Wed Jun 15 16:29:46 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.301443	82.360847	0.000000
0.506291	104.232303	0.005005
0.475413	88.755615	0.010010
0.252429	72.380653	0.015014
-0.167592	82.065330	0.020019
-0.135486	74.017547	0.025024
0.042880	71.485460	0.030029
-0.425955	83.577473	0.035034
-0.432168	68.744637	0.040038
-0.633427	51.717017	0.045043
-1.143378	41.778314	0.050048
-1.207781	48.347761	0.055053
-1.569841	47.842192	0.060058
-1.581492	25.275575	0.065062
-2.013510	27.909525	0.070067
-2.052180	23.920012	0.075072
-2.835274	-4.992701	0.080077
-3.019089	8.733369	0.085082
-3.036760	5.830820	0.090086
-4.618292	16.922516	0.095091
-4.738914	4.540265	0.100096
-4.161401	0.956463	0.105101
-4.561197	14.513540	0.110106
-4.771804	19.643431	0.115110
-5.113717	9.386963	0.120115
-4.920447	6.306025	0.125120
-4.983278	7.941139	0.130125
-5.874074	2.963055	0.135130
-6.249832	-4.883620	0.140134
-6.431889	6.504159	0.145139
-6.772009	6.312902	0.150144
-6.782403	14.424906	0.155149
-6.898490	31.907280	0.160154
-7.057943	16.713916	0.165158
-7.822678	2.824069	0.170163
-7.784974	2.583593	0.175168
-7.824510	13.964004	0.180173
-8.202060	17.144031	0.185178
-8.432738	9.250883	0.190182
-9.281503	2.904840	0.195187
-9.732249	14.778861	0.200192
-9.827734	17.340230	0.205197
-9.736972	22.952216	0.210202
-9.691689	4.199830	0.215206
-9.883082	4.823764	0.220211
-9.940371	6.050162	0.225216
-9.650222	5.663108	0.230221
-11.061943	18.288501	0.235226
-11.072909	8.741058	0.240230
-11.391155	7.681656	0.245235
-11.299685	17.650207	0.250240
-11.471782	11.079390	0.255245
-12.603262	7.651936	0.260250
-12.869912	11.149327	0.265254
-13.023433	7.419888	0.270259
-12.973695	11.623381	0.275264
-12.940633	11.387026	0.280269
-13.206270	9.518322	0.285274
-12.981805	-13.053321	0.290278
-13.431233	7.379650	0.295283
-13.808953	24.251525	0.300288
-14.227612	2.221068	0.305293
-14.389751	-7.613892	0.310298
-14.584830	-7.466200	0.315302
-15.383927	20.218692	0.320307
-15.820754	26.677734	0.325312
-16.030026	17.989807	0.330317
-16.421215	2.256198	0.335322
-16.290091	-3.464679	0.340326
-16.336924	24.084659	0.345331
-16.167426	8.453015	0.350336
-16.158909	-0.909918	0.355341
-17.002923	22.976262	0.360346
-17.196520	-7.543926	0.365350
-17.676415	9.878096	0.370355
-18.005580	24.742992	0.375360
-17.641539	18.740553	0.380365
-18.612080	12.996642	0.385370
-18.612330	-4.799730	0.390374
-19.265218	1.329624	0.395379
-19.129402	-1.282425	0.400384
-19.106799	19.118820	0.405389
-19.551805	-2.898693	0.410394
-19.329981	-2.315424	0.415398
-20.174555	26.274866	0.420403
-20.501383	26.427066	0.425408
-20.559369	15.938024	0.430413
-21.031908	-4.280867	0.435418
-20.965997	7.034959	0.440422
-21.348799	-1.903939	0.445427
-21.420309	12.251719	0.450432
-22.221745	20.850364	0.455437
-22.633821	17.304419	0.460442
-22.615482	2.961610	0.465446
-22.785135	1.649880	0.470451
-22.791522	17.744511	0.475456
-22.605562	23.792562	0.480461
-22.965004	12.043424	0.485466
-23.071944	-8.591101	0.490470
-23.952174	8.574999	0.495475
-24.184748	6.782116	0.500480
-24.067659	2.195711	0.505485
-24.483805	-1.245683	0.510490
-25.183339	-0.101268	0.515494
-25.821698	-4.448595	0.520499
-25.654331	-0.256950	0.525504
-25.820436	7.112826	0.530509
-26.619408	20.314854	0.535514
-25.961646	3.621694	0.540518
-26.030907	2.235568	0.545523
-26.043748	-1.913573	0.550528
-25.904067	0.149538	0.555533
-27.026024	9.267639	0.560538
-27.121622	-2.356207	0.565542
-27.281596	5.947123	0.570547
-28.246376	4.654041	0.575552
-28.252146	11.829428	0.580557
-28.906221	5.121837	0.585562
-28.845472	-18.864050	0.590566
-29.050505	5.015348	0.595571
-28.794461	10.900094	0.600576
-28.975367	6.845311	0.605581
-29.276022	-2.610450	0.610586
-29.966152	5.715386	0.615590
-30.333221	-2.438130	0.620595
-30.507209	-5.793176	0.625600
-30.598806	8.460398	0.630605
-30.566315	6.530196	0.635610
-30.861458	-9.357670	0.640614
-31.481301	8.417544	0.645619
-31.964728	-15.697608	0.650624
-31.773135	-5.744240	0.655629
-32.095998	2.167947	0.660634
-32.092106	10.671971	0.665638
-32.387726	0.623502	0.670643
-33.247970	-2.518207	0.675648
-33.251222	10.102292	0.680653
-33.578693	19.891192	0.685658
-33.536345	2.386376	0.690662
-33.753010	6.530117	0.695667
-33.992072	10.754405	0.700672
-34.076676	6.111860	0.705677
-34.719497	16.881818	0.710682
-34.770361	4.871577	0.715686
-35.358154	4.766431	0.720691
-35.280379	6.719524	0.725696
-35.382581	4.469872	0.730701
-36.265487	9.180050	0.735706
-36.453384	-5.347758	0.740710
-37.050926	8.049236	0.745715
-37.054118	11.317141	0.750720
-36.978037	16.156096	0.755725
-37.195715	20.883004	0.760730
-37.000699	12.226423	0.765734
-37.149513	2.996126	0.770739
-37.307948	12.813512	0.775744
-37.904533	9.435476	0.780749
-38.599527	-8.988974	0.785754
-38.512693	-7.350580	0.790758
-38.703944	0.134127	0.795763
-39.030711	16.536106	0.800768
-39.227970	14.281151	0.805773
-39.777573	-1.188829	0.810778
-39.791902	-1.485122	0.815782
-39.929484	17.300337	0.820787
-40.429579	28.058850	0.825792
-41.097660	-2.064302	0.830797
-41.808069	-1.902669	0.835802
-41.130248	-9.794718	0.840806
-41.399708	5.053582	0.845811
-41.780608	-4.141414	0.850816
-41.756120	14.673092	0.855821
-42.161160	18.743303	0.860826
-41.939761	-3.069652	0.865830
-42.407980	-0.360177	0.870835
-43.359899	21.787448	0.875840
-43.672162	9.199923	0.880845
-43.923304	-0.505308	0.885850
-43.539791	-0.327165	0.890854
-43.652954	8.289126	0.895859
-43.801955	9.251710	0.900864
-43.966193	-6.300889	0.905869
-45.090036	2.344517	0.910874
-45.185003	5.428125	0.915878
-45.372962	-14.738438	0.920883
-45.665861	-4.923800	0.925888
-45.507607	-0.687443	0.930893
-45.396230	11.662665	0.935898
-45.752305	7.342079	0.940902
-46.710546	-1.143438	0.945907
-46.841805	5.514374	0.950912
-46.996684	18.580264	0.955917
-47.325122	12.948449	0.960922
-47.171483	-14.466323	0.965926
-47.310212	-5.751017	0.970931
-48.113563	8.490362	0.975936
-48.383677	8.697903	0.980941
-48.723639	4.564252	0.985946
-48.655154	3.338054	0.990950
-48.694782	9.120634	0.995955
-48.754637	-1.072739	1.000960
-49.048039	5.361013	1.005965
-49.970994	11.142789	1.010970
-50.176403	8.481874	1.015974
-50.286973	17.966217	1.020979
-50.308301	6.241509	1.025984
-50.209736	2.551402	1.030989
-51.074082	2.888713	1.035994
-51.238365	7.535472	1.040998
-51.649688	9.661923	1.046003
-52.061894	15.363042	1.051008
-51.895321	4.431763	1.056013
-51.911110	-5.466541	1.061018
-51.848861	9.460905	1.066022
-52.419916	15.699161	1.071027
-52.995463	15.974244	1.076032
-52.649202	4.862440	1.081037
-53.087830	-5.921761	1.086042
-53.940137	17.391562	1.091046
-54.343847	19.809536	1.096051
-54.728386	1.803029	1.101056
-54.995840	0.871959	1.106061
-55.081239	23.635657	1.111066
-54.734653	0.529186	1.116070
-54.693298	21.246642	1.121075
-55.032730	25.907653	1.126080
-55.117858	15.051404	1.131085
-56.168433	-4.497437	1.136090
-55.936733	0.528474	1.141094
-56.361890	20.438766	1.146099
-56.299450	19.427035	1.151104
-57.007491	0.130834	1.156109
-57.515213	-2.066200	1.161114
-57.743603	5.838957	1.166118
-58.016172	3.403795	1.171123
-57.955608	7.148767	1.176128
-57.880252	-5.131007	1.181133
-58.102182	-5.736376	1.186138
-58.915161	5.287395	1.191142
-59.225873	17.538577	1.196147
-59.967453	13.632977	1.201152
-59.605603	-16.327912	1.206157
-60.057703	4.822741	1.211162
-59.838251	14.667148	1.216166
-59.655881	12.040399	1.221171
-59.807282	3.887150	1.226176
-60.146302	3.787454	1.231181
-61.393901	13.300881	1.236186
-61.306457	-5.161725	1.241190
-61.692396	5.481134	1.246195
-61.769268	13.413536	1.251200
-61.334268	0.660898	1.256205
-62.361501	4.561967	1.261210
-62.796789	4.720947	1.266214
-63.165164	6.958773	1.271219
-62.977873	6.770224	1.276224
-62.701637	20.939440	1.281229
-63.111226	17.926070	1.286234
-63.190116	-7.485458	1.291238
-63.880820	-0.635661	1.296243
-64.714522	22.669069	1.301248
-64.355209	6.435992	1.306253
-64.930865	7.255519	1.311258
-64.728402	15.050610	1.316262
-64.972379	4.436853	1.321267
-65.487400	-3.909423	1.326272
-65.831668	5.238482	1.331277
-66.270622	15.757037	1.336282
-66.079709	12.309822	1.341286
-65.773915	-6.179497	1.346291
-66.835525	15.999956	1.351296
-67.144092	0.117267	1.356301
-67.441566	-9.583454	1.361306
-67.540352	-9.634070	1.366310
-68.029580	14.796872	1.371315
-67.928765	3.849927	1.376320
-67.488020	-5.176530	1.381325
-68.661034	-4.494439	1.386330
-69.433326	7.542998	1.391334
-69.534382	-5.033348	1.396339
-69.315764	10.525430	1.401344
-69.266799	11.402325	1.406349
-69.784764	-1.082633	1.411354
-69.780465	-11.718173	1.416358
-70.144248	-8.432309	1.421363
-70.392757	1.563705	1.426368
-70.953912	2.794851	1.431373
-71.433444	9.676339	1.436378
-71.288291	1.795766	1.441382
-71.729529	-4.640299	1.446387
-71.407507	-3.988460	1.451392
-71.485194	-17.165759	1.456397
-72.014084	1.919417	1.461402
-72.517641	10.722249	1.466406
-72.760379	0.802855	1.471411
-73.164802	11.393629	1.476416
-73.227089	1.386409	1.481421
-73.523984	0.085352	1.486426
-73.415095	8.511648	1.491430
-74.091336	-4.573843	1.496435
-74.548279	-4.444330	1.501440
-74.595914	-5.040820	1.506445
-74.777786	13.198349	1.511450
-74.888456	3.380335	1.516454
-75.007741	-2.005784	1.521459
-75.332257	-9.984124	1.526464
-75.909140	-3.735047	1.531469
-76.152507	14.766326	1.536474
-76.255633	-9.034846	1.541478
-76.329890	-10.802001	1.546483
-76.660498	6.098855	1.551488
-76.607555	-10.869084	1.556493
-77.234703	-1.571645	1.561498
-77.815123	-17.732745	1.566502
-77.701897	-14.923947	1.571507
-77.915262	-7.713574	1.576512
-77.851110	4.633871	1.581517
-78.750684	19.927038	1.586522
-78.887681	-6.829485	1.591526
-79.272392	-4.373715	1.596531
-79.665036	4.038692	1.601536
-79.433890	0.914110	1.606541
-79.628920	-0.813752	1.611546
-79.447666	6.519823	1.616550
-79.903612	-3.141097	1.621555
-80.666574	-8.355139	1.626560
-80.726752	-1.119376	1.631565
-81.280054	3.273343	1.636570
-81.355074	-0.847664	1.641574
-81.308530	9.440018	1.646579
-81.443760	-1.152542	1.651584
-82.052490	-12.072965	1.656589
-82.798347	4.384644	1.661594
-82.907642	11.010121	1.666598
-83.095844	2.135644	1.671603
-82.906435	-13.428234	1.676608
-82.792218	2.559433	1.681613
-82.897723	9.190597	1.686618
-83.357638	-6.575428	1.691622
-84.287731	10.942593	1.696627
-84.446885	12.656464	1.701632
-84.496701	0.363046	1.706637
-84.724463	-3.804925	1.711642
-84.777947	16.598913	1.716646
-85.261546	0.008864	1.721651
-85.795958	-5.679949	1.726656
-86.019837	4.705295	1.731661
-85.996723	2.280358	1.736666
-85.753893	-14.411085	1.741670
-86.242119	1.556882	1.746675
-87.072729	22.257054	1.751680
-87.558560	3.632312	1.756685
-88.028545	-2.922899	1.761690
-87.500152	10.338029	1.766694
-87.642854	-1.060019	1.771699
-87.764579	2.374355	1.776704
-87.828138	1.008201	1.781709
-88.285300	15.892262	1.786714
-88.451984	-5.461566	1.791718
-89.135475	4.982373	1.796723
-89.467910	10.959240	1.801728
-89.271944	-3.374831	1.806733
-89.782815	1.261336	1.811738
-89.751092	5.905491	1.816742
-90.442125	15.013642	1.821747
-90.886408	6.882657	1.826752
-90.601449	0.740000	1.831757
-91.225252	28.672526	1.836762
-91.255411	6.394201	1.841766
-91.257692	-14.384553	1.846771
-91.536024	2.530938	1.851776
-92.053200	12.262007	1.856781
-92.489580	7.169183	1.861786
-92.540672	-7.018109	1.866790
-92.478911	7.345748	1.871795
-93.209552	3.371171	1.876800
-93.653287	3.041873	1.881805
-94.022737	12.757603	1.886810
-94.171073	13.097822	1.891814
-94.426320	-1.445187	1.896819
-94.255613	5.563021	1.901824
-94.294788	9.716591	1.906829
-94.686938	7.853511	1.911834
-94.487803	-1.394429	1.916838
-94.820103	9.822167	1.921843
-95.629414	14.915757	1.926848
-95.984657	-3.272249	1.931853
-96.382935	0.963060	1.936858
-96.558332	-5.260458	1.941862
-96.347677	5.387477	1.946867
-96.515849	10.244401	1.951872
-96.978457	-8.087042	1.956877
-97.664390	1.958673	1.961882
-97.902486	18.584024	1.966886
-97.821969	13.464762	1.971891
-97.990837	0.862138	1.976896
-97.919783	-7.158591	1.981901
-98.088313	12.610628	1.986906
-98.669470	-2.322323	1.991910
-98.949475	7.569106	1.996915
-99.354101	9.576846	2.006912
-99.299393	9.854517	2.016909
-98.224742	3.611706	2.026906
-98.086414	7.295827	2.036902
-97.795248	-0.984550	2.046899
-96.850392	15.547660	2.056896
-96.692916	-8.498800	2.066893
-96.077765	14.031587	2.076890
-95.226383	-5.529555	2.086886
-95.240479	-1.696287	2.096883
-94.494301	13.478643	2.106880
-93.539981	3.554047	2.116877
-93.546612	4.068141	2.126874
-93.398277	6.660859	2.136870
-92.207367	10.054274	2.146867
-91.957710	5.542184	2.156864
-91.830947	14.609505	2.166861
-90.657669	8.610854	2.176858
-90.540390	3.279402	2.186854
-90.275857	-7.465173	2.196851
-89.394965	7.266326	2.206848
-89.134288	-3.067713	2.216845
-88.504544	12.099989	2.226842
-87.613945	2.867056	2.236838
-87.139660	-0.558528	2.246835
-87.306008	-4.205962	2.256832
-86.737519	3.722603	2.266829
-86.360168	11.623498	2.276826
-84.892481	-4.338320	2.286822
-85.026476	7.568716	2.296819
-84.353370	6.293129	2.306816
-84.229053	13.959776	2.316813
-83.500305	2.870209	2.326810
-82.790231	2.815655	2.336806
-82.364915	2.313017	2.346803
-82.049481	21.561775	2.356800
-81.054150	10.026638	2.366797
-80.838131	13.026668	2.376794
-80.808815	0.316188	2.386790
-80.255561	0.991003	2.396787
-79.707075	1.538301	2.406784
-78.736736	10.306987	2.416781
-78.288078	-2.527317	2.426778
-78.362068	14.045170	2.436774
-77.541084	-9.517328	2.446771
-76.664853	2.467901	2.456768
-76.760083	3.586997	2.466765
-75.597070	5.307584	2.476762
-75.111209	-2.500048	2.486758
-75.258434	-2.208759	2.496755
-74.657516	14.195199	2.506752
-73.734410	5.374698	2.516749
-73.461878	-3.384902	2.526746
-72.902904	17.432991	2.536742
-71.902228	10.029885	2.546739
-71.935616	3.127772	2.556736
-71.997955	14.192498	2.566733
-71.168139	2.872289	2.576730
-70.576615	10.831822	2.586726
-69.494874	11.386012	2.596723
-68.947193	13.207108	2.606720
-68.619077	8.164881	2.616717
-68.554404	-0.246473	2.626714
-68.505530	9.206583	2.636710
-67.418361	-2.599244	2.646707
-67.007882	3.451415	2.656704
-66.290973	8.172832	2.666701
-65.730600	-5.063661	2.676698
-65.821411	9.812630	2.686694
-65.012097	0.825246	2.696691
-64.403154	4.805741	2.706688
-63.965110	6.510725	2.716685
-63.268082	11.000945	2.726682
-62.532444	10.709560	2.736678
-62.487664	11.021565	2.746675
-62.373141	15.968471	2.756672
-61.156744	-1.337787	2.766669
-61.096598	21.413932	2.776666
-60.141832	4.702249	2.786662
-59.489863	14.500312	2.796659
-59.252165	12.832060	2.806656
-59.042524	-1.638114	2.816653
-58.888208	9.205905	2.826650
-57.715202	-0.510860	2.836646
-57.237626	6.870329	2.846643
-57.033081	4.280979	2.856640
-56.011048	-3.686179	2.866637
-56.048828	13.646698	2.876634
-55.852213	7.407654	2.886630
-55.151849	8.811888	2.896627
-54.386005	1.497179	2.906624
-53.405878	1.731946	2.916621
-53.146001	-11.463969	2.926618
-53.122416	16.807622	2.936614
-52.557465	-1.382747	2.946611
-51.688717	4.873680	2.956608
-51.766554	15.429332	2.966605
-51.009822	4.037145	2.976602
-50.046728	0.053318	2.986598
-49.662679	8.483317	2.996595
-49.653741	12.584900	3.006592
-48.512155	3.566803	3.016589
-48.469090	9.041304	3.026586
-48.090162	10.206789	3.036582
-47.047357	-4.848509	3.046579
-46.827042	11.853232	3.056576
-46.593119	0.264861	3.066573
-46.333701	3.126748	3.076570
-45.206074	3.781613	3.086566
-44.723826	-2.896360	3.096563
-44.184137	8.277678	3.106560
-43.725834	5.587227	3.116557
-43.491814	8.566702	3.126554
-43.061696	25.560228	3.136550
-41.878832	3.312215	3.146547
-41.768107	5.402377	3.156544
-41.584125	-4.055921	3.166541
-40.794358	9.714196	3.176538
-40.268453	-2.015963	3.186534
-39.755740	6.243825	3.196531
-39.572253	3.614890	3.206528
-38.825666	-1.916765	3.216525
-38.621374	3.264407	3.226522
-37.443282	13.236383	3.236518
-36.785350	-7.291770	3.246515
-36.762993	7.816603	3.256512
-36.701525	14.512442	3.266509
-36.096445	-2.040797	3.276506
-35.104929	-2.271248	3.286502
-34.937157	7.405536	3.296499
-34.295352	8.448166	3.306496
-33.706094	6.926770	3.316493
-33.470581	0.948970	3.326490
-32.736417	-4.905293	3.336486
-32.076451	-0.027391	3.346483
-31.851921	1.365203	3.356480
-31.695993	5.648137	3.366477
-30.670322	4.553023	3.376474
-30.015815	-0.513410	3.386470
-29.877733	4.588723	3.396467
-29.306917	11.525742	3.406464
-29.057294	11.361793	3.416461
-28.772350	-2.664008	3.426458
-27.555294	-4.934823	3.436454
-27.186152	-5.180157	3.446451
-26.942493	9.132784	3.456448
-26.271824	-5.049605	3.466445
-25.738287	6.581976	3.476442
-25.845065	6.285800	3.486438
-24.408768	3.179788	3.496435
-24.007644	-3.298693	3.506432
-23.563671	11.328133	3.516429
-23.800551	-7.073450	3.526426
-22.925175	11.750706	3.536422
-22.243430	4.156147	3.546419
-22.017491	-4.240769	3.556416
-20.945915	4.512581	3.566413
-20.838534	5.933425	3.576410
-20.531818	-0.125281	3.586406
-19.420463	11.373679	3.596403
-19.122141	7.803434	3.606400
-18.997581	2.385042	3.616397
-18.214467	19.361717	3.626394
-17.055898	4.760990	3.636390
-17.257357	3.356931	3.646387
-17.455114	-1.418428	3.656384
-16.522555	3.733759	3.666381
-15.886097	0.510824	3.676378
-15.064265	6.498747	3.686374
-14.223762	15.545715	3.696371
-14.421610	8.024804	3.706368
-14.324120	7.167825	3.716365
-13.427583	21.189568	3.726362
-12.816467	4.571220	3.736358
-12.108173	19.817234	3.746355
-11.413071	13.479313	3.756352
-10.878856	10.403849	3.766349
-11.084082	11.495885	3.776346
-10.607089	0.772191	3.786342
-9.617955	6.936333	3.796339
-9.666293	0.275122	3.806336
-8.292847	7.209884	3.816333
-7.824696	16.292014	3.826330
-7.702767	-6.236199	3.836326
-7.728327	10.158701	3.846323
-6.672763	11.327837	3.856320
-6.037209	5.693435	3.866317
-5.959359	3.577200	3.876314
-5.450892	2.117753	3.886310
-4.338366	15.511959	3.896307
-4.183188	-2.378485	3.906304
-4.130108	8.088961	3.916301
-3.376743	-2.358899	3.926298
-3.299207	13.913975	3.936294
-2.765688	25.684945	3.946291
-2.034045	41.120916	3.956288
-1.373958	48.557906	3.966285
-1.223118	68.908092	3.976282
-0.707247	69.367154	3.986278
-0.269469	102.751182	3.996275
0.000000	124.217371	4.001280
0.247856	119.257153	4.006285
-0.006215	114.525978	4.011290
0.314135	133.571704	4.016294
0.597314	162.619357	4.021299
0.702182	147.505688	4.026304
0.817449	167.108667	4.031309
0.419901	168.935835	4.036314
0.791870	154.811935	4.041318
0.931035	153.858542	4.046323
0.901437	161.997770	4.051328
0.852622	177.851587	4.056333
0.827218	206.150020	4.061338
1.188397	194.640925	4.066342
1.444021	182.384843	4.071347
1.213302	188.908958	4.076352
1.068249	178.398554	4.081357
0.868384	166.285551	4.086362
0.975935	196.300938	4.091366
1.020078	203.236842	4.096371
1.337665	177.916686	4.101376
1.209362	185.472392	4.106381
1.190959	206.356441	4.111386
1.121585	185.319077	4.116390
1.237611	209.203255	4.121395
1.319456	215.236627	4.126400
1.320624	204.872133	4.131405
1.114372	210.102185	4.136410
1.150922	198.196607	4.141414
1.183434	209.340540	4.146419
1.505197	206.442824	4.151424
1.438588	184.409164	4.156429
1.175602	194.143031	4.161434
1.348769	209.391794	4.166438
1.081565	214.016560	4.171443
1.467327	197.844503	4.176448
1.151055	188.647779	4.181453
0.746195	200.912894	4.186458
0.931578	205.320026	4.191462
1.345619	204.119669	4.196467
1.404023	204.782532	4.201472
1.491178	212.674619	4.206477
1.347307	205.803703	4.211482
1.608857	200.222878	4.216486
1.547637	210.912151	4.221491
1.180032	209.536144	4.226496
1.538873	207.319771	4.231501
1.268134	212.507210	4.236506
1.467548	200.448251	4.241510
1.574640	203.048384	4.246515
1.552836	196.823364	4.251520
1.412350	215.809807	4.256525
1.172515	238.700965	4.261530
1.568655	226.290353	4.266534
1.611513	223.675081	4.271539
2.092560	243.617824	4.276544
1.856309	237.439077	4.281549
1.592012	218.810287	4.286554
1.598652	198.556918	4.291558
1.365787	217.276597	4.296563
1.589642	232.392219	4.301568
1.614486	222.251577	4.306573
1.692443	244.079392	4.311578
1.662049	249.591529	4.316582
1.752414	236.009003	4.321587
1.661642	241.002859	4.326592
1.758518	238.958013	4.331597
1.527425	229.756264	4.336602
1.461226	245.116434	4.341606
1.383110	241.156072	4.346611
1.382848	230.721461	4.351616
1.567992	242.839392	4.356621
1.360895	258.932429	4.361626
2.051703	243.442764	4.366630
1.474134	231.164941	4.371635
1.893914	253.215255	4.376640
2.109353	270.861916	4.381645
1.800419	270.989754	4.386650
1.876797	245.698028	4.391654
1.694866	243.464573	4.396659
1.869390	262.090449	4.401664
2.268603	254.291362	4.406669
2.220970	256.533927	4.411674
2.037215	246.521554	4.416678
1.925803	250.205337	4.421683
1.850692	235.304807	4.426688
1.991478	231.895519	4.431693
1.819654	258.752524	4.436698
2.266570	251.508042	4.441702
1.913055	239.001023	4.446707
1.959623	228.529179	4.451712
1.968773	245.999685	4.456717
2.188714	261.298578	4.461722
2.166729	261.735113	4.466726
2.277570	247.795740	4.471731
2.175403	247.054558	4.476736
1.706809	241.523252	4.481741
1.978907	262.446575	4.486746
2.554766	256.294215	4.491750
2.253577	245.004038	4.496755
2.133660	239.852119	4.501760
2.013622	254.049564	4.506765
1.910802	266.118130	4.511770
2.119872	254.122443	4.516774
2.110549	247.514759	4.521779
1.976867	266.412245	4.526784
2.124862	283.386440	4.531789
2.173657	261.233965	4.536794
2.447812	253.167791	4.541798
1.994128	259.863214	4.546803
2.111281	267.984265	4.551808
2.317369	266.578260	4.556813
1.837197	257.824476	4.561818
2.120806	256.835566	4.566822
1.959556	273.101171	4.571827
2.014401	265.739469	4.576832
2.393122	289.628205	4.581837
2.359417	304.308908	4.586842
2.648526	295.628133	4.591846
2.629589	302.627874	4.596851
2.382378	284.622198	4.601856
2.356970	290.565601	4.606861
2.209266	280.237298	4.611866
2.579852	294.409538	4.616870
2.560476	303.991943	4.621875
2.270929	298.381507	4.626880
2.363257	287.257104	4.631885
2.435528	299.492577	4.636890
2.596334	302.168293	4.641894
2.670617	305.604872	4.646899
2.669266	290.432459	4.651904
2.768016	299.283796	4.656909
2.792479	299.624170	4.661914
2.702941	267.288676	4.666918
2.375200	270.993515	4.671923
2.172177	282.829865	4.676928
2.919822	294.310940	4.681933
2.893012	296.309173	4.686938
2.775789	284.837832	4.691942
2.691937	275.194248	4.696947
2.137679	272.635224	4.701952
2.671751	284.116072	4.706957
2.980784	301.788537	4.711962
2.756528	293.404789	4.716966
2.714343	310.072870	4.721971
2.800902	312.480500	4.726976
2.795492	290.359235	4.731981
2.677081	276.216231	4.736986
2.667956	286.238477	4.741990
2.568046	304.119195	4.746995
2.453837	297.025719	4.752000
2.478398	311.910768	4.757005
2.728534	303.502185	4.762010
2.739774	288.417857	4.767014
2.616281	307.850255	4.772019
2.559645	313.511566	4.777024
2.529296	291.162796	4.782029
2.738734	307.041840	4.787034
2.555455	306.850307	4.792038
2.811076	305.145005	4.797043
2.945705	313.940407	4.802048
3.054885	325.198715	4.807053
2.893615	353.312590	4.812058
2.885927	335.602773	4.817062
2.801337	329.631537	4.822067
3.116438	332.041750	4.827072
3.385783	335.097875	4.832077
3.144969	336.148551	4.837082
2.366365	307.104484	4.842086
2.833584	321.170419	4.847091
3.031575	340.337935	4.852096
2.763859	341.900699	4.857101
2.703594	336.449359	4.862106
3.118521	320.815112	4.867110
3.002467	338.877584	4.872115
2.978107	330.775270	4.877120
2.920152	340.350559	4.882125
2.776749	342.033451	4.887130
2.793839	337.252365	4.892134
2.697647	345.026650	4.897139
2.815642	374.873133	4.902144
3.381829	357.183875	4.907149
3.113176	356.970049	4.912154
3.139868	369.266577	4.917158
3.507624	354.188278	4.922163
3.157331	362.032677	4.927168
3.483963	381.792183	4.932173
3.231141	385.063835	4.937178
3.500689	355.869648	4.942182
3.622602	364.446802	4.947187
3.217371	360.655291	4.952192
3.103540	367.364047	4.957197
2.869046	368.423349	4.962202
3.193638	364.439121	4.967206
3.290456	364.719103	4.972211
3.233111	363.148968	4.977216
3.218535	370.248345	4.982221
3.089222	372.303084	4.987226
3.343159	367.081056	4.992230
3.260294	369.677489	4.997235
3.161000	361.388175	5.002240
3.599717	364.974269	5.007245
3.139782	363.567930	5.012250
3.540723	359.542873	5.017254
3.441265	363.321580	5.022259
3.588605	370.109896	5.027264
3.570429	367.330770	5.032269
3.429585	367.370853	5.037274
3.187837	366.002740	5.042278
3.568887	365.922644	5.047283
3.470603	381.019042	5.052288
3.589435	391.389747	5.057293
3.432825	371.553773	5.062298
3.527312	376.642638	5.067302
3.831330	405.431811	5.072307
3.518300	404.412456	5.077312
3.813435	384.367552	5.082317
3.760252	381.282086	5.087322
3.763275	370.342450	5.092326
3.569217	383.286495	5.097331
3.474743	368.013581	5.102336
3.910922	356.280469	5.107341
3.698564	384.172598	5.112346
3.647469	385.910183	5.117350
3.485826	377.533798	5.122355
3.631729	385.221239	5.127360
3.827114	394.284145	5.132365
3.499381	393.501017	5.137370
3.682420	396.352910	5.142374
3.932403	399.997034	5.147379
3.788341	415.773220	5.152384
3.965437	391.851602	5.157389
3.833849	399.270120	5.162394
3.955357	407.183661	5.167398
3.917530	405.428784	5.172403
3.906650	401.179081	5.177408
4.159851	406.337219	5.182413
3.778404	391.424123	5.187418
3.631908	372.873636	5.192422
3.940253	385.202947	5.197427
3.580573	414.616362	5.202432
4.073953	404.701121	5.207437
3.563123	407.891119	5.212442
3.974962	408.759271	5.217446
3.962594	404.209331	5.222451
3.833811	405.140384	5.227456
4.435541	412.187752	5.232461
3.872812	416.385436	5.237466
4.015836	395.212951	5.242470
4.086962	407.268371	5.247475
3.946684	418.589279	5.252480
4.028298	418.267456	5.257485
3.453903	414.587638	5.262490
3.838750	392.782615	5.267494
4.052879	409.861933	5.272499
3.400088	413.796411	5.277504
4.234953	403.344520	5.282509
3.991710	418.616040	5.287514
3.986217	414.510259	5.292518
3.927862	416.066054	5.297523
4.239797	432.859729	5.302528
4.271647	436.063338	5.307533
4.291919	426.141131	5.312538
4.478322	432.203183	5.317542
4.462995	443.636242	5.322547
4.467142	427.160231	5.327552
4.541991	399.713431	5.332557
4.347183	399.416275	5.337562
4.448120	419.332096	5.342566
4.525371	410.927756	5.347571
4.302948	410.305679	5.352576
4.229089	395.102627	5.357581
4.156126	402.180395	5.362586
4.257686	415.721366	5.367590
4.316457	426.371527	5.372595
4.107404	422.423778	5.377600
4.364786	399.845295	5.382605
3.994073	405.403072	5.387610
4.170997	400.590226	5.392614
4.142932	412.795316	5.397619
4.329784	430.953642	5.402624
4.685872	447.294935	5.407629
4.251365	452.717864	5.412634
4.641710	440.473273	5.417638
4.337357	449.945518	5.422643
4.390132	442.526265	5.427648
4.576451	427.313135	5.432653
4.584656	442.063497	5.437658
4.637742	438.646756	5.442662
4.512072	429.111099	5.447667
4.376335	433.231223	5.452672
4.327475	443.082768	5.457677
4.525596	458.542908	5.462682
4.385359	449.355607	5.467686
4.360280	437.869615	5.472691
4.074240	439.399508	5.477696
4.421901	456.050183	5.482701
4.102675	458.348116	5.487706
4.564783	445.345188	5.492710
4.650403	454.288654	5.497715
4.625617	463.760581	5.502720
4.919016	471.904998	5.507725
4.782419	480.520793	5.512730
4.747569	457.006596	5.517734
4.514856	450.889917	5.522739
4.576456	472.587290	5.527744
4.824534	468.898110	5.532749
4.583513	472.495936	5.537754
4.833891	491.836499	5.542758
4.631973	486.659673	5.547763
4.906031	485.774133	5.552768
4.862082	479.239349	5.557773
4.670211	475.450531	5.562778
4.704429	462.607181	5.567782
4.733844	473.014618	5.572787
4.701660	476.446337	5.577792
4.898472	483.347866	5.582797
4.738546	478.436177	5.587802
5.007383	466.934838	5.592806
4.798399	476.615371	5.597811
4.656585	497.930195	5.602816
4.982132	482.600482	5.607821
4.786319	467.853538	5.612826
4.928160	475.947536	5.617830
5.029218	481.626157	5.622835
4.641390	485.002414	5.627840
4.999061	467.000738	5.632845
4.802582	475.624650	5.637850
4.749343	485.401677	5.642854
4.744637	479.783563	5.647859
5.210330	489.782917	5.652864
5.476240	482.076870	5.657869
5.054787	484.968696	5.662874
4.660336	485.920177	5.667878
4.845220	487.256441	5.672883
5.014985	503.833675	5.677888
4.942229	514.432041	5.682893
4.763560	505.334612	5.687898
4.887916	485.296293	5.692902
5.007576	495.372466	5.697907
4.684029	506.131239	5.702912
5.238355	508.659491	5.707917
4.906801	492.258911	5.712922
5.009252	489.116333	5.717926
5.114684	514.361427	5.722931
5.081408	541.808840	5.727936
5.301783	527.386869	5.732941
5.274521	522.082619	5.737946
5.239793	529.048672	5.742950
5.139120	539.776952	5.747955
5.210745	546.604888	5.752960
5.450700	541.808514	5.757965
5.120025	531.741707	5.762970
5.339253	535.029792	5.767974
5.585823	551.195646	5.772979
4.967811	539.801839	5.777984
5.269141	529.860052	5.782989
5.250307	541.813644	5.787994
5.693125	536.321713	5.792998
5.577388	528.344784	5.798003
5.498146	543.339842	5.803008
5.788670	547.855871	5.808013
5.396647	534.904737	5.813018
5.623530	515.412821	5.818022
5.810983	541.928914	5.823027
5.861360	545.492019	5.828032
5.426906	511.856285	5.833037
5.286634	520.610819	5.838042
5.501099	505.878904	5.843046
5.537084	497.066320	5.848051
5.044927	519.235855	5.853056
5.443543	511.393825	5.858061
5.745714	523.818280	5.863066
5.524774	536.599094	5.868070
5.506055	537.199052	5.873075
5.485366	528.643820	5.878080
5.732204	530.669764	5.883085
5.545474	539.535765	5.888090
5.528097	563.657497	5.893094
5.653682	546.868301	5.898099
5.447029	543.751933	5.903104
5.707042	534.121106	5.908109
5.831344	556.970815	5.913114
5.644837	535.789456	5.918118
5.442279	533.497810	5.923123
5.618599	527.366284	5.928128
5.832173	540.179470	5.933133
5.462460	544.217740	5.938138
5.662480	544.664159	5.943142
5.451447	549.781472	5.948147
5.246272	529.094578	5.953152
5.576545	544.941275	5.958157
5.666044	573.563094	5.963162
5.537949	588.463675	5.968166
5.656695	569.898220	5.973171
5.611349	588.159521	5.978176
5.728054	568.214103	5.983181
5.795865	559.098107	5.988186
6.073560	561.010146	5.993190
5.803459	582.150960	5.998195
5.679889	586.363818	6.003200
5.500884	567.551325	6.008205
5.805783	568.496842	6.013210
5.776176	579.523657	6.018214
5.952784	585.733884	6.023219
6.220889	590.676933	6.028224
6.280130	588.797185	6.033229
5.851589	574.631167	6.038234
5.788316	566.706909	6.043238
5.982884	570.941767	6.048243
6.150457	579.343102	6.053248
6.130025	574.870798	6.058253
5.917781	577.669668	6.063258
6.130767	565.818797	6.068262
5.862293	568.522291	6.073267
5.989179	572.442988	6.078272
5.915181	556.170344	6.083277
5.944558	572.704559	6.088282
5.952594	588.669956	6.093286
6.118138	567.561186	6.098291
5.914950	559.513458	6.103296
6.062575	556.929155	6.108301
5.780553	570.575378	6.113306
5.837073	577.290109	6.118310
5.683600	576.655841	6.123315
5.602032	592.298669	6.128320
6.265586	572.448337	6.133325
5.759923	581.535855	6.138330
5.882290	572.497844	6.143334
5.923796	575.765094	6.148339
5.724940	565.307930	6.153344
6.020158	577.088805	6.158349
6.092714	579.630686	6.163354
5.920198	563.125816	6.168358
5.926763	565.667749	6.173363
5.763705	574.125394	6.178368
5.990341	573.216611	6.183373
6.037782	588.256973	6.188378
5.889699	580.414000	6.193382
5.941267	565.242041	6.198387
5.770372	572.156528	6.203392
6.208266	582.112594	6.208397
5.953858	571.490094	6.213402
5.713322	564.127047	6.218406
5.873420	564.685421	6.223411
5.711274	575.275120	6.228416
6.180975	564.830295	6.233421
6.151371	575.853062	6.238426
5.924848	575.370355	6.243430
5.663411	558.786074	6.248435
5.467775	574.118638	6.253440
5.762470	568.161086	6.258445
5.953264	569.170837	6.263450
5.755364	552.472282	6.268454
5.549858	573.813816	6.273459
5.908124	604.429868	6.278464
6.009374	600.233397	6.283469
6.041562	608.035925	6.288474
6.184864	612.640423	6.293478
6.406710	576.184513	6.298483
6.249754	569.965793	6.303488
6.174839	582.237160	6.308493
5.899633	592.264117	6.313498
6.150563	581.062092	6.318502
6.159862	555.503045	6.323507
5.716428	577.638568	6.328512
5.973109	568.265450	6.333517
6.108710	567.925824	6.338522
6.038184	561.407432	6.343526
6.306290	566.029568	6.348531
5.815457	581.716734	6.353536
6.275755	555.172133	6.358541
5.991951	569.601432	6.363546
6.039663	569.856683	6.368550
6.178321	565.524711	6.373555
5.514308	541.406349	6.378560
6.049502	550.564423	6.383565
5.955913	558.226715	6.388570
6.026936	579.383266	6.393574
5.968971	550.638909	6.398579
5.500035	553.275990	6.403584
5.970863	555.178407	6.408589
6.250315	562.415533	6.413594
6.018634	561.442407	6.418598
6.019641	550.042678	6.423603
5.914975	550.209663	6.428608
6.050606	553.658751	6.433613
5.842857	553.801239	6.438618
5.498755	535.646041	6.443622
6.050228	533.555332	6.448627
5.793040	555.575800	6.453632
5.855233	562.000545	6.458637
6.164998	568.670660	6.463642
5.857972	570.687513	6.468646
6.302504	558.446699	6.473651
5.730445	558.882400	6.478656
5.853709	572.443598	6.483661
5.676663	550.664223	6.488666
6.226599	555.695147	6.493670
6.072924	552.810628	6.498675
5.784301	545.472601	6.503680
6.070462	525.293354	6.508685
5.841045	551.557250	6.513690
6.016941	545.430029	6.518694
5.887486	539.391349	6.523699
5.777634	533.039970	6.528704
5.783843	532.926522	6.533709
5.912616	551.556563	6.538714
6.045699	579.631384	6.543718
6.062890	575.655283	6.548723
5.596839	561.461543	6.553728
5.965285	560.042098	6.558733
5.664349	567.846286	6.563738
6.133697	575.825052	6.568742
6.086670	581.619925	6.573747
6.168355	580.873105	6.578752
6.126593	561.441409	6.583757
5.924563	547.167156	6.588762
6.177065	535.500761	6.593766
5.883544	540.055888	6.598771
5.600852	547.690136	6.603776
6.004978	535.654104	6.608781
6.112945	530.226191	6.613786
5.975704	535.344820	6.618790
5.840412	550.608003	6.623795
5.700657	547.717436	6.628800
5.708084	539.050123	6.633805
5.668470	552.779585	6.638810
5.843742	552.388814	6.643814
6.377012	550.088916	6.648819
5.848446	551.710295	6.653824
6.042140	551.520190	6.658829
6.021149	556.200455	6.663834
5.838416	540.800589	6.668838
5.944970	522.178903	6.673843
5.713952	544.480324	6.678848
5.905622	541.605228	6.683853
6.042063	544.464948	6.688858
5.246144	541.634871	6.693862
5.828946	535.520515	6.698867
5.673635	569.935502	6.703872
5.875723	569.484761	6.708877
5.889663	568.517805	6.713882
5.481303	553.166458	6.718886
5.793966	560.875064	6.723891
6.011874	586.289319	6.728896
6.112359	565.042935	6.733901
6.024154	554.325801	6.738906
5.932397	566.239376	6.743910
6.075600	576.423183	6.748915
5.346065	591.845375	6.753920
5.946809	572.921974	6.758925
6.183004	566.476305	6.763930
5.851782	563.304953	6.768934
6.136120	566.973429	6.773939
5.912236	580.380793	6.778944
6.028427	568.880139	6.783949
6.126064	564.408057	6.788954
6.214047	578.078079	6.793958
6.204475	576.956577	6.798963
5.824811	565.084672	6.803968
5.670993	558.583991	6.808973
5.999640	571.145571	6.813978
5.833129	570.140367	6.818982
6.063079	560.377370	6.823987
5.988390	576.779135	6.828992
5.956941	578.457758	6.833997
6.005638	575.621178	6.839002
5.904267	575.906392	6.844006
6.186535	569.933332	6.849011
5.636672	561.016381	6.854016
5.898071	569.730905	6.859021
6.150078	569.035944	6.864026
5.675589	562.196715	6.869030
6.289804	577.809188	6.874035
5.936845	567.961294	6.879040
5.972806	544.810522	6.884045
5.763591	540.465707	6.889050
5.693731	567.439381	6.894054
5.905800	582.853443	6.899059
6.009121	580.310687	6.904064
5.632228	558.170518	6.909069
6.069311	562.966073	6.914074
5.969708	583.254106	6.919078
6.324977	570.812877	6.924083
5.855377	554.010063	6.929088
5.776771	553.983730	6.934093
5.938530	553.942042	6.939098
6.001389	584.594243	6.944102
6.064487	579.425085	6.949107
5.285630	562.242764	6.954112
5.777760	566.368766	6.959117
5.937167	570.530022	6.964122
6.077258	560.832679	6.969126
6.111114	567.066290	6.974131
6.081827	568.024415	6.979136
5.999384	561.673723	6.984141
6.129215	575.187571	6.989146
5.933529	575.261478	6.994150
6.032255	549.013002	6.999155
5.565197	538.263092	7.004160
6.141179	546.955804	7.009165
5.805767	557.161081	7.014170
5.990474	564.517644	7.019174
5.909074	547.003349	7.024179
5.700584	560.727185	7.029184
6.056022	562.085384	7.034189
5.947090	559.771357	7.039194
6.108889	564.780107	7.044198
5.834664	554.793135	7.049203
5.641624	547.025480	7.054208
6.288344	583.028794	7.059213
5.986818	574.475651	7.064218
5.685266	572.671112	7.069222
5.724745	559.524256	7.074227
5.898677	582.886078	7.079232
5.914123	583.471414	7.084237
5.948133	564.873306	7.089242
5.383620	572.405670	7.094246
6.191990	572.403721	7.099251
5.929236	581.135617	7.104256
6.152096	564.865698	7.109261
6.029482	559.962121	7.114266
5.775846	570.851145	7.119270
6.059908	574.616936	7.124275
5.714321	589.697783	7.129280
6.012988	563.986927	7.134285
6.386931	566.378181	7.139290
5.576620	582.795369	7.144294
6.084457	575.902712	7.149299
5.874431	576.299796	7.154304
6.068672	564.737711	7.159309
6.087878	569.210883	7.164314
5.974117	566.226443	7.169318
6.181302	554.539703	7.174323
5.556901	557.293825	7.179328
5.906776	561.010757	7.184333
6.026793	546.908699	7.189338
5.703177	537.324497	7.194342
5.915578	541.693919	7.199347
5.733483	566.217939	7.204352
6.019718	570.204738	7.209357
6.454856	556.224812	7.214362
5.985886	558.592094	7.219366
6.082841	548.125714	7.224371
5.990689	544.984407	7.229376
6.089937	554.043762	7.234381
5.889853	549.281037	7.239386
5.918185	541.203742	7.244390
6.081639	540.509704	7.249395
5.746206	557.777075	7.254400
5.699404	547.896751	7.259405
5.782086	543.084045	7.264410
5.823566	533.931673	7.269414
5.777105	540.147274	7.274419
5.620987	563.966097	7.279424
5.962747	560.171840	7.284429
6.047968	562.054129	7.289434
5.926664	552.929534	7.294438
6.031272	556.103881	7.299443
5.788858	564.364020	7.304448
5.828978	548.648931	7.309453
5.309296	537.131152	7.314458
5.617724	572.658922	7.319462
6.423716	571.471406	7.324467
5.972223	574.830778	7.329472
6.381883	577.091834	7.334477
6.048874	570.239974	7.339482
5.825163	560.066493	7.344486
5.908999	537.212055	7.349491
5.783117	564.413095	7.354496
6.021434	568.169280	7.359501
6.208761	554.943934	7.364506
5.687178	547.582748	7.369510
5.862553	545.758983	7.374515
5.892909	569.114028	7.379520
6.022705	546.265299	7.384525
5.785572	540.774158	7.389530
5.472834	568.377300	7.394534
5.803931	588.406041	7.399539
6.006182	582.278198	7.404544
6.106444	569.037734	7.409549
6.133991	576.843675	7.414554
5.956865	596.713440	7.419558
6.022827	580.816379	7.424563
5.883605	569.769990	7.429568
6.025858	577.560133	7.434573
6.015514	567.706426	7.439578
5.963843	563.288416	7.444582
5.833780	553.379034	7.449587
5.901614	558.922796	7.454592
5.696935	572.622334	7.459597
5.899015	554.614010	7.464602
6.107821	576.888272	7.469606
6.245313	567.295133	7.474611
5.965791	558.625805	7.479616
5.870219	567.694871	7.484621
5.913875	542.468435	7.489626
5.590758	531.490835	7.494630
6.030248	542.860252	7.499635
5.733926	558.688678	7.504640
6.234243	565.106526	7.509645
6.123121	541.512664	7.514650
5.701387	549.618349	7.519654
6.020647	548.609818	7.524659
5.553633	537.154659	7.529664
6.028971	549.793689	7.534669
6.023464	547.306312	7.539674
5.694822	545.337859	7.544678
5.953629	576.827057	7.549683
6.160066	572.342419	7.554688
6.221273	557.579552	7.559693
5.996998	559.121347	7.564698
5.386796	553.462000	7.569702
5.757962	553.987960	7.574707
5.964169	577.964450	7.579712
6.134089	573.544147	7.584717
5.996825	570.392138	7.589722
5.734151	567.502053	7.594726
6.286254	550.402554	7.599731
5.860849	554.167498	7.604736
5.926863	550.969076	7.609741
6.069192	531.491803	7.614746
6.047752	547.074633	7.619750
6.385504	546.800349	7.624755
5.993642	546.699709	7.629760
6.032408	550.605271	7.634765
5.654384	559.888909	7.639770
5.778539	542.390370	7.644774
6.120330	531.523078	7.649779
5.805901	542.520087	7.654784
5.577685	553.548138	7.659789
5.942410	558.404479	7.664794
5.615615	553.318703	7.669798
5.982170	534.318235	7.674803
5.932752	547.251044	7.679808
5.858801	558.380764	7.684813
5.769631	551.361262	7.689818
5.581212	536.910357	7.694822
5.788917	559.893867	7.699827
5.701503	588.867435	7.704832
5.970705	574.577729	7.709837
6.111944	565.056183	7.714842
5.912807	572.914281	7.719846
6.252932	581.501764	7.724851
5.969214	578.871739	7.729856
6.047641	578.587729	7.734861
6.104506	586.056680	7.739866
5.717465	564.279235	7.744870
5.825901	546.639064	7.749875
5.955186	568.009019	7.754880
6.189908	581.043762	7.759885
5.921851	571.934824	7.764890
6.009586	554.992656	7.769894
6.270852	553.687205	7.774899
6.028001	550.151738	7.779904
6.215561	544.240901	7.784909
6.247180	555.460898	7.789914
5.922958	565.643517	7.794918
6.067634	548.998052	7.799923
6.212016	554.201450	7.804928
5.961346	549.096289	7.809933
6.091915	531.782656	7.814938
5.696250	556.295095	7.819942
6.101025	559.248289	7.824947
5.858944	559.338347	7.829952
5.883510	541.951956	7.834957
6.042894	544.869837	7.839962
6.103834	558.304398	7.844966
6.005504	553.343441	7.849971
5.972203	544.411471	7.854976
6.063089	544.418094	7.859981
6.153737	550.535575	7.864986
6.062773	545.274398	7.869990
5.758760	522.601763	7.874995
5.711520	549.803790	7.880000
5.939237	550.452499	7.885005
6.140412	539.246100	7.890010
6.078679	544.003727	7.895014
5.705744	531.200474	7.900019
5.624084	552.732327	7.905024
5.855473	548.137821	7.910029
5.821520	536.041005	7.915034
5.839435	553.009966	7.920038
5.956700	537.964891	7.925043
6.167889	537.780971	7.930048
5.878246	541.571913	7.935053
6.136218	552.604261	7.940058
6.144973	537.132703	7.945062
6.214186	527.170875	7.950067
5.739232	537.966923	7.955072
5.609082	522.120286	7.960077
5.798980	519.374717	7.965082
5.788444	530.894748	7.970086
5.924396	544.718698	7.975091
5.614047	557.841031	7.980096
5.899618	540.790914	7.985101
6.068009	555.298775	7.990106
5.802145	558.840452	7.995110
6.003311	547.966101	8.000115
6.072638	557.686646	8.005133
6.099518	547.899073	8.010150
6.326055	553.597854	8.015168
6.191511	542.722707	8.020186
5.989825	514.090475	8.025203
5.973664	515.347453	8.030221
5.858986	505.598551	8.035238
5.895286	515.631959	8.040256
5.584457	526.825968	8.045274
6.188150	527.290947	8.050291
5.529687	527.982999	8.055309
5.579930	543.655437	8.060326
5.901110	552.210306	8.065344
5.708483	564.656892	8.070362
5.983254	539.970829	8.075379
5.768735	553.087665	8.080397
5.756715	546.476397	8.085414
5.842379	531.103627	8.090432
5.810534	535.095005	8.095450
6.086271	542.720734	8.100467
6.065660	555.500890	8.105485
6.111210	558.209960	8.110502
6.110480	535.767630	8.115520
5.716257	541.719242	8.120538
5.597155	549.506947	8.125555
6.066940	566.780670	8.130573
6.129889	549.818776	8.135590
6.275852	543.135844	8.140608
6.107227	561.593890	8.145626
6.122989	553.993658	8.150643
6.268262	558.872444	8.155661
6.243257	564.287789	8.160678
6.208601	534.938838	8.165696
6.150330	552.841092	8.170714
6.129860	550.112606	8.175731
6.086536	544.411670	8.180749
5.780164	535.787524	8.185766
6.322548	558.090926	8.190784
5.814524	554.207332	8.195802
5.841995	547.665204	8.200819
6.103476	540.249704	8.205837
6.310669	555.183230	8.210854
6.367688	564.094270	8.215872
6.076929	553.481380	8.220890
5.933183	542.529134	8.225907
6.012578	549.400034	8.230925
5.886243	557.314888	8.235942
6.372974	570.261342	8.240960
6.345887	580.425608	8.245978
6.283162	568.432488	8.250995
6.090322	552.206072	8.256013
5.957575	557.409166	8.261030
6.153277	576.051638	8.266048
6.368980	579.368340	8.271066
6.348233	593.309250	8.276083
6.134787	559.551372	8.281101
6.132927	549.336681	8.286118
6.442683	556.401440	8.291136
5.980320	571.279137	8.296154
6.432546	576.922330	8.301171
6.103306	566.301818	8.306189
6.128522	570.505365	8.311206
6.410405	574.874906	8.316224
6.254821	570.706457	8.321242
6.241836	565.238721	8.326259
6.147138	570.463968	8.331277
5.899454	577.750445	8.336294
6.199532	568.570877	8.341312
5.967715	586.228106	8.346330
6.281794	573.996383	8.351347
6.480165	567.885918	8.356365
6.015182	589.281234	8.361382
6.361500	590.336822	8.366400
6.175308	582.837155	8.371418
6.207935	569.120093	8.376435
6.372493	583.970855	8.381453
6.167765	588.943207	8.386470
6.288167	586.575776	8.391488
6.186753	575.848138	8.396506
6.039741	561.241244	8.401523
6.228831	569.191848	8.406541
6.245308	590.459684	8.411558
6.348317	576.210755	8.416576
6.413261	602.428365	8.421594
6.315829	585.029482	8.426611
6.574324	570.667289	8.431629
6.305414	590.357842	8.436646
6.292638	582.025608	8.441664
6.193441	587.694199	8.446682
6.240624	583.467737	8.451699
6.374774	585.443769	8.456717
6.241854	567.647340	8.461734
6.433274	560.596163	8.466752
6.343678	583.263905	8.471770
6.470231	602.165602	8.476787
6.564712	596.695543	8.481805
6.440070	603.318178	8.486822
6.382640	594.136075	8.491840
6.242516	582.792956	8.496858
6.611855	579.560210	8.501875
6.892252	587.136486	8.506893
6.479691	589.325859	8.511910
6.879141	590.814670	8.516928
6.324060	575.063328	8.521946
6.431188	572.734304	8.526963
6.445637	578.913588	8.531981
6.491812	583.223686	8.536998
6.431878	570.826079	8.542016
6.123250	608.635765	8.547034
6.543879	588.230231	8.552051
6.594641	567.109783	8.557069
6.399850	577.418261	8.562087
6.484061	585.278165	8.567104
6.178266	585.974520	8.572122
6.671950	614.516594	8.577139
6.986993	611.980124	8.582157
6.482611	589.829548	8.587175
6.583340	563.421911	8.592192
6.494679	584.671788	8.597210
6.186131	586.353953	8.602227
6.717969	586.401007	8.607245
6.309210	594.299969	8.612263
6.749852	597.740482	8.617280
6.371348	606.000884	8.622298
6.331518	599.148784	8.627315
6.671618	616.000319	8.632333
6.559923	635.188408	8.637351
6.431004	616.745571	8.642368
6.485485	605.286541	8.647386
6.356290	625.179775	8.652403
6.328620	607.231789	8.657421
6.590893	624.106920	8.662439
6.523664	604.598881	8.667456
6.352874	595.110995	8.672474
6.480704	607.618605	8.677491
6.691325	610.032171	8.682509
6.568733	625.336713	8.687527
6.339050	616.499803	8.692544
6.554289	628.803079	8.697562
6.583484	612.958392	8.702579
6.625117	609.176025	8.707597
6.673136	625.669259	8.712615
7.006397	632.491751	8.717632
7.057541	613.022686	8.722650
6.845776	614.954239	8.727667
6.960945	617.649453	8.732685
6.970299	631.548033	8.737703
6.946377	618.754878	8.742720
6.817404	597.844256	8.747738
6.745820	613.930981	8.752755
6.881325	599.833999	8.757773
6.473502	630.213389	8.762791
6.343144	619.686020	8.767808
6.736446	610.734457	8.772826
6.591712	621.670739	8.777843
6.619448	612.496788	8.782861
6.503848	627.405798	8.787879
6.371623	625.762793	8.792896
6.579607	614.326602	8.797914
6.425803	627.215814	8.802931
6.815792	624.240204	8.807949
6.851314	648.835254	8.812967
7.220555	662.320155	8.817984
7.213966	643.976133	8.823002
6.807391	625.940684	8.828019
6.868818	618.614291	8.833037
6.893084	616.291966	8.838055
6.754682	624.643867	8.843072
7.066552	607.478712	8.848090
6.812470	604.699672	8.853107
7.077533	612.569258	8.858125
6.591595	633.849532	8.863143
6.804724	617.167778	8.868160
6.603482	608.253558	8.873178
7.095901	617.046726	8.878195
7.031122	612.945717	8.883213
6.764604	623.912261	8.888231
6.749385	616.093458	8.893248
6.640336	622.351126	8.898266
6.957644	644.740851	8.903283
7.378898	631.675062	8.908301
7.112850	621.855064	8.913319
6.869459	623.907954	8.918336
7.195328	636.514616	8.923354
6.891666	629.198072	8.928371
6.928701	616.131533	8.933389
6.770538	614.276439	8.938407
6.760258	608.852518	8.943424
6.705092	626.829819	8.948442
6.942561	632.854586	8.953459
7.168425	624.600283	8.958477
6.923548	641.331645	8.963495
6.762691	654.074644	8.968512
6.860255	641.701432	8.973530
6.819564	643.481918	8.978547
7.136289	654.647295	8.983565
6.932780	656.815022	8.988583
7.212119	644.328623	8.993600
7.408052	641.595256	8.998618
6.998221	657.808180	9.003635
6.973354	619.680827	9.008653
6.739061	622.288064	9.013671
6.802574	640.477297	9.018688
6.955862	651.374486	9.023706
7.020333	644.535043	9.028723
7.151673	645.989348	9.033741
7.141298	645.807883	9.038759
7.396058	639.655303	9.043776
7.324578	648.892759	9.048794
7.064616	657.891166	9.053811
7.336152	633.648967	9.058829
7.041882	629.946506	9.063847
6.832801	630.359829	9.068864
7.306637	643.093085	9.073882
6.961826	639.813524	9.078899
7.197657	619.962551	9.083917
7.324589	646.257273	9.088935
7.106600	653.795599	9.093952
7.560201	620.079674	9.098970
6.917942	617.241978	9.103987
7.098318	618.959657	9.109005
6.989746	619.396517	9.114023
7.108813	630.524088	9.119040
7.380958	636.266432	9.124058
7.234077	634.205689	9.129075
6.773854	628.947920	9.134093
6.983911	646.555716	9.139111
7.304357	634.875989	9.144128
7.403545	629.603019	9.149146
7.170211	640.315536	9.154163
7.340527	659.189212	9.159181
7.228215	661.786236	9.164199
6.941196	638.812287	9.169216
7.280250	635.265036	9.174234
7.147960	649.650099	9.179251
7.208293	646.848712	9.184269
7.060163	654.008666	9.189287
6.926408	638.431957	9.194304
7.192675	647.983674	9.199322
7.230812	641.531156	9.204339
7.295898	640.770055	9.209357
7.094746	656.253212	9.214375
6.951209	655.816073	9.219392
6.955588	639.335676	9.224410
6.993827	638.464575	9.229427
7.392613	647.333059	9.234445
7.187368	646.394940	9.239463
7.323050	653.697311	9.244480
7.788927	662.879629	9.249498
7.426188	678.476789	9.254515
7.231394	648.001841	9.259533
7.305243	638.742324	9.264551
7.280293	638.340594	9.269568
7.355228	651.014219	9.274586
7.166284	656.923293	9.279603
7.715227	656.867745	9.284621
7.483037	655.332964	9.289639
7.145073	649.643582	9.294656
7.411469	647.209606	9.299674
7.745515	656.348172	9.304691
7.334121	665.688057	9.309709
7.427895	646.312962	9.314727
7.413017	625.232602	9.319744
7.490151	639.991794	9.324762
7.369853	657.875689	9.329779
7.240029	654.186193	9.334797
7.650377	650.636800	9.339815
7.395167	654.346113	9.344832
7.324036	663.691955	9.349850
7.471929	676.390543	9.354867
7.533070	676.826910	9.359885
7.866111	658.811877	9.364903
7.489956	669.564252	9.369920
7.206240	651.144397	9.374938
7.395802	645.636370	9.379955
7.474796	674.782766	9.384973
7.436309	668.125733	9.389991
7.464133	681.123421	9.395008
7.789241	692.653876	9.400026
7.598773	679.521070	9.405043
7.543607	653.844356	9.410061
7.570477	656.180255	9.415079
7.347533	675.047599	9.420096
7.751845	683.511955	9.425114
7.568782	680.827731	9.430131
7.523071	681.610997	9.435149
7.424504	662.107277	9.440167
7.552066	669.923652	9.445184
7.590365	677.565759	9.450202
7.656322	689.504488	9.455219
7.651162	667.719998	9.460237
7.947512	684.267605	9.465255
7.637334	680.768099	9.470272
7.600735	647.988596	9.475290
7.347943	643.574648	9.480307
7.534550	664.211293	9.485325
7.658366	683.757659	9.490343
7.249447	696.675605	9.495360
7.662176	687.924865	9.500378
7.516138	678.212917	9.505395
7.538489	686.120387	9.510413
7.664021	676.300489	9.515431
7.847598	685.597169	9.520448
7.643709	692.799712	9.525466
7.344196	696.402706	9.530483
7.779301	686.251701	9.535501
7.852412	656.761218	9.540519
7.780656	674.701758	9.545536
7.808600	682.100174	9.550554
7.589505	687.489582	9.555571
7.426483	673.239754	9.560589
7.665400	671.018330	9.565607
7.670031	679.008328	9.570624
7.901086	669.900423	9.575642
7.854489	676.486478	9.580659
7.503112	671.363028	9.585677
7.958430	669.460865	9.590695
7.396271	685.776036	9.595712
7.789521	691.882436	9.600730
7.627676	675.849925	9.605747
7.270645	668.141406	9.610765
8.086894	694.516045	9.615783
7.771116	723.399119	9.620800
7.851726	710.268229	9.625818
7.954188	693.661458	9.630835
8.118732	693.878333	9.635853
8.051253	698.009364	9.640871
8.081734	698.061043	9.645888
8.060602	681.357713	9.650906
8.095445	671.293722	9.655923
7.986086	665.592337	9.660941
7.898901	682.055920	9.665959
7.623805	689.448724	9.670976
7.929208	681.764551	9.675994
8.013179	650.158297	9.681011
7.823452	670.634760	9.686029
7.937576	683.517724	9.691047
7.723270	680.375994	9.696064
7.993964	653.905279	9.701082
7.756437	661.411808	9.706099
7.855034	679.338175	9.711117
8.063975	675.059768	9.716135
7.875318	679.257362	9.721152
8.228587	678.071672	9.726170
8.201419	678.480223	9.731187
7.854515	671.678344	9.736205
8.196377	665.151812	9.741223
8.000953	673.867591	9.746240
8.508942	674.690128	9.751258
7.892681	674.835791	9.756275
7.791769	678.640544	9.761293
8.197043	669.078375	9.766311
7.869632	655.046032	9.771328
8.079117	655.994941	9.776346
8.172432	672.685112	9.781363
7.702463	665.940373	9.786381
7.825240	668.261704	9.791399
7.787255	661.800011	9.796416
7.986364	699.819638	9.801434
8.138179	716.136705	9.806451
8.158837	695.064645	9.811469
8.169431	694.338228	9.816487
8.147022	691.997727	9.821504
8.220301	694.118047	9.826522
8.065393	682.230497	9.831539
8.012789	696.644256	9.836557
8.139745	704.103759	9.841575
8.213358	693.609052	9.846592
8.377467	690.662295	9.851610
8.398130	687.743966	9.856627
7.728047	681.176639	9.861645
7.830806	673.679360	9.866663
7.928479	693.962634	9.871680
8.033975	703.666904	9.876698
8.289077	705.283292	9.881715
8.124812	710.122259	9.886733
8.393894	675.899154	9.891751
8.351927	697.137930	9.896768
8.257628	699.525740	9.901786
8.324877	707.914547	9.906803
8.381447	703.486457	9.911821
8.222184	687.045253	9.916839
8.324316	699.298101	9.921856
8.299519	703.444122	9.926874
8.213955	715.539075	9.931891
8.002367	710.827236	9.936909
8.093347	689.313267	9.941927
8.264920	703.734364	9.946944
8.267468	712.331547	9.951962
8.294212	708.166386	9.956979
8.195346	693.576302	9.961997
8.497502	680.936538	9.967015
8.275114	706.288671	9.972032
8.338330	720.468312	9.977050
8.425840	700.070839	9.982067
8.400137	684.557504	9.987085
8.453844	693.707979	9.992103
8.108199	712.080628	9.997120
8.463109	712.234065	10.002138
8.409051	695.711015	10.007155
8.639643	710.567126	10.012173
8.964634	699.016387	10.017191
8.482290	703.370856	10.022208
8.551473	702.137255	10.027226
8.788077	682.711648	10.032243
8.034081	685.065892	10.037261
8.375858	699.382502	10.042279
8.548796	714.922272	10.047296
8.387613	705.849939	10.052314
8.546309	687.525684	10.057331
8.513572	709.118366	10.062349
8.411943	710.503922	10.067367
8.424120	710.246702	10.072384
8.615305	724.268523	10.077402
8.859783	700.559090	10.082419
7.958612	689.156471	10.087437
8.209079	697.795430	10.092455
8.407200	691.748914	10.097472
8.455139	704.220999	10.102490
8.823849	707.365044	10.107507
8.471175	702.610103	10.112525
8.500741	701.817084	10.117543
8.430897	703.795846	10.122560
8.794319	697.106332	10.127578
8.470777	688.042833	10.132595
8.051268	717.640584	10.137613
8.048266	711.387007	10.142631
8.216612	702.975282	10.147648
8.091870	712.616058	10.152666
8.591461	729.030646	10.157683
8.770947	747.394490	10.162701
8.724892	724.162345	10.167719
8.536032	748.104958	10.172736
8.566260	747.900645	10.177754
8.915692	738.511692	10.182771
8.490488	731.808134	10.187789
8.698012	732.543946	10.192807
8.679832	743.551404	10.197824
8.484771	729.411514	10.202842
8.568670	732.327802	10.207859
8.580460	735.526505	10.212877
8.602847	753.257636	10.217895
8.786730	744.247714	10.222912
8.763758	739.255256	10.227930
8.678529	745.106192	10.232947
8.545769	746.502307	10.237965
8.998067	722.731929	10.242983
8.999025	732.144422	10.248000
8.668416	752.269377	10.253018
9.103873	726.612717	10.258035
8.754487	750.333601	10.263053
9.140642	748.713060	10.268071
9.113225	715.723289	10.273088
9.008816	704.752028	10.278106
8.665165	712.135310	10.283123
8.606024	721.158624	10.288141
8.390481	693.441091	10.293159
8.671709	701.039228	10.298176
8.659103	724.631407	10.303194
8.826082	749.837401	10.308211
8.864604	751.087625	10.313229
9.028602	740.981090	10.318247
8.968644	735.946333	10.323264
8.705575	735.627934	10.328282
8.851770	736.563298	10.333299
8.759898	735.911572	10.338317
8.571057	730.826973	10.343335
8.721448	739.743349	10.348352
8.615642	734.075200	10.353370
8.897629	726.820842	10.358387
9.070064	736.432204	10.363405
8.837967	743.355453	10.368423
8.610626	740.843550	10.373440
8.833454	731.455941	10.378458
8.974313	715.621724	10.383475
9.210463	738.945911	10.388493
9.405558	730.156033	10.393511
9.591624	730.904542	10.398528
9.126508	747.390700	10.403546
9.124782	728.687109	10.408563
9.081403	723.387877	10.413581
9.195738	724.162310	10.418599
9.238588	743.709734	10.423616
9.138773	732.149467	10.428634
9.219573	740.717696	10.433651
8.910260	739.090364	10.438669
9.074241	739.843606	10.443687
9.247319	727.768392	10.448704
9.064561	722.707488	10.453722
8.824731	722.867107	10.458739
8.862710	712.831992	10.463757
8.905243	731.265581	10.468775
8.793780	737.672570	10.473792
8.832959	731.874390	10.478810
9.045771	731.927327	10.483827
8.763941	737.411152	10.488845
8.921615	743.258749	10.493863
9.075951	736.957710	10.498880
8.401911	735.742622	10.503898
8.830083	745.977985	10.508915
9.058731	766.646295	10.513933
9.035348	753.354649	10.518951
9.254390	759.901369	10.523968
9.296260	758.627899	10.528986
9.331223	755.393104	10.534003
9.335099	761.978137	10.539021
9.378879	767.370577	10.544039
9.163812	778.443657	10.549056
9.303794	763.938117	10.554074
9.458283	754.856393	10.559091
9.327042	761.278469	10.564109
9.724664	764.272413	10.569127
9.513696	747.465477	10.574144
9.036657	757.480850	10.579162
9.360705	745.767775	10.584179
9.283323	733.993324	10.589197
9.347537	731.049685	10.594215
9.360459	736.992538	10.599232
9.265183	757.429992	10.604250
9.711727	739.831227	10.609267
9.088018	745.838551	10.614285
9.093963	745.464183	10.619303
9.373427	761.791496	10.624320
9.374781	768.055184	10.629338
9.583112	755.143735	10.634355
9.937931	757.351952	10.639373
9.467664	752.643980	10.644391
9.576292	721.598115	10.649408
9.607013	729.888373	10.654426
9.662134	730.525388	10.659443
9.592958	729.260135	10.664461
9.274908	732.266953	10.669479
9.630978	719.830887	10.674496
9.233625	725.414386	10.679514
9.198623	715.706697	10.684531
9.211956	736.960300	10.689549
8.942403	724.161009	10.694567
9.396806	737.032263	10.699584
9.626476	771.131538	10.704602
9.513792	765.367001	10.709619
9.999770	755.573390	10.714637
9.227468	756.022521	10.719655
9.681408	745.380405	10.724672
9.346702	727.739346	10.729690
9.452831	739.354238	10.734707
9.537455	762.840669	10.739725
9.263263	763.442463	10.744743
9.586643	755.609259	10.749760
9.205516	749.671135	10.754778
9.243594	756.374397	10.759795
9.790958	745.976418	10.764813
9.403691	762.725342	10.769831
9.562572	758.140407	10.774848
9.490034	765.157444	10.779866
9.522501	743.717814	10.784883
9.871478	743.941701	10.789901
9.698220	770.370569	10.794919
9.896849	752.722919	10.799936
9.828225	752.215047	10.804954
9.934776	757.774130	10.809971
9.954340	750.148868	10.814989
9.669999	750.831648	10.820007
10.068559	759.415568	10.825024
9.761269	774.158811	10.830042
9.907046	769.036320	10.835059
10.180731	743.138032	10.840077
9.761939	742.966199	10.845095
9.800868	723.843212	10.850112
9.485113	734.524742	10.855130
9.553449	735.531422	10.860147
9.997951	761.175892	10.865165
9.681956	763.617371	10.870183
9.965407	755.741565	10.875200
9.844089	740.753778	10.880218
9.412052	728.787121	10.885235
9.898836	731.154579	10.890253
9.949530	776.097553	10.895271
10.109089	765.389927	10.900288
9.759329	735.823344	10.905306
9.705197	738.848935	10.910323
9.843004	754.724876	10.915341
9.865093	761.436785	10.920359
10.099338	753.553270	10.925376
9.909260	772.646442	10.930394
9.684981	759.756590	10.935411
9.990615	737.070674	10.940429
10.024586	761.149863	10.945447
9.984996	771.138121	10.950464
9.876141	761.803533	10.955482
9.767596	747.856066	10.960499
9.824701	751.222433	10.965517
9.868460	759.833202	10.970535
10.094249	752.654439	10.975552
10.207094	763.334829	10.980570
9.534494	770.764922	10.985587
9.984712	747.919405	10.990605
9.420255	745.402793	10.995623
10.154780	744.580457	11.000640
10.065064	767.426004	11.005658
9.798741	761.838982	11.010675
9.951608	753.623633	11.015693
9.631355	765.701124	11.020711
9.840255	746.829965	11.025728
9.990472	769.394198	11.030746
10.056928	773.567765	11.035763
10.085622	763.261980	11.040781
9.969988	774.394590	11.045799
10.107755	775.993377	11.050816
10.107926	787.873388	11.055834
9.780887	779.961581	11.060851
10.164658	787.375144	11.065869
9.986359	795.630902	11.070887
10.298865	799.815181	11.075904
10.503407	794.239190	11.080922
10.297005	779.433491	11.085939
10.263524	785.265658	11.090957
10.260225	807.183545	11.095975
10.358347	796.517931	11.100992
10.282933	778.256953	11.106010
10.115744	758.844841	11.111027
10.166253	772.842920	11.116045
9.727388	787.469570	11.121063
10.288059	789.414111	11.126080
10.431566	786.776268	11.131098
10.110135	785.343697	11.136115
10.296007	779.695817	11.141133
10.138631	784.291017	11.146151
10.032872	800.217685	11.151168
10.142444	777.938516	11.156186
10.387399	776.134471	11.161203
10.186952	794.048891	11.166221
10.153649	781.448243	11.171239
10.518797	775.654628	11.176256
10.380497	783.848076	11.181274
10.098155	792.973260	11.186291
10.394447	778.706569	11.191309
10.196687	775.026007	11.196327
10.496671	786.392127	11.201344
10.480716	803.269547	11.206362
10.317286	786.766244	11.211379
10.837239	771.383261	11.216397
10.538379	786.414415	11.221415
10.622581	796.520779	11.226432
10.658704	800.450810	11.231450
10.618536	789.329933	11.236467
10.670478	783.312064	11.241485
10.845258	796.382192	11.246503
10.634505	783.390801	11.251520
10.557481	777.446890	11.256538
10.698629	789.854442	11.261555
10.773502	783.506295	11.266573
10.491564	759.835054	11.271591
10.550136	772.448706	11.276608
10.469132	762.020634	11.281626
10.263470	769.355262	11.286643
10.635485	793.943941	11.291661
10.682307	790.266844	11.296679
10.514825	782.452062	11.301696
10.428005	773.507225	11.306714
10.517886	779.469456	11.311731
10.704649	784.261656	11.316749
10.422168	781.169152	11.321767
10.363898	772.621066	11.326784
10.492287	783.329798	11.331802
10.312688	791.962440	11.336819
10.546960	775.116829	11.341837
10.591388	799.921223	11.346855
10.653960	785.763897	11.351872
10.508246	771.413899	11.356890
10.366937	766.322221	11.361907
10.436939	777.231885	11.366925
10.596024	794.964976	11.371943
10.717716	811.997270	11.376960
10.665178	817.068824	11.381978
10.928853	807.294401	11.386995
11.336276	814.562571	11.392013
10.774902	794.302705	11.397031
10.356718	794.163833	11.402048
11.129519	781.556910	11.407066
10.911975	781.721702	11.412083
10.917629	788.161707	11.417101
10.744576	784.644633	11.422119
10.909696	791.640515	11.427136
10.808009	780.365680	11.432154
10.535048	778.143911	11.437171
10.741333	779.805471	11.442189
10.819240	801.999618	11.447207
10.857309	809.672530	11.452224
10.849012	804.430250	11.457242
10.874447	798.744031	11.462259
11.206659	808.441898	11.467277
11.095268	826.527712	11.472295
10.757689	817.058295	11.477312
11.188521	792.363650	11.482330
10.683998	786.020425	11.487347
10.821709	805.230291	11.492365
10.952388	822.347407	11.497383
10.771535	814.080017	11.502400
11.226592	807.805809	11.507418
11.099757	819.019809	11.512435
11.021827	821.140042	11.517453
10.955852	822.034804	11.522471
11.063381	817.829401	11.527488
11.267332	809.644940	11.532506
11.255057	802.145256	11.537523
11.191338	802.808308	11.542541
11.092401	799.475584	11.547559
11.052418	785.524034	11.552576
10.857128	772.362818	11.557594
11.053510	793.491297	11.562611
11.306041	808.568917	11.567629
11.440973	809.364551	11.572647
11.334713	779.208578	11.577664
10.969271	784.551356	11.582682
10.909860	797.168979	11.587699
11.035392	812.525198	11.592717
11.476717	798.062225	11.597735
11.206731	794.198371	11.602752
11.492414	784.856922	11.607770
11.233081	768.674621	11.612787
11.109034	761.964775	11.617805
11.074957	787.179260	11.622823
10.997910	800.388815	11.627840
11.477648	780.618164	11.632858
11.481437	790.841230	11.637875
11.552850	785.911485	11.642893
11.478090	795.017913	11.647911
10.975211	786.822351	11.652928
11.034171	768.895579	11.657946
11.037025	785.951418	11.662963
11.469402	810.218618	11.667981
11.346487	797.012753	11.672999
11.253916	809.525461	11.678016
11.573517	804.556665	11.683034
11.424149	793.511492	11.688051
11.391477	798.754514	11.693069
11.377351	808.716449	11.698087
11.211718	819.129495	11.703104
11.490634	811.118915	11.708122
11.419832	820.601278	11.713139
11.463927	812.133767	11.718157
11.684764	808.318785	11.723175
11.348929	790.149437	11.728192
11.790148	793.373127	11.733210
11.228835	807.752385	11.738227
11.409344	805.133517	11.743245
11.723224	798.636448	11.748263
11.060585	801.162374	11.753280
11.419699	812.480170	11.758298
11.320760	820.620984	11.763315
11.471565	809.795120	11.768333
11.630415	797.932088	11.773351
11.159632	799.734760	11.778368
11.555622	794.374508	11.783386
11.566406	805.469817	11.788403
11.328768	825.881197	11.793421
11.434365	826.832821	11.798439
11.241292	820.190739	11.803456
11.349807	806.843400	11.808474
11.371301	808.085324	11.813491
11.577372	799.556909	11.818509
11.802940	813.428091	11.823527
11.467035	824.361176	11.828544
11.718176	833.579476	11.833562
11.824720	844.568954	11.838579
11.573081	825.970108	11.843597
11.539277	831.652681	11.848615
11.592786	840.149709	11.853632
11.920375	817.979298	11.858650
11.806808	837.449961	11.863667
11.718059	861.697186	11.868685
12.090962	836.193655	11.873703
11.692153	827.722279	11.878720
11.809633	802.704103	11.883738
11.742333	795.409526	11.888755
11.946301	817.472461	11.893773
11.765284	824.426764	11.898791
11.311140	822.048462	11.903808
11.961759	811.670079	11.908826
11.872043	837.701009	11.913843
12.166884	843.801200	11.918861
12.242038	834.159265	11.923879
11.818993	820.986051	11.928896
11.914897	789.147185	11.933914
11.720314	798.811561	11.938931
11.987817	826.257262	11.943949
12.169479	825.398562	11.948967
12.040786	809.474969	11.953984
11.952746	793.772763	11.959002
12.062600	804.526196	11.964019
11.901935	817.925719	11.969037
11.918880	799.292854	11.974055
11.699347	790.998708	11.979072
12.150134	818.281761	11.984090
12.213057	828.447553	11.989107
11.795431	805.151621	11.994125
11.967167	826.341289	11.999143
11.796834	836.546124	12.004160
11.944126	817.022340	12.009178
12.096691	820.100874	12.014195
11.957128	837.853159	12.019213
12.169666	837.053513	12.024231
11.906486	834.346978	12.029248
12.172629	817.013110	12.034266
12.086764	828.287258	12.039283
12.064960	840.960693	12.044301
12.247052	843.593130	12.049319
12.209989	823.942756	12.054336
12.242511	830.141689	12.059354
12.246570	834.220395	12.064371
12.069174	828.996506	12.069389
12.449156	825.269955	12.074407
12.272674	839.371926	12.079424
12.480400	824.195760	12.084442
12.316117	829.376016	12.089459
12.279565	848.463100	12.094477
12.717527	840.692392	12.099495
12.234530	823.714043	12.104512
12.090738	797.846669	12.109530
12.336411	815.671452	12.114547
12.087558	825.351110	12.119565
12.662390	829.431630	12.124583
12.388292	842.311085	12.129600
12.274016	839.593817	12.134618
12.532412	822.845223	12.139635
12.343862	809.029885	12.144653
12.279328	801.366736	12.149671
12.043483	829.257337	12.154688
12.254512	839.028975	12.159706
12.540292	827.631234	12.164723
12.156598	830.035006	12.169741
12.773871	832.584210	12.174759
12.291776	845.466650	12.179776
12.115308	835.332479	12.184794
12.501296	840.667607	12.189811
12.370312	841.279490	12.194829
12.530208	827.834000	12.199847
12.602373	841.202645	12.204864
12.821208	829.907575	12.209882
12.355137	815.962744	12.214899
12.372426	834.409288	12.219917
12.329059	848.207848	12.224935
12.346070	843.495780	12.229952
12.476452	822.190902	12.234970
12.800201	825.597255	12.239987
12.579113	843.555586	12.245005
12.462837	838.452072	12.250023
12.597347	832.560364	12.255040
12.680754	833.676243	12.260058
12.502127	831.591199	12.265075
12.370733	842.383738	12.270093
12.803948	850.091050	12.275111
12.673784	837.670000	12.280128
12.683070	835.740173	12.285146
12.506590	827.852956	12.290163
12.425599	839.707650	12.295181
12.584214	819.280851	12.300199
12.778804	829.425476	12.305216
12.868932	862.101151	12.310234
12.647396	839.313764	12.315251
12.868826	847.983978	12.320269
13.029005	855.140112	12.325287
12.854948	836.253112	12.330304
12.968766	834.947476	12.335322
13.150800	820.780413	12.340339
12.670961	816.541595	12.345357
12.727346	824.505111	12.350375
12.931641	851.809572	12.355392
12.815494	834.720011	12.360410
12.698844	805.009484	12.365427
12.601482	821.913071	12.370445
13.068689	845.672146	12.375463
12.914720	867.087794	12.380480
13.046256	861.560448	12.385498
12.932403	840.675529	12.390515
12.913466	848.369591	12.395533
13.170191	854.865353	12.400551
12.953594	855.821513	12.405568
12.925762	824.095714	12.410586
12.994047	825.500827	12.415603
13.164014	842.999954	12.420621
12.918715	834.866497	12.425639
12.832458	831.121051	12.430656
12.901861	849.631129	12.435674
13.054390	852.447244	12.440691
13.176679	846.272684	12.445709
13.423068	857.914771	12.450727
13.030053	864.878344	12.455744
13.051897	844.876763	12.460762
13.291626	845.260402	12.465779
13.199162	857.929489	12.470797
12.984503	835.236222	12.475815
12.974712	842.137244	12.480832
12.819818	863.679090	12.485850
13.350087	860.401292	12.490867
13.299226	864.523128	12.495885
13.234375	839.177144	12.500903
13.162779	864.201846	12.505920
13.302368	862.405757	12.510938
13.474699	848.600512	12.515955
13.321480	846.893745	12.520973
13.407226	859.442267	12.525991
13.436689	852.115043	12.531008
13.012679	845.497435	12.536026
13.275838	840.652688	12.541043
13.155516	844.226990	12.546061
13.195712	852.502760	12.551079
13.314340	848.688915	12.556096
13.624686	842.133864	12.561114
13.581597	835.754808	12.566131
13.479419	850.077422	12.571149
13.010453	863.138762	12.576167
13.357663	859.997289	12.581184
13.251659	843.152926	12.586202
13.775342	851.130057	12.591219
13.446305	857.387863	12.596237
13.696774	845.005554	12.601255
13.637053	866.694626	12.606272
13.604955	867.561062	12.611290
13.529661	851.026790	12.616307
13.527123	838.335010	12.621325
13.628069	851.115105	12.626343
13.793917	837.892678	12.631360
13.324272	833.182609	12.636378
13.392916	839.778915	12.641395
13.737428	847.417737	12.646413
13.484521	834.241390	12.651431
13.699462	837.450822	12.656448
13.581410	849.376690	12.661466
13.847385	854.287087	12.666483
13.567925	840.236218	12.671501
13.527812	845.917772	12.676519
13.538079	860.665103	12.681536
13.354826	846.787847	12.686554
13.399487	835.550780	12.691571
13.278688	844.948138	12.696589
13.705461	850.310871	12.701607
13.390815	843.048191	12.706624
13.412511	850.356405	12.711642
13.789762	860.650741	12.716659
13.456772	853.778780	12.721677
13.735282	838.741061	12.726695
13.754311	837.663237	12.731712
13.317763	864.379610	12.736730
13.711397	867.376398	12.741747
13.930637	866.302781	12.746765
14.027007	859.888665	12.751783
14.601140	866.311415	12.756800
13.767675	870.497536	12.761818
13.809771	843.071911	12.766835
14.093509	827.762150	12.771853
13.955876	825.380743	12.776871
13.811168	853.157534	12.781888
13.648387	839.490331	12.786906
13.610344	851.912982	12.791923
13.781703	847.230314	12.796941
13.756230	871.517085	12.801959
14.079710	880.433772	12.806976
13.985975	886.424517	12.811994
14.116129	862.916551	12.817011
13.932283	859.496593	12.822029
13.992766	870.810745	12.827047
14.093605	885.985045	12.832064
14.013733	868.739589	12.837082
13.893169	870.449365	12.842099
14.034603	871.275809	12.847117
13.883011	858.498928	12.852135
14.150768	861.666871	12.857152
13.737850	880.939583	12.862170
14.265421	877.291458	12.867187
13.993678	862.380364	12.872205
14.041248	866.175386	12.877223
14.169977	884.339077	12.882240
14.186169	880.231208	12.887258
14.291176	857.224915	12.892275
14.340201	857.221870	12.897293
14.277372	872.466401	12.902311
14.185507	869.249687	12.907328
14.215148	882.365424	12.912346
14.070755	886.720775	12.917363
14.164331	871.474670	12.922381
14.024737	869.834135	12.927399
14.654217	874.611949	12.932416
14.159568	855.205022	12.937434
14.613364	852.766811	12.942451
14.611401	873.298224	12.947469
14.250981	866.878213	12.952487
14.457031	859.662024	12.957504
14.350347	853.405744	12.962522
14.372382	859.245689	12.967539
14.513131	876.086470	12.972557
14.424679	865.786592	12.977575
14.667597	867.076947	12.982592
14.453871	881.843798	12.987610
14.528157	870.970906	12.992627
14.472125	852.655271	12.997645
14.474982	856.323856	13.002663
14.568149	870.694502	13.007680
14.496502	881.137127	13.012698
14.429005	864.898914	13.017715
14.627011	856.486829	13.022733
14.376408	859.573447	13.027751
14.562297	873.026154	13.032768
14.945827	889.105365	13.037786
14.839022	883.988364	13.042803
14.616361	859.713428	13.047821
14.671416	861.408253	13.052839
14.912121	877.524239	13.057856
14.397715	876.261996	13.062874
14.288947	869.340283	13.067891
14.535412	859.201641	13.072909
14.448637	892.246880	13.077927
14.654752	895.448337	13.082944
14.545143	892.349580	13.087962
14.644828	873.902014	13.092979
14.497512	891.926143	13.097997
14.535993	908.855790	13.103015
14.855806	895.288663	13.108032
14.811741	892.937835	13.113050
14.645759	890.809857	13.118067
14.672716	907.354795	13.123085
14.649339	904.567193	13.128103
15.046603	886.453114	13.133120
14.737302	880.330378	13.138138
14.717876	875.062361	13.143155
14.702023	900.069448	13.148173
14.441694	891.124186	13.153191
15.302087	907.070101	13.158208
15.165059	930.219400	13.163226
14.725322	906.953731	13.168243
15.045591	892.060103	13.173261
14.917269	898.512847	13.178279
15.489065	904.340091	13.183296
15.198946	913.763700	13.188314
15.071208	888.422517	13.193331
14.543862	882.547764	13.198349
14.643943	887.399093	13.203367
15.062496	914.780928	13.208384
15.374698	914.660397	13.213402
15.471220	921.399632	13.218419
15.568755	905.253169	13.223437
15.280418	892.539398	13.228455
15.472347	878.678342	13.233472
15.212246	885.639149	13.238490
15.389267	877.796416	13.243507
15.384279	882.517309	13.248525
14.814392	893.617029	13.253543
15.046556	884.754615	13.258560
15.224630	883.282000	13.263578
15.442434	893.629471	13.268595
15.365585	881.998579	13.273613
15.224168	881.525856	13.278631
15.614170	879.834606	13.283648
15.315794	876.277508	13.288666
15.163392	890.854950	13.293683
15.344829	887.155191	13.298701
15.224188	872.410406	13.303719
15.382852	880.910449	13.308736
15.566374	896.038624	13.313754
15.301753	884.992652	13.318771
15.641992	890.826766	13.323789
15.604191	897.785283	13.328807
15.548062	882.165288	13.333824
15.548892	872.335466	13.338842
15.568098	877.362417	13.343859
15.664114	882.000889	13.348877
15.456841	887.306053	13.353895
15.464410	867.903299	13.358912
15.423539	863.898836	13.363930
15.339769	888.566727	13.368947
15.354810	896.079258	13.373965
15.172151	895.320709	13.378983
15.392308	891.585621	13.384000
15.324235	903.624106	13.389018
15.323751	890.367227	13.394035
15.692184	907.336812	13.399053
15.842963	921.410166	13.404071
15.971164	919.982885	13.409088
15.990946	890.997583	13.414106
15.509278	901.944676	13.419123
15.592392	892.991367	13.424141
15.201631	888.246990	13.429159
15.649177	897.831884	13.434176
15.705570	922.355046	13.439194
15.899136	927.683135	13.444211
15.880379	915.027329	13.449229
15.494977	921.282667	13.454247
15.611630	928.430186	13.459264
15.940049	938.791290	13.464282
15.440926	937.946684	13.469299
15.703378	923.026073	13.474317
15.517698	915.054133	13.479335
15.996754	927.882017	13.484352
16.097406	936.011853	13.489370
15.884777	927.126781	13.494387
16.254127	910.524674	13.499405
16.005773	921.033524	13.504423
16.033994	906.028834	13.509440
15.733170	923.066522	13.514458
15.555487	937.072645	13.519475
16.402266	913.747085	13.524493
16.117627	920.281956	13.529511
16.034873	916.642378	13.534528
15.867982	907.605111	13.539546
15.772228	910.917070	13.544563
15.850572	924.805302	13.549581
16.127000	930.453472	13.554599
15.837436	909.718625	13.559616
16.027387	909.371017	13.564634
15.637578	929.312730	13.569651
16.126353	936.974990	13.574669
16.158979	931.229870	13.579687
16.414278	931.291335	13.584704
16.456936	942.209867	13.589722
16.293466	945.832356	13.594739
16.603767	914.818504	13.599757
16.022323	918.568506	13.604775
16.098721	922.339492	13.609792
16.316915	932.097805	13.614810
15.867051	942.017098	13.619827
16.454717	926.033552	13.624845
16.277025	935.271808	13.629863
15.952676	936.332273	13.634880
16.380333	932.717669	13.639898
16.470047	945.949780	13.644915
16.471001	955.368807	13.649933
16.152099	950.405306	13.654951
16.272206	936.068495	13.659968
16.569037	929.287353	13.664986
16.263455	949.390227	13.670003
16.519277	945.791223	13.675021
16.246085	935.301902	13.680039
16.270841	938.930087	13.685056
16.385631	949.220326	13.690074
16.484799	962.785450	13.695091
16.845231	935.797086	13.700109
16.659652	926.076360	13.705127
16.693789	935.885459	13.710144
16.795210	945.399365	13.715162
16.639872	942.436764	13.720179
16.747473	925.381270	13.725197
16.614275	935.714350	13.730215
16.632599	938.573323	13.735232
16.659023	945.729660	13.740250
16.607053	941.652718	13.745267
16.947352	913.940445	13.750285
16.651765	919.536914	13.755303
16.434223	945.179512	13.760320
16.759226	942.874157	13.765338
16.426555	935.510107	13.770355
16.700179	941.904025	13.775373
16.633047	935.944346	13.780391
16.779783	930.652492	13.785408
16.480529	938.617568	13.790426
16.556801	963.931205	13.795443
16.968386	956.947965	13.800461
16.961746	949.513992	13.805479
16.874297	967.646496	13.810496
17.098806	980.263993	13.815514
16.763606	967.490597	13.820531
17.123487	946.117315	13.825549
17.147055	948.997071	13.830567
17.137128	947.499133	13.835584
17.482902	948.777320	13.840602
17.075012	946.397652	13.845619
17.069805	918.948023	13.850637
16.863985	928.104331	13.855655
17.024058	940.525114	13.860672
17.206262	940.127323	13.865690
16.749264	928.349919	13.870707
17.094158	921.081532	13.875725
16.908607	930.755224	13.880743
16.766512	935.450280	13.885760
17.224764	949.213762	13.890778
17.154192	958.026068	13.895795
17.330944	949.000968	13.900813
17.168376	969.101687	13.905831
17.604340	961.189946	13.910848
17.640622	930.466655	13.915866
17.436704	924.313104	13.920883
17.130210	933.367283	13.925901
17.367289	932.039695	13.930919
16.945626	921.214184	13.935936
17.334647	940.453342	13.940954
16.989250	942.809770	13.945971
17.198150	936.059686	13.950989
17.624949	943.627789	13.956007
17.366024	958.361051	13.961024
17.456967	941.052551	13.966042
17.324059	935.331537	13.971059
17.361675	922.981977	13.976077
17.125028	954.308078	13.981095
17.625968	953.743470	13.986112
17.704139	955.467253	13.991130
17.422818	969.081483	13.996147
17.760631	958.840989	14.001165
17.950480	957.377245	14.006183
17.371984	932.115593	14.011200
17.353964	913.245221	14.016218
16.968331	927.810563	14.021235
17.378886	955.211407	14.026253
17.658606	967.347351	14.031271
17.594536	952.924552	14.036288
17.569007	947.342442	14.041306
17.274875	962.202853	14.046323
17.441883	957.745223	14.051341
17.540582	963.736572	14.056359
17.257583	949.301739	14.061376
17.799896	938.629929	14.066394
17.310216	962.665490	14.071411
17.666387	993.439296	14.076429
17.625112	986.222097	14.081447
17.819045	977.296675	14.086464
18.019572	967.619079	14.091482
18.069416	992.825348	14.096499
17.768551	998.129879	14.101517
18.065456	983.274364	14.106535
18.003282	972.669163	14.111552
17.965088	972.574357	14.116570
18.144964	972.200074	14.121587
17.886446	971.975577	14.126605
17.793681	950.044474	14.131623
17.634560	953.768484	14.136640
17.772076	975.194368	14.141658
17.875922	995.694389	14.146675
17.847573	982.911995	14.151693
17.939550	972.959593	14.156711
17.717029	987.024831	14.161728
18.318363	996.866389	14.166746
17.934933	981.323111	14.171763
18.116107	987.268073	14.176781
18.134502	977.272429	14.181799
17.897143	972.712859	14.186816
18.240327	985.564524	14.191834
18.022930	983.580723	14.196851
17.988104	983.161329	14.201869
18.320573	987.711952	14.206887
18.168829	975.478561	14.211904
17.986488	992.396379	14.216922
18.116327	980.522748	14.221939
18.042129	978.258755	14.226957
18.085961	990.905035	14.231975
18.121538	1004.267668	14.236992
18.499369	1003.821016	14.242010
18.761450	1015.918463	14.247027
18.808780	1000.639551	14.252045
18.717817	996.371943	14.257063
18.454130	987.406810	14.262080
18.507287	979.551333	14.267098
18.441418	982.511508	14.272115
18.648194	977.389396	14.277133
18.613311	974.189222	14.282151
18.489519	975.049857	14.287168
18.700483	966.449889	14.292186
18.506053	965.356753	14.297203
18.431076	984.984768	14.302221
18.548122	977.837351	14.307239
18.461101	970.465064	14.312256
18.668859	966.084534	14.317274
18.680309	962.788834	14.322291
18.459219	946.960857	14.327309
18.804447	964.366021	14.332327
18.484350	984.467896	14.337344
18.822829	971.947842	14.342362
18.682535	958.296693	14.347379
18.846046	959.775429	14.352397
18.884719	953.472258	14.357415
18.528554	976.918011	14.362432
18.729163	961.702344	14.367450
18.832642	955.353827	14.372467
18.653954	963.230801	14.377485
19.141416	971.303230	14.382503
18.742163	979.412871	14.387520
19.101002	960.900431	14.392538
18.834953	956.788801	14.397555
19.044472	972.366479	14.402573
19.116012	958.963421	14.407591
18.984395	964.351360	14.412608
18.890372	976.508827	14.417626
19.027827	970.305537	14.422643
18.752772	955.940527	14.427661
18.997700	973.633566	14.432679
18.720505	981.628967	14.437696
18.959682	974.576891	14.442714
18.357232	955.650130	14.447731
18.668474	979.617916	14.452749
19.062182	986.663296	14.457767
18.622321	1005.952425	14.462784
19.073780	1000.063578	14.467802
19.069694	994.176016	14.472819
19.006178	995.164157	14.477837
19.421097	1011.499440	14.482855
19.023795	1009.959336	14.487872
19.289276	996.513593	14.492890
19.319723	997.254671	14.497907
19.157382	1009.360650	14.502925
19.327763	991.827527	14.507943
19.205892	1007.939779	14.512960
19.295954	1004.396124	14.517978
19.338934	1003.356544	14.522995
19.338657	1004.444346	14.528013
19.345289	993.789089	14.533031
19.335561	992.627544	14.538048
19.020250	1001.015672	14.543066
19.538645	1009.383401	14.548083
19.358813	1013.893033	14.553101
19.361722	992.309674	14.558119
19.207826	993.531297	14.563136
19.122574	1025.222165	14.568154
19.679502	1032.566202	14.573171
19.760597	1020.939117	14.578189
19.766515	1014.234153	14.583207
19.615343	1032.677484	14.588224
19.748934	1024.682247	14.593242
20.112973	1012.633900	14.598259
19.873639	1022.214397	14.603277
19.863320	990.399577	14.608295
19.798554	989.138691	14.613312
19.784019	997.489709	14.618330
20.016970	1005.609134	14.623347
19.712252	1004.956555	14.628365
19.855733	987.711250	14.633383
19.823435	994.297342	14.638400
20.055102	1003.405312	14.643418
19.875674	987.864132	14.648435
19.722640	976.626567	14.653453
19.832114	993.699164	14.658471
19.615243	991.232917	14.663488
19.815618	980.516231	14.668506
19.613575	994.460701	14.673523
19.671142	1009.878018	14.678541
19.799386	982.579037	14.683559
19.492424	1003.490273	14.688576
19.792615	1023.492034	14.693594
20.007726	1024.224442	14.698611
20.122552	1016.299617	14.703629
19.935317	1021.509806	14.708647
20.112750	1030.895388	14.713664
20.025588	1028.514957	14.718682
20.230990	1013.049199	14.723699
19.846365	1010.144842	14.728717
20.403927	1014.619704	14.733735
19.977039	1036.554389	14.738752
20.154603	1029.170725	14.743770
20.508260	1017.876853	14.748787
20.128631	1004.533772	14.753805
20.031252	1012.853396	14.758823
20.194957	1017.863600	14.763840
20.121016	1008.197288	14.768858
20.110165	1011.605250	14.773875
19.846039	1039.629122	14.778893
20.423560	1020.556294	14.783911
20.387593	999.560009	14.788928
20.168520	1010.308091	14.793946
20.066571	1030.968513	14.798963
19.847122	1028.584063	14.803981
20.092473	1037.673457	14.808999
20.376281	1055.411924	14.814016
20.479755	1058.952050	14.819034
20.908781	1043.720991	14.824051
20.532567	1044.959086	14.829069
20.752588	1050.046095	14.834087
20.883421	1024.242081	14.839104
20.601888	1018.094036	14.844122
20.896694	1005.468921	14.849139
20.802449	1018.917349	14.854157
20.619191	1003.442051	14.859175
20.810514	1006.759702	14.864192
20.713007	1034.711359	14.869210
20.869897	1022.645181	14.874227
20.265736	1019.684900	14.879245
20.454848	1014.242448	14.884263
20.105129	1008.479203	14.889280
20.463143	1020.856126	14.894298
20.836636	1034.319598	14.899315
20.657543	1033.565077	14.904333
20.904806	1033.384034	14.909351
21.227256	1043.244746	14.914368
20.701760	1047.283589	14.919386
21.110688	1039.243043	14.924403
20.885611	1038.055679	14.929421
21.321344	1031.464772	14.934439
21.243754	1039.754598	14.939456
20.831547	1028.925774	14.944474
21.005129	1015.786049	14.949491
20.582813	1032.065292	14.954509
20.948556	1019.668910	14.959527
21.289022	1013.385806	14.964544
20.783448	1015.601531	14.969562
21.137388	1028.735636	14.974579
21.201757	1040.539404	14.979597
21.268838	1032.620886	14.984615
21.067427	1025.847645	14.989632
20.850964	1031.046038	14.994650
21.174948	1057.065854	14.999667
21.067594	1047.357904	15.004685
20.730204	1029.922792	15.009703
20.955511	1040.702479	15.014720
20.907698	1043.071541	15.019738
21.010065	1055.300036	15.024755
20.941058	1055.682941	15.029773
20.937227	1028.696649	15.034791
21.138523	1052.914256	15.039808
21.219263	1077.197579	15.044826
21.706854	1074.251119	15.049843
21.447841	1058.516770	15.054861
21.813606	1056.285646	15.059879
21.571447	1051.661508	15.064896
21.379549	1071.263198	15.069914
21.428132	1060.141627	15.074931
21.498165	1048.387936	15.079949
21.734699	1054.586901	15.084967
21.999408	1051.238113	15.089984
21.454350	1037.113068	15.095002
21.636662	1039.107965	15.100019
21.409519	1042.324568	15.105037
21.455869	1043.826806	15.110055
21.682134	1045.828118	15.115072
21.699408	1074.815047	15.120090
21.700646	1081.256398	15.125107
21.586519	1071.612135	15.130125
21.513812	1050.196441	15.135143
22.148596	1067.054884	15.140160
21.657224	1085.031988	15.145178
21.711071	1059.242998	15.150195
21.927938	1051.902422	15.155213
21.845988	1061.380381	15.160231
21.784369	1077.976156	15.165248
21.753084	1067.411344	15.170266
22.085500	1068.229954	15.175283
22.005802	1078.757685	15.180301
21.921372	1063.950544	15.185319
22.210125	1063.368255	15.190336
21.917048	1049.850610	15.195354
22.180162	1051.787581	15.200371
22.120217	1074.130562	15.205389
22.084163	1065.692883	15.210407
22.110948	1053.820480	15.215424
22.003805	1054.945822	15.220442
22.076377	1067.068156	15.225459
22.127445	1083.092991	15.230477
21.944776	1060.348444	15.235495
22.335687	1041.689599	15.240512
21.981821	1061.960599	15.245530
22.153583	1064.008608	15.250547
21.861054	1064.637846	15.255565
21.608890	1055.096109	15.260583
22.121671	1052.862339	15.265600
21.901969	1043.210350	15.270618
22.261302	1062.835281	15.275635
22.224769	1058.629608	15.280653
22.364632	1069.813496	15.285671
22.495927	1085.375089	15.290688
22.002315	1077.108267	15.295706
22.579836	1078.440076	15.300723
22.563274	1091.137946	15.305741
22.742388	1088.101646	15.310759
22.651798	1070.836576	15.315776
22.297424	1061.921220	15.320794
22.709438	1072.155047	15.325811
22.596981	1086.428215	15.330829
22.600800	1084.815224	15.335847
23.011927	1071.855827	15.340864
23.038656	1050.508621	15.345882
22.790429	1036.912038	15.350899
22.474876	1056.491340	15.355917
22.547305	1061.182571	15.360935
22.423598	1042.790412	15.365952
22.571779	1061.129009	15.370970
22.844260	1066.401302	15.375987
22.851846	1071.189844	15.381005
22.703744	1097.725625	15.386023
22.923558	1082.736628	15.391040
23.007183	1095.001413	15.396058
22.955698	1087.955497	15.401075
22.766512	1074.447231	15.406093
22.830579	1070.776663	15.411111
23.010200	1082.587889	15.416128
22.682892	1081.101253	15.421146
22.508391	1062.870478	15.426163
23.082368	1082.958168	15.431181
22.967189	1094.982645	15.436199
22.859977	1083.462497	15.441216
22.938467	1073.236342	15.446234
23.035875	1088.837094	15.451251
23.241842	1097.695689	15.456269
23.055571	1098.890789	15.461287
23.178212	1074.029053	15.466304
22.895393	1073.964831	15.471322
23.202158	1080.511265	15.476339
23.282241	1088.265246	15.481357
23.251069	1091.230630	15.486375
23.295582	1069.068553	15.491392
23.326955	1078.925335	15.496410
23.332836	1088.528329	15.501427
23.652576	1085.613244	15.506445
23.274099	1090.590361	15.511463
23.786705	1087.354501	15.516480
23.356114	1083.657628	15.521498
23.380722	1066.161275	15.526515
23.726614	1090.861616	15.531533
23.188807	1106.529765	15.536551
23.423957	1079.458136	15.541568
23.008291	1073.862220	15.546586
23.196386	1070.284909	15.551603
23.473119	1075.171263	15.556621
23.370104	1096.488678	15.561639
23.550818	1110.149289	15.566656
23.759392	1106.455522	15.571674
23.549507	1104.868004	15.576691
23.975532	1125.426349	15.581709
23.764602	1121.917424	15.586727
23.702734	1097.780065	15.591744
23.968906	1093.175037	15.596762
24.076510	1095.560442	15.601779
23.736026	1086.627621	15.606797
23.480786	1085.565583	15.611815
23.959990	1085.776814	15.616832
23.998490	1104.911644	15.621850
24.080396	1081.542286	15.626867
24.022168	1074.197368	15.631885
23.875321	1080.984271	15.636903
23.822068	1070.562718	15.641920
23.821954	1071.721641	15.646938
23.738027	1110.006725	15.651955
23.795489	1101.684939	15.656973
23.552156	1094.372961	15.661991
24.555382	1104.617255	15.667008
24.010654	1112.286749	15.672026
23.936473	1101.706665	15.677043
24.307256	1101.759773	15.682061
23.991412	1114.447585	15.687079
24.088868	1108.944380	15.692096
24.033822	1102.832281	15.697114
24.003985	1107.280646	15.702131
23.980252	1109.173808	15.707149
23.835609	1088.721978	15.712167
24.251557	1108.933529	15.717184
24.607950	1126.011030	15.722202
24.422044	1109.442013	15.727219
24.100301	1114.814781	15.732237
23.882797	1127.002810	15.737255
25.050025	1114.699147	15.742272
24.999666	1110.407675	15.747290
24.623068	1103.610211	15.752307
24.488768	1108.275102	15.757325
24.603674	1095.454279	15.762343
24.630929	1083.189057	15.767360
24.409682	1093.079426	15.772378
24.408914	1083.121220	15.777395
24.866995	1075.507366	15.782413
24.566547	1096.095094	15.787431
24.574100	1088.506088	15.792448
24.632191	1093.573720	15.797466
24.280741	1085.319908	15.802483
24.722836	1114.673021	15.807501
24.981614	1139.120873	15.812519
25.037616	1119.945762	15.817536
25.086893	1119.565307	15.822554
24.937104	1109.139705	15.827571
25.198427	1083.841259	15.832589
24.697838	1099.518700	15.837607
24.687616	1109.300998	15.842624
24.861936	1088.037689	15.847642
24.900222	1071.488147	15.852659
25.264240	1091.992538	15.857677
25.201578	1106.341924	15.862695
25.299846	1100.564835	15.867712
25.538688	1081.287233	15.872730
25.127481	1088.685205	15.877747
25.538487	1092.170780	15.882765
25.029897	1084.914152	15.887783
25.052226	1087.761175	15.892800
24.607736	1096.195302	15.897818
24.656630	1082.053540	15.902835
24.754702	1067.333236	15.907853
24.817998	1095.106107	15.912871
25.368504	1130.054915	15.917888
25.323281	1126.585420	15.922906
25.055434	1130.599322	15.927923
25.300700	1129.631596	15.932941
25.155377	1132.833614	15.937959
25.152114	1127.292236	15.942976
25.200707	1128.266780	15.947994
25.352811	1117.082993	15.953011
25.394116	1118.265383	15.958029
25.158865	1131.847051	15.963047
25.118486	1131.236294	15.968064
25.394681	1121.964696	15.973082
25.404864	1134.929080	15.978099
25.585716	1137.548981	15.983117
25.682854	1157.704842	15.988135
25.437454	1168.178736	15.993152
25.588454	1159.306846	15.998170
25.823764	1159.083300	16.003187
26.074965	1138.608401	16.008205
25.869121	1147.147474	16.013223
25.854720	1146.053800	16.018240
26.239422	1132.353525	16.023258
25.591817	1134.958986	16.028275
25.934019	1118.729948	16.033293
25.632762	1102.619951	16.038311
25.405056	1116.878244	16.043328
26.085375	1152.402060	16.048346
25.676001	1154.790149	16.053363
26.003262	1147.177607	16.058381
25.952675	1148.968544	16.063399
25.951001	1132.734028	16.068416
25.755610	1140.093999	16.073434
25.539564	1150.707090	16.078451
25.947090	1144.807441	16.083469
26.075998	1140.090862	16.088487
26.001784	1149.317264	16.093504
26.105540	1140.643008	16.098522
25.685085	1148.029055	16.103539
25.658875	1153.993494	16.108557
25.971079	1180.029440	16.113575
26.656576	1165.966218	16.118592
26.908445	1157.226640	16.123610
26.601968	1163.363646	16.128627
26.694538	1163.352913	16.133645
26.436041	1152.241675	16.138663
26.455388	1127.101915	16.143680
26.518853	1112.555257	16.148698
26.447031	1135.047302	16.153715
26.413889	1140.679203	16.158733
26.364194	1144.621930	16.163751
26.195954	1128.689974	16.168768
26.342020	1134.942494	16.173786
26.595656	1156.348658	16.178803
26.638711	1162.846602	16.183821
26.669171	1170.262845	16.188839
26.499907	1174.684185	16.193856
26.711784	1169.495926	16.198874
26.640221	1163.232927	16.203891
26.655229	1154.226759	16.208909
26.774457	1167.045426	16.213927
26.878132	1168.055249	16.218944
26.922335	1165.166986	16.223962
26.697966	1180.102280	16.228979
26.988322	1175.510156	16.233997
27.131359	1162.132793	16.239015
27.027662	1173.009155	16.244032
27.212997	1152.268023	16.249050
26.976897	1145.462478	16.254067
26.942451	1132.993684	16.259085
27.010068	1121.715515	16.264103
26.980335	1139.072534	16.269120
27.385190	1149.653084	16.274138
27.021793	1127.944060	16.279155
26.879396	1120.655636	16.284173
27.198395	1131.301529	16.289191
26.955234	1151.765720	16.294208
26.972952	1159.686797	16.299226
27.075355	1162.305299	16.304243
27.138245	1154.684680	16.309261
27.294955	1151.185157	16.314279
27.505107	1152.435491	16.319296
27.401376	1156.671136	16.324314
27.098109	1169.413988	16.329331
27.167314	1165.928232	16.334349
27.476291	1165.946585	16.339367
27.091707	1162.953926	16.344384
27.161483	1169.119485	16.349402
27.029553	1169.235593	16.354419
27.250518	1160.475536	16.359437
27.529820	1171.678179	16.364455
27.544702	1184.214668	16.369472
27.925893	1167.554827	16.374490
27.662872	1169.031349	16.379507
27.149775	1172.735972	16.384525
27.297089	1174.231576	16.389543
27.284384	1178.215136	16.394560
27.668408	1195.184828	16.399578
27.728899	1183.232560	16.404595
27.895393	1192.951170	16.409613
28.156122	1185.449677	16.414631
27.614018	1175.422834	16.419648
27.692705	1176.053710	16.424666
27.847969	1182.712309	16.429683
27.863486	1178.033940	16.434701
27.913274	1194.727447	16.439719
27.954881	1187.804159	16.444736
28.373769	1174.896923	16.449754
28.122471	1179.642276	16.454771
28.015009	1183.793231	16.459789
28.151845	1176.626314	16.464807
28.068702	1174.841706	16.469824
28.515317	1191.307468	16.474842
27.862867	1180.208075	16.479859
27.822687	1157.624437	16.484877
28.041947	1175.670097	16.489895
28.090560	1189.362941	16.494912
28.149705	1192.834654	16.499930
28.271882	1183.977451	16.504947
28.005921	1195.006597	16.509965
28.385866	1199.993034	16.514983
28.333788	1200.217670	16.520000
28.721050	1196.669016	16.525018
28.725396	1210.510204	16.530035
28.307685	1193.014671	16.535053
28.551495	1168.446758	16.540071
28.318485	1168.747344	16.545088
28.298925	1187.261118	16.550106
28.543193	1200.876671	16.555123
28.706291	1198.534268	16.560141
28.696805	1205.927118	16.565159
28.621805	1219.530206	16.570176
28.951918	1208.562351	16.575194
28.927071	1202.899640	16.580211
28.342594	1178.675523	16.585229
28.992644	1189.014646	16.590247
28.897463	1204.831549	16.595264
28.987795	1191.005695	16.600282
28.561237	1177.991669	16.605299
28.694866	1202.453317	16.610317
28.902194	1201.611611	16.615335
29.086544	1213.598197	16.620352
29.114662	1206.080323	16.625370
28.989307	1198.462745	16.630387
28.873753	1192.565678	16.635405
29.414207	1191.777264	16.640423
29.076049	1193.643575	16.645440
28.911908	1202.409196	16.650458
28.704075	1196.746910	16.655475
29.075076	1185.651575	16.660493
29.232685	1187.165455	16.665511
28.974061	1209.701073	16.670528
29.011918	1197.626678	16.675546
29.006005	1183.353362	16.680563
28.868938	1202.722297	16.685581
28.950092	1197.703430	16.690599
29.143515	1202.953706	16.695616
29.414016	1231.637437	16.700634
29.418179	1238.108777	16.705651
29.362626	1227.662896	16.710669
29.245312	1229.849719	16.715687
29.584993	1231.473738	16.720704
29.655921	1230.158625	16.725722
29.515989	1243.989834	16.730739
29.393033	1237.515763	16.735757
29.833910	1228.263038	16.740775
29.786569	1214.299223	16.745792
29.729730	1224.603349	16.750810
29.832492	1240.065411	16.755827
29.740105	1228.066734	16.760845
29.671683	1207.162981	16.765863
29.732012	1232.743416	16.770880
29.579689	1234.753784	16.775898
29.910536	1231.917428	16.780915
29.586634	1222.700063	16.785933
29.776402	1213.411892	16.790951
29.613774	1218.607651	16.795968
29.953396	1228.608625	16.800986
29.677480	1228.903411	16.806003
29.559973	1226.284320	16.811021
29.683606	1246.135401	16.816039
29.564493	1253.596672	16.821056
30.211490	1250.723617	16.826074
30.386182	1250.575525	16.831091
29.813727	1260.072176	16.836109
30.573731	1250.418458	16.841127
30.290743	1257.920981	16.846144
30.496320	1259.099164	16.851162
30.928981	1243.496922	16.856179
30.703987	1247.261802	16.861197
30.733859	1237.087361	16.866215
30.324973	1226.927374	16.871232
30.376894	1210.433682	16.876250
30.461773	1210.289017	16.881267
30.388982	1213.851418	16.886285
30.795825	1198.805422	16.891303
30.484998	1208.336251	16.896320
30.480811	1220.127674	16.901338
30.541177	1197.850021	16.906355
30.485637	1195.988032	16.911373
30.581005	1197.160314	16.916391
30.495805	1229.402966	16.921408
30.468938	1236.680326	16.926426
31.079591	1225.141224	16.931443
30.427184	1245.192769	16.936461
30.944981	1232.211674	16.941479
30.902382	1233.687694	16.946496
30.960951	1260.660656	16.951514
30.979618	1238.462456	16.956531
30.926637	1234.636233	16.961549
31.106824	1225.525973	16.966567
30.815421	1252.788883	16.971584
30.708997	1243.255712	16.976602
31.017243	1227.182332	16.981619
30.724940	1227.128925	16.986637
31.037990	1248.392557	16.991655
30.760293	1238.955491	16.996672
30.808811	1230.804461	17.001690
31.070583	1250.091116	17.006707
30.717743	1248.067471	17.011725
31.043956	1239.509414	17.016743
31.345695	1241.901335	17.021760
31.324135	1250.060095	17.026778
31.246164	1263.700811	17.031795
31.097492	1274.837867	17.036813
30.991338	1266.487332	17.041831
31.168176	1262.769645	17.046848
31.149105	1266.520674	17.051866
31.089850	1254.672567	17.056883
31.343335	1251.780110	17.061901
31.275964	1250.635254	17.066919
31.422474	1282.034407	17.071936
31.599855	1289.605916	17.076954
32.078307	1272.189610	17.081971
31.614424	1282.572058	17.086989
32.029801	1283.919857	17.092007
31.929458	1271.864206	17.097024
31.839029	1252.433861	17.102042
31.913589	1259.321724	17.107059
31.619735	1261.295950	17.112077
31.919930	1243.083540	17.117095
31.793247	1251.495739	17.122112
31.858055	1273.477335	17.127130
32.041508	1284.277790	17.132147
31.995168	1274.530584	17.137165
32.016300	1269.313590	17.142183
32.174024	1282.129633	17.147200
32.055135	1289.887667	17.152218
32.275680	1280.817840	17.157235
32.211241	1300.725753	17.162253
32.545161	1288.141938	17.167271
32.308898	1254.800957	17.172288
31.982325	1233.052045	17.177306
32.258063	1243.610011	17.182323
32.341276	1274.673233	17.187341
32.193535	1286.310125	17.192359
32.075645	1265.465046	17.197376
32.168022	1269.258865	17.202394
32.486566	1285.390268	17.207411
32.170451	1289.861098	17.212429
32.264474	1284.786250	17.217447
32.295519	1266.779471	17.222464
32.066825	1273.279858	17.227482
32.243609	1284.305378	17.232499
31.940658	1287.315121	17.237517
32.271423	1289.390417	17.242535
32.659192	1292.736211	17.247552
32.647794	1311.948526	17.252570
32.817822	1308.035444	17.257587
32.601518	1313.289602	17.262605
33.056860	1315.595536	17.267623
33.075398	1300.924166	17.272640
32.832129	1293.812526	17.277658
32.944156	1307.988977	17.282675
32.865121	1320.371550	17.287693
33.194483	1306.411529	17.292711
33.343162	1286.087398	17.297728
32.732879	1293.927619	17.302746
33.084166	1301.878864	17.307763
33.185526	1311.182821	17.312781
33.202507	1292.815035	17.317799
33.197446	1276.932615	17.322816
33.129126	1303.356084	17.327834
33.395950	1307.028686	17.332851
33.376889	1299.609289	17.337869
33.301935	1282.863419	17.342887
33.298434	1303.815351	17.347904
33.174968	1301.297208	17.352922
33.486732	1292.966653	17.357939
33.137504	1288.648945	17.362957
33.330622	1300.105436	17.367975
33.349315	1295.396001	17.372992
33.401834	1310.821960	17.378010
33.663789	1301.156340	17.383027
33.493393	1294.215096	17.388045
33.231823	1300.173417	17.393063
33.360652	1278.373984	17.398080
33.472322	1302.970887	17.403098
33.876577	1303.011873	17.408115
33.347410	1313.827966	17.413133
33.834892	1323.529141	17.418151
33.696486	1328.349465	17.423168
33.777922	1313.666212	17.428186
33.899930	1307.939736	17.433203
33.986027	1327.940301	17.438221
34.099845	1307.853837	17.443239
34.367467	1320.835568	17.448256
34.150588	1328.232637	17.453274
34.202142	1315.163988	17.458291
33.870239	1322.199737	17.463309
34.091799	1326.892581	17.468327
33.973317	1323.514361	17.473344
33.955373	1321.095484	17.478362
34.248090	1316.769205	17.483379
34.165116	1330.658978	17.488397
34.074014	1331.686534	17.493415
34.216256	1313.786591	17.498432
34.313111	1327.686990	17.503450
34.458704	1312.995990	17.508467
34.199195	1315.509697	17.513485
34.137441	1322.105915	17.518503
34.090135	1331.030411	17.523520
34.376049	1341.474584	17.528538
34.199031	1322.894683	17.533555
34.848705	1327.782666	17.538573
34.655482	1337.898529	17.543591
34.922734	1346.979766	17.548608
34.811610	1353.486638	17.553626
34.829446	1324.263193	17.558643
34.712538	1319.773062	17.563661
34.847139	1331.298976	17.568679
34.841634	1317.680139	17.573696
34.651965	1337.070139	17.578714
34.829937	1340.883288	17.583731
34.716877	1334.706684	17.588749
34.883529	1335.275208	17.593767
35.042287	1320.715065	17.598784
34.626028	1348.798592	17.603802
35.027316	1343.142068	17.608819
34.848477	1320.309413	17.613837
34.985704	1315.425795	17.618855
35.073261	1322.062285	17.623872
35.310723	1341.226133	17.628890
35.270301	1333.665893	17.633907
35.166764	1327.083382	17.638925
35.103941	1324.461438	17.643943
35.057204	1328.700603	17.648960
34.847117	1353.212895	17.653978
35.438106	1354.919880	17.658995
35.338446	1353.616905	17.664013
35.476291	1363.095730	17.669031
35.845781	1369.289876	17.674048
35.603261	1373.784879	17.679066
35.572215	1350.424919	17.684083
35.442294	1339.519214	17.689101
35.743755	1358.278897	17.694119
35.801106	1375.308382	17.699136
35.684974	1375.060742	17.704154
35.873877	1351.795998	17.709171
35.916908	1347.498277	17.714189
35.881866	1365.567586	17.719207
35.913605	1373.599324	17.724224
35.801137	1365.886838	17.729242
36.118487	1356.749603	17.734259
35.816312	1373.233024	17.739277
35.832886	1381.295318	17.744295
36.111219	1371.998320	17.749312
35.960684	1363.006100	17.754330
36.168117	1359.788041	17.759347
36.059233	1359.074153	17.764365
35.959902	1342.930533	17.769383
36.314149	1340.353912	17.774400
36.321278	1363.045795	17.779418
35.940897	1369.908613	17.784435
36.261695	1357.777693	17.789453
36.106413	1343.228290	17.794471
35.992813	1342.968720	17.799488
35.623663	1366.915918	17.804506
36.176643	1377.774738	17.809523
36.430846	1369.345509	17.814541
36.068730	1370.841574	17.819559
36.388829	1387.496134	17.824576
36.307836	1398.382583	17.829594
36.200435	1392.554843	17.834611
36.317612	1375.983866	17.839629
36.485130	1399.144265	17.844647
37.127080	1405.232688	17.849664
36.997263	1408.191113	17.854682
37.351248	1399.957634	17.859699
37.204436	1392.971020	17.864717
36.938640	1383.014888	17.869735
37.330368	1375.916264	17.874752
36.992436	1376.779736	17.879770
37.281516	1349.289263	17.884787
37.406031	1371.318208	17.889805
37.162811	1385.794029	17.894823
37.386675	1381.585090	17.899840
37.016279	1373.316243	17.904858
37.092469	1367.219745	17.909875
37.411856	1375.077110	17.914893
37.221258	1371.649492	17.919911
37.345658	1364.852469	17.924928
37.412187	1381.361271	17.929946
37.314640	1381.317108	17.934963
37.241812	1365.170463	17.939981
37.354235	1362.178686	17.944999
37.568897	1370.319632	17.950016
37.223790	1378.866495	17.955034
37.290398	1361.474650	17.960051
37.426278	1350.348873	17.965069
36.954975	1366.854036	17.970087
37.363114	1375.363807	17.975104
37.329681	1386.851896	17.980122
37.104624	1378.590125	17.985139
37.438647	1386.261163	17.990157
37.397554	1396.924925	17.995175
37.643519	1404.167120	18.000192
37.760780	1403.406315	18.005210
37.382183	1410.110427	18.010227
37.838913	1403.959199	18.015245
37.736445	1423.480239	18.020263
37.553112	1429.122895	18.025280
37.933999	1429.846922	18.030298
37.929482	1445.326329	18.035315
38.067199	1426.638301	18.040333
37.978275	1415.758633	18.045351
38.093610	1414.091952	18.050368
38.353679	1429.923103	18.055386
38.109455	1424.247459	18.060403
38.370129	1413.347809	18.065421
38.411580	1428.654779	18.070439
38.309934	1418.246495	18.075456
38.670701	1412.809684	18.080474
38.282839	1418.888406	18.085491
38.598935	1413.568991	18.090509
38.411526	1425.386027	18.095527
38.761962	1430.184252	18.100544
38.820122	1428.779914	18.105562
38.594758	1430.539936	18.110579
38.585463	1427.762409	18.115597
38.766582	1439.243620	18.120615
38.525358	1458.022352	18.125632
39.064807	1458.803723	18.130650
39.108097	1449.971309	18.135667
39.117354	1423.547385	18.140685
39.174143	1417.209640	18.145703
39.048180	1423.567552	18.150720
39.063070	1428.764061	18.155738
38.813503	1409.191937	18.160755
39.401950	1396.926128	18.165773
39.290321	1420.765222	18.170791
38.982936	1420.912391	18.175808
39.182739	1410.777455	18.180826
39.016132	1431.549671	18.185843
38.986432	1443.755135	18.190861
39.371642	1434.429220	18.195879
39.619740	1436.212065	18.200896
39.583334	1448.697614	18.205914
39.494090	1448.818774	18.210931
39.701562	1428.339298	18.215949
39.597751	1431.408759	18.220967
39.543121	1429.438741	18.225984
39.787387	1424.917924	18.231002
39.280663	1415.406512	18.236019
39.388791	1428.166519	18.241037
38.972545	1448.247103	18.246055
39.469837	1436.098174	18.251072
39.698569	1428.661581	18.256090
39.548829	1445.867262	18.261107
39.784920	1430.467059	18.266125
39.544301	1431.755397	18.271143
39.422761	1445.752609	18.276160
39.744058	1452.315992	18.281178
39.788081	1448.110577	18.286195
39.964487	1459.404140	18.291213
39.775703	1483.501007	18.296231
40.161663	1470.172484	18.301248
40.358690	1461.057236	18.306266
39.897182	1456.334998	18.311283
40.321067	1473.506734	18.316301
39.851778	1477.066522	18.321319
40.140703	1453.324666	18.326336
40.597986	1456.544371	18.331354
39.994892	1465.245109	18.336371
40.304186	1464.819219	18.341389
40.360025	1466.295035	18.346407
40.543816	1479.785330	18.351424
40.805748	1490.568436	18.356442
40.791956	1478.351207	18.361459
40.535165	1463.984863	18.366477
40.597516	1477.583689	18.371495
40.718549	1473.979283	18.376512
40.837237	1477.751685	18.381530
40.580456	1497.789057	18.386547
40.975367	1498.628462	18.391565
40.896145	1489.299651	18.396583
40.809090	1488.014853	18.401600
41.002646	1491.173050	18.406618
40.723903	1494.767483	18.411635
41.112490	1477.461935	18.416653
40.919944	1501.201164	18.421671
41.287169	1488.537584	18.426688
41.271924	1475.652633	18.431706
41.356573	1474.908924	18.436723
41.132713	1484.902808	18.441741
41.138085	1482.211805	18.446759
40.947385	1473.833896	18.451776
41.198030	1488.334382	18.456794
40.747346	1502.583335	18.461811
41.389972	1491.737810	18.466829
41.847265	1490.804696	18.471847
41.814637	1506.807594	18.476864
41.709413	1497.037701	18.481882
41.467311	1494.194423	18.486899
41.709001	1473.503865	18.491917
41.436852	1479.534952	18.496935
41.407976	1507.701181	18.501952
42.041068	1493.457878	18.506970
42.049286	1497.609582	18.511987
41.961787	1501.457783	18.517005
42.051134	1503.157346	18.522023
42.117710	1486.772033	18.527040
42.426926	1494.757688	18.532058
42.041224	1494.363000	18.537075
42.002226	1465.520838	18.542093
42.327252	1458.474134	18.547111
41.781498	1473.028370	18.552128
42.065879	1464.143218	18.557146
41.987616	1489.055701	18.562163
42.023882	1496.922324	18.567181
42.380254	1504.849120	18.572199
42.156116	1496.139201	18.577216
42.360286	1492.777591	18.582234
42.280739	1503.700974	18.587251
42.405346	1490.220586	18.592269
42.394941	1502.829512	18.597287
42.358525	1510.550116	18.602304
42.440446	1483.025246	18.607322
42.173351	1479.485074	18.612339
42.329473	1498.568783	18.617357
42.135659	1513.073068	18.622375
42.209813	1521.538232	18.627392
42.955127	1524.664106	18.632410
42.950954	1540.260358	18.637427
42.905215	1523.860501	18.642445
42.913310	1530.112661	18.647463
42.694270	1523.556434	18.652480
43.123524	1521.132116	18.657498
42.739310	1527.404034	18.662515
42.559520	1531.494118	18.667533
43.351856	1533.173462	18.672551
42.882865	1527.665995	18.677568
43.022824	1532.038995	18.682586
43.161384	1561.159429	18.687603
43.395346	1553.455237	18.692621
42.791656	1548.702244	18.697639
42.897134	1566.755458	18.702656
43.272733	1543.958382	18.707674
43.290635	1564.990482	18.712691
43.775114	1551.558325	18.717709
43.948629	1529.949728	18.722727
43.695004	1536.910448	18.727744
43.798179	1550.168511	18.732762
43.270840	1543.826964	18.737779
44.039318	1545.964583	18.742797
43.963218	1544.651401	18.747815
43.542513	1545.974525	18.752832
43.837193	1528.182185	18.757850
44.173222	1550.364190	18.762867
43.937039	1557.988723	18.767885
43.860371	1545.424623	18.772903
43.730045	1542.453736	18.777920
44.296849	1552.805783	18.782938
44.034077	1587.330506	18.787955
44.036294	1581.771526	18.792973
44.046537	1568.514451	18.797991
43.722276	1568.720894	18.803008
44.144005	1578.976386	18.808026
44.347578	1582.578324	18.813043
44.387871	1584.026511	18.818061
44.432896	1580.535997	18.823079
44.395385	1585.451713	18.828096
44.359845	1568.897202	18.833114
44.302921	1573.269193	18.838131
44.562596	1577.601070	18.843149
44.628783	1561.488321	18.848167
44.528981	1571.227363	18.853184
44.529771	1596.195642	18.858202
44.889785	1581.401448	18.863219
44.783883	1575.842820	18.868237
45.179860	1589.424107	18.873255
45.043750	1604.138187	18.878272
45.182584	1591.415138	18.883290
45.133490	1576.591820	18.888307
45.030345	1571.317815	18.893325
45.234869	1588.459703	18.898343
44.809086	1604.165149	18.903360
45.065235	1589.299842	18.908378
45.119705	1575.960664	18.913395
45.157786	1586.179482	18.918413
45.401498	1589.203257	18.923431
45.259172	1581.463417	18.928448
45.022786	1579.195138	18.933466
45.181830	1575.369316	18.938483
45.133126	1591.507805	18.943501
45.246404	1597.109086	18.948519
45.159327	1607.327147	18.953536
45.512168	1595.436165	18.958554
45.672738	1607.466648	18.963571
45.493560	1622.417144	18.968589
45.896958	1630.175442	18.973607
45.816283	1617.307286	18.978624
45.840738	1590.483894	18.983642
45.672185	1592.841897	18.988659
45.663624	1624.330751	18.993677
45.878069	1609.550153	18.998695
46.003792	1606.175208	19.003712
46.176963	1594.333597	19.008730
45.910827	1607.816973	19.013747
45.693415	1606.438672	19.018765
46.137262	1599.442825	19.023783
46.271076	1610.899410	19.028800
46.363769	1629.843107	19.033818
46.314973	1625.084598	19.038835
46.701750	1630.939551	19.043853
46.666300	1636.556468	19.048871
46.516030	1608.343418	19.053888
46.847860	1606.936646	19.058906
46.614738	1592.389340	19.063923
45.859290	1604.973268	19.068941
46.755287	1627.775793	19.073959
46.702990	1633.103330	19.078976
46.855704	1613.693062	19.083994
46.827610	1624.100557	19.089011
46.507081	1631.075130	19.094029
46.912373	1631.506614	19.099047
46.716827	1646.077340	19.104064
46.811958	1628.180485	19.109082
46.726800	1619.555085	19.114099
47.013663	1629.230959	19.119117
46.912247	1628.027049	19.124135
46.860709	1629.336313	19.129152
46.941708	1657.393243	19.134170
47.278075	1653.575691	19.139187
46.987891	1659.191707	19.144205
47.597561	1655.606986	19.149223
47.686656	1653.231576	19.154240
47.509261	1632.330685	19.159258
47.804387	1653.393853	19.164275
47.261470	1668.404598	19.169293
47.654281	1648.227697	19.174311
47.814791	1649.833447	19.179328
47.639615	1638.319682	19.184346
47.739931	1657.825225	19.189363
47.231985	1666.381935	19.194381
47.600775	1657.740937	19.199399
47.728611	1642.562500	19.204416
47.476806	1660.462311	19.209434
48.274805	1658.696967	19.214451
48.003717	1661.829246	19.219469
48.339448	1655.473452	19.224487
48.157002	1670.590346	19.229504
47.895272	1666.558107	19.234522
48.124723	1661.873070	19.239539
48.443168	1654.616188	19.244557
48.351068	1660.014472	19.249575
48.469063	1688.111202	19.254592
48.197398	1672.995701	19.259610
48.628324	1667.419970	19.264627
48.284597	1673.842310	19.269645
48.277227	1678.666184	19.274663
48.535038	1672.127631	19.279680
48.520029	1663.664199	19.284698
48.516659	1673.263874	19.289715
48.435136	1681.439956	19.294733
48.872637	1674.190256	19.299751
48.765684	1669.263329	19.304768
48.660273	1665.188136	19.309786
48.771220	1668.586844	19.314803
48.643086	1664.199528	19.319821
48.902024	1667.746481	19.324839
49.064088	1700.466777	19.329856
48.987193	1706.409990	19.334874
49.058507	1689.542576	19.339891
49.256788	1690.336056	19.344909
49.337424	1697.909486	19.349927
49.304374	1688.416263	19.354944
49.334381	1694.614487	19.359962
49.617722	1708.040906	19.364979
49.386890	1695.434947	19.369997
49.399053	1689.148647	19.375015
49.311414	1686.829006	19.380032
49.391297	1680.564288	19.385050
49.489526	1695.584050	19.390067
49.348369	1681.605593	19.395085
49.348031	1668.444747	19.400103
49.792524	1701.280250	19.405120
49.659239	1723.182160	19.410138
50.012183	1709.236475	19.415155
49.764235	1710.451751	19.420173
49.765864	1713.432599	19.425191
49.733472	1737.045454	19.430208
49.636416	1718.396653	19.435226
50.072623	1711.519710	19.440243
49.799643	1729.626602	19.445261
50.108512	1726.685346	19.450279
50.259040	1739.594677	19.455296
50.392220	1759.348902	19.460314
51.095431	1754.610644	19.465331
50.611145	1737.501491	19.470349
50.507251	1705.310150	19.475367
50.717233	1710.687071	19.480384
50.528706	1700.593874	19.485402
50.812021	1702.268886	19.490419
50.385221	1721.088151	19.495437
50.973976	1725.944904	19.500455
51.123601	1735.442973	19.505472
50.686330	1716.263308	19.510490
50.659193	1718.208475	19.515507
51.196051	1736.997823	19.520525
51.101523	1729.816232	19.525543
51.239742	1727.913107	19.530560
51.014912	1741.906107	19.535578
51.233320	1729.099533	19.540595
51.047892	1736.300105	19.545613
51.379697	1732.396396	19.550631
51.625304	1718.856647	19.555648
51.362337	1722.425990	19.560666
51.686153	1718.197392	19.565683
51.503735	1735.498642	19.570701
51.186991	1737.680605	19.575719
51.636655	1712.651119	19.580736
51.338616	1728.562997	19.585754
51.479369	1729.512707	19.590771
51.606060	1734.558097	19.595789
51.613981	1726.412626	19.600807
51.645061	1724.611145	19.605824
51.384993	1740.681097	19.610842
51.729636	1731.985595	19.615859
51.423336	1734.598913	19.620877
51.343068	1733.540977	19.625895
51.568711	1751.206222	19.630912
51.565582	1767.452401	19.635930
51.904168	1754.549093	19.640947
51.527525	1766.531690	19.645965
52.133431	1778.874074	19.650983
52.379244	1782.235662	19.656000
51.720210	1792.124625	19.661018
52.602319	1784.702408	19.666035
52.782058	1776.942412	19.671053
52.660680	1777.614541	19.676071
52.832041	1783.504658	19.681088
53.065778	1771.698168	19.686106
53.043728	1779.960027	19.691123
52.618849	1772.274358	19.696141
52.694381	1789.814385	19.701159
53.137256	1794.837364	19.706176
52.717709	1784.809544	19.711194
52.874159	1764.528564	19.716211
52.689816	1780.281677	19.721229
52.632971	1789.628995	19.726247
52.824340	1781.140055	19.731264
52.687025	1777.591358	19.736282
53.248783	1776.512547	19.741299
52.731067	1782.317750	19.746317
52.794276	1786.657355	19.751335
53.090465	1803.892682	19.756352
53.306774	1800.326285	19.761370
53.364927	1794.477430	19.766387
53.330191	1806.022730	19.771405
53.232073	1806.510147	19.776423
53.610984	1804.864818	19.781440
53.609409	1806.963418	19.786458
53.602176	1816.359924	19.791475
53.935389	1822.441574	19.796493
53.999014	1834.119628	19.801511
54.188205	1825.108490	19.806528
54.171802	1818.438450	19.811546
54.167505	1813.506322	19.816563
53.951339	1817.235735	19.821581
53.990799	1814.212136	19.826599
54.377284	1812.248688	19.831616
54.223690	1816.469827	19.836634
54.372925	1820.189342	19.841651
54.489481	1827.527025	19.846669
54.528377	1835.557824	19.851687
54.533496	1837.712299	19.856704
54.568736	1834.709567	19.861722
54.623626	1816.912430	19.866739
54.476497	1819.943958	19.871757
54.281484	1833.057976	19.876775
54.587325	1822.605011	19.881792
54.635180	1830.128521	19.886810
54.730546	1844.391868	19.891827
54.657418	1836.975733	19.896845
54.566078	1826.554545	19.901863
54.744359	1834.075104	19.906880
54.559938	1841.657077	19.911898
54.911012	1848.726339	19.916915
55.010901	1841.794797	19.921933
55.117890	1845.460485	19.926951
55.200088	1849.715882	19.931968
55.336087	1842.255051	19.936986
55.160602	1852.551553	19.942003
55.349605	1845.740789	19.947021
55.129598	1865.167565	19.952039
55.648829	1855.547158	19.957056
55.271761	1852.223851	19.962074
55.384314	1852.559551	19.967091
55.441022	1854.000918	19.972109
55.438507	1851.786650	19.977127
55.666710	1878.331371	19.982144
55.773482	1890.931979	19.987162
56.151488	1870.268253	19.992179
56.172991	1870.547360	19.997197
56.106355	1881.023690	20.002215
56.178893	1888.122169	20.007232
56.119051	1880.653728	20.012250
56.129237	1868.757161	20.017267
56.195492	1875.496212	20.022285
56.085088	1882.164969	20.027303
56.362334	1889.863258	20.032320
56.249482	1886.854875	20.037338
56.422173	1863.006421	20.042355
56.322556	1864.488283	20.047373
56.010302	1892.682463	20.052391
56.266943	1896.221584	20.057408
56.288519	1881.091271	20.062426
56.467673	1881.873457	20.067443
56.841987	1891.028846	20.072461
56.704530	1910.639146	20.077479
57.028036	1917.413250	20.082496
57.073645	1902.205042	20.087514
57.137766	1885.723073	20.092531
57.108705	1902.055455	20.097549
56.920907	1919.851210	20.102567
57.315844	1898.398481	20.107584
56.965787	1914.702832	20.112602
57.023815	1908.408174	20.117619
57.623018	1893.963844	20.122637
57.162718	1894.987791	20.127655
57.256928	1903.356465	20.132672
56.923498	1908.810656	20.137690
57.181735	1906.427726	20.142707
57.620342	1904.549632	20.147725
57.382256	1921.402701	20.152743
57.790147	1914.748810	20.157760
57.690515	1917.845132	20.162778
57.807790	1929.513803	20.167795
57.965832	1931.369747	20.172813
57.810266	1919.449851	20.177831
57.504948	1931.394219	20.182848
57.774283	1928.133734	20.187866
58.067042	1924.762313	20.192883
58.486573	1949.240893	20.197901
58.453185	1943.124681	20.202919
58.532785	1930.281932	20.207936
58.470171	1932.111949	20.212954
58.311380	1941.972075	20.217971
58.824472	1947.723715	20.222989
58.554953	1933.792217	20.228007
58.607253	1935.219953	20.233024
58.923665	1938.086144	20.238042
58.676939	1925.637808	20.243059
59.031251	1932.913424	20.248077
58.741524	1948.643482	20.253095
58.871920	1938.840767	20.258112
58.290362	1937.122684	20.263130
58.694274	1933.951257	20.268147
58.844165	1923.615118	20.273165
58.696983	1926.402135	20.278183
58.558355	1944.597098	20.283200
58.978796	1965.147857	20.288218
59.157703	1956.427657	20.293235
59.566259	1952.596923	20.298253
59.469691	1975.272307	20.303271
59.441439	1984.960918	20.308288
59.791542	1967.699853	20.313306
59.891649	1954.067623	20.318323
60.076720	1959.915196	20.323341
59.649528	1965.587126	20.328359
59.879838	1946.238699	20.333376
60.044797	1977.139475	20.338394
59.684752	1960.440268	20.343411
60.123760	1953.182119	20.348429
59.816395	1960.254744	20.353447
59.779792	1954.865004	20.358464
60.111121	1964.775725	20.363482
60.086942	1971.162016	20.368499
59.836075	1968.808784	20.373517
59.581230	1974.077210	20.378535
59.672256	1968.466217	20.383552
59.820755	1963.746739	20.388570
59.911557	1990.348112	20.393587
60.365408	1985.782856	20.398605
60.365511	1990.758518	20.403623
60.241093	1998.257438	20.408640
60.543404	2008.149857	20.413658
60.591273	2019.799362	20.418675
60.848245	2018.384751	20.423693
61.020250	2027.138005	20.428711
61.074911	2026.264702	20.433728
61.111415	2025.810071	20.438746
61.029952	2015.718754	20.443763
61.108853	2014.136263	20.448781
61.042951	2028.914627	20.453799
61.174657	2026.372502	20.458816
61.347230	2017.372658	20.463834
61.372647	2025.110267	20.468851
61.115056	2009.992106	20.473869
60.835407	2029.252895	20.478887
61.709773	2032.997297	20.483904
61.651679	2036.264995	20.488922
61.473178	2038.372393	20.493939
61.910990	2041.540433	20.498957
61.840081	2045.417815	20.503975
61.721924	2062.554413	20.508992
61.544274	2045.203434	20.514010
61.712034	2035.208200	20.519027
62.134895	2040.948511	20.524045
61.924641	2025.505937	20.529063
62.032835	2040.739017	20.534080
62.393879	2060.776392	20.539098
62.218650	2053.781378	20.544115
62.775889	2054.817180	20.549133
62.512833	2055.306668	20.554151
62.497692	2058.836416	20.559168
62.754424	2065.758012	20.564186
62.396312	2054.089354	20.569203
62.615005	2054.897490	20.574221
62.719914	2072.240206	20.579239
62.715169	2089.022721	20.584256
62.898052	2072.052607	20.589274
62.696320	2066.644651	20.594291
62.792375	2050.548495	20.599309
62.621285	2068.198872	20.604327
62.822330	2074.710361	20.609344
63.045391	2063.482079	20.614362
62.655733	2063.271851	20.619379
63.080561	2073.686389	20.624397
62.880426	2090.720051	20.629415
63.100725	2093.558461	20.634432
63.083779	2087.708816	20.639450
63.033288	2095.074133	20.644467
63.191122	2098.845632	20.649485
63.587796	2112.714817	20.654503
63.908315	2113.196737	20.659520
63.880800	2105.511662	20.664538
63.784777	2135.645890	20.669555
64.000811	2119.130204	20.674573
64.236741	2112.949937	20.679591
64.063213	2110.704846	20.684608
64.137116	2107.453983	20.689626
63.876397	2113.325681	20.694643
64.309225	2124.692402	20.699661
64.034959	2118.576069	20.704679
64.183556	2102.876714	20.709696
64.440911	2089.414802	20.714714
64.491717	2116.697882	20.719731
64.484032	2118.172548	20.724749
64.349943	2112.271299	20.729767
64.531013	2103.788213	20.734784
64.727325	2099.942622	20.739802
64.905926	2132.175566	20.744819
65.126950	2129.457277	20.749837
64.914868	2132.715112	20.754855
64.820579	2147.152475	20.759872
64.918239	2134.681505	20.764890
65.004974	2133.026165	20.769907
64.802953	2138.889452	20.774925
65.025597	2128.934390	20.779943
64.989193	2134.080176	20.784960
65.043215	2138.321711	20.789978
64.920063	2156.647512	20.794995
65.421258	2157.187948	20.800013
65.458648	2153.798942	20.805031
65.259882	2166.203458	20.810048
65.639239	2165.517889	20.815066
65.685070	2167.825891	20.820083
65.700164	2160.606794	20.825101
66.009176	2171.517519	20.830119
66.228712	2153.842661	20.835136
66.520532	2155.741771	20.840154
66.437192	2171.120095	20.845171
65.923019	2162.251556	20.850189
66.280500	2145.307224	20.855207
66.077765	2153.525040	20.860224
66.041855	2178.640268	20.865242
66.263209	2210.805496	20.870259
66.497191	2188.454908	20.875277
66.709385	2166.606584	20.880295
66.643023	2188.772756	20.885312
66.447412	2207.233404	20.890330
66.365921	2206.105177	20.895347
66.452981	2188.657350	20.900365
66.490303	2200.034472	20.905383
66.608959	2213.127883	20.910400
66.844011	2224.540054	20.915418
66.865582	2223.443705	20.920435
67.136121	2210.730658	20.925453
67.288127	2208.357560	20.930471
67.014861	2218.250950	20.935488
67.479925	2223.499500	20.940506
67.409441	2211.429907	20.945523
67.566329	2203.254057	20.950541
67.872734	2203.458342	20.955559
67.636481	2222.294754	20.960576
67.578320	2210.998090	20.965594
67.612087	2196.204272	20.970611
67.808358	2223.345907	20.975629
68.416753	2231.051745	20.980647
68.148312	2208.769288	20.985664
68.392960	2191.938515	20.990682
67.782619	2191.387060	20.995699
67.826295	2210.668160	21.000717
68.115337	2219.648205	21.005735
68.035268	2220.826528	21.010752
68.187935	2224.783723	21.015770
68.386059	2237.961743	21.020787
68.198567	2231.049959	21.025805
68.025250	2221.784667	21.030823
68.190766	2225.080896	21.035840
68.342380	2241.472647	21.040858
68.787686	2243.193282	21.045875
68.871986	2236.943452	21.050893
69.215365	2262.093468	21.055911
69.196468	2270.355857	21.060928
69.347522	2254.765666	21.065946
68.684023	2238.487199	21.070963
69.145801	2245.533728	21.075981
69.252273	2261.791350	21.080999
69.113380	2260.930828	21.086016
69.330456	2238.702526	21.091034
68.954163	2243.082901	21.096051
69.118105	2253.546380	21.101069
69.434588	2236.253961	21.106087
69.515030	2272.824628	21.111104
69.489888	2283.218404	21.116122
69.549256	2282.229663	21.121139
69.491863	2280.606193	21.126157
69.550245	2274.100044	21.131175
69.438111	2275.408354	21.136192
69.961697	2294.320248	21.141210
70.449467	2295.460544	21.146227
70.098244	2304.566316	21.151245
70.318432	2315.874140	21.156263
70.330801	2312.465812	21.161280
70.050142	2296.257661	21.166298
70.317107	2290.243132	21.171315
70.617974	2295.977325	21.176333
70.893058	2320.057407	21.181351
70.639196	2312.654373	21.186368
71.016123	2291.761361	21.191386
70.766332	2294.128072	21.196403
70.533142	2303.855964	21.201421
71.112821	2308.228366	21.206439
70.907942	2302.791717	21.211456
71.108252	2322.545318	21.216474
71.163216	2318.986667	21.221491
71.042595	2321.996691	21.226509
71.127008	2320.039205	21.231527
70.980440	2350.887307	21.236544
71.157664	2320.510318	21.241562
71.154283	2330.127824	21.246579
71.185606	2348.364165	21.251597
71.896299	2340.070948	21.256615
71.705468	2355.106155	21.261632
72.025028	2376.509926	21.266650
71.492590	2364.368835	21.271667
71.778216	2339.328534	21.276685
71.882584	2337.418134	21.281703
71.776400	2345.329300	21.286720
71.914108	2334.661488	21.291738
72.244377	2354.504070	21.296755
71.986976	2385.929914	21.301773
72.078826	2386.730194	21.306791
72.403599	2369.955266	21.311808
72.650774	2359.822801	21.316826
72.788219	2375.056694	21.321843
72.365116	2365.877760	21.326861
72.588719	2368.510099	21.331879
72.774826	2375.040915	21.336896
72.971929	2361.723935	21.341914
73.203296	2359.288299	21.346931
73.012400	2374.419780	21.351949
72.855732	2363.828342	21.356967
72.940270	2372.839515	21.361984
73.158967	2380.994604	21.367002
72.941725	2392.373191	21.372019
73.445200	2400.014970	21.377037
73.752198	2397.741606	21.382055
73.432416	2393.945303	21.387072
73.548744	2409.617886	21.392090
73.559250	2405.842581	21.397107
73.372568	2410.445371	21.402125
73.757056	2398.825268	21.407143
73.352911	2396.620013	21.412160
73.954327	2393.254467	21.417178
74.165410	2422.191550	21.422195
74.163144	2449.563604	21.427213
74.235683	2435.635551	21.432231
73.946845	2414.597504	21.437248
74.287385	2408.681974	21.442266
74.384057	2420.667463	21.447283
74.302955	2440.299437	21.452301
74.493586	2432.328092	21.457319
73.868472	2431.813807	21.462336
74.191683	2443.865998	21.467354
74.425374	2435.362424	21.472371
74.505654	2445.088008	21.477389
74.631379	2448.754878	21.482407
74.829880	2469.663116	21.487424
75.076586	2484.473614	21.492442
75.480789	2469.126175	21.497459
75.474923	2472.945680	21.502477
75.544057	2478.521808	21.507495
75.576638	2481.784457	21.512512
75.817414	2461.910605	21.517530
76.053461	2460.995595	21.522547
75.736531	2455.420738	21.527565
76.332651	2440.648408	21.532583
76.077918	2434.553126	21.537600
75.681128	2445.421940	21.542618
75.978061	2432.266525	21.547635
75.850597	2442.452352	21.552653
76.121919	2461.726363	21.557671
76.016953	2467.469619	21.562688
76.085259	2483.544836	21.567706
76.185076	2477.377370	21.572723
76.235205	2468.078451	21.577741
76.385518	2448.200079	21.582759
76.085136	2457.715387	21.587776
76.463279	2483.132617	21.592794
76.558285	2477.242084	21.597811
76.643066	2499.277445	21.602829
76.801974	2494.109108	21.607847
76.687421	2504.494976	21.612864
76.631608	2516.093202	21.617882
76.832750	2498.894537	21.622899
76.752708	2488.867427	21.627917
76.569144	2494.158596	21.632935
76.780304	2521.391590	21.637952
76.860933	2527.721036	21.642970
77.258129	2515.347680	21.647987
77.411978	2521.351490	21.653005
77.496563	2522.007724	21.658023
77.536835	2515.212188	21.663040
77.427521	2559.099011	21.668058
78.065528	2562.475777	21.673075
77.918302	2546.497835	21.678093
77.858366	2531.189238	21.683111
77.833368	2540.407753	21.688128
77.998281	2564.714463	21.693146
78.076879	2557.865141	21.698163
78.266906	2542.526645	21.703181
78.467276	2530.008072	21.708199
78.372722	2546.748357	21.713216
78.273913	2556.868314	21.718234
78.578943	2536.234059	21.723251
78.348045	2562.873345	21.728269
78.455213	2568.203099	21.733287
78.891501	2559.722270	21.738304
78.873164	2581.798210	21.743322
78.921529	2587.923595	21.748339
78.776600	2589.503846	21.753357
78.953757	2566.889402	21.758375
79.311725	2565.824535	21.763392
79.100028	2578.034305	21.768410
79.335221	2582.565270	21.773427
79.116944	2580.199766	21.778445
79.108716	2584.727261	21.783463
79.649201	2597.206791	21.788480
79.559471	2616.202320	21.793498
79.961598	2598.916993	21.798515
79.644006	2614.417034	21.803533
79.849051	2611.073442	21.808551
79.700080	2606.980986	21.813568
79.675234	2616.923037	21.818586
79.813681	2623.635234	21.823603
80.044993	2641.061628	21.828621
80.248551	2631.682934	21.833639
80.638700	2622.985317	21.838656
80.400401	2628.957132	21.843674
80.527489	2643.954455	21.848691
80.595677	2645.548111	21.853709
80.627952	2617.717350	21.858727
80.779503	2628.484269	21.863744
80.552799	2666.617231	21.868762
81.131800	2673.025977	21.873779
81.035995	2659.783121	21.878797
81.149266	2653.319113	21.883815
81.355947	2666.626777	21.888832
81.145913	2673.443619	21.893850
81.388279	2652.128521	21.898867
81.151432	2647.293205	21.903885
81.273635	2654.709966	21.908903
81.385139	2656.661570	21.913920
81.149055	2669.476143	21.918938
81.988201	2679.885420	21.923955
81.408144	2692.028607	21.928973
81.697205	2665.952119	21.933991
81.927654	2685.964556	21.939008
81.650105	2690.198836	21.944026
82.069965	2700.881712	21.949043
82.181152	2711.284152	21.954061
82.236163	2721.367383	21.959079
82.391912	2721.631408	21.964096
82.417060	2711.931802	21.969114
82.614334	2707.935037	21.974131
82.608076	2725.736563	21.979149
82.517051	2704.931142	21.984167
82.839620	2685.786492	21.989184
82.893882	2722.507416	21.994202
83.047699	2733.031548	21.999219
83.062101	2731.963213	22.004237
83.134185	2717.772221	22.009255
83.532581	2710.297234	22.014272
83.294852	2726.237670	22.019290
83.373048	2725.739618	22.024307
83.458281	2720.637309	22.029325
83.406571	2724.739216	22.034343
83.407770	2733.792123	22.039360
83.620704	2725.516787	22.044378
83.493292	2709.473795	22.049395
83.402073	2727.215947	22.054413
83.929097	2741.942781	22.059431
83.711954	2749.325123	22.064448
83.741105	2768.307494	22.069466
84.122343	2765.790149	22.074483
84.195380	2747.288935	22.079501
83.948860	2744.349805	22.084519
84.308377	2766.775329	22.089536
84.245310	2772.146471	22.094554
84.567269	2779.434629	22.099571
84.538286	2786.399139	22.104589
84.646579	2770.266749	22.109607
84.938333	2779.965277	22.114624
84.768229	2758.473931	22.119642
85.099973	2762.731747	22.124659
84.995445	2769.077126	22.129677
85.308314	2789.183544	22.134695
85.137726	2801.577026	22.139712
85.292546	2801.979180	22.144730
85.480940	2810.166864	22.149747
85.514441	2793.548056	22.154765
85.731744	2778.975383	22.159783
85.545469	2804.298836	22.164800
85.430341	2810.446207	22.169818
85.846992	2808.793753	22.174835
86.201812	2811.563914	22.179853
86.312883	2830.434807	22.184871
86.287876	2828.505376	22.189888
86.116747	2813.346155	22.194906
86.202932	2825.611805	22.199923
86.340250	2822.565344	22.204941
86.480983	2803.507674	22.209959
86.668898	2813.698515	22.214976
86.305072	2832.603793	22.219994
86.688083	2838.249037	22.225011
86.921351	2846.351186	22.230029
86.721618	2862.415978	22.235047
87.211304	2842.238140	22.240064
87.147078	2842.988260	22.245082
87.166383	2853.936026	22.250099
87.391854	2848.987447	22.255117
87.097204	2851.701963	22.260135
87.286450	2843.619036	22.265152
87.288366	2849.354615	22.270170
87.193315	2868.117113	22.275187
87.709663	2883.735299	22.280205
87.643808	2870.376304	22.285223
87.864261	2856.454527	22.290240
87.699461	2864.856289	22.295258
87.679016	2882.794181	22.300275
88.137802	2889.355347	22.305293
88.105381	2895.471961	22.310311
88.272571	2890.523551	22.315328
88.399859	2907.141559	22.320346
88.425326	2905.566133	22.325363
88.303091	2900.481906	22.330381
88.456047	2916.145410	22.335399
88.675990	2894.388661	22.340416
88.792165	2909.036320	22.345434
88.667950	2918.747969	22.350451
88.651605	2925.371520	22.355469
88.701131	2930.699313	22.360487
89.107014	2929.752080	22.365504
89.143970	2936.273336	22.370522
89.154461	2918.176690	22.375539
89.348983	2934.621040	22.380557
89.191185	2951.858571	22.385575
89.714107	2954.338811	22.390592
89.679490	2949.437309	22.395610
89.743221	2963.207970	22.400627
89.732202	2956.026275	22.405645
89.741514	2958.844305	22.410663
89.681272	2954.192674	22.415680
89.829054	2974.828520	22.420698
89.812218	2981.878305	22.425715
90.155150	2976.212920	22.430733
90.154914	2996.686072	22.435751
90.243296	2981.078144	22.440768
90.263913	3000.559591	22.445786
90.333087	3025.850841	22.450803
90.741062	3009.307112	22.455821
91.150394	3002.503914	22.460839
91.259926	3008.408755	22.465856
91.028054	3018.328587	22.470874
90.994092	3005.420449	22.475891
91.391772	3000.334127	22.480909
91.225125	3014.717634	22.485927
91.368201	3002.635849	22.490944
91.568023	3025.079871	22.495962
91.940519	3044.762057	22.500979
92.102451	3038.223319	22.505997
92.034201	3026.895837	22.511015
92.261494	3023.658900	22.516032
91.904166	3029.512955	22.521050
92.095688	3031.060290	22.526067
92.411369	3033.855462	22.531085
92.191182	3028.936966	22.536103
92.486204	3021.590118	22.541120
92.234498	3033.504927	22.546138
92.265448	3042.751501	22.551155
92.601687	3015.355169	22.556173
92.262164	3043.963392	22.561191
92.537254	3055.659100	22.566208
92.778271	3049.162599	22.571226
92.662450	3071.337228	22.576243
92.944916	3055.280079	22.581261
92.961282	3067.176795	22.586279
93.363447	3075.066336	22.591296
93.067053	3091.884064	22.596314
93.306683	3114.588733	22.601331
93.704000	3093.482238	22.606349
93.121419	3080.697166	22.611367
93.571495	3089.001582	22.616384
93.965090	3116.253707	22.621402
94.149044	3112.375955	22.626419
94.504422	3114.008416	22.631437
94.221125	3120.862558	22.636455
94.489634	3115.434985	22.641472
94.462671	3105.629779	22.646490
94.587683	3115.501528	22.651507
94.908603	3111.323224	22.656525
94.790784	3116.437815	22.661543
94.870806	3096.603291	22.666560
94.853448	3101.892594	22.671578
94.452901	3134.009088	22.676595
94.686051	3115.207188	22.681613
94.806198	3099.933026	22.686631
94.933792	3104.935417	22.691648
95.005239	3101.282731	22.696666
95.067446	3118.322499	22.701683
95.305052	3111.580894	22.706701
95.487239	3105.918602	22.711719
95.513433	3114.083058	22.716736
95.273877	3136.911227	22.721754
95.222885	3130.357836	22.726771
95.737127	3138.685138	22.731789
95.673307	3135.625793	22.736807
95.523800	3148.264270	22.741824
95.685882	3168.281152	22.746842
95.570725	3164.899219	22.751859
95.935130	3166.887044	22.756877
96.107731	3176.068170	22.761895
96.213025	3176.923942	22.766912
96.635245	3204.492521	22.771930
96.323227	3204.485855	22.776947
96.997780	3194.364106	22.781965
96.886997	3201.886945	22.786983
96.940587	3223.695846	22.792000
97.281409	3222.844968	22.797018
97.120511	3207.787396	22.802035
97.137844	3187.933194	22.807053
97.396302	3224.840448	22.812071
97.268501	3241.570447	22.817088
97.694907	3233.150523	22.822106
97.840948	3228.061618	22.827123
97.971554	3219.897250	22.832141
97.853452	3232.132421	22.837159
97.944227	3240.960020	22.842176
97.967130	3232.750259	22.847194
98.322475	3220.736171	22.852211
98.497951	3246.607202	22.857229
98.722200	3258.836213	22.862247
98.585755	3257.736868	22.867264
98.578627	3270.798524	22.872282
98.586805	3259.076590	22.877299
98.861926	3241.091334	22.882317
98.562319	3259.894209	22.887335
98.474541	3252.326283	22.892352
98.856275	3262.180507	22.897370
99.082447	3291.581251	22.902387
99.274743	3282.084942	22.907405
99.286102	3277.021425	22.912423
99.355811	3290.350294	22.917440
99.594935	3276.215431	22.922458
99.327782	3281.550401	22.927475
100.090260	3298.591379	22.932493
100.089964	3318.518763	22.937511
99.855024	3307.564449	22.942528
100.179269	3313.984070	22.947546
100.125677	3313.279453	22.952563
100.238914	3306.886036	22.957581
100.362345	3313.420916	22.962599
100.327099	3326.046366	22.967616
100.530188	3312.634478	22.972634
100.400458	3324.631707	22.977651
100.545720	3343.043096	22.982669
100.712705	3331.090162	22.987687
100.663363	3323.627847	22.992704
101.261025	3334.389256	22.997722
101.015350	3351.173296	23.002739
101.043393	3351.436981	23.007757
101.439346	3351.871543	23.012775
101.367523	3355.835223	23.017792
101.693795	3351.218022	23.022810
101.657269	3362.594624	23.027827
101.641925	3359.093804	23.032845
101.758621	3351.923102	23.037863
101.492009	3360.897216	23.042880
101.795528	3372.900642	23.047898
101.838348	3397.641006	23.052915
102.395531	3390.672868	23.057933
102.451611	3372.686058	23.062951
101.979591	3379.802184	23.067968
102.171565	3386.103547	23.072986
102.442379	3405.258364	23.078003
103.019782	3396.033162	23.083021
103.334095	3398.700688	23.088039
103.352507	3409.093931	23.093056
103.531145	3403.081953	23.098074
103.434975	3406.312535	23.103091
103.584379	3398.365812	23.108109
103.572502	3412.567634	23.113127
103.654343	3410.705900	23.118144
103.647652	3395.687027	23.123162
103.582828	3398.290244	23.128179
103.756776	3412.457227	23.133197
104.135019	3400.520115	23.138215
103.766120	3390.072279	23.143232
103.892464	3396.660645	23.148250
103.633680	3412.261008	23.153267
104.005892	3413.604921	23.158285
103.819608	3429.668474	23.163303
103.848117	3430.500927	23.168320
104.322159	3454.824296	23.173338
104.500522	3465.173235	23.178355
104.548351	3464.470159	23.183373
104.789977	3488.322975	23.188391
104.851419	3497.283509	23.193408
104.854547	3484.605631	23.198426
105.031703	3494.550890	23.203443
105.300833	3507.020888	23.208461
105.573143	3504.150789	23.213479
105.249628	3516.117987	23.218496
105.758930	3515.398493	23.223514
105.737068	3528.468708	23.228531
105.917686	3523.605468	23.233549
105.984368	3529.410118	23.238567
105.868823	3536.169210	23.243584
106.137619	3511.206950	23.248602
106.250646	3525.859652	23.253619
106.584051	3537.869882	23.258637
106.972402	3543.465888	23.263655
106.836681	3523.404676	23.268672
107.257195	3519.485963	23.273690
107.299516	3519.159549	23.278707
107.099945	3522.509396	23.283725
107.180483	3530.595415	23.288743
106.930959	3523.548526	23.293760
107.386899	3503.895043	23.298778
107.131542	3522.583848	23.303795
107.372539	3543.250915	23.308813
107.826256	3550.879647	23.313831
107.115933	3547.602073	23.318848
107.154586	3549.007020	23.323866
107.801266	3561.416843	23.328883
107.990964	3579.783971	23.333901
107.976157	3577.062670	23.338919
108.264325	3601.823249	23.343936
108.379751	3581.279161	23.348954
108.502807	3584.885332	23.353971
108.395274	3590.661710	23.358989
108.715311	3590.729920	23.364007
108.080982	3587.402776	23.369024
108.678395	3592.524529	23.374042
109.030745	3601.980711	23.379059
108.933740	3616.354647	23.384077
108.839119	3610.536942	23.389095
108.941444	3620.366901	23.394112
109.311224	3638.486645	23.399130
109.274780	3636.345240	23.404147
109.277955	3646.233328	23.409165
109.600966	3631.276077	23.414183
109.705172	3639.850328	23.419200
110.028715	3650.871214	23.424218
109.909010	3661.377599	23.429235
109.781809	3651.997041	23.434253
109.975925	3673.877838	23.439271
110.134918	3663.845305	23.444288
110.720214	3671.077385	23.449306
110.680571	3689.406167	23.454323
110.565820	3692.088150	23.459341
110.884101	3703.431177	23.464359
110.761451	3700.545405	23.469376
111.079769	3684.094899	23.474394
111.336858	3687.723038	23.479411
111.259943	3706.727239	23.484429
111.386749	3709.117558	23.489447
110.994059	3705.678419	23.494464
111.397783	3709.360281	23.499482
111.494332	3716.784746	23.504499
111.527620	3721.537192	23.509517
111.895909	3743.838488	23.514535
111.804972	3745.827816	23.519552
111.710474	3734.082923	23.524570
112.066803	3744.854579	23.529587
112.226261	3765.366334	23.534605
112.450120	3770.244579	23.539623
112.669110	3761.455719	23.544640
112.504394	3776.390953	23.549658
112.680504	3791.760991	23.554675
112.925385	3799.222793	23.559693
112.984194	3794.003835	23.564711
112.828147	3800.905748	23.569728
113.133991	3814.201760	23.574746
113.718012	3804.569544	23.579763
113.397170	3813.101731	23.584781
113.865748	3790.268065	23.589799
113.776088	3797.973320	23.594816
114.019026	3815.076114	23.599834
114.126934	3826.016622	23.604851
114.834889	3830.437757	23.609869
114.572474	3824.731155	23.614887
114.384500	3816.555929	23.619904
114.724835	3812.350806	23.624922
114.880553	3828.013010	23.629939
114.683208	3834.353887	23.634957
115.007512	3812.989205	23.639975
114.859522	3840.520670	23.644992
114.901605	3825.573040	23.650010
115.067764	3805.328715	23.655027
115.137782	3816.287090	23.660045
115.293076	3841.838461	23.665063
115.430167	3862.130039	23.670080
115.941268	3851.079427	23.675098
115.657483	3857.342674	23.680115
115.535648	3847.158604	23.685133
115.667257	3850.246923	23.690151
115.674626	3863.663945	23.695168
115.975354	3861.763825	23.700186
116.331477	3869.034851	23.705203
115.906542	3882.229639	23.710221
116.274642	3872.628728	23.715239
116.213734	3878.856928	23.720256
116.110075	3878.755204	23.725274
116.690523	3903.248498	23.730291
116.613811	3912.696442	23.735309
116.873513	3893.566199	23.740327
116.796260	3916.905475	23.745344
117.119064	3921.415276	23.750362
117.303374	3929.470971	23.755379
117.388332	3929.272337	23.760397
117.507007	3941.439418	23.765415
117.689652	3935.438777	23.770432
117.348502	3951.452480	23.775450
117.561051	3952.433084	23.780467
117.689592	3951.245024	23.785485
118.132933	3970.811971	23.790503
118.356728	3970.060112	23.795520
118.164757	3985.470101	23.800538
118.479549	3998.615393	23.805555
118.292339	3997.564537	23.810573
118.798130	3989.471621	23.815591
119.208929	4014.985784	23.820608
119.117262	4015.205287	23.825626
119.035837	4007.241672	23.830643
118.975645	4013.657986	23.835661
119.439890	4017.500386	23.840679
119.537158	4024.160750	23.845696
119.409826	4033.459660	23.850714
119.601774	4036.323492	23.855731
119.658215	4059.566486	23.860749
119.656395	4046.730903	23.865767
119.952946	4042.242025	23.870784
120.104994	4060.602561	23.875802
120.392307	4076.169653	23.880819
120.429610	4070.378399	23.885837
120.340180	4064.657691	23.890855
120.914619	4084.248393	23.895872
120.779606	4098.489300	23.900890
121.141883	4088.798869	23.905907
121.328482	4102.321713	23.910925
121.231287	4110.596055	23.915943
121.304116	4092.429863	23.920960
121.337102	4082.338358	23.925978
121.645619	4107.551874	23.930995
121.889469	4130.625039	23.936013
121.818245	4133.348919	23.941031
122.065750	4128.246103	23.946048
122.020572	4120.521704	23.951066
122.237748	4109.399009	23.956083
122.373976	4124.948598	23.961101
122.205952	4139.142243	23.966119
122.417191	4144.348857	23.971136
122.510366	4153.388186	23.976154
122.862990	4146.851134	23.981171
122.665436	4154.450383	23.986189
122.842329	4160.042188	23.991207
123.131399	4162.113260	23.996224
123.145449	4191.236017	24.001242
123.051543	4190.381532	24.006259
123.087368	4184.599141	24.011277
123.610520	4186.572486	24.016295
123.707644	4197.919351	24.021312
123.408048	4210.581328	24.026330
124.010584	4223.330857	24.031347
123.829065	4223.533322	24.036365
124.033462	4229.862701	24.041383
124.239331	4234.280896	24.046400
124.332241	4233.199880	24.051418
124.678863	4228.429065	24.056435
124.259706	4264.723240	24.061453
124.687154	4269.496943	24.066471
124.760767	4260.347784	24.071488
124.905831	4262.195431	24.076506
125.170488	4262.041113	24.081523
125.189919	4270.576181	24.086541
125.761594	4289.917217	24.091559
125.660425	4301.021343	24.096576
125.478245	4296.162693	24.101594
125.826557	4272.890729	24.106611
126.065781	4284.807855	24.111629
125.988034	4303.152321	24.116647
126.291594	4319.946849	24.121664
125.931018	4325.510203	24.126682
126.359638	4303.643375	24.131699
126.421791	4320.467951	24.136717
126.754928	4341.875164	24.141735
126.756126	4339.133369	24.146752
126.777490	4333.898961	24.151770
127.324783	4323.228636	24.156787
127.334923	4342.653074	24.161805
127.243218	4345.793352	24.166823
127.623065	4364.348097	24.171840
127.570141	4355.283567	24.176858
127.939071	4360.088621	24.181875
127.891058	4380.571498	24.186893
128.148891	4385.662231	24.191911
128.137007	4375.001591	24.196928
128.071281	4370.028403	24.201946
128.363760	4385.762271	24.206963
128.308557	4378.237031	24.211981
128.727167	4382.068167	24.216999
128.927857	4393.385466	24.222016
128.889805	4401.008479	24.227034
129.063510	4416.862789	24.232051
128.856775	4430.707989	24.237069
129.295864	4430.936648	24.242087
129.404550	4409.464258	24.247104
129.337413	4421.615964	24.252122
129.619609	4434.119001	24.257139
129.625745	4433.144432	24.262157
129.527010	4461.601313	24.267175
129.935509	4437.710513	24.272192
129.915485	4465.848106	24.277210
130.088723	4487.831927	24.282227
130.611955	4502.472696	24.287245
130.362828	4487.436328	24.292263
130.461303	4477.609722	24.297280
130.450044	4509.049795	24.302298
131.137748	4499.299040	24.307315
131.031520	4513.280459	24.312333
130.968536	4528.066538	24.317351
131.285141	4534.358605	24.322368
131.445598	4536.806089	24.327386
131.846938	4525.042839	24.332403
131.882894	4548.719863	24.337421
131.704591	4544.673862	24.342439
131.967780	4548.355134	24.347456
131.962832	4551.419309	24.352474
132.177352	4565.384784	24.357491
132.411806	4579.122573	24.362509
132.387506	4580.576598	24.367527
132.819145	4567.552822	24.372544
132.681024	4586.806398	24.377562
132.857872	4588.337421	24.382579
133.089776	4598.287534	24.387597
132.668944	4601.376342	24.392615
133.162409	4605.966018	24.397632
132.763884	4624.044185	24.402650
133.604983	4614.673518	24.407667
133.594451	4615.355599	24.412685
133.902096	4651.174292	24.417703
134.475852	4647.957134	24.422720
134.133906	4660.981587	24.427738
134.205075	4635.450971	24.432755
134.597222	4658.036647	24.437773
134.466837	4636.229042	24.442791
134.866728	4625.715935	24.447808
134.667671	4655.023985	24.452826
135.075069	4662.156208	24.457843
134.756380	4665.131696	24.462861
135.345558	4673.948430	24.467879
135.288702	4667.648503	24.472896
135.104461	4660.794831	24.477914
135.535574	4677.915518	24.482931
135.608467	4700.159131	24.487949
135.617438	4710.513076	24.492967
136.201808	4688.353835	24.497984
136.036491	4703.846351	24.503002
136.270135	4716.269057	24.508019
136.410237	4737.129979	24.513037
136.268809	4740.025405	24.518055
136.348719	4721.342352	24.523072
136.733353	4742.562479	24.528090
136.698573	4761.806676	24.533107
137.018601	4768.350634	24.538125
137.144036	4763.281167	24.543143
137.469262	4788.417835	24.548160
137.460980	4799.401851	24.553178
137.691786	4780.093798	24.558195
137.988142	4789.023942	24.563213
137.937985	4790.430290	24.568231
137.973482	4801.093690	24.573248
137.939081	4824.227251	24.578266
138.359386	4836.050709	24.583283
138.256582	4824.429589	24.588301
138.264075	4840.850376	24.593319
138.590870	4845.436168	24.598336
138.641860	4833.581362	24.603354
138.552192	4857.542999	24.608371
139.144971	4864.432480	24.613389
139.040962	4878.233940	24.618407
139.164831	4879.366266	24.623424
139.172486	4896.818581	24.628442
139.478906	4913.781786	24.633459
139.996330	4913.671920	24.638477
139.864092	4912.843413	24.643495
140.119240	4907.679632	24.648512
140.358704	4926.600767	24.653530
140.251699	4943.345306	24.658547
140.212293	4945.682572	24.663565
140.440981	4939.792836	24.668583
141.249080	4928.820344	24.673600
141.045548	4963.622642	24.678618
141.250960	4947.080403	24.683635
141.270744	4963.374878	24.688653
141.466863	4963.146841	24.693671
141.734171	4961.887352	24.698688
142.293294	4961.747762	24.703706
142.487875	4974.693668	24.708723
142.299345	4983.893414	24.713741
142.354364	4989.215891	24.718759
142.625992	4981.092651	24.723776
142.918193	4966.034879	24.728794
142.796779	4974.633370	24.733811
142.866270	4980.989678	24.738829
142.830072	4976.550790	24.743847
143.075905	4958.083345	24.748864
143.047890	4967.076244	24.753882
142.807066	4980.887014	24.758899
142.851483	5003.866873	24.763917
143.068400	5018.051260	24.768935
143.155012	4991.448995	24.773952
143.408763	5018.069114	24.778970
143.538587	5058.018949	24.783987
143.799186	5053.216429	24.789005
143.601599	5073.585169	24.794023
144.048633	5068.530970	24.799040
143.804124	5080.906201	24.804058
144.249235	5088.332787	24.809075
144.562230	5086.101948	24.814093
144.764578	5111.200780	24.819111
145.098393	5129.406956	24.824128
145.424964	5133.714520	24.829146
145.383630	5122.705864	24.834163
145.841971	5111.369770	24.839181
145.363446	5126.880205	24.844199
145.953637	5132.945026	24.849216
146.148795	5143.747637	24.854234
145.989183	5169.399291	24.859251
145.976594	5150.554231	24.864269
146.041549	5157.407039	24.869287
146.511108	5170.852959	24.874304
146.763806	5175.158568	24.879322
146.550048	5185.899637	24.884339
146.924461	5204.466917	24.889357
146.986705	5221.486158	24.894375
146.904180	5215.485138	24.899392
147.172595	5214.473483	24.904410
147.424295	5247.718883	24.909427
147.828393	5242.997322	24.914445
147.787428	5247.692819	24.919463
147.566169	5249.388902	24.924480
147.976606	5282.260897	24.929498
147.681017	5281.770785	24.934515
148.174836	5292.908808	24.939533
148.385195	5308.109923	24.944551
148.482889	5298.206155	24.949568
148.932688	5326.614537	24.954586
148.813936	5335.318694	24.959603
149.357284	5308.410888	24.964621
149.739367	5330.353914	24.969639
149.428517	5327.150892	24.974656
149.731464	5352.595312	24.979674
149.818676	5349.646208	24.984691
150.374845	5343.181723	24.989709
150.139046	5359.248362	24.994727
150.424113	5350.874278	24.999744
150.472440	5365.063609	25.004762
150.555624	5378.742453	25.009779
150.954512	5370.125530	25.014797
150.835547	5372.772077	25.019815
151.097514	5369.102734	25.024832
151.578030	5378.406740	25.029850
151.386784	5385.965781	25.034867
151.628395	5383.480939	25.039885
151.556760	5404.987211	25.044903
151.437680	5412.270946	25.049920
152.027570	5400.328242	25.054938
151.795539	5429.178614	25.059955
152.146892	5436.461012	25.064973
152.314645	5436.495540	25.069991
152.239994	5438.652476	25.075008
152.582557	5459.890379	25.080026
152.565444	5475.645798	25.085043
152.605406	5454.354589	25.090061
152.748954	5470.972072	25.095079
152.977443	5480.719371	25.100096
153.050161	5514.722109	25.105114
152.781314	5506.548524	25.110131
152.999074	5516.286200	25.115149
153.269214	5546.800343	25.120167
153.465800	5569.803534	25.125184
153.821891	5566.723738	25.130202
154.257343	5556.934479	25.135219
154.749342	5579.790838	25.140237
154.738111	5593.967382	25.145255
154.767664	5599.930131	25.150272
155.002994	5588.790390	25.155290
154.997552	5575.379708	25.160307
155.492087	5595.353655	25.165325
155.623251	5619.576839	25.170343
155.707268	5624.981754	25.175360
155.957052	5633.085790	25.180378
156.012677	5621.869413	25.185395
156.132175	5604.768992	25.190413
155.767972	5609.670375	25.195431
155.985196	5635.853866	25.200448
156.696078	5637.707013	25.205466
156.426254	5641.210462	25.210483
156.808241	5667.471118	25.215501
157.087037	5671.167011	25.220519
156.997028	5695.633167	25.225536
157.034012	5689.379528	25.230554
157.094393	5703.169123	25.235571
157.436580	5696.609922	25.240589
157.344848	5715.711944	25.245607
157.538333	5742.466101	25.250624
158.291014	5730.113946	25.255642
157.954309	5749.475001	25.260659
158.692251	5756.587764	25.265677
158.846842	5761.903502	25.270695
158.731895	5763.238748	25.275712
158.802364	5764.295313	25.280730
158.963060	5770.567580	25.285747
159.190690	5781.629064	25.290765
159.294679	5786.116509	25.295783
159.194379	5797.151474	25.300800
159.895175	5807.291834	25.305818
159.734109	5813.439318	25.310835
160.146479	5818.873517	25.315853
160.122084	5821.103310	25.320871
160.297926	5813.359268	25.325888
160.745572	5836.468624	25.330906
160.662982	5861.809852	25.335923
160.946405	5846.067208	25.340941
161.140310	5849.069252	25.345959
160.753841	5862.972586	25.350976
161.192498	5859.358981	25.355994
161.445701	5874.414980	25.361011
161.798009	5897.822481	25.366029
161.897414	5888.847250	25.371047
161.678308	5885.018676	25.376064
162.092447	5897.347540	25.381082
162.137258	5921.016920	25.386099
162.182362	5914.262998	25.391117
162.611946	5926.634612	25.396135
162.714286	5932.029126	25.401152
163.009472	5928.289200	25.406170
162.788956	5953.545484	25.411187
162.999690	5949.391132	25.416205
163.266806	5962.506597	25.421223
162.856321	5974.678839	25.426240
163.512359	5969.097268	25.431258
163.388152	5989.080247	25.436275
163.600612	6014.366278	25.441293
163.939437	6007.976807	25.446311
163.944347	6015.717930	25.451328
164.140598	6030.798452	25.456346
164.212578	6047.270489	25.461363
164.340114	6054.837422	25.466381
164.652290	6065.385101	25.471399
164.939719	6089.031185	25.476416
165.106369	6092.989428	25.481434
165.324665	6080.890267	25.486451
165.299853	6104.003273	25.491469
165.452274	6120.273106	25.496487
165.532616	6119.930709	25.501504
165.922623	6143.961141	25.506522
166.020220	6153.195406	25.511539
166.332201	6159.260535	25.516557
166.531061	6174.698668	25.521575
166.672405	6176.656619	25.526592
167.257017	6181.241946	25.531610
166.948983	6192.699341	25.536627
167.262037	6194.588761	25.541645
167.750605	6196.231054	25.546663
167.437500	6220.951447	25.551680
167.758342	6225.235852	25.556698
168.097337	6233.273094	25.561715
167.867817	6228.148406	25.566733
168.401728	6232.853554	25.571751
168.360606	6247.668361	25.576768
168.489978	6270.318699	25.581786
168.477600	6274.113244	25.586803
168.492883	6265.660403	25.591821
169.170889	6286.947957	25.596839
168.959375	6321.359288	25.601856
169.457125	6319.781672	25.606874
169.831653	6329.004934	25.611891
169.455639	6328.632414	25.616909
169.745014	6332.279469	25.621927
170.054812	6368.773474	25.626944
170.199623	6370.267053	25.631962
170.599453	6359.974077	25.636979
170.657724	6383.029670	25.641997
170.846882	6388.936032	25.647015
171.123248	6409.745180	25.652032
171.280729	6393.160114	25.657050
171.631191	6411.742243	25.662067
171.717675	6427.614195	25.667085
172.001521	6419.072799	25.672103
171.849952	6423.732193	25.677120
172.001728	6418.182990	25.682138
172.108171	6452.135734	25.687156
172.090703	6470.022349	25.692173
172.323486	6472.825158	25.697191
172.620447	6499.751725	25.702208
172.657686	6485.143717	25.707226
172.951590	6499.160418	25.712244
173.100275	6522.377674	25.717261
173.255974	6512.480878	25.722279
173.541606	6521.329926	25.727296
173.944674	6553.509290	25.732314
173.806768	6567.925781	25.737332
173.932063	6556.731479	25.742349
174.064412	6555.900902	25.747367
174.345358	6573.447747	25.752384
174.559060	6580.925099	25.757402
174.768734	6597.059577	25.762420
174.829457	6605.556814	25.767437
175.240299	6591.515394	25.772455
174.992991	6613.804404	25.777472
175.291255	6620.106652	25.782490
175.317415	6633.607413	25.787508
175.278764	6638.137178	25.792525
176.036635	6643.877222	25.797543
175.798954	6681.242422	25.802560
176.184369	6688.187066	25.807578
176.471121	6671.744933	25.812596
176.472388	6695.372673	25.817613
176.778658	6693.056885	25.822631
176.833278	6694.535078	25.827648
177.133034	6714.528864	25.832666
177.485937	6730.708720	25.837684
177.655530	6724.487489	25.842701
177.354377	6726.765106	25.847719
177.319563	6750.678057	25.852736
177.763020	6768.883392	25.857754
178.096201	6776.032792	25.862772
178.257772	6787.866627	25.867789
178.661519	6805.480855	25.872807
178.761126	6823.005967	25.877824
178.821848	6825.926650	25.882842
179.056393	6820.014768	25.887860
179.145036	6837.246789	25.892877
179.574970	6839.906448	25.897895
179.645406	6856.177204	25.902912
179.710475	6877.551088	25.907930
180.271275	6896.597923	25.912948
180.207906	6875.898698	25.917965
180.715517	6892.604805	25.922983
180.891370	6916.613928	25.928000
180.999555	6897.699950	25.933018
181.160109	6900.554541	25.938036
181.437553	6943.043011	25.943053
181.664089	6946.080827	25.948071
181.358725	6937.185262	25.953088
181.350764	6940.666206	25.958106
181.954714	6963.398999	25.963124
181.897686	6981.256901	25.968141
182.112733	6962.948107	25.973159
182.055153	6991.849314	25.978176
182.098309	7018.994717	25.983194
182.678426	7046.423940	25.988212
182.572270	7048.607959	25.993229
183.142369	7037.790278	25.998247
183.163485	7065.315832	26.003264
183.626403	7077.663955	26.008282
183.879402	7095.953902	26.013300
183.693041	7096.056001	26.018317
184.197272	7094.454798	26.023335
184.400010	7112.185272	26.028352
184.531381	7130.233114	26.033370
184.759579	7139.373144	26.038388
184.680531	7132.060387	26.043405
184.975046	7151.724447	26.048423
185.173701	7151.878304	26.053440
185.339226	7157.732555	26.058458
185.784613	7184.371565	26.063476
185.833600	7195.506881	26.068493
185.957811	7182.778228	26.073511
186.083415	7183.728522	26.078528
186.173613	7214.081923	26.083546
186.726235	7206.797461	26.088564
186.947047	7216.286840	26.093581
186.996756	7225.531226	26.098599
187.107457	7206.479433	26.103616
187.660448	7224.157677	26.108634
187.691068	7229.310120	26.113652
187.749370	7226.173286	26.118669
188.259360	7217.301137	26.123687
188.129886	7232.958761	26.128704
188.216198	7260.271493	26.133722
188.621655	7257.308826	26.138740
188.222570	7267.902384	26.143757
188.681342	7259.440310	26.148775
188.792236	7277.897278	26.153792
188.561393	7307.269099	26.158810
189.219597	7294.571831	26.163828
189.056956	7303.064613	26.168845
189.729988	7317.347018	26.173863
189.630731	7342.724106	26.178880
189.303591	7370.944844	26.183898
189.762809	7362.131405	26.188916
189.811491	7378.514976	26.193933
190.436140	7402.631429	26.198951
190.435733	7428.637309	26.203968
190.385652	7446.972230	26.208986
190.737128	7436.329004	26.214004
190.811967	7458.857371	26.219021
190.969638	7484.435585	26.224039
191.554262	7495.674773	26.229056
191.738645	7492.265044	26.234074
192.339691	7529.825630	26.239092
192.294503	7528.144660	26.244109
192.569724	7519.643471	26.249127
193.061496	7550.358804	26.254144
192.901694	7571.610129	26.259162
193.172171	7555.465876	26.264180
193.520291	7550.556390	26.269197
193.765653	7579.962657	26.274215
194.353650	7599.504368	26.279232
194.192425	7581.441307	26.284250
194.421779	7570.347222	26.289268
194.668533	7591.426659	26.294285
194.835472	7602.968834	26.299303
195.157281	7629.634532	26.304320
195.217630	7613.831290	26.309338
195.357407	7603.366262	26.314356
195.495666	7611.471640	26.319373
195.567689	7644.968793	26.324391
195.853530	7651.647200	26.329408
195.574397	7641.725458	26.334426
196.018537	7638.555508	26.339444
196.261991	7670.221712	26.344461
196.156781	7687.706026	26.349479
196.520703	7690.763817	26.354496
196.520536	7691.047398	26.359514
196.987045	7702.318851	26.364532
196.818057	7735.887519	26.369549
197.072866	7748.755685	26.374567
197.271255	7746.464265	26.379584
197.522246	7749.966788	26.384602
198.222428	7784.413401	26.389620
198.056021	7808.328834	26.394637
198.295833	7813.138974	26.399655
198.685305	7816.728102	26.404672
198.624054	7832.045854	26.409690
199.013399	7834.711999	26.414708
199.100621	7857.784664	26.419725
199.143355	7853.998185	26.424743
199.409841	7878.846329	26.429760
200.012168	7878.779927	26.434778
200.015380	7876.018278	26.439796
200.162881	7886.235272	26.444813
200.437984	7914.938694	26.449831
201.154274	7911.600867	26.454848
200.614182	7908.344612	26.459866
200.720160	7921.183955	26.464884
201.114072	7923.637509	26.469901
201.359370	7935.933272	26.474919
201.327610	7955.693595	26.479936
201.261719	7976.922862	26.484954
201.731527	7985.928962	26.489972
201.581509	7989.154419	26.494989
201.763656	8022.964956	26.500007
202.169319	8035.052375	26.505024
202.199889	8047.144285	26.510042
202.921142	8048.740463	26.515060
202.905571	8075.075179	26.520077
203.025570	8098.573578	26.525095
203.333292	8122.524560	26.530112
203.481437	8119.329388	26.535130
203.902309	8119.704864	26.540148
204.087779	8142.742024	26.545165
204.049091	8148.274800	26.550183
204.630730	8175.593127	26.555200
204.537377	8197.277716	26.560218
204.877419	8196.666337	26.565236
205.139499	8204.121510	26.570253
205.002780	8223.081225	26.575271
205.564570	8224.491126	26.580288
205.549610	8234.586338	26.585306
205.574776	8254.229733	26.590324
206.102486	8283.192942	26.595341
206.135749	8293.278649	26.600359
206.489285	8307.160318	26.605376
206.553038	8323.688871	26.610394
206.824285	8337.993702	26.615412
207.061639	8349.100288	26.620429
207.040462	8368.456140	26.625447
207.151082	8370.600586	26.630464
207.739314	8400.866903	26.635482
208.118180	8388.179474	26.640500
208.370400	8413.770355	26.645517
208.491459	8446.358544	26.650535
208.865845	8444.129305	26.655552
208.994886	8454.893150	26.660570
209.347851	8477.306927	26.665588
209.119125	8480.621096	26.670605
209.553569	8507.671340	26.675623
210.046273	8494.464115	26.680640
209.782191	8504.608536	26.685658
210.355329	8525.536065	26.690676
210.526654	8535.402220	26.695693
210.433967	8545.864099	26.700711
210.888984	8553.712857	26.705728
211.058371	8557.105394	26.710746
211.424494	8593.884310	26.715764
211.443618	8596.841731	26.720781
211.752267	8588.307668	26.725799
211.759114	8619.118598	26.730816
211.564080	8636.301404	26.735834
212.061655	8637.417157	26.740852
212.423830	8670.771677	26.745869
212.404849	8684.567159	26.750887
212.650239	8688.295283	26.755904
213.335443	8710.763188	26.760922
213.808751	8714.997102	26.765940
213.900864	8718.070076	26.770957
213.522777	8724.355362	26.775975
213.871209	8722.227247	26.780992
214.039827	8748.004966	26.786010
214.595599	8745.339319	26.791028
214.528155	8746.423992	26.796045
214.502199	8784.506231	26.801063
215.233550	8766.577876	26.806080
214.885964	8793.004086	26.811098
215.388764	8813.494688	26.816116
215.280993	8815.383079	26.821133
215.543161	8831.023262	26.826151
215.677858	8841.999876	26.831168
215.988756	8880.637082	26.836186
216.090157	8890.696949	26.841204
216.446931	8896.515919	26.846221
216.234719	8904.782256	26.851239
216.867939	8926.756568	26.856256
217.173311	8948.405452	26.861274
217.200108	8978.343481	26.866292
217.657539	8983.998571	26.871309
217.783331	9000.333282	26.876327
217.907614	9021.986195	26.881344
218.239082	9046.055161	26.886362
218.383148	9045.710052	26.891380
219.007141	9067.478943	26.896397
218.872305	9092.185013	26.901415
219.180746	9084.783306	26.906432
219.387684	9120.626500	26.911450
219.752712	9141.866472	26.916468
220.335167	9147.456071	26.921485
220.183936	9145.475827	26.926503
220.181525	9157.613416	26.931520
220.680610	9191.256736	26.936538
220.709660	9205.818965	26.941556
221.110853	9207.204299	26.946573
221.075412	9211.160886	26.951591
221.737280	9229.320390	26.956608
221.973658	9258.369755	26.961626
222.141335	9265.965472	26.966644
222.355673	9270.662126	26.971661
222.310754	9274.621870	26.976679
222.811381	9287.753915	26.981696
222.573276	9318.969771	26.986714
222.710110	9323.366558	26.991732
223.078987	9315.974450	26.996749
223.020294	9353.406587	27.001767
223.306174	9382.114835	27.006784
223.536719	9413.944985	27.011802
224.067566	9417.826178	27.016820
224.354710	9425.957513	27.021837
224.478187	9457.294268	27.026855
225.203584	9471.744055	27.031872
225.241237	9479.494467	27.036890
225.344311	9490.219200	27.041908
225.687447	9488.654230	27.046925
225.745083	9510.156569	27.051943
225.918135	9538.968808	27.056960
225.923420	9549.018981	27.061978
226.189692	9551.928659	27.066996
226.621427	9563.849906	27.072013
226.774414	9597.380354	27.077031
227.010547	9599.375060	27.082048
227.232856	9629.015007	27.087066
227.410846	9635.191447	27.092084
228.171306	9650.776896	27.097101
228.340168	9673.337784	27.102119
228.097191	9678.741016	27.107136
228.751799	9691.192640	27.112154
228.717905	9702.695495	27.117172
229.229061	9702.615808	27.122189
229.437435	9714.288945	27.127207
229.780396	9710.769841	27.132224
229.672759	9740.517281	27.137242
229.895229	9750.774294	27.142260
230.310678	9746.707608	27.147277
230.295591	9764.651125	27.152295
230.270006	9774.731746	27.157312
230.446390	9788.930693	27.162330
230.648520	9792.358257	27.167348
230.936284	9821.902685	27.172365
230.828744	9864.903324	27.177383
231.352747	9878.711742	27.182400
231.529236	9886.052678	27.187418
231.334037	9910.791260	27.192436
231.722423	9922.686859	27.197453
231.944023	9958.038028	27.202471
232.433974	9963.618787	27.207488
232.926840	10000.523387	27.212506
232.945752	10012.261127	27.217524
233.583419	10033.340679	27.222541
233.509266	10053.672224	27.227559
233.696702	10067.882197	27.232576
234.253830	10088.789240	27.237594
234.179476	10105.915102	27.242612
234.854381	10122.589525	27.247629
235.569157	10137.566262	27.252647
235.860361	10124.421700	27.257664
236.071255	10117.612202	27.262682
236.013253	10147.930348	27.267700
236.627584	10164.819616	27.272717
236.464212	10163.661997	27.277735
236.774821	10168.500547	27.282752
237.012213	10162.705103	27.287770
237.159467	10189.304718	27.292788
237.178365	10204.255497	27.297805
237.324619	10217.532720	27.302823
237.771814	10217.084732	27.307840
237.761334	10242.885809	27.312858
238.147930	10271.556973	27.317876
238.380504	10275.617627	27.322893
238.239678	10292.146588	27.327911
238.672367	10309.214103	27.332928
239.046546	10324.474928	27.337946
238.878005	10343.588153	27.342964
239.293513	10339.307061	27.347981
239.484991	10380.110127	27.352999
239.546204	10403.699639	27.358016
239.915513	10428.734873	27.363034
239.882937	10455.627729	27.368052
240.388196	10461.664566	27.373069
240.499139	10495.741054	27.378087
240.559588	10517.616865	27.383104
241.246317	10526.468857	27.388122
241.292569	10533.799316	27.393140
241.937715	10563.539713	27.398157
242.354220	10567.331385	27.403175
242.308452	10603.043235	27.408192
242.284594	10614.653004	27.413210
242.911330	10619.483575	27.418228
243.110722	10645.271108	27.423245
243.303643	10676.716161	27.428263
243.317246	10683.258877	27.433280
243.980219	10687.117772	27.438298
243.807999	10715.470099	27.443316
244.097569	10727.158136	27.448333
244.384542	10744.377800	27.453351
244.418839	10772.855223	27.458368
244.918478	10770.834983	27.463386
245.012623	10801.011080	27.468404
245.230288	10822.412348	27.473421
245.531926	10821.722941	27.478439
245.786146	10836.240009	27.483456
246.283688	10847.774833	27.488474
246.127946	10860.569215	27.493492
246.621801	10864.288315	27.498509
247.282109	10905.711597	27.503527
247.371663	10924.817536	27.508544
247.562427	10929.224766	27.513562
247.153505	10945.096853	27.518580
247.428004	10953.941572	27.523597
247.602389	10985.718769	27.528615
247.563958	11012.386671	27.533632
248.490649	11031.691571	27.538650
248.456558	11047.476625	27.543668
248.881843	11068.465034	27.548685
249.373782	11102.224655	27.553703
249.590731	11121.846215	27.558720
249.993004	11129.839673	27.563738
250.354703	11133.416039	27.568756
250.606590	11144.938100	27.573773
250.814938	11183.817627	27.578791
251.002943	11193.687409	27.583808
251.435195	11193.279679	27.588826
251.648985	11206.524513	27.593844
251.531126	11237.222483	27.598861
251.890019	11257.020839	27.603879
252.165641	11271.675770	27.608896
252.434924	11268.014896	27.613914
252.419366	11298.796911	27.618932
252.921770	11329.642291	27.623949
253.142629	11342.230684	27.628967
253.673600	11373.991492	27.633984
253.909727	11375.895050	27.639002
253.871506	11381.980281	27.644020
254.007334	11410.120674	27.649037
254.620826	11421.045176	27.654055
254.397376	11463.817990	27.659072
255.140509	11463.086338	27.664090
254.704735	11472.546538	27.669108
255.288182	11495.650430	27.674125
255.588264	11526.705281	27.679143
255.872615	11538.037934	27.684160
256.665698	11552.743124	27.689178
256.594796	11594.782124	27.694196
257.014123	11596.747607	27.699213
257.347691	11596.059196	27.704231
257.087147	11617.164786	27.709248
257.632502	11634.652305	27.714266
258.134377	11663.132052	27.719284
258.108884	11678.492505	27.724301
258.445327	11662.122077	27.729319
258.287332	11693.153676	27.734336
258.643306	11730.800961	27.739354
258.721287	11758.836515	27.744372
259.117258	11760.456907	27.749389
259.579671	11783.314167	27.754407
259.761400	11809.571271	27.759424
259.986204	11820.505122	27.764442
260.194046	11852.670814	27.769460
260.573136	11872.853382	27.774477
260.685601	11888.054963	27.779495
260.916237	11905.790925	27.784512
261.709677	11933.397421	27.789530
261.747306	11940.878047	27.794548
261.903030	11943.511025	27.799565
262.191916	11959.157754	27.804583
262.191480	11996.229617	27.809600
263.030151	11991.215677	27.814618
262.775430	12024.070221	27.819636
263.010074	12033.344363	27.824653
263.671507	12039.499376	27.829671
263.452795	12052.098719	27.834688
263.676810	12080.353339	27.839706
264.111253	12102.208132	27.844724
263.880921	12116.137610	27.849741
264.661124	12149.300388	27.854759
264.669532	12167.228544	27.859776
264.974595	12174.328721	27.864794
265.384831	12208.293243	27.869812
265.712908	12221.215172	27.874829
266.152763	12245.728769	27.879847
266.250438	12275.367444	27.884864
266.808860	12281.400136	27.889882
266.641296	12303.780846	27.894900
266.929374	12339.973951	27.899917
267.386039	12351.787615	27.904935
267.376835	12361.774993	27.909952
268.053485	12381.601024	27.914970
268.552199	12408.378664	27.919988
268.478279	12439.665660	27.925005
268.802283	12443.770849	27.930023
269.299671	12456.761894	27.935040
269.485568	12479.593358	27.940058
269.709933	12505.894189	27.945076
269.688032	12509.587024	27.950093
270.172104	12540.206949	27.955111
270.106350	12553.695242	27.960128
270.724520	12574.220484	27.965146
271.045134	12596.552461	27.970164
271.162180	12604.505552	27.975181
271.521462	12619.474043	27.980199
271.718389	12665.969075	27.985216
271.775602	12674.738782	27.990234
272.505161	12681.608346	27.995252
272.523408	12704.736464	28.000269
273.163894	12738.858655	28.005287
273.385375	12753.259192	28.010304
273.520185	12778.661425	28.015322
273.643607	12780.467968	28.020340
273.906920	12817.979497	28.025357
273.955187	12827.218716	28.030375
274.367650	12846.354744	28.035392
274.528283	12884.972916	28.040410
275.093110	12909.112372	28.045428
275.023822	12913.432340	28.050445
276.002931	12938.927742	28.055463
275.642097	12976.783823	28.060480
276.144380	12993.082484	28.065498
276.569610	12994.000178	28.070516
277.016393	13020.031915	28.075533
277.362334	13033.053176	28.080551
277.656626	13054.435317	28.085568
277.735757	13066.222860	28.090586
278.086972	13096.308816	28.095604
278.020113	13111.628629	28.100621
278.421686	13112.331227	28.105639
278.647559	13139.399386	28.110656
279.030094	13139.270050	28.115674
279.360125	13170.498821	28.120692
279.356779	13216.451852	28.125709
279.586038	13230.571857	28.130727
279.997051	13228.787341	28.135744
280.391310	13257.176621	28.140762
280.467050	13272.350916	28.145780
280.556358	13299.201620	28.150797
280.778559	13310.932618	28.155815
281.040571	13334.954936	28.160832
280.971047	13352.553798	28.165850
281.439991	13392.901157	28.170868
282.000040	13410.114030	28.175885
282.681232	13419.002436	28.180903
282.860364	13442.374470	28.185920
283.246213	13466.121270	28.190938
283.729907	13483.013585	28.195956
284.189697	13500.220271	28.200973
284.262959	13508.140077	28.205991
284.870658	13528.175091	28.211008
285.045872	13534.984556	28.216026
285.258847	13541.872873	28.221044
285.446404	13569.559442	28.226061
285.565042	13569.529639	28.231079
285.727248	13579.134141	28.236096
286.057416	13589.590123	28.241114
286.391671	13628.645430	28.246132
286.337970	13664.239351	28.251149
286.917017	13673.438637	28.256167
287.486137	13682.042388	28.261184
287.671159	13686.444239	28.266202
288.156195	13708.504005	28.271220
287.945793	13744.532880	28.276237
288.257882	13750.629675	28.281255
288.356121	13761.563701	28.286272
288.900496	13793.624109	28.291290
289.214435	13814.475371	28.296308
289.399998	13832.582530	28.301325
289.353787	13854.752321	28.306343
289.808399	13890.521178	28.311360
290.030313	13918.346059	28.316378
290.689200	13943.207382	28.321396
290.699758	13962.191326	28.326413
291.442378	13963.604991	28.331431
291.492855	13981.315496	28.336448
291.654394	14033.273053	28.341466
291.905689	14063.028303	28.346484
292.127111	14078.517280	28.351501
292.676646	14082.031769	28.356519
293.024085	14114.858059	28.361536
292.918247	14138.795017	28.366554
293.449931	14143.666014	28.371572
293.390539	14188.199526	28.376589
293.977805	14215.307483	28.381607
294.295534	14219.739555	28.386624
294.343410	14257.193118	28.391642
295.128189	14289.714304	28.396660
295.297806	14303.743469	28.401677
295.561329	14327.429021	28.406695
295.806277	14343.669145	28.411712
295.891006	14358.161468	28.416730
296.327435	14391.025617	28.421748
296.518405	14438.458798	28.426765
296.679646	14452.894445	28.431783
296.839047	14474.426028	28.436800
297.229978	14510.156353	28.441818
297.720605	14526.343467	28.446836
298.154087	14558.095956	28.451853
298.668790	14576.590787	28.456871
299.195268	14588.421357	28.461888
299.262386	14606.936589	28.466906
299.520941	14643.585690	28.471924
299.780658	14668.101226	28.476941
299.850247	14678.723087	28.481959
300.670766	14704.535863	28.486976
300.453285	14725.732947	28.491994
300.933091	14728.485394	28.497012
301.079584	14756.653515	28.502029
301.301909	14785.477290	28.507047
301.500197	14808.107517	28.512064
301.570936	14831.512074	28.517082
302.266566	14834.610225	28.522100
302.399835	14868.453567	28.527117
302.880802	14905.365918	28.532135
303.086954	14919.755166	28.537152
303.259880	14958.790702	28.542170
303.499047	14988.595355	28.547188
303.912827	15014.152782	28.552205
304.337409	15008.501171	28.557223
304.823845	15043.200501	28.562240
304.552027	15082.557210	28.567258
305.296629	15109.791953	28.572276
305.621586	15128.843510	28.577293
305.865013	15137.834347	28.582311
306.271597	15171.431463	28.587328
306.581265	15216.522974	28.592346
307.190970	15229.339340	28.597364
307.170247	15243.849875	28.602381
307.486748	15265.982160	28.607399
307.709602	15271.834264	28.612416
308.147412	15318.936137	28.617434
308.759669	15324.701867	28.622452
308.777674	15340.547129	28.627469
308.921909	15368.797053	28.632487
309.523135	15401.016721	28.637504
309.614402	15435.941335	28.642522
310.169874	15452.575661	28.647540
310.295634	15473.705984	28.652557
310.719991	15494.117267	28.657575
310.786859	15529.780461	28.662592
311.250962	15554.614987	28.667610
311.683736	15566.427087	28.672628
311.670009	15611.038902	28.677645
312.062499	15641.750761	28.682663
312.780165	15642.973302	28.687680
312.682271	15684.705931	28.692698
313.466853	15712.236076	28.697716
313.447852	15726.212536	28.702733
314.056450	15735.157560	28.707751
314.230199	15782.543934	28.712768
314.430901	15811.117809	28.717786
314.558328	15842.657052	28.722804
314.770626	15854.620824	28.727821
315.188642	15892.639487	28.732839
315.535377	15923.257004	28.737856
315.985507	15958.430752	28.742874
316.414903	15972.508272	28.747892
316.586756	15988.612410	28.752909
316.698522	16020.419335	28.757927
317.249420	16036.998285	28.762944
317.247184	16086.226906	28.767962
317.717626	16111.543466	28.772980
317.945872	16127.283844	28.777997
318.492542	16150.115261	28.783015
319.033733	16180.135383	28.788032
319.340531	16226.583883	28.793050
319.608110	16228.542716	28.798068
319.852539	16239.240725	28.803085
319.932837	16278.185990	28.808103
320.870999	16290.638478	28.813120
320.811257	16336.492257	28.818138
321.371929	16351.213463	28.823156
321.689097	16367.750991	28.828173
321.590937	16387.375072	28.833191
321.915502	16402.281892	28.838208
322.148617	16427.414366	28.843226
322.484955	16430.392532	28.848244
322.721464	16461.398041	28.853261
323.049862	16513.759895	28.858279
323.431845	16539.843464	28.863296
323.635334	16552.562511	28.868314
324.022813	16571.917471	28.873332
324.543716	16608.122639	28.878349
324.469320	16656.865322	28.883367
325.019381	16663.738682	28.888384
325.008138	16707.462663	28.893402
325.386115	16729.407123	28.898420
326.027381	16752.616176	28.903437
326.673317	16790.780519	28.908455
326.434002	16817.394260	28.913472
326.812742	16853.193214	28.918490
327.218028	16882.453818	28.923508
327.642440	16897.264220	28.928525
327.846999	16934.229991	28.933543
328.532452	16951.641834	28.938560
328.748231	16992.359900	28.943578
329.020547	17026.753690	28.948596
329.468340	17045.733616	28.953613
329.769591	17062.627503	28.958631
330.525331	17081.786695	28.963648
330.250149	17140.228060	28.968666
330.569675	17158.487005	28.973684
330.805347	17175.295706	28.978701
331.300796	17204.767362	28.983719
331.471331	17240.453414	28.988736
331.701628	17268.760179	28.993754
332.280603	17302.899007	28.998772
332.823259	17317.201688	29.003789
333.167781	17358.258731	29.008807
333.743533	17394.574784	29.013824
334.021678	17426.375871	29.018842
334.331836	17427.234046	29.023860
335.050017	17451.131149	29.028877
335.373047	17475.270083	29.033895
335.674777	17494.807364	29.038912
336.099211	17501.796397	29.043930
336.144598	17524.052189	29.048948
336.592032	17545.362156	29.053965
336.730158	17578.439630	29.058983
337.312342	17603.913413	29.064000
337.614790	17622.208795	29.069018
338.135107	17625.527163	29.074036
338.232617	17662.518567	29.079053
338.341567	17687.761750	29.084071
338.846562	17710.468273	29.089088
339.107113	17755.530784	29.094106
339.464820	17772.160754	29.099124
339.631464	17785.821460	29.104141
339.916703	17805.453248	29.109159
340.334932	17831.597510	29.114176
340.294913	17882.844122	29.119194
340.793135	17919.653277	29.124212
341.433096	17939.505594	29.129229
341.579061	17961.510525	29.134247
341.800536	17981.655831	29.139264
341.926583	18027.456855	29.144282
342.221379	18067.097518	29.149300
342.609316	18096.044785	29.154317
343.070319	18120.292692	29.159335
343.502648	18158.930520	29.164352
343.861577	18178.832705	29.169370
343.919083	18194.225013	29.174388
344.857757	18217.446910	29.179405
344.763210	18257.120829	29.184423
345.207873	18271.171019	29.189440
345.428583	18308.449290	29.194458
345.870910	18331.310454	29.199476
346.055564	18349.941332	29.204493
346.288440	18381.398696	29.209511
346.867809	18428.911705	29.214528
347.137848	18469.039725	29.219546
347.648704	18493.284677	29.224564
348.345402	18500.971526	29.229581
348.405913	18526.819781	29.234599
348.824419	18568.225412	29.239616
349.169034	18594.346798	29.244634
349.907530	18606.882915	29.249652
350.535279	18627.251910	29.254669
350.383466	18679.930129	29.259687
350.720807	18678.284095	29.264704
351.528866	18694.793319	29.269722
351.363525	18732.844023	29.274740
351.856220	18749.663891	29.279757
352.358866	18762.582694	29.284775
352.521693	18783.643392	29.289792
352.644417	18828.266640	29.294810
353.008724	18864.638216	29.299828
353.553607	18867.530369	29.304845
353.694628	18903.592157	29.309863
354.036449	18950.089873	29.314880
354.215117	18990.098704	29.319898
354.493281	19017.297243	29.324916
355.222378	19027.507201	29.329933
355.386982	19063.920087	29.334951
355.722140	19110.460336	29.339968
356.298212	19144.023433	29.344986
356.110019	19167.837916	29.350004
356.969331	19202.845433	29.355021
357.040722	19236.802603	29.360039
357.369613	19251.652983	29.365056
357.903871	19289.185885	29.370074
357.982802	19340.299160	29.375092
359.302220	19359.616950	29.380109
359.162816	19370.973074	29.385127
359.737174	19397.730830	29.390144
360.035798	19438.012533	29.395162
360.411204	19482.022057	29.400180
360.843005	19495.668752	29.405197
360.970083	19524.447255	29.410215
361.280387	19556.775188	29.415232
361.803010	19608.124938	29.420250
361.848085	19636.136939	29.425268
362.164125	19648.757829	29.430285
362.270095	19686.209489	29.435303
362.779580	19718.035109	29.440320
363.331004	19771.100305	29.445338
363.639511	19793.224270	29.450356
364.315400	19807.634797	29.455373
364.337936	19854.469953	29.460391
364.815834	19884.188908	29.465408
365.502081	19924.426677	29.470426
365.702016	19936.706000	29.475444
366.509953	19957.825559	29.480461
366.706473	19988.691428	29.485479
366.908639	20011.005066	29.490496
367.598983	20050.317185	29.495514
367.337576	20074.873312	29.500532
367.809797	20082.073085	29.505549
368.058175	20132.244986	29.510567
368.562880	20177.888538	29.515584
368.555173	20191.192269	29.520602
368.716494	20211.208368	29.525620
369.310452	20254.148209	29.530637
369.884520	20274.217578	29.535655
369.969740	20304.156633	29.540672
370.528749	20347.045741	29.545690
370.789380	20388.081629	29.550708
371.029951	20416.560771	29.555725
371.457138	20458.958063	29.560743
371.778073	20477.445875	29.565760
372.327213	20511.985643	29.570778
372.850644	20542.689772	29.575796
373.419939	20576.715612	29.580813
373.623597	20607.638201	29.585831
374.293402	20630.373547	29.590848
374.948584	20639.661950	29.595866
375.056895	20689.229710	29.600884
375.334879	20720.111856	29.605901
374.978671	20759.429871	29.610919
375.765455	20775.306278	29.615936
376.331568	20820.397610	29.620954
377.011671	20843.514603	29.625972
377.494396	20873.163599	29.630989
377.636178	20910.662548	29.636007
377.683507	20938.621201	29.641024
378.485169	20992.493906	29.646042
378.721350	21019.499316	29.651060
379.226740	21033.497693	29.656077
379.322866	21060.816361	29.661095
379.748117	21098.516399	29.666112
380.045088	21156.691426	29.671130
380.319902	21189.517086	29.676148
380.952902	21211.214157	29.681165
381.221681	21231.149102	29.686183
381.355749	21270.921732	29.691200
381.665539	21323.410704	29.696218
381.875743	21361.679689	29.701236
382.518741	21379.574594	29.706253
382.625372	21435.529337	29.711271
382.910913	21476.540149	29.716288
383.684469	21507.089663	29.721306
384.143685	21558.498485	29.726324
384.655493	21594.895827	29.731341
385.337055	21613.779345	29.736359
385.994880	21636.696187	29.741376
386.474543	21679.970729	29.746394
386.721322	21694.928300	29.751412
387.190337	21714.736160	29.756429
387.500652	21771.080870	29.761447
387.475995	21788.829545	29.766464
387.976863	21809.242343	29.771482
388.297933	21834.601842	29.776500
388.899670	21865.070045	29.781517
389.166024	21919.042059	29.786535
389.410554	21942.844205	29.791552
389.901995	21958.548255	29.796570
390.086082	21997.759436	29.801588
390.216417	22047.034368	29.806605
391.005527	22096.706673	29.811623
391.068464	22130.887127	29.816640
391.708343	22148.294665	29.821658
391.855896	22192.721056	29.826676
392.530415	22228.391363	29.831693
392.603625	22272.239060	29.836711
392.746815	22299.165737	29.841728
393.312529	22316.689751	29.846746
393.692230	22365.815650	29.851764
394.333304	22395.001351	29.856781
394.712272	22426.398108	29.861799
394.882263	22474.201587	29.866816
395.427015	22507.688376	29.871834
395.585111	22536.466962	29.876852
396.028820	22577.249398	29.881869
396.831212	22615.786033	29.886887
397.412528	22645.784499	29.891904
398.265906	22657.864874	29.896922
398.437960	22692.168759	29.901940
399.019260	22720.762666	29.906957
399.268700	22743.217197	29.911975
399.751571	22771.791189	29.916992
400.069124	22790.699914	29.922010
400.532443	22834.688016	29.927028
400.688622	22838.751834	29.932045
401.105139	22858.634364	29.937063
401.444927	22907.896147	29.942080
401.847804	22933.276907	29.947098
401.940187	22961.817981	29.952116
402.335270	23016.097037	29.957133
402.884388	23035.182200	29.962151
402.878821	23073.191194	29.967168
403.419709	23124.072643	29.972186
403.680610	23156.163471	29.977204
404.149813	23189.178515	29.982221
404.670411	23238.389328	29.987239
404.830428	23289.026757	29.992256
405.463713	23314.272284	29.997274
405.581232	23365.579135	30.002292
405.908531	23395.770682	30.007309
406.496778	23437.675951	30.012327
406.495797	23488.222328	30.017344
407.215301	23517.475862	30.022362
407.642445	23575.423370	30.027380
408.187807	23632.169078	30.032397
408.770707	23649.289612	30.037415
409.186204	23684.485520	30.042432
409.870109	23729.204194	30.047450
410.316978	23778.198577	30.052468
410.560335	23807.822949	30.057485
411.426190	23844.384275	30.062503
411.519490	23876.975581	30.067520
411.945235	23900.168788	30.072538
411.947578	23963.887405	30.077556
412.163591	24008.272602	30.082573
412.921084	24021.211746	30.087591
413.187440	24085.789063	30.092608
413.654371	24132.351513	30.097626
413.624603	24174.450575	30.102644
414.445986	24200.799996	30.107661
415.397664	24225.228032	30.112679
415.533610	24286.802006	30.117696
416.145009	24331.058096	30.122714
416.354243	24365.600484	30.127732
416.646801	24388.731222	30.132749
417.396718	24424.839952	30.137767
417.895802	24474.292860	30.142784
418.720968	24514.747369	30.147802
418.853434	24529.212345	30.152820
419.660413	24547.398902	30.157837
420.160542	24586.335292	30.162855
420.481511	24621.533005	30.167872
420.856218	24629.614908	30.172890
421.245667	24671.582891	30.177908
421.345090	24684.525612	30.182925
421.984513	24718.299171	30.187943
422.004131	24755.688141	30.192960
422.347712	24766.693784	30.197978
422.779202	24801.510966	30.202996
422.838621	24848.074906	30.208013
423.628808	24871.128835	30.213031
423.740581	24919.029285	30.218048
424.272952	24930.536790	30.223066
424.629004	24952.681806	30.228084
424.719635	25020.478335	30.233101
425.206428	25060.797684	30.238119
425.845687	25102.990368	30.243136
426.305562	25134.266864	30.248154
426.365871	25188.430037	30.253172
426.831885	25230.372568	30.258189
427.523630	25251.830236	30.263207
427.559570	25311.450329	30.268224
428.083691	25357.680314	30.273242
428.342705	25397.167702	30.278260
428.702876	25424.585448	30.283277
429.568910	25473.326292	30.288295
429.863342	25536.302479	30.293312
430.921200	25575.215243	30.298330
430.968655	25599.022001	30.303348
431.395934	25653.353100	30.308365
432.169654	25691.518351	30.313383
432.372067	25727.646195	30.318400
432.591620	25763.041213	30.323418
433.074816	25800.064194	30.328436
433.689514	25856.676618	30.333453
434.366561	25899.650308	30.338471
434.646376	25941.021424	30.343488
435.087923	25971.354809	30.348506
435.608300	26016.907588	30.353524
436.067041	26036.528291	30.358541
436.489164	26084.317688	30.363559
436.605291	26148.000487	30.368576
436.973003	26184.948772	30.373594
437.299275	26221.110817	30.378612
437.541672	26268.387975	30.383629
438.457837	26313.127156	30.388647
438.734836	26372.514038	30.393664
439.577173	26410.918721	30.398682
440.093740	26443.098128	30.403700
440.355614	26476.207457	30.408717
440.840091	26520.271044	30.413735
441.543952	26576.177300	30.418752
442.184239	26593.272423	30.423770
442.698046	26622.937466	30.428788
442.992005	26666.064680	30.433805
443.366311	26694.961284	30.438823
443.879645	26739.884820	30.443840
443.962873	26770.999470	30.448858
444.742615	26799.015589	30.453876
444.839497	26854.490020	30.458893
445.373400	26896.210986	30.463911
445.617214	26934.493368	30.468928
445.914354	26955.717183	30.473946
446.665876	27010.371211	30.478964
446.786473	27069.852587	30.483981
447.431569	27103.495918	30.488999
447.774977	27129.383233	30.494016
448.796293	27193.330420	30.499034
449.145490	27213.006845	30.504052
449.394468	27254.976025	30.509069
450.225678	27280.931229	30.514087
450.584895	27341.982642	30.519104
450.522907	27357.816263	30.524122
451.146881	27411.503881	30.529140
451.376814	27432.811932	30.534157
452.057709	27471.029626	30.539175
452.483421	27516.483776	30.544192
452.762802	27545.145180	30.549210
453.234216	27576.950977	30.554228
453.432181	27635.197790	30.559245
453.754194	27683.296791	30.564263
454.270330	27709.490779	30.569280
454.584698	27757.354700	30.574298
455.710332	27807.730981	30.579316
455.762982	27838.057806	30.584333
456.355024	27863.157656	30.589351
456.942091	27900.751540	30.594368
457.502154	27961.049706	30.599386
458.154900	28006.013469	30.604404
457.986108	28031.579880	30.609421
458.739102	28070.512441	30.614439
458.845743	28133.425142	30.619456
459.434681	28182.096499	30.624474
460.056735	28203.760233	30.629492
460.337183	28253.192422	30.634509
460.699004	28296.435544	30.639527
461.345686	28362.429770	30.644544
461.373969	28411.787363	30.649562
462.180012	28442.101205	30.654580
462.420655	28482.992895	30.659597
463.318745	28528.018433	30.664615
463.295580	28588.389905	30.669632
463.917313	28644.113041	30.674650
464.506073	28679.503578	30.679668
464.586971	28742.287126	30.684685
465.460649	28789.172052	30.689703
465.917441	28851.657343	30.694720
466.249854	28885.478840	30.699738
466.819750	28943.712811	30.704756
467.328352	28981.227395	30.709773
467.665606	29018.741975	30.714791
468.239880	29074.026438	30.719808
468.466028	29141.048853	30.724826
469.327017	29184.186521	30.729844
469.731258	29232.689485	30.734861
470.392877	29269.239443	30.739879
470.753691	29335.294079	30.744896
471.224475	29395.618329	30.749914
471.715825	29432.452257	30.754932
472.466493	29465.423533	30.759949
472.599977	29512.287593	30.764967
473.370660	29576.931703	30.769984
473.689086	29610.879953	30.775002
474.086824	29661.265194	30.780020
474.648495	29716.348764	30.785037
475.065295	29734.979123	30.790055
475.375913	29794.984241	30.795072
475.952152	29861.074700	30.800090
476.589927	29898.961090	30.805108
476.970873	29949.715858	30.810125
477.321357	29985.432333	30.815143
477.942780	30048.582427	30.820160
478.321050	30096.846061	30.825178
478.932672	30126.119319	30.830196
479.387472	30192.325735	30.835213
480.055114	30236.589417	30.840231
480.643422	30270.680498	30.845248
480.668856	30327.561159	30.850266
481.371626	30356.636792	30.855284
481.989394	30397.227826	30.860301
482.300753	30454.853458	30.865319
483.027990	30492.884097	30.870336
482.970964	30546.242879	30.875354
483.558103	30577.807980	30.880372
483.789906	30611.375028	30.885389
484.295004	30665.467817	30.890407
485.414710	30719.553893	30.895424
485.616935	30749.047246	30.900442
486.506505	30791.045409	30.905460
486.761370	30840.968722	30.910477
487.393789	30862.429044	30.915495
487.905113	30899.436299	30.920512
487.934422	30955.564428	30.925530
488.476135	30986.317579	30.930548
489.067290	31050.337530	30.935565
489.537925	31087.963904	30.940583
490.080061	31129.269472	30.945600
490.341361	31173.287199	30.950618
491.237108	31217.310655	30.955636
491.296576	31290.063056	30.960653
491.781659	31321.308818	30.965671
492.672665	31351.437081	30.970688
492.831704	31412.823028	30.975706
493.645987	31465.728397	30.980724
493.944339	31525.202066	30.985741
494.253011	31554.180758	30.990759
494.851653	31596.184757	30.995776
495.376877	31648.441232	31.000794
496.246988	31695.397723	31.005812
496.801791	31735.762527	31.010829
497.395786	31782.424147	31.015847
497.725499	31824.116629	31.020864
498.191580	31867.405082	31.025882
498.775159	31912.119123	31.030900
499.065267	31968.279994	31.035917
499.231473	32017.539887	31.040935
499.973928	32053.246346	31.045952
500.492837	32114.458592	31.050970
500.755122	32168.198649	31.055988
501.309582	32227.004597	31.061005
501.727839	32277.892498	31.066023
501.922507	32325.580600	31.071040
502.137697	32379.568854	31.076058
502.803427	32449.888194	31.081076
503.465664	32522.467291	31.086093
503.695480	32566.604152	31.091111
504.538848	32603.812573	31.096128
504.689561	32679.593855	31.101146
505.446396	32748.842450	31.106164
506.122598	32809.870246	31.111181
506.695611	32870.479916	31.116199
507.289830	32938.752848	31.121216
507.355678	32981.400298	31.126234
508.250630	33028.214297	31.131252
508.873864	33087.693250	31.136269
509.043684	33156.904751	31.141287
510.026149	33221.517956	31.146304
510.213735	33272.443689	31.151322
510.556742	33331.909810	31.156340
511.036797	33382.531998	31.161357
511.664875	33421.904216	31.166375
512.564567	33490.179318	31.171392
513.102071	33548.535015	31.176410
513.916211	33598.462165	31.181428
514.400291	33664.096376	31.186445
514.782781	33710.100792	31.191463
515.542757	33739.507065	31.196480
515.773548	33784.593357	31.201498
516.202982	33848.012924	31.206516
516.798307	33881.106575	31.211533
517.014978	33943.593003	31.216551
517.563417	33994.353949	31.221568
517.878420	34037.145803	31.226586
518.351401	34074.547885	31.231604
518.918062	34133.345584	31.236621
519.458482	34198.502358	31.241639
520.430255	34242.337876	31.246656
520.471195	34283.739981	31.251674
520.733879	34340.285279	31.256692
521.408774	34407.070789	31.261709
521.850867	34478.343887	31.266727
522.075318	34525.859497	31.271744
522.605546	34571.955349	31.276762
523.729074	34645.277918	31.281780
524.215733	34723.994233	31.286797
524.200087	34776.018049	31.291815
524.914401	34812.668741	31.296832
525.271150	34873.901601	31.301850
525.626542	34957.010735	31.306868
526.529089	35014.212934	31.311885
526.891461	35083.393875	31.316903
527.509417	35150.825823	31.321920
528.015206	35210.485950	31.326938
528.492098	35264.704868	31.331956
530.107065	35324.377812	31.336973
530.600505	35358.488165	31.341991
531.576157	35417.806331	31.347008
531.670673	35476.175303	31.352026
532.139560	35519.844620	31.357044
532.730474	35584.168282	31.362061
533.350054	35625.679898	31.367079
534.272267	35671.852711	31.372096
534.477174	35726.152674	31.377114
534.750508	35757.971421	31.382132
535.380071	35804.988095	31.387149
535.862164	35874.698243	31.392167
536.424313	35936.913759	31.397184
536.464270	35979.496985	31.402202
537.235690	36020.653117	31.407220
537.661783	36077.401007	31.412237
537.922696	36154.580038	31.417255
538.780615	36201.667333	31.422272
539.114086	36289.910926	31.427290
539.313243	36356.769735	31.432308
540.161922	36398.049671	31.437325
540.133274	36464.662508	31.442343
540.908518	36541.291236	31.447360
541.355549	36605.172169	31.452378
542.048315	36679.704007	31.457396
543.278319	36750.313320	31.462413
543.575531	36798.725504	31.467431
544.439853	36829.445059	31.472448
545.026720	36907.166772	31.477466
546.021396	36965.770626	31.482484
546.551409	36996.813919	31.487501
547.418895	37053.293204	31.492519
548.324815	37094.865093	31.497536
548.664643	37130.032975	31.502554
549.486110	37161.628002	31.507572
550.017807	37211.716129	31.512589
550.196273	37254.162756	31.517607
550.709855	37297.014873	31.522624
551.416517	37345.282018	31.527642
551.558242	37378.021626	31.532660
552.055539	37413.425984	31.537677
552.306177	37457.461143	31.542695
553.018483	37516.208116	31.547712
553.322093	37581.810880	31.552730
553.442831	37628.130612	31.557748
554.111195	37666.186487	31.562765
554.549051	37709.979905	31.567783
554.894245	37780.998211	31.572800
555.294012	37840.463746	31.577818
556.126117	37887.802755	31.582836
556.437188	37937.474911	31.587853
556.826353	38007.896709	31.592871
557.358185	38076.041924	31.597888
558.263845	38140.953991	31.602906
558.245465	38198.406890	31.607924
559.062604	38263.968357	31.612941
559.722363	38333.163272	31.617959
560.212957	38386.916026	31.622976
561.056770	38465.151190	31.627994
561.661146	38505.412795	31.633012
562.455417	38556.095656	31.638029
562.588120	38641.527851	31.643047
563.325102	38715.394947	31.648064
564.010670	38768.053070	31.653082
564.984328	38803.053271	31.658100
565.600844	38869.865144	31.663117
565.968625	38953.060249	31.668135
566.539292	39002.380022	31.673152
567.111730	39045.343365	31.678170
567.501673	39100.560342	31.683188
567.947907	39166.890159	31.688205
568.325699	39258.426498	31.693223
569.205344	39316.331137	31.698240
569.860170	39351.022114	31.703258
570.020150	39416.560604	31.708276
570.503811	39492.379010	31.713293
571.359355	39581.063846	31.718311
571.793225	39631.452613	31.723328
572.235836	39698.813884	31.728346
572.411518	39791.885478	31.733364
573.632034	39851.493523	31.738381
573.996085	39930.300332	31.743399
574.725669	39986.363435	31.748416
575.017812	40051.825583	31.753434
575.521950	40135.331851	31.758452
576.369781	40213.043680	31.763469
576.666033	40275.962023	31.768487
577.519399	40348.175317	31.773504
578.013690	40424.232588	31.778522
578.492122	40497.941355	31.783540
579.610224	40558.673349	31.788557
580.117136	40644.236255	31.793575
580.234254	40703.912560	31.798592
581.182492	40782.696024	31.803610
581.357747	40856.450004	31.808628
582.225970	40912.587763	31.813645
582.778900	40984.878459	31.818663
583.483277	41072.481351	31.823680
584.068458	41141.800333	31.828698
584.856954	41199.647136	31.833716
585.316687	41269.744863	31.838733
585.785645	41345.213602	31.843751
586.549108	41421.498881	31.848768
587.018850	41477.877801	31.853786
587.435618	41543.056432	31.858804
588.596609	41596.941571	31.863821
588.966253	41684.280726	31.868839
589.320372	41748.936989	31.873856
590.228551	41827.425407	31.878874
590.585838	41890.964239	31.883892
591.097250	41959.373645	31.888909
591.556026	42010.645568	31.893927
592.132637	42069.972674	31.898944
593.171137	42137.301374	31.903962
593.815706	42182.248874	31.908980
594.808438	42223.644634	31.913997
595.600175	42288.176866	31.919015
595.800611	42353.226814	31.924032
596.593079	42412.342610	31.929050
596.871636	42458.484469	31.934068
597.569636	42521.473627	31.939085
597.981631	42591.688477	31.944103
597.908639	42657.062446	31.949120
598.712179	42704.216739	31.954138
599.198503	42759.353139	31.959156
599.788141	42839.438970	31.964173
600.262761	42901.762383	31.969191
601.034194	42967.361015	31.974208
601.875242	43061.482123	31.979226
602.198934	43134.071713	31.984244
603.163876	43182.475907	31.989261
603.467117	43257.594770	31.994279
604.096244	43334.639422	31.999296
604.726282	43414.784222	32.004314
604.953484	43488.230853	32.009332
605.471020	43546.638074	32.014349
606.220417	43638.788474	32.019367
606.754883	43722.239820	32.024384
607.365301	43794.232208	32.029402
608.064461	43881.922000	32.034420
608.778475	43965.818327	32.039437
609.564672	44046.530422	32.044455
610.010177	44119.274245	32.049472
610.895324	44183.753510	32.054490
611.175246	44262.728614	32.059508
611.620474	44352.050520	32.064525
612.498674	44414.757526	32.069543
612.887747	44497.380848	32.074560
613.642124	44586.520234	32.079578
614.173134	44666.933070	32.084596
614.738735	44756.985260	32.089613
615.484524	44838.521998	32.094631
616.201361	44913.718195	32.099648
617.137457	45009.478363	32.104666
617.725877	45092.797541	32.109684
618.499023	45149.857421	32.114701
618.862821	45221.387800	32.119719
619.384096	45305.865053	32.124736
619.879579	45395.521496	32.129754
620.410153	45474.870792	32.134772
621.290593	45553.771157	32.139789
621.732802	45629.804900	32.144807
622.246267	45716.855251	32.149824
623.218057	45792.653810	32.154842
623.511580	45877.925846	32.159860
624.332590	45958.302691	32.164877
625.105731	46048.364748	32.169895
625.499736	46123.887523	32.174912
626.388542	46192.395516	32.179930
627.063011	46274.771222	32.184948
627.957933	46353.056912	32.189965
628.405715	46424.994804	32.194983
628.975885	46500.531054	32.200000
629.455462	46572.277981	32.205018
630.171136	46656.694520	32.210036
631.086384	46735.556251	32.215053
631.752337	46806.237680	32.220071
632.119422	46896.348786	32.225088
633.136247	46967.500162	32.230106
633.439078	47029.745837	32.235124
633.849408	47099.441273	32.240141
634.921884	47165.134495	32.245159
635.189144	47232.182863	32.250176
635.763640	47307.920576	32.255194
636.148208	47380.993480	32.260212
637.102449	47450.568818	32.265229
637.549282	47531.345759	32.270247
638.175027	47610.533688	32.275264
639.035556	47674.975437	32.280282
639.147879	47751.119648	32.285300
639.881591	47833.385069	32.290317
640.797972	47928.850871	32.295335
641.408574	47996.937781	32.300352
642.242168	48068.309891	32.305370
642.756061	48162.340337	32.310388
643.314762	48225.908644	32.315405
643.946043	48309.061406	32.320423
644.230332	48387.920610	32.325440
645.114728	48461.995079	32.330458
645.591051	48552.506576	32.335476
645.781429	48639.788056	32.340493
646.739519	48746.647193	32.345511
647.284499	48839.665415	32.350528
647.784213	48915.219849	32.355546
648.686006	49007.431588	32.360564
649.183124	49128.193619	32.365581
650.206373	49218.731661	32.370599
650.686704	49298.879082	32.375616
651.093778	49388.616569	32.380634
651.919557	49482.308397	32.385652
652.427364	49587.213007	32.390669
653.500507	49667.447239	32.395687
654.173302	49733.512268	32.400704
655.371824	49829.654758	32.405722
656.419031	49926.343779	32.410740
657.104007	49996.206661	32.415757
657.558140	50063.616325	32.420775
658.217529	50173.213913	32.425792
658.863721	50236.430310	32.430810
659.743977	50318.186543	32.435828
660.250802	50407.504992	32.440845
661.103734	50455.011783	32.445863
661.383407	50552.917093	32.450880
661.839746	50626.442276	32.455898
662.635140	50695.237872	32.460916
662.984942	50789.106332	32.465933
664.017360	50887.166951	32.470951
664.836093	50969.886717	32.475968
665.530695	51035.778973	32.480986
666.270632	51121.607329	32.486004
666.753081	51225.018737	32.491021
667.422914	51295.501559	32.496039
667.546328	51378.558992	32.501056
668.309385	51468.402236	32.506074
669.077721	51556.331182	32.511092
669.452494	51642.623267	32.516109
670.326032	51738.810112	32.521127
670.704000	51852.417874	32.526144
671.162943	51925.562319	32.531162
671.678173	52011.005410	32.536180
672.174844	52124.250928	32.541197
673.340992	52232.867057	32.546215
673.467630	52331.845807	32.551232
674.661697	52433.690239	32.556250
675.411304	52528.290767	32.561268
675.964039	52609.242342	32.566285
676.722623	52711.368613	32.571303
677.239855	52820.843759	32.576320
677.990411	52893.871086	32.581338
678.571761	52977.074569	32.586356
679.236520	53082.679908	32.591373
680.259926	53162.251652	32.596391
681.068239	53259.773941	32.601408
681.146508	53335.747092	32.606426
682.034413	53436.826190	32.611444
682.738949	53521.382453	32.616461
683.829049	53595.446042	32.621479
683.983499	53699.657690	32.626496
684.472561	53808.021808	32.631514
685.278473	53905.538276	32.636532
685.895213	53983.958203	32.641549
686.449473	54059.299678	32.646567
687.303171	54185.698022	32.651584
688.108080	54290.677200	32.656602
688.927272	54376.740715	32.661620
689.517582	54482.590248	32.666637
690.356702	54567.590014	32.671655
691.231500	54672.452319	32.676672
691.919875	54784.762589	32.681690
692.209350	54858.956907	32.686708
693.237060	54947.016402	32.691725
694.205118	55052.673989	32.696743
694.475508	55161.391322	32.701760
695.528741	55258.482052	32.706778
696.430844	55349.217477	32.711796
696.683796	55448.526111	32.716813
697.540700	55534.158920	32.721831
698.314629	55623.122578	32.726848
699.009359	55722.814522	32.731866
699.831017	55831.311876	32.736884
700.080609	55933.321196	32.741901
701.030469	56029.977955	32.746919
701.945870	56114.535941	32.751936
703.098100	56201.228520	32.756954
704.416190	56297.592033	32.761972
704.704090	56370.212879	32.766989
705.814728	56448.112589	32.772007
706.303061	56555.455958	32.777024
706.775420	56646.363138	32.782042
707.769135	56737.279412	32.787060
707.794651	56817.210963	32.792077
708.480238	56884.422973	32.797095
708.603242	56996.971988	32.802112
709.617470	57112.508267	32.807130
710.147014	57211.192561	32.812148
710.658683	57320.482246	32.817165
711.686183	57418.971622	32.822183
712.525274	57505.481580	32.827200
713.375308	57594.940753	32.832218
714.106657	57708.701255	32.837236
714.916443	57820.591861	32.842253
715.238410	57896.833134	32.847271
716.141344	57986.809774	32.852288
716.848338	58103.091299	32.857306
718.005825	58205.670132	32.862324
718.288996	58291.100096	32.867341
719.302488	58367.525956	32.872359
719.925147	58471.597203	32.877376
720.307424	58583.689093	32.882394
721.248152	58684.935065	32.887412
721.989004	58776.357435	32.892429
722.786671	58868.112054	32.897447
723.348135	58965.713014	32.902464
724.159091	59081.509205	32.907482
724.812120	59162.799920	32.912500
725.187031	59269.431139	32.917517
726.280652	59354.618104	32.922535
727.031545	59435.666295	32.927552
727.406174	59517.611045	32.932570
728.240605	59614.835210	32.937588
728.580866	59734.776005	32.942605
729.382323	59824.682950	32.947623
730.001553	59908.250811	32.952640
730.792870	60011.291216	32.957658
731.481481	60130.570232	32.962676
732.118357	60247.425637	32.967693
732.765481	60334.674730	32.972711
733.686886	60425.790491	32.977728
734.152257	60550.789831	32.982746
734.993286	60659.518994	32.987764
735.497193	60765.024702	32.992781
736.343598	60880.503188	32.997799
737.100503	60983.244631	33.002816
737.762032	61082.950081	33.007834
738.485040	61206.495415	33.012852
739.105362	61347.519185	33.017869
739.940552	61438.893926	33.022887
741.311746	61543.780221	33.027904
741.919367	61660.857231	33.032922
743.035215	61758.481379	33.037940
744.081869	61860.130400	33.042957
744.544766	61983.969925	33.047975
745.333950	62077.238424	33.052992
746.093963	62169.418857	33.058010
746.984311	62260.181519	33.063028
747.574096	62389.595572	33.068045
748.431116	62493.737504	33.073063
749.284177	62600.364337	33.078080
750.290737	62692.727640	33.083098
751.421638	62769.397408	33.088116
751.734513	62883.389171	33.093133
752.650381	62999.234879	33.098151
753.226487	63089.231552	33.103168
754.015198	63187.447509	33.108186
754.904793	63277.981018	33.113204
755.486899	63398.112255	33.118221
756.520735	63488.104632	33.123239
757.426577	63581.411357	33.128256
757.833603	63677.455367	33.133274
758.656890	63796.304048	33.138292
759.431418	63905.169111	33.143309
759.991850	63992.865470	33.148327
760.652520	64083.465648	33.153344
761.031593	64205.550236	33.158362
762.081677	64319.478868	33.163380
762.355994	64417.343272	33.168397
762.826573	64531.078038	33.173415
763.643580	64652.764315	33.178432
764.240290	64765.550442	33.183450
765.537055	64874.056327	33.188468
766.506698	65001.869399	33.193485
767.264833	65116.267841	33.198503
767.683282	65232.183092	33.203520
768.285311	65340.136174	33.208538
769.264437	65461.933221	33.213556
770.015848	65571.335588	33.218573
771.065670	65699.683355	33.223591
771.438752	65827.688568	33.228608
772.073466	65942.168876	33.233626
773.080541	66043.105767	33.238644
773.695918	66167.046642	33.243661
774.837860	66296.400593	33.248679
775.662209	66408.184706	33.253696
776.281278	66502.696202	33.258714
777.174681	66594.703920	33.263732
777.647518	66713.418773	33.268749
777.962219	66843.469012	33.273767
778.958488	66933.147697	33.278784
779.537275	67044.052901	33.283802
780.555453	67158.659945	33.288820
781.263319	67293.306866	33.293837
781.818000	67408.895779	33.298855
782.689590	67518.636290	33.303872
783.544522	67645.460620	33.308890
784.023242	67762.979437	33.313908
784.500435	67887.775216	33.318925
785.416081	68019.794397	33.323943
786.658502	68149.124359	33.328960
786.959560	68289.155029	33.333978
788.058519	68401.347049	33.338996
789.026785	68550.524206	33.344013
789.628731	68662.262354	33.349031
790.741012	68769.668603	33.354048
791.243771	68910.194836	33.359066
792.366642	69032.469587	33.364084
793.357808	69172.607163	33.369101
793.988562	69282.668567	33.374119
794.874240	69413.917589	33.379136
795.339228	69530.209509	33.384154
796.252072	69660.494644	33.389172
797.192474	69780.091734	33.394189
797.747224	69910.880097	33.399207
799.019832	70056.104331	33.404224
799.645698	70177.772387	33.409242
800.440202	70272.550174	33.414260
801.581345	70413.354061	33.419277
802.316655	70538.439115	33.424295
803.521974	70656.954263	33.429312
804.224430	70803.175562	33.434330
804.415160	70911.750192	33.439348
805.232640	71036.116515	33.444365
806.129832	71185.406299	33.449383
807.354161	71299.021978	33.454400
807.787559	71417.611949	33.459418
808.755251	71552.647954	33.464436
809.623446	71679.462848	33.469453
810.511173	71816.878406	33.474471
811.781600	71910.174988	33.479488
812.589281	72026.714905	33.484506
813.022161	72167.729604	33.489524
814.264695	72301.239130	33.494541
814.501166	72416.427573	33.499559
815.690306	72520.697771	33.504576
816.330700	72658.893059	33.509594
817.208178	72782.918260	33.514612
818.062246	72924.488064	33.519629
818.905014	73043.639147	33.524647
819.967599	73165.985692	33.529664
820.526343	73307.353870	33.534682
821.096168	73424.250525	33.539700
821.900227	73542.835371	33.544717
822.194688	73686.108703	33.549735
823.043196	73813.571849	33.554752
823.520953	73940.603752	33.559770
824.601921	74079.823065	33.564788
825.652813	74208.741124	33.569805
826.115062	74348.715649	33.574823
827.160173	74495.696096	33.579840
828.032774	74621.926975	33.584858
829.307685	74743.880684	33.589876
830.175370	74892.151515	33.594893
830.737956	75024.879676	33.599911
831.677341	75126.655357	33.604928
832.318403	75264.430954	33.609946
833.116572	75377.462018	33.614964
834.107082	75497.557174	33.619981
834.133227	75637.959861	33.624999
835.368185	75783.697222	33.630016
836.052541	75909.384899	33.635034
837.076217	76038.988698	33.640052
838.024118	76170.199419	33.645069
838.511266	76321.034492	33.650087
839.568846	76454.062775	33.655104
840.457673	76579.201988	33.660122
841.173085	76709.436169	33.665140
842.228375	76845.641925	33.670157
842.955109	76996.208113	33.675175
843.996330	77127.326970	33.680192
844.342093	77262.292767	33.685210
845.436116	77403.902861	33.690228
846.704772	77541.804262	33.695245
847.306495	77677.792846	33.700263
847.833815	77809.291561	33.705280
848.776357	77942.322594	33.710298
849.392030	78101.870166	33.715316
850.370959	78239.197659	33.720333
851.183407	78396.406412	33.725351
852.093846	78538.553778	33.730368
853.186707	78679.451277	33.735386
853.985398	78827.899370	33.740404
854.947163	78965.816099	33.745421
855.446578	79134.194406	33.750439
856.427050	79294.873109	33.755456
857.276831	79432.083877	33.760474
857.838110	79565.839116	33.765492
858.773936	79721.316537	33.770509
859.727811	79874.761734	33.775527
860.725582	80032.976170	33.780544
861.645669	80190.546746	33.785562
862.619340	80347.179793	33.790580
863.485012	80485.513996	33.795597
863.866606	80639.305640	33.800615
865.040212	80807.907895	33.805632
865.755605	80954.056247	33.810650
866.574945	81104.160725	33.815668
867.682897	81270.247160	33.820685
868.279075	81429.511922	33.825703
869.582472	81568.729376	33.830720
870.532151	81719.031521	33.835738
871.306694	81875.866294	33.840756
872.285385	82040.689359	33.845773
873.068025	82196.803911	33.850791
873.921009	82354.299591	33.855808
874.848821	82506.862570	33.860826
875.747587	82655.711802	33.865844
876.992220	82791.005550	33.870861
877.481287	82961.097058	33.875879
878.480905	83129.195112	33.880896
879.156348	83273.669782	33.885914
879.936692	83430.438493	33.890932
881.006273	83579.695772	33.895949
881.940677	83721.859484	33.900967
882.767611	83894.078387	33.905984
883.722175	84058.414055	33.911002
884.487098	84211.357027	33.916020
885.588496	84349.138309	33.921037
886.417028	84491.577364	33.926055
887.300606	84641.283534	33.931072
888.519462	84809.693119	33.936090
889.082400	84964.838124	33.941108
890.647471	85091.988493	33.946125
891.166529	85219.280644	33.951143
892.203041	85347.323171	33.956160
893.128332	85496.996423	33.961178
893.907901	85616.611566	33.966196
894.911920	85767.962799	33.971213
895.751241	85899.261241	33.976231
897.239295	86013.130704	33.981248
898.316354	86146.441171	33.986266
898.852967	86293.475927	33.991284
899.765119	86419.387520	33.996301
900.578630	86558.596224	34.001319
901.505107	86681.242207	34.006336
902.759358	86822.473945	34.011354
903.426613	86939.001638	34.016372
904.284018	87061.717989	34.021389
904.747071	87224.120185	34.026407
905.566645	87378.536781	34.031424
906.537556	87505.678377	34.036442
907.138063	87654.318329	34.041460
908.213942	87811.795812	34.046477
908.785199	87958.145753	34.051495
909.678830	88117.180266	34.056512
910.513744	88283.483040	34.061530
911.367081	88434.857616	34.066548
912.149403	88587.617954	34.071565
913.186280	88760.509287	34.076583
914.037061	88928.117495	34.081600
914.961866	89075.536041	34.086618
915.386309	89260.769715	34.091636
916.366331	89427.879260	34.096653
917.105410	89582.918536	34.101671
918.170043	89766.601456	34.106688
919.019708	89942.835506	34.111706
919.674390	90106.409396	34.116724
921.329871	90284.031639	34.121741
921.933917	90467.625218	34.126759
922.996039	90630.414084	34.131776
924.194829	90798.275577	34.136794
924.935815	90989.102524	34.141812
925.902761	91142.317250	34.146829
926.793932	91310.530584	34.151847
927.682170	91493.452376	34.156864
928.635983	91686.622877	34.161882
929.393661	91869.499506	34.166900
930.412995	92021.255736	34.171917
931.333881	92182.945794	34.176935
932.248666	92366.547049	34.181952
933.439687	92561.039760	34.186970
934.279593	92736.017809	34.191988
935.553695	92894.066075	34.197005
936.332433	93085.150389	34.202023
937.785255	93258.777990	34.207040
938.404039	93424.000760	34.212058
939.623666	93583.239705	34.217076
940.715876	93744.063958	34.222093
941.443549	93919.145105	34.227111
942.311275	94087.938781	34.232128
943.302359	94246.422401	34.237146
944.144332	94423.646506	34.242164
945.309346	94591.673115	34.247181
945.990707	94753.312421	34.252199
947.233842	94910.841063	34.257216
948.325982	95103.427597	34.262234
949.074243	95278.464545	34.267252
950.279878	95431.154576	34.272269
950.935510	95586.626322	34.277287
951.650808	95748.329937	34.282304
952.589958	95905.953193	34.287322
953.594110	96075.352119	34.292340
954.174695	96235.422892	34.297357
955.292856	96394.272978	34.302375
955.939613	96563.227929	34.307392
957.093776	96729.891244	34.312410
957.652851	96901.742968	34.317428
958.798556	97065.536305	34.322445
959.718734	97247.008907	34.327463
960.289456	97413.089572	34.332480
961.361037	97592.267336	34.337498
962.118943	97779.562433	34.342516
963.142224	97964.473070	34.347533
963.885180	98148.152721	34.352551
965.055602	98316.400246	34.357568
966.021187	98521.289397	34.362586
966.869397	98727.098494	34.367604
968.214321	98902.638790	34.372621
969.055410	99068.932804	34.377639
970.012080	99267.018291	34.382656
971.036092	99461.485969	34.387674
971.820588	99658.900333	34.392692
972.858183	99834.251049	34.397709
973.885117	100019.834732	34.402727
974.861069	100237.960562	34.407744
976.162495	100435.283045	34.412762
976.877732	100623.885352	34.417780
977.883573	100798.520040	34.422797
979.382922	100989.470911	34.427815
980.170843	101208.054028	34.432832
981.580823	101383.784577	34.437850
982.499576	101560.433118	34.442868
983.375156	101732.379858	34.447885
984.389773	101929.368880	34.452903
985.267370	102147.565458	34.457920
986.693891	102318.665504	34.462938
987.452152	102513.251282	34.467956
988.685905	102699.156075	34.472973
989.526543	102896.535863	34.477991
990.455768	103076.871626	34.483008
991.531878	103257.146426	34.488026
992.800754	103438.777226	34.493044
994.235555	103581.893786	34.498061
995.982190	103763.732930	34.503079
996.645273	103950.804718	34.508096
997.702798	104133.260431	34.513114
998.657299	104309.282648	34.518132
999.059994	104479.819077	34.523149
1000.548577	104647.093881	34.528167
1001.277376	104838.105848	34.533184
1002.309505	105006.192808	34.538202
1002.914833	105190.490866	34.543220
1003.698123	105386.886183	34.548237
1004.675031	105564.768468	34.553255
1005.701464	105742.244889	34.558272
1006.461403	105937.255221	34.563290
1007.290449	106140.499802	34.568308
1008.490936	106325.929730	34.573325
1009.558717	106510.053158	34.578343
1010.388748	106700.612541	34.583360
1011.339262	106890.583531	34.588378
1012.688397	107099.562615	34.593396
1013.837574	107280.321975	34.598413
1014.861195	107475.464898	34.603431
1015.924194	107665.625568	34.608448
1016.994395	107835.586193	34.613466
1017.793654	108006.466515	34.618484
1019.664681	108184.782604	34.623501
1020.774266	108359.882054	34.628519
1021.276645	108525.381478	34.633536
1022.172412	108701.898983	34.638554
1023.414655	108882.046043	34.643572
1024.028975	109033.547765	34.648589
1025.117618	109213.253818	34.653607
1025.641910	109414.598214	34.658624
1027.227764	109592.983535	34.663642
1027.740762	109754.537216	34.668660
1028.180622	109958.128809	34.673677
1029.450210	110149.349790	34.678695
1030.294659	110347.025944	34.683712
1031.555796	110547.712609	34.688730
1032.220951	110744.901992	34.693748
1033.385486	110943.112341	34.698765
1034.190569	111161.991553	34.703783
1035.154677	111361.112044	34.708800
1036.370326	111564.245757	34.713818
1037.609079	111775.040469	34.718836
1038.940420	111957.562180	34.723853
1040.245838	112144.586103	34.728871
1041.192092	112352.621583	34.733888
1042.548511	112540.488498	34.738906
1043.023675	112743.664635	34.743924
1044.036578	112961.624734	34.748941
1045.364322	113154.415474	34.753959
1046.322353	113366.548277	34.758976
1047.179443	113584.995102	34.763994
1048.502976	113786.455522	34.769012
1049.280901	113996.190774	34.774029
1050.322925	114207.138135	34.779047
1051.538843	114407.417447	34.784064
1052.625982	114606.959403	34.789082
1053.567180	114842.909392	34.794100
1054.539324	115061.729001	34.799117
1055.193370	115260.853124	34.804135
1056.145073	115477.867846	34.809152
1057.315327	115700.346273	34.814170
1058.279376	115937.644669	34.819188
1059.474714	116168.648612	34.824205
1060.815454	116366.261084	34.829223
1061.702542	116589.110080	34.834240
1062.731837	116816.118117	34.839258
1064.166860	117040.109138	34.844276
1065.020217	117266.630441	34.849293
1066.270279	117484.726405	34.854311
1067.044614	117697.252084	34.859328
1068.296317	117919.544688	34.864346
1069.201816	118163.485039	34.869364
1070.508482	118399.392080	34.874381
1071.629241	118593.927148	34.879399
1072.673267	118822.304587	34.884416
1073.663842	119065.605175	34.889434
1075.114753	119291.271204	34.894452
1075.946627	119491.029474	34.899469
1077.320846	119691.637208	34.904487
1078.215092	119946.947230	34.909504
1079.257837	120169.963473	34.914522
1080.424388	120388.082870	34.919540
1081.380125	120605.427808	34.924557
1082.398925	120819.292209	34.929575
1083.076904	121072.582622	34.934592
1084.420908	121297.103716	34.939610
1085.855287	121517.430208	34.944628
1086.672533	121751.963186	34.949645
1087.807185	121965.018668	34.954663
1088.669013	122200.105442	34.959680
1089.703858	122426.232221	34.964698
1091.117658	122619.998579	34.969716
1091.815819	122840.697403	34.974733
1092.783372	123066.244688	34.979751
1093.857934	123292.789788	34.984768
1094.805738	123512.033226	34.989786
1096.354471	123722.460795	34.994804
1097.412628	123947.518367	34.999821
1098.278638	124169.466685	35.004839
1099.522555	124413.923564	35.009856
1100.419859	124619.674966	35.014874
1101.625399	124828.152178	35.019892
1102.949039	125069.838727	35.024909
1104.048836	125314.732354	35.029927
1104.766455	125537.412412	35.034944
1105.758268	125750.404852	35.039962
1107.099260	125990.321816	35.044980
1108.069801	126241.504816	35.049997
1109.595204	126489.341333	35.055015
1110.287918	126714.353450	35.060032
1111.124111	126941.662784	35.065050
1112.338767	127195.018621	35.070068
1113.186962	127437.689919	35.075085
1114.770040	127679.075881	35.080103
1115.499760	127952.973377	35.085120
1116.422213	128195.055493	35.090138
1117.578736	128439.268144	35.095156
1118.606496	128701.970112	35.100173
1120.101805	128956.675806	35.105191
1121.463971	129211.164791	35.110208
1122.624774	129464.358320	35.115226
1123.873894	129723.724508	35.120244
1124.811373	129968.796693	35.125261
1126.825020	130209.903452	35.130279
1127.999155	130451.467546	35.135296
1129.067061	130675.040060	35.140314
1130.533855	130911.590887	35.145332
1131.745695	131160.087494	35.150349
1132.976596	131393.676941	35.155367
1133.468865	131656.340379	35.160384
1134.668119	131899.077710	35.165402
1136.556015	132115.452362	35.170420
1137.718955	132340.973170	35.175437
1138.761342	132575.565910	35.180455
1139.664206	132835.218029	35.185472
1140.785972	133065.884515	35.190490
1142.066101	133296.323730	35.195508
1143.010878	133555.721340	35.200525
1144.084932	133809.141947	35.205543
1145.131593	134036.772957	35.210560
1146.280213	134287.548416	35.215578
1147.734947	134536.868236	35.220596
1148.382247	134773.558022	35.225613
1149.593437	135017.179326	35.230631
1150.590094	135275.149911	35.235648
1151.800016	135536.446724	35.240666
1152.487227	135775.596617	35.245684
1153.535502	136024.868326	35.250701
1154.653980	136296.632257	35.255719
1155.690300	136572.227877	35.260736
1156.705478	136833.174327	35.265754
1158.555335	137079.139821	35.270772
1159.340083	137355.011796	35.275789
1160.151938	137599.770704	35.280807
1161.871254	137851.354403	35.285824
1162.833991	138139.437619	35.290842
1163.907050	138406.802064	35.295860
1164.899535	138660.667185	35.300877
1165.868879	138914.462010	35.305895
1166.884167	139177.607736	35.310912
1167.969873	139433.644060	35.315930
1169.182418	139689.838918	35.320948
1170.367827	139953.545919	35.325965
1171.517758	140215.498532	35.330983
1172.864745	140465.908383	35.336000
1173.709658	140737.576621	35.341018
1175.300190	140990.600067	35.346036
1175.940480	141262.040061	35.351053
1177.176348	141536.363527	35.356071
1178.251148	141825.017984	35.361088
1179.081419	142090.119007	35.366106
1180.233375	142371.664951	35.371124
1181.202620	142661.890835	35.376141
1182.354508	142950.389966	35.381159
1183.650236	143223.499916	35.386176
1184.437268	143534.748287	35.391194
1186.130875	143839.459121	35.396212
1187.299954	144108.716935	35.401229
1188.519802	144411.647050	35.406247
1190.122860	144710.065775	35.411264
1191.465127	144975.206001	35.416282
1192.927606	145272.651010	35.421300
1194.005615	145581.435085	35.426317
1195.315950	145856.896630	35.431335
1196.452208	146125.845769	35.436352
1197.387995	146416.070594	35.441370
1198.660208	146708.093708	35.446388
1200.161138	147003.733651	35.451405
1201.219303	147298.777038	35.456423
1202.602709	147602.468596	35.461440
1203.956918	147893.359295	35.466458
1205.076815	148195.476173	35.471476
1206.365408	148489.514899	35.476493
1207.433296	148761.957379	35.481511
1208.482188	149057.016809	35.486528
1209.668385	149379.284177	35.491546
1211.087127	149670.178608	35.496564
1212.054202	149965.969152	35.501581
1213.347034	150263.559946	35.506599
1214.849355	150564.961354	35.511616
1215.687550	150884.712294	35.516634
1217.131455	151178.430119	35.521652
1218.353719	151456.041800	35.526669
1219.913872	151757.709793	35.531687
1221.304613	152052.825786	35.536704
1222.212024	152359.831782	35.541722
1223.605528	152647.507125	35.546740
1224.847729	152961.539996	35.551757
1226.175857	153244.766245	35.556775
1227.853037	153551.781824	35.561792
1228.827222	153837.633017	35.566810
1229.874246	154134.978384	35.571828
1230.768285	154438.579040	35.576845
1231.751054	154736.662710	35.581863
1233.003251	155049.874202	35.586880
1234.515077	155359.278263	35.591898
1235.807843	155662.594558	35.596916
1237.155219	155955.350976	35.601933
1238.309379	156267.231401	35.606951
1239.901916	156564.087071	35.611968
1240.562950	156866.426261	35.616986
1242.207130	157175.785026	35.622004
1243.401700	157474.590675	35.627021
1244.312335	157779.039476	35.632039
1245.657754	158092.552017	35.637056
1246.990261	158378.606160	35.642074
1247.999509	158669.269686	35.647092
1248.980395	158980.921337	35.652109
1250.190350	159276.579539	35.657127
1251.730593	159554.616179	35.662144
1252.585171	159877.940897	35.667162
1254.201539	160154.916266	35.672180
1255.794870	160466.744863	35.677197
1256.728340	160783.213610	35.682215
1258.074836	161068.549001	35.687232
1258.877130	161350.893544	35.692250
1260.455231	161656.416254	35.697268
1261.632257	161983.738813	35.702285
1262.513757	162293.834116	35.707303
1264.049786	162578.704809	35.712320
1264.779000	162899.981116	35.717338
1266.341687	163220.932068	35.722356
1267.678831	163557.755648	35.727373
1268.568608	163863.484521	35.732391
1269.973362	164158.118495	35.737408
1271.254699	164506.973389	35.742426
1272.477787	164839.804413	35.747444
1273.643429	165160.455241	35.752461
1275.373860	165486.343920	35.757479
1276.887693	165814.859074	35.762496
1277.813716	166144.133534	35.767514
1278.922370	166455.973144	35.772532
1280.330703	166781.480860	35.777549
1281.622003	167126.955423	35.782567
1282.917797	167467.407652	35.787584
1283.900235	167805.541646	35.792602
1285.570780	168124.240896	35.797620
1287.046843	168463.503908	35.802637
1288.849182	168799.378715	35.807655
1290.658676	169117.542078	35.812672
1291.394574	169434.476528	35.817690
1292.923669	169741.423409	35.822708
1294.184160	170083.817813	35.827725
1295.680142	170418.017187	35.832743
1296.948919	170727.018656	35.837760
1297.985645	171049.472651	35.842778
1299.422214	171383.333760	35.847796
1300.293582	171717.214491	35.852813
1301.884613	172045.789067	35.857831
1303.547950	172368.593191	35.862848
1304.850882	172713.652663	35.867866
1305.930160	173040.796164	35.872884
1307.390917	173358.856819	35.877901
1308.289361	173697.975640	35.882919
1309.867177	174008.407715	35.887936
1310.799403	174349.454557	35.892954
1312.252318	174689.034769	35.897972
1313.624616	175041.802904	35.902989
1314.395502	175380.548945	35.908007
1315.802607	175727.999361	35.913024
1316.902022	176085.490307	35.918042
1318.403573	176415.011590	35.923060
1320.174202	176754.097368	35.928077
1321.225875	177105.753569	35.933095
1322.557977	177432.746344	35.938112
1323.877178	177783.563832	35.943130
1325.178756	178137.648292	35.948148
1326.511538	178488.811282	35.953165
1327.812305	178839.347531	35.958183
1329.585740	179191.153523	35.963200
1330.659390	179532.442361	35.968218
1331.873028	179848.949917	35.973236
1333.212437	180201.900784	35.978253
1334.341588	180564.927727	35.983271
1336.031385	180901.898029	35.988288
1336.912598	181233.305528	35.993306
1338.405834	181576.404717	35.998324
1339.719117	181903.417444	36.003341
1341.028663	182220.368292	36.008359
1342.485261	182551.575192	36.013376
1343.482367	182909.157800	36.018394
1344.803860	183253.045395	36.023412
1347.137415	183561.737973	36.028429
1348.143433	183880.970232	36.033447
1349.691320	184226.362650	36.038464
1350.961955	184568.033462	36.043482
1351.606382	184891.976947	36.048500
1353.397015	185254.343912	36.053517
1354.883801	185607.574037	36.058535
1355.997372	185923.081939	36.063552
1357.251812	186268.015667	36.068570
1358.329910	186631.918440	36.073588
1360.037360	186994.729743	36.078605
1361.031349	187350.578500	36.083623
1362.908319	187682.661985	36.088640
1364.033491	188025.927307	36.093658
1365.430295	188405.769994	36.098676
1367.195181	188759.139674	36.103693
1368.318632	189109.888364	36.108711
1369.797134	189463.309758	36.113728
1371.056266	189828.650769	36.118746
1372.265698	190197.328081	36.123764
1373.677782	190564.679575	36.128781
1374.756876	190923.469269	36.133799
1376.498861	191281.593273	36.138816
1377.725867	191681.529640	36.143834
1379.115091	192053.235738	36.148852
1381.075957	192409.908839	36.153869
1382.530711	192782.573508	36.158887
1384.092670	193132.715819	36.163904
1385.486232	193503.452895	36.168922
1386.751558	193868.640566	36.173940
1388.253022	194223.737411	36.178957
1389.228451	194600.897545	36.183975
1390.590413	194945.954819	36.188992
1391.953591	195328.806174	36.194010
1393.278635	195718.191368	36.199028
1394.791062	196085.357356	36.204045
1396.214174	196445.405667	36.209063
1397.541971	196811.641593	36.214080
1398.957290	197189.328936	36.219098
1400.291084	197580.069995	36.224116
1401.937525	197949.738438	36.229133
1403.303781	198308.499149	36.234151
1404.577784	198697.568432	36.239168
1405.843839	199092.633659	36.244186
1407.187496	199478.585732	36.249204
1408.747270	199836.573929	36.254221
1409.781370	200247.960271	36.259239
1411.569545	200617.265015	36.264256
1413.080648	200986.109695	36.269274
1414.272566	201377.988777	36.274292
1415.929940	201777.080852	36.279309
1417.070834	202162.929582	36.284327
1418.792514	202534.680755	36.289344
1420.382220	202923.430609	36.294362
1422.065713	203291.180145	36.299380
1423.443117	203650.767571	36.304397
1424.705998	204036.378080	36.309415
1425.979066	204432.692187	36.314432
1427.441785	204819.759478	36.319450
1428.722008	205183.535210	36.324468
1430.538639	205540.926685	36.329485
1431.331463	205929.557916	36.334503
1433.061953	206306.241101	36.339520
1434.241632	206666.714268	36.344538
1435.386145	207027.156904	36.349556
1436.853486	207401.032273	36.354573
1437.890659	207793.696031	36.359591
1439.281071	208160.794918	36.364608
1440.882791	208554.702664	36.369626
1442.183319	208962.908514	36.374644
1443.615958	209332.850248	36.379661
1444.690777	209730.736343	36.384679
1446.218489	210129.971844	36.389696
1447.761999	210540.304425	36.394714
1448.786791	210944.794930	36.399732
1450.451973	211330.744759	36.404749
1452.255250	211747.275217	36.409767
1453.166415	212147.701819	36.414784
1455.068898	212552.360253	36.419802
1456.558175	212965.279022	36.424820
1458.102202	213376.057535	36.429837
1459.547079	213791.832054	36.434855
1460.935186	214191.389776	36.439872
1462.467479	214603.065031	36.444890
1463.894236	215029.565817	36.449908
1465.489982	215444.917088	36.454925
1466.960176	215877.967164	36.459943
1468.155781	216304.182116	36.464960
1469.631688	216724.282964	36.469978
1470.914296	217157.395576	36.474996
1472.182650	217633.027543	36.480013
1473.435718	218087.584678	36.485031
1475.235989	218520.161112	36.490048
1476.832970	218941.572745	36.495066
1478.449626	219396.355574	36.500084
1479.513529	219827.002246	36.505101
1481.219712	220256.859099	36.510119
1483.037148	220714.764315	36.515136
1484.385845	221158.703809	36.520154
1485.545233	221595.107822	36.525172
1487.381336	222044.075837	36.530189
1488.931582	222485.549638	36.535207
1490.254133	222928.155031	36.540224
1492.036279	223373.505709	36.545242
1493.404337	223828.501939	36.550260
1495.280117	224260.658888	36.555277
1496.418769	224722.224259	36.560295
1498.339461	225159.126970	36.565312
1500.050168	225599.266349	36.570330
1501.730171	226060.671747	36.575348
1502.857626	226477.035417	36.580365
1504.253906	226917.714361	36.585383
1505.676565	227375.179755	36.590400
1507.820338	227799.635310	36.595418
1509.096596	228263.630597	36.600436
1510.452702	228710.520352	36.605453
1511.975637	229139.274014	36.610471
1513.756036	229585.588913	36.615488
1515.920547	230007.686457	36.620506
1517.720630	230432.055347	36.625524
1519.218589	230867.575416	36.630541
1520.442986	231299.586007	36.635559
1521.914631	231734.935463	36.640576
1523.402751	232180.291423	36.645594
1524.730627	232603.678304	36.650612
1526.841122	233009.563239	36.655629
1528.417842	233448.355243	36.660647
1529.606370	233861.786367	36.665664
1531.366065	234267.123121	36.670682
1532.436156	234704.300639	36.675700
1533.886706	235113.069037	36.680717
1535.900788	235514.125200	36.685735
1537.411277	235905.486030	36.690752
1538.848658	236320.737098	36.695770
1540.154212	236756.713095	36.700788
1541.441674	237162.211549	36.705805
1542.586109	237590.316509	36.710823
1543.948236	238008.683250	36.715840
1545.249737	238427.797663	36.720858
1546.443293	238874.593308	36.725876
1547.854175	239328.542907	36.730893
1549.260586	239769.945895	36.735911
1550.942984	240221.693757	36.740928
1552.531911	240685.752650	36.745946
1553.869562	241132.961808	36.750964
1555.479638	241587.595228	36.755981
1556.960385	242056.984225	36.760999
1558.437980	242535.519584	36.766016
1560.346083	242984.467635	36.771034
1561.879341	243455.324405	36.776052
1563.437664	243934.306778	36.781069
1565.164186	244387.250389	36.786087
1566.484270	244843.462644	36.791104
1568.526016	245327.067554	36.796122
1569.821234	245804.014118	36.801140
1571.754121	246274.505725	36.806157
1573.610436	246770.413411	36.811175
1574.957761	247227.057292	36.816192
1576.651269	247690.351110	36.821210
1577.829454	248171.258581	36.826228
1579.525583	248664.046071	36.831245
1581.177125	249133.674344	36.836263
1582.728421	249630.018233	36.841280
1584.398667	250116.664737	36.846298
1585.495504	250598.351352	36.851316
1587.263500	251069.538065	36.856333
1588.725635	251582.817760	36.861351
1590.094846	252091.794938	36.866368
1592.298332	252555.112838	36.871386
1594.018067	253055.370893	36.876404
1595.532330	253563.208109	36.881421
1596.920653	254062.251747	36.886439
1598.918371	254538.434100	36.891456
1600.848089	255015.644206	36.896474
1601.980913	255524.867171	36.901492
1604.191671	256020.448991	36.906509
1606.573925	256503.250451	36.911527
1607.903629	256966.411358	36.916544
1609.839916	257442.275679	36.921562
1611.391110	257928.060248	36.926580
1613.358294	258427.214741	36.931597
1615.068830	258882.286289	36.936615
1616.285051	259366.043651	36.941632
1618.331827	259818.748311	36.946650
1619.695888	260270.702003	36.951668
1621.314365	260753.605832	36.956685
1623.049032	261238.141770	36.961703
1624.345469	261715.840348	36.966720
1626.452919	262175.927650	36.971738
1627.773985	262640.869697	36.976756
1629.299791	263108.775514	36.981773
1631.214585	263599.048200	36.986791
1632.707590	264087.180288	36.991808
1634.275832	264530.336017	36.996826
1635.550231	265012.127679	37.001844
1637.257288	265491.840922	37.006861
1638.775529	265934.623375	37.011879
1640.302712	266391.629975	37.016896
1642.278237	266863.169232	37.021914
1643.639257	267312.276950	37.026932
1645.291628	267750.844809	37.031949
1646.737426	268209.845230	37.036967
1647.966408	268701.066905	37.041984
1649.805744	269167.343204	37.047002
1651.037400	269633.795583	37.052020
1652.390275	270113.056114	37.057037
1654.337409	270600.601153	37.062055
1655.903864	271082.238775	37.067072
1657.668348	271560.617019	37.072090
1659.511719	272067.026603	37.077108
1661.119400	272543.829186	37.082125
1662.724966	273023.324234	37.087143
1664.492388	273510.006371	37.092160
1665.938696	274012.236552	37.097178
1667.774773	274509.752964	37.102196
1669.271487	274994.674018	37.107213
1671.110750	275465.820327	37.112231
1672.701453	275987.837692	37.117248
1674.451443	276496.720073	37.122266
1676.387219	277001.938304	37.127284
1678.011691	277517.901423	37.132301
1679.687960	278016.225643	37.137319
1680.580293	278534.339710	37.142336
1681.975039	279053.030258	37.147354
1683.978850	279565.116193	37.152372
1685.382748	280094.090872	37.157389
1686.957603	280646.787170	37.162407
1688.615437	281194.159326	37.167424
1690.270491	281705.129338	37.172442
1691.982459	282244.818379	37.177460
1693.476324	282793.026201	37.182477
1695.266765	283345.146249	37.187495
1696.562902	283900.521469	37.192512
1698.870240	284433.146068	37.197530
1700.349297	284978.149343	37.202548
1701.982056	285550.102048	37.207565
1704.235505	286108.640081	37.212583
1705.962217	286676.179054	37.217600
1707.795485	287211.642038	37.222618
1709.473728	287751.142213	37.227636
1710.765358	288320.042640	37.232653
1712.540095	288878.065830	37.237671
1714.600878	289451.178736	37.242688
1716.131186	289994.429339	37.247706
1718.118293	290543.901938	37.252724
1719.551481	291123.944584	37.257741
1721.671144	291681.188884	37.262759
1723.382951	292245.635728	37.267776
1725.208976	292807.140323	37.272794
1727.106711	293356.184588	37.277812
1728.494218	293931.218825	37.282829
1730.031104	294498.885224	37.287847
1731.963208	295051.878915	37.292864
1733.570909	295621.255693	37.297882
1735.557292	296185.157196	37.302900
1736.831383	296759.765139	37.307917
1738.406430	297329.266133	37.312935
1740.181348	297911.253182	37.317952
1742.122808	298481.322970	37.322970
1743.824724	299047.492516	37.327988
1745.292966	299643.541378	37.333005
1747.135683	300215.853555	37.338023
1748.978916	300802.182600	37.343040
1750.598206	301362.384900	37.348058
1752.545645	301918.694884	37.353076
1754.022502	302473.682566	37.358093
1755.815156	303047.689020	37.363111
1757.811323	303605.378529	37.368128
1759.181096	304145.872325	37.373146
1761.073785	304730.341682	37.378164
1762.546838	305286.126770	37.383181
1764.069746	305848.046497	37.388199
1765.434286	306444.275090	37.393216
1767.184612	307007.521685	37.398234
1769.178350	307580.934140	37.403252
1770.199618	308202.147447	37.408269
1772.361579	308786.978242	37.413287
1774.040780	309374.221206	37.418304
1775.938578	309987.632893	37.423322
1777.598389	310591.581328	37.428340
1779.270305	311195.650394	37.433357
1781.021779	311797.492516	37.438375
1782.601016	312437.350095	37.443392
1784.460703	313047.621764	37.448410
1786.364656	313644.701471	37.453428
1787.901596	314278.583449	37.458445
1790.005936	314921.203980	37.463463
1792.083505	315515.980591	37.468480
1794.182506	316145.665991	37.473498
1796.082307	316778.019950	37.478516
1798.037576	317389.358771	37.483533
1800.837597	317988.897533	37.488551
1802.083984	318615.426794	37.493568
1804.201748	319237.921718	37.498586
1806.330156	319832.375720	37.503604
1807.735325	320473.488728	37.508621
1809.649195	321065.098291	37.513639
1811.274521	321706.036623	37.518656
1813.192611	322328.257560	37.523674
1814.687392	322945.641991	37.528692
1816.450997	323573.818538	37.533709
1818.407404	324186.976487	37.538727
1820.331277	324826.972348	37.543744
1821.806748	325458.885431	37.548762
1823.582263	326088.533828	37.553780
1825.183776	326731.433006	37.558797
1827.156915	327347.350936	37.563815
1829.418940	327997.364310	37.568832
1831.208120	328646.484038	37.573850
1833.401053	329271.105876	37.578868
1835.331911	329932.400712	37.583885
1837.154754	330555.166119	37.588903
1838.815652	331182.140796	37.593920
1840.190177	331821.164610	37.598938
1842.278896	332473.849204	37.603956
1843.949532	333130.403522	37.608973
1846.087500	333759.759652	37.613991
1848.049396	334401.552072	37.619008
1850.156405	335052.934781	37.624026
1851.980747	335703.239507	37.629044
1853.797295	336350.161521	37.634061
1855.425938	336973.726594	37.639079
1857.567313	337623.016969	37.644096
1859.264966	338259.451657	37.649114
1861.234764	338895.529254	37.654132
1862.957473	339548.926855	37.659149
1864.403592	340201.118125	37.664167
1866.374573	340862.530551	37.669184
1868.091485	341509.913906	37.674202
1869.911384	342158.109741	37.679220
1871.654980	342807.579041	37.684237
1873.448108	343474.291980	37.689255
1875.760741	344103.090739	37.694272
1877.489221	344738.831011	37.699290
1879.262117	345367.931140	37.704308
1881.079160	345991.888860	37.709325
1882.727843	346619.064325	37.714343
1884.738119	347276.121135	37.719360
1886.337044	347906.130602	37.724378
1888.127180	348559.728896	37.729396
1890.024922	349209.747217	37.734413
1891.970362	349844.495695	37.739431
1893.686151	350519.245114	37.744448
1894.991560	351196.184122	37.749466
1897.266252	351845.494074	37.754484
1898.970016	352530.113236	37.759501
1900.964277	353183.256866	37.764519
1902.779379	353861.518355	37.769536
1904.560465	354528.634742	37.774554
1906.613108	355220.844064	37.779572
1908.353997	355907.993297	37.784589
1910.513678	356594.859560	37.789607
1912.480450	357285.781304	37.794624
1914.264985	357973.448612	37.799642
1916.435886	358677.940247	37.804660
1918.055055	359381.775258	37.809677
1920.067006	360066.072295	37.814695
1922.474235	360763.562884	37.819712
1924.153102	361463.673677	37.824730
1926.238158	362169.718669	37.829748
1927.947690	362871.347932	37.834765
1930.032728	363578.890651	37.839783
1932.073524	364297.718131	37.844800
1933.814397	364999.888477	37.849818
1936.009213	365691.848926	37.854836
1938.304374	366411.255616	37.859853
1940.019510	367132.317563	37.864871
1941.761485	367859.526169	37.869888
1943.772995	368564.073759	37.874906
1945.700853	369281.381968	37.879924
1947.384452	370006.682121	37.884941
1949.198015	370755.918172	37.889959
1950.997304	371476.985377	37.894976
1953.069499	372213.415777	37.899994
1955.313784	372936.029935	37.905012
1957.127025	373697.432440	37.910029
1959.084917	374433.279088	37.915047
1960.964783	375177.544284	37.920064
1962.728572	375909.157146	37.925082
1964.484697	376636.977294	37.930100
1966.505568	377405.951794	37.935117
1968.312489	378182.882870	37.940135
1970.457716	378922.841110	37.945152
1972.027877	379671.221945	37.950170
1974.265065	380426.856207	37.955188
1976.297190	381199.599647	37.960205
1978.444295	381958.866639	37.965223
1980.559684	382733.818384	37.970240
1982.284316	383511.656760	37.975258
1984.654295	384267.158145	37.980276
1986.554047	385016.355526	37.985293
1988.564905	385777.916468	37.990311
1990.982760	386552.095462	37.995328
1992.758267	387326.336676	38.000346
1994.943721	388070.092643	38.005364
1997.248351	388813.963914	38.010381
1998.954977	389572.468932	38.015399
2001.024231	390320.248254	38.020416
2002.877195	391113.424540	38.025434
2005.311397	391854.465281	38.030452
2007.142141	392576.930282	38.035469
2008.740404	393306.210538	38.040487
2010.918563	394023.692093	38.045504
2012.835003	394778.335448	38.050522
2014.484081	395522.561020	38.055540
2016.221872	396265.055504	38.060557
2018.162281	397003.848458	38.065575
2020.026114	397757.209775	38.070592
2021.783988	398539.437795	38.075610
2024.098649	399297.400075	38.080628
2025.927326	400047.566472	38.085645
2027.837886	400800.234565	38.090663
2030.209034	401579.619796	38.095680
2032.332751	402372.785601	38.100698
2034.413363	403134.082874	38.105716
2036.645452	403895.258998	38.110733
2038.231647	404672.054731	38.115751
2040.198156	405471.343727	38.120768
2041.967319	406281.842276	38.125786
2043.850426	407048.616487	38.130804
2045.799562	407849.639779	38.135821
2047.834389	408668.639964	38.140839
2049.816553	409460.718286	38.145856
2051.748650	410287.870735	38.150874
2054.018416	411122.061349	38.155892
2055.831913	411918.859133	38.160909
2058.076671	412742.794757	38.165927
2060.192512	413561.482760	38.170944
2062.203000	414402.808933	38.175962
2064.083712	415231.616850	38.180980
2066.385264	416076.033588	38.185997
2068.265984	416899.849923	38.191015
2070.553502	417748.622342	38.196032
2072.775302	418612.523389	38.201050
2074.628331	419445.280117	38.206068
2077.192391	420273.815306	38.211085
2078.863402	421138.532872	38.216103
2081.189878	422005.189528	38.221120
2083.282814	422859.371002	38.226138
2085.319619	423702.112663	38.231156
2087.794084	424565.592936	38.236173
2089.459512	425409.224535	38.241191
2091.794537	426268.085761	38.246208
2093.597039	427135.967580	38.251226
2095.724762	427986.701159	38.256244
2097.707810	428854.796074	38.261261
2099.524392	429748.152356	38.266279
2101.871735	430606.251350	38.271296
2104.110612	431468.590296	38.276314
2106.045155	432354.691747	38.281332
2108.333991	433224.046543	38.286349
2110.235621	434091.661475	38.291367
2112.533076	434979.325916	38.296384
2114.632501	435870.228912	38.301402
2117.099331	436762.100181	38.306420
2119.012581	437625.735070	38.311437
2121.354973	438514.927275	38.316455
2123.702888	439398.567570	38.321472
2125.828028	440276.086771	38.326490
2127.953066	441140.819256	38.331508
2130.067955	442040.690414	38.336525
2132.091541	442943.222531	38.341543
2134.519244	443797.378820	38.346560
2136.338029	444678.774114	38.351578
2138.549876	445570.138204	38.356596
2140.649791	446438.160696	38.361613
2142.635936	447333.588653	38.366631
2144.950992	448205.957654	38.371648
2147.224202	449076.224398	38.376666
2149.678325	449913.747546	38.381684
2151.401508	450757.529914	38.386701
2153.254780	451621.895175	38.391719
2155.532308	452500.317895	38.396736
2157.571680	453344.805602	38.401754
2159.794932	454190.746514	38.406772
2161.999430	455061.286063	38.411789
2164.133653	455940.398225	38.416807
2166.607772	456786.749149	38.421824
2168.762084	457642.978992	38.426842
2170.470102	458512.444562	38.431860
2172.519870	459390.362241	38.436877
2174.418035	460291.019829	38.441895
2176.930846	461156.043800	38.446912
2179.487355	462022.944826	38.451930
2181.558479	462894.994692	38.456948
2183.819545	463809.439489	38.461965
2186.351413	464699.432668	38.466983
2188.249545	465583.525921	38.472000
2190.565687	466481.360340	38.477018
2192.643234	467372.976434	38.482036
2195.002119	468260.866730	38.487053
2196.987888	469158.127926	38.492071
2199.129108	470056.282353	38.497088
2201.367958	470968.225412	38.502106
2203.377355	471893.351982	38.507124
2206.091242	472816.549337	38.512141
2207.734992	473721.082649	38.517159
2209.833641	474625.952727	38.522176
2212.171560	475566.004471	38.527194
2214.138982	476508.646988	38.532212
2216.611791	477431.002688	38.537229
2218.983469	478373.434299	38.542247
2221.010691	479293.599340	38.547264
2223.428667	480226.130094	38.552282
2225.514778	481182.103569	38.557300
2227.989935	482124.933150	38.562317
2229.675095	483077.439693	38.567335
2232.105765	484035.530389	38.572352
2234.264158	484988.969740	38.577370
2236.151449	485939.676822	38.582388
2239.001128	486906.887392	38.587405
2240.932845	487895.856388	38.592423
2242.871820	488857.961710	38.597440
2245.128068	489817.387955	38.602458
2246.858174	490803.300198	38.607476
2249.367250	491794.985010	38.612493
2251.160784	492786.075483	38.617511
2253.602607	493758.580794	38.622528
2255.876335	494752.054119	38.627546
2258.333988	495764.566343	38.632564
2260.380572	496765.329051	38.637581
2262.791966	497763.298801	38.642599
2265.447936	498739.675394	38.647616
2267.550248	499741.465250	38.652634
2269.539231	500749.419851	38.657652
2272.228968	501760.376756	38.662669
2274.931009	502758.760444	38.667687
2277.775155	503726.291696	38.672704
2280.264326	504718.338258	38.677722
2282.389612	505728.088181	38.682740
2285.035785	506693.209018	38.687757
2287.510083	507664.453827	38.692775
2289.009191	508655.669713	38.697792
2291.537221	509630.268028	38.702810
2293.648202	510621.111843	38.707828
2295.866827	511616.414645	38.712845
2298.100915	512596.277003	38.717863
2299.711303	513547.901653	38.722880
2301.829993	514521.968522	38.727898
2303.855789	515492.865883	38.732916
2306.452511	516465.575213	38.737933
2308.485030	517446.784502	38.742951
2310.678157	518446.401121	38.747968
2313.096936	519424.903059	38.752986
2315.031435	520410.578609	38.758004
2317.490775	521383.710065	38.763021
2320.036984	522385.786334	38.768039
2322.906651	523384.015943	38.773056
2325.305403	524370.520540	38.778074
2327.139255	525368.892150	38.783092
2329.877934	526372.841538	38.788109
2331.892374	527381.678936	38.793127
2334.156094	528394.688620	38.798144
2336.787474	529401.274484	38.803162
2338.399983	530429.009422	38.808180
2340.657679	531469.457376	38.813197
2342.904473	532501.828762	38.818215
2345.456633	533521.843821	38.823232
2347.245033	534581.029786	38.828250
2349.449747	535657.386979	38.833268
2351.818375	536718.436887	38.838285
2353.724067	537772.892438	38.843303
2355.955291	538856.105352	38.848320
2358.206879	539943.712405	38.853338
2360.112164	541030.338219	38.858356
2362.589920	542125.743374	38.863373
2365.218401	543234.271500	38.868391
2367.367723	544343.747943	38.873408
2370.071679	545455.359897	38.878426
2371.959310	546565.660613	38.883444
2374.744788	547683.571580	38.888461
2377.161046	548793.859913	38.893479
2379.748603	549926.157984	38.898496
2382.138441	551061.513705	38.903514
2384.450339	552188.291659	38.908532
2387.042772	553313.372458	38.913549
2389.598655	554444.902052	38.918567
2392.109473	555560.511068	38.923584
2395.296119	556695.318448	38.928602
2397.302581	557837.060312	38.933620
2400.152962	558956.806167	38.938637
2403.065894	560066.498708	38.943655
2405.307351	561179.877741	38.948672
2407.879523	562314.361378	38.953690
2409.774076	563447.553474	38.958708
2412.301393	564562.460111	38.963725
2415.202866	565684.795122	38.968743
2417.443530	566805.736641	38.973760
2419.822794	567946.195138	38.978778
2422.117796	569074.917433	38.983796
2424.824715	570185.598181	38.988813
2427.173812	571314.718503	38.993831
2429.684492	572465.450713	38.998848
2432.049309	573593.564590	39.003866
2434.187143	574705.604300	39.008884
2436.868490	575823.580176	39.013901
2439.283122	576951.538234	39.018919
2441.497728	578079.528723	39.023936
2444.431339	579204.439372	39.028954
2446.666771	580354.600134	39.033972
2448.925806	581502.895065	39.038989
2451.520725	582626.750049	39.044007
2453.975864	583746.413073	39.049024
2456.665533	584878.373655	39.054042
2458.847934	585986.091890	39.059060
2461.890121	587073.560722	39.064077
2464.025663	588170.207377	39.069095
2466.526897	589268.349219	39.074112
2468.944729	590352.118056	39.079130
2471.130393	591442.795292	39.084148
2473.647737	592548.004417	39.089165
2476.216137	593657.363057	39.094183
2478.511736	594774.481006	39.099200
2480.881965	595873.944221	39.104218
2483.208492	596999.065325	39.109236
2485.616948	598119.757334	39.114253
2487.907701	599236.905603	39.119271
2490.188778	600366.521152	39.124288
2492.681080	601507.561896	39.129306
2494.787129	602656.767312	39.134324
2497.514778	603817.623780	39.139341
2500.070127	604981.245938	39.144359
2502.060785	606115.756912	39.149376
2504.708040	607293.447939	39.154394
2506.967207	608479.940996	39.159412
2509.821894	609650.497346	39.164429
2512.120781	610839.790536	39.169447
2514.396879	612029.362724	39.174464
2516.866264	613217.276522	39.179482
2519.215423	614430.047709	39.184500
2521.529456	615637.340954	39.189517
2524.422083	616843.907894	39.194535
2526.790090	618069.984186	39.199552
2529.587188	619297.454025	39.204570
2531.799224	620515.983782	39.209588
2534.591635	621739.731973	39.214605
2536.995552	622993.999868	39.219623
2539.360832	624244.381181	39.224640
2542.374792	625454.680499	39.229658
2544.831795	626697.117403	39.234676
2547.155133	627949.925803	39.239693
2549.703227	629207.397082	39.244711
2551.875605	630481.466880	39.249728
2554.906006	631724.525544	39.254746
2557.040753	632999.249152	39.259764
2559.649595	634275.488846	39.264781
2562.274891	635539.688239	39.269799
2564.203079	636843.838799	39.274816
2566.941179	638149.640154	39.279834
2569.133181	639436.152461	39.284852
2571.523579	640729.409481	39.289869
2574.064574	642045.483105	39.294887
2576.572667	643350.916954	39.299904
2579.581030	644664.982056	39.304922
2581.921798	645996.695458	39.309940
2584.799258	647318.969997	39.314957
2587.118111	648629.146838	39.319975
2589.768004	649953.957615	39.324992
2592.633818	651289.326939	39.330010
2594.994165	652610.445783	39.335028
2597.348663	653959.301330	39.340045
2600.213228	655303.505088	39.345063
2602.591728	656654.084445	39.350080
2605.533278	657986.352191	39.355098
2607.846599	659335.579315	39.360116
2610.391835	660690.758814	39.365133
2613.228551	662022.745489	39.370151
2615.619195	663373.843392	39.375168
2618.252049	664713.860412	39.380186
2620.837458	666080.978065	39.385204
2623.637189	667444.780831	39.390221
2626.489747	668792.655983	39.395239
2628.712171	670111.785290	39.400256
2631.460796	671430.496241	39.405274
2633.864639	672752.662596	39.410292
2636.508135	674067.343441	39.415309
2639.324903	675393.300081	39.420327
2641.608309	676711.848548	39.425344
2644.725830	678012.425154	39.430362
2647.356411	679349.337083	39.435380
2649.800958	680698.860814	39.440397
2652.093761	682016.806723	39.445415
2654.813929	683350.344357	39.450432
2656.974314	684710.906148	39.455450
2659.563127	686069.258446	39.460468
2661.659424	687443.283501	39.465485
2664.528431	688806.148810	39.470503
2666.661064	690202.593307	39.475520
2669.315398	691603.700489	39.480538
2671.576948	693027.039560	39.485556
2674.009530	694418.413835	39.490573
2677.009694	695823.123332	39.495591
2679.568066	697276.649838	39.500608
2682.316466	698715.820212	39.505626
2684.731094	700143.206568	39.510644
2687.146912	701597.733268	39.515661
2690.288778	703034.051527	39.520679
2692.858058	704492.782718	39.525696
2696.272923	705934.626675	39.530714
2699.358747	707409.387105	39.535732
2702.281036	708874.113475	39.540749
2705.651212	710308.696506	39.545767
2708.073200	711752.656230	39.550784
2711.124991	713193.545169	39.555802
2713.894159	714648.348125	39.560820
2716.411406	716100.518089	39.565837
2719.275536	717562.280874	39.570855
2722.111352	719030.574766	39.575872
2724.993974	720474.113548	39.580890
2727.507037	721936.757352	39.585908
2730.209001	723410.192888	39.590925
2733.193730	724857.458092	39.595943
2735.524739	726333.699996	39.600960
2738.451699	727806.119640	39.605978
2741.113789	729276.985156	39.610996
2743.719682	730750.067037	39.616013
2746.634332	732223.474901	39.621031
2749.297653	733698.139619	39.626048
2752.487749	735190.377762	39.631066
2755.542234	736672.190720	39.636084
2758.292924	738150.078497	39.641101
2761.077361	739632.575544	39.646119
2763.975453	741125.932853	39.651136
2766.331923	742573.259986	39.656154
2769.590786	744058.556816	39.661172
2772.029646	745543.611530	39.666189
2775.092641	747012.059132	39.671207
2777.861852	748508.878572	39.676224
2780.452547	750012.688152	39.681242
2783.397414	751495.498418	39.686260
2785.731520	752966.842125	39.691277
2788.620735	754456.488016	39.696295
2791.228158	755961.803847	39.701312
2793.983466	757480.492367	39.706330
2796.759041	758967.609911	39.711348
2799.284182	760479.636055	39.716365
2802.262121	761972.337849	39.721383
2804.706664	763463.751520	39.726400
2807.201015	764998.553327	39.731418
2810.336702	766500.815666	39.736436
2812.687927	767960.955593	39.741453
2815.549307	769455.589416	39.746471
2817.901243	770957.185528	39.751488
2820.781601	772445.022310	39.756506
2824.050659	773910.333549	39.761524
2826.204164	775395.485655	39.766541
2829.565143	776909.023060	39.771559
2831.557621	778416.187564	39.776576
2834.602915	779919.185491	39.781594
2837.398378	781424.516575	39.786612
2839.851079	782959.531817	39.791629
2842.858147	784490.940739	39.796647
2845.707091	786030.145665	39.801664
2848.358767	787576.558272	39.806682
2850.755672	789108.065553	39.811700
2854.002450	790662.196879	39.816717
2856.633928	792214.864804	39.821735
2859.224202	793801.014445	39.826752
2861.913206	795370.280333	39.831770
2864.622714	796956.142049	39.836788
2867.729229	798544.714414	39.841805
2870.529525	800146.637031	39.846823
2873.150821	801765.207089	39.851840
2876.231786	803369.816907	39.856858
2878.584843	804994.577815	39.861876
2881.620244	806614.734597	39.866893
2884.980382	808226.582210	39.871911
2887.509058	809876.960124	39.876928
2890.133209	811512.649791	39.881946
2893.314987	813150.004464	39.886964
2896.670445	814814.295393	39.891981
2899.702656	816461.817124	39.896999
2902.779619	818108.390900	39.902016
2905.317356	819753.672717	39.907034
2908.431571	821423.933187	39.912052
2911.111203	823102.044199	39.917069
2914.106560	824762.847821	39.922087
2917.359026	826447.285609	39.927104
2920.314797	828120.272902	39.932122
2923.422360	829783.254143	39.937140
2926.269479	831472.221350	39.942157
2929.539176	833145.236091	39.947175
2932.423706	834815.447752	39.952192
2935.642866	836475.677139	39.957210
2938.623719	838156.258223	39.962228
2941.117843	839856.971010	39.967245
2944.240267	841529.052157	39.972263
2947.473498	843204.714540	39.977280
2950.233172	844903.260267	39.982298
2953.358381	846575.424246	39.987316
2955.803773	848253.576410	39.992333
2958.872277	849951.976941	39.997351
2961.826563	851658.389412	40.002368
2964.876317	853335.276283	40.007386
2967.784011	855028.729263	40.012404
2970.483931	856749.617273	40.017421
2973.569009	858457.830818	40.022439
2976.303593	860147.386913	40.027456
2978.939739	861862.103076	40.032474
2982.100012	863594.192783	40.037492
2985.010537	865329.418597	40.042509
2987.793717	867040.036700	40.047527
2990.885115	868763.007412	40.052544
2993.613641	870499.494351	40.057562
2996.733552	872211.206038	40.062580
2999.533144	873962.753946	40.067597
3002.559838	875700.781977	40.072615
3005.539566	877418.959496	40.077632
3008.121377	879147.634429	40.082650
3011.215722	880854.059202	40.087668
3014.312547	882545.488710	40.092685
3016.895898	884234.968949	40.097703
3020.088654	885944.439109	40.102720
3022.741428	887667.887718	40.107738
3025.821136	889358.794812	40.112756
3028.797825	891101.928454	40.117773
3031.716642	892832.289696	40.122791
3035.042305	894549.715072	40.127808
3038.220715	896291.820414	40.132826
3041.396106	898011.991647	40.137844
3044.352522	899764.737323	40.142861
3047.273586	901507.793686	40.147879
3050.374506	903251.823824	40.152896
3053.162179	905008.557200	40.157914
3056.536264	906756.173082	40.162932
3059.243539	908517.306016	40.167949
3062.126297	910301.326192	40.172967
3065.040106	912093.038622	40.177984
3067.997062	913854.938111	40.183002
3071.350137	915664.358746	40.188020
3074.329826	917461.331877	40.193037
3077.484741	919267.002639	40.198055
3080.802429	921062.544002	40.203072
3083.577936	922853.934582	40.208090
3087.573867	924675.522948	40.213108
3090.640678	926489.456202	40.218125
3093.537607	928293.984782	40.223143
3096.589179	930115.996318	40.228160
3099.672510	931947.250528	40.233178
3102.902403	933772.486880	40.238196
3105.840832	935615.144550	40.243213
3109.208610	937444.741754	40.248231
3112.375453	939269.048146	40.253248
3115.029175	941101.892023	40.258266
3118.749213	942942.906223	40.263284
3121.964728	944782.684273	40.268301
3124.778703	946625.794467	40.273319
3128.411208	948472.125302	40.278336
3131.112159	950318.617102	40.283354
3134.526839	952149.915626	40.288372
3137.946436	954014.907174	40.293389
3140.868959	955869.856832	40.298407
3144.420707	957752.523023	40.303424
3147.012282	959660.008719	40.308442
3150.688023	961561.014792	40.313460
3153.682541	963470.400204	40.318477
3156.981402	965377.441653	40.323495
3160.387524	967272.406006	40.328512
3163.491524	969160.449108	40.333530
3166.430625	971071.422206	40.338548
3169.669158	972995.662945	40.343565
3172.736941	974902.899271	40.348583
3176.007670	976809.564901	40.353600
3178.957036	978731.244728	40.358618
3182.120878	980660.916151	40.363636
3185.228850	982587.217759	40.368653
3188.074792	984487.399696	40.373671
3191.510545	986404.081781	40.378688
3194.439001	988363.020330	40.383706
3197.397748	990298.322331	40.388724
3200.563608	992231.667789	40.393741
3203.636053	994179.147439	40.398759
3207.156701	996123.844748	40.403776
3209.652139	998067.947303	40.408794
3213.052371	1000013.176492	40.413812
3216.576864	1001960.338302	40.418829
3219.554600	1003880.232547	40.423847
3222.649540	1005784.418525	40.428864
3225.572619	1007704.089752	40.433882
3228.802102	1009597.366458	40.438900
3231.973290	1011521.514529	40.443917
3234.957537	1013445.908196	40.448935
3238.092975	1015366.907324	40.453952
3240.720572	1017308.923788	40.458970
3243.754797	1019246.524422	40.463988
3247.098300	1021185.340335	40.469005
3249.951219	1023159.351257	40.474023
3253.450976	1025134.493882	40.479040
3256.412311	1027099.460354	40.484058
3259.516231	1029065.645304	40.489076
3262.701714	1031069.852795	40.494093
3265.990446	1033068.496646	40.499111
3269.568078	1035077.185667	40.504128
3272.201894	1037121.772904	40.509146
3275.578831	1039120.064701	40.514164
3279.104305	1041147.402674	40.519181
3282.075649	1043188.547369	40.524199
3285.621005	1045231.351673	40.529216
3289.001019	1047266.015873	40.534234
3292.543203	1049321.468671	40.539252
3295.542281	1051388.275770	40.544269
3299.065986	1053443.739382	40.549287
3302.185279	1055512.350894	40.554304
3305.459413	1057607.651037	40.559322
3308.862733	1059663.028852	40.564340
3311.970401	1061733.439749	40.569357
3315.310582	1063835.964245	40.574375
3319.064673	1065915.926858	40.579392
3322.419557	1067993.920255	40.584410
3325.810878	1070089.820882	40.589428
3329.486738	1072184.010413	40.594445
3332.705648	1074296.255956	40.599463
3335.841447	1076378.579910	40.604480
3339.199360	1078481.809486	40.609498
3342.304690	1080586.184641	40.614516
3345.915698	1082705.259985	40.619533
3349.205123	1084828.728607	40.624551
3352.556566	1086930.708255	40.629568
3355.446232	1089051.733520	40.634586
3358.872021	1091200.023160	40.639604
3362.293106	1093327.600974	40.644621
3365.619647	1095477.745235	40.649639
3369.278478	1097614.863280	40.654656
3372.610470	1099737.551785	40.659674
3375.713835	1101884.613860	40.664692
3379.307944	1104033.028410	40.669709
3382.421609	1106179.141904	40.674727
3385.662488	1108338.568125	40.679744
3388.878550	1110507.412150	40.684762
3391.991739	1112659.603392	40.689780
3395.675661	1114812.264792	40.694797
3398.778546	1116997.338330	40.699815
3402.236863	1119161.790453	40.704832
3405.625603	1121344.187924	40.709850
3408.521318	1123536.031203	40.714868
3412.283834	1125736.703819	40.719885
3415.471537	1127924.419122	40.724903
3418.856936	1130104.091089	40.729920
3421.907141	1132300.369265	40.734938
3425.530657	1134499.910460	40.739956
3428.662984	1136712.546059	40.744973
3431.917844	1138927.079587	40.749991
3435.546615	1141148.860455	40.755008
3438.646514	1143327.605698	40.760013
3442.028769	1145474.095501	40.765018
3445.495829	1147563.501750	40.770023
3448.351566	1149576.111729	40.775028
3451.658357	1151516.856365	40.780032
3454.649805	1153402.222456	40.785037
3457.627875	1155197.205223	40.790042
3461.049090	1156933.323302	40.795047
3463.424728	1158583.453924	40.800052
3466.080373	1160138.855963	40.805056
3468.514629	1161646.103076	40.810061
3471.293724	1163064.984947	40.815066
3473.951018	1164400.184131	40.820071
3476.043426	1165659.864978	40.825076
3478.436149	1166850.265583	40.830080
3480.432370	1167989.106400	40.835085
3482.326488	1169044.754551	40.840090
3484.797467	1170034.417182	40.845095
3486.474751	1170994.114950	40.850100
3488.318653	1171859.278312	40.855104
3490.157380	1172676.103464	40.860109
3491.779813	1173429.747983	40.865114
3493.515954	1174138.948630	40.870119
3494.525211	1174793.019951	40.875124
3496.076781	1175391.962231	40.880128
3497.526954	1175963.140790	40.885133
3498.910840	1176458.586937	40.890138
3499.977028	1176917.944522	40.895143
3500.846461	1177352.134092	40.900148
3502.529982	1177743.092801	40.905152
3503.528414	1178092.019440	40.910157
3504.584395	1178407.373552	40.915162
3505.286704	1178695.352453	40.920167
3506.019238	1178928.390193	40.925172
3506.989834	1179131.234488	40.930176
3508.121031	1179303.242249	40.935181
3508.882504	1179465.320689	40.940186
3509.677158	1179581.705961	40.945191
3510.254695	1179694.921939	40.950196
3511.511264	1179777.695215	40.955200
3511.844480	1179823.038732	40.960205
3512.557864	1179826.877141	40.965210
3513.078102	1179839.600917	40.970215
3513.772825	1179829.220179	40.975220
3513.924928	1179786.434126	40.980224
3514.685215	1179738.178817	40.985229
3515.120268	1179663.886080	40.990234
3515.534284	1179569.815544	40.995239
3515.870920	1179471.046382	41.000244
3516.820716	1179360.588345	41.005248
3516.932469	1179223.325449	41.010253
3517.220124	1179069.639069	41.015258
3517.782509	1178884.156237	41.020263
3518.013470	1178721.236896	41.025268
3518.671613	1178535.820085	41.030272
3518.495301	1178338.097868	41.035277
3518.701177	1178137.667099	41.040282
3519.166133	1177893.844010	41.045287
3519.206746	1177689.465866	41.050292
3519.941480	1177463.198349	41.055296
3519.995657	1177207.537790	41.060301
3520.306253	1176932.786121	41.065306
3520.436997	1176670.961031	41.070311
3520.581783	1176402.900030	41.075316
3521.088373	1176129.016155	41.080320
3521.135778	1175832.288539	41.085325
3521.245368	1175536.476418	41.090330
3521.464193	1175240.252425	41.095335
3521.259865	1174948.323666	41.100340
3521.661010	1174619.414987	41.105344
3522.028685	1174296.431153	41.110349
3521.739916	1173990.885286	41.115354
3522.191688	1173652.289380	41.120359
3521.885095	1173341.710548	41.125364
3522.239925	1173010.727592	41.130368
3522.262605	1172679.212434	41.135373
3522.274832	1172331.171483	41.140378
3522.555552	1171987.590879	41.145383
3522.395821	1171649.342947	41.150388
3522.663055	1171302.983768	41.155392
3522.753397	1170940.874680	41.160397
3522.893255	1170580.241985	41.165402
3522.974257	1170213.649336	41.170407
3522.418503	1169857.233130	41.175412
3522.854832	1169471.090117	41.180416
3522.889052	1169119.150714	41.185421
3522.887865	1168754.168001	41.190426
3523.027221	1168386.776799	41.195431
3522.774910	1168027.637115	41.200436
3523.143102	1167650.905252	41.205440
3523.100640	1167273.269737	41.210445
3523.180936	1166888.788422	41.215450
3523.144923	1166515.440480	41.220455
3523.200068	1166144.222868	41.225460
3523.330602	1165738.873143	41.230464
3523.487305	1165366.450327	41.235469
3523.057635	1164964.816391	41.240474
3523.481009	1164578.030733	41.245479
3523.449827	1164191.480308	41.250484
3523.637627	1163804.959762	41.255488
3523.030597	1163416.085019	41.260493
3523.216786	1163027.428724	41.265498
3523.438381	1162630.894461	41.270503
3523.426304	1162245.803769	41.275508
3523.724050	1161825.097243	41.280512
3523.363305	1161427.906296	41.285517
3523.360810	1161043.009233	41.290522
3523.480922	1160647.570517	41.295527
3522.934095	1160240.394230	41.300532
3522.903200	1159829.224885	41.305536
3523.133052	1159441.430147	41.310541
3523.077974	1159063.960965	41.315546
3523.388143	1158656.142358	41.320551
3523.421828	1158273.967863	41.325556
3523.335202	1157871.071610	41.330560
3523.053096	1157457.393280	41.335565
3523.145513	1157040.498942	41.340570
3523.651110	1156642.235449	41.345575
3522.953959	1156258.521000	41.350580
3523.177868	1155843.118453	41.355584
3523.195420	1155423.931975	41.360589
3522.859965	1155020.479633	41.365594
3522.976154	1154631.970037	41.370599
3522.890280	1154224.345930	41.375604
3523.187314	1153809.622598	41.380608
3522.982540	1153414.450008	41.385613
3522.637568	1153025.424439	41.390618
3523.091459	1152619.196537	41.395623
3522.741081	1152232.480226	41.400628
3522.567673	1151844.380683	41.405632
3523.032627	1151427.927053	41.410637
3522.871164	1151022.056146	41.415642
3522.885497	1150615.272602	41.420647
3522.650837	1150229.432057	41.425652
3522.677916	1149818.701391	41.430656
3522.788112	1149395.798859	41.435661
3522.684963	1149005.205015	41.440666
3522.926645	1148614.525464	41.445671
3522.863777	1148199.514540	41.450676
3522.975994	1147777.145245	41.455680
3523.132351	1147363.738281	41.460685
3522.744850	1146973.135639	41.465690
3522.959242	1146558.423943	41.470695
3522.704321	1146155.890644	41.475700
3523.030884	1145742.518343	41.480704
3522.879903	1145328.623506	41.485709
3522.306673	1144921.308118	41.490714
3522.652771	1144502.525914	41.495719
3522.506369	1144105.887303	41.500724
3522.763948	1143693.409278	41.505728
3522.727472	1143281.895978	41.510733
3522.438862	1142865.364980	41.515738
3522.370935	1142459.009779	41.520743
3522.288255	1142062.586907	41.525748
3522.273421	1141649.994463	41.530752
3522.549018	1141256.962640	41.535757
3521.924007	1140852.283725	41.540762
3522.240276	1140431.950717	41.545767
3521.991814	1140049.069519	41.550772
3521.989328	1139644.575426	41.555776
3522.440040	1139242.823369	41.560781
3521.762967	1138859.831917	41.565786
3522.137192	1138445.501947	41.570791
3522.187368	1138035.750087	41.575796
3522.032925	1137628.753735	41.580800
3522.082467	1137238.594384	41.585805
3521.997561	1136838.362626	41.590810
3522.024119	1136416.999341	41.595815
3521.929609	1136013.667984	41.600820
3521.746093	1135622.288492	41.605824
3521.842290	1135233.683781	41.610829
3522.037190	1134821.380153	41.615834
3522.085673	1134411.253747	41.620839
3521.880656	1134025.650424	41.625844
3521.737590	1133631.172211	41.630848
3522.017726	1133230.608418	41.635853
3521.708090	1132817.852345	41.640858
3521.559127	1132402.566717	41.645863
3521.463527	1132015.278897	41.650868
3521.514077	1131598.757090	41.655872
3521.823341	1131225.318122	41.660877
3521.409584	1130837.616733	41.665882
3521.615042	1130421.737846	41.670887
3521.029795	1130018.317497	41.675892
3521.399424	1129621.080351	41.680896
3521.559685	1129229.553893	41.685901
3521.220333	1128842.550831	41.690906
3521.056133	1128448.072154	41.695911
3521.346044	1128045.119095	41.700916
3521.048480	1127655.930365	41.705920
3521.103687	1127267.986968	41.710925
3520.682482	1126867.725728	41.715930
3521.198958	1126466.994575	41.720935
3520.879391	1126096.439430	41.725940
3520.674680	1125703.857725	41.730944
3520.862635	1125306.328951	41.735949
3521.017245	1124929.904676	41.740954
3520.787951	1124528.484571	41.745959
3520.931530	1124124.973923	41.750964
3520.430768	1123745.242477	41.755968
3520.653404	1123376.884272	41.760973
3520.376546	1122967.452930	41.765978
3520.734194	1122581.499231	41.770983
3520.419148	1122211.625802	41.775988
3520.816167	1121820.278219	41.780992
3520.655064	1121427.660610	41.785997
3520.379565	1121030.556581	41.791002
3520.459129	1120649.842861	41.796007
3520.268860	1120257.620405	41.801012
3520.503941	1119882.827682	41.806016
3520.506687	1119518.812512	41.811021
3520.139798	1119124.535416	41.816026
3520.361597	1118741.756977	41.821031
3520.289995	1118372.721352	41.826036
3520.107722	1117973.945749	41.831040
3520.444898	1117564.094854	41.836045
3520.060376	1117193.599947	41.841050
3520.310479	1116837.558547	41.846055
3520.014637	1116446.122707	41.851060
3519.980673	1116034.118783	41.856064
3520.226701	1115659.410016	41.861069
3519.790219	1115299.661339	41.866074
3519.896180	1114919.489267	41.871079
3519.579144	1114550.040079	41.876084
3519.856280	1114179.513941	41.881088
3519.829782	1113784.310914	41.886093
3519.806593	1113421.030152	41.891098
3520.004230	1113057.211513	41.896103
3519.937218	1112662.600276	41.901108
3519.531462	1112277.555723	41.906112
3519.797816	1111905.061813	41.911117
3519.659168	1111530.414302	41.916122
3520.194911	1111137.404582	41.921127
3519.421017	1110773.782120	41.926132
3519.544089	1110410.178186	41.931136
3519.727463	1110029.074463	41.936141
3519.384411	1109669.314746	41.941146
3519.371710	1109285.899964	41.946151
3519.209304	1108908.687324	41.951156
3519.196277	1108529.036997	41.956160
3519.371604	1108166.991180	41.961165
3518.886555	1107796.532199	41.966170
3519.485197	1107424.245995	41.971175
3519.312348	1107075.933964	41.976180
3519.308286	1106698.062840	41.981184
3519.104238	1106314.658871	41.986189
3519.013980	1105942.861256	41.991194
3518.849547	1105588.338901	41.996199
3518.794748	1105217.727136	42.001204
3518.973462	1104840.746398	42.006208
3518.956701	1104496.827360	42.011213
3519.049576	1104130.606766	42.016218
3518.887239	1103768.989726	42.021223
3518.875879	1103421.465870	42.026228
3518.988691	1103036.152015	42.031232
3518.609323	1102659.206249	42.036237
3518.273882	1102311.473123	42.041242
3518.418988	1101958.285864	42.046247
3518.663734	1101595.978213	42.051252
3518.235999	1101226.300614	42.056256
3518.574245	1100864.502058	42.061261
3518.382995	1100526.763934	42.066266
3518.394597	1100180.079251	42.071271
3518.239003	1099818.387581	42.076276
3518.098392	1099465.371201	42.081280
3517.939844	1099113.386669	42.086285
3518.111068	1098764.098417	42.091290
3517.912070	1098397.249947	42.096295
3518.025749	1098048.211866	42.101300
3518.320219	1097688.025238	42.106304
3518.244402	1097351.887171	42.111309
3517.969402	1097012.603933	42.116314
3518.074940	1096646.160553	42.121319
3518.021523	1096280.005588	42.126324
3518.195366	1095938.189009	42.131328
3517.850914	1095595.957739	42.136333
3517.740658	1095239.119775	42.141338
3517.952612	1094887.277701	42.146343
3517.858498	1094546.183043	42.151348
3517.785554	1094200.468909	42.156352
3517.631523	1093869.104824	42.161357
3517.260446	1093501.857066	42.166362
3517.728620	1093162.497327	42.171367
3517.310625	1092830.060073	42.176372
3517.111453	1092475.256796	42.181376
3517.324248	1092143.056529	42.186381
3517.417531	1091811.525930	42.191386
3517.249752	1091473.218598	42.196391
3517.055088	1091136.426966	42.201396
3517.024353	1090809.452667	42.206400
3517.366139	1090457.972166	42.211405
3517.177060	1090114.028059	42.216410
3517.216988	1089787.842706	42.221415
3517.180268	1089444.118459	42.226420
3517.131668	1089098.458231	42.231424
3516.784518	1088789.426459	42.236429
3516.833281	1088444.954198	42.241434
3516.985941	1088089.806213	42.246439
3516.930316	1087780.285716	42.251444
3516.695476	1087466.464404	42.256448
3516.682014	1087109.075423	42.261453
3516.851972	1086791.123000	42.266458
3516.891403	1086460.137136	42.271463
3516.646462	1086145.282665	42.276468
3516.298212	1085808.185852	42.281472
3516.467755	1085477.789851	42.286477
3516.444624	1085166.101849	42.291482
3516.549020	1084821.007285	42.296487
3516.142531	1084492.084577	42.301492
3515.900237	1084180.088528	42.306496
3516.293845	1083859.242843	42.311501
3515.972602	1083534.180170	42.316506
3515.983652	1083228.225909	42.321511
3515.860472	1082924.003092	42.326516
3516.053349	1082599.759155	42.331520
3516.291698	1082278.845964	42.336525
3516.162958	1081965.073514	42.341530
3516.217199	1081649.238116	42.346535
3515.940252	1081330.272748	42.351540
3515.693788	1081013.490579	42.356544
3516.243211	1080697.422540	42.361549
3516.112194	1080379.912853	42.366554
3515.855328	1080066.148170	42.371559
3515.922440	1079756.630894	42.376564
3515.762301	1079425.730107	42.381568
3515.830850	1079133.645494	42.386573
3515.698567	1078819.692620	42.391578
3516.110998	1078486.336815	42.396583
3516.044893	1078176.367876	42.401588
3515.964169	1077882.992913	42.406592
3515.658067	1077555.266988	42.411597
3515.224873	1077247.226004	42.416602
3515.729430	1076938.341039	42.421607
3515.405049	1076616.419201	42.426612
3515.389870	1076297.596606	42.431616
3515.418059	1075995.747335	42.436621
3515.530456	1075698.669778	42.441626
3515.317356	1075370.893533	42.446631
3515.279476	1075084.180807	42.451636
3515.379567	1074776.008719	42.456640
3515.210303	1074469.400695	42.461645
3514.991718	1074167.587200	42.466650
3515.103810	1073860.514420	42.471655
3515.361196	1073569.254097	42.476660
3515.206048	1073248.451186	42.481664
3515.141187	1072951.637960	42.486669
3514.782360	1072672.443039	42.491674
3514.783021	1072361.652782	42.496679
3514.964551	1072057.542726	42.501684
3514.776042	1071765.394883	42.506688
3514.984381	1071469.032969	42.511693
3514.952870	1071167.119305	42.516698
3514.806558	1070887.509989	42.521703
3514.792083	1070598.347379	42.526708
3514.759428	1070277.254064	42.531712
3515.075753	1069976.755769	42.536717
3514.924039	1069696.509700	42.541722
3514.859498	1069405.754012	42.546727
3514.921558	1069097.364647	42.551732
3514.567671	1068794.027088	42.556736
3514.619268	1068498.876708	42.561741
3514.359865	1068219.053712	42.566746
3514.679826	1067925.463282	42.571751
3514.724741	1067631.613886	42.576756
3514.633624	1067348.448429	42.581760
3514.940399	1067045.097731	42.586765
3514.348374	1066737.549203	42.591770
3514.690185	1066446.473530	42.596775
3514.676349	1066157.653890	42.601780
3514.445078	1065866.256999	42.606784
3514.546692	1065579.312280	42.611789
3514.387185	1065303.365506	42.616794
3514.306255	1064998.233502	42.621799
3514.359944	1064700.568942	42.626804
3514.448986	1064428.098074	42.631808
3514.189701	1064133.726607	42.636813
3514.071539	1063851.347739	42.641818
3514.239070	1063584.789812	42.646823
3514.023640	1063305.671687	42.651828
3513.976763	1063014.959555	42.656832
3513.887584	1062719.714213	42.661837
3513.747587	1062434.474267	42.666842
3513.604535	1062166.935996	42.671847
3513.727323	1061895.296879	42.676852
3513.577997	1061626.481630	42.681856
3513.978148	1061345.044206	42.686861
3513.859074	1061059.151736	42.691866
3513.797933	1060792.014637	42.696871
3513.773624	1060505.018412	42.701876
3513.566454	1060221.889998	42.706880
3513.614081	1059954.983323	42.711885
3513.286074	1059670.305313	42.716890
3513.653004	1059408.810163	42.721895
3513.568623	1059132.444980	42.726900
3513.524363	1058853.458141	42.731904
3513.468229	1058587.562048	42.736909
3513.293649	1058326.297408	42.741914
3513.176532	1058041.693204	42.746919
3513.279035	1057779.875258	42.751924
3513.152515	1057514.420783	42.756928
3513.389896	1057239.738605	42.761933
3513.059348	1056969.376703	42.766938
3513.410547	1056709.490818	42.771943
3512.984988	1056449.431475	42.776948
3513.299551	1056173.816070	42.781952
3513.780762	1055889.484185	42.786957
3513.421158	1055622.627561	42.791962
3513.356245	1055370.362475	42.796967
3513.194304	1055097.471030	42.801972
3513.033218	1054832.760848	42.806977
3513.405355	1054554.548441	42.811981
3512.907257	1054291.988970	42.816986
3512.757729	1054010.749646	42.821991
3512.737003	1053772.578700	42.826996
3512.976833	1053513.139247	42.832001
3513.095930	1053236.637942	42.837005
3512.640413	1052966.100467	42.842010
3512.834499	1052718.783063	42.847015
3512.635272	1052466.118074	42.852020
3512.550499	1052203.101864	42.857025
3512.917276	1051951.959914	42.862029
3512.775069	1051704.073737	42.867034
3512.941530	1051431.622332	42.872039
3512.842204	1051166.147444	42.877044
3512.637656	1050909.456730	42.882049
3512.646320	1050655.517004	42.887053
3512.717662	1050404.642907	42.892058
3513.024629	1050148.701039	42.897063
3513.028510	1049903.315378	42.902068
3512.659679	1049627.582404	42.907073
3512.779745	1049359.089626	42.912077
3512.461242	1049111.019763	42.917082
3512.493607	1048845.025763	42.922087
3512.643140	1048597.241853	42.927092
3512.380737	1048350.769508	42.932097
3512.406788	1048087.153232	42.937101
3512.553486	1047840.397740	42.942106
3512.381178	1047585.188559	42.947111
3512.538371	1047329.720269	42.952116
3512.551375	1047073.781222	42.957121
3512.501850	1046829.909418	42.962125
3512.130548	1046580.479728	42.967130
3512.320419	1046332.684442	42.972135
3512.389382	1046080.842347	42.977140
3512.105745	1045816.879372	42.982145
3512.504702	1045555.205713	42.987149
3511.891017	1045324.687550	42.992154
3511.939853	1045071.644019	42.997159
3512.270940	1044821.633180	43.002164
3512.043993	1044593.338957	43.007169
3512.001244	1044348.680768	43.012173
3511.705881	1044110.332228	43.017178
3511.998225	1043859.221840	43.022183
3512.082992	1043612.191736	43.027188
3511.740749	1043361.549772	43.032193
3512.031349	1043115.043309	43.037197
3511.569830	1042883.045986	43.042202
3511.925702	1042649.068511	43.047207
3511.817482	1042410.809405	43.052212
3511.813868	1042164.695722	43.057217
3511.853408	1041912.669257	43.062221
3511.692038	1041687.626945	43.067226
3511.671680	1041429.306843	43.072231
3511.700348	1041213.685140	43.077236
3511.601092	1040974.589768	43.082241
3511.749188	1040725.391128	43.087245
3511.607148	1040490.341531	43.092250
3511.321142	1040250.569144	43.097255
3511.752882	1040009.798185	43.102260
3511.396013	1039774.463692	43.107265
3511.362268	1039554.727654	43.112269
3511.099996	1039336.180736	43.117274
3511.390385	1039098.487381	43.122279
3511.423013	1038846.806447	43.127284
3511.224725	1038629.671562	43.132289
3511.303416	1038401.652566	43.137293
3511.125275	1038159.548217	43.142298
3511.147901	1037922.042109	43.147303
3511.287457	1037701.140554	43.152308
3511.192657	1037483.073497	43.157313
3511.260793	1037240.985340	43.162317
3510.838915	1037025.081978	43.167322
3511.297343	1036806.607149	43.172327
3511.082024	1036564.632992	43.177332
3510.882187	1036338.413190	43.182337
3510.938178	1036101.984729	43.187341
3510.667198	1035882.916646	43.192346
3510.749919	1035655.655172	43.197351
3511.021377	1035444.026549	43.202356
3510.955851	1035207.096385	43.207361
3511.029364	1035000.321122	43.212365
3510.934992	1034793.372319	43.217370
3510.754572	1034554.401381	43.222375
3510.944498	1034321.552326	43.227380
3510.703635	1034130.376117	43.232385
3511.043665	1033899.807231	43.237389
3510.631665	1033652.609905	43.242394
3510.852701	1033430.460992	43.247399
3510.890917	1033217.044154	43.252404
3510.754373	1033014.198075	43.257409
3510.874245	1032783.909695	43.262413
3510.596718	1032573.133665	43.267418
3510.643477	1032334.030144	43.272423
3510.358406	1032114.429035	43.277428
3510.693234	1031918.532305	43.282433
3510.676059	1031702.452803	43.287437
3510.413204	1031475.658733	43.292442
3510.180446	1031272.862005	43.297447
3510.360012	1031062.244079	43.302452
3510.337772	1030838.482861	43.307457
3510.577932	1030611.861336	43.312461
3510.364942	1030415.711612	43.317466
3510.202406	1030198.338976	43.322471
3510.413105	1029985.641704	43.327476
3509.912374	1029789.904759	43.332481
3510.461002	1029587.014955	43.337485
3510.189458	1029369.143756	43.342490
3510.018075	1029153.087848	43.347495
3510.024984	1028937.769109	43.352500
3510.257664	1028729.669735	43.357505
3510.163638	1028513.382627	43.362509
3510.073325	1028315.976547	43.367514
3509.960545	1028124.185949	43.372519
3510.234129	1027912.271290	43.377524
3509.970614	1027722.429309	43.382529
3509.966309	1027513.645535	43.387533
3509.652884	1027297.153736	43.392538
3509.582382	1027080.516653	43.397543
3509.765507	1026904.041449	43.402548
3509.829358	1026687.076315	43.407553
3509.843155	1026481.254920	43.412557
3509.490156	1026298.259469	43.417562
3509.685384	1026108.674780	43.422567
3509.627918	1025914.764192	43.427572
3509.663659	1025722.091451	43.432577
3509.524381	1025506.083149	43.437581
3509.396740	1025311.000157	43.442586
3509.512194	1025116.161111	43.447591
3509.520260	1024903.013084	43.452596
3509.628397	1024709.130389	43.457601
3509.809226	1024518.815698	43.462605
3509.774475	1024343.749720	43.467610
3509.677788	1024142.610611	43.472615
3509.764441	1023945.990610	43.477620
3509.046794	1023739.122435	43.482625
3509.339154	1023525.875176	43.487629
3509.141214	1023343.533213	43.492634
3509.017571	1023163.306218	43.497639
3509.278735	1022967.592750	43.502644
3509.044531	1022788.244581	43.507649
3509.021956	1022600.613319	43.512653
3509.224451	1022414.393316	43.517658
3509.299017	1022219.751188	43.522663
3509.275314	1022050.818283	43.527668
3509.294970	1021858.015264	43.532673
3509.005273	1021659.825303	43.537677
3509.015681	1021472.538804	43.542682
3509.368048	1021276.848296	43.547687
3509.262113	1021096.260945	43.552692
3508.808628	1020910.002030	43.557697
3508.840327	1020745.676676	43.562701
3508.836306	1020545.945257	43.567706
3508.916514	1020375.101645	43.572711
3508.809085	1020209.522384	43.577716
3508.881326	1020011.214552	43.582721
3508.959355	1019813.286837	43.587725
3508.637531	1019656.264211	43.592730
3508.650053	1019490.935058	43.597735
3508.767305	1019299.580425	43.602740
3508.728644	1019110.185569	43.607745
3509.073755	1018924.505452	43.612749
3508.661685	1018737.585381	43.617754
3508.811811	1018564.055126	43.622759
3508.863096	1018403.054374	43.627764
3508.536413	1018240.655568	43.632769
3508.625331	1018042.566593	43.637773
3508.657910	1017872.334008	43.642778
3508.680062	1017677.057661	43.647783
3508.467612	1017504.622008	43.652788
3508.247087	1017343.441536	43.657793
3508.721990	1017165.640952	43.662797
3508.696793	1016982.966662	43.667802
3508.504545	1016813.903853	43.672807
3508.752510	1016632.629248	43.677812
3508.420625	1016460.472443	43.682817
3508.258853	1016286.729071	43.687821
3507.955064	1016125.915707	43.692826
3507.966170	1015960.774125	43.697831
3508.411641	1015766.138346	43.702836
3508.146533	1015612.391395	43.707841
3507.907671	1015461.354549	43.712845
3508.234366	1015284.295647	43.717850
3508.646408	1015118.092320	43.722855
3508.221956	1014957.459608	43.727860
3508.052114	1014781.243477	43.732865
3508.072775	1014608.486364	43.737869
3507.999808	1014455.064561	43.742874
3508.064091	1014311.618704	43.747879
3508.175101	1014124.167635	43.752884
3507.934079	1013957.454889	43.757889
3508.158107	1013791.534716	43.762893
3507.825598	1013634.054116	43.767898
3508.133859	1013465.973714	43.772903
3507.819711	1013294.396945	43.777908
3507.873113	1013131.496495	43.782913
3508.043987	1012967.697752	43.787917
3508.094032	1012819.359361	43.792922
3507.917090	1012652.597410	43.797927
3508.069385	1012496.365128	43.802932
3507.652337	1012345.759706	43.807937
3507.793534	1012182.817355	43.812941
3507.829886	1012017.653032	43.817946
3507.653035	1011859.902852	43.822951
3507.738809	1011695.983989	43.827956
3507.712068	1011534.605094	43.832961
3507.749040	1011362.620142	43.837965
3507.640447	1011224.953998	43.842970
3507.422581	1011076.419498	43.847975
3507.828607	1010915.728962	43.852980
3507.331134	1010773.937431	43.857985
3507.611862	1010605.095986	43.862989
3507.510154	1010466.146860	43.867994
3507.552424	1010308.025601	43.872999
3507.486944	1010159.927762	43.878004
3507.716246	1010002.350240	43.883009
3507.515128	1009848.046503	43.888013
3507.590434	1009721.879053	43.893018
3507.539087	1009546.159891	43.898023
3507.446409	1009379.481564	43.903028
3507.369676	1009236.998871	43.908033
3507.318621	1009069.332510	43.913037
3507.146785	1008930.454292	43.918042
3507.216017	1008787.352961	43.923047
3507.392544	1008648.313213	43.928052
3506.997150	1008507.711599	43.933057
3507.375268	1008346.174749	43.938061
3507.096827	1008204.476931	43.943066
3507.168765	1008040.940172	43.948071
3507.344392	1007904.896139	43.953076
3506.973128	1007769.230580	43.958081
3507.296883	1007626.349571	43.963085
3507.582621	1007471.803411	43.968090
3507.100103	1007323.699787	43.973095
3507.115796	1007173.176534	43.978100
3506.759678	1007019.793319	43.983105
3506.888089	1006862.825415	43.988109
3506.921563	1006741.557565	43.993114
3506.779164	1006598.921826	43.998119
3507.238846	1006460.170539	44.003124
3506.959429	1006335.639034	44.008129
3506.965114	1006185.577362	44.013133
3507.219281	1006030.510696	44.018138
3507.172189	1005891.148108	44.023143
3507.115303	1005750.616559	44.028148
3506.985875	1005610.871572	44.033153
3507.185301	1005477.974862	44.038157
3506.963991	1005343.490759	44.043162
3506.956966	1005197.003853	44.048167
3507.081082	1005032.495936	44.053172
3506.643766	1004909.028990	44.058177
3507.137388	1004790.075362	44.063181
3506.886124	1004644.781703	44.068186
3506.607720	1004492.581686	44.073191
3506.911137	1004339.017031	44.078196
3506.724641	1004206.348558	44.083201
3507.005221	1004052.098858	44.088205
3506.652998	1003937.255519	44.093210
3506.521640	1003810.892698	44.098215
3507.030813	1003667.394569	44.103220
3506.828125	1003528.875027	44.108225
3506.796483	1003382.442453	44.113229
3506.729270	1003251.677974	44.118234
3506.517509	1003112.857822	44.123239
3506.997437	1002966.622150	44.128244
3506.873409	1002863.785760	44.133249
3506.804222	1002710.530197	44.138253
3506.481797	1002585.825804	44.143258
3506.699333	1002451.297923	44.148263
3506.893856	1002320.274171	44.153268
3506.636704	1002188.153905	44.158273
3507.026882	1002031.203347	44.163277
3506.541547	1001889.673123	44.168282
3506.036622	1001777.828230	44.173287
3506.372835	1001654.941433	44.178292
3506.304142	1001510.413143	44.183297
3506.691047	1001389.458925	44.188301
3506.473086	1001255.461034	44.193306
3506.580770	1001112.256273	44.198311
3506.520434	1000987.084109	44.203316
3506.444905	1000849.646136	44.208321
3506.714620	1000735.706146	44.213325
3506.388073	1000598.303415	44.218330
3506.387970	1000461.914459	44.223335
3506.403616	1000331.068840	44.228340
3506.411933	1000210.346509	44.233345
3506.509941	1000074.613566	44.238349
3506.183934	999949.462221	44.243354
3506.162956	999825.426232	44.248359
3506.403291	999696.865677	44.253364
3506.308002	999562.904889	44.258369
3506.322051	999433.499320	44.263373
3506.424278	999337.766972	44.268378
3506.516189	999210.290915	44.273383
3506.695508	999067.996416	44.278388
3506.502163	998952.246682	44.283393
3506.482795	998822.832673	44.288397
3506.508949	998672.470883	44.293402
3506.144473	998537.653744	44.298407
3506.048471	998419.150295	44.303412
3506.046742	998292.740287	44.308417
3506.041194	998165.256780	44.313421
3506.196893	998053.521658	44.318426
3506.261775	997934.981591	44.323431
3506.048404	997812.004575	44.328436
3505.706254	997706.091073	44.333441
3505.935780	997563.847954	44.338445
3505.824469	997442.404545	44.343450
3505.854571	997338.663167	44.348455
3505.956748	997219.809792	44.353460
3505.972181	997098.435551	44.358465
3505.931869	996987.685817	44.363469
3505.734809	996868.095061	44.368474
3505.827127	996757.318986	44.373479
3505.881190	996625.115070	44.378484
3506.039245	996499.028438	44.383489
3505.720548	996375.550512	44.388493
3505.731321	996288.354922	44.393498
3505.936189	996170.729172	44.398503
3506.020167	996026.522966	44.403508
3505.858984	995917.915685	44.408513
3505.814459	995806.364143	44.413517
3505.794122	995709.129239	44.418522
3505.906279	995583.322127	44.423527
3505.706554	995443.922215	44.428532
3505.814443	995345.490701	44.433537
3505.710319	995228.188635	44.438541
3505.690697	995113.208890	44.443546
3505.500569	995005.660804	44.448551
3505.973365	994884.261325	44.453556
3505.394070	994769.464243	44.458561
3505.550822	994667.894532	44.463565
3505.714338	994575.677429	44.468570
3505.688726	994453.766119	44.473575
3505.924548	994331.711676	44.478580
3505.656202	994221.140424	44.483585
3505.577370	994104.395733	44.488589
3505.577841	994000.793142	44.493594
3505.481281	993894.573085	44.498599
3505.572574	993782.082214	44.503604
3505.106788	993677.283442	44.508609
3505.292439	993555.123112	44.513613
3505.306888	993463.009972	44.518618
3505.202006	993355.026691	44.523623
3505.562628	993247.744499	44.528628
3505.299515	993136.761366	44.533633
3505.409862	993030.686036	44.538637
3505.702629	992925.261054	44.543642
3505.382379	992809.699299	44.548647
3505.758879	992714.297432	44.553652
3505.275632	992619.620488	44.558657
3505.307910	992498.535068	44.563661
3505.311814	992390.710524	44.568666
3505.505682	992294.649261	44.573671
3505.416941	992172.991885	44.578676
3505.240586	992064.508380	44.583681
3505.397341	991955.090456	44.588685
3505.842388	991848.937954	44.593690
3505.525050	991728.966231	44.598695
3505.372620	991627.685613	44.603700
3505.065968	991528.768729	44.608705
3505.365475	991408.883668	44.613709
3505.255588	991330.700045	44.618714
3505.090961	991230.584472	44.623719
3505.174448	991107.705806	44.628724
3505.196695	991030.568937	44.633729
3505.259723	990902.423436	44.638733
3505.518864	990800.572721	44.643738
3505.564896	990709.287425	44.648743
3505.439428	990606.033776	44.653748
3504.965144	990500.397620	44.658753
3505.254471	990395.608986	44.663757
3505.198986	990292.825751	44.668762
3505.092188	990179.906123	44.673767
3505.070089	990084.038161	44.678772
3505.269914	989981.889974	44.683777
3505.223363	989879.292864	44.688781
3505.285081	989801.157488	44.693786
3505.260324	989702.455012	44.698791
3505.254423	989578.777758	44.703796
3505.142087	989463.796511	44.708801
3505.228952	989364.874715	44.713805
3505.173895	989263.731051	44.718810
3505.116859	989163.951564	44.723815
3505.084993	989071.774917	44.728820
3505.123374	988976.073428	44.733825
3504.858890	988876.323066	44.738829
3505.014180	988775.331184	44.743834
3505.061200	988696.597754	44.748839
3505.236505	988567.893428	44.753844
3505.040639	988473.295191	44.758849
3504.928354	988369.998798	44.763853
3505.091930	988261.679454	44.768858
3504.789433	988181.630606	44.773863
3504.809884	988093.819847	44.778868
3504.886099	987983.265612	44.783873
3504.870345	987902.287512	44.788877
3504.856165	987792.134727	44.793882
3504.808827	987706.085412	44.798887
3504.983950	987605.752529	44.803892
3504.832912	987527.523424	44.808897
3504.862032	987429.845995	44.813901
3504.893536	987328.556127	44.818906
3504.773394	987247.293177	44.823911
3505.098717	987153.953292	44.828916
3505.040242	987047.208724	44.833921
3505.360457	986953.768822	44.838925
3504.770211	986856.573913	44.843930
3505.040084	986766.554734	44.848935
3505.211924	986660.740868	44.853940
3504.568663	986550.765284	44.858945
3504.881070	986470.786293	44.863949
3505.202167	986374.701764	44.868954
3504.606512	986298.773676	44.873959
3505.216753	986189.951010	44.878964
3504.972478	986086.049360	44.883969
3504.925575	985971.572420	44.888973
3504.946559	985880.994650	44.893978
3504.910951	985787.301434	44.898983
3504.825078	985709.329445	44.903988
3504.491004	985624.857615	44.908993
3504.607675	985519.324475	44.913997
3504.745411	985443.947462	44.919002
3504.578842	985371.938352	44.924007
3504.444678	985273.372363	44.929012
3504.582721	985174.662223	44.934017
3504.290066	985085.587693	44.939021
3504.875291	984987.874449	44.944026
3504.657322	984901.615658	44.949031
3504.774522	984813.250326	44.954036
3504.329985	984737.374153	44.959041
3504.275214	984649.522718	44.964045
3504.386666	984563.985553	44.969050
3504.101278	984489.056113	44.974055
3504.526736	984406.686540	44.979060
3504.412530	984316.106184	44.984065
3504.467048	984210.656704	44.989069
3504.384526	984147.209811	44.994074
3504.221647	984063.077170	44.999079
3504.382861	983980.549705	45.004084
3504.579664	983875.461138	45.009089
3504.332965	983798.758795	45.014093
3504.290751	983727.489544	45.019098
3504.192571	983652.811202	45.024103
3504.608418	983544.165399	45.029108
3504.406876	983458.175001	45.034113
3504.358033	983381.922686	45.039117
3504.324510	983300.100976	45.044122
3504.026010	983228.379470	45.049127
3504.179964	983145.743487	45.054132
3504.221717	983061.269425	45.059137
3504.377028	982977.556628	45.064141
3504.207594	982906.298077	45.069146
3504.243720	982821.528436	45.074151
3504.483127	982716.899804	45.079156
3504.248358	982646.625339	45.084161
3504.432638	982582.726479	45.089165
3504.372863	982485.467295	45.094170
3504.035227	982411.300451	45.099175
3503.911707	982339.734280	45.104180
3504.094972	982265.284420	45.109185
3504.197384	982195.730184	45.114189
3504.267617	982114.167387	45.119194
3504.365677	982017.557908	45.124199
3504.242570	981945.693726	45.129204
3504.028290	981854.504765	45.134209
3504.166452	981763.451647	45.139213
3504.476318	981705.284989	45.144218
3503.965093	981618.731841	45.149223
3504.160187	981527.665589	45.154228
3503.785969	981463.846203	45.159233
3504.017050	981399.926409	45.164237
3504.293064	981313.336652	45.169242
3503.864948	981225.005595	45.174247
3504.107432	981148.382427	45.179252
3504.133122	981085.958202	45.184257
3504.052831	981006.065014	45.189261
3504.053324	980907.987557	45.194266
3503.515177	980841.648338	45.199271
3503.972998	980763.812286	45.204276
3504.195505	980711.902068	45.209281
3503.830854	980641.428930	45.214285
3504.082809	980574.956483	45.219290
3503.864237	980496.153566	45.224295
3503.916240	980392.880973	45.229300
3503.960817	980336.795713	45.234305
3503.717361	980277.728696	45.239309
3503.965606	980199.235593	45.244314
3503.779152	980133.514119	45.249319
3503.982009	980035.583765	45.254324
3504.037546	979991.315291	45.259329
3503.928030	979913.561113	45.264333
3504.035842	979828.637554	45.269338
3503.639585	979757.377067	45.274343
3504.034694	979673.283248	45.279348
3503.700419	979605.137328	45.284353
3503.977510	979542.068581	45.289357
3503.779350	979485.917243	45.294362
3503.614486	979409.044725	45.299367
3504.090978	979334.606117	45.304372
3503.688380	979271.646334	45.309377
3503.734749	979190.632039	45.314381
3503.972938	979103.526470	45.319386
3503.808053	979047.267625	45.324391
3503.826212	978962.932295	45.329396
3503.698922	978910.477019	45.334401
3503.410574	978836.451068	45.339405
3503.994176	978750.651359	45.344410
3503.375916	978682.541210	45.349415
3503.754202	978625.895582	45.354420
3503.454815	978562.715536	45.359425
3503.339710	978486.897429	45.364429
3504.081857	978427.453502	45.369434
3503.611982	978360.585565	45.374439
3503.792896	978291.655016	45.379444
3503.409105	978248.227267	45.384449
3503.615966	978170.690482	45.389453
3503.899699	978090.696595	45.394458
3503.552695	978034.653254	45.399463
3503.820235	977966.779629	45.404468
3503.616348	977909.831852	45.409473
3503.598716	977845.424611	45.414477
3503.532473	977765.483822	45.419482
3503.458815	977698.738367	45.424487
3503.972582	977637.075787	45.429492
3503.915065	977564.168269	45.434497
3503.689451	977498.325207	45.439501
3503.916351	977420.481726	45.444506
3503.602516	977363.839864	45.449511
3503.565479	977298.452183	45.454516
3503.678238	977229.226821	45.459521
3503.664390	977155.818157	45.464525
3503.656255	977093.355921	45.469530
3503.569103	977039.215078	45.474535
3503.079447	976959.528275	45.479540
3503.497737	976887.022541	45.484545
3503.462058	976831.991455	45.489549
3503.460955	976756.913706	45.494554
3502.961036	976702.251108	45.499559
3503.516881	976642.819367	45.504564
3503.286304	976582.538922	45.509569
3503.117595	976510.516148	45.514573
3503.281727	976456.230643	45.519578
3503.391554	976410.068013	45.524583
3503.399808	976358.055830	45.529588
3503.597429	976276.877611	45.534593
3503.409940	976217.954961	45.539597
3503.497091	976162.701678	45.544602
3503.218674	976106.628146	45.549607
3503.500483	976053.394908	45.554612
3503.323180	975984.593358	45.559617
3503.245171	975925.747440	45.564621
3503.298512	975856.710821	45.569626
3503.251612	975791.894202	45.574631
3503.513366	975737.683587	45.579636
3503.481763	975664.063172	45.584641
3503.633883	975605.762729	45.589645
3503.870023	975553.119036	45.594650
3503.185198	975478.723815	45.599655
3503.603590	975438.076004	45.604660
3503.138455	975391.804306	45.609665
3503.445295	975319.590449	45.614669
3503.534289	975253.376394	45.619674
3503.484234	975196.278492	45.624679
3503.535707	975113.738878	45.629684
3503.336785	975060.380024	45.634689
3503.236838	975006.026489	45.639693
3503.319245	974960.247850	45.644698
3503.055350	974904.062357	45.649703
3503.414651	974827.824274	45.654708
3503.445803	974782.932782	45.659713
3503.271859	974717.538180	45.664717
3503.056212	974652.932054	45.669722
3502.669070	974600.871245	45.674727
3503.075916	974521.198422	45.679732
3503.015428	974478.275568	45.684737
3503.140589	974441.874281	45.689741
3503.002584	974385.076175	45.694746
3503.234239	974328.118823	45.699751
3503.250088	974254.472482	45.704756
3503.379467	974212.005369	45.709761
3502.947341	974187.919473	45.714765
3503.147200	974120.989462	45.719770
3503.130761	974056.735017	45.724775
3503.271301	973990.497886	45.729780
3502.831545	973951.839195	45.734785
3503.229158	973881.254984	45.739789
3503.177038	973836.761029	45.744794
3503.166574	973805.268449	45.749799
3503.440268	973721.205052	45.754804
3503.348850	973651.970098	45.759809
3503.091574	973604.378163	45.764813
3503.225265	973525.323374	45.769818
3503.097965	973402.978316	45.774823
3503.042226	973205.200897	45.779828
3503.070517	973001.631294	45.784833
3502.653687	972692.376945	45.789837
3503.191727	972324.737698	45.794842
3502.634360	971925.261457	45.799847
3502.650488	971446.112248	45.804852
3502.781527	970897.718679	45.809857
3502.419353	970285.152397	45.814861
3502.904284	969595.839175	45.819866
3502.623674	968844.994774	45.824871
3502.553353	967999.635351	45.829876
3502.360158	967102.958355	45.834881
3502.202694	966135.815560	45.839885
3502.126051	965102.082381	45.844890
3501.584008	963992.113412	45.849895
3501.641804	962807.943125	45.854900
3501.566324	961538.570762	45.859905
3501.499656	960192.152239	45.864909
3501.559507	958758.906057	45.869914
3501.221936	957243.464405	45.874919
3501.046651	955650.376804	45.879924
3500.754745	954040.619232	45.884929
3500.215970	952310.691386	45.889933
3500.096982	950509.851338	45.894938
3499.831139	948648.653257	45.899943
3499.626744	946702.860583	45.904948
3499.080037	944664.589232	45.909953
3498.754036	942527.121708	45.914957
3498.558744	940301.384173	45.919962
3497.870136	938018.939018	45.924967
3497.821046	935643.916674	45.929972
3497.379317	933189.332749	45.934977
3497.252415	930651.026458	45.939981
3496.802399	928033.988481	45.944986
3496.142758	925347.228614	45.949991
3495.826609	922552.259786	45.954996
3495.294151	919677.128794	45.960001
3494.742062	916706.368437	45.965005
3494.499218	913678.622217	45.970010
3493.673173	910582.188238	45.975015
3493.594854	907363.381724	45.980020
3493.120769	904083.888434	45.985025
3492.317384	900712.592709	45.990029
3492.174588	897260.781451	45.995034
3491.325215	893745.379304	46.000039
3490.606425	890103.718887	46.005044
3490.073441	886412.469150	46.010049
3489.110285	882649.075089	46.015053
3488.737697	878792.011071	46.020058
3487.987917	874835.451295	46.025063
3487.728395	870813.743379	46.030068
3487.091382	866732.850251	46.035073
3486.272579	862525.841364	46.040077
3485.594181	858245.947674	46.045082
3484.500139	853915.435339	46.050087
3483.726629	849477.491072	46.055092
3483.063038	844941.020530	46.060097
3482.569694	840343.257888	46.065101
3481.914119	835652.811895	46.070106
3480.883050	830899.308766	46.075111
3480.009161	826064.173180	46.080116
3479.018787	821123.574737	46.085121
3478.321725	816114.470748	46.090125
3477.358690	811020.081367	46.095130
3476.405816	805831.433963	46.100135
3475.675730	800573.064670	46.105140
3474.291128	795232.187295	46.110145
3473.549314	789828.654277	46.115149
3472.941732	784317.197809	46.120154
3471.595555	778737.106514	46.125159
3470.737057	773065.904246	46.130164
3470.016231	767293.980476	46.135169
3468.528773	761454.227986	46.140173
3467.881397	755536.756795	46.145178
3466.572702	749522.177523	46.150183
3465.650050	743420.943687	46.155188
3464.245384	737248.661598	46.160193
3463.300640	730988.736736	46.165197
3462.432900	724639.420041	46.170202
3460.829510	718238.574898	46.175207
3459.686894	711728.218715	46.180212
3458.468540	705129.540752	46.185217
3457.347604	698438.965820	46.190221
3456.168740	691691.187366	46.195226
3454.714752	684874.648933	46.200231
3453.102520	677942.818119	46.205236
3451.514834	670955.159827	46.210241
3450.279698	663883.543693	46.215245
3449.183580	656749.352520	46.220250
3447.554903	649519.273695	46.225255
3446.520492	642216.433704	46.230260
3444.990915	634804.173931	46.235265
3443.423866	627321.124965	46.240269
3442.136952	619767.554926	46.245274
3440.228214	612156.328810	46.250279
3438.823264	604456.695912	46.255284
3437.191190	596672.592632	46.260289
3435.684101	588812.316761	46.265293
3434.233188	580878.680037	46.270298
3432.409328	572855.894262	46.275303
3430.586094	564768.947717	46.280308
3428.987200	556610.872828	46.285313
3427.168145	548380.094775	46.290317
3425.554035	540076.259496	46.295322
3423.647166	531694.980454	46.300327
3421.643723	523219.479423	46.305332
3419.879296	514691.698314	46.310337
3417.715377	506108.735345	46.315341
3416.382873	497429.791738	46.320346
3414.057735	488697.502827	46.325351
3411.855237	479864.328410	46.330356
3409.970917	470964.869310	46.335361
3407.810303	462042.140451	46.340365
3405.745328	453046.385147	46.345370
3403.540950	443964.086247	46.350375
3401.261441	434809.372224	46.355380
3399.064322	425612.810761	46.360385
3396.849167	416357.730690	46.365389
3394.782780	407011.064600	46.370394
3392.118875	397609.865288	46.375399
3389.682532	388152.219333	46.380404
3387.168274	378624.530112	46.385409
3384.707689	369062.053027	46.390413
3382.089438	359451.021011	46.395418
3379.392113	349789.849774	46.400423
3376.687982	340071.692867	46.405428
3374.175864	330286.400992	46.410433
3371.261133	320478.944938	46.415437
3368.630305	310606.684316	46.420442
3365.630477	300700.340770	46.425447
3362.688573	290747.643911	46.430452
3359.405475	280757.115102	46.435457
3356.403106	270711.316089	46.440461
3353.417747	260628.080034	46.445466
3350.182483	250524.458202	46.450471
3346.580514	240387.148952	46.455476
3343.662479	230216.976348	46.460481
3339.987305	219975.305013	46.465485
3336.884555	209711.246888	46.470490
3333.062712	199468.461286	46.475495
3329.047632	189185.140429	46.480500
3325.305163	178903.749880	46.485505
3321.265529	168612.857571	46.490509
3316.989110	158320.816758	46.495514
3312.386696	148023.551263	46.500519
3307.872547	137724.063602	46.505524
3303.042535	127459.426752	46.510529
3297.739886	117178.117046	46.515533
3292.544047	106935.736884	46.520538
3286.908811	96747.031810	46.525543
3280.604218	86577.594525	46.530548
3273.485285	76479.743754	46.535553
3263.928087	66524.643026	46.540557
3244.256772	56920.133493	46.545562
3218.206382	47685.694638	46.550567
3191.587588	38852.430366	46.555572
3157.788634	30638.113480	46.560577
3115.528354	23220.094045	46.565581
3070.987750	16631.455138	46.570586
3028.512226	10845.789615	46.575591
2990.801842	5853.471874	46.580596
2954.657545	1728.076536	46.585601
2854.248982	364.861943	46.590605
2755.535577	384.189961	46.595610
2722.523921	374.172409	46.600615
2740.922910	349.522896	46.605620
2786.298959	347.870700	46.610625
2832.405385	337.436720	46.615629
2866.341075	333.571247	46.620634
2882.889119	354.552021	46.625639
2886.175898	350.412541	46.630644
2881.674916	323.974675	46.635649
2874.146691	316.534072	46.640653
2867.345843	333.716058	46.645658
2861.858631	332.453897	46.650663
2858.210049	324.300548	46.655668
2856.028190	317.932981	46.660673
2853.549289	324.174095	46.665677
2852.500814	329.817849	46.670682
2850.079723	320.098602	46.675687
2848.153319	299.389426	46.680692
2845.051449	311.611526	46.685697
2841.859993	325.129285	46.690701
2839.175582	317.367376	46.695706
2835.962255	325.552730	46.700711
2832.801716	328.637036	46.705716
2829.896065	308.569619	46.710721
2826.506702	315.510117	46.715725
2823.236809	318.053400	46.720730
2820.250007	331.440458	46.725735
2817.416415	319.460085	46.730740
2814.254557	299.374059	46.735745
2810.823267	300.497538	46.740749
2807.707736	309.185080	46.745754
2804.201427	307.507514	46.750759
2801.101443	314.703566	46.755764
2798.100302	302.968756	46.760769
2794.449692	297.625062	46.765773
2791.522004	311.022884	46.770778
2788.042044	309.614638	46.775783
2784.856215	320.423030	46.780788
2781.208762	299.161554	46.785793
2777.707750	304.468371	46.790797
2774.681997	300.738388	46.795802
2770.954773	304.612412	46.800807
2768.010809	301.204557	46.805812
2764.589144	297.598941	46.810817
2761.009510	288.113566	46.815821
2758.041673	292.807174	46.820826
2754.590011	290.725923	46.825831
2751.142072	278.882314	46.830836
2747.607933	291.347737	46.835841
2744.406602	294.713733	46.840845
2740.773265	297.435542	46.845850
2737.127551	298.983974	46.850855
2734.026988	293.218360	46.855860
2730.624308	282.611970	46.860865
2727.225466	287.526495	46.865869
2724.016489	285.401796	46.870874
2720.706734	287.676353	46.875879
2716.971650	290.706359	46.880884
2713.567373	287.928046	46.885889
2709.540793	285.291696	46.890893
2706.533117	270.972707	46.895898
2703.156827	291.254911	46.900903
2699.484554	286.546402	46.905908
2696.708082	279.114052	46.910913
2693.246481	293.532449	46.915917
2690.278673	269.623020	46.920922
2686.425187	278.582693	46.925927
2682.443360	279.373389	46.930932
2679.172526	291.945370	46.935937
2675.197129	296.840541	46.940941
2672.155625	285.155673	46.945946
2668.497823	270.777077	46.950951
2665.073114	278.792319	46.955956
2661.677286	291.853995	46.960961
2658.100259	283.623970	46.965965
2654.978751	263.726766	46.970970
2651.379277	281.755900	46.975975
2648.000392	292.211408	46.980980
2644.906694	274.681459	46.985985
2641.498013	278.667463	46.990989
2638.277588	273.470949	46.995994
2634.236682	286.691667	47.000999
2630.640073	290.925004	47.006004
2627.398199	280.334874	47.011009
2623.553909	279.720341	47.016013
2620.384315	274.954940	47.021018
2616.865746	276.171910	47.026023
2613.154497	283.941131	47.031028
2609.880616	276.678238	47.036033
2606.990393	278.115379	47.041037
2603.351276	260.023719	47.046042
2600.004079	262.493212	47.051047
2596.336859	272.359578	47.056052
2593.032728	256.354093	47.061057
2588.830749	275.494828	47.066061
2585.479805	274.550371	47.071066
2581.815590	260.031926	47.076071
2578.941837	270.138883	47.081076
2575.199372	263.784502	47.086081
2571.526434	271.048149	47.091085
2568.606371	277.752614	47.096090
2564.863368	255.833917	47.101095
2561.332467	250.402359	47.106100
2557.762493	267.575092	47.111105
2554.006160	270.068563	47.116109
2550.881724	257.782766	47.121114
2547.183461	267.680309	47.126119
2543.812063	272.113796	47.131124
2540.283663	242.914004	47.136129
2536.972552	249.827766	47.141133
2533.748788	256.354627	47.146138
2530.540324	263.192576	47.151143
2526.509645	252.731207	47.156148
2523.315502	236.436461	47.161153
2519.531642	251.787275	47.166157
2515.839220	266.804684	47.171162
2511.931111	257.549230	47.176167
2508.703196	248.011749	47.181172
2505.985521	237.370200	47.186177
2502.253109	246.969241	47.191181
2498.714674	266.309354	47.196186
2495.246285	244.730570	47.201191
2491.715497	243.693882	47.206196
2488.607587	257.657313	47.211201
2484.578672	264.265565	47.216205
2481.299236	256.895739	47.221210
2477.985318	239.100573	47.226215
2474.312306	225.371597	47.231220
2470.510022	243.078152	47.236225
2467.354888	264.021062	47.241229
2463.771803	242.529679	47.246234
2460.368872	239.265325	47.251239
2456.554496	243.655381	47.256244
2453.497567	249.263455	47.261249
2449.675867	249.820995	47.266253
2446.453024	243.690966	47.271258
2443.047285	246.370632	47.276263
2439.175151	242.785904	47.281268
2435.900594	241.611299	47.286273
2432.627722	239.587833	47.291277
2428.849481	251.767938	47.296282
2425.059488	256.530438	47.301287
2421.639164	247.976505	47.306292
2418.142924	225.828845	47.311297
2414.463889	239.350893	47.316301
2411.551603	252.846048	47.321306
2407.929709	250.975837	47.326311
2404.381206	247.937647	47.331316
2401.167974	235.788228	47.336321
2397.942358	251.229228	47.341325
2394.472491	227.511166	47.346330
2390.291016	243.313307	47.351335
2386.542083	250.414645	47.356340
2383.536511	235.212605	47.361345
2379.591592	233.777851	47.366349
2376.499693	242.792464	47.371354
2373.005734	246.712430	47.376359
2369.089590	241.509450	47.381364
2365.990869	233.444599	47.386369
2362.467058	228.833241	47.391373
2359.229124	231.895056	47.396378
2355.580201	244.266940	47.401383
2351.942410	242.064959	47.406388
2348.777539	232.453150	47.411393
2344.992508	234.897583	47.416397
2341.722450	240.482047	47.421402
2338.086366	246.537950	47.426407
2334.641271	236.251428	47.431412
2331.146989	208.263971	47.436417
2327.283190	232.286473	47.441421
2323.709137	245.272249	47.446426
2320.686338	237.556940	47.451431
2317.108470	229.491132	47.456436
2313.971379	217.598237	47.461441
2310.132112	246.732880	47.466445
2306.523248	233.268752	47.471450
2303.076670	235.819370	47.476455
2299.226554	239.903559	47.481460
2295.990606	237.567858	47.486465
2292.507722	249.795879	47.491469
2289.009801	232.727355	47.496474
2286.134773	217.874287	47.501479
2282.183477	216.957858	47.506484
2278.722850	225.095050	47.511489
2274.819349	229.451250	47.516493
2271.596023	226.589651	47.521498
2268.040889	210.498650	47.526503
2264.310745	209.622506	47.531508
2261.093221	216.524668	47.536513
2257.505614	242.497920	47.541517
2254.318165	227.667088	47.546522
2250.817541	222.173296	47.551527
2247.256271	224.067104	47.556532
2243.833563	231.495773	47.561537
2239.933547	230.987602	47.566541
2236.698518	212.523590	47.571546
2233.336801	221.684248	47.576551
2229.451956	229.659502	47.581556
2226.119513	213.302733	47.586561
2222.487989	215.534174	47.591565
2219.097889	223.166707	47.596570
2215.294705	217.633756	47.601575
2211.870699	213.118481	47.606580
2208.804345	216.005955	47.611585
2205.045514	234.313294	47.616589
2201.495240	223.622283	47.621594
2198.511078	210.501992	47.626599
2194.423335	215.263087	47.631604
2191.279753	225.799654	47.636609
2187.995752	224.647632	47.641613
2184.144349	209.133920	47.646618
2180.565468	206.496348	47.651623
2177.195770	215.579615	47.656628
2173.670882	218.406793	47.661633
2169.962152	224.207795	47.666637
2166.754255	226.953198	47.671642
2163.563441	223.260493	47.676647
2159.747907	206.310568	47.681652
2156.795685	207.534655	47.686657
2152.736668	212.438315	47.691661
2148.875443	229.528846	47.696666
2145.427364	215.853251	47.701671
2141.575399	214.818017	47.706676
2138.718873	212.048987	47.711681
2135.085868	219.027318	47.716685
2131.723639	204.908064	47.721690
2128.196320	219.515957	47.726695
2124.467818	225.410010	47.731700
2121.172341	226.381661	47.736705
2117.875656	219.131886	47.741709
2114.202639	211.826403	47.746714
2110.641240	218.727629	47.751719
2106.893679	224.294260	47.756724
2103.794935	215.562687	47.761729
2100.056585	209.199139	47.766733
2096.588021	203.334160	47.771738
2093.301217	212.160415	47.776743
2089.826762	223.048719	47.781748
2086.125039	205.920753	47.786753
2082.479130	231.223255	47.791757
2079.052328	217.063275	47.796762
2075.761868	201.456722	47.801767
2072.196349	228.891187	47.806772
2068.960970	211.722604	47.811777
2065.478491	199.745467	47.816781
2061.602965	187.602141	47.821786
2058.111797	209.403193	47.826791
2054.742999	218.671622	47.831796
2051.183796	206.060598	47.836801
2047.422869	228.791355	47.841805
2044.360085	213.945028	47.846810
2040.561422	221.958626	47.851815
2037.111894	218.792730	47.856820
2033.834152	207.529002	47.861825
2030.217298	218.718708	47.866829
2026.845318	219.762998	47.871834
2023.283512	216.134223	47.876839
2019.316447	226.153527	47.881844
2016.039952	205.626252	47.886849
2012.357931	199.804718	47.891853
2009.107148	199.613371	47.896858
2005.848150	210.017005	47.901863
2002.288617	208.667648	47.906868
1998.747734	203.232627	47.911873
1994.840078	212.295694	47.916877
1991.518462	204.359955	47.921882
1988.378466	209.337011	47.926887
1984.579545	213.387644	47.931892
1981.123366	190.489430	47.936897
1977.877573	208.689388	47.941901
1974.210019	201.556909	47.946906
1970.684461	185.712904	47.951911
1967.109793	185.895616	47.956916
1963.794463	192.994634	47.961921
1959.863957	205.803729	47.966925
1956.355181	220.011359	47.971930
1953.032693	213.802633	47.976935
1949.623399	203.706269	47.981940
1946.758535	201.704902	47.986945
1943.078705	199.983292	47.991949
1939.188305	208.013540	47.996954
1935.809244	204.687114	48.001959
1932.123525	202.359296	48.006964
1928.625441	204.699175	48.011969
1924.731496	214.464858	48.016973
1921.331968	206.968568	48.021978
1918.298194	209.817138	48.026983
1914.275791	204.771061	48.031988
1911.291066	179.607004	48.036993
1907.520700	192.930385	48.041997
1904.078908	204.943771	48.047002
1900.558897	190.603781	48.052007
1897.163543	210.588922	48.057012
1893.802118	202.540440	48.062017
1889.975952	199.060808	48.067021
1886.711041	193.573022	48.072026
1883.160058	208.913805	48.077031
1879.684640	210.622560	48.082036
1876.188407	190.160063	48.087041
1872.648423	190.606212	48.092045
1869.185695	211.886293	48.097050
1865.684450	201.087675	48.102055
1861.804936	197.202734	48.107060
1858.546295	201.669568	48.112065
1855.038772	195.001833	48.117069
1851.804494	186.835434	48.122074
1848.437017	181.068253	48.127079
1844.573122	194.269869	48.132084
1841.071225	175.530759	48.137089
1837.348566	192.514546	48.142093
1833.988796	211.140076	48.147098
1830.712974	204.904876	48.152103
1827.147382	204.964523	48.157108
1823.971394	197.879967	48.162113
1820.322835	193.489547	48.167117
1816.570286	199.252647	48.172122
1812.789784	185.576689	48.177127
1809.455186	198.922031	48.182132
1806.180634	188.987706	48.187137
1802.459874	177.905246	48.192141
1798.762707	198.641092	48.197146
1795.815663	197.928383	48.202151
1791.727785	203.186495	48.207156
1788.979975	192.078951	48.212161
1785.075294	207.140446	48.217165
1781.816807	187.847635	48.222170
1777.971451	175.895050	48.227175
1774.556915	196.358067	48.232180
1771.128102	205.474806	48.237185
1767.649857	206.458813	48.242189
1764.324497	198.013016	48.247194
1760.680485	180.976996	48.252199
1756.812503	195.311610	48.257204
1753.311432	173.842422	48.262209
1749.874394	175.437473	48.267213
1746.610027	183.574132	48.272218
1743.314940	197.936553	48.277223
1739.458770	202.894154	48.282228
1735.774847	185.446066	48.287233
1732.279565	189.653778	48.292237
1728.983036	200.098612	48.297242
1725.634103	203.498222	48.302247
1722.039374	194.924556	48.307252
1718.843636	184.650851	48.312257
1715.056757	191.070048	48.317261
1711.677206	178.770449	48.322266
1708.045870	186.143958	48.327271
1704.418754	199.730260	48.332276
1701.033212	186.002920	48.337281
1697.461371	176.446515	48.342285
1693.935095	180.812360	48.347290
1690.569003	192.863236	48.352295
1686.808047	187.261192	48.357300
1683.497820	187.918905	48.362305
1679.778775	176.686888	48.367309
1676.677865	164.192483	48.372314
1673.250447	177.892813	48.377319
1669.250112	189.332455	48.382324
1665.964542	183.025072	48.387329
1662.592328	185.221286	48.392333
1659.173087	178.145396	48.397338
1655.246036	174.629675	48.402343
1651.737577	178.150141	48.407348
1648.657605	188.589053	48.412353
1644.855256	192.081961	48.417357
1641.236087	190.758216	48.422362
1638.161642	185.112270	48.427367
1634.528366	201.353358	48.432372
1630.899882	183.883768	48.437377
1627.503460	184.127694	48.442381
1623.705167	202.136078	48.447386
1620.636192	198.929405	48.452391
1616.590453	205.151652	48.457396
1613.425521	173.383626	48.462401
1610.227901	195.055634	48.467405
1606.790864	187.548059	48.472410
1603.135754	196.273473	48.477415
1599.516220	194.244473	48.482420
1596.213768	195.001960	48.487425
1592.412785	203.650734	48.492429
1588.568781	195.284406	48.497434
1585.440859	197.718533	48.502439
1581.783302	190.133915	48.507444
1578.495203	187.643802	48.512449
1574.799785	198.192986	48.517453
1571.254546	193.842181	48.522458
1567.941357	191.947512	48.527463
1564.193679	189.058944	48.532468
1561.005653	176.435339	48.537473
1557.476352	192.741855	48.542477
1553.897492	182.075909	48.547482
1550.750523	171.896755	48.552487
1546.777434	181.189801	48.557492
1543.792493	169.621382	48.562497
1540.249220	175.217975	48.567501
1536.127743	188.743462	48.572506
1532.759211	182.211900	48.577511
1529.293797	169.780688	48.582516
1525.908994	184.148793	48.587521
1522.418063	170.865428	48.592525
1518.807170	184.092198	48.597530
1515.222632	183.273507	48.602535
1511.685939	187.481246	48.607540
1508.489524	172.019368	48.612545
1504.890363	177.920356	48.617549
1501.110529	185.421844	48.622554
1498.035729	187.428575	48.627559
1494.469857	196.647545	48.632564
1491.110025	166.515522	48.637569
1487.479371	177.769536	48.642573
1483.724609	170.344858	48.647578
1480.410742	174.770446	48.652583
1476.564227	186.025666	48.657588
1473.351627	162.851402	48.662593
1469.797379	169.211991	48.667597
1466.103125	164.973446	48.672602
1462.578073	178.128256	48.677607
1458.973757	174.987128	48.682612
1456.001662	153.729986	48.687617
1452.381629	178.790143	48.692621
1448.914836	186.698509	48.697626
1445.553877	168.507497	48.702631
1441.798854	165.302371	48.707636
1438.377883	170.200814	48.712641
1435.079310	178.482227	48.717645
1431.467271	178.456812	48.722650
1427.707996	172.960400	48.727655
1424.011050	189.487876	48.732660
1420.492613	184.527329	48.737665
1417.194906	167.519050	48.742669
1413.687968	172.389175	48.747674
1410.429122	170.515212	48.752679
1406.616319	195.346594	48.757684
1403.495509	175.237407	48.762689
1399.738001	179.865578	48.767693
1395.694484	185.586036	48.772698
1392.975357	186.748178	48.777703
1389.220662	184.147540	48.782708
1386.208933	164.164698	48.787713
1382.617220	178.379367	48.792717
1379.074234	181.095064	48.797722
1375.446184	169.685066	48.802727
1371.884862	161.199536	48.807732
1368.161472	170.270526	48.812737
1364.657435	177.346954	48.817741
1360.699977	179.268686	48.822746
1357.734958	171.335324	48.827751
1354.111130	176.720082	48.832756
1350.916286	178.023103	48.837761
1347.112557	173.548574	48.842765
1343.590644	172.519777	48.847770
1340.565309	167.075310	48.852775
1336.677379	166.661035	48.857780
1333.296415	170.305811	48.862785
1329.875246	167.448326	48.867789
1326.301230	158.566975	48.872794
1322.744337	158.451919	48.877799
1318.699913	175.255868	48.882804
1315.641396	181.296767	48.887809
1312.132777	179.409919	48.892813
1308.515801	163.015623	48.897818
1305.184008	157.736291	48.902823
1301.744776	175.821427	48.907828
1298.397456	167.385552	48.912833
1294.851871	172.458320	48.917837
1291.017080	170.111761	48.922842
1287.651498	165.112846	48.927847
1284.003232	155.206988	48.932852
1280.585789	170.015685	48.937857
1277.166772	180.068239	48.942861
1273.680767	169.196465	48.947866
1270.577792	145.539448	48.952871
1266.996500	162.996657	48.957876
1263.352827	178.064667	48.962881
1259.558179	174.158088	48.967885
1256.107272	176.347450	48.972890
1252.886999	149.171692	48.977895
1248.956152	169.214563	48.982900
1245.303932	177.359100	48.987905
1241.851589	161.311158	48.992909
1238.420838	156.723442	48.997914
1235.181024	159.724072	49.002919
1231.534793	176.674717	49.007924
1228.414290	173.453262	49.012929
1224.808175	169.800578	49.017933
1221.422568	164.948538	49.022938
1217.812580	169.791862	49.027943
1213.962186	165.608436	49.032948
1210.681772	144.667824	49.037953
1207.030750	160.386647	49.042957
1203.123003	176.228460	49.047962
1199.852309	177.936294	49.052967
1196.654895	165.680547	49.057972
1193.410377	167.066613	49.062977
1189.845902	172.802404	49.067981
1185.707713	161.661513	49.072986
1182.445910	151.507751	49.077991
1179.150890	172.396262	49.082996
1175.754146	164.990216	49.088001
1171.946023	169.616296	49.093005
1168.323790	152.081128	49.098010
1165.208373	150.473242	49.103015
1161.529947	161.045022	49.108020
1158.376173	152.211598	49.113025
1154.649621	169.271900	49.118029
1150.914990	161.549449	49.123034
1147.725238	159.279188	49.128039
1143.897777	168.952931	49.133044
1140.319911	163.441250	49.138049
1136.961079	166.922059	49.143053
1133.471957	173.781071	49.148058
1130.301626	171.338429	49.153063
1126.452136	173.561493	49.158068
1123.033429	176.365803	49.163073
1119.476457	176.004146	49.168077
1115.838858	152.433809	49.173082
1112.852597	146.292972	49.178087
1109.175282	166.065962	49.183092
1105.490587	171.257372	49.188097
1101.801577	163.169032	49.193101
1098.091753	170.179318	49.198106
1095.298713	160.328600	49.203111
1091.418346	165.803575	49.208116
1087.948907	160.188399	49.213121
1084.608044	163.580540	49.218125
1080.983008	157.261163	49.223130
1077.539631	159.718970	49.228135
1073.914295	161.466665	49.233140
1070.314653	154.208909	49.238145
1066.938441	162.407782	49.243149
1063.340630	171.794465	49.248154
1060.378652	152.942626	49.253159
1056.641344	145.699916	49.258164
1053.177630	152.130278	49.263169
1049.657216	154.826325	49.268173
1045.681911	166.586848	49.273178
1042.416914	157.227707	49.278183
1038.882444	151.980108	49.283188
1035.450279	150.582314	49.288193
1032.195493	170.064506	49.293197
1028.498499	165.868099	49.298202
1024.988372	139.261838	49.303207
1021.194074	154.032403	49.308212
1017.708794	169.045539	49.313217
1014.441791	145.678582	49.318221
1010.861627	161.031437	49.323226
1007.725256	173.036423	49.328231
1004.059872	158.029731	49.333236
1000.563610	155.172293	49.338241
996.835976	154.229236	49.343245
993.207863	161.808099	49.348250
989.900736	171.975264	49.353255
986.420272	165.044032	49.358260
982.977808	147.062537	49.363265
979.256371	154.479245	49.368269
976.058392	155.792718	49.373274
972.239370	162.793468	49.378279
968.535438	164.108307	49.383284
965.293600	140.777882	49.388289
962.095403	159.991886	49.393293
958.522586	170.475493	49.398298
955.141922	155.566643	49.403303
951.289728	153.529657	49.408308
947.877677	169.526970	49.413313
944.272718	153.025503	49.418317
940.783710	152.056397	49.423322
937.324675	157.166727	49.428327
933.693684	169.677193	49.433332
930.337983	156.531905	49.438337
927.222886	159.987855	49.443341
922.982775	155.550818	49.448346
919.658712	156.440530	49.453351
915.928417	159.554741	49.458356
912.749736	168.213119	49.463361
909.426466	167.551570	49.468365
905.976445	162.506928	49.473370
902.488298	149.021496	49.478375
898.628509	164.896145	49.483380
895.406653	184.537104	49.488385
891.987190	165.558470	49.493389
888.356972	153.749737	49.498394
885.218236	158.027890	49.503399
881.214668	159.382484	49.508404
877.731532	152.537093	49.513409
874.185950	146.662845	49.518413
870.756848	151.264568	49.523418
867.677867	161.956984	49.528423
863.203990	150.471455	49.533428
860.155355	161.292135	49.538433
856.607833	168.045788	49.543437
853.103994	173.245537	49.548442
850.054615	149.665490	49.553447
846.172388	153.449584	49.558452
843.062811	152.889311	49.563457
839.334585	162.234584	49.568461
835.954292	145.274783	49.573466
832.673512	136.523980	49.578471
828.743044	158.615438	49.583476
825.393098	166.921054	49.588481
821.994714	157.239197	49.593485
818.085337	156.882524	49.598490
814.641031	134.510374	49.603495
810.959930	152.162166	49.608500
807.506989	174.058001	49.613505
803.990521	152.861887	49.618509
800.540764	145.429310	49.623514
797.362246	134.058735	49.628519
793.990397	146.133436	49.633524
790.592921	155.257396	49.638529
786.585906	142.005898	49.643533
783.148859	152.739413	49.648538
779.743464	143.374026	49.653543
776.117054	160.292638	49.658548
772.637344	149.021324	49.663553
769.211284	144.485184	49.668557
765.556436	151.078931	49.673562
762.520314	171.341198	49.678567
758.456010	165.656744	49.683572
755.181725	145.421857	49.688577
751.444189	152.937217	49.693581
747.962275	170.456130	49.698586
744.838676	148.230319	49.703591
741.019642	161.983102	49.708596
737.726722	171.283669	49.713601
734.288353	144.892279	49.718605
730.743714	142.638811	49.723610
727.336404	148.795924	49.728615
723.455733	175.038584	49.733620
720.024611	169.692614	49.738625
716.906241	150.248110	49.743629
712.906845	137.644907	49.748634
709.434645	152.994832	49.753639
705.926747	168.810463	49.758644
702.662391	156.523562	49.763649
699.445959	165.533718	49.768653
695.872878	158.055371	49.773658
692.418841	144.633504	49.778663
688.380879	141.606654	49.783668
685.159380	153.561574	49.788673
681.875827	151.709124	49.793677
678.049472	144.486688	49.798682
674.545924	163.487420	49.803687
670.957806	161.770011	49.808692
667.450130	150.039444	49.813697
664.362791	140.169601	49.818701
660.822897	154.049635	49.823706
657.165562	160.473879	49.828711
653.670828	148.157292	49.833716
650.154802	137.904677	49.838721
646.343984	142.990274	49.843725
642.825608	152.076158	49.848730
639.479288	154.517162	49.853735
636.181082	155.173091	49.858740
632.547641	148.143343	49.863745
629.273596	145.574554	49.868749
625.669946	163.197850	49.873754
622.311191	135.928379	49.878759
618.214806	138.933335	49.883764
614.902291	140.402616	49.888769
611.500446	149.246816	49.893773
607.620640	141.532917	49.898778
604.668141	152.729035	49.903783
600.979104	158.330103	49.908788
597.517063	141.790596	49.913793
593.791800	144.331398	49.918797
590.405830	151.865122	49.923802
587.319234	135.898020	49.928807
583.711853	155.843203	49.933812
579.979813	170.222408	49.938817
576.444001	151.190140	49.943821
572.934921	142.405478	49.948826
569.578100	133.313743	49.953831
565.710827	149.057068	49.958836
562.898867	154.789995	49.963841
559.153758	140.776471	49.968845
555.420905	150.298224	49.973850
552.136614	147.996528	49.978855
548.639169	145.724713	49.983860
545.049362	155.321001	49.988865
541.349403	147.027283	49.993869
537.485481	142.304353	49.998874
534.611649	145.386009	50.003879
531.251808	139.915338	50.008884
527.241086	133.182760	50.013889
524.211479	139.441625	50.018893
520.298098	151.122509	50.023898
517.260562	139.620399	50.028903
513.314050	144.387556	50.033908
510.106736	137.682093	50.038913
506.489804	140.729949	50.043917
503.096246	152.413862	50.048922
499.797582	142.000748	50.053927
495.759983	152.591497	50.058932
492.244390	141.905553	50.063937
488.750004	140.840510	50.068941
485.079404	157.646373	50.073946
481.760980	149.666898	50.078951
478.123614	139.888410	50.083956
474.851817	150.194147	50.088961
471.662025	146.375082	50.093965
467.746475	152.253736	50.098970
464.672845	150.720769	50.103975
461.295873	147.006021	50.108980
457.418934	131.412525	50.113985
453.835560	136.533749	50.118989
450.177800	148.459306	50.123994
446.774518	133.315535	50.128999
443.279194	131.547517	50.134004
439.866494	131.041358	50.139009
436.821783	150.336580	50.144013
433.139917	147.773605	50.149018
429.561240	136.774467	50.154023
425.481070	137.179387	50.159028
421.903983	143.226871	50.164033
418.971525	138.781634	50.169037
415.338679	143.860544	50.174042
412.306688	145.657753	50.179047
408.595286	143.813877	50.184052
404.896729	137.038003	50.189057
401.288929	156.328006	50.194061
397.926122	158.171979	50.199066
394.390508	134.106472	50.204071
391.001178	140.002507	50.209076
386.935872	154.010775	50.214081
384.140833	150.842129	50.219085
380.260395	146.554298	50.224090
376.739630	125.834344	50.229095
373.153334	150.092201	50.234100
369.777449	143.773639	50.239105
366.776820	129.363831	50.244109
362.718706	148.227399	50.249114
359.326568	141.077963	50.254119
355.697290	146.820307	50.259124
352.163631	153.126508	50.264129
348.597604	139.286274	50.269133
344.976011	130.207049	50.274138
341.937312	126.766538	50.279143
338.377008	147.308253	50.284148
334.942870	150.433922	50.289153
331.354302	143.766485	50.294157
327.484864	146.065002	50.299162
323.929303	135.709043	50.304167
320.746087	154.335964	50.309172
316.984805	137.619900	50.314177
313.879212	139.480115	50.319181
310.267861	158.720233	50.324186
307.024757	159.185516	50.329191
303.441309	137.966643	50.334196
299.381645	124.964605	50.339201
296.110464	136.763838	50.344205
292.604120	155.382102	50.349210
289.291823	141.040592	50.354215
286.173896	137.391463	50.359220
282.479934	143.017472	50.364225
279.046879	126.362615	50.369229
275.048972	148.330475	50.374234
271.369897	141.043041	50.379239
267.963265	142.762625	50.384244
264.637694	133.261439	50.389249
261.461556	135.312377	50.394253
257.698110	141.451323	50.399258
254.367679	126.341700	50.404263
250.757750	128.691001	50.409268
247.018568	143.849651	50.414273
243.686013	124.437516	50.419277
240.051116	135.368768	50.424282
236.736065	143.862598	50.429287
233.208272	136.842487	50.434292
229.546882	125.717967	50.439297
226.283597	147.087121	50.444301
222.668423	159.242600	50.449306
219.068480	140.758811	50.454311
215.777510	122.178547	50.459316
212.243529	134.787295	50.464321
208.997220	139.889550	50.469325
205.157304	139.073916	50.474330
201.350704	121.332419	50.479335
197.897246	145.427506	50.484340
194.673212	152.692398	50.489345
191.403491	130.775036	50.494349
187.539633	145.730262	50.499354
184.485921	132.507473	50.504359
180.959309	127.256925	50.509364
177.118170	138.686713	50.514369
173.472971	135.557131	50.519373
169.586067	131.686996	50.524378
166.152295	138.119913	50.529383
162.940651	142.390199	50.534388
159.555616	132.893799	50.539393
156.363754	126.402421	50.544397
152.481851	135.052188	50.549402
149.213455	121.633577	50.554407
146.026995	134.108480	50.559412
142.400483	149.713658	50.564417
138.748918	149.046479	50.569421
134.958754	133.753773	50.574426
131.541647	126.225662	50.579431
127.849602	131.302265	50.584436
124.132758	144.664845	50.589441
121.307487	131.326223	50.594445
117.465563	127.603270	50.599450
114.275521	117.956806	50.604455
110.784338	134.115419	50.609460
106.878525	131.024207	50.614465
103.413248	120.306647	50.619469
99.577170	135.188357	50.624474
96.444735	133.376060	50.629479
93.099670	123.341004	50.634484
89.982251	127.083873	50.639489
86.320488	136.226341	50.644493
82.588545	135.170789	50.649498
79.146944	120.973719	50.654503
75.465431	129.396078	50.659508
71.935812	147.794032	50.664513
68.511651	141.055305	50.669517
64.580547	135.897806	50.674522
61.273376	121.808452	50.679527
58.005579	133.158644	50.684532
54.519754	130.806967	50.689537
51.517886	121.591701	50.694541
47.412892	133.190922	50.699546
43.892788	127.512441	50.704551
40.622857	116.402388	50.709556
37.031283	139.030379	50.714561
33.371821	127.887426	50.719565
29.741126	145.484712	50.724570
26.315420	145.256443	50.729575
22.969125	135.674414	50.734580
19.442139	126.497208	50.739585
16.461028	121.600232	50.744589
12.538393	127.169267	50.749594
8.991098	127.053040	50.754599
5.597968	124.424759	50.759604
1.645242	113.996658	50.764609