Wed Jun 15 16:23:42 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
-0.151104	98.476306	0.000000
0.280408	97.769008	0.005005
0.693147	99.950908	0.010010
0.172298	102.732281	0.015014
0.115242	74.299900	0.020019
-0.238797	92.048228	0.025024
-0.180836	89.328426	0.030029
-0.143357	76.433494	0.035034
-0.356015	94.643603	0.040038
-0.193432	72.371991	0.045043
-0.979941	53.432670	0.050048
-1.210129	56.675903	0.055053
-1.400938	31.241365	0.060058
-1.883564	54.385228	0.065062
-2.203715	29.739435	0.070067
-2.668852	30.859664	0.075072
-3.167021	42.738648	0.080077
-2.800699	27.067772	0.085082
-2.984504	10.829856	0.090086
-2.828622	7.332242	0.095091
-3.642907	20.914286	0.100096
-3.776606	33.220441	0.105101
-4.136663	11.223110	0.110106
-5.249579	24.626044	0.115110
-5.292889	20.094688	0.120115
-5.543699	3.160563	0.125120
-5.441038	18.963405	0.130125
-5.464235	28.998916	0.135130
-5.828808	14.807586	0.140134
-5.829790	6.837352	0.145139
-5.912095	11.235840	0.150144
-6.784618	31.939979	0.155149
-6.803146	15.735117	0.160154
-7.217785	31.724078	0.165158
-6.759160	22.493343	0.170163
-8.069666	8.191208	0.175168
-8.328933	7.272637	0.180173
-8.354055	22.141905	0.185178
-8.811371	28.050888	0.190182
-8.431141	11.093953	0.195187
-8.627479	30.465505	0.200192
-8.867915	14.114328	0.205197
-8.818440	16.581555	0.210202
-9.741719	10.712877	0.215206
-9.977010	7.011592	0.220211
-10.292250	22.226418	0.225216
-10.371295	17.215730	0.230221
-10.312348	18.109075	0.235226
-11.184750	26.206552	0.240230
-11.669808	15.064154	0.245235
-12.022050	-3.735065	0.250240
-11.865538	10.646854	0.255245
-11.544294	18.205951	0.260250
-12.285911	12.149419	0.265254
-12.314711	20.133425	0.270259
-11.892156	16.659904	0.275264
-12.337843	3.045357	0.280269
-12.954694	17.503101	0.285274
-13.172429	15.956690	0.290278
-13.416120	14.130470	0.295283
-14.271829	9.736529	0.300288
-14.334523	16.370346	0.305293
-14.449041	22.305539	0.310298
-14.635919	27.354916	0.315302
-14.535754	-2.580817	0.320307
-14.572420	11.571912	0.325312
-15.016364	33.341723	0.330317
-15.294493	11.505558	0.335322
-15.886125	5.656653	0.340326
-16.217296	9.248013	0.345331
-17.204268	-3.228964	0.350336
-17.076733	5.218579	0.355341
-17.068839	16.383466	0.360346
-17.734170	20.631496	0.365350
-17.606440	6.103622	0.370355
-17.718189	10.403793	0.375360
-17.931483	16.512943	0.380365
-17.635368	-2.075784	0.385370
-17.848526	8.618195	0.390374
-18.613959	17.606320	0.395379
-19.141582	12.854824	0.400384
-19.169604	20.939616	0.405389
-19.166653	9.886049	0.410394
-19.454222	18.973851	0.415398
-19.851636	12.743839	0.420403
-20.397521	11.711940	0.425408
-20.881510	7.933281	0.430413
-20.984763	6.389655	0.435418
-21.265157	22.498766	0.440422
-21.069899	16.172485	0.445427
-21.024347	14.995595	0.450432
-21.049920	23.523790	0.455437
-21.624799	9.570335	0.460442
-22.388836	7.845299	0.465446
-22.394919	18.464718	0.470451
-22.864301	26.740332	0.475456
-22.877668	16.774760	0.480461
-22.785014	-10.092718	0.485466
-23.599934	11.942960	0.490470
-23.919646	24.387370	0.495475
-23.964524	16.489295	0.500480
-24.553431	20.291837	0.505485
-24.086268	15.621868	0.510490
-24.516331	6.493912	0.515494
-24.872738	8.420258	0.520499
-25.460601	30.768830	0.525504
-25.597936	40.944345	0.530509
-25.781812	12.077203	0.535514
-25.660375	16.978755	0.540518
-25.824612	20.641669	0.545523
-26.582671	17.233537	0.550528
-27.364954	16.676029	0.555533
-27.093690	29.010151	0.560538
-27.435786	15.331226	0.565542
-27.611984	5.497136	0.570547
-27.599850	22.373110	0.575552
-27.844917	32.882485	0.580557
-27.428035	19.739154	0.585562
-28.057653	20.085364	0.590566
-28.927623	17.290265	0.595571
-28.970992	31.701386	0.600576
-29.263613	21.319903	0.605581
-29.155495	10.624305	0.610586
-30.014964	27.061724	0.615590
-30.231756	7.830435	0.620595
-30.545117	17.060010	0.625600
-31.025733	14.921962	0.630605
-30.793367	0.583467	0.635610
-31.298160	14.319936	0.640614
-31.045035	24.740759	0.645619
-31.148033	11.322800	0.650624
-31.300258	5.418149	0.655629
-31.383553	10.695339	0.660634
-32.294304	12.224212	0.665638
-32.660927	18.475794	0.670643
-32.351947	32.739806	0.675648
-32.727117	19.681894	0.680653
-33.004507	2.523409	0.685658
-34.156846	14.622244	0.690662
-34.495191	21.152465	0.695667
-34.038426	9.517652	0.700672
-34.401488	23.795453	0.705677
-34.085455	25.130664	0.710682
-34.049513	8.806723	0.715686
-34.421878	8.113605	0.720691
-35.422303	20.655710	0.725696
-35.773359	14.509482	0.730701
-35.580204	7.830796	0.735706
-36.290685	30.774635	0.740710
-35.984505	10.623655	0.745715
-36.267048	2.876237	0.750720
-36.741244	0.938566	0.755725
-37.109978	12.639682	0.760730
-37.672038	23.102988	0.765734
-37.271062	4.640752	0.770739
-37.627951	-6.075053	0.775744
-37.753896	11.768259	0.780749
-37.442053	14.012590	0.785754
-38.448499	17.818239	0.790758
-38.602400	13.505119	0.795763
-38.907811	4.962152	0.800768
-39.235093	9.435354	0.805773
-40.082444	18.766988	0.810778
-40.291725	15.006656	0.815782
-39.899713	2.131526	0.820787
-40.363939	18.637282	0.825792
-41.017200	17.830976	0.830797
-40.461074	-3.848080	0.835802
-40.758561	16.487755	0.840806
-40.480222	30.525010	0.845811
-41.400101	11.146035	0.850816
-42.116324	15.677598	0.855821
-42.048467	7.844452	0.860826
-42.309817	6.009709	0.865830
-42.228854	18.241111	0.870835
-42.392290	6.022519	0.875840
-43.340131	8.586397	0.880845
-43.633666	17.514391	0.885850
-44.082129	2.487900	0.890854
-44.418775	-6.939780	0.895859
-43.927068	11.160724	0.900864
-43.923261	12.225650	0.905869
-44.394935	8.095062	0.910874
-44.670954	28.810604	0.915878
-44.311326	23.468573	0.920883
-45.037777	1.997525	0.925888
-45.645306	12.728664	0.930893
-45.753031	17.666606	0.935898
-46.081273	33.834337	0.940902
-45.769005	15.932162	0.945907
-46.546316	5.421665	0.950912
-47.158702	15.215981	0.955917
-47.291597	28.590427	0.960922
-47.799954	29.595184	0.965926
-47.534871	12.278482	0.970931
-47.409087	17.914816	0.975936
-47.780458	20.232598	0.980941
-47.727819	3.197531	0.985946
-48.589405	19.470948	0.990950
-48.889418	33.755600	0.995955
-48.895272	6.981816	1.000960
-49.271581	10.079418	1.005965
-49.363678	6.032491	1.010970
-49.573498	22.586862	1.015974
-49.915104	24.523096	1.020979
-50.481293	8.733105	1.025984
-50.745296	17.324373	1.030989
-50.599685	3.773499	1.035994
-50.833990	14.953450	1.040998
-50.871790	12.631741	1.046003
-51.371065	35.979655	1.051008
-52.093053	28.233726	1.056013
-52.029299	3.617865	1.061018
-52.064290	9.495024	1.066022
-52.233693	31.242834	1.071027
-52.631495	22.844946	1.076032
-53.610562	15.005083	1.081037
-53.717053	8.817752	1.086042
-54.118679	17.715469	1.091046
-54.039062	14.094328	1.096051
-53.902551	15.286081	1.101056
-53.871398	18.987039	1.106061
-53.628604	0.938827	1.111066
-54.276733	20.857142	1.116070
-54.852445	12.173884	1.121075
-55.275233	5.237133	1.126080
-55.512429	17.931380	1.131085
-55.652749	9.990194	1.136090
-56.625767	17.282084	1.141094
-56.939919	26.185474	1.146099
-56.650952	18.967534	1.151104
-56.504823	30.492722	1.156109
-56.625576	2.485529	1.161114
-56.833748	14.959042	1.166118
-57.391491	26.326908	1.171123
-58.225086	13.036895	1.176128
-58.826992	24.261820	1.181133
-58.383439	23.286681	1.186138
-58.357284	10.927653	1.191142
-58.699842	5.711046	1.196147
-58.493343	17.417520	1.201152
-59.154987	39.957631	1.206157
-59.027534	16.225745	1.211162
-59.997425	13.061164	1.216166
-59.953753	21.105299	1.221171
-60.408176	26.992496	1.226176
-60.643548	32.464200	1.231181
-60.322011	10.056728	1.236186
-61.386705	23.765782	1.241190
-61.517663	24.001471	1.246195
-61.338512	21.252085	1.251200
-62.069381	18.723922	1.256205
-61.556121	30.913876	1.261210
-62.003455	27.343220	1.266214
-62.340425	8.882987	1.271219
-62.851343	21.500054	1.276224
-63.346347	27.252993	1.281229
-63.150973	25.148436	1.286234
-63.356312	13.543241	1.291238
-63.733628	4.483519	1.296243
-63.870308	13.711117	1.301248
-64.498092	24.258382	1.306253
-64.614569	25.867490	1.311258
-64.791041	21.621035	1.316262
-64.551278	12.612425	1.321267
-64.818128	32.895470	1.326272
-65.881389	23.718367	1.331277
-66.200080	17.810251	1.336282
-66.477818	31.281435	1.341286
-66.591120	13.712687	1.346291
-66.671842	26.932510	1.351296
-66.876689	25.445626	1.356301
-66.740266	14.300754	1.361306
-66.788708	21.402459	1.366310
-67.555958	18.787780	1.371315
-67.752241	27.318933	1.376320
-68.178974	36.946251	1.381325
-68.260672	17.478768	1.386330
-68.434295	37.020674	1.391334
-68.542856	32.708145	1.396339
-69.141915	15.725333	1.401344
-69.686907	6.875225	1.406349
-69.446217	29.342939	1.411354
-69.875051	27.790974	1.416358
-70.032868	23.706766	1.421363
-70.118664	11.727185	1.426368
-70.974462	27.384793	1.431373
-71.046866	6.930021	1.436378
-71.233866	36.526430	1.441382
-71.479742	41.969392	1.446387
-71.644120	26.434271	1.451392
-71.937318	14.806999	1.456397
-71.944521	26.166050	1.461402
-71.680570	15.300578	1.466406
-72.342892	20.424284	1.471411
-72.708575	25.702080	1.476416
-73.298761	16.373605	1.481421
-73.218207	6.528654	1.486426
-73.133920	4.757928	1.491430
-74.044208	19.658057	1.496435
-74.319966	30.149416	1.501440
-74.759467	17.317885	1.506445
-74.467354	5.606810	1.511450
-75.023523	14.995673	1.516454
-74.834225	22.076436	1.521459
-74.894558	36.341107	1.526464
-75.472064	31.441405	1.531469
-75.957231	-1.603367	1.536474
-76.503899	18.943120	1.541478
-76.432939	14.691485	1.546483
-76.385832	24.229634	1.551488
-76.693008	38.582945	1.556493
-76.447526	20.565441	1.561498
-77.020869	22.777613	1.566502
-77.618323	13.946234	1.571507
-77.516162	15.107559	1.576512
-78.116649	11.832707	1.581517
-78.006612	20.536170	1.586522
-78.807178	11.323062	1.591526
-79.508810	20.489947	1.596531
-79.475937	32.115923	1.601536
-79.614933	29.543014	1.606541
-79.255358	0.541214	1.611546
-79.705004	6.292864	1.616550
-79.955907	23.842648	1.621555
-79.911091	15.454875	1.626560
-80.939282	22.578128	1.631565
-81.057665	27.730810	1.636570
-81.404732	19.200151	1.641574
-81.470526	10.450579	1.646579
-81.448536	22.918414	1.651584
-81.494940	33.642553	1.656589
-81.560684	15.238406	1.661594
-82.686624	3.484893	1.666598
-83.243165	9.646524	1.671603
-82.992801	12.954843	1.676608
-83.292083	16.962844	1.681613
-83.141365	7.130170	1.686618
-83.143233	18.388010	1.691622
-83.682698	17.837729	1.696627
-84.183072	1.804270	1.701632
-84.942344	10.212522	1.706637
-85.201555	13.858775	1.711642
-85.331964	22.869405	1.716646
-84.787078	11.299835	1.721651
-84.949052	7.468359	1.726656
-85.563696	18.341049	1.731661
-85.305110	23.554538	1.736666
-85.812742	17.249331	1.741670
-86.761851	20.827109	1.746675
-86.816380	22.152238	1.751680
-86.977659	31.001756	1.756685
-86.589391	20.125304	1.761690
-86.611299	23.112549	1.766694
-87.780491	33.838966	1.771699
-88.148325	14.010684	1.776704
-88.343130	13.312491	1.781709
-87.809695	18.118721	1.786714
-88.616230	14.509186	1.791718
-88.605383	25.976918	1.796723
-89.312415	26.147023	1.801728
-90.047977	11.756405	1.806733
-89.991350	10.375954	1.811738
-89.834764	28.680214	1.816742
-89.944217	34.041932	1.821747
-89.916723	20.288024	1.826752
-90.285415	12.940649	1.831757
-90.440538	20.769246	1.836762
-91.323863	10.601710	1.841766
-91.573553	32.084403	1.846771
-91.370491	32.011567	1.851776
-91.429420	30.428161	1.856781
-91.875895	16.098667	1.861786
-92.428515	11.896725	1.866790
-93.138671	22.250248	1.871795
-93.066967	26.440889	1.876800
-93.299184	27.519472	1.881805
-93.021266	18.749393	1.886810
-93.274508	26.142904	1.891814
-93.854830	32.629666	1.896819
-94.301502	34.253987	1.901824
-94.786898	21.437145	1.906829
-94.721983	11.009118	1.911834
-95.177463	28.216480	1.916838
-94.858647	29.952913	1.921843
-94.931660	13.949630	1.926848
-95.801626	24.126257	1.931853
-95.856783	13.636295	1.936858
-96.263465	14.701294	1.941862
-96.506285	34.726351	1.946867
-96.357225	28.665366	1.951872
-96.595758	14.097016	1.956877
-96.881504	7.530625	1.961882
-97.699055	10.140846	1.966886
-98.126576	18.841901	1.971891
-97.807435	6.028532	1.976896
-98.375825	21.279168	1.981901
-98.121567	10.033742	1.986906
-98.133060	16.398174	1.991910
-98.405984	27.443450	1.996915
-99.362757	20.229100	2.006912
-98.920512	20.137113	2.016909
-98.237057	16.774329	2.026906
-98.233157	18.146190	2.036902
-97.089972	10.338939	2.046899
-96.788920	8.717493	2.056896
-96.588324	18.003052	2.066893
-95.438822	23.019712	2.076890
-95.320274	9.567291	2.086886
-95.238338	18.658423	2.096883
-94.146256	27.250640	2.106880
-93.834286	9.734673	2.116877
-93.481548	15.805838	2.126874
-92.530192	24.721876	2.136870
-92.291439	22.875943	2.146867
-92.021925	10.868201	2.156864
-91.472428	22.215155	2.166861
-90.992986	24.938050	2.176858
-90.435205	13.507989	2.186854
-89.561741	7.154498	2.196851
-89.306790	18.816320	2.206848
-89.095021	14.704178	2.216845
-88.151862	-0.048942	2.226842
-87.847245	14.371271	2.236838
-87.290882	11.819472	2.246835
-86.579078	11.932533	2.256832
-86.244167	15.624364	2.266829
-86.024195	16.671705	2.276826
-85.231280	13.466647	2.286822
-84.814480	15.216322	2.296819
-84.411654	17.360531	2.306816
-83.530191	8.845079	2.316813
-83.423567	22.103473	2.326810
-83.015382	7.819033	2.336806
-82.250804	22.952228	2.346803
-81.823686	18.352613	2.356800
-81.331458	19.328093	2.366797
-80.074907	11.615003	2.376794
-80.037322	15.022618	2.386790
-79.653346	20.166687	2.396787
-79.914569	22.635472	2.406784
-78.596517	17.031470	2.416781
-78.227645	14.692892	2.426778
-78.070567	6.500629	2.436774
-77.269426	22.541325	2.446771
-76.589881	13.405765	2.456768
-76.371939	26.498893	2.466765
-75.412015	13.948472	2.476762
-75.109168	17.338422	2.486758
-75.088337	21.833819	2.496755
-74.593470	22.358166	2.506752
-73.357479	13.899387	2.516749
-73.220159	21.582759	2.526746
-73.081087	25.972979	2.536742
-71.885356	11.387899	2.546739
-71.991356	12.694657	2.556736
-71.542603	22.354053	2.566733
-70.670983	15.745736	2.576730
-70.154384	12.457151	2.586726
-69.718605	21.318440	2.596723
-68.820923	19.358868	2.606720
-68.446878	10.813193	2.616717
-68.814873	7.489557	2.626714
-68.146997	11.609652	2.636710
-67.432069	12.227122	2.646707
-66.530042	11.056220	2.656704
-66.027752	13.162262	2.666701
-66.159197	13.049920	2.676698
-65.390466	17.531153	2.686694
-64.509189	19.679359	2.696691
-64.532248	17.454347	2.706688
-63.298968	15.453044	2.716685
-62.787014	17.318165	2.726682
-62.756885	24.675033	2.736678
-62.705576	15.926971	2.746675
-61.955777	11.067201	2.756672
-61.162409	23.333627	2.766669
-60.588793	14.598414	2.776666
-59.941706	14.452229	2.786662
-59.817403	22.371251	2.796659
-59.858111	13.951998	2.806656
-58.852562	21.624633	2.816653
-58.140711	10.336826	2.826650
-57.311759	13.161083	2.836646
-57.073386	24.116767	2.846643
-56.791665	18.636527	2.856640
-56.467637	11.728857	2.866637
-55.671938	20.184370	2.876634
-55.032153	22.817951	2.886630
-54.532476	16.143194	2.896627
-54.553552	25.620371	2.906624
-53.302076	19.822027	2.916621
-53.280959	8.539133	2.926618
-52.978980	14.903551	2.936614
-52.028190	31.100580	2.946611
-51.691462	13.597697	2.956608
-51.216938	14.671223	2.966605
-50.417738	10.503287	2.976602
-50.191690	21.281835	2.986598
-50.259443	29.852890	2.996595
-48.968811	24.892378	3.006592
-48.429620	29.364734	3.016589
-48.411069	13.336950	3.026586
-47.569959	18.279540	3.036582
-46.799922	20.590241	3.046579
-46.933989	7.160008	3.056576
-46.558972	12.242541	3.066573
-45.638919	15.268154	3.076570
-45.191677	9.734685	3.086566
-44.671629	13.171118	3.096563
-43.694282	11.267328	3.106560
-43.422253	-0.280944	3.116557
-43.499040	13.021095	3.126554
-42.969523	15.548643	3.136550
-42.208578	11.521163	3.146547
-42.027167	12.559865	3.156544
-41.487123	6.820232	3.166541
-40.555990	17.722469	3.176538
-39.770340	9.218704	3.186534
-39.227169	10.583919	3.196531
-39.158168	23.007593	3.206528
-39.111867	7.466224	3.216525
-38.273873	2.490741	3.226522
-37.473695	17.081036	3.236518
-37.504824	1.812634	3.246515
-36.461157	8.858681	3.256512
-36.140793	18.113393	3.266509
-35.997043	14.503487	3.276506
-34.967957	21.907825	3.286502
-34.719070	7.388158	3.296499
-34.368046	14.966678	3.306496
-33.743396	16.988301	3.316493
-32.961984	7.916705	3.326490
-32.802884	16.870737	3.336486
-31.599319	10.992015	3.346483
-31.397491	17.250806	3.356480
-31.146689	8.791774	3.366477
-31.163644	9.783451	3.376474
-29.810415	18.935033	3.386470
-29.585466	7.115504	3.396467
-29.389846	17.027318	3.406464
-28.903157	2.962315	3.416461
-27.692939	12.308699	3.426458
-27.494015	20.417282	3.436454
-27.453181	8.365642	3.446451
-26.294021	12.577900	3.456448
-26.062606	14.954306	3.466445
-25.868165	1.393829	3.476442
-24.918702	6.722391	3.486438
-24.254758	8.748583	3.496435
-24.395052	6.961937	3.506432
-23.896196	8.703488	3.516429
-22.790568	18.262830	3.526426
-22.566581	16.550015	3.536422
-22.457534	13.404641	3.546419
-21.439268	11.422581	3.556416
-20.752309	8.342010	3.566413
-20.821261	11.676461	3.576410
-20.276796	14.692044	3.586406
-19.249018	6.953656	3.596403
-18.850418	13.178545	3.606400
-19.228820	20.980040	3.616397
-18.226016	4.395010	3.626394
-17.650893	10.865313	3.636390
-16.837197	20.476358	3.646387
-16.291722	15.902719	3.656384
-16.019771	22.449402	3.666381
-15.817262	6.915304	3.676378
-15.370018	13.013629	3.686374
-14.784709	28.372043	3.696371
-14.262792	11.526995	3.706368
-12.937397	23.396256	3.716365
-12.919156	19.994659	3.726362
-12.899830	10.790220	3.736358
-12.444897	19.960669	3.746355
-11.414113	5.500936	3.756352
-11.143540	11.267642	3.766349
-10.887324	16.720060	3.776346
-9.846497	10.085367	3.786342
-9.569411	8.867911	3.796339
-9.248026	18.893671	3.806336
-8.257272	3.063277	3.816333
-7.898040	8.204327	3.826330
-8.016118	15.595664	3.836326
-7.208555	17.936814	3.846323
-6.407590	20.366271	3.856320
-6.106492	26.914956	3.866317
-5.415722	18.792917	3.876314
-4.804901	14.421235	3.886310
-4.896264	22.916087	3.896307
-4.261546	27.760738	3.906304
-3.891937	26.148113	3.916301
-3.449062	31.875884	3.926298
-2.896937	49.917621	3.936294
-2.332890	61.734548	3.946291
-1.776657	68.119401	3.956288
-1.456385	75.697012	3.966285
-1.017445	92.514354	3.976282
-0.504832	101.025299	3.986278
0.000000	114.779071	3.991283
0.102328	135.244418	3.996288
0.332046	140.632299	4.001293
0.199733	133.903960	4.006298
0.609413	127.620820	4.011302
0.434361	145.715869	4.016307
0.193001	160.771938	4.021312
0.742959	135.538766	4.026317
0.535730	154.147568	4.031322
0.547613	130.199120	4.036326
0.895547	149.107897	4.041331
0.960746	134.464163	4.046336
0.641225	140.800541	4.051341
0.554507	133.671265	4.056346
0.514804	134.214053	4.061350
0.692158	168.148906	4.066355
1.159333	175.703795	4.071360
1.251255	140.696892	4.076365
0.739902	140.271082	4.081370
0.675607	145.169139	4.086374
0.367551	139.886109	4.091379
0.322132	155.159269	4.096384
0.879282	157.045937	4.101389
0.722757	169.749303	4.106394
1.169397	164.331880	4.111398
0.907218	163.651420	4.116403
0.776853	166.428744	4.121408
1.194203	180.793172	4.126413
1.051204	172.683750	4.131418
1.468151	160.504928	4.136422
1.122560	152.351459	4.141427
1.040371	159.763727	4.146432
0.875033	142.374371	4.151437
0.713078	135.513120	4.156442
1.085496	147.033562	4.161446
1.061749	178.987110	4.166451
1.134270	163.791787	4.171456
0.866824	164.063942	4.176461
1.056115	179.273578	4.181466
1.334476	168.465785	4.186470
1.093502	157.058696	4.191475
1.018379	149.931244	4.196480
1.257456	170.852106	4.201485
1.042737	149.375655	4.206490
1.323457	168.855507	4.211494
1.212476	155.041066	4.216499
0.670233	134.332396	4.221504
1.439006	156.123931	4.226509
1.167548	173.335114	4.231514
1.517039	165.926282	4.236518
1.334612	149.191773	4.241523
0.782506	145.342555	4.246528
1.158674	167.794739	4.251533
1.122291	176.085096	4.256538
1.228852	165.858512	4.261542
1.184838	175.489260	4.266547
1.058664	172.554538	4.271552
1.023130	180.517546	4.276557
1.068271	168.472592	4.281562
1.428650	175.553572	4.286566
1.105506	179.712048	4.291571
0.996422	178.677991	4.296576
1.586428	151.549359	4.301581
0.887142	174.551076	4.306586
1.435880	175.768535	4.311590
1.136729	179.990915	4.316595
1.067011	171.382758	4.321600
1.483885	190.622302	4.326605
1.690399	202.100064	4.331610
1.870433	181.820545	4.336614
1.639543	190.914965	4.341619
1.407644	191.953158	4.346624
1.725507	160.268689	4.351629
1.222356	168.816529	4.356634
1.557926	174.515226	4.361638
1.451990	163.598607	4.366643
1.525482	158.753126	4.371648
1.552369	166.059404	4.376653
1.214755	175.209134	4.381658
1.635392	159.676500	4.386662
1.618372	176.005662	4.391667
1.407031	189.661636	4.396672
1.997085	195.369485	4.401677
1.670227	167.455614	4.406682
1.394863	163.750159	4.411686
1.292136	186.945576	4.416691
1.681622	201.041079	4.421696
1.942176	191.338100	4.426701
1.983996	199.659839	4.431706
1.670564	186.225989	4.436710
1.409269	172.704125	4.441715
1.702673	189.259865	4.446720
1.961707	195.915862	4.451725
1.871626	212.729533	4.456730
1.530905	177.069998	4.461734
1.551644	183.788946	4.466739
1.939209	210.059089	4.471744
2.072143	214.503254	4.476749
1.721186	211.921933	4.481754
1.877342	185.652264	4.486758
1.840812	194.484621	4.491763
1.604383	203.664899	4.496768
2.077797	199.853354	4.501773
2.098750	216.151893	4.506778
1.485296	198.230538	4.511782
1.919237	197.681360	4.516787
1.945559	214.789198	4.521792
1.802210	200.180457	4.526797
1.604978	192.140358	4.531802
1.811726	207.096969	4.536806
1.744855	215.899136	4.541811
1.444675	201.873173	4.546816
1.747692	180.223348	4.551821
1.639441	185.273496	4.556826
1.696772	213.859798	4.561830
2.169111	232.123585	4.566835
2.149817	224.104868	4.571840
2.037967	208.730442	4.576845
1.787835	217.588740	4.581850
2.284334	219.692203	4.586854
2.050817	222.860456	4.591859
1.901308	238.031143	4.596864
2.326301	234.748645	4.601869
2.248667	221.521626	4.606874
2.422917	228.855544	4.611878
2.201935	212.712634	4.616883
1.784715	209.261642	4.621888
2.071903	220.222197	4.626893
2.245585	221.387208	4.631898
2.616102	228.767018	4.636902
2.359784	213.452171	4.641907
2.049052	219.245852	4.646912
2.604936	197.502524	4.651917
2.388983	194.504999	4.656922
2.121978	215.509531	4.661926
2.311490	206.745466	4.666931
2.116088	189.542238	4.671936
2.368193	194.558980	4.676941
1.750501	226.185290	4.681946
2.022284	221.831552	4.686950
2.125500	224.021414	4.691955
2.072038	244.132958	4.696960
1.953580	225.354698	4.701965
1.916293	233.098040	4.706970
2.429363	247.151165	4.711974
2.089766	245.566370	4.716979
2.283694	236.821189	4.721984
2.752777	227.754823	4.726989
2.259887	240.877719	4.731994
2.315739	229.216658	4.736998
2.207845	237.558226	4.742003
2.188360	259.540053	4.747008
2.875457	253.667951	4.752013
2.734208	249.932617	4.757018
2.632571	235.696247	4.762022
2.243258	245.545489	4.767027
2.452598	252.743404	4.772032
2.785914	255.791160	4.777037
2.242886	243.610834	4.782042
2.565256	242.476371	4.787046
2.618151	261.490865	4.792051
2.919774	258.249072	4.797056
2.860463	250.803781	4.802061
2.402424	253.610314	4.807066
2.581022	249.564161	4.812070
2.301431	241.718072	4.817075
2.826461	255.222624	4.822080
2.590707	248.043444	4.827085
2.399347	272.635293	4.832090
2.605855	270.706626	4.837094
2.549840	260.823110	4.842099
2.294973	265.352880	4.847104
2.507761	266.368098	4.852109
2.267511	259.930893	4.857114
2.354394	269.299566	4.862118
2.459779	267.245559	4.867123
2.527884	284.298726	4.872128
2.987590	275.384319	4.877133
3.064473	289.361397	4.882138
3.145524	297.662994	4.887142
2.956885	274.683426	4.892147
2.761823	282.839959	4.897152
2.971286	264.933562	4.902157
2.388112	274.605036	4.907162
2.668541	283.668874	4.912166
2.860643	278.010850	4.917171
2.721511	285.124513	4.922176
3.012546	295.051054	4.927181
2.834025	300.827159	4.932186
3.144400	283.047796	4.937190
3.173677	294.399941	4.942195
3.186279	289.807475	4.947200
3.302172	266.720969	4.952205
3.233773	291.893391	4.957210
3.140402	289.412232	4.962214
2.601003	271.092249	4.967219
2.692723	273.769363	4.972224
2.923343	279.074379	4.977229
2.840927	290.025234	4.982234
2.893484	296.452895	4.987238
3.245100	290.942619	4.992243
2.748325	281.197626	4.997248
3.115944	291.691754	5.002253
2.932754	293.999588	5.007258
3.090254	279.432894	5.012262
3.150253	290.559582	5.017267
3.089138	299.902322	5.022272
3.503242	278.940219	5.027277
3.114865	289.286319	5.032282
2.944068	281.123626	5.037286
3.043910	278.842559	5.042291
2.666343	306.993066	5.047296
3.318771	284.009444	5.052301
3.015878	302.523749	5.057306
3.244907	318.545339	5.062310
3.165484	315.375677	5.067315
3.295861	330.404712	5.072320
3.833485	307.580698	5.077325
3.298610	312.751798	5.082330
3.250142	292.072884	5.087334
3.399607	306.930448	5.092339
3.391560	305.511039	5.097344
3.513050	291.197102	5.102349
3.134682	283.182647	5.107354
3.101719	300.346052	5.112358
3.727310	322.499751	5.117363
3.567518	325.135771	5.122368
3.450212	293.429546	5.127373
3.411576	287.242820	5.132378
3.386328	301.342832	5.137382
3.393973	316.081395	5.142387
3.561708	319.551019	5.147392
3.917261	296.895117	5.152397
3.381604	293.028642	5.157402
3.382023	299.866219	5.162406
3.221264	316.426814	5.167411
3.478991	317.081549	5.172416
3.669006	320.976314	5.177421
3.703757	322.757758	5.182426
3.718629	311.210834	5.187430
3.573477	309.874750	5.192435
3.542239	327.300698	5.197440
3.511363	326.286851	5.202445
3.572354	323.771201	5.207450
3.786405	309.777748	5.212454
3.743758	325.960448	5.217459
3.648052	318.709853	5.222464
3.641989	320.354508	5.227469
3.595072	335.021905	5.232474
3.833396	316.835352	5.237478
3.591033	302.737002	5.242483
3.609513	324.698147	5.247488
3.990911	307.289278	5.252493
3.600988	327.961512	5.257498
3.397444	332.037031	5.262502
3.540503	316.350472	5.267507
3.867203	321.437299	5.272512
3.964383	325.107396	5.277517
3.691631	316.799453	5.282522
3.611725	306.056589	5.287526
3.828655	326.035663	5.292531
3.533179	341.615300	5.297536
3.693660	315.824713	5.302541
3.942494	321.647101	5.307546
3.983776	327.589516	5.312550
3.790544	315.082511	5.317555
3.548986	324.042145	5.322560
3.989614	315.286436	5.327565
3.766667	318.729768	5.332570
3.971884	324.510337	5.337574
3.904764	316.756749	5.342579
3.718657	308.788046	5.347584
4.223623	335.448096	5.352589
4.011417	355.841124	5.357594
3.705876	329.805737	5.362598
3.931862	348.842638	5.367603
3.744734	353.282716	5.372608
4.102658	343.009050	5.377613
4.190560	348.597613	5.382618
4.083297	366.525068	5.387622
4.257673	353.224031	5.392627
4.159374	353.417136	5.397632
4.371454	355.508727	5.402637
4.287665	338.507563	5.407642
4.377131	339.809614	5.412646
4.158431	337.775515	5.417651
3.781872	332.448397	5.422656
4.458831	341.627563	5.427661
4.315049	330.227687	5.432666
4.396256	341.488619	5.437670
4.281643	327.742813	5.442675
4.049097	329.436932	5.447680
4.009637	344.625840	5.452685
4.021811	338.444606	5.457690
4.435007	328.765343	5.462694
4.273170	339.609501	5.467699
3.975761	363.868624	5.472704
4.506888	351.212192	5.477709
4.531697	362.945119	5.482714
4.509995	359.532706	5.487718
4.477243	338.041627	5.492723
4.101350	335.538787	5.497728
4.379891	347.785751	5.502733
4.237736	356.922525	5.507738
4.523900	344.202014	5.512742
4.439267	361.065948	5.517747
4.359073	360.022862	5.522752
4.336343	343.153162	5.527757
4.424851	365.394199	5.532762
4.475998	358.945000	5.537766
4.509173	360.558218	5.542771
4.238366	361.761281	5.547776
4.281094	344.748573	5.552781
4.355150	340.645982	5.557786
4.256956	362.083109	5.562790
4.341451	359.736499	5.567795
3.810651	354.577607	5.572800
4.400800	353.764079	5.577805
4.196126	353.480734	5.582810
4.565914	370.277475	5.587814
4.483033	368.193701	5.592819
4.589014	381.850085	5.597824
4.722271	382.613583	5.602829
4.579033	395.944982	5.607834
4.829599	385.090826	5.612838
4.821530	381.467711	5.617843
4.685968	392.754244	5.622848
4.941903	379.834201	5.627853
4.438531	363.783472	5.632858
4.313551	380.441706	5.637862
4.513978	387.091687	5.642867
4.450115	381.749772	5.647872
4.822495	386.633157	5.652877
4.765037	391.073323	5.657882
4.370390	371.939224	5.662886
4.837161	362.870102	5.667891
4.744895	375.005436	5.672896
4.813162	375.204063	5.677901
4.751611	383.610262	5.682906
4.871234	389.057167	5.687910
5.013322	384.426899	5.692915
4.865495	363.820143	5.697920
5.178866	374.411385	5.702925
4.782641	390.252665	5.707930
4.869658	395.585399	5.712934
4.564228	374.171490	5.717939
4.578210	373.238518	5.722944
4.805791	384.110590	5.727949
4.916852	389.432148	5.732954
4.838991	388.366675	5.737958
5.083049	391.206955	5.742963
4.751871	391.552385	5.747968
5.074289	386.519425	5.752973
4.971352	381.918403	5.757978
4.932224	384.782198	5.762982
5.090570	398.326758	5.767987
5.236591	394.126633	5.772992
5.075886	383.447969	5.777997
4.913113	389.321732	5.783002
5.216149	378.194236	5.788006
5.120229	375.739824	5.793011
5.053106	382.684190	5.798016
4.981762	382.287166	5.803021
5.055273	395.943996	5.808026
5.233274	403.349292	5.813030
5.486044	412.797180	5.818035
5.065308	397.088486	5.823040
5.014454	388.648836	5.828045
5.211042	411.019459	5.833050
5.259717	410.233953	5.838054
5.411200	406.703040	5.843059
4.935113	400.743832	5.848064
5.251242	421.213393	5.853069
5.343468	418.974306	5.858074
5.294185	406.555305	5.863078
5.314024	423.583261	5.868083
5.357179	412.952272	5.873088
5.465411	403.711145	5.878093
5.090858	405.882917	5.883098
5.233524	416.350085	5.888102
5.273888	410.585393	5.893107
5.595401	409.480852	5.898112
5.456213	424.983153	5.903117
5.270129	427.199840	5.908122
5.313808	411.939490	5.913126
5.632559	428.437834	5.918131
5.531741	422.862099	5.923136
5.379647	415.428904	5.928141
5.202815	415.447063	5.933146
5.410848	402.268961	5.938150
5.620033	421.208502	5.943155
5.247984	431.404915	5.948160
5.532284	432.374293	5.953165
5.423326	413.893136	5.958170
5.439079	424.013719	5.963174
5.441136	431.565299	5.968179
5.027104	421.034519	5.973184
5.673847	414.025296	5.978189
5.552386	441.004500	5.983194
5.240194	413.541637	5.988198
5.689791	415.481625	5.993203
5.367037	426.065370	5.998208
5.412756	409.951474	6.003213
5.304773	430.245105	6.008218
5.210868	428.890381	6.013222
5.686430	430.784549	6.018227
5.486872	416.997160	6.023232
5.647173	426.622615	6.028237
5.384955	434.295603	6.033242
5.529059	444.181316	6.038246
5.759772	444.879487	6.043251
5.776395	452.724024	6.048256
5.518258	434.088054	6.053261
5.341289	432.396459	6.058266
5.459319	446.647043	6.063270
5.802156	440.069307	6.068275
5.833948	449.849385	6.073280
5.751071	451.910912	6.078285
5.672783	420.504279	6.083290
5.481652	419.186832	6.088294
5.945221	419.126092	6.093299
5.318290	414.894872	6.098304
5.404626	424.454715	6.103309
5.413635	424.986307	6.108314
5.698380	431.351091	6.113318
6.229147	429.470921	6.118323
5.489094	421.565586	6.123328
5.560670	437.197024	6.128333
5.223620	443.564143	6.133338
5.192213	437.924451	6.138342
6.044391	426.341271	6.143347
5.460571	442.087630	6.148352
5.699563	438.227561	6.153357
5.451383	428.146235	6.158362
5.572433	436.543596	6.163366
5.714211	432.064396	6.168371
5.404308	446.815904	6.173376
6.090568	434.564664	6.178381
5.720842	439.004361	6.183386
5.736740	422.070975	6.188390
5.547426	417.360905	6.193395
5.483754	424.507639	6.198400
5.568226	414.208581	6.203405
5.488920	414.694098	6.208410
5.619596	428.633905	6.213414
5.701983	414.785128	6.218419
5.373826	446.652592	6.223424
5.784650	441.211200	6.228429
5.637208	429.923228	6.233434
5.333767	421.148366	6.238438
5.681985	434.210460	6.243443
5.470278	423.176874	6.248448
5.430038	431.239241	6.253453
5.591164	451.754188	6.258458
5.597826	440.188005	6.263462
5.723877	413.853470	6.268467
5.492640	427.936935	6.273472
5.763291	438.725180	6.278477
5.785363	436.396667	6.283482
5.670954	411.159683	6.288486
5.601569	429.517668	6.293491
5.428607	423.992623	6.298496
5.339520	419.490317	6.303501
5.285772	438.755860	6.308506
5.809274	441.492063	6.313510
5.784154	460.190014	6.318515
5.879288	436.293522	6.323520
5.938865	426.975584	6.328525
5.529177	432.864420	6.333530
5.820219	422.340532	6.338534
5.565851	413.327911	6.343539
5.359081	432.192079	6.348544
5.593994	419.176631	6.353549
5.374354	435.817225	6.358554
5.311003	416.281374	6.363558
5.530274	435.912568	6.368563
5.582938	443.457369	6.373568
5.607709	420.107699	6.378573
5.518441	423.228678	6.383578
5.485486	450.603057	6.388582
5.815591	442.869684	6.393587
5.451489	441.984095	6.398592
5.626713	438.263201	6.403597
5.709732	457.640920	6.408602
5.667299	448.900940	6.413606
5.894851	430.747501	6.418611
5.541418	417.209769	6.423616
5.388293	412.297805	6.428621
5.445308	432.419061	6.433626
5.493241	439.466072	6.438630
5.980323	439.561849	6.443635
5.248870	439.713291	6.448640
5.539236	432.448955	6.453645
5.839603	440.702056	6.458650
6.012117	439.171706	6.463654
5.643718	446.073947	6.468659
5.538418	429.078210	6.473664
5.587788	432.989834	6.478669
5.876588	424.904313	6.483674
5.890213	423.554608	6.488678
5.461303	428.535501	6.493683
5.250676	416.185969	6.498688
5.688803	424.962216	6.503693
5.628728	429.214801	6.508698
5.489442	420.266220	6.513702
5.760799	424.232999	6.518707
5.700289	424.992514	6.523712
5.744427	436.511097	6.528717
5.775055	432.080352	6.533722
5.673835	432.864155	6.538726
5.697289	423.010904	6.543731
5.454052	446.011033	6.548736
5.449977	430.268273	6.553741
5.586088	418.400454	6.558746
5.498278	419.311565	6.563750
5.581222	427.301684	6.568755
5.308254	439.762876	6.573760
5.443798	430.033152	6.578765
5.389134	426.726397	6.583770
5.319702	421.835521	6.588774
5.467730	418.427798	6.593779
5.598927	451.703626	6.598784
5.718722	438.362112	6.603789
5.739955	446.887940	6.608794
5.695240	446.716859	6.613798
5.906670	419.446532	6.618803
5.648754	419.005268	6.623808
5.542593	426.315086	6.628813
5.636455	442.042481	6.633818
5.594646	423.411713	6.638822
5.720937	422.909423	6.643827
5.449207	434.133355	6.648832
5.927054	411.481638	6.653837
5.444894	420.154464	6.658842
5.455523	433.246204	6.663846
5.624162	432.473919	6.668851
5.556836	431.419429	6.673856
5.698527	419.404193	6.678861
5.768568	433.847662	6.683866
5.441847	425.841071	6.688870
6.021136	420.405189	6.693875
5.621170	434.563993	6.698880
5.691459	427.545360	6.703885
5.886322	408.444504	6.708890
5.397461	425.672439	6.713894
5.573877	436.118260	6.718899
5.528414	431.330454	6.723904
5.599978	414.392414	6.728909
5.901451	408.511376	6.733914
5.517933	427.139777	6.738918
5.715910	438.143543	6.743923
5.706123	428.816942	6.748928
5.795281	430.906168	6.753933
5.808319	427.889399	6.758938
5.611532	412.458961	6.763942
5.748259	417.867932	6.768947
5.620535	424.626810	6.773952
5.744795	419.533856	6.778957
5.813870	421.383922	6.783962
5.485227	412.136461	6.788966
5.495843	395.218281	6.793971
5.430529	424.020863	6.798976
5.640725	425.775003	6.803981
5.679714	423.691896	6.808986
5.585462	420.626173	6.813990
5.868511	403.684468	6.818995
5.640174	404.109381	6.824000
5.691183	421.829529	6.829005
5.394638	402.286756	6.834010
5.531575	394.280013	6.839014
5.473757	404.377128	6.844019
5.565938	427.443434	6.849024
5.913017	417.633086	6.854029
5.752716	409.536853	6.859034
5.441571	401.572389	6.864038
5.620157	391.798188	6.869043
5.310341	397.793817	6.874048
5.684492	405.426637	6.879053
5.921820	403.130724	6.884058
5.720888	409.632876	6.889062
5.841165	403.867015	6.894067
5.428513	386.772368	6.899072
5.360099	371.074729	6.904077
5.553030	386.527730	6.909082
5.586762	406.146734	6.914086
5.937327	386.901007	6.919091
5.328484	396.155570	6.924096
5.577989	395.534074	6.929101
5.631678	381.081213	6.934106
5.524692	401.781862	6.939110
5.552679	375.796141	6.944115
5.823428	396.977518	6.949120
5.594468	392.597081	6.954125
5.700872	384.210660	6.959130
5.503152	403.737299	6.964134
5.765754	389.982370	6.969139
5.625166	385.241076	6.974144
5.603926	391.671009	6.979149
5.883727	389.555016	6.984154
5.675317	394.609848	6.989158
5.731050	407.089596	6.994163
5.830435	396.558332	6.999168
5.883366	385.811019	7.004173
6.070178	394.562291	7.009178
5.700977	390.220913	7.014182
5.884080	384.464801	7.019187
5.687316	387.529649	7.024192
5.652741	366.562160	7.029197
5.339322	375.141968	7.034202
5.324514	370.868498	7.039206
5.518080	391.748230	7.044211
5.378212	404.127814	7.049216
5.775638	393.109204	7.054221
5.708568	383.680624	7.059226
5.544730	386.692482	7.064230
5.962976	400.036552	7.069235
5.625538	389.419348	7.074240
5.528837	408.913220	7.079245
5.363474	401.137942	7.084250
5.515846	384.760024	7.089254
5.643329	381.494009	7.094259
5.395723	406.961597	7.099264
5.256188	387.527946	7.104269
5.249235	402.980159	7.109274
5.512906	406.772018	7.114278
5.429058	385.387275	7.119283
5.355309	386.079429	7.124288
5.180062	398.073419	7.129293
5.716064	386.341375	7.134298
5.176030	399.320475	7.139302
5.451104	404.045832	7.144307
5.485799	399.521892	7.149312
5.698797	400.224666	7.154317
5.775750	405.472848	7.159322
5.555950	422.353761	7.164326
5.298703	408.120948	7.169331
5.381784	417.820319	7.174336
5.559350	431.954708	7.179341
5.326851	426.866648	7.184346
5.487752	433.665828	7.189350
6.092695	434.084537	7.194355
5.465085	433.756452	7.199360
5.810576	423.158458	7.204365
5.863633	440.331283	7.209370
5.813797	420.445063	7.214374
5.684113	398.225419	7.219379
5.405630	403.388212	7.224384
5.488896	399.390131	7.229389
5.502567	389.663013	7.234394
5.232168	411.650713	7.239398
5.534297	428.414011	7.244403
5.651711	435.291602	7.249408
5.583044	430.839189	7.254413
5.950846	426.688624	7.259418
5.697188	419.474539	7.264422
5.617304	423.073004	7.269427
5.519194	413.392556	7.274432
5.459123	422.430967	7.279437
5.487883	430.734471	7.284442
5.477838	428.189802	7.289446
5.888393	416.445911	7.294451
5.799418	418.483286	7.299456
5.300588	405.770913	7.304461
5.306328	408.381565	7.309466
5.112575	441.066205	7.314470
5.351997	434.957372	7.319475
5.025266	425.369941	7.324480
5.205048	408.672483	7.329485
5.582008	420.036024	7.334490
5.222053	440.662420	7.339494
5.663667	430.098255	7.344499
5.473991	425.299262	7.349504
5.794683	437.258974	7.354509
5.736409	419.294146	7.359514
5.417633	428.323621	7.364518
5.641273	415.137108	7.369523
5.290180	434.476742	7.374528
5.832635	443.635877	7.379533
5.863294	421.588478	7.384538
5.356108	435.913271	7.389542
5.357341	422.987930	7.394547
5.610498	448.460927	7.399552
5.606413	453.498290	7.404557
5.707364	452.414608	7.409562
5.813164	432.164782	7.414566
5.446290	438.992781	7.419571
5.596279	437.407459	7.424576
5.502157	428.713124	7.429581
5.572589	453.105247	7.434586
5.602299	458.372599	7.439590
5.711616	431.194592	7.444595
5.371653	425.044387	7.449600
5.485214	453.733713	7.454605
5.830472	451.472832	7.459610
5.298246	442.718797	7.464614
5.794074	434.992667	7.469619
5.849490	460.092324	7.474624
5.784005	465.513617	7.479629
5.910618	448.230643	7.484634
5.291235	438.952589	7.489638
5.654658	419.392376	7.494643
5.187334	434.977916	7.499648
5.349961	455.773670	7.504653
5.439186	452.650590	7.509658
5.672789	454.719500	7.514662
6.039658	459.330957	7.519667
5.539454	445.823965	7.524672
5.643767	424.951428	7.529677
5.427127	433.850878	7.534682
5.456904	446.044131	7.539686
5.710668	445.360077	7.544691
5.788745	434.208061	7.549696
5.691849	439.621218	7.554701
5.666453	429.346520	7.559706
5.571034	437.313639	7.564710
5.523156	447.365242	7.569715
5.447347	443.829660	7.574720
5.793129	427.997420	7.579725
5.798933	440.095193	7.584730
5.614300	445.863484	7.589734
5.513522	432.238904	7.594739
5.415721	450.204550	7.599744
5.266117	436.123498	7.604749
5.581948	444.586535	7.609754
5.479501	439.561620	7.614758
5.814761	454.686247	7.619763
5.760677	464.876502	7.624768
5.897363	451.819648	7.629773
5.872620	453.014904	7.634778
5.535912	443.209419	7.639782
5.646409	436.287423	7.644787
5.736752	430.830927	7.649792
5.293135	451.069368	7.654797
5.650709	438.453974	7.659802
5.141541	435.337154	7.664806
5.507998	428.430670	7.669811
5.523811	435.904612	7.674816
5.517189	444.146297	7.679821
5.824181	451.306664	7.684826
5.092689	448.644654	7.689830
5.718422	463.246196	7.694835
5.830765	452.887854	7.699840
6.067928	445.410936	7.704845
5.866847	457.251897	7.709850
5.194083	444.515458	7.714854
5.517828	433.638026	7.719859
5.399054	423.320857	7.724864
5.638205	436.791429	7.729869
5.626108	448.855469	7.734874
5.336945	434.101023	7.739878
5.782016	455.997779	7.744883
5.516541	445.284496	7.749888
5.567591	429.079337	7.754893
5.495704	452.826734	7.759898
5.522594	483.451620	7.764902
5.699473	481.056678	7.769907
5.337762	463.450911	7.774912
5.713446	465.886301	7.779917
5.515975	468.423215	7.784922
5.703851	478.437655	7.789926
5.870100	469.147540	7.794931
5.635666	468.907880	7.799936
5.706143	449.783136	7.804941
5.658394	438.873771	7.809946
5.886090	434.878151	7.814950
5.654071	442.161326	7.819955
5.820203	425.699409	7.824960
5.540673	440.116701	7.829965
5.786563	439.222051	7.834970
5.438464	429.744787	7.839974
5.489268	435.316626	7.844979
5.469312	437.884179	7.849984
5.405416	425.883873	7.854989
5.600807	422.913621	7.859994
5.191526	434.255874	7.864998
5.564020	435.454636	7.870003
5.677977	445.334480	7.875008
5.531628	445.169145	7.880013
5.527586	438.960562	7.885018
5.589889	449.792025	7.890022
5.646054	460.978462	7.895027
5.507721	458.891705	7.900032
5.763528	451.598149	7.905037
5.688389	453.117014	7.910042
5.240478	449.191901	7.915046
5.598918	440.057082	7.920051
5.824150	456.087434	7.925056
5.517641	469.850634	7.930061
5.507138	443.720325	7.935066
5.865926	455.782960	7.940070
5.790167	456.963070	7.945075
5.459286	432.898946	7.950080
5.283067	431.030350	7.955085
5.675415	458.692456	7.960090
5.484454	459.034939	7.965094
5.685114	448.080768	7.970099
5.755174	459.300322	7.975104
5.404277	465.562310	7.980109
5.780017	457.689890	7.985114
5.561283	449.954975	7.990118
5.762747	436.903265	7.995136
5.329562	442.683726	8.000154
5.408085	442.377905	8.005171
6.019076	457.108393	8.010189
5.434096	460.581247	8.015206
5.667017	453.857649	8.020224
5.618833	462.942622	8.025242
5.573655	465.244102	8.030259
5.621732	455.621671	8.035277
5.522649	471.085677	8.040294
6.222462	448.109632	8.045312
5.776855	433.515230	8.050330
5.321803	446.616589	8.055347
5.504761	444.851405	8.060365
5.291250	452.697817	8.065382
5.824214	463.606479	8.070400
5.746763	467.326176	8.075418
5.607651	474.292836	8.080435
5.881098	446.952494	8.085453
5.598211	458.262237	8.090470
5.779954	475.227822	8.095488
5.717901	481.746442	8.100506
5.801698	455.604318	8.105523
5.674529	449.255295	8.110541
5.490207	453.982031	8.115558
5.571265	476.600730	8.120576
5.666092	480.907533	8.125594
5.930994	461.417229	8.130611
5.910913	453.095753	8.135629
5.791207	476.863255	8.140646
5.775238	459.444579	8.145664
5.786329	462.843037	8.150682
5.865530	482.222724	8.155699
6.126766	460.957745	8.160717
5.486191	438.093212	8.165734
5.309098	428.042493	8.170752
5.849745	463.635895	8.175770
5.977054	472.579799	8.180787
6.155707	454.078775	8.185805
5.695082	455.865512	8.190822
5.598116	446.134416	8.195840
5.780927	452.879412	8.200858
5.917864	475.913853	8.205875
6.002676	470.540526	8.210893
5.838740	446.927228	8.215910
5.802260	428.719782	8.220928
5.896999	446.542678	8.225946
5.676982	452.454501	8.230963
5.620287	451.174757	8.235981
6.046627	478.330161	8.240998
6.109884	465.464899	8.246016
6.010813	452.231901	8.251034
5.851335	452.453854	8.256051
5.661038	437.872949	8.261069
5.640871	454.217931	8.266086
6.055339	467.814803	8.271104
6.099386	443.587188	8.276122
5.770651	442.786625	8.281139
6.248770	445.024551	8.286157
5.861114	449.373982	8.291174
5.626137	445.130662	8.296192
5.817790	456.960336	8.301210
5.993108	458.806107	8.306227
5.990675	449.556784	8.311245
5.580553	464.684402	8.316262
5.803065	464.809086	8.321280
5.764629	465.497708	8.326298
5.676140	475.426610	8.331315
5.984692	479.022007	8.336333
5.907157	469.485758	8.341350
5.810556	476.090968	8.346368
5.852679	452.228611	8.351386
5.643253	471.091379	8.356403
5.939644	477.179314	8.361421
5.874382	472.628492	8.366438
5.674599	452.662195	8.371456
5.850320	466.006773	8.376474
6.118545	474.939789	8.381491
6.097333	467.057343	8.386509
5.880117	462.989083	8.391526
5.799058	471.538606	8.396544
6.052987	466.761859	8.401562
5.685209	475.726378	8.406579
5.970412	460.528444	8.411597
6.052257	495.021500	8.416614
6.203040	485.287518	8.421632
6.045054	464.767604	8.426650
6.031161	477.661380	8.431667
5.767109	476.045828	8.436685
6.319031	477.352140	8.441702
6.201511	471.358991	8.446720
6.225790	471.665505	8.451738
5.852886	480.431521	8.456755
6.192662	467.628207	8.461773
6.211817	461.040001	8.466790
6.057293	468.733309	8.471808
6.463015	460.530188	8.476826
6.001464	478.696652	8.481843
6.096965	470.510648	8.486861
6.174217	457.153850	8.491878
6.439036	464.874877	8.496896
6.547216	462.970812	8.501914
6.135957	468.985779	8.506931
6.120717	473.086227	8.511949
6.221564	478.150184	8.516966
6.380889	461.848174	8.521984
6.352105	456.515567	8.527002
6.142856	477.659451	8.532019
6.021941	456.417288	8.537037
5.955174	453.188881	8.542054
6.005422	463.539111	8.547072
6.290877	474.727197	8.552090
6.371372	465.697558	8.557107
6.396766	461.446629	8.562125
6.051241	475.570068	8.567143
6.035505	467.995486	8.572160
6.053484	476.254118	8.577178
5.791887	475.061071	8.582195
6.377598	453.213105	8.587213
6.153973	463.317339	8.592231
5.679298	478.744139	8.597248
6.169990	470.852764	8.602266
6.113630	482.129518	8.607283
6.241023	493.815356	8.612301
5.943326	501.114447	8.617319
6.088326	488.353439	8.622336
6.279819	509.029288	8.627354
6.158420	519.110761	8.632371
6.569491	503.121632	8.637389
6.743186	484.803916	8.642407
6.201819	499.626776	8.647424
6.183178	501.232241	8.652442
6.222877	507.172799	8.657459
6.287579	502.633848	8.662477
6.661621	497.184278	8.667495
6.333434	499.057174	8.672512
6.236752	500.685867	8.677530
6.200393	500.139852	8.682547
6.546866	494.078676	8.687565
6.306935	489.693682	8.692583
6.511402	492.624685	8.697600
6.569829	487.396420	8.702618
5.973648	476.928351	8.707635
6.130179	472.188263	8.712653
6.331491	501.248275	8.717671
6.101002	485.744605	8.722688
6.507536	499.892168	8.727706
6.368084	514.701856	8.732723
6.359216	505.324072	8.737741
6.274278	491.071474	8.742759
6.232916	510.851130	8.747776
6.865923	515.809741	8.752794
6.565494	511.632813	8.757811
6.666835	497.148105	8.762829
6.612866	505.758408	8.767847
6.270167	483.096282	8.772864
6.791101	497.896598	8.777882
6.155568	490.333117	8.782899
6.306819	488.175348	8.787917
6.730637	492.705955	8.792935
5.921925	505.994808	8.797952
6.744788	494.147567	8.802970
6.223914	501.818286	8.807987
6.388809	502.569640	8.813005
6.447967	491.771770	8.818023
6.315315	498.190580	8.823040
6.786570	481.513668	8.828058
6.482534	485.989113	8.833075
6.446252	504.445857	8.838093
6.465128	499.873448	8.843111
6.491010	507.629751	8.848128
6.389083	496.174342	8.853146
6.524021	491.967095	8.858163
6.571768	504.833095	8.863181
6.564383	489.702080	8.868199
6.670394	506.380201	8.873216
6.799672	494.178519	8.878234
6.786461	498.391204	8.883251
6.401214	494.628479	8.888269
6.616883	503.528870	8.893287
6.516230	510.537603	8.898304
6.261937	493.817140	8.903322
6.243040	508.556423	8.908339
6.214525	509.827297	8.913357
6.559719	492.958569	8.918375
6.556214	503.814910	8.923392
6.472278	499.197206	8.928410
6.304238	497.414450	8.933427
6.445885	499.930661	8.938445
6.586243	506.631038	8.943463
6.502076	537.413707	8.948480
6.906818	505.524393	8.953498
6.783608	512.613899	8.958515
6.560205	519.193146	8.963533
6.608925	509.552961	8.968551
6.468309	541.103610	8.973568
6.608649	529.985297	8.978586
6.626000	514.658886	8.983603
6.445536	534.888409	8.988621
6.745588	540.211609	8.993639
6.205063	530.177980	8.998656
6.623926	539.349058	9.003674
6.452451	535.442267	9.008691
6.686903	515.245709	9.013709
6.730951	517.783956	9.018727
6.546245	538.067122	9.023744
6.665780	528.837348	9.028762
6.450395	544.617709	9.033779
6.845160	536.766851	9.038797
7.059235	528.646137	9.043815
6.788241	534.361060	9.048832
6.947256	528.406614	9.053850
7.189642	527.101842	9.058867
6.895243	527.489752	9.063885
6.789256	518.998925	9.068903
6.969757	531.475691	9.073920
6.987487	537.243071	9.078938
6.881476	538.029847	9.083955
6.860665	517.749029	9.088973
7.208623	533.339658	9.093991
6.801310	550.262845	9.099008
7.225868	527.225705	9.104026
7.440569	520.387700	9.109043
6.989835	512.918830	9.114061
6.998458	513.366771	9.119079
6.869901	503.700980	9.124096
7.035167	504.527153	9.129114
6.773125	502.095552	9.134131
7.064801	507.683338	9.139149
7.129949	508.206166	9.144167
6.886862	505.733452	9.149184
7.117163	511.902774	9.154202
7.174111	505.729739	9.159219
6.992704	494.565438	9.164237
6.916012	501.913318	9.169255
6.725214	523.140805	9.174272
7.119859	513.241639	9.179290
6.919016	501.891523	9.184307
7.129898	501.157645	9.189325
7.101418	510.341133	9.194343
6.537583	498.661352	9.199360
6.747908	505.781047	9.204378
6.830299	508.854928	9.209395
6.665119	502.421246	9.214413
6.908245	488.840312	9.219431
6.832123	501.697654	9.224448
6.622284	509.076593	9.229466
6.705416	493.184273	9.234483
6.751662	524.574812	9.239501
6.995672	519.533326	9.244519
7.074342	520.598845	9.249536
7.056797	539.662304	9.254554
7.105425	547.051585	9.259571
7.016922	541.386590	9.264589
7.172938	521.493849	9.269607
7.279151	533.724798	9.274624
6.678714	523.328934	9.279642
6.851066	516.605675	9.284659
6.918330	535.271364	9.289677
7.350534	530.602401	9.294695
7.027178	534.077398	9.299712
7.017707	532.942654	9.304730
7.124032	521.103893	9.309747
7.096152	536.070312	9.314765
7.049179	534.717419	9.319783
7.107663	551.071251	9.324800
7.210327	538.725844	9.329818
6.933575	520.661214	9.334835
7.065388	533.934979	9.339853
7.159237	540.680939	9.344871
7.134130	526.272596	9.349888
7.277480	527.801997	9.354906
7.171349	528.451036	9.359923
7.020946	532.130358	9.364941
7.015577	529.240608	9.369959
6.845193	517.307558	9.374976
7.000453	541.897489	9.379994
7.107510	540.421235	9.385011
7.074227	535.851137	9.390029
7.386843	516.404931	9.395047
6.905224	523.547176	9.400064
7.004743	547.514124	9.405082
7.312410	536.838791	9.410099
7.195378	535.524042	9.415117
7.281045	544.788168	9.420135
7.045466	539.542446	9.425152
7.029099	529.098963	9.430170
7.268941	531.329244	9.435187
7.178639	548.465420	9.440205
7.324943	537.552162	9.445223
7.314343	537.808552	9.450240
7.376778	554.231597	9.455258
7.429368	541.596121	9.460275
7.118554	549.967081	9.465293
7.144133	533.327358	9.470311
7.420996	539.690712	9.475328
7.305225	558.451519	9.480346
7.570906	549.255440	9.485363
7.520338	535.504164	9.490381
7.598336	544.279439	9.495399
7.346945	534.950472	9.500416
7.351592	507.644013	9.505434
7.345315	529.074020	9.510451
7.120877	543.274236	9.515469
7.206277	528.406808	9.520487
7.120374	541.107772	9.525504
7.479564	553.382732	9.530522
7.882057	553.582959	9.535539
7.415071	552.254998	9.540557
7.508046	521.449561	9.545575
7.438219	529.868065	9.550592
7.159050	542.231880	9.555610
7.288357	545.600883	9.560627
7.424748	548.116394	9.565645
7.745399	545.812154	9.570663
7.459138	544.702584	9.575680
7.290809	542.719633	9.580698
7.780519	530.906952	9.585715
7.527620	542.024059	9.590733
7.397502	533.131026	9.595751
7.332438	519.037965	9.600768
7.330936	528.451783	9.605786
7.662189	546.411645	9.610803
7.554676	556.802570	9.615821
7.822633	536.828535	9.620839
7.605813	530.564352	9.625856
7.499962	530.152718	9.630874
7.893550	522.175621	9.635891
7.438062	525.094957	9.640909
7.524320	524.860671	9.645927
7.432612	534.567273	9.650944
7.521979	530.259014	9.655962
7.536111	521.084448	9.660979
7.479450	537.915336	9.665997
7.456548	532.911361	9.671015
7.286131	553.849677	9.676032
7.368817	550.741688	9.681050
8.149956	550.181900	9.686067
7.648620	553.736496	9.691085
7.865724	530.511058	9.696103
7.976789	529.654638	9.701120
7.935094	543.566362	9.706138
7.992736	535.066787	9.711155
7.819819	519.322038	9.716173
7.688073	521.179891	9.721191
7.715289	532.969494	9.726208
7.724249	539.597629	9.731226
7.821480	540.582545	9.736243
7.833267	529.863913	9.741261
7.577398	528.911383	9.746279
7.631426	509.954642	9.751296
7.282007	537.303685	9.756314
7.667690	545.128367	9.761331
7.472643	526.904993	9.766349
7.566709	515.159576	9.771367
7.846819	541.141663	9.776384
7.541236	538.717449	9.781402
7.944798	520.408443	9.786419
7.805148	535.517707	9.791437
7.637211	538.993687	9.796455
7.820941	521.406347	9.801472
7.403609	527.058368	9.806490
7.289468	526.778087	9.811507
7.759271	540.665599	9.816525
7.816302	569.737874	9.821543
8.081492	570.209050	9.826560
7.548588	547.029597	9.831578
8.237121	537.331681	9.836595
7.724147	537.169262	9.841613
7.627417	535.684080	9.846631
7.779274	538.027595	9.851648
7.553872	566.434731	9.856666
7.710568	559.852287	9.861683
7.603015	570.304729	9.866701
7.577368	571.371648	9.871719
7.633355	548.490926	9.876736
7.908111	567.609237	9.881754
8.146001	567.063063	9.886771
7.932649	569.882764	9.891789
7.954285	566.227044	9.896807
7.978418	567.073493	9.901824
7.975913	568.448901	9.906842
7.936170	546.580674	9.911859
7.718101	560.691196	9.916877
7.787376	568.024629	9.921895
7.954791	560.497962	9.926912
7.573897	583.593835	9.931930
7.919434	556.967461	9.936947
7.948201	569.913206	9.941965
7.862680	565.463807	9.946983
8.006345	549.309822	9.952000
7.509814	566.936163	9.957018
7.874627	593.635732	9.962035
7.913814	599.077926	9.967053
8.266579	592.730317	9.972071
8.203744	580.037920	9.977088
7.851307	581.685763	9.982106
8.074179	574.577364	9.987123
7.912531	578.085966	9.992141
8.081474	586.726092	9.997159
8.330621	592.066677	10.002176
7.685714	597.421877	10.007194
7.934497	597.578726	10.012211
8.461964	592.929622	10.017229
7.982375	605.913553	10.022247
8.336745	594.903484	10.027264
7.991866	593.065712	10.032282
8.182610	580.146618	10.037299
8.133822	589.508264	10.042317
7.932839	580.917287	10.047335
8.127218	591.806030	10.052352
7.985624	585.003852	10.057370
8.172365	595.357296	10.062387
8.087316	597.841222	10.067405
8.060649	593.125565	10.072423
8.192094	599.309982	10.077440
8.089293	593.002134	10.082458
8.443462	578.791622	10.087475
8.148533	585.714908	10.092493
8.037251	614.562105	10.097511
8.192857	587.964012	10.102528
8.207936	591.056610	10.107546
8.296466	590.248092	10.112563
8.110860	594.685596	10.117581
8.204501	592.505058	10.122599
8.270109	593.924414	10.127616
8.080947	584.947829	10.132634
8.144806	598.257675	10.137651
8.204473	608.040463	10.142669
8.095666	598.404113	10.147687
8.350937	585.863220	10.152704
8.261669	597.607474	10.157722
8.125332	595.585970	10.162739
8.505538	600.558147	10.167757
8.244465	590.920004	10.172775
8.162041	605.997053	10.177792
8.091649	595.194343	10.182810
8.270668	579.009492	10.187827
7.998735	586.462295	10.192845
8.168647	613.709713	10.197863
8.455469	608.811082	10.202880
8.235685	617.232964	10.207898
8.306445	628.372709	10.212915
8.550057	629.672421	10.217933
8.733864	649.889031	10.222951
8.319355	613.659037	10.227968
8.257361	611.483749	10.232986
8.388985	621.858719	10.238003
8.479847	615.287230	10.243021
8.493194	632.476728	10.248039
8.095587	624.172381	10.253056
8.580602	632.540185	10.258074
8.386127	643.722001	10.263091
8.481942	622.954576	10.268109
8.559837	622.006907	10.273127
8.557959	619.883969	10.278144
8.579514	643.117700	10.283162
8.495905	628.443511	10.288179
8.664096	641.410653	10.293197
8.523048	625.494728	10.298215
8.854863	636.552570	10.303232
8.366119	614.334053	10.308250
8.367265	603.484389	10.313267
8.709730	626.446127	10.318285
8.269190	649.733304	10.323303
8.607054	629.317299	10.328320
8.617210	624.892513	10.333338
8.691566	622.298146	10.338355
8.575138	633.768746	10.343373
8.386721	637.683053	10.348391
8.765598	614.716894	10.353408
8.740002	623.035546	10.358426
8.871008	634.349246	10.363443
9.006473	619.147660	10.368461
8.579487	602.140644	10.373479
8.591697	589.824015	10.378496
8.410906	598.754949	10.383514
8.611835	599.401760	10.388531
8.733153	605.635377	10.393549
8.572008	629.411736	10.398567
8.664590	626.288518	10.403584
8.625679	619.092686	10.408602
8.917483	637.236685	10.413619
8.962428	624.077350	10.418637
8.591740	609.719247	10.423655
8.564054	618.018366	10.428672
8.626939	611.453765	10.433690
8.541083	630.137002	10.438707
8.822945	616.184793	10.443725
8.610677	625.326990	10.448743
8.842138	635.478834	10.453760
8.728096	644.608550	10.458778
8.913842	626.516367	10.463795
8.827203	617.386537	10.468813
8.554846	638.227379	10.473831
8.681166	628.916721	10.478848
8.652898	625.352380	10.483866
8.570149	614.791300	10.488883
8.989820	623.382633	10.493901
8.608848	648.823936	10.498919
8.826289	639.112394	10.503936
8.803914	636.814839	10.508954
8.603683	617.522822	10.513971
8.588984	630.044128	10.518989
8.895805	639.139321	10.524007
8.759546	622.659671	10.529024
8.800581	634.223902	10.534042
8.650721	636.441258	10.539059
8.982903	636.425708	10.544077
8.907059	636.752510	10.549095
9.039855	657.780489	10.554112
8.859658	655.295685	10.559130
8.938793	649.284136	10.564147
9.200173	643.740368	10.569165
8.888422	644.921483	10.574183
8.921020	623.702032	10.579200
8.937826	643.616401	10.584218
8.911592	668.516274	10.589235
9.044871	645.156325	10.594253
9.125361	666.408845	10.599271
9.269512	654.300614	10.604288
9.286852	628.475294	10.609306
8.745377	629.427908	10.614323
9.154016	643.583719	10.619341
8.623937	633.007302	10.624359
9.096124	639.782885	10.629376
9.387408	660.628519	10.634394
8.921320	647.418120	10.639411
9.350367	648.178078	10.644429
9.238565	643.397560	10.649447
9.209966	644.157871	10.654464
9.042366	624.496379	10.659482
8.820054	620.177709	10.664499
9.334697	634.325637	10.669517
9.017661	653.393270	10.674535
9.035977	635.648145	10.679552
9.097882	633.756134	10.684570
9.305434	646.037730	10.689587
9.435343	661.562879	10.694605
8.902509	651.334939	10.699623
8.880550	635.023935	10.704640
9.328540	657.430831	10.709658
9.203669	658.111310	10.714675
9.543437	663.175500	10.719693
9.205376	664.387532	10.724711
9.087884	643.689768	10.729728
9.130794	642.535437	10.734746
8.903028	660.183397	10.739763
9.013131	651.862045	10.744781
9.177644	661.481123	10.749799
9.466438	661.562482	10.754816
9.655475	649.638320	10.759834
9.385963	664.892168	10.764851
9.511369	658.560457	10.769869
9.135105	667.307257	10.774887
9.162038	662.000499	10.779904
9.361872	667.175390	10.784922
9.313543	654.492340	10.789939
9.334249	635.994763	10.794957
9.347254	653.700931	10.799975
9.278589	662.907978	10.804992
9.604742	658.646160	10.810010
9.414111	649.024187	10.815027
9.537283	649.263884	10.820045
9.364422	672.627300	10.825063
9.473775	673.729480	10.830080
9.423532	657.253684	10.835098
9.491136	645.133018	10.840115
9.580587	648.028939	10.845133
9.590785	672.856478	10.850151
9.343470	655.434974	10.855168
9.470613	643.921427	10.860186
9.215567	658.289460	10.865203
9.289188	657.445813	10.870221
9.146459	652.680734	10.875239
9.342630	662.449657	10.880256
9.756051	663.943790	10.885274
9.561092	654.507222	10.890291
9.080821	658.324528	10.895309
9.623090	649.416645	10.900327
9.497298	645.436939	10.905344
9.478327	664.431911	10.910362
9.518457	657.610984	10.915379
9.818468	652.170544	10.920397
9.773408	668.630763	10.925415
9.638526	659.305393	10.930432
9.834460	638.523468	10.935450
9.450480	662.785497	10.940467
9.334452	680.338952	10.945485
9.556539	673.149361	10.950503
9.515663	651.721502	10.955520
9.443728	658.234057	10.960538
9.280153	678.043670	10.965555
9.373497	667.073734	10.970573
9.399227	671.875145	10.975591
9.476942	693.508275	10.980608
9.909613	691.010744	10.985626
9.730868	684.410866	10.990643
9.944649	678.653063	10.995661
9.746110	681.012882	11.000679
9.570994	671.784483	11.005696
9.642560	671.824399	11.010714
9.758664	680.223674	11.015731
9.833105	689.929190	11.020749
10.125167	678.368586	11.025767
9.509568	676.272868	11.030784
9.589497	678.937459	11.035802
9.859709	693.791206	11.040819
9.938018	669.593879	11.045837
9.785781	681.465502	11.050855
9.801251	685.878365	11.055872
10.098464	672.567782	11.060890
9.810782	674.880931	11.065907
9.791611	661.038058	11.070925
9.846153	647.995588	11.075943
9.699955	652.946041	11.080960
9.958213	681.133737	11.085978
9.931336	685.976613	11.090995
10.048943	680.945139	11.096013
9.706736	676.010317	11.101031
9.890832	670.935191	11.106048
10.267929	663.098405	11.111066
9.617040	666.670754	11.116083
10.033422	681.525327	11.121101
10.196913	674.530309	11.126119
9.853975	664.645975	11.131136
10.017077	668.756461	11.136154
9.839298	653.045440	11.141171
9.915012	643.614136	11.146189
9.701787	667.270455	11.151207
9.848717	678.356518	11.156224
9.964139	672.492958	11.161242
9.901614	701.394644	11.166259
9.873320	687.990242	11.171277
10.215029	699.355957	11.176295
9.911680	696.726483	11.181312
10.202748	670.421919	11.186330
10.054035	698.302987	11.191347
10.128353	698.953012	11.196365
10.210254	693.213061	11.201383
9.857723	692.448101	11.206400
9.904062	687.691520	11.211418
9.939714	690.204418	11.216435
9.967371	678.065236	11.221453
10.128141	707.694688	11.226471
9.613790	701.326003	11.231488
9.966254	677.912367	11.236506
9.903203	692.951957	11.241523
10.060420	674.750388	11.246541
10.433430	684.895798	11.251559
10.198180	688.705092	11.256576
10.257575	684.562133	11.261594
10.316981	689.324135	11.266611
10.210410	699.560714	11.271629
10.017953	684.737870	11.276647
10.111788	695.332069	11.281664
10.488204	707.646619	11.286682
10.150136	694.844631	11.291699
10.184367	710.984298	11.296717
10.413090	714.134602	11.301735
10.301718	707.745371	11.306752
10.766998	709.058938	11.311770
10.423943	685.011807	11.316787
10.223819	675.114100	11.321805
10.503061	692.221645	11.326823
10.272030	704.297002	11.331840
10.165112	675.863418	11.336858
9.833363	690.771080	11.341875
10.296542	710.562571	11.346893
10.324230	719.408350	11.351911
10.742136	718.571667	11.356928
10.662002	719.661376	11.361946
10.590393	708.471492	11.366963
10.498291	689.136522	11.371981
10.417315	683.853591	11.376999
10.394094	696.540980	11.382016
10.509957	704.668532	11.387034
10.364088	683.946867	11.392051
10.258862	671.751127	11.397069
10.365301	692.882991	11.402087
10.740198	723.113923	11.407104
10.158851	699.072202	11.412122
10.338285	699.467419	11.417139
10.283726	703.234164	11.422157
10.735830	720.050154	11.427175
10.643326	729.366664	11.432192
10.673379	706.903758	11.437210
10.791746	708.052666	11.442227
10.670877	704.579770	11.447245
10.558462	706.462001	11.452263
10.575882	711.425877	11.457280
10.736989	701.032847	11.462298
10.743265	684.323431	11.467315
10.497267	685.934311	11.472333
10.803655	690.909761	11.477351
10.277897	691.942633	11.482368
10.747251	677.524660	11.487386
10.561072	694.933567	11.492403
10.264901	719.986862	11.497421
10.538951	725.203824	11.502439
10.813251	725.261602	11.507456
10.805096	705.879972	11.512474
10.753590	712.349815	11.517491
10.363624	732.612547	11.522509
10.425520	715.437040	11.527527
10.685855	714.985846	11.532544
10.740323	703.011656	11.537562
10.880576	716.567475	11.542579
10.544440	733.341640	11.547597
10.855936	714.963683	11.552615
10.685899	729.266271	11.557632
10.713162	707.843998	11.562650
10.696605	726.685342	11.567667
10.700082	725.051728	11.572685
10.920992	711.998733	11.577703
10.448321	716.722426	11.582720
10.569252	720.358726	11.587738
10.704581	710.783805	11.592755
10.666822	721.916951	11.597773
11.090791	733.564787	11.602791
10.633265	741.153031	11.607808
11.263746	755.060629	11.612826
11.233424	739.312458	11.617843
10.454219	722.519378	11.622861
10.979261	733.027486	11.627879
11.226314	759.712563	11.632896
10.750493	734.791864	11.637914
10.779045	731.492543	11.642931
10.768655	760.428726	11.647949
11.016149	745.018788	11.652967
11.260990	748.924993	11.657984
11.634825	748.264836	11.663002
11.118806	746.328097	11.668019
10.820537	725.484356	11.673037
10.991812	705.420692	11.678055
10.669357	728.551602	11.683072
11.012803	730.914260	11.688090
11.353043	755.024479	11.693107
11.038471	761.430560	11.698125
11.395781	750.755435	11.703143
11.256574	719.619955	11.708160
10.764841	720.401209	11.713178
11.232899	736.947626	11.718195
10.805574	738.290525	11.723213
11.366502	734.579199	11.728231
11.311449	753.750572	11.733248
11.214397	737.135319	11.738266
11.274113	715.615767	11.743283
10.821920	722.134019	11.748301
11.298745	740.374007	11.753319
11.303447	748.673454	11.758336
11.120389	725.664397	11.763354
11.007081	725.393224	11.768371
10.989385	752.972008	11.773389
11.417510	738.248178	11.778407
11.140862	755.386452	11.783424
11.261855	739.809385	11.788442
11.353769	742.480961	11.793459
11.281247	752.749931	11.798477
11.534875	749.395994	11.803495
11.469532	753.568264	11.808512
11.392378	761.295082	11.813530
11.676351	746.062432	11.818547
11.264355	732.462413	11.823565
11.249417	734.829488	11.828583
11.103490	746.061215	11.833600
11.164579	749.230175	11.838618
11.223877	730.893679	11.843635
11.404912	746.393048	11.848653
11.042621	754.675311	11.853671
11.030343	756.835903	11.858688
10.951060	735.286158	11.863706
11.271562	739.272352	11.868723
11.082216	755.106289	11.873741
11.207441	749.369785	11.878759
11.369658	763.106316	11.883776
11.438606	774.763160	11.888794
11.680815	773.097272	11.893811
11.730189	785.411909	11.898829
11.400424	763.850579	11.903847
11.563221	772.885718	11.908864
11.682671	769.206799	11.913882
11.753401	749.164219	11.918899
11.619591	744.585481	11.923917
11.351680	750.078675	11.928935
11.437127	748.208835	11.933952
11.664649	766.246122	11.938970
11.680277	774.243955	11.943987
11.726945	765.485407	11.949005
11.586461	754.447483	11.954023
11.550790	764.647396	11.959040
11.514490	778.987461	11.964058
11.680062	763.422977	11.969075
11.382671	757.499685	11.974093
11.834367	749.763686	11.979111
11.754597	772.607675	11.984128
11.535971	772.896970	11.989146
12.011572	761.127182	11.994163
11.578977	748.782482	11.999181
11.665913	763.775118	12.004199
11.878142	770.888522	12.009216
11.798258	763.631400	12.014234
11.770127	761.451479	12.019251
11.741609	765.593361	12.024269
11.597014	751.543930	12.029287
11.969589	748.014572	12.034304
11.773662	754.061764	12.039322
11.896500	747.161793	12.044339
11.913788	754.237737	12.049357
11.976845	770.995667	12.054375
11.746450	762.665285	12.059392
11.924603	752.577589	12.064410
12.344844	750.439586	12.069427
12.063813	761.152357	12.074445
11.985883	750.298044	12.079463
12.158425	771.654758	12.084480
11.996435	767.070240	12.089498
11.944468	741.415982	12.094515
11.763643	742.744517	12.099533
12.037803	745.249596	12.104551
12.121602	744.919774	12.109568
11.934737	760.499438	12.114586
12.044124	741.475895	12.119603
12.067401	761.145811	12.124621
12.084220	748.220188	12.129639
12.088193	724.801979	12.134656
11.763953	725.779117	12.139674
12.082123	741.268316	12.144691
12.001593	762.075461	12.149709
12.201514	772.861280	12.154727
12.293247	759.235558	12.159744
11.919910	750.155093	12.164762
12.219864	751.180419	12.169779
12.078524	749.405029	12.174797
12.156871	764.346934	12.179815
12.250448	760.674261	12.184832
12.007753	744.849989	12.189850
12.047921	749.764362	12.194867
12.049700	770.141787	12.199885
11.992596	769.476290	12.204903
12.327599	745.759218	12.209920
11.721690	760.517128	12.214938
12.197263	763.449827	12.219955
11.899535	758.672150	12.224973
11.641171	752.887056	12.229991
11.828164	757.765852	12.235008
12.217549	764.775588	12.240026
12.524100	756.125141	12.245043
12.222622	759.577484	12.250061
11.978133	773.877952	12.255079
12.317684	771.310780	12.260096
12.365989	796.399376	12.265114
12.462512	788.901335	12.270131
12.457332	790.185695	12.275149
12.620745	774.389729	12.280167
12.332831	771.311450	12.285184
12.331315	796.363508	12.290202
12.476649	784.059066	12.295219
12.454578	790.541690	12.300237
12.599183	780.617549	12.305255
12.435378	766.354701	12.310272
12.321280	775.564896	12.315290
12.699975	777.742650	12.320307
12.663735	763.949244	12.325325
12.165469	751.678763	12.330343
12.241046	766.676034	12.335360
12.694793	781.010985	12.340378
12.508270	784.598331	12.345395
12.274628	808.911022	12.350413
12.227423	790.062372	12.355431
12.790259	793.345716	12.360448
12.427525	791.141283	12.365466
12.812607	791.290076	12.370483
12.745029	782.595661	12.375501
12.725569	796.275457	12.380519
12.756648	790.424018	12.385536
12.551466	778.306211	12.390554
12.597627	789.754684	12.395571
12.572044	800.921398	12.400589
12.697197	787.328405	12.405607
12.833594	778.367768	12.410624
12.394350	802.543605	12.415642
12.661989	795.171966	12.420659
12.713270	787.389846	12.425677
12.848965	778.538154	12.430695
12.991181	791.990199	12.435712
12.466287	792.022314	12.440730
12.660070	779.603401	12.445747
12.358862	805.908715	12.450765
12.256238	791.043764	12.455783
12.684961	773.505881	12.460800
12.765624	789.399537	12.465818
12.517658	800.043601	12.470835
12.627032	799.204272	12.475853
12.465859	814.732513	12.480871
12.963146	807.713170	12.485888
12.822318	826.192893	12.490906
13.082005	820.675023	12.495923
12.903776	823.805123	12.500941
13.008667	816.692494	12.505959
13.058135	814.207200	12.510976
12.767705	823.544864	12.515994
12.987900	813.171808	12.521011
13.148917	801.325073	12.526029
12.694444	820.212234	12.531047
13.385864	829.434682	12.536064
13.038723	823.041167	12.541082
13.161614	802.678955	12.546099
13.279659	800.173967	12.551117
12.984392	806.642410	12.556135
12.743899	796.084739	12.561152
13.320477	797.031686	12.566170
13.568854	793.991026	12.571187
13.596484	785.397282	12.576205
13.307873	782.417417	12.581223
13.340401	791.258502	12.586240
12.770772	785.139306	12.591258
13.155603	782.164362	12.596275
12.977321	789.516179	12.601293
12.861322	780.893825	12.606311
13.425490	767.503818	12.611328
12.853383	783.300768	12.616346
12.675990	789.626825	12.621363
13.376322	790.762518	12.626381
12.862444	812.979180	12.631399
13.069691	792.270058	12.636416
12.767868	805.485143	12.641434
13.147451	800.901645	12.646451
13.279152	801.607234	12.651469
12.973296	821.888360	12.656487
13.306792	814.477589	12.661504
13.452066	807.682614	12.666522
13.351337	790.581917	12.671539
13.402432	813.355929	12.676557
13.228673	820.547606	12.681575
13.306705	806.968188	12.686592
13.354941	809.217777	12.691610
13.219664	806.858953	12.696627
13.313728	818.382580	12.701645
13.143694	816.425950	12.706663
13.475642	812.635842	12.711680
13.296610	836.420890	12.716698
13.674465	825.852131	12.721715
13.684648	805.772940	12.726733
13.446756	824.414036	12.731751
13.559448	809.943687	12.736768
13.284710	807.295492	12.741786
13.349641	819.939290	12.746803
13.488626	842.112262	12.751821
13.706836	831.562207	12.756839
14.101005	840.253522	12.761856
13.573942	843.567617	12.766874
13.501865	822.886902	12.771891
13.434160	805.460833	12.776909
13.455263	798.472167	12.781927
13.383568	825.013136	12.786944
13.966752	858.975957	12.791962
13.427367	850.366163	12.796979
13.623003	835.142808	12.801997
13.597704	829.308542	12.807015
13.601733	842.451862	12.812032
13.829567	841.539130	12.817050
13.760304	839.220364	12.822067
13.688085	859.863515	12.827085
13.587147	850.408239	12.832103
13.825675	833.611277	12.837120
13.734612	851.258514	12.842138
13.723321	862.120627	12.847155
13.650170	852.946608	12.852173
13.512299	854.200060	12.857191
13.755369	834.344187	12.862208
14.005278	845.236531	12.867226
13.903231	857.217681	12.872243
14.270837	838.599064	12.877261
14.006776	833.154753	12.882279
13.768038	852.122020	12.887296
13.844890	845.110835	12.892314
13.900779	831.941346	12.897331
14.056498	848.518245	12.902349
13.701333	855.235915	12.907367
14.046633	846.513676	12.912384
14.131421	847.555280	12.917402
14.234864	835.628587	12.922419
14.227497	842.776051	12.927437
14.073579	858.462938	12.932455
14.065274	840.902538	12.937472
13.852701	835.201849	12.942490
13.909432	841.787584	12.947507
14.119163	839.306208	12.952525
14.264878	842.041923	12.957543
14.536690	843.967047	12.962560
14.446516	844.332531	12.967578
14.367040	819.883653	12.972595
14.514821	823.313723	12.977613
14.023495	807.531653	12.982631
13.893728	809.889869	12.987648
14.164765	821.273258	12.992666
14.392400	825.124270	12.997683
14.134421	807.277892	13.002701
13.929872	791.013327	13.007719
14.266657	821.005049	13.012736
14.366997	819.197191	13.017754
14.318327	831.882995	13.022771
14.324743	829.939811	13.027789
14.039938	825.014346	13.032807
14.466238	815.296714	13.037824
14.459706	836.795780	13.042842
14.246777	835.138973	13.047859
14.673689	828.637516	13.052877
14.307744	815.996488	13.057895
14.041272	801.140695	13.062912
14.240576	817.324731	13.067930
14.480779	844.836168	13.072947
14.729699	829.821279	13.077965
14.316095	834.898537	13.082983
14.802838	844.180500	13.088000
14.094833	811.580673	13.093018
14.087328	820.531709	13.098035
14.467178	842.952500	13.103053
14.389776	841.494204	13.108071
14.291677	839.526667	13.113088
14.472782	846.321319	13.118106
14.436658	847.009478	13.123123
14.400044	841.110461	13.128141
14.353930	856.935102	13.133159
14.627922	838.986213	13.138176
14.509714	840.719261	13.143194
14.460654	846.030102	13.148211
14.880665	824.812081	13.153229
14.425371	842.705572	13.158247
14.603999	841.460805	13.163264
14.813426	827.968583	13.168282
14.207441	835.180527	13.173299
14.246528	838.546005	13.178317
14.517230	861.272777	13.183335
14.335776	855.903661	13.188352
14.560659	869.341917	13.193370
15.171363	862.250769	13.198387
15.374555	875.094542	13.203405
14.591484	859.033846	13.208423
14.651678	855.274860	13.213440
14.771009	851.461232	13.218458
14.886316	853.425602	13.223475
15.044343	869.055145	13.228493
14.840968	854.514280	13.233511
14.760196	848.282686	13.238528
14.768518	852.054328	13.243546
14.781678	867.935801	13.248563
14.993329	845.337985	13.253581
15.067651	855.544381	13.258599
14.696127	876.530936	13.263616
15.158286	876.855724	13.268634
15.148327	875.822780	13.273651
15.162860	848.832893	13.278669
14.947211	842.691289	13.283687
14.869229	849.440296	13.288704
15.097402	862.993917	13.293722
15.356046	870.214432	13.298739
15.028954	846.185171	13.303757
15.140991	846.731160	13.308775
14.776082	844.628331	13.313792
15.097460	849.529230	13.318810
14.930254	851.250400	13.323827
14.879560	874.332882	13.328845
14.982509	869.209797	13.333863
15.110786	856.301974	13.338880
15.167454	860.754622	13.343898
15.244178	888.354751	13.348915
15.355554	859.947332	13.353933
15.352176	853.723020	13.358951
15.078636	872.198555	13.363968
15.090065	878.591844	13.368986
15.022997	875.177422	13.374003
15.226877	854.156847	13.379021
15.138800	851.025750	13.384039
15.277331	872.932868	13.389056
15.243442	862.586319	13.394074
14.855551	864.712270	13.399091
15.262946	867.390183	13.404109
15.325783	854.528993	13.409127
15.166153	843.178109	13.414144
15.191528	857.122133	13.419162
15.377833	899.377033	13.424179
15.231556	886.915338	13.429197
15.656080	877.661915	13.434215
15.547789	881.257511	13.439232
15.633317	896.157227	13.444250
15.530184	889.069395	13.449267
15.740029	867.615447	13.454285
15.868698	865.587800	13.459303
15.555778	858.962296	13.464320
15.948419	851.493714	13.469338
15.603255	853.250394	13.474355
15.633482	849.007808	13.479373
15.406043	852.763306	13.484391
15.265939	829.991615	13.489408
15.930104	837.822777	13.494426
15.907966	861.296283	13.499443
16.096032	859.138479	13.504461
15.834823	853.830661	13.509479
15.549304	860.180519	13.514496
16.109381	845.991131	13.519514
15.738963	849.683960	13.524531
15.738998	842.748152	13.529549
15.550471	865.301081	13.534567
15.564339	846.330387	13.539584
15.746258	841.376301	13.544602
15.410698	855.033307	13.549619
15.784205	843.411396	13.554637
15.674078	853.613242	13.559655
15.324350	878.219860	13.564672
15.727825	854.334554	13.569690
15.730074	852.648583	13.574707
15.885157	855.532713	13.579725
15.798522	854.359037	13.584743
15.798970	856.677537	13.589760
15.884510	877.613163	13.594778
15.446621	882.196350	13.599795
15.977492	867.325431	13.604813
16.003885	883.232975	13.609831
15.695597	886.477666	13.614848
15.677677	878.067533	13.619866
16.096244	893.138727	13.624883
15.808225	875.552187	13.629901
16.089890	895.374997	13.634919
15.733620	891.332947	13.639936
16.287548	876.901401	13.644954
16.105546	881.600136	13.649971
16.151594	886.529030	13.654989
16.426445	869.513089	13.660007
16.015949	891.226882	13.665024
15.880419	878.414295	13.670042
15.907516	877.001604	13.675059
16.118606	877.244586	13.680077
15.984512	885.199225	13.685095
15.883058	881.941626	13.690112
16.331512	900.806118	13.695130
16.250229	917.654186	13.700147
16.180636	901.494237	13.705165
16.389318	893.275428	13.710183
16.387692	914.668997	13.715200
16.388133	890.867358	13.720218
16.421795	901.814960	13.725235
16.023321	898.620807	13.730253
16.364371	886.785681	13.735271
16.311656	889.666569	13.740288
16.716943	899.366843	13.745306
16.617468	911.910655	13.750323
16.604154	892.697019	13.755341
16.411224	878.581362	13.760359
16.253494	884.744112	13.765376
16.251301	883.416457	13.770394
16.532105	889.249326	13.775411
16.689571	910.830323	13.780429
16.875548	905.146992	13.785447
16.610518	886.823856	13.790464
16.863943	875.186341	13.795482
16.552653	888.714596	13.800499
16.239858	900.380205	13.805517
16.416578	881.316727	13.810535
16.494730	885.403721	13.815552
16.739945	881.424636	13.820570
16.546209	865.980334	13.825587
16.414648	871.690741	13.830605
16.479316	908.317331	13.835623
16.436225	918.287333	13.840640
16.772231	891.786724	13.845658
16.840181	893.804681	13.850675
16.567057	912.283836	13.855693
16.829524	921.044883	13.860711
16.789944	906.891657	13.865728
16.890120	898.323942	13.870746
16.631646	924.879714	13.875763
16.741653	919.580098	13.880781
16.953287	910.076771	13.885799
16.483443	910.492010	13.890816
16.865887	918.793479	13.895834
16.956447	897.070398	13.900851
16.608279	902.421240	13.905869
17.191508	914.024397	13.910887
16.871666	926.486754	13.915904
17.344708	902.364836	13.920922
16.968589	902.899591	13.925939
17.005380	910.700249	13.930957
17.229678	905.273904	13.935975
16.933669	906.800181	13.940992
16.639956	894.971053	13.946010
17.075234	912.450496	13.951027
16.750023	919.663903	13.956045
17.101921	908.920683	13.961063
16.698364	913.425784	13.966080
16.785778	913.040257	13.971098
16.825199	915.263176	13.976115
16.993313	924.217231	13.981133
17.434671	929.300245	13.986151
17.418721	934.792704	13.991168
17.042839	911.705712	13.996186
16.875363	927.855718	14.001203
17.222878	939.367565	14.006221
17.489868	928.847954	14.011239
17.179644	944.264772	14.016256
17.389843	932.156526	14.021274
17.611173	920.710748	14.026291
17.500287	933.973111	14.031309
17.445590	905.757380	14.036327
17.286788	893.787189	14.041344
17.747434	905.656498	14.046362
17.375674	901.497547	14.051379
17.288101	907.799265	14.056397
17.453182	892.350154	14.061415
17.238138	900.902280	14.066432
17.170588	907.139680	14.071450
17.677181	912.172155	14.076467
17.547414	912.931288	14.081485
17.845196	903.559263	14.086503
17.454481	911.548550	14.091520
17.587596	907.248207	14.096538
17.623703	881.350478	14.101555
17.475233	886.548661	14.106573
17.443300	894.269451	14.111591
17.588102	908.271817	14.116608
17.791703	914.764926	14.121626
17.910618	895.651352	14.126643
17.406805	891.125153	14.131661
17.537537	905.413528	14.136679
17.650362	914.009289	14.141696
18.084959	907.031356	14.146714
17.731688	910.549264	14.151731
17.663568	895.661683	14.156749
17.880340	884.430114	14.161767
17.772358	901.896002	14.166784
17.364537	900.748240	14.171802
17.719342	906.635110	14.176819
17.848418	934.904451	14.181837
18.080662	923.175739	14.186855
17.525954	918.962096	14.191872
17.604618	916.857394	14.196890
17.921073	930.817441	14.201907
17.346891	934.442316	14.206925
17.948325	920.696698	14.211943
17.463162	924.560632	14.216960
17.568320	932.981634	14.221978
18.024849	918.586021	14.226995
17.818439	944.330181	14.232013
17.824245	931.838200	14.237031
17.688891	928.953422	14.242048
17.721764	944.603035	14.247066
18.098485	951.383612	14.252083
17.978907	950.726857	14.257101
18.249277	961.219054	14.262119
18.502053	941.326801	14.267136
18.091438	955.882590	14.272154
18.345602	958.744759	14.277171
18.262506	959.536920	14.282189
18.485888	939.247169	14.287207
18.564310	930.817150	14.292224
18.121847	921.288084	14.297242
18.278935	909.345482	14.302259
18.275022	921.458164	14.307277
18.236959	930.182681	14.312295
18.259058	936.981017	14.317312
18.315868	931.340375	14.322330
18.522806	926.405940	14.327347
18.219990	929.002657	14.332365
18.281330	933.068630	14.337383
18.306506	933.292841	14.342400
18.457002	954.922383	14.347418
18.632150	938.560966	14.352435
18.500572	949.075397	14.357453
18.279226	956.658468	14.362471
18.556599	935.189920	14.367488
18.282830	940.302357	14.372506
18.522732	953.618256	14.377523
18.448286	960.424685	14.382541
18.681194	944.505375	14.387559
18.608514	954.051954	14.392576
18.682727	958.374008	14.397594
18.538599	945.836731	14.402611
18.814971	952.016627	14.407629
18.642312	956.577753	14.412647
18.544390	947.646095	14.417664
18.328964	946.578811	14.422682
18.992627	951.364139	14.427699
18.321691	948.614013	14.432717
18.695094	946.721164	14.437735
18.679030	956.848396	14.442752
18.331425	941.900486	14.447770
18.602916	945.277275	14.452787
18.603962	941.910228	14.457805
18.636778	941.074982	14.462823
18.499539	958.254799	14.467840
18.690534	969.827073	14.472858
18.713259	959.107022	14.477875
18.843665	966.878757	14.482893
19.265225	970.417221	14.487911
19.205981	955.463465	14.492928
18.759793	964.642847	14.497946
19.010890	965.460373	14.502963
18.741407	981.285843	14.507981
18.976875	986.025411	14.512999
19.166818	959.677555	14.518016
19.034650	958.656437	14.523034
19.202320	969.560886	14.528051
18.971094	971.398626	14.533069
19.155693	963.344645	14.538087
19.397749	977.543253	14.543104
19.187650	961.073177	14.548122
19.133280	937.779509	14.553139
19.227529	956.356925	14.558157
19.050277	954.173181	14.563175
18.991693	949.055508	14.568192
18.899244	974.215676	14.573210
19.042320	968.209377	14.578227
19.018653	950.659753	14.583245
19.115314	959.847235	14.588263
19.154742	965.884252	14.593280
18.543334	971.729391	14.598298
19.084502	970.269525	14.603315
18.992526	985.153668	14.608333
18.893746	999.511054	14.613351
19.234534	997.003567	14.618368
19.220877	997.110311	14.623386
19.469619	984.287367	14.628403
19.534852	981.181708	14.633421
19.509913	997.108849	14.638439
19.702172	1008.361732	14.643456
19.472679	995.144896	14.648474
19.676712	984.097918	14.653491
19.666100	1004.128553	14.658509
19.633729	1004.865890	14.663527
19.761150	1003.776287	14.668544
19.598756	991.826588	14.673562
19.675580	976.259063	14.678579
19.590643	990.992479	14.683597
19.727206	1011.425886	14.688615
19.821185	989.622404	14.693632
19.743855	986.138607	14.698650
19.747190	995.236835	14.703667
19.658340	1003.471585	14.708685
19.431145	991.233162	14.713703
20.001587	978.248551	14.718720
19.773575	984.137398	14.723738
19.786739	992.044904	14.728755
19.898146	1014.583125	14.733773
20.021374	996.903098	14.738791
20.055109	986.709126	14.743808
19.865673	990.874414	14.748826
20.082787	978.492149	14.753843
19.903331	985.063422	14.758861
19.826296	990.693129	14.763879
20.230569	991.107977	14.768896
20.083895	979.559649	14.773914
20.203977	989.271663	14.778931
20.080452	981.847013	14.783949
20.048915	994.384659	14.788967
20.363513	972.924790	14.793984
19.991844	995.388988	14.799002
20.240711	985.566057	14.804019
20.444436	985.502659	14.809037
20.384070	979.897229	14.814055
20.188771	990.715919	14.819072
20.305945	981.570912	14.824090
20.128034	972.736295	14.829107
20.161052	973.188779	14.834125
20.205330	975.702070	14.839143
20.315067	988.342417	14.844160
20.254516	991.620778	14.849178
20.620879	988.928305	14.854195
20.353791	973.077248	14.859213
20.149186	971.544413	14.864231
20.302792	968.704569	14.869248
20.316878	975.535046	14.874266
20.412850	987.998776	14.879283
20.400443	1000.871198	14.884301
19.966799	982.433942	14.889319
20.315995	971.970679	14.894336
20.223866	981.667992	14.899354
20.138327	974.686437	14.904371
19.960367	977.398224	14.909389
19.978302	998.154954	14.914407
20.261376	1001.514589	14.919424
20.441285	996.107651	14.924442
20.678288	999.162280	14.929459
20.518436	1023.831727	14.934477
20.559051	1023.608715	14.939495
20.757997	1018.678130	14.944512
20.691178	1012.015530	14.949530
20.840806	1017.753127	14.954547
20.880697	1029.781609	14.959565
20.623691	1029.566353	14.964583
21.044025	1007.242791	14.969600
20.623803	1007.346068	14.974618
20.608522	1025.211043	14.979635
20.880416	1032.763319	14.984653
20.642635	1007.881458	14.989671
20.918518	1007.796493	14.994688
20.869157	1027.263159	14.999706
20.861238	1016.764908	15.004723
20.750515	1005.875684	15.009741
20.589870	1027.284372	15.014759
20.860006	1017.424252	15.019776
20.843442	1021.298154	15.024794
20.881827	1009.795654	15.029811
21.282841	1030.767326	15.034829
20.974469	1042.411058	15.039847
21.050748	1013.009698	15.044864
20.854181	1004.396989	15.049882
20.971655	1033.358610	15.054899
21.369678	1055.038804	15.059917
21.345933	1050.991058	15.064935
21.573262	1027.275895	15.069952
21.276107	1033.077883	15.074970
21.489585	1016.645597	15.079987
21.454394	1014.962844	15.085005
21.053654	1018.370835	15.090023
21.383368	1017.669547	15.095040
20.856947	1010.097318	15.100058
21.215947	1006.451671	15.105075
21.339388	1009.484331	15.110093
21.279791	1001.438211	15.115111
21.239640	1023.841787	15.120128
21.305962	1044.900375	15.125146
21.568791	1026.990601	15.130163
21.776454	1028.931073	15.135181
21.585695	1034.779342	15.140199
21.536876	999.887651	15.145216
21.501651	1008.134501	15.150234
21.440434	1000.630738	15.155251
21.394306	1014.244681	15.160269
21.321672	1040.928861	15.165287
21.843172	1021.163118	15.170304
21.852159	1043.367509	15.175322
21.680288	1026.652127	15.180339
21.600419	994.827118	15.185357
21.428428	1005.702016	15.190375
21.765726	1026.654594	15.195392
21.761594	1036.549256	15.200410
21.726604	1027.230572	15.205427
21.807001	1030.788036	15.210445
21.678441	1039.913202	15.215463
21.739539	1038.611975	15.220480
21.804450	1037.908394	15.225498
22.118324	1024.241593	15.230515
21.943749	1024.690499	15.235533
21.794582	1042.410437	15.240551
22.161940	1029.609576	15.245568
21.801250	1032.564606	15.250586
21.971213	1047.010961	15.255603
22.084849	1033.349394	15.260621
21.944707	1024.649219	15.265639
21.815870	1027.819710	15.270656
21.967817	1052.033545	15.275674
21.711063	1041.874355	15.280691
22.162550	1021.112262	15.285709
21.946223	1023.952218	15.290727
22.098256	1026.685545	15.295744
21.898279	1048.092398	15.300762
22.007251	1044.047027	15.305779
22.215318	1026.255234	15.310797
21.958994	1030.421255	15.315815
21.902466	1034.296745	15.320832
21.722431	1055.447030	15.325850
21.792350	1052.891307	15.330867
22.203598	1046.250551	15.335885
22.131060	1074.701560	15.340903
22.442437	1081.392330	15.345920
22.694208	1072.911151	15.350938
22.174897	1067.625147	15.355955
22.568951	1064.092070	15.360973
22.463243	1061.854864	15.365991
22.453873	1045.906408	15.371008
22.431169	1066.412850	15.376026
22.284870	1071.501215	15.381043
22.748200	1059.567717	15.386061
22.608454	1056.638868	15.391079
22.594091	1061.002452	15.396096
22.452722	1053.840174	15.401114
22.735256	1059.935356	15.406131
22.952995	1039.600156	15.411149
22.819920	1063.849991	15.416167
22.959565	1053.804082	15.421184
22.785992	1059.106052	15.426202
22.776305	1064.033194	15.431219
22.880586	1056.260579	15.436237
22.623996	1045.531519	15.441255
22.897630	1044.397973	15.446272
22.654219	1060.866202	15.451290
22.566396	1063.080846	15.456307
22.928344	1041.588431	15.461325
22.748583	1061.047071	15.466343
22.592335	1062.088275	15.471360
22.702117	1043.431425	15.476378
22.575454	1037.252405	15.481395
22.852524	1054.814344	15.486413
22.637356	1063.863800	15.491431
22.915205	1061.122965	15.496448
23.161640	1073.155528	15.501466
23.301193	1078.866376	15.506483
23.227765	1046.203000	15.511501
22.796040	1045.563186	15.516519
22.942543	1055.719412	15.521536
22.972025	1062.805883	15.526554
23.089630	1073.088618	15.531571
23.154296	1086.460061	15.536589
22.792444	1083.204712	15.541607
23.205460	1085.042769	15.546624
23.253178	1072.147387	15.551642
23.359814	1083.116124	15.556659
23.378015	1095.502583	15.561677
23.143777	1108.268974	15.566695
23.205091	1092.300523	15.571712
23.441029	1073.392432	15.576730
23.496918	1090.183386	15.581747
23.551010	1082.927489	15.586765
23.109776	1094.780375	15.591783
23.168966	1097.008122	15.596800
23.649480	1089.316983	15.601818
23.445182	1074.564400	15.606835
23.799050	1085.078309	15.611853
23.507302	1084.274944	15.616871
23.454009	1088.027600	15.621888
23.519765	1094.649149	15.626906
23.287696	1092.656092	15.631923
23.384509	1079.946047	15.636941
23.436009	1094.782798	15.641959
23.517947	1100.786964	15.646976
23.940808	1115.118675	15.651994
24.156479	1106.842214	15.657011
24.644745	1075.616978	15.662029
24.063494	1082.586130	15.667047
23.957845	1094.918172	15.672064
24.100711	1081.906690	15.677082
23.815911	1072.168449	15.682099
23.834966	1060.635845	15.687117
23.758991	1081.546486	15.692135
23.930462	1084.788001	15.697152
23.988305	1068.979262	15.702170
23.865547	1071.860049	15.707187
24.284584	1061.392466	15.712205
23.712999	1083.357899	15.717223
23.766152	1070.832199	15.722240
24.081589	1065.001266	15.727258
23.790873	1076.656472	15.732275
23.999967	1070.376788	15.737293
23.844092	1069.257735	15.742311
24.121532	1089.766663	15.747328
24.642127	1098.154627	15.752346
24.166942	1080.497623	15.757363
24.097254	1063.519312	15.762381
24.294004	1095.702291	15.767399
24.280432	1105.559886	15.772416
24.564964	1092.060728	15.777434
24.302673	1091.558423	15.782451
24.066158	1095.025197	15.787469
24.299517	1093.092595	15.792487
24.262631	1089.514711	15.797504
24.680797	1103.313066	15.802522
24.668714	1110.596638	15.807539
24.606480	1087.104682	15.812557
24.616484	1091.514530	15.817575
24.418010	1104.905464	15.822592
24.623684	1107.634075	15.827610
24.592037	1099.942153	15.832627
24.674672	1090.230955	15.837645
24.525296	1096.154574	15.842663
24.459310	1113.403774	15.847680
24.646626	1100.923973	15.852698
24.324849	1119.484923	15.857715
25.057271	1106.808468	15.862733
24.976673	1087.876603	15.867751
24.840975	1085.504915	15.872768
24.806229	1102.904809	15.877786
24.629354	1117.667439	15.882803
24.712361	1100.382722	15.887821
25.077633	1090.114214	15.892839
25.059897	1101.182532	15.897856
24.925320	1094.561991	15.902874
24.836699	1092.247959	15.907891
24.799041	1106.728877	15.912909
24.683832	1093.391126	15.917927
24.758768	1110.961047	15.922944
24.860718	1089.831726	15.927962
24.879597	1092.588250	15.932979
24.942316	1098.074262	15.937997
24.975222	1111.765663	15.943015
24.576161	1103.694307	15.948032
24.867945	1082.712913	15.953050
25.063015	1091.948370	15.958067
25.130522	1116.313235	15.963085
25.166568	1135.125038	15.968103
25.067752	1122.444039	15.973120
25.421588	1101.141123	15.978138
24.880896	1122.183128	15.983155
25.118513	1132.920857	15.988173
25.114412	1118.230697	15.993191
25.163650	1121.196724	15.998208
25.132444	1110.288184	16.003226
25.148424	1120.304644	16.008243
25.377261	1130.961265	16.013261
25.466582	1119.087361	16.018279
25.294146	1108.959063	16.023296
25.466401	1134.597672	16.028314
25.243087	1155.029437	16.033331
25.659149	1145.250509	16.038349
25.622628	1138.251038	16.043367
25.499076	1136.596550	16.048384
25.789201	1144.263852	16.053402
25.796568	1131.956050	16.058419
25.966104	1136.538517	16.063437
25.936093	1149.312718	16.068455
26.164611	1125.717255	16.073472
26.282823	1126.480095	16.078490
25.633971	1114.763997	16.083507
26.012409	1106.858671	16.088525
26.111619	1111.872531	16.093543
25.765227	1101.756059	16.098560
26.089985	1108.578062	16.103578
25.998768	1099.360926	16.108595
25.930857	1107.733379	16.113613
25.914868	1103.723698	16.118631
25.616939	1099.215467	16.123648
26.248446	1104.004486	16.128666
25.893293	1112.580276	16.133683
25.980352	1097.123286	16.138701
25.847419	1115.099027	16.143719
25.996023	1120.164653	16.148736
26.220166	1155.782948	16.153754
26.333487	1148.658636	16.158771
26.445263	1122.521080	16.163789
26.424914	1124.481531	16.168807
26.124753	1144.067725	16.173824
26.405965	1131.778729	16.178842
26.530077	1138.579585	16.183859
26.309069	1134.481069	16.188877
26.376168	1125.045578	16.193895
26.571155	1108.595880	16.198912
26.581355	1103.149445	16.203930
26.584337	1093.661100	16.208947
26.162686	1092.721267	16.213965
26.229263	1084.715852	16.218983
26.180864	1133.318383	16.224000
26.566493	1136.827399	16.229018
26.410501	1123.771983	16.234035
26.229025	1138.174556	16.239053
26.401545	1144.291889	16.244071
26.369122	1126.939623	16.249088
26.557520	1130.034095	16.254106
26.491828	1141.736496	16.259123
26.199041	1123.697908	16.264141
26.355392	1128.500116	16.269159
26.740792	1158.170962	16.274176
26.884815	1172.409863	16.279194
26.958693	1161.628375	16.284211
26.775614	1148.819777	16.289229
27.088179	1157.229260	16.294247
26.911277	1175.854506	16.299264
27.060701	1168.205544	16.304282
26.880262	1160.641010	16.309299
26.756512	1150.679892	16.314317
27.050111	1163.605008	16.319335
26.624783	1181.939307	16.324352
26.986738	1163.317589	16.329370
27.020240	1140.412243	16.334387
27.355884	1143.491537	16.339405
27.177616	1156.218902	16.344423
27.159814	1154.319236	16.349440
27.053935	1146.920003	16.354458
26.863111	1156.045491	16.359475
26.963563	1164.595123	16.364493
27.290326	1166.788799	16.369511
27.127409	1158.170245	16.374528
27.096325	1156.635481	16.379546
27.174881	1181.152032	16.384563
27.163997	1178.331460	16.389581
27.509984	1175.300966	16.394599
27.603247	1193.787812	16.399616
27.676850	1178.005975	16.404634
27.909237	1193.169046	16.409651
27.679778	1197.409688	16.414669
27.811460	1171.389794	16.419687
27.524090	1157.569929	16.424704
27.712634	1141.003179	16.429722
27.629124	1145.602667	16.434739
27.431478	1157.413576	16.439757
27.777170	1180.965240	16.444775
27.626528	1178.285943	16.449792
27.637719	1193.008908	16.454810
27.852891	1182.308362	16.459827
28.012742	1175.116028	16.464845
28.237122	1179.785091	16.469863
27.818453	1177.189250	16.474880
27.604097	1154.404941	16.479898
28.116304	1165.318229	16.484915
27.935793	1179.849882	16.489933
28.142812	1168.436691	16.494951
27.776620	1172.379428	16.499968
27.975936	1187.296246	16.504986
28.060929	1171.784221	16.510003
28.043385	1180.966403	16.515021
28.067252	1179.670135	16.520039
27.812492	1169.343739	16.525056
27.945729	1180.485076	16.530074
28.125396	1173.864823	16.535091
27.986173	1182.247133	16.540109
27.908433	1188.620551	16.545127
27.998896	1173.106538	16.550144
28.343643	1176.101480	16.555162
28.374484	1177.623660	16.560179
27.924276	1170.230344	16.565197
28.127120	1161.956071	16.570215
28.146628	1204.233377	16.575232
28.304423	1204.936837	16.580250
28.629076	1207.782189	16.585267
28.220520	1221.733801	16.590285
28.817583	1195.227609	16.595303
28.294154	1201.570771	16.600320
28.119148	1223.377092	16.605338
28.428354	1219.350641	16.610355
28.280464	1202.940577	16.615373
28.654102	1194.987094	16.620391
28.519447	1202.822039	16.625408
28.450814	1197.308204	16.630426
28.568867	1210.104827	16.635443
28.485840	1211.421865	16.640461
29.085315	1212.177702	16.645479
28.724146	1240.375705	16.650496
29.302533	1237.070335	16.655514
29.086084	1215.541694	16.660531
28.681488	1213.929212	16.665549
28.814999	1200.117200	16.670567
28.834330	1207.288270	16.675584
29.055739	1221.240774	16.680602
29.075021	1231.672313	16.685619
29.069821	1231.713207	16.690637
29.354879	1226.033360	16.695655
29.346885	1222.339378	16.700672
29.048139	1205.991338	16.705690
29.501424	1184.444858	16.710707
29.116153	1194.025531	16.715725
29.032954	1186.360880	16.720743
29.184648	1194.079226	16.725760
29.131003	1221.628388	16.730778
29.513076	1215.558193	16.735795
29.407164	1222.865589	16.740813
29.640437	1223.942608	16.745831
29.717469	1220.175437	16.750848
29.434767	1189.396194	16.755866
29.270298	1195.236933	16.760883
29.428199	1221.595803	16.765901
29.362243	1209.794721	16.770919
29.648095	1206.100795	16.775936
29.877442	1225.555606	16.780954
29.859277	1215.599728	16.785971
29.411272	1196.576806	16.790989
29.379718	1204.040271	16.796007
29.510704	1203.934870	16.801024
29.432248	1222.227345	16.806042
29.824802	1218.762084	16.811059
29.608176	1209.611461	16.816077
30.105947	1214.043178	16.821095
30.067907	1222.090557	16.826112
29.845898	1205.797045	16.831130
29.711481	1218.688927	16.836147
29.857095	1195.145828	16.841165
29.783939	1213.056700	16.846183
29.600250	1218.378405	16.851200
29.310046	1218.726275	16.856218
29.786808	1219.613683	16.861235
29.883317	1237.645429	16.866253
30.139195	1255.145762	16.871271
30.496915	1239.446999	16.876288
30.272739	1243.965062	16.881306
30.205493	1237.941851	16.886323
30.391551	1241.400721	16.891341
30.643843	1225.454988	16.896359
30.099607	1227.621584	16.901376
30.278679	1201.826625	16.906394
30.128167	1205.958675	16.911411
30.173637	1227.066323	16.916429
30.356295	1237.269833	16.921447
30.393450	1245.479561	16.926464
30.148249	1261.775311	16.931482
30.624484	1244.343383	16.936499
30.409458	1238.822038	16.941517
30.471755	1238.577532	16.946535
30.601671	1250.930306	16.951552
30.411361	1249.709869	16.956570
30.794773	1228.865952	16.961587
30.317912	1239.536435	16.966605
30.350295	1243.504938	16.971623
30.621073	1234.287828	16.976640
30.601308	1238.548738	16.981658
30.812241	1243.518102	16.986675
30.217569	1251.988014	16.991693
30.460669	1258.573341	16.996711
30.848474	1255.932975	17.001728
30.688175	1292.103191	17.006746
31.148792	1273.477533	17.011763
31.171730	1261.797123	17.016781
31.341348	1253.835109	17.021799
31.619433	1268.287423	17.026816
31.276938	1259.578830	17.031834
31.191140	1230.673114	17.036851
30.933551	1226.536337	17.041869
31.104580	1222.172569	17.046887
31.238339	1247.187759	17.051904
31.519008	1249.120525	17.056922
31.475573	1241.758553	17.061939
31.174972	1241.282155	17.066957
31.142727	1213.459984	17.071975
31.334422	1220.489021	17.076992
31.450409	1253.948669	17.082010
31.294788	1257.533380	17.087027
31.293051	1249.139753	17.092045
31.560557	1265.278456	17.097063
31.824248	1262.658401	17.102080
31.624022	1274.866684	17.107098
31.864426	1247.615787	17.112115
31.314968	1235.060135	17.117133
31.585197	1244.204936	17.122151
31.660678	1243.426585	17.127168
31.559695	1263.661943	17.132186
32.094944	1249.879736	17.137203
31.625049	1249.991714	17.142221
31.569366	1255.768053	17.147239
31.678004	1252.876743	17.152256
31.496881	1251.756535	17.157274
31.760641	1241.383470	17.162291
31.516467	1263.451416	17.167309
31.545759	1257.123433	17.172327
31.896486	1256.167639	17.177344
31.597965	1273.253526	17.182362
31.954409	1264.592187	17.187379
31.823579	1291.804608	17.192397
32.001894	1279.588784	17.197415
32.308260	1269.040490	17.202432
32.203999	1292.648673	17.207450
32.496084	1288.121411	17.212467
32.706670	1272.586659	17.217485
31.985914	1270.662624	17.222503
32.551189	1264.613304	17.227520
32.229333	1241.839838	17.232538
32.417958	1253.204108	17.237555
32.239224	1267.586176	17.242573
32.368888	1267.576051	17.247591
32.359775	1264.939772	17.252608
32.093514	1283.501587	17.257626
32.414536	1291.859563	17.262643
32.534036	1277.928072	17.267661
32.304182	1290.725379	17.272679
32.488968	1289.102973	17.277696
32.403267	1277.259936	17.282714
32.579509	1274.560061	17.287731
32.514820	1275.498276	17.292749
32.365759	1267.867395	17.297767
32.487949	1276.631164	17.302784
32.483145	1276.389775	17.307802
32.946163	1298.433701	17.312819
33.006420	1292.675552	17.317837
33.009269	1306.973235	17.322855
33.318840	1301.769710	17.327872
32.777841	1284.357444	17.332890
32.813344	1278.500069	17.337907
32.862897	1287.048045	17.342925
32.993177	1312.557012	17.347943
33.353370	1305.868099	17.352960
33.244523	1304.552128	17.357978
33.563084	1308.356848	17.362995
33.161331	1282.024319	17.368013
32.820735	1292.424150	17.373031
33.222666	1305.675894	17.378048
33.131575	1304.547987	17.383066
33.302699	1307.054739	17.388083
33.757860	1302.443056	17.393101
33.331744	1301.549015	17.398119
33.367758	1321.688502	17.403136
33.394546	1318.835601	17.408154
33.426703	1305.936296	17.413171
33.565044	1294.055534	17.418189
33.056769	1303.550031	17.423207
33.489158	1313.999069	17.428224
33.165071	1299.064535	17.433242
33.231232	1309.539648	17.438259
33.907752	1313.419241	17.443277
33.661922	1294.009521	17.448295
33.945158	1301.938710	17.453312
33.483677	1324.030845	17.458330
33.555265	1322.779226	17.463347
34.056772	1319.018442	17.468365
34.056836	1310.126174	17.473383
34.395032	1318.284620	17.478400
33.955263	1319.589474	17.483418
33.933871	1304.323877	17.488435
34.238829	1300.375845	17.493453
33.972173	1302.960056	17.498471
34.215323	1307.565638	17.503488
33.750260	1307.993968	17.508506
33.957692	1309.669320	17.513523
34.292260	1323.325231	17.518541
33.924406	1331.040447	17.523559
34.156444	1312.006850	17.528576
34.288321	1328.723515	17.533594
33.899025	1340.880041	17.538611
34.317169	1334.989819	17.543629
34.115015	1335.135094	17.548647
34.133465	1318.144789	17.553664
34.051284	1325.507354	17.558682
34.324355	1326.847821	17.563699
33.953397	1339.265626	17.568717
33.925609	1364.286744	17.573735
34.272808	1360.396859	17.578752
34.477787	1356.547206	17.583770
34.775445	1372.904808	17.588787
34.644917	1381.491157	17.593805
34.721641	1366.720291	17.598823
34.939486	1338.596190	17.603840
34.888683	1357.057249	17.608858
34.927773	1371.260834	17.613875
35.010508	1352.163395	17.618893
34.772748	1367.374219	17.623911
35.162979	1355.973221	17.628928
35.023412	1356.264319	17.633946
35.229086	1345.625943	17.638963
35.057698	1357.159009	17.643981
34.786309	1345.877978	17.648999
35.120496	1362.342794	17.654016
35.139331	1367.398065	17.659034
35.027953	1358.761434	17.664051
35.362248	1346.061618	17.669069
34.870412	1366.335329	17.674087
35.212430	1343.527580	17.679104
35.496943	1360.998899	17.684122
35.160501	1367.009329	17.689139
35.197096	1348.343242	17.694157
35.016359	1355.875026	17.699175
35.468507	1358.704652	17.704192
35.443087	1368.026504	17.709210
35.276234	1377.150229	17.714227
35.735187	1386.242772	17.719245
35.915804	1378.831999	17.724263
36.084204	1359.017503	17.729280
35.779659	1368.009385	17.734298
35.785373	1345.457949	17.739315
35.974095	1342.020145	17.744333
35.495053	1356.610843	17.749351
35.544478	1348.782002	17.754368
35.768249	1353.433507	17.759386
35.908851	1363.306530	17.764403
36.176383	1351.053175	17.769421
35.762052	1374.363492	17.774439
35.725447	1386.290354	17.779456
36.050202	1369.243275	17.784474
35.895261	1374.979184	17.789491
36.139388	1361.217433	17.794509
35.982264	1360.061860	17.799527
36.244388	1371.299826	17.804544
35.973574	1380.816139	17.809562
36.134589	1373.783720	17.814579
36.375670	1380.892052	17.819597
36.056856	1375.489755	17.824615
36.202694	1363.726079	17.829632
36.127000	1379.742327	17.834650
36.042220	1372.554409	17.839667
36.452006	1388.260768	17.844685
36.057408	1403.981196	17.849703
36.345753	1413.099489	17.854720
36.417006	1405.661510	17.859738
36.201537	1394.745233	17.864755
36.542552	1411.068454	17.869773
36.416416	1419.372763	17.874791
36.548999	1410.163034	17.879808
36.363219	1397.605896	17.884826
36.181743	1413.586424	17.889843
36.693373	1409.479633	17.894861
36.663672	1431.025775	17.899879
37.063174	1441.917443	17.904896
37.134950	1425.402253	17.909914
37.203798	1409.498845	17.914931
37.367272	1413.084491	17.919949
37.217067	1417.698526	17.924967
37.019238	1409.373232	17.929984
37.329839	1386.684659	17.935002
37.137580	1393.505829	17.940019
37.063199	1377.572887	17.945037
36.815148	1394.349455	17.950055
37.118339	1391.173664	17.955072
37.521174	1414.227084	17.960090
37.064207	1409.706073	17.965107
37.599390	1409.437935	17.970125
37.479495	1414.977461	17.975143
37.293914	1409.447548	17.980160
37.380393	1409.857951	17.985178
37.112298	1408.238930	17.990195
37.455210	1414.041960	17.995213
37.354796	1410.144356	18.000231
37.303583	1405.002385	18.005248
37.537319	1414.955206	18.010266
37.472322	1421.775236	18.015283
37.875620	1411.939600	18.020301
37.408281	1410.383813	18.025319
37.557292	1425.685668	18.030336
38.024692	1435.054735	18.035354
38.070044	1452.521793	18.040371
38.205489	1448.858174	18.045389
38.121724	1443.317919	18.050407
37.973020	1412.191845	18.055424
38.054910	1412.542389	18.060442
37.775794	1428.577445	18.065459
37.996906	1436.305403	18.070477
38.059203	1435.108841	18.075495
38.513539	1426.028864	18.080512
38.637278	1439.146224	18.085530
38.330245	1451.264348	18.090547
38.452320	1409.533966	18.095565
38.677913	1406.328780	18.100583
37.984544	1413.546575	18.105600
38.492881	1396.908596	18.110618
38.099123	1407.524331	18.115635
38.304033	1442.670202	18.120653
38.380664	1453.538773	18.125671
38.596327	1438.289467	18.130688
38.504442	1445.372063	18.135706
38.132243	1442.446224	18.140723
38.380959	1439.902319	18.145741
38.599547	1439.343169	18.150759
38.639512	1460.828934	18.155776
38.931363	1444.881750	18.160794
38.938329	1433.181019	18.165811
38.713497	1450.467870	18.170829
38.823327	1440.038629	18.175847
38.867665	1440.556663	18.180864
38.709683	1450.895428	18.185882
38.559848	1457.496671	18.190899
38.933122	1472.120808	18.195917
38.960665	1460.795706	18.200935
38.684021	1462.883574	18.205952
39.014356	1471.174375	18.210970
39.000943	1470.590387	18.215987
39.115501	1462.558740	18.221005
39.182773	1477.410575	18.226023
38.977889	1457.461026	18.231040
39.419164	1466.263592	18.236058
39.171387	1482.299921	18.241075
39.491610	1500.176038	18.246093
39.696978	1496.064729	18.251111
39.639874	1484.231861	18.256128
39.944845	1491.115069	18.261146
39.776977	1463.206808	18.266163
39.667183	1447.702582	18.271181
39.624872	1475.923704	18.276199
39.429356	1466.639545	18.281216
39.531803	1468.354995	18.286234
39.640305	1470.774112	18.291251
40.154143	1474.492975	18.296269
39.940915	1503.837525	18.301287
39.772496	1502.259884	18.306304
39.995515	1481.286357	18.311322
40.061643	1488.309109	18.316339
39.784334	1505.425598	18.321357
40.098652	1483.487582	18.326375
40.281342	1504.813633	18.331392
40.043338	1481.182338	18.336410
39.907895	1478.722868	18.341427
40.124519	1487.199953	18.346445
40.215123	1488.373091	18.351463
40.023133	1480.757562	18.356480
40.145470	1485.482944	18.361498
40.115965	1496.213016	18.366515
40.323535	1482.392054	18.371533
40.320957	1471.765667	18.376551
40.384264	1497.087824	18.381568
40.522307	1519.769208	18.386586
40.635952	1521.090378	18.391603
40.916795	1495.692388	18.396621
40.966755	1492.473205	18.401639
40.688040	1490.045084	18.406656
40.861966	1499.472430	18.411674
40.585349	1489.085270	18.416691
40.767029	1500.788199	18.421709
40.971480	1499.343978	18.426727
40.809962	1494.639503	18.431744
40.918670	1512.684416	18.436762
40.926914	1511.159748	18.441779
40.919474	1509.173797	18.446797
40.818150	1512.707182	18.451815
40.794787	1508.713669	18.456832
41.424866	1490.255864	18.461850
41.160204	1500.319343	18.466867
41.115795	1517.376400	18.471885
41.356527	1514.825240	18.476903
41.084798	1508.186051	18.481920
41.405437	1506.314451	18.486938
41.164321	1512.253587	18.491955
41.146010	1494.868263	18.496973
41.219208	1520.822447	18.501991
41.263466	1547.596438	18.507008
41.422264	1532.457890	18.512026
41.477282	1543.884407	18.517043
41.258694	1546.926461	18.522061
41.653464	1538.550206	18.527079
41.528234	1555.675275	18.532096
41.529258	1542.460512	18.537114
41.511839	1539.340033	18.542131
41.757728	1537.581548	18.547149
41.908064	1548.331041	18.552167
42.198654	1551.513415	18.557184
42.209859	1564.305753	18.562202
41.976876	1558.240723	18.567219
41.934899	1524.441842	18.572237
42.125203	1532.641374	18.577255
41.897847	1576.696053	18.582272
42.234355	1557.475042	18.587290
42.133212	1553.402560	18.592307
42.403455	1558.092305	18.597325
42.180122	1535.810770	18.602343
42.403141	1547.988001	18.607360
42.640016	1557.021008	18.612378
42.474581	1564.304355	18.617395
42.743398	1539.920857	18.622413
42.436748	1530.411277	18.627431
42.321680	1547.437730	18.632448
42.593615	1559.443438	18.637466
42.413403	1550.871113	18.642483
42.627962	1557.698834	18.647501
42.841595	1568.800403	18.652519
42.636829	1572.251507	18.657536
42.515466	1549.093149	18.662554
42.533064	1542.957097	18.667571
42.827083	1561.343905	18.672589
42.834390	1552.631363	18.677607
42.286595	1555.032103	18.682624
42.715984	1565.918724	18.687642
42.808202	1568.792223	18.692659
42.550913	1566.405224	18.697677
43.130926	1570.588468	18.702695
43.052064	1608.611914	18.707712
43.054787	1586.448036	18.712730
43.237225	1574.058892	18.717747
43.019393	1576.268623	18.722765
43.262253	1585.478375	18.727783
43.346565	1595.231251	18.732800
43.649399	1612.374703	18.737818
43.825284	1623.939245	18.742835
43.707881	1597.648829	18.747853
43.549291	1586.591547	18.752871
43.591502	1584.596790	18.757888
43.706833	1597.391925	18.762906
43.736014	1587.729394	18.767923
43.801941	1609.083447	18.772941
44.021766	1601.879920	18.777959
43.994286	1610.817500	18.782976
43.738977	1591.722682	18.787994
43.748635	1595.065538	18.793011
43.890111	1597.569660	18.798029
44.168364	1595.864567	18.803047
44.075604	1613.509913	18.808064
44.193505	1604.244730	18.813082
44.230443	1591.115703	18.818099
44.423942	1599.259144	18.823117
44.510854	1597.106539	18.828135
44.307438	1586.715284	18.833152
44.475872	1600.008035	18.838170
44.121995	1615.834427	18.843187
44.356986	1604.140068	18.848205
44.481520	1583.230107	18.853223
44.036899	1591.529474	18.858240
44.138074	1604.098853	18.863258
44.013069	1613.867633	18.868275
44.065159	1597.861112	18.873293
44.310791	1606.377850	18.878311
44.615603	1624.353489	18.883328
44.716207	1618.346574	18.888346
44.676890	1639.162469	18.893363
44.690806	1639.241928	18.898381
44.798573	1627.163444	18.903399
44.908526	1626.434877	18.908416
45.312272	1604.790506	18.913434
45.367275	1633.135965	18.918451
45.321604	1620.230953	18.923469
45.006172	1616.691496	18.928487
45.050810	1633.330312	18.933504
45.166053	1618.530204	18.938522
44.937046	1605.159444	18.943539
45.336073	1605.645047	18.948557
45.667107	1621.821258	18.953575
45.327088	1613.461290	18.958592
45.458235	1624.923505	18.963610
45.542092	1625.487562	18.968627
45.231352	1611.649400	18.973645
45.381288	1600.061993	18.978663
45.282627	1624.736269	18.983680
45.507562	1623.180014	18.988698
45.951581	1623.068543	18.993715
45.658902	1651.029653	18.998733
45.844564	1628.340507	19.003751
45.707327	1627.318607	19.008768
45.967060	1647.940539	19.013786
45.995492	1634.312788	19.018803
45.769854	1642.927990	19.023821
46.156517	1651.631246	19.028839
45.889816	1642.461576	19.033856
46.134509	1638.700152	19.038874
46.275102	1643.500896	19.043891
45.694806	1664.529620	19.048909
46.073054	1642.637493	19.053927
46.235150	1640.675368	19.058944
45.999467	1646.340782	19.063962
46.330834	1636.516299	19.068979
46.238784	1645.116708	19.073997
46.336839	1638.829753	19.079015
46.096203	1654.869905	19.084032
46.540145	1684.519603	19.089050
46.759816	1666.399921	19.094067
46.500283	1682.702619	19.099085
46.983529	1674.476105	19.104103
46.981285	1673.223570	19.109120
46.792383	1668.885696	19.114138
46.995878	1680.056921	19.119155
46.992163	1677.527629	19.124173
46.867665	1656.883476	19.129191
46.791081	1671.691963	19.134208
47.254814	1659.884483	19.139226
47.369369	1651.866514	19.144243
46.917213	1671.251084	19.149261
47.024322	1671.645784	19.154279
47.025549	1667.685068	19.159296
47.053837	1658.738239	19.164314
47.072235	1653.620205	19.169331
46.889523	1661.577376	19.174349
47.138222	1678.202004	19.179367
47.172328	1681.477467	19.184384
47.447887	1673.343136	19.189402
47.567712	1689.213249	19.194419
47.323018	1702.155447	19.199437
47.333650	1695.099513	19.204455
47.569418	1674.264925	19.209472
47.547893	1681.827928	19.214490
47.558998	1692.223247	19.219507
47.471914	1692.979694	19.224525
47.725622	1701.698160	19.229543
47.881987	1707.147070	19.234560
48.103826	1720.167670	19.239578
48.330840	1703.993283	19.244595
48.271011	1722.100637	19.249613
48.464513	1730.247395	19.254631
48.071930	1703.988198	19.259648
48.095007	1709.312117	19.264666
48.436491	1720.181984	19.269683
47.983825	1698.899921	19.274701
48.532752	1705.906757	19.279719
48.593304	1728.715996	19.284736
48.388645	1714.144313	19.289754
48.609903	1703.186447	19.294771
48.417692	1719.156963	19.299789
48.642930	1696.113021	19.304807
48.492314	1704.521608	19.309824
48.566637	1719.531831	19.314842
48.782981	1707.732229	19.319859
48.730587	1695.450283	19.324877
48.949673	1701.489097	19.329895
48.740816	1720.051007	19.334912
48.891229	1721.451240	19.339930
49.060396	1704.316136	19.344947
49.039563	1696.487608	19.349965
49.228299	1712.176215	19.354983
49.345780	1699.725573	19.360000
49.155705	1704.810164	19.365018
48.830809	1708.267570	19.370035
48.977638	1701.073698	19.375053
49.145013	1700.997806	19.380071
48.968371	1708.359140	19.385088
49.044767	1716.406172	19.390106
49.153220	1723.372934	19.395123
49.073196	1737.973434	19.400141
49.196579	1746.541646	19.405159
49.688519	1730.891743	19.410176
49.472499	1721.420501	19.415194
49.715987	1736.067225	19.420211
49.307682	1749.561589	19.425229
49.938403	1752.489217	19.430247
50.079681	1738.089926	19.435264
49.997389	1745.927516	19.440282
49.948002	1765.105813	19.445299
50.027039	1761.500744	19.450317
50.416294	1762.788102	19.455335
50.443014	1745.380193	19.460352
50.368878	1725.560233	19.465370
50.108923	1728.470210	19.470387
50.331085	1732.400492	19.475405
50.622095	1712.337371	19.480423
50.375303	1717.933697	19.485440
50.157448	1720.165199	19.490458
50.244537	1728.904621	19.495475
50.323348	1741.898294	19.500493
50.645430	1754.122693	19.505511
50.435303	1757.393363	19.510528
50.419589	1737.983136	19.515546
50.846580	1750.624557	19.520563
50.784707	1758.440968	19.525581
50.521492	1743.340360	19.530599
50.645180	1751.766723	19.535616
50.572507	1741.523408	19.540634
50.495126	1742.557037	19.545651
50.732214	1770.090633	19.550669
50.837547	1771.586000	19.555687
51.091977	1773.799591	19.560704
50.937480	1775.654563	19.565722
51.142255	1773.100250	19.570739
50.975342	1790.580037	19.575757
51.162722	1796.532906	19.580775
51.382335	1776.916256	19.585792
50.910566	1777.234506	19.590810
51.244874	1795.798170	19.595827
51.456072	1796.261778	19.600845
51.557057	1799.884706	19.605863
51.834770	1811.447029	19.610880
51.907262	1813.296872	19.615898
52.257969	1789.486239	19.620915
52.018598	1802.640592	19.625933
51.799023	1771.457106	19.630951
51.915770	1768.091620	19.635968
51.495139	1785.273042	19.640986
51.955317	1790.664003	19.646003
51.928490	1800.521284	19.651021
51.969585	1807.550976	19.656039
52.009592	1782.443735	19.661056
52.175884	1785.925776	19.666074
52.174121	1794.463524	19.671091
52.198095	1809.585186	19.676109
52.285019	1790.206643	19.681127
52.386333	1802.892674	19.686144
52.408320	1803.176174	19.691162
52.385586	1800.138492	19.696179
52.546400	1790.247528	19.701197
52.462150	1791.805615	19.706215
52.769496	1804.050990	19.711232
52.416062	1807.388748	19.716250
52.333100	1796.159301	19.721267
52.699942	1807.506343	19.726285
52.877746	1820.639501	19.731303
52.773842	1807.352889	19.736320
52.707771	1824.398910	19.741338
52.877827	1818.672705	19.746355
52.834546	1821.586158	19.751373
52.886864	1816.074943	19.756391
53.100584	1819.094815	19.761408
53.068799	1834.871750	19.766426
53.277205	1824.269395	19.771443
53.633774	1835.566886	19.776461
53.673577	1840.092967	19.781479
53.548872	1821.985628	19.786496
53.195971	1825.150600	19.791514
53.428183	1821.827329	19.796531
53.583796	1829.380422	19.801549
53.568575	1836.952498	19.806567
53.659245	1847.280257	19.811584
53.508497	1846.001667	19.816602
53.740004	1835.460928	19.821619
54.041723	1844.123323	19.826637
53.845554	1839.947494	19.831655
53.739336	1834.308562	19.836672
53.682801	1845.192529	19.841690
53.829377	1828.188555	19.846707
54.036050	1842.843433	19.851725
54.347271	1866.754637	19.856743
54.259899	1874.316710	19.861760
54.412076	1865.721263	19.866778
54.155004	1847.041001	19.871795
54.446434	1862.687798	19.876813
54.212079	1881.944042	19.881831
54.694712	1871.173431	19.886848
54.718132	1859.404313	19.891866
54.737299	1869.697653	19.896883
54.634198	1853.599013	19.901901
54.461212	1854.456752	19.906919
54.633100	1850.100832	19.911936
54.463409	1865.409344	19.916954
54.816585	1853.483496	19.921971
54.481393	1872.523957	19.926989
54.667947	1877.503856	19.932007
55.189987	1881.932548	19.937024
54.908723	1897.355082	19.942042
54.773658	1891.756618	19.947059
55.090864	1897.356641	19.952077
55.206115	1898.810231	19.957095
55.377054	1877.088418	19.962112
55.391088	1882.727119	19.967130
55.246432	1894.846608	19.972147
55.433573	1881.724986	19.977165
55.187116	1897.959622	19.982183
55.742894	1888.247474	19.987200
55.486528	1884.431020	19.992218
55.401399	1893.375830	19.997235
55.682671	1905.930064	20.002253
55.553364	1898.938098	20.007271
55.681719	1923.567567	20.012288
55.722760	1923.032033	20.017306
55.853531	1906.070439	20.022323
56.050511	1916.929293	20.027341
55.854253	1904.915197	20.032359
56.292697	1900.224227	20.037376
56.034679	1911.341989	20.042394
55.939960	1896.246648	20.047411
56.020942	1934.962856	20.052429
56.148672	1938.865990	20.057447
56.418356	1930.410311	20.062464
56.354331	1939.254533	20.067482
56.138391	1924.229482	20.072499
56.664509	1928.224132	20.077517
56.920274	1949.466203	20.082535
57.092622	1925.929569	20.087552
56.753256	1929.613289	20.092570
56.656951	1924.253145	20.097587
56.661361	1921.843215	20.102605
56.241787	1934.536214	20.107623
56.794922	1935.846596	20.112640
56.934579	1958.336471	20.117658
56.777155	1955.692008	20.122675
57.170351	1955.494072	20.127693
56.935688	1962.461057	20.132711
57.126585	1944.607466	20.137728
57.007527	1965.751685	20.142746
56.868977	1978.180113	20.147763
57.506085	1978.806473	20.152781
57.504832	1996.769753	20.157799
57.946734	1986.527546	20.162816
57.835389	1968.573210	20.167834
57.622724	1989.063272	20.172851
57.781002	1997.683623	20.177869
58.010174	1988.777802	20.182887
57.896190	1995.220426	20.187904
57.974886	1990.545185	20.192922
57.850416	1975.263576	20.197939
58.030610	1956.415765	20.202957
57.918382	1985.380737	20.207975
58.133331	1995.792666	20.212992
57.905667	1978.446998	20.218010
58.132523	1969.223815	20.223027
58.324668	1977.531530	20.228045
58.096147	1994.315661	20.233063
58.421382	1999.235092	20.238080
58.362726	2017.473679	20.243098
58.350591	2006.663397	20.248115
58.366319	1999.537104	20.253133
58.161461	2019.035941	20.258151
58.543042	1992.452588	20.263168
58.495492	2013.945423	20.268186
58.522431	2024.894842	20.273203
58.847197	2036.264949	20.278221
59.049610	2041.766988	20.283239
59.305566	2040.412024	20.288256
59.414839	2038.496268	20.293274
59.005893	2027.745048	20.298291
58.991959	2019.661619	20.303309
59.300473	2019.955442	20.308327
59.347571	2038.612325	20.313344
59.092393	2029.482833	20.318362
58.904813	2033.320006	20.323379
59.383890	2036.244900	20.328397
59.254977	2026.419177	20.333415
59.175700	2029.681862	20.338432
59.305572	2047.873882	20.343450
59.399812	2044.829516	20.348467
59.942330	2034.510721	20.353485
59.785114	2052.267007	20.358503
60.165951	2058.054964	20.363520
60.008246	2056.150553	20.368538
60.002076	2066.902656	20.373555
60.175334	2057.930064	20.378573
60.010493	2058.869426	20.383591
60.224804	2054.314544	20.388608
60.519880	2052.661140	20.393626
60.138852	2050.925991	20.398643
60.144126	2064.737947	20.403661
60.219422	2054.696505	20.408679
60.292773	2057.802306	20.413696
60.162537	2060.179289	20.418714
60.426438	2068.146122	20.423731
61.009749	2063.919560	20.428749
60.744780	2079.820697	20.433767
61.203065	2082.382174	20.438784
61.284562	2092.589195	20.443802
61.365236	2053.042843	20.448819
60.923897	2045.782253	20.453837
60.872746	2068.905581	20.458855
60.941522	2053.760631	20.463872
61.277747	2066.263896	20.468890
61.244390	2084.739087	20.473907
61.592214	2069.148574	20.478925
61.124988	2089.317121	20.483943
61.336408	2070.656889	20.488960
61.653491	2079.968238	20.493978
61.414864	2075.400711	20.498995
61.686605	2086.472882	20.504013
61.488605	2099.081378	20.509031
61.308007	2067.473896	20.514048
61.682515	2075.524110	20.519066
61.234268	2072.991551	20.524083
61.537923	2070.774034	20.529101
61.902516	2100.223320	20.534119
62.138276	2088.036330	20.539136
61.900194	2107.186208	20.544154
61.941882	2112.046152	20.549171
62.190758	2095.925604	20.554189
61.926265	2088.152688	20.559207
62.266704	2097.779521	20.564224
62.212845	2110.023028	20.569242
61.981912	2114.832961	20.574259
62.413227	2108.217958	20.579277
62.433585	2127.227337	20.584295
62.320286	2135.497536	20.589312
63.038616	2123.700870	20.594330
62.898945	2143.876866	20.599347
62.941793	2140.923932	20.604365
62.990282	2129.742388	20.609383
62.842445	2115.434014	20.614400
62.934704	2121.768313	20.619418
63.211210	2130.726128	20.624435
63.106621	2127.392021	20.629453
63.146075	2123.206996	20.634471
63.035348	2135.228171	20.639488
63.234233	2131.102118	20.644506
63.156718	2122.129793	20.649523
63.355690	2122.015122	20.654541
63.150086	2150.604074	20.659559
63.364114	2149.991530	20.664576
63.650392	2154.344912	20.669594
63.357073	2137.966241	20.674611
63.667391	2156.895956	20.679629
63.485807	2149.410732	20.684647
63.537625	2147.848491	20.689664
64.358401	2170.502946	20.694682
63.910321	2161.330953	20.699699
63.945813	2136.053930	20.704717
63.819898	2157.699064	20.709735
63.800923	2193.910444	20.714752
64.148061	2186.699384	20.719770
64.129293	2177.011832	20.724787
64.258142	2173.492611	20.729805
64.232052	2177.767424	20.734823
64.125745	2183.729513	20.739840
64.565147	2183.676964	20.744858
64.282536	2212.273540	20.749875
64.433573	2211.793035	20.754893
64.590806	2195.550345	20.759911
64.659174	2202.064875	20.764928
65.047242	2194.361895	20.769946
65.017934	2201.920438	20.774963
65.035778	2207.526744	20.779981
65.257018	2193.438757	20.784999
65.450716	2185.062807	20.790016
65.213339	2198.992920	20.795034
65.086692	2201.982808	20.800051
65.439498	2186.188732	20.805069
65.515914	2204.097498	20.810087
65.120434	2207.666759	20.815104
65.693234	2210.145369	20.820122
65.754011	2229.756064	20.825139
65.697805	2213.358697	20.830157
65.643253	2209.118526	20.835175
65.764753	2219.285070	20.840192
66.310228	2230.017969	20.845210
66.109733	2221.535316	20.850227
66.384166	2198.258318	20.855245
66.105416	2212.713989	20.860263
65.994430	2216.520050	20.865280
66.254959	2202.195877	20.870298
65.968148	2226.315600	20.875315
66.415181	2212.475570	20.880333
66.249883	2204.534950	20.885351
66.316339	2194.822183	20.890368
66.632785	2208.619457	20.895386
66.313110	2226.429064	20.900403
66.457751	2235.959916	20.905421
66.865129	2227.377402	20.910439
66.759595	2244.916745	20.915456
66.999180	2241.290446	20.920474
66.996918	2238.151673	20.925491
66.752475	2233.776366	20.930509
66.965239	2245.924456	20.935527
66.780606	2252.296298	20.940544
67.096674	2230.648413	20.945562
67.367190	2246.141900	20.950579
67.634374	2232.257863	20.955597
67.499524	2218.984274	20.960615
67.526988	2230.098391	20.965632
67.632372	2245.557954	20.970650
67.502962	2224.361383	20.975667
67.472489	2210.095229	20.980685
68.155194	2239.240193	20.985703
67.851827	2238.391149	20.990720
67.946081	2222.262659	20.995738
67.698345	2235.626209	21.000755
67.982742	2247.303683	21.005773
68.199406	2265.976024	21.010791
67.993712	2267.916470	21.015808
68.388712	2238.884724	21.020826
68.197253	2253.685201	21.025843
68.144984	2268.936627	21.030861
68.148957	2278.345498	21.035879
68.031063	2261.696211	21.040896
68.333246	2249.294314	21.045914
68.478444	2262.129058	21.050931
68.517980	2269.295417	21.055949
68.813023	2290.665208	21.060967
68.617872	2302.132645	21.065984
68.803988	2273.372123	21.071002
68.958752	2272.032090	21.076019
68.918878	2285.397548	21.081037
69.272716	2263.588480	21.086055
69.283403	2269.520445	21.091072
69.350632	2278.081997	21.096090
68.882782	2284.818709	21.101107
69.302037	2268.768530	21.106125
69.240605	2274.631325	21.111143
69.168045	2297.674395	21.116160
69.508860	2294.322252	21.121178
69.562583	2311.872947	21.126195
69.343256	2313.747159	21.131213
69.260290	2298.683726	21.136231
69.410217	2304.992432	21.141248
69.852482	2334.412014	21.146266
69.869721	2339.660751	21.151283
70.200797	2334.171583	21.156301
70.525284	2325.597595	21.161319
70.493197	2338.640409	21.166336
70.645095	2330.807026	21.171354
70.448632	2328.319515	21.176371
70.616013	2326.354463	21.181389
70.571170	2324.615591	21.186407
70.254292	2326.061311	21.191424
70.390799	2324.334394	21.196442
70.374184	2318.716298	21.201459
70.278226	2310.585158	21.206477
70.750424	2325.576185	21.211495
70.618132	2359.427643	21.216512
70.963059	2351.444656	21.221530
70.777731	2355.674680	21.226547
71.016292	2363.171128	21.231565
71.226076	2358.484348	21.236583
70.968862	2363.249397	21.241600
71.078531	2361.063797	21.246618
70.876939	2373.359579	21.251635
71.044838	2391.331387	21.256653
71.522743	2388.115601	21.261671
71.343226	2371.109310	21.266688
71.572079	2379.288953	21.271706
71.517994	2397.610195	21.276723
71.438462	2389.136393	21.281741
71.953757	2389.838406	21.286759
71.855374	2412.158472	21.291776
72.165060	2404.975051	21.296794
72.222818	2403.344392	21.301811
72.224383	2414.170448	21.306829
72.473963	2420.914632	21.311847
72.332296	2415.094366	21.316864
72.300048	2414.353834	21.321882
72.374736	2400.140292	21.326899
72.497672	2408.138666	21.331917
72.636556	2407.274988	21.336935
72.646737	2401.221991	21.341952
72.741182	2403.934971	21.346970
72.787318	2407.479424	21.351987
72.823001	2404.867136	21.357005
72.932432	2399.537189	21.362023
72.559710	2407.488156	21.367040
72.813405	2411.503941	21.372058
73.379936	2440.417246	21.377075
72.990427	2437.460908	21.382093
73.236448	2433.021030	21.387111
73.322920	2439.525878	21.392128
73.287511	2416.159910	21.397146
73.245344	2425.985093	21.402163
73.493278	2451.800972	21.407181
73.823569	2443.687502	21.412199
73.562469	2475.373244	21.417216
73.723179	2471.087982	21.422234
73.978591	2456.246389	21.427251
73.738548	2449.334075	21.432269
73.835242	2451.189344	21.437287
73.838315	2470.252488	21.442304
73.910404	2452.963426	21.447322
74.386776	2481.092618	21.452339
74.064101	2478.878852	21.457357
74.340273	2462.231149	21.462375
74.458700	2472.918466	21.467392
74.442573	2465.284801	21.472410
74.634687	2486.101882	21.477427
74.709701	2470.757293	21.482445
74.814114	2460.919601	21.487463
74.757604	2489.607460	21.492480
74.995524	2505.096558	21.497498
75.331366	2509.297386	21.502515
75.016100	2505.418669	21.507533
75.514276	2490.632976	21.512551
75.426839	2495.727830	21.517568
75.492734	2509.822742	21.522586
75.729945	2507.260588	21.527603
75.533530	2493.535194	21.532621
75.652910	2506.924128	21.537639
75.898704	2500.603650	21.542656
75.790192	2493.956348	21.547674
75.733452	2499.721421	21.552691
76.146677	2509.409211	21.557709
76.254891	2488.712297	21.562727
75.828639	2479.572818	21.567744
75.843063	2496.100455	21.572762
75.802974	2509.152412	21.577779
75.817637	2506.191075	21.582797
76.147113	2498.682146	21.587815
76.391762	2530.438344	21.592832
75.962889	2508.373090	21.597850
76.573246	2523.819558	21.602867
76.635231	2534.912051	21.607885
76.750710	2517.552371	21.612903
76.628538	2529.369673	21.617920
76.716088	2538.707422	21.622938
76.934855	2520.420375	21.627955
76.554140	2533.774665	21.632973
76.834882	2553.243535	21.637991
77.141899	2559.044177	21.643008
77.142287	2553.484200	21.648026
77.265493	2550.559045	21.653043
77.015005	2547.987723	21.658061
77.436380	2551.389704	21.663079
77.568955	2532.994658	21.668096
77.496615	2546.455262	21.673114
77.497063	2550.367480	21.678131
77.751783	2571.332380	21.683149
77.712619	2564.491724	21.688167
77.978823	2568.055550	21.693184
78.071563	2574.312803	21.698202
78.067082	2561.783600	21.703219
77.759788	2580.885965	21.708237
78.275899	2568.267386	21.713255
78.188162	2570.627485	21.718272
78.281197	2564.003336	21.723290
78.103082	2573.552697	21.728307
77.999954	2598.913524	21.733325
78.348727	2593.412483	21.738343
78.504274	2600.782235	21.743360
78.576410	2603.190517	21.748378
78.934067	2588.695037	21.753395
78.789416	2595.039944	21.758413
78.923316	2613.530547	21.763431
79.219688	2614.105779	21.768448
79.119064	2620.369809	21.773466
79.621419	2628.281195	21.778483
79.345162	2619.161132	21.783501
79.823786	2607.559593	21.788519
79.835869	2626.997962	21.793536
79.925991	2637.542848	21.798554
80.199928	2611.543358	21.803571
79.689325	2596.617216	21.808589
80.061393	2583.244195	21.813607
79.995367	2602.437801	21.818624
79.843195	2613.163830	21.823642
80.158098	2617.224861	21.828659
80.134707	2620.596825	21.833677
80.265392	2610.805672	21.838695
80.435661	2617.550256	21.843712
80.044179	2615.963694	21.848730
79.991244	2612.135486	21.853747
79.777643	2630.498125	21.858765
80.117858	2650.084438	21.863783
80.553311	2645.239236	21.868800
80.308332	2634.313466	21.873818
80.636150	2638.255063	21.878835
80.517639	2674.487665	21.883853
80.865868	2677.471114	21.888871
80.823712	2668.468024	21.893888
80.901553	2664.466442	21.898906
81.022070	2681.240489	21.903923
80.844516	2705.554491	21.908941
81.169120	2700.341225	21.913959
81.411012	2691.974554	21.918976
81.305664	2702.205573	21.923994
81.460600	2697.115607	21.929011
81.394636	2694.537190	21.934029
81.487473	2729.661132	21.939047
81.730466	2733.015279	21.944064
81.879190	2732.556201	21.949082
82.581242	2715.583359	21.954099
82.251914	2727.569475	21.959117
82.342171	2737.272988	21.964135
82.638607	2725.967177	21.969152
82.638198	2729.265100	21.974170
82.677483	2713.864764	21.979187
82.720157	2730.629093	21.984205
82.975871	2716.307405	21.989223
82.986146	2725.096500	21.994240
82.872047	2731.370281	21.999258
83.282391	2712.614992	22.004275
83.127334	2710.173325	22.009293
83.551213	2720.323991	22.014311
83.267422	2711.452131	22.019328
83.215577	2718.722763	22.024346
83.202772	2717.211590	22.029363
83.319380	2719.188781	22.034381
83.351818	2727.553211	22.039399
83.368624	2719.751992	22.044416
83.282848	2723.918233	22.049434
83.529593	2727.331593	22.054451
83.493220	2720.403608	22.059469
83.405451	2724.720354	22.064487
83.461965	2745.063412	22.069504
83.625157	2745.001298	22.074522
84.023590	2740.470409	22.079539
83.838160	2749.297761	22.084557
84.177388	2758.277564	22.089575
84.333589	2760.201964	22.094592
84.086643	2775.838966	22.099610
84.118157	2790.385819	22.104627
84.238838	2774.397640	22.109645
84.434598	2786.519445	22.114663
84.867254	2802.825960	22.119680
84.886160	2789.611106	22.124698
85.197013	2794.404646	22.129715
84.974859	2809.776597	22.134733
84.751121	2801.726146	22.139751
85.087885	2808.703503	22.144768
84.832494	2814.500338	22.149786
85.303640	2815.845608	22.154803
85.356638	2825.258916	22.159821
85.292271	2840.979972	22.164839
85.583223	2828.425944	22.169856
85.518894	2828.787595	22.174874
85.472330	2828.693221	22.179891
85.626841	2849.119226	22.184909
86.064837	2860.845794	22.189927
86.479005	2839.177106	22.194944
86.204769	2857.263655	22.199962
86.274558	2857.175838	22.204979
86.636300	2863.933570	22.209997
86.479172	2859.841450	22.215015
86.790662	2862.079923	22.220032
86.720152	2848.213935	22.225050
86.564786	2848.147774	22.230067
86.842660	2852.224239	22.235085
86.822320	2863.724616	22.240103
87.015816	2839.748797	22.245120
86.748546	2855.888779	22.250138
86.855022	2871.628087	22.255155
87.013939	2861.789006	22.260173
86.869478	2866.240340	22.265191
87.477923	2878.587688	22.270208
87.404335	2872.891414	22.275226
87.505261	2858.463889	22.280243
87.670942	2867.070910	22.285261
87.687000	2893.878087	22.290279
88.307963	2907.985370	22.295296
88.224891	2902.630767	22.300314
88.669964	2873.677337	22.305331
88.387759	2871.952037	22.310349
87.691990	2869.426093	22.315367
87.941325	2863.185777	22.320384
87.675638	2897.327354	22.325402
88.100388	2889.600157	22.330419
88.262746	2903.241357	22.335437
88.019746	2903.646705	22.340455
88.302478	2924.913916	22.345472
87.999681	2926.335516	22.350490
88.287479	2917.291339	22.355507
88.612426	2945.372201	22.360525
88.661855	2948.717441	22.365543
89.129072	2960.496927	22.370560
88.909078	2966.211207	22.375578
89.278795	2952.604033	22.380595
88.931862	2961.277901	22.385613
88.960286	2966.161269	22.390631
89.780665	2953.265553	22.395648
89.250073	2981.015075	22.400666
89.482525	2996.533521	22.405683
89.797176	2966.572853	22.410701
89.717049	2981.622921	22.415719
89.890513	2990.873331	22.420736
90.087117	2983.874845	22.425754
89.827827	3005.131152	22.430771
90.515563	3015.318523	22.435789
90.212552	3003.347481	22.440807
90.708290	2992.006181	22.445824
90.772386	2986.517795	22.450842
90.756240	3008.240954	22.455859
90.833079	3006.082339	22.460877
90.550608	2999.653894	22.465895
90.729507	3014.061264	22.470912
91.143222	3012.543552	22.475930
91.095332	3000.747849	22.480947
91.227502	3015.499712	22.485965
90.841306	3045.398457	22.490983
91.172671	3010.840601	22.496000
90.930989	3027.096204	22.501018
91.217810	3039.305905	22.506035
91.555929	3033.093169	22.511053
91.518446	3063.552167	22.516071
91.721093	3068.441815	22.521088
91.719206	3059.632409	22.526106
91.675982	3054.475279	22.531123
92.039060	3058.905786	22.536141
92.074533	3087.543146	22.541159
92.096258	3076.434227	22.546176
92.077313	3092.514527	22.551194
92.436973	3083.634934	22.556211
92.630837	3087.804862	22.561229
92.522205	3096.625823	22.566247
92.862831	3099.688950	22.571264
92.995381	3120.244717	22.576282
93.211353	3110.367313	22.581299
93.400106	3085.618953	22.586317
93.262768	3107.964375	22.591335
93.568090	3102.988189	22.596352
93.496884	3105.474954	22.601370
93.421005	3108.985013	22.606387
93.741986	3105.153156	22.611405
93.761802	3100.444202	22.616423
94.019007	3101.104067	22.621440
93.641074	3099.345155	22.626458
93.552496	3102.966747	22.631475
94.049221	3104.171416	22.636493
93.759662	3106.879870	22.641511
93.866698	3111.574331	22.646528
93.897555	3134.453549	22.651546
94.135861	3119.113612	22.656563
94.396309	3133.989454	22.661581
94.152286	3116.163957	22.666599
94.217936	3127.772158	22.671616
94.171966	3138.888043	22.676634
94.254756	3160.553931	22.681651
94.672554	3148.080838	22.686669
94.535408	3174.278259	22.691687
94.790832	3194.217429	22.696704
94.739941	3197.486200	22.701722
94.873614	3179.040208	22.706739
95.380022	3179.927373	22.711757
95.097683	3203.894160	22.716775
95.288473	3204.118399	22.721792
95.765565	3236.671610	22.726810
95.901515	3220.515110	22.731827
96.026419	3199.096451	22.736845
96.114076	3215.621812	22.741863
96.097149	3195.167243	22.746880
96.415599	3203.785819	22.751898
96.130524	3209.896728	22.756915
96.469768	3214.746333	22.761933
96.317217	3208.488831	22.766951
96.422169	3182.548780	22.771968
96.760558	3194.115310	22.776986
96.643089	3213.770097	22.782003
96.859327	3215.292945	22.787021
96.605325	3218.958629	22.792039
96.823783	3229.551802	22.797056
96.835416	3235.328487	22.802074
96.558128	3233.785384	22.807091
96.974709	3252.814629	22.812109
97.089428	3265.002560	22.817127
97.010910	3260.712127	22.822144
97.368896	3248.007129	22.827162
97.452534	3260.738325	22.832179
97.989724	3280.038786	22.837197
98.009182	3283.842942	22.842215
98.640766	3261.194330	22.847232
98.405797	3270.131532	22.852250
98.247768	3291.300051	22.857267
98.753213	3269.750113	22.862285
98.713157	3288.802698	22.867303
98.754344	3275.306411	22.872320
99.082834	3262.662569	22.877338
98.594472	3258.904771	22.882355
98.839019	3257.712597	22.887373
98.994532	3283.017049	22.892391
99.125465	3262.351166	22.897408
99.379077	3257.307893	22.902426
98.800542	3272.525632	22.907443
99.230111	3256.263889	22.912461
99.211545	3262.204023	22.917479
99.281611	3278.602057	22.922496
99.471285	3272.554488	22.927514
99.462376	3282.993162	22.932531
99.825058	3302.716738	22.937549
99.496693	3297.571213	22.942567
99.510947	3306.710931	22.947584
99.918408	3317.571723	22.952602
99.347035	3330.225402	22.957619
99.992600	3325.296260	22.962637
100.102644	3342.657542	22.967655
100.195397	3333.290466	22.972672
100.198531	3361.829358	22.977690
100.248479	3358.334913	22.982707
100.516736	3350.554812	22.987725
100.583596	3376.912942	22.992743
100.538249	3380.068838	22.997760
100.828245	3368.045582	23.002778
101.020239	3370.919959	23.007795
101.182188	3385.520025	23.012813
101.522209	3395.585991	23.017831
101.358107	3372.707116	23.022848
101.658282	3351.001632	23.027866
101.675348	3379.793545	23.032883
101.905235	3372.761040	23.037901
101.817345	3372.784307	23.042919
101.896011	3389.864044	23.047936
102.196324	3399.197273	23.052954
102.133274	3388.364712	23.057971
102.260408	3402.790447	23.062989
102.348264	3412.642800	23.068007
102.287375	3396.304095	23.073024
102.529736	3400.662533	23.078042
102.338823	3397.362195	23.083059
102.415422	3400.356423	23.088077
102.449334	3411.595709	23.093095
102.666622	3434.495348	23.098112
102.945817	3422.262241	23.103130
102.845243	3426.198263	23.108147
103.181461	3441.711822	23.113165
103.182360	3444.303645	23.118183
102.961617	3461.329598	23.123200
103.196091	3446.075790	23.128218
103.220755	3453.789596	23.133235
103.486523	3480.077440	23.138253
103.738152	3485.700792	23.143271
103.716431	3496.102164	23.148288
104.214079	3483.837437	23.153306
104.050987	3468.989821	23.158323
104.307158	3489.095180	23.163341
104.559142	3516.183126	23.168359
104.493416	3504.620281	23.173376
104.750684	3495.644783	23.178394
104.630438	3499.731700	23.183411
104.927898	3503.192164	23.188429
104.931165	3508.574306	23.193447
104.768739	3502.599000	23.198464
105.421880	3502.165991	23.203482
105.487337	3510.885988	23.208499
105.526071	3527.572708	23.213517
105.809239	3546.313758	23.218535
106.076582	3522.075684	23.223552
106.284567	3525.280490	23.228570
105.797304	3524.926874	23.233587
106.418430	3524.544033	23.238605
106.171853	3519.806141	23.243623
106.042536	3527.113969	23.248640
106.583362	3514.483257	23.253658
106.238953	3517.685645	23.258675
106.263220	3521.538667	23.263693
106.378838	3514.836763	23.268711
106.255219	3522.440275	23.273728
106.385637	3535.083069	23.278746
106.331245	3550.666006	23.283763
106.808293	3558.466911	23.288781
106.750024	3549.952345	23.293799
106.522522	3575.617981	23.298816
107.084515	3575.875960	23.303834
107.075713	3566.384788	23.308851
107.226811	3582.768182	23.313869
107.328530	3607.649414	23.318887
107.363035	3601.092361	23.323904
108.097254	3601.860815	23.328922
107.868794	3606.654954	23.333939
108.140521	3610.214963	23.338957
108.289731	3596.939503	23.343975
107.915354	3610.149195	23.348992
108.353183	3614.885008	23.354010
108.545573	3624.505280	23.359027
108.600656	3615.147211	23.364045
109.041541	3631.836485	23.369063
108.863612	3643.924855	23.374080
109.016565	3631.673075	23.379098
109.241824	3624.654212	23.384115
109.129714	3635.859723	23.389133
109.242196	3625.623138	23.394151
109.113619	3611.399748	23.399168
109.510133	3613.056024	23.404186
109.227998	3638.912078	23.409203
109.137571	3630.974586	23.414221
109.405314	3630.051167	23.419239
109.210513	3655.267080	23.424256
109.307936	3671.991892	23.429274
109.550014	3675.201921	23.434291
109.707837	3669.602537	23.439309
109.993414	3675.776016	23.444327
109.974409	3679.511828	23.449344
110.280462	3697.387929	23.454362
110.668550	3720.742215	23.459379
110.549770	3705.703204	23.464397
110.775397	3706.738366	23.469415
110.893805	3720.686349	23.474432
111.105297	3713.803765	23.479450
111.223857	3724.013619	23.484467
111.004567	3740.097188	23.489485
111.625090	3737.149866	23.494503
111.454627	3736.964943	23.499520
111.571564	3739.749830	23.504538
111.406795	3733.807103	23.509555
111.645673	3746.652605	23.514573
112.143607	3744.513079	23.519591
112.232837	3756.755804	23.524608
112.720159	3763.362681	23.529626
112.579976	3760.662106	23.534643
112.970942	3752.561746	23.539661
113.341952	3755.248949	23.544679
112.996997	3754.154934	23.549696
113.028562	3742.488832	23.554714
113.274200	3752.428315	23.559731
113.031920	3755.513883	23.564749
113.125105	3751.242575	23.569767
113.045731	3747.917432	23.574784
113.618377	3742.909863	23.579802
113.283622	3769.724367	23.584819
113.367889	3741.977278	23.589837
113.838423	3757.127845	23.594855
113.810913	3779.486992	23.599872
113.560267	3768.145043	23.604890
113.853221	3778.775691	23.609907
113.559524	3777.816501	23.614925
114.073098	3780.049276	23.619943
113.917226	3818.973225	23.624960
114.066417	3823.908559	23.629978
113.974897	3819.854748	23.634995
114.261235	3831.902768	23.640013
114.337653	3832.628758	23.645031
114.653549	3832.734507	23.650048
114.650685	3857.290729	23.655066
115.095765	3868.924384	23.660083
115.260737	3874.820844	23.665101
115.471583	3895.072205	23.670119
115.805393	3868.358588	23.675136
115.536606	3853.247966	23.680154
115.362755	3881.786159	23.685171
115.804917	3897.524783	23.690189
116.038111	3890.932021	23.695207
115.977557	3905.325070	23.700224
115.977229	3897.023363	23.705242
116.314746	3895.941756	23.710259
116.308766	3888.231501	23.715277
116.308315	3902.435100	23.720295
116.404996	3892.868624	23.725312
116.541732	3919.867274	23.730330
117.101572	3914.510607	23.735347
117.023571	3912.290646	23.740365
117.006851	3928.505495	23.745383
116.714867	3909.638839	23.750400
116.664122	3920.648995	23.755418
116.988278	3958.626706	23.760435
116.849462	3963.095924	23.765453
117.350399	3959.937035	23.770471
117.447343	3991.107103	23.775488
117.885159	3989.523511	23.780506
117.873567	3980.112660	23.785523
117.904569	4001.506018	23.790541
118.456534	4004.261194	23.795559
118.304134	4003.163294	23.800576
118.368132	4019.203885	23.805594
118.286459	4013.620134	23.810611
118.663455	4018.735199	23.815629
118.900485	4010.161546	23.820647
118.702302	4027.413120	23.825664
119.015920	4039.911495	23.830682
119.190559	4026.066536	23.835699
118.980880	4046.385612	23.840717
119.316637	4054.038866	23.845735
119.477214	4050.977142	23.850752
119.698957	4069.713231	23.855770
119.758646	4073.152094	23.860787
119.732639	4067.724470	23.865805
120.006951	4052.409943	23.870823
120.231259	4070.131489	23.875840
120.297617	4081.958981	23.880858
120.937503	4100.745694	23.885875
120.911844	4099.572910	23.890893
120.848950	4084.028258	23.895911
121.008422	4092.209059	23.900928
120.781286	4090.825879	23.905946
121.224443	4082.757076	23.910963
121.025879	4093.566200	23.915981
121.004484	4082.427071	23.920999
121.437048	4104.119948	23.926016
121.551559	4112.505030	23.931034
121.660093	4110.174694	23.936051
121.616406	4119.417375	23.941069
121.898164	4109.408000	23.946087
121.999087	4108.406022	23.951104
122.020966	4129.273925	23.956122
122.395765	4135.498000	23.961139
122.330942	4134.035243	23.966157
122.675822	4145.415599	23.971175
122.456918	4143.035824	23.976192
122.491990	4134.986395	23.981210
122.594392	4152.151828	23.986227
122.342103	4161.453411	23.991245
122.503908	4173.116782	23.996263
122.498290	4161.348640	24.001280
123.029436	4195.990520	24.006298
123.398052	4209.353529	24.011315
123.340125	4205.095650	24.016333
123.928032	4178.611549	24.021351
123.531877	4202.763837	24.026368
123.769754	4212.688758	24.031386
124.009423	4209.694640	24.036403
123.977042	4210.416186	24.041421
124.377790	4190.085568	24.046439
124.189514	4205.391299	24.051456
124.382081	4209.033030	24.056474
124.360928	4231.007346	24.061491
124.614397	4248.560111	24.066509
124.807064	4229.091351	24.071527
124.758450	4259.828549	24.076544
125.113753	4258.610914	24.081562
125.697298	4264.894248	24.086579
125.666521	4255.212000	24.091597
125.580297	4269.591519	24.096615
125.615256	4275.425760	24.101632
125.820673	4260.556254	24.106650
126.091163	4260.614395	24.111667
126.245797	4261.784156	24.116685
126.441058	4241.257119	24.121703
126.250806	4274.859369	24.126720
126.173856	4278.694069	24.131738
126.404507	4298.936388	24.136755
126.669243	4317.916452	24.141773
126.561114	4290.229108	24.146791
126.793269	4292.566334	24.151808
126.669878	4318.614998	24.156826
127.009427	4331.707729	24.161843
126.999551	4336.914778	24.166861
127.117645	4314.685099	24.171879
127.168950	4320.944200	24.176896
127.622330	4357.362616	24.181914
127.743571	4367.675007	24.186931
127.609467	4375.196222	24.191949
127.602020	4368.750104	24.196967
128.183832	4375.758944	24.201984
128.470190	4388.451076	24.207002
128.623480	4382.093350	24.212019
128.531867	4389.010326	24.217037
128.834004	4405.539905	24.222055
128.991065	4407.499411	24.227072
129.325544	4408.191448	24.232090
129.266814	4409.611431	24.237107
129.131426	4411.103527	24.242125
129.301108	4417.539164	24.247143
129.472537	4428.662177	24.252160
129.574850	4423.648253	24.257178
130.273067	4424.584118	24.262195
129.889927	4441.749000	24.267213
130.112812	4438.369433	24.272231
130.413129	4430.873645	24.277248
130.010142	4435.379168	24.282266
130.130017	4436.602717	24.287283
130.288425	4460.441336	24.292301
130.452326	4462.243818	24.297319
130.684866	4471.660352	24.302336
130.462805	4469.902685	24.307354
130.910972	4486.490109	24.312371
131.090199	4492.496652	24.317389
130.695680	4506.493090	24.322407
131.206501	4504.046224	24.327424
131.330484	4520.093170	24.332442
131.411705	4535.559416	24.337459
131.492218	4541.254736	24.342477
132.133396	4542.203971	24.347495
132.197107	4551.355149	24.352512
132.549173	4559.212648	24.357530
132.625237	4549.327134	24.362547
132.589536	4558.903002	24.367565
132.777949	4548.443818	24.372583
133.136487	4539.481300	24.377600
132.802276	4543.731401	24.382618
133.300245	4555.346601	24.387635
133.131529	4562.047265	24.392653
133.410723	4573.490758	24.397671
133.673971	4587.727789	24.402688
133.422083	4581.408191	24.407706
133.772623	4561.924346	24.412723
133.597980	4586.853210	24.417741
133.683020	4569.109651	24.422759
133.914113	4596.988756	24.427776
133.931589	4615.603749	24.432794
134.035023	4595.501253	24.437811
134.114806	4602.942356	24.442829
134.420999	4635.664944	24.447847
134.819412	4614.125910	24.452864
134.625684	4639.587925	24.457882
135.003389	4631.248951	24.462899
135.068322	4645.884546	24.467917
134.844101	4640.693408	24.472935
135.072776	4645.132807	24.477952
135.158606	4657.763021	24.482970
135.716344	4660.468153	24.487987
135.659376	4662.084321	24.493005
135.823487	4681.436178	24.498023
136.137353	4674.155748	24.503040
136.049105	4685.854131	24.508058
136.375489	4708.400037	24.513075
136.572810	4695.930247	24.518093
136.493279	4699.843035	24.523111
137.044447	4706.450008	24.528128
136.678294	4696.898490	24.533146
136.831672	4707.640045	24.538163
137.068852	4741.291573	24.543181
137.314349	4734.279891	24.548199
137.445798	4729.137039	24.553216
137.374208	4754.820004	24.558234
137.656169	4753.469965	24.563251
137.818337	4758.548334	24.568269
137.869441	4777.236704	24.573287
138.084190	4782.372534	24.578304
138.110243	4791.499368	24.583322
138.405277	4791.711331	24.588339
138.647826	4790.764255	24.593357
138.572868	4778.496868	24.598375
138.783936	4799.735197	24.603392
139.046751	4820.383511	24.608410
139.229571	4816.177415	24.613427
139.218503	4820.637975	24.618445
139.453963	4813.529884	24.623463
139.721282	4835.327469	24.628480
139.504189	4861.422447	24.633498
139.706295	4839.158058	24.638515
139.836370	4854.275998	24.643533
139.987104	4843.833472	24.648551
140.045469	4868.743578	24.653568
140.479898	4876.846686	24.658586
140.850128	4866.139529	24.663603
140.980996	4872.723108	24.668621
140.988036	4881.637782	24.673639
141.296286	4858.644408	24.678656
141.395853	4865.774101	24.683674
141.361920	4878.408141	24.688691
141.555395	4884.212876	24.693709
141.286144	4896.847231	24.698727
141.901144	4915.831570	24.703744
141.897299	4902.652333	24.708762
142.245627	4894.199569	24.713779
142.203626	4903.432201	24.718797
142.050158	4890.206043	24.723815
142.343917	4911.494248	24.728832
142.341604	4921.504981	24.733850
142.263806	4928.847081	24.738867
142.436172	4939.847865	24.743885
142.384784	4941.615503	24.748903
142.879311	4951.792982	24.753920
143.066376	4953.918073	24.758938
142.891868	4970.336855	24.763955
143.211305	4970.900696	24.768973
143.001751	4985.885905	24.773991
143.127100	4992.222807	24.779008
143.159081	5023.305288	24.784026
143.550156	5018.974569	24.789043
143.835840	5046.443488	24.794061
144.018606	5049.661442	24.799079
144.444189	5037.697370	24.804096
144.484303	5064.430117	24.809114
144.470499	5085.154411	24.814131
145.051326	5076.843450	24.819149
144.937836	5072.564197	24.824167
145.361756	5082.576654	24.829184
145.305985	5096.407804	24.834202
145.641959	5094.883060	24.839219
146.096144	5114.216661	24.844237
146.102536	5107.530545	24.849255
146.109646	5078.069972	24.854272
145.978068	5092.903815	24.859290
146.452823	5110.093430	24.864307
146.781826	5110.205296	24.869325
146.666122	5124.268423	24.874343
146.748234	5128.510128	24.879360
146.952750	5114.087208	24.884378
147.001768	5123.184457	24.889395
147.356550	5100.822813	24.894413
147.333992	5112.485858	24.899431
147.500697	5141.002573	24.904448
147.481726	5164.453072	24.909466
147.697463	5142.278125	24.914483
147.935840	5141.293923	24.919501
147.621863	5160.447021	24.924519
147.731559	5153.830825	24.929536
147.818987	5177.126357	24.934554
148.117504	5198.875990	24.939571
148.120931	5197.001846	24.944589
148.260911	5210.836974	24.949607
148.541814	5230.572588	24.954624
148.895043	5236.403422	24.959642
149.002590	5230.491896	24.964659
149.469725	5266.895608	24.969677
149.088714	5268.332698	24.974695
149.919403	5253.653819	24.979712
149.619363	5249.132894	24.984730
150.091136	5271.175662	24.989747
150.356534	5293.998645	24.994765
150.509368	5300.161441	24.999783
150.505611	5278.235174	25.004800
150.960035	5286.383226	25.009818
150.641162	5301.783662	25.014835
150.931111	5277.521794	25.019853
150.759076	5290.182137	25.024871
151.116136	5304.566142	25.029888
151.286231	5324.124116	25.034906
151.331055	5324.269947	25.039923
151.776709	5324.978307	25.044941
151.489012	5336.833365	25.049959
152.193076	5340.849130	25.054976
152.272884	5341.888421	25.059994
152.040336	5331.737646	25.065011
152.162657	5339.802800	25.070029
152.315233	5367.408458	25.075047
152.765808	5361.781946	25.080064
152.566895	5371.469537	25.085082
152.518861	5374.849320	25.090099
152.936231	5385.726864	25.095117
152.859322	5394.426168	25.100135
153.137159	5407.656389	25.105152
153.279395	5403.888747	25.110170
153.485499	5403.973678	25.115187
153.905430	5419.904541	25.120205
153.657369	5444.416579	25.125223
154.085288	5438.678425	25.130240
154.289490	5465.407190	25.135258
154.357005	5479.492728	25.140275
154.734496	5446.028768	25.145293
154.558349	5455.825252	25.150311
154.736560	5478.082574	25.155328
154.834297	5502.508824	25.160346
154.899829	5489.458971	25.165363
155.030067	5515.193703	25.170381
155.162935	5537.422380	25.175399
155.305307	5511.125784	25.180416
155.535545	5538.914197	25.185434
155.386840	5538.863651	25.190451
155.914545	5550.977860	25.195469
156.093470	5588.581178	25.200487
156.319967	5572.286007	25.205504
156.610269	5588.167592	25.210522
156.585719	5597.745407	25.215539
157.311062	5599.374148	25.220557
156.926207	5615.060611	25.225575
157.262497	5614.210209	25.230592
157.415231	5629.624386	25.235610
157.503892	5633.041485	25.240627
157.595540	5634.644615	25.245645
157.437503	5657.979063	25.250663
157.746774	5654.532992	25.255680
158.219184	5675.167890	25.260698
158.229260	5685.226676	25.265715
158.930642	5686.810959	25.270733
159.123316	5685.090142	25.275751
159.431600	5697.336000	25.280768
159.460439	5706.554647	25.285786
159.369844	5693.564281	25.290803
159.784058	5700.000994	25.295821
159.742195	5702.958546	25.300839
159.632635	5681.705134	25.305856
159.880107	5698.862086	25.310874
159.655696	5731.222661	25.315891
160.283062	5731.736442	25.320909
160.220692	5727.331626	25.325927
160.592308	5748.717175	25.330944
160.649050	5747.872009	25.335962
160.379108	5739.341016	25.340979
160.909174	5763.530484	25.345997
160.940878	5793.286912	25.351015
161.239650	5773.703804	25.356032
161.404692	5775.578697	25.361050
161.225101	5801.585186	25.366067
161.622762	5818.118599	25.371085
161.677496	5806.122298	25.376103
161.964667	5843.030745	25.381120
162.105650	5846.434915	25.386138
161.886408	5838.745937	25.391155
162.628270	5844.885252	25.396173
162.336347	5877.946698	25.401191
163.161335	5889.548242	25.406208
163.363672	5874.468245	25.411226
163.179855	5884.389894	25.416243
163.422785	5872.393157	25.421261
163.620343	5875.399771	25.426279
163.510426	5894.074352	25.431296
163.871574	5893.217073	25.436314
163.804704	5899.137650	25.441331
164.112375	5899.408572	25.446349
163.908197	5943.367803	25.451367
164.240293	5931.988221	25.456384
164.598951	5930.281687	25.461402
164.798338	5964.168498	25.466419
165.284422	5955.664054	25.471437
165.051147	5958.227661	25.476455
164.823057	5971.914031	25.481472
165.293739	5979.410504	25.486490
165.172211	5996.857511	25.491507
165.620375	6001.474042	25.496525
165.585289	5994.799911	25.501543
166.043556	6001.972439	25.506560
166.036640	6017.841757	25.511578
166.137505	6053.647937	25.516595
166.146047	6038.761233	25.521613
166.422016	6042.258504	25.526631
166.768766	6065.299902	25.531648
167.025421	6061.701007	25.536666
167.295044	6071.306495	25.541683
167.625106	6091.566617	25.546701
167.753627	6100.622952	25.551719
167.991015	6078.853762	25.556736
168.287260	6089.431317	25.561754
168.317377	6109.792601	25.566771
168.896835	6103.680715	25.571789
168.758312	6119.763629	25.576807
168.797785	6119.889879	25.581824
169.137471	6120.149610	25.586842
168.684583	6133.777193	25.591859
169.083415	6141.387594	25.596877
169.142634	6159.599076	25.601895
169.119581	6142.346431	25.606912
169.699524	6153.205921	25.611930
169.598307	6188.356767	25.616947
169.903192	6186.486242	25.621965
169.971455	6198.492603	25.626983
169.854164	6221.636104	25.632000
170.378242	6223.527719	25.637018
170.397828	6247.725114	25.642035
170.429271	6243.592866	25.647053
170.673353	6274.203386	25.652071
170.963033	6267.304202	25.657088
171.304129	6254.271177	25.662106
171.393757	6293.712765	25.667123
171.821394	6306.969793	25.672141
172.003875	6303.809909	25.677159
171.994234	6306.424425	25.682176
172.271594	6314.367215	25.687194
172.657333	6340.233548	25.692212
173.086815	6324.066670	25.697229
173.086254	6330.307194	25.702247
173.159530	6352.423245	25.707264
173.579760	6341.184726	25.712282
173.357803	6355.767745	25.717300
173.612834	6363.416977	25.722317
173.391572	6376.787187	25.727335
173.119726	6383.389122	25.732352
173.830202	6376.555022	25.737370
173.995436	6384.536849	25.742388
174.167641	6406.359831	25.747405
174.075287	6408.780530	25.752423
174.166313	6433.029012	25.757440
174.805235	6441.953964	25.762458
174.990544	6442.965660	25.767476
175.089599	6466.693525	25.772493
175.217874	6464.648191	25.777511
175.191873	6469.403451	25.782528
176.113399	6478.213612	25.787546
176.206390	6477.000176	25.792564
176.242243	6469.854231	25.797581
176.400004	6477.042770	25.802599
176.748010	6496.937818	25.807616
176.811401	6480.604078	25.812634
176.547495	6502.918588	25.817652
176.653159	6516.633366	25.822669
176.988217	6507.503117	25.827687
177.060095	6535.566740	25.832704
177.594934	6525.336035	25.837722
177.209115	6542.890710	25.842740
177.802089	6572.806698	25.847757
178.017847	6569.794430	25.852775
177.690518	6573.528526	25.857792
178.387530	6585.528159	25.862810
178.293302	6590.944013	25.867828
178.100805	6593.417905	25.872845
178.697741	6605.534493	25.877863
178.719064	6623.913032	25.882880
178.880347	6628.639758	25.887898
179.497709	6643.623404	25.892916
179.593059	6653.670692	25.897933
179.813528	6655.804676	25.902951
179.668228	6679.270446	25.907968
180.306395	6690.008868	25.912986
180.057464	6702.385779	25.918004
180.476430	6705.370146	25.923021
180.952731	6698.838806	25.928039
180.876253	6732.383841	25.933056
181.127873	6731.343018	25.938074
181.179385	6741.622829	25.943092
181.369988	6752.009603	25.948109
181.615669	6745.135987	25.953127
181.457997	6749.384678	25.958144
181.916861	6769.118037	25.963162
182.276164	6781.324426	25.968180
182.292611	6783.487018	25.973197
182.704447	6796.326156	25.978215
182.589810	6791.512301	25.983232
182.973584	6814.172657	25.988250
182.868730	6845.095916	25.993268
183.201000	6844.355974	25.998285
183.261104	6845.286009	26.003303
183.257658	6860.046018	26.008320
183.538536	6852.161688	26.013338
183.522828	6893.953197	26.018356
183.696115	6903.944849	26.023373
184.163487	6907.448099	26.028391
183.935570	6951.775544	26.033408
184.326130	6933.536242	26.038426
184.769517	6936.698140	26.043444
185.224159	6955.824479	26.048461
185.237797	6964.316360	26.053479
185.023223	6990.658205	26.058496
185.290130	6983.052139	26.063514
185.540545	7003.784540	26.068532
185.691136	7017.543522	26.073549
186.189860	7010.395666	26.078567
186.082913	7039.065013	26.083584
186.385426	7063.323235	26.088602
186.399267	7041.363631	26.093620
186.512582	7070.452218	26.098637
186.911914	7087.100497	26.103655
186.911964	7081.889597	26.108672
187.301959	7095.139734	26.113690
187.502358	7120.363082	26.118708
187.602708	7107.528995	26.123725
188.376412	7126.846561	26.128743
188.435348	7140.874376	26.133760
188.702722	7145.329362	26.138778
188.774187	7163.820739	26.143796
188.864576	7150.449601	26.148813
189.167355	7175.111160	26.153831
189.034295	7178.106109	26.158848
189.258508	7177.298954	26.163866
189.228860	7195.073501	26.168884
189.320986	7198.051723	26.173901
190.074272	7198.074610	26.178919
189.867122	7226.238336	26.183936
190.092441	7230.775110	26.188954
190.419960	7246.666018	26.193972
190.315957	7271.826501	26.198989
190.685018	7275.975703	26.204007
190.811749	7288.889917	26.209024
191.019861	7308.175154	26.214042
191.301934	7317.320620	26.219060
191.220941	7313.200368	26.224077
191.781588	7320.239644	26.229095
192.030722	7342.449315	26.234112
192.380829	7341.188999	26.239130
192.470354	7366.772850	26.244148
192.586140	7379.044748	26.249165
192.980889	7386.709986	26.254183
193.004614	7376.091845	26.259200
193.307049	7374.968558	26.264218
193.724342	7403.188508	26.269236
193.992303	7411.711063	26.274253
194.173975	7438.045284	26.279271
194.199933	7433.615155	26.284288
194.251459	7446.273375	26.289306
194.835576	7436.269806	26.294324
194.753783	7435.911689	26.299341
195.123084	7441.467427	26.304359
195.164616	7461.133189	26.309376
195.260537	7458.365787	26.314394
195.391794	7443.852026	26.319412
195.405193	7461.161419	26.324429
195.764955	7477.185051	26.329447
195.872004	7493.288256	26.334464
196.178701	7494.167743	26.339482
196.198544	7508.255897	26.344500
196.186653	7516.351439	26.349517
196.749593	7539.560112	26.354535
196.669742	7553.804173	26.359552
197.018484	7559.889424	26.364570
197.318701	7550.014594	26.369588
197.546128	7566.526405	26.374605
197.758349	7595.550008	26.379623
197.611179	7609.067317	26.384640
198.088544	7600.838283	26.389658
198.494720	7603.491417	26.394676
198.173873	7632.275547	26.399693
198.670038	7652.031816	26.404711
198.717776	7657.989642	26.409728
198.893576	7653.989105	26.414746
199.242381	7670.514835	26.419764
198.873378	7684.051534	26.424781
199.401491	7685.871004	26.429799
199.042860	7711.924808	26.434816
199.664606	7740.160411	26.439834
199.957880	7743.206308	26.444852
200.015723	7748.050483	26.449869
200.497901	7755.827465	26.454887
200.795045	7793.687070	26.459904
200.981260	7794.008421	26.464922
201.057729	7777.651090	26.469940
201.378376	7808.772526	26.474957
201.874605	7802.446142	26.479975
202.125836	7819.748923	26.484992
202.361856	7814.477528	26.490010
202.694422	7816.219065	26.495028
202.333204	7846.341215	26.500045
203.088300	7846.583539	26.505063
202.977027	7855.791160	26.510080
202.953483	7846.290172	26.515098
203.291401	7864.170918	26.520116
203.090966	7893.463290	26.525133
203.728031	7895.641234	26.530151
203.859212	7908.367784	26.535168
203.817841	7922.846812	26.540186
203.922526	7906.809158	26.545204
203.900525	7922.246589	26.550221
204.436417	7955.054347	26.555239
204.378739	7977.968494	26.560256
204.545520	7984.930600	26.565274
204.873935	8006.049155	26.570292
205.249642	8031.284380	26.575309
205.201720	8024.422491	26.580327
205.473615	8050.461671	26.585344
206.000382	8061.850285	26.590362
206.381303	8077.752901	26.595380
206.212655	8105.297537	26.600397
206.871380	8106.580410	26.605415
206.930839	8113.447684	26.610432
206.906849	8115.786861	26.615450
207.647758	8138.831556	26.620468
207.780545	8163.646402	26.625485
208.143373	8153.211918	26.630503
208.358939	8164.428356	26.635520
208.393172	8180.323776	26.640538
208.798304	8177.898156	26.645556
208.608592	8192.050685	26.650573
209.038026	8206.560870	26.655591
209.259170	8214.752156	26.660608
209.310452	8205.136205	26.665626
209.496721	8219.588132	26.670644
209.698546	8257.051126	26.675661
209.717223	8255.521022	26.680679
209.973167	8276.228988	26.685696
210.137184	8295.683387	26.690714
210.583350	8282.775456	26.695732
210.813349	8303.076630	26.700749
210.904552	8332.357072	26.705767
210.976578	8328.799590	26.710784
211.308187	8356.264372	26.715802
211.694216	8362.374492	26.720820
211.537120	8361.242005	26.725837
211.804916	8377.875585	26.730855
212.040794	8386.240944	26.735872
212.578630	8395.885062	26.740890
212.547297	8407.274779	26.745908
212.592304	8440.986889	26.750925
213.122066	8429.368473	26.755943
213.232532	8438.238942	26.760960
212.972874	8459.138661	26.765978
213.709153	8456.218028	26.770996
213.763790	8474.383335	26.776013
213.839648	8497.723520	26.781031
214.095137	8509.720404	26.786048
214.242572	8509.638635	26.791066
215.034328	8514.079044	26.796084
215.042955	8547.238995	26.801101
215.456745	8556.126359	26.806119
215.547677	8545.780645	26.811136
215.608163	8562.742442	26.816154
215.643755	8564.936377	26.821172
215.935466	8588.259934	26.826189
216.387863	8600.711084	26.831207
216.559645	8584.162325	26.836224
216.747152	8602.175874	26.841242
216.802094	8619.721465	26.846260
216.768855	8620.279141	26.851277
217.354663	8633.038275	26.856295
217.815609	8657.906793	26.861312
217.647623	8669.757178	26.866330
217.800708	8673.721913	26.871348
217.669368	8683.966654	26.876365
217.661654	8717.159589	26.881383
218.033895	8732.855589	26.886400
218.342630	8743.952296	26.891418
218.217779	8751.225196	26.896436
218.333834	8790.717512	26.901453
218.737506	8821.808330	26.906471
219.095820	8828.617087	26.911488
219.382596	8851.610269	26.916506
219.873037	8872.800092	26.921524
220.122276	8882.954515	26.926541
220.433999	8915.053876	26.931559
220.781253	8914.855605	26.936576
221.089814	8936.114943	26.941594
221.502557	8950.441123	26.946612
221.601371	8945.865427	26.951629
221.721853	8947.227066	26.956647
222.162931	8954.679068	26.961664
222.684877	8972.016361	26.966682
223.008804	8986.751052	26.971700
222.975497	8985.335793	26.976717
222.913478	9003.333531	26.981735
223.341493	8998.834172	26.986752
223.225798	9014.883583	26.991770
223.500575	9025.756118	26.996788
223.894681	9038.815830	27.001805
223.707441	9051.909381	27.006823
224.368073	9048.493922	27.011840
224.695757	9086.257072	27.016858
224.963672	9110.402876	27.021876
224.951948	9097.502989	27.026893
225.105051	9089.646534	27.031911
225.576106	9105.454961	27.036928
225.657621	9129.647343	27.041946
225.995510	9136.317051	27.046964
226.231626	9157.912367	27.051981
226.204625	9161.300514	27.056999
226.679590	9150.609777	27.062016
226.535547	9164.617796	27.067034
227.038024	9185.470526	27.072052
227.461132	9222.722824	27.077069
227.316826	9211.442043	27.082087
227.182730	9217.238321	27.087104
227.432284	9248.150661	27.092122
227.628049	9253.671132	27.097140
227.660653	9267.895794	27.102157
228.350101	9280.830512	27.107175
228.970399	9304.413525	27.112192
228.886803	9295.751743	27.117210
229.389041	9302.461315	27.122228
229.238480	9331.765437	27.127245
229.341409	9349.041629	27.132263
229.878736	9338.004933	27.137280
229.898952	9358.237371	27.142298
230.162660	9373.773151	27.147316
230.153473	9404.254393	27.152333
230.304167	9420.953316	27.157351
230.865945	9420.577824	27.162368
230.691279	9450.187021	27.167386
231.513214	9452.098360	27.172404
231.831771	9454.733998	27.177421
232.011273	9482.510207	27.182439
232.544121	9487.207912	27.187456
232.231037	9497.435160	27.192474
232.814714	9472.344061	27.197492
233.059434	9514.583879	27.202509
233.039965	9536.073864	27.207527
233.273455	9526.085961	27.212544
233.217660	9538.320153	27.217562
233.481240	9558.046357	27.222580
233.931724	9583.841174	27.227597
233.753887	9590.808156	27.232615
234.289160	9623.270565	27.237632
234.588104	9627.869910	27.242650
234.783057	9632.400584	27.247668
235.294601	9641.629214	27.252685
235.452861	9682.611724	27.257703
235.918397	9690.393996	27.262720
235.971693	9682.365492	27.267738
236.189936	9708.569075	27.272756
236.565772	9721.115676	27.277773
236.221336	9734.959608	27.282791
236.780946	9741.728415	27.287808
236.792160	9773.367198	27.292826
236.878614	9796.946205	27.297844
236.930666	9807.555195	27.302861
237.033296	9821.942067	27.307879
237.548245	9846.922471	27.312896
237.767861	9874.241414	27.317914
238.288912	9893.490714	27.322932
238.747694	9914.869902	27.327949
238.613788	9922.597734	27.332967
239.162135	9935.594899	27.337984
239.398661	9971.917271	27.343002
239.661818	9989.110189	27.348020
239.852881	9994.438720	27.353037
240.055456	10009.288146	27.358055
240.420186	10012.990617	27.363072
240.678119	10031.399015	27.368090
240.488871	10051.017911	27.373108
240.973303	10077.580619	27.378125
241.479568	10097.072058	27.383143
241.720753	10101.928410	27.388160
241.641317	10117.110452	27.393178
241.876108	10137.558909	27.398196
242.166254	10135.884526	27.403213
242.180963	10164.781648	27.408231
242.720951	10207.854351	27.413248
242.821129	10206.017581	27.418266
242.959733	10214.249536	27.423284
243.321828	10242.694782	27.428301
243.401889	10245.013932	27.433319
244.115667	10276.550243	27.438336
244.204118	10306.525577	27.443354
244.367998	10306.776633	27.448372
244.759373	10322.933418	27.453389
245.166706	10340.603070	27.458407
245.075549	10347.373320	27.463424
245.307014	10363.775540	27.468442
245.586345	10371.315589	27.473460
245.906648	10391.450927	27.478477
246.280850	10386.883669	27.483495
246.866070	10372.452123	27.488512
247.185914	10410.997949	27.493530
247.319122	10426.134914	27.498548
247.688569	10413.139475	27.503565
247.729976	10423.927076	27.508583
248.056622	10437.489028	27.513600
247.904603	10456.853365	27.518618
248.027968	10479.244977	27.523636
248.325718	10464.788376	27.528653
248.477070	10490.571076	27.533671
248.557876	10513.464432	27.538688
248.954318	10541.425627	27.543706
249.064063	10542.171634	27.548724
249.348241	10567.748195	27.553741
249.505721	10596.693404	27.558759
249.593338	10613.894733	27.563776
250.209093	10634.273799	27.568794
250.189928	10654.503366	27.573812
250.790369	10676.707733	27.578829
250.628603	10692.167802	27.583847
251.021267	10724.904151	27.588864
251.640713	10736.666939	27.593882
251.538478	10756.229002	27.598900
251.846489	10783.518363	27.603917
251.921096	10795.382237	27.608935
252.120969	10823.285819	27.613952
252.664380	10860.107756	27.618970
253.024428	10867.434629	27.623988
253.405939	10878.304194	27.629005
253.259614	10900.043838	27.634023
253.992422	10927.069486	27.639040
254.387744	10948.930025	27.644058
254.218711	10960.716120	27.649076
254.753997	10970.286622	27.654093
254.639024	10996.061364	27.659111
255.561795	11003.182688	27.664128
255.629994	11023.962288	27.669146
255.582938	11035.709381	27.674164
256.105717	11044.929100	27.679181
256.014674	11079.761845	27.684199
256.262204	11091.472912	27.689216
256.989291	11093.198481	27.694234
256.923092	11119.270208	27.699252
257.522182	11127.283981	27.704269
257.856829	11144.711317	27.709287
258.049452	11169.569033	27.714304
258.333301	11183.860241	27.719322
258.259361	11185.915879	27.724340
258.992522	11212.281848	27.729357
258.710022	11228.272823	27.734375
258.834256	11232.766801	27.739392
259.045239	11253.265526	27.744410
259.220643	11271.982027	27.749428
259.982454	11290.050261	27.754445
260.095651	11321.002553	27.759463
260.570238	11322.678489	27.764480
261.038146	11347.083747	27.769498
261.143129	11349.472987	27.774516
261.280234	11375.318550	27.779533
261.439043	11396.843034	27.784551
261.806611	11391.369914	27.789568
262.520414	11403.526440	27.794586
262.337326	11426.860933	27.799604
262.582121	11441.933163	27.804621
262.556181	11450.407993	27.809639
262.829442	11440.222482	27.814656
263.196063	11473.368777	27.819674
263.285882	11480.385313	27.824692
263.656891	11498.747581	27.829709
263.828224	11523.799998	27.834727
264.132046	11545.344837	27.839744
264.459718	11558.360888	27.844762
264.468362	11592.307044	27.849780
264.916165	11585.754006	27.854797
264.944777	11592.797247	27.859815
265.396820	11630.726288	27.864832
265.829044	11634.538517	27.869850
265.898171	11661.419048	27.874868
266.538258	11686.514799	27.879885
266.862675	11703.672666	27.884903
266.967914	11696.583798	27.889920
267.114658	11703.045909	27.894938
267.279327	11744.105136	27.899956
267.661164	11768.894712	27.904973
267.835644	11780.409602	27.909991
268.345877	11800.080508	27.915008
268.701835	11806.475799	27.920026
268.577774	11846.327319	27.925044
268.993119	11844.606871	27.930061
269.256839	11887.034176	27.935079
269.670335	11907.746061	27.940096
270.121564	11902.248707	27.945114
270.051184	11926.189994	27.950132
270.498012	11946.352085	27.955149
270.584603	11963.212364	27.960167
271.006850	11989.181965	27.965184
271.312550	12017.637335	27.970202
271.479231	12022.942216	27.975220
272.053590	12037.229521	27.980237
271.949579	12077.977137	27.985255
272.309367	12093.102670	27.990272
272.707689	12080.167285	27.995290
272.683280	12113.448834	28.000308
272.981427	12132.446989	28.005325
273.426028	12140.834993	28.010343
274.024956	12171.846540	28.015360
273.897051	12193.419465	28.020378
274.417153	12212.848980	28.025396
274.726104	12204.950280	28.030413
275.025439	12217.367334	28.035431
274.976988	12252.925066	28.040448
275.429673	12288.330760	28.045466
275.686871	12302.515510	28.050484
276.206885	12310.116764	28.055501
276.272233	12317.517417	28.060519
276.400813	12349.757952	28.065536
276.777299	12373.113237	28.070554
276.796076	12380.379025	28.075572
277.246470	12383.516462	28.080589
277.585634	12409.482353	28.085607
277.656198	12447.121856	28.090624
278.239187	12462.091120	28.095642
278.363294	12486.430450	28.100660
278.490726	12516.104131	28.105677
278.933529	12506.332670	28.110695
279.169911	12528.606070	28.115712
279.481954	12556.412215	28.120730
279.517951	12583.868546	28.125748
280.182886	12605.870366	28.130765
280.230200	12620.487905	28.135783
280.251350	12621.765437	28.140800
280.963464	12651.126918	28.145818
281.066715	12652.648496	28.150836
281.053885	12674.929396	28.155853
281.384403	12685.759778	28.160871
281.700586	12716.236916	28.165888
282.164329	12752.791986	28.170906
282.226114	12762.401620	28.175924
282.577436	12771.719209	28.180941
282.625765	12807.622989	28.185959
283.017700	12827.223319	28.190976
283.300174	12850.687791	28.195994
283.174284	12883.400790	28.201012
283.390213	12923.905469	28.206029
284.004562	12947.090729	28.211047
284.130577	12960.725789	28.216064
284.992187	13002.675969	28.221082
285.153971	13038.084109	28.226100
285.179053	13037.553793	28.231117
285.769354	13063.510765	28.236135
285.988790	13094.239370	28.241152
286.521253	13106.969174	28.246170
286.681990	13139.975674	28.251188
287.284270	13148.270406	28.256205
287.187265	13173.762851	28.261223
287.573748	13177.860322	28.266240
288.272254	13191.820115	28.271258
288.376948	13236.169592	28.276276
288.530551	13254.932190	28.281293
288.649961	13253.522833	28.286311
288.852051	13295.217977	28.291328
289.293719	13306.520440	28.296346
289.439316	13333.743292	28.301364
289.759204	13365.335817	28.306381
290.190598	13402.581541	28.311399
290.514691	13421.101877	28.316416
290.947205	13428.884354	28.321434
291.071531	13455.460968	28.326452
291.374204	13486.487763	28.331469
291.798488	13499.242842	28.336487
291.901884	13525.133677	28.341504
292.934169	13540.291283	28.346522
293.011890	13545.713786	28.351540
293.535088	13554.641032	28.356557
293.531632	13583.466961	28.361575
293.861207	13608.215231	28.366592
294.392500	13610.785699	28.371610
294.608333	13639.970207	28.376628
294.474132	13651.747790	28.381645
294.883479	13674.059592	28.386663
295.077112	13701.767529	28.391680
295.569282	13707.760554	28.396698
295.730940	13723.746805	28.401716
295.728081	13734.590429	28.406733
296.165771	13761.523880	28.411751
296.219310	13790.180042	28.416768
296.623740	13812.447153	28.421786
296.891404	13840.990821	28.426804
297.048746	13868.944546	28.431821
297.492145	13886.755553	28.436839
297.733952	13906.597873	28.441856
297.761168	13949.282412	28.446874
298.226478	13985.610759	28.451892
298.556355	13995.391922	28.456909
298.823039	14010.104476	28.461927
299.026615	14047.654835	28.466944
298.971268	14079.767709	28.471962
299.422395	14105.829719	28.476980
300.108290	14127.801801	28.481997
300.476217	14158.625295	28.487015
300.685104	14160.998578	28.492032
301.466902	14173.818823	28.497050
301.684201	14197.764017	28.502068
301.806891	14210.234644	28.507085
302.407759	14232.882724	28.512103
302.608497	14265.962130	28.517120
303.217736	14253.425858	28.522138
303.256885	14271.010988	28.527156
303.591488	14288.331450	28.532173
304.359173	14307.392484	28.537191
304.190973	14315.767053	28.542208
304.270519	14341.416534	28.547226
304.438482	14359.514656	28.552244
304.462470	14366.392058	28.557261
305.014566	14407.248317	28.562279
305.462213	14422.645166	28.567296
306.118763	14420.006126	28.572314
306.287296	14471.719815	28.577332
306.650721	14478.421429	28.582349
307.086879	14479.948850	28.587367
307.131006	14513.297302	28.592384
307.530080	14539.409581	28.597402
307.867762	14564.369131	28.602420
307.575778	14583.912831	28.607437
308.166952	14603.086892	28.612455
308.213755	14640.360403	28.617472
308.606411	14642.044725	28.622490
308.776827	14662.659291	28.627508
309.115217	14704.107855	28.632525
309.349659	14737.849211	28.637543
309.819392	14762.899132	28.642560
309.996922	14794.604641	28.647578
310.315517	14818.004554	28.652596
310.539163	14846.238959	28.657613
310.966932	14867.676380	28.662631
310.791533	14905.942142	28.667648
311.302384	14952.659108	28.672666
311.869019	14967.371831	28.677684
311.883762	15013.001684	28.682701
312.436852	15052.869801	28.687719
312.452369	15081.841813	28.692736
313.668210	15083.577710	28.697754
314.348260	15110.028991	28.702772
314.729552	15137.892756	28.707789
315.071508	15155.123111	28.712807
315.238136	15162.651737	28.717824
315.693629	15169.877362	28.722842
315.977641	15213.767708	28.727860
316.166543	15214.526074	28.732877
316.887884	15235.896573	28.737895
316.897323	15256.361995	28.742912
317.375763	15265.539480	28.747930
317.360607	15296.292907	28.752948
317.208746	15324.744613	28.757965
317.674745	15328.511183	28.762983
318.013442	15365.214958	28.768000
317.845868	15376.770020	28.773018
318.645697	15380.913234	28.778036
318.541887	15429.463396	28.783053
318.969554	15473.434718	28.788071
319.246040	15490.587997	28.793088
319.316251	15509.962662	28.798106
319.544584	15556.496389	28.803124
319.890584	15583.258919	28.808141
320.251866	15595.487910	28.813159
320.763127	15643.707022	28.818176
320.881310	15669.254514	28.823194
321.101591	15679.623694	28.828212
321.775021	15726.530348	28.833229
322.243632	15749.824876	28.838247
322.650112	15762.700516	28.843264
322.966833	15769.503362	28.848282
323.579752	15807.057933	28.853300
323.957957	15838.834761	28.858317
324.065102	15837.690383	28.863335
324.455408	15849.377392	28.868352
324.585997	15883.111495	28.873370
324.963791	15918.387029	28.878388
325.001942	15941.485044	28.883405
325.789373	15951.696091	28.888423
325.921909	15990.622685	28.893440
326.223225	16005.451101	28.898458
326.215762	16019.600897	28.903476
326.393107	16065.982186	28.908493
327.142710	16092.971999	28.913511
327.325655	16129.115413	28.918528
327.484350	16170.553278	28.923546
328.188839	16181.455819	28.928564
327.993206	16203.262749	28.933581
328.544999	16247.576543	28.938599
328.918477	16263.226939	28.943616
329.262915	16301.807235	28.948634
329.948498	16325.563163	28.953652
329.846941	16359.357090	28.958669
330.346232	16404.847756	28.963687
330.894373	16422.300696	28.968704
330.953149	16435.702368	28.973722
331.700975	16475.951552	28.978740
331.745643	16510.251153	28.983757
332.036302	16521.769146	28.988775
332.502050	16551.840327	28.993792
332.673324	16590.193031	28.998810
333.207862	16610.229845	29.003828
333.454430	16638.268155	29.008845
333.857568	16664.392637	29.013863
334.015895	16708.154905	29.018880
334.181923	16711.194403	29.023898
334.711541	16747.953281	29.028916
334.942225	16787.450247	29.033933
335.528690	16807.526005	29.038951
336.364149	16854.081336	29.043968
336.372470	16882.469893	29.048986
336.369484	16899.254766	29.054004
336.711220	16905.554367	29.059021
337.190768	16954.331041	29.064039
337.545675	16978.035383	29.069056
337.633940	17007.425893	29.074074
338.437964	17036.491755	29.079092
338.342436	17067.372116	29.084109
339.047883	17100.044520	29.089127
339.750440	17132.629211	29.094144
339.818044	17143.357086	29.099162
340.161848	17152.761190	29.104180
340.290358	17191.103456	29.109197
340.670327	17214.203537	29.114215
341.368720	17237.622988	29.119232
341.492618	17247.832576	29.124250
341.928548	17279.222851	29.129268
341.633425	17302.795494	29.134285
342.480411	17329.539593	29.139303
342.351658	17370.845167	29.144320
342.899444	17410.611187	29.149338
343.463652	17414.163445	29.154356
343.580302	17453.237989	29.159373
343.921717	17482.239225	29.164391
344.179125	17504.575092	29.169408
344.440580	17522.856717	29.174426
345.068153	17542.326114	29.179444
345.224789	17586.276982	29.184461
345.359557	17598.860111	29.189479
345.761916	17619.025596	29.194496
345.961956	17663.150747	29.199514
346.521313	17695.941465	29.204532
346.997279	17712.033380	29.209549
347.449931	17720.026585	29.214567
347.540719	17763.326856	29.219584
347.918375	17798.100552	29.224602
348.347848	17820.780379	29.229620
348.494630	17876.472297	29.234637
349.021066	17893.378769	29.239655
349.354619	17902.539130	29.244672
349.615713	17936.229113	29.249690
350.141102	17987.456841	29.254708
350.161458	18027.309913	29.259725
350.616214	18048.414507	29.264743
350.883510	18074.147591	29.269760
351.344403	18119.483877	29.274778
351.714638	18137.734033	29.279796
352.081393	18182.813378	29.284813
352.519209	18218.575706	29.289831
353.346585	18240.314059	29.294848
353.555438	18263.117631	29.299866
353.882218	18288.781332	29.304884
354.035559	18337.099041	29.309901
354.175551	18355.190458	29.314919
354.721984	18399.624448	29.319936
355.067754	18433.400758	29.324954
355.789925	18443.081970	29.329972
355.903214	18475.769834	29.334989
356.212708	18523.319930	29.340007
356.707990	18555.853431	29.345024
357.084919	18575.636562	29.350042
357.607579	18615.549931	29.355060
357.855317	18628.783477	29.360077
358.374461	18650.557533	29.365095
358.619110	18693.060938	29.370112
358.951132	18729.639393	29.375130
359.093860	18732.733556	29.380148
359.519533	18776.865400	29.385165
359.999154	18815.421400	29.390183
360.402208	18832.037141	29.395200
360.628058	18863.911211	29.400218
360.858586	18913.125736	29.405236
361.440355	18921.299952	29.410253
361.602974	18952.859945	29.415271
362.170283	18971.770418	29.420288
362.660270	18995.270947	29.425306
363.237178	19029.342873	29.430324
363.156531	19060.011726	29.435341
363.966161	19076.785946	29.440359
364.294857	19109.319690	29.445376
364.574219	19128.623100	29.450394
364.961891	19156.585658	29.455412
364.934420	19182.528367	29.460429
365.198726	19223.048595	29.465447
365.864620	19243.019648	29.470464
365.803153	19271.452227	29.475482
366.862360	19289.964987	29.480500
366.903973	19347.756707	29.485517
367.356766	19369.192753	29.490535
367.586893	19369.533115	29.495552
367.989957	19400.691711	29.500570
368.488065	19436.505045	29.505588
368.693563	19463.467362	29.510605
368.903888	19474.491579	29.515623
369.515389	19488.758056	29.520640
369.478253	19538.286623	29.525658
369.913713	19539.529357	29.530676
370.014064	19594.552233	29.535693
370.374425	19631.022396	29.540711
370.920882	19648.360839	29.545728
371.397600	19697.595353	29.550746
371.508300	19726.400643	29.555764
372.053167	19754.937226	29.560781
372.405656	19794.080818	29.565799
372.850966	19834.383490	29.570816
372.812382	19861.355251	29.575834
373.208452	19876.146297	29.580852
374.391346	19910.923839	29.585869
374.513972	19963.658656	29.590887
375.216874	19994.202953	29.595904
375.463755	20007.020031	29.600922
375.805232	20050.086276	29.605940
376.173640	20074.383963	29.610957
376.433554	20091.888430	29.615975
376.994676	20133.667029	29.620992
376.993436	20157.549859	29.626010
377.526021	20192.745954	29.631028
378.028259	20228.896076	29.636045
378.200376	20259.506478	29.641063
378.789245	20296.938165	29.646080
379.085479	20313.552554	29.651098
379.473563	20349.250477	29.656116
379.591478	20393.161620	29.661133
379.621631	20429.043373	29.666151
380.739763	20457.581048	29.671168
380.986721	20499.516505	29.676186
381.430376	20526.236286	29.681204
381.794734	20562.599072	29.686221
381.994012	20599.331276	29.691239
382.413612	20612.839103	29.696256
382.558294	20673.367562	29.701274
383.128746	20703.917709	29.706292
383.738519	20742.283303	29.711309
384.349113	20755.933096	29.716327
384.883837	20772.117611	29.721344
385.368241	20824.465938	29.726362
385.731878	20842.292983	29.731380
386.098329	20879.174742	29.736397
386.460921	20909.286693	29.741415
386.726382	20927.993901	29.746432
386.933600	20977.778023	29.751450
387.312718	20991.797289	29.756468
387.635349	21016.668263	29.761485
387.669944	21054.926242	29.766503
387.858626	21101.816397	29.771520
388.196466	21139.734420	29.776538
388.614398	21174.319402	29.781556
389.080830	21206.484550	29.786573
389.502504	21253.927795	29.791591
389.971631	21301.338113	29.796608
390.268766	21344.564797	29.801626
390.712263	21356.711990	29.806644
391.393235	21391.369050	29.811661
391.366804	21458.053016	29.816679
391.965726	21493.105337	29.821696
392.313693	21531.344170	29.826714
392.717530	21570.054674	29.831732
393.130232	21600.284136	29.836749
393.476708	21636.316442	29.841767
393.727236	21659.779912	29.846784
393.998247	21715.610823	29.851802
394.263938	21744.209559	29.856820
395.103496	21775.765563	29.861837
394.982342	21828.824015	29.866855
395.792897	21857.854747	29.871872
396.499752	21884.629396	29.876890
396.362738	21907.736318	29.881908
396.777029	21956.335178	29.886925
397.007564	22009.142200	29.891943
397.989458	22035.390831	29.896960
398.421595	22058.233682	29.901978
398.820809	22108.445063	29.906996
399.367716	22126.047724	29.912013
399.605697	22172.849189	29.917031
400.105943	22196.153925	29.922048
400.769596	22242.579428	29.927066
400.727855	22270.654428	29.932084
401.249583	22287.608747	29.937101
401.386697	22339.513142	29.942119
401.986537	22391.759035	29.947136
401.944588	22425.260689	29.952154
402.315014	22461.128435	29.957172
402.664119	22489.375715	29.962189
403.127129	22548.989722	29.967207
404.052571	22608.283190	29.972224
404.231904	22630.561619	29.977242
404.492699	22660.217433	29.982260
405.053270	22700.109139	29.987277
405.364619	22769.600802	29.992295
405.777543	22802.260287	29.997312
406.237594	22828.041426	30.002330
406.717945	22885.675190	30.007348
407.512384	22914.618984	30.012365
407.197564	22953.810863	30.017383
408.128265	22994.791445	30.022400
408.435648	23035.164060	30.027418
408.635781	23065.705610	30.032436
409.392735	23103.544665	30.037453
409.825464	23149.815333	30.042471
410.497523	23169.832668	30.047488
410.634514	23237.909341	30.052506
411.043983	23276.624439	30.057524
411.421282	23301.792491	30.062541
411.410346	23340.690698	30.067559
411.993851	23396.983255	30.072576
412.670699	23431.159633	30.077594
413.128923	23455.426915	30.082612
413.636397	23492.281683	30.087629
413.684982	23561.425871	30.092647
414.689832	23593.298556	30.097664
414.776870	23625.264578	30.102682
414.882987	23645.732288	30.107700
415.741350	23691.446958	30.112717
416.106721	23749.239845	30.117735
416.312671	23765.552528	30.122752
417.129575	23804.136895	30.127770
417.009471	23854.467665	30.132788
417.475567	23898.612710	30.137805
417.962761	23932.354746	30.142823
418.210015	23977.770672	30.147840
418.830376	24027.295369	30.152858
418.993513	24067.432562	30.157876
419.496890	24099.343322	30.162893
419.630879	24153.137954	30.167911
420.187169	24191.772567	30.172928
420.570532	24236.857676	30.177946
420.923954	24280.669156	30.182964
421.562906	24314.339588	30.187981
421.821297	24345.606998	30.192999
422.689033	24398.262659	30.198016
423.145060	24424.784809	30.203034
423.449338	24466.075855	30.208052
423.907032	24517.230798	30.213069
423.933487	24550.271283	30.218087
424.188992	24568.506457	30.223104
424.773009	24621.859290	30.228122
425.061058	24689.502188	30.233140
425.744898	24709.177264	30.238157
425.933077	24747.323678	30.243175
426.651836	24792.684404	30.248192
426.944469	24854.824391	30.253210
427.270823	24889.354901	30.258228
428.009549	24931.308505	30.263245
428.884964	24960.560952	30.268263
429.183082	25008.006833	30.273280
429.881088	25053.366958	30.278298
429.895347	25098.819653	30.283316
430.423753	25125.288374	30.288333
430.608945	25156.309208	30.293351
431.067019	25197.814727	30.298368
431.485805	25233.517982	30.303386
431.553518	25288.072986	30.308404
432.595450	25336.292531	30.313421
432.905178	25377.821419	30.318439
433.192453	25412.476134	30.323456
433.830875	25473.703492	30.328474
434.439570	25500.903789	30.333492
435.702748	25504.022270	30.338509
436.107084	25538.476573	30.343527
436.836996	25567.328370	30.348544
437.167522	25591.096319	30.353562
437.426208	25631.700788	30.358580
437.785350	25632.240736	30.363597
437.909776	25676.271836	30.368615
438.116956	25709.453446	30.373632
438.982624	25744.292395	30.378650
438.924387	25787.768953	30.383668
439.474397	25823.882251	30.388685
440.155494	25852.438269	30.393703
440.090969	25874.291364	30.398720
440.641187	25923.355420	30.403738
440.918285	25968.820637	30.408756
441.426860	25998.234820	30.413773
441.869823	26062.684981	30.418791
442.037208	26106.170812	30.423808
442.517823	26132.584351	30.428826
443.134331	26167.487403	30.433844
443.483260	26225.214190	30.438861
443.671702	26270.825739	30.443879
444.125050	26317.634656	30.448896
444.828502	26376.090256	30.453914
445.008028	26418.278678	30.458932
445.612290	26448.746965	30.463949
446.093863	26481.394342	30.468967
446.366011	26533.735570	30.473984
447.284782	26585.314156	30.479002
447.652038	26627.749621	30.484020
448.304125	26666.126479	30.489037
448.770581	26690.218856	30.494055
448.849549	26733.328240	30.499072
449.573524	26785.963030	30.504090
449.724180	26816.308211	30.509108
450.177150	26856.208583	30.514125
450.414274	26894.211382	30.519143
450.886023	26936.176198	30.524160
451.455888	26969.588933	30.529178
451.543527	27024.963062	30.534196
451.966473	27062.115529	30.539213
452.557028	27094.859619	30.544231
452.602491	27151.833846	30.549248
453.200928	27211.460835	30.554266
453.777569	27265.133849	30.559284
454.287039	27292.776033	30.564301
454.883893	27337.397286	30.569319
455.164140	27395.705510	30.574336
455.371706	27450.547110	30.579354
456.020696	27482.162632	30.584372
456.602014	27515.984561	30.589389
456.833673	27572.828504	30.594407
457.334269	27630.066618	30.599424
457.917176	27678.264549	30.604442
458.207399	27733.768360	30.609460
458.969666	27794.275521	30.614477
459.111304	27837.500340	30.619495
459.544035	27885.900286	30.624512
460.527938	27946.273598	30.629530
461.087728	27990.691356	30.634548
461.530863	28030.526702	30.639565
462.215514	28066.303946	30.644583
462.097334	28133.653855	30.649600
462.581511	28165.629044	30.654618
463.178648	28221.853337	30.659636
463.560011	28270.294394	30.664653
464.357562	28303.422950	30.669671
464.765287	28356.181047	30.674688
465.351678	28409.367144	30.679706
465.604619	28459.870680	30.684724
466.318468	28500.485634	30.689741
466.995228	28535.309450	30.694759
467.184962	28593.229804	30.699776
467.709077	28636.775111	30.704794
467.882204	28686.147525	30.709812
468.307731	28722.492537	30.714829
468.823119	28772.076770	30.719847
469.415786	28846.134604	30.724864
469.897775	28878.105173	30.729882
470.229041	28935.050721	30.734900
470.916251	28986.660600	30.739917
471.490970	29015.865602	30.744935
471.712666	29079.213938	30.749952
472.462221	29136.393867	30.754970
472.519241	29196.164495	30.759988
472.847060	29221.912524	30.765005
473.748670	29258.823505	30.770023
474.227139	29321.392209	30.775040
474.695924	29356.933374	30.780058
475.295692	29421.706200	30.785076
475.784872	29472.208378	30.790093
476.803201	29501.826697	30.795111
477.233091	29531.280455	30.800128
478.006328	29559.967819	30.805146
478.278288	29620.994544	30.810164
478.922442	29665.033629	30.815181
479.792697	29670.091527	30.820199
479.897078	29695.978112	30.825216
480.647652	29741.927141	30.830234
480.975266	29791.179412	30.835252
481.141665	29825.364629	30.840269
481.669030	29845.841167	30.845287
481.866852	29879.074977	30.850304
482.012200	29928.379826	30.855322
482.249993	29979.988052	30.860340
482.588618	30013.681491	30.865357
483.109729	30066.331457	30.870375
483.257423	30104.412901	30.875392
483.935757	30143.513995	30.880410
484.184353	30195.856068	30.885428
484.648383	30260.058261	30.890445
485.015943	30319.428171	30.895463
485.464837	30369.497994	30.900480
486.035608	30416.109413	30.905498
486.453390	30480.086626	30.910516
486.858405	30535.444846	30.915533
487.528454	30588.560749	30.920551
487.661699	30653.175498	30.925568
488.614402	30707.879137	30.930586
488.872970	30762.063535	30.935604
489.034258	30825.418772	30.940621
489.754450	30888.385389	30.945639
490.096330	30958.878525	30.950656
490.803704	31029.289493	30.955674
491.513564	31076.763006	30.960692
491.664124	31126.496269	30.965709
492.301551	31180.493206	30.970727
492.933225	31257.431952	30.975744
493.382083	31327.725940	30.980762
494.009638	31362.014671	30.985780
494.315518	31412.603251	30.990797
495.546885	31479.648613	30.995815
495.919358	31552.391556	31.000832
496.816033	31591.226398	31.005850
496.838518	31618.489059	31.010868
497.488454	31685.047626	31.015885
498.850339	31728.881912	31.020903
499.552686	31767.339130	31.025920
499.958436	31813.167626	31.030938
500.234611	31865.954990	31.035956
500.685062	31892.478578	31.040973
500.994060	31915.990670	31.045991
501.463995	31975.800454	31.051008
501.852138	32012.357295	31.056026
502.431106	32071.092538	31.061044
502.662469	32117.313440	31.066061
503.220576	32158.918616	31.071079
503.474737	32223.815766	31.076096
503.824730	32277.112725	31.081114
504.356352	32340.954928	31.086132
504.747627	32407.776659	31.091149
505.412393	32448.879058	31.096167
505.393357	32507.733472	31.101184
505.708044	32576.016588	31.106202
506.441982	32649.117681	31.111220
506.463731	32716.973340	31.116237
507.156161	32758.841700	31.121255
507.922089	32832.067624	31.126272
508.564629	32917.255762	31.131290
509.028838	32973.630992	31.136308
510.047718	33023.835136	31.141325
510.714672	33073.961890	31.146343
511.516899	33141.280125	31.151360
511.751868	33176.785687	31.156378
512.249710	33234.957711	31.161396
512.733613	33286.443570	31.166413
513.249466	33338.747767	31.171431
513.909343	33406.491221	31.176448
514.020851	33444.472345	31.181466
514.357881	33507.060515	31.186484
514.917054	33581.156653	31.191501
515.599706	33622.555428	31.196519
515.936018	33681.601174	31.201536
516.358570	33747.110314	31.206554
517.198826	33789.777047	31.211572
517.513162	33847.445037	31.216589
517.747176	33887.287336	31.221607
518.211434	33943.952787	31.226624
518.660726	34007.953476	31.231642
519.622165	34069.206842	31.236660
520.036440	34110.991853	31.241677
520.905493	34150.332305	31.246695
520.998556	34225.539886	31.251712
521.707511	34276.032287	31.256730
522.134938	34342.650311	31.261748
522.324503	34409.415152	31.266765
522.995183	34450.940907	31.271783
523.192576	34521.989692	31.276800
523.804117	34574.650917	31.281818
524.157628	34624.928518	31.286836
524.516626	34719.638011	31.291853
525.366226	34786.733841	31.296871
525.570079	34866.860732	31.301888
526.522443	34940.490598	31.306906
526.966230	34994.808930	31.311924
527.401234	35073.945667	31.316941
528.320589	35117.369297	31.321959
528.940169	35185.053663	31.326976
529.252374	35256.058030	31.331994
529.990583	35309.915343	31.337012
530.405196	35388.952726	31.342029
531.601098	35435.041951	31.347047
531.697104	35521.468882	31.352064
532.549788	35570.524453	31.357082
533.409789	35611.538882	31.362100
533.563937	35673.010033	31.367117
534.311522	35726.917552	31.372135
534.837588	35783.518731	31.377152
535.278252	35843.245504	31.382170
536.148080	35917.984861	31.387188
536.417815	35959.375272	31.392205
537.185059	36004.296667	31.397223
537.223963	36074.311281	31.402240
537.621243	36146.075100	31.407258
538.326116	36187.523547	31.412276
538.932317	36241.332913	31.417293
539.357804	36315.601421	31.422311
539.895456	36373.376434	31.427328
540.401175	36432.864083	31.432346
540.770594	36507.373008	31.437364
540.922436	36573.470604	31.442381
541.584153	36636.691501	31.447399
542.034982	36695.753616	31.452416
542.159428	36777.947081	31.457434
543.093688	36843.837555	31.462452
543.897002	36935.342421	31.467469
544.399865	36997.098197	31.472487
544.889087	37067.058103	31.477504
545.834196	37144.349442	31.482522
546.364344	37221.201582	31.487540
547.109486	37261.162684	31.492557
547.829980	37310.339558	31.497575
548.651000	37382.088847	31.502592
548.698728	37451.211162	31.507610
549.139983	37494.918383	31.512628
549.714902	37558.305198	31.517645
550.179014	37630.527841	31.522663
550.712919	37699.794875	31.527680
551.532232	37755.770049	31.532698
552.227558	37804.586363	31.537716
552.958863	37859.957856	31.542733
553.356757	37919.187388	31.547751
553.987485	37965.660546	31.552768
554.145721	38020.975708	31.557786
554.976506	38079.260093	31.562804
555.223306	38142.984043	31.567821
555.673334	38193.410407	31.572839
556.890615	38229.619070	31.577856
556.691312	38310.471810	31.582874
557.376599	38373.732820	31.587892
557.814364	38434.917299	31.592909
558.426973	38482.493055	31.597927
558.624110	38536.585180	31.602944
559.341532	38637.337788	31.607962
559.923372	38685.660818	31.612980
560.476312	38753.316061	31.617997
560.892696	38810.140604	31.623015
561.817007	38888.878879	31.628032
561.672546	38967.522603	31.633050
562.362710	39037.498025	31.638068
562.800816	39106.660057	31.643085
563.382866	39184.420965	31.648103
563.730593	39259.752851	31.653120
564.216498	39344.107608	31.658138
565.280231	39410.030308	31.663156
565.364210	39497.302131	31.668173
566.262269	39587.081608	31.673191
567.073219	39643.543771	31.678208
567.254847	39732.665886	31.683226
568.244672	39813.079608	31.688244
568.959383	39877.082733	31.693261
569.432537	39933.301755	31.698279
570.689484	40001.659695	31.703296
571.394059	40072.725639	31.708314
571.779749	40123.821362	31.713332
572.370035	40213.938843	31.718349
573.137672	40280.437559	31.723367
574.015059	40329.341112	31.728384
574.162711	40377.547847	31.733402
574.697976	40446.642138	31.738420
575.206731	40526.807073	31.743437
575.911019	40594.822962	31.748455
576.428282	40658.425885	31.753472
576.731191	40729.926876	31.758490
577.411519	40775.098665	31.763508
577.748955	40852.645156	31.768525
578.523186	40935.896002	31.773543
579.175587	41004.685837	31.778560
579.565761	41074.122115	31.783578
580.341560	41142.538573	31.788596
580.825330	41212.146147	31.793613
581.493784	41264.464100	31.798631
581.998300	41350.608491	31.803648
582.513031	41440.785562	31.808666
582.603470	41493.988756	31.813684
583.367305	41561.370283	31.818701
583.930406	41648.298680	31.823719
585.075987	41729.837814	31.828736
585.159542	41792.515713	31.833754
585.894462	41857.838744	31.838772
586.865202	41939.051001	31.843789
586.889433	42008.791170	31.848807
587.493198	42067.545714	31.853824
587.924041	42156.300772	31.858842
588.834455	42243.872242	31.863860
588.951264	42312.452430	31.868877
589.505884	42384.281335	31.873895
590.362497	42450.732240	31.878912
590.324211	42564.030708	31.883930
591.562675	42615.080953	31.888948
592.293248	42699.988514	31.893965
592.423541	42779.004205	31.898983
593.202479	42831.892386	31.904000
593.393683	42917.597137	31.909018
593.833789	42995.224140	31.914036
594.481054	43080.532340	31.919053
595.046338	43150.626272	31.924071
595.536932	43230.594557	31.929088
595.984420	43318.313904	31.934106
596.788424	43406.486188	31.939124
597.201528	43493.059813	31.944141
597.914538	43587.511116	31.949159
598.865831	43664.567205	31.954176
599.486618	43733.101019	31.959194
600.603058	43815.797024	31.964212
601.524858	43889.910409	31.969229
602.283007	43967.331136	31.974247
603.111822	44026.436760	31.979264
603.370301	44109.054796	31.984282
604.113964	44159.187156	31.989300
604.894785	44225.941118	31.994317
605.641033	44288.956885	31.999335
606.549678	44360.501418	32.004352
606.980765	44406.597806	32.009370
607.701127	44486.303127	32.014388
608.353285	44535.024662	32.019405
608.454539	44600.657829	32.024423
608.949607	44664.319348	32.029440
609.489583	44741.498377	32.034458
609.940784	44822.698676	32.039476
610.620629	44877.620131	32.044493
610.932595	44976.128966	32.049511
611.372228	45062.228838	32.054528
612.063994	45138.756190	32.059546
612.871669	45211.422513	32.064564
613.923229	45278.864849	32.069581
614.288183	45351.633253	32.074599
614.851103	45433.098755	32.079616
615.138985	45533.890826	32.084634
615.744511	45600.861807	32.089652
616.509573	45686.626678	32.094669
616.964986	45778.110268	32.099687
617.563447	45843.482586	32.104704
617.756917	45942.922230	32.109722
618.760305	46046.301493	32.114740
619.215697	46119.755714	32.119757
619.206469	46203.911192	32.124775
619.952134	46305.500078	32.129792
620.702418	46394.658424	32.134810
621.142060	46485.589241	32.139828
622.123436	46600.284747	32.144845
622.511073	46702.528503	32.149863
623.383452	46766.163310	32.154880
624.068075	46873.909613	32.159898
624.514920	46975.532546	32.164916
625.277373	47073.157126	32.169933
626.083882	47155.533982	32.174951
627.140073	47232.410732	32.179968
627.828469	47320.554381	32.184986
628.556920	47405.588027	32.190004
629.242385	47483.947902	32.195021
629.832612	47552.595560	32.200039
630.728723	47618.079641	32.205056
631.031390	47717.314904	32.210074
631.291690	47797.097726	32.215092
632.627774	47861.468003	32.220109
632.994968	47957.144781	32.225127
633.966797	48005.175288	32.230144
634.163210	48072.686848	32.235162
635.045972	48149.798084	32.240180
634.997684	48230.764130	32.245197
635.441160	48304.437278	32.250215
636.330375	48379.780117	32.255232
636.868599	48479.760430	32.260250
637.566036	48553.793632	32.265268
638.706131	48606.985942	32.270285
639.109310	48707.185539	32.275303
640.232619	48778.310519	32.280320
640.819799	48860.437398	32.285338
641.299553	48932.752344	32.290356
642.001637	48998.175380	32.295373
642.337002	49076.378657	32.300391
643.481337	49149.910935	32.305408
644.076208	49236.399059	32.310426
644.702579	49304.273469	32.315444
645.376513	49369.026669	32.320461
645.841961	49451.523577	32.325479
646.328881	49530.919461	32.330496
646.913812	49611.692101	32.335514
647.550317	49698.140720	32.340532
648.431182	49799.517718	32.345549
648.759928	49872.735923	32.350567
649.339852	49940.636071	32.355584
650.002156	50043.515734	32.360602
650.284562	50145.043938	32.365620
651.070010	50217.464878	32.370637
651.426579	50301.322426	32.375655
652.098519	50404.492982	32.380672
652.244793	50511.063648	32.385690
652.821191	50601.922234	32.390708
653.758060	50714.306848	32.395725
654.612607	50807.308991	32.400743
655.238846	50905.364295	32.405760
656.258678	51014.919988	32.410778
656.867359	51104.398711	32.415796
657.413762	51224.095485	32.420813
657.983297	51326.182593	32.425831
659.094475	51401.181800	32.430848
659.853371	51512.943612	32.435866
659.942721	51588.203893	32.440884
660.897450	51694.072848	32.445901
661.447088	51806.013046	32.450919
662.121440	51898.560733	32.455936
662.672509	51984.345325	32.460954
663.204255	52089.171457	32.465972
664.051547	52184.449120	32.470989
664.375325	52274.529897	32.476007
665.620724	52387.470297	32.481024
666.231141	52491.972961	32.486042
666.827401	52602.094061	32.491060
667.908379	52696.233406	32.496077
668.562942	52777.535370	32.501095
668.923946	52880.817986	32.506112
669.860249	52984.457797	32.511130
670.241768	53076.819474	32.516148
671.525942	53157.959054	32.521165
671.929729	53247.623728	32.526183
672.598061	53348.565060	32.531200
673.471935	53439.163697	32.536218
674.007871	53528.744682	32.541236
674.638771	53632.662662	32.546253
675.091290	53731.373822	32.551271
676.312406	53803.970087	32.556288
677.387770	53874.240734	32.561306
677.929659	53969.381822	32.566324
678.698817	54027.347293	32.571341
679.585054	54104.226163	32.576359
679.998837	54184.379864	32.581376
680.555408	54251.370490	32.586394
681.024826	54334.585794	32.591412
681.969385	54412.391206	32.596429
681.844475	54489.943973	32.601447
682.446588	54595.293258	32.606464
683.087382	54679.157690	32.611482
683.313767	54777.361904	32.616500
684.292301	54874.747482	32.621517
684.722653	54969.014811	32.626535
685.286491	55055.900682	32.631552
686.069450	55181.167573	32.636570
685.975326	55297.027961	32.641588
687.018181	55383.059123	32.646605
687.541447	55504.232954	32.651623
688.088317	55617.645546	32.656640
688.786984	55741.855951	32.661658
689.317119	55858.071443	32.666676
690.465559	55964.797298	32.671693
691.078974	56081.398382	32.676711
692.009943	56192.211111	32.681728
692.539027	56325.077086	32.686746
692.824486	56442.922244	32.691764
693.818315	56545.709138	32.696781
694.751609	56664.705915	32.701799
695.554197	56766.710526	32.706816
696.554860	56878.210603	32.711834
697.402224	57013.347402	32.716852
698.191942	57114.553543	32.721869
698.787884	57217.839295	32.726887
699.712820	57321.545123	32.731904
700.944165	57420.222120	32.736922
701.376529	57534.239650	32.741940
702.407806	57610.773492	32.746957
703.102780	57721.324214	32.751975
703.666844	57821.737231	32.756992
704.490493	57919.106647	32.762010
705.106247	58028.895009	32.767028
706.021569	58126.585185	32.772045
706.452230	58238.888438	32.777063
707.240706	58316.766724	32.782080
708.290266	58409.823605	32.787098
708.688760	58530.392180	32.792116
709.334750	58630.877912	32.797133
709.947121	58725.821921	32.802151
710.809250	58810.065512	32.807168
711.324849	58916.589614	32.812186
711.852907	59018.480583	32.817204
712.853633	59117.728591	32.822221
713.370521	59227.432494	32.827239
713.757837	59346.876799	32.832256
714.918511	59439.029196	32.837274
714.911179	59543.715751	32.842292
716.017481	59664.496577	32.847309
717.069030	59784.396198	32.852327
717.263725	59879.503151	32.857344
717.950597	59974.434492	32.862362
718.836858	60104.435908	32.867380
719.424942	60219.757506	32.872397
719.940831	60341.733139	32.877415
720.598715	60454.681194	32.882432
721.736936	60546.526453	32.887450
722.226777	60673.576436	32.892468
722.925637	60793.906871	32.897485
723.640208	60906.601658	32.902503
724.291263	60999.515263	32.907520
725.232823	61110.922475	32.912538
725.642641	61220.490685	32.917556
726.574430	61315.350017	32.922573
727.257114	61417.012808	32.927591
727.549297	61538.072086	32.932608
728.470139	61648.253384	32.937626
729.144521	61781.232938	32.942644
729.890200	61871.006728	32.947661
730.822582	61966.766423	32.952679
731.214006	62099.270266	32.957696
732.133198	62216.147528	32.962714
733.009494	62317.530096	32.967732
733.805797	62440.736103	32.972749
734.677341	62552.213404	32.977767
735.033587	62660.894539	32.982784
735.909273	62771.708775	32.987802
736.485551	62916.549234	32.992820
737.242695	63036.700144	32.997837
738.224444	63141.753994	33.002855
738.819731	63254.127661	33.007872
739.626733	63380.377573	33.012890
740.023659	63491.300079	33.017908
741.071291	63617.555967	33.022925
741.643871	63763.231015	33.027943
742.040429	63870.079090	33.032960
743.065346	64002.124165	33.037978
743.917255	64131.272340	33.042996
744.783750	64248.890527	33.048013
745.311605	64374.807153	33.053031
745.869107	64524.149651	33.058048
746.963918	64644.766242	33.063066
747.704494	64735.046536	33.068084
749.182703	64855.133336	33.073101
750.291676	64978.657025	33.078119
750.793614	65096.017934	33.083136
751.480217	65202.799791	33.088154
751.736423	65345.163105	33.093172
752.736503	65441.635898	33.098189
753.793693	65550.185065	33.103207
754.523462	65674.338112	33.108224
755.774245	65788.096537	33.113242
756.194648	65901.935827	33.118260
756.899708	66030.570300	33.123277
757.664064	66135.795533	33.128295
758.147854	66243.558109	33.133312
759.259828	66346.950814	33.138330
759.759211	66488.238897	33.143348
760.526527	66610.450809	33.148365
761.141948	66710.387506	33.153383
761.660830	66827.584808	33.158400
762.629762	66965.909835	33.163418
763.078096	67100.528993	33.168436
763.740555	67213.090243	33.173453
764.417461	67338.020573	33.178471
765.291995	67479.658033	33.183488
766.174782	67605.599004	33.188506
766.787522	67737.647612	33.193524
767.622021	67862.972291	33.198541
768.547065	67994.060659	33.203559
769.242636	68114.276705	33.208576
769.996680	68226.101334	33.213594
770.825037	68362.360096	33.218612
771.506024	68501.488845	33.223629
772.549373	68610.562078	33.228647
773.037956	68747.480024	33.233664
773.955670	68875.319430	33.238682
774.697710	68979.595521	33.243700
775.319254	69115.330700	33.248717
776.422152	69240.511856	33.253735
776.825764	69344.352538	33.258752
777.679013	69474.652841	33.263770
778.319578	69593.274365	33.268788
778.817795	69707.463015	33.273805
779.754392	69842.126696	33.278823
780.228516	69977.619943	33.283840
780.820972	70086.067232	33.288858
781.775911	70221.615416	33.293876
782.150975	70365.852167	33.298893
783.247497	70500.133279	33.303911
783.895624	70632.630524	33.308928
784.675224	70782.373295	33.313946
786.013915	70911.407396	33.318964
786.846285	71033.722934	33.323981
788.022850	71150.039204	33.328999
788.534149	71285.604250	33.334016
789.972666	71425.455495	33.339034
790.722677	71545.473529	33.344052
791.348144	71679.055907	33.349069
792.496571	71799.635529	33.354087
793.021494	71906.099010	33.359104
793.700204	72043.557032	33.364122
794.558653	72171.413555	33.369140
795.094025	72294.076247	33.374157
795.939372	72430.269975	33.379175
796.682410	72577.072339	33.384192
797.566756	72683.651074	33.389210
798.428136	72813.825162	33.394228
798.617630	72957.680193	33.399245
799.829160	73078.477939	33.404263
800.625666	73228.355278	33.409280
801.239108	73369.177533	33.414298
802.099428	73504.996246	33.419316
802.991882	73643.207015	33.424333
804.254850	73769.861798	33.429351
804.556734	73913.160878	33.434368
805.858659	74047.095312	33.439386
807.373973	74156.821062	33.444404
808.191337	74273.397055	33.449421
809.169519	74407.785569	33.454439
809.849848	74538.265600	33.459456
810.517168	74652.756375	33.464474
811.047755	74773.796246	33.469492
811.842025	74909.223698	33.474509
812.408724	75023.752025	33.479527
813.089582	75170.108103	33.484544
813.888121	75312.853867	33.489562
814.691486	75452.779380	33.494580
815.183680	75569.567829	33.499597
815.895254	75718.243366	33.504615
816.496061	75857.016052	33.509632
817.719275	75984.670595	33.514650
818.522671	76145.077395	33.519668
819.213842	76301.152994	33.524685
819.866255	76441.179360	33.529703
821.152958	76573.721686	33.534720
821.488476	76710.640069	33.539738
822.317664	76870.592611	33.544756
822.976900	77035.532571	33.549773
824.239138	77160.347986	33.554791
824.857553	77295.876254	33.559808
825.489969	77450.388693	33.564826
826.602085	77590.036618	33.569844
827.269888	77729.537444	33.574861
828.324492	77897.416379	33.579879
829.158216	78039.187555	33.584896
829.754820	78158.635220	33.589914
830.421391	78307.550832	33.594932
831.025170	78453.448325	33.599949
832.044170	78588.039294	33.604967
832.819660	78716.548986	33.609984
833.448069	78842.439973	33.615002
834.414447	78997.534277	33.620020
835.112514	79166.183798	33.625037
836.035881	79302.388768	33.630055
836.724431	79456.804806	33.635072
837.394001	79611.958749	33.640090
838.513979	79743.036050	33.645108
839.212316	79913.070056	33.650125
840.019674	80065.421397	33.655143
840.953116	80210.112213	33.660160
841.527954	80360.853113	33.665178
842.666638	80527.536342	33.670196
843.200499	80706.743501	33.675213
844.288082	80839.407601	33.680231
844.986065	81008.741589	33.685248
845.727239	81161.807137	33.690266
846.800801	81308.056957	33.695284
847.445068	81490.573018	33.700301
848.550925	81663.342602	33.705319
849.349989	81823.057569	33.710336
850.679563	81942.765095	33.715354
851.890365	82102.148385	33.720372
852.807954	82262.808407	33.725389
853.725930	82402.550272	33.730407
854.595855	82553.282497	33.735424
855.830421	82702.494254	33.740442
856.621399	82844.252461	33.745460
857.511038	83016.233116	33.750477
858.494845	83160.865064	33.755495
859.073118	83301.870517	33.760512
860.086038	83433.638659	33.765530
861.130039	83576.947511	33.770548
861.211642	83749.421411	33.775565
862.452263	83892.427767	33.780583
863.067571	84034.045290	33.785600
863.933543	84199.503862	33.790618
864.803907	84353.189690	33.795636
865.404534	84518.188286	33.800653
866.027251	84668.462952	33.805671
866.785578	84851.929918	33.810688
867.480628	85002.498505	33.815706
868.288923	85173.218299	33.820724
869.293285	85352.650300	33.825741
870.162017	85521.034531	33.830759
871.092002	85698.811295	33.835776
871.670473	85854.655854	33.840794
873.226584	86010.415967	33.845812
874.000203	86187.754152	33.850829
875.114002	86360.014023	33.855847
876.455507	86509.568359	33.860864
877.387490	86661.475303	33.865882
878.444285	86819.227734	33.870900
878.966593	86964.263632	33.875917
880.372134	87132.501410	33.880935
881.146924	87282.976843	33.885952
881.932796	87422.594065	33.890970
883.067319	87559.541441	33.895988
883.911359	87716.126621	33.901005
884.638222	87881.419522	33.906023
885.671960	88037.342818	33.911040
886.385274	88185.050234	33.916058
887.373474	88320.121722	33.921076
888.357669	88469.760356	33.926093
889.111044	88611.737551	33.931111
890.032834	88754.383825	33.936128
890.493737	88906.338935	33.941146
891.650908	89044.797256	33.946164
892.083330	89178.718941	33.951181
892.718544	89335.393758	33.956199
893.616528	89497.322512	33.961216
894.407123	89644.146831	33.966234
895.354599	89807.360407	33.971252
895.754118	89970.007496	33.976269
896.736586	90117.385247	33.981287
897.644531	90290.214387	33.986304
898.468238	90460.597129	33.991322
899.167598	90640.443003	33.996340
900.211813	90804.843501	34.001357
900.893960	90964.001986	34.006375
901.957656	91143.924419	34.011392
902.513717	91315.661102	34.016410
903.601599	91489.715943	34.021428
904.153411	91680.238141	34.026445
905.389312	91875.648292	34.031463
906.323939	92044.986254	34.036480
906.694283	92222.411380	34.041498
908.050702	92405.642758	34.046516
909.265634	92604.036718	34.051533
910.001564	92783.994015	34.056551
910.822692	92950.066276	34.061568
911.598118	93140.050576	34.066586
913.041978	93315.597817	34.071604
913.887505	93492.314690	34.076621
914.711390	93693.339043	34.081639
915.755929	93879.854543	34.086656
916.556006	94046.950473	34.091674
917.578099	94238.174823	34.096692
918.446688	94417.324986	34.101709
919.364721	94602.322678	34.106727
920.786697	94790.795530	34.111744
921.693402	94959.652307	34.116762
923.056451	95148.352859	34.121780
923.753529	95332.652088	34.126797
924.562858	95497.496958	34.131815
925.839732	95661.379645	34.136832
926.343496	95861.715324	34.141850
927.189188	96054.970530	34.146868
927.883698	96225.567406	34.151885
928.928572	96409.159080	34.156903
929.808532	96589.456339	34.161920
930.455852	96772.926491	34.166938
931.510588	96970.287641	34.171956
932.314059	97167.634894	34.176973
933.673312	97346.377425	34.181991
934.776032	97544.463183	34.187008
935.575983	97726.180875	34.192026
936.949815	97900.506782	34.197044
937.572347	98085.851796	34.202061
938.349071	98283.877038	34.207079
939.372274	98465.487344	34.212096
939.850005	98644.296189	34.217114
940.870206	98838.645861	34.222132
941.962352	99039.378664	34.227149
942.422676	99214.288755	34.232167
943.708013	99420.075908	34.237184
944.866726	99640.014981	34.242202
945.900572	99811.181960	34.247220
946.562528	99997.275359	34.252237
947.583017	100191.743143	34.257255
948.734739	100374.245063	34.262272
949.654106	100569.707375	34.267290
950.511800	100760.224511	34.272308
951.558531	100924.110413	34.277325
952.278566	101121.129278	34.282343
953.256939	101284.598322	34.287360
954.020073	101462.164664	34.292378
954.971786	101655.148381	34.297396
955.697975	101859.699369	34.302413
956.474021	102048.334104	34.307431
957.605500	102218.507371	34.312448
958.446076	102417.725943	34.317466
960.039132	102609.452457	34.322484
961.137752	102787.783069	34.327501
962.079210	102991.889775	34.332519
963.483286	103175.908722	34.337536
964.182816	103355.531120	34.342554
965.084779	103530.879377	34.347572
965.887170	103725.036749	34.352589
966.851063	103909.785780	34.357607
967.846632	104098.481738	34.362624
968.556424	104295.286264	34.367642
969.917841	104486.976456	34.372660
970.562918	104695.780353	34.377677
971.126939	104911.038611	34.382695
972.587104	105087.945225	34.387712
973.398815	105278.066813	34.392730
974.506853	105494.937020	34.397748
975.289288	105689.283435	34.402765
976.030206	105897.251727	34.407783
977.536832	106108.425868	34.412800
978.180925	106309.562277	34.417818
979.414340	106515.890198	34.422836
980.544234	106717.430782	34.427853
980.845795	106924.327361	34.432871
982.164929	107128.967952	34.437888
983.093004	107335.701021	34.442906
984.579483	107543.369360	34.447924
985.771038	107744.198445	34.452941
986.448755	107951.357631	34.457959
987.833917	108139.227027	34.462976
988.518422	108374.428455	34.467994
989.411847	108565.839612	34.473012
990.439935	108771.794867	34.478029
991.191100	108984.484706	34.483047
992.122188	109183.379285	34.488064
992.869898	109387.853101	34.493082
994.059677	109610.316606	34.498100
995.082307	109825.476137	34.503117
995.715008	110048.655888	34.508135
997.007929	110255.870818	34.513152
997.886575	110474.327141	34.518170
998.923844	110708.870323	34.523188
999.964664	110921.692438	34.528205
1000.765201	111134.125253	34.533223
1002.216411	111347.579632	34.538240
1003.231612	111585.148700	34.543258
1004.067531	111817.986809	34.548276
1005.135722	112016.170444	34.553293
1005.810044	112226.302015	34.558311
1006.941293	112447.519322	34.563328
1007.949725	112686.821871	34.568346
1009.125419	112893.949753	34.573364
1010.410697	113125.356843	34.578381
1011.155458	113363.315470	34.583399
1012.481820	113560.479684	34.588416
1013.042178	113780.053951	34.593434
1014.215528	113983.022862	34.598452
1015.396310	114224.527260	34.603469
1016.022855	114445.324690	34.608487
1017.342756	114629.259770	34.613504
1018.000448	114844.405365	34.618522
1019.019005	115070.096275	34.623540
1020.282670	115292.543501	34.628557
1021.060918	115479.930747	34.633575
1022.333006	115674.572732	34.638592
1023.380986	115907.359907	34.643610
1024.437182	116106.867262	34.648628
1025.331122	116333.209780	34.653645
1026.278530	116550.221074	34.658663
1027.410690	116743.854795	34.663680
1028.325159	116965.017471	34.668698
1029.483715	117195.326682	34.673716
1030.322204	117412.818730	34.678733
1031.379849	117628.730628	34.683751
1032.889093	117843.480063	34.688768
1033.961062	118055.997480	34.693786
1035.222513	118275.187418	34.698804
1036.054423	118478.169449	34.703821
1036.350410	118710.825295	34.708839
1037.864976	118930.738708	34.713856
1038.676436	119148.134546	34.718874
1039.994198	119386.860866	34.723892
1041.153021	119599.755615	34.728909
1041.915181	119824.690831	34.733927
1043.262920	120039.369517	34.738944
1044.918381	120266.327364	34.743962
1046.153669	120485.538642	34.748980
1047.520058	120685.331194	34.753997
1047.981796	120895.411064	34.759015
1049.227261	121125.382993	34.764032
1050.245402	121330.407212	34.769050
1051.116918	121547.127097	34.774068
1052.084096	121776.630639	34.779085
1052.995015	122003.344947	34.784103
1054.110311	122209.626471	34.789120
1055.547472	122436.612082	34.794138
1057.654352	122649.436206	34.799156
1058.838898	122838.249434	34.804173
1059.828014	123042.454205	34.809191
1060.836728	123245.681440	34.814208
1061.823185	123458.747113	34.819226
1062.749569	123654.831182	34.824244
1063.626378	123873.354224	34.829261
1064.507598	124085.123920	34.834279
1065.542657	124282.727558	34.839296
1066.191187	124505.550831	34.844314
1067.291918	124715.856843	34.849332
1068.548134	124936.935635	34.854349
1069.684337	125176.601220	34.859367
1070.149723	125389.462701	34.864384
1070.857240	125618.215404	34.869402
1071.892225	125841.022917	34.874420
1073.228481	126064.631447	34.879437
1073.826955	126313.075916	34.884455
1074.928315	126544.495398	34.889472
1075.987128	126801.498345	34.894490
1077.292505	127034.421387	34.899508
1078.443865	127251.314374	34.904525
1079.143086	127502.730299	34.909543
1080.061816	127759.511061	34.914560
1081.180265	127998.074156	34.919578
1082.211591	128244.029705	34.924596
1083.686964	128475.224801	34.929613
1084.920061	128720.010231	34.934631
1085.920998	128964.975365	34.939648
1087.447474	129199.399428	34.944666
1088.138449	129416.307817	34.949684
1089.302945	129637.334814	34.954701
1090.365559	129880.890222	34.959719
1091.547291	130091.549853	34.964736
1092.648660	130332.073191	34.969754
1093.395860	130568.017876	34.974772
1094.625428	130778.420798	34.979789
1095.347525	131013.599850	34.984807
1096.255168	131277.725379	34.989824
1097.444749	131519.637629	34.994842
1098.443846	131749.807828	34.999860
1099.835979	131966.377505	35.004877
1100.614436	132219.352622	35.009895
1101.216479	132481.523369	35.014912
1102.741430	132733.669567	35.019930
1103.645515	132983.854118	35.024948
1104.700749	133214.862397	35.029965
1105.350550	133488.201112	35.034983
1106.739916	133762.167991	35.040000
1108.123039	134006.311094	35.045018
1109.195918	134248.415692	35.050036
1110.754020	134506.934057	35.055053
1111.665149	134785.514177	35.060071
1112.520919	135059.504237	35.065088
1114.044336	135293.226502	35.070106
1114.955768	135548.361248	35.075124
1116.520766	135806.876285	35.080141
1117.434855	136077.822929	35.085159
1118.909659	136332.820173	35.090176
1120.627286	136569.511439	35.095194
1121.161938	136838.802980	35.100212
1122.426270	137078.805507	35.105229
1123.732837	137338.021969	35.110247
1124.582642	137604.085747	35.115264
1125.715959	137868.646947	35.120282
1126.804942	138119.614276	35.125300
1127.767049	138380.087563	35.130317
1129.182522	138647.651163	35.135335
1130.162046	138894.598173	35.140352
1131.153685	139159.941143	35.145370
1132.047077	139433.441949	35.150388
1133.356210	139701.665539	35.155405
1134.676365	139957.781461	35.160423
1135.800844	140228.321909	35.165440
1136.894985	140510.026852	35.170458
1138.252418	140785.845747	35.175476
1139.468301	141026.569578	35.180493
1140.732793	141285.037761	35.185511
1141.662231	141555.532343	35.190528
1143.141366	141818.153294	35.195546
1144.025389	142080.544853	35.200564
1145.322431	142333.804466	35.205581
1146.396508	142607.034993	35.210599
1147.362924	142900.991335	35.215616
1148.658712	143159.810973	35.220634
1149.688118	143422.379050	35.225652
1150.952092	143698.706185	35.230669
1152.122973	143955.232007	35.235687
1153.129885	144227.129760	35.240704
1154.228591	144498.443888	35.245722
1155.188089	144771.038472	35.250740
1156.585066	145040.976171	35.255757
1158.160032	145317.911597	35.260775
1159.402461	145578.939201	35.265792
1160.531423	145839.150554	35.270810
1161.425880	146128.276773	35.275828
1162.633704	146391.471876	35.280845
1163.806867	146657.210870	35.285863
1164.588404	146922.559987	35.290880
1165.915110	147174.340986	35.295898
1166.712463	147434.682252	35.300916
1168.000010	147703.136686	35.305933
1169.030457	147954.807255	35.310951
1170.085259	148233.221012	35.315968
1171.586644	148499.502946	35.320986
1172.271513	148771.526976	35.326004
1173.484734	149031.747809	35.331021
1174.762773	149289.347340	35.336039
1175.355942	149568.253447	35.341056
1176.694827	149865.694045	35.346074
1177.830310	150132.137192	35.351092
1178.801148	150397.683654	35.356109
1180.042518	150705.140884	35.361127
1181.014259	151007.622912	35.366144
1182.337462	151285.977757	35.371162
1183.281593	151591.157863	35.376180
1184.180340	151895.536281	35.381197
1185.418071	152168.940214	35.386215
1186.471239	152476.113523	35.391232
1188.044954	152779.297033	35.396250
1188.790935	153107.174425	35.401268
1190.111268	153396.656112	35.406285
1191.606679	153698.566293	35.411303
1192.916185	154032.662432	35.416320
1194.251715	154335.212914	35.421338
1195.553490	154627.611681	35.426356
1197.050041	154948.189492	35.431373
1198.351629	155243.802052	35.436391
1199.636145	155538.493780	35.441408
1200.637687	155845.969398	35.446426
1201.845265	156160.072716	35.451444
1202.875185	156461.498167	35.456461
1204.265386	156767.483652	35.461479
1205.509370	157057.297482	35.466496
1207.847805	157325.178619	35.471514
1209.427619	157624.226418	35.476532
1210.719233	157897.244017	35.481549
1211.877863	158205.143695	35.486567
1212.610487	158510.300021	35.491584
1214.294778	158777.791672	35.496602
1214.985486	159060.354269	35.501620
1216.398028	159359.886858	35.506637
1217.973785	159661.056555	35.511655
1219.189189	159959.205430	35.516672
1220.681567	160227.740678	35.521690
1221.919778	160498.273274	35.526708
1223.125984	160794.438230	35.531725
1224.331913	161090.478550	35.536743
1225.437967	161366.481026	35.541760
1226.521185	161662.647273	35.546778
1227.704541	161948.383830	35.551796
1228.745512	162225.988651	35.556813
1229.925995	162519.963042	35.561831
1230.898325	162828.144612	35.566848
1232.346444	163125.479120	35.571866
1233.417927	163406.118955	35.576884
1234.240571	163696.456323	35.581901
1235.405241	164014.383733	35.586919
1236.731533	164332.933925	35.591936
1237.875723	164622.438091	35.596954
1238.731832	164929.791731	35.601972
1240.065140	165241.534728	35.606989
1241.298297	165547.853737	35.612007
1242.082116	165858.321761	35.617024
1243.734973	166187.870062	35.622042
1244.915134	166523.157571	35.627060
1246.033054	166815.002892	35.632077
1247.174538	167110.576493	35.637095
1248.448313	167429.957959	35.642112
1250.058591	167725.065081	35.647130
1251.410776	168013.758641	35.652148
1252.642796	168294.099843	35.657165
1254.055732	168603.024726	35.662183
1255.488351	168906.797126	35.667200
1256.820812	169189.005351	35.672218
1258.113848	169501.420264	35.677236
1259.224675	169800.404983	35.682253
1259.946526	170087.554050	35.687271
1261.218958	170386.833264	35.692288
1262.636895	170704.616028	35.697306
1263.872058	171025.235449	35.702324
1264.883123	171329.639646	35.707341
1266.356922	171655.578900	35.712359
1267.784060	171957.253969	35.717376
1269.101756	172257.680193	35.722394
1270.443387	172590.512828	35.727412
1271.753425	172907.719816	35.732429
1273.166796	173211.791063	35.737447
1274.118656	173512.945766	35.742464
1275.676492	173835.930061	35.747482
1276.564997	174159.712326	35.752500
1277.660360	174488.868553	35.757517
1279.151625	174800.119795	35.762535
1280.002298	175124.892122	35.767552
1281.502092	175460.599900	35.772570
1282.924179	175781.653091	35.777588
1284.279027	176112.579861	35.782605
1285.745784	176450.393997	35.787623
1287.030146	176780.232982	35.792640
1288.149032	177095.647083	35.797658
1289.707941	177435.318456	35.802676
1290.875506	177759.003121	35.807693
1292.352845	178088.844595	35.812711
1293.401371	178451.907545	35.817728
1294.779850	178763.495090	35.822746
1296.350107	179100.143082	35.827764
1297.551850	179426.180985	35.832781
1298.710099	179766.658086	35.837799
1300.036120	180128.494620	35.842816
1301.073473	180458.310354	35.847834
1302.334313	180788.599032	35.852852
1303.051205	181140.428333	35.857869
1304.885461	181487.544761	35.862887
1306.282582	181849.051954	35.867904
1307.275662	182193.900612	35.872922
1309.128037	182516.703599	35.877940
1310.315170	182864.494637	35.882957
1311.671389	183231.196640	35.887975
1312.407086	183578.635453	35.892992
1313.854596	183928.091396	35.898010
1315.097344	184288.067307	35.903028
1316.368489	184642.786348	35.908045
1317.700644	185005.163956	35.913063
1318.640352	185375.757434	35.918080
1320.390756	185724.781804	35.923098
1321.677794	186103.611303	35.928116
1322.368506	186464.848090	35.933133
1323.656998	186819.819879	35.938151
1325.083237	187190.929426	35.943168
1326.265264	187562.107185	35.948186
1327.665286	187955.312195	35.953204
1328.932296	188320.743733	35.958221
1330.465324	188692.239269	35.963239
1331.473021	189082.229441	35.968256
1333.032408	189453.674914	35.973274
1334.616657	189800.493172	35.978292
1335.682315	190163.443936	35.983309
1337.471248	190528.651376	35.988327
1338.765443	190897.141646	35.993344
1339.793693	191228.459636	35.998362
1341.362725	191593.392789	36.003380
1342.372108	191949.153935	36.008397
1344.230575	192308.915408	36.013415
1345.348579	192692.133264	36.018432
1346.960802	193060.572046	36.023450
1348.422155	193409.310956	36.028468
1349.433390	193786.612540	36.033485
1350.895818	194140.915713	36.038503
1351.924774	194502.325318	36.043520
1353.342466	194866.288028	36.048538
1355.166371	195245.622700	36.053556
1356.211207	195610.743130	36.058573
1357.559861	195960.111983	36.063591
1358.913843	196342.844339	36.068608
1360.119179	196735.302606	36.073626
1361.621741	197098.312334	36.078644
1362.637829	197478.428717	36.083661
1364.351532	197873.158788	36.088679
1365.558362	198249.693622	36.093696
1366.918609	198624.910412	36.098714
1368.501413	199011.645573	36.103732
1369.629440	199418.732956	36.108749
1370.887428	199799.546776	36.113767
1372.353278	200189.240908	36.118784
1373.831146	200575.977227	36.123802
1375.156631	200982.863933	36.128820
1376.456909	201380.717735	36.133837
1377.819340	201760.674900	36.138855
1379.617633	202156.864072	36.143872
1381.225708	202541.177907	36.148890
1382.841190	202947.685730	36.153908
1384.163447	203347.350219	36.158925
1385.816862	203716.325923	36.163943
1387.422035	204103.543660	36.168960
1388.763778	204488.178808	36.173978
1390.594234	204871.897408	36.178996
1392.199925	205252.709528	36.184013
1393.622484	205618.876450	36.189031
1394.910762	206002.246157	36.194048
1396.245829	206365.130099	36.199066
1397.662138	206745.333740	36.204084
1398.875044	207139.057115	36.209101
1399.888032	207535.507338	36.214119
1401.068599	207907.020220	36.219136
1402.644317	208292.576299	36.224154
1403.912344	208687.682658	36.229172
1405.276089	209092.323645	36.234189
1406.847922	209471.626504	36.239207
1407.878047	209888.465402	36.244224
1409.168958	210284.782369	36.249242
1410.687361	210670.448597	36.254260
1412.128701	211063.278182	36.259277
1413.549547	211468.658406	36.264295
1414.928360	211862.683089	36.269312
1415.994016	212276.506483	36.274330
1418.082375	212679.446159	36.279348
1419.455573	213075.179090	36.284365
1420.896971	213469.112217	36.289383
1422.153401	213877.807476	36.294400
1423.180253	214263.152617	36.299418
1424.986175	214677.805336	36.304436
1426.213884	215103.272791	36.309453
1427.501229	215496.554941	36.314471
1429.057900	215865.515119	36.319488
1430.165082	216278.741522	36.324506
1431.732837	216677.214377	36.329524
1432.864028	217137.856909	36.334541
1434.273194	217528.207202	36.339559
1436.173379	217919.874972	36.344576
1437.319021	218318.856380	36.349594
1438.531882	218711.783780	36.354612
1440.317745	219106.624668	36.359629
1441.396959	219521.063864	36.364647
1442.881518	219908.897203	36.369664
1444.003134	220337.784267	36.374682
1445.722188	220740.592397	36.379700
1447.257608	221150.518552	36.384717
1448.769592	221562.456711	36.389735
1450.106302	221986.642085	36.394752
1451.330353	222408.384153	36.399770
1453.112967	222826.454567	36.404788
1454.100530	223241.457618	36.409805
1455.702380	223669.822279	36.414823
1457.839150	224082.784862	36.419840
1458.944840	224503.691256	36.424858
1460.933359	224929.431805	36.429876
1462.313971	225332.796048	36.434893
1463.797499	225760.299457	36.439911
1465.472576	226197.043637	36.444928
1466.785819	226619.142910	36.449946
1468.146695	227028.790084	36.454964
1469.635283	227467.220797	36.459981
1471.156865	227893.354216	36.464999
1472.863523	228310.975068	36.470016
1473.959710	228737.842053	36.475034
1475.531230	229183.224872	36.480052
1476.691302	229622.200151	36.485069
1478.374245	230052.505414	36.490087
1479.857353	230487.721943	36.495104
1480.981471	230940.550798	36.500122
1482.834560	231350.766010	36.505140
1484.133414	231805.194602	36.510157
1486.035425	232260.617409	36.515175
1487.707037	232688.774021	36.520192
1489.215138	233118.127358	36.525210
1491.457192	233547.665690	36.530228
1492.841145	233982.731890	36.535245
1494.263282	234406.565852	36.540263
1495.839742	234841.501212	36.545280
1497.232103	235272.505629	36.550298
1498.863244	235689.501202	36.555316
1500.226389	236135.067718	36.560333
1501.365990	236568.784551	36.565351
1503.027976	236993.043237	36.570368
1504.134821	237439.519291	36.575386
1505.872852	237903.902064	36.580404
1506.880063	238339.855305	36.585421
1508.473159	238777.846702	36.590439
1509.834133	239213.032493	36.595456
1511.343514	239678.397561	36.600474
1513.200323	240149.904525	36.605492
1514.477216	240590.238617	36.610509
1515.932260	241024.016018	36.615527
1517.679729	241465.011102	36.620544
1518.970336	241939.003632	36.625562
1520.439485	242398.818808	36.630580
1521.856293	242857.094095	36.635597
1523.238741	243305.646970	36.640615
1524.573496	243774.327244	36.645632
1525.854501	244234.507573	36.650650
1527.579471	244682.168387	36.655668
1529.214838	245157.203257	36.660685
1529.924684	245606.786057	36.665703
1531.857468	246042.729929	36.670720
1533.286118	246498.343107	36.675738
1534.724703	246951.034126	36.680756
1536.096771	247423.373125	36.685773
1537.501657	247880.237251	36.690791
1539.150748	248337.569851	36.695808
1540.717443	248816.051852	36.700826
1542.644381	249272.755733	36.705844
1543.746087	249761.680227	36.710861
1545.163164	250224.617042	36.715879
1547.780676	250680.751632	36.720896
1549.431751	251155.183965	36.725914
1551.055180	251613.998615	36.730932
1552.615846	252064.771394	36.735949
1553.894981	252549.504171	36.740967
1555.596098	253008.891804	36.745984
1556.701034	253485.220515	36.751002
1558.209329	253972.228653	36.756020
1559.821344	254449.312912	36.761037
1561.101392	254917.916897	36.766055
1562.923890	255395.145040	36.771072
1564.561150	255905.047218	36.776090
1566.393531	256384.992592	36.781108
1567.976706	256859.085844	36.786125
1569.490880	257354.529482	36.791143
1571.071626	257833.729725	36.796160
1572.226556	258309.875851	36.801178
1574.036422	258825.568630	36.806196
1575.760681	259330.047478	36.811213
1577.002327	259811.108065	36.816231
1578.596850	260318.758608	36.821248
1580.301788	260815.696238	36.826266
1581.713895	261310.929420	36.831284
1583.415565	261833.601237	36.836301
1584.599692	262342.412034	36.841319
1586.531181	262834.434919	36.846336
1587.908202	263343.188394	36.851354
1589.397259	263862.694288	36.856372
1591.324953	264383.550261	36.861389
1592.750742	264895.902570	36.866407
1594.776776	265400.763294	36.871424
1596.739563	265926.947567	36.876442
1598.377088	266420.618273	36.881460
1599.829027	266912.947553	36.886477
1601.372672	267429.927923	36.891495
1603.276151	267948.652184	36.896512
1604.684006	268453.181236	36.901530
1606.264269	268984.964416	36.906548
1608.236458	269482.642247	36.911565
1609.691596	269985.104501	36.916583
1611.568935	270486.505873	36.921600
1613.233800	271010.144035	36.926618
1614.832332	271507.347986	36.931636
1616.493530	272028.902479	36.936653
1617.650621	272553.867256	36.941671
1619.741062	273038.947153	36.946688
1621.422402	273537.023972	36.951706
1622.657813	274069.162665	36.956724
1624.152359	274569.859891	36.961741
1625.714722	275095.820899	36.966759
1627.096798	275619.880149	36.971776
1628.660100	276126.304521	36.976794
1630.195708	276655.747349	36.981812
1631.654152	277193.838770	36.986829
1633.177051	277721.325617	36.991847
1635.048682	278251.878351	36.996864
1636.779458	278739.954945	37.001882
1638.273153	279245.622709	37.006900
1640.214033	279758.074230	37.011917
1642.030395	280265.871130	37.016935
1643.779312	280749.241081	37.021952
1645.188389	281243.487333	37.026970
1646.572582	281769.082697	37.031988
1648.367347	282278.910533	37.037005
1649.381182	282781.473947	37.042023
1651.080053	283298.605333	37.047040
1652.768874	283824.678412	37.052058
1654.251830	284338.921356	37.057076
1655.677858	284868.565647	37.062093
1657.353581	285428.115630	37.067111
1659.127911	285939.181471	37.072128
1660.726975	286470.570430	37.077146
1662.110651	287008.038744	37.082164
1664.177769	287564.291058	37.087181
1665.702272	288128.708518	37.092199
1667.260132	288661.443288	37.097216
1668.582624	289222.283116	37.102234
1670.318518	289785.262511	37.107252
1672.278535	290332.047862	37.112269
1673.598885	290884.956627	37.117287
1675.362418	291472.233300	37.122304
1676.521822	292029.990186	37.127322
1678.371958	292613.513797	37.132340
1680.217187	293188.602769	37.137357
1681.725925	293798.441313	37.142375
1683.447569	294360.184985	37.147392
1685.070073	294924.736493	37.152410
1686.630784	295529.605083	37.157428
1688.479828	296111.283998	37.162445
1690.191117	296710.686280	37.167463
1691.664670	297300.218951	37.172480
1693.737933	297903.238279	37.177498
1695.049849	298499.852427	37.182516
1697.026454	299111.440728	37.187533
1698.765784	299703.304454	37.192551
1700.705624	300298.713075	37.197568
1702.352325	300899.703609	37.202586
1704.352475	301522.094049	37.207604
1706.205228	302113.036588	37.212621
1707.968514	302687.049896	37.217639
1709.615063	303295.188654	37.222656
1711.181156	303899.197089	37.227674
1712.836578	304494.196262	37.232692
1714.601757	305104.462928	37.237709
1716.204970	305722.930311	37.242727
1717.929473	306324.611451	37.247744
1719.740256	306933.334781	37.252762
1721.546555	307540.073809	37.257780
1723.293313	308161.624789	37.262797
1725.074844	308780.016491	37.267815
1726.525238	309375.474787	37.272832
1728.441866	309984.540548	37.277850
1730.027831	310614.887482	37.282868
1731.891300	311235.508118	37.287885
1733.415226	311858.059383	37.292903
1734.988765	312457.691115	37.297920
1737.007755	313087.769885	37.302938
1738.766886	313693.964497	37.307956
1740.673893	314310.414927	37.312973
1742.923634	314937.114124	37.317991
1744.987605	315550.709985	37.323008
1746.751892	316141.470207	37.328026
1748.006387	316764.026928	37.333044
1750.023781	317356.183256	37.338061
1751.737604	317931.777526	37.343079
1753.292466	318529.460275	37.348096
1755.057566	319119.764773	37.353114
1756.491285	319711.693412	37.358132
1758.371098	320283.407087	37.363149
1760.065045	320871.067837	37.368167
1761.924657	321479.974986	37.373184
1763.929739	322064.247835	37.378202
1765.533452	322655.437655	37.383220
1767.300978	323266.679998	37.388237
1768.527039	323851.319725	37.393255
1770.219435	324459.287959	37.398272
1771.823739	325073.257308	37.403290
1773.829291	325663.846010	37.408308
1775.983143	326283.679944	37.413325
1777.522767	326921.966223	37.418343
1779.209904	327514.748360	37.423360
1780.570591	328119.537230	37.428378
1782.620723	328750.027458	37.433396
1784.600609	329384.254963	37.438413
1786.378078	330023.815478	37.443431
1787.887321	330643.965742	37.448448
1789.752501	331267.732117	37.453466
1791.709812	331920.647558	37.458484
1793.691591	332539.557414	37.463501
1795.734013	333195.287895	37.468519
1797.464302	333833.113596	37.473536
1799.401303	334443.581690	37.478554
1801.139254	335107.768744	37.483572
1802.976517	335721.641157	37.488589
1804.717479	336369.159166	37.493607
1806.361818	337022.118008	37.498624
1808.348684	337647.393126	37.503642
1809.784326	338297.553207	37.508660
1811.596571	338961.274902	37.513677
1813.244956	339622.553005	37.518695
1814.920268	340270.085483	37.523712
1817.217184	340937.636779	37.528730
1818.696143	341603.283680	37.533748
1820.847945	342263.048943	37.538765
1823.226300	342914.975708	37.543783
1824.919321	343565.179534	37.548800
1826.944576	344206.740895	37.553818
1828.849220	344861.309373	37.558836
1830.675961	345532.329227	37.563853
1832.858705	346185.133562	37.568871
1834.418323	346835.214599	37.573888
1836.165420	347491.271088	37.578906
1837.634164	348167.643203	37.583924
1839.642675	348826.125366	37.588941
1841.141556	349488.336988	37.593959
1843.088474	350168.636698	37.598976
1844.980227	350831.373428	37.603994
1846.715042	351501.257773	37.609012
1848.833019	352178.606301	37.614029
1850.517595	352845.865129	37.619047
1852.483728	353505.581307	37.624064
1854.373667	354188.012518	37.629082
1856.204353	354880.948791	37.634100
1858.121291	355533.080622	37.639117
1859.847312	356229.032520	37.644135
1861.368404	356896.358386	37.649152
1863.463959	357575.556033	37.654170
1865.050286	358261.119701	37.659188
1866.777459	358957.255354	37.664205
1869.133640	359628.409600	37.669223
1870.756321	360339.865127	37.674240
1873.124741	360990.569949	37.679258
1874.691650	361639.366891	37.684276
1876.640777	362302.501746	37.689293
1878.694385	362965.633900	37.694311
1880.319165	363610.863131	37.699328
1882.358430	364275.422185	37.704346
1884.090950	364933.805019	37.709364
1885.559820	365586.689749	37.714381
1887.598575	366247.638585	37.719399
1889.077737	366934.418052	37.724416
1891.248587	367611.025328	37.729434
1893.062545	368290.292500	37.734452
1894.703685	368978.277221	37.739469
1896.604395	369645.633905	37.744487
1898.279444	370331.178602	37.749504
1900.414930	371023.432995	37.754522
1902.822854	371716.517409	37.759540
1905.021396	372384.384915	37.764557
1907.376401	373049.728751	37.769575
1909.336208	373740.363253	37.774592
1911.498608	374418.649741	37.779610
1913.108909	375105.080147	37.784628
1915.101804	375798.256976	37.789645
1917.000803	376482.026380	37.794663
1918.776707	377159.538522	37.799680
1920.630565	377839.535594	37.804698
1922.479329	378554.391668	37.809716
1924.350135	379238.796923	37.814733
1926.582717	379949.731586	37.819751
1928.155081	380658.351338	37.824768
1930.206664	381345.804153	37.829786
1931.904740	382076.613507	37.834804
1933.644900	382759.423137	37.839821
1935.598020	383480.067623	37.844839
1937.713024	384192.150020	37.849856
1940.060311	384899.868305	37.854874
1941.681066	385633.199077	37.859892
1943.568289	386336.854786	37.864909
1946.029925	387055.740115	37.869927
1947.610251	387788.953133	37.874944
1949.898628	388490.188841	37.879962
1951.260878	389219.171262	37.884980
1953.035202	389960.948036	37.889997
1955.175119	390690.909362	37.895015
1957.239151	391420.359306	37.900032
1958.909137	392167.627990	37.905050
1960.678568	392900.539700	37.910068
1962.483088	393629.169638	37.915085
1964.174774	394400.665595	37.920103
1966.093507	395144.804882	37.925120
1968.221071	395911.501468	37.930138
1970.183806	396688.572684	37.935156
1972.060127	397425.363156	37.940173
1974.228744	398187.052634	37.945191
1975.845930	398970.610157	37.950208
1978.052103	399725.436279	37.955226
1980.444173	400494.126006	37.960244
1982.356459	401255.449257	37.965261
1984.293974	402012.719062	37.970279
1986.610665	402787.290837	37.975296
1988.714492	403532.532220	37.980314
1990.603234	404306.170719	37.985332
1992.966649	405063.822092	37.990349
1995.268409	405815.838184	37.995367
1997.345620	406566.655041	38.000384
1999.295015	407339.693849	38.005402
2001.224980	408087.960455	38.010420
2003.178138	408842.283741	38.015437
2005.100623	409595.122046	38.020455
2006.918835	410327.030474	38.025472
2008.782198	411048.828928	38.030490
2010.419190	411786.985597	38.035508
2012.545960	412538.518348	38.040525
2014.379668	413267.659698	38.045543
2016.121928	414022.634192	38.050560
2017.804779	414768.731440	38.055578
2019.984010	415503.352767	38.060596
2021.701845	416267.462196	38.065613
2024.126075	417035.713410	38.070631
2025.704000	417804.385567	38.075648
2027.669784	418571.704718	38.080666
2029.595877	419350.024539	38.085684
2031.542206	420124.847945	38.090701
2033.483389	420904.612403	38.095719
2035.479486	421700.728463	38.100736
2037.451290	422485.605481	38.105754
2039.665898	423288.903269	38.110772
2041.437880	424086.424463	38.115789
2043.467503	424877.952721	38.120807
2045.493782	425693.889916	38.125824
2047.727048	426500.296813	38.130842
2049.854344	427313.733215	38.135860
2052.203237	428132.726503	38.140877
2054.515929	428928.103381	38.145895
2056.555337	429755.346229	38.150912
2058.405494	430574.693775	38.155930
2060.924486	431373.196376	38.160948
2062.932476	432189.931303	38.165965
2065.226815	433012.615258	38.170983
2067.088877	433847.795035	38.176000
2069.039447	434657.164722	38.181018
2070.958809	435471.168565	38.186036
2073.118677	436306.515394	38.191053
2075.441733	437122.875156	38.196071
2077.645238	437972.630692	38.201088
2079.660974	438808.417011	38.206106
2081.871453	439647.885823	38.211124
2084.094309	440457.361792	38.216141
2085.924844	441283.776002	38.221159
2088.139555	442138.080720	38.226176
2090.636656	442967.359465	38.231194
2093.031622	443786.200605	38.236212
2094.737453	444626.983832	38.241229
2097.077735	445468.895438	38.246247
2098.939079	446297.547478	38.251264
2101.126171	447152.726296	38.256282
2103.140545	448000.311507	38.261300
2105.051736	448836.751165	38.266317
2107.423872	449653.555958	38.271335
2109.424838	450512.174130	38.276352
2111.477452	451367.360363	38.281370
2113.848920	452217.907486	38.286388
2115.777089	453060.299903	38.291405
2117.996242	453907.263858	38.296423
2120.032252	454759.332002	38.301440
2121.979360	455612.189342	38.306458
2124.146036	456458.249735	38.311476
2126.153925	457320.787206	38.316493
2128.512140	458179.741858	38.321511
2130.350871	459027.116555	38.326528
2132.078888	459891.513955	38.331546
2134.242251	460783.257048	38.336564
2136.221073	461657.801791	38.341581
2138.012962	462512.218408	38.346599
2140.316601	463381.781542	38.351616
2142.033003	464287.194068	38.356634
2144.205821	465168.530075	38.361652
2146.171946	466024.941534	38.366669
2148.612161	466871.634272	38.371687
2150.246141	467742.936625	38.376704
2152.245394	468611.663580	38.381722
2154.633574	469484.482403	38.386740
2156.186961	470361.644695	38.391757
2158.280795	471221.143083	38.396775
2160.108200	472128.499949	38.401792
2162.088949	473032.150590	38.406810
2164.866290	473918.448244	38.411828
2166.794828	474816.515585	38.416845
2169.220838	475699.503983	38.421863
2171.270717	476617.068104	38.426880
2173.340508	477526.653027	38.431898
2175.817594	478435.772954	38.436916
2178.242128	479352.130833	38.441933
2180.428813	480265.502605	38.446951
2182.487258	481187.840510	38.451968
2184.240486	482121.747891	38.456986
2186.464997	483038.409921	38.462004
2188.430659	483970.622190	38.467021
2190.851491	484897.510399	38.472039
2193.532023	485840.264236	38.477056
2196.264087	486768.772184	38.482074
2198.892565	487700.328873	38.487092
2201.004995	488634.850174	38.492109
2203.008806	489587.362679	38.497127
2205.520894	490516.771509	38.502144
2207.465057	491430.425397	38.507162
2209.947918	492363.779587	38.512180
2211.771410	493321.570765	38.517197
2214.246999	494264.868325	38.522215
2216.396380	495187.224550	38.527232
2218.474873	496128.164412	38.532250
2220.901938	497078.936139	38.537268
2222.942011	498039.911443	38.542285
2225.156062	499004.890755	38.547303
2227.171763	499948.203633	38.552320
2229.806214	500905.840953	38.557338
2231.961914	501849.932426	38.562356
2233.812795	502815.106651	38.567373
2236.595416	503783.955394	38.572391
2239.084389	504731.763263	38.577408
2241.284836	505690.105432	38.582426
2244.088675	506658.580615	38.587444
2246.242335	507614.246324	38.592461
2248.241377	508576.739678	38.597479
2250.383542	509538.547458	38.602496
2252.676929	510496.542137	38.607514
2255.125377	511454.051086	38.612532
2257.187955	512442.319545	38.617549
2259.127373	513387.143091	38.622567
2261.387465	514365.782744	38.627584
2263.515758	515346.803332	38.632602
2266.065705	516322.955804	38.637620
2268.189029	517319.479400	38.642637
2270.453589	518310.776107	38.647655
2272.693301	519279.891710	38.652672
2275.394794	520236.978956	38.657690
2278.007856	521215.133677	38.662708
2280.154004	522210.635308	38.667725
2282.206686	523174.499765	38.672743
2284.738432	524154.748265	38.677760
2286.814228	525144.831891	38.682778
2288.991290	526117.758901	38.687796
2291.080506	527092.803749	38.692813
2293.132340	528088.894232	38.697831
2295.565278	529075.388182	38.702848
2297.754742	530024.039118	38.707866
2299.892758	530987.240925	38.712884
2301.961183	531955.124809	38.717901
2304.408370	532910.850008	38.722919
2306.219512	533898.385351	38.727936
2308.139593	534867.009023	38.732954
2310.147295	535827.600926	38.737972
2312.697729	536824.683352	38.742989
2314.844496	537825.589108	38.748007
2316.827200	538821.571065	38.753024
2318.921116	539837.343788	38.758042
2321.066499	540858.722446	38.763060
2323.331322	541874.826021	38.768077
2325.781261	542891.027992	38.773095
2328.070590	543921.974706	38.778112
2330.445080	544982.210700	38.783130
2333.032238	546000.984020	38.788148
2335.033477	547036.579641	38.793165
2337.485672	548098.177330	38.798183
2340.077438	549138.348090	38.803200
2342.086655	550194.477890	38.808218
2344.453957	551263.139330	38.813236
2346.805233	552318.145308	38.818253
2348.886178	553374.321430	38.823271
2351.317877	554463.788449	38.828288
2353.680249	555552.425818	38.833306
2356.343378	556614.990632	38.838324
2358.349489	557709.444494	38.843341
2360.984771	558799.484330	38.848359
2363.104603	559890.324630	38.853376
2365.499510	560989.572519	38.858394
2368.078725	562097.190274	38.863412
2370.095803	563192.751048	38.868429
2372.922593	564307.528113	38.873447
2375.504209	565423.004640	38.878464
2377.794000	566522.563123	38.883482
2380.446937	567610.468504	38.888500
2382.747733	568749.160679	38.893517
2385.050739	569867.265740	38.898535
2387.918696	570968.511702	38.903552
2390.570032	572058.302782	38.908570
2393.547899	573156.631934	38.913588
2395.501039	574283.847709	38.918605
2397.961832	575385.433123	38.923623
2400.815807	576473.709071	38.928640
2402.846447	577608.294992	38.933658
2405.665145	578698.743180	38.938676
2408.061364	579811.443125	38.943693
2410.379220	580913.822394	38.948711
2412.956933	582019.171351	38.953728
2416.210533	583129.727594	38.958746
2418.869556	584215.154088	38.963764
2421.642624	585287.276298	38.968781
2423.848076	586375.244713	38.973799
2426.323538	587472.999914	38.978816
2428.561409	588556.656764	38.983834
2431.035639	589639.927204	38.988852
2433.919040	590726.090985	38.993869
2436.035149	591813.035190	38.998887
2438.433466	592879.987081	39.003904
2440.406366	593992.418527	39.008922
2442.854250	595086.377583	39.013940
2444.985827	596175.077045	39.018957
2447.090633	597252.608436	39.023975
2450.074595	598365.214628	39.028992
2453.773910	599438.726276	39.034010
2456.197379	600506.489637	39.039028
2458.579417	601596.799611	39.044045
2460.695880	602626.456648	39.049063
2463.322085	603672.813137	39.054080
2464.961320	604733.657560	39.059098
2467.121603	605800.226071	39.064116
2469.230945	606840.923083	39.069133
2471.444408	607907.336911	39.074151
2473.742514	608970.383840	39.079168
2475.703259	610065.466445	39.084186
2478.151003	611179.728836	39.089204
2480.327082	612271.810192	39.094221
2482.487544	613351.680649	39.099239
2484.895612	614476.580154	39.104256
2486.967132	615612.176543	39.109274
2489.604128	616734.409796	39.114292
2491.919519	617857.482873	39.119309
2494.586789	619020.638723	39.124327
2497.352432	620184.605713	39.129344
2499.445586	621342.510885	39.134362
2501.506443	622473.154443	39.139380
2504.194765	623647.664043	39.144397
2506.638989	624836.531072	39.149415
2509.294569	626020.835202	39.154432
2511.866021	627197.328253	39.159450
2514.387829	628380.146115	39.164468
2516.856587	629578.329046	39.169485
2519.106707	630784.156220	39.174503
2522.003261	631996.982501	39.179520
2524.194095	633219.924370	39.184538
2526.845932	634403.400432	39.189556
2529.097167	635632.144964	39.194573
2531.295050	636865.846684	39.199591
2534.058354	638101.755714	39.204608
2536.366645	639323.318733	39.209626
2539.377056	640561.240834	39.214644
2542.268657	641795.791074	39.219661
2544.834081	643034.388496	39.224679
2547.373399	644269.548475	39.229696
2549.930658	645524.908066	39.234714
2552.655657	646773.053301	39.239732
2555.455002	648031.754930	39.244749
2558.000517	649279.920845	39.249767
2560.780742	650523.406784	39.254784
2562.959850	651767.585960	39.259802
2565.685188	653017.801157	39.264820
2568.420049	654292.079558	39.269837
2570.585487	655549.595327	39.274855
2573.198911	656805.233746	39.279872
2575.841845	658093.040210	39.284890
2578.261475	659350.728357	39.289908
2581.109067	660616.353091	39.294925
2583.603781	661895.567149	39.299943
2585.773650	663179.895240	39.304960
2588.235717	664467.590097	39.309978
2590.840329	665765.245285	39.314996
2593.118307	667048.992822	39.320013
2595.450921	668350.326522	39.325031
2598.084218	669658.251013	39.330048
2600.553319	670962.292042	39.335066
2602.693555	672282.176939	39.340084
2605.710842	673591.885377	39.345101
2608.459664	674901.605750	39.350119
2610.775734	676224.143750	39.355136
2613.371554	677564.297921	39.360154
2615.808410	678881.270273	39.365172
2618.950261	680196.747434	39.370189
2621.277677	681529.019579	39.375207
2624.158510	682870.399989	39.380224
2626.841230	684193.782083	39.385242
2629.472356	685498.850746	39.390260
2632.470842	686767.464905	39.395277
2634.681108	688050.633030	39.400295
2637.735897	689345.000734	39.405312
2640.383905	690621.477063	39.410330
2642.982419	691894.107882	39.415348
2645.727548	693195.421097	39.420365
2648.376074	694481.773136	39.425383
2650.995396	695760.601496	39.430400
2653.631022	697062.313110	39.435418
2656.072096	698372.646077	39.440436
2658.875707	699663.481939	39.445453
2661.331638	700964.451417	39.450471
2663.742586	702282.440988	39.455488
2666.401591	703606.091015	39.460506
2669.043934	704912.938385	39.465524
2672.109364	706233.099358	39.470541
2674.479964	707574.977026	39.475559
2677.038977	708910.620747	39.480576
2679.533407	710224.569384	39.485594
2682.134227	711591.890070	39.490612
2685.347616	712927.049580	39.495629
2687.716589	714295.511436	39.500647
2690.732499	715641.369275	39.505664
2693.314308	716978.720026	39.510682
2695.997920	718367.014630	39.515700
2698.779122	719744.228006	39.520717
2700.950623	721096.826739	39.525735
2703.639754	722460.350195	39.530752
2706.221526	723859.030224	39.535770
2708.400556	725277.320713	39.540788
2711.584317	726662.226279	39.545805
2713.953908	728062.110407	39.550823
2716.954558	729486.808841	39.555840
2719.351186	730925.047113	39.560858
2721.461530	732334.325198	39.565876
2724.501067	733757.827928	39.570893
2726.725970	735208.082616	39.575911
2729.262562	736660.346753	39.580928
2731.986948	738113.108197	39.585946
2734.491294	739582.475479	39.590964
2737.861391	741045.902839	39.595981
2740.252717	742524.864848	39.600999
2743.196356	743984.170916	39.606016
2746.266163	745461.980216	39.611034
2748.943602	746948.898165	39.616052
2751.827975	748419.525576	39.621069
2754.567494	749889.802320	39.626087
2757.409365	751369.741624	39.631104
2760.667656	752859.728699	39.636122
2763.293786	754355.347465	39.641140
2766.435006	755792.958130	39.646157
2769.091984	757282.930584	39.651175
2772.324187	758776.458340	39.656192
2774.935922	760241.439592	39.661210
2777.668377	761710.008008	39.666228
2780.965496	763181.152290	39.671245
2783.363688	764676.366587	39.676263
2785.919621	766148.925146	39.681280
2789.272783	767620.375485	39.686298
2791.615887	769110.930276	39.691316
2794.728174	770563.893140	39.696333
2797.239929	772072.166429	39.701351
2799.783959	773558.406222	39.706368
2802.513521	775036.700985	39.711386
2804.991068	776526.678019	39.716404
2807.757459	778018.662764	39.721421
2810.548766	779521.682451	39.726439
2813.431935	780984.611106	39.731456
2816.557275	782416.135056	39.736474
2819.347234	783867.503202	39.741492
2822.046733	785331.253489	39.746509
2824.625465	786805.910709	39.751527
2827.435434	788256.489234	39.756544
2830.169928	789710.856031	39.761562
2832.760743	791189.903577	39.766580
2835.621090	792634.582865	39.771597
2838.395162	794108.335618	39.776615
2840.943449	795610.577680	39.781632
2844.296948	797103.647429	39.786650
2846.858635	798582.719464	39.791668
2849.445749	800063.775806	39.796685
2852.437674	801588.116352	39.801703
2855.619843	803099.611040	39.806720
2858.285852	804591.141704	39.811738
2860.517505	806099.250290	39.816756
2863.642585	807621.309443	39.821773
2866.290649	809168.096507	39.826791
2868.876566	810710.779449	39.831808
2872.101558	812254.865036	39.836826
2874.882353	813813.527614	39.841844
2877.903843	815358.258996	39.846861
2880.782693	816891.475071	39.851879
2884.025060	818456.998614	39.856896
2886.870127	820004.793029	39.861914
2889.731723	821573.604128	39.866932
2892.956132	823135.885982	39.871949
2895.866379	824722.634629	39.876967
2898.634833	826292.003727	39.881984
2901.741932	827852.848680	39.887002
2904.715218	829482.618931	39.892020
2907.787333	831071.563123	39.897037
2910.725929	832633.829905	39.902055
2913.663417	834205.366939	39.907072
2916.269919	835803.071664	39.912090
2918.841909	837415.334810	39.917108
2921.870402	838997.424998	39.922125
2924.683521	840597.264366	39.927143
2927.535101	842212.509637	39.932160
2930.612843	843809.018833	39.937178
2933.260276	845426.886318	39.942196
2936.359494	847054.767066	39.947213
2938.996993	848687.261390	39.952231
2941.824969	850316.773630	39.957248
2944.991431	851939.782462	39.962266
2947.835591	853600.887036	39.967284
2950.672649	855228.533110	39.972301
2953.547940	856884.287578	39.977319
2956.084969	858533.733878	39.982336
2959.242407	860186.323406	39.987354
2962.247121	861857.990732	39.992372
2965.150158	863531.642446	39.997389
2967.783388	865187.816123	40.002407
2970.701653	866870.145246	40.007424
2974.164624	868545.522148	40.012442
2976.661460	870231.636142	40.017460
2979.975597	871903.585016	40.022477
2982.404215	873575.503854	40.027495
2985.784686	875259.961072	40.032512
2988.884174	876954.728304	40.037530
2992.069586	878636.905772	40.042548
2995.026706	880343.108522	40.047565
2998.326479	882018.984475	40.052583
3000.783731	883693.361226	40.057600
3004.333747	885371.523605	40.062618
3006.840856	887076.034775	40.067636
3009.821824	888724.153526	40.072653
3012.729629	890364.961371	40.077671
3015.870841	892013.950609	40.082688
3018.663781	893635.027170	40.087706
3021.722090	895296.788704	40.092724
3024.885092	896935.582542	40.097741
3027.071019	898580.525057	40.102759
3029.992734	900271.995948	40.107776
3032.948103	901931.452086	40.112794
3035.559543	903614.844590	40.117812
3038.531534	905304.125166	40.122829
3041.485711	907000.696532	40.127847
3043.957996	908704.626657	40.132864
3046.943897	910415.454363	40.137882
3049.894963	912156.437890	40.142900
3053.056979	913907.221582	40.147917
3056.046497	915653.921865	40.152935
3058.711280	917409.055440	40.157952
3061.962992	919156.326533	40.162970
3064.903752	920922.676199	40.167988
3068.006269	922695.048365	40.173005
3071.098194	924481.331249	40.178023
3073.901849	926279.923984	40.183040
3077.010135	928058.592459	40.188058
3080.258433	929847.000411	40.193076
3083.457210	931650.437241	40.198093
3086.916624	933470.750089	40.203111
3090.006583	935263.783512	40.208128
3093.619787	937068.280022	40.213146
3096.525251	938899.547419	40.218164
3099.774508	940691.952425	40.223181
3102.996392	942501.917088	40.228199
3106.072172	944311.947078	40.233216
3109.378651	946135.164933	40.238234
3112.575289	947964.637089	40.243252
3115.695575	949779.531977	40.248269
3118.483288	951619.423962	40.253287
3121.253866	953443.772729	40.258304
3124.522528	955273.302230	40.263322
3127.727759	957153.883648	40.268340
3130.576128	959052.324355	40.273357
3133.468104	960964.506899	40.278375
3136.203674	962868.554807	40.283392
3139.437117	964784.691996	40.288410
3142.052068	966710.745135	40.293428
3145.336184	968625.204240	40.298445
3148.643833	970581.581863	40.303463
3151.585551	972544.769356	40.308480
3154.819535	974480.020955	40.313498
3157.858998	976418.356738	40.318516
3160.910815	978380.404935	40.323533
3164.350409	980348.440348	40.328551
3167.558329	982304.925836	40.333568
3170.342161	984263.537607	40.338586
3173.552644	986220.335978	40.343604
3176.929710	988204.364494	40.348621
3180.606479	990158.079148	40.353639
3183.642515	992141.180664	40.358656
3187.075443	994102.235353	40.363674
3190.384899	996055.636318	40.368692
3193.662582	998029.353708	40.373709
3197.208382	999990.394986	40.378727
3200.023209	1001948.547824	40.383744
3203.030334	1003933.067094	40.388762
3205.841329	1005893.057422	40.393780
3209.084758	1007876.152949	40.398797
3212.511857	1009850.572049	40.403815
3215.479064	1011826.507513	40.408832
3218.794254	1013737.463903	40.413850
3222.218375	1015675.547522	40.418868
3225.041696	1017611.513146	40.423885
3228.130371	1019526.348126	40.428903
3231.030273	1021446.462339	40.433920
3234.552978	1023365.333007	40.438938
3237.662979	1025323.155342	40.443956
3240.589159	1027248.141071	40.448973
3244.685130	1029199.901996	40.453991
3247.857611	1031140.992717	40.459008
3251.350859	1033065.619225	40.464026
3254.298156	1035030.494850	40.469044
3257.397017	1036984.619329	40.474061
3260.829020	1038930.577078	40.479079
3263.428543	1040906.166566	40.484096
3266.864588	1042886.023734	40.489114
3269.671664	1044880.114501	40.494132
3272.836827	1046876.125928	40.499149
3276.138126	1048858.110908	40.504167
3278.839976	1050878.556055	40.509184
3282.400998	1052896.774912	40.514202
3285.380033	1054919.160629	40.519220
3288.447778	1056961.939007	40.524237
3291.937650	1059011.290328	40.529255
3294.823019	1061053.927404	40.534272
3298.240126	1063101.192116	40.539290
3301.582216	1065181.205588	40.544308
3305.001418	1067273.179880	40.549325
3308.629716	1069332.479744	40.554343
3311.704274	1071409.984789	40.559360
3315.301931	1073494.570362	40.564378
3318.701248	1075598.800283	40.569396
3321.873741	1077666.154043	40.574413
3325.340458	1079753.928626	40.579431
3328.425773	1081865.751341	40.584448
3332.017172	1083947.019354	40.589466
3335.265010	1086064.361479	40.594484
3338.263692	1088202.712856	40.599501
3342.185406	1090310.070157	40.604519
3345.181291	1092421.059536	40.609536
3348.109221	1094546.227003	40.614554
3351.461721	1096681.370057	40.619572
3355.046568	1098815.155460	40.624589
3358.244907	1100960.749255	40.629607
3361.019128	1103109.945110	40.634624
3364.646191	1105262.050857	40.639642
3368.710486	1107423.320764	40.644660
3371.077184	1109575.339051	40.649677
3374.913506	1111722.067016	40.654695
3377.499842	1113914.279579	40.659712
3380.943327	1116093.569645	40.664730
3384.060719	1118280.011673	40.669748
3387.685225	1120468.517903	40.674765
3390.916563	1122659.897465	40.679783
3394.310720	1124861.838451	40.684800
3397.580558	1127065.928254	40.689818
3401.002608	1129245.178834	40.694836
3403.997474	1131469.972736	40.699853
3407.596985	1133697.433160	40.704871
3410.741856	1135924.035025	40.709888
3413.620359	1138120.296759	40.714906
3417.486603	1140349.562744	40.719924
3420.416757	1142600.847326	40.724941
3424.066737	1144827.695570	40.729959
3427.295027	1147073.433250	40.734976
3430.370380	1149318.997089	40.739994
3433.634113	1151565.463129	40.745012
3436.973146	1153806.753824	40.750016
3440.528358	1155990.104646	40.755021
3443.799923	1158114.524275	40.760026
3446.401167	1160182.510188	40.765031
3450.127687	1162174.458633	40.770036
3453.300321	1164102.823843	40.775040
3456.166402	1165945.441589	40.780045
3459.168842	1167701.195808	40.785050
3461.984536	1169402.408544	40.790055
3465.045374	1170998.680508	40.795060
3467.522979	1172508.353111	40.800064
3470.124760	1173960.709822	40.805069
3472.758593	1175336.488378	40.810074
3474.959254	1176648.925677	40.815079
3477.794321	1177860.204760	40.820084
3479.702712	1179009.275822	40.825088
3482.324183	1180086.397575	40.830093
3484.633789	1181095.455703	40.835098
3486.536915	1182037.917547	40.840103
3488.826607	1182883.096135	40.845108
3490.405701	1183703.030857	40.850112
3492.613004	1184459.025350	40.855117
3494.368409	1185159.659372	40.860122
3495.786505	1185776.430724	40.865127
3497.333173	1186348.801455	40.870132
3498.408783	1186893.157135	40.875136
3500.017859	1187364.479591	40.880141
3501.256673	1187810.993115	40.885146
3502.757276	1188216.238090	40.890151
3503.942639	1188551.546659	40.895156
3504.719589	1188865.557659	40.900160
3505.983329	1189143.272807	40.905165
3507.114414	1189389.876656	40.910170
3508.099986	1189567.960024	40.915175
3509.186180	1189734.175842	40.920180
3509.831928	1189880.530014	40.925184
3510.794741	1189970.520664	40.930189
3511.375409	1190052.676603	40.935194
3511.916575	1190085.487790	40.940199
3512.764602	1190121.538223	40.945204
3513.365327	1190163.833062	40.950208
3514.015974	1190114.470324	40.955213
3514.674945	1190065.575749	40.960218
3514.839174	1190023.154294	40.965223
3515.836698	1189949.104413	40.970228
3516.359499	1189848.904428	40.975232
3516.732831	1189721.465175	40.980237
3517.243121	1189584.317266	40.985242
3517.628908	1189428.853867	40.990247
3518.147927	1189255.594973	40.995252
3518.274936	1189093.018926	41.000256
3518.955313	1188901.199946	41.005261
3519.252548	1188701.068696	41.010266
3519.574908	1188466.792882	41.015271
3520.132961	1188241.588941	41.020276
3520.070900	1188018.264051	41.025280
3520.625531	1187754.107634	41.030285
3520.602587	1187472.822142	41.035290
3520.725301	1187203.630189	41.040295
3521.522318	1186925.001483	41.045300
3521.529724	1186667.369738	41.050304
3521.599189	1186351.675220	41.055309
3521.926631	1186033.849349	41.060314
3522.032034	1185732.034077	41.065319
3522.447587	1185426.198579	41.070324
3522.488238	1185092.367727	41.075328
3523.020605	1184746.860438	41.080333
3522.941857	1184417.710664	41.085338
3523.019393	1184090.114111	41.090343
3523.481985	1183717.257969	41.095348
3523.446930	1183358.198890	41.100352
3523.381493	1182999.402345	41.105357
3523.688433	1182653.133804	41.110362
3523.649748	1182277.997536	41.115367
3523.982692	1181899.195289	41.120372
3523.847301	1181517.900326	41.125376
3524.154011	1181139.611919	41.130381
3524.126768	1180765.776928	41.135386
3524.151118	1180357.908774	41.140391
3524.694040	1179950.959222	41.145396
3524.116382	1179567.239261	41.150400
3524.589493	1179169.941743	41.155405
3524.737836	1178777.566045	41.160410
3524.598148	1178381.533875	41.165415
3524.697978	1177955.752736	41.170420
3524.844344	1177547.738170	41.175424
3524.940033	1177147.521469	41.180429
3524.447937	1176722.773477	41.185434
3524.649717	1176323.324099	41.190439
3524.987623	1175888.286550	41.195444
3524.777429	1175470.270732	41.200448
3524.918070	1175051.315116	41.205453
3525.092308	1174652.402005	41.210458
3525.171695	1174204.632830	41.215463
3525.096921	1173768.449018	41.220468
3524.782729	1173340.944100	41.225472
3525.015840	1172908.409769	41.230477
3525.019231	1172476.726270	41.235482
3524.906862	1172053.043926	41.240487
3525.077466	1171638.714049	41.245492
3525.206840	1171205.772603	41.250496
3525.328899	1170749.586190	41.255501
3525.002067	1170314.758945	41.260506
3525.049613	1169893.988785	41.265511
3525.097991	1169462.803443	41.270516
3524.890870	1169011.049288	41.275520
3524.948788	1168557.890946	41.280525
3525.041081	1168139.615021	41.285530
3524.999901	1167717.929002	41.290535
3525.256533	1167254.334689	41.295540
3524.985881	1166806.649047	41.300544
3525.076198	1166362.926122	41.305549
3524.895726	1165921.476667	41.310554
3525.022318	1165485.889486	41.315559
3524.942502	1165038.398855	41.320564
3524.842291	1164605.137075	41.325568
3525.270978	1164161.360666	41.330573
3524.604184	1163713.003178	41.335578
3524.888261	1163262.749947	41.340583
3524.950596	1162831.676819	41.345588
3524.899278	1162386.128188	41.350592
3524.974734	1161910.655601	41.355597
3525.346455	1161461.650863	41.360602
3525.001684	1161034.088647	41.365607
3525.012376	1160583.839373	41.370612
3525.007744	1160133.270351	41.375616
3525.103135	1159660.615841	41.380621
3525.002932	1159232.582851	41.385626
3524.680935	1158783.274009	41.390631
3524.619744	1158332.748857	41.395636
3524.657763	1157892.099918	41.400640
3524.826400	1157428.123132	41.405645
3524.629521	1156977.882483	41.410650
3524.599620	1156517.547363	41.415655
3524.744879	1156093.570048	41.420660
3524.088488	1155648.778886	41.425664
3524.591403	1155179.817418	41.430669
3524.410010	1154725.406755	41.435674
3524.714607	1154302.583773	41.440679
3524.790753	1153849.285450	41.445684
3524.666451	1153400.240964	41.450688
3524.340721	1152940.588104	41.455693
3524.398520	1152503.649813	41.460698
3524.349215	1152049.838494	41.465703
3524.466250	1151592.456931	41.470708
3524.011664	1151161.646953	41.475712
3523.913646	1150710.379991	41.480717
3524.250223	1150255.119297	41.485722
3524.159122	1149804.815606	41.490727
3524.223472	1149368.089874	41.495732
3523.923730	1148900.785574	41.500736
3523.885225	1148454.810954	41.505741
3524.017519	1148025.637854	41.510746
3523.713675	1147592.995276	41.515751
3523.960392	1147130.372131	41.520756
3523.666341	1146678.318596	41.525760
3523.929715	1146235.898178	41.530765
3523.772679	1145815.219161	41.535770
3523.798838	1145365.749761	41.540775
3523.986623	1144902.846451	41.545780
3523.901502	1144461.472676	41.550784
3523.529464	1144018.402331	41.555789
3523.887564	1143584.468925	41.560794
3523.477753	1143126.060805	41.565799
3523.961076	1142674.674942	41.570804
3523.569286	1142246.826129	41.575808
3523.984574	1141785.414937	41.580813
3524.281428	1141338.689484	41.585818
3523.714696	1140891.499249	41.590823
3523.956199	1140436.451546	41.595828
3523.823280	1139991.011764	41.600832
3523.917144	1139542.270171	41.605837
3523.624413	1139082.353648	41.610842
3523.774708	1138639.316473	41.615847
3523.975062	1138184.177111	41.620852
3523.850362	1137731.520792	41.625856
3523.767702	1137275.970339	41.630861
3523.882288	1136843.233837	41.635866
3523.506683	1136387.940276	41.640871
3523.685536	1135912.096275	41.645876
3523.595657	1135486.121175	41.650880
3523.708566	1135029.775824	41.655885
3523.582345	1134594.140869	41.660890
3523.295324	1134131.799193	41.665895
3523.507355	1133680.547132	41.670900
3523.358688	1133249.176400	41.675904
3523.220875	1132803.323910	41.680909
3523.419045	1132352.151456	41.685914
3523.240127	1131912.028505	41.690919
3523.454213	1131464.199882	41.695924
3523.344327	1131013.630053	41.700928
3523.370739	1130555.298726	41.705933
3522.979892	1130106.124442	41.710938
3522.776891	1129666.865657	41.715943
3523.104387	1129226.342111	41.720948
3522.935118	1128800.700248	41.725952
3522.987019	1128335.135922	41.730957
3522.759595	1127892.025416	41.735962
3522.955309	1127447.191201	41.740967
3522.857482	1127007.125037	41.745972
3522.677828	1126583.495945	41.750976
3522.801535	1126142.180203	41.755981
3522.848309	1125687.327949	41.760986
3522.763926	1125257.297302	41.765991
3523.070167	1124817.269447	41.770996
3522.838282	1124371.773327	41.776000
3522.777659	1123915.550399	41.781005
3522.622150	1123484.436748	41.786010
3522.455370	1123059.288181	41.791015
3522.250434	1122606.309431	41.796020
3522.433425	1122173.891704	41.801024
3522.363978	1121733.005086	41.806029
3522.214145	1121301.142966	41.811034
3522.204294	1120867.698981	41.816039
3522.341139	1120430.671334	41.821044
3522.275766	1119994.403384	41.826048
3522.132767	1119556.111998	41.831053
3522.238258	1119106.120003	41.836058
3522.007206	1118692.067966	41.841063
3521.952303	1118256.609487	41.846068
3522.029352	1117846.443592	41.851072
3521.989937	1117392.424174	41.856077
3521.941991	1116953.618166	41.861082
3521.798608	1116538.146071	41.866087
3522.220027	1116121.690779	41.871092
3521.635141	1115686.110654	41.876096
3521.871050	1115262.754874	41.881101
3521.676011	1114821.605624	41.886106
3521.457254	1114387.957520	41.891111
3521.976764	1113971.605219	41.896116
3521.686769	1113543.908843	41.901120
3521.843919	1113097.695680	41.906125
3521.553603	1112696.639277	41.911130
3521.421157	1112266.239601	41.916135
3521.597931	1111819.058376	41.921140
3521.151150	1111401.425645	41.926144
3520.730427	1110997.592243	41.931149
3520.954056	1110576.826949	41.936154
3520.914225	1110167.906184	41.941159
3520.921892	1109745.202658	41.946164
3520.873698	1109335.551869	41.951168
3520.796004	1108925.492906	41.956173
3521.201607	1108490.502069	41.961178
3520.795095	1108077.568666	41.966183
3521.217755	1107666.090180	41.971188
3520.999685	1107252.012121	41.976192
3520.802860	1106824.051919	41.981197
3520.583650	1106408.763252	41.986202
3520.523350	1105997.523317	41.991207
3520.635752	1105601.792829	41.996212
3520.461353	1105182.677100	42.001216
3520.714075	1104763.267368	42.006221
3520.877444	1104355.686577	42.011226
3520.362562	1103957.263565	42.016231
3520.742614	1103531.239902	42.021236
3520.311417	1103118.790312	42.026240
3520.381619	1102695.809658	42.031245
3520.468669	1102295.348938	42.036250
3520.387336	1101900.621190	42.041255
3520.395972	1101490.842192	42.046260
3520.060261	1101079.176865	42.051264
3520.065686	1100664.460232	42.056269
3520.267654	1100271.287590	42.061274
3519.857556	1099864.800566	42.066279
3519.876435	1099468.922373	42.071284
3519.936538	1099061.245580	42.076288
3519.769939	1098653.862299	42.081293
3519.873560	1098256.733697	42.086298
3519.893372	1097877.094387	42.091303
3520.064480	1097455.504099	42.096308
3519.926662	1097061.388653	42.101312
3520.028872	1096666.726592	42.106317
3519.825276	1096263.761770	42.111322
3519.625889	1095860.957630	42.116327
3519.894026	1095453.165997	42.121332
3519.672186	1095082.748684	42.126336
3519.511244	1094669.417924	42.131341
3519.888337	1094278.269184	42.136346
3519.491049	1093866.447560	42.141351
3519.586290	1093483.328721	42.146356
3519.563714	1093085.554259	42.151360
3519.285139	1092670.367084	42.156365
3519.683540	1092291.709899	42.161370
3519.280493	1091899.081679	42.166375
3519.270221	1091498.028674	42.171380
3519.454548	1091114.919353	42.176384
3519.237907	1090716.045317	42.181389
3519.562924	1090312.933903	42.186394
3519.217386	1089941.036090	42.191399
3519.167129	1089531.606071	42.196404
3519.271892	1089143.868093	42.201408
3519.337252	1088759.941515	42.206413
3519.372378	1088358.744896	42.211418
3518.895551	1087957.315482	42.216423
3519.127932	1087565.131515	42.221428
3519.070411	1087182.072048	42.226432
3519.362101	1086780.429138	42.231437
3519.015730	1086389.214163	42.236442
3518.703099	1086019.438836	42.241447
3519.057616	1085627.190848	42.246452
3518.672700	1085244.048781	42.251456
3518.579573	1084857.092219	42.256461
3518.606074	1084479.102123	42.261466
3518.321044	1084100.849396	42.266471
3518.505604	1083725.561957	42.271476
3518.299950	1083355.492064	42.276480
3518.541302	1082959.521817	42.281485
3518.445830	1082585.928482	42.286490
3518.347305	1082213.365263	42.291495
3518.578142	1081827.770871	42.296500
3518.332000	1081453.357209	42.301504
3518.384509	1081075.510390	42.306509
3518.445966	1080694.565298	42.311514
3518.354923	1080306.421449	42.316519
3517.762657	1079922.075370	42.321524
3518.009114	1079578.834074	42.326528
3518.050740	1079207.673966	42.331533
3517.980920	1078815.485241	42.336538
3518.263080	1078441.353716	42.341543
3518.354170	1078081.532451	42.346548
3518.382269	1077705.376288	42.351552
3518.340425	1077312.306904	42.356557
3518.029634	1076933.560958	42.361562
3517.711732	1076575.724324	42.366567
3518.013409	1076203.068760	42.371572
3517.931282	1075827.569734	42.376576
3517.742531	1075459.362185	42.381581
3517.858597	1075094.057346	42.386586
3517.836282	1074726.637538	42.391591
3517.611584	1074368.448910	42.396596
3517.836529	1074010.739215	42.401600
3517.627085	1073632.708568	42.406605
3517.878237	1073261.109890	42.411610
3517.792810	1072892.904706	42.416615
3517.713251	1072531.496906	42.421620
3517.700772	1072166.498255	42.426624
3517.656814	1071793.310845	42.431629
3517.722626	1071417.869172	42.436634
3517.377245	1071049.390582	42.441639
3517.474688	1070686.486097	42.446644
3517.209514	1070335.057826	42.451648
3517.010873	1069989.364748	42.456653
3517.504283	1069608.248401	42.461658
3516.801825	1069242.207022	42.466663
3517.476822	1068892.839233	42.471668
3517.064265	1068530.068305	42.476672
3517.238433	1068182.949714	42.481677
3517.130672	1067821.139641	42.486682
3516.968321	1067468.837421	42.491687
3517.160534	1067132.614954	42.496692
3517.029408	1066771.893891	42.501696
3516.702202	1066400.406161	42.506701
3517.084175	1066049.558729	42.511706
3516.657398	1065686.121031	42.516711
3517.047495	1065337.343619	42.521716
3516.978740	1064994.874750	42.526720
3517.161582	1064633.961541	42.531725
3517.290196	1064282.658055	42.536730
3517.055921	1063919.071745	42.541735
3517.104223	1063547.617977	42.546740
3517.136506	1063186.056956	42.551744
3516.820730	1062830.594517	42.556749
3517.085123	1062489.262447	42.561754
3516.722447	1062116.624394	42.566759
3516.975024	1061769.665229	42.571764
3516.731896	1061422.765833	42.576768
3516.736841	1061068.966339	42.581773
3516.804099	1060740.366288	42.586778
3516.665575	1060384.331368	42.591783
3516.715895	1060009.171075	42.596788
3516.270855	1059655.451179	42.601792
3516.543131	1059312.957583	42.606797
3516.938971	1058965.605460	42.611802
3516.500952	1058614.322336	42.616807
3516.591720	1058276.900476	42.621812
3516.361187	1057933.151393	42.626816
3516.500076	1057587.200068	42.631821
3516.380845	1057227.103438	42.636826
3516.295283	1056880.373791	42.641831
3516.613020	1056539.917025	42.646836
3516.281732	1056190.003905	42.651840
3516.346440	1055835.858490	42.656845
3516.386229	1055508.686032	42.661850
3516.284562	1055161.851033	42.666855
3516.339271	1054810.437196	42.671860
3516.064027	1054480.845441	42.676864
3516.108025	1054113.962428	42.681869
3516.250500	1053761.599588	42.686874
3515.941736	1053443.908617	42.691879
3516.179834	1053110.389587	42.696884
3516.192667	1052754.126241	42.701888
3515.724266	1052403.802789	42.706893
3516.010327	1052077.351001	42.711898
3515.715137	1051751.843845	42.716903
3515.921854	1051404.432705	42.721908
3516.130002	1051084.591563	42.726912
3515.611826	1050752.501964	42.731917
3515.951490	1050393.524156	42.736922
3515.710369	1050044.268086	42.741927
3515.564864	1049713.212635	42.746932
3515.849407	1049390.365989	42.751936
3515.638130	1049052.429987	42.756941
3515.529849	1048718.896160	42.761946
3515.477381	1048387.070454	42.766951
3515.427351	1048064.298115	42.771956
3515.391544	1047736.967534	42.776960
3515.277533	1047407.217003	42.781965
3515.167310	1047088.066196	42.786970
3514.888389	1046766.028267	42.791975
3515.199666	1046426.204576	42.796980
3515.391631	1046099.512204	42.801985
3514.963339	1045782.559535	42.806989
3515.181061	1045455.728423	42.811994
3515.186732	1045145.621164	42.816999
3514.907506	1044804.443234	42.822004
3514.666777	1044483.039064	42.827009
3514.912740	1044184.332749	42.832013
3515.024418	1043874.716562	42.837018
3514.669526	1043554.726436	42.842023
3514.900480	1043213.076798	42.847028
3514.932400	1042909.603119	42.852033
3514.913320	1042592.883863	42.857037
3514.806269	1042276.450917	42.862042
3514.663885	1041944.930772	42.867047
3514.596055	1041610.575986	42.872052
3514.769455	1041307.764599	42.877057
3514.832461	1041019.935784	42.882061
3515.070861	1040692.820795	42.887066
3514.540121	1040369.679718	42.892071
3514.522831	1040051.558669	42.897076
3514.728744	1039738.699676	42.902081
3514.503129	1039429.374580	42.907085
3514.575405	1039126.847759	42.912090
3514.241405	1038817.699857	42.917095
3514.147628	1038502.403453	42.922100
3514.443745	1038180.642762	42.927105
3514.273725	1037887.081533	42.932109
3514.288699	1037595.892108	42.937114
3514.460927	1037273.615839	42.942119
3514.263161	1036953.799891	42.947124
3514.128994	1036653.300459	42.952129
3514.288902	1036345.771677	42.957133
3514.237618	1036046.483368	42.962138
3513.984471	1035751.759114	42.967143
3514.323912	1035446.376187	42.972148
3514.307618	1035126.425408	42.977153
3514.110295	1034805.615245	42.982157
3514.199078	1034509.124044	42.987162
3514.311812	1034227.322005	42.992167
3514.060761	1033907.533456	42.997172
3514.062256	1033597.556508	43.002177
3513.902546	1033299.493433	43.007181
3514.172405	1032991.374294	43.012186
3513.875704	1032697.947563	43.017191
3513.782909	1032404.375012	43.022196
3513.988498	1032088.085337	43.027201
3513.996747	1031775.392262	43.032205
3513.786975	1031487.502607	43.037210
3513.884121	1031207.099610	43.042215
3513.869517	1030886.227506	43.047220
3513.656798	1030590.061775	43.052225
3513.910624	1030295.449724	43.057229
3513.696368	1029998.671862	43.062234
3513.326937	1029705.002897	43.067239
3513.623281	1029393.678543	43.072244
3513.375566	1029116.229797	43.077249
3513.382924	1028820.902584	43.082253
3513.484116	1028530.775163	43.087258
3513.280653	1028262.091665	43.092263
3513.174558	1027962.862914	43.097268
3513.281615	1027665.811342	43.102273
3513.326309	1027383.190513	43.107277
3513.241447	1027100.479849	43.112282
3513.371705	1026826.440210	43.117287
3513.461602	1026530.881549	43.122292
3513.405045	1026239.595318	43.127297
3513.246274	1025944.046616	43.132301
3513.415601	1025657.538504	43.137306
3513.278222	1025358.660177	43.142311
3513.331692	1025056.535845	43.147316
3513.435360	1024800.236049	43.152321
3513.353450	1024513.710785	43.157325
3513.228937	1024210.697698	43.162330
3513.180509	1023916.574860	43.167335
3513.441020	1023631.111421	43.172340
3513.163749	1023349.115520	43.177345
3512.901533	1023065.551549	43.182349
3512.952008	1022773.194681	43.187354
3512.770624	1022503.746170	43.192359
3512.646376	1022209.158305	43.197364
3512.939640	1021923.408544	43.202369
3512.617253	1021657.821872	43.207373
3512.965972	1021366.797344	43.212378
3512.629591	1021102.156576	43.217383
3512.656687	1020830.847399	43.222388
3512.820606	1020541.750528	43.227393
3512.473344	1020262.230009	43.232397
3512.726028	1019993.850539	43.237402
3512.916110	1019719.356290	43.242407
3512.765041	1019424.238487	43.247412
3512.760108	1019154.405940	43.252417
3513.075575	1018886.642414	43.257421
3513.012288	1018580.403861	43.262426
3512.369503	1018327.133342	43.267431
3512.269904	1018048.141072	43.272436
3512.423822	1017758.514321	43.277441
3512.333207	1017468.524680	43.282445
3512.503880	1017221.476207	43.287450
3512.463673	1016968.821690	43.292455
3512.555941	1016675.557780	43.297460
3512.584043	1016390.637816	43.302465
3512.298007	1016134.685655	43.307469
3512.303741	1015873.528203	43.312474
3512.347237	1015590.118520	43.317479
3512.418327	1015309.991284	43.322484
3512.469833	1015045.486572	43.327489
3512.125781	1014789.871151	43.332493
3512.284909	1014518.817899	43.337498
3511.910320	1014247.062579	43.342503
3512.241939	1013975.080700	43.347508
3512.033984	1013710.944459	43.352513
3511.733665	1013450.501911	43.357517
3511.959987	1013177.624693	43.362522
3512.020357	1012923.217722	43.367527
3512.042256	1012665.017063	43.372532
3512.376588	1012409.181766	43.377537
3512.050813	1012140.911122	43.382541
3511.825373	1011874.845747	43.387546
3511.861767	1011614.942922	43.392551
3511.952872	1011337.820964	43.397556
3511.784086	1011081.328084	43.402561
3511.815420	1010826.150999	43.407565
3512.006194	1010571.519171	43.412570
3511.880578	1010294.381604	43.417575
3511.827448	1010026.354092	43.422580
3511.702932	1009791.662344	43.427585
3511.541218	1009537.527832	43.432589
3511.684603	1009271.375985	43.437594
3511.504242	1009012.166449	43.442599
3511.528712	1008763.798696	43.447604
3511.584399	1008511.915185	43.452609
3511.099168	1008253.595924	43.457613
3511.359600	1008019.544779	43.462618
3511.469414	1007758.188177	43.467623
3511.728861	1007507.004070	43.472628
3511.450322	1007260.953618	43.477633
3511.541267	1006999.759484	43.482637
3511.605726	1006732.625746	43.487642
3511.187822	1006478.492878	43.492647
3511.192275	1006235.949337	43.497652
3511.270138	1006003.400735	43.502657
3510.519308	1005762.614624	43.507661
3511.106176	1005514.594842	43.512666
3510.880042	1005276.716816	43.517671
3511.349865	1005017.508541	43.522676
3511.263012	1004777.057429	43.527681
3510.932995	1004536.149728	43.532685
3511.156523	1004285.801118	43.537690
3511.020074	1004046.980983	43.542695
3510.854994	1003786.847955	43.547700
3511.111577	1003556.990802	43.552705
3510.586807	1003330.172080	43.557709
3511.068047	1003091.890994	43.562714
3510.666068	1002837.494408	43.567719
3510.841423	1002591.846995	43.572724
3510.770256	1002351.484777	43.577729
3510.679287	1002113.354052	43.582733
3510.547751	1001892.252305	43.587738
3510.523713	1001634.722235	43.592743
3510.495427	1001408.133987	43.597748
3510.888118	1001187.697066	43.602753
3510.691171	1000937.950933	43.607757
3510.844831	1000713.738526	43.612762
3510.731019	1000483.428148	43.617767
3510.626424	1000224.776347	43.622772
3510.723887	999978.541584	43.627777
3510.446596	999752.512260	43.632781
3510.606441	999525.136133	43.637786
3510.423286	999295.665193	43.642791
3510.517726	999071.981793	43.647796
3510.610211	998828.716534	43.652801
3510.374919	998602.439649	43.657805
3510.517567	998370.735150	43.662810
3510.672032	998137.460967	43.667815
3510.493526	997891.473149	43.672820
3510.613860	997667.437878	43.677825
3510.092177	997426.161590	43.682829
3510.642497	997192.004087	43.687834
3510.273328	996972.210525	43.692839
3510.159521	996738.630754	43.697844
3510.175566	996524.601354	43.702849
3509.852975	996293.375707	43.707853
3510.188397	996054.822616	43.712858
3510.211822	995843.007130	43.717863
3509.990045	995609.983267	43.722868
3510.151460	995380.881734	43.727873
3510.037070	995174.325711	43.732877
3509.804647	994949.266779	43.737882
3509.823650	994735.656663	43.742887
3509.771143	994504.606001	43.747892
3509.988247	994285.878717	43.752897
3509.763488	994079.593421	43.757901
3510.284518	993850.273453	43.762906
3509.988886	993616.107796	43.767911
3509.916507	993391.643060	43.772916
3509.846107	993193.585397	43.777921
3509.933221	992963.033900	43.782925
3509.854594	992741.176478	43.787930
3509.668441	992542.725258	43.792935
3510.029079	992307.130223	43.797940
3509.641156	992100.409969	43.802945
3509.728117	991873.031641	43.807949
3509.964519	991652.834850	43.812954
3509.629056	991438.184110	43.817959
3509.600396	991241.904198	43.822964
3509.848667	991006.663843	43.827969
3509.688236	990806.490039	43.832973
3509.806772	990582.565560	43.837978
3509.836955	990364.108240	43.842983
3509.374696	990136.068258	43.847988
3509.882496	989938.874803	43.852993
3509.715348	989714.573093	43.857997
3509.617867	989504.296847	43.863002
3509.859322	989301.272776	43.868007
3509.864967	989073.600870	43.873012
3509.620898	988849.863038	43.878017
3509.369834	988642.604346	43.883021
3509.623187	988437.889104	43.888026
3509.600126	988216.138694	43.893031
3509.492313	988014.004318	43.898036
3509.567498	987800.221905	43.903041
3509.355273	987590.967157	43.908045
3509.490828	987375.890433	43.913050
3509.326689	987168.271039	43.918055
3509.464098	986964.107423	43.923060
3509.127657	986763.039734	43.928065
3509.053536	986558.213308	43.933069
3509.258188	986342.012694	43.938074
3509.072488	986126.551361	43.943079
3508.780841	985926.227552	43.948084
3508.893191	985742.715755	43.953089
3508.665890	985529.190784	43.958093
3508.735208	985323.320284	43.963098
3508.513322	985138.184686	43.968103
3508.561826	984959.929414	43.973108
3508.434607	984761.392335	43.978113
3508.264557	984560.121910	43.983117
3508.624933	984366.079126	43.988122
3508.181752	984200.963256	43.993127
3508.508813	984005.449236	43.998132
3508.457785	983814.970305	44.003137
3508.341570	983616.098648	44.008141
3508.758314	983420.940406	44.013146
3508.755169	983236.976456	44.018151
3508.719190	983038.071448	44.023156
3508.341571	982845.172676	44.028161
3508.536600	982651.391810	44.033165
3508.698696	982445.109220	44.038170
3508.318311	982271.430672	44.043175
3508.250043	982069.176660	44.048180
3508.631752	981891.161334	44.053185
3508.346909	981706.022415	44.058189
3508.461445	981524.425749	44.063194
3508.375024	981326.153160	44.068199
3508.114025	981132.005143	44.073204
3508.411554	980969.799656	44.078209
3508.319763	980784.892146	44.083213
3508.743949	980592.175967	44.088218
3508.608106	980406.384235	44.093223
3508.450893	980208.866108	44.098228
3508.383112	980030.378369	44.103233
3508.430866	979854.894890	44.108237
3508.623203	979651.144497	44.113242
3508.682836	979449.167520	44.118247
3508.578643	979257.568228	44.123252
3508.386613	979084.054894	44.128257
3508.418972	978889.098344	44.133261
3508.858237	978700.322526	44.138266
3508.546530	978502.966365	44.143271
3508.077785	978313.545511	44.148276
3508.507654	978133.450635	44.153281
3508.036999	977955.746377	44.158285
3508.287271	977769.414421	44.163290
3508.262252	977585.272109	44.168295
3508.253704	977384.015404	44.173300
3508.461478	977206.860381	44.178305
3507.964818	977043.403602	44.183309
3508.276897	976834.645534	44.188314
3508.174330	976676.196706	44.193319
3508.189290	976488.982004	44.198324
3508.264122	976291.094840	44.203329
3508.172533	976127.447421	44.208333
3508.033983	975951.972689	44.213338
3508.059190	975757.399499	44.218343
3508.051774	975576.318478	44.223348
3508.401031	975387.350483	44.228353
3508.071128	975210.711184	44.233357
3508.377184	975040.806809	44.238362
3508.010774	974860.349012	44.243367
3508.314415	974685.936158	44.248372
3508.295315	974492.500835	44.253377
3507.872833	974300.299023	44.258381
3508.153022	974110.126701	44.263386
3507.672212	973946.187672	44.268391
3507.611102	973769.361860	44.273396
3508.251825	973567.081630	44.278401
3507.600143	973399.046969	44.283405
3507.825984	973223.917752	44.288410
3507.527270	973064.716614	44.293415
3507.375406	972882.302595	44.298420
3507.610751	972711.069121	44.303425
3507.437212	972555.941977	44.308429
3507.532568	972386.091478	44.313434
3507.107208	972215.245525	44.318439
3507.472246	972018.043543	44.323444
3507.605941	971874.392344	44.328449
3507.173495	971720.165814	44.333453
3507.685305	971537.110494	44.338458
3507.866332	971363.888834	44.343463
3507.653762	971206.481082	44.348468
3507.979773	971012.871555	44.353473
3507.541389	970856.861391	44.358477
3507.777097	970686.056742	44.363482
3507.241371	970522.028853	44.368487
3507.554131	970347.188995	44.373492
3507.709734	970173.935627	44.378497
3507.561678	970006.990933	44.383501
3507.215219	969847.610508	44.388506
3507.281330	969686.787408	44.393511
3507.557894	969505.370024	44.398516
3507.322657	969351.928306	44.403521
3507.235306	969192.976461	44.408525
3507.399819	969022.231956	44.413530
3507.104701	968860.857894	44.418535
3507.139978	968706.571242	44.423540
3506.976362	968541.642323	44.428545
3507.041301	968365.608212	44.433549
3507.261629	968213.529574	44.438554
3506.968407	968057.125713	44.443559
3506.910969	967897.937307	44.448564
3507.268642	967736.717888	44.453569
3506.977754	967573.838308	44.458573
3507.180435	967421.056218	44.463578
3507.001926	967262.359743	44.468583
3506.813871	967108.654510	44.473588
3507.259628	966952.490573	44.478593
3506.990970	966796.440067	44.483597
3507.104210	966630.529370	44.488602
3507.053807	966472.769313	44.493607
3507.163908	966312.921839	44.498612
3507.084853	966156.430996	44.503617
3506.600033	966003.822440	44.508621
3506.688947	965847.981131	44.513626
3506.738464	965689.105746	44.518631
3506.698822	965540.525336	44.523636
3506.870724	965391.906248	44.528641
3506.709616	965239.517954	44.533645
3506.872094	965071.203288	44.538650
3506.807024	964947.100993	44.543655
3506.652324	964780.103527	44.548660
3506.863979	964621.563824	44.553665
3506.598237	964476.128054	44.558669
3506.729274	964333.562351	44.563674
3506.518178	964176.549572	44.568679
3506.485334	964031.064199	44.573684
3506.793160	963897.668222	44.578689
3506.650560	963748.274698	44.583693
3506.710917	963576.895808	44.588698
3506.795953	963440.978405	44.593703
3506.372106	963301.516083	44.598708
3506.568757	963146.759766	44.603713
3506.451120	962996.460722	44.608717
3506.847802	962839.507375	44.613722
3506.572411	962703.141957	44.618727
3506.349033	962559.512755	44.623732
3506.681765	962408.634203	44.628737
3506.366704	962261.484583	44.633741
3506.257643	962127.920299	44.638746
3506.413408	961998.523710	44.643751
3506.119423	961834.796102	44.648756
3506.416630	961674.691041	44.653761
3506.275707	961552.488395	44.658765
3506.182616	961410.083310	44.663770
3506.213344	961279.024839	44.668775
3505.942573	961143.503947	44.673780
3506.280351	960997.390816	44.678785
3505.925314	960858.544205	44.683789
3506.173825	960706.556680	44.688794
3506.129952	960583.337196	44.693799
3505.937637	960466.805945	44.698804
3506.197689	960320.198292	44.703809
3505.890860	960177.896021	44.708813
3505.945265	960034.158143	44.713818
3505.847124	959925.541910	44.718823
3505.519819	959775.389501	44.723828
3505.855217	959655.421336	44.728833
3505.681162	959526.906068	44.733837
3505.878713	959391.364919	44.738842
3505.957360	959273.294124	44.743847
3505.723385	959147.035547	44.748852
3505.893779	958992.858485	44.753857
3505.616269	958875.720763	44.758861
3505.806755	958744.676471	44.763866
3505.621418	958608.101287	44.768871
3505.581243	958482.874998	44.773876
3505.508765	958364.124016	44.778881
3505.467099	958252.917150	44.783885
3505.594418	958114.023101	44.788890
3505.647580	957980.336047	44.793895
3505.676636	957849.199949	44.798900
3505.498071	957739.280779	44.803905
3505.678756	957620.472810	44.808909
3505.938826	957486.249825	44.813914
3505.535040	957371.946883	44.818919
3505.608636	957233.432862	44.823924
3505.710886	957106.387643	44.828929
3505.208760	956985.913421	44.833933
3505.546853	956854.998139	44.838938
3505.241168	956739.391259	44.843943
3505.129074	956632.971642	44.848948
3505.241399	956510.914799	44.853953
3505.004819	956380.770148	44.858957
3505.226727	956264.183917	44.863962
3505.673304	956146.282918	44.868967
3505.287167	956046.078484	44.873972
3505.631879	955904.152192	44.878977
3505.297764	955788.175176	44.883981
3505.328790	955681.168593	44.888986
3505.055852	955565.603522	44.893991
3504.865814	955443.997614	44.898996
3505.436853	955330.583271	44.904001
3505.153645	955206.405021	44.909005
3504.963267	955112.428939	44.914010
3505.165349	955009.874877	44.919015
3505.276131	954878.068472	44.924020
3505.377673	954756.015557	44.929025
3505.181035	954666.623041	44.934029
3505.194936	954562.369406	44.939034
3505.319467	954436.192335	44.944039
3505.117450	954319.343894	44.949044
3505.147497	954213.167480	44.954049
3505.143781	954085.950709	44.959053
3505.012861	953980.943817	44.964058
3505.241614	953885.345594	44.969063
3505.126831	953767.322256	44.974068
3505.302676	953634.612077	44.979073
3504.948364	953545.321542	44.984077
3505.122239	953445.323599	44.989082
3504.995146	953327.005118	44.994087
3504.949803	953212.879905	44.999092
3505.025535	953109.351772	45.004097
3504.991721	952989.192346	45.009101
3505.108305	952896.942700	45.014106
3505.129905	952788.537529	45.019111
3505.082141	952672.200061	45.024116
3505.251541	952560.034189	45.029121
3504.900178	952449.291210	45.034125
3504.697870	952348.568315	45.039130
3505.055707	952236.077253	45.044135
3505.014880	952116.089859	45.049140
3504.631950	952022.471374	45.054145
3504.576940	951933.773241	45.059149
3505.126040	951819.614745	45.064154
3505.190412	951696.059443	45.069159
3504.706882	951604.268148	45.074164
3504.861793	951499.354627	45.079169
3504.904481	951400.486776	45.084173
3505.106617	951286.086448	45.089178
3505.257118	951176.094637	45.094183
3505.114565	951069.115742	45.099188
3505.221217	950967.740565	45.104193
3504.902383	950869.783441	45.109197
3505.005887	950761.417617	45.114202
3505.222965	950623.071114	45.119207
3505.008886	950527.770318	45.124212
3505.181171	950431.159735	45.129217
3504.922310	950326.290398	45.134221
3504.944787	950198.589836	45.139226
3504.806004	950097.333637	45.144231
3504.609753	950017.815528	45.149236
3504.992263	949909.098595	45.154241
3504.840410	949777.012631	45.159245
3504.717689	949669.714130	45.164250
3504.495932	949588.661812	45.169255
3504.814742	949493.158330	45.174260
3504.703401	949379.724598	45.179265
3504.597602	949292.521074	45.184269
3504.975080	949181.300291	45.189274
3504.870986	949078.773651	45.194279
3504.606624	948972.441416	45.199284
3505.106366	948877.854221	45.204289
3504.587278	948788.986732	45.209293
3504.617368	948662.491592	45.214298
3504.541469	948561.673603	45.219303
3504.478451	948475.311010	45.224308
3504.273609	948385.618741	45.229313
3504.161363	948279.438673	45.234317
3504.228689	948164.799633	45.239322
3504.458017	948092.172450	45.244327
3504.314227	948008.305238	45.249332
3504.215429	947901.349043	45.254337
3504.002435	947809.636960	45.259341
3504.165572	947720.351372	45.264346
3504.252630	947636.248550	45.269351
3504.222048	947534.062194	45.274356
3504.161331	947438.008531	45.279361
3504.215856	947370.859305	45.284365
3504.388866	947275.434576	45.289370
3504.593681	947182.780527	45.294375
3504.086329	947084.303521	45.299380
3504.319738	946993.078123	45.304385
3504.080536	946912.657119	45.309389
3504.306472	946813.479456	45.314394
3504.632068	946721.084615	45.319399
3504.569068	946645.803130	45.324404
3504.620852	946542.625699	45.329409
3504.312986	946449.947180	45.334413
3504.251956	946329.540847	45.339418
3504.014676	946248.821815	45.344423
3504.165511	946184.706913	45.349428
3504.403215	946078.807207	45.354433
3503.848091	945988.364605	45.359437
3504.229095	945894.987867	45.364442
3504.200186	945820.646831	45.369447
3504.166494	945737.874353	45.374452
3504.281376	945640.033845	45.379457
3504.301289	945551.500927	45.384461
3504.057815	945464.159644	45.389466
3504.304219	945366.963021	45.394471
3503.892643	945274.951272	45.399476
3504.097917	945178.332796	45.404481
3504.193361	945100.798932	45.409485
3503.932117	945017.190050	45.414490
3504.149161	944933.117749	45.419495
3503.677271	944843.312221	45.424500
3503.820839	944758.195114	45.429505
3503.808925	944668.885769	45.434509
3503.863261	944588.955323	45.439514
3503.998680	944521.085041	45.444519
3503.745550	944446.090429	45.449524
3503.895056	944352.628260	45.454529
3503.670886	944263.155234	45.459533
3503.751981	944185.801753	45.464538
3503.762099	944108.842168	45.469543
3503.570968	944023.864005	45.474548
3504.014206	943954.114659	45.479553
3503.568486	943881.827192	45.484557
3503.614059	943789.042918	45.489562
3503.721899	943722.125202	45.494567
3503.397535	943639.750548	45.499572
3503.588854	943553.168146	45.504577
3503.800982	943470.990006	45.509581
3503.611860	943417.919755	45.514586
3503.859204	943338.896832	45.519591
3503.431405	943253.178240	45.524596
3503.574417	943167.268364	45.529601
3503.782661	943089.014941	45.534605
3503.446017	943008.261896	45.539610
3503.855075	942934.766036	45.544615
3503.438497	942877.126435	45.549620
3503.695003	942806.433876	45.554625
3503.853762	942713.324214	45.559629
3503.769182	942632.523831	45.564634
3503.532309	942550.213399	45.569639
3503.687251	942473.014057	45.574644
3503.709576	942405.326572	45.579649
3503.366989	942323.125838	45.584653
3503.496608	942239.216188	45.589658
3503.581755	942170.748328	45.594663
3503.451412	942103.753197	45.599668
3503.659889	942012.732115	45.604673
3503.622913	941947.349515	45.609677
3503.705602	941887.507411	45.614682
3503.732291	941789.033754	45.619687
3503.615708	941708.703748	45.624692
3503.843189	941646.054425	45.629697
3503.541838	941568.341563	45.634701
3503.627907	941482.796885	45.639706
3503.367951	941419.458034	45.644711
3503.333761	941346.588168	45.649716
3503.708126	941260.321141	45.654721
3503.387656	941194.592251	45.659725
3503.470234	941123.809681	45.664730
3503.164451	941056.734127	45.669735
3503.034684	940985.601082	45.674740
3503.727694	940905.221282	45.679745
3503.291997	940839.315109	45.684749
3502.879184	940773.692035	45.689754
3503.358752	940699.194133	45.694759
3503.554145	940631.263365	45.699764
3503.458926	940587.163705	45.704769
3503.626707	940507.823355	45.709773
3503.863197	940430.868147	45.714778
3503.705418	940348.605910	45.719783
3503.583343	940276.598794	45.724788
3503.750663	940190.444159	45.729793
3503.389202	940117.898824	45.734797
3503.748244	940064.320550	45.739802
3503.913391	939972.311988	45.744807
3503.193799	939895.890058	45.749812
3503.456474	939819.113391	45.754817
3503.239654	939754.116677	45.759821
3503.427355	939603.107562	45.764826
3503.510032	939418.825574	45.769831
3503.484703	939173.448259	45.774836
3503.873524	938867.648532	45.779841
3503.497021	938484.052784	45.784845
3503.129142	938031.535828	45.789850
3503.263439	937552.796477	45.794855
3503.079985	936987.118552	45.799860
3503.437984	936346.810125	45.804865
3503.234826	935659.095969	45.809869
3503.190222	934898.397284	45.814874
3502.852536	934073.495177	45.819879
3502.299862	933155.247341	45.824884
3502.649624	932177.905913	45.829889
3502.245884	931136.907744	45.834893
3502.279236	930007.899878	45.839898
3502.299500	928817.717901	45.844903
3501.690172	927554.501905	45.849908
3502.069734	926189.373820	45.854913
3501.601078	924761.708932	45.859917
3501.405680	923252.223090	45.864922
3501.453618	921632.750606	45.869927
3501.086364	919942.390823	45.874932
3500.981584	918174.130129	45.879937
3500.374751	916313.088431	45.884941
3500.428506	914379.123988	45.889946
3500.066753	912359.421342	45.894951
3499.815563	910228.727166	45.899956
3499.873158	908021.811547	45.904961
3499.198179	905746.770868	45.909965
3498.803633	903361.064778	45.914970
3498.614127	900891.716137	45.919975
3497.967358	898359.122916	45.924980
3497.526174	895713.976999	45.929985
3497.407199	893015.701184	45.934989
3497.112614	890200.431058	45.939994
3496.798199	887278.726457	45.944999
3496.238926	884312.963647	45.950004
3495.861570	881249.603599	45.955009
3495.500639	878090.858946	45.960013
3494.854060	874847.991543	45.965018
3494.360593	871527.988682	45.970023
3493.605187	868130.415003	45.975028
3493.609113	864640.793212	45.980033
3493.012352	861041.502225	45.985037
3492.699807	857356.159768	45.990042
3491.899376	853608.419556	45.995047
3491.353428	849779.843712	46.000052
3491.137796	845827.683707	46.005057
3490.162336	841816.055433	46.010061
3489.266855	837711.098858	46.015066
3488.914338	833545.014691	46.020071
3488.254844	829283.490589	46.025076
3487.816074	824907.694045	46.030081
3487.123125	820470.115640	46.035085
3486.233261	815971.190654	46.040090
3485.580648	811350.917676	46.045095
3484.879436	806655.178170	46.050100
3484.314191	801874.987723	46.055105
3483.396383	797022.172508	46.060109
3482.561118	792071.189543	46.065114
3482.263102	787027.797290	46.070119
3481.432154	781899.449729	46.075124
3480.675268	776693.297025	46.080129
3479.878170	771419.587096	46.085133
3478.865935	766023.458670	46.090138
3478.109006	760532.159663	46.095143
3477.183371	754994.354316	46.100148
3476.457558	749347.510352	46.105153
3475.218665	743601.160205	46.110157
3474.644829	737793.560202	46.115162
3473.774368	731890.469477	46.120167
3472.610215	725904.779578	46.125172
3471.756858	719847.537242	46.130177
3470.862167	713681.431394	46.135181
3469.638257	707398.493759	46.140186
3468.423792	701061.973757	46.145191
3467.096656	694672.846757	46.150196
3466.596308	688158.383610	46.155201
3465.417973	681563.483811	46.160205
3464.365363	674907.869655	46.165210
3463.349795	668143.166161	46.170215
3461.866941	661298.372890	46.175220
3461.273010	654369.392622	46.180225
3459.859297	647358.026121	46.185229
3458.683024	640256.020618	46.190234
3457.608857	633052.748556	46.195239
3455.900970	625773.429957	46.200244
3454.941294	618426.263851	46.205249
3453.539107	611005.702244	46.210253
3451.894715	603491.147634	46.215258
3450.780394	595906.116218	46.220263
3449.026088	588233.191472	46.225268
3447.963676	580447.463305	46.230273
3446.188815	572600.213363	46.235277
3444.864414	564706.828129	46.240282
3443.632618	556707.703058	46.245287
3442.119557	548618.124699	46.250292
3440.697445	540442.301779	46.255297
3439.000233	532206.539305	46.260301
3437.088338	523889.459466	46.265306
3435.673196	515498.087310	46.270311
3433.561690	507013.391376	46.275316
3431.949843	498450.311868	46.280321
3430.424521	489853.699922	46.285325
3428.899329	481155.884174	46.290330
3427.202061	472377.179912	46.295335
3425.141346	463519.706368	46.300340
3423.522785	454585.784966	46.305345
3421.412138	445579.303875	46.310349
3419.199236	436508.209544	46.315354
3417.371884	427372.075907	46.320359
3415.476847	418177.290928	46.325364
3413.559773	408887.630136	46.330369
3410.906077	399534.693500	46.335373
3408.966109	390130.508039	46.340378
3406.900718	380662.660064	46.345383
3404.351451	371106.594955	46.350388
3401.940732	361491.760991	46.355393
3399.653830	351848.766721	46.360397
3397.068972	342159.739580	46.365402
3394.824832	332377.199419	46.370407
3391.803935	322530.301367	46.375412
3389.175339	312649.583329	46.380417
3386.788847	302734.656351	46.385421
3384.216605	292749.784913	46.390426
3381.498456	282733.515234	46.395431
3378.534156	272678.972551	46.400436
3375.601772	262533.457353	46.405441
3372.562674	252363.384068	46.410445
3369.302657	242170.506416	46.415450
3366.423802	231910.880128	46.420455
3362.630492	221621.713152	46.425460
3359.520146	211274.551841	46.430465
3355.879150	200944.157579	46.435469
3352.400056	190584.521193	46.440474
3348.712685	180219.593947	46.445479
3344.410971	169850.979003	46.450484
3340.295514	159447.064891	46.455489
3336.198493	149051.628528	46.460493
3331.644975	138666.175803	46.465498
3326.898440	128261.046613	46.470503
3321.829773	117880.421620	46.475508
3316.751716	107538.063003	46.480513
3310.706551	97225.153947	46.485517
3304.061116	86953.190425	46.490522
3296.630512	76736.987540	46.495527
3281.870005	66821.277227	46.500532
3255.217687	57371.060724	46.505537
3228.808411	48202.688338	46.510541
3203.662152	39399.480722	46.515546
3173.265437	31217.030350	46.520551
3133.332184	23891.631235	46.525556
3089.652224	17377.315888	46.530561
3047.080073	11686.671879	46.535565
3008.781701	6807.191973	46.540570
2973.492009	2753.411892	46.545575
2908.680360	432.968376	46.550580
2804.224401	392.492007	46.555585
2756.911726	357.495676	46.560589
2762.769500	341.624848	46.565594
2799.620992	325.969111	46.570599
2843.123497	350.378084	46.575604
2877.974035	349.995326	46.580609
2898.356894	336.880298	46.585613
2904.627197	352.616029	46.590618
2902.349019	321.065937	46.595623
2895.382933	320.903889	46.600628
2888.460833	323.298433	46.605633
2882.528621	336.161509	46.610637
2878.847523	322.988074	46.615642
2876.419307	320.744115	46.620647
2874.373537	322.707310	46.625652
2872.407471	316.573127	46.630657
2870.396842	315.668177	46.635661
2867.942699	311.972706	46.640666
2865.611921	306.744189	46.645671
2862.782742	323.653587	46.650676
2859.481178	326.560138	46.655681
2856.427645	306.390048	46.660685
2853.417300	306.704979	46.665690
2850.389429	310.113922	46.670695
2846.957546	307.468389	46.675700
2844.175726	297.986630	46.680705
2840.937894	302.339846	46.685709
2837.549656	307.653760	46.690714
2834.847162	301.184345	46.695719
2831.573927	307.332729	46.700724
2828.050520	300.269721	46.705729
2825.100351	321.878960	46.710733
2821.401682	301.308583	46.715738
2818.591622	295.265227	46.720743
2815.267701	308.538630	46.725748
2812.074300	316.240633	46.730753
2808.844166	301.640512	46.735757
2804.998700	303.925870	46.740762
2802.094072	290.166567	46.745767
2798.505321	310.252843	46.750772
2795.254691	295.907969	46.755777
2791.922554	274.871965	46.760781
2788.155361	291.778638	46.765786
2785.005913	298.297875	46.770791
2781.576658	296.367059	46.775796
2778.392781	294.059492	46.780801
2775.048249	300.525267	46.785805
2771.417595	291.272765	46.790810
2768.619034	267.299398	46.795815
2764.856897	286.160094	46.800820
2761.645811	293.548153	46.805825
2758.242138	274.902824	46.810829
2754.657530	275.602304	46.815834
2751.232506	288.118958	46.820839
2747.803397	287.616890	46.825844
2744.057087	277.846033	46.830849
2741.415487	281.676587	46.835853
2737.682562	288.307521	46.840858
2734.352612	275.704431	46.845863
2731.087988	271.816898	46.850868
2727.430137	288.418189	46.855873
2724.010133	293.500321	46.860877
2720.044183	270.027828	46.865882
2717.212106	262.957558	46.870887
2713.553243	268.847750	46.875892
2710.175197	260.274000	46.880897
2706.771742	277.316631	46.885901
2702.868149	291.415439	46.890906
2699.611980	274.237326	46.895911
2696.691815	263.756152	46.900916
2693.312496	259.674466	46.905921
2689.282078	266.104380	46.910925
2685.812702	288.498628	46.915930
2682.852014	262.966048	46.920935
2678.953620	269.362955	46.925940
2675.497730	267.798039	46.930945
2671.782619	263.741341	46.935949
2668.498361	269.667255	46.940954
2665.486282	268.101086	46.945959
2661.882206	264.222893	46.950964
2658.401481	273.926956	46.955969
2655.251750	262.557721	46.960973
2651.980072	254.151733	46.965978
2648.139450	246.514226	46.970983
2644.399182	267.284549	46.975988
2641.117663	251.539922	46.980993
2637.908907	269.981479	46.985997
2633.874885	277.086785	46.991002
2630.327717	255.487069	46.996007
2626.963566	253.714782	47.001012
2623.979453	268.963779	47.006017
2620.556557	256.526932	47.011021
2616.231774	267.043266	47.016026
2613.270202	259.171751	47.021031
2610.095120	257.207003	47.026036
2606.363899	264.833080	47.031041
2603.139605	262.164491	47.036045
2599.107025	263.017713	47.041050
2595.857639	250.503937	47.046055
2592.227487	262.211476	47.051060
2588.982901	255.648178	47.056065
2585.638561	248.955429	47.061069
2581.743173	257.465457	47.066074
2578.565440	245.328265	47.071079
2575.398951	252.777675	47.076084
2571.698054	258.271669	47.081089
2568.474940	241.018774	47.086093
2564.402807	241.833058	47.091098
2560.967478	240.147119	47.096103
2557.321235	262.339777	47.101108
2554.047524	252.774740	47.106113
2550.561735	230.371354	47.111117
2546.920573	245.494099	47.116122
2544.001449	254.827590	47.121127
2540.212435	252.675555	47.126132
2536.915807	257.382363	47.131137
2533.527638	256.284011	47.136141
2529.642972	253.168455	47.141146
2526.329261	232.521781	47.146151
2522.620276	245.893435	47.151156
2519.050335	246.902633	47.156161
2515.696531	232.451583	47.161165
2512.181942	235.648590	47.166170
2509.200447	236.703901	47.171175
2505.591779	244.940864	47.176180
2501.982209	234.483025	47.181185
2498.267196	240.216429	47.186189
2494.639086	248.424345	47.191194
2491.526220	228.666661	47.196199
2488.035953	232.540647	47.201204
2484.592676	245.975830	47.206209
2481.144794	251.905210	47.211213
2477.633842	235.908303	47.216218
2473.732207	215.873884	47.221223
2470.023106	233.737878	47.226228
2466.956220	241.291443	47.231233
2463.601839	237.542947	47.236237
2459.471187	234.983640	47.241242
2456.510308	235.702233	47.246247
2453.444979	232.486434	47.251252
2449.622429	228.198589	47.256257
2446.000148	237.251085	47.261261
2442.296000	237.828266	47.266266
2439.264092	233.226456	47.271271
2435.697092	232.658881	47.276276
2432.264369	241.830665	47.281281
2428.917214	235.762328	47.286285
2424.831866	219.308939	47.291290
2421.502005	215.250020	47.296295
2418.140672	226.178323	47.301300
2414.612690	239.228748	47.306305
2411.301238	227.708770	47.311309
2407.488793	232.804426	47.316314
2404.080500	221.685852	47.321319
2400.781482	248.191745	47.326324
2397.267695	232.858878	47.331329
2393.975590	212.887663	47.336333
2389.754871	217.824251	47.341338
2386.689824	236.148111	47.346343
2383.258398	241.956432	47.351348
2379.588626	222.917487	47.356353
2376.317027	209.255995	47.361357
2372.384986	233.469767	47.366362
2369.393880	220.150592	47.371367
2365.715242	230.334450	47.376372
2362.270244	222.974686	47.381377
2358.778088	235.447839	47.386381
2355.058376	218.997830	47.391386
2351.717047	213.231731	47.396391
2348.333637	236.032736	47.401396
2344.654718	231.729546	47.406401
2341.451098	222.406613	47.411405
2337.651262	225.759743	47.416410
2334.275374	232.044375	47.421415
2330.563192	237.777284	47.426420
2327.074877	220.078599	47.431425
2323.708660	207.306186	47.436429
2320.190127	225.957875	47.441434
2317.053617	222.714122	47.446439
2313.553139	215.656033	47.451444
2309.428021	225.332696	47.456449
2306.272497	226.211594	47.461453
2302.723802	216.263531	47.466458
2299.211266	198.068535	47.471463
2295.862663	221.541707	47.476468
2292.138422	243.545825	47.481473
2288.952250	230.629186	47.486477
2285.136299	213.983991	47.491482
2282.145977	207.096401	47.496487
2278.389265	219.942689	47.501492
2274.519933	214.573865	47.506497
2271.529081	211.052091	47.511501
2267.738906	227.723126	47.516506
2264.226098	219.717691	47.521511
2260.591351	200.579956	47.526516
2257.541140	214.014082	47.531521
2253.842951	221.114753	47.536525
2250.145313	232.989291	47.541530
2246.565091	206.348253	47.546535
2243.129913	215.181239	47.551540
2239.874597	214.320168	47.556545
2236.517061	209.462996	47.561549
2232.630149	220.724961	47.566554
2229.334245	204.244613	47.571559
2225.941944	233.667961	47.576564
2222.728314	222.829412	47.581569
2219.239342	209.471006	47.586573
2215.225961	220.921344	47.591578
2211.859825	217.112272	47.596583
2208.146842	221.031097	47.601588
2204.420417	238.110021	47.606593
2201.235227	217.451459	47.611597
2197.987270	200.243579	47.616602
2194.568418	206.636358	47.621607
2191.159956	225.721542	47.626612
2187.295864	214.390318	47.631617
2183.722757	215.234264	47.636621
2180.382034	221.971969	47.641626
2176.807901	194.291223	47.646631
2173.521656	198.312211	47.651636
2169.613763	209.437967	47.656641
2166.404415	216.022999	47.661645
2162.878523	216.349642	47.666650
2159.648069	191.669079	47.671655
2155.627515	208.494732	47.676660
2151.800771	225.041417	47.681665
2149.196748	212.637223	47.686669
2145.405474	213.312672	47.691674
2142.203085	221.181772	47.696679
2138.240384	209.564389	47.701684
2134.668303	196.378582	47.706689
2131.606964	208.977433	47.711693
2127.782108	228.949616	47.716698
2124.244717	205.620177	47.721703
2120.975413	195.199889	47.726708
2117.439496	211.742302	47.731713
2113.986813	217.000903	47.736717
2109.869103	220.117925	47.741722
2106.695130	203.680478	47.746727
2103.481062	197.565908	47.751732
2099.816362	220.182302	47.756737
2096.793651	224.419895	47.761741
2092.787611	222.484231	47.766746
2089.443979	199.537984	47.771751
2085.647101	219.889594	47.776756
2082.157331	226.923406	47.781761
2079.090920	200.982708	47.786765
2075.295926	228.334664	47.791770
2071.797690	212.857010	47.796775
2068.619173	196.943976	47.801780
2064.888727	207.156506	47.806785
2061.320290	198.575976	47.811789
2057.475654	205.342095	47.816794
2054.429876	203.461432	47.821799
2050.868129	212.521244	47.826804
2047.376179	208.217667	47.831809
2043.959573	192.382302	47.836813
2039.832325	200.897433	47.841818
2036.802096	203.426299	47.846823
2033.436055	203.210206	47.851828
2029.956659	216.618712	47.856833
2026.557151	218.181758	47.861837
2022.870548	209.739314	47.866842
2019.304984	189.292520	47.871847
2015.384697	197.156471	47.876852
2012.315696	215.014822	47.881857
2009.221143	203.630270	47.886861
2005.139528	208.779581	47.891866
2001.852281	207.619256	47.896871
1998.428129	203.204294	47.901876
1994.652400	193.789494	47.906881
1991.436794	211.960580	47.911885
1987.545522	220.774198	47.916890
1984.242544	206.387913	47.921895
1981.115330	196.222155	47.926900
1977.362857	196.145106	47.931905
1974.196696	214.236423	47.936909
1970.367584	201.669226	47.941914
1966.963901	200.128400	47.946919
1963.236324	202.831228	47.951924
1959.674473	209.592272	47.956929
1956.447795	217.943299	47.961933
1952.497738	208.979295	47.966938
1949.307838	205.714237	47.971943
1945.652409	202.577870	47.976948
1942.059937	215.533517	47.981953
1939.169978	204.804512	47.986957
1935.404990	201.134776	47.991962
1931.931830	188.642661	47.996967
1928.232807	211.035587	48.001972
1924.734466	215.394916	48.006977
1921.601331	193.633866	48.011981
1917.525604	201.176656	48.016986
1914.281683	196.384761	48.021991
1911.091028	190.374546	48.026996
1907.017827	200.252143	48.032001
1903.764462	205.841466	48.037005
1900.307366	211.927264	48.042010
1897.157747	193.969801	48.047015
1893.298118	202.124287	48.052020
1889.549463	202.266147	48.057025
1886.174352	173.756736	48.062029
1882.365128	195.611158	48.067034
1879.210757	212.187274	48.072039
1875.876076	187.481398	48.077044
1872.590422	184.805526	48.082049
1869.205031	178.864557	48.087053
1865.480323	203.630187	48.092058
1862.156703	199.184801	48.097063
1858.468921	184.480229	48.102068
1854.463011	188.965248	48.107073
1851.105704	196.196287	48.112077
1847.595446	190.513078	48.117082
1844.208755	195.008796	48.122087
1840.938350	194.701844	48.127092
1837.261943	197.094227	48.132097
1834.181085	179.905986	48.137101
1830.099164	189.364215	48.142106
1826.711943	205.180389	48.147111
1822.998688	199.381327	48.152116
1819.504028	179.071260	48.157121
1816.200750	179.393894	48.162125
1812.402239	193.294585	48.167130
1809.075176	205.481807	48.172135
1806.037786	197.546770	48.177140
1802.622775	197.327717	48.182145
1799.218134	183.747926	48.187149
1795.344592	196.489058	48.192154
1791.631640	191.701020	48.197159
1787.939414	198.140837	48.202164
1784.627620	192.828094	48.207169
1781.584007	206.778173	48.212173
1777.701443	200.979154	48.217178
1774.405601	182.627637	48.222183
1770.871327	183.376194	48.227188
1766.963572	196.792413	48.232193
1763.794411	184.553690	48.237197
1759.859335	186.554438	48.242202
1756.575527	174.961458	48.247207
1753.586035	189.148925	48.252212
1749.740208	195.380206	48.257217
1746.830687	185.423510	48.262221
1742.714692	207.193455	48.267226
1738.944431	189.895869	48.272231
1735.647125	178.477367	48.277236
1731.829622	193.843788	48.282241
1728.740058	176.499017	48.287245
1725.354705	192.406349	48.292250
1721.957443	190.944588	48.297255
1718.580543	182.760897	48.302260
1714.520267	177.040376	48.307265
1711.385205	174.502705	48.312269
1707.437574	191.191780	48.317274
1703.909042	199.117009	48.322279
1700.528034	176.074843	48.327284
1696.959918	181.723869	48.332289
1693.664038	178.067429	48.337293
1690.132465	180.078282	48.342298
1686.863940	191.326209	48.347303
1683.087963	192.690504	48.352308
1679.358376	184.481574	48.357313
1676.213699	183.219058	48.362317
1672.280731	176.787509	48.367322
1669.052837	179.647248	48.372327
1665.696365	185.922508	48.377332
1661.993796	204.196118	48.382337
1658.913090	170.315518	48.387341
1655.244644	174.505135	48.392346
1651.740127	193.973243	48.397351
1647.884261	196.682892	48.402356
1644.520072	182.310589	48.407361
1641.522855	183.210599	48.412365
1637.904440	191.046609	48.417370
1634.065573	184.548255	48.422375
1630.615928	179.048914	48.427380
1626.602315	191.796848	48.432385
1623.602060	200.770186	48.437389
1620.296694	186.420939	48.442394
1616.902070	169.045102	48.447399
1613.184821	192.727767	48.452404
1609.891414	199.921722	48.457409
1606.281482	186.186323	48.462413
1602.133079	194.664804	48.467418
1598.968373	178.304497	48.472423
1595.660866	179.689390	48.477428
1591.852988	177.783271	48.482433
1588.492329	186.640887	48.487437
1585.258084	196.866523	48.492442
1581.736041	175.381507	48.497447
1578.338022	184.113989	48.502452
1574.578348	170.967309	48.507457
1571.288181	176.288879	48.512461
1567.566826	191.004097	48.517466
1563.896292	188.019491	48.522471
1560.346890	176.228864	48.527476
1556.959058	174.122837	48.532481
1553.639176	178.296610	48.537485
1549.805431	191.420636	48.542490
1546.450590	180.679588	48.547495
1543.311112	163.510197	48.552500
1539.342047	171.992742	48.557505
1536.258201	181.984036	48.562509
1532.620016	183.923183	48.567514
1528.798663	185.551827	48.572519
1525.599450	177.020192	48.577524
1522.320245	169.779459	48.582529
1518.727215	184.166221	48.587533
1515.098459	200.507104	48.592538
1511.437818	176.253848	48.597543
1508.084585	164.963788	48.602548
1504.698308	184.903584	48.607553
1501.399003	182.191576	48.612557
1497.378843	181.885897	48.617562
1493.837303	166.812185	48.622567
1490.671080	184.750494	48.627572
1486.737279	198.257049	48.632577
1483.764577	178.093398	48.637581
1479.697455	179.262875	48.642586
1476.314797	181.114895	48.647591
1472.986783	179.036228	48.652596
1469.031309	167.896286	48.657601
1466.194420	172.573396	48.662605
1463.085660	192.205500	48.667610
1459.272390	181.361115	48.672615
1455.505901	171.916535	48.677620
1451.776011	181.226377	48.682625
1448.447674	171.787422	48.687629
1444.816569	173.210695	48.692634
1441.256580	190.921716	48.697639
1438.207639	179.431620	48.702644
1434.313194	165.960533	48.707649
1430.807742	173.660588	48.712653
1427.378393	183.473863	48.717658
1423.948522	187.332415	48.722663
1420.877287	174.317158	48.727668
1416.763941	156.211518	48.732673
1413.948901	166.148120	48.737677
1410.245031	179.927286	48.742682
1406.334843	176.575893	48.747687
1402.767333	175.595088	48.752692
1399.086658	172.371549	48.757697
1395.901545	182.402490	48.762701
1392.385269	185.900355	48.767706
1388.741674	183.087982	48.772711
1385.383591	189.015493	48.777716
1381.899926	175.694057	48.782721
1378.571538	159.523102	48.787725
1374.806418	175.362791	48.792730
1371.198898	191.843348	48.797735
1367.952619	169.326795	48.802740
1364.505334	181.729709	48.807745
1360.926059	181.321844	48.812749
1357.762926	161.408135	48.817754
1354.011101	170.963618	48.822759
1350.591806	180.800022	48.827764
1346.814754	168.444074	48.832769
1343.734344	173.428068	48.837773
1339.824362	175.181630	48.842778
1336.376039	161.242882	48.847783
1332.771006	154.682753	48.852788
1329.220086	181.724024	48.857793
1325.571449	167.010805	48.862797
1322.094458	167.795013	48.867802
1318.620750	155.903081	48.872807
1315.574070	165.797547	48.877812
1311.968769	189.085370	48.882817
1308.782507	171.170562	48.887821
1305.397229	166.338000	48.892826
1301.379929	167.980068	48.897831
1298.228188	176.739480	48.902836
1294.238037	182.789115	48.907841
1290.694350	165.991621	48.912845
1286.926082	161.714937	48.917850
1283.651543	158.195664	48.922855
1280.488212	164.955715	48.927860
1276.638254	188.800650	48.932865
1273.462955	162.393410	48.937869
1270.003710	152.870033	48.942874
1266.480032	166.096073	48.947879
1262.848111	178.761717	48.952884
1259.199791	159.591870	48.957889
1255.849994	157.205380	48.962893
1252.165017	170.707337	48.967898
1248.622928	171.580555	48.972903
1245.351527	170.804974	48.977908
1241.496989	177.555931	48.982913
1238.398819	170.047136	48.987917
1234.832627	158.547752	48.992922
1231.412827	162.542831	48.997927
1228.034012	171.535566	49.002932
1224.636454	175.082273	49.007937
1220.960479	154.446675	49.012941
1217.243887	162.412899	49.017946
1213.293544	155.200266	49.022951
1210.288043	170.238978	49.027956
1206.271341	174.941262	49.032961
1203.471132	155.027044	49.037965
1200.075518	152.156189	49.042970
1196.317697	161.491655	49.047975
1192.686258	171.886758	49.052980
1189.303940	172.341801	49.057985
1185.484447	158.948688	49.062989
1182.020735	164.974605	49.067994
1178.892642	173.338029	49.072999
1175.692339	173.075750	49.078004
1172.017441	161.510400	49.083009
1168.389490	161.101202	49.088013
1164.573714	167.842243	49.093018
1160.892403	163.690076	49.098023
1157.654565	172.633227	49.103028
1153.977655	184.459451	49.108033
1150.712563	160.120491	49.113037
1147.358046	158.732956	49.118042
1143.396985	171.480795	49.123047
1140.639666	156.339327	49.128052
1136.830142	173.321476	49.133057
1133.445676	154.605554	49.138061
1129.841321	171.164568	49.143066
1126.001952	177.287353	49.148071
1122.253867	159.287470	49.153076
1119.245650	163.242768	49.158081
1115.528273	179.311431	49.163085
1112.378629	185.927342	49.168090
1108.693744	169.380468	49.173095
1105.159563	147.808276	49.178100
1101.618378	168.623093	49.183105
1098.032468	158.534069	49.188109
1094.732614	164.721982	49.193114
1091.019977	169.805122	49.198119
1088.081869	164.373851	49.203124
1084.144191	149.964230	49.208129
1080.852676	140.935428	49.213133
1077.419093	172.709726	49.218138
1073.802196	168.686561	49.223143
1070.312812	160.738850	49.228148
1066.495844	149.095230	49.233153
1063.014769	164.855873	49.238157
1059.733061	168.643170	49.243162
1055.742468	160.476155	49.248167
1052.711775	171.832305	49.253172
1049.236927	168.040904	49.258177
1046.039415	142.508697	49.263181
1041.885283	166.549886	49.268186
1038.550215	174.889923	49.273191
1035.311808	160.677396	49.278196
1031.514350	159.342924	49.283201
1028.028251	161.983756	49.288205
1024.465564	151.268087	49.293210
1021.107272	166.131594	49.298215
1018.007488	166.181192	49.303220
1014.161786	174.403811	49.308225
1010.583148	155.986578	49.313229
1007.130867	159.263145	49.318234
1003.649790	161.450365	49.323239
1000.108473	159.425013	49.328244
996.333972	175.864594	49.333249
993.023328	164.323860	49.338253
989.257101	156.727223	49.343258
985.950970	159.755740	49.348263
982.456621	162.443925	49.353268
979.122668	159.307409	49.358273
976.060311	169.144701	49.363277
972.433606	175.579887	49.368282
968.338149	156.218427	49.373287
964.954657	150.404711	49.378292
961.110798	165.614758	49.383297
957.723882	160.300666	49.388301
954.397254	163.961856	49.393306
950.768720	142.684441	49.398311
947.820106	154.220705	49.403316
944.129678	162.206410	49.408321
940.557641	150.404058	49.413325
937.198576	168.050278	49.418330
933.274168	182.403184	49.423335
930.277533	157.299543	49.428340
926.720569	149.902291	49.433345
923.332123	160.918022	49.438349
919.718122	165.003217	49.443354
915.977445	158.969427	49.448359
912.346433	170.431057	49.453364
908.955445	166.287823	49.458369
905.441983	142.283661	49.463373
902.107118	159.440935	49.468378
898.247393	167.207702	49.473383
895.011357	151.553243	49.478388
891.525187	152.291436	49.483393
888.124527	159.558613	49.488397
884.400370	144.766254	49.493402
880.857026	147.682167	49.498407
877.724533	148.855205	49.503412
873.824787	164.612835	49.508417
870.599206	150.819135	49.513421
866.958966	138.993871	49.518426
863.615940	147.786493	49.523431
860.322392	165.183385	49.528436
856.420864	138.314794	49.533441
852.849477	154.880974	49.538445
849.184068	154.622752	49.543450
845.298740	152.543410	49.548455
842.702663	156.026899	49.553460
838.864358	160.923949	49.558465
835.611250	152.257391	49.563469
832.013164	141.222951	49.568474
828.451427	168.313943	49.573479
824.734738	173.662557	49.578484
821.313539	166.824865	49.583489
818.201378	151.161148	49.588493
814.648869	160.039488	49.593498
810.583428	149.093477	49.598503
807.129156	152.346989	49.603508
803.967967	160.161316	49.608513
800.606556	167.657327	49.613517
796.979756	159.498778	49.618522
793.236902	150.625167	49.623527
789.867029	147.186018	49.628532
786.432594	158.549827	49.633537
782.396099	147.743873	49.638541
779.411241	161.670786	49.643546
775.706436	172.250914	49.648551
772.664148	153.674161	49.653556
768.929599	144.879596	49.658561
765.422546	156.671993	49.663565
761.887384	160.141311	49.668570
758.569355	141.955779	49.673575
755.149319	153.770801	49.678580
751.042294	155.793786	49.683585
747.909999	137.405653	49.688589
744.324524	149.787597	49.693594
740.487898	167.440731	49.698599
737.414048	172.754648	49.703604
733.574342	153.758071	49.708609
730.516205	148.121298	49.713613
726.900753	152.247171	49.718618
722.999009	167.129009	49.723623
719.653443	160.031679	49.728628
715.963146	147.982857	49.733633
712.912326	137.983686	49.738637
709.622448	146.245649	49.743642
705.960086	164.365716	49.748647
702.826350	141.051587	49.753652
699.093677	151.731335	49.758657
695.452403	142.563720	49.763661
691.650149	146.327055	49.768666
687.900720	149.881907	49.773671
684.793106	147.780664	49.778676
681.229404	143.728827	49.783681
677.825445	140.855193	49.788685
674.096856	141.025275	49.793690
670.284913	148.149755	49.798695
667.423072	139.255718	49.803700
663.899280	161.858333	49.808705
660.350728	157.147108	49.813709
657.121610	131.770575	49.818714
653.271609	143.730723	49.823719
649.815902	154.677564	49.828724
645.902703	147.360332	49.833729
642.919997	163.321140	49.838733
639.368937	158.569797	49.843738
635.477260	144.331569	49.848743
632.409763	146.674202	49.853748
628.763100	143.302459	49.858753
625.074281	148.612628	49.863757
621.409875	152.961691	49.868762
618.139067	153.543021	49.873767
614.483650	142.408596	49.878772
611.298067	146.143319	49.883777
608.002056	151.697485	49.888781
604.588327	137.269271	49.893786
601.063525	142.970921	49.898791
597.570637	145.946808	49.903796
593.438652	158.083387	49.908801
589.929180	145.228039	49.913805
586.543748	130.939392	49.918810
582.856420	153.299821	49.923815
579.763118	131.883701	49.928820
576.082957	141.679923	49.933825
572.875072	145.978959	49.938829
569.345096	143.989559	49.943834
565.607012	152.620866	49.948839
562.210672	145.164264	49.953844
558.272605	145.995519	49.958849
555.335047	157.359622	49.963853
551.692999	148.973314	49.968858
548.192038	134.120668	49.973863
544.882808	141.654029	49.978868
541.326592	149.362450	49.983873
537.549249	142.285947	49.988877
534.169905	149.009364	49.993882
530.596647	149.225192	49.998887
527.127430	129.063555	50.003892
523.872623	136.135636	50.008897
520.520729	149.736842	50.013901
516.529955	152.881425	50.018906
512.740815	125.410703	50.023911
509.288407	130.949307	50.028916
506.086878	152.484435	50.033921
502.470496	152.760276	50.038925
499.025908	137.790133	50.043930
495.471635	141.419685	50.048935
492.501041	141.979997	50.053940
488.638283	158.617623	50.058945
485.031840	154.159132	50.063949
481.688622	145.822059	50.068954
477.873491	137.913635	50.073959
474.226831	157.891767	50.078964
471.042329	154.929119	50.083969
467.696201	139.721565	50.088973
464.232077	146.758903	50.093978
460.586337	155.688607	50.098983
457.266251	149.697797	50.103988
453.343394	136.552449	50.108993
450.075751	162.457938	50.113997
446.410053	149.073303	50.119002
442.952461	145.418198	50.124007
439.748108	139.139867	50.129012
435.983295	156.324805	50.134017
432.720465	138.762420	50.139021
429.433488	132.420802	50.144026
425.732433	144.773432	50.149031
421.827671	142.291630	50.154036
418.238342	160.777650	50.159041
414.822693	157.996055	50.164045
411.814987	133.796097	50.169050
408.075097	146.001953	50.174055
404.485137	147.785645	50.179060
400.882837	141.643211	50.184065
397.333433	141.443419	50.189069
394.083908	138.296629	50.194074
390.317839	147.527087	50.199079
387.191838	160.416289	50.204084
383.628468	163.234355	50.209089
379.727900	138.397271	50.214093
376.463325	129.265108	50.219098
372.783776	149.495612	50.224103
369.488657	138.981317	50.229108
365.846353	154.386476	50.234113
362.465812	147.851214	50.239117
359.222371	145.610299	50.244122
355.261443	132.882675	50.249127
352.176000	147.386835	50.254132
348.489449	161.246416	50.259137
345.136474	158.115357	50.264141
341.561724	139.326691	50.269146
337.827811	143.190694	50.274151
334.609710	153.515307	50.279156
330.939980	151.101370	50.284161
327.307271	139.283813	50.289165
323.960713	143.863239	50.294170
320.234775	147.586349	50.299175
316.975654	131.588082	50.304180
313.488098	150.241684	50.309185
309.789838	140.857245	50.314189
306.465251	134.905153	50.319194
302.716214	148.442329	50.324199
299.659314	135.048876	50.329204
295.574941	136.407756	50.334209
292.226439	132.550643	50.339213
289.026562	143.438589	50.344218
285.462693	147.383532	50.349223
281.973569	136.423599	50.354228
278.535673	136.266808	50.359233
274.786248	148.438196	50.364237
271.474223	128.965282	50.369242
267.940205	148.706362	50.374247
264.756467	139.026929	50.379252
260.709665	131.594627	50.384257
257.465005	139.881069	50.389261
253.792591	132.845920	50.394266
250.353231	137.525154	50.399271
247.237849	135.944891	50.404276
243.299630	148.888027	50.409281
239.727982	128.474620	50.414285
236.458218	124.539228	50.419290
232.619200	136.621257	50.424295
229.248081	156.747791	50.429300
225.787678	137.442551	50.434305
222.326153	128.581254	50.439309
219.019715	124.900890	50.444314
214.886411	150.383428	50.449319
211.822672	136.305267	50.454324
208.350137	128.084240	50.459329
204.677858	143.076439	50.464333
201.378843	131.868228	50.469338
198.093579	131.263660	50.474343
194.261121	139.349038	50.479348
190.873095	131.709884	50.484353
187.036250	120.465347	50.489357
183.852104	118.014776	50.494362
180.058149	141.800947	50.499367
177.108787	134.296084	50.504372
173.128328	133.265910	50.509377
169.798068	141.546507	50.514381
166.110372	121.998114	50.519386
162.706316	137.098736	50.524391
159.546690	122.967781	50.529396
156.028767	125.182034	50.534401
152.274084	127.330253	50.539405
148.836036	118.896117	50.544410
145.114640	135.433660	50.549415
141.986895	120.971842	50.554420
138.479608	127.284498	50.559425
134.544437	137.493082	50.564429
131.110169	128.671139	50.569434
127.460763	123.675150	50.574439
124.301734	122.901792	50.579444
120.699334	140.892187	50.584449
117.232652	125.344648	50.589453
113.877185	125.525411	50.594458
110.089831	128.080445	50.599463
107.049338	113.456665	50.604468
103.316572	123.033915	50.609473
99.756142	143.949359	50.614477
96.721700	127.470309	50.619482
92.732830	113.112156	50.624487
89.319196	122.894343	50.629492
85.919791	131.995398	50.634497
82.202631	127.578442	50.639501
78.557753	134.894807	50.644506
74.409070	140.891179	50.649511
71.096741	127.488788	50.654516
68.159453	117.025462	50.659521
64.539493	119.320843	50.664525
61.442706	123.165927	50.669530
57.845857	131.885602	50.674535
54.496678	122.402628	50.679540
50.870749	140.894016	50.684545
47.051858	124.024862	50.689549
43.617234	127.378687	50.694554
40.321633	130.764981	50.699559
36.611392	117.702615	50.704564
32.790894	138.903821	50.709569
29.758481	150.249736	50.714573
26.005938	126.869210	50.719578
22.448488	120.484834	50.724583
19.131841	121.559282	50.729588
15.706166	144.480166	50.734593
12.366639	137.932424	50.739597
9.169601	116.856155	50.744602
5.343516	113.594844	50.749607
1.839440	119.322552	50.754612