Wed Jun 15 16:35:57 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.670219	118.079757	0.000000
0.187831	113.804487	0.005005
0.393302	117.262267	0.010010
0.399928	118.228351	0.015014
0.100564	93.780364	0.020019
-0.243532	80.251735	0.025024
-0.371139	92.629876	0.030029
-0.542279	94.305303	0.035034
-0.536089	73.252861	0.040038
-0.888317	32.121134	0.045043
-1.008092	37.423065	0.050048
-1.745290	52.218803	0.055053
-1.921586	29.447587	0.060058
-1.925211	14.324176	0.065062
-2.367102	4.919183	0.070067
-2.640024	11.326088	0.075072
-2.786784	22.381342	0.080077
-3.117297	6.169247	0.085082
-3.736139	-8.543220	0.090086
-4.124159	-9.169271	0.095091
-3.983903	-0.179256	0.100096
-4.370546	7.011239	0.105101
-5.320061	2.070196	0.110106
-5.676376	2.281635	0.115110
-5.692289	-14.666335	0.120115
-5.556832	-1.281564	0.125120
-5.765350	10.401113	0.130125
-5.675102	-5.454944	0.135130
-6.009588	-1.902931	0.140134
-6.515892	1.659720	0.145139
-6.473763	-12.837032	0.150144
-7.166570	-1.382798	0.155149
-6.951823	0.143619	0.160154
-7.066049	7.266408	0.165158
-7.977494	-2.312925	0.170163
-8.641978	-14.277865	0.175168
-8.867478	-0.176169	0.180173
-8.877539	-5.228066	0.185178
-9.083186	3.387933	0.190182
-8.969300	6.651989	0.195187
-8.730509	-7.813837	0.200192
-9.238778	1.934311	0.205197
-9.179159	-2.651459	0.210202
-10.239279	3.205171	0.215206
-10.296579	11.275909	0.220211
-10.174564	7.971194	0.225216
-11.077219	12.249717	0.230221
-11.504283	-15.113275	0.235226
-11.895495	-7.999962	0.240230
-12.198574	10.265171	0.245235
-11.930643	12.008699	0.250240
-12.077059	11.694000	0.255245
-11.612259	-2.179131	0.260250
-12.016697	2.933277	0.265254
-12.993390	18.476144	0.270259
-13.337404	-1.523576	0.275264
-13.515396	-9.887462	0.280269
-13.617398	-8.183520	0.285274
-13.768455	10.035282	0.290278
-13.750523	1.215625	0.295283
-13.887128	6.801071	0.300288
-15.069477	10.093685	0.305293
-15.059960	-5.138117	0.310298
-15.483247	-8.504037	0.315302
-15.275758	10.071600	0.320307
-15.442239	10.780902	0.325312
-15.638920	3.268449	0.330317
-15.597005	-10.267559	0.335322
-16.437051	-4.990145	0.340326
-16.953916	4.720263	0.345331
-16.831321	-0.428725	0.350336
-16.999152	-7.892868	0.355341
-17.077777	-9.667971	0.360346
-17.610083	7.152497	0.365350
-18.193097	16.807356	0.370355
-18.185274	1.267264	0.375360
-18.493516	-16.063869	0.380365
-18.393180	-6.332058	0.385370
-18.402947	1.904830	0.390374
-19.039436	-12.811520	0.395379
-19.462383	-7.733148	0.400384
-20.090850	9.157862	0.405389
-19.788678	-2.991787	0.410394
-20.202805	-3.290162	0.415398
-20.223076	-4.050080	0.420403
-20.103621	1.942576	0.425408
-21.021984	2.953593	0.430413
-21.479557	-5.928443	0.435418
-21.598084	-11.437982	0.440422
-21.825590	6.048477	0.445427
-22.047622	-2.963535	0.450432
-22.148957	-4.178228	0.455437
-21.962998	-13.357388	0.460442
-22.028566	-2.015194	0.465446
-22.839657	16.607539	0.470451
-23.193399	-10.658372	0.475456
-23.569935	-16.159601	0.480461
-23.403851	6.687808	0.485466
-23.575226	15.142486	0.490470
-24.294707	1.326959	0.495475
-24.477659	-17.389638	0.500480
-25.161844	4.107451	0.505485
-25.377678	9.663868	0.510490
-25.255234	4.735870	0.515494
-25.393531	-4.030048	0.520499
-25.184485	-16.256924	0.525504
-25.279964	1.442981	0.530509
-25.677193	17.719301	0.535514
-26.225620	-5.826578	0.540518
-26.876356	-20.308944	0.545523
-26.417073	-16.302649	0.550528
-27.531933	-12.934974	0.555533
-27.627241	12.172892	0.560538
-28.131843	-13.251919	0.565542
-28.271613	-14.991071	0.570547
-28.291305	-2.255300	0.575552
-28.365826	7.644505	0.580557
-28.219494	1.649950	0.585562
-28.149374	-18.218327	0.590566
-28.651478	4.631680	0.595571
-29.263171	17.556941	0.600576
-29.636193	8.347430	0.605581
-29.644843	1.478346	0.610586
-30.085608	0.379919	0.615590
-30.952581	4.088983	0.620595
-31.120870	-6.491986	0.625600
-31.480737	9.083785	0.630605
-30.908066	7.659259	0.635610
-31.205764	-4.853212	0.640614
-31.587448	4.178370	0.645619
-31.304733	-9.499036	0.650624
-31.885178	7.830505	0.655629
-32.560676	-9.658737	0.660634
-32.570712	-1.333421	0.665638
-33.172986	3.090385	0.670643
-32.933428	-16.738914	0.675648
-33.163605	-2.209413	0.680653
-33.244097	4.924666	0.685658
-34.132544	-3.195448	0.690662
-34.465780	-1.772904	0.695667
-34.312192	-13.340937	0.700672
-34.855605	1.546526	0.705677
-34.721033	12.722680	0.710682
-34.952026	-1.528002	0.715686
-35.885557	14.604633	0.720691
-36.118342	7.861960	0.725696
-36.482097	-1.633175	0.730701
-36.491477	-15.697824	0.735706
-36.259047	-4.933029	0.740710
-36.576228	16.241719	0.745715
-36.077093	-4.726839	0.750720
-36.498188	-2.709740	0.755725
-37.269655	-1.864651	0.760730
-37.602971	-20.431309	0.765734
-38.352676	-7.522622	0.770739
-37.817162	3.883992	0.775744
-38.113638	4.229763	0.780749
-39.007451	-1.470478	0.785754
-39.348737	2.264266	0.790758
-39.477379	12.100513	0.795763
-39.155756	11.305302	0.800768
-39.592002	0.203273	0.805773
-39.327361	-7.825170	0.810778
-39.567242	-5.724082	0.815782
-40.561438	12.306846	0.820787
-40.912480	-2.383781	0.825792
-40.887387	-11.836238	0.830797
-41.321175	-23.780791	0.835802
-41.488836	-7.194317	0.840806
-41.589107	15.862941	0.845811
-42.146985	-10.847788	0.850816
-42.888983	-17.249424	0.855821
-42.984637	-19.389066	0.860826
-42.543324	-1.636322	0.865830
-42.993107	13.854187	0.870835
-43.148486	-7.965924	0.875840
-43.213186	-7.828224	0.880845
-43.266078	-0.032951	0.885850
-43.377027	12.699070	0.890854
-44.255160	11.706561	0.895859
-44.303516	-2.699876	0.900864
-44.620832	-10.038693	0.905869
-44.556762	-10.529930	0.910874
-45.054462	5.400655	0.915878
-46.073836	6.383584	0.920883
-46.160565	-15.983406	0.925888
-46.382102	1.448986	0.930893
-46.568916	11.935350	0.935898
-46.065767	-4.300756	0.940902
-46.272986	-11.118866	0.945907
-46.221370	-14.134551	0.950912
-47.295219	-0.537211	0.955917
-47.730150	-12.641191	0.960922
-47.764210	3.665060	0.965926
-47.610265	10.059916	0.970931
-47.524242	-17.627066	0.975936
-48.489927	-18.134960	0.980941
-48.967378	1.618926	0.985946
-48.886192	1.378281	0.990950
-49.504783	4.426904	0.995955
-49.344088	-14.736525	1.000960
-49.575436	4.154780	1.005965
-49.671788	7.549067	1.010970
-50.386523	3.317263	1.015974
-50.703478	-4.232322	1.020979
-51.014842	-22.806350	1.025984
-51.273689	9.651570	1.030989
-51.323160	8.115401	1.035994
-51.009279	-7.486994	1.040998
-51.248321	-12.381191	1.046003
-51.694430	-10.725341	1.051008
-52.505748	9.413798	1.056013
-52.744454	14.231688	1.061018
-52.424493	-5.478527	1.066022
-52.868898	-11.828627	1.071027
-52.702734	3.826028	1.076032
-53.782698	13.659980	1.081037
-54.281167	-5.608291	1.086042
-54.621425	-15.837175	1.091046
-54.911317	7.147530	1.096051
-53.724014	-20.706251	1.101056
-54.501435	0.135743	1.106061
-54.925514	5.466741	1.111066
-54.391816	-7.279990	1.116070
-55.483451	4.926138	1.121075
-55.981561	-4.659935	1.126080
-56.224395	-1.880467	1.131085
-56.601456	9.810131	1.136090
-56.294891	-6.217303	1.141094
-56.533547	2.365971	1.146099
-56.210692	2.208892	1.151104
-57.022841	-13.082030	1.156109
-57.537203	4.518216	1.161114
-57.723488	4.960404	1.166118
-57.824712	1.373860	1.171123
-57.997585	-6.689013	1.176128
-58.459036	0.038468	1.181133
-58.757206	13.543341	1.186138
-58.936283	-8.109394	1.191142
-59.060009	3.560345	1.196147
-59.033745	1.589655	1.201152
-60.024193	-20.369820	1.206157
-60.427859	-8.907346	1.211162
-60.560612	-1.121565	1.216166
-60.892046	-4.265616	1.221171
-60.686658	-13.888336	1.226176
-60.486053	-5.406957	1.231181
-60.867450	-0.862117	1.236186
-61.077190	-12.133750	1.241190
-61.821447	8.642404	1.246195
-61.901361	15.238773	1.251200
-62.371224	6.309642	1.256205
-62.263537	-7.272745	1.261210
-62.231104	0.249581	1.266214
-63.297879	10.307743	1.271219
-63.721166	-9.475445	1.276224
-63.661428	-12.034067	1.281229
-64.065381	3.068183	1.286234
-63.952353	-14.775775	1.291238
-64.099651	-5.063120	1.296243
-63.833160	-15.632378	1.301248
-64.470165	-11.740255	1.306253
-65.154936	4.179614	1.311258
-65.179788	18.670561	1.316262
-65.554369	8.434807	1.321267
-65.540247	6.022417	1.326272
-66.002507	6.981542	1.331277
-66.467890	-4.886281	1.336282
-66.792527	2.762430	1.341286
-67.416432	8.215036	1.346291
-67.133681	-11.033770	1.351296
-67.445269	-11.341097	1.356301
-67.637227	-2.605146	1.361306
-67.317160	4.622736	1.366310
-67.549861	-1.221480	1.371315
-67.536278	-4.733381	1.376320
-68.184194	1.024159	1.381325
-68.893790	2.535636	1.386330
-68.852938	-0.147317	1.391334
-68.886747	5.885166	1.396339
-69.468410	-0.609161	1.401344
-70.068351	3.032496	1.406349
-70.308548	8.552296	1.411354
-70.514965	8.549074	1.416358
-70.544263	8.703414	1.421363
-70.145922	-4.013551	1.426368
-70.461907	8.098525	1.431373
-71.133271	12.042992	1.436378
-71.628226	-2.251360	1.441382
-71.747454	12.832155	1.446387
-71.783204	-6.610239	1.451392
-71.936534	5.546768	1.456397
-73.025601	-0.973397	1.461402
-73.495918	-5.655164	1.466406
-73.388316	6.424886	1.471411
-73.117050	-3.099330	1.476416
-73.965498	3.528358	1.481421
-73.829173	-3.647890	1.486426
-73.858140	-0.799005	1.491430
-73.970818	5.000983	1.496435
-74.083257	-1.372907	1.501440
-74.391938	-13.407189	1.506445
-75.085747	8.285328	1.511450
-75.281474	0.075499	1.516454
-75.844900	-13.264376	1.521459
-75.723483	-19.245827	1.526464
-75.504109	-3.471344	1.531469
-76.322768	15.510225	1.536474
-76.544062	1.341893	1.541478
-76.999175	-3.692973	1.546483
-77.339611	0.145899	1.551488
-77.124815	4.336326	1.556493
-77.314183	6.609588	1.561498
-77.456265	0.135244	1.566502
-78.281789	-6.865570	1.571507
-78.417258	-7.714564	1.576512
-78.512091	-4.681376	1.581517
-78.660710	0.346040	1.586522
-78.647153	6.131085	1.591526
-79.001260	4.509822	1.596531
-79.666736	-14.462908	1.601536
-80.146327	0.363004	1.606541
-80.261999	18.049090	1.611546
-80.146046	-2.964450	1.616550
-80.426842	-13.172874	1.621555
-80.413537	-3.175534	1.626560
-80.947293	-1.420066	1.631565
-81.504319	19.632044	1.636570
-81.453872	-5.575039	1.641574
-81.670132	-14.270056	1.646579
-82.105248	-1.371332	1.651584
-81.931232	15.110652	1.656589
-82.512533	12.605883	1.661594
-82.799419	-16.145206	1.666598
-83.394356	-6.285576	1.671603
-83.497533	-5.931205	1.676608
-83.538758	13.895213	1.681613
-83.741425	-2.301089	1.686618
-83.508302	-19.506033	1.691622
-84.368626	3.916515	1.696627
-84.333509	15.985270	1.701632
-84.833235	7.383254	1.706637
-85.006233	-9.068603	1.711642
-84.688515	-6.633420	1.716646
-85.665125	11.969703	1.721651
-86.391553	9.086545	1.726656
-86.467531	-3.352077	1.731661
-86.488207	-14.659093	1.736666
-86.725081	-9.990172	1.741670
-86.925303	16.407452	1.746675
-86.970653	-7.637928	1.751680
-86.845294	1.147286	1.756685
-87.335278	4.294215	1.761690
-87.100401	-2.806086	1.766694
-87.976096	-8.742310	1.771699
-88.471053	4.817467	1.776704
-88.345725	6.305588	1.781709
-88.633139	-15.882427	1.786714
-89.349763	-18.914675	1.791718
-90.050658	14.243978	1.796723
-89.909745	17.018427	1.801728
-89.635959	-3.706219	1.806733
-90.091592	5.829627	1.811738
-90.213899	-8.563195	1.816742
-90.367224	13.507583	1.821747
-90.321792	7.070509	1.826752
-90.696669	-17.315273	1.831757
-91.472514	1.712274	1.836762
-91.552280	10.979046	1.841766
-92.003059	11.251971	1.846771
-92.022185	-1.124331	1.851776
-92.003916	-3.758766	1.856781
-92.659097	9.636616	1.861786
-93.012719	20.094914	1.866790
-93.696774	14.353994	1.871795
-93.879503	-11.601534	1.876800
-93.660026	2.383507	1.881805
-94.320699	3.358655	1.886810
-93.550603	6.720623	1.891814
-94.224511	9.232192	1.896819
-94.120805	7.719145	1.901824
-94.041962	-5.604559	1.906829
-95.196293	-1.771648	1.911834
-95.147480	-5.351319	1.916838
-95.623575	11.267004	1.921843
-95.447693	-3.513950	1.926848
-96.574984	-16.692663	1.931853
-97.120005	9.551322	1.936858
-96.050328	2.406668	1.941862
-96.603933	-13.573788	1.946867
-96.970777	-19.463200	1.951872
-96.703386	-6.892670	1.956877
-97.326252	11.200390	1.961882
-97.782151	-0.218976	1.966886
-98.076082	3.453885	1.971891
-98.322442	-5.890771	1.976896
-98.218382	1.633328	1.981901
-98.816948	-2.080542	1.986906
-99.341163	-18.843175	1.991910
-99.984160	-8.861274	1.996915
-99.625811	-1.502804	2.006912
-98.819822	-7.128108	2.016909
-98.866787	-0.886564	2.026906
-98.652506	-11.374293	2.036902
-97.753583	-5.969514	2.046899
-97.280821	1.051970	2.056896
-96.855459	-1.935550	2.066893
-96.033308	2.173788	2.076890
-95.779295	0.535857	2.086886
-95.637229	-10.809822	2.096883
-94.779949	-9.411747	2.106880
-94.383252	-6.677029	2.116877
-93.269146	6.126642	2.126874
-92.990308	-6.908911	2.136870
-92.595019	2.760706	2.146867
-92.461799	-10.521511	2.156864
-92.031114	-5.571429	2.166861
-91.326266	-7.817038	2.176858
-91.155226	-2.642206	2.186854
-89.987258	2.106026	2.196851
-89.777488	-19.432918	2.206848
-89.313680	7.583614	2.216845
-88.710392	-15.301244	2.226842
-88.054977	-4.002910	2.236838
-87.914675	-3.715655	2.246835
-86.742965	-17.709380	2.256832
-86.555861	2.452491	2.266829
-86.614029	-8.859999	2.276826
-86.009466	9.173301	2.286822
-85.272999	-8.655914	2.296819
-84.857080	-19.347443	2.306816
-83.649169	-14.954185	2.316813
-83.707920	2.106095	2.326810
-83.649175	-1.898435	2.336806
-82.824616	-7.413318	2.346803
-82.382420	-10.276696	2.356800
-81.775334	-6.273652	2.366797
-81.096191	-7.868352	2.376794
-80.719972	-11.779165	2.386790
-80.313440	-12.385937	2.396787
-79.253450	-3.442015	2.406784
-78.989066	-7.330099	2.416781
-79.139679	-4.213453	2.426778
-78.529048	-3.325661	2.436774
-77.719475	-17.105059	2.446771
-77.349687	3.125593	2.456768
-76.153456	-11.786125	2.466765
-75.915248	-9.254364	2.476762
-75.817609	-22.953633	2.486758
-75.606117	-15.108284	2.496755
-74.424483	-9.483342	2.506752
-74.141635	-17.678155	2.516749
-73.988295	1.874938	2.526746
-73.024424	-8.125970	2.536742
-72.664972	-11.221812	2.546739
-72.411886	-12.362865	2.556736
-71.633088	-6.004539	2.566733
-71.140707	-5.898144	2.576730
-70.886774	-2.243377	2.586726
-69.777826	-12.718459	2.596723
-69.381915	-2.948395	2.606720
-69.483849	-10.940354	2.616717
-68.903642	1.570198	2.626714
-67.887529	-1.862725	2.636710
-67.903422	-4.027346	2.646707
-67.562516	-2.343818	2.656704
-66.603135	-13.479065	2.666701
-66.262795	6.647911	2.676698
-65.224411	-2.048588	2.686694
-64.851231	3.814074	2.696691
-64.990383	-18.446620	2.706688
-64.544216	5.353271	2.716685
-63.757422	-5.144729	2.726682
-63.234111	-5.508265	2.736678
-62.106559	6.738098	2.746675
-62.079206	0.753046	2.756672
-61.520243	-15.894557	2.766669
-61.562338	9.808964	2.776666
-60.694499	-1.331411	2.786662
-60.250699	-1.423222	2.796659
-59.826311	-7.588856	2.806656
-58.915521	-15.693162	2.816653
-58.708995	-4.126847	2.826650
-58.493957	-11.212412	2.836646
-57.525833	-11.857076	2.846643
-57.128285	-3.564807	2.856640
-56.735039	-0.901222	2.866637
-55.623263	-16.799437	2.876634
-55.466173	-2.581623	2.886630
-55.537223	-1.747406	2.896627
-55.018204	-18.590096	2.906624
-54.395810	-5.018106	2.916621
-53.414744	4.176714	2.926618
-52.723619	0.587116	2.936614
-52.484604	-8.604574	2.946611
-52.374624	-4.214168	2.956608
-51.752367	-13.121710	2.966605
-50.967457	-6.926278	2.976602
-50.526596	-14.995296	2.986598
-50.341824	8.445407	2.996595
-49.421298	-23.606535	3.006592
-49.084679	-0.663265	3.016589
-48.718996	-4.169349	3.026586
-48.139720	-0.689637	3.036582
-47.211761	-14.569793	3.046579
-47.118446	-23.933062	3.056576
-47.009374	-3.773703	3.066573
-45.979941	-15.037668	3.076570
-45.583036	8.340225	3.086566
-45.385506	-3.207828	3.096563
-44.283449	-6.505805	3.106560
-43.961240	-8.077073	3.116557
-44.079720	0.023325	3.126554
-43.344441	-20.208802	3.136550
-42.730163	-0.988290	3.146547
-41.746538	-5.159494	3.156544
-41.301183	-4.972628	3.166541
-40.739686	-11.608454	3.176538
-40.610696	5.877334	3.186534
-40.632055	-9.434392	3.196531
-39.399266	0.593552	3.206528
-39.026715	-7.531248	3.216525
-39.024271	-5.509199	3.226522
-38.103870	0.452477	3.236518
-37.719147	-0.211731	3.246515
-36.898166	1.632084	3.256512
-36.004763	-2.004669	3.266509
-35.988953	-0.729271	3.276506
-36.090804	4.871036	3.286502
-35.293870	-9.279836	3.296499
-34.483673	-3.548756	3.306496
-34.391869	-9.334073	3.316493
-33.255864	1.271583	3.326490
-32.925779	0.269814	3.336486
-32.701017	0.245613	3.346483
-32.307064	-7.349751	3.356480
-31.362412	5.413000	3.366477
-31.168266	-8.979218	3.376474
-30.747476	0.648364	3.386470
-29.563694	-4.817231	3.396467
-29.551392	2.414984	3.406464
-29.416346	-15.801389	3.416461
-28.725202	-4.242855	3.426458
-28.216622	-9.303416	3.436454
-27.613767	-10.743668	3.446451
-26.513049	-2.245107	3.456448
-26.607410	-14.079259	3.466445
-26.567609	6.170682	3.476442
-25.512093	-9.249373	3.486438
-24.800951	4.972307	3.496435
-24.840088	2.521531	3.506432
-24.023911	-0.093011	3.516429
-22.995908	-15.374480	3.526426
-22.960002	5.982052	3.536422
-22.826868	-7.731894	3.546419
-22.390893	-3.491760	3.556416
-21.351419	5.752877	3.566413
-21.108604	13.574699	3.576410
-20.382496	8.345929	3.586406
-19.663806	-8.983531	3.596403
-19.772974	7.689715	3.606400
-19.425818	2.608514	3.616397
-18.309110	9.027566	3.626394
-18.132304	-10.409820	3.636390
-17.766698	4.530339	3.646387
-16.787702	-7.118606	3.656384
-16.347654	4.086246	3.666381
-16.386045	0.183796	3.676378
-15.604966	1.239786	3.686374
-14.866497	-3.494002	3.696371
-14.591349	-0.193474	3.706368
-13.626019	1.856332	3.716365
-13.269623	11.256920	3.726362
-13.135665	-5.293500	3.736358
-13.148154	-1.751451	3.746355
-12.124232	4.280636	3.756352
-11.649137	-12.013835	3.766349
-10.586054	14.010216	3.776346
-10.119094	-3.383634	3.786342
-9.969110	-2.957029	3.796339
-9.955361	-4.310596	3.806336
-9.176904	5.241293	3.816333
-8.386224	-6.598669	3.826330
-8.388046	-7.387059	3.836326
-7.308437	4.183050	3.846323
-6.962816	-11.006103	3.856320
-6.978844	6.532005	3.866317
-6.097089	-8.642137	3.876314
-5.340726	-9.082109	3.886310
-5.163262	-13.506481	3.896307
-4.059425	-4.712510	3.906304
-4.074619	-10.185905	3.916301
-4.024052	-9.756305	3.926298
-3.354383	22.346695	3.936294
-2.916701	12.562221	3.946291
-2.284842	39.914058	3.956288
-1.891531	40.114762	3.966285
-1.543790	62.666746	3.976282
-0.909398	89.066188	3.986278
-0.453203	86.104377	3.996275
-0.217051	126.456607	4.006272
0.000000	129.972554	4.011277
0.284009	141.561806	4.016282
0.411342	158.320290	4.021286
0.960000	164.693196	4.026291
0.998192	170.856690	4.031296
0.773279	177.662550	4.036301
1.060275	172.590704	4.041306
0.792946	190.000724	4.046310
1.059896	192.302678	4.051315
1.176380	186.848832	4.056320
1.204442	201.015351	4.061325
1.592068	207.339223	4.066330
1.060716	206.336934	4.071334
1.319260	204.126495	4.076339
1.363215	208.586407	4.081344
1.358674	206.030380	4.086349
1.599252	198.780675	4.091354
1.488315	196.119909	4.096358
1.478347	221.590262	4.101363
1.348632	202.981489	4.106368
1.521544	214.886478	4.111373
1.637582	213.622331	4.116378
1.193171	206.424854	4.121382
1.499784	207.087651	4.126387
1.240584	232.622686	4.131392
1.377879	211.608958	4.136397
1.533149	199.774234	4.141402
1.466346	212.656670	4.146406
1.610077	223.096451	4.151411
1.580807	217.442159	4.156416
1.467226	201.538088	4.161421
1.895992	195.999192	4.166426
1.466383	216.203373	4.171430
1.522744	221.990309	4.176435
1.443728	221.434422	4.181440
1.886312	202.943758	4.186445
1.975159	197.521702	4.191450
1.418334	217.543498	4.196454
1.477408	222.093940	4.201459
1.700585	207.031308	4.206464
1.282066	199.253755	4.211469
1.549202	215.330140	4.216474
1.724851	216.698597	4.221478
1.540616	217.450300	4.226483
1.935719	226.501027	4.231488
1.304027	228.994795	4.236493
1.543613	206.318640	4.241498
1.498376	216.232091	4.246502
1.707590	225.838535	4.251507
1.771402	207.558034	4.256512
1.510075	201.498383	4.261517
1.656276	208.197354	4.266522
1.453740	218.788363	4.271526
1.548901	211.464727	4.276531
1.683759	216.504164	4.281536
1.736078	227.775950	4.286541
2.193105	242.664742	4.291546
2.026451	254.469816	4.296550
1.568127	230.976936	4.301555
1.881655	232.982855	4.306560
1.941544	240.131531	4.311565
2.288862	248.116788	4.316570
1.729120	255.629380	4.321574
1.959527	239.834053	4.326579
1.910467	230.303335	4.331584
1.834489	236.005114	4.336589
2.092548	231.976587	4.341594
2.140182	221.598697	4.346598
2.338661	243.638817	4.351603
2.090652	222.189494	4.356608
1.791669	224.310637	4.361613
1.894773	218.687345	4.366618
1.943643	230.075119	4.371622
2.018178	253.364680	4.376627
2.132779	257.153673	4.381632
2.120309	245.208035	4.386637
2.464463	224.449240	4.391642
2.080882	234.964725	4.396646
1.926904	244.492106	4.401651
1.972670	239.820263	4.406656
2.347790	233.472335	4.411661
2.122632	245.438000	4.416666
2.204874	247.786171	4.421670
2.286915	237.343495	4.426675
2.421570	233.107979	4.431680
2.253908	229.829383	4.436685
2.015740	222.217828	4.441690
1.939790	246.722621	4.446694
2.322676	241.066107	4.451699
2.589833	229.322961	4.456704
2.109240	229.667791	4.461709
2.552667	250.150646	4.466714
2.161754	254.205377	4.471718
1.868637	241.689277	4.476723
2.176116	229.542512	4.481728
2.064873	244.914180	4.486733
2.588402	244.010228	4.491738
2.282732	246.041132	4.496742
1.792514	259.373467	4.501747
2.435116	248.629215	4.506752
2.166030	252.406935	4.511757
2.370675	242.105283	4.516762
2.278080	241.679288	4.521766
2.310742	253.987177	4.526771
2.765393	242.451862	4.531776
2.033801	245.216355	4.536781
2.590224	231.846361	4.541786
2.567479	251.121671	4.546790
2.548465	234.079235	4.551795
2.390421	248.170507	4.556800
2.270043	263.647282	4.561805
2.701747	255.576098	4.566810
2.424414	244.697693	4.571814
2.460296	256.278121	4.576819
2.620017	280.505789	4.581824
2.340431	294.121584	4.586829
2.548012	272.984191	4.591834
2.780970	264.825989	4.596838
2.724858	275.881836	4.601843
2.579662	293.185449	4.606848
2.588520	297.479245	4.611853
2.630319	267.194256	4.616858
2.556976	273.374053	4.621862
2.658822	287.226105	4.626867
2.810249	295.909135	4.631872
2.582280	295.523463	4.636877
2.615360	274.296233	4.641882
2.274153	268.520739	4.646886
2.458794	270.322947	4.651891
2.904688	292.818843	4.656896
2.875236	292.550211	4.661901
2.697281	279.312483	4.666906
2.291447	274.350853	4.671910
2.186886	269.375446	4.676915
2.512367	282.978150	4.681920
2.752768	295.166117	4.686925
2.979712	307.299003	4.691930
2.918623	308.007770	4.696934
3.070205	304.638818	4.701939
3.306312	293.307478	4.706944
2.913468	297.091160	4.711949
2.900668	276.702218	4.716954
2.658143	286.551446	4.721958
2.739798	288.831753	4.726963
3.109525	314.933500	4.731968
2.977105	310.963463	4.736973
3.072114	291.413144	4.741978
2.876562	299.725385	4.746982
3.394306	317.494490	4.751987
3.263122	307.497770	4.756992
2.961766	288.615001	4.761997
3.193919	267.621329	4.767002
2.841217	270.956037	4.772006
2.876429	280.997104	4.777011
2.825703	301.461660	4.782016
3.002581	313.108896	4.787021
3.153857	311.801332	4.792026
3.011604	312.188012	4.797030
2.587365	314.349103	4.802035
3.365076	306.206903	4.807040
2.854142	305.563763	4.812045
3.180969	316.490461	4.817050
3.069403	318.934298	4.822054
3.019234	309.166862	4.827059
3.012523	300.954137	4.832064
2.922335	314.450164	4.837069
3.005144	306.037284	4.842074
2.855194	318.406179	4.847078
2.901809	344.389824	4.852083
3.519479	350.664890	4.857088
3.452108	351.309097	4.862093
3.596061	348.959441	4.867098
3.359324	332.468408	4.872102
3.295968	320.960729	4.877107
3.445619	325.629409	4.882112
3.021637	329.634973	4.887117
3.417614	335.132035	4.892122
3.496150	343.735593	4.897126
3.300833	349.136825	4.902131
3.517762	342.265329	4.907136
3.352461	359.364785	4.912141
3.567755	327.820768	4.917146
3.392553	315.202258	4.922150
3.311870	342.725418	4.927155
3.455186	349.324110	4.932160
3.309187	346.761841	4.937165
3.600588	352.271456	4.942170
3.598225	340.345183	4.947174
3.363027	328.870039	4.952179
3.761812	346.404226	4.957184
3.621118	366.468626	4.962189
3.714692	341.745582	4.967194
3.595551	313.182260	4.972198
3.209493	316.585427	4.977203
3.334998	322.061579	4.982208
3.535310	348.993189	4.987213
3.443473	340.391435	4.992218
3.443044	325.215793	4.997222
3.515383	335.542659	5.002227
3.459455	357.180676	5.007232
3.325151	349.674809	5.012237
3.601730	330.047479	5.017242
3.341107	337.289710	5.022246
3.514028	350.780960	5.027251
3.436376	355.823107	5.032256
3.505937	341.930043	5.037261
4.129473	347.626852	5.042266
3.837668	363.463020	5.047270
3.580387	358.933554	5.052275
3.759626	355.186638	5.057280
3.677266	355.542903	5.062285
4.070844	355.093484	5.067290
3.811210	357.002758	5.072294
3.733151	359.786430	5.077299
3.643258	342.807672	5.082304
3.737569	355.300777	5.087309
3.942645	375.974022	5.092314
3.851244	372.459355	5.097318
3.880096	372.971948	5.102323
4.099655	390.866472	5.107328
3.962195	382.391203	5.112333
4.307395	362.609354	5.117338
4.008425	360.551888	5.122342
3.907930	359.637705	5.127347
4.043603	358.332913	5.132352
3.711578	361.640548	5.137357
3.933667	341.202248	5.142362
3.741788	348.101568	5.147366
3.977862	376.430089	5.152371
3.977489	374.584695	5.157376
4.062452	364.187518	5.162381
3.870989	382.595645	5.167386
4.063742	381.690118	5.172390
4.253623	384.180234	5.177395
4.157400	367.848243	5.182400
4.207820	384.554678	5.187405
4.102138	379.678166	5.192410
4.418285	368.778248	5.197414
3.902156	368.015218	5.202419
4.200348	375.695355	5.207424
3.871704	381.865199	5.212429
4.202539	380.972564	5.217434
4.262218	370.551840	5.222438
4.399264	366.210043	5.227443
4.197632	360.094888	5.232448
4.085664	389.021044	5.237453
4.283414	369.047021	5.242458
4.349468	368.453147	5.247462
4.487012	372.620638	5.252467
4.364594	356.048736	5.257472
3.921626	349.527973	5.262477
4.179103	367.788106	5.267482
4.129307	389.078407	5.272486
3.983935	375.024423	5.277491
4.240271	355.084635	5.282496
4.025071	363.458064	5.287501
4.318294	370.999629	5.292506
4.214775	379.137487	5.297510
3.700073	364.715032	5.302515
4.282276	352.541218	5.307520
4.393195	378.201580	5.312525
4.191128	396.064868	5.317530
4.530021	401.490299	5.322534
4.175521	382.309794	5.327539
4.504513	396.987679	5.332544
4.341185	413.653014	5.337549
4.144195	396.031839	5.342554
4.644444	414.439736	5.347558
4.802715	410.201650	5.352563
4.821403	399.601137	5.357568
4.520115	413.832538	5.362573
4.790512	408.366102	5.367578
4.694224	402.671914	5.372582
4.453802	384.415533	5.377587
4.715952	391.444835	5.382592
4.463977	391.969801	5.387597
4.454231	384.203817	5.392602
4.560648	408.061194	5.397606
4.414100	403.773452	5.402611
4.659862	394.105130	5.407616
4.265335	396.920488	5.412621
4.477192	408.598122	5.417626
4.322141	404.736367	5.422630
4.460695	400.344790	5.427635
4.558299	410.084225	5.432640
4.401640	404.186045	5.437645
4.453479	397.660341	5.442650
4.886866	395.991562	5.447654
4.803392	428.061930	5.452659
4.930203	417.506179	5.457664
4.647213	398.582851	5.462669
4.603436	393.823558	5.467674
4.838057	432.342477	5.472678
4.877909	434.713762	5.477683
5.037690	418.925482	5.482688
4.739342	405.062479	5.487693
5.015495	421.860979	5.492698
4.692833	433.018795	5.497702
4.729129	424.807577	5.502707
5.428078	410.799691	5.507712
4.843986	421.968837	5.512717
4.750752	410.689861	5.517722
4.994826	416.038434	5.522726
4.876467	429.092046	5.527731
5.029530	426.038103	5.532736
4.741306	439.320641	5.537741
4.837307	422.102434	5.542746
5.155513	431.403338	5.547750
5.259548	436.830303	5.552755
5.130898	427.783069	5.557760
4.994717	427.910290	5.562765
4.839065	427.833764	5.567770
5.129255	442.208743	5.572774
5.382811	436.067266	5.577779
5.013981	410.166211	5.582784
4.810573	411.852725	5.587789
5.072525	431.958101	5.592794
5.019582	440.129164	5.597798
4.957311	441.351204	5.602803
5.307331	424.489754	5.607808
4.905664	431.732549	5.612813
5.116267	447.866563	5.617818
5.417066	434.350316	5.622822
5.053892	426.391851	5.627827
5.200394	424.333762	5.632832
5.111372	437.658945	5.637837
4.969928	437.455873	5.642842
5.107865	441.665737	5.647846
5.047733	423.036319	5.652851
5.592924	435.644485	5.657856
5.049338	448.366686	5.662861
5.386685	436.972638	5.667866
5.331732	444.035919	5.672870
4.907227	441.161465	5.677875
5.263798	420.762392	5.682880
5.225933	435.156259	5.687885
5.182254	458.358733	5.692890
5.276553	441.803999	5.697894
5.144409	437.731486	5.702899
5.410290	445.496310	5.707904
5.076698	478.963645	5.712909
5.559973	482.207603	5.717914
5.709755	487.319440	5.722918
5.833301	456.795351	5.727923
5.676607	447.755206	5.732928
5.338173	463.323559	5.737933
5.364571	434.652405	5.742938
5.255667	428.587500	5.747942
5.272299	448.893050	5.752947
5.566134	462.538434	5.757952
5.413518	458.180357	5.762957
5.728425	479.189345	5.767962
5.936078	467.531415	5.772966
5.590793	460.897391	5.777971
5.541642	455.017235	5.782976
5.380872	471.957540	5.787981
5.602444	457.096960	5.792986
5.610522	465.128625	5.797990
5.785367	486.250045	5.802995
5.744495	465.269752	5.808000
5.883083	462.107016	5.813005
5.498833	470.748254	5.818010
5.588268	472.422883	5.823014
5.587431	466.490149	5.828019
5.721465	467.032024	5.833024
5.769668	481.029449	5.838029
5.912471	463.813425	5.843034
5.648406	465.086076	5.848038
5.629956	472.423204	5.853043
6.136210	466.406179	5.858048
5.772049	480.385331	5.863053
5.685980	475.499234	5.868058
5.698834	469.905561	5.873062
5.641954	477.972037	5.878067
5.883424	472.893115	5.883072
5.743001	459.961842	5.888077
5.638514	470.844311	5.893082
5.546028	465.458932	5.898086
5.396408	478.280896	5.903091
5.960796	480.650740	5.908096
5.446100	483.458943	5.913101
5.829325	480.176365	5.918106
5.905941	488.176789	5.923110
5.574455	477.884656	5.928115
5.837238	485.553633	5.933120
5.827251	504.025633	5.938125
5.954323	512.881008	5.943130
6.113985	496.953474	5.948134
5.825052	497.252825	5.953139
6.007639	501.853671	5.958144
6.098517	504.536946	5.963149
6.154597	521.292510	5.968154
6.023018	499.433104	5.973158
6.173748	495.441087	5.978163
6.146397	498.056989	5.983168
6.007414	524.790267	5.988173
5.863120	518.362523	5.993178
6.248146	495.101482	5.998182
5.851493	495.702249	6.003187
5.786415	500.538458	6.008192
6.120981	509.650261	6.013197
5.965389	512.035506	6.018202
5.941926	505.246278	6.023206
6.080258	496.722313	6.028211
6.180636	513.120739	6.033216
5.710511	510.685202	6.038221
6.022777	506.629791	6.043226
6.463593	501.697260	6.048230
6.001853	522.651361	6.053235
6.499201	500.103824	6.058240
6.216274	496.733337	6.063245
6.273417	494.629533	6.068250
6.676684	492.925276	6.073254
6.437492	497.077223	6.078259
6.404880	494.887729	6.083264
6.410979	499.847423	6.088269
6.200303	504.875890	6.093274
5.953991	498.734226	6.098278
5.853876	499.478059	6.103283
6.118299	489.330909	6.108288
6.141460	491.757245	6.113293
6.082250	495.048729	6.118298
6.096815	501.556007	6.123302
6.056028	508.557590	6.128307
6.224414	506.244122	6.133312
6.285502	515.731692	6.138317
6.430340	510.128229	6.143322
6.212260	499.862127	6.148326
6.104200	489.323337	6.153331
6.190580	503.933791	6.158336
6.203113	512.560485	6.163341
6.346870	506.997450	6.168346
6.530789	501.274875	6.173350
6.258856	516.383145	6.178355
6.469872	493.561339	6.183360
6.446894	507.758871	6.188365
6.163930	504.124503	6.193370
6.241274	479.399381	6.198374
6.108072	467.664503	6.203379
6.182228	474.282076	6.208384
5.876470	486.337700	6.213389
6.243170	484.775425	6.218394
6.274376	472.777604	6.223398
6.322768	472.432477	6.228403
6.193367	485.605156	6.233408
5.930214	486.773387	6.238413
6.000607	478.647952	6.243418
6.024666	467.895769	6.248422
6.095790	503.063961	6.253427
6.454143	497.857695	6.258432
6.029053	501.934316	6.263437
5.941358	504.621254	6.268442
6.414887	498.678285	6.273446
6.301205	498.256261	6.278451
6.364935	505.017822	6.283456
6.269576	498.873408	6.288461
5.877846	478.918524	6.293466
6.019264	473.704217	6.298470
6.370844	488.981595	6.303475
6.272658	469.871083	6.308480
5.870934	484.224208	6.313485
6.049696	496.855392	6.318490
6.435410	514.399924	6.323494
5.888542	498.550472	6.328499
6.410890	494.024123	6.333504
6.176236	494.815542	6.338509
6.213677	478.800499	6.343514
6.321741	477.485956	6.348518
6.105548	462.443692	6.353523
5.848639	460.540848	6.358528
6.158220	477.162829	6.363533
6.381269	496.802093	6.368538
6.579430	477.485848	6.373542
6.137813	490.631502	6.378547
6.225276	465.267854	6.383552
6.197390	472.846849	6.388557
5.899200	484.296209	6.393562
6.293600	475.262542	6.398566
5.848168	464.481602	6.403571
6.139332	465.884461	6.408576
5.962319	486.352573	6.413581
6.130479	493.006509	6.418586
6.361608	490.180750	6.423590
6.234113	506.535145	6.428595
6.271527	490.241412	6.433600
6.089751	480.870381	6.438605
5.931116	479.560351	6.443610
6.162469	473.521277	6.448614
6.260615	496.496564	6.453619
6.099878	492.303181	6.458624
6.141780	486.777307	6.463629
6.193743	489.647043	6.468634
6.419436	488.349758	6.473638
6.440014	475.844763	6.478643
6.113123	462.102830	6.483648
6.075676	469.153364	6.488653
6.172472	491.299429	6.493658
6.290086	468.487177	6.498662
5.921284	457.555470	6.503667
6.165485	464.949714	6.508672
6.319597	472.445659	6.513677
6.162785	462.304804	6.518682
5.956523	457.132764	6.523686
5.985524	458.057192	6.528691
6.111767	463.696735	6.533696
6.017706	485.933619	6.538701
6.317622	491.644305	6.543706
6.296093	494.383541	6.548710
5.958603	490.951341	6.553715
6.267249	492.380217	6.558720
6.049876	483.598278	6.563725
6.077923	491.718203	6.568730
6.434170	509.828515	6.573734
6.104392	496.307213	6.578739
6.127763	465.195339	6.583744
5.936635	471.910020	6.588749
5.995418	492.875824	6.593754
6.361902	498.348718	6.598758
6.126523	512.057233	6.603763
6.356318	503.906529	6.608768
6.160646	479.173944	6.613773
6.174146	484.419970	6.618778
6.247067	479.812818	6.623782
5.966207	480.657645	6.628787
6.278655	505.712657	6.633792
6.155345	500.712947	6.638797
5.940721	489.682246	6.643802
5.987499	493.700618	6.648806
6.082263	509.979815	6.653811
6.176513	506.595532	6.658816
6.285498	505.482571	6.663821
6.338751	511.188548	6.668826
6.571568	499.418514	6.673830
5.849006	484.642406	6.678835
6.327864	492.984077	6.683840
6.207911	486.411060	6.688845
5.945519	474.606473	6.693850
6.295162	465.347496	6.698854
5.994215	498.862158	6.703859
6.300515	494.901550	6.708864
6.245673	472.408114	6.713869
6.048239	477.817436	6.718874
6.232190	495.684131	6.723878
6.394875	482.204673	6.728883
6.064053	459.406067	6.733888
5.971848	464.135373	6.738893
5.913159	487.400842	6.743898
6.512945	497.790998	6.748902
6.227875	487.763952	6.753907
6.079970	470.834985	6.758912
6.115884	483.646813	6.763917
6.165198	475.836100	6.768922
6.129117	469.638399	6.773926
6.230281	484.207622	6.778931
6.343027	492.409634	6.783936
6.220978	480.387710	6.788941
5.980253	468.974536	6.793946
6.288528	466.493338	6.798950
6.178880	493.819327	6.803955
6.257877	487.033103	6.808960
6.198016	472.463171	6.813965
5.697475	465.643398	6.818970
6.012085	485.824586	6.823974
5.939880	516.472637	6.828979
6.218231	507.582130	6.833984
6.137381	501.495889	6.838989
6.062676	495.042746	6.843994
6.167563	499.500468	6.848998
6.023010	510.395307	6.854003
6.251844	512.005274	6.859008
6.342631	501.409448	6.864013
6.599410	500.927881	6.869018
6.611481	510.574580	6.874022
5.955411	489.287115	6.879027
5.760560	490.143673	6.884032
6.014383	500.208738	6.889037
5.814550	507.017405	6.894042
6.407439	483.136551	6.899046
5.902341	502.064936	6.904051
6.207725	515.464105	6.909056
6.263058	504.602358	6.914061
5.998292	503.102505	6.919066
6.337166	501.535948	6.924070
6.245501	507.363731	6.929075
6.515640	512.194070	6.934080
6.357776	506.202925	6.939085
5.926952	488.941584	6.944090
6.241375	491.199239	6.949094
6.045200	504.283333	6.954099
6.471390	494.041479	6.959104
6.191273	495.356935	6.964109
5.985634	491.157162	6.969114
5.983518	463.843730	6.974118
6.384937	480.270800	6.979123
6.344119	482.846703	6.984128
6.130146	484.885569	6.989133
5.879855	484.134240	6.994138
6.034164	484.942865	6.999142
5.901885	496.406250	7.004147
5.873329	505.320188	7.009152
6.253691	516.279123	7.014157
5.967192	510.015556	7.019162
6.306157	495.532897	7.024166
6.418958	510.038665	7.029171
6.138383	496.715802	7.034176
6.399812	510.909941	7.039181
6.293670	503.855201	7.044186
6.309285	498.548721	7.049190
5.899696	508.207487	7.054195
6.289074	516.047136	7.059200
6.278362	509.103979	7.064205
6.082723	489.433438	7.069210
6.284480	490.542500	7.074214
6.196253	487.967503	7.079219
6.354194	456.122055	7.084224
6.154425	485.832459	7.089229
5.987450	496.200362	7.094234
6.387710	470.303117	7.099238
5.977490	458.876626	7.104243
6.080204	459.597989	7.109248
6.022979	484.797118	7.114253
6.313016	501.963936	7.119258
6.130486	477.763068	7.124262
6.001222	482.104107	7.129267
6.144845	508.365973	7.134272
6.158166	494.717835	7.139277
6.497895	496.008399	7.144282
6.412157	500.201971	7.149286
6.288705	489.347682	7.154291
6.180521	485.067191	7.159296
6.304766	467.539934	7.164301
5.932376	489.195412	7.169306
6.136771	475.766876	7.174310
5.955841	462.877808	7.179315
6.218718	457.948850	7.184320
6.259702	480.008137	7.189325
6.079701	494.461358	7.194330
6.081094	476.844103	7.199334
6.468702	465.323942	7.204339
6.177760	476.332915	7.209344
6.453580	466.805383	7.214349
6.048388	479.386065	7.219354
6.363168	469.923218	7.224358
5.913331	470.287829	7.229363
5.959953	473.583029	7.234368
6.143330	480.820714	7.239373
5.821112	492.900668	7.244378
6.182128	483.977179	7.249382
6.184039	472.283795	7.254387
6.362859	477.800222	7.259392
6.084829	477.230551	7.264397
5.953361	475.327693	7.269402
5.887607	468.410322	7.274406
6.286407	476.986285	7.279411
6.367407	486.331748	7.284416
6.282663	489.658919	7.289421
6.284461	489.636477	7.294426
6.157776	482.402345	7.299430
6.192509	469.532285	7.304435
6.207078	476.033040	7.309440
6.012692	481.615778	7.314445
6.011327	481.273743	7.319450
6.367514	462.737855	7.324454
6.117501	480.731390	7.329459
6.284670	471.957432	7.334464
6.307536	473.554376	7.339469
6.258494	464.313635	7.344474
6.352934	457.127911	7.349478
6.453438	467.587630	7.354483
6.113809	468.353778	7.359488
6.360553	462.631391	7.364493
6.283485	484.995584	7.369498
6.346299	483.881375	7.374502
5.997428	477.888364	7.379507
6.493216	468.245858	7.384512
6.561095	469.679893	7.389517
6.085613	483.983846	7.394522
6.124325	496.389579	7.399526
6.022349	472.801334	7.404531
6.025005	460.936582	7.409536
6.351566	471.316528	7.414541
5.894744	493.127230	7.419546
5.948800	482.602397	7.424550
6.119937	467.177585	7.429555
6.281065	462.126740	7.434560
6.588623	479.259662	7.439565
6.225320	490.020072	7.444570
6.317325	471.510270	7.449574
6.268347	482.617865	7.454579
6.315770	475.754886	7.459584
6.426739	466.205074	7.464589
6.030409	480.371252	7.469594
6.029485	466.264509	7.474598
6.157592	482.496340	7.479603
6.022638	485.554900	7.484608
6.419467	469.008247	7.489613
6.233427	481.110771	7.494618
6.208537	473.290323	7.499622
6.008413	475.109181	7.504627
6.287918	479.482798	7.509632
6.089638	463.494887	7.514637
6.000443	471.330732	7.519642
6.192481	479.499116	7.524646
6.050142	498.218886	7.529651
5.998377	480.008062	7.534656
6.058090	477.523940	7.539661
5.733916	482.665069	7.544666
6.104966	468.442795	7.549670
6.202844	470.102118	7.554675
6.288415	479.548529	7.559680
6.305712	495.652192	7.564685
6.009196	484.440294	7.569690
6.478268	468.000083	7.574694
6.279066	475.129831	7.579699
6.423170	481.179668	7.584704
6.693650	490.285574	7.589709
5.985080	467.724875	7.594714
6.203690	438.827118	7.599718
6.014786	452.394824	7.604723
6.184624	471.200094	7.609728
6.189779	470.882829	7.614733
6.169166	477.983066	7.619738
6.321139	456.457155	7.624742
6.177991	450.847737	7.629747
5.886563	460.997651	7.634752
6.135159	465.885299	7.639757
5.997634	477.631079	7.644762
6.064375	471.846100	7.649766
6.120509	485.645611	7.654771
6.186826	482.417671	7.659776
6.137509	476.469270	7.664781
6.226866	474.750103	7.669786
6.103317	472.986708	7.674790
6.131970	484.980460	7.679795
6.331843	479.679840	7.684800
6.124403	462.237292	7.689805
6.124430	476.716581	7.694810
6.245352	495.209949	7.699814
6.137484	482.145330	7.704819
5.964668	473.572962	7.709824
6.692467	463.457079	7.714829
6.058434	489.914798	7.719834
6.061874	482.612404	7.724838
6.403642	477.299287	7.729843
6.363726	452.635214	7.734848
5.988759	450.084426	7.739853
5.808496	465.254541	7.744858
6.005970	454.325540	7.749862
6.089389	471.823400	7.754867
5.932645	484.260633	7.759872
6.404114	481.436986	7.764877
5.926855	481.185234	7.769882
6.192937	470.760915	7.774886
6.023859	458.122729	7.779891
5.861250	463.792741	7.784896
6.302434	488.968014	7.789901
5.952733	497.967867	7.794906
6.438981	479.459396	7.799910
6.197450	473.101898	7.804915
6.237086	470.691234	7.809920
6.492608	471.474452	7.814925
6.276661	469.476745	7.819930
6.086170	480.338314	7.824934
6.075139	500.073185	7.829939
5.898982	470.369931	7.834944
6.094479	461.477654	7.839949
6.188109	467.018217	7.844954
6.046298	484.300869	7.849958
5.922029	494.808306	7.854963
6.176060	486.989209	7.859968
6.429898	478.505158	7.864973
6.123416	478.242054	7.869978
6.202074	478.996987	7.874982
6.121913	480.491099	7.879987
6.144385	489.392748	7.884992
6.235482	473.216827	7.889997
6.072761	469.153600	7.895002
6.255571	462.555421	7.900006
6.325615	482.430960	7.905011
6.154584	498.625233	7.910016
6.307769	481.971743	7.915021
6.175907	476.511383	7.920026
6.246347	488.121000	7.925030
6.193060	485.632368	7.930035
6.309865	483.849673	7.935040
6.308051	484.189079	7.940045
6.049868	490.284878	7.945050
6.201169	479.359346	7.950054
6.040804	472.366358	7.955059
5.930297	494.603901	7.960064
6.294274	495.251017	7.965069
6.036554	490.102365	7.970074
5.977654	470.564822	7.975078
6.190623	476.406670	7.980083
6.241500	501.684836	7.985088
6.239996	481.749314	7.990093
6.137932	471.071142	7.995098
6.086154	483.225467	8.000102
6.006370	479.677683	8.005107
5.958486	479.544086	8.010112
6.369235	493.774574	8.015130
6.083146	489.926460	8.020147
6.153495	484.487108	8.025165
6.167609	478.862717	8.030182
5.849395	473.029444	8.035200
6.195696	469.419844	8.040218
5.846837	477.838234	8.045235
6.168201	492.575727	8.050253
6.131877	476.708374	8.055270
6.156621	473.138627	8.060288
6.503672	490.378044	8.065306
6.178842	493.930675	8.070323
6.038915	475.408766	8.075341
6.379929	493.510944	8.080358
6.167494	488.626346	8.085376
6.462597	474.333583	8.090394
6.132815	481.565501	8.095411
6.582521	481.229797	8.100429
6.361929	486.155746	8.105446
6.165121	491.367744	8.110464
6.432599	476.554103	8.115482
6.160439	479.321380	8.120499
6.414955	471.720025	8.125517
6.230760	481.081105	8.130534
5.957785	497.829263	8.135552
6.515382	472.302130	8.140570
6.180435	487.041904	8.145587
6.182012	471.099514	8.150605
6.804832	468.144215	8.155622
6.455287	480.467504	8.160640
6.618136	471.564352	8.165658
6.235737	470.899556	8.170675
6.309533	486.681406	8.175693
6.650829	489.064025	8.180710
6.282772	481.962283	8.185728
6.475377	478.633714	8.190746
6.671233	499.056867	8.195763
6.542469	477.640531	8.200781
6.231902	463.405751	8.205798
6.017996	473.176443	8.210816
6.142348	487.235176	8.215834
6.169310	495.599343	8.220851
6.075552	480.724562	8.225869
6.502770	463.482666	8.230886
6.450887	494.765985	8.235904
6.488714	498.137757	8.240922
6.218349	489.900797	8.245939
6.253840	476.101691	8.250957
6.099710	474.003117	8.255974
6.077686	482.668004	8.260992
6.482127	490.376849	8.266010
6.556889	478.251578	8.271027
6.490424	459.303100	8.276045
6.104474	476.443615	8.281062
6.174054	486.508119	8.286080
6.190385	489.311951	8.291098
6.361717	472.971731	8.296115
6.323175	492.008328	8.301133
6.409747	511.055269	8.306150
6.281903	510.548644	8.311168
6.456503	506.143923	8.316186
6.494936	520.387506	8.321203
6.178965	519.119772	8.326221
6.650682	506.461986	8.331238
6.641703	511.929877	8.336256
6.754100	508.099152	8.341274
6.572499	509.705634	8.346291
6.515528	527.033505	8.351309
6.645589	523.520337	8.356326
6.638652	500.404590	8.361344
6.621486	502.346885	8.366362
6.191423	490.741024	8.371379
6.094299	498.172230	8.376397
6.749137	510.746772	8.381414
6.625539	521.967409	8.386432
6.675208	503.892543	8.391450
6.792659	510.564684	8.396467
6.642169	510.276798	8.401485
6.375895	492.019085	8.406502
6.344397	501.337626	8.411520
6.455440	505.930118	8.416538
6.532639	517.194222	8.421555
6.414691	509.659220	8.426573
6.280071	510.497525	8.431590
6.384312	524.758181	8.436608
6.804717	516.246965	8.441626
6.545747	509.543108	8.446643
6.649718	508.281647	8.451661
6.961784	525.001542	8.456678
6.559846	526.857959	8.461696
6.824975	498.080149	8.466714
6.567200	507.407551	8.471731
6.832976	514.927670	8.476749
6.885526	498.860325	8.481766
6.544025	506.960382	8.486784
6.846028	516.305884	8.491802
6.594100	509.128262	8.496819
6.370505	515.418306	8.501837
6.860445	511.792142	8.506854
6.641110	507.483809	8.511872
6.957035	492.230480	8.516890
6.709595	517.761890	8.521907
6.601883	531.995884	8.526925
6.765710	496.758011	8.531942
6.337277	490.966068	8.536960
6.401909	494.825789	8.541978
6.452385	519.814904	8.546995
6.254975	520.205252	8.552013
6.894415	513.416200	8.557030
6.307008	507.934495	8.562048
6.629540	508.158924	8.567066
6.588573	518.761647	8.572083
6.491582	516.752613	8.577101
6.616436	514.755920	8.582119
6.782757	537.553606	8.587136
7.149076	540.894129	8.592154
6.655131	530.171382	8.597171
6.605860	539.974342	8.602189
6.766623	526.584780	8.607207
6.907423	535.158833	8.612224
7.058301	528.463695	8.617242
7.167039	523.485766	8.622259
6.564158	527.110920	8.627277
6.616473	512.991865	8.632295
6.469716	528.395757	8.637312
7.053433	548.047797	8.642330
7.089503	539.107206	8.647347
6.936443	524.551150	8.652365
6.876466	522.535801	8.657383
6.689579	531.196276	8.662400
6.920458	540.930014	8.667418
7.146548	535.298322	8.672435
6.822049	525.602987	8.677453
6.981495	497.004802	8.682471
6.779971	512.866025	8.687488
6.798110	508.153199	8.692506
6.757731	514.359142	8.697523
7.329116	513.507113	8.702541
7.368456	513.312331	8.707559
6.913174	525.257473	8.712576
7.074047	512.338933	8.717594
7.315924	508.915528	8.722611
7.006761	512.623698	8.727629
7.055494	511.579869	8.732647
6.851026	502.588819	8.737664
6.788146	490.315564	8.742682
7.092775	499.824158	8.747699
6.704972	515.630168	8.752717
7.207840	500.065112	8.757735
6.825459	499.689009	8.762752
6.694704	512.195396	8.767770
6.966799	528.939514	8.772787
6.881129	513.281795	8.777805
6.667633	487.381416	8.782823
6.973565	504.156420	8.787840
6.678932	499.552058	8.792858
6.818880	523.435662	8.797875
6.626272	534.390823	8.802893
7.166900	534.259322	8.807911
7.370613	548.832211	8.812928
6.968572	553.391330	8.817946
7.248226	538.609958	8.822963
6.741762	521.048212	8.827981
6.837305	536.699686	8.832999
6.910357	548.830985	8.838016
6.878451	541.881580	8.843034
6.999848	546.397985	8.848051
6.690565	545.191626	8.853069
6.909939	528.069512	8.858087
6.704088	545.708540	8.863104
6.719735	559.746141	8.868122
7.049183	553.634697	8.873139
6.792454	540.985873	8.878157
6.914953	540.010144	8.883175
7.212126	571.330398	8.888192
7.242697	572.632806	8.893210
7.195889	564.684264	8.898227
6.930267	566.465909	8.903245
6.920893	549.272843	8.908263
7.122634	556.318466	8.913280
7.133133	577.836914	8.918298
7.302823	586.608528	8.923315
7.129826	565.619340	8.928333
7.025562	564.432825	8.933351
7.109351	571.765687	8.938368
7.006520	589.118720	8.943386
7.399070	573.108662	8.948403
7.368846	567.433709	8.953421
7.254263	567.544402	8.958439
7.099622	585.015803	8.963456
7.256575	595.561176	8.968474
7.095070	574.364917	8.973491
7.198360	568.720444	8.978509
7.287329	572.984710	8.983527
7.411127	569.086061	8.988544
7.279669	558.440953	8.993562
7.323708	563.234344	8.998579
7.093320	577.902118	9.003597
7.248109	578.662983	9.008615
7.289138	581.326471	9.013632
7.266383	560.830231	9.018650
7.362148	576.782510	9.023667
7.300506	588.122941	9.028685
7.341660	570.523484	9.033703
7.449713	562.441705	9.038720
7.561467	573.922222	9.043738
7.746303	560.701538	9.048755
7.336629	549.742867	9.053773
7.277671	526.428157	9.058791
7.226019	542.706251	9.063808
6.996389	547.623579	9.068826
6.982078	541.735139	9.073843
7.629091	569.993705	9.078861
7.310384	567.453155	9.083879
7.067067	556.785599	9.088896
7.258185	563.359689	9.093914
7.507278	578.315054	9.098931
7.393083	590.900637	9.103949
7.537798	569.009869	9.108967
7.203327	582.069909	9.113984
7.292367	575.394219	9.119002
7.432452	550.640282	9.124019
6.841962	578.504218	9.129037
7.009699	594.375942	9.134055
7.392033	575.045369	9.139072
6.940498	571.116633	9.144090
7.339104	567.597158	9.149107
7.136675	588.015202	9.154125
7.111836	570.677072	9.159143
7.544067	591.405382	9.164160
7.494545	618.474189	9.169178
7.576540	614.189337	9.174195
7.387240	608.022788	9.179213
7.633293	598.272679	9.184231
7.697008	607.665585	9.189248
7.212291	613.864997	9.194266
7.674984	598.954038	9.199283
7.553717	580.196010	9.204301
7.548341	588.169915	9.209319
7.146609	593.535659	9.214336
7.414761	600.643634	9.219354
7.912474	602.768106	9.224371
7.709529	617.277095	9.229389
7.801673	595.701978	9.234407
7.375479	574.723917	9.239424
7.444715	587.221721	9.244442
7.846316	582.033217	9.249459
7.579625	579.377997	9.254477
7.483956	561.344989	9.259495
7.892720	567.606421	9.264512
7.598801	578.487139	9.269530
7.502651	576.475596	9.274547
7.467948	584.597316	9.279565
7.527214	573.647430	9.284583
8.023952	577.888198	9.289600
7.429441	588.582051	9.294618
7.409017	570.926350	9.299635
7.300889	565.078299	9.304653
7.422861	605.048283	9.309671
7.822794	616.086931	9.314688
7.759950	617.460276	9.319706
7.722772	603.523203	9.324723
7.780082	604.777408	9.329741
7.690683	614.522300	9.334759
7.824237	589.149670	9.339776
7.671059	592.933826	9.344794
7.475966	585.349642	9.349811
7.891756	581.285252	9.354829
7.836194	584.687137	9.359847
7.865820	591.883331	9.364864
7.548584	591.891821	9.369882
7.796411	565.753114	9.374899
7.631346	560.145314	9.379917
7.227172	571.758910	9.384935
7.762955	603.504531	9.389952
8.089277	600.220750	9.394970
8.039238	586.972044	9.399987
8.036386	582.837698	9.405005
7.926721	587.922270	9.410023
7.787979	578.435212	9.415040
7.514958	564.342421	9.420058
7.521391	557.930516	9.425075
7.487704	576.937782	9.430093
7.579473	598.626540	9.435111
8.032735	608.519975	9.440128
7.866531	620.251029	9.445146
7.493270	595.222206	9.450163
7.747204	607.624267	9.455181
7.698805	628.211346	9.460199
7.995957	606.994942	9.465216
7.562011	601.902786	9.470234
7.637851	604.075030	9.475251
7.783712	630.154261	9.480269
7.450019	622.916690	9.485287
7.679763	601.872412	9.490304
7.845482	610.288790	9.495322
7.796424	623.590696	9.500339
7.876067	627.968004	9.505357
8.121480	612.178228	9.510375
7.859120	603.916662	9.515392
7.962848	610.990807	9.520410
7.783203	619.191010	9.525427
8.090064	610.345158	9.530445
7.853301	627.661823	9.535463
8.260030	612.475135	9.540480
7.778428	604.076226	9.545498
8.061200	604.327694	9.550515
8.281951	628.772951	9.555533
7.837173	624.799001	9.560551
8.068761	601.279021	9.565568
7.877237	613.777428	9.570586
7.945809	616.447489	9.575603
7.899617	628.593146	9.580621
7.707848	608.325797	9.585639
7.784982	607.263000	9.590656
7.714555	616.939423	9.595674
7.914153	629.464229	9.600691
7.954290	641.762217	9.605709
7.939011	639.888244	9.610727
7.983569	641.346177	9.615744
8.014348	642.652492	9.620762
8.216412	635.829689	9.625779
8.278113	636.165609	9.630797
7.976533	648.774431	9.635815
8.424807	651.890667	9.640832
8.178273	638.129656	9.645850
7.861775	638.293099	9.650867
8.181548	649.074325	9.655885
8.061656	648.307299	9.660903
8.138350	623.376564	9.665920
7.893941	645.906159	9.670938
8.024683	655.701585	9.675955
8.300741	647.965813	9.680973
8.263518	651.300625	9.685991
8.326447	638.307245	9.691008
8.327729	645.114161	9.696026
8.041638	638.398002	9.701043
8.203580	639.792159	9.706061
8.228045	640.468589	9.711079
8.380166	621.059300	9.716096
8.106750	633.370919	9.721114
8.146798	620.633724	9.726131
8.322916	607.240571	9.731149
8.065139	612.427261	9.736167
8.167335	632.017880	9.741184
7.847384	641.555878	9.746202
8.015541	649.783344	9.751219
8.529586	638.317829	9.756237
8.274532	636.191828	9.761255
8.729213	643.938499	9.766272
8.311428	641.759981	9.771290
8.053771	646.764135	9.776307
8.027611	630.152234	9.781325
8.293908	648.038266	9.786343
8.448107	654.792070	9.791360
8.465063	644.860855	9.796378
8.746270	643.025166	9.801395
8.553299	634.773371	9.806413
8.268881	619.466308	9.811431
8.400022	608.902736	9.816448
8.227241	614.986053	9.821466
8.174088	602.950503	9.826483
8.421758	599.354219	9.831501
8.194699	613.437586	9.836519
8.292423	624.192218	9.841536
8.048000	623.483655	9.846554
8.365799	625.466650	9.851571
8.600366	632.165443	9.856589
8.169124	633.490248	9.861607
8.464376	648.288196	9.866624
8.520048	660.946328	9.871642
8.200423	648.005038	9.876659
8.318634	632.497214	9.881677
8.217394	638.198643	9.886695
8.572423	639.214925	9.891712
8.474347	655.097281	9.896730
8.090374	635.144357	9.901747
8.251239	639.126461	9.906765
8.175171	652.569629	9.911783
8.336891	639.324948	9.916800
8.099728	643.546106	9.921818
8.298225	654.554702	9.926835
8.382970	637.817802	9.931853
8.374114	635.771359	9.936871
8.406164	666.694994	9.941888
8.700284	667.597263	9.946906
8.475119	657.463990	9.951923
8.673571	665.672781	9.956941
8.608890	666.959253	9.961959
8.322650	669.070606	9.966976
8.657852	655.838767	9.971994
8.577014	666.314065	9.977011
8.600163	669.939707	9.982029
8.784273	655.271427	9.987047
8.519055	644.648559	9.992064
8.614028	648.737984	9.997082
8.645815	666.042293	10.002099
8.713232	638.281661	10.007117
8.415711	652.068130	10.012135
8.425604	645.191375	10.017152
8.548052	646.843368	10.022170
8.337224	677.437676	10.027187
8.750812	667.471700	10.032205
8.508965	666.363311	10.037223
8.850992	659.040728	10.042240
9.117648	667.783178	10.047258
8.618435	684.151126	10.052275
9.084585	657.316818	10.057293
8.836554	648.051855	10.062311
8.734781	640.860182	10.067328
8.352169	633.819124	10.072346
8.472561	654.198867	10.077363
9.012754	651.547463	10.082381
8.519722	656.639419	10.087399
8.934204	660.615337	10.092416
8.740784	651.130383	10.097434
8.397803	647.448279	10.102451
8.710817	663.374884	10.107469
8.458890	674.671549	10.112487
8.647621	671.163216	10.117504
8.831617	685.026007	10.122522
8.779549	683.452122	10.127539
8.731881	659.281050	10.132557
8.809277	675.028848	10.137575
8.660462	678.573393	10.142592
8.623187	672.110017	10.147610
8.621242	685.719755	10.152627
9.004861	669.228036	10.157645
8.933307	663.086384	10.162663
8.928804	683.756220	10.167680
8.686769	675.604316	10.172698
8.627189	671.712919	10.177715
8.960519	686.808662	10.182733
8.682607	682.990930	10.187751
8.768928	668.009655	10.192768
8.985711	676.164156	10.197786
8.709916	692.399452	10.202803
8.776131	680.480397	10.207821
8.696388	690.250506	10.212839
8.728463	666.334676	10.217856
8.810412	679.643124	10.222874
8.838383	703.684550	10.227891
9.146083	699.624904	10.232909
9.067286	689.799615	10.237927
8.729724	704.352187	10.242944
9.145338	711.710673	10.247962
9.325123	714.748095	10.252979
9.082769	675.216601	10.257997
9.270547	679.525280	10.263015
8.940738	683.604715	10.268032
9.189293	705.433222	10.273050
9.105171	687.109061	10.278067
9.338350	676.795437	10.283085
9.442705	686.425604	10.288103
9.091245	676.789240	10.293120
9.233427	663.518542	10.298138
9.041068	678.234248	10.303155
9.055484	688.402660	10.308173
8.976862	684.685619	10.313191
8.729318	693.801757	10.318208
9.045953	687.036257	10.323226
8.979349	676.261976	10.328243
9.239801	674.649437	10.333261
9.223745	692.750835	10.338279
9.087905	693.204220	10.343296
9.269552	671.755209	10.348314
9.158361	693.487579	10.353331
8.969348	678.282181	10.358349
9.284913	662.624915	10.363367
8.765070	677.113219	10.368384
8.982536	692.836511	10.373402
8.938019	695.115543	10.378419
9.244007	678.993730	10.383437
9.014093	664.901495	10.388455
9.151626	691.173884	10.393472
9.350408	707.167331	10.398490
9.277622	700.342392	10.403507
8.994790	695.057563	10.408525
9.389546	710.123695	10.413543
8.807300	734.407014	10.418560
9.571220	734.344294	10.423578
9.189858	715.209904	10.428595
9.227532	714.990696	10.433613
9.607891	713.635822	10.438631
9.291223	699.715328	10.443648
9.375566	693.467412	10.448666
9.127065	698.615010	10.453683
9.327074	698.411681	10.458701
9.285310	714.045586	10.463719
9.128679	711.907245	10.468736
9.250382	712.458388	10.473754
9.390794	729.907470	10.478771
9.374853	718.203974	10.483789
9.422843	723.064264	10.488807
9.114356	723.832027	10.493824
9.527658	720.357518	10.498842
9.308987	713.764596	10.503859
9.499730	708.801789	10.508877
9.311510	715.335016	10.513895
9.206957	715.539794	10.518912
9.235460	718.701795	10.523930
9.472942	719.710743	10.528947
9.054241	732.618046	10.533965
9.521645	713.124561	10.538983
9.120705	710.591573	10.544000
9.352899	715.152891	10.549018
9.160805	706.844333	10.554035
8.857298	722.052039	10.559053
9.350721	735.146122	10.564071
9.325996	744.715691	10.569088
9.665486	737.417794	10.574106
9.702619	758.728510	10.579123
9.455671	766.940308	10.584141
9.826810	756.933763	10.589159
9.289914	728.433981	10.594176
9.701316	724.969821	10.599194
9.503693	746.069283	10.604211
9.496947	752.614553	10.609229
9.657187	751.810282	10.614247
9.784127	745.064690	10.619264
9.752705	734.194914	10.624282
9.475187	726.910227	10.629299
9.559449	713.774614	10.634317
9.695737	723.133950	10.639335
9.428233	719.795658	10.644352
9.509907	727.468616	10.649370
9.729232	742.925385	10.654387
9.849174	746.463909	10.659405
9.783313	729.147433	10.664423
9.696894	732.463529	10.669440
9.673557	721.132117	10.674458
9.547366	722.578718	10.679475
9.441957	722.169236	10.684493
9.970944	743.192212	10.689511
9.631907	758.384080	10.694528
9.877289	739.777809	10.699546
9.915976	713.170692	10.704563
9.280901	720.315808	10.709581
9.835746	757.282972	10.714599
9.917641	742.953951	10.719616
9.727893	729.816373	10.724634
9.934323	738.684435	10.729651
9.827583	724.996478	10.734669
9.829155	703.326756	10.739687
9.648525	724.804772	10.744704
10.006608	714.825798	10.749722
9.916830	706.343879	10.754739
9.758937	702.931784	10.759757
9.970593	704.836980	10.764775
9.474905	730.518203	10.769792
10.057777	713.230725	10.774810
9.615638	713.216658	10.779827
9.721912	732.366988	10.784845
9.952323	731.664576	10.789863
9.880418	738.161175	10.794880
10.050990	747.512696	10.799898
9.902267	723.195077	10.804915
9.833030	724.694552	10.809933
9.958127	749.735769	10.814951
9.845199	738.732254	10.819968
9.872138	719.730136	10.824986
9.955733	746.160017	10.830003
9.927310	768.980389	10.835021
10.180118	762.383235	10.840039
9.881597	736.258853	10.845056
10.047841	743.245780	10.850074
9.853969	733.806703	10.855091
9.862329	749.009049	10.860109
10.247169	749.151650	10.865127
10.000727	740.662440	10.870144
10.347508	736.657825	10.875162
9.787177	732.192646	10.880179
9.762640	737.017301	10.885197
10.033415	730.599130	10.890215
10.043531	750.468037	10.895232
10.137778	745.464486	10.900250
10.195305	741.929800	10.905267
9.805203	737.310244	10.910285
10.128973	752.875419	10.915303
10.087392	769.505637	10.920320
9.513005	752.245223	10.925338
9.658921	737.777119	10.930355
9.715463	742.427101	10.935373
10.114672	739.596475	10.940391
9.950204	760.482955	10.945408
10.002956	755.579933	10.950426
10.148870	731.875441	10.955443
9.913917	746.127709	10.960461
9.945187	770.587480	10.965479
10.086373	779.854629	10.970496
10.221877	772.241699	10.975514
10.117187	771.060552	10.980531
9.926911	789.946952	10.985549
10.340622	779.801305	10.990567
10.243798	785.818904	10.995584
10.287347	788.806236	11.000602
10.753702	786.520853	11.005619
10.588909	771.257733	11.010637
10.846632	761.038690	11.015655
10.307501	773.837321	11.020672
10.000273	771.739110	11.025690
10.218131	752.139609	11.030707
10.250555	737.253074	11.035725
10.136015	746.853426	11.040743
10.104812	768.151242	11.045760
10.002094	766.849723	11.050778
10.484607	774.492774	11.055795
10.228166	777.012197	11.060813
10.462282	767.830042	11.065831
10.661104	771.021276	11.070848
10.439529	774.879164	11.075866
10.592223	782.960773	11.080883
10.146767	776.181542	11.085901
10.413918	755.817990	11.090919
10.478200	772.000419	11.095936
10.640251	777.375297	11.100954
10.639356	771.869095	11.105971
10.306865	765.033317	11.110989
10.681672	762.533994	11.116007
10.808095	770.911100	11.121024
10.528491	762.324728	11.126042
10.445624	741.460721	11.131059
10.234534	745.682912	11.136077
10.354529	750.097373	11.141095
10.616619	761.300600	11.146112
10.560840	750.691854	11.151130
10.726556	751.789120	11.156147
10.371631	741.982466	11.161165
10.609472	730.023302	11.166183
10.500425	742.772188	11.171200
10.452351	772.107642	11.176218
10.637881	763.892612	11.181235
10.315316	768.463162	11.186253
10.403315	773.244139	11.191271
10.668743	787.992048	11.196288
10.544252	783.355645	11.201306
10.685569	769.484568	11.206323
10.336344	762.831234	11.211341
10.814991	780.793816	11.216359
10.356910	778.804763	11.221376
10.257251	772.548845	11.226394
10.773478	779.134935	11.231411
10.359522	780.387033	11.236429
10.627977	782.902078	11.241447
10.624819	774.770276	11.246464
10.528750	769.130039	11.251482
10.655825	773.333157	11.256499
10.582418	795.487561	11.261517
10.492473	771.645455	11.266535
10.496860	764.509094	11.271552
10.819437	786.663976	11.276570
11.068808	799.932169	11.281587
10.741094	809.115939	11.286605
11.029364	779.696741	11.291623
10.878662	774.308182	11.296640
10.891431	795.256538	11.301658
10.734768	778.188413	11.306675
10.572606	773.913852	11.311693
11.035532	786.702374	11.316711
11.053713	770.774344	11.321728
10.530702	768.387371	11.326746
10.835044	778.979066	11.331763
10.894920	815.218833	11.336781
11.178924	799.911237	11.341799
10.617528	780.805728	11.346816
10.754794	788.366801	11.351834
10.970513	791.766116	11.356851
11.111822	807.220197	11.361869
10.966555	806.979068	11.366887
11.112483	799.504030	11.371904
10.815111	809.873120	11.376922
11.214847	794.139623	11.381939
10.733490	785.356029	11.386957
10.879553	807.946301	11.391975
11.214537	815.125397	11.396992
11.143080	801.507506	11.402010
11.011777	796.677591	11.407027
10.991987	784.432404	11.412045
11.115529	782.836082	11.417063
10.769307	776.092505	11.422080
10.823569	794.711593	11.427098
11.335389	794.276174	11.432115
11.086214	792.794972	11.437133
11.005287	806.907700	11.442151
11.180330	816.177148	11.447168
10.910899	817.346917	11.452186
11.129696	796.009475	11.457203
10.767250	813.209162	11.462221
10.811941	822.750580	11.467239
11.066484	827.864982	11.472256
11.246130	823.787989	11.477274
11.567998	794.125577	11.482291
11.455638	816.034350	11.487309
11.335281	814.056591	11.492327
11.381784	787.396984	11.497344
11.159472	800.016741	11.502362
11.443835	813.161478	11.507379
11.141991	795.892581	11.512397
11.076736	792.631451	11.517415
11.327861	780.302532	11.522432
11.132521	795.389315	11.527450
11.489201	806.339999	11.532467
11.525182	799.128045	11.537485
11.228434	797.078873	11.542503
10.930031	789.253461	11.547520
11.103019	809.602285	11.552538
10.926167	801.138342	11.557555
11.354714	808.983683	11.562573
11.323279	805.780134	11.567591
11.528252	793.280335	11.572608
11.358921	811.973785	11.577626
11.543513	819.840355	11.582643
11.314236	811.787523	11.587661
11.369342	801.407105	11.592679
11.454603	802.371743	11.597696
11.285407	823.729241	11.602714
11.283349	815.844218	11.607731
11.375925	800.626408	11.612749
11.390875	803.931279	11.617767
11.274426	795.075570	11.622784
11.351683	807.212579	11.627802
11.659223	817.421197	11.632819
11.494510	815.735239	11.637837
11.426885	801.089623	11.642855
11.577872	800.608152	11.647872
11.199092	821.207676	11.652890
11.245876	802.725069	11.657907
11.235302	811.247539	11.662925
11.189126	818.907722	11.667943
11.296399	815.197322	11.672960
11.120959	840.598408	11.677978
11.738342	835.075619	11.682995
11.591790	820.211593	11.688013
11.491960	830.464119	11.693031
11.781015	837.136679	11.698048
11.537227	853.300830	11.703066
11.602427	835.592003	11.708083
11.712152	840.912673	11.713101
11.480152	846.544867	11.718119
11.683070	840.982131	11.723136
11.440180	843.041473	11.728154
11.798820	829.036523	11.733171
11.831312	833.483770	11.738189
11.859228	850.600197	11.743207
12.126247	838.088141	11.748224
11.877231	838.592900	11.753242
11.971721	825.574761	11.758259
11.907479	818.549198	11.763277
11.282534	822.442660	11.768295
11.775543	833.942043	11.773312
11.647456	836.665403	11.778330
11.733715	836.118269	11.783347
11.814889	828.618493	11.788365
11.818449	833.249412	11.793383
12.139753	839.812538	11.798400
11.807490	839.953988	11.803418
12.089334	835.249144	11.808435
11.930896	814.496908	11.813453
11.592378	823.160465	11.818471
11.809350	819.565169	11.823488
11.520600	830.249004	11.828506
11.951358	816.584417	11.833523
12.066448	826.521971	11.838541
11.853206	846.428207	11.843559
11.943188	837.372853	11.848576
11.841489	828.470604	11.853594
11.859634	835.219616	11.858611
11.885096	838.529547	11.863629
11.860334	856.759415	11.868647
11.932810	840.134430	11.873664
11.709207	836.548468	11.878682
11.740459	838.412252	11.883699
11.739134	843.436496	11.888717
11.599548	848.925205	11.893735
11.909030	829.427165	11.898752
11.951280	824.824302	11.903770
11.991793	831.139021	11.908787
12.063391	853.761445	11.913805
12.087404	866.275214	11.918823
12.255920	844.651603	11.923840
12.108962	846.015744	11.928858
11.916448	841.526159	11.933875
12.000296	841.763469	11.938893
12.364245	867.831271	11.943911
12.433323	863.046253	11.948928
12.248395	845.469473	11.953946
12.111175	836.857463	11.958963
11.836309	847.216561	11.963981
11.840592	862.222501	11.968999
12.212087	860.286751	11.974016
12.280525	889.928191	11.979034
12.024147	871.955419	11.984051
12.480474	859.380574	11.989069
12.339811	869.687695	11.994087
12.188860	873.276229	11.999104
12.135856	871.527624	12.004122
12.191330	871.741284	12.009139
12.288978	871.782073	12.014157
11.856851	872.840087	12.019175
12.140854	855.622894	12.024192
12.290139	887.353370	12.029210
11.987562	880.433484	12.034227
12.594062	865.594933	12.039245
12.276494	877.883047	12.044263
12.388052	868.318139	12.049280
12.171120	863.545453	12.054298
12.249692	865.723679	12.059315
12.721109	873.300324	12.064333
12.206592	871.419377	12.069351
12.556842	849.738273	12.074368
12.455965	868.904014	12.079386
12.091343	888.123007	12.084403
12.501946	865.807365	12.089421
12.132321	859.149782	12.094439
12.593038	859.041326	12.099456
12.503945	879.153112	12.104474
12.699249	879.074248	12.109491
12.947673	873.390427	12.114509
12.732011	870.197235	12.119527
12.671268	862.329560	12.124544
12.420946	879.151240	12.129562
12.455975	868.921202	12.134579
12.686499	863.591628	12.139597
12.482671	864.136547	12.144615
12.464829	880.801929	12.149632
12.941788	872.973510	12.154650
12.581321	861.998512	12.159667
12.578813	865.945878	12.164685
12.194374	880.458147	12.169703
12.473884	859.855764	12.174720
12.684546	863.590980	12.179738
12.335195	874.327861	12.184755
12.767686	871.104018	12.189773
12.635826	861.061659	12.194791
12.618840	870.377436	12.199808
12.655006	891.243534	12.204826
12.792061	890.524071	12.209843
12.839048	883.523589	12.214861
12.884682	895.779545	12.219879
12.355277	887.459323	12.224896
12.784115	902.197854	12.229914
12.466277	905.972495	12.234931
12.613984	890.069185	12.239949
12.803440	888.017981	12.244967
12.776343	876.648011	12.249984
12.944185	878.986342	12.255002
12.751976	889.009256	12.260019
12.964711	888.330521	12.265037
13.037691	893.883700	12.270055
12.748078	897.588337	12.275072
12.689936	895.339035	12.280090
12.696714	888.085125	12.285107
12.694237	881.151563	12.290125
12.493791	886.768029	12.295143
12.530861	892.243797	12.300160
12.838770	900.304443	12.305178
12.909646	901.717118	12.310195
12.947651	909.283042	12.315213
13.041409	933.061562	12.320231
13.261911	933.677862	12.325248
13.655085	892.846013	12.330266
13.088456	895.995304	12.335283
13.306235	894.365686	12.340301
13.297286	899.469927	12.345319
13.118741	880.823135	12.350336
13.506292	900.128224	12.355354
12.902342	894.824066	12.360371
12.842475	869.060899	12.365389
12.652905	889.104384	12.370407
12.862343	897.881612	12.375424
13.249225	889.841160	12.380442
12.725830	884.203994	12.385459
13.107586	882.973743	12.390477
13.044651	892.129060	12.395495
13.193638	912.840753	12.400512
13.343982	925.762226	12.405530
13.265623	925.785360	12.410547
13.551768	905.009030	12.415565
13.098691	895.744345	12.420583
12.957456	897.995208	12.425600
13.424979	907.332786	12.430618
13.459458	927.887286	12.435635
13.417859	913.317950	12.440653
13.168078	901.915683	12.445671
12.939973	899.732646	12.450688
13.177624	883.924490	12.455706
13.176034	914.521004	12.460723
13.223876	932.353827	12.465741
13.352311	943.420358	12.470759
13.429857	928.354670	12.475776
13.392144	912.039671	12.480794
13.477860	920.600705	12.485811
13.393858	933.953920	12.490829
13.357262	929.328138	12.495847
13.531141	912.963609	12.500864
13.430106	896.044485	12.505882
13.311619	930.740984	12.510899
13.662872	933.988636	12.515917
13.696296	916.313011	12.520935
13.493576	902.431361	12.525952
13.834424	912.842654	12.530970
13.443983	933.578374	12.535987
13.478431	929.006879	12.541005
13.581132	915.976974	12.546023
13.387095	916.659906	12.551040
13.704579	911.807650	12.556058
13.692681	925.840200	12.561075
13.863324	914.059769	12.566093
13.641969	896.867591	12.571111
13.396140	889.035605	12.576128
13.375381	892.596528	12.581146
13.390524	927.154923	12.586163
13.452172	915.147683	12.591181
13.621338	907.197909	12.596199
13.726656	908.044998	12.601216
13.716468	919.486888	12.606234
13.671613	926.418452	12.611251
13.642704	908.552892	12.616269
13.616827	910.309522	12.621287
13.288453	928.772080	12.626304
13.646278	905.812218	12.631322
13.318765	920.738336	12.636339
13.521492	932.992765	12.641357
13.458937	920.541795	12.646375
13.828967	919.557708	12.651392
14.140511	930.716873	12.656410
13.579943	948.259115	12.661427
13.956516	933.219087	12.666445
13.897256	926.607504	12.671463
13.548100	923.344258	12.676480
13.936226	946.241889	12.681498
13.874288	959.939029	12.686515
13.919980	943.112506	12.691533
14.241044	934.431696	12.696551
14.039832	941.523716	12.701568
14.064627	920.990107	12.706586
13.966765	910.734179	12.711603
13.774189	915.575243	12.716621
13.796796	930.539748	12.721639
14.095173	948.585159	12.726656
14.154326	946.412701	12.731674
13.971800	945.584375	12.736691
14.230422	947.074957	12.741709
14.106044	932.067725	12.746727
14.025971	919.073925	12.751744
13.937887	919.175911	12.756762
13.918212	933.839710	12.761779
14.057543	936.044510	12.766797
14.270400	942.512343	12.771815
13.962544	952.824714	12.776832
13.997104	930.241774	12.781850
14.099858	941.347578	12.786867
14.023947	950.405985	12.791885
13.991878	937.646596	12.796903
13.837146	938.361114	12.801920
14.314587	950.200473	12.806938
14.275163	941.256576	12.811955
14.265476	947.478976	12.816973
14.416777	946.841976	12.821991
14.087980	945.549068	12.827008
14.212728	939.262592	12.832026
13.980066	957.363394	12.837043
13.927920	944.116104	12.842061
13.830895	938.326984	12.847079
13.586197	958.733319	12.852096
13.816391	961.236513	12.857114
14.188713	969.524779	12.862131
14.177090	976.130975	12.867149
14.084733	974.739756	12.872167
13.692675	991.870145	12.877184
14.155358	970.947358	12.882202
14.406166	964.521369	12.887219
14.436134	995.416492	12.892237
14.573870	996.535226	12.897255
14.199513	985.887745	12.902272
14.409596	1008.028279	12.907290
14.682574	1011.347997	12.912307
14.688815	1003.951072	12.917325
14.736067	977.750441	12.922343
14.524833	985.688608	12.927360
14.670208	980.967501	12.932378
14.691160	971.037086	12.937395
14.579683	976.310226	12.942413
14.649385	974.405539	12.947431
14.600152	984.147769	12.952448
14.991654	986.000944	12.957466
14.694755	977.480678	12.962483
14.737818	977.063973	12.967501
14.528994	985.173844	12.972519
14.354964	985.173822	12.977536
14.623017	971.737901	12.982554
14.637473	971.012912	12.987571
14.531228	975.051544	12.992589
14.854081	963.661072	12.997607
14.461287	982.222014	13.002624
14.528749	989.765596	13.007642
14.465328	977.669947	13.012659
14.538916	991.543193	13.017677
14.987879	1006.386443	13.022695
14.876843	1024.056084	13.027712
15.201712	1001.646098	13.032730
14.983168	997.079489	13.037747
14.808348	983.938635	13.042765
15.184318	981.922919	13.047783
14.553071	975.591812	13.052800
14.677319	976.753708	13.057818
14.739605	999.466938	13.062835
14.911377	998.085009	13.067853
15.120467	1001.022001	13.072871
15.066925	1016.017942	13.077888
14.681067	996.347094	13.082906
15.133353	994.367474	13.087923
14.898308	1001.100146	13.092941
15.247547	1005.175792	13.097959
14.939645	994.207362	13.102976
14.789092	984.444123	13.107994
14.848658	999.808488	13.113011
15.095397	1011.339920	13.118029
15.300578	989.928419	13.123047
14.836172	998.140654	13.128064
15.113660	1009.601984	13.133082
15.033428	1004.816209	13.138099
14.922737	1020.369393	13.143117
15.136718	1019.399181	13.148135
14.943874	1008.713449	13.153152
15.125778	990.706093	13.158170
14.936486	1005.226872	13.163187
14.676615	1017.075036	13.168205
15.148445	1007.149524	13.173223
15.140464	1023.213361	13.178240
14.900140	1021.056827	13.183258
15.178678	1014.360259	13.188275
15.154940	999.174093	13.193293
15.137771	992.515772	13.198311
14.957046	1012.218549	13.203328
15.091276	1035.537309	13.208346
15.649983	1035.455562	13.213363
15.372947	1015.318763	13.218381
15.149031	1026.857256	13.223399
15.268880	1039.463571	13.228416
15.333291	1028.688548	13.233434
15.136461	1048.893933	13.238451
14.918158	1042.687621	13.243469
15.187409	1022.658914	13.248487
15.309014	1039.297390	13.253504
15.255320	1053.566435	13.258522
15.416792	1036.247075	13.263539
15.005578	1036.832862	13.268557
15.327397	1039.119108	13.273575
15.352517	1031.157256	13.278592
15.233165	1040.077852	13.283610
15.596651	1056.661912	13.288627
15.473972	1065.843048	13.293645
15.755084	1053.653603	13.298663
15.692137	1068.879268	13.303680
15.490913	1060.373354	13.308698
15.622094	1032.870203	13.313715
15.418688	1046.469765	13.318733
15.801618	1061.953057	13.323751
15.436455	1055.852287	13.328768
15.665133	1073.400632	13.333786
15.833585	1082.786854	13.338803
15.805734	1072.875950	13.343821
15.709101	1058.844967	13.348839
15.439847	1055.592793	13.353856
15.724966	1075.569002	13.358874
15.908842	1079.746681	13.363891
15.857473	1074.881526	13.368909
16.125335	1060.464306	13.373927
15.574557	1059.020814	13.378944
15.692181	1056.518581	13.383962
15.741984	1061.504238	13.388979
15.860502	1067.844245	13.393997
15.963952	1069.293471	13.399015
15.886573	1063.687822	13.404032
15.749309	1077.443074	13.409050
16.075296	1085.205531	13.414067
15.591925	1072.441099	13.419085
15.876867	1048.713832	13.424103
16.054805	1058.385112	13.429120
16.060871	1082.798379	13.434138
16.087612	1077.479381	13.439155
16.226591	1067.795181	13.444173
16.078366	1048.449645	13.449191
15.894577	1050.488326	13.454208
15.679056	1049.306480	13.459226
16.062304	1054.110687	13.464243
15.894651	1052.413183	13.469261
16.017015	1061.847549	13.474279
15.968464	1076.291017	13.479296
16.004526	1077.560678	13.484314
15.978009	1064.035298	13.489331
16.121116	1071.038303	13.494349
16.374522	1069.284206	13.499367
16.129657	1057.436928	13.504384
16.083489	1076.235709	13.509402
16.211840	1082.334689	13.514419
16.064929	1075.974967	13.519437
16.333325	1059.473826	13.524455
16.143937	1080.828819	13.529472
16.088292	1091.044598	13.534490
16.196097	1071.556750	13.539507
15.955929	1066.614359	13.544525
16.085208	1071.625164	13.549543
16.461384	1062.294192	13.554560
16.042593	1062.246351	13.559578
16.172189	1078.249750	13.564595
15.845224	1076.724794	13.569613
16.075886	1067.051027	13.574631
16.290537	1091.834070	13.579648
16.269327	1122.843787	13.584666
16.551671	1107.834314	13.589683
16.603794	1107.073377	13.594701
17.020888	1113.813560	13.599719
16.709566	1086.035491	13.604736
15.968170	1063.051776	13.609754
16.490322	1078.849790	13.614771
16.289992	1097.027775	13.619789
16.614828	1086.781189	13.624807
16.474913	1106.463100	13.629824
16.639028	1112.543684	13.634842
16.259007	1096.133714	13.639859
16.325302	1107.356463	13.644877
16.541196	1112.731812	13.649895
16.561329	1114.875647	13.654912
16.659340	1103.536790	13.659930
16.403268	1096.879428	13.664947
16.340504	1114.376202	13.669965
16.560540	1115.706092	13.674983
16.592053	1114.309347	13.680000
16.375207	1112.265821	13.685018
16.376056	1098.063022	13.690035
16.473932	1112.737579	13.695053
16.604183	1108.948133	13.700071
17.048907	1122.257240	13.705088
16.689748	1149.753160	13.710106
17.166229	1132.470099	13.715123
16.960261	1107.888954	13.720141
16.837715	1097.111911	13.725159
16.890461	1106.242828	13.730176
16.732399	1115.820099	13.735194
16.997332	1097.876634	13.740211
16.755808	1113.468089	13.745229
17.057603	1106.587072	13.750247
16.913422	1113.614544	13.755264
16.833850	1097.629019	13.760282
16.984527	1087.428137	13.765299
16.906168	1103.062188	13.770317
16.834085	1137.865140	13.775335
17.253595	1138.076311	13.780352
17.256959	1123.250194	13.785370
17.210779	1103.829472	13.790387
17.143352	1098.757467	13.795405
16.874643	1103.280544	13.800423
17.075256	1108.548306	13.805440
16.862028	1102.296064	13.810458
17.108312	1109.105111	13.815475
17.326242	1134.020128	13.820493
17.010792	1121.735853	13.825511
17.376497	1109.790786	13.830528
16.968688	1102.340980	13.835546
17.358878	1111.290086	13.840563
17.236593	1129.432187	13.845581
17.123037	1103.441236	13.850599
17.422693	1090.561465	13.855616
17.280547	1103.745740	13.860634
17.255872	1110.372060	13.865651
16.972829	1106.978685	13.870669
17.231515	1119.213094	13.875687
17.409070	1118.951283	13.880704
17.236269	1138.752913	13.885722
17.073101	1134.080974	13.890739
17.236501	1131.366687	13.895757
17.059677	1112.973498	13.900775
17.299190	1116.658548	13.905792
17.074771	1137.239187	13.910810
17.149042	1140.838978	13.915827
17.456900	1135.925758	13.920845
17.158300	1118.504028	13.925863
17.625898	1118.506022	13.930880
17.142805	1122.521259	13.935898
17.233241	1113.418828	13.940915
17.628670	1143.427879	13.945933
17.578372	1159.561067	13.950951
17.638894	1156.910123	13.955968
17.613788	1161.639850	13.960986
17.887722	1167.022749	13.966003
17.720963	1123.817762	13.971021
17.408467	1115.660340	13.976039
17.460616	1132.705575	13.981056
17.146003	1158.345486	13.986074
17.693544	1157.350158	13.991091
17.669638	1151.657411	13.996109
17.766257	1162.502740	14.001127
18.066378	1147.008420	14.006144
17.719548	1161.556363	14.011162
17.916107	1151.938363	14.016179
18.066979	1154.507144	14.021197
17.873633	1163.374996	14.026215
17.889992	1153.713661	14.031232
17.495544	1142.588012	14.036250
17.857572	1147.048201	14.041267
18.242514	1151.843992	14.046285
17.729716	1146.375603	14.051303
18.167018	1159.464468	14.056320
18.084521	1154.282167	14.061338
17.958322	1154.775005	14.066355
17.807361	1144.670671	14.071373
17.830589	1139.894817	14.076391
18.329053	1146.347127	14.081408
18.089173	1167.408985	14.086426
17.866293	1148.057751	14.091443
17.836845	1146.939123	14.096461
18.115302	1143.877357	14.101479
17.840461	1152.271780	14.106496
18.096564	1166.190300	14.111514
18.141058	1150.542498	14.116531
18.264534	1154.471284	14.121549
17.879686	1159.389266	14.126567
18.171866	1144.136458	14.131584
17.932031	1149.837856	14.136602
17.899069	1153.404989	14.141619
18.213614	1151.107346	14.146637
17.913122	1151.526550	14.151655
17.905222	1151.854697	14.156672
17.633306	1155.498612	14.161690
17.787099	1168.937016	14.166707
18.062945	1165.369107	14.171725
18.014543	1184.046470	14.176743
18.379495	1191.726281	14.181760
18.430878	1190.813924	14.186778
18.114808	1179.465701	14.191795
18.230314	1179.858179	14.196813
18.111327	1184.080129	14.201831
18.400875	1167.399829	14.206848
18.285295	1202.785174	14.211866
18.328623	1179.345013	14.216883
18.559263	1179.907003	14.221901
18.082111	1192.440978	14.226919
18.482296	1176.690877	14.231936
18.355709	1176.814775	14.236954
18.341092	1190.187054	14.241971
18.486425	1192.545292	14.246989
18.490241	1220.049647	14.252007
18.935609	1203.713451	14.257024
18.913558	1224.843894	14.262042
18.715161	1204.083071	14.267059
18.812682	1169.270553	14.272077
18.214349	1177.094680	14.277095
18.559791	1180.559830	14.282112
18.756046	1203.268543	14.287130
18.921744	1219.063219	14.292147
19.011668	1189.389073	14.297165
18.815932	1188.175509	14.302183
18.851006	1187.118737	14.307200
18.841841	1184.264788	14.312218
18.526121	1163.463580	14.317235
18.765396	1175.159739	14.322253
18.611080	1192.123536	14.327271
18.533532	1200.475346	14.332288
18.758840	1206.248093	14.337306
18.700854	1213.636474	14.342323
18.930867	1212.281114	14.347341
18.843485	1211.314933	14.352359
19.298216	1207.558437	14.357376
18.883763	1220.366257	14.362394
18.869681	1212.854089	14.367411
19.122703	1192.887473	14.372429
18.601117	1202.641968	14.377447
19.193982	1196.071683	14.382464
19.234094	1203.315139	14.387482
18.741532	1216.571488	14.392499
19.087061	1212.896997	14.397517
19.143554	1213.164615	14.402535
19.241115	1191.993275	14.407552
19.208069	1205.247579	14.412570
19.018626	1217.760402	14.417587
19.297209	1211.959689	14.422605
19.376057	1234.118595	14.427623
19.436687	1216.328804	14.432640
18.984232	1212.788737	14.437658
19.172210	1208.846258	14.442675
19.397159	1204.011268	14.447693
19.119854	1212.949505	14.452711
19.466613	1207.413052	14.457728
19.590942	1219.928443	14.462746
19.270417	1207.361639	14.467763
19.163817	1198.550317	14.472781
19.150142	1215.274513	14.477799
19.237923	1207.329473	14.482816
19.165905	1205.707072	14.487834
19.314928	1196.102410	14.492851
19.389684	1207.573971	14.497869
19.156130	1214.269786	14.502887
19.362232	1199.754203	14.507904
19.610236	1232.321633	14.512922
19.319487	1226.577602	14.517939
19.333080	1220.151051	14.522957
19.509929	1233.388997	14.527975
19.538853	1241.013659	14.532992
19.659372	1260.259221	14.538010
19.537091	1238.880995	14.543027
19.791975	1244.134915	14.548045
19.518815	1230.223279	14.553063
19.315983	1219.367018	14.558080
19.738197	1231.105118	14.563098
19.155942	1259.490655	14.568115
19.581647	1227.064734	14.573133
19.420042	1225.438340	14.578151
19.536780	1240.852049	14.583168
19.680976	1245.252716	14.588186
19.669240	1229.725122	14.593203
19.816359	1229.059774	14.598221
19.906372	1240.356241	14.603239
19.761358	1249.599038	14.608256
20.293693	1246.481227	14.613274
20.172013	1235.027136	14.618291
19.849013	1221.746037	14.623309
19.904519	1230.201436	14.628327
19.810043	1233.609010	14.633344
19.728281	1243.563620	14.638362
19.885143	1235.466238	14.643379
19.946353	1231.454762	14.648397
20.033667	1265.960174	14.653415
20.190982	1259.087220	14.658432
20.193174	1260.693616	14.663450
19.854780	1255.762180	14.668467
19.923607	1243.396003	14.673485
20.229260	1250.753143	14.678503
20.245395	1262.778398	14.683520
20.082848	1276.279799	14.688538
19.983162	1263.683835	14.693555
20.448098	1274.741249	14.698573
20.482087	1274.693567	14.703591
20.141358	1270.111839	14.708608
20.641171	1270.068657	14.713626
20.332165	1233.035522	14.718643
20.495462	1223.154534	14.723661
20.360317	1231.461954	14.728679
20.126242	1229.068488	14.733696
20.287033	1222.027102	14.738714
20.397098	1222.698269	14.743731
20.632424	1233.053713	14.748749
20.601238	1228.512753	14.753767
20.410702	1209.858882	14.758784
20.632532	1219.630565	14.763802
20.186106	1224.795891	14.768819
20.184227	1218.868235	14.773837
20.192801	1246.174556	14.778855
20.290842	1252.955716	14.783872
20.665107	1238.247288	14.788890
20.438910	1260.241338	14.793907
20.634680	1272.854783	14.798925
20.510450	1270.679323	14.803943
20.359982	1252.495340	14.808960
20.536811	1240.911129	14.813978
20.485250	1257.683060	14.818995
20.519879	1257.620512	14.824013
20.284348	1263.805378	14.829031
20.607735	1250.028456	14.834048
20.757074	1241.221458	14.839066
20.606259	1260.208485	14.844083
20.832279	1262.039545	14.849101
20.718744	1256.723493	14.854119
20.529760	1254.836526	14.859136
21.122358	1276.402252	14.864154
20.385145	1267.762504	14.869171
20.678759	1285.714930	14.874189
20.938488	1303.386921	14.879207
20.986438	1286.327517	14.884224
21.344743	1270.950396	14.889242
20.983549	1294.823354	14.894259
21.349482	1291.469217	14.899277
21.141418	1276.427652	14.904295
20.988588	1258.635398	14.909312
20.931600	1259.094071	14.914330
21.159755	1253.230235	14.919347
21.215067	1237.124857	14.924365
20.947339	1255.127007	14.929383
20.886513	1271.916917	14.934400
21.204954	1259.582591	14.939418
21.006159	1268.416865	14.944435
21.047267	1280.842735	14.949453
21.477005	1299.987360	14.954471
21.086038	1293.451786	14.959488
21.264654	1285.853913	14.964506
21.435443	1277.049549	14.969523
21.217874	1281.189414	14.974541
21.504011	1271.279240	14.979559
21.154733	1276.778939	14.984576
21.300823	1281.817047	14.989594
21.386955	1282.107617	14.994611
21.548126	1278.954011	14.999629
21.572851	1277.009388	15.004647
21.457510	1262.322212	15.009664
21.577124	1245.339573	15.014682
20.999360	1259.265198	15.019699
21.235936	1284.296347	15.024717
21.447093	1281.244396	15.029735
21.295050	1266.402197	15.034752
21.592872	1265.872340	15.039770
21.653434	1281.324795	15.044787
21.649822	1291.725273	15.049805
21.534763	1265.456801	15.054823
21.571335	1267.866578	15.059840
21.603186	1274.245004	15.064858
21.393988	1295.654246	15.069875
21.312019	1285.208575	15.074893
21.387875	1272.071216	15.079911
21.527189	1276.862174	15.084928
21.717092	1272.237434	15.089946
21.422675	1283.835495	15.094963
21.663338	1307.774727	15.099981
21.698967	1300.142320	15.104999
21.854559	1318.188343	15.110016
22.092553	1318.448897	15.115034
21.972382	1313.627410	15.120051
21.873251	1293.177644	15.125069
21.927964	1306.978132	15.130087
21.714582	1319.112405	15.135104
21.931551	1312.353556	15.140122
21.861391	1313.012787	15.145139
21.778009	1312.994242	15.150157
21.990890	1295.222693	15.155175
21.740302	1297.769868	15.160192
21.965449	1290.091486	15.165210
21.955036	1304.742203	15.170227
22.166089	1291.652548	15.175245
22.077240	1293.542827	15.180263
21.511657	1317.051263	15.185280
22.105862	1294.763996	15.190298
22.017632	1302.727166	15.195315
21.826751	1299.569740	15.200333
22.306144	1328.879909	15.205351
22.353267	1327.094926	15.210368
22.610291	1334.530599	15.215386
22.591158	1326.703928	15.220403
22.484130	1306.111192	15.225421
22.580891	1300.812133	15.230439
22.308217	1318.021855	15.235456
22.275754	1304.581969	15.240474
22.483761	1297.381797	15.245491
22.406749	1296.633335	15.250509
22.734345	1313.449143	15.255527
22.598903	1313.920487	15.260544
22.477330	1301.025325	15.265562
22.328581	1309.868277	15.270579
22.208116	1298.800364	15.275597
22.080192	1280.234364	15.280615
21.968545	1293.087263	15.285632
22.285938	1309.746719	15.290650
22.265621	1311.043626	15.295667
22.267848	1335.220484	15.300685
22.554272	1326.470589	15.305703
22.214817	1326.962559	15.310720
22.841917	1316.976135	15.315738
22.713548	1331.265846	15.320755
22.704532	1326.592582	15.325773
23.100045	1331.639184	15.330791
22.915025	1320.236825	15.335808
22.821039	1313.020522	15.340826
22.950226	1334.113134	15.345843
22.711284	1342.274025	15.350861
23.136401	1322.859574	15.355879
22.650213	1331.857982	15.360896
22.816262	1315.579731	15.365914
22.696420	1325.236329	15.370931
22.618165	1339.752850	15.375949
23.004297	1331.928385	15.380967
22.957322	1343.661741	15.385984
23.209123	1355.827416	15.391002
23.181177	1348.926092	15.396019
22.919625	1356.291993	15.401037
23.187298	1351.100273	15.406055
23.134201	1354.265657	15.411072
23.365733	1357.947165	15.416090
23.086158	1326.022926	15.421107
22.906074	1342.510845	15.426125
23.404134	1362.343899	15.431143
23.360046	1367.154664	15.436160
23.207158	1347.534092	15.441178
23.094692	1335.816455	15.446195
23.048073	1347.331106	15.451213
23.271272	1360.769329	15.456231
23.410786	1368.763978	15.461248
23.518603	1346.078774	15.466266
23.655262	1351.070247	15.471283
23.699651	1353.746598	15.476301
23.617589	1360.966431	15.481319
23.185560	1341.756083	15.486336
23.511511	1342.585729	15.491354
23.633476	1351.997413	15.496371
23.573118	1371.261885	15.501389
23.784352	1358.539186	15.506407
23.483136	1333.591418	15.511424
23.328375	1337.840084	15.516442
23.443778	1342.216508	15.521459
23.427120	1345.935877	15.526477
23.812425	1348.926476	15.531495
23.641594	1337.691995	15.536512
23.771966	1350.934575	15.541530
23.893866	1354.709083	15.546547
23.497544	1355.641257	15.551565
23.672109	1348.448457	15.556583
23.746600	1353.633135	15.561600
23.812022	1336.867963	15.566618
23.936901	1337.402761	15.571635
23.763574	1353.211877	15.576653
23.787405	1346.887002	15.581671
23.525478	1350.040152	15.586688
24.027143	1352.942839	15.591706
23.957317	1347.677196	15.596723
23.488348	1342.691243	15.601741
23.456335	1342.272273	15.606759
23.360411	1358.068406	15.611776
23.399213	1363.473797	15.616794
23.906855	1350.309005	15.621811
23.898965	1381.529397	15.626829
23.997447	1392.107024	15.631847
24.039559	1382.619202	15.636864
24.087621	1373.039773	15.641882
24.365192	1380.257259	15.646899
24.101438	1395.736854	15.651917
24.316170	1369.748177	15.656935
24.332527	1382.712547	15.661952
24.356996	1382.750178	15.666970
24.092229	1378.734178	15.671987
24.138231	1378.329769	15.677005
24.194845	1362.482155	15.682023
23.948195	1377.539414	15.687040
24.279419	1374.843404	15.692058
24.443845	1390.979828	15.697075
24.226061	1397.670754	15.702093
24.523764	1393.504336	15.707111
24.556971	1410.893779	15.712128
24.681914	1422.804154	15.717146
24.869931	1396.186525	15.722163
24.801157	1377.218301	15.727181
24.786109	1362.883367	15.732199
24.556826	1372.338838	15.737216
24.846703	1362.185622	15.742234
25.016756	1363.424703	15.747251
24.640392	1374.902251	15.752269
24.760422	1375.137428	15.757287
25.212399	1364.744185	15.762304
25.168693	1362.921070	15.767322
25.133260	1363.539139	15.772339
24.743744	1367.220150	15.777357
24.745006	1357.170916	15.782375
24.452828	1361.545521	15.787392
24.793550	1372.818862	15.792410
24.994972	1360.307184	15.797427
24.884768	1352.806993	15.802445
24.939705	1364.038794	15.807463
25.014607	1374.336217	15.812480
24.856668	1355.037754	15.817498
24.967733	1351.968184	15.822515
25.148624	1356.224564	15.827533
24.894760	1365.320790	15.832551
24.830156	1363.614783	15.837568
24.874420	1370.304511	15.842586
24.974998	1369.741315	15.847603
24.757558	1366.349144	15.852621
24.848445	1353.065662	15.857639
25.025229	1371.190806	15.862656
24.703788	1395.366534	15.867674
25.237634	1391.894982	15.872691
24.988471	1385.584501	15.877709
25.178579	1383.840436	15.882727
25.099487	1388.472191	15.887744
25.295824	1384.619702	15.892762
25.608208	1398.044598	15.897779
25.218781	1393.622912	15.902797
25.001563	1397.861448	15.907815
25.269177	1385.753678	15.912832
25.061836	1393.189951	15.917850
25.103100	1404.425516	15.922867
25.282654	1405.608909	15.927885
25.526751	1410.332507	15.932903
25.674452	1429.824522	15.937920
25.480769	1447.794095	15.942938
25.688588	1418.898564	15.947955
25.664772	1415.617268	15.952973
25.872583	1417.963052	15.957991
25.787636	1422.223329	15.963008
25.451994	1422.345955	15.968026
25.917165	1417.775662	15.973043
25.971507	1424.809438	15.978061
26.027902	1410.889230	15.983079
25.692715	1388.971007	15.988096
25.734284	1398.151474	15.993114
25.790628	1416.812697	15.998131
25.838349	1420.813309	16.003149
25.931032	1402.258826	16.008167
26.200354	1423.891762	16.013184
26.020104	1429.793704	16.018202
26.174265	1403.489953	16.023219
25.739396	1406.736344	16.028237
26.001061	1398.226077	16.033255
26.032822	1391.675612	16.038272
25.599834	1423.937771	16.043290
26.468454	1427.868860	16.048307
26.285686	1421.015130	16.053325
26.439029	1398.499844	16.058343
26.224897	1400.928339	16.063360
26.221195	1392.664439	16.068378
26.339147	1383.303520	16.073395
26.220584	1396.434849	16.078413
26.686902	1388.855215	16.083431
26.408609	1379.834616	16.088448
25.967241	1390.694911	16.093466
26.269240	1395.639986	16.098483
26.116780	1400.859329	16.103501
26.226614	1430.883864	16.108519
26.298975	1420.177413	16.113536
26.090928	1406.057460	16.118554
26.147144	1417.901450	16.123571
26.078700	1435.714911	16.128589
25.828024	1439.022386	16.133607
26.164909	1423.612144	16.138624
26.246770	1430.695202	16.143642
26.785044	1448.882723	16.148659
26.658369	1450.724756	16.153677
26.603062	1453.094640	16.158695
26.780762	1475.570951	16.163712
26.471174	1468.717492	16.168730
26.977672	1460.804484	16.173747
26.643524	1456.747873	16.178765
26.624442	1441.833248	16.183783
26.818167	1437.798442	16.188800
26.912646	1458.905622	16.193818
26.934065	1431.061116	16.198835
26.666120	1445.237513	16.203853
26.804916	1459.423170	16.208871
26.869852	1435.429268	16.213888
27.206079	1450.015756	16.218906
27.061564	1439.054645	16.223923
26.768698	1455.300554	16.228941
27.133433	1464.294419	16.233959
27.023758	1443.882604	16.238976
26.904019	1447.323526	16.243994
27.157026	1456.713030	16.249011
26.942313	1455.558571	16.254029
26.691745	1452.010572	16.259047
26.824757	1457.114370	16.264064
27.186302	1468.073878	16.269082
27.352686	1447.789924	16.274099
27.161434	1483.423507	16.279117
27.111062	1504.764285	16.284135
27.570110	1477.931981	16.289152
27.555009	1474.510778	16.294170
27.759623	1466.725883	16.299187
27.399368	1469.400731	16.304205
27.148195	1469.635650	16.309223
27.414107	1456.924204	16.314240
27.696370	1473.292662	16.319258
27.501522	1482.508310	16.324275
27.494131	1474.097764	16.329293
27.631979	1479.523435	16.334311
27.774024	1484.326997	16.339328
27.277804	1461.662124	16.344346
27.673990	1450.728656	16.349363
27.931729	1475.576938	16.354381
27.603815	1498.080055	16.359399
27.477890	1488.266961	16.364416
27.724553	1469.987573	16.369434
27.454493	1471.752932	16.374451
27.950335	1487.000132	16.379469
27.967266	1488.581189	16.384487
28.115536	1461.328326	16.389504
27.654079	1476.809577	16.394522
27.817083	1468.338010	16.399539
28.027095	1468.946324	16.404557
27.790384	1466.386167	16.409575
28.223049	1485.265245	16.414592
27.953596	1479.417130	16.419610
28.022926	1456.414080	16.424627
27.947497	1461.866427	16.429645
27.847961	1485.362364	16.434663
28.066912	1471.470444	16.439680
27.720908	1466.572473	16.444698
27.982977	1460.003897	16.449715
27.777788	1470.547723	16.454733
28.106090	1493.958608	16.459751
28.395678	1498.911770	16.464768
28.174178	1488.282369	16.469786
28.568155	1501.092235	16.474803
28.583387	1505.885565	16.479821
28.591283	1490.563963	16.484839
28.259547	1482.209962	16.489856
28.332883	1486.598103	16.494874
28.339380	1476.582859	16.499891
28.408194	1480.174087	16.504909
28.185469	1497.530150	16.509927
28.666554	1484.473350	16.514944
28.474685	1491.723001	16.519962
28.598881	1500.309196	16.524979
28.804481	1504.415896	16.529997
28.677050	1518.553594	16.535015
28.845061	1492.937310	16.540032
28.565942	1486.756709	16.545050
28.551931	1489.012908	16.550067
28.557429	1497.401343	16.555085
28.769804	1512.274933	16.560103
28.969340	1499.438917	16.565120
28.911552	1493.776243	16.570138
28.869219	1491.784321	16.575155
28.976808	1505.775517	16.580173
28.839905	1495.386801	16.585191
28.959337	1475.819664	16.590208
28.743155	1486.766213	16.595226
29.077499	1498.476038	16.600243
28.999631	1500.613292	16.605261
28.849927	1483.489993	16.610279
29.131561	1482.970774	16.615296
28.829311	1497.812979	16.620314
29.214830	1489.027035	16.625331
29.102131	1487.215011	16.630349
29.229769	1499.827897	16.635367
29.056876	1489.478392	16.640384
29.163502	1479.117637	16.645402
29.078307	1481.520411	16.650419
29.510199	1480.544273	16.655437
29.306147	1490.637041	16.660455
29.541630	1472.732053	16.665472
29.367561	1467.350258	16.670490
29.408433	1486.192332	16.675507
29.389881	1481.308241	16.680525
29.233932	1494.041197	16.685543
29.470022	1484.455621	16.690560
29.204970	1506.351841	16.695578
29.420371	1522.058419	16.700595
29.502945	1511.494379	16.705613
29.489638	1504.081328	16.710631
29.417061	1514.770950	16.715648
29.984951	1497.024835	16.720666
29.543725	1512.436159	16.725683
30.028963	1495.960712	16.730701
29.823513	1513.907805	16.735719
29.965060	1517.555019	16.740736
29.819132	1512.555088	16.745754
30.050774	1491.865792	16.750771
30.088913	1497.004469	16.755789
29.854054	1515.533363	16.760807
30.139638	1521.460210	16.765824
29.715543	1511.870842	16.770842
30.160395	1508.787905	16.775859
30.069634	1513.249518	16.780877
29.737800	1504.721346	16.785895
30.134481	1515.352713	16.790912
30.033391	1511.246947	16.795930
30.003160	1491.873972	16.800947
30.084939	1506.413900	16.805965
30.065988	1511.375443	16.810983
30.046947	1505.638759	16.816000
30.022852	1494.494457	16.821018
30.008940	1520.182407	16.826035
30.232968	1533.017333	16.831053
30.316999	1539.365794	16.836071
30.280899	1518.685673	16.841088
30.370607	1522.168462	16.846106
30.339785	1547.347061	16.851123
30.599147	1529.909021	16.856141
30.525852	1532.127297	16.861159
30.292551	1520.890606	16.866176
30.463855	1544.141823	16.871194
30.270281	1552.697407	16.876211
30.519147	1528.536774	16.881229
30.486902	1529.740120	16.886247
30.607657	1527.927595	16.891264
30.906775	1549.676823	16.896282
30.760483	1555.106373	16.901299
30.720750	1530.689752	16.906317
30.550858	1529.811973	16.911335
30.571980	1538.746449	16.916352
30.687797	1532.624261	16.921370
30.417247	1534.805463	16.926387
30.794522	1531.822153	16.931405
30.648674	1556.654008	16.936423
30.867118	1563.929669	16.941440
30.964557	1564.304282	16.946458
31.064050	1569.532431	16.951475
31.199631	1566.607258	16.956493
31.230132	1558.781123	16.961511
31.363185	1544.708294	16.966528
31.203500	1562.143857	16.971546
31.089485	1576.027378	16.976563
31.514876	1552.086204	16.981581
31.226406	1545.726553	16.986599
31.377850	1559.555763	16.991616
31.174314	1562.171173	16.996634
31.117907	1556.327775	17.001651
31.273146	1566.318710	17.006669
31.244615	1566.036923	17.011687
31.242639	1544.323791	17.016704
31.256949	1549.874997	17.021722
31.027618	1555.884485	17.026739
31.427111	1551.106352	17.031757
31.199617	1564.529487	17.036775
31.157814	1555.358902	17.041792
31.667904	1569.430561	17.046810
31.818327	1593.411132	17.051827
31.837692	1584.931157	17.056845
31.756045	1575.583325	17.061863
32.117899	1568.884360	17.066880
31.703027	1561.884906	17.071898
31.432836	1561.606545	17.076915
31.999037	1570.648168	17.081933
31.886895	1580.099761	17.086951
32.041432	1579.046936	17.091968
31.998376	1585.158402	17.096986
31.815782	1590.459347	17.102003
31.963146	1572.549516	17.107021
31.750583	1570.358794	17.112039
31.876557	1599.516907	17.117056
32.000091	1578.837190	17.122074
32.224638	1582.285411	17.127091
32.249267	1583.674596	17.132109
32.357321	1587.405200	17.137127
32.319461	1580.864881	17.142144
32.380761	1580.547880	17.147162
32.162356	1587.207895	17.152179
32.264074	1583.011030	17.157197
32.280857	1574.938290	17.162215
31.887904	1574.241529	17.167232
32.268656	1588.620049	17.172250
31.986808	1584.972487	17.177267
32.294736	1567.565051	17.182285
32.375213	1575.156858	17.187303
32.526914	1586.367617	17.192320
32.340571	1580.140158	17.197338
32.098508	1593.009840	17.202355
32.580011	1604.192289	17.207373
32.549569	1597.883954	17.212391
32.610612	1602.736659	17.217408
32.528972	1606.760664	17.222426
32.455855	1624.960272	17.227443
32.780531	1606.716343	17.232461
32.425218	1598.062007	17.237479
32.569014	1608.503780	17.242496
32.577022	1607.990313	17.247514
32.603682	1608.215339	17.252531
32.709250	1622.723106	17.257549
32.299333	1614.267901	17.262567
32.807653	1620.829688	17.267584
32.908319	1641.808270	17.272602
32.627757	1640.352638	17.277619
33.177005	1652.780158	17.282637
33.147304	1638.019427	17.287655
33.056918	1648.922376	17.292672
33.130719	1624.884792	17.297690
33.184681	1631.542624	17.302707
33.496870	1644.011181	17.307725
33.860255	1631.810832	17.312743
33.204430	1631.381378	17.317760
33.779834	1637.960034	17.322778
33.786555	1631.110519	17.327795
33.843075	1612.542371	17.332813
33.621689	1611.926978	17.337831
33.527416	1593.027352	17.342848
33.753427	1575.140735	17.347866
33.624171	1595.224869	17.352883
33.551432	1610.619289	17.357901
33.754950	1603.231666	17.362919
33.720614	1591.669488	17.367936
33.936687	1585.652930	17.372954
33.571640	1598.436958	17.377971
33.588251	1600.503212	17.382989
33.826123	1580.898460	17.388007
33.586125	1600.514982	17.393024
33.833345	1601.799685	17.398042
33.799660	1597.217502	17.403059
33.691519	1576.067913	17.408077
33.515316	1590.482774	17.413095
33.714717	1624.067811	17.418112
33.821977	1623.904499	17.423130
33.520707	1624.822752	17.428147
33.737598	1624.259121	17.433165
34.052224	1617.741230	17.438183
33.787930	1633.697726	17.443200
33.930336	1634.456363	17.448218
33.918727	1641.358647	17.453235
33.529793	1633.929766	17.458253
34.070988	1655.057670	17.463271
34.079848	1665.681687	17.468288
34.259469	1663.272338	17.473306
33.918781	1661.136134	17.478323
34.400678	1666.949906	17.483341
34.632494	1662.575549	17.488359
34.401872	1664.480051	17.493376
34.481294	1655.188903	17.498394
34.377695	1640.221431	17.503411
34.293299	1663.717501	17.508429
34.606320	1663.138378	17.513447
34.654105	1665.772007	17.518464
34.766695	1660.720845	17.523482
34.516460	1669.395283	17.528499
34.787728	1664.839246	17.533517
34.832098	1676.471758	17.538535
34.867931	1695.621452	17.543552
35.145629	1694.387671	17.548570
34.783649	1658.544592	17.553587
34.803388	1652.046780	17.558605
35.086068	1680.232402	17.563623
34.793976	1687.954222	17.568640
35.172129	1666.766267	17.573658
34.811416	1659.595253	17.578675
35.208032	1674.485200	17.583693
35.478521	1683.538756	17.588711
35.353618	1682.365797	17.593728
35.322890	1659.919218	17.598746
35.172740	1648.881049	17.603763
35.022242	1648.567162	17.608781
35.156600	1647.181223	17.613799
34.911292	1656.357194	17.618816
35.191952	1669.437153	17.623834
35.292784	1681.882510	17.628851
35.457155	1680.593457	17.633869
35.556090	1679.659634	17.638887
35.537877	1694.655936	17.643904
35.723717	1673.903309	17.648922
35.393027	1682.425728	17.653939
35.477459	1695.182797	17.658957
35.371930	1686.962232	17.663975
35.296332	1683.743065	17.668992
35.524522	1675.943049	17.674010
35.714938	1690.321234	17.679027
35.542393	1687.401394	17.684045
35.401126	1681.705211	17.689063
35.733784	1673.682857	17.694080
36.034132	1678.287424	17.699098
35.934637	1692.792243	17.704115
35.762090	1689.874469	17.709133
35.974559	1676.576323	17.714151
35.853545	1680.345688	17.719168
35.654745	1686.931656	17.724186
36.053528	1695.992754	17.729203
35.981912	1699.168452	17.734221
35.953448	1701.334177	17.739239
35.762739	1686.418447	17.744256
36.182188	1676.915126	17.749274
36.041133	1694.479327	17.754291
36.049183	1697.088727	17.759309
36.457163	1695.402995	17.764327
36.180998	1691.099977	17.769344
36.234133	1691.364813	17.774362
36.438815	1696.876938	17.779379
36.339408	1697.545643	17.784397
36.765954	1698.323851	17.789415
36.277753	1698.204224	17.794432
36.395247	1694.965447	17.799450
36.537461	1686.775779	17.804467
36.403403	1700.748338	17.809485
36.800765	1722.162843	17.814503
36.569415	1739.505648	17.819520
36.836333	1723.380143	17.824538
36.942282	1706.085636	17.829555
36.732075	1715.292349	17.834573
36.714954	1733.733667	17.839591
36.700943	1733.121198	17.844608
36.751634	1719.243771	17.849626
37.016077	1709.736325	17.854643
37.271328	1723.079334	17.859661
37.450584	1711.668445	17.864679
37.025303	1716.277305	17.869696
37.098645	1732.771000	17.874714
37.330355	1717.410711	17.879731
37.366447	1703.663538	17.884749
37.411018	1706.707463	17.889767
37.351086	1714.486189	17.894784
37.094624	1693.712056	17.899802
37.122774	1679.889855	17.904819
37.254845	1706.508717	17.909837
37.286821	1703.460707	17.914855
37.427764	1701.341642	17.919872
37.398979	1700.488457	17.924890
37.651327	1697.835833	17.929907
37.561368	1709.682162	17.934925
37.419944	1710.275544	17.939943
37.672412	1702.979074	17.944960
37.201506	1706.926023	17.949978
37.359436	1705.518372	17.954995
37.310432	1720.003556	17.960013
37.551110	1710.813949	17.965031
37.695278	1704.446408	17.970048
37.439181	1707.656726	17.975066
37.386683	1716.600027	17.980083
37.638828	1726.364565	17.985101
37.900423	1719.900070	17.990119
37.859415	1740.115746	17.995136
37.657564	1731.561638	18.000154
38.143405	1717.075407	18.005171
37.845353	1736.369776	18.010189
38.266575	1740.441796	18.015207
37.795726	1734.419129	18.020224
37.927551	1715.840774	18.025242
38.081589	1727.661656	18.030259
38.201452	1746.010977	18.035277
38.096310	1746.762406	18.040295
38.241064	1757.672629	18.045312
38.713062	1744.404162	18.050330
38.603051	1745.202646	18.055347
38.589559	1755.596117	18.060365
38.466976	1741.981309	18.065383
38.413028	1717.110632	18.070400
38.156851	1720.440626	18.075418
38.679454	1758.607425	18.080435
38.518084	1773.168401	18.085453
38.436096	1771.661146	18.090471
38.613345	1750.227296	18.095488
38.913585	1747.672338	18.100506
38.897204	1763.716716	18.105523
38.820390	1771.897884	18.110541
38.811831	1755.058769	18.115559
38.946162	1751.486065	18.120576
38.682174	1764.738473	18.125594
38.842382	1746.816476	18.130611
38.709878	1767.992096	18.135629
38.718939	1769.707231	18.140647
39.099464	1748.125151	18.145664
39.009361	1744.891541	18.150682
39.005414	1753.568822	18.155699
39.036511	1775.434398	18.160717
39.325291	1798.212056	18.165735
39.415607	1782.616260	18.170752
39.574478	1775.006451	18.175770
39.742305	1787.607718	18.180787
39.470217	1778.075626	18.185805
39.449911	1752.263891	18.190823
39.417780	1753.930134	18.195840
39.247813	1759.527316	18.200858
39.886738	1755.937456	18.205875
39.564906	1767.917205	18.210893
39.433521	1778.791891	18.215911
39.549857	1780.179619	18.220928
39.503064	1767.412425	18.225946
39.825640	1778.501112	18.230963
39.581312	1795.105919	18.235981
39.829244	1778.116050	18.240999
39.890390	1785.685079	18.246016
39.841059	1785.686491	18.251034
39.918018	1774.394900	18.256051
39.642997	1770.898101	18.261069
39.884941	1777.640758	18.266087
40.007230	1790.723276	18.271104
39.723034	1786.787330	18.276122
39.993367	1786.209353	18.281139
39.950719	1801.898242	18.286157
39.846367	1779.780617	18.291175
40.047288	1805.021030	18.296192
40.218830	1806.575783	18.301210
40.590684	1798.455962	18.306227
40.364690	1817.872947	18.311245
40.410700	1805.353327	18.316263
40.421128	1802.447905	18.321280
40.424212	1812.582329	18.326298
40.698419	1802.311357	18.331315
40.277949	1805.354605	18.336333
40.267232	1809.630867	18.341351
40.475300	1815.437200	18.346368
40.365517	1802.504437	18.351386
40.376626	1805.259483	18.356403
40.320074	1818.751521	18.361421
40.611033	1814.010629	18.366439
41.012253	1815.255634	18.371456
41.079396	1824.573736	18.376474
41.210540	1824.559299	18.381491
40.910990	1813.609367	18.386509
40.965831	1794.081625	18.391527
40.780750	1800.586749	18.396544
40.597026	1831.486692	18.401562
40.879688	1820.197289	18.406579
40.941708	1842.377374	18.411597
40.799974	1826.227477	18.416615
41.226918	1829.606095	18.421632
41.073077	1830.843138	18.426650
41.542635	1829.570656	18.431667
41.234884	1834.551096	18.436685
41.318998	1830.266637	18.441703
41.588020	1814.787312	18.446720
41.412231	1838.762047	18.451738
41.454159	1832.746419	18.456755
41.170537	1831.124968	18.461773
41.488776	1835.086792	18.466791
41.624312	1846.263904	18.471808
41.566677	1862.671333	18.476826
42.112329	1874.217618	18.481843
41.799006	1861.507182	18.486861
41.586851	1867.921452	18.491879
42.152451	1855.617840	18.496896
42.196519	1861.975499	18.501914
42.159554	1855.029876	18.506931
41.778614	1860.635978	18.511949
42.110576	1845.401585	18.516967
41.935419	1842.922414	18.521984
41.822534	1843.930293	18.527002
42.029423	1852.482848	18.532019
42.220191	1860.604988	18.537037
42.124856	1852.229628	18.542055
42.111243	1868.859075	18.547072
42.058792	1860.839152	18.552090
42.083062	1849.390299	18.557107
41.931237	1856.496229	18.562125
41.955096	1867.978369	18.567143
42.450975	1878.774566	18.572160
42.290417	1880.307842	18.577178
42.579841	1877.260456	18.582195
42.588920	1880.861650	18.587213
42.530403	1879.482665	18.592231
42.715672	1879.365799	18.597248
42.494769	1889.471846	18.602266
42.640262	1876.960429	18.607283
42.689877	1880.329574	18.612301
42.937506	1877.510606	18.617319
42.893858	1867.625317	18.622336
42.798720	1872.017299	18.627354
43.055988	1869.252635	18.632371
43.001396	1870.849781	18.637389
42.729780	1876.845520	18.642407
42.782868	1885.152104	18.647424
42.817793	1871.263269	18.652442
43.113679	1885.197029	18.657459
43.150083	1914.321931	18.662477
42.757333	1918.058712	18.667495
43.337466	1903.501225	18.672512
43.239505	1898.466573	18.677530
43.141401	1896.834729	18.682547
43.187904	1905.557982	18.687565
43.568997	1907.668950	18.692583
43.345725	1897.143080	18.697600
43.387148	1888.705149	18.702618
43.795516	1902.075857	18.707635
43.523629	1911.349562	18.712653
43.422670	1894.922533	18.717671
43.584046	1903.281987	18.722688
43.459174	1901.415243	18.727706
43.388080	1911.443410	18.732723
43.767020	1912.355064	18.737741
43.970513	1925.101605	18.742759
43.740521	1929.536552	18.747776
43.971058	1923.614599	18.752794
44.119838	1921.421585	18.757811
44.015579	1938.358057	18.762829
43.906099	1930.061257	18.767847
44.298745	1897.460580	18.772864
44.152376	1921.472208	18.777882
44.326373	1920.589045	18.782899
44.356734	1935.286668	18.787917
43.991664	1936.598183	18.792935
44.309839	1935.884661	18.797952
44.481615	1939.961545	18.802970
44.228893	1920.832332	18.807987
44.469092	1916.845027	18.813005
44.456033	1939.965925	18.818023
44.728127	1958.721070	18.823040
44.202411	1943.064439	18.828058
44.382564	1960.899131	18.833075
44.793175	1969.917599	18.838093
44.685136	1961.985829	18.843111
44.931050	1951.888397	18.848128
44.888727	1946.368937	18.853146
44.956669	1942.368070	18.858163
45.212714	1935.724810	18.863181
44.924363	1952.094490	18.868199
45.049761	1955.053468	18.873216
44.738356	1942.615726	18.878234
44.910859	1943.678992	18.883251
45.209572	1940.267529	18.888269
45.175412	1961.259677	18.893287
45.624913	1940.359302	18.898304
45.071128	1956.072686	18.903322
45.107189	1951.298591	18.908339
45.190529	1934.802588	18.913357
44.960200	1945.163724	18.918375
45.286104	1965.250281	18.923392
45.241465	1979.173578	18.928410
45.201888	1972.998660	18.933427
45.577884	1958.299985	18.938445
45.390080	1965.417027	18.943463
45.508743	1975.075460	18.948480
45.634641	1985.564732	18.953498
45.443067	1971.305634	18.958515
45.772048	1964.740253	18.963533
45.454800	1980.273951	18.968551
46.090843	1991.604836	18.973568
46.124650	1998.851483	18.978586
46.246512	2000.158018	18.983603
45.936019	1979.959641	18.988621
45.908928	1980.680864	18.993639
46.253714	1998.294042	18.998656
46.176926	2002.925011	19.003674
46.160578	2003.620842	19.008691
46.429658	2008.782345	19.013709
46.302542	1997.246313	19.018727
46.765532	1991.605449	19.023744
46.667965	1982.146930	19.028762
46.081843	1975.143305	19.033779
46.363941	1979.382152	19.038797
46.519897	1973.649931	19.043815
46.950785	1973.307079	19.048832
46.793240	2004.050711	19.053850
46.919429	2002.307594	19.058867
46.873060	1968.178923	19.063885
46.400816	1974.431628	19.068903
46.898470	1980.647074	19.073920
46.507449	1982.070636	19.078938
46.502662	1993.614876	19.083955
46.676386	2013.227229	19.088973
46.813027	1989.273061	19.093991
46.936428	1974.546045	19.099008
46.699091	1993.289861	19.104026
46.878443	2003.101047	19.109043
47.217024	1997.930163	19.114061
47.388615	2015.676095	19.119079
47.333854	2026.769354	19.124096
47.549309	2009.606480	19.129114
47.451833	2013.393292	19.134131
47.277614	2022.233384	19.139149
47.507933	2009.000395	19.144167
47.507237	2014.983302	19.149184
47.671575	2030.015011	19.154202
47.562729	2015.335289	19.159219
47.643776	2007.415451	19.164237
47.847365	2029.585403	19.169255
48.031559	2021.862154	19.174272
47.812525	2005.862216	19.179290
47.635927	2009.700678	19.184307
47.984845	2015.003785	19.189325
47.633324	2026.368775	19.194343
47.949235	2001.370587	19.199360
47.677186	1992.713780	19.204378
47.889214	2015.163661	19.209395
47.976366	2020.302583	19.214413
47.693298	2009.855893	19.219431
48.072810	2010.234882	19.224448
48.104173	2041.581211	19.229466
48.204230	2053.939022	19.234483
48.103275	2044.511924	19.239501
48.161011	2045.779266	19.244519
48.888073	2045.104748	19.249536
48.728470	2036.576454	19.254554
48.368271	2041.648682	19.259571
48.790137	2048.289102	19.264589
48.527653	2045.217157	19.269607
48.516055	2041.902512	19.274624
48.527339	2029.734151	19.279642
48.282315	2041.637947	19.284659
48.344692	2047.026793	19.289677
48.404570	2038.993726	19.294695
48.794078	2065.979652	19.299712
48.855055	2070.302987	19.304730
48.829896	2054.711039	19.309747
49.187107	2053.506801	19.314765
48.518349	2072.900736	19.319783
48.993179	2075.462589	19.324800
49.271100	2055.761752	19.329818
49.065854	2068.266070	19.334835
49.196529	2057.180119	19.339853
49.021215	2061.301695	19.344871
49.482728	2071.295097	19.349888
49.276868	2076.762228	19.354906
49.194289	2085.703826	19.359923
49.714254	2079.798345	19.364941
49.777421	2102.158308	19.369959
49.966167	2104.114311	19.374976
50.112754	2076.250803	19.379994
49.811084	2066.894941	19.385011
49.764454	2059.292478	19.390029
49.658525	2053.577622	19.395047
49.892447	2065.166904	19.400064
50.112855	2052.932871	19.405082
50.274910	2067.922385	19.410099
50.463107	2069.754382	19.415117
50.201524	2066.269760	19.420135
50.112190	2053.574996	19.425152
50.124519	2036.635779	19.430170
49.808331	2038.121966	19.435187
50.024943	2078.489140	19.440205
50.044376	2089.030715	19.445223
50.040779	2064.670547	19.450240
50.205547	2079.372668	19.455258
50.022409	2086.742984	19.460275
50.200358	2068.089959	19.465293
50.349557	2083.117727	19.470311
50.679525	2089.094243	19.475328
50.666005	2096.660511	19.480346
50.659626	2116.352452	19.485363
50.728831	2104.067787	19.490381
50.596159	2108.913103	19.495399
50.613251	2118.539797	19.500416
50.950713	2097.865657	19.505434
50.737694	2107.801875	19.510451
50.935696	2109.759793	19.515469
51.033454	2113.492228	19.520487
50.740757	2100.099173	19.525504
51.113819	2111.217252	19.530522
50.740219	2145.190682	19.535539
51.516060	2129.903326	19.540557
51.932535	2126.877409	19.545575
52.152159	2116.791496	19.550592
52.036628	2086.740089	19.555610
51.747593	2085.005646	19.560627
51.819466	2093.537938	19.565645
52.047821	2103.050495	19.570663
51.547727	2097.298510	19.575680
51.871958	2074.682845	19.580698
52.167852	2076.200940	19.585715
52.231728	2073.584317	19.590733
51.992064	2083.096358	19.595751
51.967360	2089.758927	19.600768
51.956208	2089.275180	19.605786
51.905730	2084.316168	19.610803
51.970343	2068.472701	19.615821
52.059123	2065.093540	19.620839
52.114788	2083.523153	19.625856
52.369982	2089.659242	19.630874
52.046634	2080.315713	19.635891
52.140005	2087.190321	19.640909
52.432120	2072.442615	19.645927
51.843140	2077.070070	19.650944
52.135009	2084.047088	19.655962
52.219736	2071.192566	19.660979
52.236132	2071.037868	19.665997
52.017035	2098.149612	19.671015
51.868681	2110.181360	19.676032
52.416018	2108.072236	19.681050
52.569302	2121.375268	19.686067
52.430560	2109.599383	19.691085
52.272903	2130.625652	19.696103
52.434659	2153.402392	19.701120
52.764572	2141.940604	19.706138
52.790153	2142.210493	19.711155
52.783305	2141.898936	19.716173
52.802009	2135.377866	19.721191
52.881093	2157.526163	19.726208
53.069382	2185.040442	19.731226
53.273855	2166.997866	19.736243
53.411472	2155.278328	19.741261
53.362698	2168.771062	19.746279
53.438526	2160.476188	19.751296
53.921834	2169.974605	19.756314
53.570061	2175.329488	19.761331
53.750414	2154.313779	19.766349
54.014187	2167.851600	19.771367
53.804421	2175.085636	19.776384
54.075371	2165.001739	19.781402
53.960697	2162.013888	19.786419
53.802481	2143.727880	19.791437
53.846050	2141.284945	19.796455
53.501773	2157.911382	19.801472
53.601486	2151.671749	19.806490
53.726769	2156.728445	19.811507
53.534035	2165.565086	19.816525
53.861480	2161.669975	19.821543
54.221754	2187.393946	19.826560
54.794983	2190.368324	19.831578
54.538520	2183.894966	19.836595
54.401143	2178.016294	19.841613
54.334958	2166.894990	19.846631
54.259948	2168.826585	19.851648
54.240129	2196.454099	19.856666
54.187455	2197.052022	19.861683
54.063809	2181.842395	19.866701
54.299521	2194.553527	19.871719
54.333873	2189.502918	19.876736
54.661791	2201.786490	19.881754
54.596988	2226.497098	19.886771
54.775481	2237.304960	19.891789
54.864256	2217.361793	19.896807
54.646582	2211.716318	19.901824
55.118383	2223.356554	19.906842
54.817756	2226.428397	19.911859
55.322850	2218.860059	19.916877
55.317123	2225.454010	19.921895
55.178116	2225.549263	19.926912
55.479036	2232.208372	19.931930
55.328500	2235.430681	19.936947
55.361109	2242.583168	19.941965
55.562548	2255.595141	19.946983
55.515984	2230.041917	19.952000
55.923402	2235.018166	19.957018
55.932594	2243.547811	19.962035
55.816278	2236.352869	19.967053
55.548554	2242.158669	19.972071
55.596515	2251.865666	19.977088
55.983981	2231.615294	19.982106
55.838426	2225.696032	19.987123
55.979995	2235.081009	19.992141
56.004645	2230.389605	19.997159
55.819439	2239.608639	20.002176
55.835068	2239.980059	20.007194
55.883995	2237.706174	20.012211
55.750925	2228.486301	20.017229
56.051892	2253.242399	20.022247
56.230997	2261.212474	20.027264
56.525011	2272.919422	20.032282
56.395355	2278.288220	20.037299
56.269926	2273.745204	20.042317
56.516518	2260.734074	20.047335
56.342552	2263.438794	20.052352
56.639270	2279.974401	20.057370
56.408652	2282.145467	20.062387
56.816337	2276.201192	20.067405
56.972529	2288.610537	20.072423
56.988322	2292.557509	20.077440
57.099238	2307.274947	20.082458
57.022184	2303.377362	20.087475
57.038827	2282.132373	20.092493
57.337520	2293.446308	20.097511
57.074778	2316.878179	20.102528
57.488271	2287.476438	20.107546
57.475249	2298.748397	20.112563
57.118855	2301.851513	20.117581
57.616912	2280.414003	20.122599
57.244538	2301.353762	20.127616
57.497143	2294.850952	20.132634
57.440515	2278.490288	20.137651
57.476382	2302.061345	20.142669
57.871854	2293.271922	20.147687
57.506093	2272.637680	20.152704
57.768005	2289.643538	20.157722
57.936844	2318.907434	20.162739
57.948814	2316.853487	20.167757
58.427129	2322.144471	20.172775
58.091891	2335.897644	20.177792
58.360172	2313.613360	20.182810
58.272377	2325.353131	20.187827
58.173781	2330.509762	20.192845
58.645567	2328.800628	20.197863
58.598485	2317.419015	20.202880
58.578704	2321.403167	20.207898
58.680609	2303.878870	20.212915
58.472450	2301.656807	20.217933
58.522975	2313.535692	20.222951
58.762530	2310.872975	20.227968
58.640064	2312.674854	20.232986
58.476600	2298.508821	20.238003
58.392479	2315.836410	20.243021
58.698175	2326.104110	20.248039
58.447854	2331.350763	20.253056
58.572887	2312.250258	20.258074
59.050536	2325.246565	20.263091
58.714630	2345.745587	20.268109
59.262143	2343.723201	20.273127
58.991871	2340.950858	20.278144
58.912173	2329.265621	20.283162
58.802925	2349.923423	20.288179
58.936163	2351.537999	20.293197
59.198797	2362.353499	20.298215
59.644382	2379.313557	20.303232
59.836421	2361.955373	20.308250
59.794806	2359.818360	20.313267
59.648056	2370.046503	20.318285
59.908160	2376.090376	20.323303
59.709361	2370.202392	20.328320
59.742486	2364.143825	20.333338
59.806691	2362.946256	20.338355
59.829791	2378.133120	20.343373
59.611556	2372.052710	20.348391
59.922494	2367.370444	20.353408
59.875106	2358.044224	20.358426
60.105925	2373.081817	20.363443
60.020087	2405.440220	20.368461
60.451339	2388.662063	20.373479
60.486123	2383.595966	20.378496
60.491782	2403.854994	20.383514
60.418139	2396.061977	20.388531
60.366714	2404.644733	20.393549
60.892285	2395.398391	20.398567
60.249843	2391.103541	20.403584
60.360701	2396.350564	20.408602
60.832893	2381.925110	20.413619
60.488711	2392.648612	20.418637
61.197588	2407.177982	20.423655
61.060495	2399.584590	20.428672
60.968481	2384.567437	20.433690
61.252042	2408.619690	20.438707
61.010635	2434.458851	20.443725
61.219751	2435.848530	20.448743
61.364051	2432.816751	20.453760
61.190090	2412.240377	20.458778
61.701537	2411.967166	20.463795
61.437260	2437.396792	20.468813
61.623692	2421.524074	20.473831
61.469615	2436.159066	20.478848
61.766224	2426.100282	20.483866
61.483513	2397.867338	20.488883
61.831055	2405.935028	20.493901
62.300244	2408.815931	20.498919
61.728738	2417.830641	20.503936
62.021278	2411.070043	20.508954
62.090319	2391.071161	20.513971
61.689094	2398.021634	20.518989
62.154049	2410.821915	20.524007
61.770204	2416.299091	20.529024
62.252251	2412.764923	20.534042
62.512177	2411.116966	20.539059
62.052540	2440.593393	20.544077
62.630307	2427.806487	20.549095
62.268879	2434.057795	20.554112
62.477688	2426.991982	20.559130
62.618559	2414.813809	20.564147
62.304502	2432.159842	20.569165
62.315601	2414.216045	20.574183
62.472600	2455.370610	20.579200
62.286037	2465.041703	20.584218
62.587167	2463.752819	20.589235
62.653381	2457.600770	20.594253
63.095078	2453.055311	20.599271
62.985032	2479.061590	20.604288
63.062662	2494.496998	20.609306
63.380971	2486.306543	20.614323
63.277412	2491.646894	20.619341
63.534326	2485.322398	20.624359
63.471714	2471.651272	20.629376
63.192329	2485.225690	20.634394
63.654502	2496.830035	20.639411
63.490333	2488.186710	20.644429
63.556035	2464.960637	20.649447
63.600702	2473.606871	20.654464
63.703553	2491.307438	20.659482
63.898813	2485.012419	20.664499
63.619749	2463.358830	20.669517
63.714127	2480.191433	20.674535
63.981143	2509.239894	20.679552
63.965438	2503.860300	20.684570
64.152067	2514.785499	20.689587
64.140250	2519.132898	20.694605
64.046484	2501.984947	20.699623
64.361066	2505.180939	20.704640
63.916647	2516.372397	20.709658
64.185933	2515.844954	20.714675
64.378020	2526.470290	20.719693
64.531818	2536.462688	20.724711
64.497203	2536.147641	20.729728
64.605502	2517.547012	20.734746
65.103885	2526.884130	20.739763
64.821127	2542.377169	20.744781
64.879467	2536.045708	20.749799
64.894713	2538.909929	20.754816
64.923797	2538.656393	20.759834
65.446971	2533.381218	20.764851
65.239718	2541.885288	20.769869
65.359552	2540.549399	20.774887
65.881103	2534.229572	20.779904
64.955664	2516.609873	20.784922
65.337878	2529.528634	20.789939
65.464295	2544.673594	20.794957
65.854954	2543.842082	20.799975
65.905063	2565.916732	20.804992
65.648467	2568.224000	20.810010
66.044462	2539.865851	20.815027
66.083706	2556.411433	20.820045
66.188859	2547.997939	20.825063
66.147561	2566.731905	20.830080
65.960134	2548.383027	20.835098
66.367180	2551.092561	20.840115
66.166577	2568.005692	20.845133
65.948367	2549.443428	20.850151
66.170826	2552.618831	20.855168
66.436369	2574.662422	20.860186
66.488473	2552.280464	20.865203
66.617505	2544.340119	20.870221
66.539369	2560.881090	20.875239
66.319979	2555.261555	20.880256
66.092395	2556.002649	20.885274
66.753877	2585.644241	20.890291
66.684673	2585.144583	20.895309
66.853638	2574.390957	20.900327
66.958355	2587.355817	20.905344
66.666823	2604.983909	20.910362
66.716531	2598.024611	20.915379
66.581244	2588.008551	20.920397
66.839921	2593.044235	20.925415
66.807346	2606.531329	20.930432
67.081802	2641.845602	20.935450
67.023915	2623.243373	20.940467
67.200543	2633.071258	20.945485
67.394306	2643.074442	20.950503
67.463362	2651.105614	20.955520
67.643194	2654.486085	20.960538
67.590107	2637.854019	20.965555
67.833454	2632.972047	20.970573
67.905719	2656.539995	20.975591
67.968436	2656.962887	20.980608
67.784623	2639.829268	20.985626
68.192375	2617.888374	20.990643
68.273372	2632.051110	20.995661
68.092567	2645.419644	21.000679
68.002207	2651.794332	21.005696
68.460240	2650.248438	21.010714
68.601409	2658.344262	21.015731
68.808751	2672.000204	21.020749
68.363580	2670.926146	21.025767
68.663717	2662.233161	21.030784
68.845602	2655.174843	21.035802
68.961371	2669.563921	21.040819
69.020555	2655.260585	21.045837
68.932548	2660.300830	21.050855
69.487208	2658.018796	21.055872
69.169967	2663.914126	21.060890
69.294161	2638.126329	21.065907
69.253018	2644.832005	21.070925
69.074380	2657.465456	21.075943
69.265752	2641.133297	21.080960
69.112261	2658.695143	21.085978
69.231019	2656.442428	21.090995
69.077390	2651.583139	21.096013
69.075057	2639.009813	21.101031
69.266604	2666.398649	21.106048
69.287378	2690.211343	21.111066
69.518606	2683.933721	21.116083
69.359185	2680.517891	21.121101
69.376557	2693.867497	21.126119
69.866092	2716.951292	21.131136
69.691955	2724.357230	21.136154
69.888736	2710.348582	21.141171
70.010356	2707.587191	21.146189
69.922164	2726.292885	21.151207
70.447647	2728.381193	21.156224
70.615425	2739.193542	21.161242
70.586633	2747.266323	21.166259
70.968238	2732.759266	21.171277
70.635996	2743.528865	21.176295
70.997606	2728.400596	21.181312
70.843360	2723.516390	21.186330
70.804708	2724.853349	21.191347
70.995424	2737.568135	21.196365
71.026697	2728.580415	21.201383
70.932216	2726.215703	21.206400
71.026962	2743.455563	21.211418
71.289528	2728.904409	21.216435
71.308732	2733.740374	21.221453
71.209478	2742.751635	21.226471
71.208873	2747.002966	21.231488
71.139986	2735.821470	21.236506
71.308075	2725.127521	21.241523
71.589696	2749.916550	21.246541
71.517989	2774.880917	21.251559
71.936522	2761.800015	21.256576
71.721179	2755.138148	21.261594
71.753544	2747.366014	21.266611
71.739204	2756.809647	21.271629
71.696601	2770.189698	21.276647
72.075929	2763.598242	21.281664
71.868130	2753.792846	21.286682
72.045597	2768.733753	21.291699
72.159162	2799.533275	21.296717
72.309355	2792.368335	21.301735
72.808457	2775.789148	21.306752
72.650365	2768.123858	21.311770
72.956178	2781.123950	21.316787
72.947933	2788.346032	21.321805
72.806674	2784.180626	21.326823
73.096579	2770.603915	21.331840
73.047669	2762.622005	21.336858
72.808065	2786.342065	21.341875
73.139648	2784.203160	21.346893
72.947922	2769.485729	21.351911
73.297711	2764.942574	21.356928
73.310615	2772.633136	21.361946
73.305230	2782.532920	21.366963
73.259127	2767.747930	21.371981
73.280593	2768.201851	21.376999
73.298148	2777.131634	21.382016
73.513567	2779.195408	21.387034
73.648934	2788.758398	21.392051
73.811031	2805.951377	21.397069
73.514660	2813.363779	21.402087
73.693002	2787.455382	21.407104
73.670679	2799.750957	21.412122
73.765599	2805.891774	21.417139
74.239938	2809.944384	21.422157
74.183000	2802.968959	21.427175
74.278955	2782.360479	21.432192
74.427131	2789.409884	21.437210
74.464493	2819.329444	21.442227
74.535726	2810.679122	21.447245
74.602883	2819.680250	21.452263
74.686389	2824.946504	21.457280
74.570181	2827.767155	21.462298
74.780960	2818.694806	21.467315
75.096965	2807.972619	21.472333
75.007763	2813.223712	21.477351
74.842754	2821.773114	21.482368
74.838230	2813.475616	21.487386
75.090864	2804.737062	21.492403
74.943804	2804.578367	21.497421
74.965167	2829.732535	21.502439
75.045788	2833.314060	21.507456
75.221564	2834.884656	21.512474
75.171286	2858.617041	21.517491
75.373852	2839.358995	21.522509
75.285190	2846.024980	21.527527
75.659974	2861.311865	21.532544
75.612566	2877.190705	21.537562
75.762181	2882.379528	21.542579
76.214283	2867.222196	21.547597
75.828093	2883.853388	21.552615
75.923704	2860.260406	21.557632
75.880564	2878.915736	21.562650
76.127220	2900.912332	21.567667
76.474718	2906.225925	21.572685
76.240041	2910.361276	21.577703
76.559257	2885.851891	21.582720
76.602018	2894.523083	21.587738
76.580596	2912.784956	21.592755
76.683284	2897.595579	21.597773
76.711818	2905.829027	21.602791
76.794709	2887.484479	21.607808
77.085224	2903.275228	21.612826
76.619088	2907.794843	21.617843
77.096009	2926.436924	21.622861
77.041096	2937.746781	21.627879
77.101268	2936.931676	21.632896
77.163389	2921.370484	21.637914
77.360053	2933.051706	21.642931
77.645284	2915.412968	21.647949
77.464183	2925.070259	21.652967
77.620722	2916.585482	21.657984
77.778256	2919.341627	21.663002
77.754389	2929.513226	21.668019
78.049629	2939.741340	21.673037
77.603351	2955.607832	21.678055
78.026914	2956.921579	21.683072
77.811351	2950.262616	21.688090
77.868200	2954.800537	21.693107
78.168682	2954.218720	21.698125
77.958052	2957.934217	21.703143
77.931948	2963.844733	21.708160
78.001827	2968.085463	21.713178
78.153081	2979.084153	21.718195
78.351476	2980.175298	21.723213
78.335599	2998.323180	21.728231
78.655366	2975.215359	21.733248
78.852351	2987.370331	21.738266
78.793486	3011.680677	21.743283
79.088133	3009.741129	21.748301
79.163008	3000.994440	21.753319
79.504803	3009.858578	21.758336
79.541274	3017.861866	21.763354
79.650154	2994.568615	21.768371
79.598476	2985.993812	21.773389
79.544117	3001.564714	21.778407
79.747241	3005.376203	21.783424
79.666199	3001.448198	21.788442
79.622468	2988.485019	21.793459
80.336111	2986.673656	21.798477
80.006153	3008.299208	21.803495
79.971531	2997.151815	21.808512
79.930966	3013.179251	21.813530
79.909787	2997.920491	21.818547
80.278952	2980.618749	21.823565
80.080897	3007.034902	21.828583
80.005853	3016.014372	21.833600
80.401222	3013.198246	21.838618
80.270552	3016.249442	21.843635
80.537451	3016.510275	21.848653
80.593403	3027.829041	21.853671
80.551778	3029.205293	21.858688
80.507259	3020.622399	21.863706
80.411662	3026.954412	21.868723
80.728565	3030.185561	21.873741
80.804115	3056.118844	21.878759
80.861350	3059.117348	21.883776
81.060412	3062.072932	21.888794
81.030702	3069.622867	21.893811
81.110344	3074.372583	21.898829
81.479379	3067.790376	21.903847
81.669239	3055.682137	21.908864
81.889281	3079.447154	21.913882
81.968577	3081.535037	21.918899
82.217701	3071.755893	21.923917
82.080051	3078.049606	21.928935
82.185587	3069.707409	21.933952
82.509837	3056.074189	21.938970
82.141211	3076.992531	21.943987
82.243902	3054.152128	21.949005
82.596821	3062.110826	21.954023
82.573133	3072.010080	21.959040
82.421623	3076.670841	21.964058
82.170149	3061.297727	21.969075
82.524889	3070.003284	21.974093
82.786054	3082.145757	21.979111
82.785178	3094.777157	21.984128
83.106918	3109.812455	21.989146
83.146737	3106.368921	21.994163
82.979541	3085.387031	21.999181
82.852930	3099.499080	22.004199
82.866331	3113.449045	22.009216
82.890469	3103.162632	22.014234
83.003747	3109.228696	22.019251
83.061784	3108.146643	22.024269
83.060475	3111.552620	22.029287
82.962039	3120.588569	22.034304
83.264052	3141.925454	22.039322
83.220419	3150.806122	22.044339
83.501629	3142.779898	22.049357
83.572961	3158.529577	22.054375
84.037502	3162.488833	22.059392
83.922563	3166.247222	22.064410
83.988565	3167.758638	22.069427
83.719714	3182.854592	22.074445
84.355228	3194.573329	22.079463
84.740685	3176.188875	22.084480
84.821763	3173.029815	22.089498
84.893171	3190.258285	22.094515
84.799643	3187.713246	22.099533
85.102913	3174.318795	22.104551
84.977200	3168.897507	22.109568
85.096773	3161.920900	22.114586
84.917811	3168.008507	22.119603
85.213941	3168.937469	22.124621
85.070777	3165.731812	22.129639
85.296502	3183.762047	22.134656
85.141096	3182.207833	22.139674
85.302449	3181.422054	22.144691
85.360185	3176.013753	22.149709
85.660273	3182.105270	22.154727
85.398024	3196.757480	22.159744
85.553355	3199.037320	22.164762
85.882601	3192.189617	22.169779
85.942290	3187.649792	22.174797
85.992725	3192.665956	22.179815
85.971203	3211.715514	22.184832
86.243578	3214.213195	22.189850
86.001058	3218.416648	22.194867
85.953764	3212.760561	22.199885
86.070528	3227.892633	22.204903
86.261772	3236.965027	22.209920
86.779588	3233.534204	22.214938
86.697692	3241.096193	22.219955
86.517474	3243.026607	22.224973
86.974742	3239.847494	22.229991
86.862244	3257.436708	22.235008
87.310271	3239.251857	22.240026
87.093064	3257.060516	22.245043
87.099499	3262.758115	22.250061
87.431619	3241.359880	22.255079
86.954529	3253.826030	22.260096
87.429409	3269.231020	22.265114
87.289236	3268.502146	22.270131
87.281208	3289.738514	22.275149
87.563457	3289.392548	22.280167
87.371694	3278.849204	22.285184
87.903899	3287.729673	22.290202
87.883611	3317.979181	22.295219
87.947817	3324.765570	22.300237
88.132903	3334.883816	22.305255
88.297207	3312.415883	22.310272
88.601498	3300.670789	22.315290
88.116354	3310.353562	22.320307
88.746090	3310.130868	22.325325
89.257406	3323.573596	22.330343
89.063871	3308.698484	22.335360
89.109071	3316.548137	22.340378
89.014871	3310.555115	22.345395
89.190955	3293.509905	22.350413
89.229380	3303.656498	22.355431
89.105259	3317.177056	22.360448
89.437983	3280.205262	22.365466
89.000169	3289.576690	22.370483
88.852445	3321.963973	22.375501
89.268455	3328.708767	22.380519
89.282134	3328.851425	22.385536
89.532318	3314.613545	22.390554
89.368046	3333.501427	22.395571
89.462357	3353.647655	22.400589
89.597934	3365.781973	22.405607
89.427863	3352.971635	22.410624
89.982598	3346.852670	22.415642
90.045022	3360.484751	22.420659
90.193499	3395.152935	22.425677
90.476380	3387.799077	22.430695
90.187157	3375.410338	22.435712
90.634329	3396.469875	22.440730
90.516714	3384.510601	22.445747
90.362531	3379.183502	22.450765
91.016365	3398.568503	22.455783
90.970607	3405.245551	22.460800
91.221032	3385.864360	22.465818
91.215751	3413.459079	22.470835
91.337031	3412.192162	22.475853
91.870778	3408.555735	22.480871
91.679016	3404.377837	22.485888
91.980796	3383.695965	22.490906
91.735646	3401.115548	22.495923
91.949796	3410.240160	22.500941
92.297260	3392.703969	22.505959
92.123015	3372.823337	22.510976
91.751234	3353.223180	22.515994
91.761689	3391.403383	22.521011
92.052031	3401.121443	22.526029
92.386340	3386.940062	22.531047
91.961197	3383.796699	22.536064
92.140718	3406.178894	22.541082
92.048831	3419.630442	22.546099
92.161189	3414.668501	22.551117
92.454286	3425.950343	22.556135
92.113788	3431.633880	22.561152
92.403668	3436.633391	22.566170
92.876125	3442.981740	22.571187
92.844442	3449.372649	22.576205
92.881536	3458.985756	22.581223
92.563080	3471.436890	22.586240
92.740622	3473.547172	22.591258
93.088141	3491.316128	22.596275
93.029593	3479.117318	22.601293
93.656482	3476.861027	22.606311
93.449116	3488.672616	22.611328
93.710941	3510.361700	22.616346
93.877022	3521.870290	22.621363
93.848899	3526.693263	22.626381
94.244422	3500.422026	22.631399
94.187843	3500.541061	22.636416
93.999293	3509.664169	22.641434
94.208227	3521.276888	22.646451
94.262607	3511.076143	22.651469
94.498538	3529.921166	22.656487
94.613750	3530.518660	22.661504
94.852028	3537.838535	22.666522
94.760185	3551.539578	22.671539
94.894575	3533.281612	22.676557
95.525845	3525.036142	22.681575
95.146552	3532.426370	22.686592
95.268218	3525.158136	22.691610
95.324082	3532.155426	22.696627
95.101786	3547.777854	22.701645
95.389448	3532.873206	22.706663
95.250775	3519.024364	22.711680
95.478904	3549.054947	22.716698
95.697701	3555.288183	22.721715
96.018043	3561.325131	22.726733
96.462365	3562.817574	22.731751
96.325794	3548.969145	22.736768
96.579199	3548.036260	22.741786
96.539194	3553.327699	22.746803
96.721668	3554.986429	22.751821
96.843023	3535.759044	22.756839
96.123831	3534.369796	22.761856
96.414866	3523.284540	22.766874
96.457730	3547.428934	22.771891
96.502439	3541.044594	22.776909
96.838259	3550.090726	22.781927
96.703567	3555.072052	22.786944
96.953029	3542.581569	22.791962
96.916144	3558.766234	22.796979
96.773431	3577.494959	22.801997
97.196929	3576.112545	22.807015
96.840044	3579.512622	22.812032
97.340850	3601.265486	22.817050
97.462790	3606.655961	22.822067
97.267554	3624.309259	22.827085
97.557478	3611.722279	22.832103
97.625352	3612.001248	22.837120
97.939334	3629.272404	22.842138
98.128364	3634.708098	22.847155
98.067593	3628.743874	22.852173
98.532854	3626.254054	22.857191
98.161849	3636.059891	22.862208
98.312158	3630.347575	22.867226
98.741358	3648.703955	22.872243
98.728969	3668.898539	22.877261
99.071818	3650.404824	22.882279
99.081548	3650.475309	22.887296
99.198247	3648.824318	22.892314
99.430829	3667.972991	22.897331
99.144975	3676.277498	22.902349
99.400726	3649.481903	22.907367
99.570580	3640.936464	22.912384
99.544561	3655.958111	22.917402
99.788780	3664.808045	22.922419
99.406396	3659.014659	22.927437
99.735384	3647.498274	22.932455
99.672888	3672.201174	22.937472
99.787544	3687.993246	22.942490
99.906748	3677.128778	22.947507
99.845730	3682.377675	22.952525
100.327037	3703.721143	22.957543
100.242159	3710.690985	22.962560
100.431870	3712.547340	22.967578
100.149907	3728.662647	22.972595
100.224766	3714.851569	22.977613
100.640931	3714.392333	22.982631
100.801885	3740.692153	22.987648
100.716139	3755.990282	22.992666
100.906653	3742.604722	22.997683
100.652125	3750.942279	23.002701
101.104213	3746.106760	23.007719
101.193093	3779.595388	23.012736
101.467604	3774.750032	23.017754
101.866216	3748.287721	23.022771
101.987511	3747.328823	23.027789
102.112597	3757.522020	23.032807
101.826820	3772.078077	23.037824
101.953150	3761.258629	23.042842
102.311464	3746.760575	23.047859
102.030570	3749.136001	23.052877
102.354376	3763.012234	23.057895
102.300459	3790.336745	23.062912
102.218834	3776.755784	23.067930
102.731165	3777.245942	23.072947
102.311973	3793.100350	23.077965
102.361405	3786.893658	23.082983
102.528027	3784.524415	23.088000
102.821734	3820.414743	23.093018
103.263603	3814.494944	23.098035
103.101530	3810.583467	23.103053
103.474961	3828.974866	23.108071
103.332478	3823.436638	23.113088
103.164126	3821.070775	23.118106
103.546256	3815.761788	23.123123
103.508108	3845.335799	23.128141
103.284769	3846.899422	23.133159
103.544744	3838.260052	23.138176
103.724278	3829.400529	23.143194
104.018333	3858.710633	23.148211
104.262599	3885.352619	23.153229
104.411211	3875.843104	23.158247
104.506041	3869.076159	23.163264
104.809342	3871.627694	23.168282
104.771400	3868.370450	23.173299
104.724239	3865.055285	23.178317
104.597532	3866.537199	23.183335
104.870413	3883.298930	23.188352
104.908220	3890.879839	23.193370
105.212125	3885.183978	23.198387
104.959650	3907.618400	23.203405
105.402655	3911.143054	23.208423
105.287319	3898.264167	23.213440
105.525140	3906.298814	23.218458
105.762160	3927.026896	23.223475
105.871977	3923.695228	23.228493
105.813400	3941.183008	23.233511
106.021192	3935.420731	23.238528
106.274745	3925.041733	23.243546
106.206530	3929.713789	23.248563
106.000309	3938.811527	23.253581
106.412968	3961.218795	23.258599
106.576625	3962.073247	23.263616
106.499470	3957.974877	23.268634
106.892453	3944.523012	23.273651
106.713505	3951.191203	23.278669
106.931505	3970.133224	23.283687
107.326545	3968.230315	23.288704
107.156669	3998.135027	23.293722
107.348808	3989.310533	23.298739
107.266477	3978.707488	23.303757
107.146162	3981.021772	23.308775
107.312122	3994.965631	23.313792
107.502847	4022.077893	23.318810
107.532413	4008.035666	23.323827
107.551414	4008.404997	23.328845
107.982597	4018.056871	23.333863
108.264545	4015.988007	23.338880
108.042648	4025.239952	23.343898
108.368664	4040.568744	23.348915
108.187215	4050.705704	23.353933
108.670804	4033.242159	23.358951
108.862288	4050.598985	23.363968
108.765706	4058.399219	23.368986
108.795270	4035.749558	23.374003
108.889843	4044.998039	23.379021
109.128355	4060.922775	23.384039
109.135308	4056.592776	23.389056
109.200895	4051.735401	23.394074
109.429712	4046.959713	23.399091
109.641176	4051.900536	23.404109
109.455279	4063.990889	23.409127
109.871327	4052.903497	23.414144
109.636885	4058.206568	23.419162
109.769131	4061.386564	23.424179
109.979844	4083.724235	23.429197
109.981628	4100.615637	23.434215
110.318935	4089.916801	23.439232
110.248642	4090.083576	23.444250
110.396962	4079.429753	23.449267
110.342628	4091.443668	23.454285
110.321405	4124.384926	23.459303
110.616193	4122.315896	23.464320
110.785030	4109.907174	23.469338
111.002032	4101.676509	23.474355
111.040946	4137.234102	23.479373
111.116031	4155.925176	23.484391
111.370350	4142.803517	23.489408
111.346166	4158.233203	23.494426
111.762365	4141.185377	23.499443
111.609799	4134.334594	23.504461
112.043881	4155.550081	23.509479
112.010576	4172.364686	23.514496
111.829588	4171.593892	23.519514
112.268448	4179.513972	23.524531
112.292446	4179.965942	23.529549
112.272848	4156.563633	23.534567
112.483712	4157.635482	23.539584
112.279914	4182.497970	23.544602
112.632060	4185.029873	23.549619
112.533046	4190.772402	23.554637
112.372606	4191.387913	23.559655
112.923735	4208.384323	23.564672
112.883295	4239.516089	23.569690
113.253578	4219.669977	23.574707
113.610446	4220.152376	23.579725
113.667065	4231.754776	23.584743
113.648149	4234.737747	23.589760
113.633066	4228.725980	23.594778
114.172889	4264.452662	23.599795
114.234331	4265.240166	23.604813
114.033958	4250.795966	23.609831
114.248109	4251.035817	23.614848
114.111607	4277.549867	23.619866
114.043706	4256.874178	23.624883
114.130209	4264.325773	23.629901
114.016952	4277.619201	23.634919
114.525604	4284.376273	23.639936
114.791572	4279.755786	23.644954
114.738189	4307.543504	23.649971
115.021533	4330.157708	23.654989
114.716157	4311.568354	23.660007
115.081960	4296.604986	23.665024
115.180667	4341.679575	23.670042
115.468279	4349.221992	23.675059
115.708645	4341.308983	23.680077
115.657575	4328.925793	23.685095
115.906235	4342.879135	23.690112
115.832493	4373.137963	23.695130
116.106511	4377.046148	23.700147
116.573376	4368.058333	23.705165
116.127732	4394.287847	23.710183
116.601278	4376.452754	23.715200
116.386991	4374.476863	23.720218
116.830273	4373.165127	23.725235
116.362228	4371.162270	23.730253
116.421922	4397.238214	23.735271
116.789455	4408.032704	23.740288
116.521458	4424.307639	23.745306
117.161156	4415.850671	23.750323
117.457809	4415.756824	23.755341
116.968824	4436.234300	23.760359
117.673947	4419.517159	23.765376
117.489121	4431.567465	23.770394
117.668171	4455.664002	23.775411
117.916835	4462.921579	23.780429
117.790298	4447.231959	23.785447
118.437206	4465.480113	23.790464
118.228266	4478.994242	23.795482
118.666586	4462.889235	23.800499
118.850410	4448.828993	23.805517
118.625196	4464.360702	23.810535
119.001867	4482.362591	23.815552
118.951993	4482.831894	23.820570
119.113992	4478.564346	23.825587
119.328795	4490.899050	23.830605
119.459351	4478.796351	23.835623
119.402897	4465.960410	23.840640
119.288775	4477.688841	23.845658
119.820827	4490.466388	23.850675
119.863075	4495.469958	23.855693
119.843904	4492.461443	23.860711
120.156690	4498.858071	23.865728
119.981502	4508.735246	23.870746
120.094292	4490.711213	23.875763
120.305664	4504.739365	23.880781
120.167574	4517.391054	23.885799
120.081348	4520.649762	23.890816
120.012701	4525.012233	23.895834
120.683288	4543.105783	23.900851
120.570609	4561.894117	23.905869
120.610478	4559.662825	23.910887
120.714315	4560.942935	23.915904
121.264723	4576.842650	23.920922
121.411083	4605.839604	23.925939
121.578458	4610.010346	23.930957
121.817979	4593.507352	23.935975
122.053699	4587.226450	23.940992
121.883589	4591.638381	23.946010
122.177970	4597.551092	23.951027
122.873627	4612.107972	23.956045
122.520685	4624.116915	23.961063
122.548191	4612.240978	23.966080
122.643721	4617.501528	23.971098
122.887922	4615.271504	23.976115
122.886845	4597.600800	23.981133
122.874699	4613.282094	23.986151
123.114399	4613.088998	23.991168
123.287605	4613.848211	23.996186
123.007071	4638.263485	24.001203
123.215924	4633.475169	24.006221
123.145679	4638.662331	24.011239
123.241416	4646.479113	24.016256
123.219102	4679.798102	24.021274
123.360247	4675.569378	24.026291
124.140543	4670.619702	24.031309
124.216849	4687.791158	24.036327
124.578082	4688.071281	24.041344
124.575935	4689.559462	24.046362
124.628716	4698.692406	24.051379
124.819148	4678.455747	24.056397
124.715032	4691.917309	24.061415
124.803223	4695.865335	24.066432
125.364204	4688.431057	24.071450
125.516718	4681.327263	24.076467
125.488095	4672.552245	24.081485
125.223875	4685.954430	24.086503
125.598621	4688.720475	24.091520
125.622383	4671.995570	24.096538
125.427390	4673.610889	24.101555
125.845550	4693.180556	24.106573
125.748218	4716.769630	24.111591
125.963244	4703.909107	24.116608
126.170330	4684.586212	24.121626
126.202190	4706.287808	24.126643
126.397294	4740.194224	24.131661
126.374386	4755.281775	24.136679
126.564373	4745.924930	24.141696
126.584329	4743.575643	24.146714
126.560632	4737.221799	24.151731
127.306972	4752.175550	24.156749
126.930054	4773.714864	24.161767
127.355470	4762.528571	24.166784
127.189692	4777.904710	24.171802
127.175833	4782.470403	24.176819
127.371346	4802.048256	24.181837
127.557588	4798.047872	24.186855
127.696304	4819.186303	24.191872
127.709941	4828.325792	24.196890
127.501420	4836.404359	24.201907
127.902023	4846.234246	24.206925
127.981933	4844.875429	24.211943
128.423997	4850.238640	24.216960
128.733806	4868.503207	24.221978
128.879277	4896.627625	24.226995
128.890115	4884.179038	24.232013
128.841249	4896.190309	24.237031
129.349548	4894.624483	24.242048
129.658979	4919.843112	24.247066
129.523203	4928.021124	24.252083
129.982889	4908.923144	24.257101
129.789061	4904.300100	24.262119
130.174136	4916.941262	24.267136
130.341287	4929.755844	24.272154
130.378411	4929.135980	24.277171
130.147059	4904.841151	24.282189
130.164894	4933.129244	24.287207
130.401328	4930.886287	24.292224
130.603165	4938.974662	24.297242
130.742531	4935.218604	24.302259
130.761230	4949.441987	24.307277
130.986686	4962.239482	24.312295
131.088865	4951.692686	24.317312
131.382436	4955.669048	24.322330
131.303475	4977.564531	24.327347
131.415639	4988.240597	24.332365
131.575100	4993.257639	24.337383
131.941737	4993.346717	24.342400
132.026772	4990.920891	24.347418
131.965526	4997.135432	24.352435
132.502626	5001.051489	24.357453
132.412024	5017.944981	24.362471
132.466914	5037.279828	24.367488
132.439168	5038.015573	24.372506
132.781850	5035.819612	24.377523
133.026268	5043.168323	24.382541
132.703924	5044.177943	24.387559
132.982260	5058.486480	24.392576
133.198911	5046.366358	24.397594
133.140704	5047.656748	24.402611
133.358045	5073.711717	24.407629
133.280276	5093.163043	24.412647
133.381921	5079.920939	24.417664
133.482288	5092.849054	24.422682
133.742461	5111.402820	24.427699
133.991801	5125.007144	24.432717
134.010206	5119.907623	24.437735
134.276613	5122.958188	24.442752
134.592782	5141.489746	24.447770
134.511318	5155.696796	24.452787
134.954745	5130.960980	24.457805
135.043251	5136.033887	24.462823
135.223250	5168.928364	24.467840
135.643873	5162.803298	24.472858
135.317424	5183.417105	24.477875
135.651811	5175.942084	24.482893
135.639766	5161.815136	24.487911
135.568744	5152.548025	24.492928
135.898129	5180.713829	24.497946
135.847538	5217.974543	24.502963
136.146191	5194.812580	24.507981
136.130699	5200.895624	24.512999
136.107476	5217.097083	24.518016
136.102760	5218.330616	24.523034
136.243094	5235.754702	24.528051
136.661034	5249.643096	24.533069
137.082563	5275.631987	24.538087
136.847520	5268.712831	24.543104
137.380857	5271.657903	24.548122
137.250533	5283.684507	24.553139
137.650212	5296.227500	24.558157
137.719002	5295.141747	24.563175
137.855484	5283.648091	24.568192
138.038470	5310.746561	24.573210
138.173130	5333.261988	24.578227
138.346709	5313.390686	24.583245
138.498248	5326.912919	24.588263
138.453215	5315.256312	24.593280
138.962772	5308.639710	24.598298
138.709917	5345.605794	24.603315
139.106726	5360.588754	24.608333
139.343553	5340.869964	24.613351
139.018337	5345.574278	24.618368
139.402595	5353.746512	24.623386
139.383221	5373.364528	24.628403
139.640231	5362.605251	24.633421
139.727430	5377.952387	24.638439
139.670307	5381.105675	24.643456
140.145575	5376.703441	24.648474
140.313634	5404.420702	24.653491
140.420199	5386.281696	24.658509
140.450806	5390.755572	24.663527
140.712084	5407.970885	24.668544
141.022245	5419.042894	24.673562
141.115561	5405.990872	24.678579
141.565452	5411.347475	24.683597
141.466106	5425.220706	24.688615
141.549777	5430.609086	24.693632
141.685091	5412.597194	24.698650
141.677895	5415.356399	24.703667
141.495441	5434.934901	24.708685
142.024899	5449.518852	24.713703
141.880920	5459.588723	24.718720
141.853153	5441.539174	24.723738
142.004343	5460.379878	24.728755
142.169947	5479.065068	24.733773
142.561998	5488.515268	24.738791
142.107551	5497.048999	24.743808
142.529035	5511.330364	24.748826
142.879042	5519.113840	24.753843
142.868216	5504.732433	24.758861
143.325005	5528.343388	24.763879
143.179175	5549.188080	24.768896
143.744750	5547.643045	24.773914
143.641035	5555.698761	24.778931
143.494056	5562.339521	24.783949
143.839381	5552.985662	24.788967
144.102356	5567.319647	24.793984
143.945450	5566.679453	24.799002
143.990124	5567.698939	24.804019
144.427850	5588.629161	24.809037
144.839991	5604.000786	24.814055
144.544866	5615.073728	24.819072
144.938138	5601.317227	24.824090
144.885693	5640.428553	24.829107
145.082845	5636.828929	24.834125
145.163273	5624.174936	24.839143
145.169945	5653.754826	24.844160
145.530764	5668.124315	24.849178
145.432197	5681.134215	24.854195
145.950376	5690.186514	24.859213
146.475990	5667.568269	24.864231
146.559628	5688.954395	24.869248
146.398117	5704.217744	24.874266
146.482271	5690.381524	24.879283
146.661480	5719.393238	24.884301
147.145051	5721.256406	24.889319
147.101955	5721.008839	24.894336
147.754681	5714.036112	24.899354
147.475556	5719.993618	24.904371
147.256689	5736.376375	24.909389
147.813589	5735.878483	24.914407
147.558623	5729.786079	24.919424
148.240234	5753.352748	24.924442
148.069229	5761.312202	24.929459
148.181180	5767.864201	24.934477
148.538741	5767.411450	24.939495
148.367882	5779.932168	24.944512
148.657832	5787.846576	24.949530
148.559266	5793.199047	24.954547
149.106755	5788.470968	24.959565
149.359389	5807.644170	24.964583
149.125233	5814.024228	24.969600
149.389033	5820.742903	24.974618
149.537574	5827.025086	24.979635
149.932426	5816.632510	24.984653
150.201078	5832.267060	24.989671
150.230262	5850.061795	24.994688
150.239950	5831.064604	24.999706
150.261717	5831.077989	25.004723
150.107206	5846.572223	25.009741
150.877466	5850.003491	25.014759
150.819207	5868.264691	25.019776
150.918343	5869.362211	25.024794
150.980891	5885.715163	25.029811
151.238621	5892.388019	25.034829
151.252840	5888.850455	25.039847
151.345511	5909.629842	25.044864
151.548986	5905.070782	25.049882
151.590780	5906.630564	25.054899
151.434364	5931.067906	25.059917
151.553549	5953.450557	25.064935
151.801868	5953.974971	25.069952
151.978306	5963.594559	25.074970
151.954695	5973.047194	25.079987
152.090246	5994.551154	25.085005
152.346076	6002.192156	25.090023
152.460264	6010.781434	25.095040
152.536574	6040.087538	25.100058
153.137670	6051.421398	25.105075
152.868564	6043.778730	25.110093
153.464568	6062.192310	25.115111
153.375123	6077.317333	25.120128
154.130659	6069.914833	25.125146
154.383823	6090.211608	25.130163
154.370677	6094.650392	25.135181
154.897663	6098.693610	25.140199
154.557603	6097.460378	25.145216
155.014767	6099.826026	25.150234
155.426672	6109.854866	25.155251
155.526652	6104.258042	25.160269
155.870553	6075.731372	25.165287
155.657806	6083.464010	25.170304
155.978144	6079.798259	25.175322
155.922229	6082.386485	25.180339
155.919193	6093.831614	25.185357
156.249518	6082.368733	25.190375
156.148108	6093.936030	25.195392
156.378205	6097.523538	25.200410
156.339545	6121.167645	25.205427
156.578830	6132.520005	25.210445
156.313373	6126.037415	25.215463
156.448101	6133.486269	25.220480
156.926826	6144.329353	25.225498
156.805770	6173.862035	25.230515
156.808870	6187.808786	25.235533
157.324734	6171.403754	25.240551
157.314904	6194.099429	25.245568
157.794109	6216.974988	25.250586
157.650356	6232.104803	25.255603
157.856647	6241.786959	25.260621
158.643965	6234.416930	25.265639
158.329999	6258.374472	25.270656
158.491227	6253.100181	25.275674
158.775288	6259.122331	25.280691
158.700343	6288.948425	25.285709
159.279591	6279.524378	25.290727
159.025478	6282.316660	25.295744
159.537979	6307.053157	25.300762
159.700307	6310.638525	25.305779
159.727450	6301.871094	25.310797
160.252475	6290.095945	25.315815
160.066113	6321.624125	25.320832
160.391148	6323.929743	25.325850
160.529494	6339.935183	25.330867
160.247229	6340.411045	25.335885
160.270872	6338.222342	25.340903
160.288442	6345.233920	25.345920
160.570633	6373.229347	25.350938
160.992766	6389.788401	25.355955
161.178346	6387.804058	25.360973
161.371353	6405.184919	25.365991
161.373797	6422.040143	25.371008
161.630907	6421.065732	25.376026
161.956910	6430.520332	25.381043
161.940026	6457.844389	25.386061
162.410022	6446.856640	25.391079
162.431948	6467.679563	25.396096
162.745484	6457.117698	25.401114
162.721740	6454.651346	25.406131
162.896056	6484.088561	25.411149
163.010978	6490.619898	25.416167
163.121947	6482.093266	25.421184
163.393740	6512.136538	25.426202
163.408098	6511.258142	25.431219
163.770682	6503.244313	25.436237
163.986045	6520.879903	25.441255
163.839200	6517.086496	25.446272
164.009612	6543.510375	25.451290
164.218454	6559.227591	25.456307
164.110069	6559.351073	25.461325
164.147930	6554.436472	25.466343
164.527062	6578.437875	25.471360
164.219605	6596.344992	25.476378
164.604689	6600.485419	25.481395
164.807456	6615.202011	25.486413
165.044460	6643.424704	25.491431
165.398324	6646.713513	25.496448
165.290174	6657.323176	25.501466
165.622577	6677.502099	25.506483
165.979581	6709.842171	25.511501
166.259362	6697.492995	25.516519
166.442869	6699.296402	25.521536
166.655790	6715.217062	25.526554
167.055328	6729.996931	25.531571
166.993544	6734.456927	25.536589
167.332019	6726.943877	25.541607
167.545475	6739.821991	25.546624
167.599493	6753.164700	25.551642
168.225867	6747.332624	25.556659
168.206726	6753.837792	25.561677
168.670433	6753.681689	25.566695
168.780094	6774.887028	25.571712
168.695845	6782.129824	25.576730
168.950811	6766.561470	25.581747
168.864292	6757.150673	25.586765
168.862467	6747.305366	25.591783
169.211143	6786.534407	25.596800
169.271501	6795.374378	25.601818
169.396862	6783.862952	25.606835
169.020587	6779.091518	25.611853
169.565341	6801.254657	25.616871
169.715136	6833.411872	25.621888
169.823206	6836.937027	25.626906
170.230114	6829.719352	25.631923
169.849571	6843.689913	25.636941
170.373015	6864.656513	25.641959
170.614907	6873.207840	25.646976
170.502051	6874.038845	25.651994
170.714184	6913.804215	25.657011
170.582620	6923.207534	25.662029
171.088050	6918.209265	25.667047
171.425919	6924.225539	25.672064
171.818120	6953.010626	25.677082
171.544159	6989.194209	25.682100
171.736947	6978.539726	25.687117
172.264972	6993.054094	25.692135
172.585832	7005.071261	25.697152
172.405740	7013.526617	25.702170
172.952790	6996.028419	25.707188
173.224211	7014.542431	25.712205
173.579926	7026.535348	25.717223
173.608307	7041.568595	25.722240
173.893845	7046.348116	25.727258
173.956595	7030.358836	25.732276
174.009190	7025.766894	25.737293
174.157325	7025.045130	25.742311
174.347908	7067.650665	25.747328
174.168378	7079.556444	25.752346
174.378583	7060.219077	25.757364
174.422137	7051.624524	25.762381
174.641766	7078.128586	25.767399
174.830581	7101.407801	25.772416
174.775525	7106.034530	25.777434
175.077771	7109.265029	25.782452
174.974000	7131.569257	25.787469
175.369496	7143.891960	25.792487
175.676440	7164.565159	25.797504
175.717344	7156.796696	25.802522
175.915948	7142.441000	25.807540
176.441234	7174.520337	25.812557
176.501947	7197.180215	25.817575
176.545378	7187.816597	25.822592
176.726059	7200.457950	25.827610
177.118343	7207.289480	25.832628
177.112564	7231.342882	25.837645
177.179377	7235.192313	25.842663
177.564202	7254.921521	25.847680
177.551905	7258.231190	25.852698
177.964798	7270.360146	25.857716
178.219959	7284.179993	25.862733
178.192560	7275.446230	25.867751
178.641218	7287.449586	25.872768
178.393903	7312.589636	25.877786
178.997213	7283.236690	25.882804
178.853026	7311.276680	25.887821
178.920091	7344.726763	25.892839
179.617939	7345.965268	25.897856
179.381044	7356.591163	25.902874
179.498945	7365.005347	25.907892
179.842638	7378.968943	25.912909
179.953416	7379.516922	25.917927
180.362622	7405.853580	25.922944
180.152432	7423.698316	25.927962
180.511745	7414.952558	25.932980
180.331509	7431.428354	25.937997
180.295391	7454.085306	25.943015
181.104960	7451.915832	25.948032
181.062909	7481.329240	25.953050
181.415712	7500.791563	25.958068
181.478772	7515.911281	25.963085
181.412328	7512.432750	25.968103
181.893163	7530.557199	25.973120
182.024418	7568.339617	25.978138
182.504071	7560.985948	25.983156
182.714202	7560.911903	25.988173
183.235929	7597.461960	25.993191
183.396460	7598.225388	25.998208
183.249167	7602.737953	26.003226
183.670692	7598.459756	26.008244
183.848818	7611.477519	26.013261
183.568192	7600.798454	26.018279
183.907745	7614.667653	26.023296
184.217364	7638.170266	26.028314
184.491494	7654.042783	26.033332
184.407923	7656.259393	26.038349
184.616835	7669.998230	26.043367
185.010002	7658.614782	26.048384
185.015716	7686.785819	26.053402
185.245035	7683.321386	26.058420
185.479321	7685.887129	26.063437
185.645210	7704.530041	26.068455
185.944246	7706.273920	26.073472
186.036013	7715.060393	26.078490
186.431231	7732.312448	26.083508
186.804471	7740.921697	26.088525
186.730524	7732.541103	26.093543
186.944957	7730.902285	26.098560
186.800812	7757.592424	26.103578
186.951683	7767.893849	26.108596
186.704639	7778.570532	26.113613
187.186640	7766.563555	26.118631
187.526492	7774.568779	26.123648
187.704957	7820.889672	26.128666
188.017046	7815.301692	26.133684
187.808467	7816.178881	26.138701
187.698715	7825.526369	26.143719
188.116853	7835.329264	26.148736
187.963853	7855.022080	26.153754
188.242667	7868.113987	26.158772
188.683122	7911.407829	26.163789
188.543698	7911.327747	26.168807
189.055844	7916.012603	26.173824
188.820729	7939.710414	26.178842
189.112696	7965.730308	26.183860
189.725194	7975.942211	26.188877
190.369719	8001.106119	26.193895
190.680143	8012.881640	26.198912
190.257941	8021.642157	26.203930
191.116345	8009.190054	26.208948
191.403020	8030.795093	26.213965
191.490162	8022.033327	26.218983
191.956332	8035.469297	26.224000
191.891268	8062.268958	26.229018
192.286288	8061.022402	26.234036
192.315549	8062.608491	26.239053
192.190935	8057.309158	26.244071
192.481863	8065.614011	26.249088
192.542864	8091.995175	26.254106
192.789968	8091.105407	26.259124
193.088928	8110.686854	26.264141
192.758396	8126.158074	26.269159
193.611965	8110.683233	26.274176
193.463196	8117.897530	26.279194
193.618330	8137.538213	26.284212
193.801973	8158.958834	26.289229
193.788226	8184.242035	26.294247
194.270503	8164.830010	26.299264
194.489125	8179.027626	26.304282
194.667132	8192.881498	26.309300
194.823347	8226.834583	26.314317
194.899637	8228.776775	26.319335
195.232816	8231.127802	26.324352
194.870468	8242.963461	26.329370
195.668710	8280.392452	26.334388
196.029709	8275.683036	26.339405
196.045472	8291.820194	26.344423
196.237047	8292.135912	26.349440
196.391851	8296.968920	26.354458
196.810241	8308.976487	26.359476
196.824153	8314.839297	26.364493
196.706267	8329.006014	26.369511
197.211490	8357.457217	26.374528
197.250159	8368.873880	26.379546
197.374593	8355.766224	26.384564
197.830023	8380.078323	26.389581
197.681260	8415.987351	26.394599
198.292855	8403.373312	26.399616
198.301325	8422.584937	26.404634
198.501033	8441.045929	26.409652
198.872459	8447.341958	26.414669
198.936403	8478.679525	26.419687
199.177197	8463.438686	26.424704
199.244848	8485.331774	26.429722
199.431064	8495.527813	26.434740
199.626348	8505.701884	26.439757
199.809173	8527.894973	26.444775
200.082184	8527.801086	26.449792
200.091770	8534.956332	26.454810
200.186596	8552.517247	26.459828
200.658128	8566.959321	26.464845
200.264515	8592.653262	26.469863
200.534619	8594.892690	26.474880
200.643475	8624.212414	26.479898
200.961560	8651.206524	26.484916
201.297344	8639.581400	26.489933
201.567769	8659.996789	26.494951
202.030587	8685.414703	26.499968
201.946862	8702.683948	26.504986
202.245416	8703.289949	26.510004
202.725591	8719.797379	26.515021
202.570545	8755.649147	26.520039
203.254111	8764.485709	26.525056
203.366617	8764.512852	26.530074
203.626765	8778.654529	26.535092
203.736209	8799.431424	26.540109
203.879933	8803.360682	26.545127
204.007542	8809.375012	26.550144
204.213604	8814.391885	26.555162
204.233492	8819.017366	26.560180
204.975823	8854.304454	26.565197
205.035924	8852.869018	26.570215
205.321317	8836.260267	26.575232
205.511877	8878.484388	26.580250
205.433011	8886.315991	26.585268
205.591278	8894.210021	26.590285
205.724879	8919.380266	26.595303
205.769770	8925.199592	26.600320
205.997628	8941.856845	26.605338
206.182758	8978.433430	26.610356
206.850478	8987.375912	26.615373
206.927659	8982.232740	26.620391
207.590369	9009.139020	26.625408
207.626352	9023.511705	26.630426
207.485444	9027.569956	26.635444
207.841557	9068.743341	26.640461
207.927157	9080.671799	26.645479
207.868189	9070.475725	26.650496
208.624067	9094.034374	26.655514
208.613432	9119.706062	26.660532
209.050918	9122.926057	26.665549
208.866308	9129.873433	26.670567
209.475862	9144.179817	26.675584
209.789544	9160.485234	26.680602
209.706353	9182.523139	26.685620
210.035681	9180.706880	26.690637
210.428649	9183.274221	26.695655
210.205114	9205.013997	26.700672
210.890015	9218.415629	26.705690
211.019588	9228.002432	26.710708
210.998825	9227.228533	26.715725
211.149411	9251.235551	26.720743
211.599492	9262.657347	26.725760
211.649668	9252.337581	26.730778
211.869191	9277.806886	26.735796
212.395494	9304.221102	26.740813
212.361028	9321.497848	26.745831
212.449333	9301.737598	26.750848
212.840307	9323.924195	26.755866
212.869301	9353.196243	26.760884
213.313082	9348.648475	26.765901
213.024448	9349.067185	26.770919
213.337925	9365.375210	26.775936
213.438392	9380.145555	26.780954
213.795558	9394.063033	26.785972
214.284994	9398.346464	26.790989
214.195532	9427.330257	26.796007
214.655353	9427.835608	26.801024
214.677732	9426.135408	26.806042
214.652143	9452.133821	26.811060
215.055805	9482.379939	26.816077
214.915149	9493.863272	26.821095
215.139219	9501.604172	26.826112
215.586289	9525.580736	26.831130
215.680406	9547.581190	26.836148
216.298312	9559.162143	26.841165
216.044839	9570.262477	26.846183
216.301233	9577.840546	26.851200
216.652667	9611.619426	26.856218
216.807665	9629.746571	26.861236
217.618505	9643.469594	26.866253
217.685561	9646.338176	26.871271
217.908399	9667.596052	26.876288
218.119666	9662.202091	26.881306
218.114494	9671.779920	26.886324
218.530215	9706.898398	26.891341
218.597901	9728.274143	26.896359
219.084475	9720.644240	26.901376
219.263604	9723.109162	26.906394
219.237709	9745.423509	26.911412
219.780729	9773.184982	26.916429
220.122454	9773.032481	26.921447
220.211246	9761.313447	26.926464
220.553442	9770.658300	26.931482
220.692241	9802.967527	26.936500
221.035296	9801.441150	26.941517
221.371322	9791.743307	26.946535
221.424254	9813.143658	26.951552
221.480724	9829.980603	26.956570
221.561647	9852.197112	26.961588
221.949232	9854.508680	26.966605
222.154281	9860.776055	26.971623
222.351944	9870.099162	26.976640
222.614183	9883.353013	26.981658
222.753934	9898.430836	26.986676
223.002487	9911.683821	26.991693
222.958798	9915.496242	26.996711
222.867494	9930.835175	27.001728
223.222982	9959.928376	27.006746
223.416174	9987.194300	27.011764
223.750564	9972.325653	27.016781
224.263287	10007.090866	27.021799
224.468227	10025.810408	27.026816
224.762465	10044.025295	27.031834
224.819888	10051.285169	27.036852
225.485947	10048.661754	27.041869
225.474270	10073.680612	27.046887
225.371662	10092.107624	27.051904
225.875059	10103.843376	27.056922
225.795269	10100.776849	27.061940
226.221593	10121.297544	27.066957
226.263488	10154.477324	27.071975
226.659908	10162.720171	27.076992
227.151363	10190.642127	27.082010
227.236459	10192.824134	27.087028
227.455715	10201.663392	27.092045
227.623408	10212.696165	27.097063
227.519077	10235.167514	27.102080
228.023010	10236.849473	27.107098
228.228875	10259.120738	27.112116
228.560382	10278.306447	27.117133
228.742588	10289.046224	27.122151
228.949870	10303.908480	27.127168
229.351421	10327.997753	27.132186
229.258889	10332.430365	27.137204
229.292730	10354.204805	27.142221
229.522344	10363.786008	27.147239
229.782804	10385.496269	27.152256
229.879494	10395.636647	27.157274
229.896328	10408.084729	27.162292
230.245230	10413.521974	27.167309
230.461848	10439.605651	27.172327
231.040099	10476.100261	27.177344
231.406396	10489.482360	27.182362
231.407833	10490.004406	27.187380
231.913983	10494.727267	27.192397
231.927888	10527.884880	27.197415
232.102604	10567.688475	27.202432
232.466400	10571.143861	27.207450
232.694260	10593.120516	27.212468
233.138197	10597.511042	27.217485
232.841439	10611.940926	27.222503
233.085850	10624.316133	27.227520
233.505825	10640.447187	27.232538
233.566603	10676.447224	27.237556
233.973512	10706.156360	27.242573
234.253314	10708.940361	27.247591
234.506166	10707.252360	27.252608
235.032332	10726.648272	27.257626
235.019844	10759.756378	27.262644
235.688965	10763.086531	27.267661
235.903111	10765.328429	27.272679
235.882924	10793.190252	27.277696
236.446118	10810.731425	27.282714
236.303126	10812.644786	27.287732
236.414039	10834.743497	27.292749
236.591902	10865.637661	27.297767
236.785315	10861.008740	27.302784
237.743152	10870.080812	27.307802
237.445302	10909.923164	27.312820
237.943864	10914.046388	27.317837
238.142009	10918.042013	27.322855
238.361404	10946.635683	27.327872
238.752433	10943.788172	27.332890
238.946074	10962.587091	27.337908
238.517369	10983.726725	27.342925
238.945436	11016.016619	27.347943
239.155327	11022.796452	27.352960
239.648979	11038.514795	27.357978
239.706154	11064.983458	27.362996
240.372917	11082.285687	27.368013
240.894639	11074.144414	27.373031
240.711078	11099.550901	27.378048
240.997303	11107.139742	27.383066
240.929443	11132.569701	27.388084
241.196044	11140.856563	27.393101
241.906458	11159.354504	27.398119
241.825566	11163.688534	27.403136
241.996286	11189.782597	27.408154
241.833022	11226.551103	27.413172
242.049650	11231.586692	27.418189
242.809896	11262.331842	27.423207
242.777502	11287.470247	27.428224
243.356448	11277.352479	27.433242
243.330793	11312.860940	27.438260
243.509376	11337.732977	27.443277
244.327987	11344.191028	27.448295
244.263424	11371.645273	27.453312
245.130363	11375.721150	27.458330
245.183818	11371.134899	27.463348
245.109800	11387.069471	27.468365
245.554198	11392.567687	27.473383
245.575050	11417.119308	27.478400
245.995072	11402.756661	27.483418
246.025023	11415.914680	27.488436
246.205564	11433.038459	27.493453
246.501868	11437.813604	27.498471
246.636916	11474.408934	27.503488
246.908872	11484.646298	27.508506
247.055542	11488.955424	27.513524
247.155523	11497.955325	27.518541
247.309781	11533.843385	27.523559
247.668939	11559.534323	27.528576
247.879492	11563.893570	27.533594
247.914585	11578.196239	27.538612
248.301152	11615.489233	27.543629
248.645950	11651.614696	27.548647
248.670866	11670.328102	27.553664
249.325913	11676.081503	27.558682
249.610716	11702.121320	27.563700
249.510096	11731.396308	27.568717
250.016663	11723.126447	27.573735
249.739183	11766.695950	27.578752
250.587829	11795.181665	27.583770
250.871455	11785.674821	27.588788
250.993356	11799.915293	27.593805
251.362028	11828.436251	27.598823
251.864262	11863.117449	27.603840
252.136062	11855.416462	27.608858
252.491798	11886.309998	27.613876
252.758063	11888.593073	27.618893
253.417902	11899.714285	27.623911
253.460496	11924.831061	27.628928
253.618059	11913.283421	27.633946
253.817041	11911.413561	27.638964
254.047729	11941.757530	27.643981
254.251174	11969.183489	27.648999
254.484186	11971.916364	27.654016
254.892624	11971.149410	27.659034
255.177153	11965.071407	27.664052
255.302327	12001.322173	27.669069
255.269624	12009.537622	27.674087
255.339109	12011.621625	27.679104
255.297864	12024.161701	27.684122
255.807270	12060.280586	27.689140
255.923557	12102.979283	27.694157
256.403130	12123.035286	27.699175
256.573304	12130.037212	27.704192
256.861763	12137.313434	27.709210
257.211678	12181.191622	27.714228
257.015578	12212.009162	27.719245
257.599595	12210.717685	27.724263
258.039404	12224.177329	27.729280
258.591990	12251.526396	27.734298
258.573408	12271.530965	27.739316
258.764606	12301.090432	27.744333
258.858016	12292.295349	27.749351
259.095342	12308.763925	27.754368
259.630541	12347.464662	27.759386
260.180334	12361.822432	27.764404
260.090022	12372.439265	27.769421
260.727689	12408.264388	27.774439
260.817644	12408.535540	27.779456
260.926707	12404.904833	27.784474
261.346472	12437.420337	27.789492
261.407942	12465.693830	27.794509
262.196681	12451.970455	27.799527
262.107371	12497.447213	27.804544
262.648832	12496.997793	27.809562
263.248162	12489.607135	27.814580
262.842110	12503.135860	27.819597
263.299112	12501.896857	27.824615
263.095836	12517.092123	27.829632
263.096433	12536.598340	27.834650
263.603790	12546.342157	27.839668
263.900484	12586.953073	27.844685
264.422440	12602.663559	27.849703
264.271158	12614.069744	27.854720
264.229742	12630.217594	27.859738
264.877124	12643.211592	27.864756
264.971748	12682.843039	27.869773
265.243783	12701.305695	27.874791
265.666237	12729.125330	27.879808
265.720529	12727.589671	27.884826
266.086288	12742.864453	27.889844
266.105572	12784.798712	27.894861
266.724289	12807.567808	27.899879
266.476756	12829.021051	27.904896
267.039665	12849.549480	27.909914
267.304225	12883.970429	27.914932
267.217426	12917.181927	27.919949
268.149456	12923.023952	27.924967
268.219739	12957.894690	27.929984
268.828444	12970.475445	27.935002
269.530048	12991.496367	27.940020
269.278433	13011.308741	27.945037
269.719187	13031.682693	27.950055
269.861474	13050.003321	27.955072
270.076348	13072.911992	27.960090
270.605949	13067.176750	27.965108
270.579521	13097.153359	27.970125
271.042410	13101.387044	27.975143
271.596873	13121.812439	27.980160
271.532353	13131.956764	27.985178
271.887590	13165.588917	27.990196
271.912404	13182.390505	27.995213
272.516900	13191.318250	28.000231
272.596156	13207.969064	28.005248
272.769115	13216.681351	28.010266
273.366619	13233.335596	28.015284
273.421471	13271.644443	28.020301
274.215685	13306.360096	28.025319
274.195119	13311.497768	28.030336
274.229074	13324.185573	28.035354
274.747296	13345.124597	28.040372
274.501201	13363.423874	28.045389
275.346820	13374.514638	28.050407
275.391561	13396.229963	28.055424
275.418754	13418.843974	28.060442
275.950168	13424.589291	28.065460
276.089930	13452.329254	28.070477
276.493520	13486.276310	28.075495
276.787353	13503.017244	28.080512
277.132489	13522.451978	28.085530
277.310712	13546.971402	28.090548
277.301767	13553.490663	28.095565
277.837826	13566.250122	28.100583
278.235836	13607.860031	28.105600
278.539381	13620.743033	28.110618
278.703532	13630.682872	28.115636
278.586819	13647.617047	28.120653
278.541672	13667.339392	28.125671
278.907194	13711.901448	28.130688
279.406277	13728.670947	28.135706
279.969263	13754.898187	28.140724
279.875004	13777.223931	28.145741
280.468923	13803.020703	28.150759
280.903135	13824.576932	28.155776
280.848829	13827.218933	28.160794
281.394481	13855.459782	28.165812
281.542135	13856.251649	28.170829
281.861374	13880.789251	28.175847
282.365220	13909.506659	28.180864
282.599406	13942.754691	28.185882
282.683973	13920.250792	28.190900
282.785150	13950.771218	28.195917
283.184136	13988.369421	28.200935
283.372983	13997.281985	28.205952
283.525370	14020.266930	28.210970
284.021885	14050.682840	28.215988
284.015640	14080.080441	28.221005
284.496044	14084.165742	28.226023
285.320964	14117.600170	28.231040
285.268343	14149.124901	28.236058
285.730115	14154.795323	28.241076
285.438182	14171.508454	28.246093
286.120396	14173.028250	28.251111
286.461350	14221.011154	28.256128
286.611204	14251.349200	28.261146
287.174917	14246.191720	28.266164
287.424907	14265.558768	28.271181
287.644780	14297.686397	28.276199
287.799913	14327.847232	28.281216
288.134707	14341.762485	28.286234
288.390032	14379.859630	28.291252
288.166318	14407.943341	28.296269
288.791443	14416.186853	28.301287
289.139215	14431.666333	28.306304
289.238899	14478.500170	28.311322
289.620697	14496.205358	28.316340
290.188008	14519.922950	28.321357
290.470992	14557.768551	28.326375
290.918814	14577.098562	28.331392
290.816442	14590.804191	28.336410
291.274417	14619.007285	28.341428
291.391464	14643.046840	28.346445
292.029922	14672.600586	28.351463
292.202914	14696.774373	28.356480
292.577316	14724.421028	28.361498
292.862228	14740.521015	28.366516
293.287089	14762.094224	28.371533
293.711660	14769.268003	28.376551
294.078971	14795.215682	28.381568
294.056591	14823.047815	28.386586
294.438705	14845.080448	28.391604
294.806064	14858.190265	28.396621
295.173433	14880.225381	28.401639
295.331692	14892.734726	28.406656
295.823609	14903.205033	28.411674
296.142060	14928.024848	28.416692
296.291421	14946.517434	28.421709
296.383639	14980.731805	28.426727
296.603507	14992.458905	28.431744
296.700777	15013.754075	28.436762
297.321465	15048.878769	28.441780
297.348417	15068.994316	28.446797
297.806821	15077.106555	28.451815
298.121812	15105.737528	28.456832
298.256298	15143.260774	28.461850
298.927783	15173.884689	28.466868
299.127863	15186.552813	28.471885
299.444478	15214.961520	28.476903
299.699291	15219.073351	28.481920
299.993312	15245.809166	28.486938
300.400983	15254.675243	28.491956
300.512062	15284.416510	28.496973
300.826185	15287.081402	28.501991
301.103969	15314.163543	28.507008
301.047368	15338.466039	28.512026
301.270363	15364.616540	28.517044
301.616194	15385.792342	28.522061
301.928639	15414.622837	28.527079
302.438086	15430.481557	28.532096
302.930472	15470.597007	28.537114
303.082971	15472.056315	28.542132
303.209191	15512.694085	28.547149
303.896825	15525.105432	28.552167
303.979965	15557.124198	28.557184
304.482355	15571.556494	28.562202
304.827371	15581.210001	28.567220
305.351934	15602.429048	28.572237
305.066471	15646.953482	28.577255
305.449947	15674.783059	28.582272
306.048030	15685.956508	28.587290
306.126853	15709.994502	28.592308
306.339917	15750.404199	28.597325
306.518792	15767.287025	28.602343
307.207636	15781.876236	28.607360
307.200784	15837.731448	28.612378
307.727833	15850.087629	28.617396
307.849709	15852.147717	28.622413
308.365004	15899.394484	28.627431
308.700256	15926.885763	28.632448
308.867360	15956.340070	28.637466
309.254265	15969.731221	28.642484
309.463970	15991.297485	28.647501
309.850999	16037.223175	28.652519
310.437257	16063.305333	28.657536
310.701398	16073.897552	28.662554
311.017295	16098.642359	28.667572
311.507270	16133.036133	28.672589
311.746823	16159.019706	28.677607
312.306949	16165.971573	28.682624
312.068900	16178.381908	28.687642
312.303593	16197.845195	28.692660
312.759632	16234.504660	28.697677
313.071532	16268.983298	28.702695
313.220087	16283.135858	28.707712
313.513800	16325.062308	28.712730
314.090286	16330.857961	28.717748
314.286713	16356.431350	28.722765
315.154747	16388.939852	28.727783
315.646295	16393.517175	28.732800
315.698677	16429.055505	28.737818
316.168750	16445.903536	28.742836
316.314299	16452.645074	28.747853
316.534252	16458.857412	28.752871
316.940032	16482.144387	28.757888
316.958559	16523.491158	28.762906
317.065084	16531.104373	28.767924
317.425388	16572.060702	28.772941
317.855450	16580.427381	28.777959
317.932817	16593.115298	28.782976
318.287306	16646.396778	28.787994
318.708994	16684.374132	28.793012
318.832360	16706.054892	28.798029
318.921107	16713.790903	28.803047
319.794750	16748.214000	28.808064
320.077576	16789.416918	28.813082
320.007592	16814.357366	28.818100
320.384072	16829.539685	28.823117
320.739381	16856.847982	28.828135
321.039053	16895.832552	28.833152
321.237867	16945.098314	28.838170
321.863233	16943.593996	28.843188
322.343995	16976.355192	28.848205
322.415995	16997.977056	28.853223
322.888572	17012.495936	28.858240
322.820174	17045.886984	28.863258
323.482473	17061.536079	28.868276
323.829437	17066.383336	28.873293
323.954181	17107.851148	28.878311
324.610966	17133.458448	28.883328
324.428412	17155.612712	28.888346
324.902583	17196.138879	28.893364
325.378304	17209.577844	28.898381
325.772074	17250.457848	28.903399
326.340265	17265.694008	28.908416
326.632289	17287.872492	28.913434
327.099712	17328.575041	28.918452
327.458050	17343.336884	28.923469
327.395984	17367.131090	28.928487
327.986926	17378.872684	28.933504
327.973958	17409.043357	28.938522
328.683275	17420.048329	28.943540
328.874293	17442.992328	28.948557
328.782294	17488.674994	28.953575
329.224336	17515.648550	28.958592
329.733240	17543.156419	28.963610
330.020849	17560.858445	28.968628
330.204149	17593.584911	28.973645
330.616556	17633.701558	28.978663
330.971138	17652.888299	28.983680
330.960753	17678.986501	28.988698
331.281933	17702.973204	28.993716
332.116957	17743.975401	28.998733
332.272067	17760.675086	29.003751
332.803948	17795.046526	29.008768
332.909538	17844.636150	29.013786
333.219579	17857.092752	29.018804
333.411397	17879.472992	29.023821
333.784038	17922.867288	29.028839
334.126323	17968.679707	29.033856
334.391903	18002.372148	29.038874
334.808146	18023.604364	29.043892
335.786331	18051.409097	29.048909
336.047441	18077.352754	29.053927
336.345331	18077.580988	29.058944
336.595941	18106.984393	29.063962
336.529755	18153.458998	29.068980
337.377218	18183.477918	29.073997
337.629483	18205.746170	29.079015
338.005329	18220.676133	29.084032
338.143125	18261.701816	29.089050
338.413482	18267.416344	29.094068
338.831921	18292.041931	29.099085
339.324620	18337.605146	29.104103
339.872677	18352.292427	29.109120
339.985642	18357.673631	29.114138
340.541789	18397.781009	29.119156
340.689448	18422.910179	29.124173
341.093542	18453.794058	29.129191
341.274810	18458.013431	29.134208
341.474080	18476.779171	29.139226
341.899638	18509.147484	29.144244
342.439029	18549.590567	29.149261
342.165821	18587.271024	29.154279
342.364351	18606.681679	29.159296
342.420072	18632.072236	29.164314
343.347923	18675.870136	29.169332
343.831695	18717.898979	29.174349
343.947543	18728.974506	29.179367
344.683939	18742.157310	29.184384
344.960202	18780.445678	29.189402
345.186851	18833.883050	29.194420
345.448081	18837.958489	29.199437
345.585855	18860.672109	29.204455
345.968624	18898.503403	29.209472
346.223246	18908.443342	29.214490
346.662309	18940.324808	29.219508
347.276049	18983.721478	29.224525
347.457445	19023.515580	29.229543
348.069748	19035.888468	29.234560
348.367481	19067.038530	29.239578
348.698891	19111.178854	29.244596
349.061760	19127.929144	29.249613
349.211395	19136.188995	29.254631
349.656408	19162.898389	29.259648
349.959307	19204.264822	29.264666
350.348550	19260.401981	29.269684
350.958687	19266.654961	29.274701
351.067856	19292.806898	29.279719
351.712502	19331.227987	29.284736
351.691290	19342.282433	29.289754
351.786251	19372.560241	29.294772
352.401498	19418.014779	29.299789
352.546591	19449.285352	29.304807
352.863963	19467.774207	29.309824
353.392092	19516.397452	29.314842
353.595383	19555.278152	29.319860
353.854061	19590.220211	29.324877
353.932072	19638.200980	29.329895
354.430750	19677.014254	29.334912
354.797226	19708.913924	29.339930
355.223421	19759.372147	29.344948
355.732860	19784.122068	29.349965
355.960562	19810.765951	29.354983
356.468622	19859.321011	29.360000
357.056162	19902.401288	29.365018
357.080353	19923.528907	29.370036
357.712117	19954.366952	29.375053
357.980283	19999.691271	29.380071
358.568256	20027.595339	29.385088
359.324312	20055.317212	29.390106
359.473952	20092.321216	29.395124
360.116494	20094.708819	29.400141
360.815133	20128.811681	29.405159
361.186383	20163.719015	29.410176
361.658373	20188.403218	29.415194
362.020049	20195.830962	29.420212
362.364985	20200.205021	29.425229
362.257556	20228.055640	29.430247
362.666676	20264.501711	29.435264
363.120665	20290.762198	29.440282
363.182540	20306.043842	29.445300
363.866240	20314.266500	29.450317
364.285137	20361.769022	29.455335
364.318976	20392.549026	29.460352
364.305082	20404.328079	29.465370
364.651117	20430.672826	29.470388
365.389522	20474.005526	29.475405
365.528357	20515.575735	29.480423
365.975539	20536.196037	29.485440
366.306774	20559.904649	29.490458
366.448015	20593.200458	29.495476
366.671660	20624.419286	29.500493
367.371929	20662.003546	29.505511
367.617840	20694.613896	29.510528
367.797716	20726.212164	29.515546
368.084818	20756.922631	29.520564
368.890753	20765.019707	29.525581
369.076732	20800.464998	29.530599
369.341092	20836.259979	29.535616
369.718282	20865.551225	29.540634
370.096737	20887.181157	29.545652
370.739438	20912.542876	29.550669
370.894185	20956.674738	29.555687
371.118986	20985.354513	29.560704
371.617649	21001.601899	29.565722
371.691011	21032.374981	29.570740
372.572166	21067.830538	29.575757
372.869441	21108.847966	29.580775
373.055078	21130.609381	29.585792
373.634231	21136.836670	29.590810
373.885275	21179.726782	29.595828
374.320769	21215.218440	29.600845
374.425101	21248.884230	29.605863
374.644211	21296.573762	29.610880
375.257846	21326.723736	29.615898
375.286650	21362.902420	29.620916
376.116200	21377.265298	29.625933
376.079611	21436.522646	29.630951
376.066622	21478.224381	29.635968
376.587722	21510.634804	29.640986
377.035955	21551.904261	29.646004
377.710276	21592.948876	29.651021
377.937886	21636.707922	29.656039
378.476230	21693.935340	29.661056
379.183542	21712.625551	29.666074
379.188286	21760.192598	29.671092
379.768999	21801.292600	29.676109
380.299785	21811.062548	29.681127
380.226814	21857.105663	29.686144
381.177154	21903.251015	29.691162
381.389373	21948.142168	29.696180
381.534970	21975.499883	29.701197
381.922939	22000.002023	29.706215
382.664041	22045.919062	29.711232
383.280994	22093.923506	29.716250
383.459099	22120.251374	29.721268
384.292725	22131.056106	29.726285
384.444811	22186.589661	29.731303
384.925507	22207.449281	29.736320
385.078562	22239.958178	29.741338
385.693115	22265.586733	29.746356
386.101190	22298.922270	29.751373
386.357317	22314.980836	29.756391
386.834838	22352.156406	29.761408
387.233169	22403.771796	29.766426
387.407909	22431.052923	29.771444
388.080641	22450.460685	29.776461
388.691173	22474.854236	29.781479
388.823017	22501.344845	29.786496
389.349914	22531.902306	29.791514
389.404635	22550.376497	29.796532
390.215655	22597.237301	29.801549
390.514220	22630.922661	29.806567
390.606094	22650.910604	29.811584
391.204809	22665.916545	29.816602
391.392183	22710.630969	29.821620
391.928610	22752.949836	29.826637
392.155079	22772.603534	29.831655
392.215227	22808.884218	29.836672
392.730950	22831.000071	29.841690
393.017018	22882.510933	29.846708
393.388060	22906.514276	29.851725
394.083150	22930.568177	29.856743
394.155296	22982.844633	29.861760
394.336452	22991.635651	29.866778
394.526634	23023.957054	29.871796
394.917977	23064.632663	29.876813
395.553489	23128.186765	29.881831
395.350371	23174.521437	29.886848
396.099796	23183.491433	29.891866
396.165200	23227.621972	29.896884
396.657448	23281.652498	29.901901
397.121334	23346.243220	29.906919
397.478323	23367.919329	29.911936
397.919453	23399.124758	29.916954
398.098075	23469.408900	29.921972
398.525132	23512.357897	29.926989
399.211595	23546.802435	29.932007
399.436895	23593.154203	29.937024
400.198279	23640.245272	29.942042
400.329230	23678.803824	29.947060
400.991479	23720.885195	29.952077
401.576130	23765.563601	29.957095
401.895393	23811.041178	29.962112
402.298691	23835.868259	29.967130
402.664664	23882.277994	29.972148
403.397241	23933.913822	29.977165
403.899322	23980.108991	29.982183
404.100617	24002.478564	29.987200
404.886005	24041.341349	29.992218
405.233560	24085.641954	29.997236
405.709298	24103.250509	30.002253
406.333716	24127.946895	30.007271
406.851055	24159.822270	30.012288
407.152219	24191.856395	30.017306
407.557230	24235.348526	30.022324
407.781206	24253.862849	30.027341
408.244952	24288.214832	30.032359
408.320321	24329.074980	30.037376
408.772352	24352.592425	30.042394
409.397668	24394.632704	30.047412
409.965877	24435.845292	30.052429
410.271096	24471.486774	30.057447
410.359616	24518.932686	30.062464
410.933348	24534.854193	30.067482
411.568909	24570.646288	30.072500
411.802623	24617.693235	30.077517
412.406666	24636.566180	30.082535
412.390518	24671.081780	30.087552
413.033277	24709.392586	30.092570
413.389127	24755.047987	30.097588
413.711532	24791.332188	30.102605
414.194925	24813.509601	30.107623
414.173922	24839.570305	30.112640
414.997484	24895.730332	30.117658
415.355956	24953.231925	30.122676
415.635153	24991.266001	30.127693
416.192790	25003.813203	30.132711
416.298531	25047.372627	30.137728
416.642112	25100.131134	30.142746
417.351584	25125.546552	30.147764
417.801157	25183.333463	30.152781
418.490727	25222.460775	30.157799
418.499889	25254.562492	30.162816
419.206070	25291.525457	30.167834
419.440622	25344.668548	30.172852
419.708277	25369.376805	30.177869
420.518210	25398.158252	30.182887
420.924900	25442.834228	30.187904
421.074506	25483.662823	30.192922
421.325963	25520.939498	30.197940
421.767249	25550.732912	30.202957
422.417530	25612.682437	30.207975
422.356061	25632.656667	30.212992
422.873272	25655.701577	30.218010
423.303277	25710.261044	30.223028
423.808729	25764.543316	30.228045
424.322883	25797.019922	30.233063
424.432065	25836.973018	30.238080
425.117317	25865.758511	30.243098
425.314931	25936.232675	30.248116
425.571307	25962.553614	30.253133
426.012717	25999.844114	30.258151
426.144754	26053.405298	30.263168
426.695176	26098.502352	30.268186
427.418240	26147.155214	30.273204
427.565657	26204.886708	30.278221
428.257019	26264.364027	30.283239
428.354511	26314.208742	30.288256
428.945620	26333.448401	30.293274
429.852016	26392.477506	30.298292
430.074891	26459.666589	30.303309
430.385780	26490.612244	30.308327
430.948970	26530.441512	30.313344
431.264871	26582.226785	30.318362
432.016856	26630.057838	30.323380
432.261361	26674.543073	30.328397
432.984081	26716.568291	30.333415
433.609635	26744.340141	30.338432
434.037335	26798.923977	30.343450
434.542274	26856.434620	30.348468
434.531610	26885.677411	30.353485
435.088454	26911.825607	30.358503
435.516734	26957.550654	30.363520
436.133040	27018.197319	30.368538
436.254783	27056.064903	30.373556
436.413158	27106.952120	30.378573
437.094433	27156.217162	30.383591
437.463206	27206.978460	30.388608
437.928483	27249.369216	30.393626
438.827616	27286.257338	30.398644
438.952496	27327.203243	30.403661
439.423587	27375.166364	30.408679
439.814473	27419.266654	30.413696
440.294824	27461.989767	30.418714
440.986786	27526.714855	30.423732
441.257812	27583.271502	30.428749
442.046598	27596.183003	30.433767
442.473799	27648.364716	30.438784
443.247020	27700.520973	30.443802
443.611836	27735.896091	30.448820
443.664627	27763.557621	30.453837
444.397026	27794.831843	30.458855
444.639269	27845.332072	30.463872
444.938532	27895.854571	30.468890
445.275444	27935.338122	30.473908
445.818234	27960.474642	30.478925
446.531784	28006.585900	30.483943
446.707910	28066.856382	30.488960
446.827003	28118.658311	30.493978
447.231260	28161.058250	30.498996
447.530806	28191.991510	30.504013
448.345600	28249.725328	30.509031
448.643594	28317.836603	30.514048
448.933390	28346.295766	30.519066
449.536821	28397.299391	30.524084
449.678095	28455.271317	30.529101
450.611466	28494.219204	30.534119
451.483143	28531.764305	30.539136
452.018649	28567.491442	30.544154
452.299168	28594.999991	30.549172
452.935701	28642.992951	30.554189
453.788545	28658.932157	30.559207
454.362177	28667.095113	30.564224
454.554053	28711.026574	30.569242
455.445321	28742.402453	30.574260
455.129325	28766.376170	30.579277
455.837974	28793.461047	30.584295
455.917525	28833.620016	30.589312
456.259199	28861.771813	30.594330
457.026443	28896.890443	30.599348
457.199715	28960.706726	30.604365
458.015131	28989.458642	30.609383
458.158513	29019.330971	30.614400
458.305635	29052.801742	30.619418
458.985676	29101.845472	30.624436
459.098600	29152.787264	30.629453
459.563063	29185.966149	30.634471
460.146470	29223.601386	30.639488
460.233710	29283.745713	30.644506
460.609205	29334.313467	30.649524
461.005880	29397.842120	30.654541
461.558066	29453.714994	30.659559
461.567604	29502.671894	30.664576
462.317351	29563.061047	30.669594
462.814178	29628.053393	30.674612
463.000433	29682.116913	30.679629
464.222493	29715.752084	30.684647
464.629616	29784.232806	30.689664
464.936849	29838.078104	30.694682
465.397707	29887.769071	30.699700
465.325166	29946.544690	30.704717
466.136140	29998.865711	30.709735
466.485552	30052.711018	30.714752
466.994108	30111.776055	30.719770
467.803692	30173.725218	30.724788
467.976770	30226.994537	30.729805
468.802890	30280.831210	30.734823
469.262020	30348.974353	30.739840
469.547065	30396.512911	30.744858
470.086001	30465.640153	30.749876
470.580844	30508.595556	30.754893
471.055198	30549.847850	30.759911
471.500851	30628.356948	30.764928
472.082229	30686.547569	30.769946
472.793806	30726.246912	30.774964
473.002823	30774.918934	30.779981
473.821189	30837.988894	30.784999
474.445259	30886.627372	30.790016
474.635437	30930.776106	30.795034
474.953809	30981.197218	30.800052
475.108504	31048.753006	30.805069
476.175739	31081.618294	30.810087
476.479328	31156.200496	30.815104
476.526273	31204.244324	30.820122
477.586628	31240.038563	30.825140
477.813730	31295.990000	30.830157
478.363898	31363.320797	30.835175
478.945299	31398.352176	30.840192
479.088841	31485.050971	30.845210
479.469625	31520.169361	30.850228
480.157775	31583.910249	30.855245
480.802208	31627.938397	30.860263
481.091092	31695.897261	30.865280
481.039560	31765.814931	30.870298
482.042059	31801.121433	30.875316
482.374045	31853.148590	30.880333
482.338249	31906.252487	30.885351
483.311759	31970.796289	30.890368
483.321465	32034.206058	30.895386
483.972128	32073.448474	30.900404
484.358513	32137.805939	30.905421
485.101585	32200.968987	30.910439
485.596781	32237.552693	30.915456
485.800441	32315.301721	30.920474
486.898253	32362.503176	30.925492
486.992512	32425.146384	30.930509
487.555786	32468.678970	30.935527
488.320853	32523.785155	30.940544
488.633855	32578.234247	30.945562
489.377469	32637.253249	30.950580
489.781592	32694.088534	30.955597
490.336403	32727.290812	30.960615
490.838198	32801.355128	30.965632
491.363982	32861.606587	30.970650
491.927107	32906.345475	30.975668
492.547105	32968.137131	30.980685
493.024099	33005.971662	30.985703
493.237154	33044.897323	30.990720
493.694748	33121.876029	30.995738
494.193448	33182.432788	31.000756
494.745555	33230.619588	31.005773
495.488349	33275.746204	31.010791
496.278231	33339.492461	31.015808
496.522686	33406.108634	31.020826
497.174332	33439.151134	31.025844
497.323467	33521.246395	31.030861
497.832354	33566.866724	31.035879
498.425879	33608.084473	31.040896
498.735713	33664.171788	31.045914
499.632965	33708.112930	31.050932
499.765708	33756.086480	31.055949
500.002205	33817.991795	31.060967
500.658120	33903.390573	31.065984
500.753014	33969.563464	31.071002
501.568747	34010.802247	31.076020
502.047816	34079.410976	31.081037
502.331262	34150.402891	31.086055
503.183249	34214.063179	31.091072
503.418906	34271.338407	31.096090
504.191747	34341.152245	31.101108
504.558804	34399.560993	31.106125
505.651495	34434.586565	31.111143
506.333605	34495.515104	31.116160
506.598546	34575.542081	31.121178
507.524034	34622.632942	31.126196
507.742845	34654.625943	31.131213
508.369100	34694.411493	31.136231
509.264029	34769.122778	31.141248
509.766191	34820.038880	31.146266
510.328394	34862.122977	31.151284
510.786689	34904.243269	31.156301
510.997903	34945.038219	31.161319
511.669091	34988.833732	31.166336
511.603961	35029.813355	31.171354
512.128653	35096.623113	31.176372
512.620020	35176.214677	31.181389
512.622456	35226.043847	31.186407
513.639857	35270.398170	31.191424
513.963233	35352.198637	31.196442
514.688485	35391.284683	31.201460
515.265665	35453.691648	31.206477
515.549967	35498.338020	31.211495
516.658157	35572.638821	31.216512
517.088860	35632.303295	31.221530
517.783385	35660.275238	31.226548
517.949452	35686.870381	31.231565
518.616853	35734.691565	31.236583
518.654366	35807.923788	31.241600
519.055997	35860.986273	31.246618
519.850125	35895.470830	31.251636
520.082990	35961.173980	31.256653
520.476955	36030.012585	31.261671
520.964721	36076.267670	31.266688
521.257714	36136.849594	31.271706
521.753931	36195.874032	31.276724
522.083483	36268.665470	31.281741
522.564056	36340.211057	31.286759
523.117571	36398.885903	31.291776
523.218190	36468.879107	31.296794
524.069258	36552.645911	31.301812
524.466479	36629.353217	31.306829
524.994651	36712.533514	31.311847
526.049112	36770.060237	31.316864
526.038392	36829.120009	31.321882
526.928376	36902.850212	31.326900
527.249297	36976.911386	31.331917
527.820561	37059.382464	31.336935
528.216928	37116.144871	31.341952
529.256760	37175.890623	31.346970
530.052520	37250.972693	31.351988
530.310436	37336.122368	31.357005
530.728200	37390.840347	31.362023
531.644338	37437.930754	31.367040
532.059532	37512.051154	31.372058
532.879717	37580.673862	31.377076
533.406626	37649.992211	31.382093
534.264967	37701.409990	31.387111
535.206456	37744.482832	31.392128
535.577548	37793.699700	31.397146
536.126224	37866.811748	31.402164
536.516206	37924.650757	31.407181
536.981098	37982.786853	31.412199
537.840841	38034.666113	31.417216
537.856121	38085.662496	31.422234
538.365535	38158.179443	31.427252
538.899156	38214.480836	31.432269
539.335043	38270.224171	31.437287
540.008592	38340.038534	31.442304
540.511294	38407.552309	31.447322
541.055609	38464.603830	31.452340
541.529614	38535.487058	31.457357
541.879498	38595.443024	31.462375
542.831067	38641.855369	31.467392
543.063644	38716.364368	31.472410
543.743676	38777.020691	31.477428
544.422032	38854.284405	31.482445
544.658523	38916.955402	31.487463
545.503092	38968.076107	31.492480
545.571170	39040.252904	31.497498
546.400288	39114.311543	31.502516
546.816351	39165.601420	31.507533
547.143722	39242.905834	31.512551
548.122223	39295.233060	31.517568
548.954553	39346.224304	31.522586
549.713465	39420.390478	31.527604
550.294537	39471.988520	31.532621
550.520890	39527.817694	31.537639
551.231877	39575.348420	31.542656
551.419771	39650.449381	31.547674
551.879485	39715.222990	31.552692
552.370074	39770.302291	31.557709
552.591437	39838.331843	31.562727
553.503943	39914.137981	31.567744
553.617387	39966.979305	31.572762
553.978316	40018.397486	31.577780
554.852463	40100.226480	31.582797
555.263596	40174.525779	31.587815
555.827257	40239.271468	31.592832
556.507915	40296.666070	31.597850
556.905524	40364.131920	31.602868
557.367632	40437.931499	31.607885
557.941587	40493.646267	31.612903
558.724244	40548.528191	31.617920
558.784213	40635.244308	31.622938
559.386089	40730.503910	31.627956
559.818818	40791.763348	31.632973
560.853243	40860.344212	31.637991
561.517290	40931.432694	31.643008
562.081932	41000.640886	31.648026
562.569699	41088.020783	31.653044
563.471493	41139.545348	31.658061
563.905099	41196.298656	31.663079
564.694584	41265.019350	31.668096
565.219972	41337.451705	31.673114
565.590792	41396.466548	31.678132
566.389740	41464.769781	31.683149
566.787637	41531.040453	31.688167
567.596634	41608.265918	31.693184
568.080682	41695.393663	31.698202
568.548215	41742.645154	31.703220
568.892954	41793.872167	31.708237
569.394283	41886.954324	31.713255
570.101076	41969.267592	31.718272
570.870686	42046.409875	31.723290
571.321078	42105.578007	31.728308
572.242973	42155.978386	31.733325
572.907630	42250.197038	31.738343
573.363426	42321.009668	31.743360
573.978463	42376.117335	31.748378
574.356534	42458.550228	31.753396
575.053682	42500.999238	31.758413
575.431136	42574.619415	31.763431
575.671690	42660.949143	31.768448
576.153985	42730.632048	31.773466
576.391078	42820.609064	31.778484
577.190097	42898.643423	31.783501
577.741754	42978.824502	31.788519
578.260092	43062.490158	31.793536
578.926394	43119.728703	31.798554
579.694508	43201.443906	31.803572
579.946579	43285.523894	31.808589
580.616217	43387.279626	31.813607
581.322244	43464.119535	31.818624
581.973216	43535.652774	31.823642
582.713372	43622.662136	31.828660
583.100259	43706.961700	31.833677
583.805095	43795.695037	31.838695
584.585551	43864.824737	31.843712
584.801491	43944.030009	31.848730
585.549717	44041.056822	31.853748
586.426093	44114.989055	31.858765
586.870695	44187.158718	31.863783
587.165148	44258.365339	31.868800
588.144351	44340.868378	31.873818
588.289766	44424.936442	31.878836
589.549316	44483.978584	31.883853
589.813831	44569.536671	31.888871
590.416037	44639.551098	31.893888
591.149312	44702.835479	31.898906
591.521808	44777.478670	31.903924
592.732426	44842.269521	31.908941
593.278332	44931.252392	31.913959
593.841318	44995.478287	31.918976
594.443003	45042.643484	31.923994
594.861220	45099.187227	31.929012
595.668272	45159.922689	31.934029
595.964091	45240.758845	31.939047
596.475056	45307.715840	31.944064
597.003729	45363.512851	31.949082
597.580640	45437.998653	31.954100
598.360886	45526.260573	31.959117
598.815044	45605.591457	31.964135
599.084300	45653.776045	31.969152
599.885045	45745.846337	31.974170
600.110820	45826.816579	31.979188
601.035645	45887.108745	31.984205
601.811652	45970.628173	31.989223
602.289207	46066.649453	31.994240
602.693855	46134.833052	31.999258
602.932301	46211.802623	32.004276
603.635250	46298.903307	32.009293
604.438148	46396.861645	32.014311
605.189996	46460.729889	32.019328
605.836952	46527.312031	32.024346
606.222748	46625.034191	32.029364
607.223081	46688.499081	32.034381
608.122236	46776.876734	32.039399
608.703247	46856.409842	32.044416
609.460351	46925.617941	32.049434
609.783227	47014.432890	32.054452
610.806887	47092.318348	32.059469
611.426254	47179.951600	32.064487
611.718286	47227.561832	32.069504
612.482238	47291.213049	32.074522
612.784625	47392.855605	32.079540
613.544107	47478.957841	32.084557
613.704272	47561.193630	32.089575
614.356511	47613.911025	32.094592
615.527333	47696.094161	32.099610
615.719053	47801.520972	32.104628
616.134117	47881.003734	32.109645
616.651028	47951.208867	32.114663
617.322225	48028.951182	32.119680
618.077483	48117.491535	32.124698
618.641246	48211.864458	32.129716
619.086060	48309.127781	32.134733
619.979932	48392.985881	32.139751
620.725530	48478.911843	32.144768
621.731371	48561.520716	32.149786
622.115382	48652.259477	32.154804
622.545243	48726.141628	32.159821
623.243680	48805.985674	32.164839
623.849551	48883.284433	32.169856
624.467828	48959.220475	32.174874
625.264263	49050.672997	32.179892
625.791087	49137.730669	32.184909
626.587068	49220.124460	32.189927
627.241457	49302.611466	32.194944
627.567284	49397.894844	32.199962
628.177155	49481.154168	32.204980
629.155705	49559.448852	32.209997
629.504543	49633.786866	32.215015
629.817723	49713.698367	32.220032
631.029648	49813.264811	32.225050
631.407262	49902.062205	32.230068
632.451238	49965.698308	32.235085
632.861738	50034.738223	32.240103
633.471893	50120.318213	32.245120
634.092424	50203.774737	32.250138
634.572752	50280.888345	32.255156
635.288223	50319.657327	32.260173
636.394036	50399.188169	32.265191
636.624327	50494.044388	32.270208
637.448750	50564.776866	32.275226
637.756980	50637.183337	32.280244
638.279168	50727.015479	32.285261
638.834770	50798.529041	32.290279
638.838589	50871.255107	32.295296
639.440119	50965.142837	32.300314
640.114758	51069.810128	32.305332
641.189855	51151.155606	32.310349
641.870639	51233.090799	32.315367
641.891683	51344.970131	32.320384
642.851670	51440.010559	32.325402
643.441636	51530.975376	32.330420
644.271657	51634.066279	32.335437
644.757055	51719.222422	32.340455
645.321990	51814.538392	32.345472
646.028723	51905.166722	32.350490
646.528966	52006.864467	32.355508
647.475759	52102.428311	32.360525
648.374809	52198.846933	32.365543
648.546574	52288.848496	32.370560
649.491037	52387.161851	32.375578
650.179238	52494.064440	32.380596
651.205819	52580.891054	32.385613
651.873773	52665.222184	32.390631
652.301542	52752.325331	32.395648
653.590568	52843.626247	32.400666
653.677332	52919.918497	32.405684
654.416706	53013.133380	32.410701
655.138321	53113.587587	32.415719
655.941987	53193.372599	32.420736
656.981811	53279.546381	32.425754
657.465769	53371.428093	32.430772
658.190543	53448.725687	32.435789
658.896975	53537.823576	32.440807
659.467739	53629.028894	32.445824
660.530155	53710.760012	32.450842
661.002903	53798.691140	32.455860
661.435606	53890.356367	32.460877
661.960105	53964.502123	32.465895
662.367420	54058.648649	32.470912
663.113053	54161.640669	32.475930
663.497561	54259.158993	32.480948
664.308468	54344.516182	32.485965
664.558470	54422.379338	32.490983
665.116139	54540.338435	32.496000
666.046712	54641.141937	32.501018
666.530870	54738.046060	32.506036
667.205283	54841.489344	32.511053
667.831335	54939.350233	32.516071
668.279695	55036.438640	32.521088
669.256859	55136.902191	32.526106
670.065489	55255.828660	32.531124
670.764767	55348.334873	32.536141
671.243143	55446.987124	32.541159
672.062965	55562.249405	32.546176
672.644578	55660.771968	32.551194
673.369694	55758.298404	32.556212
674.072687	55872.874228	32.561229
675.092960	55966.145344	32.566247
675.290153	56066.786712	32.571264
676.161509	56155.831446	32.576282
677.072258	56255.743116	32.581300
677.862669	56345.231694	32.586317
678.322327	56433.568580	32.591335
678.755885	56542.576186	32.596352
679.844241	56602.486645	32.601370
680.160701	56707.837448	32.606388
681.078253	56801.957165	32.611405
681.681870	56876.953856	32.616423
681.977688	56968.314964	32.621440
682.573625	57079.908105	32.626458
683.404593	57187.179353	32.631476
684.203595	57260.982699	32.636493
685.032321	57365.904927	32.641511
685.256324	57486.419935	32.646528
685.970755	57578.795164	32.651546
686.796606	57677.369648	32.656564
687.628846	57775.229596	32.661581
688.335384	57885.178895	32.666599
688.863456	57979.494926	32.671616
689.714140	58068.305314	32.676634
690.263212	58165.847490	32.681652
690.674941	58275.190521	32.686669
691.629220	58384.634115	32.691687
692.206055	58516.912810	32.696704
692.653732	58600.276014	32.701722
693.314948	58722.457644	32.706740
694.126236	58827.163033	32.711757
695.057923	58930.553754	32.716775
695.626975	59048.089396	32.721792
696.585240	59173.940176	32.726810
697.201789	59291.033412	32.731828
698.148367	59375.732899	32.736845
698.860289	59470.562758	32.741863
699.499228	59573.265855	32.746880
700.626791	59665.348781	32.751898
701.057088	59783.404555	32.756916
701.757850	59904.285198	32.761933
702.719336	60013.957737	32.766951
703.231744	60103.288057	32.771968
704.191386	60190.168932	32.776986
704.541801	60299.520570	32.782004
705.685455	60425.999508	32.787021
706.520620	60513.508987	32.792039
707.026416	60607.759002	32.797056
707.522748	60716.671750	32.802074
708.374033	60828.092114	32.807092
708.855864	60925.703138	32.812109
709.574216	61030.391198	32.817127
710.109023	61150.301987	32.822144
710.804327	61259.039471	32.827162
711.668527	61362.441286	32.832180
711.758546	61476.278612	32.837197
712.931867	61581.412610	32.842215
713.607167	61694.718469	32.847232
714.682616	61796.640444	32.852250
715.152589	61913.691059	32.857268
715.718270	62031.977847	32.862285
716.610736	62150.679024	32.867303
717.260869	62248.862722	32.872320
718.058478	62350.492110	32.877338
718.622046	62460.477549	32.882356
719.236306	62581.344339	32.887373
720.170168	62689.841586	32.892391
720.692522	62810.440525	32.897408
721.740165	62914.888069	32.902426
722.510810	63018.206374	32.907444
723.111552	63135.419420	32.912461
723.768068	63248.136680	32.917479
724.429812	63352.138276	32.922496
725.363971	63444.232525	32.927514
725.689113	63554.358069	32.932532
726.312373	63667.557159	32.937549
727.463255	63752.936564	32.942567
727.945503	63869.857400	32.947584
728.591872	63987.902098	32.952602
729.584820	64078.011253	32.957620
729.977838	64200.365241	32.962637
730.795795	64285.511120	32.967655
731.351708	64390.850137	32.972672
732.202391	64513.155704	32.977690
732.568477	64638.721239	32.982708
733.451624	64744.014358	32.987725
734.484088	64845.351969	32.992743
735.209637	64958.851034	32.997760
735.816289	65079.993051	33.002778
737.191052	65180.567884	33.007796
737.374831	65295.447693	33.012813
738.353461	65417.901873	33.017831
739.048320	65532.161345	33.022848
739.989287	65623.840805	33.027866
740.630983	65755.290256	33.032884
741.026905	65884.815336	33.037901
741.923354	65977.072601	33.042919
742.430829	66095.695973	33.047936
743.286848	66213.055162	33.052954
744.285566	66319.696287	33.057972
744.664126	66447.217681	33.062989
745.579758	66556.212541	33.068007
746.667789	66688.390692	33.073024
747.071218	66813.931727	33.078042
747.737474	66929.183444	33.083060
748.550285	67050.442067	33.088077
749.704058	67159.704202	33.093095
750.174663	67281.260892	33.098112
751.169475	67384.128007	33.103130
752.340036	67499.192155	33.108148
752.790010	67611.050869	33.113165
753.705154	67721.821939	33.118183
754.345312	67846.893951	33.123200
755.019593	67962.200652	33.128218
755.863410	68075.273773	33.133236
756.337175	68203.118957	33.138253
757.266019	68316.052912	33.143271
757.885448	68433.666030	33.148288
758.291594	68552.421327	33.153306
759.268746	68695.731466	33.158324
759.554023	68816.290952	33.163341
760.682428	68917.544173	33.168359
761.019934	69054.684841	33.173376
762.055234	69181.943859	33.178394
763.050834	69323.750644	33.183412
763.453437	69441.335688	33.188429
764.698614	69552.649916	33.193447
765.298197	69708.704949	33.198464
765.897416	69839.068224	33.203482
767.170333	69954.799143	33.208500
767.827756	70064.689509	33.213517
768.575006	70182.215464	33.218535
769.143231	70331.389105	33.223552
769.910099	70464.339651	33.228570
770.789891	70571.053768	33.233588
771.199041	70677.795562	33.238605
772.462338	70824.657741	33.243623
773.207828	70946.967966	33.248640
773.702940	71091.701745	33.253658
774.907387	71216.997817	33.258676
775.358208	71321.124784	33.263693
776.118914	71416.242025	33.268711
777.006067	71548.515654	33.273728
777.642367	71673.832373	33.278746
778.323960	71767.503724	33.283764
779.102879	71902.117845	33.288781
780.326515	72016.173709	33.293799
781.026645	72126.118310	33.298816
781.312610	72247.152515	33.303834
782.367394	72374.560336	33.308852
782.834714	72486.701331	33.313869
783.789151	72619.059027	33.318887
784.216679	72748.437918	33.323904
784.900511	72853.811145	33.328922
786.120222	72991.653637	33.333940
786.717885	73130.592456	33.338957
787.553986	73250.833322	33.343975
788.634868	73385.830590	33.348992
789.445924	73498.090854	33.354010
790.122370	73629.419443	33.359028
790.962193	73765.660319	33.364045
791.942969	73884.445471	33.369063
792.670253	73999.276798	33.374080
793.500518	74127.130497	33.379098
794.454735	74255.445067	33.384116
795.070379	74393.288816	33.389133
795.881081	74517.025179	33.394151
796.596986	74637.761592	33.399168
796.923590	74760.991204	33.404186
797.946864	74902.533407	33.409204
798.470137	75053.726750	33.414221
799.276939	75191.246817	33.419239
800.234096	75312.282316	33.424256
801.254452	75445.474939	33.429274
801.892347	75589.513588	33.434292
802.287637	75756.460232	33.439309
803.638717	75874.784139	33.444327
804.693706	75996.521901	33.449344
805.292117	76151.100100	33.454362
806.127035	76304.995296	33.459380
806.762625	76440.072538	33.464397
807.551646	76567.302404	33.469415
808.491469	76692.591908	33.474432
809.060032	76849.032947	33.479450
810.704991	76992.396010	33.484468
811.335609	77117.587228	33.489485
812.131434	77245.433373	33.494503
812.999974	77383.349201	33.499520
813.500111	77517.652283	33.504538
814.396814	77652.776119	33.509556
815.175402	77810.606011	33.514573
816.256045	77936.669939	33.519591
817.077354	78058.287016	33.524608
817.207615	78201.617173	33.529626
818.246699	78368.736760	33.534644
818.939733	78504.443377	33.539661
819.903699	78629.449029	33.544679
820.820430	78760.705669	33.549696
821.281669	78925.970560	33.554714
822.079992	79079.416906	33.559732
822.852492	79220.598399	33.564749
824.046057	79342.173737	33.569767
825.619858	79474.635371	33.574784
826.381008	79618.952107	33.579802
827.571718	79737.209490	33.584820
828.054598	79867.639861	33.589837
829.127530	80010.813437	33.594855
829.874152	80120.967890	33.599872
830.782044	80241.855296	33.604890
831.694639	80375.639586	33.609908
832.540127	80485.893375	33.614925
833.131425	80606.601005	33.619943
833.886746	80723.461746	33.624960
834.486408	80840.310849	33.629978
835.483588	80955.178352	33.634996
835.988668	81088.844448	33.640013
836.613946	81201.162247	33.645031
837.755811	81332.542393	33.650048
837.637404	81466.294712	33.655066
838.703218	81604.988608	33.660084
839.371229	81778.760990	33.665101
840.168580	81906.772932	33.670119
840.986390	82049.109786	33.675136
841.442611	82206.233422	33.680154
842.440292	82349.238299	33.685172
843.230128	82495.548821	33.690189
844.028842	82657.078711	33.695207
844.767249	82803.178316	33.700224
845.670799	82970.500266	33.705242
846.709860	83140.369411	33.710260
847.323934	83295.039072	33.715277
848.259619	83432.911697	33.720295
849.098694	83590.823106	33.725312
849.662945	83776.318568	33.730330
850.586020	83925.475740	33.735348
851.471112	84100.963502	33.740365
851.939417	84269.461333	33.745383
853.420015	84424.919244	33.750400
854.145679	84587.518780	33.755418
855.328879	84752.087353	33.760436
856.199009	84934.435482	33.765453
857.232258	85081.519609	33.770471
858.024066	85238.260861	33.775488
858.419694	85410.252366	33.780506
859.591857	85555.241484	33.785524
860.657992	85731.009223	33.790541
861.294879	85891.728355	33.795559
862.574803	86048.046575	33.800576
863.463934	86220.734525	33.805594
864.405492	86358.358113	33.810612
865.226237	86514.559186	33.815629
866.121132	86681.099912	33.820647
867.371606	86825.407124	33.825664
868.210203	86992.864148	33.830682
869.156391	87155.553005	33.835700
869.592052	87304.901209	33.840717
870.933831	87466.109661	33.845735
871.884758	87633.495824	33.850752
873.016947	87773.867664	33.855770
874.001693	87900.926845	33.860788
875.062310	88052.543062	33.865805
875.934343	88199.521832	33.870823
877.161213	88348.163987	33.875840
877.707807	88471.381981	33.880858
878.645476	88609.272669	33.885876
879.574441	88764.363712	33.890893
880.352086	88907.357226	33.895911
881.134031	89048.326083	33.900928
881.858633	89201.384651	33.905946
882.652278	89343.701134	33.910964
883.360222	89501.668336	33.915981
884.314322	89654.122474	33.920999
884.908800	89808.307509	33.926016
885.406055	89959.877237	33.931034
886.416815	90107.072874	33.936052
887.398038	90262.032301	33.941069
888.093219	90439.535780	33.946087
889.107780	90579.399660	33.951104
890.054914	90706.746040	33.956122
890.687921	90861.539086	33.961140
891.707174	91029.722897	33.966157
892.421698	91183.397170	33.971175
893.128213	91328.549707	33.976192
893.841281	91503.185215	33.981210
894.703258	91651.959117	33.986228
895.452655	91797.031496	33.991245
896.069066	91982.615458	33.996263
897.413248	92166.663142	34.001280
897.842422	92321.980310	34.006298
898.567116	92477.755973	34.011316
899.608638	92663.066195	34.016333
900.321071	92833.749892	34.021351
901.468709	92996.224346	34.026368
902.108448	93177.744431	34.031386
903.389191	93355.793179	34.036404
904.381106	93531.574610	34.041421
905.215898	93727.724051	34.046439
906.080504	93894.086567	34.051456
906.953166	94075.005367	34.056474
907.503036	94240.219744	34.061492
908.830797	94439.217550	34.066509
909.193653	94625.389103	34.071527
910.632780	94795.371789	34.076544
911.255892	94981.965135	34.081562
912.919088	95176.147775	34.086580
913.909247	95347.803415	34.091597
914.575330	95520.899885	34.096615
915.742732	95685.003131	34.101632
917.063924	95864.430800	34.106650
917.988567	96049.203993	34.111668
919.148833	96233.933352	34.116685
920.156698	96397.732270	34.121703
921.226523	96536.716574	34.126720
922.197021	96729.437239	34.131738
923.124031	96899.379905	34.136756
924.190014	97053.350020	34.141773
924.914815	97224.714521	34.146791
926.143578	97369.513301	34.151808
927.118777	97540.262650	34.156826
928.019476	97686.111234	34.161844
929.227359	97851.849074	34.166861
930.310062	98016.443989	34.171879
931.209558	98164.625010	34.176896
932.148791	98341.051149	34.181914
932.752983	98480.838594	34.186932
933.889861	98645.587000	34.191949
934.351972	98811.751910	34.196967
935.229355	98964.315477	34.201984
936.180692	99138.947522	34.207002
937.032108	99330.391452	34.212020
937.731907	99494.236453	34.217037
938.360774	99658.043596	34.222055
939.723782	99839.639259	34.227072
940.407711	100003.034428	34.232090
941.012985	100183.700509	34.237108
941.955498	100375.928715	34.242125
942.700778	100565.601754	34.247143
943.685984	100732.098224	34.252160
944.408701	100916.232020	34.257178
945.093389	101112.965210	34.262196
945.961299	101316.038425	34.267213
947.004480	101503.694149	34.272231
948.336231	101667.556617	34.277248
948.973220	101872.014564	34.282266
950.195418	102079.948196	34.287284
951.285235	102260.447862	34.292301
952.166438	102412.512596	34.297319
953.098318	102590.520933	34.302336
953.981485	102770.393575	34.307354
955.260475	102934.811084	34.312372
956.140794	103124.468340	34.317389
956.818629	103303.473280	34.322407
958.224878	103463.086757	34.327424
959.154839	103640.216355	34.332442
960.690756	103800.348693	34.337460
961.539702	103972.530167	34.342477
962.230735	104167.956336	34.347495
963.327455	104326.435979	34.352512
964.091723	104496.653183	34.357530
964.798354	104670.388727	34.362548
966.029307	104848.116448	34.367565
966.732493	105031.574049	34.372583
968.197508	105204.858737	34.377600
969.091724	105401.311771	34.382618
969.878283	105562.642520	34.387636
970.902620	105731.678864	34.392653
971.998649	105930.730307	34.397671
973.031576	106120.270449	34.402688
973.911689	106288.935316	34.407706
974.544223	106479.658605	34.412724
976.058422	106650.981895	34.417741
976.305754	106850.148815	34.422759
977.382819	107040.175925	34.427776
978.446599	107235.918263	34.432794
979.389611	107427.135438	34.437812
980.386751	107612.000102	34.442829
981.178105	107813.123519	34.447847
982.202793	108007.877551	34.452864
983.362831	108190.059775	34.457882
984.040851	108407.138862	34.462900
985.341043	108612.439804	34.467917
986.358388	108793.041278	34.472935
987.562259	108980.186460	34.477952
988.915155	109172.197185	34.482970
989.586944	109377.924435	34.487988
991.129224	109577.062802	34.493005
991.826200	109762.675989	34.498023
992.963658	109922.126375	34.503040
993.845010	110126.292255	34.508058
994.684540	110341.498602	34.513076
995.714142	110527.834812	34.518093
996.120678	110721.241527	34.523111
997.377859	110917.181764	34.528128
998.279580	111108.964246	34.533146
998.943238	111331.971992	34.538164
999.962171	111511.438944	34.543181
1001.021293	111739.426022	34.548199
1001.871468	111966.144853	34.553216
1002.835698	112153.909107	34.558234
1003.761472	112369.573422	34.563252
1004.959452	112575.086279	34.568269
1005.679978	112779.070799	34.573287
1006.583233	112999.709316	34.578304
1007.760815	113228.310037	34.583322
1008.966285	113438.717739	34.588340
1009.975173	113625.180035	34.593357
1010.898712	113847.671500	34.598375
1012.215925	114072.202609	34.603392
1013.601069	114255.224814	34.608410
1014.712135	114485.544487	34.613428
1015.499615	114669.200164	34.618445
1016.447116	114862.977724	34.623463
1017.631338	115067.054737	34.628480
1018.750264	115278.542266	34.633498
1019.493314	115476.247016	34.638516
1021.083222	115655.089505	34.643533
1021.764105	115830.295348	34.648551
1022.401829	116038.434962	34.653568
1023.257398	116249.491963	34.658586
1024.170812	116450.507370	34.663604
1025.297523	116631.282240	34.668621
1025.858605	116840.061259	34.673639
1027.009700	117061.426112	34.678656
1028.159742	117260.672624	34.683674
1028.911594	117485.121977	34.688692
1030.043905	117696.587624	34.693709
1030.827779	117915.904061	34.698727
1031.817766	118105.351528	34.703744
1033.169590	118336.499460	34.708762
1033.843770	118564.682416	34.713780
1034.921427	118782.462054	34.718797
1035.789958	118997.731241	34.723815
1036.873560	119236.507382	34.728832
1038.067990	119473.480748	34.733850
1039.012641	119686.563322	34.738868
1040.400308	119919.707438	34.743885
1041.338430	120156.576742	34.748903
1042.202670	120359.009129	34.753920
1043.225925	120594.778337	34.758938
1044.280618	120838.083353	34.763956
1045.750811	121071.894757	34.768973
1046.941877	121291.233286	34.773991
1048.419751	121498.615405	34.779008
1049.407434	121738.403870	34.784026
1050.128199	121963.641169	34.789044
1051.183883	122178.586527	34.794061
1052.259118	122408.419118	34.799079
1053.367307	122651.831917	34.804096
1054.672780	122870.783355	34.809114
1055.434769	123112.977321	34.814132
1056.605341	123348.820631	34.819149
1057.282624	123570.326661	34.824167
1058.362784	123785.393848	34.829184
1059.789080	124029.893393	34.834202
1060.954689	124260.004382	34.839220
1062.142654	124497.146593	34.844237
1063.037480	124713.252254	34.849255
1064.094119	124942.778273	34.854272
1065.509879	125179.115320	34.859290
1066.625130	125405.657188	34.864308
1067.693391	125618.496605	34.869325
1068.536184	125849.991189	34.874343
1069.553837	126093.827512	34.879360
1070.996193	126312.642453	34.884378
1071.725760	126552.309939	34.889396
1073.044102	126778.562551	34.894413
1073.898615	127010.634462	34.899431
1074.947331	127256.059266	34.904448
1075.999576	127475.542724	34.909466
1077.395725	127717.479394	34.914484
1078.447751	127942.694766	34.919501
1079.465783	128151.669570	34.924519
1080.521965	128378.471718	34.929536
1081.636758	128619.764961	34.934554
1082.719465	128866.705395	34.939572
1083.777908	129080.255258	34.944589
1084.530708	129303.514886	34.949607
1085.569625	129557.096784	34.954624
1086.740115	129771.000521	34.959642
1087.512044	130030.257874	34.964660
1088.969763	130269.618980	34.969677
1089.909490	130488.293455	34.974695
1090.831803	130701.927748	34.979712
1092.146989	130920.885522	34.984730
1093.045705	131170.295726	34.989748
1094.336041	131397.182882	34.994765
1095.500365	131604.420501	34.999783
1096.419167	131817.175770	35.004800
1097.605423	132061.221997	35.009818
1098.604302	132295.502872	35.014836
1099.656572	132510.332283	35.019853
1100.809008	132755.137355	35.024871
1101.698992	132993.244123	35.029888
1102.665074	133209.093920	35.034906
1103.898669	133451.191032	35.039924
1104.996420	133707.687112	35.044941
1106.241654	133929.453507	35.049959
1107.067389	134173.854473	35.054976
1108.275998	134431.973341	35.059994
1109.383484	134672.249825	35.065012
1110.550512	134907.422304	35.070029
1111.610129	135154.809196	35.075047
1112.722541	135411.405294	35.080064
1114.084277	135653.903634	35.085082
1114.671585	135891.004482	35.090100
1115.913963	136152.681170	35.095117
1117.231392	136408.059714	35.100135
1118.293480	136653.467384	35.105152
1119.606229	136894.233653	35.110170
1120.705896	137167.833450	35.115188
1121.615378	137437.321373	35.120205
1122.837059	137674.786918	35.125223
1123.808193	137922.032056	35.130240
1124.834513	138183.291651	35.135258
1125.803531	138454.781211	35.140276
1127.022839	138713.946654	35.145293
1127.900614	138976.035772	35.150311
1128.938908	139255.697894	35.155328
1130.149140	139510.611179	35.160346
1131.441146	139778.166025	35.165364
1132.851271	140056.962091	35.170381
1134.027412	140327.722794	35.175399
1135.200295	140580.013258	35.180416
1136.769132	140850.624616	35.185434
1137.950244	141108.128707	35.190452
1139.369997	141363.452614	35.195469
1140.475604	141626.374409	35.200487
1141.271953	141895.093001	35.205504
1142.839138	142130.846951	35.210522
1143.851764	142389.732625	35.215540
1145.107581	142656.238568	35.220557
1146.345641	142893.992105	35.225575
1147.598585	143157.104290	35.230592
1149.029387	143433.300083	35.235610
1150.060267	143667.086357	35.240628
1151.133293	143913.559950	35.245645
1152.166184	144177.375630	35.250663
1152.817964	144442.942700	35.255680
1154.230734	144681.478603	35.260698
1155.195193	144962.531398	35.265716
1156.784053	145226.009677	35.270733
1157.574983	145475.013627	35.275751
1158.646452	145739.342019	35.280768
1159.920723	146010.106123	35.285786
1161.092846	146277.363895	35.290804
1162.175797	146534.366835	35.295821
1163.335585	146782.634401	35.300839
1164.412597	147054.922779	35.305856
1165.820885	147313.906669	35.310874
1166.713883	147575.310869	35.315892
1167.743531	147821.197732	35.320909
1168.851162	148064.397619	35.325927
1169.600379	148345.424128	35.330944
1171.017708	148594.321265	35.335962
1172.202919	148838.845181	35.340980
1173.511812	149086.711039	35.345997
1174.601912	149363.123761	35.351015
1175.939868	149626.764896	35.356032
1177.403350	149879.810318	35.361050
1178.374692	150125.900098	35.366068
1179.056619	150385.317700	35.371085
1180.258300	150666.376331	35.376103
1181.036583	150944.070045	35.381120
1182.085337	151215.658929	35.386138
1183.611553	151483.442294	35.391156
1184.595962	151760.435965	35.396173
1185.606158	152045.392311	35.401191
1186.675177	152333.435789	35.406208
1187.702150	152621.323560	35.411226
1189.285013	152905.443675	35.416244
1190.198095	153206.075995	35.421261
1191.445682	153505.361808	35.426279
1192.681912	153798.842842	35.431296
1193.803034	154079.369855	35.436314
1195.776678	154370.475945	35.441332
1196.783809	154674.491005	35.446349
1198.219751	154949.214063	35.451367
1199.524740	155223.351889	35.456384
1200.542140	155514.180638	35.461402
1202.205436	155812.921375	35.466420
1202.950579	156096.011402	35.471437
1204.624072	156386.649680	35.476455
1205.753082	156687.476837	35.481472
1206.612277	156949.954765	35.486490
1208.205719	157236.109628	35.491508
1209.251190	157553.929324	35.496525
1210.721153	157848.328771	35.501543
1211.807790	158135.106642	35.506560
1213.176621	158393.450987	35.511578
1215.103318	158694.859632	35.516596
1216.164915	158984.958641	35.521613
1217.906762	159252.608718	35.526631
1218.411608	159538.757072	35.531648
1219.324450	159804.353128	35.536666
1221.082461	160095.969040	35.541684
1221.935168	160404.709890	35.546701
1223.216824	160680.754603	35.551719
1224.287365	160963.902056	35.556736
1225.459977	161262.651005	35.561754
1226.658810	161542.394197	35.566772
1227.865889	161857.417982	35.571789
1229.528795	162129.794114	35.576807
1230.816610	162414.273245	35.581824
1232.260239	162699.718171	35.586842
1232.968393	163003.808692	35.591860
1233.846055	163294.286188	35.596877
1235.404302	163577.650375	35.601895
1236.234611	163890.455659	35.606912
1237.525349	164179.754751	35.611930
1239.027953	164451.246537	35.616948
1239.908842	164769.568868	35.621965
1241.680153	165085.818212	35.626983
1242.530919	165379.169264	35.632000
1243.734750	165660.322372	35.637018
1245.007443	165963.986023	35.642036
1245.852439	166253.271443	35.647053
1247.199402	166547.589049	35.652071
1248.618277	166846.159852	35.657088
1249.792111	167140.091417	35.662106
1250.944506	167424.538066	35.667124
1251.889277	167713.309359	35.672141
1253.403151	168017.975473	35.677159
1254.319665	168325.102295	35.682176
1255.339531	168600.481208	35.687194
1256.714174	168909.921903	35.692212
1257.896008	169201.074695	35.697229
1258.747276	169520.566394	35.702247
1260.346437	169799.689112	35.707264
1261.715365	170120.114785	35.712282
1263.357593	170439.368373	35.717300
1264.451648	170740.531753	35.722317
1266.243075	171023.969976	35.727335
1268.077971	171330.775779	35.732352
1268.975634	171633.144947	35.737370
1270.353767	171922.252888	35.742388
1271.217866	172256.874713	35.747405
1272.614523	172555.284791	35.752423
1273.661444	172858.931792	35.757440
1274.641408	173170.586192	35.762458
1276.065137	173508.563647	35.767476
1277.022411	173824.756377	35.772493
1278.487866	174135.842279	35.777511
1279.812496	174457.346430	35.782528
1280.829111	174782.431416	35.787546
1282.508322	175092.727032	35.792564
1283.208488	175433.375876	35.797581
1284.630270	175772.194913	35.802599
1285.677427	176110.481764	35.807616
1287.017385	176430.791295	35.812634
1288.392302	176778.609979	35.817652
1289.458757	177120.225688	35.822669
1290.951436	177446.557479	35.827687
1292.149722	177787.521632	35.832704
1293.189435	178131.801258	35.837722
1294.893161	178468.460752	35.842740
1295.994016	178818.103356	35.847757
1297.862001	179164.347560	35.852775
1298.822898	179493.610911	35.857792
1300.431242	179830.993488	35.862810
1301.854881	180186.950798	35.867828
1302.911954	180537.653461	35.872845
1304.448791	180855.446605	35.877863
1305.835900	181191.973786	35.882880
1307.073541	181555.027985	35.887898
1308.483192	181909.159499	35.892916
1309.538122	182228.741484	35.897933
1310.910461	182584.597231	35.902951
1312.114435	182952.959433	35.907968
1313.655879	183288.827666	35.912986
1314.463521	183631.876007	35.918004
1315.817711	183984.952105	35.923021
1316.828265	184326.004221	35.928039
1318.354758	184699.707078	35.933056
1319.774378	185045.265599	35.938074
1321.218003	185390.454324	35.943092
1322.683524	185772.767663	35.948109
1323.866153	186107.862669	35.953127
1325.584122	186449.065501	35.958144
1326.905357	186813.132400	35.963162
1328.985174	187157.516664	35.968180
1330.092190	187501.885949	35.973197
1331.687417	187832.557090	35.978215
1333.079955	188174.865262	35.983232
1334.332231	188491.723273	35.988250
1335.820737	188816.858254	35.993268
1336.875792	189164.381721	35.998285
1338.186371	189465.648101	36.003303
1339.974225	189778.908915	36.008320
1340.909995	190109.461204	36.013338
1342.115825	190426.198160	36.018356
1343.322401	190755.960579	36.023373
1344.436954	191075.280337	36.028391
1345.918537	191418.063156	36.033408
1346.926931	191740.983806	36.038426
1348.571155	192079.008824	36.043444
1349.855484	192439.982759	36.048461
1350.640628	192764.710396	36.053479
1352.294820	193096.938366	36.058496
1353.262783	193438.459480	36.063514
1354.684984	193797.057787	36.068532
1355.742468	194161.545219	36.073549
1356.926441	194504.217348	36.078567
1358.392983	194886.147499	36.083584
1359.494253	195233.585203	36.088602
1360.714161	195607.258200	36.093620
1362.208759	195964.740215	36.098637
1363.780680	196333.065739	36.103655
1365.351138	196698.816590	36.108672
1366.828605	197062.490228	36.113690
1368.305144	197428.717856	36.118708
1369.681066	197794.215187	36.123725
1371.147504	198153.060013	36.128743
1372.622838	198527.533440	36.133760
1373.607832	198909.770737	36.138778
1375.265347	199278.645132	36.143796
1376.558427	199642.148025	36.148813
1378.087727	200002.516199	36.153831
1379.419550	200382.038770	36.158848
1380.905193	200779.198056	36.163866
1382.348679	201135.727007	36.168884
1383.743976	201511.220915	36.173901
1384.754116	201890.525809	36.178919
1386.305449	202265.782313	36.183936
1387.386078	202642.769058	36.188954
1388.986044	203019.875303	36.193972
1389.991054	203417.383232	36.198989
1391.376680	203823.565747	36.204007
1393.085863	204199.060589	36.209024
1393.966147	204590.907713	36.214042
1395.441453	204983.572954	36.219060
1396.717861	205396.829118	36.224077
1398.124759	205776.597434	36.229095
1400.035942	206172.244431	36.234112
1401.374852	206566.083468	36.239130
1402.760431	206973.528057	36.244148
1403.910911	207381.064464	36.249165
1405.962290	207768.164442	36.254183
1407.540855	208158.467938	36.259200
1408.431741	208562.219020	36.264218
1410.242905	208945.453890	36.269236
1411.602272	209339.278641	36.274253
1413.155270	209741.060117	36.279271
1414.750880	210106.915418	36.284288
1415.989536	210513.336512	36.289306
1417.420721	210918.902567	36.294324
1418.927238	211309.563863	36.299341
1420.531253	211687.741779	36.304359
1421.986012	212075.748786	36.309376
1422.888798	212479.797231	36.314394
1424.245555	212872.154135	36.319412
1425.436166	213263.791125	36.324429
1427.051449	213651.499656	36.329447
1428.471419	214061.667039	36.334464
1429.898564	214446.159529	36.339482
1431.346576	214826.586864	36.344500
1432.567131	215215.713622	36.349517
1433.963213	215606.108375	36.354535
1435.551708	215964.396994	36.359552
1436.345245	216381.180241	36.364570
1437.918964	216832.630566	36.369588
1439.369520	217230.236170	36.374605
1440.700901	217614.326449	36.379623
1442.271415	217993.350197	36.384640
1443.748158	218403.959970	36.389658
1445.279573	218819.210267	36.394676
1446.768983	219225.148375	36.399693
1448.409811	219618.796100	36.404711
1449.684918	220021.293440	36.409728
1450.906635	220415.038952	36.414746
1452.498101	220831.710277	36.419764
1454.278245	221242.028067	36.424781
1455.815942	221641.034509	36.429799
1457.364083	222046.872961	36.434816
1458.620832	222452.964292	36.439834
1460.304815	222868.104805	36.444852
1461.952258	223272.001380	36.449869
1463.208657	223664.382186	36.454887
1465.244077	224072.433977	36.459904
1465.838172	224508.181432	36.464922
1467.295060	224908.000967	36.469940
1468.792567	225326.331231	36.474957
1470.066222	225764.943205	36.479975
1471.672913	226181.048898	36.484992
1472.749104	226591.452572	36.490010
1474.386162	227037.248298	36.495028
1476.001839	227477.283532	36.500045
1477.344337	227884.980831	36.505063
1479.316774	228294.963147	36.510080
1480.370613	228745.687455	36.515098
1481.842060	229182.145908	36.520116
1483.471151	229626.961897	36.525133
1484.657762	230050.033724	36.530151
1486.646416	230472.110991	36.535168
1487.891258	230929.009216	36.540186
1489.643404	231373.302905	36.545204
1490.952556	231809.390605	36.550221
1492.298637	232243.898775	36.555239
1494.194436	232690.332119	36.560256
1495.219253	233134.091126	36.565274
1496.621071	233569.610245	36.570292
1498.252253	234027.623428	36.575309
1499.731957	234482.259306	36.580327
1501.497925	234923.945600	36.585344
1502.889303	235382.866153	36.590362
1504.471557	235812.570598	36.595380
1506.003907	236263.799330	36.600397
1507.413517	236722.873206	36.605415
1509.096824	237171.793455	36.610432
1510.507508	237605.773036	36.615450
1512.432603	238052.242620	36.620468
1513.599842	238507.982997	36.625485
1515.065517	238967.079144	36.630503
1516.937551	239411.859045	36.635520
1518.285173	239858.809513	36.640538
1519.920739	240312.927676	36.645556
1521.710330	240770.780997	36.650573
1522.800526	241216.608657	36.655591
1524.739850	241641.467542	36.660608
1525.916835	242102.727298	36.665626
1527.466958	242545.713174	36.670644
1528.980428	242987.283504	36.675661
1530.403850	243451.960241	36.680679
1532.240830	243878.161430	36.685696
1533.185788	244295.797601	36.690714
1534.768345	244730.552140	36.695732
1536.360555	245151.512356	36.700749
1537.520124	245600.766844	36.705767
1538.852802	246046.970671	36.710784
1540.069474	246489.206208	36.715802
1542.015544	246945.166555	36.720820
1543.425629	247401.241503	36.725837
1544.834848	247850.890449	36.730855
1546.572761	248306.811137	36.735872
1547.839431	248782.675240	36.740890
1549.124742	249259.553107	36.745908
1551.043336	249711.661017	36.750925
1552.387826	250173.085510	36.755943
1553.940697	250645.094650	36.760960
1555.712692	251118.897260	36.765978
1556.920869	251601.887757	36.770996
1558.411879	252081.478977	36.776013
1559.960287	252551.916185	36.781031
1561.998827	253032.154820	36.786048
1563.326981	253530.598168	36.791066
1564.958210	254015.045707	36.796084
1566.645548	254482.946996	36.801101
1568.213831	254990.471853	36.806119
1569.803407	255482.878738	36.811136
1571.741527	255947.107152	36.816154
1573.401034	256444.177402	36.821172
1575.028871	256930.660059	36.826189
1576.633081	257404.623101	36.831207
1578.916693	257879.973083	36.836224
1580.225413	258381.852734	36.841242
1581.901749	258841.604114	36.846260
1583.754026	259322.868611	36.851277
1584.844378	259816.096902	36.856295
1586.621461	260295.443421	36.861312
1588.000116	260780.469897	36.866330
1589.704856	261294.910472	36.871348
1591.338312	261751.290884	36.876365
1592.971480	262261.602573	36.881383
1594.917921	262729.286609	36.886400
1596.717013	263220.772404	36.891418
1598.244746	263704.453272	36.896436
1599.809538	264186.603725	36.901453
1600.761491	264690.574968	36.906471
1602.559669	265180.231390	36.911488
1604.010927	265658.716614	36.916506
1605.157986	266168.218381	36.921524
1606.674179	266666.405338	36.926541
1608.520211	267164.308956	36.931559
1610.306811	267679.801077	36.936576
1611.758531	268181.782772	36.941594
1613.326849	268697.030696	36.946612
1614.733955	269209.612043	36.951629
1616.066850	269732.061573	36.956647
1617.292916	270240.429489	36.961664
1619.199272	270785.315853	36.966682
1620.629725	271309.703634	36.971700
1622.421116	271803.471419	36.976717
1623.500347	272346.612468	36.981735
1625.170200	272881.348558	36.986752
1627.079576	273427.653484	36.991770
1628.517886	273944.745794	36.996788
1630.608568	274465.133660	37.001805
1632.028170	275010.653144	37.006823
1633.838756	275538.172838	37.011840
1635.484157	276058.377481	37.016858
1637.017200	276578.396501	37.021876
1639.048592	277069.525792	37.026893
1640.643196	277578.609640	37.031911
1642.499382	278077.564546	37.036928
1643.797745	278573.104961	37.041946
1645.226541	279088.004877	37.046964
1647.493445	279616.050822	37.051981
1648.932147	280132.547151	37.056999
1650.315463	280617.247853	37.062016
1651.976300	281144.653523	37.067034
1653.462628	281676.481235	37.072052
1655.247381	282181.205185	37.077069
1656.254495	282714.658774	37.082087
1657.827830	283257.771823	37.087104
1659.651167	283783.594249	37.092122
1661.022291	284314.620953	37.097140
1662.092344	284858.422016	37.102157
1663.899535	285412.666864	37.107175
1665.321245	285968.065805	37.112192
1667.161698	286531.192081	37.117210
1668.862297	287099.318177	37.122228
1670.557781	287662.312075	37.127245
1672.208498	288222.390226	37.132263
1674.253428	288789.030995	37.137280
1676.040607	289370.673340	37.142298
1677.658141	289939.056746	37.147316
1679.483861	290513.194961	37.152333
1681.170048	291073.789935	37.157351
1682.570368	291632.956592	37.162368
1684.099971	292224.993229	37.167386
1685.766116	292810.375249	37.172404
1687.918906	293374.465202	37.177421
1689.925511	293969.717358	37.182439
1691.782132	294539.997882	37.187456
1693.422958	295105.358431	37.192474
1694.837013	295707.786640	37.197492
1697.024821	296281.103217	37.202509
1698.692880	296855.848946	37.207527
1700.506806	297426.656279	37.212544
1702.220810	298004.335060	37.217562
1704.242391	298599.129954	37.222580
1706.115782	299178.859119	37.227597
1707.547515	299738.846973	37.232615
1709.092226	300324.973964	37.237632
1710.809262	300898.827179	37.242650
1712.571032	301487.146978	37.247668
1714.705418	302040.936467	37.252685
1716.295509	302634.789427	37.257703
1718.157888	303221.533305	37.262720
1719.847325	303786.180704	37.267738
1721.612292	304381.188021	37.272756
1723.374485	304951.175534	37.277773
1725.108353	305524.770724	37.282791
1727.302148	306106.870788	37.287808
1728.888247	306683.632463	37.292826
1730.269823	307261.668677	37.297844
1732.107747	307841.302082	37.302861
1733.639323	308415.115634	37.307879
1735.381436	309002.020648	37.312896
1737.125652	309568.451972	37.317914
1738.729990	310172.006281	37.322932
1740.609721	310754.584644	37.327949
1742.101567	311330.975590	37.332967
1743.556280	311920.548920	37.337984
1745.722849	312511.194140	37.343002
1747.367191	313099.914967	37.348020
1749.200462	313704.116604	37.353037
1750.871853	314283.275675	37.358055
1752.557616	314826.367750	37.363072
1754.573876	315397.233757	37.368090
1756.105039	315979.425155	37.373108
1758.295072	316533.087462	37.378125
1759.760255	317095.143631	37.383143
1761.507685	317661.161163	37.388160
1763.554311	318217.754782	37.393178
1764.936762	318771.457286	37.398196
1766.810441	319366.388973	37.403213
1768.305643	319946.472520	37.408231
1769.933102	320522.517432	37.413248
1772.322190	321081.850690	37.418266
1773.483006	321662.254424	37.423284
1775.293219	322251.941134	37.428301
1777.216984	322858.692623	37.433319
1778.518383	323441.393938	37.438336
1780.095313	324041.107639	37.443354
1782.177982	324647.816544	37.448372
1783.576537	325222.157765	37.453389
1785.566078	325837.656112	37.458407
1787.389297	326439.033533	37.463424
1789.160646	327056.384170	37.468442
1790.566355	327681.863013	37.473460
1792.687335	328290.968216	37.478477
1793.998803	328907.639997	37.483495
1795.619582	329545.175118	37.488512
1797.969750	330159.631692	37.493530
1799.772033	330800.017875	37.498548
1801.602288	331435.746464	37.503565
1803.159551	332077.885586	37.508583
1804.869259	332723.800627	37.513600
1807.157394	333353.745867	37.518618
1808.410652	333989.693911	37.523636
1810.410242	334620.764355	37.528653
1811.985922	335290.992942	37.533671
1813.659471	335952.946773	37.538688
1815.531614	336590.413216	37.543706
1817.069982	337249.175075	37.548724
1818.752693	337919.455438	37.553741
1820.788984	338568.320300	37.558759
1822.617033	339256.202513	37.563776
1824.446634	339935.470196	37.568794
1826.213700	340613.114789	37.573812
1828.062635	341288.858623	37.578829
1829.759617	341958.425090	37.583847
1831.369491	342641.653203	37.588864
1833.395197	343324.118150	37.593882
1835.075930	344006.656085	37.598900
1837.035478	344704.393228	37.603917
1838.706100	345400.315286	37.608935
1840.515368	346091.102925	37.613952
1842.344959	346783.679405	37.618970
1844.447723	347474.424203	37.623988
1846.639318	348174.103533	37.629005
1848.788315	348858.577037	37.634023
1850.834941	349542.905159	37.639040
1852.378137	350238.320759	37.644058
1854.235979	350935.171324	37.649076
1856.291569	351606.904930	37.654093
1858.161032	352300.687325	37.659111
1860.109986	352998.861621	37.664128
1862.103956	353679.253623	37.669146
1863.799375	354378.285582	37.674164
1866.081658	355065.993326	37.679181
1867.657517	355746.726900	37.684199
1869.430819	356420.692727	37.689216
1871.757275	357111.532734	37.694234
1873.447234	357812.235840	37.699252
1874.833038	358457.483977	37.704269
1876.482699	359121.937534	37.709287
1878.471306	359802.157717	37.714304
1880.652271	360472.185822	37.719322
1882.248561	361134.636957	37.724340
1883.996836	361820.369446	37.729357
1885.877679	362473.643331	37.734375
1887.838267	363175.023117	37.739392
1889.636410	363839.375845	37.744410
1891.627721	364502.924552	37.749428
1893.214093	365207.958379	37.754445
1895.214643	365883.355625	37.759463
1897.013224	366574.985480	37.764480
1898.752031	367264.913196	37.769498
1900.668836	367974.053795	37.774516
1902.251135	368671.541896	37.779533
1904.481563	369371.548551	37.784551
1905.664940	370097.842887	37.789568
1908.284081	370813.638370	37.794586
1910.242555	371502.286107	37.799604
1912.295462	372206.454536	37.804621
1914.440763	372923.961633	37.809639
1916.301308	373646.397002	37.814656
1918.460986	374362.706724	37.819674
1920.061248	375064.992456	37.824692
1922.092831	375785.353226	37.829709
1924.284927	376509.908535	37.834727
1925.902186	377233.656209	37.839744
1927.942254	377958.080151	37.844762
1929.740433	378692.597296	37.849780
1931.965766	379409.174828	37.854797
1933.736266	380172.094203	37.859815
1935.573242	380888.806520	37.864832
1938.117923	381595.497189	37.869850
1939.896947	382329.432722	37.874868
1942.167687	383080.108681	37.879885
1944.420844	383799.987281	37.884903
1946.102514	384518.626074	37.889920
1948.254770	385235.320705	37.894938
1950.379264	385982.481555	37.899956
1951.807824	386729.004872	37.904973
1954.298082	387448.359059	37.909991
1956.043742	388172.485163	37.915008
1957.858843	388908.423447	37.920026
1959.691426	389645.178573	37.925044
1961.636663	390388.083947	37.930061
1963.923690	391137.760377	37.935079
1965.956421	391869.106954	37.940096
1967.868842	392592.521681	37.945114
1969.718512	393346.450807	37.950132
1971.539111	394107.692194	37.955149
1973.435411	394833.085104	37.960167
1975.643562	395571.970403	37.965184
1978.048172	396320.335854	37.970202
1979.809232	397071.957232	37.975220
1981.788252	397806.643564	37.980237
1983.774263	398554.743654	37.985255
1985.730249	399315.958358	37.990272
1988.135693	400032.499412	37.995290
1989.969189	400761.763651	38.000308
1992.290214	401522.759685	38.005325
1994.307903	402251.601525	38.010343
1996.274065	402994.954114	38.015360
1998.647243	403738.904588	38.020378
2000.401371	404463.983486	38.025396
2002.151809	405191.223736	38.030413
2004.037765	405953.593149	38.035431
2005.987566	406692.975159	38.040448
2007.881541	407393.225942	38.045466
2009.788545	408098.752400	38.050484
2011.755798	408823.531798	38.055501
2014.302709	409511.409495	38.060519
2016.706453	410219.814822	38.065536
2018.851487	410941.494255	38.070554
2020.544830	411646.888959	38.075572
2022.286767	412364.746392	38.080589
2024.714277	413084.574233	38.085607
2026.533323	413790.145507	38.090624
2028.170715	414494.182935	38.095642
2030.351658	415234.663472	38.100660
2032.104985	415949.965720	38.105677
2033.914131	416677.245166	38.110695
2035.915386	417434.131860	38.115712
2037.932977	418165.590654	38.120730
2039.572659	418893.798717	38.125748
2041.039712	419664.790075	38.130765
2043.544862	420416.466704	38.135783
2045.271441	421182.481924	38.140800
2047.034169	421956.672980	38.145818
2049.166292	422730.399631	38.150836
2051.106710	423520.011047	38.155853
2053.269484	424302.445701	38.160871
2054.845243	425080.546905	38.165888
2056.981071	425864.608093	38.170906
2058.733297	426688.154329	38.175924
2060.597811	427500.362706	38.180941
2062.810711	428299.119277	38.185959
2064.551375	429138.787936	38.190976
2066.703611	429953.702502	38.195994
2068.753468	430774.074354	38.201012
2070.597052	431616.626914	38.206029
2072.775574	432439.907480	38.211047
2074.882316	433306.302717	38.216064
2076.847383	434160.034132	38.221082
2078.938745	434998.831476	38.226100
2080.745035	435837.038360	38.231117
2082.737524	436706.364017	38.236135
2084.587418	437576.996559	38.241152
2087.005670	438435.406131	38.246170
2089.350329	439288.987720	38.251188
2091.273702	440182.132220	38.256205
2093.450567	441052.983498	38.261223
2095.367799	441930.675677	38.266240
2097.842597	442804.648871	38.271258
2099.630225	443690.238220	38.276276
2101.774223	444586.258117	38.281293
2103.748111	445465.674143	38.286311
2105.887624	446350.846171	38.291328
2107.777972	447237.136619	38.296346
2109.965038	448144.994899	38.301364
2111.615021	449061.655598	38.306381
2113.869618	449962.496016	38.311399
2115.862984	450856.563526	38.316416
2117.918647	451778.858743	38.321434
2120.572935	452661.360778	38.326452
2122.512666	453598.517192	38.331469
2124.900975	454512.748525	38.336487
2127.028331	455410.799659	38.341504
2129.048868	456319.196874	38.346522
2131.202215	457237.899115	38.351540
2132.896147	458177.368603	38.356557
2135.426380	459071.655182	38.361575
2137.561530	459997.114103	38.366592
2139.420714	460920.857526	38.371610
2141.772404	461835.377385	38.376628
2144.001994	462751.898199	38.381645
2146.221063	463640.574928	38.386663
2148.513942	464540.472836	38.391680
2150.492974	465433.760042	38.396698
2152.548982	466334.677347	38.401716
2154.992460	467204.607436	38.406733
2158.109007	468061.095622	38.411751
2160.478984	468937.480878	38.416768
2162.596451	469821.701627	38.421786
2165.030986	470700.877421	38.426804
2167.015328	471576.044869	38.431821
2169.292875	472453.094858	38.436839
2171.356638	473321.196538	38.441856
2173.439551	474188.447170	38.446874
2175.641478	475081.557013	38.451892
2177.729846	475974.744476	38.456909
2180.196832	476838.172855	38.461927
2182.218357	477715.476374	38.466944
2184.123692	478610.639721	38.471962
2186.919831	479518.291440	38.476980
2188.209357	480410.640935	38.481997
2190.594323	481298.019060	38.487015
2192.606206	482206.930495	38.492032
2194.804267	483122.684762	38.497050
2196.994089	484032.486004	38.502068
2199.109916	484945.081611	38.507085
2201.729111	485873.908065	38.512103
2203.806045	486805.653957	38.517120
2205.658434	487716.233766	38.522138
2207.887937	488633.924393	38.527156
2209.939845	489584.209030	38.532173
2212.325116	490522.120901	38.537191
2214.664243	491454.235968	38.542208
2216.253092	492396.217374	38.547226
2218.717447	493333.107806	38.552244
2220.573736	494300.127902	38.557261
2223.061716	495252.505896	38.562279
2225.211305	496189.495570	38.567296
2227.350143	497167.965457	38.572314
2229.872643	498129.664873	38.577332
2231.786923	499111.642876	38.582349
2234.444760	500077.145265	38.587367
2236.810554	501036.031692	38.592384
2238.816841	502010.258517	38.597402
2241.498982	502986.284531	38.602420
2243.655795	503941.861052	38.607437
2246.221861	504900.543137	38.612455
2249.279863	505873.815547	38.617472
2251.401701	506846.478742	38.622490
2254.187916	507787.506999	38.627508
2256.126343	508729.326798	38.632525
2258.508249	509691.289103	38.637543
2260.943536	510649.303156	38.642560
2263.287763	511598.754857	38.647578
2266.069673	512531.441617	38.652596
2267.924475	513477.182634	38.657613
2270.102809	514439.852260	38.662631
2272.791322	515381.410873	38.667648
2274.839361	516308.049594	38.672666
2277.393243	517251.283048	38.677684
2279.699203	518209.014864	38.682701
2281.695188	519154.493638	38.687719
2283.733963	520107.214588	38.692736
2286.013470	521061.248240	38.697754
2288.239305	521984.800014	38.702772
2290.393838	522946.446545	38.707789
2292.361884	523901.161857	38.712807
2294.457695	524869.045022	38.717824
2296.507876	525846.142554	38.722842
2299.104352	526789.894561	38.727860
2300.692176	527728.465645	38.732877
2302.887940	528670.201926	38.737895
2304.888516	529612.263823	38.742912
2306.986191	530561.753349	38.747930
2309.405422	531523.062849	38.752948
2310.994338	532486.813401	38.757965
2313.422708	533450.010351	38.762983
2315.702387	534421.978772	38.768000
2317.490984	535413.998728	38.773018
2319.744899	536402.653222	38.778036
2322.433943	537422.072783	38.783053
2324.432713	538429.657029	38.788071
2326.745167	539430.728082	38.793088
2329.054339	540441.693768	38.798106
2331.318914	541455.212123	38.803124
2333.425404	542487.904763	38.808141
2336.202969	543515.582067	38.813159
2338.701617	544536.992839	38.818176
2341.289549	545571.343642	38.823194
2344.016245	546595.585947	38.828212
2346.093757	547647.070586	38.833229
2348.339406	548678.532704	38.838247
2351.033878	549705.670458	38.843264
2353.311964	550748.137611	38.848282
2355.465103	551797.384905	38.853300
2357.408325	552850.005660	38.858317
2359.782112	553892.269182	38.863335
2362.526428	554962.844497	38.868352
2364.615996	556026.758242	38.873370
2367.185098	557099.003599	38.878388
2369.284989	558175.312013	38.883405
2371.477998	559239.759704	38.888423
2373.939087	560319.957432	38.893440
2376.096473	561418.055348	38.898458
2378.671908	562518.706698	38.903476
2380.895749	563598.677244	38.908493
2383.385268	564680.273772	38.913511
2385.861173	565780.719733	38.918528
2388.793841	566906.411401	38.923546
2391.311995	567996.970559	38.928564
2393.577902	569093.907422	38.933581
2396.141890	570174.232856	38.938599
2398.260963	571280.397923	38.943616
2400.658541	572418.953323	38.948634
2403.254240	573506.724634	38.953652
2405.289224	574605.086596	38.958669
2407.958106	575719.661203	38.963687
2410.472067	576813.737779	38.968704
2412.609979	577945.015749	38.973722
2415.510660	579074.962263	38.978740
2417.688901	580199.005602	38.983757
2420.118294	581292.253958	38.988775
2422.991883	582394.111444	38.993792
2424.960164	583530.830096	38.998810
2427.528491	584659.771875	39.003828
2429.918635	585775.750974	39.008845
2432.015428	586887.865734	39.013863
2434.941831	588018.895876	39.018880
2437.327571	589143.241894	39.023898
2439.894509	590265.648961	39.028916
2442.048044	591396.140199	39.033933
2444.535850	592516.094932	39.038951
2447.091595	593658.135427	39.043968
2449.543437	594775.779549	39.048986
2452.270480	595888.913954	39.054004
2454.473249	597021.570170	39.059021
2457.340800	598133.367949	39.064039
2459.983917	599239.437165	39.069056
2462.207062	600324.133680	39.074074
2464.815226	601392.689354	39.079092
2467.119903	602488.990881	39.084109
2469.701894	603566.615657	39.089127
2472.028004	604657.300459	39.094144
2474.199709	605755.066798	39.099162
2476.810367	606841.943036	39.104180
2478.985862	607926.985841	39.109197
2481.143555	609036.152867	39.114215
2483.878741	610159.279416	39.119232
2486.535964	611257.037002	39.124250
2489.359958	612339.849795	39.129268
2491.743102	613452.549616	39.134285
2494.018789	614584.867001	39.139303
2496.689403	615696.195956	39.144320
2498.783621	616820.463188	39.149338
2501.450902	617934.419972	39.154356
2503.618143	619085.801304	39.159373
2505.607850	620221.291596	39.164391
2508.427380	621373.576186	39.169408
2510.567348	622533.949937	39.174426
2512.933273	623698.361810	39.179444
2515.068385	624873.032783	39.184461
2517.544369	626058.014768	39.189479
2520.253875	627243.377925	39.194496
2522.361216	628424.562909	39.199514
2525.249295	629616.429766	39.204532
2527.975407	630830.668590	39.209549
2530.396534	632033.131960	39.214567
2532.770198	633218.687045	39.219584
2534.953627	634458.718987	39.224602
2537.666400	635658.225460	39.229620
2540.454723	636881.495543	39.234637
2542.637121	638122.842370	39.239655
2545.321333	639348.087046	39.244672
2547.411356	640586.709673	39.249690
2550.109344	641840.652452	39.254708
2552.578322	643095.578233	39.259725
2554.855879	644357.516213	39.264743
2557.455950	645610.117436	39.269760
2559.865550	646862.297106	39.274778
2562.809864	648134.630663	39.279796
2565.351884	649403.879078	39.284813
2568.190031	650674.016001	39.289831
2571.193801	651950.046944	39.294848
2573.658772	653233.630297	39.299866
2576.310861	654480.487597	39.304884
2578.720209	655756.678597	39.309901
2581.261331	657049.873010	39.314919
2583.930524	658316.772811	39.319936
2585.984173	659617.831333	39.324954
2588.881513	660907.123379	39.329972
2591.523694	662195.142192	39.334989
2593.706522	663477.938027	39.340007
2596.587091	664756.167981	39.345024
2599.088809	666061.420610	39.350042
2601.505637	667381.491737	39.355060
2604.165873	668702.237202	39.360077
2606.449069	670004.452404	39.365095
2609.086925	671304.043437	39.370112
2611.529260	672616.273280	39.375130
2614.383635	673931.486415	39.380148
2617.146926	675248.222196	39.385165
2619.651117	676575.407433	39.390183
2622.747931	677870.190604	39.395200
2625.719125	679174.110674	39.400218
2628.198475	680474.251260	39.405236
2631.362342	681732.601275	39.410253
2633.821746	683023.939104	39.415271
2636.532740	684270.092676	39.420288
2638.575135	685555.927374	39.425306
2641.103741	686827.743409	39.430324
2643.900289	688085.532300	39.435341
2646.082724	689340.914747	39.440359
2648.773897	690638.785793	39.445376
2651.057502	691926.113224	39.450394
2653.661306	693216.032981	39.455412
2656.307213	694518.266130	39.460429
2658.574839	695836.696540	39.465447
2661.548570	697139.337008	39.470464
2664.183806	698448.786846	39.475482
2666.493705	699767.123268	39.480500
2668.925062	701087.424725	39.485517
2671.259332	702430.103615	39.490535
2674.624011	703784.899675	39.495552
2677.007530	705140.192590	39.500570
2679.415421	706473.068451	39.505588
2682.406037	707812.233844	39.510605
2684.925593	709196.403145	39.515623
2687.598641	710555.111635	39.520640
2690.159743	711935.366073	39.525658
2692.741618	713340.005489	39.530676
2695.342668	714708.069561	39.535693
2698.175802	716108.646151	39.540711
2700.955861	717499.447522	39.545728
2703.542672	718903.165564	39.550746
2706.022741	720294.099602	39.555764
2708.786453	721711.272064	39.560781
2711.248599	723145.763226	39.565799
2714.126146	724557.338903	39.570816
2717.276100	725966.503472	39.575834
2719.724166	727410.791437	39.580852
2722.815832	728854.028271	39.585869
2724.717989	730293.501124	39.590887
2727.562246	731727.031685	39.595904
2729.689183	733190.760741	39.600922
2732.073894	734643.119912	39.605940
2735.336399	736112.802562	39.610957
2738.522657	737583.661964	39.615975
2740.828821	739063.875467	39.620992
2743.891843	740542.012760	39.626010
2746.556264	742003.904417	39.631028
2749.834001	743474.011219	39.636045
2752.737250	744966.252988	39.641063
2755.405418	746436.748551	39.646080
2758.119994	747929.151357	39.651098
2760.847588	749417.669264	39.656116
2763.975000	750880.995189	39.661133
2766.174458	752355.238406	39.666151
2769.149268	753839.963258	39.671168
2772.153266	755336.221575	39.676186
2774.835851	756828.597817	39.681204
2777.922907	758313.280296	39.686221
2781.020604	759794.620684	39.691239
2783.810483	761261.350654	39.696256
2786.819623	762740.852967	39.701274
2789.722738	764221.658595	39.706292
2792.799091	765709.229665	39.711309
2795.739025	767174.395492	39.716327
2798.737826	768645.068407	39.721344
2802.019743	770102.867873	39.726362
2804.599745	771556.466979	39.731380
2807.641881	773034.525186	39.736397
2810.134343	774489.873752	39.741415
2812.940585	775916.880450	39.746432
2815.809526	777358.679521	39.751450
2817.820365	778774.652342	39.756468
2821.061742	780190.393623	39.761485
2823.183907	781631.914764	39.766503
2825.994890	783053.551382	39.771520
2828.713404	784463.196120	39.776538
2831.339860	785896.081022	39.781556
2834.452211	787338.655978	39.786573
2836.958497	788813.947301	39.791591
2839.779334	790260.787420	39.796608
2842.114833	791698.393751	39.801626
2844.982904	793162.479538	39.806644
2847.949297	794623.600237	39.811661
2850.007256	796119.449527	39.816679
2853.066688	797606.489019	39.821696
2855.823790	799098.600572	39.826714
2858.227816	800615.518834	39.831732
2861.225644	802125.645522	39.836749
2863.758523	803632.877595	39.841767
2866.704325	805182.622364	39.846784
2869.237260	806715.944521	39.851802
2871.817535	808265.446686	39.856820
2874.809558	809791.110191	39.861837
2877.432300	811371.438029	39.866855
2880.497703	812945.070277	39.871872
2883.074344	814525.991108	39.876890
2885.439214	816123.673950	39.881908
2888.716838	817714.576215	39.886925
2891.782763	819315.828912	39.891943
2894.444736	820905.879327	39.896960
2897.845061	822523.294622	39.901978
2900.475958	824163.910685	39.906996
2903.621063	825764.866857	39.912013
2906.453052	827386.114035	39.917031
2909.014202	829019.584476	39.922048
2911.907203	830673.308090	39.927066
2914.809426	832317.888753	39.932084
2917.976380	833954.897391	39.937101
2920.717304	835615.671540	39.942119
2923.583008	837242.887708	39.947136
2926.692484	838908.596111	39.952154
2929.313066	840580.425285	39.957172
2932.808378	842237.271600	39.962189
2936.005303	843886.342684	39.967207
2938.961154	845546.161173	39.972224
2941.971345	847212.924942	39.977242
2944.644904	848882.219793	39.982260
2947.661539	850556.845515	39.987277
2950.579555	852223.170177	39.992295
2953.565547	853869.127400	39.997312
2956.841943	855555.772627	40.002330
2959.926744	857261.308449	40.007348
2963.061637	858916.093689	40.012365
2965.255359	860589.023502	40.017383
2968.681648	862248.393515	40.022400
2971.876427	863936.927092	40.027418
2975.072755	865621.308583	40.032436
2978.235683	867280.417718	40.037453
2981.715671	868951.130901	40.042471
2984.791626	870626.000294	40.047488
2987.958793	872289.832805	40.052506
2990.660000	873941.953245	40.057524
2993.598510	875592.996694	40.062541
2996.671171	877262.330399	40.067559
2999.294408	878939.683518	40.072576
3002.114791	880601.442877	40.077594
3004.938003	882266.019846	40.082612
3007.687309	883922.791946	40.087629
3011.019714	885569.143787	40.092647
3013.860353	887192.895828	40.097664
3016.894391	888816.355562	40.102682
3019.953715	890458.663684	40.107700
3022.954783	892093.179622	40.112717
3025.882666	893711.806299	40.117735
3028.805700	895339.526229	40.122752
3031.454760	896972.999415	40.127770
3034.241519	898638.275772	40.132788
3037.110853	900296.689998	40.137805
3039.789673	901959.178113	40.142823
3042.296110	903634.977986	40.147840
3045.572919	905314.195837	40.152858
3048.355320	907012.821097	40.157876
3051.214354	908704.662762	40.162893
3054.172203	910420.312311	40.167911
3056.799909	912152.315390	40.172928
3060.062577	913874.923255	40.177946
3062.975458	915624.633330	40.182964
3065.809134	917366.401540	40.187981
3069.042457	919107.069805	40.192999
3072.334033	920868.200621	40.198016
3075.384668	922619.394569	40.203034
3078.615170	924386.880865	40.208052
3082.115625	926159.020112	40.213069
3085.419476	927931.087899	40.218087
3088.349334	929720.844959	40.223104
3091.533729	931470.672686	40.228122
3094.512742	933260.672101	40.233140
3097.771229	935044.180774	40.238157
3100.924367	936827.488729	40.243175
3103.966338	938622.652630	40.248192
3107.073428	940427.237431	40.253210
3110.008168	942225.491153	40.258228
3112.868874	944025.814401	40.263245
3115.916108	945835.327081	40.268263
3118.822896	947635.346994	40.273280
3121.979842	949469.459659	40.278298
3124.942507	951330.444246	40.283316
3128.178591	953143.471857	40.288333
3131.301063	954993.174505	40.293351
3133.797592	956864.872691	40.298368
3137.447728	958746.948997	40.303386
3140.679295	960674.732308	40.308404
3143.393233	962585.241196	40.313421
3146.634932	964476.170116	40.318439
3149.850107	966374.590391	40.323456
3153.399052	968301.527783	40.328474
3156.684115	970229.034061	40.333492
3160.246465	972128.522897	40.338509
3163.483566	974033.387377	40.343527
3166.341939	975950.456915	40.348544
3169.824766	977882.770486	40.353562
3173.189780	979791.743216	40.358580
3176.172771	981691.860290	40.363597
3179.354968	983610.401635	40.368615
3181.921831	985537.161871	40.373632
3185.576578	987443.042458	40.378650
3188.400643	989381.502545	40.383668
3191.523485	991322.560219	40.388685
3194.286440	993266.028774	40.393703
3197.564247	995200.000283	40.398720
3201.363265	997123.025064	40.403738
3204.152887	999075.965424	40.408756
3207.194474	1001021.783002	40.413773
3210.615832	1002965.995741	40.418791
3213.636714	1004920.376349	40.423808
3217.170635	1006835.586512	40.428826
3220.172050	1008738.405277	40.433844
3223.160109	1010646.303316	40.438861
3226.494438	1012554.273690	40.443879
3229.226381	1014451.526063	40.448896
3232.471569	1016328.881423	40.453914
3235.402225	1018259.869271	40.458932
3238.333518	1020179.935977	40.463949
3241.519281	1022088.856648	40.468967
3244.773519	1024003.208155	40.473984
3248.140423	1025940.666811	40.479002
3251.381958	1027905.498816	40.484020
3254.185503	1029836.579112	40.489037
3257.919032	1031773.984544	40.494055
3260.752089	1033737.122329	40.499072
3264.033503	1035710.495838	40.504090
3266.979344	1037680.428133	40.509108
3269.958492	1039658.625613	40.514125
3273.134874	1041643.798423	40.519143
3276.207936	1043667.497253	40.524160
3279.945622	1045669.446322	40.529178
3282.895332	1047682.742234	40.534196
3286.417609	1049697.907269	40.539213
3289.479659	1051721.651361	40.544231
3292.547688	1053771.969967	40.549248
3295.891183	1055813.021130	40.554266
3298.956937	1057862.205445	40.559284
3302.187124	1059928.086926	40.564301
3305.714665	1061998.138609	40.569319
3308.684088	1064049.166566	40.574336
3311.957259	1066143.524589	40.579354
3315.380771	1068253.175495	40.584372
3318.274288	1070343.786595	40.589389
3321.763643	1072430.530496	40.594407
3324.487902	1074546.022091	40.599424
3328.179215	1076648.850607	40.604442
3331.675500	1078767.944854	40.609460
3335.104578	1080907.953491	40.614477
3338.349113	1083038.542195	40.619495
3341.538893	1085170.506181	40.624512
3344.823985	1087301.523624	40.629530
3348.211327	1089455.291971	40.634548
3351.525443	1091623.119454	40.639565
3355.163363	1093756.512830	40.644583
3358.009876	1095915.921387	40.649600
3361.282561	1098073.730633	40.654618
3364.755044	1100252.771597	40.659636
3367.915780	1102416.685452	40.664653
3371.206788	1104589.906487	40.669671
3374.493257	1106797.210198	40.674688
3378.214536	1108969.736562	40.679706
3380.967222	1111160.294731	40.684724
3384.115916	1113361.501553	40.689741
3387.883250	1115554.381424	40.694759
3390.710476	1117762.109028	40.699776
3393.959992	1119985.675731	40.704794
3396.998983	1122219.180858	40.709812
3400.468843	1124443.517000	40.714829
3403.524254	1126671.360217	40.719847
3406.394798	1128915.852609	40.724864
3410.179078	1131144.931161	40.729882
3413.839823	1133406.933123	40.734900
3416.947303	1135676.779826	40.739917
3420.475311	1137937.253574	40.744935
3423.889554	1140190.724595	40.749952
3427.407323	1142439.056971	40.754970
3431.140369	1144705.220006	40.759988
3434.169493	1146954.172500	40.765005
3437.668278	1149202.603826	40.770010
3440.871981	1151384.239146	40.775015
3443.801705	1153506.042066	40.780020
3447.007430	1155584.931004	40.785024
3450.304306	1157593.839106	40.790029
3453.478957	1159502.812419	40.795034
3456.471769	1161338.434875	40.800039
3459.636417	1163115.464776	40.805044
3462.607424	1164813.145794	40.810048
3465.698742	1166415.921872	40.815053
3468.599201	1167929.878240	40.820058
3470.905696	1169360.159951	40.825063
3473.746287	1170738.540576	40.830068
3476.213356	1172018.517871	40.835072
3478.731853	1173225.556890	40.840077
3481.115936	1174349.367158	40.845082
3483.089717	1175425.209429	40.850087
3485.404481	1176426.694246	40.855092
3487.572307	1177349.515809	40.860096
3489.263038	1178208.185384	40.865101
3491.198404	1179011.659227	40.870106
3492.672797	1179762.151188	40.875111
3494.532308	1180452.481680	40.880116
3496.173025	1181092.567156	40.885120
3497.469618	1181679.433902	40.890125
3499.105279	1182193.217209	40.895130
3500.369190	1182672.745634	40.900135
3501.363938	1183119.800203	40.905140
3502.943962	1183521.165925	40.910144
3503.950948	1183877.138250	40.915149
3504.983077	1184196.662388	40.920154
3505.793747	1184491.830811	40.925159
3507.015303	1184729.327013	40.930164
3507.838356	1184944.295379	40.935168
3508.723352	1185120.008806	40.940173
3509.617126	1185273.604132	40.945178
3510.386661	1185399.365989	40.950183
3511.294841	1185495.841851	40.955188
3511.915703	1185546.450792	40.960192
3512.562696	1185586.894028	40.965197
3513.462566	1185605.750524	40.970202
3513.934398	1185597.111384	40.975207
3514.691451	1185578.358421	40.980212
3515.239389	1185538.753353	40.985216
3515.544997	1185461.930444	40.990221
3516.386393	1185373.257374	40.995226
3516.612111	1185262.197099	41.000231
3517.097774	1185148.268922	41.005236
3517.610711	1185023.419004	41.010240
3517.845295	1184871.794771	41.015245
3518.235154	1184701.320848	41.020250
3518.945368	1184530.600362	41.025255
3518.999464	1184342.855212	41.030260
3519.592348	1184137.416213	41.035264
3519.689536	1183908.898972	41.040269
3520.409616	1183686.292575	41.045274
3520.281531	1183458.451410	41.050279
3520.805186	1183207.526282	41.055284
3521.236143	1182952.556689	41.060288
3521.214463	1182676.280435	41.065293
3521.578584	1182377.426341	41.070298
3521.513525	1182111.953365	41.075303
3521.927517	1181818.613478	41.080308
3522.185657	1181537.146357	41.085312
3522.310424	1181220.092927	41.090317
3522.697996	1180881.129954	41.095322
3522.637688	1180572.825098	41.100327
3523.072288	1180247.279818	41.105332
3523.206008	1179920.256732	41.110336
3523.272412	1179571.654313	41.115341
3523.211454	1179217.586002	41.120346
3523.125564	1178876.121059	41.125351
3523.433601	1178527.879868	41.130356
3523.976835	1178189.752037	41.135360
3523.785711	1177833.161246	41.140365
3523.955250	1177459.713714	41.145370
3524.441878	1177088.354601	41.150375
3524.534458	1176707.609546	41.155380
3524.194370	1176322.383868	41.160384
3524.132958	1175939.911502	41.165389
3524.556316	1175556.859881	41.170394
3524.255006	1175186.437497	41.175399
3524.629064	1174780.334703	41.180404
3525.085005	1174371.452486	41.185408
3524.673820	1173986.725704	41.190413
3525.044260	1173592.317507	41.195418
3524.875210	1173180.710104	41.200423
3525.002729	1172779.395975	41.205428
3524.878737	1172380.922037	41.210432
3524.616033	1171960.839106	41.215437
3524.750725	1171532.638242	41.220442
3524.752719	1171139.425928	41.225447
3525.090067	1170726.503638	41.230452
3524.924376	1170319.293081	41.235456
3525.071219	1169912.565486	41.240461
3525.219567	1169500.615406	41.245466
3525.086395	1169071.596154	41.250471
3524.953799	1168656.416788	41.255476
3525.184650	1168238.784659	41.260480
3524.983429	1167830.819536	41.265485
3524.964144	1167373.415209	41.270490
3525.062100	1166970.148673	41.275495
3525.056233	1166557.142164	41.280500
3525.006286	1166129.850675	41.285504
3524.797616	1165689.045135	41.290509
3525.055673	1165269.093596	41.295514
3525.219438	1164847.518112	41.300519
3525.167193	1164414.230521	41.305524
3525.071320	1163993.762640	41.310528
3524.814897	1163573.665362	41.315533
3525.009963	1163137.680438	41.320538
3524.923728	1162711.438704	41.325543
3524.824929	1162286.581929	41.330548
3524.984115	1161847.754983	41.335552
3524.756114	1161410.750951	41.340557
3524.971118	1160982.806721	41.345562
3525.025854	1160550.883488	41.350567
3525.015754	1160115.531818	41.355572
3525.308257	1159687.847371	41.360576
3525.369402	1159257.329422	41.365581
3525.446650	1158797.836111	41.370586
3524.848080	1158361.679336	41.375591
3525.043539	1157931.314261	41.380596
3524.815485	1157504.861876	41.385600
3524.937993	1157063.749042	41.390605
3525.160033	1156625.799398	41.395610
3524.824108	1156205.881772	41.400615
3524.776835	1155747.750594	41.405620
3524.893883	1155318.509167	41.410624
3524.709203	1154876.033164	41.415629
3524.872096	1154422.767748	41.420634
3524.808184	1153993.448007	41.425639
3524.618997	1153549.630702	41.430644
3524.908780	1153106.454449	41.435648
3524.671810	1152665.410550	41.440653
3525.233889	1152221.546930	41.445658
3524.583677	1151794.038088	41.450663
3524.832981	1151352.046588	41.455668
3524.774050	1150905.049215	41.460672
3524.467416	1150474.440733	41.465677
3524.871072	1150025.114084	41.470682
3524.787718	1149584.071109	41.475687
3524.769854	1149153.307177	41.480692
3524.628558	1148713.432572	41.485696
3524.371911	1148250.893515	41.490701
3524.924060	1147819.453038	41.495706
3524.461314	1147398.853686	41.500711
3524.630478	1146940.015283	41.505716
3525.019237	1146483.186200	41.510720
3524.418319	1146040.510469	41.515725
3524.592596	1145596.153102	41.520730
3524.436404	1145155.320849	41.525735
3524.598639	1144696.193908	41.530740
3524.551911	1144256.216856	41.535744
3524.331354	1143823.344530	41.540749
3524.611613	1143380.869908	41.545754
3524.403390	1142930.945429	41.550759
3524.318208	1142484.187666	41.555764
3524.433606	1142035.556666	41.560768
3523.869693	1141604.172068	41.565773
3524.272266	1141163.674085	41.570778
3524.142404	1140736.891529	41.575783
3524.143596	1140280.539340	41.580788
3524.379437	1139833.125424	41.585792
3523.994975	1139390.047093	41.590797
3524.175832	1138949.781241	41.595802
3523.541338	1138522.713601	41.600807
3523.978962	1138082.713198	41.605812
3524.208230	1137655.718306	41.610816
3523.898577	1137206.843357	41.615821
3524.046141	1136760.798969	41.620826
3523.573090	1136317.288540	41.625831
3523.655159	1135878.303562	41.630836
3523.620418	1135435.217126	41.635840
3523.553077	1134999.033659	41.640845
3523.982445	1134583.632933	41.645850
3523.700437	1134147.794940	41.650855
3523.353913	1133706.420830	41.655860
3523.659348	1133261.101690	41.660864
3523.466258	1132840.250796	41.665869
3523.581288	1132405.915172	41.670874
3523.621038	1131969.275326	41.675879
3523.390777	1131527.606143	41.680884
3523.466241	1131087.846287	41.685888
3523.442747	1130659.760210	41.690893
3523.690409	1130227.126327	41.695898
3523.309367	1129804.069529	41.700903
3523.216319	1129339.185087	41.705908
3523.069694	1128918.872216	41.710912
3522.922110	1128498.050791	41.715917
3523.109884	1128067.248657	41.720922
3523.118592	1127637.772956	41.725927
3522.670582	1127205.388744	41.730932
3523.100815	1126776.249898	41.735936
3522.773831	1126353.671333	41.740941
3523.076990	1125912.780693	41.745946
3522.591256	1125493.109946	41.750951
3522.906367	1125054.049672	41.755956
3523.137662	1124637.714926	41.760960
3522.900383	1124205.719106	41.765965
3522.797202	1123778.425968	41.770970
3522.689891	1123350.528112	41.775975
3522.585884	1122911.741537	41.780980
3522.623544	1122488.416039	41.785984
3522.671078	1122077.910725	41.790989
3522.478721	1121650.747783	41.795994
3522.707889	1121231.100471	41.800999
3522.696939	1120788.600412	41.806004
3522.860081	1120370.610926	41.811008
3522.356350	1119940.314480	41.816013
3522.769279	1119524.313530	41.821018
3522.156105	1119095.110381	41.826023
3522.193794	1118663.574052	41.831028
3522.221315	1118240.580991	41.836032
3522.320153	1117821.640696	41.841037
3522.208140	1117393.362188	41.846042
3521.994420	1116978.315047	41.851047
3521.987071	1116551.286411	41.856052
3522.474469	1116131.292063	41.861056
3522.082279	1115715.699887	41.866061
3521.977689	1115282.389233	41.871066
3522.023517	1114881.343446	41.876071
3521.898016	1114459.125979	41.881076
3521.988692	1114038.174830	41.886080
3521.967993	1113629.417009	41.891085
3521.821015	1113198.234001	41.896090
3521.483859	1112790.132064	41.901095
3521.295365	1112373.484276	41.906100
3521.251999	1111949.720315	41.911104
3520.972288	1111539.892021	41.916109
3521.315872	1111149.204477	41.921114
3521.014703	1110749.338402	41.926119
3521.471147	1110320.019745	41.931124
3521.863236	1109922.841036	41.936128
3521.247223	1109524.462755	41.941133
3521.429831	1109099.864185	41.946138
3521.609169	1108687.738266	41.951143
3521.592020	1108273.608275	41.956148
3521.541248	1107884.276002	41.961152
3521.369367	1107472.210320	41.966157
3521.200840	1107030.223617	41.971162
3521.012399	1106634.425654	41.976167
3521.158769	1106240.549088	41.981172
3520.877475	1105832.482698	41.986176
3521.025011	1105422.786445	41.991181
3521.130316	1105008.767251	41.996186
3520.963600	1104609.473460	42.001191
3520.917264	1104192.837133	42.006196
3520.885431	1103799.002557	42.011200
3520.547417	1103385.696129	42.016205
3520.362181	1102989.629913	42.021210
3520.664746	1102606.834159	42.026215
3520.815531	1102210.846584	42.031220
3520.806812	1101819.253113	42.036224
3520.180421	1101423.240167	42.041229
3520.743752	1101006.161737	42.046234
3520.546732	1100610.305249	42.051239
3520.730740	1100208.429000	42.056244
3520.528688	1099813.662317	42.061248
3520.591575	1099416.528111	42.066253
3520.251291	1099024.977889	42.071258
3520.141257	1098628.388057	42.076263
3520.042654	1098233.106319	42.081268
3520.203650	1097836.031146	42.086272
3520.037311	1097445.007430	42.091277
3520.286583	1097053.408657	42.096282
3520.353712	1096682.860140	42.101287
3519.841165	1096275.831152	42.106292
3520.117755	1095873.234683	42.111296
3519.962051	1095488.000546	42.116301
3520.307972	1095092.129027	42.121306
3520.317197	1094724.997059	42.126311
3519.985884	1094326.405531	42.131316
3519.981048	1093937.111840	42.136320
3519.812563	1093558.826145	42.141325
3520.042313	1093143.206591	42.146330
3519.757284	1092734.629347	42.151335
3519.640492	1092366.592386	42.156340
3520.020779	1091992.511583	42.161344
3519.544187	1091600.638081	42.166349
3519.730150	1091203.647003	42.171354
3519.635577	1090832.341803	42.176359
3519.495634	1090440.233259	42.181364
3519.758592	1090043.910958	42.186368
3519.356838	1089662.518101	42.191373
3520.023896	1089279.772754	42.196378
3519.718742	1088903.005136	42.201383
3519.286224	1088510.709613	42.206388
3519.475839	1088119.624865	42.211392
3519.274168	1087733.463915	42.216397
3519.593830	1087339.139095	42.221402
3519.410635	1086974.005948	42.226407
3519.527108	1086611.386955	42.231412
3519.391144	1086207.373939	42.236416
3519.132851	1085832.494625	42.241421
3519.550650	1085435.235463	42.246426
3519.149267	1085066.366964	42.251431
3519.230507	1084677.065944	42.256436
3519.152083	1084296.010251	42.261440
3519.149138	1083938.506932	42.266445
3519.291176	1083541.730404	42.271450
3519.160035	1083171.921751	42.276455
3518.754053	1082784.867605	42.281460
3519.005618	1082417.246781	42.286464
3518.920024	1082060.784946	42.291469
3518.843130	1081676.763673	42.296474
3518.927367	1081281.942769	42.301479
3518.968360	1080914.735027	42.306484
3519.085784	1080560.156648	42.311488
3518.613850	1080189.050171	42.316493
3518.878166	1079805.704618	42.321498
3518.771602	1079439.189619	42.326503
3518.595419	1079060.183305	42.331508
3518.768307	1078686.276779	42.336512
3518.493501	1078320.098300	42.341517
3518.421059	1077949.925705	42.346522
3518.574870	1077585.643493	42.351527
3518.541796	1077213.014169	42.356532
3518.577581	1076847.165855	42.361536
3518.196421	1076472.526826	42.366541
3518.429354	1076117.448728	42.371546
3518.125163	1075748.413597	42.376551
3518.136004	1075381.798979	42.381556
3518.297798	1075021.762850	42.386560
3518.276367	1074657.314284	42.391565
3518.482664	1074290.306114	42.396570
3518.248856	1073927.381007	42.401575
3517.999710	1073559.918467	42.406580
3518.169613	1073188.903025	42.411584
3518.066438	1072846.351643	42.416589
3518.079923	1072493.380677	42.421594
3518.266814	1072124.404524	42.426599
3517.839729	1071752.044516	42.431604
3518.064934	1071395.603918	42.436608
3517.667677	1071021.843659	42.441613
3517.864211	1070670.936009	42.446618
3518.059883	1070327.216490	42.451623
3517.488513	1069954.854205	42.456628
3517.637309	1069598.501587	42.461632
3517.824244	1069257.889478	42.466637
3517.628921	1068895.489885	42.471642
3517.620347	1068542.941168	42.476647
3517.377968	1068185.503279	42.481652
3517.393334	1067825.114153	42.486656
3517.302271	1067490.689996	42.491661
3517.408048	1067130.240348	42.496666
3517.440213	1066805.181268	42.501671
3517.210366	1066455.228481	42.506676
3517.111549	1066096.283957	42.511680
3517.232879	1065753.444615	42.516685
3517.518315	1065402.473900	42.521690
3517.299282	1065076.006674	42.526695
3517.015330	1064713.922897	42.531700
3517.131286	1064357.331548	42.536704
3516.984996	1064008.556517	42.541709
3516.744636	1063674.213254	42.546714
3516.973884	1063326.680697	42.551719
3516.897182	1062990.439922	42.556724
3516.847228	1062665.630752	42.561728
3516.740280	1062317.704717	42.566733
3516.801593	1061969.728966	42.571738
3516.596902	1061620.234349	42.576743
3516.306821	1061302.413542	42.581748
3516.460349	1060969.285426	42.586752
3516.384250	1060635.404499	42.591757
3516.512082	1060295.787155	42.596762
3516.605823	1059965.016006	42.601767
3516.519443	1059652.267704	42.606772
3516.597135	1059311.827339	42.611776
3516.559125	1058981.018806	42.616781
3516.236918	1058632.798960	42.621786
3516.381183	1058311.747321	42.626791
3516.034633	1057978.520677	42.631796
3516.299267	1057643.053277	42.636800
3515.922477	1057328.197301	42.641805
3516.151207	1056998.767735	42.646810
3516.106057	1056682.374675	42.651815
3516.176900	1056358.522813	42.656820
3516.098994	1056032.941429	42.661824
3515.795079	1055707.667241	42.666829
3515.844083	1055373.446863	42.671834
3516.198040	1055063.739729	42.676839
3515.794853	1054728.108656	42.681844
3515.975164	1054393.614511	42.686848
3515.834397	1054089.430044	42.691853
3515.835819	1053780.576820	42.696858
3515.991452	1053440.339706	42.701863
3515.649271	1053116.847853	42.706868
3515.929737	1052789.087326	42.711872
3515.534448	1052486.592545	42.716877
3515.543593	1052156.234986	42.721882
3515.824893	1051840.282292	42.726887
3515.721887	1051512.219829	42.731892
3515.522932	1051196.212962	42.736896
3515.488547	1050890.966624	42.741901
3515.768524	1050579.959072	42.746906
3515.804080	1050265.790121	42.751911
3515.519136	1049941.524062	42.756916
3515.781800	1049613.288749	42.761920
3515.454136	1049289.377517	42.766925
3515.918229	1048983.364805	42.771930
3515.416774	1048680.968849	42.776935
3515.566448	1048359.241006	42.781940
3515.638886	1048021.869469	42.786945
3515.450985	1047708.074797	42.791949
3515.760819	1047392.346108	42.796954
3515.779502	1047075.971564	42.801959
3515.750490	1046759.973018	42.806964
3515.661808	1046460.863696	42.811969
3515.399253	1046138.302322	42.816973
3515.388607	1045815.390984	42.821978
3515.324476	1045511.108279	42.826983
3515.512261	1045192.087461	42.831988
3515.308995	1044857.466045	42.836993
3515.236187	1044570.904692	42.841997
3515.377948	1044241.888093	42.847002
3515.091970	1043923.451919	42.852007
3514.927342	1043617.536278	42.857012
3515.372395	1043324.352656	42.862017
3515.023747	1043018.530921	42.867021
3515.065006	1042690.501693	42.872026
3515.004925	1042389.235628	42.877031
3514.926939	1042088.632596	42.882036
3514.914418	1041780.658033	42.887041
3514.742920	1041467.183907	42.892045
3515.195100	1041153.396077	42.897050
3514.975318	1040858.838732	42.902055
3514.628115	1040544.954898	42.907060
3515.233402	1040233.796410	42.912065
3514.609224	1039952.694040	42.917069
3515.075489	1039632.921215	42.922074
3514.454600	1039334.095409	42.927079
3514.598987	1039031.163384	42.932084
3514.608507	1038731.621262	42.937089
3514.466195	1038436.342649	42.942093
3514.580016	1038138.878751	42.947098
3514.562289	1037849.253838	42.952103
3514.536453	1037544.141352	42.957108
3514.803055	1037247.184910	42.962113
3514.236735	1036945.416990	42.967117
3514.269088	1036643.630835	42.972122
3514.171929	1036348.233997	42.977127
3514.281858	1036058.301421	42.982132
3514.756151	1035754.459558	42.987137
3514.358305	1035461.774027	42.992141
3514.336434	1035180.718278	42.997146
3514.530977	1034878.906560	43.002151
3514.194046	1034578.230427	43.007156
3514.093828	1034304.787690	43.012161
3514.299195	1034006.507367	43.017165
3514.238176	1033691.318748	43.022170
3513.867831	1033407.617965	43.027175
3514.168702	1033105.789534	43.032180
3514.569267	1032813.994916	43.037185
3514.352980	1032552.390981	43.042189
3514.425655	1032237.872598	43.047194
3514.131829	1031929.399017	43.052199
3514.063508	1031642.267192	43.057204
3514.146561	1031368.553496	43.062209
3513.847872	1031075.621331	43.067213
3513.749388	1030775.378642	43.072218
3513.671345	1030494.483269	43.077223
3513.520892	1030227.239953	43.082228
3513.958001	1029943.133175	43.087233
3513.733705	1029658.055552	43.092237
3513.673571	1029373.226904	43.097242
3513.930154	1029073.802804	43.102247
3513.514400	1028797.817520	43.107252
3513.535597	1028531.239711	43.112257
3513.411568	1028245.201678	43.117261
3513.345492	1027941.604535	43.122266
3513.115156	1027674.833558	43.127271
3513.283376	1027417.479175	43.132276
3513.203569	1027141.550555	43.137281
3512.883131	1026863.613119	43.142285
3513.398633	1026587.171523	43.147290
3513.153507	1026334.971205	43.152295
3512.785147	1026067.564859	43.157300
3513.358794	1025779.153757	43.162305
3513.403206	1025509.423702	43.167309
3513.320452	1025231.753739	43.172314
3512.963448	1024963.808158	43.177319
3513.318472	1024696.895694	43.182324
3513.370939	1024409.081478	43.187329
3513.350661	1024149.475192	43.192333
3513.269503	1023862.527394	43.197338
3513.401338	1023585.806914	43.202343
3513.187010	1023317.662114	43.207348
3512.920887	1023037.489598	43.212353
3512.515330	1022767.313726	43.217357
3513.182281	1022503.833229	43.222362
3512.828501	1022254.861032	43.227367
3512.759868	1021963.643935	43.232372
3513.300083	1021695.491217	43.237377
3512.940081	1021441.246648	43.242381
3513.033266	1021174.403525	43.247386
3513.316806	1020901.114360	43.252391
3512.907719	1020612.114157	43.257396
3513.131799	1020345.598079	43.262401
3513.078927	1020100.749100	43.267405
3512.955948	1019820.974349	43.272410
3512.832988	1019545.745754	43.277415
3512.902274	1019282.115379	43.282420
3512.845862	1019032.174908	43.287425
3512.845655	1018758.828165	43.292429
3512.740909	1018479.856905	43.297434
3512.703056	1018237.738407	43.302439
3512.547509	1017983.788710	43.307444
3512.693018	1017717.063746	43.312449
3512.735194	1017444.519556	43.317453
3512.514047	1017167.443483	43.322458
3512.671801	1016919.412076	43.327463
3512.428658	1016659.981110	43.332468
3512.476127	1016390.200046	43.337473
3512.201842	1016134.827244	43.342477
3512.518571	1015873.326115	43.347482
3512.575552	1015613.311982	43.352487
3512.665610	1015364.931877	43.357492
3512.410566	1015098.051513	43.362497
3512.292764	1014842.788459	43.367501
3512.198260	1014583.916946	43.372506
3512.194195	1014353.667081	43.377511
3511.890341	1014090.825718	43.382516
3511.991732	1013815.473675	43.387521
3512.200597	1013583.117645	43.392525
3512.387162	1013349.590135	43.397530
3511.977743	1013088.564829	43.402535
3511.695723	1012834.791891	43.407540
3512.169626	1012585.740201	43.412545
3512.059899	1012333.276298	43.417549
3511.902717	1012074.299681	43.422554
3512.017160	1011832.754644	43.427559
3511.702910	1011592.532947	43.432564
3511.923880	1011320.925662	43.437569
3511.935595	1011092.580304	43.442573
3511.757186	1010848.126210	43.447578
3511.804225	1010594.684012	43.452583
3511.653889	1010350.495245	43.457588
3512.207862	1010095.780947	43.462593
3511.717863	1009852.306849	43.467597
3511.839682	1009614.941944	43.472602
3511.611844	1009370.237511	43.477607
3511.536555	1009122.775642	43.482612
3511.591110	1008885.391115	43.487617
3511.379062	1008649.109835	43.492621
3511.575986	1008392.044343	43.497626
3511.959327	1008154.088823	43.502631
3511.633858	1007936.754270	43.507636
3511.804353	1007681.508024	43.512641
3511.710156	1007429.696972	43.517645
3511.468117	1007182.663640	43.522650
3511.276667	1006966.144767	43.527655
3511.303948	1006734.800421	43.532660
3511.564312	1006473.747349	43.537665
3511.294222	1006238.833451	43.542669
3511.471954	1006018.035540	43.547674
3511.345130	1005769.268030	43.552679
3511.043869	1005519.837436	43.557684
3511.219907	1005297.358130	43.562689
3511.015539	1005079.504551	43.567693
3511.226028	1004839.784216	43.572698
3511.286415	1004597.160001	43.577703
3510.987756	1004373.846996	43.582708
3511.113500	1004113.874496	43.587713
3510.748415	1003913.125372	43.592717
3510.875968	1003694.190800	43.597722
3511.044793	1003459.770142	43.602727
3510.756929	1003223.371583	43.607732
3510.982282	1003000.988401	43.612737
3510.786272	1002781.585254	43.617741
3510.869003	1002554.439696	43.622746
3510.958398	1002339.740912	43.627751
3510.479051	1002104.008347	43.632756
3510.910109	1001869.867924	43.637761
3510.544385	1001649.183548	43.642765
3510.692281	1001433.078089	43.647770
3510.913404	1001204.687541	43.652775
3510.531294	1000990.209902	43.657780
3510.852606	1000758.669879	43.662785
3510.690319	1000544.041787	43.667789
3510.739443	1000330.246933	43.672794
3510.600097	1000107.323359	43.677799
3510.217515	999867.100550	43.682804
3510.342633	999654.143925	43.687809
3510.401663	999451.803497	43.692813
3510.473484	999239.229539	43.697818
3510.193549	999002.263844	43.702823
3510.113456	998789.211138	43.707828
3510.427833	998576.669763	43.712833
3510.039148	998366.281373	43.717837
3510.243474	998144.392625	43.722842
3510.413822	997933.798721	43.727847
3509.830634	997737.151810	43.732852
3510.002758	997536.282765	43.737857
3510.050396	997325.394271	43.742861
3510.335023	997117.088972	43.747866
3510.408856	996907.349544	43.752871
3510.238201	996683.517136	43.757876
3510.427311	996452.992001	43.762881
3510.387888	996239.739381	43.767885
3510.289922	996031.554673	43.772890
3510.248380	995819.553183	43.777895
3509.682103	995610.358398	43.782900
3510.030689	995402.174493	43.787905
3509.579597	995203.371729	43.792909
3509.819962	994989.928625	43.797914
3510.624652	994792.756142	43.802919
3510.026520	994581.189873	43.807924
3509.968850	994365.530964	43.812929
3509.909178	994161.072175	43.817933
3510.081803	993950.622454	43.822938
3510.064512	993739.124072	43.827943
3509.717636	993539.563606	43.832948
3509.703880	993330.876109	43.837953
3509.476214	993140.834528	43.842957
3509.561601	992938.744809	43.847962
3509.860041	992746.751252	43.852967
3509.681881	992532.992319	43.857972
3509.883572	992328.814505	43.862977
3509.812686	992128.281587	43.867981
3509.488050	991919.203477	43.872986
3509.350938	991727.539738	43.877991
3509.278975	991541.709141	43.882996
3509.448573	991329.310256	43.888001
3509.234208	991136.761745	43.893005
3509.391404	990965.696464	43.898010
3509.362363	990764.816024	43.903015
3509.177023	990542.011677	43.908020
3509.164506	990346.477490	43.913025
3509.093428	990184.788817	43.918029
3509.180747	989998.393925	43.923034
3509.202051	989794.740050	43.928039
3508.814236	989614.750649	43.933044
3508.983088	989417.203891	43.938049
3509.456675	989229.354615	43.943053
3509.436975	989037.190711	43.948058
3509.281208	988844.067214	43.953063
3509.121699	988638.645830	43.958068
3509.146609	988454.356881	43.963073
3509.483692	988294.303338	43.968077
3509.342981	988082.614885	43.973082
3509.549910	987886.179529	43.978087
3509.317347	987696.054361	43.983092
3509.223057	987513.998764	43.988097
3509.182742	987308.314619	43.993101
3508.977433	987112.505955	43.998106
3509.099671	986950.303259	44.003111
3509.321681	986747.678369	44.008116
3509.531380	986543.779621	44.013121
3508.786647	986370.773004	44.018125
3508.751795	986180.662297	44.023130
3509.141608	985984.814470	44.028135
3508.757320	985793.284387	44.033140
3509.028663	985618.818740	44.038145
3509.126358	985436.957996	44.043149
3509.050068	985233.840391	44.048154
3508.992073	985065.073636	44.053159
3508.827526	984867.619276	44.058164
3508.954651	984685.924982	44.063169
3508.703206	984511.999705	44.068173
3508.726025	984334.802199	44.073178
3508.925231	984154.641180	44.078183
3508.842554	983971.982388	44.083188
3508.935695	983774.154837	44.088193
3508.946673	983580.923133	44.093197
3509.023855	983422.630841	44.098202
3508.880319	983230.584461	44.103207
3508.851310	983055.796979	44.108212
3508.906811	982853.256476	44.113217
3508.907791	982690.854966	44.118221
3508.663518	982503.781236	44.123226
3508.599905	982315.109005	44.128231
3508.375343	982134.758714	44.133236
3508.401878	981966.960745	44.138241
3508.362460	981802.391895	44.143245
3508.373421	981600.693358	44.148250
3508.494436	981433.157177	44.153255
3508.230667	981271.051936	44.158260
3508.479463	981088.930080	44.163265
3508.514844	980914.261823	44.168269
3508.256305	980742.274278	44.173274
3508.406194	980567.576566	44.178279
3508.400150	980407.651330	44.183284
3508.308743	980238.551982	44.188289
3508.293345	980066.992564	44.193293
3508.455334	979886.703045	44.198298
3508.284194	979716.233509	44.203303
3508.171528	979563.337181	44.208308
3508.220750	979382.073221	44.213313
3508.087999	979209.627985	44.218317
3508.046906	979020.159232	44.223322
3508.162207	978872.386033	44.228327
3508.082074	978696.007752	44.233332
3508.347333	978537.940048	44.238337
3508.065684	978388.558354	44.243341
3508.089298	978210.486596	44.248346
3508.340781	978024.943776	44.253351
3508.038250	977865.387223	44.258356
3508.416085	977695.842187	44.263361
3508.119015	977535.200362	44.268365
3508.058312	977369.236706	44.273370
3508.194780	977199.521231	44.278375
3507.861765	977033.885954	44.283380
3507.946550	976863.093728	44.288385
3507.816248	976705.236081	44.293389
3508.009099	976525.226596	44.298394
3508.182570	976373.273271	44.303399
3507.530734	976201.996059	44.308404
3507.887940	976044.430975	44.313409
3507.845134	975886.634122	44.318413
3507.930302	975711.994348	44.323418
3507.807607	975565.152731	44.328423
3507.517052	975420.779529	44.333428
3508.330081	975243.561069	44.338433
3507.386664	975078.947610	44.343437
3507.761760	974918.121640	44.348442
3507.866632	974756.748910	44.353447
3507.850770	974589.817186	44.358452
3507.882245	974441.650044	44.363457
3508.138761	974283.759751	44.368461
3507.873608	974124.092767	44.373466
3507.767036	973951.191376	44.378471
3507.500238	973798.264218	44.383476
3507.928898	973638.273813	44.388481
3507.294719	973484.029416	44.393485
3507.313843	973340.530936	44.398490
3507.516197	973187.608037	44.403495
3507.456066	973029.931016	44.408500
3507.374822	972885.948584	44.413505
3507.363593	972740.092294	44.418509
3507.518800	972568.769162	44.423514
3507.379303	972406.881398	44.428519
3507.437136	972270.393722	44.433524
3507.479244	972107.097899	44.438529
3507.353636	971979.047549	44.443533
3507.178086	971826.052764	44.448538
3507.214166	971684.956144	44.453543
3507.302491	971518.602770	44.458548
3507.142943	971359.330642	44.463553
3506.762929	971229.642010	44.468557
3506.992654	971070.199893	44.473562
3507.161136	970924.169992	44.478567
3507.075798	970789.334261	44.483572
3507.121618	970623.353389	44.488577
3506.799921	970492.855597	44.493581
3506.921866	970353.963024	44.498586
3506.903756	970205.792499	44.503591
3506.608140	970080.859644	44.508596
3506.706083	969931.292711	44.513601
3506.710157	969794.265641	44.518605
3506.910317	969652.504786	44.523610
3506.897404	969516.061156	44.528615
3506.838734	969374.140301	44.533620
3507.035703	969251.261726	44.538625
3506.840104	969093.694641	44.543629
3506.786846	968941.288055	44.548634
3506.990133	968811.448720	44.553639
3506.518702	968692.877730	44.558644
3506.790120	968548.336817	44.563649
3506.496375	968409.465702	44.568653
3506.966156	968277.318694	44.573658
3507.018318	968139.950545	44.578663
3506.711410	968008.610622	44.583668
3506.903916	967856.232695	44.588673
3506.884172	967715.439388	44.593677
3506.879763	967575.913004	44.598682
3506.895113	967447.934217	44.603687
3506.581697	967303.262497	44.608692
3506.706335	967146.568481	44.613697
3506.608473	967027.118208	44.618701
3506.551833	966894.536518	44.623706
3506.667647	966756.439350	44.628711
3506.435239	966628.189340	44.633716
3506.725124	966481.145157	44.638721
3506.641155	966355.998506	44.643725
3506.683864	966227.400442	44.648730
3507.170498	966104.015154	44.653735
3506.621022	965958.662905	44.658740
3506.744026	965807.711302	44.663745
3506.669381	965679.218261	44.668749
3506.379935	965545.272557	44.673754
3506.404414	965416.855282	44.678759
3505.901166	965287.052750	44.683764
3505.996222	965159.499694	44.688769
3506.456823	965040.601888	44.693773
3505.991093	964891.192586	44.698778
3506.469984	964780.515091	44.703783
3506.518497	964661.089549	44.708788
3506.460255	964523.751192	44.713793
3506.514832	964412.450745	44.718797
3506.610417	964275.277065	44.723802
3506.611842	964138.017654	44.728807
3506.586188	963995.076830	44.733812
3506.518967	963872.322812	44.738817
3506.272332	963759.099788	44.743821
3506.404431	963618.867084	44.748826
3506.456820	963499.122863	44.753831
3506.137742	963373.166202	44.758836
3506.304174	963243.305263	44.763841
3506.094613	963119.970721	44.768845
3506.131807	962984.049792	44.773850
3506.684245	962869.403761	44.778855
3506.146647	962741.999362	44.783860
3506.369516	962601.432958	44.788865
3506.278296	962490.217386	44.793869
3506.014669	962360.603393	44.798874
3506.282543	962233.839122	44.803879
3506.312785	962119.558209	44.808884
3505.927017	961982.605240	44.813889
3506.165744	961860.150000	44.818893
3506.205630	961736.156681	44.823898
3506.104243	961629.238799	44.828903
3505.955143	961515.563549	44.833908
3506.142648	961376.639419	44.838913
3505.971427	961272.961106	44.843917
3505.969599	961150.432395	44.848922
3506.282576	961017.066322	44.853927
3506.057975	960905.744122	44.858932
3506.460844	960779.905949	44.863937
3505.885034	960643.442613	44.868941
3505.784271	960513.368125	44.873946
3506.169569	960400.759304	44.878951
3506.007935	960294.316779	44.883956
3506.012008	960168.727040	44.888961
3505.962779	960056.281107	44.893965
3505.864632	959933.350237	44.898970
3506.153716	959796.332224	44.903975
3505.852417	959680.684926	44.908980
3505.960141	959569.870502	44.913985
3505.836056	959461.739561	44.918989
3505.787013	959338.885992	44.923994
3505.722117	959236.134102	44.928999
3505.725841	959107.481562	44.934004
3505.802681	958979.108297	44.939009
3505.523208	958877.758224	44.944013
3505.690301	958765.839896	44.949018
3506.094401	958651.526764	44.954023
3505.644368	958530.291097	44.959028
3506.086586	958426.166374	44.964033
3505.658955	958314.435322	44.969037
3505.649082	958195.277717	44.974042
3505.774744	958081.783766	44.979047
3505.874062	957960.837966	44.984052
3505.841902	957839.518966	44.989057
3505.811521	957736.734705	44.994061
3505.532736	957628.791072	44.999066
3505.666509	957519.011925	45.004071
3505.859301	957403.433786	45.009076
3505.969657	957267.071818	45.014081
3505.840013	957167.040296	45.019085
3505.699744	957061.221264	45.024090
3505.877429	956944.361214	45.029095
3505.779044	956856.090636	45.034100
3505.681956	956736.132519	45.039105
3505.718312	956614.874615	45.044109
3505.382248	956485.925334	45.049114
3505.782377	956383.830927	45.054119
3505.417501	956295.595677	45.059124
3505.352659	956169.243539	45.064129
3505.342920	956055.437761	45.069133
3505.458964	955950.635393	45.074138
3505.484872	955861.214708	45.079143
3505.360562	955753.756571	45.084148
3505.610291	955633.898969	45.089153
3505.573473	955539.235605	45.094157
3504.959839	955434.624490	45.099162
3505.054043	955336.780035	45.104167
3505.081632	955257.879827	45.109172
3505.298593	955145.857945	45.114177
3505.337454	955036.158200	45.119181
3505.264284	954946.271600	45.124186
3505.456877	954844.384698	45.129191
3505.118935	954748.991123	45.134196
3505.317239	954638.778358	45.139201
3505.091338	954525.189836	45.144205
3505.296097	954435.248449	45.149210
3505.206628	954338.371554	45.154215
3505.024826	954262.168595	45.159220
3504.827806	954151.532160	45.164225
3504.978993	954060.445160	45.169229
3505.226395	953956.522757	45.174234
3505.374086	953853.092955	45.179239
3505.248535	953780.508551	45.184244
3505.055903	953671.391540	45.189249
3505.256381	953553.310718	45.194253
3505.342362	953445.386622	45.199258
3505.352923	953361.580925	45.204263
3504.812716	953278.342912	45.209268
3504.925279	953182.080484	45.214273
3505.116834	953100.058435	45.219277
3504.973810	953007.566039	45.224282
3505.278668	952890.409459	45.229287
3504.738508	952798.935460	45.234292
3505.070788	952694.782074	45.239297
3505.230947	952613.618520	45.244301
3505.003821	952518.547733	45.249306
3505.140896	952436.428339	45.254311
3505.044875	952331.189884	45.259316
3505.132256	952213.957959	45.264321
3505.149456	952131.853426	45.269325
3504.791130	952045.790362	45.274330
3504.961435	951947.294287	45.279335
3504.808299	951852.486027	45.284340
3505.078801	951754.065433	45.289345
3504.858629	951665.772187	45.294349
3504.892469	951566.621381	45.299354
3505.073275	951485.532261	45.304359
3504.699907	951406.255805	45.309364
3504.896854	951302.670647	45.314369
3504.988265	951197.952288	45.319373
3504.914815	951114.697903	45.324378
3505.084694	951024.032340	45.329383
3504.678269	950939.968562	45.334388
3504.958637	950841.624559	45.339393
3505.130532	950759.664012	45.344397
3505.044102	950651.326585	45.349402
3505.083062	950550.623822	45.354407
3505.056322	950474.338913	45.359412
3505.031656	950384.459877	45.364417
3505.147970	950277.612747	45.369421
3504.811937	950180.314865	45.374426
3505.213457	950085.574066	45.379431
3505.059721	950017.153030	45.384436
3504.943779	949909.762131	45.389441
3504.912513	949809.630813	45.394445
3504.629813	949721.027218	45.399450
3504.850000	949638.083488	45.404455
3504.925564	949554.109120	45.409460
3504.919834	949454.158158	45.414465
3505.006756	949367.019435	45.419469
3504.365042	949280.477965	45.424474
3504.766436	949210.422871	45.429479
3504.614666	949115.180880	45.434484
3504.777575	949022.662003	45.439489
3504.826184	948939.352291	45.444493
3504.626633	948857.709880	45.449498
3504.647981	948765.401205	45.454503
3504.377685	948670.745038	45.459508
3504.319720	948591.468962	45.464513
3504.750306	948505.599664	45.469517
3504.711812	948420.668033	45.474522
3504.864399	948349.014312	45.479527
3504.847547	948248.275710	45.484532
3504.895621	948166.102751	45.489537
3504.835908	948079.349476	45.494541
3504.722057	947988.389889	45.499546
3504.890946	947892.689435	45.504551
3504.549710	947808.180665	45.509556
3504.787704	947727.980642	45.514561
3504.546098	947627.745812	45.519565
3504.562136	947555.241601	45.524570
3504.491261	947476.908290	45.529575
3504.266839	947386.243640	45.534580
3504.527683	947290.037987	45.539585
3504.074678	947222.012255	45.544589
3504.049503	947169.815121	45.549594
3504.446778	947080.192101	45.554599
3504.228086	946998.810789	45.559604
3504.493373	946915.145374	45.564609
3504.596708	946820.776901	45.569613
3504.478848	946747.325523	45.574618
3504.545834	946671.447860	45.579623
3504.128848	946613.849504	45.584628
3504.496632	946512.726344	45.589633
3504.511077	946416.832430	45.594637
3504.320024	946340.609232	45.599642
3504.425891	946280.621897	45.604647
3504.574881	946187.958758	45.609652
3504.450347	946116.128140	45.614657
3504.677547	946026.802316	45.619661
3504.395010	945945.798179	45.624666
3504.332724	945866.864250	45.629671
3504.214463	945776.058095	45.634676
3504.638409	945685.544287	45.639681
3504.420135	945602.224750	45.644685
3504.684246	945526.872732	45.649690
3504.528617	945452.834342	45.654695
3504.456547	945382.517949	45.659700
3503.875839	945287.180239	45.664705
3504.538644	945205.817205	45.669709
3504.534694	945127.341510	45.674714
3504.531859	945070.041052	45.679719
3504.203258	944981.746996	45.684724
3504.547359	944888.741049	45.689729
3504.604125	944826.061886	45.694733
3503.988525	944755.826524	45.699738
3504.305419	944667.133322	45.704743
3503.933473	944577.881246	45.709748
3504.102364	944505.692510	45.714753
3504.330643	944429.755490	45.719757
3504.079392	944335.975210	45.724762
3504.208757	944273.373259	45.729767
3504.352876	944212.589036	45.734772
3504.297560	944127.014723	45.739777
3503.685712	944041.626504	45.744781
3504.293719	943987.759605	45.749786
3504.322989	943912.518705	45.754791
3504.054047	943848.156226	45.759796
3503.980261	943772.930281	45.764801
3504.301780	943691.599785	45.769805
3503.795747	943605.611895	45.774810
3503.893763	943532.366996	45.779815
3503.998936	943401.896382	45.784820
3504.014503	943206.639081	45.789825
3504.113116	942956.433014	45.794829
3504.000893	942652.660806	45.799834
3504.503723	942268.524413	45.804839
3504.190065	941847.292600	45.809844
3504.161088	941343.898649	45.814849
3504.054217	940769.407187	45.819853
3503.801219	940130.519972	45.824858
3504.269247	939434.265096	45.829863
3503.574603	938688.797125	45.834868
3503.582544	937832.569494	45.839873
3503.397035	936918.652220	45.844877
3502.949069	935944.147278	45.849882
3503.351192	934904.517878	45.854887
3503.195849	933787.474380	45.859892
3502.783326	932577.358853	45.864897
3502.961871	931293.471452	45.869901
3502.523841	929944.991750	45.874906
3502.535932	928497.860789	45.879911
3502.086765	926979.456640	45.884916
3501.987957	925361.021319	45.889921
3501.675749	923684.121618	45.894925
3501.312984	921930.007516	45.899930
3501.420759	920065.883804	45.904935
3501.026792	918113.469323	45.909940
3500.876711	916102.801063	45.914945
3500.431950	913982.440090	45.919949
3499.939878	911781.919388	45.924954
3499.754340	909497.134189	45.929959
3499.492496	907130.074571	45.934964
3499.342721	904687.946875	45.939969
3499.139242	902159.675148	45.944973
3498.448205	899524.638823	45.949978
3498.448642	896826.585432	45.954983
3497.637068	894025.153803	45.959988
3497.553030	891116.172358	45.964993
3497.143011	888137.808563	45.969997
3496.583815	885072.014498	45.975002
3496.328480	881923.046537	45.980007
3495.527574	878689.661305	45.985012
3495.215895	875403.776249	45.990017
3494.767909	871997.265722	45.995021
3494.360010	868510.806017	46.000026
3494.074462	864939.594327	46.005031
3493.342328	861285.244365	46.010036
3492.892043	857534.366303	46.015041
3492.257777	853708.691920	46.020045
3491.929855	849785.610856	46.025050
3491.212286	845772.193328	46.030055
3490.659330	841690.003638	46.035060
3490.156765	837518.157330	46.040065
3489.158558	833257.620346	46.045069
3488.629891	828915.563462	46.050074
3488.578829	824482.998063	46.055079
3487.260701	819982.377572	46.060084
3486.676084	815368.205229	46.065089
3486.106816	810694.312164	46.070093
3485.416941	805920.217955	46.075098
3484.926147	801064.298538	46.080103
3483.709336	796134.283566	46.085108
3483.361320	791096.862825	46.090113
3482.407346	785966.700423	46.095117
3481.463883	780780.602785	46.100122
3480.837947	775494.803888	46.105127
3479.963940	770115.292032	46.110132
3479.196517	764665.828356	46.115137
3478.532877	759142.166482	46.120141
3477.285707	753488.687556	46.125146
3476.597042	747752.581898	46.130151
3475.660166	741981.798915	46.135156
3474.948614	736091.387414	46.140161
3474.203382	730108.241962	46.145165
3472.820841	724048.189916	46.150170
3472.182725	717872.101300	46.155175
3470.853549	711654.262230	46.160180
3469.825066	705317.818052	46.165185
3468.939298	698899.458992	46.170189
3467.547453	692395.111361	46.175194
3466.969709	685815.557260	46.180199
3465.341903	679147.769039	46.185204
3464.541956	672400.859043	46.190209
3463.814930	665571.078982	46.195213
3462.261428	658643.010651	46.200218
3461.128466	651639.525243	46.205223
3460.018625	644553.626517	46.210228
3458.897527	637364.329777	46.215233
3458.002523	630089.465943	46.220237
3456.239789	622749.043945	46.225242
3455.397343	615291.995338	46.230247
3454.054573	607788.540605	46.235252
3452.780251	600195.375250	46.240257
3451.556340	592517.321078	46.245261
3450.141546	584727.276130	46.250266
3448.781691	576861.490199	46.255271
3447.070862	568945.644688	46.260276
3445.641929	560929.503830	46.265281
3444.308647	552835.635427	46.270285
3442.674180	544648.624353	46.275290
3441.211582	536384.523365	46.280295
3439.494602	528047.408595	46.285300
3437.888987	519629.015105	46.290305
3436.167920	511142.697214	46.295309
3434.504099	502576.896197	46.300314
3433.379578	493920.794581	46.305319
3431.372076	485176.530659	46.310324
3429.697139	476365.370494	46.315329
3428.004301	467506.454065	46.320333
3426.084685	458542.035223	46.325338
3424.800193	449496.561383	46.330343
3422.505862	440402.250460	46.335348
3420.550672	431205.309582	46.340353
3418.777675	421957.707586	46.345357
3416.363314	412643.620490	46.350362
3414.614516	403219.546135	46.355367
3412.366797	393780.008691	46.360372
3410.170032	384229.274046	46.365377
3407.890318	374627.009530	46.370381
3405.821846	364984.992729	46.375386
3403.554295	355249.420707	46.380391
3400.982272	345461.594189	46.385396
3399.034223	335636.523331	46.390401
3396.477633	325737.738488	46.395405
3393.991961	315782.793956	46.400410
3391.467793	305749.493347	46.405415
3388.725322	295677.377437	46.410420
3386.075375	285556.956667	46.415425
3383.313149	275412.702252	46.420429
3380.183320	265189.845783	46.425434
3377.441034	254901.813199	46.430439
3374.101346	244590.163472	46.435444
3370.921427	234271.212825	46.440449
3367.651832	223881.306974	46.445453
3364.447072	213407.141680	46.450458
3361.171518	202951.158724	46.455463
3357.365430	192518.237297	46.460468
3354.058250	182017.878234	46.465473
3350.033501	171507.788289	46.470477
3345.801055	161005.358314	46.475482
3342.020602	150496.938710	46.480487
3337.452826	139971.140615	46.485492
3332.249519	129424.558924	46.490497
3327.189708	118928.574526	46.495501
3321.476256	108472.976260	46.500506
3315.073210	98039.529921	46.505511
3306.549170	87725.150651	46.510516
3294.083360	77556.962983	46.515521
3262.668305	68050.698113	46.520525
3217.909512	59244.719828	46.525530
3171.291314	51096.090579	46.530535
3125.125595	43739.748619	46.535540
3082.596202	37190.630079	46.540545
3045.054072	31491.885259	46.545549
3011.193065	26640.577205	46.550554
2983.291005	22589.635568	46.555559
2959.435426	19237.382977	46.560564
2940.682832	16536.560649	46.565569
2925.243454	14399.064041	46.570573
2913.210600	12740.000233	46.575578
2903.925242	11463.550421	46.580583
2896.473116	10520.412483	46.585588
2890.672363	9839.061779	46.590593
2886.963520	9343.811204	46.595597
2884.511154	8997.013191	46.600602
2882.418231	8791.680239	46.605607
2880.514224	8657.521687	46.610612
2879.777451	8556.299624	46.615617
2879.342164	8511.779171	46.620621
2878.460678	8477.599008	46.625626
2877.917684	8431.713125	46.630631
2877.453115	8403.976356	46.635636
2877.451848	8366.436813	46.640641
2876.990978	8288.955705	46.645645
2876.293344	8176.819600	46.650650
2875.828915	8063.188249	46.655655
2874.400181	7938.513165	46.660660
2873.367303	7778.018286	46.665665
2872.257300	7565.451935	46.670669
2870.213166	7354.751838	46.675674
2869.127657	7120.684527	46.680679
2867.255675	6874.778574	46.685684
2865.155403	6583.541312	46.690689
2862.970148	6291.286833	46.695693
2860.337367	5980.988356	46.700698
2857.932120	5647.464871	46.705703
2855.063326	5316.308422	46.710708
2852.709292	4964.049707	46.715713
2849.921227	4607.586290	46.720717
2846.505880	4225.615085	46.725722
2843.756184	3833.893301	46.730727
2840.708925	3464.899438	46.735732
2837.592441	3076.754317	46.740737
2834.194033	2660.257378	46.745741
2830.752953	2273.636305	46.750746
2827.398025	1886.874764	46.755751
2823.552475	1486.076658	46.760756
2819.442668	1074.530971	46.765761
2815.840219	699.093052	46.770765
2810.590770	350.732269	46.775770
2797.193750	246.345728	46.780775
2782.196279	270.839435	46.785780
2773.451455	260.895346	46.790785
2769.993150	272.086910	46.795789
2768.441293	275.764290	46.800794
2767.686588	288.422483	46.805799
2766.621267	270.300407	46.810804
2764.860318	249.738293	46.815809
2762.238743	253.591334	46.820813
2758.554408	276.458029	46.825818
2755.342441	270.726677	46.830823
2751.865861	254.069647	46.835828
2748.190949	266.691740	46.840833
2745.002699	258.454127	46.845837
2741.890744	264.841649	46.850842
2738.969611	260.707747	46.855847
2735.965211	273.259455	46.860852
2732.441554	264.088962	46.865857
2729.382648	249.517710	46.870861
2725.621131	266.883177	46.875866
2722.092434	261.182064	46.880871
2718.644790	253.007554	46.885876
2715.263782	255.682943	46.890881
2712.516520	265.347682	46.895885
2708.846367	273.041631	46.900890
2705.759179	257.957823	46.905895
2702.375501	260.487262	46.910900
2698.927358	267.797065	46.915905
2695.031095	247.035780	46.920909
2691.707459	251.049969	46.925914
2688.648276	250.296504	46.930919
2685.081394	272.849572	46.935924
2681.885385	258.519649	46.940929
2678.284587	233.193974	46.945933
2674.717626	245.218116	46.950938
2671.515733	261.790615	46.955943
2668.648940	256.232353	46.960948
2664.754908	246.975788	46.965953
2661.299638	237.100962	46.970957
2657.592272	249.505078	46.975962
2654.604952	247.928186	46.980967
2651.025817	246.570211	46.985972
2647.179443	254.236308	46.990977
2644.213826	238.986705	46.995981
2641.207676	247.699942	47.000986
2637.896858	246.687401	47.005991
2633.750380	253.612206	47.010996
2630.365596	247.198446	47.016001
2627.091792	246.547870	47.021005
2623.652315	246.037565	47.026010
2620.076711	225.871722	47.031015
2616.024578	245.778192	47.036020
2613.033355	250.052395	47.041025
2609.777315	239.957212	47.046029
2606.108852	235.861065	47.051034
2602.898335	222.035149	47.056039
2598.201478	243.737501	47.061044
2595.864837	244.075276	47.066049
2592.605990	241.274048	47.071053
2588.338024	244.184813	47.076058
2584.975867	246.928865	47.081063
2581.988180	241.242506	47.086068
2578.469586	228.576417	47.091073
2575.329218	236.776525	47.096077
2571.597665	250.294372	47.101082
2568.266305	229.349497	47.106087
2564.565682	220.760743	47.111092
2561.035767	235.461487	47.116097
2558.257292	245.571081	47.121101
2553.919541	246.438001	47.126106
2550.486029	228.616665	47.131111
2547.505482	232.056324	47.136116
2543.535433	243.502198	47.141121
2540.056664	246.101145	47.146125
2537.042098	247.144986	47.151130
2533.602927	228.564497	47.156135
2529.804340	217.004213	47.161140
2526.374850	240.975787	47.166145
2522.538556	228.859215	47.171149
2519.173243	221.070785	47.176154
2516.100417	230.065837	47.181159
2512.377999	235.075819	47.186164
2509.425648	231.365445	47.191169
2505.710269	234.818267	47.196173
2502.010793	229.511037	47.201178
2498.706681	220.248861	47.206183
2495.303175	230.321148	47.211188
2491.189278	227.028225	47.216193
2487.958544	222.996395	47.221197
2484.499054	231.947690	47.226202
2480.979635	222.561903	47.231207
2478.011903	225.170815	47.236212
2474.574693	213.109716	47.241217
2471.168193	224.168604	47.246221
2467.333226	233.770167	47.251226
2463.204666	226.659174	47.256231
2460.136754	246.105276	47.261236
2456.511664	235.835162	47.266241
2453.148401	205.355347	47.271245
2450.019914	221.702273	47.276250
2446.847777	231.237061	47.281255
2442.851067	224.433335	47.286260
2439.373563	216.759632	47.291265
2435.676836	215.335921	47.296269
2432.138590	217.729465	47.301274
2428.858558	213.348388	47.306279
2425.371209	215.722690	47.311284
2421.392327	219.673972	47.316289
2418.231794	218.104927	47.321293
2414.891725	232.368761	47.326298
2411.709419	219.921962	47.331303
2408.116733	207.866521	47.336308
2404.745777	205.257301	47.341313
2401.025807	224.057826	47.346317
2397.460136	226.257327	47.351322
2394.099229	205.474524	47.356327
2390.578271	225.595212	47.361332
2386.638655	214.144201	47.366337
2383.439566	184.797623	47.371341
2379.636778	220.058232	47.376346
2376.472535	200.736963	47.381351
2373.259214	219.601716	47.386356
2369.520380	206.664699	47.391361
2366.478440	199.103790	47.396365
2362.624443	217.710972	47.401370
2359.177484	218.448854	47.406375
2355.377852	221.669308	47.411380
2352.208347	221.300856	47.416385
2348.909138	209.497537	47.421389
2344.656389	202.490961	47.426394
2341.562943	204.076942	47.431399
2338.257613	202.722503	47.436404
2334.368662	212.299469	47.441409
2331.236573	212.496825	47.446413
2327.745509	226.890443	47.451418
2324.238847	216.471560	47.456423
2320.532710	195.407091	47.461428
2316.885999	209.006689	47.466433
2313.860839	214.130527	47.471437
2310.188072	206.527281	47.476442
2306.692482	190.107638	47.481447
2303.288140	206.671036	47.486452
2299.552171	217.524172	47.491457
2296.107439	210.097690	47.496461
2292.604537	198.117980	47.501466
2289.088321	204.875550	47.506471
2285.415554	208.931782	47.511476
2282.423770	206.885719	47.516481
2279.084633	198.563167	47.521485
2275.175552	225.175586	47.526490
2271.686480	199.430539	47.531495
2268.400371	193.351709	47.536500
2264.596694	193.363907	47.541505
2261.765692	202.862202	47.546509
2257.370081	205.686759	47.551514
2254.050695	204.432635	47.556519
2250.824772	215.844762	47.561524
2247.411414	216.107483	47.566529
2243.752975	202.890938	47.571533
2239.873845	188.556215	47.576538
2237.052998	192.696386	47.581543
2233.649299	211.214928	47.586548
2229.861890	202.248661	47.591553
2226.544503	186.094643	47.596557
2222.181196	201.918614	47.601562
2219.012131	214.416673	47.606567
2215.943103	218.626201	47.611572
2212.278632	200.126721	47.616577
2208.831793	195.467553	47.621581
2205.278210	209.040780	47.626586
2201.520698	216.694658	47.631591
2198.178577	208.829285	47.636596
2194.852286	203.588234	47.641601
2191.511520	210.505723	47.646605
2188.175408	196.918995	47.651610
2184.207381	199.788093	47.656615
2180.944407	199.359961	47.661620
2177.178119	206.909148	47.666625
2174.006742	193.995868	47.671629
2170.070456	209.131793	47.676634
2166.588770	202.032879	47.681639
2163.050681	205.193709	47.686644
2159.494074	193.469860	47.691649
2156.440980	197.092280	47.696653
2152.774687	216.559762	47.701658
2149.260925	192.312044	47.706663
2145.831099	183.977303	47.711668
2142.256480	194.225885	47.716673
2138.936641	208.491470	47.721677
2135.069084	213.725611	47.726682
2131.931580	186.509748	47.731687
2128.592154	182.764945	47.736692
2125.117279	209.037623	47.741697
2121.366378	196.806034	47.746701
2117.734979	191.565042	47.751706
2114.215113	197.255405	47.756711
2110.767189	202.495311	47.761716
2106.852783	196.205801	47.766721
2104.008674	191.375553	47.771725
2100.113743	211.351312	47.776730
2096.440870	187.722767	47.781735
2093.275017	180.739511	47.786740
2090.047357	198.377008	47.791745
2086.434178	199.105437	47.796749
2082.929037	190.476549	47.801754
2079.495689	196.794169	47.806759
2076.181030	202.891859	47.811764
2072.521795	181.217699	47.816769
2068.973350	173.823954	47.821773
2065.022545	194.111672	47.826778
2061.655732	196.043241	47.831783
2058.497092	189.354360	47.836788
2054.659358	175.800955	47.841793
2051.777994	189.411796	47.846797
2047.809595	187.369291	47.851802
2044.202457	188.132060	47.856807
2040.718174	194.314267	47.861812
2036.874642	199.253176	47.866817
2033.698865	184.013679	47.871821
2030.285554	180.764196	47.876826
2027.154163	195.963206	47.881831
2023.385790	188.785890	47.886836
2019.933808	174.549361	47.891841
2016.756737	178.655140	47.896845
2012.577373	204.969072	47.901850
2008.931393	184.392112	47.906855
2005.442910	182.639115	47.911860
2001.884336	196.465270	47.916865
1998.720683	201.650139	47.921869
1995.226563	202.895623	47.926874
1991.979407	175.774027	47.931879
1988.858959	178.504585	47.936884
1984.906158	190.990422	47.941889
1981.525479	201.819883	47.946893
1977.515896	203.629545	47.951898
1974.334573	192.330833	47.956903
1970.807526	182.472219	47.961908
1967.251423	183.349918	47.966913
1963.726822	183.960015	47.971917
1960.464292	192.354175	47.976922
1957.395151	177.716554	47.981927
1953.672046	174.020139	47.986932
1949.732753	185.590468	47.991937
1946.300933	189.842969	47.996941
1942.639542	183.065438	48.001946
1939.142916	183.120472	48.006951
1935.675083	185.599886	48.011956
1932.308197	184.719834	48.016961
1929.079714	174.326349	48.021965
1925.508427	191.510257	48.026970
1921.884680	182.886037	48.031975
1918.177702	161.869004	48.036980
1914.354247	182.753977	48.041985
1911.341986	193.436952	48.046989
1908.168091	192.858999	48.051994
1904.583496	167.392150	48.056999
1901.051098	163.687389	48.062004
1897.154284	189.275024	48.067009
1893.867135	177.581968	48.072013
1889.954321	180.142112	48.077018
1886.706247	183.890416	48.082023
1883.081082	190.969955	48.087028
1879.897598	202.396890	48.092033
1876.614128	174.320237	48.097037
1872.927350	167.005065	48.102042
1869.330565	172.941713	48.107047
1865.901177	180.183295	48.112052
1862.061506	180.168690	48.117057
1858.878127	181.962163	48.122061
1855.251137	192.811976	48.127066
1851.658762	173.858839	48.132071
1848.295492	160.213596	48.137076
1844.820654	172.002290	48.142081
1841.661246	176.383216	48.147085
1838.169075	179.320866	48.152090
1834.250488	162.391096	48.157095
1830.709400	173.332780	48.162100
1826.872541	199.537274	48.167105
1823.828125	180.254915	48.172109
1820.356864	174.685216	48.177114
1816.998040	155.963890	48.182119
1813.455405	177.762998	48.187124
1809.664913	188.862254	48.192129
1806.502867	176.656549	48.197133
1802.502348	168.880800	48.202138
1799.206463	162.294316	48.207143
1795.709689	172.002697	48.212148
1792.382553	184.353022	48.217153
1788.495905	176.285925	48.222157
1784.908313	162.668160	48.227162
1781.894922	167.643147	48.232167
1778.481872	158.912447	48.237172
1774.846486	153.193378	48.242177
1771.475428	168.196597	48.247181
1767.712132	177.540463	48.252186
1764.186822	176.164977	48.257191
1760.783148	182.728095	48.262196
1756.912610	165.751089	48.267201
1753.782029	166.259184	48.272205
1750.170157	157.962015	48.277210
1747.017044	169.436340	48.282215
1743.486294	169.206579	48.287220
1739.548211	173.026863	48.292225
1736.293089	163.260360	48.297229
1732.612623	157.622738	48.302234
1729.093015	182.064515	48.307239
1725.814506	168.882813	48.312244
1722.277968	168.612388	48.317249
1718.953384	171.520367	48.322253
1715.345132	179.993651	48.327258
1711.836698	163.654477	48.332263
1708.266002	168.055075	48.337268
1704.700553	181.664735	48.342273
1701.511299	156.721662	48.347277
1697.727590	160.235345	48.352282
1694.396522	170.664571	48.357287
1690.857126	153.998874	48.362292
1686.836095	169.118936	48.367297
1683.646940	176.190141	48.372301
1679.862851	161.654390	48.377306
1676.387183	165.763798	48.382311
1673.166764	173.359252	48.387316
1669.277421	164.768166	48.392321
1666.319248	157.179203	48.397325
1662.713025	178.790659	48.402330
1659.097289	163.411121	48.407335
1656.003402	156.337898	48.412340
1652.549361	163.860629	48.417345
1649.052856	173.851552	48.422349
1644.988409	170.142481	48.427354
1641.474079	152.993547	48.432359
1638.356750	146.589786	48.437364
1634.322132	165.352623	48.442369
1631.018689	164.014483	48.447373
1627.557458	166.124394	48.452378
1624.176870	179.901267	48.457383
1620.811932	185.213601	48.462388
1616.843661	177.302627	48.467393
1613.777802	158.030478	48.472397
1610.314376	164.327591	48.477402
1606.754111	158.886048	48.482407
1603.363036	145.218233	48.487412
1599.326072	158.114953	48.492417
1596.266439	171.162828	48.497421
1592.551333	175.027975	48.502426
1588.907781	160.524833	48.507431
1585.827195	149.178477	48.512436
1582.065910	174.585674	48.517441
1579.167636	155.916654	48.522445
1574.976860	163.000571	48.527450
1571.172957	175.484289	48.532455
1568.107110	156.928258	48.537460
1564.213693	170.541374	48.542465
1561.358141	160.777298	48.547469
1557.748541	154.964920	48.552474
1554.370952	160.608353	48.557479
1550.705323	167.269923	48.562484
1546.981215	179.182827	48.567489
1543.394252	156.304510	48.572493
1540.016451	157.036685	48.577498
1536.683841	163.066310	48.582503
1533.188280	156.563035	48.587508
1529.669178	155.864852	48.592513
1526.204988	169.341252	48.597517
1522.255538	162.804469	48.602522
1518.917532	150.198376	48.607527
1516.006831	156.088341	48.612532
1511.838850	179.704839	48.617537
1508.898396	149.615511	48.622541
1504.910630	151.608762	48.627546
1501.533656	151.656298	48.632551
1498.090703	151.732481	48.637556
1494.838945	148.302332	48.642561
1491.596645	158.499356	48.647565
1487.515309	175.755127	48.652570
1484.093478	164.127559	48.657575
1480.635275	147.143888	48.662580
1476.418686	159.190957	48.667585
1473.645371	162.912471	48.672589
1469.905687	167.088527	48.677594
1466.602267	159.760151	48.682599
1463.247262	160.141851	48.687604
1459.478416	155.441729	48.692609
1456.260854	169.139163	48.697613
1452.150101	160.431658	48.702618
1448.868589	152.209676	48.707623
1445.596715	147.109702	48.712628
1442.044662	165.473546	48.717633
1438.498066	166.173549	48.722637
1434.948343	150.461787	48.727642
1431.521986	148.255508	48.732647
1428.454340	156.971728	48.737652
1424.755700	174.933621	48.742657
1421.278396	152.073903	48.747661
1417.396784	153.318009	48.752666
1413.941985	146.571521	48.757671
1410.295892	159.351924	48.762676
1406.733575	165.338919	48.767681
1403.305009	148.298026	48.772685
1400.152600	152.702923	48.777690
1396.518239	146.279262	48.782695
1393.176231	142.876588	48.787700
1389.408430	152.343669	48.792705
1386.288058	166.531639	48.797709
1382.488863	168.487719	48.802714
1379.045247	160.946760	48.807719
1375.181383	136.120330	48.812724
1371.699965	148.482520	48.817729
1368.673476	146.446045	48.822733
1365.053576	153.848193	48.827738
1361.725121	159.934813	48.832743
1357.892603	166.488078	48.837748
1354.347738	160.324103	48.842753
1350.809395	147.282899	48.847757
1347.157230	153.015436	48.852762
1343.687164	166.222867	48.857767
1340.713654	156.251881	48.862772
1336.952946	143.443799	48.867777
1333.485572	153.916358	48.872781
1330.121711	159.495076	48.877786
1326.592946	145.623665	48.882791
1323.136409	145.451019	48.887796
1319.555005	164.473977	48.892801
1315.622621	141.060193	48.897805
1311.989935	134.459534	48.902810
1308.796091	152.904557	48.907815
1305.793883	157.529842	48.912820
1301.819022	155.970931	48.917825
1298.328461	150.472387	48.922829
1294.827275	150.877408	48.927834
1291.481333	151.565081	48.932839
1288.094815	139.813249	48.937844
1284.304786	144.311697	48.942849
1281.189344	146.558536	48.947853
1277.459070	152.365850	48.952858
1273.499746	143.990193	48.957863
1270.777804	160.856712	48.962868
1266.721816	152.041947	48.967873
1263.277453	147.486073	48.972877
1259.933167	146.963769	48.977882
1256.451312	157.506522	48.982887
1252.901482	166.903263	48.987892
1249.162585	158.922616	48.992897
1246.020354	136.090510	48.997901
1242.157493	151.596779	49.002906
1238.710646	157.235598	49.007911
1235.725389	166.511040	49.012916
1231.695027	150.479230	49.017921
1228.384126	141.366803	49.022925
1224.594140	156.404610	49.027930
1221.190918	155.083634	49.032935
1217.948509	144.219363	49.037940
1214.455857	138.828643	49.042945
1210.938021	147.816838	49.047949
1207.132417	161.187424	49.052954
1203.745637	164.246568	49.057959
1200.455912	144.020149	49.062964
1196.975318	151.033984	49.067969
1193.347800	149.915578	49.072973
1189.471149	151.378086	49.077978
1185.947788	141.102283	49.082983
1182.814557	133.105760	49.087988
1179.331822	145.091797	49.092993
1176.031030	140.954511	49.097997
1172.431500	137.955120	49.103002
1168.862763	148.304392	49.108007
1165.438128	156.603263	49.113012
1161.778538	145.003024	49.118017
1158.274576	137.519419	49.123021
1154.704880	162.614035	49.128026
1151.163148	145.125295	49.133031
1147.647954	138.740809	49.138036
1144.329025	137.173348	49.143041
1140.784933	146.003037	49.148045
1137.181435	167.622166	49.153050
1133.491912	151.296915	49.158055
1130.281344	152.811379	49.163060
1126.538552	153.516996	49.168065
1123.484947	134.249487	49.173069
1119.562543	148.752618	49.178074
1116.156380	156.704476	49.183079
1112.724197	138.034137	49.188084
1109.363628	132.075857	49.193089
1105.985224	138.447923	49.198093
1102.540863	145.681619	49.203098
1098.581428	146.033654	49.208103
1095.090708	149.472338	49.213108
1091.678362	149.582636	49.218113
1088.121942	138.342844	49.223117
1084.883392	133.114945	49.228122
1081.277027	124.794011	49.233127
1077.899639	146.589075	49.238132
1074.107993	157.024317	49.243137
1070.575827	127.890889	49.248141
1066.944034	125.918775	49.253146
1063.731017	147.514470	49.258151
1060.467706	147.297034	49.263156
1056.625380	141.081433	49.268161
1053.419387	146.692799	49.273165
1049.817078	143.886100	49.278170
1046.281106	156.849211	49.283175
1042.776706	140.079352	49.288180
1038.835122	138.466079	49.293185
1035.421445	140.792742	49.298189
1032.144245	142.409598	49.303194
1028.211756	133.962895	49.308199
1025.141587	142.774761	49.313204
1021.729941	148.047305	49.318209
1018.080179	137.952188	49.323213
1014.978529	134.003378	49.328218
1011.462959	147.632351	49.333223
1007.802895	153.790833	49.338228
1003.837561	149.667564	49.343233
1001.066488	130.188161	49.348237
997.267437	124.298889	49.353242
993.432877	137.960007	49.358247
990.093280	123.180238	49.363252
986.665946	135.579897	49.368257
983.224065	148.037212	49.373261
979.860051	150.309240	49.378266
976.159898	142.068263	49.383271
972.756944	129.822856	49.388276
968.721887	143.239893	49.393281
965.564130	152.061314	49.398285
962.054934	138.249266	49.403290
958.481602	121.023971	49.408295
955.274187	135.504896	49.413300
951.675114	152.994046	49.418305
948.323903	138.867674	49.423309
944.538297	130.068184	49.428314
940.759240	136.842563	49.433319
937.410972	137.844194	49.438324
933.905807	134.193475	49.443329
930.660639	134.935512	49.448333
927.403033	150.438842	49.453338
923.432841	140.044126	49.458343
920.021271	138.549586	49.463348
916.567458	134.044201	49.468353
913.267645	141.963384	49.473357
909.645137	146.969031	49.478362
905.992164	151.364546	49.483367
902.708943	135.408415	49.488372
898.729359	160.318430	49.493377
895.542610	150.110040	49.498381
892.267777	132.015239	49.503386
888.627149	137.999705	49.508391
885.233771	139.664617	49.513396
881.436016	142.828266	49.518401
878.151634	155.975604	49.523405
874.762035	153.184780	49.528410
870.910609	144.588265	49.533415
867.588616	130.749915	49.538420
863.674167	156.727692	49.543425
860.170184	152.875179	49.548429
857.332541	144.451609	49.553434
853.733378	151.144838	49.558439
849.707668	141.209271	49.563444
846.348986	134.457307	49.568449
843.177305	131.753042	49.573453
839.737094	148.575773	49.578458
836.294081	161.078520	49.583463
832.642712	133.580710	49.588468
828.624974	133.646983	49.593473
825.181703	130.983924	49.598477
821.964024	143.029611	49.603482
818.362852	138.301798	49.608487
814.947094	143.040838	49.613492
811.068427	147.547652	49.618497
808.050761	137.262079	49.623501
804.445616	132.569359	49.628506
800.926582	143.852161	49.633511
797.748355	146.376813	49.638516
793.803989	142.383391	49.643521
790.486346	140.862557	49.648525
786.839493	144.560077	49.653530
783.542937	134.392289	49.658535
780.137040	139.340229	49.663540
776.504653	141.180204	49.668545
773.094017	127.525539	49.673549
769.334241	143.886910	49.678554
765.816112	137.542395	49.683559
762.787157	128.062890	49.688564
758.650114	148.664772	49.693569
755.317142	121.332482	49.698573
751.777554	138.627786	49.703578
748.016776	144.047284	49.708583
744.945630	139.133043	49.713588
741.355187	134.189439	49.718593
738.021454	139.630950	49.723597
734.755081	135.015697	49.728602
730.679965	123.420065	49.733607
727.658210	122.081829	49.738612
724.151646	150.812404	49.743617
720.305254	134.171367	49.748621
716.862150	131.605605	49.753626
713.097506	128.469003	49.758631
710.043801	126.447099	49.763636
706.240079	133.188673	49.768641
703.188783	134.433863	49.773645
699.419932	126.893073	49.778650
695.527444	131.855808	49.783655
692.539905	135.242067	49.788660
688.848498	133.702022	49.793665
685.367985	120.772772	49.798669
681.854046	137.750561	49.803674
678.150010	142.700237	49.808679
674.994979	123.570040	49.813684
671.193469	145.755956	49.818689
667.973984	145.271047	49.823693
664.281880	128.421489	49.828698
660.495091	119.840103	49.833703
657.368464	128.862758	49.838708
653.678136	135.636928	49.843713
650.063647	128.139827	49.848717
646.658612	132.204596	49.853722
643.210396	124.687243	49.858727
640.162651	129.441046	49.863732
636.528121	131.737000	49.868737
633.036974	118.559572	49.873741
629.547134	126.589165	49.878746
625.616555	149.958185	49.883751
622.439543	126.633720	49.888756
618.246939	114.800311	49.893761
615.367901	136.924636	49.898765
611.983645	133.775776	49.903770
608.439137	120.777835	49.908775
604.868407	114.763310	49.913780
601.118917	127.763412	49.918785
597.463996	129.979003	49.923789
594.473593	136.253668	49.928794
590.822737	120.984988	49.933799
587.383781	116.025045	49.938804
583.491512	134.073226	49.943809
580.270050	135.684541	49.948813
577.003926	123.168698	49.953818
573.390804	127.243404	49.958823
569.999256	119.562355	49.963828
566.116990	131.216567	49.968833
562.562043	121.840923	49.973837
559.163687	125.116636	49.978842
555.585380	130.041068	49.983847
552.320240	126.356054	49.988852
548.664672	127.109139	49.993857
545.219404	116.800837	49.998861
541.596748	136.166029	50.003866
538.084881	126.367584	50.008871
535.116894	105.195892	50.013876
531.008127	127.511103	50.018881
527.817871	147.240814	50.023885
524.014658	135.227530	50.028890
520.557354	116.989721	50.033895
517.465400	131.602743	50.038900
513.670468	124.209224	50.043905
510.308588	124.133524	50.048909
506.754684	124.850703	50.053914
503.111468	128.691591	50.058919
499.768497	130.872380	50.063924
496.236430	120.935842	50.068929
492.815596	118.921910	50.073933
489.004909	126.290852	50.078938
485.288671	127.944084	50.083943
481.991276	129.820623	50.088948
478.319404	140.875871	50.093953
474.978638	126.988500	50.098957
471.635692	117.144938	50.103962
468.103097	138.190921	50.108967
465.105281	136.663989	50.113972
460.905253	121.051674	50.118977
457.546709	127.569597	50.123981
454.282168	141.001843	50.128986
450.835328	127.129840	50.133991
447.355072	147.501133	50.138996
443.469103	138.192072	50.144001
440.130844	130.341499	50.149005
436.531786	122.407252	50.154010
432.715027	126.451645	50.159015
429.816927	125.598393	50.164020
426.024551	141.917043	50.169025
422.623912	119.584087	50.174029
419.356205	131.930365	50.179034
415.672719	138.267800	50.184039
412.397689	126.208687	50.189044
408.822737	132.259381	50.194049
404.944589	132.113846	50.199053
401.544320	115.137350	50.204058
397.856696	122.720023	50.209063
394.688603	142.846413	50.214068
390.914266	124.999813	50.219073
387.636452	114.515169	50.224077
384.314837	123.909405	50.229082
380.314588	150.819207	50.234087
377.043427	132.320000	50.239092
373.343280	117.897110	50.244097
369.921653	129.272525	50.249101
366.588747	114.358778	50.254106
362.951597	136.869927	50.259111
359.704890	129.996764	50.264116
355.824142	140.274215	50.269121
352.426867	116.719686	50.274125
348.989007	108.670288	50.279130
345.147416	135.680947	50.284135
341.879894	139.254672	50.289140
338.639997	123.630011	50.294145
335.356153	102.675775	50.299149
331.760889	120.170398	50.304154
327.985577	133.269714	50.309159
324.562129	122.529498	50.314164
320.829276	105.939491	50.319169
317.473620	107.266210	50.324173
314.033905	131.252242	50.329178
310.351728	134.548825	50.334183
307.390583	123.872644	50.339188
303.607298	133.706974	50.344193
299.796689	122.670009	50.349197
296.511025	118.244336	50.354202
292.902016	120.361059	50.359207
289.647246	123.242764	50.364212
285.944445	138.745364	50.369217
282.437535	124.081405	50.374221
279.158641	109.905085	50.379226
275.409573	119.069974	50.384231
271.698155	112.903208	50.389236
268.085173	123.273671	50.394241
265.057612	110.527251	50.399245
261.575933	125.307229	50.404250
257.757632	142.704297	50.409255
254.596756	111.499734	50.414260
251.279975	120.193599	50.419265
247.613332	129.031686	50.424269
244.071904	105.808187	50.429274
240.238019	124.697083	50.434279
236.889709	125.927338	50.439284
233.171475	119.683888	50.444289
229.619736	127.733556	50.449293
226.292685	122.815903	50.454298
222.572425	108.958765	50.459303
219.599238	121.078689	50.464308
215.903235	134.974521	50.469313
212.695967	122.794647	50.474317
208.969399	113.188745	50.479322
204.970091	129.828331	50.484327
202.257414	124.581705	50.489332
198.705367	118.882477	50.494337
194.852344	122.900734	50.499341
191.485970	129.028937	50.504346
187.860856	115.262341	50.509351
184.303519	115.155676	50.514356
180.650474	122.838664	50.519361
177.205093	112.245731	50.524365
173.830174	119.378585	50.529370
170.224265	119.611110	50.534375
166.918857	111.638092	50.539380
163.405216	100.182054	50.544385
159.766172	97.561781	50.549389
156.331213	111.945401	50.554394
152.741174	135.052029	50.559399
149.377507	106.209329	50.564404
146.036845	102.075356	50.569409
142.626168	110.457468	50.574413
138.988367	127.087954	50.579418
135.033359	125.764323	50.584423
132.021062	118.098315	50.589428
128.087629	116.297819	50.594433
124.689876	119.067491	50.599437
121.340778	121.740244	50.604442
117.959443	125.730028	50.609447
114.815488	113.761422	50.614452
110.783342	109.668924	50.619457
107.088973	116.194549	50.624461
103.826665	127.563254	50.629466
100.027962	121.729942	50.634471
96.790212	105.683716	50.639476
93.043315	109.485128	50.644481
89.772752	120.987285	50.649485
86.558396	113.255357	50.654490
82.733794	106.665976	50.659495
79.503602	107.152729	50.664500
75.541279	105.912618	50.669505
72.134469	121.764516	50.674509
68.597642	115.187073	50.679514
65.408609	116.350355	50.684519
62.194145	107.566201	50.689524
57.897328	122.958103	50.694529
54.426144	126.328568	50.699533
51.170577	107.930428	50.704538
48.010015	119.811180	50.709543
44.158703	122.421950	50.714548
40.587267	127.316207	50.719553
37.404000	102.331848	50.724557
33.544786	111.212109	50.729562
30.069515	123.129486	50.734567
26.852944	109.933150	50.739572
23.369351	101.124149	50.744577
19.283682	120.093897	50.749581
15.900144	112.619025	50.754586
12.284463	100.803220	50.759591
9.310055	114.749946	50.764596
6.047131	127.665663	50.769601
2.471614	121.434588	50.774605