Wed Jun 15 16:39:00 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.761744	86.560233	0.000000
0.709986	97.590500	0.005005
0.626153	68.437017	0.010010
0.423208	79.559632	0.015014
0.432432	71.006050	0.020019
0.347443	63.725583	0.025024
-0.136527	63.125664	0.030029
0.253891	63.661968	0.035034
-0.545230	42.052128	0.040038
-0.246365	34.720570	0.045043
-0.906506	32.792202	0.050048
-1.010325	15.718944	0.055053
-1.351911	10.486079	0.060058
-2.134746	3.172799	0.065062
-2.041395	2.558957	0.070067
-2.295152	-3.854310	0.075072
-2.679420	6.724789	0.080077
-3.130137	-23.486135	0.085082
-4.087270	-14.832146	0.090086
-4.041657	-25.508226	0.095091
-3.812701	-29.438346	0.100096
-4.005942	-11.933264	0.105101
-3.614887	-26.108371	0.110106
-4.530774	-21.183983	0.115110
-4.998218	-11.992213	0.120115
-5.089776	-19.534642	0.125120
-5.369905	-20.471874	0.130125
-5.463073	-30.046426	0.135130
-6.297727	-24.601298	0.140134
-6.621030	-22.072490	0.145139
-6.580599	-20.108362	0.150144
-6.901801	-2.561211	0.155149
-6.537381	-23.332788	0.160154
-6.883156	-10.067237	0.165158
-7.425719	-15.105397	0.170163
-7.895395	-29.662164	0.175168
-8.111057	-21.610623	0.180173
-8.215757	-22.331810	0.185178
-8.555067	-15.024137	0.190182
-8.685593	-22.600274	0.195187
-8.595696	-28.523925	0.200192
-9.380662	-20.741711	0.205197
-9.626155	-14.110762	0.210202
-9.773193	-30.835806	0.215206
-9.850957	-40.753617	0.220211
-10.100354	-26.929596	0.225216
-10.441120	-23.477540	0.230221
-11.016449	-18.130605	0.235226
-11.441006	-17.689566	0.240230
-11.867343	-36.264513	0.245235
-11.462778	-25.270189	0.250240
-11.638292	0.195034	0.255245
-11.449229	-31.443254	0.260250
-11.846703	-30.521750	0.265254
-11.861507	-14.164109	0.270259
-12.421292	-20.866431	0.275264
-12.890576	-17.475405	0.280269
-13.002170	-9.662811	0.285274
-13.777656	-22.279884	0.290278
-14.756274	-11.956418	0.295283
-14.385912	-22.276491	0.300288
-14.021216	-21.137261	0.305293
-14.197886	-8.285753	0.310298
-14.639264	-18.748974	0.315302
-14.971117	-40.604695	0.320307
-14.838589	-11.494353	0.325312
-15.697982	-18.311112	0.330317
-16.003642	-24.924723	0.335322
-16.659757	-14.657120	0.340326
-16.585895	-15.771128	0.345331
-16.634803	-8.093383	0.350336
-16.952085	-10.188296	0.355341
-16.704084	-27.671709	0.360346
-16.941877	-34.609238	0.365350
-16.924783	-19.961369	0.370355
-17.709419	-4.318239	0.375360
-18.400729	-10.646072	0.380365
-18.228375	-29.749861	0.385370
-18.451958	-20.533192	0.390374
-18.449495	-21.716487	0.395379
-18.578268	-10.223058	0.400384
-19.533099	-10.032838	0.405389
-19.652342	-44.270456	0.410394
-19.891734	-20.995984	0.415398
-19.986300	-15.348024	0.420403
-19.776292	-31.154493	0.425408
-20.341699	-7.582370	0.430413
-20.873397	-22.629714	0.435418
-21.427314	-29.235342	0.440422
-21.556835	-17.881280	0.445427
-21.621302	-5.787366	0.450432
-21.779172	-24.922903	0.455437
-21.252254	-15.742267	0.460442
-21.962319	-13.429299	0.465446
-22.833972	-13.429203	0.470451
-22.825028	-10.063446	0.475456
-23.312013	-0.244704	0.480461
-23.076567	-15.644633	0.485466
-23.097177	-27.849818	0.490470
-23.766553	-8.305372	0.495475
-24.376633	-22.400064	0.500480
-24.887494	-10.883937	0.505485
-24.876193	-4.704210	0.510490
-24.868489	-16.384356	0.515494
-24.803585	-16.383275	0.520499
-24.400928	-20.746352	0.525504
-25.277758	-31.403548	0.530509
-26.009491	-18.585106	0.535514
-26.312662	-8.824861	0.540518
-26.595508	-14.850668	0.545523
-26.413125	-19.147849	0.550528
-26.839794	-2.994691	0.555533
-26.252831	-23.828393	0.560538
-27.358599	-26.375203	0.565542
-27.641495	-1.032710	0.570547
-27.938280	-14.034698	0.575552
-28.269401	-23.226739	0.580557
-28.162232	-27.876081	0.585562
-28.470371	-15.691202	0.590566
-28.265188	-6.960189	0.595571
-28.904387	-13.309751	0.600576
-29.593999	-34.912019	0.605581
-29.122276	-27.394705	0.610586
-29.595664	-15.479735	0.615590
-29.913934	-30.727868	0.620595
-30.344082	-15.996122	0.625600
-30.777142	-11.536930	0.630605
-30.761650	-27.352588	0.635610
-30.737597	-29.957774	0.640614
-30.766427	-15.020484	0.645619
-31.605555	-17.293523	0.650624
-32.417820	-25.779549	0.655629
-32.463212	-25.020695	0.660634
-33.172853	-19.446677	0.665638
-33.037907	-38.726172	0.670643
-32.419910	-31.260260	0.675648
-32.510131	-23.882484	0.680653
-32.249726	-26.349761	0.685658
-33.058503	-18.403607	0.690662
-34.162331	-14.562060	0.695667
-34.046716	-23.711625	0.700672
-34.434868	-1.073170	0.705677
-33.950559	-18.712637	0.710682
-34.916095	-13.025894	0.715686
-35.847441	-26.887754	0.720691
-35.677820	-16.651361	0.725696
-36.081136	-6.792097	0.730701
-35.984680	-19.162235	0.735706
-36.009829	-34.386103	0.740710
-36.087481	-14.439323	0.745715
-36.012659	-19.574280	0.750720
-36.400685	-27.133406	0.755725
-36.972866	-38.235029	0.760730
-37.537312	-9.330499	0.765734
-37.735716	-16.195725	0.770739
-37.377105	-15.171892	0.775744
-37.749873	-16.789165	0.780749
-38.399980	-39.124379	0.785754
-38.902010	-38.370851	0.790758
-39.028362	-20.942932	0.795763
-39.015318	-9.105191	0.800768
-39.459786	-15.424785	0.805773
-39.365367	-30.777419	0.810778
-39.346858	-26.581567	0.815782
-39.803595	-6.967501	0.820787
-40.486525	-24.575937	0.825792
-41.083138	-18.115131	0.830797
-41.436116	-37.571257	0.835802
-40.967772	-17.641127	0.840806
-40.851862	1.490339	0.845811
-40.861648	-23.598859	0.850816
-41.942160	-23.718722	0.855821
-42.623260	-14.395170	0.860826
-42.513841	-27.893382	0.865830
-43.005867	-19.929834	0.870835
-42.701513	-8.872580	0.875840
-42.407418	-14.197860	0.880845
-42.369525	-40.009992	0.885850
-43.114678	-26.222122	0.890854
-43.603596	-15.941608	0.895859
-44.059858	-5.969425	0.900864
-45.473865	-13.190808	0.905869
-44.390850	-17.549233	0.910874
-45.034607	-9.556362	0.915878
-45.170458	-21.471328	0.920883
-45.322393	-22.743534	0.925888
-45.841270	-12.076802	0.930893
-45.637473	-25.543362	0.935898
-45.649677	-23.980114	0.940902
-46.530937	-4.767215	0.945907
-46.770833	-33.674914	0.950912
-47.397440	-11.745985	0.955917
-47.387110	-22.934317	0.960922
-47.684541	-34.903359	0.965926
-47.942387	-12.984572	0.970931
-47.427101	-4.822796	0.975936
-47.801926	-13.507089	0.980941
-47.452456	-22.609973	0.985946
-48.401637	-10.619033	0.990950
-48.779882	-22.737889	0.995955
-48.791808	-42.027926	1.000960
-49.028119	-10.592925	1.005965
-49.919656	-12.498922	1.010970
-50.190222	-14.721998	1.015974
-50.418307	-20.969332	1.020979
-50.392518	-28.444437	1.025984
-50.831303	-25.449285	1.030989
-50.462160	-37.552555	1.035994
-50.589486	-14.486985	1.040998
-51.110667	-13.715493	1.046003
-51.419147	-31.281632	1.051008
-52.007796	-25.015292	1.056013
-51.956496	-14.634559	1.061018
-52.047819	-25.685149	1.066022
-52.562678	-24.587002	1.071027
-53.126140	-15.932571	1.076032
-53.441685	-22.148878	1.081037
-53.537782	-40.332310	1.086042
-53.406353	-22.380872	1.091046
-53.808625	-11.485810	1.096051
-53.966534	-12.952545	1.101056
-53.839151	-29.736546	1.106061
-54.555826	-18.476035	1.111066
-54.789244	-35.788723	1.116070
-55.310322	-38.665252	1.121075
-55.562197	-12.687605	1.126080
-55.558528	-16.338223	1.131085
-55.484868	-36.325728	1.136090
-56.352873	-24.668318	1.141094
-56.706841	0.523348	1.146099
-56.725446	-2.899863	1.151104
-56.839347	-13.895533	1.156109
-56.624622	-41.066328	1.161114
-57.023936	-21.550653	1.166118
-57.509219	-2.032385	1.171123
-57.848140	-21.343376	1.176128
-58.351663	-20.793992	1.181133
-58.319867	-35.136202	1.186138
-58.555786	-21.517224	1.191142
-58.707583	-8.294683	1.196147
-59.049906	-28.194806	1.201152
-59.913071	-25.757987	1.206157
-59.854711	-15.542864	1.211162
-60.185375	-23.096771	1.216166
-60.352827	-19.033541	1.221171
-60.189470	-29.354612	1.226176
-60.439557	-14.695340	1.231181
-60.239288	-26.992760	1.236186
-60.974065	-18.911656	1.241190
-61.064955	-22.310093	1.246195
-61.011961	-25.354102	1.251200
-62.083022	-34.808363	1.256205
-62.752999	-37.744822	1.261210
-62.657115	-21.816546	1.266214
-62.741783	-18.040049	1.271219
-63.012145	-24.691449	1.276224
-63.250316	-10.204108	1.281229
-63.318255	-18.046372	1.286234
-63.289282	-28.113419	1.291238
-63.617042	-11.323982	1.296243
-63.496458	-4.726601	1.301248
-64.428723	-3.544277	1.306253
-64.462285	-31.869045	1.311258
-65.093303	-28.378983	1.316262
-64.937375	-24.576651	1.321267
-65.425777	-45.948465	1.326272
-66.224764	-27.375690	1.331277
-66.450257	-6.871000	1.336282
-66.682020	-9.107689	1.341286
-66.173035	-10.322611	1.346291
-66.357003	-38.049774	1.351296
-66.891523	-11.884749	1.356301
-66.627310	-7.113064	1.361306
-66.967307	-26.680642	1.366310
-67.751499	-34.024641	1.371315
-68.156497	-15.437062	1.376320
-68.280756	-1.469560	1.381325
-68.319818	-18.906027	1.386330
-68.395114	-28.686241	1.391334
-68.355205	-16.697682	1.396339
-69.209143	-18.911448	1.401344
-70.026818	-32.330122	1.406349
-70.079787	-25.820667	1.411354
-69.811531	-9.305221	1.416358
-70.070768	-22.898761	1.421363
-69.883157	-11.883479	1.426368
-70.265233	-25.464509	1.431373
-70.851181	-10.103007	1.436378
-71.282092	-6.190072	1.441382
-72.014869	-17.346741	1.446387
-71.656210	-26.084377	1.451392
-71.764593	-19.248912	1.456397
-71.917761	-7.762799	1.461402
-72.238996	-4.027203	1.466406
-72.699226	-14.422786	1.471411
-72.970828	-28.107892	1.476416
-73.623947	-12.468851	1.481421
-73.419412	5.776237	1.486426
-73.384154	-2.960641	1.491430
-73.763154	-18.315930	1.496435
-73.510016	-26.467238	1.501440
-74.487557	-13.740453	1.506445
-74.838001	-18.411826	1.511450
-74.852604	-23.106050	1.516454
-75.344129	-15.441182	1.521459
-75.064890	-23.241583	1.526464
-75.746363	-28.152997	1.531469
-76.503569	-19.184225	1.536474
-76.759992	2.557374	1.541478
-77.127990	-9.347147	1.546483
-76.163578	-34.138127	1.551488
-76.508158	-22.152122	1.556493
-76.513116	-3.473896	1.561498
-77.161373	-7.311920	1.566502
-78.045896	-25.681714	1.571507
-78.525530	-33.465793	1.576512
-79.020160	-9.587743	1.581517
-78.421057	-18.123045	1.586522
-78.115757	-18.811668	1.591526
-78.558994	-13.751128	1.596531
-78.334616	-32.602287	1.601536
-79.138594	-22.336098	1.606541
-79.721956	-11.486178	1.611546
-79.809005	-6.962538	1.616550
-79.887730	-16.646506	1.621555
-80.236325	-40.063268	1.626560
-81.459730	-22.155942	1.631565
-81.592181	-4.699678	1.636570
-80.840123	-12.938184	1.641574
-81.618419	-19.542335	1.646579
-81.307920	-21.733694	1.651584
-81.366096	-33.824444	1.656589
-82.042409	-21.298278	1.661594
-82.336107	-12.652423	1.666598
-82.908873	-19.118109	1.671603
-82.656953	-23.528089	1.676608
-82.954640	-18.413576	1.681613
-82.967157	-13.500079	1.686618
-84.040545	-24.003347	1.691622
-84.364039	-9.468860	1.696627
-84.823056	-19.734130	1.701632
-85.116669	-26.531921	1.706637
-84.540148	-22.270460	1.711642
-84.768593	-22.155298	1.716646
-84.852863	-23.435431	1.721651
-84.486746	-10.316050	1.726656
-85.534107	0.726373	1.731661
-85.903216	-19.677548	1.736666
-86.233441	-25.263348	1.741670
-86.355333	-15.501406	1.746675
-86.345109	-8.337025	1.751680
-87.382834	-20.175634	1.756685
-87.625953	-17.609667	1.761690
-87.816474	-30.262527	1.766694
-88.234965	-19.886430	1.771699
-87.796114	-30.163163	1.776704
-88.336848	-18.101925	1.781709
-88.340016	-28.310835	1.786714
-87.925337	-40.267147	1.791718
-88.787612	-21.718137	1.796723
-89.227667	-9.944707	1.801728
-89.610589	-23.132691	1.806733
-89.602733	-15.890683	1.811738
-89.777957	-13.414853	1.816742
-89.936063	-16.766964	1.821747
-89.923717	-23.669972	1.826752
-90.889586	-25.292104	1.831757
-91.315824	-6.995070	1.836762
-91.330032	-4.626048	1.841766
-91.620845	-14.691150	1.846771
-91.146803	-38.403279	1.851776
-91.790385	-33.917388	1.856781
-92.654998	-22.010766	1.861786
-92.808560	-18.517636	1.866790
-92.898366	-25.128243	1.871795
-92.909612	-34.905028	1.876800
-93.008236	-18.260404	1.881805
-92.930833	-34.682884	1.886810
-93.243645	-17.796593	1.891814
-93.762044	-20.400020	1.896819
-94.228449	-29.008100	1.901824
-94.513610	-20.498411	1.906829
-94.419277	-9.272298	1.911834
-95.356437	-35.203428	1.916838
-95.779863	-39.982682	1.921843
-95.356278	-28.754377	1.926848
-96.035937	-8.520780	1.931853
-95.939966	-24.672203	1.936858
-96.034911	-32.430486	1.941862
-96.193748	-27.324029	1.946867
-96.226559	-8.895025	1.951872
-97.133592	2.845405	1.956877
-97.376383	-27.620310	1.961882
-97.900828	-47.854200	1.966886
-97.799226	-21.472253	1.971891
-97.875869	-20.253873	1.976896
-97.897844	-20.158827	1.981901
-98.067499	-18.766452	1.986906
-98.945067	-21.972528	1.991910
-99.262140	-18.399992	1.996915
-99.351384	-24.704090	2.006912
-98.652740	-29.949225	2.016909
-98.025435	-27.446969	2.026906
-98.206611	-24.275949	2.036902
-97.724819	-32.352683	2.046899
-96.738016	-15.275334	2.056896
-96.800208	-32.273995	2.066893
-95.569479	-25.242041	2.076890
-95.404384	-30.282444	2.086886
-95.414127	-14.896806	2.096883
-94.433234	-17.926620	2.106880
-94.095555	-22.076378	2.116877
-93.034909	-14.899857	2.126874
-92.471467	-35.130807	2.136870
-92.235358	-18.649535	2.146867
-92.201038	-27.201390	2.156864
-91.776270	-25.873242	2.166861
-91.151925	-21.085215	2.176858
-90.103503	-20.288314	2.186854
-89.538498	-12.831246	2.196851
-89.343982	-26.645072	2.206848
-89.121665	-30.807073	2.216845
-88.349068	-32.981764	2.226842
-87.691852	-29.400037	2.236838
-87.556928	-24.190164	2.246835
-86.976643	-19.416979	2.256832
-86.308246	-35.005126	2.266829
-85.923499	-24.472944	2.276826
-85.383813	-25.294195	2.286822
-84.716031	-14.052389	2.296819
-84.537935	-27.908344	2.306816
-84.048600	-18.272115	2.316813
-83.364584	-29.702978	2.326810
-83.241294	-11.014765	2.336806
-82.105121	-17.493769	2.346803
-81.816541	-28.714183	2.356800
-81.641843	-22.075038	2.366797
-80.780263	-30.538413	2.376794
-80.514764	-19.888537	2.386790
-79.987517	-14.301100	2.396787
-78.881971	-28.357152	2.406784
-78.491859	-20.812906	2.416781
-78.487111	-13.641044	2.426778
-78.372254	-26.277385	2.436774
-77.197050	-14.176861	2.446771
-77.087890	-31.283852	2.456768
-76.340358	-11.379907	2.466765
-75.420821	-30.587573	2.476762
-75.590329	-24.035945	2.486758
-75.107581	-14.287210	2.496755
-74.222006	-32.847243	2.506752
-73.715469	-27.494328	2.516749
-73.436863	-20.703751	2.526746
-72.444748	-33.510751	2.536742
-71.894273	-20.887894	2.546739
-72.124273	-24.328880	2.556736
-71.700251	-29.146084	2.566733
-70.840365	-30.170977	2.576730
-70.636380	-23.141388	2.586726
-69.571477	-25.068269	2.596723
-69.049770	-21.261957	2.606720
-69.005817	-22.988501	2.616717
-68.476276	-29.131573	2.626714
-67.655797	-22.525469	2.636710
-67.676994	-26.224978	2.646707
-66.531651	-30.776775	2.656704
-65.858396	-24.517623	2.666701
-65.828897	-26.397147	2.676698
-65.832346	-20.867198	2.686694
-64.696153	-19.527725	2.696691
-64.236248	-17.952724	2.706688
-63.917142	-29.670857	2.716685
-63.407365	-25.982285	2.726682
-62.873287	-14.681042	2.736678
-62.504479	-24.986264	2.746675
-61.575188	-24.018747	2.756672
-61.318298	-27.447256	2.766669
-61.019014	-15.516752	2.776666
-60.007561	-24.270002	2.786662
-59.495420	-33.094812	2.796659
-59.407765	-16.644704	2.806656
-59.187309	-33.910443	2.816653
-58.391933	-18.289147	2.826650
-57.990771	-29.013765	2.836646
-57.065010	-23.938440	2.846643
-56.381809	-31.411877	2.856640
-56.669583	-20.869784	2.866637
-55.977297	-11.420479	2.876634
-55.250449	-23.324826	2.886630
-54.920156	-29.591522	2.896627
-53.841802	-7.953285	2.906624
-53.543279	-28.094835	2.916621
-53.432912	-9.289507	2.926618
-53.287262	-26.042712	2.936614
-52.448016	-18.030826	2.946611
-51.805436	-9.002072	2.956608
-51.061204	-21.965658	2.966605
-50.104005	-24.186263	2.976602
-50.280198	-6.585505	2.986598
-50.321407	-24.081709	2.996595
-49.387797	-16.449389	3.006592
-48.678389	-24.263578	3.016589
-48.526846	-22.448960	3.026586
-47.528218	-21.566978	3.036582
-47.109247	-27.268836	3.046579
-47.097058	-19.220025	3.056576
-45.937534	-24.267727	3.066573
-45.355979	-24.397183	3.076570
-45.269545	-18.231477	3.086566
-45.375232	-25.628274	3.096563
-44.303237	-25.590766	3.106560
-43.655809	-22.900606	3.116557
-43.296988	-25.684486	3.126554
-42.398427	-26.906299	3.136550
-41.863214	-14.026274	3.146547
-42.032335	-19.939112	3.156544
-41.760807	-18.009993	3.166541
-40.738279	-9.163148	3.176538
-40.468016	-25.133836	3.186534
-39.308397	-20.346553	3.196531
-38.749217	-27.459227	3.206528
-38.850846	-18.632643	3.216525
-38.729623	-28.088402	3.226522
-37.714014	-16.402013	3.236518
-37.319668	-18.006010	3.246515
-36.817937	-17.989326	3.256512
-35.805632	-10.231133	3.266509
-35.452474	-34.779028	3.276506
-35.562058	-16.140330	3.286502
-34.973125	-11.728390	3.296499
-33.779543	-20.938236	3.306496
-33.554106	-13.732616	3.316493
-33.700574	-25.848708	3.326490
-32.857810	-21.738291	3.336486
-32.211328	-30.657012	3.346483
-32.013981	-44.189600	3.356480
-31.114595	-17.157009	3.366477
-30.827657	-25.441561	3.376474
-30.278773	-24.905821	3.386470
-29.547847	-25.559944	3.396467
-29.045142	-22.187847	3.406464
-29.064580	-38.471164	3.416461
-28.124279	-25.771580	3.426458
-27.657683	-21.073530	3.436454
-27.618091	-29.604432	3.446451
-26.371320	-22.451150	3.456448
-26.026816	-17.554540	3.466445
-26.155550	-17.544881	3.476442
-25.299435	-21.778144	3.486438
-24.631914	-14.252964	3.496435
-24.250721	-33.606838	3.506432
-23.345483	-11.862351	3.516429
-22.884686	-29.371487	3.526426
-22.887771	-12.563634	3.536422
-22.635285	-20.103287	3.546419
-21.491785	-24.596500	3.556416
-21.156882	-24.001494	3.566413
-20.808149	-29.332116	3.576410
-19.901978	-32.312036	3.586406
-19.717378	-22.034289	3.596403
-19.376093	-17.353950	3.606400
-18.591490	-28.285157	3.616397
-17.888929	-25.211883	3.626394
-17.834850	-23.716191	3.636390
-17.506184	-25.170261	3.646387
-16.198087	-17.779488	3.656384
-16.075563	-34.619837	3.666381
-16.170613	-23.948891	3.676378
-15.055596	-41.814541	3.686374
-14.649943	-26.896587	3.696371
-14.493327	-27.285515	3.706368
-13.366357	-28.073040	3.716365
-12.972338	-20.461870	3.726362
-12.843332	-31.452842	3.736358
-12.607555	-20.047972	3.746355
-11.586339	-34.522108	3.756352
-11.256891	-26.591608	3.766349
-10.279092	-24.831060	3.776346
-9.874778	-36.324345	3.786342
-9.854928	-20.052964	3.796339
-9.546166	-41.527442	3.806336
-8.406729	-18.628105	3.816333
-7.995335	-27.731597	3.826330
-8.058735	-29.531172	3.836326
-7.228503	-22.545607	3.846323
-6.763699	-22.719769	3.856320
-6.415162	-24.832078	3.866317
-5.514853	-25.847742	3.876314
-5.139151	-20.831439	3.886310
-4.627633	-16.953108	3.896307
-4.237562	-10.042856	3.906304
-4.277289	-10.300763	3.916301
-3.229976	11.541579	3.926298
-2.907499	16.310475	3.936294
-2.440223	9.210504	3.946291
-2.141726	19.297694	3.956288
-1.738653	55.440118	3.966285
-1.000949	58.134047	3.976282
-0.858119	80.571523	3.986278
-0.248911	107.528738	3.996275
0.000000	96.813990	4.001280
0.136134	114.092055	4.006285
0.477124	144.809824	4.011290
0.761612	165.331198	4.016294
0.827919	169.607397	4.021299
0.952082	165.743966	4.026304
0.874417	153.114510	4.031309
1.238141	155.775836	4.036314
1.028017	165.958512	4.041318
1.023261	165.174336	4.046323
1.089907	162.231316	4.051328
0.827444	166.128293	4.056333
0.828461	166.816649	4.061338
1.023764	180.033517	4.066342
1.076830	162.857002	4.071347
1.262779	165.657601	4.076352
1.321189	182.219515	4.081357
1.497293	174.387224	4.086362
1.228472	158.536057	4.091366
1.054195	160.073135	4.096371
1.412819	165.672807	4.101376
1.017357	175.955392	4.106381
1.215719	175.915183	4.111386
1.335655	182.927469	4.116390
1.218451	181.662821	4.121395
1.564459	173.802749	4.126400
1.437582	172.183585	4.131405
1.147440	173.947365	4.136410
1.476736	185.659508	4.141414
1.116169	174.686997	4.146419
1.624310	185.919065	4.151424
1.115163	187.056230	4.156429
1.206419	186.425267	4.161434
1.074269	216.748852	4.166438
0.966411	211.542004	4.171443
1.724791	177.033272	4.176448
1.540102	188.598043	4.181453
1.684335	200.313652	4.186458
1.476371	199.877937	4.191462
1.664415	190.562087	4.196467
1.504222	195.030698	4.201472
1.424924	207.868664	4.206477
1.756755	187.318421	4.211482
1.883573	199.233115	4.216486
1.614924	206.113912	4.221491
1.670959	202.003868	4.226496
1.254123	207.943599	4.231501
1.454678	195.958856	4.236506
1.823807	196.501149	4.241510
1.566860	200.662288	4.246515
1.754758	199.871330	4.251520
1.298329	186.600100	4.256525
1.174455	196.398321	4.261530
1.311875	206.620658	4.266534
1.809410	200.071015	4.271539
1.753201	206.666734	4.276544
1.923084	196.765353	4.281549
1.717863	199.518341	4.286554
1.895871	197.744620	4.291558
1.782160	206.833968	4.296563
1.547869	213.074396	4.301568
1.667672	213.581836	4.306573
2.156838	189.057046	4.311578
1.890478	193.107478	4.316582
1.409137	193.309118	4.321587
1.991327	194.542046	4.326592
1.506841	200.786428	4.331597
1.675438	208.162188	4.336602
1.798497	201.182476	4.341606
1.446678	205.376854	4.346611
1.664938	192.434087	4.351616
1.474896	225.841292	4.356621
1.943361	224.696089	4.361626
2.295157	233.298252	4.366630
1.842403	241.921412	4.371635
2.228166	229.717718	4.376640
1.522156	235.957981	4.381645
1.582142	235.760905	4.386650
1.943030	230.906097	4.391654
1.767701	248.407037	4.396659
1.931995	221.105595	4.401664
1.877062	226.406960	4.406669
1.675419	230.126006	4.411674
1.597808	224.119947	4.416678
2.242173	234.302524	4.421683
2.163282	232.151114	4.426688
1.831836	225.596699	4.431693
2.378792	226.244161	4.436698
2.411276	229.394682	4.441702
1.921942	251.286609	4.446707
2.368960	233.137382	4.451712
2.193076	228.484330	4.456717
2.042622	240.552501	4.461722
2.300074	244.874572	4.466726
2.182171	246.902780	4.471731
2.051642	241.874964	4.476736
2.052378	252.569752	4.481741
2.035027	253.622690	4.486746
2.278202	243.809195	4.491750
2.450241	255.551522	4.496755
2.402399	242.443556	4.501760
2.116869	230.828940	4.506765
2.270956	232.724599	4.511770
2.168842	238.934711	4.516774
1.890549	231.365900	4.521779
2.280267	240.313773	4.526784
2.245852	251.572415	4.531789
2.394476	265.578432	4.536794
2.623066	265.091189	4.541798
2.440274	252.062238	4.546803
2.484826	244.273749	4.551808
2.148684	253.773855	4.556813
2.301093	255.019018	4.561818
2.601235	258.214490	4.566822
2.122576	256.585187	4.571827
2.110009	252.945078	4.576832
2.128911	271.245247	4.581837
1.911578	279.255297	4.586842
2.309553	287.190894	4.591846
2.120424	274.502713	4.596851
2.428485	268.892797	4.601856
2.564309	274.508217	4.606861
2.379574	261.549225	4.611866
2.196769	268.980225	4.616870
2.498267	306.846820	4.621875
2.718468	303.741079	4.626880
2.799617	283.295662	4.631885
2.656541	287.376352	4.636890
2.425307	276.527900	4.641894
2.430142	286.120733	4.646899
2.821250	302.866006	4.651904
2.689683	305.476627	4.656909
2.533064	280.896036	4.661914
2.771241	282.170531	4.666918
2.684638	312.143386	4.671923
3.052728	291.588589	4.676928
2.893235	285.414428	4.681933
2.348187	286.968992	4.686938
2.764439	273.919452	4.691942
2.622461	283.043111	4.696947
2.487223	293.133690	4.701952
2.540663	322.975404	4.706957
2.657249	303.766868	4.711962
3.098200	301.839492	4.716966
2.645662	318.754880	4.721971
2.762748	316.993284	4.726976
2.754735	313.158762	4.731981
2.884107	292.782112	4.736986
2.999379	301.115719	4.741990
2.724100	315.484126	4.746995
2.910122	306.359818	4.752000
2.964940	305.052625	4.757005
2.749202	307.769589	4.762010
2.808956	307.286175	4.767014
2.615659	306.660997	4.772019
2.859676	310.264291	4.777024
2.927175	322.636351	4.782029
2.374504	303.166513	4.787034
2.843440	287.897759	4.792038
2.699920	307.981331	4.797043
3.158374	333.506198	4.802048
2.908964	334.228252	4.807053
3.217258	317.089315	4.812058
3.207497	301.850924	4.817062
2.979023	322.907902	4.822067
3.105987	318.635273	4.827072
2.906113	314.241557	4.832077
3.308670	310.767910	4.837082
3.123334	312.131533	4.842086
2.738366	334.930760	4.847091
3.083363	340.425321	4.852096
3.251357	327.958239	4.857101
3.266241	335.099723	4.862106
3.582118	344.476055	4.867110
3.387467	335.682369	4.872115
3.347114	311.227725	4.877120
3.253533	320.795314	4.882125
2.794655	320.488856	4.887130
3.083297	316.838809	4.892134
3.076400	321.851814	4.897139
3.390904	337.140525	4.902144
3.335647	343.571995	4.907149
3.274280	327.961917	4.912154
3.579469	327.025498	4.917158
3.252018	335.171757	4.922163
3.493354	320.163330	4.927168
3.008789	309.275335	4.932173
3.242016	315.496352	4.937178
3.664394	332.130147	4.942182
3.064462	344.982056	4.947187
3.439802	339.632672	4.952192
3.567765	345.981977	4.957197
3.384682	327.325446	4.962202
3.590338	338.594395	4.967206
3.221132	342.939063	4.972211
3.468495	341.473581	4.977216
3.796851	338.969172	4.982221
3.419493	339.378448	4.987226
3.472664	317.572126	4.992230
3.319160	309.029520	4.997235
3.389700	331.165821	5.002240
3.277698	357.464683	5.007245
3.170706	352.860186	5.012250
3.252776	346.989473	5.017254
3.346604	339.269343	5.022259
3.273847	348.581758	5.027264
3.289196	352.785440	5.032269
3.147729	332.071235	5.037274
3.538154	322.389318	5.042278
3.755828	365.269674	5.047283
3.461105	368.218600	5.052288
3.622241	361.670717	5.057293
3.678218	373.936604	5.062298
3.721910	365.215478	5.067302
3.895930	366.612450	5.072307
3.838115	359.354183	5.077312
3.810309	350.699433	5.082317
3.637948	356.035342	5.087322
3.685400	335.869468	5.092326
3.538287	346.384751	5.097331
3.651256	374.814054	5.102336
3.885033	385.631417	5.107341
3.823032	370.343092	5.112346
3.938733	369.084331	5.117350
3.767549	383.495873	5.122355
3.975059	362.255772	5.127360
3.768400	360.157421	5.132365
3.513060	380.401619	5.137370
3.958024	366.649123	5.142374
3.591956	376.137875	5.147379
3.811739	382.609142	5.152384
3.926314	399.983921	5.157389
3.672005	403.335763	5.162394
3.934898	386.005180	5.167398
3.553240	383.028873	5.172403
4.082990	387.719222	5.177408
4.159934	391.850686	5.182413
3.877619	391.647040	5.187418
4.282916	384.662628	5.192422
4.049273	369.157824	5.197427
4.201396	373.711897	5.202432
4.242179	381.215797	5.207437
4.215710	388.417903	5.212442
4.199506	373.042201	5.217446
4.183309	379.372727	5.222451
4.338200	385.802435	5.227456
3.938187	361.453808	5.232461
4.012975	372.044798	5.237466
4.100553	377.308854	5.242470
3.888011	388.594173	5.247475
3.836990	379.664069	5.252480
4.190137	381.116377	5.257485
4.227861	372.495670	5.262490
4.191110	384.738318	5.267494
4.204681	378.541635	5.272499
3.783388	367.592535	5.277504
4.104845	382.568218	5.282509
3.980899	393.111074	5.287514
4.301868	375.932392	5.292518
3.919366	377.107041	5.297523
4.120596	381.669870	5.302528
4.062476	387.966191	5.307533
3.933342	378.586731	5.312538
4.093561	396.423923	5.317542
3.992623	406.918002	5.322547
4.232259	416.841948	5.327552
4.411934	405.200434	5.332557
4.033690	402.798580	5.337562
4.467524	415.172323	5.342566
4.390807	401.742664	5.347571
4.553471	395.116977	5.352576
4.576055	413.587172	5.357581
4.425184	418.618674	5.362586
4.573120	400.456033	5.367590
4.274427	396.962907	5.372595
4.290202	397.645283	5.377600
4.329919	406.762468	5.382605
4.428560	393.668145	5.387610
4.452980	387.960046	5.392614
4.177552	392.969014	5.397619
4.401808	403.842516	5.402624
4.346842	405.360592	5.407629
4.296528	406.535491	5.412634
4.416154	395.818575	5.417638
4.363580	397.224979	5.422643
4.278192	414.178150	5.427648
4.151540	416.684889	5.432653
4.492477	420.031590	5.437658
4.896652	427.523798	5.442662
4.674288	441.874010	5.447667
4.619071	447.925228	5.452672
4.891962	440.997888	5.457677
4.077592	432.558506	5.462682
4.510340	435.721151	5.467686
4.595038	457.165743	5.472691
4.867725	438.731183	5.477696
4.603025	422.693921	5.482701
4.501403	433.585093	5.487706
4.512210	440.837590	5.492710
4.902221	455.099834	5.497715
4.634994	436.185595	5.502720
5.087888	437.887775	5.507725
4.879057	442.911305	5.512730
4.839890	436.458640	5.517734
4.974275	443.619195	5.522739
4.876774	458.805157	5.527744
4.874756	452.593954	5.532749
4.909241	438.022871	5.537754
4.755533	437.450630	5.542758
4.823525	450.356202	5.547763
5.069925	440.132657	5.552768
5.039566	430.236300	5.557773
4.904320	437.780761	5.562778
5.173965	447.268575	5.567782
4.837170	450.725703	5.572787
4.907430	445.502559	5.577792
4.919314	447.609474	5.582797
4.880865	438.792380	5.587802
4.909668	440.814028	5.592806
5.104210	430.281905	5.597811
4.904516	422.098846	5.602816
4.782154	444.294614	5.607821
4.783477	457.292890	5.612826
5.236830	436.263910	5.617830
5.102940	425.785079	5.622835
4.999335	430.098604	5.627840
4.904977	444.674681	5.632845
5.104560	436.403337	5.637850
5.226669	422.563768	5.642854
5.150710	438.642370	5.647859
5.330419	453.778076	5.652864
5.285489	443.603167	5.657869
4.963711	437.080208	5.662874
4.969133	441.314360	5.667878
4.934855	448.532582	5.672883
4.967803	446.189828	5.677888
5.243981	438.435074	5.682893
4.895469	446.549951	5.687898
5.531833	445.241740	5.692902
5.079601	435.176268	5.697907
5.212012	445.009735	5.702912
5.460372	461.838455	5.707917
4.921393	455.143332	5.712922
5.484126	449.785828	5.717926
5.338982	466.577678	5.722931
5.619154	474.489830	5.727936
5.183549	460.629242	5.732941
4.976179	448.747918	5.737946
5.479777	468.477645	5.742950
5.338017	463.216138	5.747955
5.452912	459.667375	5.752960
5.518615	478.276325	5.757965
5.477822	474.607089	5.762970
5.473960	461.289240	5.767974
5.461274	463.577982	5.772979
5.429898	465.759622	5.777984
5.355695	475.665134	5.782989
5.221102	487.649592	5.787994
5.333180	465.693540	5.792998
5.245435	463.861308	5.798003
5.283766	479.869374	5.803008
5.027540	493.788019	5.808013
5.428829	474.039273	5.813018
5.605594	458.186493	5.818022
5.519295	468.853691	5.823027
5.580690	478.341018	5.828032
5.446414	483.137382	5.833037
5.065275	474.258127	5.838042
5.365064	459.153587	5.843046
5.512000	496.161019	5.848051
5.668674	508.832788	5.853056
5.611484	516.594438	5.858061
5.442720	516.797696	5.863066
5.667409	501.786910	5.868070
5.574818	521.987630	5.873075
5.583887	512.711519	5.878080
5.528620	493.925543	5.883085
5.470222	504.795812	5.888090
5.989514	515.759041	5.893094
5.541056	519.775036	5.898099
5.374157	509.807179	5.903104
5.804588	495.725607	5.908109
5.966634	501.854487	5.913114
5.904061	524.798115	5.918118
5.831846	523.387994	5.923123
5.660951	499.993395	5.928128
5.497372	489.786272	5.933133
5.853117	507.106718	5.938138
5.865101	504.591528	5.943142
5.817602	507.251031	5.948147
5.826878	499.257231	5.953152
5.691652	497.508900	5.958157
5.653782	521.667149	5.963162
6.053424	518.147868	5.968166
5.982311	537.422986	5.973171
5.973750	534.738353	5.978176
6.041889	522.190643	5.983181
5.665513	530.685726	5.988186
6.271148	527.715714	5.993190
6.048092	551.415510	5.998195
6.011032	540.174219	6.003200
6.301308	535.972402	6.008205
5.974717	527.477020	6.013210
6.210660	531.504116	6.018214
5.793632	519.834951	6.023219
5.953881	491.959854	6.028224
5.975051	513.530541	6.033229
5.970630	523.416758	6.038234
6.354897	519.879400	6.043238
6.318294	530.301572	6.048243
6.251366	520.880473	6.053248
6.291714	494.870217	6.058253
6.209570	502.436713	6.063258
6.284033	512.562428	6.068262
6.058250	506.221860	6.073267
6.074548	515.693381	6.078272
6.373710	509.206280	6.083277
6.020646	506.330087	6.088282
6.373455	492.014231	6.093286
6.342275	510.505561	6.098291
5.951595	490.532337	6.103296
5.975544	496.713829	6.108301
6.076270	512.078588	6.113306
6.340693	490.839163	6.118310
5.971552	501.464342	6.123315
5.794698	476.240334	6.128320
5.821297	479.047102	6.133325
5.884419	510.508282	6.138330
6.019368	502.444092	6.143334
6.199946	508.280674	6.148339
6.184880	499.163537	6.153344
5.823897	495.192863	6.158349
6.181358	513.110253	6.163354
6.109732	483.659888	6.168358
5.919088	491.784707	6.173363
6.121687	484.056098	6.178368
6.003687	470.578352	6.183373
5.794166	482.074941	6.188378
5.998838	506.974087	6.193382
5.853052	499.189005	6.198387
5.818058	507.492609	6.203392
6.101470	517.842258	6.208397
5.857585	517.531046	6.213402
6.484470	510.789824	6.218406
6.186676	501.777809	6.223411
5.987086	482.257778	6.228416
5.949379	483.173619	6.233421
5.845572	503.761392	6.238426
6.055766	496.342463	6.243430
6.208991	496.356867	6.248435
6.071472	488.820203	6.253440
6.269303	474.902472	6.258445
5.754195	460.139168	6.263450
5.963191	465.393054	6.268454
6.049039	482.542133	6.273459
5.994425	479.693373	6.278464
6.127885	456.958914	6.283469
5.912293	465.197933	6.288474
6.110442	480.499802	6.293478
5.767800	482.912917	6.298483
5.910004	485.891072	6.303488
6.517115	496.655696	6.308493
6.095390	494.656200	6.313498
6.128490	480.266720	6.318502
6.113788	468.043389	6.323507
6.065796	449.733133	6.328512
6.397925	461.000706	6.333517
6.020573	472.250188	6.338522
6.246197	456.782154	6.343526
5.970099	465.357897	6.348531
5.902464	447.426543	6.353536
6.136443	471.994756	6.358541
5.899369	489.467899	6.363546
6.161339	470.667408	6.368550
6.110579	466.451433	6.373555
5.723292	469.120913	6.378560
5.886488	464.247010	6.383565
5.993185	475.355340	6.388570
6.172033	459.540786	6.393574
5.810975	483.788686	6.398579
5.877913	472.421153	6.403584
5.766625	461.549985	6.408589
5.721347	464.356198	6.413594
5.983825	464.904585	6.418598
5.758902	476.743560	6.423603
6.288100	502.400751	6.428608
6.240341	485.972831	6.433613
5.790837	469.215639	6.438618
5.508040	471.974393	6.443622
5.944876	498.967253	6.448627
5.994299	520.206358	6.453632
6.565419	502.467401	6.458637
5.981641	487.634822	6.463642
6.290133	473.077713	6.468646
6.163637	481.096039	6.473651
5.958305	477.621992	6.478656
6.033000	472.386959	6.483661
5.859238	468.026370	6.488666
6.307898	458.263915	6.493670
5.569091	485.428443	6.498675
5.933094	478.100905	6.503680
5.948945	467.171532	6.508685
5.936079	478.036527	6.513690
6.043629	488.172147	6.518694
5.986265	512.483943	6.523699
5.898749	504.236628	6.528704
5.981309	486.765957	6.533709
5.862182	501.503921	6.538714
6.231735	511.636903	6.543718
6.223432	489.719452	6.548723
5.931791	494.698776	6.553728
6.347425	508.468328	6.558733
5.908230	485.671904	6.563738
6.274617	479.205570	6.568742
5.868630	480.189375	6.573747
5.866540	464.506621	6.578752
6.018830	473.920227	6.583757
6.071432	487.469689	6.588762
6.015820	464.735389	6.593766
6.173725	469.793518	6.598771
5.935639	468.361488	6.603776
6.072369	448.017745	6.608781
5.888118	466.895372	6.613786
5.718031	472.935495	6.618790
5.785097	478.621247	6.623795
5.785212	478.440079	6.628800
5.983310	480.085426	6.633805
5.880939	503.288534	6.638810
6.103839	505.999533	6.643814
6.134154	497.426050	6.648819
6.322816	488.459035	6.653824
6.184084	498.089538	6.658829
5.907354	500.597613	6.663834
6.177913	478.044866	6.668838
6.274820	494.085982	6.673843
6.044850	476.204999	6.678848
5.780868	462.591179	6.683853
6.175077	485.826926	6.688858
5.906234	470.956129	6.693862
6.061859	478.191321	6.698867
5.922510	484.286051	6.703872
6.172699	468.324747	6.708877
5.874843	479.528246	6.713882
5.748509	485.065434	6.718886
6.609517	483.518754	6.723891
6.279951	463.562693	6.728896
6.063070	462.576504	6.733901
5.807773	482.751579	6.738906
5.775288	473.839764	6.743910
5.874872	456.122948	6.748915
5.882849	475.646733	6.753920
6.324578	485.008865	6.758925
6.055829	470.632382	6.763930
5.932747	473.158468	6.768934
5.930475	470.846291	6.773939
5.980358	481.487738	6.778944
6.138818	476.764264	6.783949
5.846601	475.909495	6.788954
6.189962	471.755053	6.793958
5.937983	471.892156	6.798963
6.002610	474.885102	6.803968
5.959334	457.412275	6.808973
6.149745	464.637963	6.813978
6.342560	467.262875	6.818982
5.978466	460.659989	6.823987
5.771588	456.975095	6.828992
5.951340	460.230062	6.833997
5.752839	473.871122	6.839002
6.023670	481.245608	6.844006
6.093580	493.161551	6.849011
6.009725	487.350463	6.854016
5.974053	482.309753	6.859021
5.867576	502.152575	6.864026
6.246491	497.462605	6.869030
6.063195	508.825058	6.874035
6.180841	488.015143	6.879040
5.872457	469.499496	6.884045
5.676331	489.124009	6.889050
6.292372	494.660054	6.894054
5.975000	491.999432	6.899059
5.942182	496.365498	6.904064
5.788032	506.043735	6.909069
5.936223	494.204337	6.914074
5.997401	486.134886	6.919078
6.119552	482.770378	6.924083
6.122557	489.707820	6.929088
6.393199	511.103312	6.934093
5.863635	489.499488	6.939098
6.053062	473.943603	6.944102
6.129896	484.629529	6.949107
5.863514	489.023734	6.954112
6.232199	471.410207	6.959117
6.002528	472.877354	6.964122
5.977659	467.116011	6.969126
5.948470	463.749487	6.974131
5.872338	451.987244	6.979136
6.034883	476.841216	6.984141
5.966896	512.459323	6.989146
6.271921	499.323701	6.994150
5.987196	472.426586	6.999155
5.517896	485.664838	7.004160
5.770774	487.666134	7.009165
6.026950	498.721960	7.014170
6.190320	481.766600	7.019174
6.529082	479.791475	7.024179
5.932094	483.697647	7.029184
6.373088	492.575540	7.034189
5.898460	481.310322	7.039194
6.057847	463.044993	7.044198
5.932598	470.770812	7.049203
5.979019	474.841248	7.054208
5.876387	468.098968	7.059213
5.846878	490.447458	7.064218
6.141764	490.757087	7.069222
6.165608	499.015549	7.074227
5.561612	500.127668	7.079232
6.281230	498.510734	7.084237
6.241561	502.398797	7.089242
6.375519	495.198051	7.094246
5.999024	482.793794	7.099251
5.777475	477.383585	7.104256
5.861290	465.995807	7.109261
5.952244	484.350023	7.114266
5.946862	479.084125	7.119270
5.930981	466.412928	7.124275
5.902462	504.186970	7.129280
6.349110	501.624317	7.134285
6.034868	489.110822	7.139290
6.147009	459.076124	7.144294
6.241900	462.203456	7.149299
5.627472	478.482065	7.154304
6.011539	477.164445	7.159309
5.870253	475.334549	7.164314
6.095578	481.716947	7.169318
6.060556	493.255833	7.174323
6.175834	481.143202	7.179328
6.145981	476.228098	7.184333
5.926267	466.121518	7.189338
6.178483	467.528364	7.194342
6.131125	475.082982	7.199347
5.770041	466.156913	7.204352
6.202256	447.776476	7.209357
6.084308	452.104118	7.214362
6.064348	477.230729	7.219366
5.919180	481.282813	7.224371
5.628180	466.450407	7.229376
5.920866	463.705251	7.234381
6.059348	478.071627	7.239386
5.972591	497.418236	7.244390
6.358539	501.234878	7.249395
6.124514	478.957782	7.254400
6.375247	464.408943	7.259405
6.069366	476.911490	7.264410
6.072064	483.036904	7.269414
6.348174	470.277793	7.274419
6.187941	461.067967	7.279424
6.144086	466.508949	7.284429
5.915939	469.817910	7.289434
5.826242	476.052503	7.294438
6.033559	464.049762	7.299443
5.928617	456.336870	7.304448
6.214152	459.636998	7.309453
5.928865	473.832896	7.314458
5.838815	466.230294	7.319462
6.010217	471.598811	7.324467
5.708416	472.810934	7.329472
5.818992	472.612597	7.334477
5.732865	485.893871	7.339482
6.100144	466.896440	7.344486
5.918473	455.678024	7.349491
5.766060	471.985533	7.354496
5.947161	475.112531	7.359501
6.135000	481.763925	7.364506
5.933543	465.711925	7.369510
6.147433	482.075021	7.374515
5.800941	484.571440	7.379520
5.614673	465.307985	7.384525
5.954168	510.443848	7.389530
6.062310	506.587913	7.394534
6.231470	492.997682	7.399539
5.852049	491.414596	7.404544
6.115111	505.769585	7.409549
5.775475	525.984303	7.414554
5.948577	508.654609	7.419558
5.896166	490.012884	7.424563
5.318023	505.289961	7.429568
5.923273	495.874990	7.434573
5.865365	500.892440	7.439578
5.916216	511.344736	7.444582
5.941443	502.178422	7.449587
5.872638	489.214382	7.454592
6.051615	489.810110	7.459597
6.011986	517.591816	7.464602
5.796131	501.957272	7.469606
6.081904	510.326347	7.474611
5.618792	515.786221	7.479616
6.229204	492.802621	7.484621
6.067405	506.085271	7.489626
5.878207	527.668448	7.494630
6.351709	524.657728	7.499635
6.336265	502.062241	7.504640
6.248503	499.296987	7.509645
6.134468	520.691052	7.514650
5.839397	527.993842	7.519654
6.146761	512.271935	7.524659
5.763255	504.421863	7.529664
6.274564	502.571620	7.534669
6.345508	524.738322	7.539674
6.082488	517.330601	7.544678
5.954854	495.455552	7.549683
5.853345	495.316333	7.554688
5.887207	505.641119	7.559693
5.907494	517.690467	7.564698
5.889292	506.619312	7.569702
6.113377	491.566809	7.574707
6.037887	505.018484	7.579712
6.112208	509.293356	7.584717
6.179678	507.020650	7.589722
5.859333	513.653837	7.594726
6.112589	510.610660	7.599731
5.932857	525.196581	7.604736
6.190650	512.086510	7.609741
6.051994	498.288387	7.614746
6.037583	491.693401	7.619750
6.143686	487.093798	7.624755
5.874550	500.132465	7.629760
5.823530	496.628079	7.634765
5.814522	504.201825	7.639770
5.569562	507.438304	7.644774
5.691921	506.631329	7.649779
5.853449	502.048309	7.654784
6.218309	513.225773	7.659789
5.798039	518.923513	7.664794
6.158650	526.636644	7.669798
6.386263	504.961532	7.674803
6.081358	504.168540	7.679808
6.321489	501.212964	7.684813
5.992473	506.292184	7.689818
5.977484	496.740488	7.694822
6.283802	512.304873	7.699827
6.198484	502.961599	7.704832
6.248967	509.821657	7.709837
5.902229	507.900030	7.714842
6.010590	496.047977	7.719846
6.152486	494.383869	7.724851
5.850333	525.511539	7.729856
6.169489	506.932490	7.734861
5.758955	491.492012	7.739866
5.961127	506.765521	7.744870
6.047838	510.469832	7.749875
5.794940	510.721816	7.754880
6.012368	503.520097	7.759885
5.759331	510.050317	7.764890
5.779547	511.029688	7.769894
6.160449	504.607506	7.774899
6.124707	517.556716	7.779904
6.294092	487.975560	7.784909
6.133424	499.225260	7.789914
5.953277	497.514144	7.794918
6.055051	510.651632	7.799923
5.681057	510.747540	7.804928
5.968272	505.433082	7.809933
6.159527	511.699193	7.814938
5.961386	504.994679	7.819942
6.139705	505.948810	7.824947
5.731228	498.888605	7.829952
5.941127	498.941785	7.834957
5.978117	517.301901	7.839962
5.880170	521.026766	7.844966
6.004293	512.120418	7.849971
5.934233	502.334156	7.854976
5.920224	514.291507	7.859981
5.949023	532.926647	7.864986
6.009231	523.453265	7.869990
5.873733	495.928604	7.874995
5.979615	513.381007	7.880000
6.134981	523.564979	7.885005
6.320882	525.807891	7.890010
6.145583	511.320533	7.895014
6.253456	512.343226	7.900019
6.274689	510.825031	7.905024
6.426172	494.316726	7.910029
6.156345	511.913686	7.915034
6.287897	524.006406	7.920038
6.412357	511.075420	7.925043
6.081512	498.488010	7.930048
6.081826	510.459959	7.935053
6.255521	520.657867	7.940058
6.347082	502.642135	7.945062
5.981531	482.279941	7.950067
5.643740	488.520320	7.955072
5.904538	500.877153	7.960077
6.206943	501.610422	7.965082
6.062574	509.562465	7.970086
6.055871	498.953164	7.975091
5.904213	487.928936	7.980096
6.173933	478.144643	7.985101
6.114091	492.159471	7.990106
5.691831	480.432703	7.995110
5.954959	475.844739	8.000115
5.972483	488.037913	8.005133
5.889144	502.495083	8.010150
6.067212	505.052588	8.015168
5.837235	513.604782	8.020186
6.335898	515.567435	8.025203
6.254222	523.680775	8.030221
6.173536	497.802508	8.035238
6.005540	486.347981	8.040256
5.787163	500.258828	8.045274
5.946990	501.785882	8.050291
5.915684	518.315471	8.055309
5.932370	503.543449	8.060326
5.789896	511.076545	8.065344
5.893776	503.716256	8.070362
5.865389	515.823980	8.075379
6.108140	523.906928	8.080397
6.314613	510.186399	8.085414
6.275006	513.172681	8.090432
6.191933	513.528212	8.095450
6.219782	521.022735	8.100467
5.895276	515.436198	8.105485
5.926100	515.873961	8.110502
5.932729	516.658539	8.115520
6.071038	512.243001	8.120538
6.095146	511.390015	8.125555
6.072231	517.435663	8.130573
6.040558	529.106957	8.135590
6.091534	515.577723	8.140608
6.097558	507.720856	8.145626
6.364962	487.052584	8.150643
6.283641	503.228616	8.155661
6.014273	526.229292	8.160678
6.306048	520.878017	8.165696
6.013182	498.568852	8.170714
6.161365	501.810138	8.175731
6.381961	515.429326	8.180749
5.979570	504.250559	8.185766
5.996919	512.682572	8.190784
5.890973	519.025719	8.195802
6.160009	500.024602	8.200819
5.870386	494.464090	8.205837
6.107103	522.201702	8.210854
6.569681	532.012789	8.215872
6.267088	528.264330	8.220890
6.144845	525.531048	8.225907
6.138519	543.395331	8.230925
6.219969	545.491287	8.235942
6.451247	542.289263	8.240960
6.431419	525.181394	8.245978
6.708349	514.290443	8.250995
6.080280	530.956055	8.256013
5.875402	508.805416	8.261030
6.195243	523.683733	8.266048
6.228055	540.223512	8.271066
6.333405	535.415199	8.276083
6.325094	532.076148	8.281101
6.157233	533.159564	8.286118
6.455365	549.393278	8.291136
5.902828	536.352135	8.296154
6.204104	543.044119	8.301171
5.873974	557.763617	8.306189
6.202657	540.132915	8.311206
6.095786	527.169171	8.316224
6.365096	527.186135	8.321242
6.676266	546.283613	8.326259
6.408640	555.175521	8.331277
6.538931	547.937583	8.336294
6.573330	526.714623	8.341312
6.443403	536.579447	8.346330
6.747734	539.280712	8.351347
6.511346	528.239409	8.356365
6.414844	546.073532	8.361382
6.660946	545.576859	8.366400
6.432156	543.409157	8.371418
6.641141	518.556107	8.376435
6.442571	519.021448	8.381453
6.106807	515.200543	8.386470
6.382473	515.461466	8.391488
6.437135	536.484253	8.396506
6.670743	529.115305	8.401523
6.155272	516.613274	8.406541
6.236969	513.876598	8.411558
6.758442	520.462518	8.416576
6.465143	529.072218	8.421594
6.472761	538.550735	8.426611
6.189657	541.587986	8.431629
6.088917	530.803419	8.436646
6.666749	510.929049	8.441664
6.277732	533.320749	8.446682
6.571856	547.346987	8.451699
6.528796	540.592099	8.456717
6.549934	540.098164	8.461734
6.696949	538.101364	8.466752
6.649443	551.463005	8.471770
6.684386	538.652931	8.476787
6.442730	530.814253	8.481805
6.786234	534.688828	8.486822
6.673564	522.548157	8.491840
6.576971	535.424138	8.496858
6.708206	521.021445	8.501875
6.492294	500.296648	8.506893
6.121647	503.458268	8.511910
6.589276	522.817575	8.516928
6.746768	539.987845	8.521946
6.759237	525.870940	8.526963
6.316337	526.055587	8.531981
6.361303	515.898637	8.536998
6.787738	505.931634	8.542016
6.403581	526.694145	8.547034
6.506029	542.209712	8.552051
6.571652	547.263456	8.557069
6.596688	537.040908	8.562087
6.907988	531.732453	8.567104
6.913766	541.767910	8.572122
6.635278	504.681100	8.577139
6.824825	509.598637	8.582157
6.607821	520.472342	8.587175
6.576361	507.611179	8.592192
6.438820	501.298868	8.597210
6.468667	494.935381	8.602227
6.517488	521.941761	8.607245
6.540959	546.264256	8.612263
6.674334	529.257014	8.617280
6.649074	522.610087	8.622298
6.873542	540.557551	8.627315
6.857505	562.940593	8.632333
6.622141	551.620542	8.637351
6.944953	528.870117	8.642368
6.619361	511.227722	8.647386
6.622649	509.110034	8.652403
6.336789	514.092656	8.657421
6.672023	521.576922	8.662439
6.794838	527.896832	8.667456
6.354849	553.933359	8.672474
6.248903	539.887866	8.677491
6.825318	527.893675	8.682509
6.568773	542.296163	8.687527
6.939851	518.407190	8.692544
6.506695	544.602173	8.697562
6.400147	551.537393	8.702579
6.654568	535.569586	8.707597
6.591853	529.925513	8.712615
7.018454	540.095404	8.717632
6.736810	557.165477	8.722650
6.814210	546.603751	8.727667
6.715318	531.107409	8.732685
6.396201	526.592312	8.737703
6.922118	545.559643	8.742720
6.374271	553.123343	8.747738
6.782525	557.641764	8.752755
6.833195	542.346911	8.757773
6.872932	565.596576	8.762791
6.847054	581.229426	8.767808
6.818462	581.541320	8.772826
6.911795	569.776492	8.777843
6.547841	572.669281	8.782861
6.928295	574.712976	8.787879
6.820423	563.584187	8.792896
6.756983	588.028660	8.797914
6.563652	577.368485	8.802931
7.073359	558.779660	8.807949
6.522111	555.887314	8.812967
6.887614	573.893671	8.817984
6.764467	590.687265	8.823002
6.972241	564.803230	8.828019
7.013984	552.838930	8.833037
7.062635	564.175413	8.838055
7.072070	574.405017	8.843072
6.852911	576.439662	8.848090
6.924728	561.277772	8.853107
7.259976	560.459464	8.858125
6.835372	583.889606	8.863143
7.001644	580.750172	8.868160
7.069278	565.872847	8.873178
7.114770	579.446935	8.878195
6.911547	563.387648	8.883213
7.024343	563.226499	8.888231
7.210774	573.503308	8.893248
6.946019	556.700570	8.898266
6.929464	574.452929	8.903283
6.915068	583.519972	8.908301
6.736449	581.787747	8.913319
7.083818	552.729872	8.918336
7.180446	561.774027	8.923354
7.261697	578.509329	8.928371
7.211188	575.714690	8.933389
6.999629	568.144662	8.938407
7.177510	569.394111	8.943424
7.031091	578.125686	8.948442
6.845629	581.027256	8.953459
7.142058	566.077878	8.958477
6.843049	555.622532	8.963495
6.797977	573.260247	8.968512
6.726442	580.343193	8.973530
6.855033	571.222095	8.978547
7.135559	552.015824	8.983565
6.993779	562.318621	8.988583
7.011014	567.102100	8.993600
6.982757	564.358592	8.998618
7.041078	558.495448	9.003635
6.945257	566.697247	9.008653
6.922589	576.192207	9.013671
7.025670	579.282149	9.018688
6.819398	585.045022	9.023706
7.162267	576.183703	9.028723
7.226148	593.432871	9.033741
7.280975	594.775275	9.038759
7.369327	594.060643	9.043776
7.275251	595.158930	9.048794
7.134730	576.158096	9.053811
7.374699	581.131970	9.058829
7.062059	584.640221	9.063847
7.159985	560.181730	9.068864
7.305492	567.478536	9.073882
6.976737	571.194115	9.078899
7.468312	579.759252	9.083917
7.085649	579.779460	9.088935
7.336490	575.289812	9.093952
7.470860	583.852581	9.098970
7.271030	572.845450	9.103987
7.317618	559.275673	9.109005
6.990475	573.608090	9.114023
7.107978	571.730501	9.119040
7.275175	591.717138	9.124058
7.404183	602.670394	9.129075
7.371189	567.284210	9.134093
7.287384	569.385143	9.139111
7.404773	581.059297	9.144128
7.256583	584.828283	9.149146
7.083126	568.584397	9.154163
7.314372	588.050549	9.159181
7.346041	602.181216	9.164199
7.400771	599.529667	9.169216
7.328558	584.702494	9.174234
6.948833	594.606964	9.179251
7.275495	594.694251	9.184269
7.377520	623.275141	9.189287
7.271752	602.268886	9.194304
7.309449	591.658195	9.199322
7.232964	609.744228	9.204339
7.448834	608.227341	9.209357
7.479182	617.352052	9.214375
7.476332	610.835795	9.219392
7.130077	617.492930	9.224410
7.262060	607.692105	9.229427
7.493160	603.168614	9.234445
7.155023	619.823310	9.239463
7.495065	614.290354	9.244480
7.921693	605.627616	9.249498
7.633893	605.265222	9.254515
7.297482	602.740204	9.259533
7.225098	602.507618	9.264551
7.266673	586.020166	9.269568
7.390566	603.767160	9.274586
6.962257	620.706369	9.279603
7.449318	605.848840	9.284621
7.160187	601.770079	9.289639
7.252078	604.612535	9.294656
7.342408	598.352660	9.299674
7.251629	625.036720	9.304691
7.148334	610.157587	9.309709
7.280121	624.864578	9.314727
7.547752	647.178039	9.319744
7.879244	638.036653	9.324762
7.602051	643.581902	9.329779
7.766761	627.199712	9.334797
7.499835	636.941316	9.339815
7.712180	610.502566	9.344832
7.596096	618.187216	9.349850
7.450620	621.984888	9.354867
7.653672	615.997242	9.359885
7.506131	616.553042	9.364903
7.566414	603.258248	9.369920
7.702286	620.375505	9.374938
7.484252	621.022559	9.379955
7.831362	625.170009	9.384973
7.966322	605.443289	9.389991
7.511309	616.331993	9.395008
7.876000	604.672351	9.400026
7.407977	609.788623	9.405043
7.643270	596.045739	9.410061
7.406307	601.799324	9.415079
7.425252	618.962962	9.420096
7.556199	609.139872	9.425114
7.594150	648.474683	9.430131
7.814309	636.955800	9.435149
7.844821	626.400685	9.440167
7.388590	619.702234	9.445184
7.828353	634.460968	9.450202
7.415408	651.692864	9.455219
8.041832	632.741744	9.460237
7.741279	649.153711	9.465255
7.640912	641.625393	9.470272
7.699665	621.728226	9.475290
7.726780	643.715487	9.480307
7.650909	652.588160	9.485325
7.570900	634.283851	9.490343
7.463497	632.001122	9.495360
7.915518	646.345161	9.500378
7.824579	633.452000	9.505395
7.962185	651.446715	9.510413
7.745340	650.929031	9.515431
7.786866	637.063745	9.520448
7.816892	628.200567	9.525466
8.197146	650.620977	9.530483
7.929027	638.594067	9.535501
7.851588	620.855434	9.540519
7.474068	625.823818	9.545536
7.840022	633.275413	9.550554
7.415964	653.327958	9.555571
7.699504	644.210237	9.560589
7.862212	625.446160	9.565607
7.911396	621.004386	9.570624
7.975452	639.262550	9.575642
7.939205	633.335893	9.580659
7.950203	634.825269	9.585677
8.213168	653.060713	9.590695
8.286690	642.323823	9.595712
8.088097	623.707423	9.600730
7.708109	619.672897	9.605747
7.773363	604.260937	9.610765
7.971045	626.479954	9.615783
7.916879	640.375107	9.620800
8.135385	629.769834	9.625818
7.865283	624.251999	9.630835
7.716069	636.261117	9.635853
7.843717	637.171036	9.640871
7.840742	632.118167	9.645888
8.014758	630.943437	9.650906
7.740278	654.677723	9.655923
7.870639	646.697706	9.660941
8.002158	635.369999	9.665959
7.864839	642.417008	9.670976
8.036934	641.285692	9.675994
8.122506	629.493862	9.681011
8.065106	635.546927	9.686029
8.008073	647.733287	9.691047
7.705579	640.327030	9.696064
7.833075	637.643672	9.701082
7.894205	653.009136	9.706099
8.122173	630.932419	9.711117
7.783470	639.524494	9.716135
7.646459	635.911199	9.721152
7.839387	629.973238	9.726170
7.830100	651.367970	9.731187
7.862527	636.636317	9.736205
8.175251	654.657593	9.741223
8.334528	660.843614	9.746240
8.046073	630.254105	9.751258
7.877785	641.855174	9.756275
7.811757	654.928904	9.761293
8.233834	661.126993	9.766311
8.073143	659.943024	9.771328
8.404951	659.563546	9.776346
8.377495	667.074660	9.781363
7.954983	673.951254	9.786381
8.267614	665.038106	9.791399
8.186329	665.867132	9.796416
8.072608	658.503764	9.801434
7.948232	666.964891	9.806451
8.091693	680.548068	9.811469
8.438626	676.364962	9.816487
8.129405	668.317753	9.821504
8.132505	679.863566	9.826522
8.074540	679.446658	9.831539
8.164243	676.685998	9.836557
8.688863	662.584402	9.841575
8.202464	685.983584	9.846592
8.061428	672.539471	9.851610
8.179809	665.509492	9.856627
8.363539	670.323937	9.861645
8.555647	679.645709	9.866663
8.327933	679.348855	9.871680
8.600593	666.649152	9.876698
7.872140	664.974227	9.881715
8.183873	660.605754	9.886733
8.172938	661.879428	9.891751
7.886922	675.695735	9.896768
8.054168	678.088961	9.901786
8.281212	661.555428	9.906803
8.233826	659.124429	9.911821
8.255001	660.168449	9.916839
8.406871	676.940108	9.921856
8.384769	680.478889	9.926874
8.279703	682.937092	9.931891
8.386739	668.887378	9.936909
8.747708	669.878000	9.941927
8.197924	677.819241	9.946944
8.530167	682.195087	9.951962
8.503783	673.746900	9.956979
8.113604	671.454120	9.961997
8.479636	673.373573	9.967015
8.238522	682.549283	9.972032
8.315308	669.096925	9.977050
8.138625	670.162916	9.982067
7.883667	672.281914	9.987085
8.196535	700.597458	9.992103
8.661883	707.177090	9.997120
8.758914	703.188972	10.002138
8.541493	690.162770	10.007155
8.540109	678.557863	10.012173
8.519509	664.531016	10.017191
8.174134	675.266442	10.022208
8.646868	700.598600	10.027226
8.776148	699.354212	10.032243
8.462922	682.403285	10.037261
8.671743	669.906400	10.042279
8.331815	677.803712	10.047296
8.358237	667.074194	10.052314
8.553627	691.493180	10.057331
8.609530	707.132717	10.062349
8.761336	696.924044	10.067367
8.596238	698.594946	10.072384
8.594956	687.792160	10.077402
8.530879	669.875817	10.082419
8.206861	689.982035	10.087437
8.993519	711.136586	10.092455
8.672526	711.687008	10.097472
8.646633	691.345398	10.102490
8.524093	672.175573	10.107507
8.383510	686.079735	10.112525
8.730274	690.116956	10.117543
8.619949	699.904748	10.122560
8.612438	702.999708	10.127578
8.711727	698.138128	10.132595
8.289358	696.833271	10.137613
8.641540	700.307941	10.142631
8.321898	709.324053	10.147648
8.681833	718.889794	10.152666
9.093328	695.570482	10.157683
8.851399	692.917267	10.162701
8.898043	701.561806	10.167719
8.709165	717.600664	10.172736
8.638159	698.396904	10.177754
8.702158	688.391968	10.182771
8.282606	690.463778	10.187789
8.616570	696.375048	10.192807
8.480595	713.808125	10.197824
8.457667	703.946347	10.202842
8.667295	688.634329	10.207859
8.789177	708.474810	10.212877
8.854412	692.773868	10.217895
8.774820	704.099472	10.222912
8.957337	704.380318	10.227930
8.856242	702.733077	10.232947
8.590172	712.448019	10.237965
8.901487	697.565622	10.242983
8.958658	705.869245	10.248000
8.681325	700.474789	10.253018
9.029150	692.712777	10.258035
8.843846	700.150808	10.263053
9.054535	693.425947	10.268071
8.806812	696.684485	10.273088
8.817241	707.638718	10.278106
8.868573	703.764914	10.283123
8.908981	698.284594	10.288141
9.046032	713.935819	10.293159
8.955625	700.553670	10.298176
8.737027	690.903223	10.303194
8.662599	687.396175	10.308211
8.684324	717.551109	10.313229
9.237031	723.652165	10.318247
9.080605	713.776034	10.323264
8.908717	704.071711	10.328282
9.149336	707.746365	10.333299
8.802503	710.494557	10.338317
8.957962	686.788158	10.343335
9.100826	714.975174	10.348352
8.841123	715.998998	10.353370
9.111124	709.240614	10.358387
9.326932	728.209827	10.363405
8.938681	726.176984	10.368423
8.921711	712.384863	10.373440
8.882785	716.250066	10.378458
9.317637	727.943503	10.383475
8.853335	726.778214	10.388493
8.926867	731.318252	10.393511
9.145236	749.272282	10.398528
9.191245	741.357913	10.403546
8.986215	721.025007	10.408563
9.136722	742.411958	10.413581
9.409188	741.476000	10.418599
9.022015	728.572969	10.423616
9.099425	715.130111	10.428634
9.045615	727.849323	10.433651
8.923184	749.289653	10.438669
9.019925	732.361252	10.443687
9.126344	725.298881	10.448704
8.963791	724.068573	10.453722
9.066397	727.880083	10.458739
9.048779	739.279799	10.463757
9.071809	736.238297	10.468775
9.121077	720.838703	10.473792
9.077399	731.902457	10.478810
9.159413	744.297743	10.483827
9.262923	750.243281	10.488845
9.223957	737.922193	10.493863
9.442798	746.242908	10.498880
9.265862	752.787596	10.503898
9.452147	730.796244	10.508915
9.178844	736.815559	10.513933
9.313481	743.701857	10.518951
9.307819	725.836803	10.523968
8.954748	731.665711	10.528986
9.351017	725.682303	10.534003
9.243762	741.968848	10.539021
9.497374	740.610726	10.544039
9.366355	731.102333	10.549056
9.412982	734.675622	10.554074
9.479284	739.021437	10.559091
9.580564	736.877192	10.564109
9.470298	726.825064	10.569127
9.375606	736.819001	10.574144
9.509636	733.156758	10.579162
9.740604	732.341604	10.584179
9.518032	736.357108	10.589197
9.581994	741.379998	10.594215
9.792327	739.336990	10.599232
9.470453	737.396889	10.604250
9.735158	722.099449	10.609267
9.379341	721.255807	10.614285
9.122328	711.832108	10.619303
9.428981	700.510342	10.624320
9.294863	713.218607	10.629338
9.645786	723.699176	10.634355
9.339959	747.141621	10.639373
9.447640	741.671521	10.644391
9.670185	717.301900	10.649408
9.382473	743.242049	10.654426
9.487674	722.416063	10.659443
9.552058	734.125660	10.664461
9.742142	714.024534	10.669479
9.895941	718.317607	10.674496
9.207694	733.762908	10.679514
9.646120	734.944322	10.684531
9.590558	726.744563	10.689549
9.517389	713.364277	10.694567
9.797832	728.059297	10.699584
9.736144	741.881691	10.704602
9.542125	742.773237	10.709619
9.475619	727.899128	10.714637
9.583748	721.431297	10.719655
9.849199	741.001606	10.724672
9.474364	742.851328	10.729690
9.514579	727.469360	10.734707
9.457633	723.277906	10.739725
9.265897	735.362909	10.744743
9.258511	736.994174	10.749760
9.362577	728.399630	10.754778
9.465796	713.762671	10.759795
9.290306	715.568524	10.764813
9.417428	720.460924	10.769831
9.662029	734.986429	10.774848
9.502426	757.955930	10.779866
9.820368	771.581989	10.784883
10.082450	785.424618	10.789901
9.610703	776.741984	10.794919
10.057853	744.320017	10.799936
9.703465	750.867658	10.804954
9.747339	745.234132	10.809971
9.819260	737.878619	10.814989
9.462172	748.518618	10.820007
10.285401	765.558461	10.825024
9.619388	754.001830	10.830042
9.971570	743.781759	10.835059
9.795598	747.591587	10.840077
9.559312	734.795077	10.845095
9.911118	750.628705	10.850112
9.677288	778.707661	10.855130
9.934752	762.277527	10.860147
9.847220	770.341290	10.865165
9.734886	776.482700	10.870183
9.977782	757.914899	10.875200
9.931453	765.031648	10.880218
9.873229	765.961468	10.885235
9.947212	775.551671	10.890253
9.937128	760.882519	10.895271
9.858297	757.992750	10.900288
9.716372	776.795512	10.905306
9.518285	778.752803	10.910323
9.755874	780.330600	10.915341
9.873188	755.804142	10.920359
9.957645	764.815991	10.925376
9.630947	773.688857	10.930394
9.667167	772.961873	10.935411
10.310588	763.311900	10.940429
9.847727	761.871641	10.945447
10.001964	774.740123	10.950464
9.723260	778.109576	10.955482
9.930644	769.068622	10.960499
10.251170	781.964339	10.965517
10.205437	797.735202	10.970535
10.339305	776.480798	10.975552
10.097280	779.704956	10.980570
10.045624	767.178025	10.985587
9.965644	781.639134	10.990605
9.991015	762.945899	10.995623
10.223741	771.254198	11.000640
10.047702	759.874988	11.005658
10.221336	781.900323	11.010675
10.285565	771.547060	11.015693
10.154352	752.137196	11.020711
10.523209	764.755497	11.025728
10.222236	761.408474	11.030746
10.054365	758.677869	11.035763
10.065769	783.763851	11.040781
10.096024	771.687135	11.045799
10.390665	751.170855	11.050816
10.237104	766.896530	11.055834
10.190444	775.153094	11.060851
10.622122	768.086546	11.065869
10.089274	763.420134	11.070887
10.547834	762.770758	11.075904
10.525166	757.292673	11.080922
10.456636	750.262842	11.085939
10.242443	766.110219	11.090957
9.797710	770.970498	11.095975
10.163790	768.362521	11.100992
10.260267	751.197788	11.106010
9.971991	759.514248	11.111027
10.104276	775.061922	11.116045
10.222984	769.131647	11.121063
10.693985	784.674425	11.126080
10.388573	793.785945	11.131098
10.065687	779.997774	11.136115
10.447540	782.163872	11.141133
10.515270	780.203365	11.146151
10.658988	778.749061	11.151168
10.420833	792.992192	11.156186
10.364570	776.297240	11.161203
10.205573	757.889233	11.166221
10.212744	774.735686	11.171239
10.887029	772.799025	11.176256
10.433628	784.737595	11.181274
10.283643	769.559707	11.186291
10.315769	773.762105	11.191309
10.351935	787.132560	11.196327
10.418986	794.485243	11.201344
10.334095	805.236065	11.206362
10.483391	795.967158	11.211379
10.629079	792.481471	11.216397
10.481423	791.932864	11.221415
10.815495	795.775413	11.226432
10.543036	799.556329	11.231450
10.450690	797.711324	11.236467
10.711143	793.956049	11.241485
10.557333	809.420953	11.246503
10.588859	796.373299	11.251520
10.669615	788.375429	11.256538
10.930157	798.502776	11.261555
11.339407	784.327246	11.266573
10.369024	783.804983	11.271591
10.213078	779.252218	11.276608
10.430773	779.435446	11.281626
10.788035	772.351871	11.286643
10.877691	788.777435	11.291661
10.706866	802.946178	11.296679
10.758172	787.962802	11.301696
10.599573	769.908164	11.306714
10.375882	797.914732	11.311731
10.687494	796.603797	11.316749
10.658204	799.566978	11.321767
10.834015	802.366280	11.326784
10.888637	805.614040	11.331802
10.748492	786.995457	11.336819
10.945695	780.955775	11.341837
10.806504	803.896683	11.346855
10.868561	781.544196	11.351872
10.830979	788.788020	11.356890
10.792497	805.358957	11.361907
10.656660	791.681166	11.366925
10.720368	796.770339	11.371943
11.016897	788.049395	11.376960
11.025669	795.781199	11.381978
10.854388	786.428598	11.386995
10.768170	786.129120	11.392013
10.683576	801.846878	11.397031
10.770704	798.529684	11.402048
11.203066	794.890351	11.407066
10.901103	789.854662	11.412083
10.861033	798.637569	11.417101
10.674706	806.668183	11.422119
10.787864	790.033088	11.427136
10.774578	785.312000	11.432154
10.876284	793.037498	11.437171
11.181718	807.778747	11.442189
10.856168	805.350987	11.447207
10.820837	791.025357	11.452224
11.062522	794.681750	11.457242
10.637604	780.028785	11.462259
10.951842	785.571205	11.467277
10.859468	796.510805	11.472295
10.847353	794.793253	11.477312
10.950855	791.834282	11.482330
10.585740	787.235000	11.487347
10.854979	794.697245	11.492365
11.040545	786.538786	11.497383
10.917580	800.823306	11.502400
11.041075	818.541588	11.507418
10.936567	831.938084	11.512435
11.278023	821.726622	11.517453
11.268317	819.226788	11.522471
11.014345	813.472226	11.527488
11.196724	831.169870	11.532506
11.232611	832.540123	11.537523
11.492381	806.246997	11.542541
11.362683	793.141759	11.547559
11.005547	794.292683	11.552576
11.145937	777.173406	11.557594
10.989469	782.648079	11.562611
11.152202	796.663099	11.567629
11.048819	826.830953	11.572647
11.108725	818.250348	11.577664
11.599542	813.647468	11.582682
11.193207	828.176329	11.587699
11.285826	821.637809	11.592717
11.202634	838.734538	11.597735
11.291565	807.837097	11.602752
11.566156	804.961729	11.607770
11.269075	828.526148	11.612787
11.434845	829.020044	11.617805
11.107023	816.336795	11.622823
10.867919	809.080961	11.627840
11.207566	819.131585	11.632858
11.357570	818.027819	11.637875
11.489032	814.118311	11.642893
11.314804	812.414853	11.647911
11.626976	799.746100	11.652928
11.622406	829.603417	11.657946
11.186859	842.839035	11.662963
11.246436	813.412290	11.667981
11.187751	834.153312	11.672999
11.189422	824.609747	11.678016
11.449359	809.851056	11.683034
11.368904	829.172325	11.688051
11.639529	835.172147	11.693069
11.369505	830.484027	11.698087
11.294438	810.421967	11.703104
11.370340	818.699727	11.708122
11.052606	833.100201	11.713139
11.481908	809.886898	11.718157
11.466604	830.202943	11.723175
11.516422	839.455832	11.728192
11.595592	814.428532	11.733210
11.427720	826.988671	11.738227
12.084825	837.709687	11.743245
11.905666	846.026857	11.748263
11.870473	828.305601	11.753280
11.984732	824.339697	11.758298
11.701441	825.416527	11.763315
12.056423	815.739208	11.768333
11.427008	821.352567	11.773351
11.325497	825.747589	11.778368
11.717110	832.562925	11.783386
11.394968	830.385517	11.788403
11.489340	823.738565	11.793421
11.235980	822.791591	11.798439
11.722128	819.847706	11.803456
11.524402	818.388422	11.808474
11.819395	825.377652	11.813491
11.727099	830.463786	11.818509
11.554512	820.222834	11.823527
11.525817	820.052790	11.828544
11.813564	837.064700	11.833562
12.231314	845.692765	11.838579
12.346750	826.881445	11.843597
11.929162	821.505499	11.848615
11.918988	823.538211	11.853632
12.106133	803.114114	11.858650
11.898173	818.115364	11.863667
11.970494	820.667668	11.868685
12.216030	812.120448	11.873703
11.817510	831.690982	11.878720
11.956968	803.243117	11.883738
11.976587	806.324955	11.888755
11.909648	823.644315	11.893773
11.944369	815.312888	11.898791
11.651478	811.185099	11.903808
11.996701	802.913754	11.908826
11.785165	806.448249	11.913843
11.973370	821.691532	11.918861
11.821948	826.208749	11.923879
11.599512	807.395331	11.928896
11.901919	816.530796	11.933914
11.658464	816.184388	11.938931
11.895450	822.501985	11.943949
11.860752	808.811007	11.948967
11.668060	822.341820	11.953984
12.081000	829.974280	11.959002
12.293262	827.243327	11.964019
12.107868	811.237807	11.969037
11.896506	822.473689	11.974055
11.932699	841.540129	11.979072
12.442049	823.832308	11.984090
12.267308	829.914386	11.989107
11.937104	815.421673	11.994125
12.166799	815.585108	11.999143
11.877588	826.587566	12.004160
12.294245	824.447081	12.009178
12.118063	831.437820	12.014195
12.307004	850.343730	12.019213
12.220438	834.643521	12.024231
12.023091	835.793626	12.029248
12.154242	837.772186	12.034266
12.120995	850.552750	12.039283
12.062673	837.930234	12.044301
12.330615	841.626579	12.049319
11.964723	847.757177	12.054336
12.281317	839.539547	12.059354
12.479352	839.251445	12.064371
12.507047	847.300536	12.069389
12.380609	825.113745	12.074407
12.342370	849.598751	12.079424
12.526506	835.964769	12.084442
12.431088	841.322218	12.089459
12.355683	853.308681	12.094477
12.429268	844.071247	12.099495
12.234016	834.083474	12.104512
12.896498	833.477936	12.109530
12.385719	837.093770	12.114547
12.115380	819.500730	12.119565
12.285103	822.288841	12.124583
12.187855	843.480521	12.129600
12.402272	836.846690	12.134618
12.702217	835.379651	12.139635
12.449804	853.700798	12.144653
12.513703	851.812255	12.149671
12.255561	839.632790	12.154688
12.377353	846.552155	12.159706
12.084299	846.491724	12.164723
12.292728	836.507890	12.169741
12.550565	828.436947	12.174759
12.330542	834.956220	12.179776
12.466187	841.911177	12.184794
12.670852	841.452733	12.189811
12.725052	842.474087	12.194829
12.448374	846.909378	12.199847
12.609919	840.744300	12.204864
12.605089	818.751441	12.209882
12.502508	835.279276	12.214899
12.394293	831.993175	12.219917
12.448721	827.888869	12.224935
12.477065	850.245221	12.229952
12.582203	849.586154	12.234970
12.543747	834.898791	12.239987
12.501272	852.741267	12.245005
12.699077	857.579914	12.250023
12.932507	864.190658	12.255040
12.708346	874.111222	12.260058
12.754650	862.246982	12.265075
12.576490	875.101501	12.270093
13.272809	866.554835	12.275111
12.693407	859.140997	12.280128
13.066304	850.037415	12.285146
13.062560	829.902733	12.290163
12.644400	848.327131	12.295181
12.686337	843.398428	12.300199
12.685232	836.467131	12.305216
12.868928	819.996284	12.310234
12.569496	838.201103	12.315251
12.833422	860.726063	12.320269
13.103257	857.414677	12.325287
12.926469	865.640445	12.330304
13.268226	851.793739	12.335322
13.091709	824.567332	12.340339
13.117278	823.413872	12.345357
12.992012	835.447330	12.350375
12.753613	849.100355	12.355392
12.915557	841.057355	12.360410
13.066534	830.518010	12.365427
12.734515	831.833934	12.370445
13.095346	841.650326	12.375463
12.870633	833.610220	12.380480
13.038112	820.048968	12.385498
13.060903	828.200801	12.390515
12.981098	836.979472	12.395533
12.824092	823.835130	12.400551
12.537988	853.064884	12.405568
13.162008	862.632929	12.410586
13.337091	865.583308	12.415603
12.969830	856.901958	12.420621
13.221196	853.857926	12.425639
12.986001	872.213642	12.430656
13.189289	866.835052	12.435674
13.600337	862.048049	12.440691
13.294323	871.426770	12.445709
13.481632	855.217229	12.450727
12.899638	858.101429	12.455744
13.236503	853.259776	12.460762
13.262411	850.317847	12.465779
13.137176	862.623003	12.470797
13.362790	876.617570	12.475815
13.422023	864.279070	12.480832
13.345256	842.650334	12.485850
13.149736	828.287969	12.490867
13.079590	842.500725	12.495885
13.354253	847.165884	12.500903
13.391525	858.225307	12.505920
12.957228	865.419009	12.510938
13.242687	857.867464	12.515955
13.218090	853.399341	12.520973
13.589963	855.406707	12.525991
13.108457	854.804832	12.531008
13.037408	874.209621	12.536026
13.038482	878.949226	12.541043
13.241292	865.375896	12.546061
13.212828	868.678530	12.551079
13.531867	877.785011	12.556096
13.413009	881.702234	12.561114
13.499198	871.208499	12.566131
13.223438	867.879033	12.571149
13.330763	865.182634	12.576167
13.363926	883.422776	12.581184
13.374111	870.536123	12.586202
13.516791	872.887488	12.591219
13.456600	881.255667	12.596237
13.704039	887.348886	12.601255
13.876257	882.217093	12.606272
13.480124	879.050984	12.611290
13.669306	878.799473	12.616307
13.506826	870.125209	12.621325
13.656743	870.429454	12.626343
13.918710	858.653659	12.631360
13.566292	864.434195	12.636378
13.718885	867.693723	12.641395
13.791372	851.201074	12.646413
13.599123	842.712997	12.651431
13.582736	866.901878	12.656448
13.469451	860.145367	12.661466
13.974887	867.489404	12.666483
13.627928	884.112781	12.671501
13.990206	879.950109	12.676519
13.742070	860.569859	12.681536
13.596091	860.981058	12.686554
13.888009	860.527480	12.691571
13.629406	870.387018	12.696589
14.002863	869.675443	12.701607
13.902234	873.688739	12.706624
13.741078	872.245252	12.711642
14.052974	881.344846	12.716659
13.410510	867.535903	12.721677
13.831102	883.649565	12.726695
13.825439	882.988734	12.731712
13.883413	885.937019	12.736730
14.114780	883.889729	12.741747
13.967600	893.126990	12.746765
13.966194	883.785518	12.751783
14.074115	873.495715	12.756800
13.985260	878.464200	12.761818
14.002059	882.315611	12.766835
14.049863	890.798493	12.771853
14.183572	877.115344	12.776871
14.004264	871.637814	12.781888
13.797028	876.937100	12.786906
14.253101	867.328158	12.791923
14.053670	874.817414	12.796941
13.857466	867.543540	12.801959
14.075208	870.212040	12.806976
14.153857	875.920754	12.811994
14.277379	872.576373	12.817011
14.187547	879.662285	12.822029
14.096192	872.171626	12.827047
14.204597	879.307335	12.832064
14.105854	883.010068	12.837082
14.286810	864.958836	12.842099
13.586110	865.476759	12.847117
14.001456	869.470322	12.852135
14.475723	874.346928	12.857152
13.996430	886.954349	12.862170
14.278653	883.034571	12.867187
14.270239	872.841926	12.872205
13.932897	872.662961	12.877223
14.043119	885.647443	12.882240
14.089734	879.365157	12.887258
14.249577	879.286857	12.892275
14.120481	893.936457	12.897293
14.145121	883.678220	12.902311
14.259612	875.857359	12.907328
14.233170	888.521506	12.912346
14.467848	878.908701	12.917363
14.305480	878.665594	12.922381
14.131659	891.951679	12.927399
14.664707	875.620628	12.932416
13.938603	887.867759	12.937434
14.129537	899.934229	12.942451
14.412372	906.874928	12.947469
14.582045	902.096314	12.952487
14.518345	906.541199	12.957504
14.237219	901.146905	12.962522
14.810762	892.907644	12.967539
14.637519	901.813478	12.972557
14.545970	897.164624	12.977575
14.665331	898.851516	12.982592
14.779033	895.094391	12.987610
14.667702	889.198050	12.992627
14.518167	895.951405	12.997645
14.526353	913.808507	13.002663
14.673986	892.727998	13.007680
14.567304	893.167930	13.012698
15.045885	894.696468	13.017715
14.812872	882.981985	13.022733
14.779505	862.174674	13.027751
14.858661	867.434993	13.032768
14.668332	861.770951	13.037786
14.501514	850.430100	13.042803
14.478894	872.593778	13.047821
14.580563	886.111426	13.052839
14.971278	886.016129	13.057856
14.700221	903.273371	13.062874
14.932279	905.276985	13.067891
14.879905	901.481967	13.072909
14.603705	880.657195	13.077927
14.860220	881.603791	13.082944
14.888877	896.478735	13.087962
14.780119	896.877978	13.092979
14.851441	914.645042	13.097997
14.766568	898.607173	13.103015
14.830736	880.384425	13.108032
14.769171	896.567546	13.113050
14.893596	895.041734	13.118067
15.014986	897.475636	13.123085
15.002318	898.507158	13.128103
15.122641	914.027530	13.133120
14.864396	916.969923	13.138138
15.151825	907.075717	13.143155
15.009006	896.324807	13.148173
14.884153	906.775493	13.153191
15.399148	903.147276	13.158208
15.106527	887.450561	13.163226
15.017078	886.628227	13.168243
14.958569	897.863407	13.173261
14.753775	886.717338	13.178279
15.156562	894.453943	13.183296
14.814674	913.902948	13.188314
14.998929	902.640916	13.193331
14.992216	915.356928	13.198349
14.787295	903.129454	13.203367
15.059404	886.183415	13.208384
14.560089	903.959061	13.213402
14.986125	913.102788	13.218419
14.885706	905.328152	13.223437
14.880782	927.121265	13.228455
15.163309	937.077791	13.233472
15.371849	920.878054	13.238490
15.451758	916.396775	13.243507
15.553781	933.203423	13.248525
15.579097	926.061079	13.253543
15.780079	931.189800	13.258560
15.455055	900.237679	13.263578
15.487427	888.138872	13.268595
15.330444	898.211891	13.273613
15.249304	897.223364	13.278631
15.179256	885.801845	13.283648
15.374333	885.858630	13.288666
15.478769	895.186758	13.293683
15.581757	879.948062	13.298701
15.366990	882.001701	13.303719
15.508223	903.111939	13.308736
15.285153	880.792354	13.313754
15.562283	896.059589	13.318771
15.480511	883.605730	13.323789
15.240433	911.266091	13.328807
15.531530	918.433030	13.333824
15.539439	920.464144	13.338842
15.439013	905.690915	13.343859
15.695825	911.285281	13.348877
15.558564	934.163976	13.353895
15.803371	922.906288	13.358912
15.725285	923.344349	13.363930
15.849041	903.398878	13.368947
16.033768	911.812701	13.373965
15.572680	902.245193	13.378983
15.541342	881.868707	13.384000
15.786893	891.464776	13.389018
15.596205	878.378497	13.394035
15.975191	881.720270	13.399053
15.543523	892.567426	13.404071
15.733753	902.198326	13.409088
15.782456	909.637442	13.414106
15.813059	903.087094	13.419123
15.828057	907.119175	13.424141
15.645474	926.033537	13.429159
16.188255	915.988986	13.434176
15.765310	890.362036	13.439194
15.479424	885.804538	13.444211
15.892958	904.656475	13.449229
15.506390	932.546247	13.454247
15.837475	901.426362	13.459264
15.962089	919.047259	13.464282
15.947889	902.967104	13.469299
15.955623	896.661519	13.474317
15.861339	925.146117	13.479335
16.210952	931.261730	13.484352
16.066498	924.579910	13.489370
15.937117	915.767114	13.494387
16.234081	906.400134	13.499405
15.982325	924.993235	13.504423
16.265908	912.327933	13.509440
16.073814	917.300207	13.514458
15.936296	920.496891	13.519475
16.170467	912.931458	13.524493
15.922089	918.123314	13.529511
16.174682	921.828316	13.534528
16.092035	935.866499	13.539546
16.088518	924.626132	13.544563
16.507084	914.512664	13.549581
16.328702	927.061141	13.554599
16.265489	914.520747	13.559616
16.450266	930.185857	13.564634
16.011683	920.605959	13.569651
16.407685	903.265212	13.574669
16.271790	922.798760	13.579687
16.365922	928.943799	13.584704
15.990303	921.765082	13.589722
15.944569	924.792996	13.594739
16.317495	909.603339	13.599757
15.974395	918.460992	13.604775
16.133643	902.720583	13.609792
16.397821	917.862947	13.614810
16.292018	936.403210	13.619827
16.275329	926.006537	13.624845
16.240426	910.393258	13.629863
16.496167	902.320754	13.634880
16.579651	907.078434	13.639898
16.384254	922.788551	13.644915
16.088790	898.973219	13.649933
16.052348	915.955249	13.654951
16.099409	940.536808	13.659968
16.541518	946.360342	13.664986
16.316510	943.220846	13.670003
16.751987	946.031876	13.675021
16.822958	946.811157	13.680039
16.654701	973.964319	13.685056
16.725837	962.387457	13.690074
16.644611	946.556067	13.695091
16.856026	930.781720	13.700109
16.801717	946.483011	13.705127
17.091595	930.333290	13.710144
16.585291	917.593548	13.715162
16.484806	927.757913	13.720179
16.686104	920.302409	13.725197
16.943310	919.887136	13.730215
17.004800	921.652080	13.735232
17.023873	907.721970	13.740250
16.627873	911.990236	13.745267
17.241940	910.537699	13.750285
17.247478	913.930369	13.755303
16.677520	910.984366	13.760320
16.830242	897.803929	13.765338
16.955414	905.660709	13.770355
17.071478	896.415731	13.775373
16.865442	910.405402	13.780391
16.525141	913.427577	13.785408
16.994747	903.713549	13.790426
16.593471	896.859867	13.795443
16.743120	903.947346	13.800461
16.372312	919.741945	13.805479
16.686313	929.800915	13.810496
16.616373	933.506183	13.815514
16.794224	942.143640	13.820531
17.015331	949.595318	13.825549
16.898224	963.598680	13.830567
16.967139	951.245128	13.835584
17.209769	927.997255	13.840602
16.778626	938.362295	13.845619
17.305768	931.629807	13.850637
17.069997	955.627286	13.855655
17.077134	958.509005	13.860672
17.207336	950.461354	13.865690
16.992896	935.451294	13.870707
17.002237	925.435358	13.875725
17.180430	951.396085	13.880743
17.034088	959.361426	13.885760
17.339921	947.709678	13.890778
17.247495	934.511764	13.895795
17.353478	950.735544	13.900813
16.985794	959.566385	13.905831
17.180311	937.220021	13.910848
17.647712	943.910215	13.915866
17.447812	952.742059	13.920883
17.406492	937.931282	13.925901
17.475485	935.336162	13.930919
17.218737	935.048823	13.935936
17.395247	926.605245	13.940954
17.401069	945.497057	13.945971
17.519865	948.360519	13.950989
17.345448	949.164607	13.956007
17.614545	937.743486	13.961024
17.628956	920.683243	13.966042
17.444939	947.183914	13.971059
17.475323	947.655907	13.976077
17.256275	941.218631	13.981095
17.546348	963.642105	13.986112
18.024319	959.416407	13.991130
17.523475	956.876485	13.996147
17.555806	946.752333	14.001165
17.601939	935.786063	14.006183
17.680331	955.268005	14.011200
18.286944	951.097015	14.016218
17.828769	944.116726	14.021235
17.758973	939.319715	14.026253
18.085893	944.780984	14.031271
17.422436	948.420106	14.036288
17.735703	939.205392	14.041306
17.369375	943.113146	14.046323
17.615800	931.636539	14.051341
17.636278	934.055635	14.056359
17.702055	932.510483	14.061376
18.097939	952.627279	14.066394
17.626945	939.266387	14.071411
18.176752	940.248552	14.076429
17.826647	941.874286	14.081447
17.553776	963.146421	14.086464
17.741789	964.991617	14.091482
17.690646	951.683447	14.096499
17.961330	945.822748	14.101517
17.914439	965.895241	14.106535
17.946538	969.820209	14.111552
18.277753	969.093765	14.116570
18.187437	971.813389	14.121587
18.043606	956.538947	14.126605
18.224631	950.812422	14.131623
18.115059	944.797591	14.136640
18.176739	961.565181	14.141658
17.883290	947.753592	14.146675
17.918966	956.136474	14.151693
18.043902	961.166286	14.156711
17.940525	958.188137	14.161728
18.269538	957.611527	14.166746
18.037320	961.889149	14.171763
18.068311	954.433138	14.176781
18.262065	967.968212	14.181799
18.209029	957.527929	14.186816
18.369404	951.233702	14.191834
18.403415	955.448434	14.196851
18.369387	965.587278	14.201869
18.504637	954.353183	14.206887
18.329638	959.225033	14.211904
18.546585	963.424690	14.216922
18.491980	967.785236	14.221939
18.461847	952.590410	14.226957
18.356324	963.058506	14.231975
18.259225	962.037680	14.236992
18.397169	952.774490	14.242010
18.243319	950.768218	14.247027
18.352156	971.908505	14.252045
18.510258	957.588637	14.257063
18.182716	965.804145	14.262080
18.649994	964.402429	14.267098
18.159586	951.464018	14.272115
18.348287	953.540733	14.277133
18.278610	961.306741	14.282151
18.116683	973.450473	14.287168
18.564060	956.326120	14.292186
18.463219	958.107069	14.297203
18.484261	981.972902	14.302221
18.655260	1004.499729	14.307239
18.797364	991.164043	14.312256
18.766931	973.874301	14.317274
18.819989	988.415958	14.322291
18.844154	997.992664	14.327309
18.805911	969.916805	14.332327
18.564947	972.790425	14.337344
18.641381	978.355682	14.342362
18.614766	982.359728	14.347379
18.749547	986.808835	14.352397
18.915675	995.691088	14.357415
18.722001	992.858162	14.362432
18.954405	985.107894	14.367450
18.906601	986.491303	14.372467
19.073264	989.784940	14.377485
18.691896	1002.459003	14.382503
18.857996	995.136020	14.387520
18.886453	969.217786	14.392538
18.728444	990.716487	14.397555
18.893971	984.898833	14.402573
18.900488	978.526110	14.407591
18.747549	1003.810509	14.412608
18.884193	980.589050	14.417626
19.018874	975.314353	14.422643
19.141250	976.896943	14.427661
18.910731	1002.491919	14.432679
18.752696	1003.959376	14.437696
18.803992	983.896895	14.442714
19.231196	996.703014	14.447731
19.433782	1012.788191	14.452749
19.382242	1021.106604	14.457767
19.226671	1011.513631	14.462784
19.312017	983.822930	14.467802
19.179701	977.861536	14.472819
19.308028	1005.789230	14.477837
19.483562	998.827882	14.482855
19.323430	991.047941	14.487872
19.595233	964.380994	14.492890
19.383379	978.897342	14.497907
19.493111	978.929068	14.502925
19.717039	975.739387	14.507943
19.523870	976.918037	14.512960
19.719271	967.571936	14.517978
19.701824	967.562195	14.522995
19.616787	968.334392	14.528013
19.733505	973.391838	14.533031
19.786803	969.093734	14.538048
19.457795	966.145687	14.543066
19.742406	976.780070	14.548083
19.874963	974.725087	14.553101
19.738331	940.576903	14.558119
19.284291	944.527588	14.563136
19.592814	972.134007	14.568154
19.742450	964.589996	14.573171
19.529985	965.376658	14.578189
19.407275	948.682854	14.583207
19.583859	967.529156	14.588224
19.763556	974.966829	14.593242
19.338746	965.850846	14.598259
19.267104	958.752455	14.603277
19.172068	967.985671	14.608295
19.270621	975.716998	14.613312
19.718084	981.086232	14.618330
19.812928	964.492153	14.623347
19.266340	968.176025	14.628365
19.711619	986.411261	14.633383
19.559683	1003.803985	14.638400
19.832234	1016.464585	14.643418
19.936055	1005.702162	14.648435
19.684003	988.418056	14.653453
20.075831	994.617148	14.658471
20.025924	1008.426299	14.663488
20.222482	993.184942	14.668506
19.832555	991.426385	14.673523
19.999962	1011.114178	14.678541
20.293087	998.974752	14.683559
20.260721	1000.541587	14.688576
20.151918	1005.464997	14.693594
20.299494	1014.423660	14.698611
19.871062	1003.784128	14.703629
20.027651	1014.060163	14.708647
19.956780	1009.615089	14.713664
19.715278	1028.274420	14.718682
19.923268	1008.456688	14.723699
20.022303	991.565824	14.728717
20.125532	993.805844	14.733735
20.329339	1008.359975	14.738752
20.440307	1014.167114	14.743770
20.284814	1006.684626	14.748787
19.979933	991.391032	14.753805
20.710123	995.285441	14.758823
20.308677	1015.117945	14.763840
20.162596	1015.037063	14.768858
20.657273	998.253873	14.773875
20.136682	994.719624	14.778893
20.271119	1002.240853	14.783911
20.452856	1021.882922	14.788928
20.607772	1007.932535	14.793946
20.280318	1009.637090	14.798963
20.114556	1031.093341	14.803981
20.739317	1033.209691	14.808999
20.703020	1034.998581	14.814016
20.791064	1018.513513	14.819034
20.578891	1014.077619	14.824051
20.742558	1021.594913	14.829069
20.654181	1001.302576	14.834087
20.270996	1004.617807	14.839104
20.510972	1026.176742	14.844122
21.065848	1018.854642	14.849139
20.719873	1006.887145	14.854157
20.557356	1012.593550	14.859175
20.451094	1002.197457	14.864192
20.299066	1022.915785	14.869210
20.805839	1047.060612	14.874227
20.654606	1032.803699	14.879245
20.862759	1014.014023	14.884263
20.955661	1030.628043	14.889280
21.107615	1044.741603	14.894298
21.221537	1035.879872	14.899315
20.655605	1040.829930	14.904333
20.954074	1034.292037	14.909351
21.128710	1023.914946	14.914368
21.042667	1038.316882	14.919386
21.257729	1027.856159	14.924403
20.876327	1023.688719	14.929421
20.835178	1020.087141	14.934439
20.833255	1030.006111	14.939456
20.951008	1020.754186	14.944474
20.750601	1020.473377	14.949491
20.950217	1029.271912	14.954509
21.073370	1032.547559	14.959527
21.170735	1036.665153	14.964544
20.814447	1038.092263	14.969562
21.232731	1012.174751	14.974579
20.726366	1038.055493	14.979597
21.044613	1021.305172	14.984615
20.645583	1025.688311	14.989632
20.808580	1037.087726	14.994650
21.166138	1052.843081	14.999667
20.944667	1055.805105	15.004685
21.644572	1047.290712	15.009703
21.342154	1044.510063	15.014720
21.258753	1043.440031	15.019738
21.545843	1046.817888	15.024755
21.410188	1052.283806	15.029773
21.533775	1058.405530	15.034791
21.431984	1060.350191	15.039808
21.565414	1048.053009	15.044826
21.540662	1037.447702	15.049843
21.660740	1053.983063	15.054861
21.535173	1054.677042	15.059879
21.560359	1054.424487	15.064896
21.283602	1037.930408	15.069914
21.767078	1045.132627	15.074931
21.321024	1043.665944	15.079949
21.560189	1052.755521	15.084967
21.608205	1052.636167	15.089984
21.597748	1051.592259	15.095002
21.736712	1025.496333	15.100019
21.544739	1037.601491	15.105037
21.421939	1050.669197	15.110055
21.663038	1041.855916	15.115072
21.404947	1049.646906	15.120090
21.504577	1057.341786	15.125107
21.718725	1047.629538	15.130125
21.866302	1068.058515	15.135143
21.907754	1074.699797	15.140160
22.013192	1077.736216	15.145178
21.879035	1059.586175	15.150195
22.049610	1082.444135	15.155213
21.841331	1060.636577	15.160231
22.157417	1062.135504	15.165248
22.015277	1056.080943	15.170266
22.353375	1036.972495	15.175283
21.812052	1038.081943	15.180301
22.010655	1033.126404	15.185319
21.861156	1036.311610	15.190336
21.737158	1066.168265	15.195354
22.056233	1054.855207	15.200371
21.929972	1063.607638	15.205389
22.133349	1076.269682	15.210407
22.352553	1059.853915	15.215424
22.093393	1068.943194	15.220442
22.234547	1075.529526	15.225459
22.237813	1084.594439	15.230477
22.149275	1063.271198	15.235495
22.439644	1072.197835	15.240512
22.550607	1060.173679	15.245530
22.651115	1060.486585	15.250547
22.269067	1077.363546	15.255565
22.327662	1085.109501	15.260583
22.528673	1072.046888	15.265600
22.161502	1067.659422	15.270618
22.449324	1053.044768	15.275635
22.204009	1079.705957	15.280653
22.180315	1082.789597	15.285671
22.535644	1055.414470	15.290688
22.517473	1058.411484	15.295706
22.786974	1072.831844	15.300723
22.449715	1065.493903	15.305741
22.322217	1061.465946	15.310759
22.589838	1062.806486	15.315776
22.526489	1071.175095	15.320794
22.624777	1067.524682	15.325811
22.250990	1067.425537	15.330829
22.523128	1060.328443	15.335847
22.563401	1046.455318	15.340864
22.263678	1068.261137	15.345882
22.520727	1073.194762	15.350899
22.581696	1082.760249	15.355917
22.846415	1077.664963	15.360935
23.120766	1094.614332	15.365952
23.097291	1087.489619	15.370970
23.037965	1067.780536	15.375987
23.181486	1072.055333	15.381005
23.220657	1074.507279	15.386023
22.919304	1064.055019	15.391040
22.933876	1057.901644	15.396058
23.046901	1051.356604	15.401075
22.972167	1054.037061	15.406093
23.062277	1054.812693	15.411111
23.254914	1061.448272	15.416128
22.758802	1055.537224	15.421146
22.981303	1049.737584	15.426163
23.048138	1040.540409	15.431181
22.653533	1063.379463	15.436199
22.893879	1078.328926	15.441216
22.853319	1072.559761	15.446234
23.143462	1061.758046	15.451251
23.481693	1081.956668	15.456269
23.197353	1097.337062	15.461287
23.302367	1077.760808	15.466304
23.228794	1081.232223	15.471322
23.289346	1081.234487	15.476339
23.461520	1075.547755	15.481357
23.040574	1088.916178	15.486375
23.490691	1089.960880	15.491392
23.424202	1082.380005	15.496410
23.463217	1082.201622	15.501427
23.422503	1080.168568	15.506445
23.006338	1084.382648	15.511463
23.569371	1069.811848	15.516480
23.142566	1093.968739	15.521498
23.705195	1084.470368	15.526515
23.412079	1079.377524	15.531533
23.417444	1091.316485	15.536551
23.565160	1087.961958	15.541568
23.167558	1095.906505	15.546586
23.550493	1084.372294	15.551603
23.751942	1077.018534	15.556621
23.538685	1095.246809	15.561639
23.920479	1084.804349	15.566656
23.683540	1079.337350	15.571674
23.422279	1096.387730	15.576691
23.736436	1098.264642	15.581709
23.653645	1102.958447	15.586727
24.133980	1110.149702	15.591744
24.332105	1107.516978	15.596762
24.142976	1087.591975	15.601779
23.919745	1072.824708	15.606797
23.800444	1064.022264	15.611815
23.629501	1075.802599	15.616832
23.844577	1084.121465	15.621850
24.019536	1064.657261	15.626867
24.000640	1089.141619	15.631885
23.828645	1087.860197	15.636903
24.265258	1077.828264	15.641920
23.990351	1098.667763	15.646938
23.956437	1104.490712	15.651955
24.229324	1114.740904	15.656973
24.198244	1112.448049	15.661991
24.386396	1092.109599	15.667008
24.027238	1104.246766	15.672026
24.021262	1119.669547	15.677043
24.002490	1115.613570	15.682061
24.300200	1106.412447	15.687079
24.346710	1111.443263	15.692096
24.109324	1110.476409	15.697114
24.318825	1104.942219	15.702131
24.421139	1107.617930	15.707149
24.108247	1121.017922	15.712167
24.694765	1118.657348	15.717184
24.278349	1112.415173	15.722202
24.386670	1098.661236	15.727219
24.083820	1100.669434	15.732237
23.766724	1114.704901	15.737255
23.802749	1116.188811	15.742272
24.056416	1128.162241	15.747290
24.378089	1140.635736	15.752307
24.595945	1123.398571	15.757325
24.641541	1112.293813	15.762343
24.946004	1126.632875	15.767360
24.739044	1136.591897	15.772378
24.943136	1122.688089	15.777395
25.033633	1138.807568	15.782413
24.986586	1126.936605	15.787431
25.088709	1106.644628	15.792448
24.546259	1108.810996	15.797466
24.811834	1124.088636	15.802483
24.798787	1112.631648	15.807501
24.486934	1119.995739	15.812519
24.740029	1123.596993	15.817536
24.820584	1124.196396	15.822554
24.900573	1121.512736	15.827571
24.894458	1129.817306	15.832589
24.757642	1117.923792	15.837607
24.950643	1130.062822	15.842624
25.444288	1129.200206	15.847642
24.952243	1112.658867	15.852659
25.044082	1117.505368	15.857677
24.985296	1136.163762	15.862695
25.082653	1125.642226	15.867712
25.259424	1124.462674	15.872730
25.376793	1133.319338	15.877747
25.422166	1117.773271	15.882765
25.186564	1116.648483	15.887783
25.553243	1122.423248	15.892800
25.434709	1126.792731	15.897818
25.190722	1114.797963	15.902835
25.357581	1115.254789	15.907853
25.354773	1132.886756	15.912871
25.164337	1123.543509	15.917888
25.487131	1120.304693	15.922906
25.272753	1116.014374	15.927923
25.656213	1123.761277	15.932941
25.575185	1130.562258	15.937959
25.600099	1103.004599	15.942976
25.424237	1109.172483	15.947994
25.109174	1129.044193	15.953011
25.397232	1112.168873	15.958029
25.462232	1115.948220	15.963047
25.633657	1121.912593	15.968064
25.654364	1108.057209	15.973082
25.679191	1107.073691	15.978099
25.738647	1122.120002	15.983117
25.278301	1119.034612	15.988135
25.594838	1102.018803	15.993152
25.516518	1115.867211	15.998170
25.624372	1110.149668	16.003187
25.768022	1112.319655	16.008205
25.772535	1115.991802	16.013223
25.727312	1131.303884	16.018240
25.340678	1117.844859	16.023258
25.551593	1141.711053	16.028275
25.773314	1137.098427	16.033293
25.667266	1155.684163	16.038311
26.071591	1151.888790	16.043328
25.777853	1140.723481	16.048346
25.917894	1166.204580	16.053363
25.967995	1160.061824	16.058381
25.948228	1158.785646	16.063399
25.852550	1144.773618	16.068416
26.132226	1145.697019	16.073434
25.877435	1155.168211	16.078451
26.099678	1152.633339	16.083469
26.322200	1168.153514	16.088487
26.432415	1174.151344	16.093504
26.419890	1172.416400	16.098522
26.294183	1158.662017	16.103539
26.240942	1132.280622	16.108557
26.503330	1143.788268	16.113575
26.614239	1165.621817	16.118592
26.406075	1150.002584	16.123610
26.556621	1145.230990	16.128627
26.591943	1143.001549	16.133645
26.457303	1124.303710	16.138663
26.391196	1140.036277	16.143680
26.529263	1143.339987	16.148698
26.493561	1147.092391	16.153715
26.439884	1129.654186	16.158733
26.662309	1144.685495	16.163751
26.928260	1131.043045	16.168768
26.433204	1122.880571	16.173786
26.541280	1142.632485	16.178803
26.581150	1153.265910	16.183821
26.626702	1142.545296	16.188839
26.611162	1158.123005	16.193856
27.100464	1159.705988	16.198874
26.111209	1149.093495	16.203891
26.566063	1158.265081	16.208909
26.840123	1167.063990	16.213927
27.014695	1167.624340	16.218944
27.157210	1156.224565	16.223962
27.181738	1156.969121	16.228979
27.241223	1169.742598	16.233997
27.018833	1160.385224	16.239015
27.386291	1134.399447	16.244032
27.320715	1113.007593	16.249050
26.862379	1135.225156	16.254067
27.240522	1143.068496	16.259085
27.070453	1128.350742	16.264103
26.814491	1104.547845	16.269120
26.934654	1129.563484	16.274138
26.730270	1152.501224	16.279155
27.420000	1155.935177	16.284173
27.206780	1158.489854	16.289191
27.404965	1151.627621	16.294208
27.385551	1167.977546	16.299226
27.348894	1174.770033	16.304243
27.766166	1160.604736	16.309261
27.188893	1134.917267	16.314279
27.366697	1145.236724	16.319296
27.449191	1158.829517	16.324314
27.231103	1166.529625	16.329331
27.462196	1165.560923	16.334349
27.397049	1171.873194	16.339367
27.102659	1167.426537	16.344384
27.903050	1142.738360	16.349402
27.390496	1157.577928	16.354419
27.518834	1149.818206	16.359437
27.331971	1159.587944	16.364455
27.135635	1160.454607	16.369472
27.549129	1144.048562	16.374490
27.390006	1156.709667	16.379507
27.918933	1167.073747	16.384525
27.667684	1156.200349	16.389543
27.359067	1168.531430	16.394560
27.810809	1178.599784	16.399578
27.782672	1197.652994	16.404595
28.046561	1186.819122	16.409613
28.293576	1193.269338	16.414631
27.717715	1182.005379	16.419648
28.126051	1165.133249	16.424666
28.105309	1169.793990	16.429683
28.071073	1162.087007	16.434701
27.974881	1172.107651	16.439719
28.027216	1179.785513	16.444736
28.396826	1164.879548	16.449754
28.358433	1176.212962	16.454771
28.070375	1160.895826	16.459789
28.202030	1168.182713	16.464807
27.960421	1152.897566	16.469824
28.630559	1151.933753	16.474842
28.205158	1174.582735	16.479859
28.254545	1161.876813	16.484877
28.058208	1147.132188	16.489895
27.705314	1153.270894	16.494912
28.325753	1179.500874	16.499930
28.287610	1193.323327	16.504947
28.385054	1186.495832	16.509965
28.149756	1196.693281	16.514983
28.005486	1193.539800	16.520000
28.702275	1173.223463	16.525018
28.435745	1180.722381	16.530035
28.497156	1190.577557	16.535053
28.452755	1186.802601	16.540071
28.184934	1189.567734	16.545088
28.505819	1184.131616	16.550106
28.242541	1209.005582	16.555123
28.504372	1224.548740	16.560141
28.990757	1204.752941	16.565159
28.723605	1200.449867	16.570176
29.146802	1197.384850	16.575194
28.944321	1214.886463	16.580211
28.920937	1202.841788	16.585229
28.951006	1176.075772	16.590247
28.610460	1178.477518	16.595264
29.065398	1194.542145	16.600282
28.943063	1216.137212	16.605299
28.969284	1189.148437	16.610317
28.936069	1189.451561	16.615335
28.972354	1206.472672	16.620352
29.054801	1210.580281	16.625370
28.849968	1201.379588	16.630387
29.084344	1190.343061	16.635405
29.134435	1184.853389	16.640423
28.918012	1206.274862	16.645440
29.320767	1197.862924	16.650458
29.147678	1197.592947	16.655475
29.104610	1181.282384	16.660493
29.211493	1200.934791	16.665511
29.047734	1206.599456	16.670528
29.082287	1190.563389	16.675546
29.359764	1202.792331	16.680563
29.002150	1197.281861	16.685581
29.491301	1188.590064	16.690599
28.989612	1198.430155	16.695616
29.469637	1217.266180	16.700634
29.597606	1216.757324	16.705651
29.617911	1212.113703	16.710669
29.587054	1219.357309	16.715687
29.646355	1226.992715	16.720704
29.772167	1247.912915	16.725722
29.878612	1233.183609	16.730739
29.869767	1209.305272	16.735757
29.782956	1197.465426	16.740775
29.559530	1189.991711	16.745792
29.880043	1210.929477	16.750810
29.834288	1211.753547	16.755827
29.597045	1189.849630	16.760845
29.469645	1208.923489	16.765863
29.691524	1224.786856	16.770880
29.991996	1218.424694	16.775898
29.670878	1212.414210	16.780915
29.825183	1222.022319	16.785933
30.302765	1220.031618	16.790951
29.886900	1227.906728	16.795968
30.038907	1232.713999	16.800986
30.443449	1227.651647	16.806003
30.206738	1224.692035	16.811021
30.202334	1228.175866	16.816039
30.233192	1224.747335	16.821056
30.275967	1216.006384	16.826074
30.212873	1212.833384	16.831091
30.082943	1219.491931	16.836109
30.416798	1218.305602	16.841127
30.046006	1218.739298	16.846144
30.065075	1223.295764	16.851162
29.872100	1218.427901	16.856179
30.170516	1221.234671	16.861197
30.462727	1224.205421	16.866215
30.220834	1257.453968	16.871232
30.601445	1260.614104	16.876250
30.544012	1246.952862	16.881267
30.495012	1237.081272	16.886285
30.539509	1258.865510	16.891303
30.332896	1260.961739	16.896320
30.178695	1242.266595	16.901338
30.331480	1243.984115	16.906355
30.320215	1255.313794	16.911373
30.458593	1233.299820	16.916391
30.265481	1257.313454	16.921408
30.669594	1279.344227	16.926426
30.865483	1277.879188	16.931443
30.703658	1277.107859	16.936461
31.183636	1278.499527	16.941479
31.407936	1269.033927	16.946496
30.970770	1240.362600	16.951514
31.240373	1237.763798	16.956531
30.682329	1253.970399	16.961549
31.087064	1246.386554	16.966567
30.906624	1232.401048	16.971584
31.202618	1230.597501	16.976602
31.427963	1244.718012	16.981619
30.958764	1257.573222	16.986637
31.221141	1233.107144	16.991655
30.841495	1226.245604	16.996672
31.374678	1255.666253	17.001690
31.501087	1272.816211	17.006707
31.457014	1275.870489	17.011725
31.373094	1239.258085	17.016743
31.279707	1227.503534	17.021760
31.422912	1254.251576	17.026778
31.809800	1252.046876	17.031795
31.455681	1249.197880	17.036813
31.109205	1241.459896	17.041831
31.578929	1244.690224	17.046848
31.442218	1257.478287	17.051866
31.477886	1284.356035	17.056883
31.358936	1267.367530	17.061901
31.525792	1255.094375	17.066919
31.781039	1273.293362	17.071936
31.579213	1272.273978	17.076954
31.835883	1267.926734	17.081971
31.570609	1280.206855	17.086989
31.899581	1269.218305	17.092007
31.989011	1252.551597	17.097024
31.646991	1259.726789	17.102042
31.397536	1271.613435	17.107059
31.534660	1267.112660	17.112077
31.667763	1273.484415	17.117095
31.555306	1273.737265	17.122112
31.988743	1280.017768	17.127130
31.874449	1298.984578	17.132147
31.662498	1290.368042	17.137165
32.193650	1274.442396	17.142183
32.567177	1296.945069	17.147200
32.149994	1299.799849	17.152218
32.325457	1289.779839	17.157235
32.217768	1282.808682	17.162253
32.740704	1293.989889	17.167271
32.910333	1303.005202	17.172288
32.420894	1286.304028	17.177306
32.409359	1262.359041	17.182323
32.628451	1266.203491	17.187341
32.753430	1267.361470	17.192359
32.358356	1273.356934	17.197376
32.463041	1264.481934	17.202394
32.562738	1245.642294	17.207411
32.421229	1260.919937	17.212429
32.418412	1242.245632	17.217447
32.287719	1267.897890	17.222464
32.126583	1289.019859	17.227482
32.589322	1269.703068	17.232499
32.406029	1277.242006	17.237517
32.618509	1275.173678	17.242535
32.529521	1291.799344	17.247552
32.733721	1287.940870	17.252570
32.986480	1271.043261	17.257587
32.646704	1290.425088	17.262605
32.844076	1278.752636	17.267623
33.009502	1293.816932	17.272640
32.862390	1279.351871	17.277658
33.237685	1262.220588	17.282675
33.112685	1274.466995	17.287693
33.077368	1288.149730	17.292711
33.174178	1284.197513	17.297728
32.983189	1276.316029	17.302746
33.177175	1261.489867	17.307763
33.133684	1271.944086	17.312781
33.265347	1286.233329	17.317799
32.953206	1283.497736	17.322816
33.096723	1270.587236	17.327834
33.298767	1278.278686	17.332851
33.181097	1305.546293	17.337869
33.294800	1308.178631	17.342887
33.433482	1308.328578	17.347904
33.612176	1317.946395	17.352922
33.260012	1313.085324	17.357939
33.543295	1327.998613	17.362957
33.256060	1318.429763	17.367975
33.649995	1295.995110	17.372992
33.410915	1304.266537	17.378010
33.780035	1309.873391	17.383027
33.497161	1316.317545	17.388045
33.674320	1308.826678	17.393063
33.757875	1308.072953	17.398080
33.760119	1304.988622	17.403098
33.583584	1296.551717	17.408115
33.642534	1315.236435	17.413133
33.653368	1317.933500	17.418151
33.900603	1304.627966	17.423168
33.573819	1289.030160	17.428186
33.900435	1310.292667	17.433203
33.855326	1341.358587	17.438221
34.129479	1342.705257	17.443239
34.287371	1342.425454	17.448256
34.329162	1346.328450	17.453274
34.254289	1334.238255	17.458291
34.406302	1332.988977	17.463309
34.319501	1332.599152	17.468327
34.072349	1314.546990	17.473344
33.964557	1303.269454	17.478362
34.279809	1318.810966	17.483379
34.200726	1337.313549	17.488397
34.542474	1334.056501	17.493415
34.636085	1339.414670	17.498432
34.392965	1347.750257	17.503450
34.585876	1332.007092	17.508467
34.413988	1329.271930	17.513485
34.438103	1326.821530	17.518503
34.688440	1331.438312	17.523520
34.321609	1322.034251	17.528538
34.353146	1339.879432	17.533555
34.484807	1345.252471	17.538573
34.540622	1325.675568	17.543591
34.566551	1330.035013	17.548608
34.621162	1327.576523	17.553626
34.905914	1318.281964	17.558643
34.747213	1326.789374	17.563661
34.541740	1352.320008	17.568679
34.582491	1340.593586	17.573696
34.502508	1335.926450	17.578714
34.785492	1359.260919	17.583731
34.882209	1378.391338	17.588749
34.872968	1376.139804	17.593767
34.923226	1361.478701	17.598784
34.631192	1359.496784	17.603802
34.913069	1365.390749	17.608819
35.232688	1358.069776	17.613837
34.878620	1370.107712	17.618855
35.219153	1384.304572	17.623872
34.937136	1372.878847	17.628890
35.294797	1367.816128	17.633907
35.620604	1383.299183	17.638925
35.641908	1397.215615	17.643943
35.382479	1386.930181	17.648960
35.288755	1386.833067	17.653978
35.514716	1371.674521	17.658995
36.042456	1386.107216	17.664013
35.516978	1383.213694	17.669031
35.856374	1367.913600	17.674048
35.230654	1358.874469	17.679066
35.727483	1356.418962	17.684083
35.786529	1386.111280	17.689101
35.513962	1397.961597	17.694119
35.720794	1371.641315	17.699136
35.672781	1390.539031	17.704154
35.941380	1387.880443	17.709171
35.642554	1400.965433	17.714189
35.556129	1384.712004	17.719207
36.086808	1388.000877	17.724224
35.915207	1375.588324	17.729242
35.783211	1379.635965	17.734259
35.986019	1383.308078	17.739277
36.051732	1371.993357	17.744295
35.665809	1370.484133	17.749312
35.911969	1389.716220	17.754330
36.180121	1396.337891	17.759347
36.077828	1403.808892	17.764365
35.952812	1407.474174	17.769383
36.391317	1411.827753	17.774400
36.170867	1399.193285	17.779418
36.602090	1404.067633	17.784435
36.662128	1430.664410	17.789453
36.456139	1407.905894	17.794471
36.557484	1401.547927	17.799488
36.609426	1410.461321	17.804506
36.566704	1399.996694	17.809523
36.610236	1402.854376	17.814541
36.735771	1418.786611	17.819559
36.854292	1413.803641	17.824576
36.757916	1398.925942	17.829594
36.699096	1409.985014	17.834611
36.777303	1414.787318	17.839629
36.887634	1411.699864	17.844647
36.943352	1395.775511	17.849664
36.944022	1409.094515	17.854682
36.939671	1408.036978	17.859699
37.193581	1413.936666	17.864717
36.940088	1409.309399	17.869735
37.159966	1387.439575	17.874752
37.378409	1398.010893	17.879770
37.233854	1394.959462	17.884787
37.115977	1381.116005	17.889805
36.970035	1370.288817	17.894823
37.206033	1363.502407	17.899840
36.908389	1393.908751	17.904858
36.937461	1420.270032	17.909875
36.863923	1401.694502	17.914893
36.658503	1392.094077	17.919911
37.105368	1388.881543	17.924928
37.238912	1407.971669	17.929946
36.903513	1412.426469	17.934963
37.102992	1420.188774	17.939981
37.334452	1408.171985	17.944999
37.653169	1420.384840	17.950016
37.768554	1440.226264	17.955034
37.783747	1426.442255	17.960051
37.911651	1441.017732	17.965069
37.496968	1442.293834	17.970087
37.582853	1410.293266	17.975104
37.514843	1422.850676	17.980122
37.585657	1439.491719	17.985139
38.044860	1422.368632	17.990157
37.559447	1414.519395	17.995175
38.115504	1401.350891	18.000192
37.829215	1431.117879	18.005210
38.040212	1437.043364	18.010227
37.770320	1411.699820	18.015245
37.624742	1405.417884	18.020263
38.072416	1412.452514	18.025280
37.942543	1432.397337	18.030298
38.198741	1444.391263	18.035315
38.454461	1432.895427	18.040333
38.403968	1451.090144	18.045351
38.500305	1444.673649	18.050368
38.633928	1442.618822	18.055386
38.478991	1421.841170	18.060403
38.520771	1390.713484	18.065421
38.424778	1406.161172	18.070439
38.812720	1424.367441	18.075456
38.545681	1411.266851	18.080474
38.180309	1413.021209	18.085491
38.494398	1399.430985	18.090509
38.444693	1426.627255	18.095527
38.746358	1443.013864	18.100544
38.817050	1448.053292	18.105562
38.916274	1440.767618	18.110579
38.828107	1441.488202	18.115597
38.871098	1444.848724	18.120615
39.015418	1439.331581	18.125632
39.087316	1431.391519	18.130650
38.716317	1434.979077	18.135667
39.054963	1449.179950	18.140685
39.039152	1460.705862	18.145703
39.176187	1445.835795	18.150720
39.202026	1441.091507	18.155738
38.761095	1453.458754	18.160755
38.857291	1433.874153	18.165773
38.829508	1445.698423	18.170791
38.592465	1432.709859	18.175808
38.832059	1432.267669	18.180826
39.120906	1457.243571	18.185843
39.330405	1465.440563	18.190861
39.249440	1469.905685	18.195879
39.538458	1463.081244	18.200896
39.790422	1480.219446	18.205914
39.572594	1463.924176	18.210931
39.580204	1457.168972	18.215949
39.762127	1479.111975	18.220967
39.978127	1478.416063	18.225984
39.906303	1456.922224	18.231002
39.651831	1441.665383	18.236019
39.676753	1446.594487	18.241037
39.478594	1469.318826	18.246055
39.531114	1466.206769	18.251072
40.019324	1451.659682	18.256090
39.618400	1460.438343	18.261107
40.034234	1471.754677	18.266125
39.943974	1480.425135	18.271143
39.983880	1474.442073	18.276160
40.015029	1460.698005	18.281178
39.898789	1457.116309	18.286195
40.067721	1468.154614	18.291213
39.977145	1473.161167	18.296231
40.129103	1448.425358	18.301248
39.974873	1451.107509	18.306266
40.182845	1463.213235	18.311283
40.306636	1471.277772	18.316301
40.088375	1463.920563	18.321319
40.309000	1447.934858	18.326336
40.524682	1473.847475	18.331354
40.669475	1487.051511	18.336371
40.741132	1489.036445	18.341389
40.520718	1480.161217	18.346407
40.375485	1459.333200	18.351424
40.939958	1464.652669	18.356442
40.417061	1471.844368	18.361459
40.709123	1468.695087	18.366477
40.441603	1494.871505	18.371495
40.611565	1495.429284	18.376512
40.714285	1484.440182	18.381530
40.763332	1498.062127	18.386547
41.025717	1479.341050	18.391565
40.730378	1470.879104	18.396583
41.104601	1470.054805	18.401600
41.165709	1477.827409	18.406618
41.029464	1467.913504	18.411635
40.970412	1478.684737	18.416653
40.948251	1488.999290	18.421671
40.789262	1486.145556	18.426688
41.365760	1470.379304	18.431706
41.385798	1500.552005	18.436723
41.481847	1509.231152	18.441741
41.207215	1494.883690	18.446759
41.318818	1489.872023	18.451776
41.575769	1488.307623	18.456794
41.652271	1495.697559	18.461811
41.565806	1514.228931	18.466829
41.519719	1513.319788	18.471847
41.676650	1503.354462	18.476864
41.722260	1503.704101	18.481882
41.488812	1498.964167	18.486899
41.642025	1491.762932	18.491917
41.322227	1511.437439	18.496935
41.285883	1511.062298	18.501952
41.835091	1492.039632	18.506970
41.562188	1494.506806	18.511987
41.417818	1500.089062	18.517005
41.686221	1541.073250	18.522023
42.034049	1537.230735	18.527040
42.208029	1519.276516	18.532058
42.159244	1535.518819	18.537075
42.263133	1540.604454	18.542093
42.395267	1541.128338	18.547111
42.254805	1524.539373	18.552128
42.596487	1518.539194	18.557146
42.444336	1534.635718	18.562163
42.642714	1536.430562	18.567181
42.721418	1532.200429	18.572199
42.318219	1491.207778	18.577216
42.614306	1499.488293	18.582234
42.398248	1507.906190	18.587251
42.442400	1509.509930	18.592269
42.583040	1523.271648	18.597287
42.498160	1526.019795	18.602304
42.602847	1529.896208	18.607322
42.568633	1515.777541	18.612339
42.765714	1528.776067	18.617357
42.694621	1534.849562	18.622375
42.182848	1527.728186	18.627392
42.581671	1510.027704	18.632410
42.515955	1519.104964	18.637427
42.518354	1535.220821	18.642445
42.883766	1547.433836	18.647463
42.737010	1540.060838	18.652480
43.145048	1560.016325	18.657498
43.168874	1563.421764	18.662515
43.092784	1539.467822	18.667533
43.288168	1543.888184	18.672551
42.885642	1551.897545	18.677568
43.380070	1551.521091	18.682586
43.108415	1557.828974	18.687603
43.369471	1545.587057	18.692621
43.411826	1546.089466	18.697639
43.409518	1572.205559	18.702656
43.386408	1551.458198	18.707674
43.064050	1546.649102	18.712691
43.172821	1569.189728	18.717709
43.449383	1573.920926	18.722727
43.423453	1575.289260	18.727744
43.543405	1582.163407	18.732762
43.714161	1571.327925	18.737779
43.972307	1577.197357	18.742797
43.459666	1567.880906	18.747815
43.650789	1548.806343	18.752832
43.882949	1579.074334	18.757850
44.092007	1602.286381	18.762867
44.407396	1595.983987	18.767885
44.463085	1582.337209	18.772903
44.138399	1580.415271	18.777920
44.302365	1572.539235	18.782938
44.134833	1574.659848	18.787955
44.217364	1561.445764	18.792973
44.283596	1581.849510	18.797991
44.131532	1573.277433	18.803008
44.548927	1570.138614	18.808026
44.362443	1599.699123	18.813043
44.513959	1590.614566	18.818061
44.387073	1595.191916	18.823079
44.335885	1608.384259	18.828096
44.747037	1585.710956	18.833114
44.705609	1594.630047	18.838131
44.563215	1609.321792	18.843149
44.700385	1602.856761	18.848167
44.545611	1595.203821	18.853184
44.953175	1582.747252	18.858202
44.716269	1594.071761	18.863219
44.549656	1603.084166	18.868237
44.750899	1591.937988	18.873255
44.585673	1602.353014	18.878272
44.867970	1610.823723	18.883290
45.119570	1618.649252	18.888307
45.152523	1622.563226	18.893325
45.142930	1624.668865	18.898343
45.148407	1637.076442	18.903360
45.452186	1615.230905	18.908378
45.484541	1617.503000	18.913395
45.398601	1628.865074	18.918413
45.728654	1607.038824	18.923431
45.394603	1616.753369	18.928448
45.368013	1629.635037	18.933466
45.421642	1616.880409	18.938483
45.627386	1602.421089	18.943501
45.676692	1616.289205	18.948519
45.637348	1629.378351	18.953536
46.082169	1614.323232	18.958554
45.703570	1615.063674	18.963571
45.750142	1614.913853	18.968589
46.061662	1600.138989	18.973607
45.598329	1606.911840	18.978624
46.004232	1623.420857	18.983642
45.849010	1612.941414	18.988659
45.706169	1599.952590	18.993677
46.447891	1591.003719	18.998695
46.390628	1617.540694	19.003712
46.454201	1602.146705	19.008730
46.346239	1614.373249	19.013747
46.024144	1624.451002	19.018765
46.335690	1590.202308	19.023783
46.121886	1602.845067	19.028800
46.219818	1613.773484	19.033818
46.219299	1607.227781	19.038835
45.973813	1596.501903	19.043853
45.981381	1591.403578	19.048871
45.857607	1621.852886	19.053888
46.152201	1636.547824	19.058906
46.256434	1646.213775	19.063923
46.310915	1637.265771	19.068941
46.933972	1640.837306	19.073959
46.704761	1663.758462	19.078976
47.406735	1673.937141	19.083994
47.221190	1653.321089	19.089011
46.993916	1629.336489	19.094029
46.998823	1610.108901	19.099047
46.636634	1626.447962	19.104064
47.199535	1633.861897	19.109082
47.245006	1658.639223	19.114099
47.207691	1653.997117	19.119117
47.525783	1642.332879	19.124135
47.491235	1645.923142	19.129152
47.284085	1644.977136	19.134170
47.414538	1638.495191	19.139187
47.516000	1639.935078	19.144205
47.913064	1637.662614	19.149223
47.375419	1620.010874	19.154240
47.813470	1602.156099	19.159258
47.592984	1630.337442	19.164275
47.456322	1624.871192	19.169293
47.726271	1624.655526	19.174311
47.392472	1640.991978	19.179328
47.616866	1652.765879	19.184346
47.702401	1672.600730	19.189363
47.368234	1659.544182	19.194381
47.778123	1647.397938	19.199399
47.941206	1665.718016	19.204416
47.971818	1652.150993	19.209434
48.033116	1645.940163	19.214451
47.836832	1642.868003	19.219469
47.938715	1654.821369	19.224487
48.027775	1684.609089	19.229504
48.188220	1676.338389	19.234522
48.523282	1665.730754	19.239539
48.036218	1684.870249	19.244557
48.431092	1695.158045	19.249575
48.180850	1673.788837	19.254592
48.497096	1676.395052	19.259610
48.516004	1680.881814	19.264627
48.432913	1684.737732	19.269645
48.305927	1678.947981	19.274663
48.728455	1694.176147	19.279680
48.564243	1685.523452	19.284698
48.639611	1669.145267	19.289715
48.794436	1668.115728	19.294733
48.606757	1680.362583	19.299751
48.469921	1689.815892	19.304768
48.844134	1695.723068	19.309786
49.033704	1705.458108	19.314803
48.974797	1707.401470	19.319821
48.939110	1684.996997	19.324839
49.314363	1701.119610	19.329856
49.539703	1713.374799	19.334874
49.221553	1700.579688	19.339891
48.924939	1690.522490	19.344909
49.215077	1700.824744	19.349927
49.296434	1717.432858	19.354944
49.263656	1707.190839	19.359962
49.596194	1683.520943	19.364979
49.210133	1697.467966	19.369997
49.392372	1702.378832	19.375015
49.372169	1715.142316	19.380032
49.857297	1708.174655	19.385050
50.136379	1700.499761	19.390067
49.708485	1711.233998	19.395085
49.946076	1721.177603	19.400103
49.947685	1718.417734	19.405120
50.122124	1724.314538	19.410138
50.334163	1709.565553	19.415155
49.846996	1682.652477	19.420173
49.997944	1687.179712	19.425191
50.014821	1710.674515	19.430208
49.966724	1722.366950	19.435226
50.313724	1708.015264	19.440243
50.211065	1702.326581	19.445261
50.193808	1698.835929	19.450279
50.172655	1696.789227	19.455296
50.062780	1702.351981	19.460314
50.092561	1713.941795	19.465331
49.910899	1734.277184	19.470349
50.382407	1728.191998	19.475367
50.480381	1732.687654	19.480384
50.573884	1751.923578	19.485402
50.793699	1733.041544	19.490419
50.531733	1736.123359	19.495437
50.815899	1749.105320	19.500455
50.894867	1741.294119	19.505472
50.784302	1720.818015	19.510490
50.957584	1728.150446	19.515507
50.807886	1744.662842	19.520525
51.040391	1755.624131	19.525543
51.235429	1742.102087	19.530560
51.200822	1738.133977	19.535578
51.301723	1741.382949	19.540595
51.141925	1759.175805	19.545613
51.354011	1762.840770	19.550631
51.275104	1776.286114	19.555648
51.422094	1763.233513	19.560666
51.576545	1767.235495	19.565683
51.529826	1762.819668	19.570701
51.454726	1771.134215	19.575719
51.868214	1767.252354	19.580736
51.561595	1765.337641	19.585754
51.578280	1767.138034	19.590771
51.242641	1770.956589	19.595789
51.564110	1770.118359	19.600807
51.783801	1763.216185	19.605824
51.709346	1762.270188	19.610842
51.874753	1771.657759	19.615859
51.902248	1794.359757	19.620877
52.032137	1781.728090	19.625895
51.903523	1777.445060	19.630912
52.624972	1787.145005	19.635930
52.850948	1793.345756	19.640947
52.322664	1777.417925	19.645965
52.294023	1766.959478	19.650983
52.648613	1778.713930	19.656000
52.361011	1758.179647	19.661018
52.366489	1763.576540	19.666035
52.629822	1794.428270	19.671053
52.666591	1795.750640	19.676071
52.989173	1782.078769	19.681088
52.625125	1772.538267	19.686106
52.682372	1788.398625	19.691123
52.507240	1774.937230	19.696141
52.422298	1787.010728	19.701159
52.757686	1795.039191	19.706176
52.590155	1783.125633	19.711194
52.863060	1767.291652	19.716211
52.647866	1789.356815	19.721229
52.843831	1794.188391	19.726247
53.266062	1802.236064	19.731264
52.889466	1801.191795	19.736282
52.872732	1817.939136	19.741299
52.834267	1817.586380	19.746317
53.126307	1811.954259	19.751335
53.303554	1806.590764	19.756352
53.023126	1824.255234	19.761370
53.357551	1842.348921	19.766387
53.328530	1843.300155	19.771405
53.159383	1820.768354	19.776423
53.486228	1839.193737	19.781440
53.575778	1846.897373	19.786458
53.856305	1831.307984	19.791475
53.756687	1835.984029	19.796493
53.837137	1834.213177	19.801511
54.041767	1844.080928	19.806528
54.506861	1854.105112	19.811546
55.006119	1848.374476	19.816563
54.637058	1842.598785	19.821581
54.284559	1826.387476	19.826599
54.567075	1832.003029	19.831616
54.177042	1826.139784	19.836634
54.245980	1816.321446	19.841651
54.611620	1818.667703	19.846669
53.705296	1832.554294	19.851687
54.350872	1822.440801	19.856704
53.947660	1836.865296	19.861722
54.434745	1838.742068	19.866739
54.581996	1847.283345	19.871757
54.565175	1853.966479	19.876775
54.918328	1861.532978	19.881792
54.865043	1852.088289	19.886810
54.816747	1832.852484	19.891827
54.866736	1857.162449	19.896845
54.608295	1869.550256	19.901863
55.010149	1852.079151	19.906880
54.727011	1849.948187	19.911898
55.124528	1854.661945	19.916915
55.208534	1888.292862	19.921933
55.488485	1900.663660	19.926951
55.670954	1871.459701	19.931968
55.588431	1873.175733	19.936986
55.309277	1867.235992	19.942003
55.668530	1870.660859	19.947021
55.567953	1843.649075	19.952039
55.790820	1852.972783	19.957056
55.116157	1846.282228	19.962074
55.890084	1848.187473	19.967091
55.538341	1876.393319	19.972109
55.457977	1895.229596	19.977127
55.611665	1876.814623	19.982144
55.391370	1864.542665	19.987162
55.776681	1866.723113	19.992179
55.967855	1883.917671	19.997197
56.009741	1889.596233	20.002215
55.813747	1873.323782	20.007232
55.792930	1883.830074	20.012250
56.189697	1895.101754	20.017267
56.231757	1897.967645	20.022285
56.029893	1899.511706	20.027303
56.439963	1913.253067	20.032320
56.202073	1898.641035	20.037338
56.123523	1882.546471	20.042355
56.200436	1900.795457	20.047373
56.212164	1925.083117	20.052391
56.879894	1924.434267	20.057408
56.841991	1918.766883	20.062426
56.620164	1918.373966	20.067443
57.133809	1929.091520	20.072461
57.095666	1933.347868	20.077479
57.456263	1911.479826	20.082496
57.062957	1920.125624	20.087514
57.367513	1918.801890	20.092531
57.313293	1937.219902	20.097549
57.056265	1933.121009	20.102567
57.444066	1900.625516	20.107584
57.472731	1910.085562	20.112602
57.547123	1917.816242	20.117619
57.671718	1925.319676	20.122637
57.144490	1910.318618	20.127655
57.256117	1892.540869	20.132672
57.293495	1902.500456	20.137690
57.321499	1925.389437	20.142707
57.234894	1933.925812	20.147725
57.256754	1918.008972	20.152743
57.463531	1913.158079	20.157760
57.535647	1940.588232	20.162778
57.815220	1961.504764	20.167795
58.062610	1946.741050	20.172813
57.899233	1943.500627	20.177831
58.077589	1931.048589	20.182848
58.298357	1949.612674	20.187866
58.095877	1951.767257	20.192883
58.489942	1933.364355	20.197901
57.997169	1924.147432	20.202919
58.219573	1943.100436	20.207936
58.225435	1960.025070	20.212954
58.440956	1956.905757	20.217971
58.862265	1964.459766	20.222989
58.823234	1968.467598	20.228007
59.045063	1950.692039	20.233024
59.008611	1959.076664	20.238042
58.747047	1947.189341	20.243059
58.842554	1944.915986	20.248077
58.728853	1959.135205	20.253095
59.101585	1967.002893	20.258112
58.651300	1983.905114	20.263130
59.031698	1975.695624	20.268147
59.072654	1970.357841	20.273165
58.886121	1962.368887	20.278183
59.322236	1967.887174	20.283200
58.839816	1975.482969	20.288218
58.622656	1974.067818	20.293235
59.304424	1968.096684	20.298253
59.399230	1991.420900	20.303271
59.725051	1996.122933	20.308288
59.271730	1987.031613	20.313306
59.259075	1979.752854	20.318323
59.687040	1973.721413	20.323341
59.331292	1989.183286	20.328359
59.626486	1994.402784	20.333376
59.418370	1998.721188	20.338394
59.588502	1989.490433	20.343411
59.543015	2013.477018	20.348429
59.733053	2030.806352	20.353447
60.383695	2019.106655	20.358464
60.397752	2013.098919	20.363482
60.398581	2003.554562	20.368499
60.265215	2006.143219	20.373517
59.947054	2017.231710	20.378535
59.865772	2014.195185	20.383552
60.379723	2019.047009	20.388570
60.585741	2034.153153	20.393587
60.725018	2041.084145	20.398605
60.534454	2033.146205	20.403623
60.848177	2044.389896	20.408640
60.955808	2035.538074	20.413658
61.014391	2023.569348	20.418675
61.039398	2032.518063	20.423693
60.976012	2054.306205	20.428711
61.189963	2040.187574	20.433728
61.188639	2029.123757	20.438746
60.936518	2026.824188	20.443763
61.233215	2027.857411	20.448781
60.927493	2046.226383	20.453799
60.983177	2023.672187	20.458816
61.271873	2007.194327	20.463834
60.853427	2038.303574	20.468851
61.377534	2046.253946	20.473869
61.181599	2054.738389	20.478887
61.423997	2043.721476	20.483904
61.465370	2055.279717	20.488922
61.560240	2071.179713	20.493939
61.619981	2069.564001	20.498957
61.897060	2090.446481	20.503975
61.635524	2095.399021	20.508992
61.910743	2082.134541	20.514010
61.872402	2095.293985	20.519027
62.252618	2086.733741	20.524045
62.331062	2097.888126	20.529063
62.418693	2076.959480	20.534080
62.588357	2089.154695	20.539098
62.411210	2079.047878	20.544115
62.857203	2075.030869	20.549133
62.594349	2096.635044	20.554151
62.463895	2083.337617	20.559168
62.848856	2084.798206	20.564186
62.717990	2100.165165	20.569203
62.673243	2083.834335	20.574221
62.407118	2092.869867	20.579239
62.059541	2079.691575	20.584256
62.894136	2094.244088	20.589274
63.134913	2113.731080	20.594291
63.019378	2093.441978	20.599309
63.526218	2106.852127	20.604327
63.110657	2127.527814	20.609344
63.591141	2112.997619	20.614362
63.549942	2102.124361	20.619379
63.620910	2108.673533	20.624397
63.481482	2108.015268	20.629415
63.477069	2100.358583	20.634432
63.592939	2095.277424	20.639450
63.457513	2101.301351	20.644467
63.469476	2113.444411	20.649485
63.322892	2101.961219	20.654503
63.431556	2093.776986	20.659520
63.690992	2092.958143	20.664538
63.570762	2105.912269	20.669555
63.814816	2105.777538	20.674573
63.713682	2109.555259	20.679591
64.118993	2133.083355	20.684608
64.275854	2119.749341	20.689626
64.064064	2133.131146	20.694643
64.344271	2142.269995	20.699661
64.299559	2144.686869	20.704679
64.129002	2123.636582	20.709696
64.217253	2121.844727	20.714714
64.139014	2146.060316	20.719731
64.226522	2147.307218	20.724749
64.409675	2153.089480	20.729767
64.465451	2156.846597	20.734784
64.557189	2161.879930	20.739802
64.809381	2172.360495	20.744819
64.866269	2153.400852	20.749837
64.997210	2145.880213	20.754855
65.036200	2156.587992	20.759872
65.316971	2166.787108	20.764890
64.950450	2164.774780	20.769907
65.513384	2171.276733	20.774925
65.548030	2199.082865	20.779943
65.518309	2186.113623	20.784960
65.870379	2184.203475	20.789978
65.553343	2174.131717	20.794995
65.572330	2142.173249	20.800013
65.604608	2160.183211	20.805031
65.820752	2182.582019	20.810048
65.825392	2191.481150	20.815066
65.819047	2191.213417	20.820083
65.852268	2168.598066	20.825101
65.684723	2177.397120	20.830119
65.811825	2192.902910	20.835136
65.987957	2184.470120	20.840154
65.802628	2178.788228	20.845171
66.255233	2166.358188	20.850189
66.172430	2196.213878	20.855207
66.466797	2206.847116	20.860224
66.339341	2205.572506	20.865242
66.058689	2212.391306	20.870259
66.496976	2207.635703	20.875277
66.427920	2219.848426	20.880295
66.422327	2204.419896	20.885312
66.642418	2194.391234	20.890330
66.363887	2201.182222	20.895347
66.714096	2216.432800	20.900365
66.815910	2234.565292	20.905383
67.024114	2239.360249	20.910400
67.056135	2215.376954	20.915418
66.916102	2218.817784	20.920435
67.200740	2241.326599	20.925453
67.218469	2240.909439	20.930471
67.269084	2236.235996	20.935488
67.465888	2215.603634	20.940506
67.358958	2238.038688	20.945523
67.747614	2252.081973	20.950541
67.840515	2250.258533	20.955559
67.981765	2262.813246	20.960576
68.058918	2256.808668	20.965594
68.101449	2240.800690	20.970611
68.250043	2223.108560	20.975629
68.118681	2223.606632	20.980647
67.867994	2218.798862	20.985664
68.262918	2202.314753	20.990682
67.835786	2217.560835	20.995699
68.126823	2219.541400	21.000717
68.321580	2215.076978	21.005735
68.227190	2249.103850	21.010752
68.391504	2262.085583	21.015770
68.402377	2256.123842	21.020787
68.243556	2244.691080	21.025805
68.567465	2264.743071	21.030823
68.443104	2270.886278	21.035840
68.444454	2257.364592	21.040858
68.532790	2260.227922	21.045875
68.502432	2265.749201	21.050893
68.899450	2267.446162	21.055911
68.827573	2278.515497	21.060928
69.159800	2264.615954	21.065946
68.980295	2262.212829	21.070963
69.093058	2277.779627	21.075981
69.163288	2269.198669	21.080999
68.511604	2271.583995	21.086016
69.361066	2273.220953	21.091034
69.205765	2300.110292	21.096051
69.437507	2293.784534	21.101069
69.891055	2287.589027	21.106087
69.582879	2296.587540	21.111104
69.687415	2287.652732	21.116122
69.736327	2296.075788	21.121139
69.628967	2294.941429	21.126157
69.916007	2295.016880	21.131175
69.630464	2318.159701	21.136192
70.324907	2319.820510	21.141210
70.419486	2332.346187	21.146227
70.398731	2326.504193	21.151245
70.630063	2321.440094	21.156263
70.742813	2327.148735	21.161280
70.924063	2307.462661	21.166298
70.644526	2311.623986	21.171315
70.564809	2320.231473	21.176333
71.016327	2300.544440	21.181351
70.927455	2316.011745	21.186368
70.719945	2303.775898	21.191386
70.621384	2319.900997	21.196403
70.989006	2312.287830	21.201421
71.064630	2302.228451	21.206439
71.133069	2304.009629	21.211456
70.963096	2323.172800	21.216474
71.363929	2319.416102	21.221491
70.976848	2296.911445	21.226509
71.224264	2315.917068	21.231527
71.335269	2347.532363	21.236544
71.522495	2338.870823	21.241562
71.706139	2332.766741	21.246579
71.735885	2344.737093	21.251597
71.724956	2345.677200	21.256615
71.598293	2347.655753	21.261632
71.771116	2331.179375	21.266650
71.962377	2343.810915	21.271667
71.606626	2341.074166	21.276685
71.986997	2355.576517	21.281703
72.206194	2365.396240	21.286720
72.333629	2380.723749	21.291738
72.249513	2365.401423	21.296755
72.187938	2352.892250	21.301773
72.440625	2353.397522	21.306791
72.378328	2357.915811	21.311808
72.688523	2353.508246	21.316826
72.772106	2368.674906	21.321843
72.811213	2364.867949	21.326861
72.923870	2351.279764	21.331879
72.584810	2366.591840	21.336896
72.811706	2350.406653	21.341914
72.753190	2356.844870	21.346931
72.941778	2382.131518	21.351949
73.387093	2386.830853	21.356967
72.869935	2378.801548	21.361984
72.957123	2383.407724	21.367002
73.069670	2405.360862	21.372019
73.088565	2393.936412	21.377037
73.191509	2384.868171	21.382055
73.193097	2412.413954	21.387072
73.157590	2409.165488	21.392090
73.387921	2415.820130	21.397107
73.473473	2426.411464	21.402125
73.842107	2433.527828	21.407143
74.036591	2433.629793	21.412160
74.639719	2440.465915	21.417178
74.542808	2434.648470	21.422195
74.539742	2417.938703	21.427213
74.809030	2393.615084	21.432231
74.685940	2385.396662	21.437248
74.518512	2384.126181	21.442266
74.706225	2393.215417	21.447283
74.667168	2407.455093	21.452301
75.158836	2387.181486	21.457319
74.893615	2387.488528	21.462336
74.868900	2406.766361	21.467354
75.010479	2415.007661	21.472371
74.732567	2394.390030	21.477389
74.835456	2387.636779	21.482407
74.919847	2411.460027	21.487424
74.627229	2416.948528	21.492442
74.818114	2423.143427	21.497459
74.645093	2450.743325	21.502477
74.844316	2425.182218	21.507495
74.903216	2448.750722	21.512512
75.000718	2460.675722	21.517530
75.109033	2480.438081	21.522547
75.044999	2479.300681	21.527565
75.260069	2481.677632	21.532583
75.426435	2496.978944	21.537600
75.622779	2496.816077	21.542618
75.932558	2499.420847	21.547635
76.233282	2516.064334	21.552653
76.515212	2497.128783	21.557671
76.700815	2497.307796	21.562688
76.583615	2501.515170	21.567706
76.690658	2488.150395	21.572723
76.505863	2476.860706	21.577741
77.134002	2456.330636	21.582759
76.822862	2479.679867	21.587776
76.464570	2476.633522	21.592794
76.813809	2473.630079	21.597811
76.675874	2479.297143	21.602829
76.714126	2462.446269	21.607847
76.839112	2483.082708	21.612864
77.097275	2516.731787	21.617882
77.063326	2502.197961	21.622899
77.090850	2498.096080	21.627917
77.033862	2496.162361	21.632935
77.307140	2509.139879	21.637952
77.293002	2515.898338	21.642970
77.509033	2492.283060	21.647987
77.127656	2502.224157	21.653005
77.389024	2531.654883	21.658023
77.626554	2540.159290	21.663040
77.273292	2546.379993	21.668058
77.875497	2522.762657	21.673075
77.675593	2530.221205	21.678093
77.717400	2537.621117	21.683111
77.647579	2536.964912	21.688128
78.165588	2537.028179	21.693146
78.286225	2535.255429	21.698163
78.377708	2558.853949	21.703181
78.173222	2570.066648	21.708199
78.505931	2564.705445	21.713216
78.483979	2548.565501	21.718234
78.598296	2557.643935	21.723251
78.754566	2557.016303	21.728269
78.885043	2548.941101	21.733287
78.694750	2556.494712	21.738304
78.587376	2570.987327	21.743322
79.242040	2568.282163	21.748339
79.146094	2579.801098	21.753357
79.050974	2602.816635	21.758375
79.379731	2592.610135	21.763392
79.277076	2583.699946	21.768410
79.447690	2581.736873	21.773427
79.347056	2585.061742	21.778445
79.420763	2569.624169	21.783463
79.498872	2596.915745	21.788480
79.671415	2609.557093	21.793498
80.054777	2591.511816	21.798515
79.700632	2604.479723	21.803533
80.162253	2604.897731	21.808551
80.113165	2625.091935	21.813568
79.893795	2601.169556	21.818586
80.379570	2585.387342	21.823603
80.234137	2605.915702	21.828621
80.348801	2611.284025	21.833639
80.436995	2605.448327	21.838656
80.498028	2617.502686	21.843674
80.596845	2593.977674	21.848691
80.479714	2620.066893	21.853709
80.878363	2620.927724	21.858727
81.191718	2627.053263	21.863744
80.803013	2631.193939	21.868762
81.057194	2632.324081	21.873779
81.095573	2633.127533	21.878797
81.170056	2629.264869	21.883815
81.392436	2628.544432	21.888832
80.997263	2652.681123	21.893850
81.462186	2643.958369	21.898867
81.653069	2627.221836	21.903885
81.333119	2645.102704	21.908903
81.574795	2632.355228	21.913920
81.355292	2655.160918	21.918938
81.672754	2666.219731	21.923955
81.501725	2667.207571	21.928973
81.834739	2645.459663	21.933991
81.810664	2666.635670	21.939008
81.872547	2672.302262	21.944026
82.193069	2667.252836	21.949043
82.304496	2676.571547	21.954061
82.434257	2665.441522	21.959079
82.587604	2678.809224	21.964096
82.288636	2684.336658	21.969114
82.659916	2673.769979	21.974131
82.730247	2698.825545	21.979149
83.178519	2701.635189	21.984167
83.004186	2683.724473	21.989184
82.613348	2690.771405	21.994202
83.408234	2682.466675	21.999219
83.279125	2683.357444	22.004237
83.119085	2710.399048	22.009255
83.469857	2681.508803	22.014272
83.518219	2703.202146	22.019290
83.547890	2699.672611	22.024307
83.320252	2705.798416	22.029325
83.522915	2698.305613	22.034343
83.443929	2698.467138	22.039360
83.587724	2706.867065	22.044378
83.519506	2696.130115	22.049395
83.417342	2708.461673	22.054413
83.883173	2726.418469	22.059431
83.872260	2723.190673	22.064448
83.765473	2719.580350	22.069466
83.945654	2742.327013	22.074483
84.263639	2752.600084	22.079501
84.024425	2745.032067	22.084519
84.633070	2739.420905	22.089536
84.530648	2749.273944	22.094554
84.649525	2759.098688	22.099571
84.829365	2754.956808	22.104589
84.469824	2765.888423	22.109607
84.914329	2771.543590	22.114624
84.829987	2770.575250	22.119642
85.026810	2774.801862	22.124659
85.314328	2785.984197	22.129677
85.512517	2778.900897	22.134695
85.551174	2770.043419	22.139712
85.695395	2780.350733	22.144730
86.046649	2772.091905	22.149747
86.046275	2768.829685	22.154765
85.766763	2763.674486	22.159783
85.903542	2775.696769	22.164800
85.521848	2765.692187	22.169818
85.651813	2767.642165	22.174835
85.615493	2774.544935	22.179853
85.815684	2775.263199	22.184871
86.069442	2779.913416	22.189888
85.942164	2805.435806	22.194906
86.393335	2809.921342	22.199923
86.458950	2798.781548	22.204941
86.451256	2794.181145	22.209959
86.679591	2797.834916	22.214976
86.676998	2837.135103	22.219994
86.898610	2826.435395	22.225011
86.930075	2813.814028	22.230029
86.805191	2815.311702	22.235047
87.141229	2824.692587	22.240064
87.078586	2838.650967	22.245082
87.194272	2834.829271	22.250099
87.079631	2814.750950	22.255117
87.324764	2839.484002	22.260135
87.549827	2864.669957	22.265152
87.327481	2857.032374	22.270170
87.620028	2847.535142	22.275187
87.553448	2846.741397	22.280205
87.848727	2867.206530	22.285223
87.944666	2860.797287	22.290240
87.728730	2880.417506	22.295258
88.063026	2892.758771	22.300275
87.971021	2878.858709	22.305293
87.512812	2871.000481	22.310311
88.145218	2898.247251	22.315328
88.183304	2920.851341	22.320346
88.486664	2908.357781	22.325363
88.625780	2896.127169	22.330381
88.573757	2909.292423	22.335399
89.036830	2917.746583	22.340416
89.264238	2913.884559	22.345434
88.720736	2901.077261	22.350451
89.224134	2892.414340	22.355469
89.010205	2903.890619	22.360487
89.276197	2901.806050	22.365504
89.521037	2921.569839	22.370522
89.584191	2936.151729	22.375539
89.731880	2926.551039	22.380557
89.759679	2932.233594	22.385575
89.725807	2943.393571	22.390592
89.387902	2936.825109	22.395610
89.812397	2934.891881	22.400627
89.710443	2933.515272	22.405645
89.660645	2944.582617	22.410663
89.689485	2932.753418	22.415680
89.626543	2961.824240	22.420698
89.920107	2960.352748	22.425715
90.030778	2957.440203	22.430733
90.248678	2988.064666	22.435751
90.754230	2979.652688	22.440768
90.584879	2971.709673	22.445786
90.964592	2995.243716	22.450803
90.914906	2977.775390	22.455821
90.909836	2983.222874	22.460839
91.133768	2994.511920	22.465856
90.980975	2983.154374	22.470874
91.191738	2974.238422	22.475891
91.279614	2979.092664	22.480909
91.629861	3005.523167	22.485927
91.601495	3011.527199	22.490944
91.303195	3018.887688	22.495962
91.741826	3000.323414	22.500979
91.643954	3011.564676	22.505997
91.793886	3029.482306	22.511015
92.008113	3004.802103	22.516032
92.161808	3006.819245	22.521050
92.084297	3005.695251	22.526067
92.222136	3003.371838	22.531085
92.250900	3027.991161	22.536103
92.616964	3041.296276	22.541120
92.836854	3043.415069	22.546138
92.790516	3047.327057	22.551155
92.782930	3028.539471	22.556173
92.630084	3039.249351	22.561191
93.015673	3040.501690	22.566208
92.904631	3043.010758	22.571226
92.803784	3025.611454	22.576243
93.057772	3036.623747	22.581261
93.235375	3062.337886	22.586279
93.435890	3052.698667	22.591296
93.386355	3046.793643	22.596314
93.318880	3059.146518	22.601331
93.506800	3057.436401	22.606349
93.355940	3074.060834	22.611367
93.646033	3052.679444	22.616384
93.481728	3087.125479	22.621402
93.535599	3093.465914	22.626419
94.129338	3079.575767	22.631437
94.047734	3092.937973	22.636455
94.088989	3095.125657	22.641472
94.349530	3111.191458	22.646490
94.341159	3104.111042	22.651507
94.460400	3112.120412	22.656525
94.585221	3105.621068	22.661543
94.685813	3095.353329	22.666560
94.760504	3111.901364	22.671578
94.602761	3103.255655	22.676595
95.023645	3128.487038	22.681613
95.102251	3142.926626	22.686631
95.234325	3123.525755	22.691648
95.456563	3121.455080	22.696666
95.200414	3130.278175	22.701683
95.666502	3132.279339	22.706701
95.497153	3140.899142	22.711719
95.748096	3131.988860	22.716736
95.792518	3122.687167	22.721754
95.697621	3132.283527	22.726771
96.006097	3145.844087	22.731789
95.774265	3139.495385	22.736807
96.121997	3131.504241	22.741824
96.343026	3165.051438	22.746842
96.375797	3175.951386	22.751859
96.443420	3163.687498	22.756877
96.252656	3150.570354	22.761895
96.139656	3160.823587	22.766912
96.672537	3165.850193	22.771930
96.570673	3184.090485	22.776947
96.863737	3193.594629	22.781965
97.045592	3186.737439	22.786983
97.020928	3196.374787	22.792000
97.363217	3172.730717	22.797018
97.319333	3187.584048	22.802035
97.546907	3201.336746	22.807053
97.219389	3185.062396	22.812071
97.312424	3196.765304	22.817088
97.430142	3215.053984	22.822106
97.217525	3218.471894	22.827123
97.506254	3207.773036	22.832141
97.290680	3226.508100	22.837159
97.510462	3246.967515	22.842176
97.753472	3246.894558	22.847194
97.754738	3262.822080	22.852211
98.276211	3268.885340	22.857229
98.247847	3283.809026	22.862247
98.291501	3278.858888	22.867264
98.660717	3269.878988	22.872282
98.359151	3305.436464	22.877299
98.840913	3310.475108	22.882317
98.836596	3303.625404	22.887335
98.912524	3310.014640	22.892352
99.261267	3313.251237	22.897370
98.982556	3296.328612	22.902387
99.538332	3321.502001	22.907405
99.620951	3323.490580	22.912423
99.654339	3336.006715	22.917440
100.316378	3329.582664	22.922458
100.359406	3338.649128	22.927475
100.668382	3310.986146	22.932493
100.414926	3286.394190	22.937511
100.225468	3294.876668	22.942528
100.335071	3282.116626	22.947546
99.941215	3291.763469	22.952563
100.591471	3297.138207	22.957581
100.546160	3296.940862	22.962599
100.334031	3327.343191	22.967616
100.547630	3323.710293	22.972634
100.311589	3320.221964	22.977651
100.610507	3319.273124	22.982669
100.814642	3339.222898	22.987687
100.882587	3329.342841	22.992704
101.252791	3345.329354	22.997722
100.970373	3369.396371	23.002739
101.061140	3350.117384	23.007757
101.200586	3350.469768	23.012775
101.268795	3375.886986	23.017792
101.786103	3371.384680	23.022810
101.723471	3379.264021	23.027827
101.932346	3381.517543	23.032845
102.046671	3377.541623	23.037863
101.767663	3365.204354	23.042880
101.915170	3374.380335	23.047898
101.939202	3385.775725	23.052915
102.077897	3376.111091	23.057933
102.336427	3383.450994	23.062951
102.255980	3389.316943	23.067968
102.399333	3405.744508	23.072986
102.385004	3400.676758	23.078003
103.176552	3406.496056	23.083021
103.098501	3415.425895	23.088039
103.028678	3443.760642	23.093056
103.523637	3427.550307	23.098074
103.266669	3418.472040	23.103091
103.345346	3421.973148	23.108109
103.355279	3426.680583	23.113127
103.651423	3410.500165	23.118144
103.726413	3424.051919	23.123162
103.503172	3439.729740	23.128179
103.547383	3432.662137	23.133197
103.990500	3445.598407	23.138215
103.891657	3472.322994	23.143232
104.310329	3470.343818	23.148250
104.116645	3462.274268	23.153267
104.206398	3450.270448	23.158285
104.572706	3469.302926	23.163303
104.473992	3490.412877	23.168320
104.274824	3475.672186	23.173338
104.488348	3475.985169	23.178355
104.764358	3476.926549	23.183373
104.793602	3503.374142	23.188391
104.867320	3506.422388	23.193408
105.293933	3501.021137	23.198426
105.174479	3493.314074	23.203443
105.275912	3500.906350	23.208461
105.436896	3501.141213	23.213479
105.186573	3521.513923	23.218496
105.658750	3548.436977	23.223514
105.622407	3536.244299	23.228531
105.490616	3521.728828	23.233549
106.288346	3552.310565	23.238567
106.109283	3581.370444	23.243584
106.468069	3563.357818	23.248602
106.581496	3575.090712	23.253619
106.912200	3565.839667	23.258637
107.220409	3539.675292	23.263655
107.007704	3544.802392	23.268672
107.158325	3552.774131	23.273690
107.122999	3553.382939	23.278707
106.789112	3547.365668	23.283725
107.278978	3562.794689	23.288743
107.365156	3554.934335	23.293760
107.233025	3546.033379	23.298778
107.450846	3566.296906	23.303795
107.612500	3576.676670	23.308813
107.564787	3581.392300	23.313831
107.131678	3575.262881	23.318848
107.701869	3587.880661	23.323866
107.737769	3615.081809	23.328883
107.449814	3611.824021	23.333901
108.025161	3603.561973	23.338919
108.083830	3614.753006	23.343936
108.329093	3643.164389	23.348954
108.461460	3657.757964	23.353971
108.698165	3640.806284	23.358989
108.790679	3626.854193	23.364007
108.731871	3643.916549	23.369024
108.967014	3650.050108	23.374042
108.607046	3644.339053	23.379059
108.802397	3646.695235	23.384077
109.030257	3671.515542	23.389095
109.063294	3687.754565	23.394112
109.542542	3679.118623	23.399130
109.354963	3664.976774	23.404147
109.605394	3656.556001	23.409165
109.853173	3677.333974	23.414183
109.803278	3704.160116	23.419200
109.903244	3697.722895	23.424218
110.057619	3701.286355	23.429235
109.986322	3690.414980	23.434253
110.498345	3682.486558	23.439271
110.316506	3723.715127	23.444288
110.703633	3724.292518	23.449306
110.492819	3729.735092	23.454323
110.319731	3717.542427	23.459341
110.797033	3727.798684	23.464359
110.667613	3740.922322	23.469376
110.949931	3735.189151	23.474394
110.905943	3740.633884	23.479411
111.148056	3760.438370	23.484429
111.603292	3768.430550	23.489447
111.453780	3764.183978	23.494464
111.649567	3769.391083	23.499482
111.813388	3782.869816	23.504499
111.989459	3803.924947	23.509517
112.160300	3790.193214	23.514535
112.187104	3780.177355	23.519552
112.418061	3777.042236	23.524570
112.683861	3759.366182	23.529587
112.290296	3764.065201	23.534605
112.573341	3791.661028	23.539623
112.663760	3808.298148	23.544640
112.813685	3778.444231	23.549658
112.933117	3782.680366	23.554675
113.055395	3803.640456	23.559693
113.230458	3810.606587	23.564711
112.969833	3809.276785	23.569728
113.329732	3825.618429	23.574746
113.548358	3836.388729	23.579763
113.537041	3836.956575	23.584781
113.749370	3837.184534	23.589799
113.565791	3827.813012	23.594816
113.830990	3827.625569	23.599834
114.186087	3861.446004	23.604851
113.956621	3871.553412	23.609869
114.265607	3856.981130	23.614887
114.183096	3861.822862	23.619904
114.401698	3863.386311	23.624922
114.361011	3865.102441	23.629939
114.371061	3899.597257	23.634957
114.813002	3904.797197	23.639975
114.713749	3890.698417	23.644992
114.869106	3881.304910	23.650010
115.061493	3905.375596	23.655027
115.004182	3914.429846	23.660045
115.464886	3911.923626	23.665063
115.380833	3913.043420	23.670080
115.686641	3911.896176	23.675098
115.832212	3928.806973	23.680115
115.869104	3947.814361	23.685133
115.939238	3933.987928	23.690151
116.034630	3949.148877	23.695168
116.194232	3927.268780	23.700186
116.383027	3936.384732	23.705203
116.239922	3951.112287	23.710221
116.687334	3962.692853	23.715239
116.616443	3973.833904	23.720256
116.997144	3984.808617	23.725274
117.091618	3962.473510	23.730291
117.070560	3949.110530	23.735309
117.113952	3964.008843	23.740327
117.039269	3969.737453	23.745344
117.156471	3967.792678	23.750362
117.611435	3960.285330	23.755379
117.242275	3979.311036	23.760397
117.587687	4003.591222	23.765415
117.786198	4008.826698	23.770432
117.848874	3995.781319	23.775450
118.014917	4000.802484	23.780467
118.038901	3998.247947	23.785485
118.188336	4020.144931	23.790503
118.435738	4032.908142	23.795520
118.581803	4025.486449	23.800538
118.842667	4019.129195	23.805555
118.447778	4018.160713	23.810573
118.972712	4030.555640	23.815591
119.079295	4049.166619	23.820608
119.114318	4049.649458	23.825626
119.355153	4036.982458	23.830643
119.376101	4043.490919	23.835661
119.314091	4038.304271	23.840679
119.460605	4048.054014	23.845696
119.721261	4067.514706	23.850714
119.735842	4072.195193	23.855731
120.050470	4081.603415	23.860749
120.077324	4067.369469	23.865767
120.163597	4061.606765	23.870784
120.165605	4075.136505	23.875802
120.714655	4097.539978	23.880819
120.426678	4096.194789	23.885837
120.651774	4099.407106	23.890855
120.834048	4097.690921	23.895872
120.798802	4108.693903	23.900890
121.286898	4113.161127	23.905907
120.922454	4124.391342	23.910925
120.822127	4121.793549	23.915943
120.702560	4130.497206	23.920960
121.056871	4145.769889	23.925978
121.439487	4158.320712	23.930995
121.507048	4171.983793	23.936013
121.717786	4174.002096	23.941031
121.864748	4188.814224	23.946048
121.816102	4193.023326	23.951066
122.239413	4185.040020	23.956083
122.426229	4202.265940	23.961101
122.688550	4191.797530	23.966119
122.742664	4195.871549	23.971136
122.681927	4224.457983	23.976154
122.981056	4224.205484	23.981171
123.101567	4217.891025	23.986189
123.107182	4211.930578	23.991207
123.359159	4215.860889	23.996224
123.121506	4223.052679	24.001242
123.473628	4226.348754	24.006259
123.437932	4214.761906	24.011277
123.715699	4232.214158	24.016295
124.183178	4248.168607	24.021312
124.174093	4236.109254	24.026330
124.381049	4218.997102	24.031347
124.263941	4231.940781	24.036365
124.726623	4232.851365	24.041383
124.556142	4223.378427	24.046400
124.265273	4245.531548	24.051418
124.612713	4250.823596	24.056435
124.716685	4249.805344	24.061453
124.819809	4256.130244	24.066471
125.066547	4269.915374	24.071488
124.997181	4271.407555	24.076506
125.001610	4260.867544	24.081523
124.894393	4270.300312	24.086541
125.044103	4298.486376	24.091559
125.598350	4307.302801	24.096576
125.727792	4305.311475	24.101594
126.160663	4309.954805	24.106611
125.873801	4314.237160	24.111629
126.338794	4334.286449	24.116647
126.034846	4333.214339	24.121664
126.023082	4322.982857	24.126682
126.702834	4336.740195	24.131699
126.608327	4344.446559	24.136717
126.453807	4338.840859	24.141735
126.699470	4356.171001	24.146752
126.930211	4385.590249	24.151770
127.247197	4365.625593	24.156787
126.915491	4365.487565	24.161805
127.360920	4379.798604	24.166823
127.713468	4393.300226	24.171840
127.704624	4404.146697	24.176858
128.012414	4386.003558	24.181875
127.649838	4398.844634	24.186893
127.489677	4390.945430	24.191911
128.125616	4414.989286	24.196928
128.038973	4417.791384	24.201946
128.155105	4411.105534	24.206963
127.943752	4443.152195	24.211981
128.289058	4443.401104	24.216999
128.634148	4448.760142	24.222016
128.832599	4480.566336	24.227034
129.300655	4478.453291	24.232051
129.566131	4472.783655	24.237069
129.640924	4476.451979	24.242087
129.729333	4498.062880	24.247104
129.680401	4496.646266	24.252122
129.810785	4479.205150	24.257139
130.053875	4471.751858	24.262157
130.293325	4507.748862	24.267175
130.542107	4499.958797	24.272192
130.101222	4506.476443	24.277210
130.609313	4510.337738	24.282227
131.011581	4507.811554	24.287245
130.623899	4500.662470	24.292263
130.829206	4508.377248	24.297280
130.852065	4528.569529	24.302298
131.060118	4517.778379	24.307315
131.169627	4517.941452	24.312333
131.219972	4533.786779	24.317351
131.564068	4550.544195	24.322368
131.596306	4555.888431	24.327386
131.689372	4540.798246	24.332403
131.783186	4548.483829	24.337421
131.754587	4570.451953	24.342439
132.017928	4576.312330	24.347456
131.897911	4583.454141	24.352474
132.673656	4571.032566	24.357491
132.343247	4596.009986	24.362509
132.266280	4613.796870	24.367527
132.752068	4601.409797	24.372544
132.664825	4599.699903	24.377562
132.648702	4619.661347	24.382579
133.161986	4627.142621	24.387597
132.825371	4613.383973	24.392615
133.091317	4633.789369	24.397632
133.165824	4670.091165	24.402650
133.547238	4669.205387	24.407667
133.918412	4646.217285	24.412685
133.686760	4658.959778	24.417703
134.183381	4672.883108	24.422720
133.740291	4685.278281	24.427738
134.344449	4676.537292	24.432755
134.425091	4672.622119	24.437773
134.771435	4670.681521	24.442791
134.842975	4690.759277	24.447808
134.715911	4707.300624	24.452826
135.010501	4704.394961	24.457843
135.054625	4707.990849	24.462861
135.163086	4706.557658	24.467879
135.184363	4700.775142	24.472896
135.369584	4737.656433	24.477914
135.740085	4738.966924	24.482931
135.771284	4734.729593	24.487949
136.076046	4731.716734	24.492967
136.186009	4734.385616	24.497984
136.163682	4750.357739	24.503002
136.201954	4756.443954	24.508019
136.590109	4771.495917	24.513037
136.458539	4771.272059	24.518055
136.627522	4757.202970	24.523072
136.787838	4783.363376	24.528090
136.716760	4795.094414	24.533107
137.120174	4780.014526	24.538125
137.193584	4796.622842	24.543143
137.496948	4810.079806	24.548160
137.473350	4804.067267	24.553178
137.714461	4798.351539	24.558195
137.815385	4821.411603	24.563213
137.736914	4839.243087	24.568231
138.297452	4838.912347	24.573248
137.923574	4839.513563	24.578266
138.267783	4846.557528	24.583283
138.371646	4868.671508	24.588301
138.412572	4884.446702	24.593319
138.569179	4876.698453	24.598336
138.602371	4892.715091	24.603354
138.963470	4897.761011	24.608371
138.877820	4897.776020	24.613389
139.067478	4913.595960	24.618407
139.395060	4948.385720	24.623424
139.656897	4942.196435	24.628442
139.760905	4926.472962	24.633459
140.055649	4944.708255	24.638477
140.184745	4973.545017	24.643495
140.365293	4958.216742	24.648512
140.472605	4984.035454	24.653530
140.413644	4959.870711	24.658547
140.955109	4965.496696	24.663565
140.732688	4966.469743	24.668583
141.346821	4964.015173	24.673600
141.269897	4997.990382	24.678618
141.316305	5010.562806	24.683635
141.830683	4995.386423	24.688653
141.445576	4984.614614	24.693671
141.911510	5000.118517	24.698688
141.682036	4994.878116	24.703706
141.857933	5001.266100	24.708723
142.132693	5019.178795	24.713741
141.806491	5025.958811	24.718759
142.126912	5001.468321	24.723776
142.298195	5017.398885	24.728794
141.902155	5050.608032	24.733811
142.448904	5056.844996	24.738829
142.865988	5050.405210	24.743847
142.892379	5043.890612	24.748864
143.192462	5069.984704	24.753882
143.240011	5090.711832	24.758899
143.450773	5079.026134	24.763917
143.382543	5059.339597	24.768935
143.451628	5072.941801	24.773952
143.994795	5120.639406	24.778970
143.739370	5117.731240	24.783987
143.753030	5107.551340	24.789005
144.035402	5115.530463	24.794023
144.451925	5126.526448	24.799040
144.487231	5131.689270	24.804058
144.697812	5132.078173	24.809075
144.759935	5152.403362	24.814093
144.736322	5153.424279	24.819111
145.070398	5165.640629	24.824128
144.949869	5167.168122	24.829146
145.357323	5171.184801	24.834163
145.470602	5196.893823	24.839181
145.386814	5213.212016	24.844199
145.618607	5210.793025	24.849216
145.552150	5212.328911	24.854234
145.788212	5227.672202	24.859251
146.178813	5249.574381	24.864269
146.190118	5252.526983	24.869287
146.510928	5239.257590	24.874304
146.826435	5246.456090	24.879322
146.909178	5269.334778	24.884339
147.024057	5260.102644	24.889357
147.017542	5282.403172	24.894375
147.212417	5285.551045	24.899392
147.390683	5290.909202	24.904410
147.537074	5283.986082	24.909427
147.826770	5304.790416	24.914445
147.794579	5327.415731	24.919463
148.289422	5325.926909	24.924480
148.553294	5314.124776	24.929498
148.744227	5325.799141	24.934515
148.784206	5338.231549	24.939533
149.023674	5326.740535	24.944551
149.140004	5334.121991	24.949568
149.179890	5338.406541	24.954586
149.217896	5345.220612	24.959603
149.467589	5343.425827	24.964621
149.246093	5366.254925	24.969639
149.359918	5374.562827	24.974656
149.883923	5372.255377	24.979674
149.789069	5391.308742	24.984691
150.176368	5393.360241	24.989709
149.836178	5405.686616	24.994727
150.143887	5406.218932	24.999744
150.268813	5413.968310	25.004762
150.250570	5409.403520	25.009779
150.428117	5426.058295	25.014797
150.686124	5467.145580	25.019815
150.964933	5452.484862	25.024832
151.006245	5466.087274	25.029850
151.262088	5477.615589	25.034867
151.619846	5477.564419	25.039885
151.475249	5493.233479	25.044903
151.823354	5517.053762	25.049920
152.042797	5516.463218	25.054938
152.085444	5510.826090	25.059955
152.594901	5509.212784	25.064973
152.513165	5510.939027	25.069991
152.839126	5524.634620	25.075008
152.826729	5508.980190	25.080026
152.903544	5512.788982	25.085043
153.296814	5541.833550	25.090061
153.040426	5558.218026	25.095079
152.969263	5554.763561	25.100096
153.183738	5557.557449	25.105114
153.110527	5571.235571	25.110131
153.399431	5575.080991	25.115149
153.698066	5593.197499	25.120167
153.758479	5594.439612	25.125184
154.200443	5584.780784	25.130202
153.768923	5620.692797	25.135219
153.971380	5634.683710	25.140237
154.240076	5643.643758	25.145255
154.395233	5634.605939	25.150272
155.030306	5650.876681	25.155290
154.900969	5680.405517	25.160307
155.506176	5680.396142	25.165325
155.720337	5674.743214	25.170343
155.761358	5691.337756	25.175360
156.405351	5692.825988	25.180378
155.978362	5696.358996	25.185395
156.130667	5682.399709	25.190413
156.321440	5701.025530	25.195431
156.714832	5709.492153	25.200448
156.524975	5700.310505	25.205466
156.691533	5721.191257	25.210483
156.584741	5726.443114	25.215501
156.751322	5738.679323	25.220519
156.918312	5737.225737	25.225536
157.152684	5729.966999	25.230554
157.238680	5764.187838	25.235571
157.466643	5771.742013	25.240589
157.526532	5783.025357	25.245607
157.744696	5809.891357	25.250624
158.112983	5806.023260	25.255642
157.889804	5813.849647	25.260659
158.073261	5834.953757	25.265677
158.275893	5832.106786	25.270695
158.460184	5837.601153	25.275712
158.868550	5878.228430	25.280730
158.826727	5894.403778	25.285747
158.736009	5890.603628	25.290765
159.204393	5891.629132	25.295783
159.279705	5906.329532	25.300800
159.731449	5921.410689	25.305818
159.774867	5941.709287	25.310835
160.337091	5945.315137	25.315853
160.522943	5938.562779	25.320871
160.177528	5934.861792	25.325888
160.840600	5941.584261	25.330906
160.541253	5953.534215	25.335923
160.711278	5963.747845	25.340941
161.342032	5974.802348	25.345959
161.057474	5981.240043	25.350976
161.223166	5992.599765	25.355994
161.507864	6010.173353	25.361011
161.580701	5998.972390	25.366029
161.832995	6000.599790	25.371047
161.932885	6023.338945	25.376064
162.161543	6012.950477	25.381082
162.328186	6029.248617	25.386099
162.250560	6034.943429	25.391117
162.573896	6041.166917	25.396135
162.749369	6044.405166	25.401152
163.348550	6053.887266	25.406170
162.923838	6076.581280	25.411187
163.149058	6075.869281	25.416205
163.532477	6071.092250	25.421223
163.401357	6084.821338	25.426240
164.106501	6070.864854	25.431258
163.796380	6099.127796	25.436275
163.943187	6092.872020	25.441293
164.538060	6097.089882	25.446311
164.281799	6108.793839	25.451328
164.785915	6112.778651	25.456346
164.357514	6125.115441	25.461363
164.519133	6128.621766	25.466381
164.968418	6136.290348	25.471399
164.671232	6153.562179	25.476416
165.253581	6149.657448	25.481434
165.784684	6176.849175	25.486451
165.284576	6194.836527	25.491469
165.709584	6185.087606	25.496487
165.689400	6186.011560	25.501504
165.957975	6211.764711	25.506522
166.468317	6231.832585	25.511539
166.769324	6214.507808	25.516557
166.765910	6199.906410	25.521575
166.324351	6223.243631	25.526592
166.440973	6252.521865	25.531610
166.832527	6270.823826	25.536627
167.219340	6282.283456	25.541645
167.293933	6293.932490	25.546663
167.292194	6298.477354	25.551680
167.679145	6302.394164	25.556698
167.806601	6332.796846	25.561715
167.930946	6350.374476	25.566733
168.270636	6342.041656	25.571751
168.341042	6356.848024	25.576768
168.637048	6357.944961	25.581786
168.631556	6375.829140	25.586803
168.794326	6397.366603	25.591821
169.241982	6398.593620	25.596839
168.969512	6425.279122	25.601856
169.408472	6426.608769	25.606874
169.411785	6425.731039	25.611891
169.628618	6434.549704	25.616909
170.115835	6455.875356	25.621927
170.286357	6479.700072	25.626944
171.063828	6461.427309	25.631962
171.258705	6452.179286	25.636979
171.139770	6463.061130	25.641997
171.442963	6472.409303	25.647015
171.512322	6464.251019	25.652032
171.583932	6448.537669	25.657050
171.959594	6467.662255	25.662067
171.522102	6502.034204	25.667085
171.664890	6494.542976	25.672103
171.710693	6493.378665	25.677120
172.167866	6508.577618	25.682138
172.143057	6522.566717	25.687156
172.309295	6521.955399	25.692173
172.624762	6541.089234	25.697191
172.654147	6563.206111	25.702208
172.707393	6555.547739	25.707226
172.791929	6554.049823	25.712244
173.285780	6580.325082	25.717261
173.551494	6592.257360	25.722279
173.393410	6602.505541	25.727296
173.706260	6615.404172	25.732314
173.842887	6625.860395	25.737332
174.055371	6639.365065	25.742349
174.598772	6647.329015	25.747367
174.265162	6672.889872	25.752384
174.597944	6664.518648	25.757402
175.033338	6662.346144	25.762420
175.105209	6678.446029	25.767437
175.349343	6664.725449	25.772455
175.193043	6690.763396	25.777472
175.125377	6666.051717	25.782490
175.233946	6685.220701	25.787508
175.577781	6708.895069	25.792525
176.096838	6719.632300	25.797543
176.202015	6727.678542	25.802560
176.557211	6748.811029	25.807578
176.696709	6730.048415	25.812596
176.762929	6747.057680	25.817613
176.934622	6764.337760	25.822631
177.239044	6766.419283	25.827648
177.078473	6765.442612	25.832666
177.342837	6797.925012	25.837684
177.378118	6799.311548	25.842701
177.575035	6784.751317	25.847719
177.675058	6810.176174	25.852736
177.776458	6844.992575	25.857754
178.220421	6862.056889	25.862772
178.308585	6857.617814	25.867789
178.556312	6870.029321	25.872807
178.644367	6888.715662	25.877824
179.251582	6907.478470	25.882842
179.434083	6903.921943	25.887860
179.169716	6911.928932	25.892877
179.373243	6934.232154	25.897895
179.279963	6930.151034	25.902912
179.552987	6953.343706	25.907930
180.052778	6978.304698	25.912948
180.151740	6998.004857	25.917965
180.269353	6986.255954	25.922983
180.673914	7004.674360	25.928000
181.114667	7017.684885	25.933018
181.171792	7015.314957	25.938036
181.119180	7025.827521	25.943053
181.614473	7042.303156	25.948071
181.762619	7045.839083	25.953088
181.746846	7054.427203	25.958106
181.734077	7055.274381	25.963124
181.953814	7071.198642	25.968141
182.023138	7089.249644	25.973159
182.245538	7108.792913	25.978176
182.374389	7108.401561	25.983194
182.486679	7111.736705	25.988212
182.604823	7150.209808	25.993229
182.885332	7154.418085	25.998247
183.623881	7148.329904	26.003264
183.913862	7153.814754	26.008282
183.962217	7158.674078	26.013300
184.264871	7180.991986	26.018317
184.761456	7182.450390	26.023335
184.674312	7188.519294	26.028352
184.951727	7199.653923	26.033370
185.004567	7188.151433	26.038388
184.989946	7191.166175	26.043405
185.162598	7210.513824	26.048423
185.605344	7236.149319	26.053440
185.351405	7221.326119	26.058458
185.495951	7218.523149	26.063476
185.274278	7258.771426	26.068493
185.796459	7272.157352	26.073511
185.851772	7264.560508	26.078528
185.819977	7287.857591	26.083546
186.297632	7306.524945	26.088564
186.379871	7340.726225	26.093581
186.681697	7330.503960	26.098599
186.839827	7333.271253	26.103616
187.109570	7335.624768	26.108634
187.766521	7357.529214	26.113652
187.832126	7378.985640	26.118669
187.757225	7379.896654	26.123687
188.213951	7379.896074	26.128704
188.480369	7394.626148	26.133722
188.375643	7386.193344	26.138740
188.262241	7420.883102	26.143757
188.821749	7405.471707	26.148775
188.864792	7412.641416	26.153792
189.154092	7417.897695	26.158810
189.401632	7434.762767	26.163828
189.062884	7456.903534	26.168845
189.367364	7468.818264	26.173863
189.469150	7472.448576	26.178880
189.659320	7504.168190	26.183898
190.182002	7515.541306	26.188916
190.303490	7533.011662	26.193933
190.492025	7529.897380	26.198951
190.637904	7532.098132	26.203968
190.855732	7570.068703	26.208986
191.319460	7557.877474	26.214004
191.400536	7583.322858	26.219021
191.469116	7613.987795	26.224039
192.128277	7615.030336	26.229056
192.106330	7596.297695	26.234074
191.939896	7628.100893	26.239092
192.310979	7647.856530	26.244109
193.005934	7634.534718	26.249127
193.147660	7657.063390	26.254144
193.524265	7671.645573	26.259162
193.828012	7646.731982	26.264180
193.858422	7649.764572	26.269197
193.724692	7658.802510	26.274215
193.980699	7674.332345	26.279232
194.198560	7676.541701	26.284250
194.745509	7666.155862	26.289268
194.281965	7688.249844	26.294285
194.802177	7695.733038	26.299303
195.259401	7708.403169	26.304320
194.990255	7720.742061	26.309338
195.198934	7702.423239	26.314356
195.081047	7727.638691	26.319373
195.483581	7747.270338	26.324391
195.558607	7748.081784	26.329408
195.534284	7775.361762	26.334426
195.810352	7781.548869	26.339444
195.733308	7800.370679	26.344461
196.072658	7822.615707	26.349479
196.238489	7837.328951	26.354496
196.779710	7842.649281	26.359514
197.169924	7849.701187	26.364532
197.175362	7882.916145	26.369549
197.393966	7887.514844	26.374567
197.419481	7883.932845	26.379584
197.962951	7896.694410	26.384602
198.186271	7909.137157	26.389620
198.563819	7934.747552	26.394637
198.615047	7934.623386	26.399655
198.994862	7929.053327	26.404672
198.764542	7947.936079	26.409690
199.071143	7962.722263	26.414708
199.416012	7975.978215	26.419725
199.395484	7978.056102	26.424743
199.535676	7993.988143	26.429760
199.618193	8012.472757	26.434778
199.689991	8004.462514	26.439796
199.559415	8039.012347	26.444813
199.907986	8047.299817	26.449831
200.112138	8050.518782	26.454848
200.212149	8070.563095	26.459866
201.009710	8094.138598	26.464884
201.089909	8107.527386	26.469901
201.267430	8101.983603	26.474919
201.663193	8109.574978	26.479936
201.576331	8142.949071	26.484954
201.834667	8158.158461	26.489972
201.659741	8160.717883	26.494989
202.097026	8151.961208	26.500007
202.346671	8168.858224	26.505024
202.316158	8202.009701	26.510042
202.917876	8212.014860	26.515060
202.946242	8223.568611	26.520077
202.954656	8226.761673	26.525095
203.373081	8258.067060	26.530112
203.345302	8280.060729	26.535130
203.994631	8282.676151	26.540148
203.863795	8309.324117	26.545165
203.908966	8326.351169	26.550183
204.291462	8332.366544	26.555200
204.462916	8361.536085	26.560218
204.770200	8363.025883	26.565236
205.113888	8392.760857	26.570253
205.381824	8405.074551	26.575271
206.063090	8411.937645	26.580288
205.953816	8421.700488	26.585306
206.273132	8421.868321	26.590324
206.502541	8427.815304	26.595341
206.813215	8466.114505	26.600359
206.853038	8468.284083	26.605376
206.848014	8467.280815	26.610394
206.851958	8464.171647	26.615412
207.409702	8491.553588	26.620429
207.410650	8510.843785	26.625447
207.712716	8507.810577	26.630464
207.719141	8528.369475	26.635482
208.049580	8549.644337	26.640500
208.531147	8541.273925	26.645517
208.462812	8570.175524	26.650535
208.471984	8593.591419	26.655552
208.838986	8610.339566	26.660570
208.884726	8611.677280	26.665588
208.963129	8639.593115	26.670605
208.933410	8635.341957	26.675623
209.559973	8661.641700	26.680640
209.844143	8690.034774	26.685658
210.267390	8702.102512	26.690676
210.929128	8693.613254	26.695693
211.052673	8695.235042	26.700711
211.218728	8718.562982	26.705728
211.369923	8751.329596	26.710746
211.428479	8752.067419	26.715764
211.598327	8739.189801	26.720781
211.333678	8766.842778	26.725799
211.981280	8785.360160	26.730816
212.247784	8790.292240	26.735834
212.414922	8800.339650	26.740852
212.703282	8807.402516	26.745869
212.643695	8828.469686	26.750887
212.521414	8829.546918	26.755904
213.212306	8861.899313	26.760922
213.285142	8883.582634	26.765940
213.478387	8884.854257	26.770957
213.304610	8888.204359	26.775975
213.707521	8902.391900	26.780992
213.855727	8946.867145	26.786010
214.138539	8946.073049	26.791028
214.424391	8944.659393	26.796045
214.698626	8978.232347	26.801063
215.152209	8960.461523	26.806080
215.300836	8996.807167	26.811098
215.558462	9012.488489	26.816116
215.772954	9009.798877	26.821133
216.037847	9027.547274	26.826151
216.607736	9041.360804	26.831168
216.330649	9034.423702	26.836186
216.762051	9054.732706	26.841204
216.752881	9060.170383	26.846221
217.167682	9074.216708	26.851239
217.316263	9089.264768	26.856256
217.463802	9100.149689	26.861274
217.480646	9104.606443	26.866292
217.914906	9118.835469	26.871309
217.974132	9148.226635	26.876327
218.227323	9158.193895	26.881344
218.387335	9161.984316	26.886362
218.648192	9182.186192	26.891380
219.016632	9194.878493	26.896397
219.097307	9209.153419	26.901415
219.459269	9212.843538	26.906432
219.759195	9218.508229	26.911450
219.672667	9235.098838	26.916468
220.054453	9256.758405	26.921485
220.228034	9257.374857	26.926503
220.824046	9276.286488	26.931520
221.173221	9284.683992	26.936538
221.086758	9288.735700	26.941556
221.543251	9303.103780	26.946573
221.478923	9313.967932	26.951591
221.585762	9315.076652	26.956608
221.774755	9343.220408	26.961626
221.979967	9364.810844	26.966644
222.481288	9361.339715	26.971661
222.726131	9380.617454	26.976679
222.856439	9408.207869	26.981696
223.066057	9420.254745	26.986714
223.043643	9428.373464	26.991732
223.356909	9446.849987	26.996749
223.228208	9464.978170	27.001767
223.479257	9476.290473	27.006784
223.658680	9511.282209	27.011802
223.624027	9532.044530	27.016820
224.293248	9533.031205	27.021837
224.199708	9552.109867	27.026855
224.765261	9576.046495	27.031872
225.093941	9607.216584	27.036890
225.294137	9625.408756	27.041908
225.717617	9613.899973	27.046925
225.402119	9641.532944	27.051943
225.767610	9672.112650	27.056960
226.403872	9681.904317	27.061978
226.586248	9696.477149	27.066996
227.006594	9708.541413	27.072013
227.135188	9724.540126	27.077031
227.344415	9732.721548	27.082048
227.540540	9744.169140	27.087066
227.529120	9760.829016	27.092084
227.983863	9774.209318	27.097101
227.909714	9777.780227	27.102119
228.450067	9790.795107	27.107136
228.762741	9829.482439	27.112154
228.658779	9832.290327	27.117172
228.989330	9831.452071	27.122189
229.237362	9864.733503	27.127207
229.551266	9845.099921	27.132224
229.887898	9863.439169	27.137242
229.713641	9903.854899	27.142260
230.187056	9901.233418	27.147277
230.037564	9913.854340	27.152295
230.520843	9923.243738	27.157312
230.873151	9937.930493	27.162330
230.558826	9975.734055	27.167348
231.314045	9983.148799	27.172365
231.578710	9982.144199	27.177383
231.493293	9997.362534	27.182400
232.168318	9995.984522	27.187418
232.259358	10011.792028	27.192436
232.742465	10028.468936	27.197453
233.173773	10047.552059	27.202471
232.919555	10043.402989	27.207488
233.314329	10042.401306	27.212506
233.505549	10072.614385	27.217524
233.936052	10092.442823	27.222541
233.562897	10111.236748	27.227559
233.628721	10105.441341	27.232576
233.930024	10133.621506	27.237594
234.291283	10176.066692	27.242612
234.786427	10189.508410	27.247629
234.887431	10189.742270	27.252647
235.011163	10222.529854	27.257664
235.430621	10224.647190	27.262682
235.596544	10239.762004	27.267700
235.827871	10269.662427	27.272717
235.995476	10292.118901	27.277735
236.426914	10292.517141	27.282752
236.985641	10295.121101	27.287770
236.828421	10316.411958	27.292788
237.342306	10337.994467	27.297805
237.341535	10345.538226	27.302823
237.646040	10355.479648	27.307840
237.833592	10367.812879	27.312858
238.050661	10408.793014	27.317876
238.111188	10410.388372	27.322893
238.264073	10420.859787	27.327911
238.612323	10440.445466	27.332928
238.755653	10463.479623	27.337946
239.106678	10494.971501	27.342964
239.682833	10510.900212	27.347981
239.810311	10516.324475	27.352999
240.202589	10525.829304	27.358016
241.048804	10529.898947	27.363034
241.132762	10567.928764	27.368052
241.282178	10557.661868	27.373069
241.606663	10545.796196	27.378087
241.768140	10555.695209	27.383104
241.926860	10573.440038	27.388122
242.109585	10595.966122	27.393140
242.219106	10611.853091	27.398157
242.762726	10620.947793	27.403175
242.541374	10627.908219	27.408192
242.842254	10626.608514	27.413210
242.813675	10664.323963	27.418228
243.280890	10665.570161	27.423245
243.286367	10676.567070	27.428263
243.430478	10710.069879	27.433280
243.871387	10738.735325	27.438298
243.978004	10741.161208	27.443316
244.146326	10743.404391	27.448333
244.658674	10783.300887	27.453351
244.770948	10803.633353	27.458368
244.863602	10804.726405	27.463386
244.896567	10832.293627	27.468404
245.594302	10827.056011	27.473421
245.828746	10842.685473	27.478439
246.016077	10870.042147	27.483456
246.199776	10867.333682	27.488474
246.154768	10897.082439	27.493492
246.300938	10902.266648	27.498509
246.610015	10928.595048	27.503527
247.158314	10969.701498	27.508544
247.343561	10977.251058	27.513562
247.393485	10988.057303	27.518580
247.524874	11008.620822	27.523597
247.983670	11044.017979	27.528615
247.847763	11055.014089	27.533632
248.221374	11070.978403	27.538650
248.196384	11117.292196	27.543668
248.609985	11120.361393	27.548685
249.117159	11150.254130	27.553703
249.545177	11196.084483	27.558720
249.794605	11195.878710	27.563738
249.870246	11237.267172	27.568756
250.178261	11238.098597	27.573773
250.600983	11253.196366	27.578791
251.104030	11286.800990	27.583808
251.300069	11277.208096	27.588826
251.758754	11297.795897	27.593844
251.847258	11316.985234	27.598861
252.174583	11319.191201	27.603879
252.339263	11339.726015	27.608896
252.804635	11357.206791	27.613914
253.037283	11362.652566	27.618932
252.827035	11376.694710	27.623949
253.065684	11418.669562	27.628967
253.259794	11427.156842	27.633984
253.618466	11447.112272	27.639002
253.607298	11466.422236	27.644020
253.918254	11490.403816	27.649037
254.228448	11513.945216	27.654055
254.599347	11548.877499	27.659072
254.977363	11560.903692	27.664090
254.883044	11586.085138	27.669108
255.500349	11619.028792	27.674125
255.550874	11632.278936	27.679143
255.664149	11634.996895	27.684160
256.121076	11663.372258	27.689178
256.644659	11698.908259	27.694196
257.085255	11713.110212	27.699213
257.652807	11719.838365	27.704231
258.047665	11724.383070	27.709248
258.175439	11742.940962	27.714266
258.298872	11753.560701	27.719284
258.399840	11741.109545	27.724301
258.952841	11769.890668	27.729319
259.194530	11794.831807	27.734336
259.570762	11779.588272	27.739354
259.468831	11805.611057	27.744372
259.661442	11821.645415	27.749389
260.250396	11817.493642	27.754407
260.136323	11835.273916	27.759424
260.360383	11854.225658	27.764442
260.826157	11873.844888	27.769460
260.792677	11883.250718	27.774477
260.886115	11882.371187	27.779495
261.068932	11910.694596	27.784512
261.589701	11946.691662	27.789530
261.670383	11947.592196	27.794548
261.932251	11969.563593	27.799565
262.390569	11986.446744	27.804583
262.312238	12012.602247	27.809600
262.581413	12016.166562	27.814618
262.851961	12031.209071	27.819636
262.786229	12060.768051	27.824653
263.431338	12081.941305	27.829671
263.300969	12098.565767	27.834688
264.008842	12118.603776	27.839706
264.133402	12142.038913	27.844724
264.406860	12155.707986	27.849741
265.041503	12182.061079	27.854759
265.014880	12193.360534	27.859776
265.374118	12206.277342	27.864794
265.169842	12235.815419	27.869812
265.464222	12268.356071	27.874829
266.028223	12284.496541	27.879847
266.057249	12301.770786	27.884864
266.415987	12319.597949	27.889882
266.557861	12368.010049	27.894900
267.065122	12383.024809	27.899917
267.279174	12396.417941	27.904935
267.409050	12431.425057	27.909952
267.741781	12430.911668	27.914970
268.293822	12461.355618	27.919988
268.358522	12482.329090	27.925005
268.911273	12480.592952	27.930023
269.143006	12530.215694	27.935040
269.663933	12538.095759	27.940058
269.691920	12552.319361	27.945076
269.869690	12578.575276	27.950093
270.316671	12571.194005	27.955111
270.449033	12612.807471	27.960128
270.978477	12642.247919	27.965146
271.214231	12646.537936	27.970164
271.381732	12648.950900	27.975181
271.780907	12670.137206	27.980199
272.046201	12693.962699	27.985216
272.712090	12715.453991	27.990234
272.895401	12714.654102	27.995252
272.805992	12737.647269	28.000269
273.256809	12749.830919	28.005287
273.383253	12759.255745	28.010304
273.662424	12778.013556	28.015322
273.811505	12805.308956	28.020340
274.017565	12839.280241	28.025357
274.447479	12839.906483	28.030375
274.355443	12879.321942	28.035392
274.748538	12893.140469	28.040410
275.208920	12897.539972	28.045428
275.156909	12926.246665	28.050445
275.531773	12932.752709	28.055463
275.949438	12974.757206	28.060480
276.063032	13000.624209	28.065498
276.598815	13013.469960	28.070516
276.728125	13034.350758	28.075533
277.293703	13045.289845	28.080551
277.474234	13070.406938	28.085568
277.796533	13095.941033	28.090586
278.132555	13102.757659	28.095604
278.050410	13122.398829	28.100621
278.529949	13144.371325	28.105639
278.634280	13176.619062	28.110656
278.906212	13187.214429	28.115674
279.050150	13209.386630	28.120692
279.131764	13241.753272	28.125709
279.533826	13259.871330	28.130727
279.919928	13290.048049	28.135744
280.301070	13302.056130	28.140762
280.542917	13313.087488	28.145780
280.980205	13351.706825	28.150797
281.457847	13356.943424	28.155815
281.501087	13382.363363	28.160832
281.847181	13413.018042	28.165850
282.426414	13411.431848	28.170868
282.294591	13434.066677	28.175885
282.785910	13442.519318	28.180903
282.649720	13459.964699	28.185920
283.262573	13484.183792	28.190938
283.468624	13482.930260	28.195956
283.270561	13526.155852	28.200973
283.416508	13541.622158	28.205991
283.914595	13582.423753	28.211008
284.040524	13606.841652	28.216026
284.192593	13627.232576	28.221044
284.023134	13657.271720	28.226061
285.220892	13696.706137	28.231079
285.206964	13728.015713	28.236096
285.479109	13752.982437	28.241114
286.172443	13759.778916	28.246132
286.408657	13808.078917	28.251149
286.596328	13807.238076	28.256167
286.720324	13853.892824	28.261184
287.079309	13892.475971	28.266202
287.847920	13897.389718	28.271220
287.607728	13925.146040	28.276237
288.095370	13947.011935	28.281255
288.744545	13976.698190	28.286272
288.899232	14002.063663	28.291290
289.634968	14002.873425	28.296308
289.712666	14015.655422	28.301325
290.255549	14048.764482	28.306343
290.660479	14050.933591	28.311360
290.637739	14067.992955	28.316378
291.045544	14091.972666	28.321396
291.266943	14098.112973	28.326413
291.343258	14092.249792	28.331431
292.017269	14132.191735	28.336448
292.071969	14154.452461	28.341466
292.574869	14157.208901	28.346484
292.824336	14190.231215	28.351501
293.549888	14196.125969	28.356519
293.814346	14199.894034	28.361536
293.888210	14214.659089	28.366554
294.749029	14226.861216	28.371572
294.268557	14247.861661	28.376589
294.790584	14258.824531	28.381607
294.749333	14256.702599	28.386624
295.137914	14280.786614	28.391642
295.292828	14300.713077	28.396660
295.671524	14344.881618	28.401677
295.959183	14351.954946	28.406695
296.399928	14356.521189	28.411712
296.308630	14385.870415	28.416730
296.538686	14406.668589	28.421748
296.255371	14421.083147	28.426765
297.007275	14465.256542	28.431783
297.043986	14482.706762	28.436800
297.228410	14509.461087	28.441818
297.776521	14536.602887	28.446836
297.847947	14555.065393	28.451853
298.060486	14596.662063	28.456871
298.625153	14629.359016	28.461888
298.557091	14650.306028	28.466906
299.196285	14689.117393	28.471924
299.383867	14710.291705	28.476941
299.591661	14716.161887	28.481959
300.159560	14747.000701	28.486976
300.604869	14774.826441	28.491994
301.005459	14806.586479	28.497012
301.017965	14828.002601	28.502029
301.566043	14839.896007	28.507047
301.805917	14859.073227	28.512064
301.984319	14882.674426	28.517082
302.546244	14909.494684	28.522100
302.600279	14940.588948	28.527117
302.909968	14965.202303	28.532135
303.022860	14983.390559	28.537152
303.461836	15010.133596	28.542170
304.076581	15032.244699	28.547188
303.954501	15063.551088	28.552205
304.156108	15074.015916	28.557223
304.911005	15109.882890	28.562240
305.056064	15132.150517	28.567258
305.662075	15143.090661	28.572276
305.894893	15160.362661	28.577293
306.103763	15184.082179	28.582311
306.650463	15195.856314	28.587328
306.783703	15233.001829	28.592346
307.115145	15267.593353	28.597364
307.154604	15288.063281	28.602381
307.632879	15286.555054	28.607399
308.032845	15317.533007	28.612416
307.935896	15361.499249	28.617434
308.454669	15388.470832	28.622452
308.714302	15407.724229	28.627469
308.995220	15423.611273	28.632487
309.292600	15457.001729	28.637504
309.164565	15513.280914	28.642522
309.803657	15514.653554	28.647540
309.918334	15551.048027	28.652557
310.364274	15588.810860	28.657575
310.861693	15613.044342	28.662592
311.169685	15645.519429	28.667610
311.593438	15671.586873	28.672628
311.981031	15709.518788	28.677645
312.370111	15707.539891	28.682663
312.795603	15731.454499	28.687680
312.741285	15782.793094	28.692698
312.912102	15805.140908	28.697716
313.224257	15821.581045	28.702733
313.619384	15857.520141	28.707751
314.223569	15866.169735	28.712768
314.424672	15890.343848	28.717786
315.154218	15924.324165	28.722804
315.308433	15955.074456	28.727821
315.500605	15978.421252	28.732839
316.147103	15995.737687	28.737856
316.077352	16024.340908	28.742874
316.431049	16042.158050	28.747892
316.809943	16073.820142	28.752909
317.234361	16114.381840	28.757927
317.359041	16122.065957	28.762944
317.676836	16138.592158	28.767962
317.801557	16182.278150	28.772980
317.994252	16193.028838	28.777997
318.247640	16226.716534	28.783015
319.053541	16257.854574	28.788032
318.792943	16288.699238	28.793050
320.001086	16314.709044	28.798068
320.158308	16326.548347	28.803085
320.460637	16353.272046	28.808103
320.769417	16372.614598	28.813120
320.945141	16398.232490	28.818138
321.258228	16399.720530	28.823156
321.687112	16433.534103	28.828173
321.721267	16468.271850	28.833191
321.936252	16483.715374	28.838208
321.883513	16511.276510	28.843226
322.347821	16539.932664	28.848244
322.820695	16562.472737	28.853261
323.009728	16605.432176	28.858279
323.734229	16624.933287	28.863296
323.663877	16666.413357	28.868314
324.092368	16695.086732	28.873332
324.150545	16720.079976	28.878349
324.340450	16749.112784	28.883367
324.891100	16774.146102	28.888384
325.158811	16822.534965	28.893402
325.456578	16849.162518	28.898420
326.137352	16850.673385	28.903437
326.249602	16886.937281	28.908455
326.722464	16911.588088	28.913472
326.987792	16955.454644	28.918490
327.485408	16966.700763	28.923508
327.842109	16994.845958	28.928525
328.094695	17030.571636	28.933543
328.602604	17046.495262	28.938560
329.135863	17082.901224	28.943578
328.989727	17110.415757	28.948596
329.498607	17138.597524	28.953613
329.539092	17165.343745	28.958631
329.950591	17199.998642	28.963648
330.376603	17232.614994	28.968666
330.344635	17262.694022	28.973684
330.956091	17291.382346	28.978701
331.050678	17333.985781	28.983719
331.809628	17349.704323	28.988736
332.237020	17380.237225	28.993754
332.813598	17403.532010	28.998772
333.555660	17421.388943	29.003789
333.475448	17464.079907	29.008807
334.114868	17498.455072	29.013824
334.093311	17505.257773	29.018842
334.588732	17525.130354	29.023860
335.109734	17550.294268	29.028877
335.198894	17561.865173	29.033895
335.897359	17596.320625	29.038912
335.712915	17625.531883	29.043930
336.150520	17635.819102	29.048948
336.732820	17644.400765	29.053965
336.615551	17687.378971	29.058983
337.156057	17709.334191	29.064000
337.255969	17731.587606	29.069018
337.565566	17785.811735	29.074036
338.006513	17800.457930	29.079053
338.116910	17846.566855	29.084071
338.405572	17861.651195	29.089088
338.676304	17880.763830	29.094106
339.128948	17927.486277	29.099124
339.592623	17955.902301	29.104141
339.888744	17990.174450	29.109159
340.151903	18022.679007	29.114176
340.667119	18052.647020	29.119194
340.861361	18061.095999	29.124212
341.273577	18101.253278	29.129229
341.578945	18140.830962	29.134247
341.935954	18156.589890	29.139264
342.177726	18181.923841	29.144282
342.521549	18208.724097	29.149300
343.236900	18233.924728	29.154317
343.518118	18263.654387	29.159335
344.228667	18287.199390	29.164352
344.542097	18286.321792	29.169370
344.510366	18321.146849	29.174388
345.315127	18358.045099	29.179405
345.205975	18381.055798	29.184423
345.597580	18374.413976	29.189440
345.592515	18404.427603	29.194458
346.143648	18443.684864	29.199476
346.333493	18474.925754	29.204493
346.380988	18501.275804	29.209511
346.831702	18538.029626	29.214528
346.860940	18564.750036	29.219546
347.059132	18609.680244	29.224564
347.749459	18630.051554	29.229581
347.802827	18685.011333	29.234599
348.056084	18711.311965	29.239616
348.505914	18732.016299	29.244634
348.722006	18796.434934	29.249652
349.647188	18815.465759	29.254669
349.584189	18865.745215	29.259687
350.047446	18918.464507	29.264704
350.465779	18936.622462	29.269722
350.853351	18969.469281	29.274740
351.283755	19004.455863	29.279757
351.503563	19064.048630	29.284775
352.265612	19080.483921	29.289792
353.369119	19090.482362	29.294810
353.289804	19135.953198	29.299828
354.102304	19140.284429	29.304845
353.923974	19169.301961	29.309863
354.243795	19202.822445	29.314880
354.870783	19226.633219	29.319898
354.719506	19266.375736	29.324916
355.434412	19278.287391	29.329933
355.277001	19316.308236	29.334951
355.900073	19351.487549	29.339968
356.528486	19390.546728	29.344986
356.540560	19425.719952	29.350004
356.961237	19450.887591	29.355021
357.418316	19473.096964	29.360039
357.582227	19516.359763	29.365056
357.865125	19523.153982	29.370074
358.235329	19571.967471	29.375092
358.800480	19606.015693	29.380109
358.654889	19665.549621	29.385127
359.120046	19682.710775	29.390144
359.689932	19726.668389	29.395162
359.908791	19750.687629	29.400180
360.427404	19779.758180	29.405197
360.884702	19837.564846	29.410215
360.970270	19862.581980	29.415232
361.965040	19890.891540	29.420250
362.061951	19942.460887	29.425268
362.765665	19958.928762	29.430285
363.035568	19976.327395	29.435303
363.453392	20006.483715	29.440320
363.939978	20037.327027	29.445338
363.963485	20061.563416	29.450356
364.531489	20097.387085	29.455373
364.625507	20125.566845	29.460391
364.971524	20164.444366	29.465408
365.242598	20203.698484	29.470426
365.599384	20226.740389	29.475444
365.911592	20225.062132	29.480461
366.066435	20290.379433	29.485479
366.281832	20338.016449	29.490496
366.658900	20356.029880	29.495514
366.760611	20402.405889	29.500532
367.180495	20438.715051	29.505549
367.834675	20460.034091	29.510567
368.152266	20501.765526	29.515584
368.444623	20538.152721	29.520602
368.665503	20582.275875	29.525620
369.300539	20619.520917	29.530637
369.634777	20663.650782	29.535655
369.825863	20683.000510	29.540672
370.239285	20711.554115	29.545690
370.849018	20749.952791	29.550708
371.307946	20797.357001	29.555725
371.854000	20830.561237	29.560743
372.126216	20854.855431	29.565760
372.611474	20882.325533	29.570778
372.768118	20935.669393	29.575796
373.285680	20968.790335	29.580813
373.614490	20986.358427	29.585831
373.921068	21011.750640	29.590848
374.740765	21041.252886	29.595866
375.154160	21079.125142	29.600884
375.579045	21111.720978	29.605901
376.087865	21121.066970	29.610919
376.574706	21146.156894	29.615936
376.546547	21187.699673	29.620954
376.823295	21227.328879	29.625972
377.252112	21245.673654	29.630989
377.663732	21280.020244	29.636007
377.700497	21317.058283	29.641024
378.251426	21365.418406	29.646042
378.423748	21405.074744	29.651060
378.777639	21424.885553	29.656077
379.134788	21460.833700	29.661095
379.606014	21496.506121	29.666112
380.308999	21519.943488	29.671130
380.586195	21584.607200	29.676148
380.798408	21620.497659	29.681165
381.406184	21643.884718	29.686183
381.260836	21660.086253	29.691200
381.747807	21696.497430	29.696218
382.274531	21755.852099	29.701236
382.967721	21793.827945	29.706253
382.977384	21828.352418	29.711271
383.470754	21853.798610	29.716288
384.047289	21904.262219	29.721306
384.028804	21949.666062	29.726324
384.462089	21977.234839	29.731341
384.875045	22022.197135	29.736359
385.068100	22065.255230	29.741376
385.530551	22103.714466	29.746394
386.107270	22157.263991	29.751412
386.717643	22181.376561	29.756429
386.949483	22211.490356	29.761447
387.212550	22245.855592	29.766464
388.015964	22293.747888	29.771482
388.243344	22331.420393	29.776500
388.578137	22346.195361	29.781517
388.953300	22390.964676	29.786535
389.470993	22450.471496	29.791552
389.907525	22471.706105	29.796570
390.488601	22506.386672	29.801588
390.618601	22543.456167	29.806605
390.845670	22573.941885	29.811623
390.996356	22600.904115	29.816640
391.691744	22640.877415	29.821658
391.841218	22698.093750	29.826676
392.371534	22719.970600	29.831693
392.953148	22764.864464	29.836711
393.083205	22801.212460	29.841728
394.003376	22812.898847	29.846746
394.488928	22857.588111	29.851764
394.418479	22887.371530	29.856781
395.192966	22895.968338	29.861799
395.654897	22911.474823	29.866816
395.933783	22954.464268	29.871834
395.962573	23007.588337	29.876852
396.304620	23030.078448	29.881869
396.787877	23054.147062	29.886887
396.939299	23094.372114	29.891904
397.322160	23146.507950	29.896922
397.626723	23175.343890	29.901940
398.049433	23210.851406	29.906957
398.549009	23257.940565	29.911975
398.661525	23312.891652	29.916992
399.385443	23346.410481	29.922010
399.289297	23387.027135	29.927028
399.822590	23421.834159	29.932045
400.478706	23463.733065	29.937063
400.574631	23504.229983	29.942080
401.207286	23570.026673	29.947098
401.173894	23596.666169	29.952116
401.857255	23641.520344	29.957133
402.817652	23683.341154	29.962151
402.626059	23739.245702	29.967168
403.280021	23759.999838	29.972186
403.748307	23819.079786	29.977204
404.521299	23844.060272	29.982221
405.325100	23872.341943	29.987239
405.499290	23933.965140	29.992256
405.523816	23951.085237	29.997274
406.666620	23998.691417	30.002292
406.728004	24038.840576	30.007309
407.110177	24053.259203	30.012327
407.486286	24089.159402	30.017344
407.895933	24114.643357	30.022362
408.264576	24154.355748	30.027380
408.355288	24201.161912	30.032397
409.029174	24235.512231	30.037415
409.140012	24268.910287	30.042432
409.606916	24312.548540	30.047450
410.422940	24354.919908	30.052468
410.616623	24402.028111	30.057485
411.314233	24438.129792	30.062503
411.255416	24473.591803	30.067520
411.628496	24504.678123	30.072538
412.072188	24556.352604	30.077556
412.644567	24599.065986	30.082573
412.746651	24651.161410	30.087591
413.196336	24700.148603	30.092608
413.745110	24718.595625	30.097626
414.279772	24742.301823	30.102644
414.503935	24795.288875	30.107661
415.241743	24853.539554	30.112679
415.736102	24877.482804	30.117696
416.667296	24920.246521	30.122714
416.739173	24942.110545	30.127732
417.139258	24969.185158	30.132749
417.710288	25000.556619	30.137767
418.134595	25058.478216	30.142784
418.726650	25082.749353	30.147802
418.833368	25098.609814	30.152820
419.273772	25133.743188	30.157837
420.073266	25179.679702	30.162855
420.072660	25221.629968	30.167872
420.404469	25246.459936	30.172890
420.626347	25258.692276	30.177908
420.838227	25319.607897	30.182925
421.516665	25343.787877	30.187943
421.673739	25388.583840	30.192960
421.981430	25417.703765	30.197978
422.517827	25468.843799	30.202996
422.547576	25516.377957	30.208013
422.901278	25545.249250	30.213031
422.924704	25587.355706	30.218048
423.572355	25630.571722	30.223066
423.804248	25688.156702	30.228084
424.207667	25761.784556	30.233101
424.940908	25788.223596	30.238119
425.192329	25825.964584	30.243136
425.562309	25888.943856	30.248154
426.275526	25939.824304	30.253172
426.328573	25985.435329	30.258189
426.842836	26054.004956	30.263207
427.038949	26096.508319	30.268224
427.771031	26127.437395	30.273242
428.446758	26191.540465	30.278260
428.880635	26250.658235	30.283277
429.779206	26302.728074	30.288295
429.833030	26340.457114	30.293312
430.584847	26391.007699	30.298330
431.207084	26432.219424	30.303348
431.283462	26469.949756	30.308365
431.987686	26530.182854	30.313383
431.961691	26565.093468	30.318400
432.416998	26600.060261	30.323418
433.078129	26652.935192	30.328436
433.553083	26684.007101	30.333453
433.977109	26729.807988	30.338471
434.515421	26777.630655	30.343488
434.936111	26818.267915	30.348506
435.463383	26862.861526	30.353524
435.789322	26900.468008	30.358541
436.273073	26948.407398	30.363559
436.833839	27013.801985	30.368576
436.886974	27044.436454	30.373594
438.007432	27076.421156	30.378612
438.352563	27117.055840	30.383629
438.871125	27168.476739	30.388647
439.233574	27217.368902	30.393664
439.823595	27247.716352	30.398682
440.440630	27259.495348	30.403700
440.862935	27323.103635	30.408717
441.298333	27355.056942	30.413735
441.174404	27396.220786	30.418752
441.910997	27453.791436	30.423770
442.323690	27479.746730	30.428788
442.506430	27512.839650	30.433805
442.939125	27553.687993	30.438823
443.550630	27617.622521	30.443840
444.315582	27649.490402	30.448858
444.740671	27679.351761	30.453876
444.958560	27716.845418	30.458893
445.680268	27773.359853	30.463911
446.075169	27809.361005	30.468928
445.894408	27839.209175	30.473946
446.479459	27886.069972	30.478964
446.689369	27925.435753	30.483981
447.306099	27985.308370	30.488999
447.760435	28032.516029	30.494016
448.160364	28071.286176	30.499034
448.787927	28128.968574	30.504052
449.118862	28183.164418	30.509069
449.712530	28211.078010	30.514087
450.299593	28249.641019	30.519104
450.271648	28309.545559	30.524122
450.575385	28355.605649	30.529140
450.607121	28393.437483	30.534157
451.317765	28444.398365	30.539175
451.778159	28482.922893	30.544192
452.072214	28524.332655	30.549210
452.595567	28582.459602	30.554228
452.908450	28655.395716	30.559245
453.814545	28690.368018	30.564263
454.377989	28720.022238	30.569280
454.414392	28780.012410	30.574298
455.157224	28833.656516	30.579316
455.333314	28873.336012	30.584333
455.778379	28930.953466	30.589351
456.054850	28995.185032	30.594368
456.578145	29028.505344	30.599386
457.265560	29077.330199	30.604404
457.649790	29155.098438	30.609421
458.553130	29194.125469	30.614439
459.046284	29232.879682	30.619456
459.369769	29301.432312	30.624474
460.380269	29329.843489	30.629492
460.839754	29377.612300	30.634509
460.952116	29427.293327	30.639527
461.906908	29458.827242	30.644544
462.492703	29500.979744	30.649562
462.777558	29540.548178	30.654580
463.024415	29585.302431	30.659597
463.360728	29616.225912	30.664615
464.083495	29657.372010	30.669632
463.933489	29708.955108	30.674650
464.502771	29752.659752	30.679668
464.639374	29819.762745	30.684685
465.473761	29885.539443	30.689703
466.185716	29918.325606	30.694720
466.330001	29962.451122	30.699738
466.660784	30024.125611	30.704756
467.185170	30081.402584	30.709773
467.511808	30125.400607	30.714791
468.079431	30191.285620	30.719808
468.598763	30251.437710	30.724826
468.786847	30280.317525	30.729844
469.473669	30330.761118	30.734861
470.043154	30406.453961	30.739879
470.778769	30450.542979	30.744896
471.242584	30504.897659	30.749914
471.672912	30566.387289	30.754932
472.038324	30604.522152	30.759949
472.456210	30656.594697	30.764967
472.915527	30727.196763	30.769984
473.474072	30775.240134	30.775002
474.007967	30822.300325	30.780020
474.148207	30874.163862	30.785037
474.563851	30937.789735	30.790055
475.367361	30962.739342	30.795072
475.431493	31036.158758	30.800090
476.140913	31105.758890	30.805108
476.952334	31153.076980	30.810125
477.594816	31178.113434	30.815143
478.293052	31247.103979	30.820160
478.413076	31309.319434	30.825178
478.979483	31348.356511	30.830196
479.613598	31383.685202	30.835213
480.200691	31425.409979	30.840231
480.754389	31481.954842	30.845248
480.665409	31536.419831	30.850266
481.308876	31570.368748	30.855284
481.672658	31607.335678	30.860301
481.991759	31664.080773	30.865319
482.496140	31731.143012	30.870336
482.428684	31787.658968	30.875354
483.068297	31820.110499	30.880372
483.598914	31864.839527	30.885389
483.777019	31934.906152	30.890407
484.411834	31999.395656	30.895424
484.436247	32057.446313	30.900442
485.090160	32118.882408	30.905460
485.761596	32185.720044	30.910477
486.027982	32229.859531	30.915495
486.650390	32276.580927	30.920512
487.412229	32347.669600	30.925530
487.777564	32400.355457	30.930548
488.315655	32451.517526	30.935565
489.070096	32527.917810	30.940583
490.005117	32573.531474	30.945600
490.606441	32612.764371	30.950618
491.009953	32668.643804	30.955636
491.800871	32712.000630	30.960653
492.198485	32750.781627	30.965671
492.498011	32807.666172	30.970688
492.782917	32871.686659	30.975706
493.847873	32903.379013	30.980724
494.040703	32931.666148	30.985741
494.194409	32996.547982	30.990759
494.893221	33058.711914	30.995776
495.101268	33107.239213	31.000794
495.844104	33171.718349	31.005812
496.119629	33221.367463	31.010829
496.214606	33268.522522	31.015847
497.049454	33332.744114	31.020864
497.433010	33410.099223	31.025882
497.557604	33474.366084	31.030900
498.413493	33519.339031	31.035917
498.487792	33575.780540	31.040935
498.934324	33658.849651	31.045952
499.556382	33741.965883	31.050970
500.620153	33786.864161	31.055988
501.231713	33849.152575	31.061005
501.692447	33913.911354	31.066023
502.355281	33971.048856	31.071040
502.397483	34038.903013	31.076058
503.136882	34064.870991	31.081076
503.666704	34143.820606	31.086093
504.109008	34206.639913	31.091111
505.007864	34256.861043	31.096128
505.388686	34302.444537	31.101146
505.878135	34363.016417	31.106164
506.681819	34429.004614	31.111181
506.860233	34494.976437	31.116199
507.490064	34531.217741	31.121216
507.715790	34599.479161	31.126234
508.349030	34654.844199	31.131252
509.068939	34703.834051	31.136269
509.374334	34786.549993	31.141287
510.039031	34827.175159	31.146304
510.335298	34870.202513	31.151322
510.722639	34930.534469	31.156340
511.208871	35007.990056	31.161357
511.273609	35068.227465	31.166375
512.212479	35111.247079	31.171392
512.975736	35169.996878	31.176410
513.002827	35242.540703	31.181428
513.562978	35325.759806	31.186445
514.078450	35384.809987	31.191463
514.779289	35434.455025	31.196480
515.128550	35498.499653	31.201498
516.038908	35563.344820	31.206516
516.417885	35620.714399	31.211533
516.680501	35673.206121	31.216551
517.100573	35713.848484	31.221568
517.696817	35780.112641	31.226586
518.082419	35851.577362	31.231604
519.037526	35893.545419	31.236621
519.261692	35937.994620	31.241639
520.116596	35998.543283	31.246656
520.597096	36054.373382	31.251674
521.283532	36109.907732	31.256692
521.872505	36159.731052	31.261709
522.331328	36214.220974	31.266727
523.416010	36257.070976	31.271744
524.263464	36287.716688	31.276762
524.567485	36345.722631	31.281780
525.283975	36371.246540	31.286797
525.547918	36423.509900	31.291815
526.036661	36474.066974	31.296832
526.473239	36526.649237	31.301850
526.602242	36585.079318	31.306868
527.197117	36617.682775	31.311885
527.533527	36686.063308	31.316903
528.050458	36728.913556	31.321920
528.393590	36797.817243	31.326938
529.028671	36862.027839	31.331956
529.439358	36903.999848	31.336973
529.799688	36991.750262	31.341991
530.379096	37034.704529	31.347008
530.836950	37116.109129	31.352026
531.244613	37180.724495	31.357044
531.754304	37243.193125	31.362061
532.026075	37323.401824	31.367079
532.412009	37383.874866	31.372096
532.932213	37448.636709	31.377114
533.277988	37523.620758	31.382132
534.113345	37611.825921	31.387149
534.695592	37694.926200	31.392167
535.053650	37753.543167	31.397184
535.518513	37818.438564	31.402202
536.271195	37903.294702	31.407220
537.058294	37992.257642	31.412237
537.548225	38065.519135	31.417255
538.027663	38133.111534	31.422272
538.947714	38202.812136	31.427290
539.509937	38251.563233	31.432308
540.398130	38328.638628	31.437325
540.669786	38398.980437	31.442343
541.219477	38461.295217	31.447360
541.759837	38537.592634	31.452378
542.129942	38597.479058	31.457396
543.007163	38667.071764	31.462413
543.592861	38729.974851	31.467431
543.943918	38794.760018	31.472448
544.713867	38872.693614	31.477466
545.055455	38937.607098	31.482484
545.589804	38984.679468	31.487501
546.036133	39067.799072	31.492519
546.715229	39140.222590	31.497536
547.175902	39189.308605	31.502554
547.182938	39258.864272	31.507572
548.323745	39330.558985	31.512589
548.597898	39424.149030	31.517607
548.946507	39487.068667	31.522624
549.816972	39536.914847	31.527642
550.357466	39614.652835	31.532660
551.477173	39683.515062	31.537677
551.784252	39735.058169	31.542695
552.401859	39801.923865	31.547712
553.246248	39859.665686	31.552730
553.270136	39917.754678	31.557748
554.121978	39972.841268	31.562765
554.421170	40029.310198	31.567783
554.595633	40090.022937	31.572800
555.237339	40151.236296	31.577818
555.521564	40230.385905	31.582836
556.129674	40289.130778	31.587853
557.088918	40355.228773	31.592871
557.466715	40415.186229	31.597888
557.747120	40498.374523	31.602906
558.129828	40574.226814	31.607924
558.824609	40626.323899	31.612941
559.321421	40710.367502	31.617959
559.692256	40792.390143	31.622976
560.532801	40882.387457	31.627994
560.825821	40947.110997	31.633012
561.520444	40995.150066	31.638029
561.799257	41082.681322	31.643047
562.700108	41181.691146	31.648064
563.450580	41253.322212	31.653082
563.638509	41337.760621	31.658100
564.689323	41404.232393	31.663117
564.858874	41477.841536	31.668135
565.715160	41567.527144	31.673152
566.499858	41612.576402	31.678170
567.045964	41717.866016	31.683188
567.734328	41783.903465	31.688205
568.228018	41841.078202	31.693223
568.661371	41921.110134	31.698240
569.280342	41994.486145	31.703258
569.917041	42073.130994	31.708276
570.455697	42133.310586	31.713293
571.169596	42217.899775	31.718311
571.545551	42287.576534	31.723328
572.449805	42356.266665	31.728346
573.059194	42436.991486	31.733364
573.742783	42496.400212	31.738381
574.505632	42562.308216	31.743399
574.659829	42636.025564	31.748416
575.570186	42710.839952	31.753434
576.162205	42770.431995	31.758452
576.929229	42832.590134	31.763469
577.320707	42903.545133	31.768487
577.715010	42983.007314	31.773504
578.624711	43059.802501	31.778522
578.886765	43136.177799	31.783540
579.163643	43185.137632	31.788557
579.922183	43256.017582	31.793575
580.128513	43352.252780	31.798592
580.798562	43428.388281	31.803610
581.294177	43504.290890	31.808628
581.974076	43582.613075	31.813645
582.689763	43654.347666	31.818663
583.285052	43721.016731	31.823680
584.443074	43786.374546	31.828698
584.496530	43896.385979	31.833716
584.936597	43941.384236	31.838733
585.808139	44015.960949	31.843751
586.146991	44102.432814	31.848768
586.888616	44187.326389	31.853786
587.271757	44261.842699	31.858804
587.807737	44323.453682	31.863821
588.571643	44391.385357	31.868839
588.815519	44483.822417	31.873856
589.726639	44566.400926	31.878874
589.836482	44646.450784	31.883892
590.409685	44736.236491	31.888909
591.148744	44793.720837	31.893927
591.681185	44866.469079	31.898944
592.537291	44953.623493	31.903962
592.766652	45040.411426	31.908980
593.308377	45105.016969	31.913997
594.211665	45178.882782	31.919015
594.918695	45251.354287	31.924032
595.322453	45316.886290	31.929050
595.393884	45401.593034	31.934068
596.041181	45490.246209	31.939085
596.662350	45570.695484	31.944103
597.393137	45661.220514	31.949120
598.125309	45750.451304	31.954138
598.496737	45824.697988	31.959156
598.966311	45901.943906	31.964173
599.848190	45984.479879	31.969191
600.469246	46063.207450	31.974208
601.779137	46140.362928	31.979226
602.092730	46239.588476	31.984244
602.641005	46300.395722	31.989261
603.589124	46385.871443	31.994279
603.921354	46474.129839	31.999296
604.641589	46530.340792	32.004314
604.492771	46611.941547	32.009332
605.409548	46720.463125	32.014349
606.235420	46807.504915	32.019367
606.406120	46892.407254	32.024384
607.315978	46956.598473	32.029402
608.292108	47053.391908	32.034420
608.640361	47154.479458	32.039437
609.006686	47228.186322	32.044455
609.935374	47308.952244	32.049472
610.840944	47390.701150	32.054490
611.190101	47484.673383	32.059508
611.788308	47575.870552	32.064525
612.569141	47658.146425	32.069543
612.871654	47731.193251	32.074560
613.412182	47807.797493	32.079578
613.896534	47909.567602	32.084596
614.747512	47992.054381	32.089613
615.440153	48057.857716	32.094631
616.136712	48166.651375	32.099648
616.732273	48233.911227	32.104666
617.378994	48324.219879	32.109684
617.836538	48406.514526	32.114701
619.003665	48494.284553	32.119719
619.538544	48584.758176	32.124736
620.135333	48660.409291	32.129754
620.478123	48745.518922	32.134772
621.061408	48826.449451	32.139789
622.400371	48898.514932	32.144807
623.161208	48978.235798	32.149824
623.471575	49049.969656	32.154842
623.984376	49156.491050	32.159860
624.317866	49229.326987	32.164877
625.635985	49279.614996	32.169895
625.662426	49365.534375	32.174912
626.501113	49455.712521	32.179930
626.930865	49545.627062	32.184948
627.259210	49622.431600	32.189965
627.893019	49722.301552	32.194983
628.478351	49820.320043	32.200000
629.299010	49889.073862	32.205018
629.760122	49965.381018	32.210036
630.382023	50070.680048	32.215053
631.395347	50136.769239	32.220071
632.155023	50231.110485	32.225088
632.734919	50325.718737	32.230106
633.114100	50385.158639	32.235124
633.588513	50459.239207	32.240141
634.305103	50550.765913	32.245159
634.493606	50640.254930	32.250176
635.253733	50712.511332	32.255194
635.902069	50789.305628	32.260212
636.470412	50868.504090	32.265229
637.384929	50955.326130	32.270247
637.863885	51055.964481	32.275264
638.367711	51131.233399	32.280282
639.381910	51217.983325	32.285300
639.726771	51302.106094	32.290317
640.569832	51384.179432	32.295335
641.018396	51490.746601	32.300352
641.139391	51586.757000	32.305370
642.275852	51655.382923	32.310388
642.628206	51763.663445	32.315405
643.423706	51863.776875	32.320423
643.693598	51974.519823	32.325440
644.323158	52060.629647	32.330458
645.383778	52136.429575	32.335476
645.973692	52249.360464	32.340493
646.248963	52347.004123	32.345511
646.482997	52452.443490	32.350528
647.559948	52541.099822	32.355546
648.075691	52650.653269	32.360564
648.627681	52751.184223	32.365581
649.881802	52849.502579	32.370599
650.591878	52952.459378	32.375616
651.237082	53054.088272	32.380634
652.406703	53150.302824	32.385652
652.880505	53232.122881	32.390669
653.884400	53318.801882	32.395687
654.526726	53433.449253	32.400704
655.571129	53516.496523	32.405722
656.388585	53572.734378	32.410740
657.053473	53654.973175	32.415757
657.890379	53747.158537	32.420775
658.362284	53832.999097	32.425792
658.651432	53906.299177	32.430810
659.422908	53991.130763	32.435828
660.101420	54075.295821	32.440845
661.198804	54151.369241	32.445863
661.412582	54250.760425	32.450880
661.875274	54343.060961	32.455898
662.514873	54405.603637	32.460916
663.107026	54494.459553	32.465933
663.642610	54594.348953	32.470951
664.066448	54687.478793	32.475968
664.943764	54774.469495	32.480986
665.725348	54883.056699	32.486004
666.291805	54975.684240	32.491021
666.861566	55055.152366	32.496039
667.329646	55152.269769	32.501056
667.812285	55252.600879	32.506074
668.303493	55358.180994	32.511092
668.827746	55465.992657	32.516109
669.815835	55557.908935	32.521127
670.168701	55664.884483	32.526144
670.537530	55776.141387	32.531162
671.507582	55885.328494	32.536180
672.092052	55982.045417	32.541197
673.027292	56085.458625	32.546215
673.362330	56208.424154	32.551232
674.213880	56310.228683	32.556250
674.928316	56417.635105	32.561268
675.397377	56528.342702	32.566285
676.082388	56636.999821	32.571303
677.143041	56741.394020	32.576320
677.415482	56831.911823	32.581338
678.560484	56932.148465	32.586356
679.093468	57033.826132	32.591373
679.740463	57114.863072	32.596391
680.654837	57214.779108	32.601408
681.517793	57324.636365	32.606426
682.256855	57395.903946	32.611444
682.786164	57502.531815	32.616461
683.400266	57592.326951	32.621479
684.287238	57661.820899	32.626496
684.784555	57775.986963	32.631514
685.695316	57881.264938	32.636532
686.119853	57983.995310	32.641549
686.957144	58058.572551	32.646567
687.510085	58167.007177	32.651584
687.638009	58291.466837	32.656602
688.561088	58382.585654	32.661620
689.024229	58487.618532	32.666637
689.712252	58580.293536	32.671655
690.339515	58703.453825	32.676672
690.600177	58841.770770	32.681690
691.683878	58940.991467	32.686708
692.146207	59042.792228	32.691725
693.134026	59158.224823	32.696743
694.233894	59284.002467	32.701760
694.991033	59396.277211	32.706778
695.617559	59473.403169	32.711796
696.148134	59593.065311	32.716813
696.667374	59718.227545	32.721831
697.391879	59815.824760	32.726848
698.009057	59949.199609	32.731866
699.151373	60068.302284	32.736884
699.755490	60173.491388	32.741901
700.773573	60284.735936	32.746919
701.271733	60401.874296	32.751936
701.862419	60513.190695	32.756954
703.062110	60613.708642	32.761972
703.343539	60737.399906	32.766989
704.660393	60838.133445	32.772007
705.139515	60922.872529	32.777024
705.981133	61033.606914	32.782042
707.074682	61141.108999	32.787060
708.226550	61227.286527	32.792077
708.836251	61338.629644	32.797095
709.300113	61423.316483	32.802112
709.843287	61528.927208	32.807130
710.892935	61627.004070	32.812148
711.928500	61713.954921	32.817165
712.349357	61795.509587	32.822183
712.781730	61907.447580	32.827200
713.403646	62023.348938	32.832218
714.203034	62116.072491	32.837236
715.219760	62200.247872	32.842253
715.485722	62302.141853	32.847271
716.601292	62400.540221	32.852288
717.083738	62513.579269	32.857306
717.663981	62595.704910	32.862324
717.878174	62693.337175	32.867341
718.379023	62807.935843	32.872359
719.447809	62933.577169	32.877376
720.190272	63045.571368	32.882394
720.864723	63131.355551	32.887412
721.207885	63254.521158	32.892429
721.782997	63376.442065	32.897447
722.533579	63487.350298	32.902464
722.966904	63606.376088	32.907482
724.013054	63720.131427	32.912500
724.748882	63819.016524	32.917517
725.326284	63916.531479	32.922535
726.274023	64037.193953	32.927552
727.244204	64150.901041	32.932570
727.960292	64231.083148	32.937588
728.731472	64354.349051	32.942605
729.288748	64456.464856	32.947623
730.099063	64554.841903	32.952640
730.719411	64658.035423	32.957658
731.273355	64777.850829	32.962676
731.701025	64893.806948	32.967693
732.195510	65005.163917	32.972711
733.224746	65118.247212	32.977728
733.337152	65255.431643	32.982746
734.641027	65357.188460	32.987764
735.445790	65488.021551	32.992781
735.698576	65616.184435	32.997799
736.559991	65735.107664	33.002816
736.950963	65847.175263	33.007834
738.233399	65984.822392	33.012852
739.013845	66114.772234	33.017869
739.482105	66239.344709	33.022887
740.381244	66359.384129	33.027904
741.338443	66481.222486	33.032922
742.057259	66611.615467	33.037940
743.080942	66737.218060	33.042957
743.615599	66852.250970	33.047975
744.605524	66983.897371	33.052992
745.443902	67112.364751	33.058010
746.512690	67202.942939	33.063028
747.345006	67317.410932	33.068045
748.060400	67450.635394	33.073063
748.946089	67574.173477	33.078080
749.733096	67688.669963	33.083098
750.616717	67787.834195	33.088116
751.164064	67899.204360	33.093133
751.464949	68030.705681	33.098151
752.690640	68144.272503	33.103168
753.166713	68279.640558	33.108186
754.046665	68377.676635	33.113204
754.442300	68508.198107	33.118221
754.880787	68620.677432	33.123239
755.834859	68741.796248	33.128256
756.249628	68867.657668	33.133274
757.435876	68990.642447	33.138292
758.305858	69133.745809	33.143309
758.867099	69269.555061	33.148327
759.817065	69373.893524	33.153344
760.461277	69515.374100	33.158362
761.107223	69639.830107	33.163380
762.218639	69784.244630	33.168397
762.782111	69907.097388	33.173415
763.760666	69995.040990	33.178432
764.540309	70134.259008	33.183450
765.410247	70263.252651	33.188468
766.164082	70371.497654	33.193485
766.569873	70514.370956	33.198503
767.583412	70641.199940	33.203520
768.327981	70755.821355	33.208538
769.192489	70882.834459	33.213556
770.179426	71008.709038	33.218573
770.612678	71138.159483	33.223591
771.417731	71240.855667	33.228608
772.695706	71368.751789	33.233626
773.129184	71503.793563	33.238644
774.093216	71619.445608	33.243661
775.227338	71729.765487	33.248679
775.988146	71850.567380	33.253696
776.814645	71956.981233	33.258714
777.242604	72061.197885	33.263732
778.161489	72163.354948	33.268749
778.669781	72284.131450	33.273767
779.452213	72391.882548	33.278784
780.195560	72487.962281	33.283802
780.722649	72602.515769	33.288820
781.435280	72718.417635	33.293837
782.493058	72829.906601	33.298855
783.392193	72950.034295	33.303872
783.718947	73083.908656	33.308890
784.541527	73179.523156	33.313908
785.409942	73295.162147	33.318925
785.896521	73433.033802	33.323943
786.851832	73562.185129	33.328960
787.434310	73686.801807	33.333978
787.896192	73806.728285	33.338996
788.369344	73943.992080	33.344013
789.166648	74077.624208	33.349031
790.316354	74213.481718	33.354048
791.120367	74358.730553	33.359066
791.854197	74502.771526	33.364084
792.801611	74610.816384	33.369101
793.496730	74746.942029	33.374119
794.402298	74909.763591	33.379136
795.509244	75032.524519	33.384154
796.061238	75159.209923	33.389172
797.093011	75293.772063	33.394189
797.627823	75441.538876	33.399207
798.499921	75564.360571	33.404224
799.393177	75722.517003	33.409242
799.996275	75874.872915	33.414260
800.871692	75987.084996	33.419277
801.624309	76106.900339	33.424295
802.875242	76270.560442	33.429312
803.574504	76402.724331	33.434330
804.127947	76540.547844	33.439348
805.039262	76668.036460	33.444365
805.703915	76822.722432	33.449383
806.595899	76971.831968	33.454400
807.291323	77111.760569	33.459418
808.418483	77242.777441	33.464436
809.351206	77383.648858	33.469453
810.093508	77518.519194	33.474471
810.994726	77645.515553	33.479488
811.940427	77798.441777	33.484506
812.281237	77935.626145	33.489524
813.322261	78058.908320	33.494541
814.309219	78210.015463	33.499559
815.119173	78338.947238	33.504576
815.973209	78472.647580	33.509594
816.707844	78625.430991	33.514612
817.652603	78754.070975	33.519629
818.532032	78884.057017	33.524647
819.404120	79029.015794	33.529664
819.981726	79148.414945	33.534682
820.778921	79280.719132	33.539700
821.781343	79434.887013	33.544717
822.598205	79589.434478	33.549735
823.286063	79715.175048	33.554752
824.112553	79850.184888	33.559770
824.922466	79993.509410	33.564788
826.001806	80106.259136	33.569805
826.946859	80233.743847	33.574823
827.437205	80377.825703	33.579840
828.217855	80520.532261	33.584858
829.111782	80656.345483	33.589876
830.379800	80780.870384	33.594893
831.041101	80892.314205	33.599911
831.492271	81031.580537	33.604928
832.459800	81168.289245	33.609946
833.167376	81287.279913	33.614964
834.295701	81401.944704	33.619981
834.889242	81533.954331	33.624999
835.556289	81673.865838	33.630016
836.462248	81795.040380	33.635034
836.965989	81946.094574	33.640052
837.780084	82085.275895	33.645069
838.508735	82213.680562	33.650087
839.186713	82346.503358	33.655104
840.170341	82514.131433	33.660122
840.641827	82673.735623	33.665140
841.615945	82799.433602	33.670157
842.208618	82942.414331	33.675175
842.973047	83113.505356	33.680192
843.916612	83275.433375	33.685210
844.577574	83424.953269	33.690228
845.531251	83566.132344	33.695245
846.375503	83719.096922	33.700263
847.417687	83890.141619	33.705280
847.904570	84052.074674	33.710298
848.710590	84203.106679	33.715316
850.079950	84354.622358	33.720333
851.114828	84522.048052	33.725351
852.195526	84679.623571	33.730368
853.200982	84818.480090	33.735386
854.143742	84979.971201	33.740404
854.983328	85126.151382	33.745421
855.617844	85259.941043	33.750439
856.536580	85415.264497	33.755456
857.977262	85560.981260	33.760474
858.598128	85716.912683	33.765492
859.239859	85882.546882	33.770509
860.229314	86027.468027	33.775527
860.787728	86156.669609	33.780544
861.904180	86318.305956	33.785562
862.702060	86479.230488	33.790580
863.685886	86628.553518	33.795597
864.381478	86774.103630	33.800615
865.515917	86941.195201	33.805632
866.332292	87089.340403	33.810650
867.120210	87255.150127	33.815668
867.884583	87385.703878	33.820685
869.061970	87537.563298	33.825703
869.446867	87716.913390	33.830720
870.524857	87879.921020	33.835738
871.185406	88024.175023	33.840756
872.089320	88163.036817	33.845773
873.059763	88340.422141	33.850791
873.806856	88489.840531	33.855808
874.586451	88655.193380	33.860826
875.510553	88847.731828	33.865844
876.247861	88999.667116	33.870861
877.208876	89143.979667	33.875879
877.782738	89322.583218	33.880896
878.901514	89474.654756	33.885914
879.774688	89650.718276	33.890932
881.146692	89805.553331	33.895949
881.797430	89974.999192	33.900967
882.649825	90132.769712	33.905984
883.779166	90278.978783	33.911002
884.492048	90456.137879	33.916020
885.378934	90599.149059	33.921037
886.820664	90767.406906	33.926055
887.844371	90905.720937	33.931072
888.770041	91062.865421	33.936090
889.085982	91207.138918	33.941108
890.476811	91318.689982	33.946125
891.396852	91475.420469	33.951143
891.925234	91626.135202	33.956160
892.874869	91756.619387	33.961178
893.683577	91909.415935	33.966196
894.590844	92060.229066	33.971213
895.395017	92206.617628	33.976231
896.189473	92355.565386	33.981248
897.216693	92502.589751	33.986266
897.523890	92681.927154	33.991284
898.366444	92813.111951	33.996301
899.494834	92956.622701	34.001319
900.212816	93128.421533	34.006336
901.310540	93300.158894	34.011354
901.897434	93461.419153	34.016372
903.115332	93629.835425	34.021389
903.995006	93786.030790	34.026407
904.665812	93938.211179	34.031424
905.432186	94118.255604	34.036442
906.396989	94285.155003	34.041460
907.421953	94454.608867	34.046477
908.093088	94615.926224	34.051495
909.112311	94803.066836	34.056512
910.228996	94967.002831	34.061530
910.941121	95127.740874	34.066548
911.878454	95305.405115	34.071565
912.869798	95492.061961	34.076583
913.733229	95666.873882	34.081600
914.698603	95827.549417	34.086618
915.338975	96006.058969	34.091636
915.986030	96189.505696	34.096653
917.341968	96368.558013	34.101671
917.906086	96550.818537	34.106688
919.087135	96733.788744	34.111706
920.043062	96922.608097	34.116724
920.741679	97104.692287	34.121741
921.936311	97283.936163	34.126759
922.137435	97457.661237	34.131776
923.649534	97648.318586	34.136794
924.231502	97850.512106	34.141812
925.124507	98042.774902	34.146829
926.352606	98211.094531	34.151847
927.322435	98397.188333	34.156864
928.765145	98583.173805	34.161882
929.406779	98774.933070	34.166900
930.278933	98970.966598	34.171917
931.412657	99135.769521	34.176935
932.203535	99331.939585	34.181952
933.204428	99518.125274	34.186970
934.115231	99701.453245	34.191988
934.751837	99899.590329	34.197005
935.941455	100082.444593	34.202023
936.493034	100265.886653	34.207040
937.961571	100462.700701	34.212058
938.607279	100647.877242	34.217076
939.367991	100847.204132	34.222093
940.854180	101028.693220	34.227111
942.026778	101211.780090	34.232128
943.036049	101401.719837	34.237146
944.097632	101588.828827	34.242164
945.167838	101747.664106	34.247181
946.192095	101915.573830	34.252199
946.968130	102110.653792	34.257216
948.038541	102289.878131	34.262234
948.864019	102456.361792	34.267252
950.217278	102628.887897	34.272269
951.273445	102796.886817	34.277287
952.052252	102985.888822	34.282304
952.798751	103128.521395	34.287322
953.935033	103284.430352	34.292340
954.586784	103461.288192	34.297357
955.642441	103631.071779	34.302375
956.082854	103802.028073	34.307392
956.948107	103947.893604	34.312410
957.907497	104128.497773	34.317428
958.638366	104313.604649	34.322445
959.532729	104498.863148	34.327463
959.959254	104690.563472	34.332480
960.819338	104868.010762	34.337498
962.181132	105057.735887	34.342516
962.921061	105257.031018	34.347533
964.178976	105434.821747	34.352551
965.108487	105619.594930	34.357568
966.105021	105833.092399	34.362586
967.005897	106015.125091	34.367604
967.986343	106200.945098	34.372621
969.374786	106405.194878	34.377639
970.042513	106600.504067	34.382656
970.845740	106794.652565	34.387674
971.787900	106983.561870	34.392692
972.798369	107190.761326	34.397709
973.900784	107383.484373	34.402727
975.005889	107583.680504	34.407744
975.893236	107786.940974	34.412762
977.229658	107988.887722	34.417780
978.326709	108170.079796	34.422797
979.755147	108356.828985	34.427815
980.204051	108555.431067	34.432832
981.257256	108746.044476	34.437850
982.377861	108939.029196	34.442868
983.791305	109135.576596	34.447885
984.550113	109316.224425	34.452903
985.502942	109499.526538	34.457920
986.459748	109701.169054	34.462938
987.727154	109894.858418	34.467956
988.667420	110107.323248	34.472973
989.666184	110278.438630	34.477991
990.578065	110473.837452	34.483008
991.317621	110659.513278	34.488026
992.641576	110862.459206	34.493044
993.469017	111070.922464	34.498061
994.412339	111247.727667	34.503079
995.347280	111457.594803	34.508096
996.239248	111659.503414	34.513114
997.483873	111824.698113	34.518132
998.524551	112027.116918	34.523149
999.650209	112239.415980	34.528167
1000.325697	112436.502075	34.533184
1001.341883	112625.578485	34.538202
1002.908008	112813.843395	34.543220
1003.045905	113022.714204	34.548237
1004.687626	113218.911751	34.553255
1005.738562	113411.319369	34.558272
1006.908250	113589.369199	34.563290
1007.963047	113801.274110	34.568308
1008.434834	114016.811179	34.573325
1009.745333	114203.202388	34.578343
1010.917615	114391.796543	34.583360
1011.651331	114572.546966	34.588378
1012.564613	114781.429839	34.593396
1013.074452	114995.435461	34.598413
1013.966855	115202.792130	34.603431
1015.229505	115396.204807	34.608448
1016.032951	115607.899074	34.613466
1017.273472	115823.969426	34.618484
1017.575417	116028.908729	34.623501
1018.903985	116219.947244	34.628519
1019.539922	116426.379904	34.633536
1020.590913	116626.968584	34.638554
1021.739962	116814.518876	34.643572
1022.384802	117021.828619	34.648589
1023.737923	117237.042502	34.653607
1024.667924	117449.249275	34.658624
1025.463294	117666.294207	34.663642
1026.717512	117864.945129	34.668660
1027.926569	118080.265266	34.673677
1029.060800	118292.761415	34.678695
1029.782762	118506.860252	34.683712
1030.388416	118733.611667	34.688730
1031.474677	118961.755255	34.693748
1032.145253	119186.409039	34.698765
1033.773738	119403.405773	34.703783
1034.730834	119641.268737	34.708800
1035.019065	119872.110740	34.713818
1036.357355	120088.983211	34.718836
1036.969335	120341.783997	34.723853
1037.913275	120585.510744	34.728871
1039.467083	120819.572499	34.733888
1040.026509	121075.480062	34.738906
1041.758110	121303.497766	34.743924
1042.531469	121552.126478	34.748941
1043.692473	121784.677032	34.753959
1044.917789	122033.057863	34.758976
1046.263865	122272.183483	34.763994
1047.508850	122498.973111	34.769012
1048.345583	122739.884629	34.774029
1049.864613	122967.899818	34.779047
1051.088713	123202.656149	34.784064
1052.136781	123426.634350	34.789082
1053.382640	123646.970109	34.794100
1054.534220	123864.839370	34.799117
1055.676720	124102.492918	34.804135
1057.134360	124339.310678	34.809152
1057.934990	124561.108050	34.814170
1059.076568	124779.758731	34.819188
1060.008662	125003.033055	34.824205
1061.112863	125220.945481	34.829223
1062.212942	125453.294386	34.834240
1063.125374	125691.721007	34.839258
1064.552358	125896.063214	34.844276
1065.278426	126132.458440	34.849293
1066.547799	126366.484686	34.854311
1067.703690	126589.531171	34.859328
1068.542297	126821.224173	34.864346
1069.780921	127039.596575	34.869364
1070.551981	127275.689210	34.874381
1071.535275	127503.358754	34.879399
1072.445157	127744.945139	34.884416
1073.385195	127966.503928	34.889434
1074.536716	128208.206199	34.894452
1075.330251	128467.370839	34.899469
1075.947610	128695.401236	34.904487
1077.394565	128929.570092	34.909504
1078.452116	129174.362683	34.914522
1079.549776	129434.562635	34.919540
1080.575506	129696.728537	34.924557
1081.810853	129920.470784	34.929575
1083.042402	130150.463891	34.934592
1084.020577	130421.706199	34.939610
1085.025594	130663.756211	34.944628
1085.950148	130919.092095	34.949645
1087.213034	131153.777229	34.954663
1088.410950	131380.121926	34.959680
1089.281013	131630.022324	34.964698
1090.424079	131867.901436	34.969716
1091.356591	132094.320478	34.974733
1092.637686	132351.041557	34.979751
1093.504160	132576.435587	34.984768
1094.530195	132822.187487	34.989786
1095.750093	133060.544635	34.994804
1096.531613	133294.577402	34.999821
1097.734242	133539.481800	35.004839
1098.982178	133770.119967	35.009856
1100.076005	134011.205105	35.014874
1101.382359	134259.685311	35.019892
1102.486128	134507.465666	35.024909
1103.179048	134742.854751	35.029927
1104.572907	134984.607606	35.034944
1105.643467	135252.833918	35.039962
1106.729578	135491.738431	35.044980
1107.946218	135735.998178	35.049997
1108.904470	136002.588607	35.055015
1110.432017	136244.265477	35.060032
1111.396626	136482.487466	35.065050
1112.863925	136742.838843	35.070068
1113.928493	136998.352635	35.075085
1114.894171	137252.312747	35.080103
1115.883034	137491.603032	35.085120
1116.868832	137750.545989	35.090138
1117.715447	138000.576127	35.095156
1118.992318	138262.467035	35.100173
1119.808797	138533.158485	35.105191
1121.214431	138784.268674	35.110208
1121.948104	139080.042867	35.115226
1122.749824	139350.591309	35.120244
1123.802254	139599.116216	35.125261
1125.333647	139868.737009	35.130279
1126.432950	140148.764375	35.135296
1127.610621	140440.306106	35.140314
1129.092549	140700.648279	35.145332
1130.545302	140953.973170	35.150349
1131.489050	141233.566156	35.155367
1132.906800	141504.195151	35.160384
1133.746652	141798.073975	35.165402
1134.872740	142044.119699	35.170420
1136.311720	142315.436357	35.175437
1137.250533	142585.569790	35.180455
1138.803537	142849.860107	35.185472
1139.487567	143135.673926	35.190490
1140.737662	143396.417425	35.195508
1142.283618	143664.227502	35.200525
1142.873239	143953.398530	35.205543
1144.327916	144212.288516	35.210560
1145.270344	144500.530956	35.215578
1146.898368	144753.715636	35.220596
1148.652064	145005.004717	35.225613
1149.674181	145262.388894	35.230631
1151.412307	145519.593375	35.235648
1152.496567	145771.163329	35.240666
1153.189897	146034.339134	35.245684
1154.554097	146291.471517	35.250701
1155.554036	146546.510143	35.255719
1156.918735	146805.408850	35.260736
1158.011858	147067.359716	35.265754
1159.008807	147315.898951	35.270772
1160.114276	147562.380317	35.275789
1161.543215	147827.007840	35.280807
1162.455381	148099.445677	35.285824
1163.537231	148343.171764	35.290842
1164.749153	148575.933734	35.295860
1166.051002	148840.031732	35.300877
1166.843715	149103.873298	35.305895
1167.786162	149356.798264	35.310912
1168.722002	149603.943072	35.315930
1169.760285	149838.910484	35.320948
1170.770370	150113.807715	35.325965
1171.966490	150378.149982	35.330983
1173.338153	150623.454252	35.336000
1174.204518	150889.845791	35.341018
1175.343573	151142.585832	35.346036
1176.723902	151411.470883	35.351053
1177.430925	151691.490368	35.356071
1178.455816	151955.035188	35.361088
1179.626424	152237.759834	35.366106
1180.625455	152516.202713	35.371124
1181.408896	152785.728956	35.376141
1182.794941	153088.007288	35.381159
1184.022943	153387.079893	35.386176
1184.987987	153668.695124	35.391194
1186.392208	153964.267971	35.396212
1187.485406	154264.181547	35.401229
1188.462523	154549.124471	35.406247
1190.281690	154830.848371	35.411264
1191.438305	155142.313400	35.416282
1193.135702	155437.621027	35.421300
1194.264045	155717.905374	35.426317
1195.240305	156015.936740	35.431335
1196.886354	156291.231021	35.436352
1197.934708	156577.864317	35.441370
1199.433300	156881.574881	35.446388
1200.962280	157133.491561	35.451405
1202.265720	157411.108218	35.456423
1203.774460	157706.654616	35.461440
1204.781159	158005.533446	35.466458
1206.159498	158277.803563	35.471476
1207.135492	158541.630305	35.476493
1208.315837	158840.233119	35.481511
1209.616646	159119.054697	35.486528
1210.495093	159403.618294	35.491546
1211.446478	159691.863346	35.496564
1212.761808	159975.610481	35.501581
1213.999018	160289.716496	35.506599
1215.453163	160595.480025	35.511616
1216.771102	160857.679962	35.516634
1218.079485	161130.767662	35.521652
1219.449866	161438.809500	35.526669
1220.490511	161759.543430	35.531687
1222.064622	162030.576245	35.536704
1223.433315	162299.830635	35.541722
1224.336134	162574.974031	35.546740
1225.745080	162867.213136	35.551757
1226.929573	163174.867412	35.556775
1228.334537	163434.900164	35.561792
1229.412812	163710.123673	35.566810
1230.763150	164017.731469	35.571828
1231.766306	164295.330991	35.576845
1233.056844	164595.594548	35.581863
1234.340759	164868.673044	35.586880
1235.205752	165154.458825	35.591898
1235.929771	165475.045437	35.596916
1237.176866	165755.481654	35.601933
1238.043989	166063.831243	35.606951
1239.561332	166385.384910	35.611968
1240.985866	166686.427827	35.616986
1242.461949	166975.360329	35.622004
1243.549260	167262.189341	35.627021
1244.732930	167586.902906	35.632039
1246.254919	167868.703262	35.637056
1247.585305	168172.449258	35.642074
1248.565093	168453.467430	35.647092
1249.967134	168727.413850	35.652109
1251.481618	169014.653400	35.657127
1252.579450	169297.370424	35.662144
1253.736341	169585.890810	35.667162
1254.880254	169867.360419	35.672180
1256.206254	170139.754809	35.677197
1257.378638	170438.238722	35.682215
1259.001050	170732.234674	35.687232
1259.829221	171014.829510	35.692250
1260.600166	171306.520826	35.697268
1262.010331	171590.177911	35.702285
1262.778201	171895.298491	35.707303
1264.076415	172221.549866	35.712320
1265.238006	172531.114389	35.717338
1266.458493	172824.022889	35.722356
1267.958943	173138.662089	35.727373
1268.950818	173478.017716	35.732391
1269.977277	173780.798712	35.737408
1271.290059	174111.895865	35.742426
1272.086702	174450.491394	35.747444
1273.751561	174771.231032	35.752461
1274.784717	175125.413639	35.757479
1276.183875	175454.792909	35.762496
1277.472258	175782.733397	35.767514
1278.725300	176124.184388	35.772532
1280.161293	176457.219336	35.777549
1281.028207	176797.406400	35.782567
1282.529840	177137.795690	35.787584
1283.908384	177497.408562	35.792602
1285.264532	177833.816553	35.797620
1286.976949	178158.606789	35.802637
1288.000960	178521.191951	35.807655
1289.606749	178837.234923	35.812672
1291.010324	179184.723589	35.817690
1292.599858	179531.067194	35.822708
1293.953874	179867.870234	35.827725
1295.077700	180202.061069	35.832743
1296.494710	180537.068765	35.837760
1297.931806	180870.730090	35.842778
1298.642102	181231.153135	35.847796
1300.431995	181549.848159	35.852813
1301.170002	181904.839404	35.857831
1302.264452	182252.083058	35.862848
1303.735465	182597.959651	35.867866
1305.059168	182979.260808	35.872884
1306.885361	183318.153792	35.877901
1308.130120	183654.999979	35.882919
1309.865072	183994.255115	35.887936
1311.500684	184328.451922	35.892954
1312.851582	184656.059724	35.897972
1314.424920	184998.508420	35.902989
1315.556596	185341.552615	35.908007
1316.308280	185677.972715	35.913024
1318.381464	186004.517672	35.918042
1319.537045	186334.440025	35.923060
1320.962826	186683.612958	35.928077
1322.902211	187009.589514	35.933095
1324.014905	187336.136023	35.938112
1325.432723	187662.113706	35.943130
1326.036586	188006.912010	35.948148
1327.753398	188314.172548	35.953165
1328.975009	188662.058985	35.958183
1330.094199	189000.203269	35.963200
1331.469096	189331.084806	35.968218
1332.678563	189659.279172	35.973236
1334.139507	189977.875643	35.978253
1335.847593	190311.919424	35.983271
1337.071833	190639.393481	35.988288
1338.288502	190949.848220	35.993306
1339.579542	191238.865051	35.998324
1340.961890	191562.218139	36.003341
1341.884597	191872.891376	36.008359
1343.319272	192183.735657	36.013376
1345.337294	192489.978882	36.018394
1346.373426	192838.936862	36.023412
1347.917568	193166.220020	36.028429
1349.058033	193473.984165	36.033447
1350.167889	193784.370005	36.038464
1351.531525	194099.615655	36.043482
1352.843577	194457.944207	36.048500
1354.490822	194781.639296	36.053517
1355.749630	195086.396211	36.058535
1356.716788	195425.377155	36.063552
1357.888696	195750.755371	36.068570
1359.210862	196086.545737	36.073588
1360.749509	196424.384173	36.078605
1361.646654	196773.844738	36.083623
1362.691632	197128.881411	36.088640
1364.193240	197470.451275	36.093658
1365.439624	197826.943970	36.098676
1366.925594	198187.195030	36.103693
1368.314509	198539.580275	36.108711
1369.753026	198899.246474	36.113728
1370.966875	199253.467264	36.118746
1372.022898	199643.695455	36.123764
1373.202789	200005.784525	36.128781
1374.506227	200378.862433	36.133799
1375.370593	200741.515433	36.138816
1377.402515	201139.780212	36.143834
1378.271284	201535.636631	36.148852
1379.279799	201904.201146	36.153869
1380.666460	202294.504517	36.158887
1381.887464	202703.031126	36.163904
1383.271218	203089.911515	36.168922
1384.644698	203510.695036	36.173940
1386.230855	203928.906703	36.178957
1387.509839	204319.315401	36.183975
1388.639664	204712.899615	36.188992
1390.340891	205129.232973	36.194010
1391.579683	205555.459627	36.199028
1393.117974	205947.751604	36.204045
1394.679297	206365.105503	36.209063
1396.083999	206782.233678	36.214080
1397.620375	207174.215091	36.219098
1399.034706	207593.593599	36.224116
1400.353968	208015.643838	36.229133
1402.085083	208441.716964	36.234151
1403.614037	208842.558226	36.239168
1405.108853	209241.362936	36.244186
1406.447364	209649.769343	36.249204
1408.068360	210073.165089	36.254221
1409.796566	210464.268240	36.259239
1411.174987	210853.094683	36.264256
1412.654671	211257.080023	36.269274
1414.246547	211655.372983	36.274292
1415.726665	212057.990892	36.279309
1417.340784	212462.048920	36.284327
1419.124507	212856.316232	36.289344
1420.987721	213228.846048	36.294362
1422.133564	213626.460244	36.299380
1423.303313	214000.123752	36.304397
1424.960409	214393.162041	36.309415
1426.013592	214792.777875	36.314432
1427.638804	215169.774424	36.319450
1428.895300	215553.665142	36.324468
1430.474297	215950.151896	36.329485
1432.125094	216307.669780	36.334503
1433.360723	216674.908448	36.339520
1434.959697	217052.298270	36.344538
1435.995576	217440.855747	36.349556
1437.306930	217859.236616	36.354573
1438.980416	218244.060440	36.359591
1440.125515	218601.467555	36.364608
1441.676504	218973.133283	36.369626
1443.059512	219366.974972	36.374644
1444.537429	219736.496922	36.379661
1446.273739	220119.209943	36.384679
1447.705221	220507.308343	36.389696
1449.031968	220869.036938	36.394714
1450.534521	221254.053365	36.399732
1451.693629	221643.674235	36.404749
1452.992758	222009.297426	36.409767
1454.335927	222432.061212	36.414784
1455.798655	222824.989066	36.419802
1457.273766	223231.530040	36.424820
1458.750349	223613.562526	36.429837
1459.783763	224028.180047	36.434855
1461.390450	224417.635792	36.439872
1462.718355	224830.709246	36.444890
1464.337600	225251.101921	36.449908
1465.388983	225668.465783	36.454925
1466.987095	226074.514465	36.459943
1468.479250	226498.666464	36.464960
1470.272470	226917.715837	36.469978
1471.865538	227326.030310	36.474996
1473.231837	227751.909401	36.480013
1475.221648	228170.752978	36.485031
1476.607920	228575.829268	36.490048
1478.279788	228999.300133	36.495066
1479.833843	229404.173656	36.500084
1481.237332	229818.725372	36.505101
1483.037726	230236.489567	36.510119
1484.045026	230656.062405	36.515136
1485.599271	231072.447490	36.520154
1487.029520	231482.402631	36.525172
1488.256908	231909.715652	36.530189
1489.639064	232343.227619	36.535207
1491.154583	232775.144097	36.540224
1492.544555	233198.751172	36.545242
1494.250063	233617.786092	36.550260
1495.547035	234057.388170	36.555277
1497.319007	234484.466702	36.560295
1498.864232	234925.452848	36.565312
1500.596743	235339.712791	36.570330
1502.398297	235773.241960	36.575348
1503.280948	236194.324935	36.580365
1505.006089	236637.165948	36.585383
1506.307763	237074.032517	36.590400
1507.646776	237503.146637	36.595418
1509.153472	237942.521804	36.600436
1510.517604	238401.277644	36.605453
1512.303383	238833.953814	36.610471
1513.534374	239282.116030	36.615488
1514.901333	239705.185359	36.620506
1516.495579	240167.413198	36.625524
1517.987154	240604.612836	36.630541
1520.244676	241030.662629	36.635559
1521.583849	241476.805467	36.640576
1523.715863	241929.524621	36.645594
1525.321514	242366.353692	36.650612
1526.650766	242781.053180	36.655629
1528.057478	243208.670423	36.660647
1529.551296	243656.240318	36.665664
1530.606280	244076.525212	36.670682
1532.270133	244483.475771	36.675700
1533.271836	244927.877846	36.680717
1534.978804	245340.919337	36.685735
1536.160541	245756.181996	36.690752
1537.411077	246195.718815	36.695770
1539.311825	246630.856050	36.700788
1540.622119	247067.386953	36.705805
1542.216138	247516.573064	36.710823
1543.517737	247956.434537	36.715840
1544.557906	248395.653931	36.720858
1546.100747	248852.776187	36.725876
1547.622986	249337.845611	36.730893
1549.390993	249781.849591	36.735911
1550.629383	250230.463257	36.740928
1552.110469	250684.321258	36.745946
1553.713071	251176.010171	36.750964
1555.156236	251657.742652	36.755981
1556.793876	252114.497864	36.760999
1558.173807	252607.851073	36.766016
1559.507919	253079.975429	36.771034
1561.035131	253572.797327	36.776052
1562.332931	254068.782155	36.781069
1564.314501	254562.165122	36.786087
1566.222098	255051.013564	36.791104
1567.856372	255534.395013	36.796122
1569.658789	256038.274868	36.801140
1570.957430	256530.349503	36.806157
1572.589509	257014.214997	36.811175
1574.151685	257526.772573	36.816192
1575.460942	258031.751181	36.821210
1577.019939	258517.128300	36.826228
1578.537599	259047.552456	36.831245
1580.241871	259541.187451	36.836263
1582.057104	260054.390220	36.841280
1583.726652	260563.425598	36.846298
1585.253873	261062.958304	36.851316
1586.904825	261584.266682	36.856333
1588.466554	262080.440526	36.861351
1590.700121	262571.041794	36.866368
1592.244880	263089.116031	36.871386
1594.115847	263594.409313	36.876404
1595.646925	264093.839600	36.881421
1597.644091	264582.498065	36.886439
1599.056784	265096.554471	36.891456
1600.748912	265591.969373	36.896474
1602.691262	266088.181074	36.901492
1603.834429	266590.341723	36.906509
1605.673784	267081.921085	36.911527
1607.102763	267586.828324	36.916544
1608.515051	268094.303682	36.921562
1610.639532	268591.144228	36.926580
1611.979398	269104.346436	36.931597
1613.533624	269595.666124	36.936615
1615.264656	270085.889255	36.941632
1616.984333	270607.511972	36.946650
1618.626092	271106.411241	36.951668
1620.136449	271608.989661	36.956685
1621.647371	272116.774998	36.961703
1623.860720	272611.742319	36.966720
1625.172523	273109.855288	36.971738
1626.766449	273621.206732	36.976756
1627.791237	274133.718247	36.981773
1629.611993	274629.941464	36.986791
1631.390267	275143.800438	36.991808
1632.563373	275668.833986	36.996826
1634.298622	276166.999439	37.001844
1635.564958	276680.025718	37.006861
1637.292207	277204.456964	37.011879
1639.000943	277685.883750	37.016896
1640.215811	278197.747088	37.021914
1642.085625	278684.886367	37.026932
1643.404924	279201.658462	37.031949
1644.756630	279725.257301	37.036967
1646.187019	280217.597180	37.041984
1648.092432	280735.564628	37.047002
1649.718166	281252.281472	37.052020
1651.336408	281764.629128	37.057037
1653.579339	282290.614930	37.062055
1655.273137	282812.447824	37.067072
1656.705390	283318.039869	37.072090
1658.736647	283846.215562	37.077108
1660.321750	284360.339998	37.082125
1661.964639	284877.577850	37.087143
1663.626243	285410.636297	37.092160
1665.260351	285930.539662	37.097178
1666.991730	286452.000276	37.102196
1669.022960	286991.749556	37.107213
1670.321668	287511.957322	37.112231
1672.649748	288033.162015	37.117248
1673.934037	288563.605367	37.122266
1675.912626	289079.834774	37.127284
1677.507757	289623.380854	37.132301
1679.307393	290157.137273	37.137319
1681.434684	290665.360731	37.142336
1682.748600	291210.979293	37.147354
1684.388372	291736.602538	37.152372
1685.999309	292277.595785	37.157389
1687.636163	292815.331335	37.162407
1689.228508	293351.294022	37.167424
1690.921292	293888.126930	37.172442
1692.697593	294414.986994	37.177460
1694.490704	294958.936212	37.182477
1696.449328	295493.635601	37.187495
1698.397749	296052.210019	37.192512
1699.825273	296585.265007	37.197530
1702.056421	297103.580316	37.202548
1703.631653	297644.225937	37.207565
1705.372932	298207.421500	37.212583
1707.317724	298725.903680	37.217600
1709.432268	299261.702924	37.222618
1711.155379	299787.175991	37.227636
1713.412542	300295.592045	37.232653
1715.512681	300807.866761	37.237671
1717.366691	301341.641287	37.242688
1718.881249	301854.388440	37.247706
1720.891167	302358.898472	37.252724
1722.359186	302871.114805	37.257741
1723.727696	303402.875946	37.262759
1725.786383	303913.744939	37.267776
1726.727880	304431.983096	37.272794
1728.473556	304963.546483	37.277812
1729.730303	305497.066956	37.282829
1731.207534	306010.966735	37.287847
1733.316148	306552.213771	37.292864
1735.027347	307087.656469	37.297882
1736.501750	307621.636646	37.302900
1738.232595	308184.853656	37.307917
1739.846696	308721.927951	37.312935
1741.399055	309263.910615	37.317952
1742.444162	309818.620843	37.322970
1744.110104	310402.887558	37.327988
1745.600519	310946.088741	37.333005
1746.719050	311509.867418	37.338023
1748.756575	312087.991439	37.343040
1750.275651	312658.857640	37.348058
1752.128476	313222.681074	37.353076
1753.669805	313791.580093	37.358093
1755.685570	314336.424087	37.363111
1757.648797	314899.760182	37.368128
1759.406204	315469.017604	37.373146
1761.125032	316003.537879	37.378164
1762.967747	316573.204638	37.383181
1764.291073	317146.609441	37.388199
1766.191621	317698.101453	37.393216
1768.193105	318281.568368	37.398234
1769.618121	318867.944324	37.403252
1771.145160	319429.692827	37.408269
1772.920962	320016.001472	37.413287
1774.636990	320603.406963	37.418304
1776.349457	321198.349611	37.423322
1778.162178	321780.803032	37.428340
1779.948378	322392.735879	37.433357
1781.358010	322990.455163	37.438375
1783.197864	323590.916580	37.443392
1784.972382	324212.356482	37.448410
1786.607254	324809.768255	37.453428
1788.393841	325424.897637	37.458445
1790.139728	326055.439880	37.463463
1791.748675	326690.365585	37.468480
1793.397725	327312.761005	37.473498
1795.641807	327942.872098	37.478516
1797.560175	328576.381904	37.483533
1799.254942	329198.268386	37.488551
1801.221449	329843.766166	37.493568
1802.872925	330472.044674	37.498586
1805.142043	331106.384044	37.503604
1806.858718	331758.401693	37.508621
1808.753846	332392.052600	37.513639
1810.991882	333010.458232	37.518656
1812.831871	333639.737848	37.523674
1814.994967	334295.765883	37.528692
1816.906114	334906.741030	37.533709
1818.906668	335534.678279	37.538727
1820.949216	336168.440296	37.543744
1822.812414	336792.324100	37.548762
1824.351496	337403.002954	37.553780
1826.566151	338039.278753	37.558797
1828.171649	338681.689100	37.563815
1830.070153	339298.531756	37.568832
1831.819828	339927.550855	37.573850
1833.830107	340564.439221	37.578868
1836.135341	341186.370848	37.583885
1837.459363	341811.426673	37.588903
1839.334962	342454.989688	37.593920
1840.888638	343094.460229	37.598938
1842.738915	343721.055551	37.603956
1844.757949	344341.904170	37.608973
1846.499217	345003.884003	37.613991
1848.373916	345630.146522	37.619008
1849.902203	346281.230144	37.624026
1851.536678	346940.891574	37.629044
1853.650441	347567.825586	37.634061
1855.114024	348229.883169	37.639079
1857.142292	348878.666225	37.644096
1859.003457	349536.299902	37.649114
1861.030946	350181.181937	37.654132
1863.333829	350814.233817	37.659149
1864.821850	351468.196240	37.664167
1867.155403	352110.285165	37.669184
1868.954216	352738.774625	37.674202
1870.750775	353402.834588	37.679220
1873.154467	354042.574952	37.684237
1874.785984	354668.476341	37.689255
1876.915209	355301.239787	37.694272
1878.848291	355905.504001	37.699290
1880.533927	356491.834779	37.704308
1883.014314	357114.211396	37.709325
1884.625841	357738.422384	37.714343
1886.244092	358334.685922	37.719360
1888.274031	358929.832804	37.724378
1890.080984	359546.575634	37.729396
1891.815332	360169.994493	37.734413
1893.221058	360804.875978	37.739431
1895.453611	361404.267416	37.744448
1897.290805	362015.792423	37.749466
1898.733298	362657.997024	37.754484
1900.766093	363292.406548	37.759501
1902.233150	363935.626967	37.764519
1904.371173	364587.377692	37.769536
1906.254894	365228.098296	37.774554
1907.838497	365863.149812	37.779572
1909.639168	366513.909544	37.784589
1911.541385	367196.175094	37.789607
1913.373588	367857.079991	37.794624
1915.690439	368507.213681	37.799642
1917.144420	369170.771203	37.804660
1919.306313	369850.790419	37.809677
1920.922879	370527.336000	37.814695
1922.839227	371190.959293	37.819712
1925.013159	371877.636416	37.824730
1926.472325	372553.308736	37.829748
1928.748638	373247.045751	37.834765
1930.631921	373953.212179	37.839783
1932.629186	374632.206866	37.844800
1934.691051	375309.351975	37.849818
1937.009407	375995.927691	37.854836
1939.276989	376688.991320	37.859853
1941.185736	377365.488598	37.864871
1943.563250	378051.177822	37.869888
1945.689820	378741.662853	37.874906
1947.609837	379400.467848	37.879924
1949.764240	380079.484176	37.884941
1951.453246	380782.604526	37.889959
1953.609408	381464.458775	37.894976
1955.535862	382132.364817	37.899994
1957.138590	382825.263159	37.905012
1959.415103	383529.370803	37.910029
1960.980695	384193.745429	37.915047
1962.550403	384901.186363	37.920064
1964.446842	385620.348668	37.925082
1966.527493	386315.352139	37.930100
1968.765641	387004.102983	37.935117
1970.332628	387717.036283	37.940135
1972.176652	388443.142685	37.945152
1974.170251	389145.604460	37.950170
1976.349126	389851.670977	37.955188
1977.968392	390576.599778	37.960205
1979.955134	391289.434878	37.965223
1981.792039	392001.594056	37.970240
1983.721976	392738.209800	37.975258
1985.340165	393481.703846	37.980276
1987.521589	394198.445504	37.985293
1989.599484	394914.832643	37.990311
1991.470325	395647.459627	37.995328
1993.866394	396394.024571	38.000346
1995.598268	397117.843524	38.005364
1997.599256	397835.948557	38.010381
1999.998933	398573.917236	38.015399
2001.856688	399319.560337	38.020416
2004.101960	400054.780420	38.025434
2005.706844	400782.408737	38.030452
2007.788463	401478.819565	38.035469
2009.932311	402183.439636	38.040487
2011.663643	402895.611662	38.045504
2013.621585	403599.518296	38.050522
2015.465955	404330.996480	38.055540
2017.773453	405025.713241	38.060557
2019.528209	405739.635031	38.065575
2021.227925	406468.826815	38.070592
2023.085408	407191.588586	38.075610
2025.179411	407923.489968	38.080628
2027.352615	408641.044040	38.085645
2029.843081	409386.041640	38.090663
2031.438021	410107.453299	38.095680
2033.862952	410841.502875	38.100698
2035.723267	411585.277884	38.105716
2037.995852	412299.046395	38.110733
2040.133399	413050.309941	38.115751
2041.760824	413799.686081	38.120768
2044.021888	414554.433483	38.125786
2046.018703	415298.057828	38.130804
2047.755392	416034.662622	38.135821
2049.791814	416807.366625	38.140839
2051.500745	417558.117278	38.145856
2053.761951	418323.090383	38.150874
2055.506344	419118.315171	38.155892
2058.024979	419883.934137	38.160909
2059.997988	420642.276060	38.165927
2062.072047	421429.802787	38.170944
2064.286726	422224.372449	38.175962
2066.406089	422993.559758	38.180980
2068.210399	423770.473328	38.185997
2070.536009	424559.253629	38.191015
2072.447173	425339.873611	38.196032
2074.314815	426137.136315	38.201050
2076.801923	426942.018569	38.206068
2078.634079	427723.588957	38.211085
2080.841538	428516.161248	38.216103
2082.813217	429316.189513	38.221120
2085.309677	430114.788413	38.226138
2087.152641	430934.175726	38.231156
2089.353196	431711.860743	38.236173
2091.604280	432523.937273	38.241191
2093.546608	433348.692828	38.246208
2096.058922	434130.297118	38.251226
2097.708752	434938.694457	38.256244
2099.919605	435761.195112	38.261261
2102.493884	436565.739175	38.266279
2104.480999	437372.224902	38.271296
2106.821921	438186.874024	38.276314
2108.709050	438989.422411	38.281332
2110.700461	439808.930200	38.286349
2113.080526	440611.998147	38.291367
2115.129122	441423.998910	38.296384
2117.349328	442245.000247	38.301402
2119.274196	443059.644401	38.306420
2121.412745	443869.112997	38.311437
2123.655173	444672.766789	38.316455
2125.871293	445493.497393	38.321472
2128.330789	446311.071033	38.326490
2130.741160	447118.706126	38.331508
2133.010226	447903.568734	38.336525
2134.892929	448722.260265	38.341543
2137.036366	449524.335847	38.346560
2139.341160	450327.821958	38.351578
2141.179280	451131.304371	38.356596
2143.339993	451934.501062	38.361613
2145.847638	452744.236156	38.366631
2147.576650	453556.799899	38.371648
2149.227914	454334.447925	38.376666
2151.464981	455107.520071	38.381684
2153.470975	455908.365789	38.386701
2155.176308	456696.992363	38.391719
2157.120482	457499.152408	38.396736
2159.202536	458294.229889	38.401754
2161.112876	459110.289095	38.406772
2163.066064	459897.083818	38.411789
2165.131966	460721.395846	38.416807
2167.018438	461569.162970	38.421824
2169.220233	462386.003455	38.426842
2170.970193	463211.782826	38.431860
2173.362754	464058.097940	38.436877
2175.778923	464906.344747	38.441895
2177.941619	465752.625832	38.446912
2180.756171	466577.786960	38.451930
2182.934500	467425.712383	38.456948
2184.842484	468274.757690	38.461965
2187.342292	469144.086225	38.466983
2189.320733	469989.861378	38.472000
2191.736682	470824.460486	38.477018
2194.036391	471692.141255	38.482036
2195.738589	472545.227761	38.487053
2198.223600	473405.170534	38.492071
2200.366090	474281.147533	38.497088
2202.367150	475156.551708	38.502106
2204.715148	476025.846214	38.507124
2206.613517	476909.875554	38.512141
2208.648386	477803.842861	38.517159
2210.570954	478691.774809	38.522176
2212.524504	479586.932844	38.527194
2214.839356	480504.009747	38.532212
2216.502187	481414.077724	38.537229
2218.994142	482332.650483	38.542247
2221.025831	483244.132359	38.547264
2223.653897	484178.598514	38.552282
2225.625134	485117.416937	38.557300
2228.233916	486037.954387	38.562317
2230.545452	486962.785394	38.567335
2232.374093	487911.680463	38.572352
2234.965615	488858.430301	38.577370
2237.000945	489772.660120	38.582388
2239.247044	490723.708677	38.587405
2241.674627	491692.948600	38.592423
2244.285393	492628.539293	38.597440
2246.327976	493540.754644	38.602458
2248.718682	494484.004070	38.607476
2251.140320	495440.570506	38.612493
2253.321389	496398.940179	38.617511
2255.530192	497338.783187	38.622528
2257.975797	498261.833916	38.627546
2260.430983	499229.182965	38.632564
2262.132220	500189.739622	38.637581
2264.979297	501126.391975	38.642599
2267.040035	502075.733389	38.647616
2269.450992	503032.327977	38.652634
2272.007164	503988.440198	38.657652
2274.129311	504925.251247	38.662669
2276.955132	505861.641022	38.667687
2279.226438	506820.511235	38.672704
2281.373577	507754.484328	38.677722
2283.817590	508695.213051	38.682740
2286.135216	509637.521776	38.687757
2288.248725	510577.389199	38.692775
2290.601327	511527.044307	38.697792
2292.885825	512465.765050	38.702810
2294.995176	513412.928795	38.707828
2297.233334	514340.607816	38.712845
2299.907475	515266.699055	38.717863
2302.066662	516193.829090	38.722880
2304.484469	517091.579770	38.727898
2306.629543	517985.745964	38.732916
2308.911161	518901.659185	38.737933
2311.453351	519816.619035	38.742951
2313.755432	520723.653703	38.747968
2315.867299	521640.743631	38.752986
2318.291893	522546.089247	38.758004
2320.428498	523466.643525	38.763021
2323.184207	524376.612578	38.768039
2325.139993	525289.077176	38.773056
2327.481811	526213.663307	38.778074
2329.988768	527151.311561	38.783092
2332.182400	528092.730527	38.788109
2334.554933	529027.010608	38.793127
2336.655595	529952.917943	38.798144
2338.875709	530890.380037	38.803162
2341.060350	531844.706895	38.808180
2342.866017	532811.923853	38.813197
2345.033737	533749.969003	38.818215
2347.215618	534720.220818	38.823232
2349.325563	535712.619307	38.828250
2351.754115	536714.058718	38.833268
2353.955903	537702.934199	38.838285
2356.249893	538697.866995	38.843303
2358.453141	539719.266962	38.848320
2360.931360	540708.243386	38.853338
2363.464180	541699.708746	38.858356
2365.478302	542716.146264	38.863373
2368.122794	543730.193620	38.868391
2370.484934	544758.703159	38.873408
2373.169837	545768.372038	38.878426
2375.549741	546795.673649	38.883444
2377.799095	547845.705185	38.888461
2380.176020	548874.514355	38.893479
2382.528958	549905.614904	38.898496
2385.157623	550934.028793	38.903514
2387.421266	551976.203004	38.908532
2389.754844	553026.431476	38.913549
2391.931254	554060.769543	38.918567
2394.310028	555119.325884	38.923584
2396.488781	556187.935993	38.928602
2399.058821	557233.026090	38.933620
2401.264569	558294.278006	38.938637
2403.908634	559353.213032	38.943655
2406.471961	560439.211991	38.948672
2408.813682	561496.620124	38.953690
2411.640804	562550.698966	38.958708
2413.627100	563625.178400	38.963725
2416.324090	564710.303422	38.968743
2418.302994	565792.393324	38.973760
2420.739706	566851.114746	38.978778
2423.614242	567920.174116	38.983796
2425.820848	569020.490034	38.988813
2428.333494	570098.920360	38.993831
2430.972512	571186.327288	38.998848
2432.904533	572271.098019	39.003866
2435.921963	573365.487157	39.008884
2437.928261	574445.442857	39.013901
2440.184612	575519.845047	39.018919
2442.297873	576624.893637	39.023936
2444.911615	577706.428474	39.028954
2447.512124	578805.835994	39.033972
2449.696982	579921.220738	39.038989
2452.218822	581020.898056	39.044007
2454.931042	582107.604757	39.049024
2457.215004	583206.224763	39.054042
2459.697966	584270.558502	39.059060
2461.997289	585342.653998	39.064077
2464.873837	586401.121318	39.069095
2467.394834	587459.856404	39.074112
2469.564748	588529.537502	39.079130
2472.167709	589614.092939	39.084148
2474.217091	590686.260521	39.089165
2477.221475	591745.844664	39.094183
2479.506086	592814.224961	39.099200
2481.381658	593902.172476	39.104218
2484.127553	594983.062203	39.109236
2486.469578	596079.252726	39.114253
2489.362325	597174.599682	39.119271
2491.497480	598254.539973	39.124288
2494.233896	599332.829313	39.129306
2497.124476	600438.542313	39.134324
2499.270987	601567.862346	39.139341
2501.742752	602660.562354	39.144359
2504.279126	603765.516907	39.149376
2506.693204	604888.160331	39.154394
2509.039239	606010.705560	39.159412
2511.283308	607140.516456	39.164429
2514.306773	608240.905917	39.169447
2516.802260	609369.703990	39.174464
2518.980343	610522.513326	39.179482
2522.082114	611666.596460	39.184500
2524.363751	612802.693342	39.189517
2526.653540	613936.873035	39.194535
2529.219189	615095.604051	39.199552
2531.616623	616255.442954	39.204570
2534.086214	617415.799202	39.209588
2536.320629	618586.424361	39.214605
2538.890788	619761.970369	39.219623
2541.521004	620918.332023	39.224640
2543.870211	622109.712329	39.229658
2546.362576	623310.936424	39.234676
2548.657958	624498.215836	39.239693
2551.132320	625680.088451	39.244711
2553.918352	626884.316899	39.249728
2556.390923	628109.397387	39.254746
2558.780096	629333.652427	39.259764
2561.394863	630533.553096	39.264781
2564.184501	631735.287767	39.269799
2566.948635	632958.115773	39.274816
2569.267120	634174.683961	39.279834
2572.238780	635394.349471	39.284852
2574.802562	636629.217401	39.289869
2577.228272	637867.057409	39.294887
2580.276330	639059.377653	39.299904
2582.359686	640269.536831	39.304922
2585.290596	641502.219587	39.309940
2587.623256	642741.789156	39.314957
2590.278363	643973.573218	39.319975
2592.952413	645217.726715	39.324992
2595.592247	646468.467687	39.330010
2598.205357	647690.633351	39.335028
2600.944958	648924.997326	39.340045
2603.435148	650153.318604	39.345063
2606.341201	651403.904924	39.350080
2609.000591	652640.070387	39.355098
2611.403875	653872.536906	39.360116
2613.882036	655123.974869	39.365133
2616.675506	656356.667549	39.370151
2619.419415	657588.417839	39.375168
2621.933909	658834.000390	39.380186
2624.364375	660056.975426	39.385204
2627.047455	661313.621839	39.390221
2629.678850	662567.027803	39.395239
2632.318131	663770.182858	39.400256
2634.404558	664987.119672	39.405274
2637.180934	666183.779253	39.410292
2639.852690	667397.130143	39.415309
2642.463072	668627.257918	39.420327
2645.188460	669830.986147	39.425344
2647.547241	671060.792556	39.430362
2650.510967	672261.985361	39.435380
2653.383893	673484.528344	39.440397
2655.701079	674719.288795	39.445415
2657.994383	675949.316580	39.450432
2660.368791	677173.849907	39.455450
2663.219470	678402.121614	39.460468
2665.808027	679670.189147	39.465485
2667.954992	680932.838695	39.470503
2670.844189	682191.516646	39.475520
2673.386395	683470.451559	39.480538
2676.159407	684733.273460	39.485556
2678.765068	686010.403787	39.490573
2681.146839	687306.464134	39.495591
2683.980191	688581.061739	39.500608
2686.643029	689874.425725	39.505626
2689.520440	691172.583647	39.510644
2691.644493	692481.698361	39.515661
2694.339828	693793.853572	39.520679
2697.399501	695109.676804	39.525696
2699.619877	696439.386320	39.530714
2702.843087	697764.217691	39.535732
2705.968564	699109.699323	39.540749
2708.494792	700432.708771	39.545767
2711.214625	701755.041428	39.550784
2713.831891	703074.514710	39.555802
2716.619357	704423.602209	39.560820
2719.498470	705785.500837	39.565837
2722.037102	707130.393713	39.570855
2724.681391	708457.619933	39.575872
2727.316595	709818.974329	39.580890
2729.850759	711174.483477	39.585908
2732.665039	712550.185406	39.590925
2735.541448	713926.051806	39.595943
2738.256595	715289.890297	39.600960
2740.733862	716656.122873	39.605978
2743.702424	718054.322229	39.610996
2746.738897	719428.378204	39.616013
2749.159566	720787.270552	39.621031
2752.378365	722186.225427	39.626048
2754.954112	723578.523257	39.631066
2757.712899	724950.579942	39.636084
2761.094999	726326.558861	39.641101
2763.722980	727718.993255	39.646119
2766.852451	729102.460094	39.651136
2769.760121	730465.370347	39.656154
2772.479842	731846.415241	39.661172
2775.227265	733241.695997	39.666189
2778.095580	734624.023486	39.671207
2781.081419	735984.564356	39.676224
2783.722289	737348.142154	39.681242
2786.648118	738737.557032	39.686260
2789.404238	740122.464965	39.691277
2792.072916	741504.383762	39.696295
2794.873509	742895.909353	39.701312
2797.669556	744269.777432	39.706330
2800.499658	745636.594688	39.711348
2803.418161	747015.390806	39.716365
2805.606209	748428.284378	39.721383
2808.420035	749831.749367	39.726400
2811.197690	751205.296199	39.731418
2814.042121	752571.690473	39.736436
2816.720718	753941.763984	39.741453
2819.313139	755321.658716	39.746471
2821.842378	756666.149478	39.751488
2824.602937	758008.200186	39.756506
2827.411606	759386.147862	39.761524
2830.242380	760770.292206	39.766541
2833.231404	762134.914256	39.771559
2835.843248	763480.948502	39.776576
2839.056048	764858.133232	39.781594
2841.587457	766232.473226	39.786612
2844.112256	767622.596913	39.791629
2846.719013	769035.462778	39.796647
2849.805219	770449.654090	39.801664
2852.393838	771842.669513	39.806682
2855.170669	773264.241340	39.811700
2858.274419	774669.074589	39.816717
2861.126831	776078.250546	39.821735
2864.343936	777488.766363	39.826752
2867.224895	778922.097922	39.831770
2870.128354	780348.712672	39.836788
2873.505902	781766.084730	39.841805
2876.115171	783183.993751	39.846823
2879.331285	784620.171489	39.851840
2881.783708	786050.694406	39.856858
2884.772779	787501.200126	39.861876
2887.690285	788938.379405	39.866893
2890.143891	790388.339053	39.871911
2893.288143	791833.870048	39.876928
2895.820679	793304.496735	39.881946
2898.532211	794793.065242	39.886964
2901.725471	796239.844013	39.891981
2904.585035	797717.775874	39.896999
2907.405049	799192.121617	39.902016
2910.296933	800689.154884	39.907034
2913.134003	802180.246251	39.912052
2916.101447	803671.778739	39.917069
2918.917430	805182.389597	39.922087
2921.777803	806671.628190	39.927104
2925.329227	808159.647674	39.932122
2927.887975	809680.511469	39.937140
2930.714487	811208.422708	39.942157
2933.256797	812721.278098	39.947175
2936.596113	814217.735697	39.952192
2939.491043	815757.754710	39.957210
2942.226681	817290.366227	39.962228
2945.328217	818828.475990	39.967245
2948.091635	820374.098816	39.972263
2950.774089	821917.327078	39.977280
2953.539612	823464.038318	39.982298
2956.282282	825002.782200	39.987316
2959.106895	826578.708491	39.992333
2961.685867	828169.072340	39.997351
2964.643020	829746.070228	40.002368
2967.920139	831308.793999	40.007386
2971.034319	832873.508749	40.012404
2973.961113	834462.136570	40.017421
2977.009351	836036.085279	40.022439
2980.165993	837631.688402	40.027456
2982.971126	839234.839280	40.032474
2986.156056	840801.320154	40.037492
2989.181439	842367.540585	40.042509
2991.982267	843970.914909	40.047527
2994.618657	845568.902637	40.052544
2997.726126	847167.673181	40.057562
3000.434872	848764.743158	40.062580
3003.622185	850363.952408	40.067597
3006.497204	851966.108196	40.072615
3009.183997	853571.283523	40.077632
3012.105468	855152.991580	40.082650
3015.184749	856721.164028	40.087668
3018.221464	858278.754530	40.092685
3020.735510	859843.509121	40.097703
3023.780345	861414.374363	40.102720
3026.886678	863001.022877	40.107738
3029.901173	864573.118009	40.112756
3033.052731	866149.824896	40.117773
3036.286363	867755.665448	40.122791
3039.078326	869352.917106	40.127808
3041.961407	870954.863755	40.132826
3044.709509	872559.503932	40.137844
3048.025577	874153.552666	40.142861
3050.465380	875766.578941	40.147879
3053.543651	877405.669536	40.152896
3056.607377	879035.410539	40.157914
3059.467226	880685.139028	40.162932
3062.773945	882328.144759	40.167949
3065.666441	883991.054100	40.172967
3068.750826	885636.647807	40.177984
3071.659801	887290.112670	40.183002
3074.619856	888966.563199	40.188020
3077.464825	890637.141576	40.193037
3080.353738	892344.769894	40.198055
3083.247933	894045.330112	40.203072
3086.719269	895744.712211	40.208090
3089.628794	897445.224175	40.213108
3092.828388	899144.987839	40.218125
3095.956246	900875.089878	40.223143
3098.971959	902611.424445	40.228160
3102.192033	904340.064243	40.233178
3105.091111	906079.970222	40.238196
3108.273018	907811.782084	40.243213
3111.235575	909543.862296	40.248231
3113.979095	911318.624725	40.253248
3117.408388	913081.071636	40.258266
3120.457377	914845.133379	40.263284
3123.654424	916602.167357	40.268301
3126.838100	918380.253785	40.273319
3129.787733	920136.290335	40.278336
3133.426453	921888.767410	40.283354
3136.520810	923673.876268	40.288372
3139.995264	925449.603608	40.293389
3143.551743	927224.444851	40.298407
3146.642074	929010.568526	40.303424
3150.179699	930783.084651	40.308442
3153.495025	932541.731568	40.313460
3156.399757	934299.289898	40.318477
3159.655728	936077.270881	40.323495
3162.497513	937874.533515	40.328512
3165.652550	939634.677965	40.333530
3168.631385	941402.103799	40.338548
3171.953023	943188.476296	40.343565
3174.969319	944995.027382	40.348583
3177.729000	946789.526733	40.353600
3181.296481	948572.000235	40.358618
3184.456323	950381.327510	40.363636
3187.589603	952163.392728	40.368653
3190.622642	953964.127897	40.373671
3193.939517	955762.655036	40.378688
3197.102460	957610.467038	40.383706
3200.244130	959466.262509	40.388724
3203.357554	961326.941076	40.393741
3206.171096	963179.249386	40.398759
3209.341176	965029.828643	40.403776
3212.588686	966904.414897	40.408794
3215.603417	968795.809330	40.413812
3218.612644	970631.918656	40.418829
3221.735361	972449.759630	40.423847
3224.815030	974289.371012	40.428864
3228.306479	976127.251421	40.433882
3230.786351	977947.745507	40.438900
3234.351882	979771.282497	40.443917
3237.893496	981615.285990	40.448935
3240.730833	983445.369636	40.453952
3244.196998	985271.257816	40.458970
3247.111894	987134.417340	40.463988
3250.240693	988993.137699	40.469005
3253.469460	990854.444622	40.474023
3256.296209	992727.266098	40.479040
3259.536434	994603.387747	40.484058
3262.852595	996475.573138	40.489076
3266.092217	998360.073019	40.494093
3269.676914	1000278.362857	40.499111
3272.920215	1002188.196088	40.504128
3276.468457	1004065.407538	40.509146
3279.486442	1005981.081035	40.514164
3282.503439	1007895.135253	40.519181
3285.894629	1009813.228932	40.524199
3289.097238	1011756.188673	40.529216
3292.716421	1013677.096677	40.534234
3295.779169	1015620.392766	40.539252
3298.863964	1017556.140124	40.544269
3302.374923	1019517.183357	40.549287
3305.292601	1021491.279900	40.554304
3308.847629	1023443.494035	40.559322
3312.194066	1025407.243349	40.564340
3315.202240	1027383.985849	40.569357
3318.522504	1029363.939138	40.574375
3321.627036	1031357.422468	40.579392
3325.006761	1033347.542047	40.584410
3327.976038	1035344.739306	40.589428
3331.289975	1037344.347381	40.594445
3334.842106	1039355.348567	40.599463
3338.348586	1041375.462706	40.604480
3342.043701	1043373.996642	40.609498
3345.631611	1045408.818939	40.614516
3348.923429	1047417.714394	40.619533
3352.649472	1049421.381960	40.624551
3355.945415	1051462.788237	40.629568
3359.252306	1053493.627881	40.634586
3362.283942	1055497.516518	40.639604
3365.892521	1057503.369975	40.644621
3369.553783	1059545.188660	40.649639
3372.824399	1061584.105710	40.654656
3376.136798	1063601.233905	40.659674
3379.718946	1065626.023506	40.664692
3383.249218	1067647.196945	40.669709
3386.894984	1069686.692048	40.674727
3390.010117	1071712.860908	40.679744
3393.559132	1073746.546292	40.684762
3396.420177	1075792.234443	40.689780
3400.100407	1077808.867815	40.694797
3403.356262	1079842.631616	40.699815
3406.519157	1081892.972719	40.704832
3410.375605	1083924.253687	40.709850
3413.679693	1085980.876340	40.714868
3416.729046	1088031.410664	40.719885
3420.301165	1090078.696457	40.724903
3423.433137	1092115.444934	40.729920
3426.678735	1094156.756454	40.734938
3430.151626	1096231.428769	40.739956
3433.590074	1098303.403468	40.744973
3437.138539	1100360.356533	40.749991
3440.115072	1102421.958986	40.755008
3443.363451	1104463.305316	40.760013
3446.834954	1106458.429180	40.765018
3450.090447	1108390.318448	40.770023
3453.590865	1110274.997398	40.775028
3456.359310	1112080.429760	40.780032
3459.791226	1113810.470546	40.785037
3463.078698	1115455.695351	40.790042
3465.732874	1117021.695090	40.795047
3468.762855	1118528.383042	40.800052
3471.314840	1119951.467009	40.805056
3473.867241	1121297.886970	40.810061
3476.659451	1122561.376823	40.815066
3479.141522	1123740.086563	40.820071
3481.612156	1124848.965438	40.825076
3483.726525	1125912.854215	40.830080
3486.089685	1126906.658696	40.835085
3487.832755	1127802.309725	40.840090
3489.965466	1128629.459200	40.845095
3491.950077	1129419.323152	40.850100
3493.514195	1130169.300734	40.855104
3495.514067	1130801.502011	40.860109
3497.220551	1131400.216098	40.865114
3498.551269	1131965.087663	40.870119
3500.411626	1132474.499612	40.875124
3501.784370	1132923.788801	40.880128
3503.027888	1133314.336818	40.885133
3504.096885	1133679.800329	40.890138
3505.008141	1134001.939545	40.895143
3506.398146	1134278.092340	40.900148
3507.398262	1134536.529617	40.905152
3508.252102	1134749.949421	40.910157
3509.650118	1134930.022866	40.915162
3510.023993	1135059.912966	40.920167
3511.065387	1135159.767900	40.925172
3511.776846	1135259.865265	40.930176
3512.795129	1135325.144733	40.935181
3513.496061	1135345.451735	40.940186
3514.152149	1135355.602402	40.945191
3514.902101	1135330.402227	40.950196
3515.247692	1135291.400219	40.955200
3515.780866	1135202.497445	40.960205
3516.057573	1135134.533562	40.965210
3516.687126	1135052.546775	40.970215
3517.185108	1134923.178039	40.975220
3517.483453	1134794.979003	40.980224
3517.774967	1134633.337999	40.985229
3518.293318	1134480.300007	40.990234
3518.717643	1134317.107469	40.995239
3519.486001	1134116.324628	41.000244
3519.456513	1133925.356939	41.005248
3519.957638	1133689.922171	41.010253
3520.536518	1133454.654221	41.015258
3520.697006	1133222.580615	41.020263
3521.235512	1132975.609978	41.025268
3521.305002	1132699.054325	41.030272
3521.461047	1132426.651787	41.035277
3521.718566	1132152.792920	41.040282
3521.673861	1131851.215201	41.045287
3522.313367	1131561.674781	41.050292
3522.284228	1131266.905355	41.055296
3522.287335	1130964.128765	41.060301
3522.586772	1130644.078222	41.065306
3522.741548	1130318.042396	41.070311
3522.539015	1129987.291290	41.075316
3523.014850	1129651.938723	41.080320
3523.301787	1129311.936490	41.085325
3522.963294	1128979.338368	41.090330
3523.317606	1128625.491531	41.095335
3523.671333	1128260.112505	41.100340
3523.484694	1127908.875269	41.105344
3523.690222	1127564.114034	41.110349
3523.552715	1127196.935642	41.115354
3523.728331	1126813.506630	41.120359
3524.083785	1126434.397190	41.125364
3524.266918	1126084.025462	41.130368
3524.333078	1125694.539421	41.135373
3524.103355	1125298.126501	41.140378
3524.014668	1124904.040256	41.145383
3524.550116	1124524.765525	41.150388
3524.400910	1124145.576621	41.155392
3524.733600	1123738.865409	41.160397
3524.362432	1123330.620722	41.165402
3524.508708	1122937.397868	41.170407
3524.821356	1122548.308185	41.175412
3524.460051	1122147.017410	41.180416
3524.591651	1121718.188939	41.185421
3524.789074	1121321.981903	41.190426
3524.645910	1120925.801609	41.195431
3524.918383	1120505.424726	41.200436
3524.523644	1120088.458795	41.205440
3524.677095	1119660.509608	41.210445
3524.652366	1119260.375780	41.215450
3524.571343	1118844.880948	41.220455
3524.768798	1118438.169905	41.225460
3524.617643	1118032.533651	41.230464
3524.483414	1117609.423305	41.235469
3524.908116	1117196.957666	41.240474
3524.845914	1116789.878314	41.245479
3525.135483	1116342.291859	41.250484
3525.103445	1115918.268544	41.255488
3524.948773	1115492.801770	41.260493
3525.213371	1115055.599586	41.265498
3524.951610	1114631.607719	41.270503
3524.973903	1114184.743425	41.275508
3524.712029	1113783.476681	41.280512
3524.810927	1113335.575347	41.285517
3524.928620	1112916.059044	41.290522
3524.574066	1112483.327855	41.295527
3524.748972	1112067.647047	41.300532
3524.567020	1111620.125895	41.305536
3524.438589	1111196.413164	41.310541
3524.486105	1110761.664115	41.315546
3524.405694	1110329.573105	41.320551
3524.630705	1109927.842627	41.325556
3524.352065	1109513.756901	41.330560
3524.357403	1109069.715001	41.335565
3524.729211	1108629.871948	41.340570
3524.412562	1108204.426994	41.345575
3524.814986	1107762.312170	41.350580
3524.522559	1107337.749504	41.355584
3524.415737	1106913.982229	41.360589
3524.460305	1106498.083277	41.365594
3524.415588	1106059.626845	41.370599
3524.458311	1105625.609613	41.375604
3524.106829	1105193.150736	41.380608
3524.316289	1104741.458334	41.385613
3524.832970	1104309.549847	41.390618
3524.575078	1103885.282602	41.395623
3524.286993	1103439.773688	41.400628
3524.054733	1102996.607860	41.405632
3524.331722	1102563.834565	41.410637
3524.321503	1102152.196697	41.415642
3523.897449	1101720.235842	41.420647
3524.198949	1101274.833408	41.425652
3524.101395	1100836.056472	41.430656
3523.986356	1100415.603716	41.435661
3523.826705	1099984.320916	41.440666
3523.569157	1099554.645422	41.445671
3524.069745	1099104.632557	41.450676
3524.066232	1098679.244711	41.455680
3523.949513	1098249.250974	41.460685
3523.900398	1097820.742387	41.465690
3524.103022	1097380.391900	41.470695
3523.892232	1096942.943773	41.475700
3523.847561	1096522.080882	41.480704
3523.920657	1096093.032615	41.485709
3523.965705	1095648.644067	41.490714
3523.888343	1095214.574916	41.495719
3524.143370	1094769.983983	41.500724
3524.085673	1094336.511188	41.505728
3523.562606	1093904.611938	41.510733
3523.716905	1093481.278271	41.515738
3523.418231	1093049.561106	41.520743
3523.835751	1092599.595429	41.525748
3523.474575	1092173.372116	41.530752
3523.517569	1091761.508799	41.535757
3523.718416	1091332.349738	41.540762
3523.676847	1090896.013378	41.545767
3523.880102	1090439.678322	41.550772
3523.459931	1090030.633463	41.555776
3523.783847	1089600.934063	41.560781
3523.578190	1089161.611309	41.565786
3523.183707	1088729.661903	41.570791
3523.557472	1088284.232201	41.575796
3523.208856	1087861.213567	41.580800
3523.148819	1087414.634070	41.585805
3523.191558	1087000.876191	41.590810
3523.230859	1086575.009881	41.595815
3523.611039	1086117.899203	41.600820
3523.079565	1085697.138811	41.605824
3523.185218	1085274.323408	41.610829
3523.609490	1084838.957778	41.615834
3523.068698	1084410.428684	41.620839
3523.250104	1083965.635834	41.625844
3523.058431	1083542.063544	41.630848
3522.999757	1083099.637172	41.635853
3522.981442	1082679.709934	41.640858
3522.757680	1082259.016730	41.645863
3523.014158	1081835.429782	41.650868
3522.786597	1081415.919299	41.655872
3522.890844	1080989.029554	41.660877
3522.702148	1080554.094052	41.665882
3522.630594	1080123.998885	41.670887
3522.543547	1079693.200535	41.675892
3522.370492	1079293.384473	41.680896
3522.408036	1078860.388258	41.685901
3522.394012	1078453.573254	41.690906
3522.310054	1078032.146901	41.695911
3522.588310	1077596.802741	41.700916
3522.455839	1077166.868595	41.705920
3522.750343	1076758.532241	41.710925
3522.114623	1076316.706813	41.715930
3522.342689	1075909.374323	41.720935
3522.460460	1075492.712963	41.725940
3522.119862	1075065.433148	41.730944
3521.932746	1074638.574976	41.735949
3522.174647	1074224.005959	41.740954
3521.865339	1073797.678710	41.745959
3522.175055	1073385.244772	41.750964
3521.964344	1072990.546487	41.755968
3522.122823	1072561.547489	41.760973
3522.284864	1072126.171202	41.765978
3521.437613	1071716.685324	41.770983
3522.196895	1071295.850196	41.775988
3521.715376	1070904.025870	41.780992
3521.703877	1070465.950715	41.785997
3521.869958	1070044.059659	41.791002
3521.609809	1069647.494100	41.796007
3521.443160	1069234.729893	41.801012
3521.409838	1068832.010017	41.806016
3521.598189	1068414.605844	41.811021
3521.681222	1068003.535132	41.816026
3521.397955	1067588.742656	41.821031
3521.546664	1067166.055929	41.826036
3521.446610	1066765.119210	41.831040
3521.277330	1066354.062703	41.836045
3521.486613	1065950.033045	41.841050
3521.456758	1065540.432125	41.846055
3521.613770	1065128.364132	41.851060
3521.307720	1064721.634555	41.856064
3520.901482	1064315.757568	41.861069
3521.471832	1063908.342237	41.866074
3520.867217	1063494.929678	41.871079
3521.593221	1063082.999663	41.876084
3521.190597	1062683.740193	41.881088
3521.158331	1062273.222248	41.886093
3521.247563	1061867.468026	41.891098
3520.696764	1061476.426022	41.896103
3521.118983	1061061.794787	41.901108
3520.965632	1060652.427789	41.906112
3520.942330	1060254.470487	41.911117
3521.212293	1059844.106839	41.916122
3520.594649	1059430.198274	41.921127
3520.730035	1059038.484746	41.926132
3520.470393	1058649.024336	41.931136
3520.412030	1058254.203976	41.936141
3520.582350	1057853.343511	41.941146
3520.484866	1057457.027139	41.946151
3520.742471	1057039.903927	41.951156
3520.685562	1056648.437718	41.956160
3520.456918	1056243.381660	41.961165
3520.737492	1055846.019794	41.966170
3520.299858	1055455.399168	41.971175
3520.733026	1055053.906374	41.976180
3520.497009	1054657.411682	41.981184
3520.531950	1054263.350812	41.986189
3520.232004	1053864.399198	41.991194
3519.998779	1053465.311338	41.996199
3520.212482	1053087.916677	42.001204
3520.129838	1052693.956095	42.006208
3519.993054	1052301.326707	42.011213
3519.953691	1051893.412482	42.016218
3519.750661	1051521.767209	42.021223
3519.876577	1051134.606836	42.026228
3519.925872	1050739.713456	42.031232
3519.988437	1050356.078850	42.036237
3520.147633	1049968.155947	42.041242
3519.791203	1049575.079673	42.046247
3519.738782	1049171.598951	42.051252
3519.815298	1048805.708711	42.056256
3519.656475	1048417.729528	42.061261
3519.743444	1048033.061188	42.066266
3519.326589	1047651.827858	42.071271
3520.012401	1047254.360660	42.076276
3519.957944	1046872.917504	42.081280
3519.637496	1046493.616126	42.086285
3519.301825	1046112.553171	42.091290
3519.610580	1045715.617121	42.096295
3519.333471	1045347.432189	42.101300
3519.194365	1044958.338320	42.106304
3519.345418	1044569.362545	42.111309
3519.393415	1044192.450954	42.116314
3519.192877	1043818.356162	42.121319
3519.226527	1043443.907753	42.126324
3519.510459	1043067.267329	42.131328
3519.440518	1042685.442058	42.136333
3519.582807	1042286.548917	42.141338
3519.209362	1041903.270417	42.146343
3519.312308	1041529.357936	42.151348
3519.024825	1041170.368455	42.156352
3519.099491	1040773.310760	42.161357
3519.109136	1040383.291740	42.166362
3518.856026	1040025.479244	42.171367
3518.985257	1039646.699024	42.176372
3519.063120	1039261.133765	42.181376
3518.948506	1038884.275413	42.186381
3519.315234	1038507.312252	42.191386
3518.697178	1038134.643898	42.196391
3518.748676	1037751.782704	42.201396
3518.454923	1037388.585024	42.206400
3518.333880	1037028.333528	42.211405
3518.700765	1036642.635940	42.216410
3518.609412	1036288.038550	42.221415
3518.545378	1035923.740143	42.226420
3518.590179	1035554.949677	42.231424
3518.013051	1035175.497714	42.236429
3518.513277	1034806.002158	42.241434
3518.303761	1034460.887051	42.246439
3518.445336	1034075.823003	42.251444
3518.348126	1033714.095203	42.256448
3518.071862	1033346.953512	42.261453
3518.614904	1032990.009294	42.266458
3518.060046	1032623.543400	42.271463
3517.894303	1032258.828596	42.276468
3518.463162	1031907.522269	42.281472
3518.212305	1031544.033290	42.286477
3518.468044	1031177.435725	42.291482
3517.960137	1030809.100128	42.296487
3517.835047	1030445.518905	42.301492
3517.883155	1030111.906068	42.306496
3517.659935	1029742.484817	42.311501
3517.717781	1029371.249486	42.316506
3517.440832	1029031.620774	42.321511
3517.354500	1028686.418719	42.326516
3517.486115	1028322.657053	42.331520
3517.394327	1027990.296783	42.336525
3517.673329	1027644.970252	42.341530
3517.369193	1027293.614430	42.346535
3517.562082	1026909.210187	42.351540
3517.621818	1026574.318416	42.356544
3517.380974	1026243.041679	42.361549
3517.454892	1025883.394789	42.366554
3517.139679	1025528.247190	42.371559
3517.206363	1025183.482141	42.376564
3517.027343	1024844.455297	42.381568
3517.118382	1024500.031882	42.386573
3516.992838	1024159.694585	42.391578
3516.731499	1023833.998301	42.396583
3516.942693	1023469.229325	42.401588
3517.043473	1023134.221953	42.406592
3516.907992	1022795.548722	42.411597
3517.222921	1022469.290332	42.416602
3516.923686	1022114.117520	42.421607
3517.093870	1021751.377044	42.426612
3517.199279	1021427.323196	42.431616
3516.800163	1021090.530197	42.436621
3516.911555	1020738.791510	42.441626
3516.761409	1020381.835378	42.446631
3517.019626	1020057.871278	42.451636
3516.669762	1019732.048232	42.456640
3517.071058	1019376.198576	42.461645
3516.978488	1019023.803841	42.466650
3516.802184	1018688.188385	42.471655
3516.480681	1018361.213679	42.476660
3516.488811	1018015.338038	42.481664
3516.732922	1017680.078346	42.486669
3516.734242	1017343.868028	42.491674
3516.504794	1017025.730049	42.496679
3516.489137	1016680.940985	42.501684
3516.638104	1016346.102753	42.506688
3516.336536	1016029.764766	42.511693
3516.399551	1015666.066184	42.516698
3515.963752	1015327.379985	42.521703
3516.004990	1015004.519511	42.526708
3516.156570	1014673.562429	42.531712
3516.071983	1014352.530305	42.536717
3516.344386	1014025.691077	42.541722
3516.222368	1013715.311799	42.546727
3516.002446	1013375.889805	42.551732
3516.252259	1013040.158266	42.556736
3515.996241	1012721.781156	42.561741
3516.242364	1012399.806064	42.566746
3515.956240	1012068.573617	42.571751
3516.242818	1011731.689355	42.576756
3516.257780	1011416.302877	42.581760
3515.830797	1011075.707540	42.586765
3516.007333	1010760.840783	42.591770
3515.762324	1010444.082264	42.596775
3516.044412	1010102.242328	42.601780
3516.136313	1009788.209871	42.606784
3515.664234	1009468.906975	42.611789
3516.020350	1009144.589456	42.616794
3515.792393	1008807.226359	42.621799
3515.739281	1008482.938208	42.626804
3515.781478	1008181.170648	42.631808
3515.991412	1007845.427870	42.636813
3516.006695	1007513.878109	42.641818
3515.432127	1007205.159325	42.646823
3515.562292	1006880.846170	42.651828
3515.921024	1006560.074895	42.656832
3515.605326	1006256.026682	42.661837
3515.611309	1005923.218023	42.666842
3515.406990	1005594.801269	42.671847
3515.580418	1005290.523262	42.676852
3515.529061	1004979.262141	42.681856
3515.493497	1004663.020005	42.686861
3515.590718	1004332.437344	42.691866
3515.465208	1004004.498903	42.696871
3515.152460	1003692.723533	42.701876
3515.473590	1003397.562480	42.706880
3514.916148	1003074.019786	42.711885
3514.881749	1002737.721754	42.716890
3514.791358	1002450.656049	42.721895
3515.169427	1002149.581434	42.726900
3515.103493	1001840.485682	42.731904
3514.804416	1001548.834163	42.736909
3514.994194	1001218.151577	42.741914
3514.809024	1000901.237038	42.746919
3514.883732	1000605.094827	42.751924
3515.024448	1000308.244777	42.756928
3514.876401	1000006.948174	42.761933
3514.834542	999692.084286	42.766938
3514.490943	999408.119048	42.771943
3515.065151	999100.910459	42.776948
3514.598706	998778.665198	42.781952
3514.670260	998488.937417	42.786957
3514.750039	998199.485648	42.791962
3514.546705	997894.092769	42.796967
3514.486809	997567.036639	42.801972
3514.573189	997270.523426	42.806977
3514.309834	996990.417518	42.811981
3514.470149	996705.357165	42.816986
3514.353699	996383.307761	42.821991
3514.059785	996076.662866	42.826996
3514.487484	995807.199159	42.832001
3514.519322	995519.177423	42.837005
3514.500600	995205.522105	42.842010
3514.328726	994928.904725	42.847015
3514.192127	994620.401193	42.852020
3514.268483	994331.239886	42.857025
3514.143024	994032.643239	42.862029
3514.133027	993743.661169	42.867034
3514.036817	993467.057588	42.872039
3513.966213	993154.272246	42.877044
3514.217968	992869.491621	42.882049
3513.831368	992569.691307	42.887053
3513.988386	992279.827387	42.892058
3513.985481	992004.599648	42.897063
3514.020983	991728.669747	42.902068
3514.208868	991434.175041	42.907073
3513.862391	991150.674450	42.912077
3513.828606	990855.601226	42.917082
3513.646427	990567.168636	42.922087
3513.581602	990274.703488	42.927092
3513.734293	989996.622199	42.932097
3513.609221	989702.674600	42.937101
3513.918594	989432.830586	42.942106
3513.629200	989165.413507	42.947111
3513.549566	988872.195908	42.952116
3513.864908	988592.653539	42.957121
3513.285047	988314.903425	42.962125
3513.429569	988023.068594	42.967130
3513.242607	987738.298485	42.972135
3513.735422	987471.746308	42.977140
3513.740751	987208.872402	42.982145
3513.454728	986917.734926	42.987149
3513.391219	986626.545925	42.992154
3513.479999	986366.254323	42.997159
3513.530978	986076.677476	43.002164
3513.531052	985782.897340	43.007169
3513.044869	985507.923041	43.012173
3513.085179	985242.024408	43.017178
3513.190179	984984.595460	43.022183
3513.015714	984706.700273	43.027188
3513.219485	984418.185518	43.032193
3513.107060	984163.879422	43.037197
3512.955307	983878.031966	43.042202
3512.898568	983624.278471	43.047207
3512.948838	983369.421972	43.052212
3513.242696	983083.558983	43.057217
3513.063295	982797.466667	43.062221
3512.640161	982537.377627	43.067226
3512.809287	982275.225911	43.072231
3512.684851	981999.925267	43.077236
3513.191869	981731.442154	43.082241
3512.925579	981473.134602	43.087245
3512.718585	981213.828781	43.092250
3512.587269	980941.115661	43.097255
3512.737531	980687.295247	43.102260
3512.816591	980413.643091	43.107265
3512.676529	980131.318583	43.112269
3512.732875	979876.402930	43.117274
3512.350081	979635.227522	43.122279
3512.737126	979368.216525	43.127284
3512.700931	979097.060895	43.132289
3512.522442	978833.440502	43.137293
3512.612704	978570.252330	43.142298
3512.552143	978294.860416	43.147303
3512.610841	978046.508588	43.152308
3512.634233	977798.738242	43.157313
3512.404192	977521.773190	43.162317
3512.215881	977246.254108	43.167322
3512.195625	977004.517057	43.172327
3512.229231	976747.803921	43.177332
3512.242974	976481.990606	43.182337
3512.189958	976232.405319	43.187341
3512.294629	975978.090155	43.192346
3512.108270	975735.544722	43.197351
3512.331137	975459.578620	43.202356
3512.554293	975215.183664	43.207361
3511.764346	974982.093047	43.212365
3512.175750	974720.630775	43.217370
3512.002352	974451.918090	43.222375
3511.845330	974220.452593	43.227380
3512.169254	973965.131767	43.232385
3512.210242	973711.606761	43.237389
3512.184809	973454.853606	43.242394
3512.151805	973225.577253	43.247399
3511.925743	972957.292279	43.252404
3512.315538	972694.273835	43.257409
3512.257165	972472.406442	43.262413
3512.184646	972199.462664	43.267418
3511.633290	971955.349830	43.272423
3512.088731	971704.896591	43.277428
3512.046021	971467.136938	43.282433
3511.643698	971214.748774	43.287437
3511.722740	970944.068790	43.292442
3511.790931	970707.140108	43.297447
3511.479195	970472.319401	43.302452
3511.787818	970225.153226	43.307457
3511.372678	969964.099654	43.312461
3511.547481	969721.436052	43.317466
3511.669823	969489.342122	43.322471
3511.374089	969243.995153	43.327476
3511.722106	969018.794973	43.332481
3511.453620	968780.178127	43.337485
3511.777439	968519.132966	43.342490
3511.744543	968284.470580	43.347495
3511.607745	968057.648254	43.352500
3511.522920	967809.561826	43.357505
3511.464258	967571.153957	43.362509
3511.420449	967312.856193	43.367514
3511.292341	967079.727022	43.372519
3511.479823	966860.637912	43.377524
3511.516476	966615.319835	43.382529
3510.965529	966372.242651	43.387533
3511.240463	966124.513954	43.392538
3511.237649	965906.986904	43.397543
3511.237315	965671.331032	43.402548
3511.280128	965445.747363	43.407553
3511.274267	965211.934661	43.412557
3510.999936	964947.887290	43.417562
3511.142693	964719.809727	43.422567
3510.827249	964499.440037	43.427572
3511.213373	964285.412430	43.432577
3510.961732	964051.005238	43.437581
3511.197365	963804.358877	43.442586
3511.153583	963575.090960	43.447591
3511.220080	963341.386353	43.452596
3511.397201	963103.048480	43.457601
3510.791730	962882.174714	43.462605
3511.113606	962653.789858	43.467610
3510.956697	962414.008527	43.472615
3510.831357	962171.467834	43.477620
3510.909400	961957.502517	43.482625
3510.453947	961724.896435	43.487629
3510.849350	961477.536092	43.492634
3510.549449	961263.999362	43.497639
3510.515799	961051.391127	43.502644
3510.900607	960824.001716	43.507649
3510.546635	960606.822461	43.512653
3510.874114	960364.719384	43.517658
3510.648720	960165.345104	43.522663
3510.514720	959957.811209	43.527668
3510.445586	959722.217420	43.532673
3510.492002	959502.283328	43.537677
3510.509475	959275.579771	43.542682
3510.344753	959072.137429	43.547687
3510.304123	958833.855081	43.552692
3510.452678	958622.794420	43.557697
3510.268203	958420.214958	43.562701
3510.149348	958194.962476	43.567706
3510.510061	957967.170269	43.572711
3510.343243	957755.149062	43.577716
3510.008271	957550.994586	43.582721
3509.972194	957336.190079	43.587725
3510.468641	957102.946557	43.592730
3510.503792	956900.081415	43.597735
3510.738832	956673.926562	43.602740
3510.522334	956461.081244	43.607745
3510.684684	956243.162212	43.612749
3510.409358	956014.612939	43.617754
3510.250851	955811.230353	43.622759
3510.133955	955604.894893	43.627764
3510.281907	955380.051019	43.632769
3509.791770	955165.726360	43.637773
3509.985673	954960.748103	43.642778
3509.876142	954767.097209	43.647783
3509.815373	954563.579537	43.652788
3509.962799	954375.131887	43.657793
3509.860624	954167.396704	43.662797
3510.258754	953947.900619	43.667802
3510.138851	953749.716968	43.672807
3510.126985	953561.265510	43.677812
3510.154519	953347.735806	43.682817
3509.878653	953124.584331	43.687821
3510.040345	952913.214828	43.692826
3509.743271	952731.668396	43.697831
3509.635703	952543.864950	43.702836
3509.590670	952321.405873	43.707841
3509.261674	952117.356498	43.712845
3509.576180	951933.767226	43.717850
3509.804098	951747.793210	43.722855
3509.710553	951538.418646	43.727860
3509.694018	951331.894003	43.732865
3509.529207	951155.055156	43.737869
3509.586078	950942.473118	43.742874
3509.516549	950755.172143	43.747879
3509.098647	950559.115530	43.752884
3509.540715	950362.526897	43.757889
3508.971156	950181.030733	43.762893
3509.193444	949987.910132	43.767898
3509.546613	949793.420454	43.772903
3509.278363	949605.440180	43.777908
3509.566211	949411.616999	43.782913
3509.283079	949221.040134	43.787917
3509.165952	949022.577538	43.792922
3509.180504	948846.682977	43.797927
3509.149055	948665.044711	43.802932
3509.462594	948472.139517	43.807937
3509.406120	948295.759073	43.812941
3509.101630	948089.534730	43.817946
3509.188943	947895.496060	43.822951
3509.414877	947703.055403	43.827956
3509.251852	947520.249249	43.832961
3509.037569	947333.134998	43.837965
3509.057799	947155.170496	43.842970
3508.991720	946965.911323	43.847975
3509.000673	946781.518141	43.852980
3509.220849	946594.209809	43.857985
3508.589682	946419.201073	43.862989
3508.883571	946234.837287	43.867994
3508.781928	946050.148876	43.872999
3508.922485	945862.635600	43.878004
3509.144938	945682.000378	43.883009
3508.782979	945507.012291	43.888013
3508.930935	945323.310826	43.893018
3508.859312	945127.757334	43.898023
3509.102503	944956.196346	43.903028
3508.983575	944782.676979	43.908033
3508.812873	944607.914555	43.913037
3508.541843	944413.708638	43.918042
3508.973478	944230.305132	43.923047
3508.591179	944040.416249	43.928052
3508.762876	943869.406213	43.933057
3508.680136	943704.087411	43.938061
3508.849762	943533.929315	43.943066
3509.192631	943334.789528	43.948071
3508.291318	943155.976968	43.953076
3508.982538	942982.264111	43.958081
3508.716388	942812.345947	43.963085
3508.869730	942635.834261	43.968090
3508.712535	942462.819046	43.973095
3508.604170	942274.929798	43.978100
3508.600628	942087.591779	43.983105
3508.656265	941916.728559	43.988109
3508.654312	941758.333938	43.993114
3508.502297	941584.329934	43.998119
3508.140942	941396.354862	44.003124
3508.406025	941215.461769	44.008129
3508.462736	941059.625403	44.013133
3508.667076	940879.977354	44.018138
3508.581178	940712.262730	44.023143
3508.422386	940558.652676	44.028148
3508.465064	940368.560140	44.033153
3508.468527	940191.511067	44.038157
3508.391856	940016.675238	44.043162
3508.312830	939868.594829	44.048167
3508.112701	939697.605365	44.053172
3508.261544	939518.111610	44.058177
3508.311166	939350.810713	44.063181
3508.472899	939184.445313	44.068186
3508.221382	939032.532544	44.073191
3508.109968	938857.759752	44.078196
3508.024578	938683.072798	44.083201
3507.766506	938533.257315	44.088205
3507.986396	938351.601291	44.093210
3507.966788	938190.895033	44.098215
3507.870283	938038.928010	44.103220
3508.156503	937895.241466	44.108225
3507.989114	937714.490815	44.113229
3508.058842	937539.260548	44.118234
3507.934503	937384.400435	44.123239
3507.985806	937218.470856	44.128244
3507.875161	937051.027236	44.133249
3507.625620	936906.250349	44.138253
3507.846468	936741.429483	44.143258
3507.576569	936571.981430	44.148263
3507.617696	936409.387265	44.153268
3507.404632	936282.823409	44.158273
3507.467198	936126.935765	44.163277
3507.368234	935968.574439	44.168282
3507.727228	935808.021141	44.173287
3507.044891	935670.096971	44.178292
3507.202024	935513.311709	44.183297
3507.165463	935366.537592	44.188301
3507.408055	935214.817345	44.193306
3507.417459	935050.650577	44.198311
3507.393146	934914.710417	44.203316
3507.335611	934773.587722	44.208321
3507.406643	934630.999909	44.213325
3507.367835	934461.830189	44.218330
3507.262834	934316.862533	44.223335
3506.823502	934176.843021	44.228340
3507.443452	934040.870346	44.233345
3507.076145	933886.427848	44.238349
3507.053549	933732.212161	44.243354
3507.124559	933578.552761	44.248359
3507.190084	933438.430598	44.253364
3507.262864	933299.071833	44.258369
3506.838868	933142.024022	44.263373
3506.745051	933019.300100	44.268378
3506.871831	932892.503178	44.273383
3507.108750	932748.396794	44.278388
3507.301228	932586.716856	44.283393
3506.815241	932471.344608	44.288397
3506.771510	932325.640123	44.293402
3507.206589	932168.998386	44.298407
3506.816877	932028.914049	44.303412
3506.897340	931888.364334	44.308417
3506.859235	931755.035258	44.313421
3506.695070	931611.540540	44.318426
3506.764074	931497.496763	44.323431
3506.385775	931360.371087	44.328436
3506.759006	931203.711160	44.333441
3506.561235	931069.334411	44.338445
3506.472051	930962.126667	44.343450
3506.682385	930834.786594	44.348455
3506.144309	930686.332352	44.353460
3506.457839	930544.363650	44.358465
3505.989452	930420.296314	44.363469
3506.143929	930283.535638	44.368474
3506.592425	930158.158107	44.373479
3506.484196	930052.376624	44.378484
3506.614663	929917.051948	44.383489
3506.527989	929785.795798	44.388493
3506.553433	929653.172531	44.393498
3506.593386	929515.546154	44.398503
3506.196742	929367.031942	44.403508
3506.276191	929247.940827	44.408513
3505.963047	929133.909517	44.413517
3505.859021	929018.495745	44.418522
3506.519443	928885.844991	44.423527
3506.101988	928771.150324	44.428532
3506.316366	928635.394948	44.433537
3506.167086	928508.539316	44.438541
3506.369834	928386.813438	44.443546
3506.065797	928269.109471	44.448551
3505.993810	928156.747919	44.453556
3506.012430	928008.992805	44.458561
3505.786218	927906.937484	44.463565
3506.002491	927785.291864	44.468570
3506.250879	927670.175559	44.473575
3506.253177	927541.926172	44.478580
3506.338700	927403.180506	44.483585
3506.266982	927306.087716	44.488589
3506.023289	927174.024295	44.493594
3505.850370	927052.618480	44.498599
3505.834947	926947.625745	44.503604
3505.927344	926821.651937	44.508609
3506.173304	926697.476831	44.513613
3505.815155	926575.225348	44.518618
3506.136047	926480.553068	44.523623
3505.669335	926362.449459	44.528628
3505.985726	926221.038918	44.533633
3505.722682	926115.686078	44.538637
3505.601939	925999.152322	44.543642
3505.924146	925884.851156	44.548647
3505.620085	925767.188540	44.553652
3505.996607	925647.006914	44.558657
3505.781589	925555.099505	44.563661
3505.719587	925438.063062	44.568666
3506.035395	925312.882759	44.573671
3505.827967	925203.271006	44.578676
3505.694524	925069.406510	44.583681
3505.797101	924960.989165	44.588685
3505.955454	924856.888911	44.593690
3506.097945	924740.573158	44.598695
3505.842141	924629.803443	44.603700
3505.985149	924493.762916	44.608705
3505.946752	924384.395273	44.613709
3506.100988	924258.447571	44.618714
3506.399429	924146.518473	44.623719
3505.944982	924035.961697	44.628724
3506.038918	923899.818103	44.633729
3505.918218	923785.834068	44.638733
3505.511994	923678.629280	44.643738
3505.820709	923558.316146	44.648743
3505.530975	923451.280086	44.653748
3505.706617	923335.024847	44.658753
3505.382534	923221.254846	44.663757
3505.339340	923118.501357	44.668762
3505.679741	923015.490297	44.673767
3505.210665	922907.510816	44.678772
3505.609202	922784.663920	44.683777
3505.607529	922690.844372	44.688781
3505.368257	922595.522686	44.693786
3505.695780	922483.939346	44.698791
3505.456694	922364.171077	44.703796
3505.306813	922252.276676	44.708801
3505.433132	922148.707010	44.713805
3505.467338	922053.426987	44.718810
3505.386358	921934.778048	44.723815
3505.478465	921836.020039	44.728820
3505.142245	921731.171209	44.733825
3505.085328	921636.476337	44.738829
3505.226124	921522.401619	44.743834
3505.218516	921412.102665	44.748839
3505.134638	921332.133011	44.753844
3505.026940	921222.616699	44.758849
3505.160072	921125.379055	44.763853
3505.142347	921017.672623	44.768858
3505.492760	920907.978265	44.773863
3505.514669	920812.389731	44.778868
3505.319771	920710.578237	44.783873
3505.191478	920601.245328	44.788877
3505.125266	920499.408686	44.793882
3505.315331	920413.219425	44.798887
3504.997799	920306.510964	44.803892
3505.459313	920191.104016	44.808897
3505.259101	920087.548871	44.813901
3505.170159	919978.678341	44.818906
3505.191131	919881.244401	44.823911
3505.465115	919794.935263	44.828916
3505.244869	919703.121970	44.833921
3505.296647	919587.095771	44.838925
3505.234830	919487.742809	44.843930
3505.370331	919388.548107	44.848935
3505.084219	919289.421045	44.853940
3505.253040	919161.619546	44.858945
3505.198400	919080.456541	44.863949
3505.158189	918977.431697	44.868954
3505.264593	918894.891319	44.873959
3505.189676	918787.631694	44.878964
3505.358462	918676.863119	44.883969
3505.217451	918591.373687	44.888973
3505.017686	918483.550861	44.893978
3505.304338	918389.802265	44.898983
3504.850216	918311.101184	44.903988
3505.204854	918204.144570	44.908993
3505.181736	918092.529012	44.913997
3505.013526	917983.920672	44.919002
3505.579228	917876.537655	44.924007
3505.159088	917792.719001	44.929012
3504.868026	917694.237993	44.934017
3504.809996	917590.130474	44.939021
3504.724718	917506.733866	44.944026
3505.086418	917411.607703	44.949031
3504.748917	917313.609091	44.954036
3505.021274	917208.861980	44.959041
3505.231688	917127.433681	44.964045
3504.986160	917019.396885	44.969050
3504.935525	916910.940545	44.974055
3504.847774	916825.414746	44.979060
3505.026509	916761.614583	44.984065
3504.833791	916655.199537	44.989069
3504.817931	916558.386767	44.994074
3505.033687	916458.740386	44.999079
3504.812655	916374.000190	45.004084
3504.657204	916294.064849	45.009089
3504.941729	916191.126747	45.014093
3505.008032	916095.544714	45.019098
3505.021546	916009.411458	45.024103
3504.763360	915922.839873	45.029108
3505.245174	915809.649467	45.034113
3504.957745	915702.075365	45.039117
3504.233566	915628.294028	45.044122
3504.405157	915553.111578	45.049127
3504.041453	915459.227286	45.054132
3504.467745	915359.622645	45.059137
3504.483486	915285.136692	45.064141
3504.492143	915185.790406	45.069146
3504.931972	915095.718265	45.074151
3504.425061	915025.169285	45.079156
3504.798553	914953.318037	45.084161
3504.620121	914848.118338	45.089165
3504.818389	914736.108925	45.094170
3504.854779	914655.154479	45.099175
3504.402725	914566.473365	45.104180
3504.720774	914478.049464	45.109185
3504.546611	914400.017080	45.114189
3504.228657	914315.839344	45.119194
3504.914039	914219.448124	45.124199
3504.742364	914157.892106	45.129204
3504.868486	914044.820380	45.134209
3504.558152	913951.383460	45.139213
3504.726268	913872.323423	45.144218
3504.689445	913791.271963	45.149223
3504.345233	913709.980788	45.154228
3504.282621	913623.919118	45.159233
3504.562608	913538.956328	45.164237
3504.638919	913449.109936	45.169242
3504.383712	913354.111589	45.174247
3504.389116	913288.757460	45.179252
3504.308641	913198.740034	45.184257
3504.253942	913104.282721	45.189261
3504.155807	913035.472423	45.194266
3504.274660	912966.721925	45.199271
3504.122402	912891.749307	45.204276
3504.491695	912790.661675	45.209281
3504.436742	912698.221873	45.214285
3504.483623	912622.923602	45.219290
3504.362788	912537.240200	45.224295
3504.378316	912456.546144	45.229300
3504.415385	912386.645027	45.234305
3504.284863	912312.046596	45.239309
3504.191740	912219.315847	45.244314
3504.175222	912122.521614	45.249319
3504.128172	912061.210921	45.254324
3504.474585	911986.625959	45.259329
3504.519180	911900.423372	45.264333
3504.347693	911832.381510	45.269338
3504.261276	911737.327565	45.274343
3504.245204	911651.613191	45.279348
3504.469334	911566.050770	45.284353
3504.569958	911500.756249	45.289357
3504.346753	911429.439568	45.294362
3504.399114	911318.734826	45.299367
3504.301329	911224.252507	45.304372
3504.108658	911162.184423	45.309377
3504.604321	911102.123729	45.314381
3504.224168	911006.719910	45.319386
3504.381694	910924.437234	45.324391
3504.241511	910835.741258	45.329396
3504.320958	910750.286517	45.334401
3504.297238	910678.445135	45.339405
3504.148647	910620.124777	45.344410
3504.211902	910521.649989	45.349415
3503.955657	910457.945011	45.354420
3503.867113	910372.319237	45.359425
3504.257715	910319.597026	45.364429
3503.921757	910238.542787	45.369434
3504.091298	910141.972659	45.374439
3504.144632	910079.755496	45.379444
3504.156178	910003.462974	45.384449
3503.870227	909909.664405	45.389453
3503.919854	909849.470739	45.394458
3504.272232	909778.906098	45.399463
3503.915238	909714.051742	45.404468
3503.855546	909637.283656	45.409473
3503.941702	909555.378277	45.414477
3503.639140	909495.238785	45.419482
3504.014255	909432.672007	45.424487
3504.132357	909357.221197	45.429492
3503.973021	909277.956596	45.434497
3503.984721	909203.389380	45.439501
3503.569252	909127.541024	45.444506
3504.112798	909046.517463	45.449511
3504.094487	908985.746848	45.454516
3503.985033	908919.395448	45.459521
3504.220466	908827.807981	45.464525
3503.688649	908764.321913	45.469530
3503.844854	908681.427432	45.474535
3503.550151	908607.095641	45.479540
3503.686322	908546.391260	45.484545
3503.731717	908501.426635	45.489549
3503.661094	908433.712401	45.494554
3504.116112	908360.122116	45.499559
3504.050663	908296.650376	45.504564
3503.692262	908214.991463	45.509569
3503.670594	908130.574407	45.514573
3503.609020	908081.475307	45.519578
3503.686863	908011.512396	45.524583
3503.688752	907948.218565	45.529588
3503.921284	907871.474489	45.534593
3503.870138	907804.617781	45.539597
3503.508471	907727.583647	45.544602
3503.970206	907648.386541	45.549607
3503.604496	907600.008726	45.554612
3503.732656	907524.338467	45.559617
3503.889094	907472.110351	45.564621
3503.358734	907425.688000	45.569626
3503.725777	907341.387971	45.574631
3503.434477	907269.739652	45.579636
3503.626711	907212.581896	45.584641
3503.557924	907161.352945	45.589645
3503.537264	907086.183756	45.594650
3503.714375	907008.182454	45.599655
3503.555259	906955.036472	45.604660
3503.193046	906889.281560	45.609665
3503.643717	906830.436780	45.614669
3503.535247	906759.330824	45.619674
3503.681227	906704.009088	45.624679
3503.447228	906652.320153	45.629684
3503.444239	906567.683381	45.634689
3503.419027	906502.350952	45.639693
3503.450269	906446.176978	45.644698
3503.490888	906383.631127	45.649703
3503.318566	906326.331338	45.654708
3503.610295	906273.201129	45.659713
3503.599525	906212.109530	45.664717
3503.458923	906151.810774	45.669722
3503.425545	906079.911688	45.674727
3503.292032	906038.913901	45.679732
3503.149319	905965.487071	45.684737
3503.196085	905905.058277	45.689741
3502.996655	905841.484188	45.694746
3503.542338	905788.886686	45.699751
3503.021516	905733.568667	45.704756
3503.190482	905676.399058	45.709761
3503.288048	905628.796579	45.714765
3503.221645	905553.710862	45.719770
3503.402551	905489.877087	45.724775
3503.425777	905459.563740	45.729780
3502.989502	905392.065927	45.734785
3503.060412	905331.626974	45.739789
3503.068091	905271.970031	45.744794
3503.027750	905214.540596	45.749799
3502.824819	905186.965916	45.754804
3503.305297	905127.036494	45.759809
3503.502100	905083.853578	45.764813
3503.252113	905009.370014	45.769818
3503.230508	904863.796422	45.774823
3502.893811	904709.099609	45.779828
3503.008739	904466.372609	45.784833
3503.325828	904163.548106	45.789837
3503.177187	903812.409687	45.794842
3503.152544	903407.926467	45.799847
3503.082934	902927.903488	45.804852
3502.976525	902371.064583	45.809857
3502.797714	901772.745290	45.814861
3502.583506	901083.079640	45.819866
3502.927066	900357.780383	45.824871
3502.667596	899555.474992	45.829876
3502.486294	898669.350294	45.834881
3502.559691	897702.624677	45.839885
3502.237592	896693.842209	45.844890
3502.248272	895593.256126	45.849895
3502.024442	894428.084481	45.854900
3502.033023	893148.488759	45.859905
3501.655482	891823.098000	45.864909
3501.458166	890415.010604	45.869914
3501.530626	888941.674549	45.874919
3500.976980	887368.231764	45.879924
3500.492643	885702.527144	45.884929
3500.724557	883960.848069	45.889933
3500.355236	882165.637351	45.894938
3500.308450	880244.176034	45.899943
3500.091289	878253.063578	45.904948
3499.762470	876179.416290	45.909953
3499.541507	874015.835637	45.914957
3499.061723	871754.035016	45.919962
3498.993958	869400.498554	45.924967
3498.466504	866990.927384	45.929972
3497.982717	864480.947245	45.934977
3497.914551	861876.699197	45.939981
3497.298292	859220.452189	45.944986
3497.139651	856438.297471	45.949991
3496.719659	853574.206767	45.954996
3496.225969	850636.714901	45.960001
3495.740733	847614.309393	45.965005
3495.206046	844523.562941	45.970010
3495.440169	841304.489747	45.975015
3494.829071	838023.066353	45.980020
3494.294380	834653.028087	45.985025
3493.874086	831183.493623	45.990029
3493.088091	827651.796392	45.995034
3492.475539	824028.755754	46.000039
3491.845142	820331.300845	46.005044
3491.293752	816535.754483	46.010049
3490.790057	812652.998254	46.015053
3489.886509	808689.054626	46.020058
3489.341689	804657.903820	46.025063
3488.900829	800529.697599	46.030068
3488.352522	796306.187304	46.035073
3487.880519	792020.023186	46.040077
3486.827298	787642.606502	46.045082
3486.280876	783182.818676	46.050087
3485.445449	778636.531281	46.055092
3484.909975	774003.367922	46.060097
3484.284899	769277.936761	46.065101
3483.613437	764462.653787	46.070106
3483.104985	759548.660026	46.075111
3482.190873	754579.756589	46.080116
3480.871398	749507.241607	46.085121
3480.454639	744373.419802	46.090125
3479.606355	739162.250701	46.095130
3478.902833	733837.281320	46.100135
3478.005009	728441.056291	46.105140
3477.488146	722941.552740	46.110145
3476.310072	717351.590131	46.115149
3475.606573	711694.340379	46.120154
3474.626107	705951.811975	46.125159
3473.900799	700090.392195	46.130164
3472.427065	694152.359195	46.135169
3471.569577	688155.519646	46.140173
3470.519419	682071.357587	46.145178
3469.601054	675867.956135	46.150183
3468.772106	669599.730092	46.155188
3467.655348	663255.603275	46.160193
3467.090571	656811.934543	46.165197
3465.216158	650293.104620	46.170202
3464.284876	643693.723077	46.175207
3463.300337	637011.828039	46.180212
3462.324498	630216.835412	46.185217
3461.118161	623365.884811	46.190221
3459.638605	616430.786099	46.195226
3458.642957	609398.102601	46.200231
3457.560259	602282.302208	46.205236
3455.932635	595088.379584	46.210241
3454.836740	587821.897509	46.215245
3453.504199	580468.118714	46.220250
3452.164856	573010.802374	46.225255
3451.127948	565496.306791	46.230260
3449.588629	557892.583343	46.235265
3448.144832	550201.515306	46.240269
3446.521612	542425.594132	46.245274
3445.160030	534554.536756	46.250279
3443.614911	526632.272564	46.255284
3441.969002	518643.983983	46.260289
3440.699531	510545.696813	46.265293
3438.308473	502373.688146	46.270298
3437.170833	494114.848035	46.275303
3435.624004	485813.613379	46.280308
3433.799075	477428.876018	46.285313
3432.329860	468933.562855	46.290317
3430.687986	460375.926177	46.295322
3428.464763	451758.902317	46.300327
3426.473567	443060.327722	46.305332
3424.675203	434290.022489	46.310337
3422.775357	425475.614845	46.315341
3420.639822	416550.644437	46.320346
3418.937699	407564.343136	46.325351
3417.105288	398518.144222	46.330356
3414.669747	389403.357971	46.335361
3412.616986	380197.881187	46.340365
3410.470935	370953.433787	46.345370
3408.267944	361647.053138	46.350375
3405.795437	352262.518761	46.355380
3403.312962	342821.342055	46.360385
3400.936113	333338.465340	46.365389
3398.764091	323806.244785	46.370394
3395.906310	314179.265745	46.375399
3393.276828	304517.267702	46.380404
3390.661858	294823.805474	46.385409
3388.127166	285049.881264	46.390413
3384.887445	275249.267759	46.395418
3381.682321	265412.264396	46.400423
3379.051405	255516.142194	46.405428
3375.737787	245575.480024	46.410433
3372.356045	235608.221152	46.415437
3368.833584	225646.886921	46.420442
3365.409514	215529.283600	46.425447
3362.063795	205455.386222	46.430452
3358.177129	195393.903427	46.435457
3354.274350	185317.812258	46.440461
3350.079262	175241.819166	46.445466
3346.213447	165126.108255	46.450471
3341.842060	155001.211795	46.455476
3336.940269	144902.116354	46.460481
3331.937273	134805.422294	46.465485
3326.382629	124753.256582	46.470490
3321.140985	114692.966393	46.475495
3314.987702	104679.754037	46.480500
3308.432306	94747.574294	46.485505
3301.578465	84873.003457	46.490509
3292.908499	75064.761410	46.495514
3282.979366	65384.808441	46.500519
3265.706972	56048.394894	46.505524
3234.062212	47289.690085	46.510529
3194.312399	39137.074808	46.515533
3149.006391	31738.542701	46.520538
3104.511713	25082.517733	46.525543
3062.008282	19255.770115	46.530548
3024.412897	14278.096350	46.535553
2991.507515	10087.727637	46.540557
2963.584059	6661.190392	46.545562
2939.654390	3959.551626	46.550567
2919.721383	1919.425046	46.555572
2898.874096	517.955947	46.560577
2857.116792	311.674053	46.565581
2834.266960	318.863240	46.570586
2835.783088	312.386532	46.575591
2851.402605	291.484021	46.580596
2870.054463	304.234102	46.585601
2885.680692	313.257707	46.590605
2893.061179	334.156246	46.595610
2894.208451	383.407935	46.600615
2894.114395	402.249623	46.605620
2893.685428	361.725736	46.610625
2892.983992	271.569269	46.615629
2888.411022	262.416714	46.620634
2882.446852	269.609434	46.625639
2879.114812	264.601025	46.630644
2875.662682	279.056717	46.635649
2873.274822	282.173875	46.640653
2870.973839	263.873701	46.645658
2868.636705	279.783083	46.650663
2866.144485	268.687213	46.655668
2863.524543	267.822922	46.660673
2860.769116	276.469265	46.665677
2857.479693	273.816517	46.670682
2854.398332	256.467260	46.675687
2851.295148	268.851083	46.680692
2847.939316	277.676218	46.685697
2845.369225	269.632023	46.690701
2841.909183	253.194882	46.695706
2838.637553	260.091327	46.700711
2835.686141	266.442424	46.705716
2831.967304	261.987013	46.710721
2828.782259	257.177347	46.715725
2825.694884	272.190169	46.720730
2822.340662	269.850286	46.725735
2819.157126	266.403327	46.730740
2815.941683	255.098115	46.735745
2812.532314	250.282725	46.740749
2809.339739	259.320373	46.745754
2806.103875	256.986045	46.750759
2802.926206	264.443427	46.755764
2799.088806	257.646779	46.760769
2795.898779	234.944186	46.765773
2792.419113	258.361759	46.770778
2789.251705	262.861398	46.775783
2785.825837	263.820077	46.780788
2782.174515	259.739876	46.785793
2778.914581	241.218758	46.790797
2775.893509	250.726517	46.795802
2772.334275	265.357132	46.800807
2768.872069	252.508699	46.805812
2765.619574	264.090271	46.810817
2762.568577	243.042215	46.815821
2758.856772	244.039859	46.820826
2754.916367	227.723132	46.825831
2752.502554	238.479912	46.830836
2748.260157	259.239535	46.835841
2744.939061	239.661720	46.840845
2741.278153	234.107322	46.845850
2737.760931	243.782319	46.850855
2734.610825	238.197965	46.855860
2731.395514	233.074505	46.860865
2727.976265	255.495625	46.865869
2724.791803	257.545850	46.870874
2721.657718	240.819380	46.875879
2718.291739	240.750145	46.880884
2714.029763	242.882531	46.885889
2710.760206	221.749528	46.890893
2707.414969	232.045980	46.895898
2703.774867	245.181768	46.900903
2700.414365	244.588397	46.905908
2696.599741	235.110008	46.910913
2693.084689	240.316801	46.915917
2689.702371	238.294436	46.920922
2686.429324	222.521484	46.925927
2683.097121	221.092232	46.930932
2679.163813	227.935436	46.935937
2676.546964	228.712435	46.940941
2673.223574	223.513108	46.945946
2669.430808	220.564531	46.950951
2665.626072	220.064940	46.955956
2661.764574	241.423510	46.960961
2658.580347	213.035079	46.965965
2655.452883	207.388443	46.970970
2652.099261	226.596839	46.975975
2649.280063	228.477069	46.980980
2645.011124	220.251705	46.985985
2641.589619	200.388990	46.990989
2638.490038	214.824838	46.995994
2635.024070	227.344561	47.000999
2631.451569	229.606282	47.006004
2627.580710	223.661977	47.011009
2623.900573	215.108607	47.016013
2620.120171	219.148445	47.021018
2616.987290	213.761574	47.026023
2614.223876	217.384243	47.031028
2610.690676	225.017587	47.036033
2607.054559	208.028625	47.041037
2603.037942	215.327840	47.046042
2599.746867	221.773867	47.051047
2596.460400	226.428150	47.056052
2592.852605	221.379537	47.061057
2589.673502	208.622184	47.066061
2586.008474	222.928931	47.071066
2582.739726	237.143320	47.076071
2578.953706	222.996717	47.081076
2575.379895	205.032316	47.086081
2572.126452	194.635599	47.091085
2568.136979	220.896256	47.096090
2565.244951	221.953156	47.101095
2562.085089	221.002601	47.106100
2558.211796	202.031156	47.111105
2554.930131	202.934291	47.116109
2551.090939	194.311512	47.121114
2547.655276	204.803635	47.126119
2544.292543	218.431456	47.131124
2540.689746	206.105449	47.136129
2537.231271	205.288294	47.141133
2533.908395	208.853785	47.146138
2530.215871	207.585923	47.151143
2526.860174	203.491552	47.156148
2523.340204	212.665030	47.161153
2519.732742	202.672578	47.166157
2516.372472	197.125957	47.171162
2512.742381	195.387806	47.176167
2509.566450	207.649210	47.181172
2505.812885	220.484916	47.186177
2502.251315	195.635862	47.191181
2498.678070	194.894078	47.196186
2495.081195	204.877630	47.201191
2492.069604	201.764426	47.206196
2488.339573	204.728722	47.211201
2485.013359	207.453400	47.216205
2481.775486	195.992791	47.221210
2478.063336	189.823535	47.226215
2474.712974	203.991898	47.231220
2470.752647	202.075312	47.236225
2467.650043	195.540177	47.241229
2464.168797	201.304862	47.246234
2460.257207	206.508765	47.251239
2457.006521	188.153203	47.256244
2453.434783	194.769754	47.261249
2450.007513	201.391095	47.266253
2446.634000	190.118216	47.271258
2442.892804	189.511782	47.276263
2439.464936	192.232128	47.281268
2435.930674	182.555480	47.286273
2432.828795	197.404786	47.291277
2429.093770	218.216435	47.296282
2425.506324	199.256348	47.301287
2422.194963	187.474464	47.306292
2418.447692	204.094526	47.311297
2415.220943	181.893245	47.316301
2411.486426	194.856534	47.321306
2407.896642	204.472561	47.326311
2404.534832	195.229459	47.331316
2400.953126	181.639931	47.336321
2397.897768	191.697075	47.341325
2394.451268	195.976018	47.346330
2390.634216	191.957208	47.351335
2387.304817	200.592736	47.356340
2383.439224	198.002485	47.361345
2380.059126	190.838296	47.366349
2376.629522	186.277840	47.371354
2372.794882	200.800930	47.376359
2369.964399	192.127525	47.381364
2366.383770	189.157447	47.386369
2362.596230	173.493265	47.391373
2359.306138	195.454972	47.396378
2355.390645	214.050937	47.401383
2352.401523	187.734795	47.406388
2348.569896	181.778178	47.411393
2345.111589	198.445405	47.416397
2341.497915	206.907847	47.421402
2338.233788	203.840992	47.426407
2334.984266	180.509940	47.431412
2331.001948	184.356406	47.436417
2327.419259	184.303651	47.441421
2324.148280	209.907720	47.446426
2320.953351	203.647622	47.451431
2317.899582	175.619373	47.456436
2313.666840	186.885323	47.461441
2310.689034	187.149314	47.466445
2306.515760	195.589918	47.471450
2302.950035	185.751518	47.476455
2299.804083	184.934032	47.481460
2296.251550	193.843147	47.486465
2292.816285	183.450236	47.491469
2289.527039	195.955894	47.496474
2286.082196	185.342308	47.501479
2282.064865	173.943893	47.506484
2278.697119	173.451842	47.511489
2275.369694	175.765039	47.516493
2271.357583	193.563676	47.521498
2268.181013	184.147754	47.526503
2265.118160	185.392059	47.531508
2261.264387	178.188275	47.536513
2257.646553	176.529421	47.541517
2254.216689	192.067275	47.546522
2250.519635	190.652131	47.551527
2247.489148	181.016309	47.556532
2244.017890	183.145488	47.561537
2240.539930	168.764367	47.566541
2236.862645	165.621586	47.571546
2232.993393	181.021389	47.576551
2229.980402	196.570206	47.581556
2226.247574	182.336081	47.586561
2222.466776	180.183749	47.591565
2219.324823	180.340884	47.596570
2215.607862	197.124003	47.601575
2212.496314	181.542266	47.606580
2208.466408	176.086822	47.611585
2205.386917	166.722407	47.616589
2202.069516	191.078812	47.621594
2198.226465	189.295941	47.626599
2194.772870	179.353092	47.631604
2191.393181	177.768144	47.636609
2188.160130	169.757473	47.641613
2184.150719	181.335662	47.646618
2180.626659	182.815292	47.651623
2177.441659	182.989903	47.656628
2174.116243	182.052125	47.661633
2170.274762	181.233109	47.666637
2166.573945	190.314407	47.671642
2163.202225	186.647349	47.676647
2159.722064	166.261772	47.681652
2155.913204	177.608113	47.686657
2152.843044	177.614635	47.691661
2149.463525	172.888987	47.696666
2145.897222	175.650442	47.701671
2142.407839	193.208320	47.706676
2138.859563	170.235173	47.711681
2135.463661	166.801087	47.716685
2131.572000	172.702844	47.721690
2128.125629	185.376021	47.726695
2125.144430	179.809595	47.731700
2121.117063	167.204692	47.736705
2118.287824	175.506640	47.741709
2114.504432	175.630529	47.746714
2110.604843	194.735915	47.751719
2107.342493	179.465592	47.756724
2103.503632	180.147914	47.761729
2100.399876	160.065299	47.766733
2096.767274	174.466944	47.771738
2093.061574	186.847504	47.776743
2089.922770	173.599841	47.781748
2086.201673	169.810224	47.786753
2083.138638	156.532226	47.791757
2079.698350	179.570537	47.796762
2075.863483	181.978474	47.801767
2072.080684	152.893223	47.806772
2068.754246	161.301659	47.811777
2065.329023	167.027558	47.816781
2061.849002	184.086911	47.821786
2058.089321	168.715081	47.826791
2054.921712	156.376618	47.831796
2050.837542	177.439556	47.836801
2048.060799	181.754257	47.841805
2044.220430	174.492655	47.846810
2040.861972	169.461132	47.851815
2037.491777	171.684710	47.856820
2033.408304	170.526381	47.861825
2030.311682	159.822374	47.866829
2026.751444	186.637634	47.871834
2023.252931	178.350720	47.876839
2019.936740	170.112261	47.881844
2016.304028	181.189391	47.886849
2012.832833	158.938179	47.891853
2009.278222	173.314754	47.896858
2005.905556	168.528664	47.901863
2002.349139	160.186414	47.906868
1999.102099	170.999171	47.911873
1995.232774	186.863712	47.916877
1991.691292	171.909122	47.921882
1988.097703	167.820927	47.926887
1984.937200	162.006160	47.931892
1981.087632	180.753215	47.936897
1977.821974	181.970323	47.941901
1974.285064	170.056142	47.946906
1970.875982	155.931177	47.951911
1967.738750	146.617462	47.956916
1963.535065	174.084290	47.961921
1959.920869	187.112823	47.966925
1956.501240	182.319901	47.971930
1953.229312	162.995911	47.976935
1949.922803	171.883796	47.981940
1946.697256	163.605172	47.986945
1943.077867	150.907057	47.991949
1939.068056	169.781268	47.996954
1935.589689	168.429354	48.001959
1932.467153	162.736593	48.006964
1928.347660	170.088581	48.011969
1925.002646	166.238786	48.016973
1922.034953	153.830623	48.021978
1918.565996	167.580484	48.026983
1914.965339	163.668005	48.031988
1911.179906	181.060808	48.036993
1907.761761	158.689840	48.041997
1904.256586	157.539170	48.047002
1900.364066	170.437638	48.052007
1897.242225	168.499054	48.057012
1893.766983	165.647678	48.062017
1890.722091	166.689208	48.067021
1887.013090	171.258187	48.072026
1883.331881	168.490022	48.077031
1879.918335	164.050193	48.082036
1876.095992	179.956935	48.087041
1872.644961	157.310567	48.092045
1869.325632	169.826131	48.097050
1865.599512	163.669107	48.102055
1862.042819	161.343468	48.107060
1858.566856	178.893969	48.112065
1855.209653	162.830546	48.117069
1852.010860	161.522023	48.122074
1848.128253	163.320308	48.127079
1844.903769	159.754704	48.132084
1841.177673	159.763431	48.137089
1837.756792	158.391625	48.142093
1834.373156	148.043462	48.147098
1830.781771	164.087595	48.152103
1827.247062	157.029526	48.157108
1823.567724	157.244517	48.162113
1820.242095	150.382403	48.167117
1816.703876	161.475178	48.172122
1812.964481	161.915335	48.177127
1809.671111	143.169730	48.182132
1805.937414	159.474694	48.187137
1802.886264	163.845894	48.192141
1799.321550	159.068122	48.197146
1795.677095	167.172121	48.202151
1792.412990	145.394466	48.207156
1788.355775	166.822271	48.212161
1785.292061	164.743439	48.217165
1781.923369	147.827875	48.222170
1778.299378	152.491387	48.227175
1774.797029	156.719225	48.232180
1771.319168	169.753135	48.237185
1767.534689	151.140765	48.242189
1764.067407	152.973061	48.247194
1760.438050	159.690936	48.252199
1757.178781	153.341335	48.257204
1753.479010	161.476968	48.262209
1749.993319	153.525881	48.267213
1746.694393	152.993917	48.272218
1743.201674	164.557265	48.277223
1739.806996	144.514224	48.282228
1736.158058	142.526159	48.287233
1732.397131	158.097849	48.292237
1729.305630	162.095937	48.297242
1725.910855	154.325581	48.302247
1722.637525	161.993902	48.307252
1718.743442	161.042545	48.312257
1715.094412	143.790924	48.317261
1711.487639	149.898600	48.322266
1707.935803	171.756908	48.327271
1704.726746	157.627712	48.332276
1701.064073	142.449084	48.337281
1697.720551	160.931787	48.342285
1694.359895	164.313554	48.347290
1690.215214	154.980068	48.352295
1687.227931	142.279823	48.357300
1683.647715	163.600342	48.362305
1679.966508	151.677910	48.367309
1676.623476	157.187285	48.372314
1672.990785	171.922027	48.377319
1670.029501	164.009929	48.382324
1666.358187	156.378262	48.387329
1662.766699	141.960628	48.392333
1659.229762	146.874205	48.397338
1655.016906	147.917576	48.402343
1651.917148	154.130527	48.407348
1648.532851	153.311720	48.412353
1644.911185	159.809575	48.417357
1641.808411	154.412308	48.422362
1637.901316	138.049342	48.427367
1634.438706	151.964163	48.432372
1631.278234	156.051503	48.437377
1627.633110	142.444951	48.442381
1624.398671	154.107373	48.447386
1620.680672	157.128981	48.452391
1617.219813	147.574588	48.457396
1613.698120	148.143468	48.462401
1609.875828	153.763820	48.467405
1606.624275	140.710763	48.472410
1602.727627	159.548552	48.477415
1599.469566	156.671552	48.482420
1595.719964	151.671273	48.487425
1592.223104	165.806431	48.492429
1588.876278	145.918662	48.497434
1585.564438	129.514335	48.502439
1582.566489	133.806002	48.507444
1578.534044	163.009084	48.512449
1574.993732	157.887270	48.517453
1572.123297	134.468516	48.522458
1568.117281	141.663540	48.527463
1564.494839	150.967406	48.532468
1560.849640	146.247839	48.537473
1557.540093	132.867604	48.542477
1553.939851	149.012317	48.547482
1550.457124	156.368310	48.552487
1546.953998	149.503181	48.557492
1543.664297	151.066362	48.562497
1539.944428	140.912859	48.567501
1536.741300	149.830778	48.572506
1533.098768	138.457655	48.577511
1529.312663	139.027596	48.582516
1525.739093	160.230356	48.587521
1522.361945	145.758301	48.592525
1519.172524	134.543322	48.597530
1515.483938	141.139475	48.602535
1511.807541	136.549877	48.607540
1508.247962	143.841225	48.612545
1505.150570	142.548487	48.617549
1501.760352	123.422332	48.622554
1498.154677	140.623387	48.627559
1494.586083	157.634955	48.632564
1490.913559	151.850390	48.637569
1487.392875	138.279036	48.642573
1484.021849	139.297118	48.647578
1480.390812	153.673842	48.652583
1477.149069	153.375833	48.657588
1473.279046	140.043555	48.662593
1469.409708	129.341134	48.667597
1466.396858	137.759287	48.672602
1463.007604	151.613920	48.677607
1459.581172	141.225792	48.682612
1456.034707	130.856694	48.687617
1452.712523	139.591367	48.692621
1449.265729	135.878971	48.697626
1445.444605	139.211063	48.702631
1441.956780	139.674902	48.707636
1438.192112	140.456801	48.712641
1434.902237	148.796000	48.717645
1431.484497	139.414640	48.722650
1427.549280	139.258928	48.727655
1424.644104	128.955362	48.732660
1420.931193	139.040904	48.737665
1417.148498	144.542154	48.742669
1413.986669	133.070834	48.747674
1410.511017	144.109526	48.752679
1407.112304	142.661475	48.757684
1403.587866	137.595444	48.762689
1400.028090	148.591995	48.767693
1396.650521	146.475374	48.772698
1393.080079	133.117387	48.777703
1389.334901	126.766313	48.782708
1385.774775	146.689582	48.787713
1382.021638	153.675263	48.792717
1378.855948	134.429157	48.797722
1374.988554	130.070334	48.802727
1372.021246	151.549008	48.807732
1368.565530	141.335246	48.812737
1364.589951	132.892895	48.817741
1361.500868	141.676434	48.822746
1357.769915	139.718880	48.827751
1354.354152	112.437194	48.832756
1351.027222	135.799600	48.837761
1347.246911	153.682001	48.842765
1344.124837	127.861629	48.847770
1340.358983	136.611865	48.852775
1336.892520	125.187425	48.857780
1333.042850	138.874325	48.862785
1329.486328	141.509949	48.867789
1326.142213	129.824025	48.872794
1322.374261	144.337433	48.877799
1319.682667	126.276410	48.882804
1316.382194	122.915785	48.887809
1312.700499	123.851658	48.892813
1309.067822	150.141923	48.897818
1305.201816	146.128176	48.902823
1301.712963	144.166007	48.907828
1298.217751	148.642361	48.912833
1294.567751	133.493595	48.917837
1291.094204	119.996581	48.922842
1287.816297	140.674208	48.927847
1284.408432	143.277622	48.932852
1281.054134	133.261540	48.937857
1276.974168	150.495688	48.942861
1273.843092	136.727778	48.947866
1270.339952	123.965061	48.952871
1267.044343	125.878160	48.957876
1263.496148	148.771756	48.962881
1259.774446	130.353527	48.967885
1256.229805	119.854539	48.972890
1252.330468	117.580069	48.977895
1249.312345	136.377010	48.982900
1245.709208	150.494996	48.987905
1242.040307	134.338047	48.992909
1238.833117	126.986752	48.997914
1235.240358	136.556143	49.002919
1232.172537	126.802954	49.007924
1228.543522	124.851238	49.012929
1224.644679	122.346162	49.017933
1221.137578	123.971023	49.022938
1217.485219	128.303872	49.027943
1214.107504	134.538005	49.032948
1210.760271	143.324160	49.037953
1207.287777	141.488077	49.042957
1204.073258	137.671868	49.047962
1200.032451	131.040817	49.052967
1196.827746	129.195654	49.057972
1193.068526	134.692542	49.062977
1189.715361	133.212126	49.067981
1186.213571	132.174216	49.072986
1182.634395	144.153822	49.077991
1179.273638	132.287840	49.082996
1175.290034	124.403417	49.088001
1172.080437	136.595463	49.093005
1169.077795	131.502223	49.098010
1165.250895	148.081641	49.103015
1161.700808	151.026237	49.108020
1157.985613	147.447875	49.113025
1154.614894	120.040519	49.118029
1151.292376	123.136459	49.123034
1147.755245	145.933653	49.128039
1144.138187	127.597773	49.133044
1140.692954	127.820936	49.138049
1136.730279	121.928038	49.143053
1133.483478	137.299833	49.148058
1129.742336	145.244280	49.153063
1126.838824	127.652995	49.158068
1123.456459	129.963926	49.163073
1119.798111	132.512881	49.168077
1116.520609	126.970919	49.173082
1112.630938	129.164462	49.178087
1109.019209	120.076156	49.183092
1105.686422	124.358175	49.188097
1101.924840	129.047572	49.193101
1098.598508	124.876795	49.198106
1094.986442	146.862865	49.203111
1091.618297	134.896745	49.208116
1088.029761	119.518992	49.213121
1084.436775	122.563236	49.218125
1081.124336	136.724132	49.223130
1077.523143	146.309094	49.228135
1074.327434	126.319619	49.233140
1070.658224	116.580779	49.238145
1067.412627	132.200686	49.243149
1064.066225	146.248925	49.248154
1059.965210	144.593828	49.253159
1056.381151	114.893400	49.258164
1053.047506	126.959270	49.263169
1049.374531	140.304305	49.268173
1046.098474	125.074353	49.273178
1042.241935	123.914859	49.278183
1038.963822	122.121945	49.283188
1035.255355	122.860551	49.288193
1031.565225	137.057581	49.293197
1028.964192	130.649818	49.298202
1025.093694	123.900999	49.303207
1021.591543	110.759782	49.308212
1018.571703	133.351730	49.313217
1014.727432	129.773755	49.318221
1011.262493	124.808614	49.323226
1007.408582	120.179767	49.328231
1003.771676	125.281493	49.333236
1000.591386	137.764406	49.338241
997.012483	141.599991	49.343245
993.750864	120.748824	49.348250
989.871762	116.005378	49.353255
986.645685	130.631961	49.358260
983.146386	127.820854	49.363265
979.261930	122.069132	49.368269
976.161005	106.985033	49.373274
972.433300	126.030091	49.378279
968.681250	122.185270	49.383284
965.540687	119.111040	49.388289
962.227145	139.925735	49.393293
958.834271	130.743871	49.398298
954.864753	114.517322	49.403303
951.516151	115.701235	49.408308
947.721896	128.957617	49.413313
944.376073	140.105165	49.418317
940.931629	120.318149	49.423322
937.172331	113.384416	49.428327
933.787844	121.930794	49.433332
930.431627	135.582549	49.438337
926.988434	119.452498	49.443341
923.521486	112.288103	49.448346
919.750390	127.649456	49.453351
916.655006	109.297372	49.458356
913.427485	114.018337	49.463361
909.655215	136.622389	49.468365
906.462957	114.594124	49.473370
902.345638	101.313377	49.478375
898.921179	113.013213	49.483380
895.426552	137.714245	49.488385
891.452588	138.749404	49.493389
888.371571	118.327995	49.498394
884.893805	106.403705	49.503399
881.153447	113.201843	49.508404
878.119683	134.768412	49.513409
874.332547	130.811062	49.518413
871.035776	120.629380	49.523418
867.380092	125.397787	49.528423
863.933519	123.332989	49.533428
860.286457	119.917079	49.538433
857.189623	112.903601	49.543437
853.615690	108.017715	49.548442
849.395209	121.829266	49.553447
846.110222	135.264102	49.558452
843.239477	116.298074	49.563457
839.546870	113.547973	49.568461
835.909182	109.376177	49.573466
832.349469	110.079576	49.578471
828.852458	101.086356	49.583476
825.208253	125.738101	49.588481
821.561994	115.752073	49.593485
818.613180	112.043913	49.598490
814.799819	122.180724	49.603495
811.336735	126.169016	49.608500
808.015961	121.430059	49.613505
804.450417	106.161772	49.618509
801.199341	94.678847	49.623514
797.377087	117.903465	49.628519
793.931803	126.084788	49.633524
790.383802	116.433639	49.638529
786.668212	107.851593	49.643533
783.732841	116.591297	49.648538
779.799227	135.243492	49.653543
776.193410	117.069400	49.658548
772.830252	103.942492	49.663553
768.753194	95.227895	49.668557
765.885650	114.408854	49.673562
762.242124	137.768344	49.678567
758.937878	117.264427	49.683572
755.678997	99.810417	49.688577
751.991569	107.098141	49.693581
748.306745	111.679152	49.698586
744.683540	134.313090	49.703591
741.271360	109.467304	49.708596
737.761762	112.856137	49.713601
733.922595	113.611954	49.718605
730.778103	97.060439	49.723610
727.307200	100.669476	49.728615
723.800563	118.600287	49.733620
720.325668	123.979327	49.738625
716.331111	109.177228	49.743629
713.496774	100.993539	49.748634
709.872840	118.770797	49.753639
706.038271	128.564321	49.758644
702.815663	116.660151	49.763649
699.249845	111.973367	49.768653
695.823647	109.885074	49.773658
692.335992	108.188303	49.778663
688.506489	94.700088	49.783668
685.401153	108.725186	49.788673
681.325908	104.858553	49.793677
678.305947	102.578490	49.798682
674.752779	125.014525	49.803687
671.271225	112.311683	49.808692
667.699840	105.180181	49.813697
664.042158	115.744136	49.818701
660.814751	101.395533	49.823706
657.351707	106.433788	49.828711
653.578487	121.040843	49.833716
650.173077	131.296606	49.838721
647.052212	123.404412	49.843725
643.745240	98.341388	49.848730
639.683722	110.421665	49.853735
636.008893	118.048686	49.858740
632.538413	120.359902	49.863745
628.951603	102.551541	49.868749
625.676095	106.145128	49.873754
622.224890	118.027353	49.878759
618.684955	111.250252	49.883764
615.217153	118.523474	49.888769
611.388140	116.171979	49.893773
608.433143	105.281666	49.898778
604.876240	113.906076	49.903783
601.025100	104.728321	49.908788
597.406451	117.246074	49.913793
593.766172	129.001415	49.918797
590.647179	106.036472	49.923802
587.429515	102.556908	49.928807
583.758917	88.629791	49.933812
580.255705	108.636589	49.938817
576.355799	121.628640	49.943821
573.356484	109.745482	49.948826
569.747311	124.641446	49.953831
566.258708	113.168487	49.958836
562.743643	123.475143	49.963841
559.270496	118.755672	49.968845
555.517663	97.053774	49.973850
551.846878	103.501824	49.978855
548.381935	122.087435	49.983860
545.178394	114.741653	49.988865
541.488103	104.145068	49.993869
538.372539	103.852125	49.998874
534.601173	112.843937	50.003879
531.108967	102.303127	50.008884
527.985839	110.070495	50.013889
523.578605	116.563559	50.018893
520.485850	113.912745	50.023898
516.782849	133.145762	50.028903
513.607666	126.484357	50.033908
510.163944	96.940989	50.038913
506.609681	117.438835	50.043917
503.333639	111.259618	50.048922
499.372673	106.173302	50.053927
495.862349	116.001156	50.058932
492.292308	113.129999	50.063937
489.060615	112.550160	50.068941
485.722678	113.546493	50.073946
482.377413	100.765441	50.078951
478.561743	99.638598	50.083956
475.445807	105.635764	50.088961
471.517757	128.667074	50.093965
468.085310	108.618603	50.098970
464.357811	109.351197	50.103975
460.596371	113.921041	50.108980
457.607883	103.741870	50.113985
453.928942	117.220203	50.118989
450.616210	116.762183	50.123994
446.888349	107.090663	50.128999
443.401268	90.524886	50.134004
440.168592	103.712300	50.139009
436.512686	118.712902	50.144013
433.149286	117.254596	50.149018
429.712559	108.699323	50.154023
426.037654	91.192717	50.159028
422.301091	106.240596	50.164033
418.869153	115.250872	50.169037
415.815132	103.185548	50.174042
411.946512	92.648803	50.179047
408.349388	102.243225	50.184052
404.849278	116.372131	50.189057
400.946796	121.506386	50.194061
397.807655	108.935088	50.199066
394.708942	108.179933	50.204071
390.739093	113.786691	50.209076
387.259916	95.301753	50.214081
383.871601	107.131455	50.219085
380.955979	119.644954	50.224090
377.121261	124.067241	50.229095
373.562545	116.578202	50.234100
370.222245	102.474017	50.239105
366.431290	123.202909	50.244109
362.802590	109.276876	50.249114
359.159586	107.220541	50.254119
355.999721	111.212227	50.259124
352.830766	106.985778	50.264129
348.835607	101.050143	50.269133
345.281798	97.899000	50.274138
341.722421	110.657132	50.279143
338.235574	123.546751	50.284148
335.145850	111.923780	50.289153
331.107347	98.373383	50.294157
327.775816	106.479188	50.299162
324.275936	98.911121	50.304167
320.560263	94.780538	50.309172
317.454427	107.894343	50.314177
314.012584	127.091013	50.319181
310.298152	107.501272	50.324186
306.751568	105.975047	50.329191
303.232302	116.916211	50.334196
299.762335	104.297139	50.339201
296.612051	109.191267	50.344205
292.891169	114.664417	50.349210
289.397715	110.761509	50.354215
285.656654	97.463767	50.359220
282.214330	104.282011	50.364225
278.365786	131.887353	50.369229
275.269187	130.885979	50.374234
271.997676	111.272212	50.379239
268.491552	111.542388	50.384244
265.362308	103.502257	50.389249
261.435404	128.228102	50.394253
257.876641	101.917069	50.399258
254.221532	89.770468	50.404263
250.821310	106.197539	50.409268
247.404952	114.235521	50.414273
243.624651	106.145233	50.419277
240.475223	94.203335	50.424282
236.775040	88.397696	50.429287
233.056758	106.139110	50.434292
229.704900	118.200301	50.439297
226.146140	121.354746	50.444301
222.929394	96.143284	50.449306
219.353728	101.466010	50.454311
215.687545	126.378736	50.459316
212.780681	112.214502	50.464321
208.709675	99.393734	50.469325
205.402756	97.645967	50.474330
201.913729	111.655407	50.479335
198.347271	127.354451	50.484340
194.841223	97.355643	50.489345
190.718146	119.003589	50.494349
187.470616	98.456810	50.499354
183.940726	99.808869	50.504359
180.630547	115.238873	50.509364
177.218710	120.796760	50.514369
173.584022	117.581836	50.519373
170.437574	105.492596	50.524378
167.156637	110.258919	50.529383
163.322158	113.443761	50.534388
160.258648	107.994137	50.539393
156.179694	119.996258	50.544397
152.681563	112.250242	50.549402
148.896048	115.897053	50.554407
145.445328	113.253198	50.559412
142.663188	93.004024	50.564417
138.701617	108.692302	50.569421
134.852344	103.624966	50.574426
131.427901	121.366912	50.579431
128.192860	111.427537	50.584436
125.039973	99.506205	50.589441
121.140344	104.735135	50.594445
117.938500	110.946900	50.599450
114.491541	119.539067	50.604455
110.711074	96.057092	50.609460
107.370572	99.834686	50.614465
103.451033	114.436948	50.619469
100.413423	119.636995	50.624474
96.820917	108.368359	50.629479
92.887773	106.888573	50.634484
89.665247	85.815124	50.639489
86.010060	100.211524	50.644493
82.713980	91.097985	50.649498
79.293778	102.408573	50.654503
75.048101	113.099057	50.659508
72.101742	98.064186	50.664513
68.463275	111.980196	50.669517
65.120916	104.499309	50.674522
61.709834	118.183616	50.679527
58.015240	112.058729	50.684532
54.893211	102.329491	50.689537
51.206022	94.155494	50.694541
47.710550	95.576121	50.699546
44.373215	89.731361	50.704551
40.509004	114.065535	50.709556
37.315708	94.304606	50.714561
33.406549	104.577860	50.719565
30.107731	101.489725	50.724570
26.737948	117.228731	50.729575
23.105880	117.178340	50.734580
19.757848	94.424612	50.739585
15.714504	87.614983	50.744589
12.671251	101.197670	50.749594
9.248579	104.663951	50.754599
5.334632	101.458883	50.759604
2.306107	89.177347	50.764609