Wed Jun 15 16:32:54 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.538484	94.514105	0.000000
0.877941	74.654149	0.005005
0.673452	91.754857	0.010010
0.286641	77.886047	0.015014
0.256968	83.359643	0.020019
-0.124685	92.335541	0.025024
-0.323254	77.794323	0.030029
-0.288631	71.435151	0.035034
-0.135262	53.775203	0.040038
-0.654079	45.434655	0.045043
-0.972746	48.397715	0.050048
-0.902446	49.935674	0.055053
-1.677325	44.120264	0.060058
-1.542499	28.367669	0.065062
-1.741413	15.949228	0.070067
-2.483019	5.072545	0.075072
-2.505226	6.899135	0.080077
-2.762241	-5.624905	0.085082
-2.886538	-15.814227	0.090086
-3.291584	-20.243898	0.095091
-3.848376	-8.074864	0.100096
-4.074168	-16.489351	0.105101
-4.766833	-18.472333	0.110106
-5.077854	-14.948072	0.115110
-4.865391	-5.912187	0.120115
-5.154270	-18.052349	0.125120
-5.035966	-37.836250	0.130125
-6.043612	-27.208435	0.135130
-6.580022	-4.393299	0.140134
-6.546365	-6.096800	0.145139
-6.592742	-15.229583	0.150144
-6.604898	-25.118312	0.155149
-6.901466	-10.595793	0.160154
-6.888300	-8.714975	0.165158
-6.794846	-9.050872	0.170163
-7.839559	2.191141	0.175168
-8.238707	-23.611453	0.180173
-8.257052	-23.803495	0.185178
-8.660194	-20.240237	0.190182
-8.336425	-23.382877	0.195187
-8.741153	-13.265056	0.200192
-9.376289	-12.652712	0.205197
-9.971834	9.405544	0.210202
-9.943439	-10.191792	0.215206
-9.942001	-30.139968	0.220211
-10.062034	-18.680371	0.225216
-10.332883	-12.780460	0.230221
-10.326123	-5.026018	0.235226
-11.155533	-13.731684	0.240230
-11.492055	-5.081038	0.245235
-11.646124	-3.361785	0.250240
-11.578234	-23.724116	0.255245
-11.906035	-31.479751	0.260250
-11.859468	-17.300609	0.265254
-12.269442	-13.909935	0.270259
-13.166976	-18.692651	0.275264
-13.212741	-17.254286	0.280269
-13.508715	-2.975907	0.285274
-13.395870	-27.588407	0.290278
-13.644928	-24.681649	0.295283
-13.549966	-18.367513	0.300288
-13.783377	-0.847426	0.305293
-14.497275	-1.255081	0.310298
-15.042572	-14.750182	0.315302
-15.201043	-34.774220	0.320307
-15.136127	-9.121994	0.325312
-15.057883	-4.939581	0.330317
-15.602610	-15.782986	0.335322
-15.824258	-28.535295	0.340326
-15.983817	-23.919697	0.345331
-16.241125	-3.716947	0.350336
-16.548132	0.143726	0.355341
-17.464195	-12.293487	0.360346
-17.747316	-28.015915	0.365350
-18.048564	-18.506775	0.370355
-17.712258	-18.319836	0.375360
-17.845439	-16.628007	0.380365
-17.918741	-8.589358	0.385370
-17.967654	-10.041575	0.390374
-18.215971	-18.464668	0.395379
-19.071014	-30.742280	0.400384
-19.375299	-20.140635	0.405389
-19.623583	-17.434747	0.410394
-19.690975	-2.702890	0.415398
-19.762402	-14.108370	0.420403
-20.364579	-29.843963	0.425408
-21.039859	-29.329449	0.430413
-21.167212	-11.557601	0.435418
-20.956787	-17.026117	0.440422
-20.657289	-37.074046	0.445427
-20.925174	-25.421830	0.450432
-21.381430	-11.265432	0.455437
-22.143518	-0.554675	0.460442
-22.612711	-13.092964	0.465446
-22.721031	-24.476457	0.470451
-22.774688	-10.437395	0.475456
-22.347285	-31.423676	0.480461
-23.099579	-8.085168	0.485466
-23.834573	-8.399173	0.490470
-23.945019	-31.887195	0.495475
-24.607313	-20.052899	0.500480
-24.221828	-13.935532	0.505485
-24.360294	-16.041568	0.510490
-24.571066	-26.416050	0.515494
-24.601789	-18.388488	0.520499
-25.359009	-11.199790	0.525504
-25.586889	-22.471785	0.530509
-25.737368	-12.122931	0.535514
-25.913659	-29.079015	0.540518
-25.758132	-16.195437	0.545523
-26.587325	-3.721846	0.550528
-26.753922	-18.441176	0.555533
-27.247670	-14.189293	0.560538
-27.415863	-8.608498	0.565542
-27.314719	-26.041021	0.570547
-27.473967	-29.224577	0.575552
-27.662690	-28.937356	0.580557
-28.278599	-14.882619	0.585562
-28.717583	-1.643313	0.590566
-28.682447	-24.752141	0.595571
-28.998957	-16.675473	0.600576
-28.981710	-17.150097	0.605581
-29.765580	-27.025716	0.610586
-30.642180	-24.750057	0.615590
-30.089447	-29.715820	0.620595
-30.762191	-10.634878	0.625600
-30.856666	-10.737493	0.630605
-30.915484	-4.840956	0.635610
-30.953538	-24.018698	0.640614
-30.845947	-18.654830	0.645619
-31.024262	-11.462765	0.650624
-31.146890	-30.852814	0.655629
-31.955842	-24.101253	0.660634
-32.158700	-8.457332	0.665638
-32.294785	-8.732902	0.670643
-32.429621	-2.918599	0.675648
-33.541724	-15.450166	0.680653
-33.958619	-23.523809	0.685658
-34.180939	-0.099557	0.690662
-33.781415	-16.883188	0.695667
-33.516560	-1.715677	0.700672
-34.103025	-21.384896	0.705677
-34.179239	-24.249641	0.710682
-34.611792	-14.664940	0.715686
-35.204312	-23.558798	0.720691
-35.467615	-2.850192	0.725696
-35.647588	-15.487668	0.730701
-35.565691	-27.391480	0.735706
-35.604241	-35.278959	0.740710
-36.189548	-30.512014	0.745715
-36.984988	-33.022034	0.750720
-36.872539	-28.639902	0.755725
-37.118685	-19.554872	0.760730
-37.163637	-15.507470	0.765734
-36.907829	-19.207965	0.770739
-37.901297	-13.489697	0.775744
-38.139123	-28.823248	0.780749
-38.516095	-21.063107	0.785754
-38.728750	-24.725836	0.790758
-38.667681	-20.719829	0.795763
-39.049879	-24.834152	0.800768
-38.862854	-28.724712	0.805773
-39.347677	-10.165982	0.810778
-39.796728	-8.448880	0.815782
-39.867408	-32.464809	0.820787
-40.368573	-22.025257	0.825792
-40.175376	-9.408917	0.830797
-40.851802	-2.568272	0.835802
-41.451863	-13.091696	0.840806
-41.702185	-29.278338	0.845811
-42.228232	-10.823378	0.850816
-41.782969	1.399148	0.855821
-42.232715	-9.549325	0.860826
-41.952394	-16.240266	0.865830
-41.881709	-27.124400	0.870835
-42.720986	-11.703203	0.875840
-43.057070	-4.260446	0.880845
-43.357350	-15.626226	0.885850
-44.020494	-33.040642	0.890854
-43.816497	-26.577919	0.895859
-43.721693	-3.130718	0.900864
-44.054463	-8.048790	0.905869
-44.793309	-12.923721	0.910874
-45.068648	-0.774662	0.915878
-45.085392	-19.349653	0.920883
-45.270420	-31.974539	0.925888
-45.308801	-31.494257	0.930893
-44.942025	-6.041763	0.935898
-46.110697	-5.846009	0.940902
-46.625345	-20.284874	0.945907
-46.875536	-15.586822	0.950912
-47.038293	-4.804658	0.955917
-46.973574	-14.633492	0.960922
-47.287385	-31.346960	0.965926
-47.013192	-31.639630	0.970931
-47.965267	-13.203736	0.975936
-48.113088	-24.091811	0.980941
-48.467975	-21.666313	0.985946
-48.614360	-3.762780	0.990950
-48.404610	-16.560939	0.995955
-48.968057	-26.009349	1.000960
-49.633900	-19.188117	1.005965
-49.905925	-20.668467	1.010970
-50.047803	5.412828	1.015974
-50.179335	-17.383572	1.020979
-50.345958	-14.466564	1.025984
-50.116357	-28.931057	1.030989
-50.228890	-15.067529	1.035994
-50.971006	-32.185879	1.040998
-51.084944	-20.979136	1.046003
-51.657851	0.837624	1.051008
-51.554017	-4.088683	1.056013
-51.887233	-18.204777	1.061018
-52.792994	-27.759179	1.066022
-53.037075	-10.597203	1.071027
-53.183530	-23.548476	1.076032
-52.968416	-27.880381	1.081037
-53.133475	-24.775418	1.086042
-53.316686	-7.575952	1.091046
-53.107609	-31.814097	1.096051
-54.460556	-32.625340	1.101056
-54.614547	-25.217520	1.106061
-54.842589	-17.667346	1.111066
-55.056766	-6.860015	1.116070
-55.026448	-33.208926	1.121075
-54.948189	-31.951951	1.126080
-55.034919	-29.083957	1.131085
-56.076578	-23.615487	1.136090
-56.537393	-30.183935	1.141094
-56.713585	-21.379967	1.146099
-56.738152	-11.178585	1.151104
-56.843128	-27.592950	1.156109
-56.771442	-24.997553	1.161114
-56.969044	-12.165408	1.166118
-57.550127	-40.820603	1.171123
-58.291115	-28.632391	1.176128
-58.437562	-17.644791	1.181133
-58.322987	-14.590973	1.186138
-58.553790	-33.175648	1.191142
-58.218908	-26.804893	1.196147
-58.645131	-5.967371	1.201152
-59.046993	-7.991601	1.206157
-59.599548	-37.082500	1.211162
-60.143092	-34.171859	1.216166
-60.133119	-15.010905	1.221171
-60.211396	-17.605317	1.226176
-60.565137	-21.984667	1.231181
-61.296712	-1.692000	1.236186
-61.866480	-14.267320	1.241190
-61.313207	-30.102713	1.246195
-61.581130	-17.658070	1.251200
-61.662802	-14.787951	1.256205
-61.651660	-4.420232	1.261210
-62.083961	-8.199464	1.266214
-62.634727	-35.196614	1.271219
-63.143513	-19.493172	1.276224
-63.133715	-27.202203	1.281229
-63.018514	-27.654840	1.286234
-63.547973	-4.249582	1.291238
-63.606010	-9.415082	1.296243
-64.440726	-14.150661	1.301248
-65.162676	-31.718907	1.306253
-64.710169	-18.754997	1.311258
-65.018672	4.106621	1.316262
-64.894470	-16.689881	1.321267
-65.427874	-22.414655	1.326272
-65.512444	-20.577566	1.331277
-65.214662	-37.820319	1.336282
-66.105930	-21.659974	1.341286
-66.149185	-15.384059	1.346291
-66.544759	-11.267563	1.351296
-66.684633	-26.190263	1.356301
-66.855634	-22.361839	1.361306
-67.781237	-11.307216	1.366310
-68.035069	-14.132644	1.371315
-68.013491	-19.259214	1.376320
-67.785526	-28.727143	1.381325
-68.064519	-14.817462	1.386330
-68.305956	3.479005	1.391334
-68.536585	-11.837299	1.396339
-69.136907	-9.044917	1.401344
-69.620249	-14.945269	1.406349
-69.442454	-17.990493	1.411354
-69.787553	-23.622290	1.416358
-69.790524	-8.153854	1.421363
-70.896428	-4.799680	1.426368
-71.110977	-18.617053	1.431373
-71.029052	-30.587942	1.436378
-71.435034	-12.919206	1.441382
-71.284809	-15.372341	1.446387
-71.517309	-8.375419	1.451392
-71.647693	-25.859536	1.456397
-71.445369	-23.297765	1.461402
-72.478542	-16.167039	1.466406
-72.461592	-12.367604	1.471411
-73.206870	-28.693601	1.476416
-73.004997	-42.051331	1.481421
-72.989694	-20.114502	1.486426
-73.724415	-4.230965	1.491430
-74.063178	-23.281564	1.496435
-74.481139	-29.586507	1.501440
-74.468755	-25.252847	1.506445
-74.566499	-27.708204	1.511450
-74.917810	-24.870270	1.516454
-74.417933	-24.984897	1.521459
-75.124060	-2.620447	1.526464
-75.833305	-12.555155	1.531469
-76.100711	-18.097992	1.536474
-76.481715	-28.679403	1.541478
-76.801983	-19.244067	1.546483
-76.484872	-4.835501	1.551488
-76.582134	-16.637498	1.556493
-76.432070	-35.133594	1.561498
-77.477137	-13.126958	1.566502
-77.621314	-24.069294	1.571507
-77.842358	-20.691695	1.576512
-77.994174	-23.888906	1.581517
-78.635383	-33.789073	1.586522
-79.149292	-15.039699	1.591526
-79.122665	-18.561254	1.596531
-79.369904	-19.539549	1.601536
-79.607357	-23.534755	1.606541
-79.304028	-12.511894	1.611546
-79.670589	-21.345528	1.616550
-79.324610	-18.125859	1.621555
-80.236784	5.244806	1.626560
-80.518007	-16.379304	1.631565
-80.951077	-32.964443	1.636570
-81.075070	-18.624545	1.641574
-81.254596	-11.751893	1.646579
-81.946133	-4.110116	1.651584
-82.290889	-19.798875	1.656589
-82.666675	-28.689970	1.661594
-82.899847	-9.159846	1.666598
-83.055672	-0.531272	1.671603
-82.565982	-10.463190	1.676608
-82.831055	-26.226961	1.681613
-82.668486	-27.928386	1.686618
-83.604560	-8.537286	1.691622
-84.096207	-28.603120	1.696627
-84.397316	-31.256880	1.701632
-84.780540	-2.059169	1.706637
-84.413725	-5.209816	1.711642
-84.634362	0.119323	1.716646
-84.803971	-9.944326	1.721651
-85.646108	-0.082007	1.726656
-86.267594	-18.434624	1.731661
-86.055666	-37.473724	1.736666
-86.235178	-19.124683	1.741670
-86.139009	-5.766085	1.746675
-86.234792	-15.970072	1.751680
-86.373849	-30.190149	1.756685
-87.212112	-31.931246	1.761690
-87.738756	-1.826266	1.766694
-87.535471	-14.475386	1.771699
-87.547624	-22.439537	1.776704
-87.862997	-30.285307	1.781709
-88.692534	-21.936034	1.786714
-89.523496	-1.207897	1.791718
-89.226511	-16.029385	1.796723
-89.838453	-23.287046	1.801728
-89.532070	-17.558300	1.806733
-89.430774	-40.059024	1.811738
-89.810717	-24.113796	1.816742
-89.666434	-9.610384	1.821747
-89.903738	-11.892638	1.826752
-90.468041	-30.366062	1.831757
-90.538766	-19.165280	1.836762
-91.145888	-24.781982	1.841766
-91.448169	-24.045305	1.846771
-92.104201	-23.216130	1.851776
-92.252089	-33.941514	1.856781
-92.607506	-28.976898	1.861786
-93.043696	-27.379604	1.866790
-92.215016	-17.318264	1.871795
-92.669772	-18.872284	1.876800
-93.062563	-23.984918	1.881805
-92.778332	-19.810417	1.886810
-93.426001	-5.153522	1.891814
-94.069896	-17.276031	1.896819
-94.170449	-11.946520	1.901824
-94.094222	-14.661660	1.906829
-94.190402	-29.681636	1.911834
-95.176989	-16.962557	1.916838
-95.457225	-25.998077	1.921843
-95.849827	-12.237713	1.926848
-96.216349	-7.031546	1.931853
-96.153314	-30.293223	1.936858
-96.094225	-22.681111	1.941862
-95.746001	-13.977723	1.946867
-96.286129	-7.449425	1.951872
-97.034559	-11.495917	1.956877
-97.266914	-1.154147	1.961882
-97.505567	-11.271685	1.966886
-97.458716	-20.225927	1.971891
-97.568688	4.485421	1.976896
-98.226735	-10.108585	1.981901
-98.864267	-15.248245	1.986906
-99.094886	-0.511813	1.991910
-98.937432	-15.870151	1.996915
-99.327954	-17.105805	2.006912
-98.971788	-7.184286	2.016909
-98.055190	-11.041301	2.026906
-97.643271	-24.552706	2.036902
-97.671088	-4.229291	2.046899
-97.126179	-21.102152	2.056896
-96.334269	-6.676953	2.066893
-96.036117	-9.831223	2.076890
-94.839179	-24.250495	2.086886
-94.365786	-14.245138	2.096883
-94.809048	-15.441791	2.106880
-94.328958	-18.460192	2.116877
-93.538756	-16.127036	2.126874
-93.091606	-12.054209	2.136870
-92.236268	-18.919265	2.146867
-92.356118	-7.758604	2.156864
-91.021436	-13.842089	2.166861
-90.480556	-28.094950	2.176858
-90.191670	-10.803627	2.186854
-90.195212	-4.891358	2.196851
-89.655280	-17.063247	2.206848
-89.147681	-12.203521	2.216845
-88.109963	-9.019263	2.226842
-87.629728	-26.928706	2.236838
-87.659086	-2.994632	2.246835
-87.128639	-24.434184	2.256832
-86.394096	-8.347843	2.266829
-85.904769	-20.530428	2.276826
-84.960173	-18.123325	2.286822
-84.643762	-19.189514	2.296819
-84.628936	-10.745703	2.306816
-84.101773	-13.133918	2.316813
-82.709207	-30.116345	2.326810
-82.798710	-9.335994	2.336806
-82.839347	-27.118856	2.346803
-82.185379	-9.410306	2.356800
-81.426989	-21.113573	2.366797
-80.442818	-12.472119	2.376794
-79.854884	-11.354400	2.386790
-79.628714	-30.047483	2.396787
-79.539796	-22.960403	2.406784
-79.391715	-18.261125	2.416781
-78.246037	-11.084774	2.426778
-78.070879	-20.562526	2.436774
-77.197965	-16.227995	2.446771
-76.734704	-13.487693	2.456768
-76.665032	-17.509245	2.466765
-75.632384	-19.630361	2.476762
-75.261684	-20.145685	2.486758
-75.306150	-4.644313	2.496755
-74.192037	-3.935255	2.506752
-73.557853	-17.886983	2.516749
-73.544475	-23.866170	2.526746
-72.595425	-17.554170	2.536742
-72.214876	-4.538008	2.546739
-72.161023	-9.517800	2.556736
-71.201777	-3.299436	2.566733
-70.437582	-20.847496	2.576730
-70.378701	-11.071028	2.586726
-70.099200	-16.261751	2.596723
-69.186794	-17.685025	2.606720
-69.124004	-21.500785	2.616717
-68.436322	-26.346791	2.626714
-67.545460	-6.940387	2.636710
-67.417335	-27.922901	2.646707
-66.894458	-16.701939	2.656704
-66.326241	-10.890191	2.666701
-65.958512	-28.288269	2.676698
-65.017059	-15.834969	2.686694
-64.234255	-25.098260	2.696691
-64.668003	-6.629652	2.706688
-64.350363	-7.903170	2.716685
-63.159075	-21.731842	2.726682
-62.867425	-11.750766	2.736678
-62.075986	-15.541755	2.746675
-61.341104	-19.299297	2.756672
-60.955218	-22.640025	2.766669
-61.001304	-10.121886	2.776666
-60.821220	-10.095254	2.786662
-59.968239	-14.741506	2.796659
-59.330663	-12.654544	2.806656
-58.396709	-23.623418	2.816653
-57.697631	-10.187772	2.826650
-57.785918	-6.290269	2.836646
-57.729239	-15.864106	2.846643
-56.921963	-11.970504	2.856640
-56.034818	-24.876951	2.866637
-56.025439	-15.207075	2.876634
-55.222615	-11.586829	2.886630
-54.701765	-14.499268	2.896627
-54.576859	-20.042243	2.906624
-53.630060	-14.952067	2.916621
-53.063980	-15.423428	2.926618
-52.999289	-12.521443	2.936614
-52.322788	-16.307956	2.946611
-51.704380	-8.790513	2.956608
-51.472599	-14.194403	2.966605
-50.525443	-22.404689	2.976602
-50.104551	-0.430467	2.986598
-49.970794	-11.707921	2.996595
-49.557540	-10.443890	3.006592
-48.711049	-5.489439	3.016589
-48.330311	-12.174522	3.026586
-47.335928	-8.480542	3.036582
-46.872064	-22.512175	3.046579
-46.954650	-5.844426	3.056576
-46.557410	-0.124323	3.066573
-45.605959	-12.243529	3.076570
-44.794213	-4.483648	3.086566
-44.855285	-21.052105	3.096563
-44.765273	-4.404977	3.106560
-43.828272	-23.705361	3.116557
-43.446359	-14.251332	3.126554
-42.485523	-14.990216	3.136550
-42.306928	-15.554190	3.146547
-42.170834	-6.388342	3.156544
-41.025647	-26.534440	3.166541
-40.555686	-9.178801	3.176538
-40.472021	-25.748259	3.186534
-39.333576	-12.006137	3.196531
-39.120947	-15.220843	3.206528
-39.237169	-13.128421	3.216525
-38.227096	-11.706908	3.226522
-37.590734	-6.057536	3.236518
-37.505430	-13.918268	3.246515
-36.682147	-1.841000	3.256512
-35.779027	-20.569331	3.266509
-35.652597	-15.614011	3.276506
-35.394510	-9.693124	3.286502
-34.359392	-19.009969	3.296499
-34.146243	-19.806236	3.306496
-33.770060	-10.588703	3.316493
-33.647665	-19.658208	3.326490
-32.481691	-23.579440	3.336486
-32.128789	-15.847541	3.346483
-32.016906	-7.708670	3.356480
-31.311198	-23.651998	3.366477
-30.904667	-7.336802	3.376474
-29.727417	-17.124179	3.386470
-29.248146	-12.866815	3.396467
-29.473738	0.830904	3.406464
-29.223737	-19.027105	3.416461
-27.948997	-19.213381	3.426458
-27.684694	-14.380604	3.436454
-27.429669	-17.547400	3.446451
-26.574785	-6.917719	3.456448
-25.845114	-15.334452	3.466445
-25.906989	-12.155237	3.476442
-25.400280	-17.164039	3.486438
-24.631431	-17.474426	3.496435
-24.092184	-20.942629	3.506432
-23.827819	-10.438386	3.516429
-22.841748	-8.958282	3.526426
-22.456532	-19.463411	3.536422
-22.752659	-8.889453	3.546419
-21.344928	-22.830342	3.556416
-20.935496	-14.069296	3.566413
-20.934414	-22.837153	3.576410
-20.383671	-16.849266	3.586406
-19.293896	-19.957064	3.596403
-19.269918	-13.219165	3.606400
-18.932495	-8.848375	3.616397
-18.237673	-12.052790	3.626394
-17.898020	-24.486214	3.636390
-17.208000	-19.450097	3.646387
-16.678779	-9.928745	3.656384
-16.367040	-11.076536	3.666381
-15.394349	-6.203975	3.676378
-14.907634	-27.870296	3.686374
-14.930879	-9.050140	3.696371
-14.325649	-25.159195	3.706368
-13.344592	-11.840267	3.716365
-13.135988	-13.703506	3.726362
-12.894255	-21.319156	3.736358
-12.124486	-9.507629	3.746355
-11.889753	-9.712758	3.756352
-10.978571	-4.967225	3.766349
-10.123252	-5.100283	3.776346
-9.996947	-21.028855	3.786342
-9.811261	-9.902975	3.796339
-9.685039	-9.719085	3.806336
-8.751842	-8.575251	3.816333
-8.311563	-33.397454	3.826330
-6.930129	-19.142955	3.836326
-6.945939	-8.071385	3.846323
-6.745348	-22.083120	3.856320
-6.444080	-3.500497	3.866317
-5.677646	-14.730204	3.876314
-5.272296	-2.925118	3.886310
-4.821876	-2.810410	3.896307
-4.037793	1.117853	3.906304
-4.159254	14.628886	3.916301
-3.440994	19.811178	3.926298
-2.948039	26.152163	3.936294
-2.411306	38.428442	3.946291
-2.065668	50.867185	3.956288
-1.511029	67.673682	3.966285
-1.137951	70.516819	3.976282
-0.393678	82.988186	3.986278
0.251095	116.720806	3.996275
0.000000	120.552989	4.001280
0.350318	118.085902	4.006285
0.500264	147.128827	4.011290
0.631662	140.722066	4.016294
0.763993	127.154704	4.021299
0.508632	148.843148	4.026304
0.633169	156.984633	4.031309
0.848157	173.063281	4.036314
1.027137	172.485965	4.041318
1.548076	151.020038	4.046323
1.345669	157.939561	4.051328
1.152863	175.861341	4.056333
1.342897	176.419299	4.061338
1.194455	165.763301	4.066342
1.461446	162.771269	4.071347
1.404778	168.907330	4.076352
1.160090	159.413220	4.081357
1.240870	147.628420	4.086362
0.768039	153.916113	4.091366
1.269136	155.805985	4.096371
1.315259	162.681972	4.101376
1.220684	178.030132	4.106381
1.108171	169.462143	4.111386
1.327843	175.252751	4.116390
1.808695	184.825845	4.121395
1.402171	167.929855	4.126400
1.450502	164.433670	4.131405
1.439697	173.573146	4.136410
1.187457	157.956989	4.141414
1.208456	159.786025	4.146419
1.434358	153.582045	4.151424
1.483994	162.799420	4.156429
1.621052	181.350636	4.161434
1.582792	176.202886	4.166438
1.928501	163.479171	4.171443
1.428361	142.161382	4.176448
1.376047	138.507725	4.181453
1.495977	152.033700	4.186458
1.079543	149.513884	4.191462
1.526090	154.537302	4.196467
1.492664	157.393760	4.201472
1.498088	178.670236	4.206477
1.468411	164.988229	4.211482
1.133399	160.455683	4.216486
1.816654	142.791716	4.221491
1.520439	168.892593	4.226496
1.418707	184.228427	4.231501
1.609202	175.785458	4.236506
1.286671	168.628423	4.241510
1.303759	155.626386	4.246515
1.486159	163.599787	4.251520
1.525585	161.779700	4.256525
1.567553	153.553871	4.261530
1.419198	171.826586	4.266534
1.431255	176.986035	4.271539
1.618858	176.117371	4.276544
1.463396	193.343090	4.281549
1.835559	198.660847	4.286554
1.769847	198.061623	4.291558
1.656765	199.615402	4.296563
1.879136	205.469894	4.301568
1.821280	197.438498	4.306573
2.114279	203.582091	4.311578
1.968914	209.980233	4.316582
2.164306	191.563563	4.321587
1.371269	186.095572	4.326592
1.748592	182.954003	4.331597
1.789917	193.266763	4.336602
1.911176	198.712893	4.341606
1.784481	198.857778	4.346611
1.808167	200.448439	4.351616
2.070037	199.148350	4.356621
1.965775	215.122065	4.361626
1.692998	210.501584	4.366630
1.966418	193.618209	4.371635
2.142296	208.919313	4.376640
2.104872	215.598026	4.381645
2.415203	203.148347	4.386650
1.802079	189.506138	4.391654
2.003519	176.616138	4.396659
2.140242	203.020803	4.401664
1.860874	203.277136	4.406669
1.782907	191.865872	4.411674
1.766811	188.584035	4.416678
2.233084	199.170356	4.421683
1.902403	206.596935	4.426688
2.062907	197.289264	4.431693
2.094424	206.175542	4.436698
2.012182	213.376894	4.441702
2.324540	198.812286	4.446707
2.360224	210.007498	4.451712
2.188326	195.929741	4.456717
2.274122	183.890858	4.461722
2.235762	198.055629	4.466726
2.205516	211.742017	4.471731
2.132316	218.016173	4.476736
1.994582	205.826290	4.481741
2.244723	193.556435	4.486746
2.022359	201.330992	4.491750
1.959644	199.704556	4.496755
2.006258	191.464227	4.501760
1.848774	197.382279	4.506765
1.964828	215.503825	4.511770
2.172716	217.116231	4.516774
2.639933	221.164189	4.521779
2.366731	209.203159	4.526784
2.096231	206.879198	4.531789
2.338939	232.698465	4.536794
2.315178	225.700075	4.541798
2.706591	222.611511	4.546803
2.621364	239.764095	4.551808
2.618605	216.593782	4.556813
2.540583	217.718968	4.561818
1.983101	202.484564	4.566822
2.452479	221.460704	4.571827
2.567419	231.691384	4.576832
2.529201	218.814639	4.581837
2.324347	209.001105	4.586842
2.397869	216.837454	4.591846
2.449485	226.247889	4.596851
2.588876	232.324249	4.601856
2.506948	221.803513	4.606861
2.573687	221.713613	4.611866
2.567570	226.625321	4.616870
2.773518	226.067913	4.621875
2.687578	235.677861	4.626880
2.723973	249.308779	4.631885
2.666383	215.326033	4.636890
2.408215	216.033329	4.641894
3.048037	225.222557	4.646899
2.468507	210.814900	4.651904
2.303952	211.159390	4.656909
2.850718	214.437478	4.661914
2.596485	221.957082	4.666918
2.844221	218.762246	4.671923
2.797359	232.074763	4.676928
2.422080	238.729810	4.681933
2.622944	230.545254	4.686938
2.470259	234.939220	4.691942
2.642286	220.628419	4.696947
2.737720	250.194204	4.701952
2.636283	241.449764	4.706957
2.786839	230.289643	4.711962
2.473270	239.889466	4.716966
2.940626	242.771595	4.721971
2.591854	256.527332	4.726976
2.875331	242.612017	4.731981
2.761608	240.027264	4.736986
2.646889	251.724715	4.741990
2.894861	233.163173	4.746995
2.907612	235.354038	4.752000
2.749532	241.534410	4.757005
3.075015	241.257232	4.762010
2.780942	243.032795	4.767014
2.992512	227.250148	4.772019
2.737274	235.971742	4.777024
2.847419	250.593320	4.782029
3.121121	260.430025	4.787034
2.879718	263.199241	4.792038
3.016868	256.703487	4.797043
3.408473	260.351803	4.802048
3.080602	261.919579	4.807053
3.022856	245.418877	4.812058
2.874858	247.500965	4.817062
3.049821	266.744813	4.822067
3.374935	255.211154	4.827072
3.021191	238.177357	4.832077
3.299420	236.364951	4.837082
3.091096	235.001596	4.842086
2.972364	239.685991	4.847091
3.055829	243.955110	4.852096
2.964233	257.662528	4.857101
3.120889	255.783795	4.862106
3.100449	283.355206	4.867110
3.247345	261.453953	4.872115
3.080879	261.817404	4.877120
2.954065	265.016627	4.882125
3.402113	274.798980	4.887130
3.183031	270.894467	4.892134
3.530080	253.270743	4.897139
3.230229	264.438975	4.902144
3.573070	258.939600	4.907149
3.438245	248.088635	4.912154
3.395483	266.047972	4.917158
3.503790	271.958135	4.922163
3.361426	271.250929	4.927168
3.129980	260.211822	4.932173
3.318206	259.998957	4.937178
3.166987	273.348781	4.942182
3.323157	281.149013	4.947187
3.142024	273.715135	4.952192
3.136613	259.672743	4.957197
2.984356	264.695522	4.962202
3.283800	281.515670	4.967206
3.308056	260.527248	4.972211
3.250697	265.793886	4.977216
2.985027	289.363859	4.982221
3.551683	283.586196	4.987226
3.427705	286.638364	4.992230
3.592578	299.455857	4.997235
3.743811	300.046571	5.002240
3.657203	292.784592	5.007245
3.690107	280.087912	5.012250
3.316914	279.427533	5.017254
3.320999	292.833389	5.022259
3.684082	286.685011	5.027264
3.374978	289.517505	5.032269
3.496416	291.499436	5.037274
3.242942	298.825405	5.042278
3.763995	280.389533	5.047283
3.791750	292.102831	5.052288
3.648842	310.742273	5.057293
3.910822	315.028768	5.062298
3.789362	304.047313	5.067302
3.596682	302.612017	5.072307
3.634423	318.035102	5.077312
3.734838	303.648558	5.082317
3.992408	277.251676	5.087322
3.519823	300.399913	5.092326
3.480745	307.029319	5.097331
3.337968	308.226868	5.102336
3.602928	284.363799	5.107341
4.050788	281.661669	5.112346
3.839750	297.183159	5.117350
4.129565	311.031498	5.122355
4.092130	297.605682	5.127360
3.755737	294.839114	5.132365
3.703478	284.074508	5.137370
3.588229	309.987292	5.142374
3.746606	309.335345	5.147379
4.006097	302.701470	5.152384
3.795092	298.693122	5.157389
3.929973	297.233091	5.162394
3.694764	303.070215	5.167398
3.721672	302.333752	5.172403
3.622295	317.612091	5.177408
3.839576	330.224738	5.182413
3.976703	322.806604	5.187418
3.961394	328.551168	5.192422
3.964771	338.557880	5.197427
4.043114	344.839006	5.202432
3.972151	333.991139	5.207437
4.064301	325.421227	5.212442
4.021383	340.741752	5.217446
4.249189	330.700875	5.222451
4.196961	331.705994	5.227456
4.081953	329.150736	5.232461
4.103337	332.951500	5.237466
3.771553	350.346196	5.242470
3.850395	353.635352	5.247475
4.093259	339.941121	5.252480
4.149928	320.937972	5.257485
4.464713	315.157430	5.262490
4.084267	344.645685	5.267494
4.342464	349.235072	5.272499
4.579264	337.383798	5.277504
4.445906	342.193064	5.282509
4.732935	327.369919	5.287514
4.171002	343.457481	5.292518
4.388258	336.307244	5.297523
4.121816	339.009191	5.302528
4.357126	324.623714	5.307533
4.310578	329.158890	5.312538
4.208194	328.552897	5.317542
4.316454	332.937504	5.322547
4.518390	332.075243	5.327552
4.110318	336.993534	5.332557
4.291981	331.399432	5.337562
3.973626	326.209950	5.342566
3.959746	329.150612	5.347571
4.241160	326.028909	5.352576
3.852384	318.318288	5.357581
4.142145	334.164864	5.362586
4.111546	335.291889	5.367590
4.300901	355.088265	5.372595
4.329953	344.077666	5.377600
4.483994	364.685646	5.382605
4.248870	371.030818	5.387610
4.646329	377.312097	5.392614
4.407971	347.360095	5.397619
4.862912	341.596236	5.402624
4.243548	357.515934	5.407629
4.888936	361.794423	5.412634
4.867573	373.838577	5.417638
4.674123	359.515145	5.422643
4.852887	366.935937	5.427648
4.179442	355.574917	5.432653
4.535118	355.224287	5.437658
4.813253	370.164866	5.442662
4.858037	355.757182	5.447667
4.647754	356.081117	5.452672
4.769597	378.528893	5.457677
4.615785	381.433304	5.462682
4.741218	370.018973	5.467686
4.710732	365.544947	5.472691
4.720458	367.530058	5.477696
4.792663	352.772479	5.482701
4.866702	351.523838	5.487706
4.650304	370.692511	5.492710
4.826429	354.647368	5.497715
4.971496	348.294589	5.502720
4.548694	347.746183	5.507725
4.588033	367.136373	5.512730
4.574957	381.314400	5.517734
4.615048	370.822819	5.522739
4.634970	352.568720	5.527744
4.714667	361.588292	5.532749
4.640602	371.728174	5.537754
4.908446	385.335268	5.542758
4.624465	361.276125	5.547763
4.929555	349.427762	5.552768
4.581308	369.409576	5.557773
5.004508	381.079490	5.562778
4.961623	375.912338	5.567782
4.798196	356.339522	5.572787
4.642414	366.380447	5.577792
4.601647	364.710808	5.582797
5.186798	390.640169	5.587802
5.129530	401.515577	5.592806
5.305214	396.998001	5.597811
5.163962	368.416706	5.602816
4.907415	371.133694	5.607821
4.971560	374.335909	5.612826
4.893279	389.904312	5.617830
5.055434	390.874697	5.622835
5.064990	387.368296	5.627840
4.954486	393.954597	5.632845
4.975003	397.474177	5.637850
4.906750	398.167951	5.642854
4.943526	407.709192	5.647859
4.896421	399.674433	5.652864
4.809902	397.385738	5.657869
5.044404	376.242456	5.662874
4.772247	395.585117	5.667878
5.101903	413.900364	5.672883
5.118688	412.853939	5.677888
4.910017	414.248534	5.682893
5.576697	408.625943	5.687898
5.268061	420.644214	5.692902
5.087016	424.252846	5.697907
5.302888	422.075958	5.702912
5.445463	422.053430	5.707917
5.604361	418.378019	5.712922
5.271768	421.983975	5.717926
5.426196	416.778775	5.722931
5.376000	411.190210	5.727936
4.813790	412.364450	5.732941
5.261211	409.692754	5.737946
5.272670	421.506900	5.742950
5.171977	419.935942	5.747955
5.003358	437.290059	5.752960
5.060582	442.038266	5.757965
5.528609	419.005294	5.762970
5.719344	421.381924	5.767974
5.533657	445.436699	5.772979
5.378681	432.858935	5.777984
5.435898	426.439060	5.782989
5.612794	413.697657	5.787994
5.549739	432.703058	5.792998
5.243385	434.556533	5.798003
5.323344	437.112565	5.803008
5.362824	444.792873	5.808013
5.604392	429.232052	5.813018
5.413554	428.835897	5.818022
5.596613	418.571717	5.823027
4.978843	436.223695	5.828032
5.153997	463.485016	5.833037
5.579495	461.776884	5.838042
5.721327	451.065515	5.843046
5.715759	455.783263	5.848051
5.893712	466.670156	5.853056
5.724018	478.626742	5.858061
5.782550	464.146545	5.863066
5.821807	450.448968	5.868070
5.676970	470.413181	5.873075
5.761163	461.764306	5.878080
5.544646	463.548484	5.883085
5.939431	448.655427	5.888090
5.651974	458.601471	5.893094
5.554732	468.407474	5.898099
5.960914	465.628743	5.903104
6.160725	466.072243	5.908109
6.180701	454.441282	5.913114
5.633579	437.541420	5.918118
5.421390	444.265687	5.923123
5.800492	450.898949	5.928128
5.814841	457.056042	5.933133
5.841280	464.057051	5.938138
5.755377	469.137689	5.943142
5.896036	449.025896	5.948147
5.994364	446.744428	5.953152
5.745788	467.081507	5.958157
5.744468	479.415123	5.963162
5.789515	472.594062	5.968166
5.544766	451.683669	5.973171
5.811259	465.425122	5.978176
5.631641	481.239919	5.983181
5.906703	471.140336	5.988186
5.622560	463.610338	5.993190
5.626720	471.473570	5.998195
6.362530	480.555348	6.003200
6.280898	492.576607	6.008205
6.250674	486.747858	6.013210
5.731168	479.104039	6.018214
5.917666	466.824260	6.023219
6.146495	496.114061	6.028224
6.022173	496.171647	6.033229
6.196223	467.942520	6.038234
6.055281	462.203795	6.043238
6.020246	469.733167	6.048243
5.922433	483.279044	6.053248
5.969456	468.991826	6.058253
6.163307	484.853324	6.063258
6.093863	481.282222	6.068262
5.563315	496.756291	6.073267
6.251865	496.005969	6.078272
6.176325	490.175138	6.083277
6.434748	473.669588	6.088282
6.024272	480.626699	6.093286
5.917629	481.362927	6.098291
6.190873	471.781451	6.103296
6.162429	473.795672	6.108301
6.165359	472.662945	6.113306
6.156594	473.282574	6.118310
5.911827	477.309759	6.123315
6.132160	473.806190	6.128320
5.969042	463.342899	6.133325
5.974377	473.578142	6.138330
5.798283	490.121380	6.143334
5.607275	477.846269	6.148339
5.994743	464.459193	6.153344
6.140264	484.565339	6.158349
5.999708	487.503388	6.163354
6.080536	484.591778	6.168358
6.029067	475.183327	6.173363
6.034095	467.040676	6.178368
5.722653	481.074159	6.183373
6.314524	500.020835	6.188378
6.087020	490.027672	6.193382
6.167383	491.333866	6.198387
6.084053	470.479341	6.203392
5.821557	466.878688	6.208397
6.211336	458.612381	6.213402
5.789991	476.610262	6.218406
6.111859	466.809053	6.223411
6.167107	467.524643	6.228416
5.829065	480.663044	6.233421
6.166347	480.400880	6.238426
6.330717	481.849647	6.243430
6.239169	471.530685	6.248435
6.317955	464.686788	6.253440
6.305096	485.562031	6.258445
6.300684	474.795894	6.263450
6.329541	473.022402	6.268454
6.137898	458.834713	6.273459
6.310185	470.323117	6.278464
5.774740	468.942477	6.283469
6.209918	445.543383	6.288474
6.405414	457.634926	6.293478
5.989073	473.480057	6.298483
6.023262	463.309305	6.303488
6.011783	465.166830	6.308493
6.451371	447.540907	6.313498
6.372717	444.831945	6.318502
5.976398	452.694763	6.323507
6.111075	434.620674	6.328512
6.007187	424.156303	6.333517
5.870530	428.532976	6.338522
5.733925	454.227575	6.343526
5.895329	458.571967	6.348531
6.117386	451.496350	6.353536
5.685354	455.985669	6.358541
5.732209	462.073369	6.363546
5.771453	482.247879	6.368550
5.835990	475.276807	6.373555
6.334322	468.604377	6.378560
5.848762	472.121092	6.383565
5.901709	480.155117	6.388570
5.809498	473.715524	6.393574
5.865084	460.505721	6.398579
5.934324	462.696557	6.403584
5.854117	477.990138	6.408589
5.928622	476.035282	6.413594
5.951717	465.428560	6.418598
5.676328	466.671219	6.423603
5.619605	473.528631	6.428608
5.983945	501.890059	6.433613
6.433824	506.995318	6.438618
6.278757	476.350003	6.443622
6.039048	458.981143	6.448627
6.420127	469.647235	6.453632
6.109099	481.454151	6.458637
6.068560	460.276892	6.463642
6.367146	457.010271	6.468646
5.845950	473.321284	6.473651
6.220833	477.087835	6.478656
5.722438	476.099415	6.483661
5.660034	452.601124	6.488666
5.726756	457.647856	6.493670
5.794236	463.783840	6.498675
5.996537	471.631690	6.503680
6.027565	489.243294	6.508685
6.394899	495.505431	6.513690
6.039939	487.649745	6.518694
5.835030	491.645587	6.523699
6.245985	480.995670	6.528704
5.873689	477.370346	6.533709
6.021033	460.862746	6.538714
6.130457	461.569284	6.543718
5.611130	469.941440	6.548723
5.853434	482.966475	6.553728
5.916956	501.486112	6.558733
6.158972	503.771120	6.563738
5.902078	513.397162	6.568742
5.947736	502.457198	6.573747
6.194694	502.682292	6.578752
5.889316	489.961929	6.583757
6.395918	487.367152	6.588762
5.965837	486.345246	6.593766
6.357614	492.617942	6.598771
6.582663	487.716231	6.603776
5.886614	482.171236	6.608781
5.928385	466.261329	6.613786
5.795379	480.433519	6.618790
6.015004	494.609005	6.623795
6.165987	467.477213	6.628800
6.246981	463.036526	6.633805
6.159131	459.250260	6.638810
6.050210	477.490977	6.643814
6.046562	478.340301	6.648819
6.207483	474.156306	6.653824
6.011864	479.405420	6.658829
6.266292	462.883574	6.663834
6.328465	476.420565	6.668838
6.024264	479.162218	6.673843
6.209740	460.128435	6.678848
6.142679	461.569969	6.683853
6.468300	458.219567	6.688858
6.173014	478.431007	6.693862
6.287980	466.269590	6.698867
6.412054	462.663947	6.703872
6.207573	465.053614	6.708877
6.113980	453.682124	6.713882
6.205298	444.137340	6.718886
5.948816	432.062787	6.723891
5.973580	447.988689	6.728896
5.746077	427.135162	6.733901
5.968437	436.208049	6.738906
5.663263	464.057479	6.743910
5.818319	457.261454	6.748915
6.402934	455.586709	6.753920
6.119919	473.492079	6.758925
6.251115	462.290302	6.763930
6.139742	460.931324	6.768934
5.841205	452.535800	6.773939
6.205806	438.985711	6.778944
5.766715	454.809327	6.783949
5.867939	453.250277	6.788954
6.061009	468.697266	6.793958
6.078073	483.834500	6.798963
6.224213	474.900348	6.803968
5.877600	466.532984	6.808973
6.213928	468.993976	6.813978
5.844125	472.769159	6.818982
5.978052	486.810234	6.823987
5.950202	481.535895	6.828992
6.027469	470.607106	6.833997
6.081220	456.345029	6.839002
6.402119	465.258312	6.844006
5.942353	483.345711	6.849011
6.422034	447.448659	6.854016
6.240582	459.335949	6.859021
5.979823	457.892751	6.864026
6.197785	451.912119	6.869030
5.708906	429.159789	6.874035
6.087433	430.597428	6.879040
5.934178	451.818308	6.884045
5.623181	445.376509	6.889050
5.846322	441.449084	6.894054
6.021423	445.799002	6.899059
6.356630	455.069094	6.904064
6.338558	473.622503	6.909069
6.088249	457.304130	6.914074
5.952275	431.903360	6.919078
5.777080	456.346572	6.924083
5.946312	448.511313	6.929088
5.843634	448.988326	6.934093
6.166810	472.655015	6.939098
6.366889	470.776183	6.944102
6.289646	456.985887	6.949107
6.008672	448.806561	6.954112
5.720239	438.835437	6.959117
5.880097	443.925271	6.964122
6.039707	469.830192	6.969126
6.153863	471.671295	6.974131
6.093773	453.609642	6.979136
5.920920	439.054951	6.984141
6.073036	456.195190	6.989146
6.121003	460.278266	6.994150
5.936823	449.154363	6.999155
6.208654	435.006607	7.004160
6.102955	434.631501	7.009165
5.632286	453.271223	7.014170
5.820094	435.812995	7.019174
5.511664	466.999850	7.024179
6.094660	473.524257	7.029184
5.976222	472.012357	7.034189
6.274801	451.829478	7.039194
6.155372	466.509326	7.044198
5.941514	482.466708	7.049203
6.162234	474.862741	7.054208
6.224870	477.479254	7.059213
6.340294	478.995200	7.064218
6.159113	445.761578	7.069222
5.818621	456.224128	7.074227
6.026384	452.603572	7.079232
6.065913	476.178047	7.084237
6.100270	461.281308	7.089242
6.056911	451.720993	7.094246
5.703603	468.828268	7.099251
6.351000	477.737617	7.104256
6.041673	473.234371	7.109261
6.297445	455.317025	7.114266
6.077149	449.412568	7.119270
5.904021	454.755421	7.124275
6.382240	450.773805	7.129280
5.933707	448.008478	7.134285
6.075147	432.142409	7.139290
6.147629	434.211268	7.144294
5.902514	425.672374	7.149299
6.068517	410.913048	7.154304
5.829774	430.723053	7.159309
5.876524	448.786288	7.164314
5.718581	453.796949	7.169318
5.868823	465.472676	7.174323
6.497916	458.363331	7.179328
5.864714	481.187095	7.184333
6.244151	451.865260	7.189338
5.989753	451.324237	7.194342
5.916300	457.660485	7.199347
6.195010	457.043199	7.204352
5.911909	473.163143	7.209357
5.792676	467.108408	7.214362
6.375888	458.936307	7.219366
5.731758	472.450923	7.224371
6.160066	468.082462	7.229376
6.118482	465.095199	7.234381
6.198430	459.364066	7.239386
6.286396	436.056893	7.244390
5.879357	443.875705	7.249395
6.195021	456.888200	7.254400
5.948013	443.552724	7.259405
5.845061	440.932222	7.264410
5.824534	436.378498	7.269414
5.712110	449.387153	7.274419
5.785840	448.287910	7.279424
5.984319	458.414376	7.284429
6.147389	481.950786	7.289434
6.296890	483.253149	7.294438
5.957000	470.447157	7.299443
6.264076	457.189976	7.304448
5.687059	474.089479	7.309453
6.077233	485.343899	7.314458
6.670536	474.659019	7.319462
6.098266	472.227543	7.324467
6.158728	453.226562	7.329472
5.808888	455.178080	7.334477
5.593597	427.639985	7.339482
5.991271	443.818846	7.344486
5.812809	472.572675	7.349491
6.238573	481.003016	7.354496
5.747609	470.032293	7.359501
5.903606	453.827108	7.364506
6.215429	468.506322	7.369510
5.907378	479.316985	7.374515
6.475272	473.277332	7.379520
6.305829	474.953110	7.384525
6.397340	460.006876	7.389530
6.326732	454.686834	7.394534
5.939203	445.718963	7.399539
6.168342	429.510595	7.404544
6.358149	433.614418	7.409549
5.938221	448.825609	7.414554
6.049093	448.615857	7.419558
5.635882	448.221924	7.424563
6.096965	432.198661	7.429568
6.098319	445.271178	7.434573
6.237322	430.542634	7.439578
6.316915	432.057493	7.444582
5.967490	455.096135	7.449587
6.032515	452.816323	7.454592
6.089153	436.735695	7.459597
5.941477	450.141909	7.464602
6.185585	441.272676	7.469606
6.112798	439.254863	7.474611
6.027922	441.502140	7.479616
6.158563	449.343078	7.484621
5.823365	433.581721	7.489626
6.270659	425.358014	7.494630
6.019606	436.992609	7.499635
6.301942	427.688044	7.504640
6.085714	432.226038	7.509645
6.059897	437.923943	7.514650
6.081701	441.728808	7.519654
5.787847	456.258326	7.524659
5.885592	429.950039	7.529664
6.130557	433.515202	7.534669
6.104495	452.038436	7.539674
6.184172	434.902410	7.544678
5.841738	430.104461	7.549683
6.068408	428.175664	7.554688
6.101290	445.534372	7.559693
5.806162	451.454848	7.564698
6.058090	438.402614	7.569702
5.942714	433.528965	7.574707
6.346321	432.095835	7.579712
5.919629	441.268291	7.584717
5.771731	437.766493	7.589722
6.062133	413.364443	7.594726
5.585635	428.382240	7.599731
6.147213	445.003483	7.604736
6.058645	455.717880	7.609741
5.593063	440.462723	7.614746
6.075172	428.350853	7.619750
5.949314	451.813725	7.624755
6.002012	447.130703	7.629760
6.068066	437.542056	7.634765
6.078241	425.113883	7.639770
5.870111	417.064490	7.644774
5.767839	445.349922	7.649779
5.986776	451.624430	7.654784
6.265064	449.410095	7.659789
5.969459	439.765993	7.664794
6.216614	445.123634	7.669798
6.573264	456.395608	7.674803
6.130397	434.824874	7.679808
6.171299	427.576779	7.684813
6.087667	429.536683	7.689818
6.102349	439.340350	7.694822
6.028736	449.752676	7.699827
5.925578	447.763655	7.704832
5.923361	430.478298	7.709837
5.774495	428.761803	7.714842
5.932050	438.298394	7.719846
5.475968	447.931862	7.724851
5.948122	426.311336	7.729856
5.884494	427.342415	7.734861
6.048673	454.947451	7.739866
6.175143	473.898893	7.744870
6.116535	469.239092	7.749875
6.176012	433.208103	7.754880
6.151521	443.603823	7.759885
5.788892	455.671095	7.764890
6.103891	440.309926	7.769894
5.707675	440.672186	7.774899
5.696538	453.509918	7.779904
5.961348	464.370914	7.784909
5.884451	479.439326	7.789914
6.071524	471.078072	7.794918
5.993894	461.387871	7.799923
6.293011	459.870991	7.804928
6.121647	479.148565	7.809933
6.112646	470.225750	7.814938
6.052067	461.847422	7.819942
6.149568	462.734681	7.824947
6.448139	455.338930	7.829952
5.955847	443.186538	7.834957
5.966614	443.273787	7.839962
5.721569	435.906326	7.844966
6.024361	458.839951	7.849971
6.503514	451.526917	7.854976
6.322841	439.880000	7.859981
5.979722	447.614955	7.864986
6.137136	443.314254	7.869990
5.898419	434.342710	7.874995
6.323907	434.248076	7.880000
5.931281	443.223032	7.885005
5.909404	435.605512	7.890010
6.324626	418.171377	7.895014
5.793927	420.141040	7.900019
6.009036	432.216104	7.905024
5.883001	430.716906	7.910029
5.938931	433.593373	7.915034
6.072012	420.492728	7.920038
6.146535	439.268831	7.925043
6.205450	444.968125	7.930048
6.064247	436.750713	7.935053
6.029315	426.878179	7.940058
6.332986	425.805848	7.945062
5.880298	448.498618	7.950067
5.923999	446.908925	7.955072
5.884076	432.462390	7.960077
5.909460	423.177503	7.965082
6.177183	426.433193	7.970086
5.967047	438.986645	7.975091
5.841491	432.931094	7.980096
6.154614	441.488837	7.985101
5.961997	450.173963	7.990106
6.104653	442.366281	7.995110
5.890874	437.126333	8.000115
6.051014	432.693517	8.005133
6.072999	434.539101	8.010150
5.979614	420.060648	8.015168
6.078606	425.319284	8.020186
5.768761	444.473379	8.025203
5.975420	464.987101	8.030221
6.062377	458.538800	8.035238
6.293016	455.461154	8.040256
6.535786	442.923698	8.045274
6.495156	462.552370	8.050291
5.959347	439.908830	8.055309
6.003758	424.338422	8.060326
5.784934	433.320172	8.065344
6.074000	442.695121	8.070362
6.293777	450.660380	8.075379
6.142089	439.147681	8.080397
6.043851	433.295580	8.085414
5.547044	439.478919	8.090432
6.309690	437.206702	8.095450
5.873968	458.502953	8.100467
5.979657	469.862386	8.105485
6.214252	478.310898	8.110502
6.119020	486.379892	8.115520
6.227167	458.336242	8.120538
5.727650	470.854146	8.125555
5.971289	475.156189	8.130573
6.327093	470.695451	8.135590
5.882550	467.132702	8.140608
6.451462	467.883765	8.145626
5.750844	458.907916	8.150643
6.077880	464.268897	8.155661
6.657264	484.513432	8.160678
6.295061	486.476631	8.165696
6.369578	463.517886	8.170714
6.379733	470.226829	8.175731
6.370648	484.109049	8.180749
6.418862	476.474965	8.185766
6.079169	476.188039	8.190784
6.363177	475.069313	8.195802
5.920274	485.586612	8.200819
6.256756	471.538602	8.205837
6.382342	472.818998	8.210854
6.040708	489.807274	8.215872
6.366696	470.317279	8.220890
6.487784	470.767850	8.225907
6.416543	469.881404	8.230925
6.563927	468.715493	8.235942
5.944118	455.163723	8.240960
6.020479	458.399233	8.245978
6.159348	486.379524	8.250995
6.510657	472.166314	8.256013
6.542748	458.380172	8.261030
6.110056	470.625789	8.266048
6.414874	476.523266	8.271066
6.307202	485.601802	8.276083
6.316049	473.906096	8.281101
6.716261	467.463783	8.286118
6.248123	455.052755	8.291136
6.438234	463.368985	8.296154
6.233709	451.002658	8.301171
5.953872	450.810142	8.306189
6.655556	441.201987	8.311206
6.489550	457.116721	8.316224
6.368233	454.059553	8.321242
5.889107	447.467768	8.326259
6.419445	452.193550	8.331277
6.473526	462.108577	8.336294
6.396462	471.638117	8.341312
6.434623	456.937751	8.346330
6.533222	458.334385	8.351347
6.179380	456.230833	8.356365
6.573631	454.360046	8.361382
6.178148	480.945989	8.366400
6.142878	468.561517	8.371418
6.375235	467.022612	8.376435
6.127253	472.081001	8.381453
6.452257	472.557403	8.386470
6.398407	469.850593	8.391488
6.060744	463.938371	8.396506
6.557377	469.084471	8.401523
6.205778	467.722362	8.406541
6.441899	464.621865	8.411558
6.140448	470.738493	8.416576
6.157625	471.268029	8.421594
6.183111	459.207484	8.426611
5.986266	465.784933	8.431629
6.346183	490.770596	8.436646
6.487344	493.616969	8.441664
6.590751	502.700976	8.446682
6.569144	498.284691	8.451699
6.272187	499.502673	8.456717
6.733818	495.565623	8.461734
6.663584	487.101350	8.466752
6.533543	494.712847	8.471770
6.307193	507.131223	8.476787
6.304009	510.478877	8.481805
6.888743	492.675621	8.486822
6.573750	487.772052	8.491840
6.608581	498.504422	8.496858
6.526254	495.302455	8.501875
6.241216	500.760172	8.506893
6.555403	498.514434	8.511910
6.576765	500.348519	8.516928
6.618446	504.524444	8.521946
6.801315	508.523931	8.526963
6.576595	507.323475	8.531981
6.703712	483.667522	8.536998
6.818781	500.246868	8.542016
6.574121	498.678062	8.547034
6.936440	514.609847	8.552051
6.889648	489.421159	8.557069
6.955542	464.875117	8.562087
6.687075	478.034472	8.567104
6.659997	486.368108	8.572122
6.633280	479.500618	8.577139
6.537696	467.396411	8.582157
6.733865	461.120065	8.587175
6.675829	482.274036	8.592192
6.534390	482.628563	8.597210
6.749597	476.812712	8.602227
6.366269	469.053546	8.607245
6.356605	467.565657	8.612263
6.212533	486.561837	8.617280
6.656917	501.430051	8.622298
6.481063	494.360198	8.627315
7.001797	498.986036	8.632333
7.034941	514.823738	8.637351
6.541864	530.003453	8.642368
6.668353	509.528357	8.647386
6.842179	495.376730	8.652403
6.399301	520.506032	8.657421
6.786554	505.985853	8.662439
6.715752	510.167577	8.667456
6.774200	522.385893	8.672474
6.899412	500.980280	8.677491
6.682560	489.450465	8.682509
6.853155	491.660953	8.687527
6.696837	516.470234	8.692544
6.713567	518.632847	8.697562
6.686769	495.323776	8.702579
6.605742	494.929652	8.707597
6.866283	500.699947	8.712615
6.661175	506.736119	8.717632
6.861310	505.282040	8.722650
6.570629	502.724666	8.727667
6.700594	516.164271	8.732685
6.657052	510.578910	8.737703
6.344287	508.672146	8.742720
6.194918	488.549862	8.747738
6.483577	508.737681	8.752755
6.483245	535.158740	8.757773
6.962663	523.702660	8.762791
6.825488	523.330607	8.767808
7.062476	540.259527	8.772826
7.095854	536.947118	8.777843
7.116699	544.662212	8.782861
7.021336	536.364420	8.787879
6.885351	532.912232	8.792896
7.198174	539.743285	8.797914
6.957775	517.702005	8.802931
6.999688	505.280936	8.807949
6.839005	494.016463	8.812967
6.776803	514.794699	8.817984
6.458375	508.724600	8.823002
6.844023	526.898951	8.828019
7.086988	537.319865	8.833037
6.852324	532.391002	8.838055
7.117374	541.843483	8.843072
7.013266	548.069024	8.848090
6.971182	535.179567	8.853107
7.044489	538.901583	8.858125
7.159110	512.198807	8.863143
6.985889	501.457413	8.868160
6.881547	511.222916	8.873178
6.416568	530.020875	8.878195
7.048180	536.117744	8.883213
7.204737	520.098118	8.888231
6.916280	527.230836	8.893248
6.658841	530.051185	8.898266
7.024478	516.747119	8.903283
6.662193	529.664516	8.908301
7.199997	541.875854	8.913319
7.174948	536.622076	8.918336
6.942139	528.563575	8.923354
6.725197	534.691452	8.928371
6.966592	529.016094	8.933389
6.897111	521.639657	8.938407
7.106369	537.899135	8.943424
6.966162	538.615071	8.948442
7.114088	532.168864	8.953459
6.775627	551.992300	8.958477
7.253464	524.458042	8.963495
7.291205	540.020089	8.968512
7.137356	548.664293	8.973530
7.284153	541.380907	8.978547
7.112559	551.108743	8.983565
6.966236	532.739834	8.988583
7.263254	518.920581	8.993600
6.705883	543.596338	8.998618
7.050659	543.742402	9.003635
6.716077	536.346006	9.008653
7.006370	538.449835	9.013671
6.994673	546.732649	9.018688
7.272524	568.006277	9.023706
7.321492	572.927953	9.028723
7.105845	563.713280	9.033741
7.525593	546.150160	9.038759
7.544143	541.095417	9.043776
7.237392	553.010039	9.048794
7.433036	563.138088	9.053811
6.990630	549.962117	9.058829
7.335185	530.375401	9.063847
7.353214	533.436957	9.068864
7.198480	553.615160	9.073882
7.330848	549.717258	9.078899
6.931387	543.782944	9.083917
7.360394	528.754311	9.088935
7.289675	542.049399	9.093952
7.003017	556.330606	9.098970
6.967165	548.969261	9.103987
7.042614	526.509635	9.109005
6.982029	534.006062	9.114023
6.871579	555.894082	9.119040
7.131637	578.006356	9.124058
7.649453	552.971826	9.129075
7.379302	571.547633	9.134093
7.309957	572.248317	9.139111
7.581691	567.751852	9.144128
7.307771	581.525607	9.149146
7.465544	581.184217	9.154163
7.242143	563.967552	9.159181
7.344745	559.299686	9.164199
7.499616	565.585653	9.169216
7.384363	563.851500	9.174234
7.093336	545.251246	9.179251
7.335198	571.361257	9.184269
7.567046	571.233152	9.189287
7.514670	569.157597	9.194304
7.194572	561.158079	9.199322
7.451573	567.196132	9.204339
7.442775	569.812255	9.209357
7.296256	566.394666	9.214375
7.502043	573.578958	9.219392
7.265147	569.164481	9.224410
7.452622	568.734446	9.229427
7.516623	577.956273	9.234445
7.268322	588.910249	9.239463
7.577933	569.391248	9.244480
7.303293	570.558907	9.249498
7.433098	567.997270	9.254515
7.542555	581.930738	9.259533
7.454670	583.963544	9.264551
7.562232	570.823305	9.269568
7.396800	578.541551	9.274586
7.329023	569.220864	9.279603
7.375421	574.850838	9.284621
7.222551	585.515792	9.289639
7.319827	565.981703	9.294656
7.440438	579.578871	9.299674
7.512973	589.886195	9.304691
7.403515	577.460858	9.309709
7.222199	570.064307	9.314727
7.424532	570.376194	9.319744
7.422404	587.414152	9.324762
7.466077	575.831083	9.329779
7.229795	580.042634	9.334797
7.551433	581.162231	9.339815
7.475918	565.408208	9.344832
7.414021	581.582758	9.349850
7.655860	611.869235	9.354867
7.648094	599.541709	9.359885
7.630744	577.525079	9.364903
7.867974	565.739803	9.369920
7.596789	578.873324	9.374938
7.342019	585.930934	9.379955
7.695940	591.974039	9.384973
7.291881	587.590133	9.389991
7.410419	583.940601	9.395008
7.477945	613.942394	9.400026
7.657042	617.925414	9.405043
7.871376	610.887257	9.410061
7.729134	606.402418	9.415079
7.850041	613.181285	9.420096
7.584990	598.228122	9.425114
7.731211	612.522466	9.430131
7.723614	626.697600	9.435149
7.302519	614.040740	9.440167
7.807731	588.672994	9.445184
7.628551	601.930660	9.450202
7.976601	611.453302	9.455219
7.858295	621.671354	9.460237
7.561818	613.239576	9.465255
7.834507	589.457070	9.470272
7.514123	604.824302	9.475290
7.731096	612.581997	9.480307
8.065682	606.190322	9.485325
7.634430	599.683251	9.490343
7.855157	601.114917	9.495360
7.861568	614.453899	9.500378
7.855788	604.214143	9.505395
8.042946	606.813731	9.510413
7.697577	617.352001	9.515431
7.929915	594.821182	9.520448
7.764575	586.151865	9.525466
7.929391	601.897839	9.530483
7.798391	603.954500	9.535501
7.815157	609.247352	9.540519
7.970878	603.734312	9.545536
7.703992	605.575701	9.550554
7.717038	588.155807	9.555571
8.212316	582.299929	9.560589
7.595994	593.718453	9.565607
7.892638	604.039819	9.570624
8.121645	615.543797	9.575642
8.041529	594.336605	9.580659
7.699175	573.230243	9.585677
7.407243	602.190545	9.590695
7.712234	610.058166	9.595712
7.948340	591.373695	9.600730
7.938770	591.973582	9.605747
8.141227	605.479512	9.610765
7.360125	619.688793	9.615783
7.737524	595.891922	9.620800
7.893369	601.020883	9.625818
7.713986	607.259477	9.630835
7.952711	594.163077	9.635853
7.640564	608.836724	9.640871
7.569044	614.743214	9.645888
7.692141	615.337217	9.650906
7.670937	616.361845	9.655923
7.855519	642.934470	9.660941
7.839942	641.804824	9.665959
8.259450	638.942220	9.670976
7.904577	638.394978	9.675994
8.002577	626.684324	9.681011
8.147032	648.751649	9.686029
7.846752	659.778816	9.691047
8.166203	642.553726	9.696064
8.244432	629.262817	9.701082
7.650472	654.261639	9.706099
8.075390	647.661666	9.711117
8.062528	625.534709	9.716135
8.111667	640.073603	9.721152
8.359428	653.106272	9.726170
8.190350	641.819757	9.731187
8.458995	628.943418	9.736205
8.282020	631.532635	9.741223
8.050057	630.471910	9.746240
8.029253	638.218829	9.751258
8.045884	642.761233	9.756275
8.381960	635.386598	9.761293
8.168076	636.877987	9.766311
8.041478	638.315593	9.771328
7.920581	647.999591	9.776346
7.766391	635.817165	9.781363
8.126657	624.919824	9.786381
8.088147	645.476272	9.791399
8.264401	634.974587	9.796416
8.498063	628.595055	9.801434
8.409396	640.412107	9.806451
8.473020	645.427913	9.811469
8.339131	654.089639	9.816487
7.991056	621.899804	9.821504
8.024032	629.390655	9.826522
8.426616	647.074099	9.831539
8.584473	649.792777	9.836557
8.191680	641.715589	9.841575
8.324668	625.093616	9.846592
8.183972	644.387973	9.851610
8.232170	634.230197	9.856627
8.599953	625.643278	9.861645
8.405898	630.219118	9.866663
8.182709	623.191369	9.871680
7.895646	618.652823	9.876698
8.434185	631.987226	9.881715
8.548535	620.986571	9.886733
8.138513	647.296641	9.891751
7.861080	654.924113	9.896768
8.501895	642.307037	9.901786
8.366723	632.206920	9.906803
8.352878	634.188335	9.911821
8.224330	631.571575	9.916839
8.374332	624.211362	9.921856
8.294311	630.892966	9.926874
8.135687	655.371350	9.931891
8.037824	628.243081	9.936909
8.162423	643.445699	9.941927
8.321835	640.622142	9.946944
8.468546	635.699984	9.951962
8.009223	640.824742	9.956979
8.135666	639.851794	9.961997
8.488288	638.945475	9.967015
8.472682	647.098809	9.972032
8.124224	654.032897	9.977050
8.315947	673.290166	9.982067
8.708676	665.768494	9.987085
8.571975	657.348271	9.992103
8.141332	651.828109	9.997120
8.584790	678.300450	10.002138
8.419545	670.762748	10.007155
8.350855	679.387934	10.012173
8.362945	678.068627	10.017191
8.724481	694.557565	10.022208
8.740159	686.526401	10.027226
8.517463	681.619422	10.032243
8.798011	662.815050	10.037261
8.559916	672.319273	10.042279
8.583112	679.655410	10.047296
8.833838	653.475318	10.052314
8.400375	634.069489	10.057331
8.428347	644.683935	10.062349
8.233450	673.470799	10.067367
8.439863	678.753687	10.072384
8.726428	675.041631	10.077402
8.247768	695.447126	10.082419
8.525008	674.009260	10.087437
8.659229	671.447762	10.092455
8.726699	663.308866	10.097472
8.791367	667.060483	10.102490
8.696752	680.881249	10.107507
8.937409	681.743642	10.112525
8.639275	673.908990	10.117543
8.436136	669.312379	10.122560
8.661835	688.060646	10.127578
8.499337	682.411142	10.132595
8.603591	656.127629	10.137613
8.921049	671.867833	10.142631
8.764179	686.998439	10.147648
8.729304	678.793302	10.152666
8.602091	684.984735	10.157683
8.520195	684.314153	10.162701
8.322574	679.640072	10.167719
8.612494	672.755199	10.172736
8.948307	683.621963	10.177754
8.484988	682.374825	10.182771
8.852072	663.697549	10.187789
8.737702	673.366512	10.192807
8.692271	681.155406	10.197824
8.762255	669.207387	10.202842
8.627296	661.333673	10.207859
8.647799	666.699234	10.212877
8.331132	678.980552	10.217895
8.633315	680.593199	10.222912
9.166814	689.780504	10.227930
8.693563	686.698893	10.232947
8.827535	683.876186	10.237965
8.988755	694.561436	10.242983
8.548986	708.282321	10.248000
8.709154	703.357130	10.253018
8.892595	700.124386	10.258035
9.209321	696.587016	10.263053
9.138089	700.782639	10.268071
8.786853	698.225693	10.273088
9.010873	693.396618	10.278106
8.906096	705.094171	10.283123
8.855454	686.375202	10.288141
9.005674	695.886508	10.293159
8.575631	698.374978	10.298176
8.850642	684.138167	10.303194
8.733675	711.757520	10.308211
8.829773	711.530031	10.313229
8.987175	695.188812	10.318247
9.067621	695.739683	10.323264
9.239823	700.297231	10.328282
8.806761	717.871677	10.333299
8.858578	705.417617	10.338317
8.946111	698.098097	10.343335
8.738707	708.564232	10.348352
8.846124	687.363410	10.353370
8.884633	698.258949	10.358387
8.644812	701.776817	10.363405
8.748567	699.184335	10.368423
8.700775	711.825269	10.373440
9.121985	733.783022	10.378458
9.107307	747.856019	10.383475
9.176940	736.121729	10.388493
9.176830	751.694871	10.393511
9.005999	744.654969	10.398528
9.238085	739.709518	10.403546
9.248434	748.991776	10.408563
9.562838	721.259235	10.413581
9.562042	709.840360	10.418599
9.385262	711.494476	10.423616
9.264579	719.259122	10.428634
9.238791	718.310540	10.433651
9.176462	705.511563	10.438669
9.291797	692.701835	10.443687
8.882097	700.363881	10.448704
9.019365	715.801518	10.453722
8.706137	714.908310	10.458739
8.900030	711.129200	10.463757
9.232546	698.639483	10.468775
9.058031	723.938686	10.473792
9.635863	719.474640	10.478810
9.386781	708.989272	10.483827
9.585903	703.341008	10.488845
9.590415	707.451300	10.493863
8.890183	707.427931	10.498880
9.203404	715.889853	10.503898
9.110620	711.328029	10.508915
9.137547	697.085563	10.513933
9.348009	703.879191	10.518951
9.050579	721.735181	10.523968
9.187083	728.137804	10.528986
9.354197	728.300045	10.534003
9.376564	729.248010	10.539021
9.794935	742.449752	10.544039
9.569310	738.473500	10.549056
9.643110	725.521436	10.554074
9.272750	709.572356	10.559091
8.994311	703.113391	10.564109
9.471986	709.600631	10.569127
8.969311	704.590446	10.574144
9.318674	717.862315	10.579162
9.414883	740.082784	10.584179
9.219358	742.106340	10.589197
9.763298	727.831540	10.594215
9.232745	741.487459	10.599232
9.803794	741.885425	10.604250
9.352268	730.411726	10.609267
9.225552	707.180639	10.614285
9.088431	722.967483	10.619303
9.259456	740.776090	10.624320
9.391650	744.153968	10.629338
9.511603	747.283739	10.634355
9.383945	743.955193	10.639373
9.504171	734.246051	10.644391
9.297747	737.492732	10.649408
9.522386	734.911853	10.654426
9.415758	755.148693	10.659443
9.346187	759.375643	10.664461
9.446184	756.107576	10.669479
9.430565	755.679217	10.674496
9.407801	752.377319	10.679514
9.208066	745.807620	10.684531
9.527314	742.910398	10.689549
9.877331	745.955607	10.694567
9.731758	753.523748	10.699584
9.701951	743.692289	10.704602
9.793796	757.235624	10.709619
9.416943	751.441450	10.714637
9.349434	741.394333	10.719655
9.408463	759.425352	10.724672
9.620111	760.918951	10.729690
9.570339	755.853583	10.734707
9.739019	762.244114	10.739725
10.344918	773.551710	10.744743
9.665652	768.832822	10.749760
9.798184	743.029494	10.754778
9.729114	736.621719	10.759795
9.328335	751.152022	10.764813
9.637578	750.671356	10.769831
9.438836	757.568646	10.774848
9.776987	776.998644	10.779866
9.662114	778.827133	10.784883
9.608330	772.832651	10.789901
10.093577	765.301153	10.794919
9.752132	786.769925	10.799936
9.715819	791.893215	10.804954
10.152164	783.277560	10.809971
9.830641	774.561623	10.814989
10.292488	748.012514	10.820007
9.979440	744.931968	10.825024
9.919410	759.549531	10.830042
9.723744	755.733044	10.835059
9.520974	756.627984	10.840077
9.636675	754.095707	10.845095
9.729263	752.177814	10.850112
9.879369	758.041732	10.855130
10.066134	768.887335	10.860147
9.814366	783.494886	10.865165
10.295814	763.563091	10.870183
9.612511	754.768112	10.875200
9.797442	755.013213	10.880218
9.665987	763.807733	10.885235
9.680348	767.330842	10.890253
10.195565	756.758199	10.895271
10.003042	793.414343	10.900288
10.137535	784.707860	10.905306
9.854351	769.507395	10.910323
9.878890	767.166020	10.915341
9.894038	780.326487	10.920359
9.839355	766.454927	10.925376
10.153328	757.216866	10.930394
9.956709	768.222945	10.935411
9.688868	781.064332	10.940429
9.704757	766.662841	10.945447
9.954413	761.219534	10.950464
9.866960	772.788719	10.955482
10.021950	790.046441	10.960499
9.784299	790.592714	10.965517
9.691707	772.679868	10.970535
9.820339	778.587391	10.975552
10.064989	802.070773	10.980570
10.047561	809.798918	10.985587
10.198681	805.843733	10.990605
10.522788	798.453975	10.995623
10.482628	789.017794	11.000640
10.008268	788.246754	11.005658
10.083565	784.814500	11.010675
9.787038	792.379957	11.015693
10.048316	782.388391	11.020711
10.099610	802.582762	11.025728
10.045472	807.953525	11.030746
10.379422	794.569635	11.035763
10.001107	815.835837	11.040781
10.551628	827.271098	11.045799
10.348695	812.802505	11.050816
10.526840	811.225294	11.055834
10.516903	804.735001	11.060851
9.971732	785.743005	11.065869
10.003664	797.366082	11.070887
9.978023	798.105506	11.075904
10.186287	813.009896	11.080922
10.101506	815.115330	11.085939
10.228245	805.096488	11.090957
10.131947	808.406754	11.095975
10.398352	803.708202	11.100992
10.200917	795.245296	11.106010
10.699227	809.654329	11.111027
10.369097	823.534513	11.116045
10.497301	808.111046	11.121063
10.355130	802.241956	11.126080
9.940396	799.050579	11.131098
10.262623	811.391927	11.136115
10.254057	806.328983	11.141133
10.612524	809.951395	11.146151
10.384239	808.411534	11.151168
10.409369	808.040794	11.156186
10.412569	820.191234	11.161203
10.370874	805.754747	11.166221
10.184566	795.403395	11.171239
10.152018	790.999166	11.176256
10.196092	818.946926	11.181274
10.409330	817.714314	11.186291
10.265550	807.593659	11.191309
10.355823	807.591383	11.196327
10.773292	825.031299	11.201344
10.760859	821.685957	11.206362
10.526282	810.564530	11.211379
10.438771	828.911109	11.216397
10.357240	807.298944	11.221415
10.396373	821.071067	11.226432
10.226976	839.569836	11.231450
10.528042	824.085511	11.236467
10.689165	823.133683	11.241485
10.634109	843.912267	11.246503
11.038263	845.848641	11.251520
10.833411	845.117585	11.256538
11.169384	819.430863	11.261555
10.440110	805.742481	11.266573
10.361481	814.454993	11.271591
10.489355	825.333393	11.276608
10.400088	838.378326	11.281626
10.695056	838.504976	11.286643
10.644138	845.369118	11.291661
10.549742	841.017014	11.296679
10.690436	817.501080	11.301696
10.657792	838.088993	11.306714
10.859066	843.834871	11.311731
10.438065	847.906888	11.316749
10.275343	819.977400	11.321767
10.507867	826.158444	11.326784
9.883574	840.720947	11.331802
10.200571	849.518354	11.336819
10.877384	861.372615	11.341837
10.918213	855.692595	11.346855
11.014188	858.201712	11.351872
10.762120	880.271137	11.356890
10.563933	848.735504	11.361907
10.674443	877.642511	11.366925
10.304349	883.584572	11.371943
10.527671	869.940920	11.376960
10.653022	878.590435	11.381978
10.722159	864.741817	11.386995
10.572085	880.722252	11.392013
10.698135	881.304856	11.397031
10.959747	880.684261	11.402048
10.530451	882.989121	11.407066
11.024975	892.942045	11.412083
11.131335	895.006850	11.417101
10.888256	893.900416	11.422119
11.240272	867.481033	11.427136
10.825236	863.149734	11.432154
10.911805	867.805221	11.437171
11.283117	864.074687	11.442189
11.063843	869.266614	11.447207
11.187214	877.094524	11.452224
11.266469	871.806273	11.457242
11.155262	862.026467	11.462259
10.951599	855.989809	11.467277
11.140549	869.259587	11.472295
11.281355	886.667952	11.477312
10.829732	866.097908	11.482330
10.867423	855.933259	11.487347
11.248663	866.147441	11.492365
11.132218	885.011039	11.497383
11.316803	866.668420	11.502400
11.119336	865.578558	11.507418
11.099741	857.474611	11.512435
10.776667	870.856853	11.517453
10.777416	893.410364	11.522471
10.969988	875.070449	11.527488
10.824201	876.591148	11.532506
11.157052	871.563665	11.537523
11.354233	893.706861	11.542541
11.245992	903.642603	11.547559
11.267648	875.406533	11.552576
11.234819	868.559952	11.557594
11.408241	857.575540	11.562611
11.331151	865.229835	11.567629
11.269324	869.508278	11.572647
11.281480	876.371850	11.577664
11.093150	876.409417	11.582682
11.282065	867.115107	11.587699
11.153469	876.674275	11.592717
10.953742	877.735309	11.597735
11.423094	895.248600	11.602752
11.291743	904.521012	11.607770
11.487471	890.320236	11.612787
11.500492	876.761024	11.617805
11.186584	885.491596	11.622823
11.225557	867.331365	11.627840
11.331153	888.394304	11.632858
11.532273	902.338892	11.637875
11.708850	903.457297	11.642893
11.452349	894.014884	11.647911
11.657672	882.479064	11.652928
11.233029	867.855179	11.657946
11.042380	861.849824	11.662963
11.302961	889.233330	11.667981
11.493870	905.270503	11.672999
11.376869	900.763890	11.678016
11.439258	899.369832	11.683034
11.449439	908.269636	11.688051
11.547982	922.180026	11.693069
11.565449	918.128721	11.698087
11.881899	884.754185	11.703104
11.752786	889.362765	11.708122
11.481721	875.546544	11.713139
11.326726	876.682546	11.718157
11.348742	883.579819	11.723175
11.380843	897.812798	11.728192
11.433813	900.495521	11.733210
11.243800	897.987174	11.738227
11.481322	897.233784	11.743245
11.383612	912.237936	11.748263
11.794233	898.007741	11.753280
11.540956	920.951214	11.758298
11.555581	915.472499	11.763315
11.808138	901.178879	11.768333
11.468187	897.124654	11.773351
11.839086	900.391188	11.778368
11.702582	923.524761	11.783386
11.376006	905.893671	11.788403
11.781828	903.712436	11.793421
11.408895	911.086595	11.798439
11.954551	905.689374	11.803456
11.846472	896.267303	11.808474
11.656987	915.892421	11.813491
11.895927	905.983579	11.818509
11.407470	905.222932	11.823527
11.758222	901.745328	11.828544
11.738630	897.778085	11.833562
11.539159	892.079510	11.838579
11.753275	900.987527	11.843597
11.826419	918.019218	11.848615
12.007274	905.648565	11.853632
11.801916	899.948303	11.858650
11.786686	887.779612	11.863667
12.042270	896.932775	11.868685
11.655740	901.970707	11.873703
11.848987	906.182309	11.878720
11.758990	915.553772	11.883738
11.666053	911.538917	11.888755
11.787472	905.442122	11.893773
11.937326	915.194016	11.898791
12.297187	931.365261	11.903808
12.200822	935.093470	11.908826
12.092600	915.055239	11.913843
12.307517	902.363096	11.918861
11.904757	898.223212	11.923879
11.984639	901.861082	11.928896
11.659741	924.056258	11.933914
11.709175	902.471810	11.938931
12.054755	926.581746	11.943949
12.120459	943.737301	11.948967
12.192714	909.874854	11.953984
11.953671	903.286688	11.959002
11.808269	920.788737	11.964019
12.518835	916.872631	11.969037
12.108369	930.778684	11.974055
12.124817	920.308921	11.979072
11.911030	914.956316	11.984090
11.982155	925.492190	11.989107
12.427668	932.301392	11.994125
12.106772	910.842387	11.999143
12.390247	908.318078	12.004160
12.023547	915.801515	12.009178
11.977270	927.420199	12.014195
12.182320	932.545075	12.019213
12.009744	958.088376	12.024231
12.325292	942.009269	12.029248
12.239026	943.496916	12.034266
12.282823	947.017268	12.039283
12.122074	939.032348	12.044301
12.346046	927.592993	12.049319
12.227299	925.093626	12.054336
12.164978	937.129527	12.059354
12.265853	961.521727	12.064371
12.724627	945.055555	12.069389
12.127127	937.805143	12.074407
12.482789	932.941839	12.079424
12.394489	932.094987	12.084442
12.164295	933.761989	12.089459
12.583715	940.287982	12.094477
12.390573	941.562740	12.099495
12.759289	926.478542	12.104512
12.660543	929.672537	12.109530
12.356291	916.760352	12.114547
12.227854	898.044140	12.119565
11.825930	936.598922	12.124583
12.052806	923.944145	12.129600
12.459580	928.606562	12.134618
11.928514	934.742820	12.139635
12.136376	931.466041	12.144653
11.985473	931.498013	12.149671
12.218452	929.984937	12.154688
12.390783	951.234718	12.159706
12.266640	957.868751	12.164723
12.378797	955.929691	12.169741
12.389299	969.440900	12.174759
12.383882	980.311623	12.179776
12.478973	975.242021	12.184794
12.356480	964.402670	12.189811
12.777736	963.687892	12.194829
12.956446	970.177024	12.199847
12.515365	984.278392	12.204864
12.769142	969.729945	12.209882
12.598406	962.857798	12.214899
12.866830	962.752478	12.219917
12.366108	974.836160	12.224935
12.705214	969.574994	12.229952
12.560163	951.501162	12.234970
12.476935	950.297164	12.239987
12.556602	956.172208	12.245005
12.404285	979.371455	12.250023
12.076127	965.411379	12.255040
12.396740	955.038435	12.260058
12.372429	988.803707	12.265075
12.921505	982.689442	12.270093
12.846118	989.036958	12.275111
13.179469	996.956674	12.280128
13.113991	985.103611	12.285146
12.536678	976.253103	12.290163
12.778699	991.623327	12.295181
12.893280	994.612045	12.300199
12.837928	991.628000	12.305216
13.228928	984.195119	12.310234
12.915454	980.794990	12.315251
13.112458	963.708545	12.320269
13.134841	972.278403	12.325287
12.915511	954.615363	12.330304
12.959073	954.670696	12.335322
12.749663	953.196089	12.340339
12.771394	945.871187	12.345357
12.750574	957.781478	12.350375
12.955833	969.600001	12.355392
13.324891	982.033034	12.360410
12.911066	973.948221	12.365427
12.958421	952.964976	12.370445
12.899608	961.914688	12.375463
12.479337	988.127158	12.380480
12.876569	996.416732	12.385498
12.801123	1007.312798	12.390515
13.278866	984.088386	12.395533
13.458218	995.021770	12.400551
13.551531	996.150793	12.405568
13.170951	1002.679598	12.410586
13.136897	1003.741601	12.415603
13.200156	982.552908	12.420621
13.065013	967.306035	12.425639
13.093350	983.420733	12.430656
13.369138	1003.058790	12.435674
12.785701	998.388863	12.440691
12.999251	995.414794	12.445709
13.086357	1006.903231	12.450727
13.051959	1000.204673	12.455744
13.160955	990.632034	12.460762
12.784773	1004.515046	12.465779
13.220350	988.155811	12.470797
13.473044	1008.062879	12.475815
13.519505	1005.317749	12.480832
13.610206	993.521158	12.485850
13.330815	988.174153	12.490867
13.348679	997.857876	12.495885
13.159861	1011.692318	12.500903
13.258500	1004.432711	12.505920
13.510938	1003.065489	12.510938
13.147475	1001.180152	12.515955
13.256127	1008.375559	12.520973
13.139746	1008.662981	12.525991
13.282600	991.115026	12.531008
13.489713	1004.265192	12.536026
13.324502	1010.683846	12.541043
13.488001	999.445746	12.546061
13.252840	980.602028	12.551079
12.945158	985.309814	12.556096
13.344834	995.632032	12.561114
13.482001	1003.265231	12.566131
13.695398	990.967877	12.571149
13.843414	1009.559807	12.576167
13.608244	1002.198638	12.581184
13.185315	988.155113	12.586202
13.532606	993.431755	12.591219
13.113941	991.086934	12.596237
12.951660	1000.711278	12.601255
13.233852	1010.008475	12.606272
13.529542	1033.578537	12.611290
13.450022	1054.470084	12.616307
13.206393	1038.581389	12.621325
13.907336	1027.912432	12.626343
13.469477	1028.206633	12.631360
13.638688	1050.682549	12.636378
13.420634	1046.058867	12.641395
13.631185	1025.966630	12.646413
13.674724	1035.295237	12.651431
13.595234	1035.115457	12.656448
13.745896	1025.806906	12.661466
13.730620	1040.785851	12.666483
13.534075	1029.055768	12.671501
13.743036	1036.859776	12.676519
13.313521	1034.387344	12.681536
13.813915	1047.566251	12.686554
13.877519	1057.711037	12.691571
14.057556	1058.688562	12.696589
13.821172	1065.588963	12.701607
14.094815	1063.948811	12.706624
14.023749	1036.352612	12.711642
13.793818	1028.059375	12.716659
13.831585	1037.212898	12.721677
13.818655	1033.346266	12.726695
13.923674	1036.171456	12.731712
14.197474	1028.560038	12.736730
14.056293	1032.337005	12.741747
14.221528	1024.203213	12.746765
14.020337	1027.795164	12.751783
13.745444	1024.551109	12.756800
13.994989	1035.532159	12.761818
13.938239	1027.338420	12.766835
13.626157	1031.065500	12.771853
13.945452	1041.171070	12.776871
13.888859	1052.490349	12.781888
14.120884	1052.425386	12.786906
14.371943	1072.263165	12.791923
14.363125	1054.839071	12.796941
13.999659	1028.745472	12.801959
13.782288	1038.056878	12.806976
14.156100	1046.794924	12.811994
14.118235	1062.231447	12.817011
13.945698	1051.078731	12.822029
14.139991	1067.726288	12.827047
13.875415	1063.505368	12.832064
14.300345	1056.911222	12.837082
14.428174	1056.076173	12.842099
14.234885	1056.614632	12.847117
14.339428	1050.604208	12.852135
14.363176	1069.850276	12.857152
14.294761	1071.047360	12.862170
14.179984	1049.789767	12.867187
14.021916	1052.073642	12.872205
14.054672	1062.767685	12.877223
14.176604	1078.831888	12.882240
14.440193	1062.163653	12.887258
14.339555	1049.745725	12.892275
14.441929	1047.978404	12.897293
14.293097	1056.655914	12.902311
14.153486	1074.299468	12.907328
14.387874	1055.683891	12.912346
14.597205	1063.564899	12.917363
14.308545	1069.391631	12.922381
14.512139	1062.392437	12.927399
14.519084	1057.082025	12.932416
14.539234	1064.576192	12.937434
14.726473	1055.915648	12.942451
14.410061	1069.069360	12.947469
14.807802	1070.541880	12.952487
14.580405	1072.105998	12.957504
14.257666	1040.371119	12.962522
14.469029	1037.209853	12.967539
14.245916	1056.175323	12.972557
14.358808	1063.001471	12.977575
14.351768	1082.703811	12.982592
14.528427	1059.809360	12.987610
14.454371	1045.980206	12.992627
14.493340	1056.499147	12.997645
14.547995	1066.186772	13.002663
14.510169	1063.725473	13.007680
14.406279	1069.296037	13.012698
14.350419	1054.020330	13.017715
14.375661	1064.631188	13.022733
14.596367	1069.293499	13.027751
14.338214	1084.327680	13.032768
14.347871	1081.599442	13.037786
14.627720	1079.159837	13.042803
14.654103	1085.491658	13.047821
14.992458	1080.419016	13.052839
14.705439	1085.033675	13.057856
14.776587	1086.617044	13.062874
14.811834	1081.112328	13.067891
14.435932	1078.638311	13.072909
14.967528	1074.809504	13.077927
15.121995	1091.593754	13.082944
14.795270	1089.789887	13.087962
14.886181	1096.152180	13.092979
14.831957	1090.501065	13.097997
14.950965	1079.778081	13.103015
14.567127	1077.540751	13.108032
14.617782	1078.953927	13.113050
14.750866	1083.218915	13.118067
14.549417	1097.713357	13.123085
15.025711	1084.018361	13.128103
15.249081	1088.787495	13.133120
14.938778	1080.896293	13.138138
14.959805	1102.990181	13.143155
15.031074	1100.248413	13.148173
15.115830	1064.966485	13.153191
14.738390	1076.926453	13.158208
14.857071	1083.900141	13.163226
15.266616	1091.700156	13.168243
14.863689	1096.722854	13.173261
15.055972	1114.506932	13.178279
14.879066	1136.412569	13.183296
15.130590	1119.868086	13.188314
15.048844	1122.468806	13.193331
15.205704	1124.477671	13.198349
15.219758	1119.865006	13.203367
15.522593	1127.836967	13.208384
15.267150	1121.878527	13.213402
15.246454	1120.540393	13.218419
15.264142	1120.296533	13.223437
15.183960	1099.184495	13.228455
15.177771	1118.871194	13.233472
15.349041	1122.302132	13.238490
15.630041	1107.927457	13.243507
15.189319	1118.923843	13.248525
15.481218	1104.918047	13.253543
15.502870	1106.952107	13.258560
15.556401	1089.992257	13.263578
15.341341	1068.084643	13.268595
15.275909	1079.096522	13.273613
15.444021	1069.154902	13.278631
15.119583	1082.678955	13.283648
15.055386	1095.325967	13.288666
15.597019	1090.307994	13.293683
15.619346	1104.379828	13.298701
15.610870	1098.861470	13.303719
15.470877	1109.118854	13.308736
15.156990	1119.398388	13.313754
15.470921	1109.283074	13.318771
15.369942	1117.770177	13.323789
15.395033	1100.256786	13.328807
15.422167	1104.496484	13.333824
15.419866	1122.115827	13.338842
15.925513	1122.247812	13.343859
15.924574	1114.547731	13.348877
15.729549	1095.732958	13.353895
15.532358	1113.648115	13.358912
15.543411	1122.183421	13.363930
15.872273	1115.887242	13.368947
15.681818	1099.386399	13.373965
15.775337	1100.206220	13.378983
15.799716	1127.095853	13.384000
15.848384	1127.380503	13.389018
15.874579	1109.150165	13.394035
15.453448	1100.019997	13.399053
15.949915	1105.777905	13.404071
15.726323	1119.096985	13.409088
15.728657	1122.365730	13.414106
15.756559	1097.727241	13.419123
15.566796	1111.715854	13.424141
15.758744	1119.496344	13.429159
15.562855	1120.466526	13.434176
15.570283	1111.240143	13.439194
15.951978	1101.667338	13.444211
15.560876	1109.477559	13.449229
15.546990	1105.148384	13.454247
15.812403	1110.566026	13.459264
15.595932	1116.281855	13.464282
16.128500	1115.763091	13.469299
15.626540	1127.160552	13.474317
16.278570	1131.681640	13.479335
15.873331	1121.408166	13.484352
15.755936	1115.264652	13.489370
15.762699	1124.248492	13.494387
16.227361	1131.685962	13.499405
16.081680	1126.986334	13.504423
16.170993	1135.134102	13.509440
15.904444	1145.365388	13.514458
16.010071	1148.864351	13.519475
16.066511	1136.416557	13.524493
16.007169	1127.688972	13.529511
16.263127	1143.611340	13.534528
16.057076	1147.872857	13.539546
16.404233	1137.114788	13.544563
15.759514	1141.816423	13.549581
15.725822	1149.336652	13.554599
16.146383	1128.344628	13.559616
16.219729	1125.323446	13.564634
16.200851	1140.980872	13.569651
15.934275	1157.942328	13.574669
16.148191	1134.032602	13.579687
16.363469	1134.180690	13.584704
16.222134	1149.655261	13.589722
15.842748	1147.676866	13.594739
16.290307	1152.677115	13.599757
16.351914	1156.291989	13.604775
16.636235	1154.727111	13.609792
16.508793	1171.132057	13.614810
16.497874	1165.174224	13.619827
16.141548	1143.865791	13.624845
16.497884	1148.506598	13.629863
16.606323	1160.488773	13.634880
16.869306	1168.316885	13.639898
16.845771	1157.262863	13.644915
16.652071	1151.092485	13.649933
16.150281	1150.441579	13.654951
16.473848	1142.932582	13.659968
16.339291	1138.579748	13.664986
16.391823	1118.992521	13.670003
16.355325	1147.330186	13.675021
16.472011	1176.123673	13.680039
16.825349	1173.202829	13.685056
16.403951	1169.889669	13.690074
16.696426	1169.032523	13.695091
16.289998	1181.901771	13.700109
16.151800	1182.429260	13.705127
16.878213	1154.213284	13.710144
16.771467	1152.959724	13.715162
16.766061	1167.319103	13.720179
16.731525	1182.489120	13.725197
16.990259	1188.156358	13.730215
16.764023	1175.533449	13.735232
16.606487	1163.945795	13.740250
16.988167	1161.090332	13.745267
16.642352	1160.488435	13.750285
16.730341	1164.908205	13.755303
17.261044	1182.194318	13.760320
17.010088	1171.983088	13.765338
17.010312	1156.469620	13.770355
17.244964	1165.492086	13.775373
17.233158	1180.628430	13.780391
17.292585	1182.770502	13.785408
16.902670	1152.778555	13.790426
16.825099	1137.265860	13.795443
17.122909	1139.155984	13.800461
16.965871	1132.548558	13.805479
17.062334	1138.145766	13.810496
16.963840	1139.999439	13.815514
17.170885	1122.996471	13.820531
17.235565	1127.691178	13.825549
17.052638	1147.885253	13.830567
17.127097	1130.117174	13.835584
16.904064	1128.887655	13.840602
16.920191	1124.638829	13.845619
17.239588	1137.146715	13.850637
17.022828	1152.534861	13.855655
17.201535	1130.364987	13.860672
16.842370	1153.495556	13.865690
17.386963	1164.390942	13.870707
17.231429	1155.503295	13.875725
17.222909	1142.406942	13.880743
17.097255	1169.164001	13.885760
16.951969	1181.067087	13.890778
17.125244	1165.533967	13.895795
17.231267	1162.062012	13.900813
17.096304	1158.962283	13.905831
17.011417	1176.514156	13.910848
16.856335	1167.580868	13.915866
17.394188	1154.601446	13.920883
17.436012	1157.928126	13.925901
17.194155	1162.600880	13.930919
17.584375	1165.284891	13.935936
17.124487	1174.094954	13.940954
17.211285	1173.630077	13.945971
17.605887	1169.992645	13.950989
17.191357	1162.959564	13.956007
17.661742	1166.193380	13.961024
17.684276	1192.057105	13.966042
17.399242	1189.835017	13.971059
17.570883	1175.822461	13.976077
17.502996	1162.520894	13.981095
17.523340	1174.181203	13.986112
17.469639	1191.948260	13.991130
17.716494	1199.049701	13.996147
17.763976	1182.653999	14.001165
17.468630	1182.038742	14.006183
17.581584	1198.967241	14.011200
17.493223	1203.624187	14.016218
17.666005	1199.670733	14.021235
17.464875	1184.686554	14.026253
17.334511	1194.368821	14.031271
17.198566	1191.800419	14.036288
17.365677	1200.261271	14.041306
17.346954	1184.145933	14.046323
17.729989	1181.787366	14.051341
18.286563	1198.109315	14.056359
18.788592	1202.461559	14.061376
18.236151	1194.124504	14.066394
18.265608	1176.686762	14.071411
18.130029	1165.279883	14.076429
18.014268	1178.957089	14.081447
18.211808	1178.588844	14.086464
18.191273	1164.899620	14.091482
18.247408	1170.436493	14.096499
18.117063	1170.849916	14.101517
17.748816	1157.403352	14.106535
17.949815	1138.412182	14.111552
17.942268	1155.378849	14.116570
17.882853	1169.379135	14.121587
18.158030	1171.797090	14.126605
18.184719	1166.198505	14.131623
18.291013	1149.257226	14.136640
18.370149	1157.534904	14.141658
17.829058	1169.275297	14.146675
17.988859	1143.576506	14.151693
17.921412	1136.615575	14.156711
18.228900	1162.074765	14.161728
18.326602	1173.759486	14.166746
18.181883	1160.909882	14.171763
18.338802	1149.454382	14.176781
18.071328	1147.383691	14.181799
18.583505	1160.888721	14.186816
18.226870	1172.853002	14.191834
17.925262	1153.052962	14.196851
18.405729	1163.632350	14.201869
18.210474	1183.708066	14.206887
18.454685	1175.383626	14.211904
18.434324	1157.607175	14.216922
18.327126	1169.462138	14.221939
18.443488	1173.900444	14.226957
18.279827	1183.060085	14.231975
18.540034	1182.675580	14.236992
18.363104	1190.913132	14.242010
18.324053	1185.846539	14.247027
18.587352	1160.069018	14.252045
18.588329	1170.811586	14.257063
18.363688	1171.696289	14.262080
18.263599	1189.982107	14.267098
18.126509	1173.536917	14.272115
18.309354	1163.894007	14.277133
17.925398	1168.195656	14.282151
18.191979	1185.231496	14.287168
18.011301	1187.361192	14.292186
18.128640	1187.133828	14.297203
18.801878	1185.341919	14.302221
18.522520	1200.639203	14.307239
18.143516	1207.630150	14.312256
18.582328	1199.452038	14.317274
18.434475	1196.446929	14.322291
18.843089	1205.352404	14.327309
18.799303	1200.131901	14.332327
18.967456	1215.617978	14.337344
18.779209	1227.942472	14.342362
18.958566	1220.399703	14.347379
19.168620	1196.292533	14.352397
19.089321	1206.333800	14.357415
18.917498	1199.506203	14.362432
18.785690	1189.392566	14.367450
18.702645	1203.515854	14.372467
18.872835	1216.234638	14.377485
18.847992	1203.975376	14.382503
19.185017	1188.187766	14.387520
19.022657	1187.411786	14.392538
18.854731	1200.802820	14.397555
18.941306	1210.871783	14.402573
18.618401	1207.409299	14.407591
18.984349	1193.671925	14.412608
18.952970	1203.102560	14.417626
18.941997	1211.880181	14.422643
19.284958	1219.275223	14.427661
19.141082	1216.296119	14.432679
19.442945	1207.591849	14.437696
19.291503	1199.829511	14.442714
19.231383	1217.127791	14.447731
19.300360	1203.526274	14.452749
18.846176	1207.191171	14.457767
19.064321	1208.733630	14.462784
19.320132	1215.648800	14.467802
19.159569	1223.299061	14.472819
19.417455	1210.823328	14.477837
19.251171	1208.027316	14.482855
19.511176	1215.595869	14.487872
19.406729	1222.962314	14.492890
18.889283	1224.357109	14.497907
19.428831	1204.041807	14.502925
19.619949	1214.360755	14.507943
19.226217	1231.876151	14.512960
19.382956	1243.951075	14.517978
19.187366	1240.001512	14.522995
19.292581	1224.057829	14.528013
19.484347	1235.624616	14.533031
19.637261	1245.212671	14.538048
19.649654	1241.842667	14.543066
19.472205	1232.070127	14.548083
19.422579	1220.725263	14.553101
19.429167	1231.247412	14.558119
19.623269	1238.319311	14.563136
19.545146	1221.091673	14.568154
19.290820	1211.521864	14.573171
19.411533	1232.942536	14.578189
19.566606	1255.505223	14.583207
19.570953	1236.611375	14.588224
19.702156	1232.900457	14.593242
19.377229	1227.721091	14.598259
19.543661	1234.984918	14.603277
19.679298	1252.270764	14.608295
19.714180	1260.383411	14.613312
19.849457	1248.269070	14.618330
19.710042	1265.928359	14.623347
19.947114	1277.343433	14.628365
20.073670	1255.188590	14.633383
19.874035	1236.660854	14.638400
20.127922	1233.748955	14.643418
19.837356	1233.212710	14.648435
19.775775	1216.725080	14.653453
19.927017	1235.853658	14.658471
20.057542	1256.108351	14.663488
20.444055	1255.817216	14.668506
19.951955	1247.157734	14.673523
19.885078	1237.421038	14.678541
19.785396	1246.168074	14.683559
19.611365	1243.641677	14.688576
19.921504	1238.647251	14.693594
20.054524	1268.819875	14.698611
20.336512	1276.533511	14.703629
20.306195	1258.231449	14.708647
20.155433	1253.897988	14.713664
20.198823	1259.312423	14.718682
20.283585	1269.581185	14.723699
20.175048	1250.648902	14.728717
20.270790	1261.163620	14.733735
20.296912	1266.301548	14.738752
20.131789	1254.418593	14.743770
20.180531	1257.777116	14.748787
20.105182	1268.202522	14.753805
20.018647	1267.862622	14.758823
19.828311	1246.394165	14.763840
20.027770	1252.359934	14.768858
19.948524	1277.292224	14.773875
20.431750	1287.204174	14.778893
20.496327	1288.233465	14.783911
20.400596	1271.879539	14.788928
20.905061	1283.701013	14.793946
20.621190	1287.034114	14.798963
20.714778	1275.647732	14.803981
20.620262	1255.540270	14.808999
20.113225	1262.185458	14.814016
20.450960	1264.440075	14.819034
20.721936	1271.318520	14.824051
20.861699	1288.407216	14.829069
20.849625	1287.385089	14.834087
20.737068	1263.711057	14.839104
20.705899	1249.567519	14.844122
20.608197	1262.003721	14.849139
20.951333	1278.377855	14.854157
20.922994	1255.486681	14.859175
20.698723	1236.055159	14.864192
21.117002	1242.430917	14.869210
20.967462	1256.951175	14.874227
21.082683	1247.829996	14.879245
21.002763	1224.723429	14.884263
20.857264	1237.899915	14.889280
21.065498	1247.136194	14.894298
20.918348	1246.567391	14.899315
20.931350	1248.964822	14.904333
20.740569	1250.470754	14.909351
20.883735	1256.033326	14.914368
21.454829	1238.901286	14.919386
20.724677	1231.570413	14.924403
21.151663	1241.639231	14.929421
21.028335	1240.337826	14.934439
20.910136	1253.883938	14.939456
21.204235	1242.930476	14.944474
20.962920	1238.491442	14.949491
20.953971	1249.299273	14.954509
20.966426	1251.888482	14.959527
20.789827	1259.303474	14.964544
20.840733	1233.578543	14.969562
20.564777	1247.858918	14.974579
20.891713	1279.537836	14.979597
21.017965	1267.401649	14.984615
20.655085	1265.246240	14.989632
21.068341	1289.108908	14.994650
20.655684	1297.064682	14.999667
20.801148	1282.899009	15.004685
21.191118	1304.132995	15.009703
21.164858	1311.860885	15.014720
21.413774	1315.527599	15.019738
21.400218	1321.528302	15.024755
21.554711	1307.699421	15.029773
21.700727	1295.564769	15.034791
21.693984	1318.004028	15.039808
21.787856	1309.691273	15.044826
21.938464	1301.112414	15.049843
21.463902	1276.704768	15.054861
21.766181	1264.828698	15.059879
21.150064	1261.842016	15.064896
21.802261	1262.639288	15.069914
21.407060	1271.861157	15.074931
21.219964	1273.197919	15.079949
22.044229	1289.172847	15.084967
21.360509	1317.891343	15.089984
21.934536	1303.644988	15.095002
21.454272	1301.577263	15.100019
21.368782	1316.217670	15.105037
21.801204	1297.344225	15.110055
22.174991	1317.296065	15.115072
22.275623	1282.812302	15.120090
21.898480	1290.795364	15.125107
21.654642	1282.850465	15.130125
21.650968	1286.302282	15.135143
21.703390	1288.546881	15.140160
21.941514	1293.593694	15.145178
22.211806	1311.388137	15.150195
22.097847	1320.102050	15.155213
21.977795	1319.569997	15.160231
21.723341	1315.285242	15.165248
21.998290	1290.341800	15.170266
21.912328	1295.182980	15.175283
21.618241	1316.223799	15.180301
22.025619	1306.943011	15.185319
21.996249	1298.993560	15.190336
21.916791	1286.654499	15.195354
21.947074	1298.867364	15.200371
21.983809	1322.332079	15.205389
22.507500	1291.330023	15.210407
22.087157	1279.706990	15.215424
22.263285	1301.593588	15.220442
22.508308	1285.674560	15.225459
22.336527	1291.521520	15.230477
22.695332	1284.797686	15.235495
22.001236	1294.507935	15.240512
22.562687	1293.903606	15.245530
22.337214	1308.148339	15.250547
22.120957	1304.606214	15.255565
22.565955	1286.750742	15.260583
22.140162	1292.622852	15.265600
22.412486	1286.631547	15.270618
22.457865	1292.219050	15.275635
22.366061	1296.673786	15.280653
22.338455	1300.069535	15.285671
22.376763	1306.495123	15.290688
22.781760	1282.347041	15.295706
22.441840	1289.680599	15.300723
22.098806	1301.733261	15.305741
22.168415	1283.670796	15.310759
22.282429	1299.955288	15.315776
22.752649	1313.654057	15.320794
22.674578	1308.451089	15.325811
22.602533	1309.090554	15.330829
22.914215	1323.111525	15.335847
22.584640	1337.069917	15.340864
22.414631	1323.028666	15.345882
22.594514	1316.607060	15.350899
22.569395	1322.287209	15.355917
22.720201	1303.533703	15.360935
22.745075	1326.171639	15.365952
22.975096	1335.533869	15.370970
22.905683	1328.363972	15.375987
22.618705	1306.135399	15.381005
22.810192	1322.272596	15.386023
22.688264	1317.892432	15.391040
23.133497	1298.409036	15.396058
23.002874	1313.574299	15.401075
22.802900	1327.730506	15.406093
23.007073	1319.869192	15.411111
22.909086	1303.426354	15.416128
22.761479	1299.406361	15.421146
22.923778	1317.715687	15.426163
22.782967	1355.644747	15.431181
23.272583	1341.551743	15.436199
23.585308	1340.931344	15.441216
23.370372	1338.570808	15.446234
23.528372	1337.590043	15.451251
22.982208	1329.275394	15.456269
23.380437	1308.376755	15.461287
22.942695	1309.094169	15.466304
23.422506	1338.848289	15.471322
23.673741	1360.033741	15.476339
23.171348	1339.557452	15.481357
23.739209	1302.167261	15.486375
23.270776	1317.208670	15.491392
23.362833	1311.330001	15.496410
23.518864	1311.738611	15.501427
23.428406	1319.887354	15.506445
23.676253	1295.871298	15.511463
23.303631	1307.511039	15.516480
23.341566	1301.441363	15.521498
23.374277	1308.702526	15.526515
23.353440	1338.796605	15.531533
23.127743	1353.060211	15.536551
23.253998	1337.736117	15.541568
23.412340	1341.015733	15.546586
23.945866	1344.818352	15.551603
23.316918	1364.446310	15.556621
23.919901	1349.346010	15.561639
24.018507	1345.332255	15.566656
23.768634	1346.207262	15.571674
24.110194	1355.420787	15.576691
23.934217	1348.508593	15.581709
23.902163	1347.172808	15.586727
23.680686	1336.245637	15.591744
23.723163	1347.824782	15.596762
24.160835	1349.676568	15.601779
24.026043	1342.805000	15.606797
24.131299	1334.767058	15.611815
24.139800	1340.161899	15.616832
23.961600	1336.617218	15.621850
24.349660	1337.500064	15.626867
23.882298	1341.677485	15.631885
24.335903	1353.478685	15.636903
24.129652	1327.444106	15.641920
23.778631	1327.381421	15.646938
24.309234	1326.694906	15.651955
24.072587	1345.122347	15.656973
23.994607	1329.903943	15.661991
23.371958	1327.564832	15.667008
23.842348	1341.010408	15.672026
24.052471	1355.993743	15.677043
23.929839	1351.404187	15.682061
24.250989	1338.339879	15.687079
23.980169	1336.226811	15.692096
23.890231	1330.844835	15.697114
24.254313	1344.801667	15.702131
24.156841	1371.860356	15.707149
24.479730	1362.214155	15.712167
24.437590	1367.877552	15.717184
24.422817	1378.270488	15.722202
24.576238	1361.609999	15.727219
24.309270	1360.351115	15.732237
24.644158	1359.285619	15.737255
24.677483	1375.812017	15.742272
24.573930	1373.853347	15.747290
24.526415	1348.794732	15.752307
24.162663	1348.268215	15.757325
24.635963	1355.396466	15.762343
24.737209	1368.728405	15.767360
24.682604	1375.755759	15.772378
24.906834	1353.117810	15.777395
24.425402	1362.681959	15.782413
24.722437	1356.210176	15.787431
24.848452	1369.286603	15.792448
24.712436	1371.595123	15.797466
24.738439	1346.966190	15.802483
24.989307	1369.349177	15.807501
24.598961	1371.840344	15.812519
24.848101	1361.795301	15.817536
24.968837	1355.791431	15.822554
24.942021	1346.520280	15.827571
24.942132	1357.299728	15.832589
25.272669	1357.094203	15.837607
24.716238	1356.681890	15.842624
24.850890	1375.787406	15.847642
25.020212	1365.299848	15.852659
24.845075	1360.616332	15.857677
24.746898	1369.310052	15.862695
25.231030	1376.595935	15.867712
25.080471	1401.256713	15.872730
25.542750	1388.451162	15.877747
25.091655	1394.736946	15.882765
25.160693	1385.187885	15.887783
25.405078	1373.109831	15.892800
25.229647	1384.164511	15.897818
25.423848	1393.326739	15.902835
25.269489	1399.215338	15.907853
25.725359	1382.422186	15.912871
25.540135	1360.208109	15.917888
25.434588	1347.251701	15.922906
25.530026	1351.861392	15.927923
25.218517	1365.202004	15.932941
25.195912	1355.921591	15.937959
25.563467	1369.080220	15.942976
25.553049	1377.972385	15.947994
25.873632	1371.824877	15.953011
25.356380	1374.489048	15.958029
25.552681	1375.055437	15.963047
26.085115	1369.052703	15.968064
25.770692	1374.062832	15.973082
25.503171	1344.009937	15.978099
25.610270	1340.509326	15.983117
25.349545	1357.504379	15.988135
25.627701	1371.038035	15.993152
25.594194	1380.825645	15.998170
25.194389	1370.884592	16.003187
25.640376	1386.270118	16.008205
25.799879	1389.704734	16.013223
25.693959	1377.951829	16.018240
25.422485	1384.472038	16.023258
25.557113	1381.313444	16.028275
25.672638	1391.806779	16.033293
25.930982	1386.298345	16.038311
26.202941	1406.355004	16.043328
25.950388	1421.798536	16.048346
26.520224	1413.607122	16.053363
26.570035	1392.092476	16.058381
26.098074	1377.742002	16.063399
26.110838	1388.146926	16.068416
25.690488	1382.254603	16.073434
26.298183	1392.523428	16.078451
26.250461	1401.865864	16.083469
26.369432	1407.775228	16.088487
26.418033	1409.120580	16.093504
26.195902	1389.302671	16.098522
26.276020	1388.134032	16.103539
25.852059	1387.711044	16.108557
26.155520	1392.214931	16.113575
26.545886	1385.788722	16.118592
26.412224	1395.042230	16.123610
26.265511	1407.503279	16.128627
26.585040	1406.140385	16.133645
26.502067	1403.264442	16.138663
26.782428	1410.591692	16.143680
26.421982	1419.065749	16.148698
26.313618	1397.316074	16.153715
26.527448	1397.448463	16.158733
26.507254	1409.682354	16.163751
26.341364	1418.386110	16.168768
26.357620	1418.083145	16.173786
26.381735	1410.015078	16.178803
26.395728	1399.124129	16.183821
26.335031	1412.197007	16.188839
26.657842	1424.020959	16.193856
26.499449	1442.071394	16.198874
26.916305	1444.253331	16.203891
27.029801	1430.742757	16.208909
27.203910	1425.112139	16.213927
27.285468	1425.904039	16.218944
26.491122	1411.302547	16.223962
26.742044	1430.739232	16.228979
26.758662	1428.615158	16.233997
26.647792	1454.945171	16.239015
26.685275	1429.807234	16.244032
26.844768	1423.383245	16.249050
27.035959	1439.339455	16.254067
27.436551	1430.165990	16.259085
26.970233	1434.023256	16.264103
27.130134	1433.989794	16.269120
27.004016	1435.317084	16.274138
27.570438	1424.338466	16.279155
27.276582	1412.199657	16.284173
26.958344	1429.995947	16.289191
27.296559	1420.712645	16.294208
27.204713	1424.908723	16.299226
27.043703	1421.119306	16.304243
27.221023	1434.198332	16.309261
26.826179	1432.027318	16.314279
27.227345	1427.718223	16.319296
27.290367	1442.576477	16.324314
27.410359	1456.498373	16.329331
27.774600	1474.049479	16.334349
27.667841	1469.619531	16.339367
27.831028	1458.555690	16.344384
27.623423	1469.291312	16.349402
27.650650	1453.960047	16.354419
27.496168	1425.623752	16.359437
27.759073	1443.473297	16.364455
28.142615	1440.382390	16.369472
27.754353	1448.945491	16.374490
27.782782	1435.934000	16.379507
27.646770	1426.444088	16.384525
27.511126	1424.362594	16.389543
27.927896	1417.757934	16.394560
27.817956	1425.156184	16.399578
27.769256	1432.794262	16.404595
27.907054	1435.029891	16.409613
27.833926	1444.953391	16.414631
28.147814	1446.087916	16.419648
27.996752	1466.091752	16.424666
28.451536	1447.450890	16.429683
28.590980	1419.476769	16.434701
27.914954	1420.569021	16.439719
28.149234	1436.233033	16.444736
27.926355	1422.322448	16.449754
27.824029	1433.794907	16.454771
27.949305	1444.171436	16.459789
28.334709	1454.191276	16.464807
28.416060	1432.677363	16.469824
28.244176	1435.802957	16.474842
28.287981	1439.638213	16.479859
28.396327	1446.356155	16.484877
28.383589	1442.833110	16.489895
28.445011	1436.861249	16.494912
28.336291	1439.222735	16.499930
28.245817	1449.941447	16.504947
28.412310	1450.117282	16.509965
28.400190	1439.285923	16.514983
28.579817	1438.358553	16.520000
28.510974	1471.100492	16.525018
28.315893	1462.860201	16.530035
28.749045	1450.552216	16.535053
28.582810	1443.207362	16.540071
28.621638	1457.769205	16.545088
28.568475	1466.433498	16.550106
28.443695	1453.624831	16.555123
28.400848	1434.234516	16.560141
28.380066	1438.438928	16.565159
28.261015	1436.065385	16.570176
28.533116	1453.683258	16.575194
28.439890	1456.782966	16.580211
28.626139	1467.167344	16.585229
28.541533	1475.048136	16.590247
28.762449	1474.005993	16.595264
28.859010	1480.101921	16.600282
28.915063	1481.627800	16.605299
28.880325	1488.818126	16.610317
28.781848	1480.757487	16.615335
29.191720	1468.998883	16.620352
29.249470	1481.970670	16.625370
29.068293	1478.786407	16.630387
29.326963	1475.658465	16.635405
29.145022	1468.534650	16.640423
28.916497	1474.646807	16.645440
29.141312	1482.988954	16.650458
29.047838	1474.995095	16.655475
29.400107	1466.406435	16.660493
29.228344	1473.489309	16.665511
29.158975	1486.318462	16.670528
29.394190	1471.576883	16.675546
29.366710	1473.187317	16.680563
29.255857	1472.090182	16.685581
29.266035	1485.139503	16.690599
29.172633	1481.177418	16.695616
29.425807	1499.439669	16.700634
29.319494	1493.374468	16.705651
29.923369	1489.699525	16.710669
29.861207	1498.298113	16.715687
29.636777	1507.125250	16.720704
29.861241	1504.213046	16.725722
29.694125	1471.122023	16.730739
29.827321	1465.040673	16.735757
29.748447	1480.483510	16.740775
29.800564	1494.025305	16.745792
29.895838	1478.816303	16.750810
29.637065	1474.046890	16.755827
29.960088	1476.320109	16.760845
29.703214	1485.240961	16.765863
29.905692	1500.030763	16.770880
29.913220	1499.891900	16.775898
29.758962	1492.875483	16.780915
30.124792	1507.389534	16.785933
30.242163	1504.578080	16.790951
29.954724	1483.346055	16.795968
29.935291	1474.357206	16.800986
30.103612	1490.881691	16.806003
29.955914	1484.439165	16.811021
30.142389	1501.174689	16.816039
30.300303	1497.147944	16.821056
30.155943	1492.658666	16.826074
30.016539	1499.774976	16.831091
30.224275	1490.350435	16.836109
30.293201	1482.884731	16.841127
30.375228	1484.560909	16.846144
30.621866	1487.878022	16.851162
30.338586	1502.717005	16.856179
30.340336	1473.101437	16.861197
30.569786	1475.699007	16.866215
30.417847	1478.550113	16.871232
30.565874	1496.194739	16.876250
30.273917	1505.064424	16.881267
30.223034	1482.237843	16.886285
30.021681	1474.258860	16.891303
30.051138	1497.602240	16.896320
30.363526	1519.176440	16.901338
30.301461	1523.168356	16.906355
30.523167	1505.002756	16.911373
30.667623	1509.898031	16.916391
30.337315	1522.715033	16.921408
30.641189	1520.870570	16.926426
30.672058	1507.349081	16.931443
30.911434	1495.544238	16.936461
31.114771	1507.442121	16.941479
30.951599	1529.543054	16.946496
31.246447	1519.711371	16.951514
30.815590	1512.513734	16.956531
30.889559	1520.346892	16.961549
31.105362	1508.576833	16.966567
31.413017	1522.351562	16.971584
31.152342	1517.912397	16.976602
31.023523	1523.326454	16.981619
31.314557	1510.991720	16.986637
31.414646	1502.187782	16.991655
31.006412	1512.006306	16.996672
31.226906	1505.553997	17.001690
31.060307	1506.722566	17.006707
30.966968	1520.824034	17.011725
31.130658	1526.524227	17.016743
31.074380	1528.119647	17.021760
31.628699	1531.996912	17.026778
31.608213	1548.815301	17.031795
31.691113	1531.327978	17.036813
31.585719	1517.179139	17.041831
31.745750	1524.602198	17.046848
31.678631	1536.887341	17.051866
31.640586	1543.672225	17.056883
31.748029	1528.505937	17.061901
32.083604	1523.555335	17.066919
31.600719	1523.820082	17.071936
31.795505	1516.497109	17.076954
31.607968	1525.493909	17.081971
31.822916	1537.003759	17.086989
31.960041	1534.849227	17.092007
31.583704	1523.099371	17.097024
31.673869	1510.534503	17.102042
31.900906	1524.118073	17.107059
31.870614	1542.094811	17.112077
31.831571	1529.683239	17.117095
31.535132	1528.455387	17.122112
32.015793	1519.684984	17.127130
32.029948	1529.575418	17.132147
32.334554	1517.705559	17.137165
32.516093	1529.180874	17.142183
32.045052	1522.012605	17.147200
32.095275	1518.035337	17.152218
32.119405	1533.201911	17.157235
32.074222	1532.004864	17.162253
31.996094	1532.934257	17.167271
32.236983	1528.717944	17.172288
32.372055	1511.194272	17.177306
32.173392	1523.030576	17.182323
32.251977	1550.632312	17.187341
32.657233	1564.357492	17.192359
32.542851	1553.312292	17.197376
32.679758	1535.876360	17.202394
32.214671	1554.413933	17.207411
32.274154	1568.902601	17.212429
32.435758	1555.783192	17.217447
32.288704	1570.028789	17.222464
32.746798	1544.159487	17.227482
32.779838	1572.269762	17.232499
32.630425	1560.140128	17.237517
32.676730	1545.214585	17.242535
32.361190	1548.393364	17.247552
32.970459	1553.765363	17.252570
33.075771	1561.581553	17.257587
32.828043	1546.123425	17.262605
32.856544	1564.226763	17.267623
32.586504	1562.185566	17.272640
32.804390	1567.015685	17.277658
32.769788	1564.761012	17.282675
32.713916	1558.412312	17.287693
32.612019	1576.558370	17.292711
32.620574	1576.137507	17.297728
33.160353	1579.749528	17.302746
33.142570	1591.197704	17.307763
33.085012	1567.332459	17.312781
33.530530	1573.264481	17.317799
33.153633	1592.943184	17.322816
33.373365	1569.490676	17.327834
33.285212	1589.750854	17.332851
33.369875	1591.257648	17.337869
33.621748	1576.455255	17.342887
33.270948	1569.973044	17.347904
33.628318	1568.324514	17.352922
33.628839	1582.306023	17.357939
33.803040	1567.306775	17.362957
34.291779	1553.633809	17.367975
33.889822	1569.863138	17.372992
33.979407	1565.188261	17.378010
33.978760	1545.893072	17.383027
33.371851	1552.145823	17.388045
33.247758	1556.450393	17.393063
33.678046	1575.264738	17.398080
33.766877	1555.164173	17.403098
33.692095	1563.448319	17.408115
33.808140	1572.207321	17.413133
33.697955	1563.084826	17.418151
34.050881	1556.063682	17.423168
33.835985	1549.480889	17.428186
33.920346	1562.597626	17.433203
33.625655	1585.478282	17.438221
33.679738	1575.335638	17.443239
33.872172	1562.021799	17.448256
34.203894	1564.189975	17.453274
33.992142	1578.967124	17.458291
33.959882	1596.420741	17.463309
34.319768	1593.829769	17.468327
34.297954	1595.773559	17.473344
34.612332	1602.558091	17.478362
34.379490	1613.286964	17.483379
34.450483	1604.604188	17.488397
34.448784	1586.584736	17.493415
34.329287	1583.606059	17.498432
34.458086	1594.706264	17.503450
34.466014	1617.855691	17.508467
34.253325	1596.458235	17.513485
34.684630	1576.459576	17.518503
34.591352	1601.297785	17.523520
34.757813	1612.362947	17.528538
34.750374	1582.969996	17.533555
34.993493	1594.814631	17.538573
34.828072	1603.749861	17.543591
34.686531	1609.319463	17.548608
34.827158	1594.214343	17.553626
35.103329	1588.796179	17.558643
34.974954	1594.170924	17.563661
34.942569	1593.971248	17.568679
34.794661	1584.337270	17.573696
34.634355	1576.603070	17.578714
35.013450	1579.636165	17.583731
34.813825	1603.757070	17.588749
34.961248	1605.436822	17.593767
34.531183	1601.804593	17.598784
34.822610	1584.422681	17.603802
34.963486	1603.031496	17.608819
34.874171	1615.810620	17.613837
34.921504	1594.867139	17.618855
35.069761	1588.592938	17.623872
35.261130	1617.676131	17.628890
35.399220	1628.718047	17.633907
35.117847	1631.736111	17.638925
35.589309	1615.571097	17.643943
35.108938	1622.527025	17.648960
35.611514	1618.480094	17.653978
35.489321	1622.770494	17.658995
35.163031	1619.608902	17.664013
35.685161	1610.149554	17.669031
35.513848	1624.825104	17.674048
35.447154	1624.358420	17.679066
35.610113	1609.827720	17.684083
35.426605	1614.305968	17.689101
35.336911	1620.970611	17.694119
35.704709	1635.388711	17.699136
35.645455	1639.260434	17.704154
36.081993	1630.454159	17.709171
36.008154	1634.758318	17.714189
36.336887	1622.983385	17.719207
35.844976	1622.568863	17.724224
35.879284	1602.880506	17.729242
35.799780	1630.424769	17.734259
35.685451	1647.333364	17.739277
36.278081	1639.382600	17.744295
35.737248	1639.494851	17.749312
36.096043	1644.616604	17.754330
36.089763	1637.680270	17.759347
35.992104	1634.745896	17.764365
36.194753	1639.412253	17.769383
36.383794	1637.614700	17.774400
36.350391	1634.816232	17.779418
36.470279	1647.951182	17.784435
36.578625	1649.260507	17.789453
36.954331	1627.488568	17.794471
36.433040	1622.201979	17.799488
36.552225	1638.949758	17.804506
36.686814	1654.342930	17.809523
36.480519	1644.281548	17.814541
37.168329	1618.608953	17.819559
36.927799	1632.379706	17.824576
36.732022	1644.294743	17.829594
36.857520	1644.469384	17.834611
36.220172	1629.920164	17.839629
36.969094	1623.482232	17.844647
36.474782	1634.030162	17.849664
36.560942	1631.998778	17.854682
36.721805	1619.371066	17.859699
36.665524	1633.074963	17.864717
36.953930	1636.205027	17.869735
37.124936	1652.176603	17.874752
36.875633	1668.407969	17.879770
36.996690	1667.345610	17.884787
36.990827	1647.352089	17.889805
37.121013	1645.839696	17.894823
36.927250	1665.852817	17.899840
36.728222	1647.648232	17.904858
37.384080	1649.679999	17.909875
36.864451	1667.043504	17.914893
37.276561	1653.834987	17.919911
37.079511	1643.145044	17.924928
37.026130	1675.395301	17.929946
37.293557	1688.010928	17.934963
37.386765	1691.548478	17.939981
37.953904	1686.865007	17.944999
37.395747	1694.739047	17.950016
37.334303	1688.227960	17.955034
37.975419	1685.199635	17.960051
37.723268	1703.195020	17.965069
37.695098	1703.937661	17.970087
37.956220	1686.600003	17.975104
37.728574	1682.758750	17.980122
38.136243	1680.423789	17.985139
37.900826	1677.524669	17.990157
37.872142	1693.383157	17.995175
37.716828	1689.231192	18.000192
38.021830	1670.086084	18.005210
37.936044	1672.737356	18.010227
37.844973	1690.406465	18.015245
37.993825	1678.774283	18.020263
37.983663	1678.992893	18.025280
37.856583	1676.667283	18.030298
38.217563	1664.785338	18.035315
38.086542	1676.714005	18.040333
38.263035	1674.815787	18.045351
38.301458	1673.745238	18.050368
37.930130	1671.907732	18.055386
38.318652	1688.069831	18.060403
38.501698	1711.608976	18.065421
38.601218	1687.423748	18.070439
38.424510	1694.976637	18.075456
38.096539	1725.895988	18.080474
38.457072	1714.053539	18.085491
38.637724	1706.811044	18.090509
38.809046	1694.269221	18.095527
39.117756	1706.786131	18.100544
38.502245	1707.883456	18.105562
38.665913	1714.584502	18.110579
38.634325	1724.964905	18.115597
38.858682	1705.984032	18.120615
38.903327	1705.363836	18.125632
38.399373	1698.334162	18.130650
38.720129	1699.925549	18.135667
38.510944	1709.531125	18.140685
38.784666	1728.224220	18.145703
38.952453	1742.386458	18.150720
38.817258	1736.424241	18.155738
39.319786	1714.943263	18.160755
39.209638	1743.036380	18.165773
39.378415	1747.095303	18.170791
39.621166	1729.878522	18.175808
39.483578	1731.045757	18.180826
39.471397	1719.668159	18.185843
39.252272	1710.241303	18.190861
39.239521	1713.427842	18.195879
39.497975	1726.263049	18.200896
39.409600	1737.934177	18.205914
39.903379	1717.922747	18.210931
39.550833	1709.607283	18.215949
39.685407	1722.476735	18.220967
39.904608	1716.408332	18.225984
39.592812	1726.639215	18.231002
39.809915	1708.137098	18.236019
39.508150	1714.001761	18.241037
39.815981	1727.216230	18.246055
39.789337	1715.448783	18.251072
39.904167	1724.780200	18.256090
40.280494	1724.699165	18.261107
40.104263	1720.375487	18.266125
39.912237	1710.670094	18.271143
40.117426	1715.637075	18.276160
39.952342	1718.001423	18.281178
40.076555	1718.533587	18.286195
39.795308	1734.091995	18.291213
40.008379	1735.717319	18.296231
40.192657	1715.336849	18.301248
40.018207	1704.809530	18.306266
40.058407	1709.331726	18.311283
40.235872	1736.550702	18.316301
40.195597	1729.506286	18.321319
40.299364	1720.553712	18.326336
40.536116	1753.527783	18.331354
40.762340	1749.245245	18.336371
40.368207	1740.214145	18.341389
40.196111	1745.236891	18.346407
40.600446	1744.457470	18.351424
40.671181	1759.109386	18.356442
40.816240	1746.855366	18.361459
40.896229	1752.583450	18.366477
40.778247	1743.158752	18.371495
40.927687	1745.295377	18.376512
40.494596	1757.694510	18.381530
40.792593	1740.567681	18.386547
40.524749	1742.508553	18.391565
40.409120	1754.371659	18.396583
40.499890	1749.180789	18.401600
40.492560	1775.377435	18.406618
41.385109	1768.328131	18.411635
41.206875	1773.091716	18.416653
41.076558	1770.568241	18.421671
41.173383	1784.241756	18.426688
40.897190	1790.546129	18.431706
41.106819	1770.308218	18.436723
41.148164	1758.758786	18.441741
41.262959	1777.702471	18.446759
41.410089	1777.286256	18.451776
41.231574	1780.244151	18.456794
41.686606	1769.883477	18.461811
41.922698	1782.513611	18.466829
41.555579	1781.295843	18.471847
42.065420	1776.147204	18.476864
41.778031	1780.935226	18.481882
41.728860	1766.658484	18.486899
41.675254	1757.828726	18.491917
41.784081	1750.449782	18.496935
41.926180	1755.745642	18.501952
41.916089	1761.592433	18.506970
42.054844	1756.660210	18.511987
42.206207	1763.531879	18.517005
42.237365	1752.760849	18.522023
42.105771	1755.038583	18.527040
42.257142	1764.764790	18.532058
42.168562	1776.427322	18.537075
42.239626	1761.905662	18.542093
42.112400	1749.280479	18.547111
42.237838	1749.233228	18.552128
42.331131	1773.357756	18.557146
42.500078	1764.419577	18.562163
42.454508	1751.059096	18.567181
42.410753	1756.296711	18.572199
42.714234	1759.541904	18.577216
42.361577	1752.976867	18.582234
42.296654	1757.150283	18.587251
42.188303	1765.950907	18.592269
42.213943	1770.230694	18.597287
42.568964	1758.788942	18.602304
42.101106	1792.953236	18.607322
42.404834	1796.141617	18.612339
42.625225	1792.416120	18.617357
42.534659	1779.367222	18.622375
42.433064	1779.841840	18.627392
42.536159	1786.247772	18.632410
42.232909	1802.957293	18.637427
42.774593	1812.652489	18.642445
42.944979	1831.165483	18.647463
43.098140	1820.020673	18.652480
43.059169	1814.186195	18.657498
43.366816	1807.933784	18.662515
43.480848	1820.389769	18.667533
42.916704	1827.430681	18.672551
43.166827	1811.157481	18.677568
43.290275	1805.842219	18.682586
43.296160	1810.742384	18.687603
43.391819	1797.508986	18.692621
43.264209	1803.945375	18.697639
43.747106	1823.697896	18.702656
43.518987	1835.537734	18.707674
43.754634	1807.744998	18.712691
44.089205	1796.066783	18.717709
43.823335	1812.214245	18.722727
43.641220	1806.603681	18.727744
44.020199	1792.000701	18.732762
43.713261	1782.753140	18.737779
43.958216	1799.800916	18.742797
44.038017	1816.330344	18.747815
43.839218	1799.994952	18.752832
44.099536	1791.216918	18.757850
44.149656	1788.993970	18.762867
44.108229	1792.615788	18.767885
43.785846	1789.243911	18.772903
43.858180	1803.068114	18.777920
44.043062	1815.231832	18.782938
44.307684	1831.159096	18.787955
44.608132	1828.489737	18.792973
44.462036	1843.496892	18.797991
44.742251	1824.965705	18.803008
44.366450	1808.218499	18.808026
44.231993	1813.556341	18.813043
44.691193	1827.479398	18.818061
44.544112	1839.200159	18.823079
44.648889	1827.765759	18.828096
44.368152	1818.006861	18.833114
44.496768	1821.112887	18.838131
44.737758	1813.900717	18.843149
44.362334	1805.502777	18.848167
44.750853	1810.860276	18.853184
44.841263	1822.786907	18.858202
44.497662	1834.356023	18.863219
44.898647	1814.134256	18.868237
44.454574	1801.419489	18.873255
44.586124	1832.259084	18.878272
44.864886	1856.712766	18.883290
44.839292	1863.745686	18.888307
45.372974	1838.422048	18.893325
45.523647	1837.422291	18.898343
45.380140	1840.858962	18.903360
45.352977	1857.596329	18.908378
45.329790	1853.016659	18.913395
45.532229	1845.273549	18.918413
45.201348	1843.940064	18.923431
45.707196	1842.310663	18.928448
45.397360	1855.609207	18.933466
45.236099	1848.667784	18.938483
45.504700	1834.035179	18.943501
45.113567	1839.557348	18.948519
45.390901	1834.632705	18.953536
45.391013	1851.466818	18.958554
45.253256	1854.157709	18.963571
45.717132	1852.397670	18.968589
45.753304	1870.034052	18.973607
45.868699	1875.648872	18.978624
45.824219	1851.713908	18.983642
45.398501	1847.187770	18.988659
46.157840	1852.750193	18.993677
45.842729	1870.533781	18.998695
46.066315	1843.176649	19.003712
46.273838	1850.991645	19.008730
46.411323	1871.249154	19.013747
46.407617	1860.411874	19.018765
46.214649	1865.186582	19.023783
46.555161	1855.667450	19.028800
46.392644	1851.902185	19.033818
46.258820	1860.421597	19.038835
46.366711	1860.201296	19.043853
46.331351	1883.304449	19.048871
46.489381	1898.242310	19.053888
46.810359	1894.741951	19.058906
46.487742	1911.470437	19.063923
46.410559	1888.337026	19.068941
46.776049	1891.632520	19.073959
46.839206	1877.306213	19.078976
46.569247	1887.852864	19.083994
46.710303	1889.954977	19.089011
46.952406	1890.938833	19.094029
46.778699	1894.888283	19.099047
46.825840	1897.816586	19.104064
47.127238	1913.469406	19.109082
47.085208	1915.773004	19.114099
47.231271	1922.716277	19.119117
47.007966	1916.740208	19.124135
47.182247	1907.692719	19.129152
47.342196	1909.847509	19.134170
47.209058	1920.193555	19.139187
47.617655	1900.556427	19.144205
47.650385	1906.840599	19.149223
47.542693	1905.396225	19.154240
47.702344	1910.870797	19.159258
47.613142	1894.794009	19.164275
47.883669	1895.408869	19.169293
48.105046	1909.957311	19.174311
47.929889	1898.256679	19.179328
47.962503	1909.496409	19.184346
47.578727	1912.786125	19.189363
47.931952	1900.895241	19.194381
47.857599	1910.113673	19.199399
47.750177	1903.481279	19.204416
48.022099	1903.577505	19.209434
47.683429	1909.578041	19.214451
47.829756	1891.586711	19.219469
48.180935	1884.390643	19.224487
47.781731	1914.559106	19.229504
48.224828	1941.106914	19.234522
47.962693	1938.840681	19.239539
48.155412	1914.921135	19.244557
48.369290	1921.714546	19.249575
48.349657	1951.895540	19.254592
48.188960	1949.511479	19.259610
47.919261	1926.523975	19.264627
48.484667	1935.991358	19.269645
48.630174	1955.886501	19.274663
48.667287	1945.971570	19.279680
48.630587	1950.711722	19.284698
49.047209	1954.925672	19.289715
49.105231	1956.663437	19.294733
48.821420	1967.800805	19.299751
49.054916	1963.350897	19.304768
49.367455	1947.473461	19.309786
48.802158	1950.494616	19.314803
49.134536	1939.288120	19.319821
49.121136	1959.706087	19.324839
48.845504	1950.166002	19.329856
49.411155	1936.961490	19.334874
49.138269	1951.937647	19.339891
49.498267	1956.553891	19.344909
49.457084	1956.299475	19.349927
49.451967	1958.113410	19.354944
49.863269	1958.282747	19.359962
49.287076	1963.791848	19.364979
49.451876	1941.392336	19.369997
49.470660	1932.166533	19.375015
49.441731	1953.490822	19.380032
49.719618	1959.209111	19.385050
49.542659	1955.016957	19.390067
49.542335	1928.222068	19.395085
49.595013	1949.527355	19.400103
49.611967	1951.038978	19.405120
49.925121	1953.030491	19.410138
49.648240	1976.606095	19.415155
49.944081	1987.304544	19.420173
49.801106	1969.537965	19.425191
49.933216	1975.958470	19.430208
50.341357	1981.238195	19.435226
49.722963	1996.517802	19.440243
49.873927	1981.700303	19.445261
50.250885	1969.544765	19.450279
50.278183	1991.389440	19.455296
50.477830	2000.310824	19.460314
50.398630	1999.028040	19.465331
50.594753	1993.535872	19.470349
50.745295	2003.256071	19.475367
50.695403	1996.439851	19.480384
50.764253	2003.758352	19.485402
50.829128	2006.903094	19.490419
51.020612	2003.022610	19.495437
50.877412	2004.713628	19.500455
50.773182	2002.163761	19.505472
50.942691	2000.033926	19.510490
50.894468	1992.282468	19.515507
51.045149	1996.693891	19.520525
50.746316	2000.954247	19.525543
51.003775	1986.328062	19.530560
51.172138	1974.464423	19.535578
51.175123	1992.043646	19.540595
51.000161	1991.833675	19.545613
51.519881	2011.271160	19.550631
51.527945	2033.262550	19.555648
51.364605	2010.662387	19.560666
51.496359	2020.492867	19.565683
51.603946	2025.516425	19.570701
51.758987	2019.181982	19.575719
51.628815	2022.481082	19.580736
52.003911	2019.843048	19.585754
52.063461	2025.639954	19.590771
52.117314	2001.832574	19.595789
51.844692	1993.778990	19.600807
51.612082	1980.862230	19.605824
51.815083	1983.748655	19.610842
51.770151	1995.864389	19.615859
51.764817	2020.949129	19.620877
52.152791	2022.059845	19.625895
51.870112	2011.400031	19.630912
51.886040	2017.653272	19.635930
52.077564	2026.459205	19.640947
52.211737	2006.815134	19.645965
52.176047	2002.060156	19.650983
51.822315	2026.088808	19.656000
52.477998	2036.442743	19.661018
52.581577	2028.103294	19.666035
52.366446	2029.806300	19.671053
52.941786	2046.547538	19.676071
53.057578	2047.427203	19.681088
52.766124	2044.962096	19.686106
52.779048	2030.594743	19.691123
52.770334	2039.133040	19.696141
52.705107	2042.168998	19.701159
52.749530	2037.748148	19.706176
52.703492	2031.145999	19.711194
53.132356	2024.473347	19.716211
52.874747	2044.970949	19.721229
52.963185	2048.739742	19.726247
52.997427	2056.239939	19.731264
53.193542	2028.140402	19.736282
53.137548	2028.018723	19.741299
52.826272	2040.930138	19.746317
53.136679	2062.706382	19.751335
53.248245	2051.506281	19.756352
53.521954	2060.379248	19.761370
53.700913	2076.755096	19.766387
53.730535	2083.607763	19.771405
53.742488	2063.064594	19.776423
53.421946	2052.095318	19.781440
54.128500	2062.491446	19.786458
53.731890	2082.656228	19.791475
53.472282	2078.140260	19.796493
53.818260	2062.590682	19.801511
53.782351	2059.758599	19.806528
53.665928	2090.019824	19.811546
54.040392	2107.146327	19.816563
54.083476	2104.116865	19.821581
54.217739	2092.623075	19.826599
54.205782	2109.581294	19.831616
54.821012	2082.145240	19.836634
54.653751	2077.907659	19.841651
54.740993	2094.323875	19.846669
54.570295	2085.098392	19.851687
54.333500	2074.373481	19.856704
54.882280	2078.156547	19.861722
54.679838	2090.261482	19.866739
54.661075	2083.437422	19.871757
54.702107	2073.639554	19.876775
54.544602	2089.671189	19.881792
54.569396	2081.854185	19.886810
54.575740	2075.225550	19.891827
54.612596	2087.049642	19.896845
54.805316	2093.410977	19.901863
54.760575	2110.334267	19.906880
54.991199	2110.248083	19.911898
55.323417	2107.586514	19.916915
55.041110	2117.383825	19.921933
55.203296	2125.081870	19.926951
55.068969	2105.995435	19.931968
55.282731	2108.834740	19.936986
55.307254	2122.776955	19.942003
55.502649	2130.821322	19.947021
55.699368	2102.447681	19.952039
55.344922	2116.077779	19.957056
55.146537	2113.750108	19.962074
55.617223	2105.855373	19.967091
55.267281	2125.725149	19.972109
55.573386	2141.917192	19.977127
55.591184	2135.458655	19.982144
55.703674	2120.951164	19.987162
55.965283	2129.045010	19.992179
55.902689	2143.064719	19.997197
56.064561	2133.714675	20.002215
56.145042	2140.301331	20.007232
56.035916	2127.638895	20.012250
56.326163	2141.413517	20.017267
56.040101	2170.282122	20.022285
56.358835	2167.022976	20.027303
56.401950	2166.179432	20.032320
56.399857	2161.818388	20.037338
56.724520	2166.783980	20.042355
56.575870	2172.581986	20.047373
57.109670	2157.649488	20.052391
56.823322	2153.809943	20.057408
57.089121	2169.259201	20.062426
57.199203	2170.190694	20.067443
56.950606	2151.532560	20.072461
57.132650	2143.484753	20.077479
56.798035	2128.654949	20.082496
56.969159	2134.922348	20.087514
57.224730	2161.088216	20.092531
57.102468	2164.504817	20.097549
57.544431	2151.067654	20.102567
57.352116	2138.582706	20.107584
57.126922	2147.556077	20.112602
57.369881	2172.757881	20.117619
57.168083	2159.030017	20.122637
56.721616	2172.195830	20.127655
57.298850	2168.565283	20.132672
57.162373	2162.929333	20.137690
57.371415	2172.288164	20.142707
57.273691	2204.483191	20.147725
57.633049	2189.704270	20.152743
57.463652	2178.501794	20.157760
57.585832	2182.771550	20.162778
57.757423	2193.429073	20.167795
57.480641	2222.572966	20.172813
58.146289	2211.489319	20.177831
58.324489	2203.212628	20.182848
58.227136	2210.628268	20.187866
58.443808	2212.570514	20.192883
58.301407	2222.281987	20.197901
58.490017	2222.449848	20.202919
58.526175	2231.509388	20.207936
58.702735	2215.522674	20.212954
58.825781	2195.856484	20.217971
59.007267	2213.192425	20.222989
58.882588	2213.258836	20.228007
58.818514	2223.784094	20.233024
58.977279	2210.542077	20.238042
58.870674	2189.595569	20.243059
58.514942	2197.197280	20.248077
59.023187	2195.820947	20.253095
59.056118	2203.714967	20.258112
58.858831	2208.959311	20.263130
58.814710	2219.843214	20.268147
58.612739	2214.338715	20.273165
58.952279	2193.901741	20.278183
58.751535	2206.932408	20.283200
59.205922	2223.748248	20.288218
59.565364	2220.318908	20.293235
59.118582	2228.853927	20.298253
59.017347	2239.603114	20.303271
59.044301	2233.930388	20.308288
59.100819	2225.206944	20.313306
59.499067	2225.115791	20.318323
59.538272	2252.184152	20.323341
59.421157	2242.699466	20.328359
59.532082	2239.170564	20.333376
59.361606	2257.959360	20.338394
59.894948	2275.280527	20.343411
59.632849	2271.337946	20.348429
59.881936	2247.429628	20.353447
60.116333	2264.261496	20.358464
59.968601	2292.244625	20.363482
60.270147	2297.195184	20.368499
60.201384	2280.091164	20.373517
60.742632	2274.602681	20.378535
60.366768	2280.836436	20.383552
60.515500	2298.093255	20.388570
60.882174	2281.162118	20.393587
60.600677	2268.368923	20.398605
60.641653	2255.154205	20.403623
60.871968	2260.645568	20.408640
60.748399	2285.475817	20.413658
60.958217	2266.898260	20.418675
61.006028	2272.324133	20.423693
60.853184	2272.044568	20.428711
60.992230	2274.979602	20.433728
60.824861	2278.543718	20.438746
61.212609	2265.690515	20.443763
61.156049	2278.850441	20.448781
60.892774	2296.761267	20.453799
60.976944	2299.356614	20.458816
61.241403	2299.958718	20.463834
61.586385	2281.480046	20.468851
61.129519	2298.276208	20.473869
61.635430	2309.051076	20.478887
61.335395	2317.653808	20.483904
61.580888	2310.347961	20.488922
61.818731	2301.568432	20.493939
61.912265	2315.149968	20.498957
61.732591	2323.972538	20.503975
61.909500	2331.360234	20.508992
62.021019	2332.987644	20.514010
62.197531	2315.483859	20.519027
62.101612	2338.888209	20.524045
62.466274	2333.294460	20.529063
62.489954	2316.013142	20.534080
62.481878	2319.761342	20.539098
62.819507	2317.845866	20.544115
62.700630	2302.105586	20.549133
62.415195	2308.977055	20.554151
62.779713	2308.063859	20.559168
62.448428	2310.160043	20.564186
62.954984	2304.030344	20.569203
62.654026	2325.179961	20.574221
62.718037	2335.377783	20.579239
62.533720	2321.281295	20.584256
62.403279	2307.766960	20.589274
62.766379	2314.420257	20.594291
62.931268	2359.139418	20.599309
62.867312	2353.232893	20.604327
63.288651	2342.706172	20.609344
63.036472	2348.898260	20.614362
63.121930	2341.896357	20.619379
63.005694	2339.043448	20.624397
62.947182	2336.997597	20.629415
63.570187	2363.789495	20.634432
63.637071	2364.853905	20.639450
63.689223	2351.913787	20.644467
63.658943	2377.195228	20.649485
63.999091	2378.476250	20.654503
64.003559	2375.647278	20.659520
63.840016	2382.013677	20.664538
63.558983	2366.915972	20.669555
63.729582	2366.660109	20.674573
63.655014	2356.437733	20.679591
64.036160	2354.871499	20.684608
63.994396	2384.487998	20.689626
64.354735	2376.528206	20.694643
63.848639	2359.879177	20.699661
64.203039	2361.555810	20.704679
64.480924	2386.434824	20.709696
64.171259	2409.938963	20.714714
64.619144	2399.345819	20.719731
64.767996	2388.704279	20.724749
65.027982	2398.641842	20.729767
65.174919	2389.626144	20.734784
64.676954	2399.211673	20.739802
65.032723	2395.947934	20.744819
65.150638	2395.853508	20.749837
65.148808	2396.192189	20.754855
65.249652	2385.636525	20.759872
64.914149	2376.588567	20.764890
65.026838	2385.686035	20.769907
64.841498	2395.124050	20.774925
64.924766	2393.988864	20.779943
65.280358	2380.159345	20.784960
65.169714	2410.576913	20.789978
65.231892	2420.683770	20.794995
65.519389	2425.904367	20.800013
65.405374	2415.859703	20.805031
65.786061	2405.753371	20.810048
65.516923	2411.186990	20.815066
65.582287	2419.973059	20.820083
65.317020	2431.332858	20.825101
65.569635	2429.814033	20.830119
66.381313	2442.570822	20.835136
65.736130	2449.596866	20.840154
66.243489	2447.684621	20.845171
66.092538	2453.450638	20.850189
66.410691	2449.826823	20.855207
66.639050	2423.242749	20.860224
66.544690	2443.643345	20.865242
66.795362	2432.963298	20.870259
66.726473	2436.439928	20.875277
66.571761	2445.037218	20.880295
66.740070	2454.309168	20.885312
66.711082	2445.449064	20.890330
66.883589	2448.997403	20.895347
66.704371	2467.320650	20.900365
67.120474	2472.388930	20.905383
67.316205	2457.003131	20.910400
66.922556	2463.393418	20.915418
67.278242	2455.482377	20.920435
67.190734	2442.876433	20.925453
67.377162	2462.617956	20.930471
67.294552	2465.214321	20.935488
67.565625	2477.161599	20.940506
67.256052	2461.640039	20.945523
67.671135	2452.004691	20.950541
67.634706	2467.165073	20.955559
67.553654	2456.247550	20.960576
67.561835	2456.713889	20.965594
67.784324	2469.618056	20.970611
68.073014	2482.915169	20.975629
67.816991	2507.986136	20.980647
68.247129	2510.914446	20.985664
68.180069	2498.235599	20.990682
68.037199	2479.646393	20.995699
68.381874	2494.477331	21.000717
68.403725	2503.230881	21.005735
68.450047	2482.554227	21.010752
68.361361	2486.071142	21.015770
68.308200	2489.936463	21.020787
68.375415	2497.513009	21.025805
68.415350	2500.216078	21.030823
68.475776	2479.840595	21.035840
68.343614	2474.343262	21.040858
68.323489	2498.259460	21.045875
68.365902	2527.483250	21.050893
68.278813	2525.711544	21.055911
68.719940	2520.915008	21.060928
68.718559	2531.088731	21.065946
68.885513	2539.231995	21.070963
69.473330	2551.497406	21.075981
69.198732	2540.657469	21.080999
69.559639	2528.029709	21.086016
69.377317	2526.832513	21.091034
69.514809	2545.198582	21.096051
69.647373	2531.516985	21.101069
69.372184	2542.285682	21.106087
69.730461	2537.785860	21.111104
69.751039	2536.996209	21.116122
69.845882	2535.855361	21.121139
70.302612	2548.211908	21.126157
70.157610	2570.134985	21.131175
70.443811	2574.144415	21.136192
70.096836	2556.331449	21.141210
70.239364	2556.871442	21.146227
70.482566	2555.923957	21.151245
70.155952	2551.874068	21.156263
70.212746	2541.144107	21.161280
70.339141	2558.800126	21.166298
70.640087	2572.336397	21.171315
70.799055	2559.120224	21.176333
70.648230	2544.615104	21.181351
70.755072	2540.908882	21.186368
70.753459	2557.488778	21.191386
70.550330	2568.695123	21.196403
70.862389	2569.218124	21.201421
70.896239	2591.659429	21.206439
71.068704	2597.827893	21.211456
71.097261	2595.146256	21.216474
71.265477	2591.182475	21.221491
71.406381	2598.328058	21.226509
71.353110	2586.424108	21.231527
71.781397	2581.335231	21.236544
71.479223	2589.007897	21.241562
71.158909	2599.947846	21.246579
71.755588	2592.743455	21.251597
72.085281	2601.606403	21.256615
71.788924	2598.870795	21.261632
71.904886	2609.709330	21.266650
71.770726	2611.059698	21.271667
72.041321	2599.204173	21.276685
71.991302	2590.976698	21.281703
72.272300	2604.786726	21.286720
71.946961	2620.151080	21.291738
71.935971	2605.688730	21.296755
72.229037	2601.851538	21.301773
72.422680	2610.350809	21.306791
72.576776	2619.816913	21.311808
72.600481	2636.278553	21.316826
72.706303	2632.206980	21.321843
72.700868	2612.196090	21.326861
73.008292	2629.308374	21.331879
73.105345	2635.337763	21.336896
73.126904	2629.556743	21.341914
73.227323	2606.585490	21.346931
73.596771	2609.709845	21.351949
73.341789	2619.489181	21.356967
73.280248	2622.025799	21.361984
73.371281	2629.528603	21.367002
73.444448	2611.200344	21.372019
73.477396	2605.691230	21.377037
72.965608	2621.205472	21.382055
73.319084	2615.386929	21.387072
73.621891	2627.705404	21.392090
73.171970	2633.293563	21.397107
73.730535	2640.507923	21.402125
73.621322	2643.892853	21.407143
73.841330	2641.765902	21.412160
73.564107	2639.990765	21.417178
73.458516	2658.283178	21.422195
73.811403	2665.469539	21.427213
74.089235	2670.058247	21.432231
74.315384	2679.661672	21.437248
74.593083	2677.125241	21.442266
74.197611	2678.603036	21.447283
74.444651	2685.553588	21.452301
74.221506	2681.190939	21.457319
74.540843	2692.366739	21.462336
75.004120	2698.009893	21.467354
74.714345	2709.195034	21.472371
75.064981	2709.597901	21.477389
74.959438	2698.498256	21.482407
75.216060	2677.547057	21.487424
75.286696	2689.504988	21.492442
75.077447	2695.634615	21.497459
75.696420	2677.936258	21.502477
75.356898	2681.319888	21.507495
75.192326	2688.591967	21.512512
75.563421	2704.205442	21.517530
75.493350	2706.600591	21.522547
75.598678	2694.995106	21.527565
75.808720	2716.257837	21.532583
75.792951	2710.310735	21.537600
76.200542	2725.123824	21.542618
75.955962	2730.290148	21.547635
76.340779	2722.885504	21.552653
75.974983	2732.294694	21.557671
76.081205	2715.511617	21.562688
76.513410	2712.790222	21.567706
76.166585	2732.334424	21.572723
76.296839	2726.622205	21.577741
75.993628	2722.150745	21.582759
76.323473	2746.729279	21.587776
76.637982	2755.984929	21.592794
76.673651	2741.573591	21.597811
76.830214	2735.516911	21.602829
76.809826	2748.677363	21.607847
76.722144	2750.666627	21.612864
76.895558	2753.494514	21.617882
76.838002	2765.288673	21.622899
77.219167	2764.694901	21.627917
77.297390	2774.082509	21.632935
77.277022	2786.575758	21.637952
77.678622	2783.702540	21.642970
77.468078	2773.626354	21.647987
77.632891	2762.718569	21.653005
77.433730	2773.636455	21.658023
77.430727	2779.257689	21.663040
77.594867	2770.325725	21.668058
77.443733	2795.156037	21.673075
78.217337	2796.536116	21.678093
77.747919	2796.589524	21.683111
77.854167	2793.153185	21.688128
78.300858	2802.907620	21.693146
78.144313	2809.486198	21.698163
78.196366	2798.613948	21.703181
78.157881	2794.896448	21.708199
78.373902	2811.248160	21.713216
78.577156	2810.297027	21.718234
78.652884	2831.432133	21.723251
78.736108	2826.870607	21.728269
78.965351	2834.662835	21.733287
78.817563	2815.225132	21.738304
78.980006	2808.547456	21.743322
78.968606	2824.660619	21.748339
78.957077	2828.541779	21.753357
79.018385	2831.690922	21.758375
78.847656	2822.471790	21.763392
79.191743	2814.327475	21.768410
79.115436	2842.739113	21.773427
79.573381	2838.316620	21.778445
79.711435	2841.504651	21.783463
79.647216	2855.107025	21.788480
79.799361	2857.660923	21.793498
79.585400	2846.382853	21.798515
79.942980	2862.411464	21.803533
80.104142	2842.698096	21.808551
80.091603	2852.889621	21.813568
80.138702	2867.689397	21.818586
80.068854	2891.732124	21.823603
80.135551	2877.155513	21.828621
80.578836	2877.740295	21.833639
80.590781	2870.592644	21.838656
80.742399	2881.593961	21.843674
80.511903	2892.498804	21.848691
80.667097	2879.597901	21.853709
80.518808	2877.488084	21.858727
80.790621	2875.917822	21.863744
80.958755	2884.522039	21.868762
81.071010	2893.658064	21.873779
81.388904	2903.535408	21.878797
81.293545	2904.723307	21.883815
81.164060	2896.429873	21.888832
81.558434	2887.629656	21.893850
81.428233	2883.926503	21.898867
81.595721	2895.422388	21.903885
81.776678	2891.291880	21.908903
81.594483	2882.869582	21.913920
81.765580	2864.039076	21.918938
81.337618	2891.773971	21.923955
81.550882	2912.947477	21.928973
82.112760	2908.812672	21.933991
82.113347	2900.710116	21.939008
82.307469	2915.513592	21.944026
82.195961	2910.893483	21.949043
82.270088	2908.325702	21.954061
82.676512	2917.919957	21.959079
82.394111	2926.198697	21.964096
82.694535	2925.582243	21.969114
82.552629	2921.764691	21.974131
82.725485	2922.897838	21.979149
82.836011	2920.952701	21.984167
82.574320	2923.983801	21.989184
82.569382	2944.966272	21.994202
83.009450	2960.314509	21.999219
83.202555	2953.396497	22.004237
83.219589	2940.450075	22.009255
82.950418	2942.067239	22.014272
83.248495	2939.270540	22.019290
83.131889	2940.144080	22.024307
83.669416	2957.933381	22.029325
83.675258	2965.451805	22.034343
83.872160	2970.627134	22.039360
84.050517	2965.658754	22.044378
83.871354	2979.410530	22.049395
83.796892	2973.792474	22.054413
83.783887	2963.656359	22.059431
84.037313	2977.204383	22.064448
84.135049	2955.438417	22.069466
83.855835	2950.280135	22.074483
84.324850	2974.997238	22.079501
84.460262	2981.874452	22.084519
84.500347	2986.588359	22.089536
84.631829	2976.156346	22.094554
84.529328	2978.922008	22.099571
84.361682	2975.859982	22.104589
84.658574	2967.213016	22.109607
84.701502	2995.665068	22.114624
84.827379	3017.627671	22.119642
84.816672	3020.900550	22.124659
84.678259	3004.776997	22.129677
84.865943	3019.778660	22.134695
85.012813	3044.991575	22.139712
85.480724	3032.185505	22.144730
85.397923	3037.927291	22.149747
85.809309	3032.366314	22.154765
85.936033	3027.233632	22.159783
85.469542	3046.722621	22.164800
85.847644	3024.666556	22.169818
86.279741	3054.973273	22.174835
86.240861	3084.678231	22.179853
86.608686	3070.864575	22.184871
86.255602	3063.211078	22.189888
86.260454	3057.888314	22.194906
86.430921	3081.451126	22.199923
86.509493	3075.018664	22.204941
86.782830	3061.592436	22.209959
86.602316	3063.364431	22.214976
86.371080	3073.147608	22.219994
86.713024	3066.040796	22.225011
86.532730	3057.599193	22.230029
86.860146	3067.725828	22.235047
86.981919	3081.887559	22.240064
86.937120	3103.668866	22.245082
86.990574	3094.181647	22.250099
86.720167	3075.990900	22.255117
87.491499	3099.362925	22.260135
87.425006	3125.330830	22.265152
87.500369	3118.344022	22.270170
87.730464	3121.358061	22.275187
87.787974	3132.498323	22.280205
87.626026	3113.148400	22.285223
87.696314	3110.025772	22.290240
88.043132	3125.179371	22.295258
88.297994	3152.179135	22.300275
88.081473	3153.368376	22.305293
88.492509	3139.742378	22.310311
88.733114	3137.033874	22.315328
88.922337	3136.644819	22.320346
88.774948	3139.534253	22.325363
88.745797	3137.605477	22.330381
88.921615	3127.886623	22.335399
88.562088	3138.911376	22.340416
88.817262	3139.625864	22.345434
88.802336	3144.827793	22.350451
88.905207	3142.692575	22.355469
89.211323	3158.965407	22.360487
89.272959	3169.910548	22.365504
89.158142	3153.086365	22.370522
89.300058	3161.909218	22.375539
89.135400	3168.334780	22.380557
89.426914	3176.136575	22.385575
89.542946	3179.240135	22.390592
89.996423	3174.936581	22.395610
89.841099	3190.803270	22.400627
89.623933	3206.990003	22.405645
89.928030	3196.046299	22.410663
89.881455	3187.052862	22.415680
89.888819	3180.155403	22.420698
90.212016	3193.177381	22.425715
90.370074	3202.404042	22.430733
90.679860	3215.351098	22.435751
90.653435	3211.840537	22.440768
90.771846	3211.978087	22.445786
90.572269	3225.416364	22.450803
90.652115	3234.903580	22.455821
91.021736	3212.329414	22.460839
90.868887	3210.739932	22.465856
91.123748	3234.242975	22.470874
91.476744	3253.431864	22.475891
91.217612	3251.928438	22.480909
91.676897	3221.941405	22.485927
91.446961	3234.525153	22.490944
91.740867	3234.885252	22.495962
91.870608	3243.673160	22.500979
91.446222	3251.289781	22.505997
92.025494	3234.237244	22.511015
91.756373	3241.812260	22.516032
92.005060	3260.329294	22.521050
91.937159	3264.525557	22.526067
91.799964	3280.331277	22.531085
92.149059	3275.793198	22.536103
92.062874	3272.633998	22.541120
92.126432	3270.149785	22.546138
92.560753	3291.375463	22.551155
92.651244	3300.672003	22.556173
92.909145	3283.241262	22.561191
92.630056	3294.761638	22.566208
92.754213	3297.987687	22.571226
93.055364	3300.440667	22.576243
93.101566	3320.111000	22.581261
93.311373	3327.424259	22.586279
93.557573	3329.953247	22.591296
93.840986	3318.807384	22.596314
93.578070	3311.240034	22.601331
93.519012	3323.071084	22.606349
93.740401	3329.090435	22.611367
93.762083	3324.720607	22.616384
93.907336	3321.800487	22.621402
93.911211	3313.813694	22.626419
93.666691	3338.609136	22.631437
94.030674	3341.478666	22.636455
94.214317	3344.453187	22.641472
94.270043	3353.837779	22.646490
94.715213	3345.568817	22.651507
94.336739	3344.485456	22.656525
94.843752	3354.064938	22.661543
94.781777	3364.260246	22.666560
95.139949	3382.312135	22.671578
95.136417	3380.448380	22.676595
95.386791	3376.977467	22.681613
95.302738	3372.816221	22.686631
95.222158	3369.447237	22.691648
95.336928	3358.534310	22.696666
95.730169	3351.181317	22.701683
95.537655	3370.481753	22.706701
95.493114	3369.559330	22.711719
95.407160	3379.433249	22.716736
95.504204	3368.286653	22.721754
95.730503	3381.850933	22.726771
95.695191	3374.275270	22.731789
95.930705	3365.272710	22.736807
95.965905	3391.415578	22.741824
95.646893	3400.312372	22.746842
95.962066	3398.100704	22.751859
96.054939	3391.042381	22.756877
96.295190	3415.340558	22.761895
96.453609	3432.952331	22.766912
96.468815	3428.513077	22.771930
96.925394	3420.495316	22.776947
96.522269	3420.421637	22.781965
97.112865	3441.694133	22.786983
97.289329	3462.564269	22.792000
97.263696	3456.896830	22.797018
97.688049	3438.427085	22.802035
97.418186	3430.858265	22.807053
97.360385	3442.695301	22.812071
97.529706	3444.427245	22.817088
97.737868	3443.405388	22.822106
97.884284	3442.871249	22.827123
97.660137	3462.926761	22.832141
97.834229	3477.191026	22.837159
98.290763	3467.333652	22.842176
98.183459	3462.065892	22.847194
98.278903	3473.423143	22.852211
98.261327	3475.947125	22.857229
98.355827	3475.668982	22.862247
98.400589	3482.862555	22.867264
98.346117	3488.381145	22.872282
98.705287	3481.347078	22.877299
98.623861	3482.126653	22.882317
98.695555	3485.805465	22.887335
99.087626	3509.560442	22.892352
99.288696	3520.562312	22.897370
99.670558	3510.702487	22.902387
99.738947	3514.927276	22.907405
99.586467	3533.803226	22.912423
99.677970	3527.867608	22.917440
99.893504	3518.548604	22.922458
99.955504	3508.868002	22.927475
100.096336	3513.928579	22.932493
100.066560	3527.286899	22.937511
100.039828	3513.403019	22.942528
99.774060	3501.855494	22.947546
100.294123	3515.590424	22.952563
100.334196	3530.847075	22.957581
100.137692	3549.810628	22.962599
100.707728	3542.971788	22.967616
100.291563	3540.969129	22.972634
100.462686	3539.974448	22.977651
100.468935	3555.483542	22.982669
100.670683	3553.347676	22.987687
100.680348	3582.165724	22.992704
100.749088	3594.466571	22.997722
101.025983	3583.333405	23.002739
101.169699	3589.124965	23.007757
100.906564	3599.721158	23.012775
101.458035	3611.133853	23.017792
101.566107	3625.035376	23.022810
101.751387	3597.813342	23.027827
102.065793	3590.725407	23.032845
102.172424	3611.592325	23.037863
102.272231	3631.325057	23.042880
102.471522	3628.771314	23.047898
102.706401	3601.301923	23.052915
102.817439	3585.851050	23.057933
102.717883	3600.710406	23.062951
102.800939	3594.508266	23.067968
102.800445	3593.141187	23.072986
102.772926	3574.712092	23.078003
102.828409	3601.999310	23.083021
102.812321	3629.040746	23.088039
102.790221	3626.306478	23.093056
102.674077	3628.689699	23.098074
102.974626	3626.344797	23.103091
103.108658	3628.007008	23.108109
103.395602	3626.834535	23.113127
103.601142	3639.357478	23.118144
103.316956	3656.024221	23.123162
103.623187	3638.697290	23.128179
103.706780	3647.619028	23.133197
103.615416	3669.189554	23.138215
104.070549	3666.579160	23.143232
103.939017	3670.921863	23.148250
104.294461	3691.543459	23.153267
104.198200	3688.023662	23.158285
104.481376	3687.463373	23.163303
104.714178	3700.117284	23.168320
104.331665	3695.559239	23.173338
104.478216	3688.135049	23.178355
105.101645	3712.296760	23.183373
105.261215	3720.846565	23.188391
105.725853	3720.415333	23.193408
105.225178	3720.857732	23.198426
105.558407	3708.845547	23.203443
105.376782	3720.875292	23.208461
105.772993	3733.600055	23.213479
106.231053	3715.409232	23.218496
106.123225	3724.311665	23.223514
105.919298	3720.408698	23.228531
106.043827	3734.241660	23.233549
105.948644	3724.305028	23.238567
105.733751	3708.330375	23.243584
105.744044	3737.792852	23.248602
106.019581	3759.328660	23.253619
106.336062	3753.571512	23.258637
106.312724	3778.848789	23.263655
106.749416	3771.997634	23.268672
106.765972	3775.077598	23.273690
106.539746	3777.227672	23.278707
106.904382	3804.331100	23.283725
106.750569	3793.025074	23.288743
107.257084	3776.961455	23.293760
106.913954	3798.782016	23.298778
106.925155	3815.712106	23.303795
107.412339	3822.564441	23.308813
107.285141	3836.271780	23.313831
107.792366	3830.609454	23.318848
107.754067	3849.230914	23.323866
108.021475	3837.827694	23.328883
108.227621	3831.591736	23.333901
108.094825	3842.625974	23.338919
108.162782	3850.697322	23.343936
108.565014	3859.411816	23.348954
108.239477	3857.440593	23.353971
108.802407	3870.015487	23.358989
108.934191	3878.597528	23.364007
109.093208	3858.348806	23.369024
109.001037	3853.089631	23.374042
109.167404	3865.689896	23.379059
109.049429	3874.027987	23.384077
108.921047	3864.667186	23.389095
109.407676	3875.236912	23.394112
109.548613	3883.975504	23.399130
109.888095	3890.871764	23.404147
109.818482	3894.463006	23.409165
109.294748	3896.675051	23.414183
109.689656	3889.076861	23.419200
109.621555	3910.459244	23.424218
110.123609	3920.929609	23.429235
110.240948	3911.237643	23.434253
110.300610	3900.005312	23.439271
110.499328	3905.347773	23.444288
110.192554	3921.160123	23.449306
110.469946	3943.721999	23.454323
110.958265	3930.383112	23.459341
110.624994	3931.835781	23.464359
111.166117	3935.070224	23.469376
111.151488	3947.470359	23.474394
111.094906	3935.460409	23.479411
111.612640	3964.575113	23.484429
111.358087	3977.442058	23.489447
111.459865	3956.265910	23.494464
111.610143	3954.360530	23.499482
111.705089	3963.617956	23.504499
111.802345	3972.562033	23.509517
111.648292	3985.199398	23.514535
112.202810	3987.269501	23.519552
112.561722	3982.266434	23.524570
112.704330	3990.390476	23.529587
112.712381	3999.982737	23.534605
112.221468	3985.918654	23.539623
112.653173	3991.747419	23.544640
113.019708	4005.794361	23.549658
113.078932	4017.539866	23.554675
113.439208	4019.077929	23.559693
113.264802	4018.563125	23.564711
113.543223	4016.943632	23.569728
113.593090	4026.290824	23.574746
113.483464	4001.255275	23.579763
113.899696	4005.988633	23.584781
113.615323	4008.888265	23.589799
114.085442	4005.925754	23.594816
113.912829	3997.274897	23.599834
113.875472	4006.179429	23.604851
114.501057	4037.646395	23.609869
114.032027	4041.738293	23.614887
114.375353	4040.912360	23.619904
114.701804	4035.691029	23.624922
114.273549	4045.895936	23.629939
114.552178	4050.657557	23.634957
114.301398	4052.064719	23.639975
114.534412	4054.537545	23.644992
114.720164	4076.027415	23.650010
114.776088	4113.811571	23.655027
115.255610	4100.749962	23.660045
115.340151	4110.475314	23.665063
115.345463	4111.468529	23.670080
115.979944	4113.527799	23.675098
116.131512	4115.731825	23.680115
115.930472	4121.141598	23.685133
115.830022	4124.913178	23.690151
116.262855	4110.240457	23.695168
116.378354	4117.367914	23.700186
116.100191	4128.702348	23.705203
116.511660	4121.856389	23.710221
116.116740	4107.046448	23.715239
116.085052	4120.112106	23.720256
116.644403	4148.350637	23.725274
116.637415	4162.561407	23.730291
117.072841	4140.136625	23.735309
116.884900	4154.704832	23.740327
117.306416	4174.077632	23.745344
117.303790	4172.752977	23.750362
117.640046	4176.273675	23.755379
117.972758	4183.252284	23.760397
117.866347	4180.753887	23.765415
118.022283	4188.453802	23.770432
117.940050	4177.692335	23.775450
117.663427	4172.026148	23.780467
117.782556	4196.605793	23.785485
117.992552	4194.755867	23.790503
118.601253	4204.334039	23.795520
118.641447	4216.227714	23.800538
118.402369	4211.051351	23.805555
118.702384	4211.152605	23.810573
119.133274	4237.367734	23.815591
119.205304	4225.249696	23.820608
119.240952	4222.992374	23.825626
118.985052	4231.828428	23.830643
119.401454	4226.123687	23.835661
119.378936	4242.825968	23.840679
119.268408	4243.057656	23.845696
119.640153	4256.565011	23.850714
119.452938	4239.108917	23.855731
119.642110	4255.425459	23.860749
119.940311	4284.098321	23.865767
120.376111	4273.233865	23.870784
120.227828	4282.855283	23.875802
119.911688	4296.575156	23.880819
120.782846	4290.064566	23.885837
120.683738	4317.300443	23.890855
120.692770	4309.149298	23.895872
121.105078	4305.511270	23.900890
121.255993	4301.061743	23.905907
121.346884	4309.139382	23.910925
121.592543	4307.133162	23.915943
121.457175	4301.008170	23.920960
121.609189	4334.101966	23.925978
121.594802	4335.614180	23.930995
121.712359	4337.716380	23.936013
121.520446	4347.776529	23.941031
121.834351	4333.853146	23.946048
122.206955	4332.679459	23.951066
121.923261	4356.206275	23.956083
122.178055	4364.905263	23.961101
122.338456	4378.597250	23.966119
122.632605	4389.827462	23.971136
122.779767	4383.734096	23.976154
122.477592	4386.488318	23.981171
122.982028	4383.847221	23.986189
123.102335	4394.534527	23.991207
123.386816	4417.865585	23.996224
123.965659	4415.973582	24.001242
123.804180	4407.969061	24.006259
124.160545	4402.717076	24.011277
124.188998	4410.725561	24.016295
123.983439	4413.085882	24.021312
124.202599	4400.550101	24.026330
124.357036	4400.649428	24.031347
124.534096	4410.780141	24.036365
124.477970	4400.941341	24.041383
124.405551	4420.888967	24.046400
124.163396	4397.090389	24.051418
124.437847	4399.601305	24.056435
124.370543	4418.811491	24.061453
124.921148	4440.901009	24.066471
124.626578	4444.877178	24.071488
124.689256	4441.832309	24.076506
124.515574	4446.896739	24.081523
125.087529	4463.734485	24.086541
125.263629	4496.041991	24.091559
125.298661	4503.327014	24.096576
125.745739	4478.903017	24.101594
125.607403	4505.959491	24.106611
125.764490	4512.247208	24.111629
126.277494	4515.445479	24.116647
125.999091	4528.395558	24.121664
126.196998	4533.082481	24.126682
125.751041	4553.488447	24.131699
126.538612	4546.798262	24.136717
126.652115	4545.803985	24.141735
126.864302	4566.152397	24.146752
127.209335	4570.431170	24.151770
127.276295	4577.475523	24.156787
127.403958	4595.193897	24.161805
127.612524	4585.008493	24.166823
127.697949	4573.003323	24.171840
127.780600	4565.839072	24.176858
127.912535	4597.167886	24.181875
128.270613	4595.708791	24.186893
128.301035	4598.823045	24.191911
127.814718	4614.703954	24.196928
128.480871	4604.232694	24.201946
128.473031	4613.676782	24.206963
128.635109	4591.684700	24.211981
129.324366	4612.520080	24.216999
129.251060	4625.839492	24.222016
129.606481	4614.704228	24.227034
129.342218	4613.552293	24.232051
129.561487	4628.278062	24.237069
129.904974	4633.311820	24.242087
129.655405	4644.962371	24.247104
130.066222	4639.473360	24.252122
129.737088	4631.411388	24.257139
130.141590	4615.725568	24.262157
130.232500	4618.045593	24.267175
129.984496	4626.047902	24.272192
130.203628	4623.768077	24.277210
130.217098	4648.741089	24.282227
130.362137	4649.380153	24.287245
130.246901	4637.926979	24.292263
130.311295	4652.687811	24.297280
130.883364	4667.150994	24.302298
130.574676	4692.821394	24.307315
130.854666	4710.545439	24.312333
131.462058	4706.878627	24.317351
131.332252	4697.733696	24.322368
131.641365	4710.863615	24.327386
131.495033	4721.339696	24.332403
131.902387	4735.448668	24.337421
131.783534	4726.604663	24.342439
131.741286	4733.350994	24.347456
132.099835	4750.000302	24.352474
132.601111	4766.536281	24.357491
132.489418	4772.026397	24.362509
133.141813	4753.419577	24.367527
132.718438	4759.348195	24.372544
132.955672	4765.350333	24.377562
132.795344	4783.003125	24.382579
132.956470	4782.542692	24.387597
133.356619	4782.708508	24.392615
133.217372	4790.735450	24.397632
133.441127	4794.527636	24.402650
133.223143	4781.904333	24.407667
133.518449	4806.395992	24.412685
134.099097	4811.385108	24.417703
134.119911	4825.232444	24.422720
134.202440	4829.096399	24.427738
134.341996	4818.920277	24.432755
134.683849	4801.261954	24.437773
134.568099	4830.749894	24.442791
134.797138	4842.477019	24.447808
135.281494	4836.523821	24.452826
135.112382	4833.372689	24.457843
134.971035	4850.316911	24.462861
135.247072	4854.595353	24.467879
135.162938	4851.801434	24.472896
135.658254	4855.385377	24.477914
135.819368	4853.990695	24.482931
136.084164	4871.478065	24.487949
135.939373	4873.555973	24.492967
135.786390	4868.917917	24.497984
136.255307	4865.320801	24.503002
136.330384	4884.302130	24.508019
136.573232	4909.223486	24.513037
136.873853	4898.891957	24.518055
136.661258	4887.340513	24.523072
136.737848	4891.916883	24.528090
136.822386	4919.835282	24.533107
136.736656	4922.007374	24.538125
137.082916	4919.356499	24.543143
137.152225	4941.977050	24.548160
137.771073	4948.085888	24.553178
137.731460	4933.302664	24.558195
137.792239	4950.039580	24.563213
138.270671	4974.753215	24.568231
138.429235	4972.444371	24.573248
138.867030	4969.469700	24.578266
139.024875	4980.365776	24.583283
138.683883	4978.128847	24.588301
139.031306	4966.071027	24.593319
138.905332	4967.050162	24.598336
139.196437	4953.928817	24.603354
139.014045	4976.948884	24.608371
138.573414	5000.711662	24.613389
138.988292	5003.448689	24.618407
138.871796	4992.937594	24.623424
138.980597	5014.382425	24.628442
139.843495	5030.740035	24.633459
139.838073	5046.402550	24.638477
140.081112	5057.651536	24.643495
139.828760	5079.873070	24.648512
140.236300	5069.821797	24.653530
140.070286	5068.981549	24.658547
140.453607	5084.151516	24.663565
140.787172	5100.109651	24.668583
140.382231	5117.609143	24.673600
141.165577	5125.395621	24.678618
140.936712	5109.476948	24.683635
141.085735	5127.366813	24.688653
141.529278	5150.441585	24.693671
141.468947	5159.398213	24.698688
141.442790	5149.730368	24.703706
141.944962	5160.808262	24.708723
142.030060	5156.640238	24.713741
142.379435	5159.807809	24.718759
142.502005	5177.290284	24.723776
142.628373	5189.338973	24.728794
142.538809	5174.680705	24.733811
142.636590	5159.904880	24.738829
143.059666	5173.190379	24.743847
142.876964	5203.050723	24.748864
142.798404	5196.585274	24.753882
143.458838	5206.985462	24.758899
143.101986	5222.070383	24.763917
143.435914	5224.097188	24.768935
143.433829	5223.545600	24.773952
143.768971	5228.516364	24.778970
143.631458	5235.815279	24.783987
143.895657	5265.385358	24.789005
144.374809	5263.213268	24.794023
144.249881	5249.211970	24.799040
144.555258	5275.372429	24.804058
145.080892	5304.477326	24.809075
145.059652	5300.110687	24.814093
145.173605	5290.802685	24.819111
144.802170	5287.168341	24.824128
145.098609	5299.774069	24.829146
145.090740	5328.072258	24.834163
145.181827	5326.628868	24.839181
145.628017	5313.511123	24.844199
145.328469	5360.044298	24.849216
145.451942	5372.018801	24.854234
145.619467	5365.707902	24.859251
145.708718	5382.667750	24.864269
146.413918	5382.644976	24.869287
146.887658	5417.058436	24.874304
146.727642	5418.597573	24.879322
147.259764	5398.669265	24.884339
147.258668	5405.546493	24.889357
147.685917	5404.557015	24.894375
147.858723	5416.070630	24.899392
147.653926	5408.305829	24.904410
147.647228	5411.874819	24.909427
148.045090	5429.268387	24.914445
148.148799	5439.948132	24.919463
147.827148	5453.332123	24.924480
148.044676	5436.618856	24.929498
148.582630	5434.959880	24.934515
148.459969	5467.254203	24.939533
148.684166	5480.929140	24.944551
148.982955	5471.811756	24.949568
149.165759	5489.222422	24.954586
149.507036	5475.668710	24.959603
149.208983	5493.784844	24.964621
149.305090	5506.737239	24.969639
149.454203	5500.273022	24.974656
149.932171	5502.468985	24.979674
150.300465	5509.197425	24.984691
150.066521	5523.907982	24.989709
150.334993	5527.891393	24.994727
150.310747	5512.774752	24.999744
150.472104	5530.802025	25.004762
150.737672	5533.765796	25.009779
150.748430	5532.884501	25.014797
151.088144	5542.428425	25.019815
151.212119	5549.503170	25.024832
151.479476	5560.917407	25.029850
151.436034	5562.133740	25.034867
151.451956	5587.224000	25.039885
151.793487	5580.305889	25.044903
151.670012	5572.703560	25.049920
151.508297	5587.331767	25.054938
152.296454	5608.951397	25.059955
152.277743	5598.519409	25.064973
152.193512	5584.699676	25.069991
152.523746	5625.509250	25.075008
152.594849	5636.815414	25.080026
153.263814	5628.928567	25.085043
153.070969	5616.753208	25.090061
153.305518	5620.492237	25.095079
153.496440	5632.305789	25.100096
153.446069	5651.670218	25.105114
153.378544	5656.215504	25.110131
153.490304	5653.107169	25.115149
153.908569	5658.421441	25.120167
153.895413	5690.905623	25.125184
153.803702	5701.168995	25.130202
154.142948	5689.433247	25.135219
154.020974	5707.928035	25.140237
154.301235	5719.565072	25.145255
154.780249	5748.893083	25.150272
155.016840	5759.424312	25.155290
155.408136	5753.318421	25.160307
155.571458	5757.853154	25.165325
155.496754	5757.972244	25.170343
155.678403	5772.680117	25.175360
155.807664	5774.302994	25.180378
156.240192	5751.638961	25.185395
156.184925	5772.363480	25.190413
156.149366	5779.806836	25.195431
156.321382	5796.039244	25.200448
156.414268	5803.357051	25.205466
156.811263	5801.374459	25.210483
156.964893	5821.553472	25.215501
157.194572	5840.012360	25.220519
157.295370	5844.271999	25.225536
157.270402	5843.319026	25.230554
157.645149	5838.382444	25.235571
157.785597	5852.071153	25.240589
157.939382	5879.670363	25.245607
157.877025	5874.468964	25.250624
158.169814	5858.845243	25.255642
158.356123	5883.714506	25.260659
158.358564	5908.188965	25.265677
158.305740	5900.660634	25.270695
158.546298	5883.828904	25.275712
158.747494	5914.200440	25.280730
159.342821	5921.317164	25.285747
159.325045	5933.698141	25.290765
159.513525	5946.353730	25.295783
159.466443	5970.936084	25.300800
159.562398	5975.201677	25.305818
159.826508	5966.367709	25.310835
159.991378	5974.622193	25.315853
159.925486	5991.994981	25.320871
160.428447	6010.890446	25.325888
160.114014	6005.331020	25.330906
160.677250	6014.845782	25.335923
160.882874	6011.093080	25.340941
160.944377	6021.327409	25.345959
161.482687	6034.176071	25.350976
161.402839	6035.070480	25.355994
161.649596	6032.764627	25.361011
161.918232	6056.934292	25.366029
161.862030	6059.622568	25.371047
162.094611	6066.042940	25.376064
161.862594	6056.449102	25.381082
162.345923	6063.649364	25.386099
162.052473	6087.510346	25.391117
162.527535	6096.716081	25.396135
162.780304	6107.942564	25.401152
162.797004	6126.436983	25.406170
163.225927	6128.711620	25.411187
163.493499	6125.480587	25.416205
163.482630	6127.078621	25.421223
163.725441	6123.743010	25.426240
163.783303	6140.133627	25.431258
163.638345	6131.267543	25.436275
163.746123	6146.637633	25.441293
164.139267	6168.372136	25.446311
164.154881	6170.657587	25.451328
163.885719	6180.033196	25.456346
164.552871	6178.787874	25.461363
164.661633	6198.727523	25.466381
164.809022	6220.084954	25.471399
165.170369	6231.012853	25.476416
165.121340	6230.165022	25.481434
165.765593	6225.999607	25.486451
165.734716	6236.230047	25.491469
165.617531	6252.879253	25.496487
166.139675	6251.345261	25.501504
166.077092	6281.557141	25.506522
166.614604	6279.379605	25.511539
166.548125	6282.333420	25.516557
166.527162	6290.616415	25.521575
167.008352	6307.136489	25.526592
166.782616	6323.089073	25.531610
166.961399	6319.520672	25.536627
167.256328	6330.330075	25.541645
167.096106	6335.659845	25.546663
167.439760	6356.184563	25.551680
167.616049	6375.210046	25.556698
167.861079	6368.200438	25.561715
167.948839	6367.671763	25.566733
168.252833	6404.289280	25.571751
168.140055	6407.880357	25.576768
168.372823	6428.379394	25.581786
169.265875	6444.563818	25.586803
169.243587	6432.213957	25.591821
169.124631	6424.120259	25.596839
169.173815	6436.443715	25.601856
169.363414	6460.814485	25.606874
169.607031	6483.373034	25.611891
170.100452	6487.752245	25.616909
169.909033	6477.211186	25.621927
170.616086	6482.190201	25.626944
170.512803	6497.539206	25.631962
170.812709	6517.400430	25.636979
171.114717	6514.625094	25.641997
171.110731	6510.576953	25.647015
171.477285	6500.563038	25.652032
171.092879	6514.897770	25.657050
171.667375	6537.063500	25.662067
171.735119	6536.254238	25.667085
171.726723	6527.726426	25.672103
172.140178	6550.602715	25.677120
172.037759	6581.860057	25.682138
172.308092	6572.873522	25.687156
172.312709	6561.529459	25.692173
172.109284	6591.176956	25.697191
172.481616	6604.937078	25.702208
172.742917	6613.463794	25.707226
172.935300	6611.938975	25.712244
172.884334	6618.167817	25.717261
173.110581	6647.284138	25.722279
173.478818	6652.583789	25.727296
173.788119	6669.058232	25.732314
173.736802	6688.573723	25.737332
173.867214	6714.940725	25.742349
174.000701	6713.052356	25.747367
174.508635	6731.176523	25.752384
174.569442	6729.400961	25.757402
174.765884	6723.322955	25.762420
175.172695	6718.333158	25.767437
175.019077	6754.141176	25.772455
175.434093	6761.910203	25.777472
175.598583	6771.722053	25.782490
175.701592	6768.183395	25.787508
176.081795	6764.291026	25.792525
176.007564	6786.635962	25.797543
176.277411	6785.729900	25.802560
176.203682	6791.372344	25.807578
176.647787	6822.673344	25.812596
176.534297	6825.421616	25.817613
176.629893	6819.722486	25.822631
177.319398	6829.330678	25.827648
177.272162	6835.966129	25.832666
177.480042	6841.581353	25.837684
177.722858	6861.226829	25.842701
177.634860	6866.166055	25.847719
178.283373	6874.751785	25.852736
178.329750	6883.361411	25.857754
178.152170	6893.291676	25.862772
178.354377	6901.126255	25.867789
178.434288	6929.718391	25.872807
178.697446	6933.850700	25.877824
178.584158	6931.826679	25.882842
178.818843	6964.113870	25.887860
179.718063	6966.256194	25.892877
179.593269	6978.156007	25.897895
179.679636	6977.514929	25.902912
179.868251	6997.655816	25.907930
180.120659	7016.804559	25.912948
180.473799	7020.767672	25.917965
180.536981	7026.238345	25.922983
180.685016	7021.129378	25.928000
181.195533	7047.490048	25.933018
181.056472	7048.798684	25.938036
181.487416	7053.821933	25.943053
181.350522	7059.181167	25.948071
182.099084	7068.946704	25.953088
181.825528	7102.156462	25.958106
181.809137	7100.957473	25.963124
182.345207	7090.838392	25.968141
182.337877	7112.902623	25.973159
182.560186	7116.755469	25.978176
182.441322	7131.147687	25.983194
182.604676	7155.128148	25.988212
183.282638	7155.796210	25.993229
182.962512	7161.347590	25.998247
183.278424	7183.777862	26.003264
183.807625	7207.033289	26.008282
183.652145	7214.082906	26.013300
184.257241	7193.779189	26.018317
184.165330	7209.106141	26.023335
184.287855	7208.852050	26.028352
184.514742	7238.617492	26.033370
184.688736	7251.582878	26.038388
185.001454	7248.244931	26.043405
185.294159	7279.695108	26.048423
185.359003	7293.492073	26.053440
185.508766	7286.089863	26.058458
185.446912	7286.171007	26.063476
185.628135	7291.691571	26.068493
185.899171	7325.042561	26.073511
186.066398	7327.854004	26.078528
186.482424	7326.801693	26.083546
186.124607	7335.238551	26.088564
186.610944	7360.312595	26.093581
186.509293	7379.872701	26.098599
187.076023	7368.286728	26.103616
187.525774	7375.452984	26.108634
187.412402	7398.740053	26.113652
187.682732	7393.622179	26.118669
187.608173	7413.588152	26.123687
187.719243	7438.347888	26.128704
188.025101	7448.919609	26.133722
188.428224	7445.420990	26.138740
188.727638	7451.089825	26.143757
188.876813	7455.426571	26.148775
188.703807	7469.889078	26.153792
188.744395	7487.594805	26.158810
189.208471	7481.354944	26.163828
189.374529	7476.374764	26.168845
189.431580	7508.679432	26.173863
190.043825	7526.048187	26.178880
190.118632	7533.044933	26.183898
190.311272	7542.641555	26.188916
190.685280	7544.359636	26.193933
190.739644	7555.223418	26.198951
190.935405	7587.837671	26.203968
191.440290	7579.091385	26.208986
191.078706	7578.232121	26.214004
191.435695	7595.851827	26.219021
191.617042	7607.254604	26.224039
191.718620	7612.277328	26.229056
192.040602	7634.785603	26.234074
191.863475	7648.791394	26.239092
192.467825	7650.710053	26.244109
192.413885	7663.031429	26.249127
192.463048	7682.733951	26.254144
193.099532	7697.518116	26.259162
193.347605	7692.332944	26.264180
193.794218	7690.568344	26.269197
193.887799	7680.920496	26.274215
194.172450	7719.815950	26.279232
194.526080	7722.763624	26.284250
194.393637	7726.784706	26.289268
194.533707	7737.270608	26.294285
195.156982	7722.329542	26.299303
195.258895	7719.513031	26.304320
195.615324	7742.778900	26.309338
195.474583	7763.198065	26.314356
195.832717	7760.919633	26.319373
196.030252	7748.122497	26.324391
196.082819	7739.706811	26.329408
196.510676	7753.296143	26.334426
196.208984	7790.514311	26.339444
196.513014	7770.395057	26.344461
196.597466	7772.031061	26.349479
196.501133	7791.497869	26.354496
196.913352	7816.343113	26.359514
196.920436	7833.471192	26.364532
196.936286	7828.707094	26.369549
197.173923	7832.645791	26.374567
197.313354	7865.151794	26.379584
197.576837	7882.232048	26.384602
197.291395	7889.405821	26.389620
198.003632	7917.962219	26.394637
198.519834	7951.738689	26.399655
198.581492	7946.773248	26.404672
198.858218	7928.484646	26.409690
198.975135	7957.790788	26.414708
199.244390	7975.379738	26.419725
199.317378	7975.571703	26.424743
199.515497	7989.003096	26.429760
199.651316	8008.806692	26.434778
199.793927	8007.157655	26.439796
200.329197	8017.155527	26.444813
200.076324	8045.773963	26.449831
200.190375	8055.825706	26.454848
200.857858	8063.551701	26.459866
200.649114	8070.592386	26.464884
200.839538	8100.149693	26.469901
200.959310	8112.059175	26.474919
201.159479	8123.344233	26.479936
201.794800	8126.545503	26.484954
201.534438	8158.534583	26.489972
201.872231	8169.874903	26.494989
202.042437	8173.619273	26.500007
202.157979	8191.938736	26.505024
202.252971	8194.830788	26.510042
202.545558	8235.120987	26.515060
203.108329	8247.794563	26.520077
203.871622	8236.028993	26.525095
203.550886	8263.172890	26.530112
203.975966	8277.810605	26.535130
204.375169	8285.092743	26.540148
204.400058	8275.244813	26.545165
204.828728	8294.332520	26.550183
204.988225	8305.376343	26.555200
205.233395	8301.746910	26.560218
205.091702	8322.960042	26.565236
205.619247	8328.740355	26.570253
205.634560	8320.007610	26.575271
205.484077	8334.125380	26.580288
205.845952	8342.157970	26.585306
206.063324	8362.150942	26.590324
206.011274	8370.646514	26.595341
206.367538	8407.913365	26.600359
206.620302	8435.836227	26.605376
206.763515	8419.251389	26.610394
207.086824	8432.938916	26.615412
207.238476	8439.767428	26.620429
207.476635	8454.738623	26.625447
207.429781	8462.696256	26.630464
207.734144	8490.899731	26.635482
208.048888	8513.263183	26.640500
208.038776	8518.651975	26.645517
208.416569	8530.323821	26.650535
208.301386	8536.241910	26.655552
208.978954	8558.878627	26.660570
209.324783	8569.387793	26.665588
209.178965	8592.539431	26.670605
210.040623	8622.502682	26.675623
209.786795	8630.700158	26.680640
210.182189	8635.165092	26.685658
210.460797	8644.511119	26.690676
210.541708	8643.391233	26.695693
210.827910	8655.425633	26.700711
211.080799	8677.588463	26.705728
211.513368	8661.932175	26.710746
211.633255	8679.419790	26.715764
211.765427	8694.400849	26.720781
211.874529	8713.399311	26.725799
211.588667	8718.619507	26.730816
212.187083	8721.346568	26.735834
212.103416	8750.792862	26.740852
212.242998	8786.123481	26.745869
212.740651	8784.923703	26.750887
212.764105	8794.473434	26.755904
212.919188	8791.965350	26.760922
213.277881	8817.603104	26.765940
213.151915	8840.970778	26.770957
213.675838	8853.715059	26.775975
213.457057	8883.276073	26.780992
213.595431	8887.267667	26.786010
214.024574	8906.634062	26.791028
214.254077	8915.918267	26.796045
214.828164	8936.864312	26.801063
214.889146	8947.282964	26.806080
215.332209	8945.882691	26.811098
215.702306	8956.163639	26.816116
215.826309	8993.574212	26.821133
216.254501	8990.308975	26.826151
216.195980	8994.410313	26.831168
216.506344	9002.862097	26.836186
216.754355	9019.512957	26.841204
216.748298	9010.945608	26.846221
217.018366	9033.407754	26.851239
217.141098	9063.656181	26.856256
217.436871	9062.961519	26.861274
217.699394	9075.327798	26.866292
217.551609	9085.023351	26.871309
217.884183	9099.696806	26.876327
217.803485	9133.731956	26.881344
218.186600	9135.621200	26.886362
218.368300	9147.332992	26.891380
218.924531	9173.346671	26.896397
219.015409	9181.850567	26.901415
219.040822	9188.753032	26.906432
219.829410	9206.073247	26.911450
219.858287	9231.011628	26.916468
219.959615	9252.706469	26.921485
220.662736	9256.157478	26.926503
220.801481	9273.151946	26.931520
220.926994	9285.952953	26.936538
221.590104	9283.050531	26.941556
221.172299	9288.491193	26.946573
221.615056	9288.534655	26.951591
221.677570	9300.944396	26.956608
222.303466	9326.362401	26.961626
222.326580	9334.994932	26.966644
222.333177	9339.626698	26.971661
222.882832	9367.173714	26.976679
222.634783	9366.426331	26.981696
222.734721	9363.119164	26.986714
222.957372	9399.390455	26.991732
223.037478	9408.428689	26.996749
223.415100	9444.654788	27.001767
223.589421	9455.753676	27.006784
224.030705	9465.695541	27.011802
224.209676	9483.944587	27.016820
224.648732	9487.377055	27.021837
224.955804	9496.376265	27.026855
225.040619	9534.325455	27.031872
225.275397	9533.088719	27.036890
225.839152	9541.680870	27.041908
225.887436	9550.294394	27.046925
226.143605	9567.046876	27.051943
226.147428	9600.762672	27.056960
226.556269	9592.568324	27.061978
226.850798	9595.219730	27.066996
226.902976	9624.248232	27.072013
227.567586	9618.152415	27.077031
227.315742	9633.032407	27.082048
227.530108	9651.405758	27.087066
227.738040	9656.242219	27.092084
227.705998	9659.133476	27.097101
228.212989	9667.939074	27.102119
228.252408	9693.015852	27.107136
228.245862	9722.029031	27.112154
228.523958	9728.849025	27.117172
229.093354	9738.639934	27.122189
229.568097	9745.117111	27.127207
229.540676	9760.145239	27.132224
229.986073	9767.069144	27.137242
230.021445	9777.545346	27.142260
230.327976	9789.452804	27.147277
230.405473	9803.407403	27.152295
230.340408	9824.275920	27.157312
230.717350	9834.286147	27.162330
230.708426	9830.219460	27.167348
231.024948	9854.103891	27.172365
231.095480	9885.790523	27.177383
231.398243	9918.402149	27.182400
231.498835	9923.840867	27.187418
231.832348	9932.670549	27.192436
231.766963	9959.125342	27.197453
232.352632	9973.304102	27.202471
232.184408	10008.845835	27.207488
232.943338	10019.045905	27.212506
233.205333	10033.048988	27.217524
233.472670	10063.202178	27.222541
234.011832	10088.363996	27.227559
234.043589	10081.032753	27.232576
234.341357	10087.410136	27.237594
234.851421	10111.846635	27.242612
235.223613	10125.081738	27.247629
235.244538	10126.189722	27.252647
235.459558	10153.795759	27.257664
235.640471	10160.349224	27.262682
236.094906	10176.253570	27.267700
236.026498	10191.339288	27.272717
236.318357	10185.780595	27.277735
236.559774	10193.489824	27.282752
236.641050	10218.310825	27.287770
237.093499	10243.288723	27.292788
237.178134	10274.824931	27.297805
237.398174	10274.094684	27.302823
237.748696	10280.936820	27.307840
238.012046	10293.855286	27.312858
238.293789	10301.396432	27.317876
238.341844	10322.962908	27.322893
238.671505	10347.380742	27.327911
238.946407	10372.783592	27.332928
239.074108	10374.159878	27.337946
239.303405	10394.975783	27.342964
239.625153	10408.895284	27.347981
239.693875	10420.522711	27.352999
240.007149	10438.032301	27.358016
240.182363	10448.922215	27.363034
240.884737	10476.923264	27.368052
240.765468	10488.838585	27.373069
241.243387	10500.125924	27.378087
241.515555	10480.713479	27.383104
241.759276	10524.180906	27.388122
242.150040	10545.507531	27.393140
242.100324	10537.371922	27.398157
242.252620	10534.183467	27.403175
242.703538	10571.075074	27.408192
242.694917	10604.509125	27.413210
243.133586	10600.309213	27.418228
242.881489	10603.893142	27.423245
243.137052	10626.231549	27.428263
243.232229	10637.015087	27.433280
243.504341	10660.756834	27.438298
244.083548	10693.085705	27.443316
244.030666	10714.947444	27.448333
244.593264	10719.647652	27.453351
244.620685	10743.612695	27.458368
244.727165	10778.423888	27.463386
245.172267	10768.152883	27.468404
245.542059	10791.441515	27.473421
246.186450	10794.880520	27.478439
246.418853	10802.233133	27.483456
246.470690	10819.032512	27.488474
246.643265	10838.238073	27.493492
246.690343	10845.818250	27.498509
246.642744	10833.516786	27.503527
247.131640	10858.822828	27.508544
247.429649	10901.876651	27.513562
248.089943	10908.187380	27.518580
247.780039	10912.575721	27.523597
247.966794	10928.005164	27.528615
248.364993	10971.904371	27.533632
248.775362	10997.685991	27.538650
249.463170	10992.305003	27.543668
249.098095	11004.833983	27.548685
249.620854	11005.164358	27.553703
250.042712	11034.119388	27.558720
249.962078	11041.082714	27.563738
250.080262	11050.670140	27.568756
250.267580	11098.747103	27.573773
250.541839	11112.555335	27.578791
251.045285	11116.154761	27.583808
250.942133	11130.437338	27.588826
251.226151	11162.958512	27.593844
251.528411	11203.731225	27.598861
252.030789	11200.976333	27.603879
252.183959	11216.415543	27.608896
252.398008	11233.566662	27.613914
253.025586	11258.054043	27.618932
253.015030	11267.782602	27.623949
253.323286	11289.746156	27.628967
253.855025	11315.410561	27.633984
253.486445	11322.708315	27.639002
253.742261	11349.315578	27.644020
254.266071	11376.148798	27.649037
254.532411	11386.014433	27.654055
255.141566	11391.053751	27.659072
255.288379	11426.977479	27.664090
255.166922	11432.622761	27.669108
255.401454	11446.819107	27.674125
255.514441	11465.243601	27.679143
256.271668	11476.274378	27.684160
256.160859	11506.143026	27.689178
256.914879	11528.258551	27.694196
256.727382	11553.408832	27.699213
257.214453	11564.619008	27.704231
257.773907	11570.802509	27.709248
257.579135	11606.974497	27.714266
258.132374	11596.895424	27.719284
258.471717	11620.583380	27.724301
258.639525	11630.921546	27.729319
258.872853	11656.999739	27.734336
258.940932	11672.645657	27.739354
259.477779	11672.254515	27.744372
259.594287	11685.030584	27.749389
259.970859	11726.490292	27.754407
259.786569	11737.843809	27.759424
259.850445	11739.759336	27.764442
260.389672	11751.718836	27.769460
260.716282	11788.644828	27.774477
261.159127	11812.806734	27.779495
261.503325	11834.412188	27.784512
261.500976	11831.386095	27.789530
261.721646	11840.758550	27.794548
262.050892	11878.001775	27.799565
262.049068	11899.384835	27.804583
262.726464	11906.513190	27.809600
262.351005	11913.357027	27.814618
262.937452	11931.949613	27.819636
262.975892	11968.257979	27.824653
263.050518	11989.938904	27.829671
263.866947	11985.501341	27.834688
263.993386	12004.929410	27.839706
264.333562	12032.480210	27.844724
264.463391	12066.233966	27.849741
264.763575	12067.758362	27.854759
265.534255	12066.926823	27.859776
265.813431	12104.431719	27.864794
265.983281	12116.794410	27.869812
266.390579	12132.621849	27.874829
266.355998	12139.509508	27.879847
266.501878	12161.708270	27.884864
266.585859	12159.327211	27.889882
266.919432	12185.564587	27.894900
267.130672	12209.873282	27.899917
267.478400	12226.310935	27.904935
267.701302	12254.167451	27.909952
268.021741	12278.612612	27.914970
268.065289	12281.980272	27.919988
268.341478	12313.011466	27.925005
268.559659	12340.046478	27.930023
268.907933	12340.186716	27.935040
269.414354	12376.374572	27.940058
269.520822	12401.502823	27.945076
269.844715	12424.548545	27.950093
270.234000	12444.552126	27.955111
270.618902	12449.821053	27.960128
270.554913	12492.810561	27.965146
270.940824	12516.333805	27.970164
271.312490	12522.675538	27.975181
271.509955	12527.824205	27.980199
272.250350	12551.388982	27.985216
272.187031	12592.085407	27.990234
272.565357	12612.590464	27.995252
272.752792	12619.696104	28.000269
272.783401	12622.888721	28.005287
273.652168	12645.950304	28.010304
273.693959	12661.394342	28.015322
273.934022	12679.855171	28.020340
274.375572	12698.057424	28.025357
274.060984	12725.740439	28.030375
274.746418	12745.015603	28.035392
275.062612	12753.897772	28.040410
275.255865	12755.383969	28.045428
275.046632	12797.326100	28.050445
275.469406	12841.428841	28.055463
275.840168	12854.580580	28.060480
275.936175	12878.336597	28.065498
276.190779	12882.109106	28.070516
276.869132	12910.531207	28.075533
276.841411	12959.348849	28.080551
277.440736	12971.271764	28.085568
277.710271	12980.343750	28.090586
277.741264	13003.217323	28.095604
278.338775	13028.423775	28.100621
277.984380	13047.489012	28.105639
278.896037	13068.785733	28.110656
278.920278	13090.243276	28.115674
279.072008	13129.441779	28.120692
279.586561	13139.319485	28.125709
279.709960	13158.747877	28.130727
279.924901	13174.924041	28.135744
280.177492	13208.398361	28.140762
280.368352	13233.780252	28.145780
280.916786	13231.256124	28.150797
280.962934	13257.014113	28.155815
281.296631	13274.016085	28.160832
281.764402	13305.169594	28.165850
282.049820	13329.593780	28.170868
282.782583	13334.803954	28.175885
282.833975	13334.589101	28.180903
283.403736	13352.730737	28.185920
283.524307	13386.180757	28.190938
283.283728	13401.734395	28.195956
283.793455	13397.087147	28.200973
284.124189	13432.627305	28.205991
284.370954	13445.903221	28.211008
284.941019	13484.812883	28.216026
284.782744	13493.721855	28.221044
285.241517	13499.435080	28.226061
285.355833	13522.901465	28.231079
285.407424	13554.293598	28.236096
285.757536	13584.569746	28.241114
286.229606	13604.602063	28.246132
286.425350	13613.343104	28.251149
286.863467	13642.223745	28.256167
287.128512	13669.929214	28.261184
287.221840	13699.829661	28.266202
287.447348	13729.846196	28.271220
287.898645	13758.226164	28.276237
287.829161	13758.160483	28.281255
288.497906	13774.572685	28.286272
288.580351	13808.040909	28.291290
288.924780	13844.703967	28.296308
289.455190	13857.726158	28.301325
289.466529	13888.045452	28.306343
289.787158	13912.590760	28.311360
290.010466	13941.638210	28.316378
290.415556	13969.360449	28.321396
291.095337	13976.884059	28.326413
291.307554	14006.625193	28.331431
291.642725	14026.691684	28.336448
291.823370	14062.627532	28.341466
292.325598	14069.860649	28.346484
292.873971	14085.837675	28.351501
292.757181	14110.855785	28.356519
293.398135	14133.667216	28.361536
293.710038	14169.050597	28.366554
294.043326	14180.969519	28.371572
294.246188	14184.205683	28.376589
294.580303	14192.798119	28.381607
294.755478	14215.967099	28.386624
294.962402	14252.458412	28.391642
295.090444	14261.839707	28.396660
295.416795	14263.211876	28.401677
295.504268	14302.471117	28.406695
295.933667	14335.504934	28.411712
296.379181	14343.327418	28.416730
296.856272	14356.598335	28.421748
296.781827	14379.838729	28.426765
297.358176	14411.209648	28.431783
297.939559	14435.596068	28.436800
297.572487	14448.276953	28.441818
298.130184	14479.512421	28.446836
298.585213	14483.457044	28.451853
299.019673	14526.866770	28.456871
299.326415	14531.316511	28.461888
299.672258	14536.834462	28.466906
299.555148	14554.034385	28.471924
299.862371	14586.318353	28.476941
300.089697	14606.906052	28.481959
300.281150	14619.940739	28.486976
300.800840	14649.260376	28.491994
301.009758	14676.680600	28.497012
301.569602	14689.682845	28.502029
301.590557	14699.373605	28.507047
301.835851	14715.239023	28.512064
302.192353	14746.580733	28.517082
301.865489	14756.247049	28.522100
302.395537	14765.095789	28.527117
302.724703	14819.506907	28.532135
303.068204	14850.923452	28.537152
303.624955	14849.156452	28.542170
303.876914	14882.691864	28.547188
304.262091	14905.378035	28.552205
304.500903	14937.932436	28.557223
304.766346	14942.423782	28.562240
305.096898	14968.733952	28.567258
305.226745	15004.752770	28.572276
305.896903	15020.888670	28.577293
306.106418	15033.054012	28.582311
306.290967	15068.206694	28.587328
306.966192	15096.297525	28.592346
307.260107	15113.822514	28.597364
307.581465	15125.031836	28.602381
307.759498	15146.444638	28.607399
308.005768	15181.749679	28.612416
308.679081	15195.675928	28.617434
308.946684	15205.839961	28.622452
309.184842	15218.653102	28.627469
309.704951	15239.883447	28.632487
310.332052	15247.085436	28.637504
310.287033	15274.403648	28.642522
310.199524	15311.207577	28.647540
310.878638	15326.890039	28.652557
310.893709	15343.901922	28.657575
310.874561	15358.828336	28.662592
311.340569	15394.222027	28.667610
311.327374	15436.987988	28.672628
311.775258	15443.995903	28.677645
312.125329	15468.201477	28.682663
312.431408	15497.628855	28.687680
312.817292	15518.635908	28.692698
313.013445	15552.976156	28.697716
313.958902	15590.060755	28.702733
313.782622	15615.358907	28.707751
314.162555	15633.579386	28.712768
314.683856	15652.709445	28.717786
314.618921	15687.862136	28.722804
315.206342	15725.055047	28.727821
315.020960	15751.535244	28.732839
315.463471	15765.901966	28.737856
316.031573	15798.701533	28.742874
316.045191	15836.427591	28.747892
316.394088	15866.575046	28.752909
316.665067	15897.496587	28.757927
316.974787	15933.706795	28.762944
317.608965	15950.654852	28.767962
317.530591	15972.498774	28.772980
317.963477	15993.479765	28.777997
318.133096	16044.895613	28.783015
318.585007	16086.043624	28.788032
318.980581	16100.211953	28.793050
318.861770	16122.204587	28.798068
319.751822	16150.575361	28.803085
319.840316	16193.898566	28.808103
320.564414	16234.677346	28.813120
320.808132	16250.264011	28.818138
321.060594	16269.516431	28.823156
321.567275	16283.545217	28.828173
322.089820	16308.487874	28.833191
322.003085	16321.453268	28.838208
322.748472	16350.896288	28.843226
323.003172	16391.338538	28.848244
323.337011	16398.206540	28.853261
323.491942	16403.266554	28.858279
323.700748	16429.307653	28.863296
324.249184	16463.864260	28.868314
324.197684	16487.433245	28.873332
324.767818	16499.488102	28.878349
324.731289	16519.045441	28.883367
324.839170	16546.723481	28.888384
325.455314	16591.999856	28.893402
325.505930	16626.333315	28.898420
325.884756	16636.541331	28.903437
326.387054	16671.755298	28.908455
326.323344	16707.441083	28.913472
327.562924	16738.339732	28.918490
327.695539	16768.760984	28.923508
327.701731	16800.826437	28.928525
328.341374	16812.430345	28.933543
328.970920	16838.859623	28.938560
329.187552	16869.492548	28.943578
329.559309	16889.624305	28.948596
329.802632	16897.213515	28.953613
330.327735	16931.726113	28.958631
330.360764	16953.452077	28.963648
330.643653	16968.597983	28.968666
330.754079	17006.789853	28.973684
331.487932	17028.236233	28.978701
331.507788	17055.239387	28.983719
331.872494	17087.660663	28.988736
332.387898	17118.845154	28.993754
332.565152	17155.368368	28.998772
333.159969	17176.032568	29.003789
333.447600	17180.970036	29.008807
333.407889	17206.462425	29.013824
333.644663	17227.972275	29.018842
333.917257	17275.163854	29.023860
334.311785	17301.508202	29.028877
334.740833	17323.427701	29.033895
334.984119	17361.086238	29.038912
335.574042	17404.659202	29.043930
335.693400	17439.378594	29.048948
336.464089	17457.553896	29.053965
336.529724	17474.884310	29.058983
336.820915	17516.729145	29.064000
337.205367	17553.562595	29.069018
337.874962	17584.478213	29.074036
338.392800	17583.598380	29.079053
339.417226	17592.712154	29.084071
339.380996	17625.057310	29.089088
340.227740	17644.370779	29.094106
340.335376	17658.392601	29.099124
340.504519	17663.649242	29.104141
340.660333	17675.217070	29.109159
340.913910	17704.321400	29.114176
341.077533	17730.390949	29.119194
341.469560	17748.102725	29.124212
341.715749	17768.932444	29.129229
341.982800	17781.452831	29.134247
342.216181	17805.410067	29.139264
342.891859	17828.737914	29.144282
342.969898	17862.869271	29.149300
343.087833	17905.021111	29.154317
343.463456	17919.184861	29.159335
343.319843	17933.885165	29.164352
343.764569	17962.252286	29.169370
343.942844	17980.491367	29.174388
344.334802	18014.916343	29.179405
344.804027	18045.747728	29.184423
344.602459	18082.341893	29.189440
345.128094	18121.391360	29.194458
345.411623	18161.623597	29.199476
345.812048	18192.483961	29.204493
346.350682	18234.986391	29.209511
346.557322	18264.037998	29.214528
346.981489	18279.517982	29.219546
347.200341	18326.617438	29.224564
347.565639	18381.181034	29.229581
348.081389	18403.461199	29.234599
348.390985	18429.744161	29.239616
348.955308	18452.010062	29.244634
349.185006	18509.495004	29.249652
349.765169	18544.476322	29.254669
350.563382	18565.261563	29.259687
350.409441	18588.897772	29.264704
351.087889	18610.315979	29.269722
351.239002	18652.643934	29.274740
351.485360	18679.624947	29.279757
351.791089	18694.379364	29.284775
352.106575	18736.488088	29.289792
352.415757	18767.719242	29.294810
353.156232	18801.468855	29.299828
353.114500	18834.329551	29.304845
353.675556	18866.200189	29.309863
353.995178	18906.836514	29.314880
354.540155	18925.247761	29.319898
355.411029	18967.017861	29.324916
355.108452	18998.144036	29.329933
355.568895	19029.722679	29.334951
355.662666	19076.580141	29.339968
356.095741	19089.453962	29.344986
356.224151	19133.150312	29.350004
356.809010	19170.791241	29.355021
357.451118	19193.202917	29.360039
357.294410	19232.514332	29.365056
357.808704	19253.378874	29.370074
358.077824	19307.498018	29.375092
358.363566	19342.340524	29.380109
359.166209	19374.835826	29.385127
359.062310	19427.186985	29.390144
359.681699	19448.759479	29.395162
360.198123	19487.157994	29.400180
360.306487	19520.211201	29.405197
360.790936	19554.386102	29.410215
361.192350	19602.962778	29.415232
361.518501	19621.439327	29.420250
362.077099	19651.973654	29.425268
362.214068	19688.137146	29.430285
362.736558	19710.813608	29.435303
362.960343	19754.945078	29.440320
363.717604	19786.162457	29.445338
364.613986	19800.534985	29.450356
364.492607	19846.805970	29.455373
364.928579	19878.949856	29.460391
365.119864	19898.265505	29.465408
365.565440	19900.217458	29.470426
365.667761	19947.860960	29.475444
366.017765	19997.411970	29.480461
366.807591	20020.333153	29.485479
367.142772	20027.062172	29.490496
367.582266	20050.849909	29.495514
367.755924	20088.417418	29.500532
368.006548	20127.651054	29.505549
368.378110	20131.617161	29.510567
368.720488	20174.696106	29.515584
369.025251	20206.926933	29.520602
369.064922	20221.958388	29.525620
369.349433	20281.522736	29.530637
369.570434	20277.052108	29.535655
369.913778	20312.605939	29.540672
370.334396	20354.788113	29.545690
370.706212	20400.998082	29.550708
370.805901	20444.015357	29.555725
371.163904	20463.906280	29.560743
371.416427	20523.418456	29.565760
371.985675	20558.940225	29.570778
372.569613	20597.907103	29.575796
372.895857	20639.426187	29.580813
373.346949	20670.886554	29.585831
373.719589	20712.666136	29.590848
373.945091	20762.682954	29.595866
374.790257	20805.097222	29.600884
374.811343	20817.641633	29.605901
375.487089	20848.418915	29.610919
375.415431	20905.386585	29.615936
376.189726	20951.113856	29.620954
376.684215	20974.143477	29.625972
377.064285	21000.368440	29.630989
377.611686	21040.926656	29.636007
377.616735	21068.192613	29.641024
377.924141	21107.300953	29.646042
378.604010	21145.900158	29.651060
378.673211	21211.495282	29.656077
379.299359	21219.910761	29.661095
379.983463	21250.026895	29.666112
380.422688	21272.200614	29.671130
381.139363	21322.576214	29.676148
381.540469	21362.760551	29.681165
381.773959	21382.174997	29.686183
382.240761	21394.660399	29.691200
382.507974	21440.086562	29.696218
382.811670	21463.440019	29.701236
382.776392	21490.346021	29.706253
383.440527	21516.100811	29.711271
383.625016	21572.886567	29.716288
383.830739	21595.105596	29.721306
384.280178	21645.879442	29.726324
384.479060	21695.867201	29.731341
384.919673	21717.872604	29.736359
385.281684	21765.264011	29.741376
385.846126	21794.415616	29.746394
386.427507	21825.522434	29.751412
386.520185	21860.982255	29.756429
386.842369	21898.322795	29.761447
387.645436	21933.906615	29.766464
387.805066	21965.148002	29.771482
388.036691	22010.231618	29.776500
388.432649	22049.942365	29.781517
389.279515	22075.689905	29.786535
389.615143	22108.953489	29.791552
389.849344	22153.171575	29.796570
390.516197	22196.403938	29.801588
390.813118	22226.215324	29.806605
391.394280	22255.926207	29.811623
391.695324	22279.653298	29.816640
391.833460	22309.303459	29.821658
392.199572	22348.272582	29.826676
392.799663	22383.474695	29.831693
392.954609	22418.308994	29.836711
393.407860	22447.703974	29.841728
393.580319	22465.105513	29.846746
394.280260	22502.451212	29.851764
394.175340	22542.118173	29.856781
394.426321	22582.476862	29.861799
394.812091	22615.936543	29.866816
395.003614	22666.079762	29.871834
395.352306	22690.105412	29.876852
395.833824	22745.331023	29.881869
396.300466	22779.354687	29.886887
396.869605	22813.743013	29.891904
397.469533	22851.296775	29.896922
398.004013	22891.585727	29.901940
398.304567	22926.931482	29.906957
398.845643	22956.591898	29.911975
399.364926	23008.898648	29.916992
399.530228	23032.363870	29.922010
400.134616	23044.335892	29.927028
400.364264	23089.889405	29.932045
400.957860	23125.880864	29.937063
401.081888	23164.627011	29.942080
401.473107	23201.511303	29.947098
401.945274	23234.693080	29.952116
402.570371	23279.164879	29.957133
402.599789	23325.392205	29.962151
403.154853	23355.117233	29.967168
403.423116	23416.412362	29.972186
404.162854	23442.383090	29.977204
404.101719	23476.213140	29.982221
404.541137	23505.700551	29.987239
404.985931	23565.841358	29.992256
405.649832	23606.301417	29.997274
406.241849	23638.808318	30.002292
406.337266	23677.005398	30.007309
406.714417	23712.393757	30.012327
407.334405	23747.072004	30.017344
407.864471	23783.562549	30.022362
408.452649	23825.891354	30.027380
408.511608	23856.421327	30.032397
408.906755	23892.174451	30.037415
409.455980	23941.795695	30.042432
409.548081	23989.810300	30.047450
410.583718	24014.396025	30.052468
410.351253	24049.315045	30.057485
410.833481	24097.790541	30.062503
411.346727	24133.918837	30.067520
411.811020	24187.699914	30.072538
412.425102	24219.701331	30.077556
412.593143	24260.274833	30.082573
412.993105	24287.310500	30.087591
413.678170	24332.798450	30.092608
413.756564	24382.424663	30.097626
414.384009	24423.570689	30.102644
414.868774	24454.808718	30.107661
415.304271	24492.519448	30.112679
415.682429	24525.457566	30.117696
415.796580	24572.803237	30.122714
415.996560	24620.395021	30.127732
416.290867	24674.521072	30.132749
416.759910	24710.270029	30.137767
417.143694	24743.152457	30.142784
417.493527	24802.567565	30.147802
418.094599	24851.282601	30.152820
418.639310	24894.701337	30.157837
418.925408	24943.229003	30.162855
419.441037	24986.964976	30.167872
420.119132	25040.183658	30.172890
420.808691	25064.539543	30.177908
420.708936	25113.126705	30.182925
421.122337	25133.244235	30.187943
421.683641	25185.710051	30.192960
421.571201	25243.296749	30.197978
421.892207	25285.249194	30.202996
422.498375	25316.687934	30.208013
422.900152	25346.761885	30.213031
423.378557	25416.099556	30.218048
423.613176	25455.775611	30.223066
424.037632	25500.193379	30.228084
424.885814	25539.564868	30.233101
425.317261	25568.286142	30.238119
425.864284	25610.794936	30.243136
426.278448	25664.268893	30.248154
426.721887	25691.752171	30.253172
426.961881	25731.435867	30.258189
427.198319	25798.225924	30.263207
427.757879	25826.380889	30.268224
428.297683	25870.260216	30.273242
428.553258	25923.705998	30.278260
428.986969	25989.092365	30.283277
429.333116	26016.131800	30.288295
430.020104	26050.352729	30.293312
430.232792	26124.871420	30.298330
430.811684	26177.566041	30.303348
431.225947	26228.834146	30.308365
431.539502	26264.383419	30.313383
432.083746	26293.412123	30.318400
432.462497	26370.067927	30.323418
432.550386	26421.936129	30.328436
433.203602	26473.334224	30.333453
433.691176	26510.466849	30.338471
434.427287	26566.900754	30.343488
434.352272	26605.621422	30.348506
435.004346	26654.290630	30.353524
435.582665	26709.797044	30.358541
436.130839	26763.553507	30.363559
436.783466	26792.872658	30.368576
436.749891	26839.706583	30.373594
437.651287	26889.740320	30.378612
438.172522	26941.686747	30.383629
438.636387	26965.899723	30.388647
439.613752	27000.973452	30.393664
439.797036	27051.399099	30.398682
440.437943	27093.706856	30.403700
441.013507	27136.649985	30.408717
441.045553	27162.629797	30.413735
441.645163	27193.098534	30.418752
441.949966	27239.224795	30.423770
441.988063	27290.211296	30.428788
442.582389	27336.037678	30.433805
442.963653	27381.779528	30.438823
443.334696	27409.473083	30.443840
443.549970	27474.516443	30.448858
443.865737	27524.798594	30.453876
444.674694	27562.601104	30.458893
445.035398	27599.736555	30.463911
445.721549	27649.383863	30.468928
445.987060	27705.232197	30.473946
446.615752	27760.497152	30.478964
447.058669	27782.950072	30.483981
447.287000	27841.154739	30.488999
448.128966	27873.366686	30.494016
448.606452	27924.897531	30.499034
448.959772	27970.361704	30.504052
449.545877	28010.797808	30.509069
449.510314	28050.901438	30.514087
450.306100	28084.748914	30.519104
450.424872	28131.207944	30.524122
450.993031	28176.324919	30.529140
451.481322	28223.316129	30.534157
451.764467	28252.142120	30.539175
452.028788	28284.415565	30.544192
452.651312	28323.830766	30.549210
452.800721	28379.132728	30.554228
453.184490	28450.665243	30.559245
453.401920	28475.572396	30.564263
454.045893	28524.980029	30.569280
454.359649	28576.905758	30.574298
454.598996	28639.359978	30.579316
455.217128	28694.708540	30.584333
455.461643	28743.905217	30.589351
456.332699	28790.882064	30.594368
456.560333	28843.936261	30.599386
457.207151	28895.442045	30.604404
457.745532	28955.211078	30.609421
458.091298	29027.165470	30.614439
459.068536	29062.136204	30.619456
459.545268	29113.424703	30.624474
460.024922	29147.831181	30.629492
460.631360	29207.993595	30.634509
460.973726	29269.458406	30.639527
461.688671	29309.447299	30.644544
462.328839	29332.409050	30.649562
462.557650	29377.146781	30.654580
463.395695	29413.188456	30.659597
463.401318	29457.171526	30.664615
463.503760	29509.065574	30.669632
463.842058	29554.823457	30.674650
464.562281	29608.076218	30.679668
465.231840	29657.599585	30.684685
465.218081	29718.172199	30.689703
466.193689	29766.859884	30.694720
466.592442	29816.062529	30.699738
467.039589	29857.428084	30.704756
467.721455	29905.890250	30.709773
467.730388	29947.574452	30.714791
468.478142	29994.120711	30.719808
468.989462	30044.958334	30.724826
469.416962	30090.866932	30.729844
470.002251	30141.282541	30.734861
470.391660	30198.269862	30.739879
471.422003	30225.407957	30.744896
471.912219	30261.915789	30.749914
472.130405	30308.559833	30.754932
473.063243	30361.259304	30.759949
473.389520	30398.589437	30.764967
473.885281	30434.850666	30.769984
474.080983	30485.218067	30.775002
474.299184	30523.537913	30.780020
474.988135	30551.729744	30.785037
475.315528	30608.299641	30.790055
475.722230	30660.030158	30.795072
475.754358	30706.346386	30.800090
476.054272	30746.252588	30.805108
476.656872	30805.938544	30.810125
476.887553	30872.317086	30.815143
477.503952	30937.455501	30.820160
477.746189	30992.397167	30.825178
477.746672	31044.012959	30.830196
478.577829	31097.482262	30.835213
479.089362	31177.279542	30.840231
479.547269	31248.082651	30.845248
480.029715	31305.348464	30.850266
481.066531	31338.588367	30.855284
481.665516	31401.545207	30.860301
481.929253	31473.920794	30.865319
482.409911	31505.792259	30.870336
483.017415	31548.662234	30.875354
483.227076	31599.942267	30.880372
483.806093	31653.552726	30.885389
484.272208	31726.955922	30.890407
484.783163	31755.904702	30.895424
485.525712	31791.932403	30.900442
485.612380	31849.066629	30.905460
486.471599	31901.773470	30.910477
486.539074	31963.548760	30.915495
487.346147	32005.017716	30.920512
487.570607	32055.451157	30.925530
487.982513	32118.517202	30.930548
488.520958	32161.264434	30.935565
488.943207	32231.026865	30.940583
489.510167	32273.066133	30.945600
490.146726	32333.297499	30.950618
490.387527	32402.428066	30.955636
490.951511	32462.403702	30.960653
491.624137	32516.878403	30.965671
492.039635	32552.314946	30.970688
492.436006	32619.448864	30.975706
492.576493	32686.262492	30.980724
493.680120	32729.744345	30.985741
494.115824	32785.054057	30.990759
494.312670	32850.824183	30.995776
495.049192	32912.508080	31.000794
495.619688	32968.553296	31.005812
496.407732	33009.532450	31.010829
496.582534	33071.167716	31.015847
497.018185	33139.830461	31.020864
497.631708	33187.246660	31.025882
497.938519	33249.677894	31.030900
498.579314	33299.071242	31.035917
498.909118	33370.920021	31.040935
499.442945	33434.301939	31.045952
499.884912	33506.508196	31.050970
499.962434	33566.012666	31.055988
500.671565	33609.331546	31.061005
501.031626	33685.347629	31.066023
501.431421	33768.418614	31.071040
502.389839	33821.928869	31.076058
502.711526	33880.848235	31.081076
503.293767	33934.159091	31.086093
503.893300	34016.870120	31.091111
504.539078	34093.260404	31.096128
505.046557	34142.435193	31.101146
505.827299	34202.059136	31.106164
506.108872	34247.321236	31.111181
506.910158	34326.151052	31.116199
507.530321	34390.247847	31.121216
508.102525	34435.948329	31.126234
508.250550	34483.539568	31.131252
509.123529	34539.713362	31.136269
509.254921	34607.075324	31.141287
510.096173	34649.500933	31.146304
510.811778	34712.636553	31.151322
510.873533	34770.002094	31.156340
511.230581	34815.155368	31.161357
511.848138	34877.954380	31.166375
512.339315	34933.173326	31.171392
512.606769	35009.592198	31.176410
513.398790	35074.234202	31.181428
514.152225	35116.183203	31.186445
514.602333	35155.831664	31.191463
515.152490	35243.444240	31.196480
515.598077	35301.290824	31.201498
515.660982	35353.723043	31.206516
516.610864	35390.582151	31.211533
517.113808	35442.216206	31.216551
517.226833	35517.608869	31.221568
518.016628	35577.030850	31.226586
518.254179	35625.758946	31.231604
518.807977	35657.707903	31.236621
519.313982	35735.870173	31.241639
519.735153	35809.001195	31.246656
520.468521	35850.245267	31.251674
520.718529	35922.764466	31.256692
521.778111	35980.395092	31.261709
521.747581	36028.206142	31.266727
522.339337	36088.940531	31.271744
522.650603	36151.255047	31.276762
522.875412	36224.732609	31.281780
523.445649	36283.407487	31.286797
524.079760	36355.713537	31.291815
524.237103	36435.069317	31.296832
525.086540	36498.930749	31.301850
525.480604	36571.296256	31.306868
526.234541	36648.045731	31.311885
526.740361	36725.249908	31.316903
527.168576	36780.071603	31.321920
527.880791	36850.542795	31.326938
528.237135	36919.993806	31.331956
528.782989	37006.375589	31.336973
529.554213	37063.669202	31.341991
530.219306	37124.704263	31.347008
531.441216	37197.573022	31.352026
531.659417	37256.318714	31.357044
531.982364	37306.078686	31.362061
532.930365	37370.706425	31.367079
533.467611	37447.147993	31.372096
534.299989	37503.536679	31.377114
534.378363	37573.294913	31.382132
535.111683	37614.397912	31.387149
535.931719	37682.468794	31.392167
536.145172	37728.606226	31.397184
536.986025	37765.305231	31.402202
537.549613	37834.933845	31.407220
537.972781	37906.877065	31.412237
538.764894	37952.244143	31.417255
539.135495	37994.061187	31.422272
539.748750	38059.239017	31.427290
540.071911	38130.432775	31.432308
540.284620	38204.071942	31.437325
540.824182	38248.282243	31.442343
541.145156	38305.376479	31.447360
541.777888	38371.098197	31.452378
542.140036	38463.605125	31.457396
542.547964	38521.907036	31.462413
543.137150	38591.294499	31.467431
543.901143	38662.370209	31.472448
544.679110	38729.855531	31.477466
544.846506	38815.434323	31.482484
545.297226	38860.045834	31.487501
546.141000	38928.669820	31.492519
546.479820	39014.353794	31.497536
546.787319	39068.713234	31.502554
547.284645	39132.686397	31.507572
547.705815	39223.041350	31.512589
548.293452	39304.715262	31.517607
548.641121	39379.716149	31.522624
549.712116	39438.564816	31.527642
550.022000	39522.718953	31.532660
550.552020	39586.713572	31.537677
551.396902	39664.729687	31.542695
552.001691	39742.331308	31.547712
552.706463	39790.220285	31.552730
553.393298	39859.217753	31.557748
553.677604	39935.156169	31.562765
554.007873	39986.841307	31.567783
554.534082	40033.778842	31.572800
555.112969	40117.724032	31.577818
555.645523	40187.335290	31.582836
556.258633	40263.861491	31.587853
556.857955	40321.010810	31.592871
557.267528	40384.232762	31.597888
558.126605	40451.505958	31.602906
558.396480	40524.554908	31.607924
558.624394	40597.415389	31.612941
559.384915	40660.286799	31.617959
559.908822	40754.369506	31.622976
560.577031	40815.839503	31.627994
561.353240	40890.434969	31.633012
561.584465	40949.976461	31.638029
562.377494	41044.322384	31.643047
562.696609	41131.635687	31.648064
563.151423	41187.706856	31.653082
563.700411	41255.476143	31.658100
564.096440	41349.797683	31.663117
564.740683	41433.384628	31.668135
565.071814	41507.295426	31.673152
565.915857	41590.382932	31.678170
565.962595	41679.022217	31.683188
566.695518	41767.463369	31.688205
567.916766	41839.858565	31.693223
568.221177	41926.136440	31.698240
569.276241	42025.630358	31.703258
569.717803	42085.667958	31.708276
570.449868	42140.594617	31.713293
571.509914	42218.819737	31.718311
571.595365	42317.853544	31.723328
572.356587	42385.036402	31.728346
573.228111	42454.837079	31.733364
573.455479	42519.292887	31.738381
574.059009	42597.661317	31.743399
574.543811	42680.431153	31.748416
574.949332	42751.307435	31.753434
575.531614	42834.708987	31.758452
576.616584	42915.019542	31.763469
577.284203	42970.625401	31.768487
577.609191	43043.498534	31.773504
578.021067	43127.295741	31.778522
578.625976	43205.521326	31.783540
579.494985	43271.515311	31.788557
580.685094	43345.209568	31.793575
580.864750	43412.448047	31.798592
581.382291	43459.714658	31.803610
582.280102	43530.203266	31.808628
582.544973	43604.992113	31.813645
583.414515	43680.281193	31.818663
583.568967	43755.663434	31.823680
584.300256	43805.793625	31.828698
584.880179	43876.200316	31.833716
585.391744	43957.156268	31.838733
585.974790	44022.518288	31.843751
586.432747	44086.562669	31.848768
587.083087	44159.143393	31.853786
587.749622	44235.320638	31.858804
588.184749	44305.831805	31.863821
588.835220	44374.388240	31.868839
589.203571	44465.039851	31.873856
589.859020	44533.892811	31.878874
590.445412	44593.412709	31.883892
590.271114	44668.679332	31.888909
591.220767	44762.680691	31.893927
592.037959	44836.960254	31.898944
592.659044	44890.284418	31.903962
593.181220	44948.171238	31.908980
593.226258	45034.620159	31.913997
594.002557	45122.442007	31.919015
594.541361	45202.937971	31.924032
595.395109	45280.203050	31.929050
595.939462	45359.012873	31.934068
596.403771	45422.912438	31.939085
597.067310	45493.301994	31.944103
597.584218	45580.616349	31.949120
598.163140	45665.246737	31.954138
599.261559	45749.403372	31.959156
599.625939	45822.135708	31.964173
600.143435	45873.244499	31.969191
600.273268	45962.941974	31.974208
601.088676	46062.219402	31.979226
602.013040	46138.532366	31.984244
602.118196	46213.029747	31.989261
602.886059	46304.432603	31.994279
603.325451	46404.998987	31.999296
604.504864	46480.153537	32.004314
604.849132	46553.646644	32.009332
605.333440	46640.999762	32.014349
605.945860	46740.945794	32.019367
606.373318	46828.754366	32.024384
607.075499	46911.163036	32.029402
607.647550	47006.902036	32.034420
608.136608	47100.021940	32.039437
609.253653	47176.370468	32.044455
609.597613	47271.608569	32.049472
610.131862	47353.819586	32.054490
610.462886	47437.646425	32.059508
610.961582	47535.522066	32.064525
612.328869	47644.403945	32.069543
612.688394	47742.609929	32.074560
613.272095	47828.723881	32.079578
614.298890	47892.554772	32.084596
615.039424	48005.637613	32.089613
615.505731	48107.048591	32.094631
616.492394	48176.551798	32.099648
616.833057	48239.243619	32.104666
617.948171	48335.720677	32.109684
617.787559	48417.236434	32.114701
618.954635	48489.830756	32.119719
619.236988	48601.230870	32.124736
620.266077	48678.433655	32.129754
620.876601	48733.226217	32.134772
621.352201	48822.504474	32.139789
622.122320	48904.885399	32.144807
622.429598	48999.475170	32.149824
623.433935	49062.252733	32.154842
624.150665	49135.050227	32.159860
624.458691	49240.664841	32.164877
624.938895	49334.817214	32.169895
625.639610	49417.502352	32.174912
625.874251	49494.097592	32.179930
626.717597	49574.922005	32.184948
627.229781	49677.549597	32.189965
627.848099	49749.194139	32.194983
628.785994	49826.198778	32.200000
629.195674	49930.338342	32.205018
630.045212	50013.961501	32.210036
630.442932	50099.134399	32.215053
631.105558	50193.043003	32.220071
631.566423	50273.680925	32.225088
632.270822	50356.587442	32.230106
632.945246	50448.941639	32.235124
633.228153	50538.765071	32.240141
633.999799	50618.446779	32.245159
634.535391	50701.316358	32.250176
635.076657	50769.996295	32.255194
635.713799	50864.654556	32.260212
636.186026	50981.664919	32.265229
636.875887	51062.969450	32.270247
637.309008	51142.661886	32.275264
637.508970	51222.424743	32.280282
638.528720	51325.637427	32.285300
639.062661	51445.252206	32.290317
639.904140	51539.412654	32.295335
640.299231	51631.970297	32.300352
641.207150	51716.295550	32.305370
642.114425	51807.679875	32.310388
642.905901	51921.023947	32.315405
643.592136	52010.588707	32.320423
644.243205	52089.159492	32.325440
644.893549	52180.025855	32.330458
646.033525	52270.808625	32.335476
646.454179	52375.190247	32.340493
647.269827	52461.539538	32.345511
647.888322	52528.886535	32.350528
648.458832	52618.413233	32.355546
649.188813	52703.296495	32.360564
649.917746	52815.039091	32.365581
650.593263	52884.272938	32.370599
651.331551	52971.777471	32.375616
652.015238	53069.739452	32.380634
652.908407	53168.523268	32.385652
653.182573	53238.235267	32.390669
654.107855	53300.367083	32.395687
654.582177	53405.023361	32.400704
655.113006	53500.662872	32.405722
656.145790	53592.303415	32.410740
656.220288	53670.476828	32.415757
657.057938	53747.077915	32.420775
657.847596	53840.591733	32.425792
658.303321	53942.581864	32.430810
659.158706	54020.634040	32.435828
659.485361	54113.821346	32.440845
660.403502	54211.617729	32.445863
661.053557	54299.673487	32.450880
661.519882	54392.655865	32.455898
662.262089	54475.744471	32.460916
662.919701	54580.667420	32.465933
663.324870	54687.319362	32.470951
663.959575	54779.460842	32.475968
664.473122	54877.510600	32.480986
665.481332	54984.254097	32.486004
666.027151	55085.388807	32.491021
666.726087	55179.220974	32.496039
667.289562	55276.000989	32.501056
667.624122	55398.500262	32.506074
668.717927	55477.138035	32.511092
669.255500	55568.876008	32.516109
670.179471	55661.289765	32.521127
670.577031	55762.711493	32.526144
671.095606	55866.293380	32.531162
672.011707	55965.690978	32.536180
673.018794	56063.658866	32.541197
673.642818	56152.378025	32.546215
674.796050	56247.713436	32.551232
674.888021	56349.011768	32.556250
675.547164	56440.348356	32.561268
676.379105	56545.594238	32.566285
677.130536	56637.851562	32.571303
678.074340	56697.729335	32.576320
678.608252	56800.985091	32.581338
679.666740	56868.798859	32.586356
679.646385	56950.134825	32.591373
680.331488	57027.279439	32.596391
680.715531	57124.755302	32.601408
681.081639	57210.223764	32.606426
682.125111	57313.770829	32.611444
682.534160	57415.590924	32.616461
683.271306	57519.941531	32.621479
684.157185	57595.191322	32.626496
684.659634	57701.369726	32.631514
685.219982	57794.997197	32.636532
685.597141	57904.685118	32.641549
686.387098	58007.734311	32.646567
687.406596	58110.234338	32.651584
687.747089	58210.869346	32.656602
688.733091	58325.589664	32.661620
689.195243	58429.352316	32.666637
689.691898	58518.905623	32.671655
690.413722	58633.412290	32.676672
691.461834	58754.020108	32.681690
692.547686	58847.047636	32.686708
693.085039	58942.453561	32.691725
693.670910	59044.644592	32.696743
694.720449	59147.290353	32.701760
695.900889	59256.827816	32.706778
696.872690	59335.564341	32.711796
697.890435	59419.234950	32.716813
698.230294	59522.309473	32.721831
699.238111	59626.955055	32.726848
699.421631	59694.670259	32.731866
700.085594	59795.026065	32.736884
700.412068	59903.994071	32.741901
701.283988	59992.708479	32.746919
702.065173	60072.705294	32.751936
702.219405	60192.799628	32.756954
702.993269	60308.210964	32.761972
703.467742	60410.332602	32.766989
703.857712	60508.525523	32.772007
704.516525	60607.439156	32.777024
705.005415	60736.511689	32.782042
705.625049	60867.762587	32.787060
706.449330	60993.672275	32.792077
707.169407	61116.231716	32.797095
707.874192	61238.611166	32.802112
708.437694	61347.914403	32.807130
709.316097	61454.391962	32.812148
710.068268	61578.415047	32.817165
710.819781	61714.319842	32.822183
712.048015	61831.939953	32.827200
712.540091	61943.590163	32.832218
713.192789	62040.470602	32.837236
714.245974	62150.759035	32.842253
714.895552	62276.054660	32.847271
715.783909	62374.547245	32.852288
716.516933	62505.075945	32.857306
717.465855	62627.158069	32.862324
718.473850	62721.815380	32.867341
719.093268	62824.367713	32.872359
719.711733	62918.129638	32.877376
720.021933	63033.272922	32.882394
720.948987	63122.933708	32.887412
721.689131	63229.437135	32.892429
722.360981	63353.193645	32.897447
722.993684	63443.163580	32.902464
723.636324	63555.834312	32.907482
724.308558	63656.947448	32.912500
725.378317	63759.998953	32.917517
726.085127	63878.488131	32.922535
726.905872	63983.054510	32.927552
727.279484	64068.538339	32.932570
727.958491	64157.814869	32.937588
728.808860	64281.187277	32.942605
728.812004	64388.526359	32.947623
729.785201	64496.028151	32.952640
730.260691	64622.024311	32.957658
730.675715	64725.890394	32.962676
731.327183	64843.477831	32.967693
732.002022	64972.375969	32.972711
733.038018	65091.791191	32.977728
733.423880	65219.215327	32.982746
734.506027	65338.156632	32.987764
735.353380	65465.038349	32.992781
735.939098	65602.443944	32.997799
736.818917	65722.704011	33.002816
737.580237	65840.765723	33.007834
738.126362	65942.018427	33.012852
739.227257	66063.805243	33.017869
739.511299	66203.293687	33.022887
740.169788	66331.425562	33.027904
741.043746	66462.525155	33.032922
741.765152	66572.298089	33.037940
742.682604	66691.912843	33.042957
743.492612	66840.730905	33.047975
744.425631	66972.614127	33.052992
745.009088	67077.665286	33.058010
746.191171	67214.439497	33.063028
747.119274	67334.277448	33.068045
747.726221	67444.554329	33.073063
748.343662	67539.096107	33.078080
749.455689	67680.771399	33.083098
749.831765	67810.937672	33.088116
751.133327	67932.348343	33.093133
751.409897	68054.719182	33.098151
752.630834	68163.103160	33.103168
753.059082	68306.558207	33.108186
753.822590	68423.034899	33.113204
754.556474	68532.879353	33.118221
755.299320	68680.033779	33.123239
756.222839	68780.504691	33.128256
756.802440	68908.431580	33.133274
757.543770	69032.779665	33.138292
758.546728	69155.801942	33.143309
758.609692	69281.976760	33.148327
759.848383	69394.113094	33.153344
760.460187	69530.396087	33.158362
760.980979	69653.045720	33.163380
762.274117	69791.689812	33.168397
762.804883	69918.119946	33.173415
763.641442	70026.564409	33.178432
764.626474	70173.449076	33.183450
765.406086	70306.744281	33.188468
766.236787	70414.806055	33.193485
766.820250	70519.823932	33.198503
767.838991	70632.471043	33.203520
768.713078	70764.590233	33.208538
769.722334	70882.026274	33.213556
770.260232	71009.056074	33.218573
771.046943	71148.924439	33.223591
771.656854	71242.864556	33.228608
772.245875	71369.900723	33.233626
773.057889	71496.572053	33.238644
774.015211	71632.571304	33.243661
774.380519	71768.277182	33.248679
775.246640	71866.439229	33.253696
775.797231	71972.348589	33.258714
776.488298	72109.950253	33.263732
777.326603	72230.431629	33.268749
778.131144	72348.466000	33.273767
778.877703	72465.378806	33.278784
779.530275	72578.589904	33.283802
780.623389	72712.474428	33.288820
781.767373	72830.910669	33.293837
782.095893	72936.931045	33.298855
782.966829	73039.226627	33.303872
784.085530	73170.871442	33.308890
784.771095	73302.626531	33.313908
785.663617	73404.888681	33.318925
785.967520	73530.296522	33.323943
786.906330	73657.022976	33.328960
787.733130	73767.979499	33.333978
788.211480	73894.916183	33.338996
788.959875	74033.772768	33.344013
789.417523	74182.479496	33.349031
790.280093	74301.520467	33.354048
790.911834	74453.735106	33.359066
791.628926	74599.391902	33.364084
792.751343	74711.581820	33.369101
793.211552	74869.392427	33.374119
794.034069	75008.660407	33.379136
794.884393	75125.330264	33.384154
795.462389	75288.588115	33.389172
796.414072	75416.549586	33.394189
797.002123	75563.941596	33.399207
798.494843	75716.294869	33.404224
799.274400	75860.678748	33.409242
799.286628	76007.764128	33.414260
800.281403	76149.382456	33.419277
801.035436	76295.961527	33.424295
802.021346	76429.102664	33.429312
802.518255	76588.658815	33.434330
803.531162	76765.901726	33.439348
804.759775	76918.363945	33.444365
805.395725	77055.980971	33.449383
806.315393	77183.091697	33.454400
807.617791	77342.242073	33.459418
808.020985	77504.887669	33.464436
809.048713	77637.004716	33.469453
810.056986	77788.206557	33.474471
810.681071	77926.710104	33.479488
811.957063	78043.812276	33.484506
812.766362	78195.909912	33.489524
813.378358	78345.226738	33.494541
814.019245	78483.427434	33.499559
814.836632	78614.003931	33.504576
815.831172	78755.500006	33.509594
816.604474	78914.470848	33.514612
817.603684	79030.662610	33.519629
818.378583	79185.467105	33.524647
818.922972	79330.646347	33.529664
820.003989	79452.892368	33.534682
820.578886	79590.275994	33.539700
821.629755	79719.321451	33.544717
822.706224	79873.302982	33.549735
823.267149	80019.546604	33.554752
824.194949	80161.081655	33.559770
824.759204	80284.840738	33.564788
825.650339	80435.839676	33.569805
826.511342	80587.837673	33.574823
827.206847	80714.132857	33.579840
828.296939	80848.017210	33.584858
828.838693	81007.654816	33.589876
829.854940	81154.349373	33.594893
830.324720	81276.409048	33.599911
831.605182	81385.874382	33.604928
832.568609	81531.783129	33.609946
833.033325	81661.208609	33.614964
833.801711	81780.546023	33.619981
834.492139	81939.242182	33.624999
835.416892	82073.977169	33.630016
836.402320	82208.683968	33.635034
836.969151	82350.387358	33.640052
837.780483	82465.362892	33.645069
838.589023	82615.795536	33.650087
839.108601	82758.666915	33.655104
839.935261	82910.793856	33.660122
840.835602	83056.634342	33.665140
841.841632	83178.432332	33.670157
842.409348	83346.527392	33.675175
843.486654	83507.960466	33.680192
844.525292	83654.667614	33.685210
845.249082	83800.523063	33.690228
845.977392	83933.289865	33.695245
846.896336	84094.070031	33.700263
847.813959	84247.734516	33.705280
848.961589	84403.544631	33.710298
849.654643	84547.651235	33.715316
850.693753	84687.146618	33.720333
850.952763	84837.267184	33.725351
851.816178	84995.291904	33.730368
852.972693	85149.055868	33.735386
853.532509	85310.460635	33.740404
854.805399	85455.559056	33.745421
855.927160	85620.226305	33.750439
856.259642	85779.609428	33.755456
857.177220	85914.861854	33.760474
858.139563	86064.595943	33.765492
859.073131	86243.527605	33.770509
859.691218	86414.673781	33.775527
860.383452	86553.700009	33.780544
861.294811	86694.892663	33.785562
862.282612	86877.508884	33.790580
863.190640	87058.032821	33.795597
864.093726	87216.749566	33.800615
864.720932	87369.793244	33.805632
865.934119	87524.474814	33.810650
866.918294	87695.981283	33.815668
867.941499	87848.235100	33.820685
869.242141	87994.547079	33.825703
870.139225	88138.237503	33.830720
871.410723	88283.100826	33.835738
871.901074	88441.305642	33.840756
872.986479	88590.162553	33.845773
874.042425	88718.334422	33.850791
874.451840	88874.442158	33.855808
875.473941	89035.973730	33.860826
876.198372	89177.579325	33.865844
877.038142	89326.025892	33.870861
878.053724	89483.530919	33.875879
878.389332	89648.040172	33.880896
879.638155	89780.767282	33.885914
880.412867	89947.268975	33.890932
881.216909	90106.489974	33.895949
882.084262	90250.021082	33.900967
882.735506	90412.888932	33.905984
883.928523	90562.006353	33.911002
884.478387	90729.240441	33.916020
885.366947	90888.073074	33.921037
886.188115	91038.204106	33.926055
887.356159	91197.017977	33.931072
887.957912	91362.203974	33.936090
888.787810	91512.102421	33.941108
889.768598	91672.007203	33.946125
890.500658	91805.368910	33.951143
891.341303	91959.185621	33.956160
892.180067	92111.535450	33.961178
893.049295	92262.419356	33.966196
893.733103	92417.347078	33.971213
895.003786	92581.532438	33.976231
895.358614	92753.185955	33.981248
896.479685	92916.018689	33.986266
897.320954	93086.081737	33.991284
898.256562	93237.334220	33.996301
898.993846	93395.360492	34.001319
899.710508	93571.504141	34.006336
900.584233	93752.160908	34.011354
901.454096	93933.712037	34.016372
902.647701	94091.781455	34.021389
903.693171	94242.079106	34.026407
904.387899	94416.257916	34.031424
905.234407	94608.406379	34.036442
906.239435	94780.447992	34.041460
906.738569	94932.593296	34.046477
908.084644	95109.574615	34.051495
908.637318	95316.271010	34.056512
909.642937	95503.469821	34.061530
910.909080	95658.891849	34.066548
912.048415	95815.057354	34.071565
913.024066	95998.847068	34.076583
913.660167	96203.625733	34.081600
914.763791	96366.041503	34.086618
915.777226	96520.801841	34.091636
916.747966	96682.760609	34.096653
918.184094	96867.436585	34.101671
918.730146	97051.077263	34.106688
919.912078	97211.352604	34.111706
920.459361	97374.556849	34.116724
921.471915	97559.706738	34.121741
922.598282	97737.249733	34.126759
923.028494	97909.180392	34.131776
924.005561	98084.535071	34.136794
924.975659	98280.869723	34.141812
925.741465	98459.971318	34.146829
926.639412	98623.239850	34.151847
927.364186	98801.090997	34.156864
928.199898	99007.891965	34.161882
929.237602	99186.257585	34.166900
930.102805	99374.983959	34.171917
931.564700	99534.759678	34.176935
932.035225	99734.885196	34.181952
932.993400	99936.235864	34.186970
934.136460	100117.300157	34.191988
935.060798	100300.737828	34.197005
936.609595	100457.555082	34.202023
937.365273	100655.786025	34.207040
938.232050	100852.297245	34.212058
939.199604	101024.603801	34.217076
940.304386	101189.089423	34.222093
941.168758	101379.660601	34.227111
941.823362	101573.274992	34.232128
943.206904	101731.792476	34.237146
944.088388	101937.476806	34.242164
944.476082	102117.230412	34.247181
945.971935	102265.343593	34.252199
946.682901	102461.070013	34.257216
947.533952	102647.214862	34.262234
948.263962	102836.369354	34.267252
949.273241	103004.997767	34.272269
950.509165	103194.394275	34.277287
951.245400	103388.078655	34.282304
952.389396	103551.287857	34.287322
953.309752	103724.760164	34.292340
954.133052	103894.856040	34.297357
955.589338	104064.455985	34.302375
955.819749	104249.860226	34.307392
956.995031	104421.155107	34.312410
957.802022	104586.034739	34.317428
958.481652	104781.271212	34.322445
959.541904	104956.254648	34.327463
960.000643	105167.669916	34.332480
961.244827	105331.715989	34.337498
962.194547	105517.346152	34.342516
962.787222	105712.983918	34.347533
963.965748	105905.088215	34.352551
964.609619	106115.138276	34.357568
965.432755	106306.576040	34.362586
966.831856	106509.476083	34.367604
967.727087	106700.974491	34.372621
968.648762	106895.357389	34.377639
969.706544	107105.765003	34.382656
971.179938	107312.331679	34.387674
972.007051	107516.549759	34.392692
972.895163	107712.476668	34.397709
973.807638	107888.162749	34.402727
974.833836	108109.310655	34.407744
975.093262	108311.627581	34.412762
976.718581	108503.930470	34.417780
977.777565	108696.264935	34.422797
978.830317	108921.290782	34.427815
979.906022	109130.939025	34.432832
981.340665	109323.469327	34.437850
982.638426	109494.910211	34.442868
983.334632	109704.486313	34.447885
985.001428	109911.320014	34.452903
985.901060	110104.501586	34.457920
986.780318	110274.078708	34.462938
987.905676	110463.552502	34.467956
988.861410	110668.229582	34.472973
989.797948	110852.645543	34.477991
990.800578	111039.813098	34.483008
991.626921	111211.887469	34.488026
992.336901	111428.390592	34.493044
993.165238	111639.125311	34.498061
994.571259	111828.106388	34.503079
995.397820	112017.513788	34.508096
996.213095	112213.612441	34.513114
997.085095	112421.369348	34.518132
997.585065	112649.380445	34.523149
998.968927	112838.828240	34.528167
999.904290	113039.232500	34.533184
1000.791418	113249.425330	34.538202
1001.905683	113459.404935	34.543220
1002.311093	113678.788436	34.548237
1003.722637	113880.374331	34.553255
1004.391368	114117.325788	34.558272
1005.457953	114321.062038	34.563290
1006.933913	114537.121382	34.568308
1007.634253	114756.338117	34.573325
1008.731681	114968.992318	34.578343
1009.696378	115182.430160	34.583360
1010.506992	115393.576795	34.588378
1012.302285	115624.489804	34.593396
1013.100539	115822.491987	34.598413
1014.458939	116029.271086	34.603431
1015.424160	116232.518740	34.608448
1016.368888	116439.419856	34.613466
1017.677754	116623.686544	34.618484
1018.488707	116834.552676	34.623501
1019.644883	117030.451981	34.628519
1020.565669	117224.465817	34.633536
1021.168171	117395.044895	34.638554
1022.446606	117605.370885	34.643572
1023.361764	117820.281384	34.648589
1024.329160	118007.185416	34.653607
1025.269021	118186.050084	34.658624
1026.390100	118383.117531	34.663642
1027.616173	118601.922899	34.668660
1028.330948	118813.782627	34.673677
1029.330107	118994.289687	34.678695
1030.589326	119221.418476	34.683712
1031.402710	119420.305054	34.688730
1032.540167	119608.661296	34.693748
1033.568527	119830.967717	34.698765
1034.544748	120048.368378	34.703783
1036.063739	120241.924004	34.708800
1036.758919	120454.128582	34.713818
1037.698370	120652.736835	34.718836
1038.481611	120875.079149	34.723853
1039.537586	121084.707343	34.728871
1040.610932	121293.675306	34.733888
1041.571965	121508.276573	34.738906
1042.685205	121731.445302	34.743924
1043.290595	121961.846143	34.748941
1044.463510	122200.822283	34.753959
1045.405705	122420.603299	34.758976
1046.109026	122659.584704	34.763994
1047.146802	122872.751502	34.769012
1048.348533	123112.845464	34.774029
1049.532380	123344.783712	34.779047
1050.613982	123597.231133	34.784064
1051.614428	123844.004389	34.789082
1052.863821	124059.717299	34.794100
1054.032030	124280.780185	34.799117
1055.051987	124514.300720	34.804135
1056.595317	124736.078096	34.809152
1057.470072	124976.646756	34.814170
1058.764372	125208.885573	34.819188
1059.928713	125442.858473	34.824205
1060.943234	125662.639078	34.829223
1062.031710	125873.626790	34.834240
1063.238326	126104.911258	34.839258
1064.460535	126344.571840	34.844276
1065.297952	126584.475287	34.849293
1066.397957	126794.960661	34.854311
1067.400458	127014.829214	34.859328
1068.368432	127253.030884	34.864346
1069.586801	127493.208192	34.869364
1070.494731	127717.153013	34.874381
1071.536801	127928.340234	34.879399
1072.487302	128163.079349	34.884416
1073.465634	128412.821624	34.889434
1074.927063	128656.618114	34.894452
1075.923024	128881.520208	34.899469
1077.171569	129112.795421	34.904487
1078.035101	129351.334960	34.909504
1079.370222	129578.454892	34.914522
1080.525027	129790.181388	34.919540
1081.040158	130029.100568	34.924557
1082.504670	130264.898991	34.929575
1083.782323	130489.842409	34.934592
1084.591223	130725.917354	34.939610
1085.901132	130969.364283	34.944628
1087.247742	131183.198061	34.949645
1088.390465	131400.261111	34.954663
1089.593039	131635.454092	34.959680
1090.358197	131859.845599	34.964698
1091.386804	132073.940790	34.969716
1092.226561	132283.137841	34.974733
1093.209999	132475.973709	34.979751
1094.719733	132707.346709	34.984768
1095.340262	132960.974789	34.989786
1096.391957	133165.161132	34.994804
1097.702160	133380.346887	34.999821
1098.576784	133609.739817	35.004839
1099.592212	133819.602571	35.009856
1100.631367	134071.142259	35.014874
1101.455296	134306.734600	35.019892
1102.409203	134545.615775	35.024909
1103.371866	134777.575908	35.029927
1104.561177	135006.280447	35.034944
1105.197439	135259.721442	35.039962
1106.679795	135507.675147	35.044980
1107.639833	135772.285715	35.049997
1108.790684	136020.348801	35.055015
1109.948098	136263.696824	35.060032
1110.986574	136512.618927	35.065050
1112.626711	136777.404349	35.070068
1113.511795	137027.344550	35.075085
1114.594195	137254.181046	35.080103
1115.960195	137524.215570	35.085120
1116.910624	137797.553742	35.090138
1118.402562	138020.271082	35.095156
1119.227035	138263.308662	35.100173
1120.700213	138528.199219	35.105191
1121.991580	138765.293523	35.110208
1122.777270	139014.200314	35.115226
1124.186425	139265.643137	35.120244
1125.035728	139535.272319	35.125261
1126.159047	139773.948344	35.130279
1127.960175	140022.352750	35.135296
1128.751657	140307.047176	35.140314
1129.786909	140539.340486	35.145332
1131.190092	140782.858841	35.150349
1131.957333	141046.250412	35.155367
1133.723174	141310.696387	35.160384
1134.719017	141553.995947	35.165402
1135.731951	141825.226786	35.170420
1137.018629	142074.530076	35.175437
1138.141857	142316.622228	35.180455
1139.378881	142548.236722	35.185472
1140.039384	142828.181168	35.190490
1141.675703	143095.172994	35.195508
1142.929287	143340.966049	35.200525
1143.775044	143580.221963	35.205543
1145.011025	143834.428223	35.210560
1145.813341	144116.185681	35.215578
1146.943908	144357.695073	35.220596
1148.029549	144622.773503	35.225613
1149.424570	144877.975604	35.230631
1150.746726	145151.438790	35.235648
1151.480277	145411.674015	35.240666
1152.453626	145662.868331	35.245684
1153.955170	145905.607971	35.250701
1155.148623	146183.564095	35.255719
1156.776020	146458.648297	35.260736
1157.193337	146718.653751	35.265754
1158.777801	146961.285537	35.270772
1159.778335	147216.290785	35.275789
1160.466703	147490.840556	35.280807
1161.795517	147766.732406	35.285824
1162.921812	148031.601553	35.290842
1164.263985	148283.679348	35.295860
1165.256951	148553.583595	35.300877
1166.368466	148817.788866	35.305895
1167.452384	149079.540348	35.310912
1168.536625	149327.901529	35.315930
1169.989553	149568.277281	35.320948
1170.824558	149834.437939	35.325965
1172.154159	150082.979390	35.330983
1173.611934	150358.983948	35.336000
1174.784337	150608.290505	35.341018
1175.393724	150879.416806	35.346036
1176.381861	151140.399934	35.351053
1177.646810	151395.847624	35.356071
1178.748991	151673.709034	35.361088
1179.556291	151950.086583	35.366106
1180.602897	152222.406195	35.371124
1181.774522	152496.812554	35.376141
1182.819961	152799.728117	35.381159
1183.924981	153089.318887	35.386176
1185.064946	153391.602165	35.391194
1186.100607	153685.546698	35.396212
1187.162627	153950.558006	35.401229
1188.984096	154265.191050	35.406247
1190.303975	154564.993417	35.411264
1191.117978	154857.563077	35.416282
1192.451181	155153.816415	35.421300
1193.856658	155454.753220	35.426317
1195.038079	155748.271101	35.431335
1196.505623	156028.298710	35.436352
1197.706760	156343.647458	35.441370
1199.038778	156639.709518	35.446388
1200.446458	156914.946046	35.451405
1201.570952	157215.613192	35.456423
1203.312960	157482.832618	35.461440
1204.389396	157791.922108	35.466458
1205.651373	158074.573441	35.471476
1206.754000	158348.982500	35.476493
1207.981821	158642.095988	35.481511
1209.551775	158931.413053	35.486528
1210.571397	159234.066498	35.491546
1211.980847	159512.416170	35.496564
1213.538535	159787.889096	35.501581
1214.815621	160077.706845	35.506599
1216.374146	160343.453657	35.511616
1217.467014	160640.726979	35.516634
1218.706182	160925.863400	35.521652
1219.848019	161185.963258	35.526669
1221.098762	161487.618767	35.531687
1222.029334	161775.514228	35.536704
1223.102553	162058.656241	35.541722
1224.437574	162342.442063	35.546740
1225.402380	162619.110494	35.551757
1226.383986	162905.965215	35.556775
1228.023215	163202.342454	35.561792
1229.034020	163502.124067	35.566810
1230.400213	163786.675899	35.571828
1231.684634	164086.568814	35.576845
1232.602115	164360.871596	35.581863
1233.862941	164648.313940	35.586880
1235.064185	164941.946682	35.591898
1236.067823	165243.924166	35.596916
1237.602419	165555.839086	35.601933
1238.901546	165842.382469	35.606951
1240.170451	166120.241907	35.611968
1241.171238	166431.172945	35.616986
1242.135524	166747.821685	35.622004
1243.442333	167040.449209	35.627021
1244.555805	167341.839817	35.632039
1245.834925	167648.686343	35.637056
1247.141546	167957.624018	35.642074
1248.056927	168242.901856	35.647092
1249.165995	168553.995279	35.652109
1250.233295	168853.424664	35.657127
1251.534767	169139.570873	35.662144
1252.630765	169440.255667	35.667162
1253.772309	169740.325948	35.672180
1255.206717	170043.420554	35.677197
1255.922664	170358.385490	35.682215
1257.429268	170674.046918	35.687232
1258.662098	170987.890509	35.692250
1259.655317	171293.413861	35.697268
1261.030218	171624.558802	35.702285
1262.427764	171941.642930	35.707303
1263.823943	172257.930085	35.712320
1264.843272	172566.173206	35.717338
1266.075741	172905.231027	35.722356
1267.530501	173227.694948	35.727373
1268.813891	173555.620534	35.732391
1270.417395	173868.204626	35.737408
1271.860368	174200.410226	35.742426
1272.299361	174528.177514	35.747444
1274.138060	174852.518228	35.752461
1275.403296	175183.643455	35.757479
1276.731553	175503.187278	35.762496
1278.150683	175840.636752	35.767514
1279.462385	176170.454149	35.772532
1280.880954	176491.779057	35.777549
1282.056217	176827.511831	35.782567
1283.441380	177152.450768	35.787584
1284.550009	177498.465843	35.792602
1285.696619	177824.438548	35.797620
1287.168503	178144.801206	35.802637
1288.332700	178489.760848	35.807655
1289.625553	178836.008855	35.812672
1291.025335	179184.678332	35.817690
1292.069713	179514.384956	35.822708
1293.683263	179860.815670	35.827725
1294.388348	180200.697741	35.832743
1296.172663	180555.379821	35.837760
1297.547256	180895.435320	35.842778
1298.664048	181238.581636	35.847796
1300.105393	181576.930044	35.852813
1301.163157	181938.252570	35.857831
1302.498358	182268.703461	35.862848
1303.801975	182620.534839	35.867866
1305.332533	182969.120096	35.872884
1306.768618	183329.438073	35.877901
1308.103379	183681.918831	35.882919
1309.314973	184013.162807	35.887936
1310.949702	184375.270216	35.892954
1312.106901	184736.380076	35.897972
1313.576890	185068.565365	35.902989
1314.838802	185416.627398	35.908007
1316.334099	185749.536238	35.913024
1317.802535	186102.531478	35.918042
1318.647213	186479.646790	35.923060
1320.482621	186788.554579	35.928077
1321.296343	187145.231385	35.933095
1322.603323	187508.873760	35.938112
1324.169501	187847.178338	35.943130
1325.595024	188200.765455	35.948148
1327.278885	188515.711882	35.953165
1328.555376	188872.640828	35.958183
1330.038954	189226.186803	35.963200
1331.343346	189558.871030	35.968218
1332.585948	189894.855059	35.973236
1334.081941	190230.621549	35.978253
1335.002284	190595.414095	35.983271
1336.207966	190916.241205	35.988288
1337.598179	191245.227217	35.993306
1338.541124	191581.676814	35.998324
1340.003247	191896.107363	36.003341
1340.931488	192237.678880	36.008359
1342.080237	192589.358657	36.013376
1344.100229	192910.747860	36.018394
1344.965479	193287.333956	36.023412
1346.496704	193640.683287	36.028429
1347.881733	193974.877458	36.033447
1349.161946	194308.405281	36.038464
1350.778178	194639.924517	36.043482
1351.852996	195008.984291	36.048500
1353.142998	195343.963386	36.053517
1354.678350	195695.216696	36.058535
1356.237047	196043.091306	36.063552
1357.369352	196396.763682	36.068570
1358.631154	196778.485486	36.073588
1360.098067	197116.910718	36.078605
1361.639779	197460.657410	36.083623
1362.743484	197825.768237	36.088640
1364.087006	198188.810320	36.093658
1364.951793	198559.652288	36.098676
1366.314387	198925.399511	36.103693
1367.559942	199287.778396	36.108711
1368.654142	199667.691561	36.113728
1370.893197	200048.687556	36.118746
1371.517546	200421.001706	36.123764
1372.761105	200815.078020	36.128781
1374.430507	201208.642020	36.133799
1375.456788	201594.201711	36.138816
1376.948625	201961.175882	36.143834
1378.367127	202363.218198	36.148852
1379.891494	202747.064407	36.153869
1381.353349	203138.655110	36.158887
1382.631687	203526.532880	36.163904
1384.015406	203933.414670	36.168922
1385.351012	204346.464558	36.173940
1386.601993	204736.410339	36.178957
1388.241086	205131.499823	36.183975
1389.452013	205523.373689	36.188992
1391.015927	205938.032947	36.194010
1392.119988	206342.282843	36.199028
1393.844161	206720.073797	36.204045
1395.051713	207157.310401	36.209063
1396.608339	207569.377146	36.214080
1398.060163	207957.173819	36.219098
1399.146394	208355.596885	36.224116
1400.722914	208761.216655	36.229133
1402.314065	209183.901376	36.234151
1403.662204	209589.182268	36.239168
1405.431921	209985.443974	36.244186
1406.720563	210386.358181	36.249204
1408.318971	210797.355979	36.254221
1409.807909	211213.719675	36.259239
1411.460378	211612.040455	36.264256
1413.159532	211992.362716	36.269274
1414.697302	212381.944714	36.274292
1415.784692	212787.551452	36.279309
1417.401767	213186.863447	36.284327
1418.632497	213571.816138	36.289344
1420.612491	213977.040064	36.294362
1421.840223	214372.688675	36.299380
1423.563890	214753.273381	36.304397
1424.479132	215137.472495	36.309415
1425.721984	215552.374561	36.314432
1427.285537	215933.168607	36.319450
1428.711831	216320.793295	36.324468
1430.078761	216782.436257	36.329485
1431.178330	217157.140600	36.334503
1432.464892	217523.434547	36.339520
1433.654636	217914.381310	36.344538
1435.042971	218311.493915	36.349556
1436.635292	218704.637924	36.354573
1437.889995	219096.061449	36.359591
1439.383058	219472.741962	36.364608
1440.782319	219869.706892	36.369626
1442.215309	220291.811830	36.374644
1443.538125	220696.843881	36.379661
1444.658241	221079.814655	36.384679
1445.691179	221483.627834	36.389696
1447.368888	221898.917868	36.394714
1448.445885	222335.059254	36.399732
1449.726490	222744.195616	36.404749
1451.422443	223173.914146	36.409767
1452.791027	223598.634096	36.414784
1454.072420	224019.865083	36.419802
1455.690708	224473.273398	36.424820
1457.166896	224898.818873	36.429837
1458.710901	225343.759756	36.434855
1459.976912	225787.986306	36.439872
1461.983110	226216.243253	36.444890
1463.687146	226646.253429	36.449908
1465.097538	227066.661831	36.454925
1466.997901	227511.882528	36.459943
1468.128153	227958.705162	36.464960
1469.574939	228389.068931	36.469978
1471.282616	228829.144734	36.474996
1472.622535	229254.982589	36.480013
1474.069662	229710.547708	36.485031
1475.755107	230158.074077	36.490048
1476.911176	230574.828033	36.495066
1478.687639	231033.086715	36.500084
1480.262629	231478.375206	36.505101
1481.908933	231928.860511	36.510119
1483.122218	232372.992407	36.515136
1485.240168	232785.022384	36.520154
1486.634790	233218.433364	36.525172
1487.737405	233669.547429	36.530189
1489.600982	234118.708462	36.535207
1490.597349	234563.441792	36.540224
1492.307346	234985.629543	36.545242
1493.905683	235434.787498	36.550260
1495.321269	235877.296397	36.555277
1496.900550	236328.492170	36.560295
1498.289082	236779.847700	36.565312
1500.013486	237222.766588	36.570330
1501.168684	237663.011825	36.575348
1503.049113	238124.272632	36.580365
1504.399145	238579.195588	36.585383
1505.824270	239041.118199	36.590400
1507.552075	239498.089518	36.595418
1509.012180	239954.217092	36.600436
1510.178838	240399.217379	36.605453
1511.734948	240838.286595	36.610471
1513.153389	241313.196332	36.615488
1514.686968	241771.703880	36.620506
1516.142451	242220.851971	36.625524
1517.495712	242673.955236	36.630541
1519.050494	243115.976248	36.635559
1520.626957	243602.804183	36.640576
1522.333539	244075.106980	36.645594
1524.003694	244532.403955	36.650612
1525.592323	244977.090268	36.655629
1527.164934	245435.141740	36.660647
1528.542792	245898.840149	36.665664
1530.143407	246331.181286	36.670682
1531.829857	246770.494686	36.675700
1533.338002	247210.066845	36.680717
1534.552490	247624.564905	36.685735
1535.877511	248072.551506	36.690752
1538.075330	248526.415221	36.695770
1539.249697	248965.587853	36.700788
1540.829309	249405.888159	36.705805
1542.173285	249864.136955	36.710823
1543.488111	250306.184132	36.715840
1545.120339	250749.068592	36.720858
1546.589951	251199.093246	36.725876
1547.952987	251650.914224	36.730893
1549.900284	252108.583611	36.735911
1551.069792	252574.510812	36.740928
1552.721465	253063.551947	36.745946
1553.806778	253529.824267	36.750964
1555.761785	253989.856780	36.755981
1557.390141	254429.595687	36.760999
1558.885112	254931.848725	36.766016
1560.268738	255382.755335	36.771034
1562.092827	255858.891175	36.776052
1563.299505	256343.918735	36.781069
1565.114055	256825.645506	36.786087
1566.716602	257317.695859	36.791104
1567.956076	257799.670491	36.796122
1569.474146	258282.361483	36.801140
1570.941015	258795.164015	36.806157
1572.687044	259279.773840	36.811175
1574.217513	259771.354481	36.816192
1575.789635	260261.582000	36.821210
1577.705695	260777.664235	36.826228
1578.928837	261282.988258	36.831245
1580.892466	261762.659812	36.836263
1581.943125	262266.107090	36.841280
1584.072723	262768.868253	36.846298
1585.530607	263278.776908	36.851316
1586.881992	263801.023646	36.856333
1588.955468	264290.482479	36.861351
1590.263548	264789.796918	36.866368
1592.061716	265315.424316	36.871386
1593.681636	265828.531681	36.876404
1595.321440	266329.924615	36.881421
1597.343507	266815.123149	36.886439
1598.759936	267319.905596	36.891456
1600.225089	267831.030463	36.896474
1602.211959	268341.255966	36.901492
1604.045436	268840.227366	36.906509
1605.935483	269323.312047	36.911527
1607.450368	269843.343523	36.916544
1608.895909	270357.085948	36.921562
1610.650563	270853.909193	36.926580
1612.277381	271346.307458	36.931597
1613.815603	271820.759858	36.936615
1615.522509	272346.142235	36.941632
1617.028526	272855.248367	36.946650
1618.689172	273340.043119	36.951668
1619.997724	273871.712782	36.956685
1621.722426	274366.580472	36.961703
1623.280364	274849.713439	36.966720
1625.101235	275359.830803	36.971738
1627.355352	275870.079048	36.976756
1628.765108	276380.465715	36.981773
1630.403910	276856.748767	36.986791
1631.985065	277343.125317	36.991808
1634.025216	277844.082494	36.996826
1635.839190	278343.475653	37.001844
1637.040946	278843.883304	37.006861
1639.148432	279299.584734	37.011879
1640.295954	279775.054250	37.016896
1641.685782	280233.844317	37.021914
1643.484787	280729.246714	37.026932
1644.721453	281186.332713	37.031949
1646.078682	281683.787158	37.036967
1647.863446	282177.181747	37.041984
1649.735396	282649.121482	37.047002
1651.026123	283117.498106	37.052020
1652.485975	283619.909556	37.057037
1654.052271	284115.215006	37.062055
1655.887068	284595.055988	37.067072
1657.543959	285104.594150	37.072090
1659.379557	285613.212298	37.077108
1660.880005	286109.208898	37.082125
1662.713101	286606.419227	37.087143
1664.453882	287123.405525	37.092160
1665.686258	287623.124999	37.097178
1667.699072	288125.736878	37.102196
1668.722377	288642.887402	37.107213
1670.108807	289173.260983	37.112231
1671.702670	289704.919309	37.117248
1673.513260	290229.021314	37.122266
1675.076279	290757.759787	37.127284
1676.288626	291311.980159	37.132301
1678.287643	291847.399152	37.137319
1679.603660	292414.018831	37.142336
1681.115674	292949.005796	37.147354
1683.244422	293499.763959	37.152372
1684.796935	294060.927280	37.157389
1686.555426	294614.789744	37.162407
1688.309626	295184.449173	37.167424
1689.980918	295728.618290	37.172442
1691.802337	296291.022520	37.177460
1693.507207	296860.555175	37.182477
1694.894420	297406.617632	37.187495
1696.725859	297971.679053	37.192512
1698.573262	298559.924423	37.197530
1700.331522	299118.134382	37.202548
1701.875522	299679.043731	37.207565
1703.632912	300254.392241	37.212583
1705.433874	300844.461636	37.217600
1707.209724	301411.114482	37.222618
1709.339282	301973.946917	37.227636
1710.633506	302570.744412	37.232653
1712.454365	303135.399182	37.237671
1714.009381	303703.116936	37.242688
1716.006164	304290.060776	37.247706
1717.866238	304868.769385	37.252724
1719.561509	305451.590640	37.257741
1721.352151	306028.017828	37.262759
1723.141266	306620.213268	37.267776
1724.676033	307187.964193	37.272794
1726.793268	307760.364644	37.277812
1728.190834	308346.314943	37.282829
1730.069688	308912.931441	37.287847
1731.460801	309492.627595	37.292864
1733.407374	310092.291103	37.297882
1735.175994	310686.316436	37.302900
1736.736624	311269.350120	37.307917
1738.601626	311829.295716	37.312935
1740.245017	312409.717315	37.317952
1741.948792	313014.021652	37.322970
1743.784194	313612.052535	37.327988
1745.175188	314205.504954	37.333005
1747.057084	314783.406559	37.338023
1748.538590	315388.440337	37.343040
1749.984846	315967.369883	37.348058
1752.347620	316519.048366	37.353076
1754.163419	317105.120082	37.358093
1756.110381	317693.654089	37.363111
1757.952038	318256.172472	37.368128
1759.523959	318804.002909	37.373146
1761.890318	319359.468372	37.378164
1763.531496	319936.201357	37.383181
1765.320555	320492.641899	37.388199
1767.290026	321058.925887	37.393216
1769.096747	321608.930271	37.398234
1770.986010	322172.018891	37.403252
1772.628391	322753.070161	37.408269
1774.164779	323328.623913	37.413287
1775.924953	323880.140929	37.418304
1777.649886	324439.708132	37.423322
1779.361908	325011.765000	37.428340
1781.130172	325594.014587	37.433357
1782.966778	326157.966475	37.438375
1784.892759	326750.818087	37.443392
1786.335226	327350.903852	37.448410
1788.171457	327938.706419	37.453428
1789.741039	328518.854361	37.458445
1791.684612	329095.329837	37.463463
1793.492808	329695.865573	37.468480
1794.757963	330320.451882	37.473498
1796.667832	330914.966880	37.478516
1798.107293	331511.076793	37.483533
1799.959706	332125.645743	37.488551
1801.659682	332765.824134	37.493568
1803.282923	333402.783865	37.498586
1805.451426	334010.552888	37.503604
1806.964521	334624.440184	37.508621
1808.738190	335258.993223	37.513639
1810.568401	335897.033001	37.518656
1812.236951	336549.155895	37.523674
1814.273803	337166.914197	37.528692
1816.273675	337808.406899	37.533709
1818.288251	338432.018415	37.538727
1820.628113	339056.102055	37.543744
1822.364231	339712.262370	37.548762
1824.382284	340339.252326	37.553780
1826.223312	340970.579180	37.558797
1827.928709	341585.066000	37.563815
1829.719605	342221.411699	37.568832
1831.537086	342873.330149	37.573850
1833.429828	343514.770119	37.578868
1835.115848	344143.925556	37.583885
1837.078053	344761.377137	37.588903
1839.043042	345411.156700	37.593920
1840.364397	346075.374209	37.598938
1842.252369	346710.148791	37.603956
1844.374269	347343.023619	37.608973
1845.914189	347992.356322	37.613991
1847.808372	348659.869834	37.619008
1849.803333	349321.849881	37.624026
1851.452804	349956.772554	37.629044
1853.457011	350619.316312	37.634061
1855.726615	351253.687397	37.639079
1857.500417	351901.886384	37.644096
1859.416996	352541.398731	37.649114
1861.752845	353202.961902	37.654132
1863.329451	353853.119348	37.659149
1865.306964	354501.297881	37.664167
1867.430127	355139.495347	37.669184
1869.245698	355790.346051	37.674202
1871.134774	356428.487117	37.679220
1872.548609	357076.694932	37.684237
1874.571084	357699.443162	37.689255
1876.506082	358313.544037	37.694272
1877.839377	358935.651935	37.699290
1880.113449	359570.561366	37.704308
1882.132620	360190.862813	37.709325
1884.125610	360802.684755	37.714343
1886.334073	361404.947378	37.719360
1887.529857	362041.696665	37.724378
1889.570324	362685.806687	37.729396
1891.372870	363299.221027	37.734413
1892.779662	363905.359081	37.739431
1895.006150	364547.175935	37.744448
1896.499246	365200.748264	37.749466
1898.877119	365849.039141	37.754484
1900.402243	366487.185393	37.759501
1901.914994	367120.452410	37.764519
1904.116469	367770.769902	37.769536
1905.759985	368441.716515	37.774554
1907.854184	369087.894382	37.779572
1909.480873	369763.335931	37.784589
1911.050407	370443.873524	37.789607
1913.033299	371089.832554	37.794624
1914.859593	371781.895813	37.799642
1916.814258	372482.726721	37.804660
1918.527861	373158.675831	37.809677
1920.146507	373840.766286	37.814695
1922.120925	374532.398166	37.819712
1923.908216	375239.468593	37.824730
1925.594520	375964.879090	37.829748
1927.408971	376665.626895	37.834765
1929.556694	377385.935935	37.839783
1931.885476	378085.404124	37.844800
1933.571617	378812.404720	37.849818
1935.462533	379534.056068	37.854836
1937.501186	380258.102531	37.859853
1939.307742	380984.631872	37.864871
1941.277903	381720.678992	37.869888
1943.125753	382446.612457	37.874906
1945.275959	383160.029885	37.879924
1947.565044	383899.729808	37.884941
1949.123878	384656.243657	37.889959
1951.512714	385388.844914	37.894976
1953.134726	386110.070409	37.899994
1955.168336	386853.498946	37.905012
1957.247619	387609.782876	37.910029
1959.368002	388347.635678	37.915047
1961.608864	389080.482502	37.920064
1963.206912	389812.024175	37.925082
1965.314186	390565.419688	37.930100
1967.214047	391324.560822	37.935117
1969.351545	392075.937850	37.940135
1971.583766	392791.791216	37.945152
1973.452421	393538.487562	37.950170
1975.678261	394288.072752	37.955188
1977.623724	395034.339936	37.960205
1979.455737	395788.592065	37.965223
1981.551633	396510.540681	37.970240
1983.833839	397248.941750	37.975258
1985.667561	398005.267324	37.980276
1987.902306	398769.440591	37.985293
1990.051366	399488.039152	37.990311
1992.840038	400204.309830	37.995328
1994.797778	400935.094998	38.000346
1996.591063	401684.465070	38.005364
1998.753606	402408.793208	38.010381
2000.378367	403123.384847	38.015399
2002.645269	403838.511686	38.020416
2004.435292	404579.495380	38.025434
2006.457260	405307.143755	38.030452
2008.263685	406023.888033	38.035469
2009.897216	406722.652614	38.040487
2012.070230	407423.768539	38.045504
2014.093580	408132.011160	38.050522
2015.980379	408838.434043	38.055540
2018.028235	409532.473944	38.060557
2019.871959	410248.672621	38.065575
2021.831245	410981.655360	38.070592
2023.618613	411683.461255	38.075610
2025.535023	412407.444560	38.080628
2027.368287	413154.271696	38.085645
2029.311916	413889.382086	38.090663
2031.172045	414614.835023	38.095680
2032.908657	415361.084458	38.100698
2034.671578	416119.669183	38.105716
2036.979910	416884.879481	38.110733
2038.711005	417632.762430	38.115751
2040.989437	418405.632758	38.120768
2042.929224	419187.121507	38.125786
2044.986518	419957.145400	38.130804
2047.042754	420714.990484	38.135821
2049.110801	421476.938954	38.140839
2051.183231	422274.417685	38.145856
2053.064267	423078.891826	38.150874
2055.107558	423865.436441	38.155892
2056.956178	424642.467829	38.160909
2059.085453	425444.925972	38.165927
2061.138277	426256.156513	38.170944
2063.450833	427065.874403	38.175962
2065.420425	427852.431295	38.180980
2066.897176	428645.272059	38.185997
2069.300843	429481.730553	38.191015
2071.502632	430299.814747	38.196032
2073.735201	431109.816170	38.201050
2075.368687	431945.860407	38.206068
2077.576429	432764.213839	38.211085
2079.670581	433582.760261	38.216103
2082.308116	434410.907961	38.221120
2084.568966	435251.642194	38.226138
2086.702110	436073.841208	38.231156
2089.232041	436913.762486	38.236173
2091.258551	437724.936954	38.241191
2093.616461	438543.721266	38.246208
2095.584204	439375.446331	38.251226
2097.595986	440191.748828	38.256244
2099.968363	441016.565666	38.261261
2101.944939	441831.195500	38.266279
2104.085336	442636.660279	38.271296
2106.143874	443491.951768	38.276314
2108.338275	444335.651423	38.281332
2110.348036	445141.705036	38.286349
2112.571164	445948.857747	38.291367
2114.677559	446784.737263	38.296384
2117.065278	447622.815091	38.301402
2119.110955	448453.379221	38.306420
2121.289741	449263.705065	38.311437
2123.629180	450107.563034	38.316455
2125.493878	450929.968016	38.321472
2127.651439	451761.246105	38.326490
2129.441950	452587.089652	38.331508
2132.078386	453410.839584	38.336525
2133.743501	454258.538854	38.341543
2135.971384	455086.589597	38.346560
2138.606875	455912.062335	38.351578
2140.377933	456751.652799	38.356596
2142.401661	457588.234688	38.361613
2144.321842	458423.029970	38.366631
2146.317357	459250.952836	38.371648
2148.429171	460066.536544	38.376666
2150.559198	460880.416158	38.381684
2152.774577	461683.480277	38.386701
2154.495333	462504.187469	38.391719
2156.512318	463325.115694	38.396736
2158.423510	464160.081097	38.401754
2160.456811	464980.938713	38.406772
2162.834174	465824.856395	38.411789
2164.619145	466681.168815	38.416807
2166.706311	467520.462336	38.421824
2169.190975	468352.427101	38.426842
2171.060739	469196.536605	38.431860
2173.496997	470039.960208	38.436877
2175.643279	470897.241322	38.441895
2177.786138	471748.623238	38.446912
2180.112143	472598.674021	38.451930
2182.250781	473470.545833	38.456948
2184.265683	474346.389676	38.461965
2186.305780	475227.241251	38.466983
2188.808124	476098.275654	38.472000
2191.393455	476953.241838	38.477018
2193.506963	477832.645973	38.482036
2196.185827	478708.783644	38.487053
2198.328211	479570.572861	38.492071
2200.837164	480436.403249	38.497088
2202.633067	481328.422315	38.502106
2204.819638	482216.646878	38.507124
2207.157696	483082.582741	38.512141
2209.167247	483971.710639	38.517159
2211.859536	484844.826503	38.522176
2213.939015	485745.167003	38.527194
2215.923036	486651.991603	38.532212
2218.189510	487542.466333	38.537229
2219.903026	488435.663600	38.542247
2222.299138	489351.572605	38.547264
2224.660011	490262.543365	38.552282
2226.549721	491173.847622	38.557300
2228.707730	492082.031793	38.562317
2230.954310	493001.409745	38.567335
2233.046736	493935.249644	38.572352
2235.257551	494855.544827	38.577370
2237.360154	495770.207187	38.582388
2239.493219	496703.890723	38.587405
2241.927619	497650.694134	38.592423
2243.899952	498594.392870	38.597440
2246.431241	499535.676604	38.602458
2248.226726	500497.714313	38.607476
2250.724021	501427.546678	38.612493
2252.967702	502381.936346	38.617511
2255.047619	503332.111790	38.622528
2257.397543	504296.462941	38.627546
2259.594321	505256.748309	38.632564
2261.791371	506200.284166	38.637581
2264.021776	507168.572445	38.642599
2266.308468	508126.708605	38.647616
2269.007352	509082.653099	38.652634
2271.082034	510067.384823	38.657652
2273.574974	511035.248574	38.662669
2276.101093	512013.283156	38.667687
2278.047442	512971.239009	38.672704
2280.586784	513927.930677	38.677722
2282.518659	514902.357815	38.682740
2285.025041	515887.315943	38.687757
2287.424615	516862.452571	38.692775
2289.541502	517846.949287	38.697792
2291.596064	518805.844564	38.702810
2293.724053	519768.952089	38.707828
2296.015150	520732.779283	38.712845
2298.349859	521697.597400	38.717863
2300.595177	522648.162275	38.722880
2303.018298	523572.996295	38.727898
2304.949988	524524.050834	38.732916
2307.483670	525485.021332	38.737933
2309.395182	526446.235133	38.742951
2311.371186	527394.332484	38.747968
2314.261158	528355.213190	38.752986
2316.376135	529330.512728	38.758004
2318.933349	530295.805984	38.763021
2320.939023	531270.493378	38.768039
2323.407432	532252.794413	38.773056
2325.720748	533224.181020	38.778074
2327.653187	534211.072111	38.783092
2330.020916	535175.323317	38.788109
2332.418962	536179.724742	38.793127
2334.350806	537194.049414	38.798144
2336.796374	538172.585428	38.803162
2339.069674	539190.539181	38.808180
2341.743460	540188.125474	38.813197
2343.907244	541225.830618	38.818215
2346.347435	542237.552985	38.823232
2348.876705	543232.988528	38.828250
2351.093424	544267.746688	38.833268
2353.607156	545295.287298	38.838285
2355.932564	546312.170608	38.843303
2358.685776	547340.779827	38.848320
2360.822267	548357.747040	38.853338
2363.181162	549411.113591	38.858356
2365.522834	550454.748207	38.863373
2368.334745	551484.348731	38.868391
2370.281129	552502.501300	38.873408
2373.019200	553546.389452	38.878426
2375.408859	554607.297066	38.883444
2377.839231	555641.122184	38.888461
2380.524054	556669.398223	38.893479
2382.888270	557700.111623	38.898496
2385.422974	558759.665019	38.903514
2387.701557	559820.081529	38.908532
2390.123603	560855.266740	38.913549
2392.576476	561909.408637	38.918567
2394.820614	562970.635212	38.923584
2396.927815	564023.962538	38.928602
2399.441088	565096.075864	38.933620
2401.866808	566156.965682	38.938637
2404.127425	567215.586869	38.943655
2405.898111	568285.853618	38.948672
2408.910178	569358.187599	38.953690
2411.315590	570443.035108	38.958708
2413.493710	571526.322596	38.963725
2415.528494	572603.367496	38.968743
2417.981558	573687.330668	38.973760
2420.916599	574772.326853	38.978778
2423.352982	575839.997272	38.983796
2426.295531	576903.378998	38.988813
2428.574067	577998.444541	38.993831
2430.619954	579101.882611	38.998848
2433.231521	580182.954208	39.003866
2435.920309	581277.514765	39.008884
2438.096368	582366.595665	39.013901
2440.801028	583438.088571	39.018919
2443.081647	584526.159418	39.023936
2445.845637	585611.647096	39.028954
2447.951429	586712.993042	39.033972
2450.362823	587808.473196	39.038989
2452.778009	588892.623520	39.044007
2455.256651	589990.252144	39.049024
2457.526461	591082.201186	39.054042
2460.054098	592163.683366	39.059060
2462.254474	593210.490206	39.064077
2464.752296	594272.090301	39.069095
2466.781695	595355.420495	39.074112
2469.320845	596416.371355	39.079130
2471.830345	597494.817181	39.084148
2474.288334	598578.082232	39.089165
2476.653968	599662.665187	39.094183
2478.781503	600747.988321	39.099200
2480.887605	601836.719781	39.104218
2483.356186	602933.852745	39.109236
2485.843099	604033.232224	39.114253
2488.258383	605140.229258	39.119271
2490.653593	606272.054303	39.124288
2493.326108	607391.507894	39.129306
2495.747687	608526.759910	39.134324
2498.037434	609652.711737	39.139341
2500.894586	610776.256460	39.144359
2502.976349	611910.275281	39.149376
2505.283294	613068.508794	39.154394
2507.855528	614236.984844	39.159412
2510.432176	615390.281508	39.164429
2512.841662	616533.733148	39.169447
2515.131612	617707.344020	39.174464
2517.763527	618889.825330	39.179482
2520.239908	620064.905420	39.184500
2522.680286	621263.213867	39.189517
2525.222380	622460.474684	39.194535
2527.501136	623652.899081	39.199552
2529.994406	624846.756769	39.204570
2532.492256	626064.519550	39.209588
2535.439566	627258.685942	39.214605
2537.922129	628451.547386	39.219623
2540.432441	629697.325733	39.224640
2542.950900	630894.904693	39.229658
2545.928974	632115.397938	39.234676
2548.896147	633347.338570	39.239693
2551.356115	634552.055290	39.244711
2554.010299	635779.469311	39.249728
2556.606012	636986.431134	39.254746
2559.515236	638206.679489	39.259764
2561.952914	639420.424275	39.264781
2564.480808	640646.538492	39.269799
2566.762910	641883.875041	39.274816
2569.973217	643114.224564	39.279834
2572.228374	644317.096595	39.284852
2574.646402	645537.558210	39.289869
2577.732306	646773.723840	39.294887
2580.359502	648028.715154	39.299904
2582.794879	649240.002732	39.304922
2585.450166	650473.993105	39.309940
2587.917584	651721.771517	39.314957
2590.961571	652928.526988	39.319975
2593.427232	654166.032283	39.324992
2595.974755	655412.240536	39.330010
2598.402584	656663.992283	39.335028
2600.852458	657885.989252	39.340045
2603.456691	659103.226544	39.345063
2605.831870	660361.790464	39.350080
2608.309028	661618.183865	39.355098
2611.124710	662854.342455	39.360116
2613.711845	664110.645371	39.365133
2616.515625	665370.383855	39.370151
2618.933704	666599.857996	39.375168
2621.775753	667849.759325	39.380186
2624.593473	669097.262593	39.385204
2626.959773	670350.051188	39.390221
2629.901541	671575.367511	39.395239
2632.283024	672807.432935	39.400256
2634.791546	674008.132427	39.405274
2637.489180	675223.567072	39.410292
2639.853132	676444.369321	39.415309
2642.882789	677651.727909	39.420327
2645.183052	678871.180208	39.425344
2647.816724	680079.880699	39.430362
2650.667072	681314.081921	39.435380
2653.089445	682525.380964	39.440397
2655.830157	683748.144450	39.445415
2658.461939	684991.677756	39.450432
2660.823592	686220.533325	39.455450
2663.313385	687457.546210	39.460468
2665.408388	688713.177152	39.465485
2668.378798	689967.397917	39.470503
2670.651444	691233.077256	39.475520
2673.419111	692513.041042	39.480538
2676.065367	693784.703398	39.485556
2678.267389	695065.587610	39.490573
2681.257773	696340.452488	39.495591
2683.749833	697659.814776	39.500608
2686.908016	698946.283410	39.505626
2689.710088	700237.930145	39.510644
2692.321642	701562.592281	39.515661
2695.225726	702857.903765	39.520679
2697.999387	704148.335868	39.525696
2700.618557	705467.102063	39.530714
2703.128312	706796.142839	39.535732
2705.815387	708128.914622	39.540749
2708.259823	709433.430970	39.545767
2710.894340	710774.868768	39.550784
2713.595370	712128.120807	39.555802
2716.335826	713465.504642	39.560820
2718.601434	714817.956665	39.565837
2721.820068	716171.521515	39.570855
2724.463739	717527.142583	39.575872
2727.111568	718882.396853	39.580890
2730.309678	720249.909681	39.585908
2732.678919	721640.339763	39.590925
2735.523051	723000.337933	39.595943
2738.369007	724365.949334	39.600960
2740.901923	725756.555593	39.605978
2743.721027	727122.854403	39.610996
2746.323265	728517.087815	39.616013
2749.202646	729900.413589	39.621031
2751.887729	731286.551934	39.626048
2754.743836	732669.363706	39.631066
2757.401721	734061.407707	39.636084
2759.492915	735472.567110	39.641101
2762.409091	736880.282750	39.646119
2765.589239	738301.976705	39.651136
2768.508911	739704.309750	39.656154
2771.308418	741119.692575	39.661172
2773.744608	742512.087331	39.666189
2776.625767	743936.775182	39.671207
2779.306964	745348.316349	39.676224
2782.100125	746762.545718	39.681242
2785.083407	748171.657358	39.686260
2788.013735	749587.327837	39.691277
2791.194110	751002.306371	39.696295
2794.436059	752419.974616	39.701312
2797.034476	753821.033045	39.706330
2800.389150	755247.379501	39.711348
2803.423428	756663.319326	39.716365
2805.859670	758039.060390	39.721383
2808.977408	759464.860407	39.726400
2811.595340	760861.530998	39.731418
2814.360035	762235.772930	39.736436
2816.892125	763614.282427	39.741453
2819.853258	764968.804561	39.746471
2822.439453	766328.310342	39.751488
2824.841038	767694.928977	39.756506
2827.513152	769052.107518	39.761524
2830.210585	770423.096548	39.766541
2832.703663	771783.249242	39.771559
2835.183697	773179.965891	39.776576
2837.806775	774576.297159	39.781594
2840.320964	775969.630968	39.786612
2843.000313	777388.460943	39.791629
2845.770041	778825.073585	39.796647
2848.701897	780239.233300	39.801664
2850.907950	781693.393523	39.806682
2853.499515	783136.597806	39.811700
2856.516702	784584.203989	39.816717
2859.533385	786051.192877	39.821735
2862.302948	787528.125600	39.826752
2865.237569	788986.631069	39.831770
2867.985924	790462.814394	39.836788
2870.996051	791967.472044	39.841805
2873.704265	793451.472657	39.846823
2876.443290	794955.589375	39.851840
2879.218011	796472.753119	39.856858
2882.049548	797981.351707	39.861876
2885.213084	799493.047296	39.866893
2888.008385	801022.541069	39.871911
2890.782305	802547.052297	39.876928
2893.314549	804077.874373	39.881946
2896.211294	805627.328684	39.886964
2898.755669	807169.351235	39.891981
2901.693643	808731.550179	39.896999
2904.610128	810310.360910	39.902016
2907.370904	811869.084568	39.907034
2910.486478	813444.495966	39.912052
2912.948867	815038.067331	39.917069
2915.695358	816622.179364	39.922087
2919.155007	818222.208762	39.927104
2921.891789	819833.936552	39.932122
2925.242673	821431.361162	39.937140
2928.235939	823029.388517	39.942157
2930.973405	824630.049063	39.947175
2934.197889	826219.560284	39.952192
2936.726112	827850.787294	39.957210
2939.715069	829481.971973	39.962228
2942.622257	831115.249182	39.967245
2945.673158	832729.626581	39.972263
2948.522941	834359.370663	39.977280
2951.312191	836006.101050	39.982298
2954.375408	837652.366205	39.987316
2957.397024	839284.344106	39.992333
2960.163094	840901.933385	39.997351
2963.224768	842545.725569	40.002368
2965.947940	844217.505651	40.007386
2969.079298	845859.407841	40.012404
2971.777650	847499.691077	40.017421
2974.994632	849138.295509	40.022439
2977.912903	850823.652034	40.027456
2980.692609	852484.581571	40.032474
2983.864148	854129.755772	40.037492
2986.634016	855822.235903	40.042509
2989.116801	857480.617128	40.047527
2992.482086	859162.959975	40.052544
2994.996785	860850.027855	40.057562
2998.049226	862526.067801	40.062580
3000.884764	864220.010140	40.067597
3003.554277	865918.258546	40.072615
3006.413340	867604.080394	40.077632
3009.308408	869272.665378	40.082650
3012.734480	870915.033616	40.087668
3015.015819	872589.192404	40.092685
3017.592396	874256.638947	40.097703
3020.925058	875910.333257	40.102720
3023.313701	877597.972521	40.107738
3026.367529	879297.208539	40.112756
3028.990710	880996.993516	40.117773
3031.791132	882707.761616	40.122791
3035.149383	884421.804323	40.127808
3037.918339	886136.310942	40.132826
3040.875578	887873.364601	40.137844
3043.431626	889605.909435	40.142861
3046.575490	891340.541203	40.147879
3049.663382	893096.757116	40.152896
3052.260334	894880.105436	40.157914
3055.562018	896655.163964	40.162932
3058.468650	898430.506440	40.167949
3061.407487	900200.566910	40.172967
3064.891276	901992.624938	40.177984
3067.825591	903797.110235	40.183002
3071.364399	905592.733216	40.188020
3074.157376	907399.742443	40.193037
3077.026708	909199.900282	40.198055
3080.006327	911011.192499	40.203072
3083.114140	912847.449286	40.208090
3086.352780	914671.058923	40.213108
3089.125548	916513.551728	40.218125
3092.100236	918358.370348	40.223143
3095.744738	920210.906353	40.228160
3098.754522	922063.300792	40.233178
3101.945910	923927.220061	40.238196
3104.960196	925782.660033	40.243213
3108.165953	927658.909831	40.248231
3111.608546	929490.177293	40.253248
3115.003603	931349.094949	40.258266
3117.997265	933207.430474	40.263284
3121.410635	935071.749962	40.268301
3124.648540	936929.315114	40.273319
3127.829520	938795.900351	40.278336
3130.933569	940685.558599	40.283354
3133.985152	942553.410601	40.288372
3137.147875	944421.435902	40.293389
3140.325289	946311.243070	40.298407
3143.737732	948166.030168	40.303424
3146.626145	950046.591289	40.308442
3149.766784	951929.477720	40.313460
3152.983880	953800.400690	40.318477
3155.841322	955684.718464	40.323495
3159.088003	957626.549407	40.328512
3162.287692	959576.322423	40.333530
3165.058266	961511.037588	40.338548
3168.701654	963444.471127	40.343565
3171.800264	965393.368768	40.348583
3174.864476	967344.444590	40.353600
3177.854291	969306.587093	40.358618
3181.248979	971277.948318	40.363636
3184.337215	973239.901697	40.368653
3187.364110	975185.978302	40.373671
3190.669549	977129.105478	40.378688
3193.293395	979109.113863	40.383706
3196.414683	981076.857445	40.388724
3199.264072	983050.104581	40.393741
3202.592748	985044.498729	40.398759
3205.728418	987026.352485	40.403776
3208.333252	989029.302486	40.408794
3211.758602	991028.300220	40.413812
3214.863097	993013.910850	40.418829
3217.587110	994999.667974	40.423847
3220.896358	996956.747995	40.428864
3223.901045	998915.728359	40.433882
3226.898379	1000864.517223	40.438900
3230.251738	1002852.178857	40.443917
3233.432157	1004828.400271	40.448935
3236.399234	1006812.404448	40.453952
3239.328279	1008803.086886	40.458970
3242.362146	1010796.151300	40.463988
3245.642358	1012798.450324	40.469005
3248.353801	1014820.858674	40.474023
3251.813681	1016862.652740	40.479040
3254.579734	1018929.177611	40.484058
3257.396882	1020974.712435	40.489076
3260.133252	1023007.715256	40.494093
3263.336529	1025089.404556	40.499111
3266.770347	1027164.966412	40.504128
3270.156914	1029259.570678	40.509146
3273.142495	1031362.726785	40.514164
3276.621151	1033470.125748	40.519181
3279.160914	1035584.120451	40.524199
3282.729138	1037735.149892	40.529216
3285.828066	1039884.268182	40.534234
3289.220401	1042032.314703	40.539252
3292.415347	1044201.627201	40.544269
3295.016031	1046373.078879	40.549287
3298.682078	1048535.610011	40.554304
3302.205183	1050709.830913	40.559322
3305.398415	1052912.014984	40.564340
3308.865577	1055113.084046	40.569357
3311.644786	1057303.199882	40.574375
3315.005481	1059517.139762	40.579392
3318.429289	1061742.089021	40.584410
3321.542281	1063956.301297	40.589428
3324.655666	1066184.400611	40.594445
3327.555467	1068437.051965	40.599463
3330.982968	1070684.759998	40.604480
3334.195090	1072946.725620	40.609498
3337.202119	1075234.041934	40.614516
3340.672630	1077495.904121	40.619533
3343.687851	1079769.828055	40.624551
3346.883435	1082057.510725	40.629568
3350.246536	1084357.596372	40.634586
3353.130932	1086651.435057	40.639604
3356.789470	1088980.016549	40.644621
3359.974992	1091320.096116	40.649639
3363.538506	1093633.132334	40.654656
3366.960281	1095953.985644	40.659674
3370.179331	1098285.802845	40.664692
3373.588459	1100634.320623	40.669709
3377.044631	1102974.279290	40.674727
3380.386645	1105304.666856	40.679744
3383.973867	1107668.577702	40.684762
3387.092180	1109998.209204	40.689780
3390.201370	1112333.684138	40.694797
3393.751912	1114691.183456	40.699815
3397.092426	1117056.332928	40.704832
3400.533557	1119417.761202	40.709850
3403.825075	1121779.977138	40.714868
3407.534550	1124140.131175	40.719885
3410.869037	1126497.880380	40.724903
3414.171502	1128841.122470	40.729920
3417.452059	1131216.429743	40.734938
3420.886851	1133601.929998	40.739956
3423.840444	1135963.418601	40.744973
3427.025437	1138354.688603	40.749991
3430.704203	1140733.062673	40.755008
3434.411993	1143090.187667	40.760013
3437.313189	1145402.862419	40.765018
3441.366786	1147642.596924	40.770023
3444.415710	1149823.573144	40.775028
3448.079813	1151926.941962	40.780032
3451.167451	1153934.249620	40.785037
3454.085380	1155857.743983	40.790042
3457.393615	1157724.191822	40.795047
3460.187625	1159501.464482	40.800052
3463.130198	1161197.199104	40.805056
3466.102719	1162808.469774	40.810061
3468.763881	1164322.090134	40.815066
3471.891630	1165755.582432	40.820071
3474.168332	1167118.670748	40.825076
3476.478397	1168406.450156	40.830080
3478.290680	1169628.972519	40.835085
3480.620292	1170749.696811	40.840090
3482.829312	1171830.015064	40.845095
3484.744808	1172838.480084	40.850100
3486.688953	1173778.097873	40.855104
3488.716904	1174669.543901	40.860109
3489.906796	1175507.621505	40.865114
3491.914711	1176265.127838	40.870119
3493.051079	1176973.569300	40.875124
3494.518936	1177628.150699	40.880128
3496.116573	1178267.177038	40.885133
3497.375467	1178833.831708	40.890138
3498.674969	1179330.807573	40.895143
3499.663907	1179805.841435	40.900148
3501.123218	1180248.639347	40.905152
3501.976979	1180650.063698	40.910157
3503.214778	1181014.763556	40.915162
3504.256485	1181332.767114	40.920167
3504.904308	1181619.086105	40.925172
3506.207125	1181872.893992	40.930176
3507.087711	1182097.762182	40.935181
3507.814527	1182281.411739	40.940186
3508.968461	1182455.570531	40.945191
3509.392886	1182588.517711	40.950196
3510.153207	1182681.869561	40.955200
3510.720569	1182775.722172	40.960205
3511.146431	1182836.556050	40.965210
3512.231311	1182862.075487	40.970215
3512.684608	1182887.228155	40.975220
3513.246522	1182875.934013	40.980224
3513.830735	1182861.906353	40.985229
3514.255536	1182814.864436	40.990234
3514.930493	1182746.694937	40.995239
3515.164354	1182660.805613	41.000244
3516.078665	1182569.248716	41.005248
3516.459688	1182467.611036	41.010253
3516.354746	1182335.173114	41.015258
3517.279386	1182174.695613	41.020263
3517.072539	1182033.887938	41.025268
3517.315482	1181871.159657	41.030272
3517.968468	1181684.632199	41.035277
3517.940806	1181517.794671	41.040282
3518.865596	1181299.572045	41.045287
3518.870556	1181108.799269	41.050292
3519.488596	1180891.551666	41.055296
3519.483418	1180674.303450	41.060301
3519.691402	1180418.116438	41.065306
3520.004564	1180148.996689	41.070311
3520.237228	1179913.594706	41.075316
3520.379105	1179661.148675	41.080320
3520.566744	1179394.930439	41.085325
3520.587464	1179102.161729	41.090330
3521.180951	1178822.753542	41.095335
3521.070041	1178532.989022	41.100340
3521.329752	1178223.267793	41.105344
3521.690592	1177930.282872	41.110349
3521.762943	1177619.425894	41.115354
3522.106261	1177296.443942	41.120359
3521.977527	1176986.618831	41.125364
3521.976903	1176644.805382	41.130368
3522.241190	1176303.962613	41.135373
3522.152390	1175986.908352	41.140378
3522.668021	1175655.501632	41.145383
3522.676686	1175315.955962	41.150388
3522.839812	1174950.908483	41.155392
3522.878849	1174609.143406	41.160397
3522.679513	1174261.172186	41.165402
3523.063872	1173888.753699	41.170407
3522.856728	1173528.099348	41.175412
3523.090240	1173167.536081	41.180416
3523.218527	1172829.128945	41.185421
3523.250354	1172439.782860	41.190426
3523.248716	1172075.975948	41.195431
3523.542351	1171721.717067	41.200436
3523.475573	1171333.059285	41.205440
3523.358126	1170956.457381	41.210445
3523.405470	1170587.726908	41.215450
3523.660948	1170180.153702	41.220455
3523.289445	1169794.639829	41.225460
3523.546193	1169423.055933	41.230464
3523.739661	1169050.606592	41.235469
3523.423677	1168658.109796	41.240474
3523.967140	1168255.435977	41.245479
3523.660589	1167868.258878	41.250484
3523.617254	1167460.428279	41.255488
3523.719523	1167075.485394	41.260493
3523.529647	1166676.587446	41.265498
3523.651562	1166290.639310	41.270503
3523.667259	1165888.153404	41.275508
3523.725753	1165469.195819	41.280512
3523.774128	1165079.298137	41.285517
3523.827477	1164682.191584	41.290522
3524.166331	1164264.319383	41.295527
3523.704309	1163869.219881	41.300532
3523.981014	1163467.071673	41.305536
3524.016922	1163060.113270	41.310541
3523.975685	1162660.223257	41.315546
3523.930770	1162256.428652	41.320551
3523.800195	1161845.150611	41.325556
3523.768529	1161416.054355	41.330560
3523.889609	1161023.857895	41.335565
3523.786522	1160624.862592	41.340570
3524.013810	1160194.962050	41.345575
3523.902130	1159781.533680	41.350580
3524.007875	1159367.469590	41.355584
3523.745284	1158961.755125	41.360589
3523.881584	1158536.367342	41.365594
3523.723966	1158117.046572	41.370599
3523.857618	1157711.359390	41.375604
3523.743770	1157289.127727	41.380608
3523.789400	1156867.119670	41.385613
3524.049519	1156474.087333	41.390618
3523.779859	1156069.285888	41.395623
3523.570276	1155644.383219	41.400628
3524.057423	1155203.149506	41.405632
3523.826217	1154782.249897	41.410637
3523.719405	1154373.221584	41.415642
3523.552089	1153936.248497	41.420647
3523.450074	1153540.216920	41.425652
3523.609818	1153127.356080	41.430656
3523.656786	1152714.765472	41.435661
3523.418056	1152305.598203	41.440666
3523.691435	1151871.884480	41.445671
3523.687442	1151451.533309	41.450676
3523.353094	1151025.141793	41.455680
3523.605770	1150614.625783	41.460685
3523.323921	1150191.378444	41.465690
3523.763597	1149766.178440	41.470695
3523.353655	1149371.968217	41.475700
3523.309983	1148950.950499	41.480704
3523.678489	1148520.829907	41.485709
3523.584796	1148111.218359	41.490714
3523.378437	1147681.124016	41.495719
3523.330275	1147274.756891	41.500724
3523.517896	1146833.060917	41.505728
3523.480064	1146417.906219	41.510733
3523.264855	1146007.108755	41.515738
3523.280845	1145579.366117	41.520743
3523.336214	1145173.009854	41.525748
3523.146843	1144739.734007	41.530752
3523.291579	1144316.608951	41.535757
3523.190556	1143903.732644	41.540762
3523.630963	1143465.981160	41.545767
3522.989286	1143047.721063	41.550772
3523.215113	1142626.249584	41.555776
3523.437844	1142202.278569	41.560781
3523.246975	1141771.605764	41.565786
3523.250843	1141345.894508	41.570791
3523.084564	1140955.095683	41.575796
3522.802161	1140522.913081	41.580800
3522.879838	1140100.410887	41.585805
3522.668052	1139697.189404	41.590810
3523.197642	1139274.641868	41.595815
3522.921675	1138854.281681	41.600820
3522.833186	1138445.628891	41.605824
3522.911035	1138025.809278	41.610829
3522.886568	1137599.896664	41.615834
3522.822160	1137162.276962	41.620839
3522.758534	1136762.036332	41.625844
3522.629570	1136333.665234	41.630848
3522.844022	1135927.142804	41.635853
3522.335764	1135525.077566	41.640858
3522.590481	1135087.614200	41.645863
3521.951390	1134680.186965	41.650868
3521.974150	1134279.459959	41.655872
3521.850114	1133846.897160	41.660877
3522.081015	1133462.511758	41.665882
3522.583175	1133054.391818	41.670887
3522.514052	1132635.690617	41.675892
3522.696553	1132207.315599	41.680896
3522.591616	1131795.492348	41.685901
3522.297034	1131398.782728	41.690906
3522.848126	1130968.155964	41.695911
3522.380370	1130540.039010	41.700916
3522.593563	1130128.890056	41.705920
3522.286965	1129713.135641	41.710925
3522.288868	1129286.171743	41.715930
3522.393033	1128877.797047	41.720935
3522.210959	1128493.310878	41.725940
3522.026456	1128066.755509	41.730944
3522.579274	1127640.044569	41.735949
3522.125818	1127221.646639	41.740954
3522.252438	1126817.486492	41.745959
3522.236685	1126407.800629	41.750964
3521.990259	1125971.477938	41.755968
3521.957487	1125566.012211	41.760973
3521.529206	1125176.474102	41.765978
3521.681536	1124772.249955	41.770983
3522.030938	1124351.781503	41.775988
3521.879257	1123932.695156	41.780992
3522.000642	1123528.953147	41.785997
3521.611407	1123115.553720	41.791002
3522.060137	1122705.697610	41.796007
3521.596751	1122318.051427	41.801012
3521.681391	1121892.862484	41.806016
3521.906438	1121477.806775	41.811021
3521.625927	1121076.802753	41.816026
3521.689285	1120648.565866	41.821031
3521.328193	1120257.895944	41.826036
3521.298077	1119850.376519	41.831040
3521.894829	1119451.201966	41.836045
3521.732032	1119041.451567	41.841050
3521.730171	1118629.356437	41.846055
3521.455523	1118229.281448	41.851060
3521.477664	1117806.636817	41.856064
3521.238810	1117378.473957	41.861069
3521.152022	1117000.292356	41.866074
3521.176089	1116581.268023	41.871079
3521.304979	1116189.362576	41.876084
3521.380210	1115770.266427	41.881088
3521.389156	1115375.461148	41.886093
3521.106749	1114966.562859	41.891098
3521.284081	1114571.193894	41.896103
3521.142908	1114168.886600	41.901108
3520.962610	1113756.255365	41.906112
3521.152156	1113353.164848	41.911117
3520.541486	1112969.443964	41.916122
3521.023828	1112549.170660	41.921127
3520.848127	1112166.179278	41.926132
3520.822809	1111774.930761	41.931136
3520.882471	1111367.991730	41.936141
3520.470003	1110958.141553	41.941146
3520.819122	1110567.506834	41.946151
3520.360218	1110184.229949	41.951156
3520.725687	1109792.677323	41.956160
3520.670177	1109376.921217	41.961165
3520.634110	1108988.239673	41.966170
3520.849616	1108600.061399	41.971175
3520.340327	1108217.320865	41.976180
3520.296476	1107808.410989	41.981184
3520.556655	1107409.732385	41.986189
3520.322345	1107026.670915	41.991194
3520.368363	1106639.429574	41.996199
3520.302580	1106239.572040	42.001204
3520.244094	1105835.194509	42.006208
3520.521607	1105460.246966	42.011213
3520.367429	1105067.863086	42.016218
3520.418826	1104656.787688	42.021223
3520.311149	1104270.738895	42.026228
3519.958703	1103893.493148	42.031232
3520.415719	1103500.799002	42.036237
3519.878137	1103114.547131	42.041242
3520.123668	1102717.148274	42.046247
3519.923263	1102323.903339	42.051252
3519.769404	1101934.636533	42.056256
3520.106844	1101549.275480	42.061261
3519.798648	1101162.176941	42.066266
3519.885706	1100783.016172	42.071271
3519.849447	1100393.332067	42.076276
3519.983207	1100011.049922	42.081280
3519.969413	1099627.521935	42.086285
3519.811037	1099251.640920	42.091290
3519.553230	1098851.267185	42.096295
3519.508859	1098462.114602	42.101300
3519.210264	1098077.471452	42.106304
3519.707697	1097700.322411	42.111309
3519.514790	1097333.305468	42.116314
3519.733461	1096946.870446	42.121319
3519.308158	1096580.701755	42.126324
3519.280368	1096192.244224	42.131328
3519.066278	1095815.176672	42.136333
3519.502509	1095429.458702	42.141338
3519.321224	1095047.451722	42.146343
3518.936247	1094677.702303	42.151348
3519.309695	1094317.182993	42.156352
3519.522277	1093925.268874	42.161357
3519.269470	1093557.527157	42.166362
3519.257356	1093189.433632	42.171367
3519.167937	1092803.519558	42.176372
3519.045053	1092432.041823	42.181376
3518.860455	1092052.122203	42.186381
3518.811227	1091668.706181	42.191386
3518.996214	1091303.899689	42.196391
3518.888437	1090939.595772	42.201396
3518.749386	1090561.575567	42.206400
3519.028168	1090173.593850	42.211405
3518.866909	1089811.905171	42.216410
3518.890334	1089429.181121	42.221415
3518.894447	1089079.966656	42.226420
3518.904779	1088711.853027	42.231424
3518.787196	1088345.747791	42.236429
3518.665450	1087969.939858	42.241434
3518.929823	1087572.095958	42.246439
3518.865469	1087216.831188	42.251444
3518.903073	1086847.915910	42.256448
3519.319526	1086471.244787	42.261453
3518.368740	1086111.548583	42.266458
3518.648271	1085750.859001	42.271463
3518.651482	1085380.795322	42.276468
3518.588474	1085003.238652	42.281472
3518.799642	1084639.610242	42.286477
3518.631054	1084265.184054	42.291482
3518.799155	1083890.676661	42.296487
3518.592925	1083517.739682	42.301492
3518.577153	1083134.291165	42.306496
3518.544479	1082794.750021	42.311501
3517.931972	1082433.891654	42.316506
3518.107820	1082059.736728	42.321511
3518.088884	1081700.362880	42.326516
3518.111317	1081323.400437	42.331520
3518.281015	1080965.098407	42.336525
3517.976230	1080628.441626	42.341530
3518.093782	1080260.602027	42.346535
3518.212874	1079893.697083	42.351540
3518.097727	1079530.453193	42.356544
3518.071418	1079170.817876	42.361549
3518.097808	1078838.507316	42.366554
3518.058131	1078475.276751	42.371559
3518.090038	1078117.290362	42.376564
3517.793455	1077758.086492	42.381568
3517.926776	1077387.266371	42.386573
3517.436158	1077044.658137	42.391578
3517.763376	1076676.734510	42.396583
3517.668854	1076320.475698	42.401588
3517.479339	1075965.361788	42.406592
3517.446042	1075627.103223	42.411597
3517.591893	1075295.133658	42.416602
3517.656299	1074923.197155	42.421607
3517.528214	1074583.160565	42.426612
3517.333335	1074230.624658	42.431616
3517.297024	1073872.755682	42.436621
3517.390130	1073513.208568	42.441626
3517.714118	1073177.622154	42.446631
3517.304889	1072827.048982	42.451636
3516.904785	1072491.731961	42.456640
3517.553444	1072140.267867	42.461645
3517.416775	1071786.123275	42.466650
3517.208037	1071447.731277	42.471655
3517.304647	1071093.984108	42.476660
3517.048305	1070741.137418	42.481664
3517.129007	1070407.247807	42.486669
3516.723439	1070064.861152	42.491674
3516.777214	1069721.127502	42.496679
3517.155209	1069380.492046	42.501684
3516.859651	1069032.830391	42.506688
3517.057694	1068696.605543	42.511693
3516.974639	1068360.887253	42.516698
3516.809595	1068026.219894	42.521703
3517.002124	1067685.605914	42.526708
3517.011847	1067329.225479	42.531712
3516.755697	1066993.740618	42.536717
3516.741131	1066655.213151	42.541722
3517.036000	1066319.307712	42.546727
3516.741688	1065991.657065	42.551732
3516.727392	1065638.345920	42.556736
3516.914494	1065320.005602	42.561741
3516.907049	1064981.470015	42.566746
3516.889394	1064630.307951	42.571751
3516.627622	1064284.072156	42.576756
3516.268686	1063942.931857	42.581760
3516.476020	1063615.826886	42.586765
3516.359046	1063284.135267	42.591770
3516.364309	1062956.735585	42.596775
3516.262385	1062633.281301	42.601780
3516.356880	1062295.815079	42.606784
3516.457670	1061956.979120	42.611789
3516.224890	1061636.087474	42.616794
3516.471181	1061301.905499	42.621799
3516.467021	1060965.914728	42.626804
3516.400620	1060650.716417	42.631808
3516.253121	1060300.262308	42.636813
3516.096902	1059971.844781	42.641818
3516.125965	1059654.454666	42.646823
3516.030053	1059326.470355	42.651828
3516.211418	1058986.763991	42.656832
3516.327454	1058662.077047	42.661837
3516.091701	1058346.678424	42.666842
3516.251104	1058002.675668	42.671847
3516.064439	1057683.473165	42.676852
3516.150545	1057367.869167	42.681856
3516.271949	1057035.376240	42.686861
3515.834964	1056694.570372	42.691866
3516.006676	1056376.678867	42.696871
3515.785426	1056054.014320	42.701876
3515.671812	1055712.998156	42.706880
3515.907424	1055399.570402	42.711885
3515.604901	1055099.421082	42.716890
3516.109791	1054759.593830	42.721895
3515.738810	1054416.804564	42.726900
3515.760730	1054104.688346	42.731904
3515.811079	1053786.089094	42.736909
3515.855953	1053476.440742	42.741914
3515.682263	1053131.706965	42.746919
3515.598767	1052824.454216	42.751924
3515.380369	1052519.039166	42.756928
3515.534405	1052200.813680	42.761933
3515.479094	1051888.102680	42.766938
3515.655583	1051549.579011	42.771943
3515.397817	1051240.434028	42.776948
3515.201012	1050923.543438	42.781952
3515.266080	1050620.871190	42.786957
3515.028285	1050337.337080	42.791962
3515.181942	1050011.845520	42.796967
3515.214710	1049704.207228	42.801972
3514.704407	1049380.428382	42.806977
3515.077947	1049081.481347	42.811981
3514.850840	1048762.155691	42.816986
3514.894579	1048466.318284	42.821991
3514.936487	1048171.623695	42.826996
3515.017810	1047854.125409	42.832001
3514.767432	1047531.836674	42.837005
3514.765184	1047243.278379	42.842010
3514.694412	1046941.585832	42.847015
3514.911024	1046637.995016	42.852020
3514.709397	1046333.973666	42.857025
3514.840700	1046026.018249	42.862029
3514.649513	1045748.324952	42.867034
3514.786700	1045424.594433	42.872039
3514.923434	1045114.945763	42.877044
3514.487637	1044829.230595	42.882049
3514.653083	1044531.617718	42.887053
3514.726404	1044235.066599	42.892058
3514.658044	1043928.090127	42.897063
3514.809044	1043638.642774	42.902068
3514.465614	1043323.080245	42.907073
3514.612637	1043016.790785	42.912077
3514.545769	1042730.423683	42.917082
3514.683316	1042416.276332	42.922087
3514.322246	1042116.011727	42.927092
3514.250900	1041824.670421	42.932097
3514.059067	1041531.304194	42.937101
3514.021254	1041240.119993	42.942106
3514.258313	1040963.373087	42.947111
3514.357935	1040675.326176	42.952116
3513.965068	1040361.826609	42.957121
3514.254115	1040065.113912	42.962125
3514.197974	1039789.613544	42.967130
3513.991162	1039498.365929	42.972135
3513.915255	1039200.217030	42.977140
3513.456675	1038905.595936	42.982145
3514.035690	1038634.091290	42.987149
3513.800210	1038358.839660	42.992154
3513.928333	1038062.240020	42.997159
3513.943132	1037771.058865	43.002164
3513.945007	1037487.698319	43.007169
3514.363051	1037206.576024	43.012173
3514.012221	1036932.626890	43.017178
3514.099152	1036619.707842	43.022183
3514.223148	1036334.914330	43.027188
3514.060853	1036035.352564	43.032193
3513.978989	1035741.662751	43.037197
3513.819656	1035467.996990	43.042202
3513.745900	1035166.922726	43.047207
3513.934721	1034899.557384	43.052212
3513.542314	1034625.888649	43.057217
3513.736971	1034340.207440	43.062221
3513.640526	1034036.269588	43.067226
3513.424700	1033771.432867	43.072231
3513.484821	1033484.762219	43.077236
3513.314487	1033203.922005	43.082241
3513.502236	1032932.300668	43.087245
3513.329150	1032652.691443	43.092250
3513.750833	1032367.355769	43.097255
3513.453607	1032098.774573	43.102260
3513.463878	1031816.092239	43.107265
3513.534067	1031523.316866	43.112269
3513.350828	1031254.192167	43.117274
3513.330086	1030964.597550	43.122279
3513.189792	1030699.989866	43.127284
3513.337817	1030428.446878	43.132289
3513.610572	1030140.407377	43.137293
3513.343208	1029853.700970	43.142298
3513.477017	1029572.337364	43.147303
3513.526199	1029301.918099	43.152308
3513.227147	1029023.697502	43.157313
3513.206145	1028757.040941	43.162317
3512.976311	1028501.352190	43.167322
3513.074622	1028210.723377	43.172327
3513.019299	1027941.514856	43.177332
3513.010453	1027678.001798	43.182337
3513.116281	1027391.010684	43.187341
3513.085903	1027132.029164	43.192346
3513.003902	1026860.447586	43.197351
3512.941005	1026599.121226	43.202356
3512.536263	1026329.795771	43.207361
3513.003861	1026060.798226	43.212365
3512.821474	1025791.700981	43.217370
3512.671889	1025530.726664	43.222375
3512.445100	1025279.251472	43.227380
3512.897078	1025001.579352	43.232385
3512.561962	1024718.885612	43.237389
3512.445010	1024475.110914	43.242394
3512.649855	1024205.679774	43.247399
3512.361369	1023944.460507	43.252404
3512.371596	1023685.700604	43.257409
3512.546623	1023422.247707	43.262413
3512.311104	1023173.878958	43.267418
3512.514611	1022922.808837	43.272423
3512.459356	1022660.036794	43.277428
3512.043124	1022393.432922	43.282433
3512.324205	1022131.647430	43.287437
3512.349262	1021891.907023	43.292442
3512.236653	1021627.835267	43.297447
3512.294507	1021370.415438	43.302452
3512.150983	1021136.199021	43.307457
3512.586968	1020881.119359	43.312461
3512.266438	1020613.251067	43.317466
3511.923100	1020341.396347	43.322471
3512.366338	1020116.159599	43.327476
3512.101642	1019868.231283	43.332481
3512.202199	1019603.932125	43.337485
3512.187691	1019360.112117	43.342490
3512.006623	1019103.403844	43.347495
3511.894246	1018854.338313	43.352500
3511.775974	1018606.039021	43.357505
3512.048942	1018355.238215	43.362509
3511.799377	1018107.908964	43.367514
3511.713356	1017851.904207	43.372519
3511.974715	1017603.012787	43.377524
3511.577578	1017358.780675	43.382529
3512.004322	1017115.081706	43.387533
3511.595014	1016870.345040	43.392538
3511.473080	1016606.038514	43.397543
3512.105334	1016390.037406	43.402548
3511.891972	1016146.984370	43.407553
3511.678295	1015890.037524	43.412557
3511.698899	1015654.109041	43.417562
3512.051923	1015395.687003	43.422567
3511.939395	1015142.281847	43.427572
3511.803636	1014903.823062	43.432577
3512.000201	1014644.324145	43.437581
3511.715446	1014417.328011	43.442586
3511.589260	1014149.993383	43.447591
3511.735438	1013905.424619	43.452596
3511.514097	1013674.794615	43.457601
3511.752107	1013435.143654	43.462605
3511.542971	1013195.167608	43.467610
3511.733006	1012945.887551	43.472615
3511.661596	1012701.399459	43.477620
3511.464669	1012451.092677	43.482625
3511.416944	1012209.590852	43.487629
3511.296768	1011985.092559	43.492634
3511.714879	1011743.688347	43.497639
3511.676616	1011497.976662	43.502644
3510.967621	1011271.895167	43.507649
3511.197534	1011014.458273	43.512653
3511.322028	1010777.919584	43.517658
3511.554350	1010551.459794	43.522663
3511.057642	1010326.471537	43.527668
3511.289432	1010091.344107	43.532673
3511.432329	1009848.154693	43.537677
3511.444146	1009610.516489	43.542682
3511.053076	1009365.936303	43.547687
3511.127306	1009140.223471	43.552692
3511.130476	1008906.542349	43.557697
3510.989822	1008669.958905	43.562701
3510.984834	1008428.385224	43.567706
3511.044430	1008215.372977	43.572711
3511.283165	1007981.809198	43.577716
3511.101651	1007760.750002	43.582721
3510.993075	1007537.628292	43.587725
3510.854185	1007300.987162	43.592730
3511.392522	1007063.932855	43.597735
3510.857561	1006835.505492	43.602740
3510.996367	1006591.981922	43.607745
3510.959983	1006350.616230	43.612749
3510.871435	1006136.674691	43.617754
3511.018158	1005915.780954	43.622759
3511.001436	1005687.416303	43.627764
3510.729374	1005472.896276	43.632769
3510.877845	1005240.206634	43.637773
3510.507382	1005015.374804	43.642778
3510.696601	1004770.597135	43.647783
3510.792879	1004562.110384	43.652788
3510.682748	1004338.084267	43.657793
3510.761726	1004098.646369	43.662797
3510.547137	1003891.450854	43.667802
3510.435313	1003679.463272	43.672807
3510.647837	1003444.451337	43.677812
3510.237661	1003227.533600	43.682817
3510.577531	1003005.034730	43.687821
3510.227495	1002782.251494	43.692826
3510.337301	1002560.454221	43.697831
3510.290245	1002345.389167	43.702836
3510.295934	1002144.808447	43.707841
3510.345195	1001918.713768	43.712845
3510.388516	1001717.625076	43.717850
3510.323086	1001482.382768	43.722855
3510.155990	1001253.863799	43.727860
3510.482532	1001048.616473	43.732865
3510.797283	1000837.717599	43.737869
3510.252754	1000613.031414	43.742874
3510.304221	1000398.947025	43.747879
3510.453315	1000193.405877	43.752884
3510.215216	999970.882948	43.757889
3510.756088	999736.831315	43.762893
3510.285929	999531.757614	43.767898
3510.107922	999315.527976	43.772903
3510.403961	999085.287268	43.777908
3510.042503	998884.067252	43.782913
3509.955242	998683.866137	43.787917
3510.055684	998465.805323	43.792922
3510.112537	998258.261446	43.797927
3510.389238	998053.400785	43.802932
3509.924966	997837.454081	43.807937
3510.240804	997604.325450	43.812941
3509.906925	997410.645879	43.817946
3510.224603	997203.799690	43.822951
3510.241935	996982.968115	43.827956
3509.832313	996785.480597	43.832961
3510.037312	996573.954064	43.837965
3509.830851	996361.318344	43.842970
3509.717563	996149.925850	43.847975
3509.569030	995950.125439	43.852980
3509.729273	995733.898338	43.857985
3509.545381	995525.612088	43.862989
3509.691851	995325.351348	43.867994
3509.210006	995111.544865	43.872999
3509.762949	994930.399716	43.878004
3509.454811	994753.580981	43.883009
3509.519174	994534.985206	43.888013
3509.619566	994350.972497	43.893018
3509.467147	994149.550035	43.898023
3509.834212	993925.033291	43.903028
3509.761415	993720.561104	43.908033
3509.524008	993527.707769	43.913037
3509.751456	993337.695562	43.918042
3509.657599	993118.096581	43.923047
3509.830294	992915.991966	43.928052
3509.467309	992720.694876	43.933057
3509.909502	992508.100451	43.938061
3509.394978	992305.599878	43.943066
3509.401013	992117.240712	43.948071
3509.598126	991918.313960	43.953076
3509.387602	991718.374864	43.958081
3509.455705	991537.883970	43.963085
3509.204049	991336.573147	43.968090
3509.224823	991125.556595	43.973095
3509.232039	990940.961260	43.978100
3509.216983	990747.976977	43.983105
3509.439470	990538.368208	43.988109
3508.972977	990352.271432	43.993114
3509.097465	990164.413235	43.998119
3508.801142	989974.277375	44.003124
3508.904514	989794.895759	44.008129
3509.059835	989604.087931	44.013133
3509.104193	989420.705162	44.018138
3509.307629	989203.051930	44.023143
3509.520472	989021.774564	44.028148
3509.279948	988838.224859	44.033153
3509.194796	988619.816454	44.038157
3509.161268	988440.122039	44.043162
3509.289451	988248.297667	44.048167
3508.947318	988058.983426	44.053172
3509.172537	987877.570040	44.058177
3509.398016	987687.271845	44.063181
3509.146192	987484.263611	44.068186
3509.036254	987279.565940	44.073191
3509.002018	987106.172154	44.078196
3508.681804	986920.231800	44.083201
3508.787147	986720.552985	44.088205
3508.708526	986537.000033	44.093210
3508.813052	986359.461847	44.098215
3508.757146	986177.747876	44.103220
3508.559624	985998.296245	44.108225
3509.054250	985815.992070	44.113229
3508.764830	985637.617862	44.118234
3508.884166	985426.861889	44.123239
3509.038286	985250.940396	44.128244
3508.633479	985068.077169	44.133249
3508.974634	984891.625709	44.138253
3508.902781	984708.598498	44.143258
3508.926917	984535.605028	44.148263
3508.957009	984327.459024	44.153268
3508.589268	984137.432936	44.158273
3509.043986	983957.126225	44.163277
3508.760003	983781.622128	44.168282
3508.519996	983583.257285	44.173287
3508.837516	983419.750544	44.178292
3508.509704	983258.396003	44.183297
3508.659382	983063.073610	44.188301
3508.403746	982886.756119	44.193306
3508.190151	982717.945810	44.198311
3508.700698	982530.455933	44.203316
3508.676975	982367.268244	44.208321
3508.678163	982178.092773	44.213325
3508.562446	981991.958028	44.218330
3508.683617	981790.834355	44.223335
3508.575562	981614.648621	44.228340
3508.426914	981438.561817	44.233345
3508.570806	981261.151546	44.238349
3508.163187	981102.484294	44.243354
3508.130739	980929.000116	44.248359
3508.408900	980734.651502	44.253364
3508.277247	980584.423466	44.258369
3508.616631	980394.644778	44.263373
3508.291596	980221.578104	44.268378
3508.223991	980041.917744	44.273383
3508.478320	979878.124653	44.278388
3508.339046	979714.293993	44.283393
3508.231163	979537.848785	44.288397
3508.215750	979360.112622	44.293402
3508.279855	979173.270160	44.298407
3508.451755	979019.726348	44.303412
3508.156243	978847.004075	44.308417
3508.122473	978680.097006	44.313421
3508.004351	978503.817034	44.318426
3507.872602	978337.404747	44.323431
3508.328560	978159.455912	44.328436
3508.139250	977990.110974	44.333441
3508.336148	977830.373680	44.338445
3508.274937	977653.764928	44.343450
3508.359191	977464.810755	44.348455
3508.397353	977287.881108	44.353460
3507.667945	977133.066634	44.358465
3507.892529	976952.283584	44.363469
3507.790346	976799.214114	44.368474
3507.915427	976651.284409	44.373479
3507.800376	976481.784850	44.378484
3507.786138	976312.068136	44.383489
3507.803274	976143.807759	44.388493
3507.949320	975980.116472	44.393498
3508.164130	975807.609484	44.398503
3508.107440	975641.790884	44.403508
3507.946162	975485.176040	44.408513
3508.007861	975321.577612	44.413517
3507.999151	975141.851464	44.418522
3508.035584	974973.749116	44.423527
3508.173631	974825.770140	44.428532
3508.081233	974656.897388	44.433537
3507.974344	974482.545411	44.438541
3507.717017	974321.220306	44.443546
3507.620578	974171.209254	44.448551
3507.747808	973998.466633	44.453556
3507.536093	973824.209700	44.458561
3507.557299	973665.461087	44.463565
3507.611584	973530.080077	44.468570
3507.541443	973382.685023	44.473575
3507.529364	973198.594597	44.478580
3507.571576	973037.086198	44.483585
3507.540472	972876.270099	44.488589
3507.378359	972736.601721	44.493594
3507.553218	972583.471812	44.498599
3507.462246	972436.936350	44.503604
3507.342091	972271.911198	44.508609
3507.616394	972104.957414	44.513613
3507.432065	971940.813848	44.518618
3507.296121	971779.788601	44.523623
3507.779733	971623.940470	44.528628
3507.218847	971479.023475	44.533633
3507.381953	971321.165100	44.538637
3507.338060	971167.642042	44.543642
3507.211275	971011.682123	44.548647
3507.280261	970849.129168	44.553652
3506.834003	970712.785530	44.558657
3507.279616	970546.247511	44.563661
3507.327876	970418.036015	44.568666
3506.952551	970279.713078	44.573671
3506.914687	970119.016561	44.578676
3506.809051	969964.982156	44.583681
3506.826840	969811.412674	44.588685
3506.723703	969676.456058	44.593690
3506.457060	969528.602846	44.598695
3506.748819	969406.397318	44.603700
3506.660054	969283.958210	44.608705
3506.757719	969114.205765	44.613709
3506.668814	968968.462411	44.618714
3506.831686	968850.475611	44.623719
3506.910292	968701.761110	44.628724
3506.864694	968573.034417	44.633729
3506.856386	968432.550681	44.638733
3506.894412	968297.636329	44.643738
3506.625677	968139.565838	44.648743
3507.011481	967996.363089	44.653748
3506.784802	967862.754929	44.658753
3506.813296	967701.784056	44.663757
3506.547908	967578.162743	44.668762
3506.311731	967449.148526	44.673767
3506.443873	967310.768418	44.678772
3506.380503	967165.856425	44.683777
3506.397701	967024.942405	44.688781
3506.598846	966915.918627	44.693786
3506.452978	966763.078056	44.698791
3506.083218	966632.990312	44.703796
3506.188003	966523.974978	44.708801
3506.415273	966383.206504	44.713805
3506.475969	966254.116580	44.718810
3506.528670	966126.690048	44.723815
3506.684977	965986.315315	44.728820
3506.269307	965840.546483	44.733825
3506.527849	965707.591881	44.738829
3506.176194	965578.162923	44.743834
3506.307416	965440.521577	44.748839
3506.747872	965321.633056	44.753844
3506.461352	965208.151399	44.758849
3506.570308	965045.133830	44.763853
3506.339537	964901.073984	44.768858
3506.545491	964773.984106	44.773863
3506.694708	964655.129798	44.778868
3506.287879	964501.194513	44.783873
3506.618163	964354.579404	44.788877
3506.380830	964244.303639	44.793882
3506.648385	964125.124988	44.798887
3506.657419	963970.127274	44.803892
3506.399762	963853.087001	44.808897
3506.296096	963716.324934	44.813901
3506.650925	963584.775175	44.818906
3506.448505	963464.386490	44.823911
3506.473503	963320.146976	44.828916
3506.207427	963199.861233	44.833921
3506.498064	963067.918293	44.838925
3506.253487	962930.082861	44.843930
3506.007489	962805.179855	44.848935
3506.441640	962675.262206	44.853940
3506.424265	962557.666042	44.858945
3506.337567	962402.053907	44.863949
3506.422120	962284.827400	44.868954
3506.224701	962159.804398	44.873959
3506.348063	962036.686031	44.878964
3506.169380	961916.261085	44.883969
3506.227669	961765.998508	44.888973
3506.346467	961634.443121	44.893978
3506.310270	961498.009353	44.898983
3506.187771	961391.090683	44.903988
3505.970724	961272.619010	44.908993
3506.131783	961142.025651	44.913997
3506.289970	961035.054150	44.919002
3506.130257	960897.646260	44.924007
3506.196195	960743.630703	44.929012
3506.330462	960624.891798	44.934017
3506.229363	960506.777426	44.939021
3506.256943	960391.286442	44.944026
3505.972014	960249.275985	44.949031
3506.101186	960112.782210	44.954036
3505.917353	960003.102739	44.959041
3505.787985	959873.606984	44.964045
3505.989367	959765.526328	44.969050
3506.167128	959644.897188	44.974055
3505.853919	959524.836653	44.979060
3505.709749	959394.254009	44.984065
3505.924164	959273.611073	44.989069
3505.945593	959160.253697	44.994074
3505.736061	959039.871820	44.999079
3506.004434	958927.940110	45.004084
3505.623951	958813.465378	45.009089
3505.869074	958688.098085	45.014093
3505.955067	958553.339735	45.019098
3505.777862	958462.360896	45.024103
3505.982242	958343.857725	45.029108
3506.004254	958214.594029	45.034113
3506.126178	958099.532019	45.039117
3505.667471	957992.213423	45.044122
3505.572052	957850.799265	45.049127
3505.629961	957727.893973	45.054132
3505.546681	957620.016211	45.059137
3505.704250	957500.914955	45.064141
3506.096668	957379.026094	45.069146
3505.502057	957293.100075	45.074151
3505.943356	957161.487691	45.079156
3505.653466	957041.371652	45.084161
3506.103495	956915.147386	45.089165
3505.955589	956816.682485	45.094170
3505.671500	956700.188012	45.099175
3505.850232	956576.453529	45.104180
3505.335082	956477.258514	45.109185
3505.615240	956357.917305	45.114189
3505.922996	956235.625860	45.119194
3505.721046	956122.049429	45.124199
3505.882639	956009.588225	45.129204
3505.593780	955911.425446	45.134209
3505.712769	955769.130665	45.139213
3505.902980	955660.662711	45.144218
3505.651949	955567.565294	45.149223
3505.678245	955456.633715	45.154228
3505.384837	955333.033556	45.159233
3505.633843	955220.721330	45.164237
3505.330791	955115.000703	45.169242
3505.510002	954988.254028	45.174247
3505.621390	954902.544421	45.179252
3505.001405	954797.921434	45.184257
3505.160992	954675.760956	45.189261
3504.702742	954585.070769	45.194266
3505.506864	954485.371598	45.199271
3505.465658	954377.105728	45.204276
3505.545455	954287.660706	45.209281
3505.325170	954181.620131	45.214285
3505.345900	954063.772206	45.219290
3505.297919	953952.054882	45.224295
3505.490273	953866.792820	45.229300
3505.302136	953759.398965	45.234305
3505.464418	953652.423445	45.239309
3505.428674	953557.436270	45.244314
3505.354430	953451.547801	45.249319
3505.590664	953332.786525	45.254324
3505.321965	953222.046267	45.259329
3505.557868	953116.195437	45.264333
3505.273757	953006.601112	45.269338
3504.998683	952918.912704	45.274343
3504.966501	952819.510150	45.279348
3505.043498	952729.081529	45.284353
3505.396782	952614.876905	45.289357
3504.950613	952512.092039	45.294362
3504.915022	952416.222490	45.299367
3505.140901	952328.824196	45.304372
3504.843039	952232.228907	45.309377
3505.052768	952130.763678	45.314381
3505.313791	952024.407686	45.319386
3505.084310	951934.589670	45.324391
3504.887530	951843.233561	45.329396
3504.561412	951742.423074	45.334401
3504.989527	951629.141132	45.339405
3504.854587	951550.880467	45.344410
3504.543433	951443.075439	45.349415
3504.890299	951347.410011	45.354420
3504.728306	951275.848945	45.359425
3504.911730	951193.989263	45.364429
3504.985244	951091.855962	45.369434
3504.958263	950982.941653	45.374439
3505.093009	950895.151095	45.379444
3504.650308	950794.628319	45.384449
3504.822762	950698.692389	45.389453
3504.988564	950621.325182	45.394458
3504.707138	950521.057641	45.399463
3504.839697	950422.538678	45.404468
3504.627902	950350.015686	45.409473
3504.922855	950232.417315	45.414477
3504.886981	950121.954606	45.419482
3504.699259	950039.084652	45.424487
3504.738652	949965.461839	45.429492
3504.734477	949874.900547	45.434497
3504.721160	949778.595120	45.439501
3504.482665	949693.621809	45.444506
3504.284821	949601.268619	45.449511
3504.688232	949497.326026	45.454516
3504.751804	949414.500360	45.459521
3504.672050	949319.250432	45.464525
3504.724749	949238.530066	45.469530
3504.449982	949159.202811	45.474535
3504.586580	949068.604149	45.479540
3504.326016	948970.696628	45.484545
3504.819406	948874.769587	45.489549
3504.893453	948801.220173	45.494554
3504.639551	948704.647033	45.499559
3504.594902	948613.687214	45.504564
3504.382791	948539.032122	45.509569
3504.657948	948457.305311	45.514573
3504.762826	948365.454659	45.519578
3504.362939	948286.613380	45.524583
3505.058749	948181.830022	45.529588
3504.847032	948086.004460	45.534593
3504.715910	947995.431047	45.539597
3504.869159	947911.608798	45.544602
3504.519565	947818.290964	45.549607
3504.696808	947741.549021	45.554612
3504.300933	947668.060858	45.559617
3504.480817	947571.969708	45.564621
3504.409346	947492.583329	45.569626
3504.225898	947400.954565	45.574631
3504.972706	947303.807273	45.579636
3504.564625	947216.809687	45.584641
3504.921041	947150.757006	45.589645
3504.721866	947055.197603	45.594650
3504.678834	946964.400037	45.599655
3504.703275	946873.589764	45.604660
3504.473954	946787.130232	45.609665
3504.545729	946680.120288	45.614669
3504.672857	946610.075225	45.619674
3504.549626	946518.325112	45.624679
3504.533100	946433.740518	45.629684
3504.323749	946364.705519	45.634689
3504.143569	946270.086461	45.639693
3504.361293	946180.669187	45.644698
3504.291519	946091.201922	45.649703
3504.470347	946012.709637	45.654708
3504.512025	945948.034720	45.659713
3504.359182	945848.900621	45.664717
3504.265208	945753.970518	45.669722
3503.813316	945676.535115	45.674727
3504.509917	945604.179026	45.679732
3503.709646	945555.255142	45.684737
3504.093901	945470.205561	45.689741
3504.337274	945397.442173	45.694746
3504.025301	945313.750303	45.699751
3504.384482	945223.909971	45.704756
3504.554018	945165.049162	45.709761
3504.742729	945067.664450	45.714765
3504.343687	944993.755537	45.719770
3504.142898	944909.463897	45.724775
3504.509236	944812.045135	45.729780
3504.419778	944734.440144	45.734785
3504.346364	944649.835827	45.739789
3504.123377	944558.354951	45.744794
3504.083873	944500.096026	45.749799
3504.391171	944415.712687	45.754804
3504.028451	944323.675694	45.759809
3504.313394	944255.202048	45.764813
3504.015823	944169.285118	45.769818
3503.848818	944037.725414	45.774823
3503.998772	943838.061298	45.779828
3504.036983	943585.307983	45.784833
3504.102884	943267.740524	45.789837
3504.076021	942884.983474	45.794842
3503.951738	942467.605661	45.799847
3504.056830	941949.580752	45.804852
3504.086095	941378.586328	45.809857
3503.941840	940747.524529	45.814861
3503.633064	940036.230349	45.819866
3503.332651	939269.488149	45.824871
3503.395518	938450.669285	45.829876
3503.368394	937532.420481	45.834881
3503.343025	936559.592454	45.839885
3503.351404	935519.958584	45.844890
3503.098459	934392.308841	45.849895
3503.203857	933164.864760	45.854900
3502.944038	931877.831135	45.859905
3502.658828	930510.739180	45.864909
3502.356225	929072.369361	45.869914
3501.857813	927553.849847	45.874919
3502.202648	925946.672247	45.879924
3501.780298	924249.581096	45.884929
3501.647638	922481.276633	45.889933
3501.299783	920629.549037	45.894938
3500.943293	918674.347847	45.899943
3500.899969	916645.664011	45.904948
3500.547830	914525.211207	45.909953
3500.151999	912323.062498	45.914957
3500.001533	910052.193560	45.919962
3499.512864	907669.779366	45.924967
3499.025072	905216.845253	45.929972
3498.961960	902688.308942	45.934977
3498.675155	900039.639535	45.939981
3498.492453	897309.674688	45.944986
3498.077935	894504.549961	45.949991
3497.718414	891630.501976	45.954996
3497.391402	888655.975846	45.960001
3496.929291	885564.580646	45.965005
3496.505117	882415.425437	45.970010
3496.135277	879190.195579	45.975015
3495.631796	875861.254648	45.980020
3494.984598	872447.470598	45.985025
3494.634650	868949.028191	45.990029
3494.430858	865361.737957	45.995034
3493.655686	861697.052576	46.000039
3493.414541	857946.104577	46.005044
3492.826973	854114.839724	46.010049
3492.180725	850175.702853	46.015053
3491.806061	846164.335294	46.020058
3490.989299	842071.081136	46.025063
3490.657772	837889.063683	46.030068
3489.817897	833624.696812	46.035073
3489.318296	829258.447368	46.040077
3488.914273	824818.302449	46.045082
3488.101039	820291.892338	46.050087
3487.791193	815695.524759	46.055092
3486.761243	810992.729492	46.060097
3486.190890	806174.689905	46.065101
3485.307202	801300.467996	46.070106
3484.550935	796351.788239	46.075111
3483.971093	791317.712217	46.080116
3483.261215	786180.837576	46.085121
3482.476826	780956.925269	46.090125
3481.661058	775656.022065	46.095130
3480.567870	770264.198944	46.100135
3480.137271	764777.157665	46.105140
3479.548990	759238.712255	46.110145
3478.523714	753580.630430	46.115149
3477.850551	747814.736909	46.120154
3477.146888	741994.049705	46.125159
3476.069623	736078.810830	46.130164
3474.809286	730086.779521	46.135169
3474.356637	723987.097535	46.140173
3473.634053	717809.743613	46.145178
3472.683575	711518.462239	46.150183
3471.894783	705128.565854	46.155188
3470.543958	698688.320531	46.160193
3469.578533	692165.491299	46.165197
3468.848352	685524.596543	46.170202
3467.413586	678793.328994	46.175207
3466.516527	672003.146019	46.180212
3465.100918	665107.321549	46.185217
3464.338809	658127.156365	46.190221
3463.618931	651080.612397	46.195226
3462.164915	643943.970328	46.200231
3461.092954	636690.934172	46.205236
3459.576710	629368.635102	46.210241
3458.675334	621947.045083	46.215245
3457.418386	614476.739890	46.220250
3455.941886	606898.444506	46.225255
3454.787524	599226.337112	46.230260
3453.742113	591489.237198	46.235265
3452.250707	583644.544667	46.240269
3451.029880	575748.270335	46.245274
3449.218418	567745.813526	46.250279
3448.326742	559650.820830	46.255284
3446.933437	551482.100856	46.260289
3445.483145	543224.007713	46.265293
3443.930068	534891.177090	46.270298
3442.651117	526476.905551	46.275303
3441.093915	517962.306265	46.280308
3439.372235	509378.800167	46.285313
3437.885495	500718.788978	46.290317
3436.156438	491975.164028	46.295322
3434.230525	483154.393491	46.300327
3432.813822	474247.053029	46.305332
3430.853489	465274.303528	46.310337
3429.220735	456208.869914	46.315341
3427.556448	447088.665325	46.320346
3425.756215	437893.634036	46.325351
3423.761243	428607.138963	46.330356
3421.813472	419250.283575	46.335361
3419.720127	409836.536314	46.340365
3418.126128	400335.373548	46.345370
3415.939513	390752.795087	46.350375
3414.094060	381112.941956	46.355380
3411.790268	371418.534021	46.360385
3409.615029	361644.931003	46.365389
3407.170940	351781.454630	46.370394
3404.777743	341878.131085	46.375399
3402.706890	331917.822297	46.380404
3400.048133	321904.377523	46.385409
3397.876270	311819.483716	46.390413
3395.498176	301661.694995	46.395418
3392.383497	291476.914204	46.400423
3389.783757	281225.075948	46.405428
3387.077465	270931.492319	46.410433
3384.434211	260595.353211	46.415437
3381.589092	250203.498275	46.420442
3378.496511	239755.549760	46.425447
3375.437365	229263.894119	46.430452
3372.683144	218666.853184	46.435457
3369.549544	208109.649140	46.440461
3366.288353	197499.461222	46.445466
3362.428856	186897.015564	46.450471
3359.208063	176259.839114	46.455476
3355.471106	165589.203100	46.460481
3351.106889	154879.116399	46.465485
3346.743073	144187.004946	46.470490
3342.848451	133506.164916	46.475495
3338.455170	122810.228998	46.480500
3333.816397	112109.965846	46.485505
3328.578854	101440.120547	46.490509
3322.843120	90774.704054	46.495514
3315.376382	80201.381734	46.500519
3300.544244	69878.433493	46.505524
3268.077563	60175.572720	46.510529
3232.387728	50904.163720	46.515533
3190.158708	42319.320558	46.520538
3143.864773	34603.776475	46.525543
3097.364822	27742.970802	46.530548
3053.247020	21782.333644	46.535553
3015.179429	16662.073874	46.540557
2983.207213	12394.847570	46.545562
2956.304381	8930.179090	46.550567
2934.583360	6176.159472	46.555572
2916.526105	4033.021106	46.560577
2902.293426	2466.847046	46.565581
2890.251106	1366.819004	46.570586
2880.617367	629.348826	46.575591
2870.147076	292.977342	46.580596
2857.940406	308.945923	46.585601
2857.860428	324.778978	46.590605
2865.010768	338.424901	46.595610
2870.771879	405.085409	46.600615
2873.143609	537.070227	46.605620
2874.309050	699.386582	46.610625
2874.585466	834.284687	46.615629
2875.926833	923.955846	46.620634
2876.111584	974.971981	46.625639
2876.574995	1021.417624	46.630644
2876.360102	1034.135035	46.635649
2876.090206	1003.632861	46.640653
2876.293826	912.970968	46.645658
2875.415512	805.974094	46.650663
2874.818352	660.936778	46.655668
2873.663686	499.219862	46.660673
2870.820560	311.809909	46.665677
2863.216885	251.914861	46.670682
2853.241863	293.339735	46.675687
2847.142969	293.534715	46.680692
2843.542640	293.654781	46.685697
2841.319617	296.639892	46.690701
2839.328285	295.933777	46.695706
2836.935611	296.003223	46.700711
2834.126634	283.849548	46.705716
2831.319175	275.948946	46.710721
2828.319512	279.836499	46.715725
2825.274500	290.055814	46.720730
2822.192343	286.878997	46.725735
2818.658174	269.545691	46.730740
2814.717073	273.760302	46.735745
2811.459702	280.532464	46.740749
2808.298882	261.933989	46.745754
2804.795567	266.039731	46.750759
2801.902621	275.678967	46.755764
2798.885246	289.587006	46.760769
2795.557744	275.711862	46.765773
2792.149354	265.928863	46.770778
2788.769212	268.903207	46.775783
2785.307335	267.446338	46.780788
2781.978533	262.308296	46.785793
2778.766923	278.757424	46.790797
2775.545784	252.562095	46.795802
2771.729838	267.230181	46.800807
2768.443081	268.718359	46.805812
2764.860973	265.211541	46.810817
2761.460753	268.206272	46.815821
2758.280022	259.957754	46.820826
2754.800574	269.992802	46.825831
2751.528610	252.186214	46.830836
2748.102421	257.190592	46.835841
2744.220387	269.700759	46.840845
2741.389486	261.226374	46.845850
2737.991795	272.210677	46.850855
2734.904247	272.047274	46.855860
2731.563931	268.019291	46.860865
2727.679193	263.168459	46.865869
2724.048829	237.962843	46.870874
2720.393460	269.879290	46.875879
2717.510931	268.429923	46.880884
2714.014363	264.516004	46.885889
2710.449717	267.231557	46.890893
2707.077548	266.482644	46.895898
2703.638751	261.163503	46.900903
2700.435927	250.411961	46.905908
2696.578498	257.508406	46.910913
2692.750959	258.499696	46.915917
2689.677034	240.755705	46.920922
2685.950776	237.301802	46.925927
2682.613393	251.124684	46.930932
2679.811656	261.367343	46.935937
2676.553743	244.332305	46.940941
2673.129311	230.001413	46.945946
2668.968520	259.483533	46.950951
2665.666619	259.706399	46.955956
2662.035926	247.744257	46.960961
2658.672170	249.733986	46.965965
2655.555134	253.256801	46.970970
2651.544700	263.026855	46.975975
2647.890432	264.587812	46.980980
2644.300399	248.903911	46.985985
2640.869701	235.876740	46.990989
2638.052836	238.858492	46.995994
2634.329148	245.446956	47.000999
2631.582519	233.631574	47.006004
2628.011720	237.645714	47.011009
2624.185265	254.971917	47.016013
2620.759470	249.167687	47.021018
2616.705105	239.198324	47.026023
2613.529316	241.484003	47.031028
2610.288846	245.526848	47.036033
2606.902647	251.076335	47.041037
2603.411190	231.252161	47.046042
2599.601009	222.891292	47.051047
2596.365690	221.759599	47.056052
2592.699031	242.819093	47.061057
2589.197502	252.831093	47.066061
2586.071155	239.711050	47.071066
2582.357499	234.591985	47.076071
2578.906383	226.181488	47.081076
2575.437487	236.302142	47.086081
2571.672752	248.064879	47.091085
2568.721623	235.569218	47.096090
2564.852333	245.096231	47.101095
2561.747875	233.521894	47.106100
2558.645379	225.855947	47.111105
2554.928553	238.507313	47.116109
2551.262281	239.541233	47.121114
2547.349872	254.122396	47.126119
2543.582448	229.746091	47.131124
2540.511522	230.821435	47.136129
2536.994301	240.646330	47.141133
2533.724545	239.707972	47.146138
2529.803241	240.216818	47.151143
2526.991789	225.601451	47.156148
2523.092310	235.441437	47.161153
2519.489475	239.844161	47.166157
2516.101368	241.356849	47.171162
2512.743691	236.208122	47.176167
2509.246026	217.265405	47.181172
2506.159202	224.412018	47.186177
2502.539065	237.464548	47.191181
2498.895879	248.381373	47.196186
2495.094645	232.986336	47.201191
2491.358680	237.425921	47.206196
2488.685188	230.090273	47.211201
2484.757929	216.025716	47.216205
2481.263711	225.036027	47.221210
2477.898647	233.399508	47.226215
2474.704473	209.925611	47.231220
2470.460334	221.794946	47.236225
2467.137978	239.811762	47.241229
2464.236346	226.206181	47.246234
2460.442392	215.013449	47.251239
2457.518140	225.962453	47.256244
2453.706207	240.030760	47.261249
2449.776704	232.015293	47.266253
2446.402305	212.393216	47.271258
2442.506002	222.054643	47.276263
2439.419486	216.308312	47.281268
2435.789628	227.902347	47.286273
2432.092779	218.890347	47.291277
2429.381951	212.587043	47.296282
2425.589870	231.513728	47.301287
2422.291557	235.827701	47.306292
2418.441200	225.270123	47.311297
2414.685934	211.491156	47.316301
2411.679614	228.091137	47.321306
2407.902199	222.018779	47.326311
2404.698416	225.356912	47.331316
2401.221259	230.840677	47.336321
2397.636847	234.899283	47.341325
2394.142160	207.341089	47.346330
2390.183170	210.698017	47.351335
2387.317997	215.110935	47.356340
2383.524705	226.153856	47.361345
2379.963603	222.998914	47.366349
2377.160739	219.818369	47.371354
2373.187345	212.531525	47.376359
2369.468538	208.483090	47.381364
2365.997149	204.681024	47.386369
2362.455443	222.079282	47.391373
2359.607278	223.979072	47.396378
2355.472579	227.320606	47.401383
2352.083697	201.525040	47.406388
2348.584142	200.193863	47.411393
2345.202514	215.940078	47.416397
2341.748310	215.986167	47.421402
2338.006910	211.078587	47.426407
2334.871910	215.234649	47.431412
2331.171563	211.350992	47.436417
2327.660149	213.374580	47.441421
2324.397485	212.921391	47.446426
2320.157799	225.416285	47.451431
2317.082654	204.530279	47.456436
2313.976485	191.175472	47.461441
2310.368278	203.570746	47.466445
2307.023351	201.352188	47.471450
2303.276726	201.536491	47.476455
2299.816144	202.148716	47.481460
2296.237249	214.827224	47.486465
2292.404594	225.181881	47.491469
2289.062426	203.702362	47.496474
2285.515925	200.405281	47.501479
2282.285204	203.740897	47.506484
2278.805181	210.988731	47.511489
2274.993457	201.937577	47.516493
2271.757215	205.141030	47.521498
2267.737104	201.364209	47.526503
2264.545078	213.573175	47.531508
2261.129912	213.338519	47.536513
2258.001648	205.119907	47.541517
2254.432969	193.627463	47.546522
2250.614525	208.857693	47.551527
2247.169988	208.554098	47.556532
2244.060079	212.581065	47.561537
2240.159117	209.968300	47.566541
2237.505330	196.455955	47.571546
2233.419232	211.434589	47.576551
2229.873555	212.131414	47.581556
2226.385187	199.914274	47.586561
2222.568406	192.150973	47.591565
2218.870144	206.882249	47.596570
2215.290822	217.991151	47.601575
2212.338024	211.295569	47.606580
2208.914567	198.194592	47.611585
2205.450710	201.618213	47.616589
2201.882579	192.847837	47.621594
2198.061080	190.127980	47.626599
2194.890315	181.794395	47.631604
2191.527159	204.280361	47.636609
2187.390701	215.329342	47.641613
2184.434064	206.595722	47.646618
2181.011318	202.494417	47.651623
2177.232798	198.269195	47.656628
2173.857349	198.076761	47.661633
2170.000955	214.875591	47.666637
2166.724324	188.894852	47.671642
2163.321499	183.837718	47.676647
2159.663974	187.807755	47.681652
2156.076274	203.114386	47.686657
2152.444268	212.962477	47.691661
2149.578278	193.962106	47.696666
2145.935845	188.487459	47.701671
2142.221710	189.737025	47.706676
2138.596679	186.195403	47.711681
2134.824205	188.929892	47.716685
2131.751512	196.103585	47.721690
2128.249949	201.205364	47.726695
2124.826540	180.593890	47.731700
2121.652006	188.436155	47.736705
2117.637123	194.591738	47.741709
2114.777074	194.923572	47.746714
2110.808918	196.557268	47.751719
2107.214508	205.241920	47.756724
2103.718979	195.703280	47.761729
2100.245185	188.356695	47.766733
2096.836926	191.165385	47.771738
2093.162957	217.737606	47.776743
2089.880368	195.786925	47.781748
2086.475732	178.853375	47.786753
2082.897695	200.141593	47.791757
2079.415178	200.709593	47.796762
2075.612294	200.273614	47.801767
2071.937631	175.581478	47.806772
2068.739589	185.520476	47.811777
2065.090140	200.744786	47.816781
2061.781067	196.538373	47.821786
2057.969853	192.231703	47.826791
2054.847905	186.027762	47.831796
2051.381983	188.159386	47.836801
2047.869243	207.999734	47.841805
2044.491734	203.560163	47.846810
2040.721146	187.103104	47.851815
2037.334165	169.431059	47.856820
2033.651386	192.784410	47.861825
2030.170055	200.615964	47.866829
2027.060341	188.945846	47.871834
2023.254590	192.751879	47.876839
2020.036978	199.580965	47.881844
2016.495459	206.336823	47.886849
2012.421559	195.558629	47.891853
2009.240548	183.626141	47.896858
2005.529656	195.500620	47.901863
2002.240441	188.709614	47.906868
1999.073268	196.250129	47.911873
1995.043873	200.128388	47.916877
1991.969716	169.579806	47.921882
1988.174444	184.557294	47.926887
1984.676024	190.362175	47.931892
1981.160409	194.941125	47.936897
1977.685652	192.597650	47.941901
1974.578963	181.889092	47.946906
1970.832228	184.602149	47.951911
1966.859814	177.639964	47.956916
1963.790410	177.271855	47.961921
1960.437481	191.695965	47.966925
1956.855801	196.825237	47.971930
1953.175012	187.821546	47.976935
1949.387686	172.584556	47.981940
1946.266506	192.107378	47.986945
1942.962336	190.522798	47.991949
1939.398650	194.790272	47.996954
1935.834601	181.917364	48.001959
1932.347350	183.882490	48.006964
1928.997366	169.125603	48.011969
1924.970505	181.774832	48.016973
1921.662077	161.061493	48.021978
1918.294010	183.745891	48.026983
1914.479667	191.077921	48.031988
1911.119058	180.788917	48.036993
1907.565840	164.976987	48.041997
1904.393131	159.021913	48.047002
1900.792941	190.002995	48.052007
1897.306641	193.420980	48.057012
1893.841762	166.090056	48.062017
1890.347171	161.804846	48.067021
1886.932838	176.634676	48.072026
1883.365380	189.667641	48.077031
1879.581353	179.894702	48.082036
1876.170003	187.745543	48.087041
1872.760373	188.385368	48.092045
1869.374997	173.775617	48.097050
1865.685657	181.509552	48.102055
1862.020909	185.134758	48.107060
1858.775737	177.400094	48.112065
1855.444591	170.826017	48.117069
1851.916200	175.457140	48.122074
1848.199693	187.851690	48.127079
1844.641019	171.512529	48.132084
1841.196546	177.064508	48.137089
1837.409926	174.561847	48.142093
1834.640613	161.620836	48.147098
1830.420913	170.659806	48.152103
1827.011720	182.860813	48.157108
1823.598756	188.933403	48.162113
1819.843132	190.619193	48.167117
1817.163799	170.191977	48.172122
1813.472932	179.978769	48.177127
1809.675470	166.500980	48.182132
1806.174963	168.880504	48.187137
1802.442667	175.188087	48.192141
1799.259589	176.953042	48.197146
1795.247463	177.408697	48.202151
1792.029966	157.812737	48.207156
1788.993333	155.332460	48.212161
1785.520861	175.500118	48.217165
1781.590867	183.515388	48.222170
1777.938016	179.959512	48.227175
1774.119941	171.195224	48.232180
1771.144844	166.013666	48.237185
1767.732062	170.973684	48.242189
1764.514957	150.131164	48.247194
1761.185590	160.905471	48.252199
1757.502746	172.648835	48.257204
1753.952781	174.772362	48.262209
1749.895595	169.858340	48.267213
1746.432183	159.158472	48.272218
1743.058002	171.163527	48.277223
1739.541854	162.269739	48.282228
1736.413988	170.557524	48.287233
1732.727641	190.704374	48.292237
1729.364700	173.121981	48.297242
1725.397864	164.212697	48.302247
1721.497943	156.444594	48.307252
1718.703013	159.454501	48.312257
1714.985047	169.479003	48.317261
1711.983606	175.507997	48.322266
1708.142177	163.798313	48.327271
1704.558471	179.041669	48.332276
1701.501589	179.363625	48.337281
1697.552920	175.614030	48.342285
1694.292273	157.720333	48.347290
1690.580665	171.987654	48.352295
1686.664308	171.109720	48.357300
1683.484509	152.655591	48.362305
1679.890864	166.805882	48.367309
1676.927445	172.326690	48.372314
1673.320159	165.548402	48.377319
1669.752821	164.849347	48.382324
1666.215937	168.046222	48.387329
1662.378508	180.561807	48.392333
1659.016841	177.375527	48.397338
1655.457903	166.148412	48.402343
1652.084558	158.124178	48.407348
1648.938462	169.717848	48.412353
1645.496465	170.676822	48.417357
1641.532023	171.962416	48.422362
1637.584604	158.910601	48.427367
1634.595556	161.758333	48.432372
1631.084560	175.767261	48.437377
1627.375872	182.306110	48.442381
1624.012583	164.149523	48.447386
1620.484702	161.020981	48.452391
1616.990563	165.293688	48.457396
1613.413858	179.340005	48.462401
1609.721601	166.487390	48.467405
1606.666680	150.186127	48.472410
1602.968213	167.096265	48.477415
1599.302752	161.303452	48.482420
1596.169516	149.761685	48.487425
1592.567503	164.184570	48.492429
1589.493155	172.079734	48.497434
1585.811781	169.622586	48.502439
1581.996767	159.815898	48.507444
1578.556575	144.421287	48.512449
1574.735678	168.936111	48.517453
1571.412457	177.557073	48.522458
1568.128532	168.096502	48.527463
1564.576871	174.256598	48.532468
1561.306067	178.494055	48.537473
1557.199704	168.033279	48.542477
1553.862912	150.461215	48.547482
1550.288243	152.075648	48.552487
1547.084684	158.886790	48.557492
1543.680161	157.192106	48.562497
1540.035737	154.938022	48.567501
1536.755489	164.977564	48.572506
1533.098144	184.927612	48.577511
1529.536081	175.715287	48.582516
1525.872797	164.617243	48.587521
1522.281857	169.737574	48.592525
1519.177760	165.606130	48.597530
1515.466749	165.452220	48.602535
1511.921860	154.264120	48.607540
1508.462550	151.384951	48.612545
1505.008959	173.522333	48.617549
1501.565593	163.597044	48.622554
1497.945559	158.857066	48.627559
1494.137493	173.232023	48.632564
1491.187619	160.663599	48.637569
1487.229737	158.590998	48.642573
1484.190564	164.017934	48.647578
1480.586531	174.856324	48.652583
1477.163350	149.550043	48.657588
1473.789614	169.555976	48.662593
1469.664592	169.381339	48.667597
1466.196902	150.963424	48.672602
1462.556407	158.175407	48.677607
1459.273462	163.407012	48.682612
1456.320001	157.545309	48.687617
1452.312152	144.914381	48.692621
1449.041363	142.153879	48.697626
1445.596100	161.043080	48.702631
1441.879929	172.135366	48.707636
1438.422982	141.233553	48.712641
1434.818101	157.964833	48.717645
1431.337907	149.534176	48.722650
1428.095434	149.688007	48.727655
1424.286078	146.844166	48.732660
1421.154059	151.445569	48.737665
1417.391117	167.602185	48.742669
1414.024925	158.153017	48.747674
1410.546945	141.184907	48.752679
1406.672197	150.417511	48.757684
1403.318163	149.895186	48.762689
1399.712512	146.082159	48.767693
1396.347502	156.593462	48.772698
1393.018917	168.104183	48.777703
1389.207149	157.247963	48.782708
1386.029863	143.159790	48.787713
1382.337181	142.257148	48.792717
1378.841895	152.687166	48.797722
1375.519887	169.209611	48.802727
1372.104183	149.871279	48.807732
1368.553683	138.203100	48.812737
1364.817375	148.988676	48.817741
1361.183895	148.364325	48.822746
1357.843884	144.944191	48.827751
1353.999892	152.107831	48.832756
1350.563033	148.871881	48.837761
1347.623027	161.226234	48.842765
1344.341342	139.009953	48.847770
1340.359744	134.255865	48.852775
1336.548076	142.008034	48.857780
1333.458364	159.811851	48.862785
1329.589212	150.458876	48.867789
1326.270616	142.437045	48.872794
1322.604336	152.071697	48.877799
1319.317069	154.700652	48.882804
1316.477891	148.197393	48.887809
1312.189893	152.356723	48.892813
1308.932580	165.877992	48.897818
1305.133149	153.127725	48.902823
1301.521107	147.439227	48.907828
1298.568051	148.853319	48.912833
1294.844028	173.159480	48.917837
1291.294340	159.213810	48.922842
1287.502326	148.343059	48.927847
1283.933196	151.772423	48.932852
1281.077411	163.645600	48.937857
1277.103832	148.398911	48.942861
1273.840254	153.318526	48.947866
1270.471881	169.131090	48.952871
1266.759864	162.620700	48.957876
1263.478879	147.316418	48.962881
1259.408722	146.224995	48.967885
1256.561865	156.905626	48.972890
1252.552498	157.793209	48.977895
1249.051286	151.771166	48.982900
1245.857237	138.246073	48.987905
1242.413049	155.624061	48.992909
1238.899911	156.879080	48.997914
1235.123176	158.887090	49.002919
1231.415948	150.418958	49.007924
1228.348794	134.623168	49.012929
1224.553651	157.544212	49.017933
1221.412596	136.431959	49.022938
1217.932520	145.787815	49.027943
1214.201628	142.926409	49.032948
1210.966959	143.176911	49.037953
1207.232485	165.179016	49.042957
1203.607187	153.083013	49.047962
1200.345178	141.428182	49.052967
1196.583431	139.894254	49.057972
1193.123077	142.371903	49.062977
1189.423971	150.339358	49.067981
1186.183541	156.304409	49.072986
1182.669858	144.393610	49.077991
1179.217310	136.740627	49.082996
1175.756056	137.958800	49.088001
1172.042379	139.054298	49.093005
1168.484174	135.145578	49.098010
1165.144505	147.132592	49.103015
1161.640734	149.610322	49.108020
1158.497274	153.930108	49.113025
1154.681145	150.701235	49.118029
1151.405236	138.647432	49.123034
1147.854420	152.139362	49.128039
1144.006252	144.921438	49.133044
1140.685214	141.995570	49.138049
1137.148053	153.123624	49.143053
1133.707673	147.505040	49.148058
1129.932413	142.791989	49.153063
1126.329651	138.164995	49.158068
1123.267603	151.785969	49.163073
1119.662003	156.647289	49.168077
1116.123266	145.728331	49.173082
1112.223945	158.403894	49.178087
1108.651170	146.814131	49.183092
1105.744410	156.375870	49.188097
1102.323737	158.944971	49.193101
1099.087684	141.163145	49.198106
1095.698603	149.088239	49.203111
1091.453069	159.960967	49.208116
1088.076799	145.643620	49.213121
1084.410555	142.569289	49.218125
1081.327900	140.387260	49.223130
1077.439201	145.520745	49.228135
1074.065012	159.144837	49.233140
1070.853055	160.349328	49.238145
1066.891239	146.798781	49.243149
1063.440491	137.915629	49.248154
1059.921849	168.545978	49.253159
1056.343578	149.377650	49.258164
1053.577004	135.557283	49.263169
1049.828409	150.226707	49.268173
1046.308358	158.340656	49.273178
1042.655331	149.727266	49.278183
1038.638348	132.856699	49.283188
1035.399425	137.663137	49.288193
1031.766804	159.515889	49.293197
1028.928263	147.057796	49.298202
1025.197407	138.694422	49.303207
1021.356844	137.738956	49.308212
1017.977498	146.501964	49.313217
1014.530241	157.071086	49.318221
1010.903078	139.822570	49.323226
1007.577793	138.772073	49.328231
1003.884695	152.742018	49.333236
1000.533515	146.800311	49.338241
996.822233	159.798136	49.343245
993.553876	137.614633	49.348250
990.344589	149.039300	49.353255
986.676613	157.771755	49.358260
982.814484	129.500313	49.363265
979.171849	144.877323	49.368269
975.977958	132.407608	49.373274
972.694986	144.037596	49.378279
968.815022	156.745834	49.383284
965.732947	146.952704	49.388289
961.766606	143.045591	49.393293
958.453717	140.034326	49.398298
954.830472	163.081659	49.403303
951.382509	156.842256	49.408308
948.132645	155.287970	49.413313
944.499921	145.816116	49.418317
940.818689	135.461592	49.423322
937.587123	147.901782	49.428327
934.128231	158.253762	49.433332
931.020757	136.817631	49.438337
926.924099	127.989232	49.443341
923.852819	135.867243	49.448346
919.854238	159.126105	49.453351
916.103124	150.934728	49.458356
912.769998	139.279288	49.463361
909.474254	135.930705	49.468365
905.954141	143.892112	49.473370
902.368187	147.064108	49.478375
898.824721	138.940957	49.483380
895.389952	113.738904	49.488385
891.893337	125.848394	49.493389
888.683972	141.322382	49.498394
885.481972	140.429450	49.503399
881.418060	123.082111	49.508404
878.306919	122.426817	49.513409
874.132927	136.509551	49.518413
870.817936	146.092505	49.523418
867.369815	134.412780	49.528423
863.626350	124.682967	49.533428
860.405771	131.773785	49.538433
856.590175	150.521187	49.543437
853.434630	141.911991	49.548442
850.046703	135.026664	49.553447
846.267106	125.246699	49.558452
842.907700	128.952085	49.563457
839.169681	157.975710	49.568461
835.830456	118.956348	49.573466
832.165900	131.084720	49.578471
828.889433	159.391024	49.583476
825.366747	150.758813	49.588481
821.937823	140.073170	49.593485
818.543096	123.560712	49.598490
814.803666	147.326165	49.603495
811.554056	136.714598	49.608500
808.264781	132.230162	49.613505
804.176062	149.420652	49.618509
800.593309	138.067428	49.623514
797.014193	138.481943	49.628519
793.504048	139.094794	49.633524
790.472209	133.904846	49.638529
787.029787	148.080491	49.643533
783.404837	126.288980	49.648538
779.901701	139.954677	49.653543
776.038391	143.990128	49.658548
773.004786	127.660832	49.663553
769.537201	128.356535	49.668557
766.214773	128.152280	49.673562
762.211707	125.314091	49.678567
758.627902	141.883680	49.683572
755.264826	147.609719	49.688577
751.313073	152.403394	49.693581
748.216264	131.619867	49.698586
744.786787	127.764512	49.703591
740.891764	133.240830	49.708596
737.917816	133.291751	49.713601
734.349146	126.082892	49.718605
730.858711	127.608362	49.723610
727.178784	137.496576	49.728615
723.535001	136.033011	49.733620
720.241739	108.519712	49.738625
716.623453	124.604914	49.743629
713.354193	138.048921	49.748634
710.112680	135.677763	49.753639
706.218603	123.901141	49.758644
702.899392	111.513567	49.763649
699.164961	127.763564	49.768653
695.926743	138.758468	49.773658
692.580168	125.004410	49.778663
688.261824	132.701669	49.783668
685.287866	126.597427	49.788673
681.479971	126.960610	49.793677
678.178881	112.683630	49.798682
674.716935	119.080645	49.803687
670.990274	126.555896	49.808692
667.737317	125.893544	49.813697
664.107338	136.180653	49.818701
661.125496	137.360845	49.823706
657.509417	135.291289	49.828711
653.567152	135.806796	49.833716
650.564769	120.460678	49.838721
646.685628	127.990522	49.843725
643.080369	128.415257	49.848730
639.602775	110.698826	49.853735
635.907619	133.284975	49.858740
632.803695	136.188682	49.863745
629.122522	143.255842	49.868749
625.628705	123.620635	49.873754
622.071809	115.695604	49.878759
618.157956	128.388265	49.883764
615.348319	121.599438	49.888769
611.749315	129.400379	49.893773
608.449673	125.042753	49.898778
604.802971	127.453510	49.903783
600.762864	119.720757	49.908788
597.701839	118.506475	49.913793
594.242075	113.454691	49.918797
590.536638	109.178014	49.923802
586.950643	124.485526	49.928807
583.543318	118.334740	49.933812
580.438502	112.957300	49.938817
576.722179	126.423101	49.943821
573.235312	137.920393	49.948826
569.886475	134.718373	49.953831
566.011420	128.540579	49.958836
562.703032	110.562659	49.963841
559.270624	117.028833	49.968845
555.911540	122.714440	49.973850
552.130695	120.363003	49.978855
548.391894	133.085776	49.983860
545.330313	128.033156	49.988865
541.406553	133.696725	49.993869
537.946290	130.791117	49.998874
534.340944	116.202646	50.003879
530.761044	134.769859	50.008884
527.360421	121.426334	50.013889
523.945399	127.279229	50.018893
520.480702	112.084142	50.023898
517.436090	135.565029	50.028903
513.664435	134.500820	50.033908
510.462489	107.155203	50.038913
506.717579	116.406721	50.043917
503.104975	134.626288	50.048922
499.506905	141.028121	50.053927
496.142274	129.655946	50.058932
492.646590	104.450283	50.063937
489.002778	130.688284	50.068941
485.532960	127.842881	50.073946
482.250571	108.847128	50.078951
478.292741	117.868275	50.083956
474.885203	124.901843	50.088961
471.254921	119.838739	50.093965
467.729750	129.513383	50.098970
464.709189	136.052444	50.103975
461.006176	111.987565	50.108980
457.795553	100.082238	50.113985
453.790891	126.317727	50.118989
450.819663	119.956775	50.123994
447.318164	133.301623	50.128999
443.534831	111.917047	50.134004
440.082126	95.259167	50.139009
436.324281	108.657517	50.144013
432.989857	116.787122	50.149018
429.535644	126.107361	50.154023
425.612643	123.250046	50.159028
422.491854	102.690508	50.164033
418.971581	117.342886	50.169037
415.356996	114.456135	50.174042
411.978234	116.593378	50.179047
408.296849	128.072455	50.184052
405.168729	136.226992	50.189057
401.481290	125.729542	50.194061
398.042793	108.835538	50.199066
394.342880	120.352030	50.204071
390.845382	122.813817	50.209076
387.369082	130.073343	50.214081
383.715190	132.222118	50.219085
380.265697	143.732753	50.224090
376.773069	138.129951	50.229095
373.333450	119.367592	50.234100
370.013921	110.302587	50.239105
366.276971	115.964189	50.244109
362.980269	122.443376	50.249114
359.656482	127.173570	50.254119
355.844387	130.068322	50.259124
352.011016	118.607738	50.264129
348.748424	114.780185	50.269133
345.611673	122.617462	50.274138
342.231524	128.457774	50.279143
338.517377	133.765433	50.284148
335.172471	137.616044	50.289153
331.494151	128.708899	50.294157
327.670021	117.352951	50.299162
324.542117	130.927058	50.304167
320.762830	134.410855	50.309172
317.421749	112.035187	50.314177
313.617288	102.549927	50.319181
310.285529	106.415437	50.324186
306.848119	116.733225	50.329191
303.150443	118.723846	50.334196
299.716562	123.751623	50.339201
296.380773	124.056269	50.344205
293.092054	114.401169	50.349210
289.661782	109.309970	50.354215
285.609376	110.491116	50.359220
282.461821	115.819126	50.364225
278.489862	134.833482	50.369229
275.376780	111.476720	50.374234
271.857517	110.779256	50.379239
268.242334	127.424038	50.384244
265.340385	126.527813	50.389249
261.393883	120.047051	50.394253
257.728191	110.090944	50.399258
254.119655	112.639606	50.404263
250.758725	130.320498	50.409268
247.426126	117.008838	50.414273
243.698039	125.134124	50.419277
240.506008	112.035408	50.424282
236.948286	107.381390	50.429287
233.365707	127.709193	50.434292
229.987335	136.300918	50.439297
226.204713	120.988984	50.444301
222.523478	113.988058	50.449306
219.035148	120.996322	50.454311
215.713186	133.279459	50.459316
212.166579	111.131302	50.464321
208.496110	106.664320	50.469325
205.312800	115.407494	50.474330
202.082997	127.541048	50.479335
198.165264	128.612794	50.484340
195.077398	120.281351	50.489345
191.252944	121.254825	50.494349
187.602058	127.923494	50.499354
184.352993	132.666974	50.504359
180.855528	121.614082	50.509364
177.248946	121.913125	50.514369
173.724993	124.362724	50.519373
169.794859	123.476329	50.524378
167.196732	134.048814	50.529383
163.193954	134.457227	50.534388
160.007523	107.658885	50.539393
156.203024	119.229044	50.544397
152.462111	132.714090	50.549402
149.426340	129.495102	50.554407
145.637162	126.202130	50.559412
142.368912	121.917411	50.564417
138.679836	133.069293	50.569421
134.782089	131.322796	50.574426
131.786289	113.404505	50.579431
128.110706	112.450033	50.584436
124.875159	126.239852	50.589441
121.302233	141.582297	50.594445
117.426833	143.972711	50.599450
114.172083	111.430052	50.604455
110.481123	111.665638	50.609460
107.261190	123.396793	50.614465
103.814101	133.333036	50.619469
100.261451	129.490511	50.624474
96.543040	126.723599	50.629479
92.928141	124.768314	50.634484
89.704418	121.339424	50.639489
86.315018	122.049301	50.644493
82.572418	133.394128	50.649498
79.277848	135.689865	50.654503
75.480751	135.910555	50.659508
72.299678	120.440344	50.664513
68.776082	113.195560	50.669517
64.895058	124.649875	50.674522
61.587285	132.458196	50.679527
57.698875	130.436066	50.684532
54.789964	121.902992	50.689537
51.475291	112.673554	50.694541
47.805775	123.059307	50.699546
44.048502	117.038982	50.704551
40.307665	121.057753	50.709556
36.928771	128.114312	50.714561
33.593714	133.691036	50.719565
30.303415	127.129020	50.724570
27.006396	125.417379	50.729575
23.146660	132.578070	50.734580
19.521297	108.615857	50.739585
15.877742	107.226161	50.744589
12.692733	125.933178	50.749594
9.413710	122.067983	50.754599
5.523376	122.228166	50.759604
2.126625	119.071872	50.764609