Wed Jun 15 16:26:45 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
0.221278	110.866657	0.000000
0.317961	116.843526	0.005005
0.202752	108.465275	0.010010
0.122283	76.837677	0.015014
0.008725	59.569589	0.020019
-1.040846	51.170977	0.025024
-1.245729	44.822523	0.030029
-1.549758	39.521503	0.035034
-1.492637	25.262851	0.040038
-1.953092	32.093796	0.045043
-2.160815	7.690591	0.050048
-1.970872	19.299576	0.055053
-2.614045	1.757637	0.060058
-2.846900	-2.134239	0.065062
-3.278729	2.855675	0.070067
-3.852390	13.838475	0.075072
-4.070473	0.025926	0.080077
-4.398403	-10.578951	0.085082
-4.782075	-13.705860	0.090086
-4.679327	1.604101	0.095091
-5.012855	-20.639531	0.100096
-5.788701	-8.034648	0.105101
-6.253580	-8.537385	0.110106
-6.342217	-8.297844	0.115110
-6.317075	-21.060436	0.120115
-6.350903	-11.233321	0.125120
-6.219204	-22.540644	0.130125
-6.599094	-13.823515	0.135130
-6.664685	-6.339405	0.140134
-7.423403	-0.507983	0.145139
-7.561717	-18.909176	0.150144
-7.894029	-15.197686	0.155149
-7.836894	7.892399	0.160154
-8.718602	-6.903468	0.165158
-9.002331	-16.748281	0.170163
-9.008778	-15.187648	0.175168
-9.069765	-9.566925	0.180173
-9.349818	2.488551	0.185178
-9.321217	-10.404932	0.190182
-9.598844	-2.982255	0.195187
-10.401086	-3.373603	0.200192
-10.518906	-21.199426	0.205197
-11.166348	8.023287	0.210202
-10.850948	-0.543157	0.215206
-10.894425	-17.618147	0.220211
-11.015585	-1.955916	0.225216
-11.369713	-12.452390	0.230221
-12.210719	5.337034	0.235226
-12.033600	11.763809	0.240230
-12.461636	10.403079	0.245235
-12.514056	-11.646916	0.250240
-12.591591	-12.252727	0.255245
-13.511499	13.620531	0.260250
-13.635479	-7.004939	0.265254
-14.245048	-7.999779	0.270259
-14.256518	5.643800	0.275264
-13.806833	-10.277357	0.280269
-14.322400	0.256169	0.285274
-14.024792	-11.385071	0.290278
-14.871905	0.984884	0.295283
-15.275052	7.279482	0.300288
-15.325932	-28.919780	0.305293
-15.794709	-10.381022	0.310298
-15.318407	-4.672908	0.315302
-16.379396	11.720444	0.320307
-17.070221	-1.888104	0.325312
-17.171660	-18.654518	0.330317
-17.309685	-11.288258	0.335322
-16.997977	4.566616	0.340326
-17.661181	11.714862	0.345331
-17.711787	-8.290807	0.350336
-17.558185	-7.762611	0.355341
-17.602061	-5.704931	0.360346
-18.139581	8.085659	0.365350
-18.759365	11.734279	0.370355
-19.142771	12.086160	0.375360
-19.211633	-11.557894	0.380365
-19.309683	6.467130	0.385370
-19.522417	3.744727	0.390374
-20.060781	-1.938866	0.395379
-20.640355	-2.031419	0.400384
-20.693976	6.488470	0.405389
-20.867720	14.638269	0.410394
-20.429688	1.016486	0.415398
-20.610083	1.358591	0.420403
-21.202045	5.664919	0.425408
-21.504285	-16.663591	0.430413
-21.929635	-19.821293	0.435418
-21.968780	-4.489470	0.440422
-22.295487	16.003586	0.445427
-23.106848	4.289024	0.450432
-23.288608	-10.863203	0.455437
-24.172253	11.895047	0.460442
-23.689338	-10.018505	0.465446
-23.422267	6.059089	0.470451
-23.665792	5.602635	0.475456
-23.743885	-15.550859	0.480461
-24.099466	-5.598953	0.485466
-24.821348	0.431269	0.490470
-25.183777	11.500000	0.495475
-25.451809	-3.561823	0.500480
-25.420165	-18.833059	0.505485
-25.698276	-2.334027	0.510490
-25.771127	6.579281	0.515494
-25.886674	-12.117571	0.520499
-26.869920	-1.313313	0.525504
-26.952718	-1.919734	0.530509
-27.443320	-7.752872	0.535514
-27.329775	-12.338549	0.540518
-27.586480	5.266912	0.545523
-27.693458	-1.501160	0.550528
-27.235163	-10.079474	0.555533
-27.958953	-7.526392	0.560538
-28.304529	-8.569296	0.565542
-28.900239	-18.024587	0.570547
-29.082049	-1.792523	0.575552
-28.968555	-7.899012	0.580557
-29.241466	-5.018954	0.585562
-29.219741	-23.466412	0.590566
-30.141938	-14.428240	0.595571
-30.096336	7.277478	0.600576
-30.228771	-2.752840	0.605581
-30.708269	-12.621527	0.610586
-31.357829	-2.431340	0.615590
-31.931942	-4.992019	0.620595
-31.881653	2.905702	0.625600
-31.520846	-5.212500	0.630605
-32.027002	-7.579226	0.635610
-32.136034	3.461432	0.640614
-32.283547	-18.533079	0.645619
-32.604559	-5.043145	0.650624
-32.563365	-14.344058	0.655629
-33.422563	-5.240335	0.660634
-33.606026	-15.240114	0.665638
-33.806201	3.595483	0.670643
-34.063688	-6.663147	0.675648
-33.872130	-17.677521	0.680653
-34.284549	-4.930671	0.685658
-35.046052	-3.314702	0.690662
-35.313427	-4.018464	0.695667
-35.379896	2.896115	0.700672
-35.371107	-18.945282	0.705677
-35.902851	3.423449	0.710682
-35.570315	10.980959	0.715686
-35.906736	-5.825548	0.720691
-36.150745	-12.866412	0.725696
-36.419551	-9.483350	0.730701
-36.641206	1.983128	0.735706
-36.879446	1.851332	0.740710
-37.569125	-4.103484	0.745715
-38.161295	-8.014003	0.750720
-37.931643	-6.813578	0.755725
-38.632598	18.376583	0.760730
-38.327637	-10.538035	0.765734
-38.286075	1.956036	0.770739
-39.195056	7.970227	0.775744
-39.513173	-10.369589	0.780749
-39.997667	13.878239	0.785754
-40.218594	9.877164	0.790758
-40.242167	-3.809292	0.795763
-40.219930	0.279129	0.800768
-40.340343	10.049440	0.805773
-40.202607	17.979079	0.810778
-40.392791	-11.525287	0.815782
-40.984622	-11.143597	0.820787
-41.580823	0.332594	0.825792
-41.367556	16.452035	0.830797
-41.635632	9.481922	0.835802
-42.325225	-1.043556	0.840806
-43.146816	8.956568	0.845811
-43.261279	-14.875454	0.850816
-43.176457	5.839887	0.855821
-43.441130	13.197987	0.860826
-43.229619	-10.498612	0.865830
-43.362955	-3.819895	0.870835
-43.840635	3.733800	0.875840
-44.074041	-6.261380	0.880845
-44.817726	10.258870	0.885850
-44.864494	5.530702	0.890854
-44.739399	-9.226553	0.895859
-44.892663	-14.505215	0.900864
-45.251553	-0.112725	0.905869
-46.177309	24.989021	0.910874
-46.268437	18.176398	0.915878
-46.280133	-2.645485	0.920883
-46.540888	-6.645201	0.925888
-46.742888	-2.266796	0.930893
-46.872994	11.019169	0.935898
-46.851251	0.206759	0.940902
-47.661676	6.415665	0.945907
-48.299885	-0.813970	0.950912
-48.211670	-6.639382	0.955917
-48.654309	1.810930	0.960922
-48.255144	3.540097	0.965926
-47.961808	-1.716097	0.970931
-48.709755	3.403103	0.975936
-49.269697	5.329642	0.980941
-49.773385	6.968013	0.985946
-49.856889	3.616401	0.990950
-50.106773	-7.905159	0.995955
-49.963352	3.214616	1.000960
-50.190204	-1.050043	1.005965
-51.082687	-20.255731	1.010970
-51.427305	-10.223074	1.015974
-51.463331	5.500059	1.020979
-51.583995	6.720400	1.025984
-51.493783	-5.965453	1.030989
-51.586494	1.441856	1.035994
-52.163996	-4.500226	1.040998
-52.728329	-12.509625	1.046003
-53.353020	5.472314	1.051008
-52.851720	-4.823230	1.056013
-53.304852	0.702891	1.061018
-53.267954	6.525447	1.066022
-53.562036	-13.063735	1.071027
-54.500767	-13.899509	1.076032
-54.590875	-8.837636	1.081037
-54.827315	14.207152	1.086042
-54.790338	3.941877	1.091046
-54.771198	-13.464549	1.096051
-55.024070	-0.328668	1.101056
-54.917898	-10.375130	1.106061
-55.835386	-10.495289	1.111066
-56.311171	-7.355903	1.116070
-56.121027	-3.173307	1.121075
-56.549138	1.498650	1.126080
-56.249158	5.312412	1.131085
-57.324027	-7.648670	1.136090
-57.765254	-9.922348	1.141094
-57.826144	1.963436	1.146099
-58.045296	7.441519	1.151104
-58.022275	-11.055781	1.156109
-58.082714	-5.920585	1.161114
-58.192649	-8.495727	1.166118
-58.086601	-5.264085	1.171123
-59.138969	9.329729	1.176128
-59.599443	-5.925586	1.181133
-59.752179	-10.707359	1.186138
-59.656592	-4.719509	1.191142
-59.551448	-8.422202	1.196147
-60.040387	-10.564097	1.201152
-60.713755	-17.456956	1.206157
-61.079249	1.244867	1.211162
-60.998711	-8.604408	1.216166
-61.233012	-0.922747	1.221171
-61.686921	1.345930	1.226176
-61.478699	-10.376517	1.231181
-62.270368	-12.043020	1.236186
-62.584491	-0.602598	1.241190
-62.813313	-12.075549	1.246195
-63.116678	13.080656	1.251200
-63.085378	15.886175	1.256205
-63.195273	-4.305502	1.261210
-63.095325	4.650072	1.266214
-63.275975	-7.005940	1.271219
-64.528422	-8.522901	1.276224
-64.499066	-5.007605	1.281229
-64.868111	18.126871	1.286234
-64.733287	5.212966	1.291238
-64.658796	-5.056825	1.296243
-64.672471	-2.120371	1.301248
-65.306285	-2.819899	1.306253
-65.877258	17.500248	1.311258
-65.913315	0.705261	1.316262
-65.975668	-3.069976	1.321267
-66.675669	-5.655419	1.326272
-67.247343	-5.340684	1.331277
-67.611142	5.704000	1.336282
-67.771333	-2.457521	1.341286
-67.673344	6.907362	1.346291
-67.828567	20.594728	1.351296
-67.911162	-2.639847	1.356301
-67.916568	-12.871866	1.361306
-68.053052	2.438164	1.366310
-68.718631	9.975664	1.371315
-69.126280	4.127043	1.376320
-69.113900	10.371711	1.381325
-69.684633	7.037390	1.386330
-69.492089	-14.789687	1.391334
-70.087045	-1.855231	1.396339
-70.873938	-1.435874	1.401344
-70.776175	-16.956261	1.406349
-70.820405	6.732565	1.411354
-71.108446	9.010331	1.416358
-71.197847	-12.850154	1.421363
-71.269551	4.890943	1.426368
-71.465665	-5.991104	1.431373
-72.217358	-1.742522	1.436378
-72.616873	7.557698	1.441382
-72.639519	1.416987	1.446387
-72.861180	-2.684086	1.451392
-72.705889	1.913748	1.456397
-73.023872	-0.245845	1.461402
-73.755572	-18.616232	1.466406
-74.322742	-1.142759	1.471411
-74.517567	9.655008	1.476416
-74.076084	-13.553213	1.481421
-74.314806	-5.849912	1.486426
-74.323637	0.603145	1.491430
-75.105485	-16.809888	1.496435
-75.463466	9.391802	1.501440
-75.813989	-22.002718	1.506445
-75.976547	-0.702874	1.511450
-75.881176	9.429412	1.516454
-76.019575	4.022122	1.521459
-76.024252	1.626381	1.526464
-76.912917	-9.741958	1.531469
-77.360698	-1.688536	1.536474
-77.486288	-6.067389	1.541478
-77.958937	-5.352932	1.546483
-77.718041	1.079667	1.551488
-77.597316	-12.519450	1.556493
-78.175045	-1.696684	1.561498
-78.976996	-12.888669	1.566502
-78.959998	4.558206	1.571507
-79.054908	4.142299	1.576512
-79.389166	-3.672123	1.581517
-79.591641	0.527714	1.586522
-79.339765	-17.662927	1.591526
-79.831372	-14.396042	1.596531
-80.505812	1.527884	1.601536
-80.629891	-15.034628	1.606541
-81.081384	-13.155212	1.611546
-80.995818	1.929409	1.616550
-81.109348	-2.837832	1.621555
-81.886462	-11.411332	1.626560
-82.426833	-5.765738	1.631565
-82.631880	-7.242427	1.636570
-82.614788	-10.374404	1.641574
-82.396163	-21.293317	1.646579
-82.799454	-17.410980	1.651584
-82.732584	9.079365	1.656589
-82.628896	5.964837	1.661594
-83.542024	-14.261376	1.666598
-83.945344	-18.632402	1.671603
-84.274224	-11.911706	1.676608
-84.193069	3.788897	1.681613
-84.541388	-7.927490	1.686618
-84.566323	5.046527	1.691622
-85.329656	-3.630267	1.696627
-85.719176	-14.536077	1.701632
-85.766615	-8.330360	1.706637
-85.971378	10.520594	1.711642
-86.029809	11.670576	1.716646
-85.753913	3.366056	1.721651
-86.769782	-1.641904	1.726656
-87.107495	1.229137	1.731661
-87.320723	5.133435	1.736666
-87.370113	-6.457854	1.741670
-87.416512	2.962257	1.746675
-87.632007	9.343724	1.751680
-87.849674	2.733729	1.756685
-88.440581	-2.502888	1.761690
-88.865169	3.659220	1.766694
-88.748606	3.699913	1.771699
-88.783712	11.651698	1.776704
-88.693215	-12.028539	1.781709
-89.708502	1.264418	1.786714
-90.573778	11.077235	1.791718
-90.620386	3.254138	1.796723
-90.780061	2.327987	1.801728
-90.507407	7.224459	1.806733
-90.971614	-15.011469	1.811738
-90.840331	-6.309176	1.816742
-90.714837	-2.244926	1.821747
-91.246316	-1.728294	1.826752
-92.012460	-3.227271	1.831757
-92.230500	4.784632	1.836762
-92.138527	1.213340	1.841766
-92.358098	-17.189204	1.846771
-93.273835	2.376541	1.851776
-93.773328	-17.144645	1.856781
-93.071625	-14.242479	1.861786
-93.726965	0.278115	1.866790
-93.641913	-10.047375	1.871795
-93.959155	-12.630571	1.876800
-93.930831	-5.325444	1.881805
-94.805835	6.808529	1.886810
-95.096330	-3.094940	1.891814
-95.227173	-8.433336	1.896819
-95.684039	9.308779	1.901824
-95.337807	-11.090254	1.906829
-95.776328	-8.693612	1.911834
-96.203247	3.900962	1.916838
-96.642527	10.324543	1.921843
-96.992907	3.687456	1.926848
-96.828736	-1.692103	1.931853
-97.441954	-9.788708	1.936858
-97.288753	-4.612272	1.941862
-97.107713	-13.523460	1.946867
-97.755036	3.240093	1.951872
-97.818175	1.633019	1.956877
-98.519586	19.901489	1.961882
-98.725770	4.215088	1.966886
-98.729865	-20.449963	1.971891
-99.041907	1.026892	1.976896
-99.090543	0.112181	1.981901
-99.881825	-2.828290	1.986906
-100.032058	-19.007672	1.991910
-100.076562	-1.919184	1.996915
-100.474481	0.485546	2.006912
-100.236973	2.980148	2.016909
-99.385503	2.860920	2.026906
-99.126109	-9.582987	2.036902
-98.982848	-9.727597	2.046899
-97.934133	5.205501	2.056896
-97.826343	-0.011108	2.066893
-96.907320	-3.052899	2.076890
-96.098292	11.292816	2.086886
-95.984774	-3.560232	2.096883
-96.226918	14.448131	2.106880
-95.117661	1.291177	2.116877
-94.682044	1.237319	2.126874
-93.852899	10.690504	2.136870
-93.335018	-11.707583	2.146867
-93.286694	6.050679	2.156864
-92.913151	10.548217	2.166861
-92.010550	-3.053228	2.176858
-91.710834	-6.886155	2.186854
-90.619875	4.209199	2.196851
-90.137359	12.071467	2.206848
-89.877297	4.071583	2.216845
-90.022988	0.279079	2.226842
-89.519414	-2.662443	2.236838
-88.920800	-4.791964	2.246835
-87.758757	-0.354419	2.256832
-87.357734	10.477559	2.266829
-87.206154	-6.732945	2.276826
-86.825143	-5.857323	2.286822
-86.033200	-4.233662	2.296819
-85.646282	-4.631691	2.306816
-84.816131	-0.790298	2.316813
-84.363545	9.929151	2.326810
-84.074239	-6.242219	2.336806
-83.774882	15.104827	2.346803
-82.747476	8.443503	2.356800
-82.669084	2.708160	2.366797
-82.514390	2.204995	2.376794
-81.292570	9.806009	2.386790
-81.257115	-4.081583	2.396787
-80.404229	5.946481	2.406784
-79.526414	1.866396	2.416781
-79.791426	-2.095931	2.426778
-79.474970	-1.528574	2.436774
-78.486024	5.366185	2.446771
-77.884866	2.000015	2.456768
-77.718351	-3.940717	2.466765
-76.760614	7.736105	2.476762
-76.420302	3.815868	2.486758
-76.319753	-15.665552	2.496755
-75.446376	-4.038406	2.506752
-74.581874	6.657018	2.516749
-74.325192	-0.021429	2.526746
-74.484750	9.182294	2.536742
-73.227950	-2.879460	2.546739
-73.125731	3.564869	2.556736
-72.765106	9.801547	2.566733
-72.171998	5.874694	2.576730
-71.574217	13.732139	2.586726
-70.831240	-10.412008	2.596723
-69.946219	9.193890	2.606720
-69.919071	8.535101	2.616717
-69.942628	4.775253	2.626714
-69.133782	5.206614	2.636710
-68.416687	2.388234	2.646707
-67.971701	1.672441	2.656704
-67.624596	1.233582	2.666701
-66.627142	10.048843	2.676698
-66.446355	12.234383	2.686694
-66.455387	-12.255042	2.696691
-65.325207	8.403447	2.706688
-65.014536	1.150804	2.716685
-64.683642	-9.565252	2.726682
-63.620895	5.537106	2.736678
-63.490434	7.565420	2.746675
-63.471635	1.014884	2.756672
-62.389830	3.238589	2.766669
-61.934632	7.853409	2.776666
-61.749562	1.319051	2.786662
-60.753401	-7.356393	2.796659
-60.405903	-1.652300	2.806656
-60.353196	-0.109144	2.816653
-59.187264	17.917009	2.826650
-58.800221	-0.800665	2.836646
-58.691201	-6.886868	2.846643
-58.168432	4.392181	2.856640
-57.417209	8.446836	2.866637
-57.072900	5.564624	2.876634
-56.003756	2.733104	2.886630
-55.662898	7.961526	2.896627
-55.650034	-8.461561	2.906624
-55.538930	5.640270	2.916621
-54.441053	2.773579	2.926618
-53.911576	-7.281228	2.936614
-53.512506	-3.598036	2.946611
-52.579787	-2.726571	2.956608
-52.283605	-1.419221	2.966605
-52.303567	-15.746369	2.976602
-51.517204	-1.585660	2.986598
-50.905632	-9.714450	2.996595
-50.597675	6.370091	3.006592
-49.679844	-5.028193	3.016589
-49.216991	1.150895	3.026586
-49.070161	6.212753	3.036582
-48.852650	4.263952	3.046579
-48.189880	-5.322977	3.056576
-47.550512	3.924723	3.066573
-46.601593	10.677257	3.076570
-45.999893	-4.529580	3.086566
-45.959663	7.609715	3.096563
-45.983558	-0.438852	3.106560
-44.859501	-6.426712	3.116557
-44.879007	10.848323	3.126554
-43.950564	4.842413	3.136550
-43.245864	4.978475	3.146547
-42.973846	2.951427	3.156544
-42.075577	7.505175	3.166541
-41.932910	-0.940029	3.176538
-41.390956	-9.056425	3.186534
-41.103747	6.515266	3.196531
-40.245578	-2.984047	3.206528
-39.995130	-4.618071	3.216525
-39.504969	11.708582	3.226522
-38.912264	-7.738924	3.236518
-38.618039	-5.349204	3.246515
-38.197476	4.195218	3.256512
-37.090540	-9.668548	3.266509
-36.594176	5.267947	3.276506
-36.847842	-8.633600	3.286502
-35.788714	-6.967760	3.296499
-35.059275	-9.088970	3.306496
-35.209134	-0.563440	3.316493
-34.779245	-6.094828	3.326490
-33.752797	-8.296926	3.336486
-33.340905	5.131060	3.346483
-32.929965	-14.212913	3.356480
-32.298131	-2.414865	3.366477
-32.028655	0.076532	3.376474
-31.489839	-16.989555	3.386470
-30.582993	6.640463	3.396467
-30.593749	-3.733194	3.406464
-29.873376	-1.037676	3.416461
-28.943766	3.144548	3.426458
-28.936849	5.326524	3.436454
-28.986558	-2.948805	3.446451
-27.787076	-16.237994	3.456448
-26.947385	5.879667	3.466445
-26.650448	4.831282	3.476442
-26.725286	-9.821249	3.486438
-25.960640	-11.501234	3.496435
-25.451647	-5.417578	3.506432
-25.353783	-8.000277	3.516429
-24.055753	-2.352715	3.526426
-23.731249	-7.744308	3.536422
-23.480364	0.869673	3.546419
-22.774559	-5.015778	3.556416
-22.054772	6.614153	3.566413
-21.964936	-0.750646	3.576410
-21.849649	2.890752	3.586406
-20.558848	9.299070	3.596403
-20.225554	-0.766485	3.606400
-20.102416	2.814056	3.616397
-19.138843	-0.888367	3.626394
-18.797853	-1.823628	3.636390
-18.589654	-10.072436	3.646387
-17.939511	-10.584386	3.656384
-17.159913	2.878348	3.666381
-17.163682	1.425702	3.676378
-16.285535	-5.539953	3.686374
-15.696207	6.472748	3.696371
-15.465186	0.109572	3.706368
-15.111220	0.952531	3.716365
-13.867197	-0.039711	3.726362
-13.844370	0.745074	3.736358
-13.658395	0.592419	3.746355
-12.902395	-0.690753	3.756352
-12.343362	9.268649	3.766349
-12.212396	-7.637402	3.776346
-11.062200	5.318038	3.786342
-10.836163	2.036382	3.796339
-10.521989	-0.778522	3.806336
-9.584055	5.344780	3.816333
-9.253861	-5.110014	3.826330
-9.017244	-10.024041	3.836326
-8.252606	1.860421	3.846323
-7.376658	1.175740	3.856320
-7.166816	-3.785521	3.866317
-7.166415	-1.643459	3.876314
-6.712758	-14.614913	3.886310
-5.883040	9.981804	3.896307
-5.200307	-6.571649	3.906304
-4.621518	7.076780	3.916301
-4.513565	2.339282	3.926298
-4.180353	10.993695	3.936294
-3.592220	16.886494	3.946291
-3.163705	29.869954	3.956288
-2.527911	49.909635	3.966285
-2.474962	39.280462	3.976282
-1.987194	59.719558	3.986278
-1.207793	88.626156	3.996275
-0.945142	99.296276	4.006272
-0.463936	126.167432	4.016269
0.000000	136.145458	4.021274
-0.077115	138.088301	4.026278
0.360876	152.716214	4.031283
0.156778	177.439837	4.036288
0.485636	169.276389	4.041293
0.433102	187.639692	4.046298
0.241090	191.174947	4.051302
0.920824	186.431523	4.056307
0.887717	200.596059	4.061312
1.048864	209.521819	4.066317
0.901296	202.895112	4.071322
1.034723	222.518300	4.076326
1.390625	226.088397	4.081331
0.947684	219.149743	4.086336
1.179049	198.668679	4.091341
0.893322	205.879915	4.096346
0.972132	210.508608	4.101350
0.938420	216.325752	4.106355
0.986244	213.279798	4.111360
1.067758	196.241719	4.116365
0.990596	206.559900	4.121370
1.242741	239.563898	4.126374
1.111445	214.352833	4.131379
1.102381	197.836273	4.136384
0.992709	209.816603	4.141389
0.870682	224.225308	4.146394
1.033851	230.727876	4.151398
1.053249	215.809017	4.156403
0.955828	206.031917	4.161408
1.240350	208.826998	4.166413
1.003654	235.663176	4.171418
0.871551	227.007297	4.176422
1.244414	231.391588	4.181427
1.183832	228.087827	4.186432
1.109083	201.210069	4.191437
1.277485	218.629717	4.196442
1.156547	213.818841	4.201446
1.257924	198.949387	4.206451
1.113772	225.159728	4.211456
1.180717	228.918051	4.216461
1.269717	222.260430	4.221466
1.060631	226.747597	4.226470
1.440277	244.813623	4.231475
1.609215	266.852097	4.236480
1.681845	249.860114	4.241485
1.773847	222.681903	4.246490
1.019736	230.740199	4.251494
1.206930	211.062698	4.256499
1.308592	226.745655	4.261504
1.523167	253.108163	4.266509
1.693434	249.495067	4.271514
1.175328	242.723108	4.276518
1.503345	242.545673	4.281523
1.349898	256.964533	4.286528
1.449217	242.657075	4.291533
1.558831	251.084526	4.296538
1.641453	259.200179	4.301542
1.652266	247.386251	4.306547
1.416610	239.744505	4.311552
1.598417	250.269201	4.316557
1.667522	252.353721	4.321562
1.550757	254.955979	4.326566
1.604264	273.006584	4.331571
1.413389	270.346121	4.336576
1.523897	248.988060	4.341581
1.649617	238.123274	4.346586
1.439742	256.583466	4.351590
1.518119	257.714804	4.356595
1.263099	245.871907	4.361600
1.589185	258.840821	4.366605
1.630692	259.935538	4.371610
1.272664	238.378017	4.376614
1.855344	258.030391	4.381619
1.448274	264.459704	4.386624
1.713129	249.778040	4.391629
1.644963	265.952252	4.396634
1.862991	283.248355	4.401638
1.740799	256.380017	4.406643
1.694331	269.065734	4.411648
1.819878	285.933999	4.416653
2.100758	278.278590	4.421658
1.628103	279.622031	4.426662
1.902490	278.927568	4.431667
2.029029	291.099466	4.436672
2.132685	275.972190	4.441677
1.707887	270.289749	4.446682
1.478815	257.462494	4.451686
1.869966	284.611887	4.456691
1.744005	298.271788	4.461696
1.822093	281.953517	4.466701
2.248563	274.436029	4.471706
1.909945	299.811918	4.476710
2.397147	291.635482	4.481715
2.413428	289.106213	4.486720
2.286072	284.117232	4.491725
2.071952	273.230354	4.496730
2.046221	256.412355	4.501734
1.915108	238.907449	4.506739
1.862972	254.112257	4.511744
1.689496	265.336784	4.516749
1.965400	262.983317	4.521754
1.924826	275.043528	4.526758
2.224755	289.634608	4.531763
2.103725	303.809725	4.536768
2.116643	295.513974	4.541773
2.157092	283.518246	4.546778
2.113617	293.584991	4.551782
2.294082	278.993992	4.556787
2.064064	286.445539	4.561792
2.339755	301.026431	4.566797
2.079378	309.116126	4.571802
2.035792	292.838470	4.576806
2.554818	284.359849	4.581811
2.100852	291.566671	4.586816
2.259784	286.281490	4.591821
2.699611	287.277633	4.596826
2.260771	315.965135	4.601830
2.518044	300.634291	4.606835
2.445692	287.053783	4.611840
2.171420	285.850410	4.616845
2.333413	291.580886	4.621850
2.083944	297.838171	4.626854
2.523030	291.969556	4.631859
2.284736	315.154305	4.636864
2.294834	292.605132	4.641869
2.116897	279.282977	4.646874
1.878301	309.315578	4.651878
2.436106	303.092431	4.656883
2.226208	304.655150	4.661888
2.341301	296.157255	4.666893
2.711707	290.212982	4.671898
2.279569	299.165023	4.676902
2.114466	290.993692	4.681907
2.019966	299.152053	4.686912
2.063751	310.531000	4.691917
2.324662	297.993456	4.696922
2.260550	305.786636	4.701926
2.751182	317.970302	4.706931
2.510095	323.984032	4.711936
2.773183	318.690111	4.716941
2.889286	311.856227	4.721946
2.809166	324.739223	4.726950
2.797732	307.340829	4.731955
2.393879	299.949791	4.736960
2.305536	317.944382	4.741965
2.578944	320.013300	4.746970
2.447304	320.556093	4.751974
2.816631	327.747326	4.756979
2.749920	316.798768	4.761984
2.530449	313.700095	4.766989
2.616273	324.313900	4.771994
2.775824	320.647217	4.776998
2.836771	328.065103	4.782003
2.338525	341.666905	4.787008
2.513574	334.324605	4.792013
2.519492	311.400049	4.797018
2.596335	328.592773	4.802022
2.627266	325.906792	4.807027
2.531193	323.350312	4.812032
2.367156	326.661582	4.817037
2.778400	343.813168	4.822042
2.837276	359.159742	4.827046
2.909835	345.151371	4.832051
3.028518	351.977014	4.837056
2.876835	364.040761	4.842061
3.001371	357.526464	4.847066
2.626194	334.474757	4.852070
2.529805	342.939853	4.857075
2.936395	358.837425	4.862080
2.829272	354.176829	4.867085
2.841321	360.615051	4.872090
2.765235	369.621639	4.877094
3.053194	358.907819	4.882099
2.636477	367.172142	4.887104
2.714340	352.153423	4.892109
2.960272	350.811992	4.897114
2.744420	367.145469	4.902118
2.877601	344.976981	4.907123
2.770595	353.874633	4.912128
3.237553	365.833189	4.917133
3.068771	363.874983	4.922138
2.759275	366.526570	4.927142
3.173466	357.812004	4.932147
3.175834	378.598407	4.937152
3.380480	393.176132	4.942157
3.149644	360.338117	4.947162
2.903440	376.978877	4.952166
3.418597	375.324927	4.957171
3.109004	375.248025	4.962176
3.043618	375.069408	4.967181
3.389484	385.866778	4.972186
3.119468	382.364587	4.977190
3.514841	375.969872	4.982195
3.154851	383.572272	4.987200
2.749029	383.953710	4.992205
3.054494	385.367347	4.997210
2.872091	378.172090	5.002214
2.887393	394.375457	5.007219
3.113467	387.984447	5.012224
3.315596	388.167361	5.017229
3.802649	390.124629	5.022234
3.491486	389.870914	5.027238
3.692750	367.406148	5.032243
3.430074	381.532435	5.037248
3.152268	393.347245	5.042253
3.405437	384.235778	5.047258
3.161865	401.041267	5.052262
3.638838	389.521802	5.057267
3.627192	396.085587	5.062272
3.238686	399.935988	5.067277
3.385682	391.974839	5.072282
3.171502	377.662636	5.077286
3.409727	393.749554	5.082291
3.238708	400.290847	5.087296
3.252956	403.397175	5.092301
3.437157	376.120197	5.097306
3.265570	386.076676	5.102310
3.414569	420.761022	5.107315
3.469619	428.488996	5.112320
3.329376	425.134630	5.117325
3.591279	414.609649	5.122330
3.591040	432.320110	5.127334
3.415049	412.213467	5.132339
3.449955	428.741439	5.137344
3.599893	440.600425	5.142349
3.539365	422.838897	5.147354
3.282456	424.393515	5.152358
3.133539	416.294908	5.157363
3.560361	419.109226	5.162368
3.495972	414.545427	5.167373
3.625182	432.573550	5.172378
3.432070	439.048767	5.177382
3.837456	437.288061	5.182387
3.757029	449.358152	5.187392
3.768497	450.607398	5.192397
3.940649	439.030052	5.197402
3.782253	451.681344	5.202406
4.003763	454.762507	5.207411
4.035573	440.203123	5.212416
3.641154	435.443487	5.217421
3.585024	424.754423	5.222426
3.671200	417.585889	5.227430
4.098859	436.383872	5.232435
3.647755	463.204485	5.237440
3.770919	462.922892	5.242445
4.319769	439.291671	5.247450
3.917521	431.059326	5.252454
3.959519	448.661810	5.257459
4.030856	439.698145	5.262464
3.698775	438.235101	5.267469
4.068014	453.550407	5.272474
3.945696	462.008706	5.277478
4.076872	450.865074	5.282483
4.062448	461.316494	5.287488
3.855911	452.354251	5.292493
4.435628	442.968009	5.297498
3.981591	453.787327	5.302502
3.874819	444.121712	5.307507
3.727246	429.193344	5.312512
3.703562	451.119495	5.317517
4.127172	461.997985	5.322522
4.037501	458.365352	5.327526
3.799525	443.691724	5.332531
3.831786	466.463342	5.337536
3.899242	459.546970	5.342541
4.108857	449.985030	5.347546
3.844404	467.440980	5.352550
3.841655	451.898639	5.357555
4.022767	460.925912	5.362560
4.248150	476.668093	5.367565
4.236867	473.097574	5.372570
4.246341	478.645670	5.377574
3.980040	473.665185	5.382579
4.342984	497.242418	5.387584
4.075825	496.756115	5.392589
4.429179	499.406008	5.397594
4.417210	505.499042	5.402598
4.541879	497.826229	5.407603
4.631143	480.228497	5.412608
4.038487	461.497050	5.417613
4.220478	465.039813	5.422618
4.127799	474.908829	5.427622
4.308477	468.303525	5.432627
4.581354	482.362316	5.437632
4.339450	494.721040	5.442637
4.487463	488.733735	5.447642
4.213455	511.403719	5.452646
4.306096	494.119314	5.457651
4.705664	490.317631	5.462656
4.420369	487.920144	5.467661
4.503331	501.913464	5.472666
4.463719	496.224303	5.477670
4.743695	491.861046	5.482675
4.440897	508.317851	5.487680
4.449969	495.308099	5.492685
4.736014	475.039590	5.497690
4.598960	481.228160	5.502694
4.531873	482.348040	5.507699
4.282958	483.608652	5.512704
4.170672	490.920885	5.517709
4.422332	496.557899	5.522714
4.415649	500.072660	5.527718
4.473193	486.772078	5.532723
4.495459	492.744623	5.537728
4.664855	495.246263	5.542733
4.670297	496.362444	5.547738
4.469939	503.272447	5.552742
4.549714	510.593298	5.557747
4.759967	501.344628	5.562752
4.418329	482.414921	5.567757
4.596013	474.595645	5.572762
4.337717	502.527506	5.577766
4.559367	508.912803	5.582771
4.801372	497.233902	5.587776
4.525203	498.898152	5.592781
4.858130	525.791539	5.597786
4.979113	524.024059	5.602790
4.864748	513.721692	5.607795
4.691882	521.143586	5.612800
4.709746	524.840546	5.617805
4.955495	508.767881	5.622810
4.692207	518.067701	5.627814
4.721966	536.005051	5.632819
4.937921	531.213769	5.637824
4.817716	531.038684	5.642829
4.904171	527.601454	5.647834
4.529088	519.734999	5.652838
4.569665	520.642653	5.657843
4.671581	528.596929	5.662848
4.354364	539.429506	5.667853
4.445882	531.832688	5.672858
4.692898	533.006416	5.677862
4.874739	554.667913	5.682867
5.032796	558.059773	5.687872
4.856444	562.457282	5.692877
5.089130	564.899248	5.697882
4.971335	565.224706	5.702886
5.253854	564.676467	5.707891
5.196699	561.289499	5.712896
4.862514	564.286821	5.717901
5.245388	568.211034	5.722906
5.032927	575.568767	5.727910
5.155163	557.528087	5.732915
5.185029	564.763000	5.737920
5.071870	578.827471	5.742925
5.194635	558.707766	5.747930
5.224277	575.225618	5.752934
5.413371	574.718072	5.757939
5.288043	565.693411	5.762944
5.226150	574.276246	5.767949
5.183410	561.188386	5.772954
4.696370	552.370991	5.777958
5.049955	571.921348	5.782963
5.187511	568.363500	5.787968
5.083035	572.147769	5.792973
5.131862	569.499728	5.797978
5.199066	561.049848	5.802982
5.263108	553.877117	5.807987
5.149113	573.042082	5.812992
5.254901	586.631684	5.817997
5.383623	573.138243	5.823002
5.191715	583.854355	5.828006
5.344763	572.795015	5.833011
5.502949	555.548936	5.838016
5.178708	569.992269	5.843021
5.244349	584.994356	5.848026
5.036122	571.881056	5.853030
5.357769	595.421861	5.858035
5.507534	594.448579	5.863040
5.543606	601.224455	5.868045
5.647657	588.375018	5.873050
5.510281	567.577162	5.878054
5.363801	577.824479	5.883059
5.460849	588.045172	5.888064
5.528995	577.209686	5.893069
5.843107	571.918393	5.898074
5.407576	579.609729	5.903078
5.548996	568.598875	5.908083
5.466993	562.929618	5.913088
5.407823	583.998051	5.918093
5.860376	582.336470	5.923098
5.525931	598.184608	5.928102
5.274502	584.084544	5.933107
5.607428	578.717930	5.938112
5.577354	583.492677	5.943117
5.373892	602.131076	5.948122
5.275168	605.187652	5.953126
5.602315	596.117796	5.958131
5.722489	605.479683	5.963136
5.378857	587.331776	5.968141
5.698743	596.929672	5.973146
5.570496	594.564911	5.978150
5.770071	593.509114	5.983155
5.552444	593.041651	5.988160
5.538210	599.691282	5.993165
5.758010	597.381465	5.998170
5.468759	591.392393	6.003174
5.564855	596.986690	6.008179
5.297781	601.161162	6.013184
5.409707	623.657442	6.018189
5.799053	635.985654	6.023194
5.524490	639.048606	6.028198
5.886247	639.831373	6.033203
6.178400	632.355342	6.038208
6.018683	647.322914	6.043213
6.363084	629.044485	6.048218
5.950372	643.686689	6.053222
5.894327	650.116752	6.058227
6.063034	632.264123	6.063232
5.517680	621.394643	6.068237
5.824280	627.166556	6.073242
5.691874	641.323148	6.078246
5.557136	648.153119	6.083251
5.896283	634.958879	6.088256
5.961756	626.896055	6.093261
5.884949	643.381458	6.098266
5.848214	635.888550	6.103270
6.073440	647.079826	6.108275
6.285402	641.952478	6.113280
6.059913	612.826017	6.118285
5.830833	598.724021	6.123290
5.362312	607.523920	6.128294
5.506215	635.556968	6.133299
6.049410	641.267395	6.138304
5.800861	631.746627	6.143309
6.165386	623.226370	6.148314
5.651873	627.681195	6.153318
5.734087	653.031135	6.158323
5.837138	639.461676	6.163328
5.696967	629.925762	6.168333
5.742018	643.222399	6.173338
5.924583	632.482795	6.178342
5.879894	631.929732	6.183347
6.358121	638.007414	6.188352
5.690262	636.099488	6.193357
6.015804	606.782044	6.198362
5.602533	606.620467	6.203366
5.708383	616.921309	6.208371
5.914164	633.296275	6.213376
5.614231	642.214730	6.218381
6.077173	628.645391	6.223386
6.138233	615.450659	6.228390
5.929189	623.698458	6.233395
5.988890	621.825082	6.238400
5.809405	604.134693	6.243405
5.676206	604.160829	6.248410
5.953222	600.451683	6.253414
5.837312	588.657250	6.258419
5.854546	592.669120	6.263424
5.728695	606.478336	6.268429
5.773844	611.959622	6.273434
5.967039	608.751652	6.278438
5.849374	613.352761	6.283443
5.855323	599.964324	6.288448
5.477936	625.293198	6.293453
5.638200	598.829495	6.298458
5.821370	609.213341	6.303462
5.622797	631.944533	6.308467
5.944010	648.477811	6.313472
5.947969	648.326796	6.318477
6.213501	622.407172	6.323482
6.182887	607.236055	6.328486
5.589405	603.802558	6.333491
5.753353	620.312768	6.338496
5.431223	613.029313	6.343501
5.865083	617.648879	6.348506
6.013697	621.293870	6.353510
5.823810	636.294138	6.358515
5.728223	629.165605	6.363520
5.862226	630.033065	6.368525
6.112167	641.152677	6.373530
5.844699	617.810766	6.378534
5.776140	594.647819	6.383539
6.103224	603.883176	6.388544
5.737019	618.339116	6.393549
5.935946	603.251409	6.398554
5.887825	599.593528	6.403558
5.650138	609.074535	6.408563
5.625117	601.720777	6.413568
5.665261	617.980256	6.418573
6.189031	605.205174	6.423578
5.996736	609.159536	6.428582
5.879921	596.500386	6.433587
5.957926	609.698127	6.438592
5.620306	619.177603	6.443597
5.829242	608.412150	6.448602
5.795103	599.540303	6.453606
5.979104	598.764186	6.458611
6.162175	606.424532	6.463616
5.809570	620.079065	6.468621
5.799142	602.115004	6.473626
5.534562	598.676382	6.478630
5.561840	598.012976	6.483635
5.771418	621.093595	6.488640
5.835515	614.475827	6.493645
6.029007	598.999752	6.498650
5.780320	589.369632	6.503654
5.596709	595.500538	6.508659
5.907618	624.451127	6.513664
5.752487	630.873486	6.518669
5.684771	616.016182	6.523674
5.854857	629.295400	6.528678
5.863998	648.444452	6.533683
5.905609	642.037060	6.538688
5.542519	638.995791	6.543693
5.665630	645.503380	6.548698
5.661577	645.672722	6.553702
5.846150	633.487763	6.558707
6.199625	651.931886	6.563712
5.692515	649.240947	6.568717
6.017300	625.543280	6.573722
5.827436	629.967409	6.578726
6.160934	641.943206	6.583731
6.143477	641.337502	6.588736
5.963256	630.511652	6.593741
5.695516	604.707804	6.598746
5.463829	603.181294	6.603750
5.941063	628.012916	6.608755
6.018536	616.462723	6.613760
5.853334	618.018877	6.618765
6.087484	610.898503	6.623770
5.808015	608.935176	6.628774
5.796287	615.302067	6.633779
5.736570	598.227295	6.638784
5.720154	609.779678	6.643789
5.810537	614.127305	6.648794
5.842951	602.167082	6.653798
5.766743	595.704207	6.658803
6.005800	606.383938	6.663808
5.979993	622.903115	6.668813
6.037558	602.543850	6.673818
5.632216	602.506051	6.678822
5.841150	601.966222	6.683827
5.587866	606.328416	6.688832
5.554028	613.293620	6.693837
5.944037	626.533730	6.698842
6.127951	615.987268	6.703846
5.611339	601.819831	6.708851
5.736683	620.596776	6.713856
6.096313	628.755929	6.718861
5.898116	620.569667	6.723866
5.719608	625.997060	6.728870
5.818466	612.390634	6.733875
6.075924	601.579680	6.738880
5.645781	618.036736	6.743885
5.898958	592.627051	6.748890
5.739482	607.231415	6.753894
5.598901	603.748426	6.758899
6.232920	624.219473	6.763904
5.813692	621.902498	6.768909
5.614472	613.669057	6.773914
5.754947	617.188332	6.778918
6.014349	636.333301	6.783923
6.108731	622.162934	6.788928
5.739506	616.917470	6.793933
5.513626	594.134181	6.798938
5.935061	595.856289	6.803942
6.205286	626.714285	6.808947
6.068868	606.381054	6.813952
5.907122	604.618361	6.818957
6.013387	608.860765	6.823962
5.746866	601.653951	6.828966
5.718890	593.668245	6.833971
6.079376	599.891244	6.838976
5.383640	607.958535	6.843981
5.833256	597.328817	6.848986
6.076698	599.449090	6.853990
6.109816	604.631182	6.858995
5.887713	581.235465	6.864000
6.104368	595.829058	6.869005
6.196911	602.335168	6.874010
6.229574	600.540250	6.879014
5.963249	592.397817	6.884019
6.221721	612.313954	6.889024
5.923178	599.319137	6.894029
5.930640	586.832416	6.899034
5.607028	583.392701	6.904038
5.811676	614.582614	6.909043
5.822352	597.544844	6.914048
5.812298	609.362332	6.919053
6.064081	600.120649	6.924058
6.252750	575.660403	6.929062
5.869355	577.827933	6.934067
5.942924	576.984044	6.939072
5.744241	589.660160	6.944077
5.875932	559.529417	6.949082
5.865993	573.726970	6.954086
5.531279	563.470157	6.959091
5.750144	550.119088	6.964096
5.697437	570.977495	6.969101
5.726117	585.759389	6.974106
5.730766	595.742617	6.979110
5.499912	597.106696	6.984115
6.001012	608.776675	6.989120
6.044069	597.622146	6.994125
5.967409	595.038934	6.999130
5.807077	611.577369	7.004134
5.681908	615.729481	7.009139
5.711635	602.090094	7.014144
6.064376	597.688247	7.019149
5.891234	605.204930	7.024154
6.065879	618.924252	7.029158
5.662058	605.402676	7.034163
5.948232	585.580389	7.039168
5.768319	587.066760	7.044173
6.084962	590.398879	7.049178
5.880536	575.359806	7.054182
5.512958	579.437533	7.059187
5.923359	591.808891	7.064192
5.386915	581.816736	7.069197
5.631359	579.541519	7.074202
5.774971	609.293432	7.079206
5.512839	609.493684	7.084211
5.884928	606.440233	7.089216
5.648250	615.670312	7.094221
5.828763	612.511890	7.099226
5.706945	591.779991	7.104230
5.693814	598.036124	7.109235
5.835697	602.616434	7.114240
5.691117	595.608671	7.119245
5.764968	614.462482	7.124250
5.747278	620.919538	7.129254
5.710335	610.226383	7.134259
5.809581	603.061818	7.139264
5.635895	613.320463	7.144269
5.354334	610.056786	7.149274
5.731408	626.922336	7.154278
5.896798	612.496875	7.159283
6.150257	612.537048	7.164288
5.763014	627.243588	7.169293
6.024533	610.917046	7.174298
6.157014	611.214958	7.179302
5.954815	617.078644	7.184307
6.308939	610.900573	7.189312
6.095358	600.786194	7.194317
6.044923	610.217316	7.199322
5.964134	622.194283	7.204326
5.747220	616.492254	7.209331
6.291174	611.469569	7.214336
5.949913	603.464302	7.219341
6.135568	600.501642	7.224346
5.859505	596.252835	7.229350
5.662309	596.451925	7.234355
5.887719	605.128564	7.239360
5.955698	597.421467	7.244365
5.736181	571.385180	7.249370
5.763468	591.472375	7.254374
6.153667	602.827440	7.259379
6.186137	588.546885	7.264384
5.738262	598.969011	7.269389
6.011653	585.738131	7.274394
5.893000	565.641540	7.279398
5.669622	568.455315	7.284403
5.848076	583.429484	7.289408
5.713681	584.629648	7.294413
5.866507	566.879454	7.299418
6.049521	576.861605	7.304422
5.819192	580.624156	7.309427
5.940505	575.162493	7.314432
5.551839	579.249131	7.319437
5.527005	589.182279	7.324442
5.593344	578.847836	7.329446
5.526707	584.078368	7.334451
6.061327	600.863003	7.339456
5.880962	597.602535	7.344461
6.039618	601.047181	7.349466
6.323965	603.800044	7.354470
5.569691	575.338435	7.359475
5.792910	579.028599	7.364480
5.993846	581.024396	7.369485
5.412630	569.867495	7.374490
5.961916	583.916215	7.379494
6.076035	603.091761	7.384499
5.959087	582.327207	7.389504
5.732978	580.336323	7.394509
5.713909	562.366733	7.399514
5.583102	575.380248	7.404518
5.362173	602.276216	7.409523
5.950012	598.161850	7.414528
5.850022	598.023180	7.419533
6.047003	589.079110	7.424538
6.074749	607.831523	7.429542
5.930087	603.184356	7.434547
5.771092	573.614699	7.439552
5.631776	580.992506	7.444557
5.982129	595.540920	7.449562
5.885241	597.730260	7.454566
5.457019	592.750253	7.459571
6.064073	606.479490	7.464576
5.699951	614.265091	7.469581
5.867436	602.735743	7.474586
6.228020	598.907035	7.479590
5.444910	606.790676	7.484595
5.469244	612.185235	7.489600
5.750361	622.386285	7.494605
5.894925	600.542865	7.499610
5.955880	600.602913	7.504614
5.650343	619.609988	7.509619
6.073739	629.861814	7.514624
5.984013	615.769230	7.519629
5.746372	596.430950	7.524634
5.962991	598.301634	7.529638
5.653947	612.718329	7.534643
5.903771	625.611669	7.539648
5.742452	612.022590	7.544653
5.853860	603.041256	7.549658
5.957292	609.657833	7.554662
5.753944	623.971050	7.559667
5.846941	612.538450	7.564672
5.626334	613.390819	7.569677
5.688739	623.072714	7.574682
6.108318	610.997107	7.579686
5.514683	599.810176	7.584691
5.880497	611.056718	7.589696
5.538974	627.407690	7.594701
5.754140	617.743514	7.599706
6.160196	609.865416	7.604710
6.089345	609.660175	7.609715
5.825916	616.935397	7.614720
5.931080	619.970712	7.619725
6.053620	606.581351	7.624730
6.000908	600.615138	7.629734
5.926656	609.714985	7.634739
5.651374	596.298450	7.639744
5.829512	596.737677	7.644749
5.989237	615.812775	7.649754
5.852959	614.114828	7.654758
5.715903	604.650822	7.659763
5.953566	596.679616	7.664768
5.922227	596.663172	7.669773
5.946464	582.716728	7.674778
5.783809	577.540821	7.679782
5.460709	579.714171	7.684787
5.698604	588.959820	7.689792
5.608549	608.267762	7.694797
5.876187	612.697471	7.699802
5.966558	597.896827	7.704806
5.690289	611.849681	7.709811
6.066196	615.151493	7.714816
5.799532	605.286586	7.719821
5.952890	620.911983	7.724826
5.877096	613.181975	7.729830
5.781420	612.896393	7.734835
6.006899	601.662585	7.739840
5.744467	615.094852	7.744845
5.795238	620.363310	7.749850
6.103689	608.315540	7.754854
5.871689	614.929448	7.759859
6.309426	598.981122	7.764864
5.750682	602.330451	7.769869
5.386191	587.996329	7.774874
5.455181	596.326510	7.779878
5.869096	596.664723	7.784883
6.075690	600.309006	7.789888
5.664083	611.361339	7.794893
5.936229	600.335271	7.799898
6.101863	614.609897	7.804902
5.760050	608.720457	7.809907
5.860260	597.218609	7.814912
6.019359	606.380514	7.819917
5.739414	599.709514	7.824922
5.757337	597.886254	7.829926
5.649282	616.995741	7.834931
6.128793	600.362788	7.839936
5.848376	582.906330	7.844941
5.882144	584.867307	7.849946
5.814952	589.978469	7.854950
5.835444	583.625199	7.859955
6.013003	574.400829	7.864960
5.741676	578.628480	7.869965
5.827006	586.798709	7.874970
5.887082	568.385428	7.879974
5.494058	581.309597	7.884979
5.768537	594.221525	7.889984
5.657750	607.247738	7.894989
5.927970	590.515714	7.899994
5.978126	604.063227	7.904998
5.666993	631.549183	7.910003
5.727509	604.803045	7.915008
5.720475	620.348405	7.920013
5.495702	616.971663	7.925018
6.035511	594.269201	7.930022
5.913965	612.735350	7.935027
6.094622	596.901426	7.940032
5.868402	607.215210	7.945037
5.649211	618.060746	7.950042
5.969701	599.912672	7.955046
5.567924	614.598815	7.960051
5.879670	622.475552	7.965056
5.559824	614.927042	7.970061
5.615104	609.531324	7.975066
5.885813	613.780393	7.980070
5.379076	610.206384	7.985075
5.701385	616.134426	7.990080
5.700113	614.644318	7.995085
5.690107	611.693963	8.000090
5.986160	598.627029	8.005094
5.762386	621.846641	8.010099
5.784744	609.151161	8.015104
5.809138	606.468678	8.020109
5.847641	613.165457	8.025126
5.950129	620.162998	8.030144
5.958583	634.537435	8.035162
6.074219	607.595241	8.040179
5.744128	615.234679	8.045197
5.801504	629.087685	8.050214
5.652816	617.733592	8.055232
5.711892	634.428449	8.060250
5.833141	615.549039	8.065267
5.929549	612.640878	8.070285
5.886048	610.783702	8.075302
6.018018	618.993849	8.080320
5.793752	612.862226	8.085338
6.022304	619.392699	8.090355
6.033470	622.331164	8.095373
5.867220	611.457504	8.100390
5.872248	614.773650	8.105408
5.819566	611.214232	8.110426
5.987962	604.062082	8.115443
5.680388	608.173379	8.120461
5.763059	631.814672	8.125478
6.050553	606.711182	8.130496
5.911551	612.543549	8.135514
6.255536	615.916346	8.140531
5.767657	595.937855	8.145549
5.630775	604.930798	8.150566
5.672108	628.115856	8.155584
5.671095	647.593808	8.160602
6.142719	637.280972	8.165619
6.227974	632.153807	8.170637
5.684337	644.720407	8.175654
6.073059	636.069243	8.180672
5.758171	641.704862	8.185690
6.480664	658.493698	8.190707
6.198740	641.901828	8.195725
5.917855	632.658464	8.200742
6.435210	646.733815	8.205760
6.070249	620.857364	8.210778
6.004274	608.763726	8.215795
5.910164	620.180040	8.220813
5.837832	612.301149	8.225830
6.463328	618.973447	8.230848
6.124591	630.471718	8.235866
6.191600	610.930692	8.240883
6.283522	608.766769	8.245901
5.543230	621.377559	8.250918
6.050647	624.063297	8.255936
5.827615	612.873912	8.260954
5.949033	629.743646	8.265971
6.283655	642.524261	8.270989
5.870955	641.505538	8.276006
6.034242	641.138669	8.281024
6.139144	647.027368	8.286042
6.246825	633.411134	8.291059
6.322230	652.449712	8.296077
6.102872	657.998015	8.301094
6.264977	641.578566	8.306112
6.060529	648.751808	8.311130
5.917873	637.178555	8.316147
6.311116	643.983806	8.321165
5.995157	649.009339	8.326182
6.553586	635.263611	8.331200
5.912289	634.253146	8.336218
6.358513	636.616413	8.341235
6.142107	630.045416	8.346253
6.194719	621.485917	8.351270
6.049544	607.037126	8.356288
5.659044	631.647409	8.361306
6.103291	648.158189	8.366323
6.229774	642.058626	8.371341
5.845994	647.883930	8.376358
6.034203	645.760077	8.381376
5.668611	645.695018	8.386394
5.908335	646.768562	8.391411
5.844817	649.113931	8.396429
6.298287	632.850912	8.401446
6.223204	650.487978	8.406464
6.412066	640.366906	8.411482
6.019321	638.426733	8.416499
6.090356	651.657594	8.421517
6.314088	664.854967	8.426534
6.389300	639.895531	8.431552
6.265635	627.905580	8.436570
6.280252	641.227229	8.441587
6.573650	650.195242	8.446605
6.409051	643.509999	8.451622
6.341535	647.452045	8.456640
6.060039	645.825679	8.461658
6.307519	652.672537	8.466675
6.524228	652.932295	8.471693
6.350462	645.480568	8.476710
6.244148	632.692098	8.481728
6.204506	657.807179	8.486746
6.065553	659.741116	8.491763
6.515365	646.472846	8.496781
6.220455	660.709894	8.501798
6.364866	650.070518	8.506816
6.340302	645.329309	8.511834
6.374848	652.353737	8.516851
6.346406	661.136228	8.521869
6.007038	660.846325	8.526886
6.398937	662.357490	8.531904
6.541707	672.366763	8.536922
6.410318	673.354631	8.541939
6.548258	654.676689	8.546957
6.298174	664.401664	8.551974
6.420968	660.070527	8.556992
6.539927	646.571873	8.562010
6.127668	645.202189	8.567027
6.652752	659.994680	8.572045
6.610463	661.718109	8.577063
6.666187	668.835475	8.582080
6.634121	649.016368	8.587098
6.171965	638.172795	8.592115
6.860568	645.455962	8.597133
6.300699	659.671458	8.602151
6.431458	652.192625	8.607168
6.461557	661.811273	8.612186
6.274820	647.248285	8.617203
6.140988	660.222930	8.622221
6.383389	648.637597	8.627239
6.359109	637.095753	8.632256
6.488890	661.048508	8.637274
6.590029	690.482988	8.642291
6.596128	674.651434	8.647309
6.168612	657.844302	8.652327
6.379136	672.892669	8.657344
6.306944	683.280884	8.662362
6.481211	698.141914	8.667379
6.289849	681.344733	8.672397
6.630671	675.173919	8.677415
6.469894	686.595592	8.682432
6.416399	682.357048	8.687450
6.298764	679.710562	8.692467
6.669009	694.915774	8.697485
6.354724	691.669181	8.702503
6.521776	677.313571	8.707520
6.505024	683.041728	8.712538
6.419055	684.671520	8.717555
6.616189	686.870010	8.722573
6.384345	679.793414	8.727591
6.201678	684.233601	8.732608
6.656108	681.493858	8.737626
6.209516	696.775904	8.742643
6.773381	703.789536	8.747661
6.792665	682.955872	8.752679
6.451160	686.221947	8.757696
6.753364	691.087579	8.762714
6.718390	673.761353	8.767731
6.783754	686.346802	8.772749
6.700797	688.192573	8.777767
6.719755	686.652735	8.782784
6.802407	688.975135	8.787802
6.641209	678.092130	8.792819
6.830245	683.320659	8.797837
6.829322	678.766130	8.802855
6.718515	666.730434	8.807872
6.661615	672.430192	8.812890
6.577476	668.420179	8.817907
6.934230	688.772861	8.822925
6.757431	694.837918	8.827943
6.260590	689.390801	8.832960
6.830580	675.016525	8.837978
6.442859	696.369171	8.842995
6.642175	669.771015	8.848013
6.382647	687.432700	8.853031
6.730022	680.254284	8.858048
7.045350	694.550317	8.863066
6.811670	702.997361	8.868083
6.944765	675.730204	8.873101
6.933030	675.767549	8.878119
6.669692	680.402217	8.883136
6.856807	674.839815	8.888154
6.624535	680.199564	8.893171
6.759677	696.348893	8.898189
6.727853	677.756246	8.903207
6.667088	668.918883	8.908224
7.007115	681.796347	8.913242
6.814343	672.234545	8.918259
7.011992	667.599678	8.923277
6.926068	683.818884	8.928295
6.864140	684.708781	8.933312
6.897818	674.567281	8.938330
6.772401	684.349106	8.943347
6.849371	682.536564	8.948365
6.895236	681.968588	8.953383
6.571791	682.722322	8.958400
6.614673	681.576847	8.963418
6.604805	711.603374	8.968435
6.998607	705.137060	8.973453
6.969418	713.458117	8.978471
6.838161	723.167231	8.983488
7.326386	691.848047	8.988506
6.580829	695.224485	8.993523
6.532668	710.942338	8.998541
6.774089	715.182565	9.003559
6.931914	701.425737	9.008576
7.068400	705.025311	9.013594
6.842404	721.904048	9.018611
7.041928	721.438301	9.023629
6.855326	716.545844	9.028647
6.935346	721.901624	9.033664
6.934253	716.009875	9.038682
6.822188	718.308173	9.043699
7.138809	709.933379	9.048717
7.005295	713.502398	9.053735
7.129903	712.476548	9.058752
7.390123	728.380992	9.063770
6.905840	724.615191	9.068787
7.310707	708.394858	9.073805
6.971705	685.561017	9.078823
6.954253	700.952416	9.083840
7.148289	691.277873	9.088858
6.957950	692.684625	9.093875
7.043353	699.760201	9.098893
6.853967	685.705350	9.103911
6.948669	688.887532	9.108928
7.315879	701.682688	9.113946
6.981445	716.217873	9.118963
7.270078	710.421417	9.123981
6.860786	704.552555	9.128999
6.972318	705.495754	9.134016
7.235791	716.152547	9.139034
6.990968	722.685131	9.144051
6.866852	708.510939	9.149069
7.099791	712.538550	9.154087
7.314829	721.068004	9.159104
7.466641	723.112221	9.164122
7.121674	715.052506	9.169139
7.189699	703.213643	9.174157
7.333452	692.298339	9.179175
7.038482	677.945675	9.184192
7.060585	667.498794	9.189210
6.928065	693.140264	9.194227
7.258478	693.501672	9.199245
7.483068	693.612728	9.204263
7.127434	697.890511	9.209280
7.038023	690.716967	9.214298
6.792750	689.646366	9.219315
6.868034	694.847745	9.224333
6.972248	724.721328	9.229351
6.795452	723.770771	9.234368
7.148567	706.304214	9.239386
7.182489	706.625765	9.244403
6.898786	706.748004	9.249421
7.061136	719.591592	9.254439
7.034935	730.076049	9.259456
7.306566	710.849316	9.264474
6.956759	713.308227	9.269491
7.277419	717.933284	9.274509
7.510660	701.749783	9.279527
7.107793	720.557822	9.284544
7.226674	721.199201	9.289562
7.024412	714.544651	9.294579
7.199782	721.361145	9.299597
7.380501	739.829428	9.304615
7.326921	755.155906	9.309632
7.477523	745.970169	9.314650
7.222608	740.708879	9.319667
7.623215	737.635397	9.324685
7.345051	715.024662	9.329703
6.949454	722.818934	9.334720
7.455944	746.670014	9.339738
7.379339	752.910808	9.344755
7.498302	731.443055	9.349773
7.403065	724.492445	9.354791
7.362000	736.150503	9.359808
7.240483	734.287608	9.364826
7.491046	737.422790	9.369843
7.173629	727.767703	9.374861
7.121808	728.319803	9.379879
7.234153	739.820559	9.384896
7.613711	734.864350	9.389914
7.463377	762.006310	9.394931
7.271804	763.052247	9.399949
7.474119	744.338761	9.404967
7.376046	734.675564	9.409984
7.669888	738.193548	9.415002
7.279729	763.554766	9.420019
7.585569	761.001431	9.425037
7.662376	740.954426	9.430055
7.594185	742.414304	9.435072
7.485471	745.687283	9.440090
7.403867	735.923949	9.445107
7.535507	737.625630	9.450125
7.401304	744.787308	9.455143
7.170111	761.893462	9.460160
7.597187	763.640886	9.465178
7.536743	758.141307	9.470195
7.329637	741.300807	9.475213
7.441366	756.283518	9.480231
7.177431	749.713239	9.485248
7.689058	739.334882	9.490266
7.485149	751.105665	9.495283
7.419930	735.952979	9.500301
7.729242	736.424146	9.505319
7.488462	761.364227	9.510336
7.565689	745.460823	9.515354
7.520931	737.542575	9.520371
7.403030	732.749458	9.525389
7.448796	745.395365	9.530407
7.321994	751.858864	9.535424
7.244335	743.129341	9.540442
7.264193	734.489978	9.545459
6.849076	746.050353	9.550477
6.907764	770.663082	9.555495
7.149631	792.708359	9.560512
7.732690	787.214012	9.565530
7.624301	788.719601	9.570547
7.996820	783.595687	9.575565
8.051170	760.932297	9.580583
7.875166	779.810370	9.585600
7.880690	771.859983	9.590618
8.081602	781.400098	9.595635
8.015100	791.133191	9.600653
7.898947	768.716116	9.605671
7.662610	753.466428	9.610688
7.833917	756.245519	9.615706
7.670194	746.638427	9.620723
7.593827	740.729686	9.625741
7.844810	720.287095	9.630759
7.399745	760.335609	9.635776
7.964747	774.235040	9.640794
8.117371	759.120228	9.645811
7.399890	763.284545	9.650829
7.904637	772.254112	9.655847
7.529684	758.963128	9.660864
7.584275	751.865633	9.665882
7.983702	769.697970	9.670899
8.083588	788.287121	9.675917
7.974477	750.420462	9.680935
7.678875	765.702028	9.685952
7.533162	753.342691	9.690970
7.675378	772.476156	9.695987
7.726037	784.718933	9.701005
7.703824	769.087972	9.706023
7.649944	770.849244	9.711040
7.994118	787.004568	9.716058
8.039045	792.319827	9.721075
7.965655	780.306294	9.726093
8.013603	778.177363	9.731111
7.649922	791.141297	9.736128
7.758319	785.682095	9.741146
8.000769	773.390057	9.746163
7.806449	796.759253	9.751181
7.856984	772.546690	9.756199
7.986847	792.236995	9.761216
7.904901	789.045366	9.766234
7.908106	768.677998	9.771251
7.995372	781.215135	9.776269
7.927166	796.078348	9.781287
7.923452	790.018348	9.786304
7.751324	783.268261	9.791322
7.796502	788.202475	9.796339
7.695788	786.045565	9.801357
8.104370	781.404637	9.806375
7.698437	790.199302	9.811392
7.956946	795.315235	9.816410
8.057664	780.144135	9.821427
7.973579	778.600553	9.826445
7.901681	778.984168	9.831463
7.920783	799.211643	9.836480
7.868010	788.141790	9.841498
7.881097	802.825970	9.846515
7.793394	797.205127	9.851533
8.177073	782.501990	9.856551
8.026386	786.599118	9.861568
7.981938	788.407148	9.866586
8.112698	774.555540	9.871603
7.750046	796.157068	9.876621
8.201734	793.117150	9.881639
8.176386	790.519452	9.886656
8.176799	799.872003	9.891674
8.132265	778.232536	9.896691
8.116955	781.774362	9.901709
8.163749	791.270286	9.906727
8.273093	792.024336	9.911744
8.061761	781.584761	9.916762
8.185672	766.958613	9.921779
8.006699	784.600407	9.926797
8.129820	762.248596	9.931815
8.111819	780.065206	9.936832
8.112978	790.517532	9.941850
8.316629	783.801285	9.946867
8.108090	785.697931	9.951885
8.360597	784.615615	9.956903
8.086147	784.734751	9.961920
7.999049	787.438077	9.966938
8.565419	801.817200	9.971955
8.230260	788.771122	9.976973
8.152442	791.431784	9.981991
8.229885	795.593254	9.987008
8.437932	801.971428	9.992026
8.478004	782.460811	9.997043
8.163650	785.368577	10.002061
8.015752	791.612804	10.007079
8.099845	796.849957	10.012096
8.253708	804.392980	10.017114
8.684449	804.734171	10.022131
8.062268	800.239173	10.027149
8.230657	806.164870	10.032167
8.388594	813.907172	10.037184
8.315916	824.075148	10.042202
8.672514	817.903540	10.047219
8.554534	799.210643	10.052237
8.485357	797.381796	10.057255
8.262700	803.783128	10.062272
8.004893	792.068495	10.067290
8.348529	778.133884	10.072307
7.990819	791.607818	10.077325
8.343774	795.735862	10.082343
8.578830	816.633588	10.087360
8.769830	801.364498	10.092378
8.559887	785.633082	10.097395
8.310962	795.190472	10.102413
8.022694	783.108440	10.107431
8.509335	786.058102	10.112448
8.355311	799.671172	10.117466
8.380564	806.437236	10.122483
8.581946	814.310708	10.127501
8.442559	810.527348	10.132519
8.631746	820.308437	10.137536
8.648997	821.355783	10.142554
8.561009	780.797783	10.147571
8.390409	793.718398	10.152589
8.303942	800.563339	10.157607
8.428906	819.390543	10.162624
8.168535	809.648439	10.167642
8.567877	805.945988	10.172659
8.273495	811.729815	10.177677
7.996389	830.529899	10.182695
8.783423	813.270967	10.187712
8.463878	814.483784	10.192730
8.375011	821.778422	10.197747
8.563712	822.100375	10.202765
8.498978	803.026331	10.207783
8.916342	813.121485	10.212800
8.564032	829.564642	10.217818
8.973137	814.575162	10.222835
8.565015	800.555762	10.227853
8.247699	806.994976	10.232871
8.713061	807.136107	10.237888
8.294604	815.467428	10.242906
8.418546	811.627957	10.247923
8.382655	821.819765	10.252941
8.351962	813.938907	10.257959
8.585692	805.300667	10.262976
8.288209	811.003728	10.267994
8.957859	824.392735	10.273011
8.586011	841.124688	10.278029
8.747081	839.660142	10.283047
8.688042	826.931790	10.288064
8.724745	835.786960	10.293082
8.707492	823.155124	10.298099
8.632308	825.011140	10.303117
9.349843	843.278268	10.308135
9.170964	844.524125	10.313152
8.710138	835.161890	10.318170
8.746797	809.031890	10.323187
8.511411	815.601231	10.328205
8.464618	821.917420	10.333223
8.704852	808.205622	10.338240
8.754335	826.690876	10.343258
8.328472	828.401452	10.348275
8.616870	829.017773	10.353293
8.893423	839.934922	10.358311
9.079708	847.423803	10.363328
8.815739	844.723834	10.368346
9.117814	853.615061	10.373363
8.923604	845.589305	10.378381
8.651809	822.885945	10.383399
8.913815	821.749610	10.388416
8.523528	840.929635	10.393434
8.866816	846.004810	10.398451
8.463041	855.030985	10.403469
8.735492	855.913359	10.408487
8.804239	846.168010	10.413504
8.691071	851.726878	10.418522
8.741455	846.224696	10.423539
8.588441	859.901021	10.428557
8.512898	855.611067	10.433575
8.995038	843.077645	10.438592
8.764568	853.030047	10.443610
8.908706	840.577181	10.448627
8.749943	848.307089	10.453645
8.996202	860.196328	10.458663
9.308703	875.595368	10.463680
8.932974	864.751324	10.468698
8.788174	850.687280	10.473715
8.860769	866.017617	10.478733
8.858370	860.832341	10.483751
9.253314	866.344047	10.488768
9.133671	869.923602	10.493786
9.032496	874.518837	10.498803
8.844839	854.334726	10.503821
9.227785	871.333215	10.508839
9.519756	885.657198	10.513856
9.111000	858.894997	10.518874
9.235455	857.464347	10.523891
9.081293	856.948215	10.528909
8.944822	856.711171	10.533927
8.984412	850.677250	10.538944
8.913220	858.593132	10.543962
9.268229	855.150882	10.548979
9.276332	859.543259	10.553997
8.907800	845.121316	10.559015
9.413591	851.241011	10.564032
8.717561	861.769634	10.569050
8.950758	852.028987	10.574067
9.347254	873.988608	10.579085
9.289537	878.375632	10.584103
9.248412	863.040439	10.589120
9.239681	871.589932	10.594138
9.139777	879.037464	10.599155
9.328170	872.180529	10.604173
9.287598	878.630127	10.609191
9.618949	866.744769	10.614208
9.138372	866.593815	10.619226
9.073828	847.868805	10.624243
9.136290	861.983613	10.629261
9.054586	861.292261	10.634279
9.680581	865.632813	10.639296
9.250325	857.744162	10.644314
9.110079	856.854075	10.649331
9.123565	871.252896	10.654349
9.108743	869.594244	10.659367
9.474493	855.295865	10.664384
9.381165	872.852759	10.669402
9.441301	879.341016	10.674419
9.479240	886.004356	10.679437
9.696434	874.701981	10.684455
9.558838	851.315059	10.689472
9.268033	864.421695	10.694490
9.182333	856.084279	10.699507
9.311593	844.188153	10.704525
9.230387	855.805999	10.709543
9.315919	865.556916	10.714560
9.689032	876.743395	10.719578
9.370711	868.771297	10.724595
9.394495	857.369337	10.729613
9.320668	888.397171	10.734631
9.718710	882.842838	10.739648
9.494937	861.617812	10.744666
9.415195	860.503510	10.749683
9.395572	864.207935	10.754701
9.361493	856.995156	10.759719
9.769074	861.524025	10.764736
9.463099	855.555768	10.769754
9.573487	870.023691	10.774771
9.590757	864.031041	10.779789
9.397370	852.847012	10.784807
9.528163	837.036111	10.789824
9.161410	854.649780	10.794842
9.336402	875.744570	10.799859
9.726372	872.224314	10.804877
9.635157	874.790871	10.809895
9.629508	882.494806	10.814912
9.507635	873.840803	10.819930
9.550056	884.227434	10.824947
9.960944	881.516697	10.829965
9.559291	888.281021	10.834983
9.798847	873.048510	10.840000
9.525904	856.541514	10.845018
9.499857	868.704539	10.850035
9.590134	848.642769	10.855053
9.386482	862.251992	10.860071
9.869698	866.889887	10.865088
9.552253	875.750961	10.870106
9.519674	874.551621	10.875123
9.642886	868.951886	10.880141
9.513712	879.961991	10.885159
9.882909	895.490720	10.890176
9.722226	893.702765	10.895194
9.805045	864.865740	10.900211
9.701486	869.566458	10.905229
9.265259	890.799766	10.910247
9.371864	873.399733	10.915264
9.578977	886.612442	10.920282
9.747554	881.103508	10.925299
9.748038	882.063594	10.930317
9.271215	875.269356	10.935335
9.126938	877.618855	10.940352
9.462113	909.963331	10.945370
9.538117	906.428236	10.950387
10.123869	906.106084	10.955405
9.637672	918.611657	10.960423
9.509833	893.824598	10.965440
9.675399	909.764749	10.970458
9.331122	922.956336	10.975475
9.690420	901.864564	10.980493
9.606763	917.514597	10.985511
9.573764	915.038190	10.990528
9.802333	922.507722	10.995546
9.661768	939.943693	11.000563
10.144499	922.058821	11.005581
10.363836	933.318871	11.010599
10.032119	938.949408	11.015616
10.141675	918.355068	11.020634
9.919214	913.621092	11.025651
10.150281	914.120152	11.030669
9.855029	894.133448	11.035687
9.868836	912.826027	11.040704
9.378213	910.688957	11.045722
9.440810	926.512023	11.050739
9.947198	937.145260	11.055757
9.730468	939.979653	11.060775
10.077579	927.795754	11.065792
10.127787	932.437526	11.070810
10.185682	942.640878	11.075827
10.464076	940.257755	11.080845
9.776313	936.979741	11.085863
9.989037	940.416713	11.090880
10.026143	939.101154	11.095898
10.098913	957.354035	11.100915
10.152279	959.443187	11.105933
10.105442	945.114112	11.110951
10.104946	917.926067	11.115968
10.255329	932.018340	11.120986
10.309124	953.531491	11.126003
10.531374	956.237649	11.131021
10.316295	938.406672	11.136039
10.447501	929.936742	11.141056
10.538370	930.326131	11.146074
10.442094	937.692798	11.151091
10.234809	914.744351	11.156109
10.013786	901.778305	11.161127
9.837968	912.724703	11.166144
9.930052	921.469911	11.171162
9.983866	943.271159	11.176179
10.394582	936.361416	11.181197
10.308401	938.628213	11.186215
10.513674	938.062027	11.191232
10.330466	925.154066	11.196250
9.959645	933.316302	11.201267
10.204060	923.467484	11.206285
10.181433	949.886294	11.211303
10.234532	945.687232	11.216320
10.197392	931.642616	11.221338
10.142387	927.777780	11.226355
10.214683	944.836838	11.231373
10.456934	947.190368	11.236391
10.344509	941.106945	11.241408
10.529684	933.710987	11.246426
9.990983	947.063430	11.251443
10.652592	936.320872	11.256461
10.610822	947.135230	11.261479
10.284252	935.407743	11.266496
10.815122	944.319663	11.271514
10.595641	937.618661	11.276531
10.741406	951.061587	11.281549
10.295853	937.670036	11.286567
10.245158	925.363344	11.291584
10.571541	937.894156	11.296602
10.304790	950.559307	11.301619
10.203803	937.979491	11.306637
10.624300	941.740795	11.311655
10.189235	930.938883	11.316672
10.628620	934.440536	11.321690
10.819175	953.625673	11.326707
10.840816	932.407816	11.331725
10.624571	927.495392	11.336743
10.615017	948.126024	11.341760
10.714533	928.085453	11.346778
10.577759	930.855266	11.351795
10.563930	933.109515	11.356813
10.893969	928.312177	11.361831
10.449607	905.148854	11.366848
10.515527	907.653435	11.371866
10.186410	924.639078	11.376883
10.826047	946.233313	11.381901
10.698674	933.483791	11.386919
10.655029	921.328654	11.391936
10.744153	937.107495	11.396954
10.514091	941.021964	11.401971
10.529881	942.689776	11.406989
10.669228	951.836831	11.412007
10.626363	947.421107	11.417024
10.800270	925.871875	11.422042
10.639677	931.273297	11.427059
10.569831	937.150150	11.432077
10.364886	936.465778	11.437095
10.525973	940.394526	11.442112
10.743691	942.001416	11.447130
10.393993	930.902988	11.452147
10.660543	934.994968	11.457165
10.629898	931.819825	11.462183
10.313103	934.595083	11.467200
10.764988	938.277203	11.472218
10.418797	960.737734	11.477235
11.018701	949.493387	11.482253
10.987469	951.030915	11.487271
10.919522	951.162863	11.492288
11.340424	944.434654	11.497306
10.712310	944.135683	11.502323
11.006536	934.971166	11.507341
10.803706	932.357117	11.512359
10.843885	938.813076	11.517376
10.996466	926.314859	11.522394
10.845109	945.763128	11.527411
10.731771	950.303521	11.532429
10.626184	937.045899	11.537447
10.783674	952.798108	11.542464
10.804308	960.827477	11.547482
11.052101	966.573720	11.552499
11.365224	970.838774	11.557517
11.173227	946.712264	11.562535
10.742975	953.149931	11.567552
11.190115	958.924729	11.572570
11.108914	934.209109	11.577587
10.839906	937.546896	11.582605
11.139878	939.751454	11.587623
11.134727	932.681952	11.592640
11.234963	933.218771	11.597658
11.064342	926.410710	11.602675
10.704651	941.923162	11.607693
11.094900	937.348784	11.612711
11.099687	963.970810	11.617728
11.389720	946.823774	11.622746
11.315281	954.877511	11.627763
10.787731	935.399592	11.632781
10.926363	936.389102	11.637799
10.960929	966.006919	11.642816
11.444804	960.731606	11.647834
11.197298	967.496469	11.652851
11.337982	964.422305	11.657869
11.481497	959.607564	11.662887
11.073055	943.514302	11.667904
11.067260	926.267395	11.672922
10.885518	935.353849	11.677939
11.274883	959.203067	11.682957
11.457882	978.046953	11.687975
11.171053	965.370003	11.692992
11.442238	968.175530	11.698010
11.458874	972.066951	11.703027
11.286832	948.293153	11.708045
11.282751	946.929492	11.713063
11.048507	968.014105	11.718080
11.349987	957.101281	11.723098
11.218489	951.238568	11.728115
11.127933	975.109654	11.733133
11.521660	971.958542	11.738151
11.247052	970.396930	11.743168
11.293557	966.950533	11.748186
11.347378	981.094529	11.753203
10.873783	965.897219	11.758221
11.333660	950.780349	11.763239
10.777236	967.402425	11.768256
10.850578	983.514842	11.773274
11.008628	980.256945	11.778291
11.257355	973.435652	11.783309
11.602044	980.856994	11.788327
11.600777	1007.412668	11.793344
11.907194	1006.545880	11.798362
11.516042	984.010910	11.803379
11.417590	963.764582	11.808397
11.675435	958.425763	11.813415
11.394352	972.729399	11.818432
11.439824	973.395613	11.823450
11.319585	955.889998	11.828467
11.318623	977.523030	11.833485
11.510317	990.203079	11.838503
11.288905	1013.192115	11.843520
11.557698	984.573307	11.848538
11.803696	1002.600594	11.853555
11.522560	988.307073	11.858573
11.896219	994.213977	11.863591
11.380458	1007.213827	11.868608
11.776977	976.890491	11.873626
12.032527	998.290832	11.878643
11.754689	1004.170593	11.883661
11.913344	965.265236	11.888679
11.637965	983.671622	11.893696
11.660604	952.337335	11.898714
11.722251	957.492742	11.903731
11.707973	969.350239	11.908749
11.827181	941.778387	11.913767
11.568194	957.972461	11.918784
11.501018	978.601930	11.923802
11.883332	983.822534	11.928819
11.970277	973.907801	11.933837
11.740823	966.383152	11.938855
11.724192	962.686921	11.943872
11.743302	985.134057	11.948890
12.117663	979.143851	11.953907
11.722231	980.617485	11.958925
11.927039	968.968358	11.963943
11.782653	964.150516	11.968960
11.617698	964.371114	11.973978
11.959901	983.843847	11.978995
11.808088	999.520552	11.984013
11.850993	1001.209276	11.989031
11.784466	989.629105	11.994048
12.080374	980.787331	11.999066
12.203781	997.517980	12.004083
11.992301	986.976469	12.009101
12.092487	964.967044	12.014119
11.986240	958.125108	12.019136
11.842323	967.891376	12.024154
11.756992	978.110351	12.029171
11.768565	1003.374557	12.034189
11.870265	990.860317	12.039207
12.040585	977.933840	12.044224
11.928982	981.117998	12.049242
12.130212	987.317304	12.054259
11.621550	995.297088	12.059277
11.968630	995.271989	12.064295
12.023843	999.342404	12.069312
11.988927	990.849241	12.074330
12.020117	996.904942	12.079347
11.980140	1000.859429	12.084365
11.999794	995.716045	12.089383
11.647720	992.674204	12.094400
11.961075	1002.006725	12.099418
11.967512	997.452558	12.104435
11.870384	995.912512	12.109453
12.310293	1009.780556	12.114471
12.554428	1001.953470	12.119488
12.196850	995.778706	12.124506
12.332365	998.306709	12.129523
12.035051	982.395901	12.134541
12.364453	967.097478	12.139559
12.447249	993.421992	12.144576
12.092796	996.532043	12.149594
12.248410	982.627531	12.154611
11.876189	978.566052	12.159629
11.986157	990.804506	12.164647
12.338036	1006.133678	12.169664
12.472419	1015.794355	12.174682
12.531992	1025.048904	12.179699
12.189943	1004.903294	12.184717
12.286598	983.464484	12.189735
12.407463	986.840091	12.194752
12.157265	1014.568714	12.199770
12.466245	1010.138912	12.204787
12.335836	1023.336275	12.209805
12.419797	1025.910317	12.214823
12.245849	1015.219683	12.219840
12.179700	1009.758250	12.224858
12.475332	1020.773334	12.229875
12.417789	1023.619812	12.234893
12.383323	1023.048272	12.239911
11.953154	1005.139601	12.244928
12.482249	1003.684874	12.249946
12.471164	1015.801262	12.254963
12.135946	1034.058779	12.259981
12.191604	1015.787696	12.264999
12.304505	1018.485269	12.270016
11.889656	1016.877160	12.275034
12.406457	1026.401733	12.280051
12.546766	1056.398116	12.285069
12.572352	1066.483987	12.290087
12.647746	1052.722360	12.295104
12.572566	1041.825964	12.300122
12.896244	1047.947889	12.305139
12.746006	1059.005883	12.310157
12.914723	1045.003503	12.315175
13.170323	1024.587788	12.320192
12.817857	1022.136212	12.325210
12.517894	1000.677680	12.330227
12.482327	1001.455295	12.335245
12.550239	1003.491177	12.340263
12.799369	1023.147801	12.345280
12.427932	1017.577603	12.350298
12.858054	993.063859	12.355315
12.649171	1005.988691	12.360333
12.718856	1017.129081	12.365351
12.738582	1017.931409	12.370368
12.732916	1025.023169	12.375386
13.016049	1023.431572	12.380403
12.748252	1020.787801	12.385421
12.698792	1003.740395	12.390439
12.972744	1023.069869	12.395456
12.786872	1039.367468	12.400474
12.798979	1023.991928	12.405491
12.986877	1025.856152	12.410509
12.811900	1033.930776	12.415527
12.718102	1033.399544	12.420544
12.719787	1036.045635	12.425562
12.961012	1024.024987	12.430579
12.623609	1022.013429	12.435597
12.609389	1027.726635	12.440615
12.785117	1047.712566	12.445632
12.826648	1041.924250	12.450650
12.928397	1032.203539	12.455667
12.877210	1039.121870	12.460685
12.842148	1038.178867	12.465703
12.942153	1037.473322	12.470720
12.666340	1057.809210	12.475738
12.715226	1040.558157	12.480755
12.658506	1041.203377	12.485773
13.196714	1062.587134	12.490791
13.033965	1048.947226	12.495808
13.053979	1058.554703	12.500826
13.235166	1064.851817	12.505843
13.186733	1060.587928	12.510861
12.912691	1038.091065	12.515879
13.092689	1032.807003	12.520896
13.060646	1058.515628	12.525914
13.294076	1052.254071	12.530931
13.183847	1064.507522	12.535949
13.452345	1076.807424	12.540967
13.404195	1042.480176	12.545984
13.212398	1029.198640	12.551002
13.465467	1022.176854	12.556019
13.135704	1043.956025	12.561037
12.986938	1028.248296	12.566055
13.416776	1040.490904	12.571072
12.840130	1034.529619	12.576090
13.183480	1023.273003	12.581107
13.325558	1052.182743	12.586125
13.520918	1075.882261	12.591143
13.627443	1066.254909	12.596160
13.275662	1039.184034	12.601178
13.261761	1012.232919	12.606195
13.454604	1033.690633	12.611213
13.021407	1047.449343	12.616231
13.429887	1040.752075	12.621248
13.674044	1034.806489	12.626266
13.669801	1021.580755	12.631283
13.356962	1028.869502	12.636301
13.120961	1042.096138	12.641319
13.599908	1025.815210	12.646336
13.363527	1024.004521	12.651354
13.588238	1023.942375	12.656371
13.670204	1046.428414	12.661389
13.502458	1040.995960	12.666407
13.563210	1041.454782	12.671424
13.578314	1036.832849	12.676442
13.586382	1019.292871	12.681459
13.498009	1011.496030	12.686477
13.429948	1030.916080	12.691495
13.701963	1042.986297	12.696512
13.657078	1039.080498	12.701530
13.480959	1033.271474	12.706547
13.702629	1021.886087	12.711565
13.554387	1012.075435	12.716583
13.717605	1022.019665	12.721600
13.384969	1036.043270	12.726618
13.723468	1028.950882	12.731635
13.222202	1037.506880	12.736653
13.280092	1050.267935	12.741671
14.040748	1068.870348	12.746688
13.749433	1083.693858	12.751706
13.991596	1051.137262	12.756723
13.953665	1047.529253	12.761741
13.863549	1047.153477	12.766759
13.694190	1051.494449	12.771776
13.315264	1049.620818	12.776794
13.704953	1045.585147	12.781811
13.702633	1053.024509	12.786829
13.612628	1058.215442	12.791847
13.932100	1068.800251	12.796864
13.916782	1073.310804	12.801882
14.006476	1058.277437	12.806899
13.891669	1064.402063	12.811917
13.936525	1091.176114	12.816935
14.203540	1063.663849	12.821952
14.108604	1054.021777	12.826970
13.809072	1036.048283	12.831987
13.911619	1044.875375	12.837005
13.679194	1075.943278	12.842023
14.202306	1060.301804	12.847040
14.015237	1065.345927	12.852058
14.195688	1065.113088	12.857075
13.883218	1036.472329	12.862093
13.546674	1044.625810	12.867111
14.246119	1053.370110	12.872128
13.967797	1060.298335	12.877146
14.060977	1063.561633	12.882163
14.174466	1068.557171	12.887181
13.841418	1079.060397	12.892199
14.150744	1053.399065	12.897216
14.010604	1076.240769	12.902234
13.854293	1089.489603	12.907251
14.085925	1064.922124	12.912269
13.839073	1056.669286	12.917287
14.030892	1075.856730	12.922304
13.921135	1078.792437	12.927322
14.140106	1068.310683	12.932339
14.124516	1066.221732	12.937357
13.912398	1070.026110	12.942375
14.082450	1063.882673	12.947392
14.169697	1048.095577	12.952410
14.161044	1066.723470	12.957427
14.338319	1069.710143	12.962445
14.045387	1066.909435	12.967463
14.148125	1057.922615	12.972480
14.383385	1089.356358	12.977498
14.553029	1103.267894	12.982515
14.418772	1081.188606	12.987533
14.057710	1059.575464	12.992551
14.556483	1068.703733	12.997568
14.478237	1069.142525	13.002586
14.294175	1062.619034	13.007603
14.131064	1077.886002	13.012621
14.119765	1104.984338	13.017639
14.467269	1076.602856	13.022656
14.479537	1091.891925	13.027674
14.532839	1096.947898	13.032691
14.500843	1092.632477	13.037709
14.392877	1094.765726	13.042727
14.519315	1084.602033	13.047744
14.676062	1104.989503	13.052762
14.435490	1118.129974	13.057779
14.578930	1101.005121	13.062797
14.214929	1103.280756	13.067815
14.611607	1103.634768	13.072832
14.313956	1089.183660	13.077850
14.015382	1089.833819	13.082867
14.515578	1108.275730	13.087885
14.417912	1110.098496	13.092903
14.495456	1090.212586	13.097920
14.580370	1091.663333	13.102938
14.036012	1098.272537	13.107955
14.705921	1108.435772	13.112973
14.648480	1125.147959	13.117991
14.968036	1119.677163	13.123008
14.976872	1086.952111	13.128026
14.720719	1091.197228	13.133043
14.953925	1093.561428	13.138061
14.586426	1088.390848	13.143079
14.780604	1078.193825	13.148096
15.028730	1076.116987	13.153114
14.624041	1089.056067	13.158131
14.897255	1101.861975	13.163149
14.731467	1097.921233	13.168167
14.771984	1083.473288	13.173184
14.720175	1084.643061	13.178202
14.561447	1087.850380	13.183219
14.836125	1108.634012	13.188237
14.814170	1121.606206	13.193255
15.070825	1113.615223	13.198272
15.440389	1113.949411	13.203290
14.996358	1103.649128	13.208307
15.010853	1111.421879	13.213325
14.662963	1093.746493	13.218343
14.643587	1082.099395	13.223360
14.860096	1102.752607	13.228378
14.879570	1109.036709	13.233395
15.031954	1108.950205	13.238413
14.839953	1110.632103	13.243431
15.377301	1115.806271	13.248448
15.372184	1109.639020	13.253466
15.216217	1115.672953	13.258483
15.414748	1123.735888	13.263501
15.408952	1113.182219	13.268519
15.086650	1078.721301	13.273536
15.159986	1066.487282	13.278554
15.257690	1084.566356	13.283571
15.342971	1090.877460	13.288589
15.225623	1078.546923	13.293607
15.668289	1071.043108	13.298624
15.315860	1087.327938	13.303642
15.499675	1069.891011	13.308659
15.288155	1077.248942	13.313677
15.066593	1081.658081	13.318695
15.091089	1080.332392	13.323712
15.240772	1068.087625	13.328730
15.073578	1070.740375	13.333747
15.370434	1081.181821	13.338765
15.247630	1090.819217	13.343783
14.874423	1082.506655	13.348800
15.351208	1088.627304	13.353818
14.850448	1079.521259	13.358835
15.270237	1094.887834	13.363853
15.400622	1123.355262	13.368871
15.335890	1100.768416	13.373888
15.566354	1108.883237	13.378906
15.214971	1124.220724	13.383923
15.474800	1122.256288	13.388941
15.315117	1120.217808	13.393959
15.256389	1103.830028	13.398976
15.579233	1111.222671	13.403994
15.165124	1117.721404	13.409011
15.686576	1112.567063	13.414029
15.267917	1122.135190	13.419047
15.211112	1122.588250	13.424064
15.325387	1107.911217	13.429082
15.494313	1111.123337	13.434099
15.658663	1119.355264	13.439117
15.695456	1130.624272	13.444135
15.656163	1098.808504	13.449152
15.921843	1102.000697	13.454170
15.388039	1114.598822	13.459187
15.643595	1123.888547	13.464205
15.594243	1121.015891	13.469223
15.536746	1099.894422	13.474240
15.528205	1118.351732	13.479258
15.792477	1140.246994	13.484275
15.793354	1126.272276	13.489293
15.771408	1149.110103	13.494311
15.813705	1138.975630	13.499328
16.119274	1139.723052	13.504346
16.142944	1135.506661	13.509363
16.008257	1112.483730	13.514381
15.851248	1122.962126	13.519399
15.515054	1115.605006	13.524416
15.684378	1103.554456	13.529434
15.631941	1124.475414	13.534451
15.795996	1128.055773	13.539469
16.100964	1138.637714	13.544487
15.883875	1130.213226	13.549504
16.358312	1127.151969	13.554522
16.099543	1132.808013	13.559539
16.217090	1103.933605	13.564557
15.807509	1108.986764	13.569575
15.707381	1123.458817	13.574592
16.009512	1115.713898	13.579610
15.731855	1111.115525	13.584627
16.159434	1134.756488	13.589645
16.112528	1133.594428	13.594663
16.137719	1146.828373	13.599680
16.145537	1137.952050	13.604698
16.219758	1137.759988	13.609715
16.483860	1126.136662	13.614733
15.947205	1124.571991	13.619751
16.002612	1115.603684	13.624768
16.111439	1114.281375	13.629786
16.072824	1153.133904	13.634803
16.051728	1142.498906	13.639821
16.144751	1137.399120	13.644839
15.932903	1152.262701	13.649856
16.391394	1144.682729	13.654874
16.324166	1134.798290	13.659891
16.466923	1133.687150	13.664909
16.447773	1140.179173	13.669927
16.444318	1143.922322	13.674944
16.330619	1132.433651	13.679962
16.236224	1140.770538	13.684979
16.600225	1146.349453	13.689997
16.448937	1148.478946	13.695015
16.616918	1140.377043	13.700032
16.441663	1121.144827	13.705050
16.367295	1142.473075	13.710067
16.919078	1154.459756	13.715085
16.782785	1135.461870	13.720103
16.332592	1108.364332	13.725120
16.126905	1109.112007	13.730138
15.897568	1132.948118	13.735155
16.310478	1131.337820	13.740173
16.585918	1133.763927	13.745191
16.426060	1127.210136	13.750208
16.420221	1141.893833	13.755226
16.455118	1160.497424	13.760243
16.467771	1137.603712	13.765261
16.722641	1139.969160	13.770279
16.402002	1140.585181	13.775296
16.518508	1134.319888	13.780314
16.330397	1146.038080	13.785331
16.462740	1134.258416	13.790349
16.710768	1147.627543	13.795367
16.817904	1148.549061	13.800384
17.094635	1146.470143	13.805402
16.528477	1152.321937	13.810419
16.569358	1143.057366	13.815437
16.698695	1136.151327	13.820455
16.486237	1152.256145	13.825472
16.891546	1164.713978	13.830490
16.979270	1178.160397	13.835507
17.076842	1173.816260	13.840525
17.075304	1147.887419	13.845543
16.889643	1147.288412	13.850560
16.818438	1135.145728	13.855578
16.568173	1152.770698	13.860595
16.763549	1160.518207	13.865613
16.850854	1180.014222	13.870631
17.003055	1178.297234	13.875648
17.085610	1163.885464	13.880666
17.151686	1166.795280	13.885683
16.762766	1167.942933	13.890701
16.958058	1179.960599	13.895719
16.886464	1176.054554	13.900736
17.283498	1161.220532	13.905754
16.812539	1165.583529	13.910771
16.730888	1189.024053	13.915789
17.200082	1174.152510	13.920807
16.929681	1156.007762	13.925824
17.207177	1170.615341	13.930842
16.933146	1178.044462	13.935859
17.063520	1172.752611	13.940877
17.116266	1174.190478	13.945895
17.140866	1177.167962	13.950912
17.306635	1177.199000	13.955930
17.152874	1179.569498	13.960947
17.066711	1189.771237	13.965965
17.316212	1184.658664	13.970983
17.293194	1172.794040	13.976000
16.934890	1152.089541	13.981018
17.154165	1167.919831	13.986035
16.854994	1180.938772	13.991053
17.039480	1183.518172	13.996071
16.967092	1185.595369	14.001088
17.480455	1186.013152	14.006106
17.919214	1192.404533	14.011123
17.710480	1208.281781	14.016141
17.868583	1191.886710	14.021159
17.603263	1164.128456	14.026176
17.630752	1158.269205	14.031194
17.758554	1170.578166	14.036211
17.542715	1164.717599	14.041229
17.564814	1144.718861	14.046247
17.426680	1154.639569	14.051264
17.638195	1167.250463	14.056282
17.501577	1179.334786	14.061299
17.543406	1164.812549	14.066317
17.676586	1156.226448	14.071335
17.479024	1168.559654	14.076352
17.446353	1177.375022	14.081370
17.521118	1168.712958	14.086387
17.705706	1158.392792	14.091405
17.489369	1152.970001	14.096423
17.789717	1182.344757	14.101440
17.804422	1170.681923	14.106458
17.557592	1166.847938	14.111475
17.634163	1153.537689	14.116493
17.687977	1161.961682	14.121511
17.583517	1189.687818	14.126528
17.900037	1198.384484	14.131546
17.756034	1190.111330	14.136563
17.926442	1180.246239	14.141581
17.929589	1184.182551	14.146599
17.986099	1205.727982	14.151616
17.901756	1198.514001	14.156634
17.825035	1184.530700	14.161651
17.969154	1175.621893	14.166669
18.464315	1182.911900	14.171687
18.168289	1186.380946	14.176704
17.938079	1162.783610	14.181722
17.936207	1158.390572	14.186739
17.744408	1168.366013	14.191757
18.134941	1156.055593	14.196775
17.764997	1169.555201	14.201792
17.771073	1157.262753	14.206810
18.077840	1164.485876	14.211827
17.899220	1184.445131	14.216845
17.817749	1190.086264	14.221863
17.871695	1197.035706	14.226880
17.927724	1196.049399	14.231898
17.997586	1184.619310	14.236915
18.169263	1177.611101	14.241933
18.219973	1192.331259	14.246951
18.088181	1193.279373	14.251968
18.232481	1181.865620	14.256986
18.282580	1198.786537	14.262003
18.234686	1193.384212	14.267021
18.394442	1168.749822	14.272039
17.985339	1166.060888	14.277056
18.165586	1183.669560	14.282074
17.944562	1198.411405	14.287091
17.951663	1191.258184	14.292109
18.112674	1199.773513	14.297127
18.440125	1213.258380	14.302144
18.514576	1211.763832	14.307162
18.779258	1210.739206	14.312179
18.460611	1216.299099	14.317197
18.529426	1219.519520	14.322215
18.481156	1213.731218	14.327232
18.572150	1214.575506	14.332250
18.671067	1201.503001	14.337267
18.262798	1189.901488	14.342285
18.641494	1200.944797	14.347303
18.758926	1215.266051	14.352320
18.651573	1199.895708	14.357338
18.695433	1171.461890	14.362355
18.341678	1183.692801	14.367373
18.509641	1200.793408	14.372391
18.501575	1206.742812	14.377408
18.749189	1195.571363	14.382426
18.675025	1204.797838	14.387443
18.705493	1211.312885	14.392461
18.739434	1197.269760	14.397479
18.502691	1210.972928	14.402496
18.606300	1213.734360	14.407514
18.851180	1191.728741	14.412531
18.691806	1201.963054	14.417549
18.708949	1202.856249	14.422567
18.423346	1224.948283	14.427584
18.813199	1220.362079	14.432602
19.167640	1199.965615	14.437619
18.884461	1189.066683	14.442637
18.731606	1205.357133	14.447655
18.776691	1218.084527	14.452672
18.491460	1220.175057	14.457690
18.754709	1220.364749	14.462707
18.477445	1212.932012	14.467725
18.754346	1228.763273	14.472743
19.004151	1251.236145	14.477760
19.019787	1245.490310	14.482778
19.170423	1235.313171	14.487795
19.152950	1230.979271	14.492813
19.123890	1251.211170	14.497831
19.233521	1246.441497	14.502848
19.446315	1238.956793	14.507866
19.337931	1242.993323	14.512883
19.450567	1244.505039	14.517901
19.408349	1219.350828	14.522919
19.253659	1210.378315	14.527936
19.185555	1212.017314	14.532954
19.391461	1194.256298	14.537971
19.155000	1203.068851	14.542989
19.305208	1202.143241	14.548007
19.309407	1219.462816	14.553024
19.348891	1208.173130	14.558042
19.335568	1183.849829	14.563059
19.105730	1204.615021	14.568077
19.524933	1193.800361	14.573095
19.530408	1192.934783	14.578112
19.267991	1212.076133	14.583130
19.434225	1199.615683	14.588147
19.264053	1200.400200	14.593165
19.234029	1195.644765	14.598183
19.095931	1202.002670	14.603200
19.385980	1221.814167	14.608218
19.680353	1214.680867	14.613235
19.511339	1225.181293	14.618253
19.816055	1233.285681	14.623271
19.622250	1224.628311	14.628288
19.600725	1227.070642	14.633306
19.592698	1239.652439	14.638323
19.299173	1232.001074	14.643341
19.539207	1238.688638	14.648359
19.655311	1220.925702	14.653376
19.635083	1217.259820	14.658394
20.163449	1219.814872	14.663411
19.644643	1241.533262	14.668429
19.726068	1237.440142	14.673447
19.596444	1232.551780	14.678464
19.408149	1222.556613	14.683482
19.540121	1218.671038	14.688499
19.824282	1220.638151	14.693517
19.366220	1230.623585	14.698535
19.359363	1231.234005	14.703552
19.471818	1232.703044	14.708570
19.952638	1255.354034	14.713587
20.151648	1269.073610	14.718605
20.109175	1243.986018	14.723623
20.357393	1226.804251	14.728640
20.026028	1249.715599	14.733658
20.008086	1221.236895	14.738675
20.202214	1222.278656	14.743693
20.561650	1240.204353	14.748711
20.490174	1219.546632	14.753728
19.934403	1209.325260	14.758746
20.159397	1217.770689	14.763763
20.043345	1240.752717	14.768781
19.943367	1224.404688	14.773799
20.169579	1216.347538	14.778816
19.911518	1209.450970	14.783834
20.261551	1223.777878	14.788851
19.797060	1230.119276	14.793869
20.043318	1222.278444	14.798887
20.326347	1242.213441	14.803904
20.299940	1221.461184	14.808922
20.220119	1198.790191	14.813939
20.022063	1226.525957	14.818957
20.318628	1233.917098	14.823975
20.199546	1231.856050	14.828992
19.919572	1242.228402	14.834010
20.103637	1245.770844	14.839027
20.121964	1264.306941	14.844045
20.012542	1280.431571	14.849063
20.297137	1266.765072	14.854080
20.167889	1249.515372	14.859098
20.621803	1254.305242	14.864115
20.395402	1276.552488	14.869133
20.620772	1270.088778	14.874151
20.493540	1256.795980	14.879168
20.224575	1259.091259	14.884186
20.455863	1256.406890	14.889203
20.302947	1244.427390	14.894221
20.442534	1266.288135	14.899239
20.708730	1275.082117	14.904256
20.773463	1274.612257	14.909274
20.984563	1268.420626	14.914291
20.843111	1253.729722	14.919309
20.809741	1269.339331	14.924327
20.882143	1248.963333	14.929344
20.894773	1258.925714	14.934362
20.856480	1246.622027	14.939379
20.804003	1257.084914	14.944397
20.978893	1236.291893	14.949415
20.890726	1238.693184	14.954432
20.704760	1267.229297	14.959450
20.738933	1252.834491	14.964467
20.823912	1244.312001	14.969485
20.722046	1262.051812	14.974503
20.879137	1246.876937	14.979520
20.976425	1247.427933	14.984538
20.631655	1238.707925	14.989555
21.069838	1267.652586	14.994573
21.043732	1268.751114	14.999591
21.136620	1253.662808	15.004608
20.985546	1269.162568	15.009626
21.186445	1274.605038	15.014643
20.996003	1261.486422	15.019661
21.173382	1256.996919	15.024679
21.241903	1267.358144	15.029696
20.948948	1266.485297	15.034714
21.137075	1270.247494	15.039731
21.307898	1280.790890	15.044749
21.152008	1275.227289	15.049767
21.415694	1280.817125	15.054784
21.042828	1293.952153	15.059802
21.282849	1274.215491	15.064819
21.351463	1257.985299	15.069837
21.508907	1261.713893	15.074855
21.710981	1273.662123	15.079872
21.285668	1299.344037	15.084890
21.357999	1285.449077	15.089907
21.390503	1266.574871	15.094925
21.251506	1282.259120	15.099943
21.551754	1256.669109	15.104960
21.117629	1271.804129	15.109978
21.281232	1277.990484	15.114995
21.346124	1267.719644	15.120013
21.288420	1262.202800	15.125031
21.505629	1267.787912	15.130048
21.175254	1276.131986	15.135066
21.035712	1269.381908	15.140083
21.070225	1284.426409	15.145101
21.299691	1303.624843	15.150119
21.767181	1286.254939	15.155136
21.289643	1299.611651	15.160154
21.521458	1300.911499	15.165171
21.613290	1292.841091	15.170189
21.366909	1315.723340	15.175207
21.709796	1306.786629	15.180224
21.755103	1295.281203	15.185242
22.030536	1289.446170	15.190259
21.892700	1309.106593	15.195277
22.007767	1324.782751	15.200295
22.413830	1309.669599	15.205312
22.144012	1297.319014	15.210330
21.938428	1299.174593	15.215347
22.029078	1308.191260	15.220365
22.070408	1299.524610	15.225383
22.009742	1294.671574	15.230400
22.095940	1302.784754	15.235418
22.225274	1296.844463	15.240435
22.314295	1304.187376	15.245453
21.959725	1278.446544	15.250471
22.192897	1285.339939	15.255488
21.786165	1283.185704	15.260506
22.010893	1280.247553	15.265523
22.165785	1279.559397	15.270541
22.207311	1299.911062	15.275559
22.471276	1304.761170	15.280576
22.178931	1289.578062	15.285594
22.379057	1276.117003	15.290611
22.379606	1290.363472	15.295629
22.014945	1279.275233	15.300647
22.252707	1279.531524	15.305664
22.187342	1289.765219	15.310682
21.909101	1294.638896	15.315699
22.280683	1280.146880	15.320717
22.215350	1283.320700	15.325735
22.360169	1297.255704	15.330752
22.261033	1288.233719	15.335770
22.224808	1288.093265	15.340787
22.406818	1290.291588	15.345805
22.196844	1279.679244	15.350823
22.457978	1284.675349	15.355840
22.217418	1285.989689	15.360858
22.415148	1282.533581	15.365875
22.521173	1293.110228	15.370893
22.118352	1307.017165	15.375911
22.240427	1290.726443	15.380928
22.431376	1298.818276	15.385946
22.379806	1316.828022	15.390963
22.521851	1310.749337	15.395981
22.748819	1322.583183	15.400999
22.776722	1337.446094	15.406016
22.800891	1329.606385	15.411034
22.617940	1316.926344	15.416051
22.830737	1331.748561	15.421069
22.655657	1322.437699	15.426087
22.816174	1307.809118	15.431104
22.644942	1321.666482	15.436122
22.739255	1323.857653	15.441139
22.818859	1312.646083	15.446157
22.831850	1316.006920	15.451175
23.127385	1330.066030	15.456192
23.077134	1323.453007	15.461210
23.076647	1323.653516	15.466227
23.057467	1308.839719	15.471245
22.803438	1322.276516	15.476263
22.640295	1311.768097	15.481280
23.063335	1344.545131	15.486298
23.067681	1341.885064	15.491315
23.449382	1341.699457	15.496333
23.183194	1342.010788	15.501351
23.267206	1347.383545	15.506368
23.269887	1345.651788	15.511386
23.144143	1345.714567	15.516403
23.442696	1340.861591	15.521421
23.101616	1346.619385	15.526439
23.566656	1344.760545	15.531456
23.479253	1323.057525	15.536474
22.914174	1313.858841	15.541491
23.315103	1328.515155	15.546509
23.491487	1324.899512	15.551527
23.601918	1320.834738	15.556544
23.530680	1321.800898	15.561562
23.282977	1324.058527	15.566579
23.460830	1319.809816	15.571597
23.397596	1310.561464	15.576615
23.796629	1315.664879	15.581632
23.863257	1313.598618	15.586650
23.770057	1321.074088	15.591667
23.697271	1291.882828	15.596685
23.460595	1294.320478	15.601703
23.301353	1302.118985	15.606720
23.380662	1288.488063	15.611738
23.351345	1307.514946	15.616755
23.637634	1312.320825	15.621773
23.821867	1329.636752	15.626791
24.065923	1337.886819	15.631808
23.659756	1338.057441	15.636826
23.755968	1336.099352	15.641843
23.879249	1328.497143	15.646861
23.978908	1342.666667	15.651879
23.875990	1331.406130	15.656896
23.849689	1323.876564	15.661914
23.844721	1322.900427	15.666931
23.998577	1332.705396	15.671949
23.847697	1338.349295	15.676967
23.823604	1327.474069	15.681984
23.957976	1350.867826	15.687002
23.761276	1337.029774	15.692019
24.101088	1326.067155	15.697037
23.897908	1348.814589	15.702055
23.734901	1330.131336	15.707072
24.100497	1331.407406	15.712090
24.010069	1363.679803	15.717107
24.005946	1335.294349	15.722125
23.869096	1330.195191	15.727143
23.876177	1334.863893	15.732160
23.942017	1345.782080	15.737178
24.127038	1342.464347	15.742195
24.166239	1346.582889	15.747213
24.376212	1348.799330	15.752231
24.549554	1363.814375	15.757248
24.571228	1347.646753	15.762266
24.145352	1342.943404	15.767283
24.892736	1332.973421	15.772301
24.445529	1331.908492	15.777319
24.069307	1316.660200	15.782336
24.587977	1312.894023	15.787354
24.205614	1333.079812	15.792371
24.489088	1351.076644	15.797389
24.435393	1351.911294	15.802407
24.776806	1335.976708	15.807424
24.623552	1359.236554	15.812442
24.231538	1360.904888	15.817459
24.862865	1342.592898	15.822477
24.931182	1347.209565	15.827495
24.666511	1344.899592	15.832512
24.982740	1348.639557	15.837530
24.765217	1361.568699	15.842547
24.631559	1326.778477	15.847565
24.554452	1331.538926	15.852583
24.710118	1349.756437	15.857600
24.891151	1340.054508	15.862618
24.701248	1356.704507	15.867635
24.809615	1346.208762	15.872653
24.493908	1341.878948	15.877671
24.503246	1366.389301	15.882688
24.776477	1359.435372	15.887706
24.545067	1360.903387	15.892723
24.841810	1342.544546	15.897741
24.748290	1357.832864	15.902759
24.748726	1356.954431	15.907776
25.101197	1357.724816	15.912794
24.888864	1385.734722	15.917811
24.998811	1365.833554	15.922829
25.316651	1366.496302	15.927847
25.130848	1379.165452	15.932864
25.381027	1383.559798	15.937882
25.368878	1382.310496	15.942899
25.618062	1354.752732	15.947917
25.570449	1355.932165	15.952935
25.217536	1368.777805	15.957952
25.255229	1354.787840	15.962970
25.061540	1345.306752	15.967987
25.267950	1346.230672	15.973005
25.337280	1343.895222	15.978023
25.498865	1346.772266	15.983040
25.796152	1346.393176	15.988058
25.408271	1354.858877	15.993075
25.453212	1340.402774	15.998093
25.477199	1324.555095	16.003111
25.355366	1337.809172	16.008128
25.657171	1339.506123	16.013146
25.421841	1350.417403	16.018163
25.707051	1358.775615	16.023181
25.742030	1336.470004	16.028199
25.300435	1352.391590	16.033216
25.447955	1372.755063	16.038234
25.324597	1380.672160	16.043251
25.721300	1373.698017	16.048269
25.603571	1367.988739	16.053287
25.489526	1383.464585	16.058304
25.790648	1389.382549	16.063322
25.388021	1368.887297	16.068339
25.438846	1369.097532	16.073357
25.453769	1387.057011	16.078375
25.698854	1384.194002	16.083392
25.965721	1396.127193	16.088410
25.955454	1415.926183	16.093427
26.213560	1407.673548	16.098445
26.351124	1399.466619	16.103463
26.045819	1399.766505	16.108480
25.870806	1378.557893	16.113498
25.945698	1397.432462	16.118515
25.997846	1401.373624	16.123533
26.028036	1412.773135	16.128551
25.893829	1403.987436	16.133568
26.435948	1384.457148	16.138586
26.272182	1416.952162	16.143603
26.133434	1419.506098	16.148621
26.089479	1413.231488	16.153639
26.105033	1406.973516	16.158656
26.360718	1404.938781	16.163674
26.148072	1390.719248	16.168691
26.215599	1393.029692	16.173709
26.463674	1383.405810	16.178727
26.393652	1402.604166	16.183744
26.251352	1408.947499	16.188762
26.401724	1397.904939	16.193779
25.908382	1388.981593	16.198797
26.308747	1403.547935	16.203815
26.242929	1417.013837	16.208832
26.964702	1441.082832	16.213850
26.755502	1445.541104	16.218867
26.809317	1425.605345	16.223885
26.795091	1397.229809	16.228903
26.078455	1413.699650	16.233920
26.702868	1422.443279	16.238938
26.465565	1419.769994	16.243955
26.945975	1421.405754	16.248973
27.046981	1432.580732	16.253991
27.142766	1413.106551	16.259008
26.856323	1402.351969	16.264026
26.837917	1411.221697	16.269043
26.723225	1389.754634	16.274061
27.063200	1378.872444	16.279079
26.826298	1395.031053	16.284096
26.893255	1403.940299	16.289114
26.893009	1399.632632	16.294131
26.669502	1397.088341	16.299149
27.360843	1415.326538	16.304167
26.961289	1423.947714	16.309184
27.234725	1410.952465	16.314202
27.062954	1421.158763	16.319219
27.247086	1420.150091	16.324237
27.325998	1436.758313	16.329255
27.132767	1427.217957	16.334272
26.749688	1401.316607	16.339290
27.143238	1409.960222	16.344307
27.302256	1423.740373	16.349325
27.483079	1438.260172	16.354343
27.476147	1426.875459	16.359360
27.251180	1415.071376	16.364378
27.695747	1417.161088	16.369395
27.425976	1437.230300	16.374413
27.318474	1440.879717	16.379431
27.429201	1428.402374	16.384448
27.536131	1410.525800	16.389466
27.338734	1425.780280	16.394483
27.355378	1422.331434	16.399501
27.645286	1428.357344	16.404519
27.455461	1435.324939	16.409536
27.647480	1425.553833	16.414554
27.643173	1414.971764	16.419571
27.487851	1421.924008	16.424589
27.676160	1419.047348	16.429607
27.429685	1426.127132	16.434624
27.350687	1419.090863	16.439642
27.424298	1427.798479	16.444659
27.515248	1420.112513	16.449677
27.443751	1419.557409	16.454695
27.533100	1452.536931	16.459712
27.572511	1442.636146	16.464730
27.568974	1460.525058	16.469747
27.514886	1454.942699	16.474765
27.769031	1444.728635	16.479783
27.725201	1436.670041	16.484800
27.835992	1464.249711	16.489818
28.233607	1480.439745	16.494835
28.263075	1478.276180	16.499853
28.265843	1451.237401	16.504871
27.927792	1458.765603	16.509888
28.160551	1467.571913	16.514906
28.476951	1467.557889	16.519923
28.467375	1463.365106	16.524941
28.297833	1445.335601	16.529959
28.039494	1452.863026	16.534976
28.069381	1430.306405	16.539994
28.257407	1449.209576	16.545011
28.300516	1475.452030	16.550029
28.522665	1476.116820	16.555047
28.381776	1480.955951	16.560064
28.638495	1477.680266	16.565082
28.413989	1466.129850	16.570099
28.467227	1475.750500	16.575117
28.451747	1476.360977	16.580135
28.467869	1485.493781	16.585152
28.728672	1488.458370	16.590170
28.615039	1464.110362	16.595187
28.296526	1456.691801	16.600205
28.671530	1472.408701	16.605223
28.856385	1478.591626	16.610240
28.773235	1462.869162	16.615258
28.812251	1477.467243	16.620275
29.084331	1474.180754	16.625293
28.940928	1456.060322	16.630311
28.622030	1432.653858	16.635328
28.983756	1444.907852	16.640346
28.724214	1455.211926	16.645363
28.587042	1448.365040	16.650381
29.147212	1455.354147	16.655399
29.100912	1467.926613	16.660416
29.161732	1462.872484	16.665434
29.096045	1464.029819	16.670451
28.950046	1474.698818	16.675469
29.034623	1456.913659	16.680487
29.048264	1479.366852	16.685504
29.173584	1485.570935	16.690522
29.351202	1475.633612	16.695539
29.131514	1462.835236	16.700557
29.287619	1464.143181	16.705575
29.183666	1473.246717	16.710592
28.916359	1483.843860	16.715610
29.297682	1457.483098	16.720627
28.995374	1455.146559	16.725645
29.568812	1471.670834	16.730663
29.260008	1474.077035	16.735680
28.936012	1466.360130	16.740698
29.012020	1476.216138	16.745715
28.956193	1477.411698	16.750733
29.152023	1466.329300	16.755751
29.444994	1491.618785	16.760768
29.670301	1506.621151	16.765786
29.734875	1506.076327	16.770803
29.535781	1506.371849	16.775821
30.050283	1488.869074	16.780839
30.095705	1493.124589	16.785856
29.747915	1498.830903	16.790874
29.874988	1471.788177	16.795891
29.699102	1457.313842	16.800909
29.553621	1451.582450	16.805927
29.771857	1484.947149	16.810944
29.634086	1500.676094	16.815962
30.006143	1492.818764	16.820979
30.062202	1501.989752	16.825997
30.013821	1504.649806	16.831015
29.745918	1514.554011	16.836032
29.892131	1507.904900	16.841050
30.152851	1479.449237	16.846067
29.796851	1501.099760	16.851085
30.221659	1501.271418	16.856103
29.819676	1492.212665	16.861120
29.767254	1494.302054	16.866138
30.319575	1497.256651	16.871155
30.059788	1504.422707	16.876173
30.238813	1481.201250	16.881191
30.309263	1487.370414	16.886208
29.881477	1493.504913	16.891226
30.234092	1486.107589	16.896243
30.133845	1487.364513	16.901261
30.287924	1479.633447	16.906279
30.229437	1504.615562	16.911296
30.445637	1516.527797	16.916314
30.627030	1526.685152	16.921331
30.527773	1523.892699	16.926349
30.233579	1501.928878	16.931367
30.731307	1502.196631	16.936384
30.413984	1527.705505	16.941402
30.654585	1523.359971	16.946419
30.503245	1521.725678	16.951437
30.338657	1533.470784	16.956455
30.496278	1519.416962	16.961472
30.716335	1520.386856	16.966490
30.616969	1539.748565	16.971507
30.774670	1521.112257	16.976525
30.833061	1517.508786	16.981543
30.817501	1521.109276	16.986560
30.732455	1510.168123	16.991578
31.108429	1517.732066	16.996595
30.726620	1532.914591	17.001613
30.621278	1508.111107	17.006631
30.763802	1524.898733	17.011648
30.569215	1532.384173	17.016666
30.886575	1524.866994	17.021683
30.797002	1546.280583	17.026701
31.170181	1543.101166	17.031719
31.214037	1550.685469	17.036736
30.896233	1547.603507	17.041754
31.476212	1538.929975	17.046771
31.333968	1550.281526	17.051789
31.301321	1546.947368	17.056807
31.590332	1538.089489	17.061824
31.546619	1537.818704	17.066842
31.393623	1542.196963	17.071859
31.427498	1542.597657	17.076877
31.493483	1555.531774	17.081895
31.408064	1549.937436	17.086912
31.049309	1540.067255	17.091930
31.438064	1545.474646	17.096947
31.342432	1550.573585	17.101965
31.160898	1537.961320	17.106983
31.529466	1556.428085	17.112000
31.536154	1547.988231	17.117018
31.450029	1529.759744	17.122035
31.515032	1555.973527	17.127053
31.470668	1584.414011	17.132071
31.721770	1580.732134	17.137088
32.043919	1571.061551	17.142106
32.160285	1575.540159	17.147123
31.892076	1588.771210	17.152141
31.812477	1581.686649	17.157159
32.270900	1571.087934	17.162176
31.823757	1570.851932	17.167194
32.083361	1569.267318	17.172211
32.149791	1583.758728	17.177229
31.768689	1592.767416	17.182247
32.328800	1583.927690	17.187264
32.012023	1561.121634	17.192282
32.211145	1567.364429	17.197299
32.098703	1585.184396	17.202317
32.065297	1582.682167	17.207335
32.188119	1563.038205	17.212352
32.015756	1566.166103	17.217370
32.077098	1581.993499	17.222387
31.887345	1582.470116	17.227405
31.990154	1561.919323	17.232423
32.268357	1568.163909	17.237440
31.971667	1573.560198	17.242458
32.331038	1585.567995	17.247475
32.420830	1588.882153	17.252493
32.509027	1584.734486	17.257511
32.795641	1578.555247	17.262528
32.702541	1599.575384	17.267546
33.001951	1604.284228	17.272563
32.879480	1589.817079	17.277581
32.739092	1574.453392	17.282599
33.091618	1552.220163	17.287616
32.553407	1569.185276	17.292634
32.886905	1572.596431	17.297651
32.584689	1560.868471	17.302669
32.638855	1549.963425	17.307687
33.223141	1564.093415	17.312704
32.623458	1580.505237	17.317722
32.949795	1575.963276	17.322739
32.997661	1600.737757	17.327757
32.827023	1589.778710	17.332775
33.071711	1584.663848	17.337792
33.025464	1595.879712	17.342810
33.268866	1590.483035	17.347827
33.148030	1596.484289	17.352845
32.917187	1593.568520	17.357863
33.162327	1575.340834	17.362880
33.374605	1590.014306	17.367898
33.322002	1612.136981	17.372915
33.077011	1594.647215	17.377933
33.177511	1583.331130	17.382951
33.651685	1593.805424	17.387968
33.560627	1598.983134	17.392986
33.383188	1583.349931	17.398003
33.300624	1575.021248	17.403021
33.254066	1577.786207	17.408039
33.174952	1590.998510	17.413056
33.131650	1592.016357	17.418074
33.354785	1597.569516	17.423091
33.328454	1604.423377	17.428109
33.265927	1602.382848	17.433127
33.376714	1612.448013	17.438144
33.613421	1628.668830	17.443162
33.573134	1633.722044	17.448179
33.897876	1631.601475	17.453197
33.518332	1618.484576	17.458215
33.759484	1627.334563	17.463232
33.926333	1617.467712	17.468250
33.798138	1616.769936	17.473267
33.949358	1608.596064	17.478285
33.830751	1611.216669	17.483303
34.091872	1606.063856	17.488320
33.767371	1621.723804	17.493338
33.909820	1624.926238	17.498355
34.261666	1624.122467	17.503373
34.382209	1650.956630	17.508391
34.679133	1629.160734	17.513408
34.600267	1618.414405	17.518426
34.646134	1625.185199	17.523443
34.254381	1611.444767	17.528461
34.328610	1610.615923	17.533479
34.821353	1618.454358	17.538496
34.495311	1607.447864	17.543514
34.514106	1599.785638	17.548531
34.459034	1610.669283	17.553549
34.405809	1612.380259	17.558567
34.415185	1602.418009	17.563584
34.317446	1599.872286	17.568602
34.706580	1596.749460	17.573619
34.488314	1612.061598	17.578637
34.393121	1608.206773	17.583655
34.510080	1603.822901	17.588672
34.666083	1606.247568	17.593690
34.653019	1607.657973	17.598707
34.849962	1620.712305	17.603725
34.763129	1629.367825	17.608743
34.936762	1626.751274	17.613760
34.986492	1626.712139	17.618778
34.933069	1628.085524	17.623795
34.925923	1625.628937	17.628813
34.968394	1625.753763	17.633831
35.161752	1620.976534	17.638848
34.934042	1634.662253	17.643866
34.650927	1629.680256	17.648883
35.047140	1625.394295	17.653901
34.974616	1641.367076	17.658919
35.006917	1633.955501	17.663936
35.116115	1629.858376	17.668954
35.123345	1609.762689	17.673971
35.075564	1628.720400	17.678989
34.962168	1648.622148	17.684007
35.144719	1646.196698	17.689024
35.147543	1643.293082	17.694042
35.218740	1648.969969	17.699059
35.531935	1654.788030	17.704077
35.659076	1665.890271	17.709095
35.776381	1655.564948	17.714112
35.732215	1665.539539	17.719130
35.536508	1659.096932	17.724147
35.642442	1658.033859	17.729165
35.464938	1676.912989	17.734183
35.748597	1662.153115	17.739200
35.866243	1644.300574	17.744218
35.664968	1653.942829	17.749235
35.986524	1669.083256	17.754253
35.841394	1674.923236	17.759271
35.616436	1649.700503	17.764288
35.786182	1647.239283	17.769306
35.653440	1662.034293	17.774323
35.449850	1647.141118	17.779341
35.804331	1660.833584	17.784359
36.173270	1677.797992	17.789376
36.093920	1676.070799	17.794394
36.240785	1664.617885	17.799411
36.385302	1682.854167	17.804429
36.127095	1689.524777	17.809447
36.099201	1675.482378	17.814464
36.161849	1689.333210	17.819482
36.141461	1690.049012	17.824499
36.296104	1677.647657	17.829517
36.155001	1676.428596	17.834535
36.258484	1671.429442	17.839552
36.553795	1686.501502	17.844570
36.221389	1682.263898	17.849587
36.727551	1657.670572	17.854605
36.409699	1677.589514	17.859623
36.383244	1688.135876	17.864640
36.137376	1685.672479	17.869658
36.272765	1686.826025	17.874675
36.720209	1701.165430	17.879693
36.909796	1711.984115	17.884711
36.994661	1723.723274	17.889728
37.211577	1707.795493	17.894746
36.817704	1703.949261	17.899763
37.337447	1712.320081	17.904781
37.095676	1687.393115	17.909799
37.350654	1681.675562	17.914816
37.212860	1692.332433	17.919834
37.084139	1678.087054	17.924851
37.352181	1662.772690	17.929869
37.110134	1668.859344	17.934887
37.114517	1654.989250	17.939904
37.241800	1654.723171	17.944922
37.103099	1669.939854	17.949939
37.023740	1658.664948	17.954957
36.851730	1683.877291	17.959975
36.516883	1689.073668	17.964992
37.176171	1682.959155	17.970010
37.012040	1683.487239	17.975027
37.261347	1703.250988	17.980045
37.350672	1698.672188	17.985063
37.294199	1711.996676	17.990080
37.472322	1722.338917	17.995098
37.442630	1708.152326	18.000115
37.512423	1700.342971	18.005133
37.466833	1719.802986	18.010151
37.775143	1737.173364	18.015168
37.913832	1745.439784	18.020186
37.891933	1728.367237	18.025203
37.854456	1726.612946	18.030221
37.923556	1735.469089	18.035239
38.111675	1723.657319	18.040256
38.122961	1723.548470	18.045274
38.116833	1705.845517	18.050291
37.942689	1690.629585	18.055309
38.247981	1713.210284	18.060327
38.220227	1694.492820	18.065344
37.979646	1707.596008	18.070362
38.141166	1704.535474	18.075379
38.119240	1700.252266	18.080397
37.983051	1726.640897	18.085415
38.238397	1734.708840	18.090432
38.769124	1724.212417	18.095450
38.283851	1729.458759	18.100467
38.560467	1725.058507	18.105485
38.540165	1731.061996	18.110503
38.293858	1717.466198	18.115520
38.829401	1724.850758	18.120538
38.533611	1731.096779	18.125555
38.495364	1710.430542	18.130573
38.502900	1721.102976	18.135591
38.429348	1737.676396	18.140608
38.765566	1717.224985	18.145626
38.651477	1726.381124	18.150643
38.962609	1716.850430	18.155661
38.598109	1729.682148	18.160679
38.491601	1728.945750	18.165696
38.862256	1714.000225	18.170714
38.410268	1710.563119	18.175731
38.308722	1722.067290	18.180749
38.372316	1732.573808	18.185767
38.499921	1755.086214	18.190784
38.714844	1749.828510	18.195802
38.754373	1747.401290	18.200819
38.988573	1748.947977	18.205837
39.099488	1768.385538	18.210855
39.288840	1762.992811	18.215872
39.598864	1743.349961	18.220890
39.437187	1748.442166	18.225907
39.657881	1755.793945	18.230925
39.537731	1762.022566	18.235943
39.357878	1744.620466	18.240960
39.737646	1730.210613	18.245978
39.488032	1748.393427	18.250995
39.484033	1744.992497	18.256013
39.583162	1736.077022	18.261031
39.454942	1737.962085	18.266048
39.427106	1745.181932	18.271066
39.450431	1740.855119	18.276083
39.618781	1728.722367	18.281101
39.615896	1742.117340	18.286119
39.591302	1773.107735	18.291136
39.965719	1763.618907	18.296154
39.903059	1761.139786	18.301171
40.129198	1766.935473	18.306189
40.041476	1771.197323	18.311207
39.839535	1764.631515	18.316224
40.110689	1782.851811	18.321242
39.802288	1782.387407	18.326259
39.909373	1765.880591	18.331277
39.784827	1773.670947	18.336295
39.704304	1776.584833	18.341312
40.117375	1764.619542	18.346330
39.784883	1772.294192	18.351347
40.176856	1765.843975	18.356365
40.411427	1778.305138	18.361383
40.164965	1791.711868	18.366400
40.607568	1783.124865	18.371418
40.476395	1796.811898	18.376435
40.683666	1801.240025	18.381453
41.233562	1782.107770	18.386471
40.515811	1766.394408	18.391488
40.519087	1752.608054	18.396506
40.588773	1775.238110	18.401523
40.797826	1776.328222	18.406541
40.853525	1771.072024	18.411559
40.674884	1766.490547	18.416576
41.051052	1757.539218	18.421594
40.897784	1768.373270	18.426611
41.000590	1783.844782	18.431629
40.993959	1777.101841	18.436647
40.878224	1779.189823	18.441664
41.247402	1774.775442	18.446682
41.264348	1780.750753	18.451699
41.136980	1763.175916	18.456717
41.002356	1761.057534	18.461735
41.173178	1793.941274	18.466752
41.495095	1770.945814	18.471770
41.075628	1761.246119	18.476787
41.052566	1781.311422	18.481805
41.497552	1779.635437	18.486823
41.329591	1787.234490	18.491840
41.894376	1776.777966	18.496858
41.593689	1785.654899	18.501875
41.321439	1783.634242	18.506893
41.445079	1777.100435	18.511911
41.529892	1787.328932	18.516928
41.610586	1772.566574	18.521946
41.518915	1787.589222	18.526963
41.808572	1780.009877	18.531981
41.875931	1771.429388	18.536999
41.575996	1791.914202	18.542016
41.733428	1775.612694	18.547034
41.378719	1787.623715	18.552051
41.356174	1793.518467	18.557069
41.541128	1790.331136	18.562087
41.768192	1816.400104	18.567104
42.028486	1807.738117	18.572122
41.890941	1802.076035	18.577139
42.065828	1806.494952	18.582157
42.165361	1815.773095	18.587175
41.838500	1825.743924	18.592192
42.298399	1808.168723	18.597210
42.102267	1801.721797	18.602227
42.333253	1811.013345	18.607245
42.466255	1797.946212	18.612263
42.197191	1809.579488	18.617280
42.291791	1814.859537	18.622298
42.537258	1825.157163	18.627315
42.544360	1814.496765	18.632333
43.287281	1823.840509	18.637351
42.591626	1821.164268	18.642368
42.761680	1811.553503	18.647386
42.593670	1805.200727	18.652403
42.538318	1814.912848	18.657421
42.850857	1800.710751	18.662439
42.620748	1813.873115	18.667456
42.718772	1824.164303	18.672474
42.922307	1824.696386	18.677491
42.891585	1820.353585	18.682509
43.045958	1823.666668	18.687527
42.879492	1841.746204	18.692544
43.207571	1835.551449	18.697562
43.023770	1817.111639	18.702579
43.150167	1825.524398	18.707597
43.323134	1827.436555	18.712615
43.297511	1826.203910	18.717632
43.212207	1815.006923	18.722650
43.122967	1834.951172	18.727667
43.401871	1820.085063	18.732685
43.404727	1801.197581	18.737703
43.280103	1827.268200	18.742720
43.458892	1826.094769	18.747738
43.556039	1805.844820	18.752755
43.227846	1833.446527	18.757773
43.311407	1834.418628	18.762791
43.218364	1840.047446	18.767808
43.591794	1847.044763	18.772826
43.781472	1862.199204	18.777843
43.463714	1855.505182	18.782861
44.049772	1845.655213	18.787879
43.873574	1862.542817	18.792896
43.951439	1845.055996	18.797914
43.876782	1846.729111	18.802931
43.959400	1861.878610	18.807949
43.896820	1843.022161	18.812967
44.039884	1843.074176	18.817984
43.882429	1864.070771	18.823002
44.335870	1868.081245	18.828019
43.945351	1865.502575	18.833037
44.746474	1883.873361	18.838055
44.473636	1900.264675	18.843072
44.787305	1885.950721	18.848090
44.578789	1857.149343	18.853107
44.228091	1850.964604	18.858125
44.563943	1866.140357	18.863143
44.603990	1870.578720	18.868160
44.600989	1856.423992	18.873178
44.666839	1849.492599	18.878195
44.398754	1873.023628	18.883213
44.515851	1874.176669	18.888231
44.506079	1873.466692	18.893248
44.531151	1866.812351	18.898266
44.540765	1869.555878	18.903283
44.383897	1874.366283	18.908301
44.457485	1887.899407	18.913319
44.594565	1896.701505	18.918336
44.753853	1903.723804	18.923354
45.285501	1890.588945	18.928371
44.906654	1908.884232	18.933389
44.953235	1891.948977	18.938407
45.211711	1915.369537	18.943424
44.829449	1904.738584	18.948442
45.188054	1918.269508	18.953459
45.318911	1925.982999	18.958477
45.761868	1915.288393	18.963495
45.410750	1925.350188	18.968512
45.479543	1921.291447	18.973530
45.481124	1915.809936	18.978547
45.357933	1925.684587	18.983565
45.663636	1930.772440	18.988583
45.688782	1944.401593	18.993600
45.631908	1929.008792	18.998618
45.853077	1931.193554	19.003635
45.474786	1922.192329	19.008653
45.900986	1920.314256	19.013671
45.633471	1931.824755	19.018688
45.688066	1938.123173	19.023706
45.715367	1920.442593	19.028723
45.820299	1913.575861	19.033741
45.898384	1921.254180	19.038759
45.925584	1929.540994	19.043776
46.217080	1953.925362	19.048794
46.322791	1934.405973	19.053811
46.289352	1944.378087	19.058829
46.482819	1949.972688	19.063847
46.705533	1955.870962	19.068864
46.407354	1927.472187	19.073882
46.771772	1906.703522	19.078899
46.370842	1909.054160	19.083917
46.418161	1907.256313	19.088935
46.791721	1927.134439	19.093952
46.091630	1923.189765	19.098970
46.929437	1929.020040	19.103987
46.683194	1939.530862	19.109005
46.884628	1928.591764	19.114023
46.578263	1942.870958	19.119040
46.875005	1957.077663	19.124058
47.096850	1959.196188	19.129075
46.654647	1944.086297	19.134093
47.062579	1946.626149	19.139111
46.865234	1939.139798	19.144128
46.545200	1945.764446	19.149146
46.887810	1936.049120	19.154163
46.717274	1932.881830	19.159181
46.950645	1961.196916	19.164199
46.978143	1978.913916	19.169216
47.279106	1988.001328	19.174234
47.448069	1983.874748	19.179251
47.339199	1989.575711	19.184269
47.371789	1978.862080	19.189287
47.473419	1968.076232	19.194304
47.004433	1965.817933	19.199322
47.428580	1969.605071	19.204339
47.385296	1983.019920	19.209357
47.838980	1986.675728	19.214375
47.858248	1972.880432	19.219392
47.445329	1979.369389	19.224410
47.641428	1991.495612	19.229427
47.744456	1996.757700	19.234445
48.165115	1983.843624	19.239463
48.442754	1990.028548	19.244480
48.369986	1990.110030	19.249498
48.345903	1975.069964	19.254515
48.441661	1974.456794	19.259533
48.367859	1968.775753	19.264551
48.095492	1960.541597	19.269568
48.202140	1953.627427	19.274586
48.491215	1945.033526	19.279603
48.019801	1962.385595	19.284621
48.273869	1974.643340	19.289639
48.500051	1978.159904	19.294656
48.448950	1981.108920	19.299674
48.569115	1966.781895	19.304691
48.418391	1991.916043	19.309709
48.461221	1982.897053	19.314727
48.694239	1974.462765	19.319744
48.643909	1974.650656	19.324762
48.907803	1972.022379	19.329779
48.704926	1972.913894	19.334797
48.532786	1969.942394	19.339815
48.717010	1976.159675	19.344832
48.410908	1991.629887	19.349850
48.473755	1987.021132	19.354867
49.079903	1990.738443	19.359885
48.797717	2008.533812	19.364903
49.291482	1999.591252	19.369920
48.961820	2003.905546	19.374938
49.062142	1997.016020	19.379955
49.169393	2000.344308	19.384973
49.512566	2016.873277	19.389991
49.292285	2025.650069	19.395008
49.369124	2032.986489	19.400026
49.806469	2005.312917	19.405043
49.548150	2003.836085	19.410061
49.690038	2005.996761	19.415079
49.641717	2023.217971	19.420096
49.500566	2022.372738	19.425114
49.643494	2010.846805	19.430131
49.470608	2017.291095	19.435149
49.806915	2021.277077	19.440167
49.831687	2038.663063	19.445184
49.522569	2055.511242	19.450202
49.793326	2031.649990	19.455219
49.721362	2040.713150	19.460237
49.891872	2049.224628	19.465255
50.109500	2051.045394	19.470272
49.932975	2035.274496	19.475290
50.033452	2031.019483	19.480307
50.120498	2070.697218	19.485325
50.029698	2078.977436	19.490343
49.737930	2060.296167	19.495360
50.318193	2070.412179	19.500378
50.743359	2048.765824	19.505395
50.507996	2065.412196	19.510413
50.571920	2058.215918	19.515431
50.995342	2055.785830	19.520448
50.607973	2073.588618	19.525466
50.567105	2059.439468	19.530483
50.654282	2075.973409	19.535501
50.787109	2073.058758	19.540519
51.025396	2065.570719	19.545536
50.762266	2074.568853	19.550554
51.394547	2083.323670	19.555571
51.556705	2098.755777	19.560589
51.147526	2061.319840	19.565607
51.275652	2035.251555	19.570624
51.467281	2053.838598	19.575642
51.055000	2057.752954	19.580659
50.928683	2066.620916	19.585677
51.288459	2065.648719	19.590695
51.517916	2076.959704	19.595712
51.358020	2079.015760	19.600730
51.467734	2065.227970	19.605747
51.622339	2087.644393	19.610765
51.533661	2079.320972	19.615783
51.625669	2090.448024	19.620800
51.598219	2084.013549	19.625818
51.992056	2083.068492	19.630835
51.652115	2062.791041	19.635853
51.209471	2078.926995	19.640871
51.748529	2088.697433	19.645888
51.524063	2081.819617	19.650906
51.679480	2081.969279	19.655923
51.965798	2106.883292	19.660941
51.958902	2118.707984	19.665959
52.191695	2121.777702	19.670976
51.889186	2109.802168	19.675994
52.087245	2111.636311	19.681011
52.480731	2124.928725	19.686029
52.454003	2123.774570	19.691047
52.421303	2115.732870	19.696064
52.224387	2101.212590	19.701082
52.418030	2111.650052	19.706099
52.403824	2095.985512	19.711117
52.314003	2116.803294	19.716135
52.695787	2136.354309	19.721152
52.411805	2137.419935	19.726170
52.748964	2143.311474	19.731187
52.931282	2153.061784	19.736205
52.714013	2136.550107	19.741223
52.712185	2146.432301	19.746240
52.939625	2155.701421	19.751258
53.017998	2138.087728	19.756275
53.389940	2122.514737	19.761293
52.994354	2131.086742	19.766311
53.207259	2132.739037	19.771328
52.641880	2142.007490	19.776346
52.871577	2146.900729	19.781363
53.524988	2161.579792	19.786381
52.982173	2164.069642	19.791399
53.414395	2164.570147	19.796416
53.574573	2171.212863	19.801434
53.635890	2174.980889	19.806451
53.978668	2177.143820	19.811469
53.756986	2159.029782	19.816487
53.737763	2154.472032	19.821504
53.874476	2170.852836	19.826522
53.673620	2173.454555	19.831539
53.843836	2161.702976	19.836557
53.898458	2152.347646	19.841575
53.953211	2141.200591	19.846592
54.147445	2159.669833	19.851610
54.070593	2157.013005	19.856627
54.175658	2151.228041	19.861645
53.950872	2170.007734	19.866663
54.477932	2146.018239	19.871680
54.015374	2140.684002	19.876698
54.296121	2167.033621	19.881715
54.363105	2184.844907	19.886733
54.162232	2186.834238	19.891751
54.849327	2171.520089	19.896768
54.771066	2183.427084	19.901786
54.653414	2169.918363	19.906803
54.741447	2159.024608	19.911821
54.750534	2177.547297	19.916839
55.046058	2187.565683	19.921856
54.706744	2173.978549	19.926874
54.690486	2160.147623	19.931891
54.898307	2157.075610	19.936909
54.723729	2177.230434	19.941927
54.749103	2168.207823	19.946944
55.167447	2163.926521	19.951962
54.851107	2153.774571	19.956979
55.262066	2176.618660	19.961997
55.159812	2212.447916	19.967015
55.048689	2199.884482	19.972032
55.274448	2195.131835	19.977050
55.501763	2193.759545	19.982067
55.715798	2207.408990	19.987085
55.546151	2217.222816	19.992103
55.760411	2197.384617	19.997120
55.718975	2196.841443	20.002138
55.790849	2203.737799	20.007155
56.083994	2210.352852	20.012173
55.873591	2205.743032	20.017191
55.690910	2191.958670	20.022208
55.875124	2196.290740	20.027226
56.181607	2200.225802	20.032243
55.986270	2179.162819	20.037261
55.768863	2193.133207	20.042279
56.278985	2180.473625	20.047296
56.099335	2178.988499	20.052314
55.872594	2199.451919	20.057331
56.245123	2205.946588	20.062349
55.959572	2206.830914	20.067367
56.109786	2198.615564	20.072384
56.194881	2219.902428	20.077402
56.545497	2233.782039	20.082419
56.575278	2223.182757	20.087437
55.982215	2229.120387	20.092455
56.404747	2223.916685	20.097472
56.677375	2228.789964	20.102490
56.789125	2245.708051	20.107507
56.997715	2249.442706	20.112525
56.819995	2245.350415	20.117543
57.233918	2259.886896	20.122560
57.186581	2261.909418	20.127578
57.101785	2245.150378	20.132595
57.502854	2235.817065	20.137613
56.962822	2250.324987	20.142631
57.415090	2263.814367	20.147648
57.299565	2243.574777	20.152666
57.158656	2231.835784	20.157683
57.050430	2238.465215	20.162701
57.156280	2253.485004	20.167719
57.428782	2279.269149	20.172736
57.588599	2261.924092	20.177754
57.631935	2260.427500	20.182771
57.818715	2274.261694	20.187789
57.639627	2265.547570	20.192807
57.847892	2258.939152	20.197824
58.085991	2270.875617	20.202842
58.034363	2259.636919	20.207859
58.283866	2258.437502	20.212877
58.226091	2266.713249	20.217895
58.165047	2271.018163	20.222912
58.156523	2262.997387	20.227930
58.062008	2264.468548	20.232947
58.455253	2251.056502	20.237965
58.559420	2261.616510	20.242983
58.008177	2257.408411	20.248000
58.509632	2267.771693	20.253018
58.458971	2264.949324	20.258035
58.573694	2244.535093	20.263053
58.595867	2266.817095	20.268071
58.692823	2293.083345	20.273088
58.484226	2297.844074	20.278106
58.895365	2283.456764	20.283123
58.807273	2293.681894	20.288141
58.529080	2303.811103	20.293159
58.872392	2298.486828	20.298176
58.994997	2288.121923	20.303194
58.620743	2296.862906	20.308211
59.088571	2289.015721	20.313229
58.881212	2309.748381	20.318247
59.017024	2326.545278	20.323264
59.152359	2325.260015	20.328282
59.066997	2330.393041	20.333299
59.498103	2313.484315	20.338317
59.320716	2324.819512	20.343335
59.006373	2326.293152	20.348352
59.590894	2333.194897	20.353370
59.703938	2368.871243	20.358387
60.262593	2354.091637	20.363405
59.733667	2331.678878	20.368423
59.871081	2334.574668	20.373440
60.004696	2351.833100	20.378458
59.989117	2376.493748	20.383475
60.021117	2351.057839	20.388493
60.190843	2344.519719	20.393511
60.106177	2342.860246	20.398528
60.256553	2348.747500	20.403546
60.087143	2355.008217	20.408563
60.696765	2339.820465	20.413581
60.439333	2340.799546	20.418599
60.414315	2369.563629	20.423616
60.355103	2346.867356	20.428634
60.389785	2342.228805	20.433651
60.733341	2335.583630	20.438669
60.614070	2343.008501	20.443687
60.962909	2352.902457	20.448704
60.775219	2338.092089	20.453722
60.670369	2348.208625	20.458739
61.250720	2366.857383	20.463757
61.207899	2356.298151	20.468775
60.951446	2355.792077	20.473792
61.046530	2354.936818	20.478810
60.969507	2379.306099	20.483827
60.997569	2370.993834	20.488845
60.956967	2351.973016	20.493863
61.138575	2364.087168	20.498880
61.302835	2349.895685	20.503898
61.497237	2363.661782	20.508915
61.432973	2390.372685	20.513933
61.567086	2399.866397	20.518951
61.486049	2400.038307	20.523968
61.770613	2377.596746	20.528986
61.718544	2399.536344	20.534003
61.756575	2407.673324	20.539021
61.535238	2406.232263	20.544039
61.368481	2393.810323	20.549056
61.910767	2413.719360	20.554074
62.059204	2427.327584	20.559091
62.387649	2415.534904	20.564109
62.292291	2428.481363	20.569127
62.423524	2437.877164	20.574144
62.640956	2414.838077	20.579162
62.578389	2408.698691	20.584179
62.575602	2409.196987	20.589197
62.683954	2418.520389	20.594215
62.724582	2420.491394	20.599232
62.774318	2405.793868	20.604250
62.707420	2399.841392	20.609267
62.915674	2413.020495	20.614285
62.904413	2415.202404	20.619303
62.716288	2409.973387	20.624320
63.363036	2383.172066	20.629338
62.960306	2399.665578	20.634355
62.837500	2409.574132	20.639373
63.020304	2397.886817	20.644391
62.727846	2414.000567	20.649408
63.221050	2418.081673	20.654426
63.489095	2427.366686	20.659443
63.368051	2440.343773	20.664461
63.339706	2428.567724	20.669479
63.477756	2430.823568	20.674496
63.454548	2446.007369	20.679514
63.684849	2453.834299	20.684531
63.643348	2439.362021	20.689549
63.584621	2423.259200	20.694567
63.374207	2434.587733	20.699584
63.622692	2426.655876	20.704602
63.857703	2451.888132	20.709619
64.061214	2460.782120	20.714637
64.143724	2462.724559	20.719655
63.909323	2443.780527	20.724672
64.167911	2447.634901	20.729690
64.229966	2469.733075	20.734707
64.324657	2457.682579	20.739725
64.468883	2439.744321	20.744743
64.232589	2450.442006	20.749760
64.009949	2464.038168	20.754778
63.765574	2483.793869	20.759795
64.253090	2478.966882	20.764813
64.497850	2466.161576	20.769831
64.525526	2488.395752	20.774848
64.911309	2486.949030	20.779866
64.972791	2500.035945	20.784883
65.322099	2507.956998	20.789901
65.284841	2502.354845	20.794919
65.131779	2497.863591	20.799936
65.486833	2481.779329	20.804954
64.906694	2492.951513	20.809971
65.276927	2527.497117	20.814989
65.533079	2516.876955	20.820007
65.229546	2504.503900	20.825024
65.358603	2500.944222	20.830042
65.627001	2507.469021	20.835059
65.532281	2501.276258	20.840077
65.287421	2509.332696	20.845095
65.294316	2505.359608	20.850112
65.643194	2521.904025	20.855130
65.637989	2550.608094	20.860147
65.985671	2546.652884	20.865165
66.421074	2539.834792	20.870183
66.030933	2550.948066	20.875200
66.508851	2529.437968	20.880218
66.368405	2524.953084	20.885235
66.470557	2545.267256	20.890253
66.348657	2545.193400	20.895271
66.272134	2530.873257	20.900288
66.278751	2527.322193	20.905306
66.751212	2531.292208	20.910323
66.677469	2526.146401	20.915341
66.984791	2531.071909	20.920359
66.736343	2534.360780	20.925376
66.641543	2519.044804	20.930394
66.555788	2559.830442	20.935411
66.630885	2563.762994	20.940429
66.952406	2548.450427	20.945447
66.984349	2559.756520	20.950464
67.263846	2561.899260	20.955482
67.280711	2560.671737	20.960499
67.150061	2571.304417	20.965517
67.634017	2552.125815	20.970535
67.267039	2556.826390	20.975552
67.155326	2552.791406	20.980570
67.350665	2562.917722	20.985587
67.401101	2592.742034	20.990605
67.362659	2583.514008	20.995623
67.415946	2596.268944	21.000640
67.962933	2591.236258	21.005658
67.951463	2579.072914	21.010675
67.681493	2578.951095	21.015693
68.133958	2586.130251	21.020711
68.159040	2586.158465	21.025728
68.200161	2567.623212	21.030746
67.893290	2594.724113	21.035763
67.775854	2611.472829	21.040781
68.207908	2599.854394	21.045799
68.064404	2608.288170	21.050816
68.517372	2619.489503	21.055834
68.383726	2608.524302	21.060851
68.250801	2616.227898	21.065869
68.771743	2636.318482	21.070887
68.798371	2639.424145	21.075904
68.902081	2632.517536	21.080922
68.845082	2648.536921	21.085939
68.983093	2635.877639	21.090957
69.317884	2637.439485	21.095975
69.005952	2650.850203	21.100992
69.116250	2629.499714	21.106010
69.245702	2628.214808	21.111027
69.066398	2648.177454	21.116045
69.204407	2642.216415	21.121063
69.235935	2637.896359	21.126080
68.984946	2635.787045	21.131098
69.588899	2666.849566	21.136115
69.828178	2676.384921	21.141133
69.721775	2668.765288	21.146151
69.484446	2666.677135	21.151168
69.608535	2673.518131	21.156186
69.875170	2664.874397	21.161203
69.744043	2653.915832	21.166221
69.707810	2681.501616	21.171239
69.978860	2711.432005	21.176256
70.303184	2689.331206	21.181274
70.607884	2684.532594	21.186291
70.649520	2698.685799	21.191309
70.537410	2698.118464	21.196327
70.481701	2696.245141	21.201344
71.030591	2703.007295	21.206362
70.761324	2691.931983	21.211379
70.554052	2684.142620	21.216397
70.586391	2679.232739	21.221415
70.593206	2690.044331	21.226432
70.603522	2680.570626	21.231450
70.774006	2698.081586	21.236467
71.135096	2724.826901	21.241485
71.289670	2706.519155	21.246503
70.997288	2704.328298	21.251520
71.220053	2715.618522	21.256538
71.446880	2709.600462	21.261555
71.053441	2726.968059	21.266573
71.585661	2721.059745	21.271591
71.121077	2713.939570	21.276608
71.294110	2713.883306	21.281626
71.497299	2741.129872	21.286643
71.184575	2758.921114	21.291661
71.894326	2743.809519	21.296679
71.781656	2744.407468	21.301696
71.907616	2739.811580	21.306714
71.886801	2740.849209	21.311731
71.821307	2770.694990	21.316749
72.259059	2760.978580	21.321767
72.393904	2757.901876	21.326784
72.367544	2773.079041	21.331802
72.451827	2748.753958	21.336819
72.197575	2763.374365	21.341837
72.427196	2777.987063	21.346855
72.528548	2770.194683	21.351872
72.534505	2763.818863	21.356890
72.693464	2749.386977	21.361907
72.702984	2755.782242	21.366925
72.862526	2762.462126	21.371943
73.228412	2769.517309	21.376960
73.174352	2779.806813	21.381978
73.386618	2794.260802	21.386995
73.314853	2775.275118	21.392013
73.510189	2776.490978	21.397031
73.327761	2768.349877	21.402048
73.622602	2761.922187	21.407066
73.543391	2780.994373	21.412083
73.239251	2798.524042	21.417101
73.728878	2777.151999	21.422119
73.520457	2777.473686	21.427136
73.690230	2782.998108	21.432154
73.807986	2786.371184	21.437171
73.542699	2786.470016	21.442189
73.763448	2782.014335	21.447207
73.711408	2807.413096	21.452224
73.799591	2798.217948	21.457242
74.033910	2797.108390	21.462259
73.849821	2812.520881	21.467277
73.781567	2828.378359	21.472295
74.044432	2836.931109	21.477312
74.338976	2837.968791	21.482330
74.341260	2848.633822	21.487347
74.341729	2856.629825	21.492365
74.741426	2859.319206	21.497383
74.940608	2842.916866	21.502400
74.988579	2829.304321	21.507418
75.214036	2841.625749	21.512435
74.973224	2855.001666	21.517453
75.134587	2856.056831	21.522471
75.185165	2866.226949	21.527488
75.154831	2868.617756	21.532506
75.564268	2848.900187	21.537523
75.585409	2860.321460	21.542541
75.459977	2864.633440	21.547559
75.417608	2861.989095	21.552576
75.329411	2866.942477	21.557594
75.757210	2867.220246	21.562611
75.723121	2862.868062	21.567629
75.870225	2861.941787	21.572647
76.164918	2866.263665	21.577664
75.748660	2878.664197	21.582682
76.313565	2893.701067	21.587699
76.191126	2907.183633	21.592717
76.558180	2888.892325	21.597735
76.651565	2869.586162	21.602752
76.727435	2878.730392	21.607770
76.974288	2879.674397	21.612787
76.710667	2888.717666	21.617805
76.588066	2868.019032	21.622823
77.199188	2869.138049	21.627840
76.955419	2880.614920	21.632858
77.043656	2861.776683	21.637875
76.884895	2882.160592	21.642893
77.164209	2892.574785	21.647911
77.164325	2877.836195	21.652928
76.914801	2866.794694	21.657946
77.106274	2882.157990	21.662963
77.080834	2893.072286	21.667981
77.230885	2870.787061	21.672999
77.257868	2875.905443	21.678016
76.996712	2887.587923	21.683034
77.494083	2874.263236	21.688051
77.670485	2899.074667	21.693069
77.782987	2912.645172	21.698087
78.081323	2925.159716	21.703104
77.426141	2920.229722	21.708122
77.801993	2899.131201	21.713139
77.781595	2915.474498	21.718157
77.748742	2912.117836	21.723175
77.831542	2911.400977	21.728192
77.497049	2935.062991	21.733210
77.984898	2951.787440	21.738227
78.140177	2949.314726	21.743245
78.124603	2951.336223	21.748263
78.605949	2963.890627	21.753280
78.437658	2955.996272	21.758298
78.549297	2961.948620	21.763315
78.202502	2975.559056	21.768333
78.662350	2976.696189	21.773351
78.948322	2973.840699	21.778368
78.800005	2990.191042	21.783386
79.379842	2979.112795	21.788403
79.002559	2987.594069	21.793421
79.337394	2993.263711	21.798439
79.810099	2977.794848	21.803456
79.665445	2989.230622	21.808474
80.210232	2967.828732	21.813491
80.137449	2980.663670	21.818509
79.978114	2975.136038	21.823527
79.775348	2967.834505	21.828544
79.726665	2979.218591	21.833562
80.087544	2974.437572	21.838579
80.049397	2979.421296	21.843597
80.093292	2969.434840	21.848615
80.497404	2988.724625	21.853632
80.148573	2978.957764	21.858650
80.086075	2953.256981	21.863667
80.145527	2990.467058	21.868685
80.326100	3011.833914	21.873703
80.438781	2995.489599	21.878720
80.465496	3016.316600	21.883738
80.374875	3012.187863	21.888755
80.371793	3017.914535	21.893773
80.647764	3038.503158	21.898791
80.877443	3023.400353	21.903808
80.935797	3045.697777	21.908826
81.089943	3029.007047	21.913843
81.127529	3031.450821	21.918861
81.440192	3024.818134	21.923879
81.358819	3043.335752	21.928896
81.400605	3058.542091	21.933914
81.809598	3056.095734	21.938931
81.982303	3047.308272	21.943949
81.921649	3054.196893	21.948967
81.935537	3043.774258	21.953984
81.944268	3060.929137	21.959002
82.301544	3066.396106	21.964019
82.273710	3059.578752	21.969037
82.399907	3060.690524	21.974055
82.554117	3046.455185	21.979072
82.399193	3037.747060	21.984090
82.427629	3051.503408	21.989107
82.186242	3073.068998	21.994125
82.015172	3054.078516	21.999143
82.225165	3038.840382	22.004160
81.934519	3070.328876	22.009178
82.276959	3070.541828	22.014195
82.741253	3077.391544	22.019213
82.323549	3101.520855	22.024231
82.814771	3099.767910	22.029248
82.784201	3110.484018	22.034266
83.287006	3122.422676	22.039283
83.234901	3111.575516	22.044301
82.861762	3116.315265	22.049319
83.172891	3117.430926	22.054336
83.257847	3117.594704	22.059354
83.357093	3106.945347	22.064371
83.785490	3119.099227	22.069389
83.664238	3128.863120	22.074407
84.046070	3150.365397	22.079424
84.281564	3139.528955	22.084442
84.391276	3125.773087	22.089459
84.430020	3134.432322	22.094477
84.105343	3136.827521	22.099495
84.377069	3135.805645	22.104512
84.401080	3133.635467	22.109530
84.600653	3112.512837	22.114547
84.612578	3118.772438	22.119565
84.587485	3134.896887	22.124583
84.766931	3138.851512	22.129600
84.706251	3129.838228	22.134618
84.458897	3107.522670	22.139635
84.881417	3124.121112	22.144653
84.913884	3159.824023	22.149671
84.946142	3169.704292	22.154688
84.800690	3162.260336	22.159706
85.065181	3144.787553	22.164723
84.902184	3162.014224	22.169741
84.726528	3182.164732	22.174759
85.180030	3173.498890	22.179776
85.246557	3188.517431	22.184794
85.600401	3189.950020	22.189811
85.688927	3185.982361	22.194829
85.376893	3218.628502	22.199847
85.952416	3207.107940	22.204864
86.058414	3207.269817	22.209882
85.972186	3228.996972	22.214899
85.837157	3218.828723	22.219917
86.092578	3224.346238	22.224935
86.364870	3230.759690	22.229952
86.599201	3240.496782	22.234970
86.597953	3242.169136	22.239987
86.878215	3245.116487	22.245005
86.785736	3243.796950	22.250023
87.095159	3236.989530	22.255040
86.840782	3250.492033	22.260058
86.860425	3239.638438	22.265075
87.063197	3248.739480	22.270093
86.888146	3251.711484	22.275111
87.168046	3251.381091	22.280128
87.179282	3246.890221	22.285146
87.552053	3268.744321	22.290163
87.758501	3268.451259	22.295181
87.409985	3269.021474	22.300199
87.802682	3259.730068	22.305216
87.650167	3263.621876	22.310234
87.490286	3263.053555	22.315251
88.101328	3271.685615	22.320269
87.869517	3286.699224	22.325287
88.127827	3308.563633	22.330304
88.152149	3305.284240	22.335322
88.395527	3293.668908	22.340339
88.347787	3299.794952	22.345357
88.186020	3308.777742	22.350375
88.345896	3299.353935	22.355392
88.317536	3295.244556	22.360410
88.386119	3332.971613	22.365427
88.504309	3318.170183	22.370445
88.477553	3332.668898	22.375463
89.069228	3328.571216	22.380480
88.974892	3312.531021	22.385498
88.871092	3323.262921	22.390515
88.850454	3356.545582	22.395533
88.742085	3353.480015	22.400551
89.279126	3354.059201	22.405568
89.548072	3347.061000	22.410586
89.281652	3367.646588	22.415603
89.559121	3375.788801	22.420621
89.714794	3376.878994	22.425639
90.049416	3388.643111	22.430656
90.074839	3389.434780	22.435674
90.101149	3370.710673	22.440691
90.263689	3377.973934	22.445709
90.421416	3382.011337	22.450727
90.276801	3361.177110	22.455744
90.387765	3390.480415	22.460762
90.163893	3387.403222	22.465779
90.822276	3371.183079	22.470797
90.420719	3375.917367	22.475815
90.966370	3401.396671	22.480832
90.819003	3405.453395	22.485850
90.893161	3402.856035	22.490867
91.238261	3400.341845	22.495885
91.381322	3393.764976	22.500903
91.716416	3397.167425	22.505920
91.568588	3393.634203	22.510938
91.511022	3392.969648	22.515955
91.569697	3383.866223	22.520973
91.363791	3391.500777	22.525991
91.755342	3396.710651	22.531008
91.572906	3401.939396	22.536026
91.841211	3396.555297	22.541043
91.967567	3410.826640	22.546061
91.710923	3430.303518	22.551079
91.954409	3420.124947	22.556096
92.202557	3416.909913	22.561114
92.296774	3433.971955	22.566131
92.366804	3416.909309	22.571149
92.461466	3428.196621	22.576167
92.546293	3450.878605	22.581184
92.871037	3447.013762	22.586202
92.580395	3461.254656	22.591219
93.058723	3446.885478	22.596237
92.879916	3448.525979	22.601255
93.003351	3449.372118	22.606272
93.006444	3444.148549	22.611290
93.209924	3470.997774	22.616307
93.426471	3475.499061	22.621325
93.456295	3464.840459	22.626343
93.426123	3486.109935	22.631360
93.597646	3467.972684	22.636378
93.360277	3467.485263	22.641395
93.514096	3488.606044	22.646413
93.480851	3507.517018	22.651431
93.658219	3500.288823	22.656448
94.454363	3504.892360	22.661466
93.915269	3509.511631	22.666483
94.338952	3495.376220	22.671501
94.270959	3512.739735	22.676519
94.407717	3513.167965	22.681536
94.650121	3517.067013	22.686554
94.557113	3515.586728	22.691571
95.017340	3528.971391	22.696589
94.944127	3548.504714	22.701607
94.944931	3542.287087	22.706624
95.120749	3517.643528	22.711642
95.102156	3531.888151	22.716659
95.162457	3522.873936	22.721677
95.078908	3513.437078	22.726695
95.064041	3533.193397	22.731712
95.400178	3549.373342	22.736730
95.445978	3555.954069	22.741747
95.534784	3544.236937	22.746765
95.588628	3557.756684	22.751783
95.598763	3570.555380	22.756800
95.875989	3557.083233	22.761818
95.704281	3567.091743	22.766835
95.796553	3565.107059	22.771853
95.830043	3576.948635	22.776871
96.270031	3576.371921	22.781888
95.989141	3566.264549	22.786906
96.026233	3597.197443	22.791923
96.460165	3597.825959	22.796941
96.513901	3605.772212	22.801959
96.526620	3610.191678	22.806976
96.880736	3616.670112	22.811994
96.863193	3614.658295	22.817011
96.951294	3626.325741	22.822029
97.448522	3644.231191	22.827047
97.212634	3648.186276	22.832064
97.639653	3641.122653	22.837082
97.439092	3635.547465	22.842099
97.548402	3632.934023	22.847117
97.507493	3626.475440	22.852135
98.019214	3658.447851	22.857152
98.152226	3653.396035	22.862170
98.262270	3661.148775	22.867187
98.278980	3657.928829	22.872205
98.536200	3666.486911	22.877223
98.598282	3676.453120	22.882240
98.632926	3651.479357	22.887258
98.581696	3665.759809	22.892275
98.784821	3666.697312	22.897293
98.936881	3659.247652	22.902311
98.643825	3650.351983	22.907328
98.637515	3648.535534	22.912346
98.735849	3664.785404	22.917363
99.070563	3655.396659	22.922381
99.128373	3671.198544	22.927399
99.148181	3691.020195	22.932416
99.099657	3678.565082	22.937434
98.777249	3688.636365	22.942451
99.264181	3692.819240	22.947469
99.414075	3692.477647	22.952487
99.614264	3711.892973	22.957504
99.620388	3718.017565	22.962522
99.338906	3740.042052	22.967539
99.814115	3723.731544	22.972557
99.863532	3744.599474	22.977575
99.771707	3753.118044	22.982592
100.013776	3740.960507	22.987610
99.960411	3769.950570	22.992627
100.502324	3788.388922	22.997645
100.888891	3764.202435	23.002663
100.863412	3780.271128	23.007680
101.481295	3765.222737	23.012698
100.935652	3754.864916	23.017715
101.102498	3776.661251	23.022733
101.415375	3778.687436	23.027751
101.305612	3768.155817	23.032768
101.470660	3747.726362	23.037786
101.802415	3767.376889	23.042803
101.673601	3745.540784	23.047821
101.944090	3753.449723	23.052839
101.776601	3772.677080	23.057856
102.148891	3757.692504	23.062874
102.068202	3767.190864	23.067891
102.405071	3786.747270	23.072909
102.610069	3764.130440	23.077927
102.129243	3760.127196	23.082944
102.316462	3758.072471	23.087962
102.324872	3772.530161	23.092979
102.444083	3776.916922	23.097997
102.567529	3761.499086	23.103015
102.400054	3785.167278	23.108032
102.575357	3777.574951	23.113050
102.870940	3796.562839	23.118067
102.687416	3817.449084	23.123085
102.609126	3815.659666	23.128103
102.707065	3817.208416	23.133120
103.237939	3826.243774	23.138138
103.400743	3845.879999	23.143155
103.314813	3848.652756	23.148173
103.553856	3855.432176	23.153191
103.516332	3865.521849	23.158208
103.720655	3866.884532	23.163226
103.806462	3867.688491	23.168243
103.786565	3886.776647	23.173261
103.850845	3878.432785	23.178279
103.990566	3873.106972	23.183296
104.336097	3883.689033	23.188314
104.309053	3909.143935	23.193331
104.673107	3902.820868	23.198349
104.750706	3897.887964	23.203367
104.723232	3919.849870	23.208384
105.187379	3913.946058	23.213402
104.998276	3915.545792	23.218419
105.101782	3937.993529	23.223437
105.117371	3922.443168	23.228455
105.429621	3930.850974	23.233472
105.516211	3937.801282	23.238490
105.913784	3926.287550	23.243507
105.873511	3910.253548	23.248525
105.867571	3905.963934	23.253543
105.617561	3940.225654	23.258560
105.996382	3958.397870	23.263578
105.779563	3951.296802	23.268595
106.021587	3944.958450	23.273613
106.375287	3954.328260	23.278631
106.286628	3971.117195	23.283648
106.679021	3969.367102	23.288666
106.664658	3991.547403	23.293683
106.599045	3994.140854	23.298701
106.863723	3970.058041	23.303719
106.937536	3979.791419	23.308736
106.967083	3972.742933	23.313754
107.494922	3978.108232	23.318771
107.381364	4000.420677	23.323789
107.555745	4014.000626	23.328807
107.529113	4009.499060	23.333824
107.663665	4006.270788	23.338842
107.662387	4019.146737	23.343859
107.782888	3998.311935	23.348877
108.076723	3996.688355	23.353895
107.629198	4002.782515	23.358912
107.925219	4001.672324	23.363930
108.287651	4012.803225	23.368947
108.125534	4037.909813	23.373965
108.358219	4037.755703	23.378983
108.559970	4024.852285	23.384000
108.826117	4013.532242	23.389018
108.665932	4023.596423	23.394035
108.455150	4040.500882	23.399053
108.725641	4038.222136	23.404071
108.952613	4044.811913	23.409088
108.657228	4034.634979	23.414106
108.962661	4051.149837	23.419123
108.801985	4090.650391	23.424141
109.492184	4090.417926	23.429159
109.636079	4083.558358	23.434176
109.737452	4074.809462	23.439194
109.893286	4077.597820	23.444211
109.612840	4105.042060	23.449229
110.055624	4106.978324	23.454247
110.068896	4104.503893	23.459264
109.997870	4116.890686	23.464282
110.076489	4126.358415	23.469299
110.437790	4121.356122	23.474317
110.484223	4121.883149	23.479335
110.750075	4123.767553	23.484352
110.657799	4135.511841	23.489370
111.119638	4157.043640	23.494387
110.640203	4152.808183	23.499405
111.293438	4147.060432	23.504423
110.889962	4150.483323	23.509440
111.469831	4170.132340	23.514458
111.614676	4185.108594	23.519475
111.583627	4181.240357	23.524493
111.957231	4160.789872	23.529511
111.677213	4164.944694	23.534528
111.861889	4179.830113	23.539546
111.939779	4184.026976	23.544563
112.367118	4191.519492	23.549581
112.240470	4192.850678	23.554599
112.338978	4194.822188	23.559616
112.471965	4199.390643	23.564634
112.695634	4193.139472	23.569651
112.686619	4214.231854	23.574669
113.052929	4226.516156	23.579687
112.711485	4233.188914	23.584704
112.924190	4227.289921	23.589722
113.296647	4231.218841	23.594739
112.979873	4222.511397	23.599757
113.303911	4235.079451	23.604775
113.089535	4251.044615	23.609792
113.363121	4260.666028	23.614810
113.774549	4259.113933	23.619827
113.624099	4265.579955	23.624845
114.254417	4263.007084	23.629863
114.336612	4268.972479	23.634880
114.097110	4293.672993	23.639898
114.667305	4297.069275	23.644915
114.373990	4295.855665	23.649933
114.456580	4288.151052	23.654951
114.756605	4274.296972	23.659968
114.874198	4286.251174	23.664986
115.067186	4305.128496	23.670003
114.816816	4320.467418	23.675021
115.227832	4309.342113	23.680039
115.351356	4311.035499	23.685056
115.345849	4318.203944	23.690074
115.649817	4297.421886	23.695091
115.461660	4299.801394	23.700109
116.008393	4296.666366	23.705127
115.843509	4328.188208	23.710144
115.767847	4321.769918	23.715162
116.240724	4311.613488	23.720179
116.106119	4332.648440	23.725197
116.490986	4332.771140	23.730215
116.504020	4320.136053	23.735232
116.385842	4345.933492	23.740250
116.614531	4313.909517	23.745267
116.495954	4316.717279	23.750285
116.531514	4323.837210	23.755303
116.835595	4344.015860	23.760320
116.658999	4345.137603	23.765338
117.411531	4347.756550	23.770355
116.788213	4357.123090	23.775373
117.124027	4374.178924	23.780391
117.266072	4380.972242	23.785408
117.355346	4389.923427	23.790426
117.732028	4371.524061	23.795443
117.768304	4384.574417	23.800461
117.923224	4410.121331	23.805479
117.979843	4429.970915	23.810496
118.435947	4429.296041	23.815514
118.481476	4400.587492	23.820531
118.288643	4410.684088	23.825549
118.531773	4413.217538	23.830567
118.838108	4431.901881	23.835584
118.598378	4427.603905	23.840602
118.983634	4421.407042	23.845619
118.979450	4427.845814	23.850637
118.769805	4429.298604	23.855655
118.892916	4440.868167	23.860672
119.275754	4444.393470	23.865690
119.091305	4447.844011	23.870707
119.215573	4464.037287	23.875725
119.546100	4468.068864	23.880743
119.562773	4491.689201	23.885760
119.347714	4505.489439	23.890778
120.006539	4501.207137	23.895795
120.124676	4497.357476	23.900813
120.638608	4512.697459	23.905831
120.535042	4516.989355	23.910848
120.581048	4503.181376	23.915866
121.094315	4512.516498	23.920883
121.124516	4542.743578	23.925901
121.063294	4517.949610	23.930919
121.056461	4528.402547	23.935936
121.294716	4534.502885	23.940954
121.595521	4521.717724	23.945971
121.764904	4545.444403	23.950989
121.824311	4536.520689	23.956007
121.836814	4514.170396	23.961024
121.798656	4526.490275	23.966042
122.168710	4545.569336	23.971059
121.915586	4557.413747	23.976077
122.318777	4552.748877	23.981095
122.507154	4562.684159	23.986112
122.447717	4557.504404	23.991130
122.342836	4547.525175	23.996147
122.327889	4572.504375	24.001165
122.450327	4578.403399	24.006183
122.476697	4593.390570	24.011200
122.465083	4606.304934	24.016218
123.164916	4608.459809	24.021235
123.202617	4615.527160	24.026253
123.266524	4632.308922	24.031271
123.242482	4635.995988	24.036288
123.381740	4646.381164	24.041306
123.655751	4642.630907	24.046323
123.968762	4653.446426	24.051341
123.993990	4649.439641	24.056359
123.962996	4646.760238	24.061376
124.158545	4682.498374	24.066394
124.614389	4675.229132	24.071411
124.734072	4688.811231	24.076429
124.634371	4686.603797	24.081447
124.542365	4672.738552	24.086464
124.736111	4678.370323	24.091482
125.225287	4682.137556	24.096499
125.236927	4687.240373	24.101517
125.252794	4680.199338	24.106535
125.765600	4692.806258	24.111552
125.736624	4690.255252	24.116570
125.843855	4686.675060	24.121587
125.880824	4696.446078	24.126605
126.004885	4682.352210	24.131623
125.938049	4701.135153	24.136640
125.892320	4701.329796	24.141658
126.219609	4698.808502	24.146675
126.397926	4732.600806	24.151693
125.829884	4733.096712	24.156711
126.101352	4717.263905	24.161728
126.158467	4750.077859	24.166746
126.718470	4759.733753	24.171763
126.555166	4759.193105	24.176781
126.645643	4773.664349	24.181799
126.972935	4784.531537	24.186816
126.943298	4767.998044	24.191834
127.447166	4794.154856	24.196851
127.076549	4825.853039	24.201869
127.639875	4815.173465	24.206887
128.068639	4809.089339	24.211904
127.705400	4828.969045	24.216922
128.057327	4848.431000	24.221939
127.934628	4859.702910	24.226957
128.053933	4851.860062	24.231975
128.223407	4854.096702	24.236992
128.200280	4880.628926	24.242010
128.867050	4863.086166	24.247027
129.050583	4878.777564	24.252045
129.162362	4901.150919	24.257063
129.166105	4900.682270	24.262080
128.682478	4902.401242	24.267098
129.310110	4918.971269	24.272115
129.664722	4928.630104	24.277133
129.966472	4927.826779	24.282151
130.382011	4946.573226	24.287168
130.084401	4944.172866	24.292186
130.179052	4923.306843	24.297203
130.698783	4915.240711	24.302221
130.719396	4924.285833	24.307239
130.595063	4920.812354	24.312256
131.107078	4921.251061	24.317274
130.938710	4915.941941	24.322291
130.917531	4923.896722	24.327309
130.891919	4949.730261	24.332327
131.454360	4940.410203	24.337344
131.236971	4945.282050	24.342362
131.374748	4950.587734	24.347379
131.491575	4945.546835	24.352397
131.970938	4954.646883	24.357415
132.153755	4937.628495	24.362432
131.808334	4963.342066	24.367450
132.154348	4976.151581	24.372467
132.110584	4982.614446	24.377485
132.621815	4972.767394	24.382503
132.865815	4955.521553	24.387520
132.287207	4971.992918	24.392538
132.376453	4963.781355	24.397555
132.580131	4993.597575	24.402573
132.795243	5017.252064	24.407591
132.972762	5001.884891	24.412608
133.009362	4996.912350	24.417626
133.143864	5022.488450	24.422643
133.302299	5035.400269	24.427661
133.021355	5027.827800	24.432679
133.446683	5049.930661	24.437696
133.540945	5071.427619	24.442714
133.616282	5056.868624	24.447731
134.148318	5057.917027	24.452749
133.831314	5076.600813	24.457767
134.566480	5075.037668	24.462784
134.246414	5093.258194	24.467802
134.724342	5080.948040	24.472819
134.556066	5088.567364	24.477837
134.634904	5120.041877	24.482855
135.015794	5117.007322	24.487872
135.215902	5139.803835	24.492890
135.184261	5114.503625	24.497907
135.175249	5147.390762	24.502925
135.766440	5145.870692	24.507943
136.090061	5131.717066	24.512960
136.145360	5143.693246	24.517978
136.073587	5157.514874	24.522995
136.261736	5154.109003	24.528013
136.396154	5173.121077	24.533031
136.562442	5163.297043	24.538048
136.516096	5173.988838	24.543066
136.529770	5184.939625	24.548083
136.739223	5177.634483	24.553101
136.870746	5204.221235	24.558119
137.145401	5208.458307	24.563136
137.132158	5204.708528	24.568154
137.237141	5208.051568	24.573171
137.620768	5218.099106	24.578189
137.414912	5234.502068	24.583207
137.729244	5241.761795	24.588224
137.663665	5241.095531	24.593242
137.676870	5243.828532	24.598259
138.237007	5261.312463	24.603277
137.636294	5277.765753	24.608295
138.292129	5290.240076	24.613312
138.636308	5288.312371	24.618330
138.641092	5280.527207	24.623347
138.966989	5293.545433	24.628365
138.950179	5315.926853	24.633383
139.442134	5323.519878	24.638400
139.470451	5311.009417	24.643418
139.509973	5304.799647	24.648435
140.016210	5319.773978	24.653453
139.800752	5313.411843	24.658471
139.967123	5337.268579	24.663488
140.322894	5357.005349	24.668506
140.313173	5348.237479	24.673523
140.464792	5342.787148	24.678541
140.344977	5349.996611	24.683559
140.790543	5338.912898	24.688576
140.333875	5346.927254	24.693594
140.428489	5380.334784	24.698611
140.422590	5365.138509	24.703629
140.949397	5380.201628	24.708647
141.297497	5411.244431	24.713664
141.077453	5416.292853	24.718682
141.271533	5422.404384	24.723699
141.649304	5426.988663	24.728717
141.099541	5433.829821	24.733735
141.546019	5462.504025	24.738752
141.842910	5470.053760	24.743770
142.251170	5473.088862	24.748787
142.549775	5479.318190	24.753805
142.552929	5474.001798	24.758823
142.747450	5473.706735	24.763840
142.685675	5493.103599	24.768858
142.885282	5511.571042	24.773875
143.312754	5495.387641	24.778893
143.307273	5496.776084	24.783911
143.561637	5512.002069	24.788928
143.891659	5511.769265	24.793946
143.921970	5515.053053	24.798963
144.080479	5524.998612	24.803981
144.201966	5539.058341	24.808999
143.986323	5515.748989	24.814016
144.073262	5503.068839	24.819034
144.128501	5521.838113	24.824051
144.550331	5544.820246	24.829069
144.314876	5548.658212	24.834087
144.459711	5563.377520	24.839104
144.680795	5579.283509	24.844122
144.808994	5577.753678	24.849139
145.048000	5585.000814	24.854157
144.991120	5592.516934	24.859175
145.066836	5605.451950	24.864192
145.446669	5633.075227	24.869210
145.682730	5653.077046	24.874227
146.017261	5632.627154	24.879245
146.010191	5643.757289	24.884263
146.514194	5648.753869	24.889280
146.848241	5664.116844	24.894298
146.639827	5657.592766	24.899315
147.130376	5677.556110	24.904333
147.331381	5660.429200	24.909351
147.146598	5651.264080	24.914368
147.545799	5659.753349	24.919386
147.696245	5672.354404	24.924403
147.662054	5657.927518	24.929421
147.455681	5680.517564	24.934439
147.613126	5686.659663	24.939456
148.021474	5676.189375	24.944474
147.882793	5700.175816	24.949491
148.213384	5707.066127	24.954509
148.113114	5713.991805	24.959527
148.396604	5728.787576	24.964544
148.676112	5729.528524	24.969562
148.437913	5734.961958	24.974579
148.613496	5741.049110	24.979597
148.667749	5777.260378	24.984615
149.013279	5773.318497	24.989632
149.252628	5773.676690	24.994650
149.194421	5791.493324	24.999667
149.801776	5809.566169	25.004685
149.455555	5832.292540	25.009703
149.743081	5818.015509	25.014720
150.040668	5837.925505	25.019738
150.055346	5861.071449	25.024755
150.412448	5838.324107	25.029773
150.566127	5853.685181	25.034791
150.860500	5883.570407	25.039808
151.074860	5876.510209	25.044826
151.122804	5879.867937	25.049843
151.617349	5887.099372	25.054861
151.719781	5885.713148	25.059879
151.528780	5868.102322	25.064896
151.880828	5857.483331	25.069914
152.050742	5887.152501	25.074931
152.042073	5901.024994	25.079949
151.977761	5904.171733	25.084967
152.089736	5883.223999	25.089984
152.403967	5897.056129	25.095002
151.945339	5935.737703	25.100019
152.640646	5942.708023	25.105037
152.588461	5934.815009	25.110055
152.568379	5933.450992	25.115072
153.077141	5954.547587	25.120090
152.912900	5959.852335	25.125107
153.227022	5950.892419	25.130125
153.230096	5972.803746	25.135143
153.156687	5983.992333	25.140160
153.450899	6006.793465	25.145178
153.702577	6017.503528	25.150195
153.810763	6018.561008	25.155213
153.922403	6047.872368	25.160231
154.174716	6042.950866	25.165248
154.754669	6033.367015	25.170266
154.695693	6058.403906	25.175283
155.063424	6067.404149	25.180301
155.243701	6068.303253	25.185319
155.657193	6091.207250	25.190336
155.823626	6077.045669	25.195354
155.711325	6075.085807	25.200371
155.797822	6082.538311	25.205389
156.034645	6101.727526	25.210407
156.386996	6114.582214	25.215424
156.345940	6112.786967	25.220442
156.164227	6118.408460	25.225459
156.466399	6111.297423	25.230477
157.034044	6120.693045	25.235495
156.806361	6144.937807	25.240512
156.998072	6132.661917	25.245530
156.805927	6142.925672	25.250547
157.250947	6147.406922	25.255565
157.358030	6174.058820	25.260583
157.209009	6170.646624	25.265600
157.497244	6195.499977	25.270618
157.375153	6203.587842	25.275635
157.797402	6210.680180	25.280653
157.840315	6238.883867	25.285671
158.004099	6264.458741	25.290688
158.469774	6266.350950	25.295706
158.425227	6256.131108	25.300723
158.709992	6260.412078	25.305741
158.780142	6293.910258	25.310759
159.227678	6309.576014	25.315776
159.511004	6296.266655	25.320794
159.523822	6302.778202	25.325811
159.768077	6318.051531	25.330829
159.833978	6330.881281	25.335847
159.974727	6350.218971	25.340864
160.347941	6345.827844	25.345882
160.373397	6341.163439	25.350899
160.627180	6357.948368	25.355917
160.697743	6369.774922	25.360935
160.684380	6383.105259	25.365952
161.138594	6369.206918	25.370970
161.350519	6378.932758	25.375987
161.200779	6385.534591	25.381005
161.297269	6392.202445	25.386023
161.517203	6407.973236	25.391040
161.779659	6416.404798	25.396058
162.011410	6426.390016	25.401075
162.341458	6441.483133	25.406093
162.303817	6448.862613	25.411111
162.378653	6441.138926	25.416128
162.450625	6444.451856	25.421146
162.658799	6475.810874	25.426163
163.098106	6469.516867	25.431181
163.242023	6476.085572	25.436199
163.238813	6471.163634	25.441216
163.547873	6469.263247	25.446234
163.380323	6484.350426	25.451251
163.312006	6483.034099	25.456269
163.727142	6493.591484	25.461287
163.724229	6502.250817	25.466304
164.201529	6513.344457	25.471322
164.234946	6543.820973	25.476339
164.430992	6536.789098	25.481357
165.063399	6548.885198	25.486375
164.860520	6557.857553	25.491392
164.979000	6545.881659	25.496410
164.840723	6555.841477	25.501427
165.132113	6579.123490	25.506445
165.410102	6590.499751	25.511463
165.617909	6602.009677	25.516480
165.655440	6608.074306	25.521498
165.876044	6613.748805	25.526515
165.895134	6631.967055	25.531533
166.098279	6636.667172	25.536551
166.255139	6640.214572	25.541568
166.510594	6670.586529	25.546586
166.847223	6670.778261	25.551603
167.074898	6676.107087	25.556621
167.341641	6692.568543	25.561639
167.321469	6692.933022	25.566656
167.520336	6672.861711	25.571674
167.628628	6716.031591	25.576691
167.853243	6727.753425	25.581709
168.134064	6712.041088	25.586727
168.116296	6729.016576	25.591744
168.396365	6737.089060	25.596762
168.598871	6735.585821	25.601779
168.510329	6740.988573	25.606797
168.846526	6759.862535	25.611815
168.775413	6775.377026	25.616832
168.864813	6755.956450	25.621850
169.081039	6788.682644	25.626867
169.191507	6797.302144	25.631885
169.601388	6807.233368	25.636903
169.834764	6826.415380	25.641920
169.930231	6838.468517	25.646938
170.063013	6837.359120	25.651955
170.066921	6860.562659	25.656973
170.422471	6873.241438	25.661991
170.440176	6884.948359	25.667008
170.831996	6888.599924	25.672026
171.000210	6890.420480	25.677044
171.187901	6905.467873	25.682061
171.306222	6911.281444	25.687079
171.454862	6911.024258	25.692096
172.038806	6934.554563	25.697114
172.015493	6945.578846	25.702132
172.143828	6939.090727	25.707149
172.795314	6935.240544	25.712167
172.678417	6957.609351	25.717184
172.781482	6962.458404	25.722202
172.918468	6954.345011	25.727220
172.958398	6975.915781	25.732237
173.429362	6982.137316	25.737255
173.288761	6990.983076	25.742272
173.716242	7004.245433	25.747290
173.907383	7020.131063	25.752308
173.774562	7023.407472	25.757325
174.259880	7001.506278	25.762343
173.906471	7008.257393	25.767360
174.081066	7037.730701	25.772378
174.407691	7049.914334	25.777396
174.402386	7037.160771	25.782413
174.999489	7041.886481	25.787431
175.022021	7070.999490	25.792448
175.087769	7067.485855	25.797466
175.558644	7056.627889	25.802484
175.414518	7085.803112	25.807501
175.741821	7081.175634	25.812519
175.534251	7099.629544	25.817536
176.044808	7097.703666	25.822554
176.314934	7098.694300	25.827572
176.445017	7120.500803	25.832589
176.909959	7133.949628	25.837607
176.619870	7146.817997	25.842624
176.910230	7140.596373	25.847642
177.241625	7154.970562	25.852660
177.020278	7161.921215	25.857677
177.241296	7154.712078	25.862695
176.930757	7191.547208	25.867712
177.085538	7204.799273	25.872730
177.565526	7207.733881	25.877748
177.491111	7249.297377	25.882765
178.185438	7243.402334	25.887783
178.276941	7255.409589	25.892800
178.574028	7276.956003	25.897818
179.094742	7295.539060	25.902836
179.115616	7285.540451	25.907853
179.602414	7274.338708	25.912871
179.176185	7301.618913	25.917888
179.441400	7315.161534	25.922906
179.576806	7311.842666	25.927924
179.722739	7336.750089	25.932941
179.870624	7355.352293	25.937959
180.328045	7360.115356	25.942976
180.717151	7355.955221	25.947994
180.698501	7361.188346	25.953012
181.017099	7367.213128	25.958029
181.264456	7390.116948	25.963047
181.389226	7393.984439	25.968064
181.642930	7381.914688	25.973082
181.928280	7405.943931	25.978100
181.780896	7418.678294	25.983117
182.088028	7415.605878	25.988135
182.373236	7414.014490	25.993152
182.534508	7434.025040	25.998170
182.812941	7446.210251	26.003188
182.951861	7450.488872	26.008205
183.015363	7458.197840	26.013223
183.112987	7464.603323	26.018240
183.163375	7485.801744	26.023258
183.311608	7486.497138	26.028276
183.574973	7487.224698	26.033293
183.706523	7500.120161	26.038311
183.725258	7527.971440	26.043328
183.718604	7516.303721	26.048346
183.839654	7543.673478	26.053364
183.793946	7575.069949	26.058381
184.190714	7590.412645	26.063399
184.696163	7603.285004	26.068416
184.728550	7631.184613	26.073434
185.229797	7615.977176	26.078452
185.145152	7644.011125	26.083469
185.438453	7654.088945	26.088487
185.781433	7670.871569	26.093504
186.035388	7679.802946	26.098522
186.251792	7690.128969	26.103540
186.678666	7691.602891	26.108557
186.988140	7679.732397	26.113575
187.151268	7704.913990	26.118592
187.126525	7717.303863	26.123610
187.551886	7703.689482	26.128628
187.548512	7720.225394	26.133645
187.551161	7706.105159	26.138663
187.604126	7718.297908	26.143680
188.200848	7731.327764	26.148698
188.583574	7736.064696	26.153716
188.141192	7734.198146	26.158733
188.658369	7735.856400	26.163751
188.872160	7749.190530	26.168768
188.577150	7742.210508	26.173786
188.881823	7761.224376	26.178804
188.850948	7789.125267	26.183821
189.233617	7794.110303	26.188839
189.268296	7808.173420	26.193856
189.263125	7809.728977	26.198874
190.024917	7834.225138	26.203892
189.886002	7847.993290	26.208909
190.419237	7837.930151	26.213927
190.330367	7850.352775	26.218944
190.578855	7867.737161	26.223962
190.933673	7872.980416	26.228980
191.164812	7893.366696	26.233997
191.071279	7904.241016	26.239015
191.340984	7907.503473	26.244032
191.343706	7924.052768	26.249050
191.621090	7924.930819	26.254068
191.956173	7947.320072	26.259085
192.110462	7942.997756	26.264103
192.050559	7982.664358	26.269120
192.513686	7979.152593	26.274138
192.943206	7974.250042	26.279156
192.891794	8019.869268	26.284173
192.984259	8022.297868	26.289191
193.272185	8030.175589	26.294208
193.352367	8061.421494	26.299226
193.707796	8041.824248	26.304244
193.734217	8056.918293	26.309261
194.079298	8086.813916	26.314279
194.352735	8091.765117	26.319296
194.425919	8105.704003	26.324314
194.915894	8123.408689	26.329332
194.917132	8124.184316	26.334349
194.900270	8128.620384	26.339367
195.150011	8152.251843	26.344384
195.287980	8154.000364	26.349402
195.321623	8164.850701	26.354420
195.420457	8206.277051	26.359437
195.940803	8208.911420	26.364455
196.289091	8214.496887	26.369472
196.416849	8244.318457	26.374490
196.929515	8235.467386	26.379508
196.855782	8238.188891	26.384525
196.854241	8250.193377	26.389543
196.977118	8271.461999	26.394560
197.447152	8283.184614	26.399578
197.754162	8306.179934	26.404596
197.721382	8314.477797	26.409613
198.068353	8321.744203	26.414631
198.563245	8328.346661	26.419648
198.387596	8339.705031	26.424666
198.917163	8364.746802	26.429684
198.805523	8363.973026	26.434701
198.609081	8358.346827	26.439719
199.014243	8387.822767	26.444736
199.196710	8410.677364	26.449754
199.648385	8413.382971	26.454772
199.780833	8428.606343	26.459789
199.552348	8440.744556	26.464807
200.031360	8445.735936	26.469824
200.064842	8453.960704	26.474842
200.260987	8471.245719	26.479860
200.575085	8507.114769	26.484877
200.686845	8495.148743	26.489895
201.131052	8517.469585	26.494912
201.146486	8533.900857	26.499930
201.579272	8537.640555	26.504948
202.122868	8562.658271	26.509965
202.225310	8556.676247	26.514983
202.440668	8567.663018	26.520000
202.231522	8601.695448	26.525018
202.623490	8599.974468	26.530036
202.608942	8602.020744	26.535053
202.720323	8624.125009	26.540071
202.944301	8632.101809	26.545088
203.132603	8660.796573	26.550106
203.626458	8668.037296	26.555124
203.652525	8673.461152	26.560141
203.865683	8686.827686	26.565159
204.090622	8697.178164	26.570176
204.257984	8715.332980	26.575194
204.464492	8744.997567	26.580212
204.739813	8747.120409	26.585229
205.067239	8749.731615	26.590247
205.412565	8757.122935	26.595264
205.160315	8779.258357	26.600282
205.985614	8776.073290	26.605300
205.822492	8810.229306	26.610317
205.728704	8817.011933	26.615335
206.135951	8827.246527	26.620352
206.267991	8846.765939	26.625370
206.932902	8844.311474	26.630388
207.416964	8858.910094	26.635405
207.683622	8887.086683	26.640423
207.660983	8888.152192	26.645440
207.507855	8890.095386	26.650458
208.047463	8889.603058	26.655476
208.265490	8917.453004	26.660493
208.212154	8918.611012	26.665511
208.538604	8923.348152	26.670528
208.303332	8939.212450	26.675546
208.520910	8951.634139	26.680564
208.843994	8976.147860	26.685581
209.010301	8984.106013	26.690599
209.473002	9024.061421	26.695616
209.511476	9037.166485	26.700634
209.711748	9050.449606	26.705652
209.859407	9041.044848	26.710669
209.959368	9054.301228	26.715687
210.442554	9067.051663	26.720704
210.538883	9102.401204	26.725722
210.893128	9114.320784	26.730740
210.736222	9110.978164	26.735757
211.105889	9117.716639	26.740775
211.523274	9146.106645	26.745792
211.456201	9178.605407	26.750810
211.910453	9178.893526	26.755828
212.561668	9183.029694	26.760845
212.290141	9208.516274	26.765863
212.723104	9207.088540	26.770880
212.802127	9221.606346	26.775898
213.245777	9227.914418	26.780916
213.513242	9219.631021	26.785933
213.412027	9226.175614	26.790951
214.092329	9259.784472	26.795968
213.770347	9270.154804	26.800986
214.353825	9253.788588	26.806004
214.097424	9250.929436	26.811021
214.535875	9280.114851	26.816039
214.530546	9310.779549	26.821056
214.671535	9326.163050	26.826074
214.849268	9338.352977	26.831092
214.958576	9325.648725	26.836109
214.953714	9364.220413	26.841127
215.378923	9373.115794	26.846144
215.465842	9408.691259	26.851162
215.611398	9428.161898	26.856180
216.177368	9436.259817	26.861197
216.080103	9443.835642	26.866215
216.540862	9462.199607	26.871232
216.764595	9502.319365	26.876250
216.909165	9512.120499	26.881268
217.000765	9515.720685	26.886285
217.271008	9551.092901	26.891303
217.999909	9539.166685	26.896320
218.003564	9558.453781	26.901338
218.191043	9588.264867	26.906356
218.770382	9603.398207	26.911373
218.721311	9595.058220	26.916391
219.140560	9628.472339	26.921408
219.239183	9628.931859	26.926426
219.290674	9639.706221	26.931444
219.813342	9648.189472	26.936461
219.603006	9666.606269	26.941479
220.245691	9686.585032	26.946496
220.026417	9688.075329	26.951514
220.618318	9719.917337	26.956532
220.762543	9738.700964	26.961549
221.150590	9759.418957	26.966567
221.245529	9745.680201	26.971584
221.450879	9760.544672	26.976602
221.562878	9785.563960	26.981620
221.908030	9784.976140	26.986637
222.150012	9816.761160	26.991655
222.425452	9838.370576	26.996672
222.523031	9843.125331	27.001690
222.713300	9840.004024	27.006708
223.239354	9852.466034	27.011725
223.068581	9892.289639	27.016743
223.759208	9894.206182	27.021760
223.586668	9894.750682	27.026778
223.811228	9926.456097	27.031796
224.165428	9918.388002	27.036813
224.290743	9952.427143	27.041831
224.666966	9954.862720	27.046848
224.924991	9963.941225	27.051866
224.769687	10004.251689	27.056884
225.277789	9999.736457	27.061901
225.636162	10010.077566	27.066919
225.945817	10004.102507	27.071936
226.119098	10045.231511	27.076954
226.302530	10066.992706	27.081972
226.672388	10048.927328	27.086989
226.625860	10059.542522	27.092007
227.062508	10067.743264	27.097024
227.180481	10099.670639	27.102042
227.296241	10119.317184	27.107060
227.663016	10101.140408	27.112077
227.938164	10127.195049	27.117095
228.332861	10143.288858	27.122112
228.433722	10152.329637	27.127130
228.652428	10158.136486	27.132148
228.840576	10183.125704	27.137165
228.966420	10184.306185	27.142183
229.128460	10172.598395	27.147200
228.897660	10199.989925	27.152218
229.109409	10231.175841	27.157236
229.520861	10238.158372	27.162253
229.487893	10242.106187	27.167271
229.900200	10255.612067	27.172288
230.096639	10275.859072	27.177306
230.336166	10315.370193	27.182324
230.448243	10314.119047	27.187341
230.724563	10345.105476	27.192359
230.969097	10344.170356	27.197376
231.217919	10366.730100	27.202394
231.426030	10375.834417	27.207412
231.922420	10385.744165	27.212429
231.916403	10426.707648	27.217447
232.475969	10443.796142	27.222464
232.694053	10446.408371	27.227482
232.905844	10454.407010	27.232500
233.472235	10473.124907	27.237517
233.412464	10497.741259	27.242535
233.773383	10493.243906	27.247552
234.198875	10527.310301	27.252570
234.392186	10539.381212	27.257588
234.701586	10526.798117	27.262605
234.857624	10549.399444	27.267623
234.768429	10571.215824	27.272640
235.139125	10599.290835	27.277658
234.957759	10610.637592	27.282676
235.587561	10605.717693	27.287693
235.269932	10634.795789	27.292711
235.723590	10656.503692	27.297728
236.309878	10683.856366	27.302746
236.479541	10692.995574	27.307764
236.797135	10698.794161	27.312781
236.935649	10722.903122	27.317799
237.249104	10748.694090	27.322816
237.749761	10747.379498	27.327834
237.748460	10764.446788	27.332852
238.100262	10780.797242	27.337869
238.088152	10793.501723	27.342887
238.607981	10777.023161	27.347904
239.155713	10795.646060	27.352922
238.940501	10822.850975	27.357940
239.370323	10836.818413	27.362957
239.455592	10858.166825	27.367975
240.359785	10835.099391	27.372992
240.426692	10852.042864	27.378010
240.651510	10881.001855	27.383028
240.782883	10888.654020	27.388045
240.881462	10893.186792	27.393063
240.982071	10899.112676	27.398080
241.169384	10921.242256	27.403098
241.351488	10934.990765	27.408116
241.535659	10937.471619	27.413133
241.618530	10960.062773	27.418151
241.569198	11002.043154	27.423168
242.025996	11018.222903	27.428186
242.295341	11021.041015	27.433204
242.590100	11023.483130	27.438221
242.634125	11072.067387	27.443239
242.704847	11082.754476	27.448256
243.494578	11099.763115	27.453274
243.642101	11118.209110	27.458292
243.732162	11131.184495	27.463309
244.164219	11157.737942	27.468327
244.479355	11161.061316	27.473344
245.057127	11175.359867	27.478362
244.899825	11182.617959	27.483380
245.126993	11197.495924	27.488397
245.545962	11231.761046	27.493415
245.584392	11221.018174	27.498432
245.908744	11232.557520	27.503450
246.007314	11244.927411	27.508468
246.495327	11279.882300	27.513485
247.041921	11292.133306	27.518503
246.891975	11291.274337	27.523520
246.907921	11309.332676	27.528538
247.286364	11320.927743	27.533556
247.502222	11329.015164	27.538573
247.846218	11350.523934	27.543591
247.913107	11357.289760	27.548608
248.331955	11378.506559	27.553626
248.055742	11409.572955	27.558644
248.394438	11411.194150	27.563661
249.148354	11427.147988	27.568679
249.209726	11441.475380	27.573696
249.513786	11484.888239	27.578714
249.718758	11498.625579	27.583732
249.778580	11510.835078	27.588749
250.038116	11534.118632	27.593767
249.950940	11551.427818	27.598784
250.790838	11577.042560	27.603802
250.822119	11603.458153	27.608820
251.267512	11614.302688	27.613837
251.734470	11615.289853	27.618855
251.801091	11645.120821	27.623872
252.387075	11660.578793	27.628890
252.532927	11684.919590	27.633908
253.267576	11684.304382	27.638925
253.226599	11714.261176	27.643943
253.394320	11710.413783	27.648960
253.921286	11703.137866	27.653978
253.668707	11725.026140	27.658996
254.086385	11745.965548	27.664013
254.340907	11751.647327	27.669031
254.418908	11779.074833	27.674048
254.552425	11791.474034	27.679066
254.676276	11828.252478	27.684084
254.994471	11826.332237	27.689101
255.148683	11858.433601	27.694119
255.406116	11875.983184	27.699136
256.146560	11885.274554	27.704154
256.177288	11913.328484	27.709172
256.380808	11911.886438	27.714189
256.859582	11920.362410	27.719207
257.271727	11940.920928	27.724224
257.732548	11947.881879	27.729242
258.011085	11971.116454	27.734260
258.247005	11972.284398	27.739277
258.404050	11980.473246	27.744295
258.531660	11996.242026	27.749312
258.677577	12005.177155	27.754330
258.682643	12022.172262	27.759348
259.272716	12050.779982	27.764365
259.562574	12060.854094	27.769383
259.301963	12063.307776	27.774400
260.082628	12082.209590	27.779418
259.908872	12104.962925	27.784436
259.893794	12138.119272	27.789453
260.729450	12141.519136	27.794471
260.797750	12183.970020	27.799488
260.970781	12199.852024	27.804506
261.173894	12218.342885	27.809524
261.371328	12222.781715	27.814541
261.828942	12244.513187	27.819559
261.566949	12279.371237	27.824576
262.450341	12297.576489	27.829594
262.286617	12311.667704	27.834612
262.657607	12324.715810	27.839629
263.108877	12346.491008	27.844647
262.911113	12374.341648	27.849664
263.445998	12380.163247	27.854682
263.743727	12413.906582	27.859700
263.595360	12429.459841	27.864717
264.063394	12436.849155	27.869735
264.496325	12457.375755	27.874752
264.716043	12484.700700	27.879770
265.107259	12508.279817	27.884788
265.207204	12529.754868	27.889805
265.537008	12546.657490	27.894823
265.925328	12570.319106	27.899840
266.123553	12593.193653	27.904858
266.368052	12626.856423	27.909876
266.436743	12631.063757	27.914893
267.238753	12651.344498	27.919911
267.315310	12674.269987	27.924928
267.762298	12687.394065	27.929946
267.825258	12712.252728	27.934964
268.311063	12723.211874	27.939981
268.538901	12733.296656	27.944999
268.566892	12776.991813	27.950016
269.261579	12791.237051	27.955034
269.549482	12803.184544	27.960052
269.679329	12800.420066	27.965069
270.129127	12822.859480	27.970087
270.028967	12849.617111	27.975104
270.403895	12849.066026	27.980122
270.970872	12885.766594	27.985140
271.015223	12894.622888	27.990157
271.383724	12894.239089	27.995175
271.229542	12931.359057	28.000192
271.883018	12961.149087	28.005210
271.621795	12970.565617	28.010228
271.938105	12982.881181	28.015245
272.638577	12996.999598	28.020263
272.835619	13031.095683	28.025280
273.048422	13039.556320	28.030298
273.157739	13062.795224	28.035316
273.558117	13106.035060	28.040333
273.702130	13101.598820	28.045351
273.677576	13131.401133	28.050368
274.444576	13162.656232	28.055386
274.951734	13177.036000	28.060404
274.885259	13205.090124	28.065421
275.477076	13212.635031	28.070439
275.326642	13241.837546	28.075456
275.873173	13253.374735	28.080474
275.945999	13283.396010	28.085492
276.339814	13322.707870	28.090509
276.611270	13326.402103	28.095527
276.725069	13351.313228	28.100544
277.194574	13378.232088	28.105562
277.615280	13391.963772	28.110580
277.744232	13425.352656	28.115597
278.386275	13425.431803	28.120615
278.672818	13437.708516	28.125632
278.894492	13448.697617	28.130650
279.244453	13486.645514	28.135668
279.083413	13491.380270	28.140685
279.617904	13497.241737	28.145703
279.691654	13507.995333	28.150720
279.418009	13547.702420	28.155738
280.322971	13559.383874	28.160756
280.277752	13582.517491	28.165773
280.664406	13592.801108	28.170791
281.017857	13617.168049	28.175808
281.803921	13642.571253	28.180826
281.820176	13638.946174	28.185844
281.660380	13650.728760	28.190861
282.197327	13693.574964	28.195879
282.311349	13705.866204	28.200896
282.419733	13718.083540	28.205914
282.835617	13753.025804	28.210932
282.796637	13778.355175	28.215949
283.406761	13786.611904	28.220967
283.462074	13814.929016	28.225984
283.761744	13851.534926	28.231002
284.061905	13867.768651	28.236020
284.343745	13882.081493	28.241037
284.830278	13907.012257	28.246055
285.176980	13947.685375	28.251072
285.430141	13957.419300	28.256090
286.053574	13971.377979	28.261108
286.252028	14007.350197	28.266125
287.123223	14005.301315	28.271143
287.160183	14021.532983	28.276160
287.264490	14037.698391	28.281178
287.440196	14059.307143	28.286196
287.826599	14060.901038	28.291213
287.829056	14075.310631	28.296231
288.615977	14108.560712	28.301248
288.828277	14133.455196	28.306266
289.300432	14125.454544	28.311284
289.155521	14154.410407	28.316301
289.517797	14167.350364	28.321319
289.987628	14192.716079	28.326336
290.047614	14198.957162	28.331354
290.228481	14220.092558	28.336372
290.561360	14252.841231	28.341389
291.045472	14260.244492	28.346407
291.188140	14291.861778	28.351424
291.153308	14322.714276	28.356442
291.541403	14338.833101	28.361460
291.748630	14361.045285	28.366477
292.184454	14370.122136	28.371495
292.530033	14404.222583	28.376512
292.488397	14434.531210	28.381530
293.385345	14448.092148	28.386548
293.471497	14473.099389	28.391565
294.044190	14482.911630	28.396583
294.108572	14499.091975	28.401600
294.350458	14544.443428	28.406618
294.985997	14559.741591	28.411636
294.910545	14567.395016	28.416653
295.647781	14582.618097	28.421671
295.724600	14605.808652	28.426688
295.718324	14599.457850	28.431706
296.254531	14635.998096	28.436724
296.253160	14663.709932	28.441741
296.849837	14677.735100	28.446759
296.817265	14707.076789	28.451776
297.465531	14740.132047	28.456794
298.167332	14737.085231	28.461812
298.226291	14750.312134	28.466829
298.123213	14769.977681	28.471847
298.836531	14807.417191	28.476864
298.966594	14819.680627	28.481882
299.039235	14833.724748	28.486900
299.280005	14864.181344	28.491917
299.844551	14868.971540	28.496935
300.001130	14879.684789	28.501952
300.031707	14922.670700	28.506970
300.555606	14930.639713	28.511988
300.633258	14955.445825	28.517005
301.037849	14971.981720	28.522023
301.299148	14986.658219	28.527040
301.350572	15000.931329	28.532058
302.034638	15038.664580	28.537076
301.944282	15073.205620	28.542093
302.221396	15073.818609	28.547111
302.697049	15115.317996	28.552128
302.763576	15132.882186	28.557146
303.476283	15131.856850	28.562164
303.634958	15177.543713	28.567181
303.707056	15216.194755	28.572199
304.169649	15238.865492	28.577216
304.523225	15251.791998	28.582234
305.123810	15258.346015	28.587252
305.121496	15314.460349	28.592269
305.314489	15351.884650	28.597287
305.699022	15365.791033	28.602304
306.108459	15376.281614	28.607322
306.333600	15406.494403	28.612340
306.682487	15438.503758	28.617357
306.860110	15461.710399	28.622375
307.368892	15502.034445	28.627392
307.890415	15514.118697	28.632410
307.987744	15534.016803	28.637428
307.879450	15570.832674	28.642445
308.692084	15592.089260	28.647463
308.903441	15611.590414	28.652480
309.016466	15642.819688	28.657498
309.995504	15644.024303	28.662516
310.329904	15673.256682	28.667533
310.727507	15703.610150	28.672551
311.006283	15720.243238	28.677568
311.424454	15719.594311	28.682586
311.680035	15749.665608	28.687604
311.651404	15772.716087	28.692621
311.666113	15799.688115	28.697639
312.136510	15812.485457	28.702656
312.493580	15841.213262	28.707674
312.829958	15873.680972	28.712692
313.009490	15897.519853	28.717709
313.080651	15923.233076	28.722727
313.809658	15950.092075	28.727744
313.853385	15976.511189	28.732762
314.306782	15987.623689	28.737780
314.572121	16029.571467	28.742797
315.061142	16069.868668	28.747815
315.517458	16088.691683	28.752832
315.627983	16097.381993	28.757850
316.300304	16105.758869	28.762868
316.300541	16143.806228	28.767885
316.685510	16184.705568	28.772903
316.702220	16196.358403	28.777920
316.911581	16218.103151	28.782938
317.467744	16235.688500	28.787956
317.754050	16270.458246	28.792973
317.880863	16301.238940	28.797991
318.440139	16305.174708	28.803008
318.946946	16347.270948	28.808026
319.379227	16366.136078	28.813044
319.523749	16377.269930	28.818061
319.963664	16413.461317	28.823079
320.354910	16449.014686	28.828096
320.330840	16474.410410	28.833114
321.332268	16460.149770	28.838132
321.407863	16497.507846	28.843149
321.493397	16508.473450	28.848167
321.765436	16516.826839	28.853184
321.844421	16548.090262	28.858202
322.111024	16559.892763	28.863220
322.532383	16593.723680	28.868237
322.464904	16630.141208	28.873255
323.262714	16649.705894	28.878272
323.125158	16672.107427	28.883290
323.902434	16689.749722	28.888308
323.846840	16725.238827	28.893325
324.254518	16774.537409	28.898343
324.532929	16792.716111	28.903360
324.718581	16792.458580	28.908378
325.000939	16826.525700	28.913396
325.387250	16855.688586	28.918413
325.765876	16906.234242	28.923431
326.198354	16924.669741	28.928448
326.485528	16954.317250	28.933466
327.295695	16963.811244	28.938484
327.504446	17005.496656	28.943501
327.326404	17024.269528	28.948519
328.210991	17057.170685	28.953536
328.397589	17112.629590	28.958554
328.932540	17128.575630	28.963572
329.130675	17144.687651	28.968589
329.362214	17151.531932	28.973607
329.975423	17186.506513	28.978624
329.948080	17233.941422	28.983642
330.712952	17236.585790	28.988660
331.122705	17268.241959	28.993677
331.060970	17284.460089	28.998695
331.742320	17313.575051	29.003712
331.734993	17344.089879	29.008730
332.261047	17344.321412	29.013748
332.596288	17378.098835	29.018765
332.912520	17397.260136	29.023783
333.391984	17423.551291	29.028800
333.256958	17454.238719	29.033818
333.505558	17464.932163	29.038836
334.061732	17513.877472	29.043853
334.411141	17538.166649	29.048871
334.737111	17550.560535	29.053888
334.844276	17590.700774	29.058906
335.103261	17633.872011	29.063924
335.432831	17653.105483	29.068941
335.791200	17686.012886	29.073959
336.540176	17720.764444	29.078976
336.403136	17763.440365	29.083994
337.118833	17780.775650	29.089012
337.204556	17804.399550	29.094029
337.353776	17860.001123	29.099047
338.165015	17880.882676	29.104064
338.181991	17907.462206	29.109082
338.656363	17941.332859	29.114100
338.901337	17981.478080	29.119117
339.015842	17994.060117	29.124135
339.955406	18017.831693	29.129152
340.232003	18053.487871	29.134170
340.474185	18087.970885	29.139188
340.868646	18109.791592	29.144205
341.149964	18142.767803	29.149223
341.574753	18180.259583	29.154240
341.841496	18202.914787	29.159258
342.314164	18232.040641	29.164276
342.718115	18257.849132	29.169293
342.876095	18273.048441	29.174311
343.348788	18293.360729	29.179328
343.495035	18336.076446	29.184346
343.965047	18345.447768	29.189364
344.553299	18381.286437	29.194381
344.627630	18412.279935	29.199399
345.323211	18438.439294	29.204416
345.517659	18445.800914	29.209434
345.973480	18442.199872	29.214452
346.506500	18468.983492	29.219469
346.589461	18508.453806	29.224487
346.707299	18539.780803	29.229504
347.084918	18548.351060	29.234522
347.158767	18562.196439	29.239540
347.673009	18598.120311	29.244557
347.442269	18645.939647	29.249575
347.975709	18651.659744	29.254592
348.462070	18680.341229	29.259610
348.508765	18731.978152	29.264628
349.264126	18765.288678	29.269645
349.542988	18789.077530	29.274663
350.068140	18830.674324	29.279680
350.201418	18859.844747	29.284698
350.388149	18880.025318	29.289716
350.734839	18922.220825	29.294733
350.794246	18966.412068	29.299751
351.206110	18991.120223	29.304768
351.636414	19029.717936	29.309786
352.132866	19074.737276	29.314804
352.588306	19099.679553	29.319821
353.034793	19130.846198	29.324839
353.679345	19172.113617	29.329856
353.771574	19193.878510	29.334874
354.402389	19218.446806	29.339892
354.852061	19266.986199	29.344909
355.231736	19295.618603	29.349927
355.872411	19300.307704	29.354944
356.085562	19337.465093	29.359962
356.506199	19355.446603	29.364980
357.183976	19358.688922	29.369997
357.503780	19387.520524	29.375015
358.246376	19419.802056	29.380032
358.404768	19424.662287	29.385050
358.662019	19432.206274	29.390068
359.078788	19463.403677	29.395085
359.522332	19500.014248	29.400103
359.544082	19504.518779	29.405120
359.941685	19546.557729	29.410138
360.123514	19573.705378	29.415156
360.499938	19579.024578	29.420173
360.583194	19598.105562	29.425191
360.950753	19644.478102	29.430208
361.113355	19691.020189	29.435226
361.476146	19701.193400	29.440244
361.970213	19739.017754	29.445261
362.206008	19768.062506	29.450279
362.590124	19773.069974	29.455296
362.604803	19823.254397	29.460314
362.796224	19878.182733	29.465332
363.257126	19898.568308	29.470349
363.523184	19923.595134	29.475367
363.795752	19975.480779	29.480384
364.384811	20023.780264	29.485402
364.612630	20057.093855	29.490420
365.264450	20083.110158	29.495437
365.479529	20131.577350	29.500455
366.315240	20167.486211	29.505472
366.499676	20199.796846	29.510490
366.803033	20230.426469	29.515508
367.403715	20261.610759	29.520525
367.662175	20293.051834	29.525543
367.859478	20318.801533	29.530560
368.472737	20329.181237	29.535578
368.828363	20373.067206	29.540596
369.474651	20388.651235	29.545613
369.699259	20414.707108	29.550631
370.047658	20450.865754	29.555648
370.094735	20474.318580	29.560666
370.776571	20496.883140	29.565684
371.155358	20531.550460	29.570701
371.088480	20581.408582	29.575719
371.592158	20592.422904	29.580736
371.807792	20595.834823	29.585754
372.042575	20651.984952	29.590772
372.659137	20693.148870	29.595789
372.758269	20730.816887	29.600807
373.302826	20760.055130	29.605824
373.469949	20792.744952	29.610842
374.030750	20844.796931	29.615860
374.812414	20855.045107	29.620877
374.792894	20911.225509	29.625895
375.402339	20944.827792	29.630912
375.757754	20983.149226	29.635930
375.893688	21001.945679	29.640948
376.670638	21032.761803	29.645965
376.964207	21082.085811	29.650983
377.331335	21116.239221	29.656000
377.772961	21132.841430	29.661018
378.068064	21159.087027	29.666036
378.701319	21209.643215	29.671053
378.762255	21241.960512	29.676071
379.075917	21267.552160	29.681088
379.605749	21306.040998	29.686106
380.026282	21347.587307	29.691124
380.622116	21365.277223	29.696141
380.936014	21404.408880	29.701159
381.445311	21431.707253	29.706176
381.654758	21462.078786	29.711194
382.007190	21496.159734	29.716212
382.585097	21518.189528	29.721229
383.017665	21556.043947	29.726247
382.906456	21606.639194	29.731264
383.562210	21622.657919	29.736282
383.900365	21658.418890	29.741300
384.249183	21687.765193	29.746317
384.532256	21719.641574	29.751335
384.756477	21766.595472	29.756352
385.435165	21789.394051	29.761370
385.149120	21838.065651	29.766388
385.804878	21871.977449	29.771405
386.388644	21928.901871	29.776423
386.524527	21960.085732	29.781440
387.413636	21970.506030	29.786458
387.695118	22016.139546	29.791476
388.562196	22050.688378	29.796493
388.972950	22080.740862	29.801511
389.214302	22117.080035	29.806528
389.449390	22136.562924	29.811546
390.083329	22164.277017	29.816564
390.826683	22175.839255	29.821581
391.401665	22225.503243	29.826599
391.549743	22257.220077	29.831616
391.873529	22259.845143	29.836634
391.866304	22301.551197	29.841652
392.609558	22323.658793	29.846669
392.840510	22334.244798	29.851687
393.044624	22385.815041	29.856704
393.537074	22386.479462	29.861722
393.649878	22432.041080	29.866740
394.068543	22456.676025	29.871757
394.489623	22498.890400	29.876775
394.717337	22504.326551	29.881792
395.118595	22543.842154	29.886810
395.469595	22602.497358	29.891828
395.977840	22628.744741	29.896845
396.402816	22649.413943	29.901863
396.289013	22676.464141	29.906880
397.040956	22705.558030	29.911898
396.867321	22742.298186	29.916916
397.115174	22782.219640	29.921933
397.380901	22833.706984	29.926951
397.825087	22890.750753	29.931968
398.404638	22925.867583	29.936986
398.548996	22964.507479	29.942004
398.806634	23006.535718	29.947021
399.176535	23072.657658	29.952039
399.777057	23117.847326	29.957056
400.211120	23160.217303	29.962074
400.516792	23209.638604	29.967092
400.933808	23267.780719	29.972109
401.598948	23328.458211	29.977127
402.120901	23367.662569	29.982144
402.687275	23388.911589	29.987162
403.100427	23449.084061	29.992180
403.752910	23487.272293	29.997197
404.481608	23517.465605	30.002215
404.931365	23571.210903	30.007232
405.344455	23615.676095	30.012250
405.462193	23637.647535	30.017268
405.986469	23667.442888	30.022285
406.483059	23706.611234	30.027303
406.716805	23736.311228	30.032320
407.473743	23785.541429	30.037338
407.773808	23834.697464	30.042356
408.067977	23857.333770	30.047373
408.304371	23882.227957	30.052391
408.707886	23929.237122	30.057408
409.501542	23958.622708	30.062426
409.616489	24011.338401	30.067444
409.915189	24023.762133	30.072461
410.415323	24067.001682	30.077479
410.530399	24123.356656	30.082496
411.093528	24170.171422	30.087514
411.259689	24208.856295	30.092532
411.690108	24238.590907	30.097549
412.358352	24281.699175	30.102567
412.846238	24336.801300	30.107584
413.216290	24357.871123	30.112602
413.272318	24431.189526	30.117620
413.908551	24473.461613	30.122637
414.206191	24500.918205	30.127655
414.551274	24543.214911	30.132672
415.414987	24594.744453	30.137690
415.975703	24633.101809	30.142708
416.245758	24667.543379	30.147725
416.833265	24710.513138	30.152743
417.141262	24732.667433	30.157760
417.430354	24769.251996	30.162778
417.631802	24815.812951	30.167796
418.137091	24848.245107	30.172813
418.631301	24904.973661	30.177831
419.101606	24964.703761	30.182848
419.412166	24978.988384	30.187866
419.932842	25024.052871	30.192884
420.502535	25072.791123	30.197901
421.258999	25115.174250	30.202919
421.349604	25133.237005	30.207936
422.074676	25153.553822	30.212954
422.375192	25181.468307	30.217972
422.368271	25208.664158	30.222989
423.168304	25235.039277	30.228007
423.408601	25277.214794	30.233024
424.076857	25319.583045	30.238042
424.199251	25361.037157	30.243060
424.108469	25392.791464	30.248077
424.745774	25414.018710	30.253095
424.929247	25473.615077	30.258112
425.598742	25521.303752	30.263130
425.759927	25562.283637	30.268148
426.281201	25618.932846	30.273165
426.654443	25651.667450	30.278183
426.589571	25688.085406	30.283200
427.327443	25737.281871	30.288218
427.825211	25797.448725	30.293236
428.347150	25836.649357	30.298253
429.189505	25878.966595	30.303271
429.248099	25919.183751	30.308288
429.983693	25959.550927	30.313306
430.470693	26009.852417	30.318324
430.384991	26066.969214	30.323341
431.273738	26114.881944	30.328359
431.662042	26153.405256	30.333376
432.261473	26183.187901	30.338394
432.641420	26242.365021	30.343412
432.720224	26273.366018	30.348429
433.485064	26331.740315	30.353447
433.905149	26378.502815	30.358464
434.564703	26410.325876	30.363482
434.704695	26458.673906	30.368500
435.178842	26489.177922	30.373517
435.383970	26521.098332	30.378535
435.804191	26598.809626	30.383552
436.443111	26647.851613	30.388570
436.485484	26680.865196	30.393588
437.208355	26726.504759	30.398605
437.893446	26788.022395	30.403623
437.972497	26817.057917	30.408640
438.550720	26874.537669	30.413658
439.118498	26931.235603	30.418676
439.684950	26962.789650	30.423693
440.317905	27016.420996	30.428711
440.666048	27052.895065	30.433728
441.289855	27103.620306	30.438746
442.015500	27132.311437	30.443764
442.315804	27168.434110	30.448781
442.635919	27212.558238	30.453799
443.219078	27253.002548	30.458816
443.504559	27271.812825	30.463834
443.964061	27321.033042	30.468852
444.322368	27363.044417	30.473869
444.912935	27402.018116	30.478887
445.148330	27461.898286	30.483904
445.234499	27497.886712	30.488922
445.611687	27546.597615	30.493940
446.391448	27583.099292	30.498957
446.477521	27626.742740	30.503975
446.946814	27673.281454	30.508992
447.589954	27732.773509	30.514010
448.323602	27767.592644	30.519028
448.312167	27814.091297	30.524045
449.071556	27853.044444	30.529063
449.349497	27911.411526	30.534080
450.095136	27939.577139	30.539098
450.416164	27984.100515	30.544116
450.644075	28057.410856	30.549133
451.421737	28074.286117	30.554151
451.554596	28111.264806	30.559168
451.740771	28160.273948	30.564186
452.272666	28207.674303	30.569204
452.413398	28267.389982	30.574221
453.329928	28294.644800	30.579239
453.103669	28332.282567	30.584256
453.995513	28391.515037	30.589274
454.401869	28443.671142	30.594292
454.784261	28500.187256	30.599309
455.269856	28524.302689	30.604327
455.706368	28599.306209	30.609344
456.311429	28633.157932	30.614362
456.966899	28677.381834	30.619380
457.247079	28743.561148	30.624397
457.968857	28805.860636	30.629415
458.272284	28836.340262	30.634432
458.817900	28870.016172	30.639450
459.302042	28931.017974	30.644468
459.745992	28958.825046	30.649485
460.268698	29011.405247	30.654503
460.878219	29059.772946	30.659520
461.218834	29094.943582	30.664538
461.553504	29146.631055	30.669556
462.121220	29200.197994	30.674573
462.898280	29235.325212	30.679591
463.018672	29289.931533	30.684608
463.296946	29349.751261	30.689626
464.198955	29383.924466	30.694644
464.573231	29423.540958	30.699661
465.018910	29468.400867	30.704679
465.513203	29526.674599	30.709696
465.814258	29587.131719	30.714714
466.374599	29632.086670	30.719732
466.688575	29664.821389	30.724749
467.077086	29704.606510	30.729767
467.616975	29762.182696	30.734784
467.974863	29842.459819	30.739802
468.477916	29874.693697	30.744820
468.773331	29919.901348	30.749837
469.760406	29984.678497	30.754855
470.284281	30036.018779	30.759872
470.737378	30081.487861	30.764890
471.272122	30127.867831	30.769908
471.398344	30183.718865	30.774925
472.157827	30210.078405	30.779943
472.411124	30270.224043	30.784960
472.746125	30316.176956	30.789978
473.269229	30366.783351	30.794996
473.793275	30443.285112	30.800013
474.440614	30484.123887	30.805031
474.945378	30521.147249	30.810048
475.152460	30573.036711	30.815066
476.106295	30633.597855	30.820084
476.473120	30690.618968	30.825101
477.222842	30709.438338	30.830119
477.995696	30742.742827	30.835136
478.305224	30803.981969	30.840154
478.900724	30827.369535	30.845172
479.306038	30873.697170	30.850189
480.077563	30911.746709	30.855207
480.051740	30957.202557	30.860224
480.518363	30998.198578	30.865242
480.821765	31026.227778	30.870260
481.035830	31094.871830	30.875277
481.436987	31137.121917	30.880295
481.924157	31202.115530	30.885312
482.142587	31236.506261	30.890330
482.698010	31287.245650	30.895348
483.231048	31350.494020	30.900365
483.632001	31390.823557	30.905383
484.169389	31433.585002	30.910400
484.352272	31479.979384	30.915418
484.912095	31515.755975	30.920436
485.181841	31578.815215	30.925453
485.447724	31641.976272	30.930471
486.307980	31717.554242	30.935488
486.299903	31760.248850	30.940506
487.105397	31809.197566	30.945524
487.428148	31896.130745	30.950541
487.920937	31942.254331	30.955559
488.524657	32004.212554	30.960576
489.413830	32079.304631	30.965594
489.753694	32121.463118	30.970612
489.832268	32169.163725	30.975629
490.322354	32243.842896	30.980647
490.854625	32287.522182	30.985664
491.422412	32367.672171	30.990682
492.145699	32440.871892	30.995700
492.567160	32493.148099	31.000717
493.098976	32551.110281	31.005735
493.847379	32615.349843	31.010752
494.150298	32669.558029	31.015770
494.872799	32716.166275	31.020788
495.317976	32783.333829	31.025805
495.952728	32834.430583	31.030823
496.895302	32877.734386	31.035840
497.024443	32935.272178	31.040858
497.883572	33001.791681	31.045876
498.425741	33061.993875	31.050893
498.901052	33106.050590	31.055911
499.425672	33147.146191	31.060928
499.530738	33215.280217	31.065946
500.060492	33248.440351	31.070964
500.677189	33322.289208	31.075981
500.815322	33381.070057	31.080999
501.589063	33426.630565	31.086016
501.794138	33501.595642	31.091034
502.095326	33544.549550	31.096052
502.741265	33608.942188	31.101069
503.374170	33674.230106	31.106087
504.120360	33721.124224	31.111104
504.359925	33805.199992	31.116122
505.073021	33856.861011	31.121140
505.512024	33914.893507	31.126157
506.059878	33986.658356	31.131175
507.016045	34034.547206	31.136192
507.266738	34071.888247	31.141210
507.710189	34138.212522	31.146228
508.319553	34186.465119	31.151245
508.627248	34234.922282	31.156263
509.368452	34307.467386	31.161280
509.683717	34365.231522	31.166298
510.601822	34419.845168	31.171316
510.862412	34466.010584	31.176333
511.364770	34525.877283	31.181351
512.269347	34582.465696	31.186368
513.138145	34647.248122	31.191386
513.681884	34662.486694	31.196404
514.374133	34686.989879	31.201421
514.714975	34739.737283	31.206439
515.157331	34801.041014	31.211456
515.332093	34845.259003	31.216474
516.162369	34874.147610	31.221492
516.323700	34919.699544	31.226509
516.884341	34985.733131	31.231527
517.053102	35040.485090	31.236544
517.168554	35074.209326	31.241562
517.594107	35125.186359	31.246580
517.963295	35178.305874	31.251597
518.414593	35225.438866	31.256615
518.853021	35291.752520	31.261632
518.843796	35379.022780	31.266650
519.768416	35439.349774	31.271668
520.073593	35484.945663	31.276685
520.347152	35555.275981	31.281703
521.288158	35633.299745	31.286720
521.397599	35709.378602	31.291738
521.903195	35778.936258	31.296756
522.443080	35840.012898	31.301773
523.256811	35923.912380	31.306791
523.913138	35988.043749	31.311808
524.639337	36055.309861	31.316826
525.346018	36116.192658	31.321844
525.944815	36188.235700	31.326861
526.831604	36252.405690	31.331879
527.539014	36304.529196	31.336896
528.179832	36360.223341	31.341914
528.706379	36417.410190	31.346932
529.480833	36460.980920	31.351949
529.596964	36511.113693	31.356967
530.164774	36567.480064	31.361984
530.350725	36647.195017	31.367002
530.909829	36687.349618	31.372020
531.260779	36743.859657	31.377037
531.535670	36813.803425	31.382055
532.445725	36877.773019	31.387072
532.401468	36956.435514	31.392090
532.886595	37025.417615	31.397108
533.418461	37080.485087	31.402125
534.020655	37149.666075	31.407143
535.268955	37230.997451	31.412160
535.352143	37318.265088	31.417178
535.902291	37370.578627	31.422196
536.782569	37404.584883	31.427213
537.458707	37482.262867	31.432231
538.097303	37552.095799	31.437248
538.520658	37629.030381	31.442266
539.216964	37678.240622	31.447284
539.578858	37739.296356	31.452301
539.981510	37812.123116	31.457319
540.774447	37856.546273	31.462336
540.892547	37938.234797	31.467354
541.565118	38007.599981	31.472372
541.996091	38069.970893	31.477389
542.395296	38122.936422	31.482407
542.970536	38199.766311	31.487424
543.500256	38274.281296	31.492442
543.765978	38332.899635	31.497460
544.700242	38418.002788	31.502477
545.470381	38496.363940	31.507495
545.931506	38538.962647	31.512512
546.357520	38619.255811	31.517530
547.132510	38697.632818	31.522548
547.623009	38753.914690	31.527565
548.239751	38831.030770	31.532583
548.724541	38883.659333	31.537600
549.457708	38938.150110	31.542618
549.975943	39001.330404	31.547636
550.692072	39076.370226	31.552653
551.118208	39141.955354	31.557671
551.736539	39201.979536	31.562688
551.881545	39278.244402	31.567706
552.756752	39322.149465	31.572724
553.175346	39363.684074	31.577741
553.599507	39446.657599	31.582759
554.546101	39493.508569	31.587776
554.902046	39556.922759	31.592794
555.492750	39594.730484	31.597812
556.122798	39655.571679	31.602829
556.663109	39708.357597	31.607847
557.129175	39778.846271	31.612864
557.503696	39839.061179	31.617882
557.660339	39900.423254	31.622900
558.669470	39989.390948	31.627917
558.972482	40044.625228	31.632935
559.401654	40101.009799	31.637952
559.835073	40181.813678	31.642970
560.237301	40261.123846	31.647988
560.648748	40327.107070	31.653005
560.901353	40412.682555	31.658023
561.376031	40502.116636	31.663040
562.229220	40571.468152	31.668058
562.783909	40640.228502	31.673076
563.458011	40729.163626	31.678093
564.015812	40813.996197	31.683111
564.857270	40876.368965	31.688128
565.450362	40965.927805	31.693146
565.677965	41040.961760	31.698164
566.681116	41118.929642	31.703181
567.166979	41200.556363	31.708199
567.958728	41280.561024	31.713216
568.718356	41356.325921	31.718234
569.082581	41418.918254	31.723252
570.006252	41488.015420	31.728269
570.523700	41570.721249	31.733287
571.004653	41641.423012	31.738304
571.417834	41698.749497	31.743322
571.969443	41779.742962	31.748340
572.948670	41856.931980	31.753357
573.290196	41921.000726	31.758375
573.963892	41990.958628	31.763392
574.441074	42079.061649	31.768410
574.966828	42150.805964	31.773428
575.706564	42193.455620	31.778445
576.175651	42276.886021	31.783463
576.741021	42357.358930	31.788480
577.805324	42435.666409	31.793498
577.989073	42494.046558	31.798516
578.921941	42556.962386	31.803533
579.393737	42644.778605	31.808551
580.293271	42691.705570	31.813568
580.858414	42767.110694	31.818586
581.555493	42834.305852	31.823604
582.058319	42888.388794	31.828621
582.800882	42947.429387	31.833639
583.510742	43004.865639	31.838656
583.937523	43073.135409	31.843674
584.258710	43145.517182	31.848692
585.103021	43210.129270	31.853709
585.208136	43286.142839	31.858727
586.040918	43345.848519	31.863744
586.696889	43421.004564	31.868762
586.846154	43505.112099	31.873780
587.387104	43550.380020	31.878797
587.744322	43619.184179	31.883815
588.070818	43702.082682	31.888832
588.628710	43785.161164	31.893850
589.268629	43865.950363	31.898868
589.978943	43942.889510	31.903885
590.452626	44010.154270	31.908903
591.261136	44091.330165	31.913920
591.849359	44179.314415	31.918938
592.040085	44231.789146	31.923956
592.857970	44286.780710	31.928973
593.594180	44361.763174	31.933991
594.198196	44450.456423	31.939008
594.298256	44538.141011	31.944026
595.391077	44601.084765	31.949044
595.796523	44659.043685	31.954061
596.209768	44752.353870	31.959079
596.673607	44813.618510	31.964096
597.771524	44898.447041	31.969114
598.021425	44989.667016	31.974132
599.023570	45044.696700	31.979149
599.509989	45119.729802	31.984167
599.863541	45207.246244	31.989184
600.582571	45281.449147	31.994202
601.199633	45365.288969	31.999220
601.836596	45457.195551	32.004237
602.286124	45540.650247	32.009255
602.870506	45604.461203	32.014272
603.505479	45671.411735	32.019290
603.623675	45768.567531	32.024308
604.481933	45871.373000	32.029325
605.283635	45943.629516	32.034343
605.738077	46029.409312	32.039360
606.527696	46142.049802	32.044378
607.030278	46217.097287	32.049396
607.748205	46284.228913	32.054413
608.002430	46383.158782	32.059431
608.805174	46482.806855	32.064448
609.270003	46566.617234	32.069466
609.775949	46645.056860	32.074484
610.870766	46742.081681	32.079501
611.555063	46828.215537	32.084519
611.975363	46913.626144	32.089536
613.014207	46992.023417	32.094554
613.634089	47076.148311	32.099572
614.232506	47158.259528	32.104589
614.647178	47239.896258	32.109607
615.164777	47341.165247	32.114624
616.580645	47407.869890	32.119642
616.924419	47473.327808	32.124660
617.858173	47554.289727	32.129677
618.690423	47632.660651	32.134695
619.369118	47702.389849	32.139712
620.080193	47775.034682	32.144730
620.378920	47834.078864	32.149748
621.102162	47911.483799	32.154765
621.583312	48011.723584	32.159783
621.907661	48085.522851	32.164800
622.803865	48150.023549	32.169818
623.032379	48231.183798	32.174836
623.930628	48319.142679	32.179853
624.291642	48379.776044	32.184871
624.742545	48479.644395	32.189888
625.358185	48571.550835	32.194906
625.774791	48645.668612	32.199924
626.723984	48721.072318	32.204941
627.365372	48814.598745	32.209959
627.787394	48923.217920	32.214976
628.430881	48996.620690	32.219994
629.018238	49070.951923	32.225012
629.684446	49151.996472	32.230029
630.228786	49244.495831	32.235047
630.607828	49327.893742	32.240064
631.093078	49410.775546	32.245082
631.763036	49521.813983	32.250100
632.589707	49599.480330	32.255117
633.360165	49667.486924	32.260135
633.732499	49765.859265	32.265152
634.588495	49855.562785	32.270170
635.128545	49931.402043	32.275188
635.918861	49986.452804	32.280205
636.894669	50077.122850	32.285223
637.525994	50176.847190	32.290240
638.042149	50253.241160	32.295258
638.444570	50328.757358	32.300276
639.346945	50398.289027	32.305293
639.874655	50473.658789	32.310311
640.402278	50576.351910	32.315328
641.132609	50647.321373	32.320346
641.557889	50727.717672	32.325364
642.388500	50794.537261	32.330381
642.824951	50895.598660	32.335399
643.512679	50995.469554	32.340416
644.361021	51083.421076	32.345434
644.638017	51170.030425	32.350452
645.302462	51255.770858	32.355469
646.095046	51330.977094	32.360487
646.630352	51431.819722	32.365504
647.520534	51535.895079	32.370522
648.155446	51624.016979	32.375540
648.444280	51702.459733	32.380557
648.965554	51806.663809	32.385575
649.766426	51907.727213	32.390592
650.645343	51987.791755	32.395610
651.091187	52102.173107	32.400628
651.734069	52195.036858	32.405645
652.850098	52269.340627	32.410663
652.864048	52371.300737	32.415680
653.989241	52469.638456	32.420698
654.782699	52584.855916	32.425716
655.485015	52655.992211	32.430733
655.981251	52730.033752	32.435751
656.519184	52829.032482	32.440768
657.507214	52941.374244	32.445786
657.845259	53042.374762	32.450804
658.581224	53125.250209	32.455821
659.451878	53220.153215	32.460839
659.815239	53319.432808	32.465856
660.693324	53419.562813	32.470874
661.317853	53514.226807	32.475892
661.938368	53589.542942	32.480909
662.673644	53688.529280	32.485927
663.016444	53806.178392	32.490944
663.929754	53911.990494	32.495962
664.568995	53993.982293	32.500980
664.974921	54072.298481	32.505997
666.024898	54184.602494	32.511015
666.470026	54281.428759	32.516032
666.797906	54370.353031	32.521050
667.704298	54483.642709	32.526068
668.265914	54589.055424	32.531085
668.836305	54684.056253	32.536103
669.709179	54775.526710	32.541120
670.354113	54878.684562	32.546138
670.988459	54997.568858	32.551156
671.413462	55090.359300	32.556173
672.428768	55196.717494	32.561191
672.958854	55302.581504	32.566208
673.705687	55402.857130	32.571226
674.415568	55510.177207	32.576244
675.106808	55597.436076	32.581261
675.857701	55684.698118	32.586279
676.450525	55809.103232	32.591296
677.555138	55893.938648	32.596314
677.971238	55979.772627	32.601332
678.853652	56052.711152	32.606349
679.547179	56148.532723	32.611367
679.924847	56243.174943	32.616384
680.859917	56302.256955	32.621402
681.545159	56408.246636	32.626420
682.168740	56510.083546	32.631437
682.888757	56584.030150	32.636455
683.349812	56685.281966	32.641472
684.407790	56757.663409	32.646490
684.706000	56857.211864	32.651508
685.389384	56960.766063	32.656525
686.323996	57037.389397	32.661543
686.765918	57144.130859	32.666560
687.217671	57237.900048	32.671578
688.137229	57332.710750	32.676596
688.527302	57452.427417	32.681613
689.380732	57556.575855	32.686631
689.947364	57651.477965	32.691648
690.394550	57762.101347	32.696666
691.018048	57864.760342	32.701684
691.589471	57975.933057	32.706701
692.313142	58068.410237	32.711719
692.783183	58186.172061	32.716736
693.955093	58314.332697	32.721754
694.639733	58431.567695	32.726772
695.336990	58543.771698	32.731789
696.031901	58645.456202	32.736807
696.750788	58758.814159	32.741824
697.619370	58849.356498	32.746842
698.376747	58975.125572	32.751860
698.827166	59102.329946	32.756877
699.771748	59190.693949	32.761895
700.349299	59290.075815	32.766912
701.383410	59410.159221	32.771930
702.032967	59526.205885	32.776948
702.464341	59629.487075	32.781965
703.517525	59731.414956	32.786983
704.139648	59847.284768	32.792000
704.946998	59951.308049	32.797018
705.841559	60041.921032	32.802036
706.575966	60150.557681	32.807053
707.380554	60267.107536	32.812071
707.869496	60373.428893	32.817088
709.093064	60465.259617	32.822106
709.687291	60551.911814	32.827124
710.322562	60662.621366	32.832141
711.370733	60764.707008	32.837159
711.763038	60856.664165	32.842176
712.676962	60966.482588	32.847194
713.190835	61069.460576	32.852212
713.849912	61171.644141	32.857229
714.770258	61255.111083	32.862247
715.386815	61359.166863	32.867264
715.946138	61467.700534	32.872282
716.509575	61564.403907	32.877300
716.985411	61674.791470	32.882317
717.925565	61782.998527	32.887335
718.465448	61895.879293	32.892352
719.199150	62001.682230	32.897370
719.932551	62090.504687	32.902388
720.308292	62215.756757	32.907405
721.450206	62329.848720	32.912423
722.076503	62443.672565	32.917440
723.095814	62534.724898	32.922458
723.898041	62628.107608	32.927476
724.684895	62743.347559	32.932493
725.487442	62840.738026	32.937511
726.779940	62926.115932	32.942528
727.514322	63001.986282	32.947546
728.317153	63089.367019	32.952564
728.321973	63194.177914	32.957581
728.976800	63256.979834	32.962599
729.237905	63372.095296	32.967616
730.210958	63467.058969	32.972634
731.152768	63557.679966	32.977652
732.051735	63662.497300	32.982669
732.461403	63740.718267	32.987687
733.056096	63850.010974	32.992704
733.885782	63961.079387	32.997722
734.579022	64067.493891	33.002740
735.299066	64167.388231	33.007757
735.987327	64256.391953	33.012775
736.323837	64382.744645	33.017792
737.000452	64511.645987	33.022810
737.734962	64596.200263	33.027828
738.343481	64710.185098	33.032845
739.077956	64829.370556	33.037863
739.548365	64967.941368	33.042880
740.262437	65095.645605	33.047898
740.890196	65200.819010	33.052916
741.481609	65329.379286	33.057933
742.263691	65450.235480	33.062951
743.105121	65585.038904	33.067968
744.116165	65704.196411	33.072986
744.816588	65843.493645	33.078004
745.674565	65963.651347	33.083021
746.687287	66061.888431	33.088039
747.265594	66191.138918	33.093056
747.779007	66332.455127	33.098074
748.867302	66451.446175	33.103092
749.362286	66573.001114	33.108109
750.303151	66679.483081	33.113127
751.175730	66825.579019	33.118144
752.067652	66965.263075	33.123162
752.768256	67078.898148	33.128180
753.378703	67190.380530	33.133197
754.223145	67328.722120	33.138215
755.046772	67432.509147	33.143232
755.722851	67566.840776	33.148250
756.806763	67711.125419	33.153268
757.244366	67832.918469	33.158285
758.747447	67929.028960	33.163303
759.682196	68049.508488	33.168320
760.838902	68162.770738	33.173338
761.706384	68272.832054	33.178356
762.516158	68363.097754	33.183373
763.352524	68455.496180	33.188391
763.837700	68575.825410	33.193408
764.424504	68702.713167	33.198426
765.425676	68798.474353	33.203444
765.948396	68899.062664	33.208461
766.651309	68978.569991	33.213479
767.437745	69112.242203	33.218496
767.595149	69236.706966	33.223514
768.589181	69356.925048	33.228532
769.015628	69482.231912	33.233549
769.758138	69584.999914	33.238567
770.340536	69713.158920	33.243584
770.535952	69841.022250	33.248602
771.460359	69961.761059	33.253620
772.063404	70094.502521	33.258637
773.357888	70213.967810	33.263655
774.075413	70361.346921	33.268672
774.733209	70490.705758	33.273690
775.616064	70592.165756	33.278708
776.014212	70733.012349	33.283725
776.781623	70851.569353	33.288743
777.552082	70976.240310	33.293760
777.962570	71124.010531	33.298778
779.141528	71236.590221	33.303796
779.827036	71349.447992	33.308813
780.587781	71476.374322	33.313831
781.167892	71617.993396	33.318848
782.464117	71767.436431	33.323866
783.102443	71871.927240	33.328884
783.864867	71986.571343	33.333901
784.652809	72124.669326	33.338919
785.798038	72248.413329	33.343936
786.186790	72380.331953	33.348954
787.173768	72521.674879	33.353972
787.996346	72644.620871	33.358989
788.716772	72765.308173	33.364007
789.715710	72892.557701	33.369024
790.403754	73025.341399	33.374042
791.299191	73149.182459	33.379060
792.068582	73285.994788	33.384077
793.050348	73418.485821	33.389095
794.025723	73531.692994	33.394112
794.773981	73663.566489	33.399130
795.579435	73790.910215	33.404148
796.165412	73921.977423	33.409165
797.141542	74054.403757	33.414183
798.184430	74196.956265	33.419200
798.604256	74322.994645	33.424218
799.802618	74441.639552	33.429236
800.317383	74566.803690	33.434253
801.169568	74709.201373	33.439271
802.234420	74830.045760	33.444288
802.699079	74963.099638	33.449306
803.370549	75096.758874	33.454324
804.172110	75239.200026	33.459341
804.577526	75372.531798	33.464359
805.705125	75497.764546	33.469376
806.225612	75651.435240	33.474394
807.592613	75797.562008	33.479412
808.211596	75916.000807	33.484429
808.815882	76043.422647	33.489447
809.942846	76186.157775	33.494464
810.300380	76342.592214	33.499482
811.475364	76479.832099	33.504500
812.317260	76611.663836	33.509517
812.912968	76750.828741	33.514535
814.283321	76875.959777	33.519552
815.116292	77022.138678	33.524570
815.830722	77173.732715	33.529588
816.855195	77298.758856	33.534605
817.820888	77433.440011	33.539623
818.812229	77559.851817	33.544640
819.335738	77691.249336	33.549658
820.176165	77822.974776	33.554676
821.042019	77942.920638	33.559693
821.612724	78083.040480	33.564711
822.768220	78206.070585	33.569728
823.372967	78335.611773	33.574746
824.414930	78459.035191	33.579764
825.064714	78609.536679	33.584781
825.689346	78759.081992	33.589799
826.628287	78867.294818	33.594816
827.177667	79004.533633	33.599834
828.024505	79146.790360	33.604852
828.726021	79299.318271	33.609869
829.158223	79426.927318	33.614887
830.211804	79569.639641	33.619904
831.248360	79689.800832	33.624922
832.150769	79810.345351	33.629940
833.216630	79937.846381	33.634957
834.092185	80056.341030	33.639975
834.654697	80187.980984	33.644992
835.148351	80333.959557	33.650010
836.397135	80442.628599	33.655028
837.527477	80557.187531	33.660045
837.861976	80703.808352	33.665063
838.697802	80840.587418	33.670080
839.630906	80990.596519	33.675098
840.623199	81110.665159	33.680116
841.335376	81235.126254	33.685133
841.757403	81380.294863	33.690151
842.569299	81539.594446	33.695168
843.112243	81680.918111	33.700186
844.239115	81811.860863	33.705204
844.956155	81967.415430	33.710221
845.638638	82141.384457	33.715239
846.561905	82284.268486	33.720256
847.029851	82416.740521	33.725274
848.100192	82567.724318	33.730292
849.204473	82747.688482	33.735309
850.050774	82914.659030	33.740327
850.709418	83062.810539	33.745344
851.468333	83211.180521	33.750362
852.672100	83365.683835	33.755380
853.527004	83513.084718	33.760397
854.263166	83662.960688	33.765415
855.205454	83828.036946	33.770432
856.251804	83987.757923	33.775450
857.064818	84119.866634	33.780468
858.134511	84281.395117	33.785485
859.308020	84432.658989	33.790503
860.487751	84566.341927	33.795520
861.159065	84723.238849	33.800538
862.392839	84877.241371	33.805556
863.144690	85009.181868	33.810573
864.095361	85143.386818	33.815591
864.847006	85288.627271	33.820608
865.559129	85455.315964	33.825626
866.569031	85595.897312	33.830644
867.513700	85723.855947	33.835661
868.257327	85873.903365	33.840679
869.447815	86011.736961	33.845696
870.347697	86144.798362	33.850714
871.137927	86303.059369	33.855732
871.784079	86444.503147	33.860749
872.342178	86582.261096	33.865767
873.578001	86719.047501	33.870784
874.171171	86880.400915	33.875802
875.246483	87041.935252	33.880820
875.857598	87174.347969	33.885837
876.663108	87320.237697	33.890855
877.906398	87482.443352	33.895872
878.456360	87636.412736	33.900890
879.256983	87786.045565	33.905908
879.914695	87950.236689	33.910925
880.793366	88110.248096	33.915943
881.518286	88255.271177	33.920960
882.911211	88412.187928	33.925978
883.306429	88563.423919	33.930996
884.567851	88702.248892	33.936013
885.099247	88882.469621	33.941031
885.890019	89044.843131	33.946048
886.746698	89205.555379	33.951066
887.625154	89370.283193	33.956084
888.631877	89510.629358	33.961101
889.267125	89662.471908	33.966119
890.123163	89826.751029	33.971136
890.999945	89959.926651	33.976154
891.973605	90110.678456	33.981172
892.898471	90285.232175	33.986189
893.355918	90442.348611	33.991207
894.418017	90596.569288	33.996224
895.319835	90779.477076	34.001242
895.799384	90946.370023	34.006260
897.271012	91091.255677	34.011277
897.870392	91257.776657	34.016295
898.818975	91419.843046	34.021312
899.772794	91590.003505	34.026330
900.668645	91756.694191	34.031348
901.922157	91899.880515	34.036365
902.344179	92085.408916	34.041383
903.418729	92249.061234	34.046400
904.165457	92430.906193	34.051418
904.911024	92592.090120	34.056436
906.004587	92761.887800	34.061453
906.826336	92961.773463	34.066471
907.953631	93096.665680	34.071488
909.000078	93290.144033	34.076506
909.950440	93465.969949	34.081524
911.007867	93624.090510	34.086541
911.712335	93791.529464	34.091559
912.642104	93973.590057	34.096576
913.796640	94135.685137	34.101594
914.760105	94322.786951	34.106612
915.864407	94490.525490	34.111629
916.534961	94650.748269	34.116647
917.469936	94814.396795	34.121664
918.383025	95003.524841	34.126682
919.554973	95182.484910	34.131700
920.556105	95349.265400	34.136717
920.957022	95524.089381	34.141735
922.399283	95688.856276	34.146752
923.242435	95856.463820	34.151770
923.744863	96042.844848	34.156788
924.979600	96200.839014	34.161805
925.798864	96390.404733	34.166823
926.614596	96581.643506	34.171840
927.556747	96750.063670	34.176858
928.004314	96920.414906	34.181876
929.074897	97091.651889	34.186893
929.973547	97309.663563	34.191911
931.053204	97503.866237	34.196928
932.071506	97671.514235	34.201946
932.532932	97863.992495	34.206964
934.165485	98042.004896	34.211981
935.169900	98224.958392	34.216999
935.830284	98403.140232	34.222016
936.916858	98596.704690	34.227034
937.787887	98775.727978	34.232052
939.150685	98935.199788	34.237069
940.041606	99136.821070	34.242087
940.811898	99292.404963	34.247104
942.215490	99475.998096	34.252122
943.174654	99671.516362	34.257140
944.270182	99849.516438	34.262157
945.048544	100015.181487	34.267175
946.145824	100161.866867	34.272192
947.002545	100345.347771	34.277210
947.796083	100535.956001	34.282228
949.207565	100699.843444	34.287245
949.813503	100869.442254	34.292263
950.540266	101024.398368	34.297280
951.741574	101203.422484	34.302298
952.326460	101374.167698	34.307316
953.184478	101521.128418	34.312333
953.732597	101703.043146	34.317351
954.833674	101884.779254	34.322368
955.917292	102064.936812	34.327386
956.334272	102220.888385	34.332404
957.556794	102400.215024	34.337421
958.466111	102577.511716	34.342439
959.230589	102768.660723	34.347456
960.455853	102938.101491	34.352474
961.462616	103130.283176	34.357492
962.412724	103320.493976	34.362509
963.373660	103492.065046	34.367527
964.134632	103682.157811	34.372544
965.164303	103835.504552	34.377562
965.754309	104052.270772	34.382580
967.079270	104236.614224	34.387597
967.923483	104420.493858	34.392615
968.633856	104616.775133	34.397632
969.916241	104818.547959	34.402650
970.665555	105010.013761	34.407668
971.978057	105216.989365	34.412685
972.935401	105408.366784	34.417703
973.567729	105590.073604	34.422720
974.638138	105799.917824	34.427738
975.362692	106002.013585	34.432756
976.305469	106198.990319	34.437773
977.408563	106400.216183	34.442791
978.274891	106593.478964	34.447808
979.939536	106813.396201	34.452826
980.872819	107002.205808	34.457844
982.498619	107206.492336	34.462861
983.196530	107404.943334	34.467879
984.210892	107593.072592	34.472896
985.550400	107777.350108	34.477914
985.855765	107980.188916	34.482932
987.111811	108183.796866	34.487949
987.873209	108386.272214	34.492967
988.822017	108596.519862	34.497984
990.060211	108781.695011	34.503002
990.575369	108979.086153	34.508020
991.479159	109180.391525	34.513037
992.923513	109394.337966	34.518055
993.761569	109612.793844	34.523072
995.020675	109800.011798	34.528090
995.619479	110002.779628	34.533108
996.603075	110199.431194	34.538125
997.710257	110430.211199	34.543143
998.324722	110641.328148	34.548160
999.704541	110827.646743	34.553178
1000.694743	111036.855515	34.558196
1001.484260	111254.712158	34.563213
1002.418917	111480.133803	34.568231
1003.163329	111694.530839	34.573248
1004.729779	111883.967237	34.578266
1005.461622	112107.008268	34.583284
1006.722564	112309.316830	34.588301
1007.745917	112538.988713	34.593319
1008.970453	112756.810966	34.598336
1009.747510	112941.761607	34.603354
1010.949508	113161.376884	34.608372
1012.311892	113379.586711	34.613389
1013.430623	113560.836949	34.618407
1014.429218	113773.270298	34.623424
1015.612724	113968.940851	34.628442
1016.196377	114157.136548	34.633460
1017.377904	114355.749090	34.638477
1018.432202	114567.672679	34.643495
1019.349767	114756.083372	34.648512
1020.776546	114931.274514	34.653530
1021.311165	115127.187108	34.658548
1022.477064	115327.418083	34.663565
1023.457103	115508.666043	34.668583
1024.020419	115701.195519	34.673600
1025.159805	115900.269516	34.678618
1025.741441	116128.701461	34.683636
1026.504061	116333.909019	34.688653
1027.623943	116532.103944	34.693671
1028.811076	116746.657359	34.698688
1029.671027	116966.992811	34.703706
1030.691151	117170.555039	34.708724
1031.931056	117369.724270	34.713741
1032.718079	117599.337885	34.718759
1033.446944	117837.312087	34.723776
1034.653321	118038.176611	34.728794
1035.333954	118249.277671	34.733812
1036.348979	118497.827286	34.738829
1037.510871	118745.848046	34.743847
1038.306811	118962.484748	34.748864
1039.683212	119168.675911	34.753882
1040.673957	119406.924147	34.758900
1041.724068	119658.252868	34.763917
1043.032728	119895.299712	34.768935
1044.159787	120107.354489	34.773952
1045.146200	120326.960318	34.778970
1046.311339	120582.282036	34.783988
1047.119576	120805.139267	34.789005
1048.368152	121037.010483	34.794023
1049.545978	121276.358401	34.799040
1050.578283	121499.690845	34.804058
1051.901109	121731.834146	34.809076
1052.961115	121958.041891	34.814093
1053.861353	122200.154907	34.819111
1055.247568	122417.442470	34.824128
1056.283478	122653.898095	34.829146
1057.698786	122866.749184	34.834164
1058.838708	123085.070766	34.839181
1060.552322	123314.792574	34.844199
1061.484123	123537.143496	34.849216
1062.559658	123740.413731	34.854234
1063.605183	123970.162257	34.859252
1064.533102	124197.866427	34.864269
1065.546049	124408.362066	34.869287
1066.393208	124617.809424	34.874304
1067.186606	124839.280607	34.879322
1068.341116	125091.906293	34.884340
1069.164930	125317.266494	34.889357
1070.288366	125536.255244	34.894375
1071.141300	125793.207381	34.899392
1072.159652	126017.881777	34.904410
1073.713802	126241.759720	34.909428
1074.372810	126481.527138	34.914445
1075.945403	126694.899396	34.919463
1076.646579	126950.340378	34.924480
1078.186345	127181.413484	34.929498
1078.907471	127411.457539	34.934516
1080.127177	127629.203670	34.939533
1081.232333	127859.263777	34.944551
1082.074889	128108.633175	34.949568
1083.170750	128343.577908	34.954586
1084.252125	128568.970642	34.959604
1084.977900	128811.267632	34.964621
1086.147903	129050.033151	34.969639
1086.813636	129290.937017	34.974656
1088.194317	129535.945329	34.979674
1089.148404	129758.262609	34.984692
1089.801715	129983.128041	34.989709
1091.304606	130226.423286	34.994727
1092.333386	130479.152712	34.999744
1093.342862	130695.624524	35.004762
1094.499507	130935.408188	35.009780
1095.455979	131173.908541	35.014797
1096.335981	131414.400675	35.019815
1097.329842	131653.773119	35.024832
1098.480330	131901.335186	35.029850
1099.880951	132159.695455	35.034868
1100.671437	132385.886554	35.039885
1102.196665	132639.945868	35.044903
1102.943097	132898.420209	35.049920
1104.013062	133151.925020	35.054938
1105.343215	133383.282011	35.059956
1106.383549	133628.695592	35.064973
1107.387785	133882.217105	35.069991
1108.733774	134143.606897	35.075008
1110.106082	134398.022484	35.080026
1111.297907	134654.738985	35.085044
1112.472318	134902.244550	35.090061
1113.777010	135124.415213	35.095079
1114.805019	135392.852562	35.100096
1115.627253	135651.767757	35.105114
1117.011257	135898.752006	35.110132
1117.868354	136148.259123	35.115149
1119.055517	136388.801633	35.120167
1119.752142	136670.995651	35.125184
1120.882173	136940.455873	35.130202
1122.408665	137172.479688	35.135220
1123.426100	137440.035655	35.140237
1124.545368	137705.396443	35.145255
1125.624625	137977.650019	35.150272
1126.356465	138247.452981	35.155290
1128.004218	138524.371449	35.160308
1129.037940	138782.477892	35.165325
1130.123961	139041.008777	35.170343
1130.910634	139325.797121	35.175360
1132.326259	139585.266749	35.180378
1133.637339	139852.109187	35.185396
1134.412379	140121.425822	35.190413
1135.795565	140400.178625	35.195431
1136.732246	140669.916750	35.200448
1137.888896	140946.353232	35.205466
1139.598026	141212.709725	35.210484
1140.912597	141479.260246	35.215501
1142.230677	141747.092892	35.220519
1142.966619	142013.235968	35.225536
1143.839794	142258.297984	35.230554
1145.966421	142532.381102	35.235572
1146.918800	142808.688997	35.240589
1148.315964	143059.071789	35.245607
1149.253182	143339.443978	35.250624
1150.468563	143580.084457	35.255642
1151.598379	143844.566435	35.260660
1152.753652	144118.708468	35.265677
1154.190945	144364.377149	35.270695
1155.161858	144647.353850	35.275712
1156.098824	144894.326183	35.280730
1157.210495	145136.148524	35.285748
1158.262208	145426.548978	35.290765
1159.309669	145677.832695	35.295783
1160.327895	145967.406242	35.300800
1161.282155	146260.441932	35.305818
1162.521177	146514.527852	35.310836
1163.412464	146778.640309	35.315853
1164.779704	147057.043918	35.320871
1165.516223	147315.935933	35.325888
1166.594388	147581.925716	35.330906
1167.697929	147868.051422	35.335924
1168.865684	148141.144878	35.340941
1169.544927	148385.356211	35.345959
1171.050089	148670.800643	35.350976
1171.928418	148951.988263	35.355994
1173.310219	149224.027395	35.361012
1174.187155	149522.112009	35.366029
1175.746898	149788.406422	35.371047
1176.736060	150065.082246	35.376064
1177.890198	150357.725340	35.381082
1179.282257	150634.212157	35.386100
1180.580813	150930.425121	35.391117
1181.679285	151221.359488	35.396135
1182.950175	151510.656991	35.401152
1184.011181	151779.508668	35.406170
1185.596130	152068.441631	35.411188
1186.507206	152362.675429	35.416205
1187.952757	152639.054304	35.421223
1189.021679	152928.713289	35.426240
1190.225086	153246.775600	35.431258
1191.702071	153521.570402	35.436276
1192.405562	153796.799293	35.441293
1194.069749	154098.874982	35.446311
1194.956036	154393.762998	35.451328
1196.253491	154694.280463	35.456346
1198.030832	154965.180319	35.461364
1198.532984	155264.882275	35.466381
1200.418020	155568.949959	35.471399
1201.620313	155872.003861	35.476416
1202.565530	156146.943487	35.481434
1204.129048	156429.266795	35.486452
1205.383535	156737.075527	35.491469
1206.329071	157033.483537	35.496487
1207.752716	157317.447349	35.501504
1208.796073	157621.606705	35.506522
1210.299874	157896.200152	35.511540
1211.249420	158204.806539	35.516557
1212.406626	158498.070228	35.521575
1213.990201	158778.263464	35.526592
1214.933227	159088.362009	35.531610
1216.588124	159392.002816	35.536628
1217.586482	159686.836460	35.541645
1218.644313	159967.099501	35.546663
1220.047412	160281.825045	35.551680
1221.251010	160579.320744	35.556698
1222.588074	160861.865436	35.561716
1223.475365	161189.407073	35.566733
1224.619268	161466.469514	35.571751
1226.067026	161782.734405	35.576768
1226.664322	162080.062122	35.581786
1228.500942	162359.413992	35.586804
1229.992375	162671.454039	35.591821
1230.938680	162976.685006	35.596839
1232.252878	163286.957502	35.601856
1233.284870	163593.384109	35.606874
1234.899571	163869.243282	35.611892
1236.030623	164176.761591	35.616909
1237.428170	164471.678142	35.621927
1238.919042	164786.081286	35.626944
1239.865249	165083.131932	35.631962
1241.478233	165376.877451	35.636980
1242.357450	165678.003243	35.641997
1243.390455	165955.964055	35.647015
1244.786211	166267.196718	35.652032
1245.573731	166580.295614	35.657050
1246.995295	166869.718538	35.662068
1248.033140	167165.690171	35.667085
1249.235194	167467.435061	35.672103
1250.538917	167745.121737	35.677120
1251.479207	168062.025251	35.682138
1252.624279	168367.947477	35.687156
1253.517553	168674.065669	35.692173
1254.644434	168961.013582	35.697191
1256.102066	169279.185497	35.702208
1257.212923	169591.009298	35.707226
1258.676776	169910.314011	35.712244
1259.075629	170226.370884	35.717261
1260.589336	170538.655094	35.722279
1261.609311	170868.292410	35.727296
1262.898544	171205.691368	35.732314
1264.297285	171518.331298	35.737332
1265.300174	171854.792642	35.742349
1266.680304	172200.647642	35.747367
1268.314392	172536.362714	35.752384
1269.505785	172872.445180	35.757402
1270.707659	173200.775138	35.762420
1271.782365	173538.176061	35.767437
1273.193859	173893.378161	35.772455
1274.745289	174209.767429	35.777472
1275.969941	174551.592384	35.782490
1277.424686	174895.526457	35.787508
1278.894381	175261.236614	35.792525
1280.048116	175572.865855	35.797543
1281.626481	175904.528288	35.802560
1282.844314	176266.899525	35.807578
1284.376450	176596.708952	35.812596
1285.652013	176925.128983	35.817613
1286.726743	177272.962843	35.822631
1288.222281	177605.856355	35.827648
1289.635416	177945.187255	35.832666
1291.093264	178277.177867	35.837684
1292.494937	178640.183840	35.842701
1293.770629	178974.709360	35.847719
1295.216191	179296.315003	35.852736
1296.275685	179628.570872	35.857754
1297.996264	179970.454030	35.862772
1299.076710	180329.540394	35.867789
1300.156457	180654.768777	35.872807
1301.884108	180984.968928	35.877824
1302.948673	181327.934177	35.882842
1304.362131	181653.520057	35.887860
1305.657798	182007.265046	35.892877
1307.022722	182342.826360	35.897895
1308.921869	182654.885136	35.902912
1310.035576	183009.492047	35.907930
1311.095996	183352.496935	35.912948
1312.740134	183685.520561	35.917965
1313.941461	184019.939390	35.922983
1315.149699	184331.614587	35.928000
1315.956219	184693.074030	35.933018
1317.611412	185051.121216	35.938036
1318.716324	185382.467631	35.943053
1319.742362	185715.111080	35.948071
1321.402314	186066.741826	35.953088
1322.606126	186413.017632	35.958106
1323.972416	186757.859931	35.963124
1325.168330	187128.105785	35.968141
1326.264347	187477.287471	35.973159
1327.889234	187801.848274	35.978176
1328.984955	188157.215884	35.983194
1330.261529	188520.019583	35.988212
1331.777346	188866.297473	35.993229
1332.626122	189225.672998	35.998247
1334.214233	189571.854465	36.003264
1335.322714	189913.433272	36.008282
1336.586673	190256.651350	36.013300
1338.349145	190598.811803	36.018317
1339.927848	190922.319307	36.023335
1341.438153	191247.071230	36.028352
1342.362899	191601.409729	36.033370
1343.980261	191940.314356	36.038388
1345.443616	192265.181277	36.043405
1346.810030	192628.427870	36.048423
1347.954037	192951.205968	36.053440
1349.391051	193280.462362	36.058458
1350.390989	193641.300255	36.063476
1351.703544	193986.296780	36.068493
1352.995488	194335.068973	36.073511
1354.147276	194677.392045	36.078528
1355.391695	195040.609950	36.083546
1356.640205	195387.605402	36.088564
1358.442389	195746.787368	36.093581
1359.503865	196125.681956	36.098599
1361.183724	196479.302591	36.103616
1362.785642	196833.915616	36.108634
1364.090913	197204.677059	36.113652
1365.527715	197555.246254	36.118669
1366.980305	197905.776696	36.123687
1368.463386	198271.754295	36.128704
1369.700571	198640.757992	36.133722
1371.399407	198982.608084	36.138740
1372.896633	199331.526600	36.143757
1373.690883	199711.768898	36.148775
1375.140283	200085.024195	36.153792
1376.632721	200435.879121	36.158810
1378.028615	200783.996833	36.163828
1379.702166	201155.557997	36.168845
1380.876549	201524.105771	36.173863
1382.522827	201903.978743	36.178880
1383.785697	202258.093172	36.183898
1385.153292	202622.285627	36.188916
1386.411587	202996.147210	36.193933
1387.846337	203367.505903	36.198951
1389.212529	203737.062301	36.203968
1390.619468	204115.691897	36.208986
1391.811152	204478.589944	36.214004
1393.205309	204852.604046	36.219021
1394.635560	205245.075106	36.224039
1396.112016	205628.068909	36.229056
1397.215486	205998.302513	36.234074
1398.535028	206393.489776	36.239092
1399.848402	206778.357568	36.244109
1401.308638	207162.111180	36.249127
1402.263370	207556.679212	36.254144
1404.091015	207941.887140	36.259162
1405.124786	208344.585114	36.264180
1406.547809	208747.525711	36.269197
1407.653042	209136.566494	36.274215
1409.036358	209544.825295	36.279232
1410.584984	209940.831292	36.284250
1411.633222	210329.087487	36.289268
1413.366017	210745.332384	36.294285
1414.370439	211187.958417	36.299303
1415.813045	211583.405992	36.304320
1417.325979	211983.465884	36.309338
1419.094671	212404.665540	36.314356
1420.550014	212804.319903	36.319373
1421.930442	213233.562136	36.324391
1423.418547	213622.485214	36.329408
1424.960166	214026.715153	36.334426
1426.266102	214448.661738	36.339444
1428.020741	214838.409847	36.344461
1429.242913	215250.164802	36.349479
1430.823495	215637.176981	36.354496
1432.562072	216011.567983	36.359514
1434.232583	216369.362234	36.364532
1435.524622	216771.436517	36.369549
1436.785677	217224.616681	36.374567
1438.246171	217621.308129	36.379584
1439.537109	217990.269981	36.384602
1440.737397	218362.930882	36.389620
1442.357920	218766.356518	36.394637
1443.408030	219183.414949	36.399655
1444.910236	219586.228644	36.404672
1446.068971	219971.728566	36.409690
1447.630400	220383.044078	36.414708
1449.149926	220797.187410	36.419725
1449.934372	221217.955702	36.424743
1451.549440	221632.112126	36.429760
1452.954990	222055.194248	36.434778
1454.110703	222478.827314	36.439796
1455.774517	222883.354721	36.444813
1457.219543	223323.706546	36.449831
1458.924022	223765.033339	36.454848
1460.395331	224189.129176	36.459866
1461.793743	224619.918637	36.464884
1463.269073	225068.882854	36.469901
1464.757169	225501.946880	36.474919
1466.103110	225921.549008	36.479936
1467.904424	226369.321664	36.484954
1469.190235	226806.640341	36.489972
1470.545665	227241.561611	36.494989
1471.800559	227685.568759	36.500007
1473.706892	228138.309180	36.505024
1474.957251	228571.347645	36.510042
1476.567361	229020.381046	36.515060
1478.503691	229464.155228	36.520077
1479.502197	229917.509178	36.525095
1481.035148	230367.118912	36.530112
1482.603447	230821.931437	36.535130
1484.099445	231270.178760	36.540148
1485.419546	231697.247212	36.545165
1486.808251	232166.038817	36.550183
1488.504609	232634.171638	36.555200
1490.355562	233064.611227	36.560218
1492.220012	233513.795695	36.565236
1494.026765	233964.083322	36.570253
1495.418765	234403.442156	36.575271
1496.920717	234847.559541	36.580288
1498.892662	235274.810540	36.585306
1500.559146	235727.209503	36.590324
1501.968684	236160.829843	36.595341
1503.554353	236602.093504	36.600359
1504.860578	237056.079776	36.605376
1506.279669	237485.993490	36.610394
1507.822176	237941.391077	36.615412
1509.219027	238368.745151	36.620429
1510.702682	238799.819996	36.625447
1512.211329	239250.832114	36.630464
1514.070356	239694.548036	36.635482
1515.547608	240127.608446	36.640500
1517.005360	240561.892364	36.645517
1518.787450	241006.436941	36.650535
1520.196428	241441.010299	36.655552
1521.912508	241878.353557	36.660570
1523.190858	242306.066370	36.665588
1525.035967	242731.857583	36.670605
1526.316888	243190.867240	36.675623
1527.587505	243637.965893	36.680640
1529.565264	244062.239075	36.685658
1530.919264	244473.609955	36.690676
1532.530609	244863.397846	36.695693
1533.724087	245299.589397	36.700711
1535.240138	245704.889859	36.705728
1536.672518	246139.671722	36.710746
1537.925986	246565.821555	36.715764
1539.746596	246973.868028	36.720781
1541.432712	247387.424275	36.725799
1542.391806	247823.887309	36.730816
1544.482806	248261.586780	36.735834
1545.559143	248707.735618	36.740852
1547.067257	249136.692360	36.745869
1548.431218	249562.650524	36.750887
1549.706666	250002.290584	36.755904
1551.287201	250476.835261	36.760922
1552.519392	250927.965730	36.765940
1554.342265	251370.692510	36.770957
1555.470422	251846.329691	36.775975
1556.912460	252295.623506	36.780992
1559.119032	252760.947984	36.786010
1560.448140	253219.279464	36.791028
1561.850633	253693.984280	36.796045
1563.134027	254172.291039	36.801063
1564.715730	254648.237322	36.806080
1566.549044	255118.198148	36.811098
1567.159028	255615.415583	36.816116
1569.018692	256094.619552	36.821133
1571.068819	256578.593629	36.826151
1572.191903	257079.817349	36.831168
1573.989398	257557.813128	36.836186
1575.532986	258074.336987	36.841204
1576.798384	258584.175128	36.846221
1578.116845	259076.628875	36.851239
1579.938066	259563.512722	36.856256
1581.762130	260086.113272	36.861274
1583.167413	260583.709979	36.866292
1585.039657	261101.044297	36.871309
1586.625209	261622.160254	36.876327
1587.800138	262141.184699	36.881344
1589.791359	262639.269132	36.886362
1591.279095	263157.403588	36.891380
1593.117793	263677.207477	36.896397
1594.540205	264181.050455	36.901415
1595.986964	264707.371179	36.906432
1597.885868	265233.032833	36.911450
1599.494002	265735.371235	36.916468
1601.710615	266231.537627	36.921485
1603.611557	266752.828832	36.926503
1605.460088	267270.292475	36.931520
1607.405601	267771.710344	36.936538
1608.882807	268263.069248	36.941556
1610.485280	268756.007505	36.946573
1611.875972	269275.221738	36.951591
1613.152933	269797.934474	36.956608
1614.865225	270285.366175	36.961626
1616.329175	270796.945866	36.966644
1617.797862	271317.288250	36.971661
1619.650984	271813.560744	36.976679
1620.970064	272344.849833	36.981696
1622.811437	272862.232830	36.986714
1624.319162	273380.864092	36.991732
1625.608045	273883.222068	36.996749
1627.472075	274390.742792	37.001767
1628.761250	274936.309325	37.006784
1630.418058	275452.296275	37.011802
1632.625221	275966.464153	37.016820
1634.456349	276470.887740	37.021837
1636.403044	276995.079976	37.026855
1637.719108	277493.591654	37.031872
1639.092661	277978.985207	37.036890
1640.938864	278470.371035	37.041908
1642.297811	278974.689889	37.046925
1644.067363	279443.706878	37.051943
1645.662858	279932.082785	37.056960
1647.477428	280440.489262	37.061978
1648.948294	280935.234095	37.066996
1650.555063	281437.448989	37.072013
1652.749916	281931.919630	37.077031
1653.932892	282446.191757	37.082048
1655.786551	282942.697561	37.087066
1657.241696	283443.662364	37.092084
1658.746091	283960.646248	37.097101
1660.590897	284465.278092	37.102119
1661.895552	284964.307675	37.107136
1663.745723	285479.553661	37.112154
1665.357002	286012.008940	37.117172
1667.221864	286530.830949	37.122189
1668.783466	287044.519493	37.127207
1669.783572	287572.625357	37.132224
1671.441088	288102.170477	37.137242
1673.234426	288647.719472	37.142260
1674.682476	289191.977230	37.147277
1676.461335	289721.979328	37.152295
1678.078887	290265.798761	37.157312
1679.867775	290817.639895	37.162330
1681.473010	291361.050770	37.167348
1682.605503	291922.292458	37.172365
1684.727225	292480.447581	37.177383
1686.175341	293039.879915	37.182400
1687.683209	293587.996923	37.187418
1689.412377	294156.674547	37.192436
1691.012894	294738.401015	37.197453
1692.790195	295303.992102	37.202471
1694.625822	295885.394970	37.207488
1696.161993	296447.566138	37.212506
1697.971512	297035.901786	37.217524
1699.804856	297630.173969	37.222541
1701.305605	298210.299778	37.227559
1703.224698	298777.857230	37.232576
1705.195328	299358.382130	37.237594
1706.953930	299926.747490	37.242612
1708.715544	300520.584208	37.247629
1710.400678	301098.505333	37.252647
1712.024420	301676.052403	37.257664
1713.792438	302260.810920	37.262682
1715.826847	302823.044794	37.267700
1717.733370	303406.808660	37.272717
1719.686991	303985.710312	37.277735
1721.516884	304571.410091	37.282752
1723.707646	305134.468382	37.287770
1725.044497	305690.171972	37.292788
1726.804529	306283.034708	37.297805
1728.663429	306841.134190	37.302823
1730.264445	307414.637889	37.307840
1732.237894	308006.920828	37.312858
1734.224479	308572.912232	37.317876
1735.203039	309145.009018	37.322893
1737.324428	309726.817997	37.327911
1738.995846	310286.018595	37.332928
1741.012481	310850.212310	37.337946
1742.868286	311410.619387	37.342964
1744.977176	311995.335192	37.347981
1747.113851	312537.835187	37.352999
1749.031054	313083.592922	37.358016
1750.738930	313634.663610	37.363034
1752.546168	314194.094341	37.368052
1754.063762	314728.250407	37.373069
1755.932500	315259.500673	37.378087
1757.002613	315788.085627	37.383104
1758.993338	316316.438839	37.388122
1761.028517	316834.369487	37.393140
1762.297045	317387.644109	37.398157
1763.792389	317920.232203	37.403175
1765.295797	318466.095798	37.408192
1766.868236	319029.973018	37.413210
1768.463462	319561.821506	37.418228
1769.581739	320122.641648	37.423245
1771.685552	320692.055156	37.428263
1773.030596	321286.473657	37.433280
1774.962115	321863.041177	37.438298
1776.821024	322423.034873	37.443316
1778.523301	323024.996834	37.448333
1780.440232	323582.508285	37.453351
1782.077130	324172.333514	37.458368
1783.721825	324767.738171	37.463386
1785.975697	325358.923566	37.468404
1787.190746	325950.858877	37.473421
1788.748004	326542.275210	37.478439
1790.345398	327163.766608	37.483456
1792.005500	327756.220929	37.488474
1793.836250	328384.136048	37.493492
1795.574938	329018.204138	37.498509
1797.252833	329635.290380	37.503527
1799.083270	330250.948754	37.508544
1800.983161	330878.141092	37.513562
1802.861046	331523.229114	37.518580
1804.615117	332167.238776	37.523597
1806.569739	332791.481992	37.528615
1808.729382	333437.619323	37.533632
1810.222282	334075.786220	37.538650
1812.415007	334708.778491	37.543668
1813.682544	335363.672481	37.548685
1816.054904	335989.461586	37.553703
1817.449539	336628.351690	37.558720
1819.461782	337284.470826	37.563738
1821.831774	337924.403310	37.568756
1823.317276	338571.150324	37.573773
1825.432525	339218.648674	37.578791
1827.483414	339859.498979	37.583808
1829.289267	340484.516795	37.588826
1831.054935	341143.446445	37.593844
1832.649865	341804.984935	37.598861
1834.771016	342457.620106	37.603879
1836.753372	343092.577947	37.608896
1838.784127	343747.774991	37.613914
1840.729852	344375.006324	37.618932
1842.480907	345019.800649	37.623949
1844.445284	345677.952731	37.628967
1846.281855	346309.212989	37.633984
1848.359845	346943.369348	37.639002
1850.043316	347605.399386	37.644020
1851.474913	348247.639893	37.649037
1853.616709	348896.074078	37.654055
1855.194364	349549.972782	37.659072
1857.363188	350188.562724	37.664090
1859.125182	350853.376380	37.669108
1860.220717	351524.025827	37.674125
1861.888196	352161.376681	37.679143
1863.993895	352833.159784	37.684160
1865.749269	353494.915854	37.689178
1867.349812	354155.977072	37.694196
1869.530792	354844.440719	37.699213
1871.635455	355509.788571	37.704231
1873.257775	356172.998135	37.709248
1874.749372	356805.540376	37.714266
1876.910445	357445.245469	37.719284
1878.369612	358116.673394	37.724301
1880.564025	358756.784613	37.729319
1882.147805	359401.630208	37.734336
1884.066590	360059.731596	37.739354
1886.075257	360726.358401	37.744372
1887.864942	361395.547799	37.749389
1889.420985	362039.316581	37.754407
1891.595861	362715.042928	37.759424
1893.205176	363395.874773	37.764442
1894.794501	364052.570704	37.769460
1896.640678	364747.218332	37.774477
1898.602282	365443.864335	37.779495
1900.498685	366118.614871	37.784512
1902.084670	366796.525355	37.789530
1904.067501	367506.373747	37.794548
1906.262019	368215.539953	37.799565
1908.280661	368904.047383	37.804583
1910.059676	369603.007810	37.809600
1912.064404	370321.399744	37.814618
1914.097507	371024.223744	37.819636
1915.959682	371717.296875	37.824653
1917.811401	372438.108415	37.829671
1919.884288	373160.061516	37.834688
1921.642748	373874.544405	37.839706
1923.959129	374566.981542	37.844724
1925.733144	375275.042580	37.849741
1927.607675	375989.743497	37.854759
1929.919057	376734.716702	37.859776
1931.783410	377440.462624	37.864794
1933.931654	378166.132250	37.869812
1935.858326	378888.069994	37.874829
1938.160195	379585.230035	37.879847
1940.092347	380317.433368	37.884864
1942.011610	381062.962128	37.889882
1943.812493	381772.738542	37.894900
1945.634179	382487.974028	37.899917
1947.741475	383205.606925	37.904935
1949.851382	383943.332112	37.909952
1952.111775	384687.634172	37.914970
1954.423595	385382.669992	37.919988
1956.536999	386104.701923	37.925005
1958.309381	386821.576462	37.930023
1960.533712	387539.045242	37.935040
1962.541746	388242.234351	37.940058
1964.530302	388964.983883	37.945076
1966.310392	389686.813437	37.950093
1968.206480	390395.297734	37.955111
1970.306853	391129.286633	37.960128
1972.068337	391845.239223	37.965146
1974.319618	392571.133318	37.970164
1976.032305	393292.587087	37.975181
1978.295678	394014.262749	37.980199
1980.291015	394739.996087	37.985216
1982.314027	395464.947219	37.990234
1984.369149	396176.669906	37.995252
1985.995202	396893.439907	38.000269
1987.993111	397631.117983	38.005287
1990.064133	398350.922708	38.010304
1992.260168	399071.551140	38.015322
1994.151262	399779.869750	38.020340
1996.175797	400516.939556	38.025357
1997.828363	401268.573635	38.030375
2000.052219	401983.322577	38.035392
2001.873870	402714.389542	38.040410
2003.798826	403447.752314	38.045428
2005.693190	404169.140777	38.050445
2007.498252	404894.453393	38.055463
2009.787662	405586.144086	38.060480
2011.641016	406293.042138	38.065498
2013.432101	407013.082995	38.070516
2015.841193	407717.243725	38.075533
2017.298425	408439.051133	38.080551
2019.526730	409160.940598	38.085568
2021.349551	409880.319192	38.090586
2023.112573	410592.873819	38.095604
2025.110800	411326.119446	38.100621
2026.867311	412073.799685	38.105639
2028.916240	412809.479465	38.110656
2030.829278	413540.779152	38.115674
2033.201739	414276.416022	38.120692
2035.530982	415034.710323	38.125709
2037.337916	415801.529143	38.130727
2039.507796	416526.625201	38.135744
2041.477514	417283.824994	38.140762
2043.588060	418030.215466	38.145780
2045.398492	418802.695132	38.150797
2047.282038	419566.123652	38.155815
2049.554231	420308.242949	38.160832
2051.437755	421074.792256	38.165850
2053.190600	421852.229227	38.170868
2055.243840	422643.950883	38.175885
2056.973299	423426.483874	38.180903
2059.593177	424196.387570	38.185920
2061.281086	425005.895860	38.190938
2063.515672	425786.018136	38.195956
2065.589071	426595.892038	38.200973
2067.403922	427392.059586	38.205991
2069.648061	428175.876947	38.211008
2071.492646	429007.481650	38.216026
2073.849375	429826.973859	38.221044
2075.887021	430633.580413	38.226061
2077.863035	431428.930731	38.231079
2080.222808	432255.781834	38.236096
2082.205768	433060.897987	38.241114
2084.222292	433875.751346	38.246132
2086.216776	434702.982205	38.251149
2088.450720	435538.294014	38.256167
2091.302632	436336.068051	38.261184
2093.326219	437160.068754	38.266202
2095.352135	437979.383264	38.271220
2097.641227	438793.310972	38.276237
2099.712444	439625.313380	38.281255
2101.897781	440443.906091	38.286272
2104.050572	441258.830982	38.291290
2106.144051	442068.979431	38.296308
2108.169199	442890.596710	38.301325
2110.228595	443734.493026	38.306343
2112.654628	444550.872409	38.311360
2114.655745	445365.470304	38.316378
2116.688591	446215.854102	38.321396
2118.980510	447032.163771	38.326413
2120.858296	447832.018539	38.331431
2123.031173	448667.410080	38.336448
2125.294152	449509.179130	38.341466
2127.404029	450335.259133	38.346484
2129.851855	451144.002692	38.351501
2131.722438	451985.233537	38.356519
2133.911511	452818.994015	38.361536
2136.046035	453660.367860	38.366554
2138.171409	454469.391958	38.371572
2140.262692	455300.895704	38.376589
2142.533296	456133.702235	38.381607
2144.534092	456968.289867	38.386624
2146.936141	457780.932612	38.391642
2149.066984	458573.968684	38.396660
2151.170440	459377.141932	38.401677
2153.086397	460176.876396	38.406695
2155.267552	460964.350902	38.411712
2156.901998	461776.658211	38.416730
2158.992327	462581.678826	38.421748
2161.275485	463382.591173	38.426765
2163.082909	464186.785266	38.431783
2165.442534	465024.521799	38.436800
2167.676309	465865.226072	38.441818
2169.636169	466689.310490	38.446836
2172.126215	467502.557929	38.451853
2173.839261	468336.924816	38.456871
2175.861254	469184.547374	38.461888
2177.677623	470012.205044	38.466906
2179.749484	470868.135014	38.471924
2182.112070	471714.479091	38.476941
2184.332723	472579.656943	38.481959
2186.400579	473432.946949	38.486976
2188.596790	474310.480249	38.491994
2190.742472	475178.685133	38.497012
2193.463399	476048.927691	38.502029
2195.002984	476941.098170	38.507047
2197.436419	477806.002370	38.512064
2199.995554	478667.057279	38.517082
2201.947402	479558.226568	38.522100
2204.583409	480433.986562	38.527117
2206.616925	481333.542252	38.532135
2208.728479	482209.758797	38.537152
2211.021678	483096.407706	38.542170
2213.195700	484003.081157	38.547188
2215.478191	484880.151063	38.552205
2217.625823	485790.577080	38.557223
2219.997976	486721.066016	38.562240
2222.386996	487618.635753	38.567258
2224.159932	488509.900674	38.572276
2226.415724	489442.286348	38.577293
2228.183766	490357.792240	38.582311
2230.634160	491268.796939	38.587328
2233.085171	492208.676766	38.592346
2235.273016	493127.350839	38.597364
2237.925036	494037.875122	38.602381
2239.870878	494977.184058	38.607399
2241.979035	495899.055243	38.612416
2244.673460	496815.935972	38.617434
2246.379772	497761.894212	38.622452
2248.767883	498706.981179	38.627469
2250.621448	499645.696073	38.632487
2252.887827	500580.355637	38.637504
2255.245355	501532.706052	38.642522
2257.154070	502470.295955	38.647540
2259.746705	503421.339935	38.652557
2261.623733	504408.915270	38.657575
2263.881102	505365.148903	38.662592
2266.225577	506317.328522	38.667610
2268.355025	507283.407287	38.672628
2270.479102	508255.985519	38.677645
2272.763826	509232.462792	38.682663
2275.110993	510187.542730	38.687680
2277.728166	511160.521178	38.692698
2279.695600	512140.908641	38.697716
2282.457372	513108.905420	38.702733
2284.488109	514086.945135	38.707751
2286.755481	515058.282512	38.712768
2289.150870	516042.492867	38.717786
2291.645853	517019.519042	38.722804
2293.710768	517983.049053	38.727821
2296.176926	518958.951295	38.732839
2298.601243	519916.759541	38.737856
2300.932088	520847.314866	38.742874
2303.064189	521786.261255	38.747892
2305.909741	522724.730569	38.752909
2308.246267	523647.055004	38.757927
2310.314220	524583.473275	38.762944
2312.995516	525537.262487	38.767962
2315.281103	526475.694497	38.772980
2317.771421	527388.499005	38.777997
2319.906258	528333.791008	38.783015
2322.013511	529279.783508	38.788032
2324.476924	530238.901301	38.793050
2326.487429	531173.056862	38.798068
2329.019541	532106.413173	38.803085
2330.695381	533093.269931	38.808103
2332.778615	534041.027644	38.813120
2335.327548	535021.066632	38.818138
2337.101143	535995.077115	38.823156
2339.077038	536992.041980	38.828173
2341.402031	538007.150700	38.833191
2343.600196	539016.220340	38.838208
2345.826367	540002.166893	38.843226
2348.016453	541018.998231	38.848244
2350.452982	542042.811265	38.853261
2352.518338	543071.341355	38.858279
2354.930787	544115.285104	38.863296
2357.487435	545153.997004	38.868314
2359.364404	546186.808920	38.873332
2361.771887	547226.448778	38.878349
2364.449529	548283.116964	38.883367
2366.364108	549361.354834	38.888384
2369.015085	550416.205837	38.893402
2370.966218	551479.136884	38.898420
2373.346920	552559.562710	38.903437
2376.250487	553654.949757	38.908455
2378.985497	554720.315898	38.913472
2381.254795	555775.019050	38.918490
2383.215411	556874.223375	38.923508
2385.815266	557971.524148	38.928525
2388.395335	559051.652405	38.933543
2390.755225	560132.131959	38.938560
2392.928397	561228.332088	38.943578
2395.743571	562320.618204	38.948596
2398.375361	563408.624596	38.953613
2401.018650	564500.005554	38.958631
2403.422158	565598.518273	38.963648
2406.150197	566671.521805	38.968666
2408.557399	567767.189870	38.973684
2411.033269	568875.710197	38.978701
2413.807204	569965.357391	38.983719
2416.121857	571047.457118	38.988736
2418.537865	572110.522243	38.993754
2420.978360	573218.925839	38.998772
2423.546271	574305.226692	39.003789
2426.030397	575385.224905	39.008807
2428.179548	576466.190050	39.013824
2430.731372	577564.811041	39.018842
2433.164263	578673.642191	39.023860
2435.709758	579744.475657	39.028877
2438.061207	580831.704837	39.033895
2440.180215	581908.041743	39.038912
2442.866503	583023.266734	39.043930
2445.186610	584128.269783	39.048948
2447.842338	585211.803959	39.053965
2449.868741	586299.909551	39.058983
2452.139603	587421.323036	39.064000
2454.869639	588534.936622	39.069018
2456.954764	589625.392748	39.074036
2459.059359	590692.236907	39.079053
2461.912415	591764.727793	39.084071
2464.459318	592843.939540	39.089088
2467.102360	593918.227027	39.094106
2469.233834	594977.168124	39.099124
2471.496726	596051.526212	39.104141
2473.979166	597143.586910	39.109159
2476.038161	598240.676183	39.114176
2478.754160	599314.412099	39.119194
2481.392424	600397.078296	39.124212
2483.171248	601510.136248	39.129229
2485.719999	602625.464794	39.134247
2488.014135	603726.807638	39.139264
2490.932218	604827.291816	39.144282
2492.940618	605961.213466	39.149300
2495.675518	607107.117742	39.154317
2498.105609	608236.389646	39.159335
2500.157573	609369.916230	39.164352
2502.951178	610520.872957	39.169370
2505.316901	611665.178072	39.174388
2507.434765	612801.552678	39.179405
2509.632908	613979.072759	39.184423
2512.049469	615159.584522	39.189440
2514.808676	616341.565531	39.194458
2517.451469	617527.591141	39.199476
2519.657682	618718.612500	39.204493
2522.050771	619905.874464	39.209511
2524.326869	621100.777034	39.214528
2526.986262	622299.235507	39.219546
2529.311071	623533.357131	39.224564
2532.086695	624736.926887	39.229581
2534.813672	625954.063979	39.234599
2537.088778	627176.784884	39.239616
2539.869546	628403.130714	39.244634
2542.264238	629638.991723	39.249652
2544.602655	630884.409642	39.254669
2547.441709	632123.456136	39.259687
2549.873080	633373.961149	39.264704
2552.460226	634607.165391	39.269722
2554.933356	635871.498764	39.274740
2557.570783	637123.122456	39.279757
2560.603874	638356.960829	39.284775
2563.347554	639605.873369	39.289792
2566.007961	640860.388342	39.294810
2568.011682	642135.067961	39.299828
2570.660875	643404.644140	39.304845
2573.794453	644646.945758	39.309863
2575.978031	645917.584540	39.314880
2578.639070	647191.527307	39.319898
2581.529731	648454.102396	39.324916
2583.963963	649723.775183	39.329933
2586.771089	650968.299655	39.334951
2589.319221	652254.784442	39.339968
2592.176856	653535.570462	39.344986
2594.723845	654785.096394	39.350004
2597.207784	656046.484547	39.355021
2600.094788	657323.738438	39.360039
2602.696121	658591.160137	39.365056
2605.084251	659854.767885	39.370074
2608.057260	661130.816288	39.375092
2610.410628	662414.219943	39.380109
2613.046246	663682.719925	39.385127
2615.695162	664972.160187	39.390144
2618.352144	666222.252777	39.395162
2621.088779	667480.730678	39.400180
2623.620443	668758.535231	39.405197
2626.509726	670037.404003	39.410215
2629.118617	671298.038345	39.415232
2631.825074	672517.400790	39.420250
2634.616858	673742.560842	39.425268
2637.256159	674971.665107	39.430285
2639.885218	676191.262342	39.435303
2642.234875	677412.139267	39.440320
2644.811654	678646.788489	39.445338
2647.500918	679864.405590	39.450356
2649.628652	681107.699703	39.455373
2652.229379	682358.997901	39.460391
2655.099414	683599.896663	39.465408
2657.449233	684832.367843	39.470426
2659.976665	686098.073361	39.475444
2662.176377	687362.515407	39.480461
2665.096187	688621.250633	39.485479
2667.623893	689921.980131	39.490496
2670.635692	691194.394193	39.495514
2673.018006	692470.852431	39.500532
2675.557410	693752.513281	39.505549
2678.106376	695053.491021	39.510567
2680.600089	696359.498045	39.515584
2683.082378	697669.284054	39.520602
2686.160601	698974.760890	39.525620
2688.778096	700313.150103	39.530637
2691.330378	701620.107839	39.535655
2694.145089	702948.592826	39.540672
2697.035237	704280.581632	39.545690
2699.940869	705617.915654	39.550708
2702.220962	706946.474912	39.555725
2704.909393	708299.884067	39.560743
2707.485456	709665.088408	39.565760
2709.878292	711008.064651	39.570778
2712.779915	712355.550743	39.575796
2714.990114	713735.470851	39.580813
2718.098946	715112.940105	39.585831
2720.654462	716503.592743	39.590848
2723.517617	717872.981498	39.595866
2726.357432	719262.440331	39.600884
2729.111197	720650.397326	39.605901
2732.095013	722018.744559	39.610919
2734.402171	723428.970307	39.615936
2737.814533	724823.939597	39.620954
2740.569243	726220.463655	39.625972
2742.997833	727622.935373	39.630989
2746.072573	729008.948918	39.636007
2748.621523	730407.960213	39.641024
2751.624177	731805.471699	39.646042
2754.521043	733220.347743	39.651060
2757.133635	734640.654977	39.656077
2759.986911	736046.055981	39.661095
2762.791838	737444.702754	39.666112
2765.919087	738841.177305	39.671130
2768.271835	740273.962120	39.676148
2770.752223	741676.119565	39.681165
2773.381267	743096.754853	39.686183
2775.938265	744545.710404	39.691200
2778.919574	745984.466229	39.696218
2781.550507	747378.536792	39.701236
2783.806668	748836.714517	39.706253
2786.798401	750281.091287	39.711271
2789.754903	751734.521523	39.716288
2792.180635	753162.833633	39.721306
2795.025127	754609.535216	39.726324
2797.580244	756070.249173	39.731341
2800.548667	757532.341596	39.736359
2803.642113	759007.429417	39.741376
2806.429542	760453.434390	39.746394
2809.346538	761900.029619	39.751412
2811.816511	763329.002209	39.756429
2814.508075	764755.897305	39.761447
2817.374394	766169.113349	39.766464
2820.101022	767604.908014	39.771482
2822.975583	769011.046389	39.776500
2825.525069	770453.404843	39.781517
2828.225622	771870.930645	39.786535
2830.636505	773336.396364	39.791552
2833.191793	774777.225798	39.796570
2835.826232	776225.768325	39.801588
2838.175867	777683.699224	39.806605
2840.989880	779158.450891	39.811623
2843.391264	780652.562323	39.816640
2846.279016	782156.496916	39.821658
2849.070150	783641.731997	39.826676
2851.345248	785151.231047	39.831693
2854.427260	786668.375146	39.836711
2857.089019	788215.577962	39.841728
2859.857231	789744.089797	39.846746
2863.010789	791290.986803	39.851764
2865.386169	792843.949083	39.856781
2868.605334	794392.315669	39.861799
2871.817765	795932.358053	39.866816
2874.523561	797492.229031	39.871834
2877.519429	799071.733930	39.876852
2880.029683	800647.779453	39.881869
2883.414434	802209.031394	39.886887
2886.453811	803794.897774	39.891904
2889.644165	805363.007021	39.896922
2892.825926	806954.337581	39.901940
2895.744154	808533.899533	39.906957
2898.541790	810108.472108	39.911975
2901.583813	811691.781582	39.916992
2903.867117	813299.574950	39.922010
2907.217675	814907.397200	39.927028
2909.767664	816523.858291	39.932045
2912.922060	818115.658685	39.937063
2915.880483	819735.820862	39.942080
2918.664356	821346.833081	39.947098
2921.801373	822950.907130	39.952116
2924.651688	824564.105250	39.957133
2927.542700	826194.510776	39.962151
2930.567120	827841.947898	39.967168
2933.264707	829462.505471	39.972186
2936.458936	831080.727888	39.977204
2939.270457	832720.343660	39.982221
2942.416862	834357.054964	39.987239
2945.314009	836006.348294	39.992256
2947.878336	837650.114042	39.997274
2951.336475	839292.338973	40.002292
2954.091034	840922.239101	40.007309
2957.362194	842554.265477	40.012327
2960.420490	844202.980848	40.017344
2963.206636	845854.084347	40.022362
2966.637741	847498.039023	40.027380
2969.719524	849157.855028	40.032397
2972.387382	850795.435956	40.037415
2975.692613	852423.934162	40.042432
2978.635064	854081.495890	40.047450
2981.621495	855716.566893	40.052468
2984.848955	857341.653439	40.057485
2987.812526	858986.929958	40.062503
2990.642687	860642.461011	40.067520
2993.580974	862268.137660	40.072538
2996.903945	863915.233819	40.077556
2999.768844	865589.007334	40.082573
3002.783318	867230.893801	40.087591
3005.797328	868865.164944	40.092608
3008.416895	870490.243567	40.097626
3011.631626	872093.093010	40.102644
3014.409850	873690.841748	40.107661
3017.140807	875291.268037	40.112679
3020.206090	876896.724370	40.117696
3023.280087	878530.378238	40.122714
3026.458560	880126.427925	40.127732
3029.460938	881734.159710	40.132749
3032.190520	883335.310653	40.137767
3035.254173	884938.191360	40.142784
3037.857148	886570.364691	40.147802
3040.572552	888207.469954	40.152820
3043.578468	889839.044903	40.157837
3046.276309	891494.050565	40.162855
3049.022035	893164.204723	40.167872
3051.852827	894826.817427	40.172890
3054.867969	896486.506039	40.177908
3057.654284	898190.096848	40.182925
3060.587275	899896.333654	40.187943
3063.777217	901594.499294	40.192960
3066.479076	903318.337426	40.197978
3069.746616	905029.710892	40.202996
3072.850535	906750.215348	40.208013
3075.881901	908487.812587	40.213031
3079.123209	910239.359704	40.218048
3082.028951	911984.543325	40.223066
3085.335617	913716.997036	40.228084
3088.262505	915464.538889	40.233101
3091.062423	917244.308866	40.238119
3094.807232	918995.107157	40.243136
3097.591924	920769.602188	40.248154
3100.880696	922552.649986	40.253172
3104.438571	924333.243964	40.258189
3107.337552	926094.942754	40.263207
3110.438379	927876.744204	40.268224
3112.976744	929664.181614	40.273242
3116.536226	931445.870499	40.278260
3119.436613	933252.457585	40.283277
3122.583983	935049.483734	40.288295
3125.780479	936860.346599	40.293312
3128.403666	938666.854372	40.298330
3131.497282	940480.699431	40.303348
3134.562807	942314.481181	40.308365
3137.412754	944142.014089	40.313383
3140.583654	945980.319392	40.318400
3143.867188	947827.315804	40.323418
3146.856758	949654.124056	40.328436
3149.995562	951518.729305	40.333453
3153.548562	953373.236884	40.338471
3156.975468	955216.980968	40.343488
3159.990687	957087.468914	40.348506
3163.230125	958982.347915	40.353524
3166.510989	960900.162881	40.358541
3169.627786	962808.765414	40.363559
3172.941753	964696.574081	40.368576
3175.803348	966603.081704	40.373594
3178.691813	968508.367143	40.378612
3181.812088	970435.044345	40.383629
3184.649603	972352.729395	40.388647
3188.216185	974287.310267	40.393664
3191.381805	976225.107455	40.398682
3194.598058	978134.164643	40.403700
3197.725263	980071.250876	40.408717
3200.806326	982020.158126	40.413735
3204.219155	983938.642696	40.418752
3207.133440	985884.797139	40.423770
3210.216451	987824.030979	40.428788
3213.935552	989773.201514	40.433805
3216.712394	991686.264465	40.438823
3220.061571	993573.117272	40.443840
3223.315297	995466.453999	40.448858
3226.434451	997358.501240	40.453876
3229.561197	999253.509641	40.458893
3232.764243	1001142.725786	40.463911
3235.761911	1003016.203843	40.468928
3238.736589	1004928.555688	40.473946
3241.897955	1006856.621836	40.478964
3244.821248	1008761.185803	40.483981
3248.122344	1010674.737486	40.488999
3251.186021	1012592.426513	40.494016
3254.285208	1014551.495128	40.499034
3257.594020	1016512.074122	40.504052
3260.851084	1018455.522618	40.509069
3263.768086	1020412.772050	40.514087
3266.889715	1022371.626508	40.519104
3270.019629	1024352.904897	40.524122
3273.220420	1026335.017252	40.529140
3276.566859	1028346.936885	40.534157
3279.128432	1030363.574113	40.539175
3282.522967	1032363.800675	40.544192
3285.406435	1034382.601859	40.549210
3288.638844	1036425.314602	40.554228
3292.162897	1038486.326961	40.559245
3295.404160	1040539.391375	40.564263
3298.612786	1042587.365811	40.569280
3301.438050	1044667.404350	40.574298
3304.852911	1046741.172787	40.579316
3308.334195	1048808.570634	40.584333
3311.410626	1050894.991050	40.589351
3314.512940	1053000.629171	40.594368
3317.991433	1055122.904083	40.599386
3321.310091	1057230.932153	40.604404
3324.957665	1059321.092911	40.609421
3328.043667	1061453.391330	40.614439
3331.698044	1063560.958942	40.619456
3335.280611	1065687.309479	40.624474
3338.685227	1067828.791848	40.629492
3342.142402	1069960.510994	40.634509
3344.993490	1072075.012379	40.639527
3348.779433	1074198.125984	40.644544
3352.116512	1076348.172504	40.649562
3355.554739	1078494.962665	40.654580
3359.225873	1080613.783216	40.659597
3362.243498	1082764.992247	40.664615
3365.633515	1084900.657836	40.669632
3369.068391	1087044.751275	40.674650
3371.858776	1089214.002904	40.679668
3375.610548	1091382.229845	40.684685
3378.956848	1093533.997202	40.689703
3382.181302	1095683.880410	40.694720
3385.878941	1097858.783770	40.699738
3389.003531	1100006.870234	40.704756
3392.725526	1102151.430274	40.709773
3396.189291	1104327.105070	40.714791
3399.806357	1106507.877933	40.719808
3403.386315	1108660.350708	40.724826
3406.689130	1110811.627275	40.729844
3409.864273	1112967.201586	40.734861
3413.242017	1115137.569508	40.739879
3416.914139	1117295.792868	40.744896
3419.799220	1119468.385968	40.749914
3423.562380	1121647.076847	40.754932
3427.322261	1123784.336350	40.759949
3430.585374	1125946.448950	40.764967
3434.009283	1128117.336124	40.769984
3437.295687	1130310.975764	40.775002
3440.187799	1132447.867862	40.780007
3443.802157	1134523.672931	40.785012
3446.732331	1136581.211017	40.790016
3449.726885	1138569.117059	40.795021
3453.001724	1140479.841055	40.800026
3455.630629	1142326.993719	40.805031
3458.844550	1144082.273291	40.810036
3461.522510	1145786.055885	40.815040
3464.058791	1147409.515297	40.820045
3466.882989	1148944.222069	40.825050
3469.422975	1150408.343730	40.830055
3472.263646	1151803.262746	40.835060
3474.436069	1153116.602271	40.840064
3477.226892	1154350.293439	40.845069
3479.525057	1155523.594732	40.850074
3481.604227	1156617.296330	40.855079
3483.972719	1157653.781306	40.860084
3485.636870	1158613.576443	40.865088
3487.932597	1159509.741289	40.870093
3489.619862	1160347.333995	40.875098
3491.198730	1161144.921583	40.880103
3493.493789	1161872.615442	40.885108
3494.919071	1162521.539310	40.890112
3496.510980	1163122.638697	40.895117
3497.744995	1163694.345277	40.900122
3499.016480	1164212.891847	40.905127
3500.525595	1164669.192977	40.910132
3501.783253	1165123.417752	40.915136
3503.294042	1165484.721592	40.920141
3503.896374	1165813.001636	40.925146
3505.153647	1166100.168542	40.930151
3506.066713	1166373.117416	40.935156
3507.313781	1166618.896915	40.940160
3508.149316	1166811.573168	40.945165
3509.118107	1166987.697057	40.950170
3510.034973	1167107.173722	40.955175
3510.689767	1167202.048506	40.960180
3511.102647	1167302.248556	40.965184
3511.910092	1167353.476283	40.970189
3512.616580	1167388.670150	40.975194
3513.126710	1167377.162376	40.980199
3514.008103	1167351.337170	40.985204
3514.367966	1167339.665236	40.990208
3514.950705	1167265.549273	40.995213
3515.784921	1167195.167460	41.000218
3515.941406	1167113.755151	41.005223
3516.307783	1166988.591183	41.010228
3516.838101	1166874.916607	41.015232
3517.634946	1166725.503608	41.020237
3517.930588	1166578.718403	41.025242
3518.075590	1166414.673343	41.030247
3518.642450	1166219.485333	41.035252
3518.849028	1166011.506011	41.040256
3519.236241	1165800.183261	41.045261
3519.608525	1165582.715559	41.050266
3519.751010	1165361.026494	41.055271
3520.288939	1165125.661753	41.060276
3520.244985	1164873.285542	41.065280
3520.624007	1164594.283687	41.070285
3521.048770	1164317.243250	41.075290
3521.212200	1164044.860337	41.080295
3521.490018	1163766.208933	41.085300
3521.537255	1163485.502075	41.090304
3521.627246	1163161.592268	41.095309
3522.150609	1162856.111839	41.100314
3522.254725	1162562.778523	41.105319
3522.672314	1162233.843487	41.110324
3522.341879	1161900.001937	41.115328
3522.405546	1161544.713371	41.120333
3522.671523	1161222.545098	41.125338
3522.620292	1160895.871894	41.130343
3522.920515	1160542.083442	41.135348
3523.173712	1160184.686299	41.140352
3523.205445	1159827.112192	41.145357
3523.262462	1159466.862029	41.150362
3523.114311	1159100.379891	41.155367
3523.542912	1158749.853692	41.160372
3523.453462	1158397.403366	41.165376
3523.658880	1158021.519447	41.170381
3523.658325	1157632.778646	41.175386
3523.599992	1157258.680750	41.180391
3523.677759	1156882.357977	41.185396
3523.471570	1156503.784431	41.190400
3523.956887	1156108.512114	41.195405
3524.037552	1155727.470047	41.200410
3523.996953	1155330.428045	41.205415
3523.979117	1154927.011687	41.210420
3524.094574	1154546.540791	41.215424
3524.043414	1154165.501924	41.220429
3524.152640	1153750.995054	41.225434
3524.131776	1153353.800629	41.230439
3524.487316	1152927.639269	41.235444
3524.281825	1152543.762926	41.240448
3524.111658	1152141.673013	41.245453
3524.512827	1151721.561176	41.250458
3524.446665	1151320.433092	41.255463
3524.684105	1150900.282755	41.260468
3524.504811	1150480.641146	41.265472
3524.602671	1150055.900120	41.270477
3524.487096	1149647.264375	41.275482
3524.095309	1149240.347749	41.280487
3524.549880	1148805.025991	41.285492
3524.421791	1148393.452784	41.290496
3524.266307	1147967.163986	41.295501
3524.443552	1147542.112728	41.300506
3524.417599	1147126.159273	41.305511
3524.564996	1146719.528112	41.310516
3524.006458	1146308.337141	41.315520
3524.488709	1145882.722938	41.320525
3524.534324	1145451.173562	41.325530
3524.608150	1145018.067274	41.330535
3524.593919	1144602.007958	41.335540
3524.371358	1144177.984546	41.340544
3524.267126	1143744.329094	41.345549
3524.671280	1143303.346138	41.350554
3524.459481	1142900.938055	41.355559
3524.543130	1142451.969338	41.360564
3524.158349	1142011.577833	41.365568
3524.421322	1141586.412917	41.370573
3524.725828	1141167.943752	41.375578
3524.142421	1140746.076797	41.380583
3524.238590	1140299.390649	41.385588
3524.480132	1139862.892841	41.390592
3524.538032	1139433.982490	41.395597
3524.528451	1138990.620369	41.400602
3524.105841	1138569.312975	41.405607
3524.218622	1138142.567425	41.410612
3524.056663	1137710.420913	41.415616
3523.959407	1137262.941083	41.420621
3524.197235	1136834.360551	41.425626
3524.065816	1136423.280425	41.430631
3523.995756	1135975.782556	41.435636
3524.019183	1135538.964790	41.440640
3524.011754	1135121.114528	41.445645
3524.245925	1134690.556718	41.450650
3524.094925	1134265.347843	41.455655
3524.104365	1133811.479080	41.460660
3523.972987	1133375.173999	41.465664
3524.240951	1132946.369783	41.470669
3524.219595	1132518.243909	41.475674
3524.103389	1132084.776628	41.480679
3524.337220	1131636.102832	41.485684
3524.114618	1131182.428095	41.490688
3524.053179	1130752.930953	41.495693
3524.013269	1130318.926974	41.500698
3523.651180	1129867.730236	41.505703
3523.607329	1129434.795866	41.510708
3523.700471	1129028.336835	41.515712
3523.791040	1128591.127346	41.520717
3523.789038	1128149.046313	41.525722
3523.381181	1127720.788417	41.530727
3523.595740	1127284.973347	41.535732
3523.434922	1126853.085193	41.540736
3523.530462	1126419.787784	41.545741
3523.691084	1125994.437453	41.550746
3523.226235	1125565.920711	41.555751
3523.269413	1125130.243309	41.560756
3523.382898	1124711.270025	41.565760
3523.177908	1124293.363347	41.570765
3523.576861	1123848.480188	41.575770
3523.603363	1123417.806214	41.580775
3523.391297	1122982.185985	41.585780
3522.926611	1122548.857023	41.590784
3523.233278	1122121.555418	41.595789
3523.469676	1121693.183693	41.600794
3523.286805	1121257.132352	41.605799
3523.277453	1120825.874456	41.610804
3523.282806	1120398.484795	41.615808
3523.122393	1119966.325195	41.620813
3522.862940	1119536.814551	41.625818
3523.238959	1119111.642807	41.630823
3523.509405	1118677.116778	41.635828
3522.875699	1118254.425382	41.640832
3522.944987	1117817.766321	41.645837
3522.864596	1117376.807458	41.650842
3522.637225	1116946.416561	41.655847
3522.881198	1116520.298340	41.660852
3522.824108	1116116.598536	41.665856
3522.598819	1115689.919614	41.670861
3522.641639	1115244.665496	41.675866
3522.705820	1114837.321606	41.680871
3522.498120	1114418.643658	41.685876
3522.454044	1113986.077699	41.690880
3522.430570	1113547.464788	41.695885
3522.767014	1113124.399701	41.700890
3522.257565	1112715.463078	41.705895
3522.442408	1112297.222726	41.710900
3522.495704	1111880.879590	41.715904
3522.336098	1111452.421774	41.720909
3522.672232	1111021.653463	41.725914
3522.455576	1110600.866241	41.730919
3522.540288	1110183.336700	41.735924
3522.203169	1109747.328182	41.740928
3522.387805	1109319.598088	41.745933
3522.207014	1108912.131392	41.750938
3522.079258	1108491.641752	41.755943
3522.382699	1108053.863008	41.760948
3522.451191	1107637.379669	41.765952
3522.121269	1107226.754516	41.770957
3522.371827	1106793.274440	41.775962
3521.898061	1106381.940075	41.780967
3522.071058	1105965.310197	41.785972
3522.223346	1105535.278970	41.790976
3522.197333	1105096.932034	41.795981
3522.538070	1104672.914636	41.800986
3522.238012	1104268.364237	41.805991
3522.223665	1103829.339064	41.810996
3521.607500	1103400.410670	41.816000
3521.639363	1102992.365407	41.821005
3521.452921	1102574.194748	41.826010
3521.346589	1102168.977101	41.831015
3521.761917	1101754.180183	41.836020
3521.251384	1101347.916030	41.841024
3521.269783	1100918.112218	41.846029
3521.579792	1100509.929078	41.851034
3521.390186	1100107.343024	41.856039
3521.461819	1099705.066430	41.861044
3521.638075	1099294.614219	41.866048
3520.982821	1098868.392174	41.871053
3521.435940	1098441.762681	41.876058
3521.104230	1098049.567552	41.881063
3521.405863	1097655.709143	41.886068
3521.316754	1097248.588997	41.891072
3521.060082	1096817.547710	41.896077
3520.876086	1096407.127004	41.901082
3520.569713	1096017.076647	41.906087
3521.228054	1095616.791455	41.911092
3520.968167	1095201.411445	41.916096
3520.764567	1094798.145268	41.921101
3520.731240	1094382.665147	41.926106
3520.877540	1093973.154125	41.931111
3520.803713	1093581.454185	41.936116
3520.628121	1093185.434540	41.941120
3520.641395	1092797.397327	41.946125
3520.960013	1092376.822541	41.951130
3520.684118	1091981.784758	41.956135
3520.521771	1091562.758189	41.961140
3520.475628	1091177.487820	41.966144
3520.457060	1090778.872250	41.971149
3520.349575	1090366.927733	41.976154
3520.225634	1089974.688152	41.981159
3520.395004	1089590.035950	41.986164
3520.532528	1089188.595493	41.991168
3520.275773	1088773.393010	41.996173
3520.329693	1088386.854138	42.001178
3520.010161	1087994.216261	42.006183
3520.046312	1087599.958063	42.011188
3519.968935	1087199.268530	42.016192
3519.924011	1086810.525289	42.021197
3520.227982	1086422.271931	42.026202
3520.018863	1086031.966380	42.031207
3520.053082	1085631.814008	42.036212
3519.965220	1085253.224614	42.041216
3519.637187	1084858.444118	42.046221
3520.120927	1084449.788910	42.051226
3519.953772	1084070.746755	42.056231
3520.056411	1083672.165187	42.061236
3519.909660	1083284.433518	42.066240
3519.910683	1082886.866241	42.071245
3519.708317	1082491.893432	42.076250
3519.727537	1082093.881592	42.081255
3519.695840	1081704.387666	42.086260
3519.607033	1081324.949640	42.091264
3519.353258	1080946.759756	42.096269
3519.698741	1080554.434884	42.101274
3519.749461	1080178.636528	42.106279
3519.650923	1079780.283246	42.111284
3519.603032	1079404.543781	42.116288
3519.477753	1079014.681189	42.121293
3519.550712	1078624.470118	42.126298
3519.209162	1078240.059433	42.131303
3519.326469	1077832.984438	42.136308
3519.556173	1077462.153932	42.141312
3518.970772	1077101.130541	42.146317
3519.388486	1076710.149775	42.151322
3518.786179	1076326.703637	42.156327
3519.049803	1075951.539526	42.161332
3518.933350	1075568.248270	42.166336
3518.519481	1075209.760953	42.171341
3518.798926	1074828.273684	42.176346
3518.746483	1074455.844742	42.181351
3518.820947	1074080.679491	42.186356
3518.710643	1073722.717202	42.191360
3518.451303	1073336.314571	42.196365
3518.876704	1072943.814104	42.201370
3518.567437	1072595.804552	42.206375
3518.294500	1072227.392504	42.211380
3518.533211	1071847.818481	42.216384
3518.465336	1071473.939672	42.221389
3518.676926	1071115.850006	42.226394
3518.589009	1070755.671373	42.231399
3518.497331	1070368.839419	42.236404
3518.633970	1069982.807862	42.241408
3518.383776	1069618.831575	42.246413
3518.532660	1069266.208171	42.251418
3518.263427	1068906.899479	42.256423
3518.177812	1068524.936931	42.261428
3518.317019	1068150.701122	42.266432
3518.422672	1067797.894264	42.271437
3518.288892	1067415.381482	42.276442
3518.180528	1067067.564805	42.281447
3518.182505	1066700.275007	42.286452
3518.258628	1066330.446989	42.291456
3518.171456	1065953.789642	42.296461
3518.208484	1065596.138001	42.301466
3517.802101	1065235.168110	42.306471
3517.774648	1064867.375654	42.311476
3517.580400	1064507.862790	42.316480
3517.658850	1064157.713728	42.321485
3517.853143	1063800.015517	42.326490
3517.616418	1063432.642782	42.331495
3517.636782	1063075.407378	42.336500
3517.760277	1062733.150261	42.341504
3517.792083	1062383.088416	42.346509
3517.834814	1062023.662902	42.351514
3517.615398	1061659.153667	42.356519
3517.681012	1061300.351177	42.361524
3517.789084	1060931.791645	42.366528
3517.468533	1060572.812727	42.371533
3518.040740	1060242.172895	42.376538
3517.756804	1059879.675390	42.381543
3517.508548	1059528.803871	42.386548
3517.827914	1059182.247893	42.391552
3517.503884	1058834.427323	42.396557
3517.679935	1058466.462338	42.401562
3517.470245	1058102.583154	42.406567
3517.422201	1057742.796781	42.411572
3517.468669	1057401.569915	42.416576
3517.514278	1057051.841391	42.421581
3517.478061	1056688.514908	42.426586
3517.331420	1056340.218595	42.431591
3517.332970	1055983.393556	42.436596
3517.257873	1055620.485090	42.441600
3517.116123	1055298.438392	42.446605
3517.226092	1054940.082011	42.451610
3517.228570	1054587.408535	42.456615
3517.189058	1054243.782989	42.461620
3517.306944	1053883.235467	42.466624
3516.818182	1053525.560886	42.471629
3517.081063	1053192.042003	42.476634
3516.803737	1052863.992866	42.481639
3516.842537	1052512.820502	42.486644
3516.968397	1052154.570131	42.491648
3516.902993	1051820.443809	42.496653
3516.485759	1051478.251866	42.501658
3516.411915	1051130.772543	42.506663
3516.559434	1050785.453992	42.511668
3516.911093	1050463.815996	42.516672
3516.831580	1050126.888055	42.521677
3516.862812	1049764.638758	42.526682
3516.844412	1049425.631582	42.531687
3516.682541	1049086.048211	42.536692
3516.535052	1048744.607825	42.541696
3516.508750	1048415.288234	42.546701
3516.663755	1048073.660136	42.551706
3516.233320	1047727.956421	42.556711
3516.438203	1047390.815102	42.561716
3516.301290	1047053.613019	42.566720
3516.162970	1046720.832027	42.571725
3516.228586	1046382.300567	42.576730
3516.107758	1046063.864319	42.581735
3515.967232	1045743.578217	42.586740
3516.494287	1045397.667979	42.591744
3516.047617	1045062.520425	42.596749
3516.219772	1044728.892662	42.601754
3516.083105	1044411.909540	42.606759
3516.074005	1044074.505194	42.611764
3515.878389	1043732.474073	42.616768
3515.742711	1043419.877887	42.621773
3516.095483	1043094.913574	42.626778
3515.893096	1042766.736582	42.631783
3515.638740	1042424.827799	42.636788
3515.840938	1042113.648443	42.641792
3515.670077	1041807.634876	42.646797
3515.442070	1041474.167299	42.651802
3515.510483	1041157.544409	42.656807
3515.383569	1040828.080643	42.661812
3515.759598	1040495.324729	42.666816
3515.525701	1040176.665889	42.671821
3515.442483	1039863.667560	42.676826
3515.664429	1039562.105845	42.681831
3515.358568	1039224.068961	42.686836
3515.220918	1038888.981152	42.691840
3515.093200	1038596.029874	42.696845
3515.110764	1038277.704256	42.701850
3515.105367	1037970.968697	42.706855
3515.131826	1037648.640768	42.711860
3515.319267	1037331.393562	42.716864
3515.297065	1037025.285665	42.721869
3515.211211	1036697.988450	42.726874
3515.106877	1036411.108771	42.731879
3514.779921	1036096.874610	42.736884
3515.074049	1035783.971555	42.741888
3514.748036	1035468.637634	42.746893
3514.939481	1035150.878567	42.751898
3514.739963	1034857.258580	42.756903
3514.895468	1034541.018793	42.761908
3515.007810	1034227.768016	42.766912
3515.113104	1033923.887910	42.771917
3515.098373	1033631.624543	42.776922
3515.130342	1033331.014703	42.781927
3515.073680	1033000.011197	42.786932
3514.899190	1032672.395314	42.791937
3514.827268	1032373.009305	42.796941
3514.728244	1032068.287344	42.801946
3514.832363	1031769.130363	42.806951
3514.419349	1031455.907248	42.811956
3514.692391	1031156.980091	42.816961
3514.429737	1030844.666134	42.821965
3514.665387	1030522.666152	42.826970
3514.351541	1030240.538725	42.831975
3514.505106	1029948.151535	42.836980
3514.603560	1029637.647464	42.841985
3514.294219	1029353.924933	42.846989
3514.410538	1029049.680721	42.851994
3514.418528	1028741.950683	42.856999
3514.200367	1028423.004084	42.862004
3514.326107	1028135.854482	42.867009
3514.074214	1027833.057815	42.872013
3514.235396	1027538.605712	42.877018
3514.368494	1027261.873587	42.882023
3514.328838	1026953.471621	42.887028
3514.393459	1026660.248824	42.892033
3513.996722	1026364.857826	42.897037
3514.543060	1026052.433469	42.902042
3514.450248	1025767.717969	42.907047
3513.955720	1025476.075863	42.912052
3514.270106	1025180.505224	42.917057
3514.018852	1024876.094496	42.922061
3514.074244	1024558.627228	42.927066
3514.086381	1024293.303670	42.932071
3513.976784	1024008.210627	42.937076
3514.096824	1023690.489617	42.942081
3514.013931	1023385.194506	42.947085
3513.936214	1023099.177342	42.952090
3513.786631	1022829.253875	42.957095
3513.683283	1022536.327582	42.962100
3513.816274	1022230.352175	42.967105
3513.173388	1021956.685833	42.972109
3513.655588	1021683.596715	42.977114
3513.570177	1021402.052576	42.982119
3513.276891	1021102.196258	42.987124
3513.588735	1020819.296487	42.992129
3513.381334	1020541.900316	42.997133
3513.535026	1020249.976323	43.002138
3513.108307	1019978.797138	43.007143
3513.200206	1019683.458302	43.012148
3513.281931	1019415.951992	43.017153
3513.001050	1019128.019264	43.022157
3513.315395	1018844.922538	43.027162
3513.487752	1018571.441909	43.032167
3513.516722	1018308.064233	43.037172
3513.494317	1018023.525905	43.042177
3512.877610	1017759.549503	43.047181
3512.965528	1017469.918146	43.052186
3513.041503	1017186.291801	43.057191
3513.123975	1016925.170018	43.062196
3513.122453	1016660.943600	43.067201
3512.969577	1016385.565748	43.072205
3512.845471	1016095.024760	43.077210
3513.073432	1015825.187541	43.082215
3512.939629	1015556.853342	43.087220
3513.201078	1015293.781562	43.092225
3513.112468	1015010.558043	43.097229
3512.817307	1014727.936921	43.102234
3513.024445	1014463.184439	43.107239
3512.835722	1014203.243364	43.112244
3512.862852	1013923.053732	43.117249
3512.599118	1013652.610567	43.122253
3512.751853	1013380.434608	43.127258
3512.443687	1013131.245078	43.132263
3512.445720	1012849.549135	43.137268
3512.873471	1012569.420428	43.142273
3512.434637	1012323.810997	43.147277
3512.662098	1012062.245285	43.152282
3512.380088	1011797.933788	43.157287
3512.632229	1011516.615775	43.162292
3512.631471	1011261.365991	43.167297
3512.331303	1011015.093653	43.172301
3512.683610	1010746.352849	43.177306
3512.124090	1010486.592768	43.182311
3512.018231	1010216.444467	43.187316
3512.705947	1009960.633653	43.192321
3511.976684	1009720.206720	43.197325
3512.146460	1009433.647101	43.202330
3512.197480	1009174.114771	43.207335
3512.043021	1008921.408809	43.212340
3511.902061	1008671.119575	43.217345
3511.958968	1008422.925382	43.222349
3512.094555	1008138.833222	43.227354
3512.231117	1007894.102577	43.232359
3511.785638	1007640.609384	43.237364
3511.985322	1007396.624604	43.242369
3511.559337	1007135.813057	43.247373
3511.924702	1006891.390210	43.252378
3511.830735	1006658.118447	43.257383
3511.878382	1006430.162448	43.262388
3511.799603	1006157.870337	43.267393
3511.691292	1005907.453168	43.272397
3511.896554	1005652.401898	43.277402
3511.524491	1005407.258190	43.282407
3511.615612	1005167.669290	43.287412
3511.849700	1004919.583725	43.292417
3511.549741	1004675.952820	43.297421
3511.732180	1004403.533140	43.302426
3511.698453	1004157.403925	43.307431
3511.505498	1003925.786838	43.312436
3511.205859	1003683.961681	43.317441
3511.250807	1003425.139039	43.322445
3511.388625	1003188.961434	43.327450
3511.370046	1002968.563821	43.332455
3511.342896	1002735.994911	43.337460
3511.390612	1002477.225758	43.342465
3511.491208	1002249.092401	43.347469
3511.407673	1001995.772849	43.352474
3511.619378	1001746.967847	43.357479
3511.316404	1001492.883288	43.362484
3511.334858	1001259.175495	43.367489
3511.314689	1001024.198965	43.372493
3511.461182	1000784.025865	43.377498
3511.377082	1000548.553394	43.382503
3511.428195	1000315.677440	43.387508
3511.439430	1000071.018067	43.392513
3511.280750	999829.297005	43.397517
3511.189729	999583.075591	43.402522
3511.267659	999351.713470	43.407527
3511.039525	999116.886804	43.412532
3511.396394	998875.527017	43.417537
3510.939356	998650.359275	43.422541
3510.766776	998405.853040	43.427546
3510.759280	998155.270779	43.432551
3510.689170	997941.405971	43.437556
3510.605379	997724.418575	43.442561
3510.710578	997493.560516	43.447565
3511.042676	997269.474186	43.452570
3510.593448	997044.241352	43.457575
3510.698650	996793.775192	43.462580
3510.887353	996563.157763	43.467585
3510.731022	996343.694015	43.472589
3510.662250	996107.547369	43.477594
3510.447864	995879.014493	43.482599
3510.665629	995645.529495	43.487604
3510.801888	995429.684735	43.492609
3510.342599	995226.889668	43.497613
3510.658820	994980.791077	43.502618
3510.581210	994752.482657	43.507623
3510.424277	994531.974448	43.512628
3510.376458	994331.710888	43.517633
3510.333970	994113.896404	43.522637
3510.641356	993878.569696	43.527642
3510.404384	993636.889926	43.532647
3510.341600	993424.998000	43.537652
3510.652261	993207.577971	43.542657
3510.311317	992981.971103	43.547661
3510.592701	992757.617559	43.552666
3510.691212	992536.892349	43.557671
3510.285181	992317.119096	43.562676
3510.423790	992083.013241	43.567681
3510.309138	991870.974423	43.572685
3510.314104	991650.522708	43.577690
3510.554498	991430.121179	43.582695
3509.922788	991218.728242	43.587700
3510.143623	990988.756764	43.592705
3510.248498	990787.465520	43.597709
3509.927774	990564.879966	43.602714
3509.937902	990349.350592	43.607719
3509.881509	990140.846125	43.612724
3510.090828	989948.578223	43.617729
3509.896208	989730.620823	43.622733
3509.891810	989504.430373	43.627738
3509.756352	989292.884116	43.632743
3509.821694	989083.540515	43.637748
3509.924573	988870.573648	43.642753
3509.579243	988651.624242	43.647757
3509.757869	988439.214097	43.652762
3509.984415	988247.959076	43.657767
3509.808591	988055.105301	43.662772
3509.800326	987833.141958	43.667777
3509.558564	987617.355497	43.672781
3509.678887	987427.944322	43.677786
3509.688629	987215.613950	43.682791
3509.773455	987022.487128	43.687796
3509.653502	986811.626805	43.692801
3509.494256	986589.737478	43.697805
3509.320303	986388.824590	43.702810
3509.548672	986201.013938	43.707815
3509.359504	986000.285055	43.712820
3509.540724	985789.825331	43.717825
3509.150850	985598.192496	43.722829
3509.395569	985389.854910	43.727834
3509.143804	985190.864833	43.732839
3509.272469	985004.495412	43.737844
3509.770166	984810.444723	43.742849
3509.357437	984619.466104	43.747853
3509.457482	984393.153135	43.752858
3509.500396	984195.251324	43.757863
3509.373289	984009.282049	43.762868
3509.439970	983809.019707	43.767873
3509.140156	983601.487611	43.772877
3509.536864	983402.328341	43.777882
3509.194451	983204.455639	43.782887
3509.003907	982983.602928	43.787892
3509.237056	982798.023110	43.792897
3509.084781	982624.708003	43.797901
3509.322178	982417.337349	43.802906
3509.089472	982223.123698	43.807911
3509.075845	982022.030584	43.812916
3509.396544	981837.088807	43.817921
3509.197822	981665.217303	43.822925
3509.142382	981448.092253	43.827930
3509.211699	981242.855571	43.832935
3509.177243	981061.561410	43.837940
3508.845956	980875.914434	43.842945
3509.070076	980672.976299	43.847949
3508.957175	980497.831726	43.852954
3509.052976	980304.084891	43.857959
3509.296418	980105.519825	43.862964
3508.995054	979905.572030	43.867969
3508.938680	979726.779458	43.872973
3508.930478	979512.895162	43.877978
3509.108382	979323.791724	43.882983
3508.736166	979150.505156	43.887988
3509.142252	978943.664704	43.892993
3508.738982	978764.508298	43.897997
3508.725076	978600.429814	43.903002
3508.737441	978403.407345	43.908007
3508.787621	978199.725984	43.913012
3508.979105	978004.419482	43.918017
3508.479447	977825.933710	43.923021
3508.626832	977661.508519	43.928026
3508.751204	977479.683654	43.933031
3508.558077	977272.881513	43.938036
3508.644843	977086.944892	43.943041
3508.715415	976886.341518	43.948045
3508.534562	976711.580961	43.953050
3508.548988	976548.025523	43.958055
3508.470749	976365.123255	43.963060
3508.592289	976162.433065	43.968065
3508.416480	975977.090266	43.973069
3508.378207	975805.505032	43.978074
3508.468341	975629.493525	43.983079
3508.291758	975466.231988	43.988084
3508.435167	975266.342119	43.993089
3508.501162	975091.295894	43.998093
3508.634127	974910.170331	44.003098
3508.806619	974742.332345	44.008103
3508.581296	974561.450359	44.013108
3508.697787	974372.291262	44.018113
3508.878811	974191.526274	44.023117
3508.460911	974005.474951	44.028122
3508.317481	973825.632111	44.033127
3508.414355	973644.961560	44.038132
3508.638541	973463.481834	44.043137
3508.235168	973292.664009	44.048141
3508.111968	973103.404712	44.053146
3508.529212	972914.930570	44.058151
3508.252481	972753.466899	44.063156
3508.347021	972568.164967	44.068161
3508.193205	972404.714639	44.073165
3508.116622	972233.028765	44.078170
3508.293449	972038.695318	44.083175
3507.922995	971872.232499	44.088180
3508.208621	971703.504213	44.093185
3508.135740	971532.090292	44.098189
3508.013578	971348.448071	44.103194
3508.205475	971175.707841	44.108199
3507.980466	971014.284553	44.113204
3508.284057	970831.729954	44.118209
3507.842920	970660.644241	44.123213
3507.968977	970487.698434	44.128218
3507.992145	970321.027922	44.133223
3507.957816	970164.051248	44.138228
3507.996657	969986.700540	44.143233
3507.847424	969828.069755	44.148237
3508.118762	969648.321275	44.153242
3507.895536	969468.844394	44.158247
3507.745446	969303.347479	44.163252
3507.981665	969148.060417	44.168257
3507.920400	968985.182683	44.173261
3507.878544	968820.339265	44.178266
3507.828743	968638.458433	44.183271
3507.532216	968475.311305	44.188276
3507.936411	968301.372781	44.193281
3508.090946	968144.407721	44.198285
3507.912578	967992.682315	44.203290
3507.820382	967812.642581	44.208295
3507.631122	967643.775356	44.213300
3507.702670	967483.183109	44.218305
3507.565029	967337.700349	44.223309
3507.613116	967162.023483	44.228314
3507.752029	966989.851582	44.233319
3507.223631	966830.123310	44.238324
3507.481325	966672.023870	44.243329
3507.444621	966499.376564	44.248333
3507.220963	966356.821149	44.253338
3507.229317	966201.492041	44.258343
3507.134450	966037.263122	44.263348
3507.236340	965862.713006	44.268353
3506.951889	965723.090215	44.273357
3507.134896	965587.990629	44.278362
3507.327060	965423.990780	44.283367
3507.174225	965256.124914	44.288372
3507.192909	965111.931471	44.293377
3507.033491	964974.620886	44.298381
3507.238861	964807.270687	44.303386
3507.230897	964648.571652	44.308391
3507.144538	964497.914467	44.313396
3507.317165	964338.687313	44.318401
3507.216170	964188.318348	44.323405
3506.760002	964040.355353	44.328410
3507.394095	963882.313253	44.333415
3507.140921	963733.525120	44.338420
3507.461741	963591.497385	44.343425
3507.071868	963453.502603	44.348429
3506.923364	963296.063250	44.353434
3507.463931	963115.086381	44.358439
3507.183128	962969.614746	44.363444
3507.049189	962827.349102	44.368449
3506.879006	962678.912038	44.373453
3506.689743	962533.904313	44.378458
3506.425036	962402.919777	44.383463
3506.656114	962248.231352	44.388468
3507.033644	962096.062865	44.393473
3506.592587	961960.490942	44.398477
3506.572815	961833.079493	44.403482
3506.712326	961688.094349	44.408487
3506.481660	961546.695155	44.413492
3506.903146	961389.011802	44.418497
3506.963121	961253.144679	44.423501
3506.600351	961107.737561	44.428506
3506.735215	960968.812635	44.433511
3506.264099	960835.669880	44.438516
3506.767510	960684.521748	44.443521
3506.668694	960534.449194	44.448525
3506.349170	960389.507012	44.453530
3506.493271	960262.720136	44.458535
3506.047633	960126.909759	44.463540
3506.396233	959995.377336	44.468545
3506.613867	959868.569691	44.473549
3506.416848	959723.884744	44.478554
3506.596396	959568.544655	44.483559
3506.381586	959442.975496	44.488564
3506.239548	959325.726305	44.493569
3506.038892	959190.147687	44.498573
3506.344992	959044.284203	44.503578
3506.402369	958915.618884	44.508583
3506.305772	958792.565715	44.513588
3506.518920	958657.200617	44.518593
3506.653194	958527.337184	44.523597
3506.334674	958385.776897	44.528602
3506.421736	958245.127070	44.533607
3506.222741	958100.499824	44.538612
3506.407586	957969.144373	44.543617
3506.224791	957859.424120	44.548621
3505.840133	957716.485193	44.553626
3505.993875	957575.415746	44.558631
3505.667278	957450.998679	44.563636
3506.268503	957335.548386	44.568641
3506.407927	957206.046755	44.573645
3506.176548	957087.295451	44.578650
3506.193399	956955.356062	44.583655
3505.839300	956827.202464	44.588660
3506.206180	956676.462406	44.593665
3506.302809	956554.310719	44.598669
3506.138630	956428.471447	44.603674
3506.646269	956312.721838	44.608679
3505.986419	956174.499170	44.613684
3506.132982	956037.121481	44.618689
3506.198061	955904.953949	44.623693
3506.087691	955770.759125	44.628698
3506.185749	955652.648490	44.633703
3505.915980	955551.234673	44.638708
3505.485746	955413.984617	44.643713
3505.631092	955299.683149	44.648717
3506.116968	955179.011247	44.653722
3506.217124	955051.514267	44.658727
3505.728269	954932.527239	44.663732
3505.855295	954814.296751	44.668737
3505.971468	954700.751774	44.673741
3506.034535	954577.839872	44.678746
3506.106004	954447.750115	44.683751
3505.774530	954336.279337	44.688756
3506.001963	954203.766446	44.693761
3506.015819	954082.572442	44.698765
3505.735098	953962.476294	44.703770
3505.864176	953868.902735	44.708775
3505.877570	953744.161436	44.713780
3505.909366	953595.785399	44.718785
3506.028401	953470.063380	44.723789
3505.803585	953367.833393	44.728794
3505.760524	953239.453720	44.733799
3505.568405	953140.275218	44.738804
3505.868004	953018.626223	44.743809
3505.922212	952902.276927	44.748813
3505.690947	952776.499874	44.753818
3505.889065	952646.917466	44.758823
3505.540067	952544.691472	44.763828
3505.735701	952433.570759	44.768833
3505.617829	952320.872599	44.773837
3505.374148	952195.944501	44.778842
3505.863362	952079.026401	44.783847
3505.263674	951990.131677	44.788852
3505.494947	951866.169930	44.793857
3505.740852	951744.212424	44.798861
3505.530694	951636.107874	44.803866
3505.585780	951512.549397	44.808871
3505.470357	951414.760356	44.813876
3505.472494	951285.845736	44.818881
3505.305103	951184.806865	44.823885
3505.328740	951080.480409	44.828890
3505.499057	950976.031961	44.833895
3505.165305	950864.103024	44.838900
3505.155863	950752.405377	44.843905
3505.197980	950646.535605	44.848909
3505.078298	950523.843574	44.853914
3505.598827	950418.273185	44.858919
3505.234206	950335.150091	44.863924
3505.392682	950228.391028	44.868929
3505.416207	950109.207362	44.873933
3504.962530	950015.659414	44.878938
3505.160876	949910.227395	44.883943
3505.205753	949807.690500	44.888948
3505.140880	949686.884139	44.893953
3505.316086	949587.767884	44.898957
3504.936003	949494.102587	44.903962
3505.467982	949387.839005	44.908967
3505.301875	949276.039354	44.913972
3505.193605	949153.695735	44.918977
3505.276781	949056.499329	44.923981
3505.066289	948933.880083	44.928986
3504.920295	948846.483929	44.933991
3504.962935	948769.875302	44.938996
3505.011422	948653.047638	44.944001
3505.165394	948535.146625	44.949005
3504.547726	948448.683227	44.954010
3504.649505	948357.599140	44.959015
3504.912011	948264.380205	44.964020
3504.911892	948159.136575	44.969025
3504.967278	948061.255642	44.974029
3504.960015	947959.648227	44.979034
3505.147557	947848.046666	44.984039
3505.008953	947752.394538	44.989044
3505.115494	947660.626972	44.994049
3504.801388	947553.890348	44.999053
3504.845936	947448.912215	45.004058
3504.792160	947353.430282	45.009063
3504.770234	947270.775959	45.014068
3504.741843	947164.271569	45.019073
3505.010500	947057.811845	45.024077
3504.739285	946970.691908	45.029082
3504.756140	946884.480935	45.034087
3504.467673	946801.288282	45.039092
3504.713706	946699.710171	45.044097
3504.688341	946593.193526	45.049101
3504.545505	946504.607697	45.054106
3504.711409	946402.270592	45.059111
3504.413587	946311.695258	45.064116
3504.609302	946204.367815	45.069121
3504.597685	946121.118631	45.074125
3504.543409	946054.161693	45.079130
3505.032106	945955.977946	45.084135
3504.717557	945849.589446	45.089140
3504.644960	945742.775675	45.094145
3504.644152	945665.361730	45.099149
3504.502426	945588.161463	45.104154
3504.985574	945483.358673	45.109159
3504.641246	945387.792535	45.114164
3504.660143	945276.929851	45.119169
3504.759603	945202.750283	45.124173
3504.772968	945103.862158	45.129178
3504.997460	945016.627709	45.134183
3504.711753	944910.311012	45.139188
3504.887399	944819.344148	45.144193
3504.626304	944738.126205	45.149197
3504.639396	944639.325108	45.154202
3504.529837	944535.271621	45.159207
3504.651321	944445.361276	45.164212
3504.678397	944348.564838	45.169217
3504.658724	944267.395607	45.174221
3504.562690	944170.616133	45.179226
3504.942512	944071.456329	45.184231
3504.577763	943978.742810	45.189236
3504.795120	943895.132694	45.194241
3504.487477	943822.054747	45.199245
3504.561632	943721.213419	45.204250
3504.962406	943602.392730	45.209255
3504.889120	943529.943020	45.214260
3504.912963	943435.430521	45.219265
3504.646710	943338.184345	45.224269
3504.456398	943254.247673	45.229274
3504.718295	943139.081774	45.234279
3504.443076	943047.583059	45.239284
3504.515158	942961.968865	45.244289
3504.560588	942889.298970	45.249293
3504.170849	942826.286010	45.254298
3504.143409	942719.977864	45.259303
3504.220871	942624.579048	45.264308
3504.288928	942542.122213	45.269313
3504.248580	942453.738026	45.274317
3504.123512	942355.875048	45.279322
3504.469343	942278.161854	45.284327
3504.008436	942197.224783	45.289332
3504.211668	942122.600735	45.294337
3504.077467	942048.702337	45.299341
3503.865463	941978.363203	45.304346
3504.482848	941873.657421	45.309351
3504.107876	941785.988204	45.314356
3503.707355	941722.004856	45.319361
3503.776455	941643.848394	45.324365
3503.599756	941557.580950	45.329370
3504.058008	941466.317236	45.334375
3504.211660	941414.224780	45.339380
3503.801019	941337.485194	45.344385
3503.690799	941255.996320	45.349389
3503.540461	941171.923672	45.354394
3503.549916	941100.193736	45.359399
3503.544207	941042.945534	45.364404
3503.642236	940949.047061	45.369409
3504.095578	940893.639560	45.374413
3503.758343	940811.509865	45.379418
3504.197152	940745.458325	45.384423
3504.060081	940689.954114	45.389428
3503.841708	940606.075384	45.394433
3504.282013	940516.524335	45.399437
3504.050435	940451.346745	45.404442
3504.059684	940337.791126	45.409447
3503.743952	940278.283828	45.414452
3503.720174	940194.846007	45.419457
3503.780444	940123.861614	45.424461
3503.560875	940053.881487	45.429466
3504.070390	939983.588510	45.434471
3503.924146	939907.359887	45.439476
3503.785394	939827.292217	45.444481
3504.111608	939755.779452	45.449485
3503.980800	939677.722488	45.454490
3503.668548	939592.691951	45.459495
3504.007079	939533.548043	45.464500
3503.573702	939465.130039	45.469505
3504.117124	939384.943259	45.474509
3503.673885	939320.362018	45.479514
3503.955532	939243.861422	45.484519
3503.701655	939150.084615	45.489524
3503.620423	939079.876845	45.494529
3503.791116	939007.516126	45.499533
3503.802600	938928.465254	45.504538
3504.056272	938864.627025	45.509543
3503.787384	938799.147234	45.514548
3503.699558	938725.865852	45.519553
3503.551777	938660.460323	45.524557
3503.518274	938603.190062	45.529562
3503.551818	938525.664537	45.534567
3504.161746	938435.186583	45.539572
3503.476260	938361.039122	45.544577
3503.775045	938294.500099	45.549581
3503.644708	938232.060679	45.554586
3503.829645	938167.841528	45.559591
3503.871798	938096.544873	45.564596
3503.606852	938019.540798	45.569601
3503.933956	937933.610487	45.574605
3503.557143	937875.525278	45.579610
3504.017151	937793.025100	45.584615
3503.681446	937723.608770	45.589620
3503.884265	937653.527081	45.594625
3503.535532	937577.393951	45.599629
3503.697778	937504.438200	45.604634
3503.664194	937446.963448	45.609639
3503.701381	937376.329587	45.614644
3503.757306	937311.929325	45.619649
3503.831301	937243.014958	45.624653
3503.350496	937165.458153	45.629658
3503.662489	937075.965598	45.634663
3503.318688	937025.351052	45.639668
3503.629296	936968.006324	45.644673
3503.389983	936892.996916	45.649677
3503.225790	936821.429076	45.654682
3503.459886	936762.751105	45.659687
3503.422504	936707.764230	45.664692
3503.456221	936633.569932	45.669697
3503.884014	936570.155099	45.674701
3503.344809	936525.230575	45.679706
3503.545067	936440.736498	45.684711
3503.661563	936363.933332	45.689716
3503.343420	936306.780963	45.694721
3503.776272	936237.986327	45.699725
3503.593425	936179.658501	45.704730
3503.782123	936100.919937	45.709735
3503.471757	936022.838320	45.714740
3503.494113	935965.530187	45.719745
3503.732803	935878.333121	45.724749
3503.406229	935819.257069	45.729754
3503.494230	935759.824097	45.734759
3503.515561	935703.089237	45.739764
3503.633810	935641.922089	45.744769
3503.429051	935556.040667	45.749773
3503.419342	935507.468427	45.754778
3503.443886	935430.186855	45.759783
3503.638108	935376.395943	45.764788
3503.349467	935308.188043	45.769793
3503.563075	935243.640584	45.774797
3503.120371	935175.648351	45.779802
3503.140905	935113.915178	45.784807
3503.084838	935050.657827	45.789812
3503.413244	934915.715610	45.794817
3503.431156	934729.263739	45.799821
3503.536224	934505.153396	45.804826
3503.320423	934204.751116	45.809831
3503.203624	933834.696640	45.814836
3503.134799	933424.946529	45.819841
3503.227616	932930.332875	45.824845
3502.618243	932374.411303	45.829850
3502.810830	931755.089649	45.834855
3503.075756	931083.322736	45.839860
3502.701531	930346.524233	45.844865
3502.850258	929514.395276	45.849869
3502.510845	928630.793106	45.854874
3502.497432	927671.331753	45.859879
3502.338956	926644.894825	45.864884
3502.083153	925534.028695	45.869889
3502.030431	924348.348056	45.874893
3501.611880	923100.310252	45.879898
3501.470714	921765.802492	45.884903
3501.526506	920353.342982	45.889908
3501.036567	918860.105596	45.894913
3501.277715	917288.319252	45.899917
3500.776996	915608.291604	45.904922
3500.760645	913854.131450	45.909927
3500.435484	912033.228171	45.914932
3500.169616	910136.873646	45.919937
3499.961634	908129.970605	45.924941
3499.518383	906035.711649	45.929946
3499.192347	903864.468464	45.934951
3498.999601	901625.522517	45.939956
3498.310197	899286.722342	45.944961
3498.438425	896848.892522	45.949965
3497.927121	894334.686526	45.954970
3497.619548	891741.741760	45.959975
3497.200052	889064.008208	45.964980
3496.622512	886297.895985	45.969985
3496.621920	883414.967787	45.974989
3495.899530	880499.715676	45.979994
3495.052468	877466.450882	45.984999
3495.027093	874371.037096	45.990004
3494.160813	871196.863960	45.995009
3493.987629	867909.464416	46.000013
3493.359002	864543.169294	46.005018
3492.689278	861090.303466	46.010023
3492.315981	857578.901277	46.015028
3491.571527	853981.431358	46.020033
3491.477354	850276.449426	46.025037
3490.395446	846494.274017	46.030042
3490.072201	842623.864162	46.035047
3489.441328	838686.435842	46.040052
3488.854444	834652.722776	46.045057
3488.338893	830535.170070	46.050061
3487.415507	826342.816519	46.055066
3486.738683	822052.537341	46.060071
3486.393323	817685.208629	46.065076
3485.524051	813238.448015	46.070081
3485.147992	808701.027682	46.075085
3484.204440	804065.368630	46.080090
3483.550190	799352.225060	46.085095
3482.705859	794571.034661	46.090100
3481.869798	789713.452374	46.095105
3481.335756	784721.557476	46.100109
3480.264686	779667.319046	46.105114
3479.707243	774557.372532	46.110119
3479.141179	769346.032996	46.115124
3477.673082	764029.431926	46.120129
3477.461880	758637.448298	46.125133
3476.243380	753170.493560	46.130138
3475.421490	747592.040441	46.135143
3474.817512	741958.382549	46.140148
3473.538661	736233.167563	46.145153
3472.681181	730409.834608	46.150157
3471.325238	724519.174212	46.155162
3470.520442	718539.349930	46.160167
3469.442861	712459.349787	46.165172
3468.673224	706302.929350	46.170177
3467.660980	700048.607096	46.175181
3466.537694	693734.637009	46.180186
3465.352972	687304.147443	46.185191
3464.409076	680822.889909	46.190196
3463.219010	674226.696369	46.195201
3462.269837	667545.365814	46.200205
3460.800576	660805.595311	46.205210
3459.504045	653969.463662	46.210215
3458.352353	647053.768123	46.215220
3457.027964	640069.499948	46.220225
3456.160391	632988.725207	46.225229
3454.666945	625822.349796	46.230234
3453.356650	618566.662939	46.235239
3452.264180	611245.769582	46.240244
3450.653388	603849.331050	46.245249
3449.418752	596352.652294	46.250253
3447.707259	588768.564982	46.255258
3446.451034	581114.070676	46.260263
3445.161111	573386.020353	46.265268
3443.401425	565562.520549	46.270273
3441.685155	557673.927298	46.275277
3440.006400	549719.400991	46.280282
3438.389396	541672.978359	46.285287
3437.156951	533540.896853	46.290292
3435.487515	525334.956468	46.295297
3433.693904	517072.663422	46.300301
3431.648675	508736.503819	46.305306
3430.158311	500296.285724	46.310311
3428.707101	491778.862151	46.315316
3426.721479	483208.877953	46.320321
3425.015447	474566.176619	46.325325
3423.104558	465841.781057	46.330330
3421.124011	457031.368802	46.335335
3419.335600	448150.986366	46.340340
3417.056480	439234.527690	46.345345
3415.285742	430221.053554	46.350349
3413.173037	421152.846594	46.355354
3411.376212	412000.896358	46.360359
3408.946550	402791.428987	46.365364
3406.647089	393489.360363	46.370369
3404.723329	384137.065569	46.375373
3402.113459	374748.661318	46.380378
3399.637096	365278.965448	46.385383
3397.608396	355755.551025	46.390388
3395.246054	346173.532045	46.395393
3392.685809	336540.396004	46.400397
3389.965831	326839.731109	46.405402
3387.498094	317075.478898	46.410407
3384.924882	307284.818859	46.415412
3382.048527	297442.667027	46.420417
3379.803516	287525.225884	46.425421
3376.577018	277561.506512	46.430426
3373.826972	267565.485465	46.435431
3371.072196	257544.894807	46.440436
3367.751884	247450.920057	46.445441
3364.890919	237335.345534	46.450445
3361.306767	227192.918102	46.455450
3358.064672	216929.640863	46.460455
3355.095299	206661.574608	46.465460
3351.368088	196426.524186	46.470465
3347.515680	186162.088695	46.475469
3343.669978	175866.224815	46.480474
3339.650683	165577.078591	46.485479
3336.159092	155259.128489	46.490484
3331.540150	144934.883178	46.495489
3327.410004	134625.997832	46.500493
3322.391736	124334.811987	46.505498
3317.214765	114012.931744	46.510503
3312.113036	103720.529174	46.515508
3306.465951	93502.538516	46.520513
3300.338027	83302.996800	46.525517
3292.748873	73186.330769	46.530522
3284.360316	63118.744375	46.535527
3272.801258	53243.573319	46.540532
3247.232160	43892.266110	46.545537
3208.675713	35190.767119	46.550541
3162.582796	27186.861301	46.555546
3113.732937	19965.277379	46.560551
3067.617841	13599.558739	46.565556
3025.215640	8112.052836	46.570561
2986.832901	3546.629779	46.575565
2926.086266	597.653610	46.580570
2808.340196	358.544309	46.585575
2746.098328	350.624258	46.590580
2745.472244	342.071543	46.595585
2783.109100	340.471038	46.600589
2831.633213	326.848934	46.605594
2872.532817	325.487444	46.610599
2897.509088	336.105361	46.615604
2906.304461	332.274601	46.620609
2904.447377	311.491444	46.625613
2897.552436	317.918783	46.630618
2889.524540	323.373257	46.635623
2883.413601	304.592472	46.640628
2879.043597	311.503677	46.645633
2876.074750	308.260725	46.650637
2874.069072	305.503974	46.655642
2872.377854	304.089811	46.660647
2870.761918	305.641897	46.665652
2868.237039	303.056960	46.670657
2866.129758	303.934677	46.675661
2863.120198	315.297463	46.680666
2859.623297	311.522733	46.685671
2856.658240	288.065359	46.690676
2853.270526	292.662572	46.695681
2850.884931	286.606648	46.700685
2847.322708	284.462641	46.705690
2844.229450	285.001170	46.710695
2841.613865	311.830061	46.715700
2837.952746	296.884089	46.720705
2834.840056	273.389532	46.725709
2831.773211	300.413249	46.730714
2828.617134	307.926776	46.735719
2825.390060	291.995856	46.740724
2821.723073	280.895586	46.745729
2818.707577	269.697492	46.750733
2815.412409	288.566905	46.755738
2812.094089	298.960942	46.760743
2808.987086	281.603885	46.765748
2805.113738	271.037811	46.770753
2802.025527	289.947393	46.775757
2798.651407	277.360040	46.780762
2795.414205	279.652450	46.785767
2792.526559	271.978392	46.790772
2789.028216	282.241699	46.795777
2786.013235	281.752727	46.800781
2782.468002	272.242488	46.805786
2778.826006	275.299788	46.810791
2775.268278	275.516864	46.815796
2771.228698	288.991203	46.820801
2768.198782	269.303782	46.825805
2765.156007	274.363352	46.830810
2761.657074	263.977867	46.835815
2758.756236	271.068233	46.840820
2755.068964	268.237369	46.845825
2751.755043	256.278206	46.850829
2748.664811	274.444783	46.855834
2744.517206	266.023541	46.860839
2741.245749	255.198964	46.865844
2737.851485	283.441208	46.870849
2734.368869	260.203251	46.875853
2731.144652	250.635295	46.880858
2727.869630	260.075153	46.885863
2724.062603	268.680744	46.890868
2720.403892	254.403144	46.895873
2717.971503	253.499705	46.900877
2714.392614	256.367378	46.905882
2710.624403	249.133119	46.910887
2707.081593	246.349789	46.915892
2703.276347	277.451289	46.920897
2699.994506	255.791022	46.925901
2696.339599	250.396265	46.930906
2692.690930	242.952309	46.935911
2689.677384	254.353635	46.940916
2685.883636	273.340775	46.945921
2682.987656	255.848110	46.950925
2679.000553	244.325238	46.955930
2675.601809	257.441186	46.960935
2673.060076	249.452981	46.965940
2669.313203	255.144212	46.970945
2665.764516	267.214934	46.975949
2662.464213	263.164923	46.980954
2658.650401	243.669689	46.985959
2655.089931	238.070374	46.990964
2651.332026	255.584766	46.995969
2648.283041	263.317137	47.000973
2645.120987	262.438337	47.005978
2641.310890	234.116288	47.010983
2637.801925	240.687227	47.015988
2634.369925	262.515033	47.020993
2631.308059	242.445204	47.025997
2627.362546	248.000413	47.031002
2623.579139	259.522482	47.036007
2620.456591	241.062377	47.041012
2617.201961	236.508458	47.046017
2613.693313	241.653467	47.051021
2610.100163	247.306747	47.056026
2606.560169	235.078255	47.061031
2603.069857	239.803843	47.066036
2599.717476	236.504107	47.071041
2596.410618	241.780004	47.076045
2592.665944	234.035075	47.081050
2589.126794	230.422247	47.086055
2585.447995	246.317683	47.091060
2582.028249	254.980411	47.096065
2579.048066	236.878242	47.101069
2575.645238	226.078299	47.106074
2571.499744	239.229892	47.111079
2568.028681	243.718620	47.116084
2564.760083	231.315088	47.121089
2561.557544	232.890998	47.126093
2558.229508	240.723755	47.131098
2554.993827	231.845976	47.136103
2551.489743	224.288200	47.141108
2547.255557	242.449168	47.146113
2543.717622	236.824690	47.151117
2540.080101	230.636773	47.156122
2536.758175	244.851672	47.161127
2533.690212	241.930840	47.166132
2529.982536	256.393440	47.171137
2526.475813	228.591567	47.176141
2523.241076	227.773933	47.181146
2519.587754	228.307180	47.186151
2516.269494	221.394534	47.191156
2512.799497	224.751097	47.196161
2509.243634	241.035183	47.201165
2505.776891	230.182383	47.206170
2501.933183	224.663597	47.211175
2498.477483	226.356941	47.216180
2494.795461	230.691272	47.221185
2491.609248	223.337009	47.226189
2488.128188	221.631322	47.231194
2484.660853	244.008323	47.236199
2481.427442	236.681276	47.241204
2477.905325	229.206713	47.246209
2474.069549	216.825647	47.251213
2470.712751	211.462955	47.256218
2467.107585	225.999303	47.261223
2463.705332	228.160130	47.266228
2460.662381	218.536401	47.271233
2456.910197	213.868400	47.276237
2453.289766	223.271173	47.281242
2449.475243	243.247281	47.286247
2446.422756	217.980166	47.291252
2442.836524	242.985967	47.296257
2439.652272	226.951013	47.301261
2435.919162	205.677735	47.306266
2432.097919	217.667963	47.311271
2429.089433	227.029219	47.316276
2425.249682	227.929650	47.321281
2421.891382	223.250375	47.326285
2418.458831	223.422113	47.331290
2414.355288	231.419601	47.336295
2411.455151	203.240229	47.341300
2407.803300	214.787312	47.346305
2404.251103	209.490912	47.351309
2401.144430	218.797436	47.356314
2397.762480	222.600616	47.361319
2393.791521	212.023706	47.366324
2390.452932	228.917843	47.371329
2386.712366	229.736136	47.376333
2383.564683	229.910137	47.381338
2379.532543	244.746699	47.386343
2376.756273	225.967246	47.391348
2373.098012	214.985810	47.396353
2369.463902	223.037005	47.401357
2366.076937	227.373043	47.406362
2362.220772	237.696267	47.411367
2359.055523	209.191199	47.416372
2355.387627	223.124423	47.421377
2351.930397	217.379215	47.426381
2348.182115	211.955567	47.431386
2344.723175	214.344004	47.436391
2341.650463	216.327321	47.441396
2338.370694	221.401838	47.446401
2334.682165	226.024676	47.451405
2331.157346	213.793765	47.456410
2327.516778	215.789155	47.461415
2324.038437	206.968301	47.466420
2320.253926	223.386315	47.471425
2316.808754	210.143453	47.476429
2313.706616	216.309637	47.481434
2310.015064	229.283175	47.486439
2307.150345	215.108233	47.491444
2303.028898	223.746588	47.496449
2299.406393	220.236146	47.501453
2296.242849	208.038999	47.506458
2292.574625	202.812995	47.511463
2289.114586	224.360250	47.516468
2285.520574	218.694557	47.521473
2282.100253	208.408682	47.526477
2278.623146	194.593629	47.531482
2274.932548	208.464221	47.536487
2271.548514	226.562497	47.541492
2267.894143	221.990530	47.546497
2264.507336	206.709251	47.551501
2261.449398	198.861527	47.556506
2257.666152	218.392722	47.561511
2254.093549	217.036963	47.566516
2250.367473	208.037316	47.571521
2247.187480	194.812034	47.576525
2243.902818	207.182014	47.581530
2240.217953	220.764119	47.586535
2236.522048	220.777243	47.591540
2232.734786	211.452485	47.596545
2229.218641	198.058225	47.601549
2226.139179	196.288205	47.606554
2222.409710	221.541971	47.611559
2219.176488	194.192776	47.616564
2215.560249	186.771193	47.621569
2212.091683	208.313338	47.626573
2208.900863	207.634108	47.631578
2205.043391	210.212046	47.636583
2201.661857	195.308465	47.641588
2198.083978	193.468548	47.646593
2194.566378	205.267111	47.651597
2191.427815	214.072887	47.656602
2187.719137	202.082124	47.661607
2184.458523	185.097937	47.666612
2180.536964	196.050426	47.671617
2176.813032	211.906540	47.676621
2173.433109	202.376330	47.681626
2170.047355	201.086769	47.686631
2166.385579	206.674393	47.691636
2162.752815	205.719846	47.696641
2159.693365	193.323809	47.701645
2156.424129	205.995601	47.706650
2152.368987	210.315661	47.711655
2149.268824	203.364675	47.716660
2145.866453	206.337638	47.721665
2142.106901	194.446652	47.726669
2138.840990	201.862266	47.731674
2135.075357	220.779067	47.736679
2131.530537	199.769037	47.741684
2128.097412	194.065457	47.746689
2124.723988	196.845824	47.751693
2121.256209	205.855177	47.756698
2117.430742	218.784471	47.761703
2113.836128	188.269539	47.766708
2110.348315	191.331285	47.771713
2107.057627	212.041610	47.776717
2103.995099	197.543496	47.781722
2099.732313	216.022032	47.786727
2096.569095	209.214745	47.791732
2093.041396	208.051523	47.796737
2089.853206	185.356679	47.801741
2086.159033	203.762031	47.806746
2082.498894	210.265578	47.811751
2079.059976	192.213583	47.816756
2075.350928	194.537345	47.821761
2072.176920	198.611276	47.826765
2068.878773	180.402313	47.831770
2064.952784	196.046046	47.836775
2061.954268	213.312784	47.841780
2058.245062	204.701122	47.846785
2054.585478	182.214777	47.851789
2050.956830	172.428061	47.856794
2047.364388	199.970276	47.861799
2043.986585	200.970488	47.866804
2040.727063	198.274439	47.871809
2036.995910	197.651765	47.876813
2033.477290	194.794948	47.881818
2029.851828	194.440432	47.886823
2026.577367	177.721830	47.891828
2023.293847	184.812179	47.896833
2019.656810	187.155260	47.901837
2016.066461	189.584259	47.906842
2012.286241	212.749744	47.911847
2009.353547	184.643928	47.916852
2005.476977	179.095746	47.921857
2002.271196	176.874629	47.926861
1998.894795	188.752946	47.931866
1994.998991	179.466384	47.936871
1991.867906	172.406651	47.941876
1987.855615	183.668843	47.946881
1984.301460	191.606166	47.951885
1981.077934	184.405324	47.956890
1977.411119	186.267886	47.961895
1973.902764	185.743048	47.966900
1970.721134	200.322321	47.971905
1967.291182	195.462047	47.976909
1963.789457	178.652435	47.981914
1960.128683	177.607023	47.986919
1956.470271	188.365650	47.991924
1953.180758	198.766099	47.996929
1949.800767	186.114882	48.001933
1946.081096	196.730422	48.006938
1942.787543	198.646942	48.011943
1939.055617	194.325800	48.016948
1935.773561	184.806324	48.021953
1932.123326	183.241478	48.026957
1928.702570	194.917511	48.031962
1924.865423	197.318609	48.036967
1920.976520	172.612431	48.041972
1917.798468	187.812012	48.046977
1914.565665	209.498724	48.051981
1911.608281	172.475751	48.056986
1907.420355	168.413252	48.061991
1904.254274	168.089849	48.066996
1900.594164	188.837461	48.072001
1896.734527	204.880696	48.077005
1893.763555	181.962722	48.082010
1889.826705	172.678366	48.087015
1886.472293	187.173795	48.092020
1883.199122	194.543148	48.097025
1879.696374	186.633661	48.102029
1876.241830	171.640348	48.107034
1872.261364	183.051329	48.112039
1868.961078	187.387860	48.117044
1865.795619	196.283403	48.122049
1861.833891	192.487445	48.127053
1858.842396	174.249933	48.132058
1855.190172	194.530149	48.137063
1851.570859	169.685935	48.142068
1847.930219	167.177555	48.147073
1844.404256	179.496889	48.152077
1840.813980	185.647878	48.157082
1837.165648	181.762843	48.162087
1834.214498	166.919123	48.167092
1830.854877	168.531406	48.172097
1827.133395	181.111082	48.177101
1823.943909	168.418758	48.182106
1819.656352	172.072578	48.187111
1816.351857	190.319001	48.192116
1812.748578	188.220572	48.197121
1809.473907	163.156275	48.202125
1806.261956	165.989841	48.207130
1802.620113	178.652863	48.212135
1799.212606	171.790163	48.217140
1795.650344	166.143097	48.222145
1791.589665	182.321521	48.227149
1788.574071	182.094085	48.232154
1785.027475	180.616981	48.237159
1781.405801	175.781835	48.242164
1777.954613	162.456388	48.247169
1774.351597	178.974810	48.252173
1770.958120	181.421653	48.257178
1767.789462	183.045863	48.262183
1764.179552	166.189929	48.267188
1760.581276	178.438950	48.272193
1757.096025	172.958245	48.277197
1753.398824	163.420868	48.282202
1749.662199	175.399140	48.287207
1746.328823	165.089591	48.292212
1742.846085	175.572389	48.297217
1739.069579	188.519770	48.302221
1735.860170	168.489350	48.307226
1732.455757	176.855055	48.312231
1729.341099	178.948521	48.317236
1725.525331	180.254742	48.322241
1721.892741	180.687096	48.327245
1718.847683	188.907398	48.332250
1715.288543	177.725470	48.337255
1711.608926	164.485401	48.342260
1708.050315	182.876171	48.347265
1704.178368	194.036613	48.352269
1700.806623	171.865291	48.357274
1697.072475	168.556992	48.362279
1693.981169	177.288922	48.367284
1690.545209	183.276502	48.372289
1686.675610	173.424013	48.377293
1683.520523	168.802158	48.382298
1679.997070	159.988157	48.387303
1676.358449	169.727437	48.392308
1672.972329	190.841269	48.397313
1669.544637	183.129246	48.402317
1665.983812	169.153806	48.407322
1662.458059	187.639302	48.412327
1658.946881	174.713676	48.417332
1655.450792	168.049357	48.422337
1651.662661	173.178518	48.427341
1648.296587	185.834768	48.432346
1644.924286	175.354224	48.437351
1641.823105	161.816722	48.442356
1638.122600	169.023269	48.447361
1634.267523	181.100550	48.452365
1630.991590	169.282423	48.457370
1627.013086	190.187024	48.462375
1623.721337	181.012129	48.467380
1620.315442	172.957882	48.472385
1616.854884	175.367623	48.477389
1613.329387	169.438967	48.482394
1609.778221	176.313301	48.487399
1606.306224	181.248068	48.492404
1603.299336	176.028647	48.497409
1599.324006	167.695688	48.502413
1596.162717	183.921985	48.507418
1592.339568	167.344623	48.512423
1588.926335	156.921784	48.517428
1585.079885	166.977726	48.522433
1581.389857	183.229920	48.527437
1578.276978	180.930930	48.532442
1575.031046	172.778594	48.537447
1571.219936	161.282425	48.542452
1567.717982	169.860005	48.547457
1564.348507	191.697269	48.552461
1561.067415	166.937058	48.557466
1557.416456	164.294304	48.562471
1553.690238	166.056586	48.567476
1550.489666	160.705797	48.572481
1547.109234	160.353608	48.577485
1543.736677	157.351316	48.582490
1539.688081	165.821030	48.587495
1536.196533	169.141612	48.592500
1532.771212	160.596005	48.597505
1529.085228	168.266021	48.602509
1525.747756	166.426634	48.607514
1522.482807	186.343329	48.612519
1518.711670	178.715892	48.617524
1515.218562	152.190592	48.622529
1511.499966	163.216682	48.627533
1508.208188	155.182642	48.632538
1504.711946	159.249102	48.637543
1501.360836	165.023877	48.642548
1498.052580	177.082585	48.647553
1494.784702	171.668153	48.652557
1491.205674	164.197454	48.657562
1487.233668	165.201578	48.662567
1483.654029	173.220545	48.667572
1480.242292	179.593381	48.672577
1476.378597	181.468853	48.677581
1473.023255	153.500903	48.682586
1469.483818	165.058160	48.687591
1466.259562	161.498928	48.692596
1462.653713	154.134088	48.697601
1459.169930	163.571782	48.702605
1455.986067	172.369279	48.707610
1452.387874	169.741844	48.712615
1448.691302	166.993626	48.717620
1445.113882	163.307725	48.722625
1441.633894	162.436259	48.727629
1438.735995	154.864428	48.732634
1434.664728	162.443489	48.737639
1431.207726	154.668092	48.742644
1427.759289	167.026069	48.747649
1424.188228	154.659569	48.752653
1420.683099	153.446701	48.757658
1417.177102	174.022602	48.762663
1413.762702	161.783843	48.767668
1410.324110	154.337271	48.772673
1406.466240	152.881653	48.777677
1403.328024	158.572399	48.782682
1399.759383	176.040972	48.787687
1396.446431	172.319041	48.792692
1392.548751	150.010057	48.797697
1388.997388	150.960197	48.802701
1385.939114	160.916520	48.807706
1382.063248	173.678398	48.812711
1378.425791	152.454415	48.817716
1375.175364	159.876224	48.822721
1371.808286	172.529369	48.827725
1368.319563	151.872242	48.832730
1364.747649	157.726328	48.837735
1361.095685	162.881490	48.842740
1357.372185	157.103254	48.847745
1353.978207	159.351885	48.852749
1350.893352	136.765754	48.857754
1347.171033	161.791072	48.862759
1343.779558	168.749054	48.867764
1340.037970	156.398719	48.872769
1336.636816	144.990918	48.877773
1333.585954	153.436123	48.882778
1329.794221	173.692734	48.887783
1326.174498	164.390147	48.892788
1322.856622	153.857521	48.897793
1318.813457	149.470827	48.902797
1315.542039	165.792700	48.907802
1311.950131	169.417313	48.912807
1308.609000	143.749513	48.917812
1305.492236	146.645607	48.922817
1301.516985	157.099962	48.927821
1298.155657	137.469125	48.932826
1294.636254	152.609577	48.937831
1290.677649	165.480931	48.942836
1287.793007	149.811436	48.947841
1283.919466	159.447102	48.952845
1280.427738	154.316063	48.957850
1277.195087	147.713151	48.962855
1273.557562	162.175084	48.967860
1270.412535	145.511399	48.972865
1266.527020	151.497000	48.977869
1263.196114	147.827926	48.982874
1259.533031	159.858661	48.987879
1256.157137	164.706392	48.992884
1252.595390	160.959217	48.997889
1248.930592	149.052324	49.002893
1245.661352	154.034171	49.007898
1241.934316	162.165166	49.012903
1238.630894	146.263561	49.017908
1234.971213	149.880750	49.022913
1231.312586	143.811332	49.027917
1228.445706	154.885259	49.032922
1224.639269	157.283519	49.037927
1221.047553	145.130985	49.042932
1217.766434	154.088737	49.047937
1213.586083	172.511351	49.052941
1210.596780	147.477854	49.057946
1206.951166	146.335342	49.062951
1203.570694	147.727325	49.067956
1200.136190	151.316042	49.072961
1196.324081	152.447922	49.077965
1193.167242	138.707011	49.082970
1189.273418	148.896517	49.087975
1186.017193	154.631786	49.092980
1182.603881	138.763952	49.097985
1178.746220	160.199568	49.102989
1175.561266	152.948510	49.107994
1171.629361	137.967808	49.112999
1168.639888	144.174381	49.118004
1165.313608	148.975089	49.123009
1161.912999	146.381690	49.128013
1157.962015	149.029355	49.133018
1154.601360	165.860331	49.138023
1150.667858	155.850858	49.143028
1147.377179	147.012173	49.148033
1143.654658	156.080703	49.153037
1140.595048	158.499152	49.158042
1137.011703	160.116134	49.163047
1133.519258	156.421411	49.168052
1130.411174	161.414389	49.173057
1126.191044	162.111352	49.178061
1122.959124	144.183631	49.183066
1119.164984	150.417906	49.188071
1115.819761	163.945096	49.193076
1112.673021	151.705160	49.198081
1108.712134	137.503576	49.203085
1105.549958	148.842027	49.208090
1102.114709	166.878382	49.213095
1098.012002	164.028230	49.218100
1095.238863	154.133238	49.223105
1091.497558	151.048230	49.228109
1087.931273	149.775690	49.233114
1084.289180	168.006897	49.238119
1080.790031	160.134684	49.243124
1077.611634	131.396142	49.248129
1073.434578	148.686951	49.253133
1070.425318	153.631772	49.258138
1066.922582	159.002248	49.263143
1063.626882	147.516043	49.268148
1060.436810	146.096570	49.273153
1056.623202	160.153603	49.278157
1053.036476	127.848612	49.283162
1049.205906	147.280391	49.288167
1045.538220	162.992915	49.293172
1042.202345	147.345882	49.298177
1038.625081	145.336014	49.303181
1035.570994	140.447156	49.308186
1031.849494	161.164777	49.313191
1028.413720	165.205592	49.318196
1025.144128	154.855561	49.323201
1021.178969	140.222174	49.328205
1018.036288	153.709735	49.333210
1014.323372	170.652287	49.338215
1010.572204	174.182597	49.343220
1007.303480	147.757486	49.348225
1003.832459	144.881628	49.353229
1000.378590	157.889161	49.358234
997.118051	150.997231	49.363239
993.260187	156.107939	49.368244
989.985714	164.583088	49.373249
986.007535	159.312151	49.378253
982.683143	136.169501	49.383258
979.395359	138.849422	49.388263
975.640873	161.541908	49.393268
972.291843	163.339186	49.398273
968.840642	137.902317	49.403277
965.519287	146.948782	49.408282
961.833358	161.292061	49.413287
957.671830	151.003419	49.418292
954.694462	140.724850	49.423297
951.407347	149.847546	49.428301
948.044878	153.433266	49.433306
944.233630	161.805388	49.438311
940.774182	157.090141	49.443316
937.438846	141.550915	49.448321
933.649553	135.473267	49.453325
930.521072	142.328798	49.458330
927.254475	150.592052	49.463335
923.206782	149.066943	49.468340
919.460693	126.163165	49.473345
915.658972	137.897889	49.478349
912.869581	141.566662	49.483354
909.192082	141.271930	49.488359
905.454157	166.339708	49.493364
902.227568	161.248853	49.498369
898.560992	145.063946	49.503373
895.553195	130.232927	49.508378
892.009892	141.965440	49.513383
888.360520	167.302805	49.518388
885.090661	152.798062	49.523393
880.951815	136.907197	49.528397
877.688085	144.950701	49.533402
874.153191	144.646646	49.538407
870.528180	138.931665	49.543412
867.084667	142.932693	49.548417
864.052240	150.349283	49.553421
860.300251	136.218745	49.558426
856.669050	142.724453	49.563431
853.053067	144.905511	49.568436
849.982204	149.452583	49.573441
846.097454	156.532569	49.578445
842.941907	137.101278	49.583450
839.558220	140.512392	49.588455
835.718261	133.840140	49.593460
832.487641	135.840183	49.598465
828.540554	141.186675	49.603469
824.807265	156.367055	49.608474
821.500794	145.055708	49.613479
817.914467	139.669278	49.618484
815.044532	149.460823	49.623489
810.986227	146.596917	49.628493
807.424982	124.233778	49.633498
803.988672	147.602563	49.638503
800.574460	153.313574	49.643508
797.344733	125.099074	49.648513
793.703202	128.695529	49.653517
790.547107	139.612644	49.658522
786.804341	150.162217	49.663527
782.974628	139.187474	49.668532
779.529424	136.005222	49.673537
775.935484	141.533829	49.678541
772.547373	130.347575	49.683546
769.366625	136.361361	49.688551
765.636587	151.413474	49.693556
761.988237	139.551352	49.698561
758.072808	132.224956	49.703565
755.010247	138.108746	49.708570
751.988169	124.764031	49.713575
747.879446	125.440364	49.718580
744.712328	145.328330	49.723585
740.900672	143.044525	49.728589
737.843352	126.366327	49.733594
734.224035	129.141161	49.738599
730.486307	131.157522	49.743604
727.353140	136.809915	49.748609
723.360643	151.361447	49.753613
719.963041	142.313982	49.758618
716.552141	140.202834	49.763623
713.375934	132.701315	49.768628
709.928225	138.444726	49.773633
706.069483	140.820137	49.778637
702.414031	124.291942	49.783642
698.825108	127.673486	49.788647
695.434356	154.515651	49.793652
692.065452	130.072712	49.798657
688.444519	131.924894	49.803661
685.165905	138.292942	49.808666
681.594938	131.363092	49.813671
678.012528	130.175219	49.818676
674.745018	131.241319	49.823681
670.957122	131.194308	49.828685
667.538577	132.985060	49.833690
664.201469	133.017985	49.838695
660.147970	136.049233	49.843700
656.942585	145.140787	49.848705
653.534395	141.599038	49.853709
649.984651	127.866938	49.858714
646.518045	122.942145	49.863719
642.990224	130.878818	49.868724
639.807861	142.919677	49.873729
635.770214	145.718179	49.878733
632.528218	124.398026	49.883738
629.112660	132.746464	49.888743
625.507484	133.069512	49.893748
621.841247	142.190237	49.898753
618.313620	129.591709	49.903757
614.762399	129.770409	49.908762
611.471279	142.926986	49.913767
607.895585	137.763054	49.918772
605.211174	124.284629	49.923777
600.719284	140.196562	49.928781
597.355425	132.223495	49.933786
593.853595	129.856944	49.938791
590.468690	141.473549	49.943796
586.982087	124.900584	49.948801
583.220943	133.058122	49.953805
579.727363	139.618865	49.958810
576.610069	123.412349	49.963815
573.116338	117.744533	49.968820
569.531287	123.631728	49.973825
565.898646	132.034890	49.978829
562.700140	149.041975	49.983834
558.950739	135.395881	49.988839
555.376711	128.071338	49.993844
551.983384	129.072653	49.998849
548.519695	137.922708	50.003853
544.972017	127.051106	50.008858
541.106754	127.397627	50.013863
537.644128	141.697072	50.018868
534.714489	124.612701	50.023873
530.870562	127.905348	50.028877
527.399311	149.174261	50.033882
524.067895	133.938507	50.038887
520.509748	133.284243	50.043892
517.252102	126.945133	50.048897
513.374221	142.063290	50.053901
509.685675	148.851496	50.058906
505.902881	141.895775	50.063911
502.427127	123.011160	50.068916
499.709007	136.665894	50.073921
495.832641	163.859909	50.078925
492.495995	149.784918	50.083930
489.254819	129.865615	50.088935
485.034480	124.088615	50.093940
481.758248	134.273796	50.098945
478.128728	143.141905	50.103949
474.605667	126.796107	50.108954
471.496370	130.345850	50.113959
467.911054	140.308941	50.118964
464.570737	119.966672	50.123969
460.689748	133.737938	50.128973
457.086543	127.266542	50.133978
453.961038	120.461634	50.138983
450.306277	143.799513	50.143988
446.916694	127.203023	50.148993
443.461340	127.897884	50.153997
439.531175	129.468741	50.159002
436.327808	118.307436	50.164007
432.342333	135.879282	50.169012
429.265015	133.280917	50.174017
425.823486	122.691453	50.179021
422.436689	147.437262	50.184026
418.977676	130.564997	50.189031
415.358867	138.014102	50.194036
411.962913	122.993099	50.199041
408.355154	120.647704	50.204045
404.623167	130.220631	50.209050
401.155917	130.214621	50.214055
397.655457	132.767278	50.219060
394.667636	124.055007	50.224065
390.838370	115.307733	50.229069
387.364536	124.259160	50.234074
383.759196	127.995944	50.239079
379.853204	125.583034	50.244084
376.666544	115.928108	50.249089
373.271389	118.947340	50.254093
369.628810	135.698843	50.259098
366.439963	127.243823	50.264103
362.716379	132.825514	50.269108
359.332561	125.646744	50.274113
355.416967	137.184594	50.279117
351.794870	141.241611	50.284122
348.768771	127.401018	50.289127
345.027227	127.809093	50.294132
341.994005	132.944996	50.299137
338.263941	142.747886	50.304141
334.754278	137.504454	50.309146
331.133044	125.072027	50.314151
327.547987	118.588913	50.319156
324.388604	133.728251	50.324161
320.378265	125.853773	50.329165
316.946300	116.408859	50.334170
313.609552	132.407219	50.339175
309.928673	131.184229	50.344180
307.099787	115.342570	50.349185
303.674094	116.959193	50.354189
299.580984	134.276045	50.359194
296.182270	139.080033	50.364199
292.127535	127.801405	50.369204
289.222485	105.419444	50.374209
285.455507	125.539095	50.379213
282.257515	115.722245	50.384218
278.766119	121.178708	50.389223
274.948485	126.254139	50.394228
271.440148	118.091577	50.399233
268.069819	116.408515	50.404237
264.437076	143.713269	50.409242
260.962015	128.329665	50.414247
257.641557	126.094231	50.419252
254.608610	111.406481	50.424257
250.876694	114.102511	50.429261
247.316243	134.950826	50.434266
243.770343	121.546651	50.439271
239.972513	108.516776	50.444276
236.393335	126.414773	50.449281
232.984074	137.587217	50.454285
229.678293	121.776943	50.459290
226.186473	113.990684	50.464295
222.685224	131.154413	50.469300
218.901224	107.958405	50.474305
215.638224	112.658322	50.479309
212.012635	113.217186	50.484314
208.728670	117.100621	50.489319
205.176216	118.684674	50.494324
201.938173	109.315544	50.499329
198.230164	111.432937	50.504333
194.464230	108.538991	50.509338
191.194141	110.300029	50.514343
187.492381	136.560159	50.519348
184.152724	130.250377	50.524353
180.386134	114.752664	50.529357
177.002682	98.907958	50.534362
173.432820	109.006123	50.539367
169.680732	136.804681	50.544372
166.504955	135.475234	50.549377
163.082997	112.847924	50.554381
159.371408	106.484895	50.559386
156.082159	119.914069	50.564391
152.666023	122.994093	50.569396
149.509873	112.069320	50.574401
145.535288	133.785601	50.579405
141.941534	116.985139	50.584410
138.367554	108.382305	50.589415
134.790072	124.059820	50.594420
131.602659	120.410373	50.599425
128.014279	122.446681	50.604429
124.329388	125.382911	50.609434
121.095795	120.398915	50.614439
117.428563	115.346597	50.619444
114.334555	118.980976	50.624449
110.362028	138.182931	50.629453
106.566678	128.793774	50.634458
103.395224	116.469393	50.639463
99.736128	110.856417	50.644468
96.760671	102.191312	50.649473
93.299615	125.283995	50.654477
89.625609	123.096717	50.659482
85.880677	121.113227	50.664487
82.385466	125.023739	50.669492
78.853242	113.539482	50.674497
75.057863	119.007014	50.679501
71.983168	118.517166	50.684506
68.642868	120.143279	50.689511
64.957930	121.910785	50.694516
61.467788	102.498580	50.699521
57.763780	122.532244	50.704525
54.588738	142.274820	50.709530
51.194298	130.594674	50.714535
47.122720	111.681027	50.719540
44.001895	104.853685	50.724545
40.750540	117.604954	50.729549
36.818078	122.161473	50.734554
33.294204	104.261981	50.739559
29.785746	115.511333	50.744564
26.438308	125.701158	50.749569
22.782020	119.953901	50.754573
19.370842	130.452868	50.759578
16.002791	134.809691	50.764583
12.462692	136.722965	50.769588
8.920074	113.177883	50.774593
5.421798	115.834847	50.779597
1.785662	125.603230	50.784602