Wed Jun 15 16:41:52 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.208229	118.535355	0.000000
0.376621	123.687390	0.005005
0.554852	118.083169	0.010010
0.670091	121.380162	0.015014
1.276805	136.862528	0.020019
0.607385	114.890197	0.025024
0.656295	109.469821	0.030029
0.426773	123.224470	0.035034
0.112013	95.917651	0.040038
0.110468	67.309177	0.045043
0.266272	76.524436	0.050048
-0.359613	69.390142	0.055053
-0.417908	50.124677	0.060058
-0.885884	41.007066	0.065062
-0.972481	10.975186	0.070067
-1.129946	18.063688	0.075072
-1.445967	-0.941016	0.080077
-1.941762	-15.485522	0.085082
-2.618776	-8.686323	0.090086
-2.885193	-33.228168	0.095091
-3.104164	-39.605079	0.100096
-3.501340	-39.745377	0.105101
-4.131638	-28.994479	0.110106
-4.238572	-43.538014	0.115110
-4.450793	-32.357555	0.120115
-5.064475	-34.642730	0.125120
-5.353951	-55.535386	0.130125
-5.634835	-34.200773	0.135130
-6.100059	-16.808912	0.140134
-5.676271	-34.912087	0.145139
-5.773483	-38.319177	0.150144
-5.845537	-19.491008	0.155149
-5.627849	-42.735550	0.160154
-6.582184	-36.288865	0.165158
-6.854082	-14.517132	0.170163
-7.016348	-24.733430	0.175168
-7.199250	-49.988149	0.180173
-7.337849	-40.819700	0.185178
-8.066621	-16.878820	0.190182
-8.369603	-23.366443	0.195187
-8.778425	-29.471387	0.200192
-8.829886	-38.968513	0.205197
-8.430160	-31.481353	0.210202
-8.545037	-12.911555	0.215206
-9.057920	-25.799433	0.220211
-9.664796	-29.750276	0.225216
-10.422418	-24.349083	0.230221
-10.083098	-37.745631	0.235226
-10.494626	-40.065100	0.240230
-10.133998	-45.192563	0.245235
-10.919847	-22.884508	0.250240
-11.831307	-11.743157	0.255245
-11.842037	-18.450721	0.260250
-12.118860	-36.143065	0.265254
-11.675919	-39.222345	0.270259
-11.755377	-24.818981	0.275264
-12.000130	-28.197153	0.280269
-12.532092	-45.051845	0.285274
-12.802628	-43.530280	0.290278
-12.820533	-36.173272	0.295283
-13.167105	-9.172034	0.300288
-13.568605	-26.992246	0.305293
-14.093440	-40.907696	0.310298
-14.561483	-41.880983	0.315302
-14.538175	-32.785451	0.320307
-14.881308	-35.577587	0.325312
-14.798970	-32.580006	0.330317
-14.468110	-22.952990	0.335322
-15.587371	-17.202703	0.340326
-15.745926	-46.761208	0.345331
-16.173294	-37.511398	0.350336
-16.350981	-20.198232	0.355341
-16.118273	-28.861914	0.360346
-16.554849	-31.522305	0.365350
-16.588199	-35.568616	0.370355
-17.577243	-12.200364	0.375360
-18.057507	-28.809013	0.380365
-18.214131	-39.256372	0.385370
-18.531426	-20.837009	0.390374
-18.246600	-30.879390	0.395379
-18.353850	-39.819616	0.400384
-18.626378	-32.073000	0.405389
-18.110172	-22.932652	0.410394
-18.756185	-12.557845	0.415398
-19.124401	-27.463548	0.420403
-19.494204	-42.516745	0.425408
-19.665328	-31.311611	0.430413
-20.443621	-19.109540	0.435418
-20.989544	-24.030671	0.440422
-21.071676	-41.011888	0.445427
-21.314034	-31.394713	0.450432
-21.401374	-17.495401	0.455437
-21.308682	-20.291892	0.460442
-21.304126	-32.916264	0.465446
-21.142808	-46.136308	0.470451
-21.916441	-38.749307	0.475456
-22.861608	-11.569645	0.480461
-22.936958	-18.390429	0.485466
-22.746630	-26.714673	0.490470
-22.636885	-41.939648	0.495475
-22.991049	-27.034852	0.500480
-24.263303	-21.520792	0.505485
-24.116768	-37.570017	0.510490
-24.416281	-38.413519	0.515494
-24.223664	-27.538585	0.520499
-24.520868	-39.861733	0.525504
-24.571839	-28.700523	0.530509
-25.407156	-34.154157	0.535514
-25.904934	-33.770298	0.540518
-25.955357	-20.565043	0.545523
-26.163146	-33.300613	0.550528
-26.338926	-33.231279	0.555533
-25.815787	-34.631947	0.560538
-26.342982	-25.116750	0.565542
-27.261495	-24.236324	0.570547
-27.598354	-31.705192	0.575552
-27.644273	-40.330120	0.580557
-27.708792	-37.696144	0.585562
-28.074771	-24.031141	0.590566
-28.004000	-21.716937	0.595571
-28.163448	-21.805273	0.600576
-28.454926	-20.763114	0.605581
-28.877669	-35.714347	0.610586
-29.395802	-35.445104	0.615590
-29.430018	-48.389571	0.620595
-29.544859	-22.830577	0.625600
-29.930126	-23.039427	0.630605
-30.567523	-28.523994	0.635610
-31.183729	-29.075648	0.640614
-30.936802	-32.811576	0.645619
-30.974477	-38.280820	0.650624
-31.245801	-45.099390	0.655629
-30.880568	-21.829781	0.660634
-31.156726	-20.047354	0.665638
-31.718548	-38.818727	0.670643
-32.286843	-19.685518	0.675648
-32.561909	-29.769824	0.680653
-32.344215	-42.217915	0.685658
-32.758164	-18.116093	0.690662
-33.574754	-22.828149	0.695667
-33.853294	-25.410093	0.700672
-33.952093	-27.026507	0.705677
-33.858025	-33.194627	0.710682
-34.010060	-41.312145	0.715686
-34.382951	-27.372657	0.720691
-34.451882	-12.302208	0.725696
-35.160808	-34.857878	0.730701
-35.596471	-42.978141	0.735706
-35.764468	-34.251498	0.740710
-35.820242	-26.026659	0.745715
-35.718774	-6.373085	0.750720
-35.793587	-17.190284	0.755725
-35.979457	-47.792966	0.760730
-37.125328	-33.116409	0.765734
-37.151687	-23.482546	0.770739
-37.602897	-24.002378	0.775744
-37.694913	-46.427968	0.780749
-37.676484	-42.077068	0.785754
-37.930269	-16.387284	0.790758
-37.817129	-33.578239	0.795763
-38.369795	-22.448643	0.800768
-38.863612	-20.346146	0.805773
-38.603952	-31.259647	0.810778
-39.142200	-20.900979	0.815782
-39.185538	-27.045604	0.820787
-40.223514	-21.288527	0.825792
-40.609038	-24.264339	0.830797
-40.495681	-46.255402	0.835802
-40.486910	-27.271430	0.840806
-40.665709	-14.304394	0.845811
-40.639257	-22.748439	0.850816
-40.602519	-33.688429	0.855821
-41.231696	-33.048768	0.860826
-41.942614	-31.790113	0.865830
-42.002971	-40.561806	0.870835
-42.347433	-18.907123	0.875840
-42.517448	-28.503724	0.880845
-42.329005	-43.262679	0.885850
-43.303321	-39.110829	0.890854
-43.809292	-37.726239	0.895859
-43.908325	-30.039763	0.900864
-44.133718	-32.029343	0.905869
-43.928365	-28.354570	0.910874
-44.047624	-30.248840	0.915878
-44.205855	-27.367756	0.920883
-44.274465	-17.248970	0.925888
-45.046028	-17.626882	0.930893
-45.544555	-49.222345	0.935898
-46.021296	-26.029832	0.940902
-45.718859	-9.828132	0.945907
-45.589800	-12.834633	0.950912
-45.708449	-29.378643	0.955917
-46.218432	-34.354536	0.960922
-47.297097	-17.963072	0.965926
-47.335049	-35.458136	0.970931
-47.364152	-28.368084	0.975936
-47.799731	-16.455057	0.980941
-47.840800	-26.672537	0.985946
-47.665050	-30.508566	0.990950
-47.603465	-37.275716	0.995955
-48.554069	-46.657383	1.000960
-48.939779	-40.064072	1.005965
-49.033597	-29.099487	1.010970
-49.206275	-18.369954	1.015974
-49.320157	-36.066134	1.020979
-49.977333	-32.859926	1.025984
-50.561452	-27.009567	1.030989
-50.604479	-37.132707	1.035994
-50.806412	-19.426678	1.040998
-50.779483	-11.674794	1.046003
-50.418216	-27.158466	1.051008
-51.171523	-26.104004	1.056013
-50.721274	-32.429337	1.061018
-51.734290	-27.031904	1.066022
-51.907162	-23.666123	1.071027
-51.814984	-29.859480	1.076032
-52.731745	-26.314633	1.081037
-53.139820	-36.579271	1.086042
-53.518687	-45.763928	1.091046
-53.766962	-36.370791	1.096051
-53.732663	-26.379601	1.101056
-54.351803	-37.041227	1.106061
-53.609740	-38.906001	1.111066
-54.011921	-32.877471	1.116070
-53.838567	-34.690084	1.121075
-54.014793	-42.519601	1.126080
-55.324972	-28.031029	1.131085
-55.381517	-19.904608	1.136090
-55.903598	-29.490275	1.141094
-55.730135	-45.197396	1.146099
-55.721533	-33.304522	1.151104
-56.517054	-12.944487	1.156109
-56.939105	-23.089337	1.161114
-57.284139	-31.168747	1.166118
-57.338525	-49.297537	1.171123
-56.879515	-33.807522	1.176128
-57.515183	-13.983213	1.181133
-57.388335	-26.422021	1.186138
-57.654821	-23.904310	1.191142
-57.966912	-11.664753	1.196147
-58.492233	-22.713491	1.201152
-58.990479	-43.819345	1.206157
-58.783583	-38.040430	1.211162
-58.950693	-12.109181	1.216166
-59.978562	-10.309354	1.221171
-60.308113	-32.580385	1.226176
-60.667212	-24.127956	1.231181
-60.381103	-18.981816	1.236186
-60.668638	-11.060180	1.241190
-60.554926	-21.795284	1.246195
-60.616797	-48.053981	1.251200
-61.015980	-24.834827	1.256205
-61.171480	-14.256100	1.261210
-62.253015	-23.698805	1.266214
-62.190829	-34.895726	1.271219
-62.385659	-30.165899	1.276224
-62.368081	-21.019208	1.281229
-62.356752	-33.368683	1.286234
-63.187386	-22.967417	1.291238
-63.645906	-12.943110	1.296243
-63.811009	-19.734161	1.301248
-64.056160	-40.908183	1.306253
-63.742998	-31.110360	1.311258
-64.214877	-3.398392	1.316262
-64.189054	-22.705076	1.321267
-64.616199	-40.743170	1.326272
-64.990366	-33.707367	1.331277
-64.999293	-20.474251	1.336282
-65.385632	-17.020020	1.341286
-65.618098	-35.065139	1.346291
-66.217830	-53.039577	1.351296
-66.723609	-29.815639	1.356301
-66.906930	-19.531707	1.361306
-67.072238	-28.241472	1.366310
-66.959469	-43.619050	1.371315
-66.933598	-44.164851	1.376320
-67.119878	-16.310806	1.381325
-67.670112	-19.894672	1.386330
-68.415243	-26.641254	1.391334
-68.585579	-39.540144	1.396339
-68.380651	-28.563576	1.401344
-68.725938	-7.175876	1.406349
-68.588112	-27.641603	1.411354
-69.348517	-37.094951	1.416358
-69.854156	-33.222184	1.421363
-69.747089	-24.002491	1.426368
-70.330935	-14.312990	1.431373
-70.205499	-42.820691	1.436378
-70.513362	-28.972548	1.441382
-70.350953	-29.867529	1.446387
-70.958707	-39.173376	1.451392
-71.642234	-11.874987	1.456397
-71.805700	-16.344884	1.461402
-72.243083	-22.351389	1.466406
-72.139128	-33.955023	1.471411
-72.081762	-22.531566	1.476416
-72.303057	-36.100617	1.481421
-72.818586	-47.553525	1.486426
-73.182988	-34.217975	1.491430
-73.477312	-21.723109	1.496435
-73.470087	-40.943044	1.501440
-73.854741	-26.924869	1.506445
-73.664553	-30.014565	1.511450
-74.339743	-36.077942	1.516454
-74.784033	-39.909057	1.521459
-74.757985	-19.658669	1.526464
-75.137860	-13.835252	1.531469
-74.952493	-43.776506	1.536474
-75.402284	-42.781477	1.541478
-76.208080	-22.674756	1.546483
-76.451986	-27.511436	1.551488
-76.475954	-28.515593	1.556493
-76.584730	-34.127466	1.561498
-76.849553	-39.829356	1.566502
-76.614515	-42.889569	1.571507
-77.127075	-36.476332	1.576512
-77.814389	-45.855241	1.581517
-78.018093	-32.121086	1.586522
-78.213202	-30.132863	1.591526
-78.328963	-27.074924	1.596531
-78.390960	-44.511149	1.601536
-78.565182	-40.973111	1.606541
-79.170627	-31.069247	1.611546
-79.899862	-50.012780	1.616550
-80.061952	-51.449060	1.621555
-80.044527	-27.072507	1.626560
-80.353581	-34.054806	1.631565
-80.100293	-46.260875	1.636570
-80.240909	-46.078877	1.641574
-80.468544	-24.170170	1.646579
-80.352746	-26.913560	1.651584
-81.533590	-31.567969	1.656589
-81.828353	-52.220224	1.661594
-81.885909	-40.954758	1.666598
-82.061636	-11.511403	1.671603
-81.907597	-28.467533	1.676608
-82.637612	-42.700135	1.681613
-82.780541	-61.672189	1.686618
-83.295777	-42.240405	1.691622
-83.589318	-23.245242	1.696627
-83.636156	-51.835920	1.701632
-83.844966	-37.377858	1.706637
-83.833924	-26.951452	1.711642
-85.084599	-28.858391	1.716646
-85.453432	-26.324555	1.721651
-84.668362	-23.339339	1.726656
-84.927882	-20.779079	1.731661
-84.989853	-47.824942	1.736666
-85.186826	-43.001152	1.741670
-85.472814	-36.082810	1.746675
-86.130461	-27.480720	1.751680
-87.028782	-29.569692	1.756685
-86.843617	-43.902740	1.761690
-87.125658	-36.258628	1.766694
-87.149731	-22.418911	1.771699
-86.918286	-35.377100	1.776704
-87.319342	-32.848790	1.781709
-87.906410	-34.781948	1.786714
-88.354858	-45.344617	1.791718
-88.404805	-35.071495	1.796723
-88.233497	-35.432401	1.801728
-88.715703	-33.145382	1.806733
-88.903627	-32.448726	1.811738
-89.444290	-34.786994	1.816742
-90.056269	-21.626157	1.821747
-89.978131	-35.622307	1.826752
-90.191884	-27.387444	1.831757
-90.053436	-39.881621	1.836762
-90.175615	-30.279577	1.841766
-90.570162	-32.175994	1.846771
-90.790335	-34.319531	1.851776
-91.285256	-26.480228	1.856781
-91.291354	-29.343450	1.861786
-92.080957	-21.210506	1.866790
-92.833690	-42.125436	1.871795
-92.730564	-37.490133	1.876800
-93.112649	-26.342272	1.881805
-92.825146	-27.222711	1.886810
-93.275173	-29.946866	1.891814
-93.206211	-35.148055	1.896819
-93.163925	-39.187033	1.901824
-93.343211	-35.614125	1.906829
-93.985725	-33.297652	1.911834
-94.658223	-29.591341	1.916838
-94.665325	-30.612983	1.921843
-94.970205	-37.814369	1.926848
-95.287251	-29.135105	1.931853
-95.070898	-30.095229	1.936858
-95.672865	-49.946119	1.941862
-96.448522	-29.401966	1.946867
-96.299898	-22.852370	1.951872
-96.858612	-31.954135	1.956877
-96.566014	-48.223289	1.961882
-96.455237	-39.546079	1.966886
-96.490745	-20.187437	1.971891
-96.857353	-27.690148	1.976896
-97.539240	-33.040098	1.981901
-97.718850	-38.542996	1.986906
-97.830716	-22.535640	1.991910
-98.879181	-21.084568	1.996915
-99.009456	-29.876345	2.006912
-98.372540	-35.519658	2.016909
-97.894461	-41.449231	2.026906
-97.022942	-27.054208	2.036902
-96.781266	-39.098185	2.046899
-96.769027	-27.232525	2.056896
-95.738690	-46.381301	2.066893
-95.545057	-33.884546	2.076890
-94.963402	-41.424918	2.086886
-94.291796	-23.227727	2.096883
-94.003301	-40.691437	2.106880
-93.094528	-39.569080	2.116877
-92.384944	-21.699171	2.126874
-92.268203	-29.792184	2.136870
-92.078332	-40.352048	2.146867
-91.573173	-43.502318	2.156864
-91.059953	-41.288549	2.166861
-90.626576	-30.588757	2.176858
-89.705870	-24.189618	2.186854
-89.510111	-32.800016	2.196851
-88.376521	-32.875775	2.206848
-87.978132	-29.555155	2.216845
-87.934541	-43.458265	2.226842
-87.677061	-22.541995	2.236838
-86.517589	-33.371648	2.246835
-86.469021	-17.104001	2.256832
-86.389807	-25.217483	2.266829
-85.298686	-17.800808	2.276826
-84.857338	-31.300500	2.286822
-83.811127	-34.443294	2.296819
-83.313837	-35.221943	2.306816
-83.130319	-30.388089	2.316813
-83.050072	-20.249818	2.326810
-83.033775	-34.983243	2.336806
-81.951148	-30.004434	2.346803
-80.895908	-35.615345	2.356800
-80.444596	-28.079995	2.366797
-80.155682	-33.679722	2.376794
-79.912846	-41.691734	2.386790
-79.546788	-26.747955	2.396787
-78.838148	-46.990009	2.406784
-78.519663	-31.232297	2.416781
-77.409653	-48.843523	2.426778
-77.002462	-29.095480	2.436774
-76.899371	-42.058439	2.446771
-76.793694	-27.938744	2.456768
-75.539539	-34.136243	2.466765
-75.421416	-36.955371	2.476762
-74.813343	-13.463676	2.486758
-73.759191	-35.256079	2.496755
-73.718176	-17.765575	2.506752
-73.633323	-25.464753	2.516749
-73.202580	-31.799767	2.526746
-72.265324	-20.607697	2.536742
-71.697259	-14.147109	2.546739
-71.155435	-31.847773	2.556736
-70.715497	-18.226004	2.566733
-70.362488	-11.924158	2.576730
-69.242312	-33.350265	2.586726
-69.052907	-28.463256	2.596723
-68.803901	-15.117603	2.606720
-68.675830	-27.249194	2.616717
-67.626850	-34.755288	2.626714
-67.280440	-30.591060	2.636710
-66.924571	-19.343697	2.646707
-65.936338	-30.040451	2.656704
-65.786617	-36.616248	2.666701
-65.737320	-31.669737	2.676698
-64.634499	-34.425514	2.686694
-64.405302	-29.410751	2.696691
-63.581022	-30.116220	2.706688
-62.906085	-30.516793	2.716685
-62.659465	-44.546600	2.726682
-62.761585	-25.611124	2.736678
-61.808668	-35.182165	2.746675
-61.424534	-35.098107	2.756672
-60.719739	-22.231761	2.766669
-59.946221	-38.053551	2.776666
-59.706482	-28.544444	2.786662
-59.483140	-28.074778	2.796659
-58.457149	-32.945202	2.806656
-57.915912	-19.966583	2.816653
-57.851983	-42.620381	2.826650
-57.496733	-25.928330	2.836646
-56.572968	-22.610082	2.846643
-56.317433	-39.905081	2.856640
-55.697689	-20.885526	2.866637
-54.728974	-32.595512	2.876634
-54.530914	-33.445603	2.886630
-54.501883	-26.554975	2.896627
-54.279415	-24.431232	2.906624
-53.190996	-21.873377	2.916621
-52.808530	-31.059262	2.926618
-52.106370	-22.136826	2.936614
-51.705385	-24.537192	2.946611
-51.441281	-32.108353	2.956608
-50.417196	-18.035824	2.966605
-50.059891	-22.972640	2.976602
-50.095272	-34.843324	2.986598
-49.230749	-26.729994	2.996595
-48.639456	-25.617684	3.006592
-48.376300	-19.598489	3.016589
-47.136787	-31.420986	3.026586
-47.188121	-25.514374	3.036582
-46.826319	-25.108382	3.046579
-46.695901	-18.714733	3.056576
-45.759639	-40.634521	3.066573
-45.152854	-18.221690	3.076570
-44.284512	-27.365793	3.086566
-44.170081	-23.599400	3.096563
-43.716799	-31.045173	3.106560
-43.523419	-21.906398	3.116557
-42.323262	-29.667219	3.126554
-42.050763	-39.388443	3.136550
-41.867815	-16.998410	3.146547
-41.536303	-40.689586	3.156544
-40.958848	-28.478387	3.166541
-39.918235	-22.406726	3.176538
-39.201515	-29.070107	3.186534
-39.353091	-24.089110	3.196531
-39.068650	-27.921172	3.206528
-38.170770	-39.894328	3.216525
-37.700528	-22.503993	3.226522
-37.508068	-29.543578	3.236518
-36.378995	-31.834426	3.246515
-35.994986	-37.228618	3.256512
-35.784685	-23.983244	3.266509
-35.530760	-38.153832	3.276506
-34.676461	-30.420761	3.286502
-34.149730	-38.824408	3.296499
-33.195842	-18.293248	3.306496
-32.645519	-42.932642	3.316493
-32.649179	-31.261102	3.326490
-32.736420	-43.845132	3.336486
-32.014298	-33.070869	3.346483
-31.427319	-34.920600	3.356480
-30.376602	-29.682168	3.366477
-29.439797	-33.107339	3.376474
-29.379964	-26.205700	3.386470
-29.544954	-17.857923	3.396467
-29.041808	-36.857463	3.406464
-28.091802	-12.317695	3.416461
-27.818256	-37.657480	3.426458
-27.085309	-30.145949	3.436454
-26.338575	-33.607861	3.446451
-26.238658	-27.332934	3.456448
-25.730730	-33.741349	3.466445
-24.561367	-35.256679	3.476442
-24.766029	-33.624656	3.486438
-24.179838	-26.569591	3.496435
-24.183874	-36.706579	3.506432
-22.890302	-27.543683	3.516429
-22.622064	-31.720742	3.526426
-22.232056	-26.334698	3.536422
-21.379353	-37.820260	3.546419
-21.139127	-24.490243	3.556416
-20.853853	-37.849171	3.566413
-19.697154	-38.989347	3.576410
-19.444677	-39.739484	3.586406
-19.289610	-20.784962	3.596403
-19.119786	-37.937796	3.606400
-17.933100	-22.787371	3.616397
-17.866747	-32.151649	3.626394
-16.840482	-22.347003	3.636390
-16.333955	-26.590705	3.646387
-16.226463	-27.947343	3.656384
-15.802715	-22.185415	3.666381
-15.060947	-40.107575	3.676378
-14.579836	-34.289745	3.686374
-14.630636	-39.117235	3.696371
-13.440999	-29.668995	3.706368
-13.117077	-40.179805	3.716365
-12.622591	-21.367798	3.726362
-11.806253	-48.342357	3.736358
-11.488510	-31.262943	3.746355
-11.655871	-26.702180	3.756352
-10.650015	-33.878159	3.766349
-10.250730	-39.307371	3.776346
-9.478862	-31.819159	3.786342
-8.578978	-42.756035	3.796339
-8.490732	-29.332258	3.806336
-8.650682	-37.603957	3.816333
-7.676882	-35.830068	3.826330
-7.175109	-25.474322	3.836326
-6.692253	-28.341380	3.846323
-5.561704	-24.562547	3.856320
-5.443155	-27.953835	3.866317
-5.183085	-22.591551	3.876314
-4.912938	-34.735856	3.886310
-3.907002	-31.739446	3.896307
-3.844514	-20.211277	3.906304
-3.369628	-16.423257	3.916301
-3.099622	-6.926539	3.926298
-2.877777	6.158135	3.936294
-2.296004	38.250013	3.946291
-1.649598	53.631444	3.956288
-1.237972	83.892742	3.966285
-0.674266	89.009516	3.976282
-0.646956	124.742596	3.986278
0.000000	156.569798	3.991283
0.167032	170.807135	3.996288
0.173089	182.733578	4.001293
0.541882	186.345588	4.006298
0.679340	191.103830	4.011302
0.620204	201.533317	4.016307
0.897522	185.989411	4.021312
1.428942	212.087651	4.026317
0.957437	231.622063	4.031322
1.038255	208.833212	4.036326
1.172225	209.616268	4.041331
1.006606	218.837576	4.046336
1.314383	237.939680	4.051341
1.149257	228.848952	4.056346
1.271400	217.533715	4.061350
1.134264	212.978996	4.066355
1.214423	220.247517	4.071360
1.301199	230.584056	4.076365
1.086628	233.499753	4.081370
1.219898	201.812956	4.086374
1.179205	219.745850	4.091379
1.330612	235.943876	4.096384
1.489392	226.599763	4.101389
1.401238	228.304489	4.106394
1.646255	223.061883	4.111398
1.629809	232.040143	4.116403
1.524557	244.640317	4.121408
1.316843	233.015768	4.126413
1.343625	216.733625	4.131418
1.287501	223.237070	4.136422
1.322250	243.743657	4.141427
1.096538	236.396366	4.146432
1.245545	214.714896	4.151437
1.496876	229.605212	4.156442
1.634985	235.934217	4.161446
1.502629	228.606225	4.166451
1.071613	239.486751	4.171456
1.181466	242.001402	4.176461
0.763407	230.057670	4.181466
1.432622	233.233250	4.186470
1.832022	269.672589	4.191475
1.661062	261.437684	4.196480
1.628743	249.437886	4.201485
1.489789	254.022927	4.206490
1.689643	256.533953	4.211494
1.392767	272.702223	4.216499
1.477906	271.149884	4.221504
1.694545	257.491121	4.226509
1.686596	271.476621	4.231514
1.550026	271.173000	4.236518
1.347019	275.727892	4.241523
1.598864	264.931182	4.246528
1.521825	274.064295	4.251533
1.670143	274.823971	4.256538
1.572390	262.330493	4.261542
1.418665	266.941458	4.266547
1.403387	270.956008	4.271552
1.783185	291.748833	4.276557
1.872186	287.857612	4.281562
1.943920	290.328654	4.286566
2.052007	306.698853	4.291571
1.868558	278.744779	4.296576
1.699185	279.921063	4.301581
1.776344	305.147909	4.306586
2.154458	280.911985	4.311590
2.081241	275.951108	4.316595
1.868508	277.676427	4.321600
2.185757	274.125606	4.326605
1.537675	272.190544	4.331610
1.547455	268.256487	4.336614
2.098512	294.304370	4.341619
2.115586	312.532055	4.346624
2.425225	291.131614	4.351629
1.804591	281.458743	4.356634
1.744054	262.714831	4.361638
1.943961	290.694247	4.366643
2.177366	311.669521	4.371648
2.261053	295.391307	4.376653
1.876222	274.931530	4.381658
2.214980	294.357179	4.386662
2.143648	295.801170	4.391667
1.857556	287.964971	4.396672
2.102174	268.637729	4.401677
2.136182	284.519610	4.406682
2.308867	289.556166	4.411686
1.975139	298.328737	4.416691
1.962623	303.906799	4.421696
2.271442	285.985407	4.426701
2.319508	302.601978	4.431706
2.017160	322.906710	4.436710
1.959317	302.635337	4.441715
2.046924	298.620738	4.446720
2.201221	290.003176	4.451725
2.005976	315.370448	4.456730
1.973370	311.468736	4.461734
2.087616	304.454693	4.466739
2.034696	308.020709	4.471744
2.411471	297.310265	4.476749
2.288873	302.979813	4.481754
2.456190	315.831635	4.486758
2.346993	304.070007	4.491763
2.349019	291.766288	4.496768
1.983027	300.244600	4.501773
1.893850	307.649362	4.506778
1.978414	316.547549	4.511782
2.188974	338.285729	4.516787
2.272215	332.264557	4.521792
2.490149	330.057540	4.526797
2.246096	332.931566	4.531802
2.401925	335.406771	4.536806
2.744031	343.693611	4.541811
2.603926	356.089812	4.546816
2.701721	345.580118	4.551821
2.112102	339.369853	4.556826
2.535523	337.500483	4.561830
2.680571	333.955614	4.566835
2.499417	339.248152	4.571840
2.869465	349.589257	4.576845
2.694197	344.366147	4.581850
2.955709	325.312158	4.586854
2.625515	329.686152	4.591859
2.592680	303.458536	4.596864
2.705351	291.486830	4.601869
2.177859	318.243713	4.606874
2.735868	328.971910	4.611878
2.672208	313.042084	4.616883
2.758583	304.826777	4.621888
2.695393	298.085718	4.626893
2.408327	315.035871	4.631898
2.677930	329.707819	4.636902
2.784831	332.227905	4.641907
2.527645	340.310338	4.646912
3.084641	338.841699	4.651917
2.747077	342.886346	4.656922
2.584393	330.412125	4.661926
2.740701	331.203333	4.666931
2.457331	343.191615	4.671936
2.734828	348.138856	4.676941
2.618315	349.059987	4.681946
3.002218	342.241079	4.686950
3.043143	340.935655	4.691955
2.499205	358.120274	4.696960
2.663200	348.541725	4.701965
2.693376	351.067686	4.706970
2.511718	336.686575	4.711974
2.842546	331.404990	4.716979
2.901664	348.839647	4.721984
3.174030	331.224708	4.726989
2.883758	337.382860	4.731994
3.014692	360.971645	4.736998
3.469642	362.110363	4.742003
2.703180	341.216378	4.747008
3.086937	334.620245	4.752013
3.184945	350.932968	4.757018
2.819475	354.466005	4.762022
3.105199	349.503891	4.767027
2.940562	336.795797	4.772032
2.977168	342.992070	4.777037
3.023627	368.751072	4.782042
2.779156	347.986560	4.787046
2.870847	350.558683	4.792051
2.992712	351.162826	4.797056
3.018319	339.854870	4.802061
3.087078	346.835408	4.807066
2.963489	361.030095	4.812070
3.112860	354.449603	4.817075
3.150057	341.228821	4.822080
2.872315	343.412061	4.827085
2.993928	344.079084	4.832090
3.563017	367.083489	4.837094
3.268896	365.020276	4.842099
2.871082	367.740376	4.847104
3.210164	360.173815	4.852109
2.926635	370.484931	4.857114
2.883847	378.818330	4.862118
2.890744	388.832576	4.867123
2.977245	370.847104	4.872128
3.260088	365.140373	4.877133
3.148870	371.450757	4.882138
3.023877	371.805473	4.887142
3.324870	357.122032	4.892147
3.321487	381.434926	4.897152
3.728404	386.694125	4.902157
3.380352	379.162188	4.907162
3.371163	368.840621	4.912166
3.351461	370.297591	4.917171
3.356068	395.597640	4.922176
3.457215	382.885045	4.927181
3.147364	370.486211	4.932186
3.016418	363.893836	4.937190
3.450121	395.310177	4.942195
3.368045	418.141613	4.947200
3.778964	401.369434	4.952205
3.709100	396.116064	4.957210
3.444191	386.518008	4.962214
3.307405	382.388354	4.967219
3.377374	398.711089	4.972224
3.819609	412.729948	4.977229
3.620073	409.466825	4.982234
3.315615	388.576627	4.987238
3.572275	397.313839	4.992243
3.502797	409.360936	4.997248
4.070289	389.759510	5.002253
3.626562	387.633614	5.007258
3.436973	395.486203	5.012262
3.871771	401.294117	5.017267
3.885501	391.694304	5.022272
3.798486	367.720172	5.027277
3.914033	377.259123	5.032282
3.492332	384.552947	5.037286
3.720000	394.425160	5.042291
3.671138	375.874306	5.047296
3.732948	384.761200	5.052301
3.640892	371.298362	5.057306
3.789804	363.496876	5.062310
3.641946	383.167302	5.067315
3.476635	390.320802	5.072320
3.593674	389.615598	5.077325
3.801021	398.023089	5.082330
3.963494	404.484470	5.087334
4.095311	416.197825	5.092339
3.549086	424.386961	5.097344
4.124449	413.298744	5.102349
3.752110	412.225857	5.107354
4.014237	407.571362	5.112358
3.888635	408.529413	5.117363
3.803890	404.427357	5.122368
4.103913	396.964697	5.127373
3.859791	411.755357	5.132378
4.325247	425.402826	5.137382
4.234322	394.257957	5.142387
3.499944	384.145991	5.147392
3.681232	387.647475	5.152397
3.790707	415.647589	5.157402
4.056233	405.522978	5.162406
4.146116	429.677397	5.167411
3.991607	427.809412	5.172416
4.171443	418.182528	5.177421
4.101286	399.002928	5.182426
3.981771	409.899474	5.187430
4.126740	406.155726	5.192435
3.784475	420.192958	5.197440
4.117810	411.437426	5.202445
3.714026	410.106443	5.207450
3.906370	428.471130	5.212454
3.907151	416.776868	5.217459
3.742446	413.750268	5.222464
3.901157	415.372393	5.227469
3.639713	426.391842	5.232474
3.824785	437.572393	5.237478
4.485647	441.286933	5.242483
4.198092	441.729184	5.247488
4.408487	450.309328	5.252493
4.091402	460.684056	5.257498
4.216223	443.398590	5.262502
4.407680	435.644096	5.267507
4.188734	448.696194	5.272512
4.307466	455.327002	5.277517
4.360981	451.232864	5.282522
4.258578	454.085181	5.287526
4.467671	450.268381	5.292531
4.301329	437.586923	5.297536
4.270856	438.436526	5.302541
4.233679	447.528529	5.307546
4.513044	439.431204	5.312550
4.366037	463.239601	5.317555
4.217219	458.176923	5.322560
4.320596	434.741016	5.327565
4.418820	457.115764	5.332570
4.656679	447.396803	5.337574
4.478379	452.513216	5.342579
4.046106	471.353870	5.347584
4.443134	445.611253	5.352589
4.349943	438.658359	5.357594
4.216000	437.244309	5.362598
4.160743	453.610584	5.367603
3.657941	464.029223	5.372608
3.968275	457.867683	5.377613
4.212384	460.713937	5.382618
4.572993	479.932600	5.387622
4.862195	486.311615	5.392627
4.660573	486.845022	5.397632
4.694489	465.503023	5.402637
4.743903	467.623634	5.407642
4.708723	495.405024	5.412646
4.470517	491.970410	5.417651
4.300744	487.042388	5.422656
4.377536	469.716590	5.427661
4.437711	479.484446	5.432666
4.433765	493.791772	5.437670
4.562290	490.374881	5.442675
4.461822	500.834980	5.447680
4.707873	497.545653	5.452685
4.628898	498.752294	5.457690
4.517355	519.284807	5.462694
4.964398	514.208776	5.467699
4.460682	506.526905	5.472704
4.709829	525.053674	5.477709
4.785955	530.772739	5.482714
4.729229	520.942404	5.487718
4.730612	510.570459	5.492723
4.743746	504.428912	5.497728
4.805331	516.531381	5.502733
4.778244	533.328424	5.507738
4.552811	513.414743	5.512742
4.817822	512.056687	5.517747
4.734542	519.784737	5.522752
4.874318	514.970197	5.527757
5.116469	517.910699	5.532762
4.852564	520.518926	5.537766
4.874333	525.245684	5.542771
4.329292	521.737866	5.547776
4.801069	527.407232	5.552781
4.777806	549.268007	5.557786
4.686009	555.210946	5.562790
5.303021	549.366157	5.567795
5.185565	566.721825	5.572800
5.270812	564.369294	5.577805
5.222967	548.108306	5.582810
5.105055	544.758764	5.587814
5.227939	548.612743	5.592819
5.162104	541.406291	5.597824
4.946413	514.714002	5.602829
5.136030	519.649582	5.607834
5.311025	540.352489	5.612838
5.273727	546.434688	5.617843
4.737060	512.991417	5.622848
4.927995	525.508546	5.627853
5.224226	556.367386	5.632858
5.350169	546.644858	5.637862
5.253783	541.976766	5.642867
5.201280	561.195731	5.647872
5.279978	539.705062	5.652877
5.208690	552.896013	5.657882
5.279226	556.864397	5.662886
5.267058	559.999544	5.667891
5.271000	542.237145	5.672896
5.501843	538.041271	5.677901
5.279532	552.675951	5.682906
5.311928	547.688160	5.687910
5.300660	550.097297	5.692915
5.172818	544.548533	5.697920
5.400403	554.549402	5.702925
5.383050	533.603768	5.707930
5.015111	548.215355	5.712934
5.359713	557.520057	5.717939
5.106267	561.845622	5.722944
5.279902	549.800803	5.727949
5.163346	550.144164	5.732954
5.340759	550.896382	5.737958
5.581374	555.527500	5.742963
5.279343	544.366463	5.747968
5.205037	536.263904	5.752973
5.102093	552.709588	5.757978
5.148844	571.319973	5.762982
5.743843	572.003085	5.767987
5.465896	564.590872	5.772992
5.788241	576.003651	5.777997
5.330621	587.574826	5.783002
5.206365	578.508408	5.788006
5.508367	566.453014	5.793011
5.641854	583.621824	5.798016
5.566895	587.366255	5.803021
5.852891	587.427940	5.808026
5.575460	584.022673	5.813030
6.047417	584.952718	5.818035
5.663688	580.693154	5.823040
5.678472	573.649356	5.828045
5.646488	586.049085	5.833050
5.844461	587.267182	5.838054
5.893372	580.250689	5.843059
5.547090	586.955244	5.848064
5.568435	592.643728	5.853069
5.522316	603.468402	5.858074
5.252312	596.155681	5.863078
5.767509	579.153388	5.868083
5.626750	593.495058	5.873088
5.429523	588.007364	5.878093
5.752177	585.218731	5.883098
5.651915	580.993413	5.888102
5.711385	576.181866	5.893107
5.495112	593.802590	5.898112
5.662351	598.794079	5.903117
5.889841	600.637177	5.908122
5.824787	618.753812	5.913126
6.404392	599.014176	5.918131
6.093747	598.028941	5.923136
5.447916	594.895662	5.928141
5.800129	600.972999	5.933146
5.728253	619.845333	5.938150
6.247016	621.393182	5.943155
5.773538	625.055208	5.948160
5.910619	629.753670	5.953165
6.307117	628.452696	5.958170
5.799249	646.218148	5.963174
6.259297	626.871132	5.968179
5.926949	610.865833	5.973184
5.988936	617.250884	5.978189
6.205894	626.428748	5.983194
5.961166	626.167064	5.988198
6.258796	636.386562	5.993203
5.911263	624.866305	5.998208
6.025480	601.614207	6.003213
5.824139	613.854907	6.008218
5.933672	633.147908	6.013222
6.219854	641.551681	6.018227
5.872305	628.779262	6.023232
6.095380	605.376188	6.028237
6.273611	620.220567	6.033242
5.975930	638.233709	6.038246
6.059780	616.283753	6.043251
6.052525	622.831872	6.048256
6.201697	625.816764	6.053261
6.009571	641.340009	6.058266
5.719721	640.784802	6.063270
6.374753	626.199155	6.068275
6.262046	615.920473	6.073280
6.047129	624.141677	6.078285
6.103494	625.630888	6.083290
6.151502	641.060489	6.088294
6.432071	619.645454	6.093299
6.113005	614.493070	6.098304
5.983355	614.238413	6.103309
6.144038	633.633449	6.108314
6.044159	627.870107	6.113318
6.177788	611.611714	6.118323
6.056464	611.834131	6.123328
6.128537	624.333990	6.128333
6.222891	633.412456	6.133338
5.884999	629.639935	6.138342
6.261550	623.433548	6.143347
5.783814	625.562178	6.148352
6.011184	624.394116	6.153357
6.152314	624.554320	6.158362
6.041072	611.417519	6.163366
6.376072	604.614960	6.168371
6.225802	626.340475	6.173376
6.066929	635.233403	6.178381
6.194682	611.270944	6.183386
6.012580	621.826694	6.188390
6.140792	606.750727	6.193395
6.038633	605.718410	6.198400
5.906514	613.036700	6.203405
6.559068	614.342648	6.208410
6.138661	612.641498	6.213414
6.033098	590.899758	6.218419
5.860930	588.638298	6.223424
6.027201	586.154389	6.228429
6.128337	598.690067	6.233434
6.034906	608.385431	6.238438
6.151137	599.965563	6.243443
5.852404	603.607290	6.248448
6.098383	619.911435	6.253453
6.000432	617.932175	6.258458
5.931194	624.184329	6.263462
6.576528	633.557366	6.268467
5.937213	617.034666	6.273472
6.158821	627.790748	6.278477
6.071580	619.803630	6.283482
6.005821	604.179463	6.288486
6.195886	594.066015	6.293491
5.778777	607.168258	6.298496
6.272314	627.777706	6.303501
6.542597	620.351815	6.308506
6.017245	594.666966	6.313510
5.938048	588.545773	6.318515
5.906645	593.359273	6.323520
6.104770	594.026685	6.328525
5.817159	614.987657	6.333530
5.852626	617.482502	6.338534
5.875617	626.744902	6.343539
5.938938	618.973017	6.348544
6.260157	613.250283	6.353549
6.192325	614.180156	6.358554
5.891802	635.861655	6.363558
6.068214	628.870830	6.368563
6.201997	622.598712	6.373568
6.333662	618.578228	6.378573
6.248956	610.262784	6.383578
5.996745	618.144974	6.388582
6.314314	615.078886	6.393587
6.224418	625.487011	6.398592
6.186210	607.077946	6.403597
6.000606	580.146673	6.408602
5.947433	586.009156	6.413606
6.231284	604.012179	6.418611
6.105803	607.659310	6.423616
5.926283	580.770930	6.428621
6.179562	589.846290	6.433626
6.111199	612.337975	6.438630
6.278192	590.557606	6.443635
6.185858	601.144673	6.448640
5.952517	589.377298	6.453645
6.220656	569.870687	6.458650
6.055646	567.943159	6.463654
6.163202	581.927316	6.468659
6.297659	589.005129	6.473664
6.281118	589.822942	6.478669
6.324368	581.484594	6.483674
5.934401	588.590769	6.488678
6.161842	567.834783	6.493683
6.084851	586.792068	6.498688
6.122556	591.324932	6.503693
6.366507	584.515431	6.508698
6.201902	600.495470	6.513702
6.335457	597.123992	6.518707
6.391419	584.534709	6.523712
6.167823	585.146823	6.528717
6.471138	593.139625	6.533722
6.181722	600.546543	6.538726
6.168946	575.860194	6.543731
6.129395	585.993817	6.548736
6.021620	573.031874	6.553741
6.277248	567.371688	6.558746
6.051871	567.488679	6.563750
5.724151	569.063651	6.568755
5.857295	587.390666	6.573760
5.851073	580.878306	6.578765
5.914182	572.788040	6.583770
6.023235	591.530506	6.588774
6.232911	594.816928	6.593779
5.919590	595.650146	6.598784
5.942551	609.429502	6.603789
6.400585	595.371069	6.608794
5.831062	590.945400	6.613798
6.157788	574.644088	6.618803
5.766379	595.752205	6.623808
5.932699	596.387091	6.628813
5.909187	601.380803	6.633818
5.450839	603.835123	6.638822
5.953910	598.499729	6.643827
5.977059	601.455525	6.648832
5.864818	582.487447	6.653837
6.038205	583.592708	6.658842
5.815203	620.351387	6.663846
5.952106	622.764559	6.668851
6.098051	619.780694	6.673856
6.235005	639.362556	6.678861
6.137931	643.719324	6.683866
6.113570	623.492007	6.688870
6.540917	624.951776	6.693875
6.190026	608.937310	6.698880
6.125875	601.733807	6.703885
6.275092	585.810149	6.708890
5.899914	589.032026	6.713894
6.272926	579.245071	6.718899
6.117072	600.489273	6.723904
5.874805	602.884702	6.728909
6.209433	598.561863	6.733914
5.967782	598.747737	6.738918
6.189783	588.468217	6.743923
5.891812	576.904588	6.748928
5.794244	586.480466	6.753933
6.074488	609.948285	6.758938
6.151845	611.886434	6.763942
6.085210	586.411583	6.768947
6.066576	586.248969	6.773952
6.030641	589.945124	6.778957
6.266894	594.798936	6.783962
6.173246	583.745489	6.788966
6.232351	577.251142	6.793971
6.002371	598.394340	6.798976
5.859816	613.859254	6.803981
6.009100	588.252238	6.808986
5.769715	602.250341	6.813990
6.214193	599.467419	6.818995
6.036859	628.028395	6.824000
6.110384	626.830020	6.829005
6.351836	617.420217	6.834010
6.044033	604.463877	6.839014
5.904735	608.606933	6.844019
6.020497	602.814574	6.849024
6.416400	615.829134	6.854029
6.186019	612.988254	6.859034
6.038340	600.768411	6.864038
6.151536	605.570153	6.869043
5.986851	594.207237	6.874048
5.830637	585.338264	6.879053
6.084168	607.765500	6.884058
6.221408	626.273992	6.889062
6.365364	604.268938	6.894067
6.081271	602.972514	6.899072
5.783504	621.756401	6.904077
6.050539	613.502788	6.909082
5.973288	606.986172	6.914086
6.034196	598.079143	6.919091
6.052867	624.107745	6.924096
6.090442	632.989121	6.929101
6.319070	615.225218	6.934106
6.129313	609.914244	6.939110
6.283029	607.931869	6.944115
5.906421	607.251411	6.949120
5.648607	588.495210	6.954125
6.248518	607.606618	6.959130
6.001807	633.023763	6.964134
6.251245	613.428640	6.969139
6.182843	624.481736	6.974144
6.123857	632.765369	6.979149
6.144148	612.267688	6.984154
5.962360	593.925871	6.989158
6.014942	591.245989	6.994163
5.888699	613.932308	6.999168
6.029825	630.704718	7.004173
6.018069	622.676122	7.009178
6.204344	629.802509	7.014182
6.155479	621.792475	7.019187
6.239065	623.554591	7.024192
6.089114	633.298968	7.029197
6.352970	624.434048	7.034202
6.263785	601.508947	7.039206
6.129906	605.425200	7.044211
6.358798	601.631134	7.049216
6.287335	615.087537	7.054221
6.284674	597.110713	7.059226
6.311614	611.886959	7.064230
6.157849	603.777566	7.069235
6.273967	592.655316	7.074240
6.062948	592.733533	7.079245
6.409342	599.646406	7.084250
5.884095	608.932311	7.089254
6.172897	579.515297	7.094259
6.044489	579.293877	7.099264
6.313709	596.470656	7.104269
6.435790	597.391043	7.109274
5.963991	590.204896	7.114278
6.328104	580.489155	7.119283
6.180939	603.576965	7.124288
5.933597	586.836320	7.129293
6.050288	598.796274	7.134298
6.214326	601.293447	7.139302
6.182129	578.567904	7.144307
6.026409	587.153582	7.149312
6.112711	584.481151	7.154317
6.146276	571.654677	7.159322
5.720274	588.650387	7.164326
5.950381	595.151969	7.169331
6.319918	592.226455	7.174336
5.857013	589.768587	7.179341
6.012018	593.497410	7.184346
5.924550	598.948376	7.189350
6.109855	598.282292	7.194355
5.871112	596.617218	7.199360
5.967426	608.154184	7.204365
6.153301	590.978124	7.209370
6.098435	597.170183	7.214374
5.969669	586.952969	7.219379
6.065736	605.571129	7.224384
5.919543	614.731856	7.229389
6.205871	598.324239	7.234394
5.801034	585.486942	7.239398
6.128754	593.866560	7.244403
5.989067	589.018175	7.249408
5.947088	608.577873	7.254413
6.169391	590.496899	7.259418
5.670753	613.120261	7.264422
5.800255	607.585668	7.269427
5.815538	591.481609	7.274432
5.887974	589.378703	7.279437
6.007904	612.398811	7.284442
6.053506	626.044717	7.289446
6.029746	622.471053	7.294451
5.930244	645.197883	7.299456
5.928649	627.841257	7.304461
6.348023	629.244140	7.309466
6.148963	633.238648	7.314470
6.248966	627.052115	7.319475
6.076743	613.059245	7.324480
6.262610	631.342578	7.329485
6.219643	608.328837	7.334490
5.718426	592.065284	7.339494
6.126184	602.126181	7.344499
6.337228	625.375607	7.349504
5.970757	615.723952	7.354509
6.308709	598.062354	7.359514
6.301287	580.592507	7.364518
5.750937	598.214681	7.369523
6.020672	610.459408	7.374528
6.128451	598.239182	7.379533
6.158669	588.568158	7.384538
6.046063	600.171407	7.389542
6.086697	592.922281	7.394547
6.277533	598.886401	7.399552
5.812675	616.952598	7.404557
6.293229	596.554571	7.409562
6.010884	578.558190	7.414566
6.156486	594.935914	7.419571
6.069318	600.571502	7.424576
5.840641	615.908990	7.429581
6.176575	604.179223	7.434586
6.112211	594.103579	7.439590
6.125553	605.532521	7.444595
6.256839	616.136508	7.449600
5.957996	592.799283	7.454605
6.267486	580.577008	7.459610
6.326430	585.823937	7.464614
6.281031	597.153475	7.469619
6.051817	615.858746	7.474624
6.096352	605.890973	7.479629
6.242948	584.996503	7.484634
6.178157	610.377824	7.489638
6.277504	611.571777	7.494643
6.141461	585.874498	7.499648
5.962050	597.461855	7.504653
6.115361	598.008330	7.509658
6.170813	582.358632	7.514662
6.258928	595.780358	7.519667
6.119528	612.851551	7.524672
6.199847	602.956589	7.529677
6.243451	579.390947	7.534682
6.115949	593.764855	7.539686
6.269560	600.562500	7.544691
6.214435	610.660338	7.549696
6.395250	599.553041	7.554701
6.520227	586.186240	7.559706
5.998162	582.985849	7.564710
5.766588	589.938690	7.569715
6.121798	573.592916	7.574720
5.809206	572.684062	7.579725
6.073541	596.304732	7.584730
5.841657	616.181513	7.589734
6.115681	610.431656	7.594739
6.291861	588.463523	7.599744
6.233767	595.715018	7.604749
6.153799	599.382049	7.609754
6.192941	595.351115	7.614758
6.079895	591.334183	7.619763
6.151166	572.793820	7.624768
5.862965	575.806587	7.629773
6.089689	580.726978	7.634778
6.092324	592.090303	7.639782
6.175116	593.138423	7.644787
6.449122	596.358379	7.649792
6.315231	576.022559	7.654797
6.148037	562.393413	7.659802
6.059434	572.437471	7.664806
5.809745	568.196404	7.669811
5.920706	561.053950	7.674816
5.452640	562.585033	7.679821
6.110051	594.851674	7.684826
5.995259	610.086875	7.689830
6.165965	587.151700	7.694835
6.461899	603.133667	7.699840
6.162476	600.156126	7.704845
6.105008	581.549031	7.709850
5.756964	566.333398	7.714854
6.139117	592.196325	7.719859
6.146234	599.641643	7.724864
6.084211	605.182123	7.729869
6.071350	590.524776	7.734874
6.140818	589.086271	7.739878
6.018528	605.142977	7.744883
6.231982	613.563687	7.749888
5.963356	605.120701	7.754893
6.295424	584.557625	7.759898
6.094599	574.299945	7.764902
6.048557	571.275604	7.769907
6.245995	583.204249	7.774912
5.885964	587.746610	7.779917
6.063182	566.122623	7.784922
6.036869	582.384322	7.789926
6.147027	593.065968	7.794931
6.187721	586.683469	7.799936
5.684683	577.650249	7.804941
6.014740	579.293696	7.809946
5.903403	609.414030	7.814950
5.641317	600.322826	7.819955
5.779751	595.946192	7.824960
5.989225	597.941326	7.829965
6.480533	583.605624	7.834970
6.061173	600.436491	7.839974
6.009198	600.971906	7.844979
6.166069	595.804015	7.849984
5.939144	598.268034	7.854989
6.182260	603.899847	7.859994
5.847220	602.194062	7.864998
6.143423	595.094771	7.870003
6.380217	605.196648	7.875008
6.011849	614.386790	7.880013
6.139988	583.772173	7.885018
6.131369	601.330081	7.890022
6.296377	611.936484	7.895027
6.408832	605.085863	7.900032
6.499240	597.150688	7.905037
6.469073	571.029797	7.910042
6.161152	579.330667	7.915046
5.878038	581.023159	7.920051
5.826377	577.888765	7.925056
5.925014	581.754750	7.930061
6.064203	604.974387	7.935066
6.161482	603.554271	7.940070
6.207246	595.876551	7.945075
6.210999	570.416926	7.950080
5.502621	585.087077	7.955085
6.180565	581.772823	7.960090
6.162065	594.501102	7.965094
6.157142	578.353932	7.970099
6.314758	583.235532	7.975104
5.858121	599.064952	7.980109
6.159972	588.516932	7.985114
6.136232	582.039922	7.990118
6.006130	596.517892	7.995136
5.976239	605.522828	8.000154
5.925930	603.735222	8.005171
5.953612	595.267586	8.010189
5.830490	599.321887	8.015206
5.686911	611.435997	8.020224
6.062189	618.779645	8.025242
5.960163	616.989858	8.030259
6.213263	592.209368	8.035277
6.091523	607.547902	8.040294
6.250532	594.408576	8.045312
6.313239	594.987851	8.050330
6.525639	595.561084	8.055347
6.257306	599.519435	8.060365
6.185849	590.594399	8.065382
5.836559	604.135415	8.070400
6.276280	605.577623	8.075418
5.825008	620.100791	8.080435
6.158031	602.913930	8.085453
6.116600	601.370949	8.090470
5.942264	595.423802	8.095488
6.244353	601.853415	8.100506
6.084155	612.390397	8.105523
6.345761	595.426705	8.110541
5.707449	579.582735	8.115558
5.654860	596.857911	8.120576
5.825496	608.467855	8.125594
6.023893	625.795755	8.130611
6.205271	611.893182	8.135629
6.094578	620.049515	8.140646
5.975614	649.021662	8.145664
6.437916	633.450946	8.150682
6.227669	626.806666	8.155699
6.413848	628.246003	8.160717
6.511945	638.912613	8.165734
6.298142	638.610772	8.170752
6.499439	635.301479	8.175770
6.232624	631.545968	8.180787
6.031280	625.747129	8.185805
6.528105	636.866698	8.190822
6.083395	629.661131	8.195840
6.533423	618.673576	8.200858
6.266616	635.610972	8.205875
6.305771	647.028856	8.210893
6.514788	646.674657	8.215910
6.466116	629.027169	8.220928
6.279518	598.655638	8.225946
5.979673	623.284732	8.230963
6.288748	620.404358	8.235981
6.643011	628.055631	8.240998
6.119370	640.737549	8.246016
6.410783	633.082372	8.251034
6.386413	640.091987	8.256051
6.226611	625.183084	8.261069
6.209518	640.916451	8.266086
6.518723	627.964421	8.271104
6.987377	632.396594	8.276122
6.156513	615.557919	8.281139
6.361869	606.416308	8.286157
6.321031	619.902530	8.291174
6.087250	625.343644	8.296192
6.243403	632.459508	8.301210
6.199763	651.782701	8.306227
6.321501	623.762560	8.311245
6.239829	621.713771	8.316262
6.212025	643.164554	8.321280
6.484883	637.502445	8.326298
6.428615	620.216065	8.331315
6.102206	623.297060	8.336333
6.387133	642.032233	8.341350
6.236478	638.747449	8.346368
6.602266	618.741955	8.351386
6.592616	612.368680	8.356403
6.417463	639.830733	8.361421
6.599079	632.894099	8.366438
6.681231	633.635569	8.371456
7.065827	639.924631	8.376474
6.702060	636.217513	8.381491
6.176278	621.882534	8.386509
6.692343	632.520903	8.391526
6.438826	644.294053	8.396544
6.701817	623.001569	8.401562
6.894330	627.905143	8.406579
6.749671	629.231974	8.411597
6.686077	629.098073	8.416614
6.530298	621.153222	8.421632
6.428563	593.757697	8.426650
6.634886	586.974043	8.431667
6.382305	607.201347	8.436685
6.513280	609.463950	8.441702
6.368481	613.551358	8.446720
6.397686	618.384108	8.451738
6.402722	622.887481	8.456755
6.532279	639.401310	8.461773
6.748060	631.666532	8.466790
6.560226	634.064674	8.471808
6.813806	632.447749	8.476826
6.350978	643.455217	8.481843
6.728372	633.260443	8.486861
6.868249	629.360581	8.491878
6.623617	644.233769	8.496896
6.635166	637.275349	8.501914
6.479932	621.497332	8.506931
6.516783	623.983603	8.511949
6.741783	638.275674	8.516966
6.396866	628.625250	8.521984
6.493301	621.104929	8.527002
6.538455	635.537711	8.532019
6.493342	650.405091	8.537037
6.656333	623.906354	8.542054
6.350418	642.761209	8.547072
6.696736	642.382254	8.552090
6.727231	643.350312	8.557107
6.678691	626.140283	8.562125
6.703139	641.685241	8.567143
6.531040	638.400163	8.572160
6.692130	627.841249	8.577178
6.608414	649.594310	8.582195
6.285577	645.351832	8.587213
6.768038	625.996647	8.592231
6.649081	629.791482	8.597248
6.816072	629.724860	8.602266
6.457931	630.872561	8.607283
6.631848	636.237745	8.612301
6.581470	632.642377	8.617319
6.562496	648.678538	8.622336
6.639807	661.214030	8.627354
6.811999	666.646519	8.632371
6.818976	675.852040	8.637389
7.171087	673.705583	8.642407
6.645488	657.817519	8.647424
6.555099	630.431272	8.652442
6.828665	645.676575	8.657459
6.716361	665.830888	8.662477
6.963450	683.286299	8.667495
7.040395	675.035810	8.672512
6.536137	635.094432	8.677530
6.722585	656.832673	8.682547
6.727154	663.316694	8.687565
7.013014	663.119828	8.692583
6.680978	679.185715	8.697600
6.896271	668.049270	8.702618
6.866639	655.954566	8.707635
7.268376	670.993922	8.712653
7.098671	649.109899	8.717671
7.086623	624.070403	8.722688
6.688389	619.072198	8.727706
6.666470	623.004496	8.732723
6.579344	633.997495	8.737741
6.741317	653.956213	8.742759
6.892057	660.991708	8.747776
6.933906	658.772838	8.752794
7.079222	669.885675	8.757811
6.989490	667.305975	8.762829
6.822968	671.497255	8.767847
7.014902	666.447459	8.772864
7.092537	665.433760	8.777882
7.138292	656.977567	8.782899
6.957687	650.334282	8.787917
6.908473	641.151673	8.792935
6.857224	649.706846	8.797952
6.769259	629.480341	8.802970
7.116080	656.690168	8.807987
6.670185	666.248695	8.813005
6.612533	655.199086	8.818023
6.762591	674.416795	8.823040
6.711333	677.251697	8.828058
7.201907	661.852807	8.833075
6.914266	663.209961	8.838093
7.010140	659.407692	8.843111
6.700472	676.939556	8.848128
6.805327	670.358901	8.853146
6.927336	668.049147	8.858163
7.153404	664.477065	8.863181
7.041601	656.158001	8.868199
7.064932	658.743041	8.873216
6.827623	679.721254	8.878234
7.167596	679.401599	8.883251
6.816280	674.666021	8.888269
6.867688	658.282517	8.893287
6.904858	669.523825	8.898304
6.972938	675.659161	8.903322
7.054761	673.715299	8.908339
6.800612	675.294318	8.913357
7.240445	687.401421	8.918375
7.036945	695.379384	8.923392
6.844516	724.488289	8.928410
7.475332	703.971690	8.933427
7.289430	693.567290	8.938445
7.188437	670.461876	8.943463
7.039680	676.724163	8.948480
6.722968	715.758762	8.953498
7.119980	711.517649	8.958515
7.251817	691.769265	8.963533
7.356976	700.018281	8.968551
7.272998	715.478504	8.973568
7.382094	713.302337	8.978586
7.340055	681.463149	8.983603
6.846091	673.069472	8.988621
7.183241	696.457506	8.993639
7.064104	714.540445	8.998656
7.167848	702.953343	9.003674
7.133594	699.455858	9.008691
7.009922	715.810588	9.013709
7.305503	727.006283	9.018727
7.301330	705.962897	9.023744
7.365651	711.104748	9.028762
7.397068	718.639386	9.033779
7.257792	719.773262	9.038797
7.466672	703.383858	9.043815
6.985898	706.219291	9.048832
7.101608	697.845781	9.053850
7.371445	692.304198	9.058867
6.999209	712.257203	9.063885
7.274536	699.670259	9.068903
7.262066	704.896531	9.073920
7.314659	720.163764	9.078938
7.675485	706.405715	9.083955
7.605209	709.704861	9.088973
7.331703	694.106015	9.093991
7.154549	683.825142	9.099008
7.351757	674.926898	9.104026
7.457652	692.253627	9.109043
6.943649	701.161210	9.114061
7.329298	708.084304	9.119079
7.284100	704.605059	9.124096
6.971573	703.213631	9.129114
7.172300	716.695932	9.134131
7.081029	717.721902	9.139149
7.229363	707.699345	9.144167
7.054756	705.982647	9.149184
7.162400	700.273035	9.154202
7.400484	712.898898	9.159219
7.328673	709.923915	9.164237
7.283904	691.460282	9.169255
7.069748	688.825078	9.174272
7.251385	723.267547	9.179290
7.325367	727.788585	9.184307
7.439801	722.940306	9.189325
7.653362	728.126183	9.194343
7.750520	745.633109	9.199360
7.332795	729.707660	9.204378
7.373404	705.476728	9.209395
7.419799	712.296876	9.214413
7.617723	721.425410	9.219431
7.653178	703.729199	9.224448
7.201365	701.546541	9.229466
7.358514	722.445556	9.234483
6.966406	744.476031	9.239501
7.317979	734.225829	9.244519
7.481727	729.198579	9.249536
7.375303	731.522964	9.254554
7.542849	739.534981	9.259571
7.051988	752.558626	9.264589
7.138223	744.247722	9.269607
7.353305	733.749971	9.274624
7.153809	737.890631	9.279642
7.471060	757.982344	9.284659
7.737431	768.524018	9.289677
7.486609	748.814984	9.294695
7.266981	745.232897	9.299712
7.675089	771.007199	9.304730
7.662162	785.844398	9.309747
7.479450	779.843754	9.314765
7.418399	765.342791	9.319783
8.092034	768.507601	9.324800
7.699068	767.626571	9.329818
7.892653	760.713878	9.334835
7.813685	747.241307	9.339853
7.188097	738.548861	9.344871
7.637876	745.781269	9.349888
7.579494	770.877449	9.354906
7.698785	748.794779	9.359923
7.333925	752.793622	9.364941
7.630296	775.855141	9.369959
7.677652	785.678496	9.374976
7.891148	781.407273	9.379994
7.834251	769.532775	9.385011
7.867731	766.932795	9.390029
7.865980	738.078651	9.395047
7.785632	738.163798	9.400064
7.527047	734.038890	9.405082
7.843880	727.689546	9.410099
7.414956	745.934611	9.415117
7.429767	751.552643	9.420135
7.888457	750.381111	9.425152
7.702472	769.089564	9.430170
7.772257	777.420825	9.435187
7.831735	772.382551	9.440205
7.876047	765.475829	9.445223
7.959086	761.689137	9.450240
7.707412	761.427204	9.455258
7.668265	756.424225	9.460275
7.907510	759.329017	9.465293
8.016632	747.876192	9.470311
7.948937	749.813278	9.475328
7.623284	757.478872	9.480346
7.856241	739.967147	9.485363
7.933224	726.562597	9.490381
7.617293	729.052966	9.495399
7.879336	741.691818	9.500416
7.698801	758.512758	9.505434
7.861837	753.290690	9.510451
8.172803	759.654059	9.515469
7.834758	759.336930	9.520487
7.756080	760.713089	9.525504
7.618122	759.213005	9.530522
7.814502	770.999775	9.535539
7.796979	758.716425	9.540557
7.778276	783.896695	9.545575
7.860244	784.281014	9.550592
7.914880	768.103399	9.555610
8.034416	753.933038	9.560627
8.191057	782.928576	9.565645
7.726361	778.921356	9.570663
7.683842	771.700131	9.575680
7.683448	766.592542	9.580698
7.619267	764.161023	9.585715
7.970373	789.022679	9.590733
7.659066	795.018549	9.595751
7.711556	784.003092	9.600768
7.619265	766.507300	9.605786
7.789416	764.201580	9.610803
7.924350	795.187796	9.615821
7.863137	779.976404	9.620839
8.199171	786.583804	9.625856
8.257870	792.281090	9.630874
8.117182	795.871541	9.635891
8.124064	806.497942	9.640909
8.051299	789.039636	9.645927
7.714729	767.693611	9.650944
7.798282	780.329422	9.655962
8.116183	812.818297	9.660979
8.431231	819.050342	9.665997
8.354852	802.926123	9.671015
8.300438	774.229098	9.676032
7.871726	787.053182	9.681050
7.769837	793.656104	9.686067
8.236531	787.046600	9.691085
7.687404	798.520779	9.696103
8.207051	801.190119	9.701120
8.396311	799.876740	9.706138
8.166019	799.070669	9.711155
8.122565	787.214402	9.716173
7.842244	777.798616	9.721191
8.504642	793.531730	9.726208
8.110800	792.064975	9.731226
7.823337	784.868477	9.736243
8.273378	791.069740	9.741261
8.023593	798.139507	9.746279
8.034626	817.128271	9.751296
8.384152	803.611014	9.756314
8.065841	802.061224	9.761331
8.329620	800.922390	9.766349
8.185959	797.550120	9.771367
8.449337	795.426279	9.776384
8.435103	812.242034	9.781402
8.183927	816.322868	9.786419
8.272514	789.158860	9.791437
8.377584	798.818790	9.796455
8.127377	791.872855	9.801472
8.257488	794.172232	9.806490
8.191533	793.472728	9.811507
8.213133	799.635376	9.816525
8.105933	799.312669	9.821543
8.104324	794.453434	9.826560
8.148700	811.659397	9.831578
8.044529	815.984272	9.836595
8.319236	797.969453	9.841613
8.439267	791.968072	9.846631
8.494523	806.705761	9.851648
8.779019	818.773105	9.856666
7.985679	815.144804	9.861683
8.400209	796.471123	9.866701
8.220903	799.960800	9.871719
8.210253	806.569609	9.876736
8.310662	799.718544	9.881754
8.106579	799.021103	9.886771
8.400340	800.237025	9.891789
8.328051	798.940596	9.896807
8.387117	796.437045	9.901824
7.873489	799.675556	9.906842
8.220708	821.188597	9.911859
8.368907	809.142514	9.916877
8.025599	819.983053	9.921895
8.449525	823.705540	9.926912
8.624147	838.837105	9.931930
8.340677	846.613556	9.936947
8.751274	834.854909	9.941965
8.293467	840.157379	9.946983
8.577584	824.767352	9.952000
8.668622	814.276564	9.957018
8.249392	831.846390	9.962035
8.705961	811.911447	9.967053
8.589915	819.258354	9.972071
8.298602	815.027248	9.977088
8.423926	815.341133	9.982106
8.583938	847.193848	9.987123
8.831830	846.553963	9.992141
8.391615	831.571938	9.997159
8.560989	825.348077	10.002176
8.545938	816.008674	10.007194
8.452372	831.341794	10.012211
8.786053	836.100189	10.017229
8.633124	838.805504	10.022247
8.669950	801.194507	10.027264
8.404789	801.297600	10.032282
8.586148	833.617107	10.037299
8.550729	825.194014	10.042317
8.473035	844.192259	10.047335
8.689902	859.660573	10.052352
8.636243	843.197901	10.057370
8.658513	837.197701	10.062387
8.778392	840.984312	10.067405
8.534022	835.706246	10.072423
8.619530	846.336410	10.077440
8.842123	830.194441	10.082458
8.531911	831.025655	10.087475
8.637714	844.034908	10.092493
8.549957	827.950230	10.097511
8.492861	831.347592	10.102528
8.700038	850.667963	10.107546
8.205041	841.283973	10.112563
8.564680	838.884642	10.117581
8.737574	844.528932	10.122599
8.329270	832.801605	10.127616
8.415846	846.592179	10.132634
8.538231	848.492159	10.137651
8.641885	829.716111	10.142669
8.264759	840.510692	10.147687
8.511103	879.167892	10.152704
8.914899	873.573209	10.157722
8.687555	865.115981	10.162739
8.888201	864.707368	10.167757
8.720555	861.679706	10.172775
8.555576	869.902116	10.177792
8.858416	876.156275	10.182810
8.705283	868.020947	10.187827
8.978580	875.716130	10.192845
8.826734	891.115914	10.197863
8.810218	869.023238	10.202880
9.006140	862.394586	10.207898
8.980052	872.644396	10.212915
9.291337	864.192523	10.217933
8.978188	877.436447	10.222951
8.919437	890.986087	10.227968
8.957280	863.938670	10.232986
8.694253	855.711695	10.238003
9.097376	867.383981	10.243021
8.734427	893.646840	10.248039
8.535848	885.564571	10.253056
8.765181	859.212200	10.258074
9.076541	868.802660	10.263091
9.215886	879.092244	10.268109
9.206656	875.266652	10.273127
9.047844	861.082659	10.278144
9.098585	856.222528	10.283162
9.168338	863.329358	10.288179
9.321040	887.782344	10.293197
9.078025	878.858529	10.298215
8.972630	877.073893	10.303232
9.303192	864.261995	10.308250
9.189102	869.280174	10.313267
9.017055	862.726304	10.318285
9.179151	846.189303	10.323303
9.018225	834.889869	10.328320
9.081616	836.664002	10.333338
8.866962	863.768513	10.338355
8.808471	850.485330	10.343373
8.591486	847.356306	10.348391
8.860087	863.439337	10.353408
9.274472	874.613835	10.358426
9.094496	889.948303	10.363443
9.103168	871.103179	10.368461
9.128215	852.611971	10.373479
9.083389	877.873759	10.378496
9.104165	889.745924	10.383514
9.065303	885.265949	10.388531
8.913063	867.495082	10.393549
9.093641	873.603543	10.398567
9.496347	884.634248	10.403584
9.486838	875.498663	10.408602
9.442097	870.687269	10.413619
9.360216	868.633857	10.418637
9.527986	862.931074	10.423655
9.407401	864.729512	10.428672
9.398107	863.868516	10.433690
9.002429	861.677443	10.438707
9.121144	856.716239	10.443725
9.200237	857.634263	10.448743
9.052051	870.992320	10.453760
9.223892	869.313013	10.458778
9.204104	872.565770	10.463795
9.193571	878.996979	10.468813
9.314491	863.049684	10.473831
8.962719	875.562977	10.478848
9.321775	881.375972	10.483866
9.083389	868.942663	10.488883
9.220684	866.090336	10.493901
9.296248	880.957186	10.498919
9.301522	886.691773	10.503936
9.417223	864.317381	10.508954
9.387370	879.316285	10.513971
9.302453	869.439621	10.518989
9.483364	850.833312	10.524007
9.047244	873.604125	10.529024
9.365533	880.024193	10.534042
8.901830	888.524265	10.539059
9.168407	857.981589	10.544077
9.474892	866.997709	10.549095
8.959808	888.681782	10.554112
9.417820	907.657014	10.559130
9.279368	906.902081	10.564147
9.381360	898.609743	10.569165
9.665548	907.961080	10.574183
9.530386	922.290697	10.579200
9.581146	907.208077	10.584218
9.603384	896.158081	10.589235
9.507546	914.614670	10.594253
9.410687	924.107018	10.599271
9.433139	913.688602	10.604288
9.350097	900.333371	10.609306
9.374028	908.062792	10.614323
9.385319	907.865542	10.619341
9.558652	904.564847	10.624359
9.581484	924.789763	10.629376
9.555988	924.903927	10.634394
9.453597	908.374650	10.639411
9.596211	897.464561	10.644429
9.741284	915.957503	10.649447
9.484139	920.158512	10.654464
9.554286	896.726324	10.659482
9.639752	916.021331	10.664499
9.334672	922.452427	10.669517
9.490946	915.692250	10.674535
9.244719	916.730949	10.679552
9.657413	889.375641	10.684570
9.500811	912.298005	10.689587
9.392141	913.883018	10.694605
9.507023	915.366637	10.699623
9.573314	909.880753	10.704640
9.430350	912.457695	10.709658
9.488890	930.501982	10.714675
9.641561	948.632579	10.719693
9.984514	946.035056	10.724711
9.807518	940.926778	10.729728
9.939627	931.599886	10.734746
9.852962	923.414578	10.739763
9.662280	920.886253	10.744781
9.962689	919.040554	10.749799
9.723272	910.715577	10.754816
9.698518	898.874338	10.759834
10.006718	896.056443	10.764851
10.115827	915.524171	10.769869
9.969331	891.917805	10.774887
9.668303	884.245378	10.779904
9.618039	886.847144	10.784922
9.795360	897.572378	10.789939
9.934443	905.391501	10.794957
9.980241	892.093213	10.799975
9.823105	898.304527	10.804992
9.930069	897.131971	10.810010
9.964162	899.976032	10.815027
10.023678	878.315840	10.820045
10.132644	876.021592	10.825063
10.119609	898.029300	10.830080
9.770721	892.473583	10.835098
9.976060	891.646783	10.840115
9.627320	902.112783	10.845133
10.353613	890.807994	10.850151
9.680215	875.540824	10.855168
10.037829	884.178718	10.860186
9.951278	906.720499	10.865203
10.205860	896.267081	10.870221
10.124739	881.911806	10.875239
10.105880	892.037927	10.880256
10.018089	887.153250	10.885274
10.286396	897.633193	10.890291
10.122949	890.471944	10.895309
10.043179	874.069936	10.900327
9.741933	897.308132	10.905344
9.905377	885.418386	10.910362
9.872916	890.671345	10.915379
9.826497	901.144654	10.920397
10.024023	885.078700	10.925415
10.049430	902.038161	10.930432
10.022383	912.784878	10.935450
10.041987	883.110804	10.940467
9.760911	875.151791	10.945485
10.310723	893.924483	10.950503
9.841952	900.223901	10.955520
10.369552	893.084343	10.960538
9.948626	909.713738	10.965555
9.783997	904.342866	10.970573
10.117929	894.389786	10.975591
10.133410	927.025902	10.980608
10.227000	938.791117	10.985626
9.876929	928.019693	10.990643
10.078522	917.897375	10.995661
10.310679	909.565612	11.000679
10.197586	921.355621	11.005696
10.052884	933.573686	11.010714
10.056636	914.538130	11.015731
10.140326	917.093559	11.020749
10.281165	921.933442	11.025767
9.890066	912.802051	11.030784
10.106966	921.853376	11.035802
10.180064	931.537369	11.040819
10.015441	927.431420	11.045837
10.342927	911.637292	11.050855
10.117663	928.375970	11.055872
10.254754	938.258001	11.060890
10.476922	930.727279	11.065907
10.044510	924.940632	11.070925
10.313558	911.681596	11.075943
10.296632	930.028928	11.080960
10.511963	933.812679	11.085978
10.315388	924.284957	11.090995
9.941560	917.653019	11.096013
10.261121	937.438957	11.101031
10.250929	969.474738	11.106048
10.148179	970.689581	11.111066
10.608645	942.946162	11.116083
10.629671	948.388087	11.121101
10.864866	950.744611	11.126119
10.587753	950.795265	11.131136
10.775238	954.723252	11.136154
10.823730	926.830478	11.141171
10.193571	931.100118	11.146189
10.388335	911.256035	11.151207
10.510912	906.177180	11.156224
10.277740	912.917763	11.161242
10.485726	936.749448	11.166259
10.424649	936.303888	11.171277
11.043760	932.267683	11.176295
10.856382	927.916049	11.181312
10.562928	939.983747	11.186330
10.528788	922.613959	11.191347
10.182713	937.641266	11.196365
10.811401	915.589303	11.201383
10.558830	925.919183	11.206400
10.548080	925.352246	11.211418
10.597123	916.056507	11.216435
10.757854	921.338461	11.221453
10.752064	924.087470	11.226471
10.605032	922.634233	11.231488
10.617331	918.999609	11.236506
10.648737	909.987425	11.241523
10.435658	923.234138	11.246541
10.903242	914.969936	11.251559
10.747566	920.561591	11.256576
10.480336	931.439524	11.261594
10.204399	907.410643	11.266611
10.396427	918.151960	11.271629
10.611345	942.949485	11.276647
11.049474	968.165954	11.281664
11.054349	951.569016	11.286682
11.118676	927.080335	11.291699
10.489952	938.410824	11.296717
10.602392	918.748599	11.301735
10.914741	948.826703	11.306752
10.816940	949.551876	11.311770
11.138377	933.049359	11.316787
10.924221	927.858765	11.321805
10.888152	918.190280	11.326823
10.301720	927.242899	11.331840
10.402779	931.194805	11.336858
10.845808	939.110333	11.341875
10.671470	964.058810	11.346893
10.992842	966.767834	11.351911
11.033634	952.134735	11.356928
10.940953	960.072972	11.361946
11.367826	954.563794	11.366963
10.886476	942.328015	11.371981
10.935502	940.067181	11.376999
10.877567	950.786656	11.382016
10.935846	973.687673	11.387034
11.335123	940.863732	11.392051
10.602254	914.718587	11.397069
11.215932	941.851663	11.402087
10.980179	940.396061	11.407104
10.549647	935.261295	11.412122
10.988524	933.223857	11.417139
10.965593	957.165664	11.422157
10.903577	940.940035	11.427175
10.829309	940.728977	11.432192
11.094788	953.584606	11.437210
11.239928	957.644855	11.442227
11.125004	947.997058	11.447245
10.968657	931.668848	11.452263
11.318655	955.035376	11.457280
10.759604	952.541352	11.462298
11.070019	951.146734	11.467315
11.081432	945.350204	11.472333
10.786309	946.249287	11.477351
11.224302	953.196610	11.482368
10.922628	951.595445	11.487386
10.973874	943.103649	11.492403
10.923351	959.476858	11.497421
10.934032	953.515724	11.502439
11.003725	960.077374	11.507456
11.156701	955.448481	11.512474
11.401704	949.954992	11.517491
11.312616	951.173973	11.522509
11.348325	946.155314	11.527527
11.315418	965.461483	11.532544
11.180418	974.128487	11.537562
11.263594	960.261704	11.542579
11.260317	963.342799	11.547597
10.886491	956.068389	11.552615
11.244273	942.475452	11.557632
10.970874	949.639029	11.562650
10.989871	966.119035	11.567667
11.284018	989.054602	11.572685
11.427573	992.648507	11.577703
11.408208	969.775153	11.582720
11.138761	990.064494	11.587738
11.626590	988.399081	11.592755
11.105312	983.781628	11.597773
11.098316	981.667412	11.602791
11.352320	994.708685	11.607808
11.199166	993.610595	11.612826
11.272678	982.919391	11.617843
11.714963	981.454271	11.622861
11.539851	976.674031	11.627879
11.484875	974.628360	11.632896
11.611594	984.617816	11.637914
11.512931	994.291759	11.642931
11.623154	992.961413	11.647949
11.771327	969.810140	11.652967
11.691956	986.886493	11.657984
11.193554	961.623646	11.663002
11.370537	981.782720	11.668019
11.475537	1004.931191	11.673037
11.379133	985.060762	11.678055
11.583882	1001.696160	11.683072
11.532172	982.278470	11.688090
11.553306	971.628205	11.693107
11.774756	987.168412	11.698125
11.750484	994.983284	11.703143
11.739840	987.248353	11.708160
11.461724	978.940361	11.713178
11.510212	977.176040	11.718195
11.609079	996.874541	11.723213
11.501380	992.525367	11.728231
11.546181	967.040594	11.733248
11.616097	972.629231	11.738266
11.578292	973.553787	11.743283
11.951074	1002.538895	11.748301
11.642688	989.763822	11.753319
11.722570	962.412409	11.758336
11.497954	974.980046	11.763354
11.505561	989.921896	11.768371
11.969085	985.584010	11.773389
11.530132	978.552479	11.778407
11.657952	970.309561	11.783424
11.427984	986.846474	11.788442
11.664443	996.846832	11.793459
11.656722	978.629914	11.798477
11.610772	977.243509	11.803495
11.892017	987.555965	11.808512
11.383009	992.695731	11.813530
11.552780	972.815748	11.818547
11.974488	985.963518	11.823565
11.619724	979.747981	11.828583
11.757817	996.077957	11.833600
11.839702	1018.572462	11.838618
11.953031	1011.580423	11.843635
11.982943	1010.566224	11.848653
11.847610	1022.602640	11.853671
11.923638	1029.123519	11.858688
11.914461	1029.995328	11.863706
11.936553	1005.789614	11.868723
12.245174	1013.168871	11.873741
11.552341	1004.720888	11.878759
11.808378	1009.585649	11.883776
12.090725	1010.585025	11.888794
12.482344	1017.719229	11.893811
12.106305	1004.555399	11.898829
11.613345	989.520558	11.903847
11.951291	1005.984577	11.908864
12.390949	1016.466396	11.913882
11.864895	1009.523437	11.918899
12.177868	1025.281768	11.923917
11.845852	1021.232090	11.928935
12.168295	1011.172494	11.933952
11.851473	1009.267309	11.938970
11.642344	1025.765101	11.943987
12.061671	1035.514847	11.949005
12.087770	1024.349090	11.954023
12.241057	1010.332324	11.959040
12.066871	1014.023219	11.964058
11.983362	1010.930259	11.969075
12.432176	1020.281225	11.974093
11.820476	1018.234658	11.979111
12.025982	1012.378771	11.984128
11.936327	1020.191767	11.989146
12.148243	1017.048706	11.994163
12.443774	1009.540164	11.999181
11.889115	1008.350097	12.004199
11.955827	1014.013866	12.009216
11.954535	1017.592354	12.014234
11.843036	1024.097578	12.019251
11.767556	1041.012856	12.024269
12.072588	1044.274359	12.029287
12.480605	1032.616849	12.034304
12.466196	1035.362874	12.039322
12.455756	1057.581648	12.044339
12.486234	1054.753925	12.049357
12.273776	1044.757019	12.054375
12.428448	1030.871075	12.059392
12.562170	1051.594929	12.064410
12.229825	1040.717372	12.069427
12.721111	1035.411542	12.074445
12.644801	1061.228796	12.079463
12.699121	1045.214286	12.084480
12.469760	1019.098424	12.089498
12.172971	1026.657733	12.094515
12.557495	1055.691898	12.099533
12.508126	1043.239117	12.104551
12.627839	1023.708397	12.109568
12.645097	1023.709421	12.114586
12.505894	1018.991031	12.119603
12.562714	1020.531193	12.124621
12.616068	1034.010576	12.129639
12.318936	1017.879512	12.134656
12.338837	1007.505537	12.139674
12.429258	1026.303927	12.144691
12.713840	1033.156099	12.149709
12.674757	1042.706573	12.154727
12.567150	1011.459279	12.159744
12.083480	1021.528472	12.164762
12.220912	1049.054633	12.169779
12.636561	1056.096422	12.174797
12.321171	1049.152974	12.179815
12.421019	1029.457067	12.184832
12.462230	1039.037862	12.189850
12.331470	1061.666291	12.194867
12.362501	1043.027838	12.199885
12.343065	1041.605557	12.204903
12.711630	1039.711582	12.209920
12.705317	1073.514904	12.214938
12.886501	1092.409274	12.219955
13.180443	1072.656539	12.224973
12.662099	1060.717848	12.229991
12.907191	1042.988275	12.235008
12.822679	1052.882204	12.240026
12.789287	1060.181619	12.245043
12.922747	1054.862786	12.250061
12.977019	1038.281896	12.255079
12.948238	1043.054695	12.260096
12.999889	1059.434349	12.265114
12.813832	1050.529261	12.270131
13.096948	1028.703985	12.275149
13.117190	1052.216373	12.280167
12.821542	1046.578099	12.285184
12.892995	1039.643643	12.290202
12.864178	1062.946492	12.295219
12.928417	1054.518907	12.300237
12.661537	1047.978660	12.305255
12.711455	1059.339476	12.310272
12.885839	1046.486913	12.315290
12.780812	1052.422718	12.320307
13.152842	1043.050600	12.325325
13.072189	1034.355901	12.330343
13.119627	1047.561539	12.335360
13.153959	1058.008425	12.340378
12.674452	1060.493701	12.345395
13.034897	1035.225976	12.350413
13.134423	1046.600331	12.355431
13.168567	1041.403302	12.360448
13.150235	1040.538377	12.365466
12.720625	1069.676996	12.370483
13.337891	1049.654673	12.375501
12.856642	1044.903354	12.380519
12.900648	1049.930104	12.385536
12.848032	1057.368290	12.390554
12.606906	1060.863224	12.395571
13.126704	1069.381631	12.400589
12.766856	1082.333325	12.405607
12.828012	1085.903871	12.410624
12.972582	1068.210954	12.415642
13.148313	1081.351337	12.420659
13.479138	1091.088979	12.425677
12.805223	1092.195217	12.430695
12.605006	1097.736044	12.435712
13.779569	1088.003480	12.440730
13.171280	1091.610066	12.445747
13.050356	1073.213760	12.450765
13.154609	1080.610783	12.455783
13.026634	1070.667304	12.460800
13.570634	1091.893842	12.465818
13.157684	1096.743131	12.470835
13.384299	1088.214599	12.475853
13.263904	1110.746627	12.480871
13.484491	1112.306770	12.485888
13.603546	1100.462963	12.490906
13.135688	1098.675616	12.495923
13.495103	1095.357414	12.500941
13.425047	1099.275451	12.505959
13.305493	1099.189366	12.510976
13.599313	1098.736913	12.515994
13.567751	1092.432594	12.521011
13.577627	1095.335995	12.526029
13.768250	1094.195946	12.531047
13.486183	1070.845410	12.536064
13.715786	1054.285319	12.541082
13.530898	1064.950085	12.546099
13.470628	1083.985895	12.551117
13.311684	1074.455600	12.556135
13.163099	1064.202615	12.561152
13.707417	1069.974638	12.566170
13.496609	1092.198924	12.571187
13.389242	1094.671219	12.576205
13.483149	1091.624692	12.581223
13.533901	1094.394203	12.586240
13.878159	1106.077975	12.591258
13.832217	1110.731417	12.596275
13.875805	1093.456439	12.601293
13.807182	1062.391725	12.606311
13.718319	1073.462079	12.611328
13.867338	1073.877539	12.616346
13.565237	1062.404170	12.621363
13.536166	1073.668726	12.626381
13.676863	1072.676658	12.631399
13.663902	1063.355062	12.636416
13.839860	1067.231650	12.641434
13.602327	1092.995600	12.646451
13.840285	1090.855552	12.651469
13.855068	1106.392739	12.656487
13.758222	1109.171392	12.661504
14.027054	1089.877593	12.666522
13.550667	1088.904744	12.671539
13.998451	1087.719247	12.676557
13.890054	1101.946010	12.681575
13.656078	1119.134848	12.686592
13.976153	1093.873895	12.691610
13.805509	1095.062575	12.696627
13.897194	1113.539190	12.701645
14.089757	1091.621434	12.706663
13.907126	1100.140807	12.711680
14.029283	1116.728010	12.716698
13.897188	1112.069919	12.721715
13.562729	1105.664111	12.726733
14.008249	1091.979200	12.731751
13.999822	1108.598700	12.736768
13.986474	1117.065705	12.741786
13.903980	1110.202709	12.746803
13.814808	1095.300668	12.751821
13.941820	1098.161489	12.756839
13.941158	1116.076147	12.761856
14.220361	1102.412414	12.766874
13.885414	1100.247776	12.771891
13.712779	1094.260005	12.776909
14.029265	1108.841162	12.781927
13.528637	1116.883500	12.786944
13.934124	1084.535570	12.791962
14.117351	1097.150742	12.796979
14.010133	1127.748127	12.801997
14.427892	1147.527950	12.807015
13.991521	1147.405068	12.812032
14.431037	1125.298950	12.817050
14.292365	1127.101687	12.822067
14.164570	1104.459088	12.827085
14.016375	1105.081599	12.832103
13.647201	1115.595992	12.837120
13.968213	1111.215300	12.842138
14.031101	1140.194831	12.847155
14.104224	1140.925026	12.852173
14.231182	1142.273633	12.857191
14.135506	1141.367166	12.862208
14.395571	1128.030706	12.867226
14.481634	1139.100146	12.872243
14.489603	1142.662865	12.877261
14.708810	1115.735684	12.882279
14.541596	1122.238054	12.887296
14.493126	1139.003441	12.892314
14.372355	1144.582029	12.897331
14.723112	1126.671355	12.902349
14.824098	1138.385317	12.907367
14.599476	1141.718131	12.912384
14.619644	1122.656282	12.917402
14.633446	1133.946368	12.922419
14.397410	1146.928727	12.927437
14.633024	1134.324276	12.932455
14.679570	1133.910127	12.937472
14.526042	1110.756739	12.942490
14.369984	1122.018995	12.947507
14.527846	1142.802254	12.952525
14.765931	1121.358213	12.957543
14.508629	1123.237725	12.962560
14.485987	1126.035115	12.967578
14.549460	1142.023923	12.972595
14.534939	1140.161754	12.977613
14.407186	1110.448220	12.982631
14.171613	1131.011018	12.987648
14.729479	1142.701832	12.992666
14.515336	1144.492639	12.997683
14.287976	1126.808079	13.002701
14.478215	1128.162759	13.007719
14.258361	1136.377159	13.012736
14.493630	1132.258601	13.017754
14.855045	1156.176565	13.022771
14.781058	1167.006691	13.027789
15.137596	1159.769620	13.032807
15.131639	1140.154131	13.037824
15.241686	1124.122260	13.042842
15.004869	1134.781978	13.047859
14.920909	1128.227901	13.052877
15.162882	1134.660590	13.057895
15.055492	1132.070840	13.062912
15.222176	1126.109048	13.067930
15.292819	1117.856017	13.072947
14.783711	1131.096822	13.077965
15.122442	1134.275432	13.082983
15.074296	1130.798447	13.088000
15.111361	1107.160923	13.093018
15.292935	1108.583158	13.098035
14.827601	1113.795747	13.103053
14.732008	1113.718987	13.108071
14.799670	1120.811915	13.113088
14.903204	1114.966346	13.118106
14.841674	1112.337236	13.123123
15.017222	1117.792751	13.128141
15.296957	1122.439019	13.133159
15.093248	1123.072968	13.138176
14.860673	1109.466544	13.143194
15.409071	1125.630059	13.148211
15.030464	1137.372696	13.153229
15.274093	1119.951370	13.158247
14.950608	1109.020640	13.163264
14.812422	1115.501087	13.168282
14.715832	1137.641324	13.173299
14.969164	1135.462615	13.178317
15.331822	1117.042924	13.183335
14.822220	1111.280769	13.188352
15.078443	1117.147258	13.193370
15.385535	1128.763388	13.198387
15.143691	1133.022739	13.203405
15.273257	1114.812886	13.208423
15.209186	1112.209288	13.213440
15.084220	1122.551275	13.218458
15.110114	1125.396635	13.223475
14.967659	1132.292360	13.228493
15.329631	1145.175698	13.233511
15.124311	1150.161714	13.238528
15.113309	1149.657984	13.243546
15.262222	1153.738818	13.248563
15.238754	1157.787721	13.253581
15.222705	1138.490951	13.258599
15.156442	1163.101891	13.263616
15.277544	1151.343709	13.268634
15.603854	1145.948892	13.273651
15.152260	1147.542677	13.278669
15.300588	1150.280526	13.283687
15.443644	1176.615921	13.288704
15.531119	1157.513780	13.293722
15.531750	1139.383950	13.298739
15.292555	1151.735099	13.303757
15.671129	1168.134055	13.308775
15.682178	1176.906239	13.313792
15.634926	1157.102618	13.318810
15.483117	1147.588613	13.323827
15.607872	1159.285379	13.328845
15.572776	1183.819073	13.333863
15.444110	1179.380420	13.338880
15.605570	1167.000646	13.343898
15.564102	1185.260236	13.348915
15.569278	1208.345928	13.353933
15.908722	1194.201601	13.358951
15.888074	1187.287219	13.363968
15.905611	1178.903200	13.368986
16.023997	1188.143854	13.374003
15.677197	1178.768917	13.379021
16.074823	1162.161658	13.384039
15.792777	1158.841991	13.389056
15.934779	1151.096315	13.394074
15.980631	1142.496664	13.399091
15.892568	1138.973924	13.404109
16.104116	1142.448978	13.409127
16.135904	1147.193891	13.414144
15.916206	1155.169750	13.419162
16.027138	1146.079341	13.424179
15.478234	1145.389370	13.429197
15.770686	1145.103342	13.434215
15.754088	1137.469393	13.439232
15.620880	1126.530232	13.444250
15.509874	1155.859514	13.449267
15.880159	1174.624630	13.454285
16.213126	1176.027364	13.459303
16.280409	1169.361487	13.464320
15.973775	1179.084871	13.469338
16.268095	1192.854514	13.474355
16.020953	1184.751281	13.479373
16.002611	1160.963518	13.484391
16.347058	1165.361859	13.489408
15.651693	1175.695313	13.494426
15.844963	1192.846299	13.499443
15.693863	1182.578005	13.504461
16.149546	1159.556590	13.509479
16.132141	1184.363280	13.514496
16.074536	1197.129330	13.519514
16.256218	1173.224656	13.524531
16.382326	1164.394951	13.529549
16.282539	1160.797194	13.534567
15.952915	1178.914480	13.539584
16.222742	1189.017002	13.544602
16.349555	1180.075782	13.549619
16.088026	1165.101982	13.554637
16.220367	1172.950597	13.559655
16.263946	1187.227209	13.564672
16.127200	1192.480383	13.569690
16.189085	1166.595600	13.574707
15.972784	1178.024311	13.579725
16.250829	1203.073869	13.584743
16.227201	1193.347262	13.589760
16.338496	1206.643544	13.594778
16.327728	1207.059337	13.599795
16.320759	1208.090990	13.604813
16.822973	1193.891524	13.609831
16.748298	1215.955533	13.614848
16.553027	1225.145901	13.619866
16.669413	1200.147414	13.624883
16.543089	1183.237734	13.629901
16.479693	1181.205136	13.634919
16.499716	1176.698517	13.639936
16.553238	1185.785657	13.644954
16.679810	1177.846895	13.649971
16.411578	1188.317203	13.654989
16.770392	1205.671205	13.660007
16.839322	1212.437569	13.665024
16.560275	1192.466252	13.670042
16.787246	1167.796508	13.675059
16.665027	1178.434071	13.680077
16.215658	1189.076502	13.685095
16.752281	1186.772546	13.690112
16.770798	1210.988247	13.695130
16.880779	1200.473203	13.700147
16.751850	1194.519400	13.705165
17.156458	1204.608614	13.710183
17.293082	1199.598190	13.715200
16.889560	1190.149470	13.720218
17.019275	1158.971784	13.725235
16.678777	1165.530655	13.730253
16.688902	1167.738035	13.735271
16.611885	1168.822589	13.740288
16.492161	1182.370065	13.745306
17.017132	1176.695715	13.750323
16.844617	1200.465721	13.755341
16.834838	1220.406918	13.760359
17.020583	1204.365012	13.765376
16.865514	1193.099278	13.770394
17.256513	1211.065144	13.775411
17.055331	1195.762913	13.780429
16.865718	1188.414850	13.785447
17.136878	1191.722621	13.790464
17.250300	1200.522871	13.795482
16.858667	1188.671579	13.800499
17.003020	1197.753655	13.805517
16.824114	1193.933193	13.810535
17.227885	1201.468234	13.815552
17.129725	1194.447985	13.820570
17.121037	1193.305441	13.825587
17.154199	1215.083189	13.830605
17.213784	1208.931338	13.835623
17.280871	1202.243437	13.840640
17.184930	1192.179258	13.845658
17.282245	1206.270376	13.850675
17.321613	1222.149303	13.855693
17.172059	1216.544683	13.860711
17.164897	1199.709267	13.865728
17.103755	1197.126721	13.870746
16.972384	1202.517658	13.875763
17.059487	1219.021121	13.880781
17.255475	1209.120548	13.885799
17.577949	1200.305410	13.890816
17.160554	1215.061081	13.895834
17.589138	1202.202986	13.900851
17.062841	1202.294030	13.905869
17.076952	1212.162022	13.910887
17.347055	1195.090482	13.915904
17.229184	1196.272614	13.920922
17.313444	1207.846317	13.925939
17.297131	1209.973839	13.930957
17.159110	1204.414847	13.935975
17.647419	1206.190342	13.940992
17.537214	1234.302806	13.946010
17.654944	1235.939690	13.951027
17.694322	1220.584200	13.956045
17.066717	1219.032537	13.961063
17.695551	1222.602392	13.966080
17.506614	1243.218840	13.971098
17.688956	1225.324566	13.976115
17.665335	1238.206069	13.981133
17.584837	1244.562794	13.986151
18.074363	1215.825632	13.991168
17.556538	1226.013666	13.996186
17.783028	1231.063653	14.001203
18.116500	1236.485438	14.006221
17.586089	1216.048269	14.011239
17.741294	1207.096043	14.016256
17.936181	1241.234117	14.021274
17.708356	1225.521691	14.026291
17.788779	1212.645353	14.031309
17.649848	1216.109558	14.036327
17.884235	1234.678852	14.041344
18.056734	1235.203009	14.046362
18.381686	1230.598358	14.051379
17.950238	1204.524135	14.056397
17.652450	1204.026958	14.061415
17.693054	1205.289865	14.066432
17.407789	1213.214793	14.071450
17.641995	1212.624980	14.076467
18.016679	1222.821293	14.081485
17.743303	1232.164697	14.086503
18.210619	1245.043011	14.091520
18.337859	1240.554474	14.096538
17.883016	1223.168061	14.101555
18.056446	1225.785367	14.106573
18.245985	1231.392413	14.111591
18.307335	1244.546918	14.116608
17.861705	1246.332890	14.121626
17.789777	1236.200064	14.126643
18.146852	1232.938013	14.131661
18.114673	1231.389799	14.136679
18.220799	1238.503290	14.141696
18.024962	1224.974727	14.146714
18.276014	1238.046414	14.151731
18.296768	1241.353067	14.156749
18.155778	1243.157677	14.161767
17.840446	1223.368948	14.166784
18.205085	1215.335720	14.171802
18.191542	1231.424337	14.176819
18.736652	1206.713174	14.181837
18.104256	1221.016800	14.186855
18.471268	1228.503414	14.191872
18.139497	1245.088622	14.196890
17.889389	1222.679987	14.201907
18.428432	1217.991842	14.206925
18.305473	1236.756871	14.211943
18.509383	1249.260608	14.216960
18.511309	1247.326925	14.221978
18.392381	1233.863087	14.226995
18.450026	1237.977427	14.232013
18.511151	1256.889380	14.237031
18.615106	1242.445815	14.242048
18.413009	1253.054808	14.247066
18.279242	1250.605880	14.252083
18.651802	1245.227494	14.257101
18.599080	1240.080866	14.262119
18.859289	1246.606039	14.267136
18.858753	1258.915178	14.272154
18.487711	1248.032060	14.277171
18.602618	1251.080693	14.282189
18.409481	1252.892445	14.287207
18.629320	1239.031461	14.292224
18.523597	1253.982260	14.297242
18.406226	1242.618451	14.302259
18.629912	1247.139209	14.307277
18.119242	1254.129687	14.312295
18.462050	1242.541344	14.317312
18.418908	1257.285394	14.322330
18.747176	1268.044986	14.327347
18.747187	1260.093147	14.332365
18.929750	1273.084668	14.337383
18.896208	1281.247102	14.342400
19.185044	1285.811226	14.347418
18.741610	1274.709397	14.352435
18.906720	1256.803960	14.357453
18.914870	1282.711346	14.362471
19.039628	1267.329794	14.367488
19.165757	1268.347623	14.372506
19.285519	1280.285801	14.377523
19.491092	1263.830711	14.382541
19.018864	1253.667983	14.387559
19.364498	1236.524776	14.392576
19.324389	1235.203508	14.397594
18.943415	1244.146984	14.402611
19.142865	1248.118728	14.407629
19.319498	1233.461043	14.412647
19.253667	1216.320909	14.417664
19.095634	1224.834614	14.422682
18.995248	1226.919451	14.427699
19.198227	1217.260179	14.432717
18.970578	1241.417320	14.437735
19.188873	1257.931422	14.442752
19.246387	1262.562598	14.447770
19.335115	1254.306701	14.452787
19.522068	1266.064119	14.457805
19.624112	1250.373812	14.462823
19.541562	1236.583661	14.467840
19.236083	1221.293424	14.472858
19.068603	1228.192836	14.477875
19.285246	1221.086309	14.482893
19.341063	1232.113286	14.487911
19.600842	1253.627119	14.492928
19.518206	1246.020265	14.497946
19.404414	1231.781353	14.502963
19.493951	1221.980430	14.507981
19.267639	1238.059147	14.512999
19.561832	1268.276085	14.518016
19.894970	1266.245648	14.523034
19.487202	1255.575237	14.528051
19.865997	1223.550936	14.533069
19.378215	1239.818793	14.538087
19.415036	1229.612599	14.543104
19.489108	1240.695312	14.548122
19.088004	1275.041471	14.553139
19.616625	1255.248637	14.558157
19.606554	1252.695526	14.563175
19.420707	1272.450977	14.568192
19.630647	1264.351480	14.573210
19.410060	1275.259046	14.578227
19.595129	1276.491886	14.583245
19.616453	1275.429593	14.588263
19.605590	1279.494059	14.593280
19.464610	1275.229518	14.598298
19.525007	1266.891997	14.603315
19.764990	1288.773928	14.608333
19.916928	1289.553985	14.613351
20.044063	1291.915136	14.618368
20.264722	1304.848924	14.623386
20.059192	1311.736751	14.628403
20.321293	1265.383007	14.633421
20.131095	1267.836545	14.638439
19.728774	1268.027546	14.643456
20.177972	1272.048851	14.648474
19.729947	1279.366901	14.653491
19.808764	1281.349314	14.658509
20.272635	1276.202621	14.663527
20.188626	1276.727347	14.668544
20.156926	1272.540986	14.673562
19.961602	1282.442452	14.678579
20.364141	1276.565417	14.683597
19.979010	1275.556711	14.688615
19.510531	1281.691511	14.693632
20.090067	1298.166231	14.698650
20.177455	1296.399774	14.703667
20.197903	1293.480280	14.708685
20.227840	1311.863427	14.713703
20.007442	1300.820564	14.718720
20.215971	1285.303426	14.723738
20.006804	1278.907444	14.728755
20.504392	1288.936281	14.733773
20.313934	1305.481572	14.738791
20.372200	1288.587422	14.743808
20.354984	1298.135033	14.748826
20.367786	1294.057525	14.753843
20.400575	1280.084435	14.758861
20.471330	1287.911602	14.763879
20.586256	1302.081966	14.768896
20.610801	1294.547316	14.773914
20.420104	1283.739758	14.778931
20.560028	1280.742269	14.783949
20.518142	1292.625790	14.788967
20.194284	1299.126666	14.793984
20.487552	1277.865860	14.799002
20.386305	1303.234501	14.804019
20.605918	1290.039594	14.809037
20.688995	1311.689672	14.814055
20.803432	1329.150228	14.819072
20.689288	1299.514767	14.824090
20.253574	1299.646341	14.829107
20.692731	1312.513031	14.834125
20.885506	1307.488176	14.839143
20.809600	1312.300729	14.844160
20.885910	1318.718953	14.849178
21.006692	1317.009067	14.854195
20.990126	1310.280526	14.859213
20.760364	1310.558339	14.864231
20.611307	1306.107176	14.869248
21.076899	1292.302459	14.874266
20.826288	1297.727009	14.879283
21.137977	1312.907637	14.884301
21.119830	1286.594050	14.889319
20.698145	1283.943737	14.894336
20.839626	1299.930841	14.899354
21.035669	1310.660751	14.904371
20.720994	1328.095585	14.909389
20.702126	1329.952349	14.914407
20.833590	1318.428099	14.919424
21.013037	1308.748157	14.924442
20.965919	1326.648106	14.929459
20.827697	1328.716183	14.934477
21.015431	1309.028814	14.939495
21.212574	1308.217221	14.944512
21.063167	1314.489026	14.949530
20.925227	1324.412722	14.954547
21.093486	1327.543183	14.959565
21.106472	1306.302185	14.964583
20.988248	1314.705251	14.969600
21.091206	1333.630854	14.974618
21.362691	1340.598098	14.979635
21.694246	1333.644046	14.984653
21.550208	1330.189258	14.989671
21.198239	1323.530208	14.994688
21.282097	1308.955877	14.999706
21.434233	1332.373688	15.004723
21.285191	1352.108694	15.009741
21.755685	1331.518072	15.014759
21.514445	1347.591497	15.019776
21.756779	1330.872643	15.024794
21.669888	1310.277330	15.029811
21.472485	1316.317850	15.034829
21.581111	1323.151111	15.039847
21.324346	1321.335249	15.044864
21.677336	1298.151110	15.049882
21.425569	1312.334650	15.054899
21.585843	1312.591011	15.059917
21.927787	1328.443664	15.064935
21.546106	1333.352904	15.069952
21.806828	1320.312065	15.074970
21.701967	1336.182570	15.079987
21.499253	1345.173598	15.085005
21.976769	1339.428309	15.090023
21.763830	1348.301272	15.095040
21.705674	1333.228556	15.100058
21.654674	1330.887169	15.105075
21.817950	1333.285946	15.110093
21.759340	1342.156724	15.115111
21.942827	1344.833693	15.120128
21.901030	1329.504497	15.125146
21.798139	1329.966219	15.130163
21.873244	1335.025218	15.135181
22.040958	1331.973925	15.140199
21.685547	1336.582240	15.145216
21.901954	1320.281169	15.150234
21.754442	1337.380587	15.155251
21.739467	1329.515618	15.160269
21.869590	1313.017150	15.165287
21.735047	1323.525876	15.170304
21.767227	1335.643197	15.175322
21.781301	1343.018841	15.180339
22.049326	1346.629359	15.185357
22.446020	1350.569815	15.190375
22.006745	1369.787974	15.195392
22.390433	1363.171376	15.200410
22.303783	1364.192885	15.205427
22.484822	1355.606987	15.210445
22.690371	1338.237857	15.215463
22.362740	1337.706738	15.220480
22.556380	1323.090438	15.225498
22.405063	1322.697861	15.230515
22.347498	1332.533100	15.235533
22.559991	1319.296440	15.240551
22.236888	1330.700896	15.245568
22.306507	1330.693660	15.250586
22.465566	1328.332518	15.255603
22.490998	1310.535022	15.260621
22.382766	1310.486720	15.265639
22.465739	1328.155872	15.270656
22.454202	1320.496690	15.275674
22.433223	1339.250699	15.280691
22.798028	1340.538076	15.285709
22.867598	1322.444953	15.290727
22.316051	1328.593990	15.295744
22.653477	1329.313286	15.300762
22.665767	1324.419310	15.305779
22.458468	1367.114198	15.310797
22.524334	1355.270816	15.315815
22.192801	1352.369820	15.320832
22.570669	1355.526954	15.325850
23.038767	1353.543676	15.330867
22.616099	1362.570372	15.335885
22.964777	1343.694360	15.340903
22.941461	1349.740074	15.345920
22.962890	1355.529045	15.350938
22.779705	1360.732090	15.355955
22.926582	1352.936994	15.360973
22.853375	1347.925378	15.365991
22.993829	1361.648964	15.371008
23.101149	1348.161709	15.376026
22.882614	1362.644262	15.381043
23.078349	1374.800517	15.386061
23.435778	1358.276541	15.391079
22.776525	1358.132036	15.396096
22.741380	1352.156178	15.401114
22.999593	1360.440875	15.406131
22.753647	1373.128575	15.411149
22.672798	1354.211154	15.416167
22.736563	1349.691647	15.421184
23.018968	1374.205160	15.426202
23.306462	1396.105568	15.431219
23.075458	1394.118352	15.436237
23.271253	1388.661769	15.441255
23.226853	1382.690972	15.446272
23.378799	1376.454614	15.451290
23.372467	1367.599544	15.456307
23.523471	1390.824368	15.461325
23.577021	1366.422475	15.466343
23.147021	1384.008093	15.471360
23.352043	1397.702935	15.476378
23.376353	1381.287022	15.481395
23.226314	1376.408046	15.486413
23.480990	1386.548727	15.491431
23.331128	1378.216174	15.496448
23.393830	1374.989258	15.501466
23.436392	1372.969827	15.506483
23.285111	1373.158508	15.511501
23.377294	1378.147588	15.516519
23.392080	1369.153330	15.521536
23.410049	1384.644023	15.526554
23.746484	1403.752341	15.531571
23.950462	1395.456264	15.536589
23.940129	1366.222126	15.541607
23.709640	1376.196770	15.546624
23.387893	1385.542258	15.551642
23.746617	1378.207305	15.556659
23.526878	1391.326417	15.561677
23.640843	1406.001942	15.566695
23.969676	1396.806887	15.571712
23.665202	1416.300103	15.576730
24.183883	1412.862721	15.581747
24.012233	1401.223378	15.586765
23.709264	1410.153174	15.591783
24.157492	1423.307962	15.596800
24.144841	1413.195038	15.601818
24.415111	1405.445258	15.606835
24.202551	1398.446871	15.611853
23.993499	1377.851482	15.616871
24.073552	1387.521035	15.621888
23.943508	1364.132726	15.626906
24.263865	1359.180450	15.631923
23.986575	1380.491942	15.636941
24.350427	1384.821802	15.641959
24.508948	1379.136298	15.646976
24.302852	1373.176775	15.651994
24.259681	1369.803023	15.657011
24.072559	1358.032541	15.662029
24.274168	1356.192589	15.667047
24.144125	1360.518546	15.672064
24.197664	1365.443060	15.677082
24.333939	1369.890033	15.682099
24.070183	1393.949960	15.687117
24.365396	1408.936108	15.692135
24.479476	1413.880056	15.697152
24.475795	1394.318872	15.702170
24.754407	1386.991544	15.707187
24.465919	1402.329696	15.712205
24.923197	1407.828404	15.717223
24.687484	1394.177373	15.722240
24.315083	1362.715401	15.727258
24.752112	1370.859162	15.732275
24.628262	1396.383725	15.737293
24.492060	1392.838868	15.742311
24.545010	1393.558141	15.747328
24.510962	1414.271932	15.752346
24.801478	1393.050684	15.757363
24.856371	1387.958845	15.762381
24.948995	1394.510693	15.767399
24.879382	1407.308227	15.772416
25.049456	1398.136159	15.777434
25.078286	1384.110688	15.782451
24.813683	1375.047071	15.787469
24.504313	1366.911513	15.792487
24.800078	1387.433395	15.797504
24.615672	1390.661509	15.802522
24.798058	1374.304108	15.807539
24.906285	1393.850821	15.812557
24.862894	1387.944603	15.817575
25.008601	1387.339395	15.822592
24.667895	1412.983858	15.827610
24.868458	1409.225803	15.832627
25.084185	1414.988494	15.837645
24.677039	1391.568786	15.842663
25.032830	1392.503210	15.847680
24.696968	1417.498207	15.852698
25.428481	1413.992984	15.857715
25.127295	1409.704104	15.862733
25.373854	1411.757907	15.867751
25.221652	1420.029177	15.872768
25.045977	1422.451507	15.877786
25.086813	1416.995528	15.882803
25.360133	1420.555496	15.887821
25.142842	1427.095396	15.892839
25.348291	1410.520118	15.897856
25.288018	1426.050155	15.902874
25.643998	1437.214251	15.907891
25.427337	1418.905085	15.912909
25.504923	1410.013096	15.917927
25.539391	1424.081640	15.922944
25.429327	1438.912596	15.927962
25.810949	1426.198659	15.932979
25.534417	1426.287495	15.937997
25.197758	1426.046283	15.943015
24.951402	1439.670117	15.948032
25.338456	1438.795253	15.953050
25.609258	1423.869124	15.958067
25.617251	1427.715700	15.963085
25.632503	1418.652453	15.968103
25.562427	1421.637715	15.973120
25.649801	1434.871727	15.978138
25.716851	1435.252526	15.983155
25.748415	1469.968665	15.988173
25.507240	1456.944818	15.993191
25.743616	1454.677451	15.998208
25.515447	1462.087869	16.003226
25.664295	1445.256513	16.008243
25.700961	1447.074200	16.013261
25.865749	1453.558943	16.018279
26.134481	1439.541798	16.023296
26.327777	1442.018783	16.028314
26.365603	1447.494813	16.033331
26.220628	1444.496844	16.038349
26.285397	1439.096435	16.043367
26.415601	1448.922172	16.048384
26.209898	1445.548201	16.053402
26.601472	1446.747915	16.058419
26.721280	1439.831365	16.063437
26.598211	1415.747589	16.068455
26.656659	1404.631708	16.073472
26.136651	1425.097054	16.078490
25.917919	1416.934191	16.083507
26.133785	1418.982833	16.088525
26.182643	1413.160847	16.093543
26.113317	1427.752338	16.098560
25.891931	1459.928156	16.103578
26.236753	1445.947928	16.108595
26.224373	1432.876945	16.113613
26.177666	1436.453687	16.118631
26.615059	1441.185491	16.123648
26.335074	1448.415334	16.128666
26.465766	1433.925545	16.133683
26.232244	1426.190125	16.138701
26.444953	1427.607148	16.143719
26.335152	1457.011594	16.148736
26.305276	1467.581156	16.153754
26.253124	1449.462338	16.158771
26.412310	1464.116866	16.163789
26.387474	1470.874337	16.168807
26.891143	1462.797440	16.173824
27.135124	1482.143525	16.178842
26.902029	1479.492222	16.183859
26.758389	1469.373945	16.188877
26.614824	1466.468927	16.193895
27.009618	1470.756895	16.198912
26.716706	1476.226088	16.203930
27.022491	1471.379115	16.208947
26.968064	1462.121104	16.213965
26.957399	1468.433416	16.218983
27.170436	1470.310129	16.224000
26.967115	1472.246200	16.229018
26.961072	1461.360375	16.234035
26.962086	1457.940925	16.239053
27.167749	1477.362809	16.244071
27.187283	1464.358949	16.249088
27.159321	1477.763992	16.254106
27.198432	1467.913581	16.259123
27.208112	1466.654521	16.264141
27.004260	1463.342137	16.269159
27.584718	1460.938005	16.274176
27.449022	1463.950355	16.279194
27.527173	1485.742802	16.284211
27.612280	1469.597885	16.289229
27.358854	1455.380954	16.294247
27.283442	1457.210866	16.299264
27.151971	1472.617411	16.304282
27.025888	1487.187438	16.309299
27.383365	1466.462393	16.314317
27.182985	1476.047271	16.319335
27.543763	1484.089643	16.324352
27.532387	1502.946279	16.329370
28.074340	1500.905218	16.334387
28.110497	1478.327078	16.339405
27.563129	1472.062967	16.344423
27.437206	1471.417820	16.349440
27.429290	1484.076904	16.354458
27.758952	1483.514605	16.359475
27.793936	1483.739421	16.364493
27.572086	1493.677190	16.369511
27.819079	1491.576038	16.374528
28.000097	1496.730359	16.379546
27.841185	1494.775990	16.384563
27.901487	1493.915068	16.389581
27.741945	1483.994347	16.394599
28.154418	1490.809847	16.399616
27.923715	1510.656266	16.404634
27.703228	1502.281587	16.409651
28.025267	1485.871960	16.414669
28.082445	1487.512973	16.419687
28.139914	1487.440635	16.424704
27.831645	1506.298807	16.429722
27.867310	1503.262512	16.434739
27.962527	1495.057666	16.439757
27.918291	1486.605554	16.444775
28.238471	1486.075031	16.449792
28.015201	1494.659101	16.454810
28.077009	1496.613553	16.459827
28.419092	1496.666880	16.464845
28.355260	1516.950493	16.469863
28.565502	1506.498476	16.474880
28.262772	1493.389318	16.479898
28.383884	1511.258338	16.484915
28.571992	1518.095280	16.489933
28.460726	1508.302658	16.494951
28.718487	1512.506613	16.499968
28.401117	1483.349755	16.504986
28.377995	1492.606598	16.510003
28.726488	1510.026320	16.515021
28.195847	1526.204142	16.520039
28.502270	1507.331959	16.525056
28.291269	1506.246932	16.530074
28.715347	1525.427318	16.535091
28.898366	1520.542460	16.540109
28.747593	1513.900658	16.545127
28.732976	1502.625065	16.550144
28.641657	1516.768307	16.555162
28.556132	1531.372314	16.560179
28.696828	1522.753530	16.565197
28.702622	1516.233854	16.570215
28.848146	1499.663560	16.575232
28.919850	1515.614990	16.580250
28.760049	1522.015538	16.585267
28.844147	1512.817362	16.590285
28.625675	1499.156893	16.595303
28.597483	1513.547025	16.600320
28.879059	1520.853752	16.605338
28.692190	1537.363668	16.610355
29.411038	1547.021245	16.615373
28.931034	1551.781975	16.620391
29.399825	1539.855433	16.625408
29.538867	1526.098270	16.630426
29.690944	1555.034032	16.635443
29.574703	1534.618426	16.640461
29.395359	1502.769812	16.645479
29.291996	1499.480471	16.650496
29.408567	1508.938009	16.655514
29.250095	1506.634626	16.660531
29.465189	1510.496791	16.665549
28.980208	1494.125162	16.670567
28.692220	1509.970019	16.675584
29.486516	1539.117763	16.680602
29.439070	1537.439983	16.685619
29.502031	1527.772362	16.690637
29.516274	1529.795098	16.695655
29.785049	1524.961506	16.700672
29.422601	1515.675640	16.705690
29.454022	1531.813331	16.710707
29.716326	1533.914636	16.715725
29.418499	1534.082270	16.720743
29.292216	1538.757679	16.725760
29.413381	1532.016612	16.730778
29.776220	1551.916446	16.735795
30.045282	1553.338338	16.740813
30.215065	1564.050231	16.745831
30.292152	1550.819118	16.750848
30.414727	1549.589417	16.755866
29.846495	1540.837630	16.760883
30.167354	1533.868626	16.765901
29.632783	1525.089636	16.770919
29.881077	1518.154771	16.775936
29.720993	1534.221278	16.780954
30.057938	1538.559762	16.785971
30.371496	1543.288642	16.790989
30.191762	1568.100146	16.796007
30.268248	1552.276086	16.801024
30.581452	1545.118027	16.806042
30.373009	1554.172118	16.811059
30.308869	1563.452905	16.816077
30.156632	1542.460586	16.821095
30.201346	1539.412259	16.826112
30.669140	1553.851936	16.831130
30.446695	1557.996213	16.836147
30.848337	1546.505179	16.841165
30.422665	1526.921651	16.846183
30.377790	1530.269717	16.851200
30.566154	1510.278802	16.856218
30.200534	1520.133087	16.861235
30.674448	1533.582282	16.866253
30.565160	1538.631179	16.871271
30.854151	1558.602267	16.876288
30.798190	1532.871645	16.881306
30.548542	1514.832816	16.886323
30.718651	1501.794398	16.891341
30.604222	1531.198965	16.896359
30.840168	1546.797570	16.901376
30.682798	1528.485461	16.906394
30.764589	1534.571643	16.911411
30.903284	1550.333535	16.916429
30.656193	1558.686392	16.921447
30.455807	1554.894384	16.926464
30.643022	1536.645178	16.931482
30.543920	1534.544237	16.936499
30.966037	1537.271551	16.941517
30.930123	1560.811418	16.946535
30.628474	1542.235500	16.951552
31.028906	1568.896775	16.956570
30.993961	1574.403376	16.961587
31.136653	1578.056704	16.966605
31.081629	1577.347583	16.971623
31.169527	1567.490127	16.976640
31.328462	1562.781837	16.981658
31.373025	1584.494658	16.986675
31.501346	1593.673791	16.991693
31.028397	1584.551093	16.996711
31.035678	1567.175795	17.001728
31.636803	1568.204798	17.006746
31.492913	1587.130472	17.011763
31.477420	1583.235281	17.016781
31.519578	1558.573208	17.021799
31.437747	1563.754948	17.026816
31.871013	1570.301652	17.031834
31.606490	1587.860650	17.036851
31.736925	1571.854561	17.041869
31.679854	1575.203964	17.046887
31.418294	1576.485837	17.051904
31.587777	1560.255539	17.056922
31.653302	1576.332929	17.061939
31.521316	1588.373370	17.066957
31.540331	1570.741754	17.071975
31.212912	1554.252310	17.076992
31.774804	1567.893154	17.082010
31.612875	1597.585558	17.087027
31.999144	1581.993286	17.092045
32.365965	1591.407751	17.097063
32.139224	1601.101962	17.102080
32.120987	1580.337296	17.107098
31.794628	1569.885641	17.112115
32.211369	1575.347025	17.117133
32.087336	1592.540760	17.122151
32.181847	1586.044771	17.127168
32.165438	1583.536344	17.132186
32.354574	1587.548948	17.137203
32.326591	1593.656738	17.142221
32.273614	1585.067069	17.147239
32.349503	1576.520368	17.152256
32.621811	1576.534548	17.157274
32.464648	1599.959009	17.162291
32.277694	1585.369927	17.167309
32.448717	1585.922681	17.172327
32.132798	1594.696588	17.177344
32.542934	1575.441119	17.182362
32.655087	1590.321801	17.187379
32.609932	1587.722180	17.192397
32.615166	1582.368067	17.197415
32.274831	1598.189389	17.202432
32.500297	1593.669166	17.207450
32.359222	1593.674902	17.212467
31.982008	1584.452641	17.217485
32.547976	1578.222375	17.222503
32.377380	1574.530436	17.227520
32.590116	1599.175188	17.232538
32.841275	1622.951509	17.237555
32.861137	1615.505054	17.242573
33.033605	1619.604754	17.247591
32.796034	1632.962698	17.252608
33.153843	1611.114411	17.257626
33.013653	1612.326340	17.262643
33.252273	1611.134729	17.267661
33.245607	1587.491783	17.272679
33.083190	1589.884592	17.277696
33.339323	1578.407641	17.282714
32.911308	1590.399778	17.287731
33.237825	1619.468318	17.292749
33.430254	1610.845167	17.297767
33.106638	1612.164162	17.302784
33.387343	1589.898816	17.307802
33.188910	1601.621380	17.312819
32.849359	1608.288035	17.317837
33.150708	1617.505997	17.322855
32.862732	1620.579164	17.327872
33.018216	1599.755063	17.332890
33.043968	1606.324252	17.337907
33.068567	1623.241151	17.342925
33.181657	1639.252393	17.347943
33.604222	1648.638394	17.352960
33.663546	1651.173076	17.357978
33.373945	1643.006845	17.362995
33.858637	1642.051282	17.368013
33.718092	1649.535875	17.373031
33.312468	1649.582178	17.378048
33.531986	1627.316065	17.383066
33.734990	1634.848581	17.388083
33.618488	1649.232179	17.393101
33.733920	1626.331730	17.398119
33.559836	1625.055692	17.403136
33.974516	1638.106292	17.408154
34.030328	1661.574869	17.413171
33.660542	1680.915665	17.418189
34.274226	1665.160853	17.423207
34.183888	1654.873933	17.428224
34.513140	1658.138554	17.433242
34.448460	1662.182592	17.438259
34.052225	1643.222658	17.443277
34.335125	1613.810680	17.448295
34.236688	1621.212036	17.453312
34.412765	1635.455461	17.458330
34.420542	1627.524093	17.463347
34.674875	1614.635505	17.468365
34.586785	1630.572525	17.473383
34.488563	1619.488380	17.478400
34.426555	1610.880115	17.483418
34.635870	1641.032208	17.488435
34.426164	1640.203498	17.493453
34.714699	1612.767635	17.498471
34.636273	1610.877198	17.503488
34.600466	1623.103895	17.508506
34.546262	1635.169404	17.513523
34.783037	1619.572572	17.518541
35.000104	1613.447181	17.523559
34.695560	1624.414627	17.528576
34.930824	1640.418572	17.533594
34.743043	1629.307299	17.538611
35.136997	1615.782086	17.543629
35.264335	1609.570660	17.548647
34.759526	1627.676095	17.553664
34.603484	1636.655250	17.558682
34.745154	1622.109248	17.563699
34.557636	1611.556095	17.568717
34.605227	1621.674965	17.573735
34.497009	1648.355486	17.578752
34.777693	1647.472505	17.583770
34.988379	1650.696100	17.588787
35.134861	1672.826070	17.593805
35.165984	1644.494005	17.598823
35.138177	1647.786434	17.603840
34.994299	1658.088215	17.608858
35.223307	1667.004350	17.613875
35.046129	1655.439530	17.618893
35.235140	1637.980982	17.623911
35.177302	1666.066101	17.628928
35.359051	1679.046097	17.633946
35.530894	1688.873570	17.638963
35.476184	1697.564222	17.643981
35.802837	1667.812695	17.648999
35.690445	1686.798431	17.654016
35.424941	1688.949978	17.659034
35.855253	1669.084293	17.664051
35.659344	1676.021766	17.669069
35.949824	1666.670914	17.674087
35.864223	1664.816785	17.679104
36.079149	1676.593417	17.684122
35.682764	1695.767009	17.689139
35.604352	1687.801437	17.694157
35.534833	1668.908421	17.699175
35.310821	1674.143117	17.704192
35.770917	1671.275578	17.709210
35.907948	1673.317897	17.714227
35.953708	1675.059025	17.719245
36.008954	1652.871092	17.724263
35.933249	1679.033212	17.729280
35.971067	1708.737795	17.734298
36.293617	1702.091104	17.739315
35.785611	1683.937223	17.744333
36.425141	1694.027108	17.749351
36.234007	1707.747446	17.754368
36.439749	1718.465609	17.759386
36.753424	1684.804790	17.764403
36.472374	1681.516136	17.769421
36.494261	1683.108781	17.774439
36.279136	1711.195767	17.779456
36.656820	1687.600448	17.784474
36.965137	1676.712905	17.789491
36.737891	1674.101242	17.794509
36.755833	1683.900809	17.799527
36.912342	1685.424368	17.804544
36.606785	1662.238782	17.809562
36.692203	1659.965825	17.814579
36.725480	1678.710695	17.819597
36.781031	1682.503520	17.824615
36.976360	1682.873559	17.829632
36.976354	1699.159996	17.834650
37.005486	1682.766776	17.839667
36.811563	1662.162893	17.844685
36.866560	1680.494517	17.849703
37.007949	1712.573327	17.854720
36.496069	1697.737204	17.859738
37.022175	1668.773412	17.864755
36.717550	1682.405614	17.869773
36.911980	1701.662155	17.874791
36.716515	1699.005481	17.879808
36.484606	1695.494081	17.884826
36.703663	1710.570163	17.889843
36.941142	1724.177668	17.894861
37.142044	1718.017415	17.899879
37.113599	1730.558960	17.904896
37.322603	1723.591723	17.909914
37.425149	1713.846296	17.914931
37.145498	1737.747611	17.919949
37.140518	1728.754439	17.924967
37.116081	1725.983197	17.929984
37.244422	1757.122913	17.935002
37.748075	1771.103910	17.940019
37.435389	1774.646058	17.945037
37.765380	1744.303989	17.950055
37.824846	1749.811879	17.955072
37.861142	1776.727056	17.960090
37.868297	1765.913720	17.965107
37.937080	1745.198316	17.970125
37.912887	1736.005305	17.975143
38.034940	1749.910690	17.980160
37.629585	1766.421039	17.985178
37.867626	1747.000624	17.990195
37.879406	1765.182829	17.995213
37.881833	1751.338416	18.000231
38.157268	1729.104442	18.005248
38.186398	1748.078578	18.010266
38.440772	1764.128500	18.015283
38.474621	1763.210137	18.020301
38.386386	1738.264167	18.025319
38.149476	1751.246984	18.030336
37.948826	1767.276944	18.035354
38.597648	1756.291156	18.040371
38.166440	1751.436578	18.045389
38.042052	1738.257688	18.050407
38.436509	1760.301245	18.055424
38.550298	1782.267716	18.060442
39.148242	1770.635535	18.065459
38.643596	1750.881637	18.070477
38.838295	1745.520169	18.075495
38.788073	1756.010435	18.080512
38.651142	1757.057106	18.085530
38.977208	1739.354383	18.090547
38.461275	1730.968570	18.095565
38.642017	1743.567566	18.100583
38.762390	1752.054844	18.105600
38.699512	1765.790449	18.110618
39.099478	1776.623083	18.115635
39.001774	1764.749143	18.120653
38.818844	1759.980969	18.125671
39.106789	1777.418974	18.130688
38.932078	1784.730180	18.135706
39.243737	1760.502089	18.140723
38.698300	1753.487595	18.145741
38.873632	1764.725869	18.150759
39.145185	1786.608807	18.155776
39.113557	1776.254242	18.160794
39.325769	1755.828937	18.165811
39.383623	1748.168209	18.170829
39.601225	1762.907545	18.175847
39.286754	1768.511184	18.180864
39.032548	1774.882368	18.185882
39.328860	1789.518977	18.190899
39.109533	1803.258721	18.195917
39.498579	1791.768799	18.200935
39.705199	1784.913323	18.205952
39.593224	1803.583549	18.210970
39.782994	1808.877446	18.215987
39.726911	1803.077869	18.221005
39.521569	1798.495635	18.226023
39.749185	1776.714287	18.231040
39.666631	1793.817453	18.236058
40.162247	1814.890036	18.241075
39.816687	1797.823127	18.246093
39.799343	1800.553144	18.251111
39.781812	1781.902726	18.256128
39.965830	1796.867285	18.261146
40.106205	1802.769715	18.266163
39.977739	1789.713083	18.271181
39.764247	1783.778731	18.276199
40.145065	1798.456983	18.281216
40.168166	1828.797174	18.286234
40.209985	1818.669766	18.291251
40.293879	1814.567678	18.296269
40.444202	1829.928803	18.301287
40.917230	1814.816152	18.306304
40.627809	1819.739230	18.311322
40.734567	1795.013258	18.316339
40.548846	1781.408823	18.321357
40.268503	1789.784325	18.326375
40.807062	1788.804206	18.331392
40.577863	1791.374191	18.336410
40.903604	1780.860489	18.341427
40.704573	1788.377939	18.346445
40.602968	1797.070099	18.351463
40.604045	1805.661650	18.356480
40.735684	1808.869607	18.361498
41.013728	1814.549922	18.366515
40.973071	1794.934899	18.371533
40.940836	1803.023690	18.376551
40.758316	1812.924266	18.381568
40.637311	1828.388188	18.386586
40.564876	1816.778482	18.391603
40.491662	1812.084171	18.396621
40.618595	1834.528174	18.401639
41.053858	1838.403833	18.406656
41.348590	1847.794058	18.411674
41.061066	1839.964516	18.416691
41.147128	1847.234234	18.421709
41.036191	1852.223184	18.426727
41.442518	1859.479740	18.431744
41.067404	1844.813060	18.436762
41.359533	1860.057493	18.441779
41.529338	1846.858628	18.446797
41.061866	1852.651821	18.451815
41.323357	1864.614860	18.456832
41.479054	1869.287170	18.461850
41.777352	1877.735176	18.466867
41.926846	1875.558272	18.471885
41.689057	1870.429319	18.476903
41.860928	1860.472186	18.481920
42.076629	1870.130356	18.486938
42.117509	1865.888343	18.491955
42.301629	1868.276873	18.496973
42.230132	1855.882686	18.501991
42.380382	1867.214730	18.507008
42.101798	1860.493523	18.512026
42.152162	1830.092887	18.517043
42.153288	1823.953894	18.522061
42.344955	1835.300227	18.527079
42.479681	1835.425118	18.532096
41.962810	1827.488433	18.537114
42.103574	1831.847217	18.542131
41.933197	1842.146121	18.547149
42.258705	1844.414353	18.552167
42.677759	1851.508303	18.557184
42.140173	1862.212617	18.562202
42.293191	1874.130904	18.567219
42.574808	1855.285322	18.572237
42.798329	1844.175892	18.577255
43.050515	1843.798102	18.582272
42.874068	1876.992365	18.587290
42.642139	1859.796985	18.592307
42.790328	1843.029264	18.597325
42.782797	1861.159176	18.602343
43.013867	1863.144847	18.607360
42.470679	1853.341306	18.612378
42.800099	1859.881089	18.617395
42.959714	1846.510615	18.622413
42.523246	1862.352326	18.627431
42.885946	1858.294490	18.632448
43.026404	1849.098115	18.637466
42.912973	1833.649568	18.642483
43.083972	1855.602558	18.647501
42.728695	1868.860004	18.652519
43.198851	1864.800646	18.657536
43.244849	1886.894392	18.662554
43.100005	1890.683777	18.667571
43.095628	1880.139438	18.672589
43.201924	1888.931717	18.677607
43.162059	1880.861268	18.682624
42.875071	1901.845424	18.687642
43.216852	1899.216252	18.692659
43.698093	1893.336016	18.697677
43.400855	1923.478198	18.702695
43.573938	1933.990040	18.707712
43.334222	1917.759281	18.712730
43.652373	1911.745095	18.717747
43.895817	1920.154758	18.722765
43.700630	1926.302414	18.727783
44.162897	1919.225042	18.732800
43.753628	1912.649105	18.737818
43.762409	1908.293509	18.742835
44.221205	1903.926630	18.747853
43.490789	1909.207003	18.752871
44.114597	1935.198564	18.757888
44.298003	1925.927934	18.762906
44.027370	1925.952914	18.767923
44.560420	1934.932622	18.772941
44.312771	1953.978040	18.777959
44.759807	1941.304828	18.782976
44.277928	1910.605641	18.787994
44.277828	1917.794865	18.793011
44.561331	1908.842089	18.798029
44.251686	1926.873900	18.803047
44.845243	1940.080598	18.808064
44.878080	1938.147919	18.813082
44.514673	1923.254961	18.818099
45.015368	1943.663132	18.823117
44.841169	1928.524474	18.828135
45.031495	1893.794911	18.833152
44.957687	1893.184235	18.838170
44.625348	1904.499319	18.843187
44.836221	1892.484246	18.848205
44.678082	1930.116865	18.853223
44.771236	1932.378535	18.858240
44.862124	1922.460330	18.863258
44.713815	1922.896312	18.868275
45.265295	1936.453694	18.873293
44.841510	1947.406729	18.878311
45.012168	1918.582095	18.883328
45.027690	1914.847115	18.888346
44.819378	1939.287341	18.893363
44.857860	1942.182829	18.898381
45.213862	1937.765321	18.903399
45.423604	1942.758974	18.908416
45.427383	1958.408863	18.913434
45.295166	1949.437375	18.918451
45.555260	1942.817730	18.923469
45.390946	1966.865172	18.928487
45.553772	1951.182604	18.933504
45.599290	1941.187648	18.938522
45.353522	1950.690280	18.943539
45.698703	1931.446182	18.948557
45.364947	1943.632229	18.953575
45.459531	1973.677583	18.958592
45.825905	1973.939655	18.963610
45.740428	1975.714018	18.968627
46.132007	1971.878700	18.973645
45.845402	1975.389325	18.978663
46.166085	1979.882268	18.983680
46.513832	1992.438717	18.988698
45.960979	1982.605200	18.993715
46.302134	1952.895008	18.998733
46.141975	1976.062516	19.003751
46.351185	1974.215725	19.008768
46.346288	1966.370708	19.013786
46.205694	1985.383123	19.018803
45.893033	1971.340724	19.023821
46.159847	1993.730454	19.028839
46.267335	2007.093009	19.033856
46.571049	1994.603643	19.038874
45.956943	1989.958017	19.043891
46.948484	1980.049674	19.048909
46.672865	2000.367743	19.053927
46.747959	2008.965284	19.058944
47.305575	1997.306336	19.063962
47.031466	1995.262296	19.068979
47.250878	2005.361194	19.073997
47.088414	2017.045263	19.079015
47.021959	2005.927838	19.084032
47.252500	1995.342337	19.089050
47.034373	1995.139980	19.094067
47.198173	2005.067787	19.099085
47.182230	1992.929713	19.104103
46.859711	1986.173396	19.109120
47.068551	1978.197795	19.114138
47.016394	1991.617422	19.119155
47.127248	1999.243284	19.124173
47.052965	2003.491421	19.129191
47.241330	2011.883765	19.134208
47.779192	2012.951204	19.139226
47.349070	2031.902191	19.144243
47.529977	2029.611039	19.149261
47.574377	2023.859919	19.154279
47.610785	2020.978587	19.159296
47.862550	2032.719982	19.164314
47.535738	2027.686971	19.169331
47.876055	2021.554140	19.174349
47.775277	2034.401729	19.179367
47.783405	2019.566058	19.184384
47.960478	2012.251081	19.189402
47.698397	2028.941246	19.194419
48.105252	2051.034936	19.199437
48.145453	2060.886666	19.204455
48.219193	2040.949330	19.209472
48.544881	2052.523632	19.214490
48.047575	2063.661308	19.219507
48.638754	2046.717032	19.224525
48.509575	2045.245482	19.229543
48.582240	2050.197366	19.234560
48.860887	2048.930420	19.239578
48.621734	2028.967752	19.244595
48.559231	2036.076415	19.249613
48.657793	2026.643498	19.254631
48.526551	2011.729309	19.259648
48.824015	2005.210824	19.264666
48.536062	2020.952776	19.269683
48.481807	2051.887482	19.274701
48.730861	2048.302722	19.279719
48.537028	2026.583381	19.284736
48.806589	2044.181294	19.289754
48.737758	2053.550144	19.294771
48.662818	2036.808653	19.299789
48.987769	2035.481507	19.304807
48.614033	2045.464806	19.309824
48.901870	2062.135578	19.314842
48.842846	2073.533060	19.319859
49.118851	2067.985438	19.324877
49.080226	2059.307124	19.329895
48.726032	2071.543590	19.334912
49.287214	2073.288158	19.339930
48.969530	2073.538786	19.344947
49.143540	2101.453048	19.349965
49.658868	2093.339750	19.354983
49.897579	2090.453808	19.360000
50.027995	2085.329576	19.365018
49.743307	2105.362128	19.370035
50.015073	2110.063748	19.375053
50.103016	2094.097202	19.380071
49.927386	2070.285404	19.385088
50.037639	2070.540303	19.390106
49.753936	2075.698596	19.395123
50.002450	2075.802227	19.400141
50.323684	2098.590326	19.405159
50.038059	2093.914300	19.410176
50.287781	2090.595219	19.415194
49.593391	2095.417027	19.420211
50.133498	2107.112996	19.425229
50.103609	2092.526604	19.430247
50.036381	2095.641817	19.435264
50.367943	2086.851635	19.440282
50.262007	2104.327054	19.445299
50.186148	2091.207053	19.450317
50.366556	2096.685143	19.455335
50.485451	2121.762311	19.460352
50.814595	2106.122758	19.465370
50.698248	2109.739900	19.470387
51.072837	2116.052093	19.475405
51.117109	2134.711269	19.480423
50.859272	2110.232898	19.485440
51.096379	2090.981169	19.490458
50.902269	2093.892389	19.495475
50.617886	2110.273687	19.500493
50.906378	2105.885493	19.505511
50.693879	2129.011889	19.510528
50.693969	2127.629284	19.515546
50.875023	2110.462605	19.520563
51.071918	2110.079972	19.525581
50.970399	2112.578329	19.530599
51.242002	2136.964954	19.535616
51.813197	2127.695366	19.540634
51.688642	2141.835523	19.545651
51.585763	2141.933059	19.550669
51.965546	2115.844266	19.555687
51.529650	2121.543576	19.560704
51.771736	2115.460006	19.565722
51.491440	2100.793254	19.570739
51.406039	2108.502478	19.575757
52.027096	2117.041647	19.580775
51.611445	2150.694162	19.585792
51.879982	2126.517888	19.590810
51.654416	2118.462255	19.595827
52.061543	2126.776296	19.600845
51.933223	2130.052470	19.605863
51.811372	2152.203660	19.610880
51.826265	2136.994973	19.615898
52.146102	2129.724250	19.620915
52.038650	2139.299892	19.625933
52.359569	2139.312340	19.630951
52.216533	2146.404446	19.635968
52.160938	2145.594131	19.640986
52.537337	2157.771836	19.646003
52.237891	2177.853862	19.651021
52.677816	2170.570557	19.656039
52.589235	2164.616399	19.661056
52.582536	2159.818585	19.666074
52.663404	2166.045895	19.671091
52.550690	2162.245052	19.676109
52.727068	2157.582213	19.681127
52.629100	2154.699246	19.686144
52.493377	2165.367475	19.691162
52.904106	2166.635332	19.696179
52.979678	2183.434406	19.701197
52.825002	2171.839989	19.706215
52.922947	2195.206768	19.711232
53.328725	2183.266230	19.716250
53.074428	2199.621198	19.721267
52.907318	2191.570432	19.726285
53.121460	2183.539430	19.731303
53.060923	2209.016011	19.736320
53.298781	2199.463824	19.741338
53.484939	2194.322866	19.746355
53.794375	2200.267284	19.751373
53.761081	2210.913305	19.756391
53.705683	2213.308108	19.761408
53.836378	2208.084692	19.766426
53.940230	2185.223309	19.771443
53.981963	2201.996308	19.776461
53.794295	2180.484749	19.781479
53.819229	2207.734687	19.786496
54.075327	2223.122126	19.791514
54.337511	2204.753557	19.796531
54.383568	2195.858451	19.801549
54.013536	2187.146556	19.806567
53.706813	2215.383139	19.811584
54.155622	2203.247417	19.816602
54.317500	2204.626071	19.821619
54.402959	2207.721882	19.826637
54.586874	2216.178547	19.831655
54.411431	2222.344315	19.836672
54.524631	2205.394022	19.841690
54.760612	2199.962889	19.846707
54.101311	2220.097153	19.851725
54.559648	2221.566166	19.856743
54.431552	2214.940584	19.861760
54.543551	2199.491713	19.866778
54.778794	2214.616494	19.871795
54.834491	2246.874629	19.876813
54.892466	2239.994803	19.881831
54.969616	2242.297641	19.886848
54.929299	2247.650280	19.891866
54.907009	2236.206547	19.896883
54.845012	2229.480975	19.901901
54.991468	2233.517139	19.906919
54.874577	2247.832279	19.911936
55.097123	2237.267221	19.916954
55.359797	2236.002605	19.921971
55.105560	2270.742693	19.926989
55.306038	2275.771543	19.932007
55.410747	2264.676819	19.937024
55.461689	2263.991978	19.942042
55.596747	2269.685858	19.947059
55.354052	2280.882583	19.952077
55.433146	2283.426208	19.957095
55.252993	2269.963407	19.962112
55.869147	2295.830294	19.967130
56.094508	2292.154330	19.972147
55.719034	2291.045941	19.977165
56.129606	2289.058770	19.982183
56.183262	2280.438986	19.987200
56.142549	2294.038943	19.992218
56.538018	2307.606788	19.997235
56.233877	2308.664200	20.002253
56.485078	2294.834084	20.007271
56.467491	2291.558640	20.012288
56.537183	2288.593523	20.017306
56.712783	2270.778167	20.022323
56.697832	2273.703017	20.027341
56.861006	2284.594331	20.032359
56.508395	2289.308548	20.037376
56.716805	2280.092225	20.042394
56.665546	2285.136304	20.047411
56.501354	2298.467741	20.052429
56.896164	2281.809257	20.057447
56.804260	2275.788293	20.062464
56.871291	2291.194939	20.067482
56.998247	2285.267705	20.072499
56.964326	2270.096180	20.077517
56.753758	2288.693243	20.082535
56.923535	2294.676817	20.087552
56.801451	2309.529594	20.092570
57.035160	2299.898123	20.097587
57.145826	2316.741634	20.102605
57.242853	2311.871129	20.107623
57.260059	2311.957285	20.112640
57.634759	2328.001989	20.117658
57.716101	2323.955984	20.122675
57.391261	2309.532772	20.127693
57.850072	2301.055440	20.132711
57.815650	2310.223419	20.137728
57.671395	2329.351806	20.142746
57.930040	2325.594757	20.147763
58.025711	2322.460406	20.152781
57.659086	2311.443928	20.157799
57.889365	2336.963890	20.162816
57.839314	2342.407526	20.167834
58.256989	2335.082061	20.172851
58.148650	2331.974926	20.177869
58.247248	2326.318460	20.182887
58.327257	2324.292224	20.187904
58.122452	2337.021648	20.192922
58.074240	2317.694067	20.197939
58.554917	2339.499448	20.202957
58.300313	2358.219797	20.207975
58.793489	2353.760118	20.212992
58.671996	2361.022553	20.218010
58.584722	2361.049216	20.223027
59.043259	2347.258008	20.228045
59.055877	2353.340201	20.233063
59.128546	2340.448845	20.238080
58.929374	2340.182829	20.243098
59.136737	2357.410931	20.248115
59.245931	2348.764021	20.253133
59.278302	2349.453871	20.258151
59.366015	2353.916832	20.263168
59.403709	2355.145282	20.268186
59.491734	2338.106596	20.273203
58.797256	2359.571833	20.278221
59.587880	2347.346942	20.283239
59.131784	2351.120561	20.288256
59.179651	2344.263811	20.293274
59.729135	2336.702033	20.298291
59.700889	2355.947284	20.303309
59.310980	2341.648161	20.308327
59.390612	2337.005879	20.313344
59.496511	2360.437530	20.318362
59.916697	2384.364240	20.323379
59.891497	2380.195297	20.328397
59.787349	2369.461729	20.333415
60.057725	2369.602885	20.338432
59.899481	2375.193326	20.343450
60.494042	2357.648347	20.348467
59.725966	2362.206473	20.353485
59.790231	2381.805307	20.358503
60.132745	2396.917561	20.363520
60.449192	2397.993079	20.368538
60.503830	2388.206725	20.373555
60.586922	2409.231977	20.378573
60.708103	2412.377036	20.383591
60.578211	2402.093297	20.388608
60.288528	2390.793815	20.393626
60.952713	2392.348791	20.398643
60.833240	2401.648380	20.403661
60.798411	2386.576677	20.408679
60.880945	2400.800943	20.413696
60.564228	2418.351307	20.418714
61.006869	2421.005326	20.423731
61.154288	2430.919189	20.428749
61.183568	2422.910147	20.433767
61.298810	2418.802619	20.438784
61.122668	2426.974563	20.443802
61.669224	2413.980040	20.448819
61.907420	2425.283596	20.453837
61.816137	2408.120550	20.458855
62.039811	2398.409193	20.463872
61.883142	2422.960139	20.468890
62.017957	2412.778691	20.473907
61.926871	2411.249342	20.478925
61.653911	2419.854340	20.483943
61.891123	2417.353958	20.488960
61.479526	2404.359924	20.493978
62.005389	2411.250099	20.498995
61.819145	2432.176211	20.504013
61.657121	2422.780305	20.509031
62.268896	2400.192290	20.514048
61.913032	2407.270087	20.519066
62.307756	2435.053027	20.524083
62.050634	2454.074453	20.529101
62.295135	2445.628323	20.534119
62.529051	2438.882104	20.539136
62.210300	2448.676388	20.544154
62.662451	2435.653359	20.549171
62.390670	2442.789510	20.554189
62.526259	2433.029115	20.559207
62.804657	2444.920830	20.564224
62.600857	2484.798712	20.569242
62.911572	2490.105041	20.574259
62.980538	2467.214560	20.579277
62.990748	2456.871025	20.584295
63.129997	2475.023757	20.589312
63.199736	2489.198259	20.594330
63.502699	2469.289704	20.599347
63.488807	2452.766081	20.604365
63.294428	2459.568634	20.609383
63.053580	2476.872509	20.614400
63.018232	2490.946286	20.619418
63.597418	2472.814241	20.624435
63.214680	2465.478875	20.629453
63.390279	2497.066249	20.634471
63.880076	2494.880754	20.639488
63.717748	2494.863331	20.644506
63.796394	2505.101944	20.649523
63.600442	2508.233099	20.654541
63.888322	2489.191642	20.659559
63.994847	2488.417501	20.664576
64.186378	2509.568650	20.669594
63.884615	2495.211714	20.674611
63.859535	2485.761649	20.679629
63.661555	2519.367584	20.684647
63.779051	2511.531292	20.689664
63.996531	2522.998949	20.694682
64.263045	2537.605476	20.699699
64.448968	2523.598569	20.704717
64.395238	2524.417991	20.709735
64.926374	2547.230529	20.714752
64.649255	2555.439697	20.719770
64.960683	2547.881726	20.724787
64.895878	2556.558294	20.729805
65.006719	2557.212159	20.734823
65.135977	2532.191858	20.739840
65.219844	2548.542490	20.744858
65.093136	2563.701150	20.749875
65.156862	2549.705161	20.754893
65.487511	2538.199929	20.759911
65.594285	2545.016919	20.764928
65.717985	2557.097646	20.769946
65.522951	2561.384195	20.774963
65.701516	2541.001886	20.779981
65.202300	2532.014926	20.784999
65.766528	2529.866528	20.790016
65.963368	2531.823698	20.795034
65.794527	2537.528333	20.800051
65.642971	2533.932507	20.805069
65.626679	2531.879644	20.810087
66.076163	2526.415479	20.815104
65.954832	2530.239318	20.820122
66.033502	2534.071048	20.825139
65.746633	2551.950242	20.830157
65.971510	2579.938256	20.835175
66.050020	2561.069870	20.840192
65.751161	2542.306574	20.845210
65.784296	2573.386822	20.850227
66.108066	2578.997869	20.855245
66.310078	2595.745107	20.860263
66.779693	2596.109801	20.865280
66.606188	2591.035525	20.870298
66.724729	2583.529092	20.875315
66.925422	2591.121804	20.880333
66.768706	2603.309329	20.885351
67.271590	2592.463290	20.890368
67.017079	2589.991189	20.895386
67.570182	2576.349087	20.900403
67.104839	2582.309987	20.905421
66.901871	2595.109192	20.910439
67.060437	2583.043079	20.915456
67.202556	2614.379376	20.920474
67.428132	2627.927162	20.925491
67.477384	2613.239513	20.930509
67.712121	2617.049214	20.935527
67.616027	2625.652656	20.940544
67.844482	2619.544176	20.945562
67.785082	2610.469139	20.950579
67.606510	2629.004641	20.955597
67.604835	2614.999718	20.960615
67.630358	2608.540776	20.965632
67.661979	2618.654775	20.970650
67.795107	2635.254211	20.975667
68.220367	2634.956057	20.980685
68.018346	2629.429460	20.985703
68.149768	2616.428967	20.990720
68.205112	2637.122551	20.995738
68.453630	2650.008196	21.000755
68.469915	2627.911501	21.005773
68.491707	2641.126884	21.010791
68.643549	2637.658432	21.015808
68.499455	2636.135458	21.020826
68.433137	2632.445614	21.025843
68.663958	2646.971148	21.030861
69.020332	2652.264872	21.035879
68.977724	2655.030411	21.040896
69.149862	2679.762634	21.045914
69.128700	2666.285810	21.050931
69.767850	2644.962811	21.055949
69.568352	2669.708011	21.060967
69.490390	2675.692324	21.065984
69.538748	2655.985813	21.071002
69.396407	2642.565248	21.076019
69.558307	2642.658988	21.081037
69.237443	2660.414023	21.086055
69.540201	2655.170881	21.091072
69.580047	2647.724068	21.096090
69.223493	2673.987335	21.101107
69.655139	2657.007640	21.106125
69.632869	2659.230724	21.111143
70.031962	2669.269469	21.116160
70.113582	2693.171516	21.121178
69.738812	2680.433527	21.126195
70.230444	2671.352427	21.131213
70.353521	2690.756924	21.136231
70.298192	2697.818848	21.141248
70.316592	2686.538700	21.146266
70.506567	2678.829697	21.151283
70.609205	2672.799065	21.156301
70.504626	2693.936218	21.161319
70.545972	2684.216823	21.166336
70.725335	2675.698667	21.171354
70.469953	2677.406022	21.176371
70.928534	2704.066458	21.181389
70.739071	2713.923589	21.186407
70.757580	2694.512866	21.191424
70.743015	2704.817795	21.196442
70.729166	2687.590861	21.201459
71.126302	2706.653087	21.206477
70.858727	2739.261105	21.211495
70.999630	2729.426819	21.216512
71.181781	2729.111954	21.221530
71.008501	2718.271866	21.226547
71.595099	2750.454548	21.231565
71.755499	2777.679668	21.236583
71.618496	2759.354652	21.241600
71.937679	2740.066802	21.246618
71.709742	2742.890143	21.251635
72.438807	2748.822416	21.256653
72.264679	2770.814161	21.261671
72.241233	2749.325350	21.266688
72.566499	2734.843122	21.271706
72.213420	2747.546803	21.276723
72.568564	2756.945122	21.281741
72.445457	2741.146225	21.286759
72.494639	2730.389626	21.291776
72.705671	2743.997981	21.296794
72.893721	2750.043469	21.301811
72.772843	2738.197600	21.306829
72.340830	2745.261169	21.311847
72.391170	2761.429404	21.316864
72.346480	2753.327703	21.321882
72.503238	2749.106943	21.326899
72.843405	2753.794015	21.331917
72.969148	2775.534472	21.336935
72.953663	2786.278130	21.341952
72.791897	2769.780570	21.346970
72.742329	2769.707904	21.351987
73.068535	2793.954679	21.357005
73.157574	2817.453583	21.362023
73.469009	2806.722286	21.367040
73.680671	2793.246243	21.372058
73.832823	2793.776772	21.377075
74.316144	2807.823195	21.382093
74.214159	2811.961778	21.387111
74.031544	2805.700708	21.392128
74.454435	2800.731524	21.397146
74.356564	2808.195947	21.402163
74.474474	2787.314939	21.407181
74.237063	2806.716758	21.412199
74.210451	2805.639645	21.417216
74.449394	2790.664217	21.422234
74.378608	2783.541681	21.427251
74.541649	2799.121725	21.432269
74.903221	2791.459694	21.437287
74.458104	2790.645609	21.442304
74.647708	2781.594080	21.447322
74.222432	2793.101428	21.452339
74.726829	2790.512747	21.457357
74.811358	2785.474103	21.462375
75.071108	2802.070510	21.467392
75.114553	2821.677085	21.472410
74.863387	2823.359550	21.477427
75.088356	2820.317498	21.482445
75.123926	2819.989063	21.487463
75.468358	2805.155421	21.492480
75.409241	2809.988400	21.497498
75.264307	2821.203020	21.502515
75.208743	2815.553151	21.507533
75.296045	2829.576069	21.512551
75.463404	2852.636944	21.517568
75.999671	2834.270459	21.522586
75.775973	2849.463929	21.527603
75.785712	2850.350824	21.532621
75.868447	2855.997866	21.537639
75.928204	2848.339425	21.542656
76.311848	2848.030629	21.547674
75.815536	2873.790233	21.552691
76.400627	2873.227901	21.557709
76.074589	2869.486047	21.562727
76.564412	2886.119321	21.567744
76.793937	2872.672535	21.572762
76.806435	2858.225341	21.577779
76.763894	2855.150135	21.582797
76.718637	2861.289330	21.587815
76.627207	2867.599128	21.592832
76.811478	2872.367109	21.597850
77.003911	2881.021626	21.602867
77.424093	2883.354087	21.607885
77.385403	2890.058670	21.612903
77.212423	2902.974813	21.617920
77.487371	2890.813451	21.622938
77.734450	2881.364031	21.627955
77.261174	2873.489169	21.632973
77.582316	2890.127292	21.637991
77.377723	2903.139002	21.643008
77.465653	2872.872499	21.648026
77.482308	2877.939600	21.653043
77.792731	2880.227411	21.658061
77.803700	2895.184340	21.663079
77.862403	2915.255579	21.668096
77.954309	2906.052032	21.673114
78.092703	2908.631429	21.678131
77.667387	2907.757970	21.683149
78.153413	2936.525817	21.688167
77.816777	2922.704490	21.693184
78.232258	2912.085636	21.698202
78.430798	2943.357185	21.703219
78.222417	2957.964248	21.708237
78.438180	2951.349530	21.713255
78.757091	2944.283770	21.718272
78.792620	2945.930880	21.723290
78.588142	2955.897916	21.728307
78.720858	2953.058855	21.733325
78.937532	2972.789538	21.738343
79.039269	2999.998763	21.743360
79.073727	2980.642124	21.748378
79.403341	2973.614537	21.753395
79.511424	2978.461471	21.758413
79.454186	2972.797452	21.763431
79.053057	2985.622443	21.768448
79.838662	2980.508630	21.773466
79.554219	3002.964747	21.778483
79.661073	2996.607741	21.783501
80.027272	2976.533968	21.788519
79.868269	2988.344464	21.793536
80.429989	2999.951438	21.798554
80.389157	2999.384080	21.803571
80.604636	2983.643932	21.808589
80.621109	2981.020900	21.813607
80.441099	3002.988951	21.818624
80.559472	2990.653802	21.823642
80.444511	2991.502459	21.828659
80.173094	2985.615197	21.833677
80.502026	2988.864808	21.838695
80.410503	3026.861595	21.843712
80.726561	3016.793680	21.848730
80.611840	3009.949329	21.853747
80.716525	3024.408673	21.858765
80.948593	3030.697952	21.863783
80.766689	3034.821457	21.868800
80.945971	3040.463439	21.873818
81.328663	3054.998315	21.878835
81.446687	3037.138248	21.883853
81.521278	3032.501905	21.888871
81.461527	3057.413391	21.893888
81.612215	3068.139235	21.898906
81.561388	3053.396453	21.903923
81.732904	3046.587258	21.908941
82.079548	3071.127712	21.913959
82.241095	3061.894260	21.918976
82.621663	3081.883203	21.923994
82.822774	3070.388550	21.929011
82.428546	3038.328583	21.934029
82.679616	3026.985136	21.939047
82.663704	3040.605470	21.944064
82.519007	3047.946070	21.949082
82.579729	3045.840259	21.954099
82.442514	3021.449544	21.959117
82.579446	3044.414173	21.964135
82.728006	3067.288144	21.969152
82.849799	3062.519992	21.974170
82.935109	3062.996623	21.979187
83.185610	3072.593706	21.984205
83.289511	3064.341319	21.989223
82.985389	3071.032368	21.994240
83.101652	3062.214816	21.999258
82.921777	3062.304018	22.004275
83.186927	3068.190059	22.009293
83.611153	3079.078560	22.014311
83.307784	3102.792528	22.019328
83.493486	3098.711164	22.024346
83.670186	3094.567517	22.029363
83.423924	3086.251537	22.034381
83.518845	3087.462716	22.039399
83.297219	3109.699577	22.044416
83.489591	3102.842428	22.049434
83.743259	3110.510689	22.054451
83.614956	3110.538424	22.059469
84.202075	3132.120478	22.064487
84.147932	3139.292041	22.069504
84.185453	3171.703133	22.074522
84.373184	3156.264016	22.079539
84.140943	3140.404995	22.084557
84.777933	3164.507310	22.089575
84.865011	3192.582392	22.094592
84.996911	3175.052119	22.099610
85.148195	3180.736374	22.104627
84.800160	3192.769186	22.109645
85.191728	3176.660805	22.114663
85.407358	3184.920365	22.119680
85.345055	3178.322171	22.124698
85.620697	3169.909473	22.129715
85.661962	3175.296979	22.134733
85.976639	3178.491709	22.139751
85.472400	3185.307007	22.144768
85.585759	3193.002234	22.149786
86.080589	3200.180543	22.154803
85.956810	3196.855531	22.159821
86.045868	3202.809890	22.164839
86.046334	3194.484181	22.169856
86.207158	3195.595118	22.174874
86.557839	3209.252258	22.179891
86.590902	3206.989399	22.184909
86.669985	3189.176925	22.189927
86.574522	3179.279060	22.194944
86.305648	3195.018661	22.199962
86.427593	3213.608542	22.204979
86.849241	3198.458056	22.209997
87.115188	3223.223285	22.215015
87.179836	3237.479821	22.220032
87.059339	3225.039679	22.225050
87.383341	3206.460021	22.230067
87.240401	3213.363054	22.235085
87.426482	3228.155165	22.240103
87.402527	3222.729229	22.245120
87.327876	3217.948809	22.250138
87.642053	3212.981515	22.255155
87.299749	3228.433907	22.260173
87.702344	3243.429206	22.265191
87.453349	3245.299919	22.270208
87.732304	3226.456449	22.275226
87.900488	3226.935728	22.280243
88.106056	3251.083290	22.285261
88.284219	3247.278301	22.290279
88.163229	3256.617824	22.295296
88.390995	3255.100854	22.300314
88.837798	3264.626844	22.305331
88.830045	3282.776084	22.310349
88.831107	3268.765586	22.315367
88.875342	3254.675928	22.320384
88.626753	3263.896397	22.325402
88.830693	3281.269787	22.330419
89.040281	3273.196261	22.335437
89.521807	3254.654878	22.340455
89.171574	3256.936965	22.345472
89.183666	3268.921548	22.350490
89.374285	3271.740973	22.355507
89.259113	3266.208454	22.360525
89.394073	3243.090780	22.365543
89.315702	3267.527387	22.370560
89.115049	3276.142957	22.375578
89.468782	3283.273958	22.380595
89.693162	3286.889299	22.385613
89.773008	3280.988955	22.390631
89.652241	3299.230109	22.395648
89.411238	3317.032931	22.400666
89.893822	3309.639596	22.405683
89.879687	3321.522659	22.410701
89.890654	3327.561420	22.415719
90.165576	3336.187603	22.420736
90.264711	3355.240237	22.425754
90.786941	3361.399430	22.430771
90.864101	3338.536023	22.435789
90.978643	3332.015814	22.440807
90.881580	3341.429970	22.445824
90.974987	3345.897199	22.450842
91.268818	3330.974968	22.455859
91.141672	3338.483063	22.460877
91.432074	3352.977375	22.465895
91.824701	3375.124337	22.470912
91.712735	3374.610054	22.475930
91.896304	3373.456640	22.480947
91.579118	3389.400072	22.485965
91.679610	3381.540560	22.490983
91.437726	3357.011310	22.496000
91.728396	3366.001998	22.501018
91.658079	3376.641557	22.506035
91.928048	3386.719628	22.511053
92.055544	3396.904704	22.516071
92.322739	3381.867152	22.521088
91.968365	3392.965234	22.526106
92.782264	3394.473145	22.531123
92.614645	3388.724270	22.536141
92.655870	3378.238783	22.541159
92.673659	3393.702697	22.546176
92.812349	3413.699563	22.551194
92.913500	3406.754410	22.556211
93.135532	3427.001670	22.561229
93.250725	3428.739595	22.566247
93.536622	3412.139227	22.571264
92.877687	3416.828619	22.576282
93.487473	3420.372631	22.581299
93.616240	3421.941399	22.586317
93.429284	3411.389077	22.591335
93.492824	3414.580675	22.596352
93.622568	3440.484008	22.601370
94.103539	3434.914333	22.606387
94.173888	3447.868668	22.611405
94.150398	3453.210087	22.616423
94.616223	3447.007930	22.621440
94.240344	3444.148695	22.626458
94.400825	3444.836519	22.631475
94.036045	3431.855330	22.636493
94.110639	3435.189777	22.641511
94.502621	3472.984748	22.646528
94.668345	3476.564161	22.651546
94.673975	3472.842543	22.656563
94.738251	3482.569661	22.661581
94.633972	3481.560054	22.666599
94.931478	3480.201798	22.671616
94.737906	3489.550502	22.676634
94.993555	3489.783075	22.681651
95.178383	3500.111882	22.686669
95.183180	3493.190682	22.691687
95.471125	3483.691824	22.696704
95.394434	3511.316243	22.701722
95.661147	3508.490762	22.706739
95.527101	3499.039776	22.711757
95.695334	3505.511240	22.716775
95.870790	3517.930989	22.721792
95.696240	3531.922231	22.726810
95.891045	3531.280486	22.731827
96.118568	3539.708532	22.736845
96.445731	3548.874975	22.741863
96.733212	3539.443673	22.746880
96.647563	3550.364010	22.751898
96.532727	3565.030001	22.756915
96.656777	3536.459629	22.761933
96.698355	3525.122484	22.766951
97.298173	3545.702912	22.771968
96.970311	3565.695776	22.776986
97.097660	3567.186650	22.782003
97.195431	3554.211990	22.787021
97.113958	3566.771470	22.792039
97.401609	3567.283377	22.797056
97.766043	3558.227701	22.802074
97.606409	3560.771225	22.807091
97.738211	3561.889938	22.812109
97.757618	3591.475225	22.817127
98.130857	3608.920017	22.822144
97.996169	3605.218601	22.827162
98.130320	3580.467030	22.832179
98.403794	3581.428094	22.837197
98.418595	3595.682372	22.842215
98.289550	3603.828062	22.847232
98.234481	3594.229135	22.852250
98.642878	3601.113674	22.857267
98.656414	3618.878719	22.862285
98.586581	3630.374405	22.867303
98.930495	3613.211130	22.872320
98.555734	3626.811362	22.877338
98.817327	3647.048437	22.882355
99.179381	3657.859048	22.887373
99.416590	3648.112391	22.892391
99.389018	3642.108999	22.897408
99.208664	3653.415304	22.902426
99.611585	3659.993514	22.907443
99.708567	3649.172279	22.912461
99.768334	3665.415292	22.917479
100.047653	3680.790022	22.922496
100.109023	3675.162048	22.927514
100.264025	3674.916215	22.932531
100.520433	3676.560761	22.937549
100.350464	3678.823160	22.942567
100.606494	3681.039378	22.947584
100.458421	3680.723358	22.952602
100.491255	3657.456205	22.957619
100.700779	3650.776084	22.962637
100.593208	3677.697692	22.967655
100.824457	3701.207710	22.972672
100.754831	3696.452293	22.977690
101.095651	3688.127159	22.982707
101.213201	3694.906464	22.987725
101.084603	3709.703991	22.992743
101.400334	3717.082795	22.997760
101.426702	3724.968043	23.002778
101.895598	3702.668651	23.007795
102.231342	3711.599145	23.012813
102.116165	3732.513110	23.017831
102.314242	3719.594763	23.022848
102.181983	3698.820195	23.027866
102.529231	3713.270023	23.032883
102.281080	3701.717650	23.037901
102.154425	3696.994293	23.042919
102.690224	3706.557228	23.047936
102.417326	3716.881111	23.052954
102.386255	3705.660161	23.057971
102.531735	3723.988915	23.062989
102.277010	3714.427431	23.068007
102.820607	3700.063923	23.073024
102.732838	3730.445276	23.078042
102.784058	3741.791524	23.083059
103.201152	3730.735264	23.088077
102.902591	3739.782396	23.093095
103.152656	3743.712869	23.098112
103.581061	3770.021112	23.103130
103.620904	3763.545149	23.108147
103.676032	3775.983217	23.113165
103.539264	3780.525612	23.118183
103.938003	3767.959867	23.123200
103.981759	3765.117445	23.128218
104.098629	3770.062776	23.133235
104.537302	3784.960917	23.138253
104.433577	3805.414066	23.143271
104.537306	3792.978735	23.148288
104.503827	3785.406688	23.153306
104.735608	3800.149871	23.158323
104.688899	3798.917753	23.163341
104.727922	3800.696454	23.168359
104.861215	3788.728256	23.173376
104.967583	3805.442620	23.178394
105.117550	3823.668591	23.183411
105.269034	3798.162088	23.188429
105.384232	3811.378983	23.193447
105.632169	3836.388708	23.198464
105.499477	3819.135467	23.203482
105.570023	3824.467971	23.208499
105.966006	3845.726534	23.213517
105.876788	3844.835665	23.218535
106.034450	3838.018768	23.223552
105.910323	3850.177875	23.228570
106.146609	3838.019207	23.233587
106.435381	3843.231806	23.238605
106.267612	3865.418729	23.243623
106.397352	3878.597062	23.248640
106.615226	3889.874545	23.253658
106.516465	3869.974667	23.258675
106.833173	3853.578761	23.263693
106.844722	3878.500064	23.268711
107.459687	3903.278395	23.273728
107.469932	3892.884484	23.278746
107.493935	3906.265930	23.283763
107.452804	3903.273740	23.288781
107.521933	3895.775427	23.293799
107.464763	3899.553177	23.298816
107.635414	3915.129943	23.303834
107.764862	3897.516783	23.308851
107.924957	3902.312897	23.313869
107.694456	3922.970602	23.318887
108.194286	3937.017498	23.323904
107.972784	3936.071913	23.328922
107.832904	3935.762801	23.333939
108.333413	3926.787372	23.338957
108.420608	3951.838017	23.343975
108.540705	3946.481129	23.348992
108.452202	3941.635455	23.354010
108.666884	3955.842077	23.359027
109.222091	3980.333967	23.364045
109.265580	3988.734601	23.369063
109.311242	3971.533210	23.374080
109.418027	3972.321067	23.379098
109.469983	3992.117673	23.384115
109.825016	3993.840046	23.389133
109.676262	3984.662436	23.394151
110.010928	3956.682434	23.399168
109.903648	3974.868025	23.404186
109.714362	3958.255045	23.409203
110.400806	3955.709912	23.414221
110.094139	3978.293548	23.419239
110.238960	3987.112845	23.424256
110.001719	3988.016601	23.429274
110.014774	3995.357368	23.434291
110.211073	3990.883886	23.439309
110.161941	4029.017462	23.444327
110.315003	4037.463399	23.449344
110.735316	4033.987872	23.454362
110.509622	4067.754895	23.459379
110.720708	4066.377604	23.464397
111.211437	4070.321935	23.469415
111.206163	4067.503307	23.474432
111.300849	4093.956020	23.479450
111.337398	4096.618781	23.484467
111.835242	4073.847562	23.489485
111.789520	4088.328818	23.494503
111.849567	4103.517378	23.499520
112.624609	4102.849220	23.504538
112.148228	4101.120190	23.509555
112.693734	4084.549824	23.514573
112.861433	4097.276227	23.519591
113.232735	4106.234539	23.524608
113.742022	4094.821859	23.529626
113.466456	4076.330978	23.534643
113.562719	4051.309732	23.539661
113.393309	4053.024681	23.544679
113.663576	4041.031489	23.549696
113.695773	4034.350979	23.554714
113.407710	4074.001625	23.559731
113.534866	4054.447428	23.564749
113.794781	4051.445227	23.569767
113.745712	4055.059086	23.574784
113.747529	4036.716109	23.579802
113.539719	4069.519211	23.584819
113.931826	4071.498839	23.589837
113.862079	4083.811734	23.594855
113.656642	4105.686738	23.599872
114.432868	4095.269268	23.604890
114.266543	4095.813298	23.609907
114.272101	4099.533096	23.614925
114.210626	4130.868520	23.619943
114.050981	4130.217017	23.624960
114.418881	4128.076443	23.629978
114.594830	4139.781489	23.634995
114.569653	4166.800957	23.640013
114.568163	4186.936549	23.645031
114.855684	4194.065530	23.650048
115.832290	4207.085903	23.655066
115.530562	4215.479926	23.660083
115.587942	4198.374767	23.665101
115.908818	4217.444184	23.670119
115.647520	4223.867442	23.675136
115.950110	4204.024630	23.680154
115.822768	4215.307427	23.685171
116.294576	4244.437336	23.690189
116.298680	4238.884169	23.695207
116.380415	4243.846874	23.700224
116.763054	4244.883641	23.705242
116.561777	4249.613596	23.710259
117.000848	4220.609608	23.715277
116.993850	4253.872023	23.720295
116.998468	4264.115376	23.725312
117.342350	4262.038593	23.730330
117.152738	4259.293301	23.735347
117.246640	4246.776753	23.740365
117.515910	4254.473716	23.745383
117.308687	4278.730266	23.750400
117.936180	4279.487609	23.755418
117.908830	4276.648969	23.760435
118.071754	4283.869444	23.765453
118.392099	4275.701115	23.770471
118.197145	4287.422679	23.775488
118.472631	4291.121936	23.780506
118.289445	4288.838945	23.785523
118.678028	4261.750237	23.790541
118.605400	4299.782068	23.795559
118.543408	4306.716895	23.800576
118.939658	4296.700254	23.805594
118.590109	4313.152324	23.810611
118.816710	4318.245835	23.815629
119.132998	4314.950421	23.820647
119.191992	4326.639108	23.825664
119.362426	4337.783424	23.830682
119.483842	4358.169787	23.835699
119.806952	4361.754108	23.840717
119.794049	4352.963267	23.845735
119.500243	4373.886748	23.850752
120.103856	4378.325876	23.855770
119.873018	4390.544770	23.860787
120.289261	4377.653999	23.865805
120.509865	4381.634778	23.870823
120.460261	4401.994734	23.875840
120.524305	4416.871139	23.880858
120.671687	4424.055272	23.885875
120.929282	4406.098322	23.890893
121.157286	4409.707425	23.895911
121.426436	4426.202261	23.900928
121.601815	4416.468095	23.905946
121.568874	4404.886131	23.910963
121.723580	4425.837931	23.915981
122.330278	4444.103729	23.920999
122.614600	4448.450758	23.926016
122.645543	4421.040564	23.931034
122.109991	4413.612389	23.936051
122.295302	4438.557848	23.941069
123.056698	4412.100170	23.946087
122.776905	4430.271888	23.951104
122.773183	4434.664541	23.956122
122.542032	4431.732386	23.961139
122.526902	4446.079004	23.966157
123.110205	4434.129452	23.971175
122.820490	4434.502943	23.976192
123.033919	4459.242613	23.981210
123.043234	4462.688263	23.986227
123.398890	4460.322903	23.991245
123.348703	4475.190288	23.996263
122.990874	4465.922926	24.001280
123.266644	4483.866691	24.006298
123.538077	4485.750176	24.011315
123.354105	4518.119588	24.016333
123.986332	4519.071434	24.021351
123.862657	4527.977530	24.026368
124.197752	4534.454335	24.031386
124.091869	4539.352863	24.036403
124.727491	4556.841198	24.041421
124.767184	4559.525566	24.046439
125.466665	4545.608348	24.051456
125.720822	4535.741014	24.056474
125.440201	4554.841734	24.061491
125.211047	4557.485094	24.066509
125.610407	4541.186024	24.071527
125.777807	4551.837700	24.076544
125.898149	4541.026747	24.081562
125.903852	4533.051609	24.086579
125.937532	4539.745933	24.091597
126.098077	4549.626710	24.096615
126.012856	4560.514617	24.101632
126.421039	4545.513665	24.106650
126.313129	4553.163261	24.111667
126.025026	4568.617279	24.116685
126.111559	4582.574005	24.121703
126.254829	4600.140593	24.126720
126.713637	4593.548010	24.131738
126.635244	4599.827028	24.136755
126.952018	4624.508943	24.141773
127.120829	4626.648768	24.146791
127.439324	4617.164446	24.151808
127.693064	4614.626537	24.156826
127.870992	4628.454818	24.161843
127.677735	4644.284572	24.166861
128.087131	4645.302774	24.171879
127.783848	4645.181274	24.176896
127.868406	4664.044624	24.181914
127.961687	4660.447016	24.186931
128.124482	4671.704644	24.191949
128.565328	4686.596212	24.196967
128.284979	4692.846041	24.201984
128.603955	4680.086444	24.207002
128.962938	4702.981611	24.212019
129.133106	4724.744637	24.217037
129.455928	4713.493418	24.222055
129.287283	4731.236889	24.227072
129.679848	4722.378842	24.232090
129.411878	4699.988362	24.237107
129.754042	4714.579731	24.242125
129.920537	4737.764233	24.247143
129.823078	4749.339721	24.252160
130.279253	4725.075236	24.257178
130.487570	4719.642089	24.262195
129.904781	4732.741838	24.267213
130.557030	4759.817725	24.272231
130.788591	4758.695652	24.277248
131.018752	4756.187206	24.282266
131.234065	4761.833118	24.287283
130.896807	4775.882483	24.292301
131.059425	4755.214859	24.297319
130.965770	4769.633018	24.302336
131.305512	4788.535063	24.307354
131.215960	4805.982088	24.312371
131.111486	4797.263212	24.317389
131.410974	4801.607049	24.322407
131.474793	4822.250388	24.327424
131.821543	4828.943500	24.332442
131.817995	4825.421302	24.337459
132.030401	4850.455072	24.342477
132.159903	4862.751016	24.347495
132.366083	4865.978399	24.352512
132.898743	4867.375462	24.357530
133.173095	4867.093160	24.362547
133.121500	4896.839521	24.367565
133.256804	4879.625067	24.372583
133.294729	4877.340099	24.377600
133.240536	4885.521533	24.382618
133.802836	4862.416070	24.387635
133.473771	4869.463388	24.392653
133.912315	4885.635055	24.397671
134.012704	4911.758693	24.402688
133.890267	4912.083293	24.407706
134.396716	4905.065384	24.412723
134.185235	4914.704715	24.417741
134.581337	4901.461327	24.422759
134.349442	4902.500077	24.427776
134.782753	4926.602979	24.432794
134.882984	4941.809737	24.437811
134.740752	4949.493545	24.442829
135.442091	4934.737088	24.447847
135.313986	4914.638945	24.452864
135.065467	4920.462737	24.457882
135.362962	4934.530591	24.462899
135.477735	4945.876275	24.467917
135.729938	4954.611058	24.472935
135.879107	4965.804616	24.477952
135.776675	4948.249445	24.482970
136.662404	4955.694898	24.487987
136.231416	4981.359208	24.493005
136.889325	4995.435675	24.498023
136.654346	4988.710711	24.503040
136.678016	4962.438173	24.508058
136.989543	4964.814308	24.513075
136.671118	4979.640670	24.518093
136.976455	4993.308460	24.523111
137.467067	5013.488617	24.528128
137.315269	5019.403552	24.533146
137.332083	4998.099848	24.538163
137.135868	5010.106418	24.543181
137.716992	5018.112867	24.548199
137.727417	5020.198602	24.553216
137.656973	5042.162068	24.558234
138.185918	5053.677194	24.563251
137.795054	5070.822723	24.568269
137.935976	5065.822251	24.573287
138.484810	5072.070263	24.578304
138.815682	5077.338530	24.583322
138.953809	5092.196256	24.588339
138.694087	5115.941124	24.593357
138.963800	5105.167304	24.598375
139.077195	5102.984007	24.603392
139.254415	5127.149221	24.608410
139.537969	5134.618670	24.613427
139.664121	5150.723332	24.618445
139.763238	5147.539221	24.623463
140.190776	5156.501056	24.628480
140.229340	5150.382804	24.633498
140.603457	5153.893135	24.638515
140.574269	5162.758784	24.643533
140.897568	5156.874195	24.648551
140.939580	5168.484038	24.653568
140.768948	5184.122015	24.658586
140.961579	5167.088327	24.663603
140.648624	5175.846931	24.668621
140.917554	5193.999739	24.673639
140.952676	5193.414041	24.678656
141.099818	5213.424040	24.683674
141.261750	5234.616294	24.688691
141.563460	5249.010515	24.693709
141.967792	5245.638942	24.698727
141.980435	5250.740161	24.703744
142.206499	5259.565264	24.708762
142.754910	5247.347230	24.713779
142.469526	5254.175687	24.718797
142.853951	5274.594206	24.723815
143.215439	5256.442728	24.728832
143.040337	5261.635210	24.733850
143.442920	5256.137888	24.738867
143.709641	5278.600714	24.743885
143.860873	5295.605736	24.748903
143.830156	5283.833374	24.753920
143.734899	5273.889447	24.758938
143.962149	5277.732743	24.763955
143.916454	5290.248136	24.768973
143.745219	5277.784805	24.773991
144.249494	5270.280860	24.779008
144.205318	5301.854768	24.784026
144.038710	5305.332823	24.789043
144.210038	5314.843398	24.794061
144.411129	5314.646425	24.799079
145.196205	5341.725006	24.804096
144.924628	5361.103180	24.809114
144.697642	5351.812878	24.814131
145.154263	5375.709472	24.819149
145.302841	5379.203183	24.824167
145.239376	5372.097339	24.829184
145.243976	5390.979114	24.834202
145.519288	5414.776194	24.839219
145.466962	5432.237849	24.844237
145.603013	5428.890093	24.849255
146.059650	5441.925383	24.854272
146.224261	5478.195636	24.859290
146.612562	5461.830503	24.864307
146.778171	5477.778585	24.869325
146.711235	5499.203117	24.874343
147.329716	5490.512434	24.879360
147.254779	5492.817070	24.884378
147.614184	5498.558740	24.889395
147.413508	5509.335279	24.894413
147.819249	5514.053509	24.899431
147.982566	5503.508027	24.904448
148.386816	5518.776143	24.909466
148.586526	5525.141871	24.914483
148.545420	5526.877907	24.919501
148.553110	5509.197210	24.924519
148.712018	5518.723348	24.929536
148.803563	5546.147992	24.934554
149.067038	5549.951510	24.939571
149.069752	5536.302487	24.944589
149.217577	5535.523344	24.949607
149.450024	5554.459012	24.954624
149.380066	5584.924713	24.959642
149.585368	5564.966318	24.964659
149.884011	5563.945708	24.969677
150.132351	5582.395299	24.974695
150.559471	5597.451043	24.979712
150.706293	5608.077315	24.984730
150.739253	5605.669039	24.989747
150.839579	5586.954002	24.994765
150.566501	5612.099139	24.999783
150.901324	5593.246919	25.004800
150.993773	5596.349147	25.009818
151.215840	5616.987079	25.014835
151.412886	5606.033967	25.019853
151.489726	5601.543542	25.024871
151.863865	5616.537583	25.029888
151.504351	5631.408361	25.034906
151.383994	5636.213950	25.039923
151.774847	5662.865293	25.044941
151.862142	5662.300879	25.049959
152.327516	5672.646597	25.054976
152.437898	5683.969135	25.059994
152.505570	5679.660132	25.065011
152.465204	5678.679388	25.070029
152.360961	5699.558756	25.075047
152.580583	5698.079517	25.080064
152.578268	5728.077603	25.085082
153.002413	5744.145060	25.090099
153.251867	5727.756132	25.095117
153.416939	5742.295836	25.100135
153.770219	5760.526712	25.105152
153.912401	5777.230983	25.110170
153.881455	5781.743481	25.115187
154.405201	5781.449094	25.120205
154.161222	5812.870031	25.125223
154.446899	5795.481680	25.130240
154.659469	5805.648379	25.135258
154.882922	5824.194106	25.140275
155.262168	5812.652050	25.145293
154.935920	5830.990169	25.150311
155.254482	5856.236379	25.155328
155.714440	5851.848337	25.160346
156.055925	5843.959575	25.165363
156.200412	5857.173571	25.170381
155.893863	5853.313386	25.175399
156.154944	5864.268613	25.180416
156.136270	5898.967273	25.185434
156.553177	5888.711542	25.190451
156.589925	5882.479122	25.195469
156.328778	5905.156458	25.200487
156.834506	5918.464766	25.205504
157.028814	5925.380013	25.210522
156.948982	5939.875715	25.215539
157.338999	5939.121499	25.220557
157.298922	5947.265722	25.225575
157.783829	5939.199267	25.230592
157.928682	5983.106763	25.235610
158.072499	5986.499422	25.240627
158.458775	5973.242973	25.245645
158.579512	5980.360178	25.250663
158.904108	5981.490131	25.255680
158.831191	6007.827327	25.260698
158.893972	6001.686628	25.265715
159.041292	5997.540768	25.270733
159.408666	6011.333466	25.275751
159.791227	5994.784460	25.280768
159.773169	5993.477546	25.285786
159.942740	6029.269487	25.290803
160.178886	6034.014718	25.295821
160.095531	6035.994029	25.300839
160.354844	6027.637614	25.305856
160.143044	6031.015414	25.310874
160.405947	6029.336852	25.315891
160.691426	6050.842111	25.320909
160.560646	6076.532242	25.325927
160.592587	6072.801126	25.330944
160.863285	6067.601712	25.335962
160.952320	6070.466392	25.340979
161.271758	6091.534961	25.345997
161.333428	6121.513782	25.351015
161.584360	6107.366911	25.356032
161.662794	6106.205474	25.361050
161.783996	6126.650888	25.366067
162.169427	6144.021715	25.371085
162.141621	6160.992298	25.376103
162.695321	6153.932168	25.381120
162.876667	6166.148128	25.386138
163.011186	6180.128676	25.391155
163.304105	6168.686849	25.396173
163.445208	6164.400623	25.401191
163.229009	6173.162301	25.406208
163.421364	6189.107086	25.411226
163.427381	6188.944698	25.416243
163.988164	6206.550818	25.421261
163.726379	6199.250574	25.426279
163.927094	6216.557113	25.431296
163.871727	6217.895547	25.436314
164.114530	6228.186671	25.441331
164.364685	6252.528211	25.446349
164.262007	6275.490556	25.451367
164.515888	6271.548297	25.456384
164.580464	6281.502731	25.461402
164.805073	6298.957789	25.466419
165.012554	6302.507729	25.471437
165.492040	6332.978601	25.476455
165.442252	6336.702960	25.481472
165.859096	6339.013479	25.486490
165.590778	6368.389754	25.491507
166.211581	6369.040833	25.496525
166.301418	6377.708748	25.501543
166.570305	6402.050182	25.506560
166.866431	6395.006516	25.511578
166.987097	6384.385197	25.516595
167.425905	6408.583594	25.521613
167.016844	6430.880185	25.526631
167.836852	6413.808021	25.531648
167.941364	6419.053513	25.536666
167.477494	6434.476598	25.541683
168.415400	6433.273138	25.546701
168.087793	6437.050511	25.551719
168.516905	6437.046190	25.556736
169.068605	6421.888614	25.561754
169.098163	6435.481968	25.566771
169.336220	6435.757664	25.571789
169.350569	6430.944616	25.576807
169.478538	6420.419320	25.581824
170.019154	6446.931500	25.586842
169.858230	6470.456174	25.591859
170.100263	6465.347595	25.596877
170.238595	6446.456336	25.601895
170.338193	6467.440858	25.606912
170.414155	6450.262829	25.611930
170.239814	6462.549210	25.616947
170.552271	6469.670791	25.621965
170.255141	6484.021780	25.626983
170.443907	6488.198936	25.632000
170.861384	6505.512504	25.637018
170.729625	6518.645132	25.642035
171.094542	6528.228804	25.647053
170.874287	6555.556722	25.652071
171.295851	6537.982875	25.657088
171.235332	6570.399537	25.662106
171.316276	6598.284522	25.667123
171.666572	6600.370618	25.672141
171.881437	6611.558836	25.677159
172.045538	6630.789813	25.682176
172.771401	6648.623910	25.687194
172.287665	6657.457625	25.692212
172.777533	6680.841222	25.697229
173.037224	6686.610834	25.702247
173.435137	6684.790986	25.707264
173.799486	6691.099671	25.712282
173.671262	6718.962338	25.717300
173.880099	6702.937019	25.722317
174.389408	6735.773711	25.727335
174.070529	6741.614527	25.732352
174.542915	6722.938639	25.737370
174.515923	6736.761309	25.742388
174.775186	6743.500813	25.747405
175.058237	6762.348081	25.752423
175.046163	6774.612227	25.757440
175.238018	6787.190367	25.762458
175.231837	6783.190151	25.767476
175.347959	6793.811279	25.772493
175.351896	6802.223116	25.777511
175.792587	6795.225868	25.782528
175.905292	6826.648966	25.787546
176.010733	6826.350051	25.792564
176.564242	6840.057210	25.797581
176.972966	6860.453714	25.802599
177.245246	6848.433628	25.807616
176.918291	6845.776716	25.812634
177.222380	6864.321775	25.817652
177.124538	6879.626936	25.822669
177.766959	6887.448617	25.827687
177.791003	6876.874036	25.832704
178.129841	6879.441653	25.837722
177.809953	6922.195344	25.842740
177.957039	6919.705403	25.847757
178.310661	6910.076475	25.852775
178.237191	6926.399441	25.857792
178.613727	6936.899282	25.862810
178.620117	6969.337214	25.867828
179.078185	6969.185179	25.872845
179.298854	6983.075034	25.877863
179.132195	6998.375537	25.882880
179.585331	6996.771364	25.887898
179.821341	7023.131281	25.892916
180.166517	7035.552380	25.897933
180.143649	7032.283698	25.902951
180.288841	7018.315313	25.907968
180.743829	7042.289941	25.912986
180.690342	7072.019098	25.918004
181.050905	7073.247931	25.923021
181.258491	7083.048518	25.928039
181.254720	7082.412475	25.933056
181.628630	7083.191009	25.938074
181.449469	7095.109337	25.943092
181.759994	7120.816464	25.948109
182.195409	7121.200925	25.953127
181.989659	7119.195296	25.958144
182.901445	7127.718762	25.963162
182.501132	7163.488936	25.968180
182.841347	7148.997983	25.973197
183.093434	7142.396363	25.978215
183.332441	7179.528871	25.983232
183.545129	7188.300577	25.988250
183.643460	7182.837895	25.993268
183.589367	7181.597080	25.998285
184.120946	7198.276332	26.003303
184.097589	7205.632502	26.008320
184.501406	7202.561436	26.013338
184.317203	7230.405514	26.018356
184.478973	7246.810436	26.023373
184.577353	7250.522343	26.028391
184.807725	7250.359889	26.033408
185.191128	7271.206063	26.038426
185.107974	7298.690207	26.043444
185.358105	7304.942805	26.048461
185.510506	7310.034204	26.053479
185.756444	7312.436506	26.058496
186.103984	7330.544163	26.063514
186.379353	7350.857024	26.068532
186.561281	7340.230057	26.073549
186.711917	7369.363363	26.078567
186.592225	7380.775546	26.083584
187.142977	7358.215654	26.088602
187.241516	7362.326837	26.093620
187.342992	7378.570966	26.098637
187.071313	7398.639577	26.103655
186.943447	7404.899543	26.108672
187.506066	7417.614994	26.113690
188.065664	7429.490660	26.118708
188.264973	7426.333636	26.123725
188.396956	7452.161766	26.128743
188.229742	7479.131681	26.133760
188.843816	7483.092351	26.138778
189.016079	7490.940830	26.143796
189.106281	7487.594700	26.148813
189.498264	7502.153677	26.153831
189.465075	7518.665123	26.158848
189.894681	7507.791574	26.163866
190.059311	7514.769526	26.168884
189.987612	7522.343316	26.173901
190.630548	7549.551211	26.178919
190.329786	7546.071993	26.183936
190.585231	7539.502730	26.188954
191.071159	7557.779156	26.193972
191.230439	7584.663805	26.198989
191.376648	7594.681582	26.204007
191.306145	7593.107167	26.209024
191.579333	7583.573811	26.214042
191.997178	7607.110482	26.219060
191.961602	7637.761927	26.224077
192.306459	7629.658688	26.229095
192.134761	7653.852777	26.234112
192.427127	7665.010436	26.239130
192.612936	7673.706526	26.244148
192.814921	7692.334014	26.249165
193.022561	7710.686524	26.254183
193.173747	7740.909602	26.259200
193.795078	7716.681330	26.264218
193.561410	7731.123380	26.269236
193.483900	7763.445293	26.274253
194.265669	7765.600836	26.279271
194.300122	7784.223824	26.284288
194.710634	7789.861032	26.289306
194.739456	7815.740668	26.294324
194.884789	7844.311059	26.299341
195.277482	7821.141856	26.304359
195.147153	7826.976332	26.309376
195.495832	7867.306729	26.314394
195.717958	7870.413186	26.319412
195.713455	7892.890719	26.324429
196.121398	7912.312156	26.329447
196.114355	7913.763245	26.334464
196.118171	7922.679343	26.339482
196.589939	7927.355901	26.344500
197.068964	7950.378944	26.349517
197.317295	7961.619695	26.354535
197.735012	7963.368397	26.359552
197.642526	7977.558167	26.364570
197.689221	7979.866696	26.369588
197.991806	7991.821483	26.374605
198.403052	7999.549612	26.379623
198.500741	8013.251996	26.384640
198.658867	8005.222734	26.389658
199.032752	8029.059486	26.394676
198.824997	8039.947217	26.399693
199.590241	8042.304784	26.404711
199.628097	8042.061512	26.409728
199.566714	8053.132984	26.414746
199.694298	8076.393054	26.419764
199.716661	8085.910240	26.424781
200.092759	8065.258898	26.429799
199.748789	8094.053134	26.434816
200.155517	8123.303825	26.439834
200.250334	8125.094083	26.444852
200.401121	8139.031161	26.449869
200.700839	8130.143622	26.454887
200.767742	8163.065457	26.459904
201.142500	8191.647400	26.464922
201.363172	8200.794024	26.469940
201.542638	8195.516842	26.474957
201.597830	8205.681571	26.479975
201.923232	8230.275616	26.484992
202.319854	8243.594092	26.490010
202.644167	8269.841490	26.495028
202.831330	8279.692272	26.500045
203.283435	8288.678636	26.505063
203.214863	8298.841821	26.510080
203.586841	8295.924659	26.515098
203.574160	8325.371821	26.520116
203.738578	8343.536892	26.525133
204.058072	8341.369502	26.530151
204.307366	8343.513085	26.535168
204.840628	8359.660109	26.540186
204.864301	8377.399555	26.545204
204.819924	8377.692028	26.550221
205.353148	8384.331452	26.555239
205.204036	8406.813920	26.560256
205.519414	8411.525127	26.565274
205.711697	8408.521860	26.570292
205.823175	8433.230325	26.575309
206.266258	8449.838899	26.580327
206.259780	8459.044468	26.585344
206.660901	8474.172259	26.590362
207.000385	8480.636601	26.595380
206.613370	8500.320849	26.600397
207.268544	8507.172514	26.605415
207.342851	8538.450222	26.610432
207.615873	8530.483620	26.615450
207.851427	8533.999110	26.620468
207.827921	8542.852341	26.625485
208.629499	8552.732519	26.630503
208.368704	8590.066315	26.635520
208.663923	8593.438858	26.640538
209.396341	8602.227871	26.645556
209.132338	8609.338562	26.650573
209.612933	8624.618761	26.655591
209.370323	8613.667286	26.660608
209.592167	8628.711433	26.665626
210.133553	8624.283191	26.670644
209.891823	8643.570295	26.675661
210.296582	8657.665918	26.680679
210.731893	8661.033445	26.685696
210.744132	8687.646561	26.690714
211.108979	8705.605664	26.695732
210.961700	8702.182739	26.700749
211.462744	8717.105232	26.705767
211.359934	8751.869378	26.710784
211.322645	8752.901814	26.715802
211.643340	8769.190705	26.720820
211.653484	8787.336096	26.725837
212.035441	8805.368883	26.730855
212.318579	8837.901192	26.735872
212.521344	8850.760750	26.740890
213.330082	8865.775103	26.745908
212.798999	8895.138068	26.750925
213.541295	8890.902600	26.755943
213.901085	8890.541541	26.760960
214.060781	8905.032296	26.765978
214.563305	8897.315067	26.770996
214.161174	8924.886249	26.776013
214.920957	8921.433913	26.781031
214.946346	8929.400315	26.786048
214.903227	8940.061411	26.791066
215.101693	8964.065605	26.796084
214.937472	8987.262602	26.801101
215.174923	8994.298489	26.806119
215.798238	9003.546028	26.811136
215.763594	9001.207079	26.816154
216.117416	9027.916340	26.821172
216.066220	9037.259590	26.826189
216.155714	9053.030133	26.831207
216.024373	9065.636324	26.836224
216.616093	9075.557020	26.841242
217.195447	9106.769736	26.846260
217.423391	9141.132751	26.851277
217.619875	9139.120261	26.856295
217.825949	9151.443152	26.861312
218.293274	9158.801861	26.866330
218.579059	9167.085301	26.871348
218.481811	9184.169068	26.876365
218.831509	9201.666544	26.881383
218.931483	9208.257396	26.886400
218.728369	9231.053189	26.891418
219.595375	9246.337885	26.896436
220.126558	9255.187294	26.901453
219.826515	9252.131316	26.906471
220.283660	9282.736049	26.911488
220.307635	9307.677722	26.916506
220.773355	9317.797393	26.921524
220.966676	9307.665789	26.926541
221.019726	9329.220636	26.931559
221.409593	9362.093972	26.936576
221.512138	9369.257858	26.941594
221.788398	9364.233665	26.946612
221.910502	9387.692690	26.951629
222.042634	9409.992280	26.956647
222.678808	9414.468058	26.961664
222.343702	9420.356643	26.966682
222.864235	9437.062155	26.971700
222.901111	9452.981201	26.976717
223.118099	9462.812830	26.981735
223.447479	9483.680313	26.986752
223.361876	9515.649559	26.991770
223.784852	9527.072872	26.996788
224.040031	9522.738142	27.001805
224.324865	9527.375969	27.006823
224.822280	9560.618677	27.011840
224.280852	9587.260983	27.016858
224.865338	9579.003742	27.021876
225.077822	9596.299850	27.026893
225.068631	9618.227687	27.031911
225.525760	9644.735038	27.036928
225.666102	9671.823281	27.041946
226.150658	9689.788930	27.046964
226.301799	9689.032277	27.051981
226.563831	9695.531970	27.056999
226.840457	9719.151052	27.062016
227.177796	9757.157512	27.067034
227.617544	9749.085565	27.072052
227.591461	9751.633220	27.077069
227.906109	9774.741222	27.082087
228.636819	9773.969149	27.087104
228.119411	9786.048962	27.092122
228.225864	9804.681337	27.097140
228.376490	9825.121968	27.102157
228.681606	9837.317971	27.107175
229.431130	9851.903543	27.112192
229.232909	9859.771881	27.117210
229.237396	9857.147512	27.122228
229.640252	9883.770564	27.127245
229.758601	9912.290864	27.132263
230.269431	9901.789000	27.137280
230.637752	9924.600859	27.142298
230.829860	9950.614542	27.147316
230.927933	9945.584162	27.152333
231.113412	9959.633687	27.157351
231.551843	9958.835070	27.162368
231.591925	9974.686370	27.167386
231.937621	9995.580976	27.172404
232.252165	9987.600484	27.177421
232.605001	9997.358804	27.182439
232.964450	10016.716808	27.187456
232.752978	10042.742184	27.192474
233.043577	10027.662511	27.197492
233.357246	10055.779811	27.202509
233.487320	10077.544282	27.207527
233.886690	10069.752164	27.212544
233.791702	10073.031177	27.217562
233.910859	10100.651386	27.222580
234.253365	10127.821217	27.227597
234.338376	10137.482093	27.232615
234.995027	10163.956562	27.237632
234.809497	10183.845115	27.242650
235.194425	10175.451979	27.247668
235.328307	10206.759370	27.252685
235.348541	10239.925596	27.257703
236.024504	10260.910128	27.262720
236.081680	10258.199796	27.267738
236.437542	10283.483579	27.272756
237.000144	10296.645616	27.277773
237.468089	10306.497746	27.282791
237.178565	10329.401546	27.287808
237.416716	10335.586441	27.292826
237.609854	10352.236738	27.297844
237.616979	10386.605853	27.302861
238.191776	10410.643794	27.307879
238.319699	10421.318584	27.312896
238.581558	10417.422822	27.317914
239.062198	10445.528192	27.322932
239.510912	10472.086366	27.327949
239.224302	10471.910055	27.332967
239.858912	10473.594857	27.337984
239.706879	10497.589177	27.343002
239.945604	10536.085616	27.348020
240.275182	10544.425558	27.353037
240.231163	10551.018704	27.358055
240.942193	10556.224445	27.363072
240.918757	10587.455390	27.368090
241.017766	10613.393379	27.373108
241.071307	10626.560239	27.378125
241.608530	10638.166341	27.383143
242.063455	10639.375940	27.388160
241.951721	10672.487676	27.393178
242.186434	10692.027013	27.398196
242.818619	10711.120250	27.403213
242.773216	10723.637149	27.408231
243.590529	10749.653608	27.413248
243.493961	10769.035883	27.418266
243.806421	10768.073721	27.423284
244.022500	10767.841135	27.428301
244.328430	10804.368120	27.433319
244.374611	10818.161786	27.438336
244.542784	10822.728685	27.443354
244.916690	10862.170084	27.448372
245.347323	10857.453905	27.453389
245.673839	10858.168005	27.458407
246.044669	10881.062746	27.463424
246.179688	10879.878617	27.468442
246.139780	10901.773912	27.473460
246.254062	10923.717019	27.478477
246.385722	10934.004774	27.483495
246.881658	10947.582459	27.488512
246.965288	10979.762208	27.493530
247.064245	10976.437530	27.498548
247.589159	10972.432006	27.503565
247.773106	11004.462110	27.508583
247.928297	10995.686653	27.513600
247.999113	11046.165528	27.518618
248.250353	11063.008623	27.523636
249.081566	11070.876048	27.528653
248.760464	11115.757828	27.533671
248.951465	11118.919699	27.538688
249.178886	11130.222088	27.543706
249.594168	11142.719919	27.548724
249.802300	11168.098834	27.553741
249.622624	11210.517171	27.558759
250.141553	11215.431907	27.563776
250.567427	11230.865458	27.568794
250.642139	11251.678088	27.573812
250.812502	11280.371057	27.578829
250.756553	11329.918628	27.583847
251.274973	11347.893166	27.588864
251.759517	11360.252113	27.593882
252.089161	11380.970803	27.598900
252.740266	11404.953529	27.603917
252.940325	11429.807992	27.608935
253.693457	11431.601721	27.613952
253.637084	11437.129113	27.618970
254.055772	11455.650391	27.623988
254.728474	11462.873056	27.629005
254.624300	11479.734349	27.634023
255.115642	11484.998754	27.639040
255.085487	11485.893910	27.644058
255.433732	11484.500421	27.649076
255.432800	11511.461527	27.654093
255.360465	11520.756159	27.659111
255.919520	11526.951520	27.664128
255.985545	11568.267560	27.669146
256.099315	11585.415929	27.674164
256.847147	11571.653554	27.679181
256.896111	11588.733072	27.684199
256.927551	11631.887265	27.689216
257.262338	11637.331983	27.694234
257.776769	11650.694524	27.699252
257.777431	11674.283329	27.704269
258.076679	11688.755932	27.709287
258.366630	11695.461374	27.714304
258.552347	11720.364348	27.719322
258.609529	11730.896518	27.724340
259.079782	11763.826134	27.729357
258.665790	11772.202131	27.734375
259.267283	11789.085807	27.739392
259.765928	11821.750108	27.744410
259.814429	11859.313025	27.749428
260.005240	11857.678467	27.754445
260.158330	11876.349674	27.759463
260.513277	11912.990835	27.764480
260.943516	11911.964248	27.769498
261.139983	11948.977498	27.774516
261.456061	11962.206068	27.779533
261.529384	11975.400706	27.784551
261.615373	12012.474894	27.789568
262.320202	12024.027537	27.794586
262.681564	12036.601151	27.799604
262.784465	12055.389569	27.804621
263.131208	12084.692139	27.809639
263.671672	12086.234337	27.814656
264.114799	12077.656501	27.819674
263.636563	12108.220333	27.824692
264.025921	12127.671283	27.829709
264.391041	12145.564125	27.834727
264.529043	12175.934894	27.839744
264.741492	12189.220162	27.844762
265.046985	12218.018531	27.849780
265.535318	12228.527850	27.854797
265.664610	12238.119661	27.859815
266.025610	12236.897311	27.864832
266.292427	12264.637879	27.869850
266.014389	12289.527762	27.874868
266.873862	12316.291353	27.879885
267.179161	12319.227396	27.884903
267.518350	12334.146955	27.889920
267.624158	12361.457382	27.894938
267.627613	12383.688646	27.899956
268.020395	12391.904101	27.904973
268.084096	12397.988638	27.909991
268.270876	12438.368423	27.915008
268.841252	12470.707876	27.920026
268.692589	12501.524451	27.925044
269.101535	12519.392352	27.930061
269.416534	12536.193380	27.935079
269.515197	12568.748037	27.940096
270.302613	12602.143766	27.945114
270.483507	12620.817548	27.950132
270.513050	12620.908815	27.955149
270.932778	12661.531128	27.960167
271.031877	12701.563678	27.965184
271.696890	12696.932715	27.970202
271.733759	12724.849144	27.975220
271.885956	12748.879290	27.980237
272.452209	12756.698375	27.985255
272.733331	12781.606931	27.990272
273.155564	12817.485123	27.995290
272.853128	12841.834736	28.000308
273.374018	12839.742983	28.005325
273.875970	12862.678774	28.010343
274.038672	12901.106019	28.015360
274.397704	12931.288868	28.020378
274.387944	12944.189998	28.025396
274.764057	12948.812962	28.030413
274.737177	12978.401053	28.035431
275.125918	13021.162769	28.040448
275.378545	13048.093230	28.045466
275.653329	13069.373060	28.050484
276.022878	13090.326864	28.055501
276.354237	13122.562950	28.060519
276.764465	13148.727787	28.065536
277.413845	13172.125744	28.070554
277.545060	13189.349363	28.075572
278.103422	13195.114559	28.080589
278.443280	13211.448952	28.085607
278.463813	13242.424916	28.090624
278.861129	13257.531898	28.095642
278.913368	13264.876015	28.100660
279.161182	13284.592038	28.105677
279.406739	13307.567673	28.110695
279.576845	13306.869172	28.115712
280.194622	13339.720143	28.120730
280.432344	13349.204105	28.125748
280.236696	13363.292018	28.130765
280.844389	13393.559917	28.135783
280.753838	13425.492884	28.140800
281.205913	13432.462192	28.145818
281.292985	13444.463784	28.150836
281.390427	13471.383564	28.155853
281.510129	13490.581343	28.160871
281.620598	13508.292458	28.165888
282.093966	13541.234664	28.170906
282.282381	13582.036963	28.175924
282.601171	13602.546817	28.180941
283.027923	13630.023028	28.185959
283.374882	13660.822176	28.190976
283.895093	13697.460590	28.195994
284.049867	13725.263944	28.201012
284.980230	13733.628417	28.206029
285.543680	13726.299833	28.211047
285.443148	13740.966392	28.216064
286.046037	13763.705591	28.221082
286.269168	13786.855000	28.226100
286.708094	13794.145716	28.231117
286.775964	13814.665781	28.236135
286.853466	13828.727091	28.241152
287.193312	13834.898121	28.246170
287.550603	13861.383275	28.251188
287.632288	13876.286933	28.256205
287.811018	13897.313495	28.261223
287.929375	13928.607875	28.266240
288.348164	13946.474951	28.271258
288.570205	13967.451904	28.276276
288.840057	13990.335471	28.281293
289.138313	14024.267990	28.286311
289.218274	14049.444158	28.291328
289.735920	14069.735819	28.296346
289.661846	14114.191219	28.301364
289.797769	14133.551745	28.306381
290.571461	14157.100778	28.311399
290.343128	14187.190779	28.316416
291.108592	14213.639016	28.321434
291.419327	14240.157695	28.326452
291.695333	14275.422759	28.331469
291.982828	14303.970202	28.336487
292.032545	14309.399901	28.341504
292.496486	14341.994699	28.346522
292.801497	14386.923971	28.351540
293.335978	14400.713314	28.356557
293.760517	14412.281693	28.361575
293.697169	14441.919458	28.366592
294.314691	14462.797052	28.371610
294.369289	14482.530703	28.376628
294.540231	14490.798857	28.381645
295.142512	14529.508752	28.386663
295.294346	14549.817332	28.391680
295.641243	14562.244830	28.396698
295.823483	14605.409652	28.401716
296.205366	14637.901996	28.406733
296.673700	14656.998654	28.411751
296.934506	14665.050352	28.416768
297.586118	14686.310244	28.421786
297.805125	14717.009635	28.426804
297.943042	14737.826574	28.431821
297.938128	14755.989883	28.436839
298.060863	14782.099290	28.441856
298.294986	14811.597191	28.446874
298.904618	14829.936393	28.451892
298.850198	14878.913159	28.456909
299.296045	14905.766737	28.461927
299.583271	14924.373619	28.466944
300.066276	14952.847360	28.471962
300.244847	14988.338080	28.476980
300.612168	15001.266799	28.481997
300.767700	14994.282383	28.487015
301.015555	15032.497352	28.492032
301.285138	15061.565956	28.497050
301.752217	15098.063470	28.502068
301.837876	15094.992274	28.507085
301.984291	15114.905351	28.512103
302.270553	15166.092726	28.517120
302.599651	15193.703554	28.522138
303.182721	15223.116189	28.527156
303.411590	15237.130079	28.532173
303.593740	15267.523010	28.537191
303.783267	15309.716213	28.542208
304.329328	15341.596634	28.547226
304.774131	15353.940806	28.552244
304.943927	15382.630934	28.557261
305.592572	15411.785672	28.562279
305.780490	15451.313176	28.567296
305.873577	15455.500628	28.572314
306.590373	15483.041595	28.577332
306.562686	15508.584500	28.582349
307.144478	15532.296464	28.587367
307.255865	15564.922026	28.592384
307.412593	15602.406431	28.597402
307.700838	15619.491658	28.602420
307.945005	15635.867164	28.607437
308.720900	15665.149466	28.612455
308.726887	15695.837048	28.617472
308.587416	15733.260377	28.622490
309.440612	15756.480282	28.627508
309.357626	15783.156356	28.632525
310.350245	15806.079095	28.637543
310.555319	15846.110584	28.642560
310.584155	15858.772851	28.647578
311.327859	15871.586506	28.652596
311.328311	15897.416912	28.657613
312.088728	15921.452935	28.662631
311.647607	15962.595310	28.667648
312.363589	15968.591554	28.672666
312.682688	16002.449125	28.677684
312.660894	16035.018836	28.682701
313.079057	16068.135261	28.687719
313.332285	16101.910942	28.692736
313.879123	16136.654653	28.697754
314.290984	16142.942321	28.702772
314.276718	16162.990389	28.707789
315.003895	16200.550554	28.712807
315.255756	16245.178563	28.717824
315.274676	16261.060823	28.722842
316.125120	16285.471767	28.727860
316.103041	16308.900101	28.732877
316.375433	16331.677813	28.737895
316.901575	16366.040905	28.742912
317.548195	16375.041469	28.747930
317.767497	16386.350467	28.752948
317.977170	16427.567731	28.757965
318.382315	16458.728202	28.762983
318.603490	16461.774254	28.768000
318.550787	16482.613886	28.773018
319.209635	16518.096363	28.778036
319.432552	16527.282054	28.783053
319.390438	16559.523641	28.788071
319.953577	16599.122746	28.793088
320.498255	16612.759425	28.798106
320.587378	16625.197997	28.803124
320.818519	16658.946962	28.808141
321.089541	16682.856935	28.813159
321.365596	16720.365172	28.818176
321.670672	16728.743113	28.823194
322.170684	16747.350025	28.828212
321.951364	16788.935355	28.833229
322.515274	16827.379694	28.838247
322.664375	16841.020452	28.843264
322.971879	16841.893216	28.848282
323.338758	16885.413392	28.853300
323.698353	16934.704597	28.858317
323.857591	16972.722846	28.863335
324.254788	16990.735534	28.868352
324.587433	17034.586419	28.873370
324.956510	17063.612216	28.878388
325.307471	17088.649028	28.883405
325.568867	17106.889160	28.888423
325.981637	17160.676498	28.893440
326.394481	17200.629702	28.898458
326.622402	17226.665760	28.903476
326.867206	17240.525868	28.908493
327.038554	17272.169377	28.913511
327.667684	17324.168968	28.918528
327.789362	17350.323640	28.923546
328.697017	17356.454224	28.928564
328.555164	17385.817165	28.933581
329.017642	17437.231568	28.938599
329.777636	17467.303034	28.943616
329.982576	17483.801928	28.948634
330.670048	17514.446534	28.953652
330.713561	17540.307093	28.958669
331.244006	17545.083195	28.963687
331.728557	17590.674076	28.968704
331.443412	17628.086401	28.973722
332.075573	17633.550225	28.978740
332.480386	17658.407222	28.983757
332.644612	17687.127537	28.988775
333.014030	17728.591194	28.993792
333.339886	17758.820024	28.998810
333.906715	17777.265770	29.003828
333.859600	17793.622215	29.008845
334.606921	17816.279407	29.013863
335.430272	17850.617011	29.018880
335.533366	17869.670610	29.023898
336.096191	17864.031433	29.028916
336.071156	17898.320163	29.033933
336.100513	17935.258840	29.038951
336.621271	17942.610414	29.043968
337.052113	17944.324986	29.048986
337.707542	17969.785676	29.054004
337.597981	18010.216451	29.059021
337.682890	18034.003110	29.064039
338.102435	18052.041646	29.069056
338.516758	18073.844797	29.074074
339.197257	18102.025056	29.079092
339.238002	18125.540173	29.084109
339.490706	18150.441959	29.089127
339.644819	18195.772312	29.094144
340.170509	18218.491893	29.099162
340.655805	18251.185555	29.104180
341.001666	18274.748199	29.109197
341.108020	18288.548532	29.114215
341.492642	18308.443488	29.119232
341.395551	18358.066596	29.124250
342.044950	18374.497690	29.129268
342.243077	18415.226954	29.134285
342.223140	18460.624616	29.139303
342.685688	18475.447494	29.144320
342.974612	18498.465063	29.149338
343.135516	18537.503273	29.154356
343.246796	18583.741749	29.159373
343.935175	18624.751480	29.164391
344.138228	18647.170319	29.169408
344.584583	18673.130029	29.174426
344.961110	18714.560323	29.179444
345.631826	18754.733201	29.184461
346.050745	18777.423909	29.189479
346.232092	18787.248204	29.194496
346.461261	18831.228161	29.199514
346.761498	18867.917701	29.204532
346.929951	18903.185310	29.209549
347.284476	18939.497215	29.214567
347.868005	18969.263286	29.219584
347.889848	19009.452559	29.224602
348.335208	19055.291981	29.229620
348.686348	19071.998442	29.234637
349.050899	19108.127799	29.239655
349.425537	19148.925863	29.244672
349.378779	19181.015737	29.249690
350.158075	19216.626020	29.254708
350.931167	19267.066442	29.259725
351.080007	19292.316542	29.264743
351.658974	19330.452167	29.269760
351.834157	19380.430575	29.274778
351.972116	19398.067881	29.279796
352.573687	19431.647858	29.284813
353.208474	19481.139247	29.289831
353.804743	19518.449653	29.294848
353.948336	19538.567181	29.299866
354.408726	19538.995561	29.304884
354.489408	19583.886323	29.309901
354.833011	19637.412612	29.314919
355.618947	19653.425216	29.319936
355.680980	19692.417862	29.324954
355.922705	19709.574939	29.329972
356.255657	19720.347298	29.334989
356.392609	19767.768617	29.340007
357.070245	19811.896198	29.345024
357.094478	19841.923323	29.350042
357.803223	19875.790718	29.355060
358.176844	19913.375238	29.360077
358.060218	19947.735369	29.365095
358.712015	19981.863018	29.370112
358.948994	20030.959919	29.375130
359.618333	20067.564350	29.380148
359.891126	20071.975503	29.385165
360.241138	20105.114483	29.390183
360.805247	20155.280034	29.395200
360.555990	20200.974138	29.400218
361.306344	20213.640365	29.405236
361.511113	20247.539759	29.410253
361.741690	20294.850964	29.415271
362.553344	20317.757919	29.420288
362.496920	20355.710831	29.425306
363.323266	20368.813876	29.430324
363.323090	20421.781571	29.435341
363.624156	20469.557679	29.440359
364.107842	20494.268785	29.445376
364.142119	20537.333364	29.450394
364.804884	20577.866665	29.455412
365.256796	20606.990639	29.460429
365.304723	20643.899194	29.465447
366.220011	20678.850167	29.470464
365.971328	20723.981278	29.475482
366.536760	20752.382123	29.480500
366.996816	20794.234171	29.485517
366.993161	20822.306681	29.490535
367.741733	20853.041990	29.495552
367.931386	20889.107966	29.500570
368.396541	20904.405510	29.505588
368.999134	20947.705153	29.510605
368.814419	20992.321984	29.515623
369.440785	21017.642428	29.520640
369.957872	21037.903428	29.525658
370.210808	21062.532118	29.530676
370.954492	21109.475551	29.535693
371.080427	21133.546791	29.540711
371.669539	21165.522844	29.545728
371.490995	21196.156569	29.550746
371.968501	21242.559505	29.555764
372.531081	21289.200741	29.560781
372.570704	21317.626358	29.565799
373.684317	21320.798611	29.570816
374.250661	21356.637849	29.575834
374.862572	21399.103205	29.580852
375.055282	21419.697283	29.585869
375.116929	21437.261083	29.590887
375.540030	21455.490347	29.595904
375.456544	21510.338599	29.600922
375.939127	21546.195234	29.605940
376.891679	21558.619428	29.610957
377.153072	21580.985306	29.615975
377.338844	21601.719481	29.620992
377.435137	21657.621531	29.626010
377.672403	21696.273061	29.631028
378.432079	21724.307696	29.636045
378.503700	21763.637819	29.641063
378.967011	21786.724161	29.646080
379.030308	21827.491960	29.651098
379.690222	21857.914295	29.656116
380.091589	21914.361133	29.661133
380.380725	21949.136029	29.666151
381.360667	21979.004400	29.671168
381.557140	22032.222184	29.676186
381.568451	22050.709302	29.681204
381.924176	22079.260562	29.686221
382.224906	22128.081959	29.691239
382.782252	22171.376493	29.696256
383.168440	22200.069540	29.701274
383.151994	22222.939359	29.706292
384.175542	22267.700518	29.711309
384.286910	22330.302454	29.716327
384.707387	22348.394395	29.721344
384.814290	22395.093504	29.726362
385.332799	22424.770893	29.731380
385.894869	22451.986501	29.736397
386.343084	22506.280380	29.741415
386.476863	22550.095174	29.746432
386.968881	22595.014383	29.751450
387.493747	22611.399324	29.756468
388.060301	22660.725418	29.761485
387.995797	22705.645419	29.766503
388.347540	22728.917031	29.771520
388.846343	22774.102035	29.776538
389.151197	22820.528416	29.781556
389.885157	22840.358493	29.786573
389.981230	22898.044648	29.791591
390.249202	22924.046783	29.796608
390.444277	22974.931325	29.801626
391.117620	23028.024621	29.806644
391.533400	23061.562216	29.811661
391.699459	23114.266611	29.816679
392.048490	23145.811568	29.821696
392.552872	23183.679834	29.826714
392.873431	23243.040686	29.831732
393.785855	23293.429310	29.836749
393.910531	23309.061212	29.841767
394.341363	23317.568354	29.846784
394.492881	23377.143642	29.851802
395.254815	23399.167548	29.856820
395.557653	23441.324950	29.861837
395.885669	23488.279091	29.866855
396.185743	23518.182119	29.871872
396.426914	23547.610907	29.876890
396.872069	23596.053248	29.881908
397.547817	23622.075816	29.886925
397.727235	23675.784075	29.891943
398.020989	23720.537239	29.896960
398.619198	23762.512639	29.901978
398.793545	23786.388919	29.906996
399.284872	23825.232000	29.912013
399.627405	23889.159046	29.917031
400.429850	23907.474948	29.922048
400.658487	23951.274569	29.927066
401.111950	23984.911841	29.932084
401.660053	24026.669138	29.937101
402.098585	24063.774544	29.942119
402.497587	24107.451828	29.947136
402.697862	24136.275075	29.952154
402.973378	24170.678420	29.957172
403.781823	24207.868093	29.962189
403.772874	24262.485971	29.967207
404.206618	24305.577807	29.972224
404.644338	24345.362767	29.977242
405.061870	24374.066966	29.982260
405.781671	24424.880245	29.987277
406.036149	24470.252069	29.992295
406.683254	24511.953220	29.997312
407.229279	24519.688276	30.002330
407.628202	24564.462570	30.007348
408.358856	24610.345803	30.012365
408.323558	24670.880476	30.017383
408.605010	24682.255824	30.022400
409.183039	24702.340912	30.027418
409.274943	24760.141343	30.032436
409.849116	24797.568108	30.037453
409.690094	24854.767003	30.042471
410.244534	24882.978006	30.047488
410.769921	24922.160139	30.052506
410.691635	24987.795945	30.057524
411.472849	25036.128566	30.062541
411.917514	25081.388620	30.067559
412.467587	25130.117617	30.072576
412.902632	25163.613641	30.077594
412.799402	25216.906762	30.082612
413.439749	25250.367466	30.087629
413.439526	25295.919179	30.092647
414.073771	25356.033494	30.097664
415.126585	25393.801938	30.102682
415.433281	25443.587494	30.107700
415.807805	25489.279652	30.112717
416.473534	25534.118081	30.117735
417.301592	25561.337357	30.122752
417.608552	25598.753269	30.127770
417.874515	25636.816223	30.132788
418.485554	25672.401843	30.137805
419.197528	25703.074834	30.142823
419.432094	25735.542327	30.147840
420.393710	25764.324576	30.152858
420.208333	25793.422490	30.157876
420.798590	25832.726891	30.162893
421.310786	25867.999691	30.167911
421.521139	25882.230628	30.172928
422.065635	25901.460152	30.177946
422.303281	25941.561013	30.182964
423.266183	25948.461521	30.187981
423.288573	25987.536832	30.192999
423.483544	26013.899537	30.198016
423.902122	26043.489431	30.203034
423.955405	26065.298018	30.208052
424.623348	26114.180672	30.213069
424.635328	26165.355781	30.218087
424.996351	26199.602473	30.223104
425.205317	26217.858086	30.228122
425.552319	26266.485127	30.233140
426.112975	26324.962465	30.238157
426.349869	26378.029581	30.243175
426.525734	26400.933205	30.248192
427.136282	26444.020195	30.253210
427.490285	26518.931997	30.258228
428.134639	26560.146651	30.263245
428.119219	26597.430361	30.268263
428.431598	26667.388751	30.273280
429.452930	26713.879348	30.278298
429.704896	26760.885083	30.283316
430.180889	26823.590068	30.288333
430.703047	26881.181556	30.293351
431.101052	26908.759458	30.298368
431.297505	26948.702338	30.303386
431.746776	27023.159073	30.308404
432.160513	27092.375490	30.313421
432.769019	27132.843667	30.318439
433.395572	27174.554756	30.323456
433.974042	27214.548693	30.328474
434.625905	27272.211538	30.333492
434.824666	27328.145368	30.338509
435.643190	27361.013088	30.343527
435.770873	27391.623213	30.348544
437.102328	27426.929495	30.353562
436.988906	27481.597039	30.358580
437.521869	27526.046323	30.363597
438.169760	27549.988448	30.368615
438.452694	27585.067701	30.373632
439.428612	27640.902565	30.378650
439.857898	27665.991171	30.383668
440.389546	27680.989001	30.388685
440.623438	27710.695877	30.393703
440.727388	27764.975168	30.398720
441.321687	27794.600577	30.403738
441.307755	27832.186363	30.408756
441.641041	27882.968168	30.413773
442.217569	27926.430387	30.418791
442.315386	27974.195081	30.423808
442.963360	28010.656313	30.428826
443.390681	28061.893070	30.433844
443.830630	28114.919416	30.438861
444.305128	28156.162823	30.443879
444.666228	28200.904037	30.448896
445.376701	28242.815193	30.453914
445.661022	28304.560564	30.458932
446.297655	28338.583077	30.463949
446.732105	28370.090514	30.468967
446.980345	28424.704471	30.473984
447.720815	28482.186428	30.479002
447.632401	28509.175423	30.484020
448.182134	28543.442950	30.489037
448.800850	28601.595177	30.494055
448.741816	28667.751331	30.499072
449.435719	28711.959465	30.504090
449.607289	28753.229111	30.509108
449.838868	28802.910690	30.514125
450.702443	28857.869123	30.519143
450.702133	28919.212660	30.524160
451.271357	28956.865440	30.529178
451.665959	29001.656824	30.534196
452.022685	29049.378578	30.539213
452.815231	29114.714460	30.544231
453.109939	29151.961951	30.549248
453.720209	29204.414676	30.554266
454.513882	29255.758496	30.559284
454.534322	29314.731134	30.564301
455.219219	29351.062940	30.569319
455.570719	29393.780616	30.574336
456.331028	29438.355010	30.579354
456.717821	29487.653330	30.584372
457.137859	29524.272135	30.589389
457.685878	29581.152372	30.594407
458.231438	29619.561245	30.599424
458.924940	29659.330535	30.604442
459.214605	29710.304732	30.609460
459.506517	29752.765016	30.614477
460.152162	29798.772448	30.619495
460.185978	29853.612456	30.624512
460.878956	29896.265505	30.629530
461.244270	29945.063971	30.634548
461.699488	29998.033653	30.639565
462.341325	30052.060955	30.644583
462.411361	30113.034344	30.649600
463.198247	30155.404392	30.654618
463.674983	30207.882221	30.659636
463.974031	30245.613986	30.664653
464.558362	30310.282181	30.669671
465.160349	30365.291778	30.674688
466.055304	30405.095753	30.679706
466.700573	30438.458540	30.684724
466.843109	30494.683220	30.689741
467.280820	30528.843860	30.694759
467.887067	30565.437266	30.699776
468.559661	30616.025958	30.704794
468.532885	30679.783865	30.709812
469.035540	30709.946777	30.714829
469.626344	30750.621971	30.719847
469.652868	30811.245379	30.724864
470.557389	30868.380105	30.729882
471.634086	30898.483226	30.734900
472.039465	30914.889606	30.739917
472.905108	30956.359010	30.744935
473.258073	31012.891305	30.749952
473.700744	31037.648221	30.754970
474.020426	31074.971434	30.759988
474.131601	31106.527798	30.765005
474.695097	31165.448572	30.770023
474.964569	31225.821932	30.775040
475.340078	31260.183565	30.780058
475.615561	31286.375430	30.785076
475.883697	31351.172287	30.790093
476.830165	31381.222046	30.795111
476.691146	31461.866296	30.800128
476.939365	31521.064333	30.805146
478.019206	31555.575204	30.810164
478.297626	31598.408177	30.815181
478.497686	31658.699860	30.820199
478.566688	31733.395880	30.825216
479.322973	31784.876407	30.830234
480.011342	31833.204075	30.835252
480.389784	31884.545403	30.840269
480.812984	31942.189054	30.845287
481.033343	32023.644100	30.850304
481.630337	32074.498750	30.855322
482.525257	32102.198475	30.860340
482.655342	32163.897886	30.865357
483.354379	32220.843846	30.870375
483.898246	32269.622494	30.875392
484.293692	32313.904893	30.880410
484.873163	32365.769683	30.885428
485.130651	32418.773085	30.890445
485.815945	32459.499762	30.895463
486.447921	32512.328015	30.900480
487.053417	32584.036555	30.905498
487.113589	32632.665803	30.910516
487.403498	32680.799775	30.915533
488.179079	32717.966015	30.920551
488.539107	32777.272877	30.925568
488.926765	32831.136252	30.930586
489.538235	32902.914518	30.935604
489.747335	32971.418427	30.940621
490.365456	33024.818409	30.945639
490.617857	33081.071127	30.950656
491.208788	33149.474801	30.955674
491.705518	33208.855192	30.960692
492.103127	33259.156229	30.965709
493.104100	33328.817981	30.970727
493.302530	33415.094537	30.975744
493.629494	33457.264631	30.980762
494.622599	33496.848072	30.985780
494.935415	33566.529783	30.990797
495.569032	33620.922867	30.995815
495.915010	33690.202048	31.000832
496.750780	33729.051622	31.005850
497.529466	33792.255570	31.010868
497.587359	33856.168810	31.015885
498.183808	33920.886230	31.020903
498.915859	33986.546966	31.025920
498.986114	34018.471863	31.030938
499.997088	34080.395345	31.035956
500.243199	34159.944010	31.040973
500.757019	34200.504275	31.045991
501.189905	34253.146631	31.051008
501.582598	34305.663264	31.056026
502.722062	34370.387298	31.061044
502.802433	34426.126872	31.066061
503.261977	34484.716279	31.071079
504.139361	34545.723200	31.076096
504.546161	34589.337387	31.081114
505.325001	34619.619186	31.086132
505.643488	34695.760090	31.091149
506.334715	34758.947240	31.096167
506.416189	34801.517646	31.101184
507.012472	34846.890223	31.106202
507.702627	34906.279092	31.111220
508.086327	34972.767776	31.116237
508.878791	35019.017126	31.121255
509.274029	35062.596526	31.126272
509.533472	35113.023486	31.131290
510.290297	35178.776069	31.136308
510.293195	35256.050641	31.141325
511.313332	35292.380462	31.146343
511.790448	35352.503356	31.151360
512.233621	35414.370687	31.156378
512.842246	35449.544505	31.161396
512.932565	35514.666900	31.166413
513.459638	35563.649929	31.171431
513.895989	35615.570015	31.176448
514.083895	35693.399688	31.181466
514.815902	35744.864265	31.186484
515.334012	35804.082609	31.191501
515.892768	35872.016199	31.196519
516.474008	35914.194331	31.201536
516.893499	35973.779790	31.206554
517.569398	36037.103404	31.211572
517.839927	36096.799077	31.216589
518.465144	36147.288468	31.221607
518.924970	36203.286501	31.226624
519.179544	36252.332214	31.231642
520.070029	36287.076160	31.236660
520.127220	36354.949281	31.241677
520.581224	36428.563394	31.246695
521.447838	36506.836745	31.251712
521.981819	36545.079682	31.256730
522.748741	36602.656539	31.261748
523.196486	36672.984543	31.266765
523.668889	36736.631418	31.271783
524.223107	36774.738968	31.276800
524.745813	36827.042781	31.281818
525.303755	36883.960819	31.286836
525.767991	36960.311397	31.291853
526.242922	37033.880370	31.296871
526.821631	37079.154258	31.301888
527.080958	37126.292390	31.306906
527.817838	37205.458053	31.311924
528.158370	37288.381744	31.316941
528.620813	37335.187082	31.321959
529.758918	37389.808196	31.326976
529.973518	37465.255435	31.331994
530.858759	37503.884216	31.337012
531.384723	37559.594714	31.342029
531.602613	37642.044840	31.347047
532.209908	37687.817319	31.352064
533.382635	37736.040111	31.357082
533.845156	37803.362626	31.362100
534.152104	37841.481735	31.367117
534.682799	37915.767806	31.372135
535.275959	37980.898187	31.377152
535.540361	38036.347251	31.382170
536.574628	38094.818894	31.387188
536.997461	38143.835690	31.392205
537.228585	38209.124529	31.397223
537.831058	38270.864989	31.402240
537.952925	38335.676856	31.407258
538.604743	38390.248794	31.412276
539.036535	38456.379579	31.417293
539.459557	38526.371786	31.422311
540.204518	38590.990133	31.427328
540.466446	38663.944530	31.432346
541.043095	38733.833270	31.437364
541.477075	38801.132675	31.442381
541.838854	38866.774726	31.447399
542.727435	38945.506413	31.452416
542.866306	39010.128533	31.457434
543.451332	39100.736716	31.462452
544.135498	39174.245179	31.467469
544.525003	39247.584840	31.472487
545.210401	39334.254608	31.477504
545.813994	39389.714934	31.482522
546.520439	39456.968626	31.487540
547.497363	39526.371403	31.492557
548.247001	39577.411697	31.497575
549.045640	39641.305343	31.502592
549.368058	39727.462531	31.507610
549.742268	39771.902722	31.512628
550.365789	39831.871283	31.517645
551.175053	39896.142816	31.522663
551.854305	39956.055240	31.527680
552.255068	40020.839712	31.532698
552.698828	40053.556398	31.537716
553.106125	40117.232302	31.542733
553.379122	40160.029985	31.547751
554.401377	40221.221723	31.552768
554.617032	40274.356398	31.557786
555.092579	40329.556690	31.562804
555.496592	40404.451525	31.567821
555.897518	40471.560602	31.572839
556.559237	40517.798410	31.577856
556.945445	40588.514846	31.582874
557.542848	40659.815314	31.587892
558.354896	40737.023995	31.592909
558.604525	40783.759806	31.597927
559.381864	40829.827809	31.602944
559.772914	40907.441322	31.607962
560.358729	40979.376231	31.612980
560.872771	41044.997867	31.617997
561.537875	41104.518714	31.623015
561.964599	41167.084032	31.628032
562.397653	41258.734992	31.633050
562.790182	41340.194635	31.638068
563.627041	41392.639719	31.643085
564.259543	41464.818193	31.648103
564.990483	41530.408909	31.653120
565.342461	41602.839432	31.658138
566.090989	41677.269099	31.663156
566.467250	41760.377841	31.668173
566.998881	41819.837841	31.673191
568.061436	41872.366976	31.678208
568.681209	41965.139621	31.683226
569.015381	42052.416976	31.688244
569.436564	42106.151201	31.693261
570.087664	42174.481542	31.698279
570.548280	42225.368675	31.703296
570.890613	42311.954624	31.708314
571.542541	42388.309732	31.713332
571.980615	42480.392130	31.718349
572.755097	42555.502918	31.723367
573.651146	42636.938834	31.728384
574.115393	42712.388760	31.733402
574.375551	42765.428633	31.738420
575.031114	42846.049734	31.743437
575.606419	42931.602609	31.748455
576.342581	43021.649757	31.753472
576.981417	43093.903054	31.758490
577.727537	43146.497582	31.763508
578.563254	43217.737099	31.768525
578.943958	43303.276493	31.773543
579.494677	43368.565782	31.778560
580.080584	43446.713470	31.783578
580.588255	43508.506311	31.788596
581.037762	43558.054168	31.793613
581.466801	43640.853336	31.798631
582.212532	43718.843194	31.803648
582.864683	43808.522930	31.808666
583.387787	43887.383682	31.813684
584.014361	43945.815214	31.818701
584.617970	44021.784161	31.823719
585.706914	44094.772055	31.828736
585.949440	44166.567809	31.833754
586.629714	44250.742522	31.838772
587.122665	44311.056719	31.843789
587.320030	44373.601393	31.848807
588.209574	44463.106192	31.853824
588.851120	44540.920996	31.858842
589.215096	44600.537644	31.863860
590.350455	44690.043983	31.868877
590.746341	44751.029148	31.873895
591.690044	44807.257933	31.878912
592.303689	44870.783670	31.883930
592.804931	44936.146655	31.888948
593.404280	44996.726492	31.893965
593.811976	45052.138469	31.898983
594.309302	45097.066904	31.904000
594.672182	45168.436240	31.909018
595.179728	45253.351227	31.914036
595.943953	45314.612064	31.919053
596.562478	45366.776208	31.924071
597.113107	45429.423953	31.929088
597.478478	45512.693478	31.934106
598.124400	45578.025356	31.939124
598.889312	45644.660669	31.944141
599.562832	45724.293691	31.949159
600.167024	45782.049600	31.954176
600.599163	45841.696861	31.959194
601.255331	45937.081845	31.964212
602.039417	46001.865135	31.969229
602.327156	46070.260433	31.974247
602.807672	46133.029473	31.979264
603.294610	46224.914060	31.984282
603.897375	46300.523071	31.989300
604.829724	46367.840552	31.994317
605.259486	46451.731938	31.999335
605.891102	46534.153778	32.004352
606.344476	46598.738016	32.009370
606.973046	46687.860916	32.014388
607.614721	46782.387496	32.019405
608.062600	46858.504265	32.024423
608.779387	46928.754691	32.029440
609.321093	47023.693675	32.034458
609.771674	47108.992774	32.039476
610.598787	47176.592615	32.044493
611.118993	47282.057045	32.049511
611.750933	47358.909552	32.054528
612.593198	47454.565185	32.059546
612.907206	47516.924319	32.064564
613.711778	47594.721788	32.069581
614.297781	47700.427145	32.074599
614.732452	47797.547467	32.079616
615.216522	47865.544303	32.084634
615.857647	47942.735540	32.089652
616.690000	48034.259347	32.094669
616.957427	48151.702911	32.099687
617.640833	48236.305577	32.104704
618.333632	48308.118673	32.109722
618.880485	48398.832529	32.114740
619.599530	48502.190071	32.119757
620.044392	48584.853844	32.124775
620.499689	48688.319118	32.129792
621.195055	48796.551343	32.134810
621.876029	48884.548697	32.139828
622.804598	48962.239762	32.144845
623.474536	49054.499519	32.149863
624.051264	49141.703744	32.154880
624.900548	49230.347515	32.159898
625.095449	49331.083619	32.164916
626.048874	49404.398844	32.169933
626.610250	49497.613402	32.174951
627.321240	49576.621843	32.179968
627.908137	49680.099222	32.184986
628.364767	49786.699712	32.190004
628.742123	49863.768673	32.195021
629.561848	49946.556478	32.200039
630.227422	50044.196520	32.205056
630.861890	50148.202279	32.210074
631.239461	50239.663442	32.215092
632.185578	50324.108889	32.220109
632.912913	50408.770848	32.225127
633.781712	50477.196697	32.230144
634.531566	50570.281173	32.235162
634.830234	50663.952218	32.240180
635.575713	50728.338123	32.245197
636.413777	50802.104130	32.250215
636.556226	50894.722056	32.255232
637.345049	50982.667107	32.260250
637.709258	51057.946126	32.265268
638.473477	51129.934963	32.270285
639.432543	51237.679615	32.275303
640.005311	51329.543268	32.280320
640.810321	51395.705936	32.285338
641.197002	51467.969993	32.290356
642.047452	51560.591066	32.295373
642.523105	51650.113145	32.300391
643.171500	51736.935278	32.305408
643.924067	51823.582689	32.310426
644.344815	51924.190966	32.315444
644.959583	52012.087379	32.320461
645.329559	52105.681061	32.325479
646.257820	52183.577976	32.330496
646.728607	52290.727004	32.335514
647.285409	52383.479504	32.340532
647.833925	52467.204189	32.345549
648.793229	52582.356296	32.350567
649.372030	52691.997438	32.355584
650.008220	52774.493014	32.360602
650.647068	52861.280745	32.365620
651.141079	52964.765964	32.370637
651.674915	53064.837231	32.375655
652.432432	53152.525773	32.380672
653.286532	53261.142413	32.385690
653.885721	53381.017474	32.390708
654.678890	53473.230825	32.395725
655.464283	53574.033855	32.400743
655.578290	53672.844719	32.405760
656.524654	53758.587605	32.410778
656.941996	53876.888078	32.415796
658.404306	53957.429792	32.420813
659.158119	54034.311195	32.425831
659.488701	54151.831714	32.430848
660.176999	54260.184435	32.435866
660.792558	54351.461607	32.440884
661.350315	54442.211786	32.445901
662.344382	54534.090621	32.450919
662.628482	54644.331622	32.455936
663.365163	54749.122415	32.460954
664.153052	54832.621966	32.465972
664.660249	54909.484388	32.470989
665.584286	55027.543934	32.476007
666.175516	55143.726000	32.481024
667.254599	55222.782151	32.486042
667.820420	55314.463741	32.491060
668.417225	55390.548837	32.496077
669.250699	55495.694080	32.501095
669.991923	55598.290157	32.506112
670.656466	55670.107059	32.511130
671.294337	55756.592015	32.516148
671.964608	55867.875434	32.521165
672.243639	55954.325760	32.526183
672.524594	56043.619157	32.531200
673.829529	56136.856758	32.536218
674.101816	56240.247559	32.541236
674.661487	56350.724347	32.546253
675.310147	56443.920162	32.551271
675.660870	56544.260689	32.556288
676.910263	56630.534789	32.561306
677.603270	56738.117054	32.566324
678.198026	56832.239728	32.571341
678.780756	56904.125207	32.576359
679.364799	56986.018600	32.581376
680.495797	57084.596638	32.586394
680.770221	57178.533781	32.591412
681.306339	57264.441962	32.596429
682.030133	57378.347151	32.601447
682.405629	57462.450435	32.606464
683.636841	57555.883863	32.611482
683.910070	57663.957516	32.616500
684.618491	57777.823322	32.621517
685.683147	57861.985093	32.626535
686.073813	57957.025096	32.631552
686.536063	58048.686006	32.636570
687.213304	58167.910927	32.641588
688.035724	58273.173949	32.646605
688.972190	58367.986783	32.651623
689.587045	58476.671904	32.656640
690.464129	58579.741301	32.661658
690.592220	58680.464337	32.666676
691.232168	58787.927521	32.671693
692.135561	58908.250589	32.676711
692.713242	59014.739563	32.681728
693.623201	59099.696711	32.686746
694.133857	59224.256940	32.691764
694.704103	59345.863523	32.696781
695.571708	59434.392928	32.701799
695.874899	59542.212787	32.706816
696.690729	59663.294193	32.711834
697.173611	59791.565460	32.716852
698.280997	59903.570338	32.721869
699.189944	59992.512450	32.726887
699.881050	60122.811471	32.731904
700.737125	60226.455264	32.736922
701.716456	60348.417459	32.741940
702.066025	60456.689573	32.746957
703.032053	60542.995921	32.751975
703.864461	60673.730178	32.756992
704.793098	60773.358402	32.762010
705.488518	60874.927756	32.767028
706.298429	60965.388230	32.772045
707.193606	61068.069378	32.777063
707.615784	61177.041161	32.782080
708.254962	61277.787676	32.787098
709.087168	61368.404271	32.792116
709.479375	61480.245374	32.797133
710.689298	61571.558852	32.802151
711.416210	61677.923604	32.807168
712.009363	61803.320433	32.812186
712.492130	61904.816352	32.817204
713.281455	61991.973343	32.822221
714.137743	62086.614833	32.827239
714.609949	62199.002846	32.832256
715.674611	62313.549809	32.837274
715.909111	62430.819322	32.842292
716.376361	62542.407444	32.847309
717.540386	62645.918054	32.852327
717.832498	62740.529375	32.857344
718.716236	62829.292284	32.862362
719.532175	62956.321619	32.867380
720.013917	63072.688177	32.872397
720.893978	63165.283099	32.877415
721.368167	63283.661890	32.882432
722.439339	63389.858711	32.887450
723.516348	63508.499509	32.892468
723.828438	63613.015285	32.897485
724.866231	63702.142103	32.902503
725.569361	63807.694020	32.907520
726.158461	63913.726695	32.912538
726.769639	64015.268852	32.917556
727.320075	64108.699902	32.922573
728.135579	64197.587503	32.927591
729.043294	64302.747937	32.932608
729.830066	64387.507566	32.937626
730.451972	64501.135033	32.942644
730.967601	64601.570842	32.947661
731.369988	64698.246169	32.952679
732.138174	64819.505406	32.957696
732.710962	64919.257034	32.962714
733.782996	65049.550152	32.967732
734.018788	65162.834211	32.972749
735.028570	65257.073223	32.977767
735.409061	65369.184158	32.982784
736.039667	65494.945187	32.987802
737.134007	65613.235060	32.992820
737.639665	65725.776047	32.997837
738.521481	65857.629027	33.002855
739.034061	65972.009594	33.007872
739.925298	66087.680949	33.012890
740.543906	66216.931214	33.017908
741.302722	66361.582459	33.022925
742.398128	66463.278003	33.027943
743.069036	66580.821617	33.032960
743.872631	66703.723279	33.037978
744.652656	66830.826826	33.042996
744.917705	66966.853259	33.048013
746.111872	67076.550823	33.053031
746.917420	67184.840282	33.058048
747.711914	67307.803923	33.063066
748.614584	67446.073418	33.068084
749.473700	67564.261597	33.073101
750.650458	67657.188111	33.078119
751.119870	67777.521608	33.083136
751.803999	67907.416390	33.088154
752.576790	68030.343640	33.093172
752.788726	68153.749849	33.098189
753.718533	68264.711088	33.103207
754.431066	68392.872082	33.108224
755.092950	68511.053954	33.113242
756.068552	68644.976367	33.118260
756.394625	68769.227120	33.123277
757.264389	68883.672215	33.128295
758.124404	69028.578182	33.133312
759.244652	69153.465014	33.138330
760.251828	69267.592390	33.143348
760.825455	69384.807552	33.148365
761.685750	69514.120575	33.153383
762.396555	69644.318877	33.158400
763.295335	69749.578000	33.163418
764.607026	69873.451266	33.168436
764.654282	70008.939200	33.173453
765.475207	70123.209459	33.178471
766.575753	70248.270434	33.183488
767.266400	70355.122221	33.188506
768.047654	70464.393664	33.193524
768.566583	70605.004452	33.198541
769.500208	70729.855600	33.203559
769.837476	70844.557363	33.208576
770.744446	70943.397549	33.213594
771.762205	71071.853249	33.218612
772.123015	71215.864080	33.223629
772.969766	71339.715250	33.228647
773.480657	71459.569833	33.233664
773.827378	71590.048901	33.238682
774.900664	71712.341089	33.243700
775.570967	71834.555105	33.248717
776.178365	71954.788553	33.253735
777.182124	72089.632355	33.258752
777.751058	72213.262616	33.263770
778.589162	72346.105779	33.268788
779.285281	72474.041373	33.273805
780.240461	72587.303737	33.278823
781.250302	72716.175352	33.283840
781.540969	72860.082431	33.288858
783.042536	72970.809609	33.293876
783.596568	73096.091429	33.298893
784.149007	73213.868732	33.303911
784.983522	73345.643778	33.308928
785.656973	73479.166134	33.313946
786.355044	73600.835558	33.318964
787.005681	73746.048635	33.323981
788.000256	73886.438136	33.328999
789.098649	74033.741787	33.334016
789.471154	74169.872758	33.339034
790.330813	74281.364013	33.344052
790.914949	74421.894340	33.349069
791.868778	74559.405143	33.354087
793.159361	74705.720484	33.359104
793.489734	74838.643955	33.364122
794.360932	74966.938587	33.369140
795.072308	75110.127269	33.374157
795.776253	75242.814475	33.379175
796.740628	75386.639844	33.384192
797.691086	75540.839458	33.389210
798.645447	75675.530543	33.394228
799.369793	75808.704777	33.399245
800.321948	75949.475152	33.404263
800.987635	76075.185862	33.409280
801.691598	76229.658731	33.414298
802.800957	76367.066790	33.419316
803.404653	76511.174178	33.424333
804.196153	76642.192244	33.429351
805.008753	76777.419486	33.434368
805.587890	76934.264212	33.439386
806.825349	77083.304776	33.444404
807.692313	77221.498175	33.449421
808.532839	77334.292097	33.454439
809.249743	77479.778523	33.459456
810.261514	77637.404310	33.464474
811.262931	77766.870272	33.469492
811.807363	77911.192723	33.474509
812.564091	78044.546000	33.479527
813.680874	78171.471822	33.484544
814.331875	78317.449018	33.489562
815.286413	78470.606105	33.494580
815.916440	78594.110897	33.499597
816.543418	78729.444066	33.504615
817.671940	78871.443742	33.509632
818.086741	79013.726627	33.514650
819.468553	79157.267512	33.519668
820.325135	79303.944639	33.524685
820.963910	79435.358766	33.529703
821.972603	79548.629604	33.534720
822.604990	79688.774696	33.539738
823.669736	79835.111042	33.544756
824.816379	79967.987768	33.549773
825.433368	80078.334240	33.554791
826.620013	80203.609347	33.559808
827.487680	80335.155458	33.564826
828.402219	80465.486494	33.569844
828.979614	80592.306533	33.574861
829.944972	80714.009346	33.579879
830.780861	80833.223060	33.584896
831.309536	80958.155633	33.589914
832.098967	81079.895816	33.594932
832.910338	81201.538158	33.599949
833.431914	81319.629840	33.604967
834.381568	81433.154053	33.609984
835.109446	81559.492971	33.615002
835.688821	81698.723267	33.620020
836.385426	81819.945128	33.625037
837.035340	81950.923118	33.630055
837.968266	82095.752594	33.635072
838.335809	82238.816604	33.640090
839.233089	82388.999063	33.645108
840.171642	82512.677046	33.650125
840.931212	82666.287355	33.655143
842.121012	82802.659307	33.660160
842.720257	82962.098907	33.665178
843.652663	83095.124445	33.670196
844.390504	83237.659196	33.675213
845.089488	83400.330638	33.680231
845.997409	83545.502496	33.685248
846.654116	83707.721321	33.690266
847.624343	83849.443436	33.695284
848.675884	84010.783159	33.700301
849.205732	84177.751947	33.705319
850.059150	84318.287961	33.710336
851.165640	84475.490849	33.715354
851.966711	84639.640985	33.720372
852.269972	84805.234676	33.725389
853.122288	84947.628385	33.730407
854.274137	85092.820442	33.735424
854.838276	85289.684367	33.740442
855.505170	85449.022662	33.745460
856.436396	85615.986294	33.750477
857.086016	85779.574906	33.755495
858.082038	85966.219009	33.760512
858.863692	86145.921587	33.765530
859.819678	86300.700734	33.770548
861.138663	86481.747070	33.775565
861.747080	86653.358509	33.780583
863.117856	86807.357627	33.785600
863.706677	86975.691004	33.790618
864.767041	87138.734258	33.795636
866.085766	87308.872962	33.800653
866.762221	87463.256827	33.805671
867.788371	87618.608982	33.810688
868.265876	87792.629496	33.815706
869.481563	87963.454371	33.820724
870.227753	88116.926264	33.825741
870.891668	88303.150517	33.830759
871.897456	88453.531972	33.835776
872.924615	88607.251761	33.840794
874.112304	88775.562560	33.845812
875.015569	88925.508404	33.850829
875.758723	89087.307884	33.855847
876.821256	89247.201755	33.860864
877.534755	89428.326719	33.865882
878.480003	89561.615281	33.870900
879.686511	89716.053077	33.875917
880.351235	89889.754550	33.880935
881.499114	90035.364198	33.885952
882.395595	90195.019840	33.890970
883.177566	90338.261872	33.895988
883.910476	90501.237109	33.901005
884.834327	90672.452643	33.906023
885.931759	90829.693740	33.911040
886.831331	90979.425472	33.916058
887.481279	91112.632341	33.921076
888.121044	91279.849176	33.926093
889.086320	91451.917806	33.931111
889.754441	91570.898432	33.936128
890.637531	91728.503619	33.941146
891.487681	91893.266299	33.946164
892.555113	92038.547164	33.951181
893.183525	92205.386348	33.956199
894.349958	92337.451626	33.961216
895.142118	92489.539469	33.966234
895.816408	92649.343231	33.971252
896.806827	92826.638669	33.976269
897.398378	92967.839556	33.981287
898.728272	93109.014296	33.986304
899.444098	93281.504362	33.991322
900.066521	93467.877363	33.996340
901.093554	93622.414481	34.001357
901.897166	93774.344031	34.006375
903.028666	93924.049602	34.011392
903.821378	94114.133517	34.016410
904.547453	94276.901481	34.021428
905.765926	94437.082959	34.026445
906.200613	94603.483445	34.031463
907.400478	94778.106802	34.036480
908.274396	94964.190334	34.041498
909.144513	95122.889554	34.046516
910.367110	95297.702774	34.051533
910.981216	95479.136865	34.056551
912.384516	95655.030440	34.061568
913.154997	95822.820589	34.066586
914.002828	95994.029657	34.071604
914.611716	96171.222728	34.076621
915.405822	96354.652704	34.081639
916.717598	96510.072650	34.086656
917.683322	96691.691886	34.091674
918.261111	96878.870638	34.096692
918.893206	97053.287547	34.101709
919.724247	97240.218358	34.106727
920.943179	97418.319811	34.111744
921.799295	97627.504906	34.116762
922.444719	97804.336595	34.121780
923.585129	97978.910335	34.126797
924.683340	98171.944113	34.131815
925.871309	98364.185986	34.136832
927.032015	98546.172824	34.141850
927.838891	98715.970665	34.146868
928.886772	98874.303966	34.151885
929.354656	99083.274269	34.156903
930.275652	99278.814692	34.161920
931.227802	99471.534524	34.166938
931.924958	99629.803928	34.171956
933.244413	99825.877903	34.176973
934.238195	100035.003570	34.181991
935.002013	100213.238197	34.187008
936.024601	100387.227898	34.192026
936.956778	100575.186312	34.197044
937.983704	100758.964940	34.202061
938.799310	100951.357855	34.207079
939.804100	101149.792161	34.212096
941.041696	101333.837747	34.217114
941.507070	101516.245875	34.222132
942.771255	101693.509396	34.227149
943.593139	101891.973401	34.232167
944.670919	102099.380334	34.237184
945.445513	102278.197561	34.242202
946.220088	102450.963573	34.247220
947.202380	102649.926165	34.252237
948.114476	102852.725911	34.257255
949.249854	103028.988047	34.262272
950.208542	103227.060013	34.267290
950.996661	103416.994320	34.272308
952.002345	103568.551615	34.277325
952.934236	103758.869927	34.282343
953.964700	103938.106067	34.287360
955.062152	104101.731700	34.292378
955.915183	104292.047991	34.297396
956.708186	104482.002038	34.302413
957.329880	104665.407247	34.307431
958.557010	104832.378189	34.312448
959.170546	105035.928302	34.317466
960.099697	105212.689026	34.322484
961.244472	105402.256184	34.327501
962.001512	105605.571803	34.332519
962.611783	105808.406697	34.337536
964.044515	106001.033305	34.342554
964.855961	106191.155146	34.347572
965.772560	106399.167939	34.352589
966.689976	106607.555847	34.357607
967.527812	106806.105790	34.362624
968.784894	107008.260676	34.367642
969.380579	107203.763520	34.372660
970.508494	107409.539521	34.377677
971.290417	107641.248075	34.382695
972.079486	107847.235421	34.387712
973.467909	108043.690136	34.392730
974.260647	108264.168693	34.397748
975.405626	108484.527610	34.402765
976.409334	108704.075789	34.407783
977.375488	108898.656147	34.412800
978.547767	109094.837729	34.417818
979.014501	109331.159986	34.422836
980.653538	109554.523930	34.427853
981.340892	109760.720270	34.432871
982.602134	109973.586961	34.437888
983.345017	110182.994492	34.442906
984.255767	110408.715014	34.447924
985.551942	110614.361451	34.452941
986.404847	110852.913299	34.457959
987.119469	111047.487521	34.462976
988.536328	111262.935343	34.467994
989.417497	111493.787070	34.473012
990.427647	111731.776087	34.478029
991.600531	111931.372991	34.483047
992.434458	112129.671985	34.488064
993.840880	112351.400257	34.493082
994.639425	112579.931522	34.498100
995.352511	112776.899830	34.503117
996.607751	113011.072161	34.508135
998.059760	113207.541578	34.513152
999.519741	113396.600697	34.518170
1000.255988	113617.170519	34.523188
1001.473930	113823.943644	34.528205
1002.544507	114040.066040	34.533223
1003.440627	114229.173328	34.538240
1004.704142	114426.075309	34.543258
1005.771486	114639.441368	34.548276
1006.824748	114838.255860	34.553293
1007.766035	115048.238198	34.558311
1008.693383	115246.176979	34.563328
1009.780475	115431.270501	34.568346
1010.374712	115661.470025	34.573364
1011.834569	115862.125004	34.578381
1012.814853	116044.807905	34.583399
1013.570460	116247.697582	34.588416
1014.880802	116452.321453	34.593434
1015.626931	116658.370198	34.598452
1016.318232	116856.942177	34.603469
1017.316344	117072.124673	34.608487
1018.262439	117256.822852	34.613504
1019.618467	117437.489115	34.618522
1020.214564	117653.401234	34.623540
1021.081255	117839.509973	34.628557
1022.059829	118052.131316	34.633575
1022.949846	118261.259413	34.638592
1024.317833	118456.170821	34.643610
1024.854126	118659.025432	34.648628
1025.777848	118870.166951	34.653645
1027.099698	119090.784768	34.658663
1028.090398	119307.619949	34.663680
1029.002685	119503.741415	34.668698
1029.535661	119717.424400	34.673716
1030.638161	119934.638667	34.678733
1031.786996	120176.554224	34.683751
1032.007392	120416.648497	34.688768
1032.895661	120620.510597	34.693786
1034.032796	120858.062470	34.698804
1035.171506	121110.795684	34.703821
1036.685454	121346.338069	34.708839
1037.608634	121578.622081	34.713856
1038.727654	121802.804119	34.718874
1039.899104	122052.156965	34.723892
1041.256026	122292.053856	34.728909
1042.202865	122516.992099	34.733927
1043.172979	122739.216527	34.738944
1044.700583	122962.934567	34.743962
1045.999695	123186.134485	34.748980
1047.223050	123429.636206	34.753997
1048.057164	123663.041315	34.759015
1048.859965	123880.816163	34.764032
1050.177338	124099.331362	34.769050
1051.018261	124318.040886	34.774068
1052.441181	124557.818710	34.779085
1053.691660	124790.048842	34.784103
1054.498157	125015.181446	34.789120
1055.405103	125233.772783	34.794138
1056.584211	125457.389876	34.799156
1057.602308	125690.032916	34.804173
1059.090219	125912.322493	34.809191
1059.838230	126153.897433	34.814208
1060.927039	126372.023534	34.819226
1062.324699	126595.156834	34.824244
1063.406157	126838.557875	34.829261
1064.288016	127060.220965	34.834279
1065.598886	127263.476357	34.839296
1066.617479	127492.343925	34.844314
1067.636326	127739.197105	34.849332
1068.850073	127962.675056	34.854349
1070.300721	128172.339075	34.859367
1070.999983	128397.527411	34.864384
1072.390322	128616.671883	34.869402
1073.420928	128849.780827	34.874420
1074.702009	129051.722331	34.879437
1075.903681	129266.973612	34.884455
1076.811699	129509.169941	34.889472
1077.787840	129736.426381	34.894490
1078.916794	129947.093597	34.899508
1079.823964	130156.696171	34.904525
1080.493772	130373.196392	34.909543
1081.753038	130624.482004	34.914560
1082.616461	130852.614487	34.919578
1083.690025	131081.765985	34.924596
1084.420069	131317.668354	34.929613
1085.990105	131543.027480	34.934631
1087.214132	131783.161405	34.939648
1088.199265	132009.976719	34.944666
1089.124664	132211.617309	34.949684
1089.938470	132436.588020	34.954701
1091.375512	132665.830571	34.959719
1092.044226	132870.610632	34.964736
1093.283936	133074.156938	34.969754
1094.388402	133305.360422	34.974772
1095.012049	133537.075954	34.979789
1096.031729	133760.222125	34.984807
1097.114153	134002.006220	34.989824
1098.016589	134237.889351	34.994842
1099.388065	134464.772613	34.999860
1100.182778	134703.453103	35.004877
1101.128331	134945.000738	35.009895
1102.028903	135214.699881	35.014912
1103.521917	135435.256966	35.019930
1104.399212	135690.056044	35.024948
1105.016843	135950.046858	35.029965
1106.817213	136195.849017	35.034983
1107.632055	136452.451889	35.040000
1108.892726	136682.424294	35.045018
1109.793061	136951.922471	35.050036
1110.535054	137197.932291	35.055053
1111.898024	137462.426783	35.060071
1112.902512	137746.873880	35.065088
1114.455443	138001.516166	35.070106
1115.592003	138254.200699	35.075124
1116.512305	138505.946667	35.080141
1117.800672	138774.026559	35.085159
1118.594082	139046.691087	35.090176
1119.319752	139337.156691	35.095194
1120.673759	139601.733238	35.100212
1121.416774	139855.914951	35.105229
1122.824229	140144.994536	35.110247
1124.157431	140440.022520	35.115264
1125.106718	140705.764997	35.120282
1126.196650	140980.957516	35.125300
1127.024917	141277.876620	35.130317
1128.375402	141559.776104	35.135335
1129.415035	141845.139968	35.140352
1130.674291	142110.360533	35.145370
1131.765738	142395.758514	35.150388
1132.829386	142692.334168	35.155405
1134.392803	142960.541564	35.160423
1135.718847	143264.344316	35.165440
1136.805925	143531.163957	35.170458
1138.557043	143807.855195	35.175476
1139.493256	144088.512556	35.180493
1141.016647	144363.901758	35.185511
1142.004668	144627.043615	35.190528
1143.166684	144889.233079	35.195546
1144.927892	145173.453033	35.200564
1145.815739	145438.595720	35.205581
1147.373863	145698.037603	35.210599
1148.401461	145973.711591	35.215616
1149.540143	146226.581903	35.220634
1150.715667	146478.027686	35.225652
1151.739712	146763.054303	35.230669
1152.955425	147036.169344	35.235687
1154.009278	147295.871093	35.240704
1155.215920	147536.641661	35.245722
1156.547324	147817.314366	35.250740
1157.737982	148100.143007	35.255757
1159.138001	148339.935963	35.260775
1160.118951	148622.017083	35.265792
1161.189776	148875.741752	35.270810
1162.392930	149118.603352	35.275828
1162.957492	149405.147269	35.280845
1164.110901	149693.485884	35.285863
1165.305465	149948.199540	35.290880
1166.310111	150198.139752	35.295898
1167.451192	150472.472684	35.300916
1168.104666	150737.122678	35.305933
1169.516120	150994.965769	35.310951
1170.243310	151259.924431	35.315968
1171.130528	151520.990355	35.320986
1172.361620	151811.983534	35.326004
1173.663666	152107.152654	35.331021
1174.334185	152365.761774	35.336039
1175.197730	152655.198815	35.341056
1176.245025	152956.073389	35.346074
1177.742614	153236.519352	35.351092
1179.023841	153562.029216	35.356109
1180.172689	153836.233571	35.361127
1181.205976	154147.482434	35.366144
1182.240963	154447.102615	35.371162
1183.857853	154728.998622	35.376180
1185.110327	155018.579897	35.381197
1186.179071	155336.415604	35.386215
1187.694959	155642.891289	35.391232
1188.810490	155918.511420	35.396250
1190.424011	156205.226190	35.401268
1191.386097	156524.915883	35.406285
1193.068585	156803.695970	35.411303
1194.467946	157113.386393	35.416320
1195.656292	157396.222578	35.421338
1196.823172	157691.381278	35.426356
1197.964261	157980.622627	35.431373
1199.327517	158277.859024	35.436391
1200.213996	158589.611971	35.441408
1201.580879	158878.099605	35.446426
1202.697242	159177.666867	35.451444
1203.788626	159476.504766	35.456461
1205.135605	159768.084701	35.461479
1206.684326	160060.838596	35.466496
1207.729728	160366.249174	35.471514
1209.205434	160681.333693	35.476532
1210.624952	160980.395064	35.481549
1211.785596	161263.377577	35.486567
1212.928319	161549.777561	35.491584
1214.027735	161850.775727	35.496602
1214.949186	162143.800505	35.501620
1216.105284	162454.270354	35.506637
1217.317428	162749.408157	35.511655
1219.030421	163055.946668	35.516672
1219.941169	163366.286294	35.521690
1221.562774	163646.519654	35.526708
1222.479277	163957.395599	35.531725
1223.340576	164271.759173	35.536743
1224.570811	164577.944578	35.541760
1225.886171	164892.390116	35.546778
1227.213023	165183.263435	35.551796
1228.077116	165516.235196	35.556813
1229.268468	165834.133778	35.561831
1230.752291	166125.723538	35.566848
1231.513326	166443.469332	35.571866
1232.933654	166767.503216	35.576884
1233.845865	167068.798273	35.581901
1235.369016	167405.444250	35.586919
1236.543582	167738.445529	35.591936
1237.722426	168052.061441	35.596954
1238.997194	168348.116198	35.601972
1240.193593	168688.454855	35.606989
1241.559348	169002.059441	35.612007
1242.867619	169336.091297	35.617024
1244.059369	169648.536511	35.622042
1245.659268	169961.690569	35.627060
1246.644761	170278.818276	35.632077
1247.931920	170598.283928	35.637095
1249.303377	170898.311413	35.642112
1250.353398	171199.015716	35.647130
1252.013336	171496.195344	35.652148
1253.150237	171822.445040	35.657165
1254.350156	172117.598302	35.662183
1255.804710	172396.964143	35.667200
1256.817256	172701.795923	35.672218
1258.233986	173030.964707	35.677236
1259.272298	173337.801392	35.682253
1260.701608	173634.144773	35.687271
1261.539635	173945.726383	35.692288
1262.432572	174279.508042	35.697306
1263.793399	174589.687951	35.702324
1264.775442	174901.341017	35.707341
1266.179204	175226.771322	35.712359
1267.523659	175567.352927	35.717376
1268.717155	175904.865502	35.722394
1269.979595	176218.524113	35.727412
1271.564843	176547.436059	35.732429
1272.939916	176878.313903	35.737447
1274.544707	177200.463115	35.742464
1275.511934	177533.887437	35.747482
1277.319983	177867.682910	35.752500
1278.636134	178182.766836	35.757517
1279.786539	178505.608885	35.762535
1281.234914	178822.604128	35.767552
1282.223580	179167.292950	35.772570
1283.579283	179483.533596	35.777588
1284.728592	179828.492414	35.782605
1285.973516	180160.975009	35.787623
1287.430389	180483.017924	35.792640
1288.529454	180816.011221	35.797658
1289.777313	181178.540738	35.802676
1291.051181	181501.280335	35.807693
1292.267716	181833.435995	35.812711
1293.697151	182162.474580	35.817728
1295.308603	182517.935086	35.822746
1296.657053	182853.477017	35.827764
1298.248668	183197.700424	35.832781
1299.052038	183530.468310	35.837799
1300.091091	183871.043203	35.842816
1301.680262	184217.507585	35.847834
1302.693897	184547.975324	35.852852
1304.020796	184920.621200	35.857869
1305.159563	185283.438644	35.862887
1307.054919	185623.883524	35.867904
1308.030382	185952.678184	35.872922
1309.393995	186308.319484	35.877940
1310.190730	186668.194559	35.882957
1311.544961	187032.866796	35.887975
1313.016033	187371.958425	35.892992
1314.521016	187733.322964	35.898010
1315.590520	188103.190033	35.903028
1316.913984	188466.467927	35.908045
1317.975404	188824.447539	35.913063
1319.338847	189180.907161	35.918080
1320.599161	189551.920152	35.923098
1321.994118	189921.136258	35.928116
1323.959259	190285.563999	35.933133
1325.047054	190652.893418	35.938151
1326.506993	190990.853674	35.943168
1327.429301	191345.571766	35.948186
1328.766590	191727.033284	35.953204
1330.257556	192095.295476	35.958221
1331.652622	192468.678870	35.963239
1332.969768	192814.797561	35.968256
1334.279607	193188.389996	35.973274
1335.362804	193549.010422	35.978292
1336.792328	193891.308520	35.983309
1338.068396	194233.735453	35.988327
1339.518264	194563.161750	35.993344
1340.469614	194945.900940	35.998362
1342.018626	195301.745236	36.003380
1343.436117	195634.597560	36.008397
1344.768479	195990.367346	36.013415
1346.277765	196341.666733	36.018432
1347.682263	196721.980904	36.023450
1349.183623	197060.603283	36.028468
1350.498700	197413.095991	36.033485
1351.503343	197778.667242	36.038503
1353.078968	198121.447088	36.043520
1354.221054	198497.816203	36.048538
1355.506009	198853.140216	36.053556
1356.917043	199205.550785	36.058573
1358.257749	199593.382963	36.063591
1359.729510	199951.894134	36.068608
1361.201275	200326.568967	36.073626
1362.570623	200689.785781	36.078644
1364.091207	201057.283526	36.083661
1365.354913	201434.347662	36.088679
1366.840954	201810.298046	36.093696
1367.901407	202183.476815	36.098714
1369.229362	202547.269081	36.103732
1370.558131	202912.739042	36.108749
1371.654709	203317.899870	36.113767
1373.116372	203699.971534	36.118784
1374.213182	204087.387222	36.123802
1375.307514	204461.943853	36.128820
1376.969753	204875.615847	36.133837
1378.368216	205275.621349	36.138855
1379.710169	205653.952353	36.143872
1380.650969	206047.054439	36.148890
1381.752201	206473.017088	36.153908
1383.592267	206897.247755	36.158925
1384.457049	207319.140483	36.163943
1386.304422	207711.873257	36.168960
1387.680327	208121.230290	36.173978
1389.168616	208536.259343	36.178996
1390.291990	208956.023476	36.184013
1391.906625	209363.951054	36.189031
1393.640017	209757.462283	36.194048
1394.730395	210198.202035	36.199066
1396.099325	210611.598491	36.204084
1397.858745	211006.648055	36.209101
1399.193065	211422.885991	36.214119
1400.980573	211834.568968	36.219136
1402.234280	212258.113003	36.224154
1403.624348	212662.983508	36.229172
1405.326829	213078.013588	36.234189
1406.790423	213497.948491	36.239207
1408.224881	213892.519528	36.244224
1409.882461	214312.401059	36.249242
1410.706290	214734.377756	36.254260
1412.332429	215129.837119	36.259277
1413.607210	215547.375140	36.264295
1414.782571	215963.153772	36.269312
1416.532741	216391.918884	36.274330
1417.634435	216794.177003	36.279348
1419.481859	217297.165814	36.284365
1420.896399	217711.363804	36.289383
1422.393237	218100.686054	36.294400
1423.504025	218518.772772	36.299418
1425.075555	218953.827092	36.304436
1426.786696	219355.436992	36.309453
1428.092262	219770.830314	36.314471
1429.463081	220166.404279	36.319488
1431.280178	220553.042292	36.324506
1432.396332	220951.429822	36.329524
1434.039253	221328.219735	36.334541
1435.170927	221732.017622	36.339559
1436.793822	222115.696712	36.344576
1438.207002	222517.901947	36.349594
1439.212256	222914.334380	36.354612
1440.952393	223305.719696	36.359629
1442.141427	223720.462688	36.364647
1443.638871	224124.387268	36.369664
1444.857159	224526.225907	36.374682
1446.096719	224964.002200	36.379700
1447.572324	225368.900143	36.384717
1448.924813	225784.004971	36.389735
1450.393242	226202.597301	36.394752
1452.137062	226632.905662	36.399770
1453.280522	227048.633755	36.404788
1454.826661	227461.833109	36.409805
1455.941526	227908.708901	36.414823
1457.405937	228339.780785	36.419840
1459.256953	228762.205231	36.424858
1460.254860	229194.550898	36.429876
1462.150875	229631.194871	36.434893
1463.760532	230058.464142	36.439911
1465.454663	230505.939495	36.444928
1467.071623	230951.219291	36.449946
1468.310404	231362.704233	36.454964
1469.947402	231795.562748	36.459981
1471.705822	232230.307649	36.464999
1473.241801	232633.593816	36.470016
1475.382777	233068.176614	36.475034
1476.893336	233512.974296	36.480052
1478.466107	233911.203264	36.485069
1479.520626	234333.090920	36.490087
1481.583675	234762.992484	36.495104
1482.537565	235183.578291	36.500122
1483.942162	235609.399725	36.505140
1485.723610	236032.366003	36.510157
1487.126691	236470.382618	36.515175
1488.667273	236888.793280	36.520192
1490.382599	237293.992833	36.525210
1491.747077	237744.999366	36.530228
1493.070805	238187.351889	36.535245
1494.619168	238613.132019	36.540263
1496.000800	239022.099375	36.545280
1497.531164	239458.121386	36.550298
1499.047867	239908.397109	36.555316
1500.583059	240336.114011	36.560333
1501.908692	240770.978996	36.565351
1503.649037	241204.938262	36.570368
1505.129234	241638.001532	36.575386
1506.494571	242081.880572	36.580404
1507.857296	242527.208921	36.585421
1509.629802	242954.968477	36.590439
1510.838284	243406.928683	36.595456
1512.447768	243834.691459	36.600474
1513.712311	244283.316483	36.605492
1515.472650	244730.234810	36.610509
1516.905646	245163.185841	36.615527
1518.353750	245607.159826	36.620544
1519.678580	246056.311650	36.625562
1521.144696	246519.234541	36.630580
1522.669392	246955.577432	36.635597
1523.964184	247395.718547	36.640615
1525.659922	247848.825774	36.645632
1527.006826	248315.226091	36.650650
1528.156502	248771.600175	36.655668
1529.891789	249228.792799	36.660685
1531.702089	249652.187907	36.665703
1532.690163	250096.778208	36.670720
1534.829167	250516.893989	36.675738
1536.250191	250942.183916	36.680756
1537.940770	251382.925659	36.685773
1539.526773	251846.776479	36.690791
1540.925732	252267.422745	36.695808
1542.695999	252711.836218	36.700826
1543.927230	253166.373290	36.705844
1545.824989	253579.393778	36.710861
1547.313621	254040.748041	36.715879
1548.528432	254505.196271	36.720896
1550.460434	254929.719799	36.725914
1552.126448	255372.577811	36.730932
1553.561287	255822.180723	36.735949
1554.933120	256281.142712	36.740967
1556.667087	256722.618623	36.745984
1558.112286	257175.142031	36.751002
1559.331062	257657.831291	36.756020
1561.062147	258098.495471	36.761037
1562.407312	258554.922731	36.766055
1563.972556	259028.892919	36.771072
1565.756291	259516.265554	36.776090
1566.835086	259987.902983	36.781108
1568.294899	260452.644159	36.786125
1569.824255	260933.327211	36.791143
1571.324115	261431.543466	36.796160
1572.701674	261906.942353	36.801178
1573.833138	262408.623461	36.806196
1575.325503	262910.753053	36.811213
1577.164893	263399.945850	36.816231
1578.640568	263896.133669	36.821248
1580.331114	264414.259759	36.826266
1581.912228	264909.286753	36.831284
1583.515638	265411.905463	36.836301
1585.673705	265926.143341	36.841319
1587.136194	266437.396529	36.846336
1588.931552	266933.632001	36.851354
1590.627291	267433.922716	36.856372
1592.205639	267933.978427	36.861389
1594.150666	268453.559116	36.866407
1595.771255	268944.842982	36.871424
1597.230567	269423.705506	36.876442
1598.891028	269946.685018	36.881460
1600.644013	270440.943244	36.886477
1602.024975	270955.102123	36.891495
1603.745982	271477.587308	36.896512
1605.437998	271955.138742	36.901530
1607.014754	272467.663106	36.906548
1608.987975	272974.329508	36.911565
1610.371239	273465.393564	36.916583
1611.915786	273970.097062	36.921600
1613.574997	274491.724564	36.926618
1615.575942	274991.270640	36.931636
1617.760936	275485.298557	36.936653
1619.367367	275966.973801	36.941671
1620.479518	276466.333831	36.946688
1622.400535	276974.425023	36.951706
1623.915667	277459.694529	36.956724
1625.848414	277951.879923	36.961741
1627.061153	278449.746295	36.966759
1628.655666	278947.243844	36.971776
1630.602892	279462.031970	36.976794
1631.729057	279971.137295	36.981812
1633.665536	280445.433731	36.986829
1635.321101	280931.943136	36.991847
1636.540396	281447.862864	36.996864
1638.165750	281916.415693	37.001882
1639.654075	282406.886576	37.006900
1641.845811	282900.618654	37.011917
1643.403223	283353.023680	37.016935
1644.897808	283853.193398	37.021952
1647.002483	284312.897749	37.026970
1648.378583	284782.831011	37.031988
1650.097014	285264.924730	37.037005
1651.639653	285765.716249	37.042023
1652.920349	286245.186891	37.047040
1654.267643	286719.133072	37.052058
1656.000744	287215.011773	37.057076
1657.584851	287737.280009	37.062093
1659.109758	288242.867733	37.067111
1660.197143	288751.675723	37.072128
1661.623702	289249.859245	37.077146
1663.400891	289769.650217	37.082164
1664.917974	290320.420427	37.087181
1666.665273	290828.147160	37.092199
1668.047860	291366.108160	37.097216
1669.733147	291900.029251	37.102234
1671.309289	292430.308595	37.107252
1672.612108	292979.173151	37.112269
1674.230583	293533.698380	37.117287
1676.027915	294102.034763	37.122304
1677.811413	294636.157122	37.127322
1679.615855	295197.299189	37.132340
1680.969413	295771.644739	37.137357
1682.753959	296327.527125	37.142375
1684.157845	296903.586108	37.147392
1686.110939	297461.670482	37.152410
1687.727490	298024.633521	37.157428
1689.479855	298615.053193	37.162445
1691.191343	299203.012773	37.167463
1692.759147	299775.423409	37.172480
1694.661039	300332.765250	37.177498
1696.381488	300920.256809	37.182516
1698.193940	301509.837961	37.187533
1699.939193	302075.298456	37.192551
1701.522756	302680.632160	37.197568
1703.714354	303256.451028	37.202586
1705.718552	303816.601588	37.207604
1707.357275	304406.194348	37.212621
1709.061359	304994.579021	37.217639
1710.688670	305584.344164	37.222656
1712.648225	306147.104330	37.227674
1714.946767	306699.366945	37.232692
1716.788445	307282.660410	37.237709
1718.847325	307858.777776	37.242727
1720.098037	308445.030981	37.247744
1722.011271	309006.257099	37.252762
1723.673807	309567.647921	37.257780
1725.372234	310131.975086	37.262797
1726.923934	310717.071142	37.267815
1728.597709	311300.060517	37.272832
1730.738232	311859.960419	37.277850
1732.130912	312426.735024	37.282868
1733.880733	313013.128002	37.287885
1735.825761	313590.875567	37.292903
1737.123661	314178.426479	37.297920
1738.899806	314738.112361	37.302938
1740.497717	315321.567386	37.307956
1742.244713	315905.552035	37.312973
1743.884743	316484.369433	37.317991
1745.633983	317092.011734	37.323008
1747.329448	317665.173365	37.328026
1749.008009	318258.673434	37.333044
1750.935690	318837.374081	37.338061
1752.862858	319379.275647	37.343079
1754.546660	319957.956649	37.348096
1756.090867	320515.376903	37.353114
1757.990002	321062.551783	37.358132
1759.524464	321634.209790	37.363149
1761.239515	322212.409749	37.368167
1762.659062	322785.194284	37.373184
1764.612078	323363.116580	37.378202
1766.156593	323936.683142	37.383220
1768.022914	324512.730727	37.388237
1770.086213	325094.758366	37.393255
1771.402508	325671.902028	37.398272
1773.164759	326267.197242	37.403290
1775.204163	326846.496110	37.408308
1776.719301	327438.672655	37.413325
1778.692505	328023.938173	37.418343
1780.320529	328610.169101	37.423360
1781.687143	329214.743160	37.428378
1783.733272	329831.106515	37.433396
1785.351852	330448.955840	37.438413
1787.438072	331043.237309	37.443431
1789.277066	331647.074141	37.448448
1790.902948	332271.783369	37.453466
1793.131200	332893.416143	37.458484
1794.483506	333499.014942	37.463501
1796.542434	334095.757579	37.468519
1798.474769	334724.476801	37.473536
1800.082282	335367.509775	37.478554
1802.264974	335974.341198	37.483572
1803.393661	336589.336378	37.488589
1805.686129	337204.488056	37.493607
1807.532548	337843.010101	37.498624
1809.347696	338494.323784	37.503642
1811.385120	339111.247259	37.508660
1812.741984	339745.334152	37.513677
1814.624980	340371.203654	37.518695
1816.312425	340997.732472	37.523712
1818.039892	341657.753334	37.528730
1820.211246	342312.666583	37.533748
1821.658697	342940.734175	37.538765
1823.536490	343571.692701	37.543783
1825.431092	344221.880213	37.548800
1827.270946	344892.424496	37.553818
1829.011906	345525.715833	37.558836
1830.441463	346176.309542	37.563853
1832.351546	346837.729013	37.568871
1834.153121	347504.334894	37.573888
1835.616807	348175.124148	37.578906
1838.045837	348819.755728	37.583924
1839.669437	349500.677018	37.588941
1841.380875	350186.142089	37.593959
1843.425616	350853.167834	37.598976
1845.437762	351501.866094	37.603994
1847.476239	352171.995140	37.609012
1848.939851	352860.074880	37.614029
1850.937646	353524.911948	37.619047
1853.231208	354190.553103	37.624064
1854.764807	354847.199443	37.629082
1856.774983	355530.326058	37.634100
1858.742377	356199.314777	37.639117
1860.691682	356876.619205	37.644135
1862.261014	357553.087499	37.649152
1863.900531	358222.428633	37.654170
1865.872394	358894.571624	37.659188
1867.512780	359580.764783	37.664205
1869.951845	360231.926739	37.669223
1872.045362	360916.932052	37.674240
1873.802759	361581.987960	37.679258
1876.016382	362235.134448	37.684276
1877.495087	362864.973676	37.689293
1879.457039	363510.554988	37.694311
1881.544963	364168.333839	37.699328
1882.934888	364810.208266	37.704346
1885.133839	365419.820472	37.709364
1886.876434	366077.649931	37.714381
1888.817045	366737.414451	37.719399
1890.766393	367385.116200	37.724416
1892.020673	368036.904549	37.729434
1893.986800	368689.325449	37.734452
1895.710768	369376.883587	37.739469
1897.521410	370060.406982	37.744487
1899.146532	370736.059604	37.749504
1900.923946	371408.910012	37.754522
1902.953669	372081.909554	37.759540
1904.505913	372797.969372	37.764557
1906.429071	373495.488651	37.769575
1908.015534	374187.140301	37.774592
1909.795668	374896.095509	37.779610
1911.819527	375600.938475	37.784628
1913.395808	376321.794451	37.789645
1915.498061	377035.802761	37.794663
1917.469539	377739.622878	37.799680
1918.979212	378468.891466	37.804698
1921.217058	379201.473749	37.809716
1923.198013	379955.004893	37.814733
1924.660156	380683.245746	37.819751
1927.067108	381414.764092	37.824768
1929.018035	382169.316563	37.829786
1930.983095	382893.395228	37.834804
1932.929163	383659.884016	37.839821
1934.707861	384411.092803	37.844839
1937.036349	385136.660389	37.849856
1939.070270	385878.792386	37.854874
1941.738556	386617.380058	37.859892
1943.817858	387368.877434	37.864909
1945.823695	388101.480975	37.869927
1948.161899	388854.244866	37.874944
1949.688089	389593.536027	37.879962
1951.663618	390326.854263	37.884980
1953.693148	391074.115224	37.889997
1955.704459	391813.553415	37.895015
1957.618809	392554.688593	37.900032
1959.393745	393295.271427	37.905050
1961.571550	394046.518054	37.910068
1963.482034	394814.418934	37.915085
1965.279366	395543.258390	37.920103
1967.201480	396271.857028	37.925120
1969.007677	397045.776745	37.930138
1971.278890	397815.595219	37.935156
1973.323956	398562.240347	37.940173
1975.393114	399317.758690	37.945191
1977.574021	400057.804875	37.950208
1979.157927	400829.812704	37.955226
1981.057423	401592.092596	37.960244
1983.030767	402344.228915	37.965261
1985.222628	403095.067920	37.970279
1987.355689	403855.855882	37.975296
1989.325272	404637.074538	37.980314
1991.157906	405371.138071	37.985332
1993.141201	406129.178683	37.990349
1995.393381	406893.793068	37.995367
1997.602275	407648.157504	38.000384
1999.444439	408405.399689	38.005402
2001.507639	409150.904934	38.010420
2003.506731	409917.454076	38.015437
2005.536949	410672.221508	38.020455
2007.709623	411391.198703	38.025472
2009.466660	412117.825331	38.030490
2011.173338	412836.461034	38.035508
2013.404873	413583.210476	38.040525
2015.293785	414331.667433	38.045543
2017.213470	415056.414486	38.050560
2019.089205	415794.396336	38.055578
2020.909238	416522.437812	38.060596
2023.006007	417283.264060	38.065613
2024.342570	418055.109625	38.070631
2026.611781	418794.714929	38.075648
2028.206151	419560.344119	38.080666
2030.044740	420332.165571	38.085684
2031.814163	421111.977674	38.090701
2033.339982	421890.945089	38.095719
2035.797948	422690.119708	38.100736
2037.420083	423492.622748	38.105754
2039.319126	424290.623262	38.110772
2041.649833	425091.742779	38.115789
2043.493559	425917.628653	38.120807
2045.337190	426746.930299	38.125824
2047.049226	427575.972515	38.130842
2049.278358	428407.129266	38.135860
2051.018950	429224.262465	38.140877
2052.830178	430068.798177	38.145895
2055.213957	430926.069560	38.150912
2057.109573	431788.048471	38.155930
2059.108912	432635.905388	38.160948
2061.343693	433496.855223	38.165965
2062.910533	434367.046285	38.170983
2065.713935	435237.659249	38.176000
2067.513991	436098.028652	38.181018
2070.091977	436946.393867	38.186036
2072.533084	437819.450098	38.191053
2074.673981	438709.325868	38.196071
2076.688118	439545.187190	38.201088
2078.633409	440412.861710	38.206106
2081.468395	441289.262999	38.211124
2083.818784	442142.584075	38.216141
2085.812884	443016.222985	38.221159
2087.721074	443871.018632	38.226176
2089.824681	444745.988530	38.231194
2092.270686	445610.697531	38.236212
2094.535592	446494.425908	38.241229
2096.124737	447349.544300	38.246247
2098.663042	448216.816692	38.251264
2100.936541	449081.012234	38.256282
2102.877108	449941.535335	38.261300
2105.221094	450816.980997	38.266317
2107.334407	451683.374711	38.271335
2109.928006	452530.989954	38.276352
2111.730196	453409.048665	38.281370
2113.622207	454262.375009	38.286388
2115.900006	455134.214285	38.291405
2118.224242	455997.108950	38.296423
2120.736697	456874.298609	38.301440
2122.394201	457733.944082	38.306458
2124.105273	458594.000015	38.311476
2126.766291	459454.722883	38.316493
2128.557164	460326.929283	38.321511
2130.466209	461189.826554	38.326528
2132.273940	462091.480872	38.331546
2134.864913	462968.345708	38.336564
2137.339008	463812.635817	38.341581
2139.035305	464678.148558	38.346599
2141.369379	465566.467316	38.351616
2143.540468	466462.658282	38.356634
2145.478191	467319.221002	38.361652
2147.380485	468188.337015	38.366669
2149.467990	469029.031501	38.371687
2151.880857	469855.687889	38.376704
2154.287667	470729.458943	38.381722
2155.892224	471585.636455	38.386740
2158.235697	472428.566730	38.391757
2159.486408	473271.084324	38.396775
2162.081071	474142.597498	38.401792
2163.956629	475022.525638	38.406810
2166.052198	475899.901073	38.411828
2168.277773	476756.956263	38.416845
2170.116118	477645.457317	38.421863
2172.535113	478536.699686	38.426880
2174.550282	479417.257545	38.431898
2176.372003	480321.898277	38.436916
2178.596501	481227.640418	38.441933
2180.377571	482142.855292	38.446951
2182.730102	483049.597431	38.451968
2184.770030	483974.727612	38.456986
2186.571685	484903.485658	38.462004
2189.102250	485843.689328	38.467021
2191.171651	486786.848382	38.472039
2193.570518	487707.789533	38.477056
2195.626718	488649.590271	38.482074
2197.782055	489616.263352	38.487092
2200.227856	490565.319043	38.492109
2202.048233	491528.610901	38.497127
2204.200110	492467.516805	38.502144
2206.414047	493410.349281	38.507162
2208.575071	494392.707276	38.512180
2210.898644	495377.304175	38.517197
2212.998298	496355.119641	38.522215
2215.355995	497325.873281	38.527232
2217.668615	498317.014583	38.532250
2219.537377	499288.948063	38.537268
2222.254263	500251.655049	38.542285
2224.571845	501238.638912	38.547303
2227.472697	502229.756524	38.552320
2229.660913	503200.604365	38.557338
2232.064751	504169.493787	38.562356
2234.857412	505133.420538	38.567373
2236.817856	506129.100937	38.572391
2239.086328	507103.035342	38.577408
2241.414077	508077.305505	38.582426
2243.298476	509064.045601	38.587444
2245.605203	510044.202129	38.592461
2248.037774	511030.732173	38.597479
2249.958320	512011.841338	38.602496
2252.619310	512974.720656	38.607514
2254.746933	513974.681100	38.612532
2256.847765	514979.422191	38.617549
2258.910131	515983.601930	38.622567
2261.466164	516955.682716	38.627584
2263.929403	517949.339060	38.632602
2265.459477	518956.541384	38.637620
2267.817919	519972.713193	38.642637
2269.875046	520957.829685	38.647655
2272.209710	521955.786420	38.652672
2274.582882	522986.621191	38.657690
2276.584208	524011.705045	38.662708
2279.095676	524995.329402	38.667725
2281.347958	525987.798219	38.672743
2283.625805	527019.988137	38.677760
2285.862059	528056.596785	38.682778
2288.199737	529081.433689	38.687796
2290.389162	530079.384666	38.692813
2292.715454	531097.287132	38.697831
2294.991035	532125.097619	38.702848
2297.383009	533119.840505	38.707866
2299.499145	534100.918749	38.712884
2301.870038	535076.905851	38.717901
2304.107872	536081.038371	38.722919
2306.689254	537052.580231	38.727936
2309.105495	538040.340915	38.732954
2310.858867	539055.621691	38.737972
2313.421101	540034.414922	38.742989
2315.612876	541035.443742	38.748007
2317.786380	542026.795268	38.753024
2320.557322	543054.153950	38.758042
2322.326020	544070.183542	38.763060
2324.224217	545078.724042	38.768077
2326.563222	546095.469799	38.773095
2328.550723	547131.866358	38.778112
2330.915914	548149.816910	38.783130
2333.174421	549215.335642	38.788148
2335.823919	550257.727323	38.793165
2338.068273	551301.263785	38.798183
2340.244173	552373.642834	38.803200
2342.552446	553432.844891	38.808218
2344.645592	554488.129558	38.813236
2347.246969	555548.124639	38.818253
2349.410809	556625.550383	38.823271
2351.715808	557693.719898	38.828288
2354.207415	558796.650938	38.833306
2355.941903	559889.465514	38.838324
2358.350968	560983.385990	38.843341
2360.967687	562069.043089	38.848359
2363.249020	563184.106369	38.853376
2365.710391	564285.934787	38.858394
2368.054482	565399.293452	38.863412
2370.468080	566529.271282	38.868429
2372.671417	567642.161034	38.873447
2375.387493	568738.048387	38.878464
2377.968114	569871.223716	38.883482
2379.775458	571023.757269	38.888500
2382.538296	572142.694770	38.893517
2385.319752	573267.404826	38.898535
2387.677544	574398.962343	38.903552
2390.377853	575513.448513	38.908570
2392.392586	576656.254604	38.913588
2395.168015	577777.354141	38.918605
2397.878471	578889.834318	38.923623
2400.425644	580031.192183	38.928640
2403.152622	581159.021175	38.933658
2405.542209	582274.112122	38.938676
2407.853136	583375.572735	38.943693
2410.709780	584510.950103	38.948711
2412.653801	585651.388048	38.953728
2415.245729	586770.251218	38.958746
2417.776140	587909.529413	38.963764
2420.399048	589032.993122	38.968781
2422.763498	590151.783190	38.973799
2425.091006	591274.285275	38.978816
2427.403030	592387.963961	38.983834
2429.895558	593511.683187	38.988852
2432.315978	594659.312377	38.993869
2435.265429	595780.136559	38.998887
2437.452734	596906.742229	39.003904
2439.677740	598015.449429	39.008922
2441.797208	599156.630259	39.013940
2444.475861	600299.461150	39.018957
2447.062829	601442.145306	39.023975
2449.235267	602564.453763	39.028992
2451.357864	603678.850383	39.034010
2453.703976	604859.193611	39.039028
2456.133358	605994.194719	39.044045
2458.386643	607107.236931	39.049063
2460.765702	608213.292724	39.054080
2463.276645	609334.184169	39.059098
2465.597754	610456.347516	39.064116
2468.065640	611578.875847	39.069133
2470.288261	612689.875099	39.074151
2472.461657	613816.131695	39.079168
2475.539752	614942.326071	39.084186
2477.688994	616082.515318	39.089204
2480.173546	617229.234362	39.094221
2482.868591	618366.398500	39.099239
2484.803436	619506.171144	39.104256
2487.505172	620656.349117	39.109274
2489.766672	621820.877160	39.114292
2492.697426	622981.621787	39.119309
2495.106406	624142.828644	39.124327
2497.346718	625310.886002	39.129344
2499.323379	626494.052182	39.134362
2501.796876	627667.962853	39.139380
2504.812482	628847.751182	39.144397
2507.329216	630032.737100	39.149415
2509.603248	631243.005855	39.154432
2511.993223	632443.928171	39.159450
2514.345293	633639.876703	39.164468
2516.129695	634849.664658	39.169485
2518.656513	636083.555430	39.174503
2520.912256	637341.657101	39.179520
2523.310260	638560.750302	39.184538
2525.673619	639803.762587	39.189556
2528.007183	641073.378777	39.194573
2530.766689	642363.126647	39.199591
2532.976436	643629.305378	39.204608
2535.784914	644899.120218	39.209626
2538.085975	646182.377956	39.214644
2540.650912	647486.875372	39.219661
2543.615603	648772.240445	39.224679
2545.922116	650051.866792	39.229696
2548.920096	651336.550956	39.234714
2551.580966	652646.348440	39.239732
2554.347339	653936.619408	39.244749
2556.982024	655242.243195	39.249767
2559.733197	656555.748093	39.254784
2562.273622	657838.075704	39.259802
2565.390727	659148.584990	39.264820
2568.148872	660435.320527	39.269837
2570.586277	661703.663200	39.274855
2573.091607	663010.071429	39.279872
2575.823430	664306.857118	39.284890
2578.032965	665608.632960	39.289908
2580.906471	666917.838793	39.294925
2583.784414	668212.980843	39.299943
2586.201106	669524.743350	39.304960
2588.784838	670818.188099	39.309978
2591.454760	672123.183102	39.314996
2593.984387	673414.243889	39.320013
2596.725043	674721.754101	39.325031
2598.903990	676016.445652	39.330048
2601.930654	677322.154924	39.335066
2604.562960	678642.511453	39.340084
2606.914586	679946.821725	39.345101
2609.579721	681256.662238	39.350119
2612.120665	682564.101873	39.355136
2614.955342	683846.962751	39.360154
2617.761098	685166.460106	39.365172
2620.309019	686485.164310	39.370189
2623.133751	687800.901090	39.375207
2625.194691	689114.190139	39.380224
2627.633890	690416.602052	39.385242
2630.163569	691704.167334	39.390260
2632.564189	692984.521895	39.395277
2635.173528	694268.381586	39.400295
2637.566494	695539.439751	39.405312
2640.044183	696829.006942	39.410330
2642.882705	698143.576881	39.415348
2645.056309	699445.562736	39.420365
2647.639916	700740.346447	39.425383
2649.965280	702064.186998	39.430400
2652.409736	703373.431225	39.435418
2655.388752	704705.391163	39.440436
2657.599725	706047.087209	39.445453
2660.199941	707374.686606	39.450471
2662.856558	708719.017744	39.455488
2665.756078	710054.034029	39.460506
2668.085094	711415.732872	39.465524
2670.953089	712806.988357	39.470541
2673.494507	714173.759760	39.475559
2676.060718	715528.178684	39.480576
2678.981202	716912.665350	39.485594
2681.636698	718307.361871	39.490612
2684.120501	719696.660299	39.495629
2686.942105	721059.650166	39.500647
2689.178005	722466.390423	39.505664
2691.758038	723876.941673	39.510682
2695.238675	725290.072059	39.515700
2697.771702	726678.051393	39.520717
2700.957216	728091.394383	39.525735
2703.413892	729534.960480	39.530752
2706.174383	730951.093867	39.535770
2709.211150	732342.480335	39.540788
2711.706651	733767.555543	39.545805
2714.772056	735192.780494	39.550823
2717.443907	736619.152404	39.555840
2719.865449	738038.401189	39.560858
2722.912427	739466.921857	39.565876
2726.262205	740896.717022	39.570893
2728.905696	742330.171877	39.575911
2731.480795	743762.294206	39.580928
2734.322831	745185.333540	39.585946
2737.003015	746611.003588	39.590964
2739.810002	748058.830144	39.595981
2742.673780	749491.738047	39.600999
2745.339046	750943.245147	39.606016
2748.194230	752379.666058	39.611034
2750.445569	753815.625142	39.616052
2753.432824	755254.349410	39.621069
2756.383352	756699.706955	39.626087
2758.806137	758172.112097	39.631104
2761.675070	759612.403976	39.636122
2764.711930	761043.240440	39.641140
2766.916145	762517.748054	39.646157
2769.924840	763990.507894	39.651175
2772.208315	765443.864069	39.656192
2775.425988	766907.213832	39.661210
2778.311306	768381.890084	39.666228
2780.758831	769850.841000	39.671245
2783.604262	771325.188659	39.676263
2786.360199	772809.874869	39.681280
2788.962199	774294.190642	39.686298
2791.787059	775756.406971	39.691316
2794.217498	777265.356097	39.696333
2797.269887	778744.426659	39.701351
2799.701997	780222.170860	39.706368
2802.339439	781737.478587	39.711386
2805.607296	783218.256158	39.716404
2808.357577	784726.491010	39.721421
2811.286312	786211.666805	39.726439
2814.057285	787677.579837	39.731456
2816.680485	789112.322742	39.736474
2819.831383	790562.968167	39.741492
2822.368436	792021.703364	39.746509
2825.283563	793452.631330	39.751527
2827.957504	794930.152696	39.756544
2830.576604	796401.151933	39.761562
2833.289785	797871.827793	39.766580
2835.900561	799325.464671	39.771597
2838.682450	800806.627826	39.776615
2841.136601	802323.359212	39.781632
2843.562015	803810.059280	39.786650
2846.761180	805293.719147	39.791668
2849.456484	806818.720779	39.796685
2852.093003	808353.712410	39.801703
2854.944630	809866.322440	39.806720
2857.635045	811382.338861	39.811738
2860.449676	812928.834952	39.816756
2862.816791	814481.843611	39.821773
2865.570712	816030.474855	39.826791
2868.235030	817602.841778	39.831808
2871.141492	819175.191076	39.836826
2873.619742	820764.521740	39.841844
2876.104427	822384.120662	39.846861
2878.762628	823993.928362	39.851879
2882.133682	825587.617911	39.856896
2884.992282	827231.285870	39.861914
2887.791692	828858.122365	39.866932
2890.674141	830500.626394	39.871949
2893.694121	832139.380977	39.876967
2896.704475	833776.944982	39.881984
2899.117758	835430.120642	39.887002
2902.001117	837074.810321	39.892020
2904.635927	838728.711067	39.897037
2907.749541	840404.932075	39.902055
2911.025941	842080.249042	39.907072
2913.860224	843766.678058	39.912090
2917.241475	845420.911345	39.917108
2920.017961	847113.996985	39.922125
2923.290369	848776.120544	39.927143
2926.216386	850461.573918	39.932160
2929.070341	852145.128293	39.937178
2932.252548	853823.220905	39.942196
2935.128937	855515.573673	39.947213
2938.129714	857201.425171	39.952231
2941.365312	858887.845408	39.957248
2944.034476	860569.336850	39.962266
2947.292125	862254.441288	39.967284
2950.142554	863965.814892	39.972301
2952.967102	865644.914983	39.977319
2955.770678	867340.320520	39.982336
2958.612985	869032.047294	39.987354
2961.820932	870744.257959	39.992372
2964.960730	872454.152093	39.997389
2967.546148	874160.357892	40.002407
2970.823509	875847.380518	40.007424
2973.738618	877556.914032	40.012442
2976.830266	879270.954879	40.017460
2979.766996	880984.040319	40.022477
2982.769531	882704.252899	40.027495
2985.950577	884385.566439	40.032512
2988.521594	886084.852770	40.037530
2991.943645	887796.928082	40.042548
2995.173313	889517.219928	40.047565
2997.777600	891216.157587	40.052583
3000.914975	892933.130554	40.057600
3003.814872	894660.337436	40.062618
3006.505424	896349.929439	40.067636
3009.627809	898016.101120	40.072653
3012.335394	899697.177781	40.077671
3015.664956	901360.791857	40.082688
3018.649496	903030.234121	40.087706
3021.613360	904711.799751	40.092724
3024.602808	906404.602043	40.097741
3027.312460	908065.276154	40.102759
3030.166553	909745.058670	40.107776
3032.533908	911443.361195	40.112794
3035.612961	913122.084403	40.117812
3038.431945	914834.943595	40.122829
3040.815589	916571.267958	40.127847
3044.008499	918301.914359	40.132864
3046.756121	920031.125961	40.137882
3049.883314	921777.773991	40.142900
3052.512797	923563.384684	40.147917
3055.245622	925324.309458	40.152935
3058.559191	927101.442711	40.157952
3061.106332	928897.768327	40.162970
3064.337488	930679.961291	40.167988
3067.299735	932468.022585	40.173005
3070.219763	934303.281476	40.178023
3073.521170	936127.023334	40.183040
3075.963458	937956.210928	40.188058
3079.158251	939786.074051	40.193076
3082.437352	941623.892605	40.198093
3085.572593	943476.672640	40.203111
3088.381479	945343.470019	40.208128
3091.460421	947185.284543	40.213146
3094.718090	949047.711228	40.218164
3097.745849	950936.807024	40.223181
3100.552080	952827.821034	40.228199
3103.832194	954723.972805	40.233216
3106.510356	956635.040716	40.238234
3109.744955	958581.915813	40.243252
3112.969813	960539.479127	40.248269
3115.770588	962498.598529	40.253287
3118.872144	964461.204361	40.258304
3122.030443	966449.506960	40.263322
3124.912350	968435.996081	40.268340
3128.193182	970429.151882	40.273357
3130.917675	972426.489104	40.278375
3134.030317	974414.970450	40.283392
3137.035404	976421.210159	40.288410
3140.251056	978427.882116	40.293428
3143.450531	980457.922335	40.298445
3146.521490	982485.119687	40.303463
3149.442592	984514.153937	40.308480
3152.683931	986552.440177	40.313498
3155.634027	988572.627352	40.318516
3158.900455	990615.488706	40.323533
3162.029175	992656.083390	40.328551
3165.494252	994691.321505	40.333568
3168.749985	996742.091797	40.338586
3171.898290	998787.961721	40.343604
3175.330442	1000848.873424	40.348621
3178.219126	1002896.797546	40.353639
3181.439598	1004961.293628	40.358656
3184.494394	1007023.898948	40.363674
3187.491857	1009056.091414	40.368692
3190.517914	1011119.919009	40.373709
3193.989195	1013208.398482	40.378727
3197.408199	1015258.824487	40.383744
3200.309022	1017311.492800	40.388762
3203.914293	1019379.651023	40.393780
3206.982233	1021447.812993	40.398797
3209.975095	1023522.187661	40.403815
3213.496850	1025570.669071	40.408832
3215.906722	1027610.176483	40.413850
3219.008874	1029636.847435	40.418868
3222.392377	1031662.640284	40.423885
3225.245652	1033683.730834	40.428903
3228.468595	1035712.326746	40.433920
3231.603580	1037770.873297	40.438938
3234.420973	1039804.122117	40.443956
3237.431716	1041841.318765	40.448973
3240.315338	1043913.440702	40.453991
3243.674864	1045985.770079	40.459008
3246.613217	1048073.858555	40.464026
3249.300843	1050153.405179	40.469044
3252.312733	1052254.341434	40.474061
3255.632439	1054384.049823	40.479079
3258.667359	1056502.793354	40.484096
3261.676206	1058652.728353	40.489114
3264.572561	1060812.794134	40.494132
3267.905364	1062961.378009	40.499149
3270.762939	1065121.582921	40.504167
3274.016231	1067295.265501	40.509184
3277.503930	1069495.766391	40.514202
3280.733075	1071691.400114	40.519220
3283.923236	1073885.393423	40.524237
3286.962274	1076109.952123	40.529255
3290.017811	1078316.175411	40.534272
3293.528654	1080540.096789	40.539290
3296.991516	1082792.300472	40.544308
3300.153476	1085033.102649	40.549325
3303.078817	1087284.875244	40.554343
3306.383228	1089529.919322	40.559360
3309.743428	1091810.418341	40.564378
3313.620261	1094060.752925	40.569396
3317.007334	1096320.445441	40.574413
3320.061695	1098615.882144	40.579431
3323.268847	1100889.340675	40.584448
3326.719535	1103172.668286	40.589466
3329.821437	1105456.801956	40.594484
3333.162265	1107750.308936	40.599501
3336.308498	1110047.059421	40.604519
3339.642293	1112360.687094	40.609536
3342.408419	1114682.352341	40.614554
3345.981318	1117015.714861	40.619572
3349.185293	1119337.668822	40.624589
3352.193220	1121688.474519	40.629607
3355.751682	1124008.437547	40.634624
3358.936484	1126345.296738	40.639642
3361.869700	1128696.446940	40.644660
3365.555403	1131046.625557	40.649677
3368.726193	1133402.296322	40.654695
3372.177439	1135767.393133	40.659712
3375.022043	1138147.918908	40.664730
3378.761674	1140539.628555	40.669748
3382.300114	1142911.937203	40.674765
3385.489582	1145299.789239	40.679783
3389.144960	1147661.436650	40.684800
3392.497502	1150038.423090	40.689818
3395.777908	1152433.993579	40.694836
3398.863588	1154831.244174	40.699853
3402.351559	1157234.884561	40.704871
3406.121143	1159631.343220	40.709888
3409.351095	1162024.911168	40.714906
3412.565535	1164421.628975	40.719924
3416.254515	1166802.008398	40.724941
3419.779337	1169225.388270	40.729959
3423.174202	1171629.505054	40.734976
3426.221694	1174032.571317	40.739994
3429.638989	1176450.638004	40.745012
3433.107462	1178831.009741	40.750016
3436.281828	1181166.812788	40.755021
3439.352724	1183465.157533	40.760026
3442.715872	1185709.657009	40.765031
3445.883212	1187863.501897	40.770036
3449.026861	1189931.851820	40.775040
3451.920109	1191934.390645	40.780045
3454.831067	1193849.451362	40.785050
3458.026300	1195674.081671	40.790055
3460.501364	1197439.142760	40.795060
3463.514419	1199114.929644	40.800064
3465.718628	1200726.890871	40.805069
3468.519530	1202237.436686	40.810074
3470.966703	1203689.282653	40.815079
3472.751980	1205090.495742	40.820084
3475.199036	1206387.769513	40.825088
3477.278885	1207637.560608	40.830093
3479.224170	1208832.466179	40.835098
3480.915554	1209945.763535	40.840103
3482.511246	1210990.024695	40.845108
3484.580433	1211998.332854	40.850112
3486.108164	1212935.501716	40.855117
3487.709614	1213812.322889	40.860122
3489.264048	1214651.580478	40.865127
3490.620543	1215441.064340	40.870132
3492.248339	1216177.727460	40.875136
3493.441353	1216852.825297	40.880141
3494.766406	1217495.554557	40.885146
3496.111672	1218112.583560	40.890151
3497.411098	1218654.949796	40.895156
3498.576134	1219145.685305	40.900160
3499.393278	1219629.795082	40.905165
3500.345356	1220061.129358	40.910170
3501.531657	1220467.064809	40.915175
3502.580632	1220832.344726	40.920180
3503.560690	1221176.867772	40.925184
3504.124442	1221470.985617	40.930189
3505.256975	1221727.343675	40.935194
3506.042561	1221976.926435	40.940199
3506.622271	1222192.621708	40.945204
3507.297728	1222380.269000	40.950208
3507.820190	1222564.385089	40.955213
3508.436242	1222685.150995	40.960218
3509.227465	1222789.913305	40.965223
3509.939724	1222905.801163	40.970228
3510.587754	1222974.530405	40.975232
3510.974932	1223037.417579	40.980237
3511.492648	1223087.860630	40.985242
3512.089768	1223097.102069	40.990247
3512.552993	1223090.207815	40.995252
3512.690478	1223064.967849	41.000256
3513.026003	1223036.799795	41.005261
3513.555842	1222977.684455	41.010266
3514.111080	1222916.042431	41.015271
3514.286204	1222850.445984	41.020276
3514.804952	1222763.682980	41.025280
3515.327926	1222657.769743	41.030285
3515.532804	1222525.192137	41.035290
3515.876296	1222410.429567	41.040295
3516.226082	1222265.864862	41.045300
3516.594951	1222121.479741	41.050304
3516.837415	1221975.429820	41.055309
3517.359953	1221799.248080	41.060314
3517.396251	1221608.285831	41.065319
3517.429100	1221425.164939	41.070324
3517.578317	1221230.152501	41.075328
3517.705195	1221020.280065	41.080333
3518.045658	1220808.775336	41.085338
3518.384005	1220584.460443	41.090343
3518.391518	1220380.561671	41.095348
3518.720112	1220140.623141	41.100352
3518.800577	1219910.527038	41.105357
3518.884966	1219674.158071	41.110362
3519.334829	1219399.864712	41.115367
3519.135536	1219152.022013	41.120372
3519.418438	1218890.440589	41.125376
3519.487682	1218620.467786	41.130381
3519.794132	1218339.877872	41.135386
3519.799344	1218068.858068	41.140391
3520.008485	1217814.432267	41.145396
3520.178305	1217513.998594	41.150400
3520.185079	1217213.480568	41.155405
3520.261312	1216912.652862	41.160410
3520.652509	1216617.740583	41.165415
3520.270219	1216327.801759	41.170420
3520.560301	1216005.001246	41.175424
3520.679903	1215719.528041	41.180429
3520.428647	1215402.016363	41.185434
3520.753239	1215097.860452	41.190439
3520.954595	1214778.738766	41.195444
3521.243936	1214431.235195	41.200448
3520.984548	1214101.855897	41.205453
3520.905695	1213784.308779	41.210458
3521.366042	1213450.651964	41.215463
3521.088451	1213119.434403	41.220468
3521.407394	1212796.051959	41.225472
3521.367874	1212471.210619	41.230477
3521.599957	1212123.185136	41.235482
3521.422092	1211781.755815	41.240487
3521.634058	1211426.291439	41.245492
3521.762077	1211071.190658	41.250496
3521.580917	1210738.024170	41.255501
3521.593774	1210405.740330	41.260506
3521.869237	1210050.825344	41.265511
3521.405986	1209688.422326	41.270516
3521.783172	1209330.725015	41.275520
3521.789199	1208991.139445	41.280525
3521.647677	1208641.721135	41.285530
3521.900040	1208271.138646	41.290535
3521.515642	1207918.057874	41.295540
3521.783722	1207550.793010	41.300544
3521.546782	1207213.565339	41.305549
3521.765341	1206842.229263	41.310554
3521.863839	1206481.193260	41.315559
3521.795247	1206127.187468	41.320564
3521.824789	1205742.496309	41.325568
3521.883291	1205384.857172	41.330573
3521.827072	1205020.932200	41.335578
3521.930035	1204645.613254	41.340583
3521.935079	1204288.562656	41.345588
3521.990317	1203919.854160	41.350592
3522.016541	1203562.093308	41.355597
3521.888167	1203195.050591	41.360602
3521.992803	1202827.005583	41.365607
3521.703262	1202448.871397	41.370612
3522.198990	1202054.730834	41.375616
3522.232670	1201695.807158	41.380621
3521.776526	1201318.086134	41.385626
3521.916996	1200942.490359	41.390631
3521.536576	1200580.461503	41.395636
3522.026345	1200210.383295	41.400640
3521.881079	1199826.121951	41.405645
3521.858051	1199439.372185	41.410650
3522.265608	1199069.319280	41.415655
3521.595421	1198698.854202	41.420660
3521.593082	1198318.022749	41.425664
3521.662402	1197952.825519	41.430669
3521.591678	1197589.315005	41.435674
3522.081091	1197201.467923	41.440679
3521.809098	1196830.427312	41.445684
3522.083673	1196437.958131	41.450688
3521.889935	1196069.290827	41.455693
3521.502848	1195672.271611	41.460698
3521.960608	1195292.830898	41.465703
3521.476655	1194938.310245	41.470708
3521.704795	1194551.151972	41.475712
3521.761859	1194156.478706	41.480717
3521.530819	1193778.636791	41.485722
3521.433933	1193409.011842	41.490727
3521.342814	1193035.225808	41.495732
3521.373673	1192669.472627	41.500736
3521.513915	1192285.729096	41.505741
3521.393315	1191906.604413	41.510746
3521.616427	1191511.701560	41.515751
3521.357451	1191153.312717	41.520756
3521.699521	1190777.882225	41.525760
3521.441944	1190402.993192	41.530765
3521.239970	1190010.865489	41.535770
3521.437974	1189620.992393	41.540775
3521.356992	1189254.733827	41.545780
3521.584495	1188872.790795	41.550784
3521.138573	1188497.606560	41.555789
3521.032796	1188132.965172	41.560794
3521.224674	1187754.989036	41.565799
3521.189625	1187359.341288	41.570804
3521.497244	1186981.195546	41.575808
3521.327931	1186614.764636	41.580813
3521.042310	1186243.811574	41.585818
3521.257684	1185857.038536	41.590823
3521.272449	1185466.976708	41.595828
3521.215224	1185098.067924	41.600832
3521.293238	1184714.807715	41.605837
3520.962093	1184337.985691	41.610842
3520.968503	1183957.316208	41.615847
3521.248485	1183572.997212	41.620852
3520.842456	1183193.280756	41.625856
3520.710635	1182835.424187	41.630861
3521.000634	1182449.325918	41.635866
3521.118967	1182071.982790	41.640871
3521.131031	1181703.668403	41.645876
3521.231875	1181312.620795	41.650880
3520.936874	1180934.321446	41.655885
3521.098593	1180566.090050	41.660890
3521.238069	1180171.748281	41.665895
3520.982192	1179790.062821	41.670900
3520.897403	1179410.958585	41.675904
3520.962000	1179029.729664	41.680909
3520.811602	1178645.116699	41.685914
3520.879678	1178260.250868	41.690919
3520.618738	1177901.604423	41.695924
3520.568499	1177522.450994	41.700928
3520.464376	1177153.361979	41.705933
3520.642974	1176775.247232	41.710938
3520.746047	1176392.593504	41.715943
3520.421027	1176018.936452	41.720948
3520.735253	1175626.200498	41.725952
3520.884563	1175251.279082	41.730957
3520.461808	1174887.455219	41.735962
3520.384630	1174502.712480	41.740967
3520.266583	1174135.768864	41.745972
3520.271143	1173765.761726	41.750976
3520.554909	1173391.721602	41.755981
3520.097664	1173008.911526	41.760986
3520.639606	1172640.150648	41.765991
3520.344689	1172276.783641	41.770996
3520.152684	1171887.244880	41.776000
3520.495202	1171534.003163	41.781005
3520.166477	1171169.243847	41.786010
3520.127293	1170780.540720	41.791015
3519.713139	1170411.874156	41.796020
3520.020006	1170058.066634	41.801024
3519.985341	1169679.188920	41.806029
3519.912179	1169303.404506	41.811034
3520.370362	1168944.211490	41.816039
3520.127548	1168567.930191	41.821044
3519.835208	1168194.461864	41.826048
3520.015136	1167836.560102	41.831053
3519.507043	1167471.005508	41.836058
3519.883142	1167077.993171	41.841063
3519.908014	1166723.628621	41.846068
3519.876443	1166360.656202	41.851072
3519.646772	1165995.519170	41.856077
3519.408888	1165630.735778	41.861082
3519.788529	1165258.174787	41.866087
3519.848460	1164908.215104	41.871092
3519.973855	1164539.139709	41.876096
3519.905110	1164157.978114	41.881101
3519.192733	1163781.996525	41.886106
3519.293992	1163420.404398	41.891111
3519.236639	1163079.506687	41.896116
3519.443328	1162706.225683	41.901120
3519.346200	1162344.213975	41.906125
3519.228809	1161978.589242	41.911130
3519.593575	1161622.027643	41.916135
3519.312512	1161271.692107	41.921140
3519.393756	1160899.248317	41.926144
3519.047452	1160537.625537	41.931149
3519.087377	1160172.227080	41.936154
3519.475766	1159815.822441	41.941159
3519.118242	1159479.372916	41.946164
3518.801062	1159118.403948	41.951168
3518.806815	1158749.224163	41.956173
3518.814584	1158384.179354	41.961178
3518.976809	1158036.108237	41.966183
3518.784650	1157698.476946	41.971188
3519.122094	1157333.304811	41.976192
3519.086882	1156985.669583	41.981197
3518.571921	1156633.833113	41.986202
3518.683246	1156264.839750	41.991207
3518.629818	1155926.504074	41.996212
3518.694777	1155563.051580	42.001216
3518.534649	1155190.621039	42.006221
3518.587092	1154869.990671	42.011226
3518.687301	1154512.611216	42.016231
3518.791834	1154155.869328	42.021236
3518.236780	1153804.985939	42.026240
3518.737761	1153450.213378	42.031245
3518.395292	1153112.217598	42.036250
3518.621064	1152761.988105	42.041255
3518.109975	1152399.074644	42.046260
3518.153543	1152053.656827	42.051264
3518.375653	1151714.531470	42.056269
3518.344903	1151384.327748	42.061274
3518.479345	1151014.299454	42.066279
3517.920960	1150669.458271	42.071284
3518.222196	1150321.232497	42.076288
3518.777756	1149988.666245	42.081293
3518.350041	1149634.736956	42.086298
3518.226072	1149277.797010	42.091303
3518.033656	1148938.940316	42.096308
3518.327574	1148571.082906	42.101312
3517.997728	1148246.985480	42.106317
3518.181700	1147900.609113	42.111322
3517.882980	1147557.132581	42.116327
3517.989782	1147227.024942	42.121332
3517.910388	1146889.155313	42.126336
3518.050601	1146542.412715	42.131341
3517.897085	1146214.559554	42.136346
3517.752698	1145859.477220	42.141351
3517.527768	1145517.277838	42.146356
3517.626591	1145158.410927	42.151360
3517.750840	1144843.700604	42.156365
3517.657530	1144511.559893	42.161370
3517.849886	1144171.764912	42.166375
3517.704807	1143823.942639	42.171380
3517.599141	1143489.937916	42.176384
3517.394482	1143149.383906	42.181389
3517.480536	1142819.668292	42.186394
3517.406150	1142492.519771	42.191399
3517.152201	1142166.518985	42.196404
3517.287444	1141822.408438	42.201408
3517.230120	1141494.246692	42.206413
3517.079100	1141165.890273	42.211418
3517.345755	1140815.809902	42.216423
3517.178333	1140505.444250	42.221428
3517.119928	1140188.399398	42.226432
3516.867902	1139850.013434	42.231437
3516.970210	1139520.184583	42.236442
3517.485420	1139191.216399	42.241447
3517.004516	1138869.226432	42.246452
3517.118877	1138531.265482	42.251456
3517.167895	1138204.401333	42.256461
3516.872651	1137889.346570	42.261466
3517.151886	1137545.694086	42.266471
3516.857402	1137211.514309	42.271476
3517.083478	1136901.347585	42.276480
3516.980539	1136561.587664	42.281485
3516.896598	1136221.802866	42.286490
3517.300820	1135895.307804	42.291495
3517.080108	1135572.884905	42.296500
3516.863160	1135251.296711	42.301504
3516.738627	1134925.304049	42.306509
3516.608337	1134594.637280	42.311514
3516.627912	1134258.794872	42.316519
3516.375691	1133959.935942	42.321524
3516.473519	1133635.917818	42.326528
3516.859379	1133307.176334	42.331533
3516.558278	1132982.708981	42.336538
3516.728452	1132668.027905	42.341543
3516.650178	1132355.935239	42.346548
3516.207109	1132029.912468	42.351552
3516.375912	1131711.753358	42.356557
3516.159094	1131397.821296	42.361562
3516.167659	1131092.389323	42.366567
3516.402088	1130772.832385	42.371572
3516.313129	1130448.175474	42.376576
3516.223689	1130128.823372	42.381581
3516.089438	1129824.102798	42.386586
3516.314261	1129484.787254	42.391591
3515.978429	1129176.354215	42.396596
3516.146644	1128870.197884	42.401600
3516.315568	1128549.567299	42.406605
3515.999801	1128243.740012	42.411610
3516.258252	1127931.903163	42.416615
3516.289482	1127613.046201	42.421620
3516.391402	1127307.667169	42.426624
3516.457921	1126992.857948	42.431629
3516.339630	1126667.880335	42.436634
3516.212535	1126358.203236	42.441639
3516.065182	1126053.078866	42.446644
3516.430030	1125733.293345	42.451648
3516.200829	1125395.980959	42.456653
3515.942854	1125093.770072	42.461658
3516.071116	1124771.681809	42.466663
3516.118273	1124482.615571	42.471668
3515.756764	1124161.142227	42.476672
3515.957833	1123847.362695	42.481677
3515.586066	1123532.611889	42.486682
3515.724250	1123222.613954	42.491687
3515.644712	1122917.679994	42.496692
3515.502003	1122609.120869	42.501696
3515.997640	1122312.722218	42.506701
3515.579601	1122004.363964	42.511706
3515.758002	1121684.081007	42.516711
3515.779029	1121377.423675	42.521716
3515.754400	1121085.042607	42.526720
3515.618000	1120777.710119	42.531725
3515.537083	1120469.969822	42.536730
3515.347246	1120148.512518	42.541735
3515.457740	1119849.754596	42.546740
3515.403229	1119549.387593	42.551744
3515.605541	1119254.963743	42.556749
3515.040055	1118942.261103	42.561754
3515.364791	1118623.771712	42.566759
3515.267694	1118347.737428	42.571764
3515.265734	1118045.848049	42.576768
3515.428908	1117746.678203	42.581773
3515.124364	1117457.861806	42.586778
3515.518925	1117143.371086	42.591783
3515.328442	1116838.585358	42.596788
3514.958678	1116528.664372	42.601792
3515.119002	1116250.477838	42.606797
3515.216168	1115954.269297	42.611802
3514.994191	1115632.832159	42.616807
3514.987560	1115337.369348	42.621812
3514.829056	1115049.161836	42.626816
3514.974029	1114766.133356	42.631821
3514.966263	1114468.143637	42.636826
3514.953101	1114162.318315	42.641831
3514.766105	1113876.436622	42.646836
3514.720260	1113576.019375	42.651840
3515.207027	1113288.469395	42.656845
3514.871410	1113016.682717	42.661850
3514.867707	1112706.003581	42.666855
3514.850697	1112411.239872	42.671860
3514.540061	1112122.518639	42.676864
3514.721720	1111827.690187	42.681869
3514.288991	1111528.557794	42.686874
3514.504976	1111243.805314	42.691879
3514.371995	1110986.862983	42.696884
3514.553858	1110680.616381	42.701888
3514.674401	1110379.706652	42.706893
3514.470691	1110106.414918	42.711898
3514.675210	1109806.031878	42.716903
3514.285168	1109541.236486	42.721908
3514.382384	1109243.321320	42.726912
3514.094592	1108957.576196	42.731917
3513.755482	1108692.730633	42.736922
3514.120199	1108408.089871	42.741927
3514.137754	1108132.847523	42.746932
3514.305724	1107848.305037	42.751936
3514.515318	1107566.700610	42.756941
3514.075691	1107274.111839	42.761946
3513.992143	1106981.162040	42.766951
3514.130430	1106712.511674	42.771956
3513.731905	1106447.183392	42.776960
3514.293276	1106150.166592	42.781965
3513.770722	1105874.420200	42.786970
3514.279825	1105598.107715	42.791975
3513.913651	1105310.558078	42.796980
3513.890265	1105043.761571	42.801985
3513.856658	1104779.055241	42.806989
3513.668150	1104511.495329	42.811994
3513.864976	1104227.998813	42.816999
3513.633723	1103958.221029	42.822004
3513.767095	1103684.929857	42.827009
3513.991444	1103408.743177	42.832013
3513.694640	1103145.815578	42.837018
3513.968761	1102847.804114	42.842023
3513.737680	1102573.847720	42.847028
3513.671178	1102311.606101	42.852033
3513.990829	1102018.128949	42.857037
3513.578028	1101759.740773	42.862042
3513.671274	1101491.697896	42.867047
3513.444546	1101204.288654	42.872052
3513.271268	1100931.960107	42.877057
3513.736246	1100667.925915	42.882061
3513.283843	1100413.017166	42.887066
3513.625853	1100142.189290	42.892071
3513.569284	1099878.298023	42.897076
3513.489365	1099590.969986	42.902081
3513.579273	1099308.380134	42.907085
3513.205144	1099061.331875	42.912090
3512.973202	1098797.512345	42.917095
3513.463229	1098529.830985	42.922100
3513.157718	1098252.989624	42.927105
3513.467771	1097992.676156	42.932109
3513.028349	1097746.535078	42.937114
3513.131489	1097467.099119	42.942119
3513.267980	1097200.845141	42.947124
3513.312335	1096934.019213	42.952129
3513.328728	1096668.715539	42.957133
3513.041159	1096418.279292	42.962138
3513.250573	1096152.631493	42.967143
3513.410995	1095899.131229	42.972148
3513.220355	1095627.303761	42.977153
3513.080558	1095340.525287	42.982157
3512.892453	1095101.782679	42.987162
3512.680551	1094824.271918	42.992167
3513.000900	1094583.317144	42.997172
3513.070100	1094328.514129	43.002177
3513.022448	1094058.307253	43.007181
3512.936158	1093811.354675	43.012186
3513.369922	1093547.552396	43.017191
3513.148326	1093278.196846	43.022196
3513.029826	1093037.245614	43.027201
3513.068930	1092771.843021	43.032205
3512.682053	1092512.434016	43.037210
3513.082454	1092243.307601	43.042215
3513.159997	1091987.627141	43.047220
3512.952317	1091722.022298	43.052225
3513.112277	1091461.706868	43.057229
3512.837671	1091219.742911	43.062234
3512.471652	1090948.667298	43.067239
3512.788653	1090685.990161	43.072244
3512.598346	1090448.958552	43.077249
3512.910693	1090179.935877	43.082253
3512.755961	1089918.736157	43.087258
3512.642310	1089666.522210	43.092263
3512.743247	1089414.931830	43.097268
3512.574736	1089171.996867	43.102273
3512.740049	1088915.007497	43.107277
3512.440514	1088665.077145	43.112282
3512.632833	1088404.418145	43.117287
3512.572561	1088157.587138	43.122292
3512.564031	1087876.141698	43.127297
3512.517967	1087640.784526	43.132301
3512.519527	1087400.904893	43.137306
3512.251925	1087145.724086	43.142311
3512.608219	1086889.182524	43.147316
3512.585683	1086648.890289	43.152321
3512.692038	1086402.814823	43.157325
3512.250934	1086148.478492	43.162330
3512.347137	1085898.835040	43.167335
3512.268479	1085648.825454	43.172340
3512.025709	1085400.461266	43.177345
3512.037385	1085161.919311	43.182349
3512.003874	1084928.456114	43.187354
3512.149157	1084677.310300	43.192359
3512.343336	1084431.802432	43.197364
3512.007573	1084180.904725	43.202369
3512.185753	1083933.171408	43.207373
3512.394180	1083700.382898	43.212378
3511.978567	1083459.055473	43.217383
3512.018598	1083216.107706	43.222388
3511.809820	1082971.463577	43.227393
3512.124089	1082718.473085	43.232397
3511.776328	1082466.155437	43.237402
3511.751370	1082232.479304	43.242407
3511.640776	1082000.150330	43.247412
3511.260442	1081753.081389	43.252417
3511.763285	1081533.583162	43.257421
3511.390510	1081319.497345	43.262426
3511.445085	1081069.543357	43.267431
3511.572900	1080828.201774	43.272436
3511.340225	1080602.454199	43.277441
3511.406743	1080362.829373	43.282445
3511.318727	1080150.857908	43.287450
3511.401690	1079914.089658	43.292455
3511.698853	1079681.786673	43.297460
3511.478724	1079445.527883	43.302465
3511.494413	1079215.938837	43.307469
3511.745758	1078978.238405	43.312474
3511.555449	1078743.192128	43.317479
3511.822347	1078504.796582	43.322484
3511.254662	1078275.648044	43.327489
3511.517533	1078027.344356	43.332493
3511.207648	1077831.351954	43.337498
3511.179634	1077610.151208	43.342503
3511.489467	1077369.106711	43.347508
3511.478047	1077125.703997	43.352513
3511.219414	1076911.522377	43.357517
3511.088331	1076695.870942	43.362522
3511.326633	1076465.841508	43.367527
3510.976794	1076219.957360	43.372532
3510.896259	1076009.072275	43.377537
3511.190414	1075788.513027	43.382541
3511.433578	1075570.066318	43.387546
3511.436551	1075340.796677	43.392551
3511.096123	1075094.380083	43.397556
3510.961715	1074886.054043	43.402561
3511.190933	1074653.452311	43.407565
3511.088301	1074438.475625	43.412570
3511.226931	1074213.747603	43.417575
3511.201031	1073981.831829	43.422580
3511.168275	1073744.623003	43.427585
3511.153757	1073530.749083	43.432589
3510.957738	1073322.661893	43.437594
3511.060637	1073082.807700	43.442599
3510.908586	1072837.507570	43.447604
3510.733060	1072639.865393	43.452609
3510.946824	1072421.201689	43.457613
3510.841335	1072205.657232	43.462618
3510.929335	1071961.912137	43.467623
3510.881983	1071751.722419	43.472628
3510.747715	1071532.407748	43.477633
3510.902290	1071325.340303	43.482637
3510.472205	1071113.170559	43.487642
3510.612015	1070890.901303	43.492647
3510.917297	1070686.476513	43.497652
3510.839396	1070466.052406	43.502657
3510.815090	1070228.785985	43.507661
3510.662568	1070018.835522	43.512666
3510.585698	1069803.384105	43.517671
3510.637766	1069595.787450	43.522676
3510.418402	1069373.419659	43.527681
3510.763786	1069158.546450	43.532685
3510.590437	1068950.097038	43.537690
3510.635442	1068729.679029	43.542695
3510.766647	1068515.873760	43.547700
3510.472793	1068302.803387	43.552705
3510.296522	1068074.605347	43.557709
3510.590914	1067866.422429	43.562714
3510.326299	1067661.978744	43.567719
3510.403573	1067459.972057	43.572724
3510.140111	1067255.416844	43.577729
3510.338329	1067046.256728	43.582733
3510.276926	1066831.551782	43.587738
3510.022655	1066622.546246	43.592743
3510.275160	1066426.533522	43.597748
3510.073147	1066222.314515	43.602753
3510.090372	1065997.269398	43.607757
3510.145092	1065797.418195	43.612762
3510.195500	1065588.419332	43.617767
3510.037548	1065402.059859	43.622772
3509.918349	1065194.228637	43.627777
3510.253692	1064976.595176	43.632781
3509.945503	1064771.858554	43.637786
3510.171380	1064581.558573	43.642791
3510.214304	1064364.622720	43.647796
3510.146550	1064175.223225	43.652801
3509.973494	1063969.279478	43.657805
3510.091875	1063751.055727	43.662810
3509.907773	1063563.483148	43.667815
3509.901159	1063370.965626	43.672820
3509.819079	1063173.544309	43.677825
3510.015621	1062956.142519	43.682829
3509.596125	1062758.665609	43.687834
3509.588154	1062571.800364	43.692839
3510.034361	1062379.269827	43.697844
3509.541820	1062158.195134	43.702849
3509.892647	1061963.162411	43.707853
3509.774257	1061775.999466	43.712858
3509.782483	1061587.461210	43.717863
3509.781202	1061380.332994	43.722868
3509.524719	1061187.106121	43.727873
3509.855398	1060984.049187	43.732877
3509.594749	1060800.728612	43.737882
3509.535138	1060608.797296	43.742887
3509.755371	1060412.671752	43.747892
3509.570139	1060202.640137	43.752897
3509.656475	1059999.972428	43.757901
3509.575920	1059820.827640	43.762906
3509.322615	1059615.601000	43.767911
3509.740168	1059438.384599	43.772916
3509.195509	1059249.568347	43.777921
3509.574383	1059040.459170	43.782925
3509.332152	1058847.533182	43.787930
3509.223672	1058656.794309	43.792935
3509.530244	1058490.259818	43.797940
3509.556627	1058306.230846	43.802945
3509.282905	1058105.479740	43.807949
3509.432155	1057925.753718	43.812954
3509.110250	1057740.510588	43.817959
3509.192413	1057529.465775	43.822964
3509.069543	1057331.456165	43.827969
3509.365809	1057141.658236	43.832973
3509.347737	1056963.566702	43.837978
3509.410243	1056792.106099	43.842983
3509.491332	1056616.010910	43.847988
3509.089118	1056427.652762	43.852993
3509.332213	1056226.940899	43.857997
3509.186901	1056051.828849	43.863002
3509.141514	1055856.645200	43.868007
3509.013394	1055677.373559	43.873012
3508.989822	1055511.863867	43.878017
3509.146505	1055304.866803	43.883021
3508.999247	1055117.675161	43.888026
3508.995049	1054932.285370	43.893031
3509.289309	1054772.967731	43.898036
3509.226982	1054571.763931	43.903041
3509.219968	1054380.185515	43.908045
3509.033396	1054198.657856	43.913050
3508.755922	1054025.817399	43.918055
3508.710944	1053855.826061	43.923060
3508.712240	1053671.260875	43.928065
3508.937068	1053482.216752	43.933069
3508.912286	1053316.255706	43.938074
3508.944841	1053113.729481	43.943079
3508.674763	1052924.458465	43.948084
3508.650098	1052782.495770	43.953089
3508.866129	1052603.839216	43.958093
3508.930746	1052425.587636	43.963098
3509.000133	1052218.875103	43.968103
3509.291418	1052046.747153	43.973108
3508.665270	1051881.131427	43.978113
3509.072826	1051685.725747	43.983117
3508.992528	1051517.308193	43.988122
3508.562504	1051329.938271	43.993127
3508.776150	1051153.261140	43.998132
3508.673107	1050998.723847	44.003137
3508.518481	1050810.615627	44.008141
3508.691543	1050626.499357	44.013146
3508.286735	1050452.217302	44.018151
3508.948557	1050289.718801	44.023156
3508.462741	1050119.588657	44.028161
3508.843099	1049934.353800	44.033165
3508.657474	1049771.979675	44.038170
3508.506313	1049588.750764	44.043175
3508.781639	1049413.358947	44.048180
3508.692708	1049237.442520	44.053185
3509.080226	1049056.712993	44.058189
3508.703436	1048881.797784	44.063194
3508.856319	1048715.186796	44.068199
3509.049456	1048539.201727	44.073204
3508.322469	1048373.497530	44.078209
3508.195031	1048187.322632	44.083213
3508.212175	1048009.129600	44.088218
3508.212129	1047857.962679	44.093223
3508.373056	1047680.797258	44.098228
3508.391643	1047499.112323	44.103233
3508.291010	1047334.721942	44.108237
3508.399870	1047168.168214	44.113242
3508.218345	1047006.774287	44.118247
3508.275190	1046837.033129	44.123252
3508.157395	1046684.598440	44.128257
3508.206890	1046499.206638	44.133261
3508.319022	1046326.061279	44.138266
3508.384636	1046167.209281	44.143271
3508.350232	1046009.624539	44.148276
3508.262543	1045844.898139	44.153281
3508.287381	1045672.036435	44.158285
3508.009702	1045502.792368	44.163290
3508.310288	1045346.292477	44.168295
3508.023189	1045158.979782	44.173300
3507.785363	1045015.597380	44.178305
3508.110537	1044867.579098	44.183309
3507.812324	1044702.660269	44.188314
3507.897018	1044533.520110	44.193319
3507.987618	1044359.350995	44.198324
3507.889764	1044212.640623	44.203329
3508.173434	1044061.516624	44.208333
3507.729723	1043918.429562	44.213338
3507.837246	1043740.181002	44.218343
3507.911864	1043570.626741	44.223348
3507.689878	1043418.602453	44.228353
3507.797738	1043258.790718	44.233357
3507.472596	1043092.862346	44.238362
3507.600272	1042961.829973	44.243367
3507.661045	1042815.539627	44.248372
3507.566748	1042654.294492	44.253377
3507.886680	1042476.646741	44.258381
3507.946903	1042337.397560	44.263386
3507.622524	1042179.461884	44.268391
3507.851083	1042013.506689	44.273396
3507.801718	1041875.326944	44.278401
3507.878384	1041717.698630	44.283405
3507.751543	1041551.208327	44.288410
3507.595752	1041373.700303	44.293415
3507.735589	1041230.447823	44.298420
3507.287280	1041099.563030	44.303425
3507.734520	1040937.115707	44.308429
3507.774182	1040775.117388	44.313434
3507.447656	1040626.320139	44.318439
3507.587746	1040467.002718	44.323444
3507.574522	1040311.959170	44.328449
3507.475387	1040177.321934	44.333453
3507.652005	1040033.549223	44.338458
3507.583214	1039880.049472	44.343463
3507.118161	1039733.377885	44.348468
3507.156521	1039582.172421	44.353473
3507.530279	1039424.236779	44.358477
3507.500111	1039288.986599	44.363482
3507.271985	1039135.492536	44.368487
3507.643561	1038976.287650	44.373492
3507.143604	1038833.175459	44.378497
3507.706797	1038693.655451	44.383501
3507.411266	1038546.247784	44.388506
3507.174903	1038403.274503	44.393511
3507.498209	1038258.077993	44.398516
3506.734976	1038101.935962	44.403521
3507.142044	1037940.568165	44.408525
3507.235619	1037811.547474	44.413530
3506.817191	1037665.780729	44.418535
3507.365160	1037533.970907	44.423540
3506.840581	1037397.789061	44.428545
3507.441495	1037251.746875	44.433549
3507.334011	1037105.914252	44.438554
3506.896043	1036970.481435	44.443559
3507.460424	1036818.050284	44.448564
3507.221866	1036662.071592	44.453569
3507.011255	1036523.205010	44.458573
3507.317731	1036393.052364	44.463578
3507.022943	1036256.611282	44.468583
3507.227794	1036093.578801	44.473588
3507.115815	1035959.131789	44.478593
3506.939795	1035816.856031	44.483597
3507.152329	1035678.769374	44.488602
3506.968208	1035536.681281	44.493607
3507.238807	1035400.126097	44.498612
3506.913269	1035274.018099	44.503617
3506.961276	1035116.691163	44.508621
3507.054125	1034978.316602	44.513626
3506.631862	1034867.115719	44.518631
3507.310751	1034716.930434	44.523636
3507.054826	1034570.281777	44.528641
3507.081807	1034431.420674	44.533645
3506.756635	1034298.226643	44.538650
3506.681279	1034163.827043	44.543655
3506.885989	1034028.120035	44.548660
3507.022070	1033900.356557	44.553665
3506.754086	1033743.236450	44.558669
3506.571222	1033605.453886	44.563674
3506.904846	1033485.777873	44.568679
3507.105285	1033325.181471	44.573684
3507.017152	1033208.182152	44.578689
3507.042949	1033077.320811	44.583693
3506.940524	1032942.121912	44.588698
3506.799489	1032802.376791	44.593703
3506.876173	1032649.621611	44.598708
3506.310516	1032510.035895	44.603713
3506.618191	1032390.147062	44.608717
3506.613206	1032274.566478	44.613722
3506.237337	1032138.812326	44.618727
3506.602230	1032009.322164	44.623732
3506.262462	1031876.363095	44.628737
3506.583564	1031746.583624	44.633741
3506.650306	1031607.258407	44.638746
3506.258489	1031489.788990	44.643751
3506.461566	1031344.141676	44.648756
3506.507883	1031224.658138	44.653761
3506.308567	1031108.214016	44.658765
3506.273929	1031000.648246	44.663770
3506.083998	1030862.799098	44.668775
3506.441323	1030731.053514	44.673780
3506.044484	1030603.883301	44.678785
3506.496359	1030474.246390	44.683789
3506.526767	1030342.932833	44.688794
3505.903886	1030230.607291	44.693799
3506.241053	1030106.210001	44.698804
3506.107951	1029984.502147	44.703809
3506.017348	1029854.262300	44.708813
3506.192094	1029749.252752	44.713818
3505.909927	1029639.764604	44.718823
3506.372616	1029501.580670	44.723828
3505.905797	1029381.464254	44.728833
3506.164463	1029264.615694	44.733837
3506.097894	1029131.933673	44.738842
3506.039132	1029026.949013	44.743847
3506.130559	1028911.960951	44.748852
3506.242715	1028792.027086	44.753857
3506.071524	1028655.185855	44.758861
3506.110460	1028535.452276	44.763866
3506.259691	1028430.228416	44.768871
3506.170418	1028293.074219	44.773876
3506.077573	1028190.404384	44.778881
3506.123998	1028059.325143	44.783885
3506.157224	1027939.095353	44.788890
3506.286157	1027817.587775	44.793895
3506.179163	1027696.503943	44.798900
3506.402758	1027572.359625	44.803905
3506.326466	1027439.057716	44.808909
3506.073572	1027321.477712	44.813914
3506.207776	1027223.015822	44.818919
3506.253934	1027094.626946	44.823924
3506.042465	1026971.122297	44.828929
3506.049685	1026856.977898	44.833933
3506.075369	1026755.037360	44.838938
3505.934182	1026620.757650	44.843943
3506.242943	1026488.435577	44.848948
3505.809849	1026379.296010	44.853953
3505.845527	1026269.398758	44.858957
3505.991243	1026151.534692	44.863962
3506.030809	1026036.399136	44.868967
3505.718796	1025907.460542	44.873972
3505.710993	1025812.486096	44.878977
3505.705326	1025676.707685	44.883981
3505.942032	1025586.922670	44.888986
3505.761237	1025470.842585	44.893991
3505.945439	1025336.478463	44.898996
3506.056137	1025240.311716	44.904001
3505.634248	1025107.011157	44.909005
3505.678683	1025001.158498	44.914010
3505.557253	1024905.218085	44.919015
3505.778173	1024796.230707	44.924020
3505.353969	1024678.526427	44.929025
3505.703202	1024551.192498	44.934029
3505.925698	1024450.922440	44.939034
3505.566533	1024342.797287	44.944039
3505.579496	1024224.526759	44.949044
3505.639994	1024141.048840	44.954049
3505.365617	1024027.280884	44.959053
3505.867543	1023918.811832	44.964058
3505.739901	1023811.704715	44.969063
3505.718894	1023691.004781	44.974068
3505.989431	1023565.309590	44.979073
3505.698179	1023466.657793	44.984077
3505.713985	1023358.451875	44.989082
3505.455749	1023260.081873	44.994087
3505.591852	1023127.708831	44.999092
3505.599688	1023023.085318	45.004097
3505.853308	1022940.333409	45.009101
3505.824541	1022808.852673	45.014106
3505.480075	1022696.426765	45.019111
3505.636701	1022596.328313	45.024116
3505.797048	1022479.160317	45.029121
3505.743081	1022356.788541	45.034125
3505.857373	1022230.022424	45.039130
3505.664574	1022135.403995	45.044135
3505.688064	1022032.214088	45.049140
3505.804146	1021926.582479	45.054145
3505.769171	1021814.960753	45.059149
3505.433148	1021711.630189	45.064154
3505.603155	1021592.890312	45.069159
3505.752710	1021487.826855	45.074164
3505.644094	1021389.787336	45.079169
3505.586213	1021250.806512	45.084173
3505.765783	1021145.343723	45.089178
3505.607562	1021047.985368	45.094183
3505.639498	1020929.060187	45.099188
3505.345501	1020846.658581	45.104193
3505.245844	1020749.091389	45.109197
3505.534038	1020629.632643	45.114202
3505.270888	1020529.566443	45.119207
3505.268184	1020430.134617	45.124212
3505.682064	1020313.946724	45.129217
3505.518803	1020202.993116	45.134221
3505.319146	1020107.662514	45.139226
3505.079839	1020002.829322	45.144231
3505.178361	1019892.117497	45.149236
3505.057682	1019809.089996	45.154241
3505.177662	1019705.065236	45.159245
3505.499933	1019597.997539	45.164250
3505.516241	1019515.816339	45.169255
3505.609475	1019409.850040	45.174260
3505.589655	1019295.847076	45.179265
3505.220134	1019178.600387	45.184269
3505.703413	1019078.773492	45.189274
3505.434194	1018980.718323	45.194279
3505.300160	1018881.668828	45.199284
3505.441306	1018781.504863	45.204289
3505.445830	1018679.614925	45.209293
3505.578909	1018558.682092	45.214298
3505.172883	1018462.775294	45.219303
3505.381882	1018351.917863	45.224308
3504.940551	1018253.975389	45.229313
3505.053651	1018166.906223	45.234317
3505.457336	1018060.281046	45.239322
3505.006451	1017961.461601	45.244327
3505.014930	1017859.459082	45.249332
3505.007709	1017780.264981	45.254337
3505.043176	1017707.274260	45.259341
3505.220198	1017594.563109	45.264346
3505.223290	1017488.963642	45.269351
3505.308102	1017373.545599	45.274356
3505.019303	1017295.361648	45.279361
3504.895607	1017187.836159	45.284365
3505.078224	1017075.793132	45.289370
3504.945651	1016989.231511	45.294375
3505.019867	1016905.546566	45.299380
3504.764912	1016825.409121	45.304385
3505.062988	1016726.250443	45.309389
3505.185284	1016624.595052	45.314394
3504.934341	1016520.087030	45.319399
3504.919543	1016406.315814	45.324404
3504.887256	1016333.415487	45.329409
3505.028337	1016228.449161	45.334413
3504.836909	1016131.108061	45.339418
3504.996587	1016055.454209	45.344423
3504.962720	1015960.122953	45.349428
3504.703879	1015863.662092	45.354433
3504.878166	1015772.079752	45.359437
3504.906096	1015687.316325	45.364442
3504.137135	1015602.682868	45.369447
3504.594267	1015498.039221	45.374452
3504.560013	1015426.486763	45.379457
3504.573940	1015357.061563	45.384461
3504.933697	1015265.052041	45.389466
3504.696915	1015160.322209	45.394471
3504.699467	1015067.300195	45.399476
3504.734077	1014991.361330	45.404481
3504.662666	1014892.813800	45.409485
3504.898231	1014821.403413	45.414490
3504.454395	1014729.226168	45.419495
3504.704844	1014622.852376	45.424500
3504.849885	1014545.529790	45.429505
3504.660512	1014456.510781	45.434509
3504.914361	1014352.170649	45.439514
3504.590024	1014274.921652	45.444519
3504.569947	1014199.855140	45.449524
3504.389639	1014115.393671	45.454529
3504.597683	1014034.071882	45.459533
3504.431432	1013938.436807	45.464538
3504.223525	1013838.630730	45.469543
3504.734612	1013754.147089	45.474548
3504.746717	1013680.622324	45.479553
3504.411550	1013593.653289	45.484557
3504.725217	1013511.043912	45.489562
3504.471340	1013442.998987	45.494567
3504.473821	1013330.813901	45.499572
3504.347098	1013242.251014	45.504577
3504.525979	1013157.424611	45.509581
3504.388168	1013074.883195	45.514586
3504.253658	1012985.054789	45.519591
3504.499768	1012911.384301	45.524596
3504.668747	1012824.903179	45.529601
3504.398565	1012755.104113	45.534605
3504.544630	1012680.475678	45.539610
3504.098956	1012590.109367	45.544615
3504.439084	1012499.417893	45.549620
3504.396498	1012436.571823	45.554625
3504.362441	1012357.208615	45.559629
3504.562412	1012278.971529	45.564634
3504.257919	1012187.992617	45.569639
3504.236558	1012084.821605	45.574644
3504.567645	1012018.606156	45.579649
3504.320410	1011940.826643	45.584653
3504.202668	1011859.235646	45.589658
3504.262924	1011798.988734	45.594663
3504.727107	1011717.299840	45.599668
3504.568811	1011631.825890	45.604673
3504.217522	1011556.875848	45.609677
3504.434862	1011471.920572	45.614682
3504.514158	1011365.513442	45.619687
3504.478484	1011276.515984	45.624692
3504.817718	1011224.087421	45.629697
3504.364097	1011132.047174	45.634701
3504.519867	1011040.099395	45.639706
3504.375817	1010963.746944	45.644711
3504.302339	1010876.498479	45.649716
3504.432996	1010800.390090	45.654721
3504.332253	1010729.954964	45.659725
3504.306132	1010651.635352	45.664730
3504.133215	1010567.410959	45.669735
3504.313334	1010483.321522	45.674740
3504.207107	1010407.149660	45.679745
3504.254676	1010323.662759	45.684749
3504.787041	1010233.389084	45.689754
3504.085389	1010170.917839	45.694759
3504.197088	1010088.583116	45.699764
3504.101389	1010001.033199	45.704769
3503.945409	1009937.206044	45.709773
3504.265906	1009859.595854	45.714778
3503.740466	1009776.098029	45.719783
3503.976435	1009700.151829	45.724788
3504.393862	1009653.041414	45.729793
3504.174259	1009577.168592	45.734797
3504.141420	1009494.654614	45.739802
3504.151846	1009426.614809	45.744807
3504.236539	1009340.774493	45.749812
3504.118501	1009255.063462	45.754817
3503.823475	1009169.671884	45.759821
3504.130098	1009020.316657	45.764826
3504.125602	1008825.612644	45.769831
3504.152085	1008560.126309	45.774836
3504.206596	1008260.013362	45.779841
3503.938368	1007903.742335	45.784845
3503.842895	1007442.507913	45.789850
3503.826173	1006927.935044	45.794855
3503.755227	1006346.902202	45.799860
3503.617640	1005718.551538	45.804865
3503.374673	1005010.773350	45.809869
3503.513490	1004212.853239	45.814874
3503.207864	1003365.172475	45.819879
3503.334577	1002464.742094	45.824884
3503.222663	1001483.615225	45.829889
3502.823633	1000409.686197	45.834893
3502.926143	999275.489695	45.839898
3502.456036	998056.136565	45.844903
3502.840210	996737.211638	45.849908
3502.585883	995357.185653	45.854913
3502.121702	993913.312099	45.859917
3502.581077	992344.911464	45.864922
3502.204710	990716.729183	45.869927
3501.674143	989012.896695	45.874932
3501.419683	987206.246209	45.879937
3501.408815	985331.338167	45.884941
3501.188306	983355.371829	45.889946
3500.472474	981287.276688	45.894951
3500.749330	979164.915953	45.899956
3500.423689	976951.150877	45.904961
3499.930059	974641.501902	45.909965
3500.014327	972240.427570	45.914970
3499.396707	969754.876859	45.919975
3499.169858	967170.754631	45.924980
3498.921027	964511.216038	45.929985
3498.488630	961777.459310	45.934989
3498.484978	958945.058936	45.939994
3497.951073	956022.271422	45.944999
3497.304806	953062.403685	45.950004
3497.294960	950057.589055	45.955009
3496.537579	946975.853779	45.960013
3496.281481	943796.259302	45.965018
3495.694562	940513.501054	45.970023
3495.072923	937166.504047	45.975028
3494.915980	933732.319499	45.980033
3494.394037	930202.378220	45.985037
3493.964269	926614.798253	45.990042
3492.947235	922933.895704	45.995047
3492.773404	919137.598297	46.000052
3492.369280	915264.502123	46.005057
3491.506622	911345.360641	46.010061
3490.871992	907308.386346	46.015066
3490.161792	903210.662054	46.020071
3489.855841	899036.636411	46.025076
3489.325709	894768.767146	46.030081
3488.425929	890403.509215	46.035085
3488.353877	885950.741505	46.040090
3487.102396	881422.839795	46.045095
3486.753936	876803.023232	46.050100
3486.105512	872123.931436	46.055105
3485.304846	867321.408457	46.060109
3484.335542	862420.970491	46.065114
3483.499855	857487.966448	46.070119
3482.884768	852451.636577	46.075124
3482.110867	847320.805300	46.080129
3481.380961	842120.180948	46.085133
3480.533584	836834.582887	46.090138
3479.490777	831453.213960	46.095143
3478.750519	825992.873785	46.100148
3477.836454	820446.452327	46.105153
3477.012722	814808.360530	46.110157
3476.409679	809062.229239	46.115162
3475.428670	803278.600952	46.120167
3474.585119	797375.648639	46.125172
3473.958712	791388.953647	46.130177
3472.635688	785309.473819	46.135181
3472.296619	779137.409573	46.140186
3470.913009	772899.494516	46.145191
3469.826499	766570.613092	46.150196
3469.098918	760154.949029	46.155201
3467.918864	753642.225221	46.160205
3466.898515	747027.732157	46.165210
3465.908122	740344.576325	46.170215
3464.618463	733591.394972	46.175220
3463.608294	726739.958619	46.180225
3461.715281	719779.100654	46.185229
3461.093667	712727.360118	46.190234
3459.610498	705631.875773	46.195239
3458.176445	698432.573481	46.200244
3457.457628	691163.442643	46.205249
3455.628205	683797.134065	46.210253
3454.795620	676337.171426	46.215258
3452.974339	668807.477176	46.220263
3451.822259	661209.135030	46.225268
3450.509062	653523.809965	46.230273
3449.375682	645751.274250	46.235277
3448.250081	637875.275434	46.240282
3446.635127	629924.695957	46.245287
3445.320688	621891.260457	46.250292
3444.172326	613784.582923	46.255297
3442.678300	605597.358030	46.260301
3441.025024	597300.903460	46.265306
3438.976034	588939.515592	46.270311
3437.598542	580494.030640	46.275316
3436.113393	571988.677908	46.280321
3434.342938	563398.552155	46.285325
3432.667590	554720.822465	46.290330
3430.803945	545977.680142	46.295335
3429.210364	537144.631013	46.300340
3427.779574	528209.440205	46.305345
3425.823499	519230.475834	46.310349
3424.425638	510179.415617	46.315354
3422.224113	501051.396214	46.320359
3420.389029	491821.093876	46.325364
3418.403987	482540.783343	46.330369
3416.609568	473186.931122	46.335373
3414.849896	463763.970908	46.340378
3412.531037	454266.790944	46.345383
3410.559699	444676.232917	46.350388
3408.177905	435035.353405	46.355393
3406.006639	425343.273653	46.360397
3403.989775	415555.476708	46.365402
3401.634806	405731.334341	46.370407
3399.741045	395807.662333	46.375412
3397.371220	385814.652041	46.380417
3394.446740	375801.930209	46.385421
3392.337294	365710.164372	46.390426
3389.773065	355551.660632	46.395431
3386.918487	345338.459553	46.400436
3384.466445	335084.111524	46.405441
3381.639183	324789.214826	46.410445
3379.528114	314410.886403	46.415450
3376.635939	304019.658230	46.420455
3374.053347	293572.050018	46.425460
3371.134455	283035.986498	46.430465
3368.053461	272465.265810	46.435469
3365.057973	261866.218472	46.440474
3361.881914	251241.011775	46.445479
3358.701286	240559.223251	46.450484
3355.777569	229842.861907	46.455489
3352.606984	218995.586223	46.460493
3349.197644	208221.166478	46.465498
3345.402266	197416.976455	46.470503
3341.840386	186574.991219	46.475508
3337.889620	175726.041697	46.480513
3333.802438	164874.984017	46.485517
3330.312110	154001.846118	46.490522
3325.812458	143121.288028	46.495527
3321.617607	132213.226030	46.500532
3317.278640	121325.721877	46.505537
3312.116472	110470.831425	46.510541
3307.083109	99627.405812	46.515546
3301.658781	88786.409322	46.520551
3295.302579	77977.219806	46.525556
3289.305250	67240.288365	46.530561
3281.274655	56582.080536	46.535565
3270.857980	46080.442680	46.540570
3243.435681	36141.573389	46.545575
3198.373894	26969.460743	46.550580
3144.700056	18618.277270	46.555585
3091.561838	11099.338110	46.560589
3041.641845	4485.385337	46.565594
2936.402362	504.209284	46.570599
2749.342413	373.082070	46.575604
2655.547381	370.461515	46.580609
2655.881458	348.709808	46.585613
2714.918693	318.362770	46.590618
2790.037565	316.285482	46.595623
2852.568077	334.984274	46.600628
2890.028621	332.458490	46.605633
2903.114639	319.145199	46.610637
2899.840024	314.064025	46.615642
2889.096200	306.349303	46.620647
2877.060958	312.474900	46.625652
2868.632462	321.560028	46.630657
2863.260706	308.468873	46.635661
2860.971968	307.302429	46.640666
2859.553603	290.181375	46.645671
2858.179368	286.032117	46.650676
2856.826613	280.988209	46.655681
2854.438519	292.093998	46.660685
2852.008785	308.745499	46.665690
2849.197976	292.043307	46.670695
2845.519526	292.380929	46.675700
2842.641235	288.036485	46.680705
2839.215682	293.738370	46.685709
2836.654123	301.644131	46.690714
2833.900590	301.347668	46.695719
2830.263196	288.748794	46.700724
2827.581511	272.028900	46.705729
2824.370188	288.504404	46.710733
2820.800280	278.065027	46.715738
2817.689670	272.850228	46.720743
2814.455253	274.287222	46.725748
2811.952428	267.826997	46.730753
2808.054180	286.247685	46.735757
2804.463074	273.600860	46.740762
2801.254955	263.751473	46.745767
2797.922397	282.290406	46.750772
2794.741347	260.868420	46.755777
2790.937252	262.041140	46.760781
2788.359091	272.807732	46.765786
2785.084383	271.986268	46.770791
2781.721268	262.167279	46.775796
2778.632138	248.482503	46.780801
2775.094319	272.049733	46.785805
2771.894339	269.672669	46.790810
2768.235324	276.468228	46.795815
2764.480151	251.181299	46.800820
2761.631515	257.351775	46.805825
2758.237534	279.686051	46.810829
2754.637094	269.148267	46.815834
2751.134319	256.019620	46.820839
2747.695118	251.811108	46.825844
2744.804006	256.404861	46.830849
2741.075009	257.501298	46.835853
2737.994772	264.988278	46.840858
2734.190992	251.593294	46.845863
2730.689301	257.577174	46.850868
2727.554489	260.056296	46.855873
2724.127086	244.212529	46.860877
2720.692965	251.367197	46.865882
2716.954071	259.421694	46.870887
2714.035778	266.837885	46.875892
2710.391437	262.972379	46.880897
2706.919257	257.166946	46.885901
2703.108006	251.011180	46.890906
2700.213288	263.472994	46.895911
2696.337509	261.274073	46.900916
2693.206280	251.482903	46.905921
2689.303756	268.222424	46.910925
2686.077998	260.978104	46.915930
2683.164584	259.450563	46.920935
2679.822285	252.920160	46.925940
2675.712316	260.957822	46.930945
2672.162763	264.997923	46.935949
2669.304009	260.473459	46.940954
2665.945840	249.023925	46.945959
2661.530660	255.958990	46.950964
2658.672750	253.964078	46.955969
2655.013614	241.148354	46.960973
2651.417012	231.657588	46.965978
2648.238625	248.015495	46.970983
2644.512671	261.391934	46.975988
2641.450225	238.782504	46.980993
2637.999811	231.001121	46.985997
2634.851079	235.013617	46.991002
2631.620891	236.211448	46.996007
2627.743228	245.799184	47.001012
2624.625990	240.754664	47.006017
2620.374722	240.441144	47.011021
2616.561136	231.956398	47.016026
2613.376115	230.004295	47.021031
2610.174009	242.677400	47.026036
2607.077767	214.360387	47.031041
2602.749117	244.320690	47.036045
2599.517739	244.831929	47.041050
2596.521022	241.687377	47.046055
2592.641531	226.782327	47.051060
2589.480389	234.378666	47.056065
2585.920766	239.358026	47.061069
2582.279452	227.515462	47.066074
2579.097622	238.532251	47.071079
2575.195132	224.352138	47.076084
2571.612986	223.124122	47.081089
2568.362552	248.860535	47.086093
2564.715692	238.322645	47.091098
2561.575422	227.473944	47.096103
2558.231621	239.922221	47.101108
2554.682072	213.926942	47.106113
2551.040690	226.185448	47.111117
2547.619985	230.963162	47.116122
2544.118321	224.555005	47.121127
2540.474708	237.909693	47.126132
2537.141473	230.216867	47.131137
2533.367693	229.645513	47.136141
2530.051340	232.923814	47.141146
2526.905554	214.466499	47.146151
2523.175214	219.725981	47.151156
2520.160914	223.278048	47.156161
2516.417856	234.729514	47.161165
2512.344672	233.216999	47.166170
2509.205656	222.198050	47.171175
2505.523652	217.014796	47.176180
2502.475125	233.343416	47.181185
2498.854602	233.820710	47.186189
2495.158226	229.020812	47.191194
2491.532955	217.717647	47.196199
2488.424437	218.985144	47.201204
2484.982636	205.068596	47.206209
2481.554373	220.686413	47.211213
2478.035616	226.334333	47.216218
2474.176675	215.245210	47.221223
2470.567251	222.640469	47.226228
2467.491150	228.500890	47.231233
2463.854111	228.875763	47.236237
2460.430374	213.366502	47.241242
2457.099573	211.909266	47.246247
2453.122724	234.826492	47.251252
2450.021383	213.068967	47.256257
2446.465895	200.799503	47.261261
2442.978095	208.454184	47.266266
2439.721436	216.780244	47.271271
2435.849705	234.034617	47.276276
2432.768856	209.100364	47.281281
2429.274011	201.916557	47.286285
2425.882872	215.023257	47.291290
2421.867070	224.959585	47.296295
2418.560919	218.267698	47.301300
2415.211994	198.378925	47.306305
2411.330018	205.458186	47.311309
2407.952230	220.190806	47.316314
2404.501787	224.037294	47.321319
2400.795365	216.965135	47.326324
2397.705800	199.398626	47.331329
2394.343197	207.921707	47.336333
2390.517304	208.037335	47.341338
2386.835637	208.704898	47.346343
2383.478408	207.762467	47.351348
2380.427359	208.492360	47.356353
2376.615371	228.507862	47.361357
2373.084863	207.446511	47.366362
2369.256570	201.015869	47.371367
2365.854618	214.510383	47.376372
2362.590782	205.278036	47.381377
2359.225068	201.265564	47.386381
2356.094941	200.773614	47.391386
2352.628987	198.381816	47.396391
2348.558204	212.615920	47.401396
2345.135558	213.095772	47.406401
2341.456271	202.489796	47.411405
2338.280826	185.850404	47.416410
2334.302129	202.837025	47.421415
2331.027975	215.534695	47.426420
2327.836351	198.156416	47.431425
2324.404898	188.411045	47.436429
2320.568940	198.747457	47.441434
2317.287524	196.200057	47.446439
2313.586515	192.325280	47.451444
2310.297335	194.529230	47.456449
2306.965062	195.184587	47.461453
2303.126499	202.850901	47.466458
2299.946546	197.469743	47.471463
2296.258347	198.567256	47.476468
2292.641556	199.304170	47.481473
2288.874668	191.216500	47.486477
2285.600785	208.306002	47.491482
2282.478795	205.726897	47.496487
2279.136486	202.568657	47.501492
2275.258588	182.960493	47.506497
2271.861051	190.454835	47.511501
2268.298883	188.556115	47.516506
2264.807015	184.962651	47.521511
2260.991417	201.803425	47.526516
2257.774652	202.507624	47.531521
2254.073719	192.345253	47.536525
2250.833166	179.143738	47.541530
2247.469229	184.834960	47.546535
2243.791382	200.887302	47.551540
2240.375777	208.003860	47.556545
2236.368700	192.804053	47.561549
2232.950675	179.337153	47.566554
2229.739789	186.464134	47.571559
2226.092039	196.451987	47.576564
2223.086111	196.582998	47.581569
2219.299098	202.529281	47.586573
2215.942574	184.109223	47.591578
2212.636941	183.338693	47.596583
2208.415031	177.141274	47.601588
2204.996847	186.926621	47.606593
2201.533610	203.108425	47.611597
2198.148567	212.988651	47.616602
2195.067676	198.052702	47.621607
2191.095415	181.418756	47.626612
2188.172481	185.137478	47.631617
2184.410450	193.835713	47.636621
2180.415846	178.504081	47.641626
2177.298812	185.843381	47.646631
2173.703188	204.446079	47.651636
2170.259245	197.693503	47.656641
2166.696195	189.818908	47.661645
2163.171501	189.637757	47.666650
2159.801462	191.097973	47.671655
2156.129503	196.567769	47.676660
2153.188243	197.935857	47.681665
2149.552485	202.577150	47.686669
2145.849418	197.385242	47.691674
2142.479212	197.514420	47.696679
2138.649713	205.253494	47.701684
2135.533851	172.404834	47.706689
2131.955219	196.991153	47.711693
2128.280080	204.479949	47.716698
2124.889278	191.009994	47.721703
2121.246328	184.724231	47.726708
2118.036728	168.507024	47.731713
2114.066823	189.958492	47.736717
2110.704658	194.980440	47.741722
2107.429292	180.763827	47.746727
2103.536547	195.102807	47.751732
2100.477106	184.172490	47.756737
2096.841361	167.357144	47.761741
2093.459080	180.954418	47.766746
2090.139780	197.353901	47.771751
2086.126139	185.339094	47.776756
2082.936516	190.712982	47.781761
2079.199748	193.329619	47.786765
2075.767675	181.276107	47.791770
2072.390017	176.960534	47.796775
2068.336248	183.680093	47.801780
2065.192309	200.613847	47.806785
2061.946300	180.360223	47.811789
2058.387121	186.626394	47.816794
2055.211417	193.567405	47.821799
2050.680234	186.949753	47.826804
2047.718084	176.514521	47.831809
2044.459826	169.290335	47.836813
2041.072195	175.221709	47.841818
2037.471488	199.205791	47.846823
2033.566225	184.829634	47.851828
2030.312693	162.890693	47.856833
2027.201469	175.198716	47.861837
2022.974399	198.407262	47.866842
2020.013218	189.884879	47.871847
2016.136764	175.946924	47.876852
2013.186914	176.606801	47.881857
2009.372938	190.270785	47.886861
2005.647629	188.399208	47.891866
2002.340546	171.134022	47.896871
1998.758210	182.465120	47.901876
1995.044351	184.545609	47.906881
1991.359623	193.652304	47.911885
1987.865568	188.926750	47.916890
1985.137906	168.501858	47.921895
1981.349990	187.087582	47.926900
1977.657667	181.402236	47.931905
1974.180475	178.416149	47.936909
1971.044634	177.166204	47.941914
1967.832790	183.625681	47.946919
1963.996628	176.606270	47.951924
1960.303598	166.752846	47.956929
1956.612947	172.279371	47.961933
1953.015633	193.193446	47.966938
1949.717845	176.370972	47.971943
1946.310192	185.001763	47.976948
1943.041206	192.871099	47.981953
1939.265609	176.065801	47.986957
1935.682547	175.072446	47.991962
1932.041674	177.386264	47.996967
1928.701389	172.204579	48.001972
1925.497631	170.384127	48.006977
1921.894090	171.688433	48.011981
1918.404749	178.239282	48.016986
1915.051253	162.255771	48.021991
1911.239604	166.443686	48.026996
1908.069560	173.656374	48.032001
1904.330938	164.454586	48.037005
1900.667851	173.847566	48.042010
1897.590125	165.439681	48.047015
1893.648171	175.845233	48.052020
1889.787547	179.780118	48.057025
1886.526903	171.967571	48.062029
1883.066829	168.238350	48.067034
1879.882377	174.496533	48.072039
1876.264861	185.585972	48.077044
1873.121097	168.540747	48.082049
1869.312073	161.216440	48.087053
1865.788876	174.125376	48.092058
1862.113860	166.028146	48.097063
1858.596634	179.846731	48.102068
1855.124692	180.458645	48.107073
1852.279887	175.585113	48.112077
1848.385919	172.689063	48.117082
1844.787899	162.259220	48.122087
1841.223662	184.997888	48.127092
1837.559575	186.928286	48.132097
1834.394763	181.690765	48.137101
1830.997681	168.015278	48.142106
1827.194056	174.090146	48.147111
1823.639136	170.464499	48.152116
1820.378462	167.693832	48.157121
1816.596036	160.536817	48.162125
1812.973785	168.453129	48.167130
1809.598231	159.587673	48.172135
1806.031056	173.678988	48.177140
1802.812760	173.660047	48.182145
1799.411889	156.072316	48.187149
1796.085697	159.625784	48.192154
1792.655646	161.719817	48.197159
1788.519649	179.280059	48.202164
1785.259142	164.767527	48.207169
1781.670036	154.072669	48.212173
1778.054880	156.662674	48.217178
1774.826358	153.713302	48.222183
1771.239994	169.922422	48.227188
1767.571167	177.271518	48.232193
1763.962340	158.660704	48.237197
1760.583231	155.914147	48.242202
1756.593697	148.696742	48.247207
1753.819548	166.245462	48.252212
1750.594082	148.953877	48.257217
1746.848772	154.727056	48.262221
1743.166603	161.224356	48.267226
1739.780942	170.199720	48.272231
1735.837252	164.079127	48.277236
1732.446062	175.227846	48.282241
1729.601089	165.268572	48.287245
1725.908595	154.236954	48.292250
1722.246145	163.304948	48.297255
1718.770118	164.143407	48.302260
1715.120755	166.297043	48.307265
1711.672235	146.787974	48.312269
1708.007339	167.412650	48.317274
1704.809439	163.079052	48.322279
1701.089144	165.671251	48.327284
1697.565166	155.737326	48.332289
1694.134837	148.450082	48.337293
1690.357742	158.637821	48.342298
1686.993321	156.105115	48.347303
1683.555014	170.741645	48.352308
1680.589862	158.962631	48.357313
1677.091756	152.426739	48.362317
1673.023999	167.689773	48.367322
1669.678876	163.285487	48.372327
1665.841611	153.819869	48.377332
1662.387376	161.278410	48.382337
1659.290168	169.332377	48.387341
1655.510928	177.499681	48.392346
1652.334343	165.606805	48.397351
1648.442611	152.104022	48.402356
1644.960969	146.467080	48.407361
1641.906572	168.600879	48.412365
1637.855180	163.041772	48.417370
1634.956198	148.964314	48.422375
1631.002511	162.854884	48.427380
1627.855896	158.221357	48.432385
1624.368192	139.928056	48.437389
1620.798165	155.010120	48.442394
1617.307660	157.323048	48.447399
1613.366433	166.736193	48.452404
1609.730941	172.278435	48.457409
1606.702383	156.963712	48.462413
1603.127771	155.469086	48.467418
1599.769474	157.674479	48.472423
1595.820984	158.248357	48.477428
1592.129301	154.232268	48.482433
1589.213772	162.916233	48.487437
1585.343939	175.899341	48.492442
1581.967692	158.230151	48.497447
1578.610637	147.710999	48.502452
1574.895659	148.791878	48.507457
1571.710156	144.263252	48.512461
1568.169893	161.858426	48.517466
1564.787309	157.138587	48.522471
1560.973117	159.387664	48.527476
1557.657551	153.858804	48.532481
1553.974194	154.239894	48.537485
1550.627925	146.774512	48.542490
1547.273288	142.457690	48.547495
1543.262951	159.463581	48.552500
1539.644561	164.507027	48.557505
1536.083113	159.011552	48.562509
1532.885488	142.237764	48.567514
1529.895026	143.485477	48.572519
1526.409839	160.132343	48.577524
1522.899797	161.467187	48.582529
1519.103253	153.339323	48.587533
1515.123407	139.347192	48.592538
1512.118474	140.419142	48.597543
1508.379219	157.608185	48.602548
1504.946703	161.433739	48.607553
1501.732115	147.929305	48.612557
1497.913396	147.262331	48.617562
1494.570328	140.754920	48.622567
1490.950265	143.774201	48.627572
1487.154782	149.473308	48.632577
1483.813259	162.184785	48.637581
1480.013033	150.338713	48.642586
1477.310810	140.747263	48.647591
1473.453155	138.104888	48.652596
1470.139520	152.665456	48.657601
1466.767311	155.508796	48.662605
1462.876004	162.413825	48.667610
1459.978555	129.798757	48.672615
1456.291303	157.986684	48.677620
1452.472633	161.847383	48.682625
1448.831333	154.051739	48.687629
1445.225210	139.840240	48.692634
1442.044559	136.832922	48.697639
1438.532224	144.860963	48.702644
1435.070920	160.839029	48.707649
1431.471841	149.656051	48.712653
1428.086047	138.846386	48.717658
1424.682062	138.872863	48.722663
1420.789963	141.758029	48.727668
1416.861907	155.467081	48.732673
1413.666902	150.421310	48.737677
1410.425326	135.941327	48.742682
1407.128961	140.498712	48.747687
1403.481019	153.339601	48.752692
1399.749500	149.747578	48.757697
1396.498480	139.898912	48.762701
1392.740863	143.880763	48.767706
1389.570118	166.065279	48.772711
1385.949057	151.993987	48.777716
1382.549376	127.398314	48.782721
1378.812937	132.887961	48.787725
1375.250277	151.527024	48.792730
1371.787354	142.353473	48.797735
1368.345253	141.643646	48.802740
1364.660408	144.402892	48.807745
1361.405486	137.250153	48.812749
1357.822711	151.164937	48.817754
1354.642693	153.653336	48.822759
1351.092752	142.885406	48.827764
1347.262560	139.919544	48.832769
1343.750949	142.824913	48.837773
1340.528956	156.272150	48.842778
1337.048270	163.767646	48.847783
1333.189892	149.579205	48.852788
1329.901683	134.118123	48.857793
1326.651775	144.705228	48.862797
1322.841115	163.380225	48.867802
1319.561915	133.753281	48.872807
1315.637216	133.266277	48.877812
1312.123071	140.065514	48.882817
1308.828026	144.481854	48.887821
1305.336038	149.524762	48.892826
1301.897143	135.440837	48.897831
1298.294634	133.200366	48.902836
1294.831597	146.329502	48.907841
1291.454124	140.913503	48.912845
1287.372146	142.636934	48.917850
1284.113563	132.873930	48.922855
1280.688827	140.101648	48.927860
1277.101873	142.609207	48.932865
1274.088852	135.600566	48.937869
1270.420419	141.129648	48.942874
1267.088538	141.403054	48.947879
1262.898666	139.775681	48.952884
1259.491302	146.630810	48.957889
1256.304457	146.836678	48.962893
1252.715072	141.547817	48.967898
1249.880996	135.833900	48.972903
1246.015955	142.325697	48.977908
1242.392478	144.137620	48.982913
1238.820102	145.906485	48.987917
1235.297285	147.071830	48.992922
1231.790246	140.919833	48.997927
1228.065076	152.203655	49.002932
1224.628298	153.579721	49.007937
1221.122015	136.229196	49.012941
1217.734014	136.906382	49.017946
1214.543831	137.354508	49.022951
1210.762122	144.888592	49.027956
1206.788481	146.376470	49.032961
1204.000701	129.991104	49.037965
1200.465008	133.702620	49.042970
1196.801769	132.936754	49.047975
1192.943846	137.463323	49.052980
1189.666015	146.788647	49.057985
1186.702696	141.318543	49.062989
1183.100345	132.003978	49.067994
1179.488686	125.971684	49.072999
1175.579703	144.611743	49.078004
1171.918214	135.782427	49.083009
1168.625281	131.040513	49.088013
1164.694133	146.894282	49.093018
1161.930335	130.944457	49.098023
1158.066835	140.408495	49.103028
1154.778795	139.654009	49.108033
1151.101500	134.128565	49.113037
1147.479325	147.750038	49.118042
1144.352673	119.109023	49.123047
1140.803025	122.782423	49.128052
1137.175510	145.857694	49.133057
1133.767839	155.220656	49.138061
1130.304292	147.447261	49.143066
1127.209096	135.010259	49.148071
1123.330803	146.095567	49.153076
1119.481457	138.440919	49.158081
1115.970650	130.622468	49.163085
1112.372131	145.082992	49.168090
1109.071670	134.223824	49.173095
1105.963398	139.510464	49.178100
1102.172818	144.545048	49.183105
1098.845401	145.973949	49.188109
1094.826060	132.689247	49.193114
1091.742092	146.522269	49.198119
1087.911509	157.436167	49.203124
1084.457186	147.574284	49.208129
1081.508093	135.510836	49.213133
1077.598296	134.550762	49.218138
1074.162078	128.572429	49.223143
1070.665002	124.611429	49.228148
1066.817077	140.642277	49.233153
1063.927550	152.681464	49.238157
1060.064818	147.509952	49.243162
1056.623722	142.853716	49.248167
1053.294723	130.548090	49.253172
1049.819573	133.670521	49.258177
1046.120091	137.200019	49.263181
1042.141960	137.352056	49.268186
1039.113924	144.935806	49.273191
1035.457742	151.787818	49.278196
1031.837516	150.054999	49.283201
1028.666890	120.483685	49.288205
1024.882709	137.932142	49.293210
1021.788394	146.480567	49.298215
1018.393576	126.323517	49.303220
1014.776944	119.836787	49.308225
1011.222105	134.674359	49.313229
1007.372828	143.149349	49.318234
1004.002209	144.245685	49.323239
1000.441346	130.956680	49.328244
996.817898	131.343364	49.333249
993.831368	133.423434	49.338253
990.050421	131.122727	49.343258
986.439130	116.946547	49.348263
983.004386	139.371702	49.353268
979.694316	137.752841	49.358273
976.246574	128.845253	49.363277
972.377624	126.376687	49.368282
969.335216	120.136299	49.373287
965.503671	141.186724	49.378292
961.986710	137.708393	49.383297
958.321523	115.672019	49.388301
954.807899	121.484845	49.393306
951.520814	134.172403	49.398311
947.860828	139.266786	49.403316
944.358883	119.030418	49.408321
941.414309	140.930444	49.413325
937.243129	146.425601	49.418330
934.176242	137.582109	49.423335
930.592160	126.143571	49.428340
926.946054	125.315738	49.433345
923.396251	131.031963	49.438349
919.742241	131.973103	49.443354
916.646679	128.515383	49.448359
913.478979	125.447693	49.453364
909.827973	133.225300	49.458369
906.342115	114.327620	49.463373
902.191813	120.109759	49.468378
898.974938	123.569704	49.473383
895.421946	135.776977	49.478388
891.694561	137.066733	49.483393
888.515528	122.804543	49.488397
884.791993	127.311249	49.493402
881.180310	116.696082	49.498407
878.097745	122.021771	49.503412
874.111946	139.072489	49.508417
871.116082	114.966131	49.513421
867.474225	133.006206	49.518426
864.248261	137.722170	49.523431
860.272777	130.954549	49.528436
856.635065	116.738430	49.533441
853.490192	135.448339	49.538445
849.773482	140.047752	49.543450
846.403949	124.024915	49.548455
843.003745	112.533887	49.553460
839.312202	136.941873	49.558465
836.186044	123.272930	49.563469
832.283971	122.888714	49.568474
829.000402	127.144148	49.573479
825.408813	139.653569	49.578484
821.692986	145.584987	49.583489
818.243538	125.369038	49.588493
815.011147	125.797290	49.593498
811.284860	128.018830	49.598503
807.851481	136.869048	49.603508
804.398659	136.296725	49.608513
801.349130	105.968825	49.613517
797.621945	120.420900	49.618522
794.157414	117.043903	49.623527
790.473311	129.010955	49.628532
786.442552	139.245700	49.633537
783.541791	125.232576	49.638541
779.594782	123.981796	49.643546
776.295405	108.778541	49.648551
772.796198	109.985303	49.653556
768.892407	136.003260	49.658561
765.571902	134.676058	49.663565
762.106511	134.368826	49.668570
758.898932	126.364189	49.673575
755.584983	120.044361	49.678580
751.968459	127.395021	49.683585
749.121736	121.063343	49.688589
744.667188	135.472802	49.693594
741.595869	140.876797	49.698599
737.826763	130.974789	49.703604
734.036424	112.799504	49.708609
730.802850	110.971834	49.713613
727.296868	134.250669	49.718618
723.794473	125.904195	49.723623
720.075540	132.444628	49.728628
716.540985	129.916652	49.733633
713.277780	136.439735	49.738637
709.767750	139.929635	49.743642
706.269491	121.362930	49.748647
702.977167	119.229896	49.753652
699.538506	122.638268	49.758657
696.184607	118.924030	49.763661
692.207404	114.961254	49.768666
688.835160	114.089510	49.773671
685.373385	131.301063	49.778676
681.738651	136.550031	49.783681
678.444260	118.214845	49.788685
674.317421	113.964575	49.793690
670.852907	130.313126	49.798695
667.530410	130.353456	49.803700
664.210479	120.349702	49.808705
660.985612	102.651473	49.813709
657.040927	122.449105	49.818714
653.824225	143.072166	49.823719
650.276920	134.978682	49.828724
646.950293	118.312824	49.833729
643.616090	114.985512	49.838733
639.597493	120.436000	49.843738
636.074527	106.998952	49.848743
632.475117	107.729889	49.853748
628.651927	133.047694	49.858753
625.526001	135.834667	49.863757
621.981400	123.241069	49.868762
618.990952	103.943949	49.873767
615.684328	104.195747	49.878772
611.882077	129.113729	49.883777
608.282660	127.892060	49.888781
604.458201	121.327448	49.893786
600.892438	119.503116	49.898791
598.004367	115.006176	49.903796
594.138229	110.089749	49.908801
590.992408	98.942489	49.913805
587.182541	122.279724	49.918810
583.934416	121.172977	49.923815
580.270127	125.560160	49.928820
576.515510	127.543440	49.933825
573.223897	112.688047	49.938829
569.584191	128.874390	49.943834
566.146092	135.759848	49.948839
562.352208	116.481909	49.953844
559.164493	121.951660	49.958849
555.567821	107.661804	49.963853
552.012497	98.756877	49.968858
548.452859	101.787062	49.973863
544.998529	110.514373	49.978868
541.720239	113.389681	49.983873
538.424557	112.275720	49.988877
534.684569	114.934013	49.993882
531.122435	106.270227	49.998887
527.561121	124.663583	50.003892
524.168207	128.578041	50.008897
520.618148	115.400838	50.013901
517.136316	109.787572	50.018906
513.745859	115.094718	50.023911
510.197796	117.956301	50.028916
506.445940	122.869371	50.033921
503.094791	116.979127	50.038925
499.410304	120.299171	50.043930
495.871447	117.345484	50.048935
492.536950	107.834920	50.053940
488.937258	118.007278	50.058945
485.782525	113.987599	50.063949
482.274971	128.720287	50.068954
478.576501	96.739302	50.073959
475.530864	99.994767	50.078964
471.675234	125.109031	50.083969
468.152678	115.134334	50.088973
464.094195	103.783761	50.093978
460.483152	106.278348	50.098983
457.546248	99.288457	50.103988
454.314094	111.785690	50.108993
450.774578	112.198660	50.113997
447.110642	116.814120	50.119002
443.479042	114.176756	50.124007
440.352956	103.396051	50.129012
436.708083	123.805770	50.134017
432.786101	124.147572	50.139021
429.216961	119.532877	50.144026
425.474617	97.501881	50.149031
422.446255	112.984767	50.154036
418.938355	131.635298	50.159041
415.705247	121.546723	50.164045
412.119310	124.034625	50.169050
408.449720	118.139035	50.174055
405.021358	114.339995	50.179060
401.455535	116.299877	50.184065
398.011928	112.603979	50.189069
394.760092	93.081760	50.194074
391.306567	105.897809	50.199079
387.618148	113.043612	50.204084
383.267832	106.992941	50.209089
380.146098	113.849419	50.214093
376.707266	135.412548	50.219098
373.602049	112.621823	50.224103
370.531359	90.249883	50.229108
366.412652	101.327877	50.234113
362.977953	106.324757	50.239117
359.363193	120.074448	50.244122
355.690281	105.085077	50.249127
352.488836	98.914801	50.254132
348.931416	106.599268	50.259137
345.686240	121.121671	50.264141
341.706896	113.935381	50.269146
338.290593	95.970305	50.274151
334.938336	104.098038	50.279156
331.092431	118.605651	50.284161
327.979605	111.483969	50.289165
324.535900	114.337088	50.294170
320.862356	105.761389	50.299175
317.626460	106.867870	50.304180
313.968202	99.831501	50.309185
310.186957	110.179037	50.314189
306.849048	126.673535	50.319194
303.670661	108.548395	50.324199
300.157374	108.645588	50.329204
296.419126	112.849814	50.334209
293.059227	120.043467	50.339213
289.137531	128.133541	50.344218
285.697694	101.842925	50.349223
282.400223	98.734859	50.354228
278.832225	122.414987	50.359233
275.608255	110.016564	50.364237
271.723904	116.506416	50.369242
268.172085	103.216838	50.374247
265.180453	100.034972	50.379252
261.231136	110.488822	50.384257
257.983145	110.045521	50.389261
254.506697	116.196613	50.394266
250.717531	118.791768	50.399271
247.093519	110.013795	50.404276
243.534318	106.770342	50.409281
240.379052	97.780382	50.414285
236.895082	120.189781	50.419290
233.147620	111.514879	50.424295
229.582459	103.513018	50.429300
226.149839	111.126221	50.434305
223.042240	112.261763	50.439309
219.815820	105.179752	50.444314
215.873423	104.182380	50.449319
212.277067	120.334267	50.454324
208.823305	103.597303	50.459329
205.494293	94.581916	50.464333
201.988909	95.841984	50.469338
198.367879	122.488812	50.474343
194.776871	109.517676	50.479348
190.895833	101.948806	50.484353
187.679319	107.479306	50.489357
184.078640	107.586069	50.494362
180.901173	105.297218	50.499367
177.573463	98.976752	50.504372
173.718237	124.820932	50.509377
170.236800	107.414315	50.514381
166.612962	104.491831	50.519386
163.154638	102.151144	50.524391
159.775308	100.734351	50.529396
156.320116	117.191720	50.534401
153.053590	103.600871	50.539405
149.258117	119.975083	50.544410
145.654567	112.882920	50.549415
142.240738	98.106622	50.554420
138.695497	111.876157	50.559425
135.507980	107.886154	50.564429
131.921212	110.965530	50.569434
128.078893	103.479186	50.574439
124.538026	105.956636	50.579444
120.925243	117.166223	50.584449
117.600538	98.490811	50.589453
114.225319	108.836949	50.594458
110.834361	100.952280	50.599463
107.445511	93.492631	50.604468
103.814676	109.598654	50.609473
100.386293	111.444345	50.614477
96.830167	125.138762	50.619482
93.220562	102.071939	50.624487
89.786041	95.012855	50.629492
85.856131	117.853675	50.634497
82.863790	103.042489	50.639501
79.179787	107.212022	50.644506
75.588425	120.337257	50.649511
72.185939	103.299137	50.654516
68.555971	101.345743	50.659521
65.047435	104.322162	50.664525
61.558363	119.129881	50.669530
57.884764	108.877671	50.674535
54.710416	95.229442	50.679540
51.386894	113.795651	50.684545
47.812937	103.038688	50.689549
44.360305	94.793443	50.694554
40.690635	112.376530	50.699559
37.330398	109.692100	50.704564
33.482990	101.997040	50.709569
29.910210	107.599899	50.714573
26.478654	108.221063	50.719578
23.303073	109.474868	50.724583
19.579331	91.187657	50.729588
15.995196	88.252394	50.734593
12.373967	102.035220	50.739597
9.063344	108.064028	50.744602
5.867649	98.456457	50.749607
2.440063	97.315748	50.754612