.651792	-29.390102	0.400384
-19.940696	-19.824622	0.405389
-19.698399	-23.743613	0.410394
-20.156072	-22.681128	0.415398
-20.451061	-12.839811	0.420403
-20.777070	-16.380294	0.425408
-21.633431	-9.630886	0.430413
-21.136482	-13.134048	0.435418
-21.498584	-20.451139	0.440422
-21.504643	-20.593470	0.445427
-21.580186	-7.146412	0.450432
-22.569741	-14.552570	0.455437
-22.676246	-29.909307	0.460442
-23.171845	-26.640952	0.465446
-22.975255	-22.654020	0.470451
-22.806144	-16.646522	0.475456
-22.811354	-22.865870	0.480461
-23.528486	-11.087920	0.485466
-23.881785	-3.300928	0.490470
-24.274744	-22.959827	0.495475
-24.505135	-26.321875	0.500480
-25.196672	-4.113399	0.505485
-25.597879	-10.951815	0.510490
-25.581320	-19.484257	0.515494
-25.403788	-33.267968	0.520499
-25.716535	-19.828776	0.525504
-26.163917	-13.568568	0.530509
-25.737196	-26.975601	0.535514
-26.569420	-11.714390	0.540518
-26.923369	-7.086721	0.545523
-27.264344	-29.144194	0.550528
-27.380021	-11.430887	0.555533
-27.587492	-23.318833	0.560538
-27.821834	-25.160689	0.565542
-27.794719	-1.767369	0.570547
-27.939387	-10.731284	0.575552
-28.812664	-23.342857	0.580557
-29.303376	-20.742548	0.585562
-29.468841	-14.807702	0.590566
-29.588809	-8.800667	0.595571
-29.385099	-10.500756	0.600576
-29.832333	-20.742338	0.605581
-29.147356	-28.360898	0.610586
-29.991968	-21.140726	0.615590
-30.533267	-13.129424	0.620595
-30.440814	-4.076289	0.625600
-31.031305	-17.368891	0.630605
-31.333073	-26.937970	0.635610
-31.970428	-11.707680	0.640614
-31.916743	-25.060269	0.645619
-31.963214	-37.127513	0.650624
-32.247491	-17.929454	0.655629
-31.929669	-18.423121	0.660634
-32.565375	-20.383610	0.665638
-33.414073	-22.600300	0.670643
-33.217362	-24.244285	0.675648
-33.677327	-12.946230	0.680653
-33.563014	-31.265882	0.685658
-33.803358	-15.694588	0.690662
-34.770994	-26.491461	0.695667
-34.777997	-7.631498	0.700672
-35.611549	-12.014784	0.705677
-35.162980	-37.155881	0.710682
-35.590960	-15.211056	0.715686
-35.743541	-36.455044	0.720691
-35.506341	-24.697106	0.725696
-35.387699	-8.368738	0.730701
-35.750524	-29.877479	0.735706
-36.640521	-21.884612	0.740710
-37.205814	-19.654329	0.745715
-37.063699	-27.073878	0.750720
-37.390192	-20.568097	0.755725
-37.284200	-8.393683	0.760730
-38.365235	1.556729	0.765734
-38.056923	-12.658782	0.770739
-38.337170	-27.662951	0.775744
-38.788844	-5.266050	0.780749
-38.647362	-21.629517	0.785754
-38.798352	-24.514910	0.790758
-38.765735	-15.531600	0.795763
-39.643828	-14.051415	0.800768
-40.205783	-12.072341	0.805773
-40.230978	-26.343503	0.810778
-40.419076	-5.266142	0.815782
-40.442977	-5.846373	0.820787
-40.408944	-19.133373	0.825792
-41.061590	-15.824167	0.830797
-41.332805	-25.977344	0.835802
-41.824357	-22.368145	0.840806
-42.154434	-9.460051	0.845811
-41.759246	-10.606716	0.850816
-42.332299	-18.635594	0.855821
-42.448725	-37.149120	0.860826
-43.044487	-26.098626	0.865830
-43.151302	-9.979321	0.870835
-43.418260	-19.869822	0.875840
-43.784232	-3.680259	0.880845
-43.708019	-17.309923	0.885850
-43.557529	-27.204497	0.890854
-44.424699	-16.360888	0.895859
-44.431669	-17.356552	0.900864
-44.745165	-16.466847	0.905869
-44.584292	-31.232091	0.910874
-45.513064	-9.141366	0.915878
-46.146665	-23.795841	0.920883
-46.016257	-33.932818	0.925888
-46.853478	-20.533123	0.930893
-46.696291	-10.231577	0.935898
-46.775585	-9.933386	0.940902
-46.985016	-17.535342	0.945907
-46.460626	-29.826255	0.950912
-46.843939	-17.380700	0.955917
-47.168736	-16.929679	0.960922
-48.033358	-23.973726	0.965926
-48.291839	-13.474855	0.970931
-48.365107	-23.264881	0.975936
-48.815168	-27.548573	0.980941
-48.646144	-23.685031	0.985946
-48.596049	-1.258395	0.990950
-49.868156	-1.320231	0.995955
-50.048378	-18.034293	1.000960
-50.256009	-24.843035	1.005965
-50.268158	-14.158285	1.010970
-50.459555	-1.483317	1.015974
-50.617402	-26.544730	1.020979
-50.110188	-23.688812	1.025984
-50.880936	-1.731616	1.030989
-51.339484	-34.991100	1.035994
-51.770367	-17.531810	1.040998
-51.812274	-7.117161	1.046003
-51.656080	-19.914250	1.051008
-52.547214	-9.434131	1.056013
-53.161117	-13.646952	1.061018
-53.215067	-25.231575	1.066022
-53.828526	-22.448018	1.071027
-53.110118	-16.662005	1.076032
-53.491855	-12.330615	1.081037
-53.607740	-7.056108	1.086042
-53.569066	-9.809983	1.091046
-53.973421	-17.523155	1.096051
-54.289266	-42.115117	1.101056
-54.977193	-15.611439	1.106061
-55.051440	-14.011564	1.111066
-54.954900	-25.545593	1.116070
-55.987807	-23.184268	1.121075
-56.032020	-15.982234	1.126080
-56.470180	-4.727631	1.131085
-56.306858	-29.289303	1.136090
-56.396585	-16.052396	1.141094
-56.399348	-29.490645	1.146099
-57.326308	-11.004340	1.151104
-57.794561	-4.297661	1.156109
-57.911312	-17.829834	1.161114
-57.937840	-13.147174	1.166118
-57.681523	-13.795120	1.171123
-57.812152	-12.687245	1.176128
-58.483134	-22.697610	1.181133
-59.170817	-11.551026	1.186138
-59.615247	-10.588682	1.191142
-59.785196	-21.130884	1.196147
-59.318141	-21.673186	1.201152
-59.549649	-21.672609	1.206157
-59.856597	-28.105569	1.211162
-60.411391	-9.085540	1.216166
-60.841233	-3.070007	1.221171
-60.850906	-24.564014	1.226176
-61.133662	-13.029594	1.231181
-60.755559	-13.590340	1.236186
-61.408524	-24.370454	1.241190
-62.405381	-17.161617	1.246195
-62.299079	-25.605602	1.251200
-62.946381	-19.404591	1.256205
-63.180865	1.082943	1.261210
-63.467124	-9.537212	1.266214
-63.758826	-33.949593	1.271219
-63.218045	-24.519657	1.276224
-63.476709	-26.804948	1.281229
-63.049302	-25.420855	1.286234
-63.803930	-16.300738	1.291238
-64.758500	-8.303997	1.296243
-65.052195	-7.333714	1.301248
-65.330723	-23.274907	1.306253
-65.275272	-15.680162	1.311258
-65.375465	1.923170	1.316262
-65.308918	-18.153373	1.321267
-65.211215	-21.876034	1.326272
-66.071395	-9.321086	1.331277
-66.274721	-20.066013	1.336282
-66.422852	-18.940252	1.341286
-66.678913	1.668335	1.346291
-67.351248	-6.877022	1.351296
-68.128115	-16.733660	1.356301
-67.962610	-37.272114	1.361306
-68.126096	-20.544087	1.366310
-68.263811	-2.300070	1.371315
-68.062172	-20.095851	1.376320
-68.366192	-29.664254	1.381325
-68.332104	-17.171378	1.386330
-68.917235	-19.535691	1.391334
-69.463404	-31.105647	1.396339
-69.760340	-16.589787	1.401344
-69.918007	-8.037678	1.406349
-69.780476	-21.965612	1.411354
-70.806904	-27.686214	1.416358
-71.357365	-11.664451	1.421363
-71.222061	-6.888681	1.426368
-71.256906	-14.194844	1.431373
-70.948294	-18.412939	1.436378
-71.112576	-17.083962	1.441382
-71.319564	-17.799364	1.446387
-71.881021	-21.844369	1.451392
-72.974934	-3.864336	1.456397
-72.907541	-14.048914	1.461402
-73.034571	-14.862168	1.466406
-72.905274	-1.306915	1.471411
-72.924799	-13.939525	1.476416
-73.989617	-7.135835	1.481421
-74.064699	-28.850743	1.486426
-74.386960	-20.983266	1.491430
-74.888059	-5.638670	1.496435
-74.749119	-4.141401	1.501440
-74.666666	-12.551463	1.506445
-74.609408	-6.423480	1.511450
-75.174625	-21.361613	1.516454
-75.973348	-34.455926	1.521459
-76.055312	-24.982854	1.526464
-76.196364	-9.338497	1.531469
-75.965864	-28.079920	1.536474
-76.437186	-25.907582	1.541478
-77.666709	-9.687573	1.546483
-77.397616	-13.769124	1.551488
-77.696162	-1.264569	1.556493
-77.903934	-25.691717	1.561498
-77.533964	-33.788832	1.566502
-77.861120	-16.260372	1.571507
-77.978424	-3.061218	1.576512
-78.400260	-17.413714	1.581517
-79.154252	-18.095930	1.586522
-79.428224	-14.714453	1.591526
-79.616025	-13.188242	1.596531
-79.462660	-8.641160	1.601536
-79.444302	-10.644533	1.606541
-80.364570	-9.135474	1.611546
-80.649356	-35.035287	1.616550
-81.055535	-22.958544	1.621555
-81.007948	-23.578111	1.626560
-81.306716	-13.282502	1.631565
-81.129275	-15.514686	1.636570
-81.360986	-23.145110	1.641574
-82.043993	-21.499476	1.646579
-81.887049	-8.006507	1.651584
-82.413126	-4.924777	1.656589
-82.499409	-16.367929	1.661594
-82.529350	-10.659678	1.666598
-83.598109	-17.275500	1.671603
-83.498263	-27.135066	1.676608
-83.829737	-9.752473	1.681613
-83.797774	-0.433655	1.686618
-83.972487	-23.838872	1.691622
-84.302790	-15.895094	1.696627
-84.847589	-12.857621	1.701632
-85.339834	-17.589097	1.706637
-85.574680	-20.779157	1.711642
-85.535880	-10.960947	1.716646
-85.945507	-19.191428	1.721651
-85.778083	-23.180118	1.726656
-85.992630	-6.987376	1.731661
-85.957893	-3.787523	1.736666
-86.807431	-16.138638	1.741670
-87.138829	-12.594276	1.746675
-87.289382	-9.368537	1.751680
-87.545965	-11.875337	1.756685
-87.498939	-30.169260	1.761690
-87.402429	-17.413356	1.766694
-88.636899	2.589068	1.771699
-88.557055	-15.930178	1.776704
-89.096263	-13.997376	1.781709
-89.000135	-16.950440	1.786714
-88.978271	-24.585680	1.791718
-89.099931	-19.785796	1.796723
-89.171456	-21.329026	1.801728
-90.264084	-11.513624	1.806733
-90.316781	-29.448766	1.811738
-90.577631	-20.692679	1.816742
-91.134662	-16.974700	1.821747
-90.721260	-41.421617	1.826752
-91.002488	-20.631639	1.831757
-91.397332	-24.414257	1.836762
-91.767659	-20.953132	1.841766
-92.479464	-24.469602	1.846771
-92.263613	-22.005889	1.851776
-92.667728	-33.452136	1.856781
-92.619110	-19.352559	1.861786
-92.738764	-15.033113	1.866790
-92.939676	-12.141057	1.871795
-93.535634	-12.022540	1.876800
-94.016307	-12.213291	1.881805
-94.223779	-28.120247	1.886810
-93.887911	-15.258595	1.891814
-94.095117	-20.710927	1.896819
-94.644542	-28.179639	1.901824
-95.070165	-20.761774	1.906829
-95.188595	-30.109890	1.911834
-95.324800	-11.887939	1.916838
-95.514790	-27.455287	1.921843
-95.780868	-25.456353	1.926848
-96.849420	-4.794491	1.931853
-97.213324	-18.710480	1.936858
-97.045500	-17.894302	1.941862
-97.076008	-9.727016	1.946867
-97.160374	-33.641952	1.951872
-97.324248	-15.648534	1.956877
-97.313745	-6.709216	1.961882
-97.264351	-19.015248	1.966886
-98.371975	-2.367427	1.971891
-98.164924	-2.228227	1.976896
-98.931167	-10.720373	1.981901
-99.080378	-13.343069	1.986906
-99.102409	-16.104173	1.991910
-99.825940	-28.950289	1.996915
-100.119669	-14.872250	2.006912
-99.346260	-24.556263	2.016909
-99.381901	-23.430201	2.026906
-98.383384	-14.148768	2.036902
-97.972985	-21.210741	2.046899
-97.418174	-23.895002	2.056896
-96.236619	-18.539882	2.066893
-96.161359	-7.345249	2.076890
-96.152419	-26.444398	2.086886
-95.778245	-13.785292	2.096883
-94.930755	-16.094785	2.106880
-94.626213	-23.911758	2.116877
-93.924239	-11.016731	2.126874
-93.170703	-10.372326	2.136870
-93.136528	-5.673559	2.146867
-92.230431	-16.183610	2.156864
-91.981949	-12.277449	2.166861
-91.965712	-21.008223	2.176858
-90.756424	-6.454103	2.186854
-90.266108	-14.025024	2.196851
-90.112523	-10.544394	2.206848
-88.832059	-10.439745	2.216845
-88.956560	-6.423839	2.226842
-88.721128	-9.916612	2.236838
-87.902873	-11.687015	2.246835
-86.983903	-18.636877	2.256832
-86.741410	-22.911705	2.266829
-86.751461	-2.684193	2.276826
-86.332090	-17.223316	2.286822
-85.518605	-26.457525	2.296819
-84.453932	-7.285025	2.306816
-84.190732	-15.748350	2.316813
-83.929288	-27.307190	2.326810
-83.711839	-15.054901	2.336806
-83.199721	-26.210005	2.346803
-82.561585	-22.045554	2.356800
-81.380426	-20.729055	2.366797
-81.334481	-19.149975	2.376794
-80.951405	-22.166371	2.386790
-80.689347	-15.140567	2.396787
-79.708122	-17.544856	2.406784
-79.148114	-12.023203	2.416781
-79.082379	-16.444438	2.426778
-78.824446	-1.566158	2.436774
-77.788949	-17.749234	2.446771
-77.506873	-1.713287	2.456768
-76.414247	-20.021205	2.466765
-76.279341	-16.999150	2.476762
-76.297360	-16.677139	2.486758
-75.160317	-10.172554	2.496755
-74.472781	-23.565983	2.506752
-74.480453	-7.902925	2.516749
-74.174564	-18.023983	2.526746
-73.251693	-14.462080	2.536742
-73.273839	-21.958775	2.546739
-72.145527	-11.788699	2.556736
-71.500848	-15.233146	2.566733
-71.394864	-16.354144	2.576730
-71.220423	-25.578650	2.586726
-70.400858	-4.581219	2.596723
-69.467226	-26.886039	2.606720
-69.606576	-17.021564	2.616717
-68.467496	-11.616351	2.626714
-68.122018	-23.501203	2.636710
-68.020210	-13.175213	2.646707
-67.715484	-11.603934	2.656704
-66.932891	-24.106048	2.666701
-66.593824	-30.111320	2.676698
-65.382076	-16.448332	2.686694
-64.965472	-19.040907	2.696691
-64.647389	-20.110037	2.706688
-64.644128	-14.615196	2.716685
-64.010675	-15.080402	2.726682
-63.260522	-18.702289	2.736678
-63.294469	-18.875852	2.746675
-62.201067	-22.229307	2.756672
-61.686259	-12.097800	2.766669
-61.373449	-18.920124	2.776666
-60.973681	-20.615338	2.786662
-60.245381	-9.975470	2.796659
-60.048841	-28.360786	2.806656
-59.252354	-10.050687	2.816653
-58.749054	-17.649432	2.826650
-58.633671	-15.409683	2.836646
-58.057951	-15.358251	2.846643
-57.541257	-7.424828	2.856640
-56.388490	-12.398575	2.866637
-55.843338	-21.990344	2.876634
-55.781275	-7.401989	2.886630
-55.946523	-17.802644	2.896627
-55.125485	-13.313822	2.906624
-54.306959	-4.055667	2.916621
-53.815922	-11.920654	2.926618
-53.111011	-16.329389	2.936614
-52.551567	-11.099115	2.946611
-52.608555	-11.226695	2.956608
-51.534426	-23.335973	2.966605
-50.821288	-20.685840	2.976602
-50.922904	-19.400716	2.986598
-50.762424	-31.428829	2.996595
-49.888473	-21.678081	3.006592
-49.595122	-14.655667	3.016589
-48.315295	-25.597473	3.026586
-47.907650	-26.066053	3.036582
-48.020936	-12.540253	3.046579
-47.754856	-7.052888	3.056576
-46.668054	-23.604363	3.066573
-46.055284	-8.942957	3.076570
-46.138638	-15.182347	3.086566
-45.034219	-23.547735	3.096563
-44.666078	-16.605734	3.106560
-44.166417	-15.106672	3.116557
-44.116728	-22.383620	3.126554
-43.201323	-11.418300	3.136550
-42.605104	-11.002031	3.146547
-42.491126	-18.450604	3.156544
-41.544251	-18.051690	3.166541
-41.306728	-7.343155	3.176538
-41.200085	-9.433414	3.186534
-40.037519	-23.009949	3.196531
-39.666699	-13.392654	3.206528
-39.523349	-18.322750	3.216525
-38.546117	-34.147416	3.226522
-38.231459	-12.360720	3.236518
-37.987022	-7.642077	3.246515
-37.205222	-21.296142	3.256512
-36.459963	-19.242762	3.266509
-36.276588	-9.965377	3.276506
-36.054931	-19.347628	3.286502
-35.516296	-19.286608	3.296499
-34.802230	-17.940120	3.306496
-34.233317	-15.769295	3.316493
-33.477210	-10.620805	3.326490
-33.154864	-20.298825	3.336486
-32.846937	-3.009674	3.346483
-32.024716	-21.895960	3.356480
-31.676605	-5.993199	3.366477
-31.592203	-12.761582	3.376474
-30.928950	-21.085770	3.386470
-30.604103	-14.074385	3.396467
-29.707175	-16.907533	3.406464
-28.862920	-17.654699	3.416461
-28.578080	-22.632375	3.426458
-28.767622	-10.339287	3.436454
-27.765763	-4.846985	3.446451
-27.097775	-17.124622	3.456448
-26.907825	-19.072488	3.466445
-25.823690	-15.388673	3.476442
-25.601424	-10.637920	3.486438
-25.454922	-13.289866	3.496435
-25.102104	2.539333	3.506432
-24.107747	-20.554158	3.516429
-23.858722	-17.317264	3.526426
-23.093097	-6.047164	3.536422
-22.447304	-9.299681	3.546419
-22.018052	-22.579808	3.556416
-21.983986	-10.655743	3.566413
-21.442578	-17.607903	3.576410
-20.748274	-23.335464	3.586406
-20.262528	-18.560892	3.596403
-19.270113	-20.116100	3.606400
-18.909654	-15.845007	3.616397
-19.131851	-15.831204	3.626394
-18.460769	-12.591556	3.636390
-17.750805	-19.317133	3.646387
-17.344840	-6.252663	3.656384
-16.563985	-15.773949	3.666381
-15.972602	-16.525155	3.676378
-15.515249	-15.096239	3.686374
-15.681313	-7.046424	3.696371
-14.776364	-29.271440	3.706368
-13.697832	-7.702130	3.716365
-13.844294	-8.243398	3.726362
-13.463879	-31.630110	3.736358
-12.443924	-8.951493	3.746355
-12.365385	-10.021928	3.756352
-12.101300	-19.660690	3.766349
-10.717069	-13.051645	3.776346
-10.850509	-7.733530	3.786342
-10.327815	-14.431025	3.796339
-9.165436	-13.968452	3.806336
-8.517051	-12.430255	3.816333
-8.907884	-17.018232	3.826330
-9.009859	-18.108420	3.836326
-7.950294	-3.256716	3.846323
-7.202077	-9.968567	3.856320
-6.352893	-23.133287	3.866317
-5.846293	-18.861552	3.876314
-5.842242	-24.476922	3.886310
-5.519414	-19.451707	3.896307
-4.506461	-10.724078	3.906304
-4.606527	-0.952406	3.916301
-3.808773	-2.398304	3.926298
-3.385177	-0.641217	3.936294
-2.925441	14.185966	3.946291
-2.450098	24.242445	3.956288
-2.296491	28.771456	3.966285
-1.741884	51.184426	3.976282
-1.159162	81.230484	3.986278
-0.976937	92.310729	3.996275
-0.195055	128.376670	4.006272
0.000000	121.945263	4.011277
0.079066	146.515891	4.016282
0.170545	161.544232	4.021286
0.861452	148.317612	4.026291
0.216094	168.463598	4.031296
0.717076	173.004889	4.036301
0.839391	206.815620	4.041306
0.275342	197.385919	4.046310
0.550081	197.396549	4.051315
0.773770	206.379295	4.056320
1.026854	202.775813	4.061325
1.162535	220.489484	4.066330
0.921573	235.327992	4.071334
0.976526	232.209445	4.076339
0.747814	229.126923	4.081344
0.764769	232.776542	4.086349
1.035102	230.836753	4.091354
0.486069	219.104987	4.096358
1.001771	227.545464	4.101363
0.543035	259.529693	4.106368
0.937908	248.785543	4.111373
1.388571	266.623697	4.116378
1.253566	264.707186	4.121382
1.276432	276.335152	4.126387
1.095953	274.302055	4.131392
1.315660	257.045815	4.136397
1.685104	269.495552	4.141402
1.423885	286.586722	4.146406
1.437518	282.809614	4.151411
1.536215	262.300035	4.156416
0.931093	256.306274	4.161421
1.090960	268.688247	4.166426
0.719153	267.695540	4.171430
1.253466	268.386954	4.176435
1.119376	290.646087	4.181440
1.199207	271.880846	4.186445
0.832107	271.425090	4.191450
1.328071	284.530358	4.196454
1.576252	294.747828	4.201459
1.452389	299.912387	4.206464
1.599312	309.221185	4.211469
1.632635	307.241931	4.216474
1.625161	291.030291	4.221478
1.621716	275.105560	4.226483
1.194241	284.965608	4.231488
1.350987	284.182781	4.236493
2.188832	305.547777	4.241498
1.425406	299.761671	4.246502
1.681518	278.151980	4.251507
1.187950	288.780468	4.256512
1.458948	275.290490	4.261517
1.856079	295.637750	4.266522
1.550933	302.278544	4.271526
2.288875	298.954684	4.276531
1.524498	300.359771	4.281536
1.694648	276.712116	4.286541
1.462637	281.822923	4.291546
1.185124	281.744881	4.296550
1.603246	285.942202	4.301555
1.482136	305.469135	4.306560
1.804060	287.350951	4.311565
1.768907	302.851572	4.316570
1.640086	313.292152	4.321574
1.657757	300.840654	4.326579
1.336955	308.516979	4.331584
1.643763	312.983269	4.336589
1.604965	301.415517	4.341594
1.809326	298.784939	4.346598
1.721933	312.917672	4.351603
1.910272	309.639551	4.356608
1.822511	293.973875	4.361613
1.982238	319.670020	4.366618
1.989367	307.533960	4.371622
2.346597	308.136460	4.376627
2.209055	312.618272	4.381632
2.308905	283.012743	4.386637
2.082344	306.065510	4.391642
2.034720	315.539439	4.396646
2.101990	299.509676	4.401651
2.078409	305.147156	4.406656
2.338367	310.941885	4.411661
1.903063	289.845565	4.416666
1.568767	297.836730	4.421670
1.941799	310.283145	4.426675
1.952594	327.101730	4.431680
1.924487	299.974143	4.436685
1.969870	308.799279	4.441690
2.179205	314.290352	4.446694
2.216132	298.224962	4.451699
2.140573	315.834657	4.456704
1.947372	318.376188	4.461709
2.062394	312.753186	4.466714
1.654713	314.349994	4.471718
2.212844	314.425167	4.476723
2.074255	302.281426	4.481728
2.170844	317.237556	4.486733
2.674033	298.952678	4.491738
2.107190	313.877471	4.496742
2.312964	302.716967	4.501747
2.323337	311.866129	4.506752
2.321052	321.022814	4.511757
2.292768	306.625676	4.516762
1.925963	302.203730	4.521766
2.330815	307.657459	4.526771
1.964685	321.065821	4.531776
2.183748	306.703865	4.536781
2.456507	308.441161	4.541786
1.950256	320.389704	4.546790
2.599801	304.659588	4.551795
2.140425	319.395473	4.556800
2.177435	306.719211	4.561805
2.252247	323.996778	4.566810
2.497638	315.757098	4.571814
2.467714	317.584170	4.576819
2.273533	306.912562	4.581824
2.116357	298.646391	4.586829
2.689949	320.991048	4.591834
2.167167	319.322392	4.596838
2.415743	302.103453	4.601843
2.211368	324.130787	4.606848
2.412159	333.621089	4.611853
2.371417	311.897637	4.616858
2.373407	327.996858	4.621862
2.661959	347.984605	4.626867
2.410062	337.849097	4.631872
2.506732	342.777958	4.636877
2.667826	354.581917	4.641882
2.536549	347.014605	4.646886
2.817650	325.569406	4.651891
2.727748	347.975014	4.656896
2.861244	352.385710	4.661901
2.430138	322.370264	4.666906
2.380387	339.540487	4.671910
2.607875	338.615751	4.676915
2.518108	357.303303	4.681920
2.737473	338.651747	4.686925
2.420613	346.743636	4.691930
2.617889	350.375224	4.696934
2.749616	356.188398	4.701939
2.798254	358.165755	4.706944
2.533233	357.371434	4.711949
2.601016	346.636384	4.716954
2.851717	353.678191	4.721958
2.630464	362.934911	4.726963
2.432970	362.394203	4.731968
2.562933	341.163955	4.736973
2.921918	345.180083	4.741978
2.554937	359.875089	4.746982
2.920858	346.992128	4.751987
2.429570	361.191156	4.756992
2.562913	347.940099	4.761997
2.603698	370.442916	4.767002
2.837401	379.273670	4.772006
3.176570	369.220795	4.777011
2.947078	380.415354	4.782016
3.196908	377.273748	4.787021
3.001954	370.647595	4.792026
2.806650	357.523346	4.797030
2.689287	343.252859	4.802035
2.759106	371.290861	4.807040
2.754449	377.652082	4.812045
3.118559	387.644085	4.817050
2.979483	391.891785	4.822054
3.067904	377.049133	4.827059
3.333276	386.146040	4.832064
3.156503	387.121093	4.837069
3.232401	381.665920	4.842074
2.988070	378.277870	4.847078
3.088002	359.414004	4.852083
2.968453	380.088448	4.857088
2.792625	391.773801	4.862093
3.285417	372.948184	4.867098
2.732027	375.155442	4.872102
3.061305	393.507835	4.877107
2.985332	381.070957	4.882112
3.011016	386.832712	4.887117
3.217465	388.070569	4.892122
3.145201	383.432717	4.897126
3.265334	363.038036	4.902131
3.069265	380.467859	4.907136
3.100398	390.754999	4.912141
3.220746	387.608745	4.917146
2.786797	386.821129	4.922150
3.323213	371.555432	4.927155
3.020063	385.394400	4.932160
3.191796	373.090414	4.937165
3.459814	366.037259	4.942170
3.146139	392.626396	4.947174
3.183827	395.537795	4.952179
3.381234	404.086310	4.957184
3.397512	416.431265	4.962189
3.233872	408.371786	4.967194
3.106532	425.193675	4.972198
3.439987	407.821694	4.977203
3.442997	417.903280	4.982208
3.427088	423.737227	4.987213
3.639062	418.202634	4.992218
3.210964	425.484200	4.997222
3.342485	431.610153	5.002227
3.647966	416.364522	5.007232
3.415406	406.005194	5.012237
3.954246	421.259854	5.017242
3.533730	424.081445	5.022246
3.643137	412.270020	5.027251
3.236264	421.902424	5.032256
3.465252	408.481321	5.037261
3.474362	398.775266	5.042266
3.684559	416.382937	5.047270
3.939545	425.882196	5.052275
3.707829	419.036192	5.057280
3.559776	396.625508	5.062285
3.564598	402.362799	5.067290
3.193473	416.944902	5.072294
3.419390	412.331457	5.077299
3.081375	423.397389	5.082304
3.315797	409.412695	5.087309
3.449028	417.740986	5.092314
3.187141	415.390653	5.097318
3.589618	411.027503	5.102323
3.680871	426.721330	5.107328
3.739346	417.948213	5.112333
3.791339	435.931267	5.117338
3.710516	454.167227	5.122342
3.795107	424.996717	5.127347
3.446852	428.250878	5.132352
3.227399	444.365803	5.137357
3.651078	432.482206	5.142362
3.227930	450.157387	5.147366
3.803698	444.607749	5.152371
3.333962	437.331601	5.157376
3.579178	437.028081	5.162381
3.884829	447.086901	5.167386
4.051210	468.774985	5.172390
4.080757	445.996909	5.177395
3.669405	460.177196	5.182400
3.622036	467.666262	5.187405
3.868248	465.214890	5.192410
3.600876	490.984862	5.197414
4.045634	481.994475	5.202419
3.659301	486.704392	5.207424
3.561777	489.025641	5.212429
3.788815	492.300166	5.217434
3.798176	482.534433	5.222438
3.808726	499.085021	5.227443
3.652444	496.171497	5.232448
3.902745	479.216651	5.237453
4.356676	489.880179	5.242458
4.061972	480.693650	5.247462
4.258317	475.514388	5.252467
4.065928	509.733621	5.257472
3.823365	479.701605	5.262477
4.037936	497.073665	5.267482
4.050532	512.760750	5.272486
4.405610	504.807472	5.277491
4.192073	500.773184	5.282496
3.941219	505.030707	5.287501
3.963494	501.259120	5.292506
3.913343	512.644028	5.297510
4.205149	527.385404	5.302515
4.046723	501.837951	5.307520
4.129015	506.825175	5.312525
4.301138	501.281156	5.317530
4.282128	533.223378	5.322534
4.338724	518.988792	5.327539
4.400719	508.717251	5.332544
3.922684	498.674644	5.337549
4.285910	513.206414	5.342554
4.359334	531.949978	5.347558
4.542133	508.951750	5.352563
4.297700	504.438003	5.357568
4.266954	504.953593	5.362573
4.583128	519.200943	5.367578
4.409328	520.141874	5.372582
4.433288	514.137770	5.377587
4.331360	523.131007	5.382592
4.173498	513.984092	5.387597
4.567550	510.248040	5.392602
4.495379	525.278724	5.397606
4.978242	537.160658	5.402611
4.487883	523.742020	5.407616
4.454039	506.263612	5.412621
4.845239	516.436583	5.417626
4.268852	504.271018	5.422630
4.587314	502.591074	5.427635
4.294209	514.945406	5.432640
4.499743	530.353707	5.437645
4.910490	513.784564	5.442650
4.517215	501.530439	5.447654
4.485859	507.124787	5.452659
4.611347	518.877835	5.457664
4.326216	518.512204	5.462669
4.531981	504.173670	5.467674
4.525563	509.049184	5.472678
4.516159	516.530717	5.477683
4.584568	519.226446	5.482688
5.056785	516.565280	5.487693
5.196789	530.289616	5.492698
4.648375	513.764839	5.497702
4.797771	515.816125	5.502707
4.685203	515.366834	5.507712
4.597805	491.481443	5.512717
4.753621	509.686551	5.517722
4.634716	536.412638	5.522726
4.738460	509.218598	5.527731
4.677848	523.031814	5.532736
4.659333	525.146462	5.537741
4.776005	524.694210	5.542746
4.927295	516.206579	5.547750
4.904648	505.728842	5.552755
4.482220	518.474384	5.557760
4.458249	524.701142	5.562765
4.954826	500.786611	5.567770
4.675532	517.458312	5.572774
4.526273	518.282826	5.577779
4.971141	519.673364	5.582784
4.477823	511.375915	5.587789
5.054157	543.956983	5.592794
4.998569	549.839857	5.597798
5.389171	536.315580	5.602803
5.177587	541.461076	5.607808
4.890512	514.323027	5.612813
4.652557	508.940392	5.617818
4.890127	518.626862	5.622822
4.964050	528.626564	5.627827
5.120438	537.978231	5.632832
4.933393	539.495688	5.637837
5.305604	552.237694	5.642842
4.961394	554.153033	5.647846
5.335272	547.754006	5.652851
5.063709	563.894931	5.657856
5.114207	556.024711	5.662861
5.188299	536.372249	5.667866
5.162896	556.271476	5.672870
5.228036	539.957112	5.677875
5.083805	546.582073	5.682880
5.014218	560.893211	5.687885
5.257866	535.490368	5.692890
5.117918	533.388981	5.697894
5.287914	539.377120	5.702899
5.383147	553.834934	5.707904
4.876641	537.717732	5.712909
5.109529	538.203272	5.717914
4.773877	560.701790	5.722918
5.036681	543.658785	5.727923
5.265930	541.030071	5.732928
4.721665	552.728389	5.737933
5.009877	560.775151	5.742938
5.059276	567.031237	5.747942
5.022074	560.393334	5.752947
5.192751	572.378874	5.757952
5.179737	573.188768	5.762957
5.360061	580.462989	5.767962
5.453146	574.531192	5.772966
4.960593	570.823159	5.777971
5.475924	592.308442	5.782976
5.149577	577.700559	5.787981
5.610550	594.315321	5.792986
5.207630	589.962001	5.797990
5.141614	565.949647	5.802995
5.571515	589.380898	5.808000
5.460941	584.633107	5.813005
5.475347	581.600306	5.818010
5.485147	606.636785	5.823014
5.781438	584.551338	5.828019
5.869480	563.892674	5.833024
5.554575	574.764701	5.838029
5.342852	583.636725	5.843034
5.063442	594.731371	5.848038
5.235117	567.820175	5.853043
5.271972	582.219003	5.858048
5.589725	598.550933	5.863053
5.580975	592.579628	5.868058
5.860668	604.908728	5.873062
5.729450	618.657542	5.878067
5.383681	589.699794	5.883072
5.346995	621.262754	5.888077
5.815249	621.733671	5.893082
5.577663	612.594939	5.898086
5.553336	604.023031	5.903091
5.460679	607.915478	5.908096
5.508565	613.909028	5.913101
5.862867	617.041606	5.918106
5.720226	623.173975	5.923110
5.789037	630.375002	5.928115
5.860301	619.480852	5.933120
5.828222	615.624995	5.938125
5.788410	622.526710	5.943130
5.568872	616.079815	5.948134
5.907614	613.072133	5.953139
6.104952	622.368549	5.958144
5.691105	637.445153	5.963149
5.564550	612.814427	5.968154
5.828064	614.189170	5.973158
5.694698	613.297415	5.978163
5.739552	602.797012	5.983168
5.916667	619.407905	5.988173
6.022567	627.610116	5.993178
5.660139	615.585587	5.998182
5.789555	604.133740	6.003187
5.830675	616.863826	6.008192
5.688780	645.832270	6.013197
6.340468	645.409094	6.018202
5.799657	662.732447	6.023206
5.996730	650.063189	6.028211
6.134341	644.728041	6.033216
6.201496	653.479441	6.038221
5.799216	627.705226	6.043226
5.257667	645.189776	6.048230
5.532106	645.028313	6.053235
5.698805	639.396751	6.058240
5.910200	665.739385	6.063245
5.918679	651.557415	6.068250
5.650970	656.104342	6.073254
5.799672	645.468172	6.078259
5.985803	638.514053	6.083264
5.810410	632.600260	6.088269
6.143836	644.038088	6.093274
5.633781	668.124453	6.098278
5.846705	650.290998	6.103283
6.465315	645.667144	6.108288
6.056202	651.972298	6.113293
6.215084	655.628652	6.118298
6.149906	646.003476	6.123302
6.109319	633.630094	6.128307
5.829335	633.130333	6.133312
5.843960	653.092916	6.138317
5.995533	640.024549	6.143322
5.534144	655.240133	6.148326
6.040128	671.078267	6.153331
6.304529	643.950564	6.158336
5.702983	656.796257	6.163341
6.208777	650.875840	6.168346
5.985442	650.499797	6.173350
5.896124	652.207393	6.178355
6.104914	657.573196	6.183360
5.824352	660.185845	6.188365
5.799488	648.913255	6.193370
6.103116	638.399068	6.198374
5.856142	651.151931	6.203379
6.081217	659.642845	6.208384
5.959373	660.465598	6.213389
5.828732	647.137947	6.218394
5.894074	649.689980	6.223398
5.933987	655.941552	6.228403
6.242375	668.250671	6.233408
6.117975	678.377849	6.238413
6.323951	663.083899	6.243418
5.751377	652.485036	6.248422
6.005966	662.589135	6.253427
6.115966	642.851188	6.258432
6.141554	654.830581	6.263437
6.402799	653.252512	6.268442
6.024702	641.003460	6.273446
6.406984	644.882147	6.278451
6.270936	664.348968	6.283456
6.272014	654.990241	6.288461
6.278036	647.726130	6.293466
6.023878	644.204000	6.298470
6.214275	632.064526	6.303475
6.046967	630.196910	6.308480
5.679519	638.879051	6.313485
5.773690	627.148010	6.318490
5.623705	633.223197	6.323494
5.996131	652.032918	6.328499
6.071976	628.127933	6.333504
5.851054	651.255162	6.338509
5.828690	648.656862	6.343514
5.990804	642.942598	6.348518
5.927127	652.452041	6.353523
6.000463	659.508403	6.358528
6.240894	638.980226	6.363533
6.132529	637.913377	6.368538
6.224680	658.000673	6.373542
6.310919	655.412442	6.378547
6.320683	649.829104	6.383552
5.836685	644.659026	6.388557
6.118752	618.562696	6.393562
5.836609	630.920243	6.398566
5.617182	611.522170	6.403571
6.005470	629.304961	6.408576
6.076208	654.356308	6.413581
6.241784	637.966052	6.418586
5.944359	647.595899	6.423590
5.954947	641.081764	6.428595
6.122477	621.090772	6.433600
5.907684	634.931936	6.438605
6.096293	624.542420	6.443610
5.943671	606.494683	6.448614
5.978411	621.223487	6.453619
5.791884	631.220720	6.458624
5.451895	630.252719	6.463629
6.060649	620.747721	6.468634
5.858948	642.552911	6.473638
6.088790	656.922187	6.478643
6.458501	652.367380	6.483648
6.152458	654.923963	6.488653
6.459167	649.008134	6.493658
6.291883	622.818742	6.498662
6.257113	611.856886	6.503667
6.441100	625.724973	6.508672
6.563238	635.207448	6.513677
6.310860	623.874809	6.518682
6.139187	614.561228	6.523686
5.779951	607.286171	6.528691
6.013403	615.225408	6.533696
6.080874	614.871351	6.538701
5.927478	621.641493	6.543706
6.141892	625.196129	6.548710
5.980087	598.055185	6.553715
5.932914	595.022101	6.558720
5.795532	595.103796	6.563725
6.083077	588.824574	6.568730
6.043662	615.895762	6.573734
6.091115	617.753193	6.578739
6.131672	596.506981	6.583744
6.016552	586.822717	6.588749
6.125507	588.160060	6.593754
5.570590	578.927392	6.598758
5.797342	592.225289	6.603763
6.407445	602.726854	6.608768
6.082376	593.848721	6.613773
5.988514	587.423982	6.618778
6.107653	585.153897	6.623782
5.837654	569.845076	6.628787
5.852887	563.643614	6.633792
5.695519	587.297098	6.638797
5.958427	595.022023	6.643802
5.718719	609.228834	6.648806
6.044431	618.294698	6.653811
6.350830	617.002161	6.658816
5.993773	605.785879	6.663821
6.255242	600.673747	6.668826
6.021222	589.325670	6.673830
5.940257	581.253720	6.678835
5.859987	585.549861	6.683840
5.683360	590.133311	6.688845
6.039986	592.940646	6.693850
5.747188	608.343183	6.698854
5.917503	615.445845	6.703859
6.026655	619.679619	6.708864
5.588673	619.240792	6.713869
5.779526	615.355987	6.718874
5.765517	607.766799	6.723878
5.620766	607.829390	6.728883
5.961964	602.059800	6.733888
5.895039	607.545234	6.738893
5.948037	610.905763	6.743898
5.901426	619.801229	6.748902
5.727115	611.290800	6.753907
5.724783	617.002915	6.758912
5.675961	620.621669	6.763917
5.658129	629.370033	6.768922
5.866699	644.015382	6.773926
6.054727	642.493411	6.778931
6.027193	628.236126	6.783936
6.020708	656.539016	6.788941
6.200497	635.866772	6.793946
6.130806	652.571954	6.798950
6.477072	652.545413	6.803955
6.863166	621.891220	6.808960
6.214534	627.791921	6.813965
6.552619	616.514720	6.818970
6.211307	618.826949	6.823974
6.096071	622.099763	6.828979
5.992619	626.370644	6.833984
5.990875	620.009293	6.838989
6.305133	595.944507	6.843994
6.219198	599.876584	6.848998
5.916830	575.457770	6.854003
5.858639	586.561824	6.859008
5.725456	591.145396	6.864013
6.030502	574.645447	6.869018
5.893484	602.294451	6.874022
5.876332	602.023729	6.879027
6.135324	603.220959	6.884032
6.022435	597.186166	6.889037
6.097097	600.634659	6.894042
5.803913	593.295917	6.899046
5.898596	583.982632	6.904051
6.174789	611.840477	6.909056
5.883328	606.364249	6.914061
6.109761	599.376358	6.919066
5.890411	596.157952	6.924070
5.859662	579.423162	6.929075
5.601465	603.748760	6.934080
5.556469	630.009501	6.939085
5.904673	626.404999	6.944090
6.148938	623.713712	6.949094
6.135765	627.319079	6.954099
6.054492	617.478267	6.959104
5.982212	614.779608	6.964109
6.263947	628.808227	6.969114
6.401780	630.486570	6.974118
6.039958	607.638271	6.979123
6.134872	583.596927	6.984128
5.779425	591.031310	6.989133
5.959029	598.439625	6.994138
6.090454	591.292927	6.999142
5.765965	599.432377	7.004147
6.227632	586.238726	7.009152
5.532657	589.186200	7.014157
5.629455	593.286266	7.019162
5.655156	597.744440	7.024166
5.840484	612.456440	7.029171
5.985886	607.139649	7.034176
5.763046	608.888443	7.039181
5.714482	622.341463	7.044186
5.828328	620.422257	7.049190
5.824918	611.472413	7.054195
5.919161	592.601506	7.059200
5.688876	616.815773	7.064205
6.030151	612.527099	7.069210
6.302453	618.161572	7.074214
5.954919	627.345701	7.079219
6.285598	609.714501	7.084224
6.022091	606.617922	7.089229
6.076366	614.753486	7.094234
6.071906	615.063391	7.099238
6.150912	607.777373	7.104243
6.319275	619.754650	7.109248
6.240288	614.118417	7.114253
6.301484	608.891994	7.119258
6.347443	617.167537	7.124262
6.100386	623.655925	7.129267
6.350515	601.535465	7.134272
5.746567	600.448116	7.139277
5.873446	571.751355	7.144282
5.973078	586.894483	7.149286
5.728674	589.682069	7.154291
6.255683	586.765804	7.159296
6.040367	608.110725	7.164301
6.065690	587.260262	7.169306
5.754243	591.933962	7.174310
5.709086	587.762818	7.179315
6.119967	609.657914	7.184320
6.048723	625.841269	7.189325
6.473040	591.911263	7.194330
6.213848	592.181482	7.199334
5.931553	599.658236	7.204339
6.115769	596.882370	7.209344
6.203962	587.179601	7.214349
6.128525	580.637090	7.219354
6.127470	586.651443	7.224358
5.901706	580.690060	7.229363
6.153241	584.875928	7.234368
6.145827	595.093813	7.239373
5.887402	575.351431	7.244378
5.939400	589.813071	7.249382
5.973715	601.351297	7.254387
6.152541	578.623329	7.259392
5.683758	588.426374	7.264397
6.041224	600.505760	7.269402
5.801959	591.994041	7.274406
5.501943	589.255185	7.279411
5.788659	583.273629	7.284416
5.628694	597.760044	7.289421
5.719323	584.685616	7.294426
5.986953	622.960533	7.299430
6.040001	617.937292	7.304435
6.230901	606.313398	7.309440
6.110018	621.337627	7.314445
6.252258	604.515625	7.319450
6.070081	595.140458	7.324454
5.925017	589.286877	7.329459
6.109334	595.945168	7.334464
5.828125	591.551412	7.339469
5.789471	566.022531	7.344474
5.527375	572.931164	7.349478
5.700812	606.298891	7.354483
5.847201	606.834932	7.359488
5.571433	608.897004	7.364493
6.117609	606.016239	7.369498
6.278923	624.520570	7.374502
6.035057	630.327750	7.379507
6.374022	612.604320	7.384512
6.379020	625.424728	7.389517
6.204264	602.889318	7.394522
6.118861	593.872832	7.399526
5.852673	593.239885	7.404531
5.911423	572.548071	7.409536
5.899179	585.290896	7.414541
5.944907	607.335707	7.419546
5.989597	591.971212	7.424550
5.917802	594.609330	7.429555
5.958407	590.545254	7.434560
5.779675	577.869103	7.439565
5.937867	576.819076	7.444570
6.038222	606.842327	7.449574
6.136275	624.696947	7.454579
6.159760	595.767347	7.459584
5.820599	591.627819	7.464589
5.943589	597.261408	7.469594
6.042568	589.747966	7.474598
5.848809	593.449755	7.479603
5.998470	616.507900	7.484608
5.856261	620.388316	7.489613
6.158371	609.935562	7.494618
6.418406	609.553433	7.499622
5.926392	606.623452	7.504627
6.187871	586.158258	7.509632
5.635293	594.151022	7.514637
5.472446	602.780095	7.519642
5.859848	599.218447	7.524646
5.901179	630.161245	7.529651
6.507197	617.135588	7.534656
5.890942	616.161253	7.539661
6.178999	611.664344	7.544666
6.221126	605.615078	7.549670
5.841516	602.368601	7.554675
6.320353	597.030550	7.559680
6.060400	601.328766	7.564685
5.896518	590.756817	7.569690
6.152772	602.811202	7.574694
5.847242	599.160745	7.579699
5.946379	578.625712	7.584704
5.761840	586.890497	7.589709
5.757548	596.850588	7.594714
5.731181	590.412031	7.599718
5.626636	617.109447	7.604723
6.299805	615.771395	7.609728
6.155241	630.888529	7.614733
6.329817	608.210248	7.619738
6.049973	590.882981	7.624742
6.050017	594.914197	7.629747
6.146788	583.077205	7.634752
5.945608	599.938815	7.639757
5.717903	592.763369	7.644762
6.236984	583.007253	7.649766
5.865488	578.970439	7.654771
6.077734	592.519233	7.659776
6.149191	599.225770	7.664781
5.893923	580.770831	7.669786
5.806520	592.997221	7.674790
5.748859	589.558053	7.679795
6.108664	590.106277	7.684800
5.908354	594.784696	7.689805
5.930333	588.906472	7.694810
6.231504	578.599107	7.699814
5.965051	603.292355	7.704819
6.033121	587.011490	7.709824
5.676880	587.980995	7.714829
5.702793	596.271972	7.719834
5.961116	603.275346	7.724838
5.944987	625.738717	7.729843
6.156539	612.859340	7.734848
5.817917	619.725100	7.739853
6.126255	634.345667	7.744858
6.246815	616.502359	7.749862
5.907720	621.847017	7.754867
5.743676	599.378996	7.759872
5.996904	616.337675	7.764877
5.951859	622.860354	7.769882
6.137134	617.521779	7.774886
6.035394	608.655071	7.779891
6.031354	602.257014	7.784896
5.859856	608.655667	7.789901
5.935387	622.291201	7.794906
5.982362	608.576133	7.799910
5.999668	631.186402	7.804915
6.208930	638.392239	7.809920
5.803523	618.634532	7.814925
6.145900	602.450772	7.819930
6.114291	601.397482	7.824934
5.720096	598.522465	7.829939
5.907788	593.035820	7.834944
5.830485	622.233658	7.839949
6.028503	616.119463	7.844954
6.091122	623.117107	7.849958
6.101822	636.564687	7.854963
6.009994	612.039698	7.859968
6.075424	606.150735	7.864973
5.909929	606.648741	7.869978
6.111803	600.444440	7.874982
5.705640	593.655103	7.879987
6.090001	623.459507	7.884992
6.088652	625.765673	7.889997
6.228184	598.029299	7.895002
5.844043	586.310447	7.900006
5.519663	601.953772	7.905011
6.051875	612.561242	7.910016
5.908758	614.302189	7.915021
5.744513	617.700790	7.920026
5.892411	626.814293	7.925030
5.848555	621.631467	7.930035
5.857891	632.032268	7.935040
5.898982	623.398833	7.940045
6.075272	627.838642	7.945050
6.506771	624.247209	7.950054
6.326709	626.686095	7.955059
6.143751	627.121978	7.960064
5.902254	598.025741	7.965069
5.888175	601.726054	7.970074
6.347861	604.315509	7.975078
6.112755	592.695632	7.980083
6.258313	581.711200	7.985088
5.982696	602.714491	7.990093
6.068808	586.578422	7.995098
6.061057	589.638338	8.000102
5.785006	588.931751	8.005107
5.806845	583.903912	8.010112
6.033628	594.436276	8.015130
6.133485	581.410074	8.020147
6.156469	598.803352	8.025165
5.934917	597.549964	8.030182
5.816871	586.400403	8.035200
5.711189	595.080539	8.040218
5.881684	584.347146	8.045235
6.124128	593.362263	8.050253
5.852232	595.402413	8.055270
5.839383	596.013030	8.060288
5.981857	625.186696	8.065306
5.855217	627.056921	8.070323
6.390885	612.501888	8.075341
6.142661	632.537833	8.080358
6.269933	604.425967	8.085376
5.913715	593.034144	8.090394
5.651832	604.444767	8.095411
5.692143	618.851476	8.100429
5.965518	616.697528	8.105446
6.157898	609.138863	8.110464
6.045671	621.680061	8.115482
6.153268	634.534848	8.120499
6.471494	630.720098	8.125517
6.157559	631.435083	8.130534
6.621256	620.750823	8.135552
6.224205	620.868785	8.140570
5.944988	597.347573	8.145587
6.159735	597.333340	8.150605
5.948362	601.692966	8.155622
6.243507	622.967580	8.160640
5.897161	623.072341	8.165658
5.929969	632.273164	8.170675
6.348511	614.787600	8.175693
6.401689	609.061188	8.180710
6.147114	627.247010	8.185728
6.155441	610.752511	8.190746
5.673114	612.590986	8.195763
5.799135	626.851981	8.200781
5.729180	637.177263	8.205798
5.774497	607.347517	8.210816
5.966710	612.151927	8.215834
5.887765	628.130585	8.220851
5.744299	625.535619	8.225869
5.777642	640.619693	8.230886
5.902957	661.368245	8.235904
5.984239	653.538134	8.240922
5.912258	638.885513	8.245939
5.977826	661.238484	8.250957
5.602015	677.940478	8.255974
5.875095	658.065577	8.260992
6.146178	675.320824	8.266010
6.264339	685.237397	8.271027
6.007506	678.158728	8.276045
6.193198	698.581099	8.281062
6.457351	707.850698	8.286080
6.327380	695.645929	8.291098
6.473532	707.134338	8.296115
6.689690	689.684888	8.301133
6.322887	664.688093	8.306150
6.341236	662.969089	8.311168
6.205559	647.298032	8.316186
5.690256	661.489890	8.321203
6.418533	681.470014	8.326221
6.207688	697.459716	8.331238
6.269046	679.658893	8.336256
6.090813	695.957490	8.341274
6.412999	686.779046	8.346291
6.575260	680.872026	8.351309
6.614422	705.306719	8.356326
6.394538	686.864851	8.361344
6.357606	703.568632	8.366362
6.624577	695.819300	8.371379
6.696469	658.233802	8.376397
6.361220	670.845449	8.381414
6.649790	648.218548	8.386432
6.868665	657.887126	8.391450
6.599681	664.118974	8.396467
6.531666	659.073415	8.401485
6.546510	647.686159	8.406502
6.625695	652.593981	8.411520
6.729118	662.530884	8.416538
6.597858	649.090086	8.421555
6.666611	663.750335	8.426573
6.551107	657.670681	8.431590
6.706879	641.836440	8.436608
6.259167	621.502313	8.441626
6.371649	632.693163	8.446643
6.674675	617.168085	8.451661
6.410706	629.188353	8.456678
6.171885	638.481889	8.461696
6.251979	630.221592	8.466714
6.345561	656.023806	8.471731
6.580658	641.750439	8.476749
6.272405	636.724907	8.481766
6.542296	644.313170	8.486784
6.898571	663.166484	8.491802
6.305421	643.594646	8.496819
6.404058	635.286215	8.501837
6.542190	657.969912	8.506854
6.499858	657.039170	8.511872
6.699427	642.413207	8.516890
6.278941	655.090192	8.521907
6.680302	673.197981	8.526925
6.499582	654.698611	8.531942
6.471352	646.424620	8.536960
6.396162	662.131014	8.541978
6.411801	670.573782	8.546995
6.651515	670.021217	8.552013
6.286416	651.686831	8.557030
6.166720	650.047022	8.562048
6.578405	657.611958	8.567066
6.431326	678.658628	8.572083
6.603709	660.920757	8.577101
6.251415	671.311021	8.582119
6.182382	667.171681	8.587136
6.603074	658.539225	8.592154
6.109051	656.742829	8.597171
6.447489	654.175182	8.602189
6.549427	671.779155	8.607207
6.927984	676.633183	8.612224
6.867512	678.007474	8.617242
6.309242	673.156280	8.622259
6.544114	659.860523	8.627277
6.896708	680.147248	8.632295
6.477298	671.114388	8.637312
6.610395	672.105998	8.642330
6.780148	689.587594	8.647347
7.024485	663.227256	8.652365
6.519056	682.216891	8.657383
6.500250	686.117276	8.662400
6.667190	667.065887	8.667418
6.083741	682.836909	8.672435
6.645378	686.623466	8.677453
7.002915	696.234419	8.682471
6.589765	704.169479	8.687488
6.908931	699.886769	8.692506
6.998332	704.296005	8.697523
7.044146	685.824696	8.702541
6.889130	684.154510	8.707559
6.857240	665.171798	8.712576
6.858966	667.603237	8.717594
6.826258	665.158026	8.722611
6.576147	653.630544	8.727629
6.655440	670.167682	8.732647
6.558677	672.984294	8.737664
6.648955	675.109053	8.742682
6.467962	661.802806	8.747699
6.765649	676.041284	8.752717
7.136386	695.611838	8.757735
6.703976	679.183407	8.762752
6.687610	677.473876	8.767770
6.492407	661.795816	8.772787
6.854132	687.688086	8.777805
7.039784	682.357949	8.782823
6.978660	694.600092	8.787840
6.934685	673.846812	8.792858
6.562052	670.750385	8.797875
6.752757	694.415534	8.802893
6.740155	683.497426	8.807911
6.531867	690.512644	8.812928
6.935420	699.246249	8.817946
6.666570	697.625278	8.822963
6.668635	720.897050	8.827981
6.913478	696.957479	8.832999
6.840339	705.730404	8.838016
7.034912	706.324559	8.843034
6.875848	690.071949	8.848051
6.917954	710.364857	8.853069
7.094215	701.733311	8.858087
6.779836	697.063302	8.863104
7.280813	697.466212	8.868122
6.611683	700.904535	8.873139
6.616629	704.195650	8.878157
6.724893	700.741476	8.883175
6.756722	709.513784	8.888192
6.704728	708.879931	8.893210
6.548239	701.792540	8.898227
6.775370	693.852110	8.903245
6.846097	702.334007	8.908263
6.744998	707.257273	8.913280
6.871212	698.916305	8.918298
7.230976	729.057239	8.923315
7.108715	714.730290	8.928333
6.819230	702.303812	8.933351
6.718306	729.272240	8.938368
6.966968	728.868056	8.943386
6.400317	715.360505	8.948403
7.110880	741.786795	8.953421
7.145232	728.251747	8.958439
7.127965	735.556986	8.963456
7.066736	722.460854	8.968474
7.312260	738.923364	8.973491
7.165172	735.758952	8.978509
7.246850	730.834951	8.983527
7.097160	729.382227	8.988544
7.046017	723.314642	8.993562
7.012776	736.336844	8.998579
7.099949	731.692569	9.003597
7.365898	730.912990	9.008615
6.952115	725.463449	9.013632
7.401182	711.132716	9.018650
7.288385	712.745221	9.023667
6.947461	712.279651	9.028685
6.912001	699.980542	9.033703
7.217461	702.759423	9.038720
6.944748	708.265821	9.043738
6.879875	715.033591	9.048755
7.308940	715.390624	9.053773
7.243821	727.950102	9.058791
6.941004	743.690555	9.063808
7.476830	729.219713	9.068826
7.146347	739.387185	9.073843
7.144303	737.651174	9.078861
6.968644	733.475120	9.083879
7.065304	738.678920	9.088896
6.882001	734.292276	9.093914
7.132539	734.232474	9.098931
7.138483	721.667912	9.103949
7.190605	735.391466	9.108967
6.967026	752.824187	9.113984
7.369518	733.524791	9.119002
7.330492	742.883182	9.124019
7.117400	749.527371	9.129037
7.418795	730.100826	9.134055
7.161520	735.800890	9.139072
7.148398	745.112494	9.144090
7.020578	741.439125	9.149107
7.298568	731.658867	9.154125
7.313505	744.671245	9.159143
6.933856	744.554503	9.164160
7.205340	736.025675	9.169178
7.580475	734.909338	9.174195
7.371029	740.171889	9.179213
7.255268	735.756667	9.184231
7.315218	744.950613	9.189248
7.348985	736.445029	9.194266
7.310922	757.092298	9.199283
7.423832	741.819417	9.204301
7.212053	726.075150	9.209319
7.007886	736.406737	9.214336
7.388837	739.227565	9.219354
7.476613	738.770166	9.224371
7.059665	738.433958	9.229389
7.283057	743.808695	9.234407
7.158929	750.158335	9.239424
7.153703	732.208261	9.244442
7.406105	738.887302	9.249459
7.339831	764.669180	9.254477
7.301708	754.172451	9.259495
7.436917	755.470427	9.264512
7.492587	762.542819	9.269530
7.362947	750.153552	9.274547
7.194128	772.902312	9.279565
7.601613	755.600946	9.284583
7.260586	780.788659	9.289600
7.608844	762.388998	9.294618
7.906165	768.578179	9.299635
7.690848	746.082519	9.304653
7.560095	742.390152	9.309671
7.162853	733.232955	9.314688
7.341273	746.508202	9.319706
7.197494	740.561894	9.324723
7.658361	757.116461	9.329741
7.684276	754.452254	9.334759
7.435972	728.392741	9.339776
7.410835	729.136954	9.344794
7.697453	740.705003	9.349811
7.287753	734.487174	9.354829
7.727244	745.821850	9.359847
7.476290	750.230272	9.364864
7.870170	746.531108	9.369882
7.806684	739.084820	9.374899
7.424073	727.200835	9.379917
7.455456	745.892151	9.384935
7.345518	745.721294	9.389952
7.672313	746.456157	9.394970
7.577644	727.294029	9.399987
7.268290	741.463734	9.405005
7.415572	751.880031	9.410023
7.359378	781.511613	9.415040
7.326594	772.489094	9.420058
7.841151	760.604521	9.425075
7.644440	774.617786	9.430093
7.724873	780.185898	9.435111
7.648117	786.472031	9.440128
7.812052	769.743532	9.445146
7.837271	772.596485	9.450163
7.507411	782.775592	9.455181
7.861930	770.826341	9.460199
8.201210	767.944150	9.465216
7.374241	760.331773	9.470234
7.434079	752.484295	9.475251
7.258844	772.205094	9.480269
7.624473	784.218955	9.485287
7.750850	776.269449	9.490304
7.570249	766.192708	9.495322
7.718825	770.505101	9.500339
7.544610	790.274660	9.505357
7.501457	767.321104	9.510375
7.636913	773.981996	9.515392
7.382500	779.807653	9.520410
7.664436	771.378429	9.525427
7.434786	760.400785	9.530445
7.874234	781.363562	9.535463
7.635772	785.649391	9.540480
7.636010	785.874194	9.545498
7.875557	775.377124	9.550515
7.459632	775.083747	9.555533
7.494729	767.431441	9.560551
7.669845	793.044377	9.565568
7.701505	822.472396	9.570586
8.176889	816.078457	9.575603
7.880562	805.727583	9.580621
8.195458	806.007054	9.585639
8.032838	789.403049	9.590656
7.589393	768.974345	9.595674
7.936570	772.611274	9.600691
7.591868	788.385852	9.605709
7.671507	772.846562	9.610727
7.108578	767.402268	9.615744
6.999727	799.688542	9.620762
7.488771	804.147778	9.625779
7.608254	808.875710	9.630797
7.503540	816.726698	9.635815
7.493983	837.847685	9.640832
7.819375	839.751378	9.645850
8.011312	839.240946	9.650867
7.939283	838.045485	9.655885
7.823177	834.790522	9.660903
7.844632	848.444952	9.665920
7.683374	847.945752	9.670938
8.015736	845.982465	9.675955
7.855992	859.444170	9.680973
8.056355	835.967718	9.685991
8.439728	840.858788	9.691008
7.862236	854.607970	9.696026
7.977386	850.920401	9.701043
7.609060	849.581827	9.706061
7.731540	851.681315	9.711079
7.985468	842.024322	9.716096
8.032796	832.732394	9.721114
8.197108	851.131077	9.726131
8.126367	851.491299	9.731149
8.105052	839.112102	9.736167
8.102443	860.224101	9.741184
7.999938	845.285457	9.746202
8.379249	829.559024	9.751219
8.319136	849.193889	9.756237
8.259217	833.154801	9.761255
8.235989	848.217137	9.766272
7.737929	858.268225	9.771290
8.129274	847.891554	9.776307
7.972117	838.627806	9.781325
8.305664	840.926112	9.786343
8.163270	852.322487	9.791360
8.072466	862.999897	9.796378
8.385844	836.575208	9.801395
8.128076	850.668791	9.806413
8.095648	851.942228	9.811431
8.144840	845.244885	9.816448
8.169306	865.811119	9.821466
8.342743	844.567762	9.826483
8.089089	848.922735	9.831501
8.524238	862.058832	9.836519
8.484076	856.245219	9.841536
8.113084	842.688691	9.846554
8.172491	838.043757	9.851571
8.485390	855.690914	9.856589
8.139559	825.685482	9.861607
8.147164	808.692988	9.866624
8.130445	833.653914	9.871642
8.267128	856.624389	9.876659
8.275085	855.034213	9.881677
8.408178	848.383126	9.886695
8.200472	845.908453	9.891712
7.992055	837.817638	9.896730
8.461447	844.648024	9.901747
8.277123	842.123044	9.906765
8.286478	836.502089	9.911783
8.400762	846.240616	9.916800
8.127853	868.932821	9.921818
8.169658	848.886203	9.926835
8.118679	845.755971	9.931853
7.947327	846.526123	9.936871
7.935236	847.582769	9.941888
7.447750	846.712589	9.946906
7.709407	840.325128	9.951923
7.972934	857.877323	9.956941
8.118906	869.003870	9.961959
8.365768	867.505676	9.966976
8.220693	876.906864	9.971994
8.168647	887.824477	9.977011
8.241929	880.961860	9.982029
8.478318	865.371185	9.987047
8.666084	869.587390	9.992064
8.635350	892.197692	9.997082
8.468874	869.644088	10.002099
8.530371	896.890616	10.007117
8.535764	885.480047	10.012135
8.514852	863.886888	10.017152
8.539772	867.192745	10.022170
8.628350	884.962219	10.027187
8.482638	879.073150	10.032205
8.674847	871.777801	10.037223
8.699933	877.382450	10.042240
8.620544	867.258610	10.047258
8.741335	869.685952	10.052275
8.667120	863.197922	10.057293
8.474331	855.331327	10.062311
8.405326	844.135983	10.067328
8.122768	855.313459	10.072346
8.168486	876.190190	10.077363
8.546904	870.740753	10.082381
8.565492	863.561282	10.087399
8.781922	865.462714	10.092416
8.204552	878.387109	10.097434
8.421927	883.956246	10.102451
8.698632	871.026133	10.107469
8.388118	868.466012	10.112487
8.917663	866.705608	10.117504
8.663465	882.400481	10.122522
8.494426	868.191523	10.127539
8.774207	873.868029	10.132557
8.557662	865.660856	10.137575
8.460078	883.424487	10.142592
8.229112	875.713857	10.147610
8.487257	876.562013	10.152627
8.204701	889.328770	10.157645
8.173170	874.900872	10.162663
8.250299	893.442719	10.167680
8.444535	899.968788	10.172698
8.781204	904.230457	10.177715
9.013555	915.796290	10.182733
8.722567	922.532243	10.187751
9.122775	909.887517	10.192768
8.786136	907.386318	10.197786
8.496638	888.918613	10.202803
8.703088	883.631611	10.207821
8.726999	893.564780	10.212839
8.790167	916.051163	10.217856
8.729116	921.488416	10.222874
8.997639	906.613859	10.227891
8.811999	915.643820	10.232909
8.594916	910.483968	10.237927
8.846189	907.720993	10.242944
8.422476	910.617654	10.247962
8.674749	918.769354	10.252979
8.871798	918.802523	10.257997
8.598534	910.159143	10.263015
8.690813	912.441931	10.268032
8.500647	923.548789	10.273050
8.647356	911.886264	10.278067
8.912189	915.988394	10.283085
8.831948	923.091585	10.288103
8.789085	901.290736	10.293120
8.565598	888.623141	10.298138
8.443942	911.942610	10.303155
8.975485	910.342362	10.308173
9.021640	907.290235	10.313191
8.850870	917.376721	10.318208
8.590903	911.216634	10.323226
8.756912	903.139776	10.328243
8.767930	933.246247	10.333261
9.238822	956.610718	10.338279
9.294293	935.938385	10.343296
9.147955	927.809416	10.348314
8.899584	911.728277	10.353331
8.954437	910.796023	10.358349
8.741325	918.422911	10.363367
8.944169	908.400594	10.368384
9.009096	923.121748	10.373402
9.074851	943.280381	10.378419
8.850404	929.835056	10.383437
8.916931	936.075924	10.388455
9.414498	941.973291	10.393472
9.070065	944.905467	10.398490
9.203159	926.781755	10.403507
9.308169	912.323879	10.408525
9.156276	905.282374	10.413543
9.018000	918.723561	10.418560
9.297103	922.559031	10.423578
9.092608	898.645085	10.428595
9.159972	897.879225	10.433613
9.014748	905.275161	10.438631
9.175398	908.188415	10.443648
8.956916	922.994286	10.448666
9.070909	900.983017	10.453683
9.390306	895.401039	10.458701
9.096952	922.613953	10.463719
9.284858	909.089975	10.468736
9.381450	914.718738	10.473754
9.347703	928.506346	10.478771
9.391505	912.446985	10.483789
9.428239	917.613910	10.488807
9.409523	894.923576	10.493824
9.287700	901.283919	10.498842
9.269551	916.300120	10.503859
9.499010	913.761559	10.508877
9.256255	920.723438	10.513895
9.402381	926.838481	10.518912
9.459142	911.860759	10.523930
9.268246	900.169310	10.528947
9.380505	902.775876	10.533965
9.410553	909.147927	10.538983
9.408949	886.029001	10.544000
9.329611	872.640927	10.549018
9.322524	881.095045	10.554035
9.322813	874.549729	10.559053
9.016982	876.683788	10.564071
9.012666	898.469176	10.569088
9.403195	901.445794	10.574106
9.762566	919.442636	10.579123
9.404761	897.057188	10.584141
9.382299	883.230189	10.589159
9.591580	869.829846	10.594176
9.655427	866.744004	10.599194
9.194803	886.043236	10.604211
9.397617	878.298116	10.609229
9.024243	878.547170	10.614247
9.041937	869.853075	10.619264
9.303381	875.585158	10.624282
9.377467	907.982732	10.629299
9.508154	890.954653	10.634317
9.421158	907.017685	10.639335
9.638822	920.438233	10.644352
9.780942	905.212810	10.649370
9.239885	891.796911	10.654387
9.547745	896.684538	10.659405
9.374049	897.178477	10.664423
9.419066	901.269597	10.669440
9.689886	914.788612	10.674458
9.739348	913.737889	10.679475
9.580711	877.710919	10.684493
9.371521	873.019144	10.689511
9.575390	871.326137	10.694528
9.539376	861.139045	10.699546
9.385770	881.234561	10.704563
9.362025	893.892625	10.709581
9.504072	908.099574	10.714599
9.422417	895.990079	10.719616
9.562516	896.893167	10.724634
9.557317	922.249280	10.729651
9.766076	920.476445	10.734669
9.530391	908.758639	10.739687
9.827830	887.044255	10.744704
9.900634	912.461163	10.749722
9.647783	925.476324	10.754739
9.720945	896.166478	10.759757
9.324206	886.557941	10.764775
9.638260	900.546055	10.769792
9.614980	904.850478	10.774810
9.572313	904.105653	10.779827
9.598469	904.263987	10.784845
9.739724	910.109818	10.789863
9.611168	908.185495	10.794880
9.857452	903.741982	10.799898
9.407459	904.381455	10.804915
9.749521	896.013371	10.809933
9.738253	914.309386	10.814951
9.644983	927.129716	10.819968
9.435733	923.485799	10.824986
9.396299	915.930950	10.830003
9.989466	898.733547	10.835021
9.695372	914.000412	10.840039
9.712799	901.248912	10.845056
9.855945	900.403813	10.850074
9.620078	923.701731	10.855091
9.881591	913.075380	10.860109
9.936426	892.728988	10.865127
9.836621	915.769136	10.870144
9.989606	921.371657	10.875162
9.770600	923.903671	10.880179
9.628585	895.201091	10.885197
9.636074	912.169737	10.890215
9.366313	920.209034	10.895232
9.808201	901.147344	10.900250
9.597045	937.999950	10.905267
9.978869	935.044376	10.910285
9.991163	948.237042	10.915303
9.815788	947.769987	10.920320
9.985677	943.696674	10.925338
9.967817	951.581865	10.930355
10.166016	925.650567	10.935373
9.981243	948.346530	10.940391
9.929813	936.655818	10.945408
9.863871	937.392319	10.950426
9.977733	955.739416	10.955443
10.038151	939.045575	10.960461
10.187751	940.534054	10.965479
9.925358	947.608218	10.970496
10.043262	948.037145	10.975514
9.922455	928.317317	10.980531
10.172604	951.801505	10.985549
10.155810	957.115246	10.990567
9.900253	941.720155	10.995584
10.241522	945.391952	11.000602
10.383031	937.785248	11.005619
10.051501	930.089633	11.010637
9.945372	920.001468	11.015655
10.287563	928.013542	11.020672
10.072809	940.038810	11.025690
9.912636	938.848363	11.030707
10.059586	938.933894	11.035725
10.040366	954.297737	11.040743
9.762107	941.108008	11.045760
10.170500	923.394891	11.050778
10.123134	938.377468	11.055795
10.242121	961.069476	11.060813
9.956419	935.571779	11.065831
9.921798	932.518137	11.070848
10.234901	937.112268	11.075866
10.202707	931.336374	11.080883
10.203526	931.318724	11.085901
10.070598	945.898624	11.090919
10.200025	935.561831	11.095936
10.140409	928.306987	11.100954
10.344405	939.171797	11.105971
10.306567	951.828475	11.110989
10.396943	942.970126	11.116007
10.312564	923.514492	11.121024
10.464975	940.186947	11.126042
10.364074	944.487775	11.131059
10.390466	927.077090	11.136077
10.450490	941.897571	11.141095
10.436054	942.362537	11.146112
10.357384	932.742245	11.151130
10.377552	958.546744	11.156147
10.104275	935.578542	11.161165
10.023034	946.426926	11.166183
9.972905	929.260125	11.171200
10.414143	942.420476	11.176218
9.868010	960.597284	11.181235
10.257511	956.210089	11.186253
10.464321	962.491353	11.191271
10.295353	982.913573	11.196288
10.608571	962.792926	11.201306
10.558643	974.962398	11.206323
10.398763	989.900346	11.211341
10.382294	977.828625	11.216359
10.129595	982.007046	11.221376
10.247063	972.898472	11.226394
10.193749	981.274086	11.231411
10.670511	987.463813	11.236429
10.633159	974.841549	11.241447
10.470252	971.737562	11.246464
10.828374	975.373913	11.251482
10.372098	971.505419	11.256499
10.572440	975.795344	11.261517
10.824518	953.330186	11.266535
10.601879	966.146244	11.271552
10.856676	977.172230	11.276570
10.276709	981.590217	11.281587
10.468684	972.740327	11.286605
10.615941	962.480274	11.291623
10.326549	980.500658	11.296640
10.562475	989.202204	11.301658
10.786909	984.080461	11.306675
10.699253	963.851002	11.311693
10.769373	966.879400	11.316711
10.530389	977.368832	11.321728
10.626933	961.397629	11.326746
10.735437	982.444693	11.331763
10.973058	988.897014	11.336781
10.861685	969.542411	11.341799
10.354726	970.115729	11.346816
10.662348	976.642085	11.351834
10.509351	969.039359	11.356851
10.617914	979.479035	11.361869
10.442920	979.388495	11.366887
10.239971	979.263903	11.371904
10.473670	974.765672	11.376922
10.676370	986.319042	11.381939
10.760504	989.469605	11.386957
10.873010	984.054231	11.391975
10.942463	999.248706	11.396992
10.950731	1000.374914	11.402010
10.753905	994.796730	11.407027
10.993207	976.072680	11.412045
10.866051	980.312617	11.417063
10.968792	1011.047722	11.422080
11.211260	996.770052	11.427098
11.060327	983.809454	11.432115
10.958539	990.728685	11.437133
10.951849	962.884400	11.442151
10.498719	975.604927	11.447168
10.759145	978.419542	11.452186
11.147064	990.775564	11.457203
10.797701	1003.723098	11.462221
10.962799	997.029758	11.467239
10.942043	994.003726	11.472256
11.087499	993.166900	11.477274
10.922618	988.590178	11.482291
11.355163	1000.583016	11.487309
11.311277	973.637648	11.492327
10.566071	978.534008	11.497344
10.718143	991.577168	11.502362
11.017690	995.995747	11.507379
11.081092	982.749006	11.512397
10.961003	981.062585	11.517415
11.048264	993.498698	11.522432
10.971873	985.524437	11.527450
10.905111	1004.076519	11.532467
10.918082	993.296842	11.537485
10.700530	987.248287	11.542503
10.954379	982.499149	11.547520
10.981751	989.102719	11.552538
10.974988	1009.815907	11.557555
11.026812	1000.086629	11.562573
11.152371	983.181311	11.567591
10.973608	987.845718	11.572608
10.835430	994.443192	11.577626
10.985546	996.745267	11.582643
11.311643	1018.308353	11.587661
11.342682	1037.523279	11.592679
11.241002	1026.749339	11.597696
11.762813	1022.695685	11.602714
11.329648	1009.305346	11.607731
11.172594	981.076430	11.612749
11.323991	991.318139	11.617767
11.060986	1010.473086	11.622784
11.253612	986.611951	11.627802
11.128347	982.888410	11.632819
11.001726	1013.409713	11.637837
11.344713	1027.231587	11.642855
11.362646	1022.955664	11.647872
11.377450	1020.554009	11.652890
11.351357	1040.593237	11.657907
11.106675	1026.249129	11.662925
11.601771	1018.049637	11.667943
11.404738	1028.082972	11.672960
11.165534	1037.630490	11.677978
11.371525	1027.304993	11.682995
11.116805	1012.871240	11.688013
11.339246	1029.255615	11.693031
11.327090	1028.180429	11.698048
11.410956	1019.624588	11.703066
11.675938	1033.706738	11.708083
11.555758	1043.313115	11.713101
11.717007	1037.671906	11.718119
11.467245	1019.229654	11.723136
11.139951	1035.073343	11.728154
11.749424	1030.471572	11.733171
11.466962	1033.207448	11.738189
11.890773	1015.408136	11.743207
11.850331	1032.964810	11.748224
11.323149	1046.007890	11.753242
11.552748	1033.380136	11.758259
11.411527	1031.839686	11.763277
11.480514	1021.605221	11.768295
11.579429	1033.277819	11.773312
11.718468	1036.745025	11.778330
11.807354	1024.727985	11.783347
11.226938	1024.085499	11.788365
11.407955	1023.232955	11.793383
11.462697	1030.120532	11.798400
11.155138	1031.998858	11.803418
11.294948	1027.285869	11.808435
11.077369	1019.685425	11.813453
11.338349	1050.348605	11.818471
11.471836	1049.480101	11.823488
11.486210	1055.059230	11.828506
11.916007	1069.304681	11.833523
11.718128	1077.114420	11.838541
11.736764	1063.487700	11.843559
11.776117	1069.785856	11.848576
11.732662	1067.366465	11.853594
12.074785	1069.112540	11.858611
11.754662	1066.440320	11.863629
11.686337	1049.111667	11.868647
11.976159	1064.124058	11.873664
11.995439	1075.657031	11.878682
12.081062	1062.528271	11.883699
11.796401	1056.484481	11.888717
11.808948	1067.063774	11.893735
11.636233	1053.000196	11.898752
11.759070	1057.112939	11.903770
11.798531	1076.634321	11.908787
11.664941	1079.148506	11.913805
12.013130	1057.679272	11.918823
11.635605	1071.859661	11.923840
11.269088	1055.974918	11.928858
11.778148	1062.953632	11.933875
11.535019	1077.490662	11.938893
11.817808	1067.142509	11.943911
11.686310	1073.179207	11.948928
11.419071	1089.823558	11.953946
11.796064	1102.162090	11.958963
11.595721	1090.118599	11.963981
12.077822	1091.094089	11.968999
12.030139	1115.797761	11.974016
11.922181	1103.060811	11.979034
12.224920	1082.566141	11.984051
12.034724	1091.802222	11.989069
12.089679	1105.060397	11.994087
12.409094	1091.808845	11.999104
12.107027	1089.826283	12.004122
12.467527	1097.514436	12.009139
12.051356	1092.158443	12.014157
12.275679	1090.394824	12.019175
12.385311	1089.973853	12.024192
12.410814	1080.284889	12.029210
12.362812	1102.285412	12.034227
12.196869	1102.183535	12.039245
12.386658	1081.350138	12.044263
12.169640	1077.996276	12.049280
12.053249	1071.343811	12.054298
12.083085	1066.882587	12.059315
12.044014	1090.012247	12.064333
12.284934	1105.811212	12.069351
12.253285	1085.823262	12.074368
12.328492	1095.807323	12.079386
12.361757	1091.568798	12.084403
11.986469	1105.227420	12.089421
12.472843	1089.530460	12.094439
12.555812	1092.534717	12.099456
12.426027	1094.063377	12.104474
12.333146	1089.399548	12.109491
12.321984	1095.741093	12.114509
12.314655	1093.407438	12.119527
12.316282	1076.227885	12.124544
11.950116	1072.878104	12.129562
12.251779	1092.261417	12.134579
12.008060	1098.127935	12.139597
12.403213	1091.559588	12.144615
12.313950	1101.811423	12.149632
11.956856	1095.552772	12.154650
12.060766	1093.920344	12.159667
12.340048	1086.017341	12.164685
12.329889	1073.946666	12.169703
12.360151	1087.326889	12.174720
12.145467	1089.362766	12.179738
12.932156	1093.233467	12.184755
12.427600	1098.124439	12.189773
12.369634	1103.986045	12.194791
12.663969	1091.127127	12.199808
12.693544	1123.715833	12.204826
12.489230	1084.538123	12.209843
12.585828	1091.116227	12.214861
12.469902	1101.927156	12.219879
12.949381	1105.284492	12.224896
12.396498	1098.616667	12.229914
12.751704	1081.816564	12.234931
12.540802	1088.956872	12.239949
12.418724	1099.206846	12.244967
12.778125	1098.999460	12.249984
12.660446	1126.488552	12.255002
13.022269	1109.225823	12.260019
12.529247	1098.873207	12.265037
12.606473	1093.366798	12.270055
12.691313	1093.218165	12.275072
12.541793	1133.253881	12.280090
12.780311	1133.569794	12.285107
12.750801	1121.177653	12.290125
12.407694	1130.696642	12.295143
12.826912	1131.970252	12.300160
12.719144	1122.133247	12.305178
12.718841	1123.495863	12.310195
12.807537	1136.310012	12.315213
12.639433	1117.489865	12.320231
13.098123	1122.385900	12.325248
12.673196	1135.712282	12.330266
12.590394	1121.514718	12.335283
12.851176	1120.607462	12.340301
12.608534	1132.490674	12.345319
12.564211	1126.605911	12.350336
12.612204	1121.407497	12.355354
12.752564	1131.800695	12.360371
12.476471	1124.884214	12.365389
12.465567	1135.935526	12.370407
13.032083	1143.835563	12.375424
12.997308	1160.457124	12.380442
13.054103	1162.320520	12.385459
12.975841	1151.124613	12.390477
12.834764	1166.892596	12.395495
12.989753	1156.396547	12.400512
12.995182	1161.824178	12.405530
13.101898	1153.390047	12.410547
13.344748	1160.849702	12.415565
13.165906	1168.498012	12.420583
13.036498	1152.562473	12.425600
12.837408	1163.796736	12.430618
13.345300	1150.242202	12.435635
13.330901	1151.290001	12.440653
13.265930	1175.731927	12.445671
12.991521	1157.020812	12.450688
12.824835	1149.120034	12.455706
13.081888	1139.521183	12.460723
12.722380	1157.316016	12.465741
12.673369	1149.608143	12.470759
12.841817	1131.467424	12.475776
12.744944	1163.450096	12.480794
13.148030	1163.669934	12.485811
13.048973	1157.205860	12.490829
12.706524	1160.628478	12.495847
13.256536	1157.519312	12.500864
13.207273	1182.704636	12.505882
13.376060	1203.255051	12.510899
13.372468	1187.927374	12.515917
13.511119	1191.987158	12.520935
13.484810	1175.380185	12.525952
13.443500	1172.260294	12.530970
13.269492	1176.728644	12.535987
13.365206	1184.327853	12.541005
13.383174	1192.430250	12.546023
13.564055	1174.577219	12.551040
13.400132	1179.381422	12.556058
13.330996	1169.974414	12.561075
13.046487	1156.365923	12.566093
13.378093	1170.863269	12.571111
13.500942	1190.577857	12.576128
13.085524	1183.438664	12.581146
13.401370	1169.543299	12.586163
13.423910	1182.830711	12.591181
13.156488	1192.416838	12.596199
13.102659	1178.624277	12.601216
13.252446	1193.857822	12.606234
13.436204	1197.780460	12.611251
13.356052	1190.721360	12.616269
13.612250	1199.630945	12.621287
13.555259	1182.021989	12.626304
13.363798	1184.566025	12.631322
13.676816	1190.893006	12.636339
13.561854	1176.973573	12.641357
13.554172	1190.792239	12.646375
13.527295	1186.202394	12.651392
13.437635	1184.625855	12.656410
13.847412	1219.331341	12.661427
13.600441	1209.085790	12.666445
13.530434	1212.792848	12.671463
14.001824	1216.298165	12.676480
13.841006	1204.604760	12.681498
13.636486	1196.017263	12.686515
13.785698	1187.581897	12.691533
13.304676	1194.741209	12.696551
13.842642	1200.324790	12.701568
14.045645	1222.579804	12.706586
13.971385	1212.013062	12.711603
14.037564	1187.547362	12.716621
13.584182	1200.955650	12.721639
13.961738	1199.699151	12.726656
13.635972	1176.884969	12.731674
13.667108	1171.730259	12.736691
13.935710	1193.399724	12.741709
14.134167	1209.476616	12.746727
14.151781	1182.737202	12.751744
13.839797	1187.487645	12.756762
13.915864	1186.925599	12.761779
14.149621	1185.534141	12.766797
13.851319	1182.623409	12.771815
13.846441	1163.507300	12.776832
13.676795	1187.500904	12.781850
13.714658	1186.495573	12.786867
13.891259	1207.318949	12.791885
14.055718	1211.160547	12.796903
14.299067	1208.304559	12.801920
14.344520	1208.549449	12.806938
13.989776	1185.973157	12.811955
13.818336	1187.505462	12.816973
13.543228	1177.181728	12.821991
14.054187	1207.111557	12.827008
14.145407	1234.908073	12.832026
14.034697	1217.094617	12.837043
14.231537	1202.473296	12.842061
14.199061	1225.809403	12.847079
14.140675	1230.713576	12.852096
14.042766	1221.235620	12.857114
14.112172	1232.997282	12.862131
14.369288	1223.624594	12.867149
14.112416	1223.917968	12.872167
14.156819	1232.128196	12.877184
14.091540	1231.857849	12.882202
14.082945	1215.505030	12.887219
14.256013	1227.020378	12.892237
13.818625	1209.819937	12.897255
14.210736	1213.922272	12.902272
14.273464	1218.590630	12.907290
14.089432	1222.308465	12.912307
14.562517	1216.874555	12.917325
13.901023	1221.768868	12.922343
14.033026	1233.031716	12.927360
14.494677	1220.061006	12.932378
14.299231	1209.197831	12.937395
14.452011	1208.743748	12.942413
13.936452	1229.662149	12.947431
14.004165	1222.952429	12.952448
14.215836	1241.956899	12.957466
14.434585	1254.380745	12.962483
14.602401	1232.419246	12.967501
14.287983	1243.087821	12.972519
14.390238	1246.195097	12.977536
14.496583	1244.381682	12.982554
14.616238	1242.480950	12.987571
14.705371	1250.491026	12.992589
14.525798	1251.594467	12.997607
14.543858	1238.840318	13.002624
14.812739	1235.547431	13.007642
14.576998	1252.270493	13.012659
14.672222	1247.546305	13.017677
14.768846	1245.798556	13.022695
14.688682	1233.976572	13.027712
14.633613	1239.591155	13.032730
14.409465	1235.243491	13.037747
14.767191	1240.448896	13.042765
14.901662	1249.566771	13.047783
14.805925	1240.622867	13.052800
14.617549	1228.927404	13.057818
14.624684	1241.969637	13.062835
15.028120	1230.190743	13.067853
14.779081	1242.838698	13.072871
14.618971	1239.314508	13.077888
14.922768	1238.578934	13.082906
14.496052	1253.015002	13.087923
14.453400	1230.891972	13.092941
14.422849	1248.443224	13.097959
14.779846	1242.322256	13.102976
14.857935	1239.653869	13.107994
14.809324	1242.177654	13.113011
14.844231	1251.708150	13.118029
14.554453	1250.541752	13.123047
14.640443	1235.263579	13.128064
14.841303	1244.513852	13.133082
14.900327	1254.158251	13.138099
14.697878	1236.055378	13.143117
14.533985	1245.276184	13.148135
14.734169	1249.812513	13.153152
15.071605	1244.324650	13.158170
14.841127	1269.328891	13.163187
15.017188	1270.573715	13.168205
14.833386	1273.303169	13.173223
14.961404	1287.418223	13.178240
14.983290	1283.528789	13.183258
15.094182	1289.488222	13.188275
15.157762	1289.042580	13.193293
15.124967	1279.075788	13.198311
15.189502	1262.202783	13.203328
15.262219	1276.279830	13.208346
15.036492	1286.434879	13.213363
15.197714	1269.365122	13.218381
15.245254	1262.304470	13.223399
15.039740	1274.981963	13.228416
15.381566	1253.919810	13.233434
15.136930	1274.239397	13.238451
15.269127	1295.090698	13.243469
15.327440	1270.432706	13.248487
15.064277	1284.079846	13.253504
15.667187	1282.110960	13.258522
14.966761	1272.359692	13.263539
15.296484	1257.204765	13.268557
15.183157	1280.010052	13.273575
15.132701	1283.735939	13.278592
15.532348	1278.655404	13.283610
15.022523	1281.000647	13.288627
15.221582	1260.787280	13.293645
15.225357	1258.202118	13.298663
15.144478	1281.567761	13.303680
15.233195	1272.677787	13.308698
15.267832	1271.143184	13.313715
15.451433	1278.813231	13.318733
15.236143	1279.210339	13.323751
15.069909	1275.083453	13.328768
15.522829	1267.694649	13.333786
15.018484	1283.411686	13.338803
15.339986	1290.912233	13.343821
15.564900	1299.733859	13.348839
15.721258	1312.983427	13.353856
15.697528	1295.975792	13.358874
15.701212	1302.136172	13.363891
15.216696	1303.425312	13.368909
15.519369	1320.331361	13.373927
15.164041	1309.154259	13.378944
15.799689	1298.701195	13.383962
15.738198	1317.551633	13.388979
15.793352	1297.997877	13.393997
15.853319	1314.182784	13.399015
15.769205	1326.192866	13.404032
15.835473	1313.068961	13.409050
15.728591	1296.148376	13.414067
15.917149	1294.077626	13.419085
15.857067	1292.943625	13.424103
15.557260	1281.151602	13.429120
15.777596	1287.986149	13.434138
15.616561	1314.867136	13.439155
15.879147	1304.540564	13.444173
16.021495	1288.976415	13.449191
15.806841	1310.401470	13.454208
15.958665	1315.540556	13.459226
15.611972	1315.504168	13.464243
16.172082	1304.121967	13.469261
15.830203	1307.626787	13.474279
15.518007	1297.394612	13.479296
16.044610	1298.850052	13.484314
15.881692	1311.690281	13.489331
15.964732	1311.401819	13.494349
16.069090	1314.831031	13.499367
15.846440	1322.553964	13.504384
16.131463	1307.238697	13.509402
15.521493	1299.079478	13.514419
16.060855	1301.920287	13.519437
16.067392	1309.493359	13.524455
15.902239	1301.178171	13.529472
16.269666	1322.925659	13.534490
16.314093	1305.283959	13.539507
15.952537	1288.241234	13.544525
15.959953	1315.520469	13.549543
15.922618	1300.638805	13.554560
16.229577	1293.523068	13.559578
15.870452	1333.038755	13.564595
15.850953	1316.951349	13.569613
15.950911	1295.173178	13.574631
15.817256	1294.912358	13.579648
15.997338	1314.608004	13.584666
15.836495	1310.280657	13.589683
16.116959	1327.689680	13.594701
16.473978	1340.984639	13.599719
16.324879	1335.118094	13.604736
16.074509	1323.322888	13.609754
16.478053	1348.677894	13.614771
16.244879	1361.827542	13.619789
16.232268	1343.270727	13.624807
15.973750	1339.998057	13.629824
16.253942	1342.201738	13.634842
16.136273	1346.404783	13.639859
15.911666	1330.638200	13.644877
16.180249	1347.242994	13.649895
15.952090	1354.388147	13.654912
16.516150	1347.220550	13.659930
16.363185	1363.786288	13.664947
16.765164	1353.583957	13.669965
16.773359	1346.215273	13.674983
16.647214	1356.886173	13.680000
16.684999	1344.526028	13.685018
16.695055	1327.962475	13.690035
16.655527	1342.858147	13.695053
16.464913	1337.739534	13.700071
16.573322	1346.187222	13.705088
16.911974	1332.170449	13.710106
16.367791	1347.680797	13.715123
16.736228	1350.050663	13.720141
16.540829	1332.100610	13.725159
16.135855	1333.668668	13.730176
16.592692	1326.087795	13.735194
16.735481	1368.504698	13.740211
16.658004	1372.051451	13.745229
17.016081	1359.838911	13.750247
17.053454	1359.259242	13.755264
17.137635	1326.007388	13.760282
16.881337	1332.116866	13.765299
17.134417	1333.647817	13.770317
17.221141	1319.490543	13.775335
17.401701	1327.310099	13.780352
17.126272	1330.850390	13.785370
17.080935	1334.467987	13.790387
16.991899	1330.986054	13.795405
17.136798	1331.002061	13.800423
16.682752	1326.916720	13.805440
16.904579	1326.713073	13.810458
17.172361	1317.760419	13.815475
17.030196	1313.180337	13.820493
17.000554	1301.305178	13.825511
16.855387	1307.328581	13.830528
16.869355	1295.674711	13.835546
16.913986	1314.697625	13.840563
16.812410	1320.335470	13.845581
17.358937	1315.832679	13.850599
16.886342	1329.969876	13.855616
17.094505	1330.708530	13.860634
17.183692	1328.757126	13.865651
16.909581	1330.939831	13.870669
17.094334	1321.885764	13.875687
17.014811	1324.708403	13.880704
16.866691	1321.820650	13.885722
16.947681	1339.300731	13.890739
17.136132	1344.088478	13.895757
17.390259	1320.126525	13.900775
17.058853	1337.722183	13.905792
17.283761	1321.693967	13.910810
17.247860	1327.907936	13.915827
16.786636	1335.974267	13.920845
17.177948	1317.072354	13.925863
16.935291	1329.927054	13.930880
16.928839	1325.944676	13.935898
17.026634	1331.669337	13.940915
17.309021	1360.829745	13.945933
17.414637	1349.285858	13.950951
17.296549	1355.397008	13.955968
17.235686	1365.965513	13.960986
17.347964	1350.702070	13.966003
17.198011	1368.439984	13.971021
17.323683	1380.693135	13.976039
17.364405	1357.826977	13.981056
17.064712	1351.277106	13.986074
17.401769	1358.803456	13.991091
17.313689	1363.753317	13.996109
17.724280	1361.222832	14.001127
17.692040	1359.977064	14.006144
17.550298	1365.593125	14.011162
17.752356	1349.445752	14.016179
17.692365	1365.384848	14.021197
17.863051	1352.784378	14.026215
17.595535	1362.822198	14.031232
17.586876	1362.502934	14.036250
17.863227	1347.898840	14.041267
17.343704	1355.047466	14.046285
17.661175	1361.969120	14.051303
17.442637	1344.652755	14.056320
17.490042	1361.383857	14.061338
17.934819	1377.499928	14.066355
17.646368	1387.064263	14.071373
17.905348	1372.006033	14.076391
17.737450	1380.913971	14.081408
17.807084	1384.046052	14.086426
17.889234	1384.471257	14.091443
17.745882	1387.743825	14.096461
17.620976	1377.412650	14.101479
17.776701	1379.512228	14.106496
17.954212	1386.532694	14.111514
18.167680	1381.784694	14.116531
18.351877	1368.476329	14.121549
18.309745	1379.986812	14.126567
18.143487	1368.242815	14.131584
17.815226	1357.164626	14.136602
17.746506	1349.036678	14.141619
18.076872	1376.264327	14.146637
18.352700	1377.116479	14.151655
17.863008	1367.112854	14.156672
17.913278	1368.347280	14.161690
17.802608	1380.750978	14.166707
17.852147	1397.117281	14.171725
18.020914	1380.413297	14.176743
17.746225	1372.950433	14.181760
17.954937	1389.114972	14.186778
18.224496	1393.727656	14.191795
18.056035	1377.033152	14.196813
18.333275	1383.395647	14.201831
18.269936	1385.601981	14.206848
18.016452	1361.310454	14.211866
18.295112	1379.226216	14.216883
17.954120	1384.888200	14.221901
18.235642	1396.874227	14.226919
18.279186	1381.207047	14.231936
18.294184	1382.017182	14.236954
18.240525	1389.000276	14.241971
18.049694	1389.307340	14.246989
18.553029	1390.329528	14.252007
18.755371	1415.508688	14.257024
18.663471	1401.384497	14.262042
18.569979	1368.953663	14.267059
18.225378	1385.182474	14.272077
18.401568	1389.742982	14.277095
18.668395	1365.665990	14.282112
18.291267	1367.109594	14.287130
18.414444	1387.926300	14.292147
18.367379	1397.986459	14.297165
18.492917	1404.388792	14.302183
18.578936	1414.250631	14.307200
18.670085	1423.671373	14.312218
18.833781	1408.276568	14.317235
18.887061	1401.763896	14.322253
18.768607	1413.211639	14.327271
18.658286	1401.816068	14.332288
18.901263	1394.114829	14.337306
18.652440	1392.401122	14.342323
18.450738	1392.286160	14.347341
18.797531	1389.844936	14.352359
18.813148	1407.566260	14.357376
18.585140	1426.589888	14.362394
18.972372	1428.538839	14.367411
18.921886	1411.589422	14.372429
18.491635	1402.043171	14.377447
18.645446	1405.131431	14.382464
18.560230	1392.992217	14.387482
18.743491	1404.369431	14.392499
18.249929	1423.178234	14.397517
18.737173	1401.727067	14.402535
18.595142	1398.853841	14.407552
18.626957	1417.850365	14.412570
19.098714	1412.217143	14.417587
18.982209	1427.403509	14.422605
19.158811	1450.466091	14.427623
19.634214	1442.815474	14.432640
19.164353	1422.839669	14.437658
19.409815	1409.780340	14.442675
18.880864	1413.675171	14.447693
19.013712	1400.714854	14.452711
19.324890	1404.425489	14.457728
19.061682	1409.208285	14.462746
19.462967	1401.022912	14.467763
19.034607	1412.833313	14.472781
19.257135	1394.041069	14.477799
19.235779	1401.166633	14.482816
18.972795	1415.808422	14.487834
19.360106	1402.021582	14.492851
19.410185	1403.864962	14.497869
19.132101	1394.848958	14.502887
19.054772	1407.733181	14.507904
18.613328	1408.771959	14.512922
19.294994	1422.003992	14.517939
19.295718	1447.948546	14.522957
19.221344	1456.672902	14.527975
19.529072	1423.856921	14.532992
19.368709	1431.227959	14.538010
19.615621	1429.678534	14.543027
19.806731	1457.533340	14.548045
19.697391	1441.783020	14.553063
19.923899	1426.843266	14.558080
19.277102	1419.000432	14.563098
19.612424	1388.042743	14.568115
19.373314	1406.673781	14.573133
19.507839	1441.534485	14.578151
19.619267	1440.310726	14.583168
19.461495	1431.962660	14.588186
19.687477	1441.087175	14.593203
19.481349	1444.806353	14.598221
19.710279	1447.871974	14.603239
19.686568	1437.845324	14.608256
19.529085	1446.908533	14.613274
19.810437	1442.900607	14.618291
19.621175	1441.465572	14.623309
19.518750	1441.374057	14.628327
19.920699	1449.714547	14.633344
19.696927	1429.805622	14.638362
19.607728	1436.131568	14.643379
19.778256	1453.097586	14.648397
19.399994	1451.476408	14.653415
19.796095	1439.033752	14.658432
19.600847	1436.467278	14.663450
19.903131	1427.838314	14.668467
20.018433	1429.033067	14.673485
19.796343	1444.185826	14.678503
19.727736	1435.886395	14.683520
19.942501	1436.826084	14.688538
20.063225	1439.367873	14.693555
19.865601	1455.701281	14.698573
19.936658	1464.328495	14.703591
20.266881	1460.542262	14.708608
20.110302	1457.397866	14.713626
20.367643	1473.515392	14.718643
20.365926	1453.434732	14.723661
20.079340	1444.229594	14.728679
20.523547	1447.194301	14.733696
20.397520	1436.007456	14.738714
20.259120	1444.843052	14.743731
20.514686	1432.413686	14.748749
20.191038	1435.696280	14.753767
20.508443	1438.262937	14.758784
20.201339	1433.051460	14.763802
20.354568	1415.669348	14.768819
20.352971	1422.180571	14.773837
20.301655	1451.748680	14.778855
20.512287	1427.715121	14.783872
20.091552	1428.287784	14.788890
20.230216	1434.247999	14.793907
20.493185	1415.383705	14.798925
20.205215	1424.849679	14.803943
20.191322	1440.747583	14.808960
20.045421	1442.461774	14.813978
20.376228	1438.428752	14.818995
20.445740	1449.715175	14.824013
20.403497	1458.525048	14.829031
20.540359	1448.728099	14.834048
20.323837	1472.018633	14.839066
20.682989	1460.739195	14.844083
20.689736	1456.201278	14.849101
20.753709	1458.351159	14.854119
20.822311	1458.586619	14.859136
20.500330	1453.283914	14.864154
20.416566	1458.067478	14.869171
20.779371	1470.578006	14.874189
20.699558	1461.088153	14.879207
20.871803	1453.780280	14.884224
19.995927	1461.845922	14.889242
20.067992	1459.384353	14.894259
20.127612	1450.278069	14.899277
20.320710	1487.553273	14.904295
20.549390	1490.042101	14.909312
20.265489	1487.925902	14.914330
20.146693	1495.426294	14.919347
20.598154	1482.618626	14.924365
20.606658	1503.150271	14.929383
20.989673	1497.152632	14.934400
21.295418	1503.363451	14.939418
21.453741	1513.325094	14.944435
21.606579	1478.048711	14.949453
21.307008	1481.502396	14.954471
21.160855	1477.541096	14.959488
21.355334	1472.563185	14.964506
21.145036	1460.922928	14.969523
21.614098	1475.958456	14.974541
21.239831	1473.057366	14.979559
21.752218	1469.303515	14.984576
21.472735	1454.432981	14.989594
21.039341	1445.496242	14.994611
21.577934	1450.803693	14.999629
21.227021	1444.712441	15.004647
21.258695	1427.587851	15.009664
21.294997	1449.669114	15.014682
21.235297	1444.129116	15.019699
21.466756	1433.802877	15.024717
21.226671	1446.575575	15.029735
21.385358	1446.104470	15.034752
21.165065	1440.364585	15.039770
21.104388	1438.535548	15.044787
20.963969	1438.317565	15.049805
20.820180	1473.168341	15.054823
21.639319	1466.181718	15.059840
21.637691	1471.465185	15.064858
21.619384	1479.070097	15.069875
21.746648	1464.372839	15.074893
21.394635	1455.484837	15.079911
21.517576	1477.938746	15.084928
21.634296	1481.130374	15.089946
21.780392	1479.654973	15.094963
22.202857	1494.531228	15.099981
21.496413	1481.425640	15.104999
21.575975	1467.923896	15.110016
21.463253	1462.077959	15.115034
21.355402	1481.043716	15.120051
21.814175	1483.618804	15.125069
21.558564	1481.984440	15.130087
21.599724	1462.917719	15.135104
21.635033	1487.141744	15.140122
21.345483	1480.831032	15.145139
21.463777	1473.350117	15.150157
21.458228	1480.748538	15.155175
21.738388	1485.563882	15.160192
21.933903	1487.624721	15.165210
21.730933	1513.967535	15.170227
22.129535	1515.274698	15.175245
21.883482	1503.301315	15.180263
22.058640	1521.225097	15.185280
21.873565	1504.198135	15.190298
22.273391	1512.576306	15.195315
21.991609	1509.794641	15.200333
22.116808	1498.544881	15.205351
21.962894	1506.340979	15.210368
22.094553	1510.804279	15.215386
21.988179	1518.288655	15.220403
22.022494	1501.624667	15.225421
21.716046	1498.285391	15.230439
22.000424	1514.241735	15.235456
21.935973	1496.773777	15.240474
21.958785	1508.695384	15.245491
22.295216	1501.246602	15.250509
22.102770	1510.050526	15.255527
21.972220	1503.801405	15.260544
22.231675	1499.827687	15.265562
22.336486	1496.201207	15.270579
22.512431	1499.227673	15.275597
22.370592	1511.995604	15.280615
22.209975	1503.172776	15.285632
22.157054	1517.641790	15.290650
22.221295	1513.010024	15.295667
22.945704	1514.733817	15.300685
22.307291	1515.845397	15.305703
22.490580	1516.987986	15.310720
23.039210	1509.965059	15.315738
22.846284	1515.986595	15.320755
23.251393	1504.570522	15.325773
22.920659	1488.937627	15.330791
22.824130	1477.359739	15.335808
22.721727	1501.458347	15.340826
22.191292	1491.329315	15.345843
22.622448	1491.127289	15.350861
22.368623	1503.359213	15.355879
22.463181	1496.461218	15.360896
22.525049	1510.725470	15.365914
22.315475	1501.174278	15.370931
22.820411	1495.964584	15.375949
23.106012	1505.289281	15.380967
23.096023	1507.941934	15.385984
23.227472	1492.005544	15.391002
22.807186	1511.968826	15.396019
23.035562	1483.367682	15.401037
22.821113	1488.532419	15.406055
22.805305	1497.768759	15.411072
22.834914	1471.341358	15.416090
22.679525	1504.321597	15.421107
22.902712	1485.493805	15.426125
23.072629	1497.017750	15.431143
23.312725	1520.464151	15.436160
23.266094	1500.859253	15.441178
22.786413	1490.646949	15.446195
23.130296	1497.409118	15.451213
22.859490	1492.656483	15.456231
23.365607	1524.229603	15.461248
23.499702	1527.553773	15.466266
23.498626	1508.731719	15.471283
23.357909	1507.367083	15.476301
23.167454	1497.533364	15.481319
23.327311	1476.486118	15.486336
23.350907	1498.375892	15.491354
23.073561	1478.988833	15.496371
23.369342	1494.246672	15.501389
23.357821	1477.862666	15.506407
23.440303	1488.306507	15.511424
23.476475	1498.154694	15.516442
23.394186	1505.802371	15.521459
23.514890	1473.314763	15.526477
23.418847	1482.676435	15.531495
23.253996	1495.886151	15.536512
23.070013	1494.413534	15.541530
23.179702	1516.229572	15.546547
23.391951	1516.206405	15.551565
23.312863	1517.409868	15.556583
22.962567	1525.996238	15.561600
23.156947	1523.084715	15.566618
23.040728	1518.708998	15.571635
23.574897	1548.898401	15.576653
23.532273	1556.691682	15.581671
23.270013	1540.583245	15.586688
23.779701	1542.841039	15.591706
23.713793	1552.441914	15.596723
23.707867	1543.519599	15.601741
23.730636	1548.494106	15.606759
23.465942	1552.010040	15.611776
23.912302	1533.238499	15.616794
23.740725	1550.263322	15.621811
23.748337	1552.701997	15.626829
23.749595	1553.295167	15.631847
23.840785	1542.576080	15.636864
23.977441	1552.857995	15.641882
23.986068	1567.466263	15.646899
24.149682	1576.747100	15.651917
23.914831	1564.052384	15.656935
23.928782	1549.236888	15.661952
24.222044	1560.026280	15.666970
24.295560	1581.824871	15.671987
24.340341	1563.010130	15.677005
24.233062	1567.081329	15.682023
24.333431	1558.713365	15.687040
24.571296	1549.843161	15.692058
24.126623	1542.683441	15.697075
24.293248	1530.508504	15.702093
24.221820	1556.123309	15.707111
23.853651	1556.405853	15.712128
24.368603	1539.853303	15.717146
24.276528	1567.426534	15.722163
24.420117	1567.841591	15.727181
24.503527	1567.636018	15.732199
24.421055	1587.672387	15.737216
24.732815	1564.378831	15.742234
24.488702	1565.398293	15.747251
24.498476	1552.449231	15.752269
24.384183	1538.141351	15.757287
24.345829	1555.400901	15.762304
24.369302	1574.929004	15.767322
24.721104	1562.685261	15.772339
24.522855	1589.838670	15.777357
24.568741	1581.781208	15.782375
24.176034	1576.847256	15.787392
24.519834	1574.178299	15.792410
24.312328	1583.163259	15.797427
24.430411	1584.293897	15.802445
24.525090	1568.289110	15.807463
24.437714	1577.904865	15.812480
24.646544	1577.328050	15.817498
24.785098	1591.747386	15.822515
25.137322	1593.527772	15.827533
25.014608	1609.191818	15.832551
24.845243	1591.306731	15.837568
25.059747	1560.777039	15.842586
24.537659	1584.846037	15.847603
25.006036	1612.089874	15.852621
25.255236	1599.116067	15.857639
24.923884	1600.988257	15.862656
25.213475	1589.928345	15.867674
25.199046	1588.788745	15.872691
25.406977	1592.443865	15.877709
25.732020	1578.352263	15.882727
25.534058	1561.081552	15.887744
25.644991	1559.019757	15.892762
25.426838	1577.761393	15.897779
25.215278	1570.256412	15.902797
25.494308	1570.098810	15.907815
25.194242	1582.581104	15.912832
25.475415	1561.008486	15.917850
25.490164	1552.951953	15.922867
25.147936	1555.683528	15.927885
25.050744	1568.697127	15.932903
24.728212	1571.549931	15.937920
25.135256	1550.514283	15.942938
25.213795	1567.253062	15.947955
25.006501	1557.427893	15.952973
25.169454	1568.986894	15.957991
24.984271	1594.193584	15.963008
25.370799	1606.793984	15.968026
25.566030	1592.396822	15.973043
25.572344	1592.021350	15.978061
25.571375	1599.175225	15.983079
25.596907	1609.526908	15.988096
26.017301	1596.317967	15.993114
25.864949	1594.728718	15.998131
25.533115	1606.572913	16.003149
26.103219	1593.803212	16.008167
25.774735	1585.908182	16.013184
25.924282	1593.872635	16.018202
25.821822	1579.166683	16.023219
25.855050	1575.945730	16.028237
25.929211	1581.467641	16.033255
25.701282	1579.956913	16.038272
25.985269	1587.271720	16.043290
26.068860	1589.025448	16.048307
25.880879	1590.737851	16.053325
26.163697	1568.587119	16.058343
26.178752	1570.905105	16.063360
25.823918	1550.658504	16.068378
26.139300	1574.794662	16.073395
26.056840	1588.435631	16.078413
26.261268	1569.030250	16.083431
25.761122	1562.400738	16.088448
25.930788	1588.332374	16.093466
26.162195	1592.439227	16.098483
25.583827	1590.850117	16.103501
25.759660	1597.557933	16.108519
25.739107	1607.926579	16.113536
25.775460	1587.219601	16.118554
26.078096	1617.598451	16.123571
25.877527	1615.114994	16.128589
26.087993	1613.974442	16.133607
26.007064	1640.596948	16.138624
26.375022	1630.335799	16.143642
26.527466	1619.568847	16.148659
26.474221	1631.658203	16.153677
26.513766	1621.414231	16.158695
26.264899	1620.707972	16.163712
26.667338	1620.361312	16.168730
26.487643	1642.987496	16.173747
26.522335	1628.304098	16.178765
26.568286	1603.254683	16.183783
26.553094	1618.251698	16.188800
26.695164	1624.479085	16.193818
26.787679	1615.580215	16.198835
26.532682	1618.741683	16.203853
26.529458	1628.036639	16.208871
26.732663	1609.209833	16.213888
26.741737	1607.521481	16.218906
26.795405	1628.156832	16.223923
26.731257	1654.215977	16.228941
26.949910	1645.771738	16.233959
26.811859	1653.751766	16.238976
27.137698	1650.572189	16.243994
26.981845	1616.992318	16.249011
27.129550	1641.137396	16.254029
27.324871	1624.695238	16.259047
26.814238	1615.461778	16.264064
27.080395	1623.655646	16.269082
27.042502	1614.398190	16.274099
27.075458	1596.605719	16.279117
27.437719	1601.355674	16.284135
27.025118	1622.730330	16.289152
27.052553	1621.590994	16.294170
27.486989	1608.787609	16.299187
27.019909	1595.721583	16.304205
27.318892	1600.082177	16.309223
27.344317	1624.620191	16.314240
27.106536	1616.678175	16.319258
27.075740	1618.022257	16.324275
27.184836	1622.889038	16.329293
27.590301	1627.525191	16.334311
27.372066	1636.504575	16.339328
27.454377	1641.792532	16.344346
27.662015	1648.445322	16.349363
27.426390	1637.871691	16.354381
27.510367	1640.953925	16.359399
27.742278	1633.462619	16.364416
27.312439	1624.532371	16.369434
27.694250	1624.205848	16.374451
27.337228	1640.420547	16.379469
27.340928	1643.687763	16.384487
27.573629	1630.853832	16.389504
27.665183	1625.962354	16.394522
27.858740	1639.925496	16.399539
27.283855	1655.682614	16.404557
27.297706	1641.656450	16.409575
27.437037	1630.358599	16.414592
27.418784	1648.080386	16.419610
27.755363	1662.736597	16.424627
27.912234	1690.526733	16.429645
28.154738	1675.591277	16.434663
28.107746	1660.992985	16.439680
27.925986	1661.564347	16.444698
28.282603	1671.043123	16.449715
27.953692	1673.033791	16.454733
28.088988	1674.224079	16.459751
27.832695	1666.595662	16.464768
28.138314	1675.566833	16.469786
28.428859	1663.071178	16.474803
28.264789	1662.657928	16.479821
28.270464	1656.237643	16.484839
28.639611	1674.146474	16.489856
28.256081	1661.031553	16.494874
28.601847	1653.483538	16.499891
27.933021	1660.479748	16.504909
28.274495	1656.883104	16.509927
28.305378	1664.226489	16.514944
28.087589	1675.398875	16.519962
28.245576	1669.304819	16.524979
28.229028	1661.174284	16.529997
28.543082	1661.189893	16.535015
28.366391	1660.136538	16.540032
28.109937	1673.789705	16.545050
28.481205	1663.940205	16.550067
28.513401	1670.888870	16.555085
28.353273	1675.341787	16.560103
28.258809	1650.111702	16.565120
28.198780	1645.703341	16.570138
28.212029	1671.477735	16.575155
28.551423	1690.796037	16.580173
28.833190	1684.587741	16.585191
28.746149	1709.950021	16.590208
28.600098	1704.549271	16.595226
28.878242	1681.835385	16.600243
28.552913	1676.483262	16.605261
28.638635	1690.629689	16.610279
28.993684	1701.848449	16.615296
28.939605	1687.787611	16.620314
29.099798	1683.452669	16.625331
28.964004	1691.835116	16.630349
29.172583	1673.476636	16.635367
29.284588	1685.732291	16.640384
28.871865	1686.246662	16.645402
29.290709	1693.249137	16.650419
29.072960	1701.170524	16.655437
29.234760	1682.286408	16.660455
29.056911	1690.318102	16.665472
28.589938	1693.339747	16.670490
28.848505	1689.770671	16.675507
29.021281	1713.546342	16.680525
29.170167	1733.355436	16.685543
29.509191	1721.998638	16.690560
29.581954	1711.790151	16.695578
29.822465	1716.136134	16.700595
29.292771	1733.220338	16.705613
29.394304	1704.284400	16.710631
29.639939	1724.772827	16.715648
29.343709	1729.837108	16.720666
29.642004	1701.776155	16.725683
29.623284	1724.349977	16.730701
29.644319	1709.321880	16.735719
30.060690	1699.034873	16.740736
29.872300	1706.779892	16.745754
30.064816	1691.085317	16.750771
29.761337	1680.037338	16.755789
29.896474	1693.265355	16.760807
30.065424	1671.199715	16.765824
29.683231	1659.880761	16.770842
29.944370	1678.553847	16.775859
29.640941	1685.281659	16.780877
29.862050	1668.020793	16.785895
30.316655	1685.233667	16.790912
29.836891	1677.028519	16.795930
30.237965	1662.507432	16.800947
29.853976	1675.901812	16.805965
29.792459	1664.822323	16.810983
30.192292	1661.105821	16.816000
30.096423	1678.484342	16.821018
30.149535	1668.724709	16.826035
29.664720	1676.462801	16.831053
29.839512	1663.714381	16.836071
30.219325	1692.563419	16.841088
29.978190	1712.008776	16.846106
30.223745	1704.569206	16.851123
30.483497	1687.093313	16.856141
30.105675	1690.825177	16.861159
30.291059	1703.469426	16.866176
30.107242	1717.672522	16.871194
30.638738	1686.918281	16.876211
30.053746	1702.356021	16.881229
30.374718	1686.796885	16.886247
30.311173	1693.451800	16.891264
30.241600	1717.846639	16.896282
30.733928	1718.070045	16.901299
30.525338	1704.460721	16.906317
30.383234	1713.796588	16.911335
30.590421	1690.218017	16.916352
30.416432	1690.167750	16.921370
30.387025	1709.808974	16.926387
30.401963	1733.025049	16.931405
30.594612	1727.648818	16.936423
31.029522	1738.684264	16.941440
31.026366	1729.389213	16.946458
31.082627	1719.958784	16.951475
30.986371	1730.592235	16.956493
30.850753	1746.676384	16.961511
31.294198	1750.837987	16.966528
30.972620	1732.782749	16.971546
31.106005	1705.314478	16.976563
30.923500	1727.730369	16.981581
30.658746	1734.190447	16.986599
30.872746	1738.221590	16.991616
30.963187	1726.413150	16.996634
31.483222	1736.616879	17.001651
31.241913	1734.328876	17.006669
31.285484	1717.349308	17.011687
31.494906	1724.176605	17.016704
31.282410	1730.510254	17.021722
31.399990	1733.046511	17.026739
31.424880	1742.139883	17.031757
31.512084	1743.204883	17.036775
31.581738	1721.132159	17.041792
31.468693	1730.108779	17.046810
31.123403	1732.042724	17.051827
31.600711	1715.817499	17.056845
31.534039	1718.922872	17.061863
31.511454	1704.318340	17.066880
31.464984	1731.642352	17.071898
31.840714	1720.142706	17.076915
31.637503	1725.158549	17.081933
31.071991	1736.256872	17.086951
31.561502	1715.250080	17.091968
31.629317	1715.090281	17.096986
31.441654	1723.324853	17.102003
31.789232	1721.966006	17.107021
31.580343	1721.878108	17.112039
31.640315	1717.663634	17.117056
31.716506	1748.164299	17.122074
31.952618	1754.078916	17.127091
31.993148	1748.720532	17.132109
31.547788	1762.973778	17.137127
31.961703	1741.752026	17.142144
31.824566	1750.253798	17.147162
31.661110	1759.424456	17.152179
32.235847	1742.215088	17.157197
31.548447	1755.974966	17.162215
31.965249	1755.561672	17.167232
32.145168	1767.564584	17.172250
32.338884	1752.923377	17.177267
32.303431	1748.890968	17.182285
32.101913	1758.673306	17.187303
32.608442	1757.787992	17.192320
32.829431	1759.841707	17.197338
32.243537	1764.521077	17.202355
32.730345	1746.977386	17.207373
32.251596	1754.118669	17.212391
32.826206	1744.755786	17.217408
32.239446	1734.170539	17.222426
32.526114	1744.134546	17.227443
32.570048	1749.556908	17.232461
32.202224	1747.697011	17.237479
32.459105	1743.182525	17.242496
32.690452	1765.562360	17.247514
32.561102	1784.579378	17.252531
33.080440	1776.721475	17.257549
32.884337	1772.877583	17.262567
33.080076	1759.317317	17.267584
32.954038	1770.445187	17.272602
32.824209	1756.398378	17.277619
32.733255	1751.984470	17.282637
32.300350	1762.344112	17.287655
32.591336	1760.666332	17.292672
32.874266	1774.382100	17.297690
32.747702	1759.851281	17.302707
32.984138	1768.464820	17.307725
32.566544	1793.239469	17.312743
32.963750	1770.242935	17.317760
32.850259	1776.067624	17.322778
33.023028	1796.354353	17.327795
33.410395	1789.222935	17.332813
33.181944	1806.657952	17.337831
33.225553	1797.910239	17.342848
33.542160	1797.260302	17.347866
33.479569	1813.944932	17.352883
33.591363	1798.473192	17.357901
33.663790	1791.646030	17.362919
33.606198	1772.704178	17.367936
33.407312	1784.232700	17.372954
33.617080	1764.080963	17.377971
33.611769	1768.569039	17.382989
33.499605	1766.007378	17.388007
33.463838	1759.900234	17.393024
33.493276	1773.580248	17.398042
33.570115	1804.057497	17.403059
33.677094	1788.231908	17.408077
33.577224	1801.789052	17.413095
33.700735	1802.354944	17.418112
33.721198	1794.567858	17.423130
33.654696	1796.457611	17.428147
33.760143	1794.428083	17.433165
33.555222	1805.219378	17.438183
33.921139	1790.105574	17.443200
33.545341	1793.628015	17.448218
33.344204	1803.467395	17.453235
33.808797	1794.403807	17.458253
33.794507	1816.959616	17.463271
33.957924	1830.378808	17.468288
34.119804	1826.999955	17.473306
33.994512	1809.264287	17.478323
34.076829	1817.416802	17.483341
34.068411	1814.498686	17.488359
34.373220	1806.225618	17.493376
34.010153	1824.565010	17.498394
34.289877	1820.509628	17.503411
34.420080	1816.674882	17.508429
34.242949	1829.348240	17.513447
34.297476	1838.804122	17.518464
34.468984	1833.908124	17.523482
34.591322	1848.365513	17.528499
35.207408	1828.131592	17.533517
34.577492	1821.399616	17.538535
34.749872	1797.332339	17.543552
34.834495	1791.789523	17.548570
34.849023	1813.397050	17.553587
35.085582	1799.833054	17.558605
34.910432	1800.898113	17.563623
35.130281	1777.906175	17.568640
35.145358	1798.682752	17.573658
35.242548	1796.733214	17.578675
35.384466	1787.261822	17.583693
35.161558	1800.119950	17.588711
35.087487	1779.367290	17.593728
35.124362	1761.060304	17.598746
34.798310	1768.260399	17.603763
35.063933	1786.528331	17.608781
34.716742	1772.841967	17.613799
35.190815	1770.459164	17.618816
35.148405	1783.660803	17.623834
34.947535	1794.049335	17.628851
35.280359	1813.143529	17.633869
34.833108	1806.019929	17.638887
35.085691	1787.304307	17.643904
35.015101	1787.737051	17.648922
34.838270	1800.273945	17.653939
35.175690	1803.158456	17.658957
34.954697	1797.176769	17.663975
35.526588	1804.060618	17.668992
35.652611	1823.136449	17.674010
35.457752	1818.996728	17.679027
35.663969	1810.923279	17.684045
35.440703	1827.829220	17.689063
35.412356	1819.722396	17.694080
35.626478	1836.011589	17.699098
35.319242	1835.104081	17.704115
35.354603	1807.294513	17.709133
35.377567	1818.989412	17.714151
35.599285	1836.839546	17.719168
35.642874	1827.802603	17.724186
35.578564	1827.327203	17.729203
35.640036	1850.168811	17.734221
35.591879	1851.357052	17.739239
35.566262	1852.822617	17.744256
36.010559	1857.305799	17.749274
36.053669	1851.546145	17.754291
35.902636	1867.710315	17.759309
35.824502	1845.463151	17.764327
36.098766	1838.528123	17.769344
36.162552	1857.226561	17.774362
35.865243	1857.213891	17.779379
36.508780	1870.943961	17.784397
36.292772	1883.864588	17.789415
36.395316	1864.559611	17.794432
36.772933	1846.710585	17.799450
36.449409	1866.014662	17.804467
36.483132	1846.744500	17.809485
36.288033	1849.661418	17.814503
36.679662	1869.874782	17.819520
36.698184	1849.727868	17.824538
36.251333	1836.892892	17.829555
36.574680	1852.498336	17.834573
37.027221	1874.142012	17.839591
36.837500	1864.126967	17.844608
36.882209	1847.657008	17.849626
36.970793	1853.329262	17.854643
37.021188	1834.937981	17.859661
36.731150	1840.483660	17.864679
36.833462	1837.469107	17.869696
36.810780	1849.787890	17.874714
36.488033	1845.601394	17.879731
36.920432	1862.376590	17.884749
37.172215	1860.178805	17.889767
36.998026	1874.447962	17.894784
37.159125	1879.589249	17.899802
36.984146	1873.378513	17.904819
37.040358	1879.326547	17.909837
37.359681	1875.527746	17.914855
37.008264	1883.538526	17.919872
37.235750	1881.494823	17.924890
37.205371	1876.468326	17.929907
37.255377	1884.168430	17.934925
37.410210	1875.213845	17.939943
37.258797	1873.144189	17.944960
37.368308	1865.917045	17.949978
37.211107	1889.192702	17.954995
37.107226	1869.614210	17.960013
37.231579	1858.706682	17.965031
37.579108	1887.724483	17.970048
37.595711	1904.912562	17.975066
37.372591	1911.711240	17.980083
37.786877	1891.861008	17.985101
37.627504	1887.188142	17.990119
37.553805	1899.342594	17.995136
38.090648	1897.817935	18.000154
38.083715	1892.331051	18.005171
38.020094	1912.167228	18.010189
37.776566	1896.650384	18.015207
37.950625	1888.532809	18.020224
38.102577	1881.076541	18.025242
37.955900	1901.156305	18.030259
38.097132	1902.610344	18.035277
38.159173	1904.827917	18.040295
37.740957	1911.717977	18.045312
38.088661	1896.161002	18.050330
37.836421	1896.394577	18.055347
38.031106	1894.640490	18.060365
38.170358	1887.618420	18.065383
38.091674	1899.037418	18.070400
38.294619	1927.167352	18.075418
38.042082	1941.557371	18.080435
38.382732	1914.056642	18.085453
38.708024	1920.345391	18.090471
38.175470	1939.171304	18.095488
38.383729	1920.677077	18.100506
38.283616	1937.467825	18.105523
38.215477	1936.734441	18.110541
38.386156	1910.786125	18.115559
38.310554	1935.386402	18.120576
38.683366	1942.676469	18.125594
38.745028	1945.148885	18.130611
38.704932	1958.987377	18.135629
38.651931	1966.558705	18.140647
38.578281	1954.091998	18.145664
38.974162	1943.324152	18.150682
38.995964	1951.998258	18.155699
38.983644	1941.285467	18.160717
39.032133	1950.647650	18.165735
38.825363	1969.011575	18.170752
39.326731	1947.287581	18.175770
39.210489	1941.653419	18.180787
39.276176	1956.518426	18.185805
39.123403	1949.811266	18.190823
39.065790	1954.168105	18.195840
39.074217	1937.203942	18.200858
39.309418	1955.990196	18.205875
39.359294	1976.321876	18.210893
39.448998	1985.718207	18.215911
39.581000	1986.176522	18.220928
39.511050	1993.286773	18.225946
39.687458	1994.362833	18.230963
39.594634	1966.955977	18.235981
39.995082	1963.617775	18.240999
39.742591	1983.353782	18.246016
39.805926	1968.629112	18.251034
39.600016	1972.617817	18.256051
39.579078	1985.482580	18.261069
39.909574	1970.819941	18.266087
39.685751	1967.841050	18.271104
39.986426	1967.758595	18.276122
39.983569	1990.844365	18.281139
39.758686	1978.632016	18.286157
40.206627	1983.349334	18.291175
40.166812	1990.385916	18.296192
40.369449	1959.055473	18.301210
40.407927	1968.285193	18.306227
40.189659	1984.622081	18.311245
40.279242	1959.454659	18.316263
40.075314	1972.874453	18.321280
40.330737	1976.643350	18.326298
40.332157	1966.151853	18.331315
40.020931	1972.232872	18.336333
40.243448	1971.029192	18.341351
40.264285	1975.108949	18.346368
40.588158	1965.064863	18.351386
40.386778	1987.054311	18.356403
40.254801	1967.325642	18.361421
40.808898	1947.004287	18.366439
40.086627	1974.656211	18.371456
40.738995	1958.772108	18.376474
40.927591	1963.699568	18.381491
40.612835	1970.344746	18.386509
40.623361	1977.614789	18.391527
40.860650	1982.403032	18.396544
40.980970	1988.130219	18.401562
40.997975	1986.540891	18.406579
40.890229	2000.548543	18.411597
40.986830	1987.701870	18.416615
40.848611	1990.818530	18.421632
41.074836	2003.126614	18.426650
40.805008	1993.979584	18.431667
40.734486	2001.956113	18.436685
41.115047	1987.629905	18.441703
40.882088	1993.071441	18.446720
41.053524	1998.814197	18.451738
40.820840	2008.621820	18.456755
41.246205	2025.552660	18.461773
41.638841	2031.506272	18.466791
41.333388	2029.792205	18.471808
41.180305	2005.381901	18.476826
41.351683	2016.632031	18.481843
41.620375	2035.047855	18.486861
41.740749	2020.292749	18.491879
41.916337	2007.950826	18.496896
41.808770	2018.817997	18.501914
41.903717	2017.721796	18.506931
41.712835	2017.746548	18.511949
42.017063	2028.544793	18.516967
42.033132	2030.924776	18.521984
41.924960	2024.218086	18.527002
42.010351	2021.025224	18.532019
42.029032	2027.416446	18.537037
42.377491	2018.379496	18.542055
41.766714	2019.905657	18.547072
42.090973	2019.162043	18.552090
42.288386	2016.469768	18.557107
42.032924	2014.882064	18.562125
42.173192	2011.425064	18.567143
41.798791	2017.585622	18.572160
42.067429	2012.175675	18.577178
42.306779	2017.030800	18.582195
41.969854	2042.917512	18.587213
42.394768	2037.903310	18.592231
42.051666	2054.020492	18.597248
42.392407	2059.864502	18.602266
42.607865	2041.946099	18.607283
42.561655	2047.196391	18.612301
42.404168	2050.814483	18.617319
42.280188	2041.281775	18.622336
42.256996	2048.316128	18.627354
42.717043	2060.204292	18.632371
42.766519	2082.736571	18.637389
42.490682	2072.806669	18.642407
42.698241	2079.928081	18.647424
42.814800	2066.489075	18.652442
42.800116	2079.122510	18.657459
42.725224	2097.225271	18.662477
42.871388	2073.042329	18.667495
42.875920	2085.887221	18.672512
42.675118	2083.088821	18.677530
43.200832	2082.511879	18.682547
43.354910	2102.444193	18.687565
43.498321	2092.952587	18.692583
43.504069	2096.624214	18.697600
43.675484	2094.432788	18.702618
43.941656	2087.344387	18.707635
43.440991	2063.886837	18.712653
43.813444	2058.348519	18.717671
43.566241	2070.702022	18.722688
43.656415	2061.219724	18.727706
43.794217	2068.833576	18.732723
43.912691	2067.159964	18.737741
43.838923	2061.243100	18.742759
44.028508	2067.865204	18.747776
43.780082	2056.886974	18.752794
43.986770	2061.822891	18.757811
43.514703	2072.181241	18.762829
43.629749	2051.472343	18.767847
43.924650	2075.770621	18.772864
43.591130	2079.278661	18.777882
43.763217	2071.606610	18.782899
43.884922	2077.469995	18.787917
44.173203	2095.858939	18.792935
44.177797	2103.191330	18.797952
44.168416	2088.661304	18.802970
44.241584	2102.395496	18.807987
44.147866	2096.103438	18.813005
44.472620	2073.257180	18.818023
44.046512	2081.562441	18.823040
44.152643	2102.096962	18.828058
44.325077	2089.756872	18.833075
44.202822	2110.761548	18.838093
44.194265	2116.023846	18.843111
44.608439	2115.814092	18.848128
44.695500	2106.904424	18.853146
44.815197	2126.012872	18.858163
44.726514	2123.248389	18.863181
44.989634	2125.568077	18.868199
44.974745	2129.584500	18.873216
44.911754	2117.541316	18.878234
45.236781	2102.891954	18.883251
45.141758	2118.022214	18.888269
45.297122	2125.488335	18.893287
45.041911	2126.382130	18.898304
45.029505	2108.147724	18.903322
45.535424	2106.332638	18.908339
45.090334	2106.732114	18.913357
45.064219	2106.399776	18.918375
45.278439	2114.908048	18.923392
45.301998	2121.241524	18.928410
45.495858	2096.840366	18.933427
45.549338	2112.990483	18.938445
45.444603	2116.056958	18.943463
45.589855	2105.690194	18.948480
45.155780	2117.137279	18.953498
45.457619	2114.669028	18.958515
45.111697	2109.865138	18.963533
45.225912	2114.007736	18.968551
45.628525	2107.727144	18.973568
45.290322	2105.573677	18.978586
45.446869	2130.375430	18.983603
45.791197	2143.229071	18.988621
45.974686	2133.267906	18.993639
45.909727	2152.896580	18.998656
45.562009	2132.960574	19.003674
46.223293	2124.320708	19.008691
46.032344	2138.467213	19.013709
45.639462	2144.879749	19.018727
46.057108	2129.533285	19.023744
45.730705	2147.753440	19.028762
46.205836	2148.277480	19.033779
46.050384	2149.446571	19.038797
46.197023	2140.167850	19.043815
46.275149	2153.404307	19.048832
46.475847	2147.017720	19.053850
46.645364	2137.505535	19.058867
45.753612	2146.472516	19.063885
46.535741	2147.287597	19.068903
46.513718	2150.317088	19.073920
46.444346	2138.058249	19.078938
46.542751	2134.914877	19.083955
46.728365	2170.511188	19.088973
46.939682	2166.843923	19.093991
46.966786	2167.805616	19.099008
46.741489	2148.555539	19.104026
46.946838	2156.163684	19.109043
47.186593	2172.850013	19.114061
46.909167	2171.374170	19.119079
47.107311	2155.467894	19.124096
47.326087	2153.571435	19.129114
47.255797	2158.961645	19.134131
47.177085	2172.966821	19.139149
47.242623	2165.427862	19.144167
47.324499	2162.463169	19.149184
47.170317	2172.225942	19.154202
47.353222	2154.863282	19.159219
47.287281	2151.112332	19.164237
47.009216	2172.601716	19.169255
47.667653	2173.384885	19.174272
47.398851	2172.869459	19.179290
47.878893	2177.117638	19.184307
47.803924	2192.146052	19.189325
48.073713	2170.342118	19.194343
47.712254	2173.768984	19.199360
47.522303	2181.618319	19.204378
47.624300	2180.366441	19.209395
47.705111	2195.911839	19.214413
47.854055	2206.414861	19.219431
48.012518	2196.437715	19.224448
47.838198	2191.442478	19.229466
47.978853	2199.840730	19.234483
48.142070	2193.818228	19.239501
48.051136	2191.911241	19.244519
47.879675	2189.917578	19.249536
48.218117	2193.524510	19.254554
48.006481	2202.668261	19.259571
48.155617	2201.403770	19.264589
48.118873	2207.930287	19.269607
48.427619	2219.551008	19.274624
48.360340	2232.173283	19.279642
48.401882	2208.391014	19.284659
48.634251	2194.509208	19.289677
48.524525	2208.004866	19.294695
48.918777	2205.158793	19.299712
48.730662	2209.905907	19.304730
48.768277	2202.275103	19.309747
48.824612	2203.898488	19.314765
48.595191	2220.540372	19.319783
49.456818	2237.050990	19.324800
49.369944	2210.502414	19.329818
49.203257	2190.432697	19.334835
49.023727	2194.604863	19.339853
49.056180	2207.546211	19.344871
49.183925	2221.797977	19.349888
49.244676	2228.845309	19.354906
49.349498	2221.720625	19.359923
49.530144	2230.736983	19.364941
49.277022	2217.934426	19.369959
49.933978	2231.495704	19.374976
49.628782	2238.934361	19.379994
49.613752	2213.516236	19.385011
49.701837	2193.175713	19.390029
49.551487	2203.823647	19.395047
49.917393	2201.849238	19.400064
49.456884	2210.291529	19.405082
49.281057	2225.748384	19.410099
49.117864	2241.829636	19.415117
49.250325	2235.545316	19.420135
50.034351	2224.265770	19.425152
49.669104	2221.311182	19.430170
50.041924	2252.855580	19.435187
50.217525	2263.779166	19.440205
49.791387	2261.587657	19.445223
49.802493	2238.969625	19.450240
49.886103	2255.695623	19.455258
50.033967	2274.851563	19.460275
50.083043	2262.288747	19.465293
50.111044	2257.110081	19.470311
50.302138	2253.167051	19.475328
50.503629	2276.509690	19.480346
50.578467	2296.325451	19.485363
50.870364	2286.939286	19.490381
50.640269	2266.980520	19.495399
50.912257	2282.019788	19.500416
50.941847	2277.303178	19.505434
50.951654	2273.230283	19.510451
51.287166	2277.780280	19.515469
51.340884	2271.575088	19.520487
51.470503	2236.444474	19.525504
51.045152	2247.082181	19.530522
50.824207	2244.183848	19.535539
51.246994	2238.599852	19.540557
51.116756	2242.045503	19.545575
50.987842	2237.109665	19.550592
50.864860	2255.065861	19.555610
51.284746	2269.498491	19.560627
51.598470	2254.458890	19.565645
51.476180	2261.801991	19.570663
51.601946	2279.056000	19.575680
51.712015	2296.180950	19.580698
51.133783	2277.676319	19.585715
51.312049	2266.391543	19.590733
51.301104	2273.358239	19.595751
51.410007	2278.861475	19.600768
51.341204	2272.430900	19.605786
51.441941	2266.397438	19.610803
51.978055	2273.695122	19.615821
51.893750	2313.706905	19.620839
51.690383	2295.969109	19.625856
51.919052	2288.337199	19.630874
51.992293	2318.225020	19.635891
52.214050	2310.545824	19.640909
51.627104	2303.964870	19.645927
52.177560	2302.923771	19.650944
52.121703	2306.208154	19.655962
52.065286	2282.924554	19.660979
52.207460	2299.865690	19.665997
52.205545	2302.713866	19.671015
52.147968	2297.445801	19.676032
52.847181	2302.152599	19.681050
52.675638	2315.895141	19.686067
53.131788	2317.790606	19.691085
52.419492	2315.266712	19.696103
52.619988	2298.357897	19.701120
52.766788	2297.131967	19.706138
52.502398	2318.929874	19.711155
53.204639	2333.396013	19.716173
52.782455	2322.652078	19.721191
53.089582	2304.541183	19.726208
53.077610	2307.962779	19.731226
53.031625	2332.633589	19.736243
53.404941	2334.745270	19.741261
53.312188	2321.881485	19.746279
53.358984	2308.948399	19.751296
53.149232	2314.909356	19.756314
52.984222	2326.086876	19.761331
53.420796	2313.329693	19.766349
52.841583	2315.112236	19.771367
53.230217	2309.636007	19.776384
53.204225	2331.749598	19.781402
53.695908	2335.601277	19.786419
53.842059	2353.213556	19.791437
53.441349	2366.997161	19.796455
53.408775	2342.972640	19.801472
53.216309	2349.841828	19.806490
53.321904	2357.488798	19.811507
53.619658	2371.752564	19.816525
53.470076	2378.999656	19.821543
53.527296	2365.895535	19.826560
53.668547	2365.428073	19.831578
53.338612	2378.139138	19.836595
53.808504	2407.675611	19.841613
54.218098	2412.209273	19.846631
54.438763	2395.667827	19.851648
54.430177	2410.856916	19.856666
54.571842	2386.170564	19.861683
54.473009	2381.560956	19.866701
54.609012	2395.102576	19.871719
54.425188	2399.714808	19.876736
54.639436	2383.970766	19.881754
54.630795	2381.069997	19.886771
55.195041	2391.349230	19.891789
54.917164	2412.534634	19.896807
55.043532	2404.013021	19.901824
55.136650	2387.527694	19.906842
54.968024	2375.805750	19.911859
55.045535	2378.823267	19.916877
55.251797	2397.497345	19.921895
54.781235	2385.442670	19.926912
55.031247	2391.069456	19.931930
54.815246	2380.989527	19.936947
54.885221	2376.614977	19.941965
55.423011	2412.953529	19.946983
55.550541	2426.582192	19.952000
55.613877	2431.310261	19.957018
55.454519	2422.443196	19.962035
56.008828	2411.757490	19.967053
55.648748	2413.705966	19.972071
55.572381	2393.229781	19.977088
55.731154	2393.633497	19.982106
55.532957	2407.267354	19.987123
55.939326	2414.780806	19.992141
55.923806	2417.840078	19.997159
55.992872	2417.712837	20.002176
56.226938	2407.650238	20.007194
56.087116	2402.339044	20.012211
56.473039	2417.240346	20.017229
56.152590	2404.414117	20.022247
56.291523	2403.635275	20.027264
56.329814	2420.168185	20.032282
56.398888	2417.159504	20.037299
56.549208	2399.446398	20.042317
56.347911	2398.329351	20.047335
56.220710	2402.269536	20.052352
56.510127	2403.986690	20.057370
56.406299	2406.305946	20.062387
56.425409	2397.702863	20.067405
56.538249	2411.273320	20.072423
56.690819	2400.673098	20.077440
56.794798	2403.440812	20.082458
56.556867	2404.905397	20.087475
56.390745	2397.677199	20.092493
56.443060	2414.003881	20.097511
56.591952	2411.845458	20.102528
56.872602	2417.602013	20.107546
56.645442	2441.004713	20.112563
57.064050	2429.978679	20.117581
57.145650	2449.436685	20.122599
57.256215	2468.686418	20.127616
57.188938	2467.274033	20.132634
57.312495	2465.882468	20.137651
57.345810	2454.248337	20.142669
57.388606	2459.491934	20.147687
57.531385	2453.207788	20.152704
57.714514	2452.417703	20.157722
57.520957	2481.335912	20.162739
57.798365	2467.139773	20.167757
57.857471	2459.467697	20.172775
58.096517	2464.819200	20.177792
58.080498	2469.271461	20.182810
57.992120	2473.367626	20.187827
58.277094	2475.125083	20.192845
58.090816	2489.506929	20.197863
58.044117	2487.839408	20.202880
58.482175	2465.520908	20.207898
58.447433	2489.414640	20.212915
58.360308	2505.957738	20.217933
58.545869	2497.022022	20.222951
58.340211	2495.175484	20.227968
58.098834	2473.165475	20.232986
58.175081	2496.273081	20.238003
58.521804	2482.901764	20.243021
58.620932	2482.498927	20.248039
58.477855	2499.332521	20.253056
58.705401	2490.865193	20.258074
58.589888	2494.946559	20.263091
58.746410	2515.024850	20.268109
59.009973	2528.822633	20.273127
58.707475	2527.365265	20.278144
59.058951	2520.822230	20.283162
58.849108	2526.271942	20.288179
59.006744	2517.244781	20.293197
59.106729	2506.299488	20.298215
58.929122	2516.467765	20.303232
59.294197	2539.056717	20.308250
59.254129	2540.094779	20.313267
59.583739	2516.948384	20.318285
59.682156	2530.695320	20.323303
59.643385	2542.201297	20.328320
59.735839	2544.261008	20.333338
59.658672	2534.238143	20.338355
59.848153	2517.451166	20.343373
59.844712	2532.815679	20.348391
59.436447	2545.272149	20.353408
59.657513	2530.682959	20.358426
59.624265	2527.764382	20.363443
60.031312	2540.641552	20.368461
60.141682	2566.247978	20.373479
60.223478	2575.529656	20.378496
60.309212	2559.714361	20.383514
60.229574	2553.116389	20.388531
60.587700	2551.806313	20.393549
60.567997	2553.549568	20.398567
60.574387	2557.205946	20.403584
60.874826	2554.031860	20.408602
60.783625	2570.372975	20.413619
60.990784	2545.614137	20.418637
61.090541	2544.898052	20.423655
60.781692	2549.232410	20.428672
61.252507	2530.855064	20.433690
61.073851	2548.349611	20.438707
61.405330	2560.315209	20.443725
61.239493	2531.924477	20.448743
60.877308	2508.671969	20.453760
61.040140	2516.322748	20.458778
60.620634	2543.256272	20.463795
60.978710	2551.268054	20.468813
61.570995	2540.139434	20.473831
61.183170	2545.530978	20.478848
61.405745	2541.413210	20.483866
61.175432	2529.095330	20.488883
61.343267	2552.440211	20.493901
61.766258	2563.485115	20.498919
61.626149	2579.323964	20.503936
62.137473	2574.814822	20.508954
62.077079	2559.462193	20.513971
62.488838	2563.297811	20.518989
62.442677	2581.535548	20.524007
61.935145	2560.746190	20.529024
61.907655	2536.029881	20.534042
62.202627	2554.532034	20.539059
62.288806	2560.681157	20.544077
62.447951	2552.240450	20.549095
62.428822	2571.607792	20.554112
62.489010	2574.732723	20.559130
62.562314	2564.999889	20.564147
62.269813	2561.138659	20.569165
62.355603	2557.355845	20.574183
62.318460	2558.106263	20.579200
62.412945	2566.336190	20.584218
62.333043	2562.049730	20.589235
62.393424	2574.128826	20.594253
62.973578	2578.516853	20.599271
62.612324	2604.222925	20.604288
62.807954	2593.746735	20.609306
62.656849	2592.449750	20.614323
62.969640	2602.129038	20.619341
63.176957	2602.321617	20.624359
63.209064	2628.864963	20.629376
63.123583	2637.494692	20.634394
63.410372	2630.138992	20.639411
63.501470	2621.822664	20.644429
63.663061	2607.446547	20.649447
63.538808	2627.316299	20.654464
63.328277	2618.496351	20.659482
63.643941	2622.867671	20.664499
63.577117	2629.054307	20.669517
63.959581	2621.804832	20.674535
63.692283	2605.897650	20.679552
63.602874	2609.319316	20.684570
63.600774	2628.390257	20.689587
63.806907	2637.711458	20.694605
64.174352	2643.972186	20.699623
64.020952	2659.540911	20.704640
64.244235	2649.255165	20.709658
64.402719	2633.849367	20.714675
64.221831	2635.909185	20.719693
64.544120	2654.157176	20.724711
64.386128	2645.439342	20.729728
64.524010	2646.262993	20.734746
64.403245	2645.224536	20.739763
64.626878	2628.031261	20.744781
64.627828	2627.815486	20.749799
64.814039	2671.466831	20.754816
64.783986	2686.341673	20.759834
65.069292	2674.223671	20.764851
64.786919	2655.968076	20.769869
65.253622	2668.068872	20.774887
64.951689	2674.346141	20.779904
64.809917	2673.891387	20.784922
65.193657	2655.147429	20.789939
64.925872	2657.510939	20.794957
65.064429	2677.080868	20.799975
65.033985	2708.170865	20.804992
65.522468	2705.125890	20.810010
65.563674	2698.436637	20.815027
65.820994	2703.854288	20.820045
65.907653	2699.395208	20.825063
65.575099	2696.271564	20.830080
65.934609	2693.199681	20.835098
65.475958	2719.805775	20.840115
65.832228	2710.801772	20.845133
66.377737	2696.921897	20.850151
66.178329	2717.474762	20.855168
66.071377	2731.213889	20.860186
66.483810	2734.680199	20.865203
66.517251	2722.218594	20.870221
66.515261	2707.964479	20.875239
66.677051	2729.001299	20.880256
66.675728	2722.663308	20.885274
66.996358	2717.925829	20.890291
66.830647	2708.782717	20.895309
66.809156	2702.395515	20.900327
66.861871	2725.455196	20.905344
66.626781	2735.028868	20.910362
66.974203	2717.755204	20.915379
66.898758	2715.639517	20.920397
67.139825	2710.933098	20.925415
66.945498	2706.249814	20.930432
67.204242	2708.239162	20.935450
67.048215	2725.552242	20.940467
66.920641	2727.176746	20.945485
67.107030	2720.506991	20.950503
67.071320	2718.446147	20.955520
67.331182	2753.175162	20.960538
67.242062	2763.488013	20.965555
67.162390	2745.139377	20.970573
67.262280	2743.272039	20.975591
67.521331	2766.158334	20.980608
67.399068	2770.573127	20.985626
67.421400	2784.828860	20.990643
67.134116	2788.993011	20.995661
67.711901	2800.503978	21.000679
68.021989	2806.640608	21.005696
68.141494	2809.806368	21.010714
68.242555	2809.991316	21.015731
68.083391	2801.449154	21.020749
68.184578	2799.529239	21.025767
68.252231	2806.013959	21.030784
68.520467	2793.304274	21.035802
68.808141	2794.825528	21.040819
68.482059	2814.408638	21.045837
68.726774	2813.107835	21.050855
68.875868	2806.514078	21.055872
68.907446	2808.036514	21.060890
69.265079	2823.123374	21.065907
69.080057	2839.409815	21.070925
68.988402	2824.230963	21.075943
68.965738	2804.952482	21.080960
69.161698	2819.494673	21.085978
69.331023	2816.364637	21.090995
69.361050	2809.396708	21.096013
69.439796	2824.580828	21.101031
69.660250	2818.591926	21.106048
69.399093	2803.568843	21.111066
69.964758	2801.251746	21.116083
69.862378	2811.888040	21.121101
70.065201	2806.148481	21.126119
69.821305	2825.550331	21.131136
69.604097	2821.734066	21.136154
69.838887	2807.096880	21.141171
69.522396	2804.493129	21.146189
69.821469	2834.020663	21.151207
69.773012	2836.605011	21.156224
69.928411	2847.242821	21.161242
70.123167	2842.886688	21.166259
70.248488	2839.792655	21.171277
70.283393	2846.477463	21.176295
70.455080	2864.321315	21.181312
70.467534	2864.210117	21.186330
70.820613	2866.115796	21.191347
70.443868	2874.136783	21.196365
70.794157	2875.487286	21.201383
71.251729	2870.202002	21.206400
70.960668	2880.396352	21.211418
70.932926	2877.421884	21.216435
71.414745	2859.949104	21.221453
71.237710	2856.797169	21.226471
71.438907	2874.568449	21.231488
70.753872	2881.955233	21.236506
71.274705	2863.399367	21.241523
70.943735	2856.584560	21.246541
71.329811	2878.960136	21.251559
71.437792	2905.647897	21.256576
71.867805	2905.453727	21.261594
71.462829	2888.014472	21.266611
71.623713	2890.981114	21.271629
71.863430	2897.577383	21.276647
72.298430	2878.989034	21.281664
71.936861	2891.432357	21.286682
72.471467	2900.477815	21.291699
72.099044	2903.857936	21.296717
72.020313	2878.658070	21.301735
72.269201	2878.056483	21.306752
72.181735	2902.120768	21.311770
72.440803	2904.906248	21.316787
72.703675	2914.045231	21.321805
72.468018	2928.292552	21.326823
72.674539	2913.447955	21.331840
72.717163	2903.655221	21.336858
72.663066	2916.697087	21.341875
72.719861	2903.607538	21.346893
72.631056	2908.975777	21.351911
72.825326	2920.664170	21.356928
72.701946	2918.158394	21.361946
73.177963	2900.557803	21.366963
72.993418	2927.593508	21.371981
73.300281	2947.241470	21.376999
73.564783	2941.476513	21.382016
73.469081	2937.207517	21.387034
73.542859	2921.660920	21.392051
73.264369	2938.311292	21.397069
73.211152	2960.860745	21.402087
73.563585	2954.826364	21.407104
73.414306	2938.313384	21.412122
73.260019	2923.649643	21.417139
73.663279	2947.097936	21.422157
73.544259	2984.217354	21.427175
73.674618	2965.523353	21.432192
73.624545	2969.598558	21.437210
73.887757	2994.167374	21.442227
73.936077	2991.686948	21.447245
74.295862	2995.239960	21.452263
74.516211	3003.447946	21.457280
74.528815	3014.270669	21.462298
74.666534	2997.818653	21.467315
74.411980	2985.531771	21.472333
74.674543	3013.956368	21.477351
75.006743	3034.437163	21.482368
74.974774	3020.008993	21.487386
75.337435	3013.468628	21.492403
75.124910	3034.113047	21.497421
75.126094	3026.845096	21.502439
75.550298	3021.756985	21.507456
74.978678	3022.440249	21.512474
75.520729	3013.524453	21.517491
75.453301	3018.705361	21.522509
75.499114	3016.836101	21.527527
75.544330	2998.651740	21.532544
75.719173	3005.663846	21.537562
75.940402	3007.121897	21.542579
75.946758	3002.541172	21.547597
75.760264	3016.264960	21.552615
75.657833	3009.753422	21.557632
75.705972	3019.345421	21.562650
75.589430	3011.895773	21.567667
75.953528	3036.022445	21.572685
75.960796	3031.015429	21.577703
75.944820	3045.922146	21.582720
76.119759	3070.645615	21.587738
76.324462	3069.402577	21.592755
76.586165	3069.481268	21.597773
76.577836	3068.657050	21.602791
76.345383	3060.823231	21.607808
76.372623	3069.876848	21.612826
76.649168	3077.119397	21.617843
76.679096	3088.795906	21.622861
76.569980	3107.080882	21.627879
76.893321	3108.467746	21.632896
76.843974	3095.499695	21.637914
77.398152	3096.277021	21.642931
77.507899	3104.991078	21.647949
77.101353	3116.055357	21.652967
77.656492	3105.175556	21.657984
77.553710	3125.658672	21.663002
77.725862	3116.983644	21.668019
77.880248	3109.079187	21.673037
77.631403	3110.136433	21.678055
77.826654	3126.087929	21.683072
77.955711	3136.793080	21.688090
77.998257	3119.467586	21.693107
78.068616	3104.958853	21.698125
78.100132	3118.375281	21.703143
78.274098	3133.097170	21.708160
78.128648	3121.616470	21.713178
78.360327	3106.288844	21.718195
78.440643	3100.607407	21.723213
78.234383	3133.753662	21.728231
78.351186	3127.633163	21.733248
78.543949	3133.325976	21.738266
78.680470	3139.418199	21.743283
78.850301	3152.117586	21.748301
78.897123	3139.153291	21.753319
79.042936	3133.081731	21.758336
79.169350	3145.240709	21.763354
79.035057	3150.653946	21.768371
79.442788	3129.406510	21.773389
79.151163	3138.521910	21.778407
79.573700	3138.525016	21.783424
79.240078	3132.196691	21.788442
79.162764	3151.078761	21.793459
79.773288	3175.863282	21.798477
79.229659	3178.753894	21.803495
79.896569	3166.572254	21.808512
79.873979	3163.759657	21.813530
79.759522	3185.988294	21.818547
80.117842	3186.679104	21.823565
79.984031	3166.488912	21.828583
80.137096	3150.704794	21.833600
80.036527	3196.850420	21.838618
80.246906	3194.987209	21.843635
80.761246	3191.094454	21.848653
80.268065	3210.333079	21.853671
80.597942	3190.029035	21.858688
80.907467	3197.055978	21.863706
80.641850	3198.965911	21.868723
80.811538	3184.781599	21.873741
80.745659	3199.729778	21.878759
80.697903	3196.464492	21.883776
80.945831	3207.540167	21.888794
81.283866	3225.257748	21.893811
81.573367	3202.680084	21.898829
81.048306	3228.765406	21.903847
81.547224	3239.315429	21.908864
81.250273	3228.755456	21.913882
81.343052	3217.266812	21.918899
81.446802	3220.084708	21.923917
81.296920	3244.012216	21.928935
81.634921	3253.812147	21.933952
81.590122	3249.892884	21.938970
81.829588	3253.064896	21.943987
82.295247	3239.716576	21.949005
82.291835	3262.372402	21.954023
82.144041	3253.480901	21.959040
81.943658	3248.698855	21.964058
82.330823	3258.623329	21.969075
82.565384	3278.795616	21.974093
82.516890	3279.198767	21.979111
82.850911	3272.074502	21.984128
82.587072	3291.055274	21.989146
82.628560	3288.727095	21.994163
83.456685	3277.824504	21.999181
83.178358	3274.433932	22.004199
83.238357	3278.496541	22.009216
83.290123	3281.958407	22.014234
82.989824	3259.246843	22.019251
83.310035	3262.843659	22.024269
83.120007	3286.055106	22.029287
83.418816	3277.120106	22.034304
83.594515	3265.630125	22.039322
83.281905	3270.817186	22.044339
83.598532	3272.192184	22.049357
83.476198	3274.785859	22.054375
83.876235	3277.328452	22.059392
83.812245	3300.573812	22.064410
83.810269	3289.803064	22.069427
83.904761	3284.011945	22.074445
83.867848	3294.289953	22.079463
83.684331	3310.505388	22.084480
83.960608	3306.695048	22.089498
84.076391	3307.865662	22.094515
84.377460	3315.916003	22.099533
84.137543	3318.736575	22.104551
84.454050	3314.876283	22.109568
84.250506	3318.387626	22.114586
84.442416	3337.181347	22.119603
84.808225	3343.758351	22.124621
84.757756	3362.777766	22.129639
84.805553	3363.007739	22.134656
85.023101	3357.943038	22.139674
85.094083	3356.206770	22.144691
85.910790	3368.044793	22.149709
85.807745	3389.238865	22.154727
85.701571	3369.895335	22.159744
86.124922	3357.849451	22.164762
85.730378	3373.335328	22.169779
85.717615	3378.271520	22.174797
85.578217	3374.510954	22.179815
85.967427	3361.898322	22.184832
86.027510	3362.964768	22.189850
86.008966	3371.876142	22.194867
86.424618	3358.423198	22.199885
86.251583	3363.536445	22.204903
86.455113	3368.234156	22.209920
86.527340	3374.178844	22.214938
86.563613	3382.940825	22.219955
86.571197	3380.006875	22.224973
86.523366	3405.550885	22.229991
86.446861	3406.622189	22.235008
86.746113	3401.489254	22.240026
86.641668	3388.452904	22.245043
86.905574	3402.118357	22.250061
87.143148	3431.127720	22.255079
86.895503	3435.128617	22.260096
87.472827	3420.977116	22.265114
87.415239	3422.721218	22.270131
87.444781	3413.620810	22.275149
87.622959	3414.324076	22.280167
87.752054	3406.170914	22.285184
87.985277	3412.757260	22.290202
87.316058	3438.168196	22.295219
87.924615	3451.630300	22.300237
87.931320	3442.693870	22.305255
88.038056	3447.373155	22.310272
88.244006	3454.785802	22.315290
88.114283	3465.379625	22.320307
88.290544	3449.855913	22.325325
88.143200	3466.102736	22.330343
88.323337	3471.811342	22.335360
88.678299	3475.385146	22.340378
88.328725	3477.891611	22.345395
88.429055	3484.622377	22.350413
88.774809	3495.771260	22.355431
88.573927	3487.907599	22.360448
88.891175	3477.196758	22.365466
88.956790	3498.900465	22.370483
89.440862	3516.037014	22.375501
89.602969	3526.106518	22.380519
89.212551	3514.921492	22.385536
89.295947	3501.393417	22.390554
89.402086	3508.889309	22.395571
89.612335	3504.370405	22.400589
89.589337	3514.291565	22.405607
89.712483	3496.658063	22.410624
89.895727	3514.561580	22.415642
89.934116	3534.788270	22.420659
89.717581	3539.158628	22.425677
89.957134	3540.304280	22.430695
89.944111	3526.182324	22.435712
90.461553	3537.406796	22.440730
90.207771	3565.686451	22.445747
90.554658	3577.674115	22.450765
90.319207	3566.061706	22.455783
90.626439	3574.996329	22.460800
90.911954	3566.134221	22.465818
90.737612	3570.988127	22.470835
90.871975	3573.031800	22.475853
90.888475	3588.476543	22.480871
91.001609	3600.683741	22.485888
91.130466	3588.110009	22.490906
91.175543	3584.172267	22.495923
91.514544	3597.588890	22.500941
91.676644	3597.149048	22.505959
91.311106	3591.946780	22.510976
91.687573	3610.460358	22.515994
91.507853	3628.244272	22.521011
91.846251	3635.879983	22.526029
92.176527	3623.934306	22.531047
92.315247	3619.059304	22.536064
92.462372	3621.538832	22.541082
92.447947	3619.426126	22.546099
92.347124	3628.958283	22.551117
92.517387	3616.788874	22.556135
92.402888	3633.329831	22.561152
92.870782	3638.004216	22.566170
92.750640	3648.426123	22.571187
93.187733	3639.500740	22.576205
93.554343	3641.068482	22.581223
93.397736	3628.294859	22.586240
93.676898	3641.501543	22.591258
93.072312	3645.163867	22.596275
93.067401	3651.275726	22.601293
93.322632	3630.906477	22.606311
93.360150	3636.829050	22.611328
93.490556	3630.839363	22.616346
93.424521	3623.376743	22.621363
93.541775	3654.535572	22.626381
93.508351	3664.626846	22.631399
93.693354	3663.927134	22.636416
94.245933	3658.283197	22.641434
94.150170	3661.103631	22.646451
94.201808	3649.140595	22.651469
94.510384	3660.194175	22.656487
94.110724	3692.012859	22.661504
94.799756	3692.959852	22.666522
94.493854	3699.431482	22.671539
94.464535	3701.391007	22.676557
94.685030	3695.068124	22.681575
94.490157	3708.065026	22.686592
94.681506	3710.507540	22.691610
94.659638	3715.526637	22.696627
94.976136	3708.838895	22.701645
95.403524	3714.627594	22.706663
95.703175	3736.018376	22.711680
95.747538	3713.712742	22.716698
95.953365	3704.107281	22.721715
95.935650	3708.892439	22.726733
96.038545	3710.468530	22.731751
95.835451	3703.073004	22.736768
96.154867	3713.651834	22.741786
96.198236	3718.681804	22.746803
95.685948	3696.965381	22.751821
96.159948	3689.213116	22.756839
95.984699	3715.842788	22.761856
96.421671	3719.549741	22.766874
96.792239	3724.059146	22.771891
96.412301	3736.193211	22.776909
96.740238	3726.529374	22.781927
96.516369	3744.868315	22.786944
96.665515	3748.438202	22.791962
96.810862	3738.310468	22.796979
96.440327	3739.067610	22.801997
96.929811	3739.109850	22.807015
96.726294	3776.677583	22.812032
97.008229	3780.271792	22.817050
97.175086	3781.879248	22.822067
97.197347	3777.436207	22.827085
97.328200	3782.254512	22.832103
96.957181	3806.703453	22.837120
97.471792	3823.206797	22.842138
97.853745	3817.165237	22.847155
97.637717	3818.521417	22.852173
97.970190	3839.936248	22.857191
98.140038	3857.742187	22.862208
98.642250	3859.235186	22.867226
98.491182	3864.528814	22.872243
98.830179	3857.246580	22.877261
98.866240	3843.055794	22.882279
98.674684	3847.829368	22.887296
98.862972	3845.351660	22.892314
98.842348	3849.759610	22.897331
99.130681	3858.971323	22.902349
99.189469	3851.801530	22.907367
99.099700	3849.043803	22.912384
99.242472	3867.695906	22.917402
99.181189	3885.555814	22.922419
99.045400	3875.671873	22.927437
99.598062	3879.813855	22.932455
99.280004	3895.443509	22.937472
99.460816	3903.017996	22.942490
99.801700	3895.430333	22.947507
100.025955	3895.859490	22.952525
100.503013	3916.019312	22.957543
100.453479	3924.368836	22.962560
100.766261	3906.108489	22.967578
100.850260	3884.976696	22.972595
100.485320	3888.405000	22.977613
100.463316	3890.120835	22.982631
100.883613	3894.556723	22.987648
101.110144	3901.105606	22.992666
101.191752	3914.531181	22.997683
100.927388	3930.439382	23.002701
101.081687	3916.638417	23.007719
101.206275	3914.690878	23.012736
101.217950	3921.823271	23.017754
101.123596	3936.533378	23.022771
101.273240	3932.658186	23.027789
101.429920	3914.612982	23.032807
101.362256	3950.113534	23.037824
101.372019	3959.504399	23.042842
101.721579	3953.446684	23.047859
101.683316	3958.749655	23.052877
101.831350	3955.400284	23.057895
101.871755	3976.085460	23.062912
101.786436	3986.354997	23.067930
102.151901	3994.149791	23.072947
102.109012	3984.139413	23.077965
102.193510	3990.634642	23.082983
102.220780	4020.697524	23.088000
102.599323	4011.866639	23.093018
102.810250	4013.043238	23.098035
102.831689	4033.763906	23.103053
103.467156	4031.413449	23.108071
103.417809	4048.089744	23.113088
103.621533	4041.045908	23.118106
103.722260	4042.407245	23.123123
103.657216	4054.164346	23.128141
104.287065	4028.122722	23.133159
103.967048	4043.835915	23.138176
103.846522	4040.158874	23.143194
103.927941	4027.085171	23.148211
103.848272	4032.938682	23.153229
104.187427	4015.228151	23.158247
103.971047	4025.076480	23.163264
104.364034	4051.451229	23.168282
104.607749	4052.700362	23.173299
104.379448	4066.898894	23.178317
104.956907	4052.631843	23.183335
104.708007	4046.375750	23.188352
104.486247	4046.835698	23.193370
104.744434	4069.209728	23.198387
104.887497	4084.557877	23.203405
105.354819	4083.136728	23.208423
105.021658	4104.730611	23.213440
105.235893	4084.635638	23.218458
105.273252	4084.742550	23.223475
105.067018	4111.426641	23.228493
105.603923	4122.890638	23.233511
105.618842	4124.152780	23.238528
105.497712	4112.778145	23.243546
105.345988	4125.754291	23.248563
105.839882	4147.855246	23.253581
105.968084	4145.220891	23.258599
106.256295	4146.344575	23.263616
106.557980	4163.090150	23.268634
106.516993	4170.606147	23.273651
106.698056	4169.838563	23.278669
107.207012	4157.644459	23.283687
106.943776	4164.813728	23.288704
106.801182	4167.462078	23.293722
107.335440	4162.535524	23.298739
107.117701	4160.087457	23.303757
107.466004	4158.821789	23.308775
107.740890	4194.809189	23.313792
107.771674	4196.908051	23.318810
107.852366	4193.547711	23.323827
107.917292	4207.379822	23.328845
108.080859	4198.044218	23.333863
107.904085	4183.274534	23.338880
107.882988	4190.631749	23.343898
108.091228	4191.104110	23.348915
108.094134	4201.000171	23.353933
108.348221	4200.892540	23.358951
108.549674	4196.343002	23.363968
108.618874	4215.178933	23.368986
108.461883	4225.926594	23.374003
108.620750	4224.987880	23.379021
108.829409	4209.519470	23.384039
109.018494	4201.385110	23.389056
108.835654	4229.611539	23.394074
108.744745	4230.485286	23.399091
108.707261	4233.968609	23.404109
108.825889	4228.940246	23.409127
109.206631	4265.914218	23.414144
109.090370	4286.065872	23.419162
109.298780	4277.992057	23.424179
109.344797	4274.550030	23.429197
109.766181	4294.594747	23.434215
110.096538	4299.480245	23.439232
109.918647	4321.163336	23.444250
110.005655	4305.683830	23.449267
110.318509	4320.825423	23.454285
110.551607	4317.763484	23.459303
110.892859	4322.090515	23.464320
110.842931	4340.600231	23.469338
111.074821	4314.812856	23.474355
111.155112	4328.966148	23.479373
111.266439	4337.554659	23.484391
111.303264	4327.950165	23.489408
111.084779	4315.461583	23.494426
111.486208	4321.736479	23.499443
111.224394	4357.356260	23.504461
111.663266	4370.365334	23.509479
111.561932	4372.682502	23.514496
111.778483	4345.899608	23.519514
112.086662	4359.838507	23.524531
111.833953	4388.677537	23.529549
112.176425	4383.506235	23.534567
112.316510	4389.982212	23.539584
112.258130	4405.033264	23.544602
112.658728	4371.750017	23.549619
112.525433	4387.409476	23.554637
112.788963	4408.725665	23.559655
113.037642	4407.254791	23.564672
112.840584	4419.385153	23.569690
113.037974	4419.084926	23.574707
113.049952	4411.408057	23.579725
113.023556	4416.905281	23.584743
113.223989	4428.897926	23.589760
113.122662	4443.321483	23.594778
113.537992	4444.808034	23.599795
113.638796	4433.304761	23.604813
114.013446	4447.314250	23.609831
114.274229	4467.691233	23.614848
114.495278	4475.878236	23.619866
114.847162	4469.848284	23.624883
114.702184	4478.013487	23.629901
114.767247	4466.127916	23.634919
114.838126	4459.781416	23.639936
114.670278	4459.542719	23.644954
115.192683	4474.526220	23.649971
115.105053	4476.487209	23.654989
114.845065	4467.235209	23.660007
115.117512	4448.574207	23.665024
115.226382	4471.413638	23.670042
115.408343	4480.782272	23.675059
115.485692	4474.838624	23.680077
115.178838	4493.859075	23.685095
115.681151	4500.379574	23.690112
115.467333	4490.697105	23.695130
115.534688	4504.042870	23.700147
115.789952	4512.375023	23.705165
115.727666	4527.601246	23.710183
115.990836	4556.167161	23.715200
116.163805	4552.689529	23.720218
116.459155	4531.224301	23.725235
116.256336	4545.378115	23.730253
116.428882	4561.359254	23.735271
116.906226	4571.272432	23.740288
116.771948	4577.892245	23.745306
116.832380	4558.992525	23.750323
117.215023	4566.643830	23.755341
117.185955	4581.291398	23.760359
117.447382	4584.435649	23.765376
117.266468	4601.758285	23.770394
117.503553	4611.805280	23.775411
117.750238	4603.480882	23.780429
117.762998	4599.402555	23.785447
118.184314	4594.069340	23.790464
118.048205	4614.624693	23.795482
118.371781	4623.112151	23.800499
118.267544	4633.011625	23.805517
118.300439	4627.767775	23.810535
118.710661	4613.730205	23.815552
118.455341	4626.419166	23.820570
118.600446	4658.785831	23.825587
118.953369	4650.239131	23.830605
118.741395	4657.528894	23.835623
119.280596	4660.161915	23.840640
119.181217	4676.570777	23.845658
119.232294	4678.225411	23.850675
119.344484	4679.294757	23.855693
119.534185	4680.450900	23.860711
119.677829	4687.602784	23.865728
119.835746	4703.269561	23.870746
119.523636	4707.597966	23.875763
119.825199	4707.982485	23.880781
119.868970	4725.170495	23.885799
120.268873	4742.879202	23.890816
120.480145	4743.726276	23.895834
120.638764	4742.063955	23.900851
120.803262	4740.743574	23.905869
120.682093	4758.275013	23.910887
121.418422	4770.809293	23.915904
121.726992	4768.235582	23.920922
121.483446	4758.772817	23.925939
121.696753	4778.225774	23.930957
121.547071	4791.116705	23.935975
122.139117	4771.422196	23.940992
121.986893	4780.669065	23.946010
121.966996	4782.059455	23.951027
122.192974	4753.768400	23.956045
121.922939	4763.550471	23.961063
122.291442	4777.972691	23.966080
122.081311	4780.231518	23.971098
121.964192	4807.412312	23.976115
122.389989	4798.653490	23.981133
122.024244	4820.771072	23.986151
122.413145	4828.526984	23.991168
122.667762	4819.996435	23.996186
122.811403	4825.722795	24.001203
123.001687	4844.339089	24.006221
122.907629	4858.426396	24.011239
123.370759	4872.203540	24.016256
123.146735	4869.995768	24.021274
123.680641	4868.073391	24.026291
123.997383	4888.527509	24.031309
123.888628	4913.877573	24.036327
124.170885	4881.651378	24.041344
124.087694	4877.676235	24.046362
124.179607	4893.207653	24.051379
124.530554	4916.377031	24.056397
124.588455	4918.537259	24.061415
125.030545	4903.600852	24.066432
125.005554	4908.084234	24.071450
124.816831	4930.846347	24.076467
124.934733	4907.479989	24.081485
124.872377	4909.731346	24.086503
125.386472	4919.654030	24.091520
125.280928	4920.205036	24.096538
125.409312	4916.039805	24.101555
125.545463	4933.596641	24.106573
125.838922	4944.840845	24.111591
125.935092	4947.545939	24.116608
125.828461	4932.040324	24.121626
126.088678	4959.046830	24.126643
126.288810	4965.619426	24.131661
126.235519	4963.065316	24.136679
126.175003	4979.592093	24.141696
126.472431	4984.665143	24.146714
126.698746	4999.249253	24.151731
126.671271	4982.298604	24.156749
126.667930	5005.807368	24.161767
126.707569	5015.704178	24.166784
127.094124	5029.742936	24.171802
126.845657	5030.913238	24.176819
127.429591	5030.553856	24.181837
127.262307	5059.263083	24.186855
127.426775	5056.402895	24.191872
127.881090	5055.648388	24.196890
128.065856	5056.800258	24.201907
128.244473	5074.925836	24.206925
128.248311	5086.281384	24.211943
128.479243	5091.641838	24.216960
128.651541	5095.898185	24.221978
128.605878	5098.690521	24.226995
128.719572	5089.516957	24.232013
128.838140	5103.897706	24.237031
129.120229	5112.283625	24.242048
129.391000	5128.569991	24.247066
129.414109	5126.514657	24.252083
129.628372	5112.958634	24.257101
129.735028	5108.071338	24.262119
129.919010	5130.668221	24.267136
129.658676	5141.840290	24.272154
129.649384	5147.094784	24.277171
129.741629	5132.465576	24.282189
130.017739	5157.090621	24.287207
130.474880	5166.097659	24.292224
130.677049	5163.054053	24.297242
130.655099	5188.444553	24.302259
130.846749	5175.821760	24.307277
130.621912	5182.645772	24.312295
130.827265	5182.910766	24.317312
130.941029	5198.192809	24.322330
131.002739	5215.317765	24.327347
130.942175	5212.778203	24.332365
131.126728	5205.326763	24.337383
131.337256	5227.256786	24.342400
131.649541	5243.482868	24.347418
131.522695	5268.168764	24.352435
131.742788	5269.546708	24.357453
131.913319	5285.415931	24.362471
132.187971	5282.113074	24.367488
132.359268	5274.018105	24.372506
132.646115	5303.751988	24.377523
133.184850	5291.369399	24.382541
132.775448	5294.117538	24.387559
132.797225	5292.169099	24.392576
133.181890	5307.657283	24.397594
133.394330	5310.107395	24.402611
133.471236	5301.976825	24.407629
133.507928	5318.734363	24.412647
133.426401	5306.490077	24.417664
133.969966	5322.516211	24.422682
133.736557	5335.782855	24.427699
134.114775	5330.423047	24.432717
134.003736	5345.827815	24.437735
134.128932	5342.516963	24.442752
134.246317	5339.877502	24.447770
134.297898	5366.610517	24.452787
134.351252	5371.039747	24.457805
134.042320	5375.456396	24.462823
134.314448	5388.742313	24.467840
135.248838	5385.950920	24.472858
135.013617	5399.567141	24.477875
135.264231	5403.030288	24.482893
135.211535	5421.898454	24.487911
135.418240	5425.864549	24.492928
135.626876	5434.721459	24.497946
135.728109	5434.706799	24.502963
136.159486	5443.063900	24.507981
136.043913	5451.622406	24.512999
136.187586	5457.795468	24.518016
136.774989	5454.303886	24.523034
136.357846	5483.120928	24.528051
136.417942	5475.424165	24.533069
136.440235	5503.312695	24.538087
136.956134	5491.260902	24.543104
137.311066	5493.123695	24.548122
137.276872	5511.867647	24.553139
137.327373	5520.143227	24.558157
137.652647	5525.000427	24.563175
137.362560	5521.905799	24.568192
138.126947	5515.802957	24.573210
137.929184	5546.341818	24.578227
138.230196	5556.541863	24.583245
138.236345	5556.103524	24.588263
138.456526	5530.887358	24.593280
138.684352	5536.190997	24.598298
138.470131	5575.556262	24.603315
138.831893	5580.632264	24.608333
139.125394	5578.292813	24.613351
138.947304	5568.336825	24.618368
139.240312	5562.758330	24.623386
139.018195	5596.382559	24.628403
139.319072	5594.352138	24.633421
139.499049	5595.124507	24.638439
139.820660	5605.697577	24.643456
139.979086	5610.894199	24.648474
140.243142	5635.468447	24.653491
140.428169	5613.758923	24.658509
140.459571	5624.500043	24.663527
140.471769	5644.241263	24.668544
140.687962	5624.912525	24.673562
140.541688	5642.183345	24.678579
140.678502	5665.932952	24.683597
141.195386	5654.002925	24.688615
140.863410	5666.201432	24.693632
141.486145	5699.152794	24.698650
141.278425	5693.895190	24.703667
142.187562	5683.491360	24.708685
141.766032	5703.944908	24.713703
141.574957	5708.235477	24.718720
142.001656	5713.018100	24.723738
141.887741	5722.406843	24.728755
141.929472	5714.785835	24.733773
142.135783	5729.091637	24.738791
142.262568	5760.702553	24.743808
142.532088	5747.020307	24.748826
142.374354	5738.751497	24.753843
143.034692	5746.635079	24.758861
143.114612	5785.617213	24.763879
143.211361	5792.404892	24.768896
143.476073	5778.991540	24.773914
143.078706	5794.407838	24.778931
143.659347	5784.929927	24.783949
144.012244	5800.106510	24.788967
143.718055	5821.710896	24.793984
144.018646	5817.414210	24.799002
144.102692	5813.783265	24.804019
144.238206	5827.705555	24.809037
144.239691	5851.239600	24.814055
144.226659	5841.904238	24.819072
144.793231	5841.787886	24.824090
144.861405	5884.694510	24.829107
144.842427	5893.140834	24.834125
144.958194	5874.781201	24.839143
144.970585	5882.908930	24.844160
145.248030	5892.472890	24.849178
145.416037	5939.142557	24.854195
145.489570	5948.731188	24.859213
145.647283	5940.023902	24.864231
145.854588	5942.783253	24.869248
146.124722	5956.569233	24.874266
146.086192	5976.457848	24.879283
146.095201	5979.820878	24.884301
146.661072	5982.209943	24.889319
146.909055	5986.178812	24.894336
146.962164	6004.703009	24.899354
146.444662	6030.993356	24.904371
146.974869	6020.435365	24.909389
147.403504	6019.274794	24.914407
147.420883	6045.841776	24.919424
147.826314	6043.476282	24.924442
147.697327	6056.398698	24.929459
148.133387	6063.767488	24.934477
148.446076	6067.948538	24.939495
148.562843	6071.044550	24.944512
149.029127	6058.302828	24.949530
149.090110	6079.891409	24.954547
149.306348	6086.824840	24.959565
149.374491	6080.498607	24.964583
149.289210	6078.873296	24.969600
149.597048	6063.611483	24.974618
149.786134	6077.234963	24.979635
149.581378	6077.838230	24.984653
149.514663	6084.925114	24.989671
149.590543	6098.297217	24.994688
149.729878	6101.970262	24.999706
149.995154	6108.612507	25.004723
149.928934	6127.071520	25.009741
150.176991	6143.853687	25.014759
149.773993	6165.066254	25.019776
150.638571	6152.228329	25.024794
150.676398	6167.433311	25.029811
150.912779	6192.816228	25.034829
151.066836	6216.612647	25.039847
150.821258	6203.144258	25.044864
151.513684	6198.347649	25.049882
151.813850	6227.731458	25.054899
151.851975	6251.097438	25.059917
152.139851	6237.538909	25.064935
152.083265	6236.933735	25.069952
152.090349	6253.101840	25.074970
152.335502	6263.921872	25.079987
152.404754	6255.758209	25.085005
152.752857	6265.945427	25.090023
152.603281	6276.402302	25.095040
152.744246	6289.891386	25.100058
152.743915	6302.462794	25.105075
152.992262	6294.248652	25.110093
153.148303	6298.454073	25.115111
153.037704	6330.242384	25.120128
153.350061	6338.767681	25.125146
153.667939	6352.007487	25.130163
153.490592	6353.659093	25.135181
153.939948	6358.452349	25.140199
154.090738	6388.319453	25.145216
154.606022	6390.838609	25.150234
154.733416	6396.820619	25.155251
154.520501	6408.180656	25.160269
154.786966	6410.322775	25.165287
155.246424	6410.660779	25.170304
155.374378	6417.549490	25.175322
155.544065	6425.646392	25.180339
155.918815	6448.742065	25.185357
156.074986	6468.386515	25.190375
155.843309	6466.700303	25.195392
156.417744	6453.135978	25.200410
156.233062	6436.548343	25.205427
156.063996	6461.857335	25.210445
156.718949	6464.744017	25.215463
156.749553	6475.423249	25.220480
157.212320	6459.273158	25.225498
157.184805	6451.303747	25.230515
157.196357	6488.297148	25.235533
157.217749	6491.082196	25.240551
157.479521	6486.783081	25.245568
157.859858	6503.016557	25.250586
157.670601	6514.254245	25.255603
157.741670	6530.613661	25.260621
158.021680	6532.656303	25.265639
157.968590	6542.542235	25.270656
158.436229	6537.516889	25.275674
158.582769	6565.854553	25.280691
158.657609	6576.981319	25.285709
158.918666	6560.688449	25.290727
158.972249	6573.078707	25.295744
159.170526	6586.988940	25.300762
159.397464	6588.100491	25.305779
159.285533	6604.035444	25.310797
159.795808	6604.917089	25.315815
159.828625	6613.999805	25.320832
159.907483	6621.430637	25.325850
160.392649	6620.003569	25.330867
160.014103	6647.357544	25.335885
160.493857	6668.805689	25.340903
160.621586	6657.379806	25.345920
161.075837	6650.478465	25.350938
161.692003	6663.833050	25.355955
161.296842	6685.094636	25.360973
161.822719	6682.761910	25.365991
161.760712	6669.788834	25.371008
161.839240	6660.335876	25.376026
162.035905	6661.063805	25.381043
162.055558	6695.992337	25.386061
161.981151	6697.023355	25.391079
162.080009	6711.158419	25.396096
162.110017	6714.607911	25.401114
162.455694	6704.895012	25.406131
162.367262	6723.346979	25.411149
162.659942	6738.743506	25.416167
163.031471	6769.616332	25.421184
162.843106	6772.156920	25.426202
163.410247	6749.741269	25.431219
163.132752	6770.087355	25.436237
163.519940	6778.511935	25.441255
163.499279	6792.696745	25.446272
163.694150	6814.488655	25.451290
163.968372	6825.475554	25.456307
164.354290	6826.895542	25.461325
164.482154	6815.747903	25.466343
164.590811	6841.836135	25.471360
164.826421	6865.709449	25.476378
164.919703	6853.044071	25.481395
164.851136	6869.787983	25.486413
165.233490	6872.464633	25.491431
165.553649	6880.688505	25.496448
165.564938	6888.733463	25.501466
165.859133	6885.892854	25.506483
166.070313	6914.083836	25.511501
165.894426	6927.222225	25.516519
166.062621	6922.760476	25.521536
166.308235	6925.258521	25.526554
166.879547	6938.172268	25.531571
166.755285	6950.133091	25.536589
166.767232	6954.630644	25.541607
167.122716	6971.546365	25.546624
167.026209	6984.841789	25.551642
167.433837	6996.447406	25.556659
167.213527	7006.706188	25.561677
167.852920	7014.093811	25.566695
167.781287	7024.315439	25.571712
167.909407	7027.140437	25.576730
167.945628	7039.840275	25.581747
168.507766	7072.725407	25.586765
168.665335	7085.483589	25.591783
168.838460	7069.889071	25.596800
168.557151	7076.220406	25.601818
168.791885	7104.460602	25.606835
168.942453	7120.489736	25.611853
169.156907	7114.694899	25.616871
169.998991	7134.016587	25.621888
169.972220	7147.567200	25.626906
170.188203	7157.642560	25.631923
170.235140	7161.125973	25.636941
170.176411	7171.255394	25.641959
170.887685	7171.043470	25.646976
170.717513	7168.018474	25.651994
171.078647	7184.362146	25.657011
170.670620	7207.696953	25.662029
171.287443	7199.534074	25.667047
171.113943	7200.592916	25.672064
171.288668	7227.879324	25.677082
171.767924	7245.666760	25.682100
171.792847	7268.467847	25.687117
171.680423	7264.082686	25.692135
172.103954	7261.979420	25.697152
172.393679	7289.058716	25.702170
172.529747	7304.253688	25.707188
172.613034	7312.001882	25.712205
172.963808	7302.734694	25.717223
173.294512	7314.307188	25.722240
173.182834	7330.166052	25.727258
173.549951	7329.795995	25.732276
173.763172	7342.947225	25.737293
173.508542	7335.164520	25.742311
174.133069	7348.205269	25.747328
174.292561	7381.508027	25.752346
174.870591	7384.605266	25.757364
174.688680	7383.727399	25.762381
174.433135	7372.543486	25.767399
175.133002	7379.113287	25.772416
174.929282	7395.804881	25.777434
175.183582	7387.394666	25.782452
175.177752	7403.512538	25.787469
175.353595	7418.425413	25.792487
175.863467	7423.023144	25.797504
175.697981	7430.276979	25.802522
176.377559	7424.048033	25.807540
176.081785	7445.576948	25.812557
176.292276	7443.727005	25.817575
176.460674	7445.991788	25.822592
176.633791	7465.834328	25.827610
176.718372	7464.766732	25.832628
176.921002	7469.085264	25.837645
176.945882	7485.732095	25.842663
176.954675	7512.395909	25.847680
177.116031	7542.561944	25.852698
177.751110	7520.811650	25.857716
177.726021	7530.217510	25.862733
178.073147	7555.845014	25.867751
178.144344	7573.302537	25.872768
178.096566	7592.041377	25.877786
178.323360	7596.918255	25.882804
178.355544	7613.825478	25.887821
178.724034	7609.000069	25.892839
179.011645	7631.006965	25.897856
179.153224	7663.543063	25.902874
179.393327	7661.337745	25.907892
179.817998	7685.931992	25.912909
179.801361	7696.569851	25.917927
180.280188	7683.301029	25.922944
180.363641	7687.295155	25.927962
180.783041	7701.055256	25.932980
180.635965	7737.997480	25.937997
180.788718	7720.105258	25.943015
181.027206	7727.689407	25.948032
181.112114	7755.642873	25.953050
181.714329	7738.723020	25.958068
181.997270	7756.485982	25.963085
182.014133	7793.577661	25.968103
182.249175	7786.604545	25.973120
182.134212	7786.693730	25.978138
182.286264	7791.241222	25.983156
182.507025	7788.039682	25.988173
182.638498	7799.839977	25.993191
183.012669	7818.646404	25.998208
183.025652	7837.367621	26.003226
183.404834	7835.023530	26.008244
183.366442	7837.624170	26.013261
183.282268	7849.928726	26.018279
184.121538	7851.929152	26.023296
184.076606	7864.917133	26.028314
184.056365	7887.235933	26.033332
184.410106	7882.602679	26.038349
184.621101	7911.591700	26.043367
184.960984	7912.322411	26.048384
184.597181	7901.783689	26.053402
184.735741	7911.941631	26.058420
185.036965	7937.107958	26.063437
185.326193	7972.154660	26.068455
185.204337	7967.051820	26.073472
185.602510	7977.258266	26.078490
185.689556	7986.181999	26.083508
185.909250	7995.133436	26.088525
186.302202	8018.039402	26.093543
186.295865	8032.215087	26.098560
186.299120	8050.680632	26.103578
186.453940	8049.127278	26.108596
187.026864	8041.997416	26.113613
187.024151	8056.583633	26.118631
187.818534	8076.211674	26.123648
187.386572	8099.856541	26.128666
187.797692	8087.423149	26.133684
187.713544	8087.719887	26.138701
187.845044	8120.065641	26.143719
188.246985	8117.872900	26.148736
188.299061	8147.239867	26.153754
188.547090	8149.159242	26.158772
188.874311	8162.545920	26.163789
189.021103	8172.362440	26.168807
189.219104	8187.385794	26.173824
189.424752	8190.984188	26.178842
189.623959	8203.224872	26.183860
189.891439	8226.248744	26.188877
189.564427	8213.073244	26.193895
190.518871	8226.792659	26.198912
190.573699	8251.511904	26.203930
190.570212	8255.466985	26.208948
191.099592	8256.103398	26.213965
191.178619	8279.895653	26.218983
191.503348	8294.832802	26.224000
191.453262	8270.001068	26.229018
191.301534	8286.699189	26.234036
191.618657	8305.662114	26.239053
191.450194	8318.522026	26.244071
191.880019	8332.324276	26.249088
191.992702	8366.384262	26.254106
192.097804	8376.034530	26.259124
192.347870	8379.821736	26.264141
192.415081	8420.081303	26.269159
192.678929	8416.388155	26.274176
193.265763	8429.695938	26.279194
193.088912	8461.482962	26.284212
193.624486	8463.915628	26.289229
193.301367	8476.099483	26.294247
193.907682	8489.248944	26.299264
194.036582	8516.449072	26.304282
194.519168	8517.966663	26.309300
194.904959	8528.940261	26.314317
194.890913	8556.868967	26.319335
195.122349	8545.815620	26.324352
195.731159	8540.038197	26.329370
196.037329	8556.945268	26.334388
196.268160	8556.541000	26.339405
196.365858	8553.962144	26.344423
196.407815	8569.469233	26.349440
196.182581	8577.877831	26.354458
196.331905	8578.443163	26.359476
196.490589	8590.512848	26.364493
196.727082	8637.530879	26.369511
197.152242	8641.670414	26.374528
197.089196	8646.203287	26.379546
197.450840	8647.027314	26.384564
197.654064	8660.056858	26.389581
197.425140	8677.244639	26.394599
197.516297	8700.212488	26.399616
197.819303	8713.782420	26.404634
197.983147	8724.736907	26.409652
198.508395	8738.370953	26.414669
198.758303	8744.646295	26.419687
199.008773	8754.220008	26.424704
199.604621	8769.379021	26.429722
199.663820	8779.983815	26.434740
200.111459	8773.209846	26.439757
199.829715	8788.099597	26.444775
199.881616	8772.906987	26.449792
200.216209	8794.304446	26.454810
200.764951	8799.955489	26.459828
201.290805	8818.110333	26.464845
200.757811	8826.780201	26.469863
200.876318	8816.926725	26.474880
201.295672	8830.679162	26.479898
201.143803	8840.238278	26.484916
201.446901	8847.935160	26.489933
201.608779	8873.042519	26.494951
201.699118	8885.925503	26.499968
201.976662	8888.626124	26.504986
201.778440	8901.407152	26.510004
202.327817	8919.504670	26.515021
202.462115	8948.588605	26.520039
202.500851	8954.142817	26.525056
202.854197	8964.525074	26.530074
203.110807	8990.013134	26.535092
203.167423	8997.193972	26.540109
203.279220	9016.016826	26.545127
203.699287	9034.442221	26.550144
204.041402	9060.091117	26.555162
204.195959	9078.903831	26.560180
204.677311	9073.081117	26.565197
204.477940	9090.311720	26.570215
204.801639	9101.426722	26.575232
204.994393	9131.450412	26.580250
205.297458	9135.698465	26.585268
205.590613	9142.835563	26.590285
206.065955	9160.325734	26.595303
205.909157	9155.010898	26.600320
206.000229	9176.997293	26.605338
206.068983	9218.760629	26.610356
206.569010	9205.871394	26.615373
206.800450	9220.522388	26.620391
207.137737	9239.456326	26.625408
207.456755	9260.224529	26.630426
207.714210	9253.649543	26.635444
207.944756	9262.796814	26.640461
208.015396	9290.374933	26.645479
208.144219	9298.564740	26.650496
208.527072	9287.712695	26.655514
208.623157	9320.934721	26.660532
208.818213	9316.365865	26.665549
208.898377	9337.812398	26.670567
209.135633	9356.579486	26.675584
209.330442	9344.887354	26.680602
209.443914	9370.752534	26.685620
210.058584	9387.129859	26.690637
209.882246	9398.171735	26.695655
210.209198	9418.734052	26.700672
210.500886	9411.194798	26.705690
210.656295	9427.450348	26.710708
210.941556	9436.829696	26.715725
210.659619	9466.503977	26.720743
211.062391	9473.985426	26.725760
211.251819	9474.119631	26.730778
211.448831	9485.419662	26.735796
211.790182	9509.220047	26.740813
211.668646	9538.703346	26.745831
212.384421	9547.896636	26.750848
212.564624	9551.479069	26.755866
212.560825	9561.011792	26.760884
212.611606	9585.814130	26.765901
212.942970	9618.049588	26.770919
213.477153	9626.675894	26.775936
213.936955	9607.275248	26.780954
213.987767	9634.743821	26.785972
214.210557	9659.804557	26.790989
214.412243	9657.008281	26.796007
214.720095	9660.411332	26.801024
215.434884	9670.162509	26.806042
215.228716	9685.225709	26.811060
215.185545	9680.856788	26.816077
215.345182	9693.743945	26.821095
215.572730	9684.315361	26.826112
215.488941	9691.385024	26.831130
215.844367	9712.383311	26.836148
216.335681	9737.949583	26.841165
216.366343	9741.859222	26.846183
216.276689	9735.317758	26.851200
216.589296	9755.296085	26.856218
216.630345	9786.072293	26.861236
216.900874	9797.684125	26.866253
217.046132	9806.034523	26.871271
217.117574	9831.926303	26.876288
217.461002	9857.704662	26.881306
217.699304	9884.001380	26.886324
217.760132	9885.606908	26.891341
218.083078	9911.465929	26.896359
218.244853	9946.169443	26.901376
219.103756	9950.287288	26.906394
218.942017	9960.894718	26.911412
219.410817	9959.476768	26.916429
220.099041	9967.702887	26.921447
220.040358	9981.727496	26.926464
220.036983	9993.809274	26.931482
220.457659	10001.484144	26.936500
220.769390	10026.632373	26.941517
220.811565	10051.554221	26.946535
220.945782	10049.990689	26.951552
221.135116	10043.262800	26.956570
221.147334	10066.982923	26.961588
221.448704	10101.448681	26.966605
221.584794	10117.790836	26.971623
221.530011	10107.397284	26.976640
221.855624	10129.225736	26.981658
222.065095	10163.315341	26.986676
222.210306	10178.923520	26.991693
222.667810	10195.431623	26.996711
223.004670	10215.542002	27.001728
223.219694	10231.167054	27.006746
223.166222	10268.889749	27.011764
223.646238	10291.184421	27.016781
223.918107	10295.359963	27.021799
224.175240	10297.130019	27.026816
224.636701	10315.470513	27.031834
224.942879	10331.650881	27.036852
225.083985	10333.217985	27.041869
226.189350	10335.919144	27.046887
226.426877	10339.794753	27.051904
226.580473	10346.693157	27.056922
226.923202	10359.201665	27.061940
227.058100	10355.018174	27.066957
227.331117	10360.972121	27.071975
227.151685	10363.271165	27.076992
227.524589	10337.081603	27.082010
227.643775	10336.917865	27.087028
227.523168	10345.989087	27.092045
227.751524	10377.486150	27.097063
227.668250	10393.662398	27.102080
228.342908	10364.888970	27.107098
228.065679	10387.546766	27.112116
227.972864	10415.306654	27.117133
228.600610	10436.551564	27.122151
228.694489	10444.253860	27.127168
228.659365	10462.473347	27.132186
228.496087	10475.079725	27.137204
229.020104	10475.091708	27.142221
229.190763	10503.534463	27.147239
229.243181	10530.655374	27.152256
229.450613	10548.860091	27.157274
229.485504	10569.663563	27.162292
229.891601	10579.199279	27.167309
230.309116	10614.042380	27.172327
230.485045	10650.779698	27.177344
230.631178	10660.693971	27.182362
230.695061	10665.337205	27.187380
231.420298	10690.800987	27.192397
231.574108	10731.213589	27.197415
231.832164	10750.751620	27.202432
232.211222	10758.178519	27.207450
232.149558	10772.885676	27.212468
232.106990	10806.211696	27.217485
232.981766	10820.219093	27.222503
233.335644	10840.429065	27.227520
233.772375	10864.044005	27.232538
233.789771	10880.239560	27.237556
234.061546	10892.242690	27.242573
234.653280	10876.809217	27.247591
234.843453	10923.249321	27.252608
235.255036	10929.122298	27.257626
235.395276	10924.992916	27.262644
235.205085	10927.462387	27.267661
235.792481	10946.534276	27.272679
235.697081	10948.682459	27.277696
236.172036	10981.255367	27.282714
236.287383	10996.013830	27.287732
236.399546	11001.074548	27.292749
236.718937	11014.185300	27.297767
236.823690	11016.431184	27.302784
237.190339	11045.390772	27.307802
236.991266	11077.752275	27.312820
237.307682	11086.116029	27.317837
237.607223	11100.582637	27.322855
237.751827	11119.686141	27.327872
238.402551	11141.919933	27.332890
238.603599	11153.697842	27.337908
238.335474	11183.761381	27.342925
239.035418	11200.203693	27.347943
238.972409	11216.625558	27.352960
239.729075	11223.409740	27.357978
239.758480	11256.040279	27.362996
239.742077	11254.669300	27.368013
240.227427	11274.063290	27.373031
240.057666	11320.096107	27.378048
240.360637	11324.743357	27.383066
240.862603	11325.030755	27.388084
240.811258	11351.386417	27.393101
241.340953	11389.613297	27.398119
241.368917	11406.236164	27.403136
241.764628	11418.467349	27.408154
242.255235	11412.033350	27.413172
242.218717	11443.850410	27.418189
242.960263	11456.490825	27.423207
243.036095	11490.594320	27.428224
243.795764	11484.877578	27.433242
243.955251	11486.226709	27.438260
243.914564	11517.977649	27.443277
244.320801	11512.515434	27.448295
244.277631	11520.898652	27.453312
244.335757	11537.144861	27.458330
244.864009	11547.253356	27.463348
244.785532	11556.148940	27.468365
245.085205	11560.859824	27.473383
245.104107	11580.681795	27.478400
245.607991	11600.905761	27.483418
245.730945	11611.649218	27.488436
245.815327	11628.491439	27.493453
246.290234	11653.204079	27.498471
246.212502	11660.171206	27.503488
246.595439	11687.945293	27.508506
247.077921	11703.258982	27.513524
247.021787	11722.984817	27.518541
247.126752	11732.899469	27.523559
247.371057	11758.310501	27.528576
247.927074	11764.028373	27.533594
247.940974	11797.814264	27.538612
247.901693	11817.060055	27.543629
248.544139	11829.078275	27.548647
248.594410	11859.463084	27.553664
248.678012	11888.021945	27.558682
249.108927	11914.768360	27.563700
249.180471	11930.955245	27.568717
249.405627	11943.093697	27.573735
249.847714	11976.534296	27.578752
250.267204	11999.370736	27.583770
251.041182	12006.176817	27.588788
251.133980	12016.495412	27.593805
251.678563	12016.099100	27.598823
251.962028	12051.292044	27.603840
252.005016	12080.904106	27.608858
252.466616	12061.010994	27.613876
252.414339	12064.996352	27.618893
252.411082	12097.487478	27.623911
252.609000	12110.843714	27.628928
253.028294	12118.664788	27.633946
253.054153	12138.641490	27.638964
253.002630	12171.008394	27.643981
253.467652	12191.260799	27.648999
253.804643	12200.738008	27.654016
253.725858	12229.725281	27.659034
254.396723	12244.842148	27.664052
254.807286	12285.529004	27.669069
255.024394	12301.255000	27.674087
255.577906	12301.074634	27.679104
255.953490	12326.616919	27.684122
256.240308	12354.666435	27.689140
256.086044	12366.983697	27.694157
256.333570	12359.445630	27.699175
256.552093	12381.010472	27.704192
256.541156	12409.338518	27.709210
256.812900	12424.479743	27.714228
257.083354	12434.074434	27.719245
257.426495	12457.229012	27.724263
257.978335	12495.821985	27.729280
258.230211	12512.980149	27.734298
258.517980	12519.645414	27.739316
258.568874	12554.839285	27.744333
259.142619	12560.727830	27.749351
259.280442	12564.920604	27.754368
259.095126	12581.507449	27.759386
259.785679	12617.262246	27.764404
259.988061	12637.753979	27.769421
260.267205	12636.105595	27.774439
260.893882	12649.905084	27.779456
260.784916	12675.936055	27.784474
261.147984	12680.721092	27.789492
261.129506	12704.514798	27.794509
261.714842	12716.476950	27.799527
261.975739	12737.372735	27.804544
261.886076	12742.934512	27.809562
262.318838	12764.542466	27.814580
262.172349	12786.935470	27.819597
262.776298	12794.163883	27.824615
262.847432	12809.067611	27.829632
262.944100	12843.540807	27.834650
263.375207	12841.643561	27.839668
263.666765	12865.405978	27.844685
263.940505	12887.437422	27.849703
264.020376	12895.647408	27.854720
264.095807	12930.697031	27.859738
264.727895	12952.440109	27.864756
264.674199	12973.572522	27.869773
265.530307	12976.227108	27.874791
265.411962	13018.062803	27.879808
265.679412	13036.380972	27.884826
266.070970	13042.703943	27.889844
266.393283	13084.358291	27.894861
266.768073	13099.172731	27.899879
267.050800	13106.636340	27.904896
267.419185	13124.614143	27.909914
267.587072	13141.043159	27.914932
267.725629	13157.221785	27.919949
267.989901	13177.648834	27.924967
268.303442	13211.210935	27.929984
268.581215	13216.768107	27.935002
268.859076	13227.939263	27.940020
269.058312	13251.140820	27.945037
269.300801	13273.609681	27.950055
269.767473	13295.903667	27.955072
269.785655	13306.607271	27.960090
270.112527	13325.404402	27.965108
270.287360	13356.532500	27.970125
270.715593	13375.940054	27.975143
271.043267	13393.204023	27.980160
271.400112	13408.728394	27.985178
272.148031	13427.077926	27.990196
272.338287	13449.207442	27.995213
272.303407	13453.639332	28.000231
272.672245	13474.938944	28.005248
272.757109	13496.341435	28.010266
273.098145	13501.507732	28.015284
273.301597	13522.159557	28.020301
273.719751	13533.545674	28.025319
274.038438	13556.455346	28.030336
273.749589	13585.595575	28.035354
274.266117	13591.426992	28.040372
274.711956	13611.945923	28.045389
274.902949	13622.589673	28.050407
275.159832	13655.027573	28.055424
275.078306	13689.910181	28.060442
275.605804	13701.951169	28.065460
275.802311	13728.663702	28.070477
276.067577	13733.077595	28.075495
276.761924	13744.200787	28.080512
276.625294	13788.352247	28.085530
277.090013	13807.251648	28.090548
277.148557	13826.397804	28.095565
277.816028	13834.512768	28.100583
278.118544	13855.919171	28.105600
278.408774	13886.364282	28.110618
278.289872	13916.900678	28.115636
278.254350	13924.378641	28.120653
278.290031	13932.514519	28.125671
278.900375	13968.771681	28.130688
279.119835	14013.706356	28.135706
279.383928	14029.005565	28.140724
279.596748	14055.908969	28.145741
279.909364	14072.073151	28.150759
280.709273	14109.399164	28.155776
280.474021	14135.049966	28.160794
281.259189	14135.654637	28.165812
281.341586	14166.230731	28.170829
281.623313	14202.703433	28.175847
282.333482	14185.261031	28.180864
281.674630	14214.391823	28.185882
282.324939	14244.867938	28.190900
282.890936	14284.651759	28.195917
282.804684	14294.126858	28.200935
283.195239	14288.626126	28.205952
283.266683	14336.116790	28.210970
283.551330	14346.463487	28.215988
283.650047	14388.708867	28.221005
284.026175	14402.035989	28.226023
285.200646	14421.789519	28.231040
285.343262	14450.358144	28.236058
285.575397	14473.229841	28.241076
285.676794	14488.271152	28.246093
285.711893	14496.015045	28.251111
286.504760	14515.800219	28.256128
286.434654	14556.679377	28.261146
286.879183	14567.582836	28.266164
287.305487	14589.661524	28.271181
287.405235	14605.765285	28.276199
287.690986	14626.581413	28.281216
287.965574	14670.218245	28.286234
288.369249	14685.881082	28.291252
288.388662	14690.893682	28.296269
288.696216	14731.515492	28.301287
289.042958	14742.931597	28.306304
289.549940	14763.300072	28.311322
289.753715	14787.647109	28.316340
289.948270	14817.184790	28.321357
290.204527	14840.393392	28.326375
290.558967	14862.979125	28.331392
289.987061	14896.330940	28.336410
290.876943	14921.445701	28.341428
291.656253	14950.636468	28.346445
291.520942	14988.623276	28.351463
291.791993	14985.110239	28.356480
292.030702	15017.671272	28.361498
292.321749	15046.279458	28.366516
292.740501	15093.070453	28.371533
293.344192	15101.979781	28.376551
293.888144	15108.497432	28.381568
293.890627	15147.145753	28.386586
294.014152	15164.903909	28.391604
294.482518	15174.524270	28.396621
294.656484	15212.277710	28.401639
295.067167	15245.444273	28.406656
295.356458	15276.084405	28.411674
295.402892	15278.949584	28.416692
295.958397	15299.421027	28.421709
296.364375	15321.682141	28.426727
297.221912	15321.786402	28.431744
297.933343	15335.418193	28.436762
297.984420	15352.480970	28.441780
298.618540	15353.148472	28.446797
298.874052	15359.787942	28.451815
299.518454	15373.616789	28.456832
299.485887	15378.207983	28.461850
299.677758	15379.263718	28.466868
299.821948	15375.298802	28.471885
299.485551	15401.384335	28.476903
300.024691	15410.274558	28.481920
299.987736	15446.738099	28.486938
299.885859	15456.567873	28.491956
300.526383	15452.013517	28.496973
300.348306	15465.069051	28.501991
300.599202	15515.743541	28.507008
300.698496	15535.102452	28.512026
300.799990	15537.241563	28.517044
301.456278	15571.546963	28.522061
301.492000	15621.456789	28.527079
302.232349	15648.772087	28.532096
302.618924	15664.377238	28.537114
302.921289	15685.604861	28.542132
303.447247	15693.413215	28.547149
303.228888	15727.107018	28.552167
304.258661	15751.427778	28.557184
304.244512	15769.140000	28.562202
304.673065	15794.266145	28.567220
304.942037	15822.193835	28.572237
305.005888	15836.509809	28.577255
305.507004	15858.658238	28.582272
305.888158	15870.674598	28.587290
306.029177	15900.576094	28.592308
306.302025	15943.707620	28.597325
306.392182	15964.146468	28.602343
306.673040	15980.134997	28.607360
307.034731	16023.879269	28.612378
307.304137	16034.711793	28.617396
307.506794	16049.134247	28.622413
307.815360	16098.499319	28.627431
308.322339	16120.079806	28.632448
308.367505	16147.542308	28.637466
308.657725	16192.777055	28.642484
308.815140	16213.008112	28.647501
309.127749	16248.586759	28.652519
309.944028	16288.472831	28.657536
310.365443	16305.919839	28.662554
310.659336	16325.956713	28.667572
310.829304	16362.774223	28.672589
311.204079	16391.659342	28.677607
311.471114	16417.429327	28.682624
311.981607	16442.963715	28.687642
312.555091	16479.867694	28.692660
313.040043	16498.604574	28.697677
313.279799	16520.529170	28.702695
313.545159	16536.709922	28.707712
313.609080	16551.882258	28.712730
313.807035	16560.988651	28.717748
314.416247	16599.329004	28.722765
314.205184	16628.814058	28.727783
314.883994	16648.080129	28.732800
315.007610	16678.181345	28.737818
315.185612	16708.740121	28.742836
315.677941	16724.294148	28.747853
315.983785	16761.205155	28.752871
316.664499	16777.437302	28.757888
316.762827	16800.192541	28.762906
317.227572	16838.388691	28.767924
317.422792	16836.159612	28.772941
317.646516	16878.234779	28.777959
317.888476	16913.594876	28.782976
318.214886	16935.795697	28.787994
318.595342	16955.302117	28.793012
319.245695	16972.050098	28.798029
319.393066	17009.750631	28.803047
319.313353	17017.913421	28.808064
319.618647	17049.282359	28.813082
320.020111	17080.709542	28.818100
320.441578	17096.360736	28.823117
320.860766	17130.634519	28.828135
321.237277	17148.942473	28.833152
321.648086	17177.871887	28.838170
321.797902	17198.620780	28.843188
322.003757	17190.024341	28.848205
322.594194	17219.020291	28.853223
323.059014	17250.582329	28.858240
323.184244	17266.433923	28.863258
323.222129	17289.608019	28.868276
323.920583	17302.320058	28.873293
323.691867	17331.071708	28.878311
324.061611	17376.567671	28.883328
324.656273	17393.265397	28.888346
324.946859	17415.800605	28.893364
326.095675	17422.502959	28.898381
326.419575	17434.802590	28.903399
326.504100	17468.103209	28.908416
326.913871	17473.400484	28.913434
326.726170	17497.004576	28.918452
327.174337	17504.640683	28.923469
327.622921	17516.754292	28.928487
327.605868	17543.017431	28.933504
328.151676	17581.545505	28.938522
327.861372	17618.660950	28.943540
328.392874	17637.990354	28.948557
328.618368	17650.744550	28.953575
328.679533	17690.541298	28.958592
329.214563	17721.134394	28.963610
329.469221	17755.167156	28.968628
330.069784	17774.611399	28.973645
329.927612	17810.818626	28.978663
330.575175	17866.032305	28.983680
331.150147	17891.203686	28.988698
331.069883	17913.925355	28.993716
331.437371	17953.285991	28.998733
331.813983	17986.807346	29.003751
332.014251	18009.208561	29.008768
332.990950	18038.058618	29.013786
333.104568	18085.885787	29.018804
333.914535	18107.100475	29.023821
333.805982	18123.342991	29.028839
334.125990	18152.421520	29.033856
335.304585	18171.425575	29.038874
335.188372	18203.903440	29.043892
335.809887	18231.553196	29.048909
336.182531	18236.932508	29.053927
336.381426	18235.714506	29.058944
336.713579	18275.140068	29.063962
336.926593	18306.501438	29.068980
337.533911	18319.104814	29.073997
337.673148	18317.105443	29.079015
337.955441	18361.661874	29.084032
338.422743	18387.457040	29.089050
338.426979	18406.693200	29.094068
338.429850	18421.610984	29.099085
339.164213	18451.389171	29.104103
339.493920	18478.882652	29.109120
340.238967	18494.396618	29.114138
340.247773	18527.787547	29.119156
340.499646	18569.101119	29.124173
340.846570	18581.210245	29.129191
341.105053	18586.323248	29.134208
341.334523	18622.461407	29.139226
341.630474	18655.117953	29.144244
341.869165	18685.909962	29.149261
342.200094	18710.761975	29.154279
342.425676	18757.423572	29.159296
342.684877	18776.781965	29.164314
343.123663	18804.128724	29.169332
343.360986	18852.963774	29.174349
343.379279	18873.577315	29.179367
343.634392	18914.941656	29.184384
344.211630	18957.031524	29.189402
344.472437	18969.650087	29.194420
345.093022	18985.189807	29.199437
345.413037	19029.941989	29.204455
345.840778	19086.009395	29.209472
346.057119	19101.332289	29.214490
346.235403	19127.368658	29.219508
346.628663	19164.943668	29.224525
347.188280	19185.203369	29.229543
347.234436	19223.803649	29.234560
347.967985	19262.862631	29.239578
347.958511	19303.032743	29.244596
348.258750	19326.656572	29.249613
348.679731	19375.893138	29.254631
349.019788	19402.585724	29.259648
349.537814	19446.113114	29.264666
349.660572	19486.662192	29.269684
350.179398	19509.977483	29.274701
350.741186	19542.137910	29.279719
350.647672	19575.021391	29.284736
351.284415	19611.149602	29.289754
351.740309	19659.879998	29.294772
352.349034	19699.340512	29.299789
352.522862	19716.491582	29.304807
352.721892	19757.736467	29.309824
353.288376	19775.130105	29.314842
353.553347	19806.534606	29.319860
354.206546	19849.526863	29.324877
354.193303	19878.319859	29.329895
354.968605	19916.128229	29.334912
355.455128	19930.923341	29.339930
355.493687	19971.457565	29.344948
355.644387	20009.761827	29.349965
356.146777	20054.016917	29.354983
356.850148	20066.840637	29.360000
357.079638	20072.004605	29.365018
357.612813	20109.706821	29.370036
358.235585	20136.383838	29.375053
358.384324	20177.983287	29.380071
358.806353	20199.643080	29.385088
359.429735	20196.017147	29.390106
359.434976	20235.772520	29.395124
359.870658	20286.737007	29.400141
360.364407	20301.624260	29.405159
360.496863	20318.871063	29.410176
360.998414	20356.276410	29.415194
361.079668	20383.070079	29.420212
361.431936	20409.986112	29.425229
361.909211	20439.781989	29.430247
362.095247	20490.354849	29.435264
362.551362	20495.837765	29.440282
362.815490	20510.178318	29.445300
363.193851	20554.899762	29.450317
363.533635	20593.073248	29.455335
363.686816	20612.140765	29.460352
364.159610	20639.313120	29.465370
364.596589	20667.092028	29.470388
364.939088	20721.758758	29.475405
365.463441	20737.093763	29.480423
365.361520	20773.603482	29.485440
365.843342	20822.080793	29.490458
366.593897	20844.926185	29.495476
366.653091	20872.887648	29.500493
367.154961	20899.459758	29.505511
367.343858	20954.811553	29.510528
368.094551	20966.437990	29.515546
368.223144	20980.284285	29.520564
368.239080	21026.197134	29.525581
368.746843	21048.799165	29.530599
368.946641	21078.054032	29.535616
369.806862	21114.594725	29.540634
369.939059	21149.974151	29.545652
370.266917	21161.520817	29.550669
370.697506	21196.772229	29.555687
370.788902	21218.907296	29.560704
371.375530	21228.235821	29.565722
371.867865	21283.811303	29.570740
372.000929	21330.017769	29.575757
372.681362	21344.159428	29.580775
373.095396	21370.005884	29.585792
373.630380	21406.646663	29.590810
373.933127	21418.241796	29.595828
373.939033	21455.075702	29.600845
374.637452	21492.767949	29.605863
374.827655	21525.873257	29.610880
375.378050	21532.944180	29.615898
375.786971	21570.381750	29.620916
375.875177	21612.368400	29.625933
376.653146	21648.372099	29.630951
376.828397	21673.470248	29.635968
377.079017	21697.132448	29.640986
378.109877	21729.145537	29.646004
377.859985	21769.913082	29.651021
378.478083	21790.696004	29.656039
378.896012	21829.988163	29.661056
379.200510	21871.208253	29.666074
379.548156	21888.580358	29.671092
379.753697	21912.349628	29.676109
380.547567	21956.553750	29.681127
380.365180	21979.048769	29.686144
380.797249	22015.772523	29.691162
381.287020	22070.007886	29.696180
381.620636	22110.400830	29.701197
381.773535	22136.471331	29.706215
382.063423	22169.488929	29.711232
382.581524	22213.709333	29.716250
383.066615	22246.932890	29.721268
383.140864	22273.658234	29.726285
384.092654	22324.428613	29.731303
384.145644	22354.296430	29.736320
384.679636	22391.220154	29.741338
385.602241	22428.245299	29.746356
385.630732	22472.231962	29.751373
386.032271	22492.304261	29.756391
386.580059	22524.947310	29.761408
386.876087	22541.009066	29.766426
387.333046	22578.221821	29.771444
387.039312	22619.750681	29.776461
387.798180	22656.186953	29.781479
388.334051	22699.866529	29.786496
389.072851	22707.460200	29.791514
389.749479	22731.149661	29.796532
390.148828	22774.522486	29.801549
390.541202	22791.566525	29.806567
390.845148	22831.581431	29.811584
391.052789	22863.054768	29.816602
391.397455	22886.258525	29.821620
391.559985	22907.017195	29.826637
392.013111	22920.029512	29.831655
392.031872	22970.935486	29.836672
392.272699	23017.939168	29.841690
392.808892	23025.374112	29.846708
393.098729	23084.857949	29.851725
393.690937	23114.926560	29.856743
393.652373	23143.592205	29.861760
394.139705	23178.423782	29.866778
394.833918	23222.783300	29.871796
394.982520	23251.870694	29.876813
395.887242	23267.362771	29.881831
396.591455	23293.867431	29.886848
396.469025	23324.529026	29.891866
397.084464	23361.908111	29.896884
396.907064	23399.503385	29.901901
397.639836	23432.101879	29.906919
397.932073	23454.258751	29.911936
398.350053	23491.637634	29.916954
398.936140	23546.984417	29.921972
398.836122	23574.035446	29.926989
399.763813	23611.306747	29.932007
400.001095	23649.642889	29.937024
400.404462	23677.065000	29.942042
400.825875	23685.132512	29.947060
400.632546	23741.425383	29.952077
401.310173	23781.727686	29.957095
401.410178	23834.937369	29.962112
402.042113	23872.910840	29.967130
402.748766	23891.286808	29.972148
402.674633	23949.242976	29.977165
403.192529	24007.295476	29.982183
403.774981	24045.813578	29.987200
404.168608	24075.867836	29.992218
404.961121	24103.462861	29.997236
405.259893	24158.550087	30.002253
406.196152	24188.327284	30.007271
406.668766	24210.054878	30.012288
407.032072	24220.724320	30.017306
407.743070	24270.728374	30.022324
407.476254	24293.147406	30.027341
408.054070	24326.252547	30.032359
408.530258	24367.973868	30.037376
408.749175	24402.048201	30.042394
409.375978	24425.956413	30.047412
409.544235	24456.756520	30.052429
409.890199	24492.593307	30.057447
410.341761	24532.814920	30.062464
410.518556	24568.892670	30.067482
411.028958	24617.893407	30.072500
411.361336	24646.522404	30.077517
412.014008	24696.748637	30.082535
412.392157	24732.870735	30.087552
412.652953	24749.191123	30.092570
413.275498	24799.063141	30.097588
413.309905	24827.870958	30.102605
413.731249	24861.174861	30.107623
414.275200	24919.587269	30.112640
414.362947	24962.790149	30.117658
415.148056	24995.450827	30.122676
415.316516	25023.237166	30.127693
415.375943	25074.365089	30.132711
416.236329	25140.590905	30.137728
416.101703	25171.980025	30.142746
416.873194	25198.288937	30.147764
417.586362	25242.358937	30.152781
418.134362	25291.301803	30.157799
418.401676	25334.983694	30.162816
419.194852	25369.510684	30.167834
419.952733	25398.889023	30.172852
420.218364	25423.558408	30.177869
420.649723	25467.757539	30.182887
421.092339	25475.571699	30.187904
421.337054	25525.065185	30.192922
422.119769	25566.037147	30.197940
422.407509	25572.550835	30.202957
422.670331	25605.316311	30.207975
422.802765	25627.631732	30.212992
422.781898	25668.619998	30.218010
423.314419	25708.132498	30.223028
423.671994	25740.322809	30.228045
424.270575	25768.097662	30.233063
424.736082	25830.711079	30.238080
424.632478	25874.520278	30.243098
425.073727	25900.397590	30.248116
425.217102	25935.854607	30.253133
425.781674	25999.830447	30.258151
426.081489	26038.384006	30.263168
426.673141	26090.731131	30.268186
427.091220	26130.156289	30.273204
427.398500	26176.735174	30.278221
427.865279	26219.861293	30.283239
428.540184	26276.448066	30.288256
428.794468	26308.746397	30.293274
429.638261	26357.567785	30.298292
430.166894	26431.446147	30.303309
430.436940	26463.832051	30.308327
431.162475	26485.582288	30.313344
431.508830	26535.599646	30.318362
431.972731	26560.737808	30.323380
432.823092	26606.343516	30.328397
433.116144	26653.408589	30.333415
434.046839	26677.323400	30.338432
434.551083	26697.587163	30.343450
435.038909	26731.544482	30.348468
435.472317	26769.506783	30.353485
435.855413	26795.664718	30.358503
436.098020	26821.068473	30.363520
436.289830	26877.743350	30.368538
436.749953	26905.590242	30.373556
437.071597	26926.441098	30.378573
437.412405	26969.066378	30.383591
437.884125	27023.285933	30.388608
437.913699	27074.607717	30.393626
438.551639	27107.060229	30.398644
438.796889	27139.968754	30.403661
439.209967	27195.649344	30.408679
439.988242	27258.662622	30.413696
439.802476	27299.126948	30.418714
440.277670	27324.447300	30.423732
440.688626	27378.873564	30.428749
441.116263	27435.031930	30.433767
441.728284	27476.257467	30.438784
442.132650	27524.856732	30.443802
442.830274	27575.237013	30.448820
443.236633	27629.768916	30.453837
443.417596	27669.019170	30.458855
444.078641	27704.206685	30.463872
444.604441	27763.920266	30.468890
445.833567	27812.084478	30.473908
446.120101	27835.989047	30.478925
446.305283	27873.166864	30.483943
447.143026	27912.921075	30.488960
447.313016	27948.193359	30.493978
447.604690	27996.270077	30.498996
448.011605	28046.305504	30.504013
448.552684	28071.064114	30.509031
449.299056	28091.568674	30.514048
449.438279	28148.054577	30.519066
449.956628	28193.678363	30.524084
450.499975	28228.274499	30.529101
450.806430	28271.063245	30.534119
451.660993	28303.586333	30.539136
451.665103	28326.226118	30.544154
452.052429	28352.587599	30.549172
452.286014	28399.530088	30.554189
452.787978	28454.174985	30.559207
453.547621	28480.487780	30.564224
453.787670	28512.526096	30.569242
454.235758	28544.785595	30.574260
454.685716	28597.222152	30.579277
454.649025	28638.857288	30.584295
455.078461	28672.854914	30.589312
455.529150	28724.187768	30.594330
456.038681	28755.081204	30.599348
456.551241	28811.267895	30.604365
456.786905	28864.658543	30.609383
457.625438	28917.363085	30.614400
457.852444	28961.024625	30.619418
458.231227	29020.807863	30.624436
458.570531	29053.158832	30.629453
459.359383	29089.428918	30.634471
460.063322	29138.027423	30.639488
460.732186	29206.377740	30.644506
460.987755	29244.480565	30.649524
461.748519	29265.479379	30.654541
462.123870	29309.861715	30.659559
462.613536	29365.612391	30.664576
463.066298	29422.467051	30.669594
463.955811	29436.972114	30.674612
464.458753	29465.104713	30.679629
464.353146	29518.153152	30.684647
464.564887	29576.010207	30.689664
465.324710	29624.187630	30.694682
465.858552	29661.441045	30.699700
465.990419	29692.663512	30.704717
466.517066	29750.570076	30.709735
467.106796	29802.069280	30.714752
467.443382	29847.677000	30.719770
467.762615	29884.742382	30.724788
468.229614	29954.728294	30.729805
468.630286	29984.582025	30.734823
469.033168	30037.456584	30.739840
469.500363	30104.594603	30.744858
470.050817	30143.227966	30.749876
470.590558	30213.597217	30.754893
470.921131	30270.884930	30.759911
471.460969	30308.192375	30.764928
472.092886	30343.743404	30.769946
472.488795	30398.888305	30.774964
473.144304	30460.226993	30.779981
473.624049	30518.916731	30.784999
474.428271	30556.304067	30.790016
474.781735	30598.898389	30.795034
475.200886	30648.084454	30.800052
475.621567	30675.617471	30.805069
476.332769	30739.212924	30.810087
476.582575	30798.714459	30.815104
476.939372	30848.731584	30.820122
477.516190	30886.614610	30.825140
477.999484	30928.440655	30.830157
478.224884	30990.246586	30.835175
479.100945	31040.762098	30.840192
479.828959	31072.995854	30.845210
479.953018	31123.260418	30.850228
480.399595	31161.279123	30.855245
480.705986	31219.441487	30.860263
481.195718	31244.497056	30.865280
481.965939	31313.002984	30.870298
482.447957	31383.954352	30.875316
482.776267	31407.632981	30.880333
483.159642	31418.522862	30.885351
483.825440	31463.222370	30.890368
484.180727	31528.819643	30.895386
484.785167	31568.523020	30.900404
485.328083	31602.517121	30.905421
485.707035	31665.186563	30.910439
485.999808	31681.826897	30.915456
486.389400	31718.789928	30.920474
486.705710	31787.353768	30.925492
487.580181	31818.454239	30.930509
487.475382	31879.213693	30.935527
487.762620	31923.904351	30.940544
488.366161	31981.452312	30.945562
489.158467	32059.702704	30.950580
489.622542	32110.248358	30.955597
490.078485	32160.969017	30.960615
490.555109	32211.203716	30.965632
490.825682	32274.760826	30.970650
491.158708	32331.758355	30.975668
492.024614	32387.541762	30.980685
492.714861	32429.778908	30.985703
493.406409	32481.717224	30.990720
493.945689	32541.404038	30.995738
494.016008	32590.640581	31.000756
494.785585	32629.852170	31.005773
495.100568	32692.144647	31.010791
495.564111	32754.551625	31.015808
495.920950	32820.557317	31.020826
496.509903	32855.344456	31.025844
497.316766	32921.033263	31.030861
497.842331	32976.587662	31.035879
498.373127	33007.276927	31.040896
499.102335	33057.816228	31.045914
499.271595	33127.532780	31.050932
500.025694	33178.566809	31.055949
500.500177	33221.223260	31.060967
501.228165	33274.744883	31.065984
501.459991	33333.904652	31.071002
501.951706	33381.149232	31.076020
502.426623	33421.080132	31.081037
502.940022	33499.730080	31.086055
503.461687	33559.145619	31.091072
503.906560	33585.303614	31.096090
504.159588	33631.685937	31.101108
504.830727	33693.525595	31.106125
505.381460	33735.921447	31.111143
505.674281	33798.420278	31.116160
506.433859	33863.896408	31.121178
506.395028	33914.684927	31.126196
507.213386	33974.863736	31.131213
507.698135	34046.437531	31.136231
508.382948	34104.846705	31.141248
509.082480	34147.512403	31.146266
509.509287	34202.345515	31.151284
509.878886	34258.182138	31.156301
510.010574	34321.867398	31.161319
510.745345	34382.124508	31.166336
511.783656	34436.926762	31.171354
512.034470	34478.212810	31.176372
512.487303	34539.343700	31.181389
512.909747	34615.987972	31.186407
513.336768	34681.705072	31.191424
513.788465	34719.465605	31.196442
514.083266	34774.675689	31.201460
514.996698	34840.647501	31.206477
515.390575	34892.809335	31.211495
515.946900	34950.926998	31.216512
516.737368	35006.125353	31.221530
516.764778	35058.373447	31.226548
517.492329	35102.923726	31.231565
518.000555	35144.411773	31.236583
518.285855	35220.743691	31.241600
518.944525	35271.676482	31.246618
519.589435	35320.283011	31.251636
520.097681	35355.517554	31.256653
520.574290	35411.513687	31.261671
521.165139	35486.729752	31.266688
521.919426	35527.887757	31.271706
521.937977	35605.871505	31.276724
522.486483	35646.300154	31.281741
522.955331	35696.801668	31.286759
523.389280	35767.731320	31.291776
524.113336	35823.697349	31.296794
524.349565	35873.205942	31.301812
525.359506	35926.209397	31.306829
525.932443	36004.134879	31.311847
526.368687	36050.338656	31.316864
527.065265	36101.437967	31.321882
527.410980	36166.192622	31.326900
528.032342	36210.245711	31.331917
528.702489	36266.553372	31.336935
529.239088	36332.731820	31.341952
529.515526	36375.365479	31.346970
529.656970	36452.117733	31.351988
530.254870	36525.178596	31.357005
531.028468	36579.829243	31.362023
531.434839	36639.823236	31.367040
532.109761	36683.963320	31.372058
532.503710	36777.330733	31.377076
532.855289	36852.724626	31.382093
533.647710	36902.696454	31.387111
534.182826	36977.224304	31.392128
534.926436	37027.141429	31.397146
535.300648	37092.712063	31.402164
535.822474	37157.968231	31.407181
536.899705	37219.121966	31.412199
537.276198	37265.736382	31.417216
538.188111	37312.473922	31.422234
538.730269	37388.507615	31.427252
538.868116	37435.714149	31.432269
539.855610	37483.380072	31.437287
540.002183	37536.871745	31.442304
540.497669	37597.936669	31.447322
540.661159	37664.967469	31.452340
541.253289	37715.981356	31.457357
541.742701	37770.266014	31.462375
542.221659	37838.476131	31.467392
542.719640	37923.589280	31.472410
543.404622	38002.284464	31.477428
543.615911	38051.257241	31.482445
544.370971	38125.144453	31.487463
544.597493	38195.966517	31.492480
545.170957	38242.509913	31.497498
546.137918	38306.478557	31.502516
546.699403	38393.082505	31.507533
547.427631	38455.364811	31.512551
547.538737	38516.401666	31.517568
548.726702	38571.864157	31.522586
548.846707	38660.669433	31.527604
549.328989	38708.848116	31.532621
550.080284	38776.171003	31.537639
550.800874	38838.537953	31.542656
551.553098	38898.387697	31.547674
551.651183	38968.766920	31.552692
552.139074	39013.735800	31.557709
552.543978	39079.718903	31.562727
553.100983	39162.117103	31.567744
553.645247	39216.494903	31.572762
553.974608	39263.914463	31.577780
554.501370	39324.828589	31.582797
555.190476	39403.112607	31.587815
555.563338	39487.916106	31.592832
556.525741	39520.035021	31.597850
556.825559	39602.632359	31.602868
557.513508	39674.690661	31.607885
557.871260	39728.993498	31.612903
558.664588	39788.337572	31.617920
559.651482	39847.015476	31.622938
560.050685	39925.504290	31.627956
560.321366	39983.344598	31.632973
561.042344	40040.400566	31.637991
561.417926	40110.233398	31.643008
562.153319	40187.029730	31.648026
562.680431	40257.851259	31.653044
563.080948	40313.095662	31.658061
563.919382	40375.934520	31.663079
564.291012	40449.048688	31.668096
565.070243	40517.648589	31.673114
565.415958	40596.931904	31.678132
565.664480	40653.663824	31.683149
566.617307	40728.368605	31.688167
567.000783	40813.605809	31.693184
567.272276	40865.918850	31.698202
568.102725	40945.527639	31.703220
568.212505	41014.678720	31.708237
569.049826	41108.187856	31.713255
569.473728	41194.707982	31.718272
570.514130	41235.901260	31.723290
571.314947	41321.895743	31.728308
571.380915	41421.294401	31.733325
572.309285	41480.018815	31.738343
572.940784	41566.395940	31.743360
573.427341	41620.525328	31.748378
573.963177	41687.945116	31.753396
574.561040	41763.249375	31.758413
574.948981	41852.628899	31.763431
575.406290	41934.295410	31.768448
576.052415	41991.174152	31.773466
576.958521	42057.129477	31.778484
577.386646	42152.959029	31.783501
578.431190	42203.307930	31.788519
579.203962	42292.038913	31.793536
579.855115	42358.596155	31.798554
580.266939	42426.683098	31.803572
580.766873	42503.919502	31.808589
581.465279	42552.464108	31.813607
581.663331	42609.106265	31.818624
582.292555	42697.231584	31.823642
583.187072	42775.363593	31.828660
583.506255	42839.262646	31.833677
584.381637	42904.500054	31.838695
584.539797	42973.615818	31.843712
585.135094	43050.633583	31.848730
585.539334	43122.878638	31.853748
586.454744	43195.292095	31.858765
587.269637	43269.202970	31.863783
587.242720	43342.555521	31.868800
588.166793	43403.297695	31.873818
588.455923	43479.165077	31.878836
589.310174	43576.140733	31.883853
590.122056	43623.450890	31.888871
590.621792	43699.120238	31.893888
591.243028	43767.578480	31.898906
591.980643	43817.720486	31.903924
592.285231	43882.812556	31.908941
593.092732	43966.851594	31.913959
593.534156	44021.494306	31.918976
594.211203	44090.332829	31.923994
594.795805	44145.870927	31.929012
594.917950	44204.162658	31.934029
595.833810	44270.061178	31.939047
596.298442	44352.725342	31.944064
596.719930	44418.876518	31.949082
597.344623	44481.335417	31.954100
597.958923	44553.630305	31.959117
598.376713	44636.906461	31.964135
598.908737	44723.510578	31.969152
599.308523	44784.650122	31.974170
600.015246	44849.189833	31.979188
600.584890	44933.821875	31.984205
601.514237	45021.880314	31.989223
601.930973	45121.802966	31.994240
602.722269	45182.812863	31.999258
603.323431	45237.780064	32.004276
603.834527	45323.812685	32.009293
604.398148	45415.674598	32.014311
604.899502	45500.800388	32.019328
605.539387	45568.763377	32.024346
606.192738	45652.794477	32.029364
607.098318	45736.929530	32.034381
607.792012	45796.953572	32.039399
608.062204	45889.740833	32.044416
608.680269	45952.717249	32.049434
609.462361	46049.477816	32.054452
609.709472	46143.173124	32.059469
610.734940	46203.399420	32.064487
611.004336	46290.205754	32.069504
611.593650	46395.483612	32.074522
612.229988	46487.578753	32.079540
612.613631	46561.236143	32.084557
613.620886	46645.409021	32.089575
614.002547	46746.706993	32.094592
614.623130	46817.743530	32.099610
615.248277	46916.097410	32.104628
615.316022	47001.020643	32.109645
616.065835	47092.358024	32.114663
617.038159	47205.019248	32.119680
617.649111	47284.748454	32.124698
618.564012	47366.382279	32.129716
619.029020	47454.026848	32.134733
620.039330	47545.951757	32.139751
620.456291	47633.942954	32.144768
621.495451	47691.607874	32.149786
622.418715	47768.603653	32.154804
622.787926	47850.891750	32.159821
623.318562	47933.977675	32.164839
623.956897	48018.804956	32.169856
624.768809	48094.819505	32.174874
625.385045	48167.870103	32.179892
625.878292	48263.789885	32.184909
626.175911	48340.032453	32.189927
626.620800	48432.285583	32.194944
627.171034	48510.492233	32.199962
628.031083	48576.784628	32.204980
627.929122	48682.265250	32.209997
628.588274	48787.251307	32.215015
629.665488	48865.565016	32.220032
630.521626	48946.602800	32.225050
631.507432	49021.221903	32.230068
632.040850	49116.618350	32.235085
632.904650	49209.740790	32.240103
633.475052	49255.826214	32.245120
634.312444	49314.268350	32.250138
634.884203	49391.900370	32.255156
634.987753	49479.866667	32.260173
635.969227	49540.616186	32.265191
636.561798	49617.598335	32.270208
637.002313	49702.930050	32.275226
637.695349	49764.956334	32.280244
638.196542	49840.902907	32.285261
638.398298	49940.371951	32.290279
639.260673	50026.112291	32.295296
639.645653	50096.413765	32.300314
640.265854	50169.790386	32.305332
640.813522	50268.120841	32.310349
641.516897	50345.864500	32.315367
642.229000	50453.582682	32.320384
642.980675	50558.942220	32.325402
643.464072	50637.083410	32.330420
643.767517	50717.354733	32.335437
644.161570	50816.483946	32.340455
645.009512	50942.060200	32.345472
645.486953	51034.036366	32.350490
646.600807	51112.849116	32.355508
646.788758	51224.937442	32.360525
647.474771	51314.631931	32.365543
648.342310	51415.025101	32.370560
648.869932	51526.496945	32.375578
649.842756	51622.566071	32.380596
650.109229	51715.521492	32.385613
651.153788	51809.144734	32.390631
651.740310	51922.744109	32.395648
652.536981	52039.676150	32.400666
653.511301	52131.114419	32.405684
654.159619	52213.334240	32.410701
654.863666	52291.916328	32.415719
655.534972	52397.390846	32.420736
656.091268	52513.136881	32.425754
656.724231	52598.639235	32.430772
657.788872	52679.983760	32.435789
658.310767	52772.507314	32.440807
659.477576	52859.865065	32.445824
660.194128	52926.897456	32.450842
661.054380	53021.643533	32.455860
661.553377	53106.159571	32.460877
662.532130	53177.688195	32.465895
663.166655	53262.305714	32.470912
663.970463	53331.558128	32.475930
664.914345	53408.424859	32.480948
665.361399	53482.221771	32.485965
666.551215	53546.319723	32.490983
667.421721	53616.143308	32.496000
668.140516	53675.992316	32.501018
668.824811	53748.437119	32.506036
669.059118	53830.665881	32.511053
669.598522	53878.959592	32.516071
670.401188	53949.193562	32.521088
670.777504	54027.148274	32.526106
671.367929	54096.552377	32.531124
671.831423	54165.150137	32.536141
672.434893	54252.878864	32.541159
672.965539	54346.943592	32.546176
673.340602	54412.726697	32.551194
673.706180	54479.282302	32.556212
674.181607	54573.174042	32.561229
674.425374	54696.126499	32.566247
675.524510	54802.677450	32.571264
675.848242	54894.561586	32.576282
676.497414	54971.634804	32.581300
677.047114	55081.815800	32.586317
677.810288	55168.423035	32.591335
678.811262	55249.804669	32.596352
679.462631	55355.251206	32.601370
680.438926	55423.636046	32.606388
680.871777	55500.942928	32.611405
681.382903	55607.829139	32.616423
682.138610	55705.622273	32.621440
682.563589	55785.742959	32.626458
683.303730	55895.448535	32.631476
683.670907	55987.463310	32.636493
684.059827	56088.300927	32.641511
684.883930	56199.940234	32.646528
685.262280	56295.195671	32.651546
685.930339	56398.762342	32.656564
686.502232	56528.021645	32.661581
687.244403	56643.644691	32.666599
688.349301	56731.687144	32.671616
688.876599	56843.556031	32.676634
689.720903	56957.755129	32.681652
690.427353	57065.754286	32.686669
691.011650	57172.567436	32.691687
692.047362	57271.541541	32.696704
692.658454	57396.017191	32.701722
693.370953	57508.156225	32.706740
694.200207	57626.632844	32.711757
694.582960	57736.060204	32.716775
695.505927	57817.060999	32.721792
696.264411	57927.400400	32.726810
697.026905	58050.553578	32.731828
697.928295	58162.987376	32.736845
698.616919	58250.846302	32.741863
699.510833	58349.817637	32.746880
700.059095	58472.876130	32.751898
700.848888	58587.826612	32.756916
701.341194	58689.570337	32.761933
701.884149	58794.276003	32.766951
703.060021	58896.893623	32.771968
703.649557	59013.610971	32.776986
704.348404	59103.146455	32.782004
704.920843	59223.690727	32.787021
705.960441	59318.042725	32.792039
706.715139	59437.401842	32.797056
707.609881	59537.111948	32.802074
708.381575	59614.568555	32.807092
709.253947	59713.297481	32.812109
709.672050	59837.409583	32.817127
710.584938	59923.096717	32.822144
710.966554	60037.838622	32.827162
711.722602	60151.830567	32.832180
712.574470	60227.399533	32.837197
713.281302	60330.506420	32.842215
713.862921	60438.639331	32.847232
714.403506	60568.454629	32.852250
715.121046	60668.155409	32.857268
716.124853	60753.142283	32.862285
716.730062	60862.840776	32.867303
717.331849	60980.130011	32.872320
717.872837	61076.064024	32.877338
718.377715	61191.341963	32.882356
719.245128	61290.951572	32.887373
719.800839	61408.124522	32.892391
720.457929	61530.792065	32.897408
721.600463	61653.089489	32.902426
721.779897	61732.010798	32.907444
722.952985	61855.088036	32.912461
723.545371	61972.416202	32.917479
724.319551	62068.158439	32.922496
725.003976	62173.130155	32.927514
725.763889	62268.572351	32.932532
726.906603	62373.532627	32.937549
727.513331	62459.230581	32.942567
728.279311	62549.181154	32.947584
728.640162	62664.409133	32.952602
729.364819	62757.754929	32.957620
730.281666	62857.793865	32.962637
730.981475	62964.309217	32.967655
731.737982	63068.319352	32.972672
731.882098	63189.090853	32.977690
732.695670	63292.764070	32.982708
733.565514	63395.379381	32.987725
734.032623	63509.223137	32.992743
734.824426	63638.214018	32.997760
735.636916	63757.797766	33.002778
736.412314	63862.036370	33.007796
737.407567	63969.961867	33.012813
737.837631	64080.566291	33.017831
738.413053	64189.276477	33.022848
739.222021	64315.506800	33.027866
740.170649	64437.758233	33.032884
741.222566	64552.712128	33.037901
741.830077	64677.334624	33.042919
742.544861	64778.054736	33.047936
743.564109	64868.416176	33.052954
744.100382	64995.176089	33.057972
745.180070	65114.199039	33.062989
745.645308	65230.296529	33.068007
746.162487	65344.218084	33.073024
747.017833	65448.590627	33.078042
747.449436	65575.959242	33.083060
748.467632	65709.426212	33.088077
749.017218	65817.965995	33.093095
750.086778	65928.215627	33.098112
750.605241	66050.781579	33.103130
751.114612	66182.805969	33.108148
752.100839	66281.023433	33.113165
752.741686	66434.772066	33.118183
753.524055	66561.564196	33.123200
754.351110	66676.529175	33.128218
755.025525	66798.163563	33.133236
756.121505	66934.887347	33.138253
756.615519	67060.592330	33.143271
757.492215	67179.616479	33.148288
758.307530	67291.110094	33.153306
758.960152	67415.855481	33.158324
759.803102	67532.718998	33.163341
760.754317	67665.021230	33.168359
761.666643	67779.567350	33.173376
762.197609	67925.203109	33.178394
762.917388	68049.726276	33.183412
763.935324	68139.722960	33.188429
764.498053	68271.347249	33.193447
765.522846	68394.519853	33.198464
766.255112	68514.877757	33.203482
766.710055	68634.194808	33.208500
767.952724	68766.696133	33.213517
768.503375	68883.824112	33.218535
769.508868	68988.568995	33.223552
770.483383	69098.471851	33.228570
770.818923	69235.734592	33.233588
771.819580	69360.478387	33.238605
772.163852	69471.226938	33.243623
773.290901	69585.886590	33.248640
774.012630	69704.337494	33.253658
774.870072	69814.105381	33.258676
775.873158	69919.519132	33.263693
776.358152	70046.830429	33.268711
777.002275	70163.924825	33.273728
777.951518	70259.676204	33.278746
778.719041	70372.502845	33.283764
779.341118	70501.880601	33.288781
779.841775	70625.013759	33.293799
780.599788	70723.764000	33.298816
781.559533	70827.975557	33.303834
781.869217	70949.858694	33.308852
783.007824	71075.297981	33.313869
783.420780	71207.079188	33.318887
783.966940	71315.091722	33.323904
785.168039	71429.293947	33.328922
785.695212	71560.641200	33.333940
786.405095	71702.258709	33.338957
787.194646	71823.410069	33.343975
787.925985	71937.174136	33.348992
788.730831	72079.518236	33.354010
789.340606	72209.509106	33.359028
790.610171	72339.176844	33.364045
791.310581	72483.494649	33.369063
791.943961	72632.181001	33.374080
792.862927	72764.824095	33.379098
793.755594	72882.398291	33.384116
794.408689	73006.835260	33.389133
794.680339	73158.689621	33.394151
795.433396	73293.570148	33.399168
796.263853	73430.323049	33.404186
797.050024	73582.620274	33.409204
798.018735	73737.784493	33.414221
798.776181	73873.888333	33.419239
799.863732	74006.903322	33.424256
800.728254	74161.581937	33.429274
801.575176	74322.916822	33.434292
802.653024	74444.402175	33.439309
803.247883	74574.827200	33.444327
804.324455	74704.028909	33.449344
805.088415	74856.737199	33.454362
805.874894	75010.404041	33.459380
806.895391	75139.560701	33.464397
807.680522	75277.989618	33.469415
808.375970	75388.799438	33.474432
809.176735	75551.276740	33.479450
810.038733	75692.889130	33.484468
810.983531	75817.155033	33.489485
811.820430	75939.479053	33.494503
812.293749	76086.438650	33.499520
813.525384	76225.508163	33.504538
814.132994	76362.626296	33.509556
815.106835	76500.582836	33.514573
815.745317	76655.158473	33.519591
816.235335	76785.645714	33.524608
817.297367	76914.281158	33.529626
817.888641	77069.291241	33.534644
819.027233	77209.590320	33.539661
819.662356	77355.349100	33.544679
820.463361	77490.013834	33.549696
821.526973	77640.484971	33.554714
822.100231	77776.694277	33.559732
822.821263	77910.027689	33.564749
823.851142	78072.397374	33.569767
824.669331	78198.999853	33.574784
825.803712	78334.866981	33.579802
826.237211	78490.020662	33.584820
827.467623	78627.916601	33.589837
828.627696	78755.161539	33.594855
828.865460	78892.331251	33.599872
829.935261	79025.670746	33.604890
830.839541	79175.324831	33.609908
832.168832	79288.073671	33.614925
832.980965	79393.970061	33.619943
833.778939	79523.568826	33.624960
834.453457	79625.118512	33.629978
834.971837	79766.712729	33.634996
836.237800	79892.979000	33.640013
836.865319	80014.500072	33.645031
838.114644	80141.491562	33.650048
838.998780	80249.663512	33.655066
839.471881	80354.652717	33.660084
840.170146	80487.056641	33.665101
841.055584	80637.805303	33.670119
841.371797	80755.302029	33.675136
842.572361	80885.272371	33.680154
843.574475	81025.048922	33.685172
844.361442	81149.788440	33.690189
844.905035	81273.101337	33.695207
845.647351	81414.567832	33.700224
846.719435	81543.671322	33.705242
847.125901	81695.840881	33.710260
847.996598	81849.927382	33.715277
848.901492	81983.444646	33.720295
849.688510	82134.263908	33.725312
850.906483	82258.622140	33.730330
852.069506	82408.103360	33.735348
852.673734	82554.287211	33.740365
853.698123	82674.036568	33.745383
854.202744	82829.702090	33.750400
855.417502	82982.214990	33.755418
855.852969	83128.291249	33.760436
856.543013	83246.839982	33.765453
857.791967	83395.630343	33.770471
858.461398	83537.735821	33.775488
859.583961	83679.406782	33.780506
860.060523	83847.502082	33.785524
860.707111	83990.113929	33.790541
861.779334	84135.193211	33.795559
862.390386	84312.594612	33.800576
863.352094	84458.371113	33.805594
864.341444	84593.673850	33.810612
865.086985	84749.793552	33.815629
865.897388	84922.029734	33.820647
866.729029	85087.405780	33.825664
867.583287	85228.453736	33.830682
868.559915	85374.746068	33.835700
869.045105	85557.055697	33.840717
870.321842	85700.118259	33.845735
871.146910	85876.775207	33.850752
872.095519	86042.005959	33.855770
872.549625	86199.980451	33.860788
873.505405	86338.019552	33.865805
874.323047	86516.023920	33.870823
875.334032	86685.949870	33.875840
876.278281	86848.858811	33.880858
876.815139	87031.753653	33.885876
877.722789	87197.499275	33.890893
878.797821	87341.238030	33.895911
879.603138	87513.772825	33.900928
880.468844	87683.255542	33.905946
881.387783	87843.708041	33.910964
882.160480	88003.363244	33.915981
883.249399	88174.818441	33.920999
884.017481	88352.857742	33.926016
884.988649	88518.969284	33.931034
886.345862	88681.626738	33.936052
886.911680	88836.569863	33.941069
888.101310	89011.868041	33.946087
888.634643	89157.719611	33.951104
889.422120	89307.219145	33.956122
890.144776	89451.111347	33.961140
891.258278	89618.738491	33.966157
892.471377	89762.058058	33.971175
893.101880	89910.043370	33.976192
893.901712	90056.723428	33.981210
894.749978	90238.022645	33.986228
895.459328	90397.951407	33.991245
896.807839	90539.652378	33.996263
897.683990	90703.244880	34.001280
898.474598	90870.510260	34.006298
899.116578	91018.614529	34.011316
900.105517	91191.766213	34.016333
901.288842	91363.001263	34.021351
901.800224	91520.078300	34.026368
902.843639	91680.264316	34.031386
904.094920	91843.112958	34.036404
904.618573	91994.274114	34.041421
905.975810	92159.094530	34.046439
906.453798	92343.559234	34.051456
907.459572	92504.902458	34.056474
908.729897	92681.904219	34.061492
909.384783	92851.870246	34.066509
910.404503	93013.107007	34.071527
910.820917	93185.608255	34.076544
911.922560	93350.934747	34.081562
912.717291	93517.205405	34.086580
913.892648	93699.869291	34.091597
914.969247	93869.203293	34.096615
915.458316	94030.521831	34.101632
916.308923	94217.129201	34.106650
917.427467	94402.586199	34.111668
918.565711	94568.623847	34.116685
919.489490	94723.400623	34.121703
920.320658	94914.978587	34.126720
921.106973	95103.527460	34.131738
922.542983	95272.470166	34.136756
923.087702	95435.092687	34.141773
924.001522	95608.048089	34.146791
925.140345	95804.379886	34.151808
925.919622	95984.081956	34.156826
927.083091	96151.588346	34.161844
927.390685	96335.358433	34.166861
928.852484	96503.463587	34.171879
929.677839	96679.093256	34.176896
930.717197	96872.019406	34.181914
931.831005	97036.615752	34.186932
932.511421	97209.741271	34.191949
933.557247	97374.787856	34.196967
934.672159	97575.568629	34.201984
935.802062	97734.096681	34.207002
936.863807	97889.003641	34.212020
937.789649	98066.639527	34.217037
938.880237	98234.925409	34.222055
939.648723	98415.229383	34.227072
940.760247	98605.188383	34.232090
941.463729	98749.683586	34.237108
942.229661	98914.805649	34.242125
943.522853	99090.641093	34.247143
944.026285	99286.940957	34.252160
945.257540	99465.523946	34.257178
946.185816	99622.805973	34.262196
947.096627	99808.641926	34.267213
947.660735	99985.078826	34.272231
948.305283	100163.301544	34.277248
949.366201	100332.024304	34.282266
950.410801	100500.238116	34.287284
951.114381	100687.938004	34.292301
952.323565	100861.584053	34.297319
953.068570	101040.872622	34.302336
953.560731	101202.452800	34.307354
954.757038	101369.033033	34.312372
955.419835	101558.208545	34.317389
956.706245	101740.894657	34.322407
957.801336	101931.831215	34.327424
958.476054	102083.732223	34.332442
959.689734	102265.408509	34.337460
960.139008	102459.304613	34.342477
961.259771	102649.457278	34.347495
962.478740	102835.498895	34.352512
963.324315	103011.815489	34.357530
964.458042	103179.798139	34.362548
965.192783	103376.503142	34.367565
966.473764	103576.684015	34.372583
967.241821	103758.754746	34.377600
968.151603	103940.429817	34.382618
969.492400	104121.116952	34.387636
970.088834	104330.078169	34.392653
971.379619	104509.940532	34.397671
972.277655	104696.308239	34.402688
973.207192	104888.820129	34.407706
974.398656	105094.966693	34.412724
975.088227	105277.871577	34.417741
976.149921	105451.332597	34.422759
977.075501	105666.392119	34.427776
978.076021	105860.659767	34.432794
979.208515	106058.744234	34.437812
979.713228	106248.670607	34.442829
981.022573	106439.339343	34.447847
981.983921	106652.761112	34.452864
982.782519	106844.884861	34.457882
983.965207	107054.271457	34.462900
985.016070	107270.456981	34.467917
986.522388	107448.296778	34.472935
987.720217	107643.285981	34.477952
988.344932	107840.308954	34.482970
989.709374	108022.330094	34.487988
990.333929	108236.364927	34.493005
991.527052	108411.919929	34.498023
992.776307	108609.301476	34.503040
993.664322	108801.842698	34.508058
994.617028	109001.796505	34.513076
995.291838	109202.494292	34.518093
996.275767	109377.444292	34.523111
997.506973	109568.807190	34.528128
998.422822	109771.571960	34.533146
999.579542	109976.249034	34.538164
1000.209676	110170.438619	34.543181
1001.199065	110357.692695	34.548199
1002.169866	110565.102815	34.553216
1002.978240	110771.376069	34.558234
1004.146631	110969.890400	34.563252
1005.084449	111175.917396	34.568269
1005.941588	111394.195058	34.573287
1007.254378	111596.844764	34.578304
1008.022359	111784.512657	34.583322
1008.931712	112015.668672	34.588340
1010.068166	112225.204896	34.593357
1010.875432	112411.983974	34.598375
1012.121473	112625.077263	34.603392
1012.798068	112848.222578	34.608410
1013.826572	113036.882157	34.613428
1014.889098	113243.917664	34.618445
1015.942865	113474.340198	34.623463
1016.931929	113692.323198	34.628480
1017.762054	113876.841051	34.633498
1018.913315	114080.169299	34.638516
1019.891193	114278.891272	34.643533
1020.813620	114485.629926	34.648551
1022.145589	114707.136709	34.653568
1023.145010	114900.032342	34.658586
1024.130547	115078.375918	34.663604
1024.878512	115288.899160	34.668621
1026.030161	115493.973318	34.673639
1027.012171	115708.641658	34.678656
1028.352264	115904.617150	34.683674
1029.206741	116111.759223	34.688692
1029.786050	116328.728505	34.693709
1030.923677	116536.105699	34.698727
1032.169054	116740.932866	34.703744
1032.920412	116952.557653	34.708762
1033.983392	117180.057640	34.713780
1034.895385	117402.187320	34.718797
1036.254818	117608.826363	34.723815
1036.995968	117821.118182	34.728832
1038.193977	118055.697816	34.733850
1039.223626	118279.550710	34.738868
1040.427242	118500.931407	34.743885
1041.223599	118730.413713	34.748903
1042.397571	118938.436096	34.753920
1043.174825	119176.832092	34.758938
1044.479625	119395.238282	34.763956
1045.412509	119617.179174	34.768973
1046.450224	119851.749430	34.773991
1047.469581	120078.621043	34.779008
1048.363566	120315.904952	34.784026
1049.492362	120565.442542	34.789044
1050.177098	120775.028851	34.794061
1051.401016	121022.172609	34.799079
1052.950121	121259.571556	34.804096
1053.673486	121492.699259	34.809114
1054.692535	121720.040014	34.814132
1055.631403	121970.875548	34.819149
1057.093425	122198.336992	34.824167
1058.437652	122455.445451	34.829184
1059.269719	122693.063202	34.834202
1060.690148	122919.840213	34.839220
1061.559932	123140.754173	34.844237
1062.286926	123376.075894	34.849255
1063.331001	123630.481777	34.854272
1064.488249	123888.026520	34.859290
1065.722392	124115.299720	34.864308
1066.834279	124334.370568	34.869325
1068.086159	124578.751938	34.874343
1069.027178	124824.707338	34.879360
1070.124953	125069.612424	34.884378
1071.741124	125297.224486	34.889396
1072.884612	125519.340311	34.894413
1073.526064	125770.472778	34.899431
1075.205534	125983.645260	34.904448
1076.088392	126227.163294	34.909466
1077.097351	126458.496270	34.914484
1078.152097	126670.598168	34.919501
1079.442957	126892.889960	34.924519
1080.684145	127122.681586	34.929536
1081.823135	127357.738672	34.934554
1082.751085	127575.114707	34.939572
1084.156895	127812.285796	34.944589
1085.386401	128044.760512	34.949607
1086.692372	128251.154172	34.954624
1087.582432	128461.977740	34.959642
1088.713957	128675.703292	34.964660
1089.845224	128900.342838	34.969677
1090.745653	129099.014573	34.974695
1091.973698	129302.906038	34.979712
1092.726373	129498.131986	34.984730
1094.059441	129710.259866	34.989748
1095.398726	129930.233754	34.994765
1096.047879	130144.923723	34.999783
1097.339397	130330.686741	35.004800
1098.299846	130549.358707	35.009818
1099.148444	130764.235527	35.014836
1099.839646	130995.946898	35.019853
1101.023063	131227.946322	35.024871
1101.693293	131434.491643	35.029888
1102.931274	131653.315694	35.034906
1103.801980	131894.586642	35.039924
1105.245005	132104.329777	35.044941
1105.533814	132361.823591	35.049959
1106.469282	132612.900277	35.054976
1108.139311	132848.418611	35.059994
1109.113084	133066.193343	35.065012
1110.180883	133316.810138	35.070029
1110.705860	133585.619950	35.075047
1112.059993	133816.393415	35.080064
1113.156822	134076.011499	35.085082
1114.441748	134340.354291	35.090100
1115.613703	134566.003984	35.095117
1116.407497	134826.857115	35.100135
1118.072848	135077.021515	35.105152
1119.203155	135331.079218	35.110170
1120.615247	135594.105666	35.115188
1122.061484	135846.416588	35.120205
1122.899728	136092.935010	35.125223
1124.140111	136357.669400	35.130240
1124.954956	136600.506493	35.135258
1126.357925	136847.114915	35.140276
1127.418013	137093.414160	35.145293
1128.521754	137351.815122	35.150311
1129.775153	137600.596441	35.155328
1130.868343	137877.740875	35.160346
1132.158001	138128.345813	35.165364
1132.939481	138372.063675	35.170381
1134.015092	138651.410817	35.175399
1135.034566	138897.552819	35.180416
1136.155338	139148.218743	35.185434
1137.621497	139413.599821	35.190452
1138.870754	139679.614711	35.195469
1139.757483	139951.130667	35.200487
1140.850667	140193.986361	35.205504
1142.005737	140452.859531	35.210522
1143.193117	140730.278514	35.215540
1145.065027	141004.176158	35.220557
1146.369085	141248.969920	35.225575
1147.888633	141483.371038	35.230592
1149.050315	141718.593608	35.235610
1150.372131	141983.321496	35.240628
1151.544747	142226.964856	35.245645
1152.486397	142475.745246	35.250663
1153.804953	142701.324987	35.255680
1155.113400	142953.636639	35.260698
1156.025864	143202.135505	35.265716
1157.159422	143452.146620	35.270733
1157.957516	143706.551472	35.275751
1159.234836	143947.260729	35.280768
1159.973525	144189.290547	35.285786
1161.194369	144444.734230	35.290804
1162.328822	144695.058527	35.295821
1163.125296	144959.591756	35.300839
1164.519013	145232.917450	35.305856
1165.485659	145486.419903	35.310874
1166.422955	145720.197879	35.315892
1167.742249	145962.676777	35.320909
1168.381849	146227.549830	35.325927
1169.799544	146467.834860	35.330944
1170.905232	146720.600456	35.335962
1172.255362	146976.776781	35.340980
1173.330681	147235.777512	35.345997
1174.187470	147490.973760	35.351015
1175.434275	147745.638248	35.356032
1176.520524	148023.030961	35.361050
1177.275671	148284.501649	35.366068
1178.761243	148549.696234	35.371085
1179.543453	148841.856243	35.376103
1180.704457	149112.625137	35.381120
1182.030401	149376.939066	35.386138
1183.222154	149648.505864	35.391156
1184.712114	149924.806655	35.396173
1185.783843	150215.484194	35.401191
1186.955919	150481.036372	35.406208
1188.096493	150776.754601	35.411226
1189.214058	151056.701886	35.416244
1190.345760	151319.096158	35.421261
1192.211166	151615.348312	35.426279
1193.416168	151887.525628	35.431296
1194.677117	152170.552320	35.436314
1195.837293	152448.790926	35.441332
1197.376149	152736.620984	35.446349
1198.263663	153009.239413	35.451367
1199.475889	153297.444786	35.456384
1200.535408	153557.114490	35.461402
1201.547776	153842.642782	35.466420
1203.139208	154153.178549	35.471437
1204.123017	154444.119329	35.476455
1205.079406	154711.031031	35.481472
1206.347310	154996.690739	35.486490
1207.605323	155306.986566	35.491508
1208.857549	155609.852976	35.496525
1209.992772	155905.295459	35.501543
1211.120334	156193.815845	35.506560
1212.328278	156495.669115	35.511578
1213.685451	156795.254953	35.516596
1215.045030	157075.080108	35.521613
1216.038474	157376.366780	35.526631
1217.186420	157666.112490	35.531648
1218.690679	157970.998026	35.536666
1219.543473	158291.469144	35.541684
1221.066459	158577.252709	35.546701
1222.130888	158898.708642	35.551719
1223.434261	159182.655429	35.556736
1224.956549	159481.042119	35.561754
1226.069967	159796.484375	35.566772
1227.504829	160098.277138	35.571789
1228.648582	160399.904570	35.576807
1229.930755	160690.614357	35.581824
1231.339500	161001.932540	35.586842
1232.236607	161293.610925	35.591860
1233.749491	161580.140733	35.596877
1234.754745	161896.911269	35.601895
1235.914835	162202.786613	35.606912
1237.200809	162487.761791	35.611930
1238.275580	162789.012406	35.616948
1239.909337	163094.841598	35.621965
1240.828404	163415.405977	35.626983
1241.960422	163709.777730	35.632000
1243.340691	164012.559991	35.637018
1244.275937	164346.310453	35.642036
1245.333979	164639.432297	35.647053
1246.388117	164946.994711	35.652071
1247.633182	165262.711079	35.657088
1248.974778	165569.012622	35.662106
1249.992611	165861.286872	35.667124
1251.102964	166146.607842	35.672141
1252.070621	166464.180559	35.677159
1253.676634	166778.008931	35.682176
1254.842252	167091.100275	35.687194
1255.877794	167420.049739	35.692212
1257.518708	167739.284369	35.697229
1258.477843	168055.068556	35.702247
1259.665548	168371.299459	35.707264
1261.184494	168692.388306	35.712282
1262.430927	168999.656218	35.717300
1263.829184	169316.379420	35.722317
1265.024114	169652.653288	35.727335
1266.063568	169989.856260	35.732352
1267.454375	170308.288063	35.737370
1268.445834	170623.958469	35.742388
1269.752969	170948.981416	35.747405
1270.890977	171289.667371	35.752423
1272.204677	171630.961358	35.757440
1273.162587	171975.032112	35.762458
1274.397034	172313.806505	35.767476
1275.944516	172644.435984	35.772493
1277.369299	173005.834494	35.777511
1278.597473	173345.899199	35.782528
1280.089620	173679.324267	35.787546
1281.417455	174033.716818	35.792564
1282.886314	174361.592563	35.797581
1284.222115	174702.030152	35.802599
1285.354076	175060.587042	35.807616
1287.137923	175378.405554	35.812634
1288.314884	175715.323494	35.817652
1289.716984	176070.328310	35.822669
1291.157599	176418.083249	35.827687
1292.691295	176749.568949	35.832704
1293.847705	177058.022520	35.837722
1295.610927	177421.632682	35.842740
1296.963042	177744.373325	35.847757
1298.256455	178069.727409	35.852775
1299.782359	178416.835467	35.857792
1301.293674	178732.576426	35.862810
1302.582021	179049.282659	35.867828
1303.769568	179375.030929	35.872845
1305.116457	179710.311501	35.877863
1306.076774	180063.248226	35.882880
1307.617926	180384.896248	35.887898
1308.770019	180709.326513	35.892916
1309.826575	181060.198371	35.897933
1310.935209	181403.512567	35.902951
1312.120700	181735.546184	35.907968
1313.608650	182069.385048	35.912986
1314.724491	182426.653208	35.918004
1316.123741	182768.646747	35.923021
1317.540605	183097.630322	35.928039
1318.431564	183461.085700	35.933056
1319.670509	183818.838155	35.938074
1321.038021	184170.276467	35.943092
1322.283275	184502.762222	35.948109
1323.863681	184855.756521	35.953127
1324.865932	185223.305386	35.958144
1326.256842	185590.792645	35.963162
1327.530834	185950.508400	35.968180
1328.630349	186288.753771	35.973197
1329.950921	186641.358491	35.978215
1330.977617	187034.733010	35.983232
1332.728185	187405.397270	35.988250
1334.044028	187741.610471	35.993268
1334.919834	188087.316705	35.998285
1336.623560	188433.421579	36.003303
1337.763985	188790.867896	36.008320
1339.047220	189149.206859	36.013338
1340.553778	189489.054868	36.018356
1342.014245	189814.759170	36.023373
1343.582960	190188.112229	36.028391
1344.683232	190550.285679	36.033408
1346.022007	190876.079605	36.038426
1347.201290	191221.983460	36.043444
1348.746596	191600.604855	36.048461
1350.680445	191960.605862	36.053479
1351.748574	192313.681324	36.058496
1353.177342	192662.167554	36.063514
1354.541231	193018.981316	36.068532
1355.970042	193388.861717	36.073549
1357.828426	193723.497194	36.078567
1358.614631	194090.631739	36.083584
1360.370498	194460.236278	36.088602
1361.745247	194809.467539	36.093620
1363.114730	195142.350837	36.098637
1364.388621	195509.235750	36.103655
1365.721592	195857.984791	36.108672
1367.003232	196228.236847	36.113690
1368.353766	196606.426835	36.118708
1369.808968	196965.838449	36.123725
1371.034165	197308.240435	36.128743
1372.262208	197673.469879	36.133760
1373.477037	198058.216330	36.138778
1375.090973	198441.566211	36.143796
1375.897041	198816.431462	36.148813
1377.507249	199176.705934	36.153831
1378.792690	199572.558368	36.158848
1380.096423	199933.484285	36.163866
1381.704869	200346.935105	36.168884
1383.261266	200710.045324	36.173901
1384.860388	201069.367084	36.178919
1385.988143	201464.787079	36.183936
1387.374690	201850.758894	36.188954
1388.666963	202234.361581	36.193972
1390.192577	202624.504546	36.198989
1392.099647	203011.057202	36.204007
1393.484834	203370.896146	36.209024
1394.874728	203745.045024	36.214042
1396.483384	204147.599917	36.219060
1397.425394	204539.957509	36.224077
1398.991484	204897.260469	36.229095
1400.480162	205276.149653	36.234112
1401.941609	205666.383520	36.239130
1403.512393	206041.047834	36.244148
1404.875522	206433.244644	36.249165
1406.169154	206828.718127	36.254183
1407.711018	207210.782789	36.259200
1409.192977	207572.874081	36.264218
1410.546236	207958.693923	36.269236
1411.829655	208361.770070	36.274253
1413.575532	208729.714844	36.279271
1414.532179	209115.732958	36.284288
1415.850332	209508.727698	36.289306
1417.559113	209869.332214	36.294324
1418.920932	210252.724204	36.299341
1420.411350	210661.072980	36.304359
1421.450218	211050.413793	36.309376
1422.871339	211426.056070	36.314394
1424.436553	211829.954243	36.319412
1425.823710	212206.177128	36.324429
1427.574895	212587.255744	36.329447
1428.638148	212994.086793	36.334464
1430.280517	213344.457799	36.339482
1431.572851	213733.845671	36.344500
1432.696759	214113.383986	36.349517
1434.402287	214477.793368	36.354535
1435.854209	214840.544579	36.359552
1436.951906	215207.114448	36.364570
1438.468221	215644.473490	36.369588
1439.767869	216069.857759	36.374605
1441.571595	216432.024140	36.379623
1442.154068	216832.641413	36.384640
1443.758900	217221.485256	36.389658
1445.157576	217600.104289	36.394676
1446.130827	218004.319404	36.399693
1447.515042	218425.713327	36.404711
1448.852173	218825.122613	36.409728
1450.183365	219223.340869	36.414746
1452.138664	219649.903303	36.419764
1453.304634	220056.127170	36.424781
1455.123562	220457.851122	36.429799
1456.262866	220887.855351	36.434816
1457.828121	221295.313730	36.439834
1459.540589	221719.004382	36.444852
1460.297144	222133.101546	36.449869
1462.130330	222570.338556	36.454887
1463.275131	222997.480751	36.459904
1464.426250	223438.669134	36.464922
1466.135097	223874.814540	36.469940
1467.656758	224323.819067	36.474957
1469.831204	224721.005284	36.479975
1471.226361	225163.684373	36.484992
1473.033871	225605.433603	36.490010
1474.346580	226013.180314	36.495028
1475.993428	226468.548057	36.500045
1477.552083	226902.367954	36.505063
1478.593273	227341.075375	36.510080
1480.175308	227751.018907	36.515098
1482.077400	228199.391714	36.520116
1483.161323	228632.280254	36.525133
1484.573707	229068.062513	36.530151
1486.105278	229536.922915	36.535168
1487.627772	229969.261122	36.540186
1488.997638	230408.738040	36.545204
1490.466966	230867.275679	36.550221
1492.060899	231303.162579	36.555239
1493.154746	231740.454244	36.560256
1494.348703	232211.665974	36.565274
1496.432143	232654.131388	36.570292
1497.606697	233114.173089	36.575309
1499.380436	233580.620017	36.580327
1501.065323	234025.771749	36.585344
1502.350260	234461.440054	36.590362
1504.269565	234916.512967	36.595380
1505.990445	235391.559880	36.600397
1507.299022	235837.896711	36.605415
1508.948168	236299.673396	36.610432
1510.233964	236766.337626	36.615450
1511.936051	237207.279059	36.620468
1513.114745	237649.933723	36.625485
1514.871695	238110.326026	36.630503
1516.076447	238582.317614	36.635520
1517.436560	239035.233560	36.640538
1519.350333	239509.117354	36.645556
1520.603293	239953.061053	36.650573
1522.044691	240423.545085	36.655591
1523.399496	240876.136193	36.660608
1524.803924	241355.163651	36.665626
1526.665526	241839.298844	36.670644
1528.294656	242293.067199	36.675661
1529.963840	242719.141556	36.680679
1531.208001	243162.662016	36.685696
1532.633125	243621.064652	36.690714
1534.338082	244069.667557	36.695732
1535.538870	244525.213168	36.700749
1537.219532	244973.720212	36.705767
1538.260795	245426.524996	36.710784
1539.689793	245865.904901	36.715802
1541.396518	246330.134246	36.720820
1542.304908	246804.707983	36.725837
1544.075728	247283.204669	36.730855
1545.775839	247759.554609	36.735872
1547.310993	248243.019911	36.740890
1548.903479	248701.759631	36.745908
1550.335697	249188.418759	36.750925
1551.890037	249660.197801	36.755943
1553.367764	250150.610462	36.760960
1554.548495	250635.585784	36.765978
1556.478317	251116.373678	36.770996
1557.894804	251622.294220	36.776013
1559.434582	252124.486219	36.781031
1560.752419	252606.291388	36.786048
1562.497995	253098.619585	36.791066
1564.332034	253594.159897	36.796084
1566.193955	254104.683946	36.801101
1567.702559	254596.468456	36.806119
1569.202758	255106.367240	36.811136
1570.923714	255585.898620	36.816154
1572.869346	256090.898099	36.821172
1574.405182	256604.450228	36.826189
1575.912614	257087.498091	36.831207
1577.587208	257609.588846	36.836224
1578.945277	258109.834492	36.841242
1580.711438	258590.782752	36.846260
1582.748077	259103.389868	36.851277
1584.755561	259612.115266	36.856295
1586.531806	260093.494201	36.861312
1587.742017	260589.040057	36.866330
1589.659328	261087.212877	36.871348
1590.746826	261576.555288	36.876365
1592.609857	262081.850050	36.881383
1594.189774	262576.242683	36.886400
1595.629915	263062.529276	36.891418
1597.382837	263570.077559	36.896436
1598.822009	264091.192050	36.901453
1600.221920	264584.293045	36.906471
1601.934691	265084.201141	36.911488
1603.549782	265598.960661	36.916506
1605.465277	266084.304213	36.921524
1607.267817	266581.427856	36.926541
1608.980640	267097.415204	36.931559
1610.541992	267599.963503	36.936576
1611.929298	268100.533308	36.941594
1613.809758	268611.919322	36.946612
1615.211668	269116.194767	36.951629
1616.478430	269610.813468	36.956647
1618.532274	270117.215895	36.961664
1620.145468	270643.301672	36.966682
1621.717243	271146.327727	36.971700
1623.412237	271633.278173	36.976717
1624.856363	272149.000209	36.981735
1626.662933	272646.828908	36.986752
1628.146916	273143.897280	36.991770
1629.768358	273655.802970	36.996788
1632.475531	274153.328585	37.001805
1634.100373	274652.073538	37.006823
1636.315213	275112.387607	37.011840
1637.721261	275600.523391	37.016858
1639.260966	276079.008706	37.021876
1640.889849	276556.614819	37.026893
1642.242319	277007.745409	37.031911
1643.844187	277468.639480	37.036928
1645.043748	277948.803404	37.041946
1646.551873	278406.459741	37.046964
1648.377956	278884.308487	37.051981
1649.559057	279382.355952	37.056999
1651.221629	279867.367745	37.062016
1652.498116	280345.354972	37.067034
1654.144690	280829.503640	37.072052
1655.869733	281336.525588	37.077069
1656.863698	281830.940491	37.082087
1658.821288	282334.543152	37.087104
1660.294775	282865.556889	37.092122
1662.063399	283366.698694	37.097140
1663.598975	283871.230661	37.102157
1664.666412	284391.663764	37.107175
1666.691176	284912.521669	37.112192
1667.980342	285455.192345	37.117210
1669.945360	285995.006455	37.122228
1671.592886	286532.585094	37.127245
1673.133748	287065.048514	37.132263
1675.069613	287602.322054	37.137280
1676.529967	288133.728352	37.142298
1677.798350	288671.387765	37.147316
1679.718375	289237.717077	37.152333
1681.008431	289800.515843	37.157351
1682.692055	290352.147370	37.162368
1684.382331	290907.128565	37.167386
1686.171569	291483.859535	37.172404
1687.746570	292028.695044	37.177421
1689.692210	292608.189513	37.182439
1691.480773	293174.296032	37.187456
1692.941277	293764.381146	37.192474
1694.858809	294317.558105	37.197492
1697.019520	294869.219317	37.202509
1698.565916	295439.318068	37.207527
1700.706009	296017.367898	37.212544
1702.425485	296585.400699	37.217562
1703.997496	297140.399776	37.222580
1705.190425	297716.032168	37.227597
1706.766703	298294.824101	37.232615
1709.057306	298887.667865	37.237632
1710.446296	299476.110778	37.242650
1712.551637	300040.227295	37.247668
1714.229621	300610.735598	37.252685
1715.458177	301204.224394	37.257703
1717.410833	301765.258243	37.262720
1719.135235	302373.973701	37.267738
1721.376971	302960.986398	37.272756
1723.390499	303527.257788	37.277773
1724.603797	304097.061219	37.282791
1726.441097	304694.441733	37.287808
1727.834296	305274.189750	37.292826
1729.603284	305860.069136	37.297844
1731.564933	306448.122586	37.302861
1732.922170	307046.684720	37.307879
1734.780819	307628.068132	37.312896
1736.501624	308216.505358	37.317914
1738.217660	308811.136171	37.322932
1740.289419	309394.885421	37.327949
1742.099446	310009.530136	37.332967
1743.847866	310600.587757	37.337984
1745.594518	311176.861177	37.343002
1747.426757	311739.098115	37.348020
1748.995294	312323.087746	37.353037
1750.674612	312919.396951	37.358055
1752.943603	313492.571159	37.363072
1754.106360	314050.813777	37.368090
1756.021968	314600.801926	37.373108
1758.052788	315165.038852	37.378125
1759.554565	315741.116441	37.383143
1761.226304	316306.648462	37.388160
1762.991257	316871.272052	37.393178
1764.677448	317427.524416	37.398196
1766.718812	318005.603176	37.403213
1768.289465	318595.080396	37.408231
1769.957851	319154.852143	37.413248
1771.682437	319746.097400	37.418266
1773.357052	320314.568714	37.423284
1775.283564	320880.200673	37.428301
1776.819534	321476.870980	37.433319
1778.734758	322062.123286	37.438336
1780.659585	322638.126333	37.443354
1782.339641	323257.381298	37.448372
1784.104576	323846.959397	37.453389
1785.773697	324440.509036	37.458407
1788.163320	325027.408957	37.463424
1789.976631	325610.818529	37.468442
1792.009363	326227.930460	37.473460
1793.783404	326800.773195	37.478477
1795.478492	327400.283177	37.483495
1796.962748	328003.046655	37.488512
1798.795340	328614.836204	37.493530
1800.372724	329211.605936	37.498548
1802.687842	329825.080960	37.503565
1804.287420	330429.502434	37.508583
1806.024209	331019.906112	37.513600
1808.084331	331645.514703	37.518618
1809.660183	332268.302263	37.523636
1812.112305	332881.316677	37.528653
1813.667005	333475.863656	37.533671
1815.934832	334078.436048	37.538688
1817.700814	334686.872984	37.543706
1819.459443	335308.302425	37.548724
1821.395715	335916.139356	37.553741
1823.300043	336519.786162	37.558759
1824.984844	337127.397291	37.563776
1826.852402	337750.710403	37.568794
1828.422475	338359.088149	37.573812
1830.599990	338980.660392	37.578829
1831.968932	339602.866394	37.583847
1833.568957	340209.009466	37.588864
1835.491361	340831.820298	37.593882
1837.323066	341466.188113	37.598900
1839.130625	342101.389704	37.603917
1840.959837	342726.477364	37.608935
1843.058972	343365.320909	37.613952
1845.019891	343986.386089	37.618970
1846.409105	344602.359873	37.623988
1848.441438	345230.783809	37.629005
1849.871962	345888.182912	37.634023
1851.869566	346535.936314	37.639040
1853.746009	347168.269543	37.644058
1855.515139	347790.637637	37.649076
1857.485085	348443.953411	37.654093
1858.765331	349094.328330	37.659111
1861.130958	349734.490351	37.664128
1862.972273	350382.166045	37.669146
1864.419295	351043.221416	37.674164
1866.413701	351684.686479	37.679181
1868.103951	352350.656880	37.684199
1870.297172	353012.677097	37.689216
1871.985081	353663.934847	37.694234
1873.606223	354290.730899	37.699252
1875.314249	354941.129099	37.704269
1876.845695	355596.215944	37.709287
1878.364916	356245.788432	37.714304
1880.604229	356870.339287	37.719322
1882.080146	357524.517907	37.724340
1883.975364	358185.671413	37.729357
1885.609792	358857.819186	37.734375
1887.692505	359491.314332	37.739392
1889.730483	360174.335821	37.744410
1891.361526	360832.903029	37.749428
1892.773984	361504.816274	37.754445
1894.661402	362196.506406	37.759463
1896.339566	362875.432007	37.764480
1898.616211	363545.189969	37.769498
1900.225775	364256.527851	37.774516
1902.180918	364942.755591	37.779533
1903.777032	365638.138391	37.784551
1905.688703	366344.593965	37.789568
1907.797663	367073.430276	37.794586
1909.654557	367796.485080	37.799604
1911.622595	368487.519006	37.804621
1913.473258	369215.063562	37.809639
1915.713763	369944.204082	37.814656
1917.391617	370652.039359	37.819674
1919.042505	371372.700891	37.824692
1921.427732	372102.181355	37.829709
1923.387970	372852.466059	37.834727
1925.036413	373564.258221	37.839744
1926.957755	374300.290160	37.844762
1929.070717	375052.457408	37.849780
1931.066359	375765.544017	37.854797
1932.970076	376534.961461	37.859815
1934.923194	377281.883490	37.864832
1937.050901	378010.348586	37.869850
1939.175768	378752.367029	37.874868
1940.905513	379503.691316	37.879885
1942.847518	380267.568040	37.884903
1944.911548	381028.592799	37.889920
1946.788945	381761.914479	37.894938
1948.520099	382520.475653	37.899956
1950.747611	383282.411866	37.904973
1952.757602	384034.401389	37.909991
1954.630618	384788.627875	37.915008
1956.847416	385560.554813	37.920026
1958.299486	386321.560295	37.925044
1960.543759	387070.475430	37.930061
1962.930110	387831.367624	37.935079
1964.080432	388606.567543	37.940096
1966.379115	389374.739465	37.945114
1968.622086	390159.938672	37.950132
1970.422337	390927.014456	37.955149
1972.635134	391697.856853	37.960167
1974.298571	392466.134462	37.965184
1976.541084	393235.590436	37.970202
1978.640525	394007.864610	37.975220
1981.070633	394779.279065	37.980237
1983.256819	395532.033051	37.985255
1985.008090	396288.008517	37.990272
1987.386362	397082.514944	37.995290
1989.248165	397845.403387	38.000308
1991.434132	398582.290852	38.005325
1993.279744	399340.758991	38.010343
1995.360177	400104.668551	38.015360
1997.314359	400879.730067	38.020378
1999.454296	401647.036286	38.025396
2001.208100	402383.646307	38.030413
2003.426751	403152.800328	38.035431
2005.152959	403908.432491	38.040448
2007.530126	404632.211864	38.045466
2009.190502	405363.844834	38.050484
2011.663624	406106.017716	38.055501
2013.329951	406827.755083	38.060519
2014.932574	407557.516266	38.065536
2017.011356	408288.015924	38.070554
2018.890298	409053.087421	38.075572
2020.668213	409815.266158	38.080589
2022.384007	410551.516830	38.085607
2024.370242	411295.961864	38.090624
2026.330531	412080.011689	38.095642
2027.521302	412843.823830	38.100660
2029.692336	413618.421198	38.105677
2031.568530	414423.644421	38.110695
2033.189979	415203.808516	38.115712
2035.966799	415979.579737	38.120730
2037.220212	416801.525367	38.125748
2039.242098	417609.616160	38.130765
2041.357571	418412.702369	38.135783
2043.579113	419214.555872	38.140800
2046.016232	420028.707683	38.145818
2047.599953	420842.214655	38.150836
2049.594277	421684.345137	38.155853
2051.843849	422491.991724	38.160871
2053.524438	423341.538449	38.165888
2055.602017	424167.872676	38.170906
2057.645260	425015.530346	38.175924
2059.410633	425864.141759	38.180941
2061.636273	426720.522249	38.185959
2063.452009	427572.282052	38.190976
2065.587428	428418.946742	38.195994
2067.577333	429284.795511	38.201012
2070.117376	430150.421334	38.206029
2072.409172	430993.983016	38.211047
2074.222253	431865.286689	38.216064
2076.581616	432715.914798	38.221082
2078.425211	433599.299841	38.226100
2080.481935	434480.186862	38.231117
2082.776143	435354.876759	38.236135
2084.688474	436236.733889	38.241152
2086.943691	437133.078184	38.246170
2089.174054	437999.884286	38.251188
2091.451129	438870.344642	38.256205
2093.841655	439745.814117	38.261223
2095.752208	440628.869591	38.266240
2098.110226	441488.639529	38.271258
2100.241235	442373.462877	38.276276
2102.520401	443249.877632	38.281293
2104.737109	444110.683598	38.286311
2106.746276	444985.758959	38.291328
2109.175141	445863.361438	38.296346
2111.268262	446750.900605	38.301364
2113.353069	447612.249337	38.306381
2115.852331	448483.208858	38.311399
2118.019722	449360.157441	38.316416
2120.017616	450236.187797	38.321434
2122.256463	451115.632938	38.326452
2124.226123	451962.511925	38.331469
2126.380982	452818.784997	38.336487
2128.437520	453699.063844	38.341504
2131.066364	454583.915039	38.346522
2133.264667	455452.009691	38.351540
2135.338326	456302.894714	38.356557
2137.707482	457160.775822	38.361575
2139.253804	458049.653300	38.366592
2141.522066	458906.568321	38.371610
2143.566907	459778.400290	38.376628
2145.308529	460650.902321	38.381645
2147.233652	461503.821234	38.386663
2149.061928	462345.041746	38.391680
2151.557079	463206.389269	38.396698
2153.364366	464075.395983	38.401716
2155.504501	464926.112209	38.406733
2157.772163	465782.230127	38.411751
2159.366101	466646.660980	38.416768
2161.541055	467495.037129	38.421786
2163.537520	468378.986685	38.426804
2165.579867	469261.170404	38.431821
2168.139917	470158.894941	38.436839
2170.141769	471028.472129	38.441856
2172.038417	471918.543236	38.446874
2174.158047	472829.606944	38.451892
2176.234778	473735.278512	38.456909
2178.593234	474628.381075	38.461927
2180.702683	475522.088891	38.466944
2182.691469	476441.286601	38.471962
2185.196385	477351.109662	38.476980
2187.244239	478280.310885	38.481997
2189.658380	479197.484565	38.487015
2191.799146	480110.465696	38.492032
2193.855705	481023.668124	38.497050
2196.319753	481954.636578	38.502068
2198.444098	482898.744179	38.507085
2200.818783	483827.561371	38.512103
2202.974278	484765.406072	38.517120
2205.255307	485700.505237	38.522138
2207.649656	486647.655048	38.527156
2209.827079	487586.813363	38.532173
2212.187089	488535.383504	38.537191
2214.290153	489482.279421	38.542208
2216.427236	490413.571033	38.547226
2219.228938	491378.675432	38.552244
2221.081683	492340.551842	38.557261
2223.784333	493256.759574	38.562279
2225.833013	494195.940114	38.567296
2228.348587	495154.422502	38.572314
2230.687001	496126.657516	38.577332
2232.724953	497087.936960	38.582349
2234.775634	498020.853119	38.587367
2236.907508	498971.767912	38.592384
2239.537098	499926.381739	38.597402
2241.709505	500884.800736	38.602420
2243.840434	501837.017429	38.607437
2246.092311	502799.955106	38.612455
2248.506227	503769.720930	38.617472
2250.638840	504722.327518	38.622490
2253.497140	505687.267582	38.627508
2255.813163	506647.550334	38.632525
2258.045264	507592.863611	38.637543
2260.053888	508574.264459	38.642560
2262.215814	509547.210584	38.647578
2264.449136	510500.321739	38.652596
2266.834998	511452.292724	38.657613
2269.007704	512424.458718	38.662631
2271.582136	513404.615714	38.667648
2273.647701	514371.740655	38.672666
2276.014615	515339.361922	38.677684
2277.972837	516316.366221	38.682701
2280.243490	517286.303411	38.687719
2282.642660	518262.257407	38.692736
2284.705876	519240.120826	38.697754
2286.724370	520232.845549	38.702772
2288.897083	521223.365123	38.707789
2290.900792	522194.300462	38.712807
2293.148340	523193.246346	38.717824
2295.614806	524197.582110	38.722842
2298.028911	525153.250252	38.727860
2299.851146	526116.461116	38.732877
2301.918753	527069.396203	38.737895
2303.977046	528058.333154	38.742912
2306.036140	529038.190461	38.747930
2308.448100	530017.573032	38.752948
2310.095481	531003.059872	38.757965
2312.935503	531999.613639	38.762983
2314.774044	533013.383461	38.768000
2317.097228	534012.555162	38.773018
2319.430273	535006.724000	38.778036
2321.349715	536027.722990	38.783053
2323.689102	537069.268187	38.788071
2326.053117	538087.482469	38.793088
2328.298271	539120.390222	38.798106
2330.726686	540152.539584	38.803124
2333.102252	541203.291701	38.808141
2335.618942	542256.811332	38.813159
2338.080419	543307.444757	38.818176
2340.833995	544352.267522	38.823194
2343.062858	545390.157670	38.828212
2345.354708	546443.252172	38.833229
2347.484818	547487.492468	38.838247
2350.352346	548552.102794	38.843264
2352.641459	549622.912563	38.848282
2355.562062	550673.622816	38.853300
2357.386551	551736.149310	38.858317
2359.860850	552797.179460	38.863335
2362.639533	553866.774555	38.868352
2364.658312	554942.996413	38.873370
2366.818793	555997.596316	38.878388
2369.189773	557076.657195	38.883405
2371.627283	558157.731674	38.888423
2373.684630	559251.495962	38.893440
2376.009308	560343.167193	38.898458
2378.360048	561428.916443	38.903476
2380.857664	562546.405406	38.908493
2383.250068	563640.055605	38.913511
2385.806352	564752.475459	38.918528
2387.903316	565852.319887	38.923546
2390.551088	566932.594733	38.928564
2393.473675	568060.845168	38.933581
2396.001286	569165.913542	38.938599
2398.505314	570255.175430	38.943616
2401.010523	571355.189766	38.948634
2403.867920	572453.294768	38.953652
2405.639781	573570.760562	38.958669
2408.406561	574677.674728	38.963687
2410.464907	575779.389540	38.968704
2412.786950	576881.868314	38.973722
2415.562354	577981.315668	38.978740
2418.086695	579092.399215	38.983757
2420.656311	580192.589763	38.988775
2422.839948	581310.054558	38.993792
2425.137403	582443.050825	38.998810
2427.527716	583541.770451	39.003828
2429.599739	584662.161175	39.008845
2431.887707	585772.033312	39.013863
2434.437864	586911.246526	39.018880
2436.522826	588049.627794	39.023898
2439.076608	589186.421369	39.028916
2441.413154	590322.542455	39.033933
2443.779428	591448.175655	39.038951
2446.247258	592584.161952	39.043968
2448.205690	593733.455328	39.048986
2450.885921	594884.172691	39.054004
2452.906413	596061.794469	39.059021
2455.116566	597203.044675	39.064039
2457.531938	598339.892475	39.069056
2459.514412	599470.891080	39.074074
2462.455287	600586.195758	39.079092
2464.555510	601725.922418	39.084109
2466.774118	602870.425460	39.089127
2469.266757	604029.341304	39.094144
2471.535077	605178.815290	39.099162
2474.064271	606317.318044	39.104180
2476.267021	607482.742338	39.109197
2478.560719	608668.954451	39.114215
2481.293418	609830.647925	39.119232
2483.369682	611025.207890	39.124250
2485.593840	612214.513539	39.129268
2488.054016	613402.854185	39.134285
2490.545740	614611.974428	39.139303
2492.937419	615827.833122	39.144320
2494.943520	617037.720928	39.149338
2498.060424	618262.246436	39.154356
2500.854244	619499.490439	39.159373
2502.989046	620711.855150	39.164391
2505.452603	621926.431383	39.169408
2507.714424	623183.094756	39.174426
2510.602669	624441.859015	39.179444
2513.294344	625689.715057	39.184461
2515.717602	626931.524983	39.189479
2518.657249	628170.858288	39.194496
2520.957550	629437.181013	39.199514
2523.705080	630678.204268	39.204532
2526.141945	631936.515390	39.209549
2528.589595	633220.194918	39.214567
2531.502906	634480.822100	39.219584
2534.301761	635743.763797	39.224602
2536.742948	636989.888658	39.229620
2539.121325	638264.527226	39.234637
2542.083414	639542.207755	39.239655
2544.835994	640815.723411	39.244672
2547.438472	642096.292297	39.249690
2549.993744	643369.425767	39.254708
2552.375227	644624.571198	39.259725
2554.937352	645898.836128	39.264743
2558.002831	647175.851234	39.269760
2560.286508	648460.214938	39.274778
2562.875935	649735.191072	39.279796
2565.367661	651028.517931	39.284813
2567.769837	652303.698261	39.289831
2570.613224	653583.976518	39.294848
2573.081360	654873.620959	39.299866
2575.852741	656193.044647	39.304884
2577.998987	657485.143391	39.309901
2580.309645	658763.147591	39.314919
2583.380807	660047.983048	39.319936
2585.673685	661370.926583	39.324954
2588.478903	662681.207557	39.329972
2590.796667	663972.771632	39.334989
2593.468318	665278.691447	39.340007
2596.043427	666589.030009	39.345024
2598.409106	667901.265297	39.350042
2601.258683	669221.153442	39.355060
2603.942402	670552.280481	39.360077
2606.154040	671873.399622	39.365095
2608.982132	673186.274849	39.370112
2611.469521	674524.089760	39.375130
2614.095054	675840.359383	39.380148
2616.825318	677178.751375	39.385165
2619.005565	678489.501974	39.390183
2621.633328	679827.630864	39.395200
2624.167957	681176.168176	39.400218
2626.731319	682494.391690	39.405236
2629.559802	683792.559328	39.410253
2632.270511	685098.759865	39.415271
2635.249295	686387.097266	39.420288
2637.592244	687661.501796	39.425306
2640.212766	688984.692659	39.430324
2642.918727	690290.051245	39.435341
2645.465093	691571.469417	39.440359
2648.178281	692844.835668	39.445376
2650.912075	694174.295517	39.450394
2653.542906	695492.559319	39.455412
2656.250332	696805.753716	39.460429
2658.629584	698111.119474	39.465447
2661.289528	699416.197145	39.470464
2663.985833	700746.367235	39.475482
2666.405152	702068.944560	39.480500
2669.115058	703413.881105	39.485517
2671.457365	704760.257569	39.490535
2674.391436	706095.524410	39.495552
2676.774362	707469.872824	39.500570
2679.183610	708828.094922	39.505588
2681.764836	710177.802208	39.510605
2684.296668	711569.851087	39.515623
2687.136273	712946.123086	39.520640
2689.820717	714322.149310	39.525658
2692.982959	715698.369327	39.530676
2695.717286	717093.245261	39.535693
2698.405659	718489.581156	39.540711
2701.510802	719868.348245	39.545728
2704.207526	721274.462646	39.550746
2706.868517	722669.464550	39.555764
2709.856435	724047.314795	39.560781
2712.459959	725428.560081	39.565799
2715.580530	726828.968731	39.570816
2718.297705	728248.088650	39.575834
2721.303373	729632.913780	39.580852
2724.327723	731006.581383	39.585869
2726.811325	732425.856473	39.590887
2729.923143	733819.687095	39.595904
2732.406980	735225.827585	39.600922
2735.023594	736635.257024	39.605940
2737.755645	738039.385121	39.610957
2740.370578	739444.422391	39.615975
2743.114784	740855.805142	39.620992
2745.446821	742271.644562	39.626010
2748.295956	743680.782335	39.631028
2750.978963	745096.948033	39.636045
2753.921132	746549.953768	39.641063
2756.457948	747980.667613	39.646080
2759.230816	749411.377450	39.651098
2761.883965	750826.959282	39.656116
2764.570417	752272.488457	39.661133
2767.029861	753741.486226	39.666151
2770.319897	755180.116140	39.671168
2772.998255	756633.847368	39.676186
2775.723142	758067.154842	39.681204
2778.632800	759526.455658	39.686221
2781.205609	760987.256038	39.691239
2784.134694	762461.153512	39.696256
2786.520717	763909.364744	39.701274
2789.244342	765360.194806	39.706292
2791.944755	766840.459040	39.711309
2794.346075	768313.153183	39.716327
2796.824270	769777.530368	39.721344
2799.433325	771285.841659	39.726362
2802.177120	772790.679185	39.731380
2805.014895	774286.301396	39.736397
2807.694961	775800.119111	39.741415
2810.470894	777277.359832	39.746432
2812.998290	778748.598162	39.751450
2815.629300	780213.385875	39.756468
2818.247654	781691.282556	39.761485
2820.672933	783187.854842	39.766503
2823.354587	784664.496833	39.771520
2826.081797	786148.825642	39.776538
2828.187947	787657.867123	39.781556
2831.006825	789196.975184	39.786573
2833.281330	790724.760952	39.791591
2836.384471	792228.946075	39.796608
2839.267114	793769.652581	39.801626
2842.001539	795342.531914	39.806644
2844.635811	796886.273449	39.811661
2847.342960	798449.400079	39.816679
2850.136571	800017.989824	39.821696
2852.851069	801601.855378	39.826714
2855.678571	803185.879607	39.831732
2859.310397	804754.632184	39.836749
2861.574817	806364.100188	39.841767
2864.554575	807978.844635	39.846784
2867.255777	809574.820964	39.851802
2869.866866	811185.348688	39.856820
2872.898715	812811.309349	39.861837
2875.523575	814451.360956	39.866855
2878.604971	816090.499651	39.871872
2881.607173	817722.464089	39.876890
2884.573942	819357.259844	39.881908
2887.547565	821029.533211	39.886925
2890.114652	822678.615368	39.891943
2893.457604	824326.428265	39.896960
2896.383453	825967.704886	39.901978
2899.033075	827658.844929	39.906996
2902.476063	829346.152599	39.912013
2905.140607	831015.900180	39.917031
2908.228268	832702.545748	39.922048
2911.153711	834380.304250	39.927066
2913.929119	836048.886742	39.932084
2916.806624	837718.968545	39.937101
2919.836617	839405.481855	39.942119
2922.816183	841114.284929	39.947136
2926.122196	842809.198406	39.952154
2928.380138	844491.576729	39.957172
2931.558472	846164.507603	39.962189
2934.362559	847889.070388	39.967207
2937.546337	849607.461026	39.972224
2940.685631	851289.436331	39.977242
2943.552008	853000.243659	39.982260
2946.602213	854710.259568	39.987277
2949.544741	856414.773632	39.992295
2952.413392	858124.459768	39.997312
2955.296050	859846.671986	40.002330
2958.157689	861556.667050	40.007348
2961.014719	863289.363278	40.012365
2964.212499	865014.239821	40.017383
2966.958700	866737.538194	40.022400
2970.080774	868460.090573	40.027418
2972.980955	870189.162470	40.032436
2975.825931	871908.256001	40.037453
2979.093045	873662.317290	40.042471
2982.166910	875385.988871	40.047488
2985.258392	877133.637734	40.052506
2988.075561	878839.804142	40.057524
2991.221947	880574.240450	40.062541
2994.290139	882315.332561	40.067559
2997.338824	884043.541149	40.072576
3000.659985	885776.024917	40.077594
3003.827044	887505.701059	40.082612
3006.806175	889215.388640	40.087629
3009.868160	890890.676085	40.092647
3012.634947	892567.745228	40.097664
3015.475881	894248.461380	40.102682
3018.016744	895941.561168	40.107700
3021.004555	897590.119910	40.112717
3023.912936	899294.793957	40.117735
3026.777392	901002.432015	40.122752
3030.076220	902691.469311	40.127770
3032.538840	904376.575068	40.132788
3035.316702	906085.095025	40.137805
3038.251560	907806.830316	40.142823
3041.057235	909541.717693	40.147840
3044.511306	911268.647216	40.152858
3047.178930	913013.340780	40.157876
3050.442941	914746.331093	40.162893
3053.561139	916505.320804	40.167911
3056.370386	918254.287498	40.172928
3059.878529	920025.530411	40.177946
3062.652652	921787.006640	40.182964
3066.022513	923535.913475	40.187981
3068.949099	925295.552486	40.192999
3071.892312	927066.218962	40.198016
3075.121732	928850.156345	40.203034
3078.035566	930639.589417	40.208052
3080.951229	932440.685622	40.213069
3084.155582	934226.279297	40.218087
3087.230010	936041.068769	40.223104
3090.722029	937858.420070	40.228122
3093.543882	939649.995748	40.233140
3096.386097	941473.283748	40.238157
3099.750287	943302.638145	40.243175
3102.268849	945127.092911	40.248192
3105.914669	946938.204731	40.253210
3108.981348	948770.267388	40.258228
3112.323691	950615.763827	40.263245
3115.456334	952460.059163	40.268263
3118.460129	954287.969286	40.273280
3122.282901	956130.071366	40.278298
3125.356024	958025.963540	40.283316
3128.350315	959918.801394	40.288333
3131.329050	961806.719281	40.293351
3134.381851	963690.879305	40.298368
3137.759244	965607.782540	40.303386
3140.514323	967520.731440	40.308404
3143.521000	969431.928523	40.313421
3146.720471	971330.941072	40.318439
3149.746858	973256.477969	40.323456
3153.080697	975191.656479	40.328474
3156.056734	977110.152324	40.333492
3159.009220	979038.438421	40.338509
3162.373392	980958.698799	40.343527
3165.625677	982888.559779	40.348544
3168.963567	984803.732783	40.353562
3172.215958	986759.451142	40.358580
3175.551405	988709.230208	40.363597
3178.763291	990630.639422	40.368615
3181.523210	992551.668608	40.373632
3184.504880	994492.522578	40.378650
3187.559415	996463.699326	40.383668
3190.822698	998397.632593	40.388685
3194.577990	1000346.167745	40.393703
3197.088051	1002304.721368	40.398720
3200.439810	1004268.765988	40.403738
3203.451632	1006220.446616	40.408756
3206.617039	1008185.294464	40.413773
3210.030502	1010146.799967	40.418791
3213.079700	1012121.055701	40.423808
3216.424068	1014049.235629	40.428826
3219.447469	1015988.331349	40.433844
3222.660968	1017899.621888	40.438861
3225.533093	1019801.608907	40.443879
3228.446726	1021740.769176	40.448896
3231.799283	1023644.276123	40.453914
3234.535375	1025570.149074	40.458932
3238.085199	1027530.884873	40.463949
3241.187636	1029455.070013	40.468967
3244.005697	1031389.648419	40.473984
3246.819191	1033351.456456	40.479002
3249.723041	1035332.439161	40.484020
3252.803563	1037310.566148	40.489037
3256.039629	1039299.633110	40.494055
3258.893314	1041308.199128	40.499072
3262.352184	1043307.073838	40.504090
3265.301655	1045327.083137	40.509108
3268.083618	1047370.168932	40.514125
3271.778356	1049404.842816	40.519143
3274.689495	1051448.520070	40.524160
3278.226763	1053517.309475	40.529178
3281.140472	1055581.484602	40.534196
3284.574944	1057644.513581	40.539213
3287.908030	1059721.295220	40.544231
3291.149096	1061810.658877	40.549248
3294.487015	1063894.124905	40.554266
3297.766723	1065999.843535	40.559284
3301.022320	1068095.357312	40.564301
3304.297736	1070207.904043	40.569319
3307.441514	1072326.272409	40.574336
3310.910383	1074453.828882	40.579354
3314.688362	1076564.989786	40.584372
3317.718832	1078703.416212	40.589389
3321.203283	1080825.808037	40.594407
3324.555843	1082942.994548	40.599424
3328.233079	1085091.246789	40.604442
3331.372499	1087225.833904	40.609460
3334.365835	1089373.749743	40.614477
3338.043920	1091529.395760	40.619495
3341.259756	1093683.879384	40.624512
3344.888868	1095831.998042	40.629530
3348.312538	1098001.623525	40.634548
3351.507868	1100143.045214	40.639565
3354.872794	1102312.094309	40.644583
3358.141873	1104460.371182	40.649600
3361.446141	1106615.120901	40.654618
3364.851781	1108795.652560	40.659636
3368.075706	1110975.044849	40.664653
3371.624786	1113167.009612	40.669671
3374.607531	1115332.210235	40.674688
3378.085315	1117513.281246	40.679706
3381.732455	1119708.735153	40.684724
3384.844176	1121884.949609	40.689741
3388.162003	1124070.688308	40.694759
3391.528462	1126268.621531	40.699776
3394.877796	1128451.611616	40.704794
3398.413938	1130675.685678	40.709812
3401.781572	1132874.971519	40.714829
3405.755426	1135063.299192	40.719847
3408.748072	1137271.154928	40.724864
3412.577049	1139461.008161	40.729882
3415.686521	1141664.932338	40.734900
3418.889618	1143861.775235	40.739917
3422.488216	1146066.812208	40.744935
3425.876415	1148289.299143	40.749952
3429.177721	1150473.452789	40.754970
3432.688847	1152671.398842	40.759988
3436.069865	1154879.210019	40.765005
3439.691559	1157077.355399	40.770010
3442.348885	1159216.930360	40.775015
3445.937279	1161283.077137	40.780020
3448.881372	1163297.966644	40.785024
3451.751956	1165272.046909	40.790029
3455.416972	1167127.799701	40.795034
3458.509243	1168916.636844	40.800039
3461.344087	1170633.101995	40.805044
3464.167122	1172266.566938	40.810048
3466.858613	1173814.394199	40.815053
3469.450437	1175296.922002	40.820058
3471.523562	1176718.421342	40.825063
3474.016371	1178045.151505	40.830068
3476.158242	1179309.997452	40.835072
3478.698088	1180508.077923	40.840077
3480.845336	1181650.490784	40.845082
3482.649881	1182707.706466	40.850087
3484.441093	1183684.146122	40.855092
3486.662080	1184631.631011	40.860096
3487.959415	1185504.111097	40.865101
3490.044066	1186319.215469	40.870106
3491.175014	1187089.767030	40.875111
3492.976917	1187799.437075	40.880116
3494.389466	1188469.675805	40.885120
3495.677602	1189086.164187	40.890125
3497.133142	1189638.344486	40.895130
3498.419318	1190159.756278	40.900135
3500.031661	1190640.176382	40.905140
3501.117906	1191095.075548	40.910144
3502.058329	1191475.343459	40.915149
3502.988666	1191823.166111	40.920154
3503.959960	1192165.508789	40.925159
3504.629012	1192452.444378	40.930164
3505.427999	1192700.446558	40.935168
3506.376938	1192932.159147	40.940173
3507.434618	1193127.956783	40.945178
3507.999778	1193313.682469	40.950183
3508.517474	1193444.455479	40.955188
3509.258129	1193567.673547	40.960192
3509.908492	1193660.938461	40.965197
3510.705941	1193744.220556	40.970202
3511.261419	1193798.140463	40.975207
3511.794661	1193828.204887	40.980212
3512.429885	1193837.493529	40.985216
3512.861371	1193842.870590	40.990221
3513.561197	1193817.393908	40.995226
3513.995179	1193771.577534	41.000231
3514.073254	1193704.214620	41.005236
3514.537495	1193621.381850	41.010240
3515.061253	1193546.146835	41.015245
3515.790049	1193431.986429	41.020250
3515.660521	1193311.952633	41.025255
3516.185827	1193193.499181	41.030260
3517.106107	1193056.376762	41.035264
3517.074942	1192895.544507	41.040269
3517.139655	1192715.337403	41.045274
3517.679164	1192536.455146	41.050279
3518.045047	1192357.407374	41.055284
3518.207602	1192163.352999	41.060288
3518.498865	1191945.308894	41.065293
3518.729874	1191721.439377	41.070298
3518.794085	1191502.098381	41.075303
3519.127430	1191274.903577	41.080308
3519.590615	1191019.388684	41.085312
3519.525372	1190767.613692	41.090317
3519.878958	1190503.538501	41.095322
3519.897296	1190243.828888	41.100327
3520.028071	1189975.627565	41.105332
3520.129745	1189700.178611	41.110336
3520.388151	1189427.603536	41.115341
3520.551531	1189125.696481	41.120346
3520.582727	1188832.443649	41.125351
3520.834541	1188550.891324	41.130356
3520.847894	1188245.760686	41.135360
3521.036149	1187934.940928	41.140365
3521.121605	1187604.276021	41.145370
3521.199763	1187295.787135	41.150375
3521.142664	1186986.549693	41.155380
3521.465217	1186663.216055	41.160384
3521.690873	1186346.086661	41.165389
3521.560046	1186011.216656	41.170394
3521.701659	1185676.562372	41.175399
3521.692789	1185346.897806	41.180404
3522.129788	1185014.316086	41.185408
3521.980500	1184670.141435	41.190413
3521.895922	1184312.288126	41.195418
3521.835756	1183966.169965	41.200423
3521.900465	1183624.431637	41.205428
3521.906408	1183278.539045	41.210432
3521.960845	1182931.109327	41.215437
3522.488599	1182585.931794	41.220442
3522.627574	1182228.462699	41.225447
3522.553707	1181841.629507	41.230452
3522.594765	1181463.787567	41.235456
3522.307853	1181115.915920	41.240461
3522.080113	1180765.374488	41.245466
3522.411824	1180390.231630	41.250471
3522.436785	1180020.103876	41.255476
3522.197097	1179641.233740	41.260480
3522.374749	1179295.141602	41.265485
3522.418898	1178921.447196	41.270490
3522.346315	1178550.006169	41.275495
3522.264377	1178183.910442	41.280500
3522.692687	1177803.665764	41.285504
3522.674392	1177421.582256	41.290509
3522.479973	1177037.238015	41.295514
3522.432442	1176678.852310	41.300519
3522.527589	1176289.693016	41.305524
3522.383548	1175899.978476	41.310528
3522.132346	1175536.929085	41.315533
3522.494249	1175155.276412	41.320538
3522.464250	1174792.892884	41.325543
3522.693583	1174399.233453	41.330548
3522.699784	1173986.251267	41.335552
3522.486295	1173622.307868	41.340557
3522.396068	1173247.850901	41.345562
3522.710150	1172868.679168	41.350567
3522.556079	1172468.335200	41.355572
3522.914233	1172078.629336	41.360576
3522.447933	1171705.349766	41.365581
3522.352633	1171314.057803	41.370586
3522.435544	1170912.706345	41.375591
3522.410137	1170519.173283	41.380596
3522.699008	1170143.864895	41.385600
3522.140907	1169763.195674	41.390605
3522.383880	1169349.524184	41.395610
3522.565259	1168965.088729	41.400615
3522.447838	1168582.467595	41.405620
3522.464476	1168185.070518	41.410624
3522.096228	1167798.940641	41.415629
3522.562176	1167392.724195	41.420634
3522.277846	1167009.260078	41.425639
3522.227750	1166638.098884	41.430644
3522.343724	1166251.397259	41.435648
3521.876310	1165853.997130	41.440653
3522.211520	1165449.351182	41.445658
3522.461240	1165088.891972	41.450663
3522.144771	1164671.731040	41.455668
3522.335788	1164277.597774	41.460672
3522.351094	1163906.420965	41.465677
3522.595023	1163517.134393	41.470682
3522.308596	1163101.544066	41.475687
3522.132544	1162702.155842	41.480692
3521.981709	1162310.009724	41.485696
3521.726423	1161923.427532	41.490701
3522.005633	1161525.481323	41.495706
3521.969505	1161155.724896	41.500711
3522.057900	1160765.692420	41.505716
3522.337547	1160366.429306	41.510720
3521.946030	1159958.359125	41.515725
3521.751676	1159573.957309	41.520730
3521.617463	1159193.583457	41.525735
3521.718930	1158807.942116	41.530740
3521.891024	1158410.439227	41.535744
3521.736017	1158015.797522	41.540749
3521.643230	1157627.264069	41.545754
3521.470423	1157261.228369	41.550759
3521.744084	1156864.821509	41.555764
3521.808398	1156448.173121	41.560768
3521.592014	1156075.250195	41.565773
3521.741840	1155676.503365	41.570778
3521.912602	1155305.543775	41.575783
3521.716933	1154903.199321	41.580788
3521.729884	1154512.714763	41.585792
3521.411436	1154119.510950	41.590797
3521.366985	1153704.177466	41.595802
3521.433007	1153330.066797	41.600807
3521.414188	1152964.179886	41.605812
3521.803362	1152572.258681	41.610816
3521.522033	1152176.441973	41.615821
3521.489441	1151763.415250	41.620826
3521.305252	1151380.306181	41.625831
3521.320541	1150978.763369	41.630836
3521.267818	1150599.837703	41.635840
3521.053684	1150223.847704	41.640845
3521.086515	1149832.349718	41.645850
3521.039433	1149439.320082	41.650855
3520.921910	1149040.872506	41.655860
3521.165601	1148658.158321	41.660864
3521.320086	1148285.380350	41.665869
3521.328789	1147879.433397	41.670874
3521.398000	1147506.709242	41.675879
3521.148692	1147110.127734	41.680884
3521.242312	1146716.113887	41.685888
3521.100040	1146334.242621	41.690893
3521.285291	1145934.467985	41.695898
3521.487345	1145533.427882	41.700903
3521.255760	1145157.079694	41.705908
3521.326187	1144776.957071	41.710912
3521.080547	1144388.230117	41.715917
3521.112413	1143973.350070	41.720922
3521.098706	1143589.267798	41.725927
3520.796157	1143212.223808	41.730932
3520.766394	1142831.219057	41.735936
3520.520923	1142444.530819	41.740941
3520.917266	1142061.028956	41.745946
3520.772626	1141676.544804	41.750951
3520.867072	1141276.053437	41.755956
3520.720055	1140892.556437	41.760960
3520.469059	1140518.822900	41.765965
3520.462219	1140139.708332	41.770970
3520.322298	1139767.042278	41.775975
3520.271683	1139367.284660	41.780980
3520.499520	1138975.899083	41.785984
3520.233223	1138620.448965	41.790989
3520.247722	1138237.777425	41.795994
3520.172391	1137861.738996	41.800999
3520.264360	1137480.044392	41.806004
3520.533370	1137084.144801	41.811008
3520.464023	1136715.715564	41.816013
3520.282262	1136335.503116	41.821018
3520.249197	1135956.568604	41.826023
3519.717330	1135588.612184	41.831028
3520.364085	1135216.066657	41.836032
3520.051708	1134821.898903	41.841037
3520.211859	1134437.599401	41.846042
3520.240145	1134072.295764	41.851047
3520.048375	1133694.176075	41.856052
3520.408181	1133308.811912	41.861056
3519.885270	1132920.429205	41.866061
3519.842487	1132545.434292	41.871066
3519.895191	1132195.773770	41.876071
3519.858760	1131810.176184	41.881076
3520.009691	1131419.576837	41.886080
3519.874562	1131049.149442	41.891085
3519.856840	1130679.342419	41.896090
3519.920517	1130326.134706	41.901095
3519.664209	1129930.073761	41.906100
3519.801245	1129546.470518	41.911104
3519.530222	1129186.110526	41.916109
3519.674742	1128808.824416	41.921114
3519.781054	1128436.463617	41.926119
3519.352018	1128071.298727	41.931124
3519.544185	1127722.843288	41.936128
3519.163482	1127342.971584	41.941133
3519.367758	1126971.919290	41.946138
3519.297590	1126608.022096	41.951143
3519.403663	1126240.931123	41.956148
3519.311895	1125871.183107	41.961152
3519.610837	1125503.819349	41.966157
3519.373980	1125142.704533	41.971162
3519.181226	1124766.425111	41.976167
3519.005230	1124380.122246	41.981172
3519.194135	1124018.956473	41.986176
3518.896160	1123682.121238	41.991181
3518.913041	1123311.226044	41.996186
3519.409810	1122940.321278	42.001191
3519.325814	1122589.862351	42.006196
3519.066994	1122211.033394	42.011200
3518.946478	1121837.773250	42.016205
3518.957606	1121484.750271	42.021210
3519.201376	1121117.284350	42.026215
3518.801229	1120766.567468	42.031220
3519.148592	1120393.510444	42.036224
3519.065638	1120032.977354	42.041229
3518.858131	1119655.197239	42.046234
3519.210221	1119299.496954	42.051239
3518.772125	1118952.668869	42.056244
3518.753376	1118578.878702	42.061248
3518.448188	1118210.160115	42.066253
3518.785649	1117855.700425	42.071258
3518.764062	1117497.654827	42.076263
3518.700796	1117136.065639	42.081268
3518.851361	1116770.222843	42.086272
3518.720089	1116404.115519	42.091277
3518.618049	1116045.700182	42.096282
3518.666991	1115693.909623	42.101287
3518.421589	1115341.191027	42.106292
3518.773821	1114970.234330	42.111296
3518.519191	1114629.865963	42.116301
3518.444061	1114270.564701	42.121306
3518.354058	1113913.530680	42.126311
3518.320004	1113569.148571	42.131316
3518.380781	1113209.563142	42.136320
3518.032214	1112839.242223	42.141325
3518.538432	1112480.488490	42.146330
3518.269900	1112143.208097	42.151335
3518.134926	1111794.817388	42.156340
3518.146956	1111423.767034	42.161344
3518.243983	1111082.161641	42.166349
3518.071947	1110719.966974	42.171354
3518.063922	1110382.246843	42.176359
3518.134076	1110036.571303	42.181364
3518.030508	1109677.540003	42.186368
3517.695881	1109338.090083	42.191373
3517.579535	1108975.864189	42.196378
3518.074364	1108618.668245	42.201383
3517.878543	1108289.248324	42.206388
3517.882741	1107929.414316	42.211392
3517.844717	1107578.633933	42.216397
3517.994998	1107238.398781	42.221402
3517.538562	1106902.730238	42.226407
3517.939156	1106553.625212	42.231412
3517.817436	1106190.066711	42.236416
3517.350960	1105852.615253	42.241421
3517.390731	1105506.558182	42.246426
3517.770511	1105182.775494	42.251431
3517.714794	1104833.634183	42.256436
3517.839243	1104492.656685	42.261440
3517.632495	1104152.667590	42.266445
3517.986424	1103777.498478	42.271450
3517.926950	1103444.511077	42.276455
3517.550676	1103093.972144	42.281460
3517.934281	1102728.759085	42.286464
3517.766746	1102412.067723	42.291469
3517.550693	1102071.471104	42.296474
3517.273508	1101719.870782	42.301479
3517.091635	1101367.371537	42.306484
3517.707781	1101030.013440	42.311488
3517.232153	1100702.852418	42.316493
3517.106023	1100340.429829	42.321498
3517.455415	1100012.995537	42.326503
3516.834356	1099692.394705	42.331508
3517.288068	1099332.103888	42.336512
3516.846479	1099005.025675	42.341517
3517.007328	1098657.935517	42.346522
3517.193635	1098323.922291	42.351527
3517.034186	1097999.893085	42.356532
3517.145925	1097636.006491	42.361536
3516.681887	1097296.201801	42.366541
3517.097702	1096974.695010	42.371546
3516.594443	1096664.897116	42.376551
3516.573218	1096335.100617	42.381556
3516.368528	1095995.936985	42.386560
3516.703797	1095675.514530	42.391565
3516.505102	1095348.845009	42.396570
3516.498690	1095005.758780	42.401575
3516.536822	1094680.828331	42.406580
3516.590001	1094366.117445	42.411584
3516.143729	1094057.596654	42.416589
3516.119922	1093710.793889	42.421594
3516.542304	1093378.351087	42.426599
3516.126095	1093071.683857	42.431604
3516.641556	1092745.314142	42.436608
3516.063223	1092410.678965	42.441613
3516.323999	1092080.864222	42.446618
3516.423245	1091773.176849	42.451623
3515.906732	1091468.446426	42.456628
3516.221786	1091126.019295	42.461632
3515.884709	1090831.854278	42.466637
3515.999095	1090489.132680	42.471642
3516.463000	1090152.941362	42.476647
3515.720077	1089857.832491	42.481652
3516.280476	1089535.285671	42.486656
3516.165903	1089223.369528	42.491661
3515.953806	1088897.079798	42.496666
3515.935507	1088563.839689	42.501671
3515.984518	1088265.256024	42.506676
3515.886891	1087954.797407	42.511680
3515.751060	1087620.177183	42.516685
3515.838628	1087298.150442	42.521690
3515.949782	1087002.170667	42.526695
3515.444889	1086688.352203	42.531700
3515.779551	1086373.418791	42.536704
3515.841564	1086048.925871	42.541709
3515.625393	1085734.046161	42.546714
3515.810347	1085431.833252	42.551719
3515.666227	1085122.850409	42.556724
3515.701514	1084779.685787	42.561728
3515.516942	1084490.809374	42.566733
3515.699597	1084183.253598	42.571738
3515.668202	1083871.496095	42.576743
3515.710289	1083548.104034	42.581748
3515.849795	1083229.760041	42.586752
3515.599722	1082931.604169	42.591757
3515.534931	1082626.974679	42.596762
3515.660455	1082304.646119	42.601767
3515.568393	1081977.921388	42.606772
3515.590617	1081664.685676	42.611776
3515.588263	1081375.614000	42.616781
3515.682200	1081066.169855	42.621786
3515.691559	1080748.565892	42.626791
3515.561860	1080428.855195	42.631796
3515.663771	1080123.674495	42.636800
3515.285577	1079805.215726	42.641805
3515.179877	1079495.235467	42.646810
3515.346556	1079205.349072	42.651815
3514.919992	1078898.075239	42.656820
3515.225662	1078563.977338	42.661824
3515.199468	1078286.841068	42.666829
3514.775477	1077991.035552	42.671834
3515.373955	1077680.068200	42.676839
3515.106373	1077365.961287	42.681844
3515.354884	1077056.360278	42.686848
3515.274819	1076769.649884	42.691853
3514.841219	1076479.909699	42.696858
3515.172622	1076163.042149	42.701863
3514.896799	1075866.328857	42.706868
3514.679955	1075552.493478	42.711872
3514.866467	1075257.399825	42.716877
3515.134245	1074945.082646	42.721882
3514.945632	1074643.389689	42.726887
3514.916828	1074359.426289	42.731892
3515.092990	1074041.116396	42.736896
3514.924227	1073751.187937	42.741901
3514.841859	1073471.895120	42.746906
3514.722544	1073159.347578	42.751911
3514.517980	1072852.081397	42.756916
3514.430980	1072551.697755	42.761920
3514.279560	1072266.877153	42.766925
3514.020032	1071991.574346	42.771930
3514.434178	1071684.332943	42.776935
3514.340840	1071397.150789	42.781940
3514.194665	1071120.728220	42.786945
3514.702711	1070832.360049	42.791949
3514.340316	1070539.024935	42.796954
3514.473575	1070231.459923	42.801959
3514.283933	1069960.754388	42.806964
3514.502739	1069681.122454	42.811969
3514.469783	1069384.498345	42.816973
3514.139706	1069073.579258	42.821978
3514.212830	1068802.869429	42.826983
3513.658297	1068521.190074	42.831988
3514.038551	1068234.245020	42.836993
3514.133019	1067935.117153	42.841997
3514.030702	1067647.162895	42.847002
3514.204452	1067377.616572	42.852007
3513.970428	1067095.715037	42.857012
3513.972154	1066790.672169	42.862017
3514.038794	1066514.751894	42.867021
3513.903004	1066237.311734	42.872026
3514.207433	1065963.922290	42.877031
3513.726369	1065665.727682	42.882036
3513.615313	1065376.308652	42.887041
3513.642832	1065106.386237	42.892045
3513.510199	1064849.661052	42.897050
3513.941354	1064563.381868	42.902055
3513.738483	1064283.640564	42.907060
3513.385680	1063999.001004	42.912065
3513.582677	1063722.341498	42.917069
3513.324782	1063442.951481	42.922074
3513.403572	1063173.792035	42.927079
3513.745544	1062909.870829	42.932084
3513.431028	1062625.731467	42.937089
3513.575100	1062359.313336	42.942093
3513.463985	1062081.755545	42.947098
3513.747824	1061821.257874	42.952103
3513.357736	1061557.488649	42.957108
3513.567731	1061260.481835	42.962113
3513.557487	1060969.658616	42.967117
3513.455322	1060709.268195	42.972122
3513.380535	1060442.697020	42.977127
3513.226576	1060156.188510	42.982132
3513.308429	1059888.601549	42.987137
3513.439733	1059631.396622	42.992141
3513.214949	1059344.664908	42.997146
3513.229535	1059062.310282	43.002151
3513.442667	1058817.095799	43.007156
3513.508954	1058548.579260	43.012161
3513.052257	1058278.208786	43.017165
3512.932531	1057997.363304	43.022170
3513.006261	1057733.912621	43.027175
3513.163866	1057467.255543	43.032180
3513.189587	1057190.585001	43.037185
3512.723507	1056944.242652	43.042189
3512.276839	1056676.008499	43.047194
3513.214966	1056409.942777	43.052199
3513.011361	1056153.883695	43.057204
3513.063461	1055876.468191	43.062209
3512.992963	1055620.073240	43.067213
3512.926858	1055360.291646	43.072218
3513.100135	1055087.540142	43.077223
3512.668436	1054828.661382	43.082228
3512.798347	1054585.007797	43.087233
3512.845438	1054306.357241	43.092237
3512.438100	1054037.699081	43.097242
3512.591894	1053793.813810	43.102247
3512.422728	1053518.919816	43.107252
3512.482437	1053262.008174	43.112257
3512.692388	1053004.288312	43.117261
3512.489997	1052777.776278	43.122266
3512.637186	1052506.637629	43.127271
3512.542465	1052262.436347	43.132276
3512.306363	1052013.135253	43.137281
3512.272372	1051739.673815	43.142285
3512.338632	1051466.954087	43.147290
3512.459872	1051234.151521	43.152295
3512.237866	1050994.545864	43.157300
3512.423468	1050726.979721	43.162305
3512.411104	1050480.563588	43.167309
3512.289184	1050221.031908	43.172314
3512.188087	1049971.134061	43.177319
3512.180178	1049723.525547	43.182324
3512.346943	1049468.156948	43.187329
3512.262738	1049211.949335	43.192333
3511.966557	1048966.091549	43.197338
3511.959526	1048719.113542	43.202343
3511.943315	1048486.700597	43.207348
3512.096248	1048235.620833	43.212353
3512.145140	1047984.643352	43.217357
3511.857603	1047724.056570	43.222362
3512.198245	1047488.936582	43.227367
3512.077849	1047240.173618	43.232372
3511.869601	1046979.731846	43.237377
3511.671230	1046760.213667	43.242381
3511.997394	1046515.979056	43.247386
3511.950060	1046267.643172	43.252391
3511.621340	1046014.224655	43.257396
3511.756245	1045769.216142	43.262401
3511.661511	1045533.215794	43.267405
3511.384359	1045305.927255	43.272410
3511.564745	1045072.083209	43.277415
3511.711029	1044825.196105	43.282420
3511.520600	1044589.074756	43.287425
3511.648900	1044358.976166	43.292429
3511.700847	1044105.987292	43.297434
3511.689542	1043848.167256	43.302439
3511.647320	1043637.193782	43.307444
3511.449714	1043413.582177	43.312449
3511.674386	1043169.506756	43.317453
3511.548636	1042922.000105	43.322458
3511.606979	1042685.466929	43.327463
3511.341310	1042452.552176	43.332468
3511.185018	1042203.279261	43.337473
3511.558776	1041972.558177	43.342477
3511.226736	1041749.674759	43.347482
3511.395237	1041516.842532	43.352487
3511.402412	1041281.031105	43.357492
3511.153394	1041034.330434	43.362497
3511.196814	1040826.618810	43.367501
3511.238206	1040602.371362	43.372506
3511.202646	1040341.106125	43.377511
3510.978183	1040112.436243	43.382516
3511.218271	1039898.277584	43.387521
3511.260014	1039688.203628	43.392525
3511.160491	1039456.199283	43.397530
3511.330485	1039207.705009	43.402535
3511.073513	1038980.250777	43.407540
3510.890476	1038757.126095	43.412545
3510.646029	1038529.651371	43.417549
3510.592220	1038282.312939	43.422554
3511.290807	1038054.566782	43.427559
3510.968290	1037858.118627	43.432564
3511.113857	1037636.828999	43.437569
3511.266352	1037398.507951	43.442573
3510.730288	1037184.082500	43.447578
3510.882898	1036945.258445	43.452583
3510.542215	1036726.334011	43.457588
3510.663363	1036504.132859	43.462593
3510.725565	1036268.293250	43.467597
3510.413444	1036054.464526	43.472602
3510.742248	1035851.647143	43.477607
3510.656406	1035639.119567	43.482612
3510.502499	1035394.087882	43.487617
3510.528855	1035179.879593	43.492621
3510.459404	1034986.964992	43.497626
3510.736620	1034755.766936	43.502631
3510.343323	1034527.669379	43.507636
3510.639401	1034300.900449	43.512641
3510.137148	1034099.317373	43.517645
3510.265167	1033902.655442	43.522650
3510.480175	1033681.390776	43.527655
3510.348440	1033468.787989	43.532660
3510.474386	1033242.584733	43.537665
3510.453227	1033035.657551	43.542669
3510.176131	1032812.890859	43.547674
3510.685691	1032600.923715	43.552679
3510.390152	1032389.758720	43.557684
3510.423706	1032185.888610	43.562689
3510.388732	1031961.983223	43.567693
3510.478542	1031743.469736	43.572698
3510.372312	1031525.560873	43.577703
3510.449654	1031313.519215	43.582708
3510.157186	1031101.627233	43.587713
3510.271357	1030899.149183	43.592717
3509.938000	1030679.598662	43.597722
3510.268999	1030473.777267	43.602727
3510.445481	1030283.758127	43.607732
3509.887309	1030066.254083	43.612737
3510.208624	1029843.076595	43.617741
3510.101069	1029638.943025	43.622746
3510.230031	1029444.448166	43.627751
3509.850684	1029236.083186	43.632756
3510.023883	1029007.569712	43.637761
3510.098875	1028803.666137	43.642765
3510.010890	1028591.451503	43.647770
3510.059594	1028368.550631	43.652775
3510.223081	1028187.761850	43.657780
3510.145602	1027978.912783	43.662785
3509.913540	1027758.843265	43.667789
3509.597918	1027566.681415	43.672794
3509.773566	1027385.767819	43.677799
3509.784636	1027170.867001	43.682804
3509.646196	1026967.125380	43.687809
3509.848130	1026780.374230	43.692813
3509.340857	1026559.624559	43.697818
3509.848211	1026358.176929	43.702823
3509.794669	1026178.424895	43.707828
3509.269634	1025976.745936	43.712833
3509.825175	1025753.269713	43.717837
3509.788533	1025550.525805	43.722842
3509.876462	1025362.970789	43.727847
3509.396627	1025179.089225	43.732852
3509.403431	1024977.189721	43.737857
3509.880416	1024768.807983	43.742861
3509.633407	1024580.215656	43.747866
3509.741644	1024390.976836	43.752871
3509.591345	1024175.793701	43.757876
3509.507795	1023974.842366	43.762881
3509.444885	1023784.447892	43.767885
3509.319553	1023591.245605	43.772890
3509.745795	1023403.860117	43.777895
3509.392025	1023201.859046	43.782900
3509.472961	1022994.833993	43.787905
3509.704721	1022795.242862	43.792909
3509.305278	1022631.724240	43.797914
3509.447588	1022432.037940	43.802919
3509.497892	1022219.461857	43.807924
3509.350335	1022020.390495	43.812929
3509.155795	1021847.408202	43.817933
3509.139232	1021651.502594	43.822938
3509.373233	1021447.207776	43.827943
3509.294505	1021244.508915	43.832948
3508.925124	1021062.898822	43.837953
3509.210177	1020885.831031	43.842957
3509.219764	1020702.594868	43.847962
3509.285214	1020508.575884	43.852967
3509.056486	1020322.359371	43.857972
3509.214109	1020123.655462	43.862977
3508.749704	1019922.621566	43.867981
3509.003738	1019754.642689	43.872986
3508.927232	1019583.220441	43.877991
3508.964709	1019379.949965	43.882996
3508.932874	1019194.439797	43.888001
3509.127634	1019025.090458	43.893005
3508.919540	1018819.705451	43.898010
3508.644765	1018625.483336	43.903015
3508.544765	1018462.861232	43.908020
3508.426975	1018300.722568	43.913025
3508.651676	1018112.805358	43.918029
3508.477184	1017918.930477	43.923034
3508.596446	1017749.263953	43.928039
3508.945429	1017590.036559	43.933044
3508.528909	1017407.636521	43.938049
3508.862440	1017207.441612	43.943053
3508.774437	1017034.487506	43.948058
3508.551230	1016858.541210	43.953063
3508.654922	1016686.321369	43.958068
3508.703463	1016491.778077	43.963073
3508.645483	1016309.283329	43.968077
3508.619704	1016155.125090	43.973082
3508.646381	1015956.780725	43.978087
3508.679900	1015778.137045	43.983092
3508.443250	1015620.600815	43.988097
3508.707767	1015426.276358	43.993101
3508.328266	1015256.422547	43.998106
3508.477969	1015079.193978	44.003111
3508.626561	1014913.126807	44.008116
3508.654231	1014716.874807	44.013121
3508.810423	1014540.599265	44.018125
3508.373538	1014391.024493	44.023130
3508.384415	1014204.856985	44.028135
3508.319771	1014028.213305	44.033140
3508.480668	1013839.581063	44.038145
3508.237218	1013685.488104	44.043149
3508.310196	1013534.641103	44.048154
3508.333059	1013337.176263	44.053159
3508.428093	1013159.119194	44.058164
3508.131171	1012992.583064	44.063169
3508.163834	1012832.884554	44.068173
3508.010213	1012655.435340	44.073178
3508.250786	1012499.675937	44.078183
3508.202660	1012341.142518	44.083188
3507.887321	1012161.664294	44.088193
3508.136378	1011977.035433	44.093197
3508.221442	1011822.254445	44.098202
3508.434262	1011669.002700	44.103207
3507.938907	1011507.701886	44.108212
3508.167136	1011325.872797	44.113217
3508.407687	1011155.112898	44.118221
3507.792543	1010994.594456	44.123226
3508.124991	1010831.000184	44.128231
3508.029209	1010673.107885	44.133236
3507.791520	1010497.548047	44.138241
3507.969881	1010331.146469	44.143245
3507.878492	1010174.114102	44.148250
3508.062117	1010010.520538	44.153255
3508.083010	1009842.186727	44.158260
3508.032252	1009689.604909	44.163265
3507.806195	1009522.565731	44.168269
3508.090956	1009347.564403	44.173274
3508.042032	1009174.556634	44.178279
3507.995503	1009035.175797	44.183284
3507.733607	1008867.539896	44.188289
3507.835663	1008682.438518	44.193293
3508.260077	1008539.954375	44.198298
3508.031148	1008383.478073	44.203303
3507.747026	1008211.937744	44.208308
3507.781274	1008033.825954	44.213313
3508.216440	1007871.781702	44.218317
3507.623682	1007725.069441	44.223322
3507.615645	1007559.394611	44.228327
3507.546236	1007400.434040	44.233332
3507.571800	1007240.383768	44.238337
3507.736158	1007101.406604	44.243341
3507.316732	1006954.159560	44.248346
3507.638743	1006789.380174	44.253351
3507.570128	1006634.773827	44.258356
3507.403965	1006470.454519	44.263361
3507.535367	1006313.764232	44.268365
3507.305846	1006175.509910	44.273370
3507.345867	1006007.933833	44.278375
3507.566150	1005863.956953	44.283380
3507.320313	1005702.059871	44.288385
3507.451362	1005569.761531	44.293389
3507.234291	1005405.127822	44.298394
3507.652839	1005253.224149	44.303399
3507.408269	1005104.441029	44.308404
3507.249214	1004940.465126	44.313409
3507.427541	1004788.491256	44.318413
3507.180816	1004646.894934	44.323418
3507.300948	1004489.961372	44.328423
3507.539950	1004361.410971	44.333428
3507.138734	1004230.044495	44.338433
3507.263031	1004046.538638	44.343437
3506.977351	1003902.205961	44.348442
3507.239913	1003755.930703	44.353447
3507.433016	1003621.436061	44.358452
3507.098808	1003472.527443	44.363457
3507.137498	1003308.277023	44.368461
3506.897623	1003163.820649	44.373466
3507.292321	1003036.284843	44.378471
3507.484747	1002880.267777	44.383476
3506.992462	1002748.006067	44.388481
3507.176918	1002602.103091	44.393485
3506.923320	1002458.506793	44.398490
3507.300588	1002297.577363	44.403495
3507.236285	1002156.375217	44.408500
3507.210009	1002027.815480	44.413505
3507.062821	1001869.393366	44.418509
3507.092771	1001716.096126	44.423514
3507.210749	1001562.098909	44.428519
3507.300561	1001422.021049	44.433524
3507.010301	1001280.055574	44.438529
3507.378173	1001134.668591	44.443533
3507.170312	1000996.284001	44.448538
3507.152260	1000842.192266	44.453543
3507.165785	1000691.887689	44.458548
3506.804561	1000546.995092	44.463553
3507.284401	1000408.093462	44.468557
3507.068400	1000279.427913	44.473562
3507.189254	1000121.399507	44.478567
3507.065140	999967.885595	44.483572
3507.162681	999837.990059	44.488577
3507.127020	999701.103247	44.493581
3507.187629	999554.947416	44.498586
3507.139643	999386.410675	44.503591
3507.128563	999260.317210	44.508596
3507.002167	999118.757413	44.513601
3507.044155	998964.215202	44.518605
3506.890098	998814.570054	44.523610
3507.221298	998674.092340	44.528615
3507.171764	998551.689962	44.533620
3506.885382	998401.568782	44.538625
3507.113981	998231.588730	44.543629
3507.193114	998088.411111	44.548634
3507.193259	997964.916568	44.553639
3506.972099	997831.326548	44.558644
3507.056970	997666.710047	44.563649
3507.247248	997510.350593	44.568653
3506.919457	997382.124663	44.573658
3506.997852	997255.095218	44.578663
3507.164104	997107.690012	44.583668
3506.614065	996959.035187	44.588673
3507.209256	996801.225738	44.593677
3507.000008	996674.425495	44.598682
3506.833470	996521.799386	44.603687
3506.952749	996388.703824	44.608692
3506.544546	996266.311183	44.613697
3506.948466	996118.256589	44.618701
3506.833098	995975.349945	44.623706
3506.576280	995837.626834	44.628711
3506.756042	995712.884506	44.633716
3506.572969	995552.635273	44.638721
3506.470325	995428.030634	44.643725
3506.309537	995304.602115	44.648730
3506.789724	995173.659741	44.653735
3506.996664	995030.286449	44.658740
3506.710361	994910.767826	44.663745
3506.907962	994760.957785	44.668749
3506.505456	994627.322167	44.673754
3506.412914	994478.916794	44.678759
3506.570161	994361.165175	44.683764
3506.350921	994222.714494	44.688769
3506.543568	994083.023067	44.693773
3506.140091	993957.071238	44.698778
3506.359877	993839.980758	44.703783
3506.348010	993706.259120	44.708788
3506.139239	993578.414943	44.713793
3506.471432	993433.811092	44.718797
3506.304149	993324.474030	44.723802
3506.614771	993190.004812	44.728807
3506.403410	993053.668813	44.733812
3506.136553	992922.992574	44.738817
3506.529126	992783.626203	44.743821
3506.201284	992661.045085	44.748826
3506.275528	992541.612181	44.753831
3506.273874	992422.481738	44.758836
3505.978325	992287.896040	44.763841
3506.288276	992148.235231	44.768845
3505.858533	992044.766414	44.773850
3506.064809	991924.616333	44.778855
3506.188919	991795.312239	44.783860
3505.955390	991677.861885	44.788865
3506.006378	991541.056380	44.793869
3505.957511	991424.837944	44.798874
3506.027428	991308.695078	44.803879
3506.161156	991182.788272	44.808884
3505.777573	991081.927110	44.813889
3506.197572	990950.019746	44.818893
3505.918488	990822.515207	44.823898
3505.674235	990712.165396	44.828903
3505.815104	990596.678938	44.833908
3505.643150	990484.947520	44.838913
3505.851457	990347.014641	44.843917
3505.844992	990231.252459	44.848922
3505.929408	990118.301293	44.853927
3506.082236	990009.530444	44.858932
3506.045228	989892.010839	44.863937
3506.012486	989753.323012	44.868941
3505.835141	989658.254737	44.873946
3505.657797	989517.439167	44.878951
3505.510227	989398.171867	44.883956
3505.428538	989294.107951	44.888961
3505.835941	989187.815592	44.893965
3505.643503	989072.158009	44.898970
3505.466159	988941.473052	44.903975
3505.618763	988832.387103	44.908980
3505.140943	988721.061628	44.913985
3505.482639	988610.086773	44.918989
3505.563077	988507.737767	44.923994
3505.388980	988411.672568	44.928999
3505.589459	988297.690585	44.934004
3505.104974	988183.721573	44.939009
3505.531520	988090.576455	44.944013
3505.183822	987967.702290	44.949018
3505.181862	987861.452610	44.954023
3505.354625	987759.074946	44.959028
3505.118228	987664.275800	44.964033
3505.465587	987532.301231	44.969037
3505.257714	987432.517294	44.974042
3505.426834	987329.449489	44.979047
3505.416435	987225.531180	44.984052
3505.056758	987116.887069	44.989057
3505.351637	987016.720305	44.994061
3505.175326	986924.338498	44.999066
3505.270438	986810.539290	45.004071
3505.480984	986687.838328	45.009076
3505.482281	986583.516036	45.014081
3505.615104	986492.637748	45.019085
3505.365204	986392.159375	45.024090
3505.218561	986264.628494	45.029095
3505.322033	986159.403258	45.034100
3505.254921	986077.042184	45.039105
3505.266501	985967.924623	45.044109
3505.389855	985852.832848	45.049114
3505.062294	985744.547684	45.054119
3505.056110	985652.214839	45.059124
3505.137894	985555.668909	45.064129
3505.278319	985449.350809	45.069133
3505.180823	985336.237160	45.074138
3505.196249	985234.035286	45.079143
3505.494903	985150.038779	45.084148
3505.150842	985038.326427	45.089153
3505.537185	984919.170246	45.094157
3505.333898	984820.608850	45.099162
3505.145451	984713.940731	45.104167
3505.391591	984614.423158	45.109172
3505.554572	984518.041542	45.114177
3505.536925	984409.094222	45.119181
3504.829602	984300.453668	45.124186
3504.960384	984188.158310	45.129191
3504.961051	984102.438117	45.134196
3504.941289	983998.657796	45.139201
3505.215106	983898.049205	45.144205
3505.105460	983798.771281	45.149210
3504.995991	983700.858544	45.154215
3504.898120	983600.403564	45.159220
3504.840666	983498.182598	45.164225
3505.077834	983393.958397	45.169229
3504.513566	983308.416967	45.174234
3504.724534	983205.658326	45.179239
3504.986571	983117.341462	45.184244
3504.339536	983043.820480	45.189249
3504.957784	982940.892347	45.194253
3504.706563	982837.519642	45.199258
3504.923980	982741.001404	45.204263
3505.078450	982648.691147	45.209268
3504.931331	982565.999581	45.214273
3504.903637	982456.918991	45.219277
3504.846883	982370.303304	45.224282
3504.784946	982272.260571	45.229287
3504.777456	982167.858966	45.234292
3504.750537	982091.586619	45.239297
3504.807386	981995.570564	45.244301
3504.943228	981885.084768	45.249306
3504.459321	981799.995830	45.254311
3504.647182	981723.097160	45.259316
3504.385803	981640.020312	45.264321
3504.712463	981538.091686	45.269325
3504.342178	981441.941324	45.274330
3504.565538	981353.408209	45.279335
3504.605640	981240.288382	45.284340
3504.517303	981173.098200	45.289345
3504.546399	981084.495234	45.294349
3504.606528	980993.639027	45.299354
3504.666180	980920.169648	45.304359
3504.674843	980826.584044	45.309364
3504.277133	980740.292859	45.314369
3504.700716	980622.213167	45.319373
3504.593651	980549.743400	45.324378
3504.564217	980460.945022	45.329383
3504.868380	980381.664492	45.334388
3504.675218	980290.643438	45.339393
3504.852351	980194.381915	45.344397
3504.608799	980109.130491	45.349402
3504.647574	980002.923104	45.354407
3504.670947	979924.952617	45.359412
3504.455233	979845.554874	45.364417
3504.676570	979751.916649	45.369421
3504.584355	979660.868939	45.374426
3504.432668	979565.823487	45.379431
3504.644003	979493.874149	45.384436
3503.973629	979410.636817	45.389441
3504.418322	979312.850707	45.394445
3504.438395	979242.493129	45.399450
3504.187396	979159.378495	45.404455
3504.779503	979068.599513	45.409460
3504.148915	978979.974861	45.414465
3504.278834	978897.086835	45.419469
3504.396593	978836.871145	45.424474
3504.725489	978737.433005	45.429479
3504.977898	978634.292173	45.434484
3504.682161	978567.007788	45.439489
3504.664664	978451.301374	45.444493
3504.623178	978364.426993	45.449498
3504.681874	978276.068821	45.454503
3504.671136	978205.996766	45.459508
3504.486220	978105.752684	45.464513
3504.916451	978006.676099	45.469517
3504.689602	977925.201063	45.474522
3504.486224	977867.960195	45.479527
3504.427122	977758.110921	45.484532
3503.986667	977666.013664	45.489537
3504.370797	977570.455833	45.494541
3504.469026	977511.402338	45.499546
3504.166344	977415.759555	45.504551
3504.191680	977336.776003	45.509556
3504.102297	977258.103503	45.514561
3504.161639	977162.885612	45.519565
3504.354825	977098.826944	45.524570
3504.468741	977006.530013	45.529575
3504.561173	976936.327668	45.534580
3504.288869	976842.038854	45.539585
3504.073934	976758.199091	45.544589
3504.200702	976699.034760	45.549594
3504.193714	976607.924419	45.554599
3504.452104	976531.335373	45.559604
3504.010556	976446.452993	45.564609
3504.443902	976367.486635	45.569613
3504.500431	976286.332647	45.574618
3504.160445	976186.764847	45.579623
3504.273332	976105.501246	45.584628
3504.233638	976043.033425	45.589633
3503.986783	975954.298662	45.594637
3504.285966	975892.360011	45.599642
3503.718793	975807.977712	45.604647
3504.127297	975716.002561	45.609652
3504.085793	975652.357474	45.614657
3504.317514	975565.200057	45.619661
3503.685274	975493.143821	45.624666
3504.162264	975416.992774	45.629671
3504.401754	975344.204407	45.634676
3503.953894	975255.491921	45.639681
3504.034794	975167.473249	45.644685
3504.055184	975097.944731	45.649690
3503.933666	975033.328088	45.654695
3504.294662	974940.468240	45.659700
3504.548005	974882.633346	45.664705
3504.512968	974786.315808	45.669709
3504.103398	974698.077336	45.674714
3503.715583	974618.048618	45.679719
3503.889000	974547.999255	45.684724
3503.913470	974478.169161	45.689729
3503.918271	974379.980101	45.694733
3503.879798	974302.921182	45.699738
3503.768809	974251.105680	45.704743
3503.789514	974171.296837	45.709748
3503.879005	974109.471267	45.714753
3504.105393	974037.255283	45.719757
3503.819437	973963.655697	45.724762
3503.847988	973878.168783	45.729767
3503.924643	973812.918899	45.734772
3504.015996	973754.805889	45.739777
3503.969531	973680.380752	45.744781
3503.850614	973602.347565	45.749786
3504.207963	973528.734252	45.754791
3504.171165	973441.295338	45.759796
3504.116457	973377.724977	45.764801
3504.065904	973293.807421	45.769805
3504.037019	973234.241693	45.774810
3503.718023	973139.801791	45.779815
3503.993633	972971.113768	45.784820
3503.868672	972788.204305	45.789825
3504.137349	972541.146293	45.794829
3504.149516	972234.441093	45.799834
3504.035940	971828.431918	45.804839
3503.965543	971368.765704	45.809844
3503.393841	970877.928712	45.814849
3503.829825	970306.143677	45.819853
3503.778442	969668.020860	45.824858
3503.345808	968945.900384	45.829863
3503.892214	968163.023552	45.834868
3503.234958	967321.193923	45.839873
3503.437775	966398.891968	45.844877
3503.302609	965395.003084	45.849882
3503.199802	964323.139373	45.854887
3503.124392	963162.392182	45.859892
3502.726130	961941.580592	45.864897
3502.850850	960636.411451	45.869901
3502.698803	959263.432812	45.874906
3502.521812	957780.576719	45.879911
3502.614516	956209.293941	45.884916
3502.181017	954614.233626	45.889921
3502.019672	952924.736133	45.894925
3501.773029	951151.142346	45.899930
3501.025736	949307.892629	45.904935
3501.176676	947389.990995	45.909940
3500.960186	945386.163723	45.914945
3500.573599	943273.181059	45.919949
3500.569652	941103.851929	45.924954
3499.896561	938845.761711	45.929959
3499.812850	936489.570963	45.934964
3499.196073	934044.940388	45.939969
3499.016222	931519.855085	45.944973
3498.813217	928928.603660	45.949978
3497.969742	926253.889178	45.954983
3497.890595	923457.070615	45.959988
3497.320023	920590.444638	45.964993
3497.052023	917655.801493	45.969997
3496.965644	914628.294815	45.975002
3496.287209	911508.391238	45.980007
3495.949454	908306.501063	45.985012
3495.449149	905033.100339	45.990017
3494.884017	901644.014781	45.995021
3494.567199	898181.235365	46.000026
3494.075698	894665.021769	46.005031
3493.387325	891038.200002	46.010036
3492.718622	887344.408586	46.015041
3492.397655	883536.683027	46.020045
3491.941138	879674.725335	46.025050
3491.128023	875715.892220	46.030055
3490.729499	871679.982939	46.035060
3489.885115	867547.575580	46.040065
3489.422139	863317.485629	46.045069
3488.993378	859037.267514	46.050074
3488.000791	854657.093604	46.055079
3487.602799	850162.560119	46.060084
3486.917131	845615.414697	46.065089
3486.326849	840991.120022	46.070093
3486.020258	836284.238640	46.075098
3485.125316	831464.036805	46.080103
3484.034468	826539.770428	46.085108
3483.536720	821569.639453	46.090113
3483.010547	816498.350021	46.095117
3482.258408	811344.714805	46.100122
3481.363767	806103.771859	46.105127
3480.715011	800755.230384	46.110132
3479.444028	795358.274416	46.115137
3479.087186	789861.909129	46.120141
3478.101299	784253.372374	46.125146
3477.165763	778589.607568	46.130151
3476.832135	772806.743462	46.135156
3475.330896	766942.282112	46.140161
3475.085037	761000.286269	46.145165
3473.658909	754986.820754	46.150170
3472.468341	748872.933744	46.155175
3471.889977	742670.320457	46.160180
3470.883687	736388.275983	46.165185
3469.505789	730012.362784	46.170189
3468.698464	723537.971276	46.175194
3467.557764	717001.575633	46.180199
3466.925161	710368.612078	46.185204
3465.344611	703632.822531	46.190209
3464.470696	696828.007147	46.195213
3463.584589	689932.218319	46.200218
3462.211076	682940.939306	46.205223
3461.204304	675858.348456	46.210228
3459.814053	668715.747301	46.215233
3458.257540	661484.962032	46.220237
3457.434133	654175.250186	46.225242
3456.419837	646753.950981	46.230247
3455.167829	639246.362419	46.235252
3453.639717	631676.758975	46.240257
3452.778562	624021.322796	46.245261
3451.219518	616265.579961	46.250266
3449.492128	608427.225993	46.255271
3447.976672	600517.709568	46.260276
3446.628064	592513.311949	46.265281
3445.216154	584449.217547	46.270285
3443.776138	576303.105803	46.275290
3442.011069	568073.099237	46.280295
3440.590155	559725.877408	46.285300
3439.037602	551341.656094	46.290305
3437.385323	542869.171240	46.295309
3435.855368	534308.943647	46.300314
3433.733468	525660.344308	46.305319
3432.470621	516958.117201	46.310324
3430.292841	508200.362640	46.315329
3428.324139	499321.323382	46.320333
3427.136693	490371.704945	46.325338
3425.021710	481382.246066	46.330343
3423.264032	472307.117686	46.335348
3421.258091	463146.234115	46.340353
3419.272351	453913.825319	46.345357
3417.606470	444610.047703	46.350362
3415.220824	435227.166706	46.355367
3412.858827	425773.801486	46.360372
3410.841406	416275.854391	46.365377
3408.583974	406704.933222	46.370381
3406.449199	397047.169934	46.375386
3403.918650	387356.930619	46.380391
3401.833706	377569.385014	46.385396
3399.198125	367768.622262	46.390401
3396.971600	357901.462323	46.395405
3394.334079	347937.364237	46.400410
3391.994910	337934.925563	46.405415
3389.742005	327888.422918	46.410420
3386.994281	317791.457066	46.415425
3384.140012	307636.657068	46.420429
3381.125650	297424.546477	46.425434
3378.134013	287154.294230	46.430439
3375.657946	276836.639724	46.435444
3372.800538	266518.038479	46.440449
3369.814275	256121.421366	46.445453
3366.423175	245678.815655	46.450458
3363.040229	235217.989703	46.455463
3360.273400	224698.179913	46.460468
3356.505726	214109.232629	46.465473
3353.400794	203537.196271	46.470477
3349.332099	192936.461274	46.475482
3345.466135	182327.131965	46.480487
3341.598494	171701.551299	46.485492
3337.721908	161104.108659	46.490497
3334.048111	150453.297604	46.495501
3329.904159	139794.264033	46.500506
3325.013676	129146.434276	46.505511
3320.095727	118505.342642	46.510516
3315.412648	107889.028110	46.515521
3309.972359	97265.242647	46.520525
3304.754081	86674.865281	46.525530
3298.461350	76144.613353	46.530535
3292.265625	65669.524285	46.535540
3284.500981	55256.214362	46.540545
3275.126709	44956.473013	46.545549
3254.231159	35089.514471	46.550554
3227.067048	25603.295596	46.555559
3197.341542	16560.827480	46.560564
3151.485028	8466.067414	46.565569
3077.966148	1811.172557	46.570573
2855.378918	386.146131	46.575578
2674.076210	381.502394	46.580583
2615.917528	335.628754	46.585588
2653.432100	340.652891	46.590593
2738.156632	341.701785	46.595597
2825.177834	335.513171	46.600602
2886.939712	348.768699	46.605607
2917.702227	316.574578	46.610612
2922.256989	312.934758	46.615617
2912.916158	311.971955	46.620621
2898.405879	315.240616	46.625626
2885.794703	342.858236	46.630631
2877.894596	319.823415	46.635636
2873.924681	312.900858	46.640641
2872.132314	286.212339	46.645645
2870.985028	300.408414	46.650650
2869.621516	318.721637	46.655655
2867.983877	317.695721	46.660660
2865.914727	300.765794	46.665665
2863.037101	284.475440	46.670669
2860.040635	289.729707	46.675674
2857.028210	307.387127	46.680679
2853.645125	289.260844	46.685684
2850.337041	290.354883	46.690689
2846.972339	295.844177	46.695693
2844.284919	296.757473	46.700698
2841.403461	293.745576	46.705703
2838.834809	277.770894	46.710708
2835.118588	289.852766	46.715713
2831.298513	299.379250	46.720717
2828.725226	286.090606	46.725722
2825.294448	292.950305	46.730727
2821.962180	295.886701	46.735732
2818.878508	291.922923	46.740737
2815.638349	304.603471	46.745741
2812.342470	278.136915	46.750746
2808.727141	279.790166	46.755751
2805.734357	282.698124	46.760756
2802.349509	286.144834	46.765761
2798.884062	286.210555	46.770765
2795.678887	265.703371	46.775770
2791.891208	276.986910	46.780775
2788.851373	273.213027	46.785780
2785.568655	290.949333	46.790785
2782.281008	279.082354	46.795789
2779.344743	264.150883	46.800794
2775.152106	266.482842	46.805799
2771.573466	274.938533	46.810804
2768.844049	284.465755	46.815809
2765.189277	267.794360	46.820813
2762.238493	259.200541	46.825818
2758.893167	273.365253	46.830823
2755.198081	285.780457	46.835828
2751.539989	272.589518	46.840833
2747.851105	261.710611	46.845837
2745.327868	267.731930	46.850842
2741.414236	268.593295	46.855847
2738.198806	255.843960	46.860852
2734.234961	274.612865	46.865857
2730.705783	287.954087	46.870861
2727.772976	266.392646	46.875866
2724.398835	255.545128	46.880871
2720.930064	260.517816	46.885876
2717.374645	277.091994	46.890881
2714.275494	274.973711	46.895885
2711.117278	255.866102	46.900890
2707.278488	250.866652	46.905895
2703.909676	258.931934	46.910900
2700.196396	267.521123	46.915905
2696.597924	255.767014	46.920909
2693.289739	258.452167	46.925914
2689.298938	263.444150	46.930919
2686.381674	259.519691	46.935924
2682.558714	253.427655	46.940929
2679.063031	251.113936	46.945933
2675.721513	264.306328	46.950938
2672.430822	248.656492	46.955943
2669.188854	239.616006	46.960948
2665.942220	242.432780	46.965953
2662.242868	243.038470	46.970957
2659.176792	254.104317	46.975962
2655.693973	247.868023	46.980967
2652.026730	227.120598	46.985972
2648.169866	239.883781	46.990977
2644.695979	244.576579	46.995981
2641.890916	243.302135	47.000986
2637.689437	240.100055	47.005991
2634.390932	234.776190	47.010996
2631.089706	250.604090	47.016001
2627.868807	245.971792	47.021005
2624.428354	230.397797	47.026010
2620.582832	230.389044	47.031015
2617.386902	237.801483	47.036020
2613.385158	232.523834	47.041025
2609.798925	242.327692	47.046029
2606.692352	245.762228	47.051034
2603.576587	241.155620	47.056039
2599.764333	234.336103	47.061044
2596.486547	247.002646	47.066049
2592.470055	229.323257	47.071053
2589.359661	226.658098	47.076058
2585.822287	227.061715	47.081063
2582.596243	226.852879	47.086068
2578.880462	238.196923	47.091073
2575.108096	221.934268	47.096077
2572.005684	232.080974	47.101082
2568.128219	247.317296	47.106087
2565.137664	236.200946	47.111092
2561.740843	222.448483	47.116097
2558.131794	247.474982	47.121101
2554.827153	220.081955	47.126106
2550.920709	238.838646	47.131111
2547.583270	234.269505	47.136116
2543.896583	226.877568	47.141121
2540.449761	242.390134	47.146125
2537.213811	223.360305	47.151130
2533.737798	230.379663	47.156135
2530.018757	239.607035	47.161140
2526.826778	234.915958	47.166145
2523.294171	233.268079	47.171149
2519.750422	243.660318	47.176154
2516.057959	235.878295	47.181159
2512.566646	230.051896	47.186164
2509.395937	233.356761	47.191169
2505.457754	249.775871	47.196173
2502.290727	226.215825	47.201178
2498.754192	232.511319	47.206183
2495.716149	214.656665	47.211188
2492.269549	215.608550	47.216193
2488.568550	236.964547	47.221197
2485.146646	228.801238	47.226202
2480.734490	221.638173	47.231207
2477.270517	213.931856	47.236212
2474.358975	216.246757	47.241217
2470.729463	214.131106	47.246221
2467.576171	207.174505	47.251226
2463.876499	232.757334	47.256231
2460.231049	238.980047	47.261236
2457.183768	219.464976	47.266241
2453.549223	215.109428	47.271245
2450.101767	215.448067	47.276250
2446.209807	224.600198	47.281255
2443.079007	213.904909	47.286260
2439.680494	217.791812	47.291265
2435.969257	223.908479	47.296269
2432.451546	219.515522	47.301274
2428.692982	233.829921	47.306279
2425.676391	224.137321	47.311284
2421.812821	210.875561	47.316289
2418.335977	201.238458	47.321293
2415.467787	213.737451	47.326298
2411.817641	215.456104	47.331303
2408.141651	211.263677	47.336308
2404.654956	216.934717	47.341313
2400.773521	222.004773	47.346317
2397.527480	206.687138	47.351322
2393.936342	206.720204	47.356327
2390.423926	218.166212	47.361332
2387.193800	217.783719	47.366337
2383.496344	222.961947	47.371341
2380.130879	213.944656	47.376346
2376.694186	206.407028	47.381351
2372.925623	198.293665	47.386356
2369.819634	208.118421	47.391361
2366.168765	229.923019	47.396365
2362.673858	223.716702	47.401370
2358.923849	207.749626	47.406375
2355.532406	193.513535	47.411380
2352.099420	204.112659	47.416385
2348.443702	227.065058	47.421389
2345.154350	207.034200	47.426394
2341.767633	214.667198	47.431399
2338.469472	225.400564	47.436404
2334.891221	202.197037	47.441409
2330.935140	223.571151	47.446413
2327.868623	198.595242	47.451418
2323.884390	211.459630	47.456423
2320.488661	206.136969	47.461428
2317.055531	202.870913	47.466433
2313.610787	214.464215	47.471437
2310.501678	200.477926	47.476442
2306.877792	210.978632	47.481447
2303.207681	212.483597	47.486452
2299.980674	197.676462	47.491457
2295.650973	203.012066	47.496461
2292.699139	207.845101	47.501466
2288.778784	210.984242	47.506471
2285.392472	192.036725	47.511476
2282.019501	201.837468	47.516481
2278.710022	213.509884	47.521485
2275.518881	207.300183	47.526490
2271.745538	210.648195	47.531495
2268.635616	203.158047	47.536500
2264.689697	202.916350	47.541505
2261.198961	195.447978	47.546509
2258.142778	197.692600	47.551514
2254.417495	190.682078	47.556519
2250.659709	182.349003	47.561524
2246.927378	194.009375	47.566529
2243.350863	217.553544	47.571533
2240.167028	208.227889	47.576538
2236.750472	198.424489	47.581543
2232.825093	207.312996	47.586548
2230.102697	205.216842	47.591553
2225.914686	213.436717	47.596557
2222.814654	194.747833	47.601562
2219.280199	187.697476	47.606567
2215.492439	190.587984	47.611572
2212.241004	195.562695	47.616577
2208.738339	206.240840	47.621581
2205.707920	188.987782	47.626586
2202.095767	202.980159	47.631591
2198.356260	200.981143	47.636596
2194.952033	192.907629	47.641601
2191.278462	192.310700	47.646605
2187.860300	179.061681	47.651610
2184.250773	180.421657	47.656615
2180.502509	203.393271	47.661620
2177.219145	204.984750	47.666625
2173.560150	187.118110	47.671629
2170.164449	168.876505	47.676634
2166.429294	189.677333	47.681639
2163.265713	210.281023	47.686644
2159.730936	206.845459	47.691649
2156.460135	199.054487	47.696653
2153.024868	175.136806	47.701658
2148.941323	191.787513	47.706663
2145.402925	214.747524	47.711668
2142.533634	199.174060	47.716673
2139.003497	208.790655	47.721677
2135.164515	186.259590	47.726682
2131.413316	184.288386	47.731687
2128.166997	200.548078	47.736692
2124.640856	194.861805	47.741697
2121.304348	181.865116	47.746701
2118.073731	205.602906	47.751706
2114.588959	197.024021	47.756711
2110.820874	191.316699	47.761716
2107.134839	184.598701	47.766721
2103.203616	197.180372	47.771725
2100.140967	200.497750	47.776730
2096.584353	195.557179	47.781735
2093.093421	191.628969	47.786740
2089.662224	178.646539	47.791745
2086.261099	191.483086	47.796749
2082.879037	174.318802	47.801754
2079.552734	182.278409	47.806759
2075.907898	201.649453	47.811764
2072.377832	190.648626	47.816769
2068.673516	194.765168	47.821773
2065.215947	185.978315	47.826778
2061.312314	181.213980	47.831783
2058.122558	179.325898	47.836788
2055.023280	182.539832	47.841793
2051.243712	195.098382	47.846797
2047.570705	190.053924	47.851802
2044.257793	190.218041	47.856807
2040.546117	184.985530	47.861812
2037.584928	189.752221	47.866817
2033.493447	203.681079	47.871821
2030.026403	194.651449	47.876826
2026.939049	198.489459	47.881831
2023.222710	188.062948	47.886836
2020.187340	176.653044	47.891841
2016.226745	193.303051	47.896845
2012.748732	193.851924	47.901850
2008.781329	176.278372	47.906855
2005.377444	172.578629	47.911860
2002.436522	181.461084	47.916865
1998.651738	194.841568	47.921869
1995.468957	185.275279	47.926874
1991.957700	172.038190	47.931879
1988.211051	178.229632	47.936884
1984.896433	192.102653	47.941889
1980.924820	183.332286	47.946893
1977.408496	163.511017	47.951898
1974.196682	193.462482	47.956903
1970.436015	186.038904	47.961908
1967.362858	168.178577	47.966913
1964.103333	178.742792	47.971917
1960.405793	191.426144	47.976922
1956.957840	188.306845	47.981927
1953.475657	171.644913	47.986932
1949.853760	163.626498	47.991937
1946.260393	192.647711	47.996941
1942.350291	191.885231	48.001946
1938.564825	177.956890	48.006951
1935.509681	165.290256	48.011956
1932.524466	179.299827	48.016961
1928.988046	193.268056	48.021965
1925.620021	183.699908	48.026970
1921.312223	176.797820	48.031975
1917.793027	161.170151	48.036980
1914.699061	182.935900	48.041985
1911.087944	199.287890	48.046989
1907.528503	189.107444	48.051994
1904.324444	174.866480	48.056999
1900.594138	176.563278	48.062004
1897.465328	162.500407	48.067009
1893.754836	171.671142	48.072013
1890.321057	175.953547	48.077018
1886.517210	184.609356	48.082023
1883.010579	197.115543	48.087028
1879.750081	180.904996	48.092033
1876.153800	189.868486	48.097037
1872.830190	187.459605	48.102042
1869.277316	177.863984	48.107047
1865.792496	164.082120	48.112052
1862.162281	164.221724	48.117057
1858.451513	183.500498	48.122061
1855.349971	179.660388	48.127066
1851.760434	165.334890	48.132071
1848.130821	179.003917	48.137076
1844.564714	183.428232	48.142081
1841.101320	178.709182	48.147085
1837.550815	170.942542	48.152090
1834.149290	197.170750	48.157095
1830.791432	195.054016	48.162100
1827.326989	171.792278	48.167105
1823.620656	164.061716	48.172109
1820.297285	178.940566	48.177114
1816.577069	183.533656	48.182119
1813.019058	172.887715	48.187124
1809.820462	170.579482	48.192129
1806.386967	183.951989	48.197133
1802.696874	174.168532	48.202138
1799.308664	169.424673	48.207143
1795.968471	181.961325	48.212148
1792.212121	178.794540	48.217153
1788.417389	184.494843	48.222157
1784.868380	182.232301	48.227162
1781.592849	162.291930	48.232167
1778.060174	151.196841	48.237172
1774.678273	169.600506	48.242177
1771.064769	169.869193	48.247181
1767.561438	174.293244	48.252186
1764.191726	187.693126	48.257191
1760.394916	183.502250	48.262196
1757.014207	155.028564	48.267201
1753.723808	173.320959	48.272205
1750.302873	186.014485	48.277210
1746.756838	173.934125	48.282215
1742.912744	176.650570	48.287220
1739.502732	174.815550	48.292225
1735.961685	173.949280	48.297229
1732.751384	169.427261	48.302234
1729.616776	183.366934	48.307239
1725.953041	182.725510	48.312244
1722.446682	169.730558	48.317249
1718.598176	155.626539	48.322253
1715.307774	151.375719	48.327258
1711.361242	168.544358	48.332263
1707.819747	183.300313	48.337268
1704.383592	174.280288	48.342273
1700.785538	163.690748	48.347277
1697.806376	167.902463	48.352282
1694.231780	192.257495	48.357287
1690.540376	161.807187	48.362292
1687.059786	161.109324	48.367297
1683.277161	160.704173	48.372301
1680.095765	175.164251	48.377306
1676.581249	192.541313	48.382311
1673.003745	183.162359	48.387316
1669.414701	157.343426	48.392321
1665.901975	156.958069	48.397325
1662.430519	169.259927	48.402330
1659.047690	180.066946	48.407335
1655.736584	160.838661	48.412340
1652.452148	164.750759	48.417345
1648.528934	171.182201	48.422349
1644.998996	154.712056	48.427354
1641.675272	177.002593	48.432359
1637.796953	191.875519	48.437364
1634.650491	170.933664	48.442369
1630.937119	159.646712	48.447373
1627.447756	170.058371	48.452378
1623.605271	189.627975	48.457383
1620.157166	184.256915	48.462388
1617.232291	159.103211	48.467393
1613.505217	163.272051	48.472397
1610.179304	186.483658	48.477402
1606.608692	193.190574	48.482407
1602.983373	172.656158	48.487412
1599.539987	158.049045	48.492417
1595.780237	177.696437	48.497421
1592.507161	182.361452	48.502426
1589.028157	181.537794	48.507431
1584.927087	171.442101	48.512436
1582.110899	178.582582	48.517441
1578.755948	180.000377	48.522445
1574.876866	173.117153	48.527450
1571.528474	179.347237	48.532455
1567.896928	163.027177	48.537460
1564.658594	161.955669	48.542465
1560.992821	175.984616	48.547469
1557.497836	183.166098	48.552474
1554.138076	179.907661	48.557479
1550.164861	166.634037	48.562484
1547.106655	165.385331	48.567489
1543.237700	183.390907	48.572493
1539.907335	181.242850	48.577498
1536.643193	162.737979	48.582503
1532.740876	172.885377	48.587508
1529.572427	172.519528	48.592513
1525.815538	161.781208	48.597517
1522.198603	168.471132	48.602522
1518.874571	188.499258	48.607527
1515.319869	173.420368	48.612532
1512.182655	151.772152	48.617537
1508.606791	168.515287	48.622541
1505.124983	180.990271	48.627546
1501.655811	176.233194	48.632551
1498.049059	177.208314	48.637556
1494.508764	146.844935	48.642561
1490.851832	166.103178	48.647565
1487.239816	176.791524	48.652570
1483.901735	166.589912	48.657575
1480.303451	156.118240	48.662580
1476.816806	165.268580	48.667585
1473.506154	173.129447	48.672589
1469.573662	167.262013	48.677594
1466.466401	154.805495	48.682599
1462.779869	172.446859	48.687604
1459.486008	169.111897	48.692609
1456.045429	171.576532	48.697613
1452.174717	155.197384	48.702618
1448.995127	149.288480	48.707623
1445.284255	159.687138	48.712628
1442.022247	169.704336	48.717633
1438.225914	164.272279	48.722637
1434.981760	179.405215	48.727642
1431.399663	176.331805	48.732647
1427.799560	176.568958	48.737652
1424.089009	150.095725	48.742657
1420.792694	166.932535	48.747661
1417.391977	159.162732	48.752666
1413.731856	160.085737	48.757671
1410.114371	182.362668	48.762676
1406.791109	166.251184	48.767681
1403.551680	165.257273	48.772685
1400.306973	168.161245	48.777690
1396.811056	178.964826	48.782695
1392.911923	176.783360	48.787700
1389.450557	158.965872	48.792705
1385.411753	151.178687	48.797709
1381.895352	162.781539	48.802714
1378.620524	154.348091	48.807719
1375.697093	158.243635	48.812724
1371.994611	169.889341	48.817729
1368.064676	172.846446	48.822733
1364.527199	144.118802	48.827738
1361.380494	146.843941	48.832743
1357.682432	167.374575	48.837748
1354.445318	174.276326	48.842753
1350.953152	158.285888	48.847757
1347.526962	150.224587	48.852762
1344.008928	152.703832	48.857767
1340.210442	177.176870	48.862772
1337.013753	162.506317	48.867777
1333.159106	155.178854	48.872781
1329.612617	159.343574	48.877786
1326.007106	156.536199	48.882791
1322.725374	158.341650	48.887796
1319.484820	146.702036	48.892801
1315.717919	147.603059	48.897805
1312.291908	147.775432	48.902810
1308.570030	161.332711	48.907815
1304.815484	174.765771	48.912820
1301.925324	165.561262	48.917825
1298.229997	146.133759	48.922829
1294.917375	165.656628	48.927834
1291.882718	161.409482	48.932839
1287.833888	156.693951	48.937844
1284.500091	148.318433	48.942849
1280.417814	159.449372	48.947853
1277.106111	162.144568	48.952858
1273.576480	151.379465	48.957863
1269.591071	151.135563	48.962868
1266.738419	153.390978	48.967873
1263.441548	160.630135	48.972877
1259.916804	146.892654	48.977882
1256.684630	150.512381	48.982887
1252.368281	169.368256	48.987892
1249.152984	157.840022	48.992897
1245.859882	146.101797	48.997901
1242.038984	159.805267	49.002906
1239.165349	156.949144	49.007911
1235.012368	154.974814	49.012916
1231.609238	167.469158	49.017921
1228.269638	163.685420	49.022925
1224.474988	147.276628	49.027930
1221.280528	140.496870	49.032935
1217.428738	158.925959	49.037940
1214.027857	158.142671	49.042945
1210.435832	142.857887	49.047949
1207.061131	156.179931	49.052954
1203.896336	153.829221	49.057959
1200.284387	173.868438	49.062964
1196.953475	143.331757	49.067969
1193.071591	150.565209	49.072973
1189.306158	154.485383	49.077978
1186.117483	158.713823	49.082983
1182.465055	164.869460	49.087988
1179.542745	143.768132	49.092993
1175.823750	150.540948	49.097997
1172.070813	156.183438	49.103002
1168.472498	147.130437	49.108007
1165.021133	163.218131	49.113012
1161.901912	151.809636	49.118017
1158.109253	139.196358	49.123021
1154.530772	150.697768	49.128026
1151.028313	159.132095	49.133031
1147.515927	140.418123	49.138036
1143.883508	162.001801	49.143041
1140.224541	156.460243	49.148045
1136.862609	142.073501	49.153050
1133.913043	143.550651	49.158055
1130.012700	155.666515	49.163060
1126.870639	153.266416	49.168065
1123.288877	148.739645	49.173069
1119.817398	141.878317	49.178074
1116.058617	149.240641	49.183079
1112.463540	141.262901	49.188084
1109.020789	143.127387	49.193089
1105.386539	144.474906	49.198093
1101.948420	146.362010	49.203098
1098.464972	137.929828	49.208103
1094.658289	141.948106	49.213108
1091.796246	139.845390	49.218113
1088.152856	157.103300	49.223117
1084.634392	131.322746	49.228122
1081.304128	128.024382	49.233127
1077.634069	142.129752	49.238132
1074.145508	161.057180	49.243137
1070.454750	156.836582	49.248141
1067.107679	150.793941	49.253146
1063.834606	133.594038	49.258151
1059.966827	139.446322	49.263156
1056.340966	147.689160	49.268161
1053.130602	138.806872	49.273165
1049.451754	127.248869	49.278170
1045.990766	132.802966	49.283175
1042.556658	154.464804	49.288180
1038.925329	136.655128	49.293185
1035.290072	137.044189	49.298189
1031.860953	131.291139	49.303194
1028.437669	126.039247	49.308199
1025.052132	129.505246	49.313204
1021.646326	140.154878	49.318209
1018.108881	141.288080	49.323213
1014.516921	127.021681	49.328218
1011.201624	139.843890	49.333223
1007.273454	144.774838	49.338228
1004.018108	124.331869	49.343233
1000.637606	136.462275	49.348237
997.122138	129.195742	49.353242
993.353170	146.532807	49.358247
989.951437	149.524635	49.363252
986.333126	136.929945	49.368257
982.966570	144.026132	49.373261
979.241699	135.491732	49.378266
975.954382	118.809297	49.383271
972.262357	133.511102	49.388276
968.510629	140.308258	49.393281
965.491517	149.869417	49.398285
961.974079	137.975455	49.403290
958.843162	125.298151	49.408295
954.922753	139.590308	49.413300
951.523092	152.774113	49.418305
948.135972	138.379522	49.423309
944.325168	137.155623	49.428314
941.072362	127.962668	49.433319
937.324632	144.322492	49.438324
933.917026	139.778028	49.443329
930.537256	135.482398	49.448333
927.009440	149.204480	49.453338
923.785959	145.053312	49.458343
919.505853	140.815883	49.463348
916.432398	127.341511	49.468353
912.708001	145.437442	49.473357
908.965141	150.512255	49.478362
905.963721	133.686265	49.483367
902.367012	137.069799	49.488372
899.083283	145.072829	49.493377
895.526517	143.872218	49.498381
891.727263	138.113674	49.503386
888.718613	128.995655	49.508391
884.910796	130.815271	49.513396
881.120187	149.398323	49.518401
877.720800	129.797898	49.523405
874.292311	133.034305	49.528410
870.687316	132.772217	49.533415
866.972380	138.317129	49.538420
864.024445	143.659143	49.543425
860.384532	142.033199	49.548429
857.263289	143.290812	49.553434
854.133699	135.124901	49.558439
850.318928	129.028220	49.563444
846.422130	116.980559	49.568449
842.429020	138.614286	49.573453
838.953575	150.948660	49.578458
835.617438	132.914209	49.583463
832.066305	124.966388	49.588468
828.690570	120.416135	49.593473
825.506698	138.122649	49.598477
821.800839	149.820523	49.603482
818.220962	131.754223	49.608487
814.637250	127.154862	49.613492
811.036257	138.896874	49.618497
807.984368	141.374772	49.623501
804.400633	137.608695	49.628506
800.955297	133.390847	49.633511
797.073668	144.963863	49.638516
793.760102	134.387427	49.643521
790.203271	120.632007	49.648525
786.793878	131.388560	49.653530
783.306927	149.985429	49.658535
779.664762	147.732305	49.663540
776.579475	130.067539	49.668545
772.874173	137.031729	49.673549
769.386378	136.945466	49.678554
765.831545	126.530922	49.683559
761.901323	141.502000	49.688564
758.223240	129.357704	49.693569
755.166795	132.591918	49.698573
751.707406	135.250973	49.703578
748.592424	129.955132	49.708583
744.916184	141.597733	49.713588
741.492932	140.672482	49.718593
737.838730	124.924905	49.723597
734.062969	137.527309	49.728602
730.837302	140.136827	49.733607
726.997044	135.178090	49.738612
723.707076	126.639614	49.743617
720.168664	122.113227	49.748621
716.752524	124.783208	49.753626
712.849530	126.797780	49.758631
709.452589	133.321318	49.763636
705.969307	139.064711	49.768641
702.735671	142.182706	49.773645
699.467558	139.723041	49.778650
696.405039	129.014257	49.783655
692.380277	121.006242	49.788660
689.060670	132.061607	49.793665
685.188304	152.764855	49.798669
681.346812	139.010336	49.803674
678.187306	121.924139	49.808679
674.655781	122.156776	49.813684
671.180772	140.955898	49.818689
667.741004	148.643275	49.823693
664.031239	133.788899	49.828698
660.503081	122.780996	49.833703
656.981797	129.529095	49.838708
653.601505	134.124409	49.843713
650.347223	142.734486	49.848717
646.366413	140.946756	49.853722
643.385035	122.888289	49.858727
639.790691	142.403188	49.863732
636.156004	143.299221	49.868737
632.809929	142.842878	49.873741
629.047482	130.052356	49.878746
625.627858	133.492506	49.883751
621.932602	136.819852	49.888756
618.821922	122.430840	49.893761
615.421421	138.567116	49.898765
611.570001	127.283543	49.903770
608.072156	137.854922	49.908775
604.378159	137.115525	49.913780
600.830288	124.145366	49.918785
597.587490	137.371151	49.923789
593.772113	141.971175	49.928794
590.648576	125.546146	49.933799
587.129610	136.535438	49.938804
583.966291	136.645161	49.943809
580.390502	120.604100	49.948813
576.477241	123.891023	49.953818
572.725598	127.360979	49.958823
569.305351	140.958095	49.963828
566.032636	122.502307	49.968833
562.466887	114.571180	49.973837
558.801709	130.299772	49.978842
555.835715	112.537835	49.983847
552.399306	118.110880	49.988852
548.811631	140.139126	49.993857
544.648826	128.349673	49.998861
541.140600	127.202403	50.003866
538.311292	114.022066	50.008871
534.747328	120.437229	50.013876
531.039013	116.356099	50.018881
527.848400	118.187412	50.023885
524.155634	137.883539	50.028890
520.690736	129.243564	50.033895
516.707245	124.968179	50.038900
513.543136	129.185050	50.043905
509.916347	111.547382	50.048909
506.367522	137.569956	50.053914
503.092979	119.368732	50.058919
499.593718	136.836424	50.063924
495.863721	144.478592	50.068929
492.384526	112.538933	50.073933
488.734834	118.101761	50.078938
485.506320	116.220749	50.083943
481.857619	141.968233	50.088948
478.421150	134.956101	50.093953
475.354321	124.364762	50.098957
471.371178	121.146355	50.103962
467.948988	132.704786	50.108967
464.412103	137.130339	50.113972
461.123418	126.506896	50.118977
457.366952	112.078572	50.123981
453.768016	119.865715	50.128986
450.693023	127.594826	50.133991
447.269969	139.480231	50.138996
443.660136	113.643700	50.144001
439.770776	106.221862	50.149005
435.724831	127.169976	50.154010
432.828285	126.395724	50.159015
429.491474	128.105137	50.164020
426.038241	125.332413	50.169025
422.776362	113.642638	50.174029
419.268750	114.193841	50.179034
415.536074	136.690876	50.184039
411.448293	120.995532	50.189044
408.433207	127.975896	50.194049
405.085701	137.477457	50.199053
401.112458	125.722897	50.204058
398.092251	110.310917	50.209063
394.715607	121.031730	50.214068
390.736861	123.744499	50.219073
387.282673	108.386462	50.224077
383.663053	119.307225	50.229082
380.304036	134.650112	50.234087
376.560747	140.557849	50.239092
373.016773	129.905408	50.244097
369.887568	129.895859	50.249101
366.407990	120.022067	50.254106
363.070774	107.965876	50.259111
359.348125	130.236743	50.264116
355.798560	125.072588	50.269121
352.496650	127.552331	50.274125
348.686834	129.521238	50.279130
345.391068	114.893972	50.284135
341.528502	107.862460	50.289140
338.374454	128.274603	50.294145
335.191818	128.701435	50.299149
331.169679	131.378694	50.304154
327.916888	114.254883	50.309159
323.998338	113.414443	50.314164
321.011938	129.669830	50.319169
317.842187	127.548066	50.324173
313.917092	126.730119	50.329178
310.357009	133.326166	50.334183
306.663477	124.728441	50.339188
302.893448	120.128503	50.344193
299.591166	127.753369	50.349197
296.171703	123.701803	50.354202
292.793495	101.733478	50.359207
289.391054	133.547648	50.364212
285.612351	143.626954	50.369217
282.396662	122.968327	50.374221
278.781857	109.454078	50.379226
275.330376	111.180538	50.384231
271.801658	127.311470	50.389236
268.028089	118.998967	50.394241
265.061149	111.881487	50.399245
260.861601	122.811801	50.404250
257.914515	117.322960	50.409255
254.392896	107.718793	50.414260
250.818804	121.574238	50.419265
247.218407	127.242097	50.424269
243.563345	131.056830	50.429274
240.087660	107.659660	50.434279
236.723370	116.043324	50.439284
233.188692	121.770172	50.444289
230.043231	114.264534	50.449293
226.152432	109.005714	50.454298
222.567885	109.040691	50.459303
219.240016	114.909163	50.464308
215.844573	98.173714	50.469313
212.474352	112.907967	50.474317
208.781273	133.703179	50.479322
205.345553	117.048454	50.484327
201.589602	119.616210	50.489332
198.124267	123.581918	50.494337
194.736695	109.633525	50.499341
191.175041	126.681721	50.504346
188.054607	110.098529	50.509351
183.997729	121.231212	50.514356
180.514568	116.923894	50.519361
177.620973	109.094543	50.524365
173.523631	117.623227	50.529370
169.983337	124.725581	50.534375
166.456368	106.153678	50.539380
163.156560	115.457255	50.544385
160.063027	124.937565	50.549389
155.995015	120.208405	50.554394
152.606190	133.575075	50.559399
149.045177	125.238478	50.564404
145.621413	121.079890	50.569409
142.209646	111.000317	50.574413
138.532342	114.828544	50.579418
135.199974	114.968886	50.584423
131.533703	125.492528	50.589428
128.002298	105.578976	50.594433
124.820315	107.913361	50.599437
121.079394	127.486771	50.604442
117.747838	108.370636	50.609447
114.178331	118.646473	50.614452
110.659098	128.318184	50.619457
106.896901	110.420870	50.624461
103.720729	122.612646	50.629466
100.558780	120.697259	50.634471
96.759650	112.743440	50.639476
92.808856	105.177289	50.644481
89.405535	125.309320	50.649485
86.034679	118.730011	50.654490
82.871354	108.210770	50.659495
78.894172	113.945802	50.664500
75.519666	111.936918	50.669505
72.261394	92.461096	50.674509
68.540452	115.635461	50.679514
64.889600	122.873843	50.684519
61.480205	108.943427	50.689524
57.838169	92.505229	50.694529
54.432973	101.196005	50.699533
51.006252	127.579704	50.704538
47.829035	110.016931	50.709543
44.196897	118.657625	50.714548
40.744824	120.168270	50.719553
37.406912	98.059428	50.724557
33.223069	113.976120	50.729562
29.914648	99.819252	50.734567
26.339649	104.913729	50.739572
22.947591	117.981873	50.744577
19.917128	110.218334	50.749581
16.419626	109.414653	50.754586
12.523091	114.503381	50.759591
8.710577	114.165682	50.764596
5.271992	108.158031	50.769601
1.731176	103.145656	50.774605